Fri Mar 05 18:15:24 2021

Number of Points = 14580

Depth (nm)	Load (N)	Time (s)
1.792992	92.091484	0.000000
1.405825	85.572494	0.005005
0.471106	54.867831	0.010010
-0.799046	9.265357	0.015014
-4.948524	-4.308097	0.020019
-10.046005	-7.517774	0.025024
-14.993966	-11.214925	0.030029
-19.477065	-7.161245	0.035034
-23.379935	-2.454207	0.040038
-27.527232	-8.404833	0.045043
-31.014885	-14.459106	0.050048
-34.683495	-5.233528	0.055053
-38.384643	-0.829889	0.060058
-42.068988	-13.097612	0.065062
-45.884406	-12.859462	0.070067
-49.860117	-10.094642	0.075072
-53.118675	-5.947677	0.080077
-57.001472	-9.209118	0.085082
-60.725956	-11.680512	0.090086
-64.596164	-7.782882	0.095091
-68.549497	-17.120190	0.100096
-72.073825	-12.848796	0.105101
-76.078857	-8.876021	0.110106
-79.633270	-15.444703	0.115110
-83.773099	-6.645352	0.120115
-87.209698	-2.758522	0.125120
-90.489798	-5.286581	0.130125
-94.617664	-9.175920	0.135130
-98.605907	-9.894147	0.140134
-102.674545	-8.210415	0.145139
-105.991950	-14.052040	0.150144
-109.720582	-11.873760	0.155149
-114.055087	1.127818	0.160154
-117.899852	-6.539367	0.165158
-121.378066	5.023005	0.170163
-125.002268	-3.688632	0.175168
-128.498439	-7.781216	0.180173
-132.665390	1.254363	0.185178
-136.190081	-4.927889	0.190182
-139.914139	0.222313	0.195187
-143.746957	-7.162878	0.200192
-147.185439	-10.414648	0.205197
-151.247221	-5.789287	0.210202
-154.894773	-5.006887	0.215206
-158.766446	-9.556751	0.220211
-162.857228	-9.752297	0.225216
-166.295785	-10.912954	0.230221
-170.150035	-4.393614	0.235226
-173.709590	-5.541259	0.240230
-177.659218	-6.976734	0.245235
-181.299845	-9.431359	0.250240
-185.013927	-12.564971	0.255245
-188.865801	-2.664941	0.260250
-192.366962	-13.912958	0.265254
-196.316126	-5.358323	0.270259
-200.046400	-7.962617	0.275264
-204.124602	-6.822824	0.280269
-207.999899	-2.485757	0.285274
-211.396461	-7.614421	0.290278
-215.300881	-5.639739	0.295283
-218.721942	-2.930056	0.300288
-222.564224	-8.555273	0.305293
-226.641710	-6.224938	0.310298
-230.309057	-6.814390	0.315302
-234.294772	-13.847010	0.320307
-237.807223	-9.870594	0.325312
-241.465810	0.132707	0.330317
-245.260486	-15.048667	0.335322
-248.784185	-16.991987	0.340326
-252.832136	-13.860489	0.345331
-256.461950	-8.651041	0.350336
-260.171566	-14.142826	0.355341
-264.436430	0.470592	0.360346
-268.142421	-7.713663	0.365350
-271.444321	-8.646821	0.370355
-275.393908	-13.141474	0.375360
-278.852584	-16.355132	0.380365
-283.116533	-3.452852	0.385370
-286.414585	-9.652128	0.390374
-290.522435	-11.290818	0.395379
-293.909183	-12.090549	0.400384
-297.544714	-13.755743	0.405389
-301.714642	-10.681963	0.410394
-305.597084	-10.910526	0.415398
-309.370866	2.886543	0.420403
-313.350618	-10.817504	0.425408
-317.089914	-10.780315	0.430413
-320.651907	-9.665968	0.435418
-324.166390	-16.388881	0.440422
-327.996394	-10.149144	0.445427
-331.692602	-16.926612	0.450432
-335.441933	-11.977093	0.455437
-339.346517	-6.700000	0.460442
-342.964605	-14.447147	0.465446
-346.821328	-3.822277	0.470451
-350.871367	-1.615966	0.475456
-354.484300	-9.315035	0.480461
-358.419966	-2.851794	0.485466
-361.937997	-11.292988	0.490470
-365.725871	-9.404484	0.495475
-369.502226	-6.347698	0.500480
-373.053554	-9.415536	0.505485
-377.009879	-1.575421	0.510490
-380.663683	-17.622730	0.515494
-384.451656	-9.850491	0.520499
-388.031914	-9.073754	0.525504
-392.159999	-13.418279	0.530509
-396.181393	-13.148261	0.535514
-399.450635	-13.217543	0.540518
-403.381663	-3.148432	0.545523
-406.975976	-12.282282	0.550528
-410.516280	-13.306488	0.555533
-414.768958	-0.006815	0.560538
-418.428052	-15.064454	0.565542
-422.401124	-13.002782	0.570547
-425.961380	-16.378199	0.575552
-429.599985	-6.664836	0.580557
-433.414988	-7.468518	0.585562
-436.935571	-15.163277	0.590566
-441.084618	-11.255221	0.595571
-445.066304	-13.555620	0.600576
-448.163253	-15.838035	0.605581
-452.271827	-13.694748	0.610586
-455.739418	-14.844041	0.615590
-459.466534	-9.953076	0.620595
-463.623773	-11.001675	0.625600
-467.029267	-12.343798	0.630605
-471.576141	-10.359137	0.635610
-474.828328	-12.539451	0.640614
-478.475642	-6.033767	0.645619
-482.260626	-3.462712	0.650624
-486.030654	-14.782437	0.655629
-489.857115	-5.584616	0.660634
-493.508254	-2.487712	0.665638
-497.513239	-2.734238	0.670643
-501.125578	-17.539001	0.675648
-504.738297	-8.263334	0.680653
-508.968116	-2.881983	0.685658
-512.298818	-22.358546	0.690662
-516.084610	-10.945233	0.695667
-519.904364	-15.504362	0.700672
-523.532240	-10.750580	0.705677
-527.556176	-5.477779	0.710682
-531.213160	-16.517436	0.715686
-534.940987	1.287581	0.720691
-538.779416	-14.698429	0.725696
-542.543290	-8.306497	0.730701
-546.601073	-6.163278	0.735706
-550.047267	-8.935401	0.740710
-553.703428	-1.841558	0.745715
-557.480618	-10.259969	0.750720
-560.974584	-0.421287	0.755725
-565.039918	-4.401789	0.760730
-568.699039	-16.762544	0.765734
-572.867281	-9.424440	0.770739
-576.683958	-8.773656	0.775744
-579.867124	-10.859195	0.780749
-583.921611	-13.190305	0.785754
-587.905111	-11.106194	0.790758
-591.361627	4.633882	0.795763
-595.095096	-5.739014	0.800768
-598.957170	-10.248674	0.805773
-602.823221	-4.874818	0.810778
-606.196486	-13.967967	0.815782
-610.399640	-12.108924	0.820787
-613.882741	-6.774159	0.825792
-617.592430	-9.220227	0.830797
-621.780841	-2.127976	0.835802
-625.094451	-12.448051	0.840806
-629.016458	-5.855677	0.845811
-632.793820	-7.037217	0.850816
-636.311205	-15.164264	0.855821
-640.429766	-7.401894	0.860826
-644.074762	-14.638051	0.865830
-647.861027	-1.671148	0.870835
-651.507038	-10.739572	0.875840
-655.486521	-12.855459	0.880845
-659.366168	-1.542050	0.885850
-662.960201	-10.308099	0.890854
-666.533411	-6.277206	0.895859
-670.139504	-6.292288	0.900864
-674.325795	-4.776452	0.905869
-677.919063	-3.028943	0.910874
-681.711816	-13.119397	0.915878
-685.678114	-8.041631	0.920883
-688.880510	-12.569826	0.925888
-692.628224	-6.956117	0.930893
-696.631971	-13.366874	0.935898
-700.548030	-13.766040	0.940902
-704.332985	-1.537284	0.945907
-708.046801	-11.022138	0.950912
-712.013327	-8.070046	0.955917
-715.760443	2.553636	0.960922
-719.306668	-8.799885	0.965926
-723.005052	-4.206427	0.970931
-726.715219	-1.233779	0.975936
-730.285342	-9.055782	0.980941
-734.500546	-2.528345	0.985946
-738.024365	-9.020466	0.990950
-742.387812	-5.709992	0.995955
-745.969549	-2.644301	1.000960
-749.457126	-13.277006	1.005965
-752.997861	2.795284	1.010970
-756.567891	-22.475836	1.015974
-760.523408	-3.298431	1.020979
-764.406245	-6.963971	1.025984
-768.178079	-14.264809	1.030989
-772.445646	-1.367450	1.035994
-775.854306	-13.966591	1.040998
-779.423615	-1.351144	1.046003
-783.168183	-2.696958	1.051008
-786.896192	-8.115565	1.056013
-790.953842	-3.276916	1.061018
-794.599251	-12.094462	1.066022
-798.399623	-5.486570	1.071027
-801.902001	-6.274973	1.076032
-805.687182	-12.551741	1.081037
-809.734062	3.834927	1.086042
-813.376885	-3.194725	1.091046
-817.298932	-0.236953	1.096051
-820.961989	-11.847598	1.101056
-824.606094	-5.420765	1.106061
-828.177566	0.234365	1.111066
-831.840096	-6.803144	1.116070
-835.790351	-4.399079	1.121075
-839.691032	-5.817615	1.126080
-843.535645	-2.514209	1.131085
-847.089479	-4.406080	1.136090
-850.585160	-13.351550	1.141094
-854.930267	3.442414	1.146099
-858.321759	-2.460391	1.151104
-862.134197	-9.071755	1.156109
-866.277374	3.887879	1.161114
-869.815606	-12.118723	1.166118
-873.421129	-14.270372	1.171123
-877.434746	-9.545855	1.176128
-880.772532	-2.781558	1.181133
-885.072624	-1.188808	1.186138
-888.350418	-7.814648	1.191142
-892.217558	3.621699	1.196147
-896.249139	-10.121879	1.201152
-899.929350	-14.410948	1.206157
-903.485877	-6.200263	1.211162
-906.965833	-8.477596	1.216166
-911.089295	-4.840909	1.221171
-915.191018	1.589847	1.226176
-918.715495	-12.395625	1.231181
-922.740089	-6.065502	1.236186
-926.097446	-10.760974	1.241190
-930.032597	-7.285255	1.246195
-933.876589	-4.535318	1.251200
-937.367336	-11.273689	1.256205
-941.093308	-2.031326	1.261210
-944.547695	-13.339236	1.266214
-948.784195	-11.788079	1.271219
-952.689084	-6.569886	1.276224
-956.310911	-12.364740	1.281229
-960.240232	-10.205093	1.286234
-963.611798	-16.390042	1.291238
-967.817500	-4.213463	1.296243
-971.510058	-3.851553	1.301248
-975.011369	-6.511724	1.306253
-979.110459	0.227803	1.311258
-982.328109	-11.854351	1.316262
-986.440796	-1.305848	1.321267
-990.207189	-7.049144	1.326272
-993.635284	-7.215200	1.331277
-997.857610	-0.206772	1.336282
-1001.354259	-11.296520	1.341286
-1005.271988	-11.150856	1.346291
-1008.936153	-17.899222	1.351296
-1012.559514	-15.299566	1.356301
-1016.526674	1.487831	1.361306
-1020.161402	-4.076200	1.366310
-1024.335957	1.648870	1.371315
-1027.612834	-1.001387	1.376320
-1031.397497	-15.186327	1.381325
-1035.368123	-9.407127	1.386330
-1039.239841	-3.960709	1.391334
-1042.763958	-5.997382	1.396339
-1046.662408	4.791347	1.401344
-1049.939436	-9.009562	1.406349
-1053.883022	-4.165063	1.411354
-1057.962249	-20.050106	1.416358
-1061.717718	1.219915	1.421363
-1065.739431	-10.864380	1.426368
-1069.292843	-9.023306	1.431373
-1072.893674	-2.495793	1.436378
-1076.388328	-4.943984	1.441382
-1079.789930	-12.402871	1.446387
-1084.198067	-9.597137	1.451392
-1088.213066	-6.310235	1.456397
-1091.832171	-3.105584	1.461402
-1095.510313	-13.078038	1.466406
-1099.548969	-10.116918	1.471411
-1103.092556	-5.840959	1.476416
-1106.607073	-7.533715	1.481421
-1110.710717	-8.345310	1.486426
-1114.059392	-2.861025	1.491430
-1117.978576	-7.540443	1.496435
-1121.724477	-9.128347	1.501440
-1125.314095	-11.245876	1.506445
-1129.403225	-5.007589	1.511450
-1132.847143	-6.154933	1.516454
-1136.701437	-4.311349	1.521459
-1140.650510	-9.134179	1.526464
-1144.010285	-7.663021	1.531469
-1148.384388	-6.602000	1.536474
-1152.032213	-9.900780	1.541478
-1155.634262	-7.794749	1.546483
-1159.333964	4.227076	1.551488
-1163.018156	-4.642005	1.556493
-1167.177772	2.601113	1.561498
-1170.568878	-8.543096	1.566502
-1174.599216	-3.597785	1.571507
-1178.084176	-11.639273	1.576512
-1181.742767	-13.236318	1.581517
-1185.718165	-2.964924	1.586522
-1189.283102	-12.859139	1.591526
-1193.492625	-5.730997	1.596531
-1197.094943	-6.338808	1.601536
-1200.818175	-11.866302	1.606541
-1204.971168	-9.127980	1.611546
-1208.455737	-20.172008	1.616550
-1212.201636	-10.411967	1.621555
-1215.954196	-9.951758	1.626560
-1219.105330	-24.564167	1.631565
-1223.261473	-14.929271	1.636570
-1226.717068	-18.998285	1.641574
-1230.654194	-14.482540	1.646579
-1234.979679	-6.815371	1.651584
-1238.558017	-18.760558	1.656589
-1242.436666	-13.074587	1.661594
-1245.756549	-14.217957	1.666598
-1249.708181	-10.053096	1.671603
-1253.391796	-14.618589	1.676608
-1256.759419	-17.539419	1.681613
-1260.945839	-2.943227	1.686618
-1264.630020	-8.603023	1.691622
-1268.518752	-19.429301	1.696627
-1272.281424	-18.243559	1.701632
-1275.802436	-10.377072	1.706637
-1279.915528	-6.971643	1.711642
-1283.394970	-17.786135	1.716646
-1287.364036	-11.093712	1.721651
-1291.159634	-4.380160	1.726656
-1294.819753	-19.514964	1.731661
-1298.893497	-7.606538	1.736666
-1302.039666	-19.294362	1.741670
-1305.846628	-16.686946	1.746675
-1309.964224	-4.984369	1.751680
-1313.593292	-7.713455	1.756685
-1317.396714	-6.281419	1.761690
-1321.189953	-21.327056	1.766694
-1324.966097	-14.468336	1.771699
-1328.560441	-11.756145	1.776704
-1332.245320	-18.272001	1.781709
-1336.113395	-4.745362	1.786714
-1340.000598	-18.235238	1.791718
-1343.674282	-8.237398	1.796723
-1347.526372	-8.634677	1.801728
-1351.032550	-13.985354	1.806733
-1355.148666	-14.521702	1.811738
-1358.569533	-9.610575	1.816742
-1362.585021	-10.837957	1.821747
-1366.164142	-3.936593	1.826752
-1370.148520	-15.307198	1.831757
-1374.165225	-8.028262	1.836762
-1377.821381	-16.988192	1.841766
-1381.325417	-23.092946	1.846771
-1384.919690	-4.641082	1.851776
-1388.218579	-14.864568	1.856781
-1392.610434	-8.391286	1.861786
-1396.001409	-15.502873	1.866790
-1400.296244	-12.804575	1.871795
-1404.168632	-9.134693	1.876800
-1407.536684	-10.230692	1.881805
-1411.522466	-7.733243	1.886810
-1415.027812	-10.439398	1.891814
-1418.973424	-7.424819	1.896819
-1423.045679	-8.830664	1.901824
-1426.442232	-11.136327	1.906829
-1430.429643	-2.827502	1.911834
-1433.749729	-13.302992	1.916838
-1437.553305	-11.058603	1.921843
-1441.799750	-9.987509	1.926848
-1445.181621	-17.912609	1.931853
-1449.237510	-11.111399	1.936858
-1452.542252	-11.140409	1.941862
-1456.276245	-4.878010	1.946867
-1460.256528	-9.606969	1.951872
-1464.094467	-13.871434	1.956877
-1467.854510	-9.102954	1.961882
-1471.750106	-12.274806	1.966886
-1475.510858	-8.526489	1.971891
-1478.993403	-6.492715	1.976896
-1482.559961	-12.423296	1.981901
-1486.599509	-16.366853	1.986906
-1490.187261	-19.133808	1.991910
-1494.044363	-16.158510	1.996915
-1498.289731	-13.481381	2.006912
-1498.922773	-17.226304	2.016909
-1496.218182	-10.929796	2.026906
-1493.869883	-14.297963	2.036902
-1491.446183	-10.934407	2.046899
-1489.436401	-16.675238	2.056896
-1487.802098	-12.850515	2.066893
-1486.021679	-10.530267	2.076890
-1483.955959	-9.291515	2.086886
-1482.065324	-10.211600	2.096883
-1479.983983	-6.892678	2.106880
-1478.198143	-4.068020	2.116877
-1476.291691	-9.280707	2.126874
-1474.260317	-7.063797	2.136870
-1472.368350	-8.561992	2.146867
-1470.644581	-10.472205	2.156864
-1468.549866	-7.584896	2.166861
-1466.859199	-16.675715	2.176858
-1465.423774	-10.365402	2.186854
-1463.072504	-13.704013	2.196851
-1460.825568	-14.041654	2.206848
-1459.349310	-13.299021	2.216845
-1457.681746	-18.962918	2.226842
-1455.470631	-10.083083	2.236838
-1453.365924	-8.515803	2.246835
-1451.548903	-13.270457	2.256832
-1449.830993	-11.982294	2.266829
-1448.087943	-8.432326	2.276826
-1446.152920	-11.041098	2.286822
-1444.498820	-20.476578	2.296819
-1442.140417	-12.041902	2.306816
-1440.237406	-13.660262	2.316813
-1438.659639	-13.625461	2.326810
-1436.662791	-13.161967	2.336806
-1434.616174	-13.524349	2.346803
-1432.996356	-16.000530	2.356800
-1431.172868	-11.782892	2.366797
-1428.907637	-7.209661	2.376794
-1427.189190	-12.379574	2.386790
-1425.377787	-11.719004	2.396787
-1423.412709	-17.792102	2.406784
-1422.137559	-15.957752	2.416781
-1420.011705	-13.817502	2.426778
-1417.638103	-19.161783	2.436774
-1415.748555	-9.601986	2.446771
-1414.015918	-10.337241	2.456768
-1412.113842	-17.230784	2.466765
-1410.414385	-5.504190	2.476762
-1408.539698	-16.037620	2.486758
-1406.628685	-15.571409	2.496755
-1404.797764	-15.927650	2.506752
-1402.416190	-8.477181	2.516749
-1400.819631	-11.754894	2.526746
-1399.249897	-14.691990	2.536742
-1397.396205	-10.277050	2.546739
-1395.356167	-11.931525	2.556736
-1393.474302	-8.558479	2.566733
-1391.428949	-9.613790	2.576730
-1389.543294	-8.227698	2.586726
-1387.899396	-8.422928	2.596723
-1385.860966	-6.188119	2.606720
-1383.998585	-1.193493	2.616717
-1382.159790	-3.205745	2.626714
-1380.572605	-9.008307	2.636710
-1378.203410	-9.003856	2.646707
-1376.282243	-4.891809	2.656704
-1374.780448	-5.896399	2.666701
-1373.105678	-2.455441	2.676698
-1370.576178	-10.404686	2.686694
-1368.767512	-14.150554	2.696691
-1367.300677	-14.619006	2.706688
-1365.272121	-14.037366	2.716685
-1363.285085	-6.733691	2.726682
-1361.514787	-7.204932	2.736678
-1359.563760	-11.275170	2.746675
-1357.762467	-13.393505	2.756672
-1355.999632	-13.445118	2.766669
-1353.811738	-11.922642	2.776666
-1351.972489	-7.846410	2.786662
-1350.495644	-10.959660	2.796659
-1348.377955	-10.521749	2.806656
-1346.420727	-15.121925	2.816653
-1344.467140	-6.824440	2.826650
-1342.798312	-9.669993	2.836646
-1340.830601	-9.236487	2.846643
-1338.671272	-11.726340	2.856640
-1337.099775	-10.056225	2.866637
-1335.325247	-11.492877	2.876634
-1333.463801	-13.739246	2.886630
-1331.131295	-10.618290	2.896627
-1329.519550	-9.867261	2.906624
-1327.604758	-15.769600	2.916621
-1326.090758	-7.488572	2.926618
-1324.126589	-2.518084	2.936614
-1321.888922	-15.651713	2.946611
-1320.320064	-8.445272	2.956608
-1318.243667	-11.946587	2.966605
-1316.247707	-8.485947	2.976602
-1314.584694	-4.406735	2.986598
-1312.828926	-9.964656	2.996595
-1310.884785	-6.138867	3.006592
-1308.755707	-10.948105	3.016589
-1307.038726	-8.987040	3.026586
-1305.075287	-14.696619	3.036582
-1303.372799	-15.164856	3.046579
-1301.418222	-15.922921	3.056576
-1299.796174	-13.086113	3.066573
-1297.435145	-13.103957	3.076570
-1295.740211	-6.863484	3.086566
-1293.983175	-5.387250	3.096563
-1292.058751	-9.170539	3.106560
-1289.969792	-6.541092	3.116557
-1288.312137	-6.054755	3.126554
-1286.547118	-5.508232	3.136550
-1284.429056	-7.691425	3.146547
-1282.381468	-11.919164	3.156544
-1280.874249	-10.895576	3.166541
-1278.968669	-12.743169	3.176538
-1277.295171	-14.023078	3.186534
-1275.113002	-10.336412	3.196531
-1273.059160	-11.579298	3.206528
-1271.193437	-14.033149	3.216525
-1269.453389	-7.101967	3.226522
-1267.677559	-7.858238	3.236518
-1266.141213	-11.550971	3.246515
-1263.620260	-4.555292	3.256512
-1261.891981	-6.552920	3.266509
-1259.965277	-9.387583	3.276506
-1258.091473	-10.334793	3.286502
-1256.364432	-9.120577	3.296499
-1254.421311	-13.453154	3.306496
-1252.830088	-10.726643	3.316493
-1250.968310	-6.753406	3.326490
-1248.881764	-8.010979	3.336486
-1246.792306	-8.735322	3.346483
-1245.052673	-3.117762	3.356480
-1243.099084	-8.364656	3.366477
-1241.341440	-7.932184	3.376474
-1239.566814	-8.718241	3.386470
-1237.780525	-5.110287	3.396467
-1235.333514	-2.714937	3.406464
-1233.863186	-8.590287	3.416461
-1231.971110	-3.598704	3.426458
-1230.082748	-2.727659	3.436454
-1228.497596	-2.580210	3.446451
-1226.597328	-8.655417	3.456448
-1224.379973	-5.560131	3.466445
-1222.471417	-3.293336	3.476442
-1220.413573	-1.970976	3.486438
-1218.690907	-1.922896	3.496435
-1216.928267	-7.327111	3.506432
-1215.267226	-5.634923	3.516429
-1213.319170	-6.706088	3.526426
-1210.996399	-1.409192	3.536422
-1209.335005	-1.360774	3.546419
-1207.662875	-7.751571	3.556416
-1205.520464	-4.446901	3.566413
-1203.824210	-5.695663	3.576410
-1201.945014	-7.442655	3.586406
-1200.039894	-8.031665	3.596403
-1198.316299	-7.750030	3.606400
-1196.465002	-1.379757	3.616397
-1194.420120	0.628400	3.626394
-1192.561336	1.861059	3.636390
-1190.585314	-8.003164	3.646387
-1188.657148	-6.525811	3.656384
-1187.058135	-4.563146	3.666381
-1185.094381	-4.282035	3.676378
-1183.237763	-8.131758	3.686374
-1181.168915	-1.712598	3.696371
-1179.419033	-0.470397	3.706368
-1177.440167	-9.439783	3.716365
-1175.724713	-4.933058	3.726362
-1173.832666	-5.935227	3.736358
-1171.814457	-4.593849	3.746355
-1169.996109	-4.043137	3.756352
-1168.123932	-0.524660	3.766349
-1166.426203	-2.032583	3.776346
-1164.260266	-5.161245	3.786342
-1162.314418	-16.403800	3.796339
-1160.773046	-7.424383	3.806336
-1158.736327	-8.100733	3.816333
-1156.973854	-12.001689	3.826330
-1154.924446	-10.995296	3.836326
-1153.168467	-8.650345	3.846323
-1151.219631	-9.470526	3.856320
-1149.521564	-12.374309	3.866317
-1147.641212	-10.991905	3.876314
-1145.456841	-15.852479	3.886310
-1143.536694	-15.889626	3.896307
-1141.832128	-12.565369	3.906304
-1140.252279	-14.971799	3.916301
-1138.074179	-16.264449	3.926298
-1136.262983	-12.723559	3.936294
-1134.405314	-12.196480	3.946291
-1132.474752	-19.189110	3.956288
-1130.439332	-19.664697	3.966285
-1128.907184	-10.825890	3.976282
-1126.938929	-14.786591	3.986278
-1124.996819	-12.160339	3.996275
-1123.127214	-11.096729	4.006272
-1121.357057	-13.648860	4.016269
-1119.475413	-14.823008	4.026266
-1117.436531	-9.207433	4.036262
-1115.453419	-6.012983	4.046259
-1113.814706	-13.817874	4.056256
-1111.857801	-8.806560	4.066253
-1110.362398	-2.755071	4.076250
-1108.036100	-13.441075	4.086246
-1106.308199	-5.555689	4.096243
-1104.379582	-5.287837	4.106240
-1102.220000	-9.451236	4.116237
-1100.578178	-7.009032	4.126234
-1098.950958	-8.139303	4.136230
-1096.865290	-11.659281	4.146227
-1094.839592	-16.151787	4.156224
-1093.158698	-9.057836	4.166221
-1091.351685	-8.018924	4.176218
-1088.976054	-4.716714	4.186214
-1087.636701	-4.414580	4.196211
-1085.666813	-6.215464	4.206208
-1083.576182	-3.451878	4.216205
-1081.564713	-8.122104	4.226202
-1080.075015	-8.818248	4.236198
-1078.325646	-9.608038	4.246195
-1075.846973	-16.250931	4.256192
-1074.309746	-15.340956	4.266189
-1072.712949	-9.083028	4.276186
-1070.718468	-7.361967	4.286182
-1068.346051	-9.640922	4.296179
-1066.557769	-16.454424	4.306176
-1065.128688	-16.951384	4.316173
-1063.308036	-16.372536	4.326170
-1061.231611	-5.012264	4.336166
-1059.148269	-8.983426	4.346163
-1057.393243	-9.333569	4.356160
-1055.536055	-8.798455	4.366157
-1053.702124	-13.426046	4.376154
-1051.659747	-11.519995	4.386150
-1049.963412	-9.806490	4.396147
-1048.013863	-13.007803	4.406144
-1046.331269	-17.364859	4.416141
-1044.333146	-10.736885	4.426138
-1042.396586	-8.836005	4.436134
-1040.573576	-10.115978	4.446131
-1038.441777	-13.460122	4.456128
-1036.882813	-11.713581	4.466125
-1035.054820	-10.619558	4.476122
-1033.106300	-8.242151	4.486118
-1031.216429	-12.567615	4.496115
-1029.086814	-13.593456	4.506112
-1027.515382	-12.177331	4.516109
-1025.440154	-11.609172	4.526106
-1023.631266	-10.742615	4.536102
-1022.024057	-10.723292	4.546099
-1019.931455	-14.279049	4.556096
-1018.159257	-14.093477	4.566093
-1016.053381	-19.279284	4.576090
-1014.327749	-15.884086	4.586086
-1012.503719	-11.977245	4.596083
-1010.217403	-17.029272	4.606080
-1008.822365	-17.714968	4.616077
-1006.496153	-13.234744	4.626074
-1004.652021	-11.418525	4.636070
-1003.447302	-12.991167	4.646067
-1001.382333	-22.038923	4.656064
-999.115183	-18.594532	4.666061
-997.328372	-16.821247	4.676058
-995.832278	-18.375748	4.686054
-993.831867	-17.702435	4.696051
-991.658495	-19.106301	4.706048
-989.616085	-19.436039	4.716045
-988.265163	-22.832094	4.726042
-986.108883	-12.910343	4.736038
-984.135062	-14.639138	4.746035
-982.386235	-13.857682	4.756032
-980.659331	-16.609639	4.766029
-978.625362	-13.697947	4.776026
-976.676919	-14.814768	4.786022
-974.725205	-19.617456	4.796019
-973.120454	-14.949182	4.806016
-970.984804	-22.438710	4.816013
-969.374965	-16.823859	4.826010
-967.678469	-11.259180	4.836006
-965.431765	-15.182174	4.846003
-963.600137	-24.191004	4.856000
-961.512560	-18.698339	4.865997
-959.780816	-16.098305	4.875994
-957.952571	-14.953734	4.885990
-956.162889	-17.892559	4.895987
-954.241629	-15.330723	4.905984
-952.366611	-17.479491	4.915981
-950.521038	-19.127747	4.925978
-948.448635	-17.306934	4.935974
-946.649979	-16.471840	4.945971
-944.920375	-22.592173	4.955968
-943.605845	-16.751653	4.965965
-940.954702	-20.748774	4.975962
-938.918511	-9.212995	4.985958
-937.234150	-16.546644	4.995955
-935.698831	-15.143629	5.005952
-933.445587	-19.547650	5.015949
-931.645028	-16.372796	5.025946
-930.004104	-10.497615	5.035942
-928.018579	-13.938274	5.045939
-925.922902	-21.072418	5.055936
-924.275120	-10.756650	5.065933
-922.440160	-16.571704	5.075930
-920.374481	-17.375640	5.085926
-918.584743	-14.704319	5.095923
-916.956673	-9.957624	5.105920
-914.961855	-7.546466	5.115917
-913.220191	-11.668137	5.125914
-910.975872	-15.451750	5.135910
-908.922053	-10.277326	5.145907
-907.281320	-14.717597	5.155904
-905.517978	-12.266261	5.165901
-903.753561	-16.315771	5.175898
-901.705910	-5.302849	5.185894
-899.681623	-14.055071	5.195891
-898.082098	-16.005006	5.205888
-895.993353	-10.676677	5.215885
-894.249752	-6.303708	5.225882
-892.312022	-8.895099	5.235878
-890.607452	-12.799239	5.245875
-888.559733	-11.389697	5.255872
-886.386953	-11.667557	5.265869
-884.667549	-10.931851	5.275866
-883.080114	-17.599426	5.285862
-881.079750	-16.663897	5.295859
-879.120519	-13.490685	5.305856
-877.367033	-17.614220	5.315853
-875.420454	-18.504866	5.325850
-873.648879	-15.596916	5.335846
-871.356027	-7.195334	5.345843
-869.776028	-13.395913	5.355840
-868.131384	-15.646733	5.365837
-866.164782	-14.754742	5.375834
-864.030424	-15.160652	5.385830
-862.592644	-16.847855	5.395827
-860.491215	-12.683654	5.405824
-858.560928	-22.871898	5.415821
-856.430370	-11.193227	5.425818
-854.530319	-15.984404	5.435814
-852.978615	-15.826614	5.445811
-851.146535	-15.749965	5.455808
-849.154725	-14.609352	5.465805
-847.342592	-17.371683	5.475802
-845.259853	-11.521281	5.485798
-843.516693	-11.581993	5.495795
-841.592988	-10.188900	5.505792
-839.565129	-10.658290	5.515789
-837.895821	-12.871979	5.525786
-836.327151	-9.884191	5.535782
-834.311723	-4.899352	5.545779
-832.271371	-16.759954	5.555776
-830.444793	-6.677959	5.565773
-828.330634	-14.874479	5.575770
-826.746563	-9.263294	5.585766
-824.804278	-6.180484	5.595763
-822.762956	-10.691058	5.605760
-820.923728	-14.660888	5.615757
-819.158712	-11.736057	5.625754
-817.195427	-9.603989	5.635750
-815.194178	-14.607109	5.645747
-813.897302	-9.485279	5.655744
-811.758130	-13.427261	5.665741
-809.730575	-13.958157	5.675738
-807.875498	-12.194057	5.685734
-806.084495	-12.766085	5.695731
-804.053152	-13.990757	5.705728
-802.213484	-7.176171	5.715725
-800.408544	-10.327328	5.725722
-798.537310	-7.053134	5.735718
-796.654940	-4.647581	5.745715
-795.036930	-8.122546	5.755712
-792.554933	-15.258336	5.765709
-790.773632	-11.863969	5.775706
-788.970982	-8.848810	5.785702
-787.480863	-7.526893	5.795699
-785.507276	-6.768584	5.805696
-783.732613	-10.363322	5.815693
-781.438403	-2.835037	5.825690
-779.704096	-13.975614	5.835686
-777.787207	-10.647121	5.845683
-776.091460	-9.959659	5.855680
-774.087831	-7.788212	5.865677
-772.185015	-6.347511	5.875674
-770.458308	-7.015027	5.885670
-768.446794	-8.059653	5.895667
-766.589245	-3.005304	5.905664
-764.625386	-6.680798	5.915661
-762.830240	-11.399875	5.925658
-761.139477	-9.007879	5.935654
-759.394535	-8.830386	5.945651
-757.219631	-10.278496	5.955648
-755.208379	-14.302616	5.965645
-753.242389	-9.890870	5.975642
-751.747465	-0.488440	5.985638
-749.651180	-10.379455	5.995635
-747.579594	-8.593067	6.005632
-746.063771	-16.014924	6.015629
-744.382342	-16.349913	6.025626
-742.036987	-12.780390	6.035622
-740.199334	-16.322003	6.045619
-738.395871	-18.391272	6.055616
-736.940285	-11.780515	6.065613
-734.736067	-14.078047	6.075610
-732.819873	-14.835823	6.085606
-731.044195	-10.279953	6.095603
-728.914883	-9.507010	6.105600
-726.976783	-17.525306	6.115597
-725.362923	-10.944573	6.125594
-723.549939	-13.612210	6.135590
-721.634096	-14.818353	6.145587
-719.440778	-10.037109	6.155584
-717.592838	-11.481876	6.165581
-716.158723	-6.391393	6.175578
-714.064142	-11.608303	6.185574
-712.139584	-6.146187	6.195571
-710.443773	-10.405656	6.205568
-708.331841	-1.221805	6.215565
-706.413653	-16.700781	6.225562
-705.012244	-13.482482	6.235558
-702.811652	-2.094318	6.245555
-700.944754	-8.556969	6.255552
-699.029026	-11.544174	6.265549
-696.886832	-14.749152	6.275546
-695.447307	-16.281794	6.285542
-693.469869	-14.330309	6.295539
-691.446957	-12.411353	6.305536
-689.709151	-13.527438	6.315533
-687.688893	-13.644949	6.325530
-685.992579	-12.040120	6.335526
-683.995881	-8.327974	6.345523
-682.206232	-14.100880	6.355520
-680.217545	-10.452189	6.365517
-678.491143	-8.812688	6.375514
-676.834834	-7.869372	6.385510
-674.663592	-7.829415	6.395507
-672.732245	-3.168895	6.405504
-671.001866	-17.239379	6.415501
-669.133678	-10.219232	6.425498
-667.343677	-12.529462	6.435494
-665.330824	-11.965226	6.445491
-663.022472	-11.637687	6.455488
-661.399169	-14.475499	6.465485
-659.934017	-11.221566	6.475482
-657.970445	-13.261096	6.485478
-655.788932	-6.180473	6.495475
-654.092463	-15.248030	6.505472
-652.189455	-11.445094	6.515469
-650.200587	-13.524976	6.525466
-648.311275	-9.784587	6.535462
-646.430617	-11.330846	6.545459
-644.744449	-14.442384	6.555456
-642.733733	-12.571964	6.565453
-640.849183	-8.829228	6.575450
-639.261413	-11.508187	6.585446
-637.139917	-16.296689	6.595443
-635.108366	-11.391617	6.605440
-633.399340	-18.177948	6.615437
-631.286822	-16.596949	6.625434
-629.470334	-18.909804	6.635430
-627.968092	-17.209186	6.645427
-626.214641	-14.931320	6.655424
-623.730203	-18.448293	6.665421
-622.374188	-15.194267	6.675418
-620.309052	-15.331523	6.685414
-618.368136	-12.884651	6.695411
-616.252783	-18.921133	6.705408
-614.739908	-15.884802	6.715405
-612.777954	-15.675556	6.725402
-610.871821	-9.548813	6.735398
-608.706595	-3.654519	6.745395
-607.340351	-11.972953	6.755392
-605.294141	-15.048828	6.765389
-603.365786	-20.289613	6.775386
-601.314376	-15.161889	6.785382
-600.010978	-14.231610	6.795379
-597.841650	-11.821214	6.805376
-595.854409	-12.647074	6.815373
-594.088888	-13.246452	6.825370
-591.861849	-9.574183	6.835366
-590.063696	-15.258381	6.845363
-588.288650	-10.492290	6.855360
-586.556195	-16.184936	6.865357
-584.549928	-13.600052	6.875354
-582.755983	-10.295963	6.885350
-580.712146	-11.656656	6.895347
-579.058379	-11.137613	6.905344
-577.297889	-14.842047	6.915341
-575.283956	-11.356776	6.925338
-573.112372	-15.433206	6.935334
-571.471514	-19.811699	6.945331
-569.872358	-17.559669	6.955328
-567.832661	-14.803264	6.965325
-565.579325	-17.086384	6.975322
-563.781629	-16.612430	6.985318
-561.979567	-7.953687	6.995315
-560.354485	-14.052332	7.005312
-558.530005	-7.303008	7.015309
-556.202238	-11.396481	7.025306
-554.480104	-5.732937	7.035302
-552.761375	-8.409077	7.045299
-550.832644	-6.899700	7.055296
-548.838046	-4.260812	7.065293
-547.082155	-6.535505	7.075290
-545.385800	-13.305546	7.085286
-543.356661	-7.509453	7.095283
-541.581352	-9.566185	7.105280
-539.415708	-6.261436	7.115277
-537.743211	-5.033230	7.125274
-535.933837	-11.832373	7.135270
-533.719918	-13.854949	7.145267
-531.906226	-9.887640	7.155264
-530.454737	-13.266359	7.165261
-528.338096	-11.726979	7.175258
-526.345248	-15.763765	7.185254
-524.794727	-15.281877	7.195251
-522.349207	-8.609620	7.205248
-520.711413	-13.540240	7.215245
-519.242860	-16.744830	7.225242
-517.106905	-18.353874	7.235238
-515.217797	-13.855426	7.245235
-513.462500	-14.551008	7.255232
-511.486006	-16.851439	7.265229
-509.237565	-12.715128	7.275226
-507.478407	-12.986574	7.285222
-506.020096	-6.603465	7.295219
-504.125532	-6.438630	7.305216
-501.876451	-3.082433	7.315213
-500.028212	-12.636783	7.325210
-498.357799	-11.185579	7.335206
-496.485501	-9.117654	7.345203
-494.698311	-14.680031	7.355200
-492.447465	-10.060916	7.365197
-490.751991	-11.969066	7.375194
-488.849921	-11.767522	7.385190
-487.123075	-8.211053	7.395187
-485.313026	-19.905139	7.405184
-483.371078	-12.304492	7.415181
-481.227729	-15.618417	7.425178
-479.871026	-11.173855	7.435174
-477.485841	-10.294706	7.445171
-475.722694	-8.581973	7.455168
-473.767604	-9.599972	7.465165
-471.944452	-11.324811	7.475162
-469.985412	-8.394378	7.485158
-468.232645	-10.499564	7.495155
-466.530792	-8.060172	7.505152
-464.650411	-11.398402	7.515149
-462.791142	-11.024207	7.525146
-460.677156	-7.507443	7.535142
-458.818614	-8.408954	7.545139
-456.945319	-15.619314	7.555136
-455.023992	-13.076015	7.565133
-453.153086	-5.503466	7.575130
-451.402949	-14.366306	7.585126
-449.571127	-16.447786	7.595123
-447.444725	-3.102187	7.605120
-445.535912	-12.170371	7.615117
-444.119252	-13.053407	7.625114
-442.172781	-8.920910	7.635110
-439.991856	-5.357973	7.645107
-438.485380	-8.019084	7.655104
-436.451058	-10.038155	7.665101
-434.342299	-13.970219	7.675098
-432.416087	-10.939773	7.685094
-430.657985	-12.984202	7.695091
-428.706425	-8.873033	7.705088
-427.059420	-11.221833	7.715085
-425.131607	-10.457490	7.725082
-423.599540	-6.070897	7.735078
-421.170232	-11.393126	7.745075
-419.423860	-7.752880	7.755072
-417.647072	-7.059152	7.765069
-415.692689	-14.323486	7.775066
-413.806358	-16.959976	7.785062
-411.861845	-11.647633	7.795059
-410.171705	-5.138843	7.805056
-408.333741	-7.038111	7.815053
-406.415402	-3.821642	7.825050
-404.490421	-6.930101	7.835046
-402.326680	-3.482808	7.845043
-401.055115	-4.295280	7.855040
-398.914142	-13.072073	7.865037
-396.865312	-13.980237	7.875034
-395.080348	-15.361017	7.885030
-393.096077	-11.976641	7.895027
-391.189590	-10.174624	7.905024
-389.290730	-12.789412	7.915021
-387.663579	-8.948519	7.925018
-385.865594	-12.624070	7.935014
-383.825891	-14.179732	7.945011
-381.925699	-6.333895	7.955008
-380.154951	-10.507213	7.965005
-378.199921	-9.290849	7.975002
-376.342037	-11.134851	7.984998
-374.452864	-14.764951	7.994995
-372.860009	-9.194311	8.004992
-370.474252	-9.949404	8.014989
-368.494571	-8.907499	8.024986
-367.055828	-8.734512	8.034982
-365.272323	-12.222993	8.044979
-363.103925	-9.932232	8.054976
-361.224440	-15.845579	8.064973
-359.492572	-8.743396	8.074970
-357.595902	-12.278363	8.084966
-355.772500	-13.188395	8.094963
-353.860945	-13.321425	8.104960
-351.823515	-9.454433	8.114957
-349.984813	-6.316784	8.124954
-348.010383	-9.175718	8.134950
-346.293512	-7.428656	8.144947
-344.663176	-10.077907	8.154944
-342.773353	-5.382051	8.164941
-340.737256	-6.630777	8.174938
-338.627999	-5.311106	8.184934
-336.912819	-3.281126	8.194931
-334.878400	-5.548031	8.204928
-333.102135	1.356032	8.214925
-331.368750	1.789904	8.224922
-329.663023	-8.827931	8.234918
-327.487565	-7.722509	8.244915
-325.775798	-5.234068	8.254912
-323.813416	-7.778419	8.264909
-321.862409	-7.834036	8.274906
-319.618906	-9.805878	8.284902
-318.188979	-10.261472	8.294899
-316.492814	-6.134694	8.304896
-314.491556	-4.518277	8.314893
-312.669091	-8.039785	8.324890
-310.385037	-12.054995	8.334886
-308.690858	-8.466333	8.344883
-306.908409	-3.004861	8.354880
-305.031296	-2.887609	8.364877
-303.066137	-5.478178	8.374874
-301.145469	-9.640637	8.384870
-299.479985	-3.072559	8.394867
-297.603713	-3.987830	8.404864
-295.572692	-2.658788	8.414861
-293.961741	-5.810190	8.424858
-292.111917	-12.143504	8.434854
-289.878649	-7.709281	8.444851
-288.246115	-4.009705	8.454848
-286.277745	-7.391850	8.464845
-284.374458	-2.110708	8.474842
-282.365837	-4.752411	8.484838
-280.721862	-5.919542	8.494835
-278.535482	-7.819068	8.504832
-276.877886	1.267208	8.514829
-275.091204	-8.899292	8.524826
-273.488561	-0.320574	8.534822
-271.323946	-4.817226	8.544819
-269.181425	-4.142296	8.554816
-267.580757	-1.092901	8.564813
-265.655970	-5.788114	8.574810
-263.653655	-3.379165	8.584807
-261.664104	-2.544015	8.594803
-259.952222	-2.641939	8.604800
-258.331082	-0.849529	8.614797
-256.405003	-8.533981	8.624794
-254.279360	-13.981267	8.634791
-252.286516	-11.758698	8.644787
-250.856799	-10.799439	8.654784
-248.777425	-7.663809	8.664781
-246.930100	-9.261284	8.674778
-244.986942	-10.510885	8.684775
-243.252509	-4.991170	8.694771
-241.250621	-11.288719	8.704768
-239.245688	-9.822829	8.714765
-237.401471	-12.678260	8.724762
-235.465843	-6.007986	8.734759
-233.725929	-12.303189	8.744755
-232.006689	-6.973678	8.754752
-230.201792	-1.897844	8.764749
-227.844016	-8.173240	8.774746
-226.068088	-9.685090	8.784743
-224.315991	-7.120903	8.794739
-222.629054	-5.695824	8.804736
-220.565820	-8.271981	8.814733
-219.304092	-7.576425	8.824730
-216.771870	-7.756304	8.834727
-214.712099	-7.415496	8.844723
-213.103585	-6.625282	8.854720
-211.194107	-4.203050	8.864717
-209.456987	-8.254037	8.874714
-207.448058	-2.249141	8.884711
-205.407337	-8.597074	8.894707
-203.551858	-3.136122	8.904704
-201.908120	-8.637509	8.914701
-200.044661	0.842300	8.924698
-198.103316	-5.260813	8.934695
-196.059995	-9.163287	8.944691
-194.261548	-10.847661	8.954688
-192.192829	-19.835392	8.964685
-190.412867	-18.106181	8.974682
-188.759331	-12.301928	8.984679
-186.806951	-18.839434	8.994675
-184.996742	-22.117305	9.004672
-183.063102	-14.980869	9.014669
-181.375046	-11.992733	9.024666
-179.189397	-14.018373	9.034663
-177.380928	-16.970689	9.044659
-175.561984	-17.251434	9.054656
-173.714972	-16.838741	9.064653
-171.645538	-19.025832	9.074650
-170.057157	-17.791837	9.084647
-168.275805	-20.188748	9.094643
-166.172759	-15.184134	9.104640
-164.389437	-20.486710	9.114637
-162.779634	-18.264519	9.124634
-160.362472	-16.469600	9.134631
-158.481142	-22.079927	9.144627
-156.912887	-14.793575	9.154624
-155.128457	-16.652531	9.164621
-152.726271	-11.701957	9.174618
-151.007834	-17.144175	9.184615
-149.566951	-17.882480	9.194611
-147.541212	-10.064369	9.204608
-145.459638	-17.691443	9.214605
-143.524843	-12.671011	9.224602
-141.796441	-21.924932	9.234599
-140.003168	-13.428647	9.244595
-137.893495	-19.024871	9.254592
-136.665923	-8.587723	9.264589
-134.354730	-12.130248	9.274586
-132.170029	-11.553507	9.284583
-130.403616	-15.236471	9.294579
-128.701375	-10.515241	9.304576
-127.099056	-13.579893	9.314573
-125.023533	-10.323534	9.324570
-122.630754	-17.453917	9.334567
-121.120993	-11.002967	9.344563
-119.205673	-17.907153	9.354560
-117.528402	-12.166636	9.364557
-115.587118	-6.488770	9.374554
-113.774475	-13.229724	9.384551
-111.686915	-10.617926	9.394547
-109.940162	-13.727720	9.404544
-108.459960	-4.243523	9.414541
-106.071933	-4.959243	9.424538
-103.983885	-15.247932	9.434535
-102.324438	-13.073095	9.444531
-100.603822	-13.431255	9.454528
-98.628513	-7.086151	9.464525
-96.790532	-12.365825	9.474522
-95.032624	-11.097248	9.484519
-92.890961	-9.769896	9.494515
-91.048631	-7.941609	9.504512
-89.199570	-7.630233	9.514509
-87.291610	-8.864619	9.524506
-85.570683	-9.401245	9.534503
-83.496072	-13.663895	9.544499
-82.042641	-12.559892	9.554496
-80.181923	-13.671467	9.564493
-77.962989	-9.297911	9.574490
-76.132853	-3.498062	9.584487
-74.117017	-4.917024	9.594483
-72.456656	-14.679542	9.604480
-70.559484	-7.851405	9.614477
-68.564152	-10.181331	9.624474
-66.748673	-10.379334	9.634471
-65.110895	-8.013111	9.644467
-62.875186	-7.686032	9.654464
-61.087473	-1.508337	9.664461
-59.128926	-4.692943	9.674458
-57.365743	-5.727359	9.684455
-55.584873	-10.063127	9.694451
-53.838489	-4.098314	9.704448
-51.818765	-4.726799	9.714445
-49.913022	-10.442003	9.724442
-48.090148	-6.643145	9.734439
-46.039725	-4.254317	9.744435
-44.075544	-11.938379	9.754432
-42.394752	-8.870032	9.764429
-40.628911	-7.424252	9.774426
-38.662347	-12.424390	9.784423
-36.628567	-11.772958	9.794419
-34.578651	-8.351374	9.804416
-32.924868	-7.408781	9.814413
-30.970974	-4.156618	9.824410
-29.389309	-3.802537	9.834407
-27.398050	-12.621471	9.844403
-25.590374	-10.034421	9.854400
-23.780098	-8.881517	9.864397
-21.741556	-8.927171	9.874394
-19.977312	-9.590665	9.884391
-17.961013	-10.434898	9.894387
-16.067888	-4.951375	9.904384
-14.343199	-7.334403	9.914381
-12.174044	-3.710760	9.924378
-10.332192	-5.654565	9.934375
-8.390837	-3.906749	9.944371
-6.878962	-4.882092	9.954368
-4.998766	1.896707	9.964365
-3.527836	14.835748	9.974362
-2.371947	46.811017	9.984359
-1.033025	100.441719	9.994355
0.000000	152.836888	9.999360
1.010768	172.628676	10.004365
1.269733	206.269024	10.009370
1.766902	235.572529	10.014375
2.250024	261.487761	10.019379
2.425626	285.717380	10.024384
3.059694	300.085372	10.029389
3.062709	300.793006	10.034394
3.095442	298.423876	10.039399
3.381071	321.282924	10.044403
3.411000	334.268081	10.049408
3.902325	331.723284	10.054413
3.468233	345.705026	10.059418
3.870587	336.071527	10.064423
4.017517	345.754677	10.069427
4.113234	345.430349	10.074432
4.042009	347.575454	10.079437
4.056071	353.755166	10.084442
4.146925	344.758002	10.089447
4.060550	336.542931	10.094451
4.005395	331.614121	10.099456
3.910569	327.566885	10.104461
3.938020	346.772206	10.109466
4.343715	345.650923	10.114471
4.419047	352.770227	10.119475
4.141055	362.201036	10.124480
4.356482	368.044267	10.129485
4.276038	373.053142	10.134490
4.510443	371.118627	10.139495
4.443499	377.880576	10.144499
4.373653	377.935910	10.149504
4.558755	379.138074	10.154509
4.303886	381.913325	10.159514
4.249736	382.863481	10.164519
4.740421	376.357297	10.169523
4.454328	382.020327	10.174528
4.745125	378.547103	10.179533
4.270451	383.683527	10.184538
4.600165	382.937077	10.189543
4.701507	393.832377	10.194547
4.813591	389.685883	10.199552
4.887220	388.280084	10.204557
4.680733	400.416724	10.209562
4.863989	414.287437	10.214567
5.222167	417.303963	10.219571
4.995616	422.821886	10.224576
4.979352	419.426021	10.229581
5.004615	424.673530	10.234586
5.238833	425.492530	10.239591
5.136522	429.082433	10.244595
4.961418	429.451039	10.249600
5.373838	432.950949	10.254605
5.129368	438.474890	10.259610
5.194504	442.534850	10.264615
5.435652	447.659615	10.269619
5.720862	463.759804	10.274624
5.995251	459.238875	10.279629
5.785482	450.433112	10.284634
5.752546	438.982853	10.289639
5.408805	440.682564	10.294643
5.718535	451.710254	10.299648
6.189088	457.206881	10.304653
5.990704	455.828696	10.309658
5.819614	442.709894	10.314663
5.881094	449.842494	10.319667
5.939807	464.868585	10.324672
6.173774	473.473439	10.329677
6.139506	470.209752	10.334682
6.364572	460.219656	10.339687
6.106124	457.307138	10.344691
5.813744	468.788875	10.349696
6.486922	469.580436	10.354701
6.430409	482.746679	10.359706
6.394788	484.001408	10.364711
6.766882	496.785464	10.369715
6.365340	481.178555	10.374720
6.529521	468.430470	10.379725
5.886450	481.928411	10.384730
6.349973	485.738743	10.389735
6.539334	489.130738	10.394739
6.211535	492.583152	10.399744
6.512396	486.204976	10.404749
6.315103	494.277786	10.409754
6.451368	494.213505	10.414759
6.587463	495.641127	10.419763
6.294845	514.886688	10.424768
6.852573	516.628698	10.429773
6.579341	526.241789	10.434778
7.052044	532.187558	10.439783
7.250962	528.503439	10.444787
6.853336	537.808357	10.449792
7.205955	524.575977	10.454797
7.186599	538.203147	10.459802
7.341424	530.995068	10.464807
7.236200	535.295129	10.469811
7.193874	543.007337	10.474816
7.230681	533.233313	10.479821
6.922422	542.859888	10.484826
7.275851	545.675337	10.489831
7.547040	558.347803	10.494835
6.945891	567.546425	10.499840
7.473717	575.114082	10.504845
7.586785	584.287099	10.509850
7.618445	578.609453	10.514855
7.932721	586.458776	10.519859
7.864289	575.731628	10.524864
7.918226	580.722292	10.529869
7.965434	587.270575	10.534874
7.883290	577.575424	10.539879
7.756961	578.070302	10.544883
7.766444	592.421516	10.549888
8.015365	583.309100	10.554893
7.871352	583.450387	10.559898
8.131593	584.333059	10.564903
7.818020	594.603950	10.569907
7.538220	590.723350	10.574912
7.838993	596.822735	10.579917
7.877632	618.821158	10.584922
8.072387	617.744543	10.589927
8.367356	620.301235	10.594931
8.453278	620.016312	10.599936
8.629117	620.455105	10.604941
8.440962	623.315959	10.609946
8.604490	625.133480	10.614951
8.629792	629.089453	10.619955
8.602613	628.656981	10.624960
8.883880	619.894219	10.629965
8.640574	631.048114	10.634970
8.659924	625.514348	10.639975
8.580642	629.991660	10.644979
8.552335	633.735398	10.649984
8.641815	629.292802	10.654989
8.680894	638.286833	10.659994
9.184582	654.057474	10.664999
9.061500	666.904898	10.670003
9.209571	667.466401	10.675008
9.315802	645.047450	10.680013
9.094811	647.066669	10.685018
9.221149	654.644792	10.690023
8.860965	647.928841	10.695027
9.298256	660.652176	10.700032
9.364990	673.399937	10.705037
9.498623	678.562437	10.710042
9.698043	667.953354	10.715047
9.649402	672.892599	10.720051
9.352153	679.402824	10.725056
9.533846	673.442571	10.730061
9.217252	677.181841	10.735066
9.586633	675.580595	10.740071
9.537342	680.270771	10.745075
9.243590	681.481532	10.750080
9.412942	675.710917	10.755085
9.357793	685.576349	10.760090
9.498932	679.365503	10.765095
9.913698	699.075670	10.770099
9.731385	706.654165	10.775104
10.251094	704.327145	10.780109
10.064671	705.792041	10.785114
10.036373	705.821824	10.790119
10.212384	717.109183	10.795123
10.145033	715.847276	10.800128
10.206037	706.428845	10.805133
9.942967	719.144094	10.810138
10.161636	712.687461	10.815143
10.355305	713.262195	10.820147
10.130354	722.512875	10.825152
10.223422	718.804590	10.830157
9.800149	726.235439	10.835162
10.151192	717.871524	10.840167
10.438215	733.708354	10.845171
10.214181	752.675187	10.850176
10.427141	752.401539	10.855181
10.261246	756.078940	10.860186
10.450043	749.228060	10.865191
10.281064	748.942792	10.870195
10.352696	765.375449	10.875200
10.769350	772.356928	10.880205
11.009084	782.109150	10.885210
11.100055	781.580551	10.890215
10.813251	792.001863	10.895219
10.887597	785.812665	10.900224
11.166878	778.832211	10.905229
11.041703	786.210809	10.910234
11.345806	787.277322	10.915239
11.481010	783.893483	10.920243
11.079151	790.953493	10.925248
11.318766	787.313284	10.930253
11.399573	800.949955	10.935258
11.278467	802.163150	10.940263
11.145227	792.146399	10.945267
11.204823	793.499515	10.950272
11.440758	792.966716	10.955277
11.260243	797.818221	10.960282
11.217185	794.297224	10.965287
11.492610	807.967516	10.970291
11.728611	828.313546	10.975296
11.897828	820.284529	10.980301
11.964290	827.276160	10.985306
12.167709	824.187383	10.990311
11.885808	823.475392	10.995315
11.910140	811.626168	11.000320
11.946768	795.955332	11.005325
12.036664	814.331234	11.010330
11.753759	818.842662	11.015335
11.950611	820.766865	11.020339
11.883332	837.903057	11.025344
12.254928	821.852307	11.030349
12.007959	841.013739	11.035354
12.172618	827.552428	11.040359
12.363221	832.776864	11.045363
12.114191	839.020828	11.050368
12.258409	845.424433	11.055373
12.078940	840.051620	11.060378
12.359519	838.511834	11.065383
12.321518	842.135738	11.070387
12.556274	853.264010	11.075392
12.713011	864.146096	11.080397
12.341235	872.510319	11.085402
12.451579	878.413100	11.090407
12.735803	875.054359	11.095411
12.626129	879.919825	11.100416
12.655859	863.595530	11.105421
12.859725	868.469329	11.110426
12.543455	866.769260	11.115431
12.818812	869.441098	11.120435
12.559574	881.277444	11.125440
12.692827	883.319042	11.130445
12.915782	892.586698	11.135450
12.712623	897.192670	11.140455
12.972594	905.902453	11.145459
13.102260	914.614101	11.150464
13.371031	901.353752	11.155469
13.113473	908.176317	11.160474
13.144229	902.635895	11.165479
13.563399	904.586152	11.170483
13.487466	917.558751	11.175488
13.745292	915.946887	11.180493
13.418766	918.676892	11.185498
13.627475	912.513521	11.190503
13.648042	916.241650	11.195507
13.489791	913.267321	11.200512
14.041873	911.269446	11.205517
13.609121	910.832269	11.210522
13.632563	918.843293	11.215527
13.843464	911.824794	11.220531
13.609094	915.595166	11.225536
13.862400	922.066566	11.230541
13.597316	941.524356	11.235546
13.721527	951.097985	11.240551
13.771793	950.547485	11.245555
13.866812	958.695359	11.250560
14.119954	948.140586	11.255565
14.051771	951.838723	11.260570
14.121930	951.996316	11.265575
14.302261	949.343316	11.270579
14.161184	947.495433	11.275584
14.060720	943.340106	11.280589
14.133194	963.436420	11.285594
14.850958	973.243417	11.290599
14.673767	984.156780	11.295603
14.395303	975.760658	11.300608
14.947282	971.457090	11.305613
14.847894	965.672453	11.310618
14.669163	962.878014	11.315623
14.457503	951.979453	11.320627
14.785053	969.358774	11.325632
14.992942	980.480391	11.330637
14.872536	985.563665	11.335642
14.735438	982.620642	11.340647
15.162671	990.871673	11.345651
14.802755	993.595979	11.350656
15.352643	982.591689	11.355661
15.031940	993.767668	11.360666
14.777013	987.962098	11.365671
15.097093	985.810394	11.370675
15.174635	985.889532	11.375680
15.131455	996.125458	11.380685
15.143954	997.270044	11.385690
15.163608	987.575729	11.390695
15.052274	991.252372	11.395699
14.966028	992.701316	11.400704
15.265400	986.141796	11.405709
15.498693	998.262403	11.410714
15.729470	1003.087796	11.415719
15.453473	1008.225862	11.420723
15.720281	1011.520464	11.425728
15.625847	1011.802092	11.430733
15.630986	1027.801701	11.435738
15.951376	1016.546174	11.440743
15.859452	1022.896054	11.445747
15.780807	1030.103334	11.450752
16.084392	1014.696425	11.455757
15.915536	1029.020531	11.460762
15.775064	1021.315217	11.465767
16.186495	1016.495479	11.470771
15.820285	1025.048940	11.475776
16.174560	1017.983075	11.480781
16.042498	1023.449089	11.485786
16.355293	1015.065084	11.490791
16.215895	1023.007514	11.495795
15.814838	1032.534085	11.500800
16.268398	1023.111973	11.505805
16.215914	1033.870639	11.510810
16.232667	1028.570544	11.515815
16.202891	1033.304246	11.520819
16.187131	1043.949819	11.525824
16.589244	1052.015640	11.530829
16.370605	1070.195842	11.535834
16.350000	1062.269518	11.540839
16.313173	1060.410511	11.545843
16.438836	1061.617483	11.550848
16.612110	1061.025279	11.555853
16.577098	1068.756311	11.560858
16.414417	1070.021107	11.565863
16.719111	1083.783983	11.570867
17.189059	1095.194288	11.575872
17.264092	1085.502902	11.580877
17.389637	1093.060878	11.585882
17.240145	1074.340143	11.590887
17.418497	1059.885228	11.595891
17.010890	1062.054130	11.600896
17.353518	1062.767558	11.605901
16.967998	1063.553766	11.610906
17.695335	1073.688130	11.615911
17.345964	1061.657806	11.620915
17.364637	1063.321855	11.625920
17.365951	1060.436382	11.630925
17.359819	1084.874534	11.635930
17.665262	1080.231757	11.640935
17.578191	1081.695036	11.645939
17.731455	1086.741788	11.650944
18.182640	1084.630664	11.655949
17.777830	1071.451584	11.660954
17.425666	1057.484244	11.665959
17.709533	1068.255521	11.670963
17.749910	1080.222448	11.675968
17.737163	1075.197515	11.680973
17.739912	1096.051890	11.685978
17.876650	1096.522959	11.690983
17.966712	1088.739831	11.695987
17.933006	1101.895110	11.700992
18.076775	1096.650431	11.705997
17.908248	1100.599599	11.711002
18.099265	1101.508329	11.716007
18.024995	1095.914406	11.721011
17.784887	1091.092118	11.726016
18.308299	1099.243495	11.731021
18.157116	1115.167989	11.736026
18.412250	1120.116494	11.741031
18.475471	1122.152737	11.746035
18.422874	1128.146273	11.751040
18.623400	1131.923818	11.756045
18.641872	1128.955162	11.761050
18.387204	1126.447220	11.766055
18.678223	1126.385852	11.771059
18.490589	1129.667807	11.776064
18.886360	1126.376380	11.781069
18.520866	1130.131449	11.786074
18.558811	1132.211153	11.791079
18.688283	1128.884925	11.796083
18.635063	1127.183081	11.801088
18.663098	1123.299757	11.806093
18.697710	1136.598726	11.811098
18.726452	1153.856393	11.816103
19.148563	1162.483691	11.821107
19.120064	1159.111685	11.826112
19.553186	1146.122183	11.831117
19.331250	1159.419513	11.836122
19.191800	1152.629478	11.841127
19.530390	1153.298608	11.846131
19.367100	1157.949558	11.851136
19.221424	1161.825705	11.856141
19.449348	1163.581767	11.861146
19.421185	1157.232917	11.866151
19.200723	1154.723456	11.871155
19.064288	1161.873781	11.876160
19.348500	1156.086233	11.881165
19.148014	1171.436700	11.886170
19.653293	1184.857774	11.891175
19.909953	1191.202592	11.896179
19.529601	1198.955660	11.901184
19.869672	1202.319052	11.906189
19.869393	1201.847576	11.911194
20.109496	1190.087430	11.916199
19.993532	1194.603885	11.921203
19.892686	1194.724096	11.926208
20.231529	1190.077534	11.931213
19.846190	1194.278953	11.936218
20.002609	1188.380088	11.941223
20.071506	1186.753384	11.946227
20.245800	1194.494467	11.951232
20.369339	1184.117121	11.956237
20.101733	1202.440929	11.961242
20.056988	1182.961315	11.966247
20.263918	1191.847693	11.971251
20.323731	1202.751802	11.976256
20.593996	1206.993742	11.981261
20.740704	1219.511583	11.986266
20.639624	1221.218409	11.991271
20.851020	1219.638364	11.996275
20.631455	1214.532032	12.001280
20.520905	1203.439728	12.006285
20.484889	1221.329187	12.011290
20.709182	1221.184624	12.016295
21.004409	1220.925446	12.021299
20.735670	1216.284320	12.026304
20.702923	1197.135544	12.031309
20.493895	1193.341272	12.036314
20.873960	1195.343545	12.041319
20.779822	1192.703530	12.046323
20.490424	1187.278729	12.051328
20.797500	1178.938126	12.056333
20.345130	1197.084798	12.061338
20.782224	1206.465958	12.066343
20.934220	1208.503035	12.071347
20.781615	1204.365413	12.076352
20.725162	1197.689863	12.081357
20.495738	1193.947735	12.086362
20.576188	1197.029231	12.091367
20.648685	1207.223986	12.096371
20.702081	1205.638391	12.101376
21.026851	1190.233438	12.106381
20.612673	1203.575667	12.111386
20.718631	1196.390038	12.116391
20.797862	1197.617046	12.121395
20.712300	1198.025008	12.126400
20.824306	1195.250386	12.131405
20.837838	1193.597816	12.136410
20.802506	1184.536677	12.141415
20.564613	1198.562059	12.146419
20.408139	1200.286392	12.151424
20.778831	1194.278432	12.156429
20.663687	1206.189838	12.161434
20.953321	1203.297774	12.166439
20.734178	1195.082892	12.171443
20.539287	1195.782711	12.176448
21.029756	1187.227538	12.181453
20.565115	1194.350588	12.186458
20.644519	1195.314190	12.191463
20.827716	1200.673206	12.196467
20.492018	1197.529195	12.201472
20.895100	1199.210798	12.206477
20.559775	1206.608934	12.211482
20.876793	1191.841581	12.216487
21.166878	1191.970404	12.221491
20.844767	1199.089646	12.226496
21.274372	1197.606486	12.231501
20.892301	1198.087767	12.236506
21.093673	1178.375703	12.241511
20.874556	1172.591157	12.246515
20.729749	1173.913829	12.251520
20.963050	1172.461984	12.256525
20.631832	1171.168790	12.261530
20.751682	1161.446548	12.266535
20.702696	1159.498784	12.271539
20.352174	1171.413010	12.276544
20.591421	1162.185072	12.281549
20.574380	1167.366261	12.286554
20.371890	1158.602276	12.291559
20.571327	1167.735863	12.296563
20.323748	1169.289415	12.301568
20.562723	1187.622295	12.306573
20.713793	1197.233595	12.311578
20.959402	1201.813814	12.316583
21.017192	1202.207584	12.321587
20.792356	1180.406802	12.326592
20.958307	1167.471727	12.331597
20.609238	1171.013643	12.336602
20.939458	1170.796197	12.341607
20.692849	1175.815292	12.346611
20.845013	1171.428771	12.351616
20.978096	1174.975000	12.356621
20.657747	1174.489129	12.361626
20.832721	1171.327539	12.366631
20.765403	1171.242109	12.371635
21.031471	1179.376228	12.376640
21.126648	1166.314446	12.381645
20.764392	1173.792563	12.386650
20.664777	1169.579471	12.391655
20.820038	1176.542123	12.396659
20.623096	1174.178732	12.401664
20.787271	1173.805616	12.406669
20.727014	1180.297185	12.411674
20.403990	1175.227871	12.416679
20.831471	1173.259302	12.421683
20.628118	1185.545919	12.426688
20.697897	1176.412819	12.431693
20.648688	1178.504855	12.436698
20.935054	1169.459438	12.441703
20.826874	1159.711275	12.446707
20.622077	1155.675829	12.451712
20.915697	1144.276226	12.456717
20.585785	1145.941478	12.461722
20.634001	1150.969524	12.466727
20.712781	1145.474183	12.471731
20.284399	1148.255962	12.476736
20.534986	1155.164759	12.481741
20.591589	1174.633054	12.486746
20.709483	1182.681990	12.491751
20.814193	1181.090579	12.496755
20.552155	1187.274469	12.501760
21.118345	1173.818972	12.506765
20.553560	1169.783380	12.511770
20.516874	1165.241675	12.516775
20.720836	1166.285553	12.521779
20.880618	1182.440455	12.526784
20.681586	1170.904140	12.531789
20.390658	1172.735081	12.536794
20.958469	1171.630463	12.541799
20.903845	1162.182869	12.546803
20.750344	1166.807027	12.551808
20.747103	1154.780554	12.556813
20.284171	1159.316070	12.561818
20.537787	1159.166831	12.566823
20.751854	1167.112888	12.571827
20.896813	1167.473039	12.576832
21.030511	1156.512927	12.581837
20.650071	1159.458965	12.586842
20.818406	1157.719411	12.591847
20.893412	1160.410645	12.596851
20.578969	1159.616297	12.601856
21.178795	1161.833482	12.606861
20.652923	1159.304921	12.611866
20.803923	1166.554494	12.616871
21.039959	1159.724274	12.621875
21.128403	1166.737008	12.626880
21.088345	1158.665485	12.631885
20.650991	1166.400818	12.636890
20.753688	1146.880384	12.641895
21.014711	1137.978603	12.646899
20.907209	1133.373291	12.651904
20.723982	1116.400584	12.656909
20.601610	1120.752442	12.661914
20.712272	1120.014878	12.666919
20.956408	1115.719370	12.671923
20.701264	1127.500064	12.676928
20.869018	1125.407335	12.681933
20.786487	1132.328252	12.686938
20.721361	1127.686218	12.691943
20.623233	1126.155556	12.696947
20.461524	1132.111299	12.701952
20.526329	1124.344009	12.706957
20.763742	1126.533835	12.711962
20.648286	1122.875269	12.716967
20.461382	1122.579446	12.721971
20.334326	1132.794151	12.726976
20.888500	1119.033086	12.731981
20.768764	1131.729772	12.736986
20.714277	1120.840709	12.741991
20.843420	1124.186473	12.746995
20.798335	1127.433861	12.752000
20.586659	1119.013596	12.757005
20.708662	1127.006647	12.762010
20.677663	1131.123139	12.767015
20.595340	1130.326463	12.772019
20.811541	1121.464960	12.777024
20.757259	1128.774858	12.782029
20.554655	1138.692505	12.787034
20.869954	1131.467208	12.792039
21.003096	1132.456141	12.797043
20.226454	1137.212018	12.802048
20.618545	1129.631452	12.807053
20.563888	1133.806917	12.812058
20.716058	1136.816241	12.817063
20.609244	1133.637312	12.822067
20.634733	1132.377117	12.827072
20.904176	1126.759109	12.832077
20.577759	1135.468729	12.837082
20.162253	1134.782763	12.842087
20.589465	1133.220347	12.847091
20.564113	1144.824038	12.852096
20.633547	1148.553895	12.857101
20.716457	1167.652884	12.862106
20.753051	1163.141284	12.867111
20.699065	1158.898048	12.872115
20.465041	1154.720594	12.877120
20.930674	1162.817351	12.882125
20.740415	1155.264212	12.887130
20.516506	1140.698324	12.892135
20.619855	1148.572925	12.897139
20.752229	1160.597002	12.902144
20.686401	1153.315781	12.907149
20.825215	1155.582846	12.912154
20.539788	1140.440875	12.917159
20.811120	1150.470608	12.922163
20.434759	1153.408109	12.927168
21.088125	1151.010812	12.932173
20.689960	1148.729990	12.937178
20.384577	1149.016093	12.942183
20.875640	1142.027707	12.947187
21.069848	1149.212814	12.952192
20.879019	1151.161840	12.957197
20.856968	1152.827664	12.962202
20.926188	1143.308283	12.967207
20.798769	1144.199994	12.972211
20.947126	1145.581567	12.977216
21.115834	1142.044054	12.982221
20.897789	1149.441591	12.987226
20.722565	1143.788840	12.992231
20.773007	1140.508335	12.997235
20.611987	1145.419141	13.002240
21.074767	1139.329488	13.007245
20.464867	1133.312373	13.012250
20.765095	1137.814467	13.017255
20.734421	1143.907812	13.022259
20.498276	1140.476671	13.027264
20.657557	1125.306362	13.032269
20.637521	1137.493516	13.037274
20.611461	1142.765242	13.042279
20.639874	1145.713877	13.047283
20.621527	1141.767765	13.052288
20.768721	1144.911151	13.057293
20.863085	1154.059913	13.062298
20.839355	1145.929806	13.067303
20.830027	1139.424979	13.072307
20.380118	1130.396884	13.077312
20.659648	1136.643403	13.082317
20.696025	1142.333353	13.087322
20.624078	1145.558219	13.092327
20.821037	1149.809470	13.097331
20.441309	1152.912316	13.102336
20.974080	1144.431642	13.107341
20.595043	1160.059762	13.112346
20.732479	1144.670544	13.117351
20.819095	1140.878018	13.122355
20.502946	1147.602796	13.127360
20.762137	1140.241350	13.132365
20.596942	1144.074870	13.137370
20.690359	1142.317303	13.142375
20.730916	1139.205548	13.147379
20.812555	1139.251703	13.152384
21.079204	1137.867088	13.157389
20.417772	1139.590740	13.162394
20.518208	1130.900677	13.167399
20.592617	1127.092753	13.172403
20.318297	1142.014167	13.177408
20.715458	1150.197540	13.182413
20.508034	1158.781738	13.187418
20.636285	1165.946620	13.192423
20.899081	1159.292711	13.197427
20.856161	1159.260166	13.202432
20.872722	1160.422254	13.207437
20.623430	1147.294787	13.212442
20.699109	1136.626247	13.217447
20.457664	1142.460659	13.222451
20.349446	1150.046490	13.227456
20.703501	1159.374627	13.232461
20.614401	1168.844427	13.237466
20.751083	1160.766791	13.242471
20.747366	1163.036879	13.247475
20.712700	1166.540470	13.252480
21.105540	1152.889483	13.257485
20.466325	1166.609018	13.262490
20.486803	1165.537296	13.267495
21.027926	1154.274054	13.272499
20.574304	1166.913631	13.277504
20.675199	1161.231023	13.282509
20.793208	1165.403400	13.287514
20.760853	1153.065364	13.292519
20.475716	1149.824191	13.297523
20.782149	1157.265029	13.302528
21.063778	1160.330987	13.307533
20.509410	1149.152596	13.312538
20.580410	1133.233041	13.317543
20.613776	1141.017078	13.322547
20.676969	1152.970174	13.327552
20.827761	1156.832149	13.332557
20.755882	1143.912163	13.337562
20.719768	1134.800712	13.342567
20.397655	1134.520937	13.347571
20.477966	1153.856100	13.352576
21.010142	1149.978305	13.357581
20.648568	1147.786274	13.362586
20.607314	1140.292962	13.367591
20.841532	1141.153799	13.372595
20.565383	1136.634529	13.377600
20.802802	1135.113426	13.382605
20.617664	1135.844017	13.387610
20.654476	1137.172412	13.392615
20.652796	1133.887605	13.397619
20.553227	1139.476225	13.402624
20.487383	1154.433001	13.407629
20.654623	1158.053421	13.412634
21.074653	1162.438633	13.417639
20.651055	1156.735600	13.422643
20.255576	1150.385413	13.427648
20.662073	1157.997966	13.432653
20.738645	1155.848018	13.437658
20.759190	1163.313959	13.442663
21.069146	1172.821832	13.447667
20.687043	1162.246797	13.452672
20.762463	1144.565683	13.457677
20.476262	1147.873616	13.462682
20.341144	1150.558937	13.467687
20.892664	1154.393265	13.472691
20.839844	1170.593894	13.477696
20.752116	1155.773644	13.482701
20.825610	1152.118051	13.487706
20.572264	1146.366574	13.492711
20.782387	1147.948838	13.497715
20.325810	1151.492127	13.502720
20.800887	1145.277495	13.507725
20.514856	1159.432744	13.512730
20.797152	1166.424807	13.517735
21.013072	1156.755848	13.522739
20.554708	1153.133836	13.527744
20.758932	1146.376512	13.532749
20.593147	1151.103559	13.537754
20.521063	1143.430642	13.542759
20.793728	1144.036164	13.547763
20.444866	1153.435415	13.552768
20.829456	1163.390315	13.557773
21.089817	1167.830962	13.562778
20.887631	1151.201105	13.567783
20.900364	1142.120497	13.572787
20.956754	1155.741682	13.577792
20.730709	1145.646441	13.582797
20.671633	1150.347003	13.587802
20.778803	1151.198141	13.592807
20.633653	1156.744359	13.597811
20.539382	1154.305454	13.602816
20.803163	1147.393536	13.607821
20.868490	1159.814698	13.612826
20.627613	1151.213763	13.617831
20.905959	1151.850709	13.622835
21.023800	1146.405124	13.627840
20.908389	1145.146113	13.632845
20.897974	1153.862902	13.637850
20.931416	1143.020515	13.642855
20.417823	1145.336446	13.647859
20.117053	1148.507917	13.652864
20.727361	1150.880351	13.657869
20.687919	1145.578926	13.662874
20.645403	1154.806298	13.667879
20.814313	1146.024871	13.672883
20.567845	1155.767371	13.677888
21.134706	1149.932374	13.682893
20.577852	1157.327183	13.687898
20.788814	1148.998773	13.692903
20.743286	1150.449913	13.697907
20.482952	1155.287457	13.702912
20.702358	1145.270986	13.707917
20.807074	1151.074630	13.712922
20.693562	1150.640143	13.717927
20.913384	1146.163983	13.722931
20.657787	1146.291530	13.727936
20.637802	1143.593171	13.732941
20.395366	1154.630619	13.737946
20.433806	1154.727036	13.742951
20.805374	1156.029634	13.747955
20.839866	1154.704129	13.752960
20.644995	1152.905016	13.757965
20.395116	1156.708677	13.762970
20.851892	1157.246192	13.767975
20.772478	1150.806950	13.772979
20.464622	1154.840654	13.777984
20.653042	1147.348553	13.782989
20.337770	1155.213443	13.787994
20.610132	1161.215087	13.792999
21.068752	1149.085771	13.798003
20.597086	1152.044783	13.803008
20.625367	1140.384703	13.808013
20.337977	1151.663521	13.813018
20.398951	1157.105102	13.818023
20.592438	1150.574227	13.823027
20.510428	1165.345129	13.828032
20.450945	1153.387559	13.833037
20.403934	1168.191520	13.838042
20.948433	1165.386555	13.843047
21.006914	1154.861896	13.848051
20.875960	1172.216817	13.853056
20.846943	1160.990891	13.858061
20.723721	1162.928346	13.863066
20.759542	1162.056835	13.868071
21.020088	1157.578907	13.873075
20.684636	1167.636836	13.878080
20.847547	1156.840026	13.883085
20.489200	1160.864437	13.888090
20.736308	1159.471109	13.893095
20.721225	1155.515799	13.898099
20.555553	1160.071715	13.903104
20.613940	1158.326042	13.908109
20.647305	1159.942811	13.913114
20.540329	1161.945489	13.918119
20.421360	1161.142040	13.923123
20.512814	1162.357632	13.928128
20.697030	1161.236136	13.933133
20.457874	1169.771780	13.938138
20.573353	1161.735376	13.943143
20.569286	1162.067254	13.948147
20.589145	1155.763576	13.953152
20.641268	1162.276638	13.958157
20.735543	1160.453482	13.963162
20.658370	1160.490273	13.968167
20.543393	1159.807624	13.973171
20.905439	1164.431555	13.978176
20.966774	1163.156966	13.983181
20.580833	1159.630643	13.988186
20.314397	1160.139214	13.993191
20.803745	1164.387201	13.998195
20.785881	1165.103100	14.003213
20.912461	1163.209401	14.008231
20.712570	1167.314039	14.013248
20.703291	1164.482428	14.018266
20.689821	1156.922008	14.023283
20.699629	1162.095928	14.028301
20.902270	1160.660448	14.033319
20.725711	1162.647138	14.038336
20.841197	1162.793140	14.043354
20.751670	1163.384779	14.048371
20.323984	1167.992959	14.053389
20.848093	1166.905765	14.058407
20.910515	1168.675790	14.063424
20.823564	1159.210285	14.068442
20.984932	1172.306472	14.073459
20.723396	1187.344461	14.078477
21.187314	1186.374623	14.083495
21.167274	1186.306280	14.088512
21.056198	1182.623347	14.093530
20.995352	1170.531335	14.098547
20.904652	1172.900748	14.103565
21.088081	1174.725406	14.108583
20.908808	1186.978496	14.113600
21.034555	1186.348116	14.118618
21.174817	1200.650320	14.123635
20.915277	1201.585269	14.128653
21.245346	1185.554012	14.133671
21.172524	1196.530087	14.138688
21.109602	1198.662256	14.143706
21.150241	1196.510117	14.148723
20.956947	1205.389611	14.153741
20.996867	1196.942083	14.158759
20.932818	1199.550292	14.163776
21.071095	1198.397220	14.168794
21.117725	1206.862476	14.173811
20.780325	1210.066444	14.178829
21.044586	1206.350376	14.183847
21.575313	1213.704897	14.188864
20.933345	1220.489823	14.193882
21.530771	1221.561010	14.198899
21.639955	1238.640782	14.203917
21.624542	1229.100897	14.208935
21.587379	1214.358344	14.213952
21.650762	1215.904056	14.218970
21.651204	1209.421316	14.223987
21.313401	1212.003191	14.229005
21.454392	1205.507473	14.234023
21.550548	1204.169989	14.239040
21.253416	1207.903956	14.244058
21.886163	1212.080294	14.249075
21.514617	1204.242684	14.254093
21.363274	1208.641623	14.259111
21.300598	1215.323919	14.264128
21.507553	1230.738700	14.269146
21.996114	1233.054265	14.274163
21.661661	1234.251288	14.279181
22.048113	1233.725619	14.284199
21.921049	1223.493296	14.289216
21.509023	1225.292601	14.294234
21.906817	1206.349737	14.299251
21.415141	1209.436735	14.304269
21.744992	1230.663359	14.309287
21.628121	1232.065572	14.314304
21.623770	1242.692544	14.319322
21.853999	1242.539447	14.324339
21.707975	1249.955530	14.329357
21.655475	1251.065893	14.334375
21.882915	1235.445012	14.339392
21.661367	1246.513277	14.344410
21.992194	1241.643729	14.349427
21.685886	1245.740195	14.354445
21.634171	1243.199281	14.359463
21.791309	1249.164593	14.364480
21.803107	1250.094019	14.369498
22.036770	1241.045315	14.374515
21.945879	1243.703433	14.379533
22.183000	1242.954607	14.384551
22.113096	1245.817026	14.389568
21.609262	1247.629405	14.394586
22.125804	1258.016778	14.399603
22.308693	1270.509484	14.404621
22.207461	1264.217552	14.409639
22.247032	1268.608079	14.414656
22.243981	1271.109825	14.419674
22.373559	1263.445517	14.424691
22.085776	1269.013025	14.429709
22.264614	1266.719276	14.434727
22.589743	1272.948037	14.439744
22.053976	1266.520128	14.444762
22.600421	1254.988731	14.449779
22.285318	1245.327531	14.454797
22.260134	1250.592797	14.459815
22.481546	1250.260987	14.464832
22.400827	1259.661342	14.469850
22.549737	1249.786119	14.474867
22.329563	1256.309504	14.479885
22.142386	1259.610648	14.484903
22.528053	1275.047309	14.489920
22.731223	1281.429241	14.494938
22.576560	1277.316701	14.499955
22.567245	1273.307612	14.504973
22.381533	1274.389673	14.509991
22.695799	1272.459729	14.515008
22.858823	1283.049021	14.520026
22.795104	1259.307823	14.525043
22.158476	1259.222996	14.530061
22.519197	1263.220933	14.535079
22.704108	1264.035439	14.540096
22.720422	1275.354448	14.545114
23.129408	1275.156320	14.550131
22.905813	1265.935135	14.555149
22.555035	1262.322664	14.560167
22.654848	1260.367938	14.565184
22.488536	1283.752629	14.570202
23.016611	1274.209396	14.575219
22.961897	1279.904119	14.580237
22.744755	1281.832015	14.585255
22.730504	1281.608584	14.590272
22.927341	1276.662866	14.595290
22.594173	1274.678885	14.600307
22.569959	1278.473161	14.605325
22.829408	1278.362596	14.610343
23.189611	1281.916221	14.615360
22.651691	1282.440168	14.620378
22.771555	1277.185816	14.625395
22.795382	1278.350863	14.630413
22.924446	1276.389896	14.635431
22.865865	1273.173641	14.640448
22.773864	1281.204069	14.645466
22.655962	1269.397154	14.650483
22.992036	1279.969853	14.655501
23.039474	1301.981771	14.660519
23.316492	1302.331681	14.665536
22.916542	1309.214116	14.670554
23.393265	1299.932328	14.675571
23.006901	1305.924580	14.680589
22.939893	1308.090452	14.685607
23.382408	1302.635180	14.690624
23.140222	1303.119034	14.695642
23.210979	1308.262833	14.700659
23.103789	1306.073694	14.705677
23.103382	1311.954831	14.710695
23.385271	1309.848354	14.715712
23.023591	1312.904412	14.720730
23.097884	1304.074582	14.725747
23.224713	1309.192920	14.730765
23.341394	1324.762993	14.735783
23.535332	1340.211429	14.740800
23.377241	1332.675560	14.745818
24.108331	1325.724634	14.750835
23.872627	1308.999297	14.755853
23.795953	1308.577387	14.760871
23.863405	1300.266201	14.765888
23.819358	1292.261468	14.770906
24.114641	1288.325703	14.775923
23.536314	1298.368626	14.780941
23.673026	1300.822914	14.785959
23.825798	1298.637142	14.790976
23.948068	1293.431166	14.795994
23.785969	1285.812586	14.801011
23.892845	1296.544558	14.806029
23.556423	1305.641220	14.811047
24.019604	1294.725571	14.816064
23.702435	1294.344383	14.821082
23.964015	1294.701475	14.826099
23.725021	1291.576917	14.831117
23.680754	1293.752531	14.836135
23.857857	1294.090849	14.841152
23.739001	1294.805154	14.846170
23.607889	1295.626811	14.851187
23.694167	1301.871661	14.856205
23.637327	1304.633688	14.861223
23.732791	1295.730483	14.866240
23.556484	1303.484134	14.871258
23.753496	1300.736788	14.876275
23.898919	1317.071514	14.881293
23.975987	1331.118072	14.886311
24.145861	1328.869003	14.891328
23.935974	1329.649742	14.896346
24.635913	1321.895213	14.901363
24.063662	1339.961590	14.906381
24.028853	1333.961068	14.911399
24.235519	1326.434663	14.916416
24.006270	1338.086274	14.921434
24.356587	1338.160998	14.926451
24.673485	1333.481628	14.931469
24.145315	1341.379519	14.936487
24.535686	1326.311454	14.941504
24.091153	1333.038982	14.946522
24.282640	1331.277274	14.951539
24.371215	1330.350781	14.956557
24.237034	1337.052404	14.961575
24.525938	1331.705785	14.966592
24.767897	1332.251633	14.971610
24.612835	1327.508328	14.976627
24.681290	1323.833689	14.981645
24.141360	1313.853572	14.986663
24.783031	1310.684494	14.991680
24.241563	1317.805808	14.996698
24.548178	1317.627155	15.001715
24.300542	1331.288971	15.006733
24.354918	1334.174843	15.011751
24.737420	1324.874246	15.016768
24.651727	1331.962981	15.021786
24.709066	1324.203980	15.026803
25.025014	1338.197497	15.031821
24.512762	1339.208160	15.036839
24.855187	1338.934127	15.041856
24.676740	1335.156503	15.046874
24.806457	1332.209089	15.051891
24.792047	1335.920014	15.056909
24.550686	1336.380141	15.061927
24.603739	1328.961612	15.066944
24.669651	1342.678823	15.071962
24.605851	1333.827741	15.076979
24.586971	1327.078244	15.081997
24.452203	1329.744949	15.087015
24.642338	1326.341925	15.092032
24.661090	1357.353505	15.097050
24.996679	1356.359294	15.102067
24.780493	1376.528008	15.107085
24.843592	1371.119860	15.112103
25.283579	1355.963622	15.117120
25.258158	1364.048759	15.122138
25.106498	1357.843486	15.127155
25.454855	1363.354392	15.132173
25.398115	1362.269383	15.137191
25.358745	1360.715963	15.142208
24.826908	1344.625377	15.147226
25.280560	1353.076133	15.152243
25.320625	1362.874948	15.157261
25.106249	1367.991100	15.162279
25.462183	1358.328973	15.167296
25.221720	1367.275080	15.172314
25.215330	1366.219007	15.177331
25.421664	1367.815083	15.182349
25.187670	1365.728749	15.187367
25.327875	1361.660391	15.192384
25.199443	1367.034981	15.197402
25.008655	1363.492924	15.202419
25.428424	1364.199185	15.207437
25.266702	1374.469877	15.212455
25.719606	1354.515962	15.217472
25.496225	1363.428667	15.222490
25.561727	1369.151443	15.227507
25.337128	1363.907958	15.232525
25.511181	1365.177257	15.237543
25.717888	1363.746616	15.242560
25.615396	1369.206736	15.247578
25.633154	1368.489749	15.252595
25.788129	1355.585256	15.257613
25.609182	1369.796177	15.262631
25.536580	1366.896759	15.267648
25.729480	1367.922367	15.272666
25.731354	1371.577218	15.277683
25.854751	1367.128488	15.282701
25.620210	1367.101438	15.287719
25.805695	1359.666488	15.292736
25.659641	1374.507702	15.297754
25.660350	1367.619774	15.302771
25.745563	1361.941461	15.307789
25.492543	1381.294895	15.312807
26.172300	1389.362737	15.317824
26.255864	1388.643904	15.322842
26.341006	1385.535267	15.327859
26.339338	1377.326302	15.332877
25.835624	1376.470686	15.337895
25.748383	1355.129713	15.342912
25.751012	1368.720182	15.347930
25.837027	1376.597992	15.352947
26.071067	1368.220080	15.357965
25.817232	1385.115670	15.362983
26.148909	1383.898700	15.368000
26.022569	1387.333321	15.373018
26.221766	1383.742424	15.378035
26.305968	1380.826644	15.383053
26.028456	1381.897399	15.388071
26.227184	1383.939879	15.393088
26.097583	1387.392325	15.398106
25.907584	1383.883959	15.403123
26.385786	1388.379172	15.408141
26.224564	1384.349449	15.413159
26.244685	1400.979551	15.418176
26.386449	1410.552951	15.423194
26.290193	1413.949745	15.428211
26.277415	1413.955752	15.433229
26.299206	1419.438541	15.438247
26.420477	1424.366673	15.443264
26.400104	1419.879508	15.448282
26.416824	1418.273875	15.453299
26.991333	1417.177839	15.458317
26.521897	1416.079999	15.463335
26.752393	1411.843846	15.468352
26.661390	1420.820418	15.473370
26.580933	1423.666464	15.478387
26.854752	1417.796014	15.483405
26.625432	1418.471312	15.488423
26.845982	1415.763450	15.493440
26.690525	1414.077524	15.498458
26.814515	1419.809867	15.503475
27.121322	1413.195581	15.508493
26.919819	1432.038256	15.513511
27.008797	1418.194074	15.518528
27.040491	1409.903474	15.523546
26.917590	1416.741767	15.528563
27.155226	1422.613295	15.533581
26.983177	1426.371412	15.538599
27.209215	1419.042442	15.543616
27.203402	1417.112409	15.548634
27.229951	1415.386439	15.553651
27.074381	1410.177546	15.558669
26.993322	1423.782202	15.563687
26.969649	1416.908366	15.568704
27.361763	1413.982005	15.573722
27.275380	1415.958277	15.578739
27.101468	1411.460210	15.583757
27.058392	1417.983734	15.588775
27.257329	1411.095629	15.593792
27.031195	1420.483887	15.598810
26.977961	1426.394734	15.603827
27.121095	1412.968233	15.608845
27.233190	1425.645407	15.613863
27.301942	1420.291398	15.618880
27.235272	1424.403174	15.623898
27.075264	1424.689083	15.628915
26.922656	1422.377388	15.633933
27.249070	1438.985420	15.638951
27.715160	1442.145434	15.643968
27.833431	1439.311516	15.648986
27.246394	1434.215485	15.654003
27.768977	1429.327874	15.659021
27.384926	1430.565859	15.664039
27.725432	1436.901570	15.669056
28.035856	1429.734536	15.674074
27.580202	1420.060244	15.679091
27.871828	1415.523313	15.684109
27.612317	1423.781110	15.689127
27.696394	1419.826301	15.694144
27.396870	1416.085272	15.699162
27.970691	1430.807784	15.704179
28.116154	1423.702461	15.709197
27.782627	1419.780441	15.714215
27.539644	1417.767109	15.719232
27.755982	1420.211863	15.724250
27.869619	1436.709105	15.729267
27.981155	1434.230999	15.734285
27.830049	1445.645276	15.739303
28.019974	1445.029031	15.744320
28.094667	1438.058479	15.749338
27.566619	1449.444003	15.754355
28.130829	1443.034051	15.759373
28.133678	1432.903561	15.764391
28.241362	1439.955997	15.769408
28.291463	1435.780074	15.774426
28.189474	1439.245431	15.779443
28.193520	1437.147860	15.784461
28.042206	1443.953730	15.789479
28.188350	1432.122657	15.794496
28.237865	1437.452371	15.799514
28.135420	1444.069538	15.804531
28.370868	1436.025650	15.809549
28.123075	1446.222027	15.814567
27.996416	1440.289599	15.819584
28.222862	1442.192379	15.824602
28.240385	1438.139635	15.829619
28.359564	1441.316444	15.834637
27.860670	1444.224519	15.839655
28.121709	1445.412306	15.844672
28.555846	1455.138886	15.849690
28.274147	1469.931043	15.854707
28.141823	1471.351474	15.859725
28.560075	1478.064936	15.864743
28.820516	1476.468402	15.869760
28.902133	1471.316827	15.874778
28.725044	1475.321954	15.879795
28.962496	1463.012221	15.884813
28.669840	1472.249092	15.889831
29.022082	1465.732934	15.894848
29.061436	1460.607769	15.899866
28.621519	1455.396235	15.904883
29.027990	1449.186844	15.909901
28.838720	1445.798690	15.914919
28.582173	1443.407611	15.919936
28.904567	1461.189067	15.924954
28.626963	1466.084090	15.929971
29.028546	1467.281710	15.934989
28.849504	1470.552501	15.940007
29.091464	1474.802263	15.945024
29.202099	1460.151510	15.950042
29.146199	1471.332744	15.955059
29.038040	1463.217800	15.960077
29.082765	1465.957364	15.965095
28.900757	1462.643558	15.970112
29.251489	1462.109421	15.975130
29.203359	1466.440847	15.980147
29.488267	1465.935301	15.985165
29.229310	1472.116522	15.990183
29.032103	1464.751214	15.995200
29.453711	1466.383754	16.000218
29.220787	1473.743807	16.005235
29.370211	1466.792783	16.010253
29.241726	1463.625391	16.015271
28.994018	1467.535594	16.020288
29.229292	1462.221079	16.025306
29.301738	1469.733781	16.030323
29.320023	1464.527027	16.035341
28.958032	1465.569575	16.040359
29.089729	1473.167214	16.045376
29.367921	1464.372408	16.050394
29.249796	1473.819768	16.055411
29.636410	1487.853284	16.060429
29.781685	1492.112967	16.065447
29.436355	1501.144314	16.070464
29.572501	1494.616991	16.075482
29.835925	1498.351285	16.080499
30.072352	1493.753132	16.085517
29.989935	1492.179035	16.090535
29.761681	1478.922618	16.095552
30.032292	1472.997598	16.100570
29.523427	1477.463870	16.105587
29.898277	1478.550132	16.110605
29.867341	1482.679821	16.115623
29.661313	1493.601856	16.120640
30.321410	1487.174232	16.125658
30.082539	1492.464231	16.130675
30.386297	1474.477533	16.135693
30.298057	1463.261942	16.140711
30.353179	1465.021369	16.145728
30.526679	1452.367108	16.150746
30.373483	1458.327735	16.155763
30.217112	1453.096144	16.160781
30.177422	1449.563000	16.165799
30.039551	1464.308613	16.170816
30.310142	1457.184887	16.175834
29.982938	1452.292023	16.180851
30.137903	1455.411214	16.185869
30.321023	1460.185553	16.190887
30.098868	1465.998297	16.195904
30.307228	1457.149350	16.200922
30.005216	1457.170029	16.205939
30.298356	1457.732890	16.210957
30.382079	1455.547097	16.215975
30.370290	1446.669560	16.220992
30.577009	1457.540677	16.226010
30.514705	1453.805847	16.231027
30.426235	1455.248384	16.236045
30.622091	1457.959909	16.241063
30.605988	1471.620319	16.246080
30.735303	1456.979961	16.251098
30.396623	1458.394765	16.256115
30.586872	1475.756058	16.261133
30.877939	1472.076550	16.266151
30.918009	1476.946862	16.271168
30.729080	1469.344263	16.276186
30.621321	1464.314925	16.281203
30.881046	1471.194465	16.286221
30.581712	1469.616429	16.291239
30.503497	1470.293583	16.296256
30.997063	1469.999375	16.301274
30.515202	1474.165592	16.306291
30.937215	1475.192417	16.311309
30.973113	1471.611029	16.316327
30.803267	1476.948218	16.321344
31.003395	1473.188041	16.326362
31.054292	1477.654694	16.331379
31.300151	1467.385526	16.336397
31.287759	1476.654778	16.341415
31.048649	1473.686724	16.346432
31.425464	1465.646227	16.351450
31.527990	1470.670179	16.356467
31.382112	1475.389242	16.361485
31.296817	1470.788927	16.366503
31.063766	1467.257518	16.371520
31.460839	1465.452777	16.376538
31.495044	1473.054169	16.381555
31.391791	1462.426959	16.386573
31.425811	1466.616286	16.391591
31.263727	1473.731432	16.396608
31.460281	1464.308602	16.401626
31.399779	1472.613339	16.406643
31.213330	1472.331637	16.411661
31.039880	1467.125576	16.416679
30.856379	1469.763111	16.421696
31.290641	1481.774644	16.426714
31.365861	1496.165383	16.431731
31.545668	1498.577436	16.436749
31.536285	1509.442160	16.441767
31.049768	1515.736780	16.446784
31.668234	1497.306575	16.451802
31.576137	1503.012854	16.456819
31.740462	1510.418894	16.461837
31.632264	1506.052683	16.466855
31.505987	1508.153315	16.471872
31.701841	1518.256954	16.476890
31.997523	1535.900395	16.481907
32.155075	1536.335440	16.486925
32.265170	1539.739462	16.491943
31.998496	1529.294010	16.496960
32.026902	1511.214326	16.501978
32.103231	1511.616705	16.506995
31.975821	1514.202826	16.512013
32.153058	1529.125559	16.517031
32.164699	1531.524326	16.522048
32.252853	1531.243656	16.527066
32.180468	1535.394916	16.532083
32.159908	1538.575158	16.537101
32.129697	1535.451066	16.542119
32.044298	1543.317767	16.547136
32.476195	1533.069218	16.552154
32.421960	1535.569734	16.557171
32.279390	1537.736681	16.562189
32.576239	1532.687616	16.567207
32.572457	1533.835063	16.572224
32.535772	1522.056676	16.577242
32.417472	1529.302514	16.582259
32.511186	1535.369302	16.587277
32.744062	1536.158083	16.592295
32.132325	1535.217433	16.597312
32.525106	1523.917203	16.602330
32.700909	1528.705316	16.607347
32.644432	1523.524624	16.612365
33.036193	1529.775119	16.617383
32.545420	1532.663037	16.622400
33.036463	1523.893236	16.627418
32.599766	1523.629426	16.632435
32.552326	1526.913846	16.637453
32.756238	1522.349187	16.642471
32.415585	1524.282655	16.647488
32.579076	1525.566239	16.652506
32.589214	1532.704283	16.657523
32.550813	1534.602913	16.662541
32.727853	1546.133251	16.667559
32.930202	1561.170782	16.672576
33.219778	1548.678832	16.677594
33.309330	1558.591016	16.682611
33.268853	1561.173505	16.687629
33.347474	1553.180525	16.692647
33.138821	1558.222679	16.697664
33.188852	1559.079955	16.702682
33.425923	1565.824718	16.707699
33.096300	1557.197598	16.712717
33.434382	1561.075740	16.717735
33.354023	1563.766844	16.722752
33.420851	1558.869299	16.727770
33.401793	1563.465908	16.732787
33.039463	1566.235811	16.737805
33.521471	1560.078823	16.742823
33.092215	1567.004594	16.747840
33.388957	1564.582660	16.752858
33.579285	1562.135226	16.757875
33.346926	1564.935524	16.762893
33.666792	1564.407882	16.767911
33.209119	1567.610658	16.772928
33.399142	1565.626559	16.777946
33.623989	1561.348790	16.782963
33.612906	1573.557285	16.787981
33.791672	1565.240778	16.792999
33.709104	1573.741014	16.798016
33.873738	1573.296337	16.803034
33.703248	1568.523951	16.808051
33.964705	1585.098464	16.813069
34.089250	1578.920616	16.818087
33.773290	1572.979786	16.823104
34.138245	1569.378922	16.828122
34.053792	1568.424955	16.833139
33.831162	1570.024192	16.838157
34.145801	1574.956927	16.843175
34.112425	1586.474452	16.848192
34.177492	1591.632631	16.853210
34.457474	1581.372098	16.858227
34.097818	1578.854287	16.863245
34.345090	1566.452446	16.868263
33.855349	1570.230598	16.873280
34.182584	1585.621852	16.878298
34.104738	1585.735772	16.883315
34.036338	1588.771848	16.888333
33.973955	1588.846333	16.893351
33.850980	1585.939961	16.898368
34.257294	1583.686963	16.903386
34.041606	1585.845915	16.908403
34.138966	1603.624112	16.913421
34.501152	1604.221586	16.918439
34.703069	1616.223098	16.923456
35.000330	1616.713731	16.928474
35.018633	1613.943705	16.933491
34.936278	1607.347357	16.938509
34.921831	1588.954280	16.943527
34.782560	1592.273813	16.948544
34.744991	1581.832680	16.953562
34.808658	1580.494052	16.958579
34.675693	1577.951882	16.963597
34.816021	1574.943735	16.968615
34.714108	1579.516596	16.973632
34.807175	1577.949895	16.978650
35.214024	1587.199540	16.983667
35.127146	1593.612144	16.988685
34.977904	1573.876681	16.993703
34.838886	1591.584808	16.998720
35.340176	1591.921765	17.003738
35.374750	1590.348661	17.008755
34.978842	1584.898023	17.013773
35.041302	1571.847637	17.018791
34.988180	1589.896015	17.023808
35.562364	1595.502347	17.028826
35.521761	1590.888572	17.033843
35.047358	1587.423947	17.038861
35.117230	1577.916637	17.043879
35.533451	1600.050307	17.048896
36.030481	1598.228820	17.053914
35.372001	1581.919051	17.058931
35.340129	1576.385967	17.063949
35.440303	1572.669238	17.068967
35.195189	1584.941815	17.073984
35.362566	1602.501190	17.079002
35.532512	1607.551404	17.084019
35.675110	1608.491452	17.089037
35.712803	1604.655684	17.094055
35.746771	1606.461764	17.099072
35.856114	1611.011164	17.104090
35.936380	1610.375437	17.109107
35.751908	1610.780876	17.114125
36.192718	1599.354155	17.119143
35.603773	1589.708087	17.124160
35.693767	1595.260294	17.129178
35.867890	1602.599533	17.134195
35.524301	1607.737951	17.139213
35.717098	1608.941358	17.144231
36.065578	1613.076636	17.149248
35.973509	1610.118922	17.154266
35.817874	1601.301204	17.159283
35.607200	1610.631271	17.164301
35.892602	1605.702779	17.169319
35.714865	1614.369239	17.174336
35.896453	1631.325445	17.179354
36.367057	1633.845304	17.184371
36.026101	1642.379715	17.189389
36.358603	1628.871684	17.194407
36.343231	1641.424650	17.199424
36.399270	1638.104295	17.204442
36.490340	1640.794812	17.209459
36.304767	1640.405207	17.214477
36.545278	1628.404756	17.219495
36.374717	1631.122058	17.224512
36.581216	1636.185330	17.229530
36.222969	1629.063503	17.234547
36.064249	1640.921197	17.239565
36.168122	1636.523481	17.244583
36.488274	1651.575351	17.249600
36.778788	1664.756782	17.254618
36.914282	1660.460202	17.259635
37.193569	1658.645909	17.264653
37.300109	1636.668742	17.269671
37.366763	1633.268825	17.274688
36.934706	1624.722500	17.279706
37.166149	1612.920936	17.284723
37.169873	1622.392218	17.289741
37.495584	1615.483796	17.294759
37.225385	1614.056050	17.299776
37.464571	1617.607826	17.304794
37.530128	1603.559551	17.309811
37.285948	1593.484869	17.314829
37.117312	1573.586534	17.319847
37.546218	1578.972984	17.324864
37.069801	1582.241678	17.329882
37.698784	1576.232712	17.334899
37.037912	1581.999068	17.339917
37.446283	1579.106266	17.344935
37.651523	1577.462680	17.349952
37.293031	1576.862329	17.354970
37.426931	1572.518047	17.359987
37.160548	1580.082492	17.365005
37.371641	1573.263949	17.370023
37.394976	1577.641429	17.375040
37.350298	1584.125167	17.380058
37.660958	1585.249207	17.385075
37.531964	1600.076130	17.390093
37.669486	1603.785701	17.395111
37.547011	1603.810778	17.400128
37.494899	1603.091552	17.405146
37.570128	1602.703610	17.410163
37.092759	1616.032648	17.415181
37.711743	1610.401243	17.420199
37.565140	1611.283593	17.425216
37.295667	1611.217279	17.430234
37.713498	1623.535952	17.435251
37.716055	1637.236803	17.440269
37.910686	1644.283336	17.445287
37.922130	1645.750856	17.450304
37.903852	1647.933389	17.455322
38.072774	1643.461583	17.460339
37.956414	1651.455198	17.465357
38.353950	1645.285692	17.470375
38.454479	1643.495982	17.475392
37.989479	1647.926203	17.480410
38.184268	1643.654779	17.485427
38.015409	1648.712641	17.490445
37.848591	1639.599359	17.495463
37.998789	1659.803626	17.500480
38.032659	1672.840371	17.505498
38.474162	1665.299145	17.510515
38.383918	1679.270473	17.515533
38.324210	1674.057206	17.520551
38.485358	1672.747070	17.525568
38.185244	1680.942269	17.530586
38.611115	1668.774569	17.535603
38.529329	1673.623482	17.540621
38.396466	1674.613764	17.545639
38.820972	1695.289531	17.550656
39.229594	1695.716783	17.555674
38.867560	1673.393484	17.560691
38.705059	1682.358024	17.565709
38.854980	1682.055701	17.570727
39.130298	1693.649138	17.575744
38.914953	1697.739083	17.580762
39.423857	1700.103397	17.585779
39.032268	1683.167307	17.590797
38.879627	1671.036820	17.595815
38.993318	1677.618045	17.600832
38.992414	1696.564355	17.605850
39.347124	1686.348462	17.610867
39.410225	1695.719865	17.615885
39.339269	1690.314890	17.620903
39.206188	1671.938271	17.625920
39.106403	1684.360009	17.630938
39.413080	1692.757326	17.635955
39.277672	1698.833199	17.640973
39.320717	1690.582317	17.645991
39.475052	1695.904059	17.651008
39.429254	1697.928956	17.656026
39.518928	1696.583023	17.661043
39.316795	1700.350727	17.666061
39.616961	1691.530256	17.671079
39.683817	1692.750612	17.676096
39.640407	1694.850638	17.681114
39.720311	1689.841629	17.686131
39.447718	1695.727795	17.691149
39.576652	1689.063100	17.696167
39.721777	1692.336506	17.701184
39.530120	1696.234683	17.706202
39.855349	1694.989615	17.711219
39.860878	1715.266588	17.716237
39.959622	1726.031637	17.721255
40.284401	1714.391297	17.726272
39.881409	1725.806640	17.731290
40.147034	1725.005264	17.736307
40.070727	1728.937751	17.741325
39.963977	1724.830026	17.746343
39.923430	1722.591650	17.751360
40.035168	1727.209924	17.756378
40.160170	1721.578611	17.761395
40.232468	1723.170937	17.766413
40.496955	1725.326470	17.771431
40.743035	1713.516985	17.776448
40.037812	1724.907382	17.781466
40.245780	1721.599744	17.786483
40.314136	1726.702387	17.791501
40.494973	1717.723168	17.796519
40.313758	1726.726116	17.801536
40.530445	1738.523224	17.806554
40.843561	1750.710046	17.811571
40.666691	1761.746403	17.816589
40.705312	1757.736614	17.821607
40.808611	1752.982635	17.826624
40.914256	1756.985216	17.831642
40.954848	1747.528087	17.836659
40.825241	1758.353967	17.841677
40.716909	1757.872594	17.846695
41.177959	1752.736698	17.851712
40.791395	1763.877295	17.856730
41.169291	1751.779318	17.861747
40.910402	1761.517538	17.866765
41.069613	1754.529421	17.871783
41.208048	1749.475661	17.876800
41.040330	1757.723723	17.881818
41.015628	1754.866928	17.886835
40.772006	1756.246932	17.891853
41.236467	1754.559620	17.896871
41.023719	1751.017037	17.901888
40.653509	1755.845123	17.906906
41.255224	1766.555934	17.911923
41.484602	1775.130022	17.916941
41.513332	1781.182895	17.921959
41.721236	1770.589206	17.926976
41.659684	1778.017253	17.931994
41.600986	1779.889263	17.937011
41.446512	1780.380377	17.942029
41.901621	1781.785798	17.947047
41.961912	1767.102652	17.952064
41.857981	1787.035359	17.957082
41.842073	1778.240868	17.962099
41.502565	1779.636168	17.967117
42.051927	1778.576371	17.972135
42.260157	1771.183207	17.977152
41.983050	1774.052821	17.982170
41.837603	1771.944436	17.987187
42.112706	1771.563152	17.992205
41.916662	1772.252821	17.997223
42.160894	1770.634458	18.002240
41.716778	1779.103598	18.007258
42.120463	1763.634168	18.012275
41.777042	1769.726730	18.017293
41.824064	1780.072173	18.022311
42.091997	1764.700692	18.027328
42.189101	1779.182609	18.032346
42.037914	1789.466071	18.037363
42.522597	1786.690842	18.042381
42.516088	1805.512335	18.047399
42.286531	1801.580705	18.052416
42.230493	1810.502385	18.057434
42.579996	1797.109474	18.062451
42.337228	1802.115464	18.067469
42.168699	1811.590747	18.072487
42.383912	1803.466508	18.077504
42.306855	1814.688349	18.082522
42.340814	1827.591499	18.087539
42.897554	1831.361687	18.092557
43.061576	1825.706807	18.097575
43.316555	1831.197392	18.102592
42.881348	1837.242483	18.107610
42.926363	1827.237925	18.112627
43.225544	1822.385821	18.117645
42.800771	1837.242857	18.122663
43.113970	1822.229855	18.127680
43.205277	1823.339348	18.132698
43.479368	1818.337864	18.137715
43.209347	1819.084956	18.142733
43.035527	1824.263230	18.147751
43.188198	1821.032822	18.152768
43.051106	1823.499409	18.157786
43.261884	1819.635190	18.162803
43.246456	1819.960971	18.167821
43.057506	1834.522392	18.172839
43.388809	1825.318531	18.177856
43.350658	1826.834095	18.182874
43.403576	1836.865579	18.187891
43.847733	1852.413876	18.192909
43.723493	1862.490152	18.197927
43.760016	1854.274041	18.202944
43.858203	1856.039233	18.207962
43.451371	1854.790571	18.212979
43.881064	1852.858662	18.217997
43.505249	1860.014378	18.223015
43.793317	1857.228022	18.228032
43.835335	1860.383408	18.233050
44.185707	1856.760418	18.238067
44.277976	1857.643225	18.243085
43.730350	1854.277522	18.248103
44.296221	1845.453122	18.253120
44.011967	1860.375865	18.258138
44.095038	1855.498440	18.263155
44.032374	1858.453427	18.268173
43.802625	1856.039911	18.273191
44.246802	1849.401160	18.278208
44.093186	1859.667753	18.283226
44.429089	1866.887719	18.288243
44.777942	1871.724644	18.293261
44.353831	1864.643882	18.298279
44.767872	1859.348693	18.303296
44.441760	1863.826044	18.308314
44.545344	1870.956429	18.313331
44.969589	1872.361276	18.318349
44.791922	1884.595815	18.323367
44.817143	1870.113231	18.328384
44.770261	1861.466787	18.333402
44.895189	1865.804552	18.338419
45.016851	1878.782643	18.343437
44.785913	1875.707799	18.348455
45.121722	1873.225311	18.353472
45.011656	1881.520881	18.358490
44.837812	1884.270217	18.363507
45.071163	1889.297045	18.368525
44.770661	1886.978187	18.373543
44.698661	1880.686831	18.378560
44.924062	1884.217274	18.383578
45.045726	1884.882230	18.388595
45.135031	1879.176320	18.393613
45.055294	1878.452834	18.398631
45.078484	1871.971677	18.403648
45.051285	1896.288495	18.408666
45.055221	1905.438215	18.413683
45.380004	1902.428111	18.418701
45.318654	1915.702863	18.423719
45.554764	1907.931557	18.428736
45.441667	1917.127481	18.433754
45.398306	1911.762071	18.438771
45.783855	1904.091211	18.443789
45.674010	1914.515257	18.448807
45.613374	1913.164175	18.453824
45.716966	1910.434764	18.458842
45.509238	1916.510463	18.463859
46.064823	1923.282462	18.468877
46.220654	1937.429524	18.473895
46.033984	1926.370074	18.478912
46.342994	1925.102404	18.483930
46.393473	1920.363089	18.488947
46.347066	1906.071235	18.493965
46.101415	1908.049379	18.498983
46.409536	1905.664905	18.504000
46.281038	1908.648494	18.509018
46.108084	1907.584339	18.514035
46.409883	1904.931076	18.519053
46.429440	1895.337982	18.524071
46.762204	1881.470995	18.529088
46.560735	1887.909085	18.534106
46.622411	1888.364940	18.539123
46.825500	1882.616495	18.544141
47.002588	1887.947265	18.549159
46.962882	1879.507323	18.554176
47.159229	1885.206286	18.559194
47.079953	1883.781096	18.564211
46.932141	1880.324872	18.569229
47.013209	1882.176962	18.574247
47.311338	1877.700207	18.579264
47.324058	1880.928703	18.584282
47.240605	1864.904454	18.589299
47.071002	1842.757071	18.594317
47.133380	1851.999691	18.599335
47.311432	1839.866658	18.604352
47.161595	1833.321873	18.609370
47.187413	1840.094955	18.614387
47.039141	1837.334937	18.619405
47.049422	1843.027379	18.624423
47.332427	1856.542120	18.629440
47.200265	1866.305818	18.634458
47.370770	1872.994484	18.639475
47.663601	1872.853423	18.644493
47.161287	1875.910787	18.649511
47.642420	1873.619070	18.654528
47.645087	1883.460383	18.659546
47.438020	1879.911355	18.664563
47.667916	1870.482160	18.669581
47.412283	1874.038199	18.674599
47.744534	1875.725158	18.679616
47.565109	1870.920272	18.684634
47.351074	1876.698847	18.689651
47.521785	1874.458216	18.694669
47.433639	1887.703394	18.699687
47.586116	1899.548631	18.704704
47.629403	1909.401574	18.709722
47.559842	1905.568675	18.714739
47.881888	1900.557942	18.719757
47.967926	1907.192450	18.724775
47.907110	1902.419765	18.729792
47.889172	1917.628880	18.734810
47.921897	1928.710591	18.739827
48.215893	1925.574033	18.744845
48.433249	1928.990930	18.749863
48.382289	1931.445370	18.754880
48.302981	1937.454973	18.759898
48.308370	1933.324582	18.764915
48.809619	1921.489962	18.769933
48.678635	1933.159408	18.774951
48.749538	1929.485800	18.779968
48.659981	1935.019580	18.784986
48.499056	1931.730618	18.790003
48.881787	1927.111355	18.795021
48.450177	1935.065737	18.800039
48.499174	1931.342921	18.805056
49.072864	1942.711199	18.810074
48.786767	1955.487744	18.815091
49.092358	1954.484911	18.820109
48.946472	1962.879844	18.825127
49.548339	1956.181284	18.830144
49.453193	1951.716106	18.835162
49.264457	1958.553354	18.840179
49.749231	1947.062719	18.845197
49.409727	1934.877651	18.850215
49.318088	1923.867544	18.855232
49.445405	1928.285965	18.860250
49.011320	1932.600430	18.865267
49.608462	1937.986141	18.870285
49.527848	1943.511418	18.875303
49.669810	1945.438755	18.880320
49.718450	1948.412189	18.885338
49.684748	1959.189884	18.890355
49.670991	1947.132978	18.895373
49.473215	1952.894043	18.900391
49.192445	1955.135008	18.905408
49.489925	1944.262614	18.910426
49.205851	1950.277351	18.915443
49.580504	1965.287819	18.920461
49.575787	1978.931158	18.925479
49.700921	1976.807902	18.930496
49.902687	1984.150793	18.935514
49.693933	1979.459099	18.940531
49.982170	1981.361536	18.945549
50.160583	2000.697317	18.950567
50.273232	2002.717435	18.955584
50.915652	2008.453061	18.960602
50.471905	2001.545266	18.965619
50.674678	1985.204646	18.970637
50.694214	1979.337562	18.975655
50.427855	1975.743693	18.980672
50.616717	1968.167884	18.985690
50.469847	1984.207031	18.990707
50.413223	1974.312974	18.995725
50.467864	1989.124374	19.000743
50.693366	2010.982322	19.005760
51.017695	2009.911210	19.010778
50.905032	2014.749429	19.015795
51.029180	2004.271973	19.020813
51.209881	2009.063399	19.025831
51.129781	2006.421476	19.030848
51.147241	2002.468483	19.035866
50.761940	2019.039674	19.040883
51.332771	2003.977528	19.045901
51.159414	2008.438424	19.050919
51.138419	2013.505077	19.055936
51.196135	2007.653130	19.060954
51.185102	2008.705021	19.065971
51.137896	2006.701281	19.070989
51.310113	2005.879394	19.076007
51.473558	2008.499443	19.081024
51.342522	1995.622699	19.086042
51.314102	2002.089085	19.091059
51.527895	1998.600328	19.096077
51.473369	2005.224264	19.101095
51.224139	2010.148764	19.106112
52.238491	2011.302187	19.111130
51.828517	2038.168273	19.116147
52.085890	2036.363724	19.121165
52.058105	2039.406001	19.126183
51.948014	2024.340746	19.131200
52.422591	2028.313661	19.136218
51.967621	2021.167737	19.141235
51.722386	2017.575207	19.146253
52.239160	2021.633421	19.151271
52.072838	2027.746611	19.156288
51.997769	2037.178815	19.161306
52.192027	2028.818671	19.166323
52.105625	2028.336937	19.171341
51.959018	2030.433019	19.176359
52.029767	2033.151236	19.181376
52.329232	2032.823482	19.186394
52.227813	2056.325699	19.191411
52.316886	2054.672273	19.196429
52.445967	2061.346395	19.201447
52.514237	2065.358955	19.206464
52.675390	2056.680000	19.211482
52.425562	2056.350972	19.216499
52.707199	2055.949762	19.221517
52.837848	2067.635793	19.226535
52.959590	2082.968321	19.231552
53.165360	2081.790259	19.236570
53.201209	2093.065885	19.241587
53.232233	2082.103741	19.246605
53.202837	2080.200193	19.251623
53.291416	2069.447551	19.256640
53.366631	2062.937560	19.261658
53.060475	2067.925434	19.266675
53.496222	2070.410817	19.271693
53.437050	2084.073952	19.276711
53.328638	2082.467753	19.281728
53.794629	2077.297135	19.286746
53.557567	2088.402333	19.291763
53.911656	2080.417043	19.296781
53.480149	2074.647818	19.301799
53.354692	2084.093595	19.306816
53.842011	2079.850113	19.311834
53.349452	2092.714769	19.316851
53.607707	2087.115551	19.321869
53.872945	2083.248871	19.326887
53.789302	2085.973631	19.331904
53.704368	2075.879506	19.336922
53.518583	2084.393355	19.341939
54.052575	2098.077523	19.346957
54.003585	2103.700861	19.351975
53.918107	2107.973147	19.356992
54.537485	2114.175795	19.362010
54.358629	2113.420124	19.367027
54.471690	2113.589336	19.372045
54.645699	2101.441000	19.377063
54.585002	2107.564906	19.382080
54.291027	2108.866447	19.387098
54.273036	2115.535734	19.392115
54.438995	2104.503282	19.397133
54.715818	2108.941962	19.402151
54.511617	2109.651037	19.407168
54.513209	2100.193608	19.412186
54.892319	2108.473425	19.417203
54.812981	2104.674284	19.422221
54.528216	2109.257596	19.427239
54.772685	2125.780376	19.432256
55.384007	2129.420018	19.437274
55.374136	2125.017486	19.442291
55.392397	2126.008865	19.447309
55.414767	2126.928008	19.452327
54.990891	2123.133472	19.457344
55.471683	2122.631276	19.462362
55.460798	2128.383839	19.467379
55.427310	2124.061374	19.472397
55.563859	2119.424682	19.477415
55.526394	2130.976326	19.482432
55.924994	2117.117495	19.487450
55.691500	2131.428314	19.492467
55.612788	2129.142474	19.497485
56.120261	2133.773272	19.502503
55.582059	2130.829187	19.507520
55.689547	2122.208308	19.512538
55.901013	2125.948696	19.517555
55.579925	2125.234588	19.522573
55.756462	2126.494908	19.527591
55.708830	2118.977980	19.532608
56.319216	2112.960756	19.537626
56.509857	2103.934115	19.542643
56.335440	2105.066347	19.547661
56.528875	2099.193503	19.552679
56.154684	2103.833553	19.557696
56.233227	2098.439192	19.562714
56.615580	2098.119454	19.567731
56.494084	2091.710046	19.572749
56.523664	2098.942017	19.577767
56.476747	2103.885408	19.582784
56.581130	2088.888134	19.587802
56.637969	2095.449513	19.592819
56.506152	2100.984590	19.597837
56.781096	2093.501177	19.602855
56.687638	2101.243608	19.607872
56.968613	2093.242442	19.612890
56.789658	2102.481238	19.617907
56.897494	2105.645844	19.622925
57.087956	2111.664406	19.627943
56.920490	2114.576378	19.632960
57.314332	2116.551662	19.637978
57.402243	2121.588397	19.642995
57.182432	2110.239118	19.648013
57.253328	2110.277402	19.653031
56.930642	2109.517140	19.658048
57.312197	2106.716615	19.663066
57.071595	2107.169560	19.668083
57.211957	2111.531681	19.673101
57.664385	2102.308329	19.678119
57.770823	2112.517103	19.683136
58.029442	2113.766691	19.688154
57.886160	2104.658015	19.693171
57.868857	2111.515973	19.698189
58.064059	2107.893288	19.703207
57.635187	2112.886590	19.708224
57.922195	2108.059147	19.713242
57.715628	2127.120625	19.718259
57.868933	2132.804527	19.723277
57.890760	2148.091706	19.728295
57.992824	2142.766730	19.733312
58.235848	2140.559361	19.738330
58.266899	2135.714525	19.743347
58.205610	2140.269283	19.748365
58.333130	2143.160955	19.753383
58.377703	2139.990196	19.758400
58.577907	2144.795075	19.763418
58.396297	2144.511012	19.768435
58.072271	2159.320840	19.773453
58.410139	2167.312295	19.778471
58.578115	2171.699134	19.783488
58.718316	2170.152384	19.788506
59.003813	2171.310378	19.793523
59.048586	2167.837527	19.798541
58.883880	2170.257447	19.803559
58.701240	2173.994631	19.808576
58.763036	2170.583565	19.813594
58.866998	2174.695867	19.818611
58.985094	2185.712242	19.823629
59.095557	2193.517375	19.828647
58.910947	2196.545367	19.833664
59.252700	2194.960175	19.838682
59.397858	2193.291496	19.843699
58.963257	2193.415910	19.848717
59.161538	2198.673408	19.853735
59.255411	2214.378648	19.858752
59.597741	2216.845134	19.863770
59.766556	2215.038171	19.868787
59.758270	2221.778325	19.873805
60.089062	2215.872515	19.878823
59.941013	2227.526826	19.883840
60.215357	2223.426610	19.888858
60.090869	2225.238375	19.893875
60.103400	2220.136100	19.898893
60.259545	2211.671808	19.903911
59.974376	2221.774786	19.908928
59.875742	2215.194917	19.913946
60.179660	2217.995542	19.918963
60.164114	2220.959605	19.923981
60.232927	2209.380937	19.928999
60.217786	2214.194228	19.934016
60.267022	2217.502713	19.939034
60.369999	2220.646881	19.944051
60.459786	2232.694319	19.949069
60.515934	2243.998288	19.954087
60.348089	2251.172937	19.959104
60.405882	2245.209186	19.964122
60.481630	2250.209362	19.969139
60.303715	2255.403385	19.974157
61.148237	2262.807513	19.979175
61.087225	2273.098170	19.984192
61.270476	2278.971643	19.989210
61.406458	2275.202616	19.994227
61.293178	2278.499279	19.999245
61.392252	2271.552759	20.004263
61.463945	2281.466711	20.009280
61.424034	2272.097596	20.014298
61.576031	2278.539262	20.019315
61.626448	2277.595199	20.024333
61.875832	2265.762718	20.029351
61.669682	2271.871349	20.034368
61.787902	2270.390236	20.039386
61.738499	2260.628555	20.044403
61.712609	2279.264180	20.049421
61.788107	2269.870367	20.054439
61.758569	2273.104116	20.059456
61.846469	2275.700079	20.064474
62.081125	2267.713286	20.069491
61.557695	2268.206626	20.074509
61.987010	2265.706015	20.079527
61.724136	2274.035618	20.084544
61.835845	2272.568916	20.089562
62.021862	2289.028837	20.094579
61.975142	2302.288235	20.099597
62.228183	2299.689090	20.104615
62.504154	2299.286418	20.109632
62.652228	2300.592984	20.114650
62.716254	2304.887105	20.119667
62.316844	2308.312004	20.124685
62.847767	2300.845082	20.129703
62.552190	2298.390861	20.134720
62.458484	2300.347180	20.139738
62.687427	2304.711750	20.144755
62.703876	2319.530364	20.149773
62.867242	2328.447257	20.154791
63.059952	2331.073710	20.159808
62.873526	2336.844914	20.164826
62.929679	2327.211875	20.169843
62.521135	2335.857364	20.174861
63.167328	2340.891659	20.179879
63.276342	2350.898032	20.184896
63.355998	2361.061695	20.189914
63.435701	2357.609973	20.194931
63.291876	2361.628125	20.199949
63.587035	2360.475116	20.204967
63.423622	2360.927556	20.209984
63.702977	2361.557945	20.215002
63.821639	2365.565698	20.220019
63.547499	2358.946108	20.225037
63.619621	2371.906582	20.230055
63.544803	2382.181425	20.235072
64.046814	2385.284010	20.240090
64.034513	2383.332073	20.245107
64.134088	2384.247572	20.250125
64.285059	2373.778947	20.255143
64.197442	2382.514867	20.260160
64.063706	2386.019334	20.265178
64.664829	2378.088877	20.270195
64.387728	2382.110199	20.275213
64.470336	2382.877375	20.280231
64.698552	2404.355550	20.285248
64.847302	2412.028050	20.290266
64.832753	2411.018826	20.295283
64.839004	2415.432320	20.300301
65.184134	2392.746557	20.305319
65.363945	2403.840567	20.310336
65.188338	2385.827736	20.315354
65.045191	2381.428291	20.320371
65.051120	2378.941699	20.325389
65.480499	2375.129785	20.330407
65.449761	2378.948199	20.335424
65.057172	2373.256813	20.340442
65.157743	2383.745172	20.345459
64.995064	2402.783490	20.350477
65.365147	2397.699640	20.355495
65.145983	2405.049311	20.360512
65.212141	2396.264169	20.365530
65.826318	2399.345722	20.370547
65.406516	2410.258484	20.375565
65.656569	2403.577294	20.380583
65.946448	2403.045758	20.385600
65.659266	2414.948165	20.390618
65.953235	2418.069780	20.395635
65.875275	2429.409441	20.400653
66.022994	2430.027791	20.405671
66.009068	2444.079710	20.410688
66.005586	2427.533150	20.415706
66.634494	2429.231859	20.420723
66.116482	2433.802915	20.425741
66.182311	2425.517307	20.430759
66.456139	2432.067827	20.435776
66.447892	2438.747506	20.440794
66.586454	2439.696121	20.445811
66.470253	2436.331475	20.450829
66.756539	2451.094599	20.455847
67.028776	2460.057925	20.460864
67.210081	2470.123644	20.465882
67.130179	2448.698090	20.470899
67.008595	2442.405746	20.475917
67.148829	2443.285659	20.480935
67.093156	2456.563930	20.485952
67.417308	2457.052669	20.490970
67.485009	2460.708307	20.495987
67.167214	2456.193531	20.501005
67.673151	2454.600218	20.506023
67.397608	2459.945181	20.511040
67.127441	2465.764403	20.516058
67.752856	2451.830538	20.521075
67.404739	2457.549703	20.526093
67.663125	2451.793792	20.531111
67.715213	2453.248618	20.536128
67.469200	2459.407734	20.541146
67.657942	2450.819327	20.546163
67.424334	2451.728188	20.551181
67.970603	2469.061417	20.556199
68.099995	2478.980460	20.561216
67.980605	2480.446120	20.566234
68.202648	2484.197500	20.571251
68.250251	2483.828888	20.576269
68.178959	2471.519569	20.581287
68.307033	2478.511048	20.586304
68.079697	2485.922631	20.591322
68.399784	2483.956212	20.596339
68.400395	2506.765605	20.601357
68.530729	2512.796284	20.606375
68.653898	2517.369722	20.611392
68.415141	2510.071864	20.616410
68.708161	2508.482613	20.621427
68.597812	2509.792657	20.626445
68.698436	2509.123754	20.631463
69.136534	2515.513601	20.636480
69.313187	2528.937379	20.641498
69.278950	2538.056612	20.646515
69.273241	2535.965159	20.651533
69.617133	2529.949368	20.656551
69.742375	2527.689933	20.661568
69.300388	2515.556905	20.666586
69.842745	2521.591096	20.671603
69.722559	2521.795942	20.676621
69.407644	2511.679199	20.681639
69.400593	2519.009255	20.686656
69.529038	2529.134576	20.691674
69.816691	2525.831357	20.696691
69.398885	2536.164158	20.701709
69.759862	2528.887843	20.706727
69.877023	2530.253637	20.711744
70.102297	2551.277834	20.716762
70.231103	2553.470868	20.721779
70.113222	2561.264634	20.726797
70.263728	2566.286820	20.731815
70.450011	2558.965197	20.736832
70.317930	2557.491725	20.741850
70.526886	2560.145520	20.746867
70.340288	2553.849338	20.751885
70.413218	2556.972413	20.756903
70.701543	2557.577783	20.761920
70.535711	2560.451037	20.766938
70.896927	2570.055492	20.771955
71.028833	2586.022517	20.776973
71.044776	2588.064433	20.781991
71.133250	2584.874776	20.787008
70.848950	2589.932493	20.792026
71.091432	2581.193848	20.797043
71.540953	2580.139702	20.802061
71.955321	2575.707130	20.807079
72.055589	2571.887086	20.812096
72.061752	2577.666213	20.817114
71.827505	2561.061912	20.822131
71.709715	2547.783752	20.827149
71.437076	2538.866131	20.832167
71.802540	2558.044602	20.837184
71.839271	2565.531316	20.842202
72.171349	2566.342095	20.847219
71.993620	2574.924165	20.852237
71.655749	2576.184761	20.857255
72.041876	2568.983077	20.862272
71.747256	2574.899063	20.867290
72.188232	2562.166573	20.872307
72.286635	2564.867893	20.877325
72.016930	2572.434161	20.882343
72.142807	2586.455267	20.887360
72.214677	2594.880334	20.892378
72.657183	2592.145514	20.897395
72.392908	2608.723238	20.902413
72.509773	2604.383730	20.907431
72.994958	2593.629592	20.912448
72.333413	2605.075836	20.917466
72.876524	2601.366866	20.922483
72.704792	2598.399629	20.927501
72.640135	2624.055380	20.932519
73.196756	2624.506263	20.937536
72.982132	2627.421137	20.942554
73.376789	2620.845005	20.947571
73.164386	2622.856482	20.952589
73.342482	2618.096588	20.957607
73.781905	2624.963752	20.962624
73.237383	2622.867760	20.967642
73.168429	2629.175697	20.972659
73.153189	2645.220531	20.977677
73.501745	2658.008952	20.982695
73.752204	2648.274703	20.987712
73.683702	2657.590625	20.992730
74.109536	2654.266126	20.997747
73.872756	2650.114373	21.002765
73.853843	2669.260686	21.007783
74.077374	2668.310228	21.012800
74.002633	2684.617101	21.017818
74.215711	2683.498398	21.022835
74.477731	2685.800786	21.027853
74.460063	2673.506343	21.032871
74.866323	2681.373116	21.037888
74.625236	2680.050742	21.042906
74.710359	2679.479485	21.047923
74.885047	2677.421383	21.052941
74.903954	2683.594191	21.057959
74.904108	2668.925237	21.062976
74.927004	2677.672812	21.067994
75.290015	2679.649948	21.073011
75.235533	2682.500747	21.078029
74.860549	2703.040369	21.083047
75.400906	2704.750877	21.088064
75.247219	2715.071569	21.093082
75.410888	2713.704305	21.098099
75.471740	2708.041155	21.103117
75.420738	2708.080003	21.108135
75.854199	2699.365893	21.113152
75.607789	2714.723977	21.118170
75.632211	2707.615312	21.123187
76.095296	2710.659676	21.128205
75.765781	2707.863894	21.133223
75.872749	2707.442544	21.138240
76.140351	2728.381583	21.143258
75.953341	2732.549103	21.148275
76.104940	2735.924763	21.153293
76.129954	2741.462599	21.158311
76.484723	2738.694549	21.163328
76.436902	2735.145870	21.168346
76.060013	2733.938758	21.173363
76.309141	2734.846947	21.178381
76.554434	2751.415931	21.183399
76.570709	2760.344749	21.188416
76.231277	2766.415843	21.193434
76.677669	2767.666221	21.198451
76.938308	2767.142485	21.203469
76.839428	2764.609613	21.208487
77.101984	2758.719977	21.213504
76.916739	2763.903548	21.218522
77.051580	2784.052040	21.223539
77.469677	2787.540962	21.228557
77.476045	2790.547269	21.233575
77.439051	2796.452932	21.238592
77.926133	2786.544767	21.243610
78.130325	2785.352744	21.248627
78.042525	2789.426580	21.253645
77.829594	2787.302063	21.258663
78.256592	2767.457346	21.263680
77.717704	2766.648145	21.268698
77.373036	2781.878803	21.273715
77.915336	2788.049203	21.278733
77.905994	2782.843239	21.283751
77.966541	2781.337449	21.288768
77.875148	2790.855337	21.293786
78.047251	2803.804968	21.298803
78.270660	2805.512547	21.303821
78.382203	2814.170549	21.308839
78.555268	2815.812216	21.313856
78.867504	2811.000187	21.318874
78.656258	2817.403269	21.323891
78.963892	2810.945555	21.328909
78.839475	2808.928845	21.333927
78.804582	2806.724799	21.338944
78.947616	2816.926657	21.343962
79.092837	2823.813305	21.348979
79.438147	2828.000576	21.353997
78.951420	2835.581925	21.359015
79.411623	2830.695947	21.364032
79.397540	2831.440809	21.369050
79.464168	2837.962416	21.374067
79.846802	2822.541644	21.379085
79.745844	2825.616993	21.384103
79.676943	2824.451216	21.389120
79.688602	2825.597875	21.394138
79.849631	2824.544888	21.399155
80.216485	2833.034748	21.404173
80.061242	2853.094299	21.409191
80.250078	2855.470530	21.414208
80.424884	2861.866339	21.419226
80.425927	2856.932440	21.424243
80.451116	2853.587626	21.429261
80.514874	2859.533884	21.434279
80.558664	2861.253597	21.439296
80.305305	2866.194771	21.444314
80.450199	2863.729199	21.449331
80.646772	2853.153058	21.454349
80.695854	2859.169307	21.459367
80.846631	2850.253189	21.464384
80.691178	2850.926990	21.469402
80.600650	2870.215569	21.474419
80.966836	2879.720321	21.479437
81.140683	2890.032164	21.484455
81.260433	2877.640117	21.489472
81.432668	2887.931763	21.494490
81.106332	2880.299206	21.499507
81.654738	2872.315539	21.504525
81.313197	2881.562660	21.509543
81.522048	2886.865921	21.514560
81.590207	2905.846049	21.519578
82.047288	2910.630667	21.524595
82.190093	2905.176203	21.529613
82.168526	2916.028971	21.534631
82.316273	2905.548682	21.539648
82.138374	2900.823448	21.544666
82.260294	2906.076862	21.549683
82.304368	2903.673774	21.554701
82.035461	2902.613046	21.559719
82.317836	2899.957989	21.564736
82.469003	2900.305208	21.569754
82.472681	2899.999442	21.574771
82.714085	2901.545263	21.579789
82.798721	2916.496774	21.584807
82.821454	2916.873917	21.589824
82.598293	2916.690858	21.594842
82.994501	2922.585694	21.599859
82.953811	2919.311943	21.604877
82.821721	2921.527763	21.609895
82.737087	2924.494333	21.614912
82.926382	2938.496223	21.619930
83.206086	2949.742271	21.624947
83.110569	2950.727467	21.629965
83.040384	2966.282686	21.634983
83.730149	2978.106043	21.640000
83.679327	2985.256879	21.645018
83.495704	2985.506459	21.650035
83.954498	2979.085922	21.655053
83.768654	2988.858141	21.660071
84.262724	2981.942686	21.665088
84.232217	2981.710809	21.670106
84.075844	2977.615362	21.675123
84.464946	2993.051735	21.680141
84.268904	3007.190664	21.685159
84.614144	3004.115722	21.690176
84.892122	3013.056448	21.695194
84.593636	3013.702723	21.700211
84.960772	3009.471857	21.705229
85.052805	3008.291411	21.710247
84.793226	3007.867154	21.715264
85.312663	3001.929374	21.720282
85.112055	3003.280601	21.725299
85.520736	2992.751556	21.730317
85.365272	2999.591846	21.735335
85.370020	2998.895733	21.740352
85.692277	2997.396954	21.745370
85.465161	3006.894936	21.750387
86.029417	2993.394318	21.755405
85.364891	3000.641465	21.760423
85.787775	2998.148056	21.765440
85.910395	2998.654012	21.770458
85.731151	3002.116324	21.775475
85.753249	2993.603737	21.780493
85.496409	3000.110139	21.785511
85.845710	3001.969152	21.790528
85.773919	3019.956195	21.795546
85.649664	3029.999449	21.800563
86.319847	3022.254300	21.805581
86.243853	3028.136384	21.810599
86.287117	3045.433315	21.815616
86.415321	3051.025609	21.820634
86.726103	3049.676544	21.825651
87.033263	3036.576386	21.830669
86.996606	3053.049871	21.835687
87.215346	3053.236068	21.840704
87.093972	3052.753582	21.845722
86.791320	3046.158677	21.850739
87.194810	3042.271274	21.855757
87.123651	3054.372590	21.860775
87.115025	3065.320949	21.865792
87.253057	3070.799980	21.870810
87.417202	3082.279315	21.875827
87.516627	3079.754094	21.880845
87.469942	3081.865852	21.885863
87.574987	3078.215619	21.890880
88.168413	3090.727801	21.895898
87.503164	3101.515807	21.900915
88.289544	3104.916180	21.905933
88.281884	3097.158740	21.910951
88.341951	3106.238901	21.915968
88.373667	3096.702078	21.920986
88.404291	3104.828012	21.926003
88.750927	3092.265869	21.931021
88.402864	3103.977946	21.936039
88.662502	3102.542635	21.941056
88.680625	3097.591772	21.946074
88.639874	3110.415934	21.951091
89.173380	3120.129367	21.956109
89.026831	3129.465116	21.961127
88.987369	3131.715753	21.966144
89.079597	3125.319789	21.971162
88.971779	3136.315486	21.976179
89.402297	3125.967726	21.981197
89.288841	3125.800993	21.986215
89.015677	3133.630840	21.991232
89.539490	3138.328588	21.996250
89.334608	3146.146764	22.001267
89.766721	3146.931400	22.006285
89.632551	3154.750891	22.011303
89.408122	3152.777616	22.016320
89.703554	3168.539054	22.021338
89.628811	3182.374826	22.026355
90.136734	3182.827993	22.031373
90.168411	3178.276920	22.036391
90.227255	3185.516562	22.041408
90.652875	3176.439990	22.046426
90.356669	3190.853091	22.051443
90.853821	3200.241196	22.056461
91.059313	3213.118214	22.061479
91.137223	3213.639962	22.066496
91.059876	3209.253371	22.071514
91.002483	3215.272587	22.076531
91.432914	3209.992402	22.081549
91.196303	3219.082975	22.086567
91.260504	3209.587311	22.091584
91.346552	3208.861703	22.096602
91.299215	3221.813663	22.101619
91.609446	3212.695686	22.106637
91.161392	3214.569400	22.111655
91.589146	3214.578309	22.116672
91.681208	3219.519577	22.121690
91.671443	3230.960685	22.126707
92.073699	3231.429133	22.131725
92.182094	3239.947865	22.136743
91.625420	3240.139733	22.141760
91.998623	3231.670130	22.146778
91.659317	3244.880284	22.151795
92.326204	3258.184857	22.156813
92.518812	3263.493992	22.161831
92.378686	3266.786503	22.166848
92.443240	3264.147241	22.171866
92.381606	3269.202716	22.176883
92.979267	3275.330672	22.181901
92.887838	3291.046955	22.186919
93.137660	3289.718604	22.191936
93.673571	3288.426441	22.196954
93.428249	3295.931763	22.201971
93.477822	3285.201758	22.206989
93.460483	3290.877142	22.212007
93.488548	3290.568266	22.217024
93.452193	3288.110290	22.222042
93.612709	3290.320406	22.227059
93.783553	3280.579558	22.232077
93.698923	3288.456511	22.237095
93.860347	3305.302243	22.242112
94.327433	3304.843898	22.247130
94.238823	3317.519328	22.252147
94.706043	3316.860364	22.257165
94.456902	3316.601989	22.262183
94.524581	3314.153378	22.267200
94.606429	3307.479726	22.272218
94.400572	3315.532572	22.277235
94.526552	3304.800594	22.282253
94.746085	3316.117881	22.287271
94.367144	3315.478225	22.292288
94.880609	3311.255404	22.297306
94.862974	3338.316170	22.302323
94.901636	3334.267397	22.307341
95.136237	3330.144110	22.312359
95.088706	3331.071331	22.317376
95.093642	3330.091976	22.322394
95.152005	3339.296058	22.327411
95.546909	3352.150858	22.332429
95.587790	3355.822798	22.337447
95.506713	3364.472512	22.342464
95.987742	3365.066856	22.347482
95.931825	3363.920204	22.352499
96.166412	3364.748155	22.357517
96.235563	3369.923619	22.362535
96.155250	3371.257268	22.367552
96.186382	3374.923688	22.372570
96.401233	3384.718798	22.377587
96.566398	3386.048699	22.382605
96.568748	3397.607578	22.387623
96.582320	3405.712011	22.392640
97.046189	3394.132338	22.397658
96.904048	3389.386295	22.402675
96.955562	3385.569884	22.407693
97.003166	3387.677662	22.412711
96.976867	3409.391425	22.417728
97.186513	3415.991961	22.422746
97.280413	3414.458760	22.427763
97.635468	3411.342051	22.432781
98.108390	3392.209755	22.437799
98.140192	3394.859705	22.442816
98.424635	3382.965671	22.447834
98.455322	3386.074421	22.452851
98.309142	3382.520031	22.457869
98.589788	3383.767795	22.462887
98.527998	3391.519228	22.467904
98.889307	3370.310665	22.472922
98.637668	3356.581905	22.477939
98.627069	3355.740332	22.482957
98.673985	3352.734136	22.487975
98.581898	3354.662016	22.492992
99.088344	3366.025625	22.498010
98.926223	3374.306739	22.503027
98.867477	3379.908522	22.508045
98.874738	3384.027148	22.513063
98.825321	3395.198590	22.518080
99.111032	3386.312549	22.523098
98.919779	3385.774329	22.528115
99.020255	3386.595350	22.533133
99.376034	3400.863772	22.538151
99.340997	3416.110211	22.543168
99.765599	3408.619574	22.548186
99.627031	3416.929210	22.553203
99.711239	3407.915598	22.558221
99.759387	3422.748367	22.563239
99.759187	3434.476814	22.568256
99.655952	3447.137382	22.573274
99.806835	3449.176778	22.578291
99.998722	3446.973442	22.583309
100.392473	3454.207794	22.588327
100.189939	3471.991253	22.593344
100.715829	3472.376275	22.598362
100.911562	3469.275522	22.603379
100.873003	3473.847521	22.608397
101.063770	3479.503163	22.613415
100.846099	3468.491536	22.618432
100.957250	3465.457767	22.623450
101.276009	3481.632757	22.628467
101.087634	3501.361783	22.633485
101.400084	3497.539129	22.638503
101.365615	3502.072725	22.643520
101.601204	3496.469511	22.648538
101.688589	3504.813962	22.653555
101.332166	3505.741681	22.658573
101.833808	3512.083293	22.663591
101.772937	3517.207959	22.668608
102.291223	3525.430995	22.673626
101.945189	3520.468838	22.678643
102.068137	3520.498826	22.683661
102.427858	3515.258918	22.688679
102.258633	3542.918505	22.693696
102.892147	3552.678428	22.698714
102.562823	3550.723399	22.703731
102.647300	3554.851786	22.708749
103.131418	3545.878941	22.713767
103.098797	3546.379781	22.718784
103.234770	3546.383306	22.723802
103.106425	3545.355965	22.728819
103.335941	3552.655104	22.733837
103.442190	3565.673341	22.738855
103.251951	3574.674136	22.743872
103.321790	3572.656234	22.748890
103.710952	3579.468150	22.753907
103.770620	3580.543491	22.758925
104.261411	3568.854762	22.763943
104.366365	3580.140967	22.768960
104.550223	3561.784583	22.773978
104.605204	3560.110467	22.778995
104.519452	3564.750594	22.784013
104.865309	3554.661479	22.789031
104.762416	3555.713183	22.794048
105.024172	3554.811643	22.799066
104.797546	3564.748868	22.804083
105.095721	3571.481677	22.809101
105.433975	3587.695370	22.814119
105.244251	3586.058703	22.819136
105.298921	3578.696204	22.824154
105.171248	3585.271157	22.829171
105.367592	3589.874958	22.834189
105.788995	3589.722042	22.839207
105.674098	3586.791165	22.844224
105.694855	3588.936294	22.849242
105.841431	3586.427068	22.854259
105.542199	3588.133131	22.859277
105.538398	3580.683982	22.864295
105.500220	3589.603896	22.869312
105.951712	3593.129386	22.874330
106.242361	3613.731684	22.879347
106.064828	3617.023944	22.884365
106.009981	3605.629097	22.889383
105.756951	3632.168620	22.894400
106.002575	3638.470876	22.899418
106.534063	3642.725455	22.904435
106.557501	3659.284437	22.909453
106.892436	3664.520674	22.914471
106.672630	3680.131191	22.919488
106.782258	3679.411241	22.924506
107.137062	3684.103082	22.929523
106.926463	3701.775610	22.934541
107.581088	3700.521125	22.939559
107.640593	3712.931764	22.944576
107.536218	3710.067625	22.949594
107.853591	3703.734626	22.954611
107.530956	3715.026190	22.959629
108.072345	3716.606862	22.964647
107.842384	3729.127399	22.969664
108.175085	3730.361387	22.974682
108.160984	3734.824938	22.979699
107.826954	3739.979869	22.984717
108.611498	3756.197311	22.989735
108.691173	3763.913006	22.994752
109.014395	3742.564447	22.999770
109.191419	3738.267720	23.004787
109.523826	3735.025541	23.009805
109.411791	3738.839179	23.014823
109.459632	3743.058424	23.019840
109.778206	3745.997044	23.024858
109.990120	3730.715834	23.029875
109.642998	3738.457098	23.034893
109.765310	3734.534904	23.039911
109.781493	3733.758266	23.044928
109.887581	3731.016321	23.049946
109.860376	3738.089023	23.054963
110.012331	3752.070114	23.059981
110.453752	3752.401749	23.064999
110.533650	3764.707698	23.070016
110.619124	3762.408004	23.075034
110.634160	3764.601272	23.080051
110.305718	3766.207384	23.085069
110.860294	3761.372925	23.090087
110.457009	3761.829042	23.095104
110.697652	3764.604664	23.100122
110.871935	3785.404338	23.105139
110.912692	3795.430453	23.110157
111.152375	3789.809170	23.115175
110.664737	3803.522567	23.120192
110.924566	3808.021910	23.125210
111.430358	3819.217629	23.130227
111.227994	3834.255967	23.135245
111.563249	3827.939731	23.140263
111.316468	3838.836963	23.145280
111.595241	3857.746189	23.150298
111.630128	3854.496363	23.155315
111.743387	3871.683983	23.160333
112.051456	3867.144475	23.165351
112.047747	3897.740213	23.170368
111.857805	3886.565725	23.175386
112.613751	3896.882213	23.180403
112.921839	3925.574058	23.185421
113.218766	3916.982493	23.190439
113.080764	3925.646335	23.195456
113.143287	3923.634272	23.200474
113.435895	3914.196131	23.205491
113.364145	3921.016416	23.210509
113.765596	3921.571557	23.215527
113.583032	3923.849070	23.220544
113.483587	3917.203267	23.225562
114.232045	3915.475162	23.230579
113.880096	3916.964675	23.235597
113.716883	3914.556718	23.240615
113.817166	3931.700063	23.245632
113.937515	3940.613003	23.250650
113.887898	3940.995416	23.255667
114.027477	3951.563642	23.260685
114.351145	3967.740748	23.265703
114.388833	3979.955272	23.270720
114.538660	3977.461983	23.275738
114.671618	3973.429464	23.280755
114.567827	4000.465067	23.285773
115.452289	4000.845635	23.290791
115.457194	4006.071691	23.295808
115.353104	3996.607077	23.300826
115.685269	3996.219797	23.305843
115.563633	4003.487051	23.310861
115.562250	4004.690164	23.315879
115.429888	4010.964750	23.320896
115.818898	4031.610952	23.325914
116.324975	4036.244170	23.330931
116.076147	4032.985267	23.335949
116.012139	4039.159280	23.340967
116.177793	4033.626807	23.345984
116.578193	4050.567451	23.351002
116.663664	4049.510696	23.356019
116.674546	4066.619680	23.361037
116.826525	4058.405950	23.366055
116.594676	4058.982634	23.371072
116.943979	4063.426880	23.376090
116.847418	4063.492663	23.381107
116.959562	4081.145644	23.386125
117.331739	4086.656161	23.391143
117.470576	4092.196023	23.396160
117.075275	4087.914942	23.401178
117.367440	4095.174468	23.406195
117.444221	4113.442820	23.411213
117.655832	4118.345660	23.416231
117.656374	4115.401773	23.421248
117.933687	4126.689233	23.426266
118.583647	4136.281721	23.431283
118.511054	4154.228583	23.436301
118.909590	4153.065253	23.441319
118.965235	4151.624615	23.446336
119.027804	4149.548004	23.451354
119.121779	4141.765151	23.456371
119.140185	4152.403194	23.461389
119.307345	4148.292011	23.466407
119.360126	4145.031400	23.471424
119.254951	4147.059807	23.476442
119.353738	4144.305577	23.481459
119.511150	4145.109695	23.486477
119.469120	4146.310648	23.491495
119.635906	4160.011270	23.496512
119.878519	4170.914093	23.501530
120.051824	4166.115133	23.506547
120.237741	4171.769457	23.511565
120.125060	4170.389489	23.516583
120.029682	4184.672406	23.521600
120.371160	4193.595865	23.526618
120.744725	4195.785519	23.531635
121.006109	4193.032099	23.536653
121.275440	4184.399152	23.541671
121.195770	4184.736015	23.546688
121.104331	4184.426510	23.551706
121.493206	4180.667020	23.556723
121.146479	4187.765717	23.561741
121.593648	4194.225669	23.566759
121.807148	4209.827436	23.571776
121.517777	4210.087602	23.576794
122.127267	4208.347800	23.581811
121.865658	4214.584080	23.586829
121.947094	4211.022297	23.591847
122.223159	4220.519485	23.596864
122.176299	4227.806393	23.601882
122.164744	4228.408529	23.606899
122.262685	4236.794195	23.611917
122.629482	4239.391663	23.616935
122.565597	4239.214650	23.621952
122.512897	4251.653865	23.626970
122.929384	4265.192039	23.631987
122.931035	4269.189868	23.637005
123.020474	4267.053886	23.642023
123.229560	4283.186676	23.647040
123.371451	4295.196034	23.652058
123.845952	4287.356356	23.657075
123.720808	4299.926743	23.662093
123.925973	4296.135157	23.667111
124.089547	4287.610274	23.672128
124.112547	4285.130078	23.677146
124.403972	4286.144126	23.682163
124.309293	4283.349918	23.687181
124.506374	4286.882323	23.692199
124.826713	4297.056152	23.697216
124.888240	4316.270455	23.702234
125.218334	4312.898715	23.707251
125.148087	4306.345632	23.712269
125.358004	4299.051635	23.717287
125.275820	4299.499042	23.722304
125.429909	4310.275264	23.727322
125.685014	4301.036390	23.732339
125.640969	4302.823777	23.737357
125.621828	4302.602653	23.742375
125.813591	4298.179901	23.747392
125.319952	4296.268278	23.752410
125.704078	4314.505176	23.757427
125.526722	4337.199465	23.762445
125.582261	4335.924037	23.767463
126.169880	4358.726877	23.772480
126.268496	4366.093714	23.777498
126.818405	4362.273097	23.782515
126.846051	4367.535778	23.787533
126.815071	4379.092089	23.792551
126.954150	4386.745929	23.797568
126.735928	4401.139905	23.802586
127.071852	4393.868251	23.807603
127.121655	4400.051801	23.812621
127.665460	4416.571922	23.817639
127.834530	4423.132182	23.822656
127.438707	4428.216958	23.827674
127.914662	4426.819408	23.832691
127.708582	4425.278872	23.837709
127.721833	4443.729269	23.842727
127.987088	4448.681883	23.847744
128.057239	4453.601888	23.852762
128.747045	4454.635026	23.857779
128.990245	4473.298181	23.862797
128.669596	4481.505281	23.867815
129.156756	4472.991627	23.872832
128.913513	4482.176865	23.877850
129.256527	4470.330049	23.882867
129.144431	4479.137987	23.887885
129.234987	4469.155836	23.892903
129.855671	4485.001357	23.897920
130.086464	4489.205015	23.902938
130.426362	4482.085309	23.907955
130.729989	4483.109227	23.912973
130.588473	4472.434004	23.917991
130.568912	4453.136565	23.923008
130.446523	4468.914898	23.928026
130.837066	4476.221077	23.933043
130.810910	4473.076043	23.938061
131.028162	4476.856241	23.943079
131.195943	4477.985214	23.948096
131.141418	4485.793494	23.953114
131.351237	4476.199841	23.958131
131.335431	4482.011543	23.963149
130.910800	4478.990627	23.968167
131.802365	4486.020236	23.973184
131.029698	4476.915251	23.978202
131.247495	4473.710860	23.983219
131.379587	4499.348736	23.988237
131.420733	4508.796248	23.993255
131.610756	4514.414648	23.998272
131.719918	4536.607254	24.003290
131.992687	4542.505918	24.008307
132.013811	4549.030035	24.013325
132.344823	4554.148426	24.018343
132.684978	4560.196842	24.023360
132.418102	4575.614408	24.028378
132.507090	4566.779488	24.033395
132.783396	4590.728242	24.038413
132.998671	4597.509362	24.043431
133.242121	4608.414738	24.048448
132.983950	4609.408670	24.053466
133.278799	4617.582206	24.058483
133.511851	4628.228061	24.063501
133.480546	4642.739583	24.068519
133.682322	4651.495998	24.073536
133.871214	4663.761716	24.078554
133.751512	4655.753832	24.083571
134.059695	4674.525677	24.088589
134.003979	4691.528783	24.093607
134.715588	4684.212814	24.098624
134.587867	4699.441531	24.103642
134.867292	4716.207914	24.108659
134.946987	4731.310754	24.113677
134.873992	4732.609527	24.118695
135.402247	4735.780831	24.123712
135.326909	4749.250763	24.128730
135.627862	4750.649613	24.133747
136.046352	4748.896155	24.138765
136.121628	4750.984770	24.143783
136.380686	4745.641689	24.148800
136.167328	4753.876673	24.153818
136.309134	4758.645314	24.158835
136.625969	4772.940167	24.163853
136.720358	4781.796392	24.168871
136.909479	4775.241077	24.173888
136.978101	4782.484668	24.178906
137.124682	4778.787270	24.183923
137.068878	4770.051630	24.188941
137.259824	4773.052512	24.193959
137.511025	4782.081202	24.198976
137.515312	4803.029794	24.203994
137.846759	4803.814065	24.209011
137.931393	4796.652306	24.214029
137.547839	4800.349806	24.219047
137.944021	4789.288077	24.224064
137.941651	4811.699500	24.229082
137.984786	4821.833718	24.234099
138.472192	4817.926973	24.239117
138.386049	4836.678511	24.244135
139.032847	4829.040017	24.249152
138.678378	4833.015326	24.254170
139.015360	4840.201204	24.259187
139.410269	4850.786794	24.264205
139.302226	4858.369356	24.269223
139.486078	4861.033875	24.274240
139.494912	4851.686023	24.279258
139.816993	4848.190350	24.284275
140.170618	4840.018772	24.289293
140.110002	4848.427711	24.294311
140.683079	4835.462938	24.299328
140.232345	4846.074015	24.304346
139.997899	4857.914903	24.309363
140.479479	4867.773898	24.314381
140.480094	4864.718919	24.319399
140.662812	4870.337834	24.324416
140.902004	4877.860315	24.329434
140.799527	4899.184036	24.334451
140.764788	4896.720026	24.339469
140.929540	4903.689509	24.344487
141.412061	4909.663444	24.349504
141.272871	4929.941188	24.354522
140.968465	4941.827915	24.359539
141.441597	4950.940904	24.364557
141.517575	4965.522965	24.369575
141.720765	4963.533174	24.374592
141.817548	4987.246853	24.379610
141.957279	4998.864543	24.384627
142.263333	4998.717432	24.389645
142.350734	5029.254569	24.394663
142.802630	5015.111531	24.399680
143.190564	5017.802542	24.404698
143.155856	5020.218712	24.409715
143.825897	5022.982752	24.414733
143.818024	5045.109030	24.419751
144.090795	5035.026634	24.424768
144.148701	5056.048070	24.429786
144.073035	5037.977491	24.434803
144.341627	5041.620623	24.439821
144.134249	5039.542876	24.444839
144.675154	5034.692099	24.449856
144.457095	5040.174366	24.454874
144.424486	5030.785804	24.459891
144.654135	5036.760778	24.464909
144.559580	5062.094324	24.469927
144.778477	5058.488389	24.474944
144.840631	5064.450745	24.479962
145.091399	5063.069382	24.484979
145.207449	5085.932029	24.489997
145.435019	5095.060663	24.495015
145.704064	5101.718577	24.500032
145.499934	5093.483958	24.505050
145.806883	5110.472200	24.510067
146.039869	5117.557571	24.515085
146.028236	5130.595991	24.520103
146.261619	5129.685513	24.525120
146.335661	5131.189820	24.530138
146.428673	5150.767604	24.535155
146.886756	5155.607102	24.540173
146.602518	5168.951014	24.545191
147.121157	5163.353968	24.550208
147.219417	5162.660937	24.555226
147.514178	5175.946360	24.560243
148.421926	5161.091647	24.565261
148.351949	5162.733002	24.570279
148.383838	5165.271538	24.575296
148.641101	5161.452544	24.580314
148.389963	5135.728720	24.585331
148.644060	5146.562777	24.590349
148.623103	5161.406743	24.595367
148.876167	5149.166191	24.600384
148.936311	5160.640135	24.605402
149.122621	5148.513294	24.610419
149.387777	5149.986341	24.615437
149.359074	5159.317953	24.620455
149.357024	5144.284187	24.625472
149.372720	5151.644185	24.630490
149.361156	5171.970357	24.635507
149.643132	5173.832529	24.640525
149.649893	5187.339334	24.645543
149.904641	5189.798280	24.650560
149.980689	5200.584452	24.655578
149.734630	5210.283554	24.660595
149.870206	5225.745407	24.665613
150.321527	5244.544721	24.670631
150.973276	5249.204671	24.675648
150.998797	5260.160230	24.680666
150.993965	5253.037694	24.685683
151.304716	5261.821155	24.690701
151.279862	5281.338444	24.695719
151.525225	5282.005869	24.700736
151.572260	5285.006201	24.705754
151.614353	5297.958311	24.710771
152.084575	5302.914725	24.715789
152.211241	5312.166585	24.720807
152.609726	5307.537483	24.725824
152.749714	5307.695366	24.730842
153.146607	5301.784094	24.735859
152.877638	5300.598880	24.740877
153.004165	5297.740881	24.745895
153.092170	5296.575848	24.750912
153.043337	5316.693375	24.755930
153.471677	5322.277231	24.760947
153.699072	5318.139600	24.765965
153.849154	5322.719068	24.770983
153.622799	5318.569606	24.776000
153.868783	5321.997693	24.781018
153.923050	5338.683461	24.786035
154.474619	5338.680517	24.791053
154.580991	5349.115786	24.796071
154.518282	5350.829958	24.801088
154.663938	5355.954585	24.806106
154.840444	5350.070569	24.811123
154.878649	5349.202216	24.816141
154.901820	5371.112392	24.821159
154.908127	5371.753425	24.826176
155.165736	5378.517142	24.831194
155.065949	5396.982822	24.836211
155.328310	5401.475962	24.841229
155.476660	5411.146135	24.846247
155.473242	5420.362945	24.851264
155.826316	5429.107500	24.856282
155.792181	5434.346582	24.861299
156.307744	5461.803007	24.866317
156.342339	5475.031052	24.871335
156.164626	5469.869867	24.876352
156.660168	5488.236011	24.881370
157.162382	5498.959168	24.886387
156.903078	5501.599269	24.891405
157.182184	5512.763200	24.896423
157.296260	5532.474243	24.901440
157.622034	5530.840125	24.906458
157.347031	5536.319065	24.911475
157.823087	5554.644339	24.916493
157.715295	5561.825177	24.921511
157.984624	5574.251919	24.926528
158.217795	5583.552269	24.931546
158.546106	5595.327613	24.936563
158.539037	5605.147793	24.941581
158.628274	5623.066697	24.946599
158.800078	5625.545237	24.951616
159.320252	5638.642500	24.956634
159.452134	5660.949617	24.961651
159.495185	5668.757910	24.966669
159.681907	5667.119199	24.971687
159.942181	5668.627697	24.976704
159.799861	5682.530087	24.981722
160.035713	5698.864724	24.986739
160.477593	5679.039705	24.991757
160.799411	5689.572254	24.996775
161.602513	5692.939918	25.001792
161.815786	5697.898887	25.006810
161.997356	5676.961950	25.011827
161.828182	5668.708846	25.016845
161.751559	5673.016940	25.021863
161.596359	5665.771053	25.026880
161.757066	5670.283632	25.031898
161.900028	5688.128747	25.036915
162.434281	5683.608489	25.041933
162.412761	5693.144642	25.046951
162.454381	5687.104974	25.051968
162.591069	5688.580466	25.056986
162.532193	5691.874717	25.062003
162.777573	5687.618459	25.067021
162.712519	5705.202505	25.072039
162.928810	5715.447413	25.077056
162.993352	5721.501708	25.082074
163.017985	5726.414446	25.087091
163.396435	5743.565111	25.092109
163.210595	5749.469726	25.097127
162.956759	5764.755051	25.102144
163.716928	5770.351473	25.107162
163.345937	5786.938754	25.112179
164.059169	5809.438216	25.117197
163.895560	5814.928606	25.122215
163.848478	5832.389558	25.127232
164.744998	5845.804657	25.132250
164.523762	5854.818069	25.137267
164.753995	5866.123817	25.142285
165.017546	5884.861834	25.147303
165.131144	5900.380612	25.152320
165.347550	5900.601063	25.157338
165.554636	5921.104259	25.162355
165.747386	5918.969665	25.167373
165.867173	5939.897515	25.172391
166.182128	5947.295165	25.177408
166.476422	5950.264075	25.182426
166.401460	5970.534572	25.187443
166.963328	5977.186320	25.192461
166.795136	5977.292641	25.197479
167.123209	5983.301088	25.202496
167.628665	6002.729260	25.207514
167.470335	6006.375403	25.212531
167.582926	6004.939670	25.217549
167.896086	6005.205280	25.222567
167.813875	6013.045529	25.227584
168.124841	6021.565046	25.232602
168.145427	6033.843005	25.237619
168.656841	6030.695324	25.242637
168.676281	6052.102760	25.247655
168.630037	6062.130910	25.252672
168.889385	6060.140678	25.257690
169.071747	6068.823139	25.262707
169.148902	6090.274143	25.267725
169.129177	6105.715257	25.272743
169.285563	6106.931151	25.277760
169.669894	6122.592680	25.282778
169.640369	6144.254326	25.287795
169.888900	6143.870111	25.292813
169.907840	6152.481115	25.297831
170.012321	6167.033849	25.302848
170.308477	6165.960663	25.307866
170.437478	6192.651572	25.312883
170.821293	6196.777821	25.317901
170.776265	6206.195309	25.322919
170.900245	6224.475268	25.327936
171.520564	6216.530295	25.332954
171.389751	6226.535848	25.337971
171.689672	6241.945018	25.342989
171.927438	6260.341424	25.348007
171.902381	6259.214015	25.353024
172.450520	6253.432471	25.358042
172.182226	6265.951027	25.363059
172.693303	6275.660708	25.368077
173.110820	6291.579920	25.373095
173.026202	6288.275442	25.378112
173.525188	6278.108142	25.383130
173.490093	6295.887174	25.388147
173.848101	6289.836942	25.393165
173.862163	6292.284883	25.398183
174.055638	6305.090206	25.403200
173.998730	6317.716727	25.408218
175.038842	6298.519373	25.413235
175.759501	6279.057466	25.418253
175.970146	6263.386738	25.423271
175.720392	6256.429449	25.428288
176.189218	6232.824261	25.433306
176.126538	6240.640273	25.438323
175.781145	6229.481709	25.443341
175.788090	6236.553307	25.448359
175.701826	6227.114317	25.453376
176.111694	6232.454410	25.458394
175.892743	6226.887244	25.463411
176.090603	6239.213429	25.468429
176.278846	6252.556149	25.473447
176.333957	6266.748624	25.478464
176.680453	6254.737755	25.483482
176.786860	6273.774347	25.488499
176.750315	6299.909603	25.493517
177.185971	6294.526012	25.498535
177.132923	6297.607814	25.503552
177.146516	6324.181243	25.508570
176.959191	6334.772617	25.513587
177.666607	6329.228446	25.518605
177.938874	6343.428072	25.523623
178.179538	6342.662713	25.528640
178.236356	6338.249075	25.533658
178.370089	6365.177161	25.538675
178.497356	6378.488801	25.543693
178.931822	6377.381746	25.548711
179.040664	6391.499681	25.553728
179.064276	6405.358191	25.558746
179.131796	6411.841898	25.563763
179.105720	6423.347878	25.568781
179.289507	6437.287887	25.573799
179.535266	6455.917736	25.578816
180.019880	6456.472323	25.583834
180.096633	6469.917205	25.588851
180.344351	6484.349847	25.593869
180.838210	6500.477425	25.598887
180.887940	6501.875593	25.603904
180.858170	6501.725370	25.608922
180.776665	6513.414147	25.613939
181.099085	6530.504632	25.618957
181.200806	6530.767773	25.623975
181.368201	6542.436557	25.628992
181.896970	6554.970684	25.634010
181.696259	6567.348889	25.639027
181.942758	6572.542839	25.644045
182.526231	6587.228911	25.649063
182.641980	6595.815294	25.654080
182.685768	6598.823492	25.659098
182.616449	6601.905590	25.664115
182.800373	6618.110253	25.669133
182.895821	6625.415777	25.674151
182.581749	6641.948508	25.679168
183.550118	6651.448617	25.684186
183.875635	6666.322248	25.689204
183.655818	6689.159090	25.694221
184.082166	6684.357531	25.699239
184.350383	6701.016226	25.704256
184.921016	6708.061119	25.709274
184.846879	6718.441941	25.714292
184.974223	6714.393843	25.719309
185.227143	6714.797330	25.724327
185.061888	6737.531125	25.729344
185.662945	6746.546941	25.734362
185.687551	6742.881097	25.739380
185.552653	6754.126141	25.744397
185.901122	6758.879791	25.749415
186.344515	6767.700050	25.754432
186.434551	6777.046006	25.759450
186.600162	6795.126468	25.764468
186.852809	6807.039952	25.769485
186.995294	6809.630379	25.774503
186.596490	6825.128746	25.779520
187.255469	6821.571823	25.784538
187.502865	6831.582787	25.789556
187.317097	6852.119221	25.794573
187.910369	6850.762563	25.799591
188.066235	6861.426272	25.804608
188.282276	6875.813987	25.809626
188.320850	6889.189798	25.814644
188.720719	6892.486708	25.819661
189.143345	6887.186818	25.824679
189.463337	6914.150722	25.829696
189.391435	6912.515346	25.834714
189.766776	6913.542176	25.839732
189.939691	6923.027659	25.844749
189.766452	6917.179906	25.849767
189.984182	6935.174330	25.854784
189.883130	6934.569653	25.859802
190.152903	6943.959446	25.864820
190.487477	6963.623071	25.869837
190.797434	6973.753200	25.874855
190.375150	6990.301995	25.879872
190.755872	6986.877529	25.884890
191.209561	7002.307039	25.889908
191.070503	7017.381779	25.894925
191.511068	7020.654132	25.899943
191.602659	7039.974974	25.904960
191.783477	7043.651488	25.909978
191.836291	7050.242470	25.914996
191.997272	7066.721960	25.920013
192.763684	7064.346238	25.925031
192.500190	7083.088757	25.930048
192.781007	7088.079916	25.935066
193.191384	7101.357294	25.940084
193.236539	7107.229547	25.945101
193.749236	7112.145187	25.950119
193.582727	7134.299083	25.955136
194.003813	7128.890767	25.960154
194.032023	7137.020090	25.965172
194.386258	7151.559149	25.970189
194.649866	7161.677911	25.975207
194.948605	7164.171884	25.980224
195.329282	7152.208354	25.985242
195.434753	7148.038514	25.990260
195.722384	7166.130660	25.995277
195.977534	7164.418718	26.000295
195.984161	7176.903644	26.005312
196.307434	7171.809130	26.010330
196.485848	7172.975178	26.015348
196.369771	7182.801977	26.020365
196.544902	7171.688755	26.025383
196.759693	7187.991411	26.030400
196.771423	7206.301492	26.035418
196.924821	7209.629117	26.040436
197.001986	7216.304420	26.045453
197.197090	7226.693815	26.050471
197.056716	7247.450958	26.055488
197.513806	7250.366639	26.060506
197.762178	7265.091077	26.065524
197.669668	7283.579968	26.070541
198.218906	7289.851126	26.075559
198.171046	7302.314156	26.080576
198.276141	7325.833530	26.085594
198.784424	7326.372582	26.090612
198.766704	7353.561091	26.095629
199.143496	7353.663935	26.100647
199.306285	7368.650773	26.105664
200.025870	7383.057055	26.110682
200.491716	7372.721191	26.115700
200.048174	7391.851617	26.120717
200.634180	7389.264615	26.125735
200.705754	7408.111493	26.130752
201.140460	7417.845123	26.135770
201.108926	7412.965259	26.140788
201.082437	7420.161568	26.145805
201.424308	7431.277599	26.150823
201.105782	7445.866767	26.155840
201.376065	7448.358243	26.160858
201.982225	7457.150998	26.165876
201.861209	7474.455696	26.170893
202.118924	7478.735397	26.175911
201.961075	7496.381204	26.180928
202.222792	7514.318955	26.185946
202.478710	7522.556183	26.190964
202.463471	7548.451805	26.195981
202.852241	7546.444681	26.200999
203.038837	7572.203509	26.206016
203.114093	7590.403998	26.211034
203.432089	7605.655902	26.216052
203.446815	7620.662665	26.221069
204.312227	7636.018143	26.226087
204.627143	7642.381894	26.231104
204.642414	7657.795822	26.236122
204.743363	7664.185828	26.241140
204.675701	7686.927146	26.246157
205.321130	7695.409649	26.251175
205.538898	7713.387696	26.256192
205.855300	7715.040121	26.261210
205.964170	7715.593296	26.266228
206.329148	7732.394312	26.271245
206.350176	7734.153635	26.276263
206.746734	7745.015672	26.281280
206.643077	7750.802919	26.286298
207.081216	7760.295832	26.291316
206.997566	7785.073576	26.296333
207.758472	7767.753523	26.301351
207.582306	7783.560861	26.306368
207.833147	7790.876413	26.311386
207.954840	7789.260435	26.316404
208.234546	7809.544164	26.321421
208.509066	7821.660356	26.326439
208.649957	7821.772882	26.331456
208.649062	7838.261722	26.336474
208.805423	7848.213523	26.341492
208.941104	7867.313584	26.346509
209.324515	7883.315883	26.351527
210.121470	7873.643361	26.356544
210.643700	7872.843270	26.361562
211.329504	7858.406880	26.366580
210.924192	7857.771982	26.371597
211.313142	7854.296437	26.376615
211.525682	7869.733823	26.381632
211.381283	7857.740527	26.386650
211.777316	7858.327795	26.391668
211.589957	7852.874587	26.396685
211.995048	7869.322735	26.401703
212.004270	7876.644981	26.406720
212.007564	7886.170319	26.411738
212.764300	7875.826686	26.416756
212.193375	7891.909932	26.421773
212.473899	7898.025501	26.426791
212.697007	7914.094704	26.431808
212.559965	7919.302670	26.436826
212.948266	7930.995162	26.441844
213.056924	7945.436837	26.446861
213.269553	7953.964099	26.451879
213.552730	7977.633949	26.456896
212.892703	7996.204756	26.461914
213.599062	8006.112650	26.466932
213.135763	8027.377191	26.471949
213.597140	8048.535260	26.476967
214.100123	8072.603409	26.481984
214.352824	8094.994065	26.487002
214.848141	8110.959488	26.492020
214.589093	8137.076382	26.497037
215.201566	8154.272794	26.502055
215.501154	8173.423838	26.507072
215.609692	8192.365751	26.512090
216.112040	8198.300892	26.517108
216.214973	8226.968863	26.522125
216.435806	8233.551681	26.527143
217.016067	8247.177181	26.532160
217.473632	8256.873882	26.537178
217.584711	8253.478353	26.542196
217.527135	8263.394897	26.547213
218.540465	8265.566992	26.552231
218.459029	8266.640387	26.557248
218.406082	8282.488018	26.562266
218.827060	8295.852912	26.567284
218.802073	8305.699368	26.572301
219.198681	8310.380139	26.577319
219.273874	8311.434468	26.582336
219.098479	8329.134021	26.587354
219.762247	8332.126747	26.592372
220.180220	8351.899704	26.597389
220.022352	8363.380580	26.602407
220.309943	8367.444094	26.607424
220.534624	8373.753690	26.612442
220.753441	8384.635484	26.617460
220.813671	8403.431521	26.622477
220.916550	8408.766661	26.627495
221.191198	8423.196104	26.632512
221.244351	8438.538301	26.637530
221.627733	8456.489660	26.642548
221.618331	8474.158985	26.647565
221.946440	8490.798725	26.652583
222.098001	8499.421024	26.657600
222.088398	8522.940893	26.662618
222.447685	8529.326282	26.667636
222.711823	8558.453939	26.672653
222.771998	8565.623996	26.677671
222.932338	8586.833182	26.682688
223.086467	8600.811423	26.687706
223.951224	8624.753930	26.692724
224.068146	8636.551230	26.697741
224.282035	8649.362005	26.702759
224.579241	8656.129176	26.707776
224.508929	8669.929608	26.712794
225.425832	8680.213206	26.717812
225.202538	8696.509052	26.722829
225.357178	8701.088448	26.727847
226.013645	8704.096189	26.732864
225.927897	8722.174597	26.737882
226.032225	8727.785837	26.742900
226.309019	8748.844480	26.747917
226.696737	8759.632729	26.752935
226.720552	8762.723243	26.757952
226.377191	8773.551721	26.762970
226.875948	8775.129554	26.767988
227.398249	8791.579707	26.773005
227.575561	8816.670497	26.778023
228.010607	8818.628359	26.783040
228.161099	8847.372564	26.788058
228.487574	8846.789753	26.793076
228.595169	8854.851480	26.798093
228.720097	8873.018067	26.803111
228.995038	8880.866621	26.808128
228.938921	8899.044395	26.813146
229.846087	8898.856918	26.818164
229.826091	8915.933120	26.823181
229.781206	8935.585869	26.828199
230.257120	8936.042015	26.833216
230.315838	8947.273574	26.838234
230.830930	8966.038722	26.843252
230.903067	8968.035573	26.848269
231.334348	8980.646321	26.853287
232.174875	8992.070026	26.858304
232.080990	9005.213871	26.863322
231.830064	8996.169251	26.868340
232.489986	9002.005623	26.873357
232.495650	9008.558950	26.878375
233.173917	9007.561196	26.883392
233.245862	9016.014304	26.888410
233.407288	9018.339255	26.893428
233.503630	9040.374971	26.898445
233.879911	9039.553241	26.903463
233.956429	9040.461429	26.908480
234.001356	9062.729265	26.913498
234.263161	9072.004418	26.918516
234.366781	9076.232027	26.923533
234.607999	9098.208531	26.928551
235.117531	9105.697937	26.933568
235.341748	9120.147505	26.938586
235.577091	9117.124274	26.943604
235.273993	9140.270087	26.948621
235.973822	9144.844942	26.953639
237.178604	9125.919566	26.958656
237.143411	9126.570131	26.963674
237.396435	9133.748277	26.968692
237.792145	9124.462378	26.973709
237.709112	9120.542003	26.978727
238.253810	9100.657912	26.983744
238.368528	9105.954033	26.988762
238.270430	9096.501341	26.993780
238.368959	9096.735531	26.998797
238.576216	9103.602632	27.003815
239.042231	9115.405254	27.008832
238.903540	9132.318836	27.013850
239.132190	9127.732969	27.018868
239.228236	9129.880669	27.023885
239.088151	9151.988081	27.028903
239.421808	9160.290553	27.033920
239.366695	9178.791950	27.038938
239.720907	9188.007193	27.043956
239.726684	9219.664541	27.048973
240.000140	9234.729651	27.053991
240.400174	9233.083314	27.059008
240.145467	9255.019095	27.064026
240.369101	9269.749457	27.069044
240.517798	9299.387243	27.074061
240.723687	9323.744801	27.079079
241.056706	9353.980136	27.084096
241.231391	9376.916357	27.089114
241.384266	9399.609766	27.094132
242.231338	9424.640052	27.099149
242.018207	9443.990542	27.104167
242.699075	9468.100657	27.109184
242.788602	9491.226126	27.114202
243.070212	9513.673712	27.119220
243.777716	9523.942491	27.124237
244.095676	9544.334622	27.129255
244.499709	9553.293460	27.134272
244.391885	9564.118793	27.139290
244.751055	9576.322469	27.144308
244.973980	9593.372913	27.149325
244.779787	9611.763224	27.154343
245.530076	9618.869807	27.159360
245.600863	9634.020356	27.164378
245.788164	9659.428121	27.169396
246.064882	9672.653159	27.174413
246.480285	9691.519319	27.179431
246.938883	9702.273342	27.184448
247.163739	9705.921855	27.189466
247.639821	9712.383181	27.194484
247.593354	9732.577102	27.199501
247.642840	9741.781060	27.204519
248.159661	9761.114751	27.209536
247.992637	9756.828658	27.214554
248.106978	9783.668010	27.219572
248.870831	9783.197240	27.224589
249.011621	9803.255159	27.229607
249.473664	9809.420886	27.234624
249.456676	9829.951403	27.239642
249.876738	9844.242167	27.244660
250.366524	9847.833134	27.249677
250.064503	9863.132276	27.254695
250.660275	9863.347810	27.259712
250.541686	9881.845628	27.264730
250.546131	9888.398352	27.269748
251.014779	9914.155199	27.274765
250.898772	9921.958411	27.279783
251.396611	9935.548231	27.284800
251.545394	9953.979905	27.289818
251.555996	9978.329517	27.294836
252.193153	9988.598815	27.299853
252.121435	10022.388836	27.304871
252.545035	10027.016269	27.309888
252.707258	10056.529237	27.314906
252.849213	10075.446161	27.319924
253.158331	10083.991525	27.324941
253.118005	10109.058568	27.329959
253.566407	10138.380280	27.334976
253.876080	10156.568155	27.339994
254.374492	10171.157219	27.345012
254.604610	10187.814467	27.350029
254.887831	10210.944397	27.355047
255.665436	10208.193785	27.360064
255.585765	10226.904613	27.365082
255.759235	10242.465184	27.370100
256.315306	10258.483035	27.375117
256.471012	10266.435538	27.380135
257.298401	10280.748751	27.385152
257.180102	10275.369432	27.390170
257.476321	10292.993352	27.395188
257.887850	10313.469988	27.400205
257.880169	10318.666815	27.405223
258.119288	10330.944549	27.410240
258.032204	10338.690634	27.415258
258.344525	10358.431927	27.420276
258.494464	10365.878161	27.425293
258.479227	10384.373498	27.430311
258.984366	10406.059172	27.435328
259.160322	10430.807364	27.440346
259.543175	10444.801623	27.445364
259.889691	10465.144802	27.450381
260.063418	10477.242617	27.455399
261.347705	10493.559402	27.460416
261.464280	10494.839073	27.465434
261.714677	10488.806691	27.470452
261.722828	10497.759158	27.475469
262.188158	10508.261229	27.480487
262.366903	10518.927049	27.485504
262.417908	10530.771762	27.490522
262.219222	10528.805177	27.495540
263.012937	10549.801259	27.500557
262.849705	10561.321257	27.505575
263.189145	10574.518202	27.510592
263.336062	10587.784807	27.515610
263.544609	10608.172211	27.520628
263.942815	10610.637146	27.525645
264.150707	10632.018722	27.530663
264.309788	10644.121760	27.535680
264.413590	10660.441561	27.540698
264.868488	10676.898238	27.545716
265.232868	10678.212011	27.550733
265.597622	10693.143219	27.555751
265.730461	10714.178768	27.560768
266.228935	10713.328035	27.565786
266.372265	10724.018928	27.570804
266.396450	10731.493260	27.575821
266.575927	10754.006988	27.580839
266.819734	10754.272747	27.585856
267.386878	10782.565426	27.590874
267.290612	10791.882195	27.595892
267.597852	10804.558330	27.600909
267.516440	10834.530960	27.605927
268.204091	10851.034940	27.610944
268.568888	10876.395211	27.615962
268.625686	10886.248417	27.620980
268.985210	10907.267776	27.625997
269.211772	10925.655181	27.631015
269.533438	10938.062513	27.636032
270.010851	10956.812353	27.641050
270.036202	10976.085659	27.646068
270.599522	10987.995260	27.651085
270.923563	11008.524960	27.656103
271.259482	11012.291071	27.661120
271.698997	11021.262449	27.666138
271.791867	11033.191000	27.671156
272.268987	11022.184220	27.676173
272.246694	11051.369053	27.681191
272.525750	11061.755600	27.686208
273.015871	11072.366273	27.691226
273.033471	11090.435763	27.696244
273.465091	11093.496774	27.701261
273.652042	11122.582473	27.706279
273.728088	11131.024112	27.711296
274.091432	11152.444807	27.716314
274.264356	11160.239788	27.721332
274.604652	11174.652953	27.726349
274.678909	11206.153806	27.731367
275.181378	11212.250313	27.736384
275.237536	11229.862436	27.741402
275.456285	11246.538407	27.746420
275.696333	11266.090918	27.751437
275.837182	11295.357061	27.756455
275.938195	11307.901797	27.761472
276.472058	11340.435120	27.766490
276.655287	11353.585827	27.771508
277.308505	11366.839116	27.776525
277.163653	11396.114002	27.781543
277.456649	11412.525863	27.786560
277.703938	11435.912708	27.791578
278.106430	11468.947568	27.796596
278.363730	11474.085235	27.801613
278.825335	11500.187907	27.806631
278.780100	11506.169558	27.811648
279.219870	11529.591587	27.816666
279.742454	11542.235787	27.821684
279.790519	11552.997155	27.826701
279.925185	11577.456285	27.831719
280.568925	11596.460810	27.836736
280.972690	11604.765467	27.841754
280.629516	11613.868063	27.846772
281.355339	11627.522446	27.851789
281.554134	11653.482700	27.856807
281.953627	11671.347968	27.861824
282.278158	11688.711428	27.866842
282.373796	11707.559067	27.871860
282.665695	11723.186111	27.876877
282.638850	11745.084448	27.881895
282.918831	11768.902454	27.886912
283.802338	11782.309289	27.891930
283.870226	11804.355148	27.896948
283.797203	11816.054556	27.901965
283.998433	11836.480594	27.906983
284.266269	11852.806623	27.912000
284.788928	11881.400862	27.917018
284.997428	11907.464689	27.922036
285.452712	11925.913665	27.927053
285.427074	11942.900912	27.932071
286.852281	11944.648831	27.937088
287.617284	11944.011564	27.942106
287.913196	11939.391504	27.947124
288.433407	11942.118020	27.952141
288.276723	11948.602274	27.957159
288.491293	11937.727994	27.962176
288.659956	11957.558623	27.967194
288.818764	11965.803941	27.972212
288.840456	11973.979223	27.977229
288.923967	11988.391986	27.982247
289.277601	12009.172370	27.987264
289.555109	12018.259703	27.992282
289.649785	12034.873476	27.997300
289.864803	12056.624890	28.002317
290.057498	12070.880023	28.007335
290.654290	12092.643246	28.012352
290.841408	12109.801024	28.017370
290.873598	12139.071552	28.022388
291.201195	12149.975728	28.027405
291.297985	12178.189160	28.032423
291.512817	12191.591767	28.037440
292.074598	12215.225447	28.042458
292.210908	12239.681642	28.047476
292.720562	12254.728455	28.052493
292.924150	12279.004757	28.057511
293.113218	12303.079151	28.062528
293.504327	12323.217596	28.067546
293.658397	12352.219782	28.072564
294.360777	12347.234717	28.077581
294.357897	12379.690726	28.082599
294.336932	12390.828921	28.087616
294.774159	12411.402306	28.092634
295.077124	12430.039507	28.097652
295.129301	12454.931561	28.102669
295.462470	12483.928277	28.107687
295.691553	12507.202785	28.112704
296.044678	12532.482875	28.117722
296.270448	12553.378448	28.122740
296.425959	12578.351543	28.127757
296.837864	12599.682615	28.132775
297.108673	12629.428876	28.137792
297.732377	12656.103768	28.142810
297.742552	12679.265349	28.147828
298.203181	12702.635785	28.152845
298.865572	12728.057985	28.157863
299.106820	12745.243766	28.162880
299.627187	12758.285082	28.167898
299.816273	12778.032842	28.172916
300.420439	12786.224639	28.177933
300.629470	12809.674504	28.182951
301.104433	12821.827721	28.187968
301.503744	12830.192703	28.192986
301.649933	12847.098074	28.198004
301.988702	12862.084174	28.203021
301.938226	12876.613397	28.208039
302.493518	12899.046691	28.213056
303.083280	12899.477169	28.218074
302.775111	12913.430268	28.223092
303.215785	12916.490708	28.228109
303.820509	12938.044619	28.233127
304.014568	12958.901526	28.238144
304.386354	12957.176759	28.243162
304.504997	12990.536664	28.248180
304.576158	12990.373238	28.253197
304.933606	13016.543139	28.258215
305.310441	13042.329005	28.263232
305.485588	13054.837193	28.268250
305.512297	13081.937323	28.273268
306.255542	13082.975837	28.278285
306.939618	13112.609939	28.283303
307.250436	13112.609140	28.288320
307.737719	13130.802884	28.293338
308.199923	13143.823694	28.298356
308.332039	13143.822941	28.303373
308.130554	13163.877775	28.308391
308.677575	13172.362374	28.313408
308.984578	13191.717378	28.318426
309.108880	13206.641770	28.323444
309.509597	13224.632163	28.328461
309.835065	13244.384767	28.333479
310.069624	13255.083961	28.338496
310.518248	13268.339753	28.343514
310.192060	13289.831357	28.348532
310.627186	13308.737171	28.353549
310.893985	13331.652398	28.358567
311.138131	13350.650007	28.363584
311.751393	13361.793008	28.368602
311.677811	13386.654378	28.373620
312.039062	13402.158939	28.378637
312.358342	13412.176024	28.383655
312.238200	13447.752941	28.388672
312.907337	13453.810516	28.393690
313.447711	13470.546101	28.398708
314.114303	13487.872350	28.403725
314.343072	13506.122213	28.408743
314.795140	13511.099055	28.413760
315.145516	13519.654651	28.418778
315.062788	13539.250711	28.423796
315.375501	13566.630144	28.428813
315.822420	13568.309867	28.433831
316.228127	13600.978178	28.438848
316.494563	13608.424364	28.443866
316.799149	13627.151924	28.448884
316.799704	13655.024758	28.453901
317.130447	13668.047390	28.458919
317.632130	13694.704097	28.463936
317.902652	13712.000939	28.468954
317.804443	13748.265338	28.473972
318.324570	13757.466778	28.478989
318.676522	13771.668379	28.484007
318.598562	13805.009147	28.489024
319.075690	13838.037552	28.494042
319.531332	13865.380471	28.499060
319.929582	13890.859609	28.504077
320.922606	13892.921016	28.509095
321.278640	13907.116706	28.514112
321.592180	13913.527826	28.519130
321.952543	13937.822421	28.524148
322.282133	13946.442285	28.529165
322.619439	13967.431246	28.534183
322.509207	13978.729181	28.539200
322.963104	13992.078837	28.544218
323.617922	14004.493837	28.549236
323.517288	14022.838639	28.554253
323.788104	14042.794152	28.559271
323.994085	14063.522449	28.564288
324.499298	14070.684207	28.569306
324.952661	14088.555248	28.574324
325.917698	14083.112023	28.579341
326.735867	14092.942291	28.584359
326.875289	14110.892424	28.589376
326.858625	14102.555068	28.594394
326.814896	14110.549150	28.599412
327.234444	14115.513271	28.604429
327.150155	14137.464243	28.609447
327.271871	14154.485174	28.614464
328.118281	14164.101487	28.619482
328.272978	14187.286895	28.624500
328.631158	14206.280678	28.629517
328.714782	14219.330474	28.634535
328.528702	14220.934923	28.639552
329.254648	14240.361561	28.644570
329.419776	14263.164893	28.649588
329.389825	14286.062231	28.654605
329.966832	14310.936243	28.659623
329.807028	14332.562987	28.664640
330.082641	14358.224819	28.669658
330.469534	14386.773179	28.674676
330.718555	14417.566338	28.679693
331.318298	14446.247877	28.684711
331.413771	14473.424826	28.689728
331.576253	14498.393650	28.694746
331.929806	14524.412063	28.699764
332.390156	14560.731060	28.704781
332.927914	14588.956893	28.709799
332.811079	14617.648848	28.714816
333.522730	14654.452421	28.719834
333.925382	14682.582954	28.724852
334.066878	14711.592505	28.729869
334.750875	14728.616566	28.734887
334.836824	14767.144932	28.739904
335.235788	14786.064246	28.744922
335.479038	14816.363249	28.749940
336.016635	14854.106002	28.754957
336.653944	14872.174586	28.759975
336.754008	14901.657651	28.764992
337.413562	14917.490750	28.770010
337.426534	14950.615018	28.775028
337.760716	14976.397464	28.780045
338.295472	14991.315156	28.785063
338.540992	15023.118480	28.790080
338.843393	15047.088597	28.795098
339.043484	15066.292765	28.800116
339.506984	15105.898727	28.805133
340.265088	15125.431093	28.810151
340.519174	15144.879273	28.815168
341.225708	15149.402389	28.820186
341.719639	15174.992510	28.825204
341.617590	15196.696581	28.830221
342.165180	15213.168996	28.835239
342.211906	15232.785157	28.840256
342.997057	15251.462127	28.845274
343.302733	15268.635655	28.850292
343.307285	15289.841641	28.855309
343.858723	15305.430011	28.860327
344.135539	15327.466544	28.865344
344.875748	15350.710171	28.870362
344.757289	15367.044254	28.875380
344.735458	15391.824348	28.880397
345.601983	15397.665944	28.885415
345.755400	15429.611640	28.890432
345.845139	15451.306170	28.895450
346.401815	15471.313934	28.900468
346.559856	15493.787294	28.905485
347.061756	15514.121911	28.910503
347.184772	15537.222683	28.915520
347.948532	15540.850301	28.920538
348.474160	15552.389047	28.925556
348.659834	15563.229127	28.930573
348.990648	15571.949310	28.935591
349.199066	15595.835864	28.940608
349.641160	15603.767563	28.945626
350.042537	15625.269972	28.950644
350.394485	15636.524494	28.955661
350.594876	15657.152205	28.960679
350.616274	15668.876898	28.965696
351.019874	15688.867222	28.970714
351.520996	15722.129398	28.975732
351.506654	15738.648043	28.980749
352.142568	15752.775942	28.985767
352.472447	15783.904185	28.990784
352.815892	15794.478171	28.995802
353.231539	15822.756538	29.000820
353.461977	15842.289085	29.005837
353.870392	15866.719908	29.010855
354.121860	15892.026280	29.015872
354.753281	15909.898528	29.020890
355.009820	15931.226636	29.025908
355.324093	15958.246348	29.030925
355.853213	15970.708575	29.035943
356.355870	15989.333251	29.040960
357.018019	15997.066715	29.045978
357.766087	16009.130338	29.050996
357.747807	16023.595007	29.056013
358.381138	16036.746711	29.061031
357.979546	16045.211090	29.066048
358.677604	16061.483684	29.071066
359.085084	16069.462871	29.076084
358.764661	16098.088360	29.081101
359.699319	16111.282648	29.086119
359.896793	16132.650760	29.091136
360.025557	16153.851128	29.096154
360.381578	16186.123746	29.101172
360.590686	16208.994697	29.106189
360.896935	16220.427978	29.111207
360.999469	16270.265615	29.116224
361.272561	16287.512201	29.121242
362.115462	16318.205265	29.126260
362.058004	16349.454839	29.131277
362.366754	16370.677800	29.136295
362.811982	16413.418531	29.141312
363.577135	16437.903832	29.146330
363.796081	16456.366233	29.151348
363.827785	16487.651084	29.156365
364.489557	16502.182810	29.161383
364.857764	16538.842694	29.166400
365.176173	16562.102036	29.171418
366.087084	16592.835003	29.176436
366.071197	16616.629955	29.181453
366.416768	16622.805040	29.186471
366.754200	16650.567896	29.191488
367.044670	16671.121587	29.196506
367.428651	16677.104953	29.201524
367.775002	16715.423563	29.206541
368.116923	16730.220246	29.211559
368.332000	16752.087955	29.216576
368.778328	16771.598098	29.221594
369.700717	16793.000407	29.226612
369.827053	16818.513269	29.231629
370.313949	16838.269381	29.236647
370.667029	16863.320218	29.241664
370.798303	16883.819644	29.246682
371.362900	16894.458351	29.251700
371.416761	16924.881537	29.256717
372.158158	16941.008401	29.261735
372.466453	16965.426803	29.266752
372.812760	16985.938551	29.271770
373.321886	17004.736253	29.276788
373.221614	17031.119798	29.281805
373.555551	17050.630883	29.286823
373.512518	17101.978985	29.291840
374.112094	17123.197773	29.296858
374.726359	17145.611853	29.301876
375.024602	17172.312433	29.306893
375.618956	17189.727130	29.311911
375.933363	17219.708989	29.316928
376.131306	17263.855224	29.321946
377.042395	17283.330136	29.326964
377.203248	17310.242609	29.331981
377.299316	17319.916926	29.336999
377.424676	17356.793625	29.342016
378.159163	17384.678181	29.347034
379.055549	17396.828908	29.352052
379.154870	17428.113148	29.357069
379.688925	17444.352715	29.362087
380.194385	17474.918001	29.367104
380.240283	17495.813728	29.372122
380.990568	17507.808301	29.377140
381.111888	17540.321143	29.382157
381.449212	17563.371299	29.387175
381.685596	17582.613956	29.392192
382.323595	17604.298148	29.397210
382.559278	17625.840578	29.402228
382.574505	17657.416239	29.407245
383.301200	17671.230848	29.412263
383.724094	17699.789647	29.417280
383.862949	17731.657571	29.422298
384.700662	17745.752589	29.427316
384.652074	17774.660285	29.432333
385.477834	17797.615236	29.437351
385.745871	17825.070189	29.442368
386.027612	17842.253546	29.447386
386.355357	17866.258844	29.452404
386.613951	17909.875979	29.457421
387.021938	17928.946046	29.462439
387.555798	17944.912936	29.467456
387.726321	17970.156469	29.472474
388.097522	17989.424996	29.477492
388.176708	18016.667462	29.482509
388.648694	18044.310779	29.487527
388.772972	18072.354447	29.492544
389.250342	18096.163416	29.497562
389.670163	18123.853377	29.502580
389.922811	18163.529123	29.507597
390.035843	18190.716891	29.512615
390.757989	18225.683154	29.517632
391.025555	18265.594587	29.522650
391.333235	18302.124772	29.527668
391.748914	18332.398560	29.532685
392.343140	18359.382769	29.537703
392.734850	18411.783287	29.542720
393.061481	18435.036057	29.547738
393.802371	18465.698066	29.552756
393.789501	18504.053134	29.557773
394.244593	18530.786568	29.562791
395.237380	18559.363223	29.567808
395.318487	18599.134740	29.572826
395.945997	18626.939359	29.577844
396.054030	18658.625494	29.582861
396.754293	18677.423117	29.587879
397.114460	18701.724558	29.592896
397.254140	18740.390959	29.597914
397.953459	18757.544220	29.602932
397.790052	18803.031628	29.607949
398.417128	18827.192298	29.612967
398.978056	18854.682713	29.617984
398.904655	18896.493155	29.623002
399.803937	18916.201952	29.628020
400.042124	18953.749940	29.633037
400.572286	18979.724479	29.638055
400.851066	19011.319153	29.643072
401.554923	19041.993319	29.648090
402.130542	19063.909986	29.653108
402.836458	19103.819857	29.658125
403.121874	19118.578607	29.663143
403.264676	19142.035364	29.668160
403.792123	19169.673809	29.673178
404.026189	19197.430322	29.678196
404.636819	19223.718857	29.683213
405.671660	19224.498183	29.688231
406.359671	19246.509414	29.693248
406.591999	19260.240821	29.698266
407.071308	19264.547231	29.703284
406.931832	19294.129771	29.708301
407.245022	19293.979889	29.713319
407.804064	19308.337697	29.718336
408.066831	19341.381813	29.723354
408.509424	19359.970114	29.728372
408.778399	19397.190603	29.733389
408.966851	19399.017123	29.738407
409.387276	19426.509673	29.743424
409.531369	19453.575777	29.748442
410.170867	19465.792310	29.753460
410.264617	19497.535576	29.758477
410.299519	19526.471794	29.763495
410.975136	19553.100966	29.768512
411.261410	19585.722507	29.773530
411.360573	19617.291509	29.778548
411.787516	19650.351065	29.783565
412.079445	19684.901694	29.788583
412.309372	19723.891227	29.793600
412.626884	19768.444842	29.798618
413.703216	19800.896443	29.803636
414.213429	19839.281285	29.808653
414.219486	19881.679416	29.813671
414.967350	19908.749323	29.818688
414.971834	19947.975367	29.823706
415.628316	19986.351437	29.828724
415.664501	20030.013865	29.833741
416.433171	20056.438093	29.838759
416.926324	20095.379124	29.843776
416.950581	20139.214649	29.848794
417.744480	20166.313893	29.853812
417.780943	20212.642576	29.858829
417.823737	20254.318413	29.863847
418.938240	20300.608669	29.868864
419.061761	20346.515928	29.873882
419.639403	20385.858463	29.878900
420.183954	20421.019785	29.883917
420.645576	20465.165334	29.888935
421.513040	20493.804102	29.893952
422.273439	20529.727485	29.898970
422.789126	20547.525089	29.903988
423.336332	20576.214251	29.909005
423.462260	20610.458264	29.914023
424.090430	20626.362871	29.919040
424.083793	20663.922461	29.924058
424.628050	20683.507358	29.929076
424.891266	20719.630894	29.934093
425.236482	20750.038723	29.939111
425.782491	20771.916039	29.944128
425.494694	20821.249172	29.949146
426.116979	20863.988854	29.954164
426.742379	20898.925721	29.959181
426.901755	20942.377306	29.964199
427.511146	20966.388558	29.969216
428.252091	21009.000255	29.974234
428.836724	21042.134880	29.979252
428.974283	21077.904375	29.984269
429.382518	21108.533614	29.989287
429.819313	21139.108744	29.994304
430.232207	21183.674402	29.999322
430.811305	21194.342112	30.004340
431.967506	21221.458698	30.009357
432.426063	21254.262598	30.014375
432.850437	21254.899903	30.019392
433.320275	21279.259144	30.024410
433.560946	21290.303755	30.029428
433.812328	21314.137096	30.034445
434.381843	21331.322147	30.039463
434.578741	21358.068078	30.044480
434.872808	21382.670498	30.049498
435.476844	21399.417735	30.054516
436.975797	21401.795314	30.059533
437.176464	21404.315177	30.064551
437.940639	21419.223881	30.069568
438.338972	21440.205751	30.074586
438.482965	21449.572550	30.079604
438.797798	21453.220968	30.084621
438.857988	21471.641942	30.089639
439.323093	21494.563334	30.094656
439.600594	21517.733603	30.099674
440.223311	21532.140414	30.104692
440.303847	21561.100270	30.109709
440.481359	21593.772448	30.114727
441.106519	21618.067299	30.119744
441.431480	21636.632152	30.124762
441.596512	21668.459011	30.129780
442.251201	21706.672599	30.134797
442.340039	21730.466310	30.139815
443.051419	21753.176352	30.144832
443.043532	21800.658011	30.149850
443.441829	21830.363218	30.154868
444.157544	21870.592435	30.159885
444.142582	21919.534242	30.164903
444.937498	21955.842895	30.169920
445.095171	22003.149133	30.174938
445.614134	22033.410460	30.179956
446.350110	22073.832298	30.184973
446.199089	22114.061612	30.189991
447.389079	22162.428606	30.195008
447.538950	22211.064653	30.200026
448.061350	22247.864773	30.205044
448.826159	22278.580458	30.210061
449.259478	22308.347931	30.215079
452.315425	22278.423911	30.220096
452.888132	22290.895502	30.225114
453.548140	22284.709822	30.230132
453.974729	22261.716953	30.235149
454.007768	22258.925858	30.240167
454.628718	22240.300209	30.245184
454.505851	22251.445162	30.250202
455.273620	22237.596759	30.255220
455.494058	22228.726781	30.260237
455.864926	22239.537078	30.265255
455.961854	22238.122044	30.270272
456.108140	22261.950722	30.275290
456.327761	22274.080802	30.280308
456.959301	22280.178125	30.285325
456.966863	22308.579941	30.290343
457.270425	22312.083070	30.295360
457.109476	22339.553234	30.300378
457.393290	22360.009529	30.305396
457.764309	22390.977213	30.310413
457.358834	22417.219942	30.315431
458.258317	22448.967585	30.320448
458.539398	22495.182860	30.325466
458.916046	22532.444801	30.330484
459.497908	22579.870275	30.335501
459.449797	22624.084180	30.340519
460.280291	22651.089733	30.345536
460.353229	22712.579932	30.350554
460.961672	22759.878047	30.355572
461.627704	22800.200254	30.360589
462.150083	22850.085644	30.365607
462.573885	22885.079514	30.370624
462.963616	22935.266714	30.375642
463.072318	22975.300082	30.380660
463.842258	23011.960144	30.385677
464.308132	23066.581253	30.390695
465.234112	23103.953931	30.395712
465.550415	23161.665624	30.400730
465.981765	23190.180297	30.405748
466.577895	23244.444136	30.410765
466.853022	23296.005551	30.415783
467.387410	23336.375300	30.420800
467.894413	23372.544822	30.425818
468.306627	23423.272699	30.430836
468.716986	23463.228512	30.435853
469.009891	23513.180112	30.440871
469.906338	23553.359606	30.445888
470.157766	23598.229543	30.450906
470.826862	23635.835813	30.455924
471.636290	23673.874321	30.460941
471.980569	23715.161488	30.465959
472.231656	23759.319845	30.470976
473.060602	23791.266530	30.475994
473.634087	23840.370199	30.481012
474.282855	23858.781304	30.486029
474.897786	23900.676484	30.491047
475.906836	23923.462745	30.496064
476.257164	23951.280382	30.501082
476.542453	23974.509718	30.506100
477.372563	23995.471086	30.511117
477.523822	24035.891047	30.516135
477.705321	24058.902301	30.521152
478.354591	24085.847010	30.526170
478.981403	24112.241571	30.531188
479.279493	24142.023002	30.536205
479.714667	24177.166783	30.541223
479.905702	24206.732223	30.546240
480.323153	24244.647854	30.551258
480.507519	24284.318760	30.556276
481.439081	24307.852878	30.561293
481.751853	24340.101106	30.566311
482.619314	24361.956606	30.571328
483.033841	24378.994793	30.576346
483.464730	24412.623376	30.581364
483.897081	24429.833657	30.586381
484.074220	24466.257516	30.591399
484.565017	24501.144222	30.596416
484.916801	24531.733143	30.601434
485.207824	24577.184820	30.606452
485.743575	24590.287229	30.611469
486.131348	24631.200382	30.616487
486.790917	24662.369932	30.621504
486.983821	24710.119743	30.626522
487.716785	24738.790802	30.631540
488.179209	24771.602151	30.636557
488.470375	24834.143410	30.641575
489.408975	24856.982414	30.646592
489.699821	24894.689731	30.651610
490.059068	24938.081010	30.656628
490.462700	24980.310465	30.661645
491.197494	25022.915820	30.666663
491.984307	25046.622195	30.671680
492.975470	25077.564055	30.676698
493.601079	25112.683495	30.681716
494.555198	25125.035116	30.686733
494.437323	25150.798497	30.691751
494.971371	25173.331364	30.696768
495.406895	25200.616095	30.701786
495.943553	25243.290630	30.706804
496.419419	25257.015236	30.711821
496.836738	25288.420761	30.716839
497.134364	25325.764056	30.721856
497.852365	25342.606034	30.726874
498.074553	25381.221149	30.731892
498.792594	25413.451881	30.736909
498.869996	25451.552169	30.741927
499.209595	25483.985923	30.746944
500.041617	25515.859164	30.751962
500.478853	25559.725772	30.756980
501.086731	25587.792773	30.761997
501.362921	25623.040689	30.767015
502.023833	25657.235549	30.772032
502.639985	25705.515685	30.777050
503.090877	25737.351610	30.782068
503.641911	25764.470792	30.787085
503.851614	25805.958901	30.792103
504.355440	25842.839616	30.797120
504.911962	25870.917659	30.802138
504.913034	25915.343955	30.807156
505.854180	25953.037608	30.812173
506.406729	25997.644922	30.817191
506.926094	26037.560654	30.822208
507.393358	26078.588526	30.827226
507.646115	26112.300265	30.832244
508.578416	26149.835074	30.837261
508.772150	26183.411404	30.842279
509.224229	26222.131360	30.847296
510.159064	26250.902178	30.852314
510.558902	26280.447631	30.857332
510.852400	26302.476804	30.862349
511.453709	26344.278924	30.867367
511.990793	26365.409061	30.872384
512.364529	26399.300664	30.877402
512.442292	26441.192742	30.882420
513.275324	26472.901492	30.887437
513.783021	26518.183122	30.892455
513.952369	26552.273841	30.897472
514.929514	26599.151149	30.902490
515.177326	26634.202535	30.907508
515.906626	26671.759874	30.912525
516.119394	26709.872299	30.917543
516.796030	26752.482060	30.922560
517.137918	26803.145177	30.927578
517.479222	26841.721182	30.932596
518.163902	26878.332800	30.937613
518.547694	26932.229337	30.942631
519.016253	26981.245104	30.947648
519.680102	27022.248789	30.952666
519.997639	27074.607404	30.957684
520.603519	27118.816179	30.962701
520.964615	27178.077848	30.967719
521.320874	27213.779759	30.972736
522.049917	27275.873111	30.977754
522.525069	27327.276159	30.982772
523.560669	27364.762682	30.987789
523.956844	27413.513954	30.992807
524.320228	27469.323797	30.997824
525.688160	27493.210683	31.002842
526.084036	27530.687620	31.007860
526.916467	27571.473600	31.012877
527.652205	27602.467332	31.017895
528.488988	27635.438412	31.022912
529.120440	27658.880307	31.027930
529.481033	27675.077295	31.032948
531.078993	27688.464507	31.037965
531.706889	27691.982566	31.042983
532.223899	27704.733598	31.048000
533.034323	27698.603869	31.053018
533.469836	27714.365072	31.058036
533.580421	27733.737801	31.063053
533.757534	27751.781001	31.068071
534.229183	27760.368135	31.073088
534.440450	27782.269818	31.078106
534.593581	27815.646425	31.083124
534.996743	27839.036703	31.088141
535.290127	27874.917128	31.093159
535.730171	27912.863815	31.098176
536.029574	27942.098174	31.103194
536.268515	27988.184711	31.108212
536.854275	28024.072469	31.113229
537.137250	28067.080911	31.118247
537.585919	28100.001306	31.123264
538.461802	28147.351514	31.128282
538.879346	28189.130167	31.133300
538.992054	28214.562284	31.138317
539.576009	28264.326270	31.143335
539.854551	28327.035938	31.148352
540.403936	28360.601107	31.153370
541.308786	28411.668099	31.158388
542.020089	28452.622154	31.163405
542.452118	28499.040258	31.168423
542.853302	28537.823509	31.173440
543.817288	28582.113189	31.178458
544.073281	28634.516587	31.183476
544.602460	28673.391663	31.188493
545.027641	28725.875565	31.193511
545.579560	28769.229120	31.198528
545.820499	28816.643024	31.203546
546.253677	28876.170470	31.208564
547.031444	28923.978254	31.213581
547.612581	28981.158028	31.218599
548.444021	29039.722777	31.223616
548.952065	29077.900895	31.228634
549.370415	29141.992439	31.233652
550.098742	29181.320820	31.238669
550.827898	29229.285384	31.243687
551.217768	29284.016138	31.248704
551.851438	29325.276310	31.253722
552.106724	29374.453052	31.258740
553.067197	29422.318300	31.263757
553.546227	29467.409436	31.268775
553.964293	29528.249728	31.273792
554.651104	29556.985581	31.278810
555.000957	29617.372155	31.283828
555.757327	29669.256319	31.288845
556.501045	29716.217663	31.293863
556.713829	29776.045113	31.298880
557.971319	29804.646373	31.303898
558.890661	29842.598438	31.308916
559.758334	29885.308934	31.313933
560.232615	29923.420337	31.318951
560.580282	29959.953909	31.323968
561.083820	29988.965576	31.328986
561.390270	30034.189785	31.334004
561.591991	30066.300860	31.339021
562.533133	30106.484883	31.344039
562.628863	30164.474249	31.349056
563.702036	30204.227712	31.354074
563.884998	30249.937119	31.359092
564.637535	30292.878212	31.364109
564.630159	30345.180897	31.369127
565.530799	30392.383968	31.374144
566.071576	30446.577627	31.379162
566.093806	30492.956349	31.384180
566.421733	30536.558318	31.389197
567.356360	30581.105556	31.394215
567.538340	30638.200251	31.399232
568.351352	30678.536905	31.404250
568.506081	30737.987817	31.409268
569.137482	30785.290069	31.414285
569.660988	30847.754462	31.419303
570.077708	30905.775699	31.424320
570.723443	30959.182036	31.429338
571.035510	31010.766106	31.434356
571.355705	31084.025557	31.439373
572.275168	31137.392026	31.444391
572.962046	31198.313910	31.449408
573.855861	31246.678994	31.454426
574.548068	31311.900178	31.459444
575.025757	31365.329873	31.464461
575.861460	31411.532753	31.469479
576.078737	31480.679241	31.474496
576.835110	31516.065198	31.479514
577.674917	31578.316487	31.484532
578.287800	31633.352134	31.489549
578.901043	31671.776462	31.494567
579.499908	31728.901533	31.499584
580.078567	31775.854089	31.504602
580.827820	31824.535496	31.509620
581.717092	31866.888344	31.514637
582.373586	31912.120285	31.519655
582.839424	31957.593929	31.524672
583.406671	31998.373330	31.529690
584.215874	32045.255257	31.534708
584.675350	32082.453516	31.539725
585.396871	32121.894078	31.544743
585.562010	32169.320286	31.549760
586.752871	32224.511742	31.554778
587.678163	32267.361130	31.559796
587.836119	32305.895708	31.564813
587.929514	32348.302474	31.569831
588.264882	32393.698796	31.574848
589.434959	32435.918538	31.579866
589.536763	32494.635486	31.584884
589.987565	32539.443215	31.589901
590.867021	32594.293017	31.594919
591.257210	32654.302857	31.599936
592.193517	32694.728857	31.604954
592.516411	32746.682327	31.609972
593.276778	32802.743464	31.614989
594.086378	32850.972197	31.620007
594.179939	32901.788337	31.625024
594.693731	32957.499922	31.630042
595.020845	33000.597812	31.635060
595.885625	33054.866667	31.640077
596.880139	33101.726809	31.645095
597.265926	33153.599026	31.650112
597.955424	33209.526230	31.655130
598.754619	33253.167510	31.660148
600.170408	33273.729231	31.665165
600.870329	33315.124440	31.670183
601.547751	33341.160262	31.675200
603.001885	33338.903096	31.680218
603.418146	33350.195987	31.685236
604.308291	33371.063816	31.690253
605.071885	33375.980248	31.695271
605.494242	33398.445369	31.700288
605.758250	33410.476637	31.705306
605.993096	33425.274330	31.710324
606.231694	33456.643672	31.715341
606.700831	33480.562736	31.720359
606.920946	33513.357005	31.725376
607.360112	33545.599403	31.730394
607.845112	33594.944475	31.735412
608.060902	33636.767549	31.740429
608.668859	33686.511050	31.745447
608.792384	33733.984617	31.750464
609.470455	33788.774295	31.755482
609.923416	33848.348104	31.760500
610.611229	33900.131990	31.765517
611.249100	33958.972095	31.770535
611.478902	34032.739799	31.775552
611.981329	34085.997782	31.780570
612.825966	34140.049549	31.785588
613.195019	34220.445253	31.790605
614.065355	34271.428775	31.795623
614.877332	34347.168703	31.800640
615.275095	34409.420647	31.805658
616.045269	34460.723379	31.810676
617.135554	34514.795569	31.815693
618.090972	34569.827410	31.820711
618.775840	34616.249293	31.825728
619.456502	34654.830612	31.830746
620.477918	34700.155508	31.835764
621.020978	34752.491642	31.840781
621.891332	34781.891585	31.845799
622.795988	34830.424655	31.850816
623.032226	34865.419792	31.855834
623.711502	34900.571460	31.860852
624.703539	34949.037359	31.865869
625.213355	34972.632064	31.870887
625.499970	35019.717567	31.875904
626.449101	35050.983058	31.880922
627.333111	35095.605722	31.885940
627.721703	35133.482668	31.890957
628.119576	35169.047046	31.895975
628.631986	35215.936337	31.900992
629.252819	35258.687451	31.906010
629.812109	35305.657814	31.911028
630.078265	35355.317266	31.916045
630.775530	35398.512184	31.921063
630.944468	35456.976634	31.926080
631.587168	35502.474384	31.931098
632.038828	35560.435393	31.936116
632.632263	35616.901516	31.941133
633.291949	35671.919451	31.946151
633.435394	35731.918186	31.951168
633.993040	35773.370547	31.956186
634.657131	35834.710382	31.961204
635.337293	35902.002652	31.966221
635.957487	35956.283659	31.971239
636.505978	36019.662195	31.976256
637.234685	36072.775382	31.981274
638.178927	36115.909169	31.986292
638.437155	36183.793196	31.991309
639.300894	36238.233407	31.996327
639.650282	36314.544664	32.001344
640.689900	36376.436829	32.006362
641.447320	36431.220960	32.011380
641.450621	36500.143295	32.016397
642.488713	36556.332071	32.021415
643.315523	36619.774183	32.026432
644.593841	36647.155817	32.031450
646.189322	36683.746714	32.036468
646.724784	36739.109568	32.041485
647.446165	36776.204077	32.046503
647.793065	36804.379155	32.051520
648.507607	36851.844694	32.056538
649.188573	36881.549685	32.061556
649.950850	36921.012481	32.066573
650.549180	36959.678447	32.071591
651.098217	37009.959947	32.076608
651.751460	37046.443111	32.081626
652.572621	37085.759744	32.086644
652.831027	37128.068794	32.091661
653.211778	37176.711017	32.096679
653.676937	37242.786255	32.101696
654.433744	37278.209646	32.106714
654.919881	37327.969181	32.111732
655.310091	37388.260899	32.116749
655.751315	37441.761610	32.121767
656.600881	37512.287716	32.126784
656.797110	37569.662473	32.131802
657.551874	37634.184180	32.136820
657.839821	37710.908877	32.141837
658.625695	37787.053218	32.146855
659.197396	37858.090160	32.151872
659.843081	37922.166765	32.156890
660.391656	37995.475369	32.161908
660.919093	38072.366969	32.166925
661.795567	38143.615169	32.171943
662.174985	38215.346482	32.176960
662.447441	38307.521137	32.181978
663.499460	38376.883301	32.186996
664.226989	38455.521849	32.192013
664.982585	38534.313974	32.197031
665.547700	38617.230274	32.202048
666.447768	38679.373870	32.207066
667.245755	38763.225137	32.212084
667.542921	38837.152961	32.217101
668.407311	38890.292830	32.222119
668.928806	38962.635418	32.227136
669.374487	39038.525749	32.232154
670.620519	39104.703082	32.237172
671.247771	39167.114245	32.242189
671.810973	39236.275496	32.247207
672.440849	39291.626928	32.252224
673.049271	39360.936020	32.257242
673.831792	39418.807114	32.262260
674.170236	39501.344355	32.267277
675.217540	39563.776815	32.272295
675.854156	39636.775704	32.277312
676.709719	39699.045229	32.282330
677.445685	39760.690631	32.287348
678.491171	39824.680782	32.292365
680.142518	39870.042301	32.297383
680.523449	39916.069863	32.302400
681.459524	39970.827539	32.307418
682.221957	40007.257114	32.312436
682.607813	40073.046899	32.317453
683.592534	40106.697355	32.322471
684.358572	40145.107335	32.327488
685.011690	40192.555740	32.332506
685.571222	40239.539774	32.337524
686.130997	40306.570664	32.342541
686.898203	40347.564035	32.347559
687.429425	40404.671066	32.352576
687.814335	40451.506862	32.357594
688.613686	40505.048495	32.362612
689.184052	40564.714053	32.367629
689.676268	40616.604912	32.372647
690.298022	40680.687824	32.377664
690.828741	40746.002943	32.382682
691.592336	40799.932834	32.387700
692.254856	40877.730259	32.392717
692.708403	40933.794799	32.397735
693.333801	41009.699960	32.402752
693.887188	41081.516547	32.407770
695.473610	41130.903828	32.412788
695.784275	41204.904398	32.417805
696.821559	41263.611722	32.422823
697.430158	41316.750989	32.427840
697.987712	41388.467263	32.432858
698.714605	41452.914820	32.437876
699.180033	41516.375977	32.442893
700.273902	41574.759935	32.447911
700.535419	41639.733346	32.452928
701.242103	41712.553288	32.457946
701.859794	41776.694558	32.462964
702.363736	41849.250858	32.467981
703.068101	41918.176508	32.472999
703.784490	41981.261909	32.478016
704.548909	42048.292246	32.483034
705.488493	42122.130375	32.488052
706.279162	42185.904959	32.493069
707.623770	42226.385051	32.498087
708.772830	42260.647605	32.503104
709.599821	42302.825323	32.508122
710.667215	42331.549353	32.513140
711.480734	42378.691217	32.518157
712.097080	42404.115162	32.523175
713.099434	42439.231034	32.528192
713.443889	42463.345128	32.533210
714.375432	42490.690508	32.538228
714.633255	42535.325214	32.543245
715.460021	42573.570095	32.548263
715.845244	42615.115485	32.553280
716.381978	42660.967874	32.558298
717.056047	42709.094946	32.563316
717.465409	42758.620707	32.568333
718.177692	42813.202282	32.573351
718.733216	42876.382815	32.578368
718.936926	42934.345315	32.583386
719.476525	42994.437431	32.588404
719.781239	43063.942316	32.593421
720.636213	43130.650145	32.598439
721.259853	43208.199301	32.603456
721.811106	43279.110567	32.608474
722.686792	43357.150222	32.613492
723.042164	43440.247819	32.618509
724.115867	43522.070558	32.623527
724.944159	43590.891666	32.628544
725.948631	43671.830230	32.633562
726.609490	43732.009697	32.638580
727.008726	43821.676360	32.643597
728.314047	43889.214476	32.648615
728.762636	43967.845393	32.653632
729.323066	44040.991807	32.658650
730.231893	44116.543715	32.663668
731.202077	44182.672556	32.668685
733.605165	44219.313585	32.673703
735.076320	44259.686824	32.678720
736.129880	44292.981202	32.683738
737.144531	44300.466736	32.688756
737.886517	44336.202083	32.693773
738.738258	44354.158886	32.698791
739.384335	44377.429477	32.703808
739.492433	44418.808786	32.708826
740.334178	44449.452504	32.713844
740.608958	44483.950164	32.718861
741.167299	44521.977091	32.723879
741.459508	44566.579998	32.728896
741.996445	44624.047100	32.733914
742.512134	44662.349280	32.738932
742.704220	44746.034352	32.743949
742.995215	44814.141373	32.748967
743.788735	44875.808524	32.753984
744.419487	44956.992395	32.759002
745.016892	45026.824481	32.764020
745.374573	45102.815451	32.769037
746.149008	45174.856743	32.774055
746.540572	45249.640947	32.779072
747.492988	45323.695732	32.784090
748.170944	45389.083798	32.789108
748.712204	45477.177827	32.794125
749.689751	45546.598113	32.799143
750.325589	45631.882580	32.804160
750.492491	45713.522403	32.809178
751.372231	45790.676300	32.814196
752.245688	45873.646210	32.819213
752.690036	45966.266625	32.824231
753.318044	46060.962699	32.829248
753.984826	46144.569405	32.834266
754.784610	46238.317811	32.839284
755.752775	46349.257227	32.844301
756.534210	46433.692618	32.849319
757.487777	46522.830537	32.854336
758.056749	46624.082762	32.859354
758.920686	46715.362489	32.864372
759.704678	46807.093984	32.869389
761.147265	46889.350203	32.874407
762.825175	46945.579971	32.879424
763.829557	47027.117799	32.884442
764.565527	47087.678635	32.889460
765.507656	47164.532040	32.894477
765.865021	47230.577491	32.899495
766.909972	47293.390020	32.904512
767.574695	47365.994159	32.909530
768.257963	47440.832741	32.914548
769.136247	47503.672552	32.919565
769.680466	47586.191791	32.924583
770.787750	47646.212669	32.929600
771.783666	47702.919452	32.934618
772.735961	47764.451568	32.939636
773.320436	47836.754882	32.944653
773.884038	47894.266300	32.949671
774.685709	47966.784843	32.954688
775.267466	48046.933720	32.959706
775.750323	48112.908845	32.964724
776.539957	48185.733119	32.969741
777.133253	48269.459409	32.974759
777.981251	48344.856189	32.979776
778.437896	48428.898442	32.984794
779.160281	48508.935510	32.989812
780.031623	48590.457551	32.994829
780.446845	48676.612280	32.999847
781.530011	48759.701217	33.004864
781.821686	48857.261605	33.009882
782.884563	48951.919715	33.014900
783.745210	49031.735172	33.019917
784.075261	49124.393473	33.024935
785.097220	49212.369646	33.029952
785.751773	49305.485283	33.034970
786.469665	49386.823974	33.039988
787.536395	49478.801986	33.045005
788.392200	49555.480693	33.050023
789.524837	49627.479978	33.055040
790.091778	49697.998075	33.060058
791.299583	49764.463500	33.065076
791.920030	49836.876514	33.070093
792.666929	49913.321639	33.075111
793.731026	49983.988937	33.080128
794.366310	50056.845439	33.085146
795.259877	50123.428495	33.090164
796.115046	50202.388542	33.095181
796.721987	50273.634683	33.100199
797.502668	50340.416398	33.105216
798.048555	50427.413997	33.110234
798.821648	50509.421201	33.115252
799.946242	50593.130630	33.120269
800.360197	50671.408733	33.125287
801.232863	50754.246976	33.130304
802.184190	50844.208538	33.135322
803.108870	50910.167860	33.140340
803.874484	50980.028202	33.145357
804.849465	51052.134065	33.150375
806.061711	51122.608703	33.155392
806.457369	51210.688095	33.160410
807.258352	51283.330693	33.165428
808.255822	51358.549143	33.170445
809.294491	51447.512005	33.175463
809.756829	51516.302331	33.180480
810.453559	51596.486705	33.185498
811.608698	51666.887357	33.190516
812.873942	51752.508141	33.195533
813.051841	51831.267557	33.200551
813.770222	51894.154612	33.205568
814.519010	51985.893122	33.210586
815.072890	52073.901049	33.215604
816.080559	52162.244311	33.220621
816.795947	52251.363597	33.225639
818.295829	52325.193162	33.230656
818.853653	52405.393774	33.235674
819.711244	52478.455105	33.240692
820.404083	52570.811476	33.245709
820.655954	52652.681009	33.250727
821.863135	52745.300425	33.255744
822.202835	52830.322468	33.260762
823.114753	52918.318543	33.265780
823.921938	53012.069806	33.270797
824.551319	53116.401308	33.275815
825.528437	53191.706390	33.280832
826.421785	53294.873260	33.285850
827.417015	53381.150754	33.290868
828.679399	53454.628197	33.295885
829.732606	53545.354000	33.300903
830.631327	53619.372918	33.305920
831.523214	53700.040571	33.310938
831.922086	53784.622079	33.315956
833.308265	53847.703172	33.320973
833.824536	53925.328860	33.325991
834.682909	53988.693309	33.331008
835.304879	54070.279899	33.336026
836.062304	54140.466249	33.341044
837.040513	54208.060984	33.346061
837.849778	54287.652253	33.351079
838.678668	54351.761277	33.356096
839.629017	54430.636286	33.361114
840.023474	54501.513101	33.366132
840.624966	54584.443616	33.371149
841.217087	54670.431541	33.376167
842.217078	54751.531718	33.381184
843.075523	54841.502680	33.386202
844.112288	54931.313126	33.391220
845.257571	55021.450812	33.396237
845.840067	55104.714998	33.401255
846.591880	55181.023787	33.406272
847.382431	55264.912167	33.411290
848.076765	55355.865089	33.416308
849.037600	55448.688997	33.421325
849.485320	55542.340026	33.426343
850.503068	55636.892014	33.431360
850.972355	55739.369958	33.436378
851.925374	55834.160550	33.441396
853.048320	55927.904949	33.446413
853.434083	56033.699807	33.451431
854.583224	56126.793910	33.456448
855.583656	56238.976190	33.461466
856.371881	56335.768610	33.466484
857.595099	56422.576627	33.471501
858.396454	56523.029892	33.476519
859.305639	56613.096170	33.481536
860.152099	56716.453959	33.486554
861.109855	56811.608718	33.491572
862.149626	56908.244146	33.496589
862.720468	57008.051684	33.501607
863.758056	57101.203193	33.506624
864.755712	57191.690719	33.511642
865.615001	57285.578700	33.516660
866.488385	57374.224268	33.521677
866.984372	57474.750252	33.526695
868.546224	57565.841204	33.531712
869.358640	57661.414945	33.536730
869.866244	57748.693528	33.541748
871.152740	57838.933039	33.546765
872.067673	57937.778425	33.551783
872.874221	58023.694208	33.556800
874.064006	58105.653486	33.561818
874.991637	58190.865674	33.566836
876.027399	58259.062854	33.571853
876.941757	58352.019267	33.576871
878.029333	58434.034149	33.581888
878.747245	58514.308616	33.586906
879.340708	58599.168581	33.591924
880.441751	58672.578940	33.596941
881.008213	58753.140591	33.601959
881.590343	58822.974877	33.606976
882.338757	58909.721739	33.611994
882.923378	58991.279228	33.617012
883.751086	59075.598916	33.622029
884.058703	59177.919547	33.627047
884.989458	59264.708501	33.632064
885.964780	59357.701275	33.637082
886.821948	59461.843041	33.642100
888.362905	59529.209866	33.647117
888.855073	59636.902759	33.652135
889.530917	59727.116005	33.657152
890.780553	59817.753029	33.662170
891.865056	59915.757833	33.667188
892.938554	60000.715115	33.672205
893.740764	60095.270477	33.677223
894.807595	60178.581425	33.682240
895.319323	60272.167196	33.687258
895.889757	60382.131633	33.692276
896.892554	60480.092399	33.697293
897.570825	60581.566005	33.702311
898.334928	60685.580976	33.707328
899.446798	60783.112321	33.712346
900.599838	60883.953109	33.717364
901.408065	60983.099988	33.722381
903.380873	61065.557071	33.727399
905.144148	61134.053152	33.732416
906.326151	61217.732460	33.737434
907.030224	61289.485867	33.742452
908.338051	61354.796513	33.747469
908.835530	61432.886088	33.752487
909.594805	61500.330725	33.757504
910.808626	61576.137548	33.762522
910.781235	61652.679014	33.767540
911.943816	61733.644894	33.772557
912.158865	61827.014036	33.777575
912.868458	61918.956566	33.782592
914.195694	62019.393619	33.787610
914.844339	62114.473018	33.792628
916.334823	62179.511147	33.797645
917.385114	62268.344384	33.802663
918.315285	62352.678265	33.807680
919.446918	62429.827893	33.812698
919.966069	62517.906831	33.817716
921.069206	62602.315350	33.822733
922.089871	62688.382641	33.827751
923.029173	62768.229530	33.832768
923.976482	62842.151194	33.837786
924.487837	62934.635467	33.842804
925.565092	63019.899453	33.847821
926.389695	63108.115683	33.852839
927.063949	63196.716259	33.857856
927.865137	63286.342348	33.862874
928.619530	63383.050280	33.867892
929.471951	63470.670055	33.872909
930.304371	63574.348967	33.877927
931.211803	63650.522339	33.882944
932.004093	63737.559193	33.887962
932.410446	63828.684433	33.892980
933.261140	63922.679603	33.897997
934.253685	64024.857484	33.903015
935.703153	64104.663538	33.908032
937.731559	64183.623002	33.913050
938.493468	64259.739853	33.918068
939.500926	64338.764518	33.923085
940.469709	64426.818630	33.928103
940.990194	64509.297602	33.933120
942.207993	64589.448895	33.938138
943.006664	64684.896243	33.943156
944.236446	64756.219052	33.948173
944.947738	64843.390686	33.953191
945.627939	64927.475708	33.958208
946.489982	65026.723557	33.963226
946.920741	65123.093843	33.968244
948.118829	65210.884513	33.973261
948.920216	65319.631141	33.978279
949.324812	65420.327692	33.983296
950.320052	65517.996654	33.988314
950.844355	65645.578400	33.993332
951.864963	65760.612588	33.998349
952.889859	65872.883151	34.003367
953.465241	65989.410843	34.008384
954.451763	66120.175385	34.013402
955.260667	66240.530249	34.018420
956.058784	66359.883172	34.023437
957.030640	66494.926052	34.028455
957.787672	66626.340130	34.033472
958.814971	66749.923043	34.038490
959.737410	66886.113602	34.043508
960.904586	67012.872438	34.048525
962.315157	67145.259977	34.053543
963.040643	67273.695387	34.058560
964.429241	67398.501045	34.063578
965.440256	67523.285458	34.068596
966.497019	67639.515890	34.073613
967.549273	67766.310565	34.078631
968.499152	67877.145341	34.083648
969.828185	67983.814008	34.088666
970.883429	68103.642143	34.093684
972.029981	68205.400702	34.098701
973.195649	68328.422004	34.103719
973.935874	68437.726544	34.108736
974.919107	68547.694300	34.113754
975.738549	68666.552572	34.118772
976.928290	68770.512109	34.123789
977.880768	68885.578814	34.128807
978.790530	69007.103551	34.133824
979.810299	69113.227399	34.138842
980.850985	69237.266218	34.143860
981.779777	69325.033073	34.148877
983.618608	69417.078138	34.153895
984.488523	69501.089612	34.158912
985.472592	69586.359533	34.163930
986.444457	69680.211747	34.168948
987.654654	69755.811325	34.173965
988.348960	69852.368454	34.178983
989.245082	69937.641258	34.184000
990.248506	70035.799151	34.189018
990.830312	70142.876482	34.194036
991.713116	70231.615080	34.199053
992.770832	70331.244286	34.204071
993.930157	70434.415056	34.209088
994.822625	70533.964166	34.214106
995.522692	70646.655089	34.219124
996.771015	70742.743012	34.224141
997.564123	70844.685232	34.229159
998.644934	70939.157960	34.234176
1000.193472	71038.004973	34.239194
1000.684717	71145.342252	34.244212
1001.839887	71254.918684	34.249229
1002.907543	71360.080280	34.254247
1003.454828	71468.712033	34.259264
1004.483000	71571.713730	34.264282
1005.221761	71686.009363	34.269300
1006.827319	71805.235410	34.274317
1007.467668	71909.924490	34.279335
1008.177670	72037.439364	34.284352
1009.349173	72149.040170	34.289370
1010.114310	72280.465540	34.294388
1011.151636	72398.205816	34.299405
1012.492126	72511.765928	34.304423
1012.973029	72634.853538	34.309440
1014.536528	72752.847108	34.314458
1015.991971	72877.082899	34.319476
1017.250242	72966.469109	34.324493
1018.725536	73074.317429	34.329511
1020.047101	73169.546042	34.334528
1021.010716	73261.425986	34.339546
1021.875980	73365.903669	34.344564
1023.033380	73468.060471	34.349581
1024.397114	73565.199012	34.354599
1025.004911	73672.221711	34.359616
1026.406197	73760.868316	34.364634
1026.933794	73861.667540	34.369652
1028.299966	73958.276768	34.374669
1029.002294	74054.195816	34.379687
1029.579705	74171.943871	34.384704
1030.568627	74265.903519	34.389722
1031.536796	74382.017069	34.394740
1032.407142	74484.490137	34.399757
1033.637778	74602.351658	34.404775
1034.400671	74715.087168	34.409792
1035.719031	74822.862429	34.414810
1036.683678	74941.893163	34.419828
1037.956155	75044.798050	34.424845
1038.743775	75144.298367	34.429863
1039.333128	75239.684887	34.434880
1040.411163	75342.634864	34.439898
1041.295624	75451.108176	34.444916
1042.227620	75557.033884	34.449933
1043.087783	75665.126691	34.454951
1043.847736	75785.509513	34.459968
1044.896708	75906.504360	34.464986
1045.630234	76016.085440	34.470004
1046.635643	76140.463547	34.475021
1047.565508	76271.389501	34.480039
1048.144261	76417.016115	34.485056
1048.874930	76537.780947	34.490074
1049.754670	76691.337817	34.495092
1051.106189	76827.894876	34.500109
1052.297725	76969.926484	34.505127
1053.003549	77124.651955	34.510144
1054.226966	77273.614135	34.515162
1055.151152	77411.374448	34.520180
1056.674296	77565.259016	34.525197
1058.391936	77704.241366	34.530215
1059.578961	77833.986086	34.535232
1061.016499	77963.198762	34.540250
1062.322194	78091.213323	34.545268
1063.534858	78205.742292	34.550285
1064.846705	78322.613787	34.555303
1066.046000	78449.370705	34.560320
1067.307283	78563.489402	34.565338
1068.565335	78689.966659	34.570356
1069.639837	78800.519777	34.575373
1070.724483	78914.327188	34.580391
1071.704297	79033.752339	34.585408
1072.536098	79136.747986	34.590426
1073.909460	79252.995521	34.595444
1074.993759	79368.006502	34.600461
1076.469090	79482.412302	34.605479
1076.882498	79600.230434	34.610496
1077.919243	79706.679310	34.615514
1078.601160	79829.001004	34.620532
1079.859417	79941.692883	34.625549
1081.044927	80071.565729	34.630567
1081.560495	80210.199940	34.635584
1082.968928	80333.641719	34.640602
1083.684832	80463.452645	34.645620
1084.908969	80580.768099	34.650637
1086.397882	80720.066361	34.655655
1086.988104	80855.443724	34.660672
1088.227687	80983.530984	34.665690
1088.784276	81126.450838	34.670708
1089.902136	81261.544617	34.675725
1091.323240	81390.130206	34.680743
1091.930335	81529.144263	34.685760
1093.570666	81662.520188	34.690778
1095.136806	81797.274291	34.695796
1096.212783	81908.425352	34.700813
1097.598959	82019.925945	34.705831
1098.662445	82123.974278	34.710848
1099.860001	82229.044933	34.715866
1101.073178	82334.044089	34.720884
1101.616293	82441.628600	34.725901
1103.049715	82555.476340	34.730919
1103.527333	82674.818932	34.735936
1104.773722	82779.815037	34.740954
1105.773645	82898.974670	34.745972
1106.710841	83018.865690	34.750989
1108.099811	83145.545208	34.756007
1109.111631	83270.300269	34.761024
1110.375096	83390.463949	34.766042
1111.235210	83501.847448	34.771060
1112.502333	83614.639923	34.776077
1114.350421	83731.513417	34.781095
1115.228823	83850.602922	34.786112
1116.397125	83970.449949	34.791130
1117.554457	84093.903260	34.796148
1118.637470	84207.101213	34.801165
1119.620961	84323.401044	34.806183
1120.765450	84444.639200	34.811200
1122.387064	84543.021475	34.816218
1123.725107	84660.860087	34.821236
1124.850722	84771.651642	34.826253
1126.059644	84876.638844	34.831271
1126.945162	84988.797506	34.836288
1128.087158	85103.982555	34.841306
1129.109013	85220.609988	34.846324
1130.119067	85337.132447	34.851341
1131.814578	85453.445356	34.856359
1132.708348	85567.439414	34.861376
1133.906154	85671.382687	34.866394
1134.926821	85790.504702	34.871412
1135.812903	85911.836578	34.876429
1136.765707	86028.909383	34.881447
1137.725164	86156.396035	34.886464
1138.849979	86276.661334	34.891482
1140.333524	86410.794045	34.896500
1141.175048	86523.973164	34.901517
1142.471112	86643.650515	34.906535
1143.253510	86783.746139	34.911552
1144.455949	86917.446151	34.916570
1145.587090	87046.219729	34.921588
1146.602158	87179.559117	34.926605
1148.318357	87302.727115	34.931623
1149.072256	87435.161095	34.936640
1150.222949	87559.204618	34.941658
1151.146089	87696.564654	34.946676
1152.097938	87825.820383	34.951693
1153.288046	87955.987548	34.956711
1153.915140	88109.269786	34.961728
1155.640505	88232.979158	34.966746
1156.903023	88383.228046	34.971764
1158.004088	88514.291742	34.976781
1159.422182	88617.575517	34.981799
1160.900543	88740.068616	34.986816
1162.311782	88851.923525	34.991834
1163.260997	88960.469151	34.996852
1164.113205	89085.637644	35.001869
1165.200075	89188.021882	35.006887
1166.263127	89316.573166	35.011904
1167.269643	89437.678045	35.016922
1168.279589	89568.496976	35.021940
1169.508377	89711.070217	35.026957
1170.613132	89826.159955	35.031975
1171.424770	89970.660557	35.036992
1172.509755	90098.346531	35.042010
1173.882748	90242.272683	35.047028
1174.824401	90391.593528	35.052045
1175.814917	90523.388896	35.057063
1176.770496	90672.121263	35.062080
1178.067851	90815.860826	35.067098
1179.216824	90967.758328	35.072116
1180.531899	91119.459700	35.077133
1182.407303	91254.812315	35.082151
1183.605303	91411.341058	35.087168
1184.680623	91543.280847	35.092186
1185.797646	91692.766057	35.097204
1187.097320	91831.274964	35.102221
1188.368498	91963.926127	35.107239
1189.825740	92112.107751	35.112256
1191.186095	92246.289704	35.117274
1192.277394	92376.473595	35.122292
1193.174557	92525.740074	35.127309
1194.790907	92655.854763	35.132327
1195.544995	92800.870106	35.137344
1196.477622	92952.948485	35.142362
1197.660071	93100.339168	35.147380
1199.097713	93244.850221	35.152397
1200.174788	93396.693606	35.157415
1201.571806	93550.637753	35.162432
1202.598929	93685.672054	35.167450
1203.971541	93841.241378	35.172468
1204.554441	94003.534792	35.177485
1206.211760	94143.835624	35.182503
1207.193940	94301.070577	35.187520
1208.306392	94458.418754	35.192538
1209.665405	94614.817942	35.197556
1210.931476	94778.539131	35.202573
1212.316625	94927.054571	35.207591
1213.213178	95088.654411	35.212608
1214.791711	95234.851215	35.217626
1216.489206	95382.801285	35.222644
1217.446141	95532.457876	35.227661
1218.537980	95693.853879	35.232679
1220.056887	95828.019478	35.237696
1221.613393	95986.604551	35.242714
1222.444668	96136.044734	35.247732
1223.682530	96273.768618	35.252749
1224.896230	96398.433762	35.257767
1226.064728	96537.568350	35.262784
1227.315013	96666.461344	35.267802
1229.182170	96791.764912	35.272820
1230.109639	96927.834045	35.277837
1231.041166	97047.828236	35.282855
1232.536523	97178.772847	35.287872
1233.604183	97311.791674	35.292890
1234.712281	97440.079028	35.297908
1235.905627	97582.701908	35.302925
1237.206648	97722.455317	35.307943
1238.361880	97859.506035	35.312960
1239.145813	97996.996203	35.317978
1240.763967	98134.594967	35.322996
1241.502184	98287.334912	35.328013
1242.859182	98432.436092	35.333031
1243.798979	98585.392711	35.338048
1244.917847	98748.438363	35.343066
1246.273942	98909.252053	35.348084
1246.961604	99073.418819	35.353101
1248.384346	99236.406961	35.358119
1249.477022	99411.248479	35.363136
1250.859497	99573.169824	35.368154
1252.656472	99738.866910	35.373172
1253.295581	99908.944131	35.378189
1254.590134	100072.445742	35.383207
1255.842877	100262.662144	35.388224
1257.210105	100420.460200	35.393242
1258.589749	100601.092449	35.398260
1259.612494	100767.723556	35.403277
1261.139872	100939.514676	35.408295
1262.214973	101116.314349	35.413312
1263.415279	101289.805181	35.418330
1264.846634	101462.400028	35.423348
1266.123690	101632.097357	35.428365
1267.716300	101816.387801	35.433383
1268.899629	101991.455787	35.438400
1270.425798	102162.148761	35.443418
1271.955420	102331.988185	35.448436
1273.021302	102503.642707	35.453453
1274.700431	102660.741905	35.458471
1276.167483	102819.217378	35.463488
1277.610248	102977.235843	35.468506
1279.568930	103130.895652	35.473524
1280.923949	103274.660542	35.478541
1283.138401	103405.608312	35.483559
1284.811598	103522.809730	35.488576
1286.251687	103660.178440	35.493594
1287.624904	103777.099752	35.498612
1288.720198	103904.399703	35.503629
1289.978384	104023.523735	35.508647
1291.022026	104154.547890	35.513664
1291.975947	104291.029334	35.518682
1293.275345	104419.223529	35.523700
1293.960821	104558.546293	35.528717
1295.500607	104677.382036	35.533735
1296.778997	104797.690147	35.538752
1297.426449	104927.541183	35.543770
1298.840608	105050.974219	35.548788
1299.649253	105181.459172	35.553805
1301.107069	105328.270508	35.558823
1302.220776	105463.897907	35.563840
1302.927502	105607.147132	35.568858
1304.328323	105740.939462	35.573876
1305.614571	105896.091071	35.578893
1306.872454	106044.520758	35.583911
1307.728528	106198.312416	35.588928
1309.067312	106348.496848	35.593946
1310.547214	106509.868169	35.598964
1311.264127	106681.886809	35.603981
1312.569784	106846.895558	35.608999
1313.553981	107017.317183	35.614016
1314.654515	107207.259220	35.619034
1316.290997	107376.370841	35.624052
1317.652856	107571.913406	35.629069
1318.693698	107748.559037	35.634087
1320.225025	107929.153366	35.639104
1321.265003	108113.358876	35.644122
1322.466362	108294.223568	35.649140
1323.692828	108497.358638	35.654157
1324.931115	108694.410952	35.659175
1326.598455	108879.756768	35.664192
1327.209469	109083.716113	35.669210
1329.225433	109275.452962	35.674228
1330.645942	109471.241980	35.679245
1332.160009	109665.163099	35.684263
1333.608080	109868.350288	35.689280
1334.878365	110060.591599	35.694298
1336.519436	110233.729058	35.699316
1337.910363	110430.334311	35.704333
1339.077061	110611.753337	35.709351
1341.425182	110786.016621	35.714368
1342.999087	110971.532344	35.719386
1344.494536	111134.837139	35.724404
1345.935773	111310.058522	35.729421
1347.843618	111460.297914	35.734439
1349.492974	111629.221649	35.739456
1350.585429	111795.854897	35.744474
1352.099018	111951.705202	35.749492
1353.714654	112112.123395	35.754509
1355.095085	112261.514589	35.759527
1356.759225	112423.104518	35.764544
1357.769351	112574.069405	35.769562
1359.222094	112723.388568	35.774580
1360.254177	112879.663057	35.779597
1361.181027	113039.962471	35.784615
1362.505221	113203.187781	35.789632
1363.355704	113381.606949	35.794650
1364.622908	113537.955788	35.799668
1366.147695	113716.270154	35.804685
1367.365631	113872.078133	35.809703
1369.084575	114012.436324	35.814720
1369.908561	114180.090394	35.819738
1371.262310	114333.499253	35.824756
1372.215570	114499.925705	35.829773
1373.995696	114661.473626	35.834791
1375.263966	114825.079200	35.839808
1376.673730	114988.220171	35.844826
1378.083607	115146.240349	35.849844
1379.410701	115317.785228	35.854861
1380.443013	115487.656049	35.859879
1382.316834	115651.063072	35.864896
1383.245723	115830.297440	35.869914
1385.106101	115996.102018	35.874932
1386.560381	116166.587743	35.879949
1387.914985	116329.549811	35.884967
1389.635132	116496.494246	35.889984
1390.692498	116677.043725	35.895002
1392.500305	116825.032726	35.900020
1393.565996	117004.823413	35.905037
1395.193667	117170.210387	35.910055
1396.779410	117345.672331	35.915072
1397.642991	117523.282704	35.920090
1399.001583	117692.825040	35.925108
1400.626158	117876.692906	35.930125
1401.589804	118053.860467	35.935143
1403.301646	118231.809447	35.940160
1403.784706	118422.568010	35.945178
1405.476304	118612.578691	35.950196
1406.281187	118811.431798	35.955213
1407.660332	119015.906625	35.960231
1409.159887	119210.872172	35.965248
1410.647208	119420.670907	35.970266
1412.100695	119618.318970	35.975284
1413.974011	119818.042089	35.980301
1415.433568	120009.663891	35.985319
1416.897453	120204.705847	35.990336
1418.102401	120402.108040	35.995354
1420.301435	120589.893145	36.000372
1421.961272	120780.475566	36.005389
1423.173823	120981.363738	36.010407
1424.623902	121158.899329	36.015424
1426.124399	121341.557482	36.020442
1427.412941	121548.048544	36.025460
1428.777891	121737.696854	36.030477
1430.055591	121927.069081	36.035495
1431.935772	122122.401026	36.040512
1433.189402	122322.165616	36.045530
1434.997017	122496.258970	36.050548
1436.518041	122690.309603	36.055565
1438.030363	122870.823220	36.060583
1440.195526	123031.450109	36.065600
1441.237081	123221.084389	36.070618
1442.409895	123397.868379	36.075636
1444.121830	123575.289834	36.080653
1445.492338	123727.560837	36.085671
1446.785837	123892.017297	36.090688
1447.820586	124057.212535	36.095706
1449.359429	124225.748635	36.100724
1450.835658	124397.728385	36.105741
1452.031816	124568.525071	36.110759
1453.374044	124740.135630	36.115776
1454.558234	124916.661787	36.120794
1455.788435	125096.285176	36.125812
1457.028062	125271.601480	36.130829
1458.240560	125487.419888	36.135847
1459.918692	125659.147561	36.140864
1461.140591	125871.344711	36.145882
1462.621678	126056.710855	36.150900
1464.315208	126266.796693	36.155917
1465.204024	126460.442870	36.160935
1466.709370	126663.885869	36.165952
1468.143955	126872.522726	36.170970
1469.718722	127080.974211	36.175988
1471.156213	127302.687077	36.181005
1472.185571	127510.595090	36.186023
1474.067387	127730.555949	36.191040
1475.144849	127942.779406	36.196058
1477.229196	128145.305253	36.201076
1479.141957	128343.387902	36.206093
1480.405677	128570.307267	36.211111
1481.920107	128775.829374	36.216128
1483.301804	128997.666042	36.221146
1484.719642	129201.483697	36.226164
1486.097008	129437.399591	36.231181
1487.423549	129650.774722	36.236199
1489.723672	129857.763587	36.241216
1490.643131	130070.003033	36.246234
1492.276434	130299.740970	36.251252
1494.561869	130505.470025	36.256269
1495.608867	130734.886589	36.261287
1497.056641	130935.265995	36.266304
1498.699274	131160.334399	36.271322
1500.374894	131369.688830	36.276340
1501.945414	131588.944007	36.281357
1503.332815	131798.132012	36.286375
1505.170536	132014.674663	36.291392
1506.775237	132227.670333	36.296410
1508.000191	132437.218274	36.301428
1510.017902	132642.574616	36.306445
1511.155200	132852.405610	36.311463
1512.859867	133051.618790	36.316480
1514.882664	133268.686386	36.321498
1516.117480	133453.456489	36.326516
1517.616665	133670.927089	36.331533
1518.962236	133885.256018	36.336551
1520.547422	134083.899810	36.341568
1522.170118	134286.745804	36.346586
1523.516163	134500.433001	36.351604
1525.182458	134707.000337	36.356621
1526.762294	134899.555714	36.361639
1528.033776	135082.493071	36.366656
1529.334623	135275.741510	36.371674
1530.934901	135447.363967	36.376692
1532.611842	135649.159128	36.381709
1533.684530	135842.042078	36.386727
1535.516980	136038.619811	36.391744
1536.675345	136233.088377	36.396762
1538.291963	136431.147634	36.401780
1540.010333	136625.732585	36.406797
1542.139309	136822.053038	36.411815
1543.728683	137012.314491	36.416832
1545.082102	137197.761158	36.421850
1546.871699	137391.034603	36.426868
1548.453681	137585.115319	36.431885
1549.595272	137788.999812	36.436903
1551.576146	137987.683303	36.441920
1553.053992	138173.395115	36.446938
1554.377321	138381.550862	36.451956
1556.027669	138574.309212	36.456973
1557.222075	138781.094212	36.461991
1558.518020	138980.374717	36.467008
1560.201732	139193.028509	36.472026
1561.947467	139409.501283	36.477044
1563.548011	139616.227529	36.482061
1564.605757	139834.662974	36.487079
1566.263509	140036.959992	36.492096
1567.703075	140265.996346	36.497114
1569.183290	140485.776163	36.502132
1570.917931	140710.535988	36.507149
1572.370253	140932.161179	36.512167
1573.773754	141154.923730	36.517184
1575.339965	141392.110528	36.522202
1577.032718	141620.685970	36.527220
1578.521648	141853.592085	36.532237
1579.758711	142099.467859	36.537255
1581.764791	142313.004906	36.542272
1583.143373	142559.989919	36.547290
1584.606562	142789.041485	36.552308
1586.608882	143010.885893	36.557325
1588.208482	143256.903454	36.562343
1589.785030	143484.940866	36.567360
1591.512341	143732.462917	36.572378
1592.955538	143960.195458	36.577396
1594.899231	144185.746074	36.582413
1596.845996	144414.162463	36.587431
1598.864868	144636.763728	36.592448
1600.652018	144862.952534	36.597466
1602.197016	145079.243766	36.602484
1604.158839	145296.851930	36.607501
1605.660831	145511.720623	36.612519
1607.258971	145724.205126	36.617536
1608.526868	145943.753321	36.622554
1609.938616	146158.399917	36.627572
1611.852509	146362.852662	36.632589
1612.994251	146579.268957	36.637607
1614.261731	146782.724261	36.642624
1616.068729	146985.410646	36.647642
1617.230554	147200.737815	36.652660
1618.691599	147411.239855	36.657677
1620.203927	147636.262549	36.662695
1621.330627	147850.674286	36.667712
1622.836043	148077.501273	36.672730
1624.485425	148318.593856	36.677748
1626.185433	148542.819810	36.682765
1627.325212	148783.603833	36.687783
1629.146622	149027.045008	36.692800
1630.681045	149272.992990	36.697818
1632.399137	149514.185008	36.702836
1634.008068	149756.334289	36.707853
1635.835339	150004.130237	36.712871
1637.096966	150235.511614	36.717888
1638.922922	150491.602656	36.722906
1640.545233	150752.862575	36.727924
1642.506298	150991.237796	36.732941
1643.736170	151259.625691	36.737959
1645.746233	151493.001621	36.742976
1647.948766	151753.822348	36.747994
1649.061793	152003.686606	36.753012
1650.970379	152260.095240	36.758029
1652.135145	152517.600240	36.763047
1654.219749	152771.588625	36.768064
1656.043834	153027.167126	36.773082
1657.386809	153275.825291	36.778100
1659.604867	153525.905824	36.783117
1661.124509	153789.855863	36.788135
1662.960333	154035.905584	36.793152
1664.616185	154292.331907	36.798170
1666.156770	154550.198563	36.803188
1668.070956	154796.659801	36.808205
1669.680874	155050.499891	36.813223
1671.475137	155315.470623	36.818240
1673.237624	155567.553240	36.823258
1674.842338	155826.890240	36.828276
1676.734378	156070.967745	36.833293
1678.193822	156331.105106	36.838311
1679.805243	156583.498153	36.843328
1681.728641	156845.619890	36.848346
1683.291382	157103.908064	36.853364
1685.332717	157348.845859	36.858381
1686.668946	157627.551198	36.863399
1688.263888	157865.196206	36.868416
1690.161072	158129.842563	36.873434
1691.286647	158394.347173	36.878452
1693.465610	158644.128939	36.883469
1694.606662	158919.515180	36.888487
1696.409601	159185.617426	36.893504
1698.371774	159451.721759	36.898522
1699.892035	159715.488854	36.903540
1701.575645	159977.380508	36.908557
1702.789828	160241.821510	36.913575
1704.511583	160483.382614	36.918592
1706.170498	160740.401454	36.923610
1707.504037	160994.252680	36.928628
1709.436596	161240.046458	36.933645
1710.676464	161511.201412	36.938663
1712.277324	161767.792980	36.943680
1713.912104	162031.622409	36.948698
1715.592781	162310.728402	36.953716
1717.170463	162585.705825	36.958733
1719.028265	162862.086629	36.963751
1720.883697	163132.750154	36.968768
1722.847333	163395.370498	36.973786
1724.662407	163684.878006	36.978804
1726.532331	163950.548352	36.983821
1728.102061	164232.806609	36.988839
1729.882428	164508.933125	36.993856
1731.679317	164778.146874	36.998874
1733.644998	165059.131009	37.003892
1735.452165	165329.691536	37.008909
1737.073808	165613.905282	37.013927
1738.832123	165891.846609	37.018944
1740.258144	166166.380192	37.023962
1741.981025	166468.150897	37.028980
1744.243762	166743.266113	37.033997
1746.840528	166999.330108	37.039015
1748.992274	167268.771801	37.044032
1751.329754	167526.237705	37.049050
1753.303087	167779.894568	37.054068
1755.492672	168028.965213	37.059085
1757.131702	168279.139635	37.064103
1759.323327	168528.340057	37.069120
1760.976223	168766.313252	37.074138
1762.472980	169003.919498	37.079156
1764.193081	169238.041577	37.084173
1766.053054	169489.774360	37.089191
1768.113442	169733.498340	37.094208
1770.322759	169966.786081	37.099226
1771.605235	170204.928431	37.104244
1773.408574	170446.592030	37.109261
1774.560784	170692.559218	37.114279
1776.038373	170946.987923	37.119296
1777.871460	171204.177923	37.124314
1779.023169	171466.564542	37.129332
1780.747112	171721.415807	37.134349
1782.796364	171992.365497	37.139367
1784.302349	172258.189586	37.144384
1786.519346	172520.198398	37.149402
1787.805596	172796.551885	37.154420
1789.692442	173056.764543	37.159437
1791.453464	173335.507395	37.164455
1793.158384	173604.480298	37.169472
1794.944452	173872.173520	37.174490
1796.471440	174145.707160	37.179508
1798.696543	174395.142395	37.184525
1800.574906	174655.988343	37.189543
1802.013978	174899.398673	37.194560
1803.819977	175159.548904	37.199578
1805.505655	175411.778197	37.204596
1807.646604	175658.583064	37.209613
1809.283946	175904.276831	37.214631
1811.135940	176156.661904	37.219648
1813.156577	176398.745504	37.224666
1814.553471	176663.867267	37.229684
1816.408096	176930.478538	37.234701
1817.954755	177188.348347	37.239719
1819.458630	177463.658529	37.244736
1821.598567	177720.473217	37.249754
1823.072788	177997.732741	37.254772
1824.793106	178271.504078	37.259789
1826.215822	178550.120260	37.264807
1828.273268	178827.279951	37.269824
1830.620056	179119.074993	37.274842
1832.076130	179404.035247	37.279860
1834.179552	179680.317744	37.284877
1835.967259	179965.787348	37.289895
1837.711789	180251.823968	37.294912
1839.724213	180531.349101	37.299930
1841.761802	180828.330785	37.304948
1843.339873	181120.223382	37.309965
1845.399679	181410.468124	37.314983
1847.056820	181708.683524	37.320000
1849.145182	182001.934784	37.325018
1850.672983	182310.236689	37.330036
1852.619067	182603.235395	37.335053
1854.267458	182903.630020	37.340071
1856.158175	183211.334981	37.345088
1858.234434	183498.824718	37.350106
1860.239265	183815.956210	37.355124
1862.418679	184114.510937	37.360141
1864.017774	184404.924564	37.365159
1865.732376	184717.578488	37.370176
1867.838393	185011.405060	37.375194
1869.484894	185316.231975	37.380212
1871.404879	185619.900849	37.385229
1873.499536	185926.094599	37.390247
1875.173691	186234.704711	37.395264
1877.407328	186537.644633	37.400282
1878.822646	186844.662944	37.405300
1880.893144	187140.843699	37.410317
1882.653904	187446.351822	37.415335
1884.400951	187762.688679	37.420352
1886.398006	188067.922243	37.425370
1888.315509	188388.246318	37.430388
1890.220748	188705.351192	37.435405
1892.496767	189010.038958	37.440423
1894.106410	189331.281215	37.445440
1896.092257	189639.382022	37.450458
1897.887225	189949.583671	37.455476
1899.744448	190246.655305	37.460493
1901.889226	190552.566637	37.465511
1903.283213	190836.174413	37.470528
1905.060831	191119.139172	37.475546
1907.259349	191409.945231	37.480564
1909.542351	191682.058419	37.485581
1911.979306	191953.222234	37.490599
1914.067451	192229.138635	37.495616
1916.362953	192491.240989	37.500634
1918.413609	192767.877055	37.505652
1920.713755	193029.930753	37.510669
1922.703452	193293.519999	37.515687
1924.433870	193569.754447	37.520704
1926.185804	193821.543033	37.525722
1927.945884	194094.120481	37.530740
1929.645599	194370.783015	37.535757
1931.350700	194652.434071	37.540775
1933.052466	194933.554156	37.545792
1935.105669	195215.495752	37.550810
1937.230498	195506.984598	37.555828
1939.117937	195792.280970	37.560845
1940.803546	196078.689779	37.565863
1942.294642	196375.094417	37.570880
1944.585551	196668.048431	37.575898
1946.362879	196976.722565	37.580916
1947.956354	197279.233791	37.585933
1949.777795	197587.967974	37.590951
1951.719871	197901.317601	37.595968
1953.706402	198213.557762	37.600986
1955.714235	198529.794577	37.606004
1957.532691	198843.854769	37.611021
1959.403893	199158.606531	37.616039
1961.220032	199491.253221	37.621056
1963.174706	199811.402727	37.626074
1965.005894	200144.444509	37.631092
1967.110606	200478.447671	37.636109
1968.801139	200798.594100	37.641127
1970.913171	201137.220437	37.646144
1972.797081	201474.260289	37.651162
1974.594962	201814.895392	37.656180
1976.646649	202148.917030	37.661197
1978.896253	202480.446681	37.666215
1980.787403	202835.442352	37.671232
1983.104560	203167.803093	37.676250
1985.348877	203514.394450	37.681268
1987.021892	203842.113828	37.686285
1989.189685	204185.446343	37.691303
1991.388272	204519.661661	37.696320
1993.360288	204853.013570	37.701338
1995.341962	205198.019146	37.706356
1997.102880	205537.704786	37.711373
1999.289563	205877.680262	37.716391
2001.135046	206222.396079	37.721408
2003.170490	206559.225842	37.726426
2005.331033	206897.116688	37.731444
2007.275271	207236.668671	37.736461
2009.445221	207546.671505	37.741479
2011.198552	207865.057115	37.746496
2013.136541	208177.359639	37.751514
2014.950226	208497.478158	37.756532
2016.895424	208811.445793	37.761549
2019.187668	209137.610677	37.766567
2020.859670	209459.470480	37.771584
2023.081381	209790.766103	37.776602
2024.951673	210104.701351	37.781620
2026.765957	210434.808177	37.786637
2028.750573	210771.199295	37.791655
2030.580536	211107.007343	37.796672
2032.802942	211435.645393	37.801690
2034.728967	211784.099158	37.806708
2036.630476	212138.500247	37.811725
2038.680549	212471.576279	37.816743
2040.890790	212825.119576	37.821760
2042.839494	213159.408578	37.826778
2045.206930	213511.749892	37.831796
2047.334678	213869.222184	37.836813
2049.186913	214229.215824	37.841831
2051.322189	214578.514435	37.846848
2053.104821	214931.565381	37.851866
2054.880368	215288.517023	37.856884
2057.076435	215661.490026	37.861901
2059.185723	216024.753381	37.866919
2061.096981	216400.606837	37.871936
2063.017154	216763.624718	37.876954
2065.384365	217139.409786	37.881972
2067.297020	217502.673890	37.886989
2069.873249	217886.301662	37.892007
2071.986024	218257.752618	37.897024
2074.655093	218606.504150	37.902042
2077.045532	218974.943667	37.907060
2079.278914	219317.622418	37.912077
2081.971479	219671.644538	37.917095
2083.774157	220028.780644	37.922112
2085.622207	220432.865312	37.927130
2087.648824	220783.366965	37.932148
2089.652252	221140.298737	37.937165
2092.153701	221504.784267	37.942183
2094.268537	221864.330090	37.947200
2096.305457	222216.322268	37.952218
2098.689653	222564.858013	37.957236
2100.617553	222918.965742	37.962253
2102.981139	223267.596757	37.967271
2104.862011	223619.912020	37.972288
2106.698007	223973.366052	37.977306
2108.805629	224335.476527	37.982324
2110.800709	224689.962371	37.987341
2113.452138	225041.082275	37.992359
2115.890763	225392.072364	37.997376
2118.088652	225725.832848	38.002394
2120.133978	226081.332539	38.007412
2122.012926	226434.472883	38.012429
2123.725992	226754.473426	38.017447
2125.161337	227091.966558	38.022464
2127.432220	227422.319038	38.027482
2129.388485	227752.290948	38.032500
2131.579124	228098.658596	38.037517
2133.641141	228425.467083	38.042535
2135.606074	228768.723970	38.047552
2137.583094	229119.980316	38.052570
2139.670172	229469.011035	38.057588
2141.745828	229822.895777	38.062605
2144.337635	230175.303171	38.067623
2146.090498	230521.800415	38.072640
2148.040471	230886.782457	38.077658
2150.598298	231240.215198	38.082676
2153.206344	231587.063307	38.087693
2155.738975	231923.790940	38.092711
2158.190594	232273.256936	38.097728
2160.578534	232617.324540	38.102746
2162.811396	232956.236762	38.107764
2164.223515	233313.389200	38.112781
2166.477220	233663.983694	38.117799
2168.192644	234027.668733	38.122816
2170.147938	234404.524209	38.127834
2172.522602	234758.430526	38.132852
2174.397779	235150.438968	38.137869
2176.735174	235518.399230	38.142887
2178.527431	235899.146638	38.147904
2180.777392	236272.711145	38.152922
2182.892454	236662.426691	38.157940
2184.805830	237053.115404	38.162957
2187.400649	237435.493521	38.167975
2189.414847	237837.446263	38.172992
2191.223429	238228.790760	38.178010
2193.447432	238622.026489	38.183028
2195.663632	239030.275918	38.188045
2198.023244	239414.628452	38.193063
2200.007915	239820.301243	38.198080
2202.510639	240213.193399	38.203098
2205.066534	240620.708729	38.208116
2207.190036	241020.191445	38.213133
2209.567159	241425.909052	38.218151
2211.861364	241825.926130	38.223168
2214.209738	242217.147445	38.228186
2216.636918	242609.805293	38.233204
2218.706500	243005.569100	38.238221
2221.259457	243409.918998	38.243239
2222.961681	243808.588355	38.248256
2225.539520	244201.658930	38.253274
2227.775624	244602.557443	38.258292
2230.041016	245010.463087	38.263309
2232.357272	245401.444957	38.268327
2234.873421	245800.041875	38.273344
2236.839232	246200.810066	38.278362
2239.269185	246604.350680	38.283380
2241.030738	246988.007778	38.288397
2243.519308	247356.690928	38.293415
2245.317808	247742.045986	38.298432
2247.303484	248108.600821	38.303450
2249.711457	248481.922512	38.308468
2251.403909	248870.370767	38.313485
2253.500469	249248.087293	38.318503
2255.254940	249651.565255	38.323520
2257.327478	250042.623221	38.328538
2259.648327	250438.088013	38.333556
2261.721989	250856.352823	38.338573
2264.056573	251279.962443	38.343591
2265.793912	251695.869445	38.348608
2268.510902	252114.238464	38.353626
2271.062579	252529.637238	38.358644
2272.791183	252962.694815	38.363661
2275.286661	253391.389647	38.368679
2278.018123	253808.185244	38.373696
2279.724421	254251.410090	38.378714
2282.007503	254685.348863	38.383732
2284.134811	255128.737488	38.388749
2286.729932	255561.460116	38.393767
2288.773899	256009.791844	38.398784
2291.073467	256465.349045	38.403802
2293.755789	256883.885918	38.408820
2296.192416	257344.808466	38.413837
2298.507633	257784.387624	38.418855
2300.878361	258234.475449	38.423872
2303.341687	258668.317122	38.428890
2305.968241	259109.144789	38.433908
2308.687947	259559.205014	38.438925
2310.859800	259996.575262	38.443943
2313.286751	260436.369821	38.448960
2315.589823	260878.572559	38.453978
2318.217907	261314.983375	38.458996
2320.248000	261767.010800	38.464013
2322.624442	262205.342574	38.469031
2325.391392	262648.896836	38.474048
2327.685839	263085.108912	38.479066
2330.318083	263525.637292	38.484084
2332.346924	263967.354196	38.489101
2334.813070	264403.540612	38.494119
2337.508516	264835.601248	38.499136
2339.904117	265270.478813	38.504154
2342.433084	265687.502639	38.509172
2345.174051	266127.889579	38.514189
2347.496042	266541.111097	38.519207
2349.992508	266961.265780	38.524224
2352.513927	267387.539023	38.529242
2355.449793	267791.671438	38.534260
2357.771421	268204.487817	38.539277
2360.036092	268605.323133	38.544295
2362.276341	269035.706620	38.549312
2364.591932	269448.473904	38.554330
2367.417919	269849.754388	38.559348
2369.656153	270254.583094	38.564365
2372.119103	270635.370166	38.569383
2374.239002	271012.883922	38.574400
2375.848084	271395.076793	38.579418
2377.990330	271780.182860	38.584436
2380.027766	272186.314256	38.589453
2382.044803	272567.020175	38.594471
2384.477063	272976.518617	38.599488
2386.397499	273387.165206	38.604506
2388.911365	273804.729117	38.609524
2390.760145	274215.031501	38.614541
2393.119532	274642.476477	38.619559
2395.130781	275072.389962	38.624576
2397.097151	275513.335622	38.629594
2399.583669	275965.782742	38.634612
2401.628321	276417.944190	38.639629
2404.027403	276871.421147	38.644647
2405.970840	277337.316267	38.649664
2408.252266	277816.291214	38.654682
2410.558343	278291.197534	38.659700
2412.837289	278782.213682	38.664717
2415.012436	279263.872201	38.669735
2418.187884	279752.230799	38.674752
2421.067497	280245.233991	38.679770
2423.654307	280717.579570	38.684788
2426.225025	281204.991511	38.689805
2428.965653	281685.745887	38.694823
2431.453899	282162.907202	38.699840
2433.602715	282652.391650	38.704858
2436.318656	283131.319621	38.709876
2438.645007	283620.216097	38.714893
2441.206321	284099.802661	38.719911
2443.319710	284590.586244	38.724928
2445.697778	285092.225206	38.729946
2448.464600	285574.089147	38.734964
2450.434255	286085.393880	38.739981
2452.998909	286589.770176	38.744999
2455.530050	287104.261402	38.750016
2457.559568	287617.205536	38.755034
2460.593422	288119.930126	38.760052
2463.264223	288627.436342	38.765069
2465.478395	289139.789763	38.770087
2467.950464	289652.660235	38.775104
2470.506060	290161.934724	38.780122
2473.291340	290655.574620	38.785140
2475.992939	291165.128825	38.790157
2479.009209	291656.951961	38.795175
2481.978500	292155.487781	38.800192
2484.325130	292645.128764	38.805210
2486.997386	293138.070192	38.810228
2489.395760	293632.857483	38.815245
2491.968571	294111.104542	38.820263
2494.999475	294597.660626	38.825280
2497.861104	295075.554858	38.830298
2500.344651	295552.618789	38.835316
2502.912810	296011.302508	38.840333
2505.315104	296457.996298	38.845351
2508.090760	296885.908677	38.850368
2510.194074	297332.342914	38.855386
2513.128330	297757.179889	38.860404
2515.352944	298199.325236	38.865421
2517.410896	298626.254894	38.870439
2519.601655	299063.373859	38.875456
2521.673693	299520.501458	38.880474
2524.320195	299970.932384	38.885492
2526.514012	300443.126525	38.890509
2528.714918	300905.894264	38.895527
2531.455500	301367.686064	38.900544
2533.299087	301842.598570	38.905562
2535.708889	302328.393090	38.910580
2537.852612	302829.138519	38.915597
2539.976039	303323.687624	38.920615
2542.453574	303831.895305	38.925632
2544.859531	304348.266091	38.930650
2547.366921	304868.479747	38.935668
2549.435257	305398.463944	38.940685
2551.870793	305923.561768	38.945703
2554.223915	306466.958720	38.950720
2556.753417	307021.730084	38.955738
2559.484625	307568.339034	38.960756
2562.303523	308117.065269	38.965773
2565.051546	308659.094715	38.970791
2568.106834	309201.200023	38.975808
2570.292671	309763.277664	38.980826
2573.306543	310306.222602	38.985844
2575.667489	310866.031966	38.990861
2578.232707	311420.726342	38.995879
2581.590337	311967.063094	39.000896
2584.281596	312515.458412	39.005914
2586.928500	313064.010357	39.010932
2589.823766	313619.123774	39.015949
2592.525300	314162.276827	39.020967
2595.672235	314697.736931	39.025984
2598.301289	315237.949552	39.031002
2601.015476	315781.676120	39.036020
2603.635053	316311.953756	39.041037
2606.429714	316851.293213	39.046055
2609.247168	317378.790713	39.051072
2611.546436	317916.424831	39.056090
2614.407299	318456.786024	39.061108
2616.844744	318992.334883	39.066125
2619.237015	319526.109979	39.071143
2621.710275	320072.821569	39.076160
2624.228063	320611.776742	39.081178
2626.924486	321155.703485	39.086196
2629.122824	321704.937441	39.091213
2631.886381	322262.814717	39.096231
2634.670601	322801.409382	39.101248
2637.059110	323355.250129	39.106266
2640.002167	323911.996071	39.111284
2642.349404	324456.972874	39.116301
2644.906753	324989.392777	39.121319
2647.889925	325503.228515	39.126336
2650.599773	326008.800030	39.131354
2653.537710	326512.910073	39.136372
2656.305887	327020.700634	39.141389
2658.859947	327524.026940	39.146407
2661.862836	328019.178006	39.151424
2664.400575	328540.504951	39.156442
2667.104821	329050.730063	39.161460
2669.613166	329560.881156	39.166477
2671.548679	330080.718352	39.171495
2674.732894	330610.536931	39.176512
2676.614283	331137.790137	39.181530
2679.275201	331666.363431	39.186548
2681.892640	332209.413765	39.191565
2684.558959	332762.634740	39.196583
2687.492246	333297.018474	39.201600
2689.927832	333855.269699	39.206618
2692.628863	334408.294327	39.211636
2695.271611	334963.685165	39.216653
2697.926587	335524.503361	39.221671
2700.608326	336080.031158	39.226688
2703.201376	336653.215398	39.231706
2705.916284	337218.961105	39.236724
2708.849885	337793.858799	39.241741
2711.005098	338375.628600	39.246759
2714.033104	338941.461963	39.251776
2716.666073	339535.637635	39.256794
2719.421793	340115.392084	39.261812
2721.999421	340701.897642	39.266829
2724.693162	341294.091890	39.271847
2727.735659	341896.914071	39.276864
2730.503065	342503.328294	39.281882
2733.110702	343090.593145	39.286900
2735.855970	343696.821049	39.291917
2738.064361	344305.590420	39.296935
2740.985147	344898.601604	39.301952
2744.284389	345506.322470	39.306970
2747.162454	346107.122055	39.311988
2750.363773	346710.174354	39.317005
2752.885368	347310.992269	39.322023
2756.012088	347906.046682	39.327040
2758.262497	348513.317441	39.332058
2760.862825	349122.023883	39.337076
2763.780814	349726.408424	39.342093
2766.551889	350339.237506	39.347111
2769.458905	350939.726226	39.352128
2772.064911	351555.918399	39.357146
2775.122894	352167.284893	39.362164
2777.873961	352775.646752	39.367181
2780.512533	353390.543040	39.372199
2783.969524	353992.788206	39.377216
2786.622972	354595.407389	39.382234
2789.650058	355207.022079	39.387252
2792.842742	355794.717847	39.392269
2795.469400	356372.241796	39.397287
2798.407288	356930.799945	39.402304
2800.839269	357484.203203	39.407322
2803.252289	358053.213009	39.412340
2805.856327	358620.739195	39.417357
2808.654653	359196.299180	39.422375
2811.294419	359763.298672	39.427392
2813.672288	360343.784600	39.432410
2816.319731	360926.352692	39.437428
2819.066646	361522.983689	39.442445
2821.241258	362131.956047	39.447463
2824.090702	362728.682309	39.452480
2826.537170	363345.184089	39.457498
2829.277187	363970.234442	39.462516
2831.957597	364602.087024	39.467533
2834.654132	365238.521623	39.472551
2837.424748	365886.025442	39.477568
2840.301314	366529.011343	39.482586
2843.155787	367171.001720	39.487604
2846.083760	367806.728507	39.492621
2848.693545	368470.105510	39.497639
2851.800080	369129.739636	39.502656
2854.545810	369797.337856	39.507674
2857.861698	370466.332502	39.512692
2860.466483	371143.980375	39.517709
2863.501698	371798.966355	39.522727
2867.045222	372451.045148	39.527744
2869.998795	373127.489285	39.532762
2872.403569	373802.360006	39.537780
2875.149774	374472.497064	39.542797
2877.962684	375151.086779	39.547815
2881.301176	375825.192642	39.552832
2884.436613	376508.376834	39.557850
2887.001536	377183.191237	39.562868
2889.956233	377871.911454	39.567885
2892.495057	378559.416988	39.572903
2895.395558	379248.705159	39.577920
2898.408157	379939.333290	39.582938
2901.571059	380636.952337	39.587956
2905.018981	381321.753503	39.592973
2907.583574	382012.237693	39.597991
2910.902773	382686.025168	39.603008
2913.617137	383388.814237	39.608026
2916.719423	384083.284716	39.613044
2919.934994	384767.273649	39.618061
2922.905234	385459.507064	39.623079
2926.078090	386139.900775	39.628096
2929.414436	386819.317442	39.633114
2932.069394	387499.539423	39.638132
2935.504128	388172.320516	39.643149
2938.171020	388862.355753	39.648167
2941.068896	389526.522250	39.653184
2943.701878	390210.880857	39.658202
2946.563799	390890.726327	39.663220
2949.635557	391555.384958	39.668237
2953.010423	392196.321701	39.673255
2956.800980	392818.541245	39.678272
2960.039637	393423.896777	39.683290
2963.186860	394032.628823	39.688308
2966.703128	394624.123830	39.693325
2969.473023	395227.771751	39.698343
2972.254693	395830.037686	39.703360
2975.287006	396434.002783	39.708378
2977.558538	397046.673299	39.713396
2980.446661	397656.597871	39.718413
2982.746706	398291.047242	39.723431
2985.653968	398914.333355	39.728448
2988.988947	399549.253815	39.733466
2990.975105	400190.029375	39.738484
2993.991710	400823.555455	39.743501
2996.617990	401478.351558	39.748519
2999.790035	402130.867565	39.753536
3002.894587	402800.797888	39.758554
3005.703212	403462.242717	39.763572
3008.655497	404140.915085	39.768589
3011.096660	404821.757766	39.773607
3014.105578	405504.219546	39.778624
3016.920060	406211.970533	39.783642
3019.409765	406919.629954	39.788660
3022.808875	407619.347218	39.793677
3025.592399	408343.479688	39.798695
3028.433585	409055.267077	39.803712
3031.426495	409795.401778	39.808730
3034.024981	410525.087479	39.813748
3037.044449	411259.833833	39.818765
3039.955871	412018.631166	39.823783
3043.136548	412759.321513	39.828800
3046.452588	413505.978146	39.833818
3049.355444	414276.858000	39.838836
3052.793838	415034.226761	39.843853
3055.373307	415795.360758	39.848871
3058.325181	416565.994449	39.853888
3061.285719	417346.285872	39.858906
3064.504122	418123.905144	39.863924
3067.580005	418896.559236	39.868941
3070.638866	419680.014071	39.873959
3074.158532	420458.788033	39.878976
3077.449102	421244.746664	39.883994
3080.112895	422027.615192	39.889012
3083.452223	422799.789878	39.894029
3087.168996	423577.152598	39.899047
3090.032530	424361.949539	39.904064
3093.119847	425146.029690	39.909082
3096.321681	425929.942255	39.914100
3100.023417	426698.579330	39.919117
3102.730528	427494.734012	39.924135
3105.993478	428264.560478	39.929152
3109.199396	429036.526493	39.934170
3112.332156	429821.829442	39.939188
3115.712682	430572.041510	39.944205
3118.680882	431316.522640	39.949223
3122.307535	432040.591906	39.954240
3125.185905	432765.189740	39.959258
3127.966788	433493.327985	39.964276
3131.190518	434222.844186	39.969293
3133.920147	434953.253275	39.974311
3137.124274	435676.805070	39.979328
3140.622323	436401.884838	39.984346
3143.432706	437142.599568	39.989364
3147.150939	437873.349699	39.994381
3149.854824	438611.201680	39.999399
3153.030742	439356.096865	40.004416
3156.082492	440106.508474	40.009434
3158.967443	440850.138441	40.014452
3162.080120	441603.633766	40.019469
3164.716900	442387.610446	40.024487
3167.622624	443146.102999	40.029504
3170.986003	443927.231257	40.034522
3173.508943	444723.300515	40.039540
3176.648197	445517.170050	40.044557
3179.738733	446309.350139	40.049575
3183.011489	447122.432025	40.054592
3186.037993	447935.625942	40.059610
3189.195725	448753.073307	40.064628
3192.401571	449572.762042	40.069645
3195.396177	450406.930809	40.074663
3198.653551	451238.952691	40.079680
3201.894079	452077.728837	40.084698
3204.952010	452934.216023	40.089716
3208.096319	453774.058242	40.094733
3211.371375	454623.969512	40.099751
3214.664603	455483.055494	40.104768
3218.036368	456341.185248	40.109786
3220.980117	457206.787670	40.114804
3224.682148	458072.337532	40.119821
3227.263537	458943.747899	40.124839
3230.501814	459821.849810	40.129856
3233.708941	460692.433891	40.134874
3236.720229	461575.509520	40.139892
3239.774056	462478.119437	40.144909
3243.091982	463368.509429	40.149927
3246.193963	464273.464322	40.154944
3249.997778	465175.841937	40.159962
3253.221121	466096.481105	40.164980
3256.857167	466976.554073	40.169997
3260.126956	467871.263950	40.175015
3263.683159	468772.363423	40.180032
3267.651605	469657.631563	40.185050
3270.887879	470549.349146	40.190068
3274.663882	471420.666171	40.195085
3278.356392	472296.307828	40.200103
3281.823300	473160.723118	40.205120
3284.870881	474037.757112	40.210138
3287.980410	474905.895934	40.215156
3291.576018	475763.101867	40.220173
3294.756740	476594.302388	40.225191
3297.397876	477431.316396	40.230208
3300.456406	478244.774897	40.235226
3303.402243	479075.807844	40.240244
3306.444964	479914.725867	40.245261
3309.515033	480764.065884	40.250279
3312.786227	481600.904537	40.255296
3316.082342	482455.644054	40.260314
3319.219808	483309.259250	40.265332
3322.998482	484160.612975	40.270349
3326.762429	485003.543293	40.275367
3330.336538	485863.595664	40.280384
3333.845332	486711.089152	40.285402
3336.511692	487576.917155	40.290420
3339.766642	488434.478541	40.295437
3343.166974	489303.496300	40.300455
3345.896627	490175.055210	40.305472
3349.435777	491058.366901	40.310490
3352.197352	491967.621760	40.315508
3355.349486	492852.273184	40.320525
3358.407522	493770.130732	40.325543
3361.671076	494696.394709	40.330560
3364.986049	495616.846470	40.335578
3368.188214	496561.307256	40.340596
3371.633777	497489.319483	40.345613
3375.327805	498416.588337	40.350631
3378.814553	499362.372536	40.355648
3382.340874	500305.172195	40.360666
3385.939884	501240.892956	40.365684
3389.505127	502194.491373	40.370701
3392.699903	503139.212339	40.375719
3395.870784	504102.916595	40.380736
3399.448444	505057.115190	40.385754
3403.889869	506012.437350	40.390772
3406.893442	506952.642013	40.395789
3410.557845	507902.834993	40.400807
3414.155778	508839.007536	40.405824
3417.954807	509792.355025	40.410842
3421.280455	510746.481062	40.415860
3424.752352	511697.957266	40.420877
3428.300189	512639.983828	40.425895
3431.874061	513588.512225	40.430912
3435.406194	514542.038434	40.435930
3438.706721	515484.802319	40.440948
3442.060588	516436.886599	40.445965
3445.305384	517396.499338	40.450983
3448.217747	518353.133265	40.456000
3452.270117	519319.063220	40.461018
3455.164442	520286.884407	40.466036
3458.170786	521254.681004	40.471053
3461.707456	522215.529028	40.476071
3464.906352	523207.029262	40.481088
3468.556627	524188.717085	40.486106
3472.069092	525174.097419	40.491124
3475.429627	526146.418103	40.496128
3478.559735	527069.268389	40.501133
3482.323615	527946.180605	40.506138
3485.543684	528744.098261	40.511143
3488.386503	529500.348304	40.516148
3491.289827	530180.862498	40.521152
3494.617581	530803.327512	40.526157
3497.094851	531355.927086	40.531162
3500.192544	531846.772241	40.536167
3502.333917	532279.502873	40.541172
3504.417863	532649.182391	40.546176
3506.581154	532953.166699	40.551181
3508.217081	533216.309192	40.556186
3510.039798	533432.740146	40.561191
3511.693654	533592.768069	40.566196
3512.915946	533713.712710	40.571200
3514.181438	533792.974161	40.576205
3515.438883	533842.634387	40.581210
3516.781404	533844.493367	40.586215
3517.585852	533829.565190	40.591220
3518.263518	533768.233087	40.596224
3518.861034	533688.980220	40.601229
3519.634538	533577.469687	40.606234
3520.644396	533450.563887	40.611239
3520.676497	533310.727616	40.616244
3520.909816	533142.214691	40.621248
3521.646167	532964.426080	40.626253
3521.896707	532771.404958	40.631258
3522.285403	532558.151720	40.636263
3522.221516	532323.344332	40.641268
3522.602872	532089.220848	40.646272
3522.757749	531843.812708	40.651277
3522.458272	531609.941202	40.656282
3522.934550	531345.073648	40.661287
3522.643928	531087.648874	40.666292
3522.676617	530812.939613	40.671296
3522.822937	530534.569682	40.676301
3522.618793	530262.363989	40.681306
3522.332820	529983.648390	40.686311
3522.529421	529702.577770	40.691316
3522.552997	529416.021720	40.696320
3522.210973	529138.613784	40.701325
3522.172935	528853.876357	40.706330
3522.266667	528566.182078	40.711335
3521.512771	528282.204413	40.716340
3521.154136	527997.350625	40.721344
3521.650278	527711.244832	40.726349
3521.063311	527436.928405	40.731354
3521.092842	527152.756135	40.736359
3520.892256	526874.224875	40.741364
3520.766632	526588.854141	40.746368
3520.367354	526316.813512	40.751373
3520.162009	526053.733818	40.756378
3520.282252	525775.284266	40.761383
3519.880113	525505.049749	40.766388
3519.726395	525224.561676	40.771392
3519.586939	524958.572589	40.776397
3519.473548	524694.900035	40.781402
3519.119953	524433.788404	40.786407
3519.047427	524174.397233	40.791412
3518.563188	523919.616214	40.796416
3518.298322	523668.183215	40.801421
3518.175471	523417.583179	40.806426
3517.964026	523163.758075	40.811431
3517.438695	522923.425020	40.816436
3517.241205	522699.769010	40.821440
3517.353743	522445.982535	40.826445
3517.034082	522219.306086	40.831450
3516.777186	521984.629117	40.836455
3516.412488	521760.632706	40.841460
3516.313477	521530.929079	40.846464
3515.961237	521307.379448	40.851469
3515.587394	521111.181027	40.856474
3515.637493	520890.241550	40.861479
3515.708661	520682.036224	40.866484
3515.268122	520475.729215	40.871488
3515.262726	520270.463112	40.876493
3514.765783	520076.142378	40.881498
3514.905441	519866.146261	40.886503
3514.333170	519688.416482	40.891508
3514.072171	519493.545937	40.896512
3513.902815	519300.124881	40.901517
3513.930102	519124.518939	40.906522
3514.094063	518940.091596	40.911527
3513.869608	518753.195411	40.916532
3513.614653	518580.207001	40.921536
3513.569852	518394.744703	40.926541
3513.375327	518223.310493	40.931546
3513.148905	518041.614740	40.936551
3512.701918	517885.639410	40.941556
3512.513043	517708.181598	40.946560
3512.742675	517550.933131	40.951565
3512.448515	517395.232419	40.956570
3512.775164	517232.554868	40.961575
3512.478767	517071.693529	40.966580
3511.914465	516909.153627	40.971584
3511.934035	516769.630091	40.976589
3511.781945	516616.883208	40.981594
3511.804636	516458.696264	40.986599
3511.595613	516311.771167	40.991604
3511.241767	516178.420758	40.996608
3511.381864	516029.516279	41.001613
3511.083957	515887.102360	41.006618
3510.784357	515753.588257	41.011623
3510.653754	515630.363247	41.016628
3510.516553	515493.382434	41.021632
3510.332352	515375.676503	41.026637
3510.376539	515254.595758	41.031642
3510.186976	515121.261499	41.036647
3509.760455	515008.092404	41.041652
3509.941758	514893.663241	41.046656
3510.040576	514774.997994	41.051661
3509.637040	514658.990677	41.056666
3509.507865	514541.523056	41.061671
3509.453249	514436.181193	41.066676
3509.517245	514325.307045	41.071680
3509.606496	514223.987256	41.076685
3509.139686	514108.845943	41.081690
3509.483019	513998.785303	41.086695
3509.152084	513902.941819	41.091700
3508.929939	513796.813174	41.096704
3508.968381	513690.136881	41.101709
3508.714991	513598.730335	41.106714
3508.740278	513496.151793	41.111719
3508.732085	513406.930938	41.116724
3508.333259	513310.083214	41.121728
3508.503818	513220.479058	41.126733
3508.490306	513136.467368	41.131738
3508.277141	513033.519056	41.136743
3508.068915	512955.708090	41.141748
3507.940540	512862.052223	41.146752
3508.142109	512776.133237	41.151757
3507.688022	512703.165209	41.156762
3507.828176	512624.791834	41.161767
3508.002741	512541.152109	41.166772
3508.029930	512467.044762	41.171776
3507.895148	512391.647544	41.176781
3507.504822	512306.629051	41.181786
3507.990117	512218.032071	41.186791
3507.752247	512141.436037	41.191796
3507.554333	512062.253575	41.196800
3507.389811	511993.283403	41.201805
3507.320993	511917.064303	41.206810
3507.160397	511844.046177	41.211815
3507.365590	511789.686173	41.216820
3507.088215	511705.810251	41.221824
3507.097190	511634.281960	41.226829
3506.734858	511581.275616	41.231834
3507.217693	511499.251329	41.236839
3506.763805	511454.807977	41.241844
3506.822706	511383.321322	41.246848
3507.223930	511320.126924	41.251853
3506.761006	511254.539580	41.256858
3506.883234	511180.209243	41.261863
3506.602851	511117.678279	41.266868
3506.829822	511067.055918	41.271872
3506.587959	511011.398250	41.276877
3506.316385	510952.305185	41.281882
3506.435807	510888.243161	41.286887
3506.497406	510852.569498	41.291892
3506.525636	510785.435680	41.296896
3506.422994	510724.999851	41.301901
3506.313808	510667.195406	41.306906
3506.110674	510617.145570	41.311911
3506.271867	510574.980327	41.316916
3505.917211	510517.315350	41.321920
3506.083763	510466.397225	41.326925
3506.024049	510414.705297	41.331930
3506.127682	510371.081581	41.336935
3506.147148	510325.143973	41.341940
3505.778903	510280.785192	41.346944
3506.105820	510233.584606	41.351949
3506.113908	510182.083612	41.356954
3505.994616	510132.626173	41.361959
3505.640005	510092.311896	41.366964
3505.681523	510041.462858	41.371968
3505.552120	509997.824434	41.376973
3505.365985	509969.523597	41.381978
3505.881460	509910.555465	41.386983
3505.828239	509886.078323	41.391988
3505.414531	509835.553578	41.396992
3505.715424	509793.263144	41.401997
3505.781714	509755.866375	41.407002
3505.523066	509714.878363	41.412007
3505.465549	509675.376182	41.417012
3505.585811	509629.673726	41.422016
3505.546622	509606.104601	41.427021
3505.379185	509571.324509	41.432026
3505.269647	509516.905826	41.437031
3505.412071	509500.643569	41.442036
3505.286779	509461.859886	41.447040
3505.491521	509414.828128	41.452045
3505.462783	509374.157099	41.457050
3505.150708	509339.702950	41.462055
3505.066279	509319.125491	41.467060
3505.175165	509276.408806	41.472064
3505.565016	509246.902708	41.477069
3505.158233	509211.856168	41.482074
3505.498118	509173.504225	41.487079
3505.333848	509136.142547	41.492084
3505.211925	509103.023857	41.497088
3505.294010	509066.078418	41.502093
3505.199943	509030.020818	41.507098
3505.281319	508985.284052	41.512103
3505.019951	508963.621094	41.517108
3505.277804	508925.736899	41.522112
3504.886234	508902.475470	41.527117
3504.851390	508874.857212	41.532122
3505.176319	508839.846032	41.537127
3505.196657	508802.403854	41.542132
3504.834268	508787.181989	41.547136
3504.726086	508748.444581	41.552141
3504.770873	508729.060233	41.557146
3504.938375	508690.633273	41.562151
3504.385537	508675.795567	41.567156
3504.761369	508650.742906	41.572160
3504.937850	508602.195578	41.577165
3504.748147	508598.936996	41.582170
3504.996506	508565.303396	41.587175
3504.758370	508538.526234	41.592180
3504.839662	508510.383093	41.597184
3504.688774	508491.383566	41.602189
3504.735952	508462.992768	41.607194
3505.107240	508423.925870	41.612199
3505.070580	508412.042010	41.617204
3504.917206	508373.057928	41.622208
3505.042033	508351.788504	41.627213
3504.655884	508329.183171	41.632218
3505.159888	508290.752725	41.637223
3504.928115	508272.069309	41.642228
3504.622429	508235.537543	41.647232
3504.688450	508230.214671	41.652237
3504.589563	508187.528122	41.657242
3504.765159	508166.604611	41.662247
3504.654972	508146.738152	41.667252
3504.505812	508123.538541	41.672256
3504.632551	508099.688145	41.677261
3504.186746	508085.136581	41.682266
3504.646217	508054.959697	41.687271
3504.531435	508046.174258	41.692276
3504.269475	508023.194724	41.697280
3504.429455	508005.663390	41.702285
3504.359683	507982.198062	41.707290
3504.803512	507953.237770	41.712295
3504.907644	507939.256902	41.717300
3504.735542	507909.331382	41.722304
3504.348994	507886.067783	41.727309
3504.233854	507862.305887	41.732314
3504.603181	507846.157990	41.737319
3504.466986	507829.280446	41.742324
3504.583772	507792.326788	41.747328
3504.638579	507776.127349	41.752333
3504.626019	507757.813495	41.757338
3504.944668	507731.048262	41.762343
3504.672108	507710.195036	41.767348
3504.422653	507673.653191	41.772352
3504.717818	507659.034741	41.777357
3504.476788	507638.227041	41.782362
3504.507397	507611.507152	41.787367
3504.414583	507597.304153	41.792372
3504.651250	507570.298646	41.797376
3504.459189	507555.099362	41.802381
3504.181663	507550.640135	41.807386
3504.292170	507524.464048	41.812391
3504.177095	507505.356579	41.817396
3504.262429	507490.720556	41.822400
3504.461498	507473.182504	41.827405
3504.119490	507467.620310	41.832410
3504.285301	507435.869653	41.837415
3504.055499	507421.485774	41.842420
3504.033038	507410.256744	41.847424
3503.882856	507384.172249	41.852429
3503.526220	507381.142212	41.857434
3504.014987	507370.540713	41.862439
3504.179556	507369.806371	41.867444
3504.072778	507354.593430	41.872448
3504.493529	507333.680757	41.877453
3504.320700	507311.192162	41.882458
3504.351227	507295.046707	41.887463
3504.149538	507292.852323	41.892468
3504.068366	507264.176254	41.897472
3504.280752	507254.326741	41.902477
3504.089772	507241.606304	41.907482
3504.356062	507223.551394	41.912487
3504.486017	507214.777445	41.917492
3504.257196	507184.657242	41.922496
3504.311301	507168.254952	41.927501
3504.323782	507158.234590	41.932506
3504.548332	507129.003992	41.937511
3504.176152	507117.222872	41.942516
3504.377220	507091.588398	41.947520
3504.170400	507082.918212	41.952525
3504.067166	507066.135908	41.957530
3504.449191	507039.612581	41.962535
3503.845514	507041.327188	41.967540
3504.406181	507024.389305	41.972544
3504.404140	507005.971796	41.977549
3504.026735	506994.191418	41.982554
3504.091994	506959.622261	41.987559
3504.129673	506956.074431	41.992564
3504.131098	506943.171566	41.997568
3504.095670	506914.538286	42.002573
3504.248311	506928.074676	42.007578
3504.334443	506897.347603	42.012583
3504.484097	506889.126962	42.017588
3504.138128	506865.501380	42.022592
3504.360484	506850.994955	42.027597
3504.170838	506842.271335	42.032602
3504.202216	506824.202543	42.037607
3503.881600	506822.330492	42.042612
3504.171392	506793.999800	42.047616
3504.224942	506774.004682	42.052621
3503.975130	506775.056189	42.057626
3504.396891	506752.928277	42.062631
3504.022040	506745.195269	42.067636
3503.989350	506729.514674	42.072640
3504.347280	506724.296996	42.077645
3504.074761	506698.635600	42.082650
3503.888331	506686.622427	42.087655
3503.731639	506690.037397	42.092660
3504.130023	506660.576134	42.097664
3503.987621	506647.088588	42.102669
3503.836533	506654.044650	42.107674
3503.875287	506636.834690	42.112679
3503.994019	506616.879688	42.117684
3503.993373	506605.849087	42.122688
3503.659395	506602.056333	42.127693
3503.982268	506597.704355	42.132698
3503.979087	506575.946984	42.137703
3503.693475	506568.857589	42.142708
3503.744110	506571.329013	42.147712
3504.037574	506564.350483	42.152717
3503.523624	506548.239797	42.157722
3504.034142	506534.446558	42.162727
3503.879159	506523.237900	42.167732
3504.095144	506518.700398	42.172736
3503.696484	506503.026845	42.177741
3503.535545	506497.992316	42.182746
3503.666413	506482.133843	42.187751
3503.906993	506483.715054	42.192756
3503.906849	506473.190291	42.197760
3504.300981	506448.586952	42.202765
3503.855016	506445.368467	42.207770
3503.798841	506430.753918	42.212775
3503.973982	506425.716845	42.217780
3503.794404	506398.572906	42.222784
3504.057995	506411.839160	42.227789
3503.883371	506398.407113	42.232794
3504.014774	506373.187392	42.237799
3503.891104	506372.802172	42.242804
3503.504058	506366.133531	42.247808
3504.184001	506348.973736	42.252813
3503.830828	506346.398372	42.257818
3504.000577	506314.695641	42.262823
3504.064050	506321.466120	42.267828
3503.869493	506298.018232	42.272832
3504.355620	506281.597416	42.277837
3504.093686	506274.099352	42.282842
3504.089507	506257.654813	42.287847
3503.987961	506257.316695	42.292852
3503.936604	506255.351418	42.297856
3504.205393	506245.543019	42.302861
3504.038927	506211.515008	42.307866
3503.994991	506204.640267	42.312871
3503.956348	506198.928508	42.317876
3504.169198	506176.023269	42.322880
3503.778462	506175.579057	42.327885
3503.653888	506174.030153	42.332890
3503.819233	506134.434033	42.337895
3503.689768	506132.379887	42.342900
3503.662278	506125.603718	42.347904
3504.136093	506123.403611	42.352909
3503.619062	506121.461326	42.357914
3503.672130	506104.096773	42.362919
3503.873679	506094.197715	42.367924
3503.882923	506092.880657	42.372928
3503.971698	506091.399224	42.377933
3503.884963	506066.719552	42.382938
3503.889039	506053.916809	42.387943
3503.802107	506051.704126	42.392948
3503.704610	506054.097836	42.397952
3504.145523	506031.763574	42.402957
3504.034534	506017.865761	42.407962
3504.100711	506009.455495	42.412967
3504.049890	505998.128831	42.417972
3503.918778	505985.904023	42.422976
3503.888773	505981.354662	42.427981
3503.718200	505973.184206	42.432986
3504.110225	505938.156553	42.437991
3504.129660	505935.016212	42.442996
3503.907727	505938.795852	42.448000
3504.182404	505921.649096	42.453005
3503.917878	505903.828526	42.458010
3503.863316	505898.169786	42.463015
3503.482375	505901.569754	42.468020
3503.649366	505880.695446	42.473024
3503.917386	505863.499083	42.478029
3503.787250	505868.478674	42.483034
3504.027249	505845.922923	42.488039
3503.969318	505840.618910	42.493044
3503.557338	505831.828721	42.498048
3503.928997	505829.239910	42.503053
3503.732696	505819.201174	42.508058
3504.170115	505807.544201	42.513063
3504.284588	505792.143111	42.518068
3504.261870	505782.886550	42.523072
3504.252594	505759.914671	42.528077
3503.939033	505743.872765	42.533082
3504.081992	505739.144194	42.538087
3504.110127	505720.922962	42.543092
3503.916886	505700.864414	42.548096
3504.226981	505695.603390	42.553101
3504.139669	505680.031686	42.558106
3503.952096	505659.617978	42.563111
3503.951964	505663.008401	42.568116
3504.004477	505651.867587	42.573120
3504.265583	505634.064861	42.578125
3503.963698	505632.948756	42.583130
3504.037546	505618.616587	42.588135
3504.081140	505600.089169	42.593140
3504.049938	505593.870008	42.598144
3503.911664	505585.846073	42.603149
3503.657616	505567.669283	42.608154
3504.102358	505535.415639	42.613159
3503.805485	505547.607279	42.618164
3503.814968	505541.179258	42.623168
3503.801449	505513.552263	42.628173
3503.670492	505516.609173	42.633178
3503.927584	505508.370899	42.638183
3503.728664	505505.467407	42.643188
3503.754756	505493.824640	42.648192
3503.968887	505473.094203	42.653197
3503.951248	505468.492150	42.658202
3503.881712	505463.038048	42.663207
3503.921930	505456.908755	42.668212
3504.104044	505422.621690	42.673216
3504.166885	505423.067221	42.678221
3503.734932	505426.171724	42.683226
3503.910716	505400.842374	42.688231
3504.154758	505394.326619	42.693236
3504.086636	505379.763678	42.698240
3503.947439	505367.438507	42.703245
3504.025424	505351.587365	42.708250
3504.288928	505352.001180	42.713255
3504.123912	505329.711195	42.718260
3504.070966	505317.169941	42.723264
3504.443427	505302.284277	42.728269
3503.614151	505284.501738	42.733274
3504.029183	505267.180343	42.738279
3503.987719	505267.642365	42.743284
3504.016319	505254.733951	42.748288
3504.018948	505231.455872	42.753293
3504.003046	505222.956993	42.758298
3503.984884	505212.181297	42.763303
3503.795774	505202.647106	42.768308
3503.878334	505188.414415	42.773312
3504.105770	505171.274390	42.778317
3503.657253	505171.294717	42.783322
3503.784011	505149.312609	42.788327
3503.847505	505151.934014	42.793332
3503.955504	505144.123967	42.798337
3503.848220	505140.446870	42.803341
3503.564227	505116.657299	42.808346
3504.019753	505102.264376	42.813351
3503.901668	505110.835168	42.818356
3503.873257	505102.287603	42.823361
3503.826312	505075.272448	42.828365
3503.753145	505067.086169	42.833370
3504.044650	505068.457045	42.838375
3503.686716	505058.848253	42.843380
3503.519868	505043.136740	42.848385
3504.106817	505025.636119	42.853389
3504.206157	505031.895388	42.858394
3504.249040	505012.861415	42.863399
3504.130711	505009.135432	42.868404
3504.084103	504995.226627	42.873409
3504.662665	504974.286180	42.878413
3504.208622	504956.393388	42.883418
3503.799231	504943.047931	42.888423
3504.110053	504918.000163	42.893428
3504.149261	504913.085351	42.898433
3503.888617	504905.535887	42.903437
3503.854147	504899.519414	42.908442
3503.993871	504865.490979	42.913447
3503.969319	504861.547722	42.918452
3503.908604	504866.162390	42.923457
3504.302059	504832.448019	42.928461
3503.945227	504842.068778	42.933466
3503.986711	504828.955594	42.938471
3504.065421	504800.604425	42.943476
3504.095037	504792.806611	42.948481
3504.100172	504775.549522	42.953485
3503.754759	504761.535947	42.958490
3504.020573	504745.148515	42.963495
3503.841037	504745.176929	42.968500
3503.740048	504741.144516	42.973505
3504.105837	504708.496987	42.978509
3503.621305	504712.419609	42.983514
3503.647464	504700.675092	42.988519
3503.784263	504709.711844	42.993524
3503.868205	504687.685319	42.998529
3503.809837	504668.160923	43.003533
3503.610306	504674.416956	43.008538
3503.860971	504659.448788	43.013543
3503.912763	504667.132653	43.018548
3503.755729	504638.767880	43.023553
3503.972504	504620.363865	43.028557
3503.870611	504624.985106	43.033562
3503.906824	504618.906758	43.038567
3503.784915	504601.922607	43.043572
3503.725358	504590.849437	43.048577
3504.165448	504575.142778	43.053581
3503.927181	504570.423546	43.058586
3503.737235	504538.723840	43.063591
3503.835440	504536.886546	43.068596
3503.707303	504542.321649	43.073601
3503.808182	504538.965760	43.078605
3503.846275	504520.539279	43.083610
3503.717447	504508.970949	43.088615
3503.731264	504505.476999	43.093620
3503.704498	504504.570360	43.098625
3503.977076	504499.466726	43.103629
3503.602204	504489.556662	43.108634
3503.726742	504461.754365	43.113639
3503.933105	504471.792363	43.118644
3503.601597	504467.745719	43.123649
3503.703049	504458.772465	43.128653
3503.754337	504442.519872	43.133658
3503.733826	504421.369824	43.138663
3503.891505	504423.470390	43.143668
3503.839756	504421.150727	43.148673
3503.744389	504420.001897	43.153677
3503.708864	504401.333896	43.158682
3503.899781	504386.324333	43.163687
3503.628697	504391.427834	43.168692
3503.241306	504387.187580	43.173697
3503.521950	504380.311420	43.178701
3503.464379	504385.229356	43.183706
3503.861452	504371.047498	43.188711
3503.538880	504363.912437	43.193716
3503.582657	504354.290365	43.198721
3503.991635	504348.355427	43.203725
3503.707583	504364.240121	43.208730
3504.002778	504338.485509	43.213735
3503.972314	504323.865130	43.218740
3503.829343	504306.175532	43.223745
3504.042755	504316.617356	43.228749
3503.993711	504288.032520	43.233754
3504.051064	504265.756635	43.238759
3503.810787	504277.383539	43.243764
3503.669572	504270.017348	43.248769
3503.780758	504243.127732	43.253773
3503.728303	504246.627913	43.258778
3503.953366	504231.815247	43.263783
3503.634795	504229.385913	43.268788
3503.539049	504224.694666	43.273793
3503.911186	504205.860806	43.278797
3503.588492	504203.027267	43.283802
3503.765771	504186.197847	43.288807
3503.607062	504195.838250	43.293812
3503.655507	504199.727345	43.298817
3503.729421	504164.392177	43.303821
3503.581594	504158.494581	43.308826
3503.670804	504147.802471	43.313831
3503.662841	504156.406929	43.318836
3503.764092	504157.554917	43.323841
3503.556396	504135.017121	43.328845
3503.148100	504126.984589	43.333850
3503.451351	504108.971224	43.338855
3503.240817	504112.901274	43.343860
3503.223473	504121.152984	43.348865
3503.466054	504119.697681	43.353869
3503.461409	504126.125531	43.358874
3503.253703	504111.836633	43.363879
3503.535483	504136.488310	43.368884
3503.494514	504126.069798	43.373889
3503.648416	504121.541490	43.378893
3503.869106	504138.055102	43.383898
3504.007650	504111.515208	43.388903
3504.028311	504093.850138	43.393908
3503.561420	504095.745826	43.398913
3503.771913	504084.326008	43.403917
3503.402177	504087.218481	43.408922
3503.934950	504086.881268	43.413927
3503.543992	504064.929026	43.418932
3503.603326	504052.318510	43.423937
3503.970336	504052.969033	43.428941
3503.566345	504044.429712	43.433946
3503.886044	504038.863032	43.438951
3503.752607	504023.195928	43.443956
3503.722968	504014.293776	43.448961
3503.747756	504014.441715	43.453965
3503.751585	504003.914835	43.458970
3504.042127	503994.709026	43.463975
3504.156869	503970.348795	43.468980
3503.803215	503969.139547	43.473985
3504.056337	503963.431545	43.478989
3503.758614	503934.480581	43.483994
3504.047939	503930.285070	43.488999
3503.664899	503919.768684	43.494004
3503.584861	503912.493886	43.499009
3504.007598	503892.993795	43.504013
3503.950410	503896.697224	43.509018
3503.579954	503886.431866	43.514023
3503.875542	503883.196899	43.519028
3503.667994	503868.351093	43.524033
3504.109653	503850.264979	43.529037
3503.890314	503843.467641	43.534042
3504.079067	503840.603807	43.539047
3504.164578	503814.932180	43.544052
3503.749437	503800.169738	43.549057
3504.077367	503810.948018	43.554061
3503.965358	503783.080821	43.559066
3504.119726	503751.881955	43.564071
3504.102964	503756.085103	43.569076
3504.064293	503744.400802	43.574081
3504.015714	503733.477179	43.579085
3504.150502	503736.694825	43.584090
3504.184915	503716.243758	43.589095
3504.235552	503700.344838	43.594100
3503.791028	503693.684253	43.599105
3504.054232	503676.182857	43.604109
3503.654099	503650.081671	43.609114
3503.853533	503641.801029	43.614119
3503.751320	503643.740337	43.619124
3504.038796	503636.964025	43.624129
3504.077004	503615.196424	43.629133
3503.550846	503609.358445	43.634138
3503.717926	503595.313535	43.639143
3504.034121	503598.856790	43.644148
3503.843642	503579.048413	43.649153
3504.101723	503563.926315	43.654157
3503.881371	503555.813204	43.659162
3504.028047	503547.034771	43.664167
3504.149790	503526.316637	43.669172
3503.923900	503513.295341	43.674177
3503.781619	503510.078910	43.679181
3503.854195	503493.872683	43.684186
3503.996938	503481.552226	43.689191
3504.101386	503476.272438	43.694196
3503.685047	503468.392701	43.699201
3503.984496	503441.573318	43.704205
3503.906216	503436.069357	43.709210
3503.804715	503438.514664	43.714215
3503.908436	503423.568671	43.719220
3503.672416	503403.413033	43.724225
3503.683389	503399.160177	43.729229
3503.513124	503395.593885	43.734234
3503.780515	503399.296722	43.739239
3503.954405	503389.501728	43.744244
3503.775064	503381.635099	43.749249
3503.818024	503362.801761	43.754253
3503.626369	503367.893002	43.759258
3503.513016	503352.829435	43.764263
3503.443439	503356.939809	43.769268
3503.705176	503335.642621	43.774273
3503.794692	503321.002443	43.779277
3503.601497	503323.361041	43.784282
3503.926391	503311.821421	43.789287
3503.831020	503315.429789	43.794292
3503.505584	503299.336905	43.799297
3503.662997	503282.206106	43.804301
3503.551128	503272.810482	43.809306
3503.563103	503278.122609	43.814311
3503.423918	503277.183067	43.819316
3503.499656	503275.501021	43.824321
3503.828943	503267.756381	43.829325
3503.489079	503267.506481	43.834330
3503.345532	503247.842141	43.839335
3503.248274	503243.859403	43.844340
3503.287981	503236.919664	43.849345
3503.337310	503237.569826	43.854349
3503.450563	503235.730018	43.859354
3503.572626	503228.777258	43.864359
3503.707578	503240.294926	43.869364
3503.417301	503249.146891	43.874369
3503.813618	503242.758099	43.879373
3503.662423	503227.396749	43.884378
3503.616136	503205.085293	43.889383
3503.968650	503198.247923	43.894388
3503.655090	503198.044474	43.899393
3503.600387	503203.367163	43.904397
3503.420745	503204.509005	43.909402
3503.283607	503179.883837	43.914407
3503.448933	503169.128491	43.919412
3503.562097	503170.274661	43.924417
3503.696184	503153.653521	43.929421
3503.406588	503166.857855	43.934426
3503.389252	503163.064904	43.939431
3503.433544	503171.661585	43.944436
3503.568197	503162.733032	43.949441
3503.669272	503165.095746	43.954445
3503.374174	503166.053401	43.959450
3503.668671	503147.686170	43.964455
3503.735483	503138.312841	43.969460
3503.382871	503129.511901	43.974465
3503.540677	503123.818695	43.979469
3503.460871	503134.560621	43.984474
3503.657078	503128.000980	43.989479
3503.975062	503122.181235	43.994484
3503.650986	503113.527607	43.999489
3503.855968	503101.905585	44.004493
3503.654816	503107.453891	44.009498
3503.758034	503101.819916	44.014503
3503.859209	503092.947229	44.019508
3503.732914	503077.227543	44.024513
3503.818845	503054.085237	44.029517
3503.343188	503058.816579	44.034522
3503.504743	503057.576438	44.039527
3503.675228	503056.739765	44.044532
3503.686306	503047.577637	44.049537
3503.596779	503028.714274	44.054541
3503.435625	503033.193469	44.059546
3503.665775	503012.255155	44.064551
3503.315088	503016.055771	44.069556
3503.204809	503018.502524	44.074561
3503.440700	503018.313442	44.079565
3503.378122	503023.536210	44.084570
3503.660033	503024.554496	44.089575
3503.584460	503027.299422	44.094580
3503.777263	503008.796291	44.099585
3503.457241	502985.768674	44.104589
3503.541000	502988.083539	44.109594
3503.753871	502994.274979	44.114599
3503.357934	502984.620443	44.119604
3503.624571	502976.480696	44.124609
3503.951668	502981.237000	44.129613
3503.601679	502958.011642	44.134618
3503.606497	502950.419372	44.139623
3503.538389	502941.219095	44.144628
3503.424271	502942.198765	44.149633
3503.509753	502945.070077	44.154637
3503.531121	502943.750866	44.159642
3503.853491	502945.218255	44.164647
3503.496058	502916.173831	44.169652
3503.637246	502904.308711	44.174657
3503.694893	502904.704518	44.179661
3503.587074	502910.389964	44.184666
3503.433767	502897.913454	44.189671
3503.627040	502903.399478	44.194676
3503.558337	502891.618137	44.199681
3503.782051	502874.729514	44.204685
3503.471479	502865.567523	44.209690
3503.779702	502866.935934	44.214695
3503.481635	502866.375758	44.219700
3503.317319	502868.679241	44.224705
3503.763996	502866.736081	44.229709
3503.618870	502860.230295	44.234714
3503.603561	502839.431796	44.239719
3503.341021	502828.743875	44.244724
3503.442946	502827.918029	44.249729
3503.601064	502825.868644	44.254733
3503.317778	502834.264216	44.259738
3503.492850	502830.592611	44.264743
3503.702495	502827.421648	44.269748
3503.380601	502840.479499	44.274753
3503.571904	502839.133420	44.279757
3503.137768	502820.223083	44.284762
3503.344410	502804.501138	44.289767
3503.485709	502795.318295	44.294772
3503.165841	502799.923858	44.299777
3503.400084	502796.850223	44.304781
3503.037549	502799.286268	44.309786
3503.587888	502791.961976	44.314791
3503.451127	502791.781186	44.319796
3503.549293	502794.751739	44.324801
3503.647557	502795.039907	44.329805
3503.541799	502794.752995	44.334810
3503.836096	502789.038106	44.339815
3503.801312	502764.497400	44.344820
3503.637490	502755.919486	44.349825
3503.879236	502745.910966	44.354829
3503.279475	502756.279812	44.359834
3503.063245	502755.858529	44.364839
3503.564037	502748.238385	44.369844
3503.389204	502751.910039	44.374849
3503.433342	502755.040972	44.379853
3503.559825	502767.673727	44.384858
3503.356402	502742.147429	44.389863
3503.632310	502720.594206	44.394868
3503.640567	502729.955962	44.399873
3503.888402	502722.122737	44.404877
3503.198488	502735.137615	44.409882
3503.257562	502731.787992	44.414887
3503.757039	502720.777111	44.419892
3503.523102	502734.833356	44.424897
3503.667466	502698.522503	44.429901
3503.569372	502694.539772	44.434906
3503.846738	502676.478426	44.439911
3503.691277	502691.332078	44.444916
3503.378786	502688.243623	44.449921
3503.982593	502680.657778	44.454925
3503.553811	502667.566704	44.459930
3503.621356	502653.283723	44.464935
3503.489993	502648.091572	44.469940
3503.442801	502657.867021	44.474945
3503.882958	502645.853248	44.479949
3503.702333	502652.916786	44.484954
3503.666300	502634.702491	44.489959
3503.875512	502622.370928	44.494964
3503.672468	502612.736308	44.499969
3503.803843	502603.706768	44.504973
3503.377094	502614.453240	44.509978
3503.620758	502609.454855	44.514983
3503.672467	502584.647171	44.519988
3503.899318	502580.106937	44.524993
3503.820140	502568.681316	44.529997
3503.607720	502566.285580	44.535002
3503.723022	502564.192323	44.540007
3503.898798	502550.904379	44.545012
3503.557771	502535.319374	44.550017
3504.075073	502522.635374	44.555021
3503.872477	502531.322003	44.560026
3503.774997	502520.709028	44.565031
3504.075494	502510.033138	44.570036
3503.461412	502487.000738	44.575041
3503.988329	502486.664427	44.580045
3503.655530	502495.978994	44.585050
3503.742962	502466.762287	44.590055
3504.039120	502455.378487	44.595060
3503.637128	502455.846959	44.600065
3503.926333	502449.930319	44.605069
3503.596581	502428.978593	44.610074
3503.300025	502411.564425	44.615079
3503.575418	502418.657199	44.620084
3503.774381	502408.554028	44.625089
3504.018359	502397.380886	44.630093
3503.473996	502417.863548	44.635098
3503.967733	502388.633100	44.640103
3503.918414	502369.965125	44.645108
3503.405955	502376.625718	44.650113
3503.750444	502373.079076	44.655117
3503.684864	502367.016042	44.660122
3503.920279	502354.882599	44.665127
3503.876904	502346.842179	44.670132
3503.699705	502338.266176	44.675137
3503.792715	502322.764212	44.680141
3503.521321	502335.308332	44.685146
3503.620362	502323.651933	44.690151
3503.785278	502299.585136	44.695156
3503.463050	502299.534881	44.700161
3503.812115	502289.053630	44.705165
3503.814969	502295.835248	44.710170
3503.951502	502296.724721	44.715175
3503.628237	502262.460764	44.720180
3503.795853	502250.135518	44.725185
3503.842491	502252.962470	44.730189
3503.604515	502253.506245	44.735194
3503.746129	502240.678979	44.740199
3503.772487	502213.749064	44.745204
3503.567845	502225.219849	44.750209
3503.633151	502203.243773	44.755213
3503.512072	502220.471171	44.760218
3503.720873	502207.177749	44.765223
3503.399935	502198.523173	44.770228
3503.398247	502177.671130	44.775233
3503.676263	502170.339016	44.780237
3503.155939	502178.468690	44.785242
3503.422159	502172.859267	44.790247
3503.422716	502169.822462	44.795252
3503.255887	502175.618697	44.800257
3503.618260	502186.139467	44.805261
3503.553408	502193.539176	44.810266
3503.355121	502180.816206	44.815271
3503.375806	502183.697885	44.820276
3503.669457	502176.110239	44.825281
3503.789490	502149.114806	44.830285
3503.664232	502145.439921	44.835290
3503.589826	502142.617411	44.840295
3503.704468	502129.490652	44.845300
3503.421681	502134.596652	44.850305
3503.827280	502133.773385	44.855309
3503.693281	502111.676863	44.860314
3503.700401	502096.795630	44.865319
3503.485263	502091.869622	44.870324
3503.484722	502096.829793	44.875329
3503.841073	502092.724480	44.880333
3503.277005	502100.000688	44.885338
3503.138093	502095.163857	44.890343
3503.479692	502085.544083	44.895348
3503.301765	502075.854586	44.900353
3503.392922	502052.710144	44.905357
3503.280547	502058.649647	44.910362
3503.180053	502041.204123	44.915367
3503.125970	502047.488707	44.920372
3503.512012	502046.213012	44.925377
3503.541432	502045.044300	44.930381
3503.281076	502047.514909	44.935386
3503.550627	502046.358853	44.940391
3503.675656	502049.477125	44.945396
3503.717610	502062.882938	44.950401
3503.680979	502061.724668	44.955405
3503.438843	502055.588209	44.960410
3503.602106	502034.659311	44.965415
3503.421181	502029.829103	44.970420
3503.441850	502033.368777	44.975425
3503.878552	502008.853721	44.980429
3503.572351	502019.986401	44.985434
3503.748848	502021.122636	44.990439
3503.770761	501998.393971	44.995444
3503.628813	501992.140427	45.000449
3503.889338	501971.094854	45.005453
3503.413174	501989.896996	45.010458
3503.510594	501978.797370	45.015463
3503.607758	501972.202345	45.020468
3503.414947	501984.430612	45.025473
3503.673553	501958.374632	45.030477
3503.345599	501948.000196	45.035482
3503.335160	501942.940563	45.040487
3503.219483	501936.784073	45.045492
3503.272714	501936.269562	45.050497
3503.565586	501939.361323	45.055501
3503.434670	501937.610590	45.060506
3503.518228	501940.229304	45.065511
3503.417963	501938.271273	45.070516
3503.478506	501956.128190	45.075521
3503.657510	501932.564800	45.080525
3503.281493	501938.647243	45.085530
3503.200844	501928.183091	45.090535
3503.371239	501919.248261	45.095540
3503.289600	501915.667660	45.100545
3503.523613	501897.106240	45.105549
3502.775127	501909.574233	45.110554
3503.181227	501909.257010	45.115559
3503.372724	501913.630132	45.120564
3503.350930	501907.408178	45.125569
3503.876103	501902.112031	45.130573
3503.304265	501917.993800	45.135578
3503.098507	501910.889888	45.140583
3503.321666	501912.575501	45.145588
3503.367154	501910.493202	45.150593
3503.591474	501911.368818	45.155597
3503.515549	501912.747414	45.160602
3503.500498	501912.142469	45.165607
3503.517705	501915.227194	45.170612
3502.913512	501919.017501	45.175617
3503.522165	501911.683631	45.180621
3503.710069	501918.334916	45.185626
3503.502161	501896.755940	45.190631
3503.375585	501896.978437	45.195636
3503.414013	501889.127331	45.200641
3503.665382	501893.035474	45.205645
3503.578018	501892.745639	45.210650
3503.690858	501884.882769	45.215655
3503.888796	501880.448155	45.220660
3503.751728	501869.334912	45.225665
3504.004585	501846.923842	45.230669
3504.089181	501838.154374	45.235674
3503.722635	501830.519097	45.240679
3503.680016	501815.949172	45.245684
3503.726194	501807.438829	45.250689
3503.601287	501802.599704	45.255693
3503.485902	501809.298971	45.260698
3503.428011	501797.920100	45.265703
3503.832961	501801.247237	45.270708
3503.606214	501789.844438	45.275713
3504.156559	501769.208337	45.280717
3503.753232	501771.701583	45.285722
3503.704638	501760.169377	45.290727
3503.656065	501754.305899	45.295732
3503.615978	501736.850526	45.300737
3503.892786	501723.748447	45.305741
3503.612739	501735.788219	45.310746
3503.791475	501723.713918	45.315751
3504.107757	501713.186897	45.320756
3503.620565	501694.233126	45.325761
3503.925205	501690.895104	45.330765
3503.618097	501683.452823	45.335770
3503.979886	501672.058147	45.340775
3503.852528	501653.199296	45.345780
3503.780020	501650.983775	45.350785
3503.828428	501640.043527	45.355789
3503.631037	501654.145465	45.360794
3503.937822	501631.725599	45.365799
3503.833516	501603.904358	45.370804
3503.670286	501603.930194	45.375809
3503.620254	501592.043807	45.380813
3503.882277	501598.177356	45.385818
3503.522851	501584.821444	45.390823
3503.345808	501570.626865	45.395828
3503.563209	501564.569439	45.400833
3503.516185	501550.657978	45.405837
3503.455437	501555.324132	45.410842
3503.386790	501549.160073	45.415847
3503.616065	501558.993656	45.420852
3503.425040	501553.000785	45.425857
3503.699362	501548.098485	45.430861
3503.876193	501536.378659	45.435866
3503.663771	501516.571435	45.440871
3503.620827	501513.895695	45.445876
3503.439650	501519.896868	45.450881
3503.811364	501509.614037	45.455885
3503.594102	501514.558013	45.460890
3503.788616	501491.244657	45.465895
3503.484159	501483.903102	45.470900
3503.305124	501479.376132	45.475905
3503.476416	501475.097472	45.480909
3503.465567	501469.076093	45.485914
3503.842467	501475.950743	45.490919
3503.592129	501480.343198	45.495924
3503.451071	501453.742278	45.500929
3503.842154	501452.111443	45.505933
3503.445468	501442.962324	45.510938
3503.631892	501437.922044	45.515943
3503.664511	501443.940064	45.520948
3503.546046	501445.173576	45.525953
3503.614045	501435.900387	45.530957
3503.694303	501416.603549	45.535962
3503.941889	501401.228191	45.540967
3503.728466	501397.820160	45.545972
3503.589627	501400.474108	45.550977
3503.818754	501401.348991	45.555981
3503.414541	501377.320289	45.560986
3503.503532	501351.442075	45.565991
3503.819945	501350.531643	45.570996
3503.872309	501352.598611	45.576001
3503.941491	501349.449588	45.581005
3503.553756	501336.553498	45.586010
3503.551841	501324.912401	45.591015
3503.464588	501314.955080	45.596020
3503.577734	501315.493995	45.601025
3503.967382	501306.220511	45.606029
3503.443283	501306.455235	45.611034
3503.599385	501304.608455	45.616039
3503.867226	501284.826289	45.621044
3503.451434	501273.908575	45.626049
3503.684767	501263.343784	45.631053
3503.258804	501269.738041	45.636058
3503.418514	501274.774341	45.641063
3503.864483	501268.832532	45.646068
3503.702451	501273.059233	45.651073
3503.897825	501246.860360	45.656077
3503.763291	501236.657393	45.661082
3503.287947	501228.887206	45.666087
3503.315008	501225.592975	45.671092
3503.266686	501219.982356	45.676097
3503.760675	501220.764767	45.681101
3503.458817	501224.051892	45.686106
3503.383742	501220.976265	45.691111
3503.456439	501197.934856	45.696116
3503.286990	501187.433687	45.701121
3503.603078	501174.982996	45.706125
3503.273958	501182.526129	45.711130
3503.357084	501163.633487	45.716135
3503.390776	501175.624045	45.721140
3503.070624	501188.581603	45.726145
3503.371033	501174.868006	45.731149
3503.422880	501179.617691	45.736154
3503.359757	501182.816472	45.741159
3503.492580	501189.324893	45.746164
3503.380468	501188.532804	45.751169
3503.728137	501180.480658	45.756173
3503.770942	501179.613466	45.761178
3503.476780	501176.623077	45.766183
3503.450026	501153.850409	45.771188
3503.184495	501143.263170	45.776193
3503.382606	501135.082798	45.781197
3503.167806	501145.796653	45.786202
3503.755052	501147.779097	45.791207
3503.538829	501130.249739	45.796212
3503.314941	501142.382265	45.801217
3503.436611	501136.339827	45.806221
3503.431913	501140.946613	45.811226
3503.474441	501137.649920	45.816231
3503.806078	501135.522300	45.821236
3503.412713	501115.641999	45.826241
3503.508771	501106.920974	45.831245
3503.279503	501111.057110	45.836250
3503.326816	501099.559931	45.841255
3503.141000	501105.308899	45.846260
3503.000512	501117.428260	45.851265
3503.361700	501110.740566	45.856269
3503.249168	501106.152373	45.861274
3503.162582	501106.267326	45.866279
3503.344178	501106.643581	45.871284
3503.276160	501105.540825	45.876289
3503.585932	501101.392034	45.881293
3503.117206	501110.830041	45.886298
3503.242525	501099.573609	45.891303
3503.292098	501103.969365	45.896308
3503.291584	501112.371666	45.901313
3503.712606	501097.677250	45.906317
3503.748393	501103.644268	45.911322
3503.564674	501096.081004	45.916327
3503.444592	501079.498095	45.921332
3503.476923	501080.252255	45.926337
3503.507378	501077.514231	45.931341
3503.401550	501084.617185	45.936346
3503.557867	501079.277869	45.941351
3503.439470	501081.675555	45.946356
3503.441320	501073.829871	45.951361
3503.375657	501068.525640	45.956365
3503.851681	501072.145376	45.961370
3503.610578	501045.762122	45.966375
3503.596724	501048.092671	45.971380
3503.507654	501032.972673	45.976385
3503.918857	501025.872115	45.981389
3503.535902	501045.318526	45.986394
3503.353727	501033.199573	45.991399
3503.576565	501030.937291	45.996404
3503.473951	501004.987627	46.001409
3503.823130	500992.430346	46.006413
3503.643528	500988.763810	46.011418
3503.627569	500993.018104	46.016423
3503.866204	500997.535849	46.021428
3503.471774	500985.602263	46.026433
3503.687312	500956.717132	46.031437
3503.384861	500959.953783	46.036442
3503.278580	500952.226370	46.041447
3503.942184	500951.564734	46.046452
3503.458763	500955.083072	46.051457
3503.729956	500960.304304	46.056461
3503.385868	500963.294456	46.061466
3503.542811	500944.339297	46.066471
3503.536175	500937.001054	46.071476
3503.186460	500926.983771	46.076481
3503.752150	500914.442827	46.081485
3503.507234	500924.554181	46.086490
3503.090381	500925.379349	46.091495
3503.126179	500923.096002	46.096500
3503.136282	500917.627901	46.101505
3503.295784	500911.579406	46.106509
3503.316999	500919.674667	46.111514
3503.175796	500924.961096	46.116519
3503.227259	500918.575369	46.121524
3503.187383	500928.350613	46.126529
3503.592040	500921.352281	46.131533
3503.347198	500929.135280	46.136538
3503.077487	500930.898895	46.141543
3503.188508	500917.873046	46.146548
3503.129501	500924.968662	46.151553
3503.390541	500925.939758	46.156557
3503.036867	500921.288401	46.161562
3503.268666	500930.463924	46.166567
3503.365078	500925.640192	46.171572
3503.135339	500939.039185	46.176577
3503.624330	500930.610276	46.181581
3503.329363	500936.123471	46.186586
3503.165471	500932.403824	46.191591
3503.804490	500927.190627	46.196596
3503.500117	500906.739249	46.201601
3503.500849	500890.137066	46.206605
3502.932851	500892.605844	46.211610
3503.745574	500888.934281	46.216615
3503.621793	500891.889621	46.221620
3503.392916	500893.849250	46.226625
3503.342749	500891.984416	46.231629
3503.283266	500900.750452	46.236634
3503.640427	500896.999052	46.241639
3503.536973	500889.423013	46.246644
3503.420339	500890.099495	46.251649
3503.311292	500896.696871	46.256653
3503.364984	500884.084988	46.261658
3503.582898	500857.932596	46.266663
3503.620964	500859.495719	46.271668
3503.375225	500851.537225	46.276673
3503.670062	500842.784650	46.281677
3503.790343	500849.295178	46.286682
3503.492650	500854.505131	46.291687
3503.894719	500839.712266	46.296692
3503.605234	500829.634790	46.301697
3503.472375	500808.346326	46.306701
3503.265136	500810.454392	46.311706
3503.384531	500817.673701	46.316711
3503.467082	500814.218773	46.321716
3503.514315	500820.892706	46.326721
3503.473993	500813.610354	46.331725
3503.585442	500814.503869	46.336730
3503.480649	500806.421842	46.341735
3503.632866	500782.911779	46.346740
3503.525428	500782.321399	46.351745
3503.675299	500778.197808	46.356749
3503.414863	500783.958674	46.361754
3503.632753	500771.776306	46.366759
3503.599685	500773.451914	46.371764
3503.287488	500779.423430	46.376769
3503.747437	500776.364388	46.381773
3503.443759	500757.076907	46.386778
3503.304610	500733.916534	46.391783
3503.311061	500743.482091	46.396788
3503.261938	500726.735787	46.401793
3503.691575	500730.970325	46.406797
3503.470793	500735.864456	46.411802
3503.319798	500738.571040	46.416807
3503.529123	500733.982492	46.421812
3503.511869	500740.514799	46.426817
3503.795107	500741.735479	46.431821
3503.539882	500712.367582	46.436826
3503.522831	500710.041945	46.441831
3503.664964	500698.327052	46.446836
3503.329553	500711.287367	46.451841
3503.441324	500693.958816	46.456845
3503.409249	500704.897136	46.461850
3503.436517	500699.071938	46.466855
3503.843975	500692.579241	46.471860
3503.463393	500697.346792	46.476865
3504.134453	500655.937448	46.481869
3503.625724	500672.468368	46.486874
3503.418907	500654.937053	46.491879
3503.588921	500665.894070	46.496884
3503.314240	500661.888177	46.501889
3503.428834	500653.265234	46.506893
3503.176266	500671.172936	46.511898
3503.183505	500658.011451	46.516903
3503.661378	500668.008700	46.521908
3503.236024	500645.298387	46.526913
3503.357421	500632.068221	46.531917
3503.427297	500641.168256	46.536922
3503.725892	500627.353291	46.541927
3503.889049	500623.683117	46.546932
3503.701346	500634.190527	46.551937
3503.509785	500625.211029	46.556941
3503.470375	500618.130921	46.561946
3503.425451	500592.171536	46.566951
3503.658743	500596.234675	46.571956
3503.112172	500595.055681	46.576961
3503.589513	500583.692663	46.581965
3503.527216	500584.056865	46.586970
3503.787601	500581.586123	46.591975
3503.727607	500588.277093	46.596980
3503.289370	500593.003167	46.601985
3503.732604	500574.103595	46.606989
3503.378178	500557.607859	46.611994
3503.754654	500544.539777	46.616999
3503.747135	500555.322455	46.622004
3503.366003	500547.942014	46.627009
3503.936650	500560.506135	46.632013
3503.835690	500545.033281	46.637018
3503.691839	500515.698072	46.642023
3503.743465	500501.466494	46.647028
3503.559131	500510.353691	46.652033
3503.751885	500506.172641	46.657037
3503.605914	500509.182169	46.662042
3503.371607	500491.503188	46.667047
3503.574419	500460.999511	46.672052
3503.198988	500465.563839	46.677057
3503.424347	500458.846755	46.682061
3503.393030	500476.871531	46.687066
3503.603197	500470.055618	46.692071
3503.446731	500469.017420	46.697076
3503.230623	500472.847919	46.702081
3503.747729	500462.035330	46.707085
3503.570261	500474.768382	46.712090
3503.457905	500456.614532	46.717095
3503.427601	500438.903252	46.722100
3503.329122	500432.338581	46.727105
3503.091828	500422.353860	46.732109
3503.110873	500437.536134	46.737114
3503.291833	500425.258132	46.742119
3503.243271	500423.494230	46.747124
3503.296430	500440.189635	46.752129
3503.262786	500430.071492	46.757133
3503.356972	500434.004804	46.762138
3503.577971	500434.526699	46.767143
3503.616160	500445.403454	46.772148
3503.524492	500433.269786	46.777153
3503.488430	500432.516260	46.782157
3503.456057	500434.090554	46.787162
3503.567550	500440.298916	46.792167
3503.741110	500427.515911	46.797172
3503.412299	500418.760473	46.802177
3503.563889	500395.249998	46.807181
3503.361689	500393.206674	46.812186
3503.302373	500401.719840	46.817191
3503.740645	500390.970287	46.822196
3503.526035	500397.280827	46.827201
3503.370825	500398.773307	46.832205
3503.405421	500398.312315	46.837210
3503.766451	500393.446612	46.842215
3503.841500	500359.875284	46.847220
3503.351071	500370.531936	46.852225
3503.756872	500351.030633	46.857229
3503.567188	500361.690370	46.862234
3503.262917	500354.702641	46.867239
3503.316368	500358.288084	46.872244
3503.319976	500367.095027	46.877249
3503.695803	500359.443003	46.882253
3503.453723	500344.042900	46.887258
3503.665662	500323.458620	46.892263
3503.742980	500308.615413	46.897268
3503.500582	500320.295863	46.902273
3503.737487	500312.868250	46.907277
3503.551243	500315.782941	46.912282
3503.587489	500308.387044	46.917287
3503.454517	500280.618881	46.922292
3503.204010	500278.937505	46.927297
3503.609391	500269.256054	46.932301
3503.243634	500273.413958	46.937306
3503.211217	500272.204287	46.942311
3503.265872	500275.232759	46.947316
3503.202377	500272.661316	46.952321
3503.457026	500269.381551	46.957325
3503.496800	500275.955632	46.962330
3503.157950	500269.428897	46.967335
3503.116409	500276.977572	46.972340
3503.078351	500279.565137	46.977345
3503.238830	500272.352060	46.982349
3503.369374	500273.445055	46.987354
3503.309927	500273.606341	46.992359
3503.128472	500272.116520	46.997364
3502.864005	500274.486785	47.002369
3503.503334	500261.832510	47.007373
3503.371669	500278.000483	47.012378
3503.251637	500273.058935	47.017383
3503.353865	500263.222928	47.022388
3503.090303	500282.904385	47.027393
3503.295688	500277.000277	47.032397
3503.100998	500275.613785	47.037402
3503.356454	500281.242648	47.042407
3503.730794	500275.210597	47.047412
3503.408406	500283.006134	47.052417
3503.638208	500280.641421	47.057421
3503.498568	500273.425165	47.062426
3503.520059	500254.186976	47.067431
3503.372646	500249.249749	47.072436
3503.030270	500247.431036	47.077441
3503.186983	500247.507537	47.082445
3503.396462	500250.916485	47.087450
3503.580791	500250.634294	47.092455
3503.719906	500240.640590	47.097460
3503.433690	500252.530483	47.102465
3503.467349	500252.221490	47.107469
3503.456237	500240.581138	47.112474
3503.423684	500249.393854	47.117479
3503.371471	500251.578717	47.122484
3503.126751	500238.912312	47.127489
3503.424208	500225.552780	47.132493
3503.465428	500216.637516	47.137498
3503.218562	500208.172730	47.142503
3503.442034	500206.213953	47.147508
3503.380434	500211.538628	47.152513
3503.239162	500200.779333	47.157517
3503.602516	500207.909709	47.162522
3503.616128	500210.742207	47.167527
3503.474178	500198.160765	47.172532
3503.456307	500207.527981	47.177537
3503.225289	500207.665769	47.182541
3503.211084	500209.895248	47.187546
3503.224688	500213.689491	47.192551
3503.414842	500209.964347	47.197556
3503.290754	500216.868060	47.202561
3503.389613	500221.003153	47.207565
3503.462580	500213.702648	47.212570
3503.313528	500195.098770	47.217575
3503.325795	500187.301668	47.222580
3503.416033	500177.265036	47.227585
3503.500326	500165.153990	47.232589
3503.501281	500170.063844	47.237594
3503.433744	500174.883287	47.242599
3503.994347	500169.732886	47.247604
3503.628881	500173.131493	47.252609
3503.770104	500165.010288	47.257613
3503.853369	500139.890493	47.262618
3503.554748	500143.025449	47.267623
3503.580004	500128.848359	47.272628
3503.359410	500125.542452	47.277633
3503.844786	500127.338644	47.282637
3503.714197	500126.043245	47.287642
3503.448103	500095.410590	47.292647
3503.725111	500095.619931	47.297652
3503.298590	500089.562553	47.302657
3503.266174	500089.618331	47.307661
3503.656128	500091.277755	47.312666
3503.503257	500089.226598	47.317671
3504.011018	500083.072156	47.322676
3503.802527	500075.360518	47.327681
3504.005387	500053.967467	47.332685
3503.595629	500048.160518	47.337690
3503.634843	500054.633532	47.342695
3503.672899	500039.745689	47.347700
3503.568380	500040.116576	47.352705
3503.905263	500018.955392	47.357709
3503.619077	500013.381992	47.362714
3503.767306	500016.496955	47.367719
3504.080752	500005.513809	47.372724
3503.605470	499986.252618	47.377729
3503.735527	499970.034087	47.382733
3503.742196	499966.287276	47.387738
3503.890992	499968.541638	47.392743
3503.912783	499961.198501	47.397748
3503.660965	499936.485719	47.402753
3503.752607	499924.322730	47.407757
3503.784147	499931.657523	47.412762
3503.837464	499935.445548	47.417767
3503.642036	499904.143349	47.422772
3503.298922	499898.376436	47.427777
3503.516427	499887.408383	47.432781
3503.666483	499884.904366	47.437786
3503.765938	499892.886488	47.442791
3503.568726	499883.603795	47.447796
3503.521430	499887.205258	47.452801
3503.986374	499852.508347	47.457805
3503.476800	499864.939994	47.462810
3503.484167	499855.068139	47.467815
3503.637338	499846.894281	47.472820
3503.511513	499842.814054	47.477825
3503.672357	499844.864051	47.482829
3503.399441	499826.785559	47.487834
3503.418511	499813.115390	47.492839
3503.804629	499803.487353	47.497844
3503.871776	499808.488082	47.502849
3503.807449	499798.627527	47.507853
3503.832126	499794.827215	47.512858
3503.785859	499785.469992	47.517863
3503.965978	499765.598771	47.522868
3503.557435	499776.951502	47.527873
3503.587420	499757.508958	47.532877
3503.878680	499767.789309	47.537882
3503.730269	499743.464870	47.542887
3503.944569	499739.887670	47.547892
3503.646438	499724.546511	47.552897
3503.715432	499728.332102	47.557901
3503.606487	499723.692365	47.562906
3503.500769	499704.979887	47.567911
3503.577070	499693.578460	47.572916
3503.721502	499681.862538	47.577921
3503.501036	499681.846803	47.582925
3503.643625	499678.938981	47.587930
3503.442129	499678.363431	47.592935
3503.681469	499674.529162	47.597940
3503.368442	499663.391734	47.602945
3503.664542	499630.239672	47.607949
3503.496869	499635.733145	47.612954
3503.407615	499646.225573	47.617959
3503.720620	499627.041869	47.622964
3503.537641	499622.160710	47.627969
3503.575894	499629.140227	47.632973
3503.716297	499619.095354	47.637978
3503.438925	499601.118577	47.642983
3503.717556	499589.685102	47.647988
3503.431556	499600.613615	47.652993
3503.472695	499581.371596	47.657997
3503.471241	499598.481379	47.663002
3503.396273	499591.760823	47.668007
3503.566752	499585.862006	47.673012
3503.181197	499589.618236	47.678017
3503.480775	499584.762029	47.683021
3503.316315	499594.253977	47.688026
3503.257248	499570.725098	47.693031
3503.567770	499567.335134	47.698036
3503.199620	499552.004894	47.703041
3503.557588	499546.076427	47.708045
3503.554209	499546.785677	47.713050
3503.247583	499555.085238	47.718055
3503.462461	499541.130810	47.723060
3503.544477	499553.367920	47.728065
3503.506585	499553.171465	47.733069
3503.437323	499552.372529	47.738074
3503.486262	499547.910270	47.743079
3503.582098	499543.643077	47.748084
3503.077268	499531.472864	47.753089
3503.587027	499514.687702	47.758093
3503.412816	499519.321702	47.763098
3503.068480	499509.707729	47.768103
3503.463893	499512.277507	47.773108
3503.187797	499516.117691	47.778113
3503.292891	499502.889268	47.783117
3503.321452	499520.753683	47.788122
3503.301683	499515.897316	47.793127
3503.452883	499511.975704	47.798132
3503.155446	499522.501112	47.803137
3503.408787	499501.251282	47.808141
3503.125065	499515.064834	47.813146
3502.986586	499516.858461	47.818151
3503.208159	499514.292469	47.823156
3503.197228	499511.560747	47.828161
3503.337718	499508.349509	47.833165
3502.912630	499517.224634	47.838170
3503.474143	499517.338392	47.843175
3503.534669	499523.504509	47.848180
3503.312995	499530.069571	47.853185
3503.483583	499525.588078	47.858189
3503.664595	499516.397268	47.863194
3503.363979	499524.139072	47.868199
3503.353867	499519.534280	47.873204
3503.126323	499524.227329	47.878209
3503.230798	499526.185033	47.883213
3503.648669	499515.944382	47.888218
3503.568327	499512.616191	47.893223
3503.295687	499479.553751	47.898228
3503.021699	499484.001051	47.903233
3503.487582	499482.712561	47.908237
3503.601718	499476.367032	47.913242
3503.481548	499462.769224	47.918247
3503.779299	499479.679965	47.923252
3503.580473	499483.609183	47.928257
3503.787009	499472.794471	47.933261
3503.387164	499458.937147	47.938266
3503.331941	499446.999530	47.943271
3503.540848	499430.059362	47.948276
3503.312444	499438.903436	47.953281
3503.479917	499438.826379	47.958285
3503.445512	499439.996120	47.963290
3503.311329	499439.713643	47.968295
3503.470550	499441.055259	47.973300
3503.415276	499442.177678	47.978305
3503.402905	499434.029800	47.983309
3503.479728	499444.951677	47.988314
3503.376752	499438.235491	47.993319
3503.730223	499433.421344	47.998324
3503.419950	499411.146850	48.003329
3503.728501	499395.861373	48.008333
3503.283416	499397.349134	48.013338
3503.130696	499393.171814	48.018343
3503.343024	499393.846973	48.023348
3503.526318	499398.930698	48.028353
3503.701304	499394.752200	48.033357
3503.431314	499402.641076	48.038362
3503.382418	499401.383330	48.043367
3503.623833	499400.737761	48.048372
3503.036903	499391.364553	48.053377
3503.368641	499381.795506	48.058381
3503.775030	499381.984407	48.063386
3503.482054	499372.767205	48.068391
3503.259193	499379.231269	48.073396
3503.359231	499370.812492	48.078401
3503.514103	499369.876878	48.083405
3503.392420	499370.604834	48.088410
3503.650162	499368.336827	48.093415
3503.599150	499364.902731	48.098420
3503.416306	499375.966937	48.103425
3503.744659	499352.528393	48.108429
3503.522939	499338.895923	48.113434
3503.704292	499326.971451	48.118439
3503.703986	499335.374555	48.123444
3503.556574	499331.702588	48.128449
3503.716014	499334.613416	48.133453
3503.365763	499317.812149	48.138458
3503.366509	499295.488349	48.143463
3503.716028	499293.813274	48.148468
3503.123575	499291.224059	48.153473
3503.585585	499287.253270	48.158477
3503.327629	499300.657948	48.163482
3503.123373	499282.416190	48.168487
3503.282742	499292.717663	48.173492
3503.037706	499294.781260	48.178497
3503.016830	499285.267899	48.183501
3503.412333	499299.733563	48.188506
3503.027194	499298.427718	48.193511
3503.411201	499284.395736	48.198516
3503.387326	499293.359414	48.203521
3503.289836	499288.464650	48.208525
3503.246580	499295.760906	48.213530
3503.555767	499295.661448	48.218535
3503.201853	499289.794802	48.223540
3503.380556	499293.917489	48.228545
3503.311116	499289.271395	48.233549
3503.633297	499291.650298	48.238554
3503.663184	499289.772643	48.243559
3503.392722	499277.160245	48.248564
3503.296916	499264.014022	48.253569
3503.442611	499253.866866	48.258573
3503.236406	499249.343621	48.263578
3503.304705	499251.965144	48.268583
3503.692473	499250.284019	48.273588
3503.113691	499261.815846	48.278593
3503.131801	499252.448168	48.283597
3503.296851	499255.408743	48.288602
3503.266907	499250.452671	48.293607
3503.610679	499246.399320	48.298612
3503.233521	499252.634715	48.303617
3503.630506	499243.004660	48.308621
3503.599437	499243.870161	48.313626
3503.263679	499246.909900	48.318631
3503.491216	499249.556873	48.323636
3503.519826	499251.830324	48.328641
3503.486798	499218.932011	48.333645
3503.164210	499225.766239	48.338650
3503.165090	499218.122377	48.343655
3503.746930	499220.055279	48.348660
3503.446134	499218.887959	48.353665
3503.389807	499220.972356	48.358669
3503.427092	499217.068687	48.363674
3503.315991	499227.412950	48.368679
3503.617625	499206.458863	48.373684
3503.486260	499222.172153	48.378689
3503.484183	499218.375948	48.383693
3503.312345	499220.681087	48.388698
3503.394815	499208.164716	48.393703
3503.608594	499188.591261	48.398708
3503.295588	499180.592031	48.403713
3503.583695	499176.648706	48.408717
3503.430771	499182.595575	48.413722
3503.431457	499171.762599	48.418727
3503.232163	499160.252532	48.423732
3503.312189	499173.603880	48.428737
3503.690070	499163.470593	48.433741
3503.565641	499171.842773	48.438746
3503.608250	499178.872398	48.443751
3503.710514	499159.164675	48.448756
3503.462588	499139.006073	48.453761
3503.595577	499131.645019	48.458765
3503.644962	499145.507444	48.463770
3503.650311	499145.658497	48.468775
3503.763088	499131.871753	48.473780
3503.373796	499119.126164	48.478785
3503.517168	499096.982057	48.483789
3503.456716	499093.600022	48.488794
3503.314992	499092.711277	48.493799
3503.524091	499091.311486	48.498804
3503.346444	499096.401729	48.503809
3503.660092	499090.176391	48.508813
3503.287269	499090.792192	48.513818
3503.401860	499090.723493	48.518823
3503.487721	499087.318330	48.523828
3503.402378	499095.684367	48.528833
3503.338037	499087.747032	48.533837
3503.738790	499088.240555	48.538842
3503.674345	499075.392965	48.543847
3503.721281	499061.616575	48.548852
3503.551065	499048.481956	48.553857
3503.261354	499045.085530	48.558861
3503.315696	499056.821140	48.563866
3503.588122	499045.287056	48.568871
3503.811590	499051.883172	48.573876
3503.289008	499033.995208	48.578881
3503.288846	499017.796399	48.583885
3503.267138	499026.962353	48.588890
3503.645477	499014.550944	48.593895
3503.556370	499005.503814	48.598900
3503.208526	499014.822569	48.603905
3503.510124	499006.270517	48.608909
3503.440939	499008.205107	48.613914
3503.324005	499008.071761	48.618919
3503.357470	499005.839160	48.623924
3503.556208	499015.071518	48.628929
3503.777395	499009.923818	48.633933
3503.689502	498988.271727	48.638938
3503.399656	498983.812257	48.643943
3503.568615	498980.849533	48.648948
3503.408062	498979.356299	48.653953
3503.575729	498968.851158	48.658957
3503.479079	498971.549417	48.663962
3503.175544	498975.799026	48.668967
3503.380009	498969.388418	48.673972
3503.331920	498975.774378	48.678977
3503.477702	498971.195425	48.683981
3503.666838	498972.177996	48.688986
3503.767870	498948.319264	48.693991
3503.614211	498925.614437	48.698996
3503.191898	498935.349978	48.704001
3503.481777	498929.988911	48.709005
3503.605924	498930.323675	48.714010
3503.403691	498925.799720	48.719015
3503.561897	498922.028739	48.724020
3503.314033	498935.027119	48.729025
3503.578661	498913.774811	48.734029
3503.519843	498900.318744	48.739034
3503.513687	498898.902342	48.744039
3503.850516	498888.269171	48.749044
3503.497102	498893.994717	48.754049
3503.689476	498886.269822	48.759053
3503.705647	498889.658966	48.764058
3503.367094	498873.817248	48.769063
3503.859225	498835.924897	48.774068
3503.556933	498850.956822	48.779073
3503.210742	498840.988428	48.784077
3503.470355	498850.768090	48.789082
3503.307746	498850.490097	48.794087
3503.581887	498841.739820	48.799092
3503.248947	498844.627314	48.804097
3503.527754	498850.657915	48.809101
3503.608126	498853.986295	48.814106
3503.754701	498831.740112	48.819111
3503.682578	498814.691921	48.824116
3503.223494	498821.244146	48.829121
3503.465613	498812.245806	48.834125
3503.678207	498809.984865	48.839130
3503.192103	498805.860106	48.844135
3503.525616	498801.200813	48.849140
3503.333755	498805.027833	48.854145
3503.628993	498800.728944	48.859149
3503.677003	498792.925586	48.864154
3503.481607	498770.125915	48.869159
3503.815410	498759.645013	48.874164
3503.444196	498765.424035	48.879169
3503.316861	498765.849176	48.884173
3503.403916	498759.052075	48.889178
3503.534614	498766.877893	48.894183
3503.707638	498752.372625	48.899188
3503.094756	498770.288556	48.904193
3503.588645	498752.847105	48.909197
3503.340563	498734.510473	48.914202
3503.424017	498733.484871	48.919207
3503.531116	498732.101176	48.924212
3503.490310	498738.536692	48.929217
3503.597916	498734.166202	48.934221
3503.630442	498725.757794	48.939226
3503.745281	498735.762892	48.944231
3503.619652	498722.519742	48.949236
3503.485639	498712.163382	48.954241
3503.661398	498684.647678	48.959245
3503.483781	498684.625167	48.964250
3503.127142	498692.072449	48.969255
3503.709376	498684.538956	48.974260
3503.400411	498681.499860	48.979265
3503.171224	498692.166832	48.984269
3503.307491	498687.437443	48.989274
3503.253671	498686.990384	48.994279
3503.624073	498685.970045	48.999284
3503.156268	498690.853155	49.004289
3503.238787	498676.362131	49.009293
3503.424402	498677.294654	49.014298
3503.111458	498688.835448	49.019303
3503.242674	498681.626358	49.024308
3503.357920	498687.531001	49.029313
3503.166137	498681.739772	49.034317
3503.056075	498680.694133	49.039322
3503.219971	498684.768679	49.044327
3503.622690	498673.416252	49.049332
3503.231250	498662.341217	49.054337
3503.467685	498653.090584	49.059341
3503.202786	498643.767324	49.064346
3503.238018	498646.141049	49.069351
3503.476972	498643.521564	49.074356
3503.078179	498652.139844	49.079361
3503.204214	498650.246924	49.084365
3503.191283	498643.263094	49.089370
3503.195876	498636.327113	49.094375
3503.216252	498640.626845	49.099380
3502.707067	498653.109888	49.104385
3503.274868	498645.274925	49.109389
3503.611707	498652.359494	49.114394
3503.002475	498646.381126	49.119399
3503.551736	498643.206366	49.124404
3503.133876	498643.981167	49.129409
3503.600136	498647.501702	49.134413
3503.374313	498648.954864	49.139418
3503.298418	498643.955265	49.144423
3503.371059	498652.347158	49.149428
3503.268648	498666.942661	49.154433
3503.363405	498650.374160	49.159437
3503.371918	498655.232612	49.164442
3503.072236	498655.229395	49.169447
3503.405982	498648.950106	49.174452
3503.159135	498642.357608	49.179457
3503.466719	498648.484974	49.184461
3503.095600	498658.870665	49.189466
3503.110620	498653.552962	49.194471
3503.491188	498636.179933	49.199476
3503.226537	498665.430998	49.204481
3503.200882	498660.625952	49.209485
3503.275546	498654.235750	49.214490
3503.117596	498656.083163	49.219495
3503.449995	498648.994126	49.224500
3503.513380	498655.261335	49.229505
3503.493454	498653.492732	49.234509
3503.519282	498644.781610	49.239514
3503.211772	498626.555507	49.244519
3503.718178	498610.731862	49.249524
3503.310006	498624.059543	49.254529
3503.487611	498608.945964	49.259533
3503.518978	498606.409909	49.264538
3503.099732	498612.449685	49.269543
3503.157971	498611.630553	49.274548
3502.801357	498618.723503	49.279553
3503.326895	498609.376526	49.284557
3503.267049	498627.559540	49.289562
3503.204580	498618.052401	49.294567
3503.501772	498610.158952	49.299572
3503.104026	498622.573778	49.304577
3503.473550	498621.300461	49.309581
3503.544806	498620.074291	49.314586
3503.285735	498611.104450	49.319591
3503.523155	498615.876107	49.324596
3503.287326	498620.773191	49.329601
3503.202052	498617.951839	49.334605
3503.066207	498619.238913	49.339610
3503.401275	498615.389288	49.344615
3503.815389	498616.538808	49.349620
3503.259192	498602.401799	49.354625
3503.348628	498593.579352	49.359629
3503.488394	498581.964696	49.364634
3503.329857	498581.534187	49.369639
3503.313971	498582.194829	49.374644
3503.246694	498587.571506	49.379649
3503.581525	498579.013999	49.384653
3503.619881	498589.638741	49.389658
3503.088233	498593.722006	49.394663
3503.577661	498583.672007	49.399668
3503.229303	498584.587693	49.404673
3503.497307	498590.518844	49.409677
3503.267101	498587.214170	49.414682
3503.372103	498590.589328	49.419687
3503.526602	498581.351610	49.424692
3503.065854	498570.793701	49.429697
3503.436279	498552.004757	49.434701
3503.472868	498543.140017	49.439706
3503.213578	498546.218407	49.444711
3503.526415	498542.169790	49.449716
3503.244909	498543.125533	49.454721
3503.621523	498541.243616	49.459725
3503.566318	498544.795976	49.464730
3503.567454	498546.263893	49.469735
3503.202644	498549.308340	49.474740
3502.913972	498561.756589	49.479745
3503.568236	498546.415744	49.484749
3503.442148	498547.802527	49.489754
3503.323319	498553.389854	49.494759
3503.397367	498552.365728	49.499764
3503.422258	498556.158539	49.504769
3503.669280	498538.148429	49.509773
3503.365661	498525.743234	49.514778
3503.381563	498513.388770	49.519783
3503.527085	498506.987315	49.524788
3503.117143	498508.115231	49.529793
3503.451691	498501.886387	49.534797
3503.684698	498509.544277	49.539802
3503.597440	498516.695935	49.544807
3503.450749	498515.099225	49.549812
3503.319681	498506.615328	49.554817
3503.609288	498510.214437	49.559821
3503.638627	498486.366424	49.564826
3503.435636	498469.692953	49.569831
3503.325131	498469.001733	49.574836
3503.233498	498472.964849	49.579841
3503.357732	498463.984970	49.584845
3503.105723	498464.581693	49.589850
3502.843494	498474.646539	49.594855
3503.285092	498468.350140	49.599860
3503.353962	498460.290224	49.604865
3503.400622	498461.497838	49.609869
3503.448405	498466.704494	49.614874
3502.987203	498466.018086	49.619879
3503.534065	498465.526695	49.624884
3503.043260	498470.109762	49.629889
3503.285136	498459.896332	49.634893
3503.658148	498461.254851	49.639898
3503.269011	498470.124807	49.644903
3503.563713	498464.104741	49.649908
3503.310897	498471.940686	49.654913
3503.696765	498453.503560	49.659917
3503.647619	498453.258248	49.664922
3503.463155	498437.644903	49.669927
3503.759287	498431.675223	49.674932
3503.672054	498439.738125	49.679937
3503.598795	498438.028554	49.684941
3503.553013	498427.303721	49.689946
3503.551200	498432.923212	49.694951
3503.749037	498400.138777	49.699956
3503.449381	498387.429121	49.704961
3503.375403	498386.175268	49.709965
3503.146076	498384.389115	49.714970
3502.916316	498387.057879	49.719975
3503.376403	498371.747579	49.724980
3503.550777	498380.528505	49.729985
3503.444154	498384.089024	49.734989
3503.527335	498388.227019	49.739994
3503.258986	498382.549043	49.744999
3503.363920	498383.494333	49.750004
3503.104446	498386.218417	49.755009
3503.414642	498383.638257	49.760013
3503.477474	498390.108138	49.765018
3503.281136	498384.570650	49.770023
3503.429403	498384.142263	49.775028
3503.319779	498390.031925	49.780033
3503.406013	498380.045545	49.785037
3503.373613	498348.411121	49.790042
3503.428197	498346.478840	49.795047
3503.647464	498346.140476	49.800052
3503.326275	498355.607228	49.805057
3503.282842	498345.438831	49.810061
3503.518472	498349.755231	49.815066
3503.559689	498349.394388	49.820071
3503.529316	498339.072054	49.825076
3503.331547	498347.101846	49.830081
3503.468199	498343.688515	49.835085
3503.489846	498347.330012	49.840090
3503.210595	498328.086671	49.845095
3503.519424	498304.143615	49.850100
3503.248737	498304.540802	49.855105
3503.084246	498316.615227	49.860109
3502.945509	498317.852155	49.865114
3503.053411	498320.315684	49.870119
3503.316873	498338.194768	49.875124
3503.287292	498338.705713	49.880129
3503.468818	498323.034418	49.885133
3503.636997	498317.135548	49.890138
3503.620751	498303.773553	49.895143
3503.581811	498313.398206	49.900148
3503.530969	498299.889806	49.905153
3503.855193	498309.305186	49.910157
3503.621418	498309.190303	49.915162
3503.582897	498290.313858	49.920167
3503.628378	498276.840838	49.925172
3503.339299	498278.506523	49.930177
3503.318327	498260.589120	49.935181
3503.546126	498268.855420	49.940186
3503.392425	498260.779973	49.945191
3503.105913	498263.305854	49.950196
3503.284252	498275.579234	49.955201
3503.348723	498265.950596	49.960205
3503.319557	498277.548043	49.965210
3503.333327	498279.823963	49.970215
3503.093085	498271.458459	49.975220
3503.073891	498277.131370	49.980225
3503.166290	498273.320031	49.985229
3503.601400	498282.869768	49.990234
3503.262152	498276.949847	49.995239
3503.515312	498276.555501	50.000244
3503.283951	498286.716820	50.005249
3503.558510	498263.082867	50.010253
3503.246418	498241.667810	50.015258
3503.269535	498244.347246	50.020263
3503.555776	498224.862537	50.025268
3503.317826	498233.607463	50.030273
3503.301188	498234.774473	50.035277
3503.505786	498229.426680	50.040282
3503.370175	498230.359378	50.045287
3503.362808	498230.461825	50.050292
3503.459663	498226.548525	50.055297
3503.361919	498231.221392	50.060301
3503.472708	498237.228135	50.065306
3503.253029	498235.389818	50.070311
3503.554680	498218.838841	50.075316
3503.292481	498237.408601	50.080321
3503.608783	498223.993981	50.085325
3503.909879	498200.052009	50.090330
3503.443559	498199.518269	50.095335
3503.795328	498187.464858	50.100340
3503.713858	498201.044952	50.105345
3503.750817	498180.536500	50.110349
3503.488634	498168.681370	50.115354
3503.414665	498151.582219	50.120359
3503.748209	498143.075334	50.125364
3503.710956	498149.510498	50.130369
3503.294115	498148.108329	50.135373
3503.444042	498142.313536	50.140378
3503.399683	498148.749824	50.145383
3503.430406	498148.137516	50.150388
3503.173787	498140.837643	50.155393
3503.207249	498148.425981	50.160397
3503.201562	498147.566308	50.165402
3503.049804	498144.147904	50.170407
3503.535459	498146.146754	50.175412
3503.440674	498149.502952	50.180417
3503.374001	498126.732742	50.185421
3503.250145	498113.336991	50.190426
3503.345124	498119.548769	50.195431
3503.762498	498105.308100	50.200436
3503.495553	498131.067334	50.205441
3503.485313	498121.906044	50.210445
3503.532572	498117.139952	50.215450
3503.313533	498124.464469	50.220455
3503.250884	498122.196327	50.225460
3503.323938	498120.463598	50.230465
3503.159414	498118.970919	50.235469
3503.494703	498123.018501	50.240474
3503.292601	498126.847283	50.245479
3503.627461	498109.379724	50.250484
3503.007493	498114.287041	50.255489
3503.405356	498108.706166	50.260493
3503.498885	498091.782978	50.265498
3502.999799	498088.014472	50.270503
3503.219578	498078.664929	50.275508
3503.117618	498094.475803	50.280513
3503.081382	498109.820659	50.285517
3503.298615	498107.812018	50.290522
3503.262996	498121.587420	50.295527
3503.423619	498120.802706	50.300532
3503.217198	498098.560791	50.305537
3502.983142	498088.422381	50.310541
3503.120888	498083.034487	50.315546
3503.092368	498112.654117	50.320551
3503.418453	498120.196212	50.325556
3503.398591	498126.881756	50.330561
3503.443666	498103.891357	50.335565
3503.309102	498092.471622	50.340570
3503.205373	498083.730083	50.345575
3503.505737	498082.113293	50.350580
3503.282685	498090.450940	50.355585
3503.419393	498082.835750	50.360589
3502.881800	498081.047669	50.365594
3502.875019	498083.428110	50.370599
3503.290452	498084.476209	50.375604
3503.540284	498084.689875	50.380609
3503.068036	498080.157763	50.385613
3503.189672	498091.579621	50.390618
3503.225823	498078.310424	50.395623
3503.409469	498087.292524	50.400628
3503.285680	498088.678978	50.405633
3503.221377	498089.549787	50.410637
3503.395308	498083.801805	50.415642
3503.308562	498079.411254	50.420647
3503.096025	498080.052374	50.425652
3503.103678	498089.062292	50.430657
3503.137257	498079.691559	50.435661
3503.260417	498080.887106	50.440666
3503.348798	498084.113114	50.445671
3503.461008	498089.866561	50.450676
3503.353101	498083.656888	50.455681
3503.224541	498090.055883	50.460685
3503.478600	498083.232129	50.465690
3503.184525	498091.834122	50.470695
3503.103958	498087.898213	50.475700
3503.259211	498081.950686	50.480705
3503.548491	498086.359918	50.485709
3503.305989	498088.068881	50.490714
3503.158901	498093.407697	50.495719
3503.674819	498090.086240	50.500724
3503.361363	498097.020699	50.505729
3502.983030	498077.489007	50.510733
3503.286741	498051.167090	50.515738
3503.284564	498031.373393	50.520743
3503.308376	498004.184414	50.525748
3502.511814	497973.935731	50.530753
3502.917324	497918.134089	50.535757
3503.527825	497852.883668	50.540762
3502.826118	497781.512312	50.545767
3503.040609	497686.758884	50.550772
3502.894567	497596.466367	50.555777
3502.928890	497505.537379	50.560781
3502.885090	497397.761820	50.565786
3502.308780	497258.630806	50.570791
3502.358006	497126.436970	50.575796
3502.269422	496985.505451	50.580801
3501.813575	496826.303693	50.585805
3501.790315	496670.626751	50.590810
3501.239319	496507.083217	50.595815
3501.516600	496323.206307	50.600820
3501.056384	496154.481085	50.605825
3500.602234	495968.336617	50.610829
3500.760140	495768.372615	50.615834
3500.231286	495565.274582	50.620839
3500.273512	495345.527440	50.625844
3499.901787	495136.779675	50.630849
3499.952305	494901.937444	50.635853
3499.790356	494672.999287	50.640858
3499.221981	494426.248613	50.645863
3499.120454	494165.293657	50.650868
3498.221608	493920.866998	50.655873
3498.301209	493645.444848	50.660877
3498.123259	493374.262177	50.665882
3497.472268	493103.251567	50.670887
3497.237572	492815.460397	50.675892
3496.638497	492530.710073	50.680897
3496.843760	492235.244399	50.685901
3496.315215	491932.293839	50.690906
3495.653378	491638.474955	50.695911
3495.438767	491310.447484	50.700916
3494.961362	491005.701231	50.705921
3494.312422	490683.808617	50.710925
3493.978366	490360.088084	50.715930
3493.595658	490018.896656	50.720935
3493.433774	489685.717016	50.725940
3492.970656	489342.246851	50.730945
3492.480566	488989.303285	50.735949
3492.000290	488639.542500	50.740954
3491.622997	488285.099052	50.745959
3491.323312	487919.138682	50.750964
3490.512199	487562.166997	50.755969
3490.149973	487196.303842	50.760973
3489.591188	486819.877828	50.765978
3489.205938	486448.381210	50.770983
3488.778313	486059.407402	50.775988
3487.947929	485681.330139	50.780993
3487.834753	485297.812830	50.785997
3486.952620	484892.726912	50.791002
3486.569393	484509.641807	50.796007
3486.434161	484107.308935	50.801012
3485.394247	483699.740377	50.806017
3485.252016	483309.601792	50.811021
3484.584871	482895.421654	50.816026
3484.287955	482481.630135	50.821031
3483.682388	482062.811845	50.826036
3482.654317	481641.467232	50.831041
3482.131835	481230.066177	50.836045
3482.365638	480786.563673	50.841050
3480.967960	480384.201231	50.846055
3480.389987	479949.574338	50.851060
3479.745268	479528.072965	50.856065
3479.297987	479100.906426	50.861069
3479.174116	478666.838232	50.866074
3478.051038	478237.884855	50.871079
3477.661268	477789.447107	50.876084
3476.778289	477354.152547	50.881089
3476.324286	476912.192168	50.886093
3475.416741	476480.582111	50.891098
3474.765445	476035.237849	50.896103
3474.150181	475596.720344	50.901108
3473.744481	475158.210829	50.906113
3473.190801	474714.088988	50.911117
3472.718796	474260.820739	50.916122
3472.140679	473822.714974	50.921127
3471.578761	473370.201340	50.926132
3470.897909	472920.940642	50.931137
3470.225509	472460.465800	50.936141
3469.677501	472007.159318	50.941146
3468.853119	471548.107360	50.946151
3468.052512	471079.003707	50.951156
3467.214452	470633.418414	50.956161
3466.767229	470167.989676	50.961165
3466.559513	469719.851532	50.966170
3465.869148	469258.800866	50.971175
3464.968420	468794.883268	50.976180
3464.249650	468333.208156	50.981185
3463.588298	467876.026330	50.986189
3463.039052	467403.149177	50.991194
3462.119172	466955.317706	50.996199
3461.595539	466486.066634	51.001204
3460.894601	466025.909802	51.006209
3460.258093	465565.631344	51.011213
3459.701675	465098.281558	51.016218
3458.836693	464643.293015	51.021223
3458.560802	464171.263809	51.026228
3457.539582	463711.513140	51.031233
3456.764422	463247.707265	51.036237
3456.646982	462769.840665	51.041242
3455.765692	462319.673938	51.046247
3454.645688	461841.894520	51.051252
3453.976782	461384.574253	51.056257
3453.416224	460913.127134	51.061261
3452.864449	460444.204431	51.066266
3451.897005	459994.865254	51.071271
3451.406874	459520.232085	51.076276
3450.665243	459071.548343	51.081281
3449.946481	458607.532854	51.086285
3449.116921	458148.090439	51.091290
3448.415176	457689.328423	51.096295
3447.597968	457223.219550	51.101300
3446.841455	456767.389320	51.106305
3446.240558	456309.039349	51.111309
3445.565660	455865.657389	51.116314
3444.754036	455401.893843	51.121319
3444.162270	454939.861599	51.126324
3443.421827	454492.962213	51.131329
3442.509743	454037.760478	51.136333
3441.821907	453587.131122	51.141338
3441.134645	453140.703907	51.146343
3440.397636	452688.643800	51.151348
3439.757024	452235.798373	51.156353
3439.023572	451779.000870	51.161357
3438.745690	451334.198685	51.166362
3437.575028	450879.076070	51.171367
3436.839585	450427.224696	51.176372
3436.078134	449993.585827	51.181377
3435.224502	449543.613371	51.186381
3435.136510	449109.546974	51.191386
3434.153520	448669.828772	51.196391
3433.423771	448210.980859	51.201396
3432.585145	447771.222874	51.206401
3431.953676	447324.877087	51.211405
3431.671727	446879.330316	51.216410
3430.441774	446442.349849	51.221415
3429.851492	445988.054841	51.226420
3429.017905	445550.842943	51.231425
3428.255240	445118.839530	51.236429
3427.585299	444672.297409	51.241434
3426.877112	444236.564181	51.246439
3426.464651	443800.522459	51.251444
3425.310984	443373.371247	51.256449
3424.969599	442937.556392	51.261453
3424.487658	442500.486859	51.266458
3423.208142	442065.972067	51.271463
3422.683632	441624.121842	51.276468
3421.985585	441196.504729	51.281473
3420.783208	440764.137246	51.286477
3420.561570	440328.865718	51.291482
3419.744882	439921.246438	51.296487
3418.758524	439477.399716	51.301492
3417.813840	439062.501375	51.306497
3417.193724	438639.320227	51.311501
3416.714900	438211.844861	51.316506
3415.804085	437806.413960	51.321511
3415.103213	437389.494362	51.326516
3414.372996	436964.525069	51.331521
3413.907048	436559.333546	51.336525
3413.179621	436127.622192	51.341530
3412.626525	435711.158985	51.346535
3412.124269	435295.188602	51.351540
3411.020591	434885.272660	51.356545
3410.307426	434465.843805	51.361549
3409.845887	434054.645019	51.366554
3408.955928	433629.746307	51.371559
3408.699396	433220.532789	51.376564
3407.827115	432796.709181	51.381569
3406.609751	432387.329590	51.386573
3406.127124	431972.368242	51.391578
3405.259632	431573.279903	51.396583
3405.251298	431157.874989	51.401588
3404.401475	430750.696581	51.406593
3403.490749	430330.139529	51.411597
3402.903843	429915.974306	51.416602
3401.766850	429519.690264	51.421607
3401.253148	429103.773856	51.426612
3400.867988	428699.054765	51.431617
3399.810706	428281.687656	51.436621
3399.396787	427880.693555	51.441626
3398.436960	427476.402119	51.446631
3398.119176	427066.111193	51.451636
3397.051123	426664.795827	51.456641
3396.129054	426267.235420	51.461645
3395.886542	425859.961631	51.466650
3395.009642	425464.210743	51.471655
3394.344065	425052.293115	51.476660
3393.444199	424657.829292	51.481665
3392.804273	424261.159750	51.486669
3392.077484	423857.869064	51.491674
3391.067107	423461.957591	51.496679
3390.726199	423047.850055	51.501684
3389.722216	422665.997362	51.506689
3388.769777	422271.227880	51.511693
3388.593038	421879.174936	51.516698
3387.635795	421493.285266	51.521703
3386.992663	421103.123920	51.526708
3386.276790	420711.520688	51.531713
3385.683776	420328.630808	51.536717
3384.710197	419934.009140	51.541722
3383.908746	419547.153321	51.546727
3383.429970	419160.114119	51.551732
3382.563039	418785.502433	51.556737
3381.952285	418401.064806	51.561741
3381.571008	418008.024470	51.566746
3380.339245	417635.843211	51.571751
3379.726928	417252.533438	51.576756
3379.299748	416869.595711	51.581761
3378.446268	416496.806233	51.586765
3377.952245	416113.310025	51.591770
3376.840577	415730.668547	51.596775
3376.688776	415355.619172	51.601780
3375.542217	414975.259763	51.606785
3375.049181	414590.294944	51.611789
3374.569036	414215.536789	51.616794
3373.626912	413839.855957	51.621799
3372.928660	413470.432938	51.626804
3372.037376	413096.817977	51.631809
3371.703993	412718.587270	51.636813
3371.150335	412342.647944	51.641818
3370.125892	411984.844371	51.646823
3369.243917	411599.063237	51.651828
3368.531699	411226.183961	51.656833
3367.993720	410857.515991	51.661837
3367.696264	410486.238947	51.666842
3366.618454	410120.162898	51.671847
3365.979263	409743.568965	51.676852
3365.544419	409370.470219	51.681857
3364.615293	409004.331658	51.686861
3364.056909	408632.463102	51.691866
3363.051027	408262.465044	51.696871
3362.625442	407891.176311	51.701876
3361.818915	407531.607947	51.706881
3361.163181	407166.852572	51.711885
3360.755611	406798.012822	51.716890
3359.970147	406434.387466	51.721895
3359.282985	406054.654969	51.726900
3358.603851	405696.290299	51.731905
3358.041083	405327.965825	51.736909
3357.206237	404965.830514	51.741914
3356.024496	404607.507362	51.746919
3355.837722	404238.119346	51.751924
3354.959975	403874.605723	51.756929
3354.365562	403513.788068	51.761933
3353.942514	403143.789152	51.766938
3352.731293	402778.333121	51.771943
3352.834882	402415.537108	51.776948
3351.834262	402056.724227	51.781953
3351.088937	401688.691067	51.786957
3350.810821	401327.442704	51.791962
3349.531414	400959.739814	51.796967
3349.223915	400589.896352	51.801972
3348.343099	400233.026792	51.806977
3347.472765	399865.348412	51.811981
3347.040256	399504.053216	51.816986
3346.415455	399144.462137	51.821991
3345.600630	398783.143155	51.826996
3344.687027	398423.513559	51.832001
3344.103277	398063.726176	51.837005
3343.579397	397703.035658	51.842010
3342.553410	397354.978737	51.847015
3342.086332	396989.187192	51.852020
3340.977137	396629.365621	51.857025
3340.383317	396276.653121	51.862029
3340.063833	395924.401961	51.867034
3339.432837	395573.009892	51.872039
3339.117753	395200.819072	51.877044
3337.695661	394856.027482	51.882049
3337.456584	394501.486057	51.887053
3336.779118	394140.222121	51.892058
3335.751755	393783.611432	51.897063
3335.337857	393427.103390	51.902068
3334.517861	393076.300106	51.907073
3333.649840	392720.492149	51.912077
3332.950612	392368.213328	51.917082
3332.567711	392031.161496	51.922087
3332.151039	391664.338396	51.927092
3331.062518	391318.263454	51.932097
3330.350383	390963.124716	51.937101
3329.598305	390605.598612	51.942106
3328.863616	390271.687416	51.947111
3328.113359	389908.890628	51.952116
3327.318435	389565.091217	51.957121
3327.019525	389227.287151	51.962125
3326.238369	388874.655578	51.967130
3325.436640	388540.560656	51.972135
3324.896177	388186.841673	51.977140
3323.827696	387858.580169	51.982145
3323.017232	387509.296304	51.987149
3322.555051	387165.980596	51.992154
3321.849590	386827.073899	51.997159
3321.496306	386477.478896	52.002164
3320.849898	386145.218966	52.007169
3320.126025	385807.043132	52.012173
3319.583502	385455.866196	52.017178
3318.756642	385117.573138	52.022183
3318.393117	384768.344883	52.027188
3317.087796	384434.851301	52.032193
3316.801969	384082.984927	52.037197
3316.234121	383741.128847	52.042202
3315.108280	383400.654888	52.047207
3314.500096	383064.292174	52.052212
3313.593568	382726.015378	52.057217
3313.069245	382390.320029	52.062221
3312.462751	382053.948019	52.067226
3311.620164	381725.036663	52.072231
3311.044822	381391.425997	52.077236
3310.098994	381052.682681	52.082241
3309.600684	380719.333721	52.087245
3309.141823	380381.855410	52.092250
3308.324353	380056.028601	52.097255
3307.841155	379716.869696	52.102260
3307.305682	379382.319659	52.107265
3306.535253	379039.614057	52.112269
3305.692945	378704.038478	52.117274
3304.569522	378377.152293	52.122279
3304.494482	378030.945043	52.127284
3303.708537	377716.208759	52.132289
3303.206540	377375.862505	52.137293
3302.539637	377039.456491	52.142298
3301.826627	376714.755393	52.147303
3301.379516	376373.450748	52.152308
3300.568879	376034.846058	52.157313
3299.662796	375699.891020	52.162317
3298.975103	375357.725514	52.167322
3298.286181	375033.235932	52.172327
3297.468572	374697.648106	52.177332
3296.710152	374363.421762	52.182337
3295.927901	374043.187070	52.187341
3295.653942	373708.878747	52.192346
3294.515734	373383.073472	52.197351
3293.976216	373050.353515	52.202356
3293.412181	372735.823143	52.207361
3293.015663	372398.216615	52.212365
3292.118483	372080.223463	52.217370
3291.460633	371744.764393	52.222375
3290.971927	371413.473336	52.227380
3290.133156	371086.025495	52.232385
3289.314903	370759.106098	52.237389
3289.155558	370426.279705	52.242394
3287.945604	370093.616886	52.247399
3287.505419	369764.060603	52.252404
3286.564601	369440.203273	52.257409
3286.023751	369112.107997	52.262413
3286.003043	368784.156916	52.267418
3284.616860	368465.094665	52.272423
3284.158425	368115.811999	52.277428
3283.231481	367796.265139	52.282433
3282.603476	367476.999397	52.287437
3282.048970	367150.672376	52.292442
3281.736565	366829.825512	52.297447
3280.981267	366492.330983	52.302452
3279.962683	366175.152953	52.307457
3279.374569	365837.830541	52.312461
3278.994396	365508.436211	52.317466
3277.772925	365191.512265	52.322471
3277.362834	364860.057047	52.327476
3276.589050	364540.513412	52.332481
3275.749984	364214.337151	52.337485
3275.604486	363884.613971	52.342490
3274.502575	363561.044397	52.347495
3274.039695	363233.122334	52.352500
3273.237544	362917.413835	52.357505
3272.547783	362583.747244	52.362509
3272.194473	362263.001658	52.367514
3271.293760	361950.024699	52.372519
3270.617867	361620.649125	52.377524
3269.736552	361294.102666	52.382529
3269.108219	360971.686912	52.387533
3268.465747	360651.739379	52.392538
3267.671915	360343.722079	52.397543
3267.035629	360020.105168	52.402548
3266.171181	359707.234812	52.407553
3265.628512	359385.252765	52.412557
3265.491342	359067.606590	52.417562
3264.452592	358754.681265	52.422567
3263.606133	358429.127522	52.427572
3262.922162	358117.134373	52.432577
3262.655892	357798.558785	52.437581
3262.043644	357475.862560	52.442586
3261.150302	357151.859987	52.447591
3260.630463	356831.358818	52.452596
3259.834283	356525.735130	52.457601
3258.858355	356194.181476	52.462605
3258.597770	355863.224998	52.467610
3257.454761	355560.500412	52.472615
3257.009404	355242.827429	52.477620
3256.558730	354928.792384	52.482625
3255.715028	354610.542241	52.487629
3254.914999	354292.486788	52.492634
3254.116625	353978.882616	52.497639
3253.617194	353655.329635	52.502644
3252.862347	353342.147325	52.507649
3251.871215	353033.734040	52.512653
3251.601736	352716.297507	52.517658
3250.576428	352401.549004	52.522663
3250.122555	352089.253174	52.527668
3249.361554	351786.700435	52.532673
3248.861531	351480.516240	52.537677
3248.290607	351162.965315	52.542682
3247.241019	350858.518725	52.547687
3247.198447	350537.902823	52.552692
3246.082275	350236.415470	52.557697
3245.091579	349923.021127	52.562701
3245.094097	349605.497523	52.567706
3243.938734	349302.764075	52.572711
3243.775469	348989.996982	52.577716
3243.035967	348673.272516	52.582721
3242.068405	348354.571644	52.587725
3241.674968	348043.031795	52.592730
3240.717507	347740.640215	52.597735
3240.278294	347423.275704	52.602740
3239.268212	347117.860310	52.607745
3238.515695	346810.799028	52.612749
3238.086214	346498.925406	52.617754
3237.403758	346191.875132	52.622759
3236.843515	345886.687353	52.627764
3236.054584	345576.698122	52.632769
3235.362699	345263.739343	52.637773
3234.827765	344954.342897	52.642778
3233.925100	344644.213927	52.647783
3233.616010	344336.356548	52.652788
3233.109844	344028.248737	52.657793
3232.071330	343728.114095	52.662797
3231.545730	343411.555584	52.667802
3230.486244	343094.570768	52.672807
3229.837117	342798.391499	52.677812
3229.247098	342491.638013	52.682817
3228.462850	342177.175638	52.687821
3227.869804	341874.390323	52.692826
3226.955173	341581.225210	52.697831
3226.881330	341275.834790	52.702836
3225.817273	340970.904954	52.707841
3225.189854	340667.788177	52.712845
3224.745062	340360.899153	52.717850
3223.883381	340045.674416	52.722855
3223.212788	339750.501938	52.727860
3222.581275	339453.616385	52.732865
3222.097832	339150.978549	52.737869
3221.162167	338836.064898	52.742874
3220.198725	338531.030854	52.747879
3219.953226	338224.201689	52.752884
3218.968640	337927.848511	52.757889
3218.522207	337624.128425	52.762893
3217.897885	337313.867385	52.767898
3217.156435	337026.304870	52.772903
3216.369837	336725.663687	52.777908
3215.685454	336418.615390	52.782913
3215.041069	336119.832713	52.787917
3214.877579	335808.804322	52.792922
3213.708227	335519.571878	52.797927
3213.470569	335219.218862	52.802932
3212.591708	334904.277254	52.807937
3211.827297	334597.869666	52.812941
3211.152078	334297.836352	52.817946
3210.332348	334000.090286	52.822951
3209.526478	333697.147413	52.827956
3209.016878	333410.881960	52.832961
3208.459943	333108.533562	52.837965
3208.000606	332808.026829	52.842970
3207.123428	332508.297735	52.847975
3206.569205	332196.805586	52.852980
3205.892558	331907.836409	52.857985
3204.962420	331613.839978	52.862989
3204.399733	331303.821833	52.867994
3203.521408	331017.248588	52.872999
3202.790235	330711.124230	52.878004
3202.147350	330420.310714	52.883009
3201.689749	330121.014424	52.888013
3201.245649	329820.849177	52.893018
3200.431922	329532.452304	52.898023
3199.903181	329224.736723	52.903028
3199.198086	328929.675514	52.908033
3198.408890	328628.770823	52.913037
3197.952121	328325.088185	52.918042
3197.239805	328033.410706	52.923047
3196.434343	327727.489499	52.928052
3195.361540	327435.663099	52.933057
3194.975869	327137.972975	52.938061
3194.285784	326844.225228	52.943066
3193.469903	326549.707020	52.948071
3193.022749	326250.444721	52.953076
3192.440397	325955.810960	52.958081
3191.600758	325666.996285	52.963085
3191.180663	325361.488596	52.968090
3190.230695	325071.849037	52.973095
3189.350430	324771.351236	52.978100
3189.077937	324487.280090	52.983105
3188.455632	324181.850865	52.988109
3187.615751	323889.032556	52.993114
3186.836411	323605.547771	52.998119
3186.422110	323304.563506	53.003124
3185.576933	323010.953653	53.008129
3184.990353	322715.850576	53.013133
3184.280208	322422.293694	53.018138
3183.685190	322129.252273	53.023143
3183.436945	321824.264508	53.028148
3182.450092	321537.572034	53.033153
3181.460243	321242.171229	53.038157
3181.138757	320940.170950	53.043162
3180.490795	320649.067995	53.048167
3179.816490	320345.466491	53.053172
3179.340873	320047.128594	53.058177
3178.403588	319750.441395	53.063181
3177.828580	319449.876586	53.068186
3177.519863	319162.025196	53.073191
3176.682769	318853.759390	53.078196
3175.838766	318564.183000	53.083201
3175.183259	318273.200909	53.088205
3174.628478	317970.438301	53.093210
3173.918831	317671.824159	53.098215
3173.328329	317375.201771	53.103220
3172.653574	317076.783937	53.108225
3171.777848	316777.225683	53.113229
3171.032794	316475.456015	53.118234
3170.115280	316189.346963	53.123239
3169.697530	315884.875532	53.128244
3169.066459	315591.666153	53.133249
3168.262902	315303.423060	53.138253
3167.732423	314998.635729	53.143258
3167.049561	314712.561685	53.148263
3166.218324	314415.764749	53.153268
3165.624114	314127.994451	53.158273
3164.859173	313826.118086	53.163277
3164.223144	313528.472874	53.168282
3163.298091	313246.303553	53.173287
3163.083180	312951.543861	53.178292
3162.102156	312668.948973	53.183297
3161.174180	312385.555563	53.188301
3160.835939	312093.919619	53.193306
3159.850488	311807.961928	53.198311
3159.479098	311518.570527	53.203316
3158.889742	311239.296670	53.208321
3158.300811	310956.227873	53.213325
3157.669225	310656.969809	53.218330
3156.501868	310375.162434	53.223335
3156.136546	310092.387124	53.228340
3155.526565	309796.408291	53.233345
3154.931906	309522.682306	53.238349
3154.310970	309228.791853	53.243354
3153.684097	308948.321496	53.248359
3153.117503	308647.876574	53.253364
3152.035169	308350.975720	53.258369
3151.511033	308065.139424	53.263373
3150.887435	307780.998880	53.268378
3150.017807	307487.016191	53.273383
3149.694196	307197.912090	53.278388
3148.962511	306912.768053	53.283393
3147.962930	306630.084954	53.288397
3147.335086	306328.421740	53.293402
3146.616126	306051.804609	53.298407
3145.902483	305763.981297	53.303412
3145.352312	305484.815183	53.308417
3144.641408	305204.222381	53.313421
3144.097140	304911.073591	53.318426
3143.228369	304633.560431	53.323431
3142.915113	304352.801063	53.328436
3142.177142	304069.052446	53.333441
3141.153356	303787.156539	53.338445
3140.897535	303503.355935	53.343450
3140.038828	303216.950784	53.348455
3139.051301	302926.236243	53.353460
3138.653546	302652.948338	53.358465
3137.982159	302370.637335	53.363469
3137.202839	302080.779461	53.368474
3136.756840	301804.212491	53.373479
3136.406698	301513.725344	53.378484
3135.421214	301240.171309	53.383489
3134.553265	300952.056982	53.388493
3134.166346	300664.910113	53.393498
3133.239409	300384.749537	53.398503
3132.780364	300096.416125	53.403508
3131.834006	299819.186252	53.408513
3131.126566	299537.283205	53.413517
3130.814899	299256.717697	53.418522
3129.579212	298982.308033	53.423527
3129.010196	298700.279784	53.428532
3128.431123	298420.239049	53.433537
3128.063758	298147.065813	53.438541
3127.270972	297872.049466	53.443546
3126.284768	297594.669421	53.448551
3125.651024	297315.425024	53.453556
3125.050059	297040.809963	53.458561
3124.448677	296761.152116	53.463565
3124.122979	296485.473983	53.468570
3122.904476	296210.395131	53.473575
3122.705723	295936.809854	53.478580
3121.790833	295661.911361	53.483585
3121.322010	295378.384964	53.488589
3120.451156	295108.113716	53.493594
3119.804893	294830.854041	53.498599
3119.386574	294548.464483	53.503604
3118.572844	294273.726324	53.508609
3118.062208	294004.975561	53.513613
3117.573682	293714.089926	53.518618
3116.395305	293442.082441	53.523623
3116.078047	293165.659832	53.528628
3115.239610	292888.631734	53.533633
3114.568675	292604.624191	53.538637
3113.991170	292317.927428	53.543642
3112.958100	292061.252096	53.548647
3112.409405	291771.315731	53.553652
3111.737841	291504.701206	53.558657
3111.105134	291225.295543	53.563661
3110.693989	290955.455760	53.568666
3109.582944	290684.427601	53.573671
3109.415920	290395.651642	53.578676
3108.784871	290120.701312	53.583681
3107.979082	289848.579788	53.588685
3107.043651	289579.127141	53.593690
3106.625819	289304.931722	53.598695
3105.784610	289022.755230	53.603700
3105.028769	288748.205271	53.608705
3104.418005	288474.752671	53.613709
3104.005345	288204.732085	53.618714
3103.324385	287930.984476	53.623719
3102.681951	287652.518971	53.628724
3101.915249	287378.682567	53.633729
3101.138426	287106.935895	53.638733
3100.955432	286824.092877	53.643738
3100.163205	286549.190158	53.648743
3099.343952	286272.330460	53.653748
3098.645890	286002.455055	53.658753
3097.832258	285720.882457	53.663757
3097.606688	285440.082485	53.668762
3096.485108	285165.663774	53.673767
3096.169033	284881.261249	53.678772
3095.238542	284609.536983	53.683777
3094.462909	284343.008984	53.688781
3093.801647	284063.499448	53.693786
3093.347177	283791.903055	53.698791
3092.709712	283510.428350	53.703796
3091.822658	283241.727046	53.708801
3090.888108	282964.221118	53.713805
3090.773116	282691.984579	53.718810
3089.518679	282423.340961	53.723815
3089.115805	282153.747449	53.728820
3088.473417	281878.512293	53.733825
3087.871482	281604.467604	53.738829
3087.355959	281327.607602	53.743834
3086.255811	281068.209347	53.748839
3085.580174	280792.265830	53.753844
3085.022707	280527.229383	53.758849
3084.647917	280259.922712	53.763853
3083.932220	279978.433115	53.768858
3082.874013	279707.286816	53.773863
3082.194226	279435.774911	53.778868
3081.749804	279174.285653	53.783873
3080.736618	278911.944006	53.788877
3080.487041	278641.102345	53.793882
3079.634310	278381.765888	53.798887
3078.935191	278109.288855	53.803892
3078.427493	277842.104345	53.808897
3077.822492	277579.111988	53.813901
3077.182405	277294.196868	53.818906
3076.132371	277013.294172	53.823911
3075.966887	276743.788602	53.828916
3074.911891	276478.626058	53.833921
3074.164018	276207.506207	53.838925
3073.893938	275942.524989	53.843930
3073.001270	275676.266990	53.848935
3072.579539	275411.386133	53.853940
3071.726442	275146.395254	53.858945
3070.941107	274878.439306	53.863949
3070.431248	274595.668082	53.868954
3069.804911	274340.472091	53.873959
3068.715734	274076.715573	53.878964
3068.326587	273807.296156	53.883969
3067.834630	273544.744019	53.888973
3067.049913	273273.375236	53.893978
3065.978375	273011.959073	53.898983
3065.598236	272745.314357	53.903988
3064.785116	272487.983224	53.908993
3064.172697	272231.944713	53.913997
3063.711428	271967.095725	53.919002
3062.938025	271695.037698	53.924007
3062.179367	271423.359414	53.929012
3061.437772	271168.742283	53.934017
3060.783236	270897.684338	53.939021
3060.312698	270636.810142	53.944026
3059.572785	270387.235651	53.949031
3058.965291	270115.584687	53.954036
3058.272465	269862.819337	53.959041
3057.622070	269593.722151	53.964045
3057.324597	269326.173694	53.969050
3056.503679	269066.246795	53.974055
3055.792584	268796.395438	53.979060
3055.170268	268530.834268	53.984065
3054.496149	268268.694150	53.989069
3053.898472	267998.621406	53.994074
3052.919818	267731.054032	53.999079
3052.383777	267467.287890	54.004084
3051.429871	267216.500400	54.009089
3050.680061	266950.476192	54.014093
3050.324091	266689.585289	54.019098
3049.754314	266426.487157	54.024103
3049.311306	266167.520408	54.029108
3048.616177	265901.946511	54.034113
3047.738690	265637.624097	54.039117
3047.257458	265363.408414	54.044122
3046.554091	265115.383817	54.049127
3045.983166	264842.074038	54.054132
3045.281395	264579.660018	54.059137
3044.316037	264319.197993	54.064141
3044.101740	264041.146168	54.069146
3043.186538	263784.191146	54.074151
3042.592372	263515.215512	54.079156
3041.588364	263254.683916	54.084161
3040.809058	262986.782161	54.089165
3040.316922	262720.312293	54.094170
3039.424954	262466.054127	54.099175
3038.791325	262204.547837	54.104180
3038.224422	261942.878382	54.109185
3037.404023	261701.954653	54.114189
3036.646209	261438.125588	54.119194
3036.138914	261186.456187	54.124199
3035.562828	260922.955343	54.129204
3034.851879	260666.989078	54.134209
3034.016702	260409.387292	54.139213
3033.476566	260146.314401	54.144218
3032.506657	259892.911116	54.149223
3031.991494	259640.582125	54.154228
3031.549917	259382.104005	54.159233
3031.022217	259127.332574	54.164237
3030.577211	258863.965704	54.169242
3029.264612	258612.604338	54.174247
3028.208177	258347.806719	54.179252
3027.574396	258114.394909	54.184257
3026.736723	257857.509056	54.189261
3026.567624	257606.935454	54.194266
3025.712369	257369.764749	54.199271
3025.007420	257121.212002	54.204276
3024.712736	256871.703214	54.209281
3023.863969	256627.248546	54.214285
3023.340761	256374.567577	54.219290
3022.593473	256118.917215	54.224295
3022.260924	255867.505471	54.229300
3021.621315	255618.383742	54.234305
3020.677937	255370.991224	54.239309
3020.113104	255114.549139	54.244314
3019.173781	254862.292330	54.249319
3018.770140	254613.287230	54.254324
3018.123193	254372.164823	54.259329
3017.486057	254112.399228	54.264333
3016.868878	253860.245464	54.269338
3015.885318	253611.358865	54.274343
3015.555418	253352.818981	54.279348
3014.922923	253110.014999	54.284353
3013.984050	252848.949093	54.289357
3013.571804	252594.727182	54.294362
3012.897284	252353.178702	54.299367
3012.145817	252090.734446	54.304372
3011.562620	251836.336905	54.309377
3010.958476	251590.347070	54.314381
3010.421508	251330.875040	54.319386
3009.512383	251085.341651	54.324391
3008.989026	250817.871684	54.329396
3008.155136	250578.821097	54.334401
3007.440810	250328.266489	54.339405
3006.943709	250065.810457	54.344410
3006.001506	249823.773032	54.349415
3005.837323	249567.096912	54.354420
3005.207603	249323.966628	54.359425
3004.568476	249057.256324	54.364429
3003.862238	248800.794556	54.369434
3003.082942	248547.196992	54.374439
3002.419099	248288.946699	54.379444
3001.612303	248036.041904	54.384449
3000.976271	247778.552044	54.389453
3000.426551	247524.614212	54.394458
2999.491692	247275.321671	54.399463
2998.984220	247013.508988	54.404468
2998.102845	246760.134272	54.409473
2997.390566	246517.938245	54.414477
2997.066242	246270.613485	54.419482
2996.218584	246024.823550	54.424487
2995.840180	245757.288328	54.429492
2994.965255	245504.271309	54.434497
2993.935593	245257.441949	54.439501
2993.635488	245004.971474	54.444506
2992.771008	244756.334254	54.449511
2992.044858	244515.035143	54.454516
2991.254661	244263.585841	54.459521
2990.612747	244019.523995	54.464525
2989.939817	243770.756393	54.469530
2988.991720	243522.745849	54.474535
2988.490327	243279.554404	54.479540
2988.135360	243044.030755	54.484545
2987.144476	242795.926499	54.489549
2986.822094	242541.936284	54.494554
2986.123501	242306.239194	54.499559
2985.461173	242059.739588	54.504564
2984.812625	241809.393056	54.509569
2984.181270	241557.592796	54.514573
2983.452484	241307.769274	54.519578
2982.559437	241069.125899	54.524583
2981.906337	240822.550892	54.529588
2981.227426	240575.369317	54.534593
2980.592455	240337.908833	54.539597
2980.294104	240094.207602	54.544602
2979.430704	239846.623838	54.549607
2978.526125	239596.500653	54.554612
2977.933351	239356.921893	54.559617
2977.125367	239112.412119	54.564621
2976.761570	238868.902048	54.569626
2975.629946	238624.877442	54.574631
2975.237150	238384.963471	54.579636
2974.757567	238151.709927	54.584641
2973.933246	237906.772432	54.589645
2973.469130	237655.768903	54.594650
2972.475226	237418.753224	54.599655
2971.860544	237168.920522	54.604660
2971.381339	236936.382465	54.609665
2970.733500	236692.667463	54.614669
2970.327685	236442.879751	54.619674
2969.318659	236208.644666	54.624679
2969.117229	235963.791161	54.629684
2968.219800	235712.427844	54.634689
2967.332835	235476.112492	54.639693
2966.864302	235223.027305	54.644698
2965.971514	234990.508049	54.649703
2965.428629	234737.868697	54.654708
2964.838070	234493.793221	54.659713
2963.952718	234262.012875	54.664717
2963.593020	234012.376452	54.669722
2962.744815	233772.239385	54.674727
2962.026916	233523.806730	54.679732
2961.306619	233286.578843	54.684737
2960.602413	233050.825832	54.689741
2960.109923	232800.678739	54.694746
2959.298691	232561.302640	54.699751
2958.783625	232320.785335	54.704756
2958.264886	232085.208992	54.709761
2957.451009	231839.774947	54.714765
2957.086573	231590.425510	54.719770
2956.187319	231363.415718	54.724775
2955.631947	231114.021372	54.729780
2954.957684	230865.741397	54.734785
2954.143693	230623.671567	54.739789
2953.574510	230383.244122	54.744794
2952.764144	230143.262882	54.749799
2952.778611	229897.269904	54.754804
2951.615395	229646.651699	54.759809
2950.723957	229406.608838	54.764813
2949.996113	229166.438863	54.769818
2949.234063	228922.633887	54.774823
2948.635159	228685.678447	54.779828
2948.160330	228438.493811	54.784833
2947.111184	228210.522552	54.789837
2946.655999	227968.886774	54.794842
2945.649185	227728.484771	54.799847
2945.319011	227491.591834	54.804852
2944.855796	227260.245742	54.809857
2944.240131	227027.294876	54.814861
2943.448552	226774.716359	54.819866
2942.426389	226555.096480	54.824871
2942.005991	226310.582703	54.829876
2941.409290	226073.506725	54.834881
2940.445561	225841.645384	54.839885
2940.046776	225595.284332	54.844890
2939.129374	225360.692666	54.849895
2938.631972	225121.312180	54.854900
2938.075974	224890.038180	54.859905
2937.147522	224655.195655	54.864909
2936.742115	224414.478703	54.869914
2935.914107	224178.106739	54.874919
2935.427500	223954.538933	54.879924
2934.807221	223709.758958	54.884929
2934.075180	223461.623935	54.889933
2933.447871	223226.877901	54.894938
2932.900103	222998.306780	54.899943
2932.173328	222753.559326	54.904948
2931.338977	222516.136680	54.909953
2930.522493	222286.948205	54.914957
2930.078006	222042.463788	54.919962
2929.222866	221809.463859	54.924967
2928.727069	221579.704763	54.929972
2928.349373	221338.025285	54.934977
2927.309516	221111.396153	54.939981
2926.832762	220874.227428	54.944986
2925.875591	220632.629200	54.949991
2925.319408	220394.812602	54.954996
2924.943991	220165.458778	54.960001
2923.935069	219936.753333	54.965005
2923.769291	219697.324117	54.970010
2922.667952	219463.708427	54.975015
2922.229586	219221.981676	54.980020
2921.632214	218989.255122	54.985025
2921.109974	218744.793664	54.990029
2920.476009	218503.240268	54.995034
2919.607987	218270.342453	55.000039
2918.958043	218028.436742	55.005044
2918.220328	217790.962768	55.010049
2917.299115	217549.827178	55.015053
2916.708092	217310.676773	55.020058
2916.089048	217082.478604	55.025063
2915.320601	216854.419386	55.030068
2914.666656	216617.356106	55.035073
2913.927204	216385.080515	55.040077
2913.591889	216147.344646	55.045082
2912.734548	215924.814127	55.050087
2912.045291	215677.003730	55.055092
2911.258266	215449.410258	55.060097
2910.411444	215209.709253	55.065101
2910.372145	214980.980628	55.070106
2909.471208	214757.747961	55.075111
2908.747124	214509.807260	55.080116
2908.461490	214274.335662	55.085121
2907.312563	214044.373011	55.090125
2906.789000	213811.486399	55.095130
2905.649882	213587.480677	55.100135
2905.431469	213349.736001	55.105140
2904.803395	213125.243596	55.110145
2903.579599	212899.764374	55.115149
2903.106589	212656.474768	55.120154
2902.542622	212433.171010	55.125159
2901.946897	212212.622322	55.130164
2901.159380	211981.476767	55.135169
2900.568237	211759.668795	55.140173
2900.046403	211525.478960	55.145178
2899.096467	211302.265642	55.150183
2898.967082	211067.022537	55.155188
2898.372169	210835.825111	55.160193
2897.370569	210604.591093	55.165197
2896.593754	210373.665968	55.170202
2895.936539	210139.222609	55.175207
2895.153600	209906.250984	55.180212
2894.712606	209690.128404	55.185217
2893.761048	209454.321424	55.190221
2893.358182	209230.214171	55.195226
2892.328651	209004.196006	55.200231
2891.683315	208773.217744	55.205236
2891.017290	208557.211075	55.210241
2890.426425	208342.631453	55.215245
2889.666514	208106.964686	55.220250
2889.220420	207884.116419	55.225255
2888.468452	207667.299205	55.230260
2887.994508	207449.484195	55.235265
2887.040706	207214.017023	55.240269
2886.653651	206983.640950	55.245274
2885.919216	206762.967872	55.250279
2885.311281	206536.497508	55.255284
2884.678119	206310.451981	55.260289
2883.843117	206083.408391	55.265293
2883.704807	205856.700778	55.270298
2882.656108	205642.852288	55.275303
2882.373464	205409.920368	55.280308
2881.815424	205172.145916	55.285313
2880.840229	204943.347152	55.290317
2880.467446	204700.836401	55.295322
2879.389485	204487.900329	55.300327
2878.934370	204244.144582	55.305332
2878.319826	204007.592829	55.310337
2877.179848	203788.484080	55.315341
2876.843063	203567.683627	55.320346
2876.093387	203335.559350	55.325351
2875.455705	203100.071270	55.330356
2874.528769	202874.467329	55.335361
2874.159549	202656.208041	55.340365
2873.598255	202420.914288	55.345370
2872.898751	202202.263636	55.350375
2872.237906	201972.294283	55.355380
2871.481270	201739.426794	55.360385
2870.972739	201505.477457	55.365389
2870.200142	201282.947830	55.370394
2869.429021	201058.191841	55.375399
2868.752070	200828.089759	55.380404
2867.972012	200609.330833	55.385409
2867.294465	200383.926476	55.390413
2866.931409	200152.594012	55.395418
2865.898538	199935.163086	55.400423
2865.077733	199701.321731	55.405428
2864.784525	199487.007727	55.410433
2864.085312	199261.076955	55.415437
2863.516083	199036.004588	55.420442
2862.674408	198818.064285	55.425447
2862.191308	198589.747915	55.430452
2861.295301	198367.847768	55.435457
2860.525005	198152.647497	55.440461
2860.560646	197913.791800	55.445466
2859.590978	197690.137347	55.450471
2858.772510	197475.507340	55.455476
2858.450802	197247.718323	55.460481
2857.567799	197012.460615	55.465485
2856.905548	196785.401941	55.470490
2856.008945	196566.359778	55.475495
2855.182303	196343.999032	55.480500
2855.021535	196118.034504	55.485505
2853.815469	195898.013459	55.490509
2853.569523	195669.468555	55.495514
2852.545077	195457.729732	55.500519
2851.868117	195230.960105	55.505524
2851.165649	195006.943978	55.510529
2850.456185	194787.866969	55.515533
2850.042771	194573.731918	55.520538
2849.287392	194351.801091	55.525543
2848.623549	194136.053394	55.530548
2848.299060	193906.867126	55.535553
2847.161963	193689.529423	55.540557
2846.826186	193462.968105	55.545562
2846.172225	193256.205724	55.550567
2845.285183	193026.590867	55.555572
2844.661138	192806.007488	55.560577
2843.994318	192581.589283	55.565581
2843.590282	192360.845791	55.570586
2842.789239	192154.009477	55.575591
2842.215841	191920.952831	55.580596
2841.761496	191699.609519	55.585601
2840.834973	191478.227471	55.590605
2840.287304	191255.959398	55.595610
2839.831644	191034.733799	55.600615
2839.151283	190816.394806	55.605620
2838.177792	190579.298270	55.610625
2837.532061	190356.998927	55.615629
2837.142035	190139.634845	55.620634
2836.053263	189918.527317	55.625639
2835.663918	189685.655760	55.630644
2834.711264	189462.378581	55.635649
2834.049499	189252.440846	55.640653
2833.574657	189027.575995	55.645658
2832.976525	188807.515490	55.650663
2832.167616	188577.451169	55.655668
2831.646258	188357.584150	55.660673
2831.069482	188136.670954	55.665677
2830.371384	187903.729773	55.670682
2829.411789	187690.411033	55.675687
2829.011317	187466.254273	55.680692
2828.425711	187244.888654	55.685697
2827.288949	187026.092223	55.690701
2827.132224	186799.775430	55.695706
2825.896104	186567.180558	55.700711
2825.491399	186358.907049	55.705716
2824.657502	186144.748536	55.710721
2823.959042	185930.684064	55.715725
2823.572494	185700.579726	55.720730
2822.790047	185492.242740	55.725735
2822.425865	185274.858860	55.730740
2821.887234	185053.534459	55.735745
2820.601603	184842.519512	55.740749
2820.497481	184610.200521	55.745754
2819.729996	184389.933325	55.750759
2818.856783	184161.109660	55.755764
2818.272573	183957.238994	55.760769
2817.278653	183735.636940	55.765773
2817.212434	183509.500192	55.770778
2816.310500	183290.849829	55.775783
2815.643415	183067.113029	55.780788
2815.108009	182851.663387	55.785793
2814.005732	182636.864299	55.790797
2813.614128	182415.745843	55.795802
2812.765777	182192.143926	55.800807
2812.055352	181967.363696	55.805812
2811.529710	181753.520679	55.810817
2810.861151	181544.026390	55.815821
2810.270250	181322.029092	55.820826
2809.197915	181107.270881	55.825831
2808.602798	180890.415572	55.830836
2808.053963	180676.479725	55.835841
2807.313020	180467.765295	55.840845
2806.816767	180253.505192	55.845850
2805.980918	180038.116951	55.850855
2805.469286	179817.577616	55.855860
2804.471497	179603.272977	55.860865
2803.833697	179390.057199	55.865869
2803.596088	179178.712542	55.870874
2802.601186	178971.393914	55.875879
2801.739318	178754.553438	55.880884
2801.775812	178554.158472	55.885889
2800.476960	178335.188812	55.890893
2800.073267	178122.400205	55.895898
2799.477404	177909.274236	55.900903
2798.869682	177697.753892	55.905908
2798.134263	177478.877501	55.910913
2797.610875	177267.396840	55.915917
2797.108016	177047.481024	55.920922
2796.329879	176839.833257	55.925927
2795.648193	176622.046697	55.930932
2795.337468	176403.159542	55.935937
2794.302070	176182.391417	55.940941
2793.800623	175966.029729	55.945946
2793.301792	175747.595557	55.950951
2792.650479	175531.666888	55.955956
2791.933562	175310.636753	55.960961
2791.001509	175098.277957	55.965965
2790.549350	174858.257295	55.970970
2789.909375	174654.134436	55.975975
2789.076208	174439.919186	55.980980
2788.553001	174215.646475	55.985985
2787.487330	173995.518119	55.990989
2786.994283	173775.923456	55.995994
2786.494631	173570.117703	56.000999
2785.677912	173350.538465	56.006004
2784.974033	173131.858260	56.011009
2784.290083	172922.651094	56.016013
2783.751706	172690.554886	56.021018
2782.759421	172488.355605	56.026023
2781.998074	172276.200785	56.031028
2781.524742	172070.843679	56.036033
2780.879936	171857.756941	56.041037
2780.336436	171637.228149	56.046042
2779.383077	171428.974454	56.051047
2778.743193	171214.745805	56.056052
2778.048125	170999.153569	56.061057
2777.467569	170799.542925	56.066061
2777.163437	170572.025723	56.071066
2776.137023	170364.971945	56.076071
2775.526455	170162.380730	56.081076
2774.962505	169942.665862	56.086081
2774.177471	169733.122784	56.091085
2773.930463	169512.864169	56.096090
2772.761024	169311.688480	56.101095
2772.150321	169103.036810	56.106100
2771.678696	168890.129532	56.111105
2770.829085	168679.012783	56.116109
2770.211593	168456.746038	56.121114
2769.747172	168256.227176	56.126119
2768.876829	168044.443217	56.131124
2768.268613	167829.541519	56.136129
2767.707238	167626.129243	56.141133
2767.138594	167406.671184	56.146138
2766.321264	167203.975673	56.151143
2765.846094	166983.894866	56.156148
2764.685816	166768.336359	56.161153
2764.220233	166564.583975	56.166157
2763.661990	166346.389297	56.171162
2762.971541	166148.498701	56.176167
2762.111677	165933.507743	56.181172
2762.073385	165721.846560	56.186177
2761.350670	165513.067014	56.191181
2760.686906	165294.907880	56.196186
2759.668927	165081.599896	56.201191
2759.175850	164872.965573	56.206196
2758.509903	164652.470901	56.211201
2757.826532	164437.613190	56.216205
2757.327281	164225.130744	56.221210
2756.396382	164011.471810	56.226215
2755.758506	163805.117031	56.231220
2755.145278	163585.968175	56.236225
2754.379279	163381.161876	56.241229
2753.827404	163169.138886	56.246234
2753.079775	162957.911024	56.251239
2752.737733	162746.429412	56.256244
2751.782340	162534.067161	56.261249
2751.329451	162321.245107	56.266253
2750.700534	162103.251947	56.271258
2749.942241	161894.371422	56.276263
2749.337920	161674.368065	56.281268
2748.478727	161462.302001	56.286273
2747.822428	161248.692051	56.291277
2747.192819	161034.926573	56.296282
2746.516583	160834.544956	56.301287
2745.713098	160621.178197	56.306292
2745.386302	160406.147955	56.311297
2744.941906	160187.425194	56.316301
2744.244299	159970.358538	56.321306
2743.503390	159755.346970	56.326311
2742.691524	159537.093262	56.331316
2742.100761	159328.709714	56.336321
2741.383235	159034.239312	56.341325
2740.871447	158821.371119	56.346330
2739.818050	158609.772350	56.351335
2739.202666	158392.778635	56.356340
2738.711558	158179.427953	56.361345
2738.095953	157966.555964	56.366349
2737.397603	157756.978325	56.371354
2736.964600	157538.041362	56.376359
2736.387506	157326.616446	56.381364
2735.569950	157106.370137	56.386369
2734.344887	156885.617716	56.391373
2734.183677	156670.215420	56.396378
2733.448250	156462.736329	56.401383
2732.897218	156245.834800	56.406388
2732.104853	156030.879720	56.411393
2731.304148	155817.872280	56.416397
2730.531750	155611.065222	56.421402
2729.914640	155396.772808	56.426407
2729.318958	155180.851205	56.431412
2728.621842	154966.345351	56.436417
2728.250033	154762.352867	56.441421
2727.593500	154541.741566	56.446426
2726.399123	154336.292984	56.451431
2726.078277	154115.504158	56.456436
2725.408150	153898.522011	56.461441
2724.522989	153688.337823	56.466445
2723.847181	153482.494493	56.471450
2722.875949	153268.716529	56.476455
2722.550496	153062.477061	56.481460
2721.799672	152855.797806	56.486465
2721.002127	152649.445007	56.491469
2721.070490	152439.867528	56.496474
2719.928202	152232.364381	56.501479
2719.118104	152015.480154	56.506484
2718.567421	151808.864655	56.511489
2717.965130	151600.542681	56.516493
2717.159096	151388.847858	56.521498
2716.357258	151194.084121	56.526503
2715.949415	150991.912482	56.531508
2714.977193	150778.481155	56.536513
2714.783304	150575.540975	56.541517
2714.358660	150349.760269	56.546522
2713.380897	150149.781283	56.551527
2712.761983	149933.973525	56.556532
2712.115080	149725.975530	56.561537
2711.141461	149512.196799	56.566541
2710.447727	149307.221133	56.571546
2709.832057	149102.882586	56.576551
2709.366501	148890.679710	56.581556
2708.615895	148687.585282	56.586561
2707.886095	148478.769578	56.591565
2707.412349	148273.956238	56.596570
2706.689658	148067.594979	56.601575
2705.814801	147858.386870	56.606580
2705.563185	147651.724878	56.611585
2704.704509	147435.628615	56.616589
2704.246239	147226.892403	56.621594
2703.383865	147025.224169	56.626599
2702.578299	146816.761711	56.631604
2702.132482	146604.901230	56.636609
2701.273288	146396.551691	56.641613
2700.861299	146183.773635	56.646618
2700.082132	145989.444322	56.651623
2699.017983	145771.447517	56.656628
2699.199109	145553.343874	56.661633
2698.169671	145351.966911	56.666637
2697.565329	145140.014265	56.671642
2696.699392	144936.275763	56.676647
2696.157048	144731.051315	56.681652
2695.854768	144512.497742	56.686657
2694.471188	144316.177727	56.691661
2694.234430	144090.830761	56.696666
2693.435145	143883.022094	56.701671
2692.532770	143671.634918	56.706676
2692.111215	143461.456450	56.711681
2691.400243	143261.402193	56.716685
2690.934384	143051.678277	56.721690
2689.924016	142848.573550	56.726695
2689.271907	142653.711136	56.731700
2688.956762	142435.186915	56.736705
2687.991054	142227.974832	56.741709
2687.682513	142015.806009	56.746714
2686.949307	141814.887884	56.751719
2685.841698	141607.575406	56.756724
2685.436973	141403.393147	56.761729
2684.747333	141192.472121	56.766733
2684.324216	140978.422665	56.771738
2683.180412	140789.507666	56.776743
2682.661953	140588.461936	56.781748
2682.275426	140369.938364	56.786753
2681.405686	140171.517700	56.791757
2680.808150	139958.837204	56.796762
2680.520619	139755.130274	56.801767
2679.670940	139549.607916	56.806772
2678.949168	139338.997109	56.811777
2678.195770	139134.796429	56.816781
2677.493758	138916.905118	56.821786
2676.761505	138715.905736	56.826791
2676.080008	138509.715868	56.831796
2675.544935	138301.191860	56.836801
2674.785179	138095.970144	56.841805
2674.628823	137884.123806	56.846810
2673.834428	137684.221151	56.851815
2672.769873	137474.770422	56.856820
2672.206254	137260.464778	56.861825
2671.057800	137056.137648	56.866829
2670.716470	136854.745867	56.871834
2669.802757	136653.903518	56.876839
2669.088814	136455.432033	56.881844
2668.960787	136256.030555	56.886849
2668.070205	136061.045318	56.891853
2667.561523	135852.851977	56.896858
2666.675270	135653.841519	56.901863
2666.288862	135439.012882	56.906868
2665.353631	135238.755307	56.911873
2664.495911	135038.677383	56.916877
2663.925153	134827.083839	56.921882
2663.221313	134634.746324	56.926887
2662.307607	134435.875565	56.931892
2661.794611	134235.519880	56.936897
2661.124371	134046.382232	56.941901
2660.608205	133837.632823	56.946906
2660.150117	133644.030718	56.951911
2659.565273	133450.043495	56.956916
2658.672761	133237.343857	56.961921
2658.111832	133044.867242	56.966925
2657.983396	132831.655739	56.971930
2657.151050	132639.758369	56.976935
2656.300519	132430.144847	56.981940
2655.860201	132222.855957	56.986945
2655.130862	132014.521948	56.991949
2654.503522	131812.016430	56.996954
2653.757420	131603.942128	57.001959
2653.314640	131398.514167	57.006964
2652.661466	131188.002051	57.011969
2651.673685	130979.500641	57.016973
2651.361254	130768.391459	57.021978
2650.386461	130568.528377	57.026983
2649.796545	130354.011343	57.031988
2649.039560	130154.929595	57.036993
2648.535683	129961.613791	57.041997
2647.845988	129742.341416	57.047002
2646.793676	129538.611265	57.052007
2646.678500	129328.612048	57.057012
2645.889437	129129.745876	57.062017
2645.073516	128920.648239	57.067021
2644.696294	128709.018647	57.072026
2643.798152	128509.437519	57.077031
2643.149098	128295.288549	57.082036
2642.460105	128078.150176	57.087041
2641.501778	127878.608519	57.092045
2640.878061	127682.685748	57.097050
2640.230113	127483.237464	57.102055
2639.962632	127269.480474	57.107060
2639.129250	127074.331864	57.112065
2638.180853	126875.507098	57.117069
2637.778599	126664.748006	57.122074
2636.878420	126461.422751	57.127079
2636.197723	126255.041637	57.132084
2635.897881	126053.237168	57.137089
2634.955801	125858.089030	57.142093
2634.632472	125652.265420	57.147098
2633.800724	125458.474217	57.152103
2633.191606	125238.615203	57.157108
2632.534204	125035.960555	57.162113
2631.294368	124839.292178	57.167117
2630.910281	124628.088750	57.172122
2630.411135	124432.144098	57.177127
2629.666052	124241.014659	57.182132
2629.176077	124031.813705	57.187137
2628.308935	123833.239545	57.192141
2627.689565	123628.963959	57.197146
2627.251312	123440.750367	57.202151
2626.662061	123229.831663	57.207156
2626.043996	123018.563626	57.212161
2625.100088	122830.713807	57.217165
2624.629375	122608.708263	57.222170
2623.703408	122411.296786	57.227175
2623.071232	122210.119687	57.232180
2622.683775	122000.931021	57.237185
2621.844769	121807.586272	57.242189
2621.095740	121598.635836	57.247194
2620.208996	121402.825539	57.252199
2619.785762	121201.965792	57.257204
2619.421017	120998.622295	57.262209
2618.496859	120801.679601	57.267213
2617.788642	120592.540176	57.272218
2616.878446	120398.353586	57.277223
2616.373574	120184.157098	57.282228
2616.077767	119990.803034	57.287233
2615.023080	119791.755487	57.292237
2614.655627	119574.939328	57.297242
2613.873072	119392.344797	57.302247
2613.143376	119187.505090	57.307252
2612.538512	118974.591289	57.312257
2611.808269	118783.797144	57.317261
2611.297427	118581.200165	57.322266
2610.637199	118381.148631	57.327271
2609.803988	118175.393765	57.332276
2609.196771	117971.731292	57.337281
2608.545222	117775.523586	57.342285
2608.107912	117566.524140	57.347290
2607.300181	117372.483482	57.352295
2606.473244	117172.347090	57.357300
2606.017628	116963.437946	57.362305
2604.983039	116769.285432	57.367309
2604.656786	116571.200842	57.372314
2603.793804	116370.390851	57.377319
2602.897355	116167.493044	57.382324
2602.353860	115972.322944	57.387329
2601.739089	115782.059516	57.392333
2601.186278	115573.354818	57.397338
2600.389720	115382.577297	57.402343
2599.733381	115190.566647	57.407348
2599.177126	114990.239367	57.412353
2598.147815	114794.469764	57.417357
2597.748106	114587.659389	57.422362
2596.992218	114401.300406	57.427367
2596.459081	114192.369075	57.432372
2595.753174	114005.725812	57.437377
2594.760737	113810.706916	57.442381
2594.579852	113613.682222	57.447386
2593.733268	113423.974608	57.452391
2592.836168	113229.732109	57.457396
2592.396937	113031.293145	57.462401
2591.643702	112840.972192	57.467405
2590.974788	112641.696861	57.472410
2590.125127	112457.950207	57.477415
2589.749597	112259.811888	57.482420
2588.966592	112068.739933	57.487425
2588.036586	111882.928579	57.492429
2587.773257	111679.477775	57.497434
2586.795716	111490.909838	57.502439
2586.601136	111299.579168	57.507444
2585.994778	111096.079610	57.512449
2585.208531	110910.589087	57.517453
2584.493006	110711.603114	57.522458
2583.842668	110521.334334	57.527463
2583.063513	110325.122120	57.532468
2582.765832	110130.377241	57.537473
2581.798958	109941.425954	57.542477
2581.320471	109745.976632	57.547482
2580.790840	109551.971136	57.552487
2579.634485	109353.484812	57.557492
2579.486477	109146.927098	57.562497
2578.572821	108949.033812	57.567501
2578.288406	108752.438444	57.572506
2577.262940	108563.075548	57.577511
2576.454592	108359.630612	57.582516
2575.790800	108160.282703	57.587521
2575.098038	107970.897055	57.592525
2574.863914	107778.565713	57.597530
2573.985249	107583.019419	57.602535
2573.154863	107393.520482	57.607540
2572.673309	107190.211197	57.612545
2572.219397	106992.787595	57.617549
2571.571355	106794.127338	57.622554
2570.597365	106601.649751	57.627559
2569.834100	106399.102417	57.632564
2569.284185	106200.729707	57.637569
2568.593608	106009.982181	57.642573
2568.270544	105814.178133	57.647578
2567.404176	105626.475340	57.652583
2566.682041	105424.488039	57.657588
2566.300018	105238.215235	57.662593
2565.363167	105041.696300	57.667597
2564.677109	104834.714977	57.672602
2564.029409	104641.890496	57.677607
2563.253416	104448.643789	57.682612
2562.889077	104256.963937	57.687617
2561.949339	104064.234828	57.692621
2561.313063	103853.498227	57.697626
2560.505263	103668.256825	57.702631
2559.767921	103476.813682	57.707636
2559.339503	103286.725196	57.712641
2558.517004	103099.898165	57.717645
2558.198415	102894.226806	57.722650
2557.247466	102708.489043	57.727655
2557.011974	102503.226629	57.732660
2556.439019	102311.589237	57.737665
2555.319981	102126.060339	57.742669
2554.778399	101927.119257	57.747674
2554.218781	101724.090960	57.752679
2553.065399	101527.794102	57.757684
2552.470182	101337.874658	57.762689
2551.890543	101148.861427	57.767693
2551.116085	100954.678850	57.772698
2550.631342	100770.817330	57.777703
2549.796908	100572.010307	57.782708
2549.381992	100381.638703	57.787713
2548.623998	100205.893819	57.792717
2548.145488	100008.836718	57.797722
2547.560139	99817.202708	57.802727
2547.027182	99619.079185	57.807732
2546.012797	99424.040335	57.812737
2545.433859	99234.021302	57.817741
2544.961816	99030.330237	57.822746
2544.008213	98849.412641	57.827751
2543.297871	98650.532657	57.832756
2542.758072	98452.756399	57.837761
2541.751899	98265.439034	57.842765
2541.521872	98068.929948	57.847770
2541.061278	97888.759984	57.852775
2539.994749	97693.014641	57.857780
2539.349925	97496.690374	57.862785
2538.540633	97302.017566	57.867789
2538.074685	97107.989674	57.872794
2537.355187	96931.210809	57.877799
2536.614393	96739.582681	57.882804
2536.201282	96550.961257	57.887809
2535.327140	96364.107878	57.892813
2534.449303	96164.013928	57.897818
2533.888409	95979.422651	57.902823
2533.060851	95795.522048	57.907828
2532.925670	95606.128721	57.912833
2532.261444	95425.446061	57.917837
2531.524613	95229.752096	57.922842
2530.617424	95039.623369	57.927847
2530.335097	94846.384787	57.932852
2529.814402	94661.861312	57.937857
2528.857799	94466.208810	57.942861
2528.315290	94272.654909	57.947866
2527.524758	94075.438438	57.952871
2527.083462	93882.461635	57.957876
2526.225811	93699.001459	57.962881
2525.584088	93508.158716	57.967885
2524.953694	93308.323584	57.972890
2523.984663	93121.512134	57.977895
2523.468613	92923.089145	57.982900
2523.372884	92726.091503	57.987905
2522.298244	92552.941732	57.992909
2521.478049	92346.708920	57.997914
2520.825297	92154.402011	58.002919
2520.476052	91966.487426	58.007924
2519.597812	91769.070628	58.012929
2518.739290	91585.133405	58.017933
2518.362034	91391.299313	58.022938
2517.294024	91205.033290	58.027943
2516.716003	91011.982574	58.032948
2516.055083	90825.813743	58.037953
2515.169289	90643.664103	58.042957
2514.456530	90458.787417	58.047962
2514.169644	90275.677214	58.052967
2513.612951	90094.938292	58.057972
2513.128551	89893.868076	58.062977
2511.844298	89714.325508	58.067981
2511.783823	89517.965900	58.072986
2511.008827	89340.108305	58.077991
2510.298129	89147.126717	58.082996
2509.769224	88954.466729	58.088001
2509.237655	88772.130672	58.093005
2508.433227	88571.053612	58.098010
2507.983828	88381.061621	58.103015
2506.970736	88190.881687	58.108020
2506.345029	87990.396648	58.113025
2505.523995	87805.718081	58.118029
2505.209905	87612.363902	58.123034
2503.924601	87425.752444	58.128039
2503.257326	87242.423703	58.133044
2502.925475	87051.492790	58.138049
2502.185384	86874.233107	58.143053
2501.376757	86677.085843	58.148058
2500.662370	86499.210233	58.153063
2499.906125	86303.738055	58.158068
2499.292739	86126.103099	58.163073
2498.688299	85944.968872	58.168077
2498.324987	85762.790001	58.173082
2497.516930	85581.152286	58.178087
2496.896428	85397.990331	58.183092
2496.219832	85204.353913	58.188097
2495.434609	85028.967651	58.193101
2494.723436	84844.398523	58.198106
2494.119094	84663.154693	58.203111
2493.462333	84479.689416	58.208116
2493.165355	84295.015013	58.213121
2492.048945	84108.329599	58.218125
2491.954201	83908.039383	58.223130
2491.183925	83737.688018	58.228135
2490.472966	83546.556896	58.233140
2489.717547	83353.710455	58.238145
2489.122352	83169.955166	58.243149
2488.334421	82970.487279	58.248154
2487.595845	82796.734711	58.253159
2486.786009	82603.466396	58.258164
2486.239988	82408.662192	58.263169
2485.311381	82242.125614	58.268173
2485.024975	82054.033768	58.273178
2484.312893	81874.713344	58.278183
2483.562584	81693.657541	58.283188
2483.116831	81505.849389	58.288193
2482.322277	81317.109495	58.293197
2482.197645	81130.103091	58.298202
2481.023743	80944.652693	58.303207
2480.280252	80757.697028	58.308212
2479.748812	80568.484874	58.313217
2478.948496	80396.048549	58.318221
2478.730471	80194.184452	58.323226
2477.884347	80008.899559	58.328231
2476.919733	79829.826853	58.333236
2476.559768	79638.935538	58.338241
2475.742253	79452.402598	58.343245
2474.863492	79260.082379	58.348250
2474.370996	79081.613048	58.353255
2473.541330	78892.792979	58.358260
2473.235401	78711.103305	58.363265
2472.375067	78540.504359	58.368269
2471.671582	78350.794721	58.373274
2471.201648	78166.423583	58.378279
2470.671624	77980.162537	58.383284
2469.781052	77790.728525	58.388289
2469.069721	77607.908843	58.393293
2468.110112	77418.856744	58.398298
2467.346138	77236.695068	58.403303
2466.883363	77057.833017	58.408308
2466.389081	76874.592592	58.413313
2465.441061	76696.900523	58.418317
2464.851360	76504.401836	58.423322
2464.098944	76331.136494	58.428327
2463.496623	76160.282000	58.433332
2462.994346	75986.669446	58.438337
2462.084377	75799.715453	58.443341
2461.864583	75613.160654	58.448346
2460.859519	75440.956741	58.453351
2460.043455	75254.911618	58.458356
2459.558500	75081.449783	58.463361
2458.780409	74910.095105	58.468365
2458.380390	74720.972991	58.473370
2457.692010	74541.795003	58.478375
2456.689912	74371.430787	58.483380
2456.267002	74180.587679	58.488385
2455.608798	74017.242648	58.493389
2455.234618	73824.152345	58.498394
2454.402536	73649.256294	58.503399
2453.727315	73462.736519	58.508404
2453.040643	73293.573180	58.513409
2452.285506	73116.388795	58.518413
2451.897862	72928.022795	58.523418
2451.364813	72743.983296	58.528423
2450.413568	72561.950380	58.533428
2449.886081	72379.541511	58.538433
2449.300408	72190.491636	58.543437
2448.625450	72005.505822	58.548442
2447.748664	71827.471567	58.553447
2447.319512	71649.912739	58.558452
2446.765476	71469.454900	58.563457
2445.910197	71287.107996	58.568461
2445.439167	71107.090059	58.573466
2444.643122	70921.652075	58.578471
2443.749779	70742.382221	58.583476
2443.101091	70567.243380	58.588481
2442.399340	70378.336827	58.593485
2441.958716	70195.592153	58.598490
2441.307388	70016.309509	58.603495
2440.548743	69827.613608	58.608500
2440.062561	69649.245603	58.613505
2439.151572	69477.933266	58.618509
2438.426028	69291.213546	58.623514
2438.016855	69113.579285	58.628519
2437.142851	68930.199294	58.633524
2436.601152	68746.825334	58.638529
2435.815199	68568.793355	58.643533
2435.104807	68381.750512	58.648538
2434.261944	68207.721206	58.653543
2433.967712	68031.110942	58.658548
2433.430090	67844.096515	58.663553
2432.576540	67666.191139	58.668557
2432.106505	67487.270200	58.673562
2431.261782	67309.189340	58.678567
2430.470251	67127.738580	58.683572
2430.179869	66944.056677	58.688577
2429.296478	66769.970624	58.693581
2428.731682	66580.223943	58.698586
2428.079474	66410.556791	58.703591
2427.373610	66228.030526	58.708596
2426.592259	66043.124016	58.713601
2425.604341	65872.403337	58.718605
2425.298275	65679.239410	58.723610
2424.796619	65503.083975	58.728615
2424.092651	65327.133213	58.733620
2423.701959	65145.441138	58.738625
2422.792833	64963.345351	58.743629
2422.276718	64773.336369	58.748634
2421.640584	64598.204765	58.753639
2420.943663	64420.396195	58.758644
2420.311688	64228.932296	58.763649
2419.525889	64046.448854	58.768653
2418.853236	63846.956108	58.773658
2418.013100	63680.281039	58.778663
2417.265539	63500.772953	58.783668
2416.590426	63316.325398	58.788673
2416.005912	63147.771752	58.793677
2415.618245	62960.916974	58.798682
2414.786672	62788.837511	58.803687
2414.133024	62605.786481	58.808692
2413.576441	62414.392122	58.813697
2412.688072	62246.790599	58.818701
2412.018569	62058.282918	58.823706
2411.247685	61884.046026	58.828711
2410.974227	61695.529803	58.833716
2410.172671	61511.914418	58.838721
2409.150087	61342.467997	58.843725
2408.424792	61163.206379	58.848730
2408.245732	60988.589466	58.853735
2407.265855	60805.300467	58.858740
2406.775645	60630.764691	58.863745
2405.922843	60448.269426	58.868749
2405.691309	60272.828557	58.873754
2404.901966	60097.129557	58.878759
2404.169240	59918.501406	58.883764
2403.738021	59735.572668	58.888769
2402.814298	59551.989410	58.893773
2402.295242	59369.100329	58.898778
2401.325634	59193.552327	58.903783
2400.699379	59014.938055	58.908788
2399.921156	58834.994802	58.913793
2399.004700	58663.669128	58.918797
2398.782533	58485.989753	58.923802
2398.140640	58309.125632	58.928807
2397.718928	58135.681575	58.933812
2396.839103	57951.559483	58.938817
2396.174503	57783.386183	58.943821
2395.868555	57600.236910	58.948826
2395.009116	57416.629638	58.953831
2394.482325	57231.711721	58.958836
2393.821093	57052.181771	58.963841
2393.171415	56872.097843	58.968845
2392.707645	56693.375629	58.973850
2391.533628	56507.602239	58.978855
2391.143370	56326.707060	58.983860
2390.662144	56138.048699	58.988865
2389.614511	55963.518369	58.993869
2389.043908	55774.111998	58.998874
2388.553339	55594.603955	59.003879
2387.506879	55416.442236	59.008884
2387.124332	55232.046812	59.013889
2386.174591	55050.439533	59.018893
2385.426006	54864.026616	59.023898
2385.055804	54698.591165	59.028903
2384.333191	54515.510073	59.033908
2383.814682	54325.657826	59.038913
2382.774724	54170.343014	59.043917
2382.347899	53980.897530	59.048922
2381.534303	53798.898161	59.053927
2380.689532	53610.804422	59.058932
2380.237740	53441.630703	59.063937
2379.564043	53271.079245	59.068941
2379.136902	53091.547701	59.073946
2378.183329	52920.869864	59.078951
2377.847161	52735.283472	59.083956
2376.991078	52556.840978	59.088961
2376.022331	52385.964895	59.093965
2375.216522	52211.061817	59.098970
2374.642622	52038.063314	59.103975
2374.215323	51866.331036	59.108980
2373.557803	51683.249117	59.113985
2372.876785	51511.304149	59.118989
2372.090502	51329.439107	59.123994
2371.497484	51165.982214	59.128999
2370.430094	50993.416850	59.134004
2370.367323	50817.798767	59.139009
2369.614526	50642.953090	59.144013
2368.576363	50472.561731	59.149018
2368.334690	50295.069263	59.154023
2367.666265	50125.426193	59.159028
2366.954251	49958.461927	59.164033
2366.144353	49779.814943	59.169037
2365.728327	49594.194412	59.174042
2365.114412	49429.200048	59.179047
2364.180940	49252.713455	59.184052
2363.837827	49075.217512	59.189057
2363.208153	48905.253996	59.194061
2362.513174	48715.659481	59.199066
2361.700690	48550.391525	59.204071
2360.749681	48379.186907	59.209076
2360.376204	48203.169187	59.214081
2359.460928	48028.033169	59.219085
2358.627994	47849.864701	59.224090
2358.421955	47688.693851	59.229095
2357.679770	47515.458812	59.234100
2357.531082	47337.038297	59.239105
2356.519239	47157.677760	59.244109
2355.753397	46980.152713	59.249114
2355.446066	46806.207166	59.254119
2354.564335	46635.517678	59.259124
2353.895354	46452.415237	59.264129
2353.007720	46278.139883	59.269133
2352.923502	46096.786209	59.274138
2351.797053	45921.742482	59.279143
2350.936722	45737.491639	59.284148
2350.536564	45568.706718	59.289153
2349.639713	45389.614783	59.294157
2349.219535	45213.529841	59.299162
2348.360564	45042.304991	59.304167
2347.603004	44870.512216	59.309172
2347.150914	44696.993175	59.314177
2346.068424	44532.593195	59.319181
2345.489442	44343.068323	59.324186
2345.101249	44176.262194	59.329191
2344.599143	44012.673298	59.334196
2343.850419	43828.785379	59.339201
2343.020256	43661.652589	59.344205
2342.323765	43487.093183	59.349210
2341.773005	43316.943298	59.354215
2341.500080	43143.632662	59.359220
2341.026184	42966.184161	59.364225
2340.039997	42790.203921	59.369229
2339.419706	42613.762632	59.374234
2338.575535	42437.165732	59.379239
2337.470263	42267.885714	59.384244
2337.197160	42086.081788	59.389249
2336.680418	41917.752296	59.394253
2336.056368	41741.390060	59.399258
2335.483768	41566.744939	59.404263
2334.737078	41387.398382	59.409268
2333.998935	41207.653887	59.414273
2333.042040	41033.802431	59.419277
2332.802297	40849.147561	59.424282
2331.920046	40681.397212	59.429287
2331.275595	40511.523768	59.434292
2330.930848	40338.565678	59.439297
2329.926865	40158.317773	59.444301
2329.291589	39982.715251	59.449306
2328.587493	39807.893812	59.454311
2327.996622	39618.340329	59.459316
2327.580812	39449.574707	59.464321
2326.351594	39288.860366	59.469325
2326.015821	39109.230536	59.474330
2325.412853	38938.656259	59.479335
2324.690572	38761.318917	59.484340
2323.910491	38584.378323	59.489345
2323.076429	38415.850502	59.494349
2322.417292	38236.319088	59.499354
2321.811814	38080.866850	59.504359
2321.505210	37905.363186	59.509364
2320.614133	37727.285616	59.514369
2319.539282	37555.451603	59.519373
2319.332378	37383.192387	59.524378
2318.491319	37214.655459	59.529383
2318.042716	37047.967510	59.534388
2317.379213	36871.336098	59.539393
2316.741622	36699.354477	59.544397
2316.279477	36521.836447	59.549402
2315.040302	36351.928076	59.554407
2314.505570	36175.898396	59.559412
2314.285862	36002.989800	59.564417
2313.445917	35829.686610	59.569421
2313.120843	35659.630751	59.574426
2312.433230	35483.201044	59.579431
2311.469850	35302.517724	59.584436
2310.739380	35130.827636	59.589441
2309.895349	34951.839340	59.594445
2309.794963	34776.272252	59.599450
2308.602592	34615.828791	59.604455
2308.002464	34440.472506	59.609460
2307.648826	34261.043967	59.614465
2306.637313	34092.517918	59.619469
2306.316809	33916.201359	59.624474
2305.528728	33750.952798	59.629479
2304.825394	33576.464320	59.634484
2304.339474	33395.542526	59.639489
2303.581782	33227.542839	59.644493
2302.944795	33044.736539	59.649498
2302.093352	32877.693996	59.654503
2301.308712	32697.870201	59.659508
2300.971864	32524.396611	59.664513
2299.984583	32365.650612	59.669517
2299.586440	32183.462250	59.674522
2299.001880	32009.051974	59.679527
2298.118133	31835.816134	59.684532
2297.242727	31665.630657	59.689537
2296.513916	31490.943732	59.694541
2296.431510	31320.778243	59.699546
2295.466773	31154.899307	59.704551
2294.492287	30988.754956	59.709556
2294.336789	30812.072259	59.714561
2293.669391	30645.326442	59.719565
2293.007379	30462.901827	59.724570
2291.964604	30298.669843	59.729575
2291.540896	30114.506350	59.734580
2290.869291	29950.397523	59.739585
2289.961055	29784.891591	59.744589
2289.633389	29606.972449	59.749594
2288.660851	29446.101774	59.754599
2288.093938	29270.753859	59.759604
2287.664691	29103.786835	59.764609
2286.834169	28925.915349	59.769613
2286.208906	28748.697365	59.774618
2285.217252	28582.347842	59.779623
2284.803138	28410.027899	59.784628
2284.280960	28250.953969	59.789633
2283.115349	28086.101682	59.794637
2282.822298	27915.339764	59.799642
2282.037424	27749.872790	59.804647
2281.100674	27587.545478	59.809652
2280.814852	27419.007311	59.814657
2279.930822	27252.060289	59.819661
2279.392244	27080.876869	59.824666
2278.972911	26912.739546	59.829671
2278.030286	26754.963378	59.834676
2277.590692	26589.944765	59.839681
2277.018340	26421.046937	59.844685
2276.127511	26245.008128	59.849690
2275.403991	26085.089279	59.854695
2274.872613	25908.675646	59.859700
2274.398124	25746.389819	59.864705
2273.574697	25584.251013	59.869709
2272.872898	25406.494812	59.874714
2272.361946	25238.024540	59.879719
2271.595881	25066.115047	59.884724
2270.960414	24901.984317	59.889729
2270.372298	24739.469973	59.894733
2270.031358	24554.181136	59.899738
2269.347208	24387.336282	59.904743
2268.394577	24216.002522	59.909748
2267.911097	24039.170574	59.914753
2266.896952	23873.283734	59.919758
2266.400136	23697.233995	59.924762
2265.736671	23539.834398	59.929767
2265.029973	23368.949268	59.934772
2264.562930	23181.658040	59.939777
2263.170382	23023.658177	59.944782
2263.241840	22843.004290	59.949786
2262.384674	22686.969723	59.954791
2261.566406	22527.805759	59.959796
2261.305792	22347.497604	59.964801
2260.437742	22181.019250	59.969806
2259.818520	22003.031894	59.974810
2258.852547	21838.868176	59.979815
2258.632463	21668.630827	59.984820
2258.123739	21500.026661	59.989825
2257.228788	21335.477076	59.994830
2256.319477	21152.573840	59.999834
2255.691244	20989.528437	60.004839
2254.924774	20817.153126	60.009844
2254.668963	20644.016487	60.014849
2253.632649	20488.702319	60.019854
2252.926046	20318.419278	60.024858
2252.021183	20151.396454	60.029863
2251.351085	19982.864857	60.034868
2250.883856	19809.114797	60.039873
2249.927541	19662.401306	60.044878
2249.675105	19496.711381	60.049882
2248.820015	19338.940167	60.054887
2247.972934	19177.193292	60.059892
2247.527650	19010.962736	60.064897
2246.625837	18840.010187	60.069902
2246.028661	18685.156548	60.074906
2245.404778	18531.908552	60.079911
2244.870819	18368.413100	60.084916
2244.418954	18204.023714	60.089921
2243.499841	18047.411296	60.094926
2242.923001	17884.965040	60.099930
2242.348137	17713.887666	60.104935
2241.405462	17552.883230	60.109940
2240.819395	17390.642913	60.114945
2239.770029	17236.487159	60.119950
2239.336208	17077.386364	60.124954
2238.436129	16923.963114	60.129959
2238.089386	16770.834872	60.134964
2237.508416	16616.569116	60.139969
2236.682386	16458.156142	60.144974
2236.225905	16292.039777	60.149978
2235.487143	16137.432810	60.154983
2234.698885	15976.341658	60.159988
2234.146689	15815.487843	60.164993
2233.434911	15657.623379	60.169998
2233.113936	15488.041590	60.175002
2232.021926	15337.804604	60.180007
2231.591996	15177.246845	60.185012
2231.278187	15014.367772	60.190017
2230.254588	14862.667705	60.195022
2229.684003	14700.252586	60.200026
2229.239194	14534.675934	60.205031
2228.283417	14379.270729	60.210036
2227.291408	14217.351884	60.215041
2226.527234	14060.596309	60.220046
2226.120138	13903.081382	60.225050
2225.471316	13750.812801	60.230055
2224.602350	13609.953422	60.235060
2223.775959	13450.349761	60.240065
2223.025829	13296.167286	60.245070
2222.635463	13141.526990	60.250074
2222.090790	12986.917567	60.255079
2221.151947	12835.399465	60.260084
2220.471802	12686.762478	60.265089
2219.834322	12543.053064	60.270094
2219.096347	12391.801949	60.275098
2218.358061	12236.015319	60.280103
2217.595147	12090.603509	60.285108
2217.194947	11935.227470	60.290113
2216.319608	11796.596875	60.295118
2215.524366	11645.663986	60.300122
2215.105823	11504.931967	60.305127
2214.450724	11358.510419	60.310132
2213.978567	11204.388208	60.315137
2212.851003	11075.700345	60.320142
2212.481936	10921.436023	60.325146
2211.808777	10780.467622	60.330151
2211.079746	10635.169485	60.335156
2210.630071	10495.887071	60.340161
2209.555559	10353.292385	60.345166
2208.858232	10219.514460	60.350170
2208.131502	10080.159885	60.355175
2207.387177	9931.750443	60.360180
2206.601806	9791.019918	60.365185
2205.963687	9662.811034	60.370190
2205.216502	9523.770184	60.375194
2204.394917	9400.332848	60.380199
2203.746670	9270.568041	60.385204
2203.141746	9136.579899	60.390209
2202.100431	9002.690586	60.395214
2201.171340	8881.755528	60.400218
2200.487513	8764.569221	60.405223
2199.574510	8633.689347	60.410228
2199.285282	8513.304264	60.415233
2198.308583	8404.378762	60.420238
2197.969459	8283.151362	60.425242
2196.909419	8168.928782	60.430247
2196.306094	8065.780354	60.435252
2195.765290	7949.367438	60.440257
2194.631150	7837.789047	60.445262
2193.660463	7719.810670	60.450266
2193.183248	7619.855818	60.455271
2192.356996	7515.517806	60.460276
2191.963044	7408.467128	60.465281
2190.907926	7312.552910	60.470286
2190.460063	7208.242996	60.475290
2189.937375	7108.909767	60.480295
2189.037014	7014.132183	60.485300
2188.483957	6913.202059	60.490305
2187.934984	6807.341507	60.495310
2187.075285	6699.848350	60.500314
2186.241073	6603.247694	60.505319
2185.728118	6494.206896	60.510324
2185.337727	6403.098957	60.515329
2184.433987	6310.359252	60.520334
2183.866728	6205.289197	60.525338
2183.241651	6114.522777	60.530343
2182.003679	6016.957396	60.535348
2181.484873	5923.074384	60.540353
2180.737035	5830.365785	60.545358
2180.214656	5740.651839	60.550362
2179.217820	5661.209907	60.555367
2178.651446	5576.139001	60.560372
2177.912916	5484.388696	60.565377
2177.154634	5407.535412	60.570382
2176.699700	5318.405701	60.575386
2176.064572	5236.655065	60.580391
2175.012487	5149.501594	60.585396
2174.623863	5063.286924	60.590401
2173.866259	4983.557465	60.595406
2173.465311	4903.491832	60.600410
2172.467841	4829.472540	60.605415
2171.602106	4745.695415	60.610420
2171.054665	4660.183471	60.615425
2170.233408	4589.220685	60.620430
2169.702023	4519.485293	60.625434
2169.051538	4449.780957	60.630439
2167.984949	4365.892724	60.635444
2167.363429	4292.410395	60.640449
2166.865076	4234.664695	60.645454
2166.215377	4165.044396	60.650458
2165.200476	4092.461537	60.655463
2164.659661	4030.154264	60.660468
2164.119156	3961.116244	60.665473
2163.130809	3909.716755	60.670478
2162.835055	3834.452198	60.675482
2162.227522	3761.739288	60.680487
2161.322606	3698.590479	60.685492
2160.776834	3641.939887	60.690497
2159.889053	3574.144206	60.695502
2159.061429	3505.416516	60.700506
2158.507618	3450.311419	60.705511
2157.537032	3388.977317	60.710516
2157.175933	3319.401975	60.715521
2156.473987	3277.023652	60.720526
2155.968070	3214.515542	60.725530
2155.332972	3162.945889	60.730535
2154.612911	3095.408938	60.735540
2154.033533	3033.341506	60.740545
2153.380260	2976.749177	60.745550
2153.118972	2913.819445	60.750554
2152.235314	2853.009293	60.755559
2151.786480	2797.998030	60.760564
2151.271469	2737.396429	60.765569
2150.191585	2669.485560	60.770574
2149.429539	2604.845577	60.775578
2148.479796	2547.735695	60.780583
2148.136652	2493.590510	60.785588
2147.193433	2443.522593	60.790593
2146.729286	2383.552393	60.795598
2145.967229	2328.355212	60.800602
2145.099885	2271.710456	60.805607
2144.537708	2217.468556	60.810612
2144.053869	2166.054270	60.815617
2143.290831	2113.617460	60.820622
2142.680385	2054.853967	60.825626
2142.040878	2003.797750	60.830631
2141.250935	1945.166489	60.835636
2140.503918	1901.678677	60.840641
2139.599232	1844.668487	60.845646
2139.162820	1795.330695	60.850650
2138.655865	1744.519322	60.855655
2137.775426	1697.140238	60.860660
2137.091801	1646.572529	60.865665
2136.867199	1598.887813	60.870670
2136.096542	1552.420745	60.875674
2135.129297	1508.819217	60.880679
2134.414251	1445.125576	60.885684
2133.932007	1410.139988	60.890689
2133.037516	1363.428208	60.895694
2132.631473	1303.183521	60.900698
2131.964190	1266.100840	60.905703
2130.886249	1213.017766	60.910708
2130.582560	1171.190341	60.915713
2129.755350	1112.133048	60.920718
2129.428117	1064.646156	60.925722
2128.538458	1026.317164	60.930727
2127.754539	980.600796	60.935732
2127.455921	928.596074	60.940737
2126.585088	889.944299	60.945742
2125.784107	847.550097	60.950746
2125.207870	797.827029	60.955751
2124.539528	758.018207	60.960756
2124.226750	700.550314	60.965761
2123.321191	658.805673	60.970766
2122.412543	617.366809	60.975770
2121.783891	577.566377	60.980775
2121.534494	538.683661	60.985780
2120.946922	493.010214	60.990785
2119.704354	442.119825	60.995790
2119.382734	399.318891	61.000794
2118.438836	359.349872	61.005799
2117.386322	324.891080	61.010804
2116.851418	290.252454	61.015809
2116.397647	261.067081	61.020814
2115.833869	223.214444	61.025818
2114.769902	184.220651	61.030823
2114.405869	143.075208	61.035828
2114.091160	104.226096	61.040833
2112.994707	75.021655	61.045838
2112.264011	40.856263	61.050842
2111.416098	10.831884	61.055847
2110.171111	-11.840444	61.060852
2109.754349	-34.443888	61.065857
2108.880415	-57.581897	61.070862
2108.056353	-84.261863	61.075866
2106.794000	-98.111077	61.080871
2104.929241	-79.020316	61.085876
2103.353321	-40.409356	61.090881
2101.761883	0.449842	61.095886
2101.781272	6.478901	61.100890
2101.807580	20.183801	61.105895
2101.876661	24.810894	61.110900
2101.771531	19.752758	61.115905
2101.650195	17.330821	61.120910
2101.266540	4.091151	61.125914
2100.755518	-9.030518	61.130919
2099.488546	1.119991	61.135924
2098.497644	15.662855	61.140929
2096.805393	34.019885	61.145934
2096.763987	33.226941	61.150938
2096.328765	41.157505	61.155943
2095.614726	36.986084	61.160948
2095.606839	34.248083	61.165953
2095.108011	35.866455	61.170958
2094.608677	30.115482	61.175962
2093.861230	33.369256	61.180967
2092.699636	36.097372	61.185972
2092.116046	31.537806	61.190977
2090.850961	53.966757	61.195982
2090.160179	50.912907	61.200986
2090.109932	46.614064	61.205991
2089.058043	51.597266	61.210996
2089.034107	51.888119	61.216001
2088.407499	55.550096	61.221006
2087.785037	52.936434	61.226010
2087.125524	53.242993	61.231015
2086.448041	52.606190	61.236020
2085.670071	53.958193	61.241025
2084.553593	64.187374	61.246030
2084.580545	60.630093	61.251034
2084.107950	50.107524	61.256039
2083.133487	58.681943	61.261044
2082.663881	56.160723	61.266049
2081.489335	57.985691	61.271054
2080.879311	54.726630	61.276058
2080.338624	55.982627	61.281063
2079.905431	59.659645	61.286068
2079.556206	56.324500	61.291073
2078.947115	58.550184	61.296078
2077.858741	58.830186	61.301082
2077.421039	51.194344	61.306087
2076.309005	61.044334	61.311092
2075.977892	49.061067	61.316097
2074.875619	62.295380	61.321102
2073.979980	66.100989	61.326106
2073.765380	56.021620	61.331111
2073.437856	65.529479	61.336116
2073.361619	51.159146	61.341121
2072.276419	62.343773	61.346126
2071.917191	54.157711	61.351130
2070.989420	53.462859	61.356135
2069.941542	63.217511	61.361140
2069.337569	63.384368	61.366145
2068.384783	68.060104	61.371150
2067.914630	65.811798	61.376154
2067.321513	58.933937	61.381159
2066.379229	64.620456	61.386164
2065.725174	61.811530	61.391169
2065.677199	65.350140	61.396174
2065.285921	63.180783	61.401178
2063.972966	62.077112	61.406183
2063.186509	70.208524	61.411188
2063.158412	56.778341	61.416193
2062.570269	65.554820	61.421198
2061.801573	69.324516	61.426202
2060.706039	63.116202	61.431207
2060.269738	71.589453	61.436212
2060.100837	61.160615	61.441217
2058.748361	74.310068	61.446222
2058.013954	71.228453	61.451226
2057.492942	65.961908	61.456231
2056.941587	71.617928	61.461236
2056.246369	66.763826	61.466241
2055.350725	73.878043	61.471246
2054.948748	65.425938	61.476250
2054.450399	68.405218	61.481255
2053.325359	68.175362	61.486260
2052.962526	74.287187	61.491265
2052.018911	73.992266	61.496270
2051.669303	60.695114	61.501274
2051.004387	66.304499	61.506279
2050.181329	69.903044	61.511284
2049.720276	54.582915	61.516289
2049.356067	67.799451	61.521294
2048.911997	69.316100	61.526298
2047.864162	64.219909	61.531303
2046.845177	71.758999	61.536308
2046.445377	57.539372	61.541313
2045.350772	72.631797	61.546318
2045.094482	61.937698	61.551322
2044.995226	63.691369	61.556327
2043.681961	67.088587	61.561332
2043.308407	63.189578	61.566337
2042.315843	64.545690	61.571342
2041.732581	60.419758	61.576346
2041.228654	63.155486	61.581351
2040.200615	64.452570	61.586356
2040.242350	63.523422	61.591361
2039.449709	61.812031	61.596366
2038.742016	65.971036	61.601370
2038.083380	60.275312	61.606375
2037.172298	64.660574	61.611380
2036.718901	61.586408	61.616385
2035.772295	65.355960	61.621390
2035.521440	63.351987	61.626394
2034.802582	64.426528	61.631399
2034.095641	66.227764	61.636404
2033.947935	65.041665	61.641409
2033.141338	70.757125	61.646414
2031.770241	61.798074	61.651418
2030.780296	61.180916	61.656423
2030.416683	72.312535	61.661428
2030.688069	61.400639	61.666433
2028.901135	67.921433	61.671438
2029.021983	65.410588	61.676442
2028.044108	62.806041	61.681447
2026.867967	68.335718	61.686452
2027.100714	63.384801	61.691457
2026.006292	69.029247	61.696462
2025.221085	66.184375	61.701466
2024.654704	57.864038	61.706471
2023.885782	69.785418	61.711476
2023.459828	60.867176	61.716481
2022.791816	63.849734	61.721486
2022.329669	65.339292	61.726490
2021.627357	57.087842	61.731495
2021.098213	72.476891	61.736500
2020.438426	62.387762	61.741505
2019.487306	66.270005	61.746510
2019.397123	61.185835	61.751514
2018.501327	63.237833	61.756519
2017.038971	57.579798	61.761524
2016.669504	56.354781	61.766529
2016.316293	69.299901	61.771534
2015.822451	64.398079	61.776538
2014.835894	59.435687	61.781543
2013.720710	66.012299	61.786548
2013.451098	54.311031	61.791553
2012.636226	66.476258	61.796558
2012.145485	62.526468	61.801562
2011.815504	60.943507	61.806567
2010.694394	60.262017	61.811572
2010.506266	54.647746	61.816577
2009.633932	61.285162	61.821582
2009.430252	51.076336	61.826586
2009.206622	60.457310	61.831591
2007.900225	53.307895	61.836596
2006.886783	54.120106	61.841601
2005.701809	63.901269	61.846606
2005.487020	58.642906	61.851610
2005.168137	60.292660	61.856615
2004.056198	60.185331	61.861620
2003.628272	59.351235	61.866625
2002.707923	68.087411	61.871630
2002.467332	58.127302	61.876634
2002.103269	51.273034	61.881639
2001.028383	58.261161	61.886644
2000.913081	59.340835	61.891649
2000.074002	59.480369	61.896654
1999.638629	59.934306	61.901658
1998.533667	58.704609	61.906663
1997.635501	67.670664	61.911668
1996.712317	50.097803	61.916673
1995.957016	65.379235	61.921678
1995.283183	54.218397	61.926682
1995.547728	59.833223	61.931687
1994.747119	58.671915	61.936692
1994.081080	55.107941	61.941697
1993.306726	67.366093	61.946702
1992.893244	59.710653	61.951706
1992.362481	58.935462	61.956711
1991.253968	60.040326	61.961716
1990.287509	54.913900	61.966721
1989.330396	60.664298	61.971726
1988.886755	59.927320	61.976730
1988.544907	63.264984	61.981735
1987.518802	68.447569	61.986740
1987.651092	59.186821	61.991745
1986.443297	58.104345	61.996750
1986.319967	53.845494	62.001754
1985.938657	48.157811	62.006759
1985.131818	54.638171	62.011764
1983.713904	53.477082	62.016769
1982.632123	58.602269	62.021774
1982.274428	55.940297	62.026778
1981.954826	51.247381	62.031783
1981.242456	52.899673	62.036788
1980.906616	49.038850	62.041793
1980.224496	61.175120	62.046798
1979.561345	56.464195	62.051802
1979.191956	64.649271	62.056807
1978.290550	65.563561	62.061812
1977.437338	48.522101	62.066817
1976.109990	66.665174	62.071822
1975.839910	62.663016	62.076826
1975.315959	60.418538	62.081831
1974.702205	67.235701	62.086836
1974.430878	52.614068	62.091841
1973.713896	61.936157	62.096846
1973.285741	58.454280	62.101850
1972.229729	61.564676	62.106855
1971.225083	62.560016	62.111860
1970.802131	59.339099	62.116865
1969.758782	58.304646	62.121870
1969.320088	56.420390	62.126874
1969.171533	60.373950	62.131879
1968.445722	59.337978	62.136884
1967.771338	56.087586	62.141889
1966.462171	54.322591	62.146894
1965.489611	49.930462	62.151898
1965.618353	54.149096	62.156903
1964.778097	56.376806	62.161908
1964.465919	46.125289	62.166913
1963.390632	59.768526	62.171918
1962.837006	62.515309	62.176922
1962.319084	58.088855	62.181927
1961.691638	66.340130	62.186932
1961.539534	61.920259	62.191937
1959.994370	54.348284	62.196942
1959.555652	64.428908	62.201946
1959.293521	57.813941	62.206951
1958.277429	55.016786	62.211956
1957.982238	57.208434	62.216961
1957.353499	66.820886	62.221966
1956.172710	65.235797	62.226970
1955.257982	61.526800	62.231975
1954.348754	65.132742	62.236980
1953.782290	63.610987	62.241985
1953.199924	61.166043	62.246990
1953.293839	58.708361	62.251994
1952.672746	64.274535	62.256999
1951.986195	64.555457	62.262004
1951.760773	59.265671	62.267009
1950.496685	61.354080	62.272014
1949.474163	60.261133	62.277018
1949.034909	64.946848	62.282023
1948.500987	57.938195	62.287028
1947.924316	66.287072	62.292033
1947.017657	62.941090	62.297038
1946.432821	58.023769	62.302042
1945.578361	65.052621	62.307047
1944.607494	65.186284	62.312052
1944.317101	62.024756	62.317057
1943.609483	70.517432	62.322062
1943.245986	58.651301	62.327066
1942.776603	56.472288	62.332071
1942.284565	66.102466	62.337076
1941.515404	59.019191	62.342081
1939.953673	61.858209	62.347086
1939.404820	65.638767	62.352090
1938.668487	62.630040	62.357095
1938.071632	63.466031	62.362100
1938.127002	57.472475	62.367105
1937.358348	57.783782	62.372110
1937.120822	50.852666	62.377114
1936.091933	58.923235	62.382119
1934.895737	65.304568	62.387124
1934.574358	64.713776	62.392129
1933.963215	61.577939	62.397134
1933.404387	65.495705	62.402138
1932.878562	72.576474	62.407143
1931.633286	62.670219	62.412148
1931.066298	61.451340	62.417153
1929.734722	62.866045	62.422158
1929.458328	54.800911	62.427162
1929.649226	59.864422	62.432167
1928.752731	67.559148	62.437172
1928.154414	61.913809	62.442177
1927.502714	55.223496	62.447182
1926.926951	57.942259	62.452186
1926.170737	53.255589	62.457191
1924.959792	61.468611	62.462196
1924.727722	50.054734	62.467201
1923.937871	61.326560	62.472206
1923.445576	58.931982	62.477210
1923.199561	49.262929	62.482215
1921.619517	58.881326	62.487220
1920.997641	53.328046	62.492225
1920.512906	60.134193	62.497230
1919.912783	53.524008	62.502234
1919.715947	48.776919	62.507239
1918.693340	59.396539	62.512244
1918.856112	48.263768	62.517249
1917.468034	58.531386	62.522254
1916.606036	49.718679	62.527258
1916.453606	50.867331	62.532263
1915.567343	50.686362	62.537268
1914.504152	46.542043	62.542273
1913.503802	58.515945	62.547278
1913.289080	52.114245	62.552282
1912.707417	52.600885	62.557287
1911.878745	55.249412	62.562292
1911.603194	47.835462	62.567297
1911.024287	59.791343	62.572302
1910.480888	54.848529	62.577306
1909.728496	52.629297	62.582311
1908.520281	53.784718	62.587316
1907.976239	56.082115	62.592321
1907.445036	60.192626	62.597326
1906.888832	55.284964	62.602330
1906.790021	51.501643	62.607335
1905.554181	62.032115	62.612340
1904.676863	52.149468	62.617345
1903.595411	57.034923	62.622350
1903.126484	51.857928	62.627354
1902.875427	43.626350	62.632359
1902.569407	49.888434	62.637364
1901.982111	44.591458	62.642369
1901.197712	46.535915	62.647374
1900.486924	48.263672	62.652378
1899.446193	50.277214	62.657383
1898.814997	50.235534	62.662388
1898.655131	44.544252	62.667393
1897.286891	44.428774	62.672398
1896.399621	49.701309	62.677402
1895.924932	46.411350	62.682407
1895.146750	51.491516	62.687412
1895.050892	42.621838	62.692417
1894.122786	54.760898	62.697422
1893.699113	43.593505	62.702426
1893.457457	50.532951	62.707431
1892.945535	47.395567	62.712436
1892.039114	42.330621	62.717441
1890.961220	41.967189	62.722446
1890.439733	45.205641	62.727450
1889.991689	41.591319	62.732455
1888.657352	50.882120	62.737460
1887.959671	44.098197	62.742465
1886.933251	56.453151	62.747470
1886.594136	58.509848	62.752474
1886.020084	57.629584	62.757479
1885.671794	52.957010	62.762484
1885.438180	48.357697	62.767489
1884.887451	47.161481	62.772494
1884.266792	46.880001	62.777498
1883.612459	43.853545	62.782503
1882.378796	50.130449	62.787508
1881.877714	53.135419	62.792513
1881.241018	54.037675	62.797518
1880.061838	51.573967	62.802522
1879.422748	53.615212	62.807527
1878.920062	55.939165	62.812532
1878.500954	59.181867	62.817537
1877.802508	66.760001	62.822542
1877.593312	60.821070	62.827546
1876.972432	58.420110	62.832551
1875.625519	62.562370	62.837556
1875.382838	57.969226	62.842561
1874.687796	62.914769	62.847566
1873.910467	61.871233	62.852570
1872.704605	60.536180	62.857575
1871.757935	52.251044	62.862580
1871.969437	56.614231	62.867585
1871.335187	65.756040	62.872590
1870.661674	60.616265	62.877594
1870.298416	52.419851	62.882599
1869.377575	63.166837	62.887604
1868.911034	58.918335	62.892609
1867.768777	61.930496	62.897614
1867.177849	58.600648	62.902618
1866.628229	57.703892	62.907623
1865.814489	66.257587	62.912628
1865.718606	51.202831	62.917633
1864.350335	50.978562	62.922638
1863.457793	50.787568	62.927642
1863.056047	55.923094	62.932647
1862.438372	63.139881	62.937652
1862.334527	48.900136	62.942657
1861.577790	61.768968	62.947662
1860.699531	51.842334	62.952666
1859.893889	61.303104	62.957671
1859.016669	60.444176	62.962676
1858.564186	51.200598	62.967681
1858.097979	62.752220	62.972686
1857.741202	52.911523	62.977690
1856.639203	53.196933	62.982695
1855.543451	61.532045	62.987700
1855.175860	51.207344	62.992705
1854.539986	51.666333	62.997710
1854.218440	52.222073	63.002714
1853.936035	54.736565	63.007719
1852.964205	61.629528	63.012724
1851.743575	57.928144	63.017729
1851.231518	55.218162	63.022734
1850.703556	52.852920	63.027738
1850.407571	57.826567	63.032743
1849.651567	55.924908	63.037748
1848.795296	62.799523	63.042753
1847.707836	62.412395	63.047758
1847.102007	61.153969	63.052762
1846.802385	50.394259	63.057767
1846.117057	62.706106	63.062772
1845.973850	53.116939	63.067777
1844.669140	63.133222	63.072782
1843.963077	64.369792	63.077786
1843.580927	58.645996	63.082791
1843.030032	58.567923	63.087796
1842.664511	52.656977	63.092801
1841.460575	52.545402	63.097806
1840.592271	55.848399	63.102810
1840.188297	56.953417	63.107815
1839.487055	53.417157	63.112820
1839.124657	53.414812	63.117825
1837.868520	57.433859	63.122830
1836.967932	56.553417	63.127834
1836.496455	51.192333	63.132839
1835.610710	49.713421	63.137844
1835.849618	46.223423	63.142849
1835.221898	51.957830	63.147854
1834.921394	46.322005	63.152858
1834.276691	50.292846	63.157863
1832.979795	57.377786	63.162868
1832.121173	48.586657	63.167873
1832.025978	66.280211	63.172878
1831.088219	63.022794	63.177882
1830.019150	59.970741	63.182887
1829.246311	63.736420	63.187892
1828.958465	58.317788	63.192897
1828.458223	62.828690	63.197902
1827.910956	56.713208	63.202906
1826.799679	48.897375	63.207911
1825.878600	49.794339	63.212916
1825.410321	48.391070	63.217921
1825.048566	50.591722	63.222926
1824.390933	56.718829	63.227930
1824.278966	51.081451	63.232935
1823.192185	53.692140	63.237940
1822.864315	58.934216	63.242945
1821.935004	54.841219	63.247950
1820.955761	62.662656	63.252954
1820.159123	56.312375	63.257959
1819.345569	66.223865	63.262964
1819.017492	58.043951	63.267969
1818.513852	62.754098	63.272974
1817.770113	64.395644	63.277978
1817.674408	57.249626	63.282983
1816.211988	60.990769	63.287988
1815.700749	57.856446	63.292993
1815.332773	54.519593	63.297998
1814.669123	56.705108	63.303002
1813.728990	54.714424	63.308007
1812.720254	51.685917	63.313012
1812.475661	49.526430	63.318017
1811.627168	56.196380	63.323022
1811.407437	54.491857	63.328026
1811.010979	59.954569	63.333031
1809.997089	57.264363	63.338036
1809.219110	57.105660	63.343041
1808.522609	59.737959	63.348046
1808.188527	56.318451	63.353050
1807.100770	49.341022	63.358055
1805.851581	52.625664	63.363060
1805.420051	48.133490	63.368065
1804.852968	56.553400	63.373070
1804.313233	58.534727	63.378074
1804.068111	52.199376	63.383079
1803.557233	63.579892	63.388084
1803.231339	53.396821	63.393089
1802.206419	47.503868	63.398094
1801.458467	55.654445	63.403098
1800.406964	50.065347	63.408103
1799.197653	60.503331	63.413108
1798.850458	48.864903	63.418113
1798.092713	51.883837	63.423118
1797.793288	49.105406	63.428122
1797.388199	54.578950	63.433127
1796.794920	54.621163	63.438132
1796.612756	52.270406	63.443137
1795.588426	55.552461	63.448142
1794.606710	54.891508	63.453146
1794.095711	45.884334	63.458151
1793.594519	53.890063	63.463156
1792.800668	54.792065	63.468161
1791.740182	57.285046	63.473166
1790.822816	51.017033	63.478170
1790.706710	54.189546	63.483175
1790.208519	63.289255	63.488180
1789.615217	50.912442	63.493185
1788.449829	57.421405	63.498190
1787.670110	56.949157	63.503194
1787.175581	57.392023	63.508199
1786.407313	55.200582	63.513204
1786.647291	41.221660	63.518209
1785.910276	57.914790	63.523214
1784.811730	55.042489	63.528218
1784.274910	50.846173	63.533223
1783.404464	54.160565	63.538228
1783.030569	57.418177	63.543233
1781.892551	49.403179	63.548238
1781.016366	56.437095	63.553242
1780.891635	55.819824	63.558247
1780.094223	55.976465	63.563252
1780.036764	49.029395	63.568257
1778.757475	60.158194	63.573262
1777.667508	58.738545	63.578266
1777.397402	50.341271	63.583271
1776.908848	53.653364	63.588276
1776.379069	50.078854	63.593281
1775.645768	61.223448	63.598286
1774.771179	52.151014	63.603290
1774.272445	50.908716	63.608295
1773.366435	53.842390	63.613300
1773.160615	52.392716	63.618305
1772.056830	52.605903	63.623310
1771.147493	53.729688	63.628314
1770.389217	58.395123	63.633319
1769.895048	61.504675	63.638324
1769.693892	52.995521	63.643329
1769.098692	55.493464	63.648334
1768.821300	57.534062	63.653338
1767.842963	60.149629	63.658343
1766.827956	55.860520	63.663348
1767.012469	50.901490	63.668353
1765.473166	64.448160	63.673358
1764.846565	47.079072	63.678362
1764.136205	47.291281	63.683367
1763.293972	52.398999	63.688372
1763.601723	46.256557	63.693377
1761.944239	50.249489	63.698382
1761.202770	55.762269	63.703386
1760.816510	44.104827	63.708391
1760.048736	51.998350	63.713396
1759.758315	55.689003	63.718401
1759.449289	51.961159	63.723406
1758.615095	59.923586	63.728410
1757.896605	52.509046	63.733415
1757.214108	54.910465	63.738420
1756.549921	50.814812	63.743425
1755.157830	50.755239	63.748430
1754.402755	46.948425	63.753434
1754.264919	42.483737	63.758439
1753.672917	45.856418	63.763444
1753.367992	50.301611	63.768449
1752.904401	44.650701	63.773454
1751.690088	48.272041	63.778458
1751.177449	46.353838	63.783463
1750.034725	49.597940	63.788468
1750.038923	46.700326	63.793473
1749.306237	52.115515	63.798478
1748.079858	50.950945	63.803482
1747.333451	45.311839	63.808487
1746.687517	49.858504	63.813492
1746.434854	47.604109	63.818497
1745.698387	53.776868	63.823502
1745.584914	45.518735	63.828506
1744.728662	42.671052	63.833511
1743.399056	51.800306	63.838516
1742.832002	47.422715	63.843521
1742.301291	52.321681	63.848526
1742.059421	46.217647	63.853530
1742.088600	37.951054	63.858535
1740.412490	53.049161	63.863540
1740.024414	46.728643	63.868545
1739.496245	50.914393	63.873550
1738.266784	54.544453	63.878554
1737.405178	53.003392	63.883559
1736.714474	53.619357	63.888564
1736.576684	37.867948	63.893569
1735.889071	41.927627	63.898574
1735.307801	54.760716	63.903578
1734.955582	45.349856	63.908583
1733.476151	45.521796	63.913588
1733.222051	40.481042	63.918593
1732.449280	54.916834	63.923598
1732.060358	37.418553	63.928602
1731.508935	41.278398	63.933607
1730.033635	55.231242	63.938612
1729.936327	43.111581	63.943617
1728.882155	49.848912	63.948622
1728.736550	49.698604	63.953626
1728.330186	48.023734	63.958631
1727.588273	53.844110	63.963636
1726.804559	44.930739	63.968641
1726.025136	47.011655	63.973646
1725.581169	44.863345	63.978650
1724.491055	52.393320	63.983655
1723.439607	53.189596	63.988660
1723.036997	47.098481	63.993665
1722.390681	46.142998	63.998670
1721.954543	46.513519	64.003674
1721.691980	44.334820	64.008679
1721.117250	52.341197	64.013684
1720.216681	50.032016	64.018689
1719.255857	49.717871	64.023694
1718.736884	47.578323	64.028698
1718.128039	39.842023	64.033703
1717.152518	51.823064	64.038708
1716.473538	41.066877	64.043713
1715.868242	50.450114	64.048718
1715.524060	53.292987	64.053722
1715.481102	45.649734	64.058727
1714.071559	47.649385	64.063732
1713.604587	45.440075	64.068737
1712.925337	51.356159	64.073742
1712.470014	48.987296	64.078746
1711.758972	58.740587	64.083751
1710.508362	47.308766	64.088756
1710.138792	46.170549	64.093761
1709.667720	62.682672	64.098766
1708.594668	47.038817	64.103770
1707.620788	56.005923	64.108775
1706.818072	56.065654	64.113780
1706.626620	44.855119	64.118785
1706.170830	55.714356	64.123790
1706.187628	49.337417	64.128794
1705.224109	48.875466	64.133799
1703.888249	55.539277	64.138804
1703.880894	53.908267	64.143809
1703.158293	58.757294	64.148814
1702.351003	60.164527	64.153818
1701.479125	49.533601	64.158823
1700.496772	62.044041	64.163828
1700.191126	55.260983	64.168833
1699.833649	62.067442	64.173838
1698.808653	64.893881	64.178842
1698.148187	54.319261	64.183847
1697.507222	60.410628	64.188852
1697.162444	49.859985	64.193857
1696.405707	61.520846	64.198862
1695.825101	57.348852	64.203866
1694.646982	51.814610	64.208871
1694.015380	54.357776	64.213876
1693.809678	51.026708	64.218881
1693.472825	57.829890	64.223886
1692.472606	48.162413	64.228890
1691.549523	44.019595	64.233895
1690.769720	54.455618	64.238900
1690.491130	50.420164	64.243905
1689.765243	59.100291	64.248910
1688.946037	56.820775	64.253914
1688.462168	57.856501	64.258919
1687.639557	55.128077	64.263924
1687.391988	47.184577	64.268929
1685.922568	47.285565	64.273934
1685.221046	54.673397	64.278938
1684.575505	48.430061	64.283943
1683.917163	52.843088	64.288948
1684.048195	48.212687	64.293953
1683.776046	53.794439	64.298958
1682.723656	51.469963	64.303962
1681.734570	47.525298	64.308967
1680.970905	48.575508	64.313972
1680.938577	49.818638	64.318977
1679.510503	50.436630	64.323982
1678.812823	46.431482	64.328986
1678.258707	40.317137	64.333991
1677.747570	51.503721	64.338996
1677.536601	42.452076	64.344001
1676.525168	49.942758	64.349006
1675.797972	48.848741	64.354010
1675.169507	53.633931	64.359015
1674.515588	53.283665	64.364020
1674.112456	48.816971	64.369025
1672.840439	48.463966	64.374030
1671.941828	48.639871	64.379034
1671.526997	44.428937	64.384039
1671.335222	50.013690	64.389044
1671.199950	48.655325	64.394049
1669.649335	58.398488	64.399054
1668.756040	56.170174	64.404058
1668.722829	49.391158	64.409063
1668.268692	48.559707	64.414068
1667.749861	43.360735	64.419073
1666.555502	52.791825	64.424078
1665.762941	48.423268	64.429082
1665.273971	46.067646	64.434087
1664.620989	48.111145	64.439092
1664.253418	42.249454	64.444097
1663.280365	49.164739	64.449102
1662.580736	53.850845	64.454106
1662.299774	44.753549	64.459111
1660.567929	52.669355	64.464116
1659.971746	47.971548	64.469121
1659.467636	49.232853	64.474126
1659.191914	49.060640	64.479130
1658.854841	42.582222	64.484135
1658.330446	43.994989	64.489140
1657.629630	44.896444	64.494145
1656.566622	55.203994	64.499150
1655.880918	53.822682	64.504154
1655.655649	59.620927	64.509159
1654.717510	58.046319	64.514164
1653.665876	48.032201	64.519169
1653.251950	53.142871	64.524174
1652.405803	47.049692	64.529178
1651.810767	50.654697	64.534183
1651.830382	58.729098	64.539188
1651.196247	52.285255	64.544193
1650.122066	47.756432	64.549198
1649.504369	46.381666	64.554202
1648.818032	47.260322	64.559207
1647.656583	57.001596	64.564212
1647.398720	47.906939	64.569217
1646.714746	50.836918	64.574222
1646.134633	52.465130	64.579226
1645.876557	49.938782	64.584231
1644.809456	49.725131	64.589236
1644.173144	44.130075	64.594241
1643.403953	48.234276	64.599246
1643.003183	42.194930	64.604250
1642.005955	46.630262	64.609255
1641.271656	50.944973	64.614260
1640.806229	44.878050	64.619265
1640.265524	51.126967	64.624270
1639.690255	50.448812	64.629274
1639.060340	46.429756	64.634279
1637.728951	50.364646	64.639284
1637.400342	51.738428	64.644289
1636.686596	56.780035	64.649294
1636.476377	50.431282	64.654298
1635.501170	45.287476	64.659303
1634.569323	58.723498	64.664308
1634.104153	51.052707	64.669313
1633.652596	45.852517	64.674318
1633.059580	51.505749	64.679322
1632.148217	49.531066	64.684327
1631.494581	50.920215	64.689332
1631.004996	48.425920	64.694337
1630.395852	49.196119	64.699342
1629.598542	49.204550	64.704346
1628.896600	48.278430	64.709351
1627.793360	55.575549	64.714356
1627.963878	40.349213	64.719361
1627.194098	51.095903	64.724366
1625.834493	51.759819	64.729370
1625.231105	45.714818	64.734375
1624.771675	51.238014	64.739380
1624.573915	47.882038	64.744385
1623.995373	52.258743	64.749390
1623.212883	46.718457	64.754394
1622.303689	42.176052	64.759399
1621.722224	49.746678	64.764404
1621.307503	48.085771	64.769409
1620.003774	48.428563	64.774414
1619.302401	39.223025	64.779418
1618.785101	44.457357	64.784423
1618.322568	51.591179	64.789428
1618.175266	42.947339	64.794433
1617.255875	52.031972	64.799438
1616.457867	48.839176	64.804442
1615.948388	38.494509	64.809447
1614.845613	48.355781	64.814452
1614.175324	50.132372	64.819457
1613.389289	46.923482	64.824462
1613.116894	49.956818	64.829466
1612.757358	48.971570	64.834471
1611.895740	53.576186	64.839476
1611.126796	53.822977	64.844481
1610.266061	59.600756	64.849486
1609.610936	54.658426	64.854490
1609.431108	42.263303	64.859495
1608.474843	56.129002	64.864500
1607.666745	48.328193	64.869505
1606.986225	53.175285	64.874510
1606.456793	56.262078	64.879514
1606.138823	54.729309	64.884519
1605.215863	57.479642	64.889524
1604.252054	43.501172	64.894529
1603.721672	41.180529	64.899534
1603.223467	55.008144	64.904538
1602.724340	47.771706	64.909543
1601.650997	53.129085	64.914548
1601.137323	48.596387	64.919553
1600.556739	50.592127	64.924558
1600.175033	49.547323	64.929562
1599.447627	50.602834	64.934567
1598.352258	48.810370	64.939572
1597.806070	55.492268	64.944577
1597.309722	57.178147	64.949582
1596.743762	50.767646	64.954586
1595.824167	49.757841	64.959591
1594.896416	57.372455	64.964596
1594.654789	48.160107	64.969601
1594.198376	48.634800	64.974606
1593.049550	49.897626	64.979610
1592.215869	48.542999	64.984615
1591.374973	53.136444	64.989620
1591.149304	45.337723	64.994625
1590.590830	49.462076	64.999630
1590.223181	46.502120	65.004634
1589.740900	45.632576	65.009639
1588.508448	57.594550	65.014644
1588.394191	46.352848	65.019649
1587.601742	51.828032	65.024654
1586.762341	46.085481	65.029658
1585.897447	43.409546	65.034663
1585.291936	49.570992	65.039668
1584.863562	39.429499	65.044673
1583.673228	54.403185	65.049678
1583.005643	54.173391	65.054682
1582.258327	44.970431	65.059687
1581.836936	49.844165	65.064692
1581.399366	39.300418	65.069697
1581.189979	44.295011	65.074702
1580.608830	45.395100	65.079706
1579.493855	47.319630	65.084711
1578.695079	44.361945	65.089716
1578.227276	42.827757	65.094721
1577.030995	51.297204	65.099726
1575.979247	52.301752	65.104730
1575.856510	39.574279	65.109735
1574.882457	45.160325	65.114740
1575.061793	44.562562	65.119745
1574.425309	50.303138	65.124750
1573.782942	38.758990	65.129754
1573.053188	44.821901	65.134759
1571.930477	51.068685	65.139764
1572.022329	47.628849	65.144769
1570.521726	48.091262	65.149774
1569.587562	50.695147	65.154778
1569.393747	38.983528	65.159783
1569.187368	47.555890	65.164788
1568.878350	44.438382	65.169793
1567.373275	45.488157	65.174798
1566.651787	44.068401	65.179802
1566.449111	42.668712	65.184807
1565.372639	46.313961	65.189812
1564.780921	41.689593	65.194817
1564.169182	46.815933	65.199822
1563.627098	42.484888	65.204826
1563.425776	41.536010	65.209831
1562.228829	47.455534	65.214836
1561.499955	43.540539	65.219841
1560.866112	46.618697	65.224846
1560.276675	39.190036	65.229850
1559.555411	35.612893	65.234855
1558.546454	41.847910	65.239860
1558.237935	38.009631	65.244865
1557.584783	47.906712	65.249870
1557.146426	46.154951	65.254874
1556.568096	40.637445	65.259879
1555.544772	43.717566	65.264884
1555.085294	42.786056	65.269889
1554.526389	45.278273	65.274894
1553.468297	40.549814	65.279898
1552.852020	42.018204	65.284903
1551.979099	48.695252	65.289908
1551.766433	31.896035	65.294913
1550.923485	44.322840	65.299918
1550.384793	39.294220	65.304922
1549.714826	31.679660	65.309927
1548.612048	37.943781	65.314932
1548.446962	39.513946	65.319937
1547.820397	46.623374	65.324942
1547.162511	41.932251	65.329946
1545.979160	40.555931	65.334951
1545.208140	45.728086	65.339956
1545.205520	44.424347	65.344961
1544.938183	44.354897	65.349966
1543.824433	41.723253	65.354970
1543.024242	38.090845	65.359975
1541.858868	50.698208	65.364980
1541.793633	28.865394	65.369985
1541.439278	41.509458	65.374990
1540.454054	44.413213	65.379994
1539.493582	36.646113	65.384999
1538.748000	42.627965	65.390004
1538.952891	41.291251	65.395009
1537.939338	47.222644	65.400014
1536.836128	44.920502	65.405018
1536.440425	33.529570	65.410023
1535.572477	38.434842	65.415028
1535.630619	39.253570	65.420033
1534.512190	42.574325	65.425038
1533.555302	40.665263	65.430042
1533.429967	36.922462	65.435047
1532.737880	43.607048	65.440052
1532.115695	36.697708	65.445057
1531.171274	36.507189	65.450062
1530.502942	40.896599	65.455066
1530.058212	39.571651	65.460071
1528.864111	44.717998	65.465076
1528.116121	41.332775	65.470081
1527.726223	40.517951	65.475086
1527.281620	39.013204	65.480090
1526.785777	34.687439	65.485095
1526.069061	46.304106	65.490100
1525.333578	35.217918	65.495105
1524.403415	45.923874	65.500110
1524.245076	41.680096	65.505114
1523.583390	39.790362	65.510119
1522.165566	35.970673	65.515124
1521.858522	35.629981	65.520129
1521.096610	39.048630	65.525134
1520.554584	42.361372	65.530138
1520.285771	41.479997	65.535143
1518.870219	41.750721	65.540148
1518.520057	40.640990	65.545153
1517.977548	44.701314	65.550158
1517.452093	42.258478	65.555162
1517.054371	41.492209	65.560167
1515.915095	42.938061	65.565172
1515.839480	43.092045	65.570177
1514.985203	44.311249	65.575182
1513.604824	43.133419	65.580186
1513.304034	43.323187	65.585191
1512.285532	43.305302	65.590196
1512.039607	43.316034	65.595201
1511.543115	44.420031	65.600206
1510.572263	43.945126	65.605210
1510.010801	38.100089	65.610215
1509.143097	43.500513	65.615220
1508.900198	37.688432	65.620225
1508.640383	47.527742	65.625230
1507.339204	37.447704	65.630234
1506.773769	39.512020	65.635239
1505.951843	39.191652	65.640244
1505.407390	48.139451	65.645249
1504.278380	46.019626	65.650254
1503.770003	38.980239	65.655258
1503.578610	41.824083	65.660263
1502.719013	44.354635	65.665268
1502.681026	33.652790	65.670273
1501.376113	47.397286	65.675278
1500.594589	40.786101	65.680282
1500.445542	37.469711	65.685287
1499.583011	45.720556	65.690292
1498.428770	39.496624	65.695297
1497.687940	38.598800	65.700302
1497.689159	38.962932	65.705306
1497.304978	43.953766	65.710311
1496.239471	42.369500	65.715316
1495.501883	38.448027	65.720321
1494.887270	39.018845	65.725326
1494.152642	46.213267	65.730330
1494.008420	43.079042	65.735335
1492.489207	41.172630	65.740340
1492.054153	43.449626	65.745345
1491.448568	38.471078	65.750350
1491.015799	32.925729	65.755354
1490.934345	38.827274	65.760359
1489.296032	44.701850	65.765364
1488.929123	37.898615	65.770369
1487.992088	41.912830	65.775374
1487.763204	40.484197	65.780378
1487.290682	39.691973	65.785383
1486.081962	46.326208	65.790388
1485.531111	48.867623	65.795393
1485.036717	46.932387	65.800398
1484.260056	44.311855	65.805402
1483.690758	38.026507	65.810407
1482.616078	42.389041	65.815412
1482.646860	32.253458	65.820417
1481.926691	34.468531	65.825422
1480.882243	43.549413	65.830426
1480.042515	42.367680	65.835431
1479.373739	50.907872	65.840436
1479.426406	46.271003	65.845441
1478.529856	47.023833	65.850446
1477.465317	37.950187	65.855450
1476.884341	43.164696	65.860455
1476.054033	53.933651	65.865460
1475.946371	54.042264	65.870465
1474.826432	49.131273	65.875470
1474.095541	53.309859	65.880474
1473.685149	46.985061	65.885479
1473.146676	50.795585	65.890484
1472.944042	44.546582	65.895489
1471.638230	50.708959	65.900494
1470.724587	43.142611	65.905498
1470.468140	46.110341	65.910503
1469.626871	43.616781	65.915508
1469.487305	37.830862	65.920513
1468.615964	40.383791	65.925518
1467.690553	48.807071	65.930522
1467.571084	47.488788	65.935527
1466.611479	49.749807	65.940532
1465.786626	47.356144	65.945537
1464.922173	48.857690	65.950542
1464.421914	49.058666	65.955546
1464.272280	44.819818	65.960551
1462.577005	51.425737	65.965556
1462.132069	48.239958	65.970561
1461.595998	51.594344	65.975566
1461.458508	47.038163	65.980570
1460.787126	42.825470	65.985575
1459.509737	48.481844	65.990580
1459.111701	39.707564	65.995585
1458.618151	39.748197	66.000590
1458.051061	52.716253	66.005594
1457.771048	46.539477	66.010599
1456.290852	45.322347	66.015604
1455.604839	44.611372	66.020609
1455.376066	45.589246	66.025614
1454.639575	52.168940	66.030618
1454.052008	40.704438	66.035623
1452.875380	45.890619	66.040628
1452.687529	40.353659	66.045633
1452.090331	45.362585	66.050638
1451.312889	47.936867	66.055642
1450.573213	40.049554	66.060647
1449.354489	44.229985	66.065652
1449.128275	36.981757	66.070657
1448.832896	48.503083	66.075662
1448.305655	44.786320	66.080666
1447.409604	37.598826	66.085671
1446.734007	45.482491	66.090676
1446.261341	38.879008	66.095681
1444.954489	41.997925	66.100686
1444.410872	44.415191	66.105690
1444.375471	38.551214	66.110695
1443.421144	39.284854	66.115700
1442.912798	38.761694	66.120705
1441.671253	47.075950	66.125710
1440.787923	43.739076	66.130714
1440.925515	43.179481	66.135719
1440.014155	52.400083	66.140724
1439.768875	36.661097	66.145729
1438.887638	44.508060	66.150734
1438.019645	47.257594	66.155738
1437.700247	40.975116	66.160743
1436.195985	42.878000	66.165748
1435.526675	40.691446	66.170753
1435.021240	41.410510	66.175758
1434.500644	44.533774	66.180762
1434.136041	38.815168	66.185767
1433.802953	42.069482	66.190772
1433.711793	39.038798	66.195777
1432.584289	48.585503	66.200782
1431.411263	46.712413	66.205786
1430.710599	44.694853	66.210791
1429.685610	43.555200	66.215796
1428.942457	39.860147	66.220801
1428.572137	49.057830	66.225806
1428.171288	40.938466	66.230810
1427.927632	43.964092	66.235815
1427.079941	47.216623	66.240820
1426.488611	41.002604	66.245825
1425.570690	44.097558	66.250830
1424.622207	46.139195	66.255834
1424.046206	37.907320	66.260839
1422.849244	46.230267	66.265844
1422.994524	34.617752	66.270849
1422.640639	40.128921	66.275854
1421.900353	42.116964	66.280858
1421.067440	40.484719	66.285863
1420.240528	34.752869	66.290868
1419.944798	37.543911	66.295873
1418.705663	37.521710	66.300878
1417.757425	42.999618	66.305882
1417.504377	38.468121	66.310887
1416.919623	46.034565	66.315892
1416.506180	52.061427	66.320897
1415.999933	47.880847	66.325902
1414.520302	42.099779	66.330906
1414.509658	41.117452	66.335911
1413.611728	38.344326	66.340916
1413.266040	34.586099	66.345921
1411.904338	43.365759	66.350926
1411.390883	43.898438	66.355930
1411.419163	36.289630	66.360935
1410.697029	51.994793	66.365940
1409.691842	45.373460	66.370945
1408.697223	41.447139	66.375950
1408.211035	41.191710	66.380954
1407.999902	40.484112	66.385959
1406.971416	46.135636	66.390964
1406.150518	38.893633	66.395969
1405.333758	41.592453	66.400974
1404.743591	46.841553	66.405978
1404.757070	43.584494	66.410983
1403.744092	40.107389	66.415988
1402.787087	44.061726	66.420993
1402.271123	47.200029	66.425998
1401.718133	49.732338	66.431002
1401.539850	37.278668	66.436007
1400.381512	42.826251	66.441012
1399.728809	33.180960	66.446017
1398.933760	38.558825	66.451022
1398.362063	41.412663	66.456026
1398.583461	39.688526	66.461031
1397.028483	49.888267	66.466036
1396.488425	37.842203	66.471041
1395.833081	44.065218	66.476046
1394.505895	38.185813	66.481050
1393.917602	31.939784	66.486055
1393.493291	35.216487	66.491060
1393.268250	40.035370	66.496065
1392.786645	33.538984	66.501070
1392.259569	39.858306	66.506074
1391.135465	30.414119	66.511079
1390.181996	38.485470	66.516084
1390.088900	29.085554	66.521089
1389.547474	34.730619	66.526094
1388.375650	30.949178	66.531098
1387.830776	27.495444	66.536103
1387.086916	38.911431	66.541108
1386.954308	34.548458	66.546113
1385.907909	35.167439	66.551118
1384.894980	35.558742	66.556122
1384.665402	37.303176	66.561127
1383.956849	46.341732	66.566132
1383.596534	35.569713	66.571137
1382.336042	33.489771	66.576142
1381.537628	38.505463	66.581146
1381.388940	31.721182	66.586151
1380.670742	41.067209	66.591156
1380.025051	36.512978	66.596161
1379.230038	35.772042	66.601166
1378.403624	37.130368	66.606170
1378.398968	30.195453	66.611175
1377.418144	48.065973	66.616180
1376.202488	36.704504	66.621185
1375.753175	28.097683	66.626190
1375.203951	33.177842	66.631194
1374.753594	32.388425	66.636199
1374.369243	28.787746	66.641204
1373.597095	41.424107	66.646209
1373.067376	34.410230	66.651214
1371.698769	41.145622	66.656218
1371.062420	34.959281	66.661223
1370.023270	31.003788	66.666228
1370.115810	26.951968	66.671233
1369.516924	33.170739	66.676238
1368.937923	36.054129	66.681242
1368.515565	43.959052	66.686247
1367.173245	34.607915	66.691252
1366.825732	35.032217	66.696257
1366.524210	41.159562	66.701262
1365.056294	43.952450	66.706266
1364.442022	40.495558	66.711271
1363.634978	39.425367	66.716276
1363.599005	30.099954	66.721281
1363.064967	29.686555	66.726286
1361.875248	43.379666	66.731290
1361.367484	33.071082	66.736295
1360.575051	34.185882	66.741300
1360.516354	31.880199	66.746305
1359.615446	31.644977	66.751310
1358.819564	36.130396	66.756314
1358.023117	40.855612	66.761319
1357.509842	45.147866	66.766324
1357.171468	42.352038	66.771329
1356.256700	38.228536	66.776334
1355.343565	39.737856	66.781338
1354.772621	29.254810	66.786343
1354.340046	39.621490	66.791348
1353.208650	42.927031	66.796353
1352.712422	42.595935	66.801358
1352.147393	38.118778	66.806362
1351.926371	38.814719	66.811367
1351.086967	36.423412	66.816372
1350.294017	34.046798	66.821377
1349.466042	29.926850	66.826382
1348.815139	28.500669	66.831386
1348.723117	29.975645	66.836391
1347.209757	42.099048	66.841396
1346.484825	32.629270	66.846401
1346.297985	40.102496	66.851406
1345.549630	39.966032	66.856410
1345.172086	37.384600	66.861415
1343.865825	47.235729	66.866420
1343.449711	37.071854	66.871425
1342.864645	34.354676	66.876430
1342.414058	37.182961	66.881434
1342.295352	30.507464	66.886439
1340.769202	36.574031	66.891444
1340.398930	39.810610	66.896449
1339.684913	27.560411	66.901454
1339.012056	38.287002	66.906458
1338.058844	32.791315	66.911463
1337.348550	41.079496	66.916468
1336.678038	30.828336	66.921473
1336.254973	47.424275	66.926478
1335.940937	46.447604	66.931482
1335.226796	35.041121	66.936487
1334.414645	42.582225	66.941492
1333.713151	35.695021	66.946497
1333.567952	38.651379	66.951502
1331.981656	36.329939	66.956506
1331.728524	35.272621	66.961511
1330.916510	37.653728	66.966516
1330.421981	29.883614	66.971521
1330.057828	41.330709	66.976526
1328.341569	34.179051	66.981530
1328.026717	26.992252	66.986535
1327.407497	33.143298	66.991540
1327.288382	34.581580	66.996545
1327.001975	34.750159	67.001550
1325.914219	42.642601	67.006554
1325.358714	35.730611	67.011559
1324.452591	38.749601	67.016564
1324.125191	36.262706	67.021569
1323.072429	41.616908	67.026574
1322.586321	34.208167	67.031578
1321.952697	37.929758	67.036583
1320.969511	31.935778	67.041588
1320.190781	28.822028	67.046593
1319.501098	36.531325	67.051598
1318.925984	36.946087	67.056602
1318.911717	33.368580	67.061607
1318.054932	35.808851	67.066612
1317.433769	35.005599	67.071617
1316.449641	30.484698	67.076622
1315.867825	39.827975	67.081626
1315.617482	33.966645	67.086631
1314.312069	33.600205	67.091636
1313.809499	37.479163	67.096641
1313.082880	37.052237	67.101646
1312.609245	46.919233	67.106650
1312.055908	42.407109	67.111655
1311.004428	40.347589	67.116660
1310.354473	40.244378	67.121665
1310.263149	37.584326	67.126670
1309.508338	34.438389	67.131674
1308.760247	33.573317	67.136679
1307.812609	41.736809	67.141684
1307.465541	36.725097	67.146689
1306.646583	32.398719	67.151694
1305.241154	43.579278	67.156698
1305.244356	38.444061	67.161703
1304.381607	45.687279	67.166708
1304.481777	36.239294	67.171713
1303.745698	36.518798	67.176718
1302.526591	43.798176	67.181722
1302.170298	34.723978	67.186727
1301.396685	33.353592	67.191732
1300.971018	40.968875	67.196737
1299.745980	36.098340	67.201742
1299.029867	41.034733	67.206746
1299.018187	25.444742	67.211751
1298.055004	35.465267	67.216756
1297.435704	29.479674	67.221761
1296.371638	32.332967	67.226766
1295.829776	37.929230	67.231770
1295.616056	35.167211	67.236775
1294.913986	34.425716	67.241780
1294.021790	29.713583	67.246785
1293.454696	33.700576	67.251790
1292.759258	37.249069	67.256794
1292.664864	36.767356	67.261799
1291.179310	41.283605	67.266804
1290.711840	41.296467	67.271809
1290.323203	31.459414	67.276814
1289.201662	41.150298	67.281818
1288.079158	30.520001	67.286823
1287.593025	35.787270	67.291828
1287.918656	34.033936	67.296833
1287.108790	31.048154	67.301838
1286.394135	27.022179	67.306842
1285.668082	30.931943	67.311847
1284.757423	29.376766	67.316852
1284.203738	34.273140	67.321857
1283.743091	30.831271	67.326862
1282.804992	33.509993	67.331866
1281.886120	27.614620	67.336871
1281.081415	41.766947	67.341876
1281.019867	33.248306	67.346881
1280.548063	40.500329	67.351886
1279.737437	34.371692	67.356890
1279.327143	29.997690	67.361895
1278.575332	35.009150	67.366900
1277.365416	36.783315	67.371905
1276.590943	30.071746	67.376910
1276.127887	39.657928	67.381914
1275.994322	35.659406	67.386919
1275.004796	37.885823	67.391924
1274.099091	33.909153	67.396929
1273.318123	30.839931	67.401934
1273.050161	39.336918	67.406938
1272.758254	32.438225	67.411943
1271.432668	37.085170	67.416948
1270.825280	32.528037	67.421953
1270.494888	36.630366	67.426958
1269.725086	42.822718	67.431962
1269.262910	33.052558	67.436967
1267.606611	46.365716	67.441972
1267.416177	32.043677	67.446977
1267.017572	34.917325	67.451982
1266.385691	45.711536	67.456986
1266.054738	30.134467	67.461991
1264.847270	36.453184	67.466996
1264.443907	35.963831	67.472001
1264.161848	39.697342	67.477006
1263.168825	35.518510	67.482010
1262.035962	28.446031	67.487015
1261.343827	35.938101	67.492020
1261.263801	28.660355	67.497025
1260.742009	32.687461	67.502030
1259.205048	35.289527	67.507034
1258.865213	34.439976	67.512039
1258.079456	43.112348	67.517044
1258.113745	42.548670	67.522049
1257.550263	39.411749	67.527054
1256.415436	36.006127	67.532058
1255.967193	29.471356	67.537063
1255.165726	30.221758	67.542068
1254.275606	30.836442	67.547073
1253.450574	36.802603	67.552078
1252.624035	36.344274	67.557082
1252.636804	33.522589	67.562087
1251.432565	38.856747	67.567092
1251.395613	36.669040	67.572097
1250.892753	30.740641	67.577102
1249.789285	31.570610	67.582106
1249.455272	28.159075	67.587111
1248.506567	37.291034	67.592116
1247.835865	26.726116	67.597121
1247.250941	30.616601	67.602126
1246.372341	30.037239	67.607130
1246.201102	27.762075	67.612135
1244.987661	31.560114	67.617140
1244.263786	26.887469	67.622145
1243.869855	30.246094	67.627150
1243.729316	30.637498	67.632154
1242.687133	28.953436	67.637159
1241.338621	36.393767	67.642164
1241.023361	34.477408	67.647169
1240.321699	30.414686	67.652174
1240.259140	25.947547	67.657178
1239.699204	28.127738	67.662183
1238.219694	36.773235	67.667188
1238.008735	36.806818	67.672193
1237.579362	35.383286	67.677198
1236.493867	35.279967	67.682202
1235.918890	27.282969	67.687207
1234.981206	29.188908	67.692212
1234.565601	25.591649	67.697217
1234.339299	20.871422	67.702222
1233.081730	34.419232	67.707226
1232.651196	27.928961	67.712231
1231.985709	32.606572	67.717236
1231.737404	21.395729	67.722241
1230.871072	24.780592	67.727246
1229.857763	30.530685	67.732250
1229.637444	26.091789	67.737255
1228.993326	27.667183	67.742260
1228.096880	35.627005	67.747265
1227.208511	25.754323	67.752270
1226.292891	30.416517	67.757274
1226.268886	23.560392	67.762279
1225.476789	30.284591	67.767284
1224.114427	16.010174	67.772289
1223.709895	24.935739	67.777294
1223.535497	22.509688	67.782298
1223.411135	22.070593	67.787303
1222.128345	29.789069	67.792308
1221.300487	26.005053	67.797313
1220.670289	29.574725	67.802318
1220.180216	30.576825	67.807322
1219.375203	25.182207	67.812327
1218.083577	26.426901	67.817332
1217.733631	22.377643	67.822337
1217.436538	27.868752	67.827342
1216.959773	26.772894	67.832346
1216.792303	30.045043	67.837351
1215.391747	43.273396	67.842356
1214.674790	31.460545	67.847361
1214.239849	37.334715	67.852366
1213.696956	33.762433	67.857370
1213.037038	21.423261	67.862375
1212.194311	32.779298	67.867380
1211.679653	31.247905	67.872385
1211.122705	29.071934	67.877390
1210.047830	37.455966	67.882394
1209.467880	33.424362	67.887399
1208.856909	29.099637	67.892404
1208.342406	24.862078	67.897409
1207.249238	31.746131	67.902414
1206.251684	38.772682	67.907418
1206.077956	31.629696	67.912423
1205.735890	36.222759	67.917428
1205.397854	28.486142	67.922433
1204.388300	31.311877	67.927438
1203.372039	36.841670	67.932442
1202.803146	25.432649	67.937447
1202.508346	33.096511	67.942452
1201.817680	28.221472	67.947457
1200.677476	25.550042	67.952462
1200.293715	31.729896	67.957466
1200.148687	23.429558	67.962471
1198.838548	28.722227	67.967476
1197.840480	29.772006	67.972481
1197.300615	31.042234	67.977486
1196.984699	45.826494	67.982490
1196.805863	38.974487	67.987495
1195.716325	44.848688	67.992500
1194.807874	38.335080	67.997505
1194.454737	31.739464	68.002510
1193.948268	34.076747	68.007514
1193.128784	30.299293	68.012519
1191.702509	43.646868	68.017524
1191.590981	39.982329	68.022529
1190.873849	37.331927	68.027534
1190.297028	33.033315	68.032538
1190.489692	34.535559	68.037543
1189.046684	38.430062	68.042548
1188.268212	44.735780	68.047553
1188.166637	35.329351	68.052558
1186.875868	35.706572	68.057562
1186.226454	26.934502	68.062567
1185.824923	28.362510	68.067572
1185.536630	30.576781	68.072577
1184.575387	33.216639	68.077582
1183.370240	37.068582	68.082586
1183.262923	27.656765	68.087591
1182.605346	38.120742	68.092596
1181.880419	31.172663	68.097601
1180.914985	37.088631	68.102606
1179.999882	41.419589	68.107610
1179.975208	33.724601	68.112615
1179.621629	39.055961	68.117620
1178.781227	31.011305	68.122625
1177.702260	32.278969	68.127630
1177.187599	37.785764	68.132634
1176.852602	25.549471	68.137639
1175.770826	27.984567	68.142644
1174.926413	22.941597	68.147649
1174.338621	34.121473	68.152654
1174.068691	37.167062	68.157658
1173.502569	25.472173	68.162663
1172.121310	38.727433	68.167668
1171.601734	23.715006	68.172673
1171.283823	34.140728	68.177678
1170.694248	38.088741	68.182682
1170.126897	28.899909	68.187687
1169.314246	35.510695	68.192692
1168.761983	35.199587	68.197697
1168.195020	32.900635	68.202702
1167.067377	34.005729	68.207706
1166.284006	32.364116	68.212711
1165.577742	45.791155	68.217716
1165.313316	35.546432	68.222721
1165.024899	26.811572	68.227726
1164.056200	36.605922	68.232730
1163.406160	36.406564	68.237735
1162.569068	38.424267	68.242740
1162.109564	27.631816	68.247745
1160.936985	32.819043	68.252750
1159.967194	35.599046	68.257754
1159.613269	29.710062	68.262759
1159.100959	38.596010	68.267764
1158.932682	27.640541	68.272769
1158.717603	29.119323	68.277774
1157.341696	42.569291	68.282778
1156.933153	36.706340	68.287783
1156.073043	39.443667	68.292788
1155.185811	26.049381	68.297793
1154.376341	31.702420	68.302798
1153.553123	35.176649	68.307802
1153.507919	34.333868	68.312807
1152.908735	40.511724	68.317812
1152.649179	30.389239	68.322817
1151.676151	36.916725	68.327822
1151.072508	34.311365	68.332826
1150.521044	27.297859	68.337831
1149.151765	41.401232	68.342836
1148.311195	37.620839	68.347841
1148.283135	40.041312	68.352846
1147.124341	37.577873	68.357850
1147.138776	31.598759	68.362855
1145.736079	43.509104	68.367860
1145.433413	28.435370	68.372865
1145.037995	25.754313	68.377870
1144.389206	32.499894	68.382874
1143.546709	32.925685	68.387879
1142.546975	37.090337	68.392884
1141.868630	38.874630	68.397889
1141.662165	33.559879	68.402894
1141.095133	43.350275	68.407898
1140.300129	35.292104	68.412903
1139.526522	36.497019	68.417908
1139.061218	32.742098	68.422913
1138.506254	32.347845	68.427918
1137.446776	36.274411	68.432922
1137.039555	29.118113	68.437927
1136.418936	34.913012	68.442932
1135.128185	28.515440	68.447937
1134.737211	35.316211	68.452942
1133.906355	39.340459	68.457946
1133.820352	31.283059	68.462951
1133.134531	35.126535	68.467956
1132.482050	33.866249	68.472961
1131.544978	34.015342	68.477966
1130.995292	38.109988	68.482970
1130.381995	29.740635	68.487975
1128.976106	35.543749	68.492980
1128.448516	25.454446	68.497985
1128.153622	35.980591	68.502990
1127.443555	34.308406	68.507994
1127.577997	29.355760	68.512999
1126.818686	36.372824	68.518004
1125.663012	39.400034	68.523009
1125.132555	35.540358	68.528014
1124.593268	37.599012	68.533018
1123.407121	34.581676	68.538023
1122.369674	43.237340	68.543028
1122.349257	32.841846	68.548033
1121.911174	28.355600	68.553038
1121.554676	45.790949	68.558042
1120.495842	36.494224	68.563047
1119.550858	38.801924	68.568052
1119.299096	43.087309	68.573057
1118.673420	36.760572	68.578062
1117.280876	34.335908	68.583066
1116.890419	29.233363	68.588071
1116.265972	34.743437	68.593076
1116.003261	32.615304	68.598081
1114.766807	37.520965	68.603086
1113.690936	34.836187	68.608090
1113.792112	36.734613	68.613095
1113.079718	38.697801	68.618100
1113.034789	36.837809	68.623105
1112.300249	36.290772	68.628110
1111.220091	32.668359	68.633114
1110.719274	31.245176	68.638119
1109.238073	31.430371	68.643124
1108.274691	33.121238	68.648129
1108.818077	32.279449	68.653134
1107.745112	33.345907	68.658138
1107.132688	33.135849	68.663143
1106.827038	36.393713	68.668148
1106.193002	34.111754	68.673153
1105.078398	28.026812	68.678158
1104.262670	32.400332	68.683162
1104.167042	26.519159	68.688167
1102.832808	40.435618	68.693172
1102.182116	34.811481	68.698177
1101.746901	31.671545	68.703182
1101.316493	40.527124	68.708186
1101.132542	32.286605	68.713191
1099.819962	37.690102	68.718196
1099.156638	35.057977	68.723201
1098.688939	33.889735	68.728206
1098.124381	33.971696	68.733210
1097.064247	18.207904	68.738215
1096.118778	38.277490	68.743220
1095.707824	33.851590	68.748225
1095.375177	34.522729	68.753230
1094.485060	29.815076	68.758234
1094.684937	25.785609	68.763239
1093.443972	32.212228	68.768244
1092.993096	25.482370	68.773249
1092.234488	29.848383	68.778254
1090.790082	30.540262	68.783258
1090.732388	26.889248	68.788263
1090.184708	27.561480	68.793268
1089.699390	25.154940	68.798273
1088.638413	31.906177	68.803278
1087.558050	30.113134	68.808282
1087.548750	27.755450	68.813287
1086.720062	40.727292	68.818292
1085.810283	30.452788	68.823297
1085.188184	28.258826	68.828302
1084.320358	28.425307	68.833306
1084.153055	29.193150	68.838311
1083.771236	29.173501	68.843316
1082.869034	30.454085	68.848321
1081.939543	37.648048	68.853326
1081.234871	30.643165	68.858330
1081.192363	31.346999	68.863335
1079.578314	30.594527	68.868340
1079.099144	30.118841	68.873345
1078.879574	27.394051	68.878350
1078.134144	33.047961	68.883354
1078.092920	25.590594	68.888359
1076.721246	33.189227	68.893364
1076.249713	28.616847	68.898369
1075.671956	29.558803	68.903374
1074.420970	34.014193	68.908378
1074.107020	21.353522	68.913383
1073.196975	33.988209	68.918388
1073.083352	24.940124	68.923393
1072.509052	27.502690	68.928398
1071.207845	27.891092	68.933402
1070.591044	26.472177	68.938407
1070.219425	29.705844	68.943412
1069.797366	30.406981	68.948417
1068.824668	26.105152	68.953422
1068.100759	34.669945	68.958426
1067.733910	31.929160	68.963431
1066.936932	34.333184	68.968436
1066.168396	27.220193	68.973441
1065.427123	28.542991	68.978446
1064.882667	31.939778	68.983450
1064.562053	32.519118	68.988455
1063.406918	26.798625	68.993460
1062.212207	31.943680	68.998465
1062.026366	24.780567	69.003470
1061.440269	30.364975	69.008474
1061.050704	22.904681	69.013479
1060.790947	38.217751	69.018484
1059.807573	27.805153	69.023489
1059.007786	28.938560	69.028494
1058.214428	35.256135	69.033498
1057.718250	22.116664	69.038503
1056.564036	33.115423	69.043508
1056.271860	32.285129	69.048513
1055.978777	22.885541	69.053518
1055.235076	37.291554	69.058522
1054.217797	22.984425	69.063527
1053.473317	36.720335	69.068532
1053.136932	33.883239	69.073537
1052.682565	23.936859	69.078542
1051.471969	27.800763	69.083546
1050.788055	30.603131	69.088551
1050.067763	35.070297	69.093556
1049.952682	28.883131	69.098561
1049.632611	26.825635	69.103566
1048.398794	40.426508	69.108570
1048.188013	35.025720	69.113575
1047.024648	33.277441	69.118580
1046.206497	30.020240	69.123585
1045.252079	38.673755	69.128590
1044.755246	37.786134	69.133594
1044.641932	30.171498	69.138599
1043.962625	34.124348	69.143604
1042.829024	30.221879	69.148609
1042.211825	31.460286	69.153614
1041.471952	32.716635	69.158618
1041.464633	23.011378	69.163623
1040.722433	32.151537	69.168628
1040.051951	24.627129	69.173633
1039.539247	36.004815	69.178638
1038.605888	32.709175	69.183642
1037.834888	27.080547	69.188647
1036.677730	32.839400	69.193652
1036.194055	26.980549	69.198657
1036.063405	28.239320	69.203662
1035.201898	31.099911	69.208666
1034.183717	28.325564	69.213671
1033.543203	30.140135	69.218676
1033.066100	28.634346	69.223681
1032.949001	32.985042	69.228686
1031.866742	35.335115	69.233690
1031.185425	29.996582	69.238695
1030.574312	31.412225	69.243700
1029.809479	32.044900	69.248705
1029.517900	21.072807	69.253710
1028.370468	37.060137	69.258714
1028.250661	16.928288	69.263719
1027.465638	32.011100	69.268724
1026.684182	25.537290	69.273729
1025.742319	24.069180	69.278734
1024.803383	34.956425	69.283738
1024.672596	29.601264	69.288743
1024.185876	26.554699	69.293748
1023.386608	37.772972	69.298753
1022.385721	25.084411	69.303758
1021.623824	31.901629	69.308762
1021.420008	26.575437	69.313767
1021.044140	42.036296	69.318772
1020.013740	27.477372	69.323777
1019.501569	21.377049	69.328782
1018.699233	31.069269	69.333786
1018.227169	18.898989	69.338791
1016.724268	32.927468	69.343796
1016.181214	27.648945	69.348801
1015.973258	24.878158	69.353806
1015.371915	26.506722	69.358810
1015.276144	24.665864	69.363815
1014.406218	33.640265	69.368820
1013.552018	30.601708	69.373825
1012.703158	28.803403	69.378830
1011.858513	30.570032	69.383834
1011.402554	21.997488	69.388839
1010.412687	31.894596	69.393844
1010.157729	25.778580	69.398849
1009.734740	30.028132	69.403854
1008.762921	33.724748	69.408858
1008.125483	27.325803	69.413863
1007.367859	32.756159	69.418868
1007.109850	25.678656	69.423873
1006.254475	23.867198	69.428878
1005.200886	29.696318	69.433882
1004.795410	22.345805	69.438887
1004.101277	33.518965	69.443892
1003.223986	30.141876	69.448897
1002.880741	27.938260	69.453902
1002.000469	30.333477	69.458906
1001.820317	23.994241	69.463911
1000.734030	32.810678	69.468916
1000.143303	29.017397	69.473921
999.689282	36.831185	69.478926
998.790001	39.473865	69.483930
998.246986	27.406341	69.488935
997.150288	36.501990	69.493940
996.301340	34.366226	69.498945
996.065294	31.946850	69.503950
995.354417	39.348912	69.508954
995.253497	30.417088	69.513959
994.704506	29.290188	69.518964
993.523436	34.532452	69.523969
993.399240	31.043418	69.528974
992.144731	36.350988	69.533978
991.609002	34.409821	69.538983
990.632855	38.018821	69.543988
990.197604	35.459250	69.548993
989.741152	37.684528	69.553998
988.633608	34.733602	69.559002
988.225014	31.559490	69.564007
987.567452	37.152131	69.569012
987.339893	33.701623	69.574017
986.385581	32.855270	69.579022
985.056494	38.791318	69.584026
984.679363	27.107424	69.589031
984.165646	34.109093	69.594036
983.978036	35.999846	69.599041
983.438738	36.407407	69.604046
981.940611	43.141512	69.609050
981.628976	34.752590	69.614055
980.994046	37.167124	69.619060
980.865980	33.344382	69.624065
979.826341	35.101048	69.629070
979.008929	37.532004	69.634074
978.586634	28.444737	69.639079
977.310359	34.621550	69.644084
976.526859	32.912208	69.649089
976.417386	35.096466	69.654094
975.797761	44.179292	69.659098
975.594982	37.384746	69.664103
974.492799	37.041337	69.669108
973.522880	27.667465	69.674113
973.257398	37.600708	69.679118
972.531558	40.512274	69.684122
971.802788	33.577497	69.689127
970.516814	36.527733	69.694132
970.228127	38.138095	69.699137
969.966477	24.879327	69.704142
969.378604	31.247804	69.709146
968.642891	30.510179	69.714151
967.809942	39.806728	69.719156
967.213946	34.889890	69.724161
966.894393	27.364856	69.729166
965.195328	30.678883	69.734170
964.757411	31.035620	69.739175
964.105728	27.264666	69.744180
964.064687	20.209419	69.749185
963.874581	24.680543	69.754190
962.442386	43.036136	69.759194
961.977257	35.557921	69.764199
961.609288	29.967690	69.769204
960.507290	28.889375	69.774209
959.521807	30.820363	69.779214
958.855949	33.034812	69.784218
958.709953	26.592372	69.789223
958.151399	26.504669	69.794228
957.282426	25.870259	69.799233
956.444266	25.148941	69.804238
956.143216	41.187691	69.809242
955.267138	22.139755	69.814247
954.253894	26.432780	69.819252
953.777556	26.663165	69.824257
953.352092	33.053109	69.829262
952.475443	32.292185	69.834266
952.625947	26.983735	69.839271
951.692729	23.730689	69.844276
950.737829	22.900214	69.849281
949.510430	40.508836	69.854286
948.189616	35.680541	69.859290
948.553278	21.711970	69.864295
948.256455	34.476185	69.869300
947.427273	27.066952	69.874305
946.983252	26.817518	69.879310
945.928175	32.467118	69.884314
945.438853	26.325329	69.889319
944.871127	29.031959	69.894324
944.042955	31.303783	69.899329
942.930263	26.141166	69.904334
942.188308	36.314243	69.909338
941.687267	29.933037	69.914343
941.153894	34.033002	69.919348
940.676216	25.801411	69.924353
940.584646	25.748208	69.929358
939.600982	30.104342	69.934362
939.180809	27.301103	69.939367
938.363833	33.157249	69.944372
937.492387	32.108487	69.949377
936.593338	25.684966	69.954382
936.128005	28.586620	69.959386
935.903322	22.148822	69.964391
934.760530	20.454096	69.969396
933.696172	27.884033	69.974401
933.461054	37.262070	69.979406
932.918103	32.940793	69.984410
932.693797	24.697267	69.989415
931.122871	30.135644	69.994420
930.280765	22.586547	69.999425
930.235509	25.661053	70.004430
929.654527	32.399035	70.009434
928.727830	38.130717	70.014439
928.023285	33.347864	70.019444
927.490452	29.253644	70.024449
926.976031	27.078860	70.029454
926.595723	39.703396	70.034458
925.649034	27.933537	70.039463
924.544906	31.133982	70.044468
924.232871	28.515391	70.049473
923.884228	30.438083	70.054478
922.630790	31.955977	70.059482
922.020866	32.288055	70.064487
921.345628	28.487745	70.069492
920.931623	35.675410	70.074497
920.691320	25.616148	70.079502
919.699546	35.018409	70.084506
918.901367	31.198240	70.089511
918.502216	32.657448	70.094516
917.347494	33.729111	70.099521
916.582899	31.830694	70.104526
915.967043	33.116227	70.109530
915.577084	25.009459	70.114535
914.943191	36.862196	70.119540
914.477410	21.920155	70.124545
913.942773	33.679820	70.129550
913.007035	25.943774	70.134554
912.609359	26.436046	70.139559
911.613476	31.593674	70.144564
910.908629	24.915322	70.149569
910.177475	20.220296	70.154574
909.736008	33.048531	70.159578
909.282359	28.317221	70.164583
908.493171	24.624941	70.169588
907.651390	37.906412	70.174593
907.237228	31.109252	70.179598
905.912355	39.247738	70.184602
905.358260	21.544232	70.189607
904.800785	24.490519	70.194612
904.450842	37.770984	70.199617
904.067681	30.590411	70.204622
903.449432	33.721419	70.209626
902.448808	24.428167	70.214631
901.705840	32.111326	70.219636
901.160575	28.378648	70.224641
900.032496	30.901650	70.229646
899.026240	31.419820	70.234650
899.136042	28.705708	70.239655
898.734509	30.133757	70.244660
898.160419	28.488886	70.249665
897.153776	27.130487	70.254670
896.239785	36.290133	70.259674
895.829091	26.773675	70.264679
895.009036	27.741619	70.269684
894.678770	21.800041	70.274689
893.984977	30.170831	70.279694
893.221442	18.788961	70.284698
892.954808	28.209068	70.289703
891.935250	25.985376	70.294708
890.701990	27.168903	70.299713
890.221685	26.906330	70.304718
889.981923	26.044059	70.309722
889.810165	23.355838	70.314727
888.378605	18.915016	70.319732
887.585496	20.101030	70.324737
887.263027	18.517042	70.329742
886.688969	19.999361	70.334746
885.865373	20.204602	70.339751
884.909922	24.616978	70.344756
884.425831	29.500762	70.349761
884.163785	26.405852	70.354766
883.778385	28.291819	70.359770
882.897431	22.916513	70.364775
881.660500	32.267126	70.369780
881.528377	20.453591	70.374785
880.367594	20.614729	70.379790
879.132618	32.004093	70.384794
879.001552	19.212650	70.389799
878.336068	28.268874	70.394804
877.986366	27.622806	70.399809
877.928333	23.382851	70.404814
877.043054	28.343896	70.409818
876.474884	12.896975	70.414823
875.458130	25.232495	70.419828
874.351307	26.906852	70.424833
873.839754	22.546690	70.429838
873.035635	28.122464	70.434842
873.021522	16.320114	70.439847
872.239171	21.205637	70.444852
871.347131	26.532047	70.449857
870.671367	17.072775	70.454862
870.231494	20.221128	70.459866
869.553944	19.684017	70.464871
868.203768	30.691162	70.469876
867.669645	23.934399	70.474881
867.672268	18.436596	70.479886
866.911136	24.741198	70.484890
866.407989	16.997826	70.489895
865.491270	18.178289	70.494900
864.746352	30.353849	70.499905
864.616305	28.456952	70.504910
862.965591	33.024949	70.509914
862.608514	15.674107	70.514919
861.815858	18.880193	70.519924
861.813828	21.674995	70.524929
861.255960	20.513268	70.529934
859.892557	31.196083	70.534938
859.312915	18.342002	70.539943
858.581888	21.314345	70.544948
858.510777	20.141373	70.549953
857.557193	19.523620	70.554958
856.698886	28.508035	70.559962
856.135425	18.469479	70.564967
855.695295	17.110812	70.569972
854.783483	29.585759	70.574977
853.981422	26.623333	70.579982
853.101464	18.783819	70.584986
852.841283	21.023607	70.589991
852.442206	27.002493	70.594996
851.757102	25.006287	70.600001
850.783380	18.347103	70.605006
850.190100	24.352170	70.610010
849.773739	26.113756	70.615015
848.566898	22.593638	70.620020
848.021025	26.925849	70.625025
847.616760	28.371687	70.630030
846.956401	28.645578	70.635034
846.583409	22.437989	70.640039
845.279454	22.096793	70.645044
844.695610	20.666384	70.650049
844.499834	24.039245	70.655054
844.127865	29.328611	70.660058
843.509552	18.060846	70.665063
842.373614	26.989318	70.670068
841.701816	30.356739	70.675073
840.601414	18.363022	70.680078
839.379659	30.113004	70.685082
839.057508	24.491063	70.690087
838.966862	28.104242	70.695092
838.418845	27.052918	70.700097
838.283970	18.853526	70.705102
837.237047	32.007595	70.710106
836.642601	28.693571	70.715111
835.923913	27.426559	70.720116
835.226905	26.831051	70.725121
834.363861	16.511389	70.730126
833.665771	25.015339	70.735130
833.014146	19.604337	70.740135
832.547676	21.025385	70.745140
831.520694	15.204192	70.750145
831.002001	32.451645	70.755150
830.114744	29.685720	70.760154
830.059131	24.294962	70.765159
829.350270	21.843638	70.770164
828.417899	19.178729	70.775169
827.739036	22.800385	70.780174
827.353129	17.621485	70.785178
826.496642	24.748699	70.790183
825.487119	23.572143	70.795188
824.825512	25.896337	70.800193
824.557561	19.508026	70.805198
824.009205	30.225906	70.810202
823.174821	18.788323	70.815207
822.476992	20.776074	70.820212
821.954481	28.343726	70.825217
821.429428	17.423046	70.830222
820.096774	31.132763	70.835226
819.809137	24.794893	70.840231
818.934286	28.165469	70.845236
818.472591	18.699735	70.850241
818.425336	21.131140	70.855246
817.126331	25.480743	70.860250
816.481707	20.128558	70.865255
816.054822	22.473736	70.870260
815.284199	18.761188	70.875265
814.508653	24.995556	70.880270
813.426900	27.271516	70.885274
813.212705	29.450369	70.890279
812.551902	28.163110	70.895284
811.957280	31.481193	70.900289
811.063498	18.307332	70.905294
810.525330	32.286404	70.910298
810.354865	30.891123	70.915303
809.492584	30.820265	70.920308
808.778260	30.599693	70.925313
808.181949	23.468848	70.930318
807.415352	29.856340	70.935322
806.526479	22.321049	70.940327
805.320729	33.230323	70.945332
804.830854	36.124078	70.950337
804.574646	31.239142	70.955342
804.190393	41.026498	70.960346
803.916250	24.843637	70.965351
802.839864	29.662447	70.970356
802.135408	25.710703	70.975361
802.017570	28.364664	70.980366
800.085263	33.174652	70.985370
799.605805	29.620764	70.990375
798.931007	32.260888	70.995380
798.458746	37.664002	71.000385
798.435980	22.237511	71.005390
797.572808	27.971732	71.010394
796.783394	19.376639	71.015399
795.831476	27.424252	71.020404
795.506484	29.985032	71.025409
795.244222	20.027071	71.030414
793.972785	29.469156	71.035418
793.539355	18.877683	71.040423
793.093571	24.523377	71.045428
791.666662	28.814505	71.050433
791.174400	14.922281	71.055438
790.090541	30.592033	71.060442
789.956073	20.608996	71.065447
789.844515	23.069563	71.070452
789.121085	24.389597	71.075457
788.463639	18.187884	71.080462
787.682045	23.264127	71.085466
787.221905	22.769699	71.090471
785.965986	26.183605	71.095476
785.057287	27.801226	71.100481
784.876624	17.707271	71.105486
784.315811	27.059879	71.110490
783.859488	13.352754	71.115495
782.670388	21.666793	71.120500
781.960921	19.879497	71.125505
781.470324	17.787690	71.130510
780.987314	28.398972	71.135514
780.379580	22.627751	71.140519
779.573005	21.571873	71.145524
778.644038	22.941980	71.150529
778.826315	18.227735	71.155534
777.333582	29.411370	71.160538
776.785887	25.756385	71.165543
776.106620	21.687097	71.170548
775.812595	16.482541	71.175553
775.392694	20.222256	71.180558
773.973524	24.849637	71.185562
773.717005	14.316742	71.190567
773.332191	23.841608	71.195572
772.147411	26.987144	71.200577
771.374155	23.289222	71.205582
770.621040	28.786726	71.210586
770.418404	27.199446	71.215591
770.048348	29.887255	71.220596
768.913679	21.667271	71.225601
768.296111	22.191420	71.230606
767.204592	28.641691	71.235610
767.326820	26.176342	71.240615
766.508814	25.805128	71.245620
765.222506	22.814961	71.250625
765.167464	24.664117	71.255630
764.788566	30.223472	71.260634
763.676873	25.098634	71.265639
762.719558	32.360197	71.270644
762.150723	31.047270	71.275649
761.917323	22.742144	71.280654
761.337731	32.149789	71.285658
760.507860	21.274503	71.290663
759.660024	27.078834	71.295668
759.087939	25.127741	71.300673
758.855336	16.861918	71.305678
757.346794	25.647887	71.310682
756.618184	26.388420	71.315687
756.330395	26.066836	71.320692
755.740295	22.896439	71.325697
755.548171	22.783557	71.330702
754.327879	37.782747	71.335706
753.765979	22.912836	71.340711
753.456873	23.883054	71.345716
752.839328	29.439404	71.350721
751.424505	20.384071	71.355726
750.559026	21.370331	71.360730
750.408708	16.234365	71.365735
750.106031	19.259963	71.370740
749.735913	23.363927	71.375745
748.900914	19.742079	71.380750
747.851959	25.821293	71.385754
747.216748	22.825242	71.390759
745.943735	29.115179	71.395764
745.324561	29.125488	71.400769
744.978294	18.819781	71.405774
744.255914	21.383911	71.410778
743.955519	17.251156	71.415783
743.596505	27.503644	71.420788
742.706807	25.562124	71.425793
741.810455	18.204677	71.430798
741.053864	26.730576	71.435802
740.691109	29.016669	71.440807
740.081051	30.137311	71.445812
738.964147	24.524446	71.450817
738.543799	19.805223	71.455822
737.604371	28.136302	71.460826
737.800027	20.437821	71.465831
736.770004	30.212086	71.470836
735.984046	31.173074	71.475841
735.748495	20.613189	71.480846
734.471749	19.073932	71.485850
733.914715	17.423233	71.490855
732.928638	22.055795	71.495860
732.498209	26.437454	71.500865
732.355762	13.126660	71.505870
731.533774	20.961207	71.510874
730.809549	20.224979	71.515879
730.088926	25.819823	71.520884
729.483418	25.697069	71.525889
729.059322	20.499038	71.530894
728.020419	23.977766	71.535898
727.748551	21.950493	71.540903
726.765602	26.251390	71.545908
725.746304	28.580522	71.550913
725.094672	22.090889	71.555918
724.636571	25.022963	71.560922
724.474547	19.680699	71.565927
723.172226	24.179111	71.570932
721.987060	14.913763	71.575937
721.983384	15.240822	71.580942
721.403790	26.763222	71.585946
721.249917	17.139690	71.590951
720.396638	15.428930	71.595956
719.564823	20.896396	71.600961
718.778407	19.599202	71.605966
718.265691	15.391447	71.610970
717.379975	15.724909	71.615975
716.349393	17.891832	71.620980
715.887402	24.901064	71.625985
715.862006	19.690014	71.630990
715.190201	22.750738	71.635994
714.079916	19.196392	71.640999
713.189913	20.486200	71.646004
712.678703	20.848342	71.651009
712.541533	23.141096	71.656014
711.500565	31.795867	71.661018
710.806179	22.594301	71.666023
710.307813	27.073516	71.671028
709.580001	25.738607	71.676033
709.299237	19.260890	71.681038
708.011757	26.292758	71.686042
707.462359	22.535558	71.691047
707.140650	23.534596	71.696052
706.135323	24.136275	71.701057
705.260575	15.409726	71.706062
704.512412	23.866478	71.711066
704.471957	17.292148	71.716071
704.164891	25.878941	71.721076
702.935762	26.423216	71.726081
702.338955	23.838967	71.731086
701.616401	28.863253	71.736090
701.284913	19.895651	71.741095
699.946406	27.465519	71.746100
699.314055	19.228666	71.751105
698.987626	18.105819	71.756110
698.317187	29.762541	71.761114
698.045099	25.055988	71.766119
696.828209	26.360006	71.771124
696.128780	19.950536	71.776129
695.721493	18.581939	71.781134
695.228500	21.204174	71.786138
694.502160	27.678324	71.791143
693.824704	24.577049	71.796148
693.304845	15.831841	71.801153
692.414052	20.999615	71.806158
691.083984	29.552190	71.811162
690.680891	16.891628	71.816167
690.499258	18.382463	71.821172
689.766877	15.446060	71.826177
689.473983	25.550820	71.831182
688.254014	22.332506	71.836186
687.383397	18.060322	71.841191
687.458499	15.591439	71.846196
686.621864	23.699574	71.851201
685.698692	15.370263	71.856206
684.822928	18.920802	71.861210
684.599315	26.368331	71.866215
684.092975	20.752886	71.871220
683.009898	26.572622	71.876225
682.718492	16.463205	71.881230
681.873729	17.089788	71.886234
681.301025	20.902735	71.891239
680.026899	18.634517	71.896244
679.518587	20.991105	71.901249
679.134277	22.082120	71.906254
678.655686	31.489460	71.911258
678.133449	23.954188	71.916263
677.141204	29.232745	71.921268
676.332354	38.733685	71.926273
676.353101	16.937895	71.931278
675.190313	20.251862	71.936282
674.156095	21.583573	71.941287
673.612617	20.219320	71.946292
673.213747	26.657095	71.951297
673.094668	21.435735	71.956302
671.841123	24.674269	71.961306
671.112958	28.519862	71.966311
670.841031	29.231849	71.971316
670.034681	20.742009	71.976321
669.018630	17.541696	71.981326
668.273207	26.482158	71.986330
667.857076	18.800680	71.991335
667.477269	20.556471	71.996340
666.576029	21.346599	72.001345
666.091693	14.726264	72.006350
665.238512	17.103082	72.011354
664.614907	20.034712	72.016359
664.242696	19.594116	72.021364
663.183756	20.691641	72.026369
662.615378	12.487196	72.031374
661.922498	19.355001	72.036378
661.723412	24.409474	72.041383
660.052584	16.606108	72.046388
659.536734	25.536819	72.051393
658.935597	18.638611	72.056398
658.787271	20.557817	72.061402
658.757914	14.546290	72.066407
657.479864	11.720454	72.071412
656.674935	13.592835	72.076417
656.495008	18.144348	72.081422
655.702260	15.206531	72.086426
654.628003	16.677093	72.091431
653.694341	15.269326	72.096436
653.192438	14.880926	72.101441
653.058105	14.202169	72.106446
652.078305	23.211499	72.111450
651.171739	12.387908	72.116455
650.343875	18.693724	72.121460
650.058280	14.762061	72.126465
649.834547	5.739470	72.131470
648.931718	15.308986	72.136474
648.257188	18.031105	72.141479
647.607298	13.176569	72.146484
646.588483	12.556671	72.151489
645.727046	18.946685	72.156494
645.032748	21.271396	72.161498
644.864090	19.927883	72.166503
644.329001	23.383178	72.171508
643.691656	17.523674	72.176513
642.896046	13.455612	72.181518
642.231132	22.107280	72.186522
641.870133	17.785493	72.191527
640.873314	13.651703	72.196532
639.782430	12.598573	72.201537
639.359547	16.518557	72.206542
638.703949	20.994436	72.211546
638.283826	11.441711	72.216551
638.187060	22.041950	72.221556
637.049202	24.016249	72.226561
636.749709	18.872513	72.231566
635.193146	24.332423	72.236570
634.663916	20.825927	72.241575
633.973085	21.081071	72.246580
633.581313	18.795356	72.251585
633.466727	24.792032	72.256590
632.113986	27.648981	72.261594
631.426728	13.833603	72.266599
631.286640	16.328677	72.271604
630.374957	24.002489	72.276609
629.121314	15.580754	72.281614
627.963168	25.476382	72.286618
628.343534	15.952288	72.291623
627.493003	20.864504	72.296628
627.183621	19.579676	72.301633
627.006786	29.419944	72.306638
625.617809	19.103713	72.311642
625.265880	22.796351	72.316647
624.710876	22.455839	72.321652
623.626356	28.685845	72.326657
622.844934	15.691312	72.331662
621.785193	26.539544	72.336666
621.713526	22.677893	72.341671
621.366108	19.550885	72.346676
620.472122	21.579392	72.351681
619.801319	17.004168	72.356686
619.002328	18.268473	72.361690
618.584271	14.972940	72.366695
617.513334	21.145588	72.371700
616.653504	17.937763	72.376705
616.509202	12.586384	72.381710
615.580778	28.422240	72.386714
615.460434	15.898022	72.391719
614.419189	21.116591	72.396724
613.575287	21.691019	72.401729
613.135248	17.023848	72.406734
612.723034	24.731656	72.411738
611.730495	18.771036	72.416743
610.836530	24.579600	72.421748
610.212434	28.006499	72.426753
609.679082	19.736562	72.431758
609.385868	29.956498	72.436762
608.427535	14.342373	72.441767
607.915920	24.581321	72.446772
606.873525	24.812041	72.451777
606.995752	16.559118	72.456782
605.809363	26.151738	72.461786
605.032140	15.624542	72.466791
604.379524	21.407282	72.471796
603.981093	23.140817	72.476801
603.499997	20.003564	72.481806
602.138098	27.266534	72.486810
601.554322	19.851477	72.491815
601.230679	29.109561	72.496820
600.843906	29.305246	72.501825
600.221221	23.845552	72.506830
599.001918	28.250375	72.511834
598.394820	25.830223	72.516839
598.055332	26.887301	72.521844
597.392247	23.176624	72.526849
596.775992	18.532793	72.531854
595.889200	32.827610	72.536858
595.314820	26.705769	72.541863
594.828099	27.800492	72.546868
593.741335	30.348584	72.551873
593.178587	23.346506	72.556878
592.619831	31.363097	72.561882
592.176961	26.131814	72.566887
591.265906	24.569079	72.571892
590.476778	28.487482	72.576897
590.244384	24.682973	72.581902
589.653276	27.213619	72.586906
588.759855	18.165235	72.591911
588.050174	20.687958	72.596916
587.186264	26.419202	72.601921
586.807660	26.687706	72.606926
585.494981	34.589416	72.611930
584.884613	21.725348	72.616935
584.767732	31.259590	72.621940
584.424051	25.089968	72.626945
584.132708	26.358581	72.631950
582.967731	28.587966	72.636954
582.125089	26.924447	72.641959
581.639066	23.934644	72.646964
580.522780	24.905717	72.651969
579.779870	25.178633	72.656974
579.040747	25.916160	72.661978
578.921667	23.301582	72.666983
578.195891	26.124925	72.671988
577.207114	25.993870	72.676993
576.953771	25.466542	72.681998
576.106941	24.630038	72.687002
575.676924	30.359983	72.692007
574.632841	24.844415	72.697012
573.481348	29.064978	72.702017
573.288642	21.546635	72.707022
572.841627	27.645150	72.712026
572.300857	27.119450	72.717031
571.888615	31.335803	72.722036
571.140374	27.367454	72.727041
570.380491	26.176472	72.732046
569.822546	28.148315	72.737050
568.791843	28.444999	72.742055
568.324952	23.176548	72.747060
567.450772	24.211565	72.752065
566.922700	19.347110	72.757070
565.705414	27.334556	72.762074
565.311656	24.635997	72.767079
565.170199	24.351051	72.772084
564.562613	22.896108	72.777089
563.591044	19.141539	72.782094
562.643357	22.572682	72.787098
562.216139	24.126300	72.792103
561.996587	21.997672	72.797108
561.281348	26.956169	72.802113
560.323597	17.165819	72.807118
559.119292	31.590070	72.812122
559.009592	23.462401	72.817127
557.922641	27.959702	72.822132
557.096535	21.915822	72.827137
556.806939	18.147240	72.832142
556.235451	22.759553	72.837146
555.747273	23.791435	72.842151
555.392620	23.209283	72.847156
554.436801	27.278832	72.852161
554.071336	23.880313	72.857166
553.207101	27.947889	72.862170
552.678400	23.499863	72.867175
551.473572	31.384405	72.872180
550.524796	29.778806	72.877185
550.428584	23.522460	72.882190
549.782410	18.694170	72.887194
549.080162	17.071380	72.892199
548.505921	25.902593	72.897204
547.433727	20.555525	72.902209
547.473166	19.361802	72.907214
546.485937	16.600087	72.912218
545.403031	23.170494	72.917223
545.042085	25.349086	72.922228
544.681973	19.453334	72.927233
543.656380	18.486043	72.932238
542.712778	32.039271	72.937242
542.161145	25.237293	72.942247
542.114800	22.092300	72.947252
541.431644	25.047638	72.952257
540.470240	16.667713	72.957262
539.438892	26.945307	72.962266
539.351880	21.627387	72.967271
538.796474	14.986868	72.972276
537.803093	31.550622	72.977281
537.363643	21.404894	72.982286
536.469492	34.417224	72.987290
535.671525	22.475639	72.992295
534.804647	22.050785	72.997300
533.842690	23.869370	73.002305
533.782132	18.110410	73.007310
533.226096	27.323512	73.012314
533.155099	17.563804	73.017319
531.972952	13.637786	73.022324
530.687687	21.046278	73.027329
530.869209	12.656178	73.032334
530.206952	18.091952	73.037338
529.267817	16.344475	73.042343
528.473850	22.558190	73.047348
527.741021	20.369405	73.052353
527.668181	17.742735	73.057358
526.395320	24.996286	73.062362
525.756976	15.908873	73.067367
525.402202	15.626374	73.072372
524.572860	9.827461	73.077377
524.257336	13.865977	73.082382
522.903477	23.133636	73.087386
522.536762	23.616304	73.092391
522.303916	20.053158	73.097396
521.348366	15.392438	73.102401
520.490921	10.720823	73.107406
519.725701	19.899436	73.112410
519.500921	13.411262	73.117415
519.051477	17.877978	73.122420
517.953089	18.508750	73.127425
517.614332	15.662663	73.132430
516.762764	27.510694	73.137434
515.856780	15.307205	73.142439
514.731915	9.030238	73.147444
513.931075	14.637906	73.152449
513.711895	12.064514	73.157454
513.047380	21.665491	73.162458
512.934796	18.583094	73.167463
512.839100	12.206823	73.172468
511.494759	20.846904	73.177473
510.953436	21.524552	73.182478
510.443274	22.053730	73.187482
509.601102	14.777645	73.192487
508.798555	21.159893	73.197492
508.228893	22.685748	73.202497
507.551242	17.553395	73.207502
506.276221	17.836989	73.212506
505.851616	19.409122	73.217511
505.414338	16.037824	73.222516
505.215254	28.855840	73.227521
504.371369	19.891067	73.232526
503.401665	25.101434	73.237530
502.469310	23.267729	73.242535
502.191716	19.446780	73.247540
501.574549	22.404230	73.252545
500.921113	14.068303	73.257550
500.315604	32.188266	73.262554
499.980866	24.556940	73.267559
498.809183	24.403016	73.272564
497.936638	25.488261	73.277569
497.517451	22.606103	73.282574
496.846803	32.329495	73.287578
496.374763	29.662343	73.292583
495.327336	22.078331	73.297588
494.469361	24.648360	73.302593
494.415472	20.577300	73.307598
493.943956	33.845588	73.312602
493.176914	29.290464	73.317607
492.366382	23.767690	73.322612
491.951694	28.954292	73.327617
490.667123	27.828005	73.332622
489.846254	28.084983	73.337626
489.444973	28.447004	73.342631
488.863994	29.287098	73.347636
488.190923	32.220343	73.352641
487.946516	23.975370	73.357646
486.763937	34.294427	73.362650
486.109985	33.659042	73.367655
485.650540	28.059831	73.372660
485.024578	31.455515	73.377665
484.286182	26.910025	73.382670
483.768940	30.267886	73.387674
483.241314	27.693174	73.392679
482.236240	18.618472	73.397684
481.109647	31.475452	73.402689
480.681972	26.055689	73.407694
480.223793	28.472137	73.412698
479.953973	20.989751	73.417703
479.615384	19.269616	73.422708
478.529759	33.851610	73.427713
477.571088	26.953648	73.432718
476.860630	32.758250	73.437722
476.339905	24.101553	73.442727
475.602997	28.514729	73.447732
474.611738	24.594595	73.452737
474.465989	13.621484	73.457742
473.863225	37.659469	73.462746
473.300204	16.962860	73.467751
472.296373	24.067911	73.472756
471.671932	31.442110	73.477761
471.368476	22.329741	73.482766
470.499316	32.788104	73.487770
469.949586	27.258477	73.492775
469.145614	23.767411	73.497780
468.518869	25.368604	73.502785
468.032528	24.708096	73.507790
466.757254	25.311880	73.512794
465.883012	28.037479	73.517799
465.566643	26.130874	73.522804
465.171647	25.744402	73.527809
464.972909	13.981777	73.532814
463.959090	25.171255	73.537818
462.932241	12.783619	73.542823
462.696892	22.453422	73.547828
461.750570	26.724921	73.552833
461.091725	18.208514	73.557838
460.064830	29.445813	73.562842
459.401908	26.499993	73.567847
459.495142	26.705953	73.572852
458.906084	23.885563	73.577857
458.168665	16.834088	73.582862
457.133708	24.226385	73.587866
456.284638	21.710783	73.592871
456.178867	20.139641	73.597876
455.099891	28.019937	73.602881
454.733168	23.836294	73.607886
453.839486	28.898944	73.612890
453.826223	27.051280	73.617895
452.782872	21.833708	73.622900
452.070281	29.825942	73.627905
451.326171	13.781947	73.632910
450.283156	29.746485	73.637914
449.639432	24.399003	73.642919
449.311781	16.742908	73.647924
448.341756	20.551397	73.652929
448.391823	16.209881	73.657934
447.436214	18.609396	73.662938
446.498297	17.733835	73.667943
446.034288	24.204086	73.672948
445.732902	19.472281	73.677953
445.146057	17.100987	73.682958
444.329358	22.592929	73.687962
443.371099	20.386474	73.692967
442.672520	16.506456	73.697972
441.670455	24.369769	73.702977
441.313352	18.661222	73.707982
440.357871	24.656263	73.712986
439.915608	18.633272	73.717991
439.879669	15.250079	73.722996
438.772425	20.356222	73.728001
438.067267	10.388490	73.733006
437.537254	22.838171	73.738010
436.881282	15.097198	73.743015
436.108991	18.979841	73.748020
434.949295	18.819307	73.753025
434.754015	17.358625	73.758030
434.281657	17.973260	73.763034
433.700681	16.067823	73.768039
432.794043	19.307962	73.773044
432.027275	13.618965	73.778049
431.989490	10.560928	73.783054
430.555082	18.855841	73.788058
429.613391	17.066232	73.793063
429.450068	17.942291	73.798068
428.773881	23.561662	73.803073
428.578875	22.318562	73.808078
427.155483	16.451915	73.813082
426.489765	15.509333	73.818087
426.191333	16.268146	73.823092
425.447151	16.019327	73.828097
425.118738	6.511976	73.833102
423.894999	23.697517	73.838106
423.523440	20.162795	73.843111
423.176945	14.544030	73.848116
422.448762	27.208225	73.853121
421.622732	11.770250	73.858126
420.711819	18.513570	73.863130
420.237804	17.999346	73.868135
420.101263	14.206398	73.873140
418.683138	24.007906	73.878145
418.445508	18.680882	73.883150
417.537634	25.182443	73.888154
416.995453	21.534559	73.893159
416.097469	21.111550	73.898164
415.160526	26.510696	73.903169
414.925581	13.411831	73.908174
414.517790	20.257912	73.913178
413.963841	15.276194	73.918183
412.996417	21.090214	73.923188
411.995962	17.559515	73.928193
411.985975	20.037019	73.933198
411.265681	28.263883	73.938202
410.398503	25.773261	73.943207
409.828551	16.599296	73.948212
409.089992	17.866651	73.953217
408.462911	15.441852	73.958222
407.298754	17.445674	73.963226
406.647615	14.359219	73.968231
406.244072	17.281070	73.973236
405.693957	21.390098	73.978241
405.375036	13.043478	73.983246
403.977514	24.650518	73.988250
403.702020	16.716456	73.993255
403.358524	22.098307	73.998260
402.713851	24.093466	74.003265
401.750687	13.055083	74.008270
400.866164	23.325089	74.013274
400.792357	22.885867	74.018279
399.848860	22.287186	74.023284
398.849071	21.606010	74.028289
398.561053	14.101311	74.033294
397.795265	21.449155	74.038298
397.330550	19.957295	74.043303
396.169979	9.246851	74.048308
395.368263	19.700784	74.053313
395.051206	15.370465	74.058318
394.765731	25.680630	74.063322
394.225051	12.471217	74.068327
393.049425	14.710267	74.073332
391.952740	23.569562	74.078337
392.134366	17.846138	74.083342
391.362693	25.504014	74.088346
390.561656	20.123273	74.093351
389.563523	23.841644	74.098356
388.839044	25.594052	74.103361
388.769501	21.178555	74.108366
387.953407	23.787677	74.113370
387.159703	23.411140	74.118375
386.876517	14.809664	74.123380
386.372482	24.694178	74.128385
385.288361	15.217375	74.133390
384.259720	20.675299	74.138394
384.021407	22.042717	74.143399
383.351151	14.684093	74.148404
382.374990	21.071963	74.153409
381.568363	17.436270	74.158414
381.065160	19.904064	74.163418
380.781087	20.707904	74.168423
380.264351	18.938902	74.173428
378.802561	15.719866	74.178433
378.167234	19.195913	74.183438
377.497898	22.240553	74.188442
377.061895	22.508775	74.193447
376.822572	22.334057	74.198452
376.398783	23.895042	74.203457
375.683801	18.787606	74.208462
374.977739	19.966211	74.213466
374.568288	23.319527	74.218471
373.213251	17.426251	74.223476
372.184523	23.770462	74.228481
372.307216	15.129536	74.233486
371.522088	17.363134	74.238490
370.499846	19.467360	74.243495
370.079550	20.715545	74.248500
369.489127	25.496494	74.253505
368.811446	17.743233	74.258510
367.623969	20.950879	74.263514
366.934911	34.160800	74.268519
366.790783	26.480200	74.273524
366.055798	24.540976	74.278529
365.868318	20.689916	74.283534
364.669560	28.038964	74.288538
364.454605	26.231331	74.293543
363.788007	15.951544	74.298548
362.467280	25.038949	74.303553
361.596061	24.192215	74.308558
361.357952	27.784738	74.313562
360.848262	24.729369	74.318567
360.657648	29.968586	74.323572
359.653779	24.151816	74.328577
358.948983	23.537186	74.333582
358.263731	23.006176	74.338586
357.543433	22.386132	74.343591
356.649782	19.082870	74.348596
355.309485	31.328959	74.353601
355.264206	22.959233	74.358606
354.560506	20.098795	74.363610
354.375246	24.660629	74.368615
354.106939	20.835068	74.373620
352.761228	17.819903	74.378625
352.515961	16.200036	74.383630
351.835486	16.519841	74.388634
350.633782	17.384777	74.393639
350.131672	23.317050	74.398644
349.415654	24.935653	74.403649
349.231398	14.998476	74.408654
348.449785	23.858034	74.413658
347.389626	13.786063	74.418663
346.953185	24.140789	74.423668
346.269016	19.586707	74.428673
346.047820	16.766068	74.433678
344.775389	23.440873	74.438682
344.198721	23.007681	74.443687
343.856333	18.277698	74.448692
342.914353	22.778784	74.453697
342.065533	14.778414	74.458702
341.399623	24.649308	74.463706
341.106608	21.191972	74.468711
340.763587	24.854834	74.473716
339.384259	17.312764	74.478721
338.983049	20.090746	74.483726
338.418427	19.378085	74.488730
337.806233	16.536185	74.493735
336.914350	15.077728	74.498740
335.860754	26.738796	74.503745
335.683638	14.669969	74.508750
335.253053	22.393343	74.513754
334.376608	21.069624	74.518759
333.675989	14.942755	74.523764
332.878850	14.065301	74.528769
332.600099	16.233971	74.533774
331.939881	20.642842	74.538778
330.888261	21.329322	74.543783
330.638861	16.136656	74.548788
329.850792	28.135459	74.553793
329.493983	19.955744	74.558798
328.023669	18.726683	74.563802
327.155653	13.979556	74.568807
326.970712	14.403316	74.573812
326.476891	19.656165	74.578817
326.380567	10.726869	74.583822
324.831045	26.910941	74.588826
324.060835	23.031338	74.593831
323.799835	18.119648	74.598836
323.369256	12.285642	74.603841
322.979870	12.678910	74.608846
321.776997	13.845251	74.613850
321.157572	19.599102	74.618855
320.894776	16.179532	74.623860
319.708811	25.765884	74.628865
319.405661	16.092095	74.633870
318.606905	19.646245	74.638874
317.888125	17.663452	74.643879
316.787310	21.322519	74.648884
316.082853	23.622125	74.653889
315.759296	20.147584	74.658894
315.036666	22.784409	74.663898
314.708800	18.422709	74.668903
314.410096	19.962189	74.673908
313.226106	29.114558	74.678913
312.846587	22.021858	74.683918
312.029637	16.101201	74.688922
310.598516	16.988531	74.693927
310.303207	25.764277	74.698932
309.625763	26.138805	74.703937
309.426639	16.554096	74.708942
308.986865	17.302335	74.713946
307.906850	17.378324	74.718951
307.170126	16.699411	74.723956
306.670742	18.124219	74.728961
306.238616	12.861334	74.733966
305.180795	15.822830	74.738970
304.469235	13.518763	74.743975
304.264387	12.617873	74.748980
303.500428	11.809259	74.753985
303.225979	4.458543	74.758990
301.989746	15.010138	74.763994
301.469700	19.947041	74.768999
300.893367	16.192667	74.774004
299.722891	18.028806	74.779009
299.264143	13.568122	74.784014
298.769365	13.621793	74.789018
298.203449	13.267325	74.794023
296.777629	10.052071	74.799028
296.166714	20.393607	74.804033
296.053075	13.622819	74.809038
295.590439	15.071733	74.814042
295.183512	14.341831	74.819047
294.308375	12.663097	74.824052
292.964729	14.832778	74.829057
292.953799	10.095705	74.834062
292.314462	15.923698	74.839066
291.249522	13.761122	74.844071
290.643649	7.844678	74.849076
289.596028	16.554255	74.854081
289.826954	12.590778	74.859086
289.317948	11.998577	74.864090
288.151322	13.097654	74.869095
287.671913	2.289738	74.874100
286.872995	2.661558	74.879105
286.032953	5.383337	74.884110
284.963233	11.775109	74.889114
284.444331	8.274943	74.894119
284.558579	7.988680	74.899124
283.573821	13.632033	74.904129
283.052311	12.239140	74.909134
281.903925	16.072964	74.914138
281.228440	7.511971	74.919143
281.268805	9.129870	74.924148
280.240668	12.536086	74.929153
279.618619	2.768068	74.934158
278.792306	5.156493	74.939162
278.355506	7.728838	74.944167
277.934764	6.991679	74.949172
276.710693	19.242919	74.954177
276.455284	7.235477	74.959182
275.467047	13.294136	74.964186
275.015540	10.349368	74.969191
274.062525	11.890650	74.974196
273.273664	16.925603	74.979201
272.918789	20.260769	74.984206
272.327833	23.393868	74.989210
271.803609	22.468197	74.994215
270.893949	17.694613	74.999220
269.776652	19.085463	75.004225
269.753947	21.684842	75.009230
269.069227	28.444195	75.014234
268.661366	21.214095	75.019239
267.418464	17.618029	75.024244
266.835487	26.004385	75.029249
266.607839	15.850207	75.034254
265.908011	14.619787	75.039258
265.092818	22.536946	75.044263
264.598603	16.361429	75.049268
263.583400	20.140914	75.054273
262.997990	16.785398	75.059278
262.358006	20.096628	75.064282
261.811042	21.543222	75.069287
261.211050	24.841771	75.074292
260.241543	21.230510	75.079297
259.668196	18.163238	75.084302
258.729913	17.324079	75.089306
258.430831	11.587400	75.094311
258.107552	20.261944	75.099316
257.193902	17.346695	75.104321
256.473690	12.462492	75.109326
255.608309	19.249067	75.114330
255.332383	26.029988	75.119335
254.507030	13.588268	75.124340
253.461178	27.454333	75.129345
253.179676	15.495205	75.134350
252.751667	20.322825	75.139354
252.021419	15.847085	75.144359
251.080588	9.059937	75.149364
250.113246	18.348100	75.154369
250.292841	17.275539	75.159374
249.084538	30.732257	75.164378
248.081990	23.546502	75.169383
247.438686	17.159785	75.174388
247.154790	24.298375	75.179393
246.937683	9.348480	75.184398
246.119165	18.767463	75.189402
244.830071	17.490639	75.194407
244.598742	15.442775	75.199412
243.954503	17.297550	75.204417
243.525325	14.670934	75.209422
242.430107	16.321633	75.214426
241.569781	18.056313	75.219431
241.443601	17.999192	75.224436
240.547071	27.011140	75.229441
239.629119	17.197258	75.234446
239.287593	14.036263	75.239450
238.394405	16.153083	75.244455
238.104377	13.452243	75.249460
237.577710	20.135938	75.254465
236.414199	20.895490	75.259470
235.889787	16.757532	75.264474
235.608639	19.150526	75.269479
235.293526	9.972266	75.274484
233.636941	22.464368	75.279489
232.884772	16.136015	75.284494
232.653742	21.700226	75.289498
232.116457	26.583120	75.294503
231.517507	17.377565	75.299508
230.554974	19.587448	75.304513
230.148672	13.262304	75.309518
229.674983	22.528545	75.314522
228.555943	17.185951	75.319527
228.016368	9.497462	75.324532
227.383651	18.112527	75.329537
227.056154	15.986955	75.334542
225.976088	20.216774	75.339546
224.918728	20.953100	75.344551
224.782651	14.285248	75.349556
224.203431	16.635875	75.354561
223.939382	12.312906	75.359566
222.866969	16.106257	75.364570
222.130120	11.372956	75.369575
221.553564	12.176134	75.374580
220.288576	17.982462	75.379585
220.016827	17.303563	75.384590
219.351962	15.365823	75.389594
219.039655	16.825477	75.394599
218.540257	21.848991	75.399604
217.409094	18.331333	75.404609
217.127847	8.573656	75.409614
216.297867	12.766759	75.414618
214.949425	11.013702	75.419623
214.575809	2.811471	75.424628
213.782220	14.913670	75.429633
213.601587	7.190037	75.434638
213.088688	17.254175	75.439642
212.001115	20.668318	75.444647
211.217476	15.245450	75.449652
210.289958	18.993628	75.454657
210.203813	10.220424	75.459662
209.836577	13.997546	75.464666
209.198154	10.995859	75.469671
208.543990	8.372005	75.474676
207.443011	15.472127	75.479681
207.333491	6.283174	75.484686
206.216179	16.520951	75.489690
205.295174	24.043402	75.494695
205.179480	18.651237	75.499700
204.386630	23.538610	75.504705
203.495474	9.949900	75.509710
202.664617	19.922807	75.514714
202.160255	21.438317	75.519719
201.948222	19.302223	75.524724
200.910134	28.190093	75.529729
200.067641	13.188526	75.534734
199.345719	16.299940	75.539738
198.977701	18.216344	75.544743
198.768430	14.375088	75.549748
197.573428	18.870831	75.554753
197.103862	15.263469	75.559758
196.035890	18.827461	75.564762
195.669975	24.985628	75.569767
195.531987	16.935064	75.574772
194.085911	21.333643	75.579777
193.567231	16.791074	75.584782
193.073560	21.310618	75.589786
192.598341	10.230817	75.594791
191.654058	11.772314	75.599796
190.923599	19.236000	75.604801
190.641682	8.108033	75.609806
189.875441	19.138260	75.614810
188.753629	16.642591	75.619815
188.395643	15.758244	75.624820
187.746659	24.587229	75.629825
187.294973	16.181399	75.634830
186.221420	11.020815	75.639834
185.493201	21.311683	75.644839
185.388671	10.768880	75.649844
184.880863	24.397781	75.654849
184.112110	12.103193	75.659854
183.352421	15.733154	75.664858
182.551302	16.662035	75.669863
181.572694	8.545235	75.674868
180.571349	15.120114	75.679873
180.097333	14.639054	75.684878
179.832092	7.930303	75.689882
179.310041	12.284058	75.694887
179.168377	13.536731	75.699892
177.838333	17.823775	75.704897
177.208597	8.684656	75.709902
176.664443	13.187019	75.714906
175.454224	17.560615	75.719911
174.965301	17.457257	75.724916
174.050310	13.099313	75.729921
173.901781	1.289330	75.734926
173.408613	17.508455	75.739930
172.683980	7.644863	75.744935
171.821487	13.950018	75.749940
171.095171	26.416830	75.754945
170.723505	15.446679	75.759950
170.341336	14.214523	75.764954
168.933954	13.511701	75.769959
168.529727	2.472633	75.774964
167.690194	22.208476	75.779969
167.598463	14.530596	75.784974
166.804730	17.998830	75.789978
165.854972	13.283727	75.794983
165.502628	12.589299	75.799988
164.620622	21.352939	75.804993
164.030396	12.973938	75.809998
163.215377	12.902078	75.815002
162.474659	26.257454	75.820007
162.432163	11.927877	75.825012
161.195491	18.281663	75.830017
160.814340	10.607356	75.835022
160.187446	7.165444	75.840026
159.475229	15.655997	75.845031
158.383591	6.115868	75.850036
157.498551	15.840373	75.855041
157.253837	6.507402	75.860046
156.697003	10.579695	75.865050
156.193326	21.815649	75.870055
155.350026	14.021066	75.875060
154.587125	12.879587	75.880065
154.280243	13.754898	75.885070
153.700386	16.908328	75.890074
152.797183	17.142276	75.895079
152.150127	9.720112	75.900084
151.326582	26.379867	75.905089
150.927994	16.759184	75.910094
149.907325	27.017847	75.915098
149.051294	22.514889	75.920103
148.767482	19.333666	75.925108
147.937102	22.913409	75.930113
147.899186	17.709126	75.935118
146.638477	27.334271	75.940122
146.056111	20.751785	75.945127
145.750844	13.033840	75.950132
144.898325	15.601533	75.955137
144.115165	13.132311	75.960142
143.426306	13.532360	75.965146
142.678968	13.613720	75.970151
142.587787	17.480874	75.975156
141.377658	17.238632	75.980161
140.821654	13.977812	75.985166
140.097776	15.588263	75.990170
139.682843	20.902677	75.995175
139.066150	16.975007	76.000180
138.423528	18.990402	76.005185
137.902870	19.004077	76.010190
136.618823	22.138916	76.015194
135.786999	18.138317	76.020199
135.258200	14.447373	76.025204
134.681218	14.602497	76.030209
134.497980	14.696410	76.035214
134.029003	19.174177	76.040218
132.849775	29.038653	76.045223
132.384506	16.793463	76.050228
131.921280	21.215120	76.055233
131.078335	26.698718	76.060238
130.175509	22.884488	76.065242
129.376158	19.142069	76.070247
129.126454	14.979257	76.075252
128.356595	20.899063	76.080257
127.524002	18.141255	76.085262
126.780143	6.910348	76.090266
126.147429	12.527577	76.095271
125.876740	12.999720	76.100276
125.115163	15.045127	76.105281
124.238942	6.793754	76.110286
123.609413	17.482063	76.115290
123.023232	21.770361	76.120295
122.869752	10.142523	76.125300
121.267051	22.099380	76.130305
120.766430	15.317784	76.135310
120.457223	12.422897	76.140314
119.906742	15.741963	76.145319
118.848460	12.953918	76.150324
118.309815	18.108285	76.155329
117.640256	15.397024	76.160334
116.837047	16.376722	76.165338
116.522877	6.196956	76.170343
116.036470	12.481574	76.175348
114.782570	22.116682	76.180353
114.469186	18.162727	76.185358
114.085374	13.486705	76.190362
112.923505	17.068857	76.195367
112.401414	5.821514	76.200372
111.757398	12.610672	76.205377
111.258427	14.495929	76.210382
110.633692	15.541787	76.215386
109.224194	12.812911	76.220391
109.201584	17.774595	76.225396
108.467633	17.617283	76.230401
108.229838	13.991904	76.235406
106.953822	14.026698	76.240410
106.380046	16.917388	76.245415
105.681731	12.179559	76.250420
104.870624	14.120905	76.255425
104.674578	13.925120	76.260430
103.906821	15.635621	76.265434
103.087623	29.853521	76.270439
102.693103	26.634765	76.275444
102.011840	22.018797	76.280449
101.395757	17.428706	76.285454
100.697082	20.683099	76.290458
99.895929	19.935676	76.295463
99.405635	5.037276	76.300468
98.478354	20.078244	76.305473
97.847416	13.325323	76.310478
97.449457	7.932457	76.315482
96.485319	19.573016	76.320487
95.660015	12.242378	76.325492
94.699391	16.109417	76.330497
94.308231	16.479348	76.335502
93.957956	20.342090	76.340506
93.618927	12.104406	76.345511
93.184571	14.961824	76.350516
91.915810	35.086276	76.355521
91.795613	20.002680	76.360526
90.924560	21.535690	76.365530
89.708104	16.765380	76.370535
89.539159	5.171559	76.375540
88.776493	23.991542	76.380545
87.898124	18.120195	76.385550
87.140248	13.645765	76.390554
86.270883	16.370709	76.395559
86.173391	17.510684	76.400564
85.669493	14.659468	76.405569
85.003116	14.779975	76.410574
84.239875	18.459417	76.415578
83.525247	28.735525	76.420583
82.753488	12.000669	76.425588
81.846446	11.363182	76.430593
81.372258	20.309388	76.435598
80.875795	19.798811	76.440602
79.837680	20.251425	76.445607
79.015097	23.768443	76.450612
78.322943	21.021371	76.455617
77.989088	22.287355	76.460622
77.373565	19.483907	76.465626
77.014375	24.574968	76.470631
76.631800	18.189303	76.475636
75.428725	27.906213	76.480641
74.918407	21.263371	76.485646
74.511531	17.139826	76.490650
73.195457	20.333421	76.495655
72.705660	12.238061	76.500660
71.983577	15.384228	76.505665
71.887851	10.160788	76.510670
70.840989	14.095207	76.515674
69.925560	20.113939	76.520679
69.575869	14.546219	76.525684
68.965629	18.609702	76.530689
68.110007	24.142648	76.535694
66.938338	19.718452	76.540698
66.519565	17.610617	76.545703
66.237070	16.402006	76.550708
65.505730	27.455081	76.555713
65.288975	14.284012	76.560718
64.447406	15.842291	76.565722
63.559870	24.102205	76.570727
63.518163	14.806257	76.575732
61.897931	21.058833	76.580737
61.205359	10.437949	76.585742
60.867020	13.626994	76.590746
60.310641	16.374567	76.595751
60.307721	21.137564	76.600756
58.941180	15.837688	76.605761
58.491639	11.012887	76.610766
57.680086	26.402849	76.615770
56.845448	31.107691	76.620775
56.215232	11.215224	76.625780
55.126841	25.182745	76.630785
55.201904	11.768012	76.635790
54.759863	16.582123	76.640794
53.706429	19.566676	76.645799
52.820118	28.545505	76.650804
52.009568	21.483769	76.655809
51.857451	19.027470	76.660814
51.092478	19.444415	76.665818
49.891693	26.035384	76.670823
49.730469	15.164167	76.675828
48.886363	19.477849	76.680833
48.668855	21.067485	76.685838
47.828972	26.399228	76.690842
47.336784	25.771279	76.695847
46.886111	25.188749	76.700852
45.375247	25.246841	76.705857
44.563030	24.483854	76.710862
43.970143	18.469216	76.715866
43.436556	23.815184	76.720871
43.603992	28.410658	76.725876
42.945409	28.145149	76.730881
41.891931	30.101520	76.735886
41.296467	26.776053	76.740890
40.390415	26.294545	76.745895
39.623419	20.001744	76.750900
38.814661	32.560582	76.755905
38.303966	20.530827	76.760910
37.836361	22.199780	76.765914
37.190800	24.461680	76.770919
37.165113	22.994485	76.775924
36.108301	27.603881	76.780929
35.380091	21.817415	76.785934
34.235576	16.174627	76.790938
33.358207	20.436848	76.795943
33.233627	13.311438	76.800948
32.393267	26.916123	76.805953
32.217085	22.699016	76.810958
31.318862	22.788709	76.815962
30.189790	24.651485	76.820967
29.882199	23.327030	76.825972
29.219576	30.518156	76.830977
28.839900	21.181498	76.835982
27.838255	27.450547	76.840986
27.277683	29.353533	76.845991
27.044171	20.692166	76.850996
25.322143	27.591798	76.856001
25.026522	26.658104	76.861006
24.458240	25.450928	76.866010
23.922720	31.374386	76.871015
23.771867	18.413589	76.876020
22.655172	22.597292	76.881025
22.028464	18.614482	76.886030
21.746710	22.595615	76.891034
20.924422	18.796970	76.896039
19.780923	9.332998	76.901044
19.032535	16.979356	76.906049
18.658626	19.926493	76.911054
17.946937	8.996435	76.916058
16.649642	19.122636	76.921063
16.400421	13.313393	76.926068
15.709508	21.515145	76.931073
15.300957	16.500885	76.936078
14.987862	21.098887	76.941082
14.222765	17.084537	76.946087
13.265588	5.499769	76.951092
12.325857	16.849444	76.956097
12.056426	14.526983	76.961102
12.062155	17.292135	76.966106
10.746446	17.153535	76.971111
9.984852	7.868350	76.976116
8.975682	14.647966	76.981121
8.796986	9.351034	76.986126
8.334908	13.906566	76.991130
7.032758	20.423832	76.996135
7.019192	14.173290	77.001140
6.255574	25.261486	77.006145
5.878184	16.261947	77.011150
4.700415	15.733910	77.016155
4.146912	13.240718	77.021159
3.841701	9.633993	77.026164