Fri Mar 05 18:18:59 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.269336	93.530749	0.000000
0.205876	78.031268	0.005005
-0.426853	53.914498	0.010010
-2.252724	1.548831	0.015014
-6.393627	-14.025573	0.020019
-11.892720	-6.100832	0.025024
-16.474775	-12.877855	0.030029
-21.369057	-8.993589	0.035034
-25.385515	-9.901421	0.040038
-29.089682	-1.441358	0.045043
-32.809766	0.451565	0.050048
-36.014765	-4.476097	0.055053
-39.780242	-6.296011	0.060058
-43.264941	-0.413023	0.065062
-47.185503	-6.243670	0.070067
-51.228884	-4.660273	0.075072
-54.910749	-3.011538	0.080077
-58.730898	7.272714	0.085082
-62.537847	-9.679526	0.090086
-66.326734	1.664204	0.095091
-70.042059	2.842054	0.100096
-73.750320	-8.996005	0.105101
-77.548335	6.793121	0.110106
-81.048212	-13.403029	0.115110
-85.107845	6.950611	0.120115
-88.809515	-6.840774	0.125120
-92.393989	4.175489	0.130125
-96.379535	-0.892491	0.135130
-99.880083	0.404103	0.140134
-103.423556	3.997322	0.145139
-107.497427	3.794231	0.150144
-111.406391	-4.432009	0.155149
-115.557542	-1.831508	0.160154
-118.730882	-2.414809	0.165158
-122.367354	-12.491717	0.170163
-126.241705	1.463014	0.175168
-130.139435	-19.257776	0.180173
-134.278485	4.103276	0.185178
-137.833436	-19.143316	0.190182
-141.533874	-0.539011	0.195187
-145.718399	-5.119409	0.200192
-149.292860	4.122813	0.205197
-153.377430	-2.403741	0.210202
-156.561744	-7.184724	0.215206
-160.285841	2.447248	0.220211
-163.996521	-10.555658	0.225216
-167.681682	-1.682107	0.230221
-171.443914	-2.811617	0.235226
-175.038578	1.113152	0.240230
-179.342623	1.768518	0.245235
-183.204754	3.398904	0.250240
-186.616068	-5.076936	0.255245
-190.737681	0.663465	0.260250
-193.801598	8.258341	0.265254
-198.046091	8.311294	0.270259
-201.714950	7.458669	0.275264
-205.412893	4.010260	0.280269
-209.596782	5.195291	0.285274
-212.913945	0.462393	0.290278
-216.845701	14.199344	0.295283
-220.328429	-1.798262	0.300288
-223.855673	-3.178084	0.305293
-228.044882	6.946118	0.310298
-231.335629	-2.625973	0.315302
-235.835153	1.342375	0.320307
-239.471562	-0.294395	0.325312
-243.037375	-4.052417	0.330317
-247.086570	9.148223	0.335322
-250.537046	3.372197	0.340326
-254.174951	-2.779187	0.345331
-257.995204	6.418839	0.350336
-262.019641	-12.280313	0.355341
-265.952315	6.271346	0.360346
-269.301562	-8.061693	0.365350
-273.326964	3.544020	0.370355
-276.917196	2.450299	0.375360
-280.333242	-1.370997	0.380365
-284.447962	8.165812	0.385370
-288.084883	-4.225759	0.390374
-292.035589	-0.281835	0.395379
-296.055260	11.069111	0.400384
-299.543143	-7.510619	0.405389
-303.315838	5.469345	0.410394
-307.181180	-3.517316	0.415398
-310.954037	0.186933	0.420403
-314.932402	5.213959	0.425408
-317.992952	-2.740507	0.430413
-322.352981	3.572767	0.435418
-325.753627	-2.116480	0.440422
-329.261300	0.629242	0.445427
-333.120966	-1.041130	0.450432
-337.104258	0.149945	0.455437
-340.943751	-4.663385	0.460442
-344.919167	2.181466	0.465446
-348.599088	-6.539832	0.470451
-352.310057	-0.058891	0.475456
-356.061682	-8.120592	0.480461
-359.877804	2.942480	0.485466
-363.272324	-6.876199	0.490470
-367.163151	-2.900715	0.495475
-370.980139	-2.344847	0.500480
-374.435936	-0.097780	0.505485
-378.782002	5.093713	0.510490
-381.997283	-11.029899	0.515494
-386.083877	0.032239	0.520499
-390.037371	1.548230	0.525504
-393.789449	-10.356413	0.530509
-397.387907	-1.426990	0.535514
-401.365332	6.104255	0.540518
-404.946831	-6.658673	0.545523
-408.430910	0.418487	0.550528
-412.180211	-5.060416	0.555533
-416.079414	-3.437933	0.560538
-419.740344	-2.258772	0.565542
-423.662149	-1.722354	0.570547
-427.563672	5.159716	0.575552
-430.940925	-10.966343	0.580557
-435.023739	1.576045	0.585562
-438.482235	-9.230524	0.590566
-442.470852	-2.547417	0.595571
-446.342162	-7.396492	0.600576
-450.063894	-2.594739	0.605581
-454.062365	-2.586928	0.610586
-457.270517	-5.822991	0.615590
-461.286722	0.481349	0.620595
-464.995474	2.240656	0.625600
-468.688830	1.731404	0.630605
-472.885725	-4.147433	0.635610
-476.558173	-0.343846	0.640614
-480.210653	-2.050220	0.645619
-483.917358	-0.128783	0.650624
-487.218857	0.247170	0.655629
-491.502654	1.536956	0.660634
-495.720821	-2.972787	0.665638
-498.993630	-0.133443	0.670643
-502.700777	3.257829	0.675648
-506.035696	-0.331663	0.680653
-510.199795	13.507488	0.685658
-513.553043	-3.814471	0.690662
-517.846251	-5.404257	0.695667
-521.644691	-0.542834	0.700672
-525.088036	4.787010	0.705677
-528.999106	1.179188	0.710682
-532.560073	-1.790681	0.715686
-536.488343	-4.809108	0.720691
-540.198913	5.370039	0.725696
-544.077611	1.320252	0.730701
-548.073993	0.030041	0.735706
-551.449922	0.110463	0.740710
-555.448109	-7.935176	0.745715
-559.441705	6.737835	0.750720
-562.774848	-1.048172	0.755725
-566.757234	9.262747	0.760730
-570.416016	3.698676	0.765734
-574.172639	4.016564	0.770739
-577.905863	8.358298	0.775744
-581.592884	-0.632725	0.780749
-585.212738	3.015965	0.785754
-589.263802	6.624737	0.790758
-592.727393	1.089446	0.795763
-596.535606	-0.531943	0.800768
-600.625330	-0.463577	0.805773
-604.485584	0.957445	0.810778
-608.043318	-1.350498	0.815782
-611.736531	-2.129211	0.820787
-615.318371	0.452151	0.825792
-619.148068	4.128110	0.830797
-623.323366	-1.400663	0.835802
-627.100602	-1.941998	0.840806
-630.562889	1.889745	0.845811
-634.583122	2.659856	0.850816
-638.146102	-0.284298	0.855821
-641.679320	4.626401	0.860826
-645.326737	-7.617815	0.865830
-649.331925	5.426602	0.870835
-653.105074	1.057355	0.875840
-656.740636	-1.654398	0.880845
-660.717512	5.855093	0.885850
-664.682311	-1.069737	0.890854
-668.253735	3.884952	0.895859
-672.198281	-1.459826	0.900864
-675.805022	-5.294223	0.905869
-679.477521	5.951381	0.910874
-682.827570	-5.957087	0.915878
-686.803681	7.730876	0.920883
-690.728565	0.449626	0.925888
-694.049053	-6.710572	0.930893
-698.332436	-0.732164	0.935898
-702.140186	-4.534399	0.940902
-705.852830	-0.077488	0.945907
-709.888024	3.551026	0.950912
-713.427259	-5.258386	0.955917
-717.195138	-1.306723	0.960922
-720.590561	-0.675738	0.965926
-724.469624	2.699190	0.970931
-728.504197	3.802915	0.975936
-732.043857	-1.141260	0.980941
-735.919895	0.621545	0.985946
-739.947245	-0.092529	0.990950
-743.544114	3.585840	0.995955
-747.307248	7.801724	1.000960
-750.804798	6.083626	1.005965
-754.987590	12.154871	1.010970
-758.172700	-1.344194	1.015974
-762.127943	2.601215	1.020979
-765.944369	3.726909	1.025984
-769.495902	2.365976	1.030989
-773.729416	6.459960	1.035994
-777.081768	1.717731	1.040998
-780.895813	7.260146	1.046003
-785.102217	3.960160	1.051008
-788.697625	7.313509	1.056013
-792.467784	4.524132	1.061018
-796.059947	3.270660	1.066022
-800.067071	10.297929	1.071027
-803.798243	7.806692	1.076032
-807.216560	6.074437	1.081037
-810.970524	11.448024	1.086042
-814.725836	5.538651	1.091046
-818.594406	-0.284800	1.096051
-822.732324	9.765951	1.101056
-825.923471	1.804673	1.106061
-829.781436	6.168308	1.111066
-833.652505	4.811243	1.116070
-837.925177	2.737786	1.121075
-841.330571	7.308216	1.126080
-844.947176	-0.228627	1.131085
-848.883643	1.332708	1.136090
-852.182995	-9.665805	1.141094
-856.214525	-1.041816	1.146099
-860.300640	2.210311	1.151104
-863.611711	0.830004	1.156109
-867.519590	11.419646	1.161114
-871.291225	10.658608	1.166118
-874.939168	1.614515	1.171123
-878.713911	-2.689448	1.176128
-882.344451	1.439214	1.181133
-886.960992	5.585170	1.186138
-890.144763	-2.574312	1.191142
-894.150392	-1.993754	1.196147
-897.631309	4.039634	1.201152
-901.483041	3.416032	1.206157
-905.380730	6.422067	1.211162
-908.929597	-0.549911	1.216166
-912.347980	2.018376	1.221171
-916.283510	4.036992	1.226176
-920.145546	6.387641	1.231181
-924.472874	0.776495	1.236186
-927.651568	1.029347	1.241190
-931.307059	2.156383	1.246195
-935.582456	9.094303	1.251200
-939.223787	8.708357	1.256205
-942.775528	12.401886	1.261210
-946.533430	7.633289	1.266214
-949.972083	3.217354	1.271219
-953.836673	4.836756	1.276224
-957.577415	3.957378	1.281229
-961.830932	3.557396	1.286234
-965.096976	4.035579	1.291238
-968.714892	0.056772	1.296243
-972.984217	-0.332776	1.301248
-976.644405	-1.166658	1.306253
-980.573751	1.797252	1.311258
-984.051867	-2.688013	1.316262
-987.999610	3.998902	1.321267
-991.870200	-3.159614	1.326272
-995.493311	-6.700727	1.331277
-999.630335	6.876254	1.336282
-1003.128849	9.585220	1.341286
-1006.619358	2.758606	1.346291
-1010.391296	8.608461	1.351296
-1013.836043	-2.360249	1.356301
-1017.968161	3.447872	1.361306
-1021.614158	7.535061	1.366310
-1025.486294	-4.319336	1.371315
-1029.470353	1.771054	1.376320
-1032.899512	4.688169	1.381325
-1037.040409	6.361361	1.386330
-1040.504801	-3.140745	1.391334
-1044.273975	8.593935	1.396339
-1048.055077	9.187729	1.401344
-1051.564841	2.780583	1.406349
-1055.708307	12.928803	1.411354
-1059.575885	-7.944894	1.416358
-1063.514130	-2.352212	1.421363
-1067.037886	3.289298	1.426368
-1070.530544	4.797360	1.431373
-1074.494907	7.634562	1.436378
-1078.200687	4.373307	1.441382
-1081.612834	-3.057081	1.446387
-1085.457147	-2.924625	1.451392
-1089.487665	7.841096	1.456397
-1093.557055	10.393932	1.461402
-1097.437920	2.817769	1.466406
-1100.747022	8.896503	1.471411
-1104.545108	-0.189422	1.476416
-1107.732433	-7.047026	1.481421
-1112.017203	4.599920	1.486426
-1115.834072	3.680934	1.491430
-1119.908654	0.683752	1.496435
-1123.570506	0.140528	1.501440
-1126.957857	-5.103360	1.506445
-1130.886762	-5.640119	1.511450
-1134.415824	3.503183	1.516454
-1138.468637	0.221852	1.521459
-1142.040029	8.985586	1.526464
-1145.869865	4.604147	1.531469
-1150.106338	6.160365	1.536474
-1153.488988	0.974110	1.541478
-1157.127837	-3.614483	1.546483
-1160.801789	1.111326	1.551488
-1164.521203	1.496743	1.556493
-1168.466538	-5.419269	1.561498
-1172.347318	-6.012542	1.566502
-1176.046560	1.005500	1.571507
-1179.589875	-1.836880	1.576512
-1183.388568	-11.346765	1.581517
-1187.425286	7.358502	1.586522
-1190.844859	-0.302342	1.591526
-1194.601011	-10.178561	1.596531
-1198.722454	-1.954368	1.601536
-1202.084548	-5.768730	1.606541
-1205.945820	-7.475246	1.611546
-1209.951703	-1.403145	1.616550
-1213.851615	-13.889842	1.621555
-1217.484012	-7.309791	1.626560
-1220.899025	-5.988973	1.631565
-1225.008881	4.300803	1.636570
-1228.531998	-5.082794	1.641574
-1232.455733	-7.503092	1.646579
-1236.315785	1.335351	1.651584
-1239.792969	-11.166909	1.656589
-1244.063512	-0.941277	1.661594
-1247.251296	0.614453	1.666598
-1250.861862	-0.001431	1.671603
-1254.947093	1.325768	1.676608
-1258.906095	-0.201016	1.681613
-1262.810422	-1.280803	1.686618
-1266.052106	-1.668692	1.691622
-1270.121492	-2.837169	1.696627
-1273.733040	-5.871909	1.701632
-1277.461420	-5.246756	1.706637
-1281.263537	5.850149	1.711642
-1284.932571	-2.466059	1.716646
-1288.866428	0.863360	1.721651
-1292.996408	0.975648	1.726656
-1296.365622	-0.501965	1.731661
-1300.250951	-1.747155	1.736666
-1303.817575	-5.580668	1.741670
-1307.143912	-0.733655	1.746675
-1311.255746	4.545020	1.751680
-1315.024636	-0.192814	1.756685
-1319.022579	-3.405333	1.761690
-1322.660921	-2.826059	1.766694
-1326.383448	0.874874	1.771699
-1330.179865	0.661024	1.776704
-1333.876307	-7.956642	1.781709
-1337.756187	-2.286121	1.786714
-1341.683874	-5.829967	1.791718
-1345.168675	1.243894	1.796723
-1349.188478	-1.603951	1.801728
-1352.347947	-5.988264	1.806733
-1356.954762	-3.207020	1.811738
-1360.455140	1.238997	1.816742
-1363.840102	-2.972009	1.821747
-1367.708289	1.020388	1.826752
-1371.275783	0.154947	1.831757
-1375.403237	2.939914	1.836762
-1379.103780	-4.790772	1.841766
-1383.362841	1.216493	1.846771
-1386.916005	3.725040	1.851776
-1390.169753	-0.447009	1.856781
-1393.996328	7.637273	1.861786
-1397.473012	-7.619748	1.866790
-1401.796751	-11.325586	1.871795
-1405.361050	6.394481	1.876800
-1409.065116	1.666927	1.881805
-1413.011299	1.421997	1.886810
-1416.753741	-10.733151	1.891814
-1420.430789	-2.185494	1.896819
-1424.174345	4.767483	1.901824
-1427.825806	-1.938075	1.906829
-1431.801131	9.904308	1.911834
-1435.471015	-5.167178	1.916838
-1439.428675	-0.199974	1.921843
-1443.489002	-3.012777	1.926848
-1446.815011	-0.439586	1.931853
-1450.546169	8.435330	1.936858
-1454.233119	4.186080	1.941862
-1458.035619	9.227822	1.946867
-1461.770769	2.690259	1.951872
-1465.425922	-2.876086	1.956877
-1469.656436	6.979258	1.961882
-1472.929062	7.795098	1.966886
-1476.831454	1.560309	1.971891
-1480.980636	13.200377	1.976896
-1484.079250	-0.325628	1.981901
-1488.163066	-5.630903	1.986906
-1491.608570	-1.983533	1.991910
-1495.342559	0.984642	1.996915
-1499.688601	4.863673	2.006912
-1500.723191	1.817859	2.016909
-1498.068993	-0.168651	2.026906
-1495.134942	-1.044167	2.036902
-1492.745477	-2.369320	2.046899
-1491.174399	-0.961275	2.056896
-1489.444771	0.874547	2.066893
-1487.701881	0.974536	2.076890
-1485.557633	-2.371900	2.086886
-1483.287414	-5.972192	2.096883
-1481.626969	-5.423200	2.106880
-1479.959383	2.662656	2.116877
-1477.880896	8.757953	2.126874
-1475.938623	3.849106	2.136870
-1473.883158	2.170080	2.146867
-1472.252250	1.237997	2.156864
-1470.312258	6.024405	2.166861
-1468.229564	4.764188	2.176858
-1466.529036	-0.143836	2.186854
-1464.588557	2.815628	2.196851
-1462.740709	5.673084	2.206848
-1460.919424	1.172049	2.216845
-1458.742575	-2.012212	2.226842
-1456.987861	-0.859340	2.236838
-1455.220363	-4.377530	2.246835
-1453.145045	-12.411914	2.256832
-1451.503612	-4.449748	2.266829
-1449.509877	-3.635147	2.276826
-1447.771448	-3.272303	2.286822
-1445.896366	-2.206592	2.296819
-1443.632319	-1.485793	2.306816
-1442.090146	3.097490	2.316813
-1440.223222	-2.898227	2.326810
-1438.166066	-5.038552	2.336806
-1436.207353	-10.717375	2.346803
-1434.391274	-9.196938	2.356800
-1432.695238	-2.944049	2.366797
-1430.508703	-4.182963	2.376794
-1428.833675	-2.682569	2.386790
-1426.853242	1.720028	2.396787
-1424.917722	2.117650	2.406784
-1423.440790	0.798142	2.416781
-1421.563136	7.067755	2.426778
-1419.384600	-0.091014	2.436774
-1417.313553	5.343943	2.446771
-1415.754125	-2.285710	2.456768
-1413.702440	3.243930	2.466765
-1412.070343	7.797050	2.476762
-1410.061712	7.761393	2.486758
-1407.951715	2.080472	2.496755
-1406.361464	-0.741401	2.506752
-1404.420555	-3.147301	2.516749
-1402.614341	1.788481	2.526746
-1400.776766	9.360867	2.536742
-1398.604563	6.224773	2.546739
-1396.611671	-2.642704	2.556736
-1394.943354	6.038379	2.566733
-1393.025926	4.026253	2.576730
-1391.292353	0.696700	2.586726
-1389.208516	-2.769454	2.596723
-1387.320721	-0.092019	2.606720
-1385.417453	1.187129	2.616717
-1383.914370	1.282956	2.626714
-1381.963949	-2.788685	2.636710
-1379.755960	-0.975674	2.646707
-1378.100349	4.066345	2.656704
-1376.230697	3.920333	2.666701
-1374.619993	7.385835	2.676698
-1372.455480	-0.534871	2.686694
-1370.478044	-3.702918	2.696691
-1368.518991	-2.202157	2.706688
-1366.629251	-2.005582	2.716685
-1365.028704	-1.303230	2.726682
-1363.113394	-5.535027	2.736678
-1361.200887	0.637478	2.746675
-1359.212554	2.008822	2.756672
-1357.224242	3.460699	2.766669
-1355.589596	5.253407	2.776666
-1353.858425	-0.998415	2.786662
-1351.957871	1.485953	2.796659
-1349.902771	4.629278	2.806656
-1348.089306	-2.688888	2.816653
-1346.154120	6.150046	2.826650
-1344.150313	0.329860	2.836646
-1342.275453	4.056264	2.846643
-1340.542820	1.977444	2.856640
-1338.729598	0.119414	2.866637
-1336.713450	3.906892	2.876634
-1334.812156	-1.678979	2.886630
-1333.007902	-2.054492	2.896627
-1331.172880	-3.759687	2.906624
-1329.213480	-1.864203	2.916621
-1327.229317	-3.200103	2.926618
-1325.310237	1.171352	2.936614
-1323.558499	2.294804	2.946611
-1321.818278	-6.003214	2.956608
-1320.090284	1.814151	2.966605
-1317.884158	1.964862	2.976602
-1316.046255	1.116600	2.986598
-1314.110143	1.954754	2.996595
-1312.732071	-1.741007	3.006592
-1310.407196	-1.514558	3.016589
-1308.505380	-1.179339	3.026586
-1306.660709	0.156623	3.036582
-1304.804756	-2.106122	3.046579
-1302.990472	-2.355320	3.056576
-1301.212493	-2.603443	3.066573
-1299.182034	-1.249842	3.076570
-1297.148061	-0.277334	3.086566
-1295.706416	-3.376934	3.096563
-1293.567519	-2.261739	3.106560
-1291.678616	-0.331256	3.116557
-1289.744808	-1.558010	3.126554
-1288.016441	2.686104	3.136550
-1285.782205	-0.987193	3.146547
-1283.856353	0.190530	3.156544
-1282.505764	-1.744996	3.166541
-1280.517879	-3.946730	3.176538
-1278.761297	-4.335098	3.186534
-1276.588133	-0.874280	3.196531
-1274.641427	1.951720	3.206528
-1273.297261	-3.562308	3.216525
-1271.112625	-3.883384	3.226522
-1269.020923	0.844185	3.236518
-1267.299618	-2.139100	3.246515
-1265.424340	7.566881	3.256512
-1263.604678	2.466241	3.266509
-1261.623040	-2.060308	3.276506
-1259.612974	6.675143	3.286502
-1257.885364	-0.774487	3.296499
-1255.779506	-1.256629	3.306496
-1254.336863	0.956886	3.316493
-1252.649249	2.818562	3.326490
-1250.422300	6.229747	3.336486
-1248.313316	4.869201	3.346483
-1246.629314	1.310837	3.356480
-1244.754113	3.027233	3.366477
-1242.999393	3.758684	3.376474
-1241.065721	-1.038072	3.386470
-1239.335728	7.862221	3.396467
-1237.038595	8.093184	3.406464
-1235.199816	-0.882143	3.416461
-1233.555604	7.152393	3.426458
-1231.757111	9.110028	3.436454
-1229.926752	-0.456064	3.446451
-1228.129955	0.478668	3.456448
-1225.857137	-1.312293	3.466445
-1224.028917	-0.166266	3.476442
-1222.262256	3.713346	3.486438
-1220.186800	1.221328	3.496435
-1218.872248	4.723281	3.506432
-1216.502880	2.558451	3.516429
-1214.909134	6.631532	3.526426
-1212.979194	8.132351	3.536422
-1210.657867	1.801980	3.546419
-1209.127673	4.345732	3.556416
-1207.197467	3.127516	3.566413
-1205.346482	4.462551	3.576410
-1203.825262	-1.337146	3.586406
-1201.807908	0.187589	3.596403
-1199.393916	0.673054	3.606400
-1197.625852	0.494492	3.616397
-1196.089991	-0.415874	3.626394
-1194.338635	5.201504	3.636390
-1192.125766	-1.567818	3.646387
-1190.272600	-1.982626	3.656384
-1188.562885	-0.490762	3.666381
-1186.602903	1.396858	3.676378
-1184.484391	-5.459992	3.686374
-1182.938021	1.210211	3.696371
-1181.283326	4.177754	3.706368
-1179.059326	-3.198085	3.716365
-1177.137977	1.119453	3.726362
-1175.133714	3.525797	3.736358
-1173.460179	8.713531	3.746355
-1171.757029	2.125256	3.756352
-1169.621071	1.044680	3.766349
-1167.800515	-7.019769	3.776346
-1166.270006	0.721950	3.786342
-1164.144118	2.791470	3.796339
-1162.010334	1.524930	3.806336
-1160.144604	1.103398	3.816333
-1158.524452	4.198066	3.826330
-1156.518995	2.786269	3.836326
-1154.732285	-5.151176	3.846323
-1152.956930	7.826745	3.856320
-1151.306625	3.337503	3.866317
-1149.038001	-2.278574	3.876314
-1147.044255	0.806858	3.886310
-1145.289597	2.439989	3.896307
-1143.728864	0.314602	3.906304
-1141.301863	-1.328837	3.916301
-1139.489292	3.312459	3.926298
-1137.917330	-4.696410	3.936294
-1135.859387	-3.077056	3.946291
-1134.172485	-7.565822	3.956288
-1131.943523	-7.748594	3.966285
-1130.364193	-9.633784	3.976282
-1128.583098	-1.163165	3.986278
-1126.604612	-0.197419	3.996275
-1124.626237	-0.242198	4.006272
-1122.707728	-6.307512	4.016269
-1120.875782	2.450249	4.026266
-1118.980673	0.074014	4.036262
-1117.166233	2.362352	4.046259
-1115.206810	3.076943	4.056256
-1113.403466	2.657534	4.066253
-1111.617796	-2.795984	4.076250
-1109.666024	-0.161708	4.086246
-1107.784983	3.101266	4.096243
-1105.738969	1.473020	4.106240
-1104.279495	4.031315	4.116237
-1102.317356	3.378087	4.126234
-1100.436663	11.007000	4.136230
-1098.387538	9.744585	4.146227
-1096.267913	5.857685	4.156224
-1094.628828	8.444099	4.166221
-1092.848676	5.618895	4.176218
-1090.606920	4.292514	4.186214
-1089.043662	-1.878583	4.196211
-1087.307309	1.735980	4.206208
-1085.288710	0.478460	4.216205
-1083.333933	5.294427	4.226202
-1081.328583	5.824855	4.236198
-1079.733713	2.170334	4.246195
-1077.533116	2.281104	4.256192
-1075.894118	-8.117970	4.266189
-1074.241560	-4.718946	4.276186
-1072.286049	2.915388	4.286182
-1070.624623	-0.923460	4.296179
-1068.321924	-5.766477	4.306176
-1066.350607	-7.237474	4.316173
-1064.559784	-7.255361	4.326170
-1062.357400	-7.007491	4.336166
-1060.842701	-6.490147	4.346163
-1059.215945	-4.148058	4.356160
-1056.919740	-8.647387	4.366157
-1055.307207	-6.740397	4.376154
-1053.561722	2.111781	4.386150
-1051.486850	-2.710570	4.396147
-1049.800539	-5.852317	4.406144
-1047.894260	-3.955989	4.416141
-1045.954896	-4.341838	4.426138
-1043.897629	-8.046607	4.436134
-1042.119889	-0.025385	4.446131
-1040.154393	-3.101251	4.456128
-1038.097104	-7.923935	4.466125
-1036.716448	-7.359872	4.476122
-1034.432192	-4.180277	4.486118
-1032.744815	-4.920556	4.496115
-1030.732819	-7.135413	4.506112
-1028.762581	-6.100368	4.516109
-1027.146451	-4.204986	4.526106
-1025.444694	-6.974969	4.536102
-1023.622619	4.135557	4.546099
-1021.407267	1.733444	4.556096
-1019.343513	-0.172307	4.566093
-1017.669966	5.629768	4.576090
-1015.936302	3.743653	4.586086
-1014.178490	4.539522	4.596083
-1012.263873	8.089319	4.606080
-1010.081709	8.451001	4.616077
-1008.302495	6.364971	4.626074
-1006.318663	6.941537	4.636070
-1004.625896	3.495623	4.646067
-1002.633501	0.991812	4.656064
-1000.856931	-4.289643	4.666061
-998.897404	6.309442	4.676058
-997.329495	-6.449846	4.686054
-995.235437	1.492408	4.696051
-993.146369	-0.122100	4.706048
-991.520484	-6.198940	4.716045
-989.454931	-5.201210	4.726042
-987.511400	-1.984446	4.736038
-985.845988	-2.850655	4.746035
-983.848943	-0.924577	4.756032
-982.263087	-1.359632	4.766029
-980.065644	-1.303530	4.776026
-978.132491	4.360743	4.786022
-976.288518	-0.746734	4.796019
-974.669846	-2.933384	4.806016
-972.795548	-6.083034	4.816013
-970.974701	-1.791878	4.826010
-969.030772	-3.661055	4.836006
-967.001226	-3.979153	4.846003
-964.924347	1.302140	4.856000
-963.372272	-5.241311	4.865997
-961.654540	2.172195	4.875994
-959.635618	2.182652	4.885990
-957.512522	5.078618	4.895987
-955.719568	1.670402	4.905984
-953.674295	-1.307622	4.915981
-952.108588	4.816491	4.925978
-950.420531	-7.590923	4.935974
-948.218819	-2.143257	4.945971
-946.606483	-2.783053	4.955968
-944.719149	-1.761522	4.965965
-942.511729	-4.815992	4.975962
-940.800572	-4.191033	4.985958
-938.774034	0.719379	4.995955
-937.133158	-1.275003	5.005952
-934.983979	-0.535337	5.015949
-933.376589	0.434648	5.025946
-931.419698	3.090366	5.035942
-929.506757	2.453043	5.045939
-927.634668	-0.039364	5.055936
-925.700825	-7.723857	5.065933
-923.915524	2.356827	5.075930
-922.075182	2.694297	5.085926
-920.427109	2.383548	5.095923
-918.425076	1.965679	5.105920
-916.396952	0.098872	5.115917
-914.284594	5.617704	5.125914
-912.803838	7.438496	5.135910
-910.711705	11.788964	5.145907
-908.959539	4.904068	5.155904
-907.030550	6.222135	5.165901
-905.058473	7.332784	5.175898
-903.339056	4.781118	5.185894
-901.049618	1.236719	5.195891
-899.413373	2.072638	5.205888
-897.441589	2.577011	5.215885
-895.995212	5.238591	5.225882
-894.275016	7.824815	5.235878
-892.072776	2.878018	5.245875
-890.173004	9.575625	5.255872
-888.118362	1.334988	5.265869
-886.274885	1.373558	5.275866
-884.534950	6.156154	5.285862
-882.594168	4.884404	5.295859
-880.836219	2.085010	5.305856
-878.892186	3.335957	5.315853
-876.808049	4.676615	5.325850
-875.034444	-0.861654	5.335846
-873.286261	0.245342	5.345843
-871.421179	7.144304	5.355840
-869.395707	0.589962	5.365837
-867.322380	-1.097710	5.375834
-866.080431	6.188250	5.385830
-863.884351	2.706180	5.395827
-861.958882	4.238010	5.405824
-860.166844	2.993215	5.415821
-858.390130	-4.456105	5.425818
-856.061723	0.440861	5.435814
-854.496786	-2.750824	5.445811
-852.581821	0.175354	5.455808
-850.665817	-2.112431	5.465805
-848.853604	6.820836	5.475802
-846.920529	-0.378732	5.485798
-845.006583	0.578625	5.495795
-843.191103	0.999081	5.505792
-841.591794	-1.249123	5.515789
-839.674360	6.819418	5.525786
-837.642360	-0.282270	5.535782
-835.482993	3.482769	5.545779
-833.686511	8.333737	5.555776
-832.225618	3.586028	5.565773
-830.204041	6.313602	5.575770
-827.953382	-0.365127	5.585766
-826.280744	8.118357	5.595763
-824.441213	4.416994	5.605760
-822.497130	1.960528	5.615757
-820.703505	-2.093500	5.625754
-818.855245	4.429240	5.635750
-816.973197	5.227505	5.645747
-815.056661	5.385507	5.655744
-813.249648	6.989998	5.665741
-811.297972	-3.034159	5.675738
-809.379579	4.260554	5.685734
-807.629303	2.307195	5.695731
-805.641016	5.706442	5.705728
-803.782769	1.105241	5.715725
-802.143555	-0.697727	5.725722
-800.304974	4.926556	5.735718
-797.955367	5.070615	5.745715
-796.109050	3.975091	5.755712
-794.492298	0.737264	5.765709
-792.479167	1.186168	5.775706
-790.546157	3.948459	5.785702
-789.106981	10.732408	5.795699
-787.309591	10.268410	5.805696
-784.915116	6.652065	5.815693
-782.987581	4.371963	5.825690
-781.343629	9.296303	5.835686
-779.290357	4.504470	5.845683
-777.604164	13.053726	5.855680
-775.541219	4.750267	5.865677
-773.565112	6.466713	5.875674
-771.918440	-2.374957	5.885670
-770.303505	4.965135	5.895667
-768.164933	3.854502	5.905664
-766.202451	0.589858	5.915661
-764.406752	4.395720	5.925658
-762.673788	5.020483	5.935654
-760.710603	4.500006	5.945651
-758.711747	4.029094	5.955648
-756.962435	-2.803134	5.965645
-755.043513	2.449916	5.975642
-753.033281	2.071930	5.985638
-751.231002	1.097165	5.995635
-749.372911	-2.092358	6.005632
-747.456996	6.657052	6.015629
-745.749490	4.424776	6.025626
-743.784065	4.582919	6.035622
-741.856513	6.881902	6.045619
-739.901280	7.828011	6.055616
-738.297787	1.162785	6.065613
-736.519432	-3.799816	6.075610
-734.515030	3.860174	6.085606
-732.550624	13.190813	6.095603
-730.346422	5.731678	6.105600
-728.899930	4.897475	6.115597
-726.766276	1.209183	6.125594
-724.798921	9.934605	6.135590
-723.048670	13.427231	6.145587
-721.490061	8.725549	6.155584
-719.160591	5.899675	6.165581
-717.394478	6.362855	6.175578
-715.590292	4.473580	6.185574
-713.678892	7.300971	6.195571
-712.001423	8.237805	6.205568
-709.994325	1.324937	6.215565
-708.084679	0.789374	6.225562
-706.463294	3.244684	6.235558
-704.377243	3.415162	6.245555
-702.219203	7.627394	6.255552
-700.655384	7.698166	6.265549
-698.892517	4.855483	6.275546
-696.768256	6.308314	6.285542
-695.067493	6.693531	6.295539
-693.126718	8.485167	6.305536
-691.253587	12.027658	6.315533
-689.346662	1.281244	6.325530
-687.467973	5.088117	6.335526
-685.746706	7.775383	6.345523
-683.466666	3.373720	6.355520
-681.934971	5.748640	6.365517
-680.070398	2.834454	6.375514
-678.150119	4.059364	6.385510
-676.155391	1.924930	6.395507
-674.407585	6.422218	6.405504
-672.483803	3.694372	6.415501
-670.332500	6.619258	6.425498
-669.050642	4.235570	6.435494
-666.839570	1.509193	6.445491
-664.847035	12.793343	6.455488
-662.983685	1.035463	6.465485
-661.186433	-0.274754	6.475482
-659.195441	8.560638	6.485478
-657.560190	9.366886	6.495475
-655.736810	11.609954	6.505472
-654.009841	7.520902	6.515469
-651.881842	9.333186	6.525466
-649.640264	6.314574	6.535462
-648.167470	1.407170	6.545459
-646.235703	6.836690	6.555456
-644.036857	2.316980	6.565453
-642.673158	2.961356	6.575450
-640.749432	1.024616	6.585446
-638.736259	5.004258	6.595443
-636.692314	2.981996	6.605440
-634.664105	-3.430489	6.615437
-633.084763	2.625362	6.625434
-631.101646	-1.780920	6.635430
-629.351835	-4.327774	6.645427
-627.669419	3.050593	6.655424
-625.653215	5.201296	6.665421
-623.755864	0.565558	6.675418
-621.599252	2.809099	6.685414
-619.747053	0.267998	6.695411
-618.264482	1.960792	6.705408
-616.228499	1.417750	6.715405
-614.310597	6.432660	6.725402
-612.240443	-1.518126	6.735398
-610.567492	7.006534	6.745395
-608.652616	-0.485222	6.755392
-606.952575	5.188199	6.765389
-604.755103	1.286127	6.775386
-602.989103	1.801517	6.785382
-601.484322	5.796095	6.795379
-599.456018	9.902833	6.805376
-597.539738	9.138925	6.815373
-595.287190	5.665440	6.825370
-593.813661	5.487016	6.835366
-591.682490	5.205112	6.845363
-589.654602	-0.897806	6.855360
-587.925021	0.982921	6.865357
-586.309874	-4.534571	6.875354
-584.258523	1.911713	6.885350
-582.381288	2.827781	6.895347
-580.407151	2.116224	6.905344
-578.722669	3.626785	6.915341
-576.577033	-0.979105	6.925338
-575.038801	-2.922108	6.935334
-573.312666	-4.138792	6.945331
-571.276978	-1.948522	6.955328
-569.431183	-4.783832	6.965325
-567.344720	-3.159052	6.975322
-565.298874	-2.686758	6.985318
-563.511358	-3.212170	6.995315
-561.984906	3.082714	7.005312
-559.834488	1.487203	7.015309
-558.100724	-3.603944	7.025306
-556.016667	-7.904707	7.035302
-554.081342	1.576003	7.045299
-552.360596	0.327036	7.055296
-550.495920	4.968388	7.065293
-548.464333	0.374424	7.075290
-546.918119	4.060833	7.085286
-545.173400	-5.067948	7.095283
-543.083466	7.877642	7.105280
-540.987729	8.387779	7.115277
-539.167738	5.918200	7.125274
-537.283616	-2.623355	7.135270
-535.577663	1.647035	7.145267
-533.864561	-1.187580	7.155264
-531.834126	7.426888	7.165261
-529.635160	5.624697	7.175258
-527.690776	-0.491677	7.185254
-526.341669	-0.519131	7.195251
-524.531220	0.699763	7.205248
-522.257159	-0.247551	7.215245
-520.599924	3.064292	7.225242
-518.703213	7.845822	7.235238
-516.451662	5.466808	7.245235
-514.862874	4.294208	7.255232
-513.011049	4.597005	7.265229
-511.277908	0.151794	7.275226
-509.044312	3.014738	7.285222
-507.329317	0.295104	7.295219
-505.698732	2.423816	7.305216
-503.700855	-1.743138	7.315213
-501.437122	2.423981	7.325210
-499.893460	-2.723610	7.335206
-497.966032	-3.410270	7.345203
-495.940423	3.510747	7.355200
-494.274654	-3.143750	7.365197
-492.680924	5.831035	7.375194
-490.412114	-1.098198	7.385190
-488.374597	3.959297	7.395187
-486.654302	10.850138	7.405184
-484.887559	10.181256	7.415181
-483.064009	7.185346	7.425178
-480.769344	5.648976	7.435174
-479.428399	1.481164	7.445171
-477.386224	4.663666	7.455168
-475.281987	0.034472	7.465165
-473.548648	0.964133	7.475162
-471.576490	-1.662331	7.485158
-469.929999	2.889192	7.495155
-467.947413	1.780052	7.505152
-466.309936	-8.258418	7.515149
-464.274298	-5.944885	7.525146
-462.347712	-3.337612	7.535142
-460.281850	-2.401044	7.545139
-458.632708	8.197595	7.555136
-456.628335	-1.038916	7.565133
-454.807799	6.047524	7.575130
-452.987921	-0.606295	7.585126
-450.994971	1.437744	7.595123
-449.059738	1.089360	7.605120
-447.507728	2.689067	7.615117
-445.173983	-1.711481	7.625114
-443.496654	0.946665	7.635110
-441.750920	5.892900	7.645107
-440.069004	1.665921	7.655104
-438.222518	0.567486	7.665101
-435.823104	0.358152	7.675098
-433.867940	-10.147882	7.685094
-432.505549	-1.755077	7.695091
-430.375558	-2.450344	7.705088
-428.523357	0.310945	7.715085
-426.687065	1.355257	7.725082
-424.880634	-0.349420	7.735078
-422.740848	-2.151538	7.745075
-421.168881	5.396213	7.755072
-419.344250	0.862242	7.765069
-417.134423	-7.165958	7.775066
-415.374926	-4.069321	7.785062
-413.770086	1.837351	7.795059
-411.675150	-3.175577	7.805056
-409.728042	1.525362	7.815053
-407.847371	-0.225894	7.825050
-405.958962	-5.040045	7.835046
-404.205105	3.132375	7.845043
-402.273978	5.115274	7.855040
-400.143179	0.237158	7.865037
-398.725449	-0.780154	7.875034
-396.694334	-4.818116	7.885030
-394.661508	0.917599	7.895027
-392.790056	-0.091627	7.905024
-391.082698	-0.041992	7.915021
-389.080373	0.298452	7.925018
-387.322576	-5.781708	7.935014
-385.325812	-1.857645	7.945011
-383.602276	-3.999068	7.955008
-381.787315	5.669973	7.965005
-379.799184	-3.069663	7.975002
-377.842129	-4.103599	7.984998
-376.060002	-4.934335	7.994995
-373.908547	-1.046013	8.004992
-372.229496	-2.090822	8.014989
-370.611221	-0.961131	8.024986
-368.389596	-0.993587	8.034982
-366.714912	2.219264	8.044979
-364.747315	-3.404891	8.054976
-362.760268	3.437140	8.064973
-360.925636	3.450687	8.074970
-359.186607	1.726819	8.084966
-357.719670	0.747465	8.094963
-355.450560	3.028556	8.104960
-353.397505	4.950975	8.114957
-351.533460	-1.204548	8.124954
-349.489572	1.144086	8.134950
-347.817227	2.102525	8.144947
-346.079604	0.304678	8.154944
-344.211768	3.347758	8.164941
-342.335394	2.119883	8.174938
-340.256179	2.917053	8.184934
-338.332750	1.956414	8.194931
-336.841547	0.298969	8.204928
-334.758213	9.775205	8.214925
-332.574089	5.851816	8.224922
-331.155494	-0.311529	8.234918
-329.319058	2.559728	8.244915
-327.155196	8.519332	8.254912
-325.161957	4.370627	8.264909
-323.348259	-1.318931	8.274906
-321.767429	-2.941726	8.284902
-319.569095	-5.886816	8.294899
-318.046331	-2.044924	8.304896
-316.047055	7.051578	8.314893
-314.233778	3.421097	8.324890
-312.111978	-2.936602	8.334886
-310.136455	-0.858081	8.344883
-308.450254	0.811878	8.354880
-306.461938	0.848303	8.364877
-304.664408	2.786291	8.374874
-303.147361	3.221643	8.384870
-301.218098	4.098049	8.394867
-298.856799	0.064300	8.404864
-297.177986	0.818053	8.414861
-295.266486	4.083156	8.424858
-293.290692	9.829650	8.434854
-291.679854	2.730874	8.444851
-289.808494	0.362229	8.454848
-288.159374	-0.570373	8.464845
-285.759261	-1.419162	8.474842
-283.883598	-1.551057	8.484838
-282.035322	2.865761	8.494835
-280.523963	3.680993	8.504832
-278.523526	3.244966	8.514829
-276.695694	2.995971	8.524826
-274.788850	-1.033111	8.534822
-272.542423	5.706020	8.544819
-270.815729	2.229922	8.554816
-269.065424	2.470163	8.564813
-267.265150	3.480873	8.574810
-265.280676	4.106910	8.584807
-263.366657	-3.147611	8.594803
-261.615078	2.708908	8.604800
-259.820109	4.513125	8.614797
-257.696935	2.317475	8.624794
-255.722768	5.211020	8.634791
-253.990482	4.689916	8.644787
-252.231746	2.356644	8.654784
-250.232083	6.204573	8.664781
-248.730675	2.912873	8.674778
-246.491356	3.825101	8.684775
-244.521800	4.090368	8.694771
-242.834810	4.591793	8.704768
-241.270190	3.079008	8.714765
-239.004701	5.228155	8.724762
-237.127129	1.968006	8.734759
-235.121742	2.420199	8.744755
-233.288498	-0.193380	8.754752
-231.557113	3.560010	8.764749
-229.755021	5.052052	8.774746
-227.576467	-2.623623	8.784743
-225.733240	-0.471809	8.794739
-224.242225	2.533611	8.804736
-221.937253	-7.830731	8.814733
-220.144339	-3.337133	8.824730
-218.230384	-8.281542	8.834727
-216.827274	-3.942051	8.844723
-214.509467	-8.890910	8.854720
-212.787754	-2.448518	8.864717
-211.113784	-2.581326	8.874714
-208.831355	-6.818723	8.884711
-207.055002	-7.804735	8.894707
-205.305102	-4.449030	8.904704
-203.536608	-4.559022	8.914701
-201.466590	-13.679496	8.924698
-199.613786	-5.753237	8.934695
-197.692181	-5.805552	8.944691
-195.845013	-5.298076	8.954688
-194.207952	-5.936577	8.964685
-192.579804	-4.143583	8.974682
-190.201807	-10.821547	8.984679
-188.197329	-5.456924	8.994675
-186.490811	-6.319667	9.004672
-184.617696	-11.579648	9.014669
-182.775455	-7.033891	9.024666
-180.844468	-8.595629	9.034663
-178.814699	-17.894402	9.044659
-177.322947	-11.508450	9.054656
-175.133374	-14.843603	9.064653
-173.431821	-11.634901	9.074650
-171.484062	-14.959885	9.084647
-169.655204	-17.009014	9.094643
-167.803062	-13.579596	9.104640
-165.918944	-12.902725	9.114637
-163.998525	-4.252992	9.124634
-162.227382	-5.080241	9.134631
-160.256846	-8.116738	9.144627
-158.491236	-10.357878	9.154624
-156.560079	-0.539816	9.164621
-154.478451	-3.938257	9.174618
-152.689648	-5.415704	9.184615
-150.865170	-4.141919	9.194611
-148.939866	-7.502778	9.204608
-147.077819	-7.537655	9.214605
-145.280149	-5.023235	9.224602
-143.426306	-4.892585	9.234599
-141.259152	-4.273489	9.244595
-139.531014	-2.430096	9.254592
-138.174127	-3.323862	9.264589
-135.665967	-3.340243	9.274586
-134.020864	-7.641674	9.284583
-132.031377	-10.374847	9.294579
-130.269310	-11.620636	9.304576
-128.435428	-9.320410	9.314573
-126.428329	-7.755210	9.324570
-124.860040	-4.122563	9.334567
-122.625593	-13.665542	9.344563
-120.675698	-7.998457	9.354560
-118.845003	-4.372938	9.364557
-117.328773	-8.137464	9.374554
-115.143571	-7.066474	9.384551
-113.246393	-2.834171	9.394547
-111.657710	0.994185	9.404544
-109.405245	0.284395	9.414541
-107.670943	-5.352871	9.424538
-106.038759	-8.077965	9.434535
-104.066644	-1.144896	9.444531
-102.169297	-3.103850	9.454528
-99.856469	-3.673258	9.464525
-98.626542	-2.953539	9.474522
-96.594400	0.851444	9.484519
-94.656956	0.030871	9.494515
-92.638974	1.924375	9.504512
-90.760474	-0.863694	9.514509
-88.904486	0.863021	9.524506
-87.034155	-1.816370	9.534503
-85.264328	-0.341177	9.544499
-83.371991	1.989235	9.554496
-81.684648	0.100118	9.564493
-79.490486	2.057107	9.574490
-77.786116	-3.330620	9.584487
-75.767477	4.125596	9.594483
-73.994400	-1.568363	9.604480
-72.046174	0.292075	9.614477
-70.064744	2.515124	9.624474
-68.086695	-2.444139	9.634471
-66.441469	-1.973822	9.644467
-64.498733	-1.508334	9.654464
-62.836826	-1.545955	9.664461
-60.875262	6.284129	9.674458
-58.587900	2.155028	9.684455
-57.185264	-1.362389	9.694451
-55.303417	2.643456	9.704448
-53.548634	1.610468	9.714445
-51.450868	5.823458	9.724442
-49.463004	3.698520	9.734439
-47.592735	1.944460	9.744435
-45.791656	1.317790	9.754432
-44.035526	2.138336	9.764429
-41.677411	4.869757	9.774426
-40.291851	1.555605	9.784423
-38.407963	2.827895	9.794419
-36.372878	1.087027	9.804416
-34.657560	7.112149	9.814413
-32.619019	7.631856	9.824410
-30.805253	10.320646	9.834407
-28.966724	-1.004955	9.844403
-27.130984	4.285676	9.854400
-25.342715	3.719487	9.864397
-23.252044	3.291383	9.874394
-21.314803	5.616262	9.884391
-19.535237	-2.646145	9.894387
-17.554727	-0.326587	9.904384
-15.816555	-1.386899	9.914381
-13.833067	6.386044	9.924378
-11.844539	5.333170	9.934375
-10.067963	1.789289	9.944371
-8.192873	3.443545	9.954368
-6.381254	2.471000	9.964365
-4.629101	3.919072	9.974362
-3.534929	25.094317	9.984359
-2.299184	64.047114	9.994355
-0.873236	119.994556	10.004352
0.000000	177.232810	10.009357
0.578669	219.127398	10.014362
1.310766	256.835126	10.019367
2.256518	276.844797	10.024371
2.731698	299.104251	10.029376
2.850122	330.078448	10.034381
3.142852	330.167446	10.039386
3.162382	336.994446	10.044391
3.504122	357.840192	10.049395
3.685304	373.934788	10.054400
3.884970	382.999253	10.059405
3.949288	377.494726	10.064410
3.815682	384.365098	10.069415
3.863841	382.367285	10.074419
4.147892	388.205905	10.079424
3.347261	388.948715	10.084429
3.821325	390.694624	10.089434
4.177272	396.187451	10.094439
4.375236	420.172414	10.099443
4.715302	411.476152	10.104448
4.248245	411.484482	10.109453
4.418933	392.887893	10.114458
4.187042	400.600309	10.119463
4.473027	426.954123	10.124467
4.685547	423.949178	10.129472
4.876346	437.813977	10.134477
4.534684	419.347965	10.139482
4.637485	419.702235	10.144487
4.620032	429.506290	10.149491
4.636443	428.719958	10.154496
4.648312	438.519342	10.159501
5.096704	440.915934	10.164506
5.406657	446.999616	10.169511
4.572967	436.123443	10.174515
5.280423	438.398284	10.179520
5.014111	442.733493	10.184525
4.965571	439.174069	10.189530
5.210974	454.214520	10.194535
5.024165	452.850292	10.199539
5.375189	452.232947	10.204544
5.133048	464.367439	10.209549
5.203451	464.450898	10.214554
5.412864	467.390261	10.219559
5.063828	468.732857	10.224563
5.421315	464.493623	10.229568
4.873911	473.945401	10.234573
5.206367	465.676118	10.239578
5.525076	478.236852	10.244583
5.293035	475.067829	10.249587
5.475811	472.709470	10.254592
5.394470	476.893754	10.259597
6.125667	474.052084	10.264602
5.740819	477.825864	10.269607
5.614278	480.159617	10.274611
5.670687	478.002772	10.279616
5.349334	491.693834	10.284621
5.890833	501.099684	10.289626
6.205840	510.634711	10.294631
5.981828	507.637874	10.299635
6.035485	507.183082	10.304640
5.893202	521.026967	10.309645
6.372069	514.275067	10.314650
6.022872	522.028336	10.319655
6.130343	521.478223	10.324659
6.150210	514.222341	10.329664
6.234477	521.682532	10.334669
6.207200	529.095860	10.339674
6.466288	532.043084	10.344679
6.427273	530.093849	10.349683
6.756424	534.241061	10.354688
6.277446	532.557555	10.359693
6.337064	531.707553	10.364698
6.868736	528.861426	10.369703
6.419184	530.716826	10.374707
6.623091	530.894114	10.379712
6.322217	536.999567	10.384717
6.516719	548.958821	10.389722
6.736958	558.942682	10.394727
6.756475	563.323803	10.399731
7.377399	573.327346	10.404736
7.012042	572.243912	10.409741
6.947523	573.150029	10.414746
6.861588	580.591663	10.419751
7.151881	578.216138	10.424755
7.233518	568.685746	10.429760
6.827120	580.425464	10.434765
7.198215	577.787878	10.439770
6.962399	580.333053	10.444775
6.896050	587.714794	10.449779
7.207322	581.935821	10.454784
7.029475	583.028758	10.459789
7.554088	600.753107	10.464794
7.656403	610.484561	10.469799
7.647514	614.715679	10.474803
7.642786	617.578836	10.479808
7.304654	617.199149	10.484813
7.945251	607.270474	10.489818
7.867154	621.345505	10.494823
7.738769	625.236120	10.499827
8.069130	626.322120	10.504832
7.872218	618.045719	10.509837
7.935531	602.960722	10.514842
8.003852	608.669829	10.519847
7.944120	612.194654	10.524851
8.080552	602.318013	10.529856
7.871524	623.505895	10.534861
8.317115	626.461239	10.539866
7.981931	632.718869	10.544871
8.109533	632.518800	10.549875
8.361973	627.034637	10.554880
7.942357	641.522150	10.559885
8.225783	635.981000	10.564890
8.150825	637.896519	10.569895
7.787941	631.827640	10.574899
7.996299	637.604313	10.579904
7.894634	650.369451	10.584909
8.352317	652.280443	10.589914
8.579067	662.275953	10.594919
8.640148	664.146120	10.599923
8.510449	661.388113	10.604928
8.226114	670.810673	10.609933
8.673100	660.548545	10.614938
8.702855	671.628952	10.619943
8.508835	670.076607	10.624947
8.735796	667.411529	10.629952
8.775113	683.749884	10.634957
9.011081	694.587669	10.639962
8.975339	698.783668	10.644967
8.980990	699.494085	10.649971
9.172408	701.324543	10.654976
8.916594	710.720501	10.659981
8.896171	701.576909	10.664986
9.157030	700.615945	10.669991
9.371680	707.968697	10.674995
9.230200	699.614018	10.680000
9.030868	714.746178	10.685005
9.206742	705.576004	10.690010
9.215314	706.796921	10.695015
9.209786	720.743770	10.700019
9.563314	737.326977	10.705024
9.212738	733.582253	10.710029
9.313161	732.609028	10.715034
9.797417	749.795912	10.720039
9.605177	749.244707	10.725043
9.801529	746.068799	10.730048
9.568423	744.502179	10.735053
9.931925	745.975590	10.740058
9.506368	753.414709	10.745063
9.491078	755.003737	10.750067
9.983792	744.568666	10.755072
10.076514	751.562394	10.760077
10.263408	763.952000	10.765082
10.213132	760.552058	10.770087
10.167152	751.877743	10.775091
10.226591	756.236785	10.780096
10.133532	768.300438	10.785101
10.474463	775.592079	10.790106
10.508559	791.202784	10.795111
10.536157	787.042887	10.800115
10.403766	774.786638	10.805120
10.340337	786.380346	10.810125
10.594972	789.916578	10.815130
10.607017	792.045337	10.820135
10.360722	800.588219	10.825139
10.635224	793.767856	10.830144
10.486474	796.426924	10.835149
10.642729	798.475907	10.840154
10.602837	804.022566	10.845159
10.251175	796.981932	10.850163
10.419359	790.828279	10.855168
10.502900	804.328886	10.860173
10.816323	807.642842	10.865178
11.057977	828.382218	10.870183
10.955206	830.478829	10.875187
11.023726	835.888351	10.880192
10.948115	832.620175	10.885197
11.144136	828.715697	10.890202
11.267466	826.355724	10.895207
11.098006	843.113940	10.900211
11.541335	824.834463	10.905216
11.099499	832.249408	10.910221
11.271355	831.640126	10.915226
11.378129	833.386324	10.920231
11.186025	836.328300	10.925235
11.676521	830.496987	10.930240
11.496958	832.946494	10.935245
11.893822	827.070187	10.940250
11.434547	832.524465	10.945255
11.457664	828.985059	10.950259
11.638638	829.369451	10.955264
11.847085	833.786757	10.960269
11.913000	832.038381	10.965274
11.878894	842.391036	10.970279
11.969665	849.875591	10.975283
11.999338	843.805514	10.980288
12.080616	865.672895	10.985293
12.420577	852.230981	10.990298
12.307205	839.536372	10.995303
12.306878	829.561533	11.000307
12.533666	822.233066	11.005312
12.438948	831.871508	11.010317
12.326049	829.568138	11.015322
12.359842	829.595933	11.020327
12.508800	829.130662	11.025331
12.500543	820.062331	11.030336
12.141575	836.424958	11.035341
12.659661	827.050303	11.040346
12.478047	835.073496	11.045351
12.345357	840.543500	11.050355
12.551881	831.835172	11.055360
12.239215	839.743642	11.060365
12.495865	843.935627	11.065370
12.778201	856.103492	11.070375
12.961855	864.770236	11.075379
13.048476	867.435932	11.080384
12.808057	862.132804	11.085389
13.090103	864.868261	11.090394
12.918737	863.534649	11.095399
12.945170	858.671542	11.100403
13.500540	850.809645	11.105408
13.115533	849.857066	11.110413
13.580192	847.395335	11.115418
13.297573	841.859230	11.120423
13.157568	830.028380	11.125427
13.341233	832.509845	11.130432
13.400273	849.816714	11.135437
13.801111	849.033703	11.140442
13.567894	834.050961	11.145447
13.379911	828.275823	11.150451
13.387300	820.182779	11.155456
13.199049	835.792725	11.160461
13.404503	843.516047	11.165466
13.767664	854.160186	11.170471
13.658713	849.574163	11.175475
13.657460	854.575319	11.180480
13.798020	861.900541	11.185485
13.682757	865.644035	11.190490
13.823492	864.065085	11.195495
13.766607	870.677426	11.200499
13.855329	866.458867	11.205504
14.001859	868.440021	11.210509
14.096697	863.594390	11.215514
13.905890	863.329978	11.220519
13.683600	870.045977	11.225523
14.232137	861.436055	11.230528
13.701471	868.918808	11.235533
14.101512	873.046926	11.240538
14.199177	891.066829	11.245543
14.166021	898.746232	11.250547
14.559747	893.934925	11.255552
14.535539	894.227458	11.260557
14.613160	896.957678	11.265562
14.599722	893.271110	11.270567
14.434753	900.752324	11.275571
14.569874	890.404151	11.280576
14.453663	906.690287	11.285581
14.992568	895.402429	11.290586
14.848564	900.733900	11.295591
14.659636	901.323963	11.300595
14.970363	895.163302	11.305600
14.644639	893.231361	11.310605
14.995657	888.959920	11.315610
15.085361	907.936821	11.320615
14.940438	899.852256	11.325619
15.052602	889.733267	11.330624
15.021494	901.714604	11.335629
15.281782	890.529541	11.340634
15.010424	903.714658	11.345639
15.065374	898.837528	11.350643
15.297202	897.453795	11.355648
15.066287	903.660213	11.360653
14.976712	894.396633	11.365658
14.845657	889.981292	11.370663
15.131830	914.853512	11.375667
15.634678	921.179463	11.380672
15.666478	926.697386	11.385677
15.795654	929.059814	11.390682
15.558288	931.463360	11.395687
15.701470	927.414307	11.400691
15.778373	931.232832	11.405696
15.678087	932.027971	11.410701
15.639954	934.907559	11.415706
15.411320	940.123222	11.420711
15.613393	931.994332	11.425715
16.021096	933.161069	11.430720
15.589734	932.089710	11.435725
16.267211	926.812055	11.440730
16.209691	934.384967	11.445735
15.948316	938.610715	11.450739
15.663607	928.829412	11.455744
15.829175	929.118487	11.460749
16.015793	934.534442	11.465754
16.080759	941.630468	11.470759
16.010365	955.135266	11.475763
16.438421	955.082829	11.480768
16.262262	963.472682	11.485773
16.926497	960.985408	11.490778
16.489324	960.075836	11.495783
16.805460	961.768155	11.500787
16.626088	962.684729	11.505792
16.617558	966.371799	11.510797
16.814891	955.554726	11.515802
16.796915	957.510087	11.520807
16.682370	965.099996	11.525811
17.018747	955.869369	11.530816
16.974932	959.953181	11.535821
16.871830	960.076934	11.540826
16.834251	965.818844	11.545831
16.741142	968.077950	11.550835
17.072629	957.619555	11.555840
16.935523	961.134727	11.560845
17.009121	950.217536	11.565850
17.020413	959.659366	11.570855
16.807860	970.124159	11.575859
16.980010	960.441868	11.580864
16.855688	960.630512	11.585869
17.089525	966.081529	11.590874
17.020403	973.955958	11.595879
17.120171	992.494512	11.600883
17.125524	993.657614	11.605888
17.139587	995.197828	11.610893
17.313769	987.373002	11.615898
17.605555	1001.282161	11.620903
17.319489	1004.658663	11.625907
17.523177	992.853292	11.630912
17.335345	1001.648763	11.635917
17.727689	1002.647630	11.640922
18.074611	1018.169257	11.645927
18.148591	1020.248743	11.650931
17.940928	1001.088776	11.655936
17.966100	1003.075112	11.660941
18.123843	1004.116129	11.665946
18.264632	996.291894	11.670951
17.812709	996.745697	11.675955
18.086424	1003.480424	11.680960
18.260460	1008.220266	11.685965
18.243636	999.791910	11.690970
18.172575	1008.135061	11.695975
18.193573	1025.083900	11.700979
18.725290	1021.005969	11.705984
18.393036	1027.720654	11.710989
18.615890	1006.623162	11.715994
18.529228	1006.517193	11.720999
18.159818	1005.357092	11.726003
18.843098	1011.051857	11.731008
18.601656	1027.026913	11.736013
18.504853	1027.477697	11.741018
18.699350	1019.728468	11.746023
18.675038	1028.814869	11.751027
19.166712	1016.302745	11.756032
19.090206	1026.725378	11.761037
19.205573	1001.885255	11.766042
18.883540	999.282450	11.771047
18.558944	993.158420	11.776051
18.954076	1012.151403	11.781056
18.960692	1022.508731	11.786061
19.119022	1023.896616	11.791066
19.138106	1026.469025	11.796071
19.314965	1030.634364	11.801075
19.412127	1024.741121	11.806080
19.136297	1032.348904	11.811085
19.235819	1026.581452	11.816090
19.466853	1033.816629	11.821095
18.979246	1026.625663	11.826099
19.243078	1028.594438	11.831104
19.185636	1029.876378	11.836109
19.237264	1023.864231	11.841114
19.104192	1018.796257	11.846119
19.177094	1022.509780	11.851123
19.426509	1033.981241	11.856128
19.259614	1049.307287	11.861133
19.304703	1059.373839	11.866138
19.629670	1056.335849	11.871143
19.326594	1062.030249	11.876147
19.861175	1056.089305	11.881152
19.753919	1061.268303	11.886157
20.152987	1052.089124	11.891162
19.825560	1062.591231	11.896167
19.800390	1061.872215	11.901171
20.079208	1064.585359	11.906176
20.152561	1086.127089	11.911181
20.333230	1089.459131	11.916186
20.368032	1083.025404	11.921191
20.375149	1075.345460	11.926195
20.505378	1062.545564	11.931200
20.174929	1059.113750	11.936205
20.393636	1049.239454	11.941210
20.416511	1063.346120	11.946215
20.877770	1072.244703	11.951219
20.685865	1050.181881	11.956224
20.525036	1057.549753	11.961229
20.455182	1049.252051	11.966234
20.749611	1056.699499	11.971239
20.529264	1055.517196	11.976243
20.787834	1065.462174	11.981248
20.757982	1085.410940	11.986253
21.070449	1076.635890	11.991258
21.004848	1075.469119	11.996263
21.006776	1074.416168	12.001267
20.872233	1061.701873	12.006272
20.941979	1070.198447	12.011277
20.963217	1080.614990	12.016282
21.122722	1078.992019	12.021287
21.083518	1073.619657	12.026291
20.931656	1059.994988	12.031296
20.625003	1084.681333	12.036301
21.087451	1073.267538	12.041306
21.214686	1082.281699	12.046311
20.887766	1080.904272	12.051315
21.501704	1080.614800	12.056320
21.443806	1073.947471	12.061325
21.034680	1061.371597	12.066330
20.877924	1057.631357	12.071335
21.002490	1057.113195	12.076339
20.981193	1052.993350	12.081344
20.931318	1062.554611	12.086349
20.971277	1052.010171	12.091354
21.190777	1055.746845	12.096359
20.923225	1052.040049	12.101363
21.142582	1048.587570	12.106368
20.843455	1059.402157	12.111373
21.042513	1057.086843	12.116378
21.076853	1058.757883	12.121383
20.983386	1060.321563	12.126387
20.915341	1051.752311	12.131392
20.816057	1062.128923	12.136397
21.315237	1064.172928	12.141402
20.886957	1060.874211	12.146407
20.676895	1067.555231	12.151411
21.160747	1064.438276	12.156416
21.133739	1057.863807	12.161421
20.951239	1058.573497	12.166426
20.966968	1057.591681	12.171431
21.144348	1063.439704	12.176435
21.207289	1060.033462	12.181440
20.971947	1065.527020	12.186445
21.017431	1066.357269	12.191450
21.024397	1057.671961	12.196455
20.812578	1069.483546	12.201459
21.048862	1065.067125	12.206464
20.890483	1069.956210	12.211469
21.234369	1060.471986	12.216474
21.251222	1068.892621	12.221479
21.141178	1067.187264	12.226483
21.006471	1069.530299	12.231488
21.072175	1070.577327	12.236493
21.178419	1064.499677	12.241498
20.953390	1069.176234	12.246503
21.098014	1069.120903	12.251507
21.446094	1068.091596	12.256512
21.184280	1072.968004	12.261517
21.175899	1080.130995	12.266522
20.946064	1069.875601	12.271527
20.715823	1075.045833	12.276531
21.111534	1067.255023	12.281536
20.748632	1075.969642	12.286541
21.079623	1065.042064	12.291546
21.038176	1071.707232	12.296551
21.113995	1078.407320	12.301555
21.270919	1075.758861	12.306560
21.018658	1079.735592	12.311565
21.074843	1068.055410	12.316570
20.824798	1062.505350	12.321575
21.225403	1064.576117	12.326579
21.058055	1047.265109	12.331584
20.626842	1048.412684	12.336589
21.289075	1061.333121	12.341594
21.124220	1055.053476	12.346599
20.835168	1040.729187	12.351603
21.295457	1041.226746	12.356608
21.072543	1047.635393	12.361613
20.909495	1041.086572	12.366618
20.932232	1047.996981	12.371623
20.839606	1045.818087	12.376627
20.998453	1034.086073	12.381632
20.711743	1045.832306	12.386637
21.342429	1062.124077	12.391642
21.309402	1048.626346	12.396647
21.000444	1047.183762	12.401651
21.216946	1044.356269	12.406656
20.912974	1040.296496	12.411661
21.130163	1031.490145	12.416666
20.832187	1041.793558	12.421671
20.856955	1046.861600	12.426675
21.078266	1041.683473	12.431680
21.150570	1043.835777	12.436685
21.032741	1034.180763	12.441690
20.832771	1039.147440	12.446695
21.051987	1044.547198	12.451699
21.077614	1034.738404	12.456704
20.931547	1043.186587	12.461709
20.931961	1035.790032	12.466714
20.829604	1048.355338	12.471719
20.940040	1047.031959	12.476723
21.052574	1037.595689	12.481728
20.794030	1052.326810	12.486733
20.789277	1047.822672	12.491738
21.013092	1057.361567	12.496743
20.891182	1076.103546	12.501747
21.395036	1074.767882	12.506752
20.935101	1066.365216	12.511757
21.631988	1046.527856	12.516762
21.182548	1043.200976	12.521767
21.029930	1050.468967	12.526771
21.287645	1044.433403	12.531776
21.233642	1056.546264	12.536781
21.095180	1046.068137	12.541786
21.166630	1047.045644	12.546791
21.071483	1058.559465	12.551795
21.404857	1050.193506	12.556800
21.230793	1049.229345	12.561805
21.198384	1052.071769	12.566810
20.956670	1038.836011	12.571815
20.815795	1029.544253	12.576819
21.496010	1025.094099	12.581824
20.872688	1026.064138	12.586829
20.650978	1015.840605	12.591834
20.985677	1027.678537	12.596839
21.062221	1039.450413	12.601843
21.064125	1034.733099	12.606848
20.835322	1041.426558	12.611853
20.984148	1046.110505	12.616858
20.954091	1046.624766	12.621863
21.096848	1055.567832	12.626867
21.317757	1037.424499	12.631872
21.011050	1042.444476	12.636877
20.869363	1020.808966	12.641882
21.105016	1014.879444	12.646887
20.857090	1018.459618	12.651891
21.310506	1019.497636	12.656896
21.160132	1022.130192	12.661901
21.351387	1026.703277	12.666906
21.205311	1020.355203	12.671911
20.851888	1018.408738	12.676915
21.296850	1013.745353	12.681920
21.160681	1017.069561	12.686925
21.048994	1020.322050	12.691930
21.159919	1023.195229	12.696935
21.209952	1027.005448	12.701939
20.837070	1018.753731	12.706944
20.407350	1027.513675	12.711949
21.220453	1030.278012	12.716954
21.028517	1030.475864	12.721959
20.804855	1031.847400	12.726963
20.965499	1014.923335	12.731968
20.629148	1024.135203	12.736973
21.143263	1028.230979	12.741978
21.100223	1018.797456	12.746983
20.723678	1030.904965	12.751987
21.121652	1027.089659	12.756992
21.150398	1031.065715	12.761997
20.944295	1021.877414	12.767002
21.145343	1023.952405	12.772007
20.895855	1026.197035	12.777011
20.943134	1024.306517	12.782016
20.644234	1032.309097	12.787021
20.726375	1030.663775	12.792026
20.642169	1030.536911	12.797031
21.037564	1035.566337	12.802035
21.114911	1035.014702	12.807040
20.820992	1037.936684	12.812045
21.055067	1036.866422	12.817050
21.111317	1041.129856	12.822055
20.865223	1034.529623	12.827059
20.949507	1032.106453	12.832064
21.157096	1050.187088	12.837069
21.254611	1038.823641	12.842074
21.270042	1033.356628	12.847079
21.022987	1034.383359	12.852083
21.140477	1022.372497	12.857088
21.047758	1028.973277	12.862093
21.076350	1022.076904	12.867098
21.168236	1030.348342	12.872103
20.876283	1033.995471	12.877107
20.952869	1033.361949	12.882112
20.928801	1037.142986	12.887117
21.039705	1035.111419	12.892122
21.046808	1034.858019	12.897127
21.026759	1035.017416	12.902131
21.462601	1030.596775	12.907136
21.235734	1041.759399	12.912141
21.023697	1035.390298	12.917146
21.267160	1033.671931	12.922151
21.231848	1040.913322	12.927155
21.300907	1034.407915	12.932160
21.097787	1035.508069	12.937165
21.156307	1021.522635	12.942170
21.096049	1018.431756	12.947175
20.826312	1008.163845	12.952179
20.933952	999.969548	12.957184
20.975302	1028.043071	12.962189
21.376744	1022.676934	12.967194
21.280909	1011.785144	12.972199
20.833715	998.886573	12.977203
20.988434	1003.280959	12.982208
20.870748	1003.284026	12.987213
20.842502	998.585726	12.992218
20.916972	1013.499468	12.997223
20.771761	1003.374138	13.002227
21.114157	1014.657275	13.007232
20.877280	1040.988359	13.012237
21.206464	1034.034573	13.017242
21.015393	1020.581001	13.022247
21.195367	1020.030346	13.027251
21.029200	1009.569281	13.032256
21.160066	1010.613009	13.037261
21.241715	1003.544164	13.042266
20.905401	1008.996242	13.047271
20.832005	1017.172599	13.052275
21.012486	1005.981253	13.057280
20.907719	1013.560165	13.062285
21.175937	1019.994553	13.067290
21.188555	1011.384860	13.072295
21.182695	1014.727710	13.077299
21.024002	1008.985679	13.082304
21.016755	1016.897574	13.087309
21.040876	1006.902943	13.092314
21.112723	1013.450657	13.097319
21.153519	1017.680276	13.102323
21.158641	1009.320960	13.107328
21.192090	1012.342123	13.112333
21.088898	1008.893787	13.117338
21.329547	1005.269174	13.122343
21.098499	1004.255753	13.127347
21.212496	1013.581881	13.132352
20.770103	1020.560155	13.137357
21.160597	1010.802001	13.142362
20.959357	1013.989918	13.147367
20.823813	1012.664771	13.152371
21.042680	1011.188470	13.157376
20.922874	1011.934684	13.162381
20.729955	1019.792609	13.167386
21.251741	1012.265596	13.172391
21.026894	1021.603192	13.177395
21.358253	1018.758961	13.182400
20.723991	1019.028940	13.187405
21.366192	1014.170079	13.192410
21.190543	1014.373218	13.197415
20.854806	1001.672929	13.202419
20.963407	994.492548	13.207424
20.667636	998.988750	13.212429
21.127338	1006.543864	13.217434
21.158273	1014.608954	13.222439
20.936418	1010.774233	13.227443
21.403110	1005.273105	13.232448
20.800882	1000.199536	13.237453
21.071058	988.858267	13.242458
21.321193	984.435719	13.247463
21.146577	994.180059	13.252467
20.854330	982.228275	13.257472
20.833325	992.474859	13.262477
20.596248	990.725902	13.267482
20.855828	994.204621	13.272487
20.964812	1006.188934	13.277491
21.112728	1003.613681	13.282496
20.981352	1021.889494	13.287501
21.096745	1021.696099	13.292506
21.063764	1015.533433	13.297511
21.118554	1018.306745	13.302515
21.141375	1005.344242	13.307520
21.077082	1008.366800	13.312525
20.990996	1009.853597	13.317530
21.237455	998.658041	13.322535
20.913301	1007.901072	13.327539
21.333256	1000.399769	13.332544
20.894657	1012.736376	13.337549
21.087893	1005.668658	13.342554
21.159549	1007.568725	13.347559
21.101312	1008.820825	13.352563
21.145874	996.238095	13.357568
21.311871	998.353368	13.362573
21.336628	998.500887	13.367578
21.217162	995.029917	13.372583
20.893352	995.111595	13.377587
21.528996	995.253149	13.382592
20.903447	994.660649	13.387597
21.051896	983.873432	13.392602
21.375672	993.752763	13.397607
20.635065	979.907444	13.402611
20.997260	985.875782	13.407616
20.991970	992.057290	13.412621
20.810946	990.531223	13.417626
20.716071	1000.398479	13.422631
20.755784	1002.568591	13.427635
20.920345	998.221193	13.432640
20.837129	1011.403210	13.437645
21.061221	994.606255	13.442650
21.038399	1002.668873	13.447655
20.773924	1005.407942	13.452659
20.766958	1006.724411	13.457664
20.785821	1014.569057	13.462669
21.186357	1011.808419	13.467674
20.992554	1008.664720	13.472679
20.927908	1012.221967	13.477683
21.041066	1006.775651	13.482688
20.913449	1016.887857	13.487693
21.049556	1014.926396	13.492698
20.920917	1017.949757	13.497703
20.825979	1025.443521	13.502707
21.043966	1017.897145	13.507712
20.739420	1017.176168	13.512717
20.912704	1010.718808	13.517722
20.696392	1008.359358	13.522727
20.879752	1005.147617	13.527731
20.899830	991.404906	13.532736
20.810506	1007.671095	13.537741
20.805977	1022.572213	13.542746
21.121244	1037.938047	13.547751
21.117344	1033.374637	13.552755
21.496530	1025.941330	13.557760
21.109683	1016.633614	13.562765
20.984396	1002.235930	13.567770
20.987476	998.204472	13.572775
20.721035	1001.453253	13.577779
21.145573	995.646589	13.582784
21.003951	1001.062880	13.587789
20.911883	996.805304	13.592794
21.168559	998.513420	13.597799
20.928773	1010.741038	13.602803
20.759915	996.952756	13.607808
20.616762	1012.093611	13.612813
21.010204	1025.016671	13.617818
21.141340	1037.992620	13.622823
21.080573	1039.376025	13.627827
21.386837	1025.188632	13.632832
21.307235	1021.788574	13.637837
20.869093	1007.516485	13.642842
21.294942	1007.128481	13.647847
20.981261	1007.907194	13.652851
21.337749	1008.946477	13.657856
21.039900	1007.951596	13.662861
21.129083	1007.978442	13.667866
21.085593	1005.397446	13.672871
20.988397	1008.907840	13.677875
21.206254	1007.728194	13.682880
21.097154	1004.594642	13.687885
20.900159	1007.521661	13.692890
21.032427	1007.675688	13.697895
20.648413	1023.695560	13.702899
21.049464	1016.452752	13.707904
20.894826	1016.908029	13.712909
21.125474	1017.327086	13.717914
21.174416	1009.214692	13.722919
20.940889	1013.193148	13.727923
21.220928	1002.951102	13.732928
21.275381	1009.938443	13.737933
20.875530	1007.993076	13.742938
21.278899	1005.877015	13.747943
21.020226	1018.336329	13.752947
21.347157	1006.156446	13.757952
21.196234	1009.621789	13.762957
21.099929	992.036930	13.767962
21.129449	976.329256	13.772967
20.824366	980.123558	13.777971
20.735843	977.899861	13.782976
20.530829	984.338745	13.787981
20.657106	1000.974272	13.792986
21.102967	1006.052414	13.797991
21.165926	1011.257867	13.802995
21.194958	1007.395747	13.808000
21.115037	1020.522048	13.813005
21.009830	1007.786561	13.818010
20.886845	1014.584567	13.823015
20.854293	1021.346072	13.828019
21.073559	1009.393112	13.833024
21.330489	1008.249814	13.838029
20.997945	1010.457223	13.843034
21.085950	1013.502803	13.848039
21.091789	1010.227905	13.853043
20.732363	988.994633	13.858048
21.061027	1009.977457	13.863053
20.915653	1011.204028	13.868058
21.350703	1015.388112	13.873063
21.027777	1003.023275	13.878067
20.973893	981.635615	13.883072
20.852944	991.518063	13.888077
20.756509	984.004507	13.893082
21.348573	999.575331	13.898087
20.972293	1001.409637	13.903091
20.849754	996.423576	13.908096
20.945213	1005.451432	13.913101
21.211243	1009.031637	13.918106
21.067630	997.718509	13.923111
20.703338	991.261738	13.928115
20.899020	997.764461	13.933120
21.052605	1011.280900	13.938125
21.041781	1015.976107	13.943130
21.163538	1013.543809	13.948135
20.850380	1009.827739	13.953139
21.063364	1013.563074	13.958144
20.637296	1015.553569	13.963149
21.032476	1019.673043	13.968154
21.131771	1017.954017	13.973159
21.152076	1029.783745	13.978163
21.080427	1014.333460	13.983168
21.051261	1006.091588	13.988173
20.899538	1000.895697	13.993178
21.081953	1002.819102	13.998183
21.024168	991.044398	14.003187
21.191935	990.478343	14.008192
20.939613	988.443527	14.013210
20.691319	999.689695	14.018227
21.030439	999.815001	14.023245
20.810936	1011.753454	14.028263
21.079540	1021.476267	14.033280
21.216063	1028.215596	14.038298
21.251472	1023.210811	14.043315
21.379466	1017.022474	14.048333
21.030205	1021.223275	14.053351
21.197133	1010.205712	14.058368
20.977597	1008.652000	14.063386
21.347967	1014.362994	14.068403
21.437347	1021.135008	14.073421
21.251434	1014.183465	14.078439
21.099477	996.403832	14.083456
20.970220	1010.703214	14.088474
21.096385	1020.826281	14.093491
21.253489	1025.924766	14.098509
21.459453	1025.928162	14.103527
21.401374	1017.317093	14.108544
21.422363	1020.618823	14.113562
21.366338	1028.590685	14.118579
21.627351	1017.812947	14.123597
21.450474	1037.790852	14.128615
21.280441	1031.396780	14.133632
21.511021	1026.107601	14.138650
21.296606	1024.180254	14.143667
21.638291	1027.808370	14.148685
21.242134	1035.360994	14.153703
21.295766	1029.824750	14.158720
21.234557	1028.418820	14.163738
21.092924	1031.925820	14.168755
21.549618	1029.938623	14.173773
21.290865	1029.948499	14.178791
21.661936	1023.520036	14.183808
21.337013	1030.235436	14.188826
21.257858	1033.861462	14.193843
21.355832	1042.384513	14.198861
21.286778	1055.326217	14.203879
21.401924	1056.295806	14.208896
21.356440	1059.375333	14.213914
21.757099	1063.510019	14.218931
21.826127	1053.112097	14.223949
21.446724	1067.283115	14.228967
21.591236	1054.532424	14.233984
21.471639	1064.041896	14.239002
21.324498	1074.663209	14.244019
21.621717	1082.886295	14.249037
21.600843	1086.836530	14.254055
21.942516	1085.560610	14.259072
21.893763	1094.825202	14.264090
21.763790	1100.360409	14.269107
22.181045	1091.660110	14.274125
21.714021	1101.951781	14.279143
21.966078	1097.358382	14.284160
22.184170	1101.145447	14.289178
22.024018	1098.241994	14.294195
22.194825	1099.814634	14.299213
21.683259	1088.965007	14.304231
22.052581	1085.187424	14.309248
22.051793	1093.172535	14.314266
22.108114	1093.411378	14.319283
22.066981	1086.205466	14.324301
22.130184	1088.326179	14.329319
21.983759	1083.089246	14.334336
21.967041	1086.898815	14.339354
21.859129	1091.013162	14.344371
22.315221	1083.788508	14.349389
21.869160	1093.090513	14.354407
22.145815	1089.389059	14.359424
22.287757	1090.380332	14.364442
22.143361	1100.534024	14.369459
22.306508	1096.478640	14.374477
22.060472	1117.840192	14.379495
22.639944	1116.940060	14.384512
22.816906	1117.804623	14.389530
22.524989	1099.123792	14.394547
22.541733	1090.393777	14.399565
22.359628	1103.520301	14.404583
22.362167	1096.616528	14.409600
22.428030	1098.400180	14.414618
22.298911	1097.716891	14.419635
22.424469	1093.989984	14.424653
22.414351	1108.725864	14.429671
22.713309	1109.393211	14.434688
22.364687	1096.617314	14.439706
22.296052	1116.309067	14.444723
22.875227	1124.476980	14.449741
22.635330	1129.148808	14.454759
22.657899	1118.979268	14.459776
22.691347	1116.944732	14.464794
22.654442	1123.027479	14.469811
22.556580	1113.145360	14.474829
22.556728	1125.866871	14.479847
22.663866	1124.198905	14.484864
22.571731	1121.641687	14.489882
22.647926	1126.236357	14.494899
22.894559	1118.784749	14.499917
22.851311	1129.555492	14.504935
23.150015	1121.990968	14.509952
23.008803	1115.010224	14.514970
22.919459	1135.304647	14.519987
22.913009	1133.404678	14.525005
23.068619	1132.152925	14.530023
23.079158	1124.208058	14.535040
22.968929	1126.907016	14.540058
23.143144	1129.472514	14.545075
23.277026	1125.444600	14.550093
22.962747	1116.026447	14.555111
22.830421	1104.198431	14.560128
23.331364	1113.958183	14.565146
22.716167	1106.246841	14.570163
22.925842	1115.401798	14.575181
22.960900	1130.623654	14.580199
22.881238	1121.477974	14.585216
23.069331	1127.634951	14.590234
22.915904	1126.850928	14.595251
23.271473	1124.220729	14.600269
23.333359	1127.106959	14.605287
23.344013	1130.065858	14.610304
23.327552	1122.406880	14.615322
23.048053	1127.995049	14.620339
23.485801	1121.487480	14.625357
23.057729	1124.455790	14.630375
23.194176	1120.233193	14.635392
23.290944	1128.124109	14.640410
23.018620	1128.996623	14.645427
23.229456	1119.159648	14.650445
22.941765	1127.311665	14.655463
23.276402	1125.622358	14.660480
23.365118	1126.017275	14.665498
23.221611	1128.668056	14.670515
23.488064	1136.734840	14.675533
23.887608	1151.185192	14.680551
23.447122	1142.185142	14.685568
23.860462	1132.038997	14.690586
23.381898	1136.417762	14.695603
22.975951	1123.097262	14.700621
23.421229	1138.417297	14.705639
23.511590	1158.476230	14.710656
23.893479	1149.206577	14.715674
24.011421	1164.408171	14.720691
23.995732	1158.041336	14.725709
24.110705	1145.735740	14.730727
23.744210	1129.259638	14.735744
23.692493	1120.856712	14.740762
23.565892	1131.127140	14.745779
23.829473	1114.003129	14.750797
23.578958	1132.299493	14.755815
23.659819	1138.440543	14.760832
24.393758	1142.320742	14.765850
23.691538	1135.969818	14.770867
23.470182	1135.937549	14.775885
24.276434	1139.807785	14.780903
23.837295	1149.691547	14.785920
24.046149	1149.014126	14.790938
23.981452	1157.814882	14.795955
24.185474	1153.380144	14.800973
23.972656	1137.947642	14.805991
23.748103	1132.909562	14.811008
24.030304	1138.044764	14.816026
23.683313	1159.722151	14.821043
23.781405	1154.527992	14.826061
23.794580	1156.129713	14.831079
23.845428	1162.199266	14.836096
24.232332	1155.179888	14.841114
23.918482	1162.341910	14.846131
23.843321	1148.835702	14.851149
24.044958	1151.707513	14.856167
23.796384	1159.677124	14.861184
24.148204	1171.348396	14.866202
24.432319	1187.124426	14.871219
24.758616	1183.304915	14.876237
24.336418	1168.749735	14.881255
24.293464	1158.146222	14.886272
24.375324	1159.083374	14.891290
24.196567	1162.208561	14.896307
24.396225	1171.771793	14.901325
24.234212	1181.534294	14.906343
24.432773	1185.374048	14.911360
24.541123	1180.640731	14.916378
24.443688	1188.574453	14.921395
24.367623	1177.668669	14.926413
24.380519	1187.079221	14.931431
24.480912	1184.554994	14.936448
24.711946	1182.278928	14.941466
24.455283	1191.421793	14.946483
24.810335	1178.503702	14.951501
24.864964	1181.306941	14.956519
24.730538	1191.123252	14.961536
25.049066	1181.842448	14.966554
25.096937	1171.495796	14.971571
24.597356	1158.472565	14.976589
24.891150	1155.892327	14.981607
24.916685	1153.538926	14.986624
24.887182	1154.560695	14.991642
24.853818	1163.896024	14.996659
24.827382	1152.884812	15.001677
25.212271	1151.385696	15.006695
24.619321	1153.037685	15.011712
24.889722	1145.278670	15.016730
24.586578	1152.220321	15.021747
24.953537	1150.804291	15.026765
24.685123	1149.439263	15.031783
24.968566	1161.311777	15.036800
25.062230	1160.366428	15.041818
24.933733	1177.200871	15.046835
24.863006	1177.902802	15.051853
25.444551	1176.340856	15.056871
24.750812	1185.444886	15.061888
25.144244	1174.694678	15.066906
25.087908	1183.136240	15.071923
25.010167	1178.462493	15.076941
24.905594	1173.821342	15.081959
24.742420	1180.415840	15.086976
25.212246	1169.629855	15.091994
25.144818	1183.798418	15.097011
24.909653	1180.065313	15.102029
25.093472	1174.236893	15.107047
25.103420	1174.572800	15.112064
25.373294	1172.538301	15.117082
25.162308	1171.560528	15.122099
25.253008	1166.489458	15.127117
25.412227	1180.702096	15.132135
25.411661	1190.813246	15.137152
25.546022	1188.524283	15.142170
24.872082	1195.941962	15.147187
25.406870	1201.212299	15.152205
25.755209	1210.777799	15.157223
25.637437	1213.823268	15.162240
25.726207	1209.214978	15.167258
25.578853	1206.612281	15.172275
25.508765	1203.883212	15.177293
25.635317	1204.810092	15.182311
25.685050	1215.032791	15.187328
25.899330	1202.445456	15.192346
25.657073	1193.451510	15.197363
25.618461	1188.580389	15.202381
25.942946	1201.052026	15.207399
25.727618	1196.802927	15.212416
25.723629	1178.863399	15.217434
25.763170	1195.911744	15.222451
25.828122	1192.922817	15.227469
25.776963	1208.293005	15.232487
25.413836	1210.096328	15.237504
26.036981	1202.133151	15.242522
25.813937	1213.269272	15.247539
25.703080	1216.916131	15.252557
25.966997	1209.137666	15.257575
25.688262	1217.252909	15.262592
25.918968	1219.169953	15.267610
25.854821	1218.517982	15.272627
25.903592	1210.502473	15.277645
26.184977	1209.494145	15.282663
25.751934	1213.824772	15.287680
25.982737	1208.209076	15.292698
25.961964	1208.313921	15.297715
25.767841	1211.329094	15.302733
26.292154	1218.934782	15.307751
26.285071	1214.300092	15.312768
26.089002	1209.184293	15.317786
26.050879	1218.343444	15.322803
26.520253	1223.020944	15.327821
26.329531	1230.729672	15.332839
26.273576	1225.051951	15.337856
26.362555	1215.202885	15.342874
26.401830	1228.961988	15.347891
26.413586	1236.406394	15.352909
26.465229	1237.579614	15.357927
26.398354	1238.600271	15.362944
26.573877	1233.034283	15.367962
26.426554	1220.534496	15.372979
26.366631	1229.486337	15.377997
26.588444	1226.414179	15.383015
26.710493	1245.245103	15.388032
26.724356	1227.338062	15.393050
26.745178	1214.891688	15.398067
26.525114	1206.738155	15.403085
26.768868	1204.891869	15.408103
26.355638	1212.437868	15.413120
26.615738	1212.904557	15.418138
26.616336	1220.021172	15.423155
26.591458	1237.424347	15.428173
26.886874	1241.010346	15.433191
26.600929	1241.581432	15.438208
26.810649	1229.751457	15.443226
27.088186	1239.500521	15.448243
26.893912	1236.585965	15.453261
27.252292	1232.175349	15.458279
26.545396	1224.270920	15.463296
26.601199	1230.220157	15.468314
27.014555	1233.606438	15.473331
27.077680	1233.386429	15.478349
27.205060	1240.447439	15.483367
26.958387	1241.833414	15.488384
27.119833	1235.439867	15.493402
26.861372	1239.916482	15.498419
26.857722	1237.466258	15.503437
27.412302	1236.149289	15.508455
27.136413	1238.717381	15.513472
27.106846	1236.143084	15.518490
27.132794	1240.549168	15.523507
26.975385	1238.406624	15.528525
27.085858	1234.152743	15.533543
27.127366	1242.066693	15.538560
27.235283	1224.451406	15.543578
27.217968	1240.243323	15.548595
26.855216	1247.628699	15.553613
27.004923	1238.093989	15.558631
26.988999	1238.238174	15.563648
27.161163	1232.839470	15.568666
27.053000	1243.483005	15.573683
27.335860	1266.094397	15.578701
27.597842	1263.713492	15.583719
27.847155	1265.756568	15.588736
27.636460	1250.791602	15.593754
27.670789	1244.961828	15.598771
27.636645	1248.090711	15.603789
27.892893	1229.777690	15.608807
27.722370	1232.730899	15.613824
27.338494	1222.879380	15.618842
27.549372	1226.529984	15.623859
27.434074	1234.441410	15.628877
27.948174	1247.682760	15.633895
27.859870	1257.781209	15.638912
28.284750	1233.863894	15.643930
28.110581	1225.106043	15.648947
27.927435	1227.487874	15.653965
27.747709	1219.763645	15.658983
27.822003	1224.781022	15.664000
27.985152	1219.501743	15.669018
28.169358	1216.786384	15.674035
27.673792	1216.128501	15.679053
27.936891	1212.054784	15.684071
27.727081	1230.217358	15.689088
27.814486	1227.679465	15.694106
27.745726	1220.475533	15.699123
27.495636	1225.805781	15.704141
28.072938	1229.459293	15.709159
28.013663	1253.430898	15.714176
28.057488	1259.065866	15.719194
28.242967	1263.039868	15.724211
27.873052	1270.193580	15.729229
28.537781	1259.562854	15.734247
28.344866	1263.203935	15.739264
28.406392	1258.021865	15.744282
28.268306	1264.761057	15.749299
27.959114	1266.081497	15.754317
28.408210	1262.100015	15.759335
28.252118	1264.114939	15.764352
28.327864	1265.700400	15.769370
28.551180	1265.281015	15.774387
28.009615	1260.453907	15.779405
28.339165	1257.873454	15.784423
28.346093	1260.323293	15.789440
28.298218	1263.329308	15.794458
28.562333	1258.950236	15.799475
28.603574	1257.420973	15.804493
28.350020	1250.764834	15.809511
28.013191	1266.877526	15.814528
28.494260	1261.232119	15.819546
28.478353	1263.811448	15.824563
28.279331	1266.857302	15.829581
28.655151	1280.344903	15.834599
28.557752	1283.294324	15.839616
28.689662	1284.724532	15.844634
28.715314	1285.886957	15.849651
28.617143	1293.700511	15.854669
29.011414	1291.542331	15.859687
28.698940	1290.447810	15.864704
29.042590	1287.434863	15.869722
29.122767	1289.694477	15.874739
28.768503	1282.978876	15.879757
29.078372	1281.908583	15.884775
28.992521	1289.519601	15.889792
28.831148	1287.223519	15.894810
28.829752	1285.051365	15.899827
29.138861	1286.362857	15.904845
29.244251	1277.502969	15.909863
29.125715	1279.239759	15.914880
29.413422	1289.590517	15.919898
29.528468	1285.798381	15.924915
29.423473	1281.790434	15.929933
29.495694	1273.945764	15.934951
29.158951	1277.613721	15.939968
29.142958	1281.553792	15.944986
29.395849	1281.873762	15.950003
29.233627	1273.478148	15.955021
29.300628	1277.235086	15.960039
29.410829	1279.552048	15.965056
29.457518	1280.847976	15.970074
29.517887	1277.419296	15.975091
29.442607	1282.554935	15.980109
29.771524	1269.859592	15.985127
29.152548	1264.135582	15.990144
29.204503	1275.917690	15.995162
29.198866	1272.785842	16.000179
29.444154	1276.007022	16.005197
29.511282	1275.879973	16.010215
29.681531	1273.387850	16.015232
29.746680	1287.337159	16.020250
29.846226	1288.564093	16.025267
29.589808	1298.554097	16.030285
29.825065	1284.968362	16.035303
29.692482	1295.677181	16.040320
29.699558	1292.979834	16.045338
30.011029	1288.253413	16.050355
29.808467	1294.197478	16.055373
29.525479	1286.585641	16.060391
29.424959	1281.953248	16.065408
29.730334	1281.538865	16.070426
29.695893	1281.423297	16.075443
29.457129	1286.824123	16.080461
29.824000	1299.103460	16.085479
29.754595	1310.108179	16.090496
29.912927	1309.670055	16.095514
30.078493	1310.579708	16.100531
29.834357	1311.808761	16.105549
29.973535	1308.383235	16.110567
29.714548	1317.340924	16.115584
29.845091	1308.534422	16.120602
30.291853	1300.712588	16.125619
30.066462	1322.780613	16.130637
30.336659	1320.270968	16.135655
30.734594	1319.955871	16.140672
30.438465	1318.710082	16.145690
30.719289	1319.797203	16.150707
30.632644	1326.148316	16.155725
30.615623	1323.029284	16.160743
30.744031	1323.612940	16.165760
30.453063	1325.626574	16.170778
30.527055	1320.024049	16.175795
30.598811	1323.965080	16.180813
30.885023	1314.425853	16.185831
30.789496	1308.382373	16.190848
30.620960	1321.860090	16.195866
30.730239	1318.189207	16.200883
30.210793	1316.767455	16.205901
30.564010	1305.418710	16.210919
30.709373	1302.471993	16.215936
30.525409	1304.857899	16.220954
30.788449	1297.188858	16.225971
30.654106	1301.946943	16.230989
30.721947	1306.894589	16.236007
30.804637	1306.579433	16.241024
30.739298	1308.962151	16.246042
30.919504	1304.927586	16.251059
30.451990	1301.142627	16.256077
30.858906	1306.917913	16.261095
30.546061	1302.685909	16.266112
30.588239	1299.737560	16.271130
30.767764	1295.502536	16.276147
31.055465	1326.795167	16.281165
31.193131	1335.511056	16.286183
31.304962	1329.206395	16.291200
30.781814	1324.771176	16.296218
31.252498	1325.027308	16.301235
31.212144	1321.560411	16.306253
31.142000	1321.375028	16.311271
31.092280	1322.250589	16.316288
31.508641	1332.184437	16.321306
31.583111	1330.782007	16.326323
31.153839	1328.142450	16.331341
31.242847	1325.640466	16.336359
31.348728	1324.656976	16.341376
31.296320	1330.835882	16.346394
31.478037	1323.282048	16.351411
31.657642	1323.852033	16.356429
31.746781	1327.308925	16.361447
31.698089	1322.933319	16.366464
31.520555	1327.884714	16.371482
31.579436	1327.943033	16.376499
31.563757	1331.407991	16.381517
31.413699	1336.584679	16.386535
31.554155	1327.532754	16.391552
31.399603	1328.438407	16.396570
31.535005	1330.737986	16.401587
31.601092	1337.112722	16.406605
31.710540	1329.493331	16.411623
31.534249	1330.099629	16.416640
31.121793	1333.988111	16.421658
31.952058	1326.166448	16.426675
31.788583	1330.742777	16.431693
31.680511	1342.474167	16.436711
31.960977	1349.031805	16.441728
32.092939	1359.005526	16.446746
32.553038	1350.685224	16.451763
32.168429	1336.997736	16.456781
32.072600	1326.486694	16.461799
31.799686	1319.607871	16.466816
31.858577	1334.423426	16.471834
32.257458	1341.300391	16.476851
32.430229	1358.381950	16.481869
32.081099	1346.337405	16.486887
32.665812	1338.790078	16.491904
32.351881	1328.810920	16.496922
32.192281	1323.822977	16.501939
32.251348	1322.369519	16.506957
32.441195	1318.503307	16.511975
32.467431	1322.474408	16.516992
32.149916	1329.006283	16.522010
32.522413	1330.309242	16.527027
32.146624	1334.035353	16.532045
32.033756	1338.259890	16.537063
32.490305	1345.166986	16.542080
32.303651	1347.930086	16.547098
32.414556	1340.566871	16.552115
32.359478	1349.559701	16.557133
32.698078	1344.364083	16.562151
32.753747	1349.290088	16.567168
32.404535	1347.217447	16.572186
32.603398	1340.769906	16.577203
32.633658	1350.955693	16.582221
32.425731	1353.943208	16.587239
32.849349	1343.037831	16.592256
32.709867	1342.036843	16.597274
32.978099	1340.051350	16.602291
32.892506	1347.266722	16.607309
32.802752	1347.247283	16.612327
33.066057	1356.418222	16.617344
33.134703	1357.687846	16.622362
32.962019	1349.131826	16.627379
33.275626	1347.334946	16.632397
32.977454	1343.022722	16.637415
33.074919	1335.095337	16.642432
33.024731	1350.220117	16.647450
33.600923	1355.590880	16.652467
33.314743	1346.647890	16.657485
32.839132	1350.196434	16.662503
32.820484	1347.078443	16.667520
33.193697	1366.998166	16.672538
33.470414	1360.774951	16.677555
33.711914	1369.747233	16.682573
33.510888	1377.050248	16.687591
33.792450	1363.486944	16.692608
33.304230	1356.590530	16.697626
33.449366	1346.605785	16.702643
33.240666	1351.993974	16.707661
33.641345	1364.769008	16.712679
33.702660	1354.986398	16.717696
33.759728	1367.640837	16.722714
33.663887	1355.913767	16.727731
33.647364	1361.888751	16.732749
33.644922	1364.994512	16.737767
33.632771	1368.037325	16.742784
33.663656	1369.889515	16.747802
34.059030	1363.622204	16.752819
34.080329	1372.613091	16.757837
33.653446	1368.803543	16.762855
33.874662	1355.573931	16.767872
33.305270	1370.718617	16.772890
33.692661	1365.463298	16.777907
33.824216	1363.746578	16.782925
34.130187	1362.444082	16.787943
33.966759	1358.327450	16.792960
33.678547	1363.542699	16.797978
33.825017	1357.692634	16.802995
33.930244	1360.165352	16.808013
33.730026	1363.780094	16.813031
33.838761	1354.781978	16.818048
33.414499	1380.241168	16.823066
33.924048	1391.796223	16.828083
34.060267	1390.398883	16.833101
34.155297	1400.934616	16.838119
34.375856	1394.857204	16.843136
34.280811	1404.082968	16.848154
33.937230	1402.090436	16.853171
34.090663	1396.769382	16.858189
33.990315	1405.413157	16.863207
34.677067	1418.088339	16.868224
34.931025	1435.272663	16.873242
34.993872	1424.400383	16.878259
34.966430	1406.292846	16.883277
34.424554	1408.053125	16.888295
34.717451	1400.708833	16.893312
34.756916	1406.797609	16.898330
34.748282	1406.973668	16.903347
34.807806	1406.060491	16.908365
34.858482	1408.704734	16.913383
35.051179	1405.449984	16.918400
35.030390	1410.500682	16.923418
34.824662	1401.533028	16.928435
35.384616	1401.973137	16.933453
34.921250	1406.653952	16.938471
34.907224	1405.150792	16.943488
34.937591	1415.175363	16.948506
34.840484	1407.827987	16.953523
35.076573	1400.381853	16.958541
34.874647	1400.426710	16.963559
35.218534	1395.846103	16.968576
35.026061	1408.652068	16.973594
35.279171	1406.193900	16.978611
35.383722	1404.767788	16.983629
35.222354	1407.377420	16.988647
35.087381	1406.927869	16.993664
35.197359	1403.433828	16.998682
35.197620	1402.444370	17.003699
35.050607	1406.694823	17.008717
34.959283	1410.281982	17.013735
35.215730	1420.003071	17.018752
35.239158	1424.536247	17.023770
35.533580	1427.195104	17.028787
35.561425	1431.193508	17.033805
35.266950	1438.505165	17.038823
35.694828	1434.700851	17.043840
35.395667	1442.957124	17.048858
35.307673	1439.036088	17.053875
35.691274	1427.223054	17.058893
35.153223	1435.493828	17.063911
35.743257	1430.985641	17.068928
35.511206	1433.584528	17.073946
35.514574	1431.581489	17.078963
35.979012	1438.863346	17.083981
35.808499	1451.634384	17.088999
36.178797	1442.743156	17.094016
35.935281	1434.396595	17.099034
36.027405	1422.254867	17.104051
36.052838	1417.595263	17.109069
35.775078	1415.585151	17.114087
36.257127	1423.270053	17.119104
36.309236	1433.592420	17.124122
36.151677	1426.734474	17.129139
35.998010	1417.675132	17.134157
36.098808	1435.477733	17.139175
36.102996	1442.080265	17.144192
36.351540	1445.311976	17.149210
36.327802	1444.982329	17.154227
36.398919	1443.740880	17.159245
36.061545	1452.031569	17.164263
36.034176	1452.279833	17.169280
35.994804	1451.015105	17.174298
36.431649	1447.171604	17.179315
36.540424	1444.270809	17.184333
36.178587	1447.769767	17.189351
36.327931	1448.648981	17.194368
36.026596	1445.424250	17.199386
36.379732	1468.692537	17.204403
36.846190	1467.993681	17.209421
36.389362	1476.303435	17.214439
36.669925	1474.110666	17.219456
36.641082	1470.435819	17.224474
36.510683	1471.671128	17.229491
36.580924	1479.143299	17.234509
36.763610	1486.135043	17.239527
37.034436	1474.074888	17.244544
36.834120	1472.908191	17.249562
36.521762	1478.995691	17.254579
37.261751	1470.121780	17.259597
36.764589	1484.141298	17.264615
36.690471	1476.429977	17.269632
37.024455	1485.630627	17.274650
37.028959	1500.371651	17.279667
37.305554	1504.193539	17.284685
37.106637	1504.598948	17.289703
37.205639	1499.272380	17.294720
37.340050	1505.544266	17.299738
37.197790	1508.743935	17.304755
37.900221	1501.382256	17.309773
37.641326	1504.022405	17.314791
37.440125	1499.269138	17.319808
37.747840	1479.332792	17.324826
37.288919	1479.728542	17.329843
37.288818	1475.592906	17.334861
37.283706	1495.055590	17.339879
37.757948	1501.034161	17.344896
37.961184	1495.359042	17.349914
37.765528	1501.902233	17.354931
37.842905	1480.096791	17.359949
37.452969	1478.150969	17.364967
37.455454	1470.097866	17.369984
37.653734	1484.243220	17.375002
37.478321	1497.048115	17.380019
37.772517	1498.826076	17.385037
37.980587	1505.525114	17.390055
38.063106	1499.318656	17.395072
37.942956	1505.952059	17.400090
37.724971	1504.469621	17.405107
38.017193	1496.927963	17.410125
38.142662	1499.513100	17.415143
37.961813	1504.549245	17.420160
38.085108	1498.117620	17.425178
37.954610	1501.963535	17.430195
37.951128	1506.644970	17.435213
37.738457	1500.803361	17.440231
37.968261	1504.118304	17.445248
38.240413	1519.599286	17.450266
38.074177	1534.504437	17.455283
38.506779	1528.480459	17.460301
38.406965	1532.615662	17.465319
38.424156	1526.903346	17.470336
38.689234	1523.558370	17.475354
38.440200	1532.183460	17.480371
38.491025	1529.678879	17.485389
38.319622	1535.176024	17.490407
38.778666	1538.335642	17.495424
38.835579	1530.300568	17.500442
38.808160	1533.085499	17.505459
38.491276	1522.632382	17.510477
38.395407	1525.716110	17.515495
38.628713	1527.419624	17.520512
38.826001	1525.835555	17.525530
38.607760	1529.663223	17.530547
38.864578	1528.983643	17.535565
38.775710	1532.538978	17.540583
39.083104	1521.710212	17.545600
39.167925	1525.560333	17.550618
38.823320	1527.560525	17.555635
39.016602	1520.966709	17.560653
39.204237	1522.927632	17.565671
38.866465	1515.806573	17.570688
39.217465	1517.700540	17.575706
39.065240	1531.072809	17.580723
39.271472	1550.409045	17.585741
39.220581	1555.516507	17.590759
39.445931	1555.734692	17.595776
39.628340	1556.997987	17.600794
39.433526	1554.873946	17.605811
39.623043	1541.673605	17.610829
39.369877	1529.472807	17.615847
39.139616	1535.506336	17.620864
39.467622	1531.613314	17.625882
39.493006	1550.420722	17.630899
39.516678	1550.894457	17.635917
39.457272	1568.902894	17.640935
39.531484	1558.049153	17.645952
39.656542	1548.948422	17.650970
39.428535	1556.491010	17.655987
39.539017	1553.470364	17.661005
39.757448	1558.017315	17.666023
39.596585	1567.240308	17.671040
39.936743	1560.941606	17.676058
39.809719	1564.445616	17.681075
39.837085	1569.169344	17.686093
40.039415	1575.951920	17.691111
39.968942	1579.951887	17.696128
40.217929	1586.217333	17.701146
40.172264	1595.716932	17.706163
40.576089	1582.828462	17.711181
40.231110	1573.080617	17.716199
39.883011	1577.908278	17.721216
40.154767	1574.297941	17.726234
40.302503	1587.469827	17.731251
40.537534	1589.026772	17.736269
40.396469	1595.337128	17.741287
40.532217	1595.893669	17.746304
40.918646	1582.280402	17.751322
40.659305	1578.200241	17.756339
40.749900	1568.378996	17.761357
40.814101	1562.845584	17.766375
40.423100	1562.498999	17.771392
40.905681	1553.398662	17.776410
40.436320	1559.747991	17.781427
40.300318	1557.154431	17.786445
40.716099	1558.161842	17.791463
40.630247	1575.612114	17.796480
41.335648	1582.244453	17.801498
41.031617	1579.392952	17.806515
40.639489	1568.443683	17.811533
40.723608	1570.896207	17.816551
40.958036	1583.217360	17.821568
41.083054	1585.259857	17.826586
41.106154	1582.905989	17.831603
41.205546	1575.761584	17.836621
41.120593	1589.386675	17.841639
41.019293	1584.691383	17.846656
41.401767	1574.609637	17.851674
41.171330	1585.828236	17.856691
41.081518	1584.656490	17.861709
41.417068	1579.189126	17.866727
41.013247	1583.492387	17.871744
41.161812	1578.172831	17.876762
41.307729	1586.715298	17.881779
41.339990	1584.024893	17.886797
41.320719	1575.693612	17.891815
41.344751	1574.389657	17.896832
41.485388	1573.697143	17.901850
41.220933	1577.363869	17.906867
41.157373	1588.123245	17.911885
41.606825	1595.981764	17.916903
41.662428	1607.169703	17.921920
41.707560	1602.212723	17.926938
41.895575	1604.834311	17.931955
41.911598	1599.661737	17.936973
41.456694	1603.797747	17.941991
41.679201	1599.711521	17.947008
41.810027	1594.186348	17.952026
41.882604	1601.816309	17.957043
41.814382	1599.941862	17.962061
42.060170	1599.979025	17.967079
41.841765	1602.814880	17.972096
42.154047	1614.138865	17.977114
42.133039	1631.832136	17.982131
42.208427	1636.434962	17.987149
42.122772	1633.886844	17.992167
42.296102	1627.982048	17.997184
42.170848	1625.105957	18.002202
42.325871	1629.703159	18.007219
42.250408	1626.487197	18.012237
42.428985	1622.480334	18.017255
42.230620	1619.576577	18.022272
42.451724	1618.849203	18.027290
42.437254	1619.248793	18.032307
42.757813	1621.727328	18.037325
42.560446	1625.927670	18.042343
42.463210	1623.690521	18.047360
42.688480	1612.957375	18.052378
42.377114	1629.834879	18.057395
42.617822	1646.187806	18.062413
42.690819	1647.027296	18.067431
42.838502	1649.203836	18.072448
43.413499	1639.211685	18.077466
43.313197	1645.314200	18.082483
43.512483	1635.787055	18.087501
43.621626	1626.181478	18.092519
43.253848	1609.105669	18.097536
43.602549	1594.800725	18.102554
43.596987	1602.633497	18.107571
43.490421	1607.144989	18.112589
43.453169	1598.972302	18.117607
43.387004	1606.290890	18.122624
43.883483	1598.309950	18.127642
44.075338	1600.043681	18.132659
43.715401	1585.858059	18.137677
43.799976	1565.461649	18.142695
43.347391	1569.769537	18.147712
43.290737	1562.677555	18.152730
43.330082	1568.952047	18.157747
43.265990	1589.134529	18.162765
43.652144	1591.952618	18.167783
43.298637	1604.962202	18.172800
43.643432	1600.269695	18.177818
43.558271	1609.284787	18.182835
43.621260	1600.664288	18.187853
43.596373	1593.455532	18.192871
43.298363	1603.635647	18.197888
43.774997	1596.173859	18.202906
43.621223	1609.422956	18.207923
43.555609	1625.756285	18.212941
43.747865	1625.649392	18.217959
43.843542	1636.448693	18.222976
43.899462	1636.076447	18.227994
43.848707	1639.745288	18.233011
43.957815	1628.961439	18.238029
44.039358	1631.626757	18.243047
43.952568	1651.727997	18.248064
44.387185	1650.066736	18.253082
44.330723	1654.994998	18.258099
44.128750	1655.089416	18.263117
44.510296	1651.350643	18.268135
44.742682	1656.927376	18.273152
44.474286	1644.395406	18.278170
44.716734	1654.424859	18.283187
44.596155	1653.081823	18.288205
45.169362	1642.120906	18.293223
44.947875	1649.618454	18.298240
45.066817	1653.485192	18.303258
44.770594	1643.716150	18.308275
44.516973	1646.964286	18.313293
45.053560	1649.626250	18.318311
45.003534	1649.727897	18.323328
44.876552	1644.541932	18.328346
44.701608	1645.542883	18.333363
44.583680	1653.724748	18.338381
45.049462	1643.013787	18.343399
44.914101	1656.678443	18.348416
44.916814	1653.204598	18.353434
45.242434	1652.948224	18.358451
45.153027	1673.319704	18.363469
45.424800	1680.779501	18.368487
45.219504	1683.444168	18.373504
45.830149	1682.248008	18.378522
45.572894	1681.148580	18.383539
45.538498	1671.109657	18.388557
45.634477	1660.522161	18.393575
45.376811	1668.664182	18.398592
45.769163	1671.950880	18.403610
45.716028	1679.224165	18.408627
45.182931	1672.542408	18.413645
45.525072	1670.647339	18.418663
45.569809	1683.528192	18.423680
45.691624	1683.043182	18.428698
45.850500	1670.726995	18.433715
45.753018	1670.089758	18.438733
45.915091	1675.092505	18.443751
45.852200	1681.141874	18.448768
45.687257	1679.299361	18.453786
46.184340	1675.339221	18.458803
45.489818	1679.313680	18.463821
45.626612	1689.374166	18.468839
45.848198	1700.237596	18.473856
45.895995	1703.555656	18.478874
45.905462	1708.316106	18.483891
45.993130	1716.478588	18.488909
46.210886	1714.677289	18.493927
46.037022	1722.657313	18.498944
46.191960	1729.851816	18.503962
46.292034	1733.989805	18.508979
46.453284	1739.009224	18.513997
47.095693	1735.247704	18.519015
46.840378	1750.904300	18.524032
46.889622	1742.182083	18.529050
47.164747	1733.487557	18.534067
46.599295	1722.878868	18.539085
46.983109	1715.714990	18.544103
46.663593	1707.988410	18.549120
46.892303	1722.834698	18.554138
47.099921	1726.546516	18.559155
46.925522	1740.259951	18.564173
47.152320	1735.841856	18.569191
47.115967	1736.155271	18.574208
47.290523	1735.788486	18.579226
47.237649	1730.353912	18.584243
46.866814	1732.667436	18.589261
47.017618	1730.121704	18.594279
47.130874	1740.144292	18.599296
47.058566	1741.993323	18.604314
47.338811	1737.853802	18.609331
47.022362	1735.329891	18.614349
47.409021	1732.475176	18.619367
47.126689	1739.818867	18.624384
47.168093	1733.124900	18.629402
47.373020	1748.303007	18.634419
47.529644	1764.025276	18.639437
47.523135	1764.675304	18.644455
47.471178	1768.930365	18.649472
47.711034	1765.660149	18.654490
48.321389	1753.839006	18.659507
48.201540	1756.307574	18.664525
47.986448	1754.110440	18.669543
48.007787	1753.195466	18.674560
48.016532	1757.817611	18.679578
48.479030	1753.331244	18.684595
48.255162	1755.811682	18.689613
48.877483	1744.331584	18.694631
48.271436	1736.120538	18.699648
48.110803	1725.281317	18.704666
48.323432	1722.634484	18.709683
48.177130	1730.711584	18.714701
48.179613	1712.810480	18.719719
48.106015	1726.462991	18.724736
48.391299	1741.779297	18.729754
48.684966	1754.244530	18.734771
48.356534	1753.865936	18.739789
48.361631	1746.779748	18.744807
48.459399	1753.183438	18.749824
48.501465	1741.794312	18.754842
48.695997	1748.099976	18.759859
48.451697	1748.295534	18.764877
48.355169	1738.822580	18.769895
48.193688	1746.504891	18.774912
48.377272	1760.778711	18.779930
48.788963	1777.870640	18.784947
48.838008	1782.994493	18.789965
49.355328	1777.940121	18.794983
49.123648	1777.479236	18.800000
49.088384	1783.528174	18.805018
49.029372	1780.005150	18.810035
48.864539	1779.221334	18.815053
48.871516	1776.674150	18.820071
49.127264	1778.876736	18.825088
49.077124	1769.297256	18.830106
49.307569	1775.364379	18.835123
49.286426	1792.030602	18.840141
49.446860	1795.829407	18.845159
49.653788	1800.593005	18.850176
49.584534	1812.586804	18.855194
49.809579	1802.213020	18.860211
49.531112	1804.922415	18.865229
49.744836	1798.158461	18.870247
49.635042	1811.248131	18.875264
49.755814	1800.035185	18.880282
50.293816	1793.199850	18.885299
50.013865	1793.232767	18.890317
50.191644	1796.607203	18.895335
50.178998	1793.010708	18.900352
50.006057	1795.890476	18.905370
50.162754	1785.652670	18.910387
49.914393	1796.920697	18.915405
50.214641	1784.645580	18.920423
50.395792	1793.991935	18.925440
50.466106	1793.977641	18.930458
50.127804	1785.153598	18.935475
50.226803	1784.769760	18.940493
50.232173	1783.426288	18.945511
50.147970	1789.752042	18.950528
50.070535	1787.053924	18.955546
50.505625	1779.781942	18.960563
50.107612	1786.324497	18.965581
50.528475	1799.376718	18.970599
50.682263	1810.784341	18.975616
50.788804	1823.598827	18.980634
51.115214	1816.009866	18.985651
51.155396	1816.095554	18.990669
50.947539	1804.158666	18.995687
51.191763	1788.123213	19.000704
50.856845	1785.249853	19.005722
50.984790	1777.945840	19.010739
50.885359	1790.106468	19.015757
50.908253	1800.379481	19.020775
51.245482	1808.411757	19.025792
51.417331	1812.156046	19.030810
51.629339	1805.532372	19.035827
51.680000	1806.978737	19.040845
51.444203	1784.430705	19.045863
51.302894	1766.468304	19.050880
51.236075	1771.078908	19.055898
51.355643	1782.624898	19.060915
51.245935	1800.506354	19.065933
51.657978	1797.376997	19.070951
51.998446	1810.354740	19.075968
51.877651	1811.789908	19.080986
51.989629	1805.286803	19.086003
51.534712	1813.085166	19.091021
51.721837	1809.690419	19.096039
51.729907	1807.950081	19.101056
51.593271	1806.300467	19.106074
51.542052	1811.898894	19.111091
51.480391	1804.999517	19.116109
51.689979	1805.737002	19.121127
51.959507	1826.469908	19.126144
52.101977	1835.327703	19.131162
52.719060	1826.885349	19.136179
52.318369	1837.476863	19.141197
52.164569	1840.900258	19.146215
52.472766	1832.595261	19.151232
52.291273	1837.346880	19.156250
52.629867	1827.310502	19.161267
52.381247	1834.038481	19.166285
52.291128	1841.938354	19.171303
52.641949	1836.770507	19.176320
52.126117	1833.435952	19.181338
52.660346	1829.868642	19.186355
52.568063	1834.890774	19.191373
52.578184	1854.666927	19.196391
53.259842	1859.200662	19.201408
52.638333	1868.229874	19.206426
53.146444	1861.144425	19.211443
53.143196	1865.471977	19.216461
53.094920	1865.378275	19.221479
53.283902	1864.098329	19.226496
52.843168	1862.712730	19.231514
53.294448	1856.780031	19.236531
53.190146	1856.618179	19.241549
53.289142	1855.010424	19.246567
53.340011	1856.141343	19.251584
53.259342	1863.266515	19.256602
53.308252	1867.366294	19.261619
53.028811	1862.922711	19.266637
53.453035	1863.509554	19.271655
53.323769	1856.845896	19.276672
52.792627	1870.549490	19.281690
53.590817	1879.514323	19.286707
53.631535	1891.102078	19.291725
53.657513	1896.702383	19.296743
53.860245	1890.596147	19.301760
53.639110	1895.078018	19.306778
53.810847	1886.683847	19.311795
53.720840	1889.487480	19.316813
53.833500	1895.497141	19.321831
54.302852	1907.743348	19.326848
54.185253	1915.414029	19.331866
54.404143	1921.764653	19.336883
54.076935	1930.592797	19.341901
54.060915	1925.950653	19.346919
54.694637	1924.325256	19.351936
54.304822	1933.202715	19.356954
54.413045	1922.541498	19.361971
54.350125	1928.629516	19.366989
54.547538	1926.890430	19.372007
54.704713	1918.397880	19.377024
54.588693	1933.525897	19.382042
54.611415	1919.435449	19.387059
54.619009	1915.953683	19.392077
54.716244	1917.016645	19.397095
54.866653	1924.932477	19.402112
54.655693	1918.919737	19.407130
54.799190	1928.689859	19.412147
55.007207	1939.203243	19.417165
54.995985	1939.604684	19.422183
55.694015	1946.438950	19.427200
55.614083	1945.057941	19.432218
55.495117	1924.017031	19.437235
55.406412	1918.690357	19.442253
55.317482	1916.166309	19.447271
55.390977	1901.485710	19.452288
55.439349	1916.251623	19.457306
55.580906	1926.500294	19.462323
55.362527	1935.420419	19.467341
55.351389	1934.463418	19.472359
55.616652	1925.963065	19.477376
55.615715	1939.099988	19.482394
55.844630	1937.652418	19.487411
56.057999	1927.746851	19.492429
55.719245	1929.436247	19.497447
55.770020	1931.943706	19.502464
55.678919	1933.940489	19.507482
55.614448	1927.600762	19.512499
55.450072	1935.962453	19.517517
55.803285	1954.270535	19.522535
56.037292	1958.652307	19.527552
56.270893	1966.112833	19.532570
56.153102	1960.528064	19.537587
56.421913	1960.198157	19.542605
56.195699	1961.287537	19.547623
56.394649	1959.685854	19.552640
56.447719	1962.409262	19.557658
56.678157	1957.424967	19.562675
56.794213	1965.680598	19.567693
56.917800	1969.912441	19.572711
57.004838	1964.265113	19.577728
56.647428	1973.285306	19.582746
56.792108	1971.415399	19.587763
56.939039	1969.829877	19.592781
56.739413	1967.572035	19.597799
56.704953	1969.938136	19.602816
56.509404	1977.508800	19.607834
56.862621	1985.964954	19.612851
57.175147	1998.204000	19.617869
57.185495	2000.399350	19.622887
57.511659	1990.745551	19.627904
57.267151	1989.998814	19.632922
57.327805	1980.000367	19.637939
57.501982	1978.997291	19.642957
57.562262	1978.184641	19.647975
57.598855	1976.322533	19.652992
57.545549	1986.310501	19.658010
57.287769	1982.279530	19.663027
57.545880	1978.463613	19.668045
57.368344	1979.673444	19.673063
57.722279	1975.961806	19.678080
57.554731	2000.207547	19.683098
57.517276	2015.730572	19.688115
58.088609	2018.772495	19.693133
58.189933	2011.181575	19.698151
58.194607	2008.430204	19.703168
58.159866	2009.990893	19.708186
58.168677	2005.895374	19.713203
58.307936	2012.242219	19.718221
57.989259	2021.673942	19.723239
58.316496	2020.246866	19.728256
58.152697	2014.184876	19.733274
58.448290	2016.376426	19.738291
58.584934	2010.678693	19.743309
57.936199	2017.828464	19.748327
58.157777	2020.115983	19.753344
58.664948	2028.030822	19.758362
58.851900	2035.993588	19.763379
59.127325	2024.419146	19.768397
59.134715	2029.865937	19.773415
59.536459	2021.446018	19.778432
59.256859	2023.380058	19.783450
59.230003	2030.231649	19.788467
59.109018	2014.706481	19.793485
59.101526	2002.068877	19.798503
59.305512	1997.768398	19.803520
59.382308	2005.178441	19.808538
59.623763	2006.904312	19.813555
59.286904	1995.857804	19.818573
59.219980	1999.389301	19.823591
59.234558	2000.102050	19.828608
59.613845	2017.090095	19.833626
59.375163	2012.434666	19.838643
59.657345	2007.862926	19.843661
59.532031	2019.828080	19.848679
59.916266	2012.081918	19.853696
59.833648	2009.840805	19.858714
59.615098	2004.234331	19.863731
59.646041	2008.471522	19.868749
59.676751	2011.830134	19.873767
60.140504	2011.658704	19.878784
59.997201	2009.016671	19.883802
59.973143	2010.395527	19.888819
60.103518	2005.580559	19.893837
60.099892	2009.247482	19.898855
60.283712	2017.034542	19.903872
60.084675	2038.502426	19.908890
60.463012	2037.232383	19.913907
60.700416	2042.636203	19.918925
60.285743	2050.979671	19.923943
60.626795	2039.712532	19.928960
60.584947	2038.494556	19.933978
60.424448	2033.585169	19.938995
60.758757	2030.070935	19.944013
60.593618	2039.578865	19.949031
60.884466	2035.424200	19.954048
60.727410	2038.843440	19.959066
60.741761	2044.824793	19.964083
60.714989	2052.779178	19.969101
60.581345	2071.208314	19.974119
61.228338	2064.297267	19.979136
61.470094	2065.571596	19.984154
61.259389	2069.007265	19.989171
61.350563	2066.947659	19.994189
61.265700	2061.950687	19.999207
61.078549	2064.175185	20.004224
61.444371	2062.170889	20.009242
61.317983	2057.291450	20.014259
61.956525	2068.116190	20.019277
61.885643	2067.791688	20.024295
61.430632	2057.213118	20.029312
61.976666	2073.985856	20.034330
61.755569	2082.083730	20.039347
62.188320	2082.106026	20.044365
62.097967	2084.193954	20.049383
62.084724	2077.806662	20.054400
62.430576	2087.593388	20.059418
62.224029	2078.569596	20.064435
62.536653	2083.292047	20.069453
62.266674	2081.720301	20.074471
62.671339	2075.046904	20.079488
62.550272	2078.111954	20.084506
62.362743	2058.742275	20.089523
62.649969	2068.700375	20.094541
62.251942	2072.747996	20.099559
62.591428	2071.247383	20.104576
62.675439	2080.041497	20.109594
62.509433	2085.935215	20.114611
62.787277	2078.094290	20.119629
62.319679	2086.580725	20.124647
62.508389	2084.500842	20.129664
62.588613	2073.175378	20.134682
62.570427	2090.283534	20.139699
62.942100	2105.278103	20.144717
63.252842	2103.004133	20.149735
63.259046	2104.091066	20.154752
63.172357	2100.626652	20.159770
62.847320	2111.057630	20.164787
63.393197	2105.912856	20.169805
63.092174	2109.510818	20.174823
63.470521	2104.544575	20.179840
63.348547	2104.055956	20.184858
63.565688	2132.781559	20.189875
63.801296	2135.990320	20.194893
63.651090	2138.874394	20.199911
63.808572	2129.933315	20.204928
63.900414	2136.714111	20.209946
63.771060	2146.176287	20.214963
64.471008	2125.547234	20.219981
64.313934	2138.837452	20.224999
64.097255	2132.847560	20.230016
64.424042	2132.124547	20.235034
64.172622	2131.980648	20.240051
64.356801	2126.918722	20.245069
64.198436	2140.933600	20.250087
64.308551	2129.880206	20.255104
64.384948	2130.509949	20.260122
63.893694	2132.965445	20.265139
64.271385	2138.846414	20.270157
64.368113	2157.927190	20.275175
64.640658	2166.740057	20.280192
65.229910	2164.844849	20.285210
64.854164	2167.136409	20.290227
64.862418	2158.960083	20.295245
65.041102	2168.381800	20.300263
64.994062	2159.021028	20.305280
65.042171	2163.110793	20.310298
64.762579	2167.477787	20.315315
65.013755	2164.340186	20.320333
65.046300	2172.309561	20.325351
64.971451	2176.761894	20.330368
65.049902	2182.900625	20.335386
65.222019	2191.190706	20.340403
65.306098	2186.339800	20.345421
65.536980	2190.556956	20.350439
65.527119	2192.589587	20.355456
65.568927	2201.299260	20.360474
65.476313	2222.818088	20.365491
65.759047	2214.965298	20.370509
65.917317	2210.990620	20.375527
65.816443	2216.701738	20.380544
66.208426	2215.714253	20.385562
66.221761	2222.004973	20.390579
66.206174	2217.936884	20.395597
65.971296	2216.120399	20.400615
66.264558	2221.870920	20.405632
66.556549	2213.539190	20.410650
66.356835	2221.243578	20.415667
66.608894	2213.078683	20.420685
66.205457	2216.685137	20.425703
66.287405	2215.064330	20.430720
66.536589	2226.031517	20.435738
66.524648	2248.453904	20.440755
66.524890	2236.411106	20.445773
66.286266	2243.963605	20.450791
66.402816	2246.558166	20.455808
66.278177	2242.715910	20.460826
66.243268	2270.385462	20.465843
66.943524	2272.705234	20.470861
66.660756	2272.027511	20.475879
66.893855	2275.351547	20.480896
67.458756	2288.201894	20.485914
67.336224	2298.404845	20.490931
67.342281	2299.715211	20.495949
67.604189	2301.258512	20.500967
67.782593	2297.565350	20.505984
68.039634	2296.632417	20.511002
67.780932	2307.512330	20.516019
68.149469	2295.263654	20.521037
68.289709	2297.678247	20.526055
67.747423	2281.383826	20.531072
67.773220	2276.181922	20.536090
68.125673	2287.072117	20.541107
68.195015	2292.238535	20.546125
68.232652	2303.576183	20.551143
68.097377	2296.143985	20.556160
68.574112	2297.280962	20.561178
68.427343	2294.950137	20.566195
68.780140	2300.396219	20.571213
68.278321	2299.132013	20.576231
68.357963	2296.082310	20.581248
68.998413	2292.984073	20.586266
68.553303	2303.075646	20.591283
68.734789	2300.871815	20.596301
68.588184	2295.828761	20.601319
68.671377	2294.786685	20.606336
69.072805	2290.582849	20.611354
68.773409	2285.538994	20.616371
68.951708	2286.932801	20.621389
69.030368	2295.222114	20.626407
68.968565	2305.764637	20.631424
68.884251	2314.703727	20.636442
69.173367	2325.514380	20.641459
69.609885	2321.096489	20.646477
69.633687	2325.075332	20.651495
69.571048	2327.031445	20.656512
69.923586	2310.710703	20.661530
69.432105	2323.329958	20.666547
69.848244	2314.079285	20.671565
70.100291	2313.332000	20.676583
69.870975	2308.003223	20.681600
70.046500	2300.056574	20.686618
70.058969	2311.354193	20.691635
70.241054	2303.319970	20.696653
70.481027	2308.552001	20.701671
70.431729	2305.072136	20.706688
70.563899	2295.088812	20.711706
70.216171	2299.237023	20.716723
70.118268	2302.905683	20.721741
70.092466	2304.461830	20.726759
70.312010	2306.167635	20.731776
70.345781	2298.736007	20.736794
70.163717	2311.704715	20.741811
70.818203	2323.064354	20.746829
70.636838	2328.816670	20.751847
70.751829	2336.243602	20.756864
71.120802	2325.808739	20.761882
71.125050	2331.091743	20.766899
71.205679	2332.704861	20.771917
71.121996	2329.603324	20.776935
71.362832	2335.993894	20.781952
71.673213	2321.981465	20.786970
71.541893	2325.792328	20.791987
71.349715	2325.760902	20.797005
71.729612	2327.100538	20.802023
71.501094	2331.642713	20.807040
71.990162	2323.963049	20.812058
71.557705	2321.026473	20.817075
71.603269	2320.354594	20.822093
71.867313	2317.442238	20.827111
71.490292	2329.026167	20.832128
71.445680	2318.445671	20.837146
71.333844	2339.528812	20.842163
71.524407	2343.279695	20.847181
71.867453	2338.883786	20.852199
71.330159	2353.179546	20.857216
71.878169	2368.252458	20.862234
72.063766	2377.066735	20.867251
72.538092	2385.569098	20.872269
72.669906	2376.127748	20.877287
72.270775	2381.803116	20.882304
72.910085	2373.071373	20.887322
72.601651	2374.319415	20.892339
72.773490	2374.426587	20.897357
72.809498	2374.688358	20.902375
72.553823	2389.588192	20.907392
73.023723	2388.791215	20.912410
73.086411	2392.959740	20.917427
72.948195	2399.827690	20.922445
73.158183	2390.160694	20.927463
72.934767	2396.818047	20.932480
73.247522	2390.296822	20.937498
73.184646	2393.843500	20.942515
73.151744	2395.074348	20.947533
73.427562	2386.641268	20.952551
73.452001	2393.349552	20.957568
74.005958	2394.499395	20.962586
74.094745	2405.920212	20.967603
74.254380	2403.586128	20.972621
74.169423	2388.867381	20.977639
73.978784	2384.035049	20.982656
74.028980	2373.883825	20.987674
74.028977	2380.682528	20.992691
73.879528	2378.707662	20.997709
74.549278	2396.523751	21.002727
74.304907	2411.531142	21.007744
74.472674	2407.957640	21.012762
74.546174	2401.904053	21.017779
74.494979	2412.378886	21.022797
74.548986	2403.842726	21.027815
74.268350	2410.993761	21.032832
74.782193	2410.122915	21.037850
74.774981	2411.835004	21.042867
74.701884	2413.626822	21.047885
74.948154	2400.710061	21.052903
74.927974	2410.988014	21.057920
74.859636	2410.493977	21.062938
74.756527	2434.359669	21.067955
74.896324	2430.066155	21.072973
75.282049	2433.673452	21.077991
75.357883	2438.861699	21.083008
75.507272	2437.276523	21.088026
75.287472	2434.755949	21.093043
75.414477	2441.224502	21.098061
75.465397	2452.142458	21.103079
75.494715	2471.162025	21.108096
75.767449	2464.947635	21.113114
75.911007	2468.502314	21.118131
75.879821	2481.910424	21.123149
76.193244	2469.461940	21.128167
75.755615	2469.415380	21.133184
76.033267	2464.369110	21.138202
75.979139	2475.593309	21.143219
76.175119	2490.849920	21.148237
76.570737	2481.936725	21.153255
76.379197	2490.780538	21.158272
76.617534	2493.583053	21.163290
76.819441	2492.471688	21.168307
76.535895	2488.015193	21.173325
77.035186	2484.578376	21.178343
76.539714	2488.427689	21.183360
76.727014	2494.671118	21.188378
76.751691	2488.706303	21.193395
76.496814	2497.458747	21.198413
76.909048	2505.241894	21.203431
76.910328	2517.484605	21.208448
76.964034	2511.869127	21.213466
77.344043	2517.989800	21.218483
77.527244	2520.593447	21.223501
77.513093	2513.115076	21.228519
77.567197	2521.673523	21.233536
77.650014	2517.514142	21.238554
77.529872	2514.231165	21.243571
77.559370	2529.285463	21.248589
78.352625	2536.102470	21.253607
78.244728	2547.514647	21.258624
78.050299	2536.102047	21.263642
78.100888	2541.365938	21.268659
77.958072	2540.418885	21.273677
78.237957	2541.848433	21.278695
78.077390	2545.628620	21.283712
78.429541	2539.777536	21.288730
78.222003	2535.912238	21.293747
77.948653	2543.094426	21.298765
78.455231	2543.402294	21.303783
78.559952	2568.862568	21.308800
78.905788	2571.349827	21.313818
78.993650	2573.094756	21.318835
79.018393	2569.492107	21.323853
79.550074	2566.253053	21.328871
79.374635	2571.629303	21.333888
79.410213	2558.998507	21.338906
79.509064	2557.640844	21.343923
79.253137	2563.051164	21.348941
79.666711	2551.576203	21.353959
79.327809	2562.018362	21.358976
79.309874	2562.737110	21.363994
79.267941	2569.028141	21.369011
79.216542	2560.105952	21.374029
79.654177	2563.897725	21.379047
79.464247	2575.219959	21.384064
79.854332	2583.325260	21.389082
80.089438	2586.107857	21.394099
80.034209	2600.228651	21.399117
79.915744	2588.243825	21.404135
79.647070	2598.189468	21.409152
79.800492	2602.815553	21.414170
80.243882	2615.130219	21.419187
80.245428	2622.045207	21.424205
80.680308	2614.005898	21.429223
80.223668	2614.417034	21.434240
80.775992	2614.389589	21.439258
81.001815	2620.154958	21.444275
80.610191	2623.038295	21.449293
80.589820	2617.595060	21.454311
80.793952	2632.826921	21.459328
80.843710	2645.508808	21.464346
81.224142	2648.542772	21.469363
81.246226	2655.126479	21.474381
81.554718	2647.705140	21.479399
81.299761	2649.176729	21.484416
81.466043	2645.405178	21.489434
81.759226	2643.938640	21.494451
81.517943	2653.016243	21.499469
81.865724	2655.031234	21.504487
81.721395	2652.675576	21.509504
81.506379	2650.280848	21.514522
81.734014	2645.913480	21.519539
81.538904	2658.922332	21.524557
81.971454	2666.735365	21.529575
81.914548	2679.702529	21.534592
82.160120	2680.177885	21.539610
82.143278	2671.850310	21.544627
82.139893	2678.847920	21.549645
82.319438	2682.075184	21.554663
82.316653	2683.236750	21.559680
82.373586	2696.133071	21.564698
82.731225	2701.688662	21.569715
82.588252	2705.897153	21.574733
82.720491	2692.130676	21.579751
82.898731	2704.726835	21.584768
82.899794	2707.446877	21.589786
83.172842	2704.472441	21.594803
83.233641	2715.207308	21.599821
83.416715	2716.783679	21.604839
83.922476	2725.750060	21.609856
83.804148	2716.014853	21.614874
83.841750	2702.782630	21.619891
83.412902	2695.550435	21.624909
83.587384	2691.673731	21.629927
83.487162	2709.924498	21.634944
83.873206	2718.014000	21.639962
84.037731	2721.835210	21.644979
84.111853	2732.087337	21.649997
84.228517	2720.986830	21.655015
83.968948	2724.513038	21.660032
84.042640	2729.258073	21.665050
84.214125	2726.229032	21.670067
83.809387	2723.106241	21.675085
84.364894	2740.446185	21.680103
84.472385	2742.012587	21.685120
84.272704	2736.079517	21.690138
84.775990	2741.411307	21.695155
84.663927	2752.970620	21.700173
84.768725	2745.071195	21.705191
84.921818	2753.900324	21.710208
85.199771	2768.131765	21.715226
85.284977	2770.211459	21.720243
85.210331	2769.414777	21.725261
85.484224	2770.092503	21.730279
85.493558	2778.754995	21.735296
85.539786	2773.390757	21.740314
85.965515	2766.926081	21.745331
85.373993	2775.859809	21.750349
85.881438	2777.360074	21.755367
85.689592	2768.173036	21.760384
85.809227	2768.583523	21.765402
86.014212	2770.219337	21.770419
85.889431	2780.111477	21.775437
85.616943	2768.722156	21.780455
85.945925	2778.302011	21.785472
85.826224	2790.348707	21.790490
86.167033	2788.166596	21.795507
86.168302	2790.575116	21.800525
86.146111	2789.119527	21.805543
86.515153	2799.581110	21.810560
86.253754	2820.651037	21.815578
86.704268	2816.047486	21.820595
86.632607	2820.579742	21.825613
87.171839	2799.786587	21.830631
87.372064	2811.101848	21.835648
87.356952	2811.235692	21.840666
87.616792	2803.656055	21.845683
87.461702	2806.510359	21.850701
87.452419	2816.286563	21.855719
87.471259	2813.008886	21.860736
87.612280	2805.648787	21.865754
87.552458	2808.251910	21.870771
87.352676	2811.085810	21.875789
87.827798	2812.308047	21.880807
87.886900	2824.386042	21.885824
87.839214	2834.464154	21.890842
88.323343	2835.588988	21.895859
88.121073	2833.569779	21.900877
88.212697	2833.318459	21.905895
88.105364	2832.781068	21.910912
88.170365	2827.299755	21.915930
88.340202	2829.239314	21.920947
88.148622	2835.653438	21.925965
88.672535	2857.786783	21.930983
88.752032	2864.825542	21.936000
88.622447	2869.677770	21.941018
88.890574	2864.323737	21.946035
88.795090	2866.769724	21.951053
88.598606	2863.372982	21.956071
88.860896	2879.178721	21.961088
89.140589	2889.556289	21.966106
89.542931	2881.596756	21.971123
89.851783	2883.511006	21.976141
90.155355	2881.110629	21.981159
89.990699	2876.285789	21.986176
89.854774	2884.583698	21.991194
90.286086	2877.071075	21.996211
90.008349	2877.317597	22.001229
90.223310	2868.773592	22.006247
90.226218	2873.625145	22.011264
90.042623	2879.022472	22.016282
90.433541	2871.135564	22.021299
90.000154	2876.906257	22.026317
90.381554	2867.427149	22.031335
90.573684	2875.004888	22.036352
89.907341	2880.270742	22.041370
90.498358	2869.711984	22.046387
90.452115	2866.517831	22.051405
90.440990	2876.620034	22.056423
90.841940	2900.335306	22.061440
90.723246	2902.229637	22.066458
90.873052	2901.268933	22.071475
90.594640	2908.693602	22.076493
90.940751	2909.580863	22.081511
91.330147	2917.550375	22.086528
91.279518	2932.085313	22.091546
91.473670	2934.137430	22.096563
91.328775	2936.318346	22.101581
91.368839	2934.136189	22.106599
91.684019	2931.396486	22.111616
91.689929	2940.320783	22.116634
92.096740	2945.307755	22.121651
91.938507	2965.232614	22.126669
92.339117	2967.299797	22.131687
92.653851	2964.007940	22.136704
92.175183	2969.404370	22.141722
92.347696	2961.137685	22.146739
92.415058	2960.703012	22.151757
92.478753	2963.361982	22.156775
92.428576	2958.736757	22.161792
92.513471	2956.369667	22.166810
92.787941	2964.818502	22.171827
92.643359	2983.765778	22.176845
93.100864	2985.844344	22.181863
93.684033	2982.271324	22.186880
93.253169	2975.581304	22.191898
93.031355	2976.067487	22.196915
93.255474	2974.593839	22.201933
92.962490	2973.299410	22.206951
93.532286	2986.290409	22.211968
93.428744	3002.172713	22.216986
93.917066	2996.975458	22.222003
94.189246	3001.509576	22.227021
94.108901	2998.254755	22.232039
94.467056	2993.223788	22.237056
94.397650	3002.953066	22.242074
94.452942	2999.869342	22.247091
94.577489	3000.238147	22.252109
94.499278	2997.444744	22.257127
94.724331	2998.255346	22.262144
94.799659	3009.152519	22.267162
94.658265	2998.634162	22.272179
94.742640	2994.593181	22.277197
94.620812	2999.998009	22.282215
94.807070	3002.933218	22.287232
94.781548	2997.900502	22.292250
94.581022	3003.077956	22.297267
94.810689	3012.908222	22.302285
95.069578	3021.571181	22.307303
95.118935	3022.553758	22.312320
95.176296	3028.652157	22.317338
95.032958	3028.468195	22.322355
95.339123	3046.789878	22.327373
95.335664	3060.056433	22.332391
95.758208	3039.991101	22.337408
95.693931	3050.570739	22.342426
95.834423	3053.878258	22.347443
96.416561	3065.431738	22.352461
96.546220	3071.605944	22.357479
96.600598	3060.055713	22.362496
96.619483	3070.261034	22.367514
96.894722	3067.703885	22.372531
96.937376	3056.673924	22.377549
96.525640	3054.241273	22.382567
96.673205	3051.761124	22.387584
96.410555	3069.770782	22.392602
96.760427	3079.762066	22.397619
96.805918	3077.983358	22.402637
96.867012	3082.121655	22.407655
97.028862	3087.557582	22.412672
96.912613	3109.139692	22.417690
97.020848	3107.130714	22.422707
97.164138	3119.749325	22.427725
96.979950	3122.335363	22.432743
97.454553	3134.249810	22.437760
97.843419	3134.430153	22.442778
97.677160	3146.800798	22.447795
97.989663	3133.358366	22.452813
98.001000	3141.450435	22.457831
98.160385	3145.696579	22.462848
98.305431	3161.815528	22.467866
98.745540	3157.026310	22.472883
98.720097	3160.495619	22.477901
98.687656	3169.639353	22.482919
99.209261	3158.382689	22.487936
99.325452	3159.102890	22.492954
99.084760	3152.457980	22.497971
99.157006	3152.018589	22.502989
99.323844	3147.436576	22.508007
99.606191	3146.436628	22.513024
99.385479	3153.857725	22.518042
99.255600	3151.749834	22.523059
99.367722	3151.243514	22.528077
99.346820	3153.989954	22.533095
99.696441	3149.593547	22.538112
99.503008	3152.632600	22.543130
99.397525	3148.046813	22.548147
99.921547	3166.388184	22.553165
99.910525	3172.639932	22.558183
100.041194	3166.204042	22.563200
99.834211	3179.921658	22.568218
100.092918	3167.935208	22.573235
100.347155	3167.650085	22.578253
100.086153	3178.226573	22.583271
100.170524	3187.745802	22.588288
100.143334	3200.018797	22.593306
100.394139	3196.313079	22.598323
100.637917	3210.644015	22.603341
100.867373	3223.272574	22.608359
101.203142	3217.699952	22.613376
101.267288	3234.461203	22.618394
101.264187	3227.479442	22.623411
101.456800	3222.031125	22.628429
101.235863	3223.631860	22.633447
101.587014	3215.692111	22.638464
101.426103	3221.183491	22.643482
101.491383	3226.373701	22.648499
101.472373	3236.106110	22.653517
101.860994	3253.919313	22.658535
102.193719	3248.034864	22.663552
102.219162	3256.927132	22.668570
102.135334	3247.855511	22.673587
102.510543	3244.115784	22.678605
102.480348	3249.856152	22.683623
102.328099	3247.148452	22.688640
102.329584	3266.473206	22.693658
102.363722	3273.275532	22.698675
102.576496	3280.393930	22.703693
102.841561	3284.648436	22.708711
103.019085	3283.591250	22.713728
103.030879	3300.845504	22.718746
103.137721	3303.418204	22.723763
103.436778	3304.209157	22.728781
103.283780	3310.024983	22.733799
103.487744	3304.626744	22.738816
103.664880	3302.926921	22.743834
103.926086	3303.177971	22.748851
104.012161	3303.961194	22.753869
103.889320	3321.974826	22.758887
104.242536	3320.770835	22.763904
104.447060	3331.770365	22.768922
104.371317	3326.460775	22.773939
104.390406	3321.576592	22.778957
104.447221	3334.668586	22.783975
104.542867	3323.412857	22.788992
104.663373	3322.529172	22.794010
104.677169	3319.506278	22.799027
104.698592	3320.940150	22.804045
104.683125	3345.012038	22.809063
104.801312	3356.263712	22.814080
105.055005	3358.047585	22.819098
104.947329	3355.545942	22.824115
105.392038	3352.443312	22.829133
105.299790	3365.980753	22.834151
105.499841	3376.370583	22.839168
105.478849	3378.019689	22.844186
105.763340	3377.485875	22.849203
106.157928	3373.959357	22.854221
106.182943	3383.500765	22.859239
106.246203	3376.974054	22.864256
106.232636	3379.691047	22.869274
106.078784	3385.564465	22.874291
106.591035	3378.670371	22.879309
106.362714	3386.517594	22.884327
107.012275	3388.367358	22.889344
107.583242	3365.188701	22.894362
107.586041	3350.499044	22.899379
107.679265	3342.915808	22.904397
107.653068	3342.598309	22.909415
107.628368	3340.010277	22.914432
107.801118	3340.037076	22.919450
107.799301	3336.035706	22.924467
107.966657	3314.672589	22.929485
107.583871	3316.363648	22.934503
107.531408	3307.802248	22.939520
107.851614	3319.676177	22.944538
107.990445	3331.678158	22.949555
108.300929	3336.111875	22.954573
108.017000	3340.755232	22.959591
108.009726	3331.473900	22.964608
108.216070	3331.102013	22.969626
107.881476	3337.373963	22.974643
108.370059	3334.324914	22.979661
108.202616	3360.787329	22.984679
108.232318	3365.691411	22.989696
108.517813	3373.498386	22.994714
108.264576	3378.444444	22.999731
108.627275	3392.452158	23.004749
108.387386	3407.968820	23.009767
108.913678	3403.216915	23.014784
109.137785	3417.815510	23.019802
109.183539	3432.887024	23.024819
109.620437	3425.627327	23.029837
109.129208	3430.255782	23.034855
109.547433	3431.580764	23.039872
110.007593	3445.738974	23.044890
110.104630	3453.321951	23.049907
109.994933	3452.644099	23.054925
109.694250	3464.189996	23.059943
110.357659	3456.168860	23.064960
110.253626	3465.385554	23.069978
110.310227	3486.195684	23.074995
110.324285	3484.008940	23.080013
110.534431	3488.969249	23.085031
110.685427	3488.703732	23.090048
110.707900	3495.939115	23.095066
110.965026	3515.942446	23.100083
111.562869	3506.267150	23.105101
111.208843	3512.405392	23.110119
111.301256	3513.445643	23.115136
111.339170	3513.298851	23.120154
111.210877	3512.465055	23.125171
111.407177	3508.843472	23.130189
111.759980	3519.381326	23.135207
112.090182	3537.064951	23.140224
112.464415	3539.772842	23.145242
112.286771	3543.497792	23.150259
112.342273	3545.034812	23.155277
112.538097	3540.905110	23.160295
112.468375	3538.782850	23.165312
112.669822	3539.682996	23.170330
112.664658	3544.448738	23.175347
112.590929	3538.541668	23.180365
112.713955	3532.618959	23.185383
112.772052	3535.150699	23.190400
112.801374	3548.023855	23.195418
112.872725	3561.269494	23.200435
113.342352	3556.174149	23.205453
113.137365	3570.530585	23.210471
113.157149	3568.291781	23.215488
113.631459	3574.579589	23.220506
113.391510	3604.955103	23.225523
113.626611	3593.052313	23.230541
113.751403	3601.700814	23.235559
113.716458	3602.315338	23.240576
114.124292	3626.796911	23.245594
114.017061	3631.000752	23.250611
114.254031	3624.889915	23.255629
114.431136	3629.417365	23.260647
114.726280	3644.798612	23.265664
114.748487	3645.047660	23.270682
114.888489	3654.055636	23.275699
115.327559	3643.533149	23.280717
115.405333	3649.512124	23.285735
115.110856	3645.477882	23.290752
115.477279	3647.714248	23.295770
115.376540	3647.007425	23.300787
115.601900	3641.246143	23.305805
115.823983	3639.218152	23.310823
116.043687	3661.738713	23.315840
115.787343	3672.602734	23.320858
115.923915	3675.722219	23.325875
116.092502	3669.755216	23.330893
116.034953	3673.822132	23.335911
115.675907	3673.999027	23.340928
116.279454	3695.130523	23.345946
116.225745	3699.538251	23.350963
116.948651	3701.197788	23.355981
117.054665	3696.419981	23.360999
117.223309	3703.917722	23.366016
117.391690	3695.800753	23.371034
116.794176	3701.284836	23.376051
117.287696	3690.803979	23.381069
117.798338	3708.587268	23.386087
117.711291	3709.304505	23.391104
117.914834	3713.200783	23.396122
117.828575	3716.419530	23.401139
118.268070	3706.500312	23.406157
117.937100	3710.938882	23.411175
118.096871	3707.244408	23.416192
118.526138	3706.663111	23.421210
118.272430	3711.062614	23.426227
118.594265	3714.348449	23.431245
118.485574	3718.296090	23.436263
118.760999	3713.060951	23.441280
118.703078	3707.836488	23.446298
118.623125	3719.979089	23.451315
118.729826	3705.537619	23.456333
118.980552	3722.944646	23.461351
118.797584	3731.027902	23.466368
119.481113	3732.010099	23.471386
119.360116	3743.514974	23.476403
119.276848	3739.736524	23.481421
119.247284	3742.051782	23.486439
119.438873	3757.905149	23.491456
119.636469	3764.655678	23.496474
119.549374	3767.909184	23.501491
119.730402	3778.821543	23.506509
120.274462	3789.100171	23.511527
119.993557	3798.978556	23.516544
120.271481	3796.121130	23.521562
120.485939	3804.427407	23.526579
120.600157	3819.250822	23.531597
120.818359	3832.971260	23.536615
120.940161	3830.145803	23.541632
121.046981	3820.455774	23.546650
120.904730	3828.436616	23.551667
121.140116	3828.440057	23.556685
121.598977	3844.628506	23.561703
121.767004	3855.534342	23.566720
122.004782	3843.293436	23.571738
121.900608	3852.710213	23.576755
121.850476	3847.999737	23.581773
122.339565	3850.421900	23.586791
122.154368	3842.165346	23.591808
122.343666	3841.784367	23.596826
122.127646	3845.738143	23.601843
122.651429	3851.029321	23.606861
123.069309	3861.563340	23.611879
123.130062	3861.310634	23.616896
123.175305	3859.919706	23.621914
123.277152	3851.607149	23.626931
123.192514	3856.060764	23.631949
123.207240	3857.791551	23.636967
123.259347	3855.855143	23.641984
123.601855	3862.330872	23.647002
123.273012	3861.062530	23.652019
123.757969	3874.679110	23.657037
123.793940	3877.482699	23.662055
123.633673	3885.653676	23.667072
123.899418	3886.478297	23.672090
123.806399	3892.544394	23.677107
123.890158	3895.623574	23.682125
124.378526	3911.467544	23.687143
124.199975	3919.007384	23.692160
124.278632	3913.801977	23.697178
124.199671	3928.132372	23.702195
124.385061	3947.228091	23.707213
124.890838	3949.018259	23.712231
124.801707	3951.653790	23.717248
125.058753	3953.343589	23.722266
125.007509	3967.564186	23.727283
125.443968	3969.670645	23.732301
125.505584	3974.271687	23.737319
125.442527	3973.126945	23.742336
125.934731	3978.239906	23.747354
125.727219	3996.395308	23.752371
125.848982	3997.331004	23.757389
126.148508	4001.183734	23.762407
126.067864	3999.584726	23.767424
126.260935	4004.582550	23.772442
126.315188	4022.804021	23.777459
126.159694	4027.435765	23.782477
126.722906	4029.679361	23.787495
126.856780	4047.992011	23.792512
127.213662	4052.413043	23.797530
127.246661	4054.793110	23.802547
127.161989	4059.295567	23.807565
127.794113	4049.527919	23.812583
127.585614	4048.232503	23.817600
127.456619	4058.292165	23.822618
127.686606	4075.118401	23.827635
127.897052	4079.665850	23.832653
128.191573	4083.717647	23.837671
127.976099	4083.133729	23.842688
128.398725	4088.966638	23.847706
128.438862	4102.706282	23.852723
128.797644	4110.415430	23.857741
128.887475	4109.226632	23.862759
129.009629	4103.414758	23.867776
129.399562	4093.493745	23.872794
129.888517	4096.159850	23.877811
129.876656	4088.897439	23.882829
129.802208	4092.689460	23.887847
129.522734	4091.745211	23.892864
130.216109	4087.747642	23.897882
130.183465	4093.495023	23.902899
130.170136	4089.688024	23.907917
130.393459	4084.586148	23.912935
130.254952	4088.111465	23.917952
130.223287	4076.359387	23.922970
130.403025	4085.553248	23.927987
130.617360	4078.054953	23.933005
130.918783	4090.137834	23.938023
130.761159	4114.004720	23.943040
130.574991	4109.665932	23.948058
130.886241	4120.410669	23.953075
130.741696	4117.069071	23.958093
131.060647	4119.841744	23.963111
130.991236	4135.713536	23.968128
131.274134	4145.066419	23.973146
131.335013	4147.091974	23.978163
131.259268	4149.151901	23.983181
131.445653	4164.292999	23.988199
131.632779	4185.704016	23.993216
131.888947	4171.496295	23.998234
131.778018	4199.760621	24.003251
131.803954	4202.987544	24.008269
132.227314	4207.728441	24.013287
132.357420	4224.367018	24.018304
132.721158	4241.831378	24.023322
132.834023	4245.169537	24.028339
132.650564	4257.665007	24.033357
133.083848	4252.301450	24.038375
133.156361	4272.428869	24.043392
133.392481	4263.960930	24.048410
133.548314	4274.886330	24.053427
133.471324	4277.599441	24.058445
133.664118	4269.482199	24.063463
133.546378	4287.121724	24.068480
134.214530	4293.035933	24.073498
134.154682	4300.575920	24.078515
134.298675	4301.106084	24.083533
134.531898	4308.118665	24.088551
134.378669	4329.016156	24.093568
135.066265	4321.492626	24.098586
135.027740	4331.221004	24.103603
134.726020	4325.774007	24.108621
135.289283	4314.443747	24.113639
135.157049	4331.864570	24.118656
135.191814	4348.819801	24.123674
135.760011	4349.729179	24.128691
135.759085	4348.071792	24.133709
135.891888	4347.078308	24.138727
135.745199	4358.065382	24.143744
136.110805	4362.856447	24.148762
136.385636	4378.289694	24.153779
136.315599	4379.088428	24.158797
136.510730	4374.829585	24.163815
136.717713	4380.949532	24.168832
137.095385	4378.551267	24.173850
137.010246	4383.752498	24.178867
137.085314	4392.620234	24.183885
137.384459	4399.553904	24.188903
137.377631	4401.910482	24.193920
137.522965	4397.950657	24.198938
137.589054	4401.942202	24.203955
137.691181	4403.076948	24.208973
137.761497	4410.520713	24.213991
137.760680	4416.091640	24.219008
137.647640	4436.460496	24.224026
138.171171	4437.299904	24.229043
137.938984	4433.675615	24.234061
138.522175	4451.309779	24.239079
138.591831	4460.986378	24.244096
138.878043	4465.344068	24.249114
138.992079	4458.293482	24.254131
138.956251	4466.396948	24.259149
138.788623	4458.590394	24.264167
138.668696	4482.000288	24.269184
139.201939	4486.610468	24.274202
139.486997	4500.110817	24.279219
139.570848	4489.512990	24.284237
139.749347	4506.764106	24.289255
140.102684	4514.146274	24.294272
140.004268	4523.443765	24.299290
140.122075	4523.001005	24.304307
140.018526	4522.825623	24.309325
139.978406	4530.040026	24.314343
140.385579	4543.328984	24.319360
140.761438	4544.925957	24.324378
141.089973	4552.928890	24.329395
140.941874	4570.970889	24.334413
141.407933	4568.966024	24.339431
141.052508	4580.801591	24.344448
141.267288	4578.815549	24.349466
141.824365	4589.219331	24.354483
141.979722	4594.720581	24.359501
142.471448	4596.956001	24.364519
142.378864	4596.181745	24.369536
142.537139	4598.495509	24.374554
143.138284	4593.885497	24.379571
142.948689	4594.712747	24.384589
143.422189	4575.283897	24.389607
143.346613	4583.238780	24.394624
143.300918	4574.257025	24.399642
143.919376	4568.062160	24.404659
143.322377	4567.657847	24.409677
143.641402	4562.973247	24.414695
143.678726	4569.894461	24.419712
143.572495	4571.314981	24.424730
143.705430	4571.365444	24.429747
143.858455	4575.475344	24.434765
143.909806	4561.143350	24.439783
143.801709	4588.802192	24.444800
143.822277	4592.772726	24.449818
144.225398	4598.665597	24.454835
144.285741	4616.298361	24.459853
144.389896	4616.832529	24.464871
144.442637	4631.196891	24.469888
144.487018	4648.372790	24.474906
145.047582	4663.371348	24.479923
144.816845	4662.460984	24.484941
145.343081	4669.100526	24.489959
145.189999	4694.686629	24.494976
145.247226	4703.487377	24.499994
145.437882	4701.099213	24.505011
145.427235	4726.491939	24.510029
145.952517	4732.117565	24.515047
145.995279	4732.032141	24.520064
146.443172	4742.794098	24.525082
146.711435	4759.587480	24.530099
146.278550	4764.321113	24.535117
146.540811	4761.868811	24.540135
146.688711	4774.981395	24.545152
146.743327	4790.203939	24.550170
147.151370	4792.348884	24.555187
147.121368	4800.247839	24.560205
147.510692	4806.114672	24.565223
147.607746	4826.035956	24.570240
147.661798	4831.025546	24.575258
147.940175	4818.944150	24.580275
148.437189	4827.986398	24.585293
148.617878	4818.528613	24.590311
148.675204	4827.182300	24.595328
148.606738	4832.984457	24.600346
149.159714	4826.238983	24.605363
148.889029	4841.487486	24.610381
149.130037	4839.209283	24.615399
149.301657	4831.172997	24.620416
149.210781	4832.732706	24.625434
149.370118	4845.769575	24.630451
149.216509	4864.755324	24.635469
149.735121	4862.026897	24.640487
149.926549	4865.871918	24.645504
150.035916	4874.533857	24.650522
150.407896	4879.584489	24.655539
150.305048	4894.353910	24.660557
150.334360	4896.168248	24.665575
150.504020	4893.567834	24.670592
150.261910	4917.267751	24.675610
150.697045	4920.273812	24.680627
150.836367	4922.979300	24.685645
151.162710	4939.270340	24.690663
151.296810	4948.656116	24.695680
151.403932	4953.328883	24.700698
151.587742	4952.701717	24.705715
151.469607	4973.381315	24.710733
151.758929	4977.997502	24.715751
152.029128	4985.714158	24.720768
152.078015	4994.835042	24.725786
152.076017	5012.052589	24.730803
152.000055	5020.584454	24.735821
152.261542	5030.411792	24.740839
152.724010	5038.837362	24.745856
152.887347	5047.054151	24.750874
153.421417	5049.265584	24.755891
153.392740	5067.476393	24.760909
153.735385	5068.934748	24.765927
153.553339	5081.711557	24.770944
153.753075	5076.674470	24.775962
154.075910	5072.415523	24.780979
153.721836	5074.759914	24.785997
154.029839	5085.579832	24.791015
154.034478	5096.437900	24.796032
154.111348	5107.520484	24.801050
154.431996	5112.737519	24.806067
154.854391	5128.907242	24.811085
154.790731	5134.815749	24.816103
154.995891	5136.348744	24.821120
154.942274	5134.434535	24.826138
155.387007	5145.102095	24.831155
155.298181	5164.496450	24.836173
155.466355	5161.693245	24.841191
155.855007	5166.150465	24.846208
155.818767	5190.891128	24.851226
156.392338	5185.024951	24.856243
156.448888	5192.394990	24.861261
156.378229	5190.423697	24.866279
156.677434	5197.334134	24.871296
156.528406	5217.991462	24.876314
157.056575	5219.309319	24.881331
156.870582	5224.505683	24.886349
157.014509	5230.101830	24.891367
157.595890	5234.588923	24.896384
157.307237	5249.928040	24.901402
157.571840	5245.192111	24.906419
157.832253	5262.825218	24.911437
157.805159	5274.940211	24.916455
158.134023	5282.509199	24.921472
158.045153	5287.181851	24.926490
158.385032	5292.848272	24.931507
158.335389	5305.858287	24.936525
158.673853	5311.205515	24.941543
159.181151	5309.656599	24.946560
159.273125	5332.362156	24.951578
159.582580	5336.073615	24.956595
159.635765	5331.293478	24.961613
159.915824	5329.023924	24.966631
159.877363	5331.251158	24.971648
159.821971	5341.881374	24.976666
160.068202	5348.971057	24.981683
160.122649	5361.994423	24.986701
160.239142	5368.498204	24.991719
160.686984	5360.927416	24.996736
160.272258	5384.905005	25.001754
160.620862	5400.772873	25.006771
160.917619	5397.852349	25.011789
160.878465	5406.059139	25.016807
161.228784	5426.724473	25.021824
161.181915	5439.227484	25.026842
161.523492	5430.011159	25.031859
161.576416	5455.202241	25.036877
161.753676	5463.288799	25.041895
162.121181	5451.757581	25.046912
162.008257	5473.156153	25.051930
162.440808	5477.672559	25.056947
162.855686	5475.696196	25.061965
163.270470	5475.097486	25.066983
163.524769	5469.972890	25.072000
163.442097	5475.108021	25.077018
163.703195	5468.307305	25.082035
164.103516	5467.445759	25.087053
163.978067	5468.384776	25.092071
163.899943	5461.698730	25.097088
163.924370	5470.919008	25.102106
164.243183	5460.469489	25.107123
164.370107	5472.122643	25.112141
164.249274	5485.784599	25.117159
164.449747	5491.976859	25.122176
164.236209	5504.389270	25.127194
164.700939	5499.593816	25.132211
164.814437	5520.500028	25.137229
164.904940	5528.187398	25.142247
165.381915	5523.327829	25.147264
165.363995	5536.327481	25.152282
165.302523	5548.773118	25.157299
165.679464	5553.767333	25.162317
165.630543	5560.750756	25.167335
166.098576	5570.674555	25.172352
165.991750	5588.989732	25.177370
166.130153	5586.950434	25.182387
166.468476	5612.259142	25.187405
166.731731	5616.988265	25.192423
167.042206	5616.715385	25.197440
166.891936	5629.381383	25.202458
167.398764	5637.217223	25.207475
167.483288	5649.038567	25.212493
167.527361	5649.443093	25.217511
167.632260	5657.502743	25.222528
168.033783	5674.555229	25.227546
168.075088	5671.760355	25.232563
168.311149	5672.099653	25.237581
168.112270	5694.332863	25.242599
168.705552	5701.811916	25.247616
168.895474	5710.444979	25.252634
168.872187	5709.395255	25.257651
168.849899	5724.084208	25.262669
169.227154	5733.548160	25.267687
169.441204	5740.130965	25.272704
169.359880	5744.449290	25.277722
169.870969	5754.470205	25.282739
169.899913	5761.778053	25.287757
170.186702	5765.364990	25.292775
170.470600	5761.008988	25.297792
170.499494	5772.090278	25.302810
170.503111	5778.337648	25.307827
171.082879	5773.035172	25.312845
171.095454	5770.639827	25.317863
171.700121	5764.586722	25.322880
171.927289	5762.390840	25.327898
172.837659	5736.805029	25.332915
173.280428	5734.519702	25.337933
173.235024	5731.240606	25.342951
173.053030	5705.696830	25.347968
172.940981	5693.715525	25.352986
173.358962	5695.713470	25.358003
173.475669	5689.587919	25.363021
173.245582	5687.618373	25.368039
173.379468	5671.483001	25.373056
173.158315	5671.997478	25.378074
173.288050	5673.243580	25.383091
173.303547	5681.209708	25.388109
173.258400	5689.865290	25.393127
173.386207	5686.638053	25.398144
173.689776	5703.015396	25.403162
173.783366	5719.592247	25.408179
173.869486	5724.071911	25.413197
173.780843	5741.940630	25.418215
174.412918	5742.441027	25.423232
174.058380	5762.659021	25.428250
174.364522	5775.140652	25.433267
174.770240	5782.169712	25.438285
174.535655	5806.729807	25.443303
174.964542	5826.717553	25.448320
175.106286	5824.560459	25.453338
175.180866	5845.294733	25.458355
175.373634	5858.257144	25.463373
175.502003	5888.688772	25.468391
176.043684	5889.367240	25.473408
176.059432	5900.648995	25.478426
176.101671	5926.019610	25.483443
176.470426	5929.907452	25.488461
176.471043	5941.932812	25.493479
176.703438	5951.548249	25.498496
176.775228	5970.349196	25.503514
177.378256	5985.303785	25.508531
177.385844	5985.534748	25.513549
177.803300	5999.441810	25.518567
178.025127	6012.748274	25.523584
178.271397	6018.598278	25.528602
178.290225	6012.891041	25.533619
178.291039	6019.688933	25.538637
178.590319	6041.349127	25.543655
178.823388	6048.716628	25.548672
179.308138	6049.404968	25.553690
179.436946	6066.853876	25.558707
179.777933	6074.624337	25.563725
179.699960	6077.553516	25.568743
179.781747	6070.118627	25.573760
180.038650	6079.580747	25.578778
179.611839	6083.575013	25.583795
180.204648	6089.384744	25.588813
180.195109	6106.939945	25.593831
180.605845	6119.950448	25.598848
180.792081	6129.264932	25.603866
180.980538	6132.751191	25.608883
181.165915	6129.811305	25.613901
181.150425	6141.593912	25.618919
181.450605	6150.808415	25.623936
181.558114	6163.560446	25.628954
181.723928	6156.987047	25.633971
181.916731	6157.586608	25.638989
181.962475	6178.882220	25.644007
182.340370	6181.272162	25.649024
182.354515	6190.054699	25.654042
182.665374	6200.348608	25.659059
183.056880	6204.302136	25.664077
183.075189	6220.332913	25.669095
183.299699	6208.637436	25.674112
183.525505	6228.253682	25.679130
183.749433	6237.158591	25.684148
184.087979	6247.412711	25.689165
183.968238	6242.138981	25.694183
184.096827	6245.138333	25.699200
184.304153	6263.177652	25.704218
184.443749	6270.452373	25.709236
184.539783	6272.246801	25.714253
184.754551	6286.407544	25.719271
185.012606	6306.464089	25.724288
184.788889	6310.832819	25.729306
185.117713	6332.123646	25.734324
185.439112	6338.781662	25.739341
185.665314	6343.014151	25.744359
185.798945	6365.491981	25.749376
186.016577	6370.385198	25.754394
185.880789	6374.633706	25.759412
186.595795	6395.002274	25.764429
186.210959	6409.314594	25.769447
186.830043	6409.869022	25.774464
186.878186	6425.069101	25.779482
186.949062	6446.496422	25.784500
187.872216	6450.995502	25.789517
187.912075	6456.563072	25.794535
188.405433	6456.584410	25.799552
188.820277	6453.549654	25.804570
188.800565	6460.635063	25.809588
189.085745	6448.234961	25.814605
188.841304	6458.110866	25.819623
188.920383	6449.857136	25.824640
189.193918	6461.263451	25.829658
188.928070	6480.155854	25.834676
189.328576	6479.128208	25.839693
189.356349	6489.450140	25.844711
189.519926	6507.233932	25.849728
189.998301	6513.942537	25.854746
189.775603	6513.057522	25.859764
190.469291	6530.015635	25.864781
190.593909	6539.040420	25.869799
191.040827	6533.024751	25.874816
191.323525	6526.856656	25.879834
191.247988	6531.014560	25.884852
191.599332	6526.836423	25.889869
191.443865	6548.567499	25.894887
191.767737	6558.898925	25.899904
192.017867	6552.776140	25.904922
192.394642	6567.999508	25.909940
192.471240	6553.645828	25.914957
191.938539	6577.510381	25.919975
192.422458	6579.530200	25.924992
192.672047	6580.391396	25.930010
192.875565	6593.130064	25.935028
193.026551	6591.788118	25.940045
192.967057	6614.777082	25.945063
193.215641	6618.397074	25.950080
193.194575	6629.998411	25.955098
193.331268	6642.917730	25.960116
194.024646	6646.815385	25.965133
194.220240	6678.958722	25.970151
194.034335	6676.547663	25.975168
194.781586	6687.570191	25.980186
194.540635	6700.771655	25.985204
195.005785	6711.522079	25.990221
195.162379	6714.013486	25.995239
195.476265	6723.465362	26.000256
195.133705	6735.313171	26.005274
195.761955	6729.437686	26.010292
196.862084	6722.262653	26.015309
196.940875	6721.848085	26.020327
197.399905	6716.000370	26.025344
197.306225	6705.735345	26.030362
197.195099	6707.111996	26.035380
197.734780	6710.954701	26.040397
197.732377	6711.534263	26.045415
197.787505	6724.786114	26.050432
198.017577	6728.117955	26.055450
198.092937	6731.668811	26.060468
198.393815	6727.560826	26.065485
197.929063	6734.717316	26.070503
198.137477	6736.351468	26.075520
198.665183	6748.483077	26.080538
198.619608	6762.705453	26.085556
198.762610	6769.773724	26.090573
198.743819	6781.624245	26.095591
198.835100	6785.706054	26.100608
199.417878	6814.240485	26.105626
199.294399	6829.400670	26.110644
199.818509	6834.662209	26.115661
199.988568	6857.436338	26.120679
199.850626	6866.160116	26.125696
200.338745	6882.815427	26.130714
200.106015	6894.638771	26.135732
200.608016	6896.424420	26.140749
200.915083	6914.995491	26.145767
201.345020	6920.584453	26.150784
201.495884	6925.604953	26.155802
201.320332	6943.854855	26.160820
201.568378	6944.616391	26.165837
201.851051	6956.391450	26.170855
201.841716	6978.568818	26.175872
202.184237	6979.788191	26.180890
202.445497	6988.879593	26.185908
203.046457	6991.740056	26.190925
203.355244	6997.236629	26.195943
203.615919	6999.822438	26.200960
204.228340	6993.337992	26.205978
203.887687	7006.577652	26.210996
204.264640	6993.847727	26.216013
204.330430	7002.659493	26.221031
204.542906	7021.574682	26.226048
204.676165	7020.610854	26.231066
204.632308	7026.063726	26.236084
205.118612	7022.692496	26.241101
205.306336	7026.107481	26.246119
205.333625	7047.646483	26.251136
205.391733	7050.225252	26.256154
205.397828	7054.570149	26.261172
205.906491	7058.618541	26.266189
205.717112	7079.321081	26.271207
206.062682	7082.100314	26.276224
206.331900	7098.252556	26.281242
206.303156	7110.391341	26.286260
206.393605	7116.357112	26.291277
206.658159	7142.659838	26.296295
206.675208	7150.130784	26.301312
207.285070	7172.197137	26.306330
207.240362	7194.347417	26.311348
207.538506	7207.971698	26.316365
207.989187	7217.911183	26.321383
207.973682	7235.260933	26.326400
208.215549	7236.774139	26.331418
208.707917	7252.584883	26.336436
208.882644	7260.908890	26.341453
208.913806	7277.198422	26.346471
208.918736	7290.705069	26.351488
209.294380	7303.401168	26.356506
209.509262	7322.381665	26.361524
209.866413	7333.516443	26.366541
209.992420	7343.547115	26.371559
210.073332	7357.188067	26.376576
210.923225	7356.442032	26.381594
210.671389	7381.160908	26.386612
211.106669	7388.564512	26.391629
211.448297	7397.953382	26.396647
211.653552	7405.023835	26.401664
211.822996	7403.484518	26.406682
211.858166	7426.029221	26.411700
212.217551	7423.926120	26.416717
212.588798	7424.806531	26.421735
212.391536	7451.275489	26.426752
212.770585	7447.117077	26.431770
212.735754	7463.546381	26.436788
213.181543	7455.653827	26.441805
213.098044	7473.091020	26.446823
213.207973	7492.079023	26.451840
213.589497	7486.638382	26.456858
213.621654	7511.284658	26.461876
213.954082	7516.132415	26.466893
214.486637	7518.548287	26.471911
214.234632	7542.896836	26.476928
214.861337	7551.210329	26.481946
214.816222	7552.401845	26.486964
215.180745	7558.551510	26.491981
215.496522	7565.827895	26.496999
215.556509	7566.798067	26.502016
215.902325	7568.010672	26.507034
215.860561	7593.709915	26.512052
216.203517	7598.641791	26.517069
216.419542	7606.662753	26.522087
216.426230	7628.600893	26.527104
216.763469	7632.334479	26.532122
216.762213	7644.119151	26.537140
217.089726	7662.589930	26.542157
217.340581	7672.700069	26.547175
217.708757	7685.652639	26.552192
217.931271	7695.557606	26.557210
217.878797	7717.144125	26.562228
218.202968	7720.341190	26.567245
218.716810	7729.562356	26.572263
218.826499	7748.921350	26.577280
218.988525	7751.238558	26.582298
219.123743	7766.436354	26.587316
219.468197	7791.917382	26.592333
219.559125	7786.076004	26.597351
219.706181	7811.076265	26.602368
219.701359	7812.238952	26.607386
220.208244	7828.311606	26.612404
220.388363	7842.051286	26.617421
220.877817	7846.937465	26.622439
221.005422	7868.126046	26.627456
221.398004	7870.622523	26.632474
221.290563	7880.562508	26.637492
221.953825	7883.466335	26.642509
222.297888	7893.524782	26.647527
222.399628	7906.440935	26.652544
222.910884	7905.427810	26.657562
223.110292	7907.205959	26.662580
223.132216	7920.855255	26.667597
223.241870	7919.932119	26.672615
222.965800	7933.256334	26.677632
223.196725	7944.609599	26.682650
223.429433	7958.808029	26.687668
223.695808	7958.982423	26.692685
224.093050	7982.168622	26.697703
224.102035	8006.177688	26.702720
224.283179	8005.426499	26.707738
224.414743	8028.018909	26.712756
224.584704	8029.419724	26.717773
225.407031	8037.295084	26.722791
225.423936	8049.919171	26.727808
225.677428	8047.428004	26.732826
225.752602	8066.079973	26.737844
225.707661	8078.097007	26.742861
226.236822	8086.961846	26.747879
226.419765	8106.297034	26.752896
226.465438	8112.936462	26.757914
226.492412	8124.484480	26.762932
226.892244	8144.991873	26.767949
227.096648	8154.620678	26.772967
227.235227	8173.986634	26.777984
227.481750	8185.141654	26.783002
227.746375	8205.856789	26.788020
227.625292	8224.131043	26.793037
228.124481	8244.514532	26.798055
228.212881	8262.239221	26.803072
228.807721	8277.016056	26.808090
229.067644	8280.818791	26.813108
228.923568	8309.888637	26.818125
229.514556	8321.259548	26.823143
229.551447	8339.974619	26.828160
229.936399	8338.658178	26.833178
230.219717	8362.497782	26.838196
230.559174	8369.087737	26.843213
230.945433	8383.673655	26.848231
231.069488	8397.311039	26.853248
231.616972	8403.720299	26.858266
231.707655	8412.441188	26.863284
231.533687	8428.234285	26.868301
231.941657	8424.108378	26.873319
232.178126	8451.126516	26.878336
232.474628	8462.395750	26.883354
232.485684	8473.404381	26.888372
232.857682	8486.181160	26.893389
233.184849	8492.292314	26.898407
233.031163	8514.340339	26.903424
233.332430	8524.556339	26.908442
233.914917	8542.674756	26.913460
233.896175	8548.281566	26.918477
234.310537	8555.440421	26.923495
234.411388	8570.336035	26.928512
234.331408	8578.724203	26.933530
234.730448	8600.469016	26.938548
234.939848	8613.028661	26.943565
235.416147	8621.284501	26.948583
236.210751	8604.688485	26.953600
237.072929	8605.926678	26.958618
237.418178	8587.739908	26.963636
237.676854	8597.772310	26.968653
238.255462	8579.876108	26.973671
238.117683	8582.130281	26.978688
238.345951	8575.971996	26.983706
238.373310	8586.939945	26.988724
238.267771	8571.170123	26.993741
238.529640	8554.174333	26.998759
238.484315	8571.699970	27.003776
238.676882	8567.234962	27.008794
238.706186	8576.488649	27.013812
238.432312	8581.505806	27.018829
238.264049	8583.095156	27.023847
238.513511	8606.474288	27.028864
238.722444	8616.666511	27.033882
239.027164	8645.098477	27.038900
239.209422	8671.666083	27.043917
239.710860	8689.325830	27.048935
239.859345	8713.431833	27.053952
240.033642	8716.922536	27.058970
240.380886	8747.509256	27.063988
240.368329	8764.090283	27.069005
240.911761	8778.546083	27.074023
240.920865	8804.229062	27.079040
240.974673	8826.909045	27.084058
241.573355	8845.200740	27.089076
241.446458	8867.335511	27.094093
241.841201	8889.460347	27.099111
242.117328	8921.769198	27.104128
242.137764	8928.432685	27.109146
242.509437	8951.607152	27.114164
242.667216	8972.733465	27.119181
242.809882	8999.495652	27.124199
243.171812	9036.203149	27.129216
243.706494	9052.838127	27.134234
244.084625	9069.318651	27.139252
244.076472	9087.856505	27.144269
244.660554	9096.232361	27.149287
244.809282	9121.212114	27.154304
245.202863	9130.317574	27.159322
245.579589	9149.548458	27.164340
245.605674	9167.383307	27.169357
246.209698	9183.162175	27.174375
246.373023	9194.658984	27.179392
246.538241	9210.070667	27.184410
246.877738	9219.748666	27.189428
246.969911	9237.325562	27.194445
247.508351	9242.742687	27.199463
247.934533	9253.019546	27.204480
247.960062	9256.900032	27.209498
248.358389	9272.391879	27.214516
248.756666	9287.962449	27.219533
248.660390	9295.751580	27.224551
248.540979	9313.932848	27.229568
249.081667	9315.335288	27.234586
249.203976	9339.661706	27.239604
249.261731	9359.450911	27.244621
249.686009	9365.223892	27.249639
249.490262	9387.470347	27.254656
250.005032	9400.406157	27.259674
250.198219	9420.920302	27.264692
250.486258	9425.962278	27.269709
250.692860	9438.484106	27.274727
250.817233	9470.165920	27.279744
251.089797	9485.709122	27.284762
251.318515	9493.084143	27.289780
251.732749	9504.219711	27.294797
252.482708	9505.473520	27.299815
253.228026	9508.217042	27.304832
253.268441	9532.087390	27.309850
254.147289	9525.501171	27.314868
254.061412	9518.144814	27.319885
254.486966	9522.007249	27.324903
254.661097	9520.848662	27.329920
254.871707	9519.291555	27.334938
254.916279	9518.366499	27.339956
254.561173	9528.033437	27.344973
254.999266	9528.930089	27.349991
255.232596	9540.425054	27.355008
255.062725	9543.185007	27.360026
255.342923	9560.123183	27.365044
255.138317	9580.366486	27.370061
255.557342	9583.028641	27.375079
255.724113	9621.384759	27.380096
255.756686	9644.188982	27.385114
256.282362	9664.067694	27.390132
256.135483	9691.179471	27.395149
256.689017	9708.310341	27.400167
256.983829	9732.706698	27.405184
257.417648	9748.723817	27.410202
257.639278	9769.322048	27.415220
257.778422	9787.884111	27.420237
258.081139	9814.489233	27.425255
258.513073	9838.299625	27.430272
258.214762	9855.617997	27.435290
258.957791	9876.675902	27.440308
259.035794	9901.557258	27.445325
259.763683	9918.433132	27.450343
260.210548	9935.661934	27.455360
260.314480	9953.936654	27.460378
260.463427	9959.499946	27.465396
260.645911	9987.624969	27.470413
261.142901	10005.369222	27.475431
261.668825	10017.505367	27.480448
261.735569	10026.769325	27.485466
262.254190	10035.792446	27.490484
262.413689	10056.202253	27.495501
262.795914	10062.245072	27.500519
263.054174	10056.338760	27.505536
263.104983	10074.947525	27.510554
263.599432	10076.207881	27.515572
263.589211	10099.731272	27.520589
263.623830	10109.574529	27.525607
264.025296	10122.233894	27.530624
263.971438	10147.129984	27.535642
264.394384	10139.576920	27.540660
264.335525	10167.733666	27.545677
264.677148	10181.043252	27.550695
265.037622	10207.720533	27.555712
264.989689	10218.704820	27.560730
265.634331	10238.439801	27.565748
265.505997	10257.786846	27.570765
265.823952	10268.115104	27.575783
266.100879	10283.878409	27.580800
266.563105	10311.780793	27.585818
267.108354	10325.502720	27.590836
267.057895	10354.495871	27.595853
267.415210	10361.304625	27.600871
268.023460	10375.152318	27.605888
267.952309	10394.182301	27.610906
268.074936	10411.889902	27.615924
268.467500	10426.342620	27.620941
268.606179	10442.545254	27.625959
268.981066	10459.735761	27.630976
269.070994	10485.674739	27.635994
269.625018	10496.597908	27.641012
271.250348	10486.976333	27.646029
272.059599	10470.091441	27.651047
272.196475	10479.166629	27.656064
272.464710	10469.888091	27.661082
272.577127	10450.657565	27.666100
272.925924	10445.113661	27.671117
273.013193	10433.770876	27.676135
272.887181	10430.474474	27.681152
272.930749	10431.079514	27.686170
273.024019	10425.444125	27.691188
273.054396	10451.584967	27.696205
273.195063	10463.550315	27.701223
273.430052	10466.415508	27.706240
273.433635	10486.907024	27.711258
273.882792	10511.833722	27.716276
273.872563	10525.502314	27.721293
273.860036	10538.952093	27.726311
274.532401	10557.448608	27.731328
274.380310	10574.547341	27.736346
274.951386	10592.967567	27.741364
275.242825	10619.456673	27.746381
275.034441	10632.430112	27.751399
275.505992	10654.886099	27.756416
275.845708	10685.312290	27.761434
276.240033	10694.665719	27.766452
276.424707	10729.992069	27.771469
276.810855	10759.137958	27.776487
276.927052	10768.101314	27.781504
277.012205	10799.434064	27.786522
277.504741	10813.539871	27.791540
277.688202	10838.989562	27.796557
277.862744	10874.869590	27.801575
278.450530	10889.580092	27.806592
278.584491	10906.165305	27.811610
279.061636	10923.864223	27.816628
279.023759	10947.973993	27.821645
279.431952	10967.779892	27.826663
279.958287	10971.389936	27.831680
280.316603	10992.153208	27.836698
280.523136	11001.769338	27.841716
281.078369	11022.035717	27.846733
281.861706	11029.087960	27.851751
282.424994	11033.458139	27.856768
282.270430	11034.556397	27.861786
282.600190	11036.927272	27.866804
282.657946	11047.492535	27.871821
283.006394	11061.634332	27.876839
283.011569	11067.380330	27.881856
282.971235	11082.260597	27.886874
283.227057	11089.973082	27.891892
283.718454	11121.873763	27.896909
283.859812	11129.725328	27.901927
284.276097	11152.096220	27.906944
284.281014	11163.166036	27.911962
284.808628	11193.852550	27.916980
284.790054	11204.747476	27.921997
285.224632	11222.223705	27.927015
285.400581	11236.254241	27.932032
285.390326	11269.697379	27.937050
286.115260	11280.172205	27.942068
286.231182	11309.917313	27.947085
286.522259	11326.511002	27.952103
286.973804	11345.423843	27.957120
286.889432	11375.222452	27.962138
287.336012	11391.175142	27.967156
287.669281	11412.301106	27.972173
288.150117	11435.560978	27.977191
288.420793	11455.319385	27.982208
288.446657	11478.439917	27.987226
288.793186	11502.298232	27.992244
289.157743	11521.043537	27.997261
289.193515	11550.739122	28.002279
289.817342	11565.807785	28.007296
290.051310	11585.683783	28.012314
290.742063	11619.618873	28.017332
290.707924	11623.876657	28.022349
290.902828	11635.719372	28.027367
291.571997	11653.024509	28.032384
291.396656	11673.252953	28.037402
292.076937	11688.528209	28.042420
292.481941	11696.578308	28.047437
292.805858	11717.091465	28.052455
293.270760	11724.434663	28.057472
293.371835	11745.849186	28.062490
293.579669	11755.993930	28.067508
293.843355	11770.325031	28.072525
293.707860	11791.233043	28.077543
293.978960	11812.217367	28.082560
294.235143	11825.584136	28.087578
294.998476	11843.329037	28.092596
295.183030	11865.313078	28.097613
294.971828	11878.193574	28.102631
295.831816	11896.287170	28.107648
295.880051	11916.969490	28.112666
296.274499	11935.480709	28.117684
296.306813	11956.233116	28.122701
296.385052	11974.013178	28.127719
296.985301	11980.452773	28.132736
297.061158	12010.475422	28.137754
297.484342	12029.859808	28.142772
298.258913	12047.259780	28.147789
298.173851	12076.245206	28.152807
298.436232	12093.185131	28.157824
298.471380	12118.897139	28.162842
298.979485	12140.992551	28.167860
299.236594	12154.204006	28.172877
299.277896	12173.676007	28.177895
299.888468	12198.417220	28.182912
299.770922	12221.109339	28.187930
300.287218	12238.202785	28.192948
300.943419	12262.895311	28.197965
300.963738	12296.274044	28.202983
301.605476	12311.429544	28.208000
301.806436	12332.010555	28.213018
302.346084	12348.890832	28.218036
302.596145	12370.324797	28.223053
302.807743	12387.740308	28.228071
303.108392	12397.908275	28.233088
303.507625	12419.070586	28.238106
303.980840	12439.165390	28.243124
304.218771	12449.993366	28.248141
304.394758	12472.026485	28.253159
304.852079	12487.218639	28.258176
305.156828	12501.665105	28.263194
305.421908	12515.771567	28.268212
306.178837	12532.218141	28.273229
306.161121	12547.361896	28.278247
306.698837	12559.794971	28.283264
306.920999	12572.936009	28.288282
306.981936	12588.567694	28.293300
307.370196	12598.002678	28.298317
307.279219	12614.971658	28.303335
307.660301	12630.965221	28.308352
308.186464	12665.230757	28.313370
308.384147	12677.838262	28.318388
308.456546	12694.609202	28.323405
308.720925	12720.274867	28.328423
309.560896	12727.507908	28.333440
309.432932	12745.618492	28.338458
309.717375	12767.409530	28.343476
310.433149	12783.334462	28.348493
310.708352	12793.838438	28.353511
311.074242	12815.594621	28.358528
310.921499	12835.472491	28.363546
311.279744	12854.009001	28.368564
311.614791	12863.900524	28.373581
311.443220	12888.864243	28.378599
311.989401	12900.842847	28.383616
312.202683	12924.368150	28.388634
312.764987	12949.548663	28.393652
313.033104	12973.881518	28.398669
313.351340	12984.578313	28.403687
313.613281	13010.251939	28.408704
314.117050	13035.306334	28.413722
314.570684	13048.735303	28.418740
314.733213	13068.974523	28.423757
314.870269	13079.696719	28.428775
315.408840	13101.376297	28.433792
315.640546	13124.753445	28.438810
315.999285	13140.094604	28.443828
316.719930	13153.009200	28.448845
316.844049	13170.381987	28.453863
317.041882	13181.548571	28.458880
317.453180	13209.789813	28.463898
317.995350	13214.929042	28.468916
318.480654	13228.508787	28.473933
318.250068	13236.159871	28.478951
318.841565	13254.778658	28.483968
318.746673	13276.434184	28.488986
318.878271	13294.199313	28.494004
319.648512	13308.484393	28.499021
320.015194	13328.462941	28.504039
320.117340	13349.522955	28.509056
320.785866	13376.668882	28.514074
321.025295	13389.591791	28.519092
321.512367	13396.808588	28.524109
321.577796	13429.704199	28.529127
321.957051	13435.576953	28.534144
321.910360	13462.542908	28.539162
322.250465	13483.319185	28.544180
322.734533	13497.560706	28.549197
323.076285	13523.865219	28.554215
323.353109	13536.889843	28.559232
323.483677	13575.345366	28.564250
323.705208	13587.018277	28.569268
324.436929	13605.424350	28.574285
324.395594	13638.461506	28.579303
324.754950	13658.457596	28.584320
324.793381	13682.295326	28.589338
325.018829	13720.732255	28.594356
325.898899	13737.076974	28.599373
326.062707	13760.337308	28.604391
326.435243	13777.027162	28.609408
326.857917	13791.778619	28.614426
327.159189	13816.508861	28.619444
327.692917	13839.436215	28.624461
327.591811	13865.563825	28.629479
328.068091	13886.702222	28.634496
328.510482	13904.901287	28.639514
328.669062	13932.386992	28.644532
329.054580	13945.456636	28.649549
329.287962	13971.268189	28.654567
329.683698	13997.854413	28.659584
329.734958	14015.212514	28.664602
329.982706	14034.065147	28.669620
330.511852	14054.081436	28.674637
330.791329	14082.852567	28.679655
331.113031	14094.534109	28.684672
331.356915	14124.180968	28.689690
331.777861	14156.382452	28.694708
332.219167	14176.244730	28.699725
332.308230	14201.722074	28.704743
332.651839	14233.271035	28.709760
332.924114	14255.070662	28.714778
333.271244	14286.224375	28.719796
333.736922	14304.333117	28.724813
333.882439	14331.263078	28.729831
334.434061	14358.584962	28.734848
334.540597	14379.799892	28.739866
335.299883	14399.102344	28.744884
335.489897	14428.945740	28.749901
335.907260	14453.024019	28.754919
336.426150	14481.215433	28.759936
336.400529	14501.545577	28.764954
336.575407	14522.861799	28.769972
337.294958	14535.140378	28.774989
337.553541	14577.082822	28.780007
337.594972	14603.786689	28.785024
338.361220	14629.843303	28.790042
338.592917	14655.150370	28.795060
339.493714	14664.909016	28.800077
340.105718	14674.198042	28.805095
340.638498	14687.537317	28.810112
340.848626	14702.960611	28.815130
341.223745	14710.249017	28.820148
341.822584	14712.349299	28.825165
342.052582	14733.454017	28.830183
342.609438	14738.090835	28.835200
342.988688	14734.808132	28.840218
342.610004	14745.293570	28.845236
342.989586	14761.868144	28.850253
343.049671	14784.373870	28.855271
343.435172	14804.938153	28.860288
343.581608	14821.856879	28.865306
343.669823	14843.695239	28.870324
344.099113	14860.849786	28.875341
343.973202	14888.759542	28.880359
344.816599	14912.123323	28.885376
344.954694	14937.979342	28.890394
345.160252	14971.443127	28.895412
345.462986	14993.408312	28.900429
345.671224	15027.747922	28.905447
346.093642	15060.259778	28.910464
346.688658	15079.910183	28.915482
346.880044	15101.534074	28.920500
347.270518	15121.986689	28.925517
347.479877	15158.951579	28.930535
347.585135	15182.121151	28.935552
348.371476	15208.056966	28.940570
348.442846	15238.764706	28.945588
349.160628	15255.674343	28.950605
349.247191	15284.958515	28.955623
349.622540	15304.892996	28.960640
349.954400	15330.870545	28.965658
349.906132	15367.619747	28.970676
350.666251	15399.372012	28.975693
351.181449	15432.012663	28.980711
351.416029	15448.052209	28.985728
351.984010	15468.595682	28.990746
352.574655	15491.208317	28.995764
353.092686	15504.760569	29.000781
353.574976	15529.276686	29.005799
353.752592	15542.163042	29.010816
353.983555	15558.136359	29.015834
353.836750	15587.457508	29.020852
354.179967	15606.734203	29.025869
354.657130	15644.579115	29.030887
354.937325	15672.962609	29.035904
355.356799	15687.768565	29.040922
355.610598	15728.999451	29.045940
356.070275	15746.450700	29.050957
356.070126	15787.420279	29.055975
356.538387	15813.465084	29.060992
357.335104	15847.826706	29.066010
357.095302	15877.978879	29.071028
357.829754	15904.875806	29.076045
358.667151	15938.085212	29.081063
358.861177	15963.758467	29.086080
359.345016	15980.406612	29.091098
359.762991	16001.210110	29.096116
360.125857	16009.251701	29.101133
360.496496	16031.433900	29.106151
361.054078	16052.367371	29.111168
361.302552	16059.724139	29.116186
361.383933	16101.194890	29.121204
361.818681	16112.020277	29.126221
362.240783	16135.838557	29.131239
362.726007	16161.515142	29.136256
362.937709	16187.567806	29.141274
363.269541	16214.258988	29.146292
363.751189	16226.231404	29.151309
363.584432	16257.382821	29.156327
363.800782	16283.801016	29.161344
364.549847	16308.359319	29.166362
364.527154	16331.655525	29.171380
364.999847	16367.075763	29.176397
365.606293	16392.373602	29.181415
365.969688	16415.682813	29.186432
366.334843	16440.646376	29.191450
366.904262	16458.495285	29.196468
367.289946	16485.064583	29.201485
367.675874	16495.838182	29.206503
367.776485	16525.459451	29.211520
368.446728	16530.634227	29.216538
368.465230	16551.987526	29.221556
369.080887	16571.376728	29.226573
369.195299	16591.197381	29.231591
369.465911	16618.105893	29.236608
369.843865	16641.588311	29.241626
370.103403	16667.999296	29.246644
370.624260	16685.398164	29.251661
370.979085	16723.565396	29.256679
371.144153	16743.159287	29.261696
371.762246	16770.599863	29.266714
371.892540	16808.325157	29.271732
372.248712	16837.052012	29.276749
372.758960	16856.961495	29.281767
373.161498	16892.579934	29.286784
373.428359	16910.991730	29.291802
373.556869	16948.337352	29.296820
374.262374	16976.652515	29.301837
374.537140	17002.838819	29.306855
375.010380	17030.700562	29.311872
375.456791	17055.396668	29.316890
376.365649	17073.693757	29.321908
376.610971	17084.637413	29.326925
377.466941	17099.764727	29.331943
377.278958	17122.323524	29.336960
378.118861	17135.265710	29.341978
378.086805	17156.083229	29.346996
378.683838	17178.457175	29.352013
378.757958	17202.562467	29.357031
379.208831	17226.690435	29.362048
379.484211	17240.853345	29.367066
380.076695	17280.003737	29.372084
380.053452	17299.194096	29.377101
380.586156	17320.303329	29.382119
380.911949	17356.216161	29.387136
381.005256	17375.938820	29.392154
381.016030	17408.389824	29.397172
381.561113	17439.756947	29.402189
382.155075	17468.658890	29.407207
382.464233	17504.479047	29.412224
383.246421	17520.366558	29.417242
383.385021	17565.276571	29.422260
383.840464	17586.825249	29.427277
384.221685	17619.618450	29.432295
384.290766	17656.301622	29.437312
384.727939	17669.741110	29.442330
385.135956	17707.609768	29.447348
385.581974	17738.511389	29.452365
385.797339	17766.479720	29.457383
386.119902	17800.517700	29.462400
386.767057	17830.326418	29.467418
387.066830	17863.101614	29.472436
387.096398	17888.063111	29.477453
387.725284	17920.871814	29.482471
388.140854	17953.482290	29.487488
388.577214	17975.580623	29.492506
388.682362	18009.465905	29.497524
389.247211	18033.153728	29.502541
389.622641	18060.551399	29.507559
389.740748	18103.811460	29.512576
390.312182	18124.318749	29.517594
390.813440	18165.365497	29.522612
391.262978	18195.902494	29.527629
391.435158	18230.067348	29.532647
391.779739	18257.924630	29.537664
391.702929	18290.999325	29.542682
392.105999	18331.460163	29.547700
392.406180	18363.638289	29.552717
393.443490	18393.024878	29.557735
393.925619	18440.237907	29.562752
394.650760	18456.873700	29.567770
395.014520	18504.445172	29.572788
395.217248	18531.835756	29.577805
396.043207	18561.144131	29.582823
396.207565	18589.889043	29.587840
396.473793	18613.037108	29.592858
396.628829	18650.351481	29.597876
396.986162	18673.723718	29.602893
397.762803	18709.259939	29.607911
397.792970	18751.219967	29.612928
398.423125	18776.013557	29.617946
398.616633	18815.531019	29.622964
398.932440	18845.660644	29.627981
399.296120	18879.794043	29.632999
399.810781	18922.810099	29.638016
400.553111	18945.548910	29.643034
400.942246	18983.713073	29.648052
401.278708	19009.097973	29.653069
401.567849	19041.987982	29.658087
401.765851	19086.432235	29.663104
402.700680	19107.633777	29.668122
403.080133	19140.724977	29.673140
403.213653	19168.680121	29.678157
403.899394	19198.178984	29.683175
403.893640	19231.606980	29.688192
404.668355	19254.695449	29.693210
405.270032	19289.973442	29.698228
405.482103	19305.703604	29.703245
406.844488	19326.657380	29.708263
406.811956	19348.189391	29.713280
407.551043	19369.730389	29.718298
408.126340	19390.060367	29.723316
408.158761	19402.068437	29.728333
408.973264	19414.909097	29.733351
408.833234	19438.205410	29.738368
409.170237	19454.777334	29.743386
409.107157	19468.890679	29.748404
409.464147	19494.070318	29.753421
409.988736	19510.995529	29.758439
409.905282	19551.657143	29.763456
410.479578	19567.347967	29.768474
410.833718	19602.406626	29.773492
411.115256	19638.825924	29.778509
411.373619	19667.149911	29.783527
411.678846	19703.482503	29.788544
412.054365	19728.377639	29.793562
412.301423	19784.326660	29.798580
412.685894	19823.439414	29.803597
413.230862	19857.659070	29.808615
413.495160	19909.096092	29.813632
413.898018	19945.048674	29.818650
414.264530	19986.070488	29.823668
414.723076	20027.779429	29.828685
415.465604	20065.781244	29.833703
415.549638	20107.622521	29.838720
415.807495	20149.690585	29.843738
416.577333	20197.561614	29.848756
416.988194	20239.305490	29.853773
417.529068	20273.582621	29.858791
417.758023	20320.556576	29.863808
418.118621	20363.149091	29.868826
418.897351	20392.013630	29.873844
419.251785	20442.715861	29.878861
419.832200	20470.804912	29.883879
419.979304	20514.013848	29.888896
420.401321	20558.627402	29.893914
420.587612	20594.936115	29.898932
421.245179	20634.547636	29.903949
422.416374	20658.984732	29.908967
422.676774	20695.986732	29.913984
423.160359	20722.648072	29.919002
423.922962	20749.446928	29.924020
424.091086	20775.631744	29.929037
425.074305	20800.313229	29.934055
425.037519	20831.991735	29.939072
425.557880	20860.359611	29.944090
426.221761	20885.504006	29.949108
426.371857	20909.374902	29.954125
427.240817	20931.868039	29.959143
427.105678	20953.283132	29.964160
427.480141	20981.083796	29.969178
428.415672	21000.269658	29.974196
428.633404	21032.794032	29.979213
428.723710	21052.801390	29.984231
429.241457	21096.265536	29.989248
429.568858	21112.651725	29.994266
430.146159	21149.853175	29.999284
430.337614	21180.213837	30.004301
431.328349	21204.693143	30.009319
431.343954	21231.076285	30.014336
431.424139	21262.717329	30.019354
432.199821	21287.679163	30.024372
432.442396	21319.616571	30.029389
432.766467	21350.939341	30.034407
433.035887	21369.988422	30.039424
433.600360	21392.074719	30.044442
434.203101	21437.063639	30.049460
434.076527	21470.188787	30.054477
435.052447	21487.521904	30.059495
435.492586	21517.105616	30.064512
435.907672	21550.691224	30.069530
436.435009	21580.288728	30.074548
436.645771	21606.108198	30.079565
437.056412	21635.939414	30.084583
437.559404	21668.470844	30.089600
438.256386	21693.567154	30.094618
438.508595	21725.127372	30.099636
438.987377	21762.861848	30.104653
439.612216	21788.608555	30.109671
439.945863	21808.537932	30.114688
440.291492	21836.245459	30.119706
440.861449	21865.508274	30.124724
441.412602	21898.567296	30.129741
441.841028	21919.380382	30.134759
442.167844	21960.783058	30.139776
442.311822	21985.926984	30.144794
443.159126	22024.106660	30.149812
442.925220	22060.542401	30.154829
443.581756	22083.985468	30.159847
443.854893	22127.691483	30.164864
444.254859	22166.941486	30.169882
445.132365	22199.514371	30.174900
445.149439	22237.262893	30.179917
445.802976	22276.998120	30.184935
446.077957	22317.300997	30.189952
446.396386	22360.931916	30.194970
447.133920	22389.493210	30.199988
447.367915	22441.886122	30.205005
447.566330	22473.474518	30.210023
447.805419	22523.707956	30.215040
448.374127	22566.647394	30.220058
449.167957	22614.899232	30.225076
449.381015	22662.590782	30.230093
450.063283	22699.582246	30.235111
450.430153	22752.576474	30.240128
450.736115	22795.354388	30.245146
451.270366	22830.006759	30.250164
451.679048	22882.638736	30.255181
452.172490	22910.587674	30.260199
452.924658	22951.606953	30.265216
453.041640	23002.853821	30.270234
453.747606	23032.991921	30.275252
454.015762	23081.194236	30.280269
454.705832	23115.046546	30.285287
455.165763	23165.383096	30.290304
455.687145	23193.009858	30.295322
456.346741	23234.763770	30.300340
456.315995	23265.930244	30.305357
456.856943	23297.264059	30.310375
457.556166	23332.710437	30.315392
458.352444	23348.936814	30.320410
459.278251	23370.226313	30.325428
459.650154	23394.642205	30.330445
460.242081	23414.215017	30.335463
460.955083	23436.222224	30.340480
460.974709	23448.496132	30.345498
461.726746	23472.501848	30.350516
461.994342	23498.114482	30.355533
462.551001	23516.795855	30.360551
462.901363	23531.870171	30.365568
463.165333	23556.803695	30.370586
463.649393	23571.862263	30.375604
463.909527	23613.727286	30.380621
464.251352	23651.622776	30.385639
464.588309	23680.221073	30.390656
464.849938	23711.796344	30.395674
465.675841	23735.077030	30.400692
465.970377	23777.935028	30.405709
466.303692	23807.736178	30.410727
466.473042	23848.209429	30.415744
467.201982	23896.143088	30.420762
467.743361	23927.511950	30.425780
468.184190	23971.044290	30.430797
468.683772	24004.609031	30.435815
469.020416	24047.905321	30.440832
468.856526	24089.356270	30.445850
469.676917	24119.175720	30.450868
470.233053	24171.431628	30.455885
470.774537	24200.808847	30.460903
471.794044	24247.628324	30.465920
471.789874	24280.521616	30.470938
472.533034	24309.428140	30.475956
472.462919	24352.687650	30.480973
472.995959	24397.342379	30.485991
473.486913	24442.773560	30.491008
473.977238	24491.014065	30.496026
474.649020	24528.654258	30.501044
474.864044	24579.614860	30.506061
475.313809	24619.528630	30.511079
475.719640	24668.574031	30.516096
476.102121	24711.004589	30.521114
476.876532	24748.799894	30.526132
477.240616	24797.493913	30.531149
477.999330	24828.821259	30.536167
478.563756	24871.661252	30.541184
479.055107	24911.584093	30.546202
479.657924	24956.791732	30.551220
480.085200	25000.541732	30.556237
480.195839	25041.682779	30.561255
481.109426	25078.021375	30.566272
481.220805	25116.807057	30.571290
481.862313	25147.876405	30.576308
482.366452	25189.442778	30.581325
483.132757	25220.431727	30.586343
482.907166	25257.760470	30.591360
483.229733	25297.739522	30.596378
484.040841	25339.294407	30.601396
484.288275	25383.793351	30.606413
484.239530	25423.079529	30.611431
485.078114	25470.573463	30.616448
485.973653	25508.367812	30.621466
486.626278	25546.101686	30.626484
486.963644	25585.908934	30.631501
487.368370	25618.158433	30.636519
487.944144	25663.017076	30.641536
487.954022	25711.069938	30.646554
488.813829	25741.887442	30.651572
489.343977	25797.825546	30.656589
489.634747	25834.741701	30.661607
490.402499	25878.428826	30.666624
490.711078	25932.838890	30.671642
491.538009	25973.962754	30.676660
491.905902	26012.628589	30.681677
492.193875	26052.557519	30.686695
492.969163	26094.732993	30.691712
493.013524	26145.516190	30.696730
493.566305	26187.574515	30.701748
493.952711	26234.643261	30.706765
494.175433	26289.437697	30.711783
494.815246	26336.764962	30.716800
495.212252	26391.251512	30.721818
496.779279	26421.691374	30.726836
497.193330	26460.862240	30.731853
497.567116	26507.302732	30.736871
498.534654	26541.770445	30.741888
499.250555	26579.475395	30.746906
499.593022	26604.195531	30.751924
500.211324	26640.297146	30.756941
500.647182	26671.154033	30.761959
501.186557	26698.983319	30.766976
501.410297	26736.195845	30.771994
501.671539	26769.712168	30.777012
502.286430	26807.910397	30.782029
502.667848	26848.988503	30.787047
503.579878	26883.605243	30.792064
503.720271	26928.503679	30.797082
504.432706	26963.473833	30.802100
505.010208	26997.184488	30.807117
505.083968	27035.557697	30.812135
505.584174	27077.049214	30.817152
506.079510	27121.596981	30.822170
506.986228	27142.677907	30.827188
507.200676	27186.572542	30.832205
507.466812	27231.844151	30.837223
508.558272	27259.666826	30.842240
509.050794	27289.964355	30.847258
509.733186	27307.486922	30.852276
510.338120	27333.649160	30.857293
510.958407	27361.263428	30.862311
511.546935	27378.931814	30.867328
511.810820	27407.858823	30.872346
512.160273	27439.961624	30.877364
512.003721	27465.282576	30.882381
512.500139	27503.288594	30.887399
513.224513	27531.362460	30.892416
513.276323	27582.616203	30.897434
513.772985	27626.437137	30.902452
514.226725	27663.013204	30.907469
514.230024	27716.723888	30.912487
515.082380	27759.714803	30.917504
515.146032	27815.266196	30.922522
516.043347	27863.664718	30.927540
516.114329	27919.850355	30.932557
516.389082	27974.954225	30.937575
517.378573	28028.270897	30.942592
517.861438	28092.403057	30.947610
518.718352	28139.028139	30.952628
519.374471	28190.258452	30.957645
519.835106	28237.425998	30.962663
520.713220	28287.165168	30.967680
521.321536	28327.433985	30.972698
521.407003	28366.621622	30.977716
522.270194	28403.772366	30.982733
522.739440	28455.208204	30.987751
523.839020	28485.133920	30.992768
524.659882	28507.979536	30.997786
525.646139	28540.961703	31.002804
526.394023	28567.509747	31.007821
526.989826	28598.357441	31.012839
527.331311	28629.004594	31.017856
527.912586	28652.214788	31.022874
528.068350	28682.521288	31.027892
528.299678	28707.695714	31.032909
528.285955	28747.041898	31.037927
528.944819	28784.921036	31.042944
529.694402	28819.427549	31.047962
530.649681	28847.503167	31.052980
531.577007	28875.928412	31.057997
532.055697	28900.132369	31.063015
532.605903	28932.141534	31.068032
532.908356	28949.040880	31.073050
533.094944	28975.904356	31.078068
533.657222	29011.873630	31.083085
533.945288	29045.015314	31.088103
534.484485	29081.976527	31.093120
535.039775	29111.241533	31.098138
535.391491	29141.867535	31.103156
536.272486	29182.459084	31.108173
536.433265	29225.573502	31.113191
536.779351	29265.971518	31.118208
537.222291	29317.801958	31.123226
537.628005	29350.038259	31.128244
538.127408	29399.122520	31.133261
538.190800	29442.736844	31.138279
538.862016	29478.661430	31.143296
539.109995	29529.924727	31.148314
539.578959	29570.762535	31.153332
540.248086	29632.726185	31.158349
540.550379	29687.588762	31.163367
541.238816	29735.134123	31.168384
541.899117	29786.386133	31.173402
542.503106	29845.724315	31.178420
542.780573	29888.159970	31.183437
542.934995	29950.189470	31.188455
543.634496	30006.942536	31.193472
544.198607	30069.867033	31.198490
544.284692	30135.953789	31.203508
545.300838	30193.705133	31.208525
545.226636	30261.660319	31.213543
546.114384	30323.640621	31.218560
546.382485	30393.874393	31.223578
547.315823	30458.473662	31.228596
547.674531	30518.724914	31.233613
548.124273	30599.860705	31.238631
548.924019	30655.553534	31.243648
549.382403	30731.634092	31.248666
549.947435	30783.935163	31.253684
550.918547	30840.778673	31.258701
551.280378	30911.764139	31.263719
552.493687	30956.988220	31.268736
553.101160	31006.802437	31.273754
554.097538	31053.826592	31.278772
554.511855	31102.775051	31.283789
555.155030	31159.071392	31.288807
555.812187	31203.459544	31.293824
556.324312	31257.482237	31.298842
556.806754	31297.155855	31.303860
557.629033	31336.712395	31.308877
558.361807	31383.349191	31.313895
559.102271	31425.756057	31.318912
559.107161	31472.748615	31.323930
559.781393	31509.835661	31.328948
560.458355	31550.826532	31.333965
560.829083	31608.376729	31.338983
561.353719	31646.564439	31.344000
561.895261	31689.424508	31.349018
562.658354	31742.073792	31.354036
563.176527	31786.357983	31.359053
563.503237	31831.508173	31.364071
565.045435	31855.086870	31.369088
566.008148	31888.368009	31.374106
566.836001	31921.423231	31.379124
567.405383	31938.822216	31.384141
567.757298	31968.668517	31.389159
568.512804	31988.985428	31.394176
569.044020	32011.070347	31.399194
569.292872	32039.478344	31.404212
569.543128	32061.431543	31.409229
569.750131	32093.298221	31.414247
570.149289	32114.613048	31.419264
570.426883	32154.482134	31.424282
570.824888	32189.909229	31.429300
571.376038	32231.251267	31.434317
571.202410	32291.002701	31.439335
572.206786	32327.359649	31.444352
573.083149	32373.503510	31.449370
573.478420	32431.010108	31.454388
574.347725	32469.319796	31.459405
574.419664	32522.891851	31.464423
574.870376	32568.099967	31.469440
575.319958	32623.675538	31.474458
576.076268	32680.543857	31.479476
576.953968	32724.086048	31.484493
576.928426	32782.583015	31.489511
577.538076	32831.749820	31.494528
578.471209	32893.302252	31.499546
578.385214	32958.098902	31.504564
579.590639	33004.531023	31.509581
580.046988	33057.297987	31.514599
581.106128	33094.227989	31.519616
582.346308	33139.959801	31.524634
582.694759	33187.479445	31.529652
583.713867	33227.611338	31.534669
584.049391	33278.035328	31.539687
584.418017	33306.120615	31.544704
585.267628	33344.094981	31.549722
585.710551	33393.129221	31.554740
586.206810	33439.855214	31.559757
586.496483	33496.710803	31.564775
586.998283	33531.955570	31.569792
587.348386	33584.411672	31.574810
587.595243	33648.658295	31.579828
588.347826	33702.631770	31.584845
588.713480	33768.001230	31.589863
589.427364	33836.733099	31.594880
589.879580	33892.109145	31.599898
590.252234	33956.768853	31.604916
590.797771	34020.964615	31.609933
591.207459	34095.041146	31.614951
591.909889	34153.950366	31.619968
592.165625	34237.523176	31.624986
592.169163	34313.158234	31.630004
593.237838	34381.539477	31.635021
593.759308	34459.966566	31.640039
594.284370	34545.935215	31.645056
595.446568	34609.875813	31.650074
595.778869	34690.578994	31.655092
596.655134	34738.357947	31.660109
597.464363	34817.242205	31.665127
597.900941	34877.813791	31.670144
599.056888	34942.002591	31.675162
599.322078	35010.039847	31.680180
600.106638	35060.183311	31.685197
600.422514	35117.573108	31.690215
601.101556	35174.908418	31.695232
601.781178	35221.479354	31.700250
602.096022	35276.112526	31.705268
603.097569	35338.763529	31.710285
603.590258	35393.479118	31.715303
603.945105	35444.384268	31.720320
604.910738	35512.015625	31.725338
605.430151	35562.726236	31.730356
606.352301	35597.960456	31.735373
607.197059	35663.913728	31.740391
607.938501	35714.546873	31.745408
609.184129	35753.658710	31.750426
609.834756	35791.058641	31.755444
610.446899	35824.947443	31.760461
611.055481	35859.910531	31.765479
611.925642	35894.221898	31.770496
613.118769	35910.307030	31.775514
613.174656	35957.955254	31.780532
613.904477	35987.297683	31.785549
614.521085	36013.832936	31.790567
614.749194	36059.590487	31.795584
615.535076	36096.745686	31.800602
615.588822	36148.257465	31.805620
616.214756	36185.405223	31.810637
616.652445	36235.121854	31.815655
617.116666	36285.444558	31.820672
618.112608	36328.326210	31.825690
618.137408	36389.692506	31.830708
619.028527	36430.656590	31.835725
619.889574	36473.293644	31.840743
620.459496	36523.620725	31.845760
621.175816	36567.917622	31.850778
621.377530	36624.627569	31.855796
622.132684	36675.013897	31.860813
622.286025	36737.623891	31.865831
622.767571	36799.447125	31.870848
623.640136	36853.731734	31.875866
623.972314	36924.853204	31.880884
624.763848	36983.211084	31.885901
625.173927	37038.326746	31.890919
626.133969	37098.599096	31.895936
627.060237	37151.933252	31.900954
627.639460	37204.293252	31.905972
628.417235	37253.853095	31.910989
629.109827	37308.819012	31.916007
629.722844	37355.747050	31.921024
630.438093	37413.495764	31.926042
630.676536	37459.719028	31.931060
631.738113	37508.431870	31.936077
632.954159	37549.427353	31.941095
633.355402	37592.619794	31.946112
634.172282	37631.214593	31.951130
634.517614	37675.031079	31.956148
635.290718	37705.760314	31.961165
635.705147	37748.156371	31.966183
636.142123	37788.544881	31.971200
636.520736	37822.757140	31.976218
636.666162	37879.458188	31.981236
637.331371	37935.171586	31.986253
637.541520	37993.366950	31.991271
637.578181	38062.749044	31.996288
638.466236	38127.730624	32.001306
638.894611	38202.810933	32.006324
639.462111	38263.741252	32.011341
639.758506	38344.007234	32.016359
640.292610	38422.151189	32.021376
641.274202	38496.944449	32.026394
641.561056	38590.436377	32.031412
642.224494	38669.281487	32.036429
642.999854	38749.846827	32.041447
643.543623	38828.829996	32.046464
644.570879	38905.590432	32.051482
645.173365	38988.997558	32.056500
645.717614	39067.887148	32.061517
646.745318	39150.180306	32.066535
647.216066	39224.802659	32.071552
647.974582	39302.490739	32.076570
648.729675	39383.518031	32.081588
649.366847	39455.218113	32.086605
650.347586	39524.611947	32.091623
651.038289	39594.377094	32.096640
652.075384	39656.943863	32.101658
652.519197	39732.209806	32.106676
653.526590	39794.650924	32.111693
654.108059	39856.784778	32.116711
654.776972	39919.396945	32.121728
655.961661	39971.749499	32.126746
657.388940	40017.739953	32.131764
658.246822	40063.713963	32.136781
659.043254	40110.032201	32.141799
659.778140	40146.942651	32.146816
660.085454	40187.863718	32.151834
660.885148	40240.388791	32.156852
661.352409	40280.177566	32.161869
662.076775	40305.215302	32.166887
662.299622	40354.757444	32.171904
663.070695	40396.242272	32.176922
663.637309	40449.407516	32.181940
664.761866	40483.518966	32.186957
665.662682	40531.313578	32.191975
666.181372	40569.899463	32.196992
666.860435	40614.758518	32.202010
666.832317	40666.038396	32.207028
667.340822	40716.971194	32.212045
668.139905	40764.306393	32.217063
668.353759	40822.543936	32.222080
669.223500	40870.454837	32.227098
669.565324	40928.397957	32.232116
670.081024	40985.146567	32.237133
670.805241	41034.607687	32.242151
671.274573	41094.817803	32.247168
671.454383	41157.020333	32.252186
671.799673	41222.092252	32.257204
672.741663	41286.750837	32.262221
673.291474	41356.165526	32.267239
673.591527	41432.262989	32.272256
674.282669	41510.837653	32.277274
674.934327	41584.296509	32.282292
675.787643	41655.925657	32.287309
676.507504	41728.118883	32.292327
677.087207	41809.176118	32.297344
677.278630	41879.157815	32.302362
678.277707	41961.303456	32.307380
679.056610	42038.702622	32.312397
679.788301	42132.590964	32.317415
680.382502	42211.499690	32.322432
681.453547	42281.756181	32.327450
681.815136	42364.241819	32.332468
682.634683	42440.715244	32.337485
683.472668	42520.189050	32.342503
684.045317	42594.046468	32.347520
685.025068	42669.060142	32.352538
685.565866	42746.030382	32.357556
686.393284	42827.936198	32.362573
687.118072	42901.420561	32.367591
687.798537	42977.732392	32.372608
689.224056	43032.494360	32.377626
689.977902	43095.382168	32.382644
691.103877	43158.009067	32.387661
692.214831	43201.342411	32.392679
693.672551	43241.412505	32.397696
694.595999	43275.025266	32.402714
695.485601	43309.201835	32.407732
695.914984	43351.517906	32.412749
696.722576	43388.092521	32.417767
697.278238	43430.865017	32.422784
697.721253	43446.349672	32.427802
698.450338	43491.151478	32.432820
698.615760	43543.670908	32.437837
699.599424	43587.561768	32.442855
700.210022	43623.830706	32.447872
700.801269	43668.389931	32.452890
701.025121	43729.515832	32.457908
701.634921	43783.091430	32.462925
701.995971	43841.741588	32.467943
702.352792	43902.471524	32.472960
703.294753	43960.717285	32.477978
703.875022	44028.118876	32.482996
704.395802	44089.145136	32.488013
705.664037	44158.526095	32.493031
706.114026	44227.832551	32.498048
706.573956	44274.035753	32.503066
707.369151	44339.394782	32.508084
707.809344	44385.194462	32.513101
708.952436	44435.116011	32.518119
709.539406	44500.448856	32.523136
710.156756	44557.495863	32.528154
710.713515	44613.546332	32.533172
710.753552	44677.263340	32.538189
711.487755	44737.936106	32.543207
712.143525	44813.509094	32.548224
713.088325	44881.792928	32.553242
713.795712	44949.086353	32.558260
714.548585	45011.198855	32.563277
715.433768	45073.315752	32.568295
715.875477	45166.979582	32.573312
716.797222	45230.021901	32.578330
717.494678	45303.113789	32.583348
718.304742	45376.367884	32.588365
719.031967	45439.637533	32.593383
719.484086	45528.685994	32.598400
720.206977	45587.394832	32.603418
720.956846	45662.779832	32.608436
721.837187	45729.827879	32.613453
722.593487	45793.008993	32.618471
723.284591	45875.155926	32.623488
724.259344	45940.262045	32.628506
725.061643	46008.642378	32.633524
725.451222	46092.860702	32.638541
726.274864	46168.516930	32.643559
726.838615	46243.167378	32.648576
727.440770	46317.799409	32.653594
728.234414	46391.281214	32.658612
728.555069	46480.939124	32.663629
729.891824	46550.829810	32.668647
730.233250	46630.682226	32.673664
730.938016	46718.185185	32.678682
731.557193	46798.618863	32.683700
732.269698	46890.497656	32.688717
732.997869	46969.166791	32.693735
733.226948	47071.358936	32.698752
733.980558	47154.811305	32.703770
734.873920	47247.445660	32.708788
735.364500	47343.293573	32.713805
736.419791	47436.893895	32.718823
736.939395	47537.045190	32.723840
737.669168	47625.088219	32.728858
738.856479	47707.436057	32.733876
739.571537	47790.563101	32.738893
740.468787	47880.464477	32.743911
741.273154	47971.245667	32.748928
742.335554	48043.631365	32.753946
743.430049	48133.000916	32.758964
743.865182	48217.607080	32.763981
744.873427	48279.248711	32.768999
745.810365	48350.538616	32.774016
746.462987	48418.784883	32.779034
747.089040	48489.541080	32.784052
747.445329	48563.663220	32.789069
748.550529	48622.027846	32.794087
749.026164	48704.711347	32.799104
749.923855	48776.100720	32.804122
750.399800	48850.896067	32.809140
750.895336	48928.194109	32.814157
751.902652	48997.515818	32.819175
752.693137	49075.404968	32.824192
753.367409	49145.562854	32.829210
753.916250	49221.335849	32.834228
754.935562	49307.179550	32.839245
755.275455	49387.612637	32.844263
755.960668	49478.969578	32.849280
756.729473	49551.991958	32.854298
757.368830	49635.474184	32.859316
758.012627	49720.899994	32.864333
759.102251	49798.053588	32.869351
759.568359	49897.093798	32.874368
759.895335	49990.312294	32.879386
761.042716	50088.916920	32.884404
761.523999	50184.784781	32.889421
762.642199	50269.443425	32.894439
763.448124	50361.801823	32.899456
764.237040	50459.512505	32.904474
765.108426	50544.309569	32.909492
765.357917	50644.158413	32.914509
766.479885	50734.303513	32.919527
767.556987	50825.592323	32.924544
768.319705	50919.090274	32.929562
769.887921	50991.751429	32.934580
771.515051	51053.171594	32.939597
772.482903	51101.451499	32.944615
773.034220	51179.176440	32.949632
774.166926	51235.203540	32.954650
774.917066	51296.442237	32.959668
775.308320	51370.952318	32.964685
776.196060	51419.327886	32.969703
777.240703	51493.068554	32.974720
777.689511	51555.908850	32.979738
778.532638	51625.478342	32.984756
779.042015	51693.125556	32.989773
780.128160	51752.923670	32.994791
780.735985	51823.083688	32.999808
781.111630	51889.701962	33.004826
781.684587	51958.842338	33.009844
781.930492	52053.040728	33.014861
782.828972	52126.071886	33.019879
783.528131	52215.108178	33.024896
783.971434	52305.517524	33.029914
784.834969	52385.707097	33.034932
785.374066	52478.939440	33.039949
786.334030	52562.235895	33.044967
787.214776	52648.565821	33.049984
788.166188	52724.412610	33.055002
789.234124	52802.014967	33.060020
790.067564	52884.521897	33.065037
790.934451	52948.553515	33.070055
791.589139	53012.795886	33.075072
791.677571	53093.033065	33.080090
792.733623	53158.351480	33.085108
793.398976	53237.405392	33.090125
794.364109	53323.488381	33.095143
794.829242	53408.745500	33.100160
795.949746	53482.318088	33.105178
797.224317	53555.260432	33.110196
798.542180	53618.351481	33.115213
800.623036	53657.193997	33.120231
801.886461	53706.229241	33.125248
802.550991	53759.362244	33.130266
803.118442	53796.132320	33.135284
804.098824	53843.745266	33.140301
804.767890	53886.925787	33.145319
805.219329	53934.171796	33.150336
805.801035	53991.466194	33.155354
806.647757	54041.013728	33.160372
807.188729	54106.168187	33.165389
807.683285	54163.637978	33.170407
808.225231	54229.799633	33.175424
808.876811	54300.126414	33.180442
809.398166	54375.205779	33.185460
809.859266	54455.515906	33.190477
810.711412	54535.896719	33.195495
811.124823	54622.218874	33.200512
812.148865	54702.844524	33.205530
812.861196	54791.373678	33.210548
813.191482	54881.053089	33.215565
813.963273	54975.476477	33.220583
814.993212	55073.830285	33.225600
815.401852	55171.118714	33.230618
816.537681	55266.331637	33.235636
816.877823	55364.623182	33.240653
817.845237	55459.292558	33.245671
818.353540	55575.261140	33.250688
819.121326	55686.949677	33.255706
820.307547	55787.602630	33.260724
821.010534	55894.078342	33.265741
821.654298	56001.122845	33.270759
822.362994	56112.586616	33.275776
823.187263	56211.806339	33.280794
824.474856	56313.118436	33.285812
825.537273	56420.606995	33.290829
826.983491	56511.360548	33.295847
828.089129	56593.029601	33.300864
829.146958	56673.456498	33.305882
830.352324	56748.960752	33.310900
831.379562	56825.604902	33.315917
832.649945	56891.189840	33.320935
833.868032	56944.992179	33.325952
834.746420	57011.255537	33.330970
835.884735	57057.759417	33.335988
836.684455	57105.750565	33.341005
837.872142	57147.454545	33.346023
838.384047	57184.401275	33.351040
838.850177	57239.921586	33.356058
839.634476	57287.151670	33.361076
839.918292	57343.932538	33.366093
840.555259	57398.258043	33.371111
841.163483	57455.262281	33.376128
841.714054	57535.833658	33.381146
842.312833	57600.344121	33.386164
842.701531	57685.882691	33.391181
843.337675	57768.108386	33.396199
844.173672	57856.585247	33.401216
844.467024	57955.295834	33.406234
845.430707	58039.841592	33.411252
845.949489	58148.168648	33.416269
846.564288	58252.853479	33.421287
847.356424	58358.890362	33.426304
848.139469	58472.516033	33.431322
849.439298	58582.309382	33.436340
849.782640	58685.818010	33.441357
850.763004	58787.890313	33.446375
851.810275	58897.612055	33.451392
852.752702	59003.922318	33.456410
854.231273	59100.016079	33.461428
855.271617	59199.217419	33.466445
856.481143	59281.184896	33.471463
857.786420	59360.557944	33.476480
859.022907	59445.069830	33.481498
860.085015	59521.886916	33.486516
860.673379	59614.702414	33.491533
861.386550	59693.719606	33.496551
862.271659	59784.161714	33.501568
862.729967	59873.352376	33.506586
863.547516	59954.674771	33.511604
864.270070	60048.614059	33.516621
864.698410	60146.676943	33.521639
865.808096	60236.343487	33.526656
866.108720	60340.231179	33.531674
867.051762	60445.775951	33.536692
867.763135	60551.733933	33.541709
868.168571	60664.078430	33.546727
869.282881	60775.281413	33.551744
869.963268	60891.041062	33.556762
870.918314	61000.126708	33.561780
871.455016	61114.309682	33.566797
872.422952	61223.707177	33.571815
873.717576	61342.393728	33.576832
874.799748	61453.429001	33.581850
876.068575	61549.290829	33.586868
877.215138	61644.569476	33.591885
878.179185	61743.199596	33.596903
879.242795	61837.813505	33.601920
879.971477	61940.577728	33.606938
880.937301	62019.823423	33.611956
881.899992	62116.216833	33.616973
882.668318	62193.631580	33.621991
883.391702	62269.762243	33.627008
884.190436	62355.638964	33.632026
884.706879	62440.515746	33.637044
885.291687	62541.386144	33.642061
886.137319	62644.817678	33.647079
887.257323	62745.783994	33.652096
887.878192	62853.370349	33.657114
888.652102	62949.024342	33.662132
889.605363	63051.124098	33.667149
890.468633	63153.279776	33.672167
891.143560	63265.726307	33.677184
891.715285	63385.848115	33.682202
892.638335	63491.008841	33.687220
893.396775	63613.865653	33.692237
894.368249	63728.699427	33.697255
895.717637	63842.829502	33.702272
896.480789	63959.816898	33.707290
898.067508	64058.887365	33.712308
899.252881	64155.773614	33.717325
900.095388	64257.894300	33.722343
900.833160	64365.047385	33.727360
901.799724	64473.159495	33.732378
902.662546	64569.931786	33.737396
903.405314	64676.356271	33.742413
904.582184	64784.345083	33.747431
905.643668	64881.286304	33.752448
906.394935	64992.830739	33.757466
907.425204	65093.716380	33.762484
908.273336	65192.976576	33.767501
909.354414	65302.414264	33.772519
910.067204	65396.075213	33.777536
910.890456	65520.048835	33.782554
911.879602	65608.938767	33.787572
912.799579	65727.042688	33.792589
913.557955	65835.940981	33.797607
914.465328	65933.502656	33.802624
915.155569	66050.839715	33.807642
916.241760	66176.171754	33.812660
917.521632	66278.868439	33.817677
918.325734	66382.358358	33.822695
919.328453	66477.421864	33.827712
919.930689	66599.864646	33.832730
920.902648	66698.793877	33.837748
921.864302	66805.912290	33.842765
923.206558	66907.752733	33.847783
924.459251	67008.357154	33.852800
925.308750	67106.347737	33.857818
926.392421	67205.268099	33.862836
928.029468	67299.306068	33.867853
928.724847	67377.991562	33.872871
929.709304	67472.961785	33.877888
930.452049	67574.717923	33.882906
930.999780	67649.062680	33.887924
931.788676	67733.584676	33.892941
932.620122	67818.719384	33.897959
933.958951	67899.275661	33.902976
934.516286	67991.321877	33.907994
935.463977	68074.512357	33.913012
936.634803	68153.693920	33.918029
937.274329	68251.382535	33.923047
938.633737	68333.061874	33.928064
939.248904	68423.047689	33.933082
940.071257	68515.837605	33.938100
940.879261	68610.544521	33.943117
941.867000	68705.646589	33.948135
943.599061	68780.609578	33.953152
944.570861	68862.706607	33.958170
945.611765	68951.679443	33.963188
946.929487	69022.893308	33.968205
947.326955	69111.798668	33.973223
948.326536	69198.334173	33.978240
949.023905	69290.913890	33.983258
950.104017	69378.802060	33.988276
950.773722	69461.865776	33.993293
951.082847	69572.451772	33.998311
952.072138	69672.764369	34.003328
952.940388	69769.906087	34.008346
953.634755	69878.852982	34.013364
954.163457	69995.825663	34.018381
955.008636	70113.690101	34.023399
956.056487	70229.463244	34.028416
957.152271	70359.407713	34.033434
958.211418	70472.349885	34.038452
959.025402	70584.832559	34.043469
959.672254	70710.655366	34.048487
960.764129	70831.075392	34.053504
961.820649	70957.346384	34.058522
962.732618	71077.000401	34.063540
963.679574	71206.266444	34.068557
965.657625	71300.755931	34.073575
967.036861	71395.012574	34.078592
968.367170	71494.610406	34.083610
969.545257	71601.069791	34.088628
970.694979	71697.828687	34.093645
971.500076	71791.666748	34.098663
972.549199	71882.787261	34.103680
973.014705	71980.951747	34.108698
973.972764	72086.696805	34.113716
974.586536	72184.029891	34.118733
975.318886	72308.775025	34.123751
976.139552	72400.768357	34.128768
976.809916	72530.169171	34.133786
977.679129	72646.578848	34.138804
978.743600	72755.444767	34.143821
979.229446	72877.389095	34.148839
980.396621	72994.960348	34.153856
981.522857	73121.878557	34.158874
982.290696	73241.897127	34.163892
983.551949	73345.932351	34.168909
984.401816	73459.487220	34.173927
985.618652	73568.851512	34.178944
986.097877	73686.612111	34.183962
986.951807	73804.579203	34.188980
987.962407	73913.346246	34.193997
988.778483	74034.745845	34.199015
989.767333	74156.030217	34.204032
990.687675	74276.959686	34.209050
991.294006	74399.342787	34.214068
992.524508	74524.066706	34.219085
993.699514	74663.449210	34.224103
994.901563	74779.236910	34.229120
995.902581	74912.543984	34.234138
996.684743	75047.586778	34.239156
998.086727	75171.762883	34.244173
999.030776	75291.595018	34.249191
1000.087144	75408.679798	34.254208
1000.964654	75533.857951	34.259226
1002.076340	75657.065710	34.264244
1003.324358	75791.382081	34.269261
1004.367470	75923.646321	34.274279
1005.288627	76028.008634	34.279296
1006.349291	76167.811546	34.284314
1007.409655	76280.798962	34.289332
1008.680662	76403.309651	34.294349
1009.679093	76530.787916	34.299367
1010.611835	76653.625697	34.304384
1011.869349	76771.823998	34.309402
1012.954984	76885.663999	34.314420
1014.124565	77006.898785	34.319437
1015.062401	77133.853230	34.324455
1016.130625	77249.929148	34.329472
1016.874862	77363.876692	34.334490
1017.909724	77487.733494	34.339508
1019.116611	77614.534356	34.344525
1020.140903	77735.208765	34.349543
1021.179041	77848.562361	34.354560
1022.425763	77965.290257	34.359578
1023.097107	78089.891165	34.364596
1024.457234	78209.099098	34.369613
1025.225996	78334.343354	34.374631
1026.221109	78439.768133	34.379648
1027.195116	78559.816989	34.384666
1028.058626	78690.383161	34.389684
1029.380188	78804.221586	34.394701
1030.525832	78930.951834	34.399719
1031.876884	79050.387328	34.404736
1033.016985	79171.285631	34.409754
1033.785386	79282.894867	34.414772
1035.050790	79403.761959	34.419789
1035.742657	79525.289898	34.424807
1036.805342	79642.587568	34.429824
1037.897979	79755.456270	34.434842
1038.605850	79873.228890	34.439860
1039.562524	79975.652390	34.444877
1040.350851	80087.528293	34.449895
1041.421198	80198.241056	34.454912
1042.671722	80305.796653	34.459930
1043.413442	80431.873395	34.464948
1044.871713	80554.688822	34.469965
1045.571318	80653.414243	34.474983
1046.382242	80773.293286	34.480000
1047.463272	80884.646488	34.485018
1048.559419	81004.127483	34.490036
1049.774621	81123.748268	34.495053
1050.848650	81241.413507	34.500071
1052.034263	81366.198892	34.505088
1053.333193	81487.420489	34.510106
1053.942322	81600.477273	34.515124
1055.103780	81714.761755	34.520141
1056.268274	81845.552788	34.525159
1057.506416	81964.030483	34.530176
1059.137158	82072.059446	34.535194
1060.019355	82176.522322	34.540212
1061.522421	82283.870950	34.545229
1062.515520	82399.614727	34.550247
1063.655357	82511.416116	34.555264
1064.835989	82601.748063	34.560282
1065.664599	82713.637966	34.565300
1067.168664	82823.296779	34.570317
1068.112805	82931.395131	34.575335
1068.957880	83043.808916	34.580352
1070.217211	83142.159911	34.585370
1070.833716	83268.368502	34.590388
1071.817733	83380.616572	34.595405
1072.685835	83500.988955	34.600423
1073.379085	83627.579475	34.605440
1074.344916	83756.245417	34.610458
1075.195474	83884.614353	34.615476
1076.462168	84017.198228	34.620493
1077.290314	84166.518979	34.625511
1078.111879	84301.002655	34.630528
1079.191398	84438.025797	34.635546
1079.940805	84585.686518	34.640564
1080.846233	84730.876551	34.645581
1081.878868	84880.650328	34.650599
1082.810407	85019.806245	34.655616
1084.235003	85189.379854	34.660634
1085.290439	85335.675625	34.665652
1086.099602	85471.660885	34.670669
1087.070527	85637.440564	34.675687
1088.525183	85797.536042	34.680704
1089.682250	85938.824570	34.685722
1090.591377	86105.825422	34.690740
1092.024913	86243.379273	34.695757
1092.874002	86391.542491	34.700775
1094.199613	86545.593791	34.705792
1095.516906	86679.381288	34.710810
1096.437680	86821.358195	34.715828
1097.819298	86944.596082	34.720845
1099.089472	87081.574246	34.725863
1099.837746	87214.393238	34.730880
1101.094994	87336.856396	34.735898
1102.055622	87475.606293	34.740916
1103.313903	87601.504479	34.745933
1104.482562	87736.612202	34.750951
1105.421945	87870.979425	34.755968
1106.674236	88012.209526	34.760986
1107.537059	88147.792149	34.766004
1108.714500	88280.827689	34.771021
1109.982926	88423.107654	34.776039
1110.961526	88555.835021	34.781056
1112.181090	88695.228214	34.786074
1113.231962	88829.571004	34.791092
1115.121362	88955.787755	34.796109
1116.196816	89088.300606	34.801127
1117.304592	89225.229640	34.806144
1118.702678	89353.038288	34.811162
1119.891450	89478.996383	34.816180
1121.207211	89598.142856	34.821197
1121.766807	89734.650015	34.826215
1122.964754	89863.511683	34.831232
1124.359962	89982.742486	34.836250
1125.316747	90116.425153	34.841268
1126.383232	90258.319178	34.846285
1127.782857	90388.916365	34.851303
1129.123861	90508.424280	34.856320
1130.470801	90630.132816	34.861338
1131.716734	90757.796797	34.866356
1132.958339	90868.449210	34.871373
1134.453655	90983.280319	34.876391
1135.686071	91105.414478	34.881408
1137.092560	91214.594082	34.886426
1137.879643	91329.324593	34.891444
1138.763207	91458.030594	34.896461
1139.865774	91572.124000	34.901479
1140.469941	91697.106287	34.906496
1141.795700	91826.882577	34.911514
1142.551956	91954.226584	34.916532
1143.643352	92079.089274	34.921549
1144.566583	92222.871940	34.926567
1145.297678	92356.085462	34.931584
1146.689215	92489.947432	34.936602
1147.721021	92646.802004	34.941620
1148.597526	92794.384507	34.946637
1150.085881	92926.253964	34.951655
1151.403197	93060.289307	34.956672
1153.339129	93173.980139	34.961690
1154.647145	93307.879301	34.966708
1155.729450	93429.917338	34.971725
1157.113649	93560.795082	34.976743
1158.165954	93693.554395	34.981760
1159.397524	93806.152330	34.986778
1160.334278	93928.387026	34.991796
1161.494956	94029.225785	34.996813
1162.356431	94143.857810	35.001831
1163.224644	94258.843579	35.006848
1164.274580	94377.267432	35.011866
1165.207493	94512.207599	35.016884
1166.375154	94633.580778	35.021901
1167.565656	94741.471053	35.026919
1168.629038	94884.280777	35.031936
1169.906728	95011.597291	35.036954
1170.652801	95147.810826	35.041972
1171.635061	95289.396176	35.046989
1172.822653	95430.956090	35.052007
1173.819611	95579.480358	35.057024
1175.318573	95719.948807	35.062042
1175.968550	95873.907210	35.067060
1177.072421	96019.437848	35.072077
1177.937082	96181.569019	35.077095
1178.830371	96335.105979	35.082112
1180.302220	96503.709377	35.087130
1180.989227	96670.528322	35.092148
1182.250626	96846.942601	35.097165
1183.879382	97003.277197	35.102183
1184.830355	97177.529209	35.107200
1185.593097	97339.551997	35.112218
1186.970582	97518.989679	35.117236
1188.317631	97679.985667	35.122253
1189.223582	97852.339403	35.127271
1190.450453	98038.973045	35.132288
1192.036340	98210.126868	35.137306
1193.203354	98387.517056	35.142324
1194.651397	98556.436772	35.147341
1196.462391	98713.253908	35.152359
1197.517675	98881.763963	35.157376
1198.802457	99039.160484	35.162394
1200.065279	99216.807569	35.167412
1201.382931	99378.471825	35.172429
1202.663940	99543.508986	35.177447
1203.792518	99714.082392	35.182464
1204.898241	99860.301526	35.187482
1206.707397	100025.720032	35.192500
1207.985540	100180.278199	35.197517
1209.776418	100315.698409	35.202535
1210.896797	100470.846718	35.207552
1212.571647	100611.329900	35.212570
1213.330030	100765.949303	35.217588
1214.803119	100899.765700	35.222605
1216.742554	101026.390429	35.227623
1217.808499	101164.733884	35.232640
1218.935232	101301.050040	35.237658
1220.034755	101439.478371	35.242676
1221.425985	101569.489836	35.247693
1222.898398	101688.947420	35.252711
1224.039524	101832.098144	35.257728
1225.463630	101950.254935	35.262746
1226.220449	102073.207206	35.267764
1227.162178	102200.490500	35.272781
1228.481733	102319.956628	35.277799
1228.847046	102450.990349	35.282816
1229.915253	102576.749569	35.287834
1230.924890	102717.344868	35.292852
1231.603289	102862.264980	35.297869
1232.559072	103018.633359	35.302887
1233.419229	103188.831896	35.307904
1234.916243	103342.667457	35.312922
1235.865820	103509.101586	35.317940
1236.592873	103673.528295	35.322957
1238.136279	103852.798708	35.327975
1238.897833	104038.276163	35.332992
1239.963116	104212.708319	35.338010
1241.202768	104395.676189	35.343028
1242.460636	104588.337566	35.348045
1243.609573	104771.499943	35.353063
1245.025157	104965.658110	35.358080
1246.314911	105151.072924	35.363098
1247.601313	105336.616281	35.368116
1248.772024	105532.836792	35.373133
1250.430179	105721.133920	35.378151
1251.285716	105917.173529	35.383168
1252.909423	106104.909570	35.388186
1254.092074	106303.621684	35.393204
1255.418888	106490.192811	35.398221
1257.253889	106661.685159	35.403239
1258.922540	106849.786950	35.408256
1260.957241	107003.345470	35.413274
1262.782565	107175.330347	35.418292
1263.852468	107339.360674	35.423309
1265.787832	107490.697607	35.428327
1267.101155	107642.602734	35.433344
1268.745984	107799.892870	35.438362
1270.393494	107920.841292	35.443380
1271.752223	108066.159487	35.448397
1274.119567	108180.190838	35.453415
1275.402537	108298.680050	35.458432
1276.706771	108426.603496	35.463450
1278.204168	108530.318734	35.468468
1279.416325	108646.795506	35.473485
1280.849584	108756.389252	35.478503
1281.842453	108867.730805	35.483520
1283.199508	108987.806619	35.488538
1283.963389	109108.692554	35.493556
1284.832022	109239.278285	35.498573
1286.079715	109370.988086	35.503591
1286.760520	109494.731116	35.508608
1288.211577	109637.145045	35.513626
1289.339322	109771.667444	35.518644
1290.409960	109924.372283	35.523661
1291.865608	110049.950826	35.528679
1292.761125	110193.336130	35.533696
1293.696839	110325.543736	35.538714
1294.731405	110467.085542	35.543732
1295.972136	110608.253573	35.548749
1296.953673	110747.513996	35.553767
1297.856726	110896.940951	35.558784
1298.973596	111051.183609	35.563802
1300.121136	111206.827624	35.568820
1300.717924	111372.846565	35.573837
1302.437601	111534.244366	35.578855
1304.015369	111690.050913	35.583872
1305.484513	111840.172183	35.588890
1306.942794	112000.563756	35.593908
1307.876923	112165.173363	35.598925
1309.341946	112332.174830	35.603943
1310.601432	112495.494155	35.608960
1312.250808	112661.056846	35.613978
1313.451376	112822.944343	35.618996
1314.425004	113001.752416	35.624013
1316.140107	113146.746402	35.629031
1317.757422	113311.894354	35.634048
1318.648344	113482.425937	35.639066
1320.215541	113643.994576	35.644084
1321.690006	113817.423753	35.649101
1323.376877	113987.939870	35.654119
1324.281654	114161.164422	35.659136
1325.162227	114328.183456	35.664154
1326.674461	114498.559853	35.669172
1327.847304	114674.075078	35.674189
1329.246303	114856.931154	35.679207
1330.514242	115036.973086	35.684224
1331.345576	115220.232231	35.689242
1332.888550	115404.449541	35.694260
1333.859418	115597.008615	35.699277
1335.602856	115772.212818	35.704295
1336.877852	115972.748023	35.709312
1338.479435	116150.332597	35.714330
1340.265104	116330.655943	35.719348
1341.263722	116521.052261	35.724365
1342.920713	116696.213233	35.729383
1344.271867	116875.355857	35.734400
1345.603313	117065.728646	35.739418
1346.726030	117247.841670	35.744436
1347.622865	117437.729111	35.749453
1349.316007	117619.798424	35.754471
1350.309660	117807.887676	35.759488
1351.847294	118009.264491	35.764506
1353.372525	118190.914966	35.769524
1354.819678	118383.330592	35.774541
1356.203678	118576.948078	35.779559
1357.537180	118764.407731	35.784576
1359.062712	118948.197327	35.789594
1360.527301	119124.868051	35.794612
1361.938841	119309.191209	35.799629
1363.208951	119497.660354	35.804647
1364.721054	119692.576528	35.809664
1365.999303	119864.406116	35.814682
1367.676243	120032.855371	35.819700
1368.932194	120195.610244	35.824717
1370.455961	120362.388912	35.829735
1371.460628	120529.086501	35.834752
1372.564407	120689.272352	35.839770
1373.893884	120861.961538	35.844788
1375.310248	121038.589518	35.849805
1377.313545	121207.754342	35.854823
1378.019660	121389.715552	35.859840
1379.158527	121567.100419	35.864858
1380.769886	121741.903652	35.869876
1381.750553	121930.170260	35.874893
1383.118857	122111.347255	35.879911
1384.368118	122300.650370	35.884928
1385.408658	122503.970894	35.889946
1386.873941	122692.507856	35.894964
1388.421080	122897.600073	35.899981
1389.785511	123091.602200	35.904999
1391.085856	123297.521998	35.910016
1392.323849	123491.585118	35.915034
1393.889424	123693.729300	35.920052
1395.171159	123916.097576	35.925069
1396.518725	124107.158478	35.930087
1398.047692	124318.825665	35.935104
1399.344111	124526.478153	35.940122
1401.113918	124730.928328	35.945140
1402.144606	124956.245757	35.950157
1403.681351	125151.261366	35.955175
1405.066873	125361.464819	35.960192
1406.605900	125581.690524	35.965210
1408.393044	125774.960763	35.970228
1409.633045	125989.891734	35.975245
1411.103261	126194.413213	35.980263
1412.991379	126404.608188	35.985280
1414.460818	126601.038308	35.990298
1416.019772	126800.584529	35.995316
1417.616154	126996.325924	36.000333
1419.619430	127183.972635	36.005351
1420.855472	127378.329881	36.010368
1422.657618	127563.490226	36.015386
1424.759518	127738.064313	36.020404
1426.631751	127906.075879	36.025421
1428.275171	128068.702812	36.030439
1430.546589	128220.488165	36.035456
1432.111351	128362.391279	36.040474
1433.625435	128519.517999	36.045492
1435.041497	128669.034728	36.050509
1436.400417	128812.455076	36.055527
1437.616547	128953.871869	36.060544
1438.680961	129124.223544	36.065562
1440.232920	129275.723604	36.070580
1441.406307	129427.208631	36.075597
1442.541104	129591.762301	36.080615
1443.828213	129761.360349	36.085632
1444.807682	129918.643264	36.090650
1445.910065	130066.405652	36.095668
1447.147254	130223.966058	36.100685
1448.749050	130374.780018	36.105703
1450.039091	130535.057673	36.110720
1450.981055	130701.954327	36.115738
1452.398189	130863.835350	36.120756
1453.905533	131035.281189	36.125773
1455.051475	131207.393640	36.130791
1456.364814	131378.517638	36.135808
1457.658024	131554.650455	36.140826
1459.053213	131745.541287	36.145844
1460.178339	131941.176888	36.150861
1462.230369	132111.985221	36.155879
1463.771998	132295.761238	36.160896
1465.068641	132492.323640	36.165914
1466.198410	132679.145080	36.170932
1467.281136	132876.897119	36.175949
1468.693322	133062.738580	36.180967
1470.242928	133275.623802	36.185984
1471.825602	133485.109604	36.191002
1473.460211	133683.767835	36.196020
1475.050074	133897.360833	36.201037
1476.017789	134110.800847	36.206055
1477.870762	134313.508777	36.211072
1478.936496	134534.057478	36.216090
1480.931489	134727.026971	36.221108
1482.514022	134938.804175	36.226125
1484.233452	135142.350093	36.231143
1485.791315	135346.759428	36.236160
1487.122596	135546.593737	36.241178
1488.837657	135753.122446	36.246196
1489.656501	135976.952594	36.251213
1491.317483	136188.295576	36.256231
1492.724913	136400.440685	36.261248
1493.924829	136625.152962	36.266266
1495.550148	136840.827483	36.271284
1496.927849	137062.612932	36.276301
1498.041985	137285.405021	36.281319
1499.783709	137520.239279	36.286336
1501.340578	137744.510525	36.291354
1503.607861	137953.095937	36.296372
1505.108501	138186.072882	36.301389
1506.610004	138407.189752	36.306407
1507.755740	138626.438503	36.311424
1509.227166	138855.205243	36.316442
1510.956857	139073.654814	36.321460
1512.520500	139300.331920	36.326477
1513.792788	139524.636429	36.331495
1515.411567	139750.623819	36.336512
1516.718199	139979.590073	36.341530
1518.124768	140211.545829	36.346548
1519.575002	140443.357019	36.351565
1520.967924	140674.874920	36.356583
1522.721386	140911.102690	36.361600
1523.863388	141126.289258	36.366618
1525.366786	141349.873531	36.371636
1527.196273	141570.619328	36.376653
1528.589047	141788.178823	36.381671
1529.715379	142004.159882	36.386688
1530.886511	142228.234301	36.391706
1532.253599	142458.629160	36.396724
1533.688253	142695.631161	36.401741
1534.964709	142937.628608	36.406759
1536.802933	143174.620882	36.411776
1538.046107	143426.627879	36.416794
1539.665661	143665.014869	36.421812
1540.982491	143913.807349	36.426829
1542.585049	144158.703167	36.431847
1544.139225	144409.692748	36.436864
1545.771166	144665.552033	36.441882
1547.528408	144906.563151	36.446900
1549.203056	145168.770205	36.451917
1551.513172	145390.379579	36.456935
1554.184678	145611.223266	36.461952
1555.730350	145844.188041	36.466970
1557.883365	146071.113022	36.471988
1559.294829	146298.258842	36.477005
1560.968328	146513.880063	36.482023
1562.237534	146729.947262	36.487040
1563.384700	146968.409056	36.492058
1564.930245	147179.326848	36.497076
1566.346613	147421.590231	36.502093
1567.775912	147651.759906	36.507111
1569.288841	147891.007153	36.512128
1570.447808	148134.115453	36.517146
1572.064257	148371.017305	36.522164
1573.703244	148622.381773	36.527181
1575.197282	148870.437150	36.532199
1576.784655	149117.237243	36.537216
1578.612840	149371.645372	36.542234
1580.637101	149612.396161	36.547252
1582.074443	149839.981324	36.552269
1583.964035	150079.324410	36.557287
1585.926783	150308.147856	36.562304
1587.437246	150543.383621	36.567322
1589.167234	150771.169674	36.572340
1590.976092	151004.066663	36.577357
1592.566846	151234.223463	36.582375
1594.291984	151460.747269	36.587392
1595.566077	151688.016218	36.592410
1597.689490	151907.899856	36.597428
1599.499094	152138.611405	36.602445
1600.700785	152372.882335	36.607463
1602.298708	152588.010786	36.612480
1603.869262	152822.834867	36.617498
1605.443258	153046.870476	36.622516
1607.041897	153277.205033	36.627533
1608.603223	153504.301308	36.632551
1610.085745	153731.221455	36.637568
1611.493497	153968.665943	36.642586
1612.983072	154179.346129	36.647604
1614.512390	154393.381312	36.652621
1615.365360	154616.743121	36.657639
1617.463152	154841.696482	36.662656
1618.890841	155064.019005	36.667674
1620.322882	155284.757348	36.672692
1621.853136	155521.812888	36.677709
1623.318984	155752.439007	36.682727
1624.832561	155987.408275	36.687744
1626.396700	156228.039037	36.692762
1628.033670	156456.791458	36.697780
1629.657764	156695.742219	36.702797
1631.436613	156947.603819	36.707815
1632.943556	157187.172559	36.712832
1634.187368	157435.407378	36.717850
1635.496155	157683.037673	36.722868
1637.344379	157950.175467	36.727885
1639.214506	158200.370523	36.732903
1640.953422	158441.293256	36.737920
1642.556411	158706.878023	36.742938
1644.650887	158953.758515	36.747956
1646.887246	159193.846569	36.752973
1648.564108	159452.932588	36.757991
1650.376732	159691.430110	36.763008
1652.046466	159933.971889	36.768026
1653.810636	160181.775764	36.773044
1655.580112	160420.957163	36.778061
1657.384717	160663.038656	36.783079
1659.457795	160893.488188	36.788096
1660.840319	161140.750631	36.793114
1662.467453	161372.022288	36.798132
1664.213293	161607.943499	36.803149
1665.798374	161859.997828	36.808167
1667.443551	162084.600512	36.813184
1669.369232	162324.239046	36.818202
1671.146888	162570.687637	36.823220
1672.852172	162795.323237	36.828237
1674.483758	163048.139393	36.833255
1676.309536	163272.898313	36.838272
1677.705822	163515.812066	36.843290
1679.229588	163760.064223	36.848308
1680.973049	163997.459844	36.853325
1681.768800	164256.542812	36.858343
1683.717557	164511.424039	36.863360
1685.627262	164751.347374	36.868378
1686.801871	165016.146239	36.873396
1688.538525	165270.254665	36.878413
1689.777230	165547.692196	36.883431
1691.268853	165802.857824	36.888448
1693.004525	166080.994082	36.893466
1694.501145	166355.454109	36.898484
1696.419319	166621.452682	36.903501
1697.749365	166915.222263	36.908519
1699.659221	167175.201328	36.913536
1701.293889	167446.971111	36.918554
1702.692810	167713.770124	36.923572
1704.477858	167974.078899	36.928589
1705.926531	168228.519391	36.933607
1707.833628	168491.628186	36.938624
1709.433095	168750.195932	36.943642
1711.035699	169013.394710	36.948660
1712.840981	169283.133647	36.953677
1713.939178	169559.392436	36.958695
1716.263624	169825.031721	36.963712
1718.279582	170096.772418	36.968730
1720.190708	170350.328978	36.973748
1721.715953	170626.210422	36.978765
1723.653644	170902.573777	36.983783
1725.842504	171148.835614	36.988800
1728.034953	171414.658905	36.993818
1729.671824	171671.832089	36.998836
1731.820904	171929.889701	37.003853
1733.205711	172196.176311	37.008871
1734.781580	172443.621817	37.013888
1736.478506	172705.346253	37.018906
1738.214405	172974.779083	37.023924
1740.192652	173243.718563	37.028941
1741.636418	173513.112598	37.033959
1743.790189	173772.488027	37.038976
1745.143116	174039.274026	37.043994
1746.536770	174303.619595	37.049012
1749.235506	174566.833588	37.054029
1750.935209	174838.377832	37.059047
1752.670994	175098.944505	37.064064
1754.423444	175374.835346	37.069082
1755.680214	175647.178413	37.074100
1757.779253	175910.648522	37.079117
1759.158296	176202.348216	37.084135
1760.975309	176470.370435	37.089152
1762.546852	176756.106082	37.094170
1763.578697	177045.684701	37.099188
1765.635098	177329.685322	37.104205
1767.312773	177631.218101	37.109223
1768.952410	177916.824009	37.114240
1770.840018	178220.319571	37.119258
1772.245833	178519.719671	37.124276
1774.026080	178821.295429	37.129293
1775.626013	179130.400282	37.134311
1777.618793	179429.396418	37.139328
1779.507753	179734.171345	37.144346
1781.121190	180042.265631	37.149364
1783.155248	180344.979123	37.154381
1784.643315	180655.343451	37.159399
1786.355600	180960.992511	37.164416
1788.160009	181286.168855	37.169434
1789.886170	181597.694801	37.174452
1791.674477	181903.059255	37.179469
1793.486268	182233.392933	37.184487
1795.437034	182545.968468	37.189504
1797.530365	182862.177901	37.194522
1799.380318	183161.653765	37.199540
1801.522437	183442.102849	37.204557
1803.191767	183722.121197	37.209575
1805.545909	183993.366040	37.214592
1807.500454	184266.820403	37.219610
1809.196567	184536.954845	37.224628
1811.332914	184797.707172	37.229645
1813.260099	185085.928335	37.234663
1815.287058	185335.953339	37.239680
1817.252355	185585.240830	37.244698
1818.824192	185854.197344	37.249716
1820.868319	186111.418788	37.254733
1823.082549	186371.152589	37.259751
1825.156211	186638.638177	37.264768
1826.989387	186894.285891	37.269786
1828.491070	187161.154669	37.274804
1830.719438	187418.392212	37.279821
1832.399039	187687.202692	37.284839
1834.241402	187940.951200	37.289856
1836.000053	188206.757267	37.294874
1837.125621	188483.908816	37.299892
1839.130211	188747.826127	37.304909
1840.500871	189031.223645	37.309927
1842.140630	189321.293352	37.314944
1843.823534	189599.073601	37.319962
1845.142056	189903.512680	37.324980
1846.974876	190194.483441	37.329997
1848.382854	190511.348975	37.335015
1850.059304	190822.133152	37.340032
1851.895430	191140.038931	37.345050
1853.635350	191463.330326	37.350068
1855.367723	191784.987910	37.355085
1857.561878	192102.919259	37.360103
1859.484289	192418.839817	37.365120
1861.685124	192729.260946	37.370138
1863.532913	193053.484796	37.375156
1865.578407	193375.306071	37.380173
1867.491104	193701.770206	37.385191
1868.805043	194024.803230	37.390208
1870.994817	194339.132414	37.395226
1872.930546	194669.533571	37.400244
1874.851553	194988.580004	37.405261
1876.776293	195312.006550	37.410279
1878.706673	195636.297294	37.415296
1880.966177	195963.228564	37.420314
1882.513789	196285.147254	37.425332
1885.128391	196594.168269	37.430349
1886.982248	196918.491870	37.435367
1889.192337	197229.383153	37.440384
1890.969463	197535.839166	37.445402
1892.800805	197854.460500	37.450420
1895.035579	198159.324383	37.455437
1896.902383	198463.017223	37.460455
1898.958815	198777.242070	37.465472
1900.564077	199071.485682	37.470490
1902.181684	199370.158764	37.475508
1904.464197	199646.032936	37.480525
1906.038133	199940.400482	37.485543
1907.551071	200234.817376	37.490560
1909.306466	200524.665912	37.495578
1910.879785	200829.434043	37.500596
1912.972274	201122.481696	37.505613
1914.911359	201427.601262	37.510631
1916.488158	201736.575338	37.515648
1918.469375	202033.516952	37.520666
1920.460129	202349.778263	37.525684
1922.232318	202655.679930	37.530701
1924.157487	202978.987458	37.535719
1925.946881	203284.508975	37.540736
1927.961833	203602.385543	37.545754
1929.619413	203943.474332	37.550772
1931.661099	204260.906011	37.555789
1933.718396	204580.964629	37.560807
1935.444320	204921.045499	37.565824
1937.152318	205258.973173	37.570842
1939.680776	205581.615596	37.575860
1942.412906	205883.649900	37.580877
1944.791641	206200.353114	37.585895
1946.921209	206519.293703	37.590912
1949.000801	206830.322517	37.595930
1951.034248	207136.371275	37.600948
1952.934678	207439.776809	37.605965
1954.622026	207765.027267	37.610983
1956.672824	208071.788901	37.616000
1958.893432	208384.897960	37.621018
1960.552250	208705.410054	37.626036
1962.711302	209018.824086	37.631053
1964.649713	209327.425192	37.636071
1966.622404	209649.720447	37.641088
1968.799294	209967.503546	37.646106
1970.310965	210288.796140	37.651124
1972.497302	210609.856354	37.656141
1974.310873	210937.934420	37.661159
1976.082166	211268.267975	37.666176
1977.866503	211595.744661	37.671194
1979.394917	211932.455229	37.676212
1981.473665	212263.100557	37.681229
1983.533581	212609.213945	37.686247
1984.857794	212951.814896	37.691264
1987.205741	213293.302992	37.696282
1989.071004	213640.239811	37.701300
1990.889009	213991.350216	37.706317
1992.669349	214340.843335	37.711335
1994.649830	214705.770387	37.716352
1996.408546	215055.626112	37.721370
1997.979393	215439.006171	37.726388
1999.875792	215802.758964	37.731405
2001.678517	216181.027816	37.736423
2003.818756	216561.555924	37.741440
2005.817009	216926.085596	37.746458
2007.567433	217283.140085	37.751476
2009.658899	217635.254041	37.756493
2011.864349	217991.554262	37.761511
2013.695879	218348.956711	37.766528
2015.811321	218703.649540	37.771546
2017.644916	219070.514363	37.776564
2019.452587	219431.709586	37.781581
2021.463640	219793.496461	37.786599
2023.313581	220176.349752	37.791616
2025.275841	220570.919362	37.796634
2027.152856	220979.712767	37.801652
2029.218281	221357.433576	37.806669
2030.898875	221748.333680	37.811687
2032.930713	222148.296792	37.816704
2035.629034	222518.444094	37.821722
2037.619800	222910.138870	37.826740
2040.084210	223291.107150	37.831757
2042.430532	223667.321669	37.836775
2044.324657	224051.863225	37.841792
2046.660689	224434.419141	37.846810
2048.637633	224811.713428	37.851828
2050.693489	225201.377398	37.856845
2053.293736	225578.830282	37.861863
2055.349817	225961.399630	37.866880
2057.731234	226333.024157	37.871898
2059.972063	226722.703984	37.876916
2062.191330	227086.357710	37.881933
2064.429821	227455.952710	37.886951
2065.904707	227843.625836	37.891968
2068.046307	228215.728311	37.896986
2070.018301	228601.065622	37.902004
2071.973780	228980.845299	37.907021
2073.941664	229372.510443	37.912039
2075.911958	229762.449899	37.917056
2078.000582	230149.451571	37.922074
2080.349715	230549.417009	37.927092
2083.041017	230931.170696	37.932109
2085.902900	231276.504152	37.937127
2088.132171	231653.864108	37.942144
2090.884663	232013.186338	37.947162
2093.315609	232358.973069	37.952180
2095.060383	232720.946794	37.957197
2097.574724	233070.557930	37.962215
2099.296045	233420.016729	37.967232
2101.447850	233769.433873	37.972250
2103.539349	234132.119731	37.977268
2105.705516	234482.400628	37.982285
2107.942451	234824.315403	37.987303
2109.362698	235188.076652	37.992320
2111.520378	235538.870480	37.997338
2114.115855	235891.754939	38.002356
2116.794712	236228.448298	38.007373
2119.054057	236576.740378	38.012391
2121.054307	236928.681346	38.017408
2123.308516	237251.729823	38.022426
2124.956481	237575.942182	38.027444
2126.848934	237889.982426	38.032461
2128.748652	238208.695878	38.037479
2130.363221	238541.094927	38.042496
2132.400755	238873.732659	38.047514
2133.889016	239214.332335	38.052532
2135.992618	239561.413913	38.057549
2137.793233	239911.668745	38.062567
2139.495242	240258.130299	38.067584
2141.507376	240621.358359	38.072602
2143.189522	241001.124394	38.077620
2144.754480	241375.220610	38.082637
2147.040079	241757.712687	38.087655
2149.201554	242157.573927	38.092672
2150.897455	242550.449021	38.097690
2153.228591	242961.080989	38.102708
2155.467284	243364.845426	38.107725
2157.371444	243764.473095	38.112743
2159.485387	244179.715430	38.117760
2161.515844	244586.386886	38.122778
2163.535269	245016.709354	38.127796
2165.280356	245441.107495	38.132813
2167.459495	245882.278847	38.137831
2169.354153	246329.135695	38.142848
2171.750605	246760.851549	38.147866
2174.026175	247209.377962	38.152884
2176.196204	247647.711202	38.157901
2178.712439	248092.722132	38.162919
2180.872125	248539.975410	38.167936
2183.336483	248980.526490	38.172954
2185.770490	249428.348417	38.177972
2187.938075	249880.100268	38.182989
2190.320505	250315.486067	38.188007
2192.344296	250765.612026	38.193024
2194.766572	251217.098472	38.198042
2196.952511	251656.938749	38.203060
2199.311659	252102.849090	38.208077
2201.802846	252550.263705	38.213095
2203.843507	252993.280105	38.218112
2206.538723	253432.078618	38.223130
2208.998862	253866.063615	38.228148
2210.895721	254315.634199	38.233165
2213.603499	254751.283805	38.238183
2215.816901	255201.365003	38.243200
2218.417102	255619.937784	38.248218
2220.819647	256048.932287	38.253236
2222.912796	256477.392437	38.258253
2226.130133	256886.801123	38.263271
2228.467623	257301.938609	38.268288
2230.892708	257712.109444	38.273306
2233.426518	258114.719175	38.278324
2235.511055	258510.872334	38.283341
2238.192819	258906.651982	38.288359
2240.547198	259302.814385	38.293376
2243.141254	259685.806165	38.298394
2245.558108	260046.294336	38.303412
2248.422949	260377.219302	38.308429
2251.333977	260705.241408	38.313447
2253.566429	261036.750060	38.318464
2255.651855	261357.587784	38.323482
2257.689469	261700.838780	38.328500
2259.514658	262031.701803	38.333517
2261.364760	262375.567526	38.338535
2263.104971	262721.330848	38.343552
2264.896056	263061.421584	38.348570
2267.153751	263429.559816	38.353588
2268.977183	263793.982221	38.358605
2271.196391	264165.455089	38.363623
2273.009887	264541.895439	38.368640
2274.880391	264930.927050	38.373658
2277.343114	265314.276431	38.378676
2278.916171	265721.442963	38.383693
2280.860676	266118.084848	38.388711
2283.069512	266528.148855	38.393728
2284.949928	266951.246321	38.398746
2287.626397	267379.857433	38.403764
2289.794796	267806.923618	38.408781
2291.774121	268228.101119	38.413799
2293.730486	268670.341881	38.418816
2295.900590	269121.922868	38.423834
2298.284240	269561.860949	38.428852
2300.224090	270010.506773	38.433869
2302.837542	270473.119495	38.438887
2305.590186	270923.440539	38.443904
2308.061260	271355.211132	38.448922
2311.201241	271801.889234	38.453940
2313.580649	272254.353015	38.458957
2315.966055	272689.033582	38.463975
2318.275517	273137.393315	38.468992
2320.994884	273572.275136	38.474010
2323.759221	274011.138215	38.479028
2325.939621	274458.604044	38.484045
2328.435228	274880.768916	38.489063
2330.512101	275316.108323	38.494080
2333.140583	275747.549741	38.499098
2335.611260	276181.404048	38.504116
2337.879091	276610.108146	38.509133
2340.805925	277034.490724	38.514151
2342.993520	277472.784427	38.519168
2345.203293	277888.186034	38.524186
2347.845566	278320.513801	38.529204
2349.903498	278755.626789	38.534221
2352.498630	279181.229785	38.539239
2354.607396	279604.597976	38.544256
2356.889793	280039.344519	38.549274
2359.004622	280472.440758	38.554292
2361.444867	280911.861371	38.559309
2364.014311	281346.688620	38.564327
2366.081034	281777.683146	38.569344
2368.727433	282191.920937	38.574362
2370.959459	282603.150307	38.579380
2372.835264	283023.479352	38.584397
2375.449390	283422.301527	38.589415
2377.339230	283825.861544	38.594432
2379.621323	284237.919873	38.599450
2382.210718	284653.129885	38.604468
2383.674135	285085.741239	38.609485
2386.025189	285509.421961	38.614503
2388.303001	285960.803106	38.619520
2390.251652	286396.511413	38.624538
2392.446346	286845.491321	38.629556
2394.412738	287305.811113	38.634573
2396.746524	287764.751064	38.639591
2399.178423	288246.816776	38.644608
2401.199832	288720.462243	38.649626
2403.672308	289203.231239	38.654644
2405.839584	289683.482106	38.659661
2408.457601	290165.235647	38.664679
2411.009012	290663.383551	38.669696
2413.314055	291151.332297	38.674714
2416.313735	291631.676242	38.679732
2418.730725	292124.406374	38.684749
2421.581890	292601.825207	38.689767
2424.588639	293074.899980	38.694784
2427.403458	293564.972900	38.699802
2430.159810	294042.810094	38.704820
2432.542912	294515.853542	38.709837
2435.171017	294991.981534	38.714855
2437.654145	295462.187290	38.719872
2440.196946	295937.970903	38.724890
2442.880178	296405.424645	38.729908
2445.148724	296881.909807	38.734925
2447.500315	297359.269635	38.739943
2449.933575	297836.462842	38.744960
2451.920854	298324.292530	38.749978
2454.631193	298796.841494	38.754996
2456.870411	299290.521664	38.760013
2459.291928	299778.278338	38.765031
2461.843344	300258.011530	38.770048
2464.055759	300749.252985	38.775066
2466.903325	301230.612775	38.780084
2469.042516	301723.844041	38.785101
2472.016140	302220.675412	38.790119
2474.734274	302705.302341	38.795136
2477.195872	303208.129937	38.800154
2479.604557	303685.233151	38.805172
2481.945325	304178.779764	38.810189
2484.331042	304664.494103	38.815207
2486.828369	305166.165947	38.820224
2489.552477	305654.794958	38.825242
2492.510479	306136.552404	38.830260
2496.281821	306601.465823	38.835277
2499.290610	307046.025870	38.840295
2502.253036	307493.207902	38.845312
2504.772505	307939.315518	38.850330
2507.651409	308343.276962	38.855348
2510.178807	308742.415997	38.860365
2512.639293	309147.050643	38.865383
2515.063293	309531.776381	38.870400
2517.370623	309940.928299	38.875418
2519.986986	310332.275589	38.880436
2521.811627	310736.522868	38.885453
2524.189214	311147.310298	38.890471
2526.623383	311560.881162	38.895488
2528.471657	311990.951117	38.900506
2530.727616	312413.716075	38.905524
2532.779578	312860.208851	38.910541
2534.805257	313300.786012	38.915559
2536.850924	313752.533577	38.920576
2538.460027	314237.214069	38.925594
2540.950700	314706.767537	38.930612
2543.353524	315199.089635	38.935629
2545.551067	315693.854677	38.940647
2547.897749	316216.175898	38.945664
2550.222460	316728.567243	38.950682
2552.520550	317236.820262	38.955700
2554.627588	317772.987453	38.960717
2557.021290	318314.693634	38.965735
2559.959486	318851.535709	38.970752
2562.100835	319403.688426	38.975770
2564.781608	319956.793615	38.980788
2567.203765	320504.018910	38.985805
2569.368083	321086.837081	38.990823
2572.274430	321648.556288	38.995840
2574.722952	322229.493258	39.000858
2577.558907	322799.546132	39.005876
2580.206577	323372.596337	39.010893
2582.779485	323943.546610	39.015911
2585.867776	324515.630287	39.020928
2588.617804	325104.575371	39.025946
2591.500148	325668.861754	39.030964
2594.371229	326237.767855	39.035981
2596.953471	326805.090345	39.040999
2599.988794	327384.551824	39.046016
2602.389265	327949.431474	39.051034
2605.746254	328515.602907	39.056052
2608.317023	329074.327188	39.061069
2611.344929	329635.336530	39.066087
2614.540329	330178.691789	39.071104
2617.004224	330738.944097	39.076122
2619.485169	331291.647540	39.081140
2622.415513	331826.398715	39.086157
2625.417486	332373.881844	39.091175
2628.159922	332909.187884	39.096192
2631.127044	333440.010526	39.101210
2634.096775	333973.266370	39.106228
2636.915952	334505.602413	39.111245
2639.580713	335035.317983	39.116263
2642.446998	335547.324737	39.121280
2644.708880	336059.194791	39.126298
2647.035009	336552.895811	39.131316
2649.797085	337040.988776	39.136333
2652.042399	337528.575956	39.141351
2654.264705	338022.206153	39.146368
2656.269090	338534.656211	39.151386
2658.813776	339044.782211	39.156404
2661.129645	339563.242974	39.161421
2663.536987	340085.087242	39.166439
2666.057089	340608.838911	39.171456
2668.419983	341150.459971	39.176474
2670.897072	341690.560184	39.181492
2673.332386	342233.124971	39.186509
2675.924062	342791.299717	39.191527
2678.624887	343351.229181	39.196544
2680.941746	343920.912577	39.201562
2684.030725	344478.840356	39.206580
2686.897902	345049.517319	39.211597
2689.231457	345618.648359	39.216615
2692.401232	346183.858586	39.221632
2695.129864	346768.173499	39.226650
2697.970319	347335.150751	39.231668
2700.805127	347913.927988	39.236685
2703.354570	348492.414376	39.241703
2706.514239	349072.245071	39.246720
2709.032737	349645.672381	39.251738
2712.481248	350213.970767	39.256756
2716.147064	350771.643050	39.261773
2718.801745	351340.055250	39.266791
2721.924374	351886.784763	39.271808
2724.723904	352453.283598	39.276826
2727.438541	352993.339307	39.281844
2730.132232	353555.172235	39.286861
2732.941409	354108.604122	39.291879
2735.930316	354669.388170	39.296896
2738.061261	355222.179287	39.301914
2741.076440	355766.600265	39.306932
2743.886243	356339.577967	39.311949
2746.441770	356915.914444	39.316967
2749.492742	357467.367486	39.321984
2752.032504	358033.845169	39.327002
2754.261733	358615.365912	39.332020
2756.751161	359189.147990	39.337037
2759.368956	359784.045169	39.342055
2762.053005	360351.538854	39.347072
2764.520402	360945.760089	39.352090
2767.168322	361539.894500	39.357108
2769.888703	362141.217713	39.362125
2772.121982	362738.498854	39.367143
2775.291472	363341.385055	39.372160
2777.883821	363962.272016	39.377178
2780.398059	364573.392272	39.382196
2783.129162	365190.992067	39.387213
2785.727924	365812.487106	39.392231
2788.825552	366431.788203	39.397248
2791.279540	367052.223023	39.402266
2793.853550	367642.990370	39.407284
2796.579441	368235.654290	39.412301
2799.104137	368835.320342	39.417319
2802.621237	369411.069519	39.422336
2804.925729	370015.829110	39.427354
2807.900369	370602.229586	39.432372
2810.813905	371195.203605	39.437389
2813.478504	371788.919176	39.442407
2816.596636	372387.680016	39.447424
2818.921778	373004.953452	39.452442
2821.705227	373620.673494	39.457460
2824.386260	374246.448063	39.462477
2826.926396	374873.300993	39.467495
2829.851429	375503.635359	39.472512
2832.224327	376133.210044	39.477530
2835.027027	376767.400432	39.482548
2838.020684	377407.867765	39.487565
2840.741387	378060.875433	39.492583
2843.780344	378703.978439	39.497600
2846.464265	379358.847692	39.502618
2849.479053	380021.188084	39.507636
2852.454250	380685.781177	39.512653
2855.078123	381347.678642	39.517671
2857.992476	382007.210193	39.522688
2861.085679	382687.020991	39.527706
2863.987737	383350.944910	39.532724
2867.144047	384024.050093	39.537741
2870.050618	384697.715315	39.542759
2873.041166	385351.164228	39.547776
2876.091182	386031.605625	39.552794
2879.224079	386699.795625	39.557812
2882.215660	387369.644352	39.562829
2885.312884	388049.989729	39.567847
2888.162642	388715.447993	39.572864
2890.972417	389394.418345	39.577882
2893.724878	390069.758013	39.582900
2896.801931	390744.018902	39.587917
2899.551200	391424.405334	39.592935
2902.669057	392103.122423	39.597952
2905.056272	392782.499786	39.602970
2907.972326	393471.543428	39.607988
2910.907260	394161.660646	39.613005
2913.644161	394857.526221	39.618023
2917.041876	395535.547709	39.623040
2919.731420	396241.104322	39.628058
2922.820402	396938.595419	39.633076
2925.749665	397631.583743	39.638093
2928.447849	398330.654153	39.643111
2931.715439	399020.872011	39.648128
2934.578114	399719.455731	39.653146
2937.567181	400420.438433	39.658164
2940.660383	401104.072934	39.663181
2943.864122	401808.490274	39.668199
2947.038840	402490.941408	39.673216
2949.698543	403177.338260	39.678234
2952.499438	403850.641884	39.683252
2955.427669	404490.954771	39.688269
2958.042639	405151.660501	39.693287
2960.934262	405804.855575	39.698304
2963.496896	406470.788950	39.703322
2965.986074	407136.085848	39.708340
2969.150193	407809.702446	39.713357
2971.914632	408480.427102	39.718375
2975.063070	409166.715309	39.723392
2977.912898	409856.811807	39.728410
2980.981960	410533.323047	39.733428
2983.988243	411221.361038	39.738445
2986.726824	411919.842166	39.743463
2989.987617	412611.482625	39.748480
2993.290813	413317.064410	39.753498
2996.062124	414003.427407	39.758516
2999.697980	414686.799080	39.763533
3002.573312	415392.677091	39.768551
3005.736057	416090.003081	39.773568
3008.657272	416779.469462	39.778586
3011.567105	417492.588446	39.783604
3014.903160	418190.849320	39.788621
3017.793405	418908.699563	39.793639
3020.682349	419616.041792	39.798656
3023.781744	420335.798808	39.803674
3026.762207	421047.625680	39.808692
3029.889059	421765.694440	39.813709
3032.629631	422494.294463	39.818727
3035.631664	423212.193221	39.823744
3039.186602	423936.243118	39.828762
3042.166877	424664.696657	39.833780
3045.089466	425388.731829	39.838797
3048.028428	426128.374744	39.843815
3051.679348	426855.548268	39.848832
3054.814649	427578.198708	39.853850
3057.679469	428309.636392	39.858868
3060.782430	429028.630173	39.863885
3063.894688	429773.969732	39.868903
3066.965174	430500.222874	39.873920
3069.794403	431240.069206	39.878938
3072.748168	431999.806485	39.883956
3075.548216	432739.994379	39.888973
3078.461110	433497.009381	39.893991
3081.725142	434254.984662	39.899008
3084.808245	435005.672847	39.904026
3088.002397	435774.680006	39.909044
3091.183055	436531.511356	39.914061
3094.358086	437295.739771	39.919079
3097.450079	438047.956110	39.924096
3100.768982	438792.897694	39.929114
3104.131615	439550.469224	39.934132
3107.507550	440291.811838	39.939149
3110.748087	441035.583852	39.944167
3114.192560	441781.731255	39.949184
3117.118135	442517.862180	39.954202
3120.069095	443233.917292	39.959220
3122.991922	443935.374601	39.964237
3126.208770	444645.118239	39.969255
3128.786812	445339.298606	39.974272
3131.948433	446053.565208	39.979290
3134.760352	446770.396647	39.984308
3138.000584	447475.445127	39.989325
3140.578982	448211.707821	39.994343
3143.658763	448928.835800	39.999360
3146.733856	449655.711255	40.004378
3149.164902	450408.833335	40.009396
3152.844112	451148.270394	40.014413
3155.317337	451908.270601	40.019431
3158.398121	452677.410901	40.024448
3161.516130	453446.367471	40.029466
3164.520685	454228.523973	40.034484
3167.668928	455013.059593	40.039501
3170.417944	455805.727286	40.044519
3173.550623	456598.963968	40.049536
3176.966650	457395.416442	40.054554
3179.696537	458206.065288	40.059572
3183.069994	459025.689596	40.064589
3186.221121	459833.732658	40.069607
3190.115070	460642.286014	40.074624
3193.514947	461457.008743	40.079642
3196.481057	462275.361116	40.084660
3200.138633	463088.261581	40.089677
3203.247980	463904.202383	40.094695
3206.945363	464731.501012	40.099712
3210.857935	465542.497387	40.104730
3214.116145	466364.086334	40.109748
3217.996498	467154.896014	40.114765
3222.159343	467945.378348	40.119783
3225.184805	468735.454385	40.124800
3229.123426	469505.987713	40.129818
3232.190564	470296.250652	40.134836
3235.481439	471065.463008	40.139853
3238.433681	471857.909144	40.144871
3241.730784	472636.871075	40.149888
3245.012331	473414.946193	40.154906
3248.014051	474206.585425	40.159924
3251.312558	474978.783633	40.164941
3254.825396	475756.226584	40.169959
3257.751176	476551.678415	40.174976
3260.829105	477349.450415	40.179994
3263.515329	478145.432659	40.185012
3267.054845	478935.991192	40.190029
3270.414797	479738.272786	40.195047
3273.956243	480537.258256	40.200064
3277.127462	481332.479178	40.205082
3279.981055	482135.349206	40.210100
3283.323293	482939.170071	40.215117
3286.555279	483752.475399	40.220135
3289.721825	484559.086580	40.225152
3292.771027	485355.627036	40.230170
3295.658228	486149.178829	40.235188
3298.922946	486920.356113	40.240205
3301.714481	487688.747590	40.245223
3304.961744	488472.747995	40.250240
3308.392343	489259.869527	40.255258
3311.533706	490032.353799	40.260276
3315.021464	490819.602870	40.265293
3317.961674	491607.511433	40.270311
3321.668636	492379.051335	40.275328
3325.194172	493177.660455	40.280346
3328.274838	493978.426597	40.285364
3331.784292	494763.837714	40.290381
3335.470663	495577.316853	40.295399
3338.712242	496385.224532	40.300416
3341.948363	497182.290638	40.305434
3344.733611	498003.125767	40.310452
3348.271762	498827.843930	40.315469
3351.344516	499660.777300	40.320487
3353.932336	500494.556381	40.325504
3357.568482	501332.169597	40.330522
3360.218289	502191.859593	40.335540
3363.567921	503053.921218	40.340557
3366.503150	503938.368186	40.345575
3369.892510	504819.417844	40.350592
3373.162293	505702.208568	40.355610
3376.615047	506591.032578	40.360628
3380.289717	507479.927351	40.365645
3383.703294	508392.132780	40.370663
3386.842044	509285.611535	40.375680
3390.171087	510196.775655	40.380698
3393.379898	511115.377864	40.385716
3397.055491	512041.878962	40.390733
3400.570950	512965.579809	40.395751
3403.320912	513900.803062	40.400768
3406.759851	514835.613098	40.405786
3410.255560	515779.593100	40.410804
3414.053929	516719.789596	40.415821
3417.128060	517642.999293	40.420839
3420.556243	518593.790311	40.425856
3424.427457	519546.322368	40.430874
3427.655217	520501.472684	40.435892
3431.382103	521451.697745	40.440909
3434.631057	522415.456268	40.445927
3437.863168	523384.353402	40.450944
3442.322614	524309.538682	40.455962
3446.176781	525249.840264	40.460980
3450.010850	526195.836686	40.465997
3453.857424	527121.813277	40.471015
3457.234084	528045.592324	40.476032
3461.163676	528980.369012	40.481050
3464.308903	529919.397410	40.486068
3467.474821	530835.738353	40.491085
3471.077845	531775.641530	40.496103
3474.260617	532703.057608	40.501120
3478.190920	533626.438482	40.506125
3481.291843	534498.746315	40.511130
3484.372559	535315.345104	40.516135
3487.553764	536090.972929	40.521140
3490.359716	536788.589183	40.526144
3493.257264	537411.817452	40.531149
3495.862309	538018.148315	40.536154
3498.487506	538533.854653	40.541159
3500.811795	538979.801901	40.546164
3502.683486	539390.055440	40.551168
3504.983523	539722.415591	40.556173
3506.651360	540026.389042	40.561178
3508.254837	540288.860214	40.566183
3510.036385	540492.827086	40.571188
3511.417214	540665.094386	40.576192
3513.388629	540765.162858	40.581197
3514.367147	540852.713976	40.586202
3515.420952	540887.336776	40.591207
3516.634163	540888.558888	40.596212
3517.187536	540886.047863	40.601216
3518.010076	540808.310958	40.606221
3518.710785	540745.387317	40.611226
3519.406618	540644.240896	40.616231
3520.014615	540527.303199	40.621236
3520.335644	540382.688737	40.626240
3521.165064	540215.673939	40.631245
3521.470531	540047.124257	40.636250
3521.860282	539852.554043	40.641255
3521.754403	539658.514124	40.646260
3521.885505	539435.802365	40.651264
3522.036739	539212.680163	40.656269
3522.186914	538986.726915	40.661274
3522.107130	538748.080772	40.666279
3522.012458	538504.433697	40.671284
3522.090830	538263.734932	40.676288
3522.483434	538006.872573	40.681293
3522.105457	537745.834925	40.686298
3521.793092	537486.752077	40.691303
3521.948142	537220.469810	40.696308
3521.641888	536963.851841	40.701312
3521.680154	536704.094228	40.706317
3521.323985	536439.798392	40.711322
3521.340179	536168.822590	40.716327
3521.176961	535904.234479	40.721332
3520.778085	535640.032619	40.726336
3520.946335	535369.271216	40.731341
3520.655187	535123.984952	40.736346
3520.604085	534866.281324	40.741351
3520.260438	534601.396235	40.746356
3520.039171	534342.094315	40.751360
3519.609941	534099.187726	40.756365
3519.631181	533835.141088	40.761370
3519.308930	533579.024814	40.766375
3518.839329	533329.191745	40.771380
3518.823043	533091.912542	40.776384
3518.896842	532835.973988	40.781389
3518.456026	532608.100492	40.786394
3518.224851	532363.821889	40.791399
3518.180259	532122.238113	40.796404
3518.085020	531891.823967	40.801408
3518.020697	531659.229051	40.806413
3517.441665	531423.175368	40.811418
3517.460854	531186.316231	40.816423
3517.382366	530958.715030	40.821428
3517.077441	530737.815708	40.826432
3517.156384	530522.865251	40.831437
3516.797998	530296.814463	40.836442
3516.450734	530081.470573	40.841447
3516.271876	529864.682314	40.846452
3515.909629	529669.192856	40.851456
3515.927648	529448.679115	40.856461
3515.735896	529250.479424	40.861466
3515.509495	529032.878734	40.866471
3515.574469	528847.013545	40.871476
3515.232107	528643.574721	40.876480
3515.182279	528435.589591	40.881485
3515.031325	528260.464654	40.886490
3514.588543	528066.332471	40.891495
3514.219317	527877.947264	40.896500
3514.219892	527692.735645	40.901504
3514.215877	527520.813580	40.906509
3513.582668	527344.087043	40.911514
3513.480544	527171.317577	40.916519
3513.281352	527010.690624	40.921524
3513.038258	526840.567803	40.926528
3513.127940	526679.032695	40.931533
3512.937436	526519.814499	40.936538
3512.784761	526357.758508	40.941543
3512.502912	526210.883359	40.946548
3511.594023	526050.257807	40.951552
3511.986985	525915.706305	40.956557
3511.768486	525767.553536	40.961562
3512.110848	525629.216998	40.966567
3511.616852	525498.137942	40.971572
3511.336489	525368.338162	40.976576
3511.547753	525224.661302	40.981581
3511.288939	525083.433008	40.986586
3511.326375	524955.449775	40.991591
3511.384682	524826.249152	40.996596
3511.159628	524688.347987	41.001600
3510.925597	524556.765237	41.006605
3510.659349	524441.057894	41.011610
3510.710457	524320.548219	41.016615
3510.767497	524196.751176	41.021620
3509.998328	524081.322917	41.026624
3510.392442	523957.369664	41.031629
3510.142555	523856.465891	41.036634
3509.898322	523735.594135	41.041639
3510.141881	523622.479377	41.046644
3509.664888	523514.431485	41.051648
3509.573503	523416.937222	41.056653
3509.635452	523310.723648	41.061658
3509.274495	523200.431142	41.066663
3509.259977	523107.775634	41.071668
3509.180363	523012.400168	41.076672
3508.901581	522909.675231	41.081677
3509.231354	522810.038167	41.086682
3508.857140	522710.966717	41.091687
3508.844335	522636.304467	41.096692
3508.596899	522544.996887	41.101696
3508.759359	522444.221327	41.106701
3508.602418	522372.259900	41.111706
3508.419689	522279.828448	41.116711
3508.273259	522196.692457	41.121716
3507.983567	522117.471271	41.126720
3508.532104	522037.611681	41.131725
3508.188800	521968.357243	41.136730
3508.276498	521879.823948	41.141735
3508.268876	521797.624497	41.146740
3507.844447	521719.534854	41.151744
3507.687200	521641.705934	41.156749
3507.638390	521577.256520	41.161754
3507.551432	521502.196335	41.166759
3507.772854	521431.485368	41.171764
3507.437536	521353.935991	41.176768
3507.931643	521295.415751	41.181773
3507.710030	521231.497837	41.186778
3507.563829	521152.451491	41.191783
3507.535140	521082.536881	41.196788
3507.549839	521015.294610	41.201792
3507.462998	520944.175241	41.206797
3507.260318	520879.444046	41.211802
3507.400896	520820.371295	41.216807
3507.416865	520752.470497	41.221812
3507.208452	520689.458403	41.226816
3507.097257	520631.486470	41.231821
3507.231094	520576.610191	41.236826
3506.998636	520505.056904	41.241831
3507.015260	520448.833654	41.246836
3506.843496	520389.202011	41.251840
3506.976286	520327.044643	41.256845
3506.858963	520269.173510	41.261850
3506.722451	520223.591037	41.266855
3506.939788	520165.717204	41.271860
3506.875918	520109.202153	41.276864
3506.992905	520042.799221	41.281869
3506.626995	519985.320290	41.286874
3506.519764	519936.547129	41.291879
3506.471202	519888.826309	41.296884
3506.357274	519847.031216	41.301888
3506.690899	519792.221851	41.306893
3506.536063	519738.298473	41.311898
3506.286295	519702.793977	41.316903
3506.660846	519643.932803	41.321908
3506.123284	519592.850278	41.326912
3506.143805	519547.190541	41.331917
3505.880640	519521.850537	41.336922
3505.858483	519471.495151	41.341927
3505.962345	519423.394956	41.346932
3505.753015	519386.164294	41.351936
3506.090658	519340.150491	41.356941
3505.826459	519310.360895	41.361946
3505.854403	519268.339657	41.366951
3505.752139	519235.793989	41.371956
3505.818686	519196.092317	41.376960
3505.917682	519165.183249	41.381965
3505.939999	519123.769278	41.386970
3505.654935	519074.920536	41.391975
3505.878103	519035.446535	41.396980
3505.546884	519006.172606	41.401984
3505.982417	518963.226601	41.406989
3505.667077	518927.629666	41.411994
3505.568612	518896.296236	41.416999
3505.712745	518864.772713	41.422004
3505.918800	518822.722186	41.427008
3506.115639	518784.819206	41.432013
3505.740421	518750.950507	41.437018
3505.485831	518702.803733	41.442023
3505.818935	518675.699581	41.447028
3505.411881	518639.712008	41.452032
3505.620104	518593.109806	41.457037
3505.449905	518575.135987	41.462042
3505.412080	518537.117834	41.467047
3505.532164	518511.311184	41.472052
3505.655052	518481.256649	41.477056
3505.634430	518444.095156	41.482061
3505.257512	518418.821994	41.487066
3505.464704	518370.297874	41.492071
3505.460476	518342.184633	41.497076
3505.362799	518323.592299	41.502080
3505.535265	518287.461797	41.507085
3505.331597	518254.323436	41.512090
3505.138308	518234.279728	41.517095
3505.417652	518201.216614	41.522100
3505.235153	518171.159215	41.527104
3505.487454	518131.880707	41.532109
3505.281429	518117.198800	41.537114
3505.107329	518083.600334	41.542119
3505.444043	518050.072760	41.547124
3505.302334	518025.672000	41.552128
3505.456635	517987.925610	41.557133
3505.645781	517968.326793	41.562138
3505.852059	517935.122997	41.567143
3505.485150	517890.885184	41.572148
3505.220111	517860.789700	41.577152
3505.331167	517831.241513	41.582157
3505.193972	517824.386244	41.587162
3505.282993	517793.071650	41.592167
3505.244111	517756.973392	41.597172
3505.239766	517728.404025	41.602176
3505.133735	517702.834117	41.607181
3505.184291	517677.542821	41.612186
3505.128975	517645.441692	41.617191
3505.218865	517626.110991	41.622196
3505.055845	517592.509774	41.627200
3505.387117	517565.960331	41.632205
3505.068701	517545.480459	41.637210
3504.889788	517518.859874	41.642215
3505.119487	517485.954879	41.647220
3505.017947	517472.267232	41.652224
3505.335824	517446.377090	41.657229
3505.214245	517418.078554	41.662234
3505.007198	517388.478720	41.667239
3505.075286	517361.009759	41.672244
3505.065169	517336.435480	41.677248
3504.943496	517306.063487	41.682253
3504.989763	517287.902348	41.687258
3505.213597	517258.183610	41.692263
3504.980735	517227.475070	41.697268
3504.788705	517208.694122	41.702272
3505.230553	517193.858427	41.707277
3505.203614	517170.702473	41.712282
3505.112058	517150.439097	41.717287
3505.233126	517134.541545	41.722292
3504.994516	517107.474618	41.727296
3505.427242	517067.507678	41.732301
3505.045109	517059.325450	41.737306
3504.724478	517026.051406	41.742311
3504.964669	516996.885872	41.747316
3504.929975	516983.895219	41.752320
3504.981889	516948.943934	41.757325
3504.830028	516934.859243	41.762330
3504.957482	516904.851692	41.767335
3504.873756	516886.660091	41.772340
3504.639303	516871.981570	41.777344
3505.014242	516847.042291	41.782349
3504.827517	516837.008572	41.787354
3505.004596	516810.987986	41.792359
3504.859067	516805.043860	41.797364
3505.068335	516769.207645	41.802368
3504.846705	516738.900981	41.807373
3505.121584	516718.933149	41.812378
3504.717755	516692.953622	41.817383
3504.625908	516667.430443	41.822388
3504.979526	516655.794116	41.827392
3504.975593	516622.165787	41.832397
3504.881645	516613.128669	41.837402
3504.826087	516579.811834	41.842407
3504.856944	516574.547729	41.847412
3505.022801	516548.427364	41.852416
3505.036121	516522.229928	41.857421
3505.043068	516500.938784	41.862426
3504.796182	516480.395718	41.867431
3504.850947	516457.276424	41.872436
3504.574578	516436.434540	41.877440
3504.879920	516410.848190	41.882445
3504.573150	516405.030547	41.887450
3504.679218	516377.655098	41.892455
3504.431639	516363.231055	41.897460
3504.484208	516354.524635	41.902464
3504.940205	516329.015489	41.907469
3504.531141	516307.486424	41.912474
3504.529107	516286.499851	41.917479
3504.589901	516275.465822	41.922484
3504.032704	516263.973179	41.927488
3504.407109	516247.124458	41.932493
3504.369619	516237.420788	41.937498
3504.263855	516234.251586	41.942503
3504.378183	516205.761983	41.947508
3504.597068	516208.559444	41.952512
3504.697869	516182.195932	41.957517
3504.712459	516167.376283	41.962522
3504.352105	516160.403880	41.967527
3504.513906	516133.777793	41.972532
3504.641086	516130.470611	41.977536
3504.537678	516112.331844	41.982541
3504.543495	516090.534637	41.987546
3504.468438	516088.978846	41.992551
3504.769021	516056.666678	41.997556
3504.579520	516045.773200	42.002560
3504.661446	516029.324490	42.007565
3504.657395	516007.275875	42.012570
3504.715336	516001.198158	42.017575
3504.423016	515975.705603	42.022580
3504.203829	515963.552464	42.027584
3504.585545	515962.227898	42.032589
3504.547913	515933.104411	42.037594
3504.485963	515928.158202	42.042599
3504.807679	515909.749734	42.047604
3504.746705	515890.339714	42.052608
3504.826330	515866.608804	42.057613
3504.417419	515852.766113	42.062618
3504.438898	515843.659761	42.067623
3504.870103	515818.659478	42.072628
3504.617234	515812.883679	42.077632
3504.598526	515797.209232	42.082637
3504.533657	515785.284435	42.087642
3504.368484	515757.799120	42.092647
3504.444598	515734.321441	42.097652
3504.418511	515728.560341	42.102656
3504.599684	515726.104282	42.107661
3504.539502	515711.194900	42.112666
3504.377575	515697.161324	42.117671
3504.361461	515669.955742	42.122676
3504.251917	515666.180154	42.127680
3504.533143	515653.694832	42.132685
3504.450532	515636.664865	42.137690
3504.352940	515622.064754	42.142695
3504.698013	515612.603692	42.147700
3504.447786	515580.023647	42.152704
3504.683670	515570.680966	42.157709
3504.488391	515572.026800	42.162714
3504.591358	515538.581679	42.167719
3504.678536	515536.342741	42.172724
3504.131855	515513.671213	42.177728
3504.564974	515495.902135	42.182733
3504.651941	515498.417126	42.187738
3504.537948	515474.463394	42.192743
3504.752680	515448.080714	42.197748
3504.240301	515440.575727	42.202752
3504.381062	515418.908035	42.207757
3504.413359	515421.279959	42.212762
3504.552715	515399.207874	42.217767
3504.679820	515370.360809	42.222772
3504.325784	515364.904287	42.227776
3504.583557	515347.415635	42.232781
3504.328425	515336.835509	42.237786
3504.277954	515330.016074	42.242791
3504.655378	515313.975120	42.247796
3504.092810	515304.606766	42.252800
3504.742046	515297.626153	42.257805
3504.516317	515276.066775	42.262810
3504.115722	515256.911993	42.267815
3504.467246	515258.576020	42.272820
3504.230683	515238.232085	42.277824
3504.728249	515209.275615	42.282829
3504.792373	515206.180515	42.287834
3504.411629	515187.983427	42.292839
3504.307010	515177.379411	42.297844
3504.157497	515173.357157	42.302848
3504.589396	515142.236251	42.307853
3504.376993	515138.173354	42.312858
3504.703940	515124.820645	42.317863
3504.895273	515089.236528	42.322868
3504.598608	515097.881172	42.327872
3504.472929	515069.781586	42.332877
3504.697347	515059.125490	42.337882
3504.502932	515043.326382	42.342887
3504.600678	515019.692555	42.347892
3504.363216	515016.543936	42.352896
3504.719751	514979.264504	42.357901
3504.355026	514984.936038	42.362906
3504.582031	514963.709301	42.367911
3504.543907	514941.664664	42.372916
3504.286696	514938.670878	42.377920
3504.126710	514918.213299	42.382925
3504.345457	514893.346365	42.387930
3504.261573	514880.462997	42.392935
3504.242301	514887.496072	42.397940
3504.241376	514883.197387	42.402944
3504.411892	514850.650569	42.407949
3504.372486	514845.751052	42.412954
3504.307100	514827.958906	42.417959
3504.357948	514813.941533	42.422964
3504.219454	514815.076149	42.427968
3504.180861	514804.512036	42.432973
3503.906957	514785.640142	42.437978
3503.952886	514770.207393	42.442983
3504.319961	514771.110378	42.447988
3504.078345	514774.891227	42.452992
3503.976356	514746.686204	42.457997
3504.086573	514739.942282	42.463002
3504.072884	514731.548942	42.468007
3504.352584	514730.240407	42.473012
3504.244912	514730.914976	42.478016
3504.202113	514714.686988	42.483021
3504.341195	514693.979563	42.488026
3504.466676	514689.762001	42.493031
3504.248501	514676.393943	42.498036
3504.150803	514662.905680	42.503040
3504.375290	514647.394020	42.508045
3504.585658	514655.807024	42.513050
3504.222278	514619.854401	42.518055
3504.663711	514617.357045	42.523060
3504.496628	514604.486615	42.528064
3504.472573	514578.544916	42.533069
3504.602339	514577.968134	42.538074
3504.372483	514550.946243	42.543079
3504.595474	514542.768281	42.548084
3504.284963	514544.840477	42.553088
3504.547488	514509.699064	42.558093
3504.596638	514508.072917	42.563098
3504.321560	514487.177814	42.568103
3504.275136	514473.276683	42.573108
3504.267210	514466.601901	42.578112
3504.365160	514452.475627	42.583117
3504.162667	514441.633731	42.588122
3504.144100	514417.511673	42.593127
3504.304203	514403.274381	42.598132
3503.932804	514413.043876	42.603136
3504.597354	514385.071126	42.608141
3504.400877	514383.483789	42.613146
3503.679169	514385.317535	42.618151
3504.311463	514374.545961	42.623156
3504.182946	514355.498872	42.628160
3504.326623	514345.563160	42.633165
3504.241554	514341.125904	42.638170
3504.309508	514331.910230	42.643175
3504.505527	514306.641403	42.648180
3504.270172	514301.570389	42.653184
3504.227542	514292.372171	42.658189
3504.487607	514269.824327	42.663194
3504.262520	514258.378958	42.668199
3504.305208	514258.625163	42.673204
3504.134295	514244.591786	42.678208
3504.707365	514227.911946	42.683213
3504.559196	514214.886495	42.688218
3504.321065	514196.918673	42.693223
3504.242339	514175.587529	42.698228
3504.147242	514189.511408	42.703232
3504.291462	514171.786592	42.708237
3504.515277	514147.474103	42.713242
3504.282962	514146.347605	42.718247
3504.413491	514133.530929	42.723252
3504.429657	514121.389827	42.728256
3504.476290	514100.139929	42.733261
3504.334013	514098.139377	42.738266
3504.272769	514081.357337	42.743271
3504.236968	514063.711438	42.748276
3504.270639	514054.501030	42.753280
3504.135044	514046.177192	42.758285
3504.244734	514025.979368	42.763290
3504.247074	514023.703060	42.768295
3504.335704	514012.612561	42.773300
3504.188350	513995.186533	42.778304
3504.348845	513974.019635	42.783309
3504.267748	513982.883669	42.788314
3504.243874	513960.784913	42.793319
3504.374427	513940.330797	42.798324
3504.187191	513946.278096	42.803329
3504.258024	513925.732245	42.808333
3504.058799	513906.139462	42.813338
3504.115736	513913.616104	42.818343
3504.365375	513905.281887	42.823348
3504.105779	513899.253596	42.828353
3504.337897	513888.646119	42.833357
3504.271291	513870.802572	42.838362
3504.082660	513857.328034	42.843367
3504.392096	513850.552268	42.848372
3504.240448	513836.464927	42.853377
3504.328040	513824.413478	42.858381
3504.366187	513816.972479	42.863386
3504.528641	513797.271825	42.868391
3504.772404	513777.254825	42.873396
3504.388649	513782.626298	42.878401
3504.175618	513748.165399	42.883405
3504.125332	513748.982673	42.888410
3503.862463	513746.647088	42.893415
3504.446388	513739.170370	42.898420
3504.118546	513728.550139	42.903425
3504.622142	513702.169637	42.908429
3504.725113	513697.854227	42.913434
3504.174786	513670.578096	42.918439
3504.551192	513657.975090	42.923444
3504.303304	513653.209334	42.928449
3504.136503	513630.728102	42.933453
3504.080417	513612.781461	42.938458
3503.916611	513612.048731	42.943463
3504.125707	513613.836596	42.948468
3504.164528	513597.139415	42.953473
3504.178326	513583.834979	42.958477
3504.228034	513581.045333	42.963482
3504.056258	513572.120029	42.968487
3504.098608	513563.059718	42.973492
3504.204546	513537.146443	42.978497
3504.126724	513543.582383	42.983501
3504.300971	513532.933250	42.988506
3504.336756	513529.387106	42.993511
3504.600681	513496.873482	42.998516
3503.909929	513498.044893	43.003521
3504.304983	513494.239639	43.008525
3504.295628	513474.211706	43.013530
3504.421747	513458.259283	43.018535
3504.279005	513458.231331	43.023540
3503.945956	513449.483190	43.028545
3504.175435	513421.021230	43.033549
3504.231017	513428.650041	43.038554
3504.203042	513409.282510	43.043559
3504.285776	513411.242108	43.048564
3504.018206	513393.227500	43.053569
3504.076782	513366.866231	43.058573
3503.898170	513389.200223	43.063578
3503.912756	513383.887106	43.068583
3504.320523	513361.769920	43.073588
3503.706301	513357.517199	43.078593
3504.352648	513338.751125	43.083597
3504.091116	513342.940080	43.088602
3503.712619	513331.164266	43.093607
3504.300730	513336.028213	43.098612
3504.093312	513323.466654	43.103617
3504.395017	513299.899331	43.108621
3504.126385	513295.844872	43.113626
3504.042516	513294.340793	43.118631
3504.324744	513268.298081	43.123636
3503.840328	513277.023913	43.128641
3504.239051	513265.125209	43.133645
3504.421821	513263.730723	43.138650
3503.997920	513245.690085	43.143655
3504.313769	513218.428058	43.148660
3504.148945	513227.153982	43.153665
3504.223762	513222.741740	43.158669
3504.067739	513199.448944	43.163674
3503.966865	513192.990668	43.168679
3504.520258	513176.666964	43.173684
3504.193790	513188.352121	43.178689
3504.006124	513163.597445	43.183693
3504.277690	513150.858891	43.188698
3504.111800	513155.184518	43.193703
3504.319599	513142.152553	43.198708
3504.242756	513128.103376	43.203713
3504.344811	513113.773008	43.208717
3504.233709	513105.394253	43.213722
3504.343361	513094.755053	43.218727
3504.494891	513071.969858	43.223732
3504.327891	513071.642254	43.228737
3504.322225	513045.391798	43.233741
3504.414813	513036.222102	43.238746
3504.020960	513028.393807	43.243751
3504.557325	513023.301592	43.248756
3504.003080	513003.865032	43.253761
3503.995615	512990.158840	43.258765
3504.160691	512996.253112	43.263770
3504.109278	512983.261994	43.268775
3504.484880	512970.608023	43.273780
3504.038589	512961.472878	43.278785
3504.218948	512951.378804	43.283789
3504.325782	512946.910848	43.288794
3504.122913	512920.489042	43.293799
3504.333524	512902.246586	43.298804
3504.130630	512904.049064	43.303809
3504.082293	512890.197507	43.308813
3504.195189	512872.425694	43.313818
3504.025894	512868.608337	43.318823
3504.052184	512860.764139	43.323828
3503.860016	512874.502121	43.328833
3503.637457	512862.397844	43.333837
3503.862040	512858.771137	43.338842
3503.829063	512859.332810	43.343847
3503.990130	512841.098118	43.348852
3504.369969	512826.774183	43.353857
3504.226284	512827.859170	43.358861
3503.900335	512832.109015	43.363866
3504.042472	512821.970323	43.368871
3504.307344	512798.155215	43.373876
3503.925984	512783.749229	43.378881
3504.028529	512780.394702	43.383885
3504.389529	512794.298226	43.388890
3503.967115	512766.089943	43.393895
3504.215640	512743.288974	43.398900
3504.043866	512750.195301	43.403905
3504.216809	512732.970249	43.408909
3503.915355	512740.959293	43.413914
3503.772676	512722.468992	43.418919
3504.214834	512707.781034	43.423924
3503.960818	512710.400921	43.428929
3503.659776	512712.067186	43.433933
3503.868845	512712.944681	43.438938
3503.803363	512711.134152	43.443943
3504.361802	512712.816317	43.448948
3503.940664	512682.989075	43.453953
3504.222444	512666.808973	43.458957
3504.100319	512671.330134	43.463962
3504.107545	512671.784295	43.468967
3504.172674	512649.113350	43.473972
3504.192588	512652.195770	43.478977
3503.913141	512637.925297	43.483981
3503.853082	512639.300570	43.488986
3503.818321	512644.465496	43.493991
3503.892169	512641.520134	43.498996
3504.044940	512614.636982	43.504001
3504.334962	512604.019548	43.509005
3504.309560	512596.588055	43.514010
3504.369699	512583.376669	43.519015
3504.378531	512569.364067	43.524020
3504.168335	512554.677920	43.529025
3503.975301	512543.125151	43.534029
3504.133110	512548.512582	43.539034
3504.387369	512530.009914	43.544039
3504.497347	512505.257811	43.549044
3504.329299	512508.420548	43.554049
3504.037595	512481.051029	43.559053
3504.190078	512472.023308	43.564058
3503.935943	512480.207325	43.569063
3504.272699	512470.037663	43.574068
3504.175257	512444.761847	43.579073
3504.261031	512436.098729	43.584077
3504.203703	512428.267547	43.589082
3504.161275	512433.332584	43.594087
3504.297295	512404.276692	43.599092
3504.013475	512396.633041	43.604097
3503.965352	512387.839313	43.609101
3504.195195	512398.728927	43.614106
3504.328797	512382.521392	43.619111
3504.478835	512349.011904	43.624116
3504.474356	512350.732496	43.629121
3504.296726	512340.542892	43.634125
3504.520431	512329.379356	43.639130
3504.257209	512309.845413	43.644135
3504.266403	512298.766344	43.649140
3504.254353	512275.854182	43.654145
3504.291718	512264.214223	43.659149
3504.090144	512271.934785	43.664154
3504.052063	512254.894350	43.669159
3504.297346	512225.922049	43.674164
3504.286148	512231.488043	43.679169
3504.210020	512220.472991	43.684173
3504.367681	512198.849067	43.689178
3504.384674	512185.138357	43.694183
3504.217534	512185.974174	43.699188
3504.005197	512184.035050	43.704193
3504.252063	512158.046802	43.709197
3503.898470	512147.176724	43.714202
3503.964493	512153.236373	43.719207
3503.935655	512146.260476	43.724212
3504.117734	512141.476915	43.729217
3504.430015	512116.135850	43.734221
3504.422865	512107.335500	43.739226
3504.161170	512107.022843	43.744231
3504.361066	512092.979648	43.749236
3504.194499	512083.445727	43.754241
3504.432135	512064.793428	43.759245
3504.220187	512067.963185	43.764250
3504.161353	512036.762361	43.769255
3504.363107	512031.621572	43.774260
3504.211000	512023.299344	43.779265
3504.356866	512011.945566	43.784269
3504.160070	512000.393021	43.789274
3504.136628	511995.692486	43.794279
3504.167615	511993.714881	43.799284
3504.383473	511987.155498	43.804289
3504.238389	511956.473998	43.809293
3504.392002	511949.216262	43.814298
3504.388159	511943.956190	43.819303
3504.224125	511918.234857	43.824308
3504.029641	511916.798721	43.829313
3504.183443	511906.404718	43.834317
3504.202832	511904.580688	43.839322
3504.313389	511873.251620	43.844327
3504.602062	511860.559978	43.849332
3504.076329	511865.701573	43.854337
3504.127810	511848.191314	43.859341
3504.136268	511829.676148	43.864346
3504.030985	511827.365971	43.869351
3504.237160	511820.909224	43.874356
3504.247435	511803.759523	43.879361
3504.329083	511792.162826	43.884365
3504.451291	511785.618168	43.889370
3504.334700	511766.869776	43.894375
3504.277295	511741.738336	43.899380
3504.037498	511739.601161	43.904385
3504.280530	511731.772768	43.909389
3504.513777	511721.669604	43.914394
3503.939084	511709.468401	43.919399
3504.184495	511691.067387	43.924404
3503.859045	511692.029420	43.929409
3503.894792	511684.739616	43.934413
3504.049892	511668.578585	43.939418
3504.397433	511657.900884	43.944423
3504.483712	511652.272383	43.949428
3504.077473	511640.095090	43.954433
3503.814801	511617.828671	43.959437
3504.617668	511614.312640	43.964442
3504.166460	511617.065031	43.969447
3504.034432	511604.287936	43.974452
3504.076898	511585.868300	43.979457
3504.314066	511567.923722	43.984461
3504.212291	511562.830766	43.989466
3504.050786	511569.381853	43.994471
3504.184697	511538.453158	43.999476
3503.796427	511531.989087	44.004481
3503.842799	511522.218852	44.009485
3503.960464	511521.289785	44.014490
3503.984496	511520.982540	44.019495
3504.187378	511516.347272	44.024500
3503.854190	511498.948037	44.029505
3503.940895	511493.622928	44.034509
3504.149198	511490.909042	44.039514
3504.094873	511490.563597	44.044519
3504.252587	511486.593070	44.049524
3504.038429	511470.945484	44.054529
3504.010134	511456.179047	44.059533
3504.284403	511446.625677	44.064538
3504.314432	511440.398969	44.069543
3504.379116	511430.119932	44.074548
3504.187389	511419.122631	44.079553
3504.013684	511403.620346	44.084557
3503.888775	511406.978811	44.089562
3503.614129	511398.422715	44.094567
3504.158956	511367.833449	44.099572
3504.038141	511376.705126	44.104577
3503.918551	511366.303418	44.109581
3503.925065	511366.251869	44.114586
3504.065686	511360.311167	44.119591
3504.073357	511362.940484	44.124596
3503.830449	511351.900643	44.129601
3504.297063	511337.207637	44.134605
3504.120844	511345.784572	44.139610
3504.303743	511341.658274	44.144615
3504.145302	511306.829665	44.149620
3504.040149	511301.787751	44.154625
3503.980932	511300.937214	44.159629
3503.739436	511296.625052	44.164634
3503.856426	511297.668934	44.169639
3503.917376	511283.545860	44.174644
3503.937870	511275.297156	44.179649
3504.196081	511262.205194	44.184653
3504.069238	511241.889672	44.189658
3503.579431	511255.625420	44.194663
3504.059995	511243.864126	44.199668
3504.026765	511250.192717	44.204673
3504.236059	511221.274977	44.209677
3503.956095	511220.459327	44.214682
3504.027982	511206.233287	44.219687
3504.126128	511202.575627	44.224692
3503.807710	511203.334229	44.229697
3503.795288	511197.771764	44.234701
3503.890268	511174.841199	44.239706
3503.630417	511184.089057	44.244711
3503.773677	511160.847323	44.249716
3504.044549	511172.591211	44.254721
3503.762775	511175.468652	44.259725
3503.779090	511161.200771	44.264730
3503.769790	511166.109191	44.269735
3503.668886	511168.249835	44.274740
3503.619462	511175.997432	44.279745
3503.837307	511168.324520	44.284749
3503.785833	511159.227166	44.289754
3503.915882	511151.568123	44.294759
3504.200566	511132.249742	44.299764
3503.907591	511138.164149	44.304769
3503.957523	511118.882856	44.309773
3504.224743	511132.043773	44.314778
3503.941677	511116.609098	44.319783
3504.106510	511100.901269	44.324788
3503.991159	511097.378504	44.329793
3504.067555	511107.989683	44.334797
3504.226587	511094.103882	44.339802
3504.029071	511087.761250	44.344807
3504.119391	511054.157472	44.349812
3504.280084	511053.272165	44.354817
3503.932220	511056.210658	44.359821
3503.986738	511055.949173	44.364826
3503.984506	511040.014761	44.369831
3504.268806	511020.645726	44.374836
3503.703679	511021.190395	44.379841
3503.727952	511012.283338	44.384845
3504.229730	511016.200458	44.389850
3503.890327	511003.152166	44.394855
3504.420308	510976.055040	44.399860
3504.060623	510973.784955	44.404865
3504.139622	510964.616287	44.409869
3504.288653	510965.250429	44.414874
3503.857782	510951.761272	44.419879
3504.233420	510928.280145	44.424884
3504.013492	510934.992471	44.429889
3504.134564	510937.452169	44.434893
3504.291009	510928.119480	44.439898
3504.058668	510907.719058	44.444903
3504.144945	510893.541070	44.449908
3503.856117	510890.956252	44.454913
3503.956730	510888.309879	44.459917
3503.794972	510900.628207	44.464922
3503.799636	510882.163196	44.469927
3504.090678	510850.044908	44.474932
3503.752874	510853.892417	44.479937
3503.907289	510853.969252	44.484941
3504.291402	510850.266318	44.489946
3504.092741	510852.624802	44.494951
3503.953155	510838.634229	44.499956
3503.979258	510813.336456	44.504961
3503.772466	510811.548058	44.509965
3503.842712	510810.575860	44.514970
3503.778406	510804.768529	44.519975
3504.395217	510803.507593	44.524980
3504.094783	510802.037520	44.529985
3504.181136	510780.777175	44.534989
3504.321464	510767.045827	44.539994
3504.447612	510770.364736	44.544999
3504.286814	510743.224658	44.550004
3504.196824	510739.596635	44.555009
3504.069380	510734.760426	44.560013
3504.098129	510720.338448	44.565018
3504.104196	510708.297669	44.570023
3503.816860	510701.867914	44.575028
3503.910276	510700.942635	44.580033
3504.138405	510699.540773	44.585037
3503.921607	510692.644575	44.590042
3503.659311	510690.713174	44.595047
3503.732814	510663.586524	44.600052
3503.807973	510658.971211	44.605057
3504.037275	510652.308015	44.610061
3504.010099	510642.498313	44.615066
3504.092017	510648.859515	44.620071
3504.073982	510649.267136	44.625076
3503.893187	510647.676963	44.630081
3504.177695	510619.758074	44.635085
3503.894240	510615.047666	44.640090
3503.874915	510620.261355	44.645095
3503.964227	510613.519095	44.650100
3503.774891	510608.085575	44.655105
3504.062758	510594.077828	44.660109
3503.840957	510576.710631	44.665114
3503.688593	510576.380662	44.670119
3503.969757	510557.011597	44.675124
3503.930771	510567.944879	44.680129
3503.613515	510566.629208	44.685133
3503.955397	510567.688178	44.690138
3504.093780	510565.136962	44.695143
3504.047784	510557.556066	44.700148
3503.814277	510547.475392	44.705153
3503.805140	510533.767480	44.710157
3503.755239	510526.086011	44.715162
3503.701127	510520.985209	44.720167
3504.146850	510527.491308	44.725172
3503.993640	510534.142658	44.730177
3503.879229	510518.427841	44.735181
3503.664599	510505.713564	44.740186
3503.596835	510494.696071	44.745191
3504.158136	510482.213255	44.750196
3504.126789	510489.806541	44.755201
3504.150999	510492.079260	44.760205
3504.070215	510488.753259	44.765210
3503.762095	510476.761975	44.770215
3503.911068	510447.397161	44.775220
3503.906889	510455.947351	44.780225
3504.020881	510453.298796	44.785229
3503.745967	510451.167007	44.790234
3503.716618	510457.950575	44.795239
3503.799707	510449.236281	44.800244
3503.793374	510468.966869	44.805249
3504.143256	510443.971493	44.810253
3504.253974	510429.182193	44.815258
3503.810140	510427.734752	44.820263
3503.828229	510421.863679	44.825268
3503.973587	510413.493645	44.830273
3504.041703	510422.083014	44.835277
3503.931888	510403.837934	44.840282
3503.701837	510389.153048	44.845287
3503.865527	510376.125936	44.850292
3503.921353	510378.950149	44.855297
3503.934840	510377.835131	44.860301
3503.929778	510373.788896	44.865306
3503.920731	510380.215165	44.870311
3504.377143	510365.775882	44.875316
3503.689247	510345.851500	44.880321
3503.778109	510340.424513	44.885325
3503.964665	510339.939793	44.890330
3504.064702	510330.565105	44.895335
3504.345776	510320.200608	44.900340
3503.933191	510321.125897	44.905345
3504.118573	510301.518737	44.910349
3504.326064	510298.450669	44.915354
3504.029294	510297.131739	44.920359
3504.098430	510282.955953	44.925364
3504.079706	510272.689401	44.930369
3504.204363	510257.998928	44.935373
3504.084937	510259.383776	44.940378
3504.023022	510253.120578	44.945383
3504.112215	510228.823749	44.950388
3503.978856	510227.883698	44.955393
3504.005838	510218.672263	44.960397
3503.891821	510219.145653	44.965402
3503.959700	510209.725392	44.970407
3504.259811	510205.985008	44.975412
3503.962622	510180.282091	44.980417
3503.899762	510173.867245	44.985421
3503.973624	510168.999057	44.990426
3504.177803	510173.165770	44.995431
3504.165351	510162.898160	45.000436
3504.204074	510139.064485	45.005441
3504.292257	510131.816319	45.010445
3504.135169	510131.992982	45.015450
3503.930955	510124.082774	45.020455
3503.879782	510091.410075	45.025460
3503.611601	510098.079766	45.030465
3503.802461	510088.538821	45.035469
3504.251280	510090.036227	45.040474
3503.744830	510091.937566	45.045479
3504.067081	510086.321841	45.050484
3503.803036	510082.923547	45.055489
3504.012298	510062.604084	45.060493
3504.227072	510052.300494	45.065498
3503.938136	510058.113455	45.070503
3503.869165	510052.407786	45.075508
3503.827949	510058.485131	45.080513
3504.092694	510042.457000	45.085517
3503.854499	510026.811884	45.090522
3503.611237	510019.160749	45.095527
3503.924149	510014.710043	45.100532
3504.290427	510020.925355	45.105537
3503.955155	510021.889029	45.110541
3503.826424	510017.103409	45.115546
3503.967803	510009.695014	45.120551
3503.901285	509983.803572	45.125556
3503.940914	509969.682780	45.130561
3503.988268	509971.091881	45.135565
3503.929704	509978.436746	45.140570
3503.856374	509978.701353	45.145575
3504.032920	509962.029417	45.150580
3503.874491	509943.336218	45.155585
3503.976514	509929.053761	45.160589
3503.832130	509939.751152	45.165594
3503.619925	509933.815131	45.170599
3503.907680	509932.960275	45.175604
3503.961077	509932.496591	45.180609
3504.022439	509927.883261	45.185613
3503.896694	509931.242148	45.190618
3504.024522	509903.195083	45.195623
3504.062747	509882.649489	45.200628
3504.014505	509885.439643	45.205633
3503.972141	509896.424478	45.210637
3504.282831	509886.156218	45.215642
3503.929474	509865.116003	45.220647
3503.786809	509848.190867	45.225652
3503.852484	509850.659479	45.230657
3503.904211	509851.460815	45.235661
3504.220085	509849.488523	45.240666
3503.821975	509849.703284	45.245671
3503.936625	509821.354626	45.250676
3504.278677	509808.855386	45.255681
3504.112683	509808.274603	45.260685
3504.067920	509812.126617	45.265690
3503.874647	509799.357847	45.270695
3504.133833	509785.101020	45.275700
3504.024427	509772.571927	45.280705
3504.254954	509762.468035	45.285709
3504.213381	509762.120538	45.290714
3504.040351	509765.233978	45.295719
3504.093632	509733.910031	45.300724
3504.147614	509724.643472	45.305729
3504.073510	509735.582836	45.310733
3503.984975	509732.915591	45.315738
3504.040027	509707.459832	45.320743
3503.873358	509684.467439	45.325748
3503.366698	509691.124389	45.330753
3503.866186	509684.569886	45.335757
3504.002613	509683.081256	45.340762
3503.593745	509694.528875	45.345767
3503.822712	509687.106497	45.350772
3503.820989	509686.550336	45.355777
3503.844263	509680.425236	45.360781
3504.018878	509680.296522	45.365786
3503.959123	509660.626192	45.370791
3504.017875	509654.900202	45.375796
3503.569548	509657.095946	45.380801
3503.454399	509645.984213	45.385805
3503.828214	509647.746469	45.390810
3503.602057	509653.448462	45.395815
3503.519855	509644.355156	45.400820
3503.981995	509648.784771	45.405825
3503.770172	509647.654726	45.410829
3503.445324	509653.726454	45.415834
3503.643609	509651.620953	45.420839
3503.895019	509645.662146	45.425844
3503.894879	509630.990860	45.430849
3503.962571	509618.686618	45.435853
3504.100928	509607.939520	45.440858
3503.736614	509614.270455	45.445863
3503.967564	509600.675621	45.450868
3504.133252	509611.223027	45.455873
3504.175417	509607.826830	45.460877
3504.015161	509584.934471	45.465882
3504.287685	509571.687180	45.470887
3504.381238	509565.803887	45.475892
3503.619561	509559.499262	45.480897
3504.020020	509534.191017	45.485901
3504.375513	509533.628983	45.490906
3503.977696	509525.799689	45.495911
3504.051851	509529.987110	45.500916
3504.100601	509514.397354	45.505921
3503.692848	509488.053183	45.510925
3503.991796	509476.572342	45.515930
3504.084955	509486.170051	45.520935
3504.216616	509476.385166	45.525940
3504.042930	509484.608493	45.530945
3503.561271	509467.635378	45.535949
3503.887537	509448.966213	45.540954
3503.297801	509442.786142	45.545959
3503.788973	509440.280183	45.550964
3503.725466	509446.563635	45.555969
3503.642604	509438.785704	45.560973
3503.683692	509436.705023	45.565978
3503.825411	509443.664321	45.570983
3503.855987	509432.175275	45.575988
3503.901014	509447.244501	45.580993
3504.012342	509440.397116	45.585997
3504.177266	509431.517596	45.591002
3504.165081	509420.844766	45.596007
3504.109109	509411.595416	45.601012
3504.024362	509408.573380	45.606017
3503.846985	509404.655334	45.611021
3503.936158	509408.891003	45.616026
3503.925562	509381.876797	45.621031
3504.280437	509358.497982	45.626036
3504.030623	509377.560028	45.631041
3503.732043	509362.834500	45.636045
3504.088954	509360.754484	45.641050
3504.137792	509349.464864	45.646055
3504.142901	509324.623532	45.651060
3503.658101	509325.712061	45.656065
3504.020971	509321.253280	45.661069
3504.029558	509319.329498	45.666074
3503.785702	509318.912780	45.671079
3504.009154	509291.659071	45.676084
3503.929767	509288.433798	45.681089
3503.764743	509279.100429	45.686093
3503.872431	509277.768082	45.691098
3503.885081	509275.388325	45.696103
3503.832544	509281.518328	45.701108
3503.868262	509278.072492	45.706113
3504.020084	509277.643826	45.711117
3504.037021	509249.764995	45.716122
3503.711245	509255.027537	45.721127
3504.383723	509237.821184	45.726132
3503.947014	509243.000079	45.731137
3503.723831	509245.463841	45.736141
3503.587944	509241.387424	45.741146
3503.782853	509233.312536	45.746151
3504.004221	509212.383047	45.751156
3503.567901	509205.571535	45.756161
3503.897660	509209.162121	45.761165
3503.981048	509198.727008	45.766170
3503.754314	509211.006229	45.771175
3504.352356	509209.039860	45.776180
3504.022167	509200.086698	45.781185
3504.009336	509178.991816	45.786189
3504.365031	509172.105701	45.791194
3503.943579	509167.467293	45.796199
3504.178252	509156.148174	45.801204
3503.490820	509133.945644	45.806209
3504.058010	509126.469566	45.811213
3504.164117	509116.131997	45.816218
3503.585251	509118.500218	45.821223
3503.776077	509109.009327	45.826228
3503.660689	509117.577763	45.831233
3503.789599	509116.393827	45.836237
3503.992853	509117.525395	45.841242
3503.876171	509119.820565	45.846247
3504.221949	509104.841192	45.851252
3503.927018	509093.453961	45.856257
3503.832338	509090.281661	45.861261
3503.886926	509085.163249	45.866266
3503.641878	509086.871602	45.871271
3504.022873	509087.570338	45.876276
3504.165058	509066.906151	45.881281
3503.839201	509042.521462	45.886285
3504.063106	509040.867172	45.891290
3503.715935	509032.624905	45.896295
3504.079489	509025.231562	45.901300
3503.968261	509037.947985	45.906305
3503.833552	509016.568610	45.911309
3504.121269	509003.419666	45.916314
3503.662002	509001.923945	45.921319
3503.996936	508996.407047	45.926324
3503.790728	508991.835757	45.931329
3504.014739	509003.639140	45.936333
3504.397158	508989.513954	45.941338
3503.992291	508980.015959	45.946343
3504.422550	508952.627840	45.951348
3504.150217	508946.903350	45.956353
3504.005978	508943.131740	45.961357
3504.281979	508921.130809	45.966362
3503.917681	508925.539457	45.971367
3504.433116	508912.556824	45.976372
3503.909796	508915.321037	45.981377
3503.809181	508905.623132	45.986381
3504.122437	508879.113472	45.991386
3503.822500	508862.009847	45.996391
3504.081290	508869.254434	46.001396
3503.759913	508874.819955	46.006401
3504.039150	508861.216904	46.011405
3504.274525	508857.385275	46.016410
3504.177573	508849.103370	46.021415
3503.932530	508831.485106	46.026420
3503.603759	508834.319769	46.031425
3503.889369	508830.379007	46.036429
3503.951581	508832.392973	46.041434
3504.049277	508831.315138	46.046439
3504.110788	508791.640270	46.051444
3503.892695	508800.326284	46.056449
3503.987769	508794.037738	46.061453
3504.081079	508788.204810	46.066458
3503.731691	508786.489328	46.071463
3504.383025	508771.866119	46.076468
3503.950745	508766.217444	46.081473
3503.943032	508762.070060	46.086477
3503.888727	508755.046208	46.091482
3503.876997	508763.952590	46.096487
3504.180281	508757.934684	46.101492
3503.931341	508739.254476	46.106497
3504.404145	508714.540714	46.111501
3504.388077	508699.618182	46.116506
3503.953627	508697.258417	46.121511
3504.214835	508681.836700	46.126516
3504.178740	508665.905428	46.131521
3504.191067	508658.314473	46.136525
3504.158403	508662.518989	46.141530
3503.668624	508650.251571	46.146535
3504.055846	508623.780421	46.151540
3503.783844	508629.591186	46.156545
3503.950477	508617.169400	46.161549
3504.044566	508613.005891	46.166554
3503.790623	508616.790047	46.171559
3504.048149	508623.731374	46.176564
3503.822110	508604.237897	46.181569
3503.904203	508593.549652	46.186573
3503.909021	508586.566980	46.191578
3503.690629	508579.872555	46.196583
3504.041564	508572.278637	46.201588
3504.041847	508587.052126	46.206593
3503.634566	508585.649338	46.211597
3504.075408	508573.892497	46.216602
3503.899701	508550.343477	46.221607
3503.824510	508545.194823	46.226612
3503.785059	508542.266663	46.231617
3504.166808	508527.888234	46.236621
3503.746804	508539.743133	46.241626
3503.759788	508536.857278	46.246631
3504.221976	508532.028438	46.251636
3503.649092	508503.482708	46.256641
3503.588764	508502.733395	46.261645
3503.918459	508494.383885	46.266650
3503.472368	508488.130168	46.271655
3503.693336	508494.723166	46.276660
3503.640541	508501.561808	46.281665
3503.347393	508490.325676	46.286669
3503.712846	508494.619092	46.291674
3503.419110	508488.391889	46.296679
3503.728869	508485.863874	46.301684
3503.559235	508498.083983	46.306689
3503.547356	508490.749751	46.311693
3503.890191	508494.793770	46.316698
3503.398811	508494.770313	46.321703
3503.513877	508488.276119	46.326708
3503.448277	508500.580973	46.331713
3503.576999	508487.962709	46.336717
3504.114169	508504.118646	46.341722
3503.791188	508503.562630	46.346727
3504.104406	508489.144406	46.351732
3504.074291	508482.521374	46.356737
3503.516846	508473.654345	46.361741
3503.896973	508461.097514	46.366746
3503.753404	508466.129119	46.371751
3503.711508	508460.570422	46.376756
3503.774185	508458.081455	46.381761
3503.825692	508465.864920	46.386765
3503.615163	508453.907384	46.391770
3503.505397	508465.359138	46.396775
3503.956408	508454.663092	46.401780
3503.979737	508454.153527	46.406785
3503.942905	508436.805515	46.411789
3503.950023	508421.271942	46.416794
3504.028008	508426.622702	46.421799
3503.782998	508416.239020	46.426804
3503.743621	508429.349292	46.431809
3503.915513	508415.611073	46.436813
3503.937348	508409.131585	46.441818
3503.551737	508396.746331	46.446823
3503.650439	508373.558453	46.451828
3503.428173	508371.468674	46.456833
3503.363692	508372.895583	46.461837
3503.762077	508365.294074	46.466842
3503.846952	508370.340194	46.471847
3503.642559	508364.604771	46.476852
3503.842649	508370.846953	46.481857
3503.890106	508375.898986	46.486861
3503.961709	508361.468249	46.491866
3503.640053	508371.891067	46.496871
3503.766367	508367.671810	46.501876
3503.620694	508367.340738	46.506881
3504.164415	508371.353035	46.511885
3504.254377	508345.889741	46.516890
3504.152620	508338.873218	46.521895
3503.969656	508332.021313	46.526900
3504.114411	508331.846715	46.531905
3504.083565	508321.580911	46.536909
3504.002210	508298.219011	46.541914
3503.942657	508286.794041	46.546919
3504.026053	508292.498151	46.551924
3503.914287	508285.129024	46.556929
3503.657925	508285.928534	46.561933
3503.857718	508287.870224	46.566938
3503.678756	508261.336221	46.571943
3504.279900	508244.848485	46.576948
3503.840125	508251.191845	46.581953
3503.455547	508250.544366	46.586957
3503.816465	508252.207618	46.591962
3504.238749	508253.051650	46.596967
3503.864061	508252.301418	46.601972
3503.644115	508254.613024	46.606977
3503.384546	508241.904167	46.611981
3503.872680	508239.246732	46.616986
3503.738199	508227.024044	46.621991
3503.791641	508212.241887	46.626996
3503.795249	508215.327687	46.632001
3503.818380	508217.651473	46.637005
3504.051248	508199.248692	46.642010
3504.040183	508213.164176	46.647015
3504.138549	508196.502886	46.652020
3504.146469	508188.305277	46.657025
3503.731218	508177.442406	46.662029
3503.720111	508172.738870	46.667034
3503.569473	508174.230008	46.672039
3504.005704	508168.190884	46.677044
3503.915318	508168.964165	46.682049
3503.715235	508167.781569	46.687053
3503.951411	508172.550857	46.692058
3503.638759	508155.397942	46.697063
3503.826306	508144.540965	46.702068
3503.584676	508126.820248	46.707073
3503.778722	508126.384881	46.712077
3503.822085	508117.372110	46.717082
3503.525128	508126.475691	46.722087
3504.074823	508118.900754	46.727092
3503.616551	508131.419721	46.732097
3503.657079	508130.502665	46.737101
3503.788724	508122.639637	46.742106
3503.925238	508125.451469	46.747111
3504.095326	508122.996073	46.752116
3503.798874	508109.483421	46.757121
3503.790669	508106.398461	46.762125
3503.843028	508104.973579	46.767130
3503.408401	508107.319136	46.772135
3503.598134	508099.801086	46.777140
3503.412064	508106.205590	46.782145
3503.497116	508095.465973	46.787149
3503.900794	508096.312954	46.792154
3503.756251	508106.303174	46.797159
3503.959304	508107.738415	46.802164
3503.986249	508102.067531	46.807169
3504.287542	508086.082396	46.812173
3504.201065	508057.813214	46.817178
3503.826745	508065.057018	46.822183
3504.274593	508043.634952	46.827188
3503.781484	508053.832082	46.832193
3503.672174	508053.191682	46.837197
3503.769410	508026.208898	46.842202
3503.772891	508028.535816	46.847207
3503.767032	508012.396777	46.852212
3503.836813	508015.927515	46.857217
3504.038697	508019.133798	46.862221
3504.178092	508009.346857	46.867226
3503.709207	508019.894348	46.872231
3504.086778	508009.310827	46.877236
3503.879642	507995.379202	46.882241
3503.980803	507980.184538	46.887245
3504.348207	507969.804982	46.892250
3504.026464	507977.192299	46.897255
3504.046500	507969.953993	46.902260
3503.851681	507955.413239	46.907265
3504.153438	507936.189755	46.912269
3503.964557	507940.520330	46.917274
3503.526463	507937.351499	46.922279
3504.038320	507927.252662	46.927284
3503.861108	507927.837294	46.932289
3503.703229	507929.531981	46.937293
3504.151186	507918.077147	46.942298
3503.876045	507911.543218	46.947303
3504.086453	507892.334124	46.952308
3503.867822	507896.770604	46.957313
3504.162250	507890.551413	46.962317
3504.259319	507880.922877	46.967322
3503.666821	507860.879325	46.972327
3503.952238	507847.729865	46.977332
3504.003534	507854.248734	46.982337
3504.170746	507842.534647	46.987341
3503.997221	507842.916313	46.992346
3503.962874	507835.737142	46.997351
3504.198616	507806.961254	47.002356
3503.846000	507810.457604	47.007361
3503.916123	507805.235165	47.012365
3504.196654	507806.455800	47.017370
3503.616847	507809.937462	47.022375
3504.060428	507795.295670	47.027380
3503.967785	507770.669931	47.032385
3504.128809	507768.013531	47.037389
3504.053426	507772.022631	47.042394
3504.046104	507764.434387	47.047399
3503.935799	507745.984171	47.052404
3503.492280	507735.833839	47.057409
3504.055267	507725.220838	47.062413
3504.308957	507708.838106	47.067418
3503.917112	507725.849966	47.072423
3503.862707	507718.977496	47.077428
3504.089216	507723.191874	47.082433
3504.127282	507700.670432	47.087437
3503.916897	507680.262694	47.092442
3503.715848	507683.077356	47.097447
3504.084314	507681.855460	47.102452
3504.128481	507682.708689	47.107457
3504.073514	507674.470179	47.112461
3503.844316	507645.514526	47.117466
3503.612449	507641.503495	47.122471
3503.953655	507639.779936	47.127476
3503.863626	507628.612331	47.132481
3503.787264	507631.255503	47.137485
3504.010572	507636.836523	47.142490
3504.197029	507640.298300	47.147495
3503.966603	507622.069324	47.152500
3503.691580	507606.174836	47.157505
3503.997093	507606.278405	47.162509
3504.029533	507594.180675	47.167514
3504.023172	507594.637120	47.172519
3503.641529	507602.843615	47.177524
3503.757878	507601.054399	47.182529
3503.805988	507580.099716	47.187533
3503.479701	507564.921651	47.192538
3503.587981	507562.374751	47.197543
3503.832277	507559.907546	47.202548
3503.831590	507557.782644	47.207553
3503.793613	507557.687519	47.212557
3504.137156	507559.707765	47.217562
3503.864811	507555.905501	47.222567
3504.003924	507558.261641	47.227572
3503.882765	507546.441141	47.232577
3503.936355	507529.533298	47.237581
3503.977993	507517.434061	47.242586
3503.884565	507520.282336	47.247591
3503.831774	507522.365231	47.252596
3503.595260	507520.328195	47.257601
3503.767678	507515.291889	47.262605
3503.854391	507510.269127	47.267610
3503.636611	507511.517948	47.272615
3503.645606	507490.923520	47.277620
3503.792083	507491.305213	47.282625
3503.462206	507472.383436	47.287629
3503.782551	507470.916145	47.292634
3503.554362	507483.500408	47.297639
3503.722673	507459.035368	47.302644
3503.726561	507475.630743	47.307649
3503.649088	507469.824363	47.312653
3503.727968	507467.484485	47.317658
3503.641481	507479.135603	47.322663
3503.994228	507470.377179	47.327668
3504.049620	507466.573690	47.332673
3503.860126	507467.716849	47.337677
3503.753155	507454.983291	47.342682
3503.870600	507445.199500	47.347687
3504.057011	507444.613532	47.352692
3503.864609	507447.629254	47.357697
3503.597600	507443.977913	47.362701
3503.817719	507455.024015	47.367706
3503.643973	507442.756379	47.372711
3503.736966	507438.036188	47.377716
3503.582044	507454.251905	47.382721
3503.588792	507444.030234	47.387725
3504.210896	507445.500492	47.392730
3503.680235	507426.458608	47.397735
3504.039884	507404.391926	47.402740
3504.024104	507393.465420	47.407745
3503.457378	507398.665412	47.412749
3503.730067	507385.163430	47.417754
3503.692587	507397.616418	47.422759
3503.827223	507395.672498	47.427764
3503.867168	507397.538359	47.432769
3503.924616	507392.520189	47.437773
3503.648980	507373.437938	47.442778
3503.879829	507361.258088	47.447783
3503.975410	507351.983677	47.452788
3504.043343	507364.015246	47.457793
3503.723396	507359.815680	47.462797
3504.120710	507351.303140	47.467802
3503.931072	507351.080191	47.472807
3504.195718	507337.731237	47.477812
3503.702245	507324.097315	47.482817
3503.796601	507319.528670	47.487821
3503.710996	507309.574505	47.492826
3503.529955	507308.996013	47.497831
3503.774132	507314.624437	47.502836
3503.716463	507313.014489	47.507841
3503.770474	507308.452218	47.512845
3503.951954	507309.637947	47.517850
3503.753894	507315.842247	47.522855
3503.984523	507291.012935	47.527860
3503.956930	507272.650336	47.532865
3503.522609	507286.886455	47.537869
3503.979960	507272.596230	47.542874
3503.509606	507275.554719	47.547879
3503.860471	507258.245440	47.552884
3503.930484	507277.259255	47.557889
3503.432064	507274.605813	47.562893
3503.663698	507270.420241	47.567898
3503.490260	507272.572832	47.572903
3503.890273	507272.003695	47.577908
3503.894942	507274.431722	47.582913
3503.597322	507271.240563	47.587917
3503.962879	507237.687008	47.592922
3503.621336	507233.592020	47.597927
3503.805623	507224.505912	47.602932
3504.000362	507232.520285	47.607937
3503.822280	507223.339657	47.612941
3503.952905	507233.489281	47.617946
3503.752077	507230.586404	47.622951
3503.963035	507218.460196	47.627956
3503.911716	507203.744333	47.632961
3503.781672	507195.568060	47.637965
3503.815739	507196.524106	47.642970
3503.796905	507182.309071	47.647975
3503.920155	507184.313583	47.652980
3503.832631	507186.452606	47.657985
3503.890569	507196.208954	47.662989
3504.008212	507192.142576	47.667994
3503.809207	507162.725958	47.672999
3503.739437	507149.682707	47.678004
3503.636552	507151.975956	47.683009
3503.730137	507146.041234	47.688013
3503.763511	507148.363545	47.693018
3503.596103	507153.095709	47.698023
3503.762092	507148.616894	47.703028
3503.644584	507152.481000	47.708033
3503.462297	507152.206288	47.713037
3503.914622	507146.164267	47.718042
3503.341171	507156.172229	47.723047
3503.485446	507145.321465	47.728052
3503.589124	507157.347528	47.733057
3503.608471	507155.270009	47.738061
3504.068040	507151.554364	47.743066
3503.696537	507164.667492	47.748071
3503.475046	507140.820193	47.753076
3503.561734	507136.151515	47.758081
3503.749920	507147.759442	47.763085
3503.870396	507124.515848	47.768090
3503.691373	507118.978393	47.773095
3504.127059	507103.628888	47.778100
3503.864979	507114.043045	47.783105
3503.724148	507113.660584	47.788109
3504.277873	507106.944744	47.793114
3503.803214	507111.674883	47.798119
3504.063280	507074.545201	47.803124
3503.945081	507071.224449	47.808129
3504.154053	507064.006500	47.813133
3503.939479	507060.397388	47.818138
3503.998343	507068.433313	47.823143
3503.922295	507049.066164	47.828148
3503.610550	507033.075756	47.833153
3503.729888	507017.573782	47.838157
3504.126939	507015.790738	47.843162
3503.849991	507015.480387	47.848167
3504.060815	507012.107620	47.853172
3504.009987	507003.615143	47.858177
3503.909993	507003.428619	47.863181
3503.919921	506987.437925	47.868186
3503.697024	506980.288200	47.873191
3503.984252	506964.709044	47.878196
3503.947338	506975.037097	47.883201
3503.909760	506971.804781	47.888205
3503.995318	506965.365278	47.893210
3503.847393	506980.163567	47.898215
3503.676911	506951.551662	47.903220
3503.934660	506949.284640	47.908225
3503.662010	506939.612820	47.913229
3504.125143	506930.178891	47.918234
3503.539318	506932.649699	47.923239
3503.732380	506927.053372	47.928244
3503.822402	506937.917971	47.933249
3504.085555	506929.679424	47.938253
3504.052042	506928.521013	47.943258
3503.807631	506920.716878	47.948263
3503.682775	506898.979127	47.953268
3503.686292	506885.418103	47.958273
3503.685111	506881.825824	47.963277
3503.675513	506882.434596	47.968282
3503.881772	506888.828138	47.973287
3503.991280	506885.370162	47.978292
3503.884642	506889.232609	47.983297
3503.712688	506895.787126	47.988301
3503.922160	506877.993826	47.993306
3503.672010	506858.299789	47.998311
3503.660127	506847.169926	48.003316
3503.812245	506852.307061	48.008321
3503.673402	506850.811098	48.013325
3503.910244	506844.752433	48.018330
3503.641456	506842.214426	48.023335
3503.933259	506846.621096	48.028340
3503.920897	506850.468650	48.033345
3503.411344	506852.016629	48.038349
3503.858568	506855.285551	48.043354
3503.849670	506860.852926	48.048359
3503.668376	506823.286474	48.053364
3503.849179	506816.629465	48.058369
3503.599732	506806.953903	48.063373
3503.909727	506799.315083	48.068378
3503.551328	506805.241312	48.073383
3503.874546	506801.951938	48.078388
3503.906554	506800.327769	48.083393
3503.856541	506805.800461	48.088397
3503.795575	506800.952633	48.093402
3504.003303	506796.568329	48.098407
3503.835940	506804.083541	48.103412
3503.641202	506784.987853	48.108417
3503.805629	506773.374682	48.113421
3503.922640	506774.064645	48.118426
3503.698935	506778.907007	48.123431
3504.046670	506776.473943	48.128436
3504.068321	506769.639674	48.133441
3503.882263	506770.326939	48.138445
3504.117575	506754.553403	48.143450
3503.904376	506746.643058	48.148455
3503.581589	506734.398476	48.153460
3504.056915	506727.391285	48.158465
3503.806874	506726.216484	48.163469
3503.963657	506722.700404	48.168474
3503.423065	506730.426438	48.173479
3503.916206	506738.545674	48.178484
3504.042985	506731.087580	48.183489
3503.789847	506708.003679	48.188493
3504.051386	506699.360482	48.193498
3503.939094	506691.838959	48.198503
3504.049683	506682.308820	48.203508
3503.720104	506694.606082	48.208513
3503.842839	506690.741181	48.213517
3504.353283	506673.912093	48.218522
3503.656817	506664.458905	48.223527
3503.703769	506648.107848	48.228532
3503.660582	506647.355744	48.233537
3503.644130	506649.483599	48.238541
3503.929915	506638.306554	48.243546
3503.852427	506644.239037	48.248551
3503.831252	506638.322280	48.253556
3503.916962	506643.368774	48.258561
3503.547548	506627.032906	48.263565
3504.018275	506601.658662	48.268570
3503.508009	506618.538523	48.273575
3503.889508	506607.700528	48.278580
3504.003121	506604.039449	48.283585
3503.888472	506606.739428	48.288589
3503.944535	506605.718636	48.293594
3503.752748	506594.819445	48.298599
3503.815801	506601.893527	48.303604
3503.494982	506582.868144	48.308609
3503.587624	506570.760185	48.313613
3503.891990	506561.199352	48.318618
3503.478394	506563.035788	48.323623
3503.728474	506550.852331	48.328628
3503.468477	506569.514283	48.333633
3503.553673	506561.404889	48.338637
3503.871041	506561.911393	48.343642
3503.518349	506571.226997	48.348647
3503.544033	506557.965813	48.353652
3503.710512	506569.526959	48.358657
3503.691864	506566.746975	48.363661
3503.996342	506561.132920	48.368666
3503.561312	506567.577342	48.373671
3503.620135	506566.809111	48.378676
3503.830527	506559.337728	48.383681
3503.807444	506569.613236	48.388685
3503.684091	506572.516995	48.393690
3503.719604	506564.314256	48.398695
3504.099063	506545.481749	48.403700
3503.750315	506525.701718	48.408705
3503.651622	506521.011575	48.413709
3503.928808	506524.762837	48.418714
3503.796545	506521.849003	48.423719
3503.571469	506526.236251	48.428724
3503.575107	506516.925326	48.433729
3503.725800	506528.337194	48.438733
3503.610498	506520.310071	48.443738
3503.356303	506529.863130	48.448743
3503.540482	506521.889873	48.453748
3503.681227	506526.522901	48.458753
3503.625668	506528.049751	48.463757
3503.817123	506521.087346	48.468762
3503.729038	506532.941752	48.473767
3503.673116	506521.717440	48.478772
3503.426710	506517.253044	48.483777
3503.710913	506514.172184	48.488781
3503.982307	506493.130295	48.493786
3503.574152	506491.474467	48.498791
3503.825002	506480.657044	48.503796
3503.840431	506490.218108	48.508801
3503.926355	506481.956762	48.513805
3503.771109	506491.696603	48.518810
3503.735529	506497.470712	48.523815
3503.664851	506488.019717	48.528820
3503.754536	506487.044204	48.533825
3503.824725	506498.823017	48.538829
3503.840866	506483.235677	48.543834
3503.777681	506466.547655	48.548839
3503.874257	506457.981012	48.553844
3503.830191	506464.262477	48.558849
3503.645845	506461.407465	48.563853
3504.124449	506455.765855	48.568858
3503.908234	506449.576259	48.573863
3503.972775	506456.295963	48.578868
3504.111525	506445.901039	48.583873
3504.092921	506417.719649	48.588877
3504.116370	506401.827479	48.593882
3503.928086	506408.738963	48.598887
3504.012104	506410.648565	48.603892
3504.142721	506403.392126	48.608897
3503.939017	506381.413186	48.613901
3504.080514	506367.172142	48.618906
3503.691623	506374.014146	48.623911
3504.020533	506368.750372	48.628916
3503.754972	506375.572882	48.633921
3503.689305	506368.347452	48.638925
3503.971779	506358.385163	48.643930
3503.802373	506334.477922	48.648935
3503.777754	506321.426910	48.653940
3504.086937	506323.250333	48.658945
3503.942947	506324.487574	48.663949
3503.965917	506315.021683	48.668954
3503.987137	506312.640162	48.673959
3504.093990	506295.469694	48.678964
3504.044090	506295.072842	48.683969
3503.781964	506290.357867	48.688973
3503.930683	506274.040974	48.693978
3503.566569	506292.112470	48.698983
3503.823424	506282.963800	48.703988
3503.960161	506283.853068	48.708993
3503.454044	506264.047011	48.713997
3503.754248	506277.257043	48.719002
3503.571956	506270.657215	48.724007
3503.883223	506237.970523	48.729012
3503.650038	506243.877151	48.734017
3503.624754	506244.184819	48.739021
3504.014954	506240.429346	48.744026
3503.569165	506239.740858	48.749031
3503.974656	506233.402320	48.754036
3503.841123	506231.146450	48.759041
3503.655157	506239.929869	48.764045
3503.841798	506235.194550	48.769050
3503.913030	506235.891771	48.774055
3503.816991	506216.729256	48.779060
3503.601889	506200.621602	48.784065
3503.362357	506196.510243	48.789069
3503.623313	506191.914969	48.794074
3503.331112	506196.667117	48.799079
3503.298014	506200.265088	48.804084
3503.811938	506225.029011	48.809089
3503.397124	506219.528535	48.814093
3503.680318	506201.824093	48.819098
3503.836030	506215.765425	48.824103
3503.930464	506196.825788	48.829108
3503.748048	506191.996986	48.834113
3503.720096	506200.148237	48.839117
3503.774627	506196.698815	48.844122
3503.607500	506206.390092	48.849127
3503.764759	506192.652423	48.854132
3504.019783	506192.612181	48.859137
3503.853177	506194.865027	48.864141
3503.872511	506187.423683	48.869146
3503.692554	506174.751321	48.874151
3503.733294	506157.995976	48.879156
3503.951399	506163.224088	48.884161
3503.630997	506152.749756	48.889165
3504.121083	506149.029077	48.894170
3503.715325	506163.059195	48.899175
3503.862326	506161.062582	48.904180
3504.136695	506156.414578	48.909185
3504.181841	506139.000704	48.914189
3503.967114	506132.456551	48.919194
3503.959615	506132.103594	48.924199
3504.068237	506129.354025	48.929204
3503.902642	506123.105711	48.934209
3503.568680	506095.176048	48.939213
3504.005921	506091.716716	48.944218
3503.496086	506083.245736	48.949223
3503.489328	506079.552971	48.954228
3503.313621	506077.860362	48.959233
3503.590746	506090.568170	48.964237
3503.717422	506080.731550	48.969242
3503.542638	506091.891541	48.974247
3504.127260	506081.425926	48.979252
3503.910180	506088.898703	48.984257
3503.615230	506086.415320	48.989261
3504.019377	506073.245752	48.994266
3503.931025	506085.505316	48.999271
3503.688952	506082.709967	49.004276
3504.046543	506070.407979	49.009281
3503.655362	506040.817426	49.014285
3503.942787	506040.772063	49.019290
3503.873176	506046.804708	49.024295
3503.918750	506040.775995	49.029300
3504.181501	506041.695960	49.034305
3503.899982	506033.745485	49.039309
3503.920452	506014.766739	49.044314
3503.764326	506011.907193	49.049319
3503.871209	505990.890700	49.054324
3504.143627	505992.365757	49.059329
3503.911190	506003.787925	49.064333
3503.613335	505997.155657	49.069338
3503.290954	505988.098384	49.074343
3503.582604	505992.100484	49.079348
3503.759547	505989.390697	49.084353
3503.353883	505995.678881	49.089357
3503.886953	505990.483928	49.094362
3503.525354	505987.960464	49.099367
3503.700046	505993.094285	49.104372
3503.528007	505979.509700	49.109377
3503.697228	505980.899867	49.114381
3503.840718	505970.605113	49.119386
3503.562174	505959.415625	49.124391
3503.617559	505957.838283	49.129396
3503.538708	505962.354366	49.134401
3503.219843	505958.103684	49.139405
3503.678340	505956.007213	49.144410
3503.499447	505963.575211	49.149415
3503.929831	505959.104903	49.154420
3503.973043	505958.237910	49.159425
3503.818164	505966.156324	49.164429
3503.818924	505964.688820	49.169434
3503.659039	505955.808254	49.174439
3503.624288	505953.992150	49.179444
3503.814767	505959.275292	49.184449
3503.437891	505964.698708	49.189453
3503.831842	505958.108886	49.194458
3503.864036	505950.817213	49.199463
3503.553114	505926.931778	49.204468
3503.387473	505923.921915	49.209473
3503.425222	505919.614859	49.214477
3503.727461	505918.656321	49.219482
3503.744210	505928.116282	49.224487
3503.494697	505917.276392	49.229492
3503.588600	505911.493004	49.234497
3503.598715	505916.754065	49.239501
3503.710177	505912.232949	49.244506
3503.688587	505918.662863	49.249511
3503.766178	505905.291773	49.254516
3503.922892	505909.163414	49.259521
3503.581103	505908.610280	49.264525
3503.557433	505908.057467	49.269530
3503.503134	505917.174451	49.274535
3503.731333	505906.157844	49.279540
3504.031470	505909.652603	49.284545
3503.612442	505912.755011	49.289549
3503.938309	505909.566256	49.294554
3503.938730	505910.831303	49.299559
3503.816532	505886.966585	49.304564
3503.562053	505876.684075	49.309569
3503.735500	505863.753221	49.314573
3503.665973	505860.475146	49.319578
3503.702370	505868.666983	49.324583
3503.577318	505877.946977	49.329588
3503.932066	505866.151313	49.334593
3503.709949	505859.405818	49.339597
3503.865826	505863.277601	49.344602
3503.724659	505869.422822	49.349607
3504.113848	505866.881876	49.354612
3504.071890	505846.850173	49.359617
3503.761592	505828.986147	49.364621
3503.640501	505826.880064	49.369626
3503.589351	505841.360413	49.374631
3503.615921	505827.390103	49.379636
3504.128084	505828.220056	49.384641
3503.819394	505832.620694	49.389645
3503.836591	505828.418068	49.394650
3503.908902	505829.064532	49.399655
3503.881040	505807.310083	49.404660
3503.944009	505795.509888	49.409665
3503.841767	505795.880329	49.414669
3504.089150	505788.099156	49.419674
3503.896128	505797.440538	49.424679
3504.023889	505785.326481	49.429684
3503.978941	505779.008372	49.434689
3504.097012	505758.141636	49.439693
3504.195405	505752.205680	49.444698
3504.253339	505748.350812	49.449703
3503.936089	505735.952841	49.454708
3503.923749	505718.547632	49.459713
3503.878798	505707.169253	49.464717
3503.698560	505706.641180	49.469722
3503.837658	505702.368654	49.474727
3503.827421	505698.878767	49.479732
3503.994325	505699.662093	49.484737
3503.976168	505703.105998	49.489741
3504.082284	505694.335062	49.494746
3503.759500	505673.537905	49.499751
3503.920506	505661.722124	49.504756
3503.783275	505656.835428	49.509761
3503.641639	505662.424166	49.514765
3503.599720	505657.218791	49.519770
3503.699243	505653.053713	49.524775
3503.754884	505666.606480	49.529780
3503.757216	505664.025447	49.534785
3503.807487	505656.578985	49.539789
3504.126051	505648.938308	49.544794
3503.714129	505640.957662	49.549799
3503.621860	505619.567377	49.554804
3503.990631	505628.010410	49.559809
3503.575105	505619.473694	49.564813
3504.116234	505613.467713	49.569818
3504.031148	505621.729470	49.574823
3503.756675	505628.756091	49.579828
3504.137512	505617.968191	49.584833
3503.891661	505597.462399	49.589837
3504.101250	505578.858110	49.594842
3503.617620	505580.402099	49.599847
3504.024484	505577.048673	49.604852
3503.832760	505579.356170	49.609857
3503.783861	505576.175987	49.614861
3503.970697	505575.893508	49.619866
3503.841751	505559.721039	49.624871
3504.111657	505529.215480	49.629876
3503.906718	505537.293809	49.634881
3503.987383	505529.083446	49.639885
3504.127280	505530.883107	49.644890
3503.968030	505530.857741	49.649895
3503.769552	505506.346720	49.654900
3503.912375	505478.694929	49.659905
3503.638408	505490.022790	49.664909
3503.756170	505488.941579	49.669914
3503.731796	505488.186451	49.674919
3503.714284	505492.237532	49.679924
3503.945455	505485.268437	49.684929
3503.928245	505491.394197	49.689933
3504.057423	505483.783382	49.694938
3503.932666	505467.913784	49.699943
3504.032323	505463.546227	49.704948
3503.770017	505462.272070	49.709953
3503.481084	505464.291327	49.714957
3503.837212	505472.888244	49.719962
3503.880264	505460.230716	49.724967
3503.670623	505454.849377	49.729972
3503.766929	505462.525905	49.734977
3503.920389	505456.125715	49.739981
3503.934212	505417.766338	49.744986
3503.768668	505420.626354	49.749991
3503.740818	505411.522228	49.754996
3504.223671	505409.573653	49.760001
3503.703201	505420.383884	49.765005
3503.689689	505409.506375	49.770010
3503.645038	505416.041326	49.775015
3503.849187	505412.011464	49.780020
3503.826201	505411.053700	49.785025
3503.751356	505387.332623	49.790029
3503.886464	505372.636346	49.795034
3503.500647	505383.374714	49.800039
3503.710269	505375.801740	49.805044
3503.630490	505370.956487	49.810049
3503.553517	505371.677167	49.815053
3504.100457	505366.682252	49.820058
3503.804956	505364.401266	49.825063
3503.927528	505375.666525	49.830068
3503.905976	505368.737328	49.835073
3503.891857	505352.445310	49.840077
3504.112852	505335.559477	49.845082
3504.016817	505330.008332	49.850087
3503.769051	505326.657121	49.855092
3503.717646	505327.272554	49.860097
3503.851897	505336.360040	49.865101
3504.100923	505323.872272	49.870106
3503.704816	505319.481831	49.875111
3503.803040	505292.899470	49.880116
3503.801201	505291.887754	49.885121
3503.918757	505294.601837	49.890125
3503.642164	505276.023465	49.895130
3503.507140	505298.512906	49.900135
3503.719633	505284.057342	49.905140
3503.618969	505271.270581	49.910145
3504.172607	505286.212441	49.915149
3503.986014	505285.179322	49.920154
3503.796956	505285.664703	49.925159
3504.095804	505249.941902	49.930164
3503.895501	505242.130039	49.935169
3503.436229	505242.556923	49.940173
3504.111741	505236.883800	49.945178
3503.967505	505233.111377	49.950183
3503.629433	505237.061372	49.955188
3503.919166	505228.767219	49.960193
3503.717175	505241.247753	49.965197
3503.905258	505223.557353	49.970202
3503.839298	505206.008296	49.975207
3503.547304	505197.148223	49.980212
3503.648360	505196.676881	49.985217
3503.492005	505199.231857	49.990221
3503.795862	505193.921087	49.995226
3503.553301	505194.718550	50.000231
3503.564217	505198.765207	50.005236
3503.728497	505193.071666	50.010241
3503.806344	505194.830566	50.015245
3503.584179	505190.058371	50.020250
3503.684326	505201.732119	50.025255
3504.143531	505197.611291	50.030260
3503.676708	505198.393596	50.035265
3503.554188	505196.237058	50.040269
3504.046766	505185.886666	50.045274
3503.788359	505167.305304	50.050279
3503.740516	505157.141520	50.055284
3503.861160	505153.276610	50.060289
3503.976334	505148.198064	50.065293
3504.066237	505157.343257	50.070298
3503.678751	505153.508055	50.075303
3503.982358	505159.026581	50.080308
3504.171563	505131.721138	50.085313
3503.987952	505127.752499	50.090317
3504.178141	505106.873587	50.095322
3503.846018	505115.427651	50.100327
3503.871413	505116.536995	50.105332
3503.882801	505105.301131	50.110337
3503.735114	505084.273179	50.115341
3503.647332	505078.568836	50.120346
3503.844551	505066.038469	50.125351
3504.035680	505070.967548	50.130356
3503.874662	505066.337468	50.135361
3503.899554	505075.492979	50.140365
3504.303295	505067.686773	50.145370
3504.265083	505045.781197	50.150375
3504.171430	505028.388152	50.155380
3503.674285	505025.076298	50.160385
3503.644253	505026.245013	50.165389
3503.742858	505024.104108	50.170394
3503.802150	505025.157496	50.175399
3503.875468	505020.793991	50.180404
3503.894068	505004.648291	50.185409
3503.795463	504984.624551	50.190413
3503.865718	504986.485881	50.195418
3503.755244	504991.412049	50.200423
3504.154799	504977.280897	50.205428
3504.177287	504981.528192	50.210433
3503.808763	504975.564562	50.215437
3503.799699	504944.646635	50.220442
3503.754232	504945.767190	50.225447
3503.621995	504932.681544	50.230452
3504.189480	504928.543539	50.235457
3503.513938	504925.715305	50.240461
3503.928728	504934.100798	50.245466
3503.962441	504932.425580	50.250471
3503.752142	504939.442334	50.255476
3503.878977	504929.048389	50.260481
3503.890704	504913.814576	50.265485
3503.910845	504900.401193	50.270490
3503.638346	504897.155017	50.275495
3503.312016	504882.683076	50.280500
3503.762357	504879.322648	50.285505
3503.823316	504893.684853	50.290509
3503.811641	504889.840798	50.295514
3503.482133	504894.751008	50.300519
3503.760701	504884.687289	50.305524
3503.674959	504888.243245	50.310529
3503.701723	504895.829805	50.315533
3503.694044	504890.365764	50.320538
3503.472513	504893.184110	50.325543
3503.987586	504887.384420	50.330548
3504.052279	504867.587760	50.335553
3503.684660	504862.787860	50.340557
3503.633462	504849.790553	50.345562
3503.909880	504848.684225	50.350567
3503.801137	504843.387959	50.355572
3503.730438	504857.720398	50.360577
3503.593676	504852.124933	50.365581
3503.900458	504845.548472	50.370586
3503.676401	504847.759965	50.375591
3503.361194	504855.704223	50.380596
3503.700207	504846.845446	50.385601
3503.457010	504847.339396	50.390605
3503.884140	504843.678999	50.395610
3503.505243	504850.266992	50.400615
3503.701450	504838.951140	50.405620
3503.911486	504825.052240	50.410625
3503.735305	504816.477298	50.415629
3504.145623	504794.905355	50.420634
3503.480982	504809.129290	50.425639
3503.507590	504800.168053	50.430644
3503.575332	504806.786677	50.435649
3503.248278	504806.079361	50.440653
3503.677714	504801.457095	50.445658
3503.631113	504797.011278	50.450663
3503.684692	504794.371411	50.455668
3503.535063	504800.670159	50.460673
3503.170407	504808.166808	50.465677
3503.780679	504799.366343	50.470682
3503.444110	504809.591226	50.475687
3503.615319	504790.233088	50.480692
3504.021555	504797.962132	50.485697
3503.843681	504803.354452	50.490701
3503.865440	504795.406080	50.495706
3503.614901	504806.072813	50.500711
3503.502818	504805.837570	50.505716
3503.529609	504795.965410	50.510721
3503.507354	504808.468449	50.515725
3503.538906	504792.016874	50.520730
3503.483109	504769.202840	50.525735
3503.370750	504739.616611	50.530740
3503.550563	504710.388996	50.535745
3503.272289	504669.341454	50.540749
3503.125777	504612.332225	50.545754
3503.138980	504561.926923	50.550759
3503.262056	504486.605978	50.555764
3503.209298	504406.302487	50.560769
3502.923145	504329.375542	50.565773
3503.041451	504207.445552	50.570778
3502.911671	504108.934414	50.575783
3502.691861	503973.291106	50.580788
3502.714307	503851.879871	50.585793
3502.237253	503700.333641	50.590797
3502.189859	503558.384452	50.595802
3501.903197	503410.348235	50.600807
3501.880420	503235.850874	50.605812
3501.836309	503063.278341	50.610817
3501.073988	502887.629170	50.615821
3501.496190	502692.862463	50.620826
3500.700302	502501.575900	50.625831
3500.479991	502300.833021	50.630836
3500.378401	502087.415882	50.635841
3499.970620	501870.197941	50.640845
3499.550638	501645.184687	50.645850
3499.273459	501411.541491	50.650855
3498.965859	501178.709877	50.655860
3498.735006	500930.931315	50.660865
3498.181772	500689.324902	50.665869
3498.226339	500436.231769	50.670874
3497.640155	500169.820887	50.675879
3497.118203	499914.076504	50.680884
3496.730871	499639.932190	50.685889
3496.451459	499369.158201	50.690893
3496.181644	499075.295244	50.695898
3495.647505	498789.265083	50.700903
3494.917907	498502.046310	50.705908
3494.505196	498202.724382	50.710913
3493.932874	497912.180786	50.715917
3493.720091	497610.134311	50.720922
3493.516055	497301.803730	50.725927
3493.005804	496979.290026	50.730932
3492.632452	496670.064160	50.735937
3491.843964	496354.316867	50.740941
3491.471682	496015.613551	50.745946
3491.266838	495691.104758	50.750951
3491.009902	495359.712498	50.755956
3490.403418	495006.344217	50.760961
3489.665235	494675.521944	50.765965
3489.339622	494322.804943	50.770970
3488.832910	493973.755554	50.775975
3488.414756	493619.723149	50.780980
3487.954697	493261.740825	50.785985
3487.107304	492891.558231	50.790989
3486.953404	492520.600284	50.795994
3486.372308	492163.324759	50.800999
3485.872791	491778.075269	50.806004
3485.373943	491394.033105	50.811009
3484.311884	491018.580189	50.816013
3484.095283	490629.919714	50.821018
3483.329738	490258.000397	50.826023
3482.864792	489866.628429	50.831028
3482.406409	489484.313225	50.836033
3481.721320	489094.681974	50.841037
3481.237482	488694.273037	50.846042
3480.596185	488309.227758	50.851047
3480.331712	487913.022250	50.856052
3479.782003	487517.765289	50.861057
3479.080412	487116.445582	50.866061
3478.429072	486695.353864	50.871066
3477.955120	486288.864506	50.876071
3477.345507	485887.200390	50.881076
3476.968994	485459.097841	50.886081
3475.518740	485048.582403	50.891085
3475.549440	484634.176496	50.896090
3474.713638	484223.191651	50.901095
3473.928121	483807.579750	50.906100
3473.552318	483390.779521	50.911105
3472.982720	482976.027549	50.916109
3472.263650	482553.791717	50.921114
3471.355138	482142.216795	50.926119
3471.041300	481702.468830	50.931124
3470.471391	481298.980189	50.936129
3469.463812	480862.464470	50.941133
3469.013560	480439.785660	50.946138
3468.171039	480017.869171	50.951143
3467.507030	479591.101382	50.956148
3467.126264	479157.185065	50.961153
3466.281545	478744.008427	50.966157
3465.471485	478309.989343	50.971162
3464.772777	477883.595585	50.976167
3464.041527	477453.650261	50.981172
3463.779597	477029.652446	50.986177
3462.758275	476612.810405	50.991181
3462.074875	476171.173123	50.996186
3461.388300	475736.571657	51.001191
3460.818918	475318.465525	51.006196
3460.161290	474892.254916	51.011201
3459.468573	474476.482362	51.016205
3459.047380	474049.760415	51.021210
3458.189033	473613.670415	51.026215
3457.551434	473188.485231	51.031220
3457.090012	472760.373914	51.036225
3456.404511	472320.731188	51.041229
3455.844596	471881.059154	51.046234
3454.812622	471464.670376	51.051239
3454.382756	471028.660205	51.056244
3453.770627	470596.269068	51.061249
3452.786990	470157.641087	51.066253
3452.027783	469731.288106	51.071258
3451.272568	469290.983287	51.076263
3450.850703	468864.407061	51.081268
3450.207053	468428.223800	51.086273
3448.844745	468014.859929	51.091277
3448.801939	467582.772364	51.096282
3448.058538	467148.352808	51.101287
3447.087149	466718.168907	51.106292
3446.486553	466294.661632	51.111297
3445.736118	465873.147157	51.116301
3445.205398	465451.082455	51.121306
3444.381152	465031.591254	51.126311
3443.550201	464591.250573	51.131316
3442.993714	464171.852215	51.136321
3442.526831	463759.125579	51.141325
3441.994881	463313.639956	51.146330
3440.924127	462900.231517	51.151335
3440.213864	462470.782558	51.156340
3439.804366	462030.322583	51.161345
3439.033134	461614.458402	51.166349
3438.167610	461186.073510	51.171354
3437.188206	460777.377564	51.176359
3436.921240	460345.381771	51.181364
3436.096108	459936.848534	51.186369
3435.256051	459511.064186	51.191373
3435.005858	459085.634817	51.196378
3433.901490	458657.136564	51.201383
3433.208770	458238.862256	51.206388
3432.688237	457827.451653	51.211393
3431.652046	457400.135626	51.216397
3430.997597	456982.135842	51.221402
3430.364624	456571.480614	51.226407
3429.709157	456148.392328	51.231412
3429.148734	455743.341476	51.236417
3428.501000	455327.541773	51.241421
3427.782042	454907.636195	51.246426
3426.726452	454485.746604	51.251431
3426.133590	454082.091447	51.256436
3425.774166	453658.300565	51.261441
3424.888190	453241.485265	51.266445
3424.430452	452834.387077	51.271450
3423.623140	452417.391990	51.276455
3423.064664	452003.445073	51.281460
3422.632977	451591.703211	51.286465
3421.315131	451169.488981	51.291469
3420.870441	450744.236589	51.296474
3420.251718	450339.961030	51.301479
3419.156035	449912.817198	51.306484
3418.621738	449513.233065	51.311489
3417.956540	449099.656712	51.316493
3417.226377	448681.363756	51.321498
3416.114961	448285.706540	51.326503
3415.693139	447876.485069	51.331508
3415.016786	447470.037180	51.336513
3414.164092	447070.359992	51.341517
3413.890377	446669.011162	51.346522
3413.000384	446263.844977	51.351527
3412.233458	445853.221756	51.356532
3411.641568	445453.323663	51.361537
3410.500399	445051.272441	51.366541
3410.154046	444641.982905	51.371546
3409.166744	444241.923929	51.376551
3408.690314	443857.918455	51.381556
3407.974805	443443.489463	51.386561
3406.966317	443060.062918	51.391565
3406.647774	442655.810987	51.396570
3405.827639	442268.941131	51.401575
3404.938683	441870.553007	51.406580
3404.259979	441473.495687	51.411585
3403.853342	441096.745058	51.416589
3403.301024	440686.659437	51.421594
3402.377619	440292.413592	51.426599
3401.584180	439892.048919	51.431604
3401.057265	439502.347383	51.436609
3400.230356	439111.265609	51.441613
3399.619683	438715.599661	51.446618
3399.173165	438333.507592	51.451623
3398.259065	437939.781058	51.456628
3397.480754	437550.723117	51.461633
3396.506756	437159.506851	51.466637
3396.136701	436766.310380	51.471642
3395.127843	436383.007967	51.476647
3394.394492	435997.371302	51.481652
3394.138057	435603.199307	51.486657
3393.168500	435224.290416	51.491661
3392.628485	434838.072293	51.496666
3392.091107	434448.496571	51.501671
3391.577482	434064.699795	51.506676
3390.789037	433680.331338	51.511681
3389.826073	433294.334350	51.516685
3389.466331	432891.580244	51.521690
3388.647286	432507.732189	51.526695
3387.866501	432126.665346	51.531700
3387.326044	431729.152114	51.536705
3386.491077	431353.008311	51.541709
3385.561758	430967.351958	51.546714
3385.348569	430585.537855	51.551719
3384.534952	430195.738188	51.556724
3383.909207	429814.231940	51.561729
3382.849473	429436.724739	51.566733
3382.519357	429045.764951	51.571738
3381.501946	428673.750554	51.576743
3380.924293	428294.068382	51.581748
3380.400921	427906.169593	51.586753
3379.535333	427531.600997	51.591757
3378.926524	427145.685426	51.596762
3378.479255	426757.960991	51.601767
3377.563662	426385.796798	51.606772
3376.835219	426011.616884	51.611777
3375.846673	425634.552205	51.616781
3375.274029	425242.279562	51.621786
3374.690529	424881.013718	51.626791
3373.986562	424509.323434	51.631796
3373.210813	424134.743965	51.636801
3372.680042	423756.869532	51.641805
3371.956702	423385.141524	51.646810
3370.991696	423013.294267	51.651815
3370.281152	422635.483533	51.656820
3369.958132	422267.080627	51.661825
3369.085853	421903.433351	51.666829
3368.620229	421525.263830	51.671834
3367.946989	421158.019126	51.676839
3367.308277	420785.912382	51.681844
3366.724456	420414.147602	51.686849
3365.755629	420039.949312	51.691853
3365.212808	419663.646431	51.696858
3364.455925	419293.494466	51.701863
3363.485056	418914.200851	51.706868
3363.099792	418550.331172	51.711873
3362.340713	418187.328840	51.716877
3361.782749	417817.557902	51.721882
3360.729465	417451.848999	51.726887
3360.223874	417083.076402	51.731892
3359.544726	416715.393504	51.736897
3358.794430	416363.798893	51.741901
3358.222196	415986.588021	51.746906
3357.671518	415626.695877	51.751911
3357.018997	415256.652701	51.756916
3356.410649	414890.535874	51.761921
3355.359374	414523.137874	51.766925
3354.964150	414148.491957	51.771930
3354.272755	413795.002011	51.776935
3353.252012	413431.980975	51.781940
3352.788618	413064.497038	51.786945
3352.199923	412704.701781	51.791949
3351.540627	412332.970992	51.796954
3350.815542	411978.702222	51.801959
3349.986722	411601.983381	51.806964
3349.721037	411235.410972	51.811969
3348.570517	410880.611930	51.816973
3348.093387	410504.255548	51.821978
3347.350468	410147.325070	51.826983
3346.484178	409779.991211	51.831988
3346.246034	409422.311599	51.836993
3345.448647	409071.399517	51.841997
3344.755275	408691.293674	51.847002
3344.017812	408344.480471	51.852007
3343.230868	407972.715735	51.857012
3343.128108	407616.746899	51.862017
3342.150901	407260.048143	51.867021
3341.633763	406884.288420	51.872026
3340.552757	406523.607560	51.877031
3339.638547	406163.836431	51.882036
3338.890921	405807.186184	51.887041
3338.392632	405442.740850	51.892045
3337.990983	405083.663988	51.897050
3337.402388	404735.261651	51.902055
3336.504967	404376.661702	51.907060
3336.095630	404009.643985	51.912065
3335.173834	403655.741627	51.917069
3334.399928	403295.330657	51.922074
3334.132608	402938.927594	51.927079
3333.386988	402572.353011	51.932084
3332.745324	402209.544974	51.937089
3331.820024	401854.047160	51.942093
3331.082229	401492.720409	51.947098
3330.281736	401139.762151	51.952103
3329.441543	400777.401386	51.957108
3328.948849	400417.218462	51.962113
3327.781777	400072.694745	51.967117
3327.670820	399717.197059	51.972122
3326.962901	399370.102162	51.977127
3326.062491	399013.654010	51.982132
3325.356279	398660.196280	51.987137
3324.895157	398312.924027	51.992141
3324.551633	397949.995673	51.997146
3323.698870	397605.497931	52.002151
3322.535645	397248.284147	52.007156
3322.368285	396894.798543	52.012161
3321.404347	396552.468287	52.017165
3320.827236	396187.472990	52.022170
3320.253523	395847.056727	52.027175
3319.479262	395488.643997	52.032180
3319.018978	395139.838544	52.037185
3318.077324	394787.826011	52.042189
3317.439335	394430.372000	52.047194
3316.774884	394090.257452	52.052199
3316.288352	393732.873852	52.057204
3315.607591	393381.441100	52.062209
3314.620966	393041.341633	52.067213
3314.037053	392689.886481	52.072218
3313.378258	392346.931570	52.077223
3312.843184	391992.308878	52.082228
3312.040525	391640.979355	52.087233
3311.397229	391292.901016	52.092237
3311.081968	390939.732952	52.097242
3310.120320	390597.902009	52.102247
3309.538208	390236.810605	52.107252
3308.872420	389888.696445	52.112257
3308.091972	389544.233067	52.117261
3307.546478	389191.541561	52.122266
3306.926997	388845.367730	52.127271
3305.996949	388477.219099	52.132276
3305.388207	388129.332954	52.137281
3304.528517	387791.171338	52.142285
3304.008326	387440.009676	52.147290
3302.952465	387090.556763	52.152295
3302.076263	386747.098762	52.157300
3301.599166	386404.006690	52.162305
3300.703985	386078.574786	52.167309
3300.519172	385732.048030	52.172314
3299.556240	385391.057665	52.177319
3298.946718	385064.020334	52.182324
3298.458114	384712.471383	52.187329
3297.421451	384378.909028	52.192333
3297.093337	384028.243706	52.197338
3296.393192	383695.028883	52.202343
3295.639852	383358.335388	52.207348
3294.944426	383012.296275	52.212353
3293.991248	382671.152237	52.217357
3293.808228	382330.163057	52.222362
3292.864755	381986.976726	52.227367
3292.073454	381652.842662	52.232372
3291.589983	381315.706769	52.237377
3290.683864	380980.440489	52.242381
3290.428810	380647.459028	52.247386
3289.813356	380320.025316	52.252391
3288.923115	379972.107273	52.257396
3288.357038	379616.657246	52.262401
3287.689622	379290.850805	52.267405
3287.302111	378949.965643	52.272410
3286.480450	378611.333547	52.277415
3285.608147	378271.053267	52.282420
3284.866684	377928.511061	52.287425
3283.952934	377589.732112	52.292429
3283.789249	377241.623979	52.297434
3282.929584	376917.634182	52.302439
3282.601276	376577.482208	52.307444
3281.595586	376236.442467	52.312449
3280.738463	375900.412721	52.317453
3280.462644	375555.970469	52.322458
3279.512818	375221.348730	52.327463
3278.653314	374885.794208	52.332468
3278.580158	374545.304910	52.337473
3277.646401	374209.120620	52.342477
3277.188587	373869.271585	52.347482
3276.593649	373531.756265	52.352487
3275.803384	373189.944607	52.357492
3275.283764	372843.254046	52.362497
3274.630920	372500.575497	52.367501
3273.878560	372159.512502	52.372506
3273.135814	371824.118070	52.377511
3272.386463	371477.248972	52.382516
3271.591534	371136.871241	52.387521
3270.442651	370811.963081	52.392525
3269.879543	370471.797722	52.397530
3269.386719	370126.912143	52.402535
3268.691207	369801.542948	52.407540
3268.153256	369463.731498	52.412545
3267.259117	369138.465007	52.417549
3266.778830	368794.202737	52.422554
3265.821797	368468.177924	52.427559
3264.971699	368132.466140	52.432564
3264.785683	367793.008629	52.437569
3263.763611	367474.542722	52.442573
3263.474052	367135.859739	52.447578
3262.754392	366809.225290	52.452583
3261.915797	366469.402824	52.457588
3261.636009	366143.737013	52.462593
3260.422413	365816.562767	52.467597
3259.873494	365481.546439	52.472602
3259.028161	365160.186384	52.477607
3258.577277	364832.121027	52.482612
3257.995671	364488.502754	52.487617
3257.248765	364170.351367	52.492621
3256.542479	363845.016258	52.497626
3256.008009	363498.889590	52.502631
3255.283368	363180.524236	52.507636
3254.808434	362849.115262	52.512641
3253.710303	362522.178896	52.517645
3253.563690	362188.804941	52.522650
3252.781480	361853.417232	52.527655
3251.925316	361532.135228	52.532660
3251.296008	361198.296215	52.537665
3250.231768	360869.994337	52.542669
3249.906570	360548.112725	52.547674
3249.236386	360225.672806	52.552679
3248.498338	359890.416819	52.557684
3248.056998	359562.516289	52.562689
3247.183355	359236.183216	52.567693
3246.429331	358899.879546	52.572698
3246.041036	358578.834401	52.577703
3245.362653	358254.957561	52.582708
3244.676881	357917.007707	52.587713
3244.076528	357597.516443	52.592717
3243.187122	357257.838420	52.597722
3242.538410	356927.586352	52.602727
3242.069539	356606.693720	52.607732
3241.350974	356274.234429	52.612737
3240.578634	355951.222535	52.617741
3239.822020	355620.189987	52.622746
3238.990463	355294.027693	52.627751
3238.157318	354974.072910	52.632756
3237.925976	354642.136519	52.637761
3236.980844	354322.526177	52.642765
3236.225884	353991.559082	52.647770
3235.734693	353673.577948	52.652775
3235.210839	353348.219803	52.657780
3234.698118	353011.685661	52.662785
3233.470793	352702.645877	52.667789
3233.359257	352376.249351	52.672794
3232.312908	352046.410267	52.677799
3231.560547	351726.727986	52.682804
3231.166310	351396.476283	52.687809
3230.337028	351085.938841	52.692813
3229.933862	350754.692012	52.697818
3229.119247	350432.059566	52.702823
3228.397418	350111.650157	52.707828
3227.742662	349779.979011	52.712833
3227.028129	349461.167992	52.717837
3226.451511	349125.484702	52.722842
3225.550170	348802.245453	52.727847
3224.686240	348486.150210	52.732852
3224.369960	348162.305625	52.737857
3223.745368	347848.790381	52.742861
3222.802070	347514.606040	52.747866
3222.473880	347211.348296	52.752871
3221.711660	346887.770473	52.757876
3221.055902	346558.956248	52.762881
3220.081925	346246.021821	52.767885
3219.779881	345916.435255	52.772890
3218.962380	345602.098107	52.777895
3218.271930	345281.019605	52.782900
3217.801974	344949.977793	52.787905
3216.896233	344636.056587	52.792909
3215.957056	344318.473716	52.797914
3215.644771	343997.481014	52.802919
3214.775206	343678.687357	52.807924
3214.445236	343359.857523	52.812929
3213.532298	343044.885355	52.817933
3213.230805	342716.400591	52.822938
3212.356915	342407.985991	52.827943
3211.336715	342088.774937	52.832948
3210.890674	341755.675135	52.837953
3210.262101	341444.544107	52.842957
3209.517233	341131.469888	52.847962
3208.662737	340814.567753	52.852967
3208.230224	340495.739029	52.857972
3207.777437	340176.046401	52.862977
3206.755598	339858.758566	52.867981
3206.360156	339537.475376	52.872986
3205.414855	339221.114045	52.877991
3204.942886	338895.130445	52.882996
3204.106224	338584.119847	52.888001
3203.418758	338267.534779	52.893005
3202.707050	337960.523381	52.898010
3202.046822	337646.272879	52.903015
3201.296794	337326.587453	52.908020
3200.876242	337004.226339	52.913025
3200.017137	336700.108845	52.918029
3199.551266	336376.937212	52.923034
3199.125972	336057.983370	52.928039
3198.214453	335749.924019	52.933044
3197.441636	335435.757121	52.938049
3196.725642	335119.517747	52.943053
3196.083398	334801.457770	52.948058
3195.501457	334488.681854	52.953063
3194.967253	334169.278051	52.958068
3194.116964	333848.726265	52.963073
3193.452481	333543.545399	52.968077
3192.824407	333225.526773	52.973082
3191.986171	332917.061146	52.978087
3191.474234	332602.483561	52.983092
3191.087708	332286.128126	52.988097
3190.314471	331966.370154	52.993101
3189.330605	331647.407813	52.998106
3188.392796	331341.420510	53.003111
3187.709912	331026.913913	53.008116
3187.263273	330717.027487	53.013121
3186.304690	330407.806282	53.018125
3185.857988	330092.341763	53.023130
3185.315093	329777.985840	53.028135
3184.410215	329478.375680	53.033140
3183.728273	329172.593403	53.038145
3182.930176	328872.276517	53.043149
3182.605109	328558.237415	53.048154
3181.808711	328260.412832	53.053159
3180.963650	327944.747677	53.058164
3180.722875	327640.697028	53.063169
3179.806229	327336.242914	53.068173
3179.124090	327021.337442	53.073178
3178.479348	326715.463043	53.078183
3177.633784	326406.920461	53.083188
3177.123261	326100.436850	53.088193
3176.472341	325805.838717	53.093197
3175.683742	325497.538180	53.098202
3174.978208	325196.021238	53.103207
3174.368160	324888.148401	53.108212
3173.785914	324583.630793	53.113217
3172.909933	324281.449982	53.118221
3172.287144	323977.114756	53.123226
3171.979594	323679.552043	53.128231
3171.040034	323361.312121	53.133236
3170.585919	323064.152315	53.138241
3169.395939	322759.062165	53.143245
3168.816568	322454.027076	53.148250
3168.445453	322160.593767	53.153255
3167.745431	321856.492241	53.158260
3167.195837	321548.037388	53.163265
3166.474960	321251.550024	53.168269
3165.770867	320941.640698	53.173274
3165.273650	320641.627635	53.178279
3164.542187	320332.153349	53.183284
3163.899681	320019.888563	53.188289
3163.109675	319722.719546	53.193293
3162.325199	319421.602051	53.198298
3161.871352	319115.898977	53.203303
3160.742773	318820.231926	53.208308
3160.553391	318504.732924	53.213313
3159.592641	318212.449333	53.218317
3159.163277	317911.983670	53.223322
3158.554359	317600.036360	53.228327
3157.707950	317299.354646	53.233332
3157.033021	316993.348597	53.238337
3156.319321	316696.208780	53.243341
3156.031372	316387.364131	53.248346
3155.440348	316085.594247	53.253351
3154.552524	315784.557901	53.258356
3154.020691	315468.262805	53.263361
3153.184319	315169.482676	53.268365
3152.228639	314863.310711	53.273370
3152.070419	314557.469984	53.278375
3151.204987	314256.018101	53.283380
3150.721963	313954.835854	53.288385
3149.965025	313656.980878	53.293389
3149.529137	313340.587614	53.298394
3148.248376	313042.711919	53.303399
3147.322207	312739.253629	53.308404
3147.267784	312436.547781	53.313409
3146.932524	312138.825531	53.318413
3145.809778	311824.471721	53.323418
3145.290088	311524.587067	53.328423
3144.470508	311215.632869	53.333428
3144.094565	310909.485079	53.338433
3143.278202	310605.774324	53.343437
3142.638197	310300.685236	53.348442
3141.880081	309990.190090	53.353447
3141.143981	309694.332731	53.358452
3140.576714	309381.972307	53.363457
3139.636435	309082.326013	53.368461
3139.113204	308785.337696	53.373466
3138.736470	308486.110021	53.378471
3137.728122	308187.974673	53.383476
3137.113010	307877.425883	53.388481
3136.321092	307584.118611	53.393485
3135.793453	307277.425142	53.398490
3135.361317	306976.929294	53.403495
3134.338167	306682.332304	53.408500
3133.631554	306370.928426	53.413505
3132.934777	306075.565366	53.418509
3132.423389	305770.164417	53.423514
3131.741578	305471.079676	53.428519
3130.936625	305177.386955	53.433524
3130.490156	304872.763086	53.438529
3129.597380	304580.203435	53.443533
3129.237903	304286.463745	53.448538
3128.477767	303976.667047	53.453543
3127.754252	303680.207910	53.458548
3127.161499	303385.128074	53.463553
3126.410786	303083.808019	53.468557
3125.879265	302776.773749	53.473562
3125.072323	302481.751407	53.478567
3124.425408	302185.429847	53.483572
3124.057042	301882.467908	53.488577
3122.931407	301581.713402	53.493581
3122.506562	301281.636857	53.498586
3121.683478	300990.281249	53.503591
3120.637323	300698.552929	53.508596
3120.331646	300392.802291	53.513601
3119.597459	300103.137202	53.518605
3118.914503	299803.404254	53.523610
3118.399178	299509.144976	53.528615
3117.582021	299210.756427	53.533620
3117.038697	298914.743328	53.538625
3116.286593	298627.013916	53.543629
3115.309566	298329.107491	53.548634
3114.958290	298027.459796	53.553639
3114.286380	297735.030331	53.558644
3113.701851	297440.880280	53.563649
3112.594172	297145.284521	53.568653
3112.166517	296851.439748	53.573658
3111.380148	296558.873677	53.578663
3110.331274	296269.532048	53.583668
3110.359185	295978.542496	53.588673
3109.480368	295694.775807	53.593677
3109.117499	295394.322551	53.598682
3108.251627	295101.690420	53.603687
3107.106366	294817.047807	53.608692
3106.758197	294521.480587	53.613697
3106.083351	294240.531861	53.618701
3105.669752	293943.115060	53.623706
3104.887150	293654.389629	53.628711
3104.112195	293364.185495	53.633716
3103.850996	293060.580266	53.638721
3102.918677	292777.174561	53.643725
3102.163186	292478.332747	53.648730
3101.925597	292185.673569	53.653735
3101.001632	291887.112320	53.658740
3100.500387	291595.665627	53.663745
3099.534832	291310.276921	53.668749
3099.069703	291010.827007	53.673754
3098.467665	290713.690479	53.678759
3097.294161	290422.145037	53.683764
3096.997913	290121.190220	53.688769
3096.118048	289844.241548	53.693773
3095.203901	289551.711789	53.698778
3094.626166	289263.865472	53.703783
3094.077299	288972.678015	53.708788
3093.564349	288683.878543	53.713793
3092.579481	288395.662819	53.718797
3091.945947	288106.550776	53.723802
3091.245909	287821.014477	53.728807
3090.623049	287543.513543	53.733812
3090.159979	287248.592511	53.738817
3089.516425	286957.647296	53.743821
3088.571456	286680.986095	53.748826
3088.021891	286390.280188	53.753831
3087.105123	286106.253819	53.758836
3086.858635	285820.847747	53.763841
3085.658909	285542.723347	53.768845
3085.559937	285249.653081	53.773850
3085.058195	284967.928675	53.778855
3083.970676	284678.860093	53.783860
3083.464473	284389.393689	53.788865
3082.555451	284104.422282	53.793869
3082.006440	283816.719556	53.798874
3081.360260	283531.731643	53.803879
3080.227474	283260.191340	53.808884
3080.008800	282969.914451	53.813889
3079.234709	282686.907314	53.818893
3078.550074	282410.991487	53.823898
3078.122265	282135.315018	53.828903
3077.178568	281844.897546	53.833908
3076.907137	281551.903110	53.838913
3076.075134	281272.750097	53.843917
3075.446216	280986.280892	53.848922
3074.451815	280700.786256	53.853927
3073.882117	280418.000326	53.858932
3073.513890	280134.749435	53.863937
3072.531616	279858.675800	53.868941
3072.191522	279580.768589	53.873946
3071.551469	279288.493684	53.878951
3070.588708	279015.065378	53.883956
3069.772203	278713.140243	53.888961
3068.786203	278430.776059	53.893965
3068.588915	278145.383583	53.898970
3067.763090	277864.547470	53.903975
3067.303971	277585.283233	53.908980
3066.727166	277297.556595	53.913985
3065.800977	277017.372897	53.918989
3065.396422	276728.014384	53.923994
3064.802312	276461.480026	53.928999
3064.231063	276172.300623	53.934004
3063.744283	275877.555710	53.939009
3062.739508	275594.073370	53.944013
3062.005502	275306.065719	53.949018
3061.373262	275034.239842	53.954023
3060.852660	274751.011916	53.959028
3059.969815	274466.440555	53.964033
3059.417127	274181.995220	53.969037
3059.064035	273900.523572	53.974042
3058.210292	273616.049498	53.979047
3057.381742	273331.902543	53.984052
3056.886168	273046.123872	53.989057
3056.228752	272763.910949	53.994061
3055.647677	272475.191542	53.999066
3054.712101	272191.087121	54.004071
3053.967879	271908.556968	54.009076
3053.107730	271616.188956	54.014081
3052.290111	271349.613723	54.019085
3051.738094	271074.948508	54.024090
3051.310032	270794.813510	54.029095
3050.177318	270524.289802	54.034100
3050.043563	270240.517334	54.039105
3049.056962	269968.187868	54.044109
3048.074487	269695.297529	54.049114
3047.665723	269419.387620	54.054119
3046.845723	269140.715911	54.059124
3046.472783	268864.163819	54.064129
3045.705343	268608.074367	54.069133
3045.101479	268324.962750	54.074138
3044.694731	268046.022318	54.079143
3043.923761	267778.269282	54.084148
3043.390282	267490.104184	54.089153
3042.564521	267227.784803	54.094157
3041.809136	266938.967462	54.099162
3041.232218	266666.166995	54.104167
3040.294715	266394.646216	54.109172
3039.913165	266117.307251	54.114177
3039.344115	265842.697744	54.119181
3038.493091	265571.392949	54.124186
3037.680667	265288.927166	54.129191
3036.904863	265014.070732	54.134196
3036.672870	264744.196552	54.139201
3036.149894	264472.356623	54.144205
3035.223803	264194.341005	54.149210
3034.559785	263912.896851	54.154215
3033.902006	263641.562721	54.159220
3033.633935	263362.654043	54.164225
3032.371459	263098.521594	54.169229
3031.836281	262821.234624	54.174234
3031.492051	262547.967054	54.179239
3030.401503	262271.914486	54.184244
3029.840641	261991.295957	54.189249
3028.949501	261720.968034	54.194253
3028.628329	261443.062573	54.199258
3027.990830	261168.187165	54.204263
3026.646252	260897.345964	54.209268
3026.314253	260623.874360	54.214273
3025.417400	260358.463827	54.219277
3024.981290	260086.308061	54.224282
3024.610538	259813.530986	54.229287
3023.642202	259551.112247	54.234292
3023.111721	259281.926458	54.239297
3022.206294	259004.319560	54.244301
3021.434477	258736.853387	54.249306
3020.907304	258475.919404	54.254311
3020.220712	258208.644031	54.259316
3020.060319	257927.507715	54.264321
3019.033030	257674.370391	54.269325
3018.471386	257404.503893	54.274330
3017.866472	257125.145189	54.279335
3017.179548	256858.406171	54.284340
3016.734838	256580.423468	54.289345
3015.931341	256320.656125	54.294349
3015.334067	256044.251738	54.299354
3014.646876	255769.746509	54.304359
3013.853793	255506.209313	54.309364
3013.041960	255221.894143	54.314369
3012.442307	254956.060424	54.319373
3011.772071	254684.278898	54.324378
3011.042072	254412.863730	54.329383
3010.264478	254139.775629	54.334388
3009.660607	253882.882923	54.339393
3008.789076	253617.170390	54.344397
3008.362837	253350.369053	54.349402
3007.749136	253080.006915	54.354407
3006.671772	252813.996998	54.359412
3006.537064	252547.609041	54.364417
3005.730813	252293.399054	54.369421
3004.956604	252023.445851	54.374426
3004.117136	251746.423614	54.379431
3003.319513	251489.259240	54.384436
3002.991076	251222.521888	54.389441
3002.401382	250968.814297	54.394445
3002.040951	250695.690681	54.399450
3001.320791	250432.811076	54.404455
3000.348383	250165.540629	54.409460
3000.008808	249892.364070	54.414465
2999.234843	249635.351528	54.419469
2998.771029	249361.227788	54.424474
2998.095217	249092.995335	54.429479
2997.285894	248818.316014	54.434484
2996.634805	248557.414852	54.439489
2995.596531	248288.477143	54.444493
2995.398666	248015.663332	54.449498
2994.322331	247748.286024	54.454503
2993.592721	247492.874308	54.459508
2993.278905	247212.873373	54.464513
2992.591786	246950.478146	54.469517
2991.591630	246691.952835	54.474522
2990.895908	246419.908306	54.479527
2990.183420	246161.924112	54.484532
2989.902012	245882.659092	54.489537
2988.872689	245624.853347	54.494541
2988.273635	245360.868181	54.499546
2987.639342	245093.527618	54.504551
2986.543087	244839.426440	54.509556
2986.408589	244570.276106	54.514561
2985.727262	244318.096528	54.519565
2984.990202	244049.475525	54.524570
2984.060419	243794.153070	54.529575
2983.280033	243525.616375	54.534580
2983.218588	243276.320088	54.539585
2981.972672	243017.000190	54.544589
2981.445158	242753.772763	54.549594
2980.801547	242494.944269	54.554599
2980.271990	242239.867086	54.559604
2979.499422	241971.510639	54.564609
2979.096739	241717.789543	54.569613
2978.368374	241455.615212	54.574618
2977.857954	241198.678177	54.579623
2976.920435	240933.736923	54.584628
2976.949613	240660.647258	54.589633
2975.738902	240407.998984	54.594637
2975.091354	240137.538647	54.599642
2974.644528	239875.068518	54.604647
2973.610983	239612.539066	54.609652
2973.408469	239351.915809	54.614657
2972.564483	239091.598400	54.619661
2972.034189	238812.490101	54.624666
2971.288154	238551.318084	54.629671
2970.279001	238292.862073	54.634676
2969.776980	238027.680203	54.639681
2969.372312	237762.534477	54.644685
2968.506624	237498.582788	54.649690
2967.530381	237238.850803	54.654695
2966.971524	236976.583349	54.659700
2966.479170	236709.391457	54.664705
2965.884373	236461.237964	54.669709
2964.996545	236193.677072	54.674714
2964.720352	235934.397601	54.679719
2963.962664	235670.789769	54.684724
2963.454334	235400.089696	54.689729
2962.340071	235138.347570	54.694733
2961.794921	234879.316995	54.699738
2961.175492	234611.157454	54.704743
2960.597629	234356.309378	54.709748
2960.029766	234086.946272	54.714753
2959.317677	233829.956388	54.719757
2958.667582	233562.262813	54.724762
2957.877133	233297.927843	54.729767
2957.077476	233032.423736	54.734772
2956.729088	232769.726218	54.739777
2955.567747	232519.533078	54.744781
2954.962657	232250.511871	54.749786
2954.655445	231994.786743	54.754791
2953.751221	231738.978571	54.759796
2953.278728	231475.845886	54.764801
2952.272817	231209.590097	54.769805
2951.857474	230948.766922	54.774810
2951.364814	230696.664859	54.779815
2950.599115	230430.220478	54.784820
2949.864794	230169.195359	54.789825
2949.347116	229910.886599	54.794829
2948.358595	229645.447328	54.799834
2947.980270	229378.995592	54.804839
2946.941721	229120.033138	54.809844
2946.651246	228864.212121	54.814849
2945.514982	228604.553693	54.819853
2944.900618	228350.313136	54.824858
2944.235020	228099.951597	54.829863
2943.649119	227838.527812	54.834868
2942.841577	227580.729975	54.839873
2942.351039	227331.157688	54.844877
2941.483255	227073.880123	54.849882
2941.377681	226818.443174	54.854887
2940.600609	226561.152782	54.859892
2939.714792	226304.746064	54.864897
2939.372174	226047.286601	54.869901
2938.575055	225786.984596	54.874906
2937.870644	225524.899187	54.879911
2936.842817	225269.383783	54.884916
2936.377281	225010.342939	54.889921
2935.817488	224752.298067	54.894925
2935.289251	224494.350852	54.899930
2934.577044	224231.506967	54.904935
2933.750570	223986.746209	54.909940
2933.143792	223717.343965	54.914945
2932.394673	223460.657108	54.919949
2931.813610	223202.098603	54.924954
2931.074899	222954.870189	54.929959
2930.484847	222701.750472	54.934964
2929.998524	222437.069055	54.939969
2928.963690	222179.680516	54.944973
2928.263161	221922.532685	54.949978
2928.006859	221666.091894	54.954983
2927.177422	221406.993056	54.959988
2926.714585	221147.722481	54.964993
2925.428131	220906.697580	54.969997
2925.036471	220646.742762	54.975002
2924.531112	220386.997780	54.980007
2923.735336	220142.486078	54.985012
2923.479332	219880.577521	54.990017
2922.294608	219623.501381	54.995021
2921.731021	219368.810032	55.000026
2920.939250	219107.549118	55.005031
2920.786067	218859.401113	55.010036
2920.073698	218602.635620	55.015041
2919.023978	218352.823715	55.020045
2918.456205	218090.639914	55.025050
2917.633133	217838.400799	55.030055
2916.832937	217584.911487	55.035060
2916.736726	217326.716402	55.040065
2915.855852	217076.996749	55.045069
2915.297481	216830.218230	55.050074
2914.501826	216571.767487	55.055079
2913.731217	216318.863537	55.060084
2913.281212	216062.943908	55.065089
2912.457845	215811.844915	55.070093
2911.839622	215554.948207	55.075098
2911.363804	215297.189807	55.080103
2910.333491	215045.833596	55.085108
2909.913513	214796.749197	55.090113
2909.126985	214544.070635	55.095117
2908.208988	214287.047933	55.100122
2907.655347	214037.580161	55.105127
2906.924040	213790.114351	55.110132
2906.297389	213529.026213	55.115137
2905.357946	213288.150340	55.120141
2904.895141	213040.975722	55.125146
2904.436806	212785.769780	55.130151
2903.527277	212550.008611	55.135156
2903.104785	212284.616356	55.140161
2902.310595	212042.996513	55.145165
2901.841681	211801.949736	55.150170
2901.057893	211543.325392	55.155175
2900.209829	211295.136468	55.160180
2899.557647	211045.071932	55.165185
2898.709506	210800.168731	55.170189
2898.041197	210560.061839	55.175194
2897.581539	210315.735372	55.180199
2896.862059	210065.583499	55.185204
2896.326433	209807.194150	55.190209
2895.515406	209572.891956	55.195213
2894.669070	209315.852038	55.200218
2893.979333	209079.266974	55.205223
2893.371438	208835.886100	55.210228
2893.130476	208587.891658	55.215233
2892.170592	208352.332148	55.220237
2891.674345	208104.889160	55.225242
2891.195905	207855.675256	55.230247
2890.307692	207609.212696	55.235252
2889.971677	207361.594611	55.240257
2889.141182	207114.017651	55.245261
2888.703148	206855.268826	55.250266
2888.078120	206608.285029	55.255271
2887.011404	206362.021261	55.260276
2886.569715	206101.265399	55.265281
2885.781523	205862.723000	55.270285
2885.226857	205608.706965	55.275290
2884.831374	205364.275510	55.280295
2883.839368	205109.452724	55.285300
2883.380552	204849.468683	55.290305
2882.512639	204605.115190	55.295309
2882.115303	204357.837461	55.300314
2881.284852	204110.922075	55.305319
2880.595865	203863.259933	55.310324
2880.177989	203597.344489	55.315329
2879.531609	203356.333668	55.320333
2878.815268	203090.913249	55.325338
2878.474956	202840.425980	55.330343
2877.199876	202588.700682	55.335348
2876.528404	202333.444877	55.340353
2876.120849	202085.313188	55.345357
2875.223084	201836.509382	55.350362
2874.903453	201576.759926	55.355367
2873.838200	201337.300228	55.360372
2873.222752	201079.725144	55.365377
2872.439790	200828.375215	55.370381
2871.792355	200580.848124	55.375386
2871.297699	200322.341184	55.380391
2870.383414	200083.512009	55.385396
2869.523211	199843.390033	55.390401
2868.858394	199594.508509	55.395405
2868.281401	199351.162489	55.400410
2867.795448	199109.737395	55.405415
2866.818094	198874.537506	55.410420
2866.526293	198628.108231	55.415425
2865.835146	198384.504685	55.420429
2865.298187	198139.745294	55.425434
2864.811700	197889.074606	55.430439
2863.579082	197654.518572	55.435444
2863.380779	197395.584226	55.440449
2862.690281	197154.811137	55.445453
2862.327505	196912.002179	55.450458
2861.647944	196650.259165	55.455463
2860.608974	196401.413591	55.460468
2860.356455	196149.047185	55.465473
2859.108951	195902.476550	55.470477
2858.383583	195651.587140	55.475482
2857.837372	195398.863705	55.480487
2857.030967	195169.353826	55.485492
2856.632006	194917.156585	55.490497
2856.043355	194676.467913	55.495501
2855.556225	194420.546144	55.500506
2854.926320	194171.824688	55.505511
2853.947533	193925.119207	55.510516
2853.641141	193668.116508	55.515521
2852.462519	193428.786855	55.520525
2851.623690	193183.589710	55.525530
2851.420160	192930.111734	55.530535
2850.522740	192687.407444	55.535540
2850.066618	192439.977575	55.540545
2849.335418	192201.804418	55.545549
2848.324957	191959.706871	55.550554
2847.720833	191709.784815	55.555559
2846.784700	191472.245634	55.560564
2846.850911	191222.652493	55.565569
2845.762817	190982.951323	55.570573
2845.062316	190744.920314	55.575578
2844.498528	190495.010791	55.580583
2843.678858	190261.823113	55.585588
2843.217664	190010.792924	55.590593
2842.354947	189780.489801	55.595597
2841.837714	189538.796916	55.600602
2841.040586	189289.121431	55.605607
2840.277010	189064.200548	55.610612
2839.883132	188812.606159	55.615617
2839.509038	188570.717381	55.620621
2838.503361	188320.253024	55.625626
2837.831141	188082.905035	55.630631
2837.251888	187842.006663	55.635636
2836.657415	187598.351166	55.640641
2835.627335	187356.559773	55.645645
2835.226430	187107.456446	55.650650
2834.775460	186864.303658	55.655655
2833.804760	186635.228834	55.660660
2833.226373	186377.938997	55.665665
2832.761575	186143.786699	55.670669
2832.267057	185896.727497	55.675674
2831.641557	185651.636815	55.680679
2830.618326	185417.805642	55.685684
2830.258625	185154.801349	55.690689
2829.617691	184914.220563	55.695693
2828.643575	184673.388496	55.700698
2827.991132	184433.257336	55.705703
2827.308066	184195.447610	55.710708
2826.656537	183941.350722	55.715713
2825.542640	183700.749518	55.720717
2825.237220	183456.294227	55.725722
2824.734810	183216.845463	55.730727
2823.827573	182979.917277	55.735732
2823.220762	182733.669106	55.740737
2822.434119	182496.037460	55.745741
2821.833521	182256.762065	55.750746
2821.542176	182016.192342	55.755751
2820.744262	181777.396025	55.760756
2819.972308	181526.982866	55.765761
2819.114700	181291.747728	55.770765
2818.262162	181056.398568	55.775770
2818.094120	180815.421563	55.780775
2817.243323	180580.596238	55.785780
2817.065991	180339.216289	55.790785
2815.932159	180101.894307	55.795789
2815.119241	179853.150909	55.800794
2814.803816	179604.393757	55.805799
2813.740140	179376.045104	55.810804
2813.325539	179132.101874	55.815809
2812.640229	178892.807534	55.820813
2812.208663	178653.169072	55.825818
2811.576647	178406.809487	55.830823
2810.821796	178168.369744	55.835828
2810.516929	177923.792796	55.840833
2809.682035	177676.299386	55.845837
2808.644884	177435.542651	55.850842
2808.311965	177190.033163	55.855847
2807.198003	176955.485718	55.860852
2806.882799	176708.958697	55.865857
2806.216466	176466.164601	55.870861
2805.551480	176227.632624	55.875866
2805.183484	175975.471009	55.880871
2804.253888	175736.157032	55.885876
2803.695039	175479.131860	55.890881
2802.901715	175251.220707	55.895885
2802.209081	175005.501305	55.900890
2801.694572	174755.608870	55.905895
2800.947593	174522.352581	55.910900
2799.975058	174273.858377	55.915905
2799.009957	174036.149775	55.920909
2798.742119	173799.756592	55.925914
2798.365278	173557.264541	55.930919
2797.341965	173320.892067	55.935924
2797.226503	173072.740067	55.940929
2796.180469	172848.774180	55.945933
2795.693462	172588.741728	55.950938
2795.116278	172343.834154	55.955943
2794.188217	172103.587522	55.960948
2793.678417	171849.146640	55.965953
2792.672600	171609.627506	55.970957
2792.026218	171368.857434	55.975962
2791.361201	171122.330733	55.980967
2790.432708	170896.640365	55.985972
2790.267304	170653.038793	55.990977
2789.340351	170418.105388	55.995981
2788.604334	170175.932478	56.000986
2788.087677	169942.628336	56.005991
2787.424990	169705.202952	56.010996
2786.971632	169467.288049	56.016001
2785.942212	169230.890143	56.021005
2785.428482	168979.952946	56.026010
2785.001261	168748.409462	56.031015
2784.056574	168515.232578	56.036020
2783.634804	168270.402165	56.041025
2782.825904	168032.959355	56.046029
2781.809139	167786.891038	56.051034
2781.447332	167558.243729	56.056039
2780.865810	167325.703256	56.061044
2780.297926	167076.910722	56.066049
2779.850016	166850.938992	56.071053
2779.085408	166603.719377	56.076058
2778.401773	166365.389737	56.081063
2777.253932	166122.837159	56.086068
2777.073315	165870.863121	56.091073
2776.404323	165643.102578	56.096077
2775.281772	165411.994753	56.101082
2774.932318	165167.821454	56.106087
2774.296985	164937.554917	56.111092
2773.746409	164693.442017	56.116097
2772.571523	164454.172427	56.121101
2772.263311	164212.363926	56.126106
2771.828218	163992.841353	56.131111
2771.036179	163689.075679	56.136116
2770.593494	163435.112552	56.141121
2769.864510	163196.339963	56.146125
2768.930562	162953.392797	56.151130
2768.667227	162707.187774	56.156135
2767.742060	162477.389411	56.161140
2767.255627	162233.714997	56.166145
2766.407497	161990.442804	56.171149
2765.643569	161751.786943	56.176154
2765.081484	161500.640676	56.181159
2764.168770	161270.275863	56.186164
2763.923711	161020.951714	56.191169
2763.103747	160780.365908	56.196173
2762.320508	160531.982248	56.201178
2761.852977	160304.401051	56.206183
2761.060308	160070.948182	56.211188
2760.430707	159819.544695	56.216193
2759.670824	159596.858251	56.221197
2759.056361	159345.188742	56.226202
2758.418721	159107.242497	56.231207
2757.152889	158875.105663	56.236212
2756.682967	158636.080823	56.241217
2756.055796	158398.658953	56.246221
2755.318821	158167.116824	56.251226
2754.826472	157934.393306	56.256231
2753.851464	157704.137824	56.261236
2753.814542	157461.124122	56.266241
2753.114755	157228.018654	56.271245
2752.537530	156998.035368	56.276250
2751.591627	156753.924758	56.281255
2750.909497	156519.893240	56.286260
2750.344333	156284.243016	56.291265
2749.631342	156049.151739	56.296269
2748.961216	155824.644578	56.301274
2748.223687	155574.509145	56.306279
2747.641978	155350.105497	56.311284
2747.039762	155105.799609	56.316289
2746.335388	154882.232035	56.321293
2745.442917	154637.174637	56.326298
2745.274641	154403.139751	56.331303
2744.471690	154170.986645	56.336308
2743.775278	153922.166142	56.341313
2743.116107	153688.671575	56.346317
2742.391092	153456.142408	56.351322
2741.764441	153206.744127	56.356327
2740.944174	152979.470391	56.361332
2740.393862	152732.732891	56.366337
2739.578039	152511.956991	56.371341
2738.970296	152272.324729	56.376346
2738.433273	152027.496976	56.381351
2737.498552	151804.393102	56.386356
2737.031610	151571.073536	56.391361
2736.399897	151342.611725	56.396365
2735.982943	151105.931935	56.401370
2735.152755	150875.509256	56.406375
2734.482566	150638.656861	56.411380
2733.889821	150397.116557	56.416385
2733.211041	150156.303425	56.421389
2732.323063	149922.858878	56.426394
2731.858268	149680.032596	56.431399
2731.085441	149459.028839	56.436404
2730.540024	149216.917821	56.441409
2729.666236	148979.626740	56.446413
2728.819083	148746.667131	56.451418
2728.628231	148512.296159	56.456423
2727.725293	148282.068558	56.461428
2727.078751	148050.365839	56.466433
2726.289561	147806.384903	56.471437
2725.768259	147577.487188	56.476442
2724.806497	147344.555880	56.481447
2724.401295	147112.173544	56.486452
2723.954744	146877.003512	56.491457
2723.433677	146645.252954	56.496461
2722.273404	146404.175551	56.501466
2721.833289	146180.663448	56.506471
2720.925100	145950.300975	56.511476
2720.395929	145705.684922	56.516481
2720.143912	145474.675506	56.521485
2718.991905	145241.891427	56.526490
2718.508284	144997.489690	56.531495
2717.742212	144768.917880	56.536500
2716.906706	144532.301951	56.541505
2716.250865	144305.355376	56.546509
2715.736368	144074.410554	56.551514
2715.129433	143836.924975	56.556519
2714.105115	143617.755280	56.561524
2713.778899	143368.957261	56.566529
2712.874371	143147.624360	56.571533
2712.143078	142918.641275	56.576538
2711.742409	142685.769962	56.581543
2710.961467	142457.153963	56.586548
2710.547091	142216.117760	56.591553
2709.902022	142000.597165	56.596557
2709.525202	141766.839548	56.601562
2708.629796	141516.011923	56.606567
2707.853760	141291.952800	56.611572
2707.223588	141059.549497	56.616577
2706.762363	140823.461777	56.621581
2705.865267	140586.555506	56.626586
2705.053045	140356.956372	56.631591
2704.276149	140127.950566	56.636596
2703.833134	139895.119931	56.641601
2702.956497	139670.034122	56.646605
2702.173020	139432.775827	56.651610
2701.772447	139206.118783	56.656615
2700.975701	138986.463449	56.661620
2700.323939	138756.012518	56.666625
2699.760970	138531.952799	56.671629
2699.007887	138302.156683	56.676634
2698.504310	138061.726695	56.681639
2697.487262	137844.363470	56.686644
2697.176073	137620.080135	56.691649
2696.189012	137384.979372	56.696653
2695.411505	137162.031161	56.701658
2694.893043	136937.264932	56.706663
2694.097351	136707.284634	56.711668
2693.786946	136488.752220	56.716673
2692.905157	136265.306418	56.721677
2692.372777	136035.226128	56.726682
2691.564810	135805.000741	56.731687
2690.955477	135583.956167	56.736692
2690.396447	135357.785578	56.741697
2689.559557	135143.729477	56.746701
2688.722910	134911.699010	56.751706
2688.572578	134677.122544	56.756711
2687.850440	134456.549017	56.761716
2687.039216	134238.862275	56.766721
2686.555840	134008.180443	56.771725
2685.878886	133782.701368	56.776730
2685.405274	133550.446430	56.781735
2684.897970	133326.468428	56.786740
2683.913021	133085.825271	56.791745
2683.088616	132860.478401	56.796749
2682.596685	132629.580308	56.801754
2681.991283	132406.438004	56.806759
2680.965260	132186.552438	56.811764
2680.408134	131953.180424	56.816769
2679.945159	131721.205370	56.821773
2679.207024	131497.913368	56.826778
2678.197999	131274.958192	56.831783
2677.818829	131051.257167	56.836788
2677.520543	130820.114422	56.841793
2676.450432	130598.533364	56.846797
2675.428913	130373.161211	56.851802
2675.227340	130147.711755	56.856807
2674.169977	129931.379726	56.861812
2674.082852	129695.436942	56.866817
2673.035982	129478.319249	56.871821
2672.205562	129254.665882	56.876826
2671.914563	129025.721349	56.881831
2671.350237	128803.337656	56.886836
2670.563844	128567.718392	56.891841
2670.043729	128349.433735	56.896845
2669.155147	128124.630167	56.901850
2668.515601	127887.304202	56.906855
2667.798121	127675.609663	56.911860
2667.448671	127439.651334	56.916865
2666.494902	127212.388913	56.921869
2665.821934	126991.764211	56.926874
2665.174482	126768.965507	56.931879
2664.656203	126539.137713	56.936884
2664.247559	126308.608674	56.941889
2663.183630	126084.776617	56.946893
2662.463205	125870.683463	56.951898
2662.229858	125638.087639	56.956903
2661.174989	125411.249853	56.961908
2660.619784	125177.654892	56.966913
2659.925076	124963.615586	56.971917
2659.324042	124734.692344	56.976922
2658.710090	124511.513078	56.981927
2657.729544	124291.606584	56.986932
2657.226524	124059.473372	56.991937
2656.555778	123839.978629	56.996941
2655.881745	123624.841845	57.001946
2655.284452	123384.627620	57.006951
2654.642017	123175.711725	57.011956
2654.236341	122951.445702	57.016961
2653.257782	122717.901011	57.021965
2652.641781	122485.304066	57.026970
2652.370501	122269.352453	57.031975
2651.169851	122040.293196	57.036980
2650.888817	121815.229689	57.041985
2650.045841	121592.631601	57.046989
2649.259388	121366.153650	57.051994
2648.647529	121144.297258	57.056999
2647.825235	120927.491544	57.062004
2647.321692	120700.631630	57.067009
2646.701729	120481.638976	57.072013
2646.078608	120250.459442	57.077018
2645.429704	120018.105205	57.082023
2644.457509	119805.852593	57.087028
2643.999118	119572.862660	57.092033
2643.252257	119361.923794	57.097037
2642.495928	119144.589069	57.102042
2642.044947	118914.219314	57.107047
2641.204627	118687.703138	57.112052
2640.700122	118462.354557	57.117057
2640.097226	118241.460807	57.122061
2639.255111	118027.748340	57.127066
2638.830120	117795.124488	57.132071
2637.823009	117574.871781	57.137076
2637.273915	117347.940278	57.142081
2636.462442	117131.221488	57.147085
2635.791788	116916.196093	57.152090
2635.362085	116693.250502	57.157095
2634.453127	116478.380784	57.162100
2633.913773	116253.698090	57.167105
2633.269237	116038.739374	57.172109
2632.534167	115825.142469	57.177114
2632.400865	115591.381508	57.182119
2631.410458	115372.319306	57.187124
2630.624930	115144.022953	57.192129
2629.937024	114929.416854	57.197133
2629.110880	114715.519968	57.202138
2628.885352	114490.098536	57.207143
2628.284645	114265.366917	57.212148
2627.189401	114041.731179	57.217153
2626.292532	113826.881910	57.222157
2625.959897	113602.799173	57.227162
2625.395547	113386.510992	57.232167
2624.223033	113180.653621	57.237172
2624.035986	112950.390879	57.242177
2623.463809	112736.546676	57.247181
2622.579358	112524.937021	57.252186
2622.017907	112295.482176	57.257191
2621.552007	112080.953993	57.262196
2621.051532	111865.373272	57.267201
2620.049843	111645.329810	57.272205
2619.675988	111420.238651	57.277210
2619.107989	111184.385252	57.282215
2618.028808	110965.470688	57.287220
2617.291036	110746.700688	57.292225
2616.875430	110533.332887	57.297229
2616.141033	110309.463935	57.302234
2615.759079	110083.466016	57.307239
2614.813855	109860.300878	57.312244
2613.994981	109637.454072	57.317249
2613.162593	109420.005387	57.322253
2612.650933	109211.379205	57.327258
2612.079654	108984.958137	57.332263
2611.144775	108771.941718	57.337268
2610.640685	108556.263533	57.342273
2610.301697	108336.867973	57.347277
2609.543160	108120.098106	57.352282
2608.900868	107893.171730	57.357287
2608.005164	107674.904658	57.362292
2607.649572	107448.622299	57.367297
2606.794154	107234.712038	57.372301
2605.957220	107019.208087	57.377306
2605.571525	106799.573649	57.382311
2604.772584	106584.353084	57.387316
2604.324626	106356.598125	57.392321
2603.712729	106144.644916	57.397325
2602.627627	105917.959509	57.402330
2602.085118	105694.553032	57.407335
2600.878997	105479.641631	57.412340
2600.610463	105269.849718	57.417345
2599.866086	105062.533345	57.422349
2598.869983	104844.377603	57.427354
2598.556438	104633.646705	57.432359
2598.008048	104426.729878	57.437364
2596.823722	104217.834639	57.442369
2596.367031	104005.882115	57.447373
2595.833831	103796.081654	57.452378
2595.068568	103584.632238	57.457383
2594.348036	103376.444907	57.462388
2594.159072	103158.011772	57.467393
2593.456650	102951.309850	57.472397
2592.478378	102744.570980	57.477402
2592.022702	102517.913354	57.482407
2591.191670	102304.956902	57.487412
2590.729338	102085.879177	57.492417
2589.948236	101884.026796	57.497421
2589.297122	101676.940955	57.502426
2588.956068	101456.403500	57.507431
2587.934836	101244.419341	57.512436
2587.200218	101029.365778	57.517441
2586.629423	100821.919533	57.522445
2586.038898	100611.687118	57.527450
2585.806081	100396.249034	57.532455
2584.601588	100186.682325	57.537460
2584.053914	99964.339448	57.542465
2583.167468	99761.900470	57.547469
2582.923966	99550.093932	57.552474
2582.377965	99334.030270	57.557479
2581.286212	99127.170145	57.562484
2580.743508	98899.210382	57.567489
2580.235357	98693.695177	57.572493
2579.316505	98484.466513	57.577498
2578.964800	98268.813353	57.582503
2578.313332	98061.112853	57.587508
2577.828560	97836.535146	57.592513
2577.065049	97627.657549	57.597517
2576.091778	97411.679649	57.602522
2575.276283	97189.196688	57.607527
2574.352082	96982.481552	57.612532
2574.241204	96776.540018	57.617537
2573.697113	96570.852930	57.622541
2572.461285	96351.768169	57.627546
2572.287714	96139.639535	57.632551
2571.451442	95925.429849	57.637556
2570.788906	95715.716604	57.642561
2569.982701	95504.360100	57.647565
2569.489704	95300.477583	57.652570
2569.164344	95085.186491	57.657575
2568.188608	94880.591526	57.662580
2567.453903	94661.481760	57.667585
2566.581929	94450.519721	57.672589
2565.952953	94248.450313	57.677594
2565.615214	94033.710283	57.682599
2564.848394	93822.439418	57.687604
2564.594247	93607.994612	57.692609
2563.825817	93393.519222	57.697613
2563.244808	93180.385935	57.702618
2562.716927	92965.312143	57.707623
2561.416944	92753.755398	57.712628
2561.225609	92530.249249	57.717633
2560.521072	92317.035995	57.722637
2559.472688	92102.604717	57.727642
2559.076770	91888.706208	57.732647
2558.432000	91679.845917	57.737652
2557.518732	91462.438168	57.742657
2556.774708	91255.049694	57.747661
2556.117931	91043.667302	57.752666
2555.820171	90835.647705	57.757671
2554.926353	90631.535307	57.762676
2554.971216	90407.100094	57.767681
2553.825584	90193.057848	57.772685
2552.779110	89977.714848	57.777690
2552.443117	89769.204157	57.782695
2551.453179	89554.306531	57.787700
2551.040114	89345.076608	57.792705
2550.322022	89125.486304	57.797709
2549.555959	88917.635200	57.802714
2549.172524	88716.934185	57.807719
2548.197861	88500.300973	57.812724
2547.804732	88284.135671	57.817729
2547.032001	88071.335806	57.822733
2545.931950	87866.267529	57.827738
2545.760376	87658.125025	57.832743
2544.775074	87445.720025	57.837748
2544.301856	87238.453537	57.842753
2543.844431	87029.880563	57.847757
2542.767078	86820.628092	57.852762
2542.412189	86600.593707	57.857767
2541.368821	86402.700357	57.862772
2540.896510	86190.315167	57.867777
2540.343606	85985.691537	57.872781
2539.797104	85768.859371	57.877786
2539.171436	85556.371636	57.882791
2538.235574	85360.879763	57.887796
2537.881484	85144.689033	57.892801
2536.955337	84927.583254	57.897805
2536.384138	84724.324800	57.902810
2536.036805	84504.817856	57.907815
2534.992444	84309.149974	57.912820
2534.498578	84093.030096	57.917825
2533.844001	83887.327063	57.922829
2533.221090	83665.064413	57.927834
2532.321250	83453.395414	57.932839
2531.640815	83256.735107	57.937844
2531.325157	83036.382627	57.942849
2530.638356	82825.503810	57.947853
2529.927691	82619.378306	57.952858
2529.215672	82398.974877	57.957863
2528.365826	82199.562433	57.962868
2527.574833	81985.121113	57.967873
2526.824157	81781.849653	57.972877
2526.350739	81564.339021	57.977882
2525.718596	81361.160598	57.982887
2525.067777	81161.156062	57.987892
2524.305385	80942.366735	57.992897
2523.764848	80741.131871	57.997901
2523.063156	80533.415655	58.002906
2522.460869	80323.980922	58.007911
2521.557545	80122.752495	58.012916
2521.029107	79907.606414	58.017921
2520.509902	79708.000562	58.022925
2519.855507	79502.784104	58.027930
2519.326119	79278.411099	58.032935
2518.354363	79081.652426	58.037940
2517.644932	78874.410317	58.042945
2516.766144	78668.103344	58.047949
2516.266372	78456.047654	58.052954
2516.022353	78252.876129	58.057959
2514.860117	78048.895273	58.062964
2514.485302	77844.145264	58.067969
2513.933472	77637.486281	58.072973
2512.986851	77433.496369	58.077978
2512.340867	77230.683817	58.082983
2511.878993	77030.340727	58.087988
2511.165204	76815.319654	58.092993
2510.421708	76609.512504	58.097997
2509.778433	76407.018180	58.103002
2509.385471	76191.477586	58.108007
2508.143283	75984.995422	58.113012
2507.649823	75785.429916	58.118017
2507.167359	75574.858655	58.123021
2506.322879	75371.975660	58.128026
2505.513937	75166.136455	58.133031
2504.942650	74965.792997	58.138036
2504.464295	74756.553805	58.143041
2503.855238	74566.966034	58.148045
2503.047840	74358.815865	58.153050
2502.480534	74143.039561	58.158055
2501.740327	73941.763664	58.163060
2501.237817	73727.064944	58.168065
2500.474367	73527.729233	58.173069
2499.675384	73337.644612	58.178074
2499.441250	73123.967817	58.183079
2498.401547	72928.045962	58.188084
2498.040870	72714.539301	58.193089
2497.278930	72518.602763	58.198093
2496.543558	72306.287526	58.203098
2496.145182	72092.128294	58.208103
2495.308416	71888.366951	58.213108
2494.829342	71682.802540	58.218113
2494.226428	71470.804618	58.223117
2493.117217	71271.615895	58.228122
2492.395942	71057.455626	58.233127
2491.789359	70860.459198	58.238132
2491.279676	70646.029109	58.243137
2490.781165	70446.707519	58.248141
2489.853138	70238.087288	58.253146
2489.916146	70030.205314	58.258151
2488.673465	69826.054418	58.263156
2487.813617	69612.134457	58.268161
2487.262926	69408.999358	58.273165
2486.636839	69210.198214	58.278170
2486.225933	68999.387166	58.283175
2485.194449	68798.108144	58.288180
2484.567222	68593.517772	58.293185
2483.913433	68380.820007	58.298189
2483.138516	68187.113612	58.303194
2482.665954	67976.171326	58.308199
2481.949813	67775.695216	58.313204
2481.446711	67568.328053	58.318209
2480.684267	67365.171702	58.323213
2479.842033	67153.549545	58.328218
2479.218603	66960.211325	58.333223
2478.683249	66758.399664	58.338228
2477.922404	66552.851190	58.343233
2477.140568	66353.996131	58.348237
2476.583564	66149.838261	58.353242
2476.040690	65939.347186	58.358247
2475.611574	65739.242397	58.363252
2474.789051	65532.983056	58.368257
2474.337084	65322.924422	58.373261
2473.352212	65114.614928	58.378266
2473.024656	64907.593526	58.383271
2472.189673	64713.336044	58.388276
2471.493570	64503.958314	58.393281
2471.005276	64301.867212	58.398285
2469.964623	64093.973403	58.403290
2469.390679	63884.146124	58.408295
2468.615118	63686.552420	58.413300
2468.245302	63476.399626	58.418305
2467.633229	63274.750580	58.423309
2466.678584	63075.364733	58.428314
2466.320294	62856.551356	58.433319
2465.180898	62657.680406	58.438324
2464.836777	62451.315049	58.443329
2464.055903	62256.798498	58.448333
2463.334481	62050.073073	58.453338
2462.753180	61850.194481	58.458343
2462.131403	61643.204419	58.463348
2461.326289	61435.213629	58.468353
2460.585982	61241.432364	58.473357
2460.177129	61034.592484	58.478362
2459.926109	60836.008181	58.483367
2458.989870	60629.557088	58.488372
2458.209970	60420.443325	58.493377
2457.478548	60219.513626	58.498381
2456.821894	60017.697354	58.503386
2456.398887	59811.607549	58.508391
2455.268714	59615.869363	58.513396
2454.836898	59391.115416	58.518401
2454.135179	59192.306531	58.523405
2453.383682	58989.186874	58.528410
2452.983310	58787.124799	58.533415
2452.275471	58580.026963	58.538420
2451.505540	58379.743493	58.543425
2450.871305	58178.548056	58.548429
2450.382839	57986.292449	58.553434
2449.743169	57780.158084	58.558439
2448.825726	57564.824608	58.563444
2448.165285	57365.689971	58.568449
2447.448348	57157.985865	58.573453
2446.523907	56965.841584	58.578458
2446.254060	56756.919007	58.583463
2445.246888	56564.573619	58.588468
2444.693828	56355.336503	58.593473
2444.413741	56151.894586	58.598477
2443.531240	55959.652833	58.603482
2443.016678	55755.508711	58.608487
2441.902228	55562.519827	58.613492
2441.621624	55344.807245	58.618497
2440.939109	55151.564305	58.623501
2439.972178	54958.590020	58.628506
2439.561649	54755.681068	58.633511
2438.874463	54550.074477	58.638516
2438.095193	54350.276026	58.643521
2437.677425	54140.770493	58.648525
2436.918209	53942.618891	58.653530
2436.370480	53747.347252	58.658535
2435.621158	53544.261778	58.663540
2435.157480	53345.322989	58.668545
2434.345740	53142.656934	58.673549
2433.414155	52943.926456	58.678554
2433.025297	52733.337633	58.683559
2432.359126	52544.293427	58.688564
2431.717141	52344.976162	58.693569
2430.823776	52140.473644	58.698573
2430.184769	51933.518830	58.703578
2429.690755	51731.618696	58.708583
2428.786174	51539.113732	58.713588
2428.151394	51333.933852	58.718593
2427.529179	51144.248661	58.723597
2426.883155	50947.329971	58.728602
2426.423348	50737.566623	58.733607
2425.671401	50544.842415	58.738612
2424.944985	50333.531420	58.743617
2424.384789	50139.670622	58.748621
2423.512511	49933.440168	58.753626
2422.943030	49732.317910	58.758631
2422.170094	49538.791571	58.763636
2421.652607	49332.344104	58.768641
2421.280047	49142.960001	58.773645
2419.901178	48951.089470	58.778650
2419.565516	48742.842004	58.783655
2419.145468	48543.193169	58.788660
2418.161642	48345.350607	58.793665
2417.660014	48156.332778	58.798669
2416.811087	47954.977476	58.803674
2416.608227	47750.785633	58.808679
2415.557445	47556.508695	58.813684
2415.009070	47355.485820	58.818689
2414.451805	47156.013509	58.823693
2413.521464	46958.165273	58.828698
2412.937763	46757.331933	58.833703
2412.279660	46565.043926	58.838708
2411.536129	46364.740182	58.843713
2410.971708	46169.234144	58.848717
2410.395261	45971.869095	58.853722
2409.950501	45770.809858	58.858727
2408.910461	45576.043741	58.863732
2408.302745	45361.426512	58.868737
2407.546832	45173.021772	58.873741
2406.780167	44977.067624	58.878746
2406.536803	44782.193483	58.883751
2405.660504	44599.219426	58.888756
2404.998666	44396.341084	58.893761
2404.384359	44199.277136	58.898765
2403.584691	44009.427470	58.903770
2402.955042	43808.635119	58.908775
2402.105170	43618.927335	58.913780
2401.585080	43425.997164	58.918785
2400.790054	43236.047653	58.923789
2400.181793	43037.392419	58.928794
2399.882462	42825.676512	58.933799
2399.059736	42648.220462	58.938804
2398.383424	42448.507491	58.943809
2397.876018	42252.077970	58.948813
2397.332997	42050.621746	58.953818
2397.058352	41852.980260	58.958823
2395.859503	41657.397636	58.963828
2395.209043	41444.906764	58.968833
2394.831364	41247.120941	58.973837
2393.780952	41055.104467	58.978842
2393.569464	40851.528903	58.983847
2392.504383	40646.614363	58.988852
2391.843869	40446.877762	58.993857
2391.357615	40251.710372	58.998861
2390.711568	40057.677257	59.003866
2390.119272	39844.336843	59.008871
2389.178236	39651.711603	59.013876
2388.323430	39442.031971	59.018881
2387.836333	39255.071821	59.023885
2386.892569	39057.195454	59.028890
2386.506920	38866.516173	59.033895
2385.826461	38674.466119	59.038900
2385.096940	38473.925601	59.043905
2384.303476	38267.989449	59.048909
2383.759407	38089.567217	59.053914
2383.202604	37894.676633	59.058919
2382.317080	37705.882268	59.063924
2381.737469	37495.986919	59.068929
2381.362418	37298.067696	59.073933
2380.184535	37119.915815	59.078938
2379.665278	36928.405292	59.083943
2378.737464	36730.313210	59.088948
2378.444569	36537.196824	59.093953
2377.976690	36341.899014	59.098957
2376.970879	36159.098573	59.103962
2376.647926	35970.746496	59.108967
2375.660007	35774.660457	59.113972
2375.037835	35582.876454	59.118977
2374.446795	35378.438626	59.123981
2373.671397	35195.447731	59.128986
2373.173781	34996.925311	59.133991
2372.474075	34806.559675	59.138996
2371.821327	34613.444970	59.144001
2371.223673	34420.938569	59.149005
2370.103205	34224.973839	59.154010
2369.710619	34032.360366	59.159015
2368.808264	33846.017405	59.164020
2368.402566	33656.964768	59.169025
2367.964225	33471.571784	59.174029
2366.994382	33278.958975	59.179034
2366.451618	33085.522089	59.184039
2365.924839	32900.497167	59.189044
2365.075836	32703.009097	59.194049
2364.612264	32513.830060	59.199053
2363.699470	32332.074414	59.204058
2363.550723	32135.831626	59.209063
2362.643696	31937.194038	59.214068
2362.056440	31737.171235	59.219073
2361.502099	31551.277628	59.224077
2360.532143	31356.413202	59.229082
2360.010940	31168.633451	59.234087
2358.868562	30977.801889	59.239092
2358.344446	30781.271254	59.244097
2357.747253	30595.087078	59.249101
2356.960280	30403.464723	59.254106
2356.520895	30208.438082	59.259111
2355.680479	30033.184163	59.264116
2355.276946	29840.308279	59.269121
2354.826651	29646.140117	59.274125
2353.740296	29452.689751	59.279130
2353.489412	29263.803393	59.284135
2352.540230	29074.582812	59.289140
2351.951875	28878.195733	59.294145
2351.255581	28701.065676	59.299149
2350.658189	28507.716420	59.304154
2350.551848	28304.982696	59.309159
2349.500897	28110.651526	59.314164
2348.834175	27925.752090	59.319169
2348.041781	27722.368166	59.324173
2347.271853	27533.885884	59.329178
2346.765947	27333.695328	59.334183
2345.879957	27152.954895	59.339188
2345.309490	26959.005217	59.344193
2344.873838	26768.440882	59.349197
2344.039457	26577.276944	59.354202
2343.578598	26379.746579	59.359207
2342.339133	26198.261661	59.364212
2341.910419	26008.495028	59.369217
2341.488542	25822.174814	59.374221
2340.865424	25630.878777	59.379226
2340.048867	25436.594625	59.384231
2339.354056	25249.179075	59.389236
2339.008434	25053.350284	59.394241
2337.992389	24861.496226	59.399245
2337.030144	24685.369973	59.404250
2336.212753	24489.882701	59.409255
2335.745966	24308.289439	59.414260
2335.157023	24117.328996	59.419265
2334.776884	23935.557205	59.424269
2333.582575	23747.270961	59.429274
2333.181028	23551.527803	59.434279
2332.360613	23380.111235	59.439284
2331.859214	23191.398654	59.444289
2331.241526	23003.253218	59.449293
2330.299371	22827.510645	59.454298
2329.850419	22630.853663	59.459303
2329.191505	22460.028635	59.464308
2328.479768	22275.158584	59.469313
2327.931233	22088.896328	59.474317
2327.185258	21904.481382	59.479322
2326.816262	21707.129829	59.484327
2325.523509	21538.290617	59.489332
2325.046890	21347.835097	59.494337
2324.618466	21171.544540	59.499341
2323.621465	21001.212059	59.504346
2323.148925	20805.217844	59.509351
2322.296056	20622.246564	59.514356
2321.620674	20442.574144	59.519361
2320.969240	20264.880987	59.524365
2320.331713	20087.449758	59.529370
2319.623444	19900.549302	59.534375
2319.041739	19730.747353	59.539380
2318.476844	19553.670251	59.544385
2317.896456	19364.949432	59.549389
2317.009802	19194.344221	59.554394
2316.470652	19006.499102	59.559399
2315.733578	18833.176370	59.564404
2315.176954	18653.001854	59.569409
2314.577753	18468.352740	59.574413
2313.722556	18292.146307	59.579418
2313.289996	18111.534795	59.584423
2312.324242	17942.299416	59.589428
2311.701161	17762.499364	59.594433
2310.906951	17581.723186	59.599437
2309.993927	17408.508880	59.604442
2309.716106	17226.766818	59.609447
2308.841023	17059.423987	59.614452
2308.245827	16885.067034	59.619457
2307.614179	16714.520677	59.624461
2306.992614	16538.737871	59.629466
2306.338037	16359.670826	59.634471
2305.331128	16188.915057	59.639476
2304.604330	16011.423059	59.644481
2303.697888	15852.144836	59.649485
2303.033409	15690.618953	59.654490
2302.491945	15521.441688	59.659495
2301.853600	15359.211436	59.664500
2301.418079	15186.926513	59.669505
2300.490799	15021.004321	59.674509
2299.846360	14861.127837	59.679514
2299.318243	14693.699677	59.684519
2298.450659	14541.453904	59.689524
2297.606418	14365.135301	59.694529
2297.117569	14200.310058	59.699533
2295.943991	14052.064731	59.704538
2295.451924	13892.125004	59.709543
2294.826682	13739.576637	59.714548
2294.186216	13580.000204	59.719553
2293.517534	13431.199387	59.724557
2292.247722	13279.576244	59.729562
2291.893058	13112.136410	59.734567
2290.990766	12978.072339	59.739572
2290.454683	12829.051220	59.744577
2289.847086	12679.280153	59.749581
2289.001971	12528.211543	59.754586
2288.743533	12389.311048	59.759591
2287.917261	12239.802502	59.764596
2287.107233	12092.652790	59.769601
2286.405211	11947.404585	59.774605
2285.908159	11805.744612	59.779610
2284.913455	11659.400541	59.784615
2283.942260	11521.341865	59.789620
2283.382176	11379.894116	59.794625
2282.860812	11248.128978	59.799629
2281.794602	11116.740804	59.804634
2280.968031	10984.688034	59.809639
2279.952370	10853.856739	59.814644
2279.529713	10732.445829	59.819649
2278.701672	10609.540590	59.824653
2277.731733	10490.971292	59.829658
2277.228701	10367.207872	59.834663
2276.499370	10252.766928	59.839668
2275.320112	10133.491922	59.844673
2275.033517	10032.919350	59.849677
2274.036833	9917.923674	59.854682
2273.337464	9810.154199	59.859687
2272.441601	9704.805233	59.864692
2271.636377	9591.916376	59.869697
2270.834010	9494.767926	59.874701
2270.020580	9408.121193	59.879706
2269.627169	9300.133641	59.884711
2268.655370	9211.446365	59.889716
2267.912847	9108.293738	59.894721
2267.254379	9018.227263	59.899725
2266.518968	8934.403742	59.904730
2265.783766	8838.358577	59.909735
2265.196693	8759.251111	59.914740
2264.496230	8668.887266	59.919745
2263.969584	8579.735463	59.924750
2263.230706	8493.045090	59.929754
2262.769554	8403.720627	59.934759
2261.929398	8330.689104	59.939764
2261.534628	8241.728643	59.944769
2260.677472	8159.358330	59.949774
2259.848120	8076.244823	59.954778
2259.426086	7990.362304	59.959783
2258.699357	7905.991285	59.964788
2258.108593	7823.124562	59.969793
2257.340405	7735.130051	59.974798
2256.779623	7659.505718	59.979802
2256.023756	7567.900941	59.984807
2254.912832	7500.844696	59.989812
2254.508599	7419.988366	59.994817
2253.916782	7333.104265	59.999822
2253.007150	7261.989829	60.004826
2252.380619	7188.846761	60.009831
2251.560798	7133.374268	60.014836
2250.865093	7053.467855	60.019841
2250.304266	6992.373441	60.024846
2248.975529	6922.544350	60.029850
2248.738581	6854.671572	60.034855
2247.456214	6801.114133	60.039860
2247.099590	6738.427190	60.044865
2246.174322	6683.552917	60.049870
2245.298063	6631.533067	60.054874
2244.883922	6572.631443	60.059879
2244.182793	6530.458327	60.064884
2243.828074	6466.153491	60.069889
2242.963853	6415.349294	60.074894
2242.068781	6358.643662	60.079898
2241.503261	6301.580686	60.084903
2240.471524	6255.135557	60.089908
2240.073262	6199.150822	60.094913
2239.354032	6159.996575	60.099918
2238.945095	6102.641319	60.104922
2238.397846	6049.257117	60.109927
2237.561128	6008.858987	60.114932
2236.953251	5952.696236	60.119937
2236.632717	5901.814256	60.124942
2235.830747	5847.019751	60.129946
2235.392419	5792.843781	60.134951
2234.976156	5738.460994	60.139956
2234.192720	5681.298503	60.144961
2233.672312	5612.973874	60.149966
2232.595014	5564.196164	60.154970
2232.416555	5496.756506	60.159975
2231.360122	5448.346605	60.164980
2230.667898	5395.294596	60.169985
2230.031467	5350.476832	60.174990
2229.034899	5296.631812	60.179994
2228.553962	5252.521678	60.184999
2227.936137	5195.196753	60.190004
2227.303195	5148.246168	60.195009
2226.505041	5089.007486	60.200014
2226.109439	5049.742522	60.205018
2225.348680	4987.757305	60.210023
2224.545640	4949.102287	60.215028
2223.742019	4886.263743	60.220033
2223.552010	4838.851856	60.225038
2222.487753	4798.639050	60.230042
2221.831361	4737.118686	60.235047
2221.011447	4705.885295	60.240052
2220.728709	4648.562966	60.245057
2220.048590	4606.710652	60.250062
2219.188526	4544.197231	60.255066
2218.746554	4495.629089	60.260071
2218.279925	4452.457683	60.265076
2217.848964	4404.758870	60.270081
2217.398780	4344.825142	60.275086
2216.651722	4297.878800	60.280090
2216.135186	4226.927931	60.285095
2215.384785	4172.522662	60.290100
2214.747835	4117.320332	60.295105
2214.045115	4059.622069	60.300110
2213.280500	4012.983079	60.305114
2212.829046	3937.449468	60.310119
2211.948268	3890.097364	60.315124
2211.153175	3838.893934	60.320129
2210.676895	3778.425588	60.325134
2209.818983	3731.544382	60.330138
2209.178511	3674.199772	60.335143
2208.172767	3631.981505	60.340148
2207.568852	3574.405125	60.345153
2207.180276	3518.941644	60.350158
2206.387564	3472.319868	60.355162
2206.071236	3419.568662	60.360167
2205.286042	3371.592617	60.365172
2204.581756	3316.967883	60.370177
2203.786671	3268.324150	60.375182
2202.677287	3219.013529	60.380186
2202.659205	3176.859926	60.385191
2201.670473	3128.364892	60.390196
2201.076232	3074.349811	60.395201
2200.395254	3013.895787	60.400206
2199.533508	2981.694748	60.405210
2199.311033	2929.641790	60.410215
2198.360981	2890.254445	60.415220
2197.752428	2839.774134	60.420225
2197.563931	2788.881136	60.425230
2196.811404	2725.322085	60.430234
2196.538700	2679.199993	60.435239
2195.507037	2626.263067	60.440244
2194.980048	2570.026222	60.445249
2194.178625	2521.673039	60.450254
2193.071193	2472.654844	60.455258
2192.633583	2415.730123	60.460263
2191.761707	2374.513954	60.465268
2191.166390	2329.089250	60.470273
2190.324310	2284.096574	60.475278
2189.733764	2234.586297	60.480282
2189.095459	2186.634992	60.485287
2188.555431	2137.660391	60.490292
2187.801620	2094.921586	60.495297
2187.341888	2045.852538	60.500302
2186.705405	2007.690654	60.505306
2186.450016	1955.416886	60.510311
2185.811253	1909.437307	60.515316
2184.672845	1854.822232	60.520321
2183.862928	1802.513176	60.525326
2183.435804	1750.425895	60.530330
2182.832872	1710.328179	60.535335
2182.194161	1674.321188	60.540340
2181.326874	1613.721125	60.545345
2180.706167	1557.964367	60.550350
2179.798015	1525.461624	60.555354
2179.877559	1472.616761	60.560359
2178.960401	1424.946407	60.565364
2177.874325	1365.060273	60.570369
2177.083345	1329.230490	60.575374
2176.885143	1286.200874	60.580378
2176.232461	1244.462627	60.585383
2175.563997	1194.062166	60.590388
2174.672801	1141.558617	60.595393
2173.904088	1104.598988	60.600398
2172.924636	1056.769394	60.605402
2172.461018	1008.653880	60.610407
2171.749669	975.643274	60.615412
2171.225359	938.045199	60.620417
2170.434167	895.703024	60.625422
2169.785729	858.233670	60.630426
2169.204594	810.262836	60.635431
2168.583028	771.555358	60.640436
2168.111036	726.754012	60.645441
2167.695943	689.094305	60.650446
2166.736270	659.603668	60.655450
2166.382689	604.554927	60.660455
2165.511245	566.695105	60.665460
2164.503602	525.333811	60.670465
2163.917545	485.482815	60.675470
2162.964763	446.216853	60.680474
2162.565034	391.565774	60.685479
2161.672509	366.263212	60.690484
2161.243288	332.498844	60.695489
2160.490110	284.016904	60.700494
2159.661476	255.274323	60.705498
2159.362351	214.220997	60.710503
2158.337013	179.064420	60.715508
2157.800693	145.333250	60.720513
2157.038928	109.892159	60.725518
2156.242855	72.564170	60.730522
2155.714174	32.282673	60.735527
2154.658544	4.850839	60.740532
2153.895661	-29.496860	60.745537
2153.194467	-45.800655	60.750542
2152.266463	-66.118204	60.755546
2151.372013	-99.053940	60.760551
2150.729347	-110.680087	60.765556
2149.672192	-125.722481	60.770561
2149.122007	-139.022285	60.775566
2147.861352	-135.117819	60.780570
2147.271250	-139.291488	60.785575
2146.263048	-110.702833	60.790580
2144.998116	-104.665571	60.795585
2143.304180	-66.231596	60.800590
2141.611249	-24.282519	60.805594
2141.810427	0.290523	60.810599
2141.847642	10.935853	60.815604
2142.324909	21.941894	60.820609
2142.136803	13.809164	60.825614
2141.796486	7.039476	60.830618
2141.564608	-2.420456	60.835623
2140.951054	-2.969613	60.840628
2140.237946	-4.884440	60.845633
2139.007017	-1.432526	60.850638
2137.206355	27.808863	60.855642
2136.234545	24.534689	60.860647
2135.919009	35.986668	60.865652
2135.635496	31.489905	60.870657
2135.772173	28.607572	60.875662
2135.143714	30.634474	60.880666
2134.382700	32.447433	60.885671
2132.947116	35.384606	60.890676
2132.772827	45.169349	60.895681
2132.375147	51.438093	60.900686
2131.592828	49.851225	60.905690
2130.976268	48.908288	60.910695
2129.794956	52.461160	60.915700
2129.594029	47.493952	60.920705
2129.403957	49.880247	60.925710
2128.771334	57.004747	60.930714
2128.352065	42.136953	60.935719
2126.905567	50.426693	60.940724
2126.493652	55.112792	60.945729
2125.758401	45.516653	60.950734
2124.876677	66.826563	60.955738
2124.482209	53.229059	60.960743
2123.591988	60.493788	60.965748
2122.794218	63.597859	60.970753
2122.204010	59.736406	60.975758
2121.999587	58.202927	60.980762
2121.827882	60.333986	60.985767
2121.071828	62.876326	60.990772
2119.645157	61.899505	60.995777
2119.177797	69.207532	61.000782
2118.549386	68.137163	61.005786
2118.238253	64.206194	61.010791
2117.393771	64.854371	61.015796
2116.411396	79.039516	61.020801
2115.943525	72.105531	61.025806
2114.985389	74.629477	61.030810
2114.581237	66.351223	61.035815
2113.696977	70.937230	61.040820
2112.921777	61.844186	61.045825
2112.867396	65.339677	61.050830
2112.400060	70.137083	61.055834
2111.843901	58.588554	61.060839
2110.367046	68.028046	61.065844
2110.141691	61.285831	61.070849
2109.711710	65.859679	61.075854
2109.077860	74.971434	61.080858
2108.131699	61.299036	61.085863
2106.911898	67.709284	61.090868
2106.603145	69.601883	61.095873
2106.156306	60.907766	61.100878
2105.513871	71.151606	61.105882
2104.868426	60.911981	61.110887
2104.165928	66.355434	61.115892
2103.609212	71.979190	61.120897
2102.994865	61.600585	61.125902
2102.219362	75.596777	61.130906
2101.648877	58.885775	61.135911
2100.757680	69.090237	61.140916
2100.198125	61.500576	61.145921
2099.896205	62.456917	61.150926
2098.744861	71.701254	61.155930
2098.410825	68.720136	61.160935
2097.796591	69.475291	61.165940
2097.057498	65.292101	61.170945
2096.718347	68.813857	61.175950
2095.648573	67.846649	61.180954
2095.309964	63.038489	61.185959
2094.521822	73.076785	61.190964
2093.461510	66.564842	61.195969
2093.101774	70.605553	61.200974
2092.372717	70.662961	61.205978
2091.686439	76.042342	61.210983
2091.222339	61.009759	61.215988
2089.886273	77.230197	61.220993
2089.916713	69.939588	61.225998
2089.333793	69.639478	61.231002
2088.507538	71.098515	61.236007
2087.257376	78.672704	61.241012
2087.344513	77.523487	61.246017
2086.706065	69.324998	61.251022
2085.354170	76.404376	61.256026
2085.272536	66.731325	61.261031
2084.472690	67.659446	61.266036
2083.726817	69.468443	61.271041
2083.275639	67.455284	61.276046
2081.938027	79.238233	61.281050
2082.224354	64.302616	61.286055
2081.182091	65.641385	61.291060
2080.456803	63.835736	61.296065
2079.827371	64.564920	61.301070
2079.068616	67.142395	61.306074
2078.687350	67.543603	61.311079
2077.788049	68.320344	61.316084
2077.396247	67.158818	61.321089
2076.877856	68.088011	61.326094
2076.081897	71.961395	61.331098
2075.608887	61.740150	61.336103
2075.139872	59.868602	61.341108
2074.332912	72.284881	61.346113
2073.556137	61.512575	61.351118
2072.127391	65.631464	61.356122
2071.584669	60.253279	61.361127
2071.784469	68.075205	61.366132
2070.775713	69.471742	61.371137
2070.185032	58.505896	61.376142
2068.923869	68.582989	61.381146
2068.279439	65.815144	61.386151
2067.642819	66.244261	61.391156
2067.732766	65.827912	61.396161
2066.822963	67.593540	61.401166
2065.887465	71.361333	61.406170
2065.448803	73.632537	61.411175
2064.848184	71.496434	61.416180
2063.847375	74.695825	61.421185
2063.580047	65.924341	61.426190
2062.986907	75.632064	61.431194
2062.632369	65.022996	61.436199
2062.064515	77.743549	61.441204
2061.227207	74.271422	61.446209
2059.976087	64.864401	61.451214
2059.048955	68.544131	61.456218
2058.594532	72.189846	61.461223
2058.013908	72.353024	61.466228
2057.355318	66.698326	61.471233
2056.827135	69.423726	61.476238
2056.206752	76.628310	61.481242
2055.906104	77.043536	61.486247
2055.206758	69.301019	61.491252
2054.755251	76.057737	61.496257
2053.927300	64.730560	61.501262
2052.464199	72.988287	61.506266
2051.813188	57.766179	61.511271
2051.647755	65.540403	61.516276
2050.782659	62.944785	61.521281
2050.133661	67.220648	61.526286
2049.205951	68.112299	61.531290
2048.760625	64.905991	61.536295
2048.233076	77.359940	61.541300
2047.583872	68.817803	61.546305
2047.349197	77.598124	61.551310
2046.526708	76.839282	61.556314
2045.832215	59.931930	61.561319
2045.488887	71.213298	61.566324
2044.706302	66.347869	61.571329
2043.933782	70.025144	61.576334
2042.504619	83.975276	61.581338
2042.321822	64.241114	61.586343
2041.671742	75.845570	61.591348
2040.871725	76.765847	61.596353
2040.536238	71.802651	61.601358
2039.937240	76.128932	61.606362
2039.444825	69.823364	61.611367
2038.713237	77.249035	61.616372
2038.046338	71.169864	61.621377
2036.820893	67.606377	61.626382
2035.719214	73.703005	61.631386
2035.336367	70.409508	61.636391
2035.723636	69.524906	61.641396
2034.815905	80.343899	61.646401
2034.225529	74.771423	61.651406
2033.061406	77.239775	61.656410
2032.746322	76.441410	61.661415
2032.185719	76.470523	61.666420
2030.648125	70.862294	61.671425
2030.184393	66.837282	61.676430
2029.057673	79.028345	61.681434
2029.469665	71.328661	61.686439
2028.742150	75.788887	61.691444
2027.910670	78.169752	61.696449
2027.323189	68.879780	61.701454
2026.578297	81.532239	61.706458
2026.453838	71.706711	61.711463
2025.793625	70.603563	61.716468
2024.536474	72.047425	61.721473
2023.653945	79.208462	61.726478
2022.991814	82.909229	61.731482
2022.488424	72.039926	61.736487
2021.841363	73.568318	61.741492
2021.273627	81.338589	61.746497
2020.974258	69.285682	61.751502
2020.025335	73.181782	61.756506
2019.661137	64.226977	61.761511
2018.790412	74.202698	61.766516
2017.699809	75.613822	61.771521
2017.296534	68.921935	61.776526
2016.464517	80.976339	61.781530
2016.278055	72.482197	61.786535
2015.578526	74.690729	61.791540
2015.146457	75.336562	61.796545
2014.316320	72.670749	61.801550
2012.906744	79.281477	61.806554
2012.371856	69.251424	61.811559
2011.676185	75.031297	61.816564
2011.107260	79.031099	61.821569
2010.581609	66.280797	61.826574
2010.073853	61.466383	61.831578
2009.934011	69.337475	61.836583
2009.374727	64.996460	61.841588
2008.511354	68.304948	61.846593
2007.647118	71.050578	61.851598
2006.754475	78.670560	61.856602
2005.903700	69.797715	61.861607
2005.299281	71.286225	61.866612
2005.067415	78.413381	61.871617
2004.824940	65.318502	61.876622
2003.577389	67.508358	61.881626
2002.800457	67.560774	61.886631
2001.758415	74.423842	61.891636
2001.308414	77.269315	61.896641
2001.021622	59.365253	61.901646
2000.098716	81.609021	61.906650
1999.709579	67.963383	61.911655
1999.360663	70.349667	61.916660
1998.108295	73.024435	61.921665
1997.308635	80.022509	61.926670
1996.460499	78.499744	61.931674
1996.234717	66.416242	61.936679
1995.418825	72.992670	61.941684
1995.116072	71.156251	61.946689
1994.813897	65.940185	61.951694
1994.055920	68.005027	61.956698
1992.824681	70.648058	61.961703
1991.942084	72.570248	61.966708
1991.430416	71.904021	61.971713
1991.048396	66.908796	61.976718
1990.162110	65.049878	61.981722
1990.035819	71.188829	61.986727
1989.687877	74.636295	61.991732
1988.270615	71.976947	61.996737
1987.644022	66.498549	62.001742
1986.325188	79.302039	62.006746
1986.207672	66.518503	62.011751
1985.494004	75.977273	62.016756
1984.903167	66.399254	62.021761
1984.746004	68.638403	62.026766
1984.315008	76.554136	62.031770
1983.429924	64.176302	62.036775
1982.460018	70.198412	62.041780
1981.484713	68.142306	62.046785
1981.350864	57.588124	62.051790
1980.463523	74.935903	62.056794
1980.169573	69.193385	62.061799
1979.264317	64.265447	62.066804
1978.258168	78.317194	62.071809
1977.780607	66.715225	62.076814
1977.228770	63.792354	62.081818
1976.772698	73.446789	62.086823
1975.643527	68.697901	62.091828
1974.261970	77.215547	62.096833
1974.813540	70.532961	62.101838
1973.608409	82.041023	62.106842
1972.927482	71.389160	62.111847
1972.455849	68.352629	62.116852
1971.878228	80.125376	62.121857
1971.362554	61.860241	62.126862
1970.998358	71.859652	62.131866
1970.032171	66.115029	62.136871
1968.731162	64.034931	62.141876
1968.226740	64.402084	62.146881
1967.952305	69.794964	62.151886
1967.539215	65.672037	62.156890
1966.955848	59.902923	62.161895
1966.466781	64.541362	62.166900
1964.916608	65.900871	62.171905
1964.334796	75.936405	62.176910
1963.804805	68.769460	62.181914
1963.160952	70.833542	62.186919
1962.931809	68.304170	62.191924
1962.290981	68.293991	62.196929
1961.529457	70.982328	62.201934
1960.348432	74.282905	62.206938
1959.641377	67.655023	62.211943
1959.219497	69.377929	62.216948
1958.665687	67.048335	62.221953
1958.485004	65.552104	62.226958
1957.601954	73.478092	62.231962
1956.406446	67.490744	62.236967
1955.745995	66.602128	62.241972
1954.932402	63.779163	62.246977
1954.834807	68.399619	62.251982
1954.109879	72.626051	62.256986
1953.795538	67.831410	62.261991
1953.067654	69.664396	62.266996
1952.046105	74.163428	62.272001
1951.477779	66.969456	62.277006
1950.341719	71.702718	62.282010
1950.193506	70.445772	62.287015
1949.557512	68.200191	62.292020
1949.072725	68.318216	62.297025
1947.815860	60.317299	62.302030
1947.151736	56.294155	62.307034
1946.942389	60.716297	62.312039
1946.390810	60.707724	62.317044
1945.407490	68.657515	62.322049
1945.250407	60.204462	62.327054
1944.022690	73.146468	62.332058
1943.185925	67.999503	62.337063
1942.516959	55.707241	62.342068
1942.079562	67.878785	62.347073
1942.190131	58.619968	62.352078
1941.356645	71.040479	62.357082
1940.009647	62.088738	62.362087
1939.536636	68.807874	62.367092
1938.651724	61.586891	62.372097
1938.275414	61.287135	62.377102
1937.577674	68.229611	62.382106
1937.207258	62.131797	62.387111
1935.954212	66.013119	62.392116
1934.866335	71.109337	62.397121
1934.793123	61.323006	62.402126
1934.060901	65.492249	62.407130
1933.925701	58.929724	62.412135
1933.341339	67.383911	62.417140
1932.705864	58.834909	62.422145
1931.665598	56.880603	62.427150
1930.713744	71.721706	62.432154
1930.756968	63.785658	62.437159
1930.178177	61.314951	62.442164
1928.771828	66.136861	62.447169
1928.284096	62.065218	62.452174
1927.365775	60.533120	62.457178
1926.775248	63.356752	62.462183
1926.528034	69.529091	62.467188
1925.706142	72.022008	62.472193
1925.122027	57.008539	62.477198
1923.970716	62.017053	62.482202
1923.450698	56.851356	62.487207
1922.702795	65.476591	62.492212
1921.897588	67.113693	62.497217
1921.862661	67.505674	62.502222
1921.368354	69.052417	62.507226
1920.942803	63.996306	62.512231
1919.864415	68.017072	62.517236
1918.846597	66.589085	62.522241
1918.864000	59.619121	62.527246
1917.851480	73.939982	62.532250
1917.286496	59.382389	62.537255
1916.222451	64.228813	62.542260
1915.447732	72.888274	62.547265
1915.067921	63.598491	62.552270
1914.485262	64.582073	62.557274
1914.099691	57.143051	62.562279
1913.369577	60.777354	62.567284
1912.361140	67.092619	62.572289
1912.066092	56.344836	62.577294
1911.238750	62.215016	62.582298
1910.797140	57.770188	62.587303
1909.624827	63.501162	62.592308
1908.482409	65.226496	62.597313
1908.091736	54.285730	62.602318
1907.221429	58.372816	62.607322
1907.244912	59.700158	62.612327
1906.921570	57.441226	62.617332
1906.316478	54.940007	62.622337
1905.906085	46.995557	62.627342
1904.595496	57.172016	62.632346
1904.096573	58.296854	62.637351
1903.471229	57.104621	62.642356
1902.842613	49.619033	62.647361
1901.720298	48.482045	62.652366
1900.731420	54.051428	62.657370
1900.190945	53.741469	62.662375
1899.846723	53.125952	62.667380
1899.255664	55.672117	62.672385
1899.107254	52.290965	62.677390
1898.275503	59.950185	62.682394
1897.400965	58.027932	62.687399
1896.643746	52.828936	62.692404
1896.033020	57.677515	62.697409
1895.688753	60.272814	62.702414
1894.406289	58.614029	62.707418
1893.404065	50.085423	62.712423
1892.799200	51.703341	62.717428
1892.262077	51.361311	62.722433
1891.918890	50.457037	62.727438
1891.466325	61.449799	62.732442
1890.887997	59.139885	62.737447
1890.717795	60.024871	62.742452
1889.315832	60.652812	62.747457
1888.660622	51.033014	62.752462
1887.819240	50.862298	62.757466
1887.850310	58.822945	62.762471
1887.443719	52.076426	62.767476
1885.951768	52.783314	62.772481
1885.732838	50.596122	62.777486
1884.892621	64.944822	62.782490
1884.290094	58.070130	62.787495
1883.360911	57.784040	62.792500
1882.609359	56.615004	62.797505
1881.933971	49.477484	62.802510
1881.216733	68.234926	62.807514
1881.098862	53.000791	62.812519
1880.384731	58.304202	62.817524
1879.112387	58.399038	62.822529
1878.613723	46.757888	62.827534
1877.478243	64.600824	62.832538
1877.216726	58.805869	62.837543
1876.912161	60.712018	62.842548
1876.388761	65.928377	62.847553
1875.912037	56.072075	62.852558
1874.949277	71.728662	62.857562
1874.235684	58.754353	62.862567
1873.748105	56.603507	62.867572
1873.006001	54.950407	62.872577
1872.310801	52.887722	62.877582
1871.365442	56.594057	62.882586
1870.657463	55.774513	62.887591
1870.326310	52.969602	62.892596
1869.538441	62.537939	62.897601
1869.345140	55.319148	62.902606
1868.083728	59.627620	62.907610
1867.357728	52.375133	62.912615
1866.821559	51.980915	62.917620
1866.196538	60.547222	62.922625
1866.260037	45.623360	62.927630
1865.085658	58.151618	62.932634
1864.162947	53.871500	62.937639
1863.532970	46.830860	62.942644
1862.905583	42.122219	62.947649
1862.589038	56.599088	62.952654
1861.404087	59.556537	62.957658
1860.895208	55.358954	62.962663
1860.076409	47.473051	62.967668
1859.524532	55.914197	62.972673
1859.388484	49.495330	62.977678
1859.002588	57.153156	62.982682
1857.700037	55.784596	62.987687
1856.977078	57.132679	62.992692
1856.268770	60.667335	62.997697
1855.840242	54.785357	63.002702
1855.255861	63.111815	63.007706
1854.330314	50.095479	63.012711
1853.564280	52.341415	63.017716
1852.847806	56.397783	63.022721
1852.537281	47.406120	63.027726
1851.959298	54.810581	63.032730
1851.230382	50.848220	63.037735
1850.200776	56.129184	63.042740
1849.333653	54.038607	63.047745
1849.348092	58.426796	63.052750
1848.591688	60.499311	63.057754
1848.116478	54.741446	63.062759
1847.082176	44.041676	63.067764
1846.144129	57.544858	63.072769
1845.485009	52.271954	63.077774
1845.061163	54.346861	63.082778
1844.969687	54.804593	63.087783
1844.184783	50.709193	63.092788
1842.772894	58.302838	63.097793
1842.222641	49.380781	63.102798
1841.471753	57.530242	63.107802
1841.758085	56.276849	63.112807
1841.189420	59.630057	63.117812
1839.585109	56.268761	63.122817
1839.104978	56.135321	63.127822
1838.556029	58.386219	63.132826
1838.488757	59.682235	63.137831
1837.149717	60.748086	63.142836
1836.181121	54.374678	63.147841
1835.876948	48.316837	63.152846
1834.848164	63.767856	63.157850
1834.722886	57.317314	63.162855
1834.178630	54.981503	63.167860
1832.952398	60.205383	63.172865
1832.598248	56.746514	63.177870
1831.743289	66.387016	63.182874
1831.285438	58.164674	63.187879
1830.933055	54.535207	63.192884
1830.286457	63.521279	63.197889
1829.489507	50.921368	63.202894
1828.498444	54.915682	63.207898
1827.846199	52.472436	63.212903
1827.472873	51.210243	63.217908
1826.654013	61.204571	63.222913
1825.660126	55.756162	63.227918
1824.823088	56.431634	63.232922
1824.381310	45.139452	63.237927
1824.159510	53.067700	63.242932
1823.404043	53.294964	63.247937
1823.623677	54.916021	63.252942
1822.235478	56.918547	63.257946
1821.336106	69.567169	63.262951
1820.701468	67.370295	63.267956
1820.150628	53.840292	63.272961
1819.403729	52.366173	63.277966
1818.138286	61.562480	63.282970
1817.902705	54.135937	63.287975
1817.468299	56.081632	63.292980
1817.146948	59.860793	63.297985
1816.852078	54.768187	63.302990
1815.435616	68.440397	63.307994
1814.772159	57.449925	63.312999
1814.496173	60.001272	63.318004
1813.046431	60.384518	63.323009
1812.606884	60.143710	63.328014
1811.638864	70.645877	63.333018
1811.301999	54.826762	63.338023
1811.046215	55.528215	63.343028
1810.274047	56.789503	63.348033
1810.061679	52.333529	63.353038
1808.915505	58.432565	63.358042
1807.987829	57.841898	63.363047
1807.746581	57.776190	63.368052
1806.899386	54.622709	63.373057
1805.954152	47.532797	63.378062
1805.106617	51.786613	63.383066
1804.742729	50.686934	63.388071
1804.103149	54.838339	63.393076
1803.402376	57.345173	63.398081
1803.794321	55.945691	63.403086
1802.807876	51.333506	63.408090
1801.755823	56.146524	63.413095
1801.186571	56.874100	63.418100
1800.127041	62.410581	63.423105
1799.489839	57.366030	63.428110
1798.594267	59.468543	63.433114
1798.288684	58.165633	63.438119
1798.129085	62.523107	63.443124
1797.070244	65.173541	63.448129
1796.488112	62.947835	63.453134
1795.652816	64.362661	63.458138
1795.045855	65.395860	63.463143
1794.440268	69.351055	63.468148
1793.228094	73.776329	63.473153
1792.646289	56.706115	63.478158
1791.979126	72.112342	63.483162
1791.696044	64.858928	63.488167
1791.151639	56.120464	63.493172
1790.569995	57.565976	63.498177
1790.148581	46.824102	63.503182
1788.534114	60.330632	63.508186
1787.992850	54.349873	63.513191
1787.456733	48.696319	63.518196
1787.207730	57.933081	63.523201
1786.962385	58.503563	63.528206
1785.614252	59.067815	63.533210
1785.130467	49.121199	63.538215
1784.530672	53.734663	63.543220
1783.967065	59.760120	63.548225
1783.217805	58.396777	63.553230
1782.357587	67.069839	63.558234
1781.926748	59.398329	63.563239
1781.353317	60.328432	63.568244
1780.424623	65.296918	63.573249
1779.634548	53.944932	63.578254
1778.654495	63.641582	63.583258
1778.428470	51.206504	63.588263
1777.846739	55.985842	63.593268
1777.514579	60.653005	63.598273
1776.837937	58.656788	63.603278
1775.563552	56.968394	63.608282
1775.229318	61.661120	63.613287
1774.669428	62.108084	63.618292
1774.221058	62.289746	63.623297
1772.986241	60.041537	63.628302
1772.066213	61.332625	63.633306
1771.857395	59.706833	63.638311
1771.359125	54.282246	63.643316
1770.660363	52.106611	63.648321
1769.637640	58.443110	63.653326
1768.693249	59.816919	63.658330
1768.288728	54.817431	63.663335
1767.768070	48.970608	63.668340
1767.312488	55.112955	63.673345
1767.180094	43.916743	63.678350
1766.151072	59.208532	63.683354
1765.224202	54.063332	63.688359
1764.776837	49.641531	63.693364
1764.105381	55.499605	63.698369
1763.144277	47.888663	63.703374
1762.151683	53.012385	63.708378
1761.640411	54.844134	63.713383
1761.015842	57.780440	63.718388
1760.320418	60.619186	63.723393
1760.607314	46.401058	63.728398
1759.904275	57.031463	63.733402
1758.756926	53.638652	63.738407
1758.223253	53.818094	63.743412
1757.291112	63.608069	63.748417
1756.487085	52.972698	63.753422
1755.665771	59.789745	63.758426
1755.169243	61.182321	63.763431
1754.854925	55.761640	63.768436
1754.284013	59.283961	63.773441
1753.766454	53.192211	63.778446
1752.582446	56.687317	63.783450
1752.218919	53.367151	63.788455
1751.735747	50.159033	63.793460
1750.746730	53.104333	63.798465
1750.128357	53.596861	63.803470
1749.167906	59.505568	63.808474
1748.667435	46.290886	63.813479
1748.199458	56.936003	63.818484
1747.366584	52.602239	63.823489
1746.846240	52.640789	63.828494
1746.046528	59.295129	63.833498
1745.524864	53.844301	63.838503
1744.989636	55.205176	63.843508
1744.309010	65.098719	63.848513
1743.390504	55.613830	63.853518
1742.653496	55.369812	63.858522
1742.436411	48.843976	63.863527
1741.878555	48.275027	63.868532
1740.605862	61.979622	63.873537
1740.019807	46.051876	63.878542
1739.390943	52.515071	63.883546
1738.697885	56.922574	63.888551
1738.508949	57.104041	63.893556
1737.304129	59.214687	63.898561
1737.038903	51.307146	63.903566
1736.092674	59.534964	63.908570
1735.696735	56.663090	63.913575
1735.299948	58.202261	63.918580
1734.015233	57.102178	63.923585
1733.436509	51.346590	63.928590
1732.560747	54.658701	63.933594
1732.465414	56.071144	63.938599
1731.807629	60.178146	63.943604
1730.662722	57.795825	63.948609
1730.474185	60.511493	63.953614
1729.596863	68.086527	63.958618
1729.075720	56.941016	63.963623
1728.443163	44.084802	63.968628
1726.925782	53.937766	63.973633
1726.694547	55.144704	63.978638
1725.939427	53.741307	63.983642
1725.773695	51.269706	63.988647
1725.479390	51.226626	63.993652
1724.631252	52.730248	63.998657
1723.797975	41.094987	64.003662
1722.738501	53.019962	64.008666
1722.560734	50.051937	64.013671
1722.043249	57.760634	64.018676
1720.933755	58.050465	64.023681
1720.499829	47.217553	64.028686
1719.699718	56.568655	64.033690
1719.263755	54.449069	64.038695
1718.299190	55.657359	64.043700
1717.353021	52.737258	64.048705
1716.862152	52.624471	64.053710
1715.944657	51.865057	64.058714
1715.933015	47.656346	64.063719
1715.646005	49.706383	64.068724
1714.247933	59.486788	64.073729
1713.798566	52.094220	64.078734
1713.060123	57.376295	64.083738
1712.973018	50.088622	64.088743
1711.706444	48.657651	64.093748
1710.604769	56.582145	64.098753
1710.249773	47.367333	64.103758
1709.600895	47.500425	64.108762
1709.712212	45.599857	64.113767
1708.781484	51.844488	64.118772
1707.592058	55.987048	64.123777
1707.496614	56.967407	64.128782
1706.899932	59.222756	64.133786
1705.968177	57.058914	64.138791
1705.274484	53.303901	64.143796
1704.058605	55.726989	64.148801
1704.134684	56.626486	64.153806
1702.870544	60.367739	64.158810
1702.147300	53.945958	64.163815
1701.358392	50.223418	64.168820
1700.985766	60.260438	64.173825
1700.781953	50.583203	64.178830
1700.249250	65.230031	64.183834
1699.555828	51.112416	64.188839
1698.708927	47.850115	64.193844
1697.808606	54.966739	64.198849
1697.502289	43.235171	64.203854
1696.825473	50.814629	64.208858
1695.711804	50.854388	64.213863
1695.241088	53.416172	64.218868
1694.804482	62.998138	64.223873
1694.535757	46.773991	64.228878
1693.096867	55.012259	64.233882
1692.303650	56.019870	64.238887
1692.068423	58.988969	64.243892
1691.587798	56.598928	64.248897
1690.900788	59.682368	64.253902
1689.465782	57.093823	64.258906
1688.916520	54.429246	64.263911
1688.610151	53.421377	64.268916
1688.090826	54.734004	64.273921
1687.803502	61.090919	64.278926
1686.555352	63.301514	64.283930
1685.900541	55.099458	64.288935
1685.410826	54.024515	64.293940
1684.685345	53.624135	64.298945
1684.556507	52.148081	64.303950
1683.333718	51.566487	64.308954
1682.619116	52.806051	64.313959
1682.212404	54.616474	64.318964
1681.318808	59.193045	64.323969
1680.686114	43.118187	64.328974
1679.939173	55.911354	64.333978
1679.120739	52.775429	64.338983
1678.627153	47.610331	64.343988
1678.193274	60.003676	64.348993
1678.075378	49.451748	64.353998
1676.673220	52.858530	64.359002
1676.256523	54.213207	64.364007
1675.802177	51.423165	64.369012
1674.451952	55.474582	64.374017
1673.837282	51.475206	64.379022
1672.986708	53.381369	64.384026
1672.753210	41.914219	64.389031
1672.179550	49.464678	64.394036
1671.639338	55.666213	64.399041
1671.393544	47.224147	64.404046
1670.154076	53.352245	64.409050
1669.565007	48.676997	64.414055
1668.763400	48.230365	64.419060
1667.947636	51.135556	64.424065
1667.469342	44.711153	64.429070
1666.789546	47.651519	64.434074
1666.450265	46.633111	64.439079
1665.939306	53.497075	64.444084
1664.932657	50.954047	64.449089
1664.178273	44.553001	64.454094
1663.308416	53.287540	64.459098
1663.109342	47.750797	64.464103
1662.497330	52.282642	64.469108
1661.177902	51.691178	64.474113
1660.732890	46.693417	64.479118
1660.060905	60.946036	64.484122
1659.457478	46.247999	64.489127
1659.518708	50.879487	64.494132
1658.525792	60.685447	64.499137
1657.675870	51.752699	64.504142
1656.947826	56.694077	64.509146
1656.483752	49.382712	64.514151
1655.699755	50.459834	64.519156
1654.641745	57.170996	64.524161
1654.213587	50.391687	64.529166
1653.836963	61.673608	64.534170
1653.433606	55.401309	64.539175
1652.612042	55.363144	64.544180
1651.457434	53.021827	64.549185
1651.375391	43.743170	64.554190
1650.587672	56.744677	64.559194
1649.373412	48.046438	64.564199
1649.032595	46.921040	64.569204
1648.093356	45.425486	64.574209
1647.931804	52.364838	64.579214
1647.312243	53.448959	64.584218
1646.343832	47.477748	64.589223
1645.775320	55.502076	64.594228
1644.757734	54.137245	64.599233
1644.885775	51.794032	64.604238
1643.734202	55.561585	64.609242
1642.679629	54.700966	64.614247
1642.078201	48.945858	64.619252
1641.434491	50.451724	64.624257
1641.419440	49.545823	64.629262
1640.711213	61.415028	64.634266
1640.346186	53.305732	64.639271
1639.416263	50.890880	64.644276
1638.799433	54.759573	64.649281
1637.695047	45.157606	64.654286
1636.588849	55.792149	64.659290
1636.366547	58.040080	64.664295
1635.963785	46.573014	64.669300
1635.498701	54.626646	64.674305
1634.914901	50.299090	64.679310
1633.855354	53.326601	64.684314
1633.008296	53.385536	64.689319
1632.571623	52.737433	64.694324
1631.620327	55.317224	64.699329
1630.754099	48.861413	64.704334
1630.060841	47.492375	64.709338
1629.460025	56.494855	64.714343
1629.430883	44.482718	64.719348
1628.543211	55.555651	64.724353
1628.542406	46.175777	64.729358
1627.686914	50.945011	64.734362
1626.905307	42.395683	64.739367
1626.269577	47.517949	64.744372
1624.807131	48.781712	64.749377
1624.528472	42.197869	64.754382
1623.874942	47.466471	64.759386
1623.286734	46.142250	64.764391
1623.098664	42.119275	64.769396
1622.023452	54.658660	64.774401
1621.534506	44.009568	64.779406
1620.637616	50.398664	64.784410
1619.933590	46.069711	64.789415
1618.993611	45.984135	64.794420
1618.085238	47.949961	64.799425
1617.559240	44.777063	64.804430
1616.887240	54.361730	64.809434
1616.813248	52.888006	64.814439
1616.518874	51.414599	64.819444
1616.073485	62.177569	64.824449
1615.346570	51.993650	64.829454
1614.400365	58.266001	64.834458
1613.220279	52.552367	64.839463
1612.464818	45.698907	64.844468
1611.421982	57.359489	64.849473
1611.590180	53.418690	64.854478
1610.943851	50.985603	64.859482
1610.169068	67.809325	64.864487
1609.340993	58.038883	64.869492
1608.283262	54.855841	64.874497
1608.295513	55.651930	64.879502
1607.619951	60.711143	64.884506
1607.075640	58.507863	64.889511
1606.041553	43.865653	64.894516
1605.197377	56.655355	64.899521
1605.115766	49.884081	64.904526
1604.110373	56.692560	64.909530
1603.072755	56.169899	64.914535
1602.666398	44.676606	64.919540
1602.008808	48.756792	64.924545
1601.561537	48.083569	64.929550
1600.980344	56.240810	64.934554
1600.402164	52.346048	64.939559
1599.787400	50.217045	64.944564
1598.690425	56.051288	64.949569
1598.473295	45.559299	64.954574
1597.309713	57.474043	64.959578
1596.998335	51.245495	64.964583
1596.254242	59.124257	64.969588
1595.816071	59.668619	64.974593
1595.250805	51.840315	64.979598
1594.104527	51.927877	64.984602
1593.548061	54.490685	64.989607
1592.981147	52.917074	64.994612
1592.311749	57.483282	64.999617
1591.376532	56.070692	65.004622
1590.356913	65.857262	65.009626
1589.983151	57.449730	65.014631
1589.765127	59.564515	65.019636
1589.185051	59.235681	65.024641
1588.700711	43.026901	65.029646
1587.677376	55.353042	65.034650
1586.989257	56.496956	65.039655
1586.628713	53.035992	65.044660
1585.762905	57.586098	65.049665
1584.831601	46.565734	65.054670
1584.052848	52.142834	65.059674
1583.836174	50.978797	65.064679
1583.341315	58.847926	65.069684
1581.917417	56.029013	65.074689
1581.232974	50.395926	65.079694
1580.509606	68.178190	65.084698
1580.100519	60.295109	65.089703
1580.356053	56.256850	65.094708
1579.270108	52.468001	65.099713
1578.403780	53.506185	65.104718
1577.889947	60.200302	65.109722
1577.079352	64.162876	65.114727
1576.605925	63.927491	65.119732
1575.386849	62.228834	65.124737
1575.162419	53.493218	65.129742
1574.461562	59.051638	65.134746
1573.993195	60.523354	65.139751
1573.138027	53.435002	65.144756
1571.978288	57.339504	65.149761
1571.768744	47.272107	65.154766
1571.158141	50.253542	65.159770
1570.791904	55.479665	65.164775
1569.911646	50.871211	65.169780
1568.954237	55.852206	65.174785
1568.632510	47.303948	65.179790
1568.057763	50.885260	65.184794
1567.215067	43.047430	65.189799
1566.357215	48.200269	65.194804
1565.735075	54.347024	65.199809
1565.712515	51.105186	65.204814
1564.027094	57.974415	65.209818
1563.675237	50.173717	65.214823
1562.668637	52.383835	65.219828
1562.094821	58.333673	65.224833
1561.866622	45.982575	65.229838
1561.528852	51.784514	65.234842
1561.252303	50.301975	65.239847
1560.203865	51.668732	65.244852
1559.203451	52.029612	65.249857
1558.934142	42.705027	65.254862
1557.748827	49.348132	65.259866
1557.313268	44.864576	65.264871
1556.820569	48.349270	65.269876
1555.884822	51.833397	65.274881
1555.062571	49.936076	65.279886
1554.263627	57.027170	65.284890
1553.718788	52.187224	65.289895
1553.562284	41.652496	65.294900
1552.955383	49.747590	65.299905
1552.166016	44.840841	65.304910
1551.469084	46.493962	65.309914
1550.644176	40.550458	65.314919
1550.162973	49.111299	65.319924
1549.105199	54.139787	65.324929
1548.647887	45.225134	65.329934
1548.436757	41.980144	65.334938
1547.760953	46.583648	65.339943
1546.574897	45.130505	65.344948
1545.695689	51.010592	65.349953
1545.363303	41.850579	65.354958
1544.716816	42.603097	65.359962
1544.183604	41.412088	65.364967
1543.022555	40.792366	65.369972
1542.303457	48.649814	65.374977
1542.046201	36.082565	65.379982
1541.546426	41.011348	65.384986
1540.913773	40.791808	65.389991
1540.059757	39.120323	65.394996
1538.891861	45.181903	65.400001
1538.690435	32.870724	65.405006
1538.092993	48.562347	65.410010
1537.706435	43.533249	65.415015
1536.649734	48.321863	65.420020
1535.716235	47.352162	65.425025
1535.497551	41.857980	65.430030
1535.173386	53.338149	65.435034
1534.392778	47.785016	65.440039
1533.362423	46.376527	65.445044
1532.676862	46.532840	65.450049
1532.485591	41.928468	65.455054
1531.537038	48.836747	65.460058
1530.704893	47.795747	65.465063
1529.794098	40.552250	65.470068
1529.362071	45.192717	65.475073
1529.067328	42.055636	65.480078
1528.638463	44.402629	65.485082
1527.701094	47.503808	65.490087
1527.417842	40.682584	65.495092
1526.122367	52.454296	65.500097
1525.263657	38.069708	65.505102
1524.274607	52.144049	65.510106
1523.925679	41.926919	65.515111
1523.330944	36.143978	65.520116
1522.878334	48.299012	65.525121
1522.805765	44.120495	65.530126
1521.914648	45.809211	65.535130
1520.887712	46.216899	65.540135
1520.509077	44.223866	65.545140
1519.541670	58.613331	65.550145
1518.981134	44.700195	65.555150
1517.935941	44.735457	65.560154
1517.514164	47.620663	65.565159
1517.660218	41.516571	65.570164
1516.356900	46.593549	65.575169
1515.760155	41.408615	65.580174
1514.640186	48.749430	65.585178
1514.218184	42.634678	65.590183
1513.981632	43.058702	65.595188
1512.849875	46.450982	65.600193
1512.425156	45.709534	65.605198
1511.719560	50.179003	65.610202
1511.193284	55.503105	65.615207
1510.355792	41.537788	65.620212
1509.299722	42.557259	65.625217
1508.836885	40.959245	65.630222
1508.009580	49.623977	65.635226
1507.916006	36.745286	65.640231
1507.519302	43.471255	65.645236
1506.387968	48.793730	65.650241
1505.588201	36.959274	65.655246
1505.108468	39.776416	65.660250
1504.648406	47.092795	65.665255
1503.355593	42.668205	65.670260
1502.601263	53.067093	65.675265
1502.262157	41.769732	65.680270
1501.925001	50.593127	65.685274
1501.632878	42.325621	65.690279
1500.965120	45.048061	65.695284
1500.273068	47.165636	65.700289
1499.573513	45.065904	65.705294
1498.139309	47.273032	65.710298
1497.503004	47.888321	65.715303
1496.934602	48.521206	65.720308
1496.261346	48.382249	65.725313
1496.285605	47.184665	65.730318
1494.807918	53.587243	65.735322
1494.074919	44.205465	65.740327
1493.832801	44.382784	65.745332
1493.476382	49.372377	65.750337
1492.947014	46.387708	65.755342
1491.987490	49.110783	65.760346
1491.032815	48.239084	65.765351
1490.836004	44.630690	65.770356
1489.771245	53.419899	65.775361
1489.246370	43.024149	65.780366
1488.307428	54.510551	65.785370
1488.233753	57.023464	65.790375
1487.308899	50.291589	65.795380
1486.531960	52.670249	65.800385
1485.894180	40.008935	65.805390
1484.724083	43.836265	65.810394
1484.174618	42.666776	65.815399
1484.011892	47.291261	65.820404
1483.691953	60.645828	65.825409
1482.850992	46.570680	65.830414
1481.794595	46.521002	65.835418
1481.341652	52.516298	65.840423
1481.279779	47.131248	65.845428
1479.706953	52.008214	65.850433
1479.088710	43.462945	65.855438
1478.786305	45.233164	65.860442
1478.583441	46.457689	65.865447
1477.339405	42.686128	65.870452
1476.322063	47.747639	65.875457
1476.118620	38.007315	65.880462
1475.634634	48.039953	65.885466
1474.768278	41.962711	65.890471
1473.555106	38.239867	65.895476
1472.714995	47.908041	65.900481
1472.617259	42.621737	65.905486
1472.269305	47.334008	65.910490
1471.899545	43.311540	65.915495
1471.034601	37.622021	65.920500
1470.159086	46.087833	65.925505
1469.571044	36.115309	65.930510
1468.165146	42.649995	65.935514
1467.627740	38.893877	65.940519
1467.189009	40.256816	65.945524
1466.256965	41.507337	65.950529
1466.268210	41.314798	65.955534
1465.971907	46.974529	65.960538
1465.307175	45.362876	65.965543
1464.323671	48.537642	65.970548
1463.748732	42.440900	65.975553
1463.005285	44.145591	65.980558
1461.793134	48.380175	65.985562
1461.201418	57.119448	65.990567
1460.962978	40.586198	65.995572
1460.317616	48.316821	66.000577
1459.574996	36.949560	66.005582
1458.767798	43.631959	66.010586
1458.099569	38.018418	66.015591
1457.702676	42.120280	66.020596
1456.941684	45.516737	66.025601
1456.389559	34.201208	66.030606
1455.886740	40.450442	66.035610
1455.114353	38.684008	66.040615
1454.057395	39.795109	66.045620
1453.298506	50.010217	66.050625
1452.976353	40.014363	66.055630
1452.542422	42.277013	66.060634
1451.574398	45.819920	66.065639
1450.860687	48.074996	66.070644
1449.764770	49.037743	66.075649
1449.590796	42.710116	66.080654
1449.124319	46.920813	66.085658
1448.557695	47.021974	66.090663
1447.504378	47.052248	66.095668
1446.820101	50.248852	66.100673
1446.617974	40.451550	66.105678
1445.800935	44.699040	66.110682
1444.618647	44.426526	66.115687
1443.962490	48.675257	66.120692
1443.429887	47.130923	66.125697
1443.515574	33.263357	66.130702
1442.715515	42.978787	66.135706
1441.597421	45.845357	66.140711
1441.032391	43.576023	66.145716
1440.442943	46.514697	66.150721
1439.860892	42.612711	66.155726
1438.786998	45.866509	66.160730
1438.164132	49.583229	66.165735
1437.730915	41.483247	66.170740
1437.108241	48.655162	66.175745
1436.617993	39.077127	66.180750
1435.260442	46.403688	66.185754
1434.354279	47.404094	66.190759
1434.456061	52.776622	66.195764
1434.021265	58.305401	66.200769
1433.637006	46.482202	66.205774
1432.591253	53.295570	66.210778
1432.005173	40.586634	66.215783
1431.351012	50.625824	66.220788
1429.784162	48.525183	66.225793
1429.363885	48.282955	66.230798
1428.671321	45.467748	66.235802
1428.402280	46.089338	66.240807
1428.045943	44.964862	66.245812
1427.578800	52.785442	66.250817
1426.872411	54.723959	66.255822
1425.932185	42.590148	66.260826
1425.079396	46.955294	66.265831
1424.764817	46.775117	66.270836
1423.418719	47.514279	66.275841
1423.002909	41.155706	66.280846
1422.346419	44.811538	66.285850
1421.999612	49.840611	66.290855
1421.456383	45.197572	66.295860
1420.185338	51.937940	66.300865
1419.714102	46.053392	66.305870
1419.326476	45.000125	66.310874
1418.730316	45.154874	66.315879
1418.175739	48.999521	66.320884
1416.829448	45.138584	66.325889
1416.509248	35.427870	66.330894
1416.019239	47.409073	66.335898
1415.606358	47.241368	66.340903
1414.835315	43.768411	66.345908
1413.891897	52.174068	66.350913
1413.563927	34.924913	66.355918
1412.508553	42.203453	66.360922
1411.380599	47.279413	66.365927
1410.997666	38.526451	66.370932
1410.487699	46.497344	66.375937
1410.328576	35.193483	66.380942
1409.773924	37.330242	66.385946
1408.697786	51.804817	66.390951
1407.749180	42.580352	66.395956
1407.244077	44.445876	66.400961
1406.964332	35.171873	66.405966
1406.201136	46.054746	66.410970
1405.577296	40.244924	66.415975
1405.255291	33.929797	66.420980
1403.322116	46.354864	66.425985
1403.063812	35.766960	66.430990
1402.533220	43.870445	66.435994
1402.278451	34.783291	66.440999
1401.978083	41.191170	66.446004
1400.750225	46.948511	66.451009
1399.977789	33.244160	66.456014
1399.537499	33.544455	66.461018
1398.939909	38.484074	66.466023
1397.981921	36.094280	66.471028
1396.975108	47.242967	66.476033
1396.961782	36.286530	66.481038
1396.073621	45.276358	66.486042
1395.629491	44.558517	66.491047
1394.619293	37.181065	66.496052
1393.515998	41.251711	66.501057
1393.618792	40.683486	66.506062
1392.832572	46.676570	66.511066
1392.332959	37.811268	66.516071
1391.933033	36.813579	66.521076
1390.686665	47.066759	66.526081
1390.251490	38.413572	66.531086
1389.719972	38.021871	66.536090
1388.728507	41.582717	66.541095
1388.344028	35.889402	66.546100
1387.332204	42.892936	66.551105
1387.214096	38.030941	66.556110
1385.806656	44.387709	66.561114
1384.911218	37.712712	66.566119
1384.837483	34.788113	66.571124
1384.057757	32.885671	66.576129
1383.881033	33.962538	66.581134
1383.114732	37.274698	66.586138
1382.079067	39.954717	66.591143
1381.867127	36.444940	66.596148
1381.019548	48.891430	66.601153
1380.539499	39.732851	66.606158
1379.701777	30.402468	66.611162
1378.995656	44.132229	66.616167
1378.639438	35.537461	66.621172
1377.088757	45.955718	66.626177
1376.222046	38.208523	66.631182
1375.776297	38.169056	66.636186
1375.353387	34.680200	66.641191
1375.197732	31.890054	66.646196
1374.946788	39.515411	66.651201
1374.380212	35.003837	66.656206
1373.388494	34.123879	66.661210
1372.205976	37.601555	66.666215
1371.419197	33.404117	66.671220
1370.607402	44.687395	66.676225
1370.032731	38.759378	66.681230
1369.776679	47.907362	66.686234
1369.259758	47.943867	66.691239
1368.873315	33.468518	66.696244
1367.334155	37.805586	66.701249
1367.043215	36.268588	66.706254
1366.548491	36.956022	66.711258
1365.519747	43.662623	66.716263
1364.858045	36.300752	66.721268
1364.253593	42.509381	66.726273
1363.679215	39.292195	66.731278
1363.346380	38.318540	66.736282
1362.936404	39.587034	66.741287
1361.904251	35.922208	66.746292
1361.405711	43.041281	66.751297
1360.443074	43.717941	66.756302
1359.358559	51.507354	66.761306
1358.515352	49.430499	66.766311
1358.540103	33.746456	66.771316
1357.990771	48.064754	66.776321
1357.754692	45.672182	66.781326
1356.485245	38.388001	66.786330
1355.505895	42.008436	66.791335
1355.443586	37.370971	66.796340
1354.440719	54.207309	66.801345
1353.626221	37.958063	66.806350
1353.128440	48.331960	66.811354
1352.318327	39.777812	66.816359
1351.957838	45.233279	66.821364
1351.234836	36.777252	66.826369
1350.312201	52.328191	66.831374
1349.804702	50.655303	66.836378
1348.948221	46.350674	66.841383
1348.739123	46.085927	66.846388
1348.070393	49.491401	66.851393
1347.235215	49.679433	66.856398
1346.394457	48.362310	66.861402
1345.905955	48.452651	66.866407
1345.937294	35.245040	66.871412
1344.249000	41.031443	66.876417
1343.787613	38.048620	66.881422
1343.117244	45.218668	66.886426
1342.319292	40.130428	66.891431
1342.442659	51.318669	66.896436
1341.032329	45.279070	66.901441
1340.600210	44.064149	66.906446
1340.066112	42.255140	66.911450
1339.648038	43.436613	66.916455
1338.667683	35.674385	66.921460
1337.721160	43.937044	66.926465
1337.114948	33.052793	66.931470
1336.980279	44.004495	66.936474
1335.967838	39.410843	66.941479
1335.362122	34.638988	66.946484
1334.465352	48.529959	66.951489
1334.461239	39.824027	66.956494
1333.530742	40.665904	66.961498
1332.479715	37.890368	66.966503
1332.112911	38.040215	66.971508
1331.343888	42.158672	66.976513
1331.147518	40.712302	66.981518
1329.986516	37.034856	66.986522
1329.331259	36.355323	66.991527
1328.576097	33.821345	66.996532
1328.197175	39.890043	67.001537
1327.344617	31.706946	67.006542
1326.460413	35.977760	67.011546
1325.822949	45.112260	67.016551
1325.831702	41.827608	67.021556
1325.045267	38.745073	67.026561
1324.096378	34.535575	67.031566
1323.246256	34.533596	67.036570
1322.801447	33.943614	67.041575
1322.404487	36.843822	67.046580
1321.216508	32.418439	67.051585
1320.412054	33.631379	67.056590
1319.802747	43.743876	67.061594
1319.344413	34.387894	67.066599
1319.269497	40.157517	67.071604
1318.376589	46.479827	67.076609
1317.603810	45.191333	67.081614
1317.170885	36.586696	67.086618
1316.359497	45.225283	67.091623
1315.462372	28.692726	67.096628
1314.541959	40.602003	67.101633
1314.148121	35.693963	67.106638
1313.608625	45.328570	67.111642
1313.133001	35.418655	67.116647
1312.347204	33.345307	67.121652
1311.281879	41.883912	67.126657
1311.155544	35.260141	67.131662
1310.511148	43.790174	67.136666
1309.434143	38.282673	67.141671
1309.199694	41.639611	67.146676
1308.493479	37.350534	67.151681
1307.651514	38.832802	67.156686
1306.744545	42.280892	67.161690
1306.041849	43.889257	67.166695
1305.957189	28.310936	67.171700
1304.975800	37.414956	67.176705
1304.120047	39.268436	67.181710
1303.329972	31.919113	67.186714
1302.897118	35.105737	67.191719
1302.986633	37.744094	67.196724
1301.488843	45.865743	67.201729
1300.760917	36.543166	67.206734
1299.846762	40.981182	67.211738
1299.540595	35.324322	67.216743
1299.339265	32.118808	67.221748
1298.315922	37.600814	67.226753
1297.745894	40.030208	67.231758
1296.982499	35.280280	67.236762
1296.475162	47.350980	67.241767
1296.283915	32.611223	67.246772
1294.597118	37.019114	67.251777
1294.368128	29.651553	67.256782
1293.799266	35.941269	67.261786
1293.258160	38.790280	67.266791
1292.376830	40.893843	67.271796
1291.520017	36.373242	67.276801
1291.110160	32.169522	67.281806
1290.481436	32.036155	67.286810
1290.122778	35.575272	67.291815
1288.884390	28.853918	67.296820
1288.258994	37.391970	67.301825
1288.137550	33.353713	67.306830
1287.355421	40.252946	67.311834
1286.335873	30.153548	67.316839
1285.691826	37.701053	67.321844
1285.167048	39.519262	67.326849
1284.831882	29.902428	67.331854
1283.632067	30.810798	67.336858
1282.742254	40.253514	67.341863
1282.315366	29.514244	67.346868
1281.745659	37.781660	67.351873
1281.447135	26.831165	67.356878
1280.458233	36.988247	67.361882
1279.278502	26.201518	67.366887
1279.074908	25.847590	67.371892
1278.464031	24.282624	67.376897
1278.442619	24.981553	67.381902
1277.390771	42.748229	67.386906
1276.306725	45.177353	67.391911
1275.625046	30.736362	67.396916
1275.110161	37.545795	67.401921
1275.219756	35.885198	67.406926
1274.062649	46.923769	67.411930
1273.103160	36.253411	67.416935
1272.942272	33.470414	67.421940
1271.848554	38.153038	67.426945
1271.091039	29.063848	67.431950
1270.548115	35.420407	67.436954
1269.903848	32.824660	67.441959
1269.761852	37.535738	67.446964
1268.384422	38.778295	67.451969
1267.750530	37.289532	67.456974
1267.334630	37.988106	67.461978
1266.880740	42.083282	67.466983
1266.288107	35.369651	67.471988
1265.081631	37.269447	67.476993
1264.906960	37.327250	67.481998
1264.576279	42.156643	67.487002
1263.311114	39.610734	67.492007
1262.723920	35.264901	67.497012
1261.735968	41.687495	67.502017
1261.607960	30.197363	67.507022
1260.557865	33.665069	67.512026
1259.536366	37.397897	67.517031
1259.399606	33.568666	67.522036
1258.671070	37.327453	67.527041
1258.567296	35.192987	67.532046
1257.187448	32.171716	67.537050
1256.414102	44.697889	67.542055
1256.455477	34.939181	67.547060
1255.660646	43.292864	67.552065
1255.167351	38.667164	67.557070
1254.001015	42.147050	67.562074
1253.490149	38.005130	67.567079
1253.217327	36.763320	67.572084
1251.847387	43.087380	67.577089
1250.937507	42.147147	67.582094
1250.566391	41.677928	67.587098
1249.929429	41.225749	67.592103
1249.528298	33.945491	67.597108
1249.002018	35.751330	67.602113
1248.179510	33.188662	67.607118
1247.529329	39.707366	67.612122
1246.941908	36.426050	67.617127
1246.887631	33.391130	67.622132
1245.257321	39.009094	67.627137
1245.242681	33.812107	67.632142
1244.485436	40.715278	67.637146
1242.928934	40.371471	67.642151
1242.356881	38.111188	67.647156
1241.636997	38.232034	67.652161
1241.689903	41.499126	67.657166
1241.134613	34.390044	67.662170
1240.419964	34.057458	67.667175
1239.626661	25.292527	67.672180
1238.706877	34.497158	67.677185
1238.519936	32.030555	67.682190
1237.884259	29.091241	67.687194
1236.391493	33.750597	67.692199
1236.152020	29.338440	67.697204
1235.562188	29.782394	67.702209
1235.370331	25.433632	67.707214
1234.692023	22.993124	67.712218
1233.322904	33.945561	67.717223
1232.819793	27.504723	67.722228
1232.298003	32.561631	67.727233
1231.938361	25.363096	67.732238
1230.820890	26.054963	67.737242
1230.277005	32.231901	67.742247
1230.009510	31.700475	67.747252
1229.069373	38.847205	67.752257
1228.581541	23.596376	67.757262
1227.624528	30.184373	67.762266
1227.142686	37.608320	67.767271
1226.720344	35.800490	67.772276
1225.297336	37.021931	67.777281
1224.899315	36.339368	67.782286
1224.394532	39.945885	67.787290
1223.799052	40.307159	67.792295
1223.053904	30.922697	67.797300
1221.944791	37.105940	67.802305
1221.775432	34.176057	67.807310
1221.094070	33.972228	67.812314
1220.470042	35.907160	67.817319
1220.182522	29.023597	67.822324
1219.169072	35.939128	67.827329
1219.035306	35.723916	67.832334
1217.869787	32.813669	67.837338
1217.214193	37.163283	67.842343
1216.153334	36.275458	67.847348
1215.698248	42.430397	67.852353
1215.339246	33.082304	67.857358
1214.086954	32.237539	67.862362
1213.338308	36.321244	67.867367
1213.007196	33.893340	67.872372
1212.420904	39.700124	67.877377
1212.335472	39.078244	67.882382
1210.992571	31.793215	67.887386
1210.292438	43.304778	67.892391
1209.823224	26.705808	67.897396
1209.171235	43.697684	67.902401
1208.849376	39.088888	67.907406
1207.914150	41.495949	67.912410
1207.133606	43.550396	67.917415
1206.854137	37.578636	67.922420
1205.763574	38.252042	67.927425
1205.040217	35.202097	67.932430
1204.270615	33.148287	67.937434
1203.839582	41.499321	67.942439
1203.423437	35.386867	67.947444
1202.848037	44.664484	67.952449
1202.040624	33.949477	67.957454
1201.202467	30.618160	67.962458
1200.612225	31.902729	67.967463
1200.094019	37.309167	67.972468
1199.014850	41.333473	67.977473
1198.260281	31.486879	67.982478
1197.816103	28.666938	67.987482
1197.524568	30.427569	67.992487
1196.936298	31.237148	67.997492
1195.811425	40.449177	68.002497
1195.440746	36.426909	68.007502
1194.602411	32.179383	68.012506
1194.433041	39.895851	68.017511
1193.313646	29.635756	68.022516
1192.602039	31.904753	68.027521
1192.202070	34.315007	68.032526
1191.623452	30.489819	68.037530
1190.453423	30.399983	68.042535
1189.648477	26.634445	68.047540
1189.085306	34.268453	68.052545
1189.016143	28.931904	68.057550
1188.401074	27.463825	68.062554
1187.056254	33.386511	68.067559
1186.538169	31.839928	68.072564
1185.647917	26.063087	68.077569
1185.747794	37.778590	68.082574
1184.897032	31.913463	68.087578
1184.026404	41.220684	68.092583
1183.604486	27.766631	68.097588
1183.043475	43.364163	68.102593
1182.094915	32.009272	68.107598
1181.371500	33.586269	68.112602
1180.886192	32.810359	68.117607
1180.394701	25.224362	68.122612
1179.245211	39.578183	68.127617
1178.456008	34.457074	68.132622
1178.085827	31.615906	68.137626
1177.514953	32.946287	68.142631
1177.475722	31.421324	68.147636
1176.053734	36.824840	68.152641
1175.632929	32.298023	68.157646
1174.849559	35.791153	68.162650
1174.455029	39.990444	68.167655
1173.338573	32.986401	68.172660
1172.501860	46.391596	68.177665
1172.052489	38.496110	68.182670
1171.598350	43.428726	68.187674
1170.889169	35.342743	68.192679
1170.390623	28.546370	68.197684
1169.576941	38.191477	68.202689
1168.767616	34.396678	68.207694
1168.495670	45.764453	68.212698
1167.780141	31.144382	68.217703
1166.926292	34.476830	68.222708
1166.314762	42.724106	68.227713
1165.853186	37.175568	68.232718
1164.670142	40.951470	68.237722
1163.899706	43.605160	68.242727
1163.540285	33.850279	68.247732
1162.977256	38.314497	68.252737
1162.664147	34.297272	68.257742
1161.664222	43.117270	68.262746
1160.442236	41.245812	68.267751
1160.238182	42.470547	68.272756
1159.895045	46.008788	68.277761
1159.316287	36.998443	68.282766
1158.163404	30.619964	68.287770
1157.630105	44.819022	68.292775
1157.383748	34.866382	68.297780
1156.120276	41.783853	68.302785
1155.353843	37.198465	68.307790
1154.721388	40.520938	68.312794
1154.140067	37.915211	68.317799
1154.240421	28.962446	68.322804
1153.334152	33.456023	68.327809
1152.551322	35.074018	68.332814
1152.097698	31.232114	68.337818
1150.932797	41.286336	68.342823
1150.063836	32.210186	68.347828
1149.546032	35.419804	68.352833
1149.188227	34.470651	68.357838
1148.978599	31.100889	68.362842
1147.744307	35.599331	68.367847
1147.208008	39.472655	68.372852
1146.189730	38.939221	68.377857
1145.995732	31.179753	68.382862
1145.215746	33.525872	68.387866
1144.040960	38.737119	68.392871
1143.518197	30.208324	68.397876
1143.056083	35.542768	68.402881
1142.736424	37.162794	68.407886
1142.077438	32.869416	68.412890
1140.989750	32.432182	68.417895
1140.399228	35.143995	68.422900
1139.647662	34.910352	68.427905
1139.450427	32.068493	68.432910
1138.333743	33.294878	68.437914
1137.645137	34.722843	68.442919
1137.191175	27.111963	68.447924
1136.657204	36.226871	68.452929
1136.606516	27.820119	68.457934
1135.570236	35.395341	68.462938
1134.900673	32.873043	68.467943
1134.013191	36.456862	68.472948
1132.576983	47.894700	68.477953
1131.945086	35.596880	68.482958
1131.679415	32.586128	68.487962
1131.096069	33.814421	68.492967
1131.012003	27.466235	68.497972
1130.058623	35.143394	68.502977
1129.243339	36.990492	68.507982
1128.765731	34.770411	68.512986
1128.189965	35.729408	68.517991
1127.399214	24.679043	68.522996
1126.361470	35.197183	68.528001
1126.134265	28.032801	68.533006
1125.632725	33.477599	68.538010
1124.560015	31.684923	68.543015
1124.273204	33.979413	68.548020
1123.427289	41.237348	68.553025
1122.807133	32.359762	68.558030
1121.856523	25.972787	68.563034
1121.012664	34.490415	68.568039
1120.673121	25.885177	68.573044
1120.039406	42.547712	68.578049
1119.619348	32.788295	68.583054
1118.571265	32.313231	68.588058
1117.990196	32.661198	68.593063
1117.771111	28.764649	68.598068
1116.720529	38.316558	68.603073
1115.670568	33.255873	68.608078
1115.036545	36.733149	68.613082
1114.648726	44.077499	68.618087
1114.633331	31.965487	68.623092
1113.713281	40.930492	68.628097
1113.044008	29.419246	68.633102
1112.232365	25.897659	68.638106
1111.429069	38.967949	68.643111
1110.568631	32.896226	68.648116
1109.635432	36.947810	68.653121
1109.385397	29.589936	68.658126
1109.046707	33.417639	68.663130
1108.397643	35.474854	68.668135
1107.520249	27.759442	68.673140
1106.466584	41.475128	68.678145
1106.247885	24.581665	68.683150
1105.902370	35.652830	68.688154
1104.559197	32.804014	68.693159
1104.377972	36.874761	68.698164
1103.311721	41.710781	68.703169
1103.193990	33.535475	68.708174
1101.917742	34.424547	68.713178
1101.073520	39.941208	68.718183
1100.757183	35.427752	68.723188
1100.256462	37.280017	68.728193
1099.831683	35.387440	68.733198
1098.943807	31.818056	68.738202
1097.959710	35.369945	68.743207
1097.608433	30.325869	68.748212
1096.932156	41.358975	68.753217
1096.632280	31.197237	68.758222
1095.318341	27.719284	68.763226
1094.427404	35.050619	68.768231
1094.155754	24.415238	68.773236
1093.842435	35.873955	68.778241
1093.341479	31.279479	68.783246
1092.295278	27.627259	68.788250
1091.472471	33.740563	68.793255
1091.425021	33.514781	68.798260
1090.151785	37.462762	68.803265
1089.556032	26.658156	68.808270
1088.953896	31.747578	68.813274
1088.503756	26.048217	68.818279
1088.073145	28.692812	68.823284
1086.666508	33.340124	68.828289
1086.254982	35.058350	68.833294
1085.654836	27.826352	68.838298
1085.125664	28.718020	68.843303
1084.480671	26.639697	68.848308
1083.594929	29.933875	68.853313
1082.954436	29.753545	68.858318
1082.635213	33.406261	68.863322
1081.863797	35.733688	68.868327
1081.143266	21.283989	68.873332
1080.430283	30.224731	68.878337
1079.657263	28.161256	68.883342
1078.667901	28.701918	68.888346
1077.723347	35.976341	68.893351
1077.637879	30.560391	68.898356
1076.703544	29.822027	68.903361
1076.621300	32.579946	68.908366
1076.522205	27.293113	68.913370
1075.471489	30.670309	68.918375
1074.699353	17.361112	68.923380
1073.783830	29.186077	68.928385
1072.966375	26.733057	68.933390
1072.238076	32.826600	68.938394
1071.376948	35.627209	68.943399
1071.478967	22.825519	68.948404
1070.684240	37.560551	68.953409
1069.958828	33.080636	68.958414
1069.258905	32.266348	68.963418
1068.526478	40.912927	68.968423
1068.282816	33.959333	68.973428
1066.738421	36.240992	68.978433
1066.252378	32.200831	68.983438
1065.991064	33.346368	68.988442
1065.259837	30.254353	68.993447
1064.845785	24.703015	68.998452
1063.588384	34.242894	69.003457
1063.159319	26.578398	69.008462
1062.698604	36.406291	69.013466
1062.109146	33.650491	69.018471
1061.352739	23.354017	69.023476
1060.078706	35.760375	69.028481
1059.808048	27.455649	69.033486
1059.678311	31.313196	69.038490
1058.725051	35.184266	69.043495
1057.981883	24.130305	69.048500
1057.140595	38.653544	69.053505
1057.012098	32.554503	69.058510
1055.880524	24.381219	69.063514
1054.818960	30.750928	69.068519
1054.449835	29.291066	69.073524
1053.983409	36.002140	69.078529
1053.713177	27.071279	69.083534
1052.511641	29.203780	69.088538
1051.847645	34.387420	69.093543
1051.681364	27.107700	69.098548
1050.473328	33.519637	69.103553
1050.285800	32.947124	69.108558
1049.198419	28.766083	69.113562
1048.445282	36.621939	69.118567
1048.308937	32.479627	69.123572
1047.484502	39.583560	69.128577
1046.233824	34.197649	69.133582
1045.721126	34.597834	69.138586
1044.977351	33.893034	69.143591
1045.254914	28.608573	69.148596
1044.266005	37.533297	69.153601
1043.397945	31.823159	69.158606
1042.644441	37.797714	69.163610
1041.837816	34.749240	69.168615
1041.575020	27.019661	69.173620
1041.005111	33.940381	69.178625
1040.111826	31.671329	69.183630
1039.421175	23.249707	69.188634
1039.100793	30.671638	69.193639
1038.247878	30.036244	69.198644
1037.014808	35.392427	69.203649
1036.988189	24.766175	69.208654
1036.404212	26.923440	69.213658
1035.713247	30.193742	69.218663
1035.228359	22.081595	69.223668
1034.556368	31.420324	69.228673
1033.521121	27.374505	69.233678
1032.679730	35.436009	69.238682
1031.898356	37.104271	69.243687
1031.611034	29.891120	69.248692
1031.029183	38.806282	69.253697
1030.235623	31.603493	69.258702
1029.378118	32.410210	69.263706
1028.790394	37.184318	69.268711
1028.373308	27.692546	69.273716
1027.019364	36.693486	69.278721
1026.505626	33.181304	69.283726
1026.064103	34.620452	69.288730
1025.533722	33.954249	69.293735
1025.157284	30.018089	69.298740
1024.566284	40.402895	69.303745
1023.812436	38.969553	69.308750
1023.029197	41.052866	69.313754
1022.430693	39.203713	69.318759
1021.632712	34.422325	69.323764
1020.566802	34.095222	69.328769
1020.330899	34.159630	69.333774
1019.718583	29.015170	69.338778
1019.130922	36.861263	69.343783
1018.377025	27.467238	69.348788
1017.338126	42.187513	69.353793
1017.199026	32.321132	69.358798
1016.861292	33.169741	69.363802
1015.309117	28.206355	69.368807
1014.822815	34.774722	69.373812
1014.138552	32.399882	69.378817
1013.655060	27.258584	69.383822
1013.365613	31.403323	69.388826
1012.233564	38.777774	69.393831
1011.866377	33.930215	69.398836
1011.230935	35.292982	69.403841
1010.008737	33.856887	69.408846
1009.461558	33.254863	69.413850
1008.736325	34.578299	69.418855
1008.285092	32.790877	69.423860
1007.866149	38.637303	69.428865
1007.380125	39.850138	69.433870
1006.268339	33.998226	69.438874
1005.467840	40.009442	69.443879
1005.208974	27.672828	69.448884
1004.369792	33.885744	69.453889
1004.274040	30.450572	69.458894
1003.105766	30.056182	69.463898
1002.361122	30.389199	69.468903
1002.264264	14.959557	69.473908
1001.123768	34.025639	69.478913
1000.333519	30.142709	69.483918
999.547608	27.151670	69.488922
998.903357	32.623924	69.493927
998.947191	28.365427	69.498932
997.685426	32.357356	69.503937
997.066288	28.377814	69.508942
996.657848	33.274792	69.513946
995.800886	37.298513	69.518951
995.347500	33.243710	69.523956
994.342267	43.195310	69.528961
993.723123	35.519280	69.533966
993.249658	27.720724	69.538970
992.849416	32.020292	69.543975
992.268130	23.540284	69.548980
990.977522	40.876640	69.553985
990.834932	37.581387	69.558990
989.903546	36.978996	69.563994
989.051977	39.107885	69.568999
988.682904	32.860256	69.574004
987.948054	47.052757	69.579009
987.464091	35.927610	69.584014
986.655147	31.904151	69.589018
985.622870	35.700296	69.594023
985.437527	26.977510	69.599028
984.774925	42.332587	69.604033
984.081154	28.489753	69.609038
983.390488	40.395668	69.614042
982.689913	40.600249	69.619047
982.128176	28.663502	69.624052
980.769993	31.089051	69.629057
980.076845	37.460094	69.634062
979.808359	40.393521	69.639066
979.395529	37.726335	69.644071
979.255591	36.646346	69.649076
978.258919	41.876629	69.654081
977.197911	35.863682	69.659086
976.825650	37.600909	69.664090
976.129623	38.421375	69.669095
975.183951	36.622743	69.674100
974.255007	46.147462	69.679105
974.104179	35.479471	69.684110
973.442194	38.795641	69.689114
972.880667	33.431795	69.694119
971.992243	28.183045	69.699124
971.194679	41.846978	69.704129
970.952271	35.738473	69.709134
970.172529	40.424871	69.714138
969.333499	34.297757	69.719143
968.501433	28.811377	69.724148
967.704996	34.583827	69.729153
967.423945	32.360891	69.734158
967.219476	31.529297	69.739162
966.649773	37.970590	69.744167
965.926004	32.440167	69.749172
965.146716	33.374813	69.754177
964.150323	36.471376	69.759182
963.123430	39.815651	69.764186
962.348344	43.727004	69.769191
962.574128	38.371924	69.774196
961.825503	40.713106	69.779201
960.602036	35.019340	69.784206
959.999337	33.096752	69.789210
959.177227	33.109361	69.794215
959.068456	30.810126	69.799220
958.372059	41.021683	69.804225
957.519651	29.801421	69.809230
956.898974	32.773543	69.814234
956.225653	44.690898	69.819239
955.810326	29.759794	69.824244
954.631852	39.841475	69.829249
953.881118	35.502827	69.834254
953.300024	37.541377	69.839258
953.005219	45.642091	69.844263
952.730372	35.306084	69.849268
951.738782	40.576570	69.854273
950.830674	33.053773	69.859278
950.560939	34.858269	69.864282
949.324878	37.835276	69.869287
948.758295	36.551936	69.874292
947.753265	33.654131	69.879297
947.489925	37.581827	69.884302
947.551570	33.646935	69.889306
946.840179	39.951501	69.894311
945.567304	30.425615	69.899316
944.904651	39.926886	69.904321
944.697264	30.523195	69.909326
943.974480	32.991160	69.914330
942.654887	35.897880	69.919335
942.602900	27.092378	69.924340
941.997593	41.662458	69.929345
941.037270	42.534453	69.934350
940.275162	37.525818	69.939354
939.744384	44.787270	69.944359
939.388174	30.430254	69.949364
938.025469	40.334671	69.954369
937.274661	36.243629	69.959374
936.907480	39.140724	69.964378
936.522929	42.890586	69.969383
935.992823	29.898539	69.974388
934.885327	41.389808	69.979393
934.021156	37.029793	69.984398
933.540220	36.511864	69.989402
932.743921	38.649323	69.994407
933.083386	31.170861	69.999412
932.259277	34.452914	70.004417
931.540411	30.460874	70.009422
930.648457	35.307067	70.014426
929.277987	51.515995	70.019431
928.888302	24.565667	70.024436
927.919747	41.152184	70.029441
927.975451	40.616668	70.034446
927.597457	28.258028	70.039450
926.835409	37.555915	70.044455
925.777766	33.868531	70.049460
924.877150	40.094402	70.054465
924.866026	37.087326	70.059470
924.279937	35.075369	70.064474
922.769670	47.669984	70.069479
922.717670	23.991814	70.074484
922.036698	37.810667	70.079489
921.192083	35.615918	70.084494
920.274562	27.750850	70.089498
919.513466	38.150908	70.094503
919.256359	31.472303	70.099508
918.839836	45.230154	70.104513
918.412011	27.049283	70.109518
917.254354	31.527743	70.114522
916.517453	34.483677	70.119527
916.377774	28.759393	70.124532
915.056129	29.580085	70.129537
914.319264	38.708383	70.134542
913.959850	30.549489	70.139546
913.121019	44.507014	70.144551
913.191281	33.706077	70.149556
911.933139	39.585137	70.154561
911.128972	32.093127	70.159566
910.638540	34.904179	70.164570
909.858727	32.752740	70.169575
909.223184	33.106269	70.174580
908.255984	38.529010	70.179585
907.842572	41.411387	70.184590
907.627359	38.982433	70.189594
906.929573	39.262287	70.194599
906.291438	32.384117	70.199604
905.232589	43.180084	70.204609
904.699786	39.426529	70.209614
904.184017	32.842708	70.214618
903.172514	38.375006	70.219623
902.729246	33.730393	70.224628
902.238090	29.610659	70.229633
901.525600	29.233670	70.234638
900.431599	36.833924	70.239642
899.683421	35.275136	70.244647
899.431768	29.704296	70.249652
898.814845	41.038653	70.254657
898.606776	35.880356	70.259662
897.842285	36.076208	70.264666
897.031609	38.569212	70.269671
896.395140	34.202938	70.274676
895.006331	39.580814	70.279681
894.403132	29.530478	70.284686
894.048108	32.807275	70.289690
893.488338	33.339565	70.294695
893.168764	26.374432	70.299700
892.132885	37.912663	70.304705
891.633772	35.349116	70.309710
891.139653	37.640349	70.314714
889.769676	44.368297	70.319719
889.144936	30.355240	70.324724
888.634671	37.873636	70.329729
887.842175	34.634517	70.334734
887.798224	43.494844	70.339738
887.124500	46.585817	70.344743
886.306493	31.095908	70.349748
885.420874	38.577846	70.354753
885.156998	42.873073	70.359758
884.989414	34.150628	70.364762
883.508181	37.545164	70.369767
882.940192	30.725226	70.374772
882.351087	42.242821	70.379777
881.442190	37.844212	70.384782
880.727235	37.636359	70.389786
879.881953	30.622429	70.394791
879.641926	37.914884	70.399796
879.183180	40.694091	70.404801
878.132611	36.149292	70.409806
877.599401	41.241190	70.414810
876.651355	40.324517	70.419815
876.608090	35.731368	70.424820
875.936011	48.208372	70.429825
874.988870	42.213621	70.434830
874.358620	36.649420	70.439834
873.522896	40.668221	70.444839
873.261304	33.465196	70.449844
871.994158	35.526219	70.454849
870.959967	33.566671	70.459854
870.952249	34.720751	70.464858
870.109327	37.258319	70.469863
870.103441	41.223895	70.474868
869.469246	44.154034	70.479873
868.487380	34.342172	70.484878
867.903899	42.395789	70.489882
866.933108	38.790804	70.494887
865.985073	33.001212	70.499892
865.257343	35.507833	70.504897
864.920150	29.263042	70.509902
864.694731	33.706693	70.514906
863.900182	37.509201	70.519911
863.484881	32.897994	70.524916
862.405050	44.312343	70.529921
861.961491	30.374542	70.534926
861.365365	35.279329	70.539930
860.342568	38.525216	70.544935
859.651999	29.469690	70.549940
858.925442	35.836613	70.554945
858.808267	38.320176	70.559950
857.822601	38.724714	70.564954
857.014739	40.409860	70.569959
856.642095	36.381661	70.574964
855.945388	42.242351	70.579969
855.220831	35.674427	70.584974
854.335547	37.359280	70.589978
853.547458	37.051109	70.594983
853.240077	34.100653	70.599988
852.941640	27.532721	70.604993
851.962118	34.209574	70.609998
851.524215	37.204669	70.615002
850.608661	40.092859	70.620007
850.058721	36.548634	70.625012
848.951845	40.055497	70.630017
848.477931	36.792492	70.635022
847.947443	31.102034	70.640026
847.122356	36.003843	70.645031
846.165757	32.841323	70.650036
845.460303	43.342932	70.655041
844.902759	33.350000	70.660046
844.449590	41.507461	70.665050
844.028322	39.817805	70.670055
844.052181	30.374173	70.675060
843.049067	33.785671	70.680065
842.158556	34.815329	70.685070
841.069827	33.268186	70.690074
840.254930	35.206775	70.695079
839.897590	26.060371	70.700084
839.392032	42.237311	70.705089
839.048685	36.100738	70.710094
838.313948	41.987986	70.715098
837.213484	32.817933	70.720103
836.682844	31.767025	70.725108
836.083521	32.368704	70.730113
835.284881	30.822699	70.735118
834.612065	30.439414	70.740122
834.026737	32.816140	70.745127
833.641865	33.754278	70.750132
832.490096	33.477193	70.755137
831.791858	41.217911	70.760142
831.364905	30.820988	70.765146
830.842666	28.869858	70.770151
830.427603	27.772169	70.775156
829.214978	32.847635	70.780161
828.653106	38.820911	70.785166
828.109877	34.550205	70.790170
827.326528	44.663660	70.795175
827.210955	28.621991	70.800180
825.756442	30.321765	70.805185
825.420006	21.213041	70.810190
825.255555	31.442445	70.815194
824.035277	32.663376	70.820199
823.479404	24.614628	70.825204
822.677724	32.750288	70.830209
821.968369	30.721708	70.835214
821.968063	24.992599	70.840218
820.640208	29.129173	70.845223
820.028857	25.716162	70.850228
819.233665	35.222777	70.855233
819.070984	26.021737	70.860238
818.485098	29.962934	70.865242
817.199998	37.637792	70.870247
816.650579	22.953597	70.875252
816.117126	36.835714	70.880257
816.025042	31.766203	70.885262
814.804657	30.790401	70.890266
813.967328	42.125159	70.895271
813.837292	28.777729	70.900276
813.071657	33.272679	70.905281
812.189473	30.044711	70.910286
811.969613	39.226352	70.915290
810.825992	35.563746	70.920295
810.603814	32.125058	70.925300
809.117901	40.082629	70.930305
808.888718	35.471770	70.935310
808.469302	39.206694	70.940314
807.773701	38.789195	70.945319
807.027301	32.188497	70.950324
806.056407	42.415389	70.955329
806.005989	30.078756	70.960334
805.280127	34.572109	70.965338
803.866364	38.173574	70.970343
803.636710	25.600542	70.975348
802.917922	33.667817	70.980353
802.534644	40.388550	70.985358
801.705190	32.454320	70.990362
800.617354	41.203260	70.995367
800.390632	38.470212	71.000372
799.920177	34.560100	71.005377
799.072801	33.949139	71.010382
798.333550	27.135990	71.015386
797.454630	36.479316	71.020391
796.960410	25.776139	71.025396
796.570593	32.501065	71.030401
795.861369	36.059767	71.035406
795.010067	31.505366	71.040410
794.579969	35.976872	71.045415
794.073347	36.013431	71.050420
792.705171	42.074068	71.055425
791.896870	30.104096	71.060430
791.488189	32.544175	71.065434
791.018139	34.273338	71.070439
790.888286	30.610215	71.075444
789.844297	41.307653	71.080449
788.790986	34.495613	71.085454
788.265917	29.627500	71.090458
787.852302	37.078481	71.095463
787.481054	28.115657	71.100468
786.565131	28.476002	71.105473
785.849571	34.886923	71.110478
785.591699	31.610042	71.115482
784.408898	38.002303	71.120487
783.416642	32.437413	71.125492
782.941273	37.302491	71.130497
782.374204	32.196631	71.135502
782.470446	34.061155	71.140506
781.217438	37.045668	71.145511
780.757409	31.090115	71.150516
780.084513	40.533117	71.155521
778.951788	41.235494	71.160526
778.458104	29.821009	71.165530
777.389649	39.882085	71.170535
777.181531	35.075483	71.175540
776.572348	40.457042	71.180545
776.205427	34.912455	71.185550
775.375723	26.356943	71.190554
774.262305	35.089459	71.195559
773.847455	25.860761	71.200564
773.317957	28.409965	71.205569
772.767674	37.018140	71.210574
771.848194	35.469316	71.215578
770.814499	40.711871	71.220583
770.953380	30.075072	71.225588
770.315155	35.451792	71.230593
769.373976	35.784625	71.235598
768.731354	28.601279	71.240602
768.155298	32.236561	71.245607
767.282511	30.093664	71.250612
766.208544	33.125375	71.255617
765.455871	37.608813	71.260622
765.497436	26.758845	71.265626
764.965397	34.447882	71.270631
764.450987	21.633182	71.275636
763.316111	35.713552	71.280641
762.440152	30.357246	71.285646
762.244656	30.656525	71.290650
761.340134	40.051247	71.295655
760.440294	30.573323	71.300660
759.948636	39.765118	71.305665
759.575486	36.900841	71.310670
759.417663	34.718241	71.315674
758.284344	34.094468	71.320679
757.621408	31.711578	71.325684
756.607032	29.554956	71.330689
755.775809	32.164815	71.335694
754.930129	27.529109	71.340698
754.368290	38.247569	71.345703
754.414589	30.145549	71.350708
753.766058	35.123357	71.355713
753.227178	35.254949	71.360718
752.128225	33.504464	71.365722
751.198192	32.644898	71.370727
751.312111	33.748071	71.375732
749.906735	39.117618	71.380737
749.378856	34.390315	71.385742
748.961608	29.528702	71.390746
748.555349	42.136866	71.395751
747.519197	34.615621	71.400756
746.560152	37.439805	71.405761
745.888992	39.540048	71.410766
745.962191	38.441911	71.415770
744.633168	44.824353	71.420775
744.096607	31.570043	71.425780
743.220115	29.687948	71.430785
743.047964	44.280550	71.435790
742.900790	27.233078	71.440794
741.727379	41.037313	71.445799
740.936384	25.628339	71.450804
740.313131	42.644057	71.455809
739.653085	32.911914	71.460814
739.007174	30.300810	71.465818
738.077436	30.988233	71.470823
737.786960	24.523139	71.475828
736.920934	30.413961	71.480833
735.778445	26.595092	71.485838
734.945447	26.499118	71.490842
734.333938	35.063427	71.495847
733.999528	28.810336	71.500852
733.736161	37.106323	71.505857
733.370860	31.140431	71.510862
732.794530	27.971034	71.515866
731.594335	35.346974	71.520871
730.991195	31.872754	71.525876
730.872500	33.719455	71.530881
729.725605	23.006673	71.535886
729.145212	23.535974	71.540890
728.230197	34.266508	71.545895
727.885052	25.074035	71.550900
727.048197	35.856783	71.555905
726.064041	32.287105	71.560910
725.665934	32.022542	71.565914
725.115869	34.381060	71.570919
724.269402	36.184359	71.575924
723.374201	30.588274	71.580929
722.815466	28.111532	71.585934
722.623140	31.755114	71.590938
722.200038	32.164754	71.595943
721.080058	27.916519	71.600948
720.342344	39.254358	71.605953
719.668294	39.101542	71.610958
719.559826	30.429640	71.615962
718.326303	30.797999	71.620967
717.872206	16.792549	71.625972
716.946779	26.047096	71.630977
716.789187	30.410564	71.635982
715.586395	27.046018	71.640986
715.028529	36.324053	71.645991
714.670597	34.772576	71.650996
714.205687	41.511045	71.656001
713.117963	30.657955	71.661006
712.210875	26.437332	71.666010
711.586076	29.241424	71.671015
711.382320	29.762801	71.676020
710.773482	33.195151	71.681025
709.615088	28.375858	71.686030
709.299388	34.174334	71.691034
708.349505	33.439374	71.696039
708.289151	21.955922	71.701044
707.069321	32.116812	71.706049
706.209604	30.597923	71.711054
705.759825	34.916450	71.716058
705.287069	34.982329	71.721063
705.039040	31.902594	71.726068
704.105911	39.313297	71.731073
703.154375	39.896968	71.736078
702.864945	38.780875	71.741082
701.914059	45.211940	71.746087
701.179067	34.596011	71.751092
700.754173	35.960022	71.756097
699.897453	33.059210	71.761102
699.015642	35.319165	71.766106
697.938662	37.514000	71.771111
697.665649	27.661901	71.776116
697.086002	45.246284	71.781121
696.689263	40.554883	71.786126
696.618895	30.612167	71.791130
695.564598	36.911460	71.796135
694.954376	27.045246	71.801140
694.429082	39.181918	71.806145
693.492743	34.822450	71.811150
692.305013	28.165909	71.816154
691.526296	41.092008	71.821159
691.344081	30.101054	71.826164
691.046400	35.322637	71.831169
690.004169	32.705265	71.836174
689.520617	20.688368	71.841178
688.527053	37.359338	71.846183
688.174945	30.188108	71.851188
687.442664	34.176297	71.856193
686.394830	40.709537	71.861198
686.107949	32.064471	71.866202
685.450578	37.895277	71.871207
685.219545	36.400870	71.876212
683.709540	32.664201	71.881217
683.180533	36.230505	71.886222
682.889263	21.224552	71.891226
682.252496	30.582962	71.896231
681.669628	24.621765	71.901236
680.797455	29.193638	71.906241
680.197419	34.994813	71.911246
679.749973	29.704351	71.916250
678.665992	35.293998	71.921255
677.921211	31.017579	71.926260
677.123558	33.076478	71.931265
676.595301	38.643869	71.936270
676.502443	33.033585	71.941274
675.361881	41.311558	71.946279
675.108727	28.718640	71.951284
674.108705	41.068107	71.956289
673.623756	24.433997	71.961294
672.994317	27.092176	71.966298
672.162479	33.251970	71.971303
671.702856	21.032567	71.976308
671.097677	32.205798	71.981313
670.161167	34.543860	71.986318
669.755526	24.859550	71.991322
669.183567	30.968499	71.996327
668.796139	23.451233	72.001332
667.356706	33.331710	72.006337
666.471169	21.711578	72.011342
665.909161	30.742686	72.016346
665.700288	36.017940	72.021351
665.395756	32.485148	72.026356
664.022396	34.058547	72.031361
663.314488	35.407705	72.036366
662.937768	22.230483	72.041370
662.354040	33.815050	72.046375
661.995188	28.906309	72.051380
660.680645	26.964689	72.056385
659.994230	29.250312	72.061390
659.738609	29.119192	72.066394
659.115401	34.829441	72.071399
658.771978	25.773908	72.076404
657.836114	37.178004	72.081409
657.107629	29.457998	72.086414
656.670948	22.850618	72.091418
655.127740	35.180926	72.096423
654.963646	32.764362	72.101428
654.382523	31.152239	72.106433
653.909403	32.656404	72.111438
652.791847	32.392878	72.116442
651.955486	36.910173	72.121447
652.106158	36.752201	72.126452
651.532899	28.822970	72.131457
650.509149	32.750347	72.136462
649.892761	25.711103	72.141466
649.074539	34.384038	72.146471
648.736943	30.175254	72.151476
647.678996	32.638321	72.156481
646.681626	26.391473	72.161486
646.587007	30.298624	72.166490
645.853653	28.806944	72.171495
645.159291	30.847826	72.176500
644.193416	33.936490	72.181505
643.691466	32.685510	72.186510
643.298121	29.904899	72.191514
642.883762	27.972903	72.196519
641.970981	28.118329	72.201524
641.190433	26.889639	72.206529
640.489365	29.828898	72.211534
639.976445	24.145164	72.216538
638.361122	31.353854	72.221543
637.876614	29.740544	72.226548
637.399708	32.727687	72.231553
636.828572	31.593384	72.236558
636.824020	14.332425	72.241562
636.516472	24.143045	72.246567
635.762671	27.060740	72.251572
634.838954	35.171724	72.256577
633.989547	26.149465	72.261582
633.106964	23.396306	72.266586
631.991105	31.353380	72.271591
631.675284	20.246524	72.276596
631.234951	25.492402	72.281601
630.888145	26.626361	72.286606
630.224339	19.671951	72.291610
629.146434	27.176690	72.296615
629.194439	13.957079	72.301620
628.067324	27.239865	72.306625
626.856813	24.966297	72.311630
626.317263	25.001826	72.316634
625.447770	27.280343	72.321639
625.449163	25.184366	72.326644
625.107105	30.922387	72.331649
624.238592	31.108080	72.336654
623.449555	26.159046	72.341658
622.765131	38.103440	72.346663
622.209796	24.274991	72.351668
620.952593	32.708753	72.356673
620.227955	31.231462	72.361678
620.033234	33.760495	72.366682
619.318137	27.131229	72.371687
619.350369	25.410395	72.376692
617.929211	27.589110	72.381697
617.090563	34.030708	72.386702
617.088226	28.290896	72.391706
616.092260	27.689470	72.396711
615.049537	26.056253	72.401716
614.575891	38.476449	72.406721
613.765698	37.157868	72.411726
613.620904	25.405595	72.416730
612.762592	30.074631	72.421735
611.832983	23.175174	72.426740
611.442307	33.221395	72.431745
610.833724	31.974789	72.436750
610.646358	26.477339	72.441754
609.340300	38.446620	72.446759
608.678639	27.161450	72.451764
607.870483	35.203572	72.456769
607.693690	32.902578	72.461774
607.260720	26.488588	72.466778
605.719793	37.433960	72.471783
605.379298	35.299390	72.476788
605.052319	35.616467	72.481793
604.640440	33.199946	72.486798
603.883885	26.301314	72.491802
602.742516	40.422196	72.496807
602.363145	27.180754	72.501812
601.170084	31.652367	72.506817
600.398721	28.009429	72.511822
600.207018	24.767771	72.516826
599.690926	30.315886	72.521831
599.428980	29.402015	72.526836
597.961310	34.204379	72.531841
597.132610	33.811293	72.536846
596.904337	31.456996	72.541850
596.176230	32.329983	72.546855
596.083722	27.514458	72.551860
595.107041	32.003652	72.556865
594.079527	32.970058	72.561870
593.969658	22.860184	72.566874
592.463114	27.787015	72.571879
591.950049	31.890126	72.576884
591.249482	28.871444	72.581889
590.825267	28.478594	72.586894
590.504699	29.048548	72.591898
590.313868	36.279553	72.596903
589.259867	27.244167	72.601908
588.479191	29.139534	72.606913
587.580669	37.965628	72.611918
586.701990	28.509647	72.616922
585.813605	39.962973	72.621927
585.392271	32.132569	72.626932
584.644981	31.803793	72.631937
584.648012	29.704401	72.636942
584.535079	32.303990	72.641946
583.202294	34.336182	72.646951
582.341584	21.860561	72.651956
582.052440	31.848033	72.656961
580.753081	33.457000	72.661966
580.304699	29.458267	72.666970
579.756609	27.219568	72.671975
579.348790	29.918166	72.676980
578.897284	33.137821	72.681985
578.000538	27.597240	72.686990
577.440397	35.577789	72.691994
576.010874	33.118350	72.696999
575.329283	37.406007	72.702004
574.826399	32.993321	72.707009
574.196102	33.915393	72.712014
574.130762	35.043954	72.717018
573.163001	33.687404	72.722023
572.621474	24.646099	72.727028
571.646611	40.880446	72.732033
571.190161	39.239025	72.737038
571.193454	34.264734	72.742042
570.021630	41.038543	72.747047
569.050064	23.188848	72.752052
568.690031	33.449392	72.757057
568.119109	38.616732	72.762062
566.971541	35.937342	72.767066
565.688070	37.848146	72.772071
565.843500	29.720873	72.777076
565.425560	34.187315	72.782081
564.652343	33.037908	72.787086
563.993560	35.065259	72.792090
563.232487	39.688862	72.797095
562.773089	36.362108	72.802100
561.800050	33.210210	72.807105
560.930824	40.656509	72.812110
560.667190	31.881607	72.817114
559.959751	41.375881	72.822119
559.546493	25.146720	72.827124
558.263152	33.160460	72.832129
557.572122	37.634133	72.837134
557.161362	33.738224	72.842138
556.682751	31.676125	72.847143
556.652588	33.412533	72.852148
555.429606	39.834942	72.857153
554.462834	32.842074	72.862158
554.496163	31.294534	72.867162
552.960349	39.719089	72.872167
552.256040	31.522173	72.877172
551.478071	35.207006	72.882177
551.323705	26.911456	72.887182
551.172387	21.431930	72.892186
549.897233	32.025902	72.897191
549.006258	36.610274	72.902196
548.625611	35.442496	72.907201
548.247549	42.127726	72.912206
547.806127	36.416853	72.917210
546.744431	40.776103	72.922215
546.146200	32.330474	72.927220
545.570147	39.838890	72.932225
544.402219	34.844577	72.937230
543.754378	27.253699	72.942234
542.950913	43.627914	72.947239
542.740455	33.619222	72.952244
542.030744	34.306363	72.957249
541.995525	33.178183	72.962254
540.827589	28.242224	72.967258
540.201207	34.616914	72.972263
539.916455	18.260063	72.977268
538.642440	34.098927	72.982273
538.002580	32.418918	72.987278
537.618782	34.832991	72.992282
536.668560	28.348443	72.997287
536.315754	31.501919	73.002292
535.664111	34.684074	73.007297
534.638170	37.036429	73.012302
534.471246	34.172461	73.017306
533.477380	38.106160	73.022311
532.821830	28.647778	73.027316
532.070387	33.186273	73.032321
531.586966	32.351845	73.037326
531.412324	28.180205	73.042330
529.722667	37.837252	73.047335
529.112166	31.374286	73.052340
528.995786	28.735662	73.057345
528.320425	23.934140	73.062350
528.005424	28.056173	73.067354
527.108050	30.164118	73.072359
526.376836	27.014717	73.077364
525.793833	31.551613	73.082369
524.411117	28.968053	73.087374
523.958641	21.543187	73.092378
523.159949	29.620090	73.097383
523.125240	32.060559	73.102388
522.610303	32.577903	73.107393
521.860602	33.321884	73.112398
520.727640	21.482611	73.117402
520.208576	31.982960	73.122407
519.835675	22.914810	73.127412
518.776032	30.681615	73.132417
517.797829	29.635842	73.137422
517.589523	31.908418	73.142426
517.148123	34.986121	73.147431
516.944913	22.727498	73.152436
515.961941	33.260747	73.157441
514.591965	30.722472	73.162446
514.290362	28.214283	73.167450
513.765923	28.936575	73.172455
512.884816	26.353541	73.177460
511.982932	28.632524	73.182465
511.319674	32.868387	73.187470
511.838775	21.674288	73.192474
510.722674	32.097856	73.197479
509.489343	28.809247	73.202484
508.939846	35.323086	73.207489
508.281480	36.503540	73.212494
508.155117	26.106139	73.217498
507.010414	27.895514	73.222503
506.357142	22.609499	73.227508
505.957477	39.289980	73.232513
505.019859	36.954076	73.237518
503.918734	27.864739	73.242522
502.976871	27.027653	73.247527
502.791120	16.833690	73.252532
502.507857	26.208350	73.257537
502.108625	23.053381	73.262542
501.786837	23.926322	73.267546
500.835219	23.650624	73.272551
500.177957	23.835823	73.277556
499.209957	22.391032	73.282561
498.147823	26.122723	73.287566
497.828539	18.263476	73.292570
496.992020	35.584417	73.297575
496.812401	29.115899	73.302580
495.577149	35.737410	73.307585
494.931048	23.383763	73.312590
494.422108	23.024928	73.317594
493.812602	29.534134	73.322599
493.476252	24.637614	73.327604
492.851922	33.800103	73.332609
491.576348	25.411940	73.337614
491.550795	26.376465	73.342618
490.642522	33.594028	73.347623
490.313779	19.660147	73.352628
489.159543	35.498872	73.357633
488.497191	29.239727	73.362638
488.408888	31.169904	73.367642
487.219734	37.404020	73.372647
486.680610	27.717368	73.377652
486.101481	28.497265	73.382657
485.076805	30.111406	73.387662
484.563530	25.850215	73.392666
483.684121	37.696379	73.397671
483.559729	26.825570	73.402676
483.038603	28.895666	73.407681
481.980676	28.299435	73.412686
481.399999	24.645085	73.417690
480.453869	29.887983	73.422695
480.270118	21.664939	73.427700
478.876792	33.995108	73.432705
478.139029	29.394358	73.437710
478.173375	29.374760	73.442714
477.415664	36.431144	73.447719
476.887230	32.894629	73.452724
476.241587	31.125671	73.457729
475.144079	30.529440	73.462734
474.670860	28.780322	73.467738
474.209572	36.196344	73.472743
473.916567	23.892110	73.477748
472.895200	21.869191	73.482753
472.247560	31.204133	73.487758
471.426005	15.562046	73.492762
470.234298	28.982909	73.497767
469.722409	17.134609	73.502772
469.275955	26.243526	73.507777
468.830981	31.873373	73.512782
468.518427	15.159845	73.517786
467.090683	32.768950	73.522791
466.972479	29.261701	73.527796
466.242860	35.323262	73.532801
465.173187	42.197535	73.537806
464.598472	30.854411	73.542810
463.905137	31.483770	73.547815
463.640504	32.558926	73.552820
463.406493	31.189601	73.557825
462.119351	32.080728	73.562830
461.772571	27.629009	73.567834
460.986388	30.296439	73.572839
460.533046	30.695170	73.577844
459.411800	35.303641	73.582849
458.674392	32.182057	73.587854
458.200183	27.067804	73.592858
457.662946	27.076193	73.597863
456.661557	20.345942	73.602868
455.686041	28.898897	73.607873
455.185276	25.039430	73.612878
454.996608	26.794781	73.617882
454.285494	33.387995	73.622887
454.026330	32.396425	73.627892
452.816555	36.899153	73.632897
451.997699	32.202519	73.637902
451.669409	28.867518	73.642906
451.142071	33.105393	73.647911
450.031318	32.454513	73.652916
449.273263	40.886095	73.657921
448.800308	33.920256	73.662926
448.862424	32.048001	73.667930
447.982120	34.452882	73.672935
446.936155	29.760896	73.677940
446.449004	31.937552	73.682945
445.540699	28.513611	73.687950
444.957781	29.726216	73.692954
444.040670	33.469517	73.697959
443.911661	24.700002	73.702964
443.586670	31.870377	73.707969
442.243177	30.532745	73.712974
441.451245	32.795811	73.717978
440.958182	31.581306	73.722983
440.588293	18.901395	73.727988
440.000743	29.639748	73.732993
438.701764	28.992054	73.737998
438.331163	21.112610	73.743002
437.974523	31.074565	73.748007
437.202832	24.369226	73.753012
436.216832	31.685923	73.758017
435.571253	36.918798	73.763022
435.132100	25.229229	73.768026
434.539733	36.493492	73.773031
433.766174	27.077605	73.778036
433.079685	29.330181	73.783041
432.511901	26.258852	73.788046
432.153343	31.103787	73.793050
430.856903	33.529245	73.798055
430.190864	30.192868	73.803060
429.661429	34.019487	73.808065
429.388930	31.022537	73.813070
428.850667	29.044090	73.818074
427.375439	35.054147	73.823079
426.952990	31.514951	73.828084
426.634520	42.480105	73.833089
426.103885	38.861949	73.838094
425.284412	29.153753	73.843098
424.159643	38.299797	73.848103
423.668649	23.524440	73.853108
423.748457	43.099571	73.858113
422.458450	31.567652	73.863118
422.043390	29.851856	73.868122
421.206329	41.259195	73.873127
420.660294	30.684242	73.878132
419.457805	38.207334	73.883137
418.813524	31.693014	73.888142
418.435895	32.070226	73.893146
417.957473	39.739728	73.898151
417.748914	30.248012	73.903156
416.627861	37.570467	73.908161
415.484745	36.872719	73.913166
415.477535	31.723488	73.918170
414.756023	38.911317	73.923175
414.027112	39.987916	73.928180
412.938890	38.453502	73.933185
412.366169	37.420434	73.938190
412.031488	34.632095	73.943194
411.505423	44.597403	73.948199
410.908104	27.008292	73.953204
409.874030	40.000358	73.958209
409.223537	29.971922	73.963214
409.299913	27.506025	73.968218
407.679630	37.658301	73.973223
407.036124	28.816226	73.978228
406.845127	26.774565	73.983233
406.122741	40.923363	73.988238
405.665181	31.280510	73.993242
404.469595	32.876184	73.998247
403.799484	35.285433	74.003252
403.566791	27.125393	74.008257
402.418968	34.963062	74.013262
401.615857	27.906342	74.018266
400.966815	29.970027	74.023271
400.658671	27.853991	74.028276
400.260816	26.777292	74.033281
399.616971	33.971670	74.038286
399.320315	24.973404	74.043290
398.267499	34.939062	74.048295
397.897920	36.816289	74.053300
397.013641	27.178358	74.058305
396.198846	32.922339	74.063310
395.799346	35.595982	74.068314
394.694516	35.313198	74.073319
393.954090	33.581444	74.078324
393.247123	26.326477	74.083329
392.801514	28.340400	74.088334
392.700349	29.432094	74.093338
391.242269	35.417359	74.098343
390.855483	33.697063	74.103348
390.079947	36.315509	74.108353
389.622145	33.308668	74.113358
388.886268	30.294099	74.118362
387.918168	35.143128	74.123367
387.200137	32.944172	74.128372
386.871435	39.134259	74.133377
386.515590	36.954860	74.138382
385.773490	29.164586	74.143386
384.711470	35.290173	74.148391
384.232903	32.220409	74.153396
384.072510	34.589440	74.158401
383.053710	35.880980	74.163406
382.559353	26.428508	74.168410
381.245659	32.198377	74.173415
380.899278	28.694379	74.178420
379.554091	32.712503	74.183425
379.020082	27.680341	74.188430
378.852385	21.328218	74.193434
378.210115	33.092457	74.198439
378.049068	28.420340	74.203444
377.525549	33.487115	74.208449
376.178571	29.751476	74.213454
375.713255	32.014553	74.218458
375.023517	39.629423	74.223463
374.114100	33.660427	74.228468
373.329131	25.970033	74.233473
372.705223	34.077468	74.238478
372.514674	26.483165	74.243482
371.894503	30.171284	74.248487
371.199104	31.545336	74.253492
370.343284	32.870834	74.258497
369.294040	30.336727	74.263502
369.439358	28.544256	74.268506
368.363850	36.121251	74.273511
367.694858	28.442339	74.278516
366.978840	42.531780	74.283521
366.418862	39.186404	74.288526
366.087136	29.618130	74.293530
364.784942	42.946258	74.298535
364.027480	31.394167	74.303540
363.820425	26.557493	74.308545
363.118359	32.527951	74.313550
362.713822	28.752520	74.318554
361.477641	34.896409	74.323559
361.148911	26.374781	74.328564
360.527109	30.757038	74.333569
359.912155	42.706172	74.338574
359.078072	27.285328	74.343578
358.407654	34.826154	74.348583
357.847592	35.992558	74.353588
357.617232	31.840856	74.358593
356.393935	29.049058	74.363598
355.762018	28.995285	74.368602
355.180036	29.988559	74.373607
354.583646	24.362360	74.378612
353.630880	26.138562	74.383617
353.064295	31.649028	74.388622
352.731986	25.488724	74.393626
351.950187	25.553457	74.398631
350.996645	28.533025	74.403636
350.623702	23.949876	74.408641
349.922272	29.678956	74.413646
349.558788	20.044789	74.418650
348.368281	34.481085	74.423655
347.788388	28.645672	74.428660
347.265530	31.028313	74.433665
346.399513	36.897169	74.438670
346.447652	32.011941	74.443674
345.268692	28.993882	74.448679
344.424688	24.413266	74.453684
344.222429	30.291458	74.458689
343.238403	32.534702	74.463694
342.696828	28.049394	74.468698
341.931908	36.026341	74.473703
341.446939	20.001083	74.478708
340.478913	35.759711	74.483713
339.365215	29.183032	74.488718
338.860213	23.114910	74.493722
338.297378	24.892052	74.498727
338.665217	26.057238	74.503732
338.066645	26.321438	74.508737
336.698517	24.918404	74.513742
336.230787	24.857393	74.518746
335.455592	36.086148	74.523751
334.276043	24.826854	74.528756
333.902290	30.199356	74.533761
333.088653	34.139096	74.538766
332.754254	26.891007	74.543770
332.112784	19.832213	74.548775
331.347646	22.661908	74.553780
330.594834	29.086747	74.558785
329.486050	28.173828	74.563790
329.785884	27.206725	74.568794
329.133026	33.095230	74.573799
328.439119	26.973636	74.578804
327.597851	36.959220	74.583809
326.553513	29.963053	74.588814
325.424288	24.204161	74.593818
324.943712	32.533192	74.598823
324.562167	24.395314	74.603828
324.277231	19.536367	74.608833
323.775186	26.389604	74.613838
323.384883	24.723499	74.618842
322.089555	28.880364	74.623847
321.339974	21.211162	74.628852
321.093169	24.138026	74.633857
320.379108	32.535810	74.638862
319.529888	24.343158	74.643866
318.861450	29.175989	74.648871
318.143858	28.101378	74.653876
317.350400	28.197943	74.658881
316.507582	32.596511	74.663886
315.858807	24.356144	74.668890
315.474989	35.777997	74.673895
315.376616	24.068846	74.678900
314.771924	23.247483	74.683905
313.280425	33.511748	74.688910
312.815155	24.898351	74.693914
312.665312	27.486480	74.698919
311.614173	28.496191	74.703924
310.862521	26.524974	74.708929
310.349875	34.054856	74.713934
310.003077	20.945514	74.718938
308.622194	26.927978	74.723943
308.112865	21.407769	74.728948
307.525766	26.751197	74.733953
307.321003	24.137717	74.738958
306.544493	21.530208	74.743962
305.524303	24.567723	74.748967
305.208317	17.349826	74.753972
304.288609	24.589762	74.758977
303.232815	22.239661	74.763982
302.632970	22.194983	74.768986
302.205546	18.743344	74.773991
301.863210	15.599849	74.778996
301.500276	19.552916	74.784001
300.574578	24.776844	74.789006
299.731582	15.999729	74.794010
299.452310	21.186857	74.799015
297.988066	14.520996	74.804020
297.340629	30.356265	74.809025
296.675608	23.375353	74.814030
296.330650	16.805487	74.819034
295.885518	21.049206	74.824039
295.234982	27.374170	74.829044
294.615213	22.947072	74.834049
293.688176	17.286862	74.839054
293.373533	15.495161	74.844058
291.995319	22.636290	74.849063
291.479514	19.602448	74.854068
291.141130	22.258476	74.859073
290.593155	24.075838	74.864078
289.985093	18.636029	74.869082
288.750395	32.803414	74.874087
288.106114	26.610845	74.879092
287.836962	23.301141	74.884097
287.252421	21.809509	74.889102
286.914463	23.836252	74.894106
285.638694	22.995703	74.899111
285.057591	28.672501	74.904116
284.650381	21.880740	74.909121
283.738280	23.987960	74.914126
283.616101	15.619518	74.919130
282.638391	18.229214	74.924135
281.806119	20.574451	74.929140
280.902604	20.210744	74.934145
280.079790	15.040140	74.939150
279.779198	19.826960	74.944154
278.827765	18.519970	74.949159
278.763017	23.291275	74.954164
278.266756	17.305359	74.959169
276.970118	21.005127	74.964174
276.725534	18.215069	74.969178
276.092249	16.467853	74.974183
275.564762	16.389571	74.979188
274.172080	12.959332	74.984193
273.598783	21.721042	74.989198
273.469882	17.988432	74.994202
272.862053	17.257468	74.999207
272.025455	18.210920	75.004212
271.153074	9.099454	75.009217
270.399972	24.500545	75.014222
270.283362	15.749586	75.019226
269.166466	16.127962	75.024231
268.133216	27.013074	75.029236
267.542457	17.143916	75.034241
267.317360	23.798469	75.039246
267.119110	15.737051	75.044250
266.352632	27.330284	75.049255
265.428645	21.051420	75.054260
264.946772	19.920328	75.059265
264.173913	20.802119	75.064270
263.412779	15.669000	75.069274
262.554533	19.221621	75.074279
262.031881	18.079683	75.079284
261.644997	21.391586	75.084289
260.589443	29.687694	75.089294
259.787847	18.518016	75.094298
258.925329	27.959783	75.099303
258.895374	18.969502	75.104308
258.395176	15.349697	75.109313
257.172151	25.241599	75.114318
256.702037	19.317753	75.119322
256.273735	18.652796	75.124327
255.793302	20.951417	75.129332
254.506510	21.801593	75.134337
253.587209	21.525570	75.139342
253.340751	16.695195	75.144346
252.799931	30.152728	75.149351
252.666165	20.224918	75.154356
251.895487	20.379376	75.159361
250.763298	24.997557	75.164366
250.366376	15.755110	75.169370
249.206643	29.986252	75.174375
248.264492	19.266347	75.179380
248.179805	23.365881	75.184385
247.623133	25.025363	75.189390
247.239705	20.691495	75.194394
246.005381	20.043060	75.199399
245.058374	24.749998	75.204404
244.572757	30.017335	75.209409
244.186040	30.061702	75.214414
243.953990	24.440537	75.219418
242.690818	31.080797	75.224423
241.715673	28.396162	75.229428
241.770780	33.295023	75.234433
240.956395	29.930311	75.239438
240.898201	17.998726	75.244442
239.738278	22.750645	75.249447
238.789716	20.608988	75.254452
238.575234	18.665708	75.259457
237.241116	28.431823	75.264462
236.628306	18.807469	75.269466
236.112715	26.894502	75.274471
235.935967	21.551534	75.279476
235.180039	23.603912	75.284481
234.277982	25.826245	75.289486
233.822498	17.632370	75.294490
232.812077	25.233725	75.299495
232.330695	26.622583	75.304500
231.486075	24.658328	75.309505
230.766816	29.898257	75.314510
230.577234	19.291784	75.319514
229.950469	26.532353	75.324519
229.024379	21.963292	75.329524
228.073528	12.279292	75.334529
227.672292	15.855265	75.339534
227.387494	21.603107	75.344538
226.016614	30.383166	75.349543
225.308546	32.304914	75.354548
225.153308	22.818932	75.359553
224.524138	30.651256	75.364558
224.195712	29.593483	75.369562
223.240082	28.438574	75.374567
222.521268	27.509269	75.379572
222.043113	22.827800	75.384577
220.812546	32.282521	75.389582
220.060836	29.306803	75.394586
219.387865	33.713017	75.399591
219.418672	25.982522	75.404596
218.718017	24.140404	75.409601
217.642359	28.795320	75.414606
217.387245	20.496964	75.419610
216.427867	30.654365	75.424615
216.011042	28.858464	75.429620
214.968307	23.210423	75.434625
214.017776	32.347684	75.439630
214.097671	15.120654	75.444634
213.653132	18.252515	75.449639
212.762902	11.422661	75.454644
211.869398	13.269892	75.459649
210.998907	18.567048	75.464654
210.689791	21.667859	75.469658
209.293569	27.701704	75.474663
208.695318	14.129427	75.479668
208.673929	18.748734	75.484673
208.055118	27.065119	75.489678
207.790136	19.533175	75.494682
206.328157	20.204720	75.499687
205.647038	23.465765	75.504692
205.369268	22.959748	75.509697
204.658609	17.231965	75.514702
203.894277	14.363926	75.519706
203.068521	23.011351	75.524711
202.677113	28.489183	75.529716
202.425380	23.760582	75.534721
201.111386	23.342496	75.539726
200.371499	22.391326	75.544730
200.001555	29.958395	75.549735
199.593378	30.583366	75.554740
198.424745	24.351419	75.559745
198.009891	30.776027	75.564750
197.818241	27.699988	75.569754
196.726261	26.445401	75.574759
195.704600	21.219796	75.579764
194.856426	26.221660	75.584769
194.055982	23.785166	75.589774
194.009121	23.136678	75.594778
193.962684	32.349006	75.599783
192.978818	24.256726	75.604788
192.136505	23.493780	75.609793
191.244085	20.814902	75.614798
191.127050	15.905555	75.619802
189.702312	27.763025	75.624807
189.088750	18.988803	75.629812
188.759626	26.533592	75.634817
187.910001	29.474572	75.639822
187.828037	19.620518	75.644826
186.424733	23.764699	75.649831
185.801356	22.471677	75.654836
185.395417	21.623391	75.659841
184.869766	19.297633	75.664846
184.439509	20.703580	75.669850
183.355346	26.919501	75.674855
182.596138	20.176002	75.679860
182.215447	14.447660	75.684865
181.374675	22.570772	75.689870
180.808311	12.767146	75.694874
179.852806	26.711850	75.699879
179.417695	24.377966	75.704884
179.458926	19.373998	75.709889
178.195631	25.255775	75.714894
177.778005	19.910219	75.719898
177.102280	18.922019	75.724903
175.760691	16.209105	75.729908
175.094579	15.496921	75.734913
174.320764	29.721750	75.739918
174.335656	21.381929	75.744922
173.614372	26.440840	75.749927
173.394042	18.690468	75.754932
172.137281	24.640593	75.759937
171.278942	23.646816	75.764942
171.054532	20.848823	75.769946
170.327654	25.761967	75.774951
169.411697	30.549138	75.779956
168.968441	24.546913	75.784961
168.534037	27.371232	75.789966
167.977385	21.464361	75.794970
166.485639	22.796700	75.799975
166.203377	21.189092	75.804980
165.696368	29.027180	75.809985
164.869222	29.012469	75.814990
164.116060	23.149546	75.819994
163.471239	31.031686	75.824999
162.803423	25.580940	75.830004
162.719004	29.352419	75.835009
161.847548	27.323081	75.840014
161.143381	26.312610	75.845018
160.110303	30.763637	75.850023
159.600869	21.310488	75.855028
159.265235	28.943052	75.860033
157.924195	18.255255	75.865038
157.260175	19.446161	75.870042
156.730422	22.266760	75.875047
156.391709	35.810353	75.880052
156.335866	25.939518	75.885057
155.212437	32.694734	75.890062
154.722405	30.931017	75.895066
153.987758	34.159611	75.900071
152.839469	31.671357	75.905076
152.115145	27.921728	75.910081
151.412177	28.875991	75.915086
151.110795	11.818580	75.920090
150.681520	20.544727	75.925095
149.381779	19.056779	75.930100
148.973636	24.184039	75.935105
148.197455	23.688112	75.940110
148.251441	22.815384	75.945114
147.384236	35.484439	75.950119
146.484866	24.021309	75.955124
145.859595	23.405125	75.960129
145.310935	25.295168	75.965134
144.466092	10.287760	75.970138
143.562690	33.372244	75.975143
142.934540	23.553244	75.980148
142.774455	27.119164	75.985153
141.815067	28.822381	75.990158
140.753728	19.499819	75.995162
140.065627	26.426902	76.000167
139.754179	24.659946	76.005172
139.528323	27.837376	76.010177
138.682179	21.032061	76.015182
138.051512	20.001993	76.020186
136.872290	23.828190	76.025191
136.420227	27.628328	76.030196
136.308721	18.121199	76.035201
134.938215	25.253290	76.040206
134.343384	18.120894	76.045210
133.702335	24.206251	76.050215
133.624997	22.217459	76.055220
132.789528	22.759184	76.060225
131.453241	23.797091	76.065230
131.335710	14.779790	76.070234
130.902322	27.362320	76.075239
129.764814	27.362416	76.080244
128.986194	18.379564	76.085249
128.389953	31.948448	76.090254
128.262389	18.376840	76.095258
127.664056	30.181413	76.100263
126.871593	24.900369	76.105268
126.067714	17.162632	76.110273
125.446479	26.630613	76.115278
124.885715	22.285623	76.120282
123.908001	32.188927	76.125287
123.227585	25.131681	76.130292
123.206732	22.782214	76.135297
121.903163	18.848992	76.140302
121.356518	20.301893	76.145306
120.757379	17.319230	76.150311
120.203340	23.808615	76.155316
119.103988	15.531361	76.160321
117.866936	18.313363	76.165326
117.914252	12.709176	76.170330
117.428500	23.190052	76.175335
117.111853	20.734787	76.180340
116.472059	20.102003	76.185345
115.160136	26.455195	76.190350
114.755309	19.303545	76.195354
114.367029	26.600724	76.200359
113.148517	26.057070	76.205364
112.749451	26.239047	76.210369
111.908162	33.326188	76.215374
111.734989	27.140556	76.220378
110.886237	24.550942	76.225383
109.969285	19.105251	76.230388
109.324117	20.491863	76.235393
108.360488	27.746747	76.240398
108.871759	29.215458	76.245402
107.429116	18.878217	76.250407
106.511070	29.943707	76.255412
106.054579	20.847992	76.260417
105.555240	30.987259	76.265422
105.363915	16.506444	76.270426
104.159673	25.334101	76.275431
103.433246	26.400930	76.280436
103.139542	18.868856	76.285441
101.900865	25.569926	76.290446
101.404049	14.622962	76.295450
100.557653	28.318471	76.300455
100.293961	23.479827	76.305460
99.979258	21.845862	76.310465
98.616265	24.324677	76.315470
98.043714	20.721179	76.320474
97.628913	25.057861	76.325479
97.151949	18.627362	76.330484
96.797722	15.151479	76.335489
95.249043	24.912445	76.340494
95.136925	15.151527	76.345498
94.182258	23.797459	76.350503
93.080514	14.528679	76.355508
92.450345	21.709887	76.360513
91.945216	24.644846	76.365518
91.564531	14.359044	76.370522
91.290663	20.026301	76.375527
90.664056	21.823127	76.380532
89.777603	24.702200	76.385537
88.840743	26.179490	76.390542
88.863978	22.476251	76.395546
87.668855	16.474101	76.400551
86.805238	19.352686	76.405556
86.283989	17.112985	76.410561
85.664995	18.522237	76.415566
85.281731	7.232317	76.420570
84.333817	19.332336	76.425575
83.834956	20.224105	76.430580
83.251965	22.657385	76.435585
82.212715	29.952724	76.440590
81.563791	16.241917	76.445594
80.650027	23.553512	76.450599
80.163871	15.093332	76.455604
79.877493	16.291842	76.460609
79.428817	22.654042	76.465614
78.410550	17.953088	76.470618
77.941011	12.724649	76.475623
77.567620	18.608054	76.480628
76.451440	17.838361	76.485633
75.322242	24.460481	76.490638
75.147655	24.193495	76.495642
74.378190	26.511434	76.500647
74.200037	16.835168	76.505652
73.257255	21.274978	76.510657
72.231320	29.498616	76.515662
71.862359	18.818279	76.520666
70.858669	11.869384	76.525671
70.203221	15.534805	76.530676
69.688108	16.441784	76.535681
68.992034	18.711748	76.540686
68.925890	12.163701	76.545690
67.867986	25.667437	76.550695
67.018085	20.300959	76.555700
66.608080	17.513655	76.560705
66.203657	21.083849	76.565710
65.484495	13.922420	76.570714
64.014037	20.510656	76.575719
63.574476	21.784062	76.580724
63.103466	11.454328	76.585729
62.486632	23.329663	76.590734
62.303599	14.899994	76.595738
60.961929	18.977640	76.600743
60.495584	17.642260	76.605748
60.225081	14.602471	76.610753
59.369942	27.119800	76.615758
58.487909	24.847756	76.620762
57.945314	24.256257	76.625767
57.505071	25.357882	76.630772
57.204229	21.389357	76.635777
55.733600	32.076205	76.640782
55.284697	25.325842	76.645786
54.728872	28.753026	76.650791
53.792634	24.718678	76.655796
53.178159	7.162448	76.660801
52.517686	29.681482	76.665806
52.064657	23.026398	76.670810
51.653296	26.066259	76.675815
50.586573	23.511432	76.680820
49.892926	17.315781	76.685825
49.428347	31.877672	76.690830
49.034839	18.988749	76.695834
47.803100	22.097950	76.700839
46.969448	21.928196	76.705844
46.858026	21.051885	76.710849
46.146273	20.102584	76.715854
46.109066	15.396567	76.720858
44.974929	24.949516	76.725863
44.118258	21.421310	76.730868
43.552650	13.820652	76.735873
42.129764	25.217413	76.740878
41.724743	14.993855	76.745882
40.815278	14.963930	76.750887
40.619705	20.642357	76.755892
40.240891	20.087819	76.760897
39.830944	22.274309	76.765902
39.129340	19.579251	76.770906
38.215293	22.815986	76.775911
37.623670	20.114426	76.780916
36.599209	22.808943	76.785921
35.763041	33.960745	76.790926
35.452729	27.136241	76.795930
35.036832	27.251528	76.800935
34.391886	30.077908	76.805940
33.606126	29.050526	76.810945
32.743863	34.103573	76.815950
32.727160	23.021700	76.820954
31.683621	26.294861	76.825959
31.064569	20.765419	76.830964
30.409136	30.871241	76.835969
29.014000	27.581890	76.840974
28.431516	29.605087	76.845978
27.555057	31.536399	76.850983
27.043906	26.685195	76.855988
26.663560	34.679722	76.860993
26.285489	36.761782	76.865998
26.292867	18.813047	76.871002
25.367591	31.791013	76.876007
24.561312	34.783480	76.881012
24.071664	24.519800	76.886017
22.532792	35.490369	76.891022
22.117571	30.939261	76.896026
21.305442	36.654533	76.901031
21.370101	28.172740	76.906036
20.468319	26.583540	76.911041
19.299745	33.107884	76.916046
18.944184	34.432557	76.921050
18.357699	37.648594	76.926055
17.720569	36.157533	76.931060
16.944752	17.745508	76.936065
15.840758	37.526695	76.941070
15.623666	25.270394	76.946074
14.975057	26.384762	76.951079
14.397241	32.532600	76.956084
14.204789	29.838340	76.961089
13.231421	36.833033	76.966094
12.643262	35.219042	76.971098
11.283143	35.915457	76.976103
10.369151	29.482143	76.981108
10.232526	26.119801	76.986113
9.708723	35.603803	76.991118
9.812250	26.218510	76.996122
8.488157	30.367499	77.001127
7.514495	39.104807	77.006132
6.957982	30.299464	77.011137
6.261371	30.170944	77.016142
6.220109	21.756514	77.021147
5.155204	21.931172	77.026151
4.506643	30.451036	77.031156
4.033989	25.398153	77.036161