Fri Mar 05 18:22:32 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-0.941863	98.690026	0.000000
-1.619122	85.641358	0.005005
-1.958551	50.554108	0.010010
-4.013672	21.572270	0.015014
-8.320849	-10.183734	0.020019
-13.737557	-15.010919	0.025024
-18.904448	-13.120609	0.030029
-23.284574	-15.039599	0.035034
-27.086915	-12.638375	0.040038
-31.401823	-15.518668	0.045043
-35.089497	-21.219287	0.050048
-38.629163	-15.428455	0.055053
-41.917107	-22.096434	0.060058
-45.857466	-13.289579	0.065062
-49.624725	-17.439932	0.070067
-53.218245	-17.038465	0.075072
-56.994232	-10.118641	0.080077
-60.799864	-19.785413	0.085082
-64.853855	-16.785738	0.090086
-68.822932	-15.240955	0.095091
-71.825216	-26.932963	0.100096
-75.787387	-12.109589	0.105101
-79.497206	-19.399348	0.110106
-83.359373	-15.186014	0.115110
-87.495983	-20.371798	0.120115
-90.852941	-22.994801	0.125120
-95.030029	-10.885770	0.130125
-98.329421	-16.604084	0.135130
-102.221424	-10.747486	0.140134
-105.791532	-12.861794	0.145139
-109.615523	-18.496392	0.150144
-113.679911	-13.533224	0.155149
-117.514097	-20.637496	0.160154
-121.245957	-13.734080	0.165158
-125.012451	-8.435219	0.170163
-128.447575	-20.624225	0.175168
-132.196882	-11.475555	0.180173
-135.786578	-25.838180	0.185178
-139.952706	-24.517310	0.190182
-144.111929	-16.206823	0.195187
-148.115419	-18.119449	0.200192
-152.018229	-10.949009	0.205197
-154.864275	-17.446064	0.210202
-158.884895	-12.633311	0.215206
-162.855058	-5.220291	0.220211
-166.245515	-17.066280	0.225216
-170.378104	-4.741872	0.230221
-173.776555	-14.042922	0.235226
-177.244426	-6.749457	0.240230
-181.059616	-11.529049	0.245235
-184.507528	-8.315230	0.250240
-188.813606	-3.332292	0.255245
-192.566815	-25.134113	0.260250
-196.569535	-11.228193	0.265254
-200.861623	-7.140033	0.270259
-203.993072	-16.967775	0.275264
-207.772657	-14.170930	0.280269
-211.160986	-11.491715	0.285274
-215.090929	-12.159121	0.290278
-219.033882	-11.413056	0.295283
-222.487149	-4.757379	0.300288
-226.473879	-5.097156	0.305293
-230.059049	-6.453506	0.310298
-233.960233	-11.667146	0.315302
-237.940324	-15.388987	0.320307
-241.458511	-18.006545	0.325312
-245.534014	2.483887	0.330317
-248.853113	-12.069990	0.335322
-252.591260	-15.943964	0.340326
-256.542438	-17.063656	0.345331
-260.315785	-20.228669	0.350336
-264.253905	-6.304569	0.355341
-268.329680	-15.131506	0.360346
-271.839151	-24.812075	0.365350
-275.268337	-10.704266	0.370355
-278.794890	-16.387639	0.375360
-283.172464	-6.807300	0.380365
-286.792091	-17.660880	0.385370
-290.668748	-14.424208	0.390374
-294.169329	-13.286582	0.395379
-297.676279	-13.441049	0.400384
-301.745563	-2.231992	0.405389
-305.270363	-14.428490	0.410394
-309.372544	-3.493294	0.415398
-313.122337	-5.605417	0.420403
-316.639957	-13.450607	0.425408
-320.849335	-8.192716	0.430413
-324.130959	-5.279640	0.435418
-327.520541	-13.444877	0.440422
-331.871736	-4.478951	0.445427
-335.312599	-15.871929	0.450432
-339.537998	-7.594708	0.455437
-342.998619	-12.131015	0.460442
-347.035696	-8.239433	0.465446
-350.870317	-8.188544	0.470451
-354.083432	-0.894507	0.475456
-358.295629	-0.638245	0.480461
-362.213628	-11.578112	0.485466
-365.910945	-10.953027	0.490470
-369.951234	-9.749624	0.495475
-373.233631	-8.744490	0.500480
-376.573154	-7.186178	0.505485
-380.281967	-11.913040	0.510490
-384.225818	-17.140113	0.515494
-388.363770	-4.901238	0.520499
-392.257390	-12.060221	0.525504
-396.421820	0.083550	0.530509
-399.768224	-9.187622	0.535514
-403.137388	-2.297543	0.540518
-406.982484	-6.054846	0.545523
-410.605599	-10.178750	0.550528
-414.761640	-9.873007	0.555533
-418.454006	-16.983653	0.560538
-422.189932	-8.364980	0.565542
-426.151438	-14.464380	0.570547
-429.509306	-11.371831	0.575552
-433.312612	-2.264557	0.580557
-436.595396	-11.817070	0.585562
-440.686019	-9.780758	0.590566
-444.690232	-3.207110	0.595571
-448.403170	-9.850797	0.600576
-452.485629	-2.413080	0.605581
-456.041930	-9.969601	0.610586
-459.623469	-4.961546	0.615590
-463.671690	-5.841469	0.620595
-467.149522	-5.192931	0.625600
-470.982287	-0.215702	0.630605
-474.703732	-2.682182	0.635610
-478.512078	-6.095149	0.640614
-482.473193	3.300756	0.645619
-486.103917	-11.967814	0.650624
-490.129616	-3.943008	0.655629
-493.263196	-5.085652	0.660634
-497.566086	-0.823358	0.665638
-501.489846	-2.907397	0.670643
-504.900612	-5.259443	0.675648
-508.594049	1.685724	0.680653
-512.163608	-8.065306	0.685658
-516.281504	-6.626911	0.690662
-519.878267	1.805680	0.695667
-523.678422	-9.578507	0.700672
-527.817811	-15.583087	0.705677
-531.439083	-6.403818	0.710682
-534.736568	-2.259470	0.715686
-538.861178	-8.009348	0.720691
-542.283647	-4.677665	0.725696
-546.023315	-3.509369	0.730701
-549.818346	-1.849672	0.735706
-553.673865	-9.128007	0.740710
-557.751880	-2.253804	0.745715
-561.162627	-12.250896	0.750720
-565.186396	-6.129675	0.755725
-569.171020	3.522436	0.760730
-572.880567	-0.473868	0.765734
-576.257193	2.308065	0.770739
-579.893511	-5.462563	0.775744
-583.995472	-1.612264	0.780749
-587.606267	-4.736487	0.785754
-591.328392	-9.766815	0.790758
-595.154901	-1.418844	0.795763
-598.603405	-5.546694	0.800768
-603.114633	-7.104624	0.805773
-606.664491	-9.644036	0.810778
-610.279035	-0.000523	0.815782
-614.086847	-1.949931	0.820787
-617.967927	-19.212557	0.825792
-621.401640	-14.139578	0.830797
-624.857945	-16.451055	0.835802
-628.887974	-15.078544	0.840806
-633.032856	-6.496724	0.845811
-636.521831	-16.556892	0.850816
-640.339090	-5.490071	0.855821
-644.012087	-11.469609	0.860826
-648.041584	-3.869723	0.865830
-651.349120	-3.385322	0.870835
-654.942810	-21.015496	0.875840
-658.967243	-5.846984	0.880845
-662.979543	2.175961	0.885850
-666.967764	-10.139877	0.890854
-670.462354	-6.634062	0.895859
-674.127025	-17.806240	0.900864
-678.492067	-0.000205	0.905869
-681.932703	-13.945780	0.910874
-685.162418	-2.417682	0.915878
-689.138676	-4.827333	0.920883
-692.809465	-9.616539	0.925888
-696.697880	4.968907	0.930893
-700.274058	-16.434513	0.935898
-704.137877	-4.417133	0.940902
-708.146189	-7.699997	0.945907
-711.603441	-18.599327	0.950912
-715.604433	2.961689	0.955917
-719.431484	-3.228080	0.960922
-723.224014	-5.107212	0.965926
-726.847129	-2.142175	0.970931
-730.226794	-15.731558	0.975936
-734.715941	-10.732604	0.980941
-738.267829	-9.685480	0.985946
-741.986936	-7.875186	0.990950
-745.689462	-5.263285	0.995955
-749.312537	-6.321051	1.000960
-753.106689	-4.423051	1.005965
-756.566380	-12.268926	1.010970
-760.155605	-6.499112	1.015974
-764.563082	2.672104	1.020979
-768.224801	-0.372736	1.025984
-772.400111	-1.553518	1.030989
-775.715124	-4.589103	1.035994
-779.255967	-13.675656	1.040998
-783.383216	-2.508612	1.046003
-786.965892	-10.446748	1.051008
-791.151771	-2.059962	1.056013
-794.653706	0.445836	1.061018
-798.563537	1.791538	1.066022
-802.010895	-2.058646	1.071027
-805.142885	-11.464400	1.076032
-809.609922	4.415345	1.081037
-813.654701	6.126419	1.086042
-817.214018	-12.639662	1.091046
-820.738401	-5.711597	1.096051
-824.704170	-12.834648	1.101056
-828.636801	-7.449812	1.106061
-832.074934	-6.901705	1.111066
-835.742129	-11.024201	1.116070
-839.949468	-3.297803	1.121075
-843.280543	-7.579674	1.126080
-847.011046	0.109936	1.131085
-851.077788	-4.815995	1.136090
-854.506544	-8.992348	1.141094
-858.462140	-7.897853	1.146099
-862.039949	-11.484237	1.151104
-865.920595	-5.929456	1.156109
-869.693876	-9.659622	1.161114
-873.279108	-6.432338	1.166118
-877.601320	-5.432166	1.171123
-881.000050	-9.916055	1.176128
-884.847529	-1.053353	1.181133
-888.582068	-12.400087	1.186138
-892.164566	-11.297376	1.191142
-896.230008	-0.111642	1.196147
-899.631606	-10.537027	1.201152
-903.897341	-0.645480	1.206157
-907.570004	-0.752050	1.211162
-911.107488	-0.889690	1.216166
-914.924495	-1.309062	1.221171
-918.351194	0.087324	1.226176
-922.268566	-2.318728	1.231181
-926.239733	-2.672432	1.236186
-929.878487	-12.764957	1.241190
-934.140658	-6.762709	1.246195
-937.386166	-9.608899	1.251200
-941.569790	-5.864786	1.256205
-944.817603	-6.160656	1.261210
-948.819346	-0.786651	1.266214
-952.582489	-2.734763	1.271219
-955.968264	-12.834580	1.276224
-959.954406	-7.302204	1.281229
-963.772223	-9.206861	1.286234
-967.691873	-9.745351	1.291238
-971.534493	1.781766	1.296243
-974.812935	-12.200311	1.301248
-978.733894	-18.820894	1.306253
-982.571969	-12.455873	1.311258
-986.323030	-6.726080	1.316262
-990.319865	-4.390013	1.321267
-993.643432	-11.725852	1.326272
-997.609182	-2.265320	1.331277
-1001.438384	-15.840728	1.336282
-1005.055849	-9.667070	1.341286
-1009.136744	-2.749083	1.346291
-1012.819635	-13.430500	1.351296
-1017.015838	-2.837097	1.356301
-1020.558337	-7.969568	1.361306
-1023.994979	-8.069548	1.366310
-1027.752064	0.045633	1.371315
-1030.949491	-10.869517	1.376320
-1035.375645	-1.075091	1.381325
-1039.119532	3.458306	1.386330
-1042.903526	-2.070747	1.391334
-1046.514957	-3.274993	1.396339
-1050.112961	-6.309073	1.401344
-1053.920317	0.795475	1.406349
-1057.733568	-5.030071	1.411354
-1061.757810	5.474406	1.416358
-1065.624023	-2.974598	1.421363
-1068.963372	-5.474431	1.426368
-1072.817310	-10.164341	1.431373
-1076.544681	-0.856930	1.436378
-1080.308217	-6.343459	1.441382
-1084.479386	-2.202117	1.446387
-1087.651633	7.163175	1.451392
-1091.701039	-0.296115	1.456397
-1095.305284	-6.637578	1.461402
-1098.919972	-8.014685	1.466406
-1103.506332	-2.756642	1.471411
-1106.970860	1.159737	1.476416
-1110.570806	-1.257348	1.481421
-1113.867520	-11.530439	1.486426
-1117.641269	-12.114094	1.491430
-1122.008967	-9.299007	1.496435
-1125.626699	-6.146571	1.501440
-1129.734616	-2.642897	1.506445
-1133.281302	0.837231	1.511450
-1136.391387	-8.765516	1.516454
-1140.466679	-0.353252	1.521459
-1143.942875	-15.161288	1.526464
-1148.350882	-6.175389	1.531469
-1152.150708	-1.175551	1.536474
-1155.369215	-6.019023	1.541478
-1159.484220	2.330242	1.546483
-1163.033752	-3.303929	1.551488
-1166.930077	-7.963243	1.556493
-1170.481919	-7.338099	1.561498
-1174.239295	-3.297499	1.566502
-1178.457382	1.971153	1.571507
-1181.939731	-3.169112	1.576512
-1185.962739	-0.861642	1.581517
-1189.778296	-2.126043	1.586522
-1193.137432	-1.530122	1.591526
-1197.064882	5.683754	1.596531
-1200.283584	-2.040720	1.601536
-1204.505954	1.240124	1.606541
-1208.591451	-7.053690	1.611546
-1212.115149	2.804809	1.616550
-1216.010339	-9.862373	1.621555
-1219.382907	-7.425537	1.626560
-1223.532118	-5.247619	1.631565
-1226.896186	-0.721092	1.636570
-1230.862564	-7.513743	1.641574
-1234.341953	3.364294	1.646579
-1238.125678	-6.050085	1.651584
-1242.275472	0.381003	1.656589
-1246.410208	-3.577703	1.661594
-1249.785077	-8.659366	1.666598
-1253.662005	0.410471	1.671603
-1256.930810	-11.106352	1.676608
-1260.945650	-1.708506	1.681613
-1264.557072	-2.160205	1.686618
-1268.131181	-5.226149	1.691622
-1272.207286	1.003964	1.696627
-1276.083391	-4.801689	1.701632
-1279.899517	-3.561649	1.706637
-1283.494238	-5.287014	1.711642
-1287.300458	-8.944983	1.716646
-1291.167661	-0.663543	1.721651
-1294.655601	-8.545055	1.726656
-1298.381521	-2.648490	1.731661
-1302.670630	-2.048647	1.736666
-1305.958811	-4.285087	1.741670
-1309.889508	8.223320	1.746675
-1313.375754	-3.889401	1.751680
-1317.309173	-0.347099	1.756685
-1321.191124	-1.316803	1.761690
-1324.654090	-7.924934	1.766694
-1328.959631	-5.510495	1.771699
-1332.333730	-9.658600	1.776704
-1336.267734	-4.340528	1.781709
-1340.038668	-1.667866	1.786714
-1343.577069	-9.214793	1.791718
-1347.482199	-0.712728	1.796723
-1351.229509	-5.244189	1.801728
-1355.142845	0.173110	1.806733
-1358.431143	5.058278	1.811738
-1362.231284	-6.847994	1.816742
-1366.052178	0.651870	1.821747
-1369.848793	-0.377145	1.826752
-1373.768168	-3.253610	1.831757
-1377.873594	-6.070322	1.836762
-1381.294179	-12.283024	1.841766
-1385.124944	-3.606725	1.846771
-1388.804442	-12.755248	1.851776
-1392.748856	-8.542435	1.856781
-1396.397414	-9.303371	1.861786
-1399.634761	-10.420293	1.866790
-1404.048067	-8.092542	1.871795
-1407.629865	-2.100610	1.876800
-1411.419139	-7.483112	1.881805
-1415.375973	-6.575136	1.886810
-1418.883724	-7.330194	1.891814
-1422.501740	-3.186935	1.896819
-1426.024504	-10.185876	1.901824
-1430.340789	-8.242615	1.906829
-1434.043227	-9.926841	1.911834
-1437.756974	-12.615344	1.916838
-1441.889291	-8.150014	1.921843
-1445.233189	-5.908256	1.926848
-1448.837850	-3.776128	1.931853
-1452.712313	-8.764873	1.936858
-1456.364960	-9.249093	1.941862
-1460.376120	-1.983544	1.946867
-1464.210371	-18.561393	1.951872
-1467.945395	0.132251	1.956877
-1471.715002	-5.466186	1.961882
-1474.985705	-9.236395	1.966886
-1479.088754	-7.014953	1.971891
-1482.476013	-11.994929	1.976896
-1486.482969	-2.522283	1.981901
-1490.395352	2.902970	1.986906
-1494.256615	-9.173048	1.991910
-1498.176442	-3.081120	1.996915
-1502.148267	-6.153852	2.006912
-1502.525166	-1.160611	2.016909
-1500.211111	-5.449988	2.026906
-1497.329169	-0.566499	2.036902
-1495.308099	-0.458897	2.046899
-1493.213505	-6.671044	2.056896
-1491.454186	-3.140954	2.066893
-1489.750720	-8.990460	2.076890
-1487.684894	-5.673662	2.086886
-1485.852661	-9.904816	2.096883
-1484.001962	-5.434078	2.106880
-1481.926093	-6.198936	2.116877
-1480.012580	-1.540881	2.126874
-1477.839609	-5.196584	2.136870
-1476.421532	-5.878210	2.146867
-1474.460334	-7.382603	2.156864
-1472.436888	-13.985973	2.166861
-1470.519970	-11.826384	2.176858
-1468.683187	-5.474434	2.186854
-1467.028994	-8.276521	2.196851
-1465.221104	-6.933164	2.206848
-1462.967433	-7.874897	2.216845
-1460.844663	-4.658772	2.226842
-1459.208924	-7.442109	2.236838
-1457.448065	-6.748066	2.246835
-1455.514979	-7.971622	2.256832
-1453.508612	-10.230081	2.266829
-1451.666261	-2.165826	2.276826
-1450.040684	-5.255430	2.286822
-1448.064221	-6.056446	2.296819
-1446.153381	-3.900598	2.306816
-1444.211273	-8.758796	2.316813
-1442.111426	-8.209018	2.326810
-1440.600410	-6.147046	2.336806
-1438.767077	-7.348301	2.346803
-1436.807677	-4.022310	2.356800
-1434.518688	-5.167042	2.366797
-1432.918990	-2.926629	2.376794
-1430.985990	-4.674369	2.386790
-1429.068497	-2.432728	2.396787
-1427.277112	0.301217	2.406784
-1425.640408	-5.731771	2.416781
-1423.511984	-11.354002	2.426778
-1421.614623	-4.100645	2.436774
-1419.557548	0.722377	2.446771
-1417.665992	-5.135090	2.456768
-1416.100352	-4.738185	2.466765
-1414.167983	-7.586351	2.476762
-1412.243929	-7.567356	2.486758
-1410.016199	-12.992314	2.496755
-1408.363962	-9.225538	2.506752
-1406.535928	-5.357429	2.516749
-1405.057357	-4.823417	2.526746
-1402.922151	-3.088722	2.536742
-1400.897441	-3.766368	2.546739
-1398.828757	-7.466883	2.556736
-1397.339807	-7.855066	2.566733
-1395.245264	-5.425423	2.576730
-1393.228804	-4.418561	2.586726
-1391.664693	-8.581457	2.596723
-1389.721346	-4.273893	2.606720
-1387.696319	-3.890511	2.616717
-1385.788619	-6.597335	2.626714
-1383.993352	-2.705014	2.636710
-1381.967168	-7.603465	2.646707
-1380.373133	-5.556321	2.656704
-1378.384375	-7.447156	2.666701
-1376.777595	-5.083098	2.676698
-1374.856108	-7.648434	2.686694
-1372.925232	-4.837301	2.696691
-1370.633768	-11.652446	2.706688
-1368.734549	-12.123656	2.716685
-1367.436570	-2.585848	2.726682
-1365.397604	-2.000990	2.736678
-1363.157297	-6.897386	2.746675
-1361.459084	-5.845867	2.756672
-1359.465096	-12.768120	2.766669
-1357.569979	-3.103258	2.776666
-1356.175181	-3.152655	2.786662
-1354.074115	-2.239829	2.796659
-1352.186404	-6.907665	2.806656
-1350.421198	-4.431577	2.816653
-1348.229433	-7.521742	2.826650
-1346.358806	-3.292501	2.836646
-1344.571381	-8.681657	2.846643
-1342.713129	-11.298425	2.856640
-1340.799371	-14.824088	2.866637
-1338.998836	-6.942518	2.876634
-1337.160808	-8.141287	2.886630
-1335.207455	-4.277388	2.896627
-1333.377325	-6.877016	2.906624
-1331.292658	-8.671057	2.916621
-1329.676552	-10.974314	2.926618
-1327.862715	-14.447657	2.936614
-1326.047292	-15.394900	2.946611
-1323.624896	-12.633979	2.956608
-1322.014337	-13.722115	2.966605
-1320.204895	-14.039967	2.976602
-1318.286694	-15.224711	2.986598
-1316.190135	-13.872176	2.996595
-1314.488490	-12.176951	3.006592
-1312.861732	-10.725532	3.016589
-1310.684749	-10.007978	3.026586
-1309.135574	-12.019452	3.036582
-1307.240719	-8.155640	3.046579
-1305.373484	-11.324877	3.056576
-1303.126447	-5.250028	3.066573
-1301.314549	-12.552045	3.076570
-1299.630875	-7.790730	3.086566
-1297.620014	-7.007101	3.096563
-1295.909044	-10.503431	3.106560
-1293.719949	-10.570968	3.116557
-1291.884044	-11.232512	3.126554
-1290.309526	-7.257416	3.136550
-1288.359723	-6.710325	3.146547
-1286.536131	-3.277201	3.156544
-1284.240703	-7.626549	3.166541
-1282.560013	-10.233800	3.176538
-1280.960225	-6.449059	3.186534
-1279.010679	-4.071892	3.196531
-1277.013019	-10.931510	3.206528
-1275.117619	-7.168812	3.216525
-1273.189556	-5.138733	3.226522
-1271.348083	-8.894357	3.236518
-1269.543041	-7.572493	3.246515
-1267.578062	-9.961542	3.256512
-1265.876802	-10.369409	3.266509
-1263.674235	-11.714882	3.276506
-1262.113299	-8.656553	3.286502
-1260.300325	-8.142806	3.296499
-1258.185400	-14.815907	3.306496
-1256.270723	-15.363712	3.316493
-1254.667324	-11.655321	3.326490
-1252.547167	-8.983325	3.336486
-1250.853565	-15.840052	3.346483
-1248.830102	-12.181512	3.356480
-1246.503723	-7.333531	3.366477
-1245.386070	-12.694381	3.376474
-1243.382060	-6.353207	3.386470
-1241.467471	-5.206749	3.396467
-1239.495336	-12.888054	3.406464
-1237.407216	-16.364168	3.416461
-1235.779780	-8.330071	3.426458
-1233.808270	-10.036443	3.436454
-1232.087032	-11.882767	3.446451
-1230.347727	-10.472983	3.456448
-1228.161623	-4.304619	3.466445
-1226.369991	-13.559687	3.476442
-1224.417052	-15.057813	3.486438
-1222.548810	-10.573872	3.496435
-1220.738170	-10.568149	3.506432
-1218.639297	-11.511718	3.516429
-1216.984651	-18.638508	3.526426
-1215.374431	-9.827945	3.536422
-1213.106980	-17.586483	3.546419
-1211.180826	-13.691283	3.556416
-1209.408397	-9.403581	3.566413
-1207.744035	-18.829323	3.576410
-1205.739059	-8.158730	3.586406
-1203.927520	-7.930503	3.596403
-1201.958961	-5.644734	3.606400
-1200.041094	-8.525145	3.616397
-1198.040545	-11.774053	3.626394
-1196.334738	-7.873581	3.636390
-1194.322841	-12.314846	3.646387
-1192.641097	-14.726410	3.656384
-1190.575339	-12.543028	3.666381
-1188.678767	-7.384632	3.676378
-1186.992907	-4.902035	3.686374
-1185.073266	-7.681664	3.696371
-1183.236749	-5.677915	3.706368
-1181.325070	-7.327301	3.716365
-1179.739072	-6.434537	3.726362
-1177.588546	-7.487389	3.736358
-1175.746088	-15.545797	3.746355
-1173.722656	-12.485614	3.756352
-1171.610203	-8.348602	3.766349
-1169.855951	-11.196495	3.776346
-1168.071975	-7.617986	3.786342
-1166.386280	-9.371732	3.796339
-1164.564238	-5.845101	3.806336
-1162.308603	-7.808454	3.816333
-1160.694029	-8.221323	3.826330
-1158.768562	-8.210238	3.836326
-1157.026415	-12.044622	3.846323
-1155.413178	-15.229949	3.856320
-1152.985387	-14.505003	3.866317
-1151.297820	-16.345881	3.876314
-1149.451437	-11.411532	3.886310
-1147.417618	-8.763519	3.896307
-1145.517137	-13.455345	3.906304
-1143.817020	-21.917278	3.916301
-1142.177170	-16.185659	3.926298
-1139.816899	-14.428302	3.936294
-1138.092536	-4.399599	3.946291
-1136.426761	-5.993820	3.956288
-1134.504756	-9.983280	3.966285
-1132.235709	-10.644519	3.976282
-1130.629902	-18.022393	3.986278
-1129.015458	-6.610288	3.996275
-1126.894141	-8.661069	4.006272
-1124.965174	-13.183749	4.016269
-1123.237183	-10.796268	4.026266
-1121.270913	-8.061635	4.036262
-1119.342867	-4.937193	4.046259
-1117.469546	-10.720462	4.056256
-1115.370710	-15.167675	4.066253
-1113.962197	-6.261603	4.076250
-1111.747778	-5.676167	4.086246
-1110.160152	-9.620012	4.096243
-1107.944412	-8.486880	4.106240
-1106.315870	-3.301324	4.116237
-1104.534069	-9.785218	4.126234
-1102.508127	-10.049112	4.136230
-1100.760288	-9.100075	4.146227
-1098.627302	-12.196400	4.156224
-1096.998013	-5.512510	4.166221
-1094.972277	-5.283724	4.176218
-1092.832531	-6.225825	4.186214
-1091.135225	-11.824599	4.196211
-1089.178506	-8.575243	4.206208
-1087.767206	-18.156226	4.216205
-1085.733616	-22.255075	4.226202
-1083.716099	-12.980605	4.236198
-1081.602597	-8.182084	4.246195
-1079.768954	-11.828941	4.256192
-1078.288273	-5.073897	4.266189
-1076.453892	-15.894149	4.276186
-1074.284021	-12.999408	4.286182
-1072.534042	-9.808549	4.296179
-1070.387483	-14.381781	4.306176
-1068.649643	-11.098977	4.316173
-1066.697662	-13.631048	4.326170
-1065.250861	-6.782153	4.336166
-1063.223922	-8.843046	4.346163
-1061.215313	-12.492611	4.356160
-1059.287727	-17.108178	4.366157
-1057.456548	-11.637625	4.376154
-1055.184311	-15.070399	4.386150
-1053.761761	-11.721363	4.396147
-1052.028391	-11.129982	4.406144
-1049.874615	-11.412698	4.416141
-1048.046542	-10.838040	4.426138
-1046.320703	-13.427084	4.436134
-1044.261910	-16.726234	4.446131
-1042.555335	-5.982488	4.456128
-1040.577827	-15.952436	4.466125
-1038.579297	-13.601845	4.476122
-1036.803476	-10.833520	4.486118
-1035.061586	-5.643933	4.496115
-1033.187543	-14.342042	4.506112
-1031.342462	-4.856776	4.516109
-1029.213679	-12.100336	4.526106
-1027.371815	-14.815293	4.536102
-1025.685896	-16.564239	4.546099
-1023.505207	-11.601143	4.556096
-1021.630876	-16.803437	4.566093
-1020.111142	-17.941580	4.576090
-1018.177177	-14.127988	4.586086
-1016.308075	-11.290880	4.596083
-1014.241424	-19.640823	4.606080
-1012.468430	-18.209419	4.616077
-1010.495415	-15.769458	4.626074
-1008.259235	-14.805292	4.636070
-1006.841344	-12.194442	4.646067
-1004.833895	-13.982162	4.656064
-1003.013537	-14.235198	4.666061
-1001.272535	-16.815581	4.676058
-999.447795	-21.180965	4.686054
-997.679563	-15.903985	4.696051
-995.370421	-16.029914	4.706048
-993.591567	-16.953685	4.716045
-991.763323	-15.428467	4.726042
-989.783679	-18.872810	4.736038
-988.179972	-13.024764	4.746035
-986.169061	-15.940411	4.756032
-983.978409	-16.475284	4.766029
-982.546759	-19.590404	4.776026
-980.553425	-21.492691	4.786022
-978.495077	-15.169437	4.796019
-976.616401	-17.381813	4.806016
-974.821915	-15.846446	4.816013
-973.538863	-18.072521	4.826010
-971.302360	-9.270334	4.836006
-969.181519	-11.567219	4.846003
-967.322337	-17.149163	4.856000
-965.443890	-17.540934	4.865997
-963.634169	-16.780114	4.875994
-961.466781	-17.052293	4.885990
-959.918358	-12.756992	4.895987
-958.175585	-20.819832	4.905984
-956.048026	-10.893348	4.915981
-954.443115	-14.817752	4.925978
-952.163437	-7.151415	4.935974
-950.515850	-11.884762	4.945971
-948.804958	-13.154481	4.955968
-946.969630	-6.681846	4.965965
-944.949717	-8.773095	4.975962
-942.838669	-11.521558	4.985958
-941.172877	-11.768778	4.995955
-939.276200	-6.087539	5.005952
-937.210173	-17.761069	5.015949
-935.543693	-12.805668	5.025946
-933.730706	-8.997921	5.035942
-931.828122	-4.741858	5.045939
-929.474482	-12.848672	5.055936
-928.053027	-6.965121	5.065933
-926.014019	-8.097810	5.075930
-924.105238	-2.019011	5.085926
-922.722340	-6.324749	5.095923
-920.448254	-4.057586	5.105920
-918.287916	-3.592794	5.115917
-916.602449	-7.406895	5.125914
-915.060649	-4.528423	5.135910
-913.096809	-0.653196	5.145907
-911.082985	-1.304994	5.155904
-909.164752	-6.757390	5.165901
-907.486743	-12.588225	5.175898
-905.470761	-7.789733	5.185894
-903.632058	-5.497154	5.195891
-901.736169	-7.603275	5.205888
-899.779073	-11.607638	5.215885
-897.817163	-9.363175	5.225882
-896.254625	-3.210046	5.235878
-894.330500	-2.533779	5.245875
-892.233958	-2.912991	5.255872
-890.409126	-9.997314	5.265869
-888.581212	-8.213008	5.275866
-886.496720	-17.190979	5.285862
-884.851400	-12.317421	5.295859
-883.119036	-9.218336	5.305856
-881.258227	-11.713577	5.315853
-879.018832	-11.004015	5.325850
-877.316831	-14.552305	5.335846
-875.468340	-12.984441	5.345843
-873.557476	-11.383915	5.355840
-871.507255	-12.253081	5.365837
-870.050155	-7.864166	5.375834
-868.021233	-7.060945	5.385830
-865.676174	-6.551424	5.395827
-864.207791	-9.339186	5.405824
-862.585710	-8.101439	5.415821
-860.690539	-14.347493	5.425818
-858.372737	-7.931387	5.435814
-856.708664	-7.609840	5.445811
-854.550333	-13.541110	5.455808
-852.954625	-12.665464	5.465805
-851.340218	-15.542878	5.475802
-849.030266	-15.392472	5.485798
-847.069170	-10.750947	5.495795
-845.454889	-7.190843	5.505792
-843.674896	-11.626332	5.515789
-842.066600	-17.346503	5.525786
-839.668951	-8.650466	5.535782
-837.908082	-10.998642	5.545779
-836.149367	-1.453603	5.555776
-834.122254	-11.837129	5.565773
-832.012970	-7.951924	5.575770
-830.510695	-7.498703	5.585766
-828.544711	-8.611741	5.595763
-826.837988	-3.580580	5.605760
-824.514190	-11.470946	5.615757
-822.756858	-11.832190	5.625754
-821.210827	-8.761695	5.635750
-819.161460	-0.944714	5.645747
-817.525290	-7.923039	5.655744
-815.424691	-15.024544	5.665741
-813.651670	-2.137496	5.675738
-811.683505	-7.395690	5.685734
-809.613317	-12.480712	5.695731
-807.897214	-7.777885	5.705728
-805.915366	-6.622867	5.715725
-804.367512	-7.237989	5.725722
-802.120284	-4.107450	5.735718
-800.561371	-10.359716	5.745715
-798.359515	-8.377735	5.755712
-796.482764	-11.085464	5.765709
-794.878204	-7.804827	5.775706
-792.805811	-10.914884	5.785702
-791.278837	-4.217563	5.795699
-789.149561	-5.007713	5.805696
-787.195999	-7.228755	5.815693
-785.172607	-7.136697	5.825690
-783.932096	-4.697883	5.835686
-781.428406	-3.983101	5.845683
-779.533423	-11.839626	5.855680
-777.667217	-0.615893	5.865677
-776.122640	-6.809011	5.875674
-774.103242	-4.090461	5.885670
-772.385532	0.116340	5.895667
-770.169030	-16.913334	5.905664
-768.402678	-10.176888	5.915661
-766.805116	-8.052505	5.925658
-764.713315	-10.412466	5.935654
-763.048885	-5.129754	5.945651
-760.894806	-2.266925	5.955648
-759.190102	-14.938915	5.965645
-757.028325	-11.358878	5.975642
-755.258703	-10.536223	5.985638
-753.559309	-8.909694	5.995635
-751.733840	-6.643300	6.005632
-749.536088	-7.018034	6.015629
-747.795182	-1.842270	6.025626
-745.978920	-0.243886	6.035622
-744.140464	2.160970	6.045619
-742.606847	-2.797194	6.055616
-739.976277	-1.474209	6.065613
-738.498438	-2.929171	6.075610
-736.975160	-5.635629	6.085606
-734.529632	-1.428269	6.095603
-732.944823	-1.465028	6.105600
-730.825305	-5.683114	6.115597
-729.206275	-7.129054	6.125594
-727.020338	-0.085403	6.135590
-725.365471	0.758772	6.145587
-723.617135	0.083242	6.155584
-721.494222	-5.363827	6.165581
-719.651952	-6.984385	6.175578
-717.828357	-4.845561	6.185574
-716.037158	-8.876954	6.195571
-714.045401	-3.414402	6.205568
-712.206872	-7.810206	6.215565
-710.555551	-8.681806	6.225562
-708.646130	-11.052050	6.235558
-706.342344	-3.864578	6.245555
-704.589508	-3.599740	6.255552
-703.088097	-9.441698	6.265549
-700.859933	-11.643391	6.275546
-699.000416	-4.547555	6.285542
-697.191036	-0.096391	6.295539
-695.374582	-7.553460	6.305536
-693.383681	-2.774451	6.315533
-691.482567	-6.926024	6.325530
-689.564008	-0.597523	6.335526
-687.875284	-8.545766	6.345523
-685.987497	-4.673978	6.355520
-684.113056	-12.493994	6.365517
-682.401189	-2.552910	6.375514
-680.383535	-2.365106	6.385510
-678.324434	-4.703979	6.395507
-676.525724	-0.859003	6.405504
-674.458610	-2.955990	6.415501
-672.849213	-5.957229	6.425498
-670.881992	-1.652847	6.435494
-669.417786	-4.621411	6.445491
-667.207218	3.496810	6.455488
-665.265539	-3.767085	6.465485
-663.231647	0.488755	6.475482
-661.714418	-2.786704	6.485478
-659.609086	-3.430805	6.495475
-657.856604	-6.597005	6.505472
-655.849112	-7.650216	6.515469
-653.994678	-11.549559	6.525466
-652.021667	-6.982398	6.535462
-650.337122	-10.325635	6.545459
-648.462919	-7.179557	6.555456
-646.454066	-10.075650	6.565453
-644.667283	-12.082031	6.575450
-642.765420	-8.921420	6.585446
-640.844757	-7.154894	6.595443
-639.085526	-10.331632	6.605440
-637.245143	-13.483438	6.615437
-635.210997	-8.951293	6.625434
-633.286838	-11.085406	6.635430
-631.529323	-4.131112	6.645427
-630.019826	-8.662187	6.655424
-627.744900	-9.745470	6.665421
-625.860173	-12.217495	6.675418
-624.003866	-17.081872	6.685414
-622.070457	-19.455879	6.695411
-620.228773	-16.839859	6.705408
-618.259635	-14.241042	6.715405
-616.554873	-13.128440	6.725402
-614.730119	-6.878049	6.735398
-612.763768	-13.457407	6.745395
-610.903982	-9.786352	6.755392
-608.797738	-13.034296	6.765389
-607.190194	-12.005632	6.775386
-605.439869	-15.763566	6.785382
-603.605432	-16.569608	6.795379
-601.602027	-6.480819	6.805376
-599.538613	-6.099726	6.815373
-597.651789	-13.594810	6.825370
-595.700361	-9.475741	6.835366
-594.036554	-8.590269	6.845363
-592.210846	-6.998011	6.855360
-590.138229	-9.269494	6.865357
-588.289264	-7.164621	6.875354
-586.460251	-11.688289	6.885350
-584.843823	-8.947831	6.895347
-582.892049	-5.064073	6.905344
-580.831962	-12.725774	6.915341
-578.705960	-10.739362	6.925338
-577.236316	-6.859110	6.935334
-575.703003	-9.630232	6.945331
-573.231779	-6.569988	6.955328
-571.280790	-11.076813	6.965325
-569.809517	-13.228533	6.975322
-567.574336	-18.938145	6.985318
-565.777571	-9.839496	6.995315
-564.058480	-13.413988	7.005312
-562.137514	-10.358996	7.015309
-560.159920	-9.409937	7.025306
-558.313633	-8.758856	7.035302
-556.552399	-9.605276	7.045299
-554.499868	-11.346139	7.055296
-552.572718	-5.146789	7.065293
-551.155861	-4.502899	7.075290
-549.088682	-11.085684	7.085286
-547.090654	-6.350316	7.095283
-544.922812	-9.104350	7.105280
-543.444725	-14.981965	7.115277
-541.517115	-17.847626	7.125274
-539.512560	-17.905511	7.135270
-538.011645	-17.676102	7.145267
-535.991285	-13.301145	7.155264
-533.840069	-15.195124	7.165261
-531.952235	-19.102868	7.175258
-530.010693	-10.829437	7.185254
-528.463599	-9.036309	7.195251
-526.377763	-10.125610	7.205248
-524.427628	-15.977557	7.215245
-522.876528	-12.771874	7.225242
-520.970813	-16.461410	7.235238
-518.968556	-12.563556	7.245235
-517.197633	-11.294077	7.255232
-515.146122	-13.022111	7.265229
-513.597684	-15.460865	7.275226
-511.078801	-15.157180	7.285222
-509.532452	-6.975349	7.295219
-507.690791	-5.622420	7.305216
-505.841358	-4.930748	7.315213
-503.971657	-15.217833	7.325210
-502.060539	-16.835010	7.335206
-500.161779	-15.685412	7.345203
-498.125607	-13.461943	7.355200
-496.536768	-15.272387	7.365197
-494.577476	-18.330970	7.375194
-492.777654	-17.271356	7.385190
-490.825486	-19.297721	7.395187
-488.835322	-14.845266	7.405184
-487.082279	-11.719181	7.415181
-485.008675	-11.745415	7.425178
-483.348259	-9.754034	7.435174
-481.424279	-9.480047	7.445171
-479.620372	-8.184227	7.455168
-477.529158	-6.402171	7.465165
-475.741720	-17.002948	7.475162
-473.889667	-13.445812	7.485158
-471.860431	-8.716942	7.495155
-470.346487	-11.057000	7.505152
-468.455069	-5.477149	7.515149
-466.294485	-10.047367	7.525146
-464.474475	-3.290816	7.535142
-462.776274	-11.374645	7.545139
-460.745519	-6.225996	7.555136
-458.933207	-14.773318	7.565133
-456.989488	-9.394446	7.575130
-455.153058	-15.010283	7.585126
-453.161994	-7.411020	7.595123
-451.455547	-6.838580	7.605120
-449.552457	-6.220170	7.615117
-447.668195	-6.584039	7.625114
-445.888224	-12.647181	7.635110
-443.957148	-12.446930	7.645107
-442.088366	-6.471853	7.655104
-439.790483	-11.556617	7.665101
-438.184183	-7.977576	7.675098
-436.533049	-13.192749	7.685094
-434.576985	-13.705446	7.695091
-432.725819	-11.622906	7.705088
-430.670588	-12.072486	7.715085
-428.719734	-7.021578	7.725082
-426.908560	-5.793195	7.735078
-425.350084	-7.096628	7.745075
-423.300412	-8.800608	7.755072
-421.373187	-9.654487	7.765069
-419.300926	-4.850330	7.775066
-417.481948	-7.861186	7.785062
-415.808595	-6.942374	7.795059
-414.376542	-7.390329	7.805056
-411.897520	-6.630162	7.815053
-409.835115	-5.141874	7.825050
-408.314681	-15.008380	7.835046
-406.240201	-9.561920	7.845043
-404.900657	-10.094575	7.855040
-402.551235	-8.536843	7.865037
-400.623517	-14.606176	7.875034
-398.766693	-6.827530	7.885030
-397.034808	-8.014946	7.895027
-395.182288	-7.187887	7.905024
-393.247626	-8.835582	7.915021
-391.141252	-10.704908	7.925018
-389.198062	-11.635522	7.935014
-388.108994	-8.097022	7.945011
-385.898480	-7.494487	7.955008
-383.552530	-6.324613	7.965005
-381.944776	-8.839075	7.975002
-380.011712	-12.700243	7.984998
-378.305213	-5.849707	7.994995
-376.352219	-10.261964	8.004992
-374.550503	-10.863656	8.014989
-372.503453	-8.633918	8.024986
-370.575489	-14.415892	8.034982
-368.910084	-9.178829	8.044979
-367.332794	-8.386754	8.054976
-364.958422	-6.662438	8.064973
-363.289087	-3.576577	8.074970
-361.375663	-4.374519	8.084966
-359.567560	-6.952533	8.094963
-357.581469	-8.112609	8.104960
-355.576440	-9.585188	8.114957
-353.925727	-1.516220	8.124954
-351.748045	-8.214388	8.134950
-349.575983	-5.112460	8.144947
-348.307582	-7.879046	8.154944
-346.537081	-8.663633	8.164941
-344.498867	-12.107340	8.174938
-342.502264	-7.906841	8.184934
-340.486586	-11.612217	8.194931
-339.057325	-10.292795	8.204928
-337.022929	-4.080376	8.214925
-334.937190	-15.230807	8.224922
-333.164202	-10.887230	8.234918
-331.301152	-12.337124	8.244915
-329.633303	-16.217494	8.254912
-327.539712	-8.280791	8.264909
-325.749529	-7.656890	8.274906
-323.720744	-12.351213	8.284902
-321.804350	-14.319627	8.294899
-320.001944	-4.984818	8.304896
-318.362273	-0.463623	8.314893
-316.140162	-9.508916	8.324890
-314.236545	-14.135880	8.334886
-312.555169	-7.374442	8.344883
-310.565861	-9.878712	8.354880
-308.568721	-6.950933	8.364877
-306.933688	-12.444514	8.374874
-305.524485	-12.233477	8.384870
-303.221687	-12.551937	8.394867
-301.421852	-12.496415	8.404864
-299.260823	-9.918482	8.414861
-297.360806	-7.493097	8.424858
-295.571430	-12.425504	8.434854
-293.982980	-12.429394	8.444851
-292.212350	-13.545549	8.454848
-290.071970	-11.504326	8.464845
-288.012127	-13.122971	8.474842
-286.158196	-14.591902	8.484838
-284.285988	-11.661529	8.494835
-282.705695	-10.197229	8.504832
-280.750465	-9.703852	8.514829
-278.924396	-10.719897	8.524826
-276.677830	-6.507131	8.534822
-275.203929	-6.442197	8.544819
-273.215326	-5.800979	8.554816
-271.298877	-6.747758	8.564813
-269.144330	-13.333213	8.574810
-267.482207	-9.822963	8.584807
-265.754068	-11.369697	8.594803
-263.880729	-10.950080	8.604800
-261.701130	-4.759190	8.614797
-259.744185	-8.862508	8.624794
-258.250917	-13.198138	8.634791
-256.506342	-8.639960	8.644787
-254.239767	-10.743165	8.654784
-252.786748	-10.722253	8.664781
-250.791236	-12.641661	8.674778
-248.613135	-13.720186	8.684775
-246.610522	-13.973311	8.694771
-245.105623	-7.346290	8.704768
-243.205545	-8.773605	8.714765
-241.260186	-14.641946	8.724762
-239.162826	-7.834737	8.734759
-237.669443	-8.295534	8.744755
-235.739204	-7.164957	8.754752
-233.602928	-7.395192	8.764749
-231.688774	-15.101227	8.774746
-229.787455	-16.885581	8.784743
-228.381970	-11.036914	8.794739
-226.211890	-10.506728	8.804736
-223.906227	-18.021023	8.814733
-222.262142	-15.924216	8.824730
-220.678403	-17.332606	8.834727
-218.902220	-17.985371	8.844723
-216.898175	-17.264464	8.854720
-214.835987	-19.489754	8.864717
-213.113399	-17.759163	8.874714
-211.204033	-15.300463	8.884711
-209.332875	-11.648264	8.894707
-207.359471	-17.323682	8.904704
-205.783123	-13.433373	8.914701
-203.829483	-21.155161	8.924698
-201.887159	-12.922613	8.934695
-199.816825	-18.504543	8.944691
-198.026684	-15.213627	8.954688
-196.560548	-14.400543	8.964685
-194.547369	-17.143799	8.974682
-192.442263	-24.659216	8.984679
-190.583827	-16.135371	8.994675
-188.779381	-18.294244	9.004672
-186.754028	-20.799429	9.014669
-184.588064	-20.409079	9.024666
-183.199896	-19.675126	9.034663
-181.469117	-13.698337	9.044659
-179.350436	-19.262701	9.054656
-177.462141	-12.523129	9.064653
-175.630653	-19.606440	9.074650
-173.531205	-14.397442	9.084647
-171.903461	-16.212307	9.094643
-170.083759	-11.492363	9.104640
-168.361676	-6.886314	9.114637
-166.241021	-12.660992	9.124634
-164.098732	-14.145844	9.134631
-162.608769	-14.321831	9.144627
-160.459096	-18.269503	9.154624
-158.911691	-17.808848	9.164621
-156.935161	-18.457221	9.174618
-154.835158	-23.514886	9.184615
-153.103162	-20.058338	9.194611
-151.148511	-15.808346	9.204608
-149.016646	-20.877408	9.214605
-147.464709	-14.742577	9.224602
-145.609497	-16.427928	9.234599
-143.657382	-14.339162	9.244595
-142.054100	-21.733414	9.254592
-140.074100	-22.325483	9.264589
-138.241109	-17.337628	9.274586
-136.076844	-15.650612	9.284583
-134.035188	-26.838063	9.294579
-132.420785	-16.352021	9.304576
-130.621826	-17.647848	9.314573
-128.860162	-21.640953	9.324570
-126.646950	-14.896338	9.334567
-124.720424	-14.347726	9.344563
-123.142021	-10.857172	9.354560
-121.375037	-14.121630	9.364557
-119.156764	-11.154758	9.374554
-117.416646	-13.131207	9.384551
-115.461997	-15.493997	9.394547
-113.846815	-12.018779	9.404544
-111.818663	-14.578037	9.414541
-110.032126	-11.445955	9.424538
-107.953113	-14.447547	9.434535
-106.197750	-12.145774	9.444531
-104.451386	-6.049825	9.454528
-102.273012	-2.692875	9.464525
-100.563009	-14.260041	9.474522
-98.698860	-12.452474	9.484519
-96.766425	-10.371582	9.494515
-94.662595	-3.751587	9.504512
-93.179575	-5.818057	9.514509
-91.302400	-8.776381	9.524506
-89.217079	-11.019470	9.534503
-87.416646	-11.200732	9.544499
-85.667144	-5.784236	9.554496
-83.715004	-8.582404	9.564493
-81.826722	-8.416089	9.574490
-80.071720	-17.396135	9.584487
-78.037734	-15.674071	9.594483
-75.974749	-13.394510	9.604480
-74.239187	-3.916191	9.614477
-72.341727	-6.340880	9.624474
-70.493865	-12.600923	9.634471
-68.701293	-10.368217	9.644467
-66.880422	-4.056749	9.654464
-64.717440	-7.322763	9.664461
-62.737668	-9.542675	9.674458
-61.376494	-11.682847	9.684455
-59.292409	-5.174937	9.694451
-57.385608	-11.554902	9.704448
-55.592457	-8.700156	9.714445
-53.753373	-6.250641	9.724442
-51.727644	-9.936865	9.734439
-49.905708	-11.064189	9.744435
-47.937636	-5.106198	9.754432
-46.177559	-5.050459	9.764429
-44.279336	-6.796282	9.774426
-42.408107	-7.121440	9.784423
-40.770792	-8.677214	9.794419
-38.568367	-10.552087	9.804416
-36.696254	-14.565909	9.814413
-34.955980	-8.985266	9.824410
-33.137333	-17.135411	9.834407
-30.952901	-8.849748	9.844403
-29.261659	-7.912991	9.854400
-27.374888	-9.236962	9.864397
-25.425479	-12.790987	9.874394
-23.681843	-8.377746	9.884391
-21.397580	-9.071940	9.894387
-20.007677	-5.933362	9.904384
-18.021592	-3.134625	9.914381
-16.079377	-6.700128	9.924378
-14.129429	-10.824248	9.934375
-12.168611	-6.668279	9.944371
-10.524041	-2.599235	9.954368
-8.770248	-7.104180	9.964365
-7.133502	-2.236494	9.974362
-5.319035	22.457142	9.984359
-4.221558	46.426739	9.994355
-2.553231	93.712470	10.004352
-1.153767	149.368942	10.014349
0.000000	196.986019	10.019354
0.390036	232.467087	10.024359
1.759799	260.401340	10.029363
2.174037	290.066643	10.034368
2.557892	302.843930	10.039373
2.731150	312.677426	10.044378
2.882199	326.550041	10.049383
3.231842	339.345434	10.054387
3.248860	352.712730	10.059392
3.218282	361.695644	10.064397
3.762417	361.124804	10.069402
3.775342	362.185745	10.074407
3.870623	355.679651	10.079411
3.665095	364.461805	10.084416
3.979089	370.816076	10.089421
3.764800	360.792149	10.094426
3.791193	366.124652	10.099431
4.365197	362.251510	10.104435
4.015627	370.886325	10.109440
4.054870	375.256380	10.114445
4.203708	371.506246	10.119450
4.164966	382.988469	10.124455
4.568496	370.899449	10.129459
4.290720	376.867123	10.134464
4.012879	364.424725	10.139469
4.201639	370.516685	10.144474
4.385994	390.684228	10.149479
4.493568	376.658522	10.154483
4.059710	378.513002	10.159488
4.224794	382.227449	10.164493
4.460879	384.474985	10.169498
4.326670	395.010464	10.174503
4.506519	393.627214	10.179507
4.466163	396.450300	10.184512
4.546427	395.425147	10.189517
4.587232	394.959821	10.194522
4.413186	397.991897	10.199527
4.829072	395.561706	10.204531
4.460584	402.013810	10.209536
4.643436	404.717714	10.214541
4.700894	407.400617	10.219546
4.713115	414.463812	10.224551
5.061820	418.816060	10.229555
5.065044	429.640316	10.234560
5.271989	432.857645	10.239565
5.151525	425.032847	10.244570
5.343969	424.309934	10.249575
5.295773	410.633908	10.254579
5.047793	414.638186	10.259584
4.850361	421.022011	10.264589
5.541996	435.111293	10.269594
5.339839	442.483098	10.274599
5.881729	444.093637	10.279603
5.544851	439.662411	10.284608
5.144582	432.569821	10.289613
5.598232	440.787966	10.294618
5.209571	444.486670	10.299623
5.718080	443.615567	10.304627
5.612804	448.560654	10.309632
5.835922	444.549483	10.314637
5.927281	443.987779	10.319642
5.824981	455.527507	10.324647
6.002160	444.621028	10.329651
5.867833	461.502519	10.334656
5.971025	449.182207	10.339661
6.184151	459.075678	10.344666
5.965234	463.461704	10.349671
6.187397	451.027793	10.354675
6.140959	456.895518	10.359680
6.291604	457.813069	10.364685
6.237212	463.395048	10.369690
5.898893	461.145071	10.374695
6.060252	460.635282	10.379699
6.046577	462.515796	10.384704
6.233839	463.477971	10.389709
6.217435	458.388467	10.394714
6.157038	468.131598	10.399719
6.384319	473.854742	10.404723
6.197203	472.008021	10.409728
6.696499	496.206822	10.414733
6.913381	504.114245	10.419738
6.828757	495.040993	10.424743
6.720533	494.580511	10.429747
6.776952	496.370997	10.434752
6.886902	496.020801	10.439757
6.673456	489.649050	10.444762
6.767760	506.836341	10.449767
7.025004	504.177535	10.454771
6.943683	502.438520	10.459776
7.007212	499.624523	10.464781
6.600152	502.816796	10.469786
6.730610	512.111601	10.474791
7.007392	509.463871	10.479795
6.984715	515.111777	10.484800
6.894972	506.391012	10.489805
7.271018	513.747903	10.494810
6.871230	524.426766	10.499815
7.289539	529.441338	10.504819
7.378384	546.263675	10.509824
7.209685	541.188972	10.514829
7.542771	554.411418	10.519834
7.329207	548.214711	10.524839
7.566044	536.994280	10.529843
7.274282	550.570290	10.534848
7.621984	551.517920	10.539853
7.940531	539.882309	10.544858
7.995656	554.738742	10.549863
7.919324	549.141497	10.554867
7.879870	550.597181	10.559872
7.998477	554.405822	10.564877
7.829927	556.508181	10.569882
8.131724	557.912588	10.574887
7.905780	551.965449	10.579891
8.013127	566.666900	10.584896
8.173262	551.975017	10.589901
8.265169	555.521399	10.594906
7.946789	555.133860	10.599911
8.093000	565.241515	10.604915
8.287111	573.105297	10.609920
8.432744	575.450874	10.614925
8.361588	576.816994	10.619930
8.045168	583.331839	10.624935
8.506223	575.409475	10.629939
8.771619	585.081795	10.634944
8.783276	586.830544	10.639949
8.589443	584.051272	10.644954
8.638381	583.605145	10.649959
8.580392	590.933528	10.654963
8.871244	592.883764	10.659968
8.627304	588.289426	10.664973
8.841766	591.231187	10.669978
8.490216	596.679254	10.674983
8.896221	595.666789	10.679987
8.968896	592.570603	10.684992
8.595463	595.391658	10.689997
9.011250	593.130194	10.695002
8.703760	594.750066	10.700007
8.629270	596.231844	10.705011
9.041521	611.668497	10.710016
9.051674	619.397633	10.715021
9.178381	622.041143	10.720026
9.364874	631.577838	10.725031
9.799698	618.985277	10.730035
9.663446	628.906204	10.735040
9.682490	628.100547	10.740045
9.703413	612.107668	10.745050
9.428324	599.180477	10.750055
9.217310	613.795552	10.755059
9.724709	629.436257	10.760064
9.413628	641.428927	10.765069
9.770032	635.369942	10.770074
9.640809	645.747103	10.775079
9.996105	631.495548	10.780083
9.566388	629.517181	10.785088
9.549435	631.428203	10.790093
10.023547	633.342906	10.795098
9.827797	638.401841	10.800103
9.943439	635.601584	10.805107
9.796176	642.463234	10.810112
9.752763	644.979332	10.815117
10.071543	632.999815	10.820122
9.726860	644.078430	10.825127
10.281028	657.959608	10.830131
10.301647	668.341272	10.835136
10.440044	664.379827	10.840141
10.648462	666.611319	10.845146
10.258729	671.912531	10.850151
10.652749	660.687435	10.855155
10.414775	675.428305	10.860160
10.614342	670.094532	10.865165
10.895543	666.931951	10.870170
10.445514	669.812549	10.875175
10.671953	657.078141	10.880179
10.942969	670.581846	10.885184
10.733752	667.663078	10.890189
10.778279	666.498518	10.895194
10.582928	682.055815	10.900199
10.818598	670.143143	10.905203
10.494959	669.078308	10.910208
10.750202	674.398079	10.915213
10.808812	675.338209	10.920218
10.451826	671.741222	10.925223
10.873791	678.636683	10.930227
10.848050	686.459895	10.935232
11.196301	695.226464	10.940237
11.421166	700.921696	10.945242
11.151152	707.444965	10.950247
11.638546	705.287188	10.955251
11.557187	711.004458	10.960256
11.690936	702.981258	10.965261
11.378440	693.666666	10.970266
11.076162	698.485554	10.975271
11.251764	706.019603	10.980275
11.193062	698.385091	10.985280
11.285926	710.355969	10.990285
11.474793	710.131962	10.995290
11.661751	714.033829	11.000295
11.357738	699.269164	11.005299
11.592811	717.877254	11.010304
11.988368	732.709534	11.015309
12.186363	727.292407	11.020314
11.903481	729.867217	11.025319
12.164288	718.123973	11.030323
11.871973	722.651101	11.035328
12.099792	725.105027	11.040333
12.375197	729.495872	11.045338
12.053167	742.028146	11.050343
12.419935	738.785666	11.055347
12.208051	737.436479	11.060352
12.125381	736.501949	11.065357
12.571853	732.186976	11.070362
12.377423	742.643997	11.075367
12.531983	735.172583	11.080371
12.227318	739.901972	11.085376
12.530827	739.962474	11.090381
12.625328	745.752640	11.095386
12.390402	748.466470	11.100391
12.708076	743.107525	11.105395
12.345179	745.990010	11.110400
12.265588	756.431877	11.115405
12.626203	746.472113	11.120410
12.353452	750.969320	11.125415
12.541900	748.914416	11.130419
12.897370	754.153571	11.135424
12.722302	768.589592	11.140429
13.071680	774.422699	11.145434
13.061995	781.361825	11.150439
13.353360	772.679469	11.155443
13.270598	782.989388	11.160448
13.664071	770.138347	11.165453
13.294433	749.914857	11.170458
12.987495	754.382823	11.175463
13.426085	758.313958	11.180467
13.348067	766.371070	11.185472
13.544486	762.111743	11.190477
13.267103	753.881259	11.195482
13.139728	762.687459	11.200487
13.642776	767.669675	11.205491
13.473549	776.954099	11.210496
13.540300	784.071859	11.215501
14.090905	774.994891	11.220506
13.642404	780.480568	11.225511
13.724876	779.819337	11.230515
13.797514	785.419027	11.235520
13.797407	775.379574	11.240525
13.734541	780.221808	11.245530
13.819513	780.708278	11.250535
14.099595	779.250654	11.255539
13.999283	780.367537	11.260544
14.083430	775.933711	11.265549
14.039815	778.754237	11.270554
14.344705	781.665845	11.275559
14.539099	769.370141	11.280563
14.413183	775.963503	11.285568
14.070251	779.437361	11.290573
14.049526	782.126495	11.295578
13.798179	780.102308	11.300583
14.097665	778.860801	11.305587
14.073916	782.430417	11.310592
14.163839	782.819897	11.315597
14.592249	788.605710	11.320602
14.252537	805.709605	11.325607
14.704911	799.867075	11.330611
14.760457	810.388358	11.335616
14.705575	810.537566	11.340621
15.167546	802.495077	11.345626
15.073783	812.196449	11.350631
15.567251	794.686563	11.355635
14.846039	786.414879	11.360640
14.625896	785.234173	11.365645
15.028449	783.310707	11.370650
15.051819	779.651448	11.375655
14.770482	778.642941	11.380659
15.082531	790.451182	11.385664
14.983555	799.413735	11.390669
15.218812	809.114669	11.395674
15.036248	808.990907	11.400679
15.441729	805.100374	11.405683
15.425822	816.530407	11.410688
14.991061	813.529303	11.415693
15.194444	812.296813	11.420698
14.768775	825.135869	11.425703
15.469936	814.998730	11.430707
15.104428	819.359355	11.435712
15.463837	808.768915	11.440717
15.730371	821.675770	11.445722
15.762549	847.861068	11.450727
16.052953	835.706125	11.455731
15.670046	809.663718	11.460736
15.678692	815.975420	11.465741
16.280512	823.094594	11.470746
15.782646	819.455380	11.475751
15.730484	801.907925	11.480755
15.819864	824.098821	11.485760
16.366582	830.797826	11.490765
16.484047	836.349382	11.495770
15.964213	824.038233	11.500775
16.057057	810.131161	11.505779
16.176459	827.556120	11.510784
15.848691	832.726071	11.515789
16.498313	834.054528	11.520794
16.760186	842.920126	11.525799
16.658534	830.020262	11.530803
15.937839	828.361108	11.535808
16.316052	836.175168	11.540813
16.379380	839.842881	11.545818
16.262789	843.409972	11.550823
16.184273	839.880499	11.555827
16.543236	842.310374	11.560832
16.369784	849.354506	11.565837
16.610609	838.284606	11.570842
16.545708	843.740664	11.575847
16.479627	838.644757	11.580851
16.731752	862.279579	11.585856
17.155777	862.383943	11.590861
17.177481	863.717931	11.595866
17.008958	871.929896	11.600871
17.170063	859.486451	11.605875
17.154306	846.009859	11.610880
16.849587	849.572263	11.615885
17.146770	862.934769	11.620890
17.289874	871.596962	11.625895
17.327921	858.040809	11.630899
17.320577	866.369000	11.635904
17.198344	868.610682	11.640909
17.724103	867.586985	11.645914
17.494184	866.403100	11.650919
17.908287	866.736145	11.655923
17.535664	862.122817	11.660928
17.268604	855.515009	11.665933
17.817300	867.862776	11.670938
17.503414	869.270793	11.675943
17.796811	866.159845	11.680947
17.719647	875.388644	11.685952
17.544512	878.810529	11.690957
17.743840	875.088486	11.695962
17.668209	880.759174	11.700967
17.661104	877.618877	11.705971
17.817541	868.547946	11.710976
17.918583	870.602618	11.715981
17.938659	874.404981	11.720986
17.700154	875.122834	11.725991
17.788603	872.814185	11.730995
18.015746	892.349504	11.736000
18.071241	904.184565	11.741005
18.416736	904.817159	11.746010
18.212008	906.184112	11.751015
18.307363	906.985922	11.756019
18.560141	906.190281	11.761024
18.226111	908.502023	11.766029
18.648997	909.103348	11.771034
18.601357	905.680906	11.776039
18.914889	907.853090	11.781043
18.528531	906.769853	11.786048
18.475817	909.801606	11.791053
18.809729	905.774217	11.796058
18.728075	905.762102	11.801063
18.751445	900.871119	11.806067
18.749836	911.614497	11.811072
18.626556	905.570406	11.816077
18.621783	900.130359	11.821082
18.644803	909.343200	11.826087
18.845199	907.707448	11.831091
18.857878	907.908963	11.836096
18.630660	907.566801	11.841101
18.920673	914.522850	11.846106
19.003312	928.421146	11.851111
19.207668	930.658060	11.856115
19.495216	929.013136	11.861120
19.203314	935.358633	11.866125
19.681491	929.933016	11.871130
19.460648	942.140215	11.876135
19.563647	932.595182	11.881139
19.756659	933.510738	11.886144
19.559909	940.063428	11.891149
19.718317	934.177838	11.896154
19.467138	936.818596	11.901159
19.666664	934.034867	11.906163
19.576682	940.471173	11.911168
19.789241	935.217239	11.916173
19.876056	930.448601	11.921178
19.759044	939.584441	11.926183
19.927590	933.146835	11.931187
19.901193	932.089768	11.936192
19.647152	944.002619	11.941197
19.948836	930.811235	11.946202
19.759594	935.859772	11.951207
19.871613	934.859481	11.956211
19.514629	932.456275	11.961216
19.694435	945.977940	11.966221
19.875253	956.731681	11.971226
20.358603	971.854581	11.976231
20.212181	963.850690	11.981235
20.363462	976.168890	11.986240
20.269891	970.765059	11.991245
20.505064	960.864584	11.996250
20.627197	965.519665	12.001255
20.587896	961.800965	12.006259
20.783601	963.575602	12.011264
20.560551	970.485766	12.016269
20.589532	962.029666	12.021274
20.552424	967.328360	12.026279
20.849461	969.820178	12.031283
20.669129	961.365921	12.036288
20.679025	964.550139	12.041293
20.577248	961.707221	12.046298
20.430459	964.132622	12.051303
20.790171	959.274713	12.056307
20.599380	965.433771	12.061312
20.774161	961.890677	12.066317
20.987285	954.550171	12.071322
20.800437	964.605562	12.076327
20.804086	956.278095	12.081331
20.706500	968.063501	12.086336
20.550540	964.639397	12.091341
21.112317	960.889487	12.096346
21.001943	966.136784	12.101351
20.979509	954.138881	12.106355
20.777248	950.528184	12.111360
20.618326	942.953687	12.116365
21.017992	926.920556	12.121370
20.686989	939.443390	12.126375
20.862704	927.081142	12.131379
20.958718	929.354261	12.136384
20.932304	928.322430	12.141389
20.696327	927.670980	12.146394
20.681427	935.106213	12.151399
20.829148	929.373730	12.156403
20.943310	934.999974	12.161408
20.824896	931.451608	12.166413
21.062597	932.530360	12.171418
20.672025	930.417962	12.176423
20.709942	929.401103	12.181427
20.875811	929.489869	12.186432
20.478893	922.185173	12.191437
20.683297	913.246923	12.196442
20.582821	918.306529	12.201447
20.899279	916.051399	12.206451
20.639432	909.611163	12.211456
20.425809	905.940783	12.216461
20.741323	912.518997	12.221466
20.623212	918.384147	12.226471
20.462752	910.671129	12.231475
20.522625	920.811728	12.236480
20.474474	931.736023	12.241485
20.825788	929.730818	12.246490
20.855714	938.352750	12.251495
20.841898	933.040299	12.256499
20.955762	931.714837	12.261504
20.353824	922.845262	12.266509
20.745716	918.589407	12.271514
20.819606	916.130097	12.276519
20.553580	915.349389	12.281523
20.898679	911.656131	12.286528
20.362823	916.190621	12.291533
20.747893	912.399517	12.296538
20.569354	911.101769	12.301543
20.468118	909.908394	12.306547
20.801890	927.078491	12.311552
20.716923	938.254687	12.316557
21.176180	920.780071	12.321562
20.475615	919.434687	12.326567
20.680817	910.521545	12.331571
20.669820	915.745088	12.336576
20.465836	917.214433	12.341581
20.834248	915.217542	12.346586
20.428474	916.397349	12.351591
20.791840	912.172857	12.356595
20.542092	905.238964	12.361600
20.774750	912.724595	12.366605
20.782507	911.745666	12.371610
21.043266	912.439087	12.376615
20.779288	912.257342	12.381619
20.831468	918.011745	12.386624
20.823413	916.309884	12.391629
21.052064	916.292435	12.396634
20.855628	922.367213	12.401639
20.952948	922.660893	12.406643
21.025027	920.477858	12.411648
20.830329	925.151918	12.416653
21.054415	911.073995	12.421658
20.504499	902.358574	12.426663
20.809724	894.910360	12.431667
20.750066	889.952192	12.436672
20.528317	889.956114	12.441677
20.865180	882.698417	12.446682
20.470366	894.419199	12.451687
20.752813	895.569666	12.456691
20.658659	887.347730	12.461696
20.892983	894.776311	12.466701
20.687044	881.930883	12.471706
20.497700	888.365666	12.476711
20.703098	887.793642	12.481715
20.809850	883.668438	12.486720
20.678041	885.607275	12.491725
20.992375	891.507527	12.496730
20.471821	892.601553	12.501735
20.716467	894.262711	12.506739
20.659043	897.023957	12.511744
20.603137	896.252318	12.516749
20.684964	900.276668	12.521754
20.459570	894.698334	12.526759
20.185687	899.653117	12.531763
20.733034	886.914637	12.536768
20.708125	897.175983	12.541773
20.881351	882.415442	12.546778
20.434996	901.891027	12.551783
20.469543	899.810183	12.556787
20.515163	896.992658	12.561792
20.374338	908.890577	12.566797
21.018721	924.358356	12.571802
20.679761	925.491234	12.576807
20.653558	904.395825	12.581811
20.774774	904.269345	12.586816
20.863845	903.488776	12.591821
21.020531	892.810753	12.596826
20.928789	896.974758	12.601831
21.174071	903.843312	12.606835
20.981526	895.383156	12.611840
20.630740	900.861177	12.616845
20.863142	898.862325	12.621850
20.763630	902.459825	12.626855
20.593673	901.733187	12.631859
20.758339	903.643664	12.636864
20.733807	903.461578	12.641869
20.541992	897.598744	12.646874
20.786495	900.710833	12.651879
20.572118	901.883768	12.656883
20.697606	900.222115	12.661888
20.260096	905.062638	12.666893
20.613643	908.310313	12.671898
20.694331	906.657382	12.676903
20.735592	904.274246	12.681907
20.742505	905.809308	12.686912
20.643673	904.675480	12.691917
20.800796	898.269675	12.696922
20.557946	904.331347	12.701927
21.045779	895.387329	12.706931
20.805493	896.329412	12.711936
20.498578	905.673728	12.716941
20.834785	899.409684	12.721946
20.707579	898.076940	12.726951
20.862152	901.706459	12.731955
20.118085	888.533663	12.736960
20.510287	899.849781	12.741965
20.510543	897.895841	12.746970
20.358056	906.485343	12.751975
20.314858	900.034212	12.756979
20.634535	900.305043	12.761984
20.601962	906.136042	12.766989
20.908331	901.892257	12.771994
20.603206	912.226694	12.776999
20.762053	903.208978	12.782003
20.739531	912.321844	12.787008
20.524358	908.531854	12.792013
20.625212	903.470804	12.797018
20.520115	911.830383	12.802023
20.429332	915.776604	12.807027
20.605285	910.457550	12.812032
20.597764	915.350930	12.817037
20.823987	898.033368	12.822042
20.466669	918.344815	12.827047
20.724585	902.367438	12.832051
20.735308	903.064466	12.837056
20.550186	912.976034	12.842061
20.852908	900.681867	12.847066
20.086498	913.958575	12.852071
20.470961	912.320275	12.857075
20.759932	909.755692	12.862080
20.743878	909.069167	12.867085
20.665758	907.403715	12.872090
20.413758	914.987150	12.877095
20.895418	906.758524	12.882099
20.907950	913.353522	12.887104
20.253735	914.588725	12.892109
20.699473	915.128054	12.897114
20.675729	913.751995	12.902119
20.787488	910.679472	12.907123
20.839388	905.750818	12.912128
20.774965	915.416037	12.917133
20.943757	913.544033	12.922138
20.625478	910.489633	12.927143
20.766915	916.747080	12.932147
20.547615	911.804905	12.937152
20.587205	908.253423	12.942157
20.756796	910.106341	12.947162
20.611964	916.967732	12.952167
20.508933	918.495098	12.957171
20.694212	927.426585	12.962176
20.702020	921.435701	12.967181
20.842729	920.156424	12.972186
20.507204	928.426599	12.977191
20.856624	923.120877	12.982195
20.668971	928.227509	12.987200
20.513472	921.636573	12.992205
20.712639	923.099969	12.997210
20.660106	927.090559	13.002215
20.822873	920.772161	13.007219
21.081095	925.310898	13.012224
20.665660	923.850644	13.017229
20.868021	918.008518	13.022234
20.577937	930.233059	13.027239
20.578905	921.030762	13.032243
20.987985	925.286797	13.037248
20.666670	925.598358	13.042253
20.768553	922.680384	13.047258
20.882917	923.064392	13.052263
20.959055	924.602609	13.057267
20.667075	922.425598	13.062272
20.928645	924.358472	13.067277
20.527451	914.895444	13.072282
20.587355	904.010481	13.077287
20.542721	913.308239	13.082291
20.986851	919.987377	13.087296
20.432316	908.399258	13.092301
20.381681	915.684050	13.097306
20.680219	927.005666	13.102311
20.784783	923.727691	13.107315
20.964726	925.938533	13.112320
20.194847	921.024242	13.117325
20.739178	916.557980	13.122330
20.479593	930.698534	13.127335
20.305837	923.388208	13.132339
20.699294	931.568925	13.137344
20.751569	926.072457	13.142349
20.807030	933.026498	13.147354
20.950950	925.648154	13.152359
20.588645	932.536353	13.157363
20.762271	930.744006	13.162368
20.799376	933.423945	13.167373
20.962335	926.815331	13.172378
20.071196	916.828005	13.177383
20.455818	924.820878	13.182387
21.149526	921.083054	13.187392
20.489843	925.665685	13.192397
21.009747	927.361798	13.197402
20.978094	913.289967	13.202407
20.654037	909.118343	13.207411
20.390172	901.363472	13.212416
20.474935	899.705160	13.217421
20.843710	910.731687	13.222426
20.452884	916.410081	13.227431
20.646967	919.407204	13.232435
21.118853	922.285897	13.237440
20.582116	912.112727	13.242445
20.470283	897.359787	13.247450
20.472846	905.484555	13.252455
20.806792	919.923124	13.257459
20.639795	922.115179	13.262464
20.997663	923.753552	13.267469
20.963045	905.534493	13.272474
20.539842	910.910519	13.277479
20.485119	908.345557	13.282483
20.480117	894.614872	13.287488
20.584058	908.323658	13.292493
20.815377	899.325926	13.297498
20.387863	911.233301	13.302503
20.750330	914.541060	13.307507
20.764561	918.562004	13.312512
20.769450	919.460252	13.317517
21.019556	909.147391	13.322522
20.586563	910.845665	13.327527
20.774667	909.327000	13.332531
20.903148	899.427813	13.337536
20.416246	907.532872	13.342541
20.721746	900.901535	13.347546
20.524938	906.306110	13.352551
20.586064	912.079587	13.357555
20.616414	906.485690	13.362560
20.723069	907.443406	13.367565
20.760367	898.725798	13.372570
20.552642	902.160771	13.377575
20.255710	908.721541	13.382579
20.785732	904.957785	13.387584
20.667294	908.848487	13.392589
21.019891	902.432005	13.397594
20.934993	908.567842	13.402599
20.676061	906.910727	13.407603
20.851059	914.145337	13.412608
20.661652	915.740100	13.417613
21.007145	904.044705	13.422618
20.733476	911.142702	13.427623
20.809974	912.135192	13.432627
20.958205	908.097991	13.437632
20.774413	914.758998	13.442637
21.153654	908.694682	13.447642
21.098446	911.800957	13.452647
20.678392	880.320287	13.457651
20.757981	880.331344	13.462656
19.972193	884.716439	13.467661
20.560768	888.484906	13.472666
20.532237	905.468318	13.477671
20.688153	909.531320	13.482675
20.897999	909.622534	13.487680
20.959976	907.937892	13.492685
20.792597	894.665224	13.497690
20.629424	891.064078	13.502695
20.495209	884.308903	13.507699
20.850639	897.045517	13.512704
20.641812	895.979699	13.517709
20.470480	888.698968	13.522714
20.284400	891.422381	13.527719
20.610325	900.736727	13.532723
20.733622	913.499341	13.537728
20.949908	912.472959	13.542733
20.822720	909.876973	13.547738
20.428243	906.281175	13.552743
20.839515	914.616747	13.557747
20.769240	906.001455	13.562752
20.425337	896.114532	13.567757
20.873349	900.613528	13.572762
20.893380	906.951841	13.577767
20.724027	888.033571	13.582771
20.529150	879.406626	13.587776
20.370422	880.176415	13.592781
20.688661	888.794914	13.597786
20.617426	892.739588	13.602791
20.402027	909.036818	13.607795
20.928746	910.277645	13.612800
20.753542	911.330783	13.617805
20.757527	885.217069	13.622810
20.575972	881.085807	13.627815
20.586384	887.190662	13.632819
20.990197	899.424360	13.637824
20.528070	900.841830	13.642829
20.441546	883.526855	13.647834
20.539958	908.080469	13.652839
20.764656	911.583679	13.657843
20.999160	906.398802	13.662848
20.666118	889.927446	13.667853
20.851898	878.358478	13.672858
20.817705	881.707417	13.677863
20.853334	871.816751	13.682867
20.750430	871.916843	13.687872
20.596233	876.926652	13.692877
20.771981	869.450213	13.697882
20.567053	883.455838	13.702887
20.552711	876.473374	13.707891
20.499169	875.821216	13.712896
20.245441	877.386807	13.717901
20.574380	873.495848	13.722906
20.673994	882.653875	13.727911
20.992344	888.638647	13.732915
21.108779	876.013064	13.737920
20.812081	880.982519	13.742925
20.976001	880.322487	13.747930
20.932516	882.942724	13.752935
20.630668	875.972998	13.757939
20.685050	878.389954	13.762944
20.790198	882.864776	13.767949
20.908964	882.749727	13.772954
20.772388	891.910736	13.777959
20.721397	884.926228	13.782963
20.792165	877.324592	13.787968
20.633747	889.964948	13.792973
20.887556	877.741685	13.797978
20.869633	879.886301	13.802983
20.587439	877.688810	13.807987
20.974438	878.379443	13.812992
20.883638	876.181390	13.817997
20.836330	854.979024	13.823002
20.295650	864.357445	13.828007
20.625122	864.593594	13.833011
20.727689	855.704740	13.838016
20.607789	855.641952	13.843021
20.650939	851.630988	13.848026
20.545954	864.756423	13.853031
20.503544	858.344611	13.858035
20.799583	859.877711	13.863040
20.405573	871.615695	13.868045
20.803737	878.835195	13.873050
20.748380	872.296123	13.878055
20.569611	871.346948	13.883059
20.681522	872.978808	13.888064
20.372256	876.015202	13.893069
21.004672	873.826387	13.898074
20.696892	873.375641	13.903079
20.606321	870.832174	13.908083
20.872390	859.777156	13.913088
20.668945	862.897601	13.918093
20.691165	858.514632	13.923098
20.862455	860.261609	13.928103
20.558273	853.126673	13.933107
20.791415	851.238105	13.938112
20.672895	861.424463	13.943117
20.871820	853.384476	13.948122
20.701782	860.183624	13.953127
20.669737	863.981681	13.958131
20.799449	852.216658	13.963136
20.555088	865.503104	13.968141
20.451900	866.033782	13.973146
20.440668	859.273196	13.978151
20.668730	855.210660	13.983155
20.631644	856.774814	13.988160
20.319477	866.675072	13.993165
20.682411	855.699231	13.998170
20.666752	869.222037	14.003175
20.518165	878.072694	14.008179
20.913691	872.013682	14.013184
20.631112	875.335999	14.018189
20.529324	860.638203	14.023207
20.415509	862.902761	14.028224
20.752459	881.311966	14.033242
21.174290	884.353123	14.038259
20.644787	878.864364	14.043277
20.628482	872.472622	14.048295
20.717504	878.812057	14.053312
20.715987	880.784996	14.058330
20.999070	887.266518	14.063347
20.917640	895.849572	14.068365
20.954437	879.158472	14.073383
21.045406	875.162674	14.078400
20.982584	864.167754	14.083418
20.822758	865.986614	14.088435
20.443298	873.177853	14.093453
20.995123	884.809139	14.098471
21.050853	893.588969	14.103488
20.896666	890.555650	14.108506
20.814834	886.208306	14.113523
20.785219	896.290077	14.118541
21.066678	902.771864	14.123559
21.084072	905.632137	14.128576
20.827974	908.075127	14.133594
21.177074	901.922398	14.138611
20.812014	902.064091	14.143629
21.147549	902.926185	14.148647
21.279805	910.226164	14.153664
21.032808	905.035260	14.158682
21.341837	902.977281	14.163699
21.067609	907.041832	14.168717
21.033397	906.857045	14.173735
21.017789	904.331737	14.178752
21.087850	906.167419	14.183770
21.455176	904.402167	14.188787
21.124233	907.008108	14.193805
21.222533	901.752693	14.198823
21.233608	903.110138	14.203840
20.877518	903.200062	14.208858
20.874360	902.735038	14.213875
21.054163	914.307706	14.218893
21.264154	921.990128	14.223911
21.308544	931.950006	14.228928
21.158409	932.623719	14.233946
21.468603	937.417772	14.238963
21.162918	938.679447	14.243981
21.501796	935.707477	14.248999
21.739099	935.241853	14.254016
21.579089	942.261268	14.259034
21.801574	938.400210	14.264051
21.537279	936.029394	14.269069
21.484882	935.086149	14.274087
21.285717	937.427254	14.279104
21.258693	934.966684	14.284122
21.897508	934.194769	14.289139
21.386562	941.204089	14.294157
21.378822	927.987048	14.299175
21.640994	926.767111	14.304192
21.290444	936.925267	14.309210
21.360716	937.209888	14.314227
21.374999	938.629746	14.319245
22.124195	950.320842	14.324263
21.627623	949.088211	14.329280
21.828639	953.139897	14.334298
22.059626	958.552217	14.339315
21.920554	953.540714	14.344333
21.789508	932.674691	14.349351
22.055074	927.545175	14.354368
21.552591	936.500583	14.359386
21.846735	933.611255	14.364403
22.076788	957.672285	14.369421
22.184631	955.190201	14.374439
21.927455	939.569978	14.379456
21.783734	939.141530	14.384474
21.958594	927.433813	14.389491
21.825005	939.960991	14.394509
21.994760	955.681866	14.399527
22.384463	959.404579	14.404544
22.060422	960.165806	14.409562
21.992216	949.942478	14.414579
22.071488	950.132854	14.419597
22.269471	953.856255	14.424615
22.018918	960.202695	14.429632
22.079718	971.147862	14.434650
22.238881	959.837460	14.439667
22.217381	968.702014	14.444685
21.904575	965.978701	14.449703
22.475281	961.321186	14.454720
22.269211	960.583351	14.459738
22.164549	964.977957	14.464755
22.165123	969.936237	14.469773
22.251452	966.818921	14.474791
22.544654	967.819907	14.479808
22.110991	977.124593	14.484826
22.420740	965.363870	14.489843
22.327062	974.040161	14.494861
22.138160	973.137562	14.499879
22.316018	966.735261	14.504896
21.965075	968.867766	14.509914
22.271009	970.272571	14.514931
22.152247	965.259398	14.519949
22.535424	966.562218	14.524967
22.409577	972.283146	14.529984
22.633657	991.855680	14.535002
22.780450	985.747767	14.540019
22.545090	981.383983	14.545037
22.393454	983.099302	14.550055
22.488646	987.477768	14.555072
22.576888	999.923998	14.560090
22.768023	1000.485079	14.565107
22.906100	1000.198877	14.570125
22.968294	999.187013	14.575143
22.928333	973.245869	14.580160
22.709118	975.190620	14.585178
22.902754	965.808004	14.590195
22.569174	956.402515	14.595213
22.514245	960.526486	14.600231
22.947218	978.697126	14.605248
23.008822	984.732660	14.610266
22.961400	968.866588	14.615283
22.734772	972.195239	14.620301
22.666167	974.885194	14.625319
23.058195	977.548872	14.630336
22.862895	994.954557	14.635354
23.408173	990.673905	14.640371
23.207148	974.903113	14.645389
22.838208	966.145065	14.650407
23.175670	965.325257	14.655424
22.894929	958.327555	14.660442
23.018657	960.088616	14.665459
22.758380	961.473614	14.670477
22.779986	987.493363	14.675495
22.992226	990.541230	14.680512
23.084831	996.378339	14.685530
22.977638	991.067576	14.690547
22.974630	987.914167	14.695565
22.940090	995.610461	14.700583
23.429919	986.720149	14.705600
23.392701	987.394730	14.710618
23.703219	984.320306	14.715635
23.639020	982.795335	14.720653
23.373284	992.449208	14.725671
23.579720	984.599844	14.730688
23.516540	996.300997	14.735706
23.482395	980.011214	14.740723
23.605993	968.431193	14.745741
23.186443	955.114639	14.750759
23.401225	958.004788	14.755776
23.707059	984.183695	14.760794
23.497970	972.014925	14.765811
23.543593	965.337980	14.770829
23.325125	966.148437	14.775847
23.652607	970.604683	14.780864
23.270513	974.389148	14.785882
23.455607	974.257473	14.790899
23.734714	986.772352	14.795917
23.514796	994.704284	14.800935
23.377839	993.870479	14.805952
23.567782	1001.161302	14.810970
23.367959	997.109603	14.815987
23.530408	993.130688	14.821005
23.593841	993.933938	14.826023
23.802721	982.381203	14.831040
23.682215	988.623540	14.836058
23.415021	993.102281	14.841075
23.874352	994.728019	14.846093
23.543484	989.825748	14.851111
23.762411	987.667295	14.856128
23.519751	989.436459	14.861146
23.738332	990.265301	14.866163
23.981995	1007.248622	14.871181
23.891361	1002.695003	14.876199
23.991459	998.411419	14.881216
23.913425	1008.000757	14.886234
23.987786	1009.478681	14.891251
24.126488	1014.402361	14.896269
23.815035	1012.086246	14.901287
23.808423	1010.699956	14.906304
23.962760	1022.706217	14.911322
24.213894	1020.984653	14.916339
24.103536	1025.391197	14.921357
24.004643	1021.043387	14.926375
24.150096	1012.045961	14.931392
24.009593	1027.662239	14.936410
24.169164	1015.736661	14.941427
23.895429	1014.122408	14.946445
24.153378	1020.538784	14.951463
24.238386	1018.194041	14.956480
23.911591	1023.121181	14.961498
24.106363	1025.558348	14.966515
24.058407	1024.040220	14.971533
23.920736	1021.825377	14.976551
24.098400	1020.644081	14.981568
24.198904	1047.747778	14.986586
24.711500	1054.836153	14.991603
24.709495	1050.161414	14.996621
24.732578	1045.633690	15.001639
24.569625	1026.334676	15.006656
24.380934	1025.107989	15.011674
24.197846	1019.084138	15.016691
24.540977	1029.373971	15.021709
24.317032	1042.173631	15.026727
24.672722	1043.282637	15.031744
24.811030	1053.727854	15.036762
24.596704	1045.797699	15.041779
25.012267	1042.354142	15.046797
24.428929	1033.479234	15.051815
24.925342	1029.391986	15.056832
24.671679	1023.211073	15.061850
24.768798	1030.828183	15.066867
24.783932	1028.496157	15.071885
24.688358	1041.273768	15.076903
25.037421	1035.193351	15.081920
24.825403	1027.457898	15.086938
24.741092	1012.093177	15.091955
24.994514	1011.831051	15.096973
24.999915	1010.707119	15.101991
24.928505	1015.182954	15.107008
24.824632	1014.686798	15.112026
25.040327	1023.582769	15.117043
25.026146	1013.970566	15.122061
25.000730	1021.382267	15.127079
25.248394	1016.305914	15.132096
24.941363	1012.208387	15.137114
24.884005	1018.780447	15.142131
25.248407	1015.307303	15.147149
25.232435	1021.948271	15.152167
25.132545	1008.031684	15.157184
24.785456	1019.085990	15.162202
24.897752	1024.632099	15.167219
25.074954	1035.229979	15.172237
25.484940	1046.391650	15.177255
25.363506	1045.421654	15.182272
25.269420	1036.250055	15.187290
25.041928	1034.729100	15.192307
25.103385	1040.988057	15.197325
25.276642	1044.024850	15.202343
25.268475	1048.687242	15.207360
25.062437	1049.124477	15.212378
25.473850	1048.277140	15.217395
25.551453	1043.613303	15.222413
25.420987	1051.405152	15.227431
25.533311	1048.291538	15.232448
25.589688	1048.708942	15.237466
25.445234	1051.845175	15.242483
25.783563	1042.337183	15.247501
25.591906	1045.600496	15.252519
25.605302	1040.979935	15.257536
25.564520	1042.130153	15.262554
25.497367	1048.771431	15.267571
25.671463	1044.383220	15.272589
25.488100	1052.314071	15.277607
25.665929	1052.115912	15.282624
25.818293	1046.189562	15.287642
25.621812	1044.454443	15.292659
25.648303	1037.223651	15.297677
25.621711	1050.108248	15.302695
25.906154	1052.084366	15.307712
25.466352	1048.517679	15.312730
25.681249	1048.777662	15.317747
25.862339	1041.176136	15.322765
25.590310	1057.897266	15.327783
25.810423	1042.869360	15.332800
26.157349	1044.953491	15.337818
25.829355	1049.228009	15.342835
25.763419	1045.409778	15.347853
25.686090	1051.467500	15.352871
26.123688	1055.261252	15.357888
25.935356	1063.334478	15.362906
26.246377	1065.661872	15.367923
26.183377	1063.548374	15.372941
25.866847	1056.608243	15.377959
25.949801	1070.916316	15.382976
26.207536	1080.124949	15.387994
26.027661	1082.769749	15.393011
26.245021	1081.761446	15.398029
26.262506	1088.176878	15.403047
26.512809	1076.644204	15.408064
26.613761	1077.222818	15.413082
26.251748	1069.033053	15.418099
26.390964	1063.333742	15.423117
26.148660	1062.095152	15.428135
26.372268	1068.853663	15.433152
26.603957	1075.675385	15.438170
26.326343	1067.623174	15.443187
26.355071	1071.774734	15.448205
26.210558	1082.384633	15.453223
26.545961	1069.926011	15.458240
26.360168	1071.689261	15.463258
26.261667	1076.591018	15.468275
26.555150	1078.411538	15.473293
26.479973	1079.977816	15.478311
26.433156	1074.270418	15.483328
26.667939	1073.945195	15.488346
26.504592	1079.856195	15.493363
26.565966	1075.165047	15.498381
26.625561	1076.860844	15.503399
26.563056	1073.998485	15.508416
26.563601	1069.153442	15.513434
26.375114	1074.997661	15.518451
26.404690	1075.403610	15.523469
26.368355	1091.972353	15.528487
26.581761	1109.263436	15.533504
27.144088	1108.716079	15.538522
27.022343	1110.676764	15.543539
26.664550	1105.937627	15.548557
27.021831	1112.030665	15.553575
27.093025	1098.615257	15.558592
26.986096	1094.130277	15.563610
27.020723	1096.729855	15.568627
27.285613	1092.638617	15.573645
27.399415	1100.830421	15.578663
27.481604	1094.142865	15.583680
27.194726	1073.041938	15.588698
26.977962	1070.032718	15.593715
27.113536	1064.928607	15.598733
26.881690	1069.999499	15.603751
27.357924	1084.189801	15.608768
27.527031	1087.364122	15.613786
27.098896	1087.037662	15.618803
27.424819	1074.174696	15.623821
27.001884	1086.894445	15.628839
27.454376	1091.514840	15.633856
27.493757	1091.835853	15.638874
27.171246	1098.876542	15.643891
27.355142	1105.490389	15.648909
27.296475	1102.967195	15.653927
27.612957	1099.485944	15.658944
27.544417	1095.918233	15.663962
27.599218	1102.417385	15.668979
27.725290	1099.402244	15.673997
27.424512	1093.208365	15.679015
27.278608	1105.924059	15.684032
27.860116	1091.089368	15.689050
27.388884	1096.975546	15.694067
27.534367	1100.246449	15.699085
27.669495	1101.974248	15.704103
27.651331	1100.858787	15.709120
27.668105	1093.580752	15.714138
27.623934	1103.558019	15.719155
27.338277	1094.147942	15.724173
27.681759	1091.609375	15.729191
27.511329	1098.404005	15.734208
27.829311	1095.112857	15.739226
27.974243	1095.527150	15.744243
27.913044	1099.299793	15.749261
27.742326	1097.914498	15.754279
27.744070	1094.945930	15.759296
28.186889	1088.377043	15.764314
27.643961	1100.725821	15.769331
27.825746	1092.076492	15.774349
27.858166	1098.020771	15.779367
27.865819	1103.331909	15.784384
28.040838	1109.858296	15.789402
28.168887	1123.543370	15.794419
28.125828	1114.602690	15.799437
28.091212	1123.642468	15.804455
28.308582	1127.548446	15.809472
28.608198	1121.313853	15.814490
27.573213	1114.802111	15.819507
27.905032	1120.087508	15.824525
28.303459	1119.234374	15.829543
28.415938	1123.276633	15.834560
28.793079	1122.673079	15.839578
28.520580	1129.019159	15.844595
28.689546	1118.868786	15.849613
28.634654	1105.699218	15.854631
28.511054	1100.622273	15.859648
28.670745	1084.830009	15.864666
28.494891	1096.148080	15.869683
28.540529	1095.604479	15.874701
28.526409	1092.054832	15.879719
28.587759	1094.785432	15.884736
28.926528	1082.159517	15.889754
28.504988	1096.452122	15.894771
28.440912	1095.966919	15.899789
28.631110	1094.267651	15.904807
28.641425	1086.929299	15.909824
28.848676	1086.471610	15.914842
28.557465	1090.397344	15.919859
28.722910	1092.966618	15.924877
28.742357	1090.254784	15.929895
28.582257	1101.092132	15.934912
28.809931	1116.465734	15.939930
28.866087	1115.988097	15.944947
29.191927	1114.335620	15.949965
29.060128	1126.603903	15.954983
28.808020	1114.363221	15.960000
29.256362	1100.662708	15.965018
28.848773	1098.739449	15.970035
28.932010	1101.543640	15.975053
29.086194	1113.790682	15.980071
28.927437	1115.205908	15.985088
29.436538	1114.075565	15.990106
29.136464	1105.577016	15.995123
29.090819	1094.400639	16.000141
28.743316	1097.449713	16.005159
29.224222	1109.495986	16.010176
29.086641	1121.909124	16.015194
28.976243	1123.908113	16.020211
28.918051	1125.587308	16.025229
29.061430	1118.508512	16.030247
29.057442	1119.300499	16.035264
29.232888	1117.796282	16.040282
28.955719	1118.907915	16.045299
29.149935	1118.506575	16.050317
29.691089	1132.821856	16.055335
29.589932	1140.513121	16.060352
29.621884	1125.010970	16.065370
29.627704	1130.637025	16.070387
29.430026	1128.244540	16.075405
29.485229	1120.596196	16.080423
29.636063	1126.840934	16.085440
29.670553	1117.340454	16.090458
29.509409	1124.832846	16.095475
29.545103	1144.279898	16.100493
30.001811	1141.294601	16.105511
29.625118	1151.640338	16.110528
29.709794	1144.880788	16.115546
29.930501	1144.962876	16.120563
29.653447	1154.514837	16.125581
30.206353	1153.488407	16.130599
29.668030	1141.615045	16.135616
29.748740	1150.710381	16.140634
29.687557	1149.534921	16.145651
29.989582	1148.272430	16.150669
29.759559	1151.803803	16.155687
29.389169	1155.061826	16.160704
29.846923	1159.108016	16.165722
29.719424	1156.243422	16.170739
29.948417	1152.389135	16.175757
30.166521	1146.569454	16.180775
29.555926	1154.341191	16.185792
29.992751	1163.017143	16.190810
29.739178	1170.227775	16.195827
29.848337	1175.607696	16.200845
30.087813	1178.028320	16.205863
30.251997	1181.279741	16.210880
30.372728	1167.897269	16.215898
30.455150	1181.786311	16.220915
30.290073	1171.848060	16.225933
30.563859	1160.442926	16.230951
30.635903	1162.974412	16.235968
30.647843	1159.329354	16.240986
30.730247	1172.013411	16.246003
30.543212	1162.109344	16.251021
30.847499	1158.652834	16.256039
30.395644	1170.862085	16.261056
31.042648	1160.209922	16.266074
31.262012	1152.483466	16.271091
30.915227	1148.282911	16.276109
31.038886	1125.540992	16.281127
30.761197	1129.896388	16.286144
31.349902	1131.259256	16.291162
30.997055	1136.242500	16.296179
30.902588	1141.182176	16.301197
31.151039	1132.467920	16.306215
30.898049	1135.097647	16.311232
30.781861	1122.479764	16.316250
31.078584	1130.485102	16.321267
30.680611	1134.909236	16.326285
30.766773	1134.514118	16.331303
31.143822	1134.060021	16.336320
30.982124	1126.386491	16.341338
30.697083	1133.265485	16.346355
30.837734	1127.860872	16.351373
31.220174	1130.316890	16.356391
30.562121	1137.362349	16.361408
31.069969	1135.678482	16.366426
30.963301	1133.254177	16.371443
31.104955	1133.716973	16.376461
31.268208	1140.843019	16.381479
31.027468	1137.220963	16.386496
31.142245	1129.169057	16.391514
31.006996	1138.044778	16.396531
31.238401	1137.923806	16.401549
31.336971	1134.732927	16.406567
31.126902	1148.648924	16.411584
31.289967	1151.136788	16.416602
31.440123	1157.181081	16.421619
31.279543	1160.124061	16.426637
31.405513	1154.807512	16.431655
31.301930	1167.404035	16.436672
31.723581	1162.152012	16.441690
31.411844	1159.006905	16.446707
31.105108	1158.134886	16.451725
31.500530	1154.463274	16.456743
31.349661	1159.924775	16.461760
31.283358	1160.350738	16.466778
31.685184	1169.133739	16.471795
31.604927	1178.392410	16.476813
31.962272	1186.869474	16.481831
31.944273	1187.964944	16.486848
31.958262	1187.369757	16.491866
32.111261	1189.108087	16.496883
31.911675	1180.983591	16.501901
31.828216	1163.089061	16.506919
31.661142	1159.867396	16.511936
31.826658	1174.645339	16.516954
32.066122	1179.550645	16.521971
32.116389	1189.228182	16.526989
32.245280	1178.256718	16.532007
32.359319	1192.249270	16.537024
32.364176	1159.944608	16.542042
32.182920	1149.898051	16.547059
32.062900	1145.545708	16.552077
32.400331	1138.652250	16.557095
32.146836	1148.199663	16.562112
32.197372	1146.392098	16.567130
32.277031	1137.386998	16.572147
32.057369	1154.757432	16.577165
32.559122	1157.392634	16.582183
32.142368	1175.494547	16.587200
32.469303	1172.194876	16.592218
32.491646	1171.252279	16.597235
32.233218	1172.270474	16.602253
32.486456	1158.767772	16.607271
32.502992	1174.008364	16.612288
32.521139	1178.191530	16.617306
32.562808	1178.741850	16.622323
32.554609	1174.834936	16.627341
32.571288	1162.778652	16.632359
32.279369	1182.535206	16.637376
32.603849	1174.338927	16.642394
32.924866	1168.928341	16.647411
32.564416	1175.578701	16.652429
32.924538	1160.157097	16.657447
32.458013	1177.349060	16.662464
32.593577	1171.037574	16.667482
32.944021	1162.894578	16.672499
32.739104	1173.925538	16.677517
32.998474	1185.600568	16.682535
33.032697	1192.508110	16.687552
33.059040	1195.351282	16.692570
33.363750	1183.876702	16.697587
33.176078	1183.548067	16.702605
32.904942	1173.045477	16.707623
33.025999	1185.022575	16.712640
33.419472	1197.852890	16.717658
33.317326	1182.419258	16.722675
32.959319	1179.211524	16.727693
33.024594	1185.845901	16.732711
33.171819	1203.721041	16.737728
33.078377	1205.873859	16.742746
33.529855	1199.752657	16.747763
33.584605	1195.254444	16.752781
33.855946	1196.180281	16.757799
34.060707	1184.735799	16.762816
33.540390	1172.637734	16.767834
33.687508	1159.901528	16.772851
33.768039	1170.503128	16.777869
33.827848	1166.955830	16.782887
33.287994	1169.690306	16.787904
33.333706	1170.268296	16.792922
33.356460	1163.778171	16.797939
33.516903	1166.550398	16.802957
33.599425	1160.595027	16.807975
33.457888	1167.915208	16.812992
33.516307	1187.400381	16.818010
33.895092	1188.020420	16.823027
33.845608	1193.735548	16.828045
33.810254	1192.813163	16.833063
33.950285	1194.508730	16.838080
34.296567	1188.983205	16.843098
34.086605	1185.497018	16.848115
33.710615	1200.915078	16.853133
34.139782	1185.517829	16.858151
33.905368	1188.305844	16.863168
33.827483	1195.200593	16.868186
34.056345	1182.938199	16.873203
33.930799	1183.262709	16.878221
34.082706	1185.427518	16.883239
34.046124	1190.059093	16.888256
33.928692	1195.324932	16.893274
34.088735	1201.164739	16.898291
33.510971	1191.171954	16.903309
34.023457	1204.633763	16.908327
34.389399	1212.405516	16.913344
34.163963	1222.517172	16.918362
34.585243	1210.453736	16.923379
34.595754	1222.513779	16.928397
34.897190	1220.928893	16.933415
34.855620	1222.038351	16.938432
34.747367	1197.392121	16.943450
34.599253	1187.595091	16.948467
34.155037	1191.903916	16.953485
34.398032	1207.467874	16.958503
34.911248	1205.057166	16.963520
34.557234	1221.643689	16.968538
34.796026	1220.187563	16.973555
34.495547	1214.747091	16.978573
34.556122	1210.039510	16.983591
34.805896	1210.409557	16.988608
34.935573	1220.407156	16.993626
35.334418	1215.258644	16.998643
35.046461	1209.308070	17.003661
34.721689	1208.668593	17.008679
35.156835	1211.297911	17.013696
34.822103	1212.207938	17.018714
34.893550	1208.263142	17.023731
35.044649	1214.115393	17.028749
35.130416	1208.168924	17.033767
35.047859	1215.985468	17.038784
35.057107	1212.725445	17.043802
35.528452	1207.287723	17.048819
35.166826	1210.784255	17.053837
35.012636	1220.041373	17.058855
35.149632	1211.564291	17.063872
35.256205	1219.638547	17.068890
35.599851	1210.727370	17.073907
35.492371	1207.065952	17.078925
35.539878	1200.001620	17.083943
35.545556	1205.844026	17.088960
35.448845	1214.178798	17.093978
35.506567	1207.639817	17.098995
35.552546	1209.046781	17.104013
35.513264	1209.150672	17.109031
35.756361	1204.868604	17.114048
35.560586	1208.195533	17.119066
35.726726	1204.801159	17.124083
35.912326	1210.083955	17.129101
35.788796	1208.582580	17.134119
35.559297	1212.537044	17.139136
35.760865	1209.627034	17.144154
35.919020	1203.560479	17.149171
35.528834	1212.167794	17.154189
35.535326	1220.469592	17.159207
35.870273	1221.045500	17.164224
35.483831	1235.060499	17.169242
36.187683	1229.403208	17.174259
35.865896	1237.777824	17.179277
36.191276	1234.386361	17.184295
36.069159	1239.360369	17.189312
36.168534	1238.646951	17.194330
36.404001	1233.616515	17.199347
36.012706	1237.747806	17.204365
35.887320	1239.058617	17.209383
36.352272	1238.386784	17.214400
36.252745	1247.295414	17.219418
36.340470	1238.382564	17.224435
36.411603	1237.375550	17.229453
36.179560	1234.102881	17.234471
36.340283	1243.842278	17.239488
35.936140	1251.437201	17.244506
36.407446	1259.602751	17.249523
36.348674	1272.003447	17.254541
36.714597	1274.889219	17.259559
36.777270	1273.159931	17.264576
36.560520	1272.566933	17.269594
36.730911	1263.964939	17.274611
36.946283	1277.071493	17.279629
37.022079	1262.845844	17.284647
37.267084	1263.061704	17.289664
36.756363	1279.490808	17.294682
37.009368	1271.278345	17.299699
37.019818	1269.890881	17.304717
37.064034	1267.812952	17.309735
37.073586	1267.786354	17.314752
36.622478	1262.829229	17.319770
36.918172	1261.333349	17.324787
36.677435	1270.002596	17.329805
36.730587	1271.619216	17.334823
37.112210	1265.490251	17.339840
36.799284	1269.052965	17.344858
37.196130	1270.635219	17.349875
36.985108	1265.054613	17.354893
36.753549	1265.971783	17.359911
36.825679	1278.227332	17.364928
37.170157	1296.373160	17.369946
37.494711	1299.160925	17.374963
37.391944	1296.974294	17.379981
37.543890	1295.393580	17.384999
37.598248	1297.646326	17.390016
37.477252	1302.150608	17.395034
37.763005	1292.331502	17.400051
37.901739	1294.766641	17.405069
37.636033	1292.023953	17.410087
37.917506	1275.148650	17.415104
37.774482	1279.791724	17.420122
37.700824	1261.812921	17.425139
37.423206	1258.654485	17.430157
37.266300	1270.791608	17.435175
37.996529	1276.885800	17.440192
37.872541	1293.311443	17.445210
38.002932	1291.152910	17.450227
38.053360	1296.898549	17.455245
37.484127	1296.110859	17.460263
37.855503	1285.814824	17.465280
37.843985	1290.630418	17.470298
38.310546	1287.531046	17.475315
38.033638	1290.679802	17.480333
37.948262	1287.993301	17.485351
38.304311	1288.613040	17.490368
37.706297	1298.194261	17.495386
37.918695	1288.728217	17.500403
38.280728	1288.897884	17.505421
38.086886	1300.369998	17.510439
38.373372	1302.982143	17.515456
38.084839	1322.514967	17.520474
38.436039	1321.863633	17.525491
38.507358	1320.577359	17.530509
38.389117	1324.599842	17.535527
38.914826	1321.749803	17.540544
38.487846	1325.772760	17.545562
38.253473	1314.946438	17.550579
38.732903	1324.356621	17.555597
38.469036	1324.980059	17.560615
38.672229	1313.461004	17.565632
38.494098	1323.285961	17.570650
38.589206	1316.729956	17.575667
38.874762	1317.059691	17.580685
38.781099	1317.081017	17.585703
38.860711	1314.308420	17.590720
38.470668	1315.299636	17.595738
38.373672	1316.678288	17.600755
38.800312	1332.212304	17.605773
38.814689	1342.109607	17.610791
39.055632	1338.637989	17.615808
39.090673	1349.232030	17.620826
39.249660	1340.679004	17.625843
39.597506	1337.728335	17.630861
39.234810	1347.753425	17.635879
39.572138	1337.349522	17.640896
39.365358	1340.108774	17.645914
39.463265	1340.392143	17.650931
39.147857	1324.319087	17.655949
39.093911	1334.328747	17.660967
39.457213	1337.504400	17.665984
39.818485	1338.833562	17.671002
39.704066	1325.983974	17.676019
39.532889	1320.346652	17.681037
39.530212	1332.694406	17.686055
39.860438	1329.359568	17.691072
39.557788	1330.882710	17.696090
39.486517	1321.595601	17.701107
39.761808	1326.404005	17.706125
39.668915	1332.642872	17.711143
39.718250	1330.196799	17.716160
39.931113	1338.496426	17.721178
39.709368	1336.847100	17.726195
39.954125	1342.369846	17.731213
39.718502	1334.664734	17.736231
39.863716	1330.977927	17.741248
39.690004	1341.491994	17.746266
39.523073	1336.806499	17.751283
39.743495	1332.422612	17.756301
39.580494	1340.248121	17.761319
40.023075	1350.102305	17.766336
39.931956	1370.887357	17.771354
40.363856	1356.302000	17.776371
40.704083	1366.130047	17.781389
40.794548	1367.842978	17.786407
40.376637	1348.268004	17.791424
40.101586	1346.135585	17.796442
40.449027	1359.806343	17.801459
40.542218	1361.080731	17.806477
40.376601	1360.559015	17.811495
40.514624	1362.844048	17.816512
40.239456	1368.275899	17.821530
40.274056	1359.841804	17.826547
40.591207	1355.392931	17.831565
40.624160	1354.378628	17.836583
40.973483	1349.196280	17.841600
40.934886	1353.184044	17.846618
41.098681	1350.891181	17.851635
41.347713	1347.478048	17.856653
40.701933	1349.395707	17.861671
41.247150	1344.083800	17.866688
40.841469	1345.370108	17.871706
40.857312	1348.121385	17.876723
41.025879	1345.984284	17.881741
40.991784	1356.693182	17.886759
41.057095	1348.507465	17.891776
41.315954	1344.977929	17.896794
41.093401	1348.241517	17.901811
41.401431	1351.460598	17.906829
41.185982	1345.191649	17.911847
41.176070	1352.496435	17.916864
41.353367	1346.981285	17.921882
41.082321	1344.933175	17.926899
41.254133	1337.879627	17.931917
41.047397	1351.647414	17.936935
41.360618	1339.613692	17.941952
41.302682	1343.358348	17.946970
41.081609	1346.842720	17.951987
41.267482	1351.722024	17.957005
41.122425	1372.982106	17.962023
41.409964	1374.008410	17.967040
41.412923	1370.430801	17.972058
41.489564	1364.774388	17.977075
41.470665	1372.155340	17.982093
41.191157	1379.234924	17.987111
41.863780	1384.009079	17.992128
42.208689	1402.753537	17.997146
42.261138	1395.591577	18.002163
42.423171	1383.659800	18.007181
42.197425	1373.292977	18.012199
42.384388	1362.982254	18.017216
42.054015	1360.953042	18.022234
42.344091	1360.602478	18.027251
42.700534	1353.255195	18.032269
42.539488	1369.193668	18.037287
42.408312	1359.570793	18.042304
42.462886	1359.036769	18.047322
41.906005	1366.589254	18.052339
42.481099	1361.565172	18.057357
42.431518	1360.037043	18.062375
42.404618	1358.613054	18.067392
42.595172	1358.864343	18.072410
42.765922	1370.657482	18.077427
42.649895	1352.855218	18.082445
42.241928	1366.215432	18.087463
42.613727	1362.684398	18.092480
42.565947	1357.195702	18.097498
41.916306	1357.566835	18.102515
42.264643	1374.810760	18.107533
42.551613	1393.938060	18.112551
42.779010	1391.303908	18.117568
42.720790	1393.015386	18.122586
42.682616	1395.131888	18.127603
43.111676	1391.016745	18.132621
43.150693	1394.358968	18.137639
43.014317	1385.227713	18.142656
43.147589	1391.022315	18.147674
43.083375	1391.967074	18.152691
43.297857	1380.588533	18.157709
43.083296	1387.741923	18.162727
42.758554	1379.640421	18.167744
43.017113	1388.882157	18.172762
43.331666	1405.613956	18.177779
43.433268	1402.765472	18.182797
43.426831	1409.729156	18.187815
43.476144	1409.781164	18.192832
43.794100	1410.278777	18.197850
43.277425	1398.760415	18.202867
43.596322	1397.831858	18.207885
43.651957	1414.156627	18.212903
43.628103	1417.965084	18.217920
43.647504	1414.095390	18.222938
43.596999	1422.584156	18.227955
43.980539	1413.579186	18.232973
44.133566	1417.758214	18.237991
43.640363	1401.450719	18.243008
43.869917	1411.555224	18.248026
43.952345	1415.598426	18.253043
43.855133	1413.604382	18.258061
43.936538	1416.736920	18.263079
43.830064	1418.928029	18.268096
43.925247	1413.494380	18.273114
43.541434	1418.567604	18.278131
44.109545	1413.053810	18.283149
43.639141	1410.213965	18.288167
43.927002	1423.072338	18.293184
44.482163	1440.876418	18.298202
44.081973	1438.752931	18.303219
44.429010	1435.815744	18.308237
44.152381	1443.447847	18.313255
44.372678	1440.495477	18.318272
44.509389	1444.774648	18.323290
44.313287	1449.809293	18.328307
44.668503	1432.019083	18.333325
44.293487	1452.073200	18.338343
44.523109	1444.840484	18.343360
44.468121	1445.347238	18.348378
44.333321	1448.599999	18.353395
44.629425	1453.895150	18.358413
44.768371	1468.330759	18.363431
44.698674	1476.350683	18.368448
45.261901	1469.628710	18.373466
45.178409	1477.621733	18.378483
45.100325	1470.034577	18.383501
44.937463	1473.948593	18.388519
44.865346	1473.323866	18.393536
45.232365	1464.736015	18.398554
45.105369	1463.549002	18.403571
44.986266	1461.483720	18.408589
45.141418	1467.368463	18.413607
45.299986	1466.847738	18.418624
45.354298	1464.250617	18.423642
45.681156	1466.039122	18.428659
45.709432	1461.033788	18.433677
45.725875	1461.646347	18.438695
45.547328	1462.240452	18.443712
46.013438	1446.322631	18.448730
45.742547	1456.336299	18.453747
46.157765	1453.510937	18.458765
45.766845	1457.031075	18.463783
45.625571	1443.006620	18.468800
45.735430	1447.347493	18.473818
45.586651	1463.160623	18.478835
46.155951	1455.858783	18.483853
45.998411	1454.169314	18.488871
45.674163	1462.543663	18.493888
45.832792	1453.313404	18.498906
45.771073	1459.095084	18.503923
46.080185	1456.996903	18.508941
45.895973	1458.785902	18.513959
46.131792	1455.709138	18.518976
46.331352	1455.866179	18.523994
45.822030	1461.506877	18.529011
45.878092	1452.564338	18.534029
46.073752	1461.092521	18.539047
45.912733	1464.673527	18.544064
46.320324	1472.174497	18.549082
46.217922	1490.351726	18.554099
46.819582	1488.192726	18.559117
46.553157	1481.588122	18.564135
46.738909	1487.893520	18.569152
46.863988	1487.641632	18.574170
46.571671	1490.722098	18.579187
46.828754	1486.206470	18.584205
46.812307	1488.640435	18.589223
46.654308	1491.337663	18.594240
47.034465	1483.778096	18.599258
46.817500	1492.103890	18.604275
46.985257	1483.818383	18.609293
46.868300	1487.115500	18.614311
46.966206	1488.639272	18.619328
47.097962	1481.964871	18.624346
46.908828	1492.439818	18.629363
47.038109	1483.358947	18.634381
47.050595	1482.580719	18.639399
46.641051	1492.156390	18.644416
47.095886	1494.557667	18.649434
46.978712	1500.646313	18.654451
47.247556	1509.089703	18.659469
47.261660	1493.549104	18.664487
47.366142	1503.576087	18.669504
47.462570	1497.491726	18.674522
47.206393	1504.905082	18.679539
47.382062	1505.559892	18.684557
47.865128	1497.200494	18.689575
47.454448	1503.568772	18.694592
47.463667	1500.354310	18.699610
48.008757	1518.666635	18.704627
48.188461	1514.440994	18.709645
47.624761	1511.361163	18.714663
47.794205	1517.756482	18.719680
48.053850	1524.135845	18.724698
47.956587	1530.831698	18.729715
47.893641	1532.314271	18.734733
48.144912	1535.378055	18.739751
48.003605	1523.861079	18.744768
48.291571	1519.338942	18.749786
48.107885	1527.714508	18.754803
48.417918	1531.615257	18.759821
48.323194	1524.615926	18.764839
48.109085	1523.685847	18.769856
48.401798	1518.127843	18.774874
48.104223	1520.551590	18.779891
48.581184	1518.983515	18.784909
48.695503	1521.493378	18.789927
48.497444	1522.097675	18.794944
48.707419	1515.097734	18.799962
48.461938	1525.998567	18.804979
48.413069	1523.388002	18.809997
48.544065	1527.715303	18.815015
48.362858	1531.101332	18.820032
49.070342	1542.203359	18.825050
48.959495	1554.707774	18.830067
49.205627	1550.786939	18.835085
49.147244	1550.278789	18.840103
49.183718	1553.782699	18.845120
49.465369	1545.290219	18.850138
49.022879	1537.061107	18.855155
49.037677	1537.705394	18.860173
49.351140	1542.568348	18.865191
49.120575	1551.796169	18.870208
49.308103	1546.797656	18.875226
49.263993	1557.905512	18.880243
49.338118	1547.450624	18.885261
49.493146	1543.681969	18.890279
49.425770	1553.107934	18.895296
49.326591	1549.162729	18.900314
49.307798	1547.764172	18.905331
49.297205	1541.328750	18.910349
49.086193	1544.321537	18.915367
48.938333	1561.199629	18.920384
49.484211	1570.940744	18.925402
49.882047	1578.465349	18.930419
49.940289	1592.076265	18.935437
50.010398	1580.320233	18.940455
50.323606	1576.955805	18.945472
50.348991	1577.562223	18.950490
49.676988	1576.057042	18.955507
50.153968	1575.699477	18.960525
50.132478	1564.844521	18.965543
50.256187	1577.752022	18.970560
50.184305	1578.000336	18.975578
50.236056	1581.748011	18.980595
49.984733	1584.260353	18.985613
50.274080	1589.964071	18.990631
50.105390	1600.234474	18.995648
50.537525	1600.114524	19.000666
50.405618	1603.899360	19.005683
50.639298	1607.769046	19.010701
50.778863	1605.272355	19.015719
50.488673	1612.502414	19.020736
50.602058	1601.658170	19.025754
50.886779	1605.754897	19.030771
50.521293	1603.958566	19.035789
50.864899	1609.937588	19.040807
50.842619	1601.510853	19.045824
51.008979	1602.735838	19.050842
51.056480	1600.611716	19.055859
50.897956	1597.941543	19.060877
51.135087	1595.352996	19.065895
50.690837	1591.012900	19.070912
50.929118	1603.917883	19.075930
50.922434	1627.261109	19.080947
51.054640	1629.758699	19.085965
51.475334	1628.510280	19.090983
51.448398	1623.444478	19.096000
51.430195	1624.845201	19.101018
51.440222	1630.255260	19.106035
51.526076	1626.653356	19.111053
51.981761	1624.099166	19.116071
51.732475	1625.982725	19.121088
51.538508	1619.149410	19.126106
51.922150	1626.028962	19.131123
51.631966	1627.091578	19.136141
52.136950	1616.324090	19.141159
51.962921	1627.294620	19.146176
52.230728	1623.782469	19.151194
51.734300	1622.164331	19.156211
51.848769	1618.296727	19.161229
52.362090	1621.983383	19.166247
51.912294	1629.733654	19.171264
52.055904	1628.497177	19.176282
52.195767	1626.780706	19.181299
51.798274	1621.766924	19.186317
52.858517	1629.034892	19.191335
52.354952	1639.458624	19.196352
52.625580	1625.516175	19.201370
52.417186	1625.766597	19.206387
52.474913	1638.929297	19.211405
52.613065	1643.500113	19.216423
52.814700	1652.838405	19.221440
52.597216	1654.549357	19.226458
52.677765	1642.981959	19.231475
52.301844	1650.832152	19.236493
52.764262	1649.161770	19.241511
52.765110	1654.936696	19.246528
52.723763	1652.007135	19.251546
52.540864	1656.717253	19.256563
52.456446	1647.641258	19.261581
52.967432	1662.255269	19.266599
53.377334	1676.138177	19.271616
53.418823	1673.274845	19.276634
53.484550	1675.547861	19.281651
53.124690	1666.447352	19.286669
53.488285	1661.849399	19.291687
53.496936	1671.806833	19.296704
53.480840	1668.782786	19.301722
53.468423	1658.954356	19.306739
53.148055	1674.966552	19.311757
53.348099	1665.787760	19.316775
53.121014	1684.505822	19.321792
53.232544	1682.630258	19.326810
53.429475	1680.630955	19.331827
53.522432	1672.424916	19.336845
53.435674	1680.435875	19.341863
53.645138	1702.537369	19.346880
54.026979	1697.380390	19.351898
54.340279	1698.815560	19.356915
53.881799	1706.170826	19.361933
54.246329	1700.158461	19.366951
53.986103	1703.837937	19.371968
54.093578	1701.952005	19.376986
54.040078	1701.430486	19.382003
54.111976	1705.433760	19.387021
54.300438	1692.875340	19.392039
54.318279	1701.221224	19.397056
54.353706	1697.694989	19.402074
54.530501	1704.045171	19.407091
54.212771	1712.363563	19.412109
54.626507	1713.055140	19.417127
54.464521	1730.398182	19.422144
54.984539	1730.108475	19.427162
55.187546	1726.293580	19.432179
55.023705	1709.510821	19.437197
54.820869	1695.177379	19.442215
54.747657	1706.054806	19.447232
54.841545	1709.982210	19.452250
55.070670	1715.841098	19.457267
55.003069	1731.758770	19.462285
55.035975	1722.202301	19.467303
55.418681	1724.361061	19.472320
55.439550	1718.268994	19.477338
55.493059	1709.506828	19.482355
55.204839	1718.662933	19.487373
55.454239	1717.194056	19.492391
55.415160	1719.444466	19.497408
55.361023	1718.655614	19.502426
55.474273	1719.101724	19.507443
55.337100	1716.084392	19.512461
55.669298	1711.050952	19.517479
55.271146	1713.175357	19.522496
55.075196	1714.263065	19.527514
55.780847	1725.732855	19.532531
55.530841	1744.702419	19.537549
55.958620	1743.821764	19.542567
55.763928	1752.852067	19.547584
55.746419	1750.737505	19.552602
55.975570	1734.397019	19.557619
55.436195	1741.194940	19.562637
55.973795	1745.052376	19.567655
56.267365	1750.532099	19.572672
56.315500	1764.688308	19.577690
56.816828	1761.947478	19.582707
56.358965	1759.737964	19.587725
56.639537	1746.746352	19.592743
56.272280	1736.529261	19.597760
56.492405	1752.333424	19.602778
56.634089	1758.946438	19.607795
56.797651	1775.502170	19.612813
57.086564	1764.649475	19.617831
57.079335	1755.577621	19.622848
56.651973	1742.855443	19.627866
56.918539	1737.544577	19.632883
56.308370	1748.181243	19.637901
56.562683	1765.127574	19.642919
56.718702	1766.025435	19.647936
56.585336	1757.237198	19.652954
57.002235	1764.228712	19.657971
57.004791	1778.497605	19.662989
56.914713	1777.991355	19.668007
57.522010	1791.987623	19.673024
57.562346	1790.874577	19.678042
57.696425	1790.543379	19.683059
57.801416	1792.425518	19.688077
57.579637	1774.777253	19.693095
57.269562	1777.641156	19.698112
57.592568	1785.311521	19.703130
57.609373	1785.378155	19.708147
57.633075	1798.385965	19.713165
57.823094	1795.788379	19.718183
58.097458	1793.439272	19.723200
57.724390	1799.406818	19.728218
58.028482	1786.488504	19.733235
57.986706	1794.055016	19.738253
58.135018	1788.165982	19.743271
58.142724	1790.937518	19.748288
57.925372	1798.591814	19.753306
58.501352	1781.248142	19.758323
57.992032	1797.897054	19.763341
57.912102	1789.401533	19.768359
58.180172	1790.432548	19.773376
58.331351	1812.209998	19.778394
58.557716	1811.178975	19.783411
58.384706	1825.519175	19.788429
58.752133	1822.522815	19.793447
58.891832	1822.298481	19.798464
58.686855	1824.742905	19.803482
58.742379	1815.391997	19.808499
58.609389	1830.654764	19.813517
59.083101	1815.598205	19.818535
58.862720	1817.989237	19.823552
58.735937	1821.385531	19.828570
59.008675	1820.271601	19.833587
58.571579	1827.212924	19.838605
58.767192	1829.685492	19.843623
59.114310	1842.688170	19.848640
59.140606	1846.841912	19.853658
59.370888	1843.571668	19.858675
59.576731	1851.475489	19.863693
59.872712	1842.233305	19.868711
59.987454	1839.194650	19.873728
59.796848	1829.712298	19.878746
59.890626	1821.499752	19.883763
59.940370	1811.057216	19.888781
59.984842	1801.215684	19.893799
59.786671	1797.040001	19.898816
59.572143	1802.872931	19.903834
59.941293	1791.116232	19.908851
59.871422	1815.394847	19.913869
60.168312	1828.170338	19.918887
60.526197	1833.484094	19.923904
60.171505	1815.292215	19.928922
60.225460	1800.932661	19.933939
60.318641	1823.174016	19.938957
60.390007	1823.064408	19.943975
60.418141	1821.971397	19.948992
60.329616	1827.727608	19.954010
60.595801	1826.697313	19.959027
60.408350	1833.364426	19.964045
60.169522	1832.922012	19.969063
60.449274	1832.266323	19.974080
60.427691	1824.010821	19.979098
60.363398	1823.832391	19.984115
60.395598	1832.585080	19.989133
60.822827	1842.411376	19.994151
61.039350	1847.680036	19.999168
60.965530	1857.010476	20.004186
60.897756	1852.255512	20.009203
60.905216	1856.633290	20.014221
61.230999	1861.340219	20.019239
61.113248	1854.740049	20.024256
61.016687	1855.434360	20.029274
61.098341	1853.281158	20.034291
61.164988	1856.628520	20.039309
61.423608	1863.369236	20.044327
61.600567	1865.792084	20.049344
61.430078	1887.386546	20.054362
61.379397	1872.739203	20.059379
61.572493	1879.031015	20.064397
61.345474	1875.467149	20.069415
61.885131	1873.780494	20.074432
61.467845	1877.781600	20.079450
61.789850	1883.289875	20.084467
61.732569	1902.034623	20.089485
61.899244	1908.959139	20.094503
62.416607	1910.274477	20.099520
62.313291	1906.426584	20.104538
62.711621	1896.025143	20.109555
62.573434	1890.837766	20.114573
62.530578	1890.188689	20.119591
62.616197	1868.485242	20.124608
62.482842	1860.902763	20.129626
62.399233	1864.132506	20.134643
62.584480	1867.544334	20.139661
62.854547	1863.101246	20.144679
62.925938	1858.029906	20.149696
62.276790	1868.587137	20.154714
62.940090	1875.334900	20.159731
62.830109	1892.665908	20.164749
62.717681	1902.625505	20.169767
62.921472	1895.176445	20.174784
62.979004	1900.022917	20.179802
63.202805	1890.576692	20.184819
63.112858	1896.021671	20.189837
63.129204	1898.016284	20.194855
63.435401	1895.470158	20.199872
63.423196	1887.780248	20.204890
63.368898	1889.692522	20.209907
63.229755	1893.340149	20.214925
63.387056	1897.233107	20.219943
63.488547	1898.269459	20.224960
63.588355	1911.704930	20.229978
64.005625	1913.242316	20.234995
63.844172	1912.524055	20.240013
63.835106	1922.239073	20.245031
63.966335	1917.617532	20.250048
63.757550	1930.746701	20.255066
63.911723	1922.141402	20.260083
64.035129	1923.216736	20.265101
63.958577	1920.679734	20.270119
63.890556	1924.914613	20.275136
63.999932	1932.472823	20.280154
64.196123	1918.074738	20.285171
64.225841	1935.514877	20.290189
64.292646	1943.549471	20.295207
63.965326	1944.200355	20.300224
64.142716	1959.519946	20.305242
63.897574	1950.164987	20.310259
64.558864	1966.126348	20.315277
64.501794	1978.394441	20.320295
64.543416	1967.949155	20.325312
65.010371	1971.779378	20.330330
65.160360	1975.673523	20.335347
65.020287	1969.646347	20.340365
64.909764	1968.097196	20.345383
65.353594	1965.104354	20.350400
64.847579	1968.088425	20.355418
65.033267	1968.372753	20.360435
65.366730	1976.234266	20.365453
65.428314	1986.025370	20.370471
65.661584	1983.167575	20.375488
65.618381	1985.506780	20.380506
66.178228	1980.342555	20.385523
66.309011	1964.087507	20.390541
65.981160	1963.073281	20.395559
66.142332	1950.025806	20.400576
65.792393	1948.003560	20.405594
65.887824	1943.447500	20.410611
65.987113	1953.979822	20.415629
65.918307	1954.477785	20.420647
66.183936	1950.613516	20.425664
66.186249	1952.938378	20.430682
66.259033	1949.454107	20.435699
65.943170	1947.514524	20.440717
65.666854	1957.069248	20.445735
66.031300	1967.238367	20.450752
66.130598	1987.606145	20.455770
66.423103	1986.115424	20.460787
66.316549	1987.169229	20.465805
66.364835	1993.715442	20.470823
66.605027	1985.298540	20.475840
66.587046	2001.134654	20.480858
66.685578	2011.581400	20.485875
66.951269	2019.939068	20.490893
66.646016	2029.007624	20.495911
67.059296	2027.986894	20.500928
66.700557	2028.211743	20.505946
66.952271	2025.732493	20.510963
66.917993	2020.703906	20.515981
66.793372	2031.894182	20.520999
67.222515	2041.314430	20.526016
67.489471	2045.292983	20.531034
67.846617	2044.368516	20.536051
67.902239	2037.336309	20.541069
68.172810	2045.691640	20.546087
68.363620	2038.223341	20.551104
68.124436	2016.135705	20.556122
67.721768	2010.269951	20.561139
68.070304	2001.460560	20.566157
67.895106	1998.165276	20.571175
67.996513	1995.639209	20.576192
67.734120	2016.105611	20.581210
68.199593	2032.048720	20.586227
68.560849	2040.907160	20.591245
67.952439	2035.255909	20.596263
67.943872	2039.290986	20.601280
68.432051	2041.763341	20.606298
68.329476	2034.323741	20.611315
68.949810	2027.414644	20.616333
68.462823	2034.792709	20.621351
68.675412	2032.496679	20.626368
68.254648	2033.116060	20.631386
68.625298	2031.434317	20.636403
68.771051	2038.058610	20.641421
68.397438	2055.888075	20.646439
69.139222	2058.277513	20.651456
68.743714	2069.878355	20.656474
68.619882	2079.870568	20.661491
68.838556	2062.199693	20.666509
68.702625	2064.665395	20.671527
69.064334	2069.144846	20.676544
69.108413	2084.528304	20.681562
69.230962	2085.678513	20.686579
69.386911	2086.706195	20.691597
68.942137	2096.611949	20.696615
69.480675	2088.047511	20.701632
69.756128	2079.159272	20.706650
69.830839	2101.078350	20.711667
70.031562	2097.062356	20.716685
70.265880	2114.793369	20.721703
70.456723	2094.966915	20.726720
70.001731	2093.260306	20.731738
69.801485	2086.050208	20.736755
70.285493	2091.158311	20.741773
70.148908	2103.233103	20.746791
70.402725	2104.965694	20.751808
70.415154	2105.508128	20.756826
70.359498	2103.317006	20.761843
70.504174	2099.263542	20.766861
70.644520	2100.538342	20.771879
70.858389	2103.696312	20.776896
70.632491	2105.798019	20.781914
70.566261	2099.928129	20.786931
71.206442	2092.513993	20.791949
70.865713	2108.531482	20.796967
70.791506	2104.895992	20.801984
70.816625	2110.837918	20.807002
70.788503	2106.330616	20.812019
71.069389	2116.303933	20.817037
70.843076	2143.660015	20.822055
71.412272	2135.446201	20.827072
71.004422	2138.649054	20.832090
71.163531	2144.741888	20.837107
71.433807	2138.777415	20.842125
71.440142	2144.858430	20.847143
71.381375	2154.769525	20.852160
71.788126	2161.198864	20.857178
71.647656	2170.538560	20.862195
72.002020	2166.457930	20.867213
71.895135	2170.470180	20.872231
71.958811	2164.782488	20.877248
72.110808	2171.801502	20.882266
72.397190	2158.675665	20.887283
72.870909	2136.291665	20.892301
72.996849	2149.548566	20.897319
72.755134	2136.207275	20.902336
73.243955	2140.197669	20.907354
72.889790	2133.467530	20.912371
72.929446	2121.077994	20.917389
72.762547	2117.512345	20.922407
72.762640	2112.120346	20.927424
72.685525	2106.732009	20.932442
72.614288	2109.679021	20.937459
72.953343	2107.863869	20.942477
72.942560	2120.182120	20.947495
72.689992	2128.209540	20.952512
73.136642	2141.917134	20.957530
73.125086	2136.935225	20.962547
73.171686	2131.262855	20.967565
73.091266	2137.039920	20.972583
73.330201	2135.471203	20.977600
73.361325	2140.933148	20.982618
72.920780	2140.717967	20.987635
73.237745	2147.749204	20.992653
73.194479	2163.722461	20.997671
73.617037	2179.457837	21.002688
73.256115	2174.345995	21.007706
73.560951	2186.209658	21.012723
73.752127	2188.049001	21.017741
73.651297	2198.891082	21.022759
73.611047	2200.444829	21.027776
74.142842	2198.432957	21.032794
73.882932	2211.425010	21.037811
74.287650	2207.403200	21.042829
74.257131	2231.152358	21.047847
74.526023	2232.220246	21.052864
74.623534	2229.448555	21.057882
74.851496	2228.500630	21.062899
75.065481	2232.725236	21.067917
74.397794	2230.648218	21.072935
74.884466	2229.283828	21.077952
74.871241	2223.135633	21.082970
74.744835	2229.631938	21.087987
74.979797	2223.005242	21.093005
74.935692	2223.011584	21.098023
74.934519	2217.073851	21.103040
75.169940	2234.379285	21.108058
75.362352	2240.506179	21.113075
75.828868	2240.133756	21.118093
75.595945	2247.941795	21.123111
75.687492	2252.974889	21.128128
75.688857	2246.887286	21.133146
75.616297	2248.140990	21.138163
75.748102	2246.357300	21.143181
75.462609	2248.853963	21.148199
75.610643	2250.802452	21.153216
76.151756	2242.071544	21.158234
75.625450	2241.258064	21.163251
75.616497	2255.729054	21.168269
75.740641	2264.321819	21.173287
76.077201	2273.688550	21.178304
76.353290	2271.243916	21.183322
76.047259	2280.230157	21.188339
76.306968	2289.059321	21.193357
76.663408	2290.471156	21.198375
76.468303	2298.850555	21.203392
76.768495	2304.217736	21.208410
76.922065	2306.399756	21.213427
76.995878	2298.901214	21.218445
77.116003	2297.578756	21.223463
76.964952	2298.313240	21.228480
77.187945	2293.820109	21.233498
77.123581	2303.586675	21.238515
77.539405	2296.297104	21.243533
77.210137	2303.544745	21.248551
77.104002	2303.950346	21.253568
77.293830	2302.914893	21.258586
77.279888	2299.084893	21.263603
77.512426	2301.062389	21.268621
77.566058	2314.290854	21.273639
77.586594	2324.715652	21.278656
77.762283	2331.559486	21.283674
77.436781	2335.562595	21.288691
77.956647	2334.406859	21.293709
78.063348	2333.722899	21.298727
78.109878	2333.083932	21.303744
78.156019	2331.804733	21.308762
78.067720	2343.357584	21.313779
78.217166	2345.633874	21.318797
78.456047	2350.317853	21.323815
78.488730	2353.421393	21.328832
78.979456	2344.704753	21.333850
78.852402	2355.870493	21.338867
79.541077	2342.768436	21.343885
79.556557	2325.143808	21.348903
79.703764	2318.501173	21.353920
79.621238	2302.835107	21.358938
79.425121	2300.428015	21.363955
79.497080	2301.897017	21.368973
79.616880	2299.839138	21.373991
79.492738	2301.666639	21.379008
79.900596	2295.374962	21.384026
79.629188	2302.375035	21.389043
79.418805	2296.955965	21.394061
79.760455	2298.623445	21.399079
79.803963	2302.566124	21.404096
79.954136	2306.206258	21.409114
79.520525	2296.682906	21.414131
79.855486	2294.941540	21.419149
80.061842	2297.190655	21.424167
79.702749	2297.900894	21.429184
79.968311	2286.789600	21.434202
79.850174	2297.988485	21.439219
79.808702	2305.085613	21.444237
80.166649	2315.311863	21.449255
80.414170	2321.686435	21.454272
80.189316	2318.487095	21.459290
80.105247	2319.936145	21.464307
80.383314	2320.664339	21.469325
80.437682	2353.713528	21.474343
80.375345	2357.945266	21.479360
80.479645	2358.437661	21.484378
80.690037	2364.425657	21.489395
80.869579	2358.048440	21.494413
80.562733	2368.252527	21.499431
80.525762	2394.389537	21.504448
80.752477	2387.958374	21.509466
81.088999	2387.550831	21.514483
81.335365	2385.826729	21.519501
81.592951	2395.425597	21.524519
81.765076	2416.296801	21.529536
81.998505	2418.166406	21.534554
82.324047	2419.623298	21.539571
82.373643	2388.481609	21.544589
82.365796	2380.341591	21.549607
82.317146	2382.305732	21.554624
82.338912	2369.934569	21.559642
82.116128	2373.446198	21.564659
82.147955	2366.764519	21.569677
82.377244	2367.520946	21.574695
82.249091	2381.579225	21.579712
82.181728	2361.407365	21.584730
81.845377	2387.990128	21.589747
82.057391	2401.374334	21.594765
82.408077	2402.907449	21.599783
82.515585	2410.857149	21.604800
82.614355	2414.805204	21.609818
82.766336	2429.256209	21.614835
82.911115	2427.529424	21.619853
83.084090	2431.106957	21.624871
83.130219	2436.004196	21.629888
82.943036	2433.598804	21.634906
83.050300	2446.843221	21.639923
82.976421	2461.172167	21.644941
83.312615	2469.890132	21.649959
83.663671	2473.331511	21.654976
83.664665	2464.109235	21.659994
83.523147	2465.167077	21.665011
83.494286	2465.469900	21.670029
83.554305	2473.950303	21.675047
83.545884	2491.309088	21.680064
83.938028	2487.909844	21.685082
84.149935	2489.147309	21.690099
84.045244	2499.671651	21.695117
84.370983	2489.754123	21.700135
84.419772	2493.084815	21.705152
84.377775	2494.819005	21.710170
84.378380	2520.667068	21.715187
84.697886	2518.962752	21.720205
84.836500	2516.728789	21.725223
85.015599	2522.113790	21.730240
85.024056	2518.824496	21.735258
85.157519	2508.385416	21.740275
85.506612	2507.419732	21.745293
85.463415	2506.044639	21.750311
85.497309	2511.009929	21.755328
85.626647	2514.210575	21.760346
85.476218	2513.989237	21.765363
85.449373	2506.311561	21.770381
85.917616	2508.301054	21.775399
85.568239	2515.200389	21.780416
85.600763	2500.075046	21.785434
85.720927	2507.324269	21.790451
85.753092	2512.446372	21.795469
85.948394	2512.987189	21.800487
85.705564	2507.455223	21.805504
85.958018	2507.603846	21.810522
85.924687	2506.056485	21.815539
86.038341	2523.170083	21.820557
86.370567	2532.986043	21.825575
86.296102	2543.274332	21.830592
86.471127	2541.289421	21.835610
86.192346	2533.581898	21.840627
86.329342	2528.875079	21.845645
86.367398	2538.617603	21.850663
86.652727	2559.149234	21.855680
87.020639	2561.693566	21.860698
86.839887	2569.237804	21.865715
87.029795	2568.102421	21.870733
87.224422	2557.352279	21.875751
87.153525	2559.772294	21.880768
87.385077	2559.574994	21.885786
87.883938	2570.600179	21.890803
87.493668	2579.109974	21.895821
87.942106	2574.173340	21.900839
87.958520	2579.764441	21.905856
88.189977	2572.324787	21.910874
87.938092	2563.266274	21.915891
87.969600	2574.311714	21.920909
88.261761	2564.793585	21.925927
88.137328	2574.437760	21.930944
88.317546	2575.671634	21.935962
88.136738	2570.984016	21.940979
88.325253	2575.656436	21.945997
88.623445	2569.316056	21.951015
88.499610	2576.822904	21.956032
88.776892	2562.758152	21.961050
88.533101	2577.148132	21.966067
88.314092	2582.311887	21.971085
88.852821	2595.742498	21.976103
88.630239	2611.246124	21.981120
88.977535	2604.396037	21.986138
88.778228	2605.570084	21.991155
88.529909	2608.347992	21.996173
89.337756	2616.718663	22.001191
89.109962	2627.803134	22.006208
89.511340	2620.289161	22.011226
89.426866	2621.111371	22.016243
89.576668	2633.951146	22.021261
90.185950	2621.769263	22.026279
89.892708	2619.949477	22.031296
89.822069	2625.670897	22.036314
90.232007	2642.134837	22.041331
90.129875	2648.776126	22.046349
90.049737	2650.415730	22.051367
90.002135	2664.333215	22.056384
90.428024	2644.315932	22.061402
90.659003	2646.227649	22.066419
90.742808	2653.156297	22.071437
91.085406	2644.812363	22.076455
90.476542	2647.080622	22.081472
90.432971	2638.882442	22.086490
90.837137	2640.697318	22.091507
90.779249	2651.727180	22.096525
91.167161	2660.930224	22.101543
91.421878	2666.285128	22.106560
91.510145	2659.064133	22.111578
91.627667	2658.009509	22.116595
91.250266	2669.170572	22.121613
91.638459	2653.319725	22.126631
91.823470	2663.308708	22.131648
91.703816	2659.549748	22.136666
91.847886	2658.911732	22.141683
91.525089	2658.765075	22.146701
92.010468	2656.990242	22.151719
91.772421	2661.436516	22.156736
91.934420	2658.262724	22.161754
92.250960	2675.857811	22.166771
92.066431	2695.272830	22.171789
92.322665	2692.174465	22.176807
92.085817	2698.498226	22.181824
92.288712	2698.631156	22.186842
92.358770	2704.223190	22.191859
92.292038	2712.642136	22.196877
92.615756	2723.057416	22.201895
92.588165	2731.285274	22.206912
92.946791	2725.756426	22.211930
93.249415	2737.346362	22.216947
92.864881	2760.539267	22.221965
93.210895	2754.416944	22.226983
93.422119	2759.174690	22.232000
93.059642	2752.641456	22.237018
93.578702	2756.494263	22.242035
93.375760	2763.165053	22.247053
93.951783	2775.538952	22.252071
93.904940	2777.221244	22.257088
93.897394	2785.864422	22.262106
94.403303	2780.091811	22.267123
94.198493	2778.506476	22.272141
94.409257	2780.268830	22.277159
94.637067	2779.603295	22.282176
94.316518	2783.429528	22.287194
94.706902	2787.671005	22.292211
94.140261	2781.359893	22.297229
94.697103	2782.160865	22.302247
94.653426	2783.970873	22.307264
94.677545	2787.740571	22.312282
94.957557	2800.346553	22.317299
95.084307	2816.103833	22.322317
95.227629	2806.752450	22.327335
95.459093	2805.478268	22.332352
95.367655	2813.151556	22.337370
95.184083	2807.710713	22.342387
94.883017	2811.571604	22.347405
95.207627	2796.014715	22.352423
95.109154	2815.579002	22.357440
95.269415	2824.897116	22.362458
95.715253	2826.403306	22.367475
95.509696	2828.410620	22.372493
95.933160	2845.345397	22.377511
96.013670	2858.502418	22.382528
96.219171	2860.854021	22.387546
96.497188	2860.477823	22.392563
96.025088	2858.695181	22.397581
96.493132	2851.191701	22.402599
96.718195	2854.694169	22.407616
96.475856	2855.778341	22.412634
97.150159	2863.355504	22.417651
96.742891	2881.566558	22.422669
96.994141	2893.423614	22.427687
97.119848	2889.826845	22.432704
96.901532	2888.994885	22.437722
97.006221	2886.455557	22.442739
96.914737	2885.575053	22.447757
97.363618	2892.331535	22.452775
97.579348	2924.755295	22.457792
97.244749	2925.228023	22.462810
97.935651	2912.588438	22.467827
97.734151	2918.295442	22.472845
97.832877	2922.328599	22.477863
97.797027	2920.899590	22.482880
97.846202	2949.516697	22.487898
98.344360	2950.583481	22.492915
98.117444	2946.767608	22.497933
98.309445	2951.105272	22.502951
98.382347	2959.782922	22.507968
98.355399	2953.486361	22.512986
98.670805	2956.814761	22.518003
98.616630	2970.835061	22.523021
98.761069	2973.343520	22.528039
98.757460	2976.021903	22.533056
98.877997	2972.871962	22.538074
98.956609	2972.897280	22.543091
98.858336	2998.312784	22.548109
99.353741	2997.399257	22.553127
99.498037	3001.355944	22.558144
99.673283	3003.989292	22.563162
99.718156	2997.250967	22.568179
99.754869	3007.804256	22.573197
99.489875	3002.563544	22.578215
100.091307	3019.584993	22.583232
99.743093	3034.518333	22.588250
100.337372	3032.822849	22.593267
100.220880	3035.345396	22.598285
100.172425	3032.077649	22.603303
100.433307	3041.664619	22.608320
100.057191	3038.525425	22.613338
100.207928	3033.957063	22.618355
100.441522	3054.100386	22.623373
100.494628	3050.899824	22.628391
100.859326	3054.677424	22.633408
100.964729	3055.987775	22.638426
101.362322	3056.725270	22.643443
101.006830	3059.281213	22.648461
101.091639	3067.163306	22.653479
101.457143	3078.341513	22.658496
101.300215	3079.319257	22.663514
101.866602	3076.788869	22.668531
101.868841	3075.531553	22.673549
101.710012	3076.924946	22.678567
101.656667	3074.907944	22.683584
101.870956	3075.041423	22.688602
102.165790	3087.383337	22.693619
102.249844	3101.335308	22.698637
102.531538	3099.102041	22.703655
102.449871	3103.046804	22.708672
102.704306	3106.399908	22.713690
103.233916	3089.397994	22.718707
102.745989	3096.780665	22.723725
102.938948	3091.055479	22.728743
103.012896	3100.615660	22.733760
102.781342	3103.814987	22.738778
103.411781	3092.921014	22.743795
103.233603	3101.459432	22.748813
103.223397	3093.195891	22.753831
103.581922	3103.873353	22.758848
103.181604	3126.306305	22.763866
103.614766	3122.426819	22.768883
103.324835	3134.020312	22.773901
103.382297	3132.842289	22.778919
103.857160	3123.665963	22.783936
104.426218	3131.884647	22.788954
104.944319	3129.866977	22.793971
104.997482	3120.424361	22.798989
105.101369	3106.793436	22.804007
104.841109	3104.217082	22.809024
104.884686	3104.371490	22.814042
105.346401	3106.503709	22.819059
104.961215	3115.854709	22.824077
104.702609	3104.613991	22.829095
104.982024	3098.451802	22.834112
105.067079	3102.269289	22.839130
105.267354	3102.706287	22.844147
104.919658	3095.898361	22.849165
105.232109	3108.652833	22.854183
105.897829	3120.679975	22.859200
105.699464	3136.398980	22.864218
105.491041	3118.094040	22.869235
105.938987	3130.006454	22.874253
106.042030	3121.349608	22.879271
105.752378	3118.963586	22.884288
106.093226	3128.109142	22.889306
106.212135	3122.509029	22.894323
105.880056	3121.593719	22.899341
105.898653	3120.185114	22.904359
106.222670	3138.819512	22.909376
105.877640	3152.600814	22.914394
106.253034	3154.974146	22.919411
106.202158	3168.917805	22.924429
106.366795	3185.174469	22.929447
106.333436	3182.432122	22.934464
106.622593	3195.999845	22.939482
107.053921	3203.538056	22.944499
107.350731	3211.671188	22.949517
107.377756	3211.040801	22.954535
107.823447	3216.526719	22.959552
107.502555	3206.044746	22.964570
107.418265	3215.192070	22.969587
107.763309	3217.984817	22.974605
107.979454	3241.186531	22.979623
108.226062	3237.940125	22.984640
108.376596	3233.691900	22.989658
108.523138	3239.188557	22.994675
108.518311	3238.785870	22.999693
108.537326	3231.817926	23.004711
108.680244	3231.719713	23.009728
108.622012	3233.407020	23.014746
108.657902	3225.504994	23.019763
108.730398	3232.342895	23.024781
108.992243	3246.656833	23.029799
109.139046	3249.294761	23.034816
109.205198	3266.976900	23.039834
109.146410	3262.116991	23.044851
109.332513	3259.403353	23.049869
109.119753	3272.292064	23.054887
109.375327	3277.633685	23.059904
109.394267	3283.095641	23.064922
109.922156	3282.289410	23.069939
109.721450	3299.084318	23.074957
109.653404	3298.396715	23.079975
110.252266	3311.993826	23.084992
110.213217	3331.417953	23.090010
110.363794	3329.572141	23.095027
110.277150	3329.966794	23.100045
110.585791	3326.343896	23.105063
110.993955	3322.193802	23.110080
110.339662	3330.341000	23.115098
110.703595	3340.244490	23.120115
110.647673	3353.210528	23.125133
110.613912	3360.928396	23.130151
111.162720	3350.604993	23.135168
111.194816	3363.232115	23.140186
111.652423	3372.852440	23.145203
111.591325	3382.575937	23.150221
111.472948	3380.549596	23.155239
111.625752	3377.795620	23.160256
111.687637	3377.312279	23.165274
112.334355	3363.986312	23.170291
112.504198	3350.196752	23.175309
112.396491	3355.404386	23.180327
112.754851	3346.664216	23.185344
112.780212	3343.630852	23.190362
112.217040	3357.811353	23.195379
112.541799	3353.175023	23.200397
112.985574	3362.821934	23.205415
113.321115	3366.487055	23.210432
112.887937	3382.006195	23.215450
112.861705	3380.779352	23.220467
113.027523	3379.246555	23.225485
113.292333	3384.154867	23.230503
113.340416	3381.180805	23.235520
113.439574	3390.736368	23.240538
113.752297	3395.719643	23.245555
113.926859	3408.039316	23.250573
113.631870	3414.946128	23.255591
113.989808	3413.008242	23.260608
113.940238	3415.116625	23.265626
114.270951	3410.088358	23.270643
114.340453	3419.004394	23.275661
114.109597	3416.190443	23.280679
114.825209	3430.289818	23.285696
114.955018	3436.515306	23.290714
114.456915	3434.617161	23.295731
114.646675	3439.922924	23.300749
114.786703	3445.446658	23.305767
115.247055	3434.915463	23.310784
115.217477	3454.769333	23.315802
115.314476	3466.365107	23.320819
115.434991	3476.820410	23.325837
115.618574	3474.243228	23.330855
115.582383	3464.701359	23.335872
115.948155	3470.609184	23.340890
115.992515	3460.961648	23.345907
116.014776	3460.161303	23.350925
115.719102	3481.648274	23.355943
116.013466	3486.127897	23.360960
116.328880	3496.897482	23.365978
115.891432	3497.932570	23.370995
116.216065	3511.977156	23.376013
116.405230	3526.809570	23.381031
116.821981	3528.152918	23.386048
116.516291	3536.482999	23.391066
116.783118	3532.185465	23.396083
117.029438	3544.180717	23.401101
116.768527	3553.639615	23.406119
117.284069	3548.182989	23.411136
116.921105	3553.373182	23.416154
117.058153	3573.269083	23.421171
117.346037	3571.557894	23.426189
117.678455	3584.898814	23.431207
117.961818	3577.721780	23.436224
117.864993	3586.144451	23.441242
118.028604	3602.747091	23.446259
118.674693	3606.432768	23.451277
118.274805	3617.060834	23.456295
118.823980	3604.996293	23.461312
118.982498	3613.305890	23.466330
118.855203	3611.232165	23.471347
118.997617	3611.915982	23.476365
118.744234	3616.122691	23.481383
118.810884	3601.032464	23.486400
118.909874	3608.385519	23.491418
119.164780	3630.780839	23.496435
119.441739	3629.616550	23.501453
119.444840	3641.834745	23.506471
119.202383	3631.948843	23.511488
119.385582	3649.670207	23.516506
119.457460	3663.612068	23.521523
119.633706	3674.623457	23.526541
119.772061	3672.835407	23.531559
120.086803	3688.332367	23.536576
120.123352	3691.753392	23.541594
120.326726	3699.848203	23.546611
120.463464	3698.047821	23.551629
120.175892	3717.098294	23.556647
120.595061	3723.417006	23.561664
120.711347	3734.128837	23.566682
120.816527	3730.873410	23.571699
121.335188	3740.422883	23.576717
121.500818	3749.046094	23.581735
121.740167	3749.443843	23.586752
122.032981	3750.132792	23.591770
121.756245	3747.833499	23.596787
122.788169	3745.888796	23.601805
122.370877	3742.219496	23.606823
122.933295	3734.751659	23.611840
122.827844	3725.443295	23.616858
122.408023	3708.360781	23.621875
122.701034	3702.595019	23.626893
122.657928	3704.757480	23.631911
122.628663	3716.744896	23.636928
122.868534	3734.831784	23.641946
122.828892	3735.443156	23.646963
123.115125	3736.252729	23.651981
122.934820	3736.888890	23.656999
123.037840	3736.908745	23.662016
123.285664	3736.787509	23.667034
123.314585	3752.998003	23.672051
123.432075	3769.279354	23.677069
123.345352	3764.853259	23.682087
123.466378	3757.300818	23.687104
123.801294	3779.199012	23.692122
123.467665	3796.577370	23.697139
124.038990	3786.707924	23.702157
123.939435	3799.258865	23.707175
124.278782	3803.359313	23.712192
124.324464	3816.348105	23.717210
124.311292	3819.965105	23.722227
124.524665	3822.774247	23.727245
124.594463	3841.103936	23.732263
125.514678	3842.153844	23.737280
125.227805	3851.507723	23.742298
125.337004	3853.254152	23.747315
125.410134	3850.523806	23.752333
125.423952	3862.518632	23.757351
125.669136	3850.392229	23.762368
125.888914	3855.817653	23.767386
125.946478	3852.036420	23.772403
126.198813	3843.856463	23.777421
126.092554	3870.258889	23.782439
126.411189	3862.635550	23.787456
126.809823	3858.216210	23.792474
126.667324	3869.313186	23.797491
127.029536	3853.561958	23.802509
126.546758	3867.793846	23.807527
126.597054	3865.169408	23.812544
126.803610	3867.226001	23.817562
126.729967	3883.629998	23.822579
126.915258	3879.719042	23.827597
127.183172	3894.747744	23.832615
127.485448	3906.986897	23.837632
127.728834	3914.833935	23.842650
127.738680	3925.458249	23.847667
127.822084	3925.639357	23.852685
127.661687	3924.435435	23.857703
128.033971	3925.454717	23.862720
128.058867	3948.998789	23.867738
128.254841	3954.774189	23.872755
128.530033	3951.387761	23.877773
128.431168	3956.730294	23.882791
128.521151	3955.569048	23.887808
128.934220	3968.706293	23.892826
128.605518	3982.297744	23.897843
128.909777	3975.523906	23.902861
129.234718	3989.150383	23.907879
129.449851	4004.087703	23.912896
129.318614	4009.203343	23.917914
129.566113	4000.970576	23.922931
129.694340	4007.152505	23.927949
129.824188	4019.500275	23.932967
129.866609	4030.043162	23.937984
130.060997	4030.833569	23.943002
129.878104	4044.000614	23.948019
130.325835	4040.351433	23.953037
130.347506	4044.144658	23.958055
130.256005	4061.732528	23.963072
130.683454	4074.034465	23.968090
130.627179	4075.205483	23.973107
131.034247	4060.490041	23.978125
131.270247	4093.089373	23.983143
131.836495	4083.571408	23.988160
133.282825	4027.915087	23.993178
133.490933	4015.316939	23.998195
133.318276	4003.112285	24.003213
133.542520	3982.080616	24.008231
133.351002	3952.873123	24.013248
133.204240	3932.231879	24.018266
133.308493	3936.554724	24.023283
133.319225	3917.503458	24.028301
132.998927	3901.098706	24.033319
132.967366	3891.924777	24.038336
133.297322	3895.505178	24.043354
132.918279	3897.891157	24.048371
133.065712	3890.992106	24.053389
133.079657	3897.868762	24.058407
133.346463	3914.596118	24.063424
133.580088	3915.074242	24.068442
133.348496	3925.643439	24.073459
133.624988	3921.535418	24.078477
133.461891	3931.802623	24.083495
133.256190	3935.171863	24.088512
133.958686	3948.360491	24.093530
133.892365	3957.359087	24.098547
134.129269	3968.885749	24.103565
133.878311	3984.157764	24.108583
133.976824	3994.715282	24.113600
134.320353	3999.907835	24.118618
133.966889	4022.664301	24.123635
134.449032	4028.490864	24.128653
134.480839	4041.567031	24.133671
134.643736	4069.139193	24.138688
134.954215	4073.902787	24.143706
134.846489	4087.736804	24.148723
135.217893	4091.351552	24.153741
135.173075	4103.495955	24.158759
135.615252	4126.766875	24.163776
135.321054	4134.866529	24.168794
135.560079	4145.648775	24.173811
136.096654	4155.244442	24.178829
136.443746	4161.208237	24.183847
136.308933	4168.037149	24.188864
136.735940	4169.949284	24.193882
137.096603	4186.150629	24.198899
137.319224	4187.298427	24.203917
137.249730	4194.943759	24.208935
137.232134	4200.333212	24.213952
137.444216	4194.043633	24.218970
137.446170	4189.523813	24.223987
137.836155	4177.315839	24.229005
137.845229	4205.125192	24.234023
137.893869	4206.248810	24.239040
137.870671	4210.271870	24.244058
137.608028	4219.831380	24.249075
137.670600	4228.180226	24.254093
138.297591	4238.773234	24.259111
138.267879	4247.737848	24.264128
138.267459	4252.974320	24.269146
138.530591	4264.196510	24.274163
138.807640	4262.957424	24.279181
138.993915	4272.364358	24.284199
138.721812	4277.774752	24.289216
139.396474	4282.670728	24.294234
139.039648	4304.341721	24.299251
139.349529	4313.724253	24.304269
139.247003	4309.817380	24.309287
139.455664	4328.426058	24.314304
139.868703	4340.431569	24.319322
139.660764	4354.567390	24.324339
139.920193	4357.853120	24.329357
140.368222	4379.675172	24.334375
140.174621	4381.941186	24.339392
140.577051	4374.297931	24.344410
140.532272	4396.233988	24.349427
140.599687	4402.175605	24.354445
140.851944	4405.242996	24.359463
141.048461	4418.848655	24.364480
141.418799	4435.192701	24.369498
141.238377	4439.664931	24.374515
141.575904	4440.430179	24.379533
141.931130	4448.874096	24.384551
141.750810	4465.510522	24.389568
142.311835	4470.131237	24.394586
142.029977	4469.368316	24.399603
142.145302	4463.085397	24.404621
142.570245	4484.170199	24.409639
142.664790	4489.661458	24.414656
142.852845	4495.149609	24.419674
142.749374	4491.439518	24.424691
143.076584	4521.393685	24.429709
143.206408	4528.871307	24.434727
143.503221	4527.268731	24.439744
143.853378	4519.994054	24.444762
143.793733	4520.102786	24.449779
143.787795	4515.221447	24.454797
144.042032	4532.546271	24.459815
144.064112	4552.971625	24.464832
144.314507	4546.551487	24.469850
144.325032	4546.292646	24.474867
144.659563	4540.520728	24.479885
144.892089	4540.231210	24.484903
144.781794	4569.035029	24.489920
145.064010	4564.913332	24.494938
145.111437	4580.199748	24.499955
145.308621	4581.716674	24.504973
145.239751	4574.858087	24.509991
145.527699	4579.302096	24.515008
145.750824	4588.330451	24.520026
145.885047	4607.627933	24.525043
146.043472	4600.112368	24.530061
146.072011	4602.127433	24.535079
145.939598	4613.929050	24.540096
146.259502	4604.453968	24.545114
146.119440	4621.685208	24.550131
146.332730	4636.992440	24.555149
146.092363	4644.808434	24.560167
146.160076	4658.925769	24.565184
146.465449	4669.003927	24.570202
147.105991	4673.913346	24.575219
147.396790	4691.291532	24.580237
147.626708	4685.104324	24.585255
147.334661	4698.530881	24.590272
147.589341	4685.626567	24.595290
148.304072	4712.427492	24.600307
148.293611	4719.325730	24.605325
148.371254	4725.791383	24.610343
148.208333	4729.605564	24.615360
148.684645	4716.009752	24.620378
148.640811	4729.119830	24.625395
148.511016	4735.719264	24.630413
148.843870	4741.128563	24.635431
149.005611	4743.377310	24.640448
149.291429	4738.741255	24.645466
149.252037	4759.905997	24.650483
149.428761	4764.095587	24.655501
149.851480	4773.801864	24.660519
150.158174	4776.962144	24.665536
150.335684	4775.034762	24.670554
150.025913	4777.111660	24.675571
150.029825	4789.338545	24.680589
150.865987	4787.410779	24.685607
150.534261	4804.272344	24.690624
150.788539	4804.305849	24.695642
150.854123	4806.869684	24.700659
151.270694	4823.434157	24.705677
151.170049	4828.984987	24.710695
151.045727	4829.752303	24.715712
151.150067	4822.875425	24.720730
151.536063	4842.646023	24.725747
151.375769	4847.400752	24.730765
151.741377	4853.708830	24.735783
151.884623	4877.824781	24.740800
151.992615	4885.130623	24.745818
152.401915	4893.004444	24.750835
152.360443	4892.678361	24.755853
152.454401	4900.301930	24.760871
152.874737	4916.097263	24.765888
152.989496	4916.847706	24.770906
152.942511	4927.337043	24.775923
153.005204	4946.603103	24.780941
153.526038	4940.732093	24.785959
153.385685	4952.233136	24.790976
153.489759	4950.691931	24.795994
153.753430	4963.608427	24.801011
153.814977	4977.218814	24.806029
153.881622	4985.569013	24.811047
154.201776	4983.136587	24.816064
154.212600	4991.049605	24.821082
154.248953	5000.943516	24.826099
154.596514	5009.964877	24.831117
155.426630	5001.224835	24.836135
155.464499	4998.964081	24.841152
155.605821	4993.968629	24.846170
155.818716	4981.561649	24.851187
155.776838	4983.080544	24.856205
156.275752	4994.421475	24.861223
156.268484	5013.731034	24.866240
156.382682	5010.405442	24.871258
156.561463	5018.885689	24.876275
156.911557	5019.150958	24.881293
157.043278	5008.990470	24.886311
156.962517	5007.817029	24.891328
157.260282	5008.514697	24.896346
157.020927	5011.070541	24.901363
156.989861	5006.064807	24.906381
157.488079	4997.520087	24.911399
157.420777	5014.150124	24.916416
157.611745	5012.790957	24.921434
157.833193	5025.624552	24.926451
157.881276	5042.389639	24.931469
157.919096	5030.347261	24.936487
157.957138	5036.451167	24.941504
157.993554	5058.570375	24.946522
158.402021	5062.805710	24.951539
158.140725	5059.175712	24.956557
158.500774	5080.093912	24.961575
158.738431	5088.084895	24.966592
158.943690	5086.023236	24.971610
159.126371	5109.544790	24.976627
158.888111	5127.686024	24.981645
159.434954	5132.959859	24.986663
159.429684	5136.920519	24.991680
160.117606	5145.296846	24.996698
160.484272	5147.573563	25.001715
160.462484	5146.991788	25.006733
161.481577	5124.282650	25.011751
161.762474	5123.445700	25.016768
161.864627	5116.199262	25.021786
162.022155	5105.141631	25.026803
161.879305	5093.305025	25.031821
162.022361	5081.994812	25.036839
162.021777	5083.785642	25.041856
162.005769	5081.836364	25.046874
161.838506	5079.882879	25.051891
162.036434	5080.309305	25.056909
162.248485	5071.659900	25.061927
162.143204	5080.526136	25.066944
162.460840	5088.098406	25.071962
163.125533	5089.799688	25.076979
162.970331	5095.445071	25.081997
163.424923	5095.122500	25.087015
163.283558	5099.515533	25.092032
163.226765	5090.361403	25.097050
163.208984	5092.331995	25.102067
163.421570	5092.730908	25.107085
163.767949	5086.330639	25.112103
163.410307	5083.265933	25.117120
163.737666	5095.825436	25.122138
163.928251	5102.454201	25.127155
163.806733	5110.045361	25.132173
164.180438	5117.689742	25.137191
164.394578	5136.684078	25.142208
164.528549	5145.305291	25.147226
164.625496	5153.342348	25.152243
164.440947	5160.322835	25.157261
164.708502	5176.014567	25.162279
164.531065	5190.702558	25.167296
165.168195	5200.913076	25.172314
165.235607	5210.574803	25.177331
165.062854	5225.557901	25.182349
165.602462	5234.438637	25.187367
165.815828	5249.680408	25.192384
165.855565	5265.542307	25.197402
166.271372	5269.782042	25.202419
166.257665	5291.455629	25.207437
166.705110	5298.281918	25.212455
166.850486	5301.947171	25.217472
166.845357	5305.695428	25.222490
167.106235	5317.956523	25.227507
167.077730	5341.103001	25.232525
167.085243	5345.410215	25.237543
167.011776	5370.142941	25.242560
167.146631	5387.284821	25.247578
167.350394	5402.296184	25.252595
167.767630	5421.629859	25.257613
168.173121	5432.884534	25.262631
168.147757	5450.039442	25.267648
168.438334	5464.130669	25.272666
169.108773	5469.494284	25.277683
169.300654	5471.706868	25.282701
169.867558	5462.669430	25.287719
169.808730	5457.826109	25.292736
170.002771	5464.159447	25.297754
170.424440	5489.112403	25.302771
170.270235	5487.072596	25.307789
170.803591	5483.278817	25.312807
170.745713	5495.478373	25.317824
170.263347	5490.365044	25.322842
170.645564	5490.070529	25.327859
170.754992	5487.829762	25.332877
170.739634	5493.521449	25.337895
170.968691	5517.040192	25.342912
171.865365	5509.885610	25.347930
172.550592	5499.029937	25.352947
172.392161	5492.299285	25.357965
172.785589	5487.350805	25.362983
172.533522	5480.782999	25.368000
172.405913	5463.086946	25.373018
172.596101	5467.872538	25.378035
172.306794	5483.226952	25.383053
172.861723	5487.421753	25.388071
172.872796	5486.336699	25.393088
172.841662	5488.820874	25.398106
172.844133	5498.304318	25.403123
172.850000	5514.964951	25.408141
173.178274	5523.710401	25.413159
173.258392	5537.540214	25.418176
173.197266	5548.498803	25.423194
173.655047	5560.647669	25.428211
173.688488	5568.800505	25.433229
174.223586	5574.711304	25.438247
174.337828	5586.128975	25.443264
174.287285	5600.768028	25.448282
174.551043	5606.224858	25.453299
174.783144	5616.515979	25.458317
174.854379	5627.787903	25.463335
175.284233	5634.200948	25.468352
175.037810	5644.952330	25.473370
175.808609	5667.128454	25.478387
175.279677	5674.625141	25.483405
175.500889	5689.095070	25.488423
175.690674	5706.820222	25.493440
176.113067	5720.846620	25.498458
176.396591	5728.397908	25.503475
176.481597	5743.452156	25.508493
177.742658	5716.604398	25.513511
178.602948	5720.281660	25.518528
178.445374	5725.796267	25.523546
178.695513	5708.768257	25.528563
178.473666	5699.526768	25.533581
178.647920	5697.659585	25.538599
178.921351	5702.026788	25.543616
178.653894	5696.578570	25.548634
179.081952	5684.783435	25.553651
179.059932	5696.869651	25.558669
179.018910	5694.616648	25.563687
179.053114	5688.060544	25.568704
178.916318	5687.970725	25.573722
179.281837	5680.973132	25.578739
179.218196	5705.597850	25.583757
179.195480	5721.202689	25.588775
179.143079	5727.565203	25.593792
179.313419	5745.184140	25.598810
179.811828	5757.425828	25.603827
180.035767	5781.330546	25.608845
180.058050	5781.745659	25.613863
180.317196	5795.439381	25.618880
180.170639	5822.460691	25.623898
180.646770	5825.329040	25.628915
180.472045	5838.342164	25.633933
180.860566	5847.024700	25.638951
181.482334	5860.914802	25.643968
181.179252	5883.556724	25.648986
181.491772	5882.928701	25.654003
181.651084	5892.616348	25.659021
182.111235	5901.219833	25.664039
182.421609	5913.707998	25.669056
182.362543	5919.074789	25.674074
182.658500	5931.224585	25.679092
182.928777	5946.546124	25.684109
182.843101	5951.562325	25.689127
182.788658	5962.248708	25.694144
183.116325	5974.416302	25.699162
183.475239	5978.675544	25.704180
183.833784	6005.678028	25.709197
184.113713	6008.845207	25.714215
184.467585	6009.656723	25.719232
184.292693	6020.450473	25.724250
184.894214	6021.909384	25.729268
185.348000	6031.547814	25.734285
185.088661	6029.799286	25.739303
185.523206	6029.156525	25.744320
185.485797	6032.516712	25.749338
185.656018	6026.915192	25.754356
185.450286	6037.603720	25.759373
185.829449	6055.557955	25.764391
185.880504	6060.444602	25.769408
185.787163	6069.678535	25.774426
186.826437	6083.230052	25.779444
186.631967	6094.106443	25.784461
186.340994	6092.222113	25.789479
186.753669	6113.629077	25.794496
186.947523	6126.447573	25.799514
187.426550	6124.966064	25.804532
187.289190	6147.900622	25.809549
187.560240	6152.206969	25.814567
187.951635	6151.637174	25.819584
188.158885	6174.971607	25.824602
188.352936	6182.564933	25.829620
187.997639	6185.705960	25.834637
188.580802	6206.377750	25.839655
189.160770	6208.479793	25.844672
189.294690	6214.752227	25.849690
189.609486	6202.078566	25.854708
189.545361	6213.873714	25.859725
189.746403	6228.131801	25.864743
190.010959	6220.102022	25.869760
190.290088	6230.661458	25.874778
190.366310	6233.158540	25.879796
190.750114	6230.545820	25.884813
190.771564	6233.458416	25.889831
191.025342	6240.529248	25.894848
190.955554	6253.508695	25.899866
191.190521	6254.573653	25.904884
191.154211	6266.126791	25.909901
190.877717	6266.938109	25.914919
191.592341	6273.310757	25.919936
191.324755	6296.363083	25.924954
191.634987	6301.704183	25.929972
191.558623	6322.183079	25.934989
191.786303	6323.198062	25.940007
192.336586	6343.185249	25.945024
192.511306	6364.055349	25.950042
192.802969	6351.935235	25.955060
192.829518	6374.236588	25.960077
192.657470	6378.239117	25.965095
193.234341	6389.990438	25.970112
193.553151	6414.385404	25.975130
193.632472	6420.816913	25.980148
193.890714	6440.851578	25.985165
194.030389	6456.897885	25.990183
194.422348	6457.967730	25.995200
194.528557	6472.959540	26.000218
195.119688	6466.814724	26.005236
195.234357	6482.544022	26.010253
195.153852	6485.877349	26.015271
195.636108	6484.478696	26.020288
195.722490	6498.699458	26.025306
195.675972	6493.672866	26.030324
196.021104	6502.845032	26.035341
196.271486	6521.238168	26.040359
196.326661	6518.656547	26.045376
196.373627	6530.975572	26.050394
196.918980	6551.066114	26.055412
196.986169	6561.093846	26.060429
197.175083	6566.630633	26.065447
197.914258	6567.900850	26.070464
198.299497	6569.310899	26.075482
198.552212	6563.223930	26.080500
198.631991	6568.965381	26.085517
198.730204	6568.962408	26.090535
199.266794	6559.207627	26.095552
199.071619	6562.497879	26.100570
199.465576	6556.866000	26.105588
199.496879	6559.641755	26.110605
199.319055	6553.896457	26.115623
199.851030	6546.207056	26.120640
199.955237	6556.843396	26.125658
200.110048	6570.920345	26.130676
199.964653	6578.896884	26.135693
199.934528	6586.006062	26.140711
200.122188	6586.053349	26.145728
200.285244	6603.660305	26.150746
200.085261	6614.233451	26.155764
200.700267	6629.879207	26.160781
200.508466	6647.772542	26.165799
200.985100	6669.710669	26.170816
200.905106	6687.055114	26.175834
200.770345	6696.172505	26.180852
201.204099	6717.758742	26.185869
201.379497	6738.854296	26.190887
201.757183	6749.256760	26.195904
201.862027	6767.558526	26.200922
202.056879	6777.666767	26.205940
202.220565	6795.555538	26.210957
202.344355	6815.964650	26.215975
202.937059	6838.302728	26.220992
203.014955	6853.064170	26.226010
203.398026	6865.176454	26.231028
203.645846	6880.079218	26.236045
204.235823	6883.138932	26.241063
204.455285	6892.941180	26.246080
204.364189	6909.847807	26.251098
204.506378	6915.941393	26.256116
204.954640	6921.727314	26.261133
204.499407	6945.568291	26.266151
205.324046	6956.689643	26.271168
205.389434	6962.056640	26.276186
205.380417	6977.856539	26.281204
206.179631	6973.275652	26.286221
206.164281	6982.648004	26.291239
206.489651	6999.617383	26.296256
206.975325	7006.659483	26.301274
207.081182	6998.781271	26.306292
207.469205	7003.408354	26.311309
207.192749	7022.599775	26.316327
207.584291	7024.359801	26.321344
207.505056	7035.618227	26.326362
207.489414	7030.641611	26.331380
207.921765	7049.457260	26.336397
207.526965	7060.603134	26.341415
208.198425	7072.118029	26.346432
208.185607	7089.978638	26.351450
208.716750	7108.255353	26.356468
209.418990	7110.120082	26.361485
209.355975	7125.150544	26.366503
209.598981	7121.481338	26.371520
209.873800	7138.634404	26.376538
209.824366	7145.414873	26.381556
210.067903	7150.801536	26.386573
209.975167	7161.559407	26.391591
210.431197	7180.255778	26.396608
210.641510	7185.447889	26.401626
210.925822	7201.781179	26.406644
211.178985	7217.238167	26.411661
211.530527	7217.993475	26.416679
212.142712	7213.342403	26.421696
212.432552	7212.677819	26.426714
212.833874	7216.900763	26.431732
213.010992	7216.925343	26.436749
212.885148	7207.583411	26.441767
213.091126	7202.092995	26.446784
213.139902	7216.610791	26.451802
213.340323	7220.772914	26.456820
213.616003	7208.900156	26.461837
213.719146	7217.467691	26.466855
213.429486	7209.188958	26.471872
213.590304	7223.434744	26.476890
213.750901	7233.083720	26.481908
214.142360	7234.384258	26.486925
213.995274	7263.388801	26.491943
214.341478	7271.009576	26.496960
214.414130	7283.251951	26.501978
214.372986	7302.120585	26.506996
214.803155	7313.183917	26.512013
214.983882	7336.094773	26.517031
215.198568	7348.230363	26.522048
215.351013	7357.292142	26.527066
215.783360	7369.374165	26.532084
216.092651	7400.265528	26.537101
216.399693	7415.459187	26.542119
217.004699	7425.419076	26.547136
217.083013	7425.384654	26.552154
217.020513	7436.548650	26.557172
217.232756	7444.995843	26.562189
217.121441	7466.023252	26.567207
217.593745	7474.277136	26.572224
218.297925	7490.529647	26.577242
218.175428	7495.832364	26.582260
218.530345	7506.293286	26.587277
218.234983	7528.209392	26.592295
218.427282	7535.444088	26.597312
218.568046	7556.047440	26.602330
218.744338	7574.592184	26.607348
219.013408	7596.789032	26.612365
218.978992	7617.789444	26.617383
219.575505	7638.786880	26.622400
220.076653	7655.123085	26.627418
220.299730	7675.513611	26.632436
220.312136	7679.810492	26.637453
220.361495	7707.010148	26.642471
220.973588	7716.738152	26.647488
221.386799	7728.874274	26.652506
221.221371	7740.665532	26.657524
221.807785	7765.269500	26.662541
222.133407	7775.138031	26.667559
221.639609	7774.732513	26.672576
222.583809	7782.992393	26.677594
223.168946	7784.884933	26.682612
223.305953	7792.697098	26.687629
223.681096	7802.119847	26.692647
224.260285	7807.484719	26.697664
224.386879	7814.433365	26.702682
224.105132	7813.852794	26.707700
224.657535	7808.031127	26.712717
224.756810	7810.761655	26.717735
224.988065	7812.610677	26.722752
224.950055	7811.319243	26.727770
224.882211	7809.617873	26.732788
225.304492	7823.440121	26.737805
225.173346	7840.604417	26.742823
225.219035	7847.481779	26.747840
225.568720	7856.653273	26.752858
225.566369	7877.146111	26.757876
225.795569	7884.576540	26.762893
225.757650	7903.486338	26.767911
226.331383	7914.049980	26.772928
226.605795	7930.643359	26.777946
226.474402	7943.865443	26.782964
226.825413	7965.210155	26.787981
226.886277	7977.448289	26.792999
227.123191	7997.233889	26.798016
227.665169	8009.690837	26.803034
228.330546	8023.797936	26.808052
228.679929	8021.112893	26.813069
229.252186	8012.973695	26.818087
229.522010	8030.980805	26.823104
229.557690	8030.218209	26.828122
229.511381	8046.428865	26.833140
229.908715	8033.350984	26.838157
229.838083	8048.815599	26.843175
229.917462	8066.288111	26.848192
230.361442	8065.133073	26.853210
230.341905	8087.625323	26.858228
231.011700	8087.662650	26.863245
230.982154	8106.829475	26.868263
230.886292	8115.522499	26.873280
231.200124	8133.426320	26.878298
231.381185	8143.540837	26.883316
231.615425	8162.458725	26.888333
231.910432	8183.615556	26.893351
232.062482	8195.154718	26.898368
232.407780	8202.372431	26.903386
232.659929	8228.676678	26.908404
232.855467	8234.734759	26.913421
233.091807	8249.858701	26.918439
233.731249	8271.866886	26.923456
233.851780	8275.687928	26.928474
234.220429	8277.736625	26.933492
234.575046	8277.622746	26.938509
234.687064	8292.496243	26.943527
234.796791	8298.510977	26.948544
234.950213	8301.812925	26.953562
235.049130	8334.685811	26.958580
234.988381	8333.323199	26.963597
235.545827	8348.899291	26.968615
235.652252	8369.781515	26.973632
235.880171	8371.166855	26.978650
236.176087	8394.044841	26.983668
236.352531	8398.218987	26.988685
236.692594	8418.316850	26.993703
236.471172	8424.306517	26.998720
237.076783	8427.324333	27.003738
237.063117	8458.798577	27.008756
237.187960	8464.105094	27.013773
237.219316	8483.458244	27.018791
237.595803	8496.453880	27.023808
237.712115	8508.522682	27.028826
238.043177	8527.468880	27.033844
238.494352	8544.426263	27.038861
238.684744	8554.596623	27.043879
238.861823	8585.554008	27.048896
239.742262	8588.897122	27.053914
239.810121	8597.944022	27.058932
240.100515	8613.174215	27.063949
240.268930	8612.877938	27.068967
240.555146	8632.591992	27.073984
240.771474	8648.469872	27.079002
240.540675	8658.176654	27.084020
240.882254	8672.295067	27.089037
241.117235	8690.116905	27.094055
241.273196	8706.843742	27.099072
241.471988	8712.307358	27.104090
241.714667	8744.357906	27.109108
241.936925	8743.240132	27.114125
242.431888	8780.175624	27.119143
242.803664	8783.686825	27.124160
242.866183	8791.581425	27.129178
243.190108	8804.717915	27.134196
243.403950	8830.533943	27.139213
244.261208	8827.126047	27.144231
244.465689	8833.838473	27.149248
245.212888	8841.847059	27.154266
245.145687	8857.034166	27.159284
245.628475	8862.501752	27.164301
245.620389	8863.328646	27.169319
245.825204	8863.990969	27.174336
246.029050	8857.490636	27.179354
245.859619	8875.919369	27.184372
245.900710	8888.541103	27.189389
245.935912	8896.523137	27.194407
246.055845	8910.516568	27.199424
246.597431	8935.400328	27.204442
246.680491	8955.327010	27.209460
247.148874	8963.518610	27.214477
247.050757	8976.227532	27.219495
247.558145	8993.752517	27.224512
247.842781	9012.802345	27.229530
247.572604	9033.452777	27.234548
248.358647	9056.610927	27.239565
248.478696	9067.348836	27.244583
248.711947	9095.211863	27.249600
248.715774	9092.784360	27.254618
249.345871	9122.285983	27.259636
250.283679	9108.475710	27.264653
251.600101	9101.137665	27.269671
251.415915	9097.525062	27.274688
251.886917	9083.278877	27.279706
251.986514	9088.019094	27.284724
252.270307	9076.303326	27.289741
252.426450	9075.512426	27.294759
252.287322	9068.977746	27.299776
252.102060	9055.280043	27.304794
252.411941	9061.370993	27.309812
252.309407	9070.904137	27.314829
252.540815	9072.593936	27.319847
252.446595	9084.942688	27.324864
252.531788	9097.328563	27.329882
252.630007	9117.721680	27.334900
253.092219	9132.212420	27.339917
253.165335	9152.416386	27.344935
253.244871	9175.840405	27.349952
253.898627	9197.888994	27.354970
253.900055	9224.372674	27.359988
253.814503	9243.314968	27.365005
254.525537	9259.344042	27.370023
254.518728	9284.746271	27.375040
254.951191	9293.766558	27.380058
255.228488	9324.578070	27.385076
255.184728	9345.546976	27.390093
255.557166	9365.989582	27.395111
255.565060	9393.773794	27.400128
256.300681	9406.473736	27.405146
256.240165	9432.486420	27.410164
256.565070	9450.970845	27.415181
257.027218	9474.827385	27.420199
257.274243	9497.258007	27.425216
257.507068	9517.161168	27.430234
257.310272	9546.821797	27.435252
257.602493	9572.906775	27.440269
258.558437	9584.727708	27.445287
258.654825	9614.066291	27.450304
258.967444	9624.048300	27.455322
259.509973	9642.038277	27.460340
260.187171	9647.111970	27.465357
260.615968	9653.085834	27.470375
261.023847	9663.011762	27.475392
261.330287	9663.250656	27.480410
261.591149	9669.045497	27.485428
261.888202	9660.697454	27.490445
262.200630	9649.400473	27.495463
262.150474	9656.013774	27.500480
262.509028	9667.927242	27.505498
262.616247	9681.479163	27.510516
263.140699	9688.654484	27.515533
263.233544	9692.540508	27.520551
263.088280	9702.683305	27.525568
263.540016	9711.524094	27.530586
263.396780	9720.442018	27.535604
263.578669	9734.919788	27.540621
263.707591	9748.265658	27.545639
263.785031	9765.011699	27.550656
264.122290	9774.672722	27.555674
264.162618	9788.460089	27.560692
264.545771	9819.835760	27.565709
264.884024	9827.375303	27.570727
265.229359	9855.015680	27.575744
265.444827	9864.244435	27.580762
265.913745	9895.156035	27.585780
265.652144	9899.060440	27.590797
265.784036	9914.076005	27.595815
266.145056	9947.548114	27.600832
266.441651	9962.106588	27.605850
267.614849	9971.631739	27.610868
268.931275	9936.803175	27.615885
269.959076	9923.111616	27.620903
270.033343	9927.406757	27.625920
270.121358	9902.856787	27.630938
270.228886	9893.136780	27.635956
270.324418	9887.409187	27.640973
270.681863	9888.707527	27.645991
270.001303	9886.755726	27.651008
270.818725	9883.540085	27.656026
270.767053	9878.879524	27.661044
270.474961	9882.107634	27.666061
270.599380	9904.753192	27.671079
270.444870	9914.711872	27.676096
270.888382	9930.502958	27.681114
271.340115	9948.638028	27.686132
271.233800	9958.944781	27.691149
271.521217	9982.493930	27.696167
271.481925	10007.785686	27.701184
271.705558	10021.924568	27.706202
271.868029	10055.359310	27.711220
272.324703	10077.727870	27.716237
273.281108	10093.327981	27.721255
273.353051	10114.095353	27.726272
273.919452	10131.769080	27.731290
274.019008	10144.613145	27.736308
273.912916	10166.911775	27.741325
274.350090	10174.443203	27.746343
274.433327	10201.531009	27.751360
274.675265	10224.322015	27.756378
275.104196	10252.362198	27.761396
275.199636	10265.895273	27.766413
275.330879	10286.840741	27.771431
275.598472	10325.641387	27.776448
276.282707	10342.993774	27.781466
276.392636	10362.938500	27.786484
276.487002	10396.598924	27.791501
276.900083	10410.432908	27.796519
277.173139	10434.178660	27.801536
277.267102	10448.719534	27.806554
277.734521	10474.569588	27.811572
277.717954	10498.109754	27.816589
278.621627	10511.038068	27.821607
278.394069	10535.469003	27.826624
278.855285	10557.774196	27.831642
279.113284	10564.876324	27.836660
279.440750	10590.668607	27.841677
280.153364	10595.884163	27.846695
280.203584	10627.374399	27.851712
280.171977	10637.321047	27.856730
280.376168	10656.275204	27.861748
280.784189	10666.696432	27.866765
281.677590	10676.722338	27.871783
281.659161	10699.384380	27.876800
282.017952	10722.737959	27.881818
282.146403	10733.125877	27.886836
282.255361	10757.017924	27.891853
282.794702	10763.336265	27.896871
282.943500	10787.295206	27.901888
283.406630	10791.927253	27.906906
284.057861	10806.933340	27.911924
284.352023	10825.239793	27.916941
284.763914	10816.248682	27.921959
284.525287	10835.853701	27.926976
284.897487	10854.319329	27.931994
284.914850	10868.998352	27.937012
285.219181	10891.632455	27.942029
285.458248	10907.089599	27.947047
286.075326	10923.908326	27.952064
286.219046	10935.835400	27.957082
286.595210	10953.853076	27.962100
286.689419	10971.114487	27.967117
287.079111	10982.819796	27.972135
286.842019	11009.957942	27.977152
287.221002	11031.107174	27.982170
287.854688	11049.908367	27.987188
287.843979	11079.989000	27.992205
288.312317	11095.255922	27.997223
288.755724	11115.000324	28.002240
288.764287	11130.679986	28.007258
289.113828	11160.679946	28.012276
289.337783	11175.610666	28.017293
290.114497	11191.089646	28.022311
290.534271	11204.099034	28.027328
290.927683	11223.135901	28.032346
291.386942	11226.891707	28.037364
291.060036	11240.865059	28.042381
291.371205	11254.394937	28.047399
291.931150	11272.103109	28.052416
292.257646	11277.831247	28.057434
293.410499	11259.330206	28.062452
293.633639	11265.641309	28.067469
294.497787	11272.636930	28.072487
294.307010	11264.117835	28.077504
294.287259	11271.513282	28.082522
295.052634	11275.847020	28.087540
294.974236	11284.530817	28.092557
295.502592	11284.137381	28.097575
294.915356	11292.298597	28.102592
295.307954	11282.987980	28.107610
295.514022	11282.484167	28.112628
295.451908	11301.029797	28.117645
296.069945	11307.218161	28.122663
296.001723	11328.850926	28.127680
296.055458	11347.011763	28.132698
296.746335	11347.678197	28.137716
297.184572	11368.516221	28.142733
297.202451	11382.417434	28.147751
297.637996	11389.450727	28.152768
297.621929	11394.963541	28.157786
297.666914	11422.682605	28.162804
297.956499	11441.805364	28.167821
298.693803	11456.634080	28.172839
298.611973	11476.681085	28.177856
298.596277	11508.768268	28.182874
298.992785	11521.301910	28.187892
299.200802	11552.391117	28.192909
299.523918	11575.600975	28.197927
299.482772	11611.713480	28.202944
299.707381	11637.398600	28.207962
300.281489	11662.071345	28.212980
300.545099	11700.207516	28.217997
301.274692	11722.425023	28.223015
301.566465	11753.045759	28.228032
301.775246	11773.732795	28.233050
302.441781	11787.891488	28.238068
302.701600	11820.061549	28.243085
303.046721	11833.381102	28.248103
303.252071	11863.587257	28.253120
303.629306	11880.674526	28.258138
304.240070	11888.072106	28.263156
304.309432	11928.200098	28.268173
304.999432	11929.029438	28.273191
305.557488	11945.988590	28.278208
305.242492	11959.132267	28.283226
305.871300	11971.273879	28.288244
306.118460	11985.628488	28.293261
306.068174	12006.599562	28.298279
306.020825	12026.205538	28.303296
306.476984	12051.390254	28.308314
307.269127	12065.848955	28.313332
307.644030	12084.636013	28.318349
308.093893	12099.016276	28.323367
309.014104	12101.392028	28.328384
309.009330	12105.829474	28.333402
309.096468	12112.245256	28.338420
309.022503	12138.871993	28.343437
309.184876	12140.461773	28.348455
310.275013	12154.912620	28.353472
310.668276	12170.567071	28.358490
311.028907	12171.519960	28.363508
310.940887	12195.386635	28.368525
311.076240	12187.960894	28.373543
311.510012	12195.900827	28.378560
311.257481	12226.633866	28.383578
311.513073	12241.797128	28.388596
311.808939	12257.001607	28.393613
312.062093	12274.012083	28.398631
312.119671	12298.079454	28.403648
312.225690	12328.318107	28.408666
312.879795	12334.869331	28.413684
312.438487	12373.457218	28.418701
313.044410	12399.354612	28.423719
313.128522	12426.395485	28.428736
313.652662	12460.256077	28.433754
314.065012	12483.396035	28.438772
314.366643	12506.528290	28.443789
314.655641	12533.999340	28.448807
315.130933	12565.398300	28.453824
315.400149	12596.322658	28.458842
315.982083	12615.413882	28.463860
316.027732	12658.175852	28.468877
316.579092	12685.352687	28.473895
317.051357	12704.696859	28.478912
316.883720	12730.147322	28.483930
317.380056	12753.729673	28.488948
317.508011	12784.663446	28.493965
318.150826	12813.913073	28.498983
318.099256	12838.675841	28.504000
318.362872	12876.244468	28.509018
318.991421	12891.341559	28.514036
319.003640	12937.881014	28.519053
319.415860	12961.863098	28.524071
319.984500	12989.402769	28.529088
319.982999	13022.189115	28.534106
320.291012	13041.224560	28.539124
321.070405	13073.279435	28.544141
321.385995	13096.876070	28.549159
321.812525	13131.262223	28.554176
322.129430	13148.552310	28.559194
322.699145	13172.015379	28.564212
322.569552	13198.411068	28.569229
323.320793	13221.327814	28.574247
323.821473	13236.517654	28.579264
323.901441	13263.681502	28.584282
323.998239	13288.785719	28.589300
324.284781	13307.058304	28.594317
324.780731	13330.036761	28.599335
325.424521	13355.398894	28.604352
325.366905	13380.683142	28.609370
326.221415	13393.965588	28.614388
326.372448	13421.405122	28.619405
326.651052	13438.143529	28.624423
326.661384	13455.469539	28.629440
327.056512	13483.179549	28.634458
327.529295	13508.582672	28.639476
327.927701	13537.497938	28.644493
328.288162	13544.950693	28.649511
329.251650	13564.013298	28.654528
329.220861	13570.855467	28.659546
329.838356	13571.938337	28.664564
329.552963	13587.023943	28.669581
329.719456	13605.851704	28.674599
330.221106	13614.674935	28.679616
330.234410	13637.984941	28.684634
330.333914	13653.445871	28.689652
330.654754	13685.162328	28.694669
330.849343	13709.536775	28.699687
331.491349	13734.563986	28.704704
331.721323	13768.866395	28.709722
332.245270	13783.396743	28.714740
332.236549	13813.553794	28.719757
332.464169	13841.554347	28.724775
333.118684	13874.782202	28.729792
333.300850	13899.480900	28.734810
333.997351	13911.049545	28.739828
333.975165	13943.101353	28.744845
334.596758	13967.620314	28.749863
335.086725	13998.490880	28.754880
335.106904	14024.956917	28.759898
335.235519	14041.966778	28.764916
335.534891	14069.832352	28.769933
335.722429	14098.118462	28.774951
336.722295	14117.666404	28.779968
338.396709	14103.458166	28.784986
339.100087	14097.862289	28.790004
340.470687	14100.462504	28.795021
340.790771	14071.671665	28.800039
340.834930	14056.872882	28.805056
340.904144	14060.250135	28.810074
341.427931	14024.491429	28.815092
341.499668	14026.514850	28.820109
341.473664	14023.636006	28.825127
341.644254	14020.240514	28.830144
341.780605	14019.985863	28.835162
341.883097	14013.659692	28.840180
341.900564	14029.432333	28.845197
342.046718	14054.424848	28.850215
342.147679	14057.821938	28.855232
342.242983	14075.341852	28.860250
342.570256	14092.421762	28.865268
342.818780	14118.390555	28.870285
342.779087	14147.974495	28.875303
343.390787	14170.270374	28.880320
342.907945	14202.546005	28.885338
343.222407	14222.382212	28.890356
343.306062	14267.424794	28.895373
344.002066	14313.757418	28.900391
344.596349	14339.009815	28.905408
344.398272	14390.790909	28.910426
344.536772	14421.217167	28.915444
345.451850	14460.136549	28.920461
345.690215	14494.719800	28.925479
346.162291	14529.936713	28.930496
346.445838	14557.758266	28.935514
346.978809	14573.513277	28.940532
347.372587	14605.214803	28.945549
347.658761	14638.315852	28.950567
348.549611	14655.985284	28.955584
348.640770	14692.132987	28.960602
348.427433	14707.800711	28.965620
348.915970	14743.386582	28.970637
349.132195	14764.639177	28.975655
349.677563	14804.197378	28.980672
350.109609	14842.711137	28.985690
350.644085	14868.547753	28.990708
350.568570	14912.918307	28.995725
350.573662	14936.955777	29.000743
351.939732	14955.239862	29.005760
352.268587	15000.809986	29.010778
352.631109	15022.517102	29.015796
353.321822	15027.586266	29.020813
353.788420	15056.955664	29.025831
354.113369	15077.602096	29.030848
354.293310	15103.868379	29.035866
354.408993	15126.311910	29.040884
355.144957	15152.296000	29.045901
355.020315	15182.871883	29.050919
355.552190	15198.489842	29.055936
355.786129	15226.853105	29.060954
356.319692	15249.791160	29.065972
356.608926	15274.584835	29.070989
356.690171	15298.617721	29.076007
357.081380	15331.790027	29.081024
357.332361	15367.038582	29.086042
357.735449	15395.790101	29.091060
357.915282	15427.781318	29.096077
358.502163	15458.177637	29.101095
359.315342	15481.349589	29.106112
359.584653	15512.894501	29.111130
359.955875	15527.622776	29.116148
360.300493	15548.724714	29.121165
361.094734	15570.375617	29.126183
361.620670	15572.817349	29.131200
362.017119	15598.691559	29.136218
362.441977	15611.756468	29.141236
362.731534	15629.913941	29.146253
362.628914	15643.772488	29.151271
363.417310	15661.341910	29.156288
363.733503	15681.719323	29.161306
364.375895	15688.516569	29.166324
364.822621	15696.844021	29.171341
364.833689	15706.894041	29.176359
365.591600	15725.013012	29.181376
365.672221	15728.404561	29.186394
366.070183	15740.898349	29.191412
366.367999	15753.340199	29.196429
366.223259	15764.375204	29.201447
366.998510	15773.510282	29.206464
366.807230	15797.674174	29.211482
367.252508	15816.229443	29.216500
367.702028	15830.210383	29.221517
367.847572	15858.643615	29.226535
368.319017	15877.664813	29.231552
368.623849	15899.230607	29.236570
369.151669	15905.033527	29.241588
370.600651	15891.161550	29.246605
370.895122	15903.751677	29.251623
371.771364	15917.261791	29.256640
371.367383	15934.182260	29.261658
371.575061	15937.590219	29.266676
371.737313	15940.098628	29.271693
372.031390	15968.715064	29.276711
372.446212	15970.503187	29.281728
372.292239	15989.962338	29.286746
372.288865	16013.874208	29.291764
372.707344	16037.273269	29.296781
372.638274	16079.272185	29.301799
373.323783	16101.023836	29.306816
373.558726	16132.854207	29.311834
373.944393	16170.802165	29.316852
374.585638	16197.307797	29.321869
374.543230	16242.103037	29.326887
375.303012	16268.580456	29.331904
375.451696	16297.207088	29.336922
375.447672	16334.446352	29.341940
376.263368	16358.902588	29.346957
376.345958	16400.048354	29.351975
376.773322	16432.219516	29.356992
377.050592	16473.978697	29.362010
378.457659	16489.806911	29.367028
380.147591	16476.950280	29.372045
380.608869	16487.377853	29.377063
381.398136	16484.045137	29.382080
382.127736	16479.174606	29.387098
382.222864	16471.709517	29.392116
382.477856	16468.869389	29.397133
382.827640	16480.384524	29.402151
383.026783	16470.215859	29.407168
383.053459	16473.283518	29.412186
383.147698	16474.570859	29.417204
383.484933	16481.652899	29.422221
383.655620	16489.916906	29.427239
383.975693	16505.106993	29.432256
384.279828	16527.785311	29.437274
384.477212	16538.181353	29.442292
384.553518	16559.853774	29.447309
384.425099	16591.179251	29.452327
384.997373	16605.011622	29.457344
385.232288	16645.559007	29.462362
385.570413	16675.368082	29.467380
385.942017	16699.503329	29.472397
386.156244	16732.518283	29.477415
386.605083	16752.568123	29.482432
387.017727	16781.175636	29.487450
387.277138	16813.000754	29.492468
387.605901	16836.637754	29.497485
387.819786	16878.817361	29.502503
388.212551	16901.756500	29.507520
388.804871	16944.488159	29.512538
388.831778	16987.937957	29.517556
389.391259	17010.075528	29.522573
389.284768	17048.902457	29.527591
389.814760	17079.928344	29.532608
390.508667	17131.678254	29.537626
390.685579	17163.850691	29.542644
391.260620	17194.515703	29.547661
391.709858	17246.080972	29.552679
391.915541	17271.691347	29.557696
392.293967	17312.056979	29.562714
392.317764	17359.604285	29.567732
393.185676	17394.593811	29.572749
393.462782	17434.190485	29.577767
393.553641	17481.960547	29.582784
394.187867	17520.484800	29.587802
394.575528	17554.890981	29.592820
395.147813	17601.487462	29.597837
395.196126	17647.069147	29.602855
395.757777	17688.797113	29.607872
396.559953	17730.847104	29.612890
396.529841	17779.845236	29.617908
397.541721	17800.414989	29.622925
397.948743	17849.322820	29.627943
398.400452	17873.111103	29.632960
398.645847	17912.632157	29.637978
398.604631	17950.062718	29.642996
399.332407	17983.899897	29.648013
401.241445	17977.077954	29.653031
402.044607	17985.591595	29.658048
402.842774	17981.930185	29.663066
403.187572	18001.084027	29.668084
403.348587	18011.081135	29.673101
403.723832	18022.372493	29.678119
403.799845	18029.696479	29.683136
403.890011	18051.990639	29.688154
404.249327	18062.732188	29.693172
404.735661	18070.506575	29.698189
404.915989	18096.917253	29.703207
405.340727	18120.253901	29.708224
405.355277	18139.849918	29.713242
405.563231	18170.078485	29.718260
406.190005	18198.382045	29.723277
406.308747	18221.822722	29.728295
406.683168	18251.039846	29.733312
407.027660	18284.870643	29.738330
407.164739	18323.734776	29.743348
407.778389	18348.480311	29.748365
407.874015	18384.110110	29.753383
408.373002	18415.322750	29.758400
408.745973	18445.513353	29.763418
409.059551	18486.689258	29.768436
409.507997	18519.182669	29.773453
409.791070	18547.327049	29.778471
410.193713	18575.154772	29.783488
410.229266	18609.839483	29.788506
410.658170	18663.925445	29.793524
411.079650	18686.673659	29.798541
411.544448	18736.375516	29.803559
411.685319	18779.996811	29.808576
412.585986	18812.468782	29.813594
413.506527	18838.911604	29.818612
413.789818	18872.910132	29.823629
414.141293	18910.387915	29.828647
414.506615	18936.763058	29.833664
415.053898	18967.059584	29.838682
415.422596	19003.137484	29.843700
416.513736	19012.478330	29.848717
417.711668	19031.012427	29.853735
418.475282	19025.526602	29.858752
419.286466	19022.663745	29.863770
419.797342	19025.436630	29.868788
420.134264	19023.877792	29.873805
420.698038	19031.076105	29.878823
420.858511	19030.198981	29.883840
421.530086	19035.179532	29.888858
421.220996	19037.114475	29.893876
421.752725	19028.673598	29.898893
421.670943	19048.549906	29.903911
421.776323	19065.099663	29.908928
422.112167	19077.528092	29.913946
422.318279	19098.863455	29.918964
422.801585	19124.907098	29.923981
422.860034	19153.921906	29.928999
422.990067	19181.269295	29.934016
423.431144	19216.360471	29.939034
423.561013	19253.216053	29.944052
423.846583	19291.206485	29.949069
424.054268	19334.854119	29.954087
424.335629	19383.543452	29.959104
425.173368	19425.070649	29.964122
425.697084	19460.896142	29.969140
426.349052	19501.178190	29.974157
426.846515	19535.427535	29.979175
427.387939	19562.335194	29.984192
427.712840	19591.366633	29.989210
428.063846	19633.317253	29.994228
428.684312	19659.615166	29.999245
429.439111	19704.004718	30.004263
429.342199	19738.775248	30.009280
429.965622	19764.305441	30.014298
430.203257	19795.311270	30.019316
431.082241	19817.618507	30.024333
431.528618	19855.835509	30.029351
431.589020	19883.751201	30.034368
432.289703	19897.186480	30.039386
432.291794	19935.050779	30.044404
432.984999	19966.613588	30.049421
432.993078	19997.256724	30.054439
433.519295	20028.106781	30.059456
433.975549	20062.485123	30.064474
434.196266	20095.675679	30.069492
434.691131	20130.822156	30.074509
435.114566	20171.100601	30.079527
434.863254	20213.853969	30.084544
435.689391	20247.754031	30.089562
435.730595	20288.092099	30.094580
436.477584	20336.969697	30.099597
436.847786	20380.744373	30.104615
437.160722	20427.941497	30.109632
437.419035	20470.236345	30.114650
438.007931	20512.333729	30.119668
438.119695	20564.301187	30.124685
438.512860	20632.557791	30.129703
438.709277	20678.502335	30.134720
439.718864	20727.740175	30.139738
439.851221	20786.168558	30.144756
440.044416	20838.850864	30.149773
441.000381	20898.970076	30.154791
441.018952	20947.057561	30.159808
441.757200	21002.436837	30.164826
442.167271	21053.740926	30.169844
442.871704	21107.887896	30.174861
443.672973	21153.616172	30.179879
443.980570	21205.226909	30.184896
444.403346	21248.405722	30.189914
445.034068	21288.922566	30.194932
445.919966	21328.692396	30.199949
446.740542	21361.868022	30.204967
447.040983	21405.192769	30.209984
447.492292	21423.678166	30.215002
447.752962	21461.818394	30.220020
448.016836	21496.340782	30.225037
448.696487	21531.901214	30.230055
448.955172	21581.697689	30.235072
449.877779	21610.960546	30.240090
449.975893	21646.583958	30.245108
450.397337	21686.254627	30.250125
451.046709	21728.196769	30.255143
451.487974	21762.538682	30.260160
452.033722	21796.021281	30.265178
451.995825	21840.145414	30.270196
452.381944	21877.780703	30.275213
453.140643	21911.538365	30.280231
453.244418	21953.405779	30.285248
453.915832	21995.932682	30.290266
454.135538	22041.208790	30.295284
454.634037	22077.762574	30.300301
455.745471	22105.633681	30.305319
456.128638	22129.852858	30.310336
456.534591	22167.710939	30.315354
456.945169	22193.006471	30.320372
457.314087	22219.679159	30.325389
457.902038	22249.768398	30.330407
458.067559	22278.977472	30.335424
458.852786	22311.492816	30.340442
459.110670	22338.456703	30.345460
459.309748	22379.189252	30.350477
461.124453	22376.449896	30.355495
463.106771	22367.400064	30.360512
464.154280	22360.708488	30.365530
464.306368	22352.857602	30.370548
464.728180	22330.911529	30.375565
465.335655	22324.676013	30.380583
465.582406	22313.569732	30.385600
465.825095	22310.471202	30.390618
465.700519	22317.348295	30.395636
465.796331	22329.927420	30.400653
466.734837	22320.461845	30.405671
466.382557	22337.039513	30.410688
466.856674	22340.828220	30.415706
466.721505	22363.754335	30.420724
467.195305	22393.961281	30.425741
467.576290	22422.772407	30.430759
467.290446	22453.541566	30.435776
467.719000	22482.527955	30.440794
468.064540	22513.176163	30.445812
468.127249	22564.799635	30.450829
468.549909	22599.015582	30.455847
468.934101	22644.587786	30.460864
469.426452	22695.483971	30.465882
469.395871	22753.839245	30.470900
469.732050	22809.174704	30.475917
470.461231	22863.727823	30.480935
470.678484	22914.620489	30.485952
471.406185	22980.687547	30.490970
471.842047	23035.057984	30.495988
472.320336	23096.779508	30.501005
473.319702	23145.234916	30.506023
473.777957	23184.213471	30.511040
474.479801	23233.288400	30.516058
475.269007	23271.659919	30.521076
476.093010	23299.309545	30.526093
476.427185	23341.654335	30.531111
476.797872	23381.790258	30.536128
477.508181	23415.595865	30.541146
478.197488	23447.261582	30.546164
478.273615	23498.329046	30.551181
478.898160	23530.551906	30.556199
479.289306	23565.019927	30.561216
480.074556	23599.548909	30.566234
480.471899	23638.836821	30.571252
480.703444	23662.545285	30.576269
481.675582	23696.773737	30.581287
482.365029	23726.409289	30.586304
482.979681	23735.362201	30.591322
483.478452	23749.441852	30.596340
483.489108	23771.257362	30.601357
484.016443	23785.910672	30.606375
484.187210	23811.549473	30.611392
484.700061	23840.123969	30.616410
484.819542	23882.328740	30.621428
485.515255	23919.789583	30.626445
486.073611	23948.594914	30.631463
486.240374	23996.980754	30.636480
486.425507	24028.032391	30.641498
487.156548	24068.179595	30.646516
487.466623	24115.588244	30.651533
488.004794	24144.728778	30.656551
488.458682	24197.197955	30.661568
488.859642	24232.900229	30.666586
489.398304	24284.774844	30.671604
489.684081	24332.568483	30.676621
490.560447	24374.280593	30.681639
490.858933	24417.645381	30.686656
491.536388	24452.555748	30.691674
492.176901	24492.181990	30.696692
492.676004	24530.518474	30.701709
493.021714	24578.925621	30.706727
493.381241	24621.840888	30.711744
494.060273	24651.294702	30.716762
495.401728	24675.803887	30.721780
496.346484	24699.805183	30.726797
496.918359	24714.995019	30.731815
497.399700	24752.477790	30.736832
497.552064	24778.233723	30.741850
498.059495	24787.925899	30.746868
498.152909	24835.060821	30.751885
498.676009	24864.869153	30.756903
499.189552	24898.659629	30.761920
499.575910	24923.185059	30.766938
500.050397	24967.979879	30.771956
500.251802	25005.909598	30.776973
500.583992	25025.421794	30.781991
500.970877	25068.920003	30.787008
501.442825	25118.805439	30.792026
501.905120	25161.084229	30.797044
502.163558	25213.285367	30.802061
502.979968	25255.789235	30.807079
503.490884	25305.323207	30.812096
503.738607	25350.293080	30.817114
504.197225	25398.156113	30.822132
504.384093	25451.945790	30.827149
505.235780	25495.377417	30.832167
505.539664	25543.590890	30.837184
505.983304	25603.657497	30.842202
506.401184	25655.811829	30.847220
506.742661	25710.691693	30.852237
507.447672	25757.720867	30.857255
508.061385	25804.101389	30.862272
508.399002	25854.955091	30.867290
508.989917	25901.295408	30.872308
509.474719	25956.460526	30.877325
510.506074	25987.159785	30.882343
510.765310	26042.505300	30.887360
511.283116	26083.503773	30.892378
512.201301	26121.998686	30.897396
511.963469	26171.924035	30.902413
512.793146	26213.572750	30.907431
513.244327	26253.606152	30.912448
513.339499	26310.452749	30.917466
514.515324	26352.718706	30.922484
515.127796	26396.709272	30.927501
515.766994	26447.159128	30.932519
516.064158	26485.208651	30.937536
516.372035	26525.560208	30.942554
517.286763	26570.584022	30.947572
517.408841	26622.500254	30.952589
518.328079	26669.350644	30.957607
518.926038	26719.298182	30.962624
518.893841	26757.867220	30.967642
519.736876	26800.965767	30.972660
520.168059	26852.804350	30.977677
520.576570	26889.576517	30.982695
521.154691	26938.710095	30.987712
521.719987	26987.510236	30.992730
522.790132	27022.598435	30.997748
523.823605	27050.248774	31.002765
526.038791	27038.230852	31.007783
526.803036	27058.688321	31.012800
527.471630	27070.247101	31.017818
528.127786	27067.914586	31.022836
528.197928	27076.834792	31.027853
528.489469	27067.231598	31.032871
528.466836	27093.160928	31.037888
528.611980	27110.767293	31.042906
529.275458	27127.002156	31.047924
529.226702	27161.005139	31.052941
529.708638	27185.418741	31.057959
530.097989	27224.085624	31.062976
530.161635	27256.441575	31.067994
530.783770	27287.760025	31.073012
530.859475	27342.003109	31.078029
531.835154	27373.293774	31.083047
532.606194	27405.130798	31.088064
532.768581	27450.367519	31.093082
533.080763	27491.056444	31.098100
533.211483	27537.938839	31.103117
533.728023	27585.937027	31.108135
534.242471	27643.286447	31.113152
534.255886	27702.947207	31.118170
535.077696	27755.498608	31.123188
535.317452	27824.997758	31.128205
536.292779	27870.467023	31.133223
536.946944	27917.555513	31.138240
536.994269	27959.201775	31.143258
537.388653	28011.902457	31.148276
537.703391	28073.450124	31.153293
538.793428	28116.287499	31.158311
539.219734	28172.527680	31.163328
539.641916	28221.426828	31.168346
540.484594	28281.338981	31.173364
540.619470	28350.976850	31.178381
541.256101	28390.685019	31.183399
541.844388	28451.746154	31.188416
542.073781	28518.433835	31.193434
542.864554	28563.100801	31.198452
543.168599	28630.369583	31.203469
544.226053	28671.981272	31.208487
544.739882	28719.833536	31.213504
545.470138	28775.275685	31.218522
546.058904	28834.406124	31.223540
546.003157	28903.093348	31.228557
546.828719	28944.515739	31.233575
547.182086	28997.623279	31.238592
548.026695	29057.777527	31.243610
549.463350	29103.870183	31.248628
550.601234	29135.537138	31.253645
551.250691	29168.864194	31.258663
551.773404	29208.860417	31.263680
552.031679	29236.762479	31.268698
552.592884	29280.851788	31.273716
553.164085	29312.270517	31.278733
553.795659	29336.873131	31.283751
554.730949	29381.427924	31.288768
554.856736	29427.173973	31.293786
555.437361	29460.395969	31.298804
555.879755	29499.146498	31.303821
556.889042	29529.241397	31.308839
556.807882	29574.637858	31.313856
557.429373	29618.253564	31.318874
558.176879	29639.019560	31.323892
558.700334	29691.530187	31.328909
558.988159	29721.644216	31.333927
559.463686	29767.064441	31.338944
559.743795	29802.074901	31.343962
560.219486	29852.811194	31.348980
560.742604	29908.318560	31.353997
561.516086	29949.078848	31.359015
562.027607	29999.918637	31.364032
562.297768	30059.280775	31.369050
562.803658	30107.533959	31.374068
563.111188	30156.006426	31.379085
563.848157	30209.474460	31.384103
564.800446	30253.721602	31.389120
565.291642	30314.367035	31.394138
565.943527	30365.757710	31.399156
566.368018	30417.477912	31.404173
566.796346	30457.826351	31.409191
567.582268	30509.457757	31.414208
568.073447	30555.314249	31.419226
568.491033	30593.407795	31.424244
568.697708	30638.980432	31.429261
569.723841	30694.996653	31.434279
570.869743	30719.730635	31.439296
572.187462	30742.473478	31.444314
572.836327	30770.066927	31.449332
573.371338	30806.399106	31.454349
573.946507	30832.565419	31.459367
574.140034	30862.230039	31.464384
574.588625	30904.670994	31.469402
575.154705	30921.751061	31.474420
575.862189	30967.467082	31.479437
575.843855	30996.768506	31.484455
576.240629	31036.150932	31.489472
576.527285	31074.895321	31.494490
577.059277	31127.568381	31.499508
577.521162	31194.381250	31.504525
578.064596	31230.958904	31.509543
578.709784	31285.800548	31.514560
578.641764	31350.211288	31.519578
579.643586	31407.954975	31.524596
580.066299	31469.859170	31.529613
580.259367	31542.261201	31.534631
580.734488	31605.725847	31.539648
581.268979	31665.765698	31.544666
581.891556	31746.855908	31.549684
582.452179	31803.774399	31.554701
584.376680	31840.598435	31.559719
585.358135	31888.478484	31.564736
585.728698	31945.370991	31.569754
587.026250	31976.649210	31.574772
587.952539	32012.341695	31.579789
588.399815	32050.052445	31.584807
589.098450	32072.823240	31.589824
589.767482	32114.491386	31.594842
590.509713	32138.588814	31.599860
590.992360	32175.876519	31.604877
591.094274	32194.812977	31.609895
591.722255	32226.997460	31.614912
591.860571	32279.785765	31.619930
592.335200	32313.777567	31.624948
593.072585	32354.511756	31.629965
593.191424	32400.963887	31.634983
594.205023	32453.400557	31.640000
594.654516	32507.564966	31.645018
595.118136	32543.417406	31.650036
596.146578	32579.569310	31.655053
596.571340	32620.530485	31.660071
597.408921	32656.602616	31.665088
597.454110	32721.315923	31.670106
598.322829	32754.104642	31.675124
598.868870	32802.940990	31.680141
599.451407	32854.586930	31.685159
599.807933	32888.926593	31.690176
599.683097	32939.897303	31.695194
600.230014	32986.796778	31.700212
600.858413	33051.795232	31.705229
601.006310	33112.338547	31.710247
601.901910	33159.449379	31.715264
602.087303	33226.234107	31.720282
602.474757	33297.791595	31.725300
603.022382	33356.000639	31.730317
603.414546	33427.844831	31.735335
603.906950	33494.313764	31.740352
604.781191	33577.529321	31.745370
605.327769	33644.139980	31.750388
605.615541	33720.244069	31.755405
605.946840	33795.305889	31.760423
606.974108	33861.806188	31.765440
607.795199	33951.403848	31.770458
610.000340	33986.422448	31.775476
611.653067	34018.984779	31.780493
612.265064	34058.232935	31.785511
613.046163	34095.348168	31.790528
613.591015	34128.774462	31.795546
614.181797	34160.615515	31.800564
614.951149	34205.036409	31.805581
615.220481	34241.732166	31.810599
615.860061	34279.396874	31.815616
616.358836	34323.925809	31.820634
616.530153	34361.999478	31.825652
617.296811	34408.051379	31.830669
617.702373	34451.012751	31.835687
618.247152	34489.525394	31.840704
618.669095	34548.474335	31.845722
619.156529	34599.075161	31.850740
620.010354	34657.128069	31.855757
620.228839	34706.586549	31.860775
620.791646	34748.093787	31.865792
621.686301	34809.213269	31.870810
622.291548	34865.562903	31.875828
622.831997	34914.994375	31.880845
622.937104	34972.412473	31.885863
623.515016	35030.620973	31.890880
624.020968	35107.598404	31.895898
624.758018	35170.141090	31.900916
625.258575	35232.426862	31.905933
625.662332	35304.129098	31.910951
626.232681	35366.397948	31.915968
627.104871	35425.137969	31.920986
627.610305	35506.016089	31.926004
628.472436	35571.974073	31.931021
628.861792	35655.002893	31.936039
629.621025	35717.365940	31.941056
630.050296	35797.423592	31.946074
630.438638	35873.959758	31.951092
631.070390	35940.296418	31.956109
631.559702	36014.713982	31.961127
632.582693	36070.700019	31.966144
632.884151	36136.684865	31.971162
634.316114	36172.159157	31.976180
635.897934	36225.449017	31.981197
636.264643	36270.488183	31.986215
637.198719	36325.221631	31.991232
637.722020	36366.110101	31.996250
638.357082	36415.739049	32.001268
639.362589	36453.779232	32.006285
639.667725	36499.379062	32.011303
640.233539	36537.082678	32.016320
640.641918	36586.401366	32.021338
641.181121	36639.699329	32.026356
641.737835	36687.490568	32.031373
642.520036	36735.577135	32.036391
642.697388	36785.590662	32.041408
643.390585	36848.583326	32.046426
643.963575	36915.013600	32.051444
644.337339	36982.171177	32.056461
644.982237	37046.630703	32.061479
645.927349	37104.529347	32.066496
646.357814	37170.500854	32.071514
647.018218	37230.651070	32.076532
647.342584	37306.507031	32.081549
647.941469	37373.923587	32.086567
648.607321	37433.252187	32.091584
648.973332	37511.563703	32.096602
649.566369	37589.090480	32.101620
650.446156	37663.156720	32.106637
650.870966	37727.827333	32.111655
651.835528	37814.452185	32.116672
652.256689	37887.752023	32.121690
652.698374	37962.731328	32.126708
654.054795	38026.422202	32.131725
654.482772	38106.722806	32.136743
655.240189	38177.021761	32.141760
656.159818	38245.820870	32.146778
656.958566	38314.735692	32.151796
658.298041	38366.449975	32.156813
659.306686	38426.564761	32.161831
660.410414	38461.982636	32.166848
660.780027	38522.524342	32.171866
661.478342	38565.547371	32.176884
662.268645	38613.913945	32.181901
662.763375	38663.619151	32.186919
663.378476	38702.251667	32.191936
663.821749	38762.519167	32.196954
664.416949	38811.522879	32.201972
665.288135	38870.331842	32.206989
665.164468	38928.738053	32.212007
666.344463	38978.549521	32.217024
667.108177	39035.088131	32.222042
667.747733	39087.414357	32.227060
668.480581	39132.598380	32.232077
668.915923	39187.592401	32.237095
669.563060	39235.248712	32.242112
669.876926	39277.014901	32.247130
670.905549	39328.647585	32.252148
671.289780	39368.944163	32.257165
671.652462	39442.512326	32.262183
672.169424	39491.987762	32.267200
672.756889	39555.863594	32.272218
673.496944	39620.478603	32.277236
674.157780	39679.574589	32.282253
674.206100	39751.374356	32.287271
674.683296	39819.677857	32.292288
675.408357	39883.526700	32.297306
675.643703	39966.973347	32.302324
676.562415	40042.956620	32.307341
676.795408	40134.301906	32.312359
677.702297	40217.696468	32.317376
678.561190	40297.746398	32.322394
679.379821	40377.576025	32.327412
680.319129	40455.175851	32.332429
680.972907	40535.537104	32.337447
681.841838	40611.546601	32.342464
682.645824	40687.002200	32.347482
683.032731	40769.690576	32.352500
684.150494	40829.925793	32.357517
684.583262	40914.884811	32.362535
685.059458	40988.479393	32.367552
685.972484	41066.379503	32.372570
686.305207	41151.390315	32.377588
687.443516	41216.414753	32.382605
687.807308	41305.080190	32.387623
688.758432	41374.771654	32.392640
689.562861	41455.810303	32.397658
690.490769	41522.345562	32.402676
691.815508	41577.746602	32.407693
692.630556	41644.581030	32.412711
693.604628	41708.630439	32.417728
694.379022	41765.324628	32.422746
694.781445	41827.039877	32.427764
695.255313	41887.520115	32.432781
695.898119	41945.658424	32.437799
696.628391	42011.078884	32.442816
697.158570	42067.286183	32.447834
697.746053	42144.309335	32.452852
698.740552	42206.543614	32.457869
699.258684	42287.824176	32.462887
699.974107	42343.605435	32.467904
700.600655	42411.567412	32.472922
701.225603	42476.391304	32.477940
701.882270	42541.412270	32.482957
702.489179	42620.585748	32.487975
702.921468	42686.579842	32.492992
703.803627	42775.567762	32.498010
703.827582	42851.529264	32.503028
704.858678	42917.775892	32.508045
705.213380	43011.637471	32.513063
706.024368	43067.437396	32.518080
707.342837	43125.159810	32.523098
708.135068	43186.508711	32.528116
710.097574	43215.605857	32.533133
710.990637	43273.920148	32.538151
711.630486	43306.966140	32.543168
712.608935	43350.377721	32.548186
712.562938	43405.507616	32.553204
713.223831	43451.225509	32.558221
713.764482	43512.091963	32.563239
714.179869	43562.924936	32.568256
714.838066	43625.732066	32.573274
715.008121	43690.689710	32.578292
715.744372	43755.264076	32.583309
716.288924	43832.509778	32.588327
716.786761	43901.346687	32.593344
717.535148	43985.289459	32.598362
717.609248	44068.810003	32.603380
718.589735	44141.993867	32.608397
719.994252	44224.830148	32.613415
720.791232	44279.724498	32.618432
721.876969	44351.867212	32.623450
722.515663	44425.106683	32.628468
723.378103	44482.313135	32.633485
723.872564	44558.166172	32.638503
724.461473	44623.325609	32.643520
725.420339	44687.278052	32.648538
726.127757	44765.934236	32.653556
727.311008	44838.274811	32.658573
727.894986	44901.650453	32.663591
728.283429	44975.436847	32.668608
729.166315	45041.323977	32.673626
729.895470	45124.821002	32.678644
730.107926	45182.496038	32.683661
730.908715	45261.417217	32.688679
731.604785	45338.134375	32.693696
732.577891	45415.243144	32.698714
733.123648	45495.729802	32.703732
734.210238	45566.123265	32.708749
734.533416	45641.680156	32.713767
735.053388	45732.785267	32.718784
735.866913	45813.495774	32.723802
736.845595	45898.916010	32.728820
737.364232	45971.020030	32.733837
737.834149	46056.922716	32.738855
738.292430	46141.896936	32.743872
739.765574	46235.563094	32.748890
740.217208	46317.005555	32.753908
741.110134	46390.086574	32.758925
742.180904	46467.228593	32.763943
742.446727	46545.565523	32.768960
743.699028	46621.193262	32.773978
744.366016	46704.956959	32.778996
744.973405	46785.584852	32.784013
745.610326	46857.364471	32.789031
746.432913	46928.783531	32.794048
747.220030	46995.163372	32.799066
747.707901	47080.534966	32.804084
748.683171	47142.180992	32.809101
749.755802	47214.744614	32.814119
749.845193	47283.808130	32.819136
750.954377	47356.700974	32.824154
751.566576	47431.948185	32.829172
752.734983	47488.156542	32.834189
753.702300	47564.385874	32.839207
753.946309	47636.209123	32.844224
754.801647	47690.271867	32.849242
755.702763	47761.003403	32.854260
756.569512	47838.638274	32.859277
757.636460	47905.680636	32.864295
758.057372	47973.125855	32.869312
758.683679	48043.141822	32.874330
759.874566	48111.806035	32.879348
760.723448	48171.995900	32.884365
761.757337	48227.290871	32.889383
762.369860	48295.940583	32.894400
763.462626	48346.218895	32.899418
763.838423	48425.111469	32.904436
764.537656	48488.036761	32.909453
765.358733	48553.268462	32.914471
766.271816	48623.932122	32.919488
766.901496	48689.519807	32.924506
767.246370	48760.817208	32.929524
767.936040	48833.309593	32.934541
768.521966	48909.501297	32.939559
769.611852	48997.645212	32.944576
770.523024	49062.586755	32.949594
771.189174	49145.986628	32.954612
771.766497	49221.619345	32.959629
772.863777	49269.513932	32.964647
773.569898	49353.646824	32.969664
774.762808	49410.172951	32.974682
774.913100	49494.079421	32.979700
775.569954	49563.127736	32.984717
776.394286	49644.582971	32.989735
777.107260	49734.456723	32.994752
778.018963	49804.248013	32.999770
778.407947	49889.847666	33.004788
778.966647	49979.513686	33.009805
780.275700	50057.599073	33.014823
780.777270	50137.896133	33.019840
781.373018	50233.345176	33.024858
781.783330	50321.310323	33.029876
782.642861	50397.780407	33.034893
783.945695	50501.440165	33.039911
784.546537	50581.767594	33.044928
785.915721	50641.258136	33.049946
787.050509	50726.597905	33.054964
787.582470	50793.079892	33.059981
788.675743	50868.918325	33.064999
789.025833	50946.648987	33.070016
790.050792	51011.491143	33.075034
791.001823	51070.740396	33.080052
791.711492	51125.515290	33.085069
792.733753	51188.906794	33.090087
793.062962	51260.532246	33.095104
793.834951	51318.709391	33.100122
794.759196	51390.111252	33.105140
795.236236	51458.141401	33.110157
795.976920	51519.817854	33.115175
796.550103	51595.095161	33.120192
797.752724	51674.997157	33.125210
798.047188	51753.475511	33.130228
799.087325	51825.766437	33.135245
800.316691	51893.040959	33.140263
800.965738	51965.457818	33.145280
801.639310	52037.864751	33.150298
802.313532	52130.960100	33.155316
802.912465	52204.411626	33.160333
803.702644	52290.220811	33.165351
804.414291	52370.585932	33.170368
805.121180	52453.833739	33.175386
805.785614	52553.122044	33.180404
806.441640	52635.438243	33.185421
806.969735	52737.624549	33.190439
807.615987	52831.665349	33.195456
808.339848	52929.469147	33.200474
809.079233	53042.143288	33.205492
809.869699	53145.533698	33.210509
810.570099	53254.759242	33.215527
811.716923	53352.542187	33.220544
812.567406	53449.845719	33.225562
813.498834	53547.723970	33.230580
814.498574	53638.698377	33.235597
815.800312	53737.714973	33.240615
816.164965	53843.039392	33.245632
817.312173	53934.746188	33.250650
818.202566	54028.602819	33.255668
818.879514	54114.615417	33.260685
820.281346	54198.881156	33.265703
821.321296	54279.167755	33.270720
822.404514	54364.495045	33.275738
823.000389	54449.543616	33.280756
823.973368	54527.929130	33.285773
825.320417	54601.785797	33.290791
826.064951	54675.239927	33.295808
827.434895	54737.351168	33.300826
827.952220	54792.840122	33.305844
828.436071	54873.044234	33.310861
829.414817	54946.471648	33.315879
829.835546	55027.582955	33.320896
830.604082	55110.533235	33.325914
831.082639	55195.061010	33.330932
831.601384	55280.002612	33.335949
832.352926	55361.473110	33.340967
832.847500	55453.322979	33.345984
833.709075	55533.425671	33.351002
834.367249	55623.864569	33.356020
835.073314	55713.579714	33.361037
835.758560	55804.501328	33.366055
836.458644	55907.006313	33.371072
837.225316	56005.848888	33.376090
837.977061	56106.882023	33.381108
838.470293	56198.325446	33.386125
839.810440	56286.591359	33.391143
840.420263	56406.990569	33.396160
841.384958	56498.755053	33.401178
842.277849	56602.098202	33.406196
843.034372	56702.751864	33.411213
844.540951	56786.018427	33.416231
846.159766	56875.139376	33.421248
847.229316	56954.255454	33.426266
848.280659	57034.340796	33.431284
849.151248	57117.050275	33.436301
850.249506	57179.958081	33.441319
850.850710	57264.573706	33.446336
851.534847	57339.970709	33.451354
852.664793	57416.209445	33.456372
853.344653	57500.580013	33.461389
854.451395	57569.887092	33.466407
854.718144	57658.999701	33.471424
855.613003	57727.921204	33.476442
856.182428	57822.946970	33.481460
856.747486	57925.213143	33.486477
857.639416	58017.795501	33.491495
858.519745	58112.479659	33.496512
859.255833	58199.035505	33.501530
860.340341	58288.485092	33.506548
860.876484	58389.997549	33.511565
861.846417	58483.977919	33.516583
862.545088	58590.712861	33.521600
863.450050	58678.478533	33.526618
864.343820	58788.785958	33.531636
864.833500	58889.497120	33.536653
866.526257	58971.654640	33.541671
866.886061	59077.767486	33.546688
868.277321	59174.525855	33.551706
869.029641	59277.457949	33.556724
869.667205	59377.118919	33.561741
870.684257	59479.097522	33.566759
871.343922	59571.301481	33.571776
871.878697	59668.770200	33.576794
873.141616	59764.330140	33.581812
873.698617	59878.309672	33.586829
875.280470	59975.063961	33.591847
875.964937	60070.610168	33.596864
876.774754	60173.222294	33.601882
878.021660	60258.430781	33.606900
878.197953	60364.513815	33.611917
879.633660	60448.013323	33.616935
880.040428	60544.360783	33.621952
881.187391	60627.420780	33.626970
882.120178	60725.270550	33.631988
882.404329	60825.289114	33.637005
883.800301	60902.781767	33.642023
884.659975	60994.357791	33.647040
885.607464	61085.459273	33.652058
886.200396	61174.824074	33.657076
886.860387	61283.389848	33.662093
887.699290	61374.876298	33.667111
888.508764	61475.648342	33.672128
889.270537	61592.327608	33.677146
890.602441	61688.950518	33.682164
891.150754	61795.778153	33.687181
891.881738	61895.942854	33.692199
892.353990	61999.076522	33.697216
893.529552	62115.797379	33.702234
894.184016	62216.692775	33.707252
895.327597	62341.627289	33.712269
896.372258	62451.041696	33.717287
897.161973	62550.243680	33.722304
898.560069	62649.548318	33.727322
900.724146	62735.095745	33.732340
901.656600	62841.110248	33.737357
902.733610	62919.558795	33.742375
903.401975	63009.381315	33.747392
904.165763	63091.553112	33.752410
905.343003	63187.314581	33.757428
905.967507	63276.081100	33.762445
907.034101	63368.507296	33.767463
907.598407	63461.133874	33.772480
908.168063	63556.810718	33.777498
909.189430	63653.354107	33.782516
909.504369	63759.500411	33.787533
910.842790	63848.433905	33.792551
911.456189	63963.982863	33.797568
912.186933	64065.318063	33.802586
913.139017	64170.847334	33.807604
913.902550	64286.958610	33.812621
914.999679	64398.905555	33.817639
915.521032	64512.056460	33.822656
916.556195	64624.968363	33.827674
917.746393	64724.822222	33.832692
918.537351	64843.421196	33.837709
919.631595	64945.549626	33.842727
921.042057	65045.089021	33.847744
921.978281	65148.105887	33.852762
923.187808	65239.820405	33.857780
924.047586	65341.574512	33.862797
925.260266	65439.075554	33.867815
925.885952	65536.743134	33.872832
926.485189	65634.210123	33.877850
927.659941	65733.443170	33.882868
928.610915	65840.216736	33.887885
929.541436	65930.273398	33.892903
930.436339	66024.113651	33.897920
931.260954	66117.870792	33.902938
932.493047	66197.839967	33.907956
933.128478	66280.178524	33.912973
934.243846	66364.749934	33.917991
934.949327	66454.996461	33.923008
935.536346	66556.790907	33.928026
936.985154	66652.415934	33.933044
937.086035	66743.404351	33.938061
938.173181	66850.338715	33.943079
938.981384	66951.689428	33.948096
939.688332	67062.065157	33.953114
940.467615	67177.502772	33.958132
940.940212	67281.656622	33.963149
942.436382	67399.198865	33.968167
943.390179	67506.208602	33.973184
943.960942	67633.318719	33.978202
945.129952	67747.080450	33.983220
946.194978	67870.285093	33.988237
946.860866	67993.977299	33.993255
947.819766	68105.083281	33.998272
948.828765	68230.781925	34.003290
949.878162	68339.290941	34.008308
950.940012	68461.173119	34.013325
951.603671	68574.647342	34.018343
953.235962	68702.454741	34.023360
954.250150	68820.979378	34.028378
954.982184	68936.251713	34.033396
955.923780	69050.120405	34.038413
956.660797	69183.892159	34.043431
957.788496	69291.010374	34.048448
958.788954	69419.238880	34.053466
959.939340	69536.021362	34.058484
960.573607	69664.353958	34.063501
961.721525	69781.182516	34.068519
962.441318	69894.617540	34.073536
963.247838	70026.659119	34.078554
964.374981	70145.249604	34.083572
965.321762	70278.028741	34.088589
966.742785	70395.822104	34.093607
967.737631	70523.370005	34.098624
968.365296	70630.777263	34.103642
969.566587	70747.432467	34.108660
970.743513	70878.087629	34.113677
971.743752	70990.694530	34.118695
972.844001	71109.238222	34.123712
973.645838	71237.946143	34.128730
974.922263	71336.926136	34.133748
975.538207	71457.191802	34.138765
976.379648	71587.292112	34.143783
977.389101	71705.847501	34.148800
978.450122	71826.253112	34.153818
979.524930	71951.819722	34.158836
980.447080	72070.024685	34.163853
981.668800	72177.604887	34.168871
982.660241	72287.560305	34.173888
983.135214	72398.919157	34.178906
984.096059	72497.594966	34.183924
985.177371	72612.763678	34.188941
986.428539	72722.294716	34.193959
987.500181	72825.485281	34.198976
988.125522	72944.014370	34.203994
989.079986	73053.657622	34.209012
989.959731	73158.725632	34.214029
991.050225	73273.700802	34.219047
992.223363	73398.009673	34.224064
992.567220	73522.091046	34.229082
994.083084	73624.380918	34.234100
994.787280	73750.586550	34.239117
995.904482	73877.239142	34.244135
997.094508	73997.732122	34.249152
997.517215	74127.612270	34.254170
998.602769	74248.312958	34.259188
999.342430	74382.207783	34.264205
1000.339945	74506.121728	34.269223
1001.500533	74639.041274	34.274240
1001.968543	74782.771121	34.279258
1002.957329	74912.503075	34.284276
1004.272845	75047.580978	34.289293
1005.344698	75181.693696	34.294311
1006.689978	75311.396780	34.299328
1007.274217	75452.054084	34.304346
1008.448358	75585.002982	34.309364
1009.741753	75735.705600	34.314381
1010.657311	75856.190149	34.319399
1011.325011	75991.339490	34.324416
1012.385714	76143.681136	34.329434
1014.021771	76277.540713	34.334452
1014.967400	76405.841785	34.339469
1015.613605	76541.971518	34.344487
1017.040376	76672.397176	34.349504
1017.870285	76815.458150	34.354522
1018.810357	76948.503773	34.359540
1019.712586	77091.770074	34.364557
1020.238419	77232.347856	34.369575
1022.005634	77363.602324	34.374592
1022.713312	77514.556665	34.379610
1023.854782	77643.902543	34.384628
1025.023256	77787.542205	34.389645
1026.328962	77923.582557	34.394663
1027.599577	78043.353562	34.399680
1028.944335	78178.561382	34.404698
1030.163979	78301.180020	34.409716
1032.048707	78404.061116	34.414733
1034.178550	78492.827208	34.419751
1035.942222	78578.270267	34.424768
1037.345283	78654.422436	34.429786
1038.998691	78723.411389	34.434804
1040.382216	78781.457716	34.439821
1041.521744	78839.561984	34.444839
1042.630443	78885.471848	34.449856
1043.183574	78931.508114	34.454874
1044.024424	78974.534169	34.459892
1044.853815	79026.247206	34.464909
1045.419810	79088.779624	34.469927
1046.159846	79134.476884	34.474944
1046.577260	79214.359309	34.479962
1047.599497	79284.032088	34.484980
1048.253195	79366.905321	34.489997
1048.793698	79450.719779	34.495015
1049.770146	79542.657466	34.500032
1050.620049	79634.678904	34.505050
1051.727590	79714.093178	34.510068
1052.434447	79818.180117	34.515085
1052.975265	79927.597550	34.520103
1054.115976	80034.322076	34.525120
1054.791803	80161.254614	34.530138
1055.662495	80277.657095	34.535156
1056.752902	80398.608318	34.540173
1057.249513	80525.413553	34.545191
1058.051152	80652.803193	34.550208
1059.102314	80787.967356	34.555226
1060.309554	80926.723521	34.560244
1060.909218	81072.341400	34.565261
1061.818361	81203.750515	34.570279
1062.892273	81347.297231	34.575296
1064.043945	81509.513378	34.580314
1064.852953	81658.066953	34.585332
1066.113194	81805.936591	34.590349
1067.005237	81964.556176	34.595367
1068.196930	82108.380192	34.600384
1069.181302	82274.776081	34.605402
1070.137307	82432.055088	34.610420
1071.414313	82579.421755	34.615437
1071.863911	82740.336632	34.620455
1073.384702	82891.207107	34.625472
1074.570860	83050.957723	34.630490
1075.757236	83212.878058	34.635508
1077.103799	83357.931484	34.640525
1079.037490	83503.075873	34.645543
1080.635287	83644.114543	34.650560
1082.037571	83776.169440	34.655578
1083.497516	83901.539447	34.660596
1084.828228	84016.757817	34.665613
1085.426333	84138.257828	34.670631
1086.795747	84264.358835	34.675648
1087.679001	84385.656846	34.680666
1088.601756	84515.364738	34.685684
1089.866690	84645.328813	34.690701
1090.407498	84771.779598	34.695719
1091.619815	84906.419825	34.700736
1092.679473	85032.878160	34.705754
1093.670903	85173.378528	34.710772
1094.872932	85303.799234	34.715789
1095.553145	85438.097496	34.720807
1096.747955	85564.594400	34.725824
1097.573238	85678.903145	34.730842
1098.447399	85806.034195	34.735860
1099.668252	85933.445985	34.740877
1101.119976	86055.453483	34.745895
1102.174509	86173.048051	34.750912
1103.303546	86308.703112	34.755930
1104.584492	86432.630560	34.760948
1105.542132	86560.562189	34.765965
1106.047765	86699.467860	34.770983
1107.169246	86822.423838	34.776000
1108.262758	86971.639684	34.781018
1109.046576	87119.729659	34.786036
1110.349596	87259.327851	34.791053
1111.174058	87408.532604	34.796071
1112.187187	87553.623360	34.801088
1113.344699	87701.506135	34.806106
1114.478300	87858.948764	34.811124
1115.665269	87999.468162	34.816141
1116.475837	88156.129602	34.821159
1117.516060	88301.195773	34.826176
1118.937846	88471.984483	34.831194
1120.307334	88619.017719	34.836212
1121.503098	88773.605045	34.841229
1122.411628	88928.365631	34.846247
1123.687384	89087.767656	34.851264
1124.301901	89238.700588	34.856282
1125.495638	89403.866539	34.861300
1127.091927	89569.203716	34.866317
1127.382647	89737.222537	34.871335
1128.550446	89898.911726	34.876352
1129.770625	90073.109560	34.881370
1130.663071	90247.373550	34.886388
1132.051915	90422.382155	34.891405
1132.857325	90587.656752	34.896423
1134.165753	90771.585752	34.901440
1135.587359	90936.119880	34.906458
1137.100739	91108.729800	34.911476
1138.489691	91266.308215	34.916493
1139.670943	91435.090185	34.921511
1141.116507	91585.767974	34.926528
1142.301818	91763.956694	34.931546
1143.310681	91916.534051	34.936564
1144.325092	92070.028685	34.941581
1145.334312	92242.575857	34.946599
1146.391069	92394.630252	34.951616
1147.643652	92567.805377	34.956634
1148.611370	92728.168310	34.961652
1150.415008	92879.000369	34.966669
1151.183323	93044.185393	34.971687
1152.246711	93216.067379	34.976704
1153.742824	93371.701908	34.981722
1155.150399	93537.358207	34.986740
1156.416216	93686.276150	34.991757
1157.518552	93834.601198	34.996775
1159.134525	93966.405811	35.001792
1159.843843	94119.880879	35.006810
1160.762236	94242.145408	35.011828
1162.169447	94383.024797	35.016845
1163.644293	94523.261760	35.021863
1164.849688	94654.598045	35.026880
1165.951282	94790.506066	35.031898
1166.905129	94926.792642	35.036916
1168.505277	95052.337419	35.041933
1169.455247	95189.562410	35.046951
1170.755983	95320.564816	35.051968
1171.758776	95463.457311	35.056986
1173.846620	95585.872142	35.062004
1175.263135	95701.701591	35.067021
1176.432777	95838.332600	35.072039
1177.371595	95942.257927	35.077056
1179.186796	96066.262259	35.082074
1180.375374	96179.846723	35.087092
1181.615242	96302.659654	35.092109
1182.938757	96425.415668	35.097127
1184.049394	96537.312600	35.102144
1185.251792	96664.175848	35.107162
1185.932705	96782.696228	35.112180
1187.132418	96912.414405	35.117197
1187.955597	97040.788763	35.122215
1189.025350	97169.371364	35.127232
1189.842380	97308.945775	35.132250
1190.762423	97452.028456	35.137268
1192.334212	97583.121057	35.142285
1193.260458	97733.600105	35.147303
1194.312533	97881.586473	35.152320
1195.162477	98027.233486	35.157338
1196.090531	98188.046482	35.162356
1197.599800	98340.695412	35.167373
1198.436170	98500.114338	35.172391
1199.155585	98662.874494	35.177408
1201.121127	98818.516188	35.182426
1201.982427	98986.152987	35.187444
1203.282119	99145.958254	35.192461
1204.461818	99318.057888	35.197479
1205.516616	99476.974336	35.202496
1206.983866	99640.679096	35.207514
1208.002752	99805.601500	35.212532
1209.611132	99966.666741	35.217549
1210.273190	100130.737099	35.222567
1211.501655	100302.336467	35.227584
1213.242157	100448.977104	35.232602
1214.441610	100625.455427	35.237620
1215.998629	100780.624838	35.242637
1216.713227	100945.262055	35.247655
1218.057458	101092.475949	35.252672
1219.616529	101263.238929	35.257690
1220.321566	101433.702350	35.262708
1222.067841	101590.416283	35.267725
1223.095831	101733.666535	35.272743
1224.043846	101897.488740	35.277760
1225.312317	102039.740836	35.282778
1226.781442	102191.649569	35.287796
1228.179651	102344.203335	35.292813
1229.082842	102482.833465	35.297831
1230.246420	102632.540952	35.302848
1231.592545	102782.701285	35.307866
1232.632290	102935.594309	35.312884
1233.654036	103090.927437	35.317901
1235.001398	103257.283756	35.322919
1236.241424	103408.021806	35.327936
1237.252716	103556.879787	35.332954
1238.628733	103731.436040	35.337972
1239.605532	103892.211088	35.342989
1240.883293	104048.585592	35.348007
1242.163598	104216.655275	35.353024
1243.018252	104387.369424	35.358042
1244.253006	104561.751745	35.363060
1245.823902	104726.285607	35.368077
1247.222699	104895.050026	35.373095
1248.355199	105075.337782	35.378112
1249.745098	105239.612858	35.383130
1250.747539	105419.449253	35.388148
1252.055799	105593.156610	35.393165
1253.085167	105765.150207	35.398183
1254.577639	105951.146396	35.403200
1256.021334	106124.722161	35.408218
1257.073411	106305.848380	35.413236
1258.414891	106482.132708	35.418253
1259.742812	106662.831705	35.423271
1260.836839	106847.543801	35.428288
1262.264144	107025.565245	35.433306
1263.190068	107215.882702	35.438324
1264.789983	107397.081926	35.443341
1266.159373	107577.186246	35.448359
1267.443303	107759.432088	35.453376
1268.569362	107942.938591	35.458394
1269.794372	108142.424772	35.463412
1270.881555	108311.553850	35.468429
1271.942269	108502.163779	35.473447
1273.135484	108695.823894	35.478464
1275.344604	108878.108268	35.483482
1276.359877	109057.476011	35.488500
1277.954529	109238.215091	35.493517
1279.463940	109417.652503	35.498535
1280.817411	109607.838419	35.503552
1282.326678	109767.042584	35.508570
1283.480509	109936.026732	35.513588
1284.942087	110109.748421	35.518605
1286.482810	110276.673203	35.523623
1288.065105	110456.448437	35.528640
1288.896844	110607.714182	35.533658
1290.334380	110789.375843	35.538676
1291.942852	110950.072091	35.543693
1292.919284	111112.692902	35.548711
1293.708844	111271.369208	35.553728
1295.289084	111410.278547	35.558746
1296.196564	111574.255328	35.563764
1297.597372	111732.153764	35.568781
1299.069629	111883.116589	35.573799
1300.201323	112046.111312	35.578816
1301.677811	112200.031620	35.583834
1302.605427	112362.782323	35.588852
1304.203943	112516.431975	35.593869
1305.893357	112678.436938	35.598887
1306.957834	112833.990266	35.603904
1308.557668	112994.428903	35.608922
1309.389304	113161.606093	35.613940
1310.382701	113323.599261	35.618957
1311.487685	113498.635812	35.623975
1312.498695	113670.016733	35.628992
1313.925057	113841.687320	35.634010
1315.068359	114024.596847	35.639028
1316.733262	114193.509691	35.644045
1318.209682	114383.883536	35.649063
1319.279074	114565.719829	35.654080
1321.155129	114737.375682	35.659098
1322.552171	114914.464848	35.664116
1323.954252	115077.727499	35.669133
1325.445817	115257.095865	35.674151
1326.536198	115428.362136	35.679168
1327.827723	115596.349709	35.684186
1328.952226	115775.621799	35.689204
1330.521137	115945.428957	35.694221
1331.931596	116134.053672	35.699239
1332.976558	116317.660149	35.704256
1334.961870	116491.925326	35.709274
1335.844105	116661.048633	35.714292
1336.960654	116841.298170	35.719309
1338.219570	117029.022843	35.724327
1339.433694	117224.334874	35.729344
1340.933142	117409.453485	35.734362
1341.706751	117601.495310	35.739380
1342.732817	117800.811543	35.744397
1344.459600	118003.975280	35.749415
1345.560876	118202.516516	35.754432
1346.809799	118404.898229	35.759450
1347.971664	118613.006725	35.764468
1349.035059	118831.694221	35.769485
1350.602881	119035.872764	35.774503
1351.735141	119246.618814	35.779520
1353.214607	119446.705123	35.784538
1354.881482	119669.368940	35.789556
1356.339577	119862.103875	35.794573
1358.049812	120067.008720	35.799591
1359.835801	120272.814980	35.804608
1362.005026	120448.242704	35.809626
1363.950296	120621.085593	35.814644
1365.580909	120789.483612	35.819661
1367.346227	120940.966307	35.824679
1368.773299	121102.584961	35.829696
1370.280879	121230.540757	35.834714
1372.725617	121362.489724	35.839732
1374.098630	121485.478093	35.844749
1375.234882	121610.923722	35.849767
1376.381247	121750.908095	35.854784
1377.434911	121870.314069	35.859802
1378.510662	122013.477391	35.864820
1379.242544	122165.283339	35.869837
1380.487261	122305.546316	35.874855
1381.113930	122465.679309	35.879872
1382.280525	122622.978997	35.884890
1383.209562	122796.972882	35.889908
1384.337478	122982.436912	35.894925
1385.842810	123162.585872	35.899943
1386.669858	123355.585894	35.904960
1388.156668	123553.270258	35.909978
1389.342906	123736.880989	35.914996
1390.458745	123934.513122	35.920013
1391.677216	124138.349611	35.925031
1392.917415	124343.488843	35.930048
1394.652869	124562.572880	35.935066
1395.390332	124778.219946	35.940084
1397.253712	124996.945174	35.945101
1399.115050	125196.418767	35.950119
1400.150975	125418.255623	35.955136
1401.798862	125619.666304	35.960154
1403.407103	125835.778749	35.965172
1404.494464	126033.228058	35.970189
1406.308312	126246.980306	35.975207
1407.868235	126469.844520	35.980224
1409.271050	126669.553787	35.985242
1410.233530	126886.499222	35.990260
1411.893803	127111.024843	35.995277
1413.308927	127315.791315	36.000295
1414.458849	127541.123620	36.005312
1415.810075	127760.649120	36.010330
1417.361400	127977.446239	36.015348
1418.533118	128208.379875	36.020365
1420.337940	128434.261479	36.025383
1421.349126	128647.843226	36.030400
1422.821665	128867.801625	36.035418
1424.495708	129096.610513	36.040436
1425.977618	129328.555675	36.045453
1427.957673	129531.082385	36.050471
1429.487149	129759.450936	36.055488
1431.104693	129966.383880	36.060506
1432.717693	130174.015882	36.065524
1433.877204	130394.441461	36.070541
1435.556487	130599.367515	36.075559
1437.100452	130815.883810	36.080576
1438.515692	131004.131040	36.085594
1440.545034	131214.403185	36.090612
1442.119420	131406.073959	36.095629
1444.134071	131593.900461	36.100647
1445.182797	131780.779411	36.105664
1446.675653	131948.001193	36.110682
1448.145902	132112.794898	36.115700
1449.480037	132278.536107	36.120717
1451.005383	132456.335292	36.125735
1452.080840	132635.157345	36.130752
1453.675248	132809.159336	36.135770
1455.162559	132992.403500	36.140788
1456.089795	133172.494171	36.145805
1458.011509	133353.390924	36.150823
1459.241987	133540.087798	36.155840
1460.607389	133727.081217	36.160858
1462.022557	133905.895233	36.165876
1462.988038	134114.609230	36.170893
1464.513150	134309.196297	36.175911
1465.752485	134514.309106	36.180928
1467.692040	134702.003227	36.185946
1469.148024	134910.569004	36.190964
1470.118675	135102.829284	36.195981
1471.392563	135299.857814	36.200999
1473.225542	135514.754452	36.206016
1474.682566	135719.980575	36.211034
1475.948920	135927.253244	36.216052
1477.906643	136120.643251	36.221069
1479.965944	136318.238146	36.226087
1481.287193	136514.608407	36.231104
1482.673077	136719.485355	36.236122
1484.299733	136924.883051	36.241140
1485.781653	137134.284269	36.246157
1487.753406	137320.963655	36.251175
1489.382836	137516.037070	36.256192
1490.993277	137697.593219	36.261210
1492.774812	137887.563244	36.266228
1494.220301	138085.102771	36.271245
1495.822215	138265.358469	36.276263
1497.387508	138454.454041	36.281280
1498.390486	138646.009987	36.286298
1499.891639	138852.049288	36.291316
1500.775363	139049.431002	36.296333
1502.574060	139237.886149	36.301351
1503.795627	139445.621468	36.306368
1505.068639	139649.497358	36.311386
1506.788452	139857.980138	36.316404
1508.499647	140063.373397	36.321421
1510.003620	140276.531872	36.326439
1511.072594	140489.013214	36.331456
1512.287273	140706.073481	36.336474
1513.512636	140916.923409	36.341492
1514.857644	141150.682988	36.346509
1516.276886	141369.717989	36.351527
1517.729236	141597.126917	36.356544
1519.393844	141833.502535	36.361562
1520.794960	142054.560539	36.366580
1521.902350	142284.310765	36.371597
1523.465271	142516.728043	36.376615
1524.496176	142748.483795	36.381632
1525.884782	142977.383352	36.386650
1527.499895	143198.035346	36.391668
1528.546773	143434.280597	36.396685
1530.213826	143657.842852	36.401703
1531.412161	143891.253679	36.406720
1532.785837	144144.766611	36.411738
1534.553227	144382.615772	36.416756
1535.844743	144636.779527	36.421773
1537.373380	144887.802183	36.426791
1538.804393	145146.067454	36.431808
1540.127026	145401.094413	36.436826
1541.625140	145659.226490	36.441844
1542.866580	145927.123886	36.446861
1544.732144	146194.518776	36.451879
1546.390500	146463.977027	36.456896
1547.678983	146728.539917	36.461914
1549.489277	146995.113716	36.466932
1551.227210	147270.498702	36.471949
1552.662600	147539.202873	36.476967
1554.315139	147808.926973	36.481984
1555.851035	148084.186270	36.487002
1557.627021	148344.400364	36.492020
1560.036524	148597.480206	36.497037
1562.565536	148860.722750	36.502055
1564.229209	149103.821414	36.507072
1565.559611	149354.365696	36.512090
1567.561598	149592.444798	36.517108
1569.204330	149839.355518	36.522125
1570.878340	150071.912150	36.527143
1572.676968	150317.457912	36.532160
1573.982971	150572.110327	36.537178
1576.024851	150797.907168	36.542196
1577.600972	151034.441683	36.547213
1579.337113	151270.813026	36.552231
1580.821834	151513.869332	36.557248
1582.132038	151756.688907	36.562266
1583.808842	151982.171521	36.567284
1585.075251	152235.347051	36.572301
1586.729784	152465.362675	36.577319
1588.296768	152706.614327	36.582336
1589.928915	152950.684716	36.587354
1591.898760	153176.407819	36.592372
1593.174266	153437.109534	36.597389
1594.864739	153666.405036	36.602407
1596.494218	153910.292664	36.607424
1598.102880	154150.876119	36.612442
1599.991600	154383.860004	36.617460
1601.627378	154616.441900	36.622477
1603.810314	154839.124654	36.627495
1605.487663	155074.200928	36.632512
1606.885085	155299.902389	36.637530
1608.630717	155523.774894	36.642548
1610.510350	155749.592940	36.647565
1612.526917	155951.742928	36.652583
1614.429635	156144.541781	36.657600
1615.900425	156333.365426	36.662618
1617.268600	156520.710169	36.667636
1618.898022	156710.943535	36.672653
1620.345626	156894.486360	36.677671
1621.987426	157092.188463	36.682688
1623.163280	157303.774525	36.687706
1624.598888	157491.240634	36.692724
1625.275089	157718.556138	36.697741
1626.765315	157936.068611	36.702759
1628.701410	158152.763474	36.707776
1629.623169	158392.458676	36.712794
1631.193967	158630.644874	36.717812
1632.956395	158862.614003	36.722829
1634.314158	159090.324739	36.727847
1635.961772	159336.200852	36.732864
1636.962239	159592.554605	36.737882
1638.770158	159841.084491	36.742900
1639.964766	160094.291473	36.747917
1641.882755	160361.791425	36.752935
1643.364451	160623.072668	36.757952
1645.063222	160900.667898	36.762970
1646.776427	161158.923446	36.767988
1648.260416	161440.500975	36.773005
1649.762552	161707.075185	36.778023
1651.047950	161981.789560	36.783040
1652.845981	162271.795266	36.788058
1654.292268	162557.027255	36.793076
1656.257613	162832.261530	36.798093
1658.341227	163114.670002	36.803111
1660.474230	163376.514574	36.808128
1662.168673	163652.939494	36.813146
1664.228093	163914.203524	36.818164
1665.776231	164190.528905	36.823181
1667.821423	164448.514170	36.828199
1669.793528	164711.345034	36.833216
1671.116996	164986.050593	36.838234
1672.810826	165235.586860	36.843252
1674.780314	165511.855204	36.848269
1676.164560	165773.708878	36.853287
1677.973775	166047.964641	36.858304
1679.073271	166324.364470	36.863322
1681.212643	166587.080543	36.868340
1682.522666	166862.410846	36.873357
1684.097934	167149.103708	36.878375
1686.001098	167418.940609	36.883392
1686.890730	167709.272689	36.888410
1689.013897	168003.609511	36.893428
1690.229056	168287.552298	36.898445
1691.377748	168577.482008	36.903463
1693.288235	168878.163385	36.908480
1694.879598	169184.948250	36.913498
1696.818387	169482.103586	36.918516
1698.705990	169777.696445	36.923533
1700.276556	170066.860021	36.928551
1702.278874	170340.824242	36.933568
1703.683901	170617.193879	36.938586
1705.720238	170889.570941	36.943604
1707.290958	171164.928709	36.948621
1708.893286	171442.921895	36.953639
1710.449473	171716.674818	36.958656
1711.810619	171999.835055	36.963674
1713.421890	172286.192377	36.968692
1715.182041	172580.164795	36.973709
1716.375402	172870.131931	36.978727
1718.400600	173165.322447	36.983744
1719.985626	173463.528131	36.988762
1722.190472	173749.712890	36.993780
1723.679752	174055.904893	36.998797
1725.537356	174346.474934	37.003815
1727.437900	174651.832292	37.008832
1729.237135	174954.239446	37.013850
1731.135146	175245.443807	37.018868
1733.052224	175548.331415	37.023885
1734.856175	175846.215356	37.028903
1737.033563	176119.544316	37.033920
1738.356198	176420.376001	37.038938
1740.226346	176713.485491	37.043956
1742.435837	177011.897034	37.048973
1744.277805	177300.409799	37.053991
1746.119930	177599.327917	37.059008
1747.957357	177883.582572	37.064026
1750.152113	178168.987703	37.069044
1752.140708	178447.538289	37.074061
1753.933216	178720.793137	37.079079
1755.875786	179003.693779	37.084096
1757.361433	179286.732285	37.089114
1759.106262	179566.242417	37.094132
1760.814036	179850.797286	37.099149
1762.559483	180129.448227	37.104167
1764.482786	180407.451029	37.109184
1766.445106	180692.491254	37.114202
1768.559889	180961.116180	37.119220
1770.266348	181242.254656	37.124237
1771.980481	181513.674554	37.129255
1774.509853	181782.340234	37.134272
1775.945209	182055.863259	37.139290
1777.797251	182314.920443	37.144308
1779.545102	182594.043562	37.149325
1781.391091	182874.206018	37.154343
1783.281183	183129.379222	37.159360
1785.277619	183413.086715	37.164378
1786.482479	183679.880569	37.169396
1787.934362	183951.039849	37.174413
1789.636688	184235.116470	37.179431
1791.679213	184502.175588	37.184448
1793.345480	184785.449302	37.189466
1794.938466	185070.005344	37.194484
1796.781400	185348.293040	37.199501
1798.262995	185625.155140	37.204519
1799.987581	185894.442804	37.209536
1801.366487	186161.642395	37.214554
1803.205872	186426.118310	37.219572
1804.814066	186694.071345	37.224589
1806.180811	186978.535561	37.229607
1808.443677	187242.809332	37.234624
1809.911985	187532.539782	37.239642
1811.375319	187822.970767	37.244660
1813.365189	188089.259613	37.249677
1814.821230	188380.824621	37.254695
1817.059275	188672.343433	37.259712
1818.876238	188970.529837	37.264730
1820.801367	189247.749144	37.269748
1822.839210	189541.411675	37.274765
1824.229974	189833.478197	37.279783
1826.677283	190117.041058	37.284800
1828.257251	190422.000150	37.289818
1830.337197	190703.226236	37.294836
1832.287191	191008.561772	37.299853
1834.089643	191318.478680	37.304871
1835.620523	191608.109700	37.309888
1837.229855	191915.560919	37.314906
1839.169435	192214.382426	37.319924
1841.019174	192533.932073	37.324941
1842.468424	192848.166237	37.329959
1844.289576	193150.578442	37.334976
1845.801393	193484.897143	37.339994
1847.315347	193789.176845	37.345012
1849.518235	194129.253630	37.350029
1851.238396	194451.298256	37.355047
1853.414253	194781.890318	37.360064
1855.162458	195123.315112	37.365082
1856.394437	195451.231034	37.370100
1858.273237	195785.202017	37.375117
1860.130180	196143.598271	37.380135
1862.299595	196474.836847	37.385152
1864.205211	196818.875149	37.390170
1866.034392	197153.319721	37.395188
1868.298384	197493.713629	37.400205
1869.948101	197856.127242	37.405223
1871.610855	198189.462464	37.410240
1873.479447	198542.390014	37.415258
1875.815435	198877.526583	37.420276
1878.286237	199220.691120	37.425293
1879.719431	199554.972457	37.430311
1882.055297	199896.093746	37.435328
1884.089646	200244.690490	37.440346
1885.651043	200568.980924	37.445364
1887.717380	200903.538128	37.450381
1889.765383	201250.323947	37.455399
1891.606688	201569.498497	37.460416
1893.605433	201915.483904	37.465434
1895.325446	202251.221209	37.470452
1897.358657	202574.420275	37.475469
1898.876209	202919.840853	37.480487
1901.049114	203221.886423	37.485504
1903.014984	203539.884533	37.490522
1904.984536	203851.105273	37.495540
1907.131709	204146.101988	37.500557
1908.773466	204470.224403	37.505575
1910.924169	204764.969832	37.510592
1912.421170	205074.368027	37.515610
1914.958264	205360.054964	37.520628
1917.144194	205674.640493	37.525645
1919.154368	205973.362230	37.530663
1921.519191	206274.885439	37.535680
1923.473154	206569.594958	37.540698
1925.471888	206864.578105	37.545716
1927.400128	207151.525495	37.550733
1929.306315	207460.693453	37.555751
1931.201759	207751.216102	37.560768
1932.944572	208053.862515	37.565786
1934.765800	208356.383728	37.570804
1936.677818	208658.143021	37.575821
1938.166059	208978.188368	37.580839
1940.016563	209293.925029	37.585856
1941.945693	209613.598998	37.590874
1943.063040	209938.659233	37.595892
1945.176946	210260.097194	37.600909
1946.777399	210609.509908	37.605927
1948.459020	210947.765098	37.610944
1950.190930	211298.544522	37.615962
1952.317975	211652.729039	37.620980
1954.046599	211996.707973	37.625997
1955.828248	212374.679333	37.631015
1957.623092	212720.835233	37.636032
1959.758954	213086.845878	37.641050
1961.739985	213466.404237	37.646068
1963.667698	213817.496184	37.651085
1966.028713	214196.680998	37.656103
1967.870289	214556.588823	37.661120
1969.839304	214927.079632	37.666138
1971.483266	215297.916044	37.671156
1973.933225	215675.622227	37.676173
1975.373710	216051.890912	37.681191
1977.405322	216430.175443	37.686208
1979.653680	216808.059428	37.691226
1981.715254	217184.159467	37.696244
1984.052381	217563.226882	37.701261
1985.867860	217933.123182	37.706279
1987.791436	218312.323665	37.711296
1989.845275	218689.740605	37.716314
1991.688088	219070.836997	37.721332
1994.124804	219447.371802	37.726349
1996.204795	219824.066704	37.731367
1998.231986	220188.354131	37.736384
2000.299993	220558.325183	37.741402
2002.158734	220974.269820	37.746420
2004.057109	221368.320304	37.751437
2006.026384	221742.464807	37.756455
2008.191611	222091.553428	37.761472
2010.200100	222435.754568	37.766490
2012.304641	222797.553458	37.771508
2014.417749	223143.302906	37.776525
2015.821042	223491.109222	37.781543
2017.931605	223858.930691	37.786560
2019.490912	224212.238889	37.791578
2021.489184	224574.710294	37.796596
2023.192833	224949.343823	37.801613
2025.093474	225327.363551	37.806631
2027.037207	225704.502010	37.811648
2028.937107	226084.988716	37.816666
2030.965262	226477.418410	37.821684
2033.331199	226852.425252	37.826701
2034.883728	227255.067127	37.831719
2037.282419	227643.684728	37.836736
2039.195210	228029.892286	37.841754
2040.726138	228432.263687	37.846772
2042.988580	228822.508140	37.851789
2045.286837	229241.675811	37.856807
2047.301179	229638.591807	37.861824
2049.520603	230040.454865	37.866842
2051.314027	230452.825581	37.871860
2054.035102	230846.002883	37.876877
2055.818213	231269.731532	37.881895
2057.846550	231675.721005	37.886912
2060.160603	232070.771240	37.891930
2062.128337	232487.440854	37.896948
2064.339512	232883.475867	37.901965
2066.845415	233296.203081	37.906983
2069.272003	233697.286829	37.912000
2071.834263	234092.915435	37.917018
2073.531632	234491.324235	37.922036
2076.122665	234890.380186	37.927053
2077.866909	235294.753335	37.932071
2079.713965	235687.174364	37.937088
2082.085260	236087.412728	37.942106
2083.971477	236496.873157	37.947124
2085.981230	236891.126964	37.952141
2088.603975	237293.184086	37.957159
2090.917808	237689.475282	37.962176
2093.320355	238070.209483	37.967194
2095.350416	238461.443203	37.972212
2097.781382	238853.021080	37.977229
2099.730945	239242.543106	37.982247
2102.028759	239639.046901	37.987264
2104.024820	240016.372345	37.992282
2105.587735	240404.130811	37.997300
2108.292516	240786.959643	38.002317
2110.329225	241184.145027	38.007335
2112.708587	241565.580145	38.012352
2115.281278	241946.807979	38.017370
2117.054206	242321.127989	38.022388
2119.066894	242696.782694	38.027405
2121.126123	243074.513948	38.032423
2123.294478	243437.039566	38.037440
2125.647033	243781.934457	38.042458
2127.673694	244133.511478	38.047476
2129.382676	244478.053047	38.052493
2131.598621	244836.866455	38.057511
2133.493996	245189.889485	38.062528
2135.637704	245545.693515	38.067546
2137.172658	245918.308763	38.072564
2139.215602	246297.423254	38.077581
2141.026459	246662.986031	38.082599
2143.221034	247043.246873	38.087616
2146.026967	247415.435781	38.092634
2148.016757	247790.879405	38.097652
2150.014202	248170.412343	38.102669
2152.098590	248553.996636	38.107687
2153.876674	248943.244153	38.112704
2156.574696	249331.686285	38.117722
2157.906751	249736.298132	38.122740
2160.004230	250125.904274	38.127757
2162.188734	250535.717209	38.132775
2164.422456	250936.073910	38.137792
2168.009896	251300.324212	38.142810
2170.171905	251694.394416	38.147828
2172.545799	252078.398166	38.152845
2174.788920	252476.064288	38.157863
2176.809171	252854.257924	38.162880
2178.964868	253244.369782	38.167898
2180.910424	253638.249866	38.172916
2183.444317	254031.656415	38.177933
2185.275431	254431.373324	38.182951
2187.477009	254826.028042	38.187968
2189.795539	255221.858877	38.192986
2191.411943	255634.211688	38.198004
2193.423947	256029.711608	38.203021
2195.909635	256441.496260	38.208039
2197.685024	256861.497689	38.213056
2200.249900	257264.812273	38.218074
2202.343383	257699.777642	38.223092
2204.730089	258117.271136	38.228109
2207.144559	258530.315479	38.233127
2208.674996	258951.273898	38.238144
2211.132149	259366.726073	38.243162
2213.285243	259803.031951	38.248180
2215.226228	260222.225288	38.253197
2217.343085	260659.732186	38.258215
2219.093594	261099.787313	38.263232
2221.876473	261530.204102	38.268250
2224.318507	261965.222660	38.273268
2226.256096	262401.109291	38.278285
2228.661600	262834.661430	38.283303
2230.621375	263282.104034	38.288320
2232.803332	263716.531009	38.293338
2235.006659	264168.711852	38.298356
2237.441447	264598.222354	38.303373
2240.145130	265021.593924	38.308391
2242.691097	265426.141788	38.313408
2245.628406	265809.924385	38.318426
2247.685497	266201.112187	38.323444
2250.025466	266583.135699	38.328461
2252.307015	266972.992961	38.333479
2254.280895	267368.996076	38.338496
2256.760356	267762.709222	38.343514
2258.485967	268161.902255	38.348532
2260.308728	268562.299496	38.353549
2262.574282	268974.185279	38.358567
2264.394029	269385.506902	38.363584
2266.857349	269805.871906	38.368602
2268.678593	270226.923203	38.373620
2271.000847	270658.945721	38.378637
2272.885870	271086.134895	38.383655
2274.728872	271534.466510	38.388672
2277.016893	271972.210716	38.393690
2278.977982	272428.297334	38.398708
2281.301721	272889.686687	38.403725
2283.281943	273338.809943	38.408743
2285.061895	273817.814030	38.413760
2287.580930	274284.024681	38.418778
2289.902451	274765.940576	38.423796
2292.255623	275253.821252	38.428813
2294.640166	275724.295582	38.433831
2296.749040	276216.787511	38.438848
2299.206730	276705.565956	38.443866
2302.105744	277190.768647	38.448884
2304.751307	277669.965370	38.453901
2307.312113	278152.426995	38.458919
2309.836076	278630.677305	38.463936
2312.422203	279093.726333	38.468954
2314.844867	279566.555927	38.473972
2317.360295	280041.072571	38.478989
2319.940042	280496.500837	38.484007
2322.464825	280965.147235	38.489024
2325.130918	281431.459195	38.494042
2327.023951	281893.574796	38.499060
2329.262971	282360.131543	38.504077
2331.735520	282837.447223	38.509095
2333.682564	283309.968344	38.514112
2335.969520	283780.504468	38.519130
2338.133704	284261.119200	38.524148
2340.429138	284743.998864	38.529165
2342.951685	285225.470184	38.534183
2344.913066	285716.022537	38.539200
2347.144799	286202.289083	38.544218
2349.129191	286695.046523	38.549236
2351.610455	287184.853953	38.554253
2354.814111	287660.193504	38.559271
2357.278931	288154.422163	38.564288
2359.386964	288629.883092	38.569306
2361.645679	289112.025694	38.574324
2364.231177	289606.563007	38.579341
2366.848694	290080.238756	38.584359
2369.133319	290537.124482	38.589376
2371.740485	290989.055572	38.594394
2374.015265	291432.808110	38.599412
2376.336771	291878.508426	38.604429
2378.802230	292314.811586	38.609447
2381.014892	292773.939944	38.614464
2383.054675	293226.896598	38.619482
2384.981322	293694.679788	38.624500
2387.398662	294150.902372	38.629517
2389.750333	294603.933698	38.634535
2391.677330	295084.516429	38.639552
2394.079429	295564.667072	38.644570
2396.556392	296037.361885	38.649588
2399.160943	296526.749778	38.654605
2401.684310	297008.884324	38.659623
2404.099294	297496.140538	38.664640
2406.805809	297964.145515	38.669658
2409.544341	298445.149818	38.674676
2411.418466	298936.780631	38.679693
2414.236410	299418.582445	38.684711
2416.276521	299915.797796	38.689728
2419.175527	300405.940922	38.694746
2421.415139	300906.245946	38.699764
2423.224190	301397.117556	38.704781
2426.203468	301888.741963	38.709799
2428.101772	302398.062787	38.714816
2430.186305	302911.086271	38.719834
2432.709474	303420.228292	38.724852
2434.758881	303950.246785	38.729869
2437.424170	304480.521266	38.734887
2439.501673	305010.099431	38.739904
2442.253828	305531.161043	38.744922
2444.941366	306056.193299	38.749940
2447.812445	306576.546105	38.754957
2451.076041	307088.427142	38.759975
2453.904204	307594.406096	38.764992
2456.688815	308095.005102	38.770010
2459.722169	308593.098854	38.775028
2461.752913	309092.568618	38.780045
2464.739383	309581.013786	38.785063
2467.589213	310072.831304	38.790080
2470.185865	310560.876935	38.795098
2472.257408	311050.222853	38.800116
2474.570891	311541.103046	38.805133
2477.186531	312038.232152	38.810151
2479.506472	312537.031386	38.815168
2481.672620	313030.645923	38.820186
2484.644538	313518.060192	38.825204
2487.356931	314006.884850	38.830221
2490.179651	314497.950188	38.835239
2492.269816	314986.589419	38.840256
2494.747909	315472.599600	38.845274
2497.329263	315962.146793	38.850292
2499.734909	316458.373675	38.855309
2502.239215	316935.635605	38.860327
2504.218430	317402.057356	38.865344
2506.515814	317861.213493	38.870362
2509.349865	318323.253868	38.875380
2511.719691	318781.301942	38.880397
2514.192475	319238.340942	38.885415
2516.421268	319712.026028	38.890432
2518.505361	320180.474394	38.895450
2521.296166	320648.249605	38.900468
2523.673178	321122.741852	38.905485
2526.713014	321589.101200	38.910503
2528.957216	322065.514116	38.915520
2531.173896	322536.646330	38.920538
2533.791550	323026.962685	38.925556
2535.542896	323520.791118	38.930573
2538.112694	324012.252122	38.935591
2540.362087	324523.163275	38.940608
2542.700457	325039.847320	38.945626
2545.048192	325553.707702	38.950644
2547.686753	326078.057720	38.955661
2549.982326	326603.347442	38.960679
2552.632320	327140.030577	38.965696
2554.990610	327673.962812	38.970714
2557.968333	328209.900948	38.975732
2560.375231	328751.283953	38.980749
2563.248268	329284.793224	38.985767
2565.670287	329832.920874	38.990784
2568.307117	330375.652348	38.995802
2571.013637	330912.020366	39.000820
2573.505552	331469.317171	39.005837
2576.206400	332020.736120	39.010855
2579.475929	332557.104234	39.015872
2582.072157	333093.422577	39.020890
2585.122015	333643.453116	39.025908
2587.338314	334195.845865	39.030925
2589.990270	334737.728958	39.035943
2592.459866	335294.313182	39.040960
2594.906818	335833.198326	39.045978
2597.529085	336396.478028	39.050996
2599.872020	336960.076485	39.056013
2602.396295	337509.447727	39.061031
2604.894384	338071.590095	39.066048
2606.941419	338648.804899	39.071066
2609.690306	339229.026320	39.076084
2612.030850	339804.787642	39.081101
2614.433590	340387.439893	39.086119
2616.863402	340987.525134	39.091136
2619.511012	341577.185721	39.096154
2622.098951	342170.099879	39.101172
2624.887372	342774.452284	39.106189
2627.673633	343362.093149	39.111207
2630.467838	343947.213479	39.116224
2633.165727	344551.562138	39.121242
2635.924586	345143.353228	39.126260
2639.645964	345710.105852	39.131277
2642.939758	346269.456695	39.136295
2645.976601	346803.277815	39.141312
2648.420354	347337.416319	39.146330
2650.793824	347862.599352	39.151348
2653.073343	348398.987764	39.156365
2655.840174	348926.662460	39.161383
2658.115879	349466.468230	39.166400
2660.265359	350001.693827	39.171418
2663.101517	350557.697635	39.176436
2665.562888	351104.616368	39.181453
2667.950868	351659.207379	39.186471
2670.245065	352220.965924	39.191488
2672.678548	352784.625622	39.196506
2675.487379	353341.670671	39.201524
2677.935788	353936.258799	39.206541
2680.568065	354504.158176	39.211559
2683.322176	355088.505700	39.216576
2685.715344	355689.174154	39.221594
2688.324473	356279.851220	39.226612
2691.142017	356892.088702	39.231629
2693.942900	357485.081653	39.236647
2696.091287	358105.887681	39.241664
2698.760806	358717.846694	39.246682
2701.916029	359318.781801	39.251700
2705.000798	359926.725666	39.256717
2708.023072	360545.940626	39.261735
2711.019531	361144.086077	39.266752
2713.573144	361760.694438	39.271770
2716.702274	362362.813365	39.276788
2719.820400	362971.677087	39.281805
2722.679496	363555.398005	39.286823
2725.260071	364169.863580	39.291840
2727.847843	364779.167958	39.296858
2731.043498	365377.176249	39.301876
2733.546172	365998.760473	39.306893
2736.042404	366600.035370	39.311911
2739.170284	367206.201307	39.316928
2741.710314	367814.177585	39.321946
2744.672890	368435.426306	39.326964
2747.139729	369048.928933	39.331981
2750.075918	369663.871037	39.336999
2753.010971	370274.363883	39.342016
2755.513742	370890.245101	39.347034
2758.312876	371505.182332	39.352052
2760.723794	372127.200606	39.357069
2763.649068	372764.225393	39.362087
2766.620071	373381.086936	39.367104
2769.265070	374000.604266	39.372122
2772.031517	374617.809497	39.377140
2774.626265	375255.837551	39.382157
2777.535570	375877.364992	39.387175
2780.127367	376521.310449	39.392192
2782.832795	377164.745499	39.397210
2785.646344	377778.951773	39.402228
2788.198001	378423.659238	39.407245
2791.133659	379051.652919	39.412263
2794.258369	379649.747119	39.417280
2796.852568	380258.570955	39.422298
2799.980506	380843.200763	39.427316
2803.023700	381432.528143	39.432333
2805.820769	382006.436544	39.437351
2808.947444	382591.445627	39.442368
2811.682102	383175.264731	39.447386
2814.607873	383748.086216	39.452404
2817.403444	384339.132297	39.457421
2820.130142	384927.136001	39.462439
2823.305507	385505.572728	39.467456
2825.624606	386109.728960	39.472474
2828.294896	386700.503316	39.477492
2830.960895	387304.787719	39.482509
2833.856541	387903.851502	39.487527
2836.330607	388516.845644	39.492544
2838.783776	389140.205899	39.497562
2841.915818	389743.538428	39.502580
2844.395409	390389.292709	39.507597
2847.036016	391024.433990	39.512615
2850.090313	391656.607111	39.517632
2852.680244	392307.735709	39.522650
2855.580668	392949.419745	39.527668
2858.212002	393590.196110	39.532685
2861.173342	394247.949417	39.537703
2864.672425	394889.679791	39.542720
2867.237615	395541.689005	39.547738
2870.699224	396191.413655	39.552756
2873.766089	396841.314963	39.557773
2876.723697	397492.108354	39.562791
2880.005488	398135.459051	39.567808
2883.003593	398784.876687	39.572826
2885.689547	399427.485024	39.577844
2888.579688	400084.094736	39.582861
2891.428142	400734.790281	39.587879
2894.633844	401390.258652	39.592896
2897.220867	402044.163623	39.597914
2900.422550	402688.349349	39.602932
2903.048984	403345.010126	39.607949
2905.773521	404005.976804	39.612967
2908.869566	404670.293134	39.617984
2911.488157	405335.355380	39.623002
2914.641773	405996.338815	39.628020
2917.663766	406671.296357	39.633037
2920.451111	407336.390285	39.638055
2923.451051	407993.400786	39.643072
2926.372272	408672.284485	39.648090
2929.886461	409329.869088	39.653108
2932.184608	409992.320913	39.658125
2935.287930	410659.877270	39.663143
2938.710076	411314.492853	39.668160
2941.470234	411986.306472	39.673178
2944.632591	412649.728305	39.678196
2947.955423	413310.499401	39.683213
2950.887642	413950.992334	39.688231
2954.063743	414568.168226	39.693248
2956.579618	415194.710631	39.698266
2959.743635	415798.329634	39.703284
2962.423706	416406.599261	39.708301
2964.856734	417024.270986	39.713319
2967.960014	417651.021589	39.718336
2970.067036	418291.447152	39.723354
2972.695796	418920.550638	39.728372
2975.673445	419569.297836	39.733389
2978.100565	420222.779227	39.738407
2981.485285	420879.311539	39.743424
2984.158902	421554.132271	39.748442
2986.591080	422225.402416	39.753460
2989.369053	422904.683317	39.758477
2991.814791	423609.080933	39.763495
2995.028057	424300.013370	39.768512
2997.801024	425010.478975	39.773530
3001.118010	425716.355966	39.778548
3004.193062	426421.315421	39.783565
3007.472976	427134.532442	39.788583
3010.359149	427840.750823	39.793600
3013.250157	428569.341016	39.798618
3016.634538	429289.601095	39.803636
3020.233200	430002.639596	39.808653
3023.532947	430717.960077	39.813671
3026.578271	431436.112412	39.818688
3029.326703	432151.531241	39.823706
3032.703890	432863.867627	39.828724
3035.689284	433590.073521	39.833741
3038.592858	434316.955441	39.838759
3041.651461	435044.551728	39.843776
3044.590516	435783.389201	39.848794
3047.749430	436509.737189	39.853812
3050.776651	437259.430972	39.858829
3053.513875	437997.120959	39.863847
3056.549796	438740.160141	39.868864
3059.621768	439491.045409	39.873882
3063.058345	440242.558962	39.878900
3066.122857	441007.526428	39.883917
3068.831242	441755.462960	39.888935
3072.325376	442490.087968	39.893952
3075.138084	443265.352843	39.898970
3078.167789	444010.485300	39.903988
3081.549777	444777.510715	39.909005
3084.946648	445516.462885	39.914023
3088.032467	446278.373591	39.919040
3091.213677	447036.346742	39.924058
3094.307608	447788.741047	39.929076
3097.434426	448538.676267	39.934093
3100.379436	449305.927030	39.939111
3104.164497	450047.813192	39.944128
3107.135236	450805.950033	39.949146
3110.540844	451554.832338	39.954164
3113.760764	452291.623687	39.959181
3116.461666	453046.945426	39.964199
3119.474803	453763.377188	39.969216
3122.126890	454471.898326	39.974234
3125.205742	455184.124926	39.979252
3128.809534	455881.773654	39.984269
3132.313733	456590.599047	39.989287
3135.708771	457289.805324	39.994304
3138.593599	458001.011203	39.999322
3141.321568	458701.087929	40.004340
3144.480533	459421.868326	40.009357
3147.234713	460134.746026	40.014375
3150.377049	460855.127625	40.019392
3153.269889	461595.709803	40.024410
3156.097709	462322.112488	40.029428
3158.992353	463065.223927	40.034445
3161.907234	463833.244211	40.039463
3164.640660	464579.464804	40.044480
3167.645183	465354.952824	40.049498
3170.211085	466137.765123	40.054516
3173.634840	466929.364714	40.059533
3176.740276	467737.623817	40.064551
3180.118955	468524.062345	40.069568
3183.575503	469320.623561	40.074586
3186.928151	470110.242746	40.079604
3190.509669	470913.802528	40.084621
3194.197689	471687.278670	40.089639
3198.073932	472484.005301	40.094656
3201.242259	473276.767945	40.099674
3203.987909	474068.302568	40.104692
3207.696049	474842.818591	40.109709
3210.839267	475645.654415	40.114727
3214.281679	476423.387161	40.119744
3217.390565	477221.767202	40.124762
3220.518242	478014.501366	40.129780
3223.544465	478814.801945	40.134797
3226.467427	479625.397598	40.139815
3230.134233	480420.729975	40.144832
3233.196506	481244.984403	40.149850
3236.024407	482063.782965	40.154868
3239.606225	482864.740110	40.159885
3242.460796	483691.298959	40.164903
3246.264772	484507.212125	40.169920
3249.735003	485329.510204	40.174938
3253.442636	486138.497145	40.179956
3256.948640	486946.016406	40.184973
3259.968168	487751.607853	40.189991
3263.582046	488568.791958	40.195008
3266.663721	489379.507825	40.200026
3269.323328	490190.912153	40.205044
3272.364270	491005.554953	40.210061
3275.458645	491839.651507	40.215079
3278.756029	492660.545813	40.220096
3281.587818	493494.104283	40.225114
3284.878778	494336.037360	40.230132
3288.407185	495174.763033	40.235149
3291.173900	496010.136575	40.240167
3294.362525	496814.499831	40.245184
3297.140177	497617.125006	40.250202
3300.543636	498435.016317	40.255220
3303.864257	499221.477526	40.260237
3306.674988	500058.878534	40.265255
3310.091563	500863.630630	40.270272
3313.213001	501689.192855	40.275290
3316.396388	502524.500486	40.280308
3319.781584	503353.880989	40.285325
3322.625396	504201.076220	40.290343
3325.996767	505039.061518	40.295360
3329.143531	505903.893747	40.300378
3332.116420	506762.855906	40.305396
3335.350619	507631.777299	40.310413
3338.417291	508514.862210	40.315431
3341.458289	509410.471055	40.320448
3344.855952	510301.283898	40.325466
3348.175128	511204.828368	40.330484
3351.628662	512101.542626	40.335501
3354.517095	513029.730332	40.340519
3357.860017	513951.690741	40.345536
3361.105597	514882.746728	40.350554
3364.273818	515818.807481	40.355572
3367.579610	516752.019653	40.360589
3371.200309	517707.221342	40.365607
3374.551445	518666.092185	40.370624
3378.012749	519613.794716	40.375642
3381.303662	520583.103455	40.380660
3385.479675	521537.187764	40.385677
3388.454977	522495.137213	40.390695
3392.647752	523445.677885	40.395712
3396.364977	524409.245332	40.400730
3399.888834	525356.300151	40.405748
3403.193150	526314.474489	40.410765
3406.765393	527278.194586	40.415783
3410.212698	528230.282790	40.420800
3413.665372	529193.653275	40.425818
3416.765906	530152.434220	40.430836
3421.133155	531101.582735	40.435853
3424.052046	532067.834516	40.440871
3427.303145	533042.993565	40.445888
3431.068417	534009.041259	40.450906
3434.164042	534987.679822	40.455924
3437.338378	535960.550782	40.460941
3440.829073	536934.519048	40.465959
3444.362207	537910.030446	40.470976
3447.822898	538902.314428	40.475994
3451.002040	539877.654622	40.481012
3454.744062	540856.116478	40.486029
3458.068685	541844.400934	40.491047
3461.648487	542829.608789	40.496064
3465.280030	543822.497905	40.501082
3468.691314	544807.551200	40.506100
3471.977555	545801.872947	40.511117
3475.649285	546778.511094	40.516122
3479.122527	547703.951649	40.521127
3482.662847	548576.686877	40.526132
3485.595253	549388.304391	40.531136
3489.360360	550114.567184	40.536141
3492.594029	550784.464974	40.541146
3495.293858	551394.928037	40.546151
3498.070099	551943.546489	40.551156
3500.436255	552422.836294	40.556160
3503.034169	552835.780446	40.561165
3505.333981	553199.722351	40.566170
3507.479220	553498.297537	40.571175
3509.574651	553742.844386	40.576180
3511.431392	553919.270186	40.581184
3513.568253	554057.107968	40.586189
3514.524934	554141.556481	40.591194
3515.768784	554206.486729	40.596199
3516.801415	554221.810730	40.601204
3517.635419	554213.103100	40.606208
3518.734399	554159.910044	40.611213
3519.101750	554089.175968	40.616218
3520.115830	553985.346776	40.621223
3520.502880	553848.976190	40.626228
3521.031407	553723.781479	40.631232
3521.650910	553542.472170	40.636237
3522.308168	553355.907846	40.641242
3522.184457	553154.632137	40.646247
3522.678741	552937.515210	40.651252
3522.851053	552709.649192	40.656256
3522.890741	552462.578041	40.661261
3522.683923	552216.802948	40.666266
3523.134142	551963.503017	40.671271
3523.157475	551695.280849	40.676276
3523.489755	551426.500309	40.681280
3523.498194	551145.050706	40.686285
3523.488039	550873.084729	40.691290
3523.385114	550581.398728	40.696295
3523.380465	550287.471072	40.701300
3523.517198	549994.726193	40.706304
3523.279769	549680.032940	40.711309
3523.198418	549392.407106	40.716314
3523.233004	549081.795932	40.721319
3523.024023	548786.406769	40.726324
3522.431034	548480.827601	40.731328
3522.498260	548176.197522	40.736333
3522.499128	547874.549240	40.741338
3522.048947	547576.549381	40.746343
3522.100214	547281.845754	40.751348
3521.623016	546984.241898	40.756352
3521.746451	546677.754825	40.761357
3521.558448	546402.856713	40.766362
3521.449683	546103.561654	40.771367
3521.650175	545798.154550	40.776372
3520.933712	545501.669016	40.781376
3520.894784	545202.041784	40.786381
3520.684924	544933.025663	40.791386
3520.641353	544632.832379	40.796391
3520.387598	544345.437876	40.801396
3519.918841	544076.245205	40.806400
3519.788592	543785.438074	40.811405
3519.046930	543526.526557	40.816410
3518.965744	543253.875352	40.821415
3519.338022	542987.508654	40.826420
3518.753885	542726.538929	40.831424
3518.580146	542462.672503	40.836429
3518.716713	542204.709967	40.841434
3518.124057	541935.750677	40.846439
3517.983043	541684.386608	40.851444
3517.232650	541448.867698	40.856448
3517.421039	541198.857172	40.861453
3517.053099	540959.382302	40.866458
3516.548155	540725.731967	40.871463
3516.700168	540501.063053	40.876468
3516.178587	540273.619061	40.881472
3516.132616	540040.743972	40.886477
3516.127590	539825.330447	40.891482
3515.656211	539604.180432	40.896487
3515.491270	539402.066786	40.901492
3515.352911	539176.464609	40.906496
3515.607167	538971.400568	40.911501
3515.161229	538763.969939	40.916506
3514.695647	538557.802083	40.921511
3515.023884	538364.484697	40.926516
3514.269874	538157.296470	40.931520
3514.185047	537959.544578	40.936525
3514.050712	537774.726672	40.941530
3513.724211	537586.199640	40.946535
3513.903488	537393.701524	40.951540
3513.468982	537220.590780	40.956544
3513.578252	537042.947669	40.961549
3513.201038	536875.834085	40.966554
3513.080319	536690.344317	40.971559
3512.925493	536516.625823	40.976564
3512.608121	536357.982294	40.981568
3512.644156	536186.149171	40.986573
3512.697095	536030.827770	40.991578
3512.279315	535865.325839	40.996583
3512.236894	535703.096438	41.001588
3511.981954	535555.647883	41.006592
3512.115428	535385.356211	41.011597
3511.584480	535243.100371	41.016602
3511.378033	535101.044487	41.021607
3511.504101	534942.922391	41.026612
3511.037719	534801.662508	41.031616
3511.148792	534653.591823	41.036621
3511.050765	534519.241944	41.041626
3510.831449	534390.668657	41.046631
3510.774503	534253.935819	41.051636
3510.422950	534121.441065	41.056640
3510.448713	533983.227827	41.061645
3510.317716	533863.678434	41.066650
3510.305005	533745.119743	41.071655
3510.343589	533615.034278	41.076660
3510.041524	533500.358699	41.081664
3510.020628	533373.614721	41.086669
3509.832653	533260.586406	41.091674
3509.803120	533137.428616	41.096679
3509.777315	533021.291325	41.101684
3509.270145	532916.191823	41.106688
3509.511002	532801.728382	41.111693
3509.259415	532698.304663	41.116698
3509.137013	532589.807853	41.121703
3508.956994	532475.812691	41.126708
3509.185083	532381.960413	41.131712
3508.698211	532274.933586	41.136717
3508.596626	532179.869172	41.141722
3508.686986	532077.751354	41.146727
3508.698629	531994.186812	41.151732
3507.974321	531902.654607	41.156736
3508.351767	531797.862435	41.161741
3508.432676	531707.212268	41.166746
3507.984129	531631.751624	41.171751
3507.963727	531541.318597	41.176756
3507.822546	531451.459894	41.181760
3507.872029	531367.886018	41.186765
3507.833961	531299.785891	41.191770
3507.611601	531217.012032	41.196775
3508.009300	531142.021565	41.201780
3508.005964	531054.867121	41.206784
3507.897037	530956.360729	41.211789
3507.254051	530890.476482	41.216794
3507.160942	530820.260902	41.221799
3507.406746	530731.549514	41.226804
3507.418212	530674.857679	41.231808
3507.408608	530597.200572	41.236813
3506.921147	530530.987073	41.241818
3507.025823	530456.898590	41.246823
3507.202369	530377.796226	41.251828
3506.921730	530324.736709	41.256832
3507.269270	530251.316252	41.261837
3507.045096	530196.630500	41.266842
3506.757971	530122.046557	41.271847
3506.719159	530052.223179	41.276852
3506.395580	529996.137654	41.281856
3506.381929	529939.497660	41.286861
3506.583517	529886.107802	41.291866
3506.371620	529835.309551	41.296871
3506.270895	529767.768488	41.301876
3506.160898	529732.011422	41.306880
3506.345431	529662.656305	41.311885
3506.190613	529616.901257	41.316890
3506.083828	529554.110001	41.321895
3506.309003	529504.252195	41.326900
3506.130359	529461.026949	41.331904
3506.345239	529401.114982	41.336909
3506.398517	529344.411738	41.341914
3506.170157	529302.406642	41.346919
3506.208235	529241.814586	41.351924
3506.062637	529197.926497	41.356928
3505.994791	529142.959719	41.361933
3506.269696	529094.709749	41.366938
3505.851768	529052.683417	41.371943
3505.723635	529006.720253	41.376948
3505.839831	528952.229037	41.381952
3505.589819	528902.494963	41.386957
3505.553984	528875.668346	41.391962
3505.428933	528832.635034	41.396967
3505.665450	528779.842292	41.401972
3505.668275	528754.929581	41.406976
3505.991729	528697.726522	41.411981
3505.900659	528653.878834	41.416986
3505.582075	528614.614921	41.421991
3505.755891	528558.647794	41.426996
3505.480462	528523.672125	41.432000
3505.489552	528472.480823	41.437005
3505.539329	528448.318205	41.442010
3505.451196	528409.522692	41.447015
3505.766187	528360.708280	41.452020
3505.263308	528327.688398	41.457024
3505.352293	528284.973500	41.462029
3505.304843	528252.942689	41.467034
3505.032098	528216.753105	41.472039
3505.363082	528176.324227	41.477044
3505.093069	528161.964784	41.482048
3505.365599	528113.510060	41.487053
3505.388954	528071.108164	41.492058
3505.337676	528039.178594	41.497063
3505.512113	527998.420263	41.502068
3505.171970	527960.472034	41.507072
3505.152806	527931.821930	41.512077
3505.444711	527897.715371	41.517082
3505.346442	527862.558636	41.522087
3504.867086	527833.172526	41.527092
3504.905966	527793.850078	41.532096
3505.305737	527769.226825	41.537101
3505.250026	527737.044670	41.542106
3504.932783	527692.269890	41.547111
3505.493796	527670.046708	41.552116
3504.885724	527637.749509	41.557120
3504.976969	527596.043113	41.562125
3504.936726	527576.845912	41.567130
3504.698531	527538.981631	41.572135
3504.714106	527522.302345	41.577140
3504.704848	527486.878028	41.582144
3504.665483	527458.432407	41.587149
3504.918944	527435.701606	41.592154
3504.452902	527411.164104	41.597159
3505.072157	527382.715325	41.602164
3504.738341	527365.585730	41.607168
3504.631253	527334.926979	41.612173
3504.560003	527305.071094	41.617178
3504.686034	527282.865584	41.622183
3504.809568	527257.476607	41.627188
3504.400141	527241.217957	41.632192
3504.969034	527194.381310	41.637197
3504.843783	527182.373346	41.642202
3504.631988	527154.864104	41.647207
3504.613952	527139.705848	41.652212
3504.666495	527108.819282	41.657216
3504.470444	527100.208454	41.662221
3504.458979	527069.079239	41.667226
3504.303578	527043.531857	41.672231
3504.809503	527022.428307	41.677236
3504.392557	527009.960937	41.682240
3504.687475	526968.119628	41.687245
3504.657438	526951.194263	41.692250
3504.563337	526930.943496	41.697255
3504.742450	526910.649521	41.702260
3504.791993	526880.824286	41.707264
3504.494276	526863.789520	41.712269
3504.876548	526831.788999	41.717274
3504.939583	526799.889408	41.722279
3504.585159	526778.517207	41.727284
3504.534049	526770.085446	41.732288
3504.449973	526735.277742	41.737293
3504.682953	526710.325443	41.742298
3504.257587	526696.999999	41.747303
3504.392062	526669.283572	41.752308
3504.508099	526655.569292	41.757312
3504.346561	526625.069394	41.762317
3504.550659	526614.424039	41.767322
3504.265670	526588.239399	41.772327
3504.804527	526565.057937	41.777332
3504.351922	526557.851921	41.782336
3504.330870	526528.896352	41.787341
3504.496503	526502.741429	41.792346
3504.392442	526486.181045	41.797351
3504.800856	526461.756563	41.802356
3504.666335	526441.309404	41.807360
3504.915389	526417.971374	41.812365
3504.722526	526390.912675	41.817370
3504.287860	526360.960837	41.822375
3504.651370	526349.784712	41.827380
3503.920752	526327.410025	41.832384
3504.702766	526297.467931	41.837389
3504.692017	526283.621749	41.842394
3504.148305	526271.628695	41.847399
3504.366802	526247.082282	41.852404
3504.394823	526227.064019	41.857408
3504.555599	526206.367725	41.862413
3504.578450	526184.682396	41.867418
3504.358393	526170.010011	41.872423
3504.614379	526143.132653	41.877428
3504.304516	526121.701985	41.882432
3504.726611	526098.083436	41.887437
3504.393039	526079.638358	41.892442
3504.152766	526065.828264	41.897447
3504.648731	526040.176324	41.902452
3504.404290	526024.446300	41.907456
3504.358999	525991.045986	41.912461
3504.116468	525986.990590	41.917466
3504.151601	525964.747070	41.922471
3504.042876	525938.786210	41.927476
3504.119370	525934.629838	41.932480
3504.466044	525906.524761	41.937485
3504.393736	525907.092237	41.942490
3503.999979	525878.497641	41.947495
3504.408675	525853.010818	41.952500
3503.907379	525853.393391	41.957504
3504.675599	525835.481471	41.962509
3504.414963	525810.403618	41.967514
3504.159293	525794.270809	41.972519
3504.397351	525766.688070	41.977524
3504.204191	525760.350436	41.982528
3504.244856	525746.192412	41.987533
3504.479037	525734.935216	41.992538
3504.046928	525712.512484	41.997543
3504.447758	525688.492356	42.002548
3504.363768	525673.191505	42.007552
3504.206019	525647.086293	42.012557
3504.315279	525650.607064	42.017562
3504.364136	525615.169401	42.022567
3504.099717	525607.225619	42.027572
3504.030879	525602.536166	42.032576
3503.920634	525572.228319	42.037581
3504.156899	525572.696494	42.042586
3504.110832	525554.407538	42.047591
3504.266678	525530.729148	42.052596
3504.160569	525533.424763	42.057600
3503.964436	525499.289125	42.062605
3503.995644	525484.576397	42.067610
3503.870515	525483.787586	42.072615
3504.084738	525478.699561	42.077620
3504.091758	525460.098850	42.082624
3504.109515	525436.947574	42.087629
3504.284332	525432.977703	42.092634
3503.910653	525409.433369	42.097639
3503.991189	525396.936649	42.102644
3504.420581	525392.977075	42.107648
3503.828055	525364.059173	42.112653
3504.343462	525350.432281	42.117658
3504.202596	525339.284627	42.122663
3504.202440	525314.771343	42.127668
3504.346765	525311.716038	42.132672
3504.265058	525286.305823	42.137677
3504.530322	525266.905924	42.142682
3504.489879	525246.745626	42.147687
3504.484223	525228.348823	42.152692
3504.227772	525204.532942	42.157696
3504.516703	525192.660191	42.162701
3504.752511	525164.369161	42.167706
3504.338955	525155.640028	42.172711
3504.601782	525124.413126	42.177716
3504.401056	525108.321484	42.182720
3504.281068	525091.509453	42.187725
3504.512835	525071.558630	42.192730
3504.331734	525051.066509	42.197735
3504.402301	525021.689377	42.202740
3504.312248	525015.891136	42.207744
3504.230135	524982.545081	42.212749
3504.378977	524991.013071	42.217754
3504.282381	524956.810001	42.222759
3504.461118	524946.268635	42.227764
3504.004723	524924.859521	42.232768
3504.178267	524909.517236	42.237773
3504.153892	524902.697685	42.242778
3504.335119	524876.032196	42.247783
3504.348658	524855.155250	42.252788
3504.362277	524843.022487	42.257792
3504.215369	524818.228370	42.262797
3504.196701	524808.779553	42.267802
3504.154412	524794.583255	42.272807
3504.397974	524772.911675	42.277812
3504.154934	524758.544894	42.282816
3504.028409	524732.635436	42.287821
3503.947595	524725.824730	42.292826
3504.159804	524716.187733	42.297831
3504.149835	524688.490706	42.302836
3504.105113	524683.999353	42.307840
3504.142882	524662.511785	42.312845
3504.599205	524643.080937	42.317850
3504.256897	524628.375912	42.322855
3504.466257	524609.438964	42.327860
3504.191989	524606.601321	42.332864
3504.136551	524578.759655	42.337869
3504.076329	524555.316158	42.342874
3504.211883	524547.814088	42.347879
3504.213598	524526.483674	42.352884
3503.843404	524516.028785	42.357888
3504.131482	524500.061459	42.362893
3504.093134	524487.178455	42.367898
3503.892264	524483.975369	42.372903
3504.064998	524458.776357	42.377908
3504.100467	524442.040166	42.382912
3503.908820	524439.745439	42.387917
3504.119632	524430.007399	42.392922
3504.264243	524417.651428	42.397927
3504.385737	524402.316886	42.402932
3503.950702	524388.131756	42.407936
3504.048831	524360.063256	42.412941
3504.341815	524347.431049	42.417946
3504.408972	524339.686961	42.422951
3504.360909	524322.205654	42.427956
3504.039827	524314.927286	42.432960
3504.265669	524277.032473	42.437965
3504.094975	524274.026761	42.442970
3504.235464	524267.281977	42.447975
3504.528491	524234.633274	42.452980
3504.347285	524230.769924	42.457984
3504.049141	524198.871689	42.462989
3504.357955	524181.889839	42.467994
3503.849565	524177.825454	42.472999
3504.154348	524155.233526	42.478004
3504.458287	524149.119967	42.483008
3504.348239	524114.715042	42.488013
3504.046249	524103.844729	42.493018
3503.900267	524097.600073	42.498023
3503.777978	524068.757151	42.503028
3503.780262	524068.099772	42.508032
3503.900167	524058.022047	42.513037
3504.035508	524052.743852	42.518042
3503.974485	524030.512848	42.523047
3504.209326	524014.452361	42.528052
3503.843875	524014.864046	42.533056
3503.911623	523984.373426	42.538061
3504.025206	523978.492077	42.543066
3503.976036	523974.405608	42.548071
3504.314683	523957.823185	42.553076
3504.041164	523951.952461	42.558080
3503.943556	523931.951190	42.563085
3504.215839	523915.530855	42.568090
3503.872783	523907.345919	42.573095
3503.854192	523904.113907	42.578100
3503.714540	523892.712317	42.583104
3503.867320	523870.194562	42.588109
3503.673399	523852.028130	42.593114
3503.804121	523844.880330	42.598119
3504.161880	523848.109484	42.603124
3503.718438	523829.881369	42.608128
3503.877626	523809.687715	42.613133
3504.012096	523809.211626	42.618138
3503.579859	523791.739914	42.623143
3503.832746	523772.087431	42.628148
3503.652966	523775.249915	42.633152
3503.676844	523767.209104	42.638157
3503.520465	523768.800903	42.643162
3503.628294	523778.286975	42.648167
3504.003489	523756.997608	42.653172
3503.527152	523748.075435	42.658176
3503.860461	523745.596542	42.663181
3503.760603	523735.654445	42.668186
3503.405047	523737.227179	42.673191
3503.708463	523713.219501	42.678196
3503.647599	523705.950276	42.683200
3503.950836	523694.882933	42.688205
3503.821891	523697.026432	42.693210
3503.594694	523706.161113	42.698215
3503.660482	523668.189070	42.703220
3503.551615	523665.881148	42.708224
3503.504840	523653.099904	42.713229
3503.469840	523663.013006	42.718234
3503.510292	523666.595638	42.723239
3503.872942	523670.329538	42.728244
3503.869345	523651.981155	42.733248
3503.688396	523635.379427	42.738253
3503.449669	523623.032886	42.743258
3503.340082	523615.164739	42.748263
3503.781173	523614.690730	42.753268
3503.794835	523613.576598	42.758272
3503.395723	523619.705590	42.763277
3503.721744	523597.867752	42.768282
3503.661141	523586.402903	42.773287
3503.635193	523588.934527	42.778292
3503.658189	523588.880438	42.783296
3503.640930	523576.347211	42.788301
3503.677051	523570.023020	42.793306
3503.555742	523556.798543	42.798311
3503.986270	523539.392390	42.803316
3504.001229	523554.049242	42.808321
3504.033205	523538.171991	42.813325
3504.057590	523506.878542	42.818330
3503.754791	523512.436314	42.823335
3504.015257	523505.368956	42.828340
3503.875141	523480.420058	42.833345
3503.605058	523468.078353	42.838349
3503.982390	523460.335368	42.843354
3503.821163	523462.938941	42.848359
3503.948013	523429.354444	42.853364
3504.034584	523431.463916	42.858369
3503.722777	523429.137486	42.863373
3503.873608	523422.239067	42.868378
3503.746975	523405.679067	42.873383
3503.979128	523382.288751	42.878388
3503.532569	523390.952788	42.883393
3503.838802	523387.062743	42.888397
3503.485098	523375.694619	42.893402
3503.631350	523349.133230	42.898407
3503.793530	523344.356055	42.903412
3503.643665	523345.896315	42.908417
3504.131348	523347.032514	42.913421
3504.134092	523335.860771	42.918426
3503.969376	523310.814399	42.923431
3503.989142	523293.169607	42.928436
3503.940400	523306.168618	42.933441
3504.085248	523269.699626	42.938445
3504.004644	523262.888267	42.943450
3504.000497	523256.772516	42.948455
3503.923101	523227.364947	42.953460
3503.902152	523223.273827	42.958465
3503.564328	523223.630613	42.963469
3503.779847	523224.809837	42.968474
3503.875207	523200.935382	42.973479
3504.220815	523181.722475	42.978484
3503.672970	523187.723487	42.983489
3503.476289	523178.807346	42.988493
3503.613629	523158.464682	42.993498
3503.325977	523149.310154	42.998503
3503.889500	523141.941990	43.003508
3504.148014	523138.463828	43.008513
3503.967722	523134.802269	43.013517
3503.964408	523110.639976	43.018522
3503.785754	523122.547567	43.023527
3504.124970	523106.368582	43.028532
3503.839644	523099.387310	43.033537
3503.967552	523073.384419	43.038541
3504.193538	523067.889376	43.043546
3503.701266	523070.444234	43.048551
3504.121489	523029.381658	43.053556
3503.677627	523034.911339	43.058561
3503.700892	523020.197613	43.063565
3503.690522	523022.878514	43.068570
3503.757488	523010.988691	43.073575
3504.340133	522991.434793	43.078580
3503.682690	522994.066318	43.083585
3503.850711	522986.457291	43.088589
3504.110902	522969.987357	43.093594
3503.672615	522952.818994	43.098599
3503.709132	522958.879382	43.103604
3503.415215	522959.532536	43.108609
3504.148332	522946.020864	43.113613
3503.926678	522938.523953	43.118618
3503.551269	522927.108392	43.123623
3504.009764	522918.947917	43.128628
3503.849818	522906.942229	43.133633
3503.619119	522878.316516	43.138637
3503.837181	522869.941263	43.143642
3503.607844	522863.001591	43.148647
3503.993220	522861.120945	43.153652
3503.953931	522833.829773	43.158657
3503.766821	522828.147185	43.163661
3503.793386	522816.668012	43.168666
3503.805187	522828.191860	43.173671
3503.747839	522801.661752	43.178676
3503.756528	522785.281932	43.183681
3503.431908	522790.337889	43.188685
3503.933645	522781.260591	43.193690
3504.280082	522784.542302	43.198695
3503.978290	522764.824611	43.203700
3503.620930	522761.848118	43.208705
3504.153644	522750.491106	43.213709
3503.892122	522736.580401	43.218714
3503.558931	522730.870315	43.223719
3503.869562	522711.763483	43.228724
3503.529954	522709.441341	43.233729
3504.138339	522693.320505	43.238733
3504.025933	522667.557149	43.243738
3503.581981	522664.038258	43.248743
3503.940548	522655.590136	43.253748
3503.932629	522643.155813	43.258753
3503.931522	522628.951098	43.263757
3503.975152	522622.018731	43.268762
3504.006701	522616.604818	43.273767
3504.178115	522591.504206	43.278772
3504.013305	522575.151596	43.283777
3503.753874	522572.007934	43.288781
3503.976967	522550.943230	43.293786
3503.790543	522540.104146	43.298791
3503.845168	522538.680155	43.303796
3503.852066	522526.597263	43.308801
3503.812400	522509.062114	43.313805
3503.624450	522494.836261	43.318810
3503.677506	522485.020882	43.323815
3503.691605	522484.513228	43.328820
3503.582720	522492.366091	43.333825
3503.683167	522486.435726	43.338829
3503.970485	522461.164937	43.343834
3503.506992	522456.536942	43.348839
3503.831452	522452.896555	43.353844
3503.849142	522460.881085	43.358849
3503.642689	522441.754557	43.363853
3503.677327	522416.776396	43.368858
3503.349416	522423.652866	43.373863
3503.867864	522413.005604	43.378868
3503.821928	522423.022299	43.383873
3503.688463	522405.097444	43.388877
3503.706904	522385.025363	43.393882
3503.593534	522374.022965	43.398887
3503.725384	522372.131783	43.403892
3503.664399	522372.647039	43.408897
3503.851014	522375.499123	43.413901
3504.001237	522342.919725	43.418906
3503.714966	522345.290478	43.423911
3504.017627	522336.042187	43.428916
3503.618151	522327.208181	43.433921
3503.742136	522311.264632	43.438925
3504.152407	522295.730793	43.443930
3503.742478	522291.650363	43.448935
3504.205625	522280.556782	43.453940
3503.670476	522260.673148	43.458945
3503.839858	522251.951403	43.463949
3503.857588	522252.909197	43.468954
3503.785927	522249.331372	43.473959
3504.129126	522219.198310	43.478964
3504.006113	522212.039342	43.483969
3503.929904	522203.002516	43.488973
3503.816892	522191.140538	43.493978
3503.701534	522170.482703	43.498983
3503.925903	522163.319362	43.503988
3503.689883	522170.939710	43.508993
3503.866728	522143.309897	43.513997
3504.145457	522132.953106	43.519002
3503.868983	522128.396564	43.524007
3503.504286	522127.038811	43.529012
3503.886399	522108.880481	43.534017
3503.767331	522094.795050	43.539021
3503.919805	522085.722015	43.544026
3503.582593	522085.472086	43.549031
3504.144265	522066.021498	43.554036
3503.764687	522060.925146	43.559041
3503.932592	522043.356686	43.564045
3504.197414	522031.586534	43.569050
3503.718629	522027.011385	43.574055
3504.044520	522003.149283	43.579060
3503.905102	522006.912372	43.584065
3503.473151	521991.865233	43.589069
3503.759684	521967.149889	43.594074
3503.647381	521965.297249	43.599079
3503.783622	521958.653283	43.604084
3504.081892	521960.173398	43.609089
3503.401472	521959.623836	43.614093
3504.114887	521930.038369	43.619098
3503.515199	521932.256502	43.624103
3503.901616	521918.343793	43.629108
3503.643546	521924.855558	43.634113
3503.811979	521913.454431	43.639117
3503.662561	521889.616733	43.644122
3503.747719	521881.514747	43.649127
3504.256952	521885.781991	43.654132
3503.995475	521879.403067	43.659137
3504.193041	521852.679455	43.664141
3503.805743	521845.663204	43.669146
3503.932958	521842.559397	43.674151
3504.043033	521811.906332	43.679156
3504.327033	521809.081063	43.684161
3504.315929	521791.338407	43.689165
3504.105498	521783.940295	43.694170
3504.068614	521765.038939	43.699175
3504.184059	521746.517919	43.704180
3504.014198	521722.935979	43.709185
3503.779255	521729.241949	43.714189
3503.957030	521708.436088	43.719194
3503.889125	521689.034001	43.724199
3503.853482	521682.821525	43.729204
3503.816034	521672.059424	43.734209
3503.720607	521671.872382	43.739213
3503.668095	521640.233600	43.744218
3503.529513	521643.996641	43.749223
3503.528796	521621.601131	43.754228
3503.395964	521639.771347	43.759233
3503.640394	521630.076869	43.764237
3504.116323	521634.450552	43.769242
3503.672220	521612.478990	43.774247
3503.767833	521594.870918	43.779252
3503.677769	521590.992528	43.784257
3503.174097	521599.110439	43.789261
3504.013012	521590.282518	43.794266
3503.128668	521572.525976	43.799271
3503.492820	521548.960491	43.804276
3503.577706	521560.271469	43.809281
3503.779017	521549.724324	43.814285
3503.892712	521546.521488	43.819290
3503.695810	521550.293768	43.824295
3503.798486	521543.199943	43.829300
3503.596902	521518.914952	43.834305
3503.988716	521507.276015	43.839309
3504.280195	521501.668984	43.844314
3503.689693	521490.286402	43.849319
3503.813592	521478.588679	43.854324
3503.606294	521468.662171	43.859329
3503.666096	521463.192853	43.864333
3504.118838	521462.160842	43.869338
3503.808801	521445.122273	43.874343
3503.715474	521428.453877	43.879348
3503.909694	521429.282714	43.884353
3504.083059	521417.374908	43.889357
3503.984836	521397.673934	43.894362
3503.694808	521391.804885	43.899367
3503.888643	521369.782723	43.904372
3503.760759	521370.005252	43.909377
3503.513248	521352.602815	43.914381
3503.813120	521334.911622	43.919386
3503.650797	521330.943479	43.924391
3504.019466	521324.919742	43.929396
3503.818318	521324.041627	43.934401
3503.801615	521307.815997	43.939405
3503.662027	521292.519777	43.944410
3503.503344	521301.088866	43.949415
3503.643338	521300.156831	43.954420
3503.720111	521292.409768	43.959425
3503.211901	521284.603491	43.964429
3503.843671	521253.310807	43.969434
3503.867971	521264.581009	43.974439
3503.824849	521256.397876	43.979444
3503.644118	521265.122136	43.984449
3503.519192	521230.460654	43.989453
3503.570526	521209.320248	43.994458
3503.644859	521225.537056	43.999463
3503.677909	521216.583524	44.004468
3503.739044	521207.827773	44.009473
3503.615340	521218.818064	44.014477
3503.395613	521178.003626	44.019482
3503.745880	521178.959482	44.024487
3503.728032	521179.670182	44.029492
3503.747462	521182.801681	44.034497
3503.739379	521177.899114	44.039501
3504.264325	521167.856689	44.044506
3503.486288	521156.554069	44.049511
3503.549687	521140.568393	44.054516
3503.925526	521148.699186	44.059521
3503.883177	521137.128607	44.064525
3503.686986	521112.589376	44.069530
3503.543665	521111.499884	44.074535
3503.559792	521102.852302	44.079540
3503.859700	521110.438996	44.084545
3504.024797	521099.341166	44.089549
3503.737742	521073.451216	44.094554
3503.281330	521065.383864	44.099559
3503.552765	521048.657428	44.104564
3503.581734	521056.337527	44.109569
3503.498994	521063.529713	44.114573
3503.356758	521055.412700	44.119578
3503.531940	521056.901800	44.124583
3503.717898	521051.564075	44.129588
3503.725706	521026.385793	44.134593
3503.360838	521015.472781	44.139597
3503.894965	521007.349957	44.144602
3503.557276	521017.009176	44.149607
3503.875277	521017.767914	44.154612
3503.763948	520989.423341	44.159617
3503.612175	520978.021614	44.164621
3503.861649	520980.004546	44.169626
3503.670281	520971.591916	44.174631
3503.682892	520971.438347	44.179636
3503.634472	520953.549006	44.184641
3503.926449	520929.134570	44.189645
3503.340843	520924.272648	44.194650
3503.108030	520928.303530	44.199655
3503.399445	520931.341534	44.204660
3503.485650	520924.502828	44.209665
3503.370519	520932.003533	44.214669
3503.606192	520931.460810	44.219674
3503.613646	520932.470863	44.224679
3503.605823	520905.323148	44.229684
3503.719606	520911.169860	44.234689
3503.422359	520896.605983	44.239693
3504.118231	520890.429258	44.244698
3503.687133	520897.524905	44.249703
3503.309587	520867.503260	44.254708
3503.736580	520859.245624	44.259713
3503.726625	520848.630305	44.264717
3503.735232	520849.791852	44.269722
3503.506631	520840.475011	44.274727
3503.756838	520847.361884	44.279732
3503.692954	520832.002709	44.284737
3503.551333	520821.054281	44.289741
3504.149334	520813.376281	44.294746
3503.583042	520809.016844	44.299751
3503.485957	520811.661258	44.304756
3503.796356	520806.202670	44.309761
3503.675310	520776.747004	44.314765
3503.567951	520775.955149	44.319770
3503.623530	520774.985870	44.324775
3503.397395	520771.432134	44.329780
3503.688930	520765.420384	44.334785
3503.504635	520761.809476	44.339789
3503.601982	520740.307289	44.344794
3503.637736	520728.521846	44.349799
3503.946443	520721.192871	44.354804
3503.657024	520730.237939	44.359809
3503.377304	520733.770709	44.364813
3503.719676	520717.234951	44.369818
3503.394704	520696.861163	44.374823
3503.637974	520683.222816	44.379828
3503.513623	520686.326578	44.384833
3503.591629	520687.477168	44.389837
3503.634504	520684.538145	44.394842
3503.343919	520685.848107	44.399847
3503.303238	520693.286597	44.404852
3503.343344	520689.791879	44.409857
3503.453068	520687.853442	44.414861
3503.638649	520664.719367	44.419866
3503.148935	520650.741823	44.424871
3503.647710	520648.994680	44.429876
3503.487208	520659.687817	44.434881
3503.215861	520654.017779	44.439885
3503.865867	520652.095061	44.444890
3503.706833	520660.563426	44.449895
3503.941477	520648.594817	44.454900
3503.713530	520623.402618	44.459905
3503.691955	520631.343694	44.464909
3503.832030	520617.620487	44.469914
3503.749779	520621.223185	44.474919
3503.373002	520585.285635	44.479924
3503.768468	520579.510179	44.484929
3503.245517	520570.290265	44.489933
3503.726740	520561.568887	44.494938
3503.481270	520572.427184	44.499943
3503.629646	520568.611980	44.504948
3503.509627	520578.135938	44.509953
3503.765937	520567.225562	44.514957
3504.026686	520543.573855	44.519962
3503.468773	520538.555766	44.524967
3503.492886	520531.423361	44.529972
3503.682166	520527.702799	44.534977
3503.915963	520524.935804	44.539981
3503.869796	520498.248495	44.544986
3503.609307	520501.778275	44.549991
3503.785637	520487.594205	44.554996
3503.698873	520498.983607	44.560001
3503.467470	520477.128568	44.565005
3503.551295	520466.295945	44.570010
3503.246797	520461.136662	44.575015
3503.539076	520449.563264	44.580020
3503.634454	520455.109699	44.585025
3503.178988	520451.946048	44.590029
3503.671914	520452.727726	44.595034
3503.514191	520448.758641	44.600039
3503.647712	520458.899854	44.605044
3503.368674	520436.698381	44.610049
3503.562931	520417.202787	44.615053
3503.525813	520414.175242	44.620058
3503.323252	520412.589481	44.625063
3503.619707	520415.272875	44.630068
3503.560561	520409.518655	44.635073
3503.134850	520416.057515	44.640077
3503.403741	520420.919278	44.645082
3503.438019	520423.087966	44.650087
3503.656416	520404.700827	44.655092
3503.717307	520394.731275	44.660097
3503.458232	520386.935747	44.665101
3503.607774	520374.070334	44.670106
3503.552570	520376.910433	44.675111
3503.298849	520377.152863	44.680116
3503.261811	520382.871927	44.685121
3503.146069	520389.715716	44.690125
3503.664192	520376.387582	44.695130
3503.576771	520384.339185	44.700135
3504.019571	520367.332176	44.705140
3503.615025	520352.885888	44.710145
3503.701714	520333.912782	44.715149
3503.894114	520336.865430	44.720154
3503.537385	520350.673862	44.725159
3503.459429	520329.401076	44.730164
3503.539722	520304.918048	44.735169
3503.469998	520298.407078	44.740173
3503.485859	520302.196575	44.745178
3503.228023	520307.091063	44.750183
3503.631002	520293.730503	44.755188
3503.673032	520296.504689	44.760193
3503.384634	520299.887246	44.765197
3503.603221	520291.662265	44.770202
3503.250568	520279.027827	44.775207
3503.620755	520248.532950	44.780212
3503.620861	520256.875252	44.785217
3503.500806	520259.169473	44.790221
3503.487523	520259.930050	44.795226
3503.639413	520263.141909	44.800231
3503.596821	520256.373839	44.805236
3503.666244	520254.694516	44.810241
3503.553759	520229.685696	44.815245
3503.872607	520221.242597	44.820250
3503.736818	520219.191232	44.825255
3503.669419	520224.359001	44.830260
3503.798722	520219.990581	44.835265
3503.853054	520201.275232	44.840269
3503.896819	520189.387016	44.845274
3503.635683	520191.046275	44.850279
3503.818457	520175.647498	44.855284
3503.995370	520159.946277	44.860289
3503.661974	520148.218761	44.865293
3503.751265	520136.070514	44.870298
3503.644835	520134.823447	44.875303
3503.813671	520125.342263	44.880308
3503.723335	520100.026389	44.885313
3503.650885	520093.212411	44.890317
3503.790457	520095.768977	44.895322
3503.527133	520098.844255	44.900327
3503.700150	520089.362390	44.905332
3503.413022	520069.285193	44.910337
3503.183607	520057.086141	44.915341
3503.814124	520045.105083	44.920346
3503.575477	520055.760405	44.925351
3503.544082	520055.462104	44.930356
3503.818094	520045.913691	44.935361
3503.497332	520039.745653	44.940365
3504.014830	520033.697921	44.945370
3503.626004	520019.501652	44.950375
3503.531375	520003.539841	44.955380
3503.648725	520007.465045	44.960385
3503.660341	520013.884383	44.965389
3503.541581	520003.134032	44.970394
3503.573395	519971.984285	44.975399
3503.798306	519971.594913	44.980404
3503.715001	519962.861324	44.985409
3503.549515	519967.488519	44.990413
3503.577316	519972.186281	44.995418
3503.419538	519975.902178	45.000423
3503.870947	519939.832311	45.005428
3503.876693	519927.595995	45.010433
3503.511937	519924.114543	45.015437
3503.692874	519916.249244	45.020442
3503.823037	519934.329229	45.025447
3503.706275	519899.966993	45.030452
3503.807842	519894.237749	45.035457
3503.513681	519879.116315	45.040461
3503.755334	519868.561712	45.045466
3503.495707	519889.787520	45.050471
3503.663562	519872.924575	45.055476
3503.742737	519855.519467	45.060481
3503.744425	519853.547447	45.065485
3503.807760	519838.925634	45.070490
3503.659306	519849.415154	45.075495
3503.423764	519838.582032	45.080500
3503.636524	519819.234484	45.085505
3503.758593	519808.092019	45.090509
3503.587533	519803.113678	45.095514
3503.670222	519810.785871	45.100519
3503.792285	519806.620727	45.105524
3503.815162	519788.061558	45.110529
3503.493657	519776.685818	45.115533
3503.694676	519762.143295	45.120538
3503.799431	519764.250372	45.125543
3503.774574	519763.546548	45.130548
3503.801097	519756.565107	45.135553
3503.860145	519738.303527	45.140557
3503.931764	519716.197335	45.145562
3503.662489	519726.706029	45.150567
3503.634665	519714.980466	45.155572
3503.827295	519692.248388	45.160577
3503.675464	519679.986232	45.165581
3503.870269	519681.826283	45.170586
3503.662070	519678.016669	45.175591
3503.707546	519663.852569	45.180596
3503.773755	519653.426679	45.185601
3503.751808	519635.329469	45.190605
3503.705401	519632.758294	45.195610
3503.522534	519638.702910	45.200615
3503.528273	519633.443769	45.205620
3503.700160	519617.439459	45.210625
3503.550893	519597.491576	45.215629
3503.618528	519596.621444	45.220634
3503.456601	519593.006741	45.225639
3503.163362	519584.407253	45.230644
3503.411416	519595.188193	45.235649
3503.188654	519592.543764	45.240653
3503.864041	519584.145108	45.245658
3503.690982	519602.778994	45.250663
3503.691430	519568.802026	45.255668
3503.784250	519563.023488	45.260673
3503.742089	519547.052940	45.265677
3503.606967	519554.759679	45.270682
3503.687975	519556.112119	45.275687
3503.611826	519534.635771	45.280692
3503.472423	519518.427758	45.285697
3503.718135	519510.905957	45.290701
3503.840578	519516.296749	45.295706
3503.478287	519510.033951	45.300711
3503.628315	519522.397831	45.305716
3503.425959	519486.935910	45.310721
3503.417650	519481.426135	45.315725
3503.455732	519471.813556	45.320730
3503.451357	519474.595216	45.325735
3503.524950	519471.347752	45.330740
3503.460388	519472.217593	45.335745
3503.438650	519472.170562	45.340749
3503.646594	519470.570388	45.345754
3503.456281	519473.229752	45.350759
3503.450421	519466.860041	45.355764
3503.588566	519429.776778	45.360769
3503.493429	519438.336796	45.365773
3503.427706	519440.015806	45.370778
3503.530981	519436.763644	45.375783
3503.632764	519436.090352	45.380788
3503.329361	519424.205891	45.385793
3503.109788	519435.414776	45.390797
3503.623235	519427.901182	45.395802
3503.497452	519429.690808	45.400807
3503.833264	519415.177237	45.405812
3503.485777	519400.417719	45.410817
3503.421941	519401.135764	45.415821
3503.530088	519389.236792	45.420826
3503.736997	519383.187352	45.425831
3504.054161	519385.210344	45.430836
3503.825941	519372.151045	45.435841
3503.577403	519358.842138	45.440845
3504.128348	519343.283267	45.445850
3503.673455	519349.068734	45.450855
3503.344660	519325.306203	45.455860
3503.546765	519315.768733	45.460865
3503.688314	519303.611611	45.465869
3503.604229	519299.226111	45.470874
3503.689764	519302.903704	45.475879
3503.815825	519300.911960	45.480884
3503.566112	519290.333525	45.485889
3503.393386	519277.113693	45.490893
3503.591988	519268.132930	45.495898
3503.578431	519264.241894	45.500903
3503.322933	519265.596982	45.505908
3503.360232	519263.821511	45.510913
3503.328377	519263.270458	45.515917
3503.663748	519257.655726	45.520922
3503.509315	519261.371255	45.525927
3503.958374	519254.828437	45.530932
3503.548179	519229.308962	45.535937
3503.651797	519225.854456	45.540941
3503.912132	519218.026837	45.545946
3503.666600	519207.447687	45.550951
3503.407326	519211.988792	45.555956
3503.777534	519190.643694	45.560961
3503.520247	519186.791162	45.565965
3503.842979	519182.594145	45.570970
3503.575798	519195.630958	45.575975
3503.580522	519193.810066	45.580980
3503.628062	519190.768914	45.585985
3503.524848	519175.464963	45.590989
3503.670840	519159.110363	45.595994
3503.628238	519150.774407	45.600999
3503.605106	519145.873610	45.606004
3503.546087	519152.911198	45.611009
3503.737236	519153.639515	45.616013
3504.130164	519133.655936	45.621018
3503.738233	519121.633560	45.626023
3503.746501	519119.508725	45.631028
3503.634129	519107.947778	45.636033
3503.462485	519103.222128	45.641037
3503.467990	519074.249022	45.646042
3503.615065	519067.652735	45.651047
3503.723626	519077.293123	45.656052
3503.738188	519067.532338	45.661057
3503.839387	519062.359052	45.666061
3503.901617	519052.894099	45.671066
3503.774070	519047.858088	45.676071
3503.647780	519021.282164	45.681076
3503.887453	519024.177016	45.686081
3503.733676	519019.296829	45.691085
3503.610863	518979.220030	45.696090
3503.775755	518989.963950	45.701095
3503.778174	518978.334206	45.706100
3503.487604	518964.424867	45.711105
3503.788482	518986.372259	45.716109
3503.922461	518959.401159	45.721114
3503.790497	518947.438693	45.726119
3503.637375	518943.468513	45.731124
3503.778750	518938.541653	45.736129
3503.533629	518928.922955	45.741133
3503.852018	518916.737598	45.746138
3503.862892	518893.881455	45.751143
3503.660619	518887.744816	45.756148
3503.552792	518898.430773	45.761153
3503.927676	518896.601907	45.766157
3503.828023	518868.302380	45.771162
3503.763535	518856.076366	45.776167
3503.810182	518848.686852	45.781172
3504.185866	518850.397282	45.786177
3503.901296	518828.346193	45.791181
3504.057764	518811.635650	45.796186
3503.773186	518820.630438	45.801191
3503.548087	518796.193428	45.806196
3503.642679	518770.947402	45.811201
3503.617930	518770.395209	45.816205
3503.679595	518757.036785	45.821210
3503.597195	518761.499494	45.826215
3503.698408	518766.438817	45.831220
3503.859132	518743.912727	45.836225
3503.419525	518737.307907	45.841229
3503.871983	518729.095745	45.846234
3503.597010	518717.206278	45.851239
3503.704443	518715.571354	45.856244
3503.716277	518716.277469	45.861249
3503.389358	518687.457351	45.866253
3503.736243	518664.396090	45.871258
3503.275711	518683.480963	45.876263
3503.772620	518683.604775	45.881268
3503.716164	518675.675277	45.886273
3503.517573	518683.594710	45.891277
3503.747463	518668.692713	45.896282
3503.887339	518649.254181	45.901287
3503.795552	518631.520851	45.906292
3503.805594	518642.542292	45.911297
3503.786959	518624.494009	45.916301
3503.695944	518602.108641	45.921306
3503.694844	518603.726957	45.926311
3503.686886	518591.036736	45.931316
3504.022006	518585.168995	45.936321
3503.805744	518584.394245	45.941325
3503.609823	518552.165391	45.946330
3503.628355	518547.156702	45.951335
3503.949368	518546.195903	45.956340
3503.646227	518558.935518	45.961345
3503.599250	518536.644229	45.966349
3503.716274	518529.344577	45.971354
3503.483945	518518.712331	45.976359
3503.591406	518519.251648	45.981364
3503.845775	518514.761881	45.986369
3503.700975	518519.082826	45.991373
3503.410726	518488.537377	45.996378
3503.148470	518481.449344	46.001383
3503.466027	518467.038952	46.006388
3503.626989	518478.036650	46.011393
3503.458741	518467.849323	46.016397
3503.667376	518476.918038	46.021402
3503.452716	518467.698770	46.026407
3503.504389	518472.646012	46.031412
3503.490639	518456.063140	46.036417
3503.369214	518445.868399	46.041421
3503.313062	518432.730592	46.046426
3503.278217	518434.809340	46.051431
3503.200019	518418.337746	46.056436
3503.228120	518434.615188	46.061441
3503.212835	518438.410038	46.066445
3503.215086	518425.768640	46.071450
3503.362579	518438.487688	46.076455
3502.797536	518440.801928	46.081460
3503.187480	518429.767886	46.086465
3503.307971	518432.732244	46.091469
3503.466556	518430.229611	46.096474
3503.426816	518435.292440	46.101479
3503.201450	518429.310973	46.106484
3503.364158	518439.246565	46.111489
3503.146913	518434.578494	46.116493
3503.660632	518431.716344	46.121498
3503.582530	518442.650721	46.126503
3503.454521	518430.080478	46.131508
3503.531804	518429.158195	46.136513
3503.311717	518431.013399	46.141517
3503.552765	518406.805522	46.146522
3503.278599	518403.511684	46.151527
3503.259994	518388.901533	46.156532
3503.343746	518392.427917	46.161537
3503.175368	518403.022636	46.166541
3503.681151	518393.183812	46.171546
3503.584018	518403.817834	46.176551
3503.097315	518397.321450	46.181556
3503.534965	518390.325013	46.186561
3503.338797	518390.457241	46.191565
3503.635063	518385.505736	46.196570
3503.578871	518392.694896	46.201575
3503.686104	518379.328964	46.206580
3503.848377	518352.554658	46.211585
3503.618063	518353.754144	46.216589
3503.295402	518344.450747	46.221594
3503.441581	518349.029135	46.226599
3503.763076	518352.720211	46.231604
3503.603091	518337.930101	46.236609
3503.636086	518312.591979	46.241613
3503.642125	518306.877282	46.246618
3503.398307	518307.320432	46.251623
3503.684680	518295.190242	46.256628
3503.913986	518305.873863	46.261633
3503.376537	518304.694779	46.266637
3503.493205	518263.415393	46.271642
3503.538282	518269.172779	46.276647
3503.601855	518264.005190	46.281652
3503.540896	518264.166614	46.286657
3503.664113	518273.451202	46.291661
3504.111163	518254.115350	46.296666
3503.760913	518247.344513	46.301671
3503.606333	518229.115023	46.306676
3503.720062	518221.107844	46.311681
3503.459045	518227.975492	46.316685
3503.934839	518226.838517	46.321690
3503.602225	518196.198092	46.326695
3503.464155	518187.472214	46.331700
3503.401505	518193.044392	46.336705
3503.307583	518184.564362	46.341709
3503.745991	518186.871734	46.346714
3503.554790	518193.728361	46.351719
3503.547409	518187.762918	46.356724
3503.698136	518173.732597	46.361729
3503.784554	518163.403700	46.366733
3503.609253	518143.003079	46.371738
3503.611742	518145.834444	46.376743
3503.964530	518141.379587	46.381748
3503.625863	518142.393951	46.386753
3503.395011	518116.541010	46.391757
3503.840353	518102.008973	46.396762
3503.791444	518097.213069	46.401767
3503.912537	518100.531351	46.406772
3503.811446	518083.911345	46.411777
3503.471564	518076.633143	46.416781
3503.668183	518054.504963	46.421786
3503.770399	518053.174194	46.426791
3503.645151	518060.172150	46.431796
3503.828306	518048.310921	46.436801
3503.531806	518031.671181	46.441805
3503.561654	518022.817545	46.446810
3503.737714	518013.789097	46.451815
3503.964654	518012.539743	46.456820
3503.851249	518009.827206	46.461825
3503.523875	517983.281390	46.466829
3503.460426	517972.015308	46.471834
3503.499947	517962.755583	46.476839
3503.911444	517968.151764	46.481844
3503.706379	517967.830308	46.486849
3503.472225	517973.581364	46.491853
3503.642509	517940.686644	46.496858
3503.616494	517937.302923	46.501863
3503.619026	517922.335056	46.506868
3503.866725	517919.717129	46.511873
3503.636561	517920.056998	46.516877
3503.387431	517924.748550	46.521882
3503.627431	517911.310689	46.526887
3503.573220	517893.014398	46.531892
3503.733856	517892.786839	46.536897
3503.546215	517885.383357	46.541901
3503.916385	517873.593578	46.546906
3503.947303	517883.702033	46.551911
3503.618960	517870.657365	46.556916
3504.077450	517852.987924	46.561921
3503.569349	517858.327221	46.566925
3503.482311	517845.750058	46.571930
3503.776330	517848.636529	46.576935
3503.610980	517828.992442	46.581940
3503.748465	517803.990989	46.586945
3503.226947	517804.326343	46.591949
3503.601435	517796.126045	46.596954
3503.437342	517803.079682	46.601959
3503.211186	517805.896677	46.606964
3503.681004	517800.513035	46.611969
3503.302569	517811.748131	46.616973
3503.556186	517789.711721	46.621978
3503.588767	517780.200159	46.626983
3503.175333	517760.544634	46.631988
3503.172055	517751.847788	46.636993
3503.577614	517750.721883	46.641997
3503.696476	517755.203621	46.647002
3503.516371	517756.648046	46.652007
3503.265037	517769.430646	46.657012
3503.661237	517766.334125	46.662017
3503.836029	517753.209842	46.667021
3503.604260	517741.413974	46.672026
3503.778581	517726.469344	46.677031
3503.766815	517723.032762	46.682036
3503.689318	517711.515889	46.687041
3503.509245	517717.663020	46.692045
3503.742805	517695.933056	46.697050
3503.598788	517679.117160	46.702055
3503.330342	517682.041993	46.707060
3503.321630	517674.610136	46.712065
3503.403025	517672.524124	46.717069
3503.504704	517676.755764	46.722074
3503.793062	517673.018901	46.727079
3503.806086	517663.055261	46.732084
3503.760447	517640.004046	46.737089
3503.103031	517642.939796	46.742093
3503.407090	517626.811531	46.747098
3503.805325	517619.365898	46.752103
3503.195352	517636.554049	46.757108
3503.904343	517638.667032	46.762113
3503.545508	517632.554669	46.767117
3503.468322	517608.851025	46.772122
3503.441282	517601.320899	46.777127
3503.387678	517599.205647	46.782132
3503.618070	517572.773282	46.787137
3503.485949	517591.453536	46.792141
3503.509469	517590.286869	46.797146
3503.264998	517589.819931	46.802151
3503.333325	517587.584272	46.807156
3503.433360	517593.990580	46.812161
3503.097151	517600.465835	46.817165
3503.390165	517590.306196	46.822170
3503.579100	517586.787296	46.827175
3503.436543	517573.460193	46.832180
3503.475973	517558.637867	46.837185
3503.341284	517545.107228	46.842189
3503.391242	517543.784678	46.847194
3503.370917	517549.198681	46.852199
3503.251569	517546.942112	46.857204
3503.622743	517543.444967	46.862209
3503.635512	517542.735101	46.867213
3503.359861	517541.059476	46.872218
3502.979593	517550.322914	46.877223
3503.274018	517545.624286	46.882228
3503.602316	517554.522894	46.887233
3503.022843	517550.518629	46.892237
3503.447071	517555.306128	46.897242
3503.533982	517525.862331	46.902247
3503.460904	517516.519019	46.907252
3503.246249	517509.827581	46.912257
3503.297515	517517.606945	46.917261
3503.744612	517503.579781	46.922266
3503.433764	517511.214112	46.927271
3503.283265	517511.187426	46.932276
3503.641389	517502.129924	46.937281
3503.328229	517512.950365	46.942285
3503.608598	517500.416004	46.947290
3503.808216	517507.312280	46.952295
3503.424645	517485.477310	46.957300
3503.509846	517471.608453	46.962305
3503.484143	517463.319540	46.967309
3504.161660	517463.718225	46.972314
3503.619956	517462.337479	46.977319
3503.716926	517451.854769	46.982324
3503.820591	517421.093382	46.987329
3503.373201	517431.985659	46.992333
3503.670839	517428.752950	46.997338
3503.553847	517424.827261	47.002343
3503.562677	517424.067445	47.007348
3503.565388	517392.361176	47.012353
3503.022886	517399.475927	47.017357
3503.443912	517379.030679	47.022362
3503.212959	517389.433665	47.027367
3503.461504	517376.347994	47.032372
3503.879343	517385.434813	47.037377
3503.795008	517380.796003	47.042381
3504.077083	517387.527593	47.047386
3503.833716	517368.603238	47.052391
3503.306962	517354.072486	47.057396
3503.784798	517354.907278	47.062401
3503.744133	517343.637167	47.067405
3503.954498	517334.248953	47.072410
3503.546297	517313.631278	47.077415
3503.280295	517311.903536	47.082420
3504.112068	517307.221048	47.087425
3503.497100	517290.175783	47.092429
3503.534461	517303.823337	47.097434
3503.676761	517297.176531	47.102439
3503.737516	517271.579586	47.107444
3503.836976	517254.471935	47.112449
3503.306731	517267.400141	47.117453
3503.637909	517248.182566	47.122458
3503.413611	517251.353338	47.127463
3503.906341	517255.270438	47.132468
3503.610981	517239.438810	47.137473
3503.659578	517213.894265	47.142477
3503.378992	517210.196654	47.147482
3503.669693	517209.240573	47.152487
3503.324477	517213.846375	47.157492
3504.054886	517201.240658	47.162497
3503.552687	517198.589437	47.167501
3503.708554	517182.787573	47.172506
3503.884100	517183.720720	47.177511
3503.396847	517177.426211	47.182516
3503.672753	517173.236089	47.187521
3503.793076	517169.171694	47.192525
3503.762761	517150.769669	47.197530
3503.651519	517132.430982	47.202535
3503.687730	517130.402612	47.207540
3503.734762	517129.080491	47.212545
3503.679293	517126.308083	47.217549
3503.698440	517112.449365	47.222554
3503.292884	517098.910604	47.227559
3503.444143	517088.823633	47.232564
3503.489586	517068.690208	47.237569
3503.360312	517084.639872	47.242573
3503.501837	517086.134657	47.247578
3503.745977	517073.706838	47.252583
3503.447489	517089.531536	47.257588
3503.624388	517069.731316	47.262593
3503.713109	517049.894440	47.267597
3503.743919	517034.516751	47.272602
3503.742687	517037.601738	47.277607
3503.565443	517039.146910	47.282612
3503.412751	517036.743835	47.287617
3503.503682	517037.943208	47.292621
3503.701771	517020.870297	47.297626
3503.519953	517002.744897	47.302631
3503.264506	517003.392192	47.307636
3503.388998	516997.759459	47.312641
3503.462701	516989.909718	47.317645
3503.398321	517001.904826	47.322650
3503.080975	517000.387441	47.327655
3503.079496	516993.712670	47.332660
3503.009394	517008.995658	47.337665
3502.970394	517004.703559	47.342669
3503.399716	516992.903806	47.347674
3503.522225	517005.476200	47.352679
3503.583592	517001.117668	47.357684
3503.648664	516991.145397	47.362689
3503.212026	517000.316912	47.367693
3503.525733	516990.153636	47.372698
3503.627931	516962.880889	47.377703
3503.648629	516964.091368	47.382708
3503.723308	516947.796422	47.387713
3503.559832	516953.182677	47.392717
3503.520782	516955.616258	47.397722
3503.779609	516953.552681	47.402727
3503.587240	516929.562856	47.407732
3503.610659	516921.265908	47.412737
3503.202485	516919.611163	47.417741
3503.309529	516915.397097	47.422746
3503.556578	516909.643826	47.427751
3503.180730	516909.045924	47.432756
3503.590415	516912.116557	47.437761
3503.002135	516917.974517	47.442765
3503.276402	516907.716286	47.447770
3503.424287	516913.508464	47.452775
3503.329533	516907.556369	47.457780
3503.529419	516916.576756	47.462785
3503.314676	516924.904134	47.467789
3503.372930	516911.645898	47.472794
3503.241347	516881.375814	47.477799
3503.100562	516879.931651	47.482804
3503.773528	516867.587608	47.487809
3503.415548	516874.117154	47.492813
3503.400169	516863.803537	47.497818
3503.667973	516860.170881	47.502823
3503.402391	516879.024738	47.507828
3503.590269	516866.656226	47.512833
3503.778255	516873.756882	47.517837
3503.590210	516857.149386	47.522842
3503.595032	516840.612530	47.527847
3503.823936	516845.886232	47.532852
3503.839426	516835.668857	47.537857
3503.320369	516842.729569	47.542861
3503.525444	516835.971518	47.547866
3503.561120	516827.470308	47.552871
3503.675347	516810.157588	47.557876
3503.802150	516788.038753	47.562881
3503.447041	516790.218895	47.567885
3503.668784	516786.391224	47.572890
3503.379219	516796.298149	47.577895
3503.139914	516787.688672	47.582900
3503.392832	516794.576821	47.587905
3503.733605	516791.539451	47.592909
3503.866681	516757.384025	47.597914
3503.675208	516753.571087	47.602919
3503.569947	516743.271601	47.607924
3503.868166	516743.275130	47.612929
3503.549154	516734.779363	47.617933
3503.860925	516714.249426	47.622938
3503.971943	516711.298925	47.627943
3503.748290	516703.040919	47.632948
3503.570377	516698.315568	47.637953
3503.448142	516699.801507	47.642957
3503.615960	516661.139675	47.647962
3503.653331	516663.055521	47.652967
3503.442849	516656.059658	47.657972
3503.614967	516657.751927	47.662977
3503.330396	516655.976480	47.667981
3503.372334	516647.170768	47.672986
3503.499634	516660.400076	47.677991
3503.557316	516663.526391	47.682996
3503.898000	516636.872824	47.688001
3503.384033	516629.570926	47.693005
3503.256129	516618.111830	47.698010
3503.383953	516615.664357	47.703015
3503.245315	516612.551017	47.708020
3503.679003	516608.386386	47.713025
3503.402299	516612.425253	47.718029
3503.093895	516614.142905	47.723034
3503.587260	516619.627731	47.728039
3503.585745	516610.474877	47.733044
3503.555273	516592.628529	47.738049
3503.524685	516588.891265	47.743053
3503.441605	516570.952068	47.748058
3503.454344	516580.103358	47.753063
3503.544683	516582.516543	47.758068
3503.909178	516567.287962	47.763073
3503.451887	516582.733679	47.768077
3503.694357	516559.534285	47.773082
3503.658872	516538.199321	47.778087
3503.530433	516533.567245	47.783092
3503.266206	516532.951686	47.788097
3503.319510	516532.892785	47.793101
3503.471606	516530.087471	47.798106
3503.459185	516531.758350	47.803111
3503.213115	516541.001137	47.808116
3503.510521	516527.350803	47.813121
3503.279107	516522.937280	47.818125
3503.294255	516520.204180	47.823130
3503.722675	516508.505368	47.828135
3503.829328	516499.183645	47.833140
3503.880063	516490.983306	47.838145
3503.392561	516497.735752	47.843149
3503.681240	516497.943072	47.848154
3503.872011	516479.606500	47.853159
3503.414952	516472.851814	47.858164
3503.878169	516453.713595	47.863169
3503.460679	516450.340874	47.868173
3503.547214	516446.483925	47.873178
3503.596952	516449.611536	47.878183
3503.860123	516438.747923	47.883188
3503.743810	516410.042256	47.888193
3503.562880	516411.790351	47.893197
3503.670901	516406.412876	47.898202
3503.574181	516399.955202	47.903207
3503.317740	516407.176873	47.908212
3503.366109	516405.095922	47.913217
3503.308159	516404.498326	47.918221
3503.645557	516398.022609	47.923226
3503.225579	516377.203346	47.928231
3503.288261	516361.668284	47.933236
3503.577724	516354.036996	47.938241
3503.500716	516364.264578	47.943245
3503.642937	516354.886582	47.948250
3503.324487	516359.791813	47.953255
3503.470625	516353.346307	47.958260
3504.039879	516354.368988	47.963265
3503.564477	516336.137549	47.968269
3503.483723	516326.390211	47.973274
3503.659621	516315.388599	47.978279
3503.456364	516314.864538	47.983284
3503.568633	516316.667444	47.988289
3503.361557	516325.095051	47.993293
3503.586579	516309.331998	47.998298
3503.516551	516305.499762	48.003303
3503.164724	516297.008956	48.008308
3503.260825	516274.540294	48.013313
3503.408752	516268.549613	48.018317
3503.750331	516268.091150	48.023322
3503.583206	516271.404783	48.028327
3503.106830	516274.919007	48.033332
3503.422562	516266.120391	48.038337
3503.358127	516275.031191	48.043341
3503.523220	516268.683799	48.048346
3503.452036	516269.453711	48.053351
3503.372206	516276.040670	48.058356
3503.847717	516259.175986	48.063361
3503.359441	516241.452189	48.068365
3503.571249	516230.191989	48.073370
3503.345129	516226.940689	48.078375
3503.542478	516226.505021	48.083380
3504.013804	516219.148355	48.088385
3503.519276	516229.897152	48.093389
3503.620001	516214.355940	48.098394
3503.798297	516188.637606	48.103399
3503.622287	516194.329514	48.108404
3504.120241	516177.663485	48.113409
3503.588782	516189.581288	48.118413
3503.616344	516164.240740	48.123418
3503.322832	516153.212070	48.128423
3503.360765	516150.475307	48.133428
3503.437395	516142.624704	48.138433
3503.306453	516135.767764	48.143437
3503.272272	516146.342712	48.148442
3503.688048	516140.815366	48.153447
3503.474274	516141.658392	48.158452
3503.705428	516135.603938	48.163457
3503.528376	516142.560317	48.168461
3503.631566	516112.201154	48.173466
3503.546111	516094.059531	48.178471
3503.305414	516101.177702	48.183476
3503.797510	516081.983921	48.188481
3503.553185	516096.182706	48.193485
3503.449611	516097.261176	48.198490
3503.540010	516088.498081	48.203495
3503.552756	516076.106090	48.208500
3503.258793	516065.128004	48.213505
3503.395118	516061.515955	48.218509
3503.271888	516050.258016	48.223514
3503.331468	516047.972961	48.228519
3503.297212	516052.327646	48.233524
3503.439348	516048.461817	48.238529
3503.613595	516055.160421	48.243533
3503.595746	516054.607047	48.248538
3503.809619	516049.718444	48.253543
3503.463098	516052.504185	48.258548
3503.592842	516021.179795	48.263553
3503.502878	516020.637817	48.268557
3503.408903	516009.071794	48.273562
3503.365395	516003.060703	48.278567
3503.240167	516011.930680	48.283572
3503.726144	516007.707065	48.288577
3503.563412	516006.266293	48.293581
3503.523518	516008.396715	48.298586
3503.805219	516005.874260	48.303591
3503.495436	515981.497047	48.308596
3503.665375	515965.590659	48.313601
3503.427774	515974.984138	48.318605
3503.440367	515960.923208	48.323610
3503.433791	515969.572165	48.328615
3503.249742	515970.663362	48.333620
3503.402160	515965.784448	48.338625
3503.219851	515960.756149	48.343629
3503.420256	515957.589099	48.348634
3503.348046	515966.248432	48.353639
3503.050127	515967.913920	48.358644
3503.413617	515966.238257	48.363649
3503.310516	515951.083019	48.368653
3503.184831	515928.345511	48.373658
3503.396701	515926.491520	48.378663
3503.318089	515930.600385	48.383668
3503.510904	515915.499489	48.388673
3503.453897	515927.089628	48.393677
3503.499791	515924.958437	48.398682
3503.260161	515936.476289	48.403687
3503.452755	515931.843876	48.408692
3503.624127	515925.798795	48.413697
3503.736860	515930.383140	48.418701
3503.895048	515918.979488	48.423706
3503.801683	515893.505924	48.428711
3503.548077	515901.182516	48.433716
3503.702306	515892.611518	48.438721
3503.850287	515889.705603	48.443725
3503.522105	515867.556312	48.448730
3503.768287	515843.799039	48.453735
3503.553896	515846.209923	48.458740
3503.803375	515831.706864	48.463745
3503.626020	515843.872380	48.468749
3503.559585	515837.763708	48.473754
3503.849231	515802.620700	48.478759
3503.367400	515810.282832	48.483764
3503.896098	515801.500884	48.488769
3503.806466	515806.471256	48.493773
3503.635375	515800.277966	48.498778
3503.607607	515784.352081	48.503783
3503.428222	515764.758340	48.508788
3503.659488	515748.083461	48.513793
3503.420190	515763.849489	48.518797
3503.581055	515753.456755	48.523802
3503.914789	515758.865953	48.528807
3503.393403	515753.941757	48.533812
3503.545629	515721.804087	48.538817
3503.637547	515710.107331	48.543821
3503.604175	515706.471454	48.548826
3503.442503	515716.409378	48.553831
3503.056474	515716.672777	48.558836
3503.527014	515697.835971	48.563841
3503.572859	515703.695273	48.568845
3503.462592	515708.264352	48.573850
3503.673637	515701.960055	48.578855
3503.291116	515678.858218	48.583860
3503.508994	515667.900117	48.588865
3502.946273	515663.538729	48.593869
3503.421775	515668.217528	48.598874
3503.608563	515673.649980	48.603879
3503.369052	515666.304276	48.608884
3503.778460	515663.458148	48.613889
3503.555383	515666.679598	48.618893
3503.587932	515670.518094	48.623898
3503.934571	515659.539636	48.628903
3503.249907	515645.184060	48.633908
3503.493620	515639.734318	48.638913
3503.174858	515634.980352	48.643917
3503.600787	515611.851790	48.648922
3503.560688	515617.775278	48.653927
3503.260127	515625.661710	48.658932
3503.796860	515624.970094	48.663937
3503.573929	515630.821329	48.668941
3503.289378	515617.616244	48.673946
3503.592274	515595.012835	48.678951
3503.612690	515591.267285	48.683956
3503.696525	515568.698464	48.688961
3503.535578	515590.521063	48.693965
3503.236499	515579.695185	48.698970
3503.602235	515582.216708	48.703975
3502.990093	515585.600813	48.708980
3503.427336	515591.246573	48.713985
3502.984737	515578.420449	48.718989
3502.983483	515590.406596	48.723994
3503.486067	515588.253753	48.728999
3503.024122	515590.804947	48.734004
3503.580408	515588.036738	48.739009
3503.396925	515600.304546	48.744013
3503.734440	515573.700355	48.749018
3503.547932	515554.764944	48.754023
3503.225010	515559.165382	48.759028
3503.481062	515539.451980	48.764033
3503.364618	515544.831254	48.769037
3503.340344	515548.628185	48.774042
3503.356957	515547.159027	48.779047
3503.403881	515546.949411	48.784052
3503.424942	515537.792399	48.789057
3503.088740	515546.797115	48.794061
3503.322420	515542.613261	48.799066
3503.426464	515533.443131	48.804071
3503.131640	515555.438656	48.809076
3503.461283	515539.810061	48.814081
3503.523707	515538.283088	48.819085
3503.389001	515515.597016	48.824090
3503.395771	515504.975615	48.829095
3503.217481	515497.974175	48.834100
3503.287502	515494.119617	48.839105
3503.399646	515503.710948	48.844109
3503.576177	515497.766044	48.849114
3503.743503	515492.783489	48.854119
3503.456501	515498.493176	48.859124
3503.488714	515501.573162	48.864129
3503.493192	515497.273802	48.869133
3503.293081	515477.733572	48.874138
3503.178553	515463.742889	48.879143
3503.711335	515460.169196	48.884148
3503.652988	515449.406332	48.889153
3503.303850	515450.776523	48.894157
3503.372921	515456.278225	48.899162
3503.623751	515459.677680	48.904167
3503.651366	515456.740140	48.909172
3503.715771	515461.079385	48.914177
3503.598566	515432.776764	48.919181
3503.446183	515415.656454	48.924186
3503.306664	515415.779747	48.929191
3503.406085	515406.964295	48.934196
3503.413642	515411.615980	48.939201
3502.930902	515419.076139	48.944205
3503.164052	515412.211929	48.949210
3503.721363	515406.307956	48.954215
3503.327420	515423.312517	48.959220
3503.401143	515417.333259	48.964225
3503.384163	515424.011769	48.969229
3503.483541	515413.679115	48.974234
3503.538334	515414.530303	48.979239
3503.294583	515399.042777	48.984244
3503.309581	515375.321377	48.989249
3503.184678	515383.382455	48.994253
3503.337138	515371.473596	48.999258
3503.295488	515367.080346	49.004263
3503.328387	515377.038293	49.009268
3503.391322	515370.302116	49.014273
3503.496345	515374.533816	49.019277
3503.540537	515362.945506	49.024282
3503.818600	515373.218724	49.029287
3503.442457	515382.887300	49.034292
3503.562594	515357.884912	49.039297
3503.558506	515350.097268	49.044301
3503.115226	515326.903398	49.049306
3503.422987	515324.477871	49.054311
3503.298172	515335.573397	49.059316
3503.625218	515328.947182	49.064321
3503.568856	515327.843556	49.069325
3503.573213	515333.861267	49.074330
3503.552559	515330.273872	49.079335
3503.360904	515333.389272	49.084340
3503.557229	515324.052720	49.089345
3503.450462	515304.952701	49.094349
3503.022215	515288.432177	49.099354
3503.576599	515289.811298	49.104359
3503.578216	515297.447827	49.109364
3503.488921	515276.574920	49.114369
3503.428527	515293.931487	49.119373
3503.266905	515289.860623	49.124378
3503.520587	515273.738044	49.129383
3503.493369	515290.229610	49.134388
3503.689938	515274.824098	49.139393
3503.337015	515251.211247	49.144397
3503.339699	515242.663869	49.149402
3503.313773	515229.013005	49.154407
3502.985727	515247.828003	49.159412
3503.297876	515236.854721	49.164417
3503.400584	515243.008642	49.169421
3503.355465	515239.121649	49.174426
3503.326393	515229.921818	49.179431
3503.336557	515246.458094	49.184436
3503.545805	515234.641311	49.189441
3503.315479	515236.498483	49.194445
3503.366025	515237.451500	49.199450
3503.735683	515234.662157	49.204455
3503.067275	515240.331066	49.209460
3503.378373	515238.865910	49.214465
3503.429382	515235.317743	49.219469
3503.646044	515228.102043	49.224474
3503.623591	515210.455244	49.229479
3503.281214	515202.215255	49.234484
3503.640798	515193.156273	49.239489
3503.599426	515197.208859	49.244493
3503.429996	515201.483981	49.249498
3503.772445	515196.220787	49.254503
3503.518181	515184.628952	49.259508
3503.523998	515167.533959	49.264513
3503.362800	515168.520446	49.269517
3503.416105	515156.424809	49.274522
3503.758697	515152.527091	49.279527
3503.334109	515160.231045	49.284532
3503.713887	515160.474561	49.289537
3503.815829	515154.490750	49.294541
3503.839025	515148.114786	49.299546
3503.880162	515125.956712	49.304551
3503.517293	515125.963584	49.309556
3503.783743	515131.029600	49.314561
3503.713069	515124.061569	49.319565
3503.464530	515089.861893	49.324570
3503.623761	515090.494291	49.329575
3503.367661	515081.684284	49.334580
3503.852040	515070.380223	49.339585
3503.450967	515075.703485	49.344589
3503.292728	515082.657330	49.349594
3503.579563	515074.570703	49.354599
3503.376139	515080.317897	49.359604
3503.506058	515075.644579	49.364609
3503.386400	515057.709534	49.369613
3503.389877	515041.626278	49.374618
3503.582501	515034.414294	49.379623
3503.198002	515040.594720	49.384628
3503.453857	515023.712935	49.389633
3503.072792	515041.474471	49.394637
3503.369150	515039.859904	49.399642
3503.833106	515031.947561	49.404647
3503.666877	515042.139480	49.409652
3503.594786	515031.934842	49.414657
3503.350305	515014.070053	49.419661
3503.115968	515003.638167	49.424666
3503.320748	514989.090868	49.429671
3503.098696	514987.912258	49.434676
3503.061247	514986.653895	49.439681
3503.136236	514998.072091	49.444685
3503.147428	514993.417515	49.449690
3503.436784	515002.728251	49.454695
3503.492146	514996.701170	49.459700
3503.457025	514998.881540	49.464705
3503.227846	515001.851207	49.469709
3503.373859	514989.892521	49.474714
3503.541586	514991.585656	49.479719
3503.119610	515001.666296	49.484724
3503.236866	514986.728229	49.489729
3503.220260	514997.908027	49.494733
3503.266734	515006.296224	49.499738
3503.590035	514994.258945	49.504743
3503.396668	514998.386177	49.509748
3503.543265	514992.192950	49.514753
3503.356560	514995.408780	49.519757
3503.294307	514996.581938	49.524762
3503.658130	514981.099145	49.529767
3502.848705	514972.427110	49.534772
3503.492511	514954.219561	49.539777
3503.276560	514958.046921	49.544781
3503.294758	514953.542953	49.549786
3503.532407	514946.829566	49.554791
3503.389709	514952.718931	49.559796
3503.514889	514949.209556	49.564801
3503.235718	514958.256148	49.569805
3503.273924	514960.172058	49.574810
3503.665838	514949.944607	49.579815
3503.433945	514962.726285	49.584820
3503.361912	514959.399807	49.589825
3503.685960	514963.647568	49.594829
3503.467235	514948.560269	49.599834
3503.413665	514918.527164	49.604839
3503.367920	514921.923029	49.609844
3503.217820	514911.477771	49.614849
3503.265220	514910.863471	49.619853
3503.058661	514916.611216	49.624858
3503.477619	514910.374911	49.629863
3502.967513	514909.899301	49.634868
3503.175376	514900.813567	49.639873
3503.025791	514900.989029	49.644877
3502.948054	514895.539277	49.649882
3503.299921	514901.653944	49.654887
3503.155180	514904.306830	49.659892
3503.372791	514901.035712	49.664897
3503.125606	514893.286277	49.669901
3502.673617	514905.141855	49.674906
3503.532210	514909.203993	49.679911
3502.898731	514910.720318	49.684916
3502.980033	514915.107610	49.689921
3503.162601	514931.364072	49.694925
3503.036259	514945.090009	49.699930
3503.173910	514959.735137	49.704935
3503.077097	514964.504593	49.709940
3503.248032	514957.852331	49.714945
3503.152016	514957.614725	49.719949
3502.908440	514961.497026	49.724954
3503.373642	514954.545377	49.729959
3503.245430	514963.820982	49.734964
3503.377761	514955.809292	49.739969
3503.424725	514947.305340	49.744973
3503.528536	514938.488947	49.749978
3503.623175	514916.018688	49.754983
3503.362541	514919.145066	49.759988
3503.212592	514909.104384	49.764993
3503.451980	514909.572395	49.769997
3503.123224	514914.580826	49.775002
3502.978085	514913.086602	49.780007
3503.560987	514907.987615	49.785012
3503.805467	514914.675578	49.790017
3503.661911	514916.165044	49.795021
3503.447932	514912.254089	49.800026
3503.731007	514899.413896	49.805031
3503.430582	514880.495726	49.810036
3503.819572	514878.815927	49.815041
3503.542532	514873.549395	49.820045
3503.649753	514877.932599	49.825050
3504.089193	514867.899889	49.830055
3503.587638	514846.231822	49.835060
3503.456404	514831.585769	49.840065
3503.583569	514831.717490	49.845069
3503.224820	514828.335152	49.850074
3503.345905	514820.578052	49.855079
3503.195990	514831.070974	49.860084
3503.544361	514822.215867	49.865089
3503.508823	514824.396325	49.870093
3503.057156	514834.178305	49.875098
3503.257634	514822.666072	49.880103
3503.325314	514825.841727	49.885108
3503.399701	514816.321863	49.890113
3503.389737	514830.737557	49.895117
3503.384747	514809.749592	49.900122
3503.420240	514780.309069	49.905127
3503.146593	514793.653807	49.910132
3503.325258	514790.489974	49.915137
3503.478074	514782.474964	49.920141
3503.404988	514786.128056	49.925146
3503.933487	514781.442235	49.930151
3503.305022	514781.693387	49.935156
3503.390022	514788.710061	49.940161
3503.175603	514793.700456	49.945165
3503.236054	514792.628908	49.950170
3503.653701	514788.061760	49.955175
3503.233130	514791.264017	49.960180
3503.374114	514761.907939	49.965185
3503.583487	514749.585038	49.970189
3503.463917	514749.250000	49.975194
3503.514247	514737.862591	49.980199
3503.743360	514745.665719	49.985204
3503.537401	514743.220153	49.990209
3503.226873	514742.460115	49.995213
3503.140187	514749.301638	50.000218
3503.483104	514751.877472	50.005223
3503.100304	514751.685190	50.010228
3503.329046	514744.214494	50.015233
3503.423656	514746.172090	50.020237
3503.446643	514732.513090	50.025242
3503.529392	514716.973326	50.030247
3503.583013	514709.783173	50.035252
3503.643220	514700.214909	50.040257
3503.203413	514712.928487	50.045261
3503.328636	514710.936330	50.050266
3503.655898	514704.613290	50.055271
3503.029106	514718.165632	50.060276
3503.796201	514704.743031	50.065281
3503.782684	514698.575002	50.070285
3503.386283	514679.722350	50.075290
3503.304040	514667.799511	50.080295
3503.194159	514666.400844	50.085300
3503.481328	514665.091150	50.090305
3503.524543	514660.684301	50.095309
3503.279550	514661.330029	50.100314
3503.774254	514650.529815	50.105319
3503.304609	514665.068882	50.110324
3503.668176	514652.822691	50.115329
3503.512292	514658.107331	50.120333
3503.247645	514639.132656	50.125338
3503.218940	514629.376100	50.130343
3503.438382	514619.529742	50.135348
3503.513545	514615.168407	50.140353
3503.425633	514616.901985	50.145357
3503.571555	514619.964161	50.150362
3503.716727	514617.513655	50.155367
3503.393240	514624.038623	50.160372
3503.411490	514614.072332	50.165377
3503.957250	514612.367730	50.170381
3503.420271	514590.856659	50.175386
3503.631579	514574.335496	50.180391
3503.551577	514570.099827	50.185396
3503.679537	514563.959964	50.190401
3503.485517	514574.460017	50.195405
3503.688980	514569.825511	50.200410
3504.054536	514541.900266	50.205415
3503.609825	514537.975114	50.210420
3503.696115	514532.903930	50.215425
3503.775934	514534.155819	50.220429
3503.380321	514524.558345	50.225434
3503.585711	514509.403617	50.230439
3503.703530	514497.095002	50.235444
3503.512263	514488.223858	50.240449
3503.420202	514488.643115	50.245453
3503.218702	514487.360067	50.250458
3503.760792	514480.446647	50.255463
3503.366214	514489.865767	50.260468
3503.436451	514485.049988	50.265473
3503.474334	514475.738007	50.270477
3503.250542	514466.113343	50.275482
3503.261163	514452.506646	50.280487
3503.054892	514453.702605	50.285492
3503.564875	514447.300013	50.290497
3503.413157	514439.939892	50.295501
3503.413331	514443.429750	50.300506
3503.604226	514445.169856	50.305511
3503.369746	514447.938150	50.310516
3503.118656	514446.106593	50.315521
3503.281903	514443.501475	50.320525
3503.511526	514444.830847	50.325530
3503.884769	514448.008855	50.330535
3503.389191	514458.455490	50.335540
3503.696511	514444.346702	50.340545
3503.427774	514417.634190	50.345549
3503.455394	514418.489723	50.350554
3503.577652	514398.189205	50.355559
3503.389541	514407.019394	50.360564
3503.657964	514412.894545	50.365569
3503.741370	514408.076663	50.370573
3503.050304	514411.979241	50.375578
3503.558819	514400.519185	50.380583
3503.118171	514387.590682	50.385588
3503.313512	514367.076267	50.390593
3503.446628	514358.507823	50.395597
3503.016729	514370.461439	50.400602
3503.568409	514356.617417	50.405607
3503.266096	514359.244716	50.410612
3503.411302	514365.291090	50.415617
3503.266413	514362.785239	50.420621
3503.116572	514372.216320	50.425626
3503.525835	514363.250194	50.430631
3503.575295	514365.214970	50.435636
3503.517765	514358.598581	50.440641
3503.388858	514366.711356	50.445645
3503.297301	514368.900728	50.450650
3503.278575	514354.792821	50.455655
3503.183193	514368.160298	50.460660
3503.569143	514363.800354	50.465665
3503.314438	514337.995882	50.470669
3503.532838	514345.244542	50.475674
3503.945331	514315.237847	50.480679
3503.300112	514322.825324	50.485684
3503.313047	514314.579314	50.490689
3503.705290	514314.618567	50.495693
3503.294260	514318.881521	50.500698
3503.126535	514314.558498	50.505703
3503.486205	514315.816749	50.510708
3503.250973	514319.090954	50.515713
3503.305605	514325.252812	50.520717
3503.570223	514309.026424	50.525722
3503.533736	514279.394090	50.530727
3503.081325	514281.438199	50.535732
3503.300251	514252.422951	50.540737
3503.356663	514222.320638	50.545741
3503.238984	514172.571154	50.550746
3503.277579	514121.330071	50.555751
3503.024635	514057.389300	50.560756
3503.149470	513981.249845	50.565761
3502.946962	513896.310578	50.570765
3502.709301	513800.350304	50.575770
3503.057324	513695.749076	50.580775
3502.199165	513586.128178	50.585780
3502.385786	513457.222338	50.590785
3502.310396	513330.734186	50.595789
3501.941094	513188.813928	50.600794
3501.943902	513044.861007	50.605799
3501.731057	512884.704334	50.610804
3501.473965	512713.374545	50.615809
3500.977513	512536.112128	50.620813
3500.615319	512363.480260	50.625818
3501.195856	512178.911681	50.630823
3500.333772	511982.479522	50.635828
3500.363386	511776.697739	50.640833
3499.950951	511570.629231	50.645837
3499.603809	511357.465874	50.650842
3499.375450	511118.228973	50.655847
3499.261531	510892.426847	50.660852
3498.944298	510655.170389	50.665857
3498.536743	510413.220153	50.670861
3498.281545	510152.271354	50.675866
3498.136741	509870.356735	50.680871
3497.453163	509607.747260	50.685876
3497.439013	509329.900968	50.690881
3497.436145	509051.744835	50.695885
3496.610063	508764.405092	50.700890
3496.272659	508469.697703	50.705895
3495.607561	508168.662049	50.710900
3495.628065	507869.030656	50.715905
3494.953807	507557.815941	50.720909
3494.361140	507249.011429	50.725914
3494.343399	506918.352973	50.730919
3493.590006	506604.198868	50.735924
3493.466748	506279.212095	50.740929
3493.334771	505950.020671	50.745933
3492.752411	505607.889290	50.750938
3492.390497	505253.773843	50.755943
3491.480544	504908.037034	50.760948
3491.310225	504553.674694	50.765953
3490.901584	504198.178895	50.770957
3490.357742	503840.774160	50.775962
3490.322311	503457.774858	50.780967
3489.304682	503092.838449	50.785972
3488.940258	502716.909839	50.790977
3488.331276	502329.674736	50.795981
3488.025552	501949.671546	50.800986
3487.633006	501563.802654	50.805991
3486.882287	501174.135204	50.810996
3486.443885	500778.285229	50.816001
3486.467619	500380.379315	50.821005
3485.437347	499981.163183	50.826010
3485.343920	499568.274484	50.831015
3484.707104	499150.754380	50.836020
3484.417814	498739.548060	50.841025
3483.440303	498315.835836	50.846029
3482.939086	497898.366461	50.851034
3482.449053	497474.405534	50.856039
3481.549306	497043.715385	50.861044
3481.093777	496618.463277	50.866049
3480.229125	496190.025584	50.871053
3479.789458	495764.497838	50.876058
3479.209274	495330.577464	50.881063
3478.696067	494899.977983	50.886068
3478.060570	494470.096583	50.891073
3477.512525	494028.342560	50.896077
3476.662978	493590.372697	50.901082
3476.376856	493143.087239	50.906087
3475.470907	492712.397301	50.911092
3475.045073	492267.543408	50.916097
3474.601921	491822.023233	50.921101
3473.644120	491382.549572	50.926106
3473.448170	490919.598196	50.931111
3472.892679	490474.620603	50.936116
3471.882109	490020.790563	50.941121
3471.442833	489564.681364	50.946125
3470.587979	489108.576123	50.951130
3470.234526	488650.658456	50.956135
3469.355970	488201.676670	50.961140
3468.907731	487730.683594	50.966145
3468.214949	487274.711016	50.971149
3467.326659	486815.820389	50.976154
3466.771296	486354.890462	50.981159
3466.145796	485893.555215	50.986164
3465.461643	485449.239443	50.991169
3464.717997	484978.579587	50.996173
3464.027444	484519.602532	51.001178
3463.710781	484046.521928	51.006183
3462.784226	483600.732503	51.011188
3461.913204	483134.759417	51.016193
3461.322975	482671.010699	51.021197
3460.513735	482214.328267	51.026202
3460.181073	481744.943332	51.031207
3459.285491	481295.650594	51.036212
3458.746715	480819.182228	51.041217
3457.973302	480356.370149	51.046221
3457.204725	479897.954965	51.051226
3457.031267	479432.695324	51.056231
3456.420519	478970.027617	51.061236
3455.474522	478490.830752	51.066241
3454.974095	478019.609673	51.071245
3454.196443	477559.165235	51.076250
3453.615876	477092.901425	51.081255
3452.979367	476617.715600	51.086260
3452.204364	476157.086342	51.091265
3451.157522	475684.528058	51.096269
3450.367032	475221.751053	51.101274
3449.971702	474754.035062	51.106279
3448.748923	474298.046475	51.111284
3448.211545	473831.294652	51.116289
3447.975700	473370.415128	51.121293
3447.149523	472915.549319	51.126298
3446.377359	472448.802879	51.131303
3445.375512	471987.303487	51.136308
3445.159640	471524.351390	51.141313
3444.168311	471060.548229	51.146317
3443.620037	470594.535313	51.151322
3443.075035	470137.180674	51.156327
3441.915503	469678.240005	51.161332
3441.130792	469216.340016	51.166337
3440.881451	468759.820847	51.171341
3440.248254	468314.912464	51.176346
3439.300858	467850.777011	51.181351
3438.810764	467389.398419	51.186356
3437.934658	466932.786322	51.191361
3437.074743	466476.973056	51.196365
3436.258595	466020.686645	51.201370
3436.024482	465563.284191	51.206375
3435.097296	465114.804959	51.211380
3434.681492	464647.878023	51.216385
3434.039269	464198.370899	51.221389
3432.896278	463738.283706	51.226394
3432.672178	463285.039917	51.231399
3431.872216	462834.362640	51.236404
3431.107309	462377.736554	51.241409
3430.153670	461927.013856	51.246413
3429.316007	461470.836535	51.251418
3429.018630	461017.252329	51.256423
3427.806130	460575.874834	51.261428
3427.340226	460121.639215	51.266433
3426.384350	459666.457146	51.271437
3425.446360	459227.545107	51.276442
3424.989854	458774.598845	51.281447
3424.087322	458343.373689	51.286452
3423.549721	457903.509569	51.291457
3422.978227	457463.743505	51.296461
3422.369420	457025.141367	51.301466
3421.856255	456572.006710	51.306471
3420.820952	456143.600569	51.311476
3420.397087	455702.000723	51.316481
3419.490987	455257.272229	51.321485
3418.746870	454812.357099	51.326490
3418.123550	454376.495599	51.331495
3417.238467	453944.573706	51.336500
3416.637273	453504.632996	51.341505
3415.781710	453070.406582	51.346509
3415.180179	452642.068127	51.351514
3414.673038	452200.768066	51.356519
3413.787950	451770.174761	51.361524
3413.071866	451331.275743	51.366529
3412.346280	450908.049280	51.371533
3411.545467	450476.048289	51.376538
3410.846414	450050.924353	51.381543
3410.071733	449617.634541	51.386548
3409.635840	449192.148738	51.391553
3408.983409	448756.844401	51.396557
3408.030655	448332.997750	51.401562
3407.517306	447895.168661	51.406567
3406.588040	447472.774409	51.411572
3405.982628	447051.691619	51.416577
3405.371119	446625.933075	51.421581
3404.517853	446201.372375	51.426586
3403.782077	445779.779937	51.431591
3403.269501	445360.124133	51.436596
3402.487692	444945.020717	51.441601
3401.929473	444517.337880	51.446605
3401.069073	444098.577682	51.451610
3400.580926	443670.411787	51.456615
3399.951429	443255.204166	51.461620
3399.051339	442826.377724	51.466625
3398.628009	442409.803165	51.471629
3397.407548	441986.799192	51.476634
3397.072324	441567.404302	51.481639
3396.350721	441153.545718	51.486644
3395.647292	440732.722509	51.491649
3394.907981	440316.923476	51.496653
3394.320958	439905.763780	51.501658
3393.944217	439471.160378	51.506663
3392.679059	439047.325635	51.511668
3391.857341	438638.111036	51.516673
3391.364720	438225.359917	51.521677
3390.763339	437814.167619	51.526682
3390.214494	437399.939324	51.531687
3389.205744	436986.589212	51.536692
3388.608104	436565.957504	51.541697
3388.140938	436143.774889	51.546701
3386.964290	435750.131134	51.551706
3386.495308	435326.919600	51.556711
3385.832801	434927.418692	51.561716
3384.879921	434516.481779	51.566721
3384.740546	434099.697071	51.571725
3383.454494	433698.218895	51.576730
3382.919142	433283.870047	51.581735
3382.014966	432881.430007	51.586740
3381.170220	432481.640260	51.591745
3380.715812	432080.055991	51.596749
3379.978180	431683.740863	51.601754
3379.478255	431271.105971	51.606759
3378.713526	430866.834997	51.611764
3377.579578	430475.413943	51.616769
3377.132063	430077.022383	51.621773
3376.537918	429680.019166	51.626778
3375.951999	429276.253909	51.631783
3375.083251	428885.401953	51.636788
3374.583738	428487.375363	51.641793
3373.894155	428077.488042	51.646797
3373.127498	427697.090400	51.651802
3372.700923	427296.113904	51.656807
3371.884384	426899.586525	51.661812
3371.141629	426503.244751	51.666817
3370.633666	426104.777443	51.671821
3369.718344	425704.235268	51.676826
3369.138235	425304.396042	51.681831
3368.246600	424911.635345	51.686836
3367.742570	424517.359951	51.691841
3366.932327	424117.056975	51.696845
3366.087824	423737.047279	51.701850
3365.485143	423338.554147	51.706855
3364.989023	422946.870863	51.711860
3364.095752	422559.181781	51.716865
3363.489790	422161.256233	51.721869
3362.679688	421782.306180	51.726874
3362.167556	421388.977581	51.731879
3361.204508	421012.174845	51.736884
3360.466337	420612.190377	51.741889
3360.093641	420226.469200	51.746893
3359.031398	419841.232763	51.751898
3358.446703	419451.622419	51.756903
3357.876737	419071.327320	51.761908
3357.102112	418688.671504	51.766913
3356.652661	418304.790497	51.771917
3355.762673	417923.006279	51.776922
3354.805426	417536.883368	51.781927
3353.965778	417161.076427	51.786932
3353.307492	416786.252062	51.791937
3353.181697	416402.192560	51.796941
3352.127751	416028.538684	51.801946
3351.683922	415648.203244	51.806951
3351.046387	415269.163746	51.811956
3350.422866	414885.975725	51.816961
3349.657591	414516.448761	51.821965
3348.878002	414133.834444	51.826970
3348.654746	413742.513834	51.831975
3347.825981	413365.486963	51.836980
3346.937296	412988.185218	51.841985
3346.209901	412597.360977	51.846989
3345.755304	412227.069919	51.851994
3345.121715	411843.386263	51.856999
3344.149474	411456.752819	51.862004
3343.577504	411078.385606	51.867009
3342.829729	410705.834996	51.872013
3341.845044	410337.459175	51.877018
3341.684337	409950.068006	51.882023
3340.870568	409571.287975	51.887028
3340.063028	409201.421750	51.892033
3339.423280	408817.649429	51.897037
3338.753940	408454.689736	51.902042
3338.108250	408070.451476	51.907047
3337.456685	407698.915847	51.912052
3336.655084	407318.199774	51.917057
3336.136167	406949.327886	51.922061
3335.257296	406579.466518	51.927066
3334.867316	406186.625085	51.932071
3334.197239	405826.734923	51.937076
3333.627671	405449.262967	51.942081
3332.945084	405069.135697	51.947085
3332.108370	404692.992992	51.952090
3331.424327	404308.764787	51.957095
3330.521430	403949.448918	51.962100
3329.971052	403566.969630	51.967105
3329.273587	403201.207784	51.972109
3328.214371	402823.934151	51.977114
3327.799768	402441.902711	51.982119
3327.305469	402082.297673	51.987124
3326.542851	401708.420708	51.992129
3325.587800	401333.349730	51.997133
3324.725610	400971.248561	52.002138
3324.342167	400602.738320	52.007143
3323.685905	400232.157230	52.012148
3323.210557	399861.899160	52.017153
3322.360095	399497.873180	52.022157
3321.759143	399134.566272	52.027162
3321.281728	398769.354687	52.032167
3320.309843	398399.006017	52.037172
3319.580483	398031.106062	52.042177
3319.118081	397660.871880	52.047181
3318.449354	397287.742722	52.052186
3317.816520	396926.628148	52.057191
3317.107677	396563.081166	52.062196
3316.234844	396193.836153	52.067201
3315.877203	395821.709112	52.072205
3315.038493	395462.111199	52.077210
3314.229880	395081.581494	52.082215
3313.655373	394714.967905	52.087220
3312.763283	394352.188696	52.092225
3312.269837	393990.486644	52.097229
3311.389602	393636.952235	52.102234
3310.587989	393267.994529	52.107239
3310.013563	392917.734931	52.112244
3309.442754	392551.885694	52.117249
3309.296976	392179.354797	52.122253
3307.648849	391830.448955	52.127258
3307.380757	391463.065656	52.132263
3307.067840	391102.906565	52.137268
3306.019598	390744.792453	52.142273
3305.590545	390380.423530	52.147277
3304.813470	390018.623127	52.152282
3304.419320	389643.739787	52.157287
3303.683532	389288.943255	52.162292
3302.909004	388926.470170	52.167297
3302.498045	388556.841523	52.172301
3301.077665	388197.463659	52.177306
3300.385409	387834.279921	52.182311
3299.861187	387473.176514	52.187316
3299.108905	387119.403650	52.192321
3298.464164	386768.331235	52.197325
3297.949463	386406.096793	52.202330
3297.227714	386052.868151	52.207335
3296.422199	385708.982103	52.212340
3295.731840	385339.186765	52.217345
3295.367831	384978.135001	52.222349
3294.250267	384631.058566	52.227354
3293.963196	384270.394609	52.232359
3293.098335	383913.429746	52.237364
3292.530300	383567.578874	52.242369
3291.756568	383210.999780	52.247373
3291.192800	382856.800109	52.252378
3290.510728	382492.214104	52.257383
3289.347421	382144.994652	52.262388
3288.895606	381793.132496	52.267393
3288.604000	381438.113513	52.272397
3287.482228	381095.633827	52.277402
3287.080423	380733.758816	52.282407
3286.270790	380389.926358	52.287412
3285.326898	380037.769812	52.292417
3285.154129	379691.719405	52.297421
3284.362543	379348.383499	52.302426
3283.808444	378985.931218	52.307431
3282.595555	378634.313174	52.312436
3282.249781	378294.407459	52.317441
3281.845941	377922.383504	52.322445
3280.707821	377582.037385	52.327450
3280.044464	377232.202107	52.332455
3279.850830	376887.452907	52.337460
3278.802523	376538.740713	52.342465
3278.188427	376190.770757	52.347469
3277.565674	375843.282442	52.352474
3276.815507	375501.127532	52.357479
3276.157621	375150.001361	52.362484
3275.208408	374801.004063	52.367489
3274.659267	374456.417452	52.372493
3273.881476	374119.495341	52.377498
3272.886724	373768.741229	52.382503
3272.451090	373429.800630	52.387508
3272.015806	373087.804616	52.392513
3271.388919	372750.440418	52.397517
3270.518676	372403.216379	52.402522
3269.954978	372062.402402	52.407527
3269.274377	371729.337578	52.412532
3268.439671	371377.596706	52.417537
3268.128505	371035.920395	52.422541
3267.329878	370695.259688	52.427546
3266.368755	370348.643598	52.432551
3265.841743	370011.063535	52.437556
3265.177738	369669.966288	52.442561
3264.953301	369323.937685	52.447565
3263.902243	368991.647762	52.452570
3263.433141	368637.765768	52.457575
3262.850905	368297.306185	52.462580
3261.999196	367960.041266	52.467585
3261.355448	367608.519112	52.472589
3260.537056	367276.408254	52.477594
3260.073322	366922.638717	52.482599
3259.561560	366579.712229	52.487604
3258.705531	366243.350740	52.492609
3258.083153	365896.772799	52.497613
3257.124539	365557.242059	52.502618
3256.740604	365212.147652	52.507623
3256.009385	364863.034656	52.512628
3255.158621	364526.328687	52.517633
3254.816260	364178.293841	52.522637
3253.646490	363838.351038	52.527642
3253.407042	363504.390486	52.532647
3252.706937	363168.210416	52.537652
3252.060303	362826.854281	52.542657
3251.747363	362475.341459	52.547661
3250.671773	362135.574736	52.552666
3249.971446	361791.547805	52.557671
3249.208239	361448.647862	52.562676
3248.349514	361103.877591	52.567681
3247.986054	360761.952657	52.572685
3247.618330	360434.707922	52.577690
3246.747644	360079.015998	52.582695
3245.803631	359740.916048	52.587700
3244.966228	359408.751197	52.592705
3244.670922	359072.274245	52.597709
3243.508357	358731.708047	52.602714
3243.145838	358385.236551	52.607719
3242.522995	358057.227147	52.612724
3241.631255	357725.924541	52.617729
3240.998128	357383.814709	52.622733
3240.452342	357049.653650	52.627738
3239.743383	356708.085520	52.632743
3239.069936	356373.380253	52.637748
3238.736089	356046.685938	52.642753
3238.238812	355695.916222	52.647757
3237.301336	355363.205453	52.652762
3236.634104	355017.216677	52.657767
3235.890299	354676.683606	52.662772
3235.139824	354340.577360	52.667777
3234.526093	354002.640415	52.672781
3233.406205	353663.305278	52.677786
3232.918909	353335.370808	52.682791
3232.210829	353004.567978	52.687796
3231.496176	352667.936178	52.692801
3230.929660	352332.424005	52.697805
3230.080841	352012.071458	52.702810
3229.432343	351673.794034	52.707815
3228.549724	351339.598034	52.712820
3227.859388	351015.447781	52.717825
3227.464478	350692.266838	52.722829
3226.688813	350367.897106	52.727834
3226.339648	350034.804737	52.732839
3225.755364	349702.256526	52.737844
3224.985039	349367.292418	52.742849
3224.370848	349033.319597	52.747853
3222.952040	348713.037539	52.752858
3222.932729	348375.505244	52.757863
3222.410269	348040.926508	52.762868
3221.644747	347717.048472	52.767873
3220.876445	347382.860994	52.772877
3220.072904	347055.956371	52.777882
3219.493358	346720.717013	52.782887
3218.662674	346401.473989	52.787892
3218.158440	346075.330821	52.792897
3217.727050	345742.429330	52.797901
3216.892429	345420.330750	52.802906
3216.367879	345076.342745	52.807911
3215.629552	344749.872747	52.812916
3214.715210	344420.348926	52.817921
3214.640572	344090.232251	52.822925
3213.699981	343755.643632	52.827930
3213.308084	343423.588036	52.832935
3212.079689	343093.622848	52.837940
3211.478160	342751.975144	52.842945
3211.210718	342427.199570	52.847949
3210.171029	342092.464559	52.852954
3209.494199	341767.648380	52.857959
3208.977951	341437.052355	52.862964
3207.970287	341107.525009	52.867969
3207.337623	340765.718302	52.872973
3206.679943	340452.346734	52.877978
3205.815160	340117.980526	52.882983
3205.595564	339797.179855	52.887988
3204.847354	339473.813821	52.892993
3204.541383	339133.550152	52.897997
3203.458213	338816.164839	52.903002
3202.936400	338480.793814	52.908007
3202.297145	338155.978301	52.913012
3201.402936	337819.517216	52.918017
3200.759406	337501.826732	52.923021
3199.911869	337170.471550	52.928026
3199.564338	336846.468819	52.933031
3198.742952	336524.143207	52.938036
3197.852875	336192.840724	52.943041
3197.474738	335872.274678	52.948045
3196.427405	335559.449995	52.953050
3195.787777	335230.216013	52.958055
3195.224751	334901.146500	52.963060
3194.567505	334579.040098	52.968065
3194.207892	334260.118157	52.973069
3193.043439	333932.157395	52.978074
3192.607984	333611.309673	52.983079
3192.047845	333293.687850	52.988084
3191.001615	332963.488975	52.993089
3190.189530	332652.446731	52.998093
3189.798516	332338.816154	53.003098
3189.256459	332017.825234	53.008103
3188.782260	331696.974877	53.013108
3188.069513	331383.874691	53.018113
3187.281371	331063.122081	53.023117
3186.351068	330744.299929	53.028122
3186.168492	330416.778513	53.033127
3185.430841	330093.442309	53.038132
3184.793043	329767.873963	53.043137
3184.267485	329437.092791	53.048141
3183.218788	329125.283572	53.053146
3182.336960	328801.913630	53.058151
3181.758494	328477.425011	53.063156
3181.171260	328159.912274	53.068161
3180.891337	327834.024325	53.073165
3179.869037	327523.324552	53.078170
3179.310014	327202.875527	53.083175
3178.410378	326887.596497	53.088180
3177.816062	326558.112153	53.093185
3177.003163	326233.320200	53.098189
3176.451847	325925.849359	53.103194
3175.744916	325609.134413	53.108199
3175.011292	325286.770236	53.113204
3174.081679	324979.712054	53.118209
3173.778580	324667.512394	53.123213
3172.785852	324357.584803	53.128218
3172.338646	324040.186112	53.133223
3171.555440	323729.204574	53.138228
3170.779099	323423.618505	53.143233
3170.447626	323095.071458	53.148237
3169.737582	322784.405822	53.153242
3169.091612	322475.180199	53.158247
3168.411598	322166.391683	53.163252
3167.847664	321842.128610	53.168257
3167.283079	321522.014649	53.173261
3166.375637	321218.732951	53.178266
3165.521629	320891.966068	53.183271
3164.837044	320580.040852	53.188276
3164.136591	320271.325246	53.193281
3163.692686	319952.154039	53.198285
3163.169585	319646.896511	53.203290
3161.981369	319326.440443	53.208295
3161.788290	319016.850943	53.213300
3160.760827	318705.431818	53.218305
3160.393245	318390.622589	53.223309
3159.607870	318091.919763	53.228314
3159.186653	317769.350872	53.233319
3158.510996	317456.598795	53.238324
3157.495015	317146.776826	53.243329
3156.902936	316835.588182	53.248333
3156.265009	316528.836334	53.253338
3155.741457	316214.859400	53.258343
3154.804359	315905.530242	53.263348
3154.342646	315601.421232	53.268353
3153.994821	315280.716719	53.273357
3152.844157	314977.402323	53.278362
3152.403825	314661.752207	53.283367
3151.873290	314343.238014	53.288372
3151.291260	314040.874858	53.293377
3150.594726	313713.752849	53.298381
3149.658478	313411.418443	53.303386
3148.958883	313097.790743	53.308391
3148.248358	312784.316627	53.313396
3147.679680	312465.548119	53.318401
3147.461237	312144.584276	53.323405
3146.547148	311853.547963	53.328410
3146.049742	311523.408445	53.333415
3145.157278	311206.571834	53.338420
3144.304350	310889.193318	53.343425
3143.615279	310583.043217	53.348429
3142.927620	310266.553516	53.353434
3142.302473	309953.847255	53.358439
3141.388148	309651.244400	53.363444
3140.984264	309341.073394	53.368449
3140.384520	309022.096315	53.373453
3139.239585	308725.486299	53.378458
3138.297805	308419.701534	53.383463
3138.130028	308113.564339	53.388468
3137.302383	307817.945946	53.393473
3136.627233	307506.565340	53.398477
3136.079028	307202.345015	53.403482
3135.301267	306893.041781	53.408487
3134.766341	306594.598467	53.413492
3133.930223	306296.711418	53.418497
3133.566301	305986.652940	53.423501
3132.662740	305688.698766	53.428506
3132.128545	305387.909737	53.433511
3131.455658	305078.840223	53.438516
3130.730991	304772.477536	53.443521
3130.063516	304460.273483	53.448525
3129.416785	304165.254751	53.453530
3128.868732	303860.873859	53.458535
3128.107465	303558.232246	53.463540
3127.324492	303260.712047	53.468545
3127.128605	302951.766014	53.473549
3126.434856	302649.111784	53.478554
3125.602491	302334.917301	53.483559
3125.150785	302036.094331	53.488564
3124.264691	301723.154886	53.493569
3123.893414	301411.686760	53.498573
3122.928063	301108.384784	53.503578
3122.515979	300790.580769	53.508583
3121.606165	300489.000495	53.513588
3120.750547	300180.433290	53.518593
3120.755055	299870.252332	53.523597
3119.440149	299567.028166	53.528602
3118.788923	299261.890296	53.533607
3118.455786	298957.058061	53.538612
3117.245342	298647.092512	53.543617
3117.072248	298340.272908	53.548621
3116.286451	298049.695578	53.553626
3115.592788	297741.352885	53.558631
3115.005414	297428.510684	53.563636
3113.985488	297134.811015	53.568641
3113.769824	296816.764635	53.573645
3112.754648	296507.681229	53.578650
3112.273157	296205.490797	53.583655
3111.363125	295910.065506	53.588660
3110.756124	295610.593486	53.593665
3110.379582	295297.103127	53.598669
3109.414086	295005.581693	53.603674
3109.033347	294692.778653	53.608679
3108.492834	294385.373985	53.613684
3107.161418	294089.095845	53.618689
3106.814614	293786.116395	53.623693
3105.890309	293489.671119	53.628698
3105.205613	293192.474435	53.633703
3104.876382	292898.226242	53.638708
3103.884610	292595.474532	53.643713
3103.468989	292280.024876	53.648717
3102.768843	291992.379325	53.653722
3102.446543	291680.072049	53.658727
3101.388132	291379.239358	53.663732
3100.490587	291086.504983	53.668737
3100.013042	290774.654056	53.673741
3099.150254	290481.658795	53.678746
3098.426121	290175.499961	53.683751
3098.061116	289895.108140	53.688756
3097.253262	289597.162468	53.693761
3096.368700	289290.493182	53.698765
3095.553282	289012.234611	53.703770
3095.102383	288713.696677	53.708775
3094.484644	288406.678594	53.713780
3093.747341	288128.101195	53.718785
3093.108124	287822.715848	53.723789
3092.475128	287540.097485	53.728794
3092.188292	287243.544088	53.733799
3091.337764	286943.437712	53.738804
3090.722177	286657.810605	53.743809
3090.333524	286353.351992	53.748813
3089.281274	286064.202509	53.753818
3088.290188	285762.538324	53.758823
3087.872713	285474.001015	53.763828
3086.911040	285179.539148	53.768833
3086.253488	284875.503872	53.773837
3085.790686	284595.708620	53.778842
3085.097481	284309.735422	53.783847
3084.510847	284020.688990	53.788852
3083.878183	283728.822687	53.793857
3083.419119	283427.607377	53.798861
3082.548243	283138.885505	53.803866
3082.103686	282845.358908	53.808871
3081.522130	282543.602123	53.813876
3080.322536	282252.563210	53.818881
3079.875859	281953.433430	53.823885
3078.817786	281670.114145	53.828890
3078.546846	281377.323304	53.833895
3078.012145	281084.115633	53.838900
3076.953948	280782.713484	53.843905
3076.627547	280485.626864	53.848909
3075.841406	280201.117805	53.853914
3075.166229	279899.298096	53.858919
3074.382127	279607.300805	53.863924
3073.323741	279318.861444	53.868929
3073.080299	279031.133468	53.873933
3072.316759	278749.651049	53.878938
3071.640787	278454.121633	53.883943
3071.130556	278165.544230	53.888948
3070.038054	277885.310651	53.893953
3069.745921	277590.611653	53.898957
3068.879662	277313.372879	53.903962
3068.357496	277017.665962	53.908967
3067.621623	276729.022085	53.913972
3066.946602	276452.924445	53.918977
3066.608535	276164.115655	53.923981
3065.487492	275876.092926	53.928986
3064.742010	275596.364363	53.933991
3064.366793	275306.440761	53.938996
3063.798617	275026.225670	53.944001
3063.200785	274733.535752	53.949005
3062.591562	274443.598218	53.954010
3061.965049	274151.473140	53.959015
3061.126291	273861.062575	53.964020
3060.528730	273578.712798	53.969025
3059.975146	273285.888573	53.974029
3059.085099	273003.814346	53.979034
3058.378511	272713.179206	53.984039
3057.818746	272422.801018	53.989044
3057.013961	272142.165102	53.994049
3056.392298	271850.319636	53.999053
3055.778034	271566.826678	54.004058
3054.989551	271281.705909	54.009063
3054.493765	270992.209260	54.014068
3053.378185	270715.035583	54.019073
3053.283640	270425.144488	54.024077
3052.419510	270147.421800	54.029082
3051.479211	269865.254294	54.034087
3050.931729	269577.778234	54.039092
3050.171222	269291.965962	54.044097
3049.645553	269004.257440	54.049101
3048.985252	268730.654302	54.054106
3048.548232	268446.166444	54.059111
3047.949246	268154.114799	54.064116
3046.533983	267876.276424	54.069121
3046.495183	267586.479460	54.074125
3045.486624	267311.302079	54.079130
3045.163891	267022.110637	54.084135
3044.420948	266731.203083	54.089140
3043.672343	266460.238178	54.094145
3043.117044	266173.325214	54.099149
3042.488233	265894.344650	54.104154
3041.622501	265607.837710	54.109159
3040.867225	265328.087990	54.114164
3039.916354	265048.853297	54.119169
3039.609014	264762.869758	54.124173
3039.077855	264492.406430	54.129178
3038.246359	264219.673225	54.134183
3037.638065	263929.841290	54.139188
3036.554517	263659.287685	54.144193
3036.020144	263369.750093	54.149197
3035.662758	263088.971172	54.154202
3034.996996	262814.328123	54.159207
3034.680167	262528.245892	54.164212
3034.017742	262251.081437	54.169217
3033.338595	261963.936443	54.174221
3032.201887	261692.628741	54.179226
3031.737276	261393.938818	54.184231
3031.390310	261116.954620	54.189236
3029.874064	260841.072589	54.194241
3029.650419	260548.814177	54.199245
3028.620981	260280.292211	54.204250
3028.026000	260001.922119	54.209255
3027.780252	259724.872283	54.214260
3026.632160	259453.874051	54.219265
3026.346474	259167.331654	54.224269
3025.640099	258894.404932	54.229274
3025.172819	258609.903826	54.234279
3024.172310	258329.154766	54.239284
3023.481395	258054.902176	54.244289
3023.224099	257781.498085	54.249293
3022.348403	257503.404294	54.254298
3021.500538	257220.365732	54.259303
3021.095120	256934.252322	54.264308
3019.886091	256670.550436	54.269313
3019.555426	256385.342700	54.274317
3018.871714	256114.733056	54.279322
3018.123290	255834.329072	54.284327
3017.637714	255568.782198	54.289332
3016.933999	255298.227665	54.294337
3016.445885	255010.678189	54.299341
3015.610361	254729.831030	54.304346
3014.952824	254455.552069	54.309351
3014.403488	254176.901476	54.314356
3013.243127	253898.857328	54.319361
3012.868674	253625.171369	54.324365
3012.007054	253357.420315	54.329370
3011.041304	253076.545163	54.334375
3010.845731	252809.962794	54.339380
3010.090474	252550.727457	54.344385
3009.733780	252269.706169	54.349389
3008.804720	251998.860767	54.354394
3007.685233	251733.393935	54.359399
3007.023064	251459.909486	54.364404
3006.706306	251190.292656	54.369409
3006.005081	250914.192166	54.374413
3005.206214	250652.980078	54.379418
3004.726221	250378.449826	54.384423
3004.022460	250108.106485	54.389428
3003.682255	249848.809425	54.394433
3002.543223	249567.636201	54.399437
3002.260292	249306.701076	54.404442
3001.673491	249031.960765	54.409447
3001.285536	248760.525537	54.414452
2999.981382	248487.427696	54.419457
2999.431232	248205.730720	54.424461
2999.191224	247935.903339	54.429466
2998.396414	247670.518964	54.434471
2997.707844	247395.517514	54.439476
2996.749485	247119.413300	54.444481
2995.920037	246837.177350	54.449485
2995.416615	246581.196667	54.454490
2994.338779	246317.158267	54.459495
2993.861479	246041.158191	54.464500
2993.342731	245772.473897	54.469505
2992.804176	245503.538589	54.474509
2992.224806	245239.066756	54.479514
2991.078112	244972.215060	54.484519
2991.008935	244695.185321	54.489524
2989.999000	244431.114244	54.494529
2989.298959	244162.232573	54.499533
2988.668934	243897.618555	54.504538
2988.266335	243636.483289	54.509543
2987.188501	243370.031303	54.514548
2986.808379	243098.809258	54.519553
2986.314991	242824.549877	54.524557
2985.573141	242555.372522	54.529562
2984.745589	242289.952679	54.534567
2984.329744	242019.909964	54.539572
2983.592905	241742.533780	54.544577
2982.964148	241469.750267	54.549581
2982.383975	241212.264091	54.554586
2981.368029	240934.730182	54.559591
2980.689610	240677.948237	54.564596
2979.848305	240408.205590	54.569601
2979.496344	240137.240175	54.574605
2978.945879	239873.233187	54.579610
2978.153936	239607.533424	54.584615
2977.887399	239330.724946	54.589620
2976.820136	239072.378309	54.594625
2976.488026	238794.053626	54.599629
2975.571199	238524.047171	54.604634
2975.084640	238255.297389	54.609639
2974.170284	237972.737962	54.614644
2973.343959	237711.275111	54.619649
2972.785447	237443.124347	54.624653
2972.192203	237189.774347	54.629658
2971.209989	236918.025116	54.634663
2970.734139	236646.323725	54.639668
2969.978663	236387.883029	54.644673
2969.737647	236122.257113	54.649677
2968.865619	235860.118430	54.654682
2968.055727	235583.278023	54.659687
2967.567638	235322.582255	54.664692
2966.892526	235062.196845	54.669697
2966.144042	234784.381224	54.674701
2965.469927	234528.173014	54.679706
2964.497491	234261.878263	54.684711
2964.305777	233998.490745	54.689716
2963.122626	233730.601101	54.694721
2962.453877	233460.619150	54.699725
2961.814127	233216.682069	54.704730
2960.892841	232949.847985	54.709735
2960.669970	232690.186459	54.714740
2959.736431	232433.108030	54.719745
2959.404146	232173.439741	54.724749
2958.193640	231919.971315	54.729754
2957.656317	231661.457229	54.734759
2957.310290	231396.777072	54.739764
2956.434714	231147.739096	54.744769
2955.923323	230885.250867	54.749773
2955.416565	230632.769360	54.754778
2954.642975	230368.541726	54.759783
2954.034672	230112.334750	54.764788
2953.204132	229856.876613	54.769793
2953.053131	229586.696358	54.774797
2952.230663	229327.215414	54.779802
2951.300472	229070.222079	54.784807
2951.002328	228806.152861	54.789812
2949.968421	228550.628764	54.794817
2949.695151	228272.833272	54.799821
2948.881532	228028.351661	54.804826
2947.967378	227758.450521	54.809831
2947.422253	227494.831708	54.814836
2946.540368	227237.199522	54.819841
2946.214831	226978.105112	54.824845
2945.258782	226725.705775	54.829850
2944.720739	226462.725530	54.834855
2944.063867	226193.221404	54.839860
2943.044979	225935.843984	54.844865
2942.838252	225676.391007	54.849869
2941.841267	225426.815468	54.854874
2941.244500	225167.120295	54.859879
2940.833541	224908.274916	54.864884
2939.492978	224648.597290	54.869889
2939.338871	224402.086716	54.874893
2938.847684	224139.386462	54.879898
2938.374331	223881.814506	54.884903
2937.577731	223622.397756	54.889908
2936.714745	223362.101246	54.894913
2936.608332	223095.651746	54.899917
2935.837072	222842.611288	54.904922
2934.815335	222566.353595	54.909927
2934.331871	222303.963677	54.914932
2933.897374	222044.278357	54.919937
2932.823834	221774.689405	54.924941
2932.184100	221516.527738	54.929946
2931.691068	221254.792102	54.934951
2930.810046	220994.799112	54.939956
2930.373231	220736.760700	54.944961
2929.647651	220475.713768	54.949965
2929.057142	220223.671643	54.954970
2928.009258	219953.728636	54.959975
2927.465809	219689.638692	54.964980
2927.066480	219431.547905	54.969985
2926.391777	219163.407181	54.974989
2925.481475	218907.512208	54.979994
2924.858540	218642.878494	54.984999
2924.259105	218388.018111	54.990004
2923.374074	218136.717110	54.995009
2922.535439	217864.915624	55.000013
2922.015385	217622.774565	55.005018
2921.562938	217358.869569	55.010023
2920.902150	217093.649254	55.015028
2919.907552	216846.443420	55.020033
2919.525241	216596.022909	55.025037
2918.427621	216334.782395	55.030042
2917.890477	216087.061284	55.035047
2917.243611	215833.554075	55.040052
2916.444573	215590.687692	55.045057
2915.874076	215316.638748	55.050061
2915.355473	215068.574659	55.055066
2914.745707	214812.443211	55.060071
2914.006035	214552.756555	55.065076
2913.110219	214309.108126	55.070081
2912.602333	214054.910865	55.075085
2912.154732	213801.379623	55.080090
2911.282834	213537.899262	55.085095
2910.446629	213287.142642	55.090100
2909.798394	213042.084943	55.095105
2909.474370	212791.007259	55.100109
2908.175944	212533.606150	55.105114
2907.709036	212295.497567	55.110119
2907.446990	212036.852414	55.115124
2906.492410	211785.916592	55.120129
2905.863561	211541.141436	55.125133
2905.269762	211291.155915	55.130138
2904.449128	211037.045249	55.135143
2904.053814	210788.786702	55.140148
2903.139051	210541.209572	55.145153
2902.667987	210285.493743	55.150157
2902.450678	210035.962618	55.155162
2901.605439	209791.444782	55.160167
2901.098971	209529.526509	55.165172
2900.207429	209279.570573	55.170177
2899.501516	209010.482245	55.175181
2898.901956	208757.313018	55.180186
2898.276930	208513.121679	55.185191
2898.056787	208262.236241	55.190196
2896.710106	208001.921084	55.195201
2896.332957	207736.273526	55.200205
2895.563646	207492.719994	55.205210
2894.817650	207239.682021	55.210215
2894.338639	206978.432035	55.215220
2893.552822	206713.286377	55.220225
2892.855366	206466.111120	55.225229
2891.966184	206217.096381	55.230234
2891.524913	205966.102726	55.235239
2891.034616	205705.598228	55.240244
2890.403810	205460.160161	55.245249
2889.621859	205194.244311	55.250253
2888.847522	204946.413034	55.255258
2888.328366	204684.924934	55.260263
2887.587990	204430.383545	55.265268
2886.589609	204183.087317	55.270273
2886.264998	203927.998688	55.275277
2885.473209	203676.408555	55.280282
2884.592484	203432.316682	55.285287
2883.938463	203176.125447	55.290292
2883.529688	202925.725130	55.295297
2882.967006	202669.750774	55.300301
2882.008496	202415.660082	55.305306
2881.360396	202164.384738	55.310311
2880.900004	201918.502060	55.315316
2880.260944	201669.289103	55.320321
2879.479137	201414.615008	55.325325
2878.692854	201172.401357	55.330330
2878.160106	200915.844860	55.335335
2877.853849	200672.055740	55.340340
2876.887413	200418.077187	55.345345
2876.407642	200156.234685	55.350349
2875.700296	199916.037410	55.355354
2875.215392	199656.310548	55.360359
2874.377770	199410.040630	55.365364
2873.414499	199154.464043	55.370369
2872.866756	198903.034935	55.375373
2872.410829	198653.603046	55.380378
2871.484521	198400.632850	55.385383
2870.816058	198141.260463	55.390388
2870.136444	197895.010626	55.395393
2869.681770	197647.479259	55.400397
2868.984271	197400.623745	55.405402
2867.928991	197148.468868	55.410407
2867.781832	196894.860737	55.415412
2866.891772	196650.024300	55.420417
2866.330343	196395.453478	55.425421
2865.701459	196146.086227	55.430426
2865.024994	195897.007645	55.435431
2864.505907	195636.249691	55.440436
2863.586919	195396.233596	55.445441
2863.238166	195129.992438	55.450445
2862.374837	194884.396638	55.455450
2861.608359	194633.162558	55.460455
2861.066395	194378.751285	55.465460
2859.970796	194134.264707	55.470465
2859.568526	193878.586852	55.475469
2858.846397	193631.994982	55.480474
2858.224049	193374.687683	55.485479
2857.880520	193130.799408	55.490484
2856.798947	192878.338830	55.495489
2856.485987	192628.455246	55.500493
2855.747901	192378.360316	55.505498
2854.849162	192132.974380	55.510503
2854.210473	191875.270246	55.515508
2853.602373	191627.283360	55.520513
2852.991353	191377.427842	55.525517
2852.680868	191138.302693	55.530522
2851.819529	190886.046436	55.535527
2851.622344	190630.200141	55.540532
2850.371655	190383.402797	55.545537
2849.852728	190125.676190	55.550541
2849.242735	189874.301450	55.555546
2848.376000	189614.520629	55.560551
2847.835435	189362.514143	55.565556
2846.949965	189128.617304	55.570561
2846.397938	188856.831290	55.575565
2845.650542	188612.138939	55.580570
2844.888646	188359.193157	55.585575
2844.432163	188112.078186	55.590580
2843.435359	187874.350222	55.595585
2843.024801	187616.861737	55.600589
2842.319285	187366.062447	55.605594
2841.290095	187135.238879	55.610599
2840.954140	186881.241258	55.615604
2840.114627	186637.629721	55.620609
2839.505950	186386.871255	55.625613
2838.864362	186152.607109	55.630618
2838.443932	185901.923238	55.635623
2837.563430	185652.433119	55.640628
2836.950673	185404.733898	55.645633
2836.227511	185162.472970	55.650637
2835.756911	184922.959380	55.655642
2834.829532	184669.589215	55.660647
2834.174163	184423.504999	55.665652
2833.314665	184190.735677	55.670657
2832.935905	183947.485302	55.675661
2832.077716	183698.892874	55.680666
2831.064923	183455.338490	55.685671
2830.973193	183211.092552	55.690676
2830.076043	182971.809534	55.695681
2829.304461	182732.457033	55.700685
2829.045574	182487.707247	55.705690
2828.074196	182245.679441	55.710695
2827.982614	182010.662751	55.715700
2826.562229	181768.250724	55.720705
2826.502405	181512.827515	55.725709
2825.478495	181275.494590	55.730714
2824.675765	181035.532927	55.735719
2824.476186	180787.844756	55.740724
2823.511741	180552.376265	55.745729
2822.798247	180306.947421	55.750733
2822.358052	180066.806490	55.755738
2821.234193	179819.143035	55.760743
2821.082060	179575.143154	55.765748
2820.470178	179340.757531	55.770753
2819.561148	179086.869598	55.775757
2818.882207	178841.392768	55.780762
2818.152841	178608.098246	55.785767
2817.702083	178363.847300	55.790772
2817.013312	178124.468948	55.795777
2816.389645	177879.014369	55.800781
2815.801279	177638.007478	55.805786
2814.942235	177389.667527	55.810791
2814.553250	177142.513823	55.815796
2813.620112	176899.416196	55.820801
2813.221047	176656.209960	55.825805
2812.174691	176419.708926	55.830810
2811.552786	176181.704753	55.835815
2811.167111	175923.263174	55.840820
2810.209923	175693.353350	55.845825
2809.924418	175447.477954	55.850829
2809.194568	175207.461469	55.855834
2808.693320	174957.298773	55.860839
2808.230496	174708.734073	55.865844
2807.279972	174472.547011	55.870849
2806.645678	174218.734237	55.875853
2805.865259	173971.636091	55.880858
2805.307195	173728.256153	55.885863
2804.728653	173468.690544	55.890868
2803.679165	173235.171772	55.895873
2803.137817	172980.334594	55.900877
2802.343845	172739.961315	55.905882
2801.741730	172491.584921	55.910887
2801.223658	172247.457256	55.915892
2800.322945	172007.664878	55.920897
2799.943037	171761.966734	55.925901
2799.320076	171524.422478	55.930906
2798.424447	171276.952245	55.935911
2798.121019	171025.561799	55.940916
2797.084800	170779.592187	55.945921
2796.499643	170545.863067	55.950925
2795.840580	170304.503966	55.955930
2795.528742	170057.686553	55.960935
2794.708114	169807.428647	55.965940
2793.735458	169561.520219	55.970945
2793.112364	169317.312923	55.975949
2792.600048	169082.792593	55.980954
2791.675048	168836.474282	55.985959
2791.335749	168587.852070	55.990964
2790.658555	168348.835171	55.995969
2789.900288	168108.649963	56.000973
2788.806249	167864.793519	56.005978
2788.470370	167631.780076	56.010983
2788.140430	167379.069552	56.015988
2787.024759	167146.614944	56.020993
2786.492657	166901.836394	56.025997
2785.851264	166657.725256	56.031002
2784.927905	166423.489813	56.036007
2784.486484	166178.561712	56.041012
2783.916170	165940.712902	56.046017
2783.491298	165703.452918	56.051021
2783.041403	165461.302872	56.056026
2782.034750	165209.159129	56.061031
2781.483551	164962.514337	56.066036
2780.612911	164726.513713	56.071041
2779.880929	164479.977052	56.076045
2779.278327	164234.438761	56.081050
2778.530409	163986.254936	56.086055
2778.216886	163732.650934	56.091060
2777.387834	163436.827623	56.096065
2776.770815	163193.015084	56.101069
2775.994882	162947.652705	56.106074
2775.375406	162704.428695	56.111079
2774.870966	162461.900108	56.116084
2773.894229	162228.119265	56.121089
2773.083081	161967.537056	56.126093
2772.874193	161729.149609	56.131098
2771.897698	161492.512749	56.136103
2771.305609	161252.523578	56.141108
2770.611956	161012.844520	56.146113
2770.236086	160766.263867	56.151117
2769.363332	160523.539656	56.156122
2768.662447	160279.734622	56.161127
2768.246875	160031.639664	56.166132
2767.208027	159795.761300	56.171137
2766.425995	159547.791336	56.176141
2765.894040	159314.925283	56.181146
2764.936062	159075.504552	56.186151
2764.606766	158832.032016	56.191156
2763.894493	158592.944332	56.196161
2763.371763	158361.227314	56.201165
2762.536335	158112.385989	56.206170
2761.705856	157871.160731	56.211175
2761.446138	157634.944604	56.216180
2760.858016	157402.888337	56.221185
2760.237336	157159.117639	56.226189
2759.721095	156920.747696	56.231194
2758.718582	156672.108403	56.236199
2758.140759	156423.212943	56.241204
2757.249952	156181.564056	56.246209
2756.653420	155934.594658	56.251213
2755.918780	155696.127942	56.256218
2754.851356	155462.190260	56.261223
2754.773358	155220.660923	56.266228
2753.824817	154982.830530	56.271233
2753.237428	154746.584418	56.276237
2752.425278	154510.426398	56.281242
2751.774546	154277.028306	56.286247
2751.305022	154042.204847	56.291252
2750.354453	153803.086469	56.296257
2750.096400	153564.406680	56.301261
2749.295434	153327.073002	56.306266
2748.402465	153092.590176	56.311271
2748.230671	152850.342656	56.316276
2747.417160	152617.566571	56.321281
2746.448556	152369.957589	56.326285
2746.012473	152138.624950	56.331290
2745.261479	151906.174415	56.336295
2744.538072	151674.725281	56.341300
2743.860337	151436.381395	56.346305
2743.522417	151192.888491	56.351309
2742.675470	150954.193574	56.356314
2741.631850	150727.809697	56.361319
2741.379887	150488.756989	56.366324
2740.292899	150258.252401	56.371329
2739.895618	150019.772668	56.376333
2739.451077	149790.605838	56.381338
2738.808509	149554.405309	56.386343
2737.978920	149314.639259	56.391348
2737.322104	149082.422568	56.396353
2736.762796	148846.569866	56.401357
2736.043279	148621.903187	56.406362
2734.984830	148379.701959	56.411367
2734.717034	148131.950433	56.416372
2733.861961	147906.306179	56.421377
2733.022493	147666.464960	56.426381
2732.326774	147432.207439	56.431386
2731.626536	147201.027908	56.436391
2731.214522	146976.120681	56.441396
2730.109057	146746.711619	56.446401
2729.629915	146511.524224	56.451405
2729.508039	146285.584637	56.456410
2728.546313	146054.861526	56.461415
2727.931851	145820.857159	56.466420
2727.314693	145578.988527	56.471425
2726.698392	145357.848659	56.476429
2725.762451	145120.812322	56.481434
2724.974954	144890.413247	56.486439
2724.540598	144652.843495	56.491444
2724.082074	144429.245254	56.496449
2723.190989	144197.266505	56.501453
2722.796662	143958.831559	56.506458
2721.944032	143734.665347	56.511463
2721.483647	143494.401831	56.516468
2720.337268	143262.330714	56.521473
2719.930777	143034.794973	56.526477
2719.101828	142804.354358	56.531482
2718.553262	142565.598756	56.536487
2718.002148	142334.482285	56.541492
2717.155718	142123.630951	56.546497
2716.731269	141888.723825	56.551501
2716.117491	141643.098651	56.556506
2715.238805	141414.455270	56.561511
2714.763510	141180.476508	56.566516
2714.272034	140949.627872	56.571521
2713.395446	140707.762122	56.576525
2712.792945	140480.314507	56.581530
2712.143916	140253.536685	56.586535
2711.746913	140012.312043	56.591540
2710.914009	139786.075095	56.596545
2710.090303	139547.170710	56.601549
2709.492927	139308.842238	56.606554
2708.486485	139087.008791	56.611559
2708.071310	138852.581102	56.616564
2707.530086	138615.380028	56.621569
2706.527318	138383.602885	56.626573
2705.937067	138143.948492	56.631578
2705.059776	137928.417661	56.636583
2704.732470	137697.390085	56.641588
2704.238076	137466.009629	56.646593
2703.390770	137239.667172	56.651597
2702.845667	137002.720955	56.656602
2701.868485	136783.199587	56.661607
2701.618526	136549.488037	56.666612
2700.821473	136317.491179	56.671617
2699.871169	136077.402377	56.676621
2699.661164	135847.958718	56.681626
2698.411198	135620.955649	56.686631
2698.274295	135385.177386	56.691636
2697.087166	135160.492773	56.696641
2696.860894	134926.142509	56.701645
2695.927321	134697.241746	56.706650
2694.827386	134480.755163	56.711655
2694.597708	134249.688424	56.716660
2694.008455	134029.389471	56.721665
2693.277814	133785.549950	56.726669
2692.722613	133569.021994	56.731674
2692.015718	133352.748354	56.736679
2691.919478	133112.624949	56.741684
2690.712463	132882.321038	56.746689
2689.938465	132649.486029	56.751693
2689.544539	132421.991347	56.756698
2688.931659	132205.457406	56.761703
2688.093981	131971.634499	56.766708
2687.572792	131741.358149	56.771713
2686.881746	131508.671730	56.776717
2686.461929	131285.204147	56.781722
2685.558660	131052.669410	56.786727
2685.070862	130806.416120	56.791732
2684.394377	130593.207060	56.796737
2683.877753	130356.044114	56.801741
2683.096948	130117.248398	56.806746
2682.218969	129888.580555	56.811751
2681.904532	129650.769142	56.816756
2680.981437	129418.771790	56.821761
2680.259631	129183.073808	56.826765
2679.652312	128955.056568	56.831770
2678.954676	128723.003869	56.836775
2678.096749	128485.390087	56.841780
2677.602731	128253.651964	56.846785
2676.928597	128038.213942	56.851789
2676.182015	127799.216711	56.856794
2675.611296	127571.128822	56.861799
2674.861397	127332.771172	56.866804
2674.166477	127117.407117	56.871809
2673.640306	126888.504991	56.876813
2673.106308	126657.002490	56.881818
2672.154545	126421.389835	56.886823
2671.497779	126186.608756	56.891828
2671.001983	125966.421624	56.896833
2670.063872	125732.793898	56.901837
2669.805061	125505.105532	56.906842
2669.014823	125272.588579	56.911847
2668.025605	125042.213232	56.916852
2667.336298	124817.786362	56.921857
2666.951556	124583.445865	56.926861
2666.249543	124366.961697	56.931866
2665.452764	124136.220688	56.936871
2665.343888	123905.893308	56.941876
2664.453343	123689.571431	56.946881
2663.723096	123460.552687	56.951885
2663.001448	123220.397956	56.956890
2661.966157	122991.368054	56.961895
2661.486174	122767.420322	56.966900
2660.802196	122560.141390	56.971905
2660.598994	122316.788867	56.976909
2659.903016	122084.309894	56.981914
2658.620898	121860.801614	56.986919
2658.293392	121642.299239	56.991924
2657.480266	121412.523925	56.996929
2656.764426	121179.357648	57.001933
2656.214762	120945.951238	57.006938
2655.311360	120730.988624	57.011943
2655.014992	120503.056622	57.016948
2654.228759	120283.508102	57.021953
2653.506224	120064.294139	57.026957
2653.048361	119835.822139	57.031962
2652.144564	119617.097718	57.036967
2651.404797	119388.801248	57.041972
2650.704015	119171.241870	57.046977
2649.781949	118950.043746	57.051981
2649.304761	118716.924985	57.056986
2648.600210	118504.469340	57.061991
2648.333993	118277.421620	57.066996
2647.164558	118063.215004	57.072001
2646.346174	117846.567704	57.077005
2646.162929	117616.427517	57.082010
2645.358747	117403.425368	57.087015
2644.840310	117187.567628	57.092020
2644.121743	116968.728231	57.097025
2643.614877	116744.779004	57.102029
2642.791282	116517.206640	57.107034
2642.106532	116299.967177	57.112039
2641.522929	116080.383988	57.117044
2640.853793	115864.021703	57.122049
2640.024948	115635.632830	57.127053
2639.472479	115414.165249	57.132058
2638.659079	115200.116495	57.137063
2638.271742	114973.040960	57.142068
2637.795675	114760.319804	57.147073
2637.106870	114533.556199	57.152077
2636.222019	114307.707931	57.157082
2635.470285	114093.315994	57.162087
2635.342511	113872.226159	57.167092
2634.320068	113650.537438	57.172097
2633.934381	113425.392282	57.177101
2633.412788	113198.061989	57.182106
2632.261661	112977.104083	57.187111
2631.771463	112748.744709	57.192116
2630.695612	112531.954914	57.197121
2630.181989	112290.059734	57.202125
2629.423604	112072.607997	57.207130
2628.657608	111856.638085	57.212135
2628.393549	111632.708279	57.217140
2627.451813	111425.261436	57.222145
2626.753239	111193.287463	57.227149
2626.369837	110976.046081	57.232154
2625.456864	110768.422474	57.237159
2624.801114	110547.655106	57.242164
2624.172783	110326.212680	57.247169
2623.825396	110107.228048	57.252173
2622.882504	109887.762243	57.257178
2622.104771	109667.015735	57.262183
2621.846987	109441.784805	57.267188
2621.113311	109237.280521	57.272193
2620.569657	109012.048066	57.277197
2619.808357	108786.547579	57.282202
2618.729777	108563.383867	57.287207
2618.256082	108345.957903	57.292212
2617.361285	108125.986262	57.297217
2616.952054	107910.851032	57.302221
2616.306951	107692.265120	57.307226
2615.511294	107479.263537	57.312231
2615.030693	107253.466252	57.317236
2614.229116	107048.191585	57.322241
2613.541403	106824.417172	57.327245
2613.077535	106599.054810	57.332250
2612.214212	106393.693964	57.337255
2611.856069	106174.105495	57.342260
2611.139601	105946.149750	57.347265
2610.495272	105724.561323	57.352269
2609.939709	105510.549265	57.357274
2609.066832	105293.302818	57.362279
2608.452951	105068.974691	57.367284
2607.857362	104854.651256	57.372289
2606.901264	104635.920291	57.377293
2606.566696	104411.446217	57.382298
2605.675934	104199.338926	57.387303
2605.298016	103965.124493	57.392308
2604.165969	103758.445767	57.397313
2603.529165	103529.295035	57.402317
2603.120951	103318.368967	57.407322
2602.107953	103098.544589	57.412327
2602.097338	102879.819539	57.417332
2601.075980	102671.419858	57.422337
2600.298238	102453.448389	57.427341
2599.816976	102230.026923	57.432346
2598.783726	102017.048256	57.437351
2598.124748	101804.576810	57.442356
2597.597973	101588.533830	57.447361
2596.979989	101369.900036	57.452365
2596.350455	101153.687042	57.457370
2595.256425	100946.113499	57.462375
2595.059895	100728.142086	57.467380
2594.354875	100517.586343	57.472385
2593.627915	100304.454212	57.477389
2592.980999	100083.813508	57.482394
2592.202073	99873.383147	57.487399
2591.449073	99655.104006	57.492404
2590.945004	99446.194401	57.497409
2590.292424	99222.219941	57.502413
2589.856411	99006.364156	57.507418
2589.157642	98801.474672	57.512423
2588.528601	98583.331898	57.517428
2587.611822	98375.049228	57.522433
2587.146886	98159.041050	57.527437
2586.587652	97940.734738	57.532442
2585.802060	97723.506580	57.537447
2585.000609	97505.179376	57.542452
2584.254706	97292.566461	57.547457
2583.571736	97079.507916	57.552461
2583.292725	96860.863055	57.557466
2582.531736	96650.389581	57.562471
2581.924693	96434.172860	57.567476
2581.130581	96220.480359	57.572481
2580.496302	96007.208494	57.577485
2580.191354	95796.455019	57.582490
2579.355717	95577.200395	57.587495
2578.992271	95355.165011	57.592500
2577.884564	95139.667844	57.597505
2577.611956	94922.664190	57.602509
2576.882853	94692.220470	57.607514
2575.747537	94475.224670	57.612519
2575.062791	94260.544051	57.617524
2574.151121	94054.748084	57.622529
2573.626049	93838.834931	57.627533
2573.187716	93627.869208	57.632538
2572.662523	93414.033858	57.637543
2572.099407	93197.961695	57.642548
2571.127589	92982.793458	57.647553
2570.431296	92767.431440	57.652557
2570.082173	92552.656948	57.657562
2569.036533	92338.140765	57.662567
2568.698870	92120.464367	57.667572
2568.091500	91904.240565	57.672577
2567.231545	91696.841194	57.677581
2566.882223	91483.015552	57.682586
2566.131162	91261.450020	57.687591
2565.481524	91037.029951	57.692596
2564.654331	90824.637012	57.697601
2563.923571	90603.125602	57.702605
2563.355586	90381.311636	57.707610
2562.708282	90176.632009	57.712615
2561.940262	89972.011466	57.717620
2561.008900	89745.322261	57.722625
2560.282573	89541.009817	57.727629
2559.704072	89321.966300	57.732634
2559.004464	89118.655339	57.737639
2558.489156	88901.267176	57.742644
2557.811386	88695.040210	57.747649
2557.151230	88486.637759	57.752653
2556.639324	88266.624258	57.757658
2555.831284	88058.617070	57.762663
2554.970303	87843.494229	57.767668
2553.984111	87644.052750	57.772673
2553.409860	87441.872434	57.777677
2552.989085	87234.604252	57.782682
2552.209589	87025.486679	57.787687
2551.596939	86814.271642	57.792692
2550.976554	86619.181325	57.797697
2550.264506	86423.498714	57.802701
2549.782842	86192.274325	57.807706
2549.151161	85995.467138	57.812711
2548.761889	85776.309046	57.817716
2547.827424	85570.830894	57.822721
2547.098793	85362.608930	57.827725
2546.490361	85161.387327	57.832730
2545.712265	84947.079037	57.837735
2545.248146	84740.196788	57.842740
2544.581545	84527.859139	57.847745
2543.965183	84324.225228	57.852749
2543.633328	84107.946657	57.857754
2542.734582	83908.101375	57.862759
2541.721546	83686.673919	57.867764
2541.186983	83474.097686	57.872769
2540.475486	83270.140347	57.877773
2540.146968	83058.251887	57.882778
2539.122534	82856.015165	57.887783
2538.922336	82635.040345	57.892788
2537.861487	82428.313272	57.897793
2537.084444	82221.302395	57.902797
2536.491312	82011.437587	57.907802
2535.716215	81805.260798	57.912807
2535.203152	81589.055763	57.917812
2534.696015	81395.915892	57.922817
2533.962842	81182.779489	57.927821
2533.690421	80970.110945	57.932826
2532.549389	80767.475519	57.937831
2532.059138	80545.630690	57.942836
2531.611292	80344.974607	57.947841
2530.690512	80130.921700	57.952845
2530.394435	79922.703902	57.957850
2529.505746	79714.068787	57.962855
2528.613940	79503.256200	57.967860
2528.094807	79290.022861	57.972865
2527.509692	79069.976941	57.977869
2526.779934	78868.074345	57.982874
2525.861629	78661.640867	57.987879
2525.442552	78455.757695	57.992884
2524.794238	78246.060010	57.997889
2524.086842	78034.174904	58.002893
2523.380619	77823.660562	58.007898
2522.432848	77614.175207	58.012903
2522.043747	77409.381351	58.017908
2521.471238	77203.579393	58.022913
2520.693309	76996.208898	58.027917
2520.080117	76773.543282	58.032922
2519.189616	76575.319544	58.037927
2518.828985	76363.212993	58.042932
2518.055855	76164.302983	58.047937
2517.454198	75950.566129	58.052941
2516.879646	75740.362842	58.057946
2515.892057	75539.788485	58.062951
2515.284393	75329.518664	58.067956
2514.589098	75116.356669	58.072961
2513.816135	74915.355297	58.077965
2513.099787	74717.774679	58.082970
2512.702467	74516.698717	58.087975
2512.176561	74301.294575	58.092980
2511.373764	74104.069460	58.097985
2510.495551	73893.616698	58.102989
2510.084489	73688.255596	58.107994
2509.077749	73485.385843	58.112999
2508.360397	73283.093143	58.118004
2507.812551	73083.379464	58.123009
2507.090890	72891.399101	58.128013
2506.623708	72680.646819	58.133018
2506.202941	72485.619730	58.138023
2505.247933	72269.741559	58.143028
2504.880520	72077.415103	58.148033
2504.100298	71872.447884	58.153037
2503.157720	71665.398969	58.158042
2502.051210	71459.917572	58.163047
2501.751651	71250.845237	58.168052
2501.165574	71063.263677	58.173057
2500.816159	70865.675556	58.178061
2500.132910	70648.853364	58.183066
2499.272924	70450.488806	58.188071
2498.706174	70241.811528	58.193076
2498.291061	70046.433732	58.198081
2497.644073	69834.986317	58.203085
2497.008517	69638.253944	58.208090
2496.154008	69429.117794	58.213095
2495.855455	69222.321724	58.218100
2494.874055	69018.309065	58.223105
2494.099124	68814.227793	58.228109
2493.874933	68602.162873	58.233114
2492.822615	68396.983465	58.238119
2492.130827	68185.643234	58.243124
2491.248642	67978.306743	58.248129
2490.671443	67777.365483	58.253133
2490.262018	67573.422883	58.258138
2489.661370	67372.223498	58.263143
2489.159671	67166.171704	58.268148
2488.483891	66960.130687	58.273153
2487.893105	66749.657684	58.278157
2487.153007	66537.462640	58.283162
2486.172491	66345.416054	58.288167
2485.372163	66142.234418	58.293172
2484.930563	65923.652935	58.298177
2484.405428	65722.376344	58.303181
2483.695334	65523.787850	58.308186
2482.904230	65321.101019	58.313191
2482.448129	65099.390037	58.318196
2481.607649	64899.315096	58.323201
2480.959307	64696.358894	58.328205
2480.460344	64491.253389	58.333210
2479.924463	64287.457268	58.338215
2479.558328	64078.906026	58.343220
2478.518969	63876.276944	58.348225
2477.679166	63655.757954	58.353229
2477.002133	63449.843282	58.358234
2476.404541	63251.668873	58.363239
2476.524221	63036.073870	58.368244
2475.573749	62835.699142	58.373249
2474.457175	62617.629545	58.378253
2473.837773	62397.894315	58.383258
2472.933201	62202.100140	58.388263
2472.185387	61989.826771	58.393268
2471.699788	61780.866860	58.398273
2470.944284	61579.002348	58.403277
2470.375087	61377.414368	58.408282
2469.841060	61185.332922	58.413287
2469.229342	60968.440066	58.418292
2468.481488	60768.197517	58.423297
2467.822954	60558.205355	58.428301
2467.349428	60350.449625	58.433306
2466.762982	60151.169387	58.438311
2466.059256	59933.695228	58.443316
2465.131852	59735.549738	58.448321
2464.382332	59515.900300	58.453325
2463.795802	59310.494282	58.458330
2463.140122	59108.152940	58.463335
2462.289911	58897.937499	58.468340
2461.595602	58704.539357	58.473345
2461.018864	58498.760855	58.478349
2460.428621	58290.220308	58.483354
2459.558831	58085.844394	58.488359
2458.735239	57885.565511	58.493364
2458.196065	57689.447049	58.498369
2457.603655	57471.657872	58.503373
2457.200595	57279.010146	58.508378
2456.140827	57074.976149	58.513383
2455.909847	56872.110671	58.518388
2455.170691	56672.644902	58.523393
2454.354288	56481.615516	58.528397
2453.719755	56265.530956	58.533402
2452.953733	56073.519838	58.538407
2452.624053	55865.145642	58.543412
2451.852408	55667.227677	58.548417
2451.244018	55463.662114	58.553421
2450.466212	55253.748668	58.558426
2449.562700	55049.737608	58.563431
2449.109760	54845.454841	58.568436
2448.650584	54645.602690	58.573441
2447.521538	54450.609015	58.578445
2447.012182	54248.326065	58.583450
2446.771951	54041.939399	58.588455
2445.838712	53839.073116	58.593460
2445.200628	53642.260249	58.598465
2444.341807	53437.772744	58.603469
2443.760283	53224.329426	58.608474
2442.882369	53039.370673	58.613479
2442.704338	52834.807320	58.618484
2442.018151	52633.693654	58.623489
2440.835852	52430.977479	58.628493
2440.603288	52236.229264	58.633498
2439.716682	52028.699037	58.638503
2439.170733	51825.423610	58.643508
2438.295475	51628.337927	58.648513
2437.801321	51424.435461	58.653517
2437.402671	51230.255971	58.658522
2436.737950	51024.290459	58.663527
2436.081074	50817.117413	58.668532
2435.234063	50618.699915	58.673537
2434.518050	50423.304364	58.678541
2434.211632	50207.410473	58.683546
2433.185309	50018.946800	58.688551
2432.674054	49815.258267	58.693556
2431.653666	49612.801221	58.698561
2431.316729	49411.778847	58.703565
2430.870861	49197.539061	58.708570
2429.597139	49013.633476	58.713575
2429.131402	48800.009032	58.718580
2428.421019	48614.977404	58.723585
2427.810638	48413.386392	58.728589
2427.332596	48212.770026	58.733594
2426.211220	48013.387290	58.738599
2425.764688	47810.859712	58.743604
2424.964185	47622.439325	58.748609
2424.253163	47421.470241	58.753613
2423.789884	47228.011915	58.758618
2423.175103	47035.639434	58.763623
2422.648126	46840.161431	58.768628
2421.931732	46638.569427	58.773633
2420.994046	46443.388684	58.778637
2420.872239	46239.707810	58.783642
2419.842615	46040.114496	58.788647
2419.547171	45834.033382	58.793652
2418.525117	45639.305104	58.798657
2417.826846	45439.795748	58.803661
2417.371334	45246.541370	58.808666
2416.368960	45040.853657	58.813671
2415.861059	44846.024190	58.818676
2415.430933	44651.349026	58.823681
2414.526215	44453.373345	58.828685
2413.853984	44259.009776	58.833690
2412.828078	44068.942577	58.838695
2412.095466	43868.175639	58.843700
2411.462126	43677.667766	58.848705
2411.078713	43478.769711	58.853709
2410.644830	43292.330094	58.858714
2409.459616	43098.924193	58.863719
2408.881164	42901.214852	58.868724
2408.531136	42714.508804	58.873729
2408.022062	42519.006591	58.878733
2407.648106	42318.352471	58.883738
2406.982893	42125.346179	58.888743
2405.933611	41921.843695	58.893748
2405.462709	41728.143758	58.898753
2404.450489	41535.657611	58.903757
2404.021625	41323.459117	58.908762
2403.184987	41132.296763	58.913767
2402.776475	40938.219490	58.918772
2401.973079	40741.889138	58.923777
2401.485445	40544.075346	58.928781
2400.693828	40338.697679	58.933786
2399.975946	40150.882393	58.938791
2399.627585	39950.406701	58.943796
2398.950601	39756.486524	58.948801
2398.129520	39547.459828	58.953805
2397.194128	39354.133783	58.958810
2396.483679	39160.739476	58.963815
2396.243255	38968.683015	58.968820
2395.809118	38767.668805	58.973825
2394.863111	38571.629398	58.978829
2394.503222	38374.217223	58.983834
2393.376111	38176.494255	58.988839
2392.792845	37969.902657	58.993844
2392.182310	37769.494137	58.998849
2391.493790	37579.947775	59.003853
2391.255317	37379.310975	59.008858
2390.339925	37180.242926	59.013863
2389.420243	36981.411847	59.018868
2388.894017	36782.553911	59.023873
2387.848706	36585.843442	59.028877
2387.287825	36391.190796	59.033882
2386.644950	36190.260756	59.038887
2385.895791	35997.270596	59.043892
2385.339895	35801.356284	59.048897
2384.775288	35610.486207	59.053901
2384.401984	35414.635955	59.058906
2383.241188	35232.339858	59.063911
2382.794532	35028.421087	59.068916
2382.386901	34833.770049	59.073921
2381.433177	34637.050452	59.078925
2380.843861	34443.494866	59.083930
2380.189557	34256.178936	59.088935
2379.473362	34050.331297	59.093940
2378.912231	33857.381762	59.098945
2377.999852	33657.043170	59.103949
2377.494454	33458.090106	59.108954
2376.716472	33264.322072	59.113959
2376.167386	33069.457986	59.118964
2375.328845	32876.486355	59.123969
2374.649103	32680.708810	59.128973
2374.240404	32485.219297	59.133978
2373.068116	32301.041693	59.138983
2372.495900	32096.707724	59.143988
2371.929686	31917.792263	59.148993
2371.156920	31726.220534	59.153997
2370.940991	31537.317058	59.159002
2369.905565	31354.744853	59.164007
2369.256408	31154.713925	59.169012
2368.945981	30964.697402	59.174017
2367.953989	30779.082847	59.179021
2367.494312	30581.827273	59.184026
2366.623757	30391.037112	59.189031
2365.968910	30195.266087	59.194036
2365.436491	30007.233014	59.199041
2364.699165	29828.536419	59.204045
2364.521078	29625.609994	59.209050
2363.787482	29435.626095	59.214055
2362.972929	29237.194719	59.219060
2362.101739	29041.147871	59.224065
2361.274488	28858.210152	59.229069
2360.774187	28664.837610	59.234074
2360.153116	28478.798438	59.239079
2359.556631	28279.353491	59.244084
2358.822730	28087.999719	59.249089
2358.011378	27904.221770	59.254093
2357.299497	27715.905404	59.259098
2356.615696	27524.570848	59.264103
2355.966727	27335.672266	59.269108
2355.679595	27153.088273	59.274113
2354.615161	26950.697437	59.279117
2354.351816	26770.344634	59.284122
2353.159118	26584.157124	59.289127
2352.775771	26387.406127	59.294132
2352.283524	26200.714648	59.299137
2351.213521	26013.709386	59.304141
2350.983929	25823.634029	59.309146
2350.002594	25638.424622	59.314151
2349.081614	25456.499740	59.319156
2348.700463	25271.500292	59.324161
2347.736738	25084.730634	59.329165
2347.440087	24891.519276	59.334170
2346.629707	24718.313981	59.339175
2345.860280	24529.485480	59.344180
2345.507988	24345.316633	59.349185
2344.591952	24169.131335	59.354189
2344.235265	23976.574679	59.359194
2343.138574	23797.504004	59.364199
2342.820572	23609.068065	59.369204
2342.089507	23423.626553	59.374209
2340.885042	23241.034942	59.379213
2340.890069	23056.184593	59.384218
2339.879129	22888.366129	59.389223
2339.425799	22691.101336	59.394228
2339.042242	22505.417174	59.399233
2338.045166	22317.245532	59.404237
2337.554829	22134.667851	59.409242
2336.869550	21953.294227	59.414247
2335.744985	21764.505788	59.419252
2335.448363	21586.992893	59.424257
2334.690576	21399.466153	59.429261
2334.241047	21205.260023	59.434266
2333.157218	21033.818401	59.439271
2332.674670	20858.291891	59.444276
2332.091695	20674.367877	59.449281
2331.489121	20486.902346	59.454285
2330.660178	20304.997945	59.459290
2329.872508	20120.776488	59.464295
2329.229599	19934.235069	59.469300
2328.481001	19756.682549	59.474305
2327.478050	19587.589928	59.479309
2327.389369	19401.743818	59.484314
2326.504111	19239.983934	59.489319
2325.865779	19052.810369	59.494324
2325.341489	18861.559011	59.499329
2324.802879	18688.873001	59.504333
2324.207916	18511.890852	59.509338
2323.195056	18334.036332	59.514343
2322.915800	18150.968782	59.519348
2321.808115	17966.918481	59.524353
2320.912237	17793.722320	59.529357
2321.132671	17606.758643	59.534362
2320.322603	17444.035582	59.539367
2319.891763	17258.614137	59.544372
2319.098081	17067.943322	59.549377
2318.245784	16878.292586	59.554381
2317.719540	16691.942196	59.559386
2316.729293	16523.813750	59.564391
2316.324457	16335.389100	59.569396
2315.646870	16160.752867	59.574401
2314.958943	15974.196767	59.579405
2314.339441	15788.700427	59.584410
2313.573626	15607.915750	59.589415
2312.786912	15420.552402	59.594420
2312.337341	15253.528465	59.599425
2311.200588	15068.525343	59.604429
2310.731713	14876.830109	59.609434
2309.585187	14710.422401	59.614439
2309.566255	14532.444301	59.619444
2308.937103	14352.836943	59.624449
2307.776091	14182.694153	59.629453
2307.435801	14001.251995	59.634458
2306.483764	13823.021651	59.639463
2305.947444	13653.911875	59.644468
2305.187727	13472.755692	59.649473
2304.463964	13297.958032	59.654477
2304.193046	13123.040130	59.659482
2302.878753	12955.712250	59.664487
2302.761602	12779.831681	59.669492
2302.216714	12608.055204	59.674497
2301.540335	12432.977474	59.679501
2301.050484	12251.813030	59.684506
2300.055121	12074.098395	59.689511
2299.395173	11901.108489	59.694516
2298.917307	11723.746924	59.699521
2298.118202	11549.674154	59.704525
2297.435021	11368.011113	59.709530
2296.608234	11201.410118	59.714535
2296.213612	11023.973467	59.719540
2295.458544	10849.044382	59.724545
2294.573918	10686.081679	59.729549
2293.781365	10507.770835	59.734554
2293.107301	10336.161316	59.739559
2292.357922	10167.066176	59.744564
2291.606973	10001.610640	59.749569
2291.310018	9831.090741	59.754573
2291.129236	9662.619402	59.759578
2289.713765	9500.217405	59.764583
2289.162949	9323.106723	59.769588
2288.541145	9152.612469	59.774593
2287.526052	8981.132777	59.779597
2287.110782	8818.105303	59.784602
2286.555129	8650.223669	59.789607
2285.848264	8491.390431	59.794612
2285.054758	8332.800619	59.799617
2284.399652	8160.135908	59.804621
2283.633751	7987.321923	59.809626
2282.777244	7827.033880	59.814631
2282.214558	7661.692905	59.819636
2281.822306	7497.678512	59.824641
2280.835131	7356.715674	59.829645
2280.161044	7190.902921	59.834650
2279.413025	7024.894678	59.839655
2278.943290	6861.686450	59.844660
2278.397287	6702.444317	59.849665
2277.579496	6543.741603	59.854669
2277.324405	6385.090556	59.859674
2276.155437	6228.109006	59.864679
2275.335219	6056.807768	59.869684
2274.727633	5898.117235	59.874689
2273.801129	5741.800461	59.879693
2273.168060	5583.492799	59.884698
2272.328357	5434.850826	59.889703
2272.064443	5276.424774	59.894708
2271.070150	5141.981663	59.899713
2270.359152	4991.438521	59.904718
2269.891780	4837.248075	59.909722
2268.928781	4693.029674	59.914727
2268.165856	4549.719555	59.919732
2267.753937	4396.779798	59.924737
2266.623738	4257.051721	59.929742
2266.374579	4112.026141	59.934746
2265.312581	3972.416132	59.939751
2264.613189	3829.416035	59.944756
2263.940575	3693.491709	59.949761
2262.989833	3566.506122	59.954766
2262.502452	3420.114136	59.959770
2261.360360	3292.837105	59.964775
2260.414601	3161.466766	59.969780
2259.953238	3032.086290	59.974785
2259.028290	2915.586024	59.979790
2258.120313	2787.799873	59.984794
2257.652752	2682.869488	59.989799
2256.970173	2566.490485	59.994804
2256.248899	2446.691903	59.999809
2255.223089	2334.497710	60.004814
2254.625949	2224.707147	60.009818
2254.101068	2118.891636	60.014823
2253.403013	2010.322909	60.019828
2252.884923	1899.868475	60.024833
2251.659209	1801.642448	60.029838
2251.165607	1687.316049	60.034842
2250.070255	1587.159222	60.039847
2249.460167	1486.369361	60.044852
2248.915425	1390.624643	60.049857
2247.773071	1295.897195	60.054862
2247.551275	1199.117569	60.059866
2246.816820	1108.775756	60.064871
2245.907714	1015.429396	60.069876
2245.467894	923.069012	60.074881
2244.262721	830.806963	60.079886
2243.659812	743.629141	60.084890
2242.817946	665.641578	60.089895
2242.164717	579.504135	60.094900
2241.854240	491.756264	60.099905
2240.694260	420.696494	60.104910
2239.941705	331.515200	60.109914
2239.012347	269.552288	60.114919
2238.114679	193.429135	60.119924
2237.754542	127.038110	60.124929
2236.838912	63.728694	60.129934
2236.075830	-7.587492	60.134938
2235.032010	-59.032657	60.139943
2233.568398	-99.261632	60.144948
2230.770119	-97.664844	60.149953
2228.757368	-89.805798	60.154958
2228.317566	-86.216060	60.159962
2227.423275	-78.985458	60.164967
2227.158056	-72.934896	60.169972
2226.576387	-65.583564	60.174977
2226.420800	-64.581043	60.179982
2226.640522	-62.562540	60.184986
2226.191478	-67.520288	60.189991
2225.439978	-90.493077	60.194996
2225.217046	-105.267262	60.200001
2224.583447	-103.198555	60.205006
2223.846958	-118.823266	60.210010
2222.853754	-110.206572	60.215015
2219.912891	-60.212515	60.220020
2218.569915	-23.554672	60.225025
2217.760127	2.993591	60.230030
2218.683215	11.501907	60.235034
2218.150092	25.562096	60.240039
2218.724147	30.247909	60.245044
2218.825334	16.328969	60.250049
2218.156107	7.875188	60.255054
2217.786433	-6.382211	60.260058
2217.146469	-12.167584	60.265063
2216.824220	-11.173314	60.270068
2216.204884	-16.873644	60.275073
2214.423816	-5.698570	60.280078
2213.018315	-5.827179	60.285082
2211.566566	25.287493	60.290087
2211.007539	21.610357	60.295092
2211.255298	30.618494	60.300097
2210.778355	39.177032	60.305102
2210.858206	21.233769	60.310106
2210.406216	22.693343	60.315111
2209.312575	22.579918	60.320116
2209.047467	20.363782	60.325121
2208.457029	25.444073	60.330126
2207.516872	20.889076	60.335130
2206.601242	28.682962	60.340135
2205.779609	37.557967	60.345140
2205.201764	29.843495	60.350145
2204.412132	39.120296	60.355150
2204.314181	34.288176	60.360154
2203.539989	42.108518	60.365159
2202.952079	46.524491	60.370164
2202.567851	36.205605	60.375169
2201.650124	30.932659	60.380174
2201.069737	28.973130	60.385178
2200.244100	34.563844	60.390183
2199.702594	36.986987	60.395188
2199.390635	40.619558	60.400193
2197.965299	37.552963	60.405198
2197.591446	49.129337	60.410202
2197.120998	44.780528	60.415207
2196.256778	51.219498	60.420212
2195.592854	43.659032	60.425217
2194.986393	44.274180	60.430222
2194.816864	52.041180	60.435226
2193.858500	42.623966	60.440231
2193.337223	45.133792	60.445236
2192.402265	40.366650	60.450241
2191.470336	53.573889	60.455246
2191.371704	44.149594	60.460250
2190.448006	50.534921	60.465255
2190.025154	51.171405	60.470260
2189.367194	49.027055	60.475265
2188.670857	56.164823	60.480270
2188.226684	45.882253	60.485274
2187.279814	51.067992	60.490279
2186.328530	48.539653	60.495284
2185.836571	44.886571	60.500289
2185.088553	58.304345	60.505294
2184.822540	48.127555	60.510298
2184.153290	57.487779	60.515303
2183.149557	51.132450	60.520308
2182.760417	52.720837	60.525313
2182.222108	56.662149	60.530318
2181.947945	51.324949	60.535322
2181.177293	53.331849	60.540327
2180.633579	49.182331	60.545332
2179.957874	47.048685	60.550337
2178.646162	53.165979	60.555342
2178.084844	48.763778	60.560346
2177.132469	52.363912	60.565351
2176.196588	45.392248	60.570356
2176.084083	51.992670	60.575361
2175.363659	61.890895	60.580366
2175.154118	47.620666	60.585370
2174.367894	58.865064	60.590375
2173.727433	43.469403	60.595380
2173.092480	50.430269	60.600385
2172.237316	50.250637	60.605390
2171.805624	46.192164	60.610394
2170.767320	54.131697	60.615399
2170.676217	56.500736	60.620404
2170.154444	48.610204	60.625409
2169.568581	52.003951	60.630414
2168.720385	47.562109	60.635418
2167.478066	55.183914	60.640423
2166.685333	46.910579	60.645428
2166.738865	48.767793	60.650433
2165.710519	57.333403	60.655438
2165.427240	49.567466	60.660442
2164.416822	50.404414	60.665447
2163.691117	50.849245	60.670452
2162.885259	53.096711	60.675457
2162.111817	53.216366	60.680462
2161.945184	46.628882	60.685466
2161.343026	49.077427	60.690471
2160.902068	57.854207	60.695476
2159.858759	45.930406	60.700481
2159.282522	54.220849	60.705486
2158.915579	56.725120	60.710490
2158.437266	57.591191	60.715495
2157.218648	60.128086	60.720500
2156.473502	54.378317	60.725505
2155.725032	66.198654	60.730510
2155.318894	54.815600	60.735514
2154.904717	50.602956	60.740519
2154.320809	62.400334	60.745524
2153.817477	56.098090	60.750529
2152.351373	57.215510	60.755534
2152.038389	59.419473	60.760538
2151.411895	54.956652	60.765543
2150.411728	63.582457	60.770548
2150.109556	63.190507	60.775553
2149.274745	61.813849	60.780558
2148.914413	56.219077	60.785562
2148.333352	54.970900	60.790567
2147.312185	62.874608	60.795572
2146.941801	58.110943	60.800577
2145.798167	68.691364	60.805582
2145.616022	67.471359	60.810586
2144.840167	63.241980	60.815591
2143.966333	65.918149	60.820596
2143.701269	58.803784	60.825601
2142.872331	63.617576	60.830606
2141.929428	56.968747	60.835610
2141.408877	60.535073	60.840615
2140.942754	61.807661	60.845620
2140.122339	61.871695	60.850625
2139.367780	62.999230	60.855630
2138.793436	64.156521	60.860634
2138.566662	54.158023	60.865639
2137.521961	60.870086	60.870644
2137.411741	54.029213	60.875649
2135.953402	66.176662	60.880654
2135.792798	63.652198	60.885658
2135.077594	60.927139	60.890663
2134.316595	67.468030	60.895668
2133.937024	66.027028	60.900673
2132.967438	66.699807	60.905678
2132.621971	66.827261	60.910682
2132.158722	65.666053	60.915687
2131.495476	65.034918	60.920692
2130.419663	65.726130	60.925697
2128.725799	70.965763	60.930702
2129.248764	72.366853	60.935706
2128.811882	71.354433	60.940711
2127.960765	69.816358	60.945716
2126.852050	59.024204	60.950721
2125.754229	70.567230	60.955726
2126.094453	63.255893	60.960730
2125.353397	63.447694	60.965735
2124.110801	71.414935	60.970740
2123.669013	64.081021	60.975745
2123.008646	64.155936	60.980750
2122.865441	57.209905	60.985754
2121.948156	65.172835	60.990759
2121.049367	69.543537	60.995764
2120.583942	67.351305	61.000769
2119.563470	69.481445	61.005774
2118.987084	70.719493	61.010778
2118.367604	65.236810	61.015783
2117.783889	60.677320	61.020788
2117.381911	66.948348	61.025793
2116.475227	67.667925	61.030798
2115.951150	63.561037	61.035802
2115.573247	63.422392	61.040807
2114.997377	65.153965	61.045812
2114.395032	56.905630	61.050817
2113.677700	62.570657	61.055822
2112.423828	65.228288	61.060826
2111.561193	61.247667	61.065831
2111.097179	71.365430	61.070836
2110.904078	70.528805	61.075841
2109.704036	71.815351	61.080846
2109.212080	67.294919	61.085850
2108.511437	60.237061	61.090855
2107.889358	66.273346	61.095860
2107.582069	62.496352	61.100865
2106.544192	68.592309	61.105870
2105.804534	61.807159	61.110874
2105.238363	75.825334	61.115879
2104.398599	71.695998	61.120884
2104.193977	62.655968	61.125889
2103.686208	82.749024	61.130894
2103.341904	62.431806	61.135898
2102.670021	66.943132	61.140903
2102.008939	64.487049	61.145908
2100.705293	61.935804	61.150913
2099.295949	72.403858	61.155918
2099.052219	72.537250	61.160922
2099.734475	76.630264	61.165927
2098.344320	68.683566	61.170932
2097.680254	69.525506	61.175937
2096.664933	79.746530	61.180942
2096.451591	67.654769	61.185946
2095.544181	77.809781	61.190951
2095.109096	69.216345	61.195956
2094.050139	68.566008	61.200961
2092.767968	75.533404	61.205966
2092.728946	68.564531	61.210970
2092.823976	73.875142	61.215975
2091.436637	74.907555	61.220980
2090.735782	69.552914	61.225985
2089.984054	73.662159	61.230990
2089.312030	70.966531	61.235994
2088.805813	69.999815	61.240999
2088.325407	84.400222	61.246004
2088.133032	77.501414	61.251009
2087.245448	78.353594	61.256014
2086.654922	70.527603	61.261018
2085.948110	74.233890	61.266023
2085.017394	74.719161	61.271028
2084.748022	58.017211	61.276033
2083.348342	70.978581	61.281038
2082.644231	64.979461	61.286042
2082.598795	66.481780	61.291047
2081.904785	70.853114	61.296052
2081.503899	69.983229	61.301057
2080.231195	69.660143	61.306062
2079.558321	62.684624	61.311066
2078.639193	63.204330	61.316071
2077.757908	69.625545	61.321076
2078.018137	65.026757	61.326081
2077.453501	66.863792	61.331086
2076.747050	64.454342	61.336090
2076.197042	72.933039	61.341095
2075.245737	74.030311	61.346100
2074.243263	62.514817	61.351105
2073.495868	70.829287	61.356110
2073.034862	65.300968	61.361114
2071.986475	70.160645	61.366119
2071.445876	66.914287	61.371124
2071.275896	65.558311	61.376129
2070.053561	70.436131	61.381134
2069.834090	63.935887	61.386138
2069.277775	64.481602	61.391143
2068.848006	70.490530	61.396148
2068.349411	66.221907	61.401153
2067.417682	65.906220	61.406158
2066.778482	63.088691	61.411162
2065.882934	77.457198	61.416167
2064.942655	73.217666	61.421172
2064.405314	64.448072	61.426177
2063.903416	71.466700	61.431182
2063.266058	65.255134	61.436186
2062.666811	68.286737	61.441191
2062.088834	69.141833	61.446196
2062.003587	66.496602	61.451201
2060.826566	65.431335	61.456206
2059.926672	61.399873	61.461210
2059.019504	65.893352	61.466215
2058.340724	67.388945	61.471220
2058.232918	58.863439	61.476225
2057.442346	68.870595	61.481230
2056.463450	67.512103	61.486234
2055.638154	67.550128	61.491239
2055.160566	67.826297	61.496244
2054.349011	64.581943	61.501249
2053.631373	69.901667	61.506254
2053.213449	73.681967	61.511258
2052.693573	65.431598	61.516263
2052.182414	75.274563	61.521268
2052.024135	63.109420	61.526273
2051.309245	69.289759	61.531278
2050.166084	61.494716	61.536282
2049.179769	70.826436	61.541287
2048.281785	70.893347	61.546292
2048.292907	74.348503	61.551297
2047.365738	67.943228	61.556302
2046.815148	72.462126	61.561306
2046.293895	70.714026	61.566311
2045.825385	69.801262	61.571316
2045.091895	62.272378	61.576321
2043.927723	61.350166	61.581326
2043.038033	67.676525	61.586330
2042.593302	67.053312	61.591335
2042.270793	70.898898	61.596340
2041.795671	68.131032	61.601345
2041.396627	66.513355	61.606350
2040.292794	64.342031	61.611354
2039.282823	65.177379	61.616359
2038.224402	69.956655	61.621364
2037.649036	63.872459	61.626369
2036.933771	65.720792	61.631374
2036.834537	59.879590	61.636378
2036.550260	61.520744	61.641383
2035.929814	63.038624	61.646388
2035.613151	64.306434	61.651393
2034.362411	69.485256	61.656398
2033.465549	61.731559	61.661402
2032.922302	61.461466	61.666407
2032.333012	70.247611	61.671412
2031.850906	61.212209	61.676417
2031.159667	68.633066	61.681422
2030.237681	60.172124	61.686426
2029.204377	61.416472	61.691431
2028.409459	64.474404	61.696436
2028.131456	62.892716	61.701441
2027.325195	68.125580	61.706446
2027.123788	59.389421	61.711450
2026.939243	62.656422	61.716455
2026.379190	69.736325	61.721460
2025.022781	65.537623	61.726465
2023.700193	66.438363	61.731470
2023.333470	60.358907	61.736474
2022.839230	63.496859	61.741479
2022.225837	63.802473	61.746484
2022.239444	58.482704	61.751489
2021.648682	64.556612	61.756494
2020.521078	58.575841	61.761498
2019.680249	59.925268	61.766503
2018.687667	66.543941	61.771508
2018.414150	61.321784	61.776513
2017.542272	74.688288	61.781518
2017.386798	67.092905	61.786522
2016.692106	66.706497	61.791527
2015.751339	64.312175	61.796532
2015.080189	68.943257	61.801537
2013.836341	77.711867	61.806542
2013.546693	58.146135	61.811546
2013.411724	58.913581	61.816551
2012.456111	67.781524	61.821556
2012.348350	64.873353	61.826561
2011.527776	69.397259	61.831566
2010.489851	60.320766	61.836570
2009.703600	64.793490	61.841575
2008.852771	66.996097	61.846580
2008.796234	60.946263	61.851585
2008.026228	70.231045	61.856590
2007.218297	61.266289	61.861594
2005.993958	76.245254	61.866599
2005.255407	71.057481	61.871604
2005.205828	65.105893	61.876609
2004.263875	63.993880	61.881614
2004.040934	71.039204	61.886618
2003.690732	63.782251	61.891623
2003.188554	63.403139	61.896628
2002.637912	63.244617	61.901633
2001.282916	74.759112	61.906638
2000.539571	63.730827	61.911642
2000.217523	73.898609	61.916647
1998.863029	70.920229	61.921652
1998.735241	63.957571	61.926657
1997.828325	63.008740	61.931662
1997.111148	77.434106	61.936666
1996.603344	63.712738	61.941671
1995.952758	62.347892	61.946676
1995.820169	55.780255	61.951681
1994.749476	69.616725	61.956686
1993.989132	58.116463	61.961690
1993.200334	62.201648	61.966695
1992.471427	68.780056	61.971700
1992.286938	61.389566	61.976705
1991.838632	56.406479	61.981710
1990.571985	61.849626	61.986714
1989.933675	66.327259	61.991719
1988.847003	70.027625	61.996724
1988.572546	51.924548	62.001729
1987.676383	70.443867	62.006734
1987.390301	67.455188	62.011738
1987.277623	65.768411	62.016743
1986.375179	65.661002	62.021748
1985.501904	60.157141	62.026753
1984.640186	62.803048	62.031758
1984.087309	59.880374	62.036762
1983.590450	57.174322	62.041767
1983.129902	62.645647	62.046772
1982.426454	62.008315	62.051777
1980.876641	71.798519	62.056782
1980.511880	63.536167	62.061786
1979.762320	63.338258	62.066791
1979.533648	67.859687	62.071796
1979.304318	55.235891	62.076801
1979.159662	68.852833	62.081806
1977.833135	60.082374	62.086810
1976.852068	54.062597	62.091815
1975.893480	58.412866	62.096820
1975.731677	60.476149	62.101825
1974.523142	65.668796	62.106830
1973.541898	63.079058	62.111834
1973.310448	61.190354	62.116839
1972.623600	63.623996	62.121844
1972.001033	54.377512	62.126849
1971.311648	63.166932	62.131854
1971.367622	56.209807	62.136858
1970.758929	60.983952	62.141863
1969.954563	65.699268	62.146868
1968.887098	55.536191	62.151873
1968.016080	63.663711	62.156878
1967.716990	57.922053	62.161882
1967.165744	62.008963	62.166887
1966.617833	69.804490	62.171892
1965.662896	56.836962	62.176897
1964.431294	65.827577	62.181902
1963.927947	61.793133	62.186906
1963.441189	60.777621	62.191911
1962.823111	62.930679	62.196916
1962.578334	64.368442	62.201921
1962.217889	64.026767	62.206926
1961.062685	64.276469	62.211930
1960.361729	64.403601	62.216935
1959.511332	66.383794	62.221940
1959.183022	59.276348	62.226945
1958.390071	64.308412	62.231950
1957.973316	61.722119	62.236954
1956.582917	71.827665	62.241959
1955.750071	54.756289	62.246964
1955.502873	46.744960	62.251969
1954.927699	65.262210	62.256974
1954.795913	62.540792	62.261978
1954.451477	54.235800	62.266983
1953.235317	55.608554	62.271988
1952.330737	46.545626	62.276993
1951.620434	52.140178	62.281998
1951.360077	57.821010	62.287002
1951.050715	56.436705	62.292007
1949.509566	60.482051	62.297012
1948.814275	53.984820	62.302017
1948.128381	62.653837	62.307022
1947.712442	65.132793	62.312026
1947.350678	62.465230	62.317031
1946.763509	64.801050	62.322036
1946.041719	61.570871	62.327041
1944.869629	68.208601	62.332046
1944.359189	60.013541	62.337050
1943.886660	60.680027	62.342055
1942.846188	68.079064	62.347060
1942.783556	56.296173	62.352065
1942.305582	65.846856	62.357070
1941.154318	55.361192	62.362074
1940.532217	58.123621	62.367079
1939.668351	60.672107	62.372084
1939.534711	57.652929	62.377089
1938.992849	58.940727	62.382094
1937.952479	62.485521	62.387098
1937.042129	55.427897	62.392103
1936.395982	57.747849	62.397108
1936.002393	53.306468	62.402113
1935.765337	56.875131	62.407118
1934.879416	57.231913	62.412122
1933.885730	56.385193	62.417127
1933.130092	49.496987	62.422132
1933.062285	56.192813	62.427137
1931.947544	57.404392	62.432142
1930.832321	54.354952	62.437146
1930.117802	62.741499	62.442151
1929.544302	65.737500	62.447156
1929.498484	54.128569	62.452161
1929.039285	60.940148	62.457166
1928.614403	55.786193	62.462170
1927.543228	63.587515	62.467175
1926.367450	59.152029	62.472180
1926.104844	51.423858	62.477185
1924.855552	61.451814	62.482190
1924.677965	61.874355	62.487194
1924.356513	55.753041	62.492199
1923.535869	59.877993	62.497204
1922.690964	50.110138	62.502209
1921.869451	61.193020	62.507214
1921.419493	59.042531	62.512218
1920.782383	50.900709	62.517223
1920.413317	59.399579	62.522228
1919.412009	63.996355	62.527233
1918.498042	64.471140	62.532238
1917.833461	59.823613	62.537242
1917.533174	51.675631	62.542247
1916.747153	55.930711	62.547252
1916.783022	62.521767	62.552257
1915.657015	60.978518	62.557262
1914.785276	66.299079	62.562266
1914.521540	61.564261	62.567271
1913.444116	58.978777	62.572276
1912.249140	55.038377	62.577281
1911.552207	60.055207	62.582286
1911.022797	60.142502	62.587290
1910.306082	54.493966	62.592295
1909.767878	65.412023	62.597300
1909.722745	53.402424	62.602305
1909.513729	57.073875	62.607310
1909.113972	58.335965	62.612314
1908.031478	62.243862	62.617319
1906.631793	60.871803	62.622324
1907.004021	58.715373	62.627329
1905.540973	60.188848	62.632334
1904.678394	56.723981	62.637338
1904.163116	52.320849	62.642343
1903.411459	60.271732	62.647348
1903.048468	56.503615	62.652353
1902.237869	57.469794	62.657358
1901.978465	56.211611	62.662362
1900.937380	52.484914	62.667367
1900.310024	60.341944	62.672372
1899.473600	52.310622	62.677377
1899.110901	64.374115	62.682382
1898.356082	56.519078	62.687386
1897.284226	56.309280	62.692391
1896.486723	59.992156	62.697396
1896.082230	50.351519	62.702401
1895.948660	64.171701	62.707406
1895.580031	65.223839	62.712410
1894.490715	54.606936	62.717415
1893.459539	64.084594	62.722420
1892.962250	57.497595	62.727425
1892.625230	65.693326	62.732430
1892.038549	65.122640	62.737434
1891.123155	59.892019	62.742439
1889.804465	57.346427	62.747444
1889.602362	56.213194	62.752449
1889.228988	60.727635	62.757454
1888.576091	65.466234	62.762458
1888.287252	59.448561	62.767463
1886.824042	60.827451	62.772468
1886.295908	50.365898	62.777473
1885.965736	56.335370	62.782478
1885.233372	60.829532	62.787482
1884.387073	59.140960	62.792487
1883.243766	66.058004	62.797492
1882.866775	58.570357	62.802497
1882.352727	61.799787	62.807502
1881.917316	56.551316	62.812506
1881.762239	62.961365	62.817511
1880.693623	61.778041	62.822516
1879.974939	50.586621	62.827521
1879.272802	68.097397	62.832526
1878.650948	61.504945	62.837530
1877.803867	57.931967	62.842535
1876.772820	65.517192	62.847540
1876.535986	60.765493	62.852545
1875.918141	58.121253	62.857550
1875.469010	63.685398	62.862554
1875.079074	61.463885	62.867559
1873.894067	72.279630	62.872564
1873.505293	50.173350	62.877569
1872.463220	53.877713	62.882574
1872.003605	59.714769	62.887578
1870.856832	59.526338	62.892583
1869.929414	66.464307	62.897588
1869.592355	63.545243	62.902593
1869.096378	58.845729	62.907598
1868.712495	60.606795	62.912602
1868.284127	52.874988	62.917607
1867.929553	61.496145	62.922612
1866.719218	55.135911	62.927617
1865.614603	61.778724	62.932622
1865.234976	62.105609	62.937626
1864.692648	62.642837	62.942631
1863.783331	58.467863	62.947636
1863.542954	52.866720	62.952641
1862.086962	63.689216	62.957646
1862.006161	54.487644	62.962650
1861.680367	62.035016	62.967655
1860.700887	61.048868	62.972660
1860.601466	61.307608	62.977665
1859.043557	59.686297	62.982670
1858.474620	53.064952	62.987674
1858.183435	56.945000	62.992679
1857.370923	64.938674	62.997684
1856.794807	50.450744	63.002689
1856.037628	65.259372	63.007694
1855.307490	56.607194	63.012698
1855.097219	55.420066	63.017703
1854.080747	61.167337	63.022708
1853.000615	58.987603	63.027713
1852.097926	62.384405	63.032718
1851.901520	61.450552	63.037722
1851.721920	57.557128	63.042727
1851.087293	61.747186	63.047732
1850.447635	53.560057	63.052737
1849.583391	63.115304	63.057742
1848.909181	59.158482	63.062746
1848.479740	58.767852	63.067751
1847.344333	72.269271	63.072756
1846.251490	60.670469	63.077761
1845.850817	65.460496	63.082766
1845.557289	58.550985	63.087770
1844.965658	59.517108	63.092775
1844.360133	62.161803	63.097780
1844.081639	51.231677	63.102785
1842.780689	55.582729	63.107790
1842.077368	53.278513	63.112794
1841.350352	46.251751	63.117799
1840.794493	58.049431	63.122804
1840.570814	51.583014	63.127809
1839.228881	62.447336	63.132814
1838.319447	49.316530	63.137818
1837.942116	56.900470	63.142823
1837.325022	62.115960	63.147828
1837.467859	54.110529	63.152833
1836.860735	57.974511	63.157838
1835.874228	59.138959	63.162842
1834.964994	58.237864	63.167847
1834.358947	63.612457	63.172852
1833.708205	58.581120	63.177857
1832.666483	54.061317	63.182862
1831.933693	55.855710	63.187866
1831.402181	51.442558	63.192871
1831.017091	65.182819	63.197876
1830.883859	53.575167	63.202881
1829.752371	61.968014	63.207886
1828.433659	69.050132	63.212890
1828.222036	54.971128	63.217895
1827.488737	69.446376	63.222900
1827.639726	49.698781	63.227905
1826.724587	61.574015	63.232910
1825.909801	57.027641	63.237914
1825.326849	58.714662	63.242919
1824.247856	58.882934	63.247924
1823.544067	49.925378	63.252929
1823.052260	63.520149	63.257934
1822.256193	64.392578	63.262938
1822.181199	52.677906	63.267943
1821.547779	63.983264	63.272948
1820.723027	53.333854	63.277953
1819.626195	59.959677	63.282958
1819.337204	59.382740	63.287962
1818.477832	63.083346	63.292967
1817.131051	63.478653	63.297972
1816.550257	51.323885	63.302977
1816.222108	53.216461	63.307982
1815.482368	64.417272	63.312986
1815.675569	55.063382	63.317991
1814.922708	66.151157	63.322996
1813.833039	58.240508	63.328001
1812.966281	57.558190	63.333006
1812.311620	59.236099	63.338010
1811.993393	62.983247	63.343015
1811.505532	63.784660	63.348020
1810.652904	56.713193	63.353025
1809.572743	61.316218	63.358030
1809.046974	62.699261	63.363034
1808.722709	64.357824	63.368039
1807.760282	69.945139	63.373044
1806.867988	61.766597	63.378049
1806.137033	68.476260	63.383054
1805.599106	64.553004	63.388058
1805.631852	60.207957	63.393063
1804.827371	67.724110	63.398068
1804.827579	55.814563	63.403073
1803.201659	57.539469	63.408078
1802.635855	59.627487	63.413082
1802.102775	58.378080	63.418087
1800.703156	59.076687	63.423092
1800.105934	57.542564	63.428097
1799.713629	60.467235	63.433102
1799.309649	54.838463	63.438106
1799.086155	58.813427	63.443111
1798.055687	62.613751	63.448116
1797.171137	49.040605	63.453121
1796.546393	56.111881	63.458126
1796.062983	52.747698	63.463130
1795.698304	53.196803	63.468135
1794.656103	57.314392	63.473140
1793.866262	53.363335	63.478145
1792.997883	50.944991	63.483150
1792.581628	49.571374	63.488154
1792.315718	55.969056	63.493159
1791.905567	57.223351	63.498164
1790.538653	51.006300	63.503169
1789.905500	52.116228	63.508174
1789.477710	52.613204	63.513178
1789.205342	47.559647	63.518183
1787.791619	59.193930	63.523188
1787.198885	50.316526	63.528193
1786.270513	57.631571	63.533198
1785.740044	56.891128	63.538202
1785.746769	53.226753	63.543207
1784.733055	56.778406	63.548212
1784.331339	48.406855	63.553217
1783.195949	58.886723	63.558222
1782.379094	59.096965	63.563226
1782.355271	48.610555	63.568231
1781.744825	54.731778	63.573236
1781.022040	48.003997	63.578241
1779.996083	56.410063	63.583246
1779.600163	53.648602	63.588250
1779.284259	53.358229	63.593255
1777.836518	54.203268	63.598260
1777.177384	54.776409	63.603265
1776.584442	57.526356	63.608270
1775.900331	59.090675	63.613274
1775.846644	56.993983	63.618279
1775.207090	55.403508	63.623284
1774.375233	54.047008	63.628289
1773.581673	53.398812	63.633294
1772.822562	52.417128	63.638298
1772.704007	51.768974	63.643303
1771.152635	57.916620	63.648308
1770.650975	53.593363	63.653313
1770.206678	55.447617	63.658318
1769.736607	51.997740	63.663322
1769.343805	52.675250	63.668327
1767.711846	52.907706	63.673332
1767.288985	42.287546	63.678337
1766.802945	51.178747	63.683342
1766.297852	55.204740	63.688346
1766.208982	55.192139	63.693351
1764.669369	51.749685	63.698356
1764.196867	45.762785	63.703361
1763.562775	52.217361	63.708366
1762.831654	55.760414	63.713370
1762.713624	49.330850	63.718375
1761.140460	56.174270	63.723380
1760.600695	52.166162	63.728385
1760.144629	48.158956	63.733390
1759.745517	57.187748	63.738394
1759.489899	48.706264	63.743399
1758.711767	62.912657	63.748404
1757.757869	57.328648	63.753409
1756.882277	59.920053	63.758414
1756.539775	53.155540	63.763418
1755.997737	45.746181	63.768423
1754.573917	56.300249	63.773428
1754.275104	53.312051	63.778433
1753.806671	52.456103	63.783438
1753.296586	55.994017	63.788442
1752.650716	52.879581	63.793447
1751.450356	61.601949	63.798452
1750.939991	52.457575	63.803457
1750.291204	50.657254	63.808462
1750.018997	51.720907	63.813466
1749.510680	53.848692	63.818471
1748.185538	54.283177	63.823476
1747.730025	50.122915	63.828481
1746.914886	56.156800	63.833486
1746.545371	51.628053	63.838490
1746.238923	48.365092	63.843495
1744.722797	55.256234	63.848500
1744.369166	51.029327	63.853505
1743.803948	48.204872	63.858510
1743.404914	49.063154	63.863514
1742.374211	47.571082	63.868519
1741.477028	58.032055	63.873524
1741.296602	48.729626	63.878529
1740.849203	44.799899	63.883534
1739.809327	51.613827	63.888538
1738.968552	50.960525	63.893543
1738.091230	51.972043	63.898548
1737.774663	44.705083	63.903553
1737.599104	54.893745	63.908558
1737.273425	51.439867	63.913562
1735.889768	45.766425	63.918567
1734.982043	56.020907	63.923572
1734.555295	53.311661	63.928577
1734.063760	50.081252	63.933582
1733.208790	44.128296	63.938586
1732.128554	47.219004	63.943591
1731.428344	55.380951	63.948596
1731.187612	40.661610	63.953601
1730.808296	53.543048	63.958606
1730.342002	51.436195	63.963610
1729.470472	46.250719	63.968615
1728.255382	60.092836	63.973620
1727.847601	50.534770	63.978625
1727.520527	45.482027	63.983630
1726.577266	45.953646	63.988634
1725.915705	49.307455	63.993639
1725.300839	49.993432	63.998644
1724.931158	47.674108	64.003649
1724.299445	57.654513	64.008654
1723.536047	48.570839	64.013658
1722.653897	44.549311	64.018663
1721.816930	53.890506	64.023668
1722.005690	45.463036	64.028673
1720.709866	47.449388	64.033678
1719.558638	54.574333	64.038682
1719.322911	46.042389	64.043687
1718.712508	51.873445	64.048692
1718.515795	44.185315	64.053697
1717.283245	47.150405	64.058702
1716.708546	47.610799	64.063706
1716.391676	56.486176	64.068711
1715.385991	56.100357	64.073716
1714.389297	48.971388	64.078721
1713.476543	50.187245	64.083726
1713.265753	53.223449	64.088730
1712.776821	45.534422	64.093735
1712.002471	56.259753	64.098740
1711.730834	49.073972	64.103745
1711.151036	50.423035	64.108750
1710.122809	49.900444	64.113754
1709.114779	47.512197	64.118759
1708.674194	52.146140	64.123764
1708.710336	45.122796	64.128769
1708.145867	57.612585	64.133774
1706.482095	49.640211	64.138778
1706.200691	51.023884	64.143783
1705.681251	60.246841	64.148788
1704.442167	48.922099	64.153793
1703.958856	55.866843	64.158798
1703.185655	56.180567	64.163802
1702.828355	52.048871	64.168807
1702.496391	51.992879	64.173812
1702.131611	50.454978	64.178817
1700.547073	59.290426	64.183822
1699.619501	53.741686	64.188826
1699.584782	44.804068	64.193831
1698.789610	55.963232	64.198836
1698.499441	54.415057	64.203841
1697.738565	54.206411	64.208846
1696.843971	58.038807	64.213850
1696.688925	50.333020	64.218855
1695.895026	52.717494	64.223860
1695.113426	53.333763	64.228865
1694.027094	54.851599	64.233870
1693.245473	60.509578	64.238874
1692.779551	53.652713	64.243879
1692.751779	54.797398	64.248884
1691.532060	48.643763	64.253889
1690.706338	46.838445	64.258894
1690.155890	52.549592	64.263898
1689.855179	35.157299	64.268903
1689.480626	50.348296	64.273908
1688.255854	40.653503	64.278913
1687.430962	45.736435	64.283918
1687.013682	43.880435	64.288922
1686.547605	47.901818	64.293927
1685.568754	38.391901	64.298932
1684.846722	44.368429	64.303937
1684.181261	45.179149	64.308942
1683.694466	44.393943	64.313946
1683.345054	50.237166	64.318951
1682.681326	49.057425	64.323956
1681.963509	43.674082	64.328961
1681.269208	46.993677	64.333966
1680.683838	43.235695	64.338970
1679.709387	47.098125	64.343975
1678.570114	49.714089	64.348980
1678.051736	40.618328	64.353985
1677.451083	38.182732	64.358990
1677.204199	54.154575	64.363994
1677.093184	49.695170	64.368999
1676.087249	54.472539	64.374004
1675.005182	44.125856	64.379009
1674.625261	50.650463	64.384014
1674.192524	50.418087	64.389018
1673.193037	39.837509	64.394023
1672.020068	49.257317	64.399028
1672.183207	40.846537	64.404033
1671.427899	48.645070	64.409038
1670.582315	51.510864	64.414042
1669.943305	38.565862	64.419047
1669.503135	48.369180	64.424052
1668.766774	46.209041	64.429057
1667.512907	51.524130	64.434062
1666.882785	52.602065	64.439066
1666.392360	48.663417	64.444071
1665.989075	50.042799	64.449076
1665.686865	46.238264	64.454081
1664.286994	42.448815	64.459086
1663.616392	43.701920	64.464090
1663.068317	40.978845	64.469095
1662.320497	49.988911	64.474100
1662.076279	44.478302	64.479105
1661.652643	43.624718	64.484110
1660.137299	49.421331	64.489114
1659.843825	50.502563	64.494119
1658.927853	47.752770	64.499124
1659.082226	45.735002	64.504129
1658.354817	48.820156	64.509134
1657.146001	54.055552	64.514138
1656.694762	47.603236	64.519143
1655.934767	51.387451	64.524148
1655.733646	51.760129	64.529153
1654.388056	55.140611	64.534158
1653.820881	48.325075	64.539162
1653.307384	43.831836	64.544167
1652.643783	57.651025	64.549172
1652.475248	54.227393	64.554177
1651.431172	58.999791	64.559182
1650.820446	57.013671	64.564186
1650.110391	50.722322	64.569191
1648.901040	56.249554	64.574196
1648.252769	43.750744	64.579201
1647.517372	52.779342	64.584206
1647.155629	46.850572	64.589210
1646.902285	44.596363	64.594215
1646.640053	50.190765	64.599220
1646.131942	51.307672	64.604225
1645.146253	49.455239	64.609230
1644.264640	39.731191	64.614234
1643.111743	42.812974	64.619239
1641.931830	43.148745	64.624244
1641.540968	49.528431	64.629249
1641.616001	44.104310	64.634254
1640.971312	56.190515	64.639258
1641.141969	43.203634	64.644263
1639.408259	55.611078	64.649268
1638.734295	44.031019	64.654273
1638.004342	50.502422	64.659278
1637.657102	44.483038	64.664282
1637.165937	39.945254	64.669287
1636.079208	39.605459	64.674292
1635.526544	39.001043	64.679297
1635.054440	42.419394	64.684302
1634.134251	45.673955	64.689306
1633.316653	37.051536	64.694311
1632.594397	45.633329	64.699316
1632.275917	39.123661	64.704321
1631.962701	41.491716	64.709326
1630.809197	45.018317	64.714330
1630.005838	47.304961	64.719335
1629.226297	49.086332	64.724340
1629.137517	47.195503	64.729345
1628.498391	54.056194	64.734350
1627.641799	50.264038	64.739354
1626.856469	48.979047	64.744359
1626.005398	48.070365	64.749364
1625.837398	43.260463	64.754369
1625.400050	44.620029	64.759374
1624.078059	45.751114	64.764378
1623.442722	43.784683	64.769383
1623.078436	50.538630	64.774388
1622.778748	37.432505	64.779393
1621.674356	42.175065	64.784398
1621.213961	44.148596	64.789402
1621.027643	44.009550	64.794407
1619.279606	50.406144	64.799412
1619.041472	42.655223	64.804417
1617.970672	52.711702	64.809422
1617.334593	48.165402	64.814426
1617.310957	44.937960	64.819431
1616.102698	54.842808	64.824436
1615.342373	48.841743	64.829441
1614.674769	50.889197	64.834446
1614.228026	45.942222	64.839450
1613.810629	45.209084	64.844455
1613.227305	50.624256	64.849460
1612.896173	45.253623	64.854465
1612.252873	46.690068	64.859470
1611.302733	48.115334	64.864474
1610.336751	42.351957	64.869479
1609.258548	48.121727	64.874484
1608.567080	40.815004	64.879489
1608.139141	48.591503	64.884494
1607.747723	57.198020	64.889498
1607.609733	39.401413	64.894503
1606.391110	45.161951	64.899508
1605.391117	43.554666	64.904513
1604.986134	47.765057	64.909518
1604.406032	45.856090	64.914522
1604.043477	41.324690	64.919527
1603.348148	53.010497	64.924532
1602.915164	48.485554	64.929537
1602.162989	48.961552	64.934542
1600.884010	53.887985	64.939546
1600.105434	45.085904	64.944551
1599.262853	52.147663	64.949556
1598.794624	46.754657	64.954561
1598.782541	49.740372	64.959566
1598.026234	45.902332	64.964570
1597.684716	48.208654	64.969575
1596.722321	54.620798	64.974580
1596.323492	43.304561	64.979585
1595.631572	50.504815	64.984590
1594.358284	50.014898	64.989594
1593.542400	42.884070	64.994599
1592.967951	52.448522	64.999604
1592.497091	54.191901	65.004609
1592.422638	49.971132	65.009614
1591.539554	55.446550	65.014618
1590.956633	47.908111	65.019623
1589.963693	61.358573	65.024628
1589.153296	45.952304	65.029633
1588.002606	45.110163	65.034638
1587.473094	42.776832	65.039642
1587.140081	47.833682	65.044647
1586.246323	56.428545	65.049652
1586.099586	47.551314	65.054657
1585.654533	53.903344	65.059662
1584.988688	54.742537	65.064666
1584.471277	52.186502	65.069671
1583.242974	54.815074	65.074676
1582.885663	49.907515	65.079681
1581.852077	45.162599	65.084686
1580.833164	48.771920	65.089690
1580.724849	39.711965	65.094695
1579.986613	46.074303	65.099700
1579.538056	45.286195	65.104705
1578.609814	38.818223	65.109710
1578.025069	45.977795	65.114714
1577.815549	37.403871	65.119719
1577.166057	55.947116	65.124724
1575.929822	50.100529	65.129729
1575.114885	49.805888	65.134734
1574.360480	49.514246	65.139738
1574.263022	41.482353	65.144743
1573.708470	49.714227	65.149748
1572.863417	45.779905	65.154753
1572.003410	47.042625	65.159758
1571.492300	53.726862	65.164762
1571.453755	48.770235	65.169767
1570.061893	52.952921	65.174772
1569.273336	47.673898	65.179777
1568.920132	56.559783	65.184782
1568.076492	53.647139	65.189786
1567.362288	48.026708	65.194791
1566.271649	52.536864	65.199796
1565.831100	45.295945	65.204801
1565.517648	43.250000	65.209806
1565.322684	55.072363	65.214810
1564.987045	49.836500	65.219815
1563.352950	48.694271	65.224820
1562.818845	43.475751	65.229825
1562.502773	50.400244	65.234830
1561.336053	62.940006	65.239834
1560.540778	47.950830	65.244839
1559.972598	60.067471	65.249844
1559.566528	51.144712	65.254849
1559.275559	46.868459	65.259854
1558.325245	47.218252	65.264858
1557.465768	50.303914	65.269863
1556.935476	51.818613	65.274868
1556.667794	47.201181	65.279873
1555.647207	49.249539	65.284878
1554.579750	44.970504	65.289882
1554.350060	41.435172	65.294887
1553.434405	41.095039	65.299892
1553.293895	36.559909	65.304897
1552.258598	43.464632	65.309902
1551.340418	41.979993	65.314906
1550.856501	40.634518	65.319911
1550.380744	48.759254	65.324916
1549.912728	36.425819	65.329921
1549.063647	38.183567	65.334926
1548.481117	44.664678	65.339930
1547.962247	33.913180	65.344935
1546.821172	43.954032	65.349940
1546.030247	44.330544	65.354945
1545.502057	42.099518	65.359950
1544.952134	41.612962	65.364954
1544.572077	42.621228	65.369959
1544.077544	36.186863	65.374964
1542.932672	36.433530	65.379969
1542.229372	35.064567	65.384974
1541.791131	43.153376	65.389978
1541.635890	28.518286	65.394983
1540.350958	37.041259	65.399988
1539.315921	33.712749	65.404993
1539.144564	36.640186	65.409998
1538.566620	41.223430	65.415002
1538.391435	30.616030	65.420007
1536.600643	48.422799	65.425012
1536.187207	44.525569	65.430017
1536.024032	42.545638	65.435022
1535.217101	47.928542	65.440026
1534.387210	43.195437	65.445031
1533.211501	49.740845	65.450036
1532.861171	41.306000	65.455041
1532.161106	45.714679	65.460046
1532.005580	47.747017	65.465050
1532.062961	38.424190	65.470055
1530.521846	48.533348	65.475060
1529.765559	40.222937	65.480065
1529.737735	42.118284	65.485070
1528.491136	50.100572	65.490074
1528.042083	43.447663	65.495079
1526.660568	50.677080	65.500084
1526.674875	44.869937	65.505089
1526.458474	39.979426	65.510094
1525.025117	42.205352	65.515098
1524.826578	36.449381	65.520103
1523.932665	41.497588	65.525108
1523.448245	30.450457	65.530113
1522.464965	35.579098	65.535118
1521.896595	37.606072	65.540122
1521.455815	34.042787	65.545127
1520.189821	48.444998	65.550132
1519.397248	37.819003	65.555137
1518.635763	37.473308	65.560142
1518.278764	46.058584	65.565146
1518.225617	45.165076	65.570151
1518.016947	43.547203	65.575156
1517.185744	45.943962	65.580161
1516.226513	42.762692	65.585166
1515.455269	47.874992	65.590170
1514.741094	40.114578	65.595175
1513.474049	49.338072	65.600180
1512.962325	44.792544	65.605185
1512.558760	46.623016	65.610190
1511.981932	53.417055	65.615194
1512.128323	46.418783	65.620199
1510.607256	42.065189	65.625204
1509.769558	46.260770	65.630209
1509.419893	45.638317	65.635214
1508.785770	48.837998	65.640218
1508.502506	49.260011	65.645223
1507.134813	55.785475	65.650228
1506.664234	45.057849	65.655233
1506.083158	52.712032	65.660238
1505.344454	50.383575	65.665242
1504.352046	50.822081	65.670247
1503.533188	57.706625	65.675252
1503.030061	47.050405	65.680257
1503.124801	42.219266	65.685262
1502.474612	47.354911	65.690266
1501.736443	36.761282	65.695271
1501.084755	44.177515	65.700276
1500.481445	44.398067	65.705281
1499.311431	44.604592	65.710286
1498.341190	52.050951	65.715290
1497.860558	47.871082	65.720295
1497.278271	49.307320	65.725300
1497.300213	41.906189	65.730305
1496.706187	44.295227	65.735310
1495.299043	50.281319	65.740314
1494.765111	37.706055	65.745319
1494.174997	47.902230	65.750324
1493.614679	36.651115	65.755329
1492.718649	39.589634	65.760334
1491.587872	42.795701	65.765338
1491.746784	37.995368	65.770343
1491.289049	47.169107	65.775348
1490.426295	46.475224	65.780353
1489.677464	45.272789	65.785358
1488.828708	43.960073	65.790362
1488.517192	34.248006	65.795367
1487.432629	52.281629	65.800372
1486.392036	46.730442	65.805377
1485.638756	39.829414	65.810382
1485.348659	41.321725	65.815386
1485.226486	35.293418	65.820391
1484.745421	36.823962	65.825396
1484.168723	42.342182	65.830401
1483.213937	35.880047	65.835406
1482.159286	47.309146	65.840410
1481.873974	35.326758	65.845415
1480.262238	44.139822	65.850420
1479.847918	44.948531	65.855425
1479.484160	43.967187	65.860430
1479.087659	47.707872	65.865434
1478.811242	44.701965	65.870439
1477.663771	49.052444	65.875444
1477.100871	41.190730	65.880449
1476.543747	43.283738	65.885454
1475.819631	44.646322	65.890458
1474.803332	42.939177	65.895463
1473.966075	50.523685	65.900468
1473.906396	51.446351	65.905473
1473.718633	46.305281	65.910478
1472.426690	51.405723	65.915482
1471.843626	41.706848	65.920487
1470.885777	44.998986	65.925492
1470.428014	46.208851	65.930497
1469.821990	40.760505	65.935502
1468.652834	45.034006	65.940506
1468.515933	42.641461	65.945511
1467.754106	41.977280	65.950516
1467.498643	46.532942	65.955521
1466.448990	46.199942	65.960526
1465.150520	46.950464	65.965530
1465.209150	49.415564	65.970535
1464.608348	52.299289	65.975540
1464.101931	48.707018	65.980545
1463.117016	41.965817	65.985550
1462.009444	46.524434	65.990554
1461.736722	45.451351	65.995559
1461.531316	37.143308	66.000564
1460.409618	44.422927	66.005569
1459.754811	41.885604	66.010574
1459.054603	47.674203	66.015578
1458.769475	47.328515	66.020583
1458.076293	44.347844	66.025588
1456.753733	36.206310	66.030593
1456.386237	37.860740	66.035598
1455.517054	44.109870	66.040602
1455.562565	44.629451	66.045607
1454.970874	41.249440	66.050612
1453.839317	37.360699	66.055617
1453.547486	45.940351	66.060622
1452.364640	40.613647	66.065626
1452.417803	32.652457	66.070631
1451.211367	43.757167	66.075636
1450.701662	34.622251	66.080641
1450.152096	32.899287	66.085646
1448.518909	37.976697	66.090650
1448.070865	37.037140	66.095655
1447.072228	46.268463	66.100660
1447.373815	39.027903	66.105665
1446.833482	45.776723	66.110670
1446.436411	46.153749	66.115674
1445.840742	35.767738	66.120679
1444.582921	45.648978	66.125684
1443.816047	45.969658	66.130689
1443.803824	40.458484	66.135694
1442.750739	46.836198	66.140698
1441.984187	41.072739	66.145703
1440.997801	43.648731	66.150708
1440.305501	43.826668	66.155713
1440.445939	51.350415	66.160718
1439.440949	45.979678	66.165722
1438.579704	35.993860	66.170727
1437.806330	47.457116	66.175732
1437.733397	44.176014	66.180737
1436.768478	46.682362	66.185742
1435.617807	52.028459	66.190746
1435.067899	43.432960	66.195751
1434.717286	52.003035	66.200756
1434.202798	45.218617	66.205761
1433.666389	47.343036	66.210766
1432.794589	47.169446	66.215770
1432.222161	36.562118	66.220775
1431.520948	50.932945	66.225780
1431.106483	42.825294	66.230785
1430.250024	40.622815	66.235790
1429.185510	50.132706	66.240794
1429.028636	43.780324	66.245799
1428.075448	41.066499	66.250804
1427.270053	47.531011	66.255809
1426.930763	49.568906	66.260814
1425.913859	48.681919	66.265818
1425.946797	48.291989	66.270823
1424.695578	48.434182	66.275828
1424.215975	40.578169	66.280833
1423.976091	40.343569	66.285838
1423.066902	45.804256	66.290842
1422.254985	42.874009	66.295847
1421.280094	40.704550	66.300852
1420.937756	43.643399	66.305857
1420.365863	43.515188	66.310862
1419.304031	52.188845	66.315866
1418.419519	51.466905	66.320871
1417.713915	43.299872	66.325876
1417.496967	39.491288	66.330881
1417.399279	41.949690	66.335886
1416.304887	41.407772	66.340890
1415.675498	34.319919	66.345895
1414.436446	41.714403	66.350900
1414.097362	41.617001	66.355905
1414.196213	36.081868	66.360910
1413.054413	52.566526	66.365914
1412.352118	43.788667	66.370919
1411.831914	45.164590	66.375924
1410.929405	37.505116	66.380929
1410.177167	39.603917	66.385934
1409.025109	44.882431	66.390938
1408.912953	37.490008	66.395943
1408.173265	48.632515	66.400948
1407.851563	49.016492	66.405953
1407.523984	47.091090	66.410958
1406.531871	53.719333	66.415962
1405.727054	42.666384	66.420967
1405.193710	42.177223	66.425972
1403.871500	47.960618	66.430977
1403.277026	39.775929	66.435982
1402.436986	50.961199	66.440986
1402.438960	47.004273	66.445991
1401.748804	47.956189	66.450996
1401.562486	38.279434	66.456001
1400.563342	41.914061	66.461006
1399.502553	51.721425	66.466010
1399.467141	48.950041	66.471015
1398.655680	52.387677	66.476020
1397.694385	47.932561	66.481025
1396.951424	34.835453	66.486030
1396.598939	44.511302	66.491034
1396.087472	39.592014	66.496039
1395.173165	48.713751	66.501044
1394.361094	38.157144	66.506049
1393.863301	50.541732	66.511054
1392.914643	44.436640	66.516058
1392.135761	36.576168	66.521063
1391.252222	40.242886	66.526068
1390.767529	53.980042	66.531073
1390.526767	43.946075	66.536078
1389.759431	51.013272	66.541082
1389.902716	41.684685	66.546087
1388.903736	42.701462	66.551092
1387.662236	52.909728	66.556097
1387.613085	40.429334	66.561102
1386.404124	43.721991	66.566106
1385.843650	38.965042	66.571111
1385.375118	52.543505	66.576116
1384.349243	43.266718	66.581121
1384.385167	37.091862	66.586126
1382.922173	52.733422	66.591130
1382.681500	53.175487	66.596135
1382.031673	43.012575	66.601140
1381.385859	50.449976	66.606145
1380.662237	41.825336	66.611150
1379.336647	56.811105	66.616154
1378.952478	34.808395	66.621159
1378.715986	56.340655	66.626164
1378.337366	47.117105	66.631169
1377.286804	38.563363	66.636174
1376.154591	46.573260	66.641178
1376.356614	44.174157	66.646183
1375.539615	45.609882	66.651188
1374.279111	44.914609	66.656193
1373.929103	44.691211	66.661198
1372.938655	47.903406	66.666202
1372.938820	41.079777	66.671207
1372.409090	50.876849	66.676212
1371.536452	46.934372	66.681217
1371.091113	39.769963	66.686222
1369.963334	45.497232	66.691226
1369.019242	45.175878	66.696231
1368.093787	54.006075	66.701236
1367.565158	47.832646	66.706241
1367.283038	43.208078	66.711246
1366.762085	51.574990	66.716250
1366.672381	40.119791	66.721255
1365.559119	52.561219	66.726260
1364.835598	39.546189	66.731265
1364.408711	53.673138	66.736270
1363.562324	46.785376	66.741274
1362.590565	48.578454	66.746279
1361.898294	48.664941	66.751284
1361.668533	50.071977	66.756289
1360.925969	46.629238	66.761294
1359.577283	53.899248	66.766298
1359.472685	39.476918	66.771303
1358.728260	46.969422	66.776308
1358.417451	40.985307	66.781313
1357.313931	49.353362	66.786318
1356.230629	50.774655	66.791322
1355.942378	44.258657	66.796327
1355.709199	48.367645	66.801332
1355.103619	38.629810	66.806337
1354.454023	50.735749	66.811342
1353.330803	52.868309	66.816346
1352.543637	39.202637	66.821351
1352.465608	54.300759	66.826356
1351.608942	45.031782	66.831361
1350.587366	50.168148	66.836366
1349.890134	47.271735	66.841370
1349.558413	41.234174	66.846375
1348.725527	49.532400	66.851380
1348.323686	45.090875	66.856385
1347.820314	48.727135	66.861390
1346.606989	49.800083	66.866394
1346.604600	46.223911	66.871399
1346.014515	48.572929	66.876404
1344.943579	56.926350	66.881409
1344.414644	42.626673	66.886414
1343.404871	56.120867	66.891418
1342.910458	42.470159	66.896423
1341.912995	41.066014	66.901428
1341.036299	48.538548	66.906433
1340.695518	41.310214	66.911438
1340.560787	45.783609	66.916442
1340.113371	41.915476	66.921447
1338.815654	47.002701	66.926452
1338.229234	50.076559	66.931457
1337.999085	47.769814	66.936462
1337.339541	49.527460	66.941466
1336.383905	39.618193	66.946471
1335.546028	49.366482	66.951476
1335.166849	56.737851	66.956481
1334.947187	40.416179	66.961486
1333.601039	50.442397	66.966490
1333.142170	46.520890	66.971495
1332.289326	45.341346	66.976500
1331.298290	44.276815	66.981505
1330.527221	45.023986	66.986510
1329.855432	44.832827	66.991514
1329.664092	41.668331	66.996519
1329.111416	43.498878	67.001524
1328.773321	49.684114	67.006529
1328.476423	41.409560	67.011534
1327.489141	42.170604	67.016538
1326.664257	49.127110	67.021543
1325.223742	50.907990	67.026548
1324.414464	48.562424	67.031553
1323.985607	48.414649	67.036558
1323.625067	40.047710	67.041562
1323.570837	40.906431	67.046567
1323.019305	42.284197	67.051572
1322.127204	48.984877	67.056577
1321.470213	49.475787	67.061582
1320.396471	43.053134	67.066586
1319.714116	48.356361	67.071591
1318.671329	44.873054	67.076596
1318.009948	43.322443	67.081601
1317.689057	44.655658	67.086606
1316.988944	43.877628	67.091610
1317.143103	31.044799	67.096615
1315.958326	53.405918	67.101620
1315.004424	42.334132	67.106625
1314.756728	41.760152	67.111630
1314.323093	50.764490	67.116634
1313.246159	41.786025	67.121639
1312.433349	51.746385	67.126644
1311.938275	44.869026	67.131649
1311.460301	50.071950	67.136654
1310.176191	49.262186	67.141658
1309.690462	48.164637	67.146663
1308.800241	48.405616	67.151668
1308.183628	43.236552	67.156673
1308.197600	47.878700	67.161678
1307.520028	46.023151	67.166682
1306.931514	48.728329	67.171687
1305.792705	43.913533	67.176692
1305.281594	41.441720	67.181697
1304.924460	42.932091	67.186702
1303.502674	45.315573	67.191706
1303.368148	34.585051	67.196711
1302.917269	44.237121	67.201716
1302.154335	51.573305	67.206721
1301.281581	37.875532	67.211726
1300.321935	40.639717	67.216730
1300.345123	36.922284	67.221735
1299.621253	36.152768	67.226740
1298.514667	38.022500	67.231745
1298.000837	31.616502	67.236750
1297.035875	44.960065	67.241754
1296.731004	37.036883	67.246759
1296.429548	40.753014	67.251764
1295.155036	39.304623	67.256769
1294.696701	36.630451	67.261774
1294.102696	41.509614	67.266778
1293.533491	39.326170	67.271783
1292.633965	35.763327	67.276788
1291.713189	38.251667	67.281793
1291.570305	29.618316	67.286798
1290.756389	40.818371	67.291802
1290.453106	30.508937	67.296807
1289.626139	32.851470	67.301812
1289.053344	28.662654	67.306817
1288.310573	32.958322	67.311822
1287.547624	36.077602	67.316826
1286.889457	31.744658	67.321831
1286.125529	43.829352	67.326836
1285.345695	40.794700	67.331841
1284.610278	37.713563	67.336846
1283.608916	41.591441	67.341850
1283.083715	31.326754	67.346855
1282.852093	47.576836	67.351860
1282.546818	43.424333	67.356865
1281.877577	42.830645	67.361870
1280.893705	43.897103	67.366874
1280.389077	41.078902	67.371879
1279.761445	47.188746	67.376884
1278.593078	44.529695	67.381889
1277.991687	40.154608	67.386894
1277.333996	42.638971	67.391898
1276.683501	40.451109	67.396903
1276.446534	35.551288	67.401908
1275.452341	42.351791	67.406913
1274.778720	43.463542	67.411918
1274.073912	47.007259	67.416922
1273.776514	36.553381	67.421927
1273.192351	38.481988	67.426932
1272.532820	47.522244	67.431937
1271.654327	42.798544	67.436942
1270.984941	48.106026	67.441946
1270.470947	43.344871	67.446951
1269.315390	40.691674	67.451956
1268.656084	43.816559	67.456961
1268.778972	37.823430	67.461966
1267.802719	36.822809	67.466970
1266.808670	42.872639	67.471975
1266.108705	43.496556	67.476980
1265.493223	34.405324	67.481985
1265.154906	43.022333	67.486990
1264.452328	45.748810	67.491994
1263.652952	35.152394	67.496999
1262.814589	41.300477	67.502004
1262.318544	41.762656	67.507009
1262.134526	35.113408	67.512014
1260.883087	50.221467	67.517018
1260.029658	41.869833	67.522023
1259.780019	37.538173	67.527028
1258.940646	45.250804	67.532033
1258.918805	35.669354	67.537038
1257.543911	46.138578	67.542042
1256.915748	37.642316	67.547047
1256.161175	44.510384	67.552052
1255.937223	44.222804	67.557057
1255.456868	40.244806	67.562062
1253.827308	46.313689	67.567066
1253.863865	42.250344	67.572071
1253.125624	46.807086	67.577076
1252.696384	40.718817	67.582081
1251.370919	41.746558	67.587086
1250.822033	35.805053	67.592090
1250.573140	38.460970	67.597095
1250.084097	40.204141	67.602100
1249.437229	43.915274	67.607105
1248.647971	34.302883	67.612110
1247.495868	49.095519	67.617114
1247.424473	31.810411	67.622119
1247.180474	35.772883	67.627124
1245.569533	29.960835	67.632129
1245.177871	37.931868	67.637134
1244.646568	34.018748	67.642138
1244.132656	36.127007	67.647143
1243.099389	32.757344	67.652148
1242.592639	27.757711	67.657153
1242.582888	24.138564	67.662158
1241.031803	46.599726	67.667162
1240.417368	31.731780	67.672167
1239.725847	34.074868	67.677172
1239.227126	34.979038	67.682177
1238.800436	38.163136	67.687182
1237.596077	32.040429	67.692186
1237.189635	33.806737	67.697191
1237.073967	41.908933	67.702196
1235.710047	36.691564	67.707201
1235.045381	30.123483	67.712206
1234.036997	37.079223	67.717210
1233.785048	36.939603	67.722215
1233.233675	34.248699	67.727220
1232.675708	37.816384	67.732225
1232.675531	32.140880	67.737230
1231.538143	49.105865	67.742234
1231.209466	34.525227	67.747239
1229.811896	32.454600	67.752244
1228.823014	36.680606	67.757249
1228.365006	31.347573	67.762254
1227.627848	41.933022	67.767258
1227.510488	41.407714	67.772263
1226.965529	40.237596	67.777268
1226.356545	48.323622	67.782273
1225.722085	37.754614	67.787278
1224.602384	32.362796	67.792282
1223.111851	36.813660	67.797287
1222.830349	39.782279	67.802292
1222.816304	37.070588	67.807297
1222.392529	34.045573	67.812302
1221.324013	40.760138	67.817306
1221.122081	38.308567	67.822311
1220.350053	40.793778	67.827316
1219.517542	37.217152	67.832321
1219.381146	32.559976	67.837326
1217.854650	40.552198	67.842330
1217.091718	37.994291	67.847335
1216.423973	35.602603	67.852340
1215.749736	36.206672	67.857345
1216.145203	29.754661	67.862350
1215.082904	44.544849	67.867354
1213.844393	30.109693	67.872359
1213.527454	43.858806	67.877364
1212.776140	40.535783	67.882369
1212.320300	40.710872	67.887374
1211.400738	35.304579	67.892378
1210.924064	44.650089	67.897383
1210.489351	37.715852	67.902388
1209.657677	42.916685	67.907393
1208.566029	31.929156	67.912398
1207.659244	45.160194	67.917402
1207.237055	41.045220	67.922407
1207.087547	32.626618	67.927412
1206.351762	45.653839	67.932417
1205.691769	33.460649	67.937422
1204.727953	38.542931	67.942426
1204.235678	32.979592	67.947431
1203.854585	31.330822	67.952436
1202.618674	35.507021	67.957441
1202.134058	31.416960	67.962446
1201.652832	32.770953	67.967450
1201.236716	34.417376	67.972455
1200.726965	29.214009	67.977460
1199.294174	43.008105	67.982465
1198.665626	29.890527	67.987470
1198.489116	39.373597	67.992474
1198.174569	29.637639	67.997479
1197.073918	43.626506	68.002484
1196.323438	30.462086	68.007489
1196.267400	37.245096	68.012494
1194.612338	31.959721	68.017498
1193.900188	34.785510	68.022503
1193.576179	40.024675	68.027508
1192.566104	38.165266	68.032513
1192.781542	37.449835	68.037518
1191.541949	34.285688	68.042522
1190.672243	37.545766	68.047527
1189.954434	40.265221	68.052532
1189.185720	33.630908	68.057537
1189.349607	41.949637	68.062542
1189.007703	34.495218	68.067546
1187.716475	36.817784	68.072551
1187.390132	36.279191	68.077556
1186.689917	39.744135	68.082561
1185.816147	36.140179	68.087566
1184.672538	45.053211	68.092570
1184.408843	42.311836	68.097575
1184.005470	32.815516	68.102580
1182.967145	48.352555	68.107585
1182.118888	31.015175	68.112590
1181.165860	50.482728	68.117594
1181.075457	39.037133	68.122599
1180.750471	36.467150	68.127604
1180.215794	47.366560	68.132609
1179.404213	37.946197	68.137614
1178.378552	44.303080	68.142618
1178.164541	37.227303	68.147623
1176.655958	43.012841	68.152628
1175.817113	35.115470	68.157633
1175.221478	36.993881	68.162638
1174.657893	40.087004	68.167642
1174.465822	32.752267	68.172647
1174.388349	37.185014	68.177652
1174.019596	39.359300	68.182657
1173.190452	31.717440	68.187662
1171.939876	37.989452	68.192666
1171.238857	33.455195	68.197671
1170.115415	43.096751	68.202676
1169.805344	38.496374	68.207681
1169.418170	36.870655	68.212686
1168.824470	35.858119	68.217690
1167.989292	45.494834	68.222695
1167.069265	49.318817	68.227700
1166.495267	43.354518	68.232705
1166.276967	43.427180	68.237710
1165.299105	47.179934	68.242714
1164.341917	38.282645	68.247719
1164.039162	42.523346	68.252724
1163.149314	43.585933	68.257729
1163.053560	38.401098	68.262734
1161.749194	39.214212	68.267738
1160.858195	45.775195	68.272743
1160.672432	46.331552	68.277748
1160.349291	38.547714	68.282753
1159.482464	38.359234	68.287758
1158.174596	48.261949	68.292762
1157.607765	42.067847	68.297767
1157.612367	43.462856	68.302772
1156.788723	37.587942	68.307777
1156.286022	41.854136	68.312782
1154.978738	37.232586	68.317786
1154.975758	38.294476	68.322791
1154.317968	39.305965	68.327796
1153.476147	39.851545	68.332801
1152.857963	33.738159	68.337806
1152.160154	46.877624	68.342810
1151.627325	43.321170	68.347815
1150.577419	49.394117	68.352820
1150.127981	42.038810	68.357825
1149.777580	31.430964	68.362830
1148.613765	47.762275	68.367834
1147.726262	39.820611	68.372839
1147.235300	37.545909	68.377844
1146.486912	42.766629	68.382849
1146.379465	31.057245	68.387854
1145.596343	37.906220	68.392858
1145.174629	33.354357	68.397863
1144.203136	37.009907	68.402868
1143.423763	42.550956	68.407873
1143.029684	39.056017	68.412878
1141.557913	40.638534	68.417882
1141.299703	34.064184	68.422887
1140.857024	37.039520	68.427892
1140.452812	35.225700	68.432897
1139.880675	30.339785	68.437902
1138.282870	40.688387	68.442906
1138.208583	29.126700	68.447911
1137.626584	44.794599	68.452916
1137.259789	37.927638	68.457921
1136.203922	30.802051	68.462926
1135.472051	27.256762	68.467930
1134.858601	39.591941	68.472935
1133.939233	36.524340	68.477940
1132.866354	41.528585	68.482945
1132.663726	32.240843	68.487950
1132.108609	45.773942	68.492954
1131.689991	35.970967	68.497959
1131.621728	44.519795	68.502964
1130.383443	42.676208	68.507969
1129.955131	30.155244	68.512974
1128.863493	29.420619	68.517978
1128.313529	40.143471	68.522983
1127.593111	42.942207	68.527988
1126.795933	37.659989	68.532993
1126.448708	37.879321	68.537998
1125.888341	40.745642	68.543002
1124.721207	29.438210	68.548007
1124.145284	37.225664	68.553012
1123.046136	36.744556	68.558017
1123.322280	43.398245	68.563022
1122.785600	40.246123	68.568026
1121.748153	33.362047	68.573031
1120.606374	29.713223	68.578036
1120.164883	30.986791	68.583041
1120.011497	37.916961	68.588046
1119.049378	39.446811	68.593050
1117.953004	31.712646	68.598055
1117.600866	38.165060	68.603060
1117.146685	40.022560	68.608065
1116.855489	30.012451	68.613070
1115.557004	42.464482	68.618074
1115.089204	34.494713	68.623079
1114.354571	28.459789	68.628084
1113.830538	41.644944	68.633089
1113.358281	35.461047	68.638094
1111.941511	40.619351	68.643098
1111.716211	37.122804	68.648103
1111.483187	33.515520	68.653108
1110.391602	37.893525	68.658113
1109.595140	28.566202	68.663118
1108.882537	33.970476	68.668122
1108.702875	24.764248	68.673127
1108.018223	43.169584	68.678132
1106.775598	40.754248	68.683137
1106.464593	30.942840	68.688142
1106.033303	30.508476	68.693146
1105.620486	32.556522	68.698151
1104.839999	28.914894	68.703156
1103.789187	43.103233	68.708161
1103.432663	33.868361	68.713166
1102.031754	41.883245	68.718170
1101.341381	35.428109	68.723175
1100.704754	45.792581	68.728180
1100.188954	34.141850	68.733185
1100.125913	28.582015	68.738190
1099.353639	40.522980	68.743194
1099.056747	34.226035	68.748199
1098.174816	33.863354	68.753204
1097.542681	36.200186	68.758209
1096.728913	30.198357	68.763214
1095.343052	32.301835	68.768218
1095.108466	31.102879	68.773223
1094.491052	41.623569	68.778228
1094.168620	34.244135	68.783233
1093.311275	33.361867	68.788238
1092.585728	39.848449	68.793242
1091.802253	36.491159	68.798247
1091.263027	37.379721	68.803252
1090.809115	37.092465	68.808257
1090.038420	34.283515	68.813262
1089.023014	41.626785	68.818266
1088.678235	28.332433	68.823271
1088.132568	32.779727	68.828276
1087.232330	36.630548	68.833281
1086.840145	33.616305	68.838286
1085.935479	31.133029	68.843290
1085.352411	40.036565	68.848295
1084.955682	31.479895	68.853300
1083.857077	33.747426	68.858305
1083.260366	31.003846	68.863310
1082.686210	35.126081	68.868314
1082.159111	36.966800	68.873319
1081.484166	33.396702	68.878324
1080.285586	38.588123	68.883329
1080.313047	30.834480	68.888334
1079.663421	38.032829	68.893338
1078.741959	36.198796	68.898343
1078.011689	36.277212	68.903348
1077.098347	40.808231	68.908353
1076.974703	44.399897	68.913358
1076.195066	43.442193	68.918362
1075.259936	36.239078	68.923367
1074.796279	32.144924	68.928372
1074.187039	30.414195	68.933377
1073.996429	35.377461	68.938382
1072.708610	42.833460	68.943386
1071.880578	33.172116	68.948391
1071.687468	23.898646	68.953396
1070.769246	38.994749	68.958401
1070.109785	22.615395	68.963406
1069.038267	38.726238	68.968410
1068.615065	24.968117	68.973415
1068.250685	27.773306	68.978420
1067.896282	30.382938	68.983425
1067.161045	23.774102	68.988430
1065.996188	27.788452	68.993434
1065.883816	29.235183	68.998439
1065.176415	34.551904	69.003444
1063.893544	32.767486	69.008449
1063.405877	27.188470	69.013454
1062.886686	36.427207	69.018458
1062.476283	34.387297	69.023463
1061.399146	31.124045	69.028468
1060.346375	32.606834	69.033473
1060.060769	32.336964	69.038478
1059.775205	39.464785	69.043482
1059.465505	27.215144	69.048487
1058.639987	35.621071	69.053492
1057.962280	37.651338	69.058497
1057.333845	25.952312	69.063502
1055.806388	39.910550	69.068506
1055.500101	33.692381	69.073511
1055.061812	37.261559	69.078516
1054.224209	41.018846	69.083521
1053.868273	29.842610	69.088526
1052.789519	41.562675	69.093530
1052.481467	31.812311	69.098535
1051.948836	40.340387	69.103540
1050.366034	45.626065	69.108545
1049.958795	34.495835	69.113550
1049.165067	38.954216	69.118554
1048.667012	24.949382	69.123559
1048.466186	33.011494	69.128564
1048.192070	37.746766	69.133569
1047.767098	39.199073	69.138574
1046.519471	44.549704	69.143578
1045.793219	38.794173	69.148583
1045.080273	33.394506	69.153588
1043.680355	40.786345	69.158593
1043.306372	36.483961	69.163598
1042.911783	31.703871	69.168602
1042.717212	34.652366	69.173607
1042.253466	37.694147	69.178612
1041.376611	41.367794	69.183617
1040.671023	35.421316	69.188622
1039.864884	37.008383	69.193626
1039.216825	32.790605	69.198631
1038.200893	34.647599	69.203636
1037.275085	40.431172	69.208641
1037.227888	27.693483	69.213646
1036.977207	34.246457	69.218650
1035.919594	36.504332	69.223655
1035.162505	38.398997	69.228660
1034.395533	40.356738	69.233665
1034.136456	34.156293	69.238670
1032.649963	42.364604	69.243674
1032.654944	28.262395	69.248679
1031.854626	30.422565	69.253684
1031.239393	42.404793	69.258689
1030.575334	32.036118	69.263694
1029.288405	41.228266	69.268698
1028.761844	36.962775	69.273703
1028.634356	30.282492	69.278708
1027.918685	35.982170	69.283713
1027.921399	37.123580	69.288718
1026.613608	45.644095	69.293722
1026.022646	28.966842	69.298727
1025.262783	32.036812	69.303732
1023.972154	28.886394	69.308737
1023.503140	33.788295	69.313742
1022.956878	35.168437	69.318746
1022.693532	31.739459	69.323751
1022.363351	36.354337	69.328756
1021.454009	37.235565	69.333761
1020.552507	30.598000	69.338766
1019.665591	38.534299	69.343770
1019.091619	34.068191	69.348775
1018.799643	34.256669	69.353780
1018.287625	47.790016	69.358785
1017.248229	38.816776	69.363790
1016.388727	37.564283	69.368794
1016.125332	35.471030	69.373799
1015.564213	29.575696	69.378804
1014.767582	34.996514	69.383809
1014.417049	30.704599	69.388814
1013.472634	38.817209	69.393818
1012.597115	38.253260	69.398823
1011.948975	41.185609	69.403828
1011.271893	46.338246	69.408833
1010.814411	35.075668	69.413838
1010.075107	46.891557	69.418842
1008.906294	41.458770	69.423847
1008.509781	36.013500	69.428852
1007.984201	40.321992	69.433857
1007.529914	36.663190	69.438862
1007.361253	43.304047	69.443866
1005.878940	45.609006	69.448871
1005.424367	37.421112	69.453876
1004.783356	42.030253	69.458881
1004.505880	36.449347	69.463886
1003.086995	45.227252	69.468890
1002.641153	39.980646	69.473895
1002.080920	34.689163	69.478900
1001.768937	40.387700	69.483905
1000.717808	35.087588	69.488910
999.660364	43.718097	69.493914
999.032236	40.031760	69.498919
999.157158	38.070695	69.503924
998.492335	42.141140	69.508929
997.476410	40.703801	69.513934
996.693820	38.675811	69.518938
996.198968	36.882745	69.523943
996.131463	33.192369	69.528948
994.770338	43.435579	69.533953
994.213035	32.509021	69.538958
993.512324	41.283050	69.543962
993.418997	30.117087	69.548967
992.421468	36.900861	69.553972
990.709321	36.000090	69.558977
990.791040	37.975776	69.563982
990.446169	41.350322	69.568986
989.488530	36.812799	69.573991
988.874977	30.995203	69.578996
987.949172	42.858113	69.584001
987.872966	30.610761	69.589006
987.172612	35.782871	69.594010
986.119009	36.884190	69.599015
985.713361	34.193815	69.604020
984.965594	38.528201	69.609025
984.547607	30.929023	69.614030
983.270412	34.087628	69.619034
982.740108	39.485003	69.624039
982.380495	37.888048	69.629044
981.688832	37.391052	69.634049
981.006464	31.513443	69.639054
979.952224	34.890471	69.644058
979.665299	40.596061	69.649063
979.102462	25.100258	69.654068
978.337523	40.594625	69.659073
977.966848	31.546545	69.664078
977.080008	38.531915	69.669082
976.567283	41.559423	69.674087
975.987895	31.899561	69.679092
974.803857	34.436204	69.684097
974.108646	37.506941	69.689102
973.472016	38.179207	69.694106
973.102115	37.296693	69.699111
972.771902	32.195706	69.704116
971.646074	35.415390	69.709121
971.070947	33.620910	69.714126
970.331054	31.111460	69.719130
969.964742	32.259546	69.724135
969.084578	34.796726	69.729140
968.081316	38.104144	69.734145
967.659536	39.436104	69.739150
967.101825	41.720121	69.744154
966.601209	36.393930	69.749159
966.228107	37.904229	69.754164
965.323269	48.664647	69.759169
965.024279	41.013417	69.764174
963.842781	39.219228	69.769178
962.833064	39.318488	69.774183
962.425118	42.077006	69.779188
962.021810	37.189506	69.784193
961.451252	34.123243	69.789198
960.177414	38.104517	69.794202
959.775103	37.307589	69.799207
959.273487	36.643160	69.804212
958.468690	33.177343	69.809217
957.857693	30.527535	69.814222
956.854289	39.141571	69.819226
956.430854	44.274358	69.824231
956.260328	30.849810	69.829236
955.095333	42.676670	69.834241
954.483843	35.206062	69.839246
954.059690	45.785910	69.844250
953.415980	38.687868	69.849255
952.550131	39.570083	69.854260
951.190020	46.432072	69.859265
951.112621	27.949472	69.864270
950.672829	36.152116	69.869274
950.148149	35.697945	69.874279
949.774002	29.541060	69.879284
948.535798	41.806937	69.884289
947.955756	33.938656	69.889294
947.801122	40.552047	69.894298
946.302943	41.761974	69.899303
945.751395	39.184711	69.904308
944.793041	39.920796	69.909313
944.981075	34.191706	69.914318
944.192009	44.905317	69.919322
943.550888	45.135170	69.924327
942.806726	46.830680	69.929332
942.026312	40.727402	69.934337
941.885251	34.240104	69.939342
940.510544	41.012952	69.944346
939.770136	34.561103	69.949351
939.230696	32.309932	69.954356
938.927157	41.572716	69.959361
937.822028	32.475936	69.964366
936.719092	36.217130	69.969370
936.518995	32.852218	69.974375
936.298768	37.629384	69.979380
936.048398	32.179799	69.984385
935.021799	28.971643	69.989390
934.083954	31.041760	69.994394
933.433770	31.410256	69.999399
933.262506	29.084728	70.004404
932.052239	30.917492	70.009409
931.461244	29.191782	70.014414
930.496859	34.246644	70.019418
930.073729	24.752753	70.024423
929.586471	26.718050	70.029428
928.188114	31.621194	70.034433
927.943465	29.947604	70.039438
927.497641	30.628942	70.044442
927.200539	30.177986	70.049447
926.128821	24.009112	70.054452
925.045248	34.572462	70.059457
924.769825	26.124268	70.064462
924.623626	34.899951	70.069466
923.658488	34.957438	70.074471
923.001820	35.285967	70.079476
922.047442	35.824303	70.084481
921.845622	40.071825	70.089486
921.192966	28.124384	70.094490
919.928729	26.187262	70.099495
919.315414	31.031714	70.104500
918.912500	36.915040	70.109505
918.773072	31.094556	70.114510
917.443785	32.115191	70.119514
916.696556	26.869264	70.124519
916.457141	29.094751	70.129524
915.992978	32.157118	70.134529
914.975430	32.226103	70.139534
913.806775	35.832681	70.144538
913.525798	33.349567	70.149543
913.174193	33.552277	70.154548
912.310015	36.627841	70.159553
911.387275	36.536656	70.164558
910.643129	42.193585	70.169562
910.657206	38.534386	70.174567
910.037497	34.498221	70.179572
908.792986	35.737188	70.184577
908.250977	25.760736	70.189582
907.501994	35.047097	70.194586
907.185953	33.548879	70.199591
906.516665	32.004373	70.204596
905.230589	42.864897	70.209601
905.029428	36.836611	70.214606
904.324602	33.266592	70.219610
904.209072	39.072645	70.224615
903.226671	33.831030	70.229620
902.134918	38.426766	70.234625
901.633058	30.995503	70.239630
901.245403	41.157945	70.244634
900.400143	37.413151	70.249639
899.938529	37.936154	70.254644
898.691509	47.459485	70.259649
898.611832	42.416410	70.264654
897.232040	42.013182	70.269658
896.912262	42.486804	70.274663
896.661774	37.945591	70.279668
895.706100	49.414302	70.284673
895.461543	40.857112	70.289678
894.390214	38.193847	70.294682
893.748728	36.838890	70.299687
893.407279	31.664011	70.304692
892.873865	50.359123	70.309697
892.012065	38.224191	70.314702
891.053813	38.744231	70.319706
890.423497	40.356980	70.324711
889.853089	32.540802	70.329716
888.697108	40.236099	70.334721
888.178129	37.705709	70.339726
887.715844	40.548581	70.344730
886.705647	37.862974	70.349735
886.984862	27.353695	70.354740
886.241375	47.108859	70.359745
885.561919	42.495566	70.364750
884.756352	32.149467	70.369754
883.750186	32.081032	70.374759
882.789818	29.685550	70.379764
881.594148	31.172229	70.384769
881.671069	33.489302	70.389774
881.016537	36.468430	70.394778
880.819486	37.925490	70.399783
880.543140	37.218916	70.404788
879.448493	40.260206	70.409793
878.522776	35.074237	70.414798
878.125785	38.990113	70.419802
877.140214	35.726565	70.424807
876.668122	31.753651	70.429812
875.992081	33.834162	70.434817
875.735349	30.740052	70.439822
874.992628	32.662437	70.444826
874.121222	34.630536	70.449831
873.816045	29.203878	70.454836
873.055476	31.488658	70.459841
871.747357	36.481551	70.464846
871.216261	33.782779	70.469850
870.165848	34.476771	70.474855
870.301915	36.565229	70.479860
869.398014	39.390078	70.484865
868.299749	37.491223	70.489870
867.503561	32.331953	70.494874
867.120886	35.710951	70.499879
866.674697	34.757014	70.504884
866.374241	46.413190	70.509889
865.831843	34.175397	70.514894
864.636202	38.322470	70.519898
864.206680	43.166069	70.524903
863.812981	35.326504	70.529908
862.682453	41.407649	70.534913
862.052350	31.718050	70.539918
861.570083	42.619394	70.544922
860.752800	40.924986	70.549927
859.568837	34.892279	70.554932
858.942019	40.111064	70.559937
858.729963	29.588511	70.564942
858.348040	33.725923	70.569946
857.863681	38.505707	70.574951
857.011097	29.498090	70.579956
856.080128	40.565470	70.584961
855.696686	30.256280	70.589966
854.919930	37.974811	70.594970
853.856276	36.570361	70.599975
853.338518	34.249526	70.604980
852.970786	34.289227	70.609985
852.772610	25.715210	70.614990
851.577907	39.163248	70.619994
850.638958	39.410565	70.624999
850.352383	32.567962	70.630004
849.692703	34.879270	70.635009
848.977463	27.650725	70.640014
848.038635	37.052473	70.645018
847.343811	34.281992	70.650023
847.544010	29.169148	70.655028
845.974771	31.674116	70.660033
845.196311	29.021031	70.665038
844.466724	26.185122	70.670042
844.061734	35.539747	70.675047
844.309878	31.636710	70.680052
843.114578	28.097470	70.685057
842.287609	31.313792	70.690062
841.463137	31.993912	70.695066
841.274359	28.449010	70.700071
840.277851	31.600853	70.705076
839.297393	35.891885	70.710081
839.077869	33.006329	70.715086
838.493285	36.439546	70.720090
837.743747	37.199205	70.725095
836.666359	33.838323	70.730100
835.748877	40.193081	70.735105
835.437502	27.529014	70.740110
835.263371	31.593928	70.745114
835.041002	32.408453	70.750119
833.942086	35.010458	70.755124
832.918570	40.683487	70.760129
832.568840	30.285357	70.765134
831.734011	33.712674	70.770138
830.723095	36.455219	70.775143
830.696264	31.463668	70.780148
829.866392	34.846041	70.785153
829.412644	22.562620	70.790158
828.399549	26.150779	70.795162
827.962904	28.302007	70.800167
827.298998	32.832823	70.805172
825.918567	35.088547	70.810177
825.612646	29.709326	70.815182
825.107221	28.722248	70.820186
824.768438	38.383314	70.825191
823.876002	29.869346	70.830196
822.710236	38.321604	70.835201
822.327426	27.816777	70.840206
821.988846	36.560000	70.845210
821.307433	34.769860	70.850215
820.412356	34.634880	70.855220
819.484402	37.778973	70.860225
819.220245	31.822233	70.865230
818.767456	32.413233	70.870234
818.030654	32.032281	70.875239
817.056544	26.322597	70.880244
816.323900	37.651736	70.885249
815.889150	33.266027	70.890254
815.481851	35.071956	70.895258
814.454853	41.882559	70.900263
813.988823	27.186715	70.905268
813.084442	38.738740	70.910273
812.849002	35.830488	70.915278
811.800204	35.984916	70.920282
811.110536	29.402034	70.925287
810.978477	26.857383	70.930292
810.150955	34.923056	70.935297
809.201729	36.892525	70.940302
808.253845	43.043968	70.945306
807.415445	44.035407	70.950311
807.887367	27.373562	70.955316
806.545403	39.274372	70.960321
805.598637	38.174621	70.965326
804.852241	41.887499	70.970330
804.792045	31.610447	70.975335
804.680218	35.651253	70.980340
803.203488	36.474639	70.985345
802.670683	28.696661	70.990350
802.178103	33.813660	70.995354
801.522238	37.515280	71.000359
800.255936	37.869921	71.005364
799.601967	46.780054	71.010369
799.352922	31.013585	71.015374
798.569461	35.093495	71.020378
798.338789	30.582262	71.025383
797.759167	33.581023	71.030388
796.594854	34.578613	71.035393
796.416011	27.862380	71.040398
795.258608	35.778715	71.045402
794.013438	32.744190	71.050407
793.754478	33.257030	71.055412
793.074551	36.249682	71.060417
792.614848	36.277223	71.065422
792.337514	35.473044	71.070426
791.906525	36.670875	71.075431
790.935126	34.576814	71.080436
790.316596	44.455887	71.085441
789.548397	33.553510	71.090446
788.461627	36.289222	71.095450
787.651560	38.583484	71.100455
787.425313	39.184159	71.105460
786.819684	45.672221	71.110465
786.461047	32.197227	71.115470
785.662763	38.370593	71.120474
784.673736	33.272015	71.125479
784.193883	32.230411	71.130484
783.767530	37.611268	71.135489
782.934526	34.372359	71.140494
782.016469	38.410622	71.145498
781.677245	31.524373	71.150503
781.408118	27.624830	71.155508
780.144825	42.930472	71.160513
779.577889	30.545227	71.165518
778.981487	39.854636	71.170522
778.187397	34.154156	71.175527
777.575669	33.813231	71.180532
776.469709	43.432425	71.185537
776.074538	30.759633	71.190542
775.852073	41.168603	71.195546
775.176121	33.307761	71.200551
774.357040	37.590472	71.205556
773.642973	41.582071	71.210561
773.420422	32.275488	71.215566
772.015249	32.505590	71.220570
771.441361	38.148061	71.225575
771.065561	33.369769	71.230580
770.217286	42.219371	71.235585
769.211451	34.838412	71.240590
768.720605	33.164610	71.245594
768.098287	38.385849	71.250599
767.829813	26.713208	71.255604
767.185350	40.059484	71.260609
766.396521	37.037482	71.265614
765.268156	44.137058	71.270618
764.497570	40.165956	71.275623
764.323358	31.460400	71.280628
763.891114	37.171787	71.285633
763.239023	35.429037	71.290638
762.331402	31.295245	71.295642
762.101386	35.187705	71.300647
761.190532	29.761296	71.305652
759.768641	28.215219	71.310657
759.027178	29.167586	71.315662
758.617072	36.720530	71.320666
758.229520	39.255049	71.325671
757.956647	29.314647	71.330676
757.625026	38.913072	71.335681
756.656314	31.871571	71.340686
756.135534	38.402899	71.345690
755.357449	44.008496	71.350695
754.197417	25.411293	71.355700
753.581875	35.351391	71.360705
753.166103	33.523711	71.365710
752.650254	28.881264	71.370714
751.869969	22.964130	71.375719
751.217198	21.096910	71.380724
750.292815	28.212897	71.385729
750.120469	29.733841	71.390734
749.338367	28.451775	71.395738
748.074252	36.139107	71.400743
747.922923	33.731572	71.405748
747.074262	37.175310	71.410753
746.949448	22.507174	71.415758
745.960009	27.755323	71.420762
744.951809	35.390873	71.425767
744.358109	32.765178	71.430772
743.965922	34.321124	71.435777
743.566438	35.769419	71.440782
742.686909	28.343136	71.445786
741.806010	32.302952	71.450791
741.340548	34.491899	71.455796
740.307295	37.340539	71.460801
739.810064	33.092531	71.465806
739.344199	32.179599	71.470810
738.430996	42.323218	71.475815
738.346109	34.155390	71.480820
737.055388	40.131197	71.485825
736.460052	36.315135	71.490830
736.286900	34.120815	71.495834
735.116941	23.985772	71.500839
734.289541	33.167953	71.505844
733.777785	26.151487	71.510849
733.142124	34.461028	71.515854
733.017089	31.931034	71.520858
732.233276	37.728363	71.525863
731.355820	27.890533	71.530868
730.736842	38.227009	71.535873
730.098018	32.123349	71.540878
729.565684	30.883526	71.545882
728.231762	30.498321	71.550887
727.953261	26.696476	71.555892
727.379020	30.668974	71.560897
726.982500	31.419769	71.565902
726.212327	33.967900	71.570906
724.990477	34.988877	71.575911
725.011040	27.059738	71.580916
724.307115	38.395359	71.585921
723.136604	32.972458	71.590926
722.612161	39.660496	71.595930
721.911836	35.637221	71.600935
721.724605	28.136992	71.605940
720.514506	42.420178	71.610945
719.775699	28.504253	71.615950
719.266277	35.398061	71.620954
718.741362	29.801408	71.625959
718.556017	31.232959	71.630964
717.801920	32.438090	71.635969
716.802954	27.011537	71.640974
716.298495	27.640744	71.645978
715.496437	30.840521	71.650983
714.777587	25.795156	71.655988
713.991544	35.128457	71.660993
713.500724	34.951228	71.665998
713.441561	29.379770	71.671002
711.875711	32.762663	71.676007
711.481716	27.894238	71.681012
710.842447	35.002691	71.686017
709.903440	34.918902	71.691022
709.421004	42.524371	71.696026
708.179345	39.680148	71.701031
707.540771	39.556408	71.706036
706.994194	40.186016	71.711041
706.650747	32.540345	71.716046
706.466601	27.219029	71.721050
705.812766	32.869508	71.726055
705.775009	33.932199	71.731060
704.632477	33.480261	71.736065
704.274499	23.058251	71.741070
702.753277	32.765660	71.746074
701.800613	32.996293	71.751079
701.647310	29.936203	71.756084
701.222418	31.003763	71.761089
700.231825	28.573744	71.766094
699.164543	28.262796	71.771098
698.492554	30.468864	71.776103
698.138132	23.984035	71.781108
697.787783	28.688883	71.786113
697.208201	26.682288	71.791118
696.403580	34.551949	71.796122
695.458820	32.792740	71.801127
695.055616	27.069479	71.806132
694.352905	24.391769	71.811137
693.765386	22.652952	71.816142
692.437703	28.218334	71.821146
691.997358	31.661728	71.826151
692.223179	23.974307	71.831156
691.282868	28.538123	71.836161
690.738769	24.890541	71.841166
690.567212	27.187242	71.846170
689.130205	34.763352	71.851175
688.522439	16.614444	71.856180
687.793943	33.216394	71.861185
686.631203	26.409256	71.866190
686.018369	30.835772	71.871194
685.395256	33.481927	71.876199
685.155055	25.099140	71.881204
684.311026	28.305608	71.886209
684.249278	25.431220	71.891214
683.266077	26.243900	71.896218
682.424584	33.685763	71.901223
682.005520	28.491745	71.906228
681.276397	34.936405	71.911233
680.060633	33.537330	71.916238
679.494578	32.225615	71.921242
678.993715	37.533190	71.926247
678.745780	32.206264	71.931252
678.178151	30.808065	71.936257
677.157083	27.066121	71.941262
676.311944	34.510144	71.946266
675.866208	29.460727	71.951271
675.356623	19.485501	71.956276
674.271162	31.511097	71.961281
673.680548	30.870362	71.966286
673.194186	29.117017	71.971290
672.446900	31.535360	71.976295
672.115157	23.644981	71.981300
670.744632	31.205781	71.986305
670.263630	30.645365	71.991310
670.118936	19.555453	71.996314
669.309527	20.659016	72.001319
669.093822	29.136663	72.006324
668.135924	34.548556	72.011329
667.566687	31.313422	72.016334
666.500630	30.767321	72.021338
665.298547	30.531471	72.026343
664.992320	19.962457	72.031348
664.577810	33.365162	72.036353
664.412497	23.770364	72.041358
663.163570	30.070713	72.046362
662.116280	30.275427	72.051367
661.703261	25.935181	72.056372
661.171436	23.703367	72.061377
661.137431	24.678725	72.066382
660.320792	18.841535	72.071386
659.443865	25.014835	72.076391
658.771835	17.656478	72.081396
658.103712	33.518672	72.086401
657.731249	22.294715	72.091406
656.626182	20.225151	72.096410
656.134123	23.474929	72.101415
655.536818	27.511038	72.106420
654.137218	29.165918	72.111425
653.574142	19.782703	72.116430
653.175255	20.721547	72.121434
652.905269	23.464442	72.126439
652.296084	20.729274	72.131444
651.497752	23.802315	72.136449
650.314933	27.427029	72.141454
650.113208	25.923260	72.146458
649.649583	26.415087	72.151463
649.079223	24.377074	72.156468
647.882821	25.061289	72.161473
647.262349	23.964834	72.166478
646.764262	22.762156	72.171482
646.398870	31.862897	72.176487
645.474477	28.274310	72.181492
644.415412	35.985803	72.186497
643.900929	26.173793	72.191502
643.842369	23.455022	72.196506
642.834813	31.855340	72.201511
642.275300	21.482787	72.206516
641.361761	37.437686	72.211521
640.978761	23.034622	72.216526
640.269634	27.399208	72.221530
638.896083	30.104954	72.226535
638.945548	22.376231	72.231540
638.115350	30.464447	72.236545
637.757597	29.884411	72.241550
636.829368	37.772195	72.246554
635.914765	35.561918	72.251559
635.959043	22.674109	72.256564
635.358150	34.138416	72.261569
634.363950	29.212623	72.266574
633.336700	33.471753	72.271578
632.570137	36.295310	72.276583
632.499310	21.803110	72.281588
631.582713	31.953597	72.286593
630.948404	27.763718	72.291598
630.153422	34.004407	72.296602
629.479005	34.819974	72.301607
629.341795	36.627073	72.306612
628.115285	31.752472	72.311617
627.328312	35.798293	72.316622
627.175163	32.012770	72.321626
626.362438	31.085712	72.326631
625.597364	34.191314	72.331636
624.630496	40.016246	72.336641
624.642909	32.646665	72.341646
624.166746	28.095704	72.346650
622.997117	38.117757	72.351655
622.398503	25.143094	72.356660
621.752729	25.995102	72.361665
621.129797	26.945978	72.366670
620.267901	29.929802	72.371674
619.434006	32.634772	72.376679
619.006512	14.479265	72.381684
618.242565	29.572956	72.386689
617.512256	26.547996	72.391694
616.638998	18.895264	72.396698
615.952294	25.415182	72.401703
615.860603	13.425844	72.406708
615.373244	27.124004	72.411713
614.808820	22.503524	72.416718
614.043639	20.291538	72.421722
613.142219	29.318372	72.426727
612.709414	19.241050	72.431732
611.567198	25.052904	72.436737
610.844139	19.771700	72.441742
610.339318	22.775930	72.446746
609.616556	20.771661	72.451751
609.570756	25.387011	72.456756
608.300538	32.474538	72.461761
607.439773	24.572230	72.466766
606.850596	22.808467	72.471770
606.414498	24.565394	72.476775
606.201447	26.688930	72.481780
604.819849	30.947733	72.486785
604.168741	33.191500	72.491790
603.800490	21.386556	72.496794
603.301288	23.352235	72.501799
603.421433	18.185905	72.506804
601.893289	29.523494	72.511809
601.278643	23.012321	72.516814
601.019331	23.985715	72.521818
599.404357	28.136606	72.526823
599.191704	23.477450	72.531828
598.445290	28.278504	72.536833
598.209616	26.903151	72.541838
597.556458	22.386696	72.546842
596.420031	29.530192	72.551847
596.070647	19.531053	72.556852
595.479199	33.671585	72.561857
594.425117	26.359902	72.566862
593.732985	27.638780	72.571866
592.857614	29.613910	72.576871
592.975594	21.519455	72.581876
592.104588	26.800834	72.586881
591.012020	28.895714	72.591886
590.665835	23.983431	72.596890
589.952211	25.019723	72.601895
589.620249	25.821759	72.606900
588.323284	35.920874	72.611905
587.646918	15.836933	72.616910
587.156737	22.808114	72.621914
586.955031	28.232058	72.626919
586.515467	17.988660	72.631924
585.087673	28.729942	72.636929
584.600029	30.012525	72.641934
583.964761	20.170888	72.646938
583.356030	25.263836	72.651943
582.548399	29.399692	72.656948
581.833849	22.609540	72.661953
581.090150	16.625144	72.666958
580.824869	14.929651	72.671962
580.538645	19.565944	72.676967
579.754782	19.930590	72.681972
579.214466	24.228878	72.686977
578.021014	22.600793	72.691982
577.057098	24.455985	72.696986
576.487806	24.974118	72.701991
576.255756	18.783647	72.706996
575.698270	30.534364	72.712001
575.021517	23.522146	72.717006
573.588458	23.215895	72.722010
573.214423	22.780390	72.727015
572.916385	24.898541	72.732020
572.124493	31.298026	72.737025
571.652624	20.518869	72.742030
570.999893	22.360770	72.747034
569.966148	24.165585	72.752039
569.910348	10.500510	72.757044
568.628272	21.860419	72.762049
567.853723	21.841954	72.767054
567.473600	17.646306	72.772058
566.616650	17.980018	72.777063
566.843207	18.786138	72.782068
565.364791	27.245706	72.787073
564.557453	25.523010	72.792078
564.087688	18.410019	72.797082
563.356468	25.254012	72.802087
563.531176	17.271954	72.807092
561.951263	30.287839	72.812097
561.772138	24.470569	72.817102
561.256973	18.642171	72.822106
559.987224	20.118719	72.827111
559.390449	17.785309	72.832116
558.662978	23.322960	72.837121
558.438858	25.604384	72.842126
558.046041	27.674554	72.847130
556.961472	23.013934	72.852135
556.227968	24.084942	72.857140
555.547367	19.951349	72.862145
555.230333	23.657399	72.867150
554.622867	25.165658	72.872154
553.678353	25.126960	72.877159
553.135816	23.653832	72.882164
552.385009	24.959414	72.887169
551.227122	25.539767	72.892174
550.823865	21.781477	72.897178
550.221317	25.779017	72.902183
549.751279	21.630809	72.907188
549.111060	28.207994	72.912193
548.328596	21.769301	72.917198
547.910430	23.269486	72.922202
547.174334	26.482458	72.927207
546.754029	17.604830	72.932212
545.475068	24.569192	72.937217
544.859327	24.437127	72.942222
544.639225	21.903369	72.947226
543.795717	31.815149	72.952231
542.773808	16.615010	72.957236
542.193033	20.501846	72.962241
541.617337	25.985363	72.967246
541.170689	21.125365	72.972250
540.569768	28.295546	72.977255
539.469014	20.497732	72.982260
539.265134	23.744202	72.987265
538.836672	17.972964	72.992270
537.740554	29.181841	72.997274
536.711253	22.774587	73.002279
536.308339	25.371504	73.007284
535.803255	24.233044	73.012289
535.324522	22.806528	73.017294
535.127809	21.396591	73.022298
533.898052	25.192839	73.027303
533.389294	14.151486	73.032308
532.433064	27.749293	73.037313
531.340149	28.609472	73.042318
531.137784	24.625215	73.047322
530.392532	26.365167	73.052327
529.960501	14.896845	73.057332
529.366933	25.861662	73.062337
528.162537	24.751019	73.067342
527.763695	15.642892	73.072346
526.834799	20.086667	73.077351
526.570803	21.557565	73.082356
526.154600	23.281373	73.087361
525.170659	21.968453	73.092366
524.812302	13.459442	73.097370
524.318684	16.067655	73.102375
523.485315	10.804056	73.107380
522.396352	21.884057	73.112385
521.756304	12.293951	73.117390
521.175710	15.420654	73.122394
520.760905	29.293347	73.127399
520.305507	11.167559	73.132404
518.853236	16.065300	73.137409
518.474261	16.529474	73.142414
518.125260	22.975114	73.147418
517.639986	22.264019	73.152423
516.616012	12.966890	73.157428
515.782547	22.162697	73.162433
515.432468	19.105587	73.167438
515.034383	16.339984	73.172442
513.649640	24.890312	73.177447
513.444366	27.831072	73.182452
512.833659	22.147218	73.187457
512.075139	24.326114	73.192462
511.364092	25.789380	73.197466
510.480722	32.009484	73.202471
510.204600	20.322358	73.207476
509.882707	21.638475	73.212481
508.821721	19.593498	73.217486
508.458305	23.150819	73.222490
507.619064	26.310846	73.227495
506.548331	22.961677	73.232500
505.802938	30.071300	73.237505
505.421764	19.679847	73.242510
504.856779	17.836561	73.247514
503.978542	22.534054	73.252519
503.194364	17.844532	73.257524
502.580357	24.040648	73.262529
502.250140	24.995385	73.267534
501.749857	27.297152	73.272538
500.809874	35.183693	73.277543
500.102796	23.912158	73.282548
499.311835	27.676366	73.287553
498.942366	18.771728	73.292558
498.553845	24.495098	73.297562
497.039588	28.931210	73.302567
496.590313	23.939173	73.307572
496.151159	23.427320	73.312577
495.795044	20.924698	73.317582
494.901329	7.680137	73.322586
493.670608	21.529838	73.327591
493.307644	19.509288	73.332596
493.003776	23.911852	73.337601
492.452975	24.181047	73.342606
491.797459	19.048400	73.347610
490.771884	20.520778	73.352615
490.550397	22.074795	73.357620
489.776114	25.416871	73.362625
488.582547	19.568832	73.367630
487.907467	11.296373	73.372634
487.099402	21.890079	73.377639
487.064343	15.860634	73.382644
486.964697	23.495023	73.387649
485.660347	23.956811	73.392654
485.022408	10.815011	73.397658
484.437201	26.118365	73.402663
483.521232	12.038395	73.407668
482.152363	12.493116	73.412673
481.899212	21.806218	73.417678
481.612214	18.021536	73.422682
481.186740	17.901753	73.427687
480.643578	15.954070	73.432692
479.891228	16.482464	73.437697
479.060993	18.642831	73.442702
478.834301	21.922901	73.447706
477.774551	23.940058	73.452711
477.091460	7.459092	73.457716
475.999355	23.854049	73.462721
475.670253	24.453789	73.467726
475.267232	12.009441	73.472730
474.129439	29.556574	73.477735
473.712293	19.949893	73.482740
473.190686	21.911279	73.487745
472.458832	23.634919	73.492750
471.635916	20.345636	73.497754
470.579385	25.618760	73.502759
470.367310	19.770484	73.507764
469.695970	22.681416	73.512769
469.484052	23.407570	73.517774
468.214989	19.556997	73.522778
467.424587	28.323325	73.527783
467.217535	15.492933	73.532788
466.817115	20.191583	73.537793
465.882079	18.467188	73.542798
465.216952	28.710118	73.547802
464.533278	31.157807	73.552807
464.102644	17.891516	73.557812
463.004966	18.746174	73.562817
462.669204	14.010459	73.567822
462.250755	23.761490	73.572826
461.049242	23.508301	73.577831
460.426433	24.755669	73.582836
459.626247	26.132224	73.587841
459.223857	14.660779	73.592846
458.858421	17.142922	73.597850
457.584166	20.071066	73.602855
457.177854	21.979392	73.607860
456.814229	27.296670	73.612865
455.908677	25.567581	73.617870
455.199897	16.609779	73.622874
454.092318	20.813959	73.627879
453.862064	23.982633	73.632884
453.527132	23.592958	73.637889
452.812121	24.094910	73.642894
451.889533	20.985521	73.647898
450.914312	27.075192	73.652903
450.960631	15.357212	73.657908
450.253051	24.425743	73.662913
448.842345	20.074188	73.667918
448.168197	28.017736	73.672922
447.486717	30.365729	73.677927
447.473580	15.276164	73.682932
447.019775	21.109289	73.687937
445.572363	24.150186	73.692942
445.126347	18.810706	73.697946
444.628595	28.113896	73.702951
444.433009	24.576434	73.707956
443.706999	26.963063	73.712961
442.701032	28.976396	73.717966
442.321633	27.306987	73.722970
441.480864	28.444004	73.727975
440.832091	17.180556	73.732980
439.878688	23.750887	73.737985
439.226799	28.358719	73.742990
439.196835	18.963177	73.747994
437.671750	25.326545	73.752999
436.679186	26.904074	73.758004
436.511526	34.912011	73.763009
436.113354	27.675677	73.768014
436.047132	22.471231	73.773018
434.754273	29.773756	73.778023
433.776307	21.641036	73.783028
433.176936	24.695055	73.788033
432.675981	26.539615	73.793038
432.367714	27.908765	73.798042
431.514547	21.932401	73.803047
430.709873	24.177022	73.808052
430.226815	26.766223	73.813057
429.678453	32.385758	73.818062
428.841377	17.525249	73.823066
428.283846	36.426042	73.828071
427.873136	27.802382	73.833076
426.458975	21.611049	73.838081
425.544116	22.531213	73.843086
425.129562	20.982529	73.848090
424.384802	27.798748	73.853095
424.535664	19.178658	73.858100
423.845130	28.615072	73.863105
423.240172	31.537518	73.868110
422.498331	24.045282	73.873114
421.675850	29.216476	73.878119
420.874278	18.803721	73.883124
419.839259	21.156012	73.888129
419.201914	25.529713	73.893134
418.861012	18.845670	73.898138
418.473131	25.795840	73.903143
418.400272	21.380947	73.908148
417.255438	18.748540	73.913153
416.420700	22.737370	73.918158
415.263493	23.409143	73.923162
414.343803	21.242344	73.928167
413.953858	18.346150	73.933172
413.573274	22.306771	73.938177
413.143657	16.409588	73.943182
412.736458	21.099863	73.948186
411.611450	25.623812	73.953191
410.918765	24.805436	73.958196
410.530073	17.551833	73.963201
409.324906	19.809812	73.968206
408.967199	11.401653	73.973210
407.825444	14.742378	73.978215
407.911455	20.826967	73.983220
406.949694	21.844499	73.988225
406.692003	22.155320	73.993230
405.645653	21.420109	73.998234
404.534117	26.039688	74.003239
404.594352	17.965484	74.008244
404.116295	11.260723	74.013249
403.135784	18.455137	74.018254
402.529668	18.319997	74.023258
401.528669	29.351332	74.028263
401.316921	20.699134	74.033268
400.225503	27.061231	74.038273
399.495898	29.681839	74.043278
398.960264	16.820239	74.048282
398.492834	26.834552	74.053287
397.939464	16.724465	74.058292
397.036659	23.179511	74.063297
396.451922	23.482522	74.068302
396.176521	23.435036	74.073306
395.066454	27.182312	74.078311
394.187676	17.676023	74.083316
393.644990	26.049649	74.088321
393.197434	28.251569	74.093326
393.060828	19.601592	74.098330
391.452996	28.386228	74.103335
391.158488	23.278089	74.108340
390.417983	29.494384	74.113345
389.795462	25.843607	74.118350
389.205094	23.589647	74.123354
388.439362	26.596068	74.128359
387.656187	27.580419	74.133364
387.427295	18.336434	74.138369
386.477722	23.996251	74.143374
385.940766	23.113642	74.148378
384.663218	30.822190	74.153383
384.535157	26.561176	74.158388
384.322107	26.107933	74.163393
383.493175	45.730091	74.168398
382.556931	28.761195	74.173402
381.847046	32.575597	74.178407
381.334106	26.882511	74.183412
380.135393	25.938196	74.188417
379.327784	31.230037	74.193422
379.249376	21.026918	74.198426
378.538661	34.166165	74.203431
378.301288	21.094610	74.208436
377.593385	25.651456	74.213441
376.550173	31.015535	74.218446
376.126304	20.299754	74.223450
375.384782	25.087466	74.228455
374.631071	24.225208	74.233460
373.722309	27.566669	74.238465
373.279666	31.701193	74.243470
373.127806	18.977143	74.248474
371.936127	29.753439	74.253479
371.147064	28.049974	74.258484
370.535240	21.314494	74.263489
370.061334	27.679124	74.268494
369.950489	24.569723	74.273498
368.345962	33.705516	74.278503
367.594666	28.004684	74.283508
367.370917	28.959818	74.288513
366.867807	30.104553	74.293518
366.527539	24.516422	74.298522
365.412126	28.687194	74.303527
364.494809	24.671810	74.308532
364.217336	23.531808	74.313537
363.126588	23.759343	74.318542
362.610213	17.193164	74.323546
361.834074	30.008515	74.328551
361.803750	27.993325	74.333556
361.219828	26.053742	74.338561
360.288568	27.744535	74.343566
359.935595	17.928960	74.348570
358.750136	23.164321	74.353575
357.781625	15.760278	74.358580
357.095437	24.066888	74.363585
356.446297	22.014695	74.368590
356.129419	18.755200	74.373594
355.552638	26.441969	74.378599
355.321250	23.537863	74.383604
354.054311	24.263422	74.388609
353.294080	27.891884	74.393614
353.161877	21.292868	74.398618
352.058213	24.525044	74.403623
351.075945	21.338472	74.408628
350.471710	24.270279	74.413633
349.897050	19.504845	74.418638
349.792233	8.523765	74.423642
348.960479	29.024733	74.428647
348.521470	15.404994	74.433652
347.369373	20.336993	74.438657
347.037844	25.084604	74.443662
346.491388	20.278406	74.448666
345.759780	22.658067	74.453671
344.898326	18.928687	74.458676
344.405108	16.962038	74.463681
343.885079	21.607222	74.468686
342.945727	20.277810	74.473690
341.672397	27.768079	74.478695
341.580645	21.121615	74.483700
340.939941	27.426098	74.488705
340.753486	20.176550	74.493710
339.470505	22.532120	74.498714
338.595369	25.988083	74.503719
338.469021	20.435254	74.508724
338.221175	17.156875	74.513729
337.170757	25.237681	74.518734
336.431538	21.288545	74.523738
335.868374	23.929952	74.528743
334.907314	17.234374	74.533748
334.007074	29.708379	74.538753
332.969983	24.447356	74.543758
333.196455	16.758257	74.548762
332.668186	25.913353	74.553767
331.475068	23.323377	74.558772
330.934680	17.459638	74.563777
330.156046	21.956801	74.568782
330.157285	17.891236	74.573786
329.463853	31.816225	74.578791
328.771434	20.715895	74.583796
327.940541	19.077461	74.588801
327.105884	24.387817	74.593806
326.184886	26.341921	74.598810
325.451758	33.044345	74.603815
325.566720	27.952959	74.608820
324.897727	26.528424	74.613825
323.674897	22.684755	74.618830
323.227082	28.717220	74.623834
322.659501	28.240060	74.628839
321.948393	18.301797	74.633844
320.888894	26.726261	74.638849
320.095869	23.435424	74.643854
319.885578	20.811817	74.648858
319.394910	23.775994	74.653863
318.283100	26.162643	74.658868
317.705389	20.041498	74.663873
317.014424	22.905131	74.668878
316.751428	22.235923	74.673882
315.998131	26.803172	74.678887
315.335663	19.273098	74.683892
314.249918	19.313773	74.688897
313.929465	21.003428	74.693902
313.590716	7.750935	74.698906
312.225625	24.845468	74.703911
311.684814	16.647867	74.708916
311.172992	22.647954	74.713921
310.428268	27.874595	74.718926
310.061470	22.509904	74.723930
308.627765	29.237257	74.728935
308.316794	25.853822	74.733940
308.140710	28.310537	74.738945
307.583953	30.075703	74.743950
307.275280	19.504012	74.748954
306.084089	32.262523	74.753959
305.470168	30.387660	74.758964
304.725059	23.878452	74.763969
304.023701	31.460504	74.768974
303.450191	23.394272	74.773978
302.582131	26.991048	74.778983
302.492692	16.881167	74.783988
301.298804	22.043777	74.788993
300.349847	19.637257	74.793998
300.172642	17.006803	74.799002
299.091043	17.750158	74.804007
298.046293	13.988510	74.809012
297.463732	19.058415	74.814017
296.771412	25.366400	74.819022
296.513647	13.739485	74.824026
296.270848	23.333217	74.829031
295.769658	15.167153	74.834036
295.002714	17.093558	74.839041
293.986721	13.701073	74.844046
294.100513	14.053622	74.849050
292.477185	21.497190	74.854055
291.537740	15.900499	74.859060
291.322045	22.149862	74.864065
290.845269	26.475920	74.869070
290.700011	7.605342	74.874074
289.621745	17.013685	74.879079
288.732123	15.086577	74.884084
288.346943	19.117331	74.889089
287.279043	20.266947	74.894094
286.709198	20.974471	74.899098
285.793542	23.902312	74.904103
285.502818	14.029526	74.909108
285.111677	16.597791	74.914113
284.238000	17.754297	74.919118
283.474282	16.747005	74.924122
282.624294	17.880812	74.929127
282.023101	12.952469	74.934132
281.913433	7.553113	74.939137
280.927458	22.497726	74.944142
280.480848	13.935031	74.949146
279.741930	22.980202	74.954151
279.218161	7.084225	74.959156
277.837194	15.990454	74.964161
277.242331	23.758964	74.969166
276.718954	18.409779	74.974170
276.252174	22.502428	74.979175
275.847567	24.498820	74.984180
274.771158	13.344604	74.989185
274.038223	18.935231	74.994190
273.724497	13.046419	74.999194
273.027494	15.505741	75.004199
271.944546	15.530219	75.009204
271.600083	20.989539	75.014209
270.689789	19.655524	75.019214
270.523068	10.471043	75.024218
269.595634	17.811583	75.029223
268.630229	14.702788	75.034228
267.931658	16.487412	75.039233
267.604062	21.746921	75.044238
267.359255	17.769464	75.049242
266.442805	20.244844	75.054247
265.694936	13.917448	75.059252
265.163868	17.816915	75.064257
264.197839	21.881911	75.069262
263.647138	17.216765	75.074266
262.555774	23.307662	75.079271
262.045210	24.590803	75.084276
262.044189	14.678151	75.089281
261.672476	18.197396	75.094286
260.472843	15.299408	75.099290
259.671209	12.609220	75.104295
259.272068	19.376688	75.109300
258.571893	24.900597	75.114305
257.385996	30.897756	75.119310
256.965764	21.424093	75.124314
256.226871	20.736132	75.129319
255.968945	14.418951	75.134324
254.833599	21.111384	75.139329
254.057989	21.067955	75.144334
253.696546	22.656916	75.149338
252.896360	22.776680	75.154343
252.781420	17.368702	75.159348
251.937130	20.047054	75.164353
251.342082	24.557553	75.169358
250.643576	14.018059	75.174362
250.061451	19.967858	75.179367
249.007651	21.220900	75.184372
248.032227	18.683000	75.189377
247.473479	20.748122	75.194382
247.372530	21.958085	75.199386
246.935239	14.895199	75.204391
245.900224	24.184701	75.209396
245.175396	18.962256	75.214401
244.627742	25.865369	75.219406
243.874100	14.872610	75.224410
242.697886	29.257774	75.229415
242.037089	20.976815	75.234420
241.754611	17.912132	75.239425
241.242585	32.651900	75.244430
241.424435	22.516125	75.249434
239.850021	24.773120	75.254439
239.277314	23.322222	75.259444
239.271474	20.713343	75.264449
237.948127	30.679607	75.269454
237.203450	17.900276	75.274458
236.695866	20.375144	75.279463
235.907166	14.984686	75.284468
235.242983	18.683024	75.289473
234.445090	32.178392	75.294478
233.862692	24.435303	75.299482
233.446401	31.965619	75.304487
232.989055	21.988512	75.309492
231.921143	27.522164	75.314497
231.120494	24.831827	75.319502
231.040700	18.724376	75.324506
229.622189	28.406186	75.329511
228.919237	24.774587	75.334516
228.502021	21.370255	75.339521
228.039831	24.938623	75.344526
227.797172	11.019540	75.349530
226.861904	28.816732	75.354535
226.170625	13.698116	75.359540
225.698622	19.171463	75.364545
224.635372	22.670066	75.369550
223.376105	13.615608	75.374554
222.926221	20.189315	75.379559
222.622950	22.740427	75.384564
222.331040	15.491942	75.389569
221.683908	22.494495	75.394574
220.872240	18.673646	75.399578
219.928889	23.455724	75.404583
219.328055	18.407490	75.409588
218.931707	14.324888	75.414593
218.065068	15.347828	75.419598
217.368260	9.294592	75.424602
216.716975	24.480761	75.429607
216.247769	28.852933	75.434612
216.105018	26.705858	75.439617
214.823516	18.714678	75.444622
214.486823	20.031611	75.449626
213.446450	28.544529	75.454631
212.714889	22.048966	75.459636
211.716224	25.464737	75.464641
211.197261	28.023429	75.469646
211.206827	17.520878	75.474650
210.597312	23.831450	75.479655
209.246208	18.201073	75.484660
208.873911	19.733421	75.489665
208.372465	23.569828	75.494670
207.593442	14.273234	75.499674
206.466540	24.846867	75.504679
205.717825	19.686592	75.509684
205.644500	18.011007	75.514689
204.958469	25.380895	75.519694
204.748989	21.183345	75.524698
203.916926	17.526606	75.529703
202.948044	21.013327	75.534708
202.273615	21.945705	75.539713
200.904627	17.590808	75.544718
200.353703	21.685844	75.549722
199.707417	30.654766	75.554727
199.645585	20.218792	75.559732
199.391545	19.300584	75.564737
198.685208	22.888955	75.569742
197.706444	24.107978	75.574746
197.377514	30.406939	75.579751
196.717294	19.735200	75.584756
195.509760	17.943969	75.589761
194.502227	18.308124	75.594766
194.454141	15.466282	75.599770
193.825849	21.923355	75.604775
193.224663	18.203003	75.609780
192.362459	13.373071	75.614785
191.433621	15.617058	75.619790
191.306641	9.999694	75.624794
190.387475	17.365747	75.629799
189.450905	21.460767	75.634804
189.151452	21.428179	75.639809
188.481739	17.789718	75.644814
188.259171	12.457256	75.649818
186.703961	26.087561	75.654823
186.178792	22.132736	75.659828
185.937038	29.816580	75.664833
185.129639	24.794980	75.669838
184.428817	17.668467	75.674842
183.325711	30.775680	75.679847
183.003674	24.213259	75.684852
182.617698	21.873149	75.689857
181.712761	33.712418	75.694862
180.993537	19.904013	75.699866
180.108797	17.219218	75.704871
179.827836	27.495560	75.709876
179.812767	30.229390	75.714881
178.631538	35.752745	75.719886
177.759281	24.059816	75.724890
177.155140	32.337613	75.729895
176.501795	32.402451	75.734900
175.730408	27.256838	75.739905
174.550167	32.573452	75.744910
174.315814	24.133059	75.749914
174.053847	34.061019	75.754919
173.722469	26.861409	75.759924
172.510054	25.364286	75.764929
171.815356	18.941711	75.769934
171.370997	19.872108	75.774938
170.745711	25.642721	75.779943
169.812587	16.074239	75.784948
168.899776	25.150313	75.789953
168.484364	26.706888	75.794958
168.338487	12.696693	75.799962
167.225775	20.792217	75.804967
166.239726	19.806217	75.809972
166.014543	19.728673	75.814977
164.995390	15.797423	75.819982
165.064517	13.252289	75.824986
163.717868	23.794740	75.829991
162.893510	24.905578	75.834996
162.717025	22.696076	75.840001
162.048540	30.982557	75.845006
161.952209	19.733637	75.850010
160.640682	30.221607	75.855015
160.105204	23.513446	75.860020
159.167173	20.256826	75.865025
157.759543	26.940673	75.870030
157.790572	19.120304	75.875034
157.001867	29.259982	75.880039
156.532382	31.279352	75.885044
156.463751	22.533414	75.890049
155.779644	28.597267	75.895054
154.971407	26.354452	75.900058
154.351022	23.577052	75.905063
153.719372	27.992480	75.910068
152.945534	25.523404	75.915073
151.765352	28.580204	75.920078
151.417600	20.336098	75.925082
150.626991	23.535788	75.930087
149.854442	26.551247	75.935092
149.092698	29.257472	75.940097
148.293524	31.868739	75.945102
148.375703	18.181732	75.950106
147.809374	27.415460	75.955111
146.677870	25.949603	75.960116
146.216759	20.276706	75.965121
145.406670	29.571380	75.970126
145.068476	26.630713	75.975130
144.107389	30.059443	75.980135
143.620605	21.306064	75.985140
143.351064	24.272859	75.990145
142.013858	34.419576	75.995150
141.501009	25.649850	76.000154
140.455522	31.023841	76.005159
140.248441	30.754175	76.010164
140.171388	23.666988	76.015169
138.412312	35.795430	76.020174
138.156073	22.327965	76.025178
137.887173	28.044912	76.030183
136.760641	24.111871	76.035188
135.766885	19.085313	76.040193
135.098941	30.457862	76.045198
134.994799	17.489707	76.050202
134.021636	24.504840	76.055207
133.664647	25.386619	76.060212
133.276496	30.259974	76.065217
132.065615	34.398757	76.070222
131.774746	22.786614	76.075226
131.178224	33.412904	76.080231
130.364434	29.926745	76.085236
129.292544	27.273387	76.090241
128.727414	33.575323	76.095246
128.403244	27.973632	76.100250
127.818384	25.893908	76.105255
126.472922	21.614153	76.110260
126.244423	21.721648	76.115265
125.636726	33.262792	76.120270
125.257417	24.776136	76.125274
124.365015	21.904923	76.130279
123.428953	25.921036	76.135284
123.525136	20.630795	76.140289
122.367075	26.371254	76.145294
121.492620	17.329612	76.150298
120.679601	22.642883	76.155303
120.208574	29.659955	76.160308
120.283799	21.545530	76.165313
119.221496	21.776522	76.170318
118.116189	16.791416	76.175322
117.357078	18.249838	76.180327
117.342168	18.282273	76.185332
116.844354	20.214701	76.190337
115.417602	29.371169	76.195342
114.970957	17.995190	76.200346
114.320589	22.647003	76.205351
114.064324	24.108821	76.210356
112.956893	16.233453	76.215361
111.849668	30.284378	76.220366
111.690327	23.191393	76.225370
111.123045	31.628906	76.230375
110.906755	24.390458	76.235380
109.623767	23.254710	76.240385
108.694567	34.314107	76.245390
108.756934	20.978773	76.250394
108.460343	25.523710	76.255399
107.325531	23.397647	76.260404
106.385257	29.033996	76.265409
105.389470	29.894641	76.270414
105.454767	18.290368	76.275418
104.220926	25.492162	76.280423
103.124918	26.359328	76.285428
103.128609	17.966149	76.290433
102.372431	22.514988	76.295438
102.179365	22.090123	76.300442
101.245713	18.982643	76.305447
100.014575	19.677390	76.310452
99.963808	17.247572	76.315457
98.965160	27.452279	76.320462
98.967284	20.197929	76.325466
98.126194	17.627632	76.330471
97.413183	17.312492	76.335476
97.248120	16.446339	76.340481
96.060388	19.332475	76.345486
95.131739	14.882191	76.350490
94.645896	23.494375	76.355495
94.209977	23.133471	76.360500
93.255608	14.460985	76.365505
92.138735	22.386887	76.370510
92.153063	17.630105	76.375514
91.333091	20.164278	76.380519
90.791699	21.602181	76.385524
89.811925	20.596289	76.390529
88.873472	33.535347	76.395534
88.550857	19.551771	76.400538
88.159262	27.371476	76.405543
87.211990	20.356841	76.410548
86.435584	13.717091	76.415553
85.702529	22.878062	76.420558
85.422026	20.406031	76.425562
85.037446	18.844746	76.430567
84.315716	25.671562	76.435572
83.390761	21.920871	76.440577
82.591160	22.064252	76.445582
82.173904	19.409023	76.450586
80.918498	21.337694	76.455591
80.486833	28.178179	76.460596
79.973411	19.399105	76.465601
79.617612	31.038856	76.470606
79.388587	17.251674	76.475610
77.960390	21.787840	76.480615
77.385264	16.401230	76.485620
76.918180	27.546208	76.490625
75.915903	24.990585	76.495630
75.142969	24.297071	76.500634
74.655081	27.473738	76.505639
74.363423	23.423354	76.510644
73.747546	27.957711	76.515649
72.654817	18.059908	76.520654
71.993355	22.549493	76.525658
71.440181	14.800225	76.530663
70.970075	24.382897	76.535668
70.169691	25.824261	76.540673
68.877620	34.099822	76.545678
68.694079	23.019367	76.550682
68.306347	20.133924	76.555687
67.810435	26.864805	76.560692
67.138697	13.630790	76.565697
66.013024	25.341277	76.570702
65.666280	20.847087	76.575706
64.963917	26.876022	76.580711
64.177008	32.642472	76.585716
63.299130	26.894131	76.590721
62.567849	19.979104	76.595726
62.665414	21.173182	76.600730
61.781921	32.586428	76.605735
60.781110	27.980503	76.610740
60.041735	13.601352	76.615745
59.599063	27.344451	76.620750
58.929291	26.006852	76.625754
57.949176	24.635168	76.630759
57.169170	27.408987	76.635764
57.010986	26.068646	76.640769
56.487217	33.105178	76.645774
56.002565	21.605963	76.650778
54.920235	28.263213	76.655783
54.363383	32.365531	76.660788
54.233443	17.857642	76.665793
52.865029	26.019223	76.670798
52.407606	11.544646	76.675802
51.951880	22.889664	76.680807
51.071936	20.393391	76.685812
50.445042	17.096657	76.690817
49.132581	18.293263	76.695822
49.075071	18.704660	76.700826
48.511954	22.461041	76.705831
47.534844	22.821982	76.710836
47.280463	14.216076	76.715841
46.456907	33.701781	76.720846
45.928647	15.515251	76.725850
44.874031	24.733826	76.730855
44.067814	15.501562	76.735860
43.827247	11.890899	76.740865
43.011646	30.462261	76.745870
42.766209	20.659576	76.750874
41.753590	30.456516	76.755879
40.860357	24.746905	76.760884
40.353929	24.114977	76.765889
40.085294	22.317584	76.770894
39.602727	22.560227	76.775898
38.418566	28.210265	76.780903
37.661569	22.209265	76.785908
36.853903	27.578478	76.790913
36.230626	21.371644	76.795918
35.425764	12.632764	76.800922
34.894021	26.942012	76.805927
34.394492	24.528576	76.810932
34.210066	23.501510	76.815937
33.320044	22.875571	76.820942
32.503899	21.387858	76.825946
32.320874	23.177052	76.830951
31.211933	24.782761	76.835956
30.405177	20.194789	76.840961
29.560717	32.018139	76.845966
29.368037	18.826000	76.850970
28.674498	24.112355	76.855975
27.689361	25.747206	76.860980
26.533742	22.861242	76.865985
26.151714	23.858995	76.870990
26.046093	14.503957	76.875994
25.421274	24.283200	76.880999
24.854076	13.396420	76.886004
23.817164	24.419394	76.891009
22.984281	21.232794	76.896014
22.864554	22.149286	76.901018
22.598181	18.211575	76.906023
21.551539	29.196681	76.911028
20.619042	11.615547	76.916033
19.913263	26.876662	76.921038
18.901802	26.541338	76.926042
17.981370	22.789953	76.931047
17.658891	23.672552	76.936052
17.425518	20.339868	76.941057
17.094613	29.056662	76.946062
16.701372	21.171509	76.951066
15.380188	17.573935	76.956071
14.850809	29.652963	76.961076
14.330332	19.608721	76.966081
13.175236	18.572478	76.971086
12.378640	22.198946	76.976090
12.112057	22.312526	76.981095
11.476397	15.301843	76.986100
10.746044	19.748813	76.991105
9.980520	28.137532	76.996110
9.348344	13.394370	77.001114
9.037294	25.370761	77.006119
8.056993	27.298166	77.011124
7.339317	19.969399	77.016129
7.094723	21.328438	77.021134
6.276213	24.898480	77.026139
5.133787	19.575570	77.031143
4.458293	27.319138	77.036148
4.197430	11.387637	77.041153
3.539860	17.890415	77.046158