Fri Mar 05 18:25:45 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.727879	94.529264	0.000000
-1.944741	81.561679	0.005005
-2.241689	67.786851	0.010010
-3.865509	23.654022	0.015014
-8.115728	7.060966	0.020019
-13.240650	13.139210	0.025024
-18.010244	9.161212	0.030029
-22.905143	13.949094	0.035034
-26.902497	13.601126	0.040038
-30.301122	11.724194	0.045043
-34.010722	14.864331	0.050048
-37.529998	11.035441	0.055053
-41.492738	10.708785	0.060058
-45.327595	17.849194	0.065062
-49.172652	15.942576	0.070067
-53.112116	15.405642	0.075072
-56.133568	4.232265	0.080077
-59.949197	23.573806	0.085082
-63.705126	20.452917	0.090086
-67.788242	8.832318	0.095091
-72.011798	16.574099	0.100096
-75.492491	16.222638	0.105101
-79.265985	18.179269	0.110106
-82.425731	11.508159	0.115110
-86.090372	10.366035	0.120115
-90.713154	19.679121	0.125120
-94.024192	10.843329	0.130125
-98.001005	13.408019	0.135130
-101.918767	4.353645	0.140134
-105.409834	11.034012	0.145139
-109.251530	9.111186	0.150144
-112.781162	10.404481	0.155149
-116.660086	19.595782	0.160154
-120.294658	14.993770	0.165158
-124.143309	3.299599	0.170163
-128.051463	15.365661	0.175168
-131.724752	11.960458	0.180173
-135.413913	15.499612	0.185178
-139.139308	12.463860	0.190182
-142.764851	4.968285	0.195187
-146.959415	1.942752	0.200192
-150.576856	-2.717134	0.205197
-154.742075	14.253353	0.210202
-158.198011	6.762277	0.215206
-162.335346	12.651703	0.220211
-166.236790	16.237393	0.225216
-169.223015	8.557841	0.230221
-173.383784	20.896098	0.235226
-176.815671	8.503146	0.240230
-180.542966	16.257381	0.245235
-184.584851	19.040756	0.250240
-188.119139	15.615035	0.255245
-192.212837	17.164039	0.260250
-195.573437	13.311641	0.265254
-199.182238	14.806931	0.270259
-203.560051	23.541808	0.275264
-207.080902	9.143003	0.280269
-210.977328	9.570871	0.285274
-214.639786	12.922954	0.290278
-218.380012	9.839231	0.295283
-222.151004	15.343860	0.300288
-225.920456	7.590681	0.305293
-229.801746	13.018305	0.310298
-233.042633	9.050661	0.315302
-236.858827	11.003310	0.320307
-241.091697	20.000549	0.325312
-244.611308	7.692668	0.330317
-248.488462	7.679124	0.335322
-252.226565	8.977508	0.340326
-255.731327	11.564885	0.345331
-259.841545	14.196861	0.350336
-263.283977	6.386820	0.355341
-267.371464	18.030701	0.360346
-271.034283	14.428500	0.365350
-274.882490	3.735892	0.370355
-278.594763	6.424232	0.375360
-282.252937	11.026264	0.380365
-286.175263	14.631245	0.385370
-289.784428	10.547420	0.390374
-293.351490	14.226594	0.395379
-297.255941	19.560250	0.400384
-300.748076	12.198169	0.405389
-305.292539	16.271499	0.410394
-308.775805	13.027052	0.415398
-312.752084	8.472004	0.420403
-316.235728	17.176302	0.425408
-319.637784	13.182464	0.430413
-323.374675	15.676105	0.435418
-327.403195	14.623976	0.440422
-331.332938	8.099785	0.445427
-335.235153	15.429580	0.450432
-338.653804	17.626435	0.455437
-342.577109	15.392157	0.460442
-346.242308	17.308257	0.465446
-349.609076	11.473243	0.470451
-353.662315	12.162921	0.475456
-357.396168	7.815253	0.480461
-361.605410	21.278040	0.485466
-364.674131	2.505352	0.490470
-368.485278	13.611681	0.495475
-372.572756	21.527783	0.500480
-376.534912	13.239486	0.505485
-380.177249	9.008131	0.510490
-384.136062	11.994615	0.515494
-387.749986	9.321509	0.520499
-391.346852	9.247676	0.525504
-395.045140	7.983664	0.530509
-399.070768	23.074585	0.535514
-402.405193	15.788405	0.540518
-405.969708	11.585666	0.545523
-410.318119	22.982852	0.550528
-413.889952	20.351948	0.555533
-417.876749	16.834822	0.560538
-421.593856	18.150615	0.565542
-425.399335	18.228416	0.570547
-429.164970	23.287800	0.575552
-432.587046	8.521926	0.580557
-437.005826	20.868686	0.585562
-440.350419	14.451516	0.590566
-443.755762	7.977823	0.595571
-447.527792	17.370174	0.600576
-451.346255	16.117553	0.605581
-455.258611	15.886036	0.610586
-459.205932	14.702892	0.615590
-462.874541	14.385155	0.620595
-466.920758	15.843461	0.625600
-470.509385	10.241174	0.630605
-474.320936	15.509809	0.635610
-477.727189	19.120992	0.640614
-481.252711	9.328114	0.645619
-485.391185	13.734336	0.650624
-489.135257	13.300956	0.655629
-493.185186	14.230040	0.660634
-496.831725	10.179313	0.665638
-500.498468	15.997299	0.670643
-504.648982	28.498457	0.675648
-508.001704	16.105990	0.680653
-511.531173	14.753696	0.685658
-515.401542	16.295963	0.690662
-519.082046	9.333315	0.695667
-523.442645	22.714881	0.700672
-527.091909	15.460246	0.705677
-530.743555	24.259481	0.710682
-534.148933	11.550615	0.715686
-537.867443	11.356082	0.720691
-542.183064	15.286066	0.725696
-545.681727	12.884953	0.730701
-549.522711	19.349012	0.735706
-552.798432	11.214736	0.740710
-556.510861	11.206919	0.745715
-560.503731	11.146132	0.750720
-564.314450	9.269559	0.755725
-568.533060	16.189782	0.760730
-572.116041	17.293571	0.765734
-575.477775	11.341391	0.770739
-579.502141	13.192213	0.775744
-582.981785	11.735872	0.780749
-587.268370	20.598765	0.785754
-591.037171	14.121848	0.790758
-594.473448	12.524555	0.795763
-598.429333	18.363644	0.800768
-601.853239	11.826919	0.805773
-605.559733	19.668345	0.810778
-609.478117	15.866226	0.815782
-613.310555	23.261004	0.820787
-617.134123	17.387393	0.825792
-620.510267	17.824273	0.830797
-624.787114	21.156849	0.835802
-628.506567	21.369465	0.840806
-631.972656	1.347053	0.845811
-635.902344	19.554845	0.850816
-639.240767	10.233800	0.855821
-643.671891	12.490338	0.860826
-647.463361	5.985602	0.865830
-650.953536	8.487637	0.870835
-655.128868	16.672123	0.875840
-658.535302	14.150787	0.880845
-662.107939	14.358922	0.885850
-665.698058	12.966087	0.890854
-669.809128	11.659647	0.895859
-673.656694	21.324602	0.900864
-677.347816	19.999961	0.905869
-681.321947	17.993568	0.910874
-684.574665	11.921627	0.915878
-688.417807	5.720107	0.920883
-692.459872	18.779820	0.925888
-696.121779	12.044724	0.930893
-699.864590	18.810297	0.935898
-703.518378	20.952198	0.940902
-707.369257	18.729034	0.945907
-710.991432	21.156056	0.950912
-714.668775	14.051292	0.955917
-718.787895	16.234458	0.960922
-722.628831	20.491035	0.965926
-726.142113	21.776306	0.970931
-729.978994	22.671746	0.975936
-733.674600	14.601678	0.980941
-737.754679	18.664681	0.985946
-741.035982	18.772761	0.990950
-744.550795	16.994272	0.995955
-748.827750	22.957454	1.000960
-752.511302	10.932056	1.005965
-756.717102	26.030242	1.010970
-760.371149	19.935812	1.015974
-763.693795	13.622847	1.020979
-767.577767	13.939245	1.025984
-770.862013	13.513248	1.030989
-775.007223	13.756291	1.035994
-778.970776	16.179626	1.040998
-782.743653	15.677198	1.046003
-786.436367	10.404283	1.051008
-790.137524	8.270869	1.056013
-793.763043	21.702562	1.061018
-797.567762	23.490260	1.066022
-801.412193	14.485301	1.071027
-805.040213	30.953061	1.076032
-808.762634	15.239152	1.081037
-812.925626	22.182444	1.086042
-816.484586	26.471371	1.091046
-820.047415	14.696449	1.096051
-824.010226	26.658760	1.101056
-827.832792	18.818875	1.106061
-831.658750	27.324710	1.111066
-835.190228	14.046691	1.116070
-838.895473	15.307620	1.121075
-842.925906	25.159761	1.126080
-846.424288	10.015664	1.131085
-850.363353	14.187201	1.136090
-854.186455	14.467203	1.141094
-858.065212	9.754001	1.146099
-861.748216	11.405649	1.151104
-865.107552	15.583885	1.156109
-869.148488	19.292345	1.161114
-872.990846	18.943095	1.166118
-876.410926	10.188976	1.171123
-880.251849	21.474294	1.176128
-884.129575	13.931910	1.181133
-888.129880	20.707394	1.186138
-891.985252	18.870032	1.191142
-895.444612	11.566714	1.196147
-899.172852	18.415414	1.201152
-903.079734	13.016078	1.206157
-906.886375	25.024512	1.211162
-910.381285	18.272524	1.216166
-913.858511	16.727979	1.221171
-918.125894	25.205172	1.226176
-921.639123	12.362774	1.231181
-925.434871	17.268460	1.236186
-929.523650	22.806055	1.241190
-932.879138	20.141359	1.246195
-936.705792	14.792330	1.251200
-940.372094	10.452154	1.256205
-944.677871	22.073670	1.261210
-948.130710	11.929294	1.266214
-951.610391	15.644344	1.271219
-955.591837	25.179750	1.276224
-959.244189	12.764937	1.281229
-963.161407	23.330874	1.286234
-967.262645	18.932552	1.291238
-970.588902	13.883613	1.296243
-974.529797	19.202093	1.301248
-977.883362	10.497420	1.306253
-982.048435	15.350287	1.311258
-985.780833	10.235430	1.316262
-989.462137	13.594845	1.321267
-993.387789	19.959594	1.326272
-996.746137	11.899111	1.331277
-1000.809986	11.246447	1.336282
-1004.752719	13.401899	1.341286
-1008.380914	15.478672	1.346291
-1012.223039	22.273217	1.351296
-1016.039165	15.560151	1.356301
-1019.522867	22.021420	1.361306
-1023.076753	14.980998	1.366310
-1026.786806	24.335920	1.371315
-1031.146957	25.992047	1.376320
-1034.831911	17.256878	1.381325
-1038.465682	15.598785	1.386330
-1041.853496	22.140945	1.391334
-1045.590775	19.706210	1.396339
-1049.565133	19.220666	1.401344
-1053.628181	12.537696	1.406349
-1057.620959	26.873747	1.411354
-1061.237973	20.385952	1.416358
-1064.515091	10.656781	1.421363
-1068.443669	16.351911	1.426368
-1071.939065	4.738516	1.431373
-1075.787044	22.052370	1.436378
-1079.752745	17.206795	1.441382
-1083.618463	15.249983	1.446387
-1087.678358	13.988133	1.451392
-1091.349228	1.057700	1.456397
-1095.030371	14.866134	1.461402
-1098.526874	15.818113	1.466406
-1101.787863	13.684175	1.471411
-1106.331658	23.374430	1.476416
-1109.515824	20.151154	1.481421
-1113.515105	11.486901	1.486426
-1117.777378	7.546699	1.491430
-1121.063366	11.000774	1.496435
-1124.851467	14.438983	1.501440
-1128.588313	16.233701	1.506445
-1132.333926	8.233802	1.511450
-1136.297665	17.746159	1.516454
-1139.734459	11.888832	1.521459
-1143.709855	11.277460	1.526464
-1147.699296	13.785975	1.531469
-1151.262920	15.873137	1.536474
-1155.000111	12.019312	1.541478
-1158.598416	7.033100	1.546483
-1162.572062	8.326438	1.551488
-1166.091204	-2.544986	1.556493
-1170.187484	16.147554	1.561498
-1173.907945	12.240620	1.566502
-1177.467552	9.347169	1.571507
-1181.366403	18.037087	1.576512
-1184.854686	10.104915	1.581517
-1188.505566	10.242791	1.586522
-1192.687690	14.586242	1.591526
-1196.208339	2.365235	1.596531
-1200.369673	12.268851	1.601536
-1204.110331	6.062853	1.606541
-1207.745713	10.448158	1.611546
-1211.325659	9.237466	1.616550
-1215.094903	13.823975	1.621555
-1218.999077	17.646759	1.626560
-1222.482815	16.611500	1.631565
-1226.503528	15.217470	1.636570
-1230.317703	11.551128	1.641574
-1234.154928	8.758959	1.646579
-1237.757081	11.760739	1.651584
-1241.457719	11.359459	1.656589
-1245.178134	8.084993	1.661594
-1249.150856	15.723974	1.666598
-1252.958362	-1.907277	1.671603
-1256.686743	12.285836	1.676608
-1260.222151	17.774858	1.681613
-1264.147063	11.119052	1.686618
-1267.783439	6.159609	1.691622
-1271.441160	12.925049	1.696627
-1275.368505	22.698312	1.701632
-1279.142031	12.200509	1.706637
-1282.792042	5.333588	1.711642
-1286.724009	16.531589	1.716646
-1289.957074	7.464338	1.721651
-1294.106889	13.095894	1.726656
-1297.700892	13.645884	1.731661
-1302.046948	17.690912	1.736666
-1305.816559	12.234037	1.741670
-1309.125100	8.319747	1.746675
-1313.188403	18.188944	1.751680
-1316.503992	19.135948	1.756685
-1320.360531	12.898227	1.761690
-1324.182876	16.102539	1.766694
-1327.710890	10.783650	1.771699
-1331.685498	15.407944	1.776704
-1335.551340	11.751627	1.781709
-1339.473520	17.914529	1.786714
-1343.226836	21.205595	1.791718
-1346.676138	12.223500	1.796723
-1350.571385	25.725960	1.801728
-1354.262141	7.994194	1.806733
-1358.053971	9.246146	1.811738
-1361.901639	11.019549	1.816742
-1365.720890	-0.781216	1.821747
-1369.485431	17.030637	1.826752
-1373.074564	-2.439376	1.831757
-1376.770709	7.303336	1.836762
-1380.569511	7.930393	1.841766
-1384.095351	5.358289	1.846771
-1388.215893	15.241501	1.851776
-1391.591581	10.112794	1.856781
-1395.698518	3.412248	1.861786
-1399.560467	9.023133	1.866790
-1403.278901	4.879714	1.871795
-1406.989488	4.879259	1.876800
-1410.571565	3.188252	1.881805
-1414.720858	15.216026	1.886810
-1418.471506	11.735375	1.891814
-1421.972850	4.160489	1.896819
-1425.767467	15.145909	1.901824
-1429.552191	10.092208	1.906829
-1433.102156	9.529918	1.911834
-1437.087012	11.495720	1.916838
-1440.688899	10.602711	1.921843
-1444.461317	11.987313	1.926848
-1448.193684	0.448749	1.931853
-1452.425646	5.377796	1.936858
-1456.208176	10.413088	1.941862
-1459.610009	2.503788	1.946867
-1463.502627	8.733118	1.951872
-1467.332371	1.622471	1.956877
-1470.898448	14.880013	1.961882
-1474.646932	13.086441	1.966886
-1477.956513	-2.089970	1.971891
-1482.432588	18.004276	1.976896
-1486.152768	12.881988	1.981901
-1489.598908	8.677764	1.986906
-1493.440782	11.388739	1.991910
-1496.914893	-0.142208	1.996915
-1501.039483	10.192752	2.006912
-1502.497758	14.525309	2.016909
-1499.653257	10.180873	2.026906
-1496.774702	9.296814	2.036902
-1494.409305	11.684438	2.046899
-1492.779079	5.592327	2.056896
-1490.939261	11.743100	2.066893
-1488.943757	10.450972	2.076890
-1486.540466	5.724040	2.086886
-1484.918089	10.456990	2.096883
-1483.431116	15.173728	2.106880
-1481.648814	7.295148	2.116877
-1479.584159	7.719342	2.126874
-1477.363579	8.920685	2.136870
-1475.600159	10.234706	2.146867
-1473.702075	5.441837	2.156864
-1471.880211	9.899694	2.166861
-1469.852031	7.195493	2.176858
-1468.166632	3.500906	2.186854
-1466.257606	10.395364	2.196851
-1464.112036	5.881826	2.206848
-1462.130271	8.943547	2.216845
-1460.751647	12.084474	2.226842
-1458.795310	8.551776	2.236838
-1456.821956	9.822724	2.246835
-1455.002693	10.039913	2.256832
-1452.852087	12.845660	2.266829
-1451.123216	7.159364	2.276826
-1449.106462	7.610203	2.286822
-1447.218967	9.689126	2.296819
-1445.511678	5.051565	2.306816
-1443.673689	6.465778	2.316813
-1441.501992	5.710750	2.326810
-1439.763957	7.145706	2.336806
-1437.759537	8.230116	2.346803
-1435.872334	7.342220	2.356800
-1434.506118	12.610436	2.366797
-1432.523109	12.048260	2.376794
-1430.215902	10.335221	2.386790
-1428.420929	10.052630	2.396787
-1426.815050	17.698300	2.406784
-1424.748498	11.717956	2.416781
-1422.770450	11.571850	2.426778
-1420.709031	9.803433	2.436774
-1419.288726	11.579803	2.446771
-1417.189294	7.296327	2.456768
-1415.485540	13.516319	2.466765
-1413.655106	18.484440	2.476762
-1411.461178	12.936877	2.486758
-1409.476470	14.013416	2.496755
-1407.713227	12.142744	2.506752
-1406.122048	13.125968	2.516749
-1404.002284	11.367172	2.526746
-1402.215557	18.031794	2.536742
-1400.462401	8.373702	2.546739
-1398.383028	11.732490	2.556736
-1396.442233	16.094004	2.566733
-1394.786751	18.871701	2.576730
-1392.870101	3.673694	2.586726
-1390.845346	8.077033	2.596723
-1389.105540	13.994429	2.606720
-1387.196198	9.998780	2.616717
-1385.084938	10.603497	2.626714
-1383.279897	7.036658	2.636710
-1381.587990	7.451137	2.646707
-1379.657109	7.664728	2.656704
-1377.990155	9.284796	2.666701
-1375.882119	8.893710	2.676698
-1373.637128	3.985386	2.686694
-1371.996753	10.542403	2.696691
-1370.436457	14.986953	2.706688
-1368.542340	10.033745	2.716685
-1366.642519	8.706511	2.726682
-1364.496420	8.391448	2.736678
-1362.659040	5.176295	2.746675
-1360.941567	3.949309	2.756672
-1359.229582	9.850655	2.766669
-1357.095677	0.079544	2.776666
-1355.039176	3.712035	2.786662
-1353.124005	6.332928	2.796659
-1351.485112	8.202248	2.806656
-1349.659309	8.140575	2.816653
-1347.906410	9.751646	2.826650
-1345.595659	2.555952	2.836646
-1343.889172	6.096056	2.846643
-1341.931809	9.854957	2.856640
-1340.466215	15.276279	2.866637
-1338.380363	10.308193	2.876634
-1336.360645	1.651179	2.886630
-1334.605559	3.896653	2.896627
-1332.476151	12.570191	2.906624
-1330.923032	7.835804	2.916621
-1328.976121	6.944753	2.926618
-1327.036767	10.209175	2.936614
-1325.282943	4.777924	2.946611
-1323.313959	8.486033	2.956608
-1321.396096	7.752797	2.966605
-1319.292387	6.779816	2.976602
-1317.622547	10.122120	2.986598
-1316.010045	4.972444	2.996595
-1314.045080	11.318080	3.006592
-1312.238659	12.082181	3.016589
-1310.130854	11.249080	3.026586
-1308.086097	10.588705	3.036582
-1306.366727	11.275163	3.046579
-1304.775350	10.215242	3.056576
-1302.607509	15.238405	3.066573
-1300.559733	12.633844	3.076570
-1298.925616	12.981842	3.086566
-1296.963455	14.191562	3.096563
-1295.149767	5.535972	3.106560
-1293.449785	12.620360	3.116557
-1291.666958	14.100368	3.126554
-1289.321194	16.568720	3.136550
-1287.532560	13.007736	3.146547
-1286.009062	13.613449	3.156544
-1284.029559	8.422427	3.166541
-1282.011614	3.757368	3.176538
-1279.951588	1.444554	3.186534
-1278.101073	5.869565	3.196531
-1276.169161	-0.434898	3.206528
-1274.555559	2.108006	3.216525
-1272.828424	3.949050	3.226522
-1270.681850	11.432519	3.236518
-1268.884349	3.398494	3.246515
-1267.172749	5.647823	3.256512
-1265.297139	5.368243	3.266509
-1263.157077	7.004265	3.276506
-1261.056579	8.682937	3.286502
-1259.625458	5.346557	3.296499
-1257.840891	7.355266	3.306496
-1255.490560	11.190308	3.316493
-1253.994340	9.654590	3.326490
-1251.839912	9.390404	3.336486
-1250.169842	10.054793	3.346483
-1248.020668	14.177826	3.356480
-1246.300481	18.527407	3.366477
-1244.578920	12.262939	3.376474
-1242.812457	12.651379	3.386470
-1240.674717	19.601026	3.396467
-1238.648056	11.334555	3.406464
-1237.021798	15.002847	3.416461
-1235.147870	6.929771	3.426458
-1233.009504	9.455052	3.436454
-1231.296286	11.206776	3.446451
-1229.675551	12.370133	3.456448
-1227.884363	6.208223	3.466445
-1225.487770	5.654256	3.476442
-1223.765350	2.184443	3.486438
-1221.874313	8.873575	3.496435
-1220.047892	9.468757	3.506432
-1218.338441	4.952587	3.516429
-1216.526446	12.792809	3.526426
-1214.347140	7.618821	3.536422
-1212.420077	5.224706	3.546419
-1211.147253	-1.034249	3.556416
-1208.613769	3.248382	3.566413
-1206.809384	2.018655	3.576410
-1204.933676	5.383367	3.586406
-1203.219883	6.835015	3.596403
-1201.478813	7.391762	3.606400
-1199.488019	10.337008	3.616397
-1197.557049	10.932848	3.626394
-1195.472772	10.670465	3.636390
-1193.609804	2.984443	3.646387
-1192.197100	0.538430	3.656384
-1190.233515	6.975979	3.666381
-1188.077381	2.085200	3.676378
-1186.355973	-1.536005	3.686374
-1184.282100	0.772268	3.696371
-1182.425988	7.394390	3.706368
-1181.065159	0.477148	3.716365
-1178.758121	3.483921	3.726362
-1176.815943	5.939590	3.736358
-1174.938664	5.141914	3.746355
-1173.021917	-2.761119	3.756352
-1171.215760	0.207375	3.766349
-1169.532309	1.787061	3.776346
-1167.667791	3.344097	3.786342
-1165.678680	4.740672	3.796339
-1163.881554	10.529079	3.806336
-1161.909569	8.574667	3.816333
-1160.067344	8.565780	3.826330
-1158.127706	15.297724	3.836326
-1156.167738	8.417272	3.846323
-1154.181232	5.459476	3.856320
-1152.626860	4.561897	3.866317
-1150.555439	1.617362	3.876314
-1148.701251	4.549769	3.886310
-1146.971436	4.912565	3.896307
-1145.085844	9.328921	3.906304
-1143.072579	11.403768	3.916301
-1141.244489	9.950820	3.926298
-1139.686852	8.016922	3.936294
-1137.329511	5.752984	3.946291
-1135.671950	8.041059	3.956288
-1133.547510	9.693913	3.966285
-1131.920305	9.057857	3.976282
-1130.281357	10.257846	3.986278
-1127.964838	-5.836063	3.996275
-1126.229671	2.766533	4.006272
-1124.604796	-0.324443	4.016269
-1122.210134	1.305719	4.026266
-1120.567773	6.097325	4.036262
-1118.887455	2.408528	4.046259
-1116.952647	5.157536	4.056256
-1115.010616	6.806428	4.066253
-1113.162038	5.542859	4.076250
-1111.400582	11.368596	4.086246
-1109.231885	7.827474	4.096243
-1107.342869	10.348550	4.106240
-1105.488540	10.339349	4.116237
-1103.740236	8.076549	4.126234
-1101.943545	9.717121	4.136230
-1099.966366	3.786081	4.146227
-1098.026956	4.895398	4.156224
-1096.231048	6.618207	4.166221
-1094.249549	2.852828	4.176218
-1092.460334	3.769856	4.186214
-1090.604222	-3.515513	4.196211
-1088.755300	6.259464	4.206208
-1087.093346	2.843630	4.216205
-1085.028237	2.489673	4.226202
-1083.064653	7.747829	4.236198
-1081.051525	5.379528	4.246195
-1079.097233	2.753794	4.256192
-1077.721335	-3.283159	4.266189
-1075.392901	6.890403	4.276186
-1073.806963	-1.175964	4.286182
-1071.902395	-0.596324	4.296179
-1070.078105	0.343533	4.306176
-1068.109469	3.196121	4.316173
-1065.967173	2.774571	4.326170
-1064.508570	1.541835	4.336166
-1062.567850	2.703079	4.346163
-1060.443348	-0.031970	4.356160
-1058.822490	4.224692	4.366157
-1056.868575	8.808619	4.376154
-1054.751850	10.647520	4.386150
-1053.129734	9.429692	4.396147
-1050.986145	6.200537	4.406144
-1049.399554	8.629502	4.416141
-1047.463184	3.246618	4.426138
-1045.520591	0.733310	4.436134
-1043.882477	6.095662	4.446131
-1041.434953	8.358517	4.456128
-1039.878971	2.186989	4.466125
-1038.509852	2.154389	4.476122
-1036.287974	4.473864	4.486118
-1034.067261	3.716113	4.496115
-1032.438410	4.946207	4.506112
-1030.563972	10.430251	4.516109
-1028.571952	5.737965	4.526106
-1026.750266	5.426147	4.536102
-1024.958177	4.639057	4.546099
-1023.070520	3.743525	4.556096
-1020.943758	3.476082	4.566093
-1019.520223	-0.242635	4.576090
-1017.506284	-2.334691	4.586086
-1015.224232	4.988416	4.596083
-1013.548967	1.232603	4.606080
-1012.068857	6.318663	4.616077
-1010.057343	8.078114	4.626074
-1008.203863	4.124853	4.636070
-1005.847262	4.183831	4.646067
-1004.166962	0.340375	4.656064
-1002.470229	-2.619903	4.666061
-1000.694786	2.707887	4.676058
-998.446369	1.364677	4.686054
-996.613845	3.667507	4.696051
-994.892833	2.081793	4.706048
-993.039991	-1.800299	4.716045
-991.484969	-0.728899	4.726042
-989.317965	-1.095908	4.736038
-987.365011	1.640835	4.746035
-985.433775	7.899005	4.756032
-983.569947	8.423654	4.766029
-981.887097	9.739888	4.776026
-979.747048	2.633405	4.786022
-978.013391	4.301523	4.796019
-975.930336	1.481595	4.806016
-974.395288	4.923081	4.816013
-972.691771	13.125077	4.826010
-970.377479	10.820817	4.836006
-968.440857	3.172126	4.846003
-966.748028	1.931997	4.856000
-964.840089	8.391282	4.865997
-962.839189	0.365997	4.875994
-961.158581	6.716369	4.885990
-959.235211	3.410402	4.895987
-957.458667	0.615816	4.905984
-955.580450	2.028727	4.915981
-953.766871	6.976242	4.925978
-951.772749	8.253780	4.935974
-949.849269	1.314585	4.945971
-947.922147	9.752429	4.955968
-945.995228	14.860256	4.965965
-944.435738	7.568728	4.975962
-942.371844	7.614571	4.985958
-940.676785	-0.166003	4.995955
-938.565247	5.063889	5.005952
-936.315191	7.784754	5.015949
-935.136516	9.690064	5.025946
-933.205137	4.650702	5.035942
-931.071427	10.821284	5.045939
-929.025568	10.301592	5.055936
-927.497175	16.085796	5.065933
-925.522365	7.981020	5.075930
-923.730327	5.720832	5.085926
-921.593788	7.844061	5.095923
-919.767793	10.651691	5.105920
-917.812233	12.262271	5.115917
-916.017157	8.015253	5.125914
-914.230307	6.453808	5.135910
-912.158427	12.309026	5.145907
-910.597816	7.614753	5.155904
-908.807779	2.564849	5.165901
-907.045685	9.216453	5.175898
-904.559190	14.039059	5.185894
-903.043192	10.820369	5.195891
-901.027756	5.532325	5.205888
-899.142282	3.328272	5.215885
-897.278915	13.800602	5.225882
-895.304367	9.243848	5.235878
-893.419161	5.118230	5.245875
-891.774478	12.049149	5.255872
-889.726003	13.415948	5.265869
-887.855761	13.677538	5.275866
-886.148320	2.940755	5.285862
-884.198566	10.437130	5.295859
-882.202028	8.453758	5.305856
-880.582727	12.333429	5.315853
-878.678399	18.831268	5.325850
-876.790724	11.330994	5.335846
-874.645526	11.326003	5.345843
-873.008798	9.807535	5.355840
-871.223766	8.217991	5.365837
-869.177073	14.004644	5.375834
-867.031995	10.691727	5.385830
-865.499509	12.611567	5.395827
-863.467708	11.641013	5.405824
-861.654579	14.321271	5.415821
-859.776935	12.574822	5.425818
-857.984583	14.898398	5.435814
-856.187664	7.886342	5.445811
-854.338684	12.864599	5.455808
-852.353783	15.708462	5.465805
-850.339750	12.509666	5.475802
-848.611096	15.797134	5.485798
-846.539375	8.755366	5.495795
-844.979035	13.032916	5.505792
-842.816799	13.789455	5.515789
-841.249241	12.109957	5.525786
-839.212852	17.039324	5.535782
-837.324982	6.428466	5.545779
-835.355655	8.709559	5.555776
-833.615228	7.965609	5.565773
-831.247937	7.700943	5.575770
-829.775771	12.033650	5.585766
-827.970860	11.918882	5.595763
-826.040822	12.556234	5.605760
-824.016645	11.795357	5.615757
-822.387569	16.699843	5.625754
-820.373281	6.452481	5.635750
-818.207419	10.931689	5.645747
-816.722839	10.186013	5.655744
-814.855516	12.783434	5.665741
-812.970643	12.158518	5.675738
-810.974055	12.987354	5.685734
-809.207445	11.132374	5.695731
-807.165967	9.115039	5.705728
-805.353860	10.851277	5.715725
-803.497478	8.170359	5.725722
-802.128880	12.720169	5.735718
-799.527630	7.592788	5.745715
-797.697855	10.966765	5.755712
-795.957260	8.275937	5.765709
-794.129688	16.292461	5.775706
-792.382097	14.126316	5.785702
-789.996974	11.315109	5.795699
-788.763439	10.716945	5.805696
-786.998649	9.620181	5.815693
-784.569920	10.893140	5.825690
-782.789092	10.145927	5.835686
-780.867436	17.130565	5.845683
-779.082636	9.214164	5.855680
-777.352042	8.542881	5.865677
-775.607670	14.052670	5.875674
-773.641247	14.782146	5.885670
-771.686607	12.530820	5.895667
-769.809579	12.458255	5.905664
-767.365484	9.359746	5.915661
-766.059181	13.065309	5.925658
-764.288019	7.693252	5.935654
-762.118492	14.178809	5.945651
-760.341127	11.772661	5.955648
-758.486674	16.671177	5.965645
-756.755762	14.705096	5.975642
-754.686127	13.038574	5.985638
-752.642029	12.031411	5.995635
-751.019118	3.064042	6.005632
-749.535719	13.868814	6.015629
-747.239278	13.936087	6.025626
-745.242792	12.762852	6.035622
-743.460425	10.498025	6.045619
-741.499502	11.697364	6.055616
-739.684016	7.245101	6.065613
-737.646527	10.464351	6.075610
-736.110762	14.644851	6.085606
-734.210419	19.340262	6.095603
-732.107669	9.813051	6.105600
-730.276426	16.085852	6.115597
-728.390271	19.062449	6.125594
-726.679934	14.472256	6.135590
-724.675266	16.124102	6.145587
-722.714243	12.684403	6.155584
-721.024096	14.223876	6.165581
-719.084479	18.725125	6.175578
-717.359428	19.059001	6.185574
-715.297489	20.169588	6.195571
-713.329570	17.554599	6.205568
-711.319574	17.588731	6.215565
-709.842288	17.452193	6.225562
-707.952325	17.563930	6.235558
-705.883211	16.630180	6.245555
-703.850827	12.410130	6.255552
-702.417671	9.217431	6.265549
-700.337663	17.717920	6.275546
-698.139310	16.553521	6.285542
-696.830942	18.184018	6.295539
-694.747316	15.193707	6.305536
-692.693576	10.831304	6.315533
-690.850091	9.227816	6.325530
-689.093924	10.914661	6.335526
-687.163570	9.278348	6.345523
-685.430444	11.535731	6.355520
-683.433482	13.533061	6.365517
-681.598826	13.213121	6.375514
-679.715795	15.842881	6.385510
-677.709610	15.059739	6.395507
-675.861455	7.930669	6.405504
-674.045232	11.115855	6.415501
-672.105483	15.247641	6.425498
-670.318821	15.364861	6.435494
-668.496059	13.676278	6.445491
-666.537044	12.098560	6.455488
-664.500738	15.155431	6.465485
-662.872154	13.999992	6.475482
-660.771650	15.759741	6.485478
-658.935214	14.454251	6.495475
-657.035986	10.249199	6.505472
-655.318388	9.594291	6.515469
-653.627553	11.413183	6.525466
-651.468202	11.521399	6.535462
-649.496017	10.045804	6.545459
-647.720083	8.442089	6.555456
-645.965723	7.598152	6.565453
-644.125401	6.866802	6.575450
-642.286741	3.775145	6.585446
-640.221778	9.475405	6.595443
-638.628498	2.022340	6.605440
-636.445564	9.808534	6.615437
-634.501669	8.504843	6.625434
-632.785824	8.494455	6.635430
-630.838567	8.327094	6.645427
-629.246326	8.769096	6.655424
-627.195634	9.352598	6.665421
-625.224389	14.772577	6.675418
-623.254588	13.818448	6.685414
-621.437308	6.673822	6.695411
-619.401093	9.703904	6.705408
-617.717909	11.520887	6.715405
-616.254569	16.902013	6.725402
-613.876083	14.264147	6.735398
-611.997017	8.393368	6.745395
-610.472205	11.734108	6.755392
-608.475146	9.169814	6.765389
-606.298491	6.325773	6.775386
-604.786129	10.184832	6.785382
-602.903207	13.425737	6.795379
-600.657108	14.961751	6.805376
-598.849227	9.002877	6.815373
-597.117865	10.788494	6.825370
-595.317717	12.929447	6.835366
-593.098617	10.062848	6.845363
-591.414962	15.369321	6.855360
-589.807179	13.896721	6.865357
-587.841331	16.049107	6.875354
-586.016788	12.171834	6.885350
-583.975243	16.570074	6.895347
-582.122486	13.076726	6.905344
-580.197679	16.083586	6.915341
-578.081534	9.685476	6.925338
-576.660200	15.417556	6.935334
-574.693557	19.123544	6.945331
-572.723722	8.196608	6.955328
-570.607986	16.130977	6.965325
-569.015457	11.093910	6.975322
-567.186885	15.041436	6.985318
-565.424588	13.645226	6.995315
-563.368556	7.651476	7.005312
-561.309763	9.823775	7.015309
-559.591198	10.834605	7.025306
-557.672286	12.201865	7.035302
-555.934945	6.980620	7.045299
-553.971197	13.083979	7.055296
-552.049247	8.741163	7.065293
-550.125098	12.182373	7.075290
-548.400677	10.694329	7.085286
-546.433297	6.543213	7.095283
-544.345317	10.420901	7.105280
-542.735418	7.845866	7.115277
-541.121177	8.567050	7.125274
-538.911220	2.482419	7.135270
-537.056694	5.884232	7.145267
-535.499148	4.017053	7.155264
-533.377945	2.118269	7.165261
-531.268369	5.583563	7.175258
-529.700420	7.745863	7.185254
-527.728112	7.626693	7.195251
-525.601799	3.096518	7.205248
-523.665506	7.184770	7.215245
-522.044496	5.386412	7.225242
-520.458505	8.684283	7.235238
-518.252421	2.840293	7.245235
-516.678966	6.741760	7.255232
-514.410435	-2.552797	7.265229
-512.460397	3.110670	7.275226
-510.767624	3.554063	7.285222
-509.056653	1.073438	7.295219
-507.103807	2.602690	7.305216
-505.070096	-1.423193	7.315213
-503.277538	5.515987	7.325210
-501.641673	4.975296	7.335206
-499.661756	5.041253	7.345203
-497.203202	11.062481	7.355200
-495.860374	5.370587	7.365197
-494.043968	13.292833	7.375194
-491.984478	11.132355	7.385190
-490.123564	13.244738	7.395187
-488.293738	8.338776	7.405184
-486.370344	16.799745	7.415181
-484.535377	11.569272	7.425178
-482.752140	17.052562	7.435174
-480.917866	12.949595	7.445171
-478.889537	11.534648	7.455168
-476.968553	-0.764444	7.465165
-475.163885	6.872314	7.475162
-473.392288	5.563109	7.485158
-471.316773	7.925453	7.495155
-469.248738	10.590579	7.505152
-467.621373	2.641107	7.515149
-465.853958	4.127373	7.525146
-464.075121	6.811842	7.535142
-461.958967	11.842501	7.545139
-460.066200	10.659222	7.555136
-458.103833	3.788389	7.565133
-456.328398	5.628653	7.575130
-454.805305	5.696542	7.585126
-452.751487	13.058268	7.595123
-450.682638	6.312545	7.605120
-448.835112	8.662367	7.615117
-447.157547	7.529252	7.625114
-445.132470	13.059218	7.635110
-443.308608	10.745351	7.645107
-441.104368	4.723296	7.655104
-439.282740	8.342026	7.665101
-437.804425	7.596005	7.675098
-435.820752	8.348273	7.685094
-433.867604	9.834906	7.695091
-431.723344	7.496730	7.705088
-430.046463	8.961163	7.715085
-428.418563	9.550767	7.725082
-426.894125	8.067898	7.735078
-424.442144	8.866980	7.745075
-422.517976	6.486584	7.755072
-420.814285	3.220848	7.765069
-418.812453	3.941809	7.775066
-416.989662	-1.124033	7.785062
-414.982533	5.206209	7.795059
-413.191516	4.023423	7.805056
-411.274369	8.833267	7.815053
-409.305979	13.639669	7.825050
-407.868261	10.864838	7.835046
-405.906599	12.392769	7.845043
-403.751910	12.184579	7.855040
-401.774160	7.907180	7.865037
-400.199097	10.248437	7.875034
-398.378979	17.011200	7.885030
-396.367516	19.666477	7.895027
-394.596330	11.959350	7.905024
-392.423405	9.035565	7.915021
-390.638966	13.355025	7.925018
-388.909593	14.915321	7.935014
-386.932767	13.603412	7.945011
-385.179895	9.197714	7.955008
-383.011017	11.407860	7.965005
-381.119877	10.706492	7.975002
-379.611450	9.669903	7.984998
-377.525626	14.662852	7.994995
-375.664851	18.199594	8.004992
-374.050725	11.106518	8.014989
-372.077519	8.224110	8.024986
-369.974070	12.565289	8.034982
-367.919213	10.497236	8.044979
-366.157562	7.954931	8.054976
-364.375436	2.764561	8.064973
-362.703348	4.160332	8.074970
-361.061933	7.706840	8.084966
-359.149919	14.047585	8.094963
-356.920099	12.051085	8.104960
-354.339970	14.102443	8.114957
-353.118791	8.862681	8.124954
-351.359916	14.520495	8.134950
-349.413670	13.567191	8.144947
-347.459876	11.079490	8.154944
-345.861113	9.299010	8.164941
-343.953723	13.120446	8.174938
-341.994979	5.718160	8.184934
-339.938051	4.867197	8.194931
-338.551093	9.899114	8.204928
-336.365466	10.071317	8.214925
-334.515800	11.599817	8.224922
-332.645820	13.197710	8.234918
-330.644286	5.299115	8.244915
-328.860369	4.278581	8.254912
-326.203343	1.564951	8.264909
-324.994832	3.585816	8.274906
-323.123259	6.670864	8.284902
-321.396555	8.680066	8.294899
-319.459390	7.361911	8.304896
-317.964109	3.889507	8.314893
-316.045185	10.563930	8.324890
-313.911372	8.456476	8.334886
-311.994665	11.185373	8.344883
-309.722042	7.165720	8.354880
-307.788747	4.573952	8.364877
-306.415137	5.687400	8.374874
-304.719082	10.088932	8.384870
-302.679155	8.754387	8.394867
-300.499118	5.965340	8.404864
-298.676865	9.107229	8.414861
-296.788724	6.142141	8.424858
-294.923822	8.843005	8.434854
-293.281629	7.553007	8.444851
-291.555162	10.509660	8.454848
-289.654341	8.210464	8.464845
-287.448318	9.519484	8.474842
-285.383813	4.633051	8.484838
-283.761260	3.690413	8.494835
-281.732670	8.923116	8.504832
-279.987363	9.453028	8.514829
-278.266034	4.430320	8.524826
-276.426656	3.045700	8.534822
-274.283626	7.663287	8.544819
-272.389084	5.388791	8.554816
-270.572805	2.138345	8.564813
-268.729027	4.111530	8.574810
-266.928031	5.598902	8.584807
-265.225320	8.079355	8.594803
-263.306843	9.189549	8.604800
-261.239519	3.064761	8.614797
-259.206266	10.385738	8.624794
-257.588263	5.723753	8.634791
-255.454515	3.902157	8.644787
-253.638050	10.585092	8.654784
-251.925428	4.472711	8.664781
-250.040352	7.156179	8.674778
-248.379910	12.349774	8.684775
-246.299036	10.708733	8.694771
-243.981324	5.431386	8.704768
-242.357925	8.905064	8.714765
-240.536802	2.634845	8.724762
-238.765591	-0.734705	8.734759
-236.625704	2.165481	8.744755
-234.659345	9.050304	8.754752
-233.240759	4.827538	8.764749
-231.415736	6.404263	8.774746
-229.011184	4.375256	8.784743
-227.673804	4.883465	8.794739
-225.511566	3.788418	8.804736
-223.592073	0.527850	8.814733
-221.708225	-1.719636	8.824730
-219.942791	5.276213	8.834727
-218.159542	2.582141	8.844723
-216.404001	-0.030137	8.854720
-214.443673	-0.822944	8.864717
-212.428187	-0.034514	8.874714
-210.586907	2.011749	8.884711
-208.982450	-4.670722	8.894707
-207.118543	2.637849	8.904704
-205.036207	-1.477660	8.914701
-202.952476	-6.422356	8.924698
-201.217070	-2.897051	8.934695
-199.229625	2.438608	8.944691
-197.392325	-5.245774	8.954688
-195.551678	1.775986	8.964685
-193.403468	-3.182152	8.974682
-192.187765	3.342483	8.984679
-190.156960	2.402655	8.994675
-187.975248	-1.368689	9.004672
-186.282217	-2.429880	9.014669
-184.332774	-5.800989	9.024666
-182.478934	3.711896	9.034663
-180.615398	1.039777	9.044659
-178.711918	2.045061	9.054656
-176.902368	2.285316	9.064653
-175.018288	1.918402	9.074650
-172.942819	4.029959	9.084647
-170.976016	7.966798	9.094643
-169.412181	9.261557	9.104640
-167.660726	3.940422	9.114637
-165.566862	7.969099	9.124634
-163.601781	4.807093	9.134631
-161.893476	5.748795	9.144627
-159.859027	6.155287	9.154624
-158.022780	5.821282	9.164621
-156.098326	1.448366	9.174618
-154.615211	-0.559859	9.184615
-152.617519	3.877342	9.194611
-150.529661	5.023760	9.204608
-148.737293	2.258807	9.214605
-146.777994	-1.641229	9.224602
-144.803416	4.673925	9.234599
-143.050648	7.722811	9.244595
-141.311818	4.773769	9.254592
-139.253636	12.891427	9.264589
-137.544944	8.781902	9.274586
-135.299521	7.282073	9.284583
-133.712603	10.027420	9.294579
-131.969358	5.509744	9.304576
-129.781632	11.345631	9.314573
-127.830979	3.685839	9.324570
-126.283536	2.194748	9.334567
-124.451499	8.936885	9.344563
-122.696496	4.066805	9.354560
-120.799638	15.120296	9.364557
-118.359990	6.136668	9.374554
-116.655743	7.931704	9.384551
-114.837025	11.600106	9.394547
-113.049817	14.908792	9.404544
-111.288351	10.347168	9.414541
-109.352736	6.130403	9.424538
-107.374057	10.772790	9.434535
-105.476778	9.173791	9.444531
-103.594652	15.761111	9.454528
-101.671730	9.956334	9.464525
-99.862070	7.907096	9.474522
-98.060646	9.730854	9.484519
-96.486966	15.920536	9.494515
-94.443501	14.050321	9.504512
-92.292698	7.621812	9.514509
-90.423756	14.711786	9.524506
-88.480291	13.871242	9.534503
-86.817897	19.159387	9.544499
-84.670229	15.196185	9.554496
-82.918388	17.139973	9.564493
-81.456005	15.670375	9.574490
-79.220405	10.722071	9.584487
-77.357724	12.758710	9.594483
-75.594800	12.872266	9.604480
-73.392090	15.923639	9.614477
-71.976435	7.618161	9.624474
-69.959232	17.703529	9.634471
-68.109888	11.741561	9.644467
-66.150263	12.839035	9.654464
-64.359246	7.655344	9.664461
-62.278020	8.586576	9.674458
-60.861647	4.310572	9.684455
-58.660788	10.532863	9.694451
-56.659776	10.876880	9.704448
-54.392703	15.675420	9.714445
-52.672872	8.676201	9.724442
-51.427031	10.999159	9.734439
-49.284606	13.368574	9.744435
-47.294779	12.346977	9.754432
-45.486687	13.782859	9.764429
-43.874935	7.686701	9.774426
-41.734439	8.220064	9.784423
-39.774445	11.810725	9.794419
-38.106946	6.574123	9.804416
-36.131504	12.777130	9.814413
-33.999211	4.928952	9.824410
-32.541811	8.110302	9.834407
-30.436060	12.154576	9.844403
-28.697446	21.625985	9.854400
-26.762993	14.796235	9.864397
-24.884847	11.796627	9.874394
-22.869623	4.958738	9.884391
-21.019893	11.743930	9.894387
-19.411669	17.612360	9.904384
-17.134428	7.958393	9.914381
-15.607340	4.653200	9.924378
-13.604015	9.875963	9.934375
-11.908183	12.850344	9.944371
-9.913050	9.568396	9.954368
-7.876590	3.011350	9.964365
-5.870307	5.164090	9.974362
-4.081458	11.892690	9.984359
-3.426647	32.018339	9.994355
-1.943701	74.828426	10.004352
-0.891012	141.965499	10.014349
0.000000	187.049601	10.019354
0.867759	237.155803	10.024359
1.262583	280.784382	10.029363
1.966605	314.938806	10.034368
2.158132	351.958473	10.039373
2.734912	365.447705	10.044378
3.226774	382.981336	10.049383
2.939317	411.566421	10.054387
3.626358	419.639996	10.059392
3.488285	441.519499	10.064397
3.930453	460.316456	10.069402
4.185880	460.983823	10.074407
4.159372	471.765436	10.079411
4.389103	480.517562	10.084416
3.897903	479.711222	10.089421
4.255886	487.865706	10.094426
4.185005	481.972662	10.099431
4.022069	488.464468	10.104435
4.393220	495.177035	10.109440
4.069237	514.938393	10.114445
4.618466	522.062559	10.119450
4.283934	533.128323	10.124455
4.573189	531.899441	10.129459
4.731508	525.462020	10.134464
4.161789	535.037158	10.139469
4.689778	536.093161	10.144474
5.064594	553.295567	10.149479
5.105169	571.021259	10.154483
5.385722	568.170996	10.159488
5.119077	554.111737	10.164493
5.112436	545.896494	10.169498
5.023869	550.758434	10.174503
5.206139	551.219843	10.179507
4.981642	551.036467	10.184512
5.026736	569.318128	10.189517
5.458928	576.091963	10.194522
5.566024	581.868925	10.199527
5.366859	586.491461	10.204531
5.517122	583.624127	10.209536
5.365119	588.355841	10.214541
5.528253	579.559962	10.219546
5.720897	593.918118	10.224551
5.830897	592.828214	10.229555
5.993071	587.956145	10.234560
5.724695	576.518171	10.239565
5.318386	571.706816	10.244570
5.920247	591.637592	10.249575
5.452020	602.904515	10.254579
5.961906	600.547552	10.259584
5.715083	603.342025	10.264589
5.863064	606.401552	10.269594
5.886196	608.601006	10.274599
5.834708	618.978260	10.279603
6.144775	603.495950	10.284608
5.799497	612.328828	10.289613
5.934028	614.789651	10.294618
6.014713	617.397843	10.299623
6.083846	615.297266	10.304627
6.373933	622.683600	10.309632
6.193012	642.848113	10.314637
6.356093	639.070349	10.319642
6.409067	644.179419	10.324647
6.098827	657.917640	10.329651
6.749440	654.579382	10.334656
6.361188	659.421344	10.339661
6.522612	653.218350	10.344666
6.665310	664.283795	10.349671
6.105808	668.238390	10.354675
6.284466	656.899372	10.359680
6.442577	670.523479	10.364685
6.912983	679.868156	10.369690
6.891286	691.995961	10.374695
6.798071	703.900202	10.379699
6.977318	691.670033	10.384704
7.060068	704.722685	10.389709
7.208408	698.603765	10.394714
7.187149	705.131421	10.399719
7.155226	701.905168	10.404723
7.112662	703.697198	10.409728
7.057799	709.315529	10.414733
7.329820	707.061147	10.419738
7.433749	710.234961	10.424743
7.126734	715.382548	10.429747
7.192141	702.886658	10.434752
7.261756	716.099120	10.439757
7.324914	723.053316	10.444762
6.998658	717.866422	10.449767
6.928883	721.400701	10.454771
7.612920	736.525921	10.459776
7.732642	754.024733	10.464781
7.818835	751.990807	10.469786
8.013630	763.095329	10.474791
7.773183	773.498100	10.479795
7.772149	759.254343	10.484800
7.778255	761.339834	10.489805
7.812031	756.051346	10.494810
8.155939	765.805786	10.499815
7.944969	763.628431	10.504819
7.935643	764.415315	10.509824
7.743524	768.227756	10.514829
7.645889	765.849385	10.519834
7.818717	765.815536	10.524839
7.791200	770.721432	10.529843
7.893201	770.648413	10.534848
7.805565	790.137466	10.539853
7.895836	794.264442	10.544858
8.303248	797.878759	10.549863
8.260380	806.299221	10.554867
8.501974	805.727666	10.559872
8.296736	801.033984	10.564877
8.421292	803.805534	10.569882
8.511766	815.029244	10.574887
8.540648	833.197119	10.579891
9.023716	832.006692	10.584896
8.838863	843.315340	10.589901
8.855491	841.797156	10.594906
8.747854	844.701948	10.599911
8.361518	842.929469	10.604915
8.821714	843.075305	10.609920
8.171772	856.949902	10.614925
8.352475	854.856729	10.619930
8.747718	849.764461	10.624935
8.789023	873.789194	10.629939
9.237995	883.539573	10.634944
9.281513	881.999749	10.639949
9.345954	878.373283	10.644954
9.340440	886.958157	10.649959
9.244838	881.497856	10.654963
9.362589	882.242399	10.659968
9.283187	892.957061	10.664973
9.456238	881.483136	10.669978
10.056520	885.326930	10.674983
9.462096	891.578629	10.679987
9.285336	891.859177	10.684992
9.497697	893.627918	10.689997
9.700308	892.895409	10.695002
9.765006	898.751805	10.700007
9.503487	902.824526	10.705011
9.930162	894.535244	10.710016
9.561655	896.593765	10.715021
9.384481	896.267207	10.720026
9.796327	890.702311	10.725031
9.584501	919.434034	10.730035
9.722789	932.250934	10.735040
9.787821	936.366205	10.740045
10.107410	928.682232	10.745050
9.853127	936.597130	10.750055
9.754138	943.671918	10.755059
10.182494	935.305068	10.760064
10.238392	943.389711	10.765069
10.289062	947.056233	10.770074
10.335047	956.587063	10.775079
10.315086	971.020505	10.780083
10.188349	964.607854	10.785088
10.203842	963.575577	10.790093
10.609964	965.453783	10.795098
10.620335	967.246865	10.800103
10.354121	967.325622	10.805107
10.971159	966.765149	10.810112
10.317551	975.071790	10.815117
10.464003	970.583754	10.820122
10.538544	970.165004	10.825127
10.322854	986.239873	10.830131
10.688174	989.474568	10.835136
10.915889	1007.470588	10.840141
10.947628	1004.035403	10.845146
11.214198	1012.520180	10.850151
11.147231	1011.795966	10.855155
11.225495	1005.736985	10.860160
11.066536	1018.528824	10.865165
10.805567	1014.361244	10.870170
11.268166	1017.048954	10.875175
11.245955	1012.679277	10.880179
11.289742	1009.499233	10.885184
11.093534	1020.732553	10.890189
11.547282	1010.920159	10.895194
11.270928	1015.252340	10.900199
11.576345	1021.642873	10.905203
11.616297	1015.634156	10.910208
11.358211	1029.307632	10.915213
11.623073	1020.637201	10.920218
11.695558	1029.504632	10.925223
11.761945	1032.804363	10.930227
12.025779	1046.670602	10.935232
11.876418	1049.854925	10.940237
12.006924	1041.149135	10.945242
11.915141	1042.239369	10.950247
11.926385	1050.113556	10.955251
12.205546	1049.395641	10.960256
12.223608	1039.536012	10.965261
12.019780	1030.229064	10.970266
12.104002	1041.056520	10.975271
11.856749	1049.421404	10.980275
12.129772	1055.534820	10.985280
11.879032	1058.076093	10.990285
12.298721	1057.916131	10.995290
12.324332	1056.361796	11.000295
12.295935	1062.598990	11.005299
12.411190	1068.363805	11.010304
12.012398	1070.640086	11.015309
12.384195	1075.174864	11.020314
12.631878	1067.857131	11.025319
12.464944	1065.582812	11.030323
12.787808	1062.817177	11.035328
12.232353	1076.642214	11.040333
12.581118	1082.756178	11.045338
12.688588	1087.976570	11.050343
12.634174	1104.017960	11.055347
12.991277	1101.202699	11.060352
13.013139	1100.393344	11.065357
13.002176	1095.023551	11.070362
12.883148	1107.777558	11.075367
13.052824	1098.955090	11.080371
12.810572	1103.441145	11.085376
12.947663	1100.801335	11.090381
13.247212	1102.513615	11.095386
12.933082	1107.313936	11.100391
12.820697	1108.768615	11.105395
13.130841	1112.937890	11.110400
13.198529	1130.307459	11.115405
13.281286	1134.718819	11.120410
13.338929	1132.757997	11.125415
13.395791	1139.384572	11.130419
13.718285	1126.076906	11.135424
13.518472	1141.533558	11.140429
13.755551	1139.179019	11.145434
13.644635	1135.938458	11.150439
13.334833	1147.753015	11.155443
13.840525	1138.224803	11.160448
13.670124	1138.733018	11.165453
13.643532	1132.364250	11.170458
13.942592	1136.053498	11.175463
13.634871	1133.608429	11.180467
14.135927	1127.403899	11.185472
13.657813	1143.733703	11.190477
13.728949	1150.943897	11.195482
14.400298	1158.201882	11.200487
14.360105	1172.438459	11.205491
14.558125	1167.566789	11.210496
14.535517	1147.756577	11.215501
14.340815	1141.892477	11.220506
14.055924	1138.174205	11.225511
14.254277	1145.137005	11.230515
14.549729	1140.721356	11.235520
14.392111	1156.412590	11.240525
14.468961	1171.008212	11.245530
14.650672	1167.400822	11.250535
14.430152	1171.039684	11.255539
15.049297	1172.252316	11.260544
14.942249	1168.085375	11.265549
14.669989	1148.928470	11.270554
14.826785	1152.221694	11.275559
14.902705	1160.822917	11.280563
14.990562	1143.934799	11.285568
14.758629	1147.588881	11.290573
14.686285	1153.775559	11.295578
14.920067	1160.121592	11.300583
15.023745	1168.622190	11.305587
15.210340	1168.721775	11.310592
15.081275	1170.765800	11.315597
15.182424	1179.396918	11.320602
14.764026	1179.282308	11.325607
14.740537	1176.848673	11.330611
15.087774	1175.416509	11.335616
14.988009	1173.789899	11.340621
14.809146	1183.415091	11.345626
15.252095	1197.386960	11.350631
15.324966	1208.141440	11.355635
15.425851	1208.533054	11.360640
15.214772	1215.141681	11.365645
15.596968	1207.636828	11.370650
15.599386	1205.437988	11.375655
15.556364	1212.854884	11.380659
15.898119	1217.265177	11.385664
15.644869	1216.194524	11.390669
15.715462	1208.188173	11.395674
15.864425	1208.542154	11.400679
15.661493	1215.145539	11.405683
15.604463	1215.405418	11.410688
16.016472	1239.239153	11.415693
16.174414	1243.266357	11.420698
16.017449	1238.221025	11.425703
16.261980	1254.199130	11.430707
16.309086	1242.290803	11.435712
16.229832	1247.839107	11.440717
16.356597	1249.742982	11.445722
16.635317	1250.942100	11.450727
16.277224	1238.427344	11.455731
16.157733	1234.602234	11.460736
16.302836	1246.975159	11.465741
16.267054	1237.253308	11.470746
16.520790	1242.986643	11.475751
16.394485	1244.548432	11.480755
16.396351	1238.251568	11.485760
16.380031	1244.698245	11.490765
16.425002	1248.365753	11.495770
16.600551	1240.524011	11.500775
16.579261	1242.162100	11.505779
16.642389	1240.530004	11.510784
16.563772	1262.389426	11.515789
16.923278	1270.759386	11.520794
17.003643	1270.159908	11.525799
16.683056	1277.326188	11.530803
17.290191	1272.071446	11.535808
17.227493	1269.810435	11.540813
17.347502	1273.314578	11.545818
17.559860	1273.872937	11.550823
17.357350	1276.132137	11.555827
17.607831	1267.055382	11.560832
17.284264	1270.096421	11.565837
17.571864	1254.140719	11.570842
17.192002	1248.691709	11.575847
17.334865	1255.822701	11.580851
17.671407	1264.436829	11.585856
17.814274	1272.797183	11.590861
17.320921	1265.303410	11.595866
17.674607	1267.684444	11.600871
17.956788	1267.345332	11.605875
18.020294	1268.844520	11.610880
17.625457	1263.869447	11.615885
17.455699	1252.290619	11.620890
17.466657	1266.768313	11.625895
17.564869	1276.150660	11.630899
17.934510	1277.806047	11.635904
17.937978	1281.419463	11.640909
17.795422	1280.454954	11.645914
17.659007	1278.823136	11.650919
17.545873	1290.044990	11.655923
18.131945	1287.091452	11.660928
18.234323	1300.034265	11.665933
17.922179	1315.382848	11.670938
18.036533	1316.348752	11.675943
18.560903	1314.334758	11.680947
18.626714	1314.810037	11.685952
18.650115	1316.605814	11.690957
18.631176	1309.744477	11.695962
18.779702	1312.001317	11.700967
18.700789	1304.690607	11.705971
18.357764	1291.548865	11.710976
18.473002	1292.410538	11.715981
18.613415	1305.725007	11.720986
18.813501	1318.711394	11.725991
18.422410	1311.758008	11.730995
19.043245	1306.736847	11.736000
18.990376	1311.795217	11.741005
19.231687	1307.980359	11.746010
19.050488	1308.795473	11.751015
18.580866	1317.169164	11.756019
19.094082	1307.377843	11.761024
18.952147	1312.872295	11.766029
18.819308	1314.459579	11.771034
18.927645	1312.203613	11.776039
18.861155	1314.452953	11.781043
18.935824	1316.316256	11.786048
18.742300	1322.232143	11.791053
18.815070	1334.376169	11.796058
19.159863	1346.536750	11.801063
19.159948	1350.340766	11.806067
19.482162	1352.287607	11.811072
19.290096	1348.588383	11.816077
19.717243	1351.973378	11.821082
19.871996	1339.860126	11.826087
19.352916	1349.120965	11.831091
19.939976	1344.684769	11.836096
19.667934	1341.223041	11.841101
19.685548	1346.852926	11.846106
19.901275	1342.312724	11.851111
19.838738	1339.805645	11.856115
20.059903	1345.537908	11.861120
19.787348	1352.727317	11.866125
19.713445	1345.228111	11.871130
19.929621	1342.477076	11.876135
19.722651	1349.018868	11.881139
20.325114	1363.203601	11.886144
20.351431	1379.094420	11.891149
20.327874	1360.719249	11.896154
20.143668	1352.513735	11.901159
20.175135	1368.004710	11.906163
20.542186	1368.658262	11.911168
20.219009	1384.672644	11.916173
20.565855	1377.684331	11.921178
20.973374	1372.558384	11.926183
20.618178	1354.401711	11.931187
20.744937	1348.918386	11.936192
20.200830	1346.731777	11.941197
20.598780	1353.634456	11.946202
20.815284	1370.133665	11.951207
20.436071	1379.727856	11.956211
20.924227	1377.065125	11.961216
21.008412	1371.915834	11.966221
20.913916	1383.277516	11.971226
21.353778	1372.340244	11.976231
21.049652	1371.827320	11.981235
20.888262	1351.263811	11.986240
20.699056	1364.208238	11.991245
21.331783	1365.866624	11.996250
21.302682	1383.039809	12.001255
21.122463	1383.600854	12.006259
21.548713	1367.374520	12.011264
21.099711	1377.811771	12.016269
21.210926	1387.240218	12.021274
21.349035	1378.134792	12.026279
21.320814	1377.932715	12.031283
21.371574	1366.659282	12.036288
21.140997	1379.348519	12.041293
21.159542	1371.226575	12.046298
21.452444	1371.932170	12.051303
21.207307	1384.467599	12.056307
21.542114	1380.916961	12.061312
21.368576	1381.226967	12.066317
21.124248	1376.495173	12.071322
21.186452	1373.797865	12.076327
21.254288	1376.143286	12.081331
21.303082	1374.019823	12.086336
21.369274	1378.855778	12.091341
21.267821	1376.076539	12.096346
21.523440	1380.205698	12.101351
21.101082	1383.594500	12.106355
21.499478	1377.484306	12.111360
21.332068	1379.616485	12.116365
21.263579	1386.127534	12.121370
21.810307	1374.937436	12.126375
21.527625	1359.208996	12.131379
21.254630	1343.612293	12.136384
20.984448	1350.903047	12.141389
20.924359	1357.028715	12.146394
20.954220	1357.676114	12.151399
21.178909	1377.816380	12.156403
21.462033	1367.420616	12.161408
21.434862	1380.436996	12.166413
21.293632	1374.988517	12.171418
21.365439	1379.955267	12.176423
21.251403	1386.368701	12.181427
21.513282	1377.311352	12.186432
21.324411	1387.278144	12.191437
21.358464	1374.169236	12.196442
21.370695	1366.976437	12.201447
21.238824	1365.858025	12.206451
21.569595	1353.612599	12.211456
20.938145	1352.949220	12.216461
21.208838	1363.855998	12.221466
21.357280	1373.647545	12.226471
21.284642	1377.806190	12.231475
21.571390	1380.432121	12.236480
21.295188	1369.693432	12.241485
21.232400	1350.289152	12.246490
21.116365	1352.327181	12.251495
21.192683	1375.140663	12.256499
21.690038	1372.119249	12.261504
21.323502	1355.097543	12.266509
21.587296	1346.841871	12.271514
21.591247	1348.490929	12.276519
21.409213	1354.269365	12.281523
21.362297	1349.072387	12.286528
21.060990	1352.926838	12.291533
21.047586	1353.722290	12.296538
21.244092	1348.690725	12.301543
20.816713	1352.282979	12.306547
21.200879	1367.731107	12.311552
21.654617	1380.198440	12.316557
21.624648	1375.240048	12.321562
21.654930	1357.973682	12.326567
21.258919	1351.058912	12.331571
21.726778	1354.470534	12.336576
21.772838	1358.958785	12.341581
21.546685	1348.901330	12.346586
21.678439	1348.190353	12.351591
21.079319	1355.307254	12.356595
21.302293	1348.429395	12.361600
21.391961	1357.186254	12.366605
21.401941	1364.508822	12.371610
21.287257	1359.563947	12.376615
21.390863	1363.245000	12.381619
21.566727	1356.170414	12.386624
21.357284	1357.816445	12.391629
21.223788	1343.117742	12.396634
21.351497	1331.258783	12.401639
21.293292	1344.401518	12.406643
21.401668	1334.684997	12.411648
21.400424	1328.161486	12.416653
21.170684	1333.412092	12.421658
21.598976	1325.198012	12.426663
21.079773	1327.233311	12.431667
21.635094	1322.766699	12.436672
21.292989	1330.434015	12.441677
21.218123	1328.096080	12.446682
21.380908	1327.263448	12.451687
21.033410	1335.697316	12.456691
20.901444	1333.489924	12.461696
21.062882	1342.102061	12.466701
21.654689	1362.568570	12.471706
21.574865	1351.700004	12.476711
21.339363	1340.998216	12.481715
21.401348	1338.634509	12.486720
21.376739	1337.895637	12.491725
21.072120	1328.256818	12.496730
21.558599	1324.435185	12.501735
21.323519	1327.903714	12.506739
21.832205	1316.352261	12.511744
21.353664	1324.650100	12.516749
21.446689	1334.489887	12.521754
21.468238	1331.689461	12.526759
21.114433	1336.105059	12.531763
21.486532	1326.645346	12.536768
21.403492	1342.862682	12.541773
21.155665	1333.560190	12.546778
21.549460	1336.888993	12.551783
21.484603	1341.599954	12.556787
21.564580	1334.187398	12.561792
21.483440	1335.185272	12.566797
21.225762	1340.807015	12.571802
21.434939	1327.684413	12.576807
21.168127	1332.337685	12.581811
21.481483	1334.137688	12.586816
21.548615	1335.081949	12.591821
21.603199	1329.122025	12.596826
21.574226	1314.015557	12.601831
21.405547	1308.198494	12.606835
21.365648	1299.774432	12.611840
21.203043	1304.499394	12.616845
21.354076	1301.727213	12.621850
21.361630	1294.214253	12.626855
21.300008	1298.958592	12.631859
21.506855	1288.132670	12.636864
21.157673	1296.650372	12.641869
21.317234	1296.999511	12.646874
21.606395	1297.202601	12.651879
21.476695	1300.199319	12.656883
21.519885	1295.461123	12.661888
21.565633	1300.420961	12.666893
21.429186	1298.831729	12.671898
21.426289	1299.749305	12.676903
21.318832	1297.429189	12.681907
21.274371	1299.619815	12.686912
21.378837	1305.699502	12.691917
21.506463	1296.434934	12.696922
21.275725	1305.666317	12.701927
21.172498	1306.808075	12.706931
21.399133	1303.021581	12.711936
21.089192	1313.786726	12.716941
21.125801	1311.615536	12.721946
21.340429	1302.572866	12.726951
21.013404	1309.606133	12.731955
21.155342	1302.102490	12.736960
21.035919	1309.273763	12.741965
20.997025	1307.967045	12.746970
21.340033	1309.263948	12.751975
21.170003	1307.962373	12.756979
21.202093	1300.297248	12.761984
21.069109	1305.802099	12.766989
21.376546	1302.994722	12.771994
21.153560	1304.183179	12.776999
21.039711	1315.249032	12.782003
21.358107	1306.943669	12.787008
21.182462	1315.384025	12.792013
21.243739	1320.262538	12.797018
21.195638	1320.562788	12.802023
21.225403	1334.930307	12.807027
21.310201	1336.256566	12.812032
21.424630	1345.753078	12.817037
21.703526	1342.998348	12.822042
21.763393	1326.567115	12.827047
21.461693	1321.141884	12.832051
21.337520	1318.233013	12.837056
21.573559	1319.942833	12.842061
21.220699	1314.289197	12.847066
21.539442	1319.032809	12.852071
21.263036	1317.243523	12.857075
21.231432	1314.761481	12.862080
21.249126	1321.503996	12.867085
21.162778	1322.987662	12.872090
21.258097	1321.948937	12.877095
21.245074	1327.102681	12.882099
21.107874	1324.187212	12.887104
21.095798	1320.501871	12.892109
21.254386	1317.387826	12.897114
21.297548	1313.926300	12.902119
21.024627	1324.133559	12.907123
21.324091	1312.427802	12.912128
21.210116	1322.451209	12.917133
21.119215	1324.662650	12.922138
21.377735	1320.693642	12.927143
21.184356	1322.683283	12.932147
21.195322	1323.575782	12.937152
21.452605	1344.929913	12.942157
21.453164	1345.548077	12.947162
21.487506	1332.001512	12.952167
21.272260	1333.803023	12.957171
21.392512	1330.773156	12.962176
21.428601	1328.155723	12.967181
21.206779	1322.643628	12.972186
21.228447	1323.364092	12.977191
21.233482	1328.305988	12.982195
21.407389	1327.898980	12.987200
21.205248	1327.120607	12.992205
21.348855	1326.961307	12.997210
21.446271	1330.148914	13.002215
21.180218	1332.418257	13.007219
21.432121	1323.666126	13.012224
21.335583	1325.780686	13.017229
21.393166	1330.085722	13.022234
21.743217	1326.885151	13.027239
21.479616	1326.672513	13.032243
21.865838	1324.200320	13.037248
21.316877	1326.895656	13.042253
21.646570	1323.688081	13.047258
21.640508	1328.166499	13.052263
21.278110	1329.559349	13.057267
21.455380	1312.948541	13.062272
21.426791	1308.368460	13.067277
20.943751	1303.738634	13.072282
21.518178	1312.283308	13.077287
21.312613	1321.628182	13.082291
21.519346	1303.570415	13.087296
21.271167	1310.844234	13.092301
21.277299	1301.784350	13.097306
21.457950	1303.498270	13.102311
21.281366	1301.019639	13.107315
21.244723	1296.300483	13.112320
21.299059	1299.356168	13.117325
21.100828	1303.760349	13.122330
21.110362	1303.120123	13.127335
21.140809	1310.284053	13.132339
21.616097	1323.419750	13.137344
21.188672	1312.270727	13.142349
21.593360	1316.373728	13.147354
21.343849	1305.919441	13.152359
21.143190	1310.300355	13.157363
21.474603	1299.549185	13.162368
21.311938	1309.301989	13.167373
21.627961	1310.763273	13.172378
21.262983	1308.659287	13.177383
21.006805	1316.946102	13.182387
21.107333	1311.716158	13.187392
21.135034	1306.997776	13.192397
21.188596	1309.990502	13.197402
21.371362	1315.904726	13.202407
21.104945	1329.832150	13.207411
21.690750	1327.307622	13.212416
21.645222	1322.477111	13.217421
21.013327	1305.209963	13.222426
21.147960	1308.774079	13.227431
20.957465	1307.629537	13.232435
21.264623	1318.819077	13.237440
21.200563	1338.364244	13.242445
21.215918	1342.478879	13.247450
21.586775	1337.371409	13.252455
21.751259	1338.900235	13.257459
21.518962	1317.173132	13.262464
21.435490	1304.426842	13.267469
21.411586	1311.257997	13.272474
21.413453	1300.021590	13.277479
21.086661	1310.403817	13.282483
21.112899	1301.731850	13.287488
20.983172	1304.770367	13.292493
21.320267	1305.155065	13.297498
21.447092	1294.635245	13.302503
21.510321	1306.428285	13.307507
21.390680	1305.291368	13.312512
21.393339	1307.664522	13.317517
21.132792	1305.293119	13.322522
21.382441	1311.063408	13.327527
21.158468	1311.279733	13.332531
21.412138	1306.020636	13.337536
21.261352	1315.050809	13.342541
21.547344	1312.650591	13.347546
21.316117	1294.238443	13.352551
21.329631	1309.781899	13.357555
21.522160	1307.074857	13.362560
21.682253	1312.789248	13.367565
21.225145	1304.655674	13.372570
21.497057	1302.610188	13.377575
20.826682	1316.498726	13.382579
21.182099	1307.632314	13.387584
20.941569	1314.423896	13.392589
21.210103	1311.324647	13.397594
21.410541	1308.974349	13.402599
21.143690	1307.517099	13.407603
21.328691	1314.981268	13.412608
21.401262	1317.556971	13.417613
21.055516	1313.463543	13.422618
21.361104	1312.224898	13.427623
21.497732	1321.404797	13.432627
21.571139	1317.777582	13.437632
21.299993	1321.592517	13.442637
21.160067	1321.573065	13.447642
21.409923	1313.455267	13.452647
21.007985	1321.692785	13.457651
21.491220	1316.614712	13.462656
21.368518	1307.774876	13.467661
21.252569	1314.619136	13.472666
21.427423	1309.073745	13.477671
21.199942	1318.306194	13.482675
21.427548	1314.283764	13.487680
21.529023	1316.256344	13.492685
21.468871	1315.072087	13.497690
21.496547	1309.157468	13.502695
21.234032	1322.108819	13.507699
21.453390	1318.241472	13.512704
21.412363	1320.165809	13.517709
21.155672	1319.356709	13.522714
21.431867	1321.928326	13.527719
21.372974	1323.771138	13.532723
21.357958	1310.966610	13.537728
21.399867	1314.338126	13.542733
21.455852	1324.767345	13.547738
21.274538	1310.944503	13.552743
21.017130	1323.562269	13.557747
21.325877	1315.068398	13.562752
21.705812	1322.120607	13.567757
21.505684	1320.760747	13.572762
21.219603	1321.289784	13.577767
21.030951	1322.287456	13.582771
21.431128	1322.117201	13.587776
21.545690	1325.241353	13.592781
21.297961	1323.193577	13.597786
21.409851	1313.090118	13.602791
21.107607	1327.001173	13.607795
21.570944	1316.284938	13.612800
21.178663	1329.634710	13.617805
21.330920	1321.305368	13.622810
21.357942	1329.957073	13.627815
21.184722	1328.551916	13.632819
21.456492	1329.188332	13.637824
21.538807	1328.107521	13.642829
20.980837	1307.431477	13.647834
21.218377	1308.100950	13.652839
20.987068	1315.729297	13.657843
21.019784	1320.690433	13.662848
20.946677	1321.856564	13.667853
21.256843	1329.723443	13.672858
21.674269	1328.101069	13.677863
21.052013	1327.081375	13.682867
21.364697	1316.322928	13.687872
21.575487	1315.565439	13.692877
21.487565	1326.839287	13.697882
21.349407	1320.438551	13.702887
21.111927	1331.246562	13.707891
21.250897	1328.240522	13.712896
21.319554	1321.936911	13.717901
21.168689	1318.745263	13.722906
21.748356	1323.053771	13.727911
21.271780	1327.140405	13.732915
21.315812	1335.934495	13.737920
21.161206	1326.072247	13.742925
20.791106	1331.730054	13.747930
21.482506	1325.939041	13.752935
21.580723	1329.146233	13.757939
21.399689	1333.409683	13.762944
21.368152	1339.466128	13.767949
21.436785	1327.028330	13.772954
21.548966	1334.994605	13.777959
21.080127	1344.636976	13.782963
21.180758	1339.250872	13.787968
21.044967	1336.668736	13.792973
20.978192	1330.710031	13.797978
21.259779	1326.344640	13.802983
21.046489	1333.821085	13.807987
21.276117	1330.435483	13.812992
21.496221	1334.076657	13.817997
21.341891	1339.838052	13.823002
21.438156	1328.726931	13.828007
21.286660	1337.597943	13.833011
21.658088	1332.858639	13.838016
21.386557	1343.428426	13.843021
21.456723	1343.476402	13.848026
21.607810	1338.154798	13.853031
21.812621	1329.179916	13.858035
21.337983	1310.584195	13.863040
21.126434	1311.721150	13.868045
21.061069	1308.562392	13.873050
21.065675	1309.219338	13.878055
20.936686	1332.118330	13.883059
21.170450	1329.870745	13.888064
21.528549	1336.688300	13.893069
21.378733	1339.312881	13.898074
21.555672	1340.480928	13.903079
21.499599	1342.988046	13.908083
21.660728	1328.622454	13.913088
21.597383	1313.764344	13.918093
21.483998	1305.615376	13.923098
21.383593	1298.780442	13.928103
21.068861	1308.167163	13.933107
21.506171	1303.564821	13.938112
21.489187	1312.252711	13.943117
21.156982	1304.919314	13.948122
21.474801	1303.659793	13.953127
21.303617	1302.871753	13.958131
21.489205	1294.638835	13.963136
21.270250	1305.761660	13.968141
21.599999	1309.873457	13.973146
21.188603	1304.056468	13.978151
20.795462	1305.134854	13.983155
21.485029	1308.290309	13.988160
21.052280	1303.974982	13.993165
21.105896	1306.887266	13.998170
21.305811	1305.327973	14.003175
21.240530	1310.681665	14.008179
21.185308	1305.728902	14.013184
20.969526	1305.875316	14.018189
21.051744	1309.923965	14.023207
21.388772	1307.876346	14.028224
21.147721	1315.138442	14.033242
21.495545	1329.969146	14.038259
21.629294	1324.498652	14.043277
21.507697	1319.405526	14.048295
21.207497	1311.659557	14.053312
20.656954	1316.409238	14.058330
21.305885	1329.223982	14.063347
21.445533	1340.665640	14.068365
21.443181	1344.459552	14.073383
21.853091	1344.000927	14.078400
21.595921	1349.836455	14.083418
21.833079	1345.242978	14.088435
21.506732	1345.109427	14.093453
21.720354	1349.096206	14.098471
21.631341	1346.333131	14.103488
21.409512	1346.626522	14.108506
21.677434	1339.734571	14.113523
21.377347	1351.512223	14.118541
21.351315	1339.486958	14.123559
21.757523	1337.251329	14.128576
21.541825	1344.257701	14.133594
21.376106	1338.317416	14.138611
21.398428	1349.040013	14.143629
21.815067	1348.233447	14.148647
21.797213	1347.204370	14.153664
21.579901	1355.425431	14.158682
21.679496	1346.312372	14.163699
21.448621	1344.310491	14.168717
21.438252	1351.635704	14.173735
21.767156	1354.514731	14.178752
21.539190	1377.647296	14.183770
21.729771	1377.156007	14.188787
21.732386	1380.809917	14.193805
21.998870	1382.252443	14.198823
21.966909	1376.749368	14.203840
21.722256	1389.467573	14.208858
22.001003	1380.946506	14.213875
22.157706	1388.704436	14.218893
22.168054	1381.873995	14.223911
22.296203	1377.503182	14.228928
22.175148	1386.358598	14.233946
22.197194	1380.268795	14.238963
22.214398	1379.051645	14.243981
22.313316	1389.428558	14.248999
22.461522	1378.056624	14.254016
22.008498	1367.981646	14.259034
22.253880	1370.624662	14.264051
22.241681	1364.721233	14.269069
22.010537	1374.203774	14.274087
22.049779	1367.907517	14.279104
21.999361	1379.291425	14.284122
21.649741	1381.183014	14.289139
21.742562	1376.179159	14.294157
21.500378	1374.078399	14.299175
22.033288	1385.436134	14.304192
21.925602	1403.577783	14.309210
22.391607	1410.449505	14.314227
22.382376	1417.282189	14.319245
22.363844	1416.049498	14.324263
22.555380	1405.497296	14.329280
22.502502	1415.682924	14.334298
22.434033	1418.719727	14.339315
22.637725	1414.366744	14.344333
22.289800	1417.381261	14.349351
22.575859	1407.630421	14.354368
22.251957	1418.559305	14.359386
22.664359	1418.021626	14.364403
22.845679	1408.175800	14.369421
22.401990	1417.191235	14.374439
22.624769	1409.769237	14.379456
22.467102	1416.244118	14.384474
22.598835	1417.520940	14.389491
22.860034	1417.126145	14.394509
22.664951	1418.746115	14.399527
22.498543	1408.921926	14.404544
22.484936	1424.846257	14.409562
22.592597	1417.052486	14.414579
22.852411	1415.062788	14.419597
22.525333	1414.801145	14.424615
22.487214	1416.167194	14.429632
22.351355	1416.678907	14.434650
22.315073	1411.568210	14.439667
22.513326	1427.766296	14.444685
22.503668	1447.554347	14.449703
23.164111	1444.172263	14.454720
23.070391	1451.000347	14.459738
23.019801	1456.489923	14.464755
23.517301	1453.806327	14.469773
23.390162	1447.259705	14.474791
22.991710	1420.965948	14.479808
23.055799	1416.412635	14.484826
23.059914	1414.103479	14.489843
22.924360	1416.615341	14.494861
23.095240	1421.357753	14.499879
23.222283	1405.123572	14.504896
22.932316	1418.795249	14.509914
22.985447	1422.228744	14.514931
23.135526	1419.097958	14.519949
22.614013	1415.548869	14.524967
22.800389	1431.278497	14.529984
23.312182	1442.634139	14.535002
23.106103	1444.911063	14.540019
23.306094	1449.860424	14.545037
23.263302	1452.149847	14.550055
23.372232	1438.742240	14.555072
23.265742	1446.454084	14.560090
23.420338	1452.481969	14.565107
23.445436	1449.153235	14.570125
23.080122	1452.661341	14.575143
23.133079	1453.897245	14.580160
23.457293	1450.346190	14.585178
23.413550	1442.999717	14.590195
23.607942	1445.354350	14.595213
23.355117	1455.678865	14.600231
23.707554	1446.296531	14.605248
23.605509	1450.966859	14.610266
23.421279	1450.910532	14.615283
23.790967	1449.856607	14.620301
23.758328	1445.379277	14.625319
23.766810	1447.530741	14.630336
23.648636	1440.941792	14.635354
23.560208	1440.982662	14.640371
23.489079	1432.046223	14.645389
23.537789	1447.101726	14.650407
23.851469	1434.894781	14.655424
23.970867	1445.016771	14.660442
23.331888	1434.799937	14.665459
23.787543	1427.817438	14.670477
23.741526	1437.456120	14.675495
23.679508	1431.946806	14.680512
23.575235	1448.610037	14.685530
23.872900	1444.666796	14.690547
23.696025	1444.544798	14.695565
23.686475	1446.936677	14.700583
24.041660	1440.776412	14.705600
23.894147	1445.405223	14.710618
23.786305	1447.779743	14.715635
23.956611	1443.546913	14.720653
23.774383	1441.688277	14.725671
23.451707	1443.369499	14.730688
23.638584	1446.032872	14.735706
23.686343	1446.527099	14.740723
23.687736	1444.647829	14.745741
23.540340	1454.023465	14.750759
23.740060	1471.693793	14.755776
23.808617	1467.757983	14.760794
24.160976	1473.266673	14.765811
24.531339	1472.422649	14.770829
24.399357	1470.751060	14.775847
24.045418	1477.947079	14.780864
24.114996	1477.388565	14.785882
24.123313	1481.020354	14.790899
24.336802	1472.906065	14.795917
24.365487	1480.144886	14.800935
24.655009	1476.231251	14.805952
24.497450	1477.615568	14.810970
24.331974	1474.993659	14.815987
24.538986	1468.075967	14.821005
24.452231	1471.736288	14.826023
24.765677	1463.580106	14.831040
24.447943	1445.459874	14.836058
24.032895	1441.845818	14.841075
24.527682	1437.123130	14.846093
24.451819	1452.592569	14.851111
24.425032	1449.095135	14.856128
24.505821	1452.477034	14.861146
24.234242	1462.902865	14.866163
24.524136	1469.504600	14.871181
24.441381	1480.643620	14.876199
24.203424	1479.516710	14.881216
24.417709	1473.890950	14.886234
24.221680	1474.477545	14.891251
24.196850	1474.170055	14.896269
24.270236	1475.227301	14.901287
24.604106	1464.436840	14.906304
24.652700	1459.974866	14.911322
24.375109	1470.892470	14.916339
24.699361	1483.291922	14.921357
25.062006	1500.299978	14.926375
25.077308	1497.041225	14.931392
25.186586	1473.259666	14.936410
24.862457	1480.831624	14.941427
25.077857	1464.900266	14.946445
24.568719	1468.438392	14.951463
24.966616	1467.730769	14.956480
24.960773	1468.198152	14.961498
24.838979	1478.171433	14.966515
25.099138	1467.049789	14.971533
24.965262	1471.939142	14.976551
24.858842	1482.006720	14.981568
24.979236	1467.231801	14.986586
24.685761	1473.904556	14.991603
25.045529	1474.344303	14.996621
24.970446	1496.016425	15.001639
24.876160	1497.545604	15.006656
25.007082	1497.594752	15.011674
24.929371	1508.477359	15.016691
25.355587	1496.869073	15.021709
25.322440	1503.009511	15.026727
25.466340	1501.859452	15.031744
25.387223	1498.869815	15.036762
25.105183	1504.216201	15.041779
25.387369	1499.110526	15.046797
25.350076	1504.147303	15.051815
25.198965	1503.145761	15.056832
25.834989	1497.390591	15.061850
25.018833	1502.032461	15.066867
25.395800	1502.266535	15.071885
25.566304	1513.738802	15.076903
25.509900	1507.108509	15.081920
25.440442	1506.716895	15.086938
25.427755	1508.938602	15.091955
25.478434	1509.934188	15.096973
25.320770	1506.551214	15.101991
25.579007	1504.497258	15.107008
25.688755	1497.238755	15.112026
25.409408	1513.275570	15.117043
25.750829	1507.051401	15.122061
25.691266	1503.976843	15.127079
25.633501	1509.256786	15.132096
25.641073	1515.248368	15.137114
25.643488	1515.514650	15.142131
25.578439	1508.441331	15.147149
25.517240	1502.923207	15.152167
25.495003	1506.072998	15.157184
25.686901	1497.439866	15.162202
25.329438	1512.430436	15.167219
25.194465	1506.673952	15.172237
25.518812	1511.546869	15.177255
26.011739	1521.960930	15.182272
26.163230	1530.235747	15.187290
25.940108	1531.246686	15.192307
25.850028	1506.707166	15.197325
25.829449	1525.809616	15.202343
26.260349	1537.883776	15.207360
25.862744	1527.526913	15.212378
25.720345	1531.789187	15.217395
26.347508	1534.538881	15.222413
26.272233	1539.268678	15.227431
26.097573	1534.554408	15.232448
25.999662	1532.959180	15.237466
26.295949	1548.344197	15.242483
26.330479	1531.956307	15.247501
26.295311	1522.693162	15.252519
26.246999	1511.187289	15.257536
26.268571	1505.815634	15.262554
26.144396	1503.390850	15.267571
26.221564	1499.950761	15.272589
25.981539	1520.416694	15.277607
26.149168	1527.629445	15.282624
26.874380	1527.080415	15.287642
26.566108	1531.544545	15.292659
26.320422	1508.886898	15.297677
26.121793	1517.102711	15.302695
26.055684	1533.792988	15.307712
26.560685	1532.070928	15.312730
26.452148	1547.805242	15.317747
26.475946	1539.060462	15.322765
26.788671	1538.159556	15.327783
26.767923	1537.822311	15.332800
26.905770	1532.305465	15.337818
26.325309	1525.724136	15.342835
26.639529	1529.942687	15.347853
26.701380	1536.169453	15.352871
26.444798	1539.868675	15.357888
26.630148	1537.466097	15.362906
26.888837	1540.885713	15.367923
27.109376	1534.405518	15.372941
26.875338	1535.951484	15.377959
26.557572	1526.489575	15.382976
26.706267	1521.768571	15.387994
26.356201	1535.396456	15.393011
26.675294	1529.769690	15.398029
26.543102	1538.262012	15.403047
26.599022	1535.010144	15.408064
26.806865	1531.763150	15.413082
26.859171	1541.373635	15.418099
27.025520	1539.448380	15.423117
26.815692	1541.240610	15.428135
26.833569	1541.467458	15.433152
26.923134	1534.016304	15.438170
26.899479	1540.545376	15.443187
26.779665	1535.204911	15.448205
26.822945	1544.950552	15.453223
26.945871	1569.425955	15.458240
27.398928	1562.705732	15.463258
27.135328	1568.418882	15.468275
27.047208	1563.066274	15.473293
27.083457	1568.692274	15.478311
27.111971	1567.573984	15.483328
27.431647	1564.759845	15.488346
27.229323	1572.415462	15.493363
27.514529	1566.434629	15.498381
27.588347	1563.146865	15.503399
27.224543	1569.273996	15.508416
27.788212	1562.374887	15.513434
27.460417	1565.642640	15.518451
27.683303	1566.687062	15.523469
27.552935	1544.100635	15.528487
27.244216	1538.162625	15.533504
27.668854	1537.573437	15.538522
27.296906	1544.960348	15.543539
27.619148	1554.261933	15.548557
27.737488	1562.299796	15.553575
27.392956	1570.000116	15.558592
27.607700	1558.761370	15.563610
27.470613	1569.743160	15.568627
27.848696	1564.604077	15.573645
27.939768	1565.947963	15.578663
27.497330	1571.810767	15.583680
28.004476	1568.077917	15.588698
27.734051	1564.436045	15.593715
27.934951	1556.939593	15.598733
28.116743	1561.161183	15.603751
27.524628	1540.225454	15.608768
27.841415	1552.869203	15.613786
27.498688	1561.527258	15.618803
27.778533	1567.362173	15.623821
27.425128	1566.350415	15.628839
27.695795	1570.089044	15.633856
27.902476	1562.450873	15.638874
27.596290	1562.520181	15.643891
27.819867	1561.288192	15.648909
28.028770	1556.438018	15.653927
27.612540	1565.675693	15.658944
27.910774	1581.810026	15.663962
28.239258	1595.196031	15.668979
28.205683	1594.597332	15.673997
28.382563	1595.184236	15.679015
28.329549	1605.574523	15.684032
28.332819	1594.696686	15.689050
28.346492	1580.365775	15.694067
27.936662	1582.366884	15.699085
28.358488	1582.349186	15.704103
28.138294	1596.152267	15.709120
28.511458	1599.699155	15.714138
28.380345	1597.935385	15.719155
28.289418	1596.834569	15.724173
28.660686	1597.098657	15.729191
28.417486	1603.905032	15.734208
28.636364	1590.099056	15.739226
28.502882	1593.155703	15.744243
28.371104	1591.169444	15.749261
28.740425	1589.461151	15.754279
28.490537	1589.165955	15.759296
28.598926	1593.817711	15.764314
28.544375	1596.687940	15.769331
28.564308	1596.261617	15.774349
28.697453	1590.485148	15.779367
28.283424	1596.384332	15.784384
28.783063	1594.183318	15.789402
28.884510	1589.657030	15.794419
28.527011	1596.072620	15.799437
28.496630	1591.866248	15.804455
28.471712	1600.309249	15.809472
28.456302	1599.269538	15.814490
28.566812	1597.013388	15.819507
28.662701	1595.984243	15.824525
28.945537	1594.829323	15.829543
28.715169	1617.891860	15.834560
29.238899	1608.733803	15.839578
29.051933	1611.581107	15.844595
28.802080	1610.002238	15.849613
29.032828	1620.064904	15.854631
28.960930	1615.980771	15.859648
28.895019	1611.443412	15.864666
29.265579	1616.478106	15.869683
29.021339	1619.933118	15.874701
29.166145	1618.648404	15.879719
28.760174	1619.723120	15.884736
29.228217	1618.618889	15.889754
29.215256	1617.560696	15.894771
29.094729	1619.452745	15.899789
29.245089	1619.600259	15.904807
28.965121	1631.643144	15.909824
29.122032	1615.709938	15.914842
29.117283	1626.829551	15.919859
29.074651	1625.180662	15.924877
29.357516	1638.756465	15.929895
29.273132	1652.360177	15.934912
29.561913	1644.662462	15.939930
29.520428	1640.044115	15.944947
29.588559	1647.836760	15.949965
29.858130	1633.547574	15.954983
29.629453	1649.120250	15.960000
29.665867	1644.650724	15.965018
29.946985	1641.178074	15.970035
29.732966	1637.004124	15.975053
29.617780	1611.106892	15.980071
29.421037	1618.918955	15.985088
29.667089	1627.953510	15.990106
29.935225	1640.458007	15.995123
29.956102	1634.909439	16.000141
29.828579	1633.859290	16.005159
29.798810	1642.265333	16.010176
29.934704	1649.560290	16.015194
30.215142	1638.502926	16.020211
29.678444	1614.832814	16.025229
30.180440	1616.453321	16.030247
29.931488	1622.121682	16.035264
29.920955	1605.076252	16.040282
29.940242	1609.321414	16.045299
30.048670	1637.304945	16.050317
30.245001	1640.429345	16.055335
30.114541	1632.750520	16.060352
30.164217	1629.114212	16.065370
30.157103	1629.044580	16.070387
29.956860	1640.927671	16.075405
29.715961	1640.550024	16.080423
30.016888	1639.071298	16.085440
30.323713	1631.118225	16.090458
30.057726	1637.977804	16.095475
29.944072	1642.996132	16.100493
30.400417	1641.157543	16.105511
30.241793	1639.220392	16.110528
30.604805	1640.923634	16.115546
30.407422	1643.549221	16.120563
29.990041	1648.364291	16.125581
30.658886	1639.692764	16.130599
30.281664	1646.442664	16.135616
30.579694	1641.967596	16.140634
30.519876	1641.738833	16.145651
30.403569	1648.314192	16.150669
30.729446	1658.273618	16.155687
30.431901	1667.400400	16.160704
30.648675	1666.633560	16.165722
30.512797	1672.087266	16.170739
30.927730	1670.215163	16.175757
31.160221	1666.563848	16.180775
30.610900	1657.089229	16.185792
30.591337	1666.035600	16.190810
31.007925	1667.811316	16.195827
30.621576	1673.614875	16.200845
30.857483	1666.018396	16.205863
30.896856	1674.299379	16.210880
31.020615	1666.744383	16.215898
30.847534	1675.631081	16.220915
31.002434	1673.826407	16.225933
31.093895	1667.199988	16.230951
30.921990	1664.456364	16.235968
30.791411	1670.497574	16.240986
31.125094	1668.632137	16.246003
30.982614	1670.546571	16.251021
31.193874	1662.132852	16.256039
30.962966	1670.004665	16.261056
30.935810	1669.527643	16.266074
31.290110	1670.892482	16.271091
31.168035	1671.435041	16.276109
31.194032	1663.052442	16.281127
30.889044	1662.526130	16.286144
31.053405	1667.314497	16.291162
31.268388	1671.725107	16.296179
31.154132	1689.964907	16.301197
31.553011	1690.261563	16.306215
31.230650	1698.822849	16.311232
31.447377	1699.361715	16.316250
31.785383	1686.023533	16.321267
31.209325	1694.899002	16.326285
31.305793	1700.381733	16.331303
31.523071	1696.391467	16.336320
31.554785	1703.966566	16.341338
31.748210	1697.957843	16.346355
31.696128	1698.315409	16.351373
31.517993	1697.624923	16.356391
31.399810	1699.655830	16.361408
31.731777	1697.930672	16.366426
31.852749	1697.061912	16.371443
31.769639	1696.423129	16.376461
31.502619	1685.146282	16.381479
31.946939	1692.919069	16.386496
31.906467	1695.381991	16.391514
32.121804	1695.565551	16.396531
31.768663	1696.598024	16.401549
31.664317	1698.590543	16.406567
31.909837	1708.437755	16.411584
32.267537	1720.658245	16.416602
32.489602	1721.727979	16.421619
32.293763	1717.084672	16.426637
32.037690	1694.144442	16.431655
31.714279	1694.447746	16.436672
32.013919	1714.621803	16.441690
32.223003	1719.355074	16.446707
32.236106	1729.278696	16.451725
32.548754	1723.589958	16.456743
32.607558	1725.819960	16.461760
32.279529	1728.194246	16.466778
32.914805	1723.623680	16.471795
32.355188	1705.117741	16.476813
32.366467	1695.645717	16.481831
32.249115	1701.341100	16.486848
32.332741	1710.278907	16.491866
32.510451	1712.076996	16.496883
32.358313	1723.699207	16.501901
32.629092	1722.359784	16.506919
32.598974	1721.445115	16.511936
32.275687	1722.789815	16.516954
32.773491	1725.852781	16.521971
32.225548	1727.820876	16.526989
32.918202	1716.331958	16.532007
32.898494	1715.647667	16.537024
32.448573	1718.050830	16.542042
32.649058	1711.194630	16.547059
32.735473	1728.217905	16.552077
32.450992	1731.084717	16.557095
32.681627	1722.863729	16.562112
32.473959	1729.986201	16.567130
32.953851	1718.335358	16.572147
32.821364	1735.881226	16.577165
33.173741	1742.630434	16.582183
32.892044	1736.353741	16.587200
33.216579	1744.663222	16.592218
33.139244	1729.117274	16.597235
32.919238	1738.931778	16.602253
33.193580	1740.811994	16.607271
33.467805	1750.256653	16.612288
33.322697	1740.146465	16.617306
33.332845	1717.615229	16.622323
33.312140	1711.056232	16.627341
33.110072	1715.848783	16.632359
33.610455	1711.317038	16.637376
33.505961	1714.761584	16.642394
33.251640	1706.397709	16.647411
33.405282	1710.196728	16.652429
33.281039	1717.714117	16.657447
33.385479	1724.660960	16.662464
33.427384	1743.879581	16.667482
33.870977	1740.452574	16.672499
33.642067	1735.441702	16.677517
33.549879	1722.703030	16.682535
33.550537	1717.014499	16.687552
33.737996	1737.282775	16.692570
33.926521	1737.470612	16.697587
33.629587	1728.425274	16.702605
33.640074	1728.771289	16.707623
33.795943	1737.813216	16.712640
33.730608	1748.402212	16.717658
34.022330	1742.417909	16.722675
33.959875	1752.337866	16.727693
33.658855	1751.944634	16.732711
33.710562	1745.233278	16.737728
33.771323	1745.729375	16.742746
33.860492	1747.502261	16.747763
33.553326	1750.268080	16.752781
33.972100	1737.665783	16.757799
33.623500	1736.734262	16.762816
33.679888	1747.549253	16.767834
34.039683	1740.600774	16.772851
34.124037	1754.592190	16.777869
33.976985	1764.660937	16.782887
34.452467	1769.547594	16.787904
34.266688	1777.971518	16.792922
34.284820	1763.040350	16.797939
34.050598	1763.614170	16.802957
34.070039	1773.783007	16.807975
34.266539	1776.661214	16.812992
34.110844	1783.821044	16.818010
34.484693	1778.968875	16.823027
34.189910	1780.205206	16.828045
34.300266	1779.420725	16.833063
34.486433	1772.103491	16.838080
33.906085	1778.842585	16.843098
34.006254	1770.102791	16.848115
34.463853	1798.392766	16.853133
34.349840	1802.718237	16.858151
34.606717	1802.752017	16.863168
34.494149	1819.661619	16.868186
35.166421	1809.524850	16.873203
35.014794	1805.594962	16.878221
34.859567	1813.275443	16.883239
35.147808	1797.796969	16.888256
35.139319	1799.811182	16.893274
34.974285	1803.884435	16.898291
35.365064	1806.623903	16.903309
35.014875	1787.165743	16.908327
35.359273	1771.543051	16.913344
35.001364	1778.554218	16.918362
35.123757	1761.996315	16.923379
34.802856	1758.485148	16.928397
34.851973	1772.931333	16.933415
35.009496	1777.008195	16.938432
34.956839	1790.546410	16.943450
35.274674	1797.935916	16.948467
35.354457	1795.465969	16.953485
35.243769	1792.290170	16.958503
35.475823	1786.850233	16.963520
35.526181	1800.648114	16.968538
35.452291	1793.422685	16.973555
35.474786	1800.195429	16.978573
35.162381	1805.968368	16.983591
35.530872	1798.159539	16.988608
35.422024	1799.583312	16.993626
35.487105	1802.153696	16.998643
35.476531	1799.940423	17.003661
35.664807	1798.047821	17.008679
35.963961	1791.888480	17.013696
35.492527	1799.788497	17.018714
35.799037	1796.024663	17.023731
35.611209	1794.008773	17.028749
35.324501	1796.547952	17.033767
36.057686	1791.378902	17.038784
35.960624	1792.177830	17.043802
36.155234	1800.386146	17.048819
35.907478	1796.839707	17.053837
36.106962	1795.200953	17.058855
36.420483	1793.127916	17.063872
36.063053	1794.484359	17.068890
36.198320	1791.660260	17.073907
35.760032	1789.962760	17.078925
35.625418	1798.417077	17.083943
35.912397	1787.315297	17.088960
35.811016	1794.658394	17.093978
35.949618	1797.859680	17.098995
35.922815	1799.308910	17.104013
35.891095	1795.896343	17.109031
35.975880	1796.925839	17.114048
35.800511	1809.270749	17.119066
36.093320	1811.494907	17.124083
36.395211	1814.731507	17.129101
36.282354	1828.383185	17.134119
36.251920	1823.022067	17.139136
36.181539	1828.945194	17.144154
36.435620	1820.909189	17.149171
36.518782	1821.938158	17.154189
36.491245	1822.036176	17.159207
36.626725	1815.195015	17.164224
36.267393	1825.588690	17.169242
36.581832	1825.818586	17.174259
36.785390	1824.164235	17.179277
36.543470	1830.239785	17.184295
36.710566	1821.045659	17.189312
36.580869	1829.434711	17.194330
36.790248	1839.887932	17.199347
36.609273	1844.721208	17.204365
36.342466	1856.498676	17.209383
36.831975	1849.992751	17.214400
37.137704	1865.883153	17.219418
37.137622	1862.545755	17.224435
37.153102	1846.710365	17.229453
36.849554	1855.061086	17.234471
37.258146	1849.284634	17.239488
37.447225	1857.259466	17.244506
37.353926	1842.507236	17.249523
37.482037	1846.832647	17.254541
37.223232	1848.944994	17.259559
37.643681	1841.209660	17.264576
37.352400	1844.514912	17.269594
37.437628	1847.337728	17.274611
37.582665	1851.870455	17.279629
37.120596	1855.420829	17.284647
37.669905	1843.258556	17.289664
37.511161	1846.415246	17.294682
37.474512	1846.776646	17.299699
37.442906	1849.346728	17.304717
37.372183	1848.400771	17.309735
37.793236	1854.523193	17.314752
37.396484	1845.282900	17.319770
37.578868	1849.859225	17.324787
37.617136	1848.738571	17.329805
37.641730	1854.793651	17.334823
37.917821	1846.653440	17.339840
37.663825	1856.249271	17.344858
37.495441	1854.314434	17.349875
37.766042	1853.260555	17.354893
37.503624	1854.689160	17.359911
38.033184	1847.831542	17.364928
37.540960	1852.749856	17.369946
37.615054	1857.669882	17.374963
37.984942	1867.451747	17.379981
37.804841	1885.731396	17.384999
38.008736	1878.644894	17.390016
37.555847	1891.675192	17.395034
38.059501	1883.442822	17.400051
38.016356	1880.104422	17.405069
37.537417	1889.516694	17.410087
38.116758	1881.097635	17.415104
38.327670	1907.698273	17.420122
38.215347	1919.307211	17.425139
38.613439	1912.210173	17.430157
38.306433	1918.410980	17.435175
38.625804	1911.174688	17.440192
38.279385	1914.305476	17.445210
38.363043	1912.121993	17.450227
38.851699	1911.845081	17.455245
38.633708	1919.821941	17.460263
38.754769	1912.672336	17.465280
38.741249	1908.766802	17.470298
38.740904	1918.138947	17.475315
38.858487	1912.566984	17.480333
38.536781	1916.416696	17.485351
38.949096	1908.699929	17.490368
38.752445	1920.045441	17.495386
38.627164	1914.354108	17.500403
39.075546	1907.391422	17.505421
38.494547	1913.855379	17.510439
38.791363	1907.554780	17.515456
38.827539	1909.605147	17.520474
38.536035	1913.243171	17.525491
38.856882	1905.002975	17.530509
38.905056	1908.571094	17.535527
39.447391	1925.452670	17.540544
39.170517	1927.851078	17.545562
39.152672	1942.809947	17.550579
39.187243	1933.749367	17.555597
39.053088	1937.809867	17.560615
39.430168	1934.240041	17.565632
39.447765	1936.123473	17.570650
39.638754	1941.208158	17.575667
39.439970	1926.238266	17.580685
39.508492	1934.677570	17.585703
39.586358	1938.808871	17.590720
39.810633	1932.854912	17.595738
39.749983	1932.648300	17.600755
39.769447	1918.161965	17.605773
39.948094	1923.481438	17.610791
39.948364	1913.454918	17.615808
39.892237	1906.395714	17.620826
39.478096	1896.408553	17.625843
39.817323	1902.179861	17.630861
40.130925	1902.458660	17.635879
39.890156	1893.239867	17.640896
39.983723	1895.740440	17.645914
39.604034	1896.339036	17.650931
40.067266	1892.732670	17.655949
40.122798	1909.775242	17.660967
40.309307	1901.952119	17.665984
40.228823	1898.556744	17.671002
39.932294	1890.108252	17.676019
40.132236	1889.014512	17.681037
40.154715	1895.813260	17.686055
40.597044	1899.260309	17.691072
40.182110	1901.550160	17.696090
40.464804	1893.262567	17.701107
40.438096	1881.023014	17.706125
40.123872	1898.152859	17.711143
40.391022	1903.565971	17.716160
40.360107	1906.320011	17.721178
40.141425	1914.108987	17.726195
40.464795	1916.825404	17.731213
40.544443	1919.487876	17.736231
40.367710	1917.885511	17.741248
40.681960	1922.108893	17.746266
40.538327	1920.831612	17.751283
40.626818	1913.787882	17.756301
40.276122	1924.623880	17.761319
40.095677	1918.798185	17.766336
40.576913	1931.003872	17.771354
40.771374	1946.835811	17.776371
40.860074	1944.399813	17.781389
40.815804	1956.307839	17.786407
40.845708	1950.625565	17.791424
41.012647	1951.527129	17.796442
40.524755	1956.020819	17.801459
40.740707	1946.676453	17.806477
40.604286	1957.862152	17.811495
41.049126	1966.124257	17.816512
41.285789	1980.799523	17.821530
41.407104	1992.965913	17.826547
41.427334	1987.168754	17.831565
41.419166	1983.771265	17.836583
41.359915	1982.675592	17.841600
41.359440	1986.088667	17.846618
40.939329	1983.910003	17.851635
41.247450	1981.417768	17.856653
41.249317	1978.819418	17.861671
41.463067	1981.430624	17.866688
41.495692	1982.706786	17.871706
41.438894	1986.511121	17.876723
41.434751	1979.477414	17.881741
41.470986	1983.901682	17.886759
41.764952	1975.773495	17.891776
41.620796	1982.672011	17.896794
41.368510	1993.361005	17.901811
42.096917	1997.943899	17.906829
41.880075	2010.327843	17.911847
41.799415	2015.816918	17.916864
41.956419	2010.842726	17.921882
41.961286	2009.855600	17.926899
42.173190	2007.879758	17.931917
41.990042	2013.532268	17.936935
42.056621	2011.375091	17.941952
42.356355	2010.513987	17.946970
42.152819	2010.124077	17.951987
42.301081	2009.778744	17.957005
42.245443	2014.288466	17.962023
42.205136	2009.110555	17.967040
42.566986	2000.313158	17.972058
42.470386	2009.024252	17.977075
42.499456	2003.375128	17.982093
42.651520	2007.117842	17.987111
42.693478	2001.640497	17.992128
42.851295	1997.897967	17.997146
42.843975	1987.060068	18.002163
42.607978	1964.447360	18.007181
42.693973	1973.500578	18.012199
42.416127	1967.513417	18.017216
42.899484	1974.056214	18.022234
42.701106	1992.934353	18.027251
43.296327	1986.341503	18.032269
42.763932	1974.536481	18.037287
42.816936	1972.018861	18.042304
42.834429	1966.675217	18.047322
42.687756	1994.622248	18.052339
42.934125	1992.133566	18.057357
42.795041	1996.270380	18.062375
42.806442	2005.081448	18.067392
43.141640	2003.427320	18.072410
42.954150	1999.653336	18.077427
42.794336	1997.034360	18.082445
43.135571	2002.238263	18.087463
42.951664	1994.265722	18.092480
43.200565	2002.714840	18.097498
43.162021	2015.795582	18.102515
43.567220	2010.264237	18.107533
43.625157	2016.277883	18.112551
43.497293	2024.342682	18.117568
43.670869	2017.655027	18.122586
43.860099	2022.952398	18.127603
43.804920	2016.916334	18.132621
43.524709	1997.272896	18.137639
43.516853	2009.407986	18.142656
43.751769	2009.501118	18.147674
43.567519	2020.513579	18.152691
44.045102	2011.188800	18.157709
43.797788	2019.263207	18.162727
43.760682	2020.315304	18.167744
44.081698	2013.067688	18.172762
44.069423	2015.892715	18.177779
43.982151	2010.468226	18.182797
43.953452	2017.249236	18.187815
44.152321	2015.329746	18.192832
43.823581	2015.043181	18.197850
44.235291	2020.579588	18.202867
44.008550	2014.717976	18.207885
44.198186	2015.706381	18.212903
43.888237	2015.265796	18.217920
43.982836	2010.052210	18.222938
43.924800	2014.499388	18.227955
44.160183	2008.962876	18.232973
44.399746	2026.640110	18.237991
44.539509	2039.177224	18.243008
44.677881	2035.353622	18.248026
44.340227	2052.265566	18.253043
44.523610	2040.568940	18.258061
44.874094	2040.384856	18.263079
44.850710	2039.111984	18.268096
44.949003	2039.382649	18.273114
44.973300	2038.504117	18.278131
44.852317	2033.678080	18.283149
45.105641	2034.200898	18.288167
44.928434	2014.842271	18.293184
45.195989	1995.034392	18.298202
45.095604	2004.551547	18.303219
44.845900	1999.007450	18.308237
45.237704	2006.393133	18.313255
45.081484	2009.404724	18.318272
45.156748	1992.859582	18.323290
44.836031	2007.500273	18.328307
45.247335	2028.430169	18.333325
44.999722	2027.102601	18.338343
45.212885	2033.074981	18.343360
45.385590	2027.709707	18.348378
45.328051	2035.097060	18.353395
45.459167	2029.957875	18.358413
45.626205	2031.949634	18.363431
45.210521	2027.965047	18.368448
45.205705	2031.800433	18.373466
45.473341	2032.799998	18.378483
45.287351	2029.210614	18.383501
45.711826	2030.185953	18.388519
45.382201	2047.241342	18.393536
45.530027	2051.254542	18.398554
45.646283	2060.013525	18.403571
46.091112	2058.468548	18.408589
46.180130	2064.175209	18.413607
45.974597	2066.802170	18.418624
45.929126	2059.598033	18.423642
46.045661	2059.314393	18.428659
46.108620	2055.258971	18.433677
45.828110	2061.915764	18.438695
45.663723	2060.064427	18.443712
46.285416	2054.009283	18.448730
46.171309	2060.925854	18.453747
45.996281	2057.960836	18.458765
46.373025	2061.083300	18.463783
46.015795	2063.329362	18.468800
45.982039	2058.072516	18.473818
46.012744	2088.112857	18.478835
46.610834	2087.044491	18.483853
46.617512	2093.163094	18.488871
46.341198	2092.229457	18.493888
46.601477	2092.067625	18.498906
46.428984	2092.647342	18.503923
46.397728	2093.453097	18.508941
46.527091	2089.740252	18.513959
46.508967	2090.347266	18.518976
46.850559	2082.713266	18.523994
46.595995	2086.988869	18.529011
46.671491	2097.178883	18.534029
47.092956	2106.416233	18.539047
46.696931	2118.193281	18.544064
47.071021	2113.028689	18.549082
46.960187	2107.597696	18.554099
47.151484	2118.388302	18.559117
47.420076	2113.021077	18.564135
47.397554	2117.828386	18.569152
47.276941	2117.363894	18.574170
47.178238	2125.561751	18.579187
47.417447	2122.854732	18.584205
47.494900	2112.844869	18.589223
47.209451	2117.130126	18.594240
47.156145	2113.178968	18.599258
47.285965	2110.005645	18.604275
47.271394	2105.228687	18.609293
47.588281	2104.250788	18.614311
46.890831	2111.044889	18.619328
47.703332	2123.687167	18.624346
47.519967	2144.431254	18.629363
47.865726	2140.337001	18.634381
48.207553	2131.120321	18.639399
47.734885	2145.750773	18.644416
48.037991	2133.644832	18.649434
47.993711	2129.559296	18.654451
47.915121	2136.830496	18.659469
48.362461	2131.492179	18.664487
48.201781	2143.717827	18.669504
47.875994	2138.944082	18.674522
47.975706	2141.991970	18.679539
48.062409	2138.897096	18.684557
48.469887	2126.241995	18.689575
48.195259	2138.752464	18.694592
48.217216	2134.033385	18.699610
48.353363	2132.355927	18.704627
48.643106	2133.111277	18.709645
48.755796	2133.732827	18.714663
48.385004	2133.125744	18.719680
48.373029	2126.877444	18.724698
48.653943	2142.241160	18.729715
48.717786	2151.621310	18.734733
49.347429	2137.237241	18.739751
48.831956	2135.459189	18.744768
49.137682	2119.386860	18.749786
49.151078	2115.327526	18.754803
48.824011	2124.799892	18.759821
48.931988	2112.865099	18.764839
48.914220	2108.006845	18.769856
48.784267	2113.072767	18.774874
49.017271	2108.691308	18.779891
48.944211	2112.507709	18.784909
49.442904	2122.936233	18.789927
49.463258	2124.340218	18.794944
49.224521	2116.939551	18.799962
49.616763	2113.832139	18.804979
49.313733	2109.044548	18.809997
49.399151	2112.822303	18.815015
49.573081	2110.533936	18.820032
49.729414	2110.284065	18.825050
49.566757	2111.960291	18.830067
49.590385	2110.866336	18.835085
49.964534	2111.780488	18.840103
49.519600	2115.159071	18.845120
49.375148	2115.108193	18.850138
49.507673	2126.306978	18.855155
49.739846	2134.265651	18.860173
50.107397	2140.254356	18.865191
49.864232	2145.718268	18.870208
50.163039	2143.825300	18.875226
50.166008	2142.020414	18.880243
50.033474	2146.071273	18.885261
50.125657	2137.138246	18.890279
50.209006	2139.126847	18.895296
50.278509	2148.550929	18.900314
50.061064	2145.824701	18.905331
49.709516	2152.988415	18.910349
50.165375	2145.832499	18.915367
49.663311	2147.126299	18.920384
50.118605	2155.599227	18.925402
50.173247	2166.610669	18.930419
50.126319	2178.848882	18.935437
50.554183	2173.481406	18.940455
50.387156	2178.084455	18.945472
50.173655	2173.074119	18.950490
50.408737	2180.322848	18.955507
50.433498	2194.746591	18.960525
50.781958	2198.883581	18.965543
50.885637	2203.312106	18.970560
51.184398	2197.799239	18.975578
51.292608	2202.750912	18.980595
51.003002	2196.086701	18.985613
51.664686	2193.500290	18.990631
51.246468	2177.320744	18.995648
51.305286	2166.000996	19.000666
51.305121	2156.632755	19.005683
51.365669	2166.083447	19.010701
51.539500	2157.792616	19.015719
51.227084	2161.063551	19.020736
51.326020	2159.135596	19.025754
51.428575	2160.343200	19.030771
51.386173	2164.491385	19.035789
51.395651	2155.287577	19.040807
51.416579	2155.821505	19.045824
51.518224	2163.332203	19.050842
51.514790	2168.766543	19.055859
51.394618	2181.172184	19.060877
51.689693	2178.783468	19.065895
51.818364	2188.438836	19.070912
51.816196	2189.491666	19.075930
51.837899	2182.696009	19.080947
51.730983	2181.171365	19.085965
52.165813	2175.107431	19.090983
52.225825	2179.214117	19.096000
52.169451	2182.371071	19.101018
52.279239	2182.469215	19.106035
52.138553	2182.863734	19.111053
52.140624	2176.263926	19.116071
52.024079	2183.171504	19.121088
52.075525	2175.633284	19.126106
52.204334	2177.692514	19.131123
52.027072	2191.643481	19.136141
52.545311	2202.024897	19.141159
52.594800	2210.995200	19.146176
52.568793	2218.619101	19.151194
52.447797	2218.728880	19.156211
52.458909	2214.435479	19.161229
52.698656	2214.621448	19.166247
52.521534	2219.739765	19.171264
52.344324	2216.374686	19.176282
52.621053	2215.931776	19.181299
52.576051	2224.018080	19.186317
53.000817	2228.282137	19.191335
52.896549	2235.057207	19.196352
52.860820	2245.099091	19.201370
53.535211	2238.047507	19.206387
53.087091	2246.236655	19.211405
53.365189	2244.951869	19.216423
53.405399	2253.207090	19.221440
53.235251	2250.220802	19.226458
53.521301	2247.970382	19.231475
52.988622	2252.538162	19.236493
53.157647	2252.763728	19.241511
53.120391	2254.038472	19.246528
52.962058	2255.313648	19.251546
53.400885	2264.130648	19.256563
53.563176	2283.178182	19.261581
53.716415	2274.080375	19.266599
53.848816	2283.012329	19.271616
53.667920	2283.997704	19.276634
53.716118	2281.380900	19.281651
53.542692	2279.667056	19.286669
53.634054	2273.211857	19.291687
53.892931	2277.658917	19.296704
54.284934	2271.240726	19.301722
54.079975	2275.440824	19.306739
53.955613	2281.878525	19.311757
54.207440	2277.308377	19.316775
54.071470	2282.866154	19.321792
54.182604	2292.008380	19.326810
54.651244	2293.828581	19.331827
54.846201	2304.016994	19.336845
54.768197	2288.232216	19.341863
54.869238	2273.269213	19.346880
54.530845	2267.868944	19.351898
54.337229	2261.039155	19.356915
54.495514	2272.615443	19.361933
54.575480	2284.658884	19.366951
54.325540	2292.987930	19.371968
54.755919	2296.143583	19.376986
55.102684	2296.708932	19.382003
54.637670	2299.706113	19.387021
54.723737	2300.043234	19.392039
54.838969	2293.128779	19.397056
54.606969	2300.130338	19.402074
54.806778	2305.429273	19.407091
54.757061	2321.890510	19.412109
54.934860	2329.755704	19.417127
55.295624	2326.350428	19.422144
55.453146	2330.465991	19.427162
55.484941	2324.385251	19.432179
55.407283	2333.930459	19.437197
55.473794	2324.500347	19.442215
55.770032	2328.982368	19.447232
55.413519	2336.257873	19.452250
55.445983	2335.320599	19.457267
55.862875	2330.597469	19.462285
55.808228	2328.671960	19.467303
55.867865	2324.731050	19.472320
55.503373	2326.859532	19.477338
56.038401	2336.448621	19.482355
55.786045	2363.209712	19.487373
55.724234	2364.751107	19.492391
55.952984	2364.369333	19.497408
55.738412	2362.200306	19.502426
55.903539	2358.487984	19.507443
56.011799	2363.368909	19.512461
55.795420	2363.937543	19.517479
56.296686	2370.508343	19.522496
56.080332	2384.581358	19.527514
56.787615	2389.281023	19.532531
56.699666	2393.488453	19.537549
56.610961	2385.295997	19.542567
56.910301	2385.082311	19.547584
56.721444	2385.810956	19.552602
56.832942	2385.787693	19.557619
56.885208	2386.859388	19.562637
56.938405	2372.976839	19.567655
56.734865	2360.245140	19.572672
56.797761	2372.298454	19.577690
57.250712	2379.435452	19.582707
57.124974	2381.798030	19.587725
57.019034	2381.250955	19.592743
56.983224	2381.565038	19.597760
56.920837	2377.821346	19.602778
57.304632	2377.697237	19.607795
56.948623	2379.279257	19.612813
57.182377	2378.707114	19.617831
57.103210	2383.150694	19.622848
57.363193	2389.626260	19.627866
57.637595	2379.179706	19.632883
57.211548	2387.146736	19.637901
57.058994	2385.814986	19.642919
57.471152	2390.734769	19.647936
57.462925	2399.737991	19.652954
57.449023	2397.640002	19.657971
57.282045	2407.079938	19.662989
57.499226	2406.994198	19.668007
57.694473	2413.054545	19.673024
57.356877	2427.367972	19.678042
57.677689	2431.561355	19.683059
57.729088	2433.946035	19.688077
57.949615	2432.486349	19.693095
57.971700	2426.343400	19.698112
58.258107	2443.267183	19.703130
58.443577	2459.218318	19.708147
58.463756	2457.194333	19.713165
58.715310	2465.363267	19.718183
58.741804	2455.002605	19.723200
58.371695	2450.854882	19.728218
58.673402	2447.060975	19.733235
58.752130	2453.596939	19.738253
59.014455	2451.603559	19.743271
58.892341	2454.627893	19.748288
58.717249	2464.046349	19.753306
59.192159	2451.465955	19.758323
59.037092	2463.788513	19.763341
58.842739	2460.526010	19.768359
58.967913	2459.484270	19.773376
58.790402	2459.024907	19.778394
59.130353	2453.923851	19.783411
58.954869	2449.161430	19.788429
58.984745	2459.532813	19.793447
59.101485	2450.338458	19.798464
59.058788	2453.700167	19.803482
59.127979	2464.835371	19.808499
59.309347	2487.003745	19.813517
59.331339	2492.084110	19.818535
59.577280	2484.133996	19.823552
59.255451	2491.788697	19.828570
59.662395	2481.224968	19.833587
59.561556	2487.721149	19.838605
59.869341	2483.341027	19.843623
59.729792	2475.842551	19.848640
59.921056	2478.094022	19.853658
60.065865	2478.085112	19.858675
60.235275	2480.203985	19.863693
60.242741	2476.511270	19.868711
60.718217	2469.237225	19.873728
60.014911	2479.875001	19.878746
60.145295	2472.173011	19.883763
60.197115	2477.615961	19.888781
60.344514	2469.989133	19.893799
60.533470	2469.582239	19.898816
60.337714	2477.062652	19.903834
60.795369	2469.701776	19.908851
60.537808	2469.860866	19.913869
60.446193	2475.924510	19.918887
60.907042	2489.582852	19.923904
60.679759	2499.272380	19.928922
61.050980	2497.283654	19.933939
60.986171	2492.281745	19.938957
61.044103	2494.622130	19.943975
61.402141	2492.907673	19.948992
61.133555	2504.844052	19.954010
61.026941	2486.844598	19.959027
61.215625	2499.161923	19.964045
61.362991	2496.513534	19.969063
61.477944	2482.641484	19.974080
61.196562	2484.413772	19.979098
61.155864	2485.976197	19.984115
61.216229	2483.398320	19.989133
61.474992	2483.116376	19.994151
61.308661	2487.874373	19.999168
61.308663	2489.333555	20.004186
61.605760	2483.915241	20.009203
61.545322	2499.379396	20.014221
61.451807	2512.014688	20.019239
61.647332	2511.506846	20.024256
61.552040	2526.833425	20.029274
61.614296	2516.466229	20.034291
61.883078	2521.936737	20.039309
61.719358	2521.507424	20.044327
62.070194	2536.864340	20.049344
62.218530	2547.522099	20.054362
62.306240	2549.071919	20.059379
62.449016	2554.609731	20.064397
62.482587	2550.765738	20.069415
62.180323	2549.698550	20.074432
62.193429	2554.698547	20.079450
62.085421	2551.121768	20.084467
62.599741	2540.411868	20.089485
62.311479	2543.985813	20.094503
62.672239	2560.316570	20.099520
62.673560	2579.479835	20.104538
62.957092	2578.611060	20.109555
63.171787	2574.918310	20.114573
63.460584	2583.312636	20.119591
63.648493	2563.566249	20.124608
63.153859	2547.367799	20.129626
63.330666	2543.210705	20.134643
63.268724	2535.094918	20.139661
63.057278	2541.714954	20.144679
63.254946	2550.276396	20.149696
63.536121	2562.833101	20.154714
63.597004	2561.934544	20.159731
63.517746	2559.121698	20.164749
63.384183	2573.331934	20.169767
63.700314	2562.475064	20.174784
63.707175	2573.244290	20.179802
63.566554	2574.751078	20.184819
63.804056	2567.286818	20.189837
63.687299	2570.807461	20.194855
64.044726	2578.649650	20.199872
63.830575	2573.360030	20.204890
64.050893	2567.307335	20.209907
64.087400	2565.170604	20.214925
63.941442	2571.070686	20.219943
63.645886	2559.833891	20.224960
63.849078	2583.422700	20.229978
63.924925	2584.478063	20.234995
64.506871	2591.984755	20.240013
64.355105	2588.214359	20.245031
64.448107	2591.597722	20.250048
64.712815	2590.936468	20.255066
65.003284	2582.026611	20.260083
64.933647	2580.644649	20.265101
64.472102	2593.107438	20.270119
64.809547	2578.281838	20.275136
64.924851	2592.203048	20.280154
65.298320	2607.758591	20.285171
65.381128	2597.037230	20.290189
65.209843	2584.667540	20.295207
65.200910	2579.964256	20.300224
65.617919	2578.805174	20.305242
65.531238	2574.925288	20.310259
65.727902	2580.087954	20.315277
65.533952	2573.737905	20.320295
65.722358	2568.018316	20.325312
65.438102	2569.207405	20.330330
65.719142	2572.123421	20.335347
65.747763	2569.623746	20.340365
65.673522	2570.290858	20.345383
65.653266	2565.504430	20.350400
65.616275	2574.992180	20.355418
66.023758	2589.499231	20.360435
66.065179	2593.463475	20.365453
66.064514	2603.322239	20.370471
66.147228	2603.825092	20.375488
66.470880	2601.284655	20.380506
66.558004	2601.263706	20.385523
66.616854	2587.439835	20.390541
66.472201	2569.194629	20.395559
66.367613	2562.893262	20.400576
66.161933	2566.927583	20.405594
66.357381	2585.016851	20.410611
66.408230	2587.009124	20.415629
66.660142	2598.353636	20.420647
66.678422	2594.283165	20.425664
66.538034	2594.202530	20.430682
66.718152	2597.347818	20.435699
66.644769	2595.483471	20.440717
66.775525	2603.233603	20.445735
66.780007	2591.748349	20.450752
66.596056	2598.566973	20.455770
66.843203	2614.668126	20.460787
67.097422	2627.443931	20.465805
66.776359	2631.447899	20.470823
67.392323	2630.529255	20.475840
67.087864	2629.076183	20.480858
66.920113	2628.587725	20.485875
67.201307	2652.207470	20.490893
67.388671	2665.309403	20.495911
67.632547	2659.279658	20.500928
67.935660	2666.931543	20.505946
67.588450	2666.219985	20.510963
68.169827	2663.532246	20.515981
67.907120	2667.771556	20.520999
68.143244	2653.787200	20.526016
67.985215	2658.267038	20.531034
68.012982	2658.293312	20.536051
68.073503	2655.484902	20.541069
67.735833	2661.251189	20.546087
68.118150	2673.263253	20.551104
68.191617	2675.465891	20.556122
68.125955	2692.684455	20.561139
68.362615	2680.351888	20.566157
68.508215	2682.853739	20.571175
68.655436	2684.128993	20.576192
68.752044	2682.055031	20.581210
68.595971	2686.033489	20.586227
68.760776	2696.377230	20.591245
68.573498	2707.002098	20.596263
69.071077	2709.380961	20.601280
69.133584	2708.489216	20.606298
68.911045	2707.275576	20.611315
69.510989	2699.859645	20.616333
69.338100	2702.226647	20.621351
69.311180	2703.841961	20.626368
69.298340	2705.058574	20.631386
69.298035	2711.907746	20.636403
69.743451	2698.511402	20.641421
69.551592	2697.603585	20.646439
69.433568	2700.573827	20.651456
69.417232	2703.393341	20.656474
69.607662	2705.697685	20.661491
70.000952	2709.712042	20.666509
69.742187	2720.286177	20.671527
69.748716	2734.021134	20.676544
70.302165	2730.563801	20.681562
70.119441	2731.822453	20.686579
70.376642	2729.007836	20.691597
70.438792	2738.507414	20.696615
70.374000	2734.705017	20.701632
70.293136	2719.543232	20.706650
70.514104	2727.297137	20.711667
70.765965	2722.723702	20.716685
70.445816	2729.023696	20.721703
70.501278	2720.336089	20.726720
70.403259	2727.473022	20.731738
70.536810	2728.530993	20.736755
70.808791	2719.330593	20.741773
70.656919	2724.328638	20.746791
70.745610	2723.168413	20.751808
70.922791	2725.847731	20.756826
71.017964	2756.733437	20.761843
71.322571	2753.514798	20.766861
71.158078	2757.931980	20.771879
71.198596	2755.878751	20.776896
71.718282	2755.563061	20.781914
71.567163	2760.649887	20.786931
71.612796	2748.384698	20.791949
71.663342	2759.459384	20.796967
71.406398	2754.957638	20.801984
71.934212	2755.871716	20.807002
71.816517	2755.877924	20.812019
72.116315	2741.475860	20.817037
71.901357	2748.471767	20.822055
71.725714	2755.005953	20.827072
71.811372	2748.591573	20.832090
71.722428	2753.059636	20.837107
71.819869	2749.725362	20.842125
71.999715	2772.996473	20.847143
72.088048	2776.075414	20.852160
72.220675	2773.610249	20.857178
72.245002	2776.387895	20.862195
72.487009	2770.740702	20.867213
72.469679	2773.833346	20.872231
72.200034	2773.795349	20.877248
72.515621	2784.727887	20.882266
72.826930	2805.836895	20.887283
72.954371	2795.223906	20.892301
72.927369	2805.582579	20.897319
72.989794	2806.047770	20.902336
73.151521	2796.436193	20.907354
73.010401	2797.454589	20.912371
73.464173	2794.810775	20.917389
73.472708	2796.888487	20.922407
73.511614	2796.047699	20.927424
73.842750	2795.740051	20.932442
73.820328	2799.158388	20.937459
73.626111	2794.427159	20.942477
73.669998	2792.196397	20.947495
73.678721	2785.367132	20.952512
74.061642	2782.945434	20.957530
73.838374	2784.057164	20.962547
73.930326	2792.735509	20.967565
74.128865	2787.689143	20.972583
73.995374	2793.154682	20.977600
74.098656	2789.592133	20.982618
74.029708	2790.853099	20.987635
74.125589	2784.959391	20.992653
74.309942	2792.786033	20.997671
73.962830	2791.902181	21.002688
74.377059	2796.227874	21.007706
74.303393	2816.949127	21.012723
74.311566	2808.491624	21.017741
74.170018	2821.238677	21.022759
74.010352	2824.494836	21.027776
74.529822	2830.679073	21.032794
74.786744	2845.539200	21.037811
74.954804	2847.269749	21.042829
75.079383	2843.458364	21.047847
74.880924	2850.076467	21.052864
75.196753	2845.874307	21.057882
75.182590	2852.787899	21.062899
74.935161	2852.329445	21.067917
75.352560	2858.013944	21.072935
75.392397	2871.771251	21.077952
75.557154	2879.737938	21.082970
75.621338	2883.697845	21.087987
75.609984	2882.661329	21.093005
75.431879	2880.604402	21.098023
75.567427	2888.496302	21.103040
75.762304	2871.761967	21.108058
75.359229	2876.853613	21.113075
75.731832	2898.691626	21.118093
75.667858	2909.654108	21.123111
75.240562	2909.575959	21.128128
75.799114	2916.893042	21.133146
75.548490	2947.132618	21.138163
76.233367	2942.838541	21.143181
76.254878	2938.801285	21.148199
76.265509	2958.636920	21.153216
76.965589	2968.256749	21.158234
76.871416	2970.790592	21.163251
77.048647	2972.175149	21.168269
77.031047	2967.056206	21.173287
77.165569	2966.653261	21.178304
77.379183	2964.632185	21.183322
77.135240	2956.423258	21.188339
77.355405	2945.708058	21.193357
77.079840	2952.162297	21.198375
77.224930	2962.838970	21.203392
77.492601	2960.190193	21.208410
77.353886	2968.638757	21.213427
77.123432	2967.083385	21.218445
77.359438	2965.615674	21.223463
77.343797	2971.075072	21.228480
77.433383	2972.259640	21.233498
77.499252	2974.898544	21.238515
77.707784	2983.042380	21.243533
78.151317	2984.855666	21.248551
77.954793	2994.691648	21.253568
78.420839	2982.098058	21.258586
78.414580	2989.349494	21.263603
78.569742	2977.379727	21.268621
78.415755	2973.255598	21.273639
78.401786	2972.486162	21.278656
78.683795	2965.356004	21.283674
78.431849	2976.656871	21.288691
78.725196	2973.283441	21.293709
78.994066	2971.284230	21.298727
78.634859	2971.466611	21.303744
78.906377	2965.455146	21.308762
78.832656	2965.323759	21.313779
78.793933	2970.041895	21.318797
79.136750	2972.990621	21.323815
79.047157	2975.971330	21.328832
79.196338	2970.602386	21.333850
78.960699	2980.592483	21.338867
79.304713	2987.885604	21.343885
79.623183	2994.475617	21.348903
79.599439	3001.128070	21.353920
79.719179	2997.266286	21.358938
79.525311	3004.306935	21.363955
79.648480	3002.636957	21.368973
80.001675	3000.948389	21.373991
79.927409	3004.103653	21.379008
80.301673	2996.354632	21.384026
79.747785	3002.108332	21.389043
79.589973	3001.314634	21.394061
79.814265	3006.517886	21.399079
79.848706	3023.528936	21.404096
79.990889	3023.837461	21.409114
79.921467	3031.968224	21.414131
80.184539	3041.221206	21.419149
80.649575	3057.262144	21.424167
80.587566	3062.780888	21.429184
80.935097	3063.519212	21.434202
80.842291	3071.366602	21.439219
80.848941	3062.755014	21.444237
80.967285	3062.240584	21.449255
80.719593	3063.394774	21.454272
81.043582	3065.323890	21.459290
81.064210	3062.624813	21.464307
80.951693	3080.634010	21.469325
81.274304	3088.345154	21.474343
81.057985	3101.075267	21.479360
81.590535	3081.326716	21.484378
81.564545	3097.538823	21.489395
81.505271	3086.597477	21.494413
81.830302	3086.950790	21.499431
81.638649	3090.629814	21.504448
81.922076	3101.066630	21.509466
82.087010	3112.472611	21.514483
81.751468	3123.581607	21.519501
82.189841	3115.992216	21.524519
82.276535	3115.405740	21.529536
82.470827	3109.424625	21.534554
82.060897	3113.787442	21.539571
82.087747	3113.976698	21.544589
82.465094	3111.415815	21.549607
82.054979	3116.059493	21.554624
82.286277	3125.433232	21.559642
82.385920	3137.247685	21.564659
82.773537	3130.210737	21.569677
82.970577	3139.770877	21.574695
82.847232	3148.321717	21.579712
83.263305	3135.117664	21.584730
82.964078	3140.459512	21.589747
83.339013	3162.493422	21.594765
83.710520	3161.398194	21.599783
83.733875	3165.651813	21.604800
84.013077	3152.939198	21.609818
83.903261	3139.760791	21.614835
83.201736	3135.200811	21.619853
83.741409	3139.154188	21.624871
83.791089	3158.938242	21.629888
83.902484	3156.641595	21.634906
84.000943	3157.935681	21.639923
83.775805	3159.391500	21.644941
84.107617	3156.867763	21.649959
84.105925	3164.588183	21.654976
84.224699	3149.880264	21.659994
84.484211	3148.530717	21.665011
84.615840	3152.523207	21.670029
84.634201	3154.490847	21.675047
84.672604	3167.963896	21.680064
84.796518	3176.256636	21.685082
85.032312	3170.205947	21.690099
84.714466	3170.501302	21.695117
85.149509	3160.583165	21.700135
85.187644	3167.072430	21.705152
85.072252	3173.424132	21.710170
85.178556	3166.527997	21.715187
85.511331	3172.401537	21.720205
85.415351	3169.042947	21.725223
85.437232	3163.215953	21.730240
85.204532	3163.810029	21.735258
85.317602	3167.598595	21.740275
85.140262	3187.761867	21.745293
85.342757	3191.523593	21.750311
85.696002	3195.939370	21.755328
85.700290	3190.904963	21.760346
85.906469	3194.012400	21.765363
86.024853	3200.834222	21.770381
86.258935	3202.306493	21.775399
86.302026	3229.612822	21.780416
86.777441	3215.182292	21.785434
86.748872	3213.132936	21.790451
86.166331	3204.379225	21.795469
86.870194	3205.883568	21.800487
86.452245	3212.524247	21.805504
86.901620	3206.762009	21.810522
87.160623	3207.421634	21.815539
87.013891	3213.225338	21.820557
87.143661	3211.418194	21.825575
87.084575	3210.039995	21.830592
87.518084	3206.151721	21.835610
87.339713	3210.631036	21.840627
87.005832	3208.120620	21.845645
87.124150	3203.960870	21.850663
87.401744	3198.620924	21.855680
87.295943	3200.289777	21.860698
87.489637	3219.854288	21.865715
87.407990	3230.492582	21.870733
87.804992	3233.890551	21.875751
87.601824	3238.993707	21.880768
87.840121	3230.389134	21.885786
88.025368	3239.354153	21.890803
87.947328	3260.536920	21.895821
88.502063	3260.171584	21.900839
88.474949	3259.612691	21.905856
88.522922	3264.745821	21.910874
88.565875	3255.316508	21.915891
88.248700	3268.128927	21.920909
88.704864	3249.626586	21.925927
88.917547	3253.970398	21.930944
88.850635	3252.133253	21.935962
89.016146	3256.520774	21.940979
88.914210	3254.794625	21.945997
89.351259	3265.257407	21.951015
89.517446	3277.242292	21.956032
89.218194	3287.527508	21.961050
89.479928	3286.519789	21.966067
89.507253	3287.223442	21.971085
89.815354	3282.467804	21.976103
89.091368	3290.954816	21.981120
89.310028	3292.402810	21.986138
89.438232	3284.349110	21.991155
89.161304	3296.526601	21.996173
89.919731	3306.516520	22.001191
89.964349	3313.039430	22.006208
89.954870	3314.084853	22.011226
90.105210	3314.367699	22.016243
90.062802	3324.665477	22.021261
90.380639	3339.643045	22.026279
90.526081	3351.042094	22.031296
90.166708	3347.733331	22.036314
90.616000	3351.968643	22.041331
90.596055	3347.935524	22.046349
90.655501	3344.306674	22.051367
90.918833	3351.966052	22.056384
90.775242	3346.846614	22.061402
91.004337	3363.277148	22.066419
91.031552	3375.231568	22.071437
90.913166	3376.258176	22.076455
91.025333	3375.264074	22.081472
91.108471	3391.159388	22.086490
91.717062	3376.950541	22.091507
91.308340	3381.904807	22.096525
91.379551	3397.397689	22.101543
91.633572	3410.546302	22.106560
91.957242	3406.840689	22.111578
92.149402	3406.572501	22.116595
92.061954	3413.680548	22.121613
92.547934	3402.977695	22.126631
91.940501	3393.721230	22.131648
91.935078	3407.096076	22.136666
92.223329	3413.950696	22.141683
92.038355	3434.583584	22.146701
92.516859	3440.135852	22.151719
92.233636	3438.439375	22.156736
92.609376	3430.968371	22.161754
92.515139	3448.363083	22.166771
92.746187	3463.069846	22.171789
93.003005	3463.364035	22.176807
92.907486	3472.845966	22.181824
93.271874	3471.494614	22.186842
93.498089	3457.809220	22.191859
93.253161	3467.057734	22.196877
93.660902	3475.146479	22.201895
93.940052	3485.944543	22.206912
94.000898	3483.891905	22.211930
94.157862	3470.449607	22.216947
93.997814	3464.395839	22.221965
94.112112	3466.335636	22.226983
94.129921	3483.920202	22.232000
94.154509	3488.772368	22.237018
94.265357	3483.623322	22.242035
94.320502	3481.587327	22.247053
94.378203	3483.067300	22.252071
94.671585	3485.851737	22.257088
94.425667	3478.121907	22.262106
94.637327	3475.408812	22.267123
94.856230	3494.976751	22.272141
94.748491	3481.097575	22.277159
94.936995	3492.533922	22.282176
94.899532	3507.652491	22.287194
95.009205	3510.442627	22.292211
95.122027	3520.777935	22.297229
95.053697	3516.157768	22.302247
95.337311	3516.501966	22.307264
95.501629	3510.393309	22.312282
95.562544	3503.310735	22.317299
95.336009	3517.937907	22.322317
95.932576	3533.060814	22.327335
95.731851	3545.529224	22.332352
95.675084	3552.948685	22.337370
96.109363	3547.936843	22.342387
95.773077	3544.109087	22.347405
95.999618	3537.326552	22.352423
95.836157	3547.525789	22.357440
96.176058	3559.886764	22.362458
96.481786	3563.676966	22.367475
96.205051	3578.002256	22.372493
96.441340	3572.461870	22.377511
96.442440	3580.879838	22.382528
96.418094	3597.061554	22.387546
96.816288	3599.926060	22.392563
96.845065	3605.819931	22.397581
96.753189	3607.315902	22.402599
96.841035	3621.011190	22.407616
96.837816	3629.815342	22.412634
97.167056	3642.320473	22.417651
96.829289	3633.344962	22.422669
97.219198	3651.225968	22.427687
97.475184	3657.721620	22.432704
97.421226	3668.272427	22.437722
97.997218	3664.087554	22.442739
98.011911	3661.763769	22.447757
97.864834	3680.388095	22.452775
98.121397	3694.631606	22.457792
98.139305	3692.363157	22.462810
98.418606	3688.167373	22.467827
98.346890	3697.296370	22.472845
98.697732	3685.699962	22.477863
98.944542	3679.006171	22.482880
98.554196	3683.178014	22.487898
99.047964	3700.124472	22.492915
98.819854	3722.057146	22.497933
99.418623	3719.087184	22.502951
99.385274	3705.803247	22.507968
99.178371	3725.160121	22.512986
99.507476	3715.710844	22.518003
99.126742	3722.560577	22.523021
99.570976	3722.188469	22.528039
99.561707	3726.611868	22.533056
99.286925	3726.883057	22.538074
99.730216	3739.024736	22.543091
99.692815	3758.975313	22.548109
99.748810	3755.655289	22.553127
100.124228	3746.241088	22.558144
99.814826	3760.784953	22.563162
100.499950	3764.927715	22.568179
100.166144	3777.032070	22.573197
100.316715	3780.677148	22.578215
100.662057	3778.653052	22.583232
100.341742	3780.169733	22.588250
100.775279	3778.767995	22.593267
100.795966	3777.214966	22.598285
101.054798	3774.481709	22.603303
101.120804	3778.163871	22.608320
101.000626	3797.903497	22.613338
101.125009	3799.351630	22.618355
101.321892	3812.886535	22.623373
101.271411	3805.851472	22.628391
101.656603	3803.804498	22.633408
101.364328	3809.636363	22.638426
101.479901	3802.263299	22.643443
101.881765	3820.528865	22.648461
101.929721	3829.389484	22.653479
101.990487	3839.779732	22.658496
101.842670	3837.349670	22.663514
101.978405	3827.756513	22.668531
102.024044	3831.507230	22.673549
102.378936	3845.813091	22.678567
102.645737	3859.337676	22.683584
102.428057	3867.920496	22.688602
102.928285	3849.235737	22.693619
103.178434	3860.896185	22.698637
102.873017	3858.307167	22.703655
103.159548	3855.487663	22.708672
102.981259	3857.348298	22.713690
103.422475	3856.640756	22.718707
103.179958	3857.282049	22.723725
103.215851	3873.335675	22.728743
104.021282	3872.585789	22.733760
103.999754	3883.264529	22.738778
103.864265	3879.395225	22.743795
104.025804	3881.208755	22.748813
104.285372	3879.833176	22.753831
104.131063	3876.150171	22.758848
104.017049	3879.156983	22.763866
104.250715	3870.222369	22.768883
104.358822	3871.701425	22.773901
103.938835	3888.737952	22.778919
104.509495	3891.442067	22.783936
104.539937	3900.975775	22.788954
104.364248	3908.747145	22.793971
104.550160	3906.887697	22.798989
104.815446	3916.557039	22.804007
104.978002	3913.135813	22.809024
105.003364	3934.061548	22.814042
105.218942	3938.987251	22.819059
105.370231	3934.162009	22.824077
105.122764	3942.297277	22.829095
105.510495	3930.262119	22.834112
105.545227	3954.234795	22.839130
105.615363	3963.980128	22.844147
105.940998	3964.737729	22.849165
105.764896	3966.974852	22.854183
106.139841	3959.534390	22.859200
105.776691	3969.274080	22.864218
106.204424	3963.143688	22.869235
106.019085	3985.533291	22.874253
106.218121	3990.891181	22.879271
106.546374	3993.843228	22.884288
106.384806	3997.459464	22.889306
106.337523	3988.040137	22.894323
106.623980	4014.905548	22.899341
106.724668	4027.629179	22.904359
107.166753	4030.552069	22.909376
107.011368	4034.652715	22.914394
107.114052	4022.181480	22.919411
107.229634	4018.497885	22.924429
107.096701	4040.312012	22.929447
107.400908	4042.749473	22.934464
107.529356	4044.206423	22.939482
107.316558	4037.990903	22.944499
107.685351	4052.194052	22.949517
107.872519	4064.451578	22.954535
108.463690	4081.679531	22.959552
107.964968	4068.953288	22.964570
108.174527	4070.688383	22.969587
108.097498	4076.774747	22.974605
108.427603	4099.099640	22.979623
108.695995	4095.452235	22.984640
108.579215	4098.948856	22.989658
108.969300	4091.985011	22.994675
108.951373	4097.206823	22.999693
109.015242	4099.205881	23.004711
109.511847	4100.829126	23.009728
109.444792	4121.364717	23.014746
109.645845	4123.673102	23.019763
109.866208	4131.213871	23.024781
109.863530	4125.650022	23.029799
110.180306	4117.675150	23.034816
110.059223	4125.226305	23.039834
110.353560	4119.225684	23.044851
110.241742	4126.289184	23.049869
110.170341	4116.455885	23.054887
110.456158	4113.510576	23.059904
110.379775	4119.849384	23.064922
110.606873	4108.565029	23.069939
110.526859	4103.159845	23.074957
110.134424	4121.531200	23.079975
110.481492	4120.626252	23.084992
110.641184	4142.494566	23.090010
111.044679	4141.087361	23.095027
111.017455	4139.456184	23.100045
110.632106	4140.932134	23.105063
111.558147	4155.819853	23.110080
111.717911	4172.654125	23.115098
111.791475	4169.820533	23.120115
111.705687	4162.075820	23.125133
111.816285	4175.803400	23.130151
112.053985	4169.399559	23.135168
111.922914	4177.300054	23.140186
111.974457	4172.110664	23.145203
112.226515	4173.514875	23.150221
112.193985	4174.995933	23.155239
112.335057	4179.503273	23.160256
112.487472	4197.620278	23.165274
112.663285	4202.457220	23.170291
112.658269	4199.202681	23.175309
112.631516	4205.480903	23.180327
112.945897	4203.608801	23.185344
112.689477	4208.043433	23.190362
112.867583	4218.028181	23.195379
112.728883	4227.633127	23.200397
113.043463	4229.154820	23.205415
113.413449	4224.331587	23.210432
113.315721	4240.836459	23.215450
113.518855	4259.710127	23.220467
113.605373	4263.117728	23.225485
113.304083	4266.555698	23.230503
113.647412	4271.328977	23.235520
113.903136	4283.195776	23.240538
113.658909	4290.093232	23.245555
114.019447	4297.124765	23.250573
114.186973	4304.666181	23.255591
114.682205	4304.704459	23.260608
114.832820	4316.929475	23.265626
114.740885	4312.337996	23.270643
115.260044	4309.383764	23.275661
115.229455	4320.239701	23.280679
115.150658	4309.291115	23.285696
115.408159	4318.470274	23.290714
115.383232	4333.066105	23.295731
115.683019	4345.925048	23.300749
115.577444	4353.376295	23.305767
115.701665	4339.078556	23.310784
115.925838	4347.020049	23.315802
116.015878	4342.630836	23.320819
116.061600	4343.798910	23.325837
115.761024	4352.304756	23.330855
115.984076	4364.409697	23.335872
115.911543	4368.605003	23.340890
116.184769	4368.743978	23.345907
116.792443	4390.587647	23.350925
116.728808	4408.399502	23.355943
116.967267	4394.700275	23.360960
117.401381	4403.593285	23.365978
117.129735	4405.216338	23.370995
117.274446	4391.900243	23.376013
117.006738	4409.730478	23.381031
117.363681	4408.672105	23.386048
117.319448	4414.333275	23.391066
117.483393	4428.539558	23.396083
117.744007	4437.937001	23.401101
117.941321	4428.684509	23.406119
118.476637	4411.123167	23.411136
118.549354	4418.200652	23.416154
118.345765	4417.713909	23.421171
118.755044	4410.041176	23.426189
119.210267	4407.901139	23.431207
118.966499	4401.770647	23.436224
119.056837	4401.859326	23.441242
118.834512	4402.658696	23.446259
119.028823	4388.104279	23.451277
118.955142	4395.267246	23.456295
119.335162	4392.512195	23.461312
119.329855	4399.552549	23.466330
119.298720	4393.989202	23.471347
119.701594	4384.940761	23.476365
119.511484	4410.837349	23.481383
119.568373	4419.723647	23.486400
119.721318	4425.964657	23.491418
120.122046	4428.791165	23.496435
119.988519	4430.547967	23.501453
119.982357	4433.955438	23.506471
120.331526	4434.834402	23.511488
120.236395	4441.237700	23.516506
120.073794	4458.712949	23.521523
120.416241	4452.530659	23.526541
120.288736	4462.406962	23.531559
120.578684	4480.336389	23.536576
120.773055	4489.100108	23.541594
120.604889	4484.209977	23.546611
121.070172	4491.473505	23.551629
121.080420	4513.133332	23.556647
121.201739	4510.628775	23.561664
121.380041	4510.481575	23.566682
121.139555	4526.472202	23.571699
121.814126	4533.222482	23.576717
122.026798	4546.287450	23.581735
122.181377	4545.129166	23.586752
122.069591	4544.737134	23.591770
122.352905	4544.392245	23.596787
122.458012	4547.975533	23.601805
122.456803	4566.054550	23.606823
122.664368	4559.757620	23.611840
122.942252	4561.482668	23.616858
122.879620	4571.612250	23.621875
123.444706	4565.640658	23.626893
123.134428	4564.185161	23.631911
123.134499	4568.005484	23.636928
123.579423	4585.187333	23.641946
123.612389	4593.368716	23.646963
124.044246	4593.395862	23.651981
123.673365	4611.080726	23.656999
123.853331	4599.793284	23.662016
123.957934	4597.983693	23.667034
123.928536	4600.874097	23.672051
124.046752	4606.771417	23.677069
123.825864	4625.090081	23.682087
124.113391	4624.525810	23.687104
124.440213	4617.395583	23.692122
124.259210	4625.788899	23.697139
124.948229	4632.846105	23.702157
124.848317	4655.112175	23.707175
125.003363	4652.018467	23.712192
125.519919	4649.373768	23.717210
125.301258	4653.228202	23.722227
125.641563	4645.383827	23.727245
125.608798	4649.679867	23.732263
125.479334	4651.430539	23.737280
125.848834	4665.874124	23.742298
125.870095	4670.849153	23.747315
126.015590	4669.909444	23.752333
125.911601	4679.873401	23.757351
126.169774	4673.284347	23.762368
126.426141	4676.824667	23.767386
126.102797	4696.386260	23.772403
126.829385	4694.580545	23.777421
126.655691	4704.212621	23.782439
126.582404	4700.919292	23.787456
126.782410	4711.012600	23.792474
126.992336	4718.396417	23.797491
127.358345	4717.194181	23.802509
127.471818	4722.890901	23.807527
127.460815	4725.012125	23.812544
127.699946	4718.945327	23.817562
127.448085	4728.747227	23.822579
127.829952	4745.405131	23.827597
127.922747	4759.026738	23.832615
127.898243	4753.267876	23.837632
128.148098	4760.521045	23.842650
128.351867	4778.467724	23.847667
128.931405	4785.128641	23.852685
128.632944	4786.691498	23.857703
129.016476	4793.440316	23.862720
129.026734	4783.056213	23.867738
128.805183	4787.585371	23.872755
129.320701	4779.143395	23.877773
129.154849	4787.976530	23.882791
129.134820	4806.235856	23.887808
129.488994	4809.423893	23.892826
129.501943	4825.761505	23.897843
129.607227	4806.910362	23.902861
129.812084	4829.373560	23.907879
129.686073	4848.060511	23.912896
130.143321	4846.604550	23.917914
130.130656	4847.546742	23.922931
130.486387	4853.307161	23.927949
130.453586	4874.902004	23.932967
130.488213	4885.496989	23.937984
130.745870	4872.312720	23.943002
130.948663	4889.281777	23.948019
131.106441	4874.668196	23.953037
130.678735	4889.722166	23.958055
130.947154	4907.045826	23.963072
131.484902	4903.124765	23.968090
131.349618	4905.061278	23.973107
131.623746	4901.417485	23.978125
131.663918	4909.771763	23.983143
131.524327	4921.929477	23.988160
131.927809	4925.565199	23.993178
131.989430	4932.219862	23.998195
132.367884	4925.733462	24.003213
132.569866	4936.543329	24.008231
132.641350	4956.589883	24.013248
132.988919	4947.623086	24.018266
132.791232	4951.710274	24.023283
133.326396	4948.020915	24.028301
133.314049	4953.408142	24.033319
133.296282	4946.064423	24.038336
133.483653	4942.056031	24.043354
133.080509	4953.147277	24.048371
133.362360	4961.213654	24.053389
133.539789	4978.429174	24.058407
133.329718	4986.495324	24.063424
133.946385	4977.588667	24.068442
134.035027	4997.509809	24.073459
134.384895	4999.848106	24.078477
134.304656	5005.849609	24.083495
134.204347	5011.460156	24.088512
134.538073	5016.081798	24.093530
134.509376	5028.995288	24.098547
134.446206	5031.308971	24.103565
134.866449	5032.970467	24.108583
134.675803	5051.025997	24.113600
135.009022	5058.882043	24.118618
135.086294	5082.479214	24.123635
135.444666	5080.562229	24.128653
135.465028	5097.990178	24.133671
135.647218	5095.675652	24.138688
136.020079	5100.143172	24.143706
135.833775	5107.921583	24.148723
136.496861	5116.171151	24.153741
136.599386	5124.916851	24.158759
136.575097	5127.453293	24.163776
136.861284	5124.034107	24.168794
137.038540	5123.039742	24.173811
136.896555	5115.408125	24.178829
137.330285	5126.215011	24.183847
137.036499	5131.754175	24.188864
137.625560	5147.452709	24.193882
137.438519	5158.807830	24.198899
137.646357	5155.828335	24.203917
137.973926	5157.473152	24.208935
137.911334	5156.444645	24.213952
138.209045	5154.049538	24.218970
137.923671	5169.015010	24.223987
138.157848	5175.411752	24.229005
138.146930	5181.097800	24.234023
138.068504	5185.579868	24.239040
138.700201	5187.197440	24.244058
138.588130	5204.464104	24.249075
138.792177	5212.160661	24.254093
139.013700	5225.410496	24.259111
138.615527	5230.176437	24.264128
139.118335	5228.730487	24.269146
139.073456	5248.910856	24.274163
139.167674	5261.623211	24.279181
139.426232	5259.416857	24.284199
139.407466	5289.314281	24.289216
139.692464	5279.081141	24.294234
139.505164	5289.592213	24.299251
139.601499	5301.560778	24.304269
140.078249	5316.192460	24.309287
140.004134	5320.301744	24.314304
140.311470	5330.434224	24.319322
140.528964	5349.793218	24.324339
140.760638	5348.900309	24.329357
141.377060	5353.969498	24.334375
141.860232	5352.720997	24.339392
142.513419	5346.447098	24.344410
142.286791	5335.224711	24.349427
142.690052	5312.141425	24.354445
142.757587	5303.683252	24.359463
142.938964	5303.847113	24.364480
143.367079	5298.552443	24.369498
143.288779	5284.358462	24.374515
143.083831	5268.622189	24.379533
143.287585	5255.829324	24.384551
143.116137	5259.563092	24.389568
143.329076	5257.493041	24.394586
143.230849	5259.939803	24.399603
143.174544	5250.613157	24.404621
143.302367	5248.142057	24.409639
143.077898	5257.055625	24.414656
143.744739	5271.992901	24.419674
143.776234	5283.642139	24.424691
143.821695	5282.757680	24.429709
144.419350	5280.551545	24.434727
144.484296	5285.873857	24.439744
144.561604	5277.393685	24.444762
144.311697	5279.260404	24.449779
144.393792	5280.776009	24.454797
144.826965	5270.287944	24.459815
144.851167	5286.828042	24.464832
144.748619	5285.963248	24.469850
145.083342	5303.899917	24.474867
145.152768	5296.274624	24.479885
145.043271	5293.617129	24.484903
144.783965	5314.651578	24.489920
145.283911	5323.736066	24.494938
145.434806	5331.897482	24.499955
145.828589	5350.293701	24.504973
145.690965	5355.754548	24.509991
145.573573	5366.289933	24.515008
145.729951	5372.303424	24.520026
145.920777	5386.496905	24.525043
145.967255	5398.856653	24.530061
146.632820	5399.730081	24.535079
146.613194	5421.073430	24.540096
147.012220	5427.835808	24.545114
146.785939	5427.164608	24.550131
146.693001	5431.450800	24.555149
147.146129	5448.645729	24.560167
147.423430	5462.421098	24.565184
147.430411	5464.396368	24.570202
147.555002	5479.148089	24.575219
147.707861	5490.498838	24.580237
147.965726	5481.975599	24.585255
148.007709	5501.147202	24.590272
147.927185	5505.103352	24.595290
148.296925	5526.672731	24.600307
148.029339	5541.763198	24.605325
148.422821	5548.307007	24.610343
148.631898	5558.262552	24.615360
148.982465	5573.154575	24.620378
149.336404	5579.242866	24.625395
149.615358	5583.126774	24.630413
150.027175	5580.379029	24.635431
149.528561	5584.497059	24.640448
150.089845	5595.546738	24.645466
150.476738	5613.314964	24.650483
150.234569	5610.832772	24.655501
150.585415	5606.828036	24.660519
150.263922	5607.481987	24.665536
150.412354	5607.063385	24.670554
151.005344	5618.131629	24.675571
150.994356	5625.154591	24.680589
151.199204	5640.291785	24.685607
150.913769	5650.380523	24.690624
151.484082	5631.741362	24.695642
151.735007	5641.137975	24.700659
151.603942	5657.597028	24.705677
151.739085	5650.208123	24.710695
151.939083	5659.142375	24.715712
152.029049	5668.452945	24.720730
152.273094	5683.346327	24.725747
152.127289	5695.031238	24.730765
152.405732	5691.073429	24.735783
152.400529	5702.885417	24.740800
152.717542	5716.882858	24.745818
153.171001	5712.662679	24.750835
152.840113	5720.150535	24.755853
153.594410	5736.957108	24.760871
153.679180	5759.072654	24.765888
153.640045	5752.063177	24.770906
153.953916	5746.182316	24.775923
153.847277	5747.808312	24.780941
154.067896	5739.057191	24.785959
154.310291	5751.527617	24.790976
155.014530	5751.780429	24.795994
154.935269	5766.138501	24.801011
154.550276	5758.255759	24.806029
155.221978	5757.291097	24.811047
155.135776	5758.754906	24.816064
154.921650	5761.824478	24.821082
155.180572	5761.577871	24.826099
155.347620	5767.460790	24.831117
155.658280	5780.006116	24.836135
155.533149	5792.397487	24.841152
155.321132	5798.432121	24.846170
155.808824	5801.501530	24.851187
155.556463	5820.607965	24.856205
156.107261	5824.174008	24.861223
156.107095	5832.049792	24.866240
156.174797	5844.294803	24.871258
156.700625	5854.893995	24.876275
156.754511	5867.125493	24.881293
156.982502	5871.854747	24.886311
156.809816	5883.599166	24.891328
157.111783	5889.605393	24.896346
157.372082	5910.690023	24.901363
157.506163	5925.866330	24.906381
157.789372	5919.633873	24.911399
157.442417	5928.036286	24.916416
157.597101	5946.496546	24.921434
157.644938	5964.196511	24.926451
157.948446	5980.193238	24.931469
158.471542	5980.155498	24.936487
158.357788	6003.646118	24.941504
158.266048	6018.426573	24.946522
158.742428	6025.098215	24.951539
159.272883	6039.791294	24.956557
159.285722	6052.606999	24.961575
159.464224	6057.162452	24.966592
159.586220	6067.240016	24.971610
159.923809	6087.055270	24.976627
159.978758	6089.052874	24.981645
160.264549	6078.917410	24.986663
160.419178	6092.537470	24.991680
160.326930	6110.548700	24.996698
160.776831	6112.991613	25.001715
160.935847	6123.662856	25.006733
161.484877	6112.689944	25.011751
161.371094	6115.273082	25.016768
161.643829	6127.387289	25.021786
161.963548	6134.855812	25.026803
161.797288	6149.175408	25.031821
161.875158	6130.000431	25.036839
162.056734	6137.298213	25.041856
161.808791	6138.603733	25.046874
162.341234	6140.444963	25.051891
162.003173	6164.927566	25.056909
162.580652	6167.539768	25.061927
162.605532	6175.666665	25.066944
162.827981	6186.345937	25.071962
163.080897	6186.596757	25.076979
163.216549	6200.633014	25.081997
163.546473	6191.413362	25.087015
163.494982	6192.029796	25.092032
163.397004	6208.863424	25.097050
163.891430	6209.167796	25.102067
163.877473	6221.921040	25.107085
164.136117	6228.284442	25.112103
164.001805	6229.929851	25.117120
164.399533	6236.274229	25.122138
164.366123	6239.069602	25.127155
164.178135	6250.571266	25.132173
164.798841	6269.031590	25.137191
165.053097	6272.187887	25.142208
165.075423	6281.721279	25.147226
165.278985	6285.286934	25.152243
165.295260	6300.291999	25.157261
165.619109	6307.677336	25.162279
165.859576	6321.870096	25.167296
165.883428	6334.019430	25.172314
166.485143	6331.976160	25.177331
166.284780	6343.739517	25.182349
166.642132	6344.728245	25.187367
167.159198	6362.504945	25.192384
167.033656	6370.574889	25.197402
167.391963	6368.886720	25.202419
167.333352	6374.128411	25.207437
167.511300	6363.520549	25.212455
167.803015	6377.703618	25.217472
167.965158	6393.508531	25.222490
168.254155	6388.397744	25.227507
168.051329	6391.566354	25.232525
168.265764	6393.453597	25.237543
168.544314	6404.172865	25.242560
168.809234	6420.756893	25.247578
168.911101	6430.539710	25.252595
168.632029	6432.164157	25.257613
169.017347	6424.060682	25.262631
169.139593	6449.793793	25.267648
169.266297	6466.307063	25.272666
169.501882	6460.797194	25.277683
169.341927	6475.409583	25.282701
169.979796	6486.386353	25.287719
170.061503	6489.748028	25.292736
170.121513	6500.104076	25.297754
170.501631	6498.653184	25.302771
170.411000	6522.833341	25.307789
170.657547	6526.595202	25.312807
170.684927	6539.563226	25.317824
170.498226	6555.263413	25.322842
171.165658	6542.407324	25.327859
171.060726	6569.769394	25.332877
171.506499	6589.613710	25.337895
171.728181	6589.154292	25.342912
171.740806	6593.671051	25.347930
171.916734	6598.455262	25.352947
171.865738	6614.337665	25.357965
172.492239	6615.447163	25.362983
172.635754	6620.050857	25.368000
172.670254	6624.696325	25.373018
172.911193	6636.962369	25.378035
172.649855	6642.511077	25.383053
172.894407	6646.838231	25.388071
173.491439	6659.331568	25.393088
173.606626	6682.211586	25.398106
173.430591	6671.887335	25.403123
173.660905	6694.092013	25.408141
173.726489	6704.631433	25.413159
173.975856	6715.221818	25.418176
174.247184	6718.417979	25.423194
174.398624	6728.269411	25.428211
174.438737	6740.431435	25.433229
174.305023	6753.478832	25.438247
174.768992	6771.650039	25.443264
175.028341	6768.351214	25.448282
175.225593	6785.198225	25.453299
175.326852	6802.072362	25.458317
175.550768	6811.794270	25.463335
175.623382	6828.936594	25.468352
176.129855	6822.150429	25.473370
176.822687	6816.449508	25.478387
176.804709	6832.829670	25.483405
176.901942	6839.784020	25.488423
177.351205	6838.349613	25.493440
177.350050	6847.725810	25.498458
177.809971	6838.772233	25.503475
177.972917	6844.753017	25.508493
177.876437	6845.746465	25.513511
177.948194	6837.078235	25.518528
177.902640	6848.409725	25.523546
178.146455	6862.493099	25.528563
178.156575	6873.271239	25.533581
178.241033	6873.704724	25.538599
178.698835	6890.149550	25.543616
178.409755	6903.208471	25.548634
178.724675	6911.847403	25.553651
178.816121	6928.805866	25.558669
179.081631	6939.598417	25.563687
179.200658	6949.274977	25.568704
179.466444	6967.045254	25.573722
179.650622	6971.670115	25.578739
179.568860	6976.240593	25.583757
179.790121	7008.482637	25.588775
180.188691	7004.997114	25.593792
180.812251	7019.250643	25.598810
180.923327	7020.024530	25.603827
181.140696	7032.286003	25.608845
181.299416	7036.049408	25.613863
181.383046	7031.577019	25.618880
181.346870	7037.325244	25.623898
181.594298	7048.410319	25.628915
181.844980	7061.960876	25.633933
182.210607	7065.264828	25.638951
182.395891	7062.056433	25.643968
182.394726	7068.982514	25.648986
182.516101	7055.386848	25.654003
182.821140	7076.547836	25.659021
182.686047	7085.510406	25.664039
183.253743	7085.829877	25.669056
182.923457	7091.058476	25.674074
183.419802	7092.265090	25.679092
183.983631	7110.773305	25.684109
184.014326	7112.560890	25.689127
184.393138	7104.524182	25.694144
183.991551	7101.932596	25.699162
184.325045	7118.190157	25.704180
184.722274	7134.012673	25.709197
184.964744	7127.970335	25.714215
185.218127	7123.881595	25.719232
185.199323	7134.117671	25.724250
185.342435	7138.119646	25.729268
185.521333	7149.524169	25.734285
185.371117	7165.375766	25.739303
185.647390	7167.276071	25.744320
185.623473	7185.258822	25.749338
186.281423	7180.721583	25.754356
186.380912	7195.360984	25.759373
186.243039	7203.600157	25.764391
186.243388	7210.698385	25.769408
186.437018	7230.595560	25.774426
186.608685	7251.726128	25.779444
186.925364	7257.730570	25.784461
187.031279	7263.866972	25.789479
187.506577	7278.498476	25.794496
187.749233	7279.578735	25.799514
188.278131	7294.344919	25.804532
188.537880	7302.804816	25.809549
188.521598	7310.451826	25.814567
188.817504	7306.032856	25.819584
188.865294	7309.037380	25.824602
189.062418	7319.948125	25.829620
189.484086	7329.575111	25.834637
189.443624	7343.045654	25.839655
189.886390	7339.196560	25.844672
189.750419	7347.013748	25.849690
189.811631	7348.169364	25.854708
189.993718	7359.680554	25.859725
190.133499	7362.576786	25.864743
190.634767	7361.295351	25.869760
190.217877	7374.465547	25.874778
190.729231	7385.017793	25.879796
191.017813	7392.935713	25.884813
191.283443	7407.282875	25.889831
191.388798	7410.576466	25.894848
191.176370	7427.007952	25.899866
191.216686	7436.407808	25.904884
191.734943	7441.435943	25.909901
191.480288	7461.454466	25.914919
191.813811	7459.210666	25.919936
191.573953	7490.086502	25.924954
192.132124	7492.571409	25.929972
192.709022	7512.285895	25.934989
192.465695	7528.696451	25.940007
192.704261	7533.521340	25.945024
193.469568	7550.020564	25.950042
193.832929	7554.341636	25.955060
193.909431	7563.146432	25.960077
193.755463	7572.342857	25.965095
193.937340	7587.879142	25.970112
194.321032	7599.606245	25.975130
194.246289	7599.691364	25.980148
194.647650	7612.996503	25.985165
194.402948	7627.787199	25.990183
194.753853	7644.821574	25.995200
195.065840	7664.127610	26.000218
195.452448	7662.813283	26.005236
195.836991	7668.327862	26.010253
196.159110	7672.286495	26.015271
196.632571	7660.171722	26.020288
196.405257	7664.634990	26.025306
196.710222	7658.841362	26.030324
197.339641	7668.034140	26.035341
197.367397	7686.607289	26.040359
197.562920	7693.802108	26.045376
197.382112	7689.425974	26.050394
197.680831	7683.240677	26.055412
198.133509	7687.832402	26.060429
197.643250	7697.505071	26.065447
198.137031	7706.377988	26.070464
198.219098	7722.777801	26.075482
198.227948	7726.855635	26.080500
198.764982	7733.058455	26.085517
198.550797	7763.228071	26.090535
198.909576	7762.188076	26.095552
198.730856	7779.297200	26.100570
198.919458	7780.956610	26.105588
199.179051	7798.313785	26.110605
199.339898	7824.772960	26.115623
199.723089	7832.351834	26.120640
199.661168	7856.145570	26.125658
200.081997	7865.864713	26.130676
200.259069	7873.903356	26.135693
200.505318	7892.993543	26.140711
200.538236	7893.886168	26.145728
200.696938	7918.666616	26.150746
201.100840	7925.687080	26.155764
201.328763	7942.964094	26.160781
201.167885	7962.617772	26.165799
201.512255	7966.163356	26.170816
202.011674	7982.539808	26.175834
201.952020	7994.270226	26.180852
202.445497	8012.256870	26.185869
202.596054	8022.265108	26.190887
202.972706	8023.743876	26.195904
203.148668	8040.866004	26.200922
203.328615	8038.394401	26.205940
203.609532	8040.712320	26.210957
203.735821	8052.977745	26.215975
204.355412	8068.486066	26.220992
204.459835	8071.974318	26.226010
204.225242	8076.351915	26.231028
204.741840	8066.099234	26.236045
204.933040	8089.105036	26.241063
204.949385	8099.085539	26.246080
204.961427	8106.957431	26.251098
205.065311	8111.879129	26.256116
205.483962	8128.005397	26.261133
205.227028	8139.113064	26.266151
205.700194	8150.296750	26.271168
205.929251	8162.171313	26.276186
205.814929	8175.991178	26.281204
206.294083	8189.816384	26.286221
206.296701	8205.186341	26.291239
206.538553	8218.630766	26.296256
206.827451	8234.752653	26.301274
207.264401	8252.128904	26.306292
207.487997	8255.639908	26.311309
207.165003	8273.766074	26.316327
207.655716	8283.644325	26.321344
207.971458	8291.147232	26.326362
208.243514	8321.081106	26.331380
208.430977	8319.557676	26.336397
208.859741	8340.099926	26.341415
209.551401	8338.282864	26.346432
209.685653	8342.192935	26.351450
209.589062	8347.016434	26.356468
209.862787	8342.378395	26.361485
210.231171	8368.125550	26.366503
210.522611	8374.860798	26.371520
210.448962	8364.029191	26.376538
210.416375	8382.201657	26.381556
210.872132	8386.510606	26.386573
211.078243	8406.044983	26.391591
211.329497	8403.408504	26.396608
211.263877	8418.623911	26.401626
211.248462	8438.513921	26.406644
211.619069	8436.861739	26.411661
211.525843	8459.389753	26.416679
211.645035	8476.875547	26.421696
211.967645	8487.544837	26.426714
212.170669	8510.527762	26.431732
212.830789	8517.694166	26.436749
212.930982	8538.081318	26.441767
213.232137	8541.817286	26.446784
213.405829	8551.923311	26.451802
213.157287	8555.223601	26.456820
213.865402	8566.106920	26.461837
213.915514	8583.480302	26.466855
214.009007	8581.969465	26.471872
214.396094	8594.189433	26.476890
214.563649	8609.283267	26.481908
214.659718	8601.404549	26.486925
214.885211	8635.344488	26.491943
215.234825	8637.161291	26.496960
215.497260	8647.182017	26.501978
215.759435	8657.595866	26.506996
216.241727	8652.545969	26.512013
216.052298	8658.727273	26.517031
216.309786	8673.163515	26.522048
216.756523	8680.690593	26.527066
216.329693	8684.144061	26.532084
217.027769	8693.006646	26.537101
216.935066	8712.888093	26.542119
217.257392	8717.844027	26.547136
217.535201	8727.381537	26.552154
217.501058	8755.306851	26.557172
218.031297	8757.748038	26.562189
218.133038	8779.495105	26.567207
218.361682	8777.850959	26.572224
218.720686	8790.111370	26.577242
218.773553	8803.314166	26.582260
219.494705	8803.120145	26.587277
219.746763	8815.315390	26.592295
219.946349	8828.733264	26.597312
220.129800	8836.395251	26.602330
219.664745	8839.192632	26.607348
220.327692	8855.694285	26.612365
220.569356	8870.695514	26.617383
220.422388	8877.253381	26.622400
220.702649	8892.332683	26.627418
221.007910	8906.516795	26.632436
221.319573	8908.536026	26.637453
221.355685	8932.334335	26.642471
221.701551	8939.858345	26.647488
221.976908	8951.275233	26.652506
221.777694	8978.434816	26.657524
221.935237	8983.440322	26.662541
222.427065	9000.960974	26.667559
222.227112	9015.060463	26.672576
222.763972	9029.689783	26.677594
222.742378	9045.380422	26.682612
223.261211	9066.369291	26.687629
223.347890	9087.520724	26.692647
223.501963	9108.265210	26.697664
223.889614	9115.976633	26.702682
224.091277	9139.202730	26.707700
224.670870	9134.093489	26.712717
225.320214	9145.972272	26.717735
225.549547	9155.632286	26.722752
225.511197	9152.944260	26.727770
225.944640	9163.402381	26.732788
226.088357	9159.160593	26.737805
225.688068	9164.272000	26.742823
225.747678	9173.427094	26.747840
226.187010	9184.210094	26.752858
226.273436	9195.884718	26.757876
226.532697	9210.131538	26.762893
226.595676	9228.977995	26.767911
226.856983	9253.686455	26.772928
227.218306	9258.154337	26.777946
227.111102	9274.724132	26.782964
227.436283	9280.325114	26.787981
227.827320	9319.907566	26.792999
227.903714	9335.689523	26.798016
228.407107	9345.583381	26.803034
227.852814	9365.192215	26.808052
228.309971	9389.046898	26.813069
228.838755	9407.937374	26.818087
229.166907	9425.686474	26.823104
229.674603	9431.535434	26.828122
229.404615	9459.885663	26.833140
229.894725	9461.557801	26.838157
230.418918	9476.935634	26.843175
230.608500	9487.043693	26.848192
231.199311	9511.831873	26.853210
230.791039	9530.246617	26.858228
231.435261	9527.123517	26.863245
231.921667	9543.666665	26.868263
231.812103	9549.013598	26.873280
232.313674	9555.527404	26.878298
232.523093	9565.789357	26.883316
232.611923	9573.211822	26.888333
232.981459	9591.150480	26.893351
232.621961	9592.371760	26.898368
233.156917	9601.936519	26.903386
233.245208	9624.972101	26.908404
233.647377	9637.853556	26.913421
233.724442	9650.775433	26.918439
233.729775	9662.036799	26.923456
233.868227	9673.182121	26.928474
233.889124	9694.148540	26.933492
234.837226	9711.459965	26.938509
234.913765	9730.110107	26.943527
234.863147	9750.322655	26.948544
235.350051	9750.720410	26.953562
235.231672	9778.047588	26.958580
235.809748	9790.108631	26.963597
236.326916	9808.151509	26.968615
236.192186	9817.101087	26.973632
236.250807	9829.612491	26.978650
236.734806	9845.515741	26.983668
237.050274	9859.088812	26.988685
237.353718	9882.250253	26.993703
237.675945	9880.652853	26.998720
237.893937	9889.034700	27.003738
237.669163	9907.420259	27.008756
238.274218	9906.976376	27.013773
238.629804	9921.417073	27.018791
238.845772	9940.883016	27.023808
239.147990	9948.647052	27.028826
238.937170	9949.585735	27.033844
239.390372	9956.682333	27.038861
239.780623	9969.772562	27.043879
239.841783	9971.658731	27.048896
240.405614	9992.387524	27.053914
240.996652	9995.322915	27.058932
241.019925	10002.830020	27.063949
240.769933	9999.000972	27.068967
241.197009	10034.595346	27.073984
241.102383	10027.776867	27.079002
241.727427	10042.075173	27.084020
241.689918	10058.449773	27.089037
242.276551	10057.587775	27.094055
242.323124	10076.029450	27.099072
242.772719	10069.498821	27.104090
243.099185	10085.540767	27.109108
243.488947	10097.539603	27.114125
243.795334	10106.401725	27.119143
243.731954	10111.422361	27.124160
244.238309	10103.975246	27.129178
244.151973	10107.403087	27.134196
244.289774	10128.182662	27.139213
244.354773	10137.819136	27.144231
244.339086	10153.186918	27.149248
245.372488	10154.807169	27.154266
245.492632	10169.051694	27.159284
245.508891	10177.322622	27.164301
245.818348	10194.487712	27.169319
246.173376	10199.941440	27.174336
246.375418	10210.933788	27.179354
246.125882	10231.058666	27.184372
246.576960	10235.862761	27.189389
246.868739	10263.170300	27.194407
246.670131	10272.097273	27.199424
247.071359	10285.234037	27.204442
247.230269	10304.245596	27.209460
247.686020	10327.869432	27.214477
247.881322	10344.762085	27.219495
248.244883	10362.573547	27.224512
248.308325	10380.736266	27.229530
248.483941	10406.496005	27.234548
248.640992	10412.296965	27.239565
248.972947	10429.294248	27.244583
248.992046	10462.856841	27.249600
249.903964	10468.574491	27.254618
250.118817	10494.074309	27.259636
249.631069	10513.215964	27.264653
250.303342	10526.301078	27.269671
249.983740	10550.848477	27.274688
250.238341	10566.063805	27.279706
250.928713	10587.490240	27.284724
251.140638	10602.632917	27.289741
251.594254	10611.632819	27.294759
251.831576	10638.236660	27.299776
252.207288	10645.669807	27.304794
252.348779	10659.022627	27.309812
252.655504	10677.269703	27.314829
253.038183	10681.546902	27.319847
253.010452	10710.231949	27.324864
253.138547	10700.725331	27.329882
253.748338	10725.892241	27.334900
254.403879	10717.503357	27.339917
254.907935	10714.217805	27.344935
254.870058	10735.462239	27.349952
255.628447	10728.472455	27.354970
256.018762	10726.742521	27.359988
256.471780	10725.577134	27.365005
256.462649	10714.981074	27.370023
256.962008	10720.057425	27.375040
257.007183	10717.813865	27.380058
257.414285	10714.700782	27.385076
257.422022	10723.555779	27.390093
257.429315	10710.272105	27.395111
257.148091	10714.873146	27.400128
257.598762	10726.516873	27.405146
257.630458	10746.546451	27.410164
257.827770	10764.117686	27.415181
257.856369	10774.658388	27.420199
257.951846	10786.834939	27.425216
258.316538	10807.290832	27.430234
258.650159	10827.350311	27.435252
258.688245	10848.796481	27.440269
259.257673	10859.319511	27.445287
259.283038	10889.558338	27.450304
259.623064	10907.931824	27.455322
260.053657	10920.415932	27.460340
259.859610	10936.583859	27.465357
260.526588	10952.221036	27.470375
260.845457	10971.212269	27.475392
261.342769	10983.731051	27.480410
261.739382	11003.929478	27.485428
261.593516	11010.601034	27.490445
262.138334	11015.269234	27.495463
262.112602	11036.607980	27.500480
262.632702	11049.752637	27.505498
263.080149	11067.544283	27.510516
262.922005	11077.400309	27.515533
263.194046	11089.660921	27.520551
263.295573	11113.641141	27.525568
263.692796	11126.759604	27.530586
263.966238	11149.848479	27.535604
264.040170	11159.530815	27.540621
264.682812	11170.762758	27.545639
264.519046	11192.833462	27.550656
264.793671	11201.185174	27.555674
265.211580	11213.797479	27.560692
265.003514	11222.832379	27.565709
265.373905	11234.067425	27.570727
265.715160	11264.170073	27.575744
265.940976	11276.184374	27.580762
266.195505	11298.340268	27.585780
266.194594	11315.366617	27.590797
266.924994	11330.534626	27.595815
266.850865	11358.607687	27.600832
267.211855	11381.630032	27.605850
267.740889	11395.451044	27.610868
267.635761	11424.862873	27.615885
268.132739	11437.927928	27.620903
268.467779	11458.342992	27.625920
268.767089	11478.634696	27.630938
269.032212	11484.747452	27.635956
269.302749	11503.006412	27.640973
269.896634	11519.707375	27.645991
270.030771	11542.383401	27.651008
270.246184	11547.357518	27.656026
270.900222	11574.666754	27.661044
271.103568	11581.893680	27.666061
271.287072	11577.254482	27.671079
271.881214	11599.745707	27.676096
271.950365	11601.880708	27.681114
272.176049	11613.494670	27.686132
272.138247	11634.622092	27.691149
272.991703	11639.748579	27.696167
273.229017	11648.544699	27.701184
273.720402	11655.933150	27.706202
274.389529	11653.623849	27.711220
274.423774	11663.017279	27.716237
274.807404	11651.151549	27.721255
274.838945	11663.408260	27.726272
275.083877	11668.682514	27.731290
274.899881	11673.289400	27.736308
275.191222	11683.478939	27.741325
275.550792	11701.287111	27.746343
275.719180	11712.160377	27.751360
275.686959	11715.579955	27.756378
275.640176	11731.813017	27.761396
275.846109	11757.948033	27.766413
276.298139	11776.264583	27.771431
276.704878	11801.541215	27.776448
276.678766	11822.837443	27.781466
277.181486	11849.453459	27.786484
276.949718	11869.089473	27.791501
277.573803	11888.184729	27.796519
277.635135	11918.820511	27.801536
278.088479	11925.907204	27.806554
278.900413	11942.204927	27.811572
279.271573	11960.969270	27.816589
279.627068	11975.103998	27.821607
279.633450	11990.332186	27.826624
280.003997	11992.761794	27.831642
280.312390	12008.581982	27.836660
280.265693	12027.767403	27.841677
280.947916	12035.882040	27.846695
281.300723	12044.845742	27.851712
281.340124	12047.046353	27.856730
281.389844	12062.596719	27.861748
281.710218	12076.301275	27.866765
281.948815	12088.111306	27.871783
281.747922	12110.906124	27.876800
282.397607	12128.866323	27.881818
282.471432	12146.744372	27.886836
282.900792	12182.177560	27.891853
283.131508	12184.347895	27.896871
283.534853	12208.017662	27.901888
283.573469	12236.691675	27.906906
284.050889	12253.582623	27.911924
284.507683	12278.292823	27.916941
284.541595	12290.043737	27.921959
284.330801	12314.266707	27.926976
284.602667	12336.728533	27.931994
285.159827	12363.544773	27.937012
285.083792	12396.960920	27.942029
285.429401	12406.981329	27.947047
286.029714	12441.189861	27.952064
286.543122	12460.303480	27.957082
287.159910	12481.274618	27.962100
287.401854	12505.913364	27.967117
287.552809	12518.556320	27.972135
287.775377	12541.100690	27.977152
288.388140	12550.296791	27.982170
288.937068	12570.491533	27.987188
289.095482	12594.038198	27.992205
289.727549	12599.895156	27.997223
289.861813	12613.163086	28.002240
290.074094	12617.998732	28.007258
290.573836	12623.304930	28.012276
290.839010	12634.342113	28.017293
290.903137	12645.953689	28.022311
291.238083	12655.501906	28.027328
290.927823	12670.686192	28.032346
291.727345	12680.626076	28.037364
291.896543	12708.190658	28.042381
292.120564	12716.211817	28.047399
292.428144	12723.440683	28.052416
292.665211	12738.832789	28.057434
292.877267	12757.584020	28.062452
292.997310	12772.051215	28.067469
293.335739	12797.298675	28.072487
293.551415	12819.202044	28.077504
293.600683	12844.078772	28.082522
294.367346	12854.491381	28.087540
294.495216	12873.137804	28.092557
294.833262	12889.104530	28.097575
295.416794	12898.850807	28.102592
295.503021	12915.218114	28.107610
296.020561	12929.978001	28.112628
296.255390	12941.987957	28.117645
296.387234	12956.464861	28.122663
297.115348	12974.737876	28.127680
297.237693	12982.640384	28.132698
297.416921	12985.766488	28.137716
297.365901	12994.843230	28.142733
298.137958	13023.637488	28.147751
298.235388	13037.218946	28.152768
298.315216	13042.317301	28.157786
298.748373	13068.379613	28.162804
298.852017	13079.332169	28.167821
298.998293	13094.151583	28.172839
299.299995	13122.646004	28.177856
299.403578	13144.794509	28.182874
299.703979	13161.077272	28.187892
299.961846	13189.997678	28.192909
300.141350	13219.233493	28.197927
300.916280	13243.083280	28.202944
301.050495	13270.011429	28.207962
301.265752	13282.702039	28.212980
301.380019	13308.400423	28.217997
301.910700	13337.208259	28.223015
302.204093	13359.182867	28.228032
302.125938	13390.250514	28.233050
302.622953	13405.310115	28.238068
302.780983	13433.783046	28.243085
303.192329	13463.311126	28.248103
303.566708	13490.875220	28.253120
304.108196	13522.442741	28.258138
303.965942	13540.224318	28.263156
304.097300	13570.253895	28.268173
304.972542	13592.031707	28.273191
305.699683	13618.635722	28.278208
305.463938	13636.823348	28.283226
306.182599	13657.778599	28.288244
306.466525	13678.692758	28.293261
306.964886	13699.140796	28.298279
307.476127	13723.515324	28.303296
307.786139	13738.217855	28.308314
307.499178	13756.283898	28.313332
308.132601	13766.389226	28.318349
308.807302	13783.040551	28.323367
309.711401	13793.834366	28.328384
309.677704	13794.542732	28.333402
310.313950	13791.135797	28.338420
310.924894	13803.863460	28.343437
311.072582	13806.078753	28.348455
311.435876	13790.026597	28.353472
311.609438	13793.131829	28.358490
311.856283	13791.913186	28.363508
312.118272	13796.739123	28.368525
312.006158	13794.132679	28.373543
312.274757	13807.448727	28.378560
312.060032	13821.528156	28.383578
312.666635	13819.872843	28.388596
312.879557	13841.064519	28.393613
312.869955	13852.761677	28.398631
313.281057	13868.521284	28.403648
313.400861	13885.848583	28.408666
313.682818	13886.332184	28.413684
313.759892	13911.038346	28.418701
314.359606	13939.571621	28.423719
314.519867	13951.734676	28.428736
315.016051	13977.377649	28.433754
315.409473	13982.310916	28.438772
315.643684	14007.646168	28.443789
315.604814	14037.780053	28.448807
316.429125	14047.401419	28.453824
316.577413	14073.390577	28.458842
316.879417	14091.006247	28.463860
317.284015	14119.108069	28.468877
317.445026	14128.906635	28.473895
317.748601	14141.060482	28.478912
317.917351	14174.910293	28.483930
318.183957	14190.648585	28.488948
318.807794	14211.039431	28.493965
319.184079	14245.038958	28.498983
319.535718	14260.865029	28.504000
319.846261	14288.993862	28.509018
320.163094	14299.575499	28.514036
320.445471	14321.034957	28.519053
320.504732	14340.043436	28.524071
321.165860	14360.083534	28.529088
321.188729	14381.182748	28.534106
321.971189	14396.282963	28.539124
321.957899	14421.586113	28.544141
322.265331	14441.484105	28.549159
322.448312	14460.566600	28.554176
322.884715	14499.727387	28.559194
323.147132	14505.789643	28.564212
323.374280	14536.297185	28.569229
323.536708	14556.914159	28.574247
323.757591	14574.709028	28.579264
324.019706	14621.327896	28.584282
324.417152	14646.113392	28.589300
324.624495	14670.854731	28.594317
324.894366	14700.172852	28.599335
325.555388	14722.877100	28.604352
326.066669	14756.555518	28.609370
326.801180	14757.986620	28.614388
327.191840	14791.833523	28.619405
328.228817	14798.278763	28.624423
328.708355	14797.405174	28.629440
328.888980	14814.520842	28.634458
329.582651	14826.650366	28.639476
329.830247	14821.259369	28.644493
329.881201	14821.400458	28.649511
330.216840	14826.351477	28.654528
330.351148	14816.792700	28.659546
330.312036	14810.276061	28.664564
330.690003	14829.441602	28.669581
330.959518	14843.896582	28.674599
330.881207	14839.401455	28.679616
331.011768	14868.217294	28.684634
331.382600	14880.306200	28.689652
331.725203	14898.152015	28.694669
331.817986	14913.882342	28.699687
332.827732	14931.410895	28.704704
332.867141	14955.216044	28.709722
332.953588	14966.356813	28.714740
333.406318	14991.939823	28.719757
333.448027	15017.194547	28.724775
333.779369	15027.434869	28.729792
333.849817	15066.519619	28.734810
334.249892	15087.985407	28.739828
334.437148	15104.319864	28.744845
334.730645	15134.272935	28.749863
335.432662	15168.969723	28.754880
335.894063	15183.278519	28.759898
336.663540	15200.909145	28.764916
337.365658	15214.492516	28.769933
337.385305	15230.608876	28.774951
337.797249	15243.979108	28.779968
338.018427	15268.768116	28.784986
338.259048	15275.820612	28.790004
338.922484	15298.669995	28.795021
338.560020	15313.818164	28.800039
339.113069	15331.178950	28.805056
339.321349	15358.239101	28.810074
339.930173	15378.087919	28.815092
340.132291	15399.061850	28.820109
340.217178	15432.317650	28.825127
340.830686	15439.524154	28.830144
340.932537	15468.053215	28.835162
340.799119	15494.601801	28.840180
341.616234	15517.835428	28.845197
341.793726	15553.915309	28.850215
342.225971	15580.969292	28.855232
342.192800	15601.845382	28.860250
342.356039	15628.675423	28.865268
343.142849	15666.992607	28.870285
343.232668	15691.544207	28.875303
343.954938	15717.838132	28.880320
344.325671	15749.259135	28.885338
344.874779	15778.181809	28.890356
345.417660	15789.396877	28.895373
345.209426	15824.412029	28.900391
345.720887	15840.663816	28.905408
345.645543	15872.377192	28.910426
346.274141	15907.967757	28.915444
346.956915	15928.729216	28.920461
346.893267	15961.231371	28.925479
347.427655	15972.370179	28.930496
347.726765	16004.355220	28.935514
348.039091	16018.167349	28.940532
348.487369	16032.683338	28.945549
348.882320	16056.428904	28.950567
349.007626	16069.176509	28.955584
349.419971	16094.952614	28.960602
350.140810	16105.573670	28.965620
350.833184	16124.776742	28.970637
350.888954	16141.696088	28.975655
351.305746	16159.509995	28.980672
351.573797	16179.334633	28.985690
352.216303	16190.193996	28.990708
352.555967	16209.494714	28.995725
352.202412	16230.831526	29.000743
353.047637	16243.668275	29.005760
353.103078	16266.641574	29.010778
353.542611	16280.242347	29.015796
354.097574	16300.354462	29.020813
354.193135	16329.178807	29.025831
354.923372	16331.770102	29.030848
355.364156	16358.910304	29.035866
355.370551	16372.281977	29.040884
356.009934	16381.115179	29.045901
356.176004	16405.535892	29.050919
356.933289	16422.077246	29.055936
356.691828	16440.155609	29.060954
357.049288	16463.360775	29.065972
357.444702	16472.871242	29.070989
357.433487	16499.967389	29.076007
357.639855	16527.503875	29.081024
358.329752	16557.309251	29.086042
358.335798	16584.168166	29.091060
358.711024	16614.399948	29.096077
358.947441	16651.944161	29.101095
359.562505	16675.437315	29.106112
359.711009	16717.841637	29.111130
359.882133	16753.741095	29.116148
360.302568	16781.505520	29.121165
360.276909	16821.230558	29.126183
360.859662	16856.049954	29.131200
361.579706	16894.504447	29.136218
361.439060	16922.103820	29.141236
361.998398	16957.854295	29.146253
362.610122	16999.388762	29.151271
362.947725	17022.470968	29.156288
363.682346	17043.793954	29.161306
364.147767	17072.528464	29.166324
365.137501	17084.354548	29.171341
365.191795	17110.307902	29.176359
365.783505	17124.185949	29.181376
366.170073	17129.861564	29.186394
366.329254	17155.486088	29.191412
367.296525	17173.602609	29.196429
367.059177	17204.551245	29.201447
367.655678	17204.393623	29.206464
367.882160	17218.759072	29.211482
367.834140	17233.126151	29.216500
368.360954	17252.787316	29.221517
368.192919	17273.126534	29.226535
368.758795	17294.694468	29.231552
369.069944	17315.922715	29.236570
369.269344	17347.258722	29.241588
370.148577	17356.868820	29.246605
370.666222	17375.626111	29.251623
370.987729	17399.679142	29.256640
371.505768	17405.503199	29.261658
371.973072	17433.279042	29.266676
372.375964	17449.424045	29.271693
372.364630	17474.849499	29.276711
372.964635	17484.231734	29.281728
373.382222	17494.778459	29.286746
373.380554	17516.666662	29.291764
373.669329	17537.870433	29.296781
374.122143	17562.928768	29.301799
374.455889	17579.558543	29.306816
374.915408	17604.335958	29.311834
374.940152	17636.809822	29.316852
375.655215	17654.544266	29.321869
375.892890	17688.383518	29.326887
376.292275	17708.009268	29.331904
376.296794	17739.038930	29.336922
376.559861	17766.495944	29.341940
377.191274	17797.437250	29.346957
377.218731	17831.973306	29.351975
377.806181	17864.731214	29.356992
378.176989	17893.722089	29.362010
378.477916	17922.450134	29.367028
379.034358	17958.382911	29.372045
379.422725	17982.375010	29.377063
379.811686	18009.173012	29.382080
380.481115	18034.377124	29.387098
380.637883	18069.856116	29.392116
380.969932	18087.850911	29.397133
381.489927	18117.307421	29.402151
382.010815	18136.157246	29.407168
382.739774	18162.520619	29.412186
382.754338	18180.799975	29.417204
383.364459	18204.549203	29.422221
383.536268	18237.612717	29.427239
384.117895	18258.253862	29.432256
384.881894	18270.424721	29.437274
384.797733	18293.255539	29.442292
385.368919	18310.593569	29.447309
385.710249	18344.167720	29.452327
386.212300	18355.171280	29.457344
386.361113	18374.327148	29.462362
386.569520	18408.723440	29.467380
387.515581	18433.284885	29.472397
387.531597	18451.833631	29.477415
387.804175	18468.620176	29.482432
387.892160	18486.749997	29.487450
388.329216	18514.776702	29.492468
388.416300	18534.269785	29.497485
388.679878	18565.931110	29.502503
389.428450	18602.133991	29.507520
390.146319	18622.527916	29.512538
389.714991	18650.462509	29.517556
390.228108	18674.349179	29.522573
390.934389	18708.604989	29.527591
391.075526	18737.547412	29.532608
391.630165	18750.372917	29.537626
392.231112	18775.125335	29.542644
393.307075	18793.025646	29.547661
393.248333	18813.134086	29.552679
393.663709	18833.918243	29.557696
394.174656	18861.733786	29.562714
394.170320	18885.199648	29.567732
394.451694	18907.196684	29.572749
395.237474	18930.280402	29.577767
395.184240	18950.066068	29.582784
395.765547	18973.740349	29.587802
396.152403	19002.568909	29.592820
396.850939	19031.326206	29.597837
396.850577	19062.967203	29.602855
397.471244	19080.715963	29.607872
398.300217	19108.745865	29.612890
398.291826	19132.183608	29.617908
398.625199	19146.389701	29.622925
399.261594	19168.712858	29.627943
399.345391	19208.013509	29.632960
399.988788	19220.967795	29.637978
400.826786	19236.582690	29.642996
401.359324	19261.354263	29.648013
401.408276	19273.829235	29.653031
401.843255	19286.556916	29.658048
402.324767	19312.727000	29.663066
402.215747	19342.347868	29.668084
402.831765	19354.215964	29.673101
403.306919	19384.469896	29.678119
403.225423	19415.592586	29.683136
403.602380	19437.851155	29.688154
403.764129	19478.794973	29.693172
404.401083	19518.827260	29.698189
404.377516	19555.999971	29.703207
404.961771	19585.764413	29.708224
405.444580	19627.270924	29.713242
405.367815	19659.865966	29.718260
406.353675	19694.702705	29.723277
406.766663	19732.750887	29.728295
406.892431	19770.812243	29.733312
407.402982	19801.158599	29.738330
407.616438	19834.751604	29.743348
408.353745	19869.674798	29.748365
408.459377	19907.384526	29.753383
409.045173	19926.817997	29.758400
409.699354	19954.986736	29.763418
409.728792	19985.305758	29.768436
409.998890	20021.355852	29.773453
410.664588	20054.303960	29.778471
410.801444	20082.979433	29.783488
411.268403	20116.436967	29.788506
411.696840	20138.509169	29.793524
412.725961	20175.773933	29.798541
413.709599	20186.901703	29.803559
414.306606	20197.410658	29.808576
415.189639	20193.698557	29.813594
415.653521	20214.557154	29.818612
416.383968	20222.287730	29.823629
416.742783	20217.769239	29.828647
416.789811	20220.206258	29.833664
417.502952	20223.918474	29.838682
417.251586	20239.558707	29.843700
418.078394	20247.604707	29.848717
417.921351	20257.991283	29.853735
417.827112	20281.867718	29.858752
418.074069	20309.792873	29.863770
418.426122	20335.282028	29.868788
418.908058	20355.348828	29.873805
419.353488	20382.579386	29.878823
419.199298	20417.654899	29.883840
419.652181	20450.879130	29.888858
419.954041	20495.013683	29.893876
420.464674	20525.933975	29.898893
421.029502	20561.786752	29.903911
421.006329	20600.833079	29.908928
421.733425	20637.762743	29.913946
421.743338	20677.300144	29.918964
422.522760	20704.712739	29.923981
423.381355	20749.222386	29.928999
423.766794	20784.030813	29.934016
424.307151	20813.770327	29.939034
424.741861	20841.838989	29.944052
425.265186	20871.460041	29.949069
425.552063	20900.659672	29.954087
425.353231	20935.455988	29.959104
426.520258	20955.317536	29.964122
426.612409	20994.959191	29.969140
427.007495	21032.453811	29.974157
427.531868	21061.736400	29.979175
427.874862	21098.522000	29.984192
428.179653	21132.073692	29.989210
428.402561	21178.565772	29.994228
429.224237	21208.077707	29.999245
429.844551	21235.856813	30.004263
430.545326	21272.614171	30.009280
431.141210	21296.672020	30.014298
431.305390	21322.879481	30.019316
431.635668	21360.426160	30.024333
432.236777	21393.861106	30.029351
432.722387	21405.354208	30.034368
434.225835	21399.002240	30.039386
434.522011	21413.526236	30.044404
434.866803	21412.426200	30.049421
435.390463	21421.229152	30.054439
435.559780	21452.009535	30.059456
435.663167	21448.708839	30.064474
436.016365	21464.510719	30.069492
436.194238	21481.710955	30.074509
436.585310	21503.106615	30.079527
436.752245	21526.384919	30.084544
437.115856	21556.050034	30.089562
437.133451	21596.919551	30.094580
437.669629	21617.640906	30.099597
438.668547	21652.822927	30.104615
438.206276	21679.253648	30.109632
439.014734	21713.450142	30.114650
439.361746	21751.605480	30.119668
439.498226	21785.223970	30.124685
439.842037	21829.466629	30.129703
440.596994	21863.242725	30.134720
440.697174	21903.703709	30.139738
440.998863	21945.707921	30.144756
441.483898	21997.018655	30.149773
442.651654	22021.552016	30.154791
442.849380	22067.342655	30.159808
443.386812	22099.167533	30.164826
444.226541	22141.603228	30.169844
444.878334	22165.019462	30.174861
445.239932	22185.422034	30.179879
445.650318	22222.668155	30.184896
446.302641	22237.265343	30.189914
446.724278	22262.409428	30.194932
446.817403	22304.925912	30.199949
447.418741	22329.479106	30.204967
448.102863	22365.062579	30.209984
448.366447	22393.205375	30.215002
448.941106	22422.379302	30.220020
449.182712	22454.185863	30.225037
449.988186	22465.223149	30.230055
450.862185	22495.937408	30.235072
451.356032	22502.463922	30.240090
451.746773	22539.867510	30.245108
451.813815	22552.135440	30.250125
452.390193	22567.614593	30.255143
452.827084	22595.611993	30.260160
453.245233	22618.047696	30.265178
453.413918	22641.796801	30.270196
453.556318	22663.383303	30.275213
453.924745	22701.263418	30.280231
454.622230	22738.265739	30.285248
454.708168	22770.068590	30.290266
454.704713	22811.349445	30.295284
454.725254	22850.235251	30.300301
455.516363	22899.144260	30.305319
455.919998	22948.524734	30.310336
456.415441	22979.833490	30.315354
457.582657	23001.682530	30.320372
459.013770	23016.438359	30.325389
459.834546	23022.908283	30.330407
459.742664	23041.941197	30.335424
460.832090	23052.636713	30.340442
461.169278	23063.161424	30.345460
461.512419	23077.634573	30.350477
461.969738	23085.226568	30.355495
462.243065	23098.033906	30.360512
462.300572	23117.964687	30.365530
462.865508	23131.705462	30.370548
463.269690	23158.062044	30.375565
463.675054	23169.662168	30.380583
463.752720	23200.425104	30.385600
464.183377	23225.575585	30.390618
464.620533	23256.938285	30.395636
464.750747	23292.686917	30.400653
465.395117	23313.302682	30.405671
465.430896	23355.041856	30.410688
465.829687	23392.666725	30.415706
466.201663	23435.721551	30.420724
466.548245	23477.732123	30.425741
467.225221	23519.976892	30.430759
467.668430	23557.005880	30.435776
468.369223	23598.373511	30.440794
469.009390	23639.587855	30.445812
469.872913	23669.694811	30.450829
470.281820	23696.955026	30.455847
470.471925	23735.221267	30.460864
470.887759	23771.750986	30.465882
471.074701	23803.693414	30.470900
472.055686	23849.147796	30.475917
472.798887	23861.498861	30.480935
473.335183	23903.265289	30.485952
473.701411	23930.978548	30.490970
473.774906	23960.044519	30.495988
474.208441	24004.972927	30.501005
474.518888	24028.892935	30.506023
475.140052	24073.009442	30.511040
475.711941	24104.092402	30.516058
476.347472	24140.037351	30.521076
476.476187	24174.371084	30.526093
477.298020	24215.843137	30.531111
477.204240	24252.558332	30.536128
477.509048	24299.237927	30.541146
478.272171	24334.565889	30.546164
478.411620	24378.579587	30.551181
479.091522	24416.485853	30.556199
479.175219	24463.450862	30.561216
479.486691	24513.012356	30.566234
480.150033	24561.813708	30.571252
480.726965	24608.142847	30.576269
481.309598	24652.013438	30.581287
481.334410	24691.852288	30.586304
482.023678	24742.769111	30.591322
482.615665	24781.122723	30.596340
482.836305	24834.298932	30.601357
483.547706	24875.780051	30.606375
484.324208	24911.891770	30.611392
484.698869	24952.817791	30.616410
484.998886	24985.169172	30.621428
485.926316	25035.963124	30.626445
486.181796	25067.243313	30.631463
486.215809	25122.790668	30.636480
487.257789	25153.211535	30.641498
487.473436	25198.525414	30.646516
488.123236	25249.999217	30.651533
488.670568	25283.791252	30.656551
489.173331	25333.232641	30.661568
489.457871	25370.522718	30.666586
490.606699	25404.624901	30.671604
490.768805	25441.510818	30.676621
491.540295	25482.811415	30.681639
492.355856	25509.230036	30.686656
492.627105	25533.931364	30.691674
493.544352	25566.883582	30.696692
493.873346	25597.983720	30.701709
494.755072	25627.324957	30.706727
495.289827	25646.862235	30.711744
495.985953	25667.738299	30.716762
496.584515	25692.522446	30.721780
496.527498	25716.757186	30.726797
497.135991	25738.235000	30.731815
497.336321	25779.606862	30.736832
497.753884	25813.652300	30.741850
498.436915	25838.946322	30.746868
498.650107	25873.805159	30.751885
498.949882	25905.339903	30.756903
499.471257	25948.881896	30.761920
499.550102	26000.136295	30.766938
499.941381	26033.249674	30.771956
500.591944	26086.136232	30.776973
501.152666	26114.547086	30.781991
501.914811	26158.984075	30.787008
502.190002	26193.188502	30.792026
502.645817	26240.338143	30.797044
502.946209	26297.514951	30.802061
503.573977	26334.311409	30.807079
504.148982	26380.017288	30.812096
504.404881	26431.723071	30.817114
505.029962	26468.893698	30.822132
505.691705	26518.471767	30.827149
506.637382	26546.171311	30.832167
507.094419	26591.495571	30.837184
508.101440	26611.514230	30.842202
508.944789	26629.963599	30.847220
509.287228	26661.140073	30.852237
510.058625	26680.513288	30.857255
510.658363	26693.113162	30.862272
510.970733	26718.581852	30.867290
511.464587	26729.150213	30.872308
511.798956	26754.650121	30.877325
512.276160	26768.210267	30.882343
513.101338	26779.018967	30.887360
513.217003	26804.774390	30.892378
513.750441	26823.333224	30.897396
513.783796	26861.367171	30.902413
514.275178	26890.523150	30.907431
514.890610	26929.414699	30.912448
514.989580	26956.373720	30.917466
515.572475	26990.204653	30.922484
515.889499	27035.821914	30.927501
516.883145	27063.851920	30.932519
517.491344	27089.627040	30.937536
517.831928	27129.826590	30.942554
518.484595	27150.629572	30.947572
518.718847	27189.464283	30.952589
519.364876	27224.656549	30.957607
520.019633	27257.750177	30.962624
520.174638	27298.044311	30.967642
520.672617	27327.743666	30.972660
520.828598	27369.649823	30.977677
521.722584	27401.082605	30.982695
522.369688	27448.878165	30.987712
522.872533	27493.460203	30.992730
523.463366	27528.910897	30.997748
523.376288	27575.820002	31.002765
523.894950	27614.359882	31.007783
524.594219	27660.362393	31.012800
525.096985	27709.402950	31.017818
525.599421	27757.710961	31.022836
526.116326	27804.488282	31.027853
526.880108	27849.143196	31.032871
527.648866	27888.735930	31.037888
527.772219	27939.935024	31.042906
528.310999	27971.497983	31.047924
528.963255	28018.336305	31.052941
529.350835	28068.932727	31.057959
529.765496	28116.806677	31.062976
530.337460	28163.595175	31.067994
531.105267	28201.573590	31.073012
531.706268	28261.835936	31.078029
532.361110	28293.043805	31.083047
533.284022	28332.669802	31.088064
533.234579	28376.305323	31.093082
534.207215	28408.567475	31.098100
534.350408	28443.927582	31.103117
534.647497	28492.639242	31.108135
535.607714	28529.522492	31.113152
535.855430	28578.284821	31.118170
536.231114	28616.046158	31.123188
536.910402	28655.354023	31.128205
538.067804	28695.023929	31.133223
538.674802	28730.804042	31.138240
539.095381	28765.433577	31.143258
539.496530	28789.342279	31.148276
539.748291	28814.069065	31.153293
540.234879	28859.910292	31.158311
541.118292	28889.031073	31.163328
541.650985	28918.781399	31.168346
541.881359	28955.528142	31.173364
542.559667	28993.894585	31.178381
543.125233	29026.987127	31.183399
543.515380	29065.112818	31.188416
544.165084	29102.960868	31.193434
544.596072	29139.148136	31.198452
545.274951	29180.997745	31.203469
545.640665	29222.167678	31.208487
546.224605	29257.100038	31.213504
546.410608	29309.185445	31.218522
547.245894	29348.878314	31.223540
547.585227	29402.222424	31.228557
548.066383	29445.218406	31.233575
548.361223	29482.559663	31.238592
548.606625	29539.811820	31.243610
549.554925	29590.585279	31.248628
550.206051	29635.595582	31.253645
550.596378	29685.840421	31.258663
551.386191	29735.771206	31.263680
551.660983	29783.725920	31.268698
552.404892	29823.502267	31.273716
552.540893	29879.680871	31.278733
553.577810	29934.034577	31.283751
554.507559	29959.827671	31.288768
554.960285	30003.300879	31.293786
556.183278	30039.003096	31.298804
557.343266	30065.746278	31.303821
558.619927	30090.615941	31.308839
559.218594	30111.358838	31.313856
559.677334	30119.790047	31.318874
560.379776	30140.273745	31.323892
560.636253	30169.042776	31.328909
560.892744	30174.926259	31.333927
561.545968	30196.451745	31.338944
561.761109	30227.292069	31.343962
562.204224	30245.814057	31.348980
562.471049	30276.832216	31.353997
562.931501	30306.788862	31.359015
563.232121	30348.403839	31.364032
563.220401	30391.113590	31.369050
564.004528	30430.000847	31.374068
563.851377	30488.621623	31.379085
564.327075	30541.218014	31.384103
565.361949	30582.124043	31.389120
565.603824	30655.281667	31.394138
566.057244	30702.707855	31.399156
566.919703	30766.316940	31.404173
567.012114	30816.262804	31.409191
567.456660	30860.456715	31.414208
567.892248	30918.225579	31.419226
568.533496	30957.950114	31.424244
568.935916	31019.010802	31.429261
569.684915	31075.948553	31.434279
570.855629	31114.437002	31.439296
571.563425	31160.274671	31.444314
572.354942	31203.495364	31.449332
573.109724	31241.813934	31.454349
573.577527	31284.794811	31.459367
574.327645	31325.246836	31.464384
574.504379	31379.702938	31.469402
575.309697	31423.054409	31.474420
575.554748	31459.293760	31.479437
575.796380	31509.367697	31.484455
576.624339	31548.094588	31.489472
576.802754	31605.572677	31.494490
577.646102	31646.950044	31.499508
578.541809	31702.952424	31.504525
579.020946	31757.840774	31.509543
579.548740	31798.345133	31.514560
580.064144	31855.772002	31.519578
580.600273	31897.870387	31.524596
581.113409	31960.594010	31.529613
581.621805	32010.724710	31.534631
582.729171	32048.936998	31.539648
582.964995	32107.834166	31.544666
583.242487	32162.316209	31.549684
584.192579	32216.948243	31.554701
584.617173	32263.652151	31.559719
585.409983	32319.871621	31.564736
585.610269	32380.083696	31.569754
586.317634	32429.173609	31.574772
587.391840	32488.020580	31.579789
587.853515	32533.570256	31.584807
588.301009	32585.772572	31.589824
588.958509	32642.446585	31.594842
589.280121	32699.331912	31.599860
589.906180	32751.728569	31.604877
590.330108	32814.305705	31.609895
591.172246	32857.035606	31.614912
591.152896	32927.382363	31.619930
592.113945	32980.337999	31.624948
592.776659	33045.214059	31.629965
593.346827	33107.526262	31.634983
594.227242	33164.614237	31.640000
594.446185	33225.635064	31.645018
595.287915	33280.152307	31.650036
595.843768	33332.027605	31.655053
596.412204	33390.185928	31.660071
596.670061	33441.705481	31.665088
597.377680	33510.286926	31.670106
598.294742	33563.199412	31.675124
599.054261	33618.684557	31.680141
599.551280	33676.893090	31.685159
600.124000	33708.805351	31.690176
601.263252	33748.403707	31.695194
601.715641	33795.120117	31.700212
602.447560	33840.526308	31.705229
602.918544	33885.039379	31.710247
603.928620	33911.448578	31.715264
604.297689	33960.164972	31.720282
604.714434	33993.521374	31.725300
605.328871	34032.116270	31.730317
605.912100	34087.709877	31.735335
606.696859	34116.767390	31.740352
607.200826	34173.769028	31.745370
607.470561	34215.983517	31.750388
608.178415	34268.846443	31.755405
608.498303	34316.677879	31.760423
609.171971	34363.854071	31.765440
609.533227	34415.777929	31.770458
610.242331	34470.474693	31.775476
610.834971	34525.445567	31.780493
611.462376	34579.676459	31.785511
611.877576	34630.247680	31.790528
612.565104	34688.598095	31.795546
613.304246	34744.176947	31.800564
613.852653	34803.128480	31.805581
614.608480	34864.350429	31.810599
615.354325	34914.119453	31.815616
616.024510	34975.900912	31.820634
616.547224	35020.013079	31.825652
617.235413	35090.385566	31.830669
617.676205	35152.907328	31.835687
618.525358	35198.267025	31.840704
619.158067	35255.032720	31.845722
620.423283	35279.618856	31.850740
621.533828	35319.088376	31.855757
621.557217	35363.638833	31.860775
622.498177	35410.285123	31.865792
622.917148	35458.291658	31.870810
623.081937	35500.669569	31.875828
624.151523	35547.823901	31.880845
624.298451	35601.191848	31.885863
625.179519	35646.489349	31.890880
625.921355	35697.480023	31.895898
626.357350	35746.914612	31.900916
626.771611	35797.749646	31.905933
627.401192	35850.660001	31.910951
628.366463	35889.597474	31.915968
628.968542	35944.000791	31.920986
629.233987	35987.842738	31.926004
630.113707	36035.233635	31.931021
630.479429	36102.128587	31.936039
631.302026	36150.137472	31.941056
631.510799	36205.036252	31.946074
631.854271	36262.986576	31.951092
632.277271	36329.668353	31.956109
632.544382	36396.349991	31.961127
633.497294	36454.073070	31.966144
634.263632	36506.968447	31.971162
634.445099	36566.150160	31.976180
635.356663	36616.671988	31.981197
635.895757	36688.028792	31.986215
636.851920	36745.810692	31.991232
637.226632	36797.880111	31.996250
637.830202	36855.035836	32.001268
638.630317	36914.303156	32.006285
638.937615	36985.043808	32.011303
639.787368	37037.132925	32.016320
640.638994	37104.323430	32.021338
641.051938	37164.648172	32.026356
642.031785	37211.958649	32.031373
642.514933	37286.502367	32.036391
643.465902	37334.916753	32.041408
644.155282	37395.672894	32.046426
644.881558	37443.820641	32.051444
646.037128	37503.202144	32.056461
646.683197	37549.213885	32.061479
647.455452	37584.608425	32.066496
647.955432	37646.669629	32.071514
648.619485	37697.603072	32.076532
649.426694	37740.660086	32.081549
649.963794	37794.108451	32.086567
650.246736	37849.234130	32.091584
650.869960	37896.497672	32.096602
651.146194	37954.987999	32.101620
652.069060	38017.013185	32.106637
652.613674	38067.752320	32.111655
653.463336	38127.537927	32.116672
654.248219	38182.824441	32.121690
654.984617	38239.222612	32.126708
655.896785	38290.288628	32.131725
656.022637	38352.776232	32.136743
656.518656	38396.154099	32.141760
658.004545	38449.349394	32.146778
658.934444	38496.466443	32.151796
659.890659	38537.116035	32.156813
660.418394	38578.847849	32.161831
661.458734	38619.454285	32.166848
662.159465	38663.164491	32.171866
662.367719	38707.804715	32.176884
662.856882	38734.397524	32.181901
663.775907	38772.067067	32.186919
664.505569	38805.976101	32.191936
665.251954	38850.425370	32.196954
665.689761	38893.616674	32.201972
666.156447	38938.820293	32.206989
666.720193	38981.692165	32.212007
667.044062	39028.676966	32.217024
667.745304	39080.318239	32.222042
668.137857	39133.949955	32.227060
668.849470	39190.296892	32.232077
669.134302	39248.813960	32.237095
669.618676	39301.873367	32.242112
670.149589	39359.880144	32.247130
670.915205	39421.631168	32.252148
671.400234	39471.235999	32.257165
672.014579	39543.862267	32.262183
672.351277	39602.356522	32.267200
673.312349	39655.593438	32.272218
673.615279	39728.145496	32.277236
674.234864	39790.376840	32.282253
675.155639	39847.167307	32.287271
675.878151	39921.698679	32.292288
676.577480	39986.829095	32.297306
676.944412	40060.149812	32.302324
678.172846	40108.540568	32.307341
678.892791	40180.184472	32.312359
679.832096	40234.929522	32.317376
680.643001	40286.295212	32.322394
681.077822	40367.494516	32.327412
681.640805	40414.717882	32.332429
682.386907	40492.534449	32.337447
683.015889	40555.438887	32.342464
683.657953	40625.125793	32.347482
684.224927	40689.825779	32.352500
684.580363	40745.343542	32.357517
685.039445	40823.828659	32.362535
686.154801	40893.971188	32.367552
687.155005	40957.357347	32.372570
687.774610	41028.320567	32.377588
688.559200	41091.798325	32.382605
689.597216	41163.493481	32.387623
690.012977	41218.567901	32.392640
690.750009	41295.358153	32.397658
691.086058	41362.958260	32.402676
691.820005	41429.586881	32.407693
692.744497	41505.685849	32.412711
693.381167	41564.445000	32.417728
694.408794	41620.391634	32.422746
694.656523	41692.536549	32.427764
695.771422	41756.695958	32.432781
695.994117	41830.895693	32.437799
696.658309	41906.132605	32.442816
697.298229	41975.465745	32.447834
698.256615	42046.669425	32.452852
698.584517	42112.419047	32.457869
699.546647	42190.956485	32.462887
700.468984	42257.416373	32.467904
701.774959	42308.062663	32.472922
702.192267	42370.755099	32.477940
702.802743	42437.725868	32.482957
703.712020	42499.883067	32.487975
704.364597	42561.229672	32.492992
705.254282	42616.586402	32.498010
705.834875	42685.550160	32.503028
707.056153	42727.880381	32.508045
707.649470	42781.909499	32.513063
708.460071	42834.008379	32.518080
709.247949	42872.903378	32.523098
709.265866	42929.510263	32.528116
710.046997	42973.687119	32.533133
710.363860	43022.183914	32.538151
711.037522	43080.096944	32.543168
711.900320	43144.090305	32.548186
712.073533	43211.644713	32.553204
712.918611	43272.799164	32.558221
713.638654	43351.408810	32.563239
714.008232	43427.705546	32.568256
714.838755	43489.897770	32.573274
714.807510	43565.312554	32.578292
715.557062	43639.445630	32.583309
716.424798	43725.083948	32.588327
716.749982	43808.641842	32.593344
717.305852	43894.112973	32.598362
718.029953	43980.844836	32.603380
719.003631	44073.051743	32.608397
719.525333	44157.097389	32.613415
720.273396	44255.805113	32.618432
721.639217	44323.126657	32.623450
722.319499	44401.422448	32.628468
723.400991	44480.683162	32.633485
724.386185	44560.454864	32.638503
725.087915	44638.451759	32.643520
726.109386	44715.256073	32.648538
726.454489	44788.477296	32.653556
727.448921	44872.851795	32.658573
728.046045	44938.588190	32.663591
728.128640	45017.871554	32.668608
729.178358	45088.423296	32.673626
729.922034	45171.592994	32.678644
730.501460	45250.549086	32.683661
731.162097	45339.503065	32.688679
732.209705	45421.335218	32.693696
732.852312	45497.398784	32.698714
733.132163	45589.692611	32.703732
734.056927	45665.847653	32.708749
734.877598	45751.216312	32.713767
735.760812	45841.459336	32.718784
737.268769	45898.507506	32.723802
738.218830	45977.221728	32.728820
738.825521	46042.156219	32.733837
739.625225	46117.260428	32.738855
740.480004	46181.947712	32.743872
740.966805	46249.706886	32.748890
741.850636	46318.658835	32.753908
742.894605	46381.385838	32.758925
743.528131	46443.446423	32.763943
743.881568	46520.828805	32.768960
744.776687	46586.943575	32.773978
745.539066	46658.629589	32.778996
746.103660	46721.184862	32.784013
747.261657	46799.330141	32.789031
747.641937	46860.195691	32.794048
748.532152	46912.738968	32.799066
749.004754	46977.307018	32.804084
749.813775	47033.441558	32.809101
750.392194	47096.740589	32.814119
751.014338	47158.158689	32.819136
752.086346	47215.649707	32.824154
753.036653	47271.263990	32.829172
753.898959	47343.252409	32.834189
754.646586	47392.194437	32.839207
755.287478	47456.182126	32.844224
755.944866	47506.322061	32.849242
756.529792	47580.848272	32.854260
757.206530	47648.718270	32.859277
758.186751	47713.530051	32.864295
758.312431	47786.997476	32.869312
759.387973	47850.368378	32.874330
760.113544	47927.827060	32.879348
760.853041	47997.808804	32.884365
761.519084	48072.633400	32.889383
762.343745	48142.949254	32.894400
763.185832	48212.246573	32.899418
764.049301	48280.723508	32.904436
765.228867	48345.007317	32.909453
766.276100	48414.222286	32.914471
766.719273	48487.585278	32.919488
767.510225	48545.273672	32.924506
768.411951	48616.487912	32.929524
768.857782	48688.311439	32.934541
769.758076	48762.947042	32.939559
770.039165	48836.797979	32.944576
770.524793	48905.277514	32.949594
771.172516	48996.180018	32.954612
772.148749	49071.533760	32.959629
773.045587	49149.585848	32.964647
773.286749	49230.712049	32.969664
774.372559	49317.715586	32.974682
775.466128	49391.120779	32.979700
776.459800	49462.386885	32.984717
777.529431	49538.043299	32.989735
778.484013	49615.324574	32.994752
779.183801	49684.975322	32.999770
779.975406	49760.364525	33.004788
780.634275	49831.360364	33.009805
781.184578	49899.719822	33.014823
782.025426	49971.706544	33.019840
782.568557	50048.465069	33.024858
783.539855	50129.573809	33.029876
784.044948	50198.976690	33.034893
784.961493	50280.729137	33.039911
785.030092	50359.022490	33.044928
786.249568	50437.420177	33.049946
787.014272	50522.066514	33.054964
787.553635	50604.568443	33.059981
788.848903	50681.456119	33.064999
789.235846	50752.855507	33.070016
790.333779	50830.368533	33.075034
791.113377	50901.153737	33.080052
791.623459	50964.284906	33.085069
792.653971	51041.216268	33.090087
793.106733	51113.199922	33.095104
793.997725	51186.720481	33.100122
794.552908	51266.969605	33.105140
795.252155	51354.912469	33.110157
795.823424	51434.323450	33.115175
796.220149	51529.321574	33.120192
797.158158	51612.739882	33.125210
798.129956	51712.457188	33.130228
798.555012	51802.307931	33.135245
799.699101	51894.212883	33.140263
800.341546	51987.779338	33.145280
801.368920	52077.005362	33.150298
802.971851	52154.156518	33.155316
803.870564	52233.421065	33.160333
805.358503	52300.965020	33.165351
806.250589	52369.244761	33.170368
807.211938	52420.511586	33.175386
808.785905	52480.979079	33.180404
809.614218	52538.806967	33.185421
810.319283	52590.822049	33.190439
810.707443	52647.483120	33.195456
811.712278	52698.541819	33.200474
812.633730	52763.261351	33.205492
813.452451	52817.705055	33.210509
813.804217	52888.657696	33.215527
814.414006	52955.037192	33.220544
815.186599	53022.423114	33.225562
816.159684	53080.775726	33.230580
816.789713	53157.372709	33.235597
817.449456	53221.772563	33.240615
817.842689	53304.218571	33.245632
818.962273	53366.642506	33.250650
819.132410	53450.892220	33.255668
819.881095	53537.209178	33.260685
821.134894	53614.889286	33.265703
822.110532	53694.211118	33.270720
823.168047	53769.618983	33.275738
823.763655	53844.551463	33.280756
824.469071	53930.832989	33.285773
825.171937	54012.933072	33.290791
825.578163	54094.310567	33.295808
827.274746	54175.546190	33.300826
827.775607	54251.019393	33.305844
828.397280	54343.464988	33.310861
829.327834	54409.442066	33.315879
830.125691	54491.945847	33.320896
831.123580	54576.675075	33.325914
831.546279	54660.991194	33.330932
832.115426	54756.262865	33.335949
833.006419	54832.061479	33.340967
833.687281	54918.471534	33.345984
834.631275	54998.204966	33.351002
836.091060	55074.267602	33.356020
836.080090	55163.576199	33.361037
837.139129	55231.281411	33.366055
837.742149	55308.093759	33.371072
838.334067	55393.061840	33.376090
839.459698	55488.712789	33.381108
839.973523	55579.922284	33.386125
840.706657	55660.888547	33.391143
841.676970	55764.615251	33.396160
841.917960	55846.853898	33.401178
843.310433	55942.044899	33.406196
844.466139	56027.497565	33.411213
845.844524	56112.489027	33.416231
846.560141	56204.566035	33.421248
848.067157	56273.687502	33.426266
849.233038	56346.885310	33.431284
849.992060	56418.440311	33.436301
851.049530	56469.498058	33.441319
852.108537	56541.776069	33.446336
852.818986	56610.769869	33.451354
853.322713	56688.876011	33.456372
854.139548	56764.539729	33.461389
854.843434	56845.354863	33.466407
855.461418	56919.447153	33.471424
856.173848	57016.437738	33.476442
856.842608	57090.412142	33.481460
857.341261	57183.665071	33.486477
858.081477	57266.446212	33.491495
858.929313	57369.513227	33.496512
859.525830	57463.156086	33.501530
860.459061	57566.308475	33.506548
861.000371	57678.571908	33.511565
861.652475	57777.823902	33.516583
862.742508	57888.088098	33.521600
863.467197	57994.445770	33.526618
864.266982	58110.291877	33.531636
865.448126	58218.819752	33.536653
866.168078	58331.140788	33.541671
867.001854	58446.926757	33.546688
867.722321	58542.995838	33.551706
868.682741	58649.648094	33.556724
869.357709	58769.452059	33.561741
870.369885	58879.472479	33.566759
871.573458	58986.937274	33.571776
871.984394	59101.070727	33.576794
873.166814	59208.398087	33.581812
873.818295	59319.845617	33.586829
875.448542	59415.843884	33.591847
875.863940	59526.335652	33.596864
877.126420	59646.844254	33.601882
878.106132	59739.866104	33.606900
878.794852	59853.164280	33.611917
879.841976	59943.805197	33.616935
880.748345	60040.193405	33.621952
882.070759	60125.723693	33.626970
882.976945	60213.120369	33.631988
883.493155	60293.573036	33.637005
884.318241	60371.908731	33.642023
885.029942	60460.354224	33.647040
886.361952	60557.432007	33.652058
887.682985	60629.655813	33.657076
888.327883	60718.981480	33.662093
889.387316	60795.431322	33.667111
890.179179	60893.187262	33.672128
890.998015	60977.961654	33.677146
891.934568	61065.913207	33.682164
892.379449	61165.282480	33.687181
893.663014	61247.284356	33.692199
894.172943	61348.475681	33.697216
894.890955	61436.738459	33.702234
895.945527	61531.790826	33.707252
896.211466	61639.609495	33.712269
897.026385	61736.576711	33.717287
898.279385	61849.471877	33.722304
899.175901	61950.462814	33.727322
900.310863	62056.358282	33.732340
900.747734	62162.337004	33.737357
902.234042	62260.093731	33.742375
902.955520	62368.582997	33.747392
903.692759	62473.025163	33.752410
904.781459	62574.105687	33.757428
905.863826	62676.122494	33.762445
907.235976	62770.963189	33.767463
907.989622	62867.317524	33.772480
908.882909	62957.817420	33.777498
910.335221	63044.644523	33.782516
910.774934	63153.811543	33.787533
911.826276	63243.428683	33.792551
912.981844	63348.642809	33.797568
913.449800	63448.494084	33.802586
914.732968	63538.239943	33.807604
915.105718	63647.887837	33.812621
915.623220	63740.845053	33.817639
916.502964	63853.189395	33.822656
917.552781	63960.062770	33.827674
918.440669	64064.426539	33.832692
919.261427	64181.279359	33.837709
920.325226	64291.171542	33.842727
920.998475	64394.200623	33.847744
921.376473	64517.000144	33.852762
922.485761	64631.122179	33.857780
923.842630	64753.732726	33.862797
924.982585	64851.169418	33.867815
925.950650	64954.978909	33.872832
926.976319	65064.480498	33.877850
928.182221	65159.337421	33.882868
929.041063	65277.460502	33.887885
930.202526	65374.609025	33.892903
930.858517	65464.207892	33.897920
931.361092	65568.113711	33.902938
932.729646	65659.533033	33.907956
933.354009	65759.270394	33.912973
934.332290	65844.603293	33.917991
934.938593	65948.166183	33.923008
935.860181	66051.862654	33.928026
936.781459	66145.503192	33.933044
937.617146	66258.519269	33.938061
938.849181	66352.983111	33.943079
940.615861	66438.152139	33.948096
941.688618	66533.513957	33.953114
942.817439	66602.822028	33.958132
943.868751	66707.771116	33.963149
944.432846	66791.067347	33.968167
945.183635	66890.240844	33.973184
946.128556	66975.435598	33.978202
947.067383	67069.254703	33.983220
947.633579	67184.719612	33.988237
948.300801	67289.057012	33.993255
949.401373	67382.043282	33.998272
949.842408	67499.355681	34.003290
951.070202	67599.808829	34.008308
951.654779	67718.445316	34.013325
952.549746	67837.254255	34.018343
953.607956	67954.193234	34.023360
953.934340	68068.589661	34.028378
955.532660	68182.923383	34.033396
956.271844	68312.184017	34.038413
957.394963	68433.101965	34.043431
958.655013	68559.798529	34.048448
959.132613	68671.975871	34.053466
960.469439	68786.512679	34.058484
961.611322	68904.473840	34.063501
962.581993	69002.296372	34.068519
964.240069	69114.282124	34.073536
964.896516	69227.647231	34.078554
966.208846	69320.501657	34.083572
967.014447	69434.160126	34.088589
967.985782	69539.718455	34.093607
969.611106	69639.442832	34.098624
970.394505	69746.479006	34.103642
971.464485	69835.280308	34.108660
972.760153	69941.705327	34.113677
973.728460	70024.022283	34.118695
975.076918	70111.251532	34.123712
975.773026	70207.392568	34.128730
977.352212	70284.179749	34.133748
978.109968	70378.688022	34.138765
979.107592	70462.524858	34.143783
980.259064	70538.938797	34.148800
980.700672	70651.227945	34.153818
981.931623	70721.937093	34.158836
982.650227	70809.471830	34.163853
983.572253	70897.549572	34.168871
984.402736	70978.022180	34.173888
985.043458	71057.103640	34.178906
986.548297	71135.732021	34.183924
986.979160	71226.517876	34.188941
987.752408	71331.744528	34.193959
988.508585	71422.542715	34.198976
989.246993	71523.529813	34.203994
990.062423	71621.908193	34.209012
990.914943	71722.998209	34.214029
991.554582	71836.014498	34.219047
992.200678	71946.692450	34.224064
992.877243	72067.634264	34.229082
993.799861	72192.133106	34.234100
994.517501	72315.957617	34.239117
995.639486	72449.045340	34.244135
996.609132	72594.088446	34.249152
997.224795	72728.598208	34.254170
998.158886	72875.449940	34.259188
999.145987	73014.540748	34.264205
1000.595666	73142.279219	34.269223
1001.642132	73280.743158	34.274240
1002.202625	73421.377036	34.279258
1004.071351	73551.692912	34.284276
1006.357031	73655.509537	34.289293
1008.323695	73746.043602	34.294311
1009.594911	73844.208778	34.299328
1010.339812	73956.019640	34.304346
1011.447142	74052.000107	34.309364
1012.223873	74155.288392	34.314381
1013.326103	74256.541101	34.319399
1013.859770	74357.290726	34.324416
1015.155763	74470.091108	34.329434
1016.237237	74560.662235	34.334452
1016.850400	74672.453800	34.339469
1018.000879	74782.523715	34.344487
1019.084507	74882.272129	34.349504
1020.290229	74980.611271	34.354522
1021.659289	75080.169908	34.359540
1022.024582	75183.680591	34.364557
1023.080680	75279.302194	34.369575
1024.836076	75382.719171	34.374592
1025.370807	75485.035269	34.379610
1026.272744	75595.351391	34.384628
1027.489727	75702.780334	34.389645
1028.194785	75795.742633	34.394663
1029.824788	75899.472923	34.399680
1030.768631	76007.123890	34.404698
1031.800794	76099.428825	34.409716
1032.661914	76206.537841	34.414733
1033.253867	76317.722501	34.419751
1034.564285	76420.134817	34.424768
1034.839005	76539.378837	34.429786
1035.859085	76658.726203	34.434804
1036.795148	76775.755440	34.439821
1037.793591	76890.076643	34.444839
1038.911834	76995.322335	34.449856
1040.061005	77113.887071	34.454874
1040.327767	77215.439171	34.459892
1041.815480	77324.110355	34.464909
1042.485655	77437.178502	34.469927
1043.787711	77547.447893	34.474944
1044.572969	77675.346012	34.479962
1045.833625	77778.904460	34.484980
1046.847069	77887.976435	34.489997
1047.977316	78013.615888	34.495015
1049.031594	78125.356283	34.500032
1050.079236	78240.960324	34.505050
1050.932749	78361.033092	34.510068
1052.050379	78484.755917	34.515085
1052.860413	78614.899850	34.520103
1054.262746	78725.374544	34.525120
1054.814472	78867.280122	34.530138
1055.908246	78986.262727	34.535156
1057.330938	79108.746117	34.540173
1057.884950	79245.970060	34.545191
1058.974958	79380.625467	34.550208
1060.212142	79524.310227	34.555226
1060.845844	79653.717584	34.560244
1061.887316	79792.473204	34.565261
1062.609609	79937.791435	34.570279
1063.631633	80071.918527	34.575296
1064.664578	80232.935823	34.580314
1065.752669	80382.377411	34.585332
1066.755759	80529.102726	34.590349
1067.984260	80681.722794	34.595367
1069.080731	80834.643130	34.600384
1070.013205	80987.280915	34.605402
1071.555393	81129.347887	34.610420
1072.995488	81270.407954	34.615437
1073.842241	81424.548171	34.620455
1075.090615	81569.503331	34.625472
1076.142519	81720.559689	34.630490
1077.267745	81866.630171	34.635508
1078.409966	82006.200053	34.640525
1079.274068	82142.799531	34.645543
1080.465162	82285.284239	34.650560
1081.579049	82433.705938	34.655578
1083.275686	82575.890946	34.660596
1084.764451	82711.667742	34.665613
1085.280222	82838.167512	34.670631
1086.620571	82968.658966	34.675648
1087.372627	83118.135632	34.680666
1088.524331	83264.578324	34.685684
1089.765877	83397.149213	34.690701
1090.879863	83542.449172	34.695719
1091.907872	83672.836606	34.700736
1093.419121	83795.801313	34.705754
1094.619267	83927.263046	34.710772
1095.901585	84052.756717	34.715789
1097.147447	84183.865037	34.720807
1098.478776	84290.365696	34.725824
1099.121225	84407.459356	34.730842
1099.843273	84516.270968	34.735860
1101.052820	84627.376615	34.740877
1101.785217	84755.276010	34.745895
1102.974045	84876.704949	34.750912
1103.939235	84999.415741	34.755930
1104.887935	85122.920217	34.760948
1106.541700	85251.112340	34.765965
1107.167097	85382.940062	34.770983
1108.181519	85506.196038	34.776000
1108.984744	85648.480570	34.781018
1109.958077	85777.542832	34.786036
1110.842841	85914.213964	34.791053
1111.693630	86056.449386	34.796071
1112.695329	86216.417176	34.801088
1113.864088	86374.001037	34.806106
1115.062798	86522.216560	34.811124
1116.001598	86674.508702	34.816141
1116.716628	86834.450811	34.821159
1117.880942	86988.277501	34.826176
1119.149967	87157.245910	34.831194
1120.515721	87316.835183	34.836212
1121.762684	87474.585413	34.841229
1122.626433	87637.646306	34.846247
1123.984231	87797.556582	34.851264
1125.658882	87944.763997	34.856282
1127.754049	88080.491252	34.861300
1129.323268	88208.765098	34.866317
1130.508481	88347.870173	34.871335
1131.532073	88463.736508	34.876352
1132.583196	88602.453493	34.881370
1133.605024	88739.019575	34.886388
1135.144003	88871.014283	34.891405
1135.962369	89008.638893	34.896423
1137.185262	89140.407249	34.901440
1138.494762	89283.115891	34.906458
1139.318783	89419.034704	34.911476
1140.220048	89544.070896	34.916493
1141.191291	89694.684272	34.921511
1142.505207	89827.043104	34.926528
1143.623021	89976.591623	34.931546
1143.912096	90121.087025	34.936564
1145.154912	90269.346483	34.941581
1146.272150	90425.393259	34.946599
1147.665501	90579.012929	34.951616
1148.939255	90722.046554	34.956634
1150.331367	90878.830758	34.961652
1151.467257	91016.000098	34.966669
1152.513301	91174.473178	34.971687
1153.562628	91318.052339	34.976704
1154.866606	91463.185764	34.981722
1155.799639	91613.521133	34.986740
1157.163786	91755.680619	34.991757
1158.095291	91908.978235	34.996775
1159.127457	92048.213409	35.001792
1160.534750	92190.242336	35.006810
1161.739187	92335.447924	35.011828
1162.526686	92454.314009	35.016845
1163.337355	92605.750825	35.021863
1164.694059	92738.828779	35.026880
1165.642046	92888.974358	35.031898
1166.551861	93039.228223	35.036916
1168.199067	93189.776988	35.041933
1168.985037	93348.275363	35.046951
1170.448748	93488.191005	35.051968
1171.442337	93632.021737	35.056986
1172.744655	93787.411312	35.062004
1174.245310	93927.298535	35.067021
1175.728295	94089.018496	35.072039
1176.700121	94222.425859	35.077056
1178.263311	94366.980414	35.082074
1179.099064	94513.485978	35.087092
1180.509793	94656.244884	35.092109
1181.191325	94809.184725	35.097127
1182.068883	94960.683812	35.102144
1183.170907	95129.126464	35.107162
1184.190946	95288.303508	35.112180
1185.818728	95441.318592	35.117197
1186.691532	95619.321704	35.122215
1188.116636	95770.239432	35.127232
1189.605801	95936.513711	35.132250
1190.817517	96094.103456	35.137268
1192.113971	96248.758196	35.142285
1193.287000	96404.768420	35.147303
1194.912265	96557.430882	35.152320
1196.564589	96712.595233	35.157338
1197.169004	96876.334793	35.162356
1198.659590	97014.541052	35.167373
1199.801243	97171.611694	35.172391
1200.899673	97325.875073	35.177408
1202.032748	97477.344055	35.182426
1203.343213	97630.202957	35.187444
1204.453124	97782.025598	35.192461
1206.018494	97936.851515	35.197479
1206.618881	98096.836208	35.202496
1208.054744	98253.538539	35.207514
1208.918193	98419.266165	35.212532
1210.490958	98566.079315	35.217549
1211.906599	98720.573718	35.222567
1212.923138	98873.626846	35.227584
1214.446325	99033.528294	35.232602
1215.655972	99184.072678	35.237620
1216.778069	99341.205605	35.242637
1217.923048	99500.328950	35.247655
1219.303553	99656.638404	35.252672
1220.474219	99811.659930	35.257690
1221.128475	99975.856591	35.262708
1222.810070	100124.471920	35.267725
1223.802204	100276.753675	35.272743
1224.950871	100426.044093	35.277760
1226.115053	100572.340226	35.282778
1227.381028	100718.462917	35.287796
1228.659747	100864.552865	35.292813
1229.395587	101019.499744	35.297831
1230.697726	101161.816735	35.302848
1232.175511	101303.258797	35.307866
1233.052330	101463.286121	35.312884
1234.581712	101615.421628	35.317901
1235.769830	101769.694147	35.322919
1237.222295	101923.501710	35.327936
1238.589908	102062.403213	35.332954
1239.944160	102222.815424	35.337972
1241.146096	102369.275022	35.342989
1242.372719	102519.971206	35.348007
1243.469028	102676.795398	35.353024
1244.391310	102836.400913	35.358042
1245.232396	103003.493649	35.363060
1246.973307	103159.022609	35.368077
1247.933919	103327.686951	35.373095
1248.906728	103496.521416	35.378112
1250.472793	103661.712733	35.383130
1251.707711	103838.500315	35.388148
1252.930142	104010.621025	35.393165
1253.975260	104194.832725	35.398183
1255.239142	104348.293761	35.403200
1256.967191	104515.446024	35.408218
1258.534938	104686.320695	35.413236
1259.944964	104847.058292	35.418253
1261.252171	105018.843758	35.423271
1262.320063	105177.359741	35.428288
1263.671608	105342.894300	35.433306
1265.108922	105512.080605	35.438324
1266.402027	105675.494037	35.443341
1267.298371	105835.528878	35.448359
1268.808334	106007.789187	35.453376
1270.133525	106171.732514	35.458394
1270.797005	106343.515910	35.463412
1272.732714	106518.844953	35.468429
1273.792454	106692.352576	35.473447
1274.871931	106850.884116	35.478464
1276.281200	107022.996830	35.483482
1277.551047	107196.354432	35.488500
1279.257370	107355.264317	35.493517
1280.749413	107522.589014	35.498535
1282.136611	107685.368236	35.503552
1283.223056	107851.474869	35.508570
1284.216327	108021.439282	35.513588
1285.574512	108181.011205	35.518605
1287.234478	108343.833770	35.523623
1288.087883	108518.210092	35.528640
1289.757730	108673.571003	35.533658
1291.309001	108831.515170	35.538676
1292.930568	108992.354411	35.543693
1293.970927	109140.811648	35.548711
1295.030415	109288.886974	35.553728
1296.263949	109426.206897	35.558746
1297.057838	109580.858331	35.563764
1298.301308	109735.470925	35.568781
1299.673580	109884.500220	35.573799
1301.101736	110036.509171	35.578816
1302.416695	110186.657114	35.583834
1303.371956	110343.604398	35.588852
1304.456182	110512.122144	35.593869
1305.734502	110669.361965	35.598887
1306.914130	110835.068940	35.603904
1308.233668	110990.183725	35.608922
1309.308330	111173.880470	35.613940
1310.847134	111341.141575	35.618957
1312.281216	111505.502275	35.623975
1313.648513	111681.572802	35.628992
1315.292939	111839.920290	35.634010
1316.454780	112012.829076	35.639028
1318.043812	112173.738584	35.644045
1319.440421	112339.060299	35.649063
1320.648347	112504.362459	35.654080
1322.245217	112665.906938	35.659098
1323.073513	112843.286791	35.664116
1324.960293	113003.850471	35.669133
1326.519262	113163.853225	35.674151
1327.529214	113335.200019	35.679168
1329.099224	113500.900687	35.684186
1330.250541	113675.038125	35.689204
1331.697708	113829.238690	35.694221
1333.558729	113996.080213	35.699239
1334.833540	114147.284029	35.704256
1336.640778	114302.436858	35.709274
1337.306464	114459.658675	35.714292
1338.660703	114625.477013	35.719309
1340.102943	114782.317845	35.724327
1341.132863	114954.046000	35.729344
1342.535243	115114.130354	35.734362
1343.382533	115289.682088	35.739380
1345.076034	115465.657680	35.744397
1346.129947	115643.996364	35.749415
1347.204319	115821.193431	35.754432
1348.807465	115979.966099	35.759450
1349.741654	116164.430762	35.764468
1351.227335	116347.042668	35.769485
1352.466874	116532.696068	35.774503
1353.785629	116727.664403	35.779520
1355.053245	116906.256517	35.784538
1356.386344	117094.457027	35.789556
1357.857519	117281.763218	35.794573
1359.235750	117473.131437	35.799591
1360.398576	117657.006984	35.804608
1361.950493	117834.591619	35.809626
1363.859075	118018.351221	35.814644
1365.899878	118179.651298	35.819661
1367.686560	118341.758919	35.824679
1368.791775	118500.499670	35.829696
1370.233330	118651.450370	35.834714
1371.363599	118794.029959	35.839732
1372.421186	118946.012178	35.844749
1373.882774	119106.472950	35.849767
1375.129877	119260.497454	35.854784
1376.681612	119396.972605	35.859802
1377.899712	119553.941535	35.864820
1379.200985	119719.851849	35.869837
1380.908568	119871.501881	35.874855
1381.875543	120037.771286	35.879872
1383.307081	120192.937112	35.884890
1384.598959	120365.083960	35.889908
1385.374382	120536.807424	35.894925
1386.957322	120710.771994	35.899943
1387.732154	120892.743682	35.904960
1389.192504	121068.414526	35.909978
1390.366184	121252.453025	35.914996
1391.475018	121450.802043	35.920013
1393.007583	121643.373194	35.925031
1394.879440	121825.658256	35.930048
1396.766702	121993.972194	35.935066
1398.317681	122181.756819	35.940084
1399.873521	122364.070473	35.945101
1401.114331	122540.469917	35.950119
1402.131244	122735.816060	35.955136
1403.731477	122918.113789	35.960154
1405.032558	123105.881316	35.965172
1406.410401	123294.917230	35.970189
1408.187344	123488.210200	35.975207
1408.984890	123695.073700	35.980224
1410.457044	123876.258355	35.985242
1411.483489	124064.126903	35.990260
1412.664528	124275.291160	35.995277
1414.158165	124466.913554	36.000295
1415.472483	124684.557784	36.005312
1417.101302	124881.658974	36.010330
1418.475762	125091.582872	36.015348
1420.071081	125292.226428	36.020365
1421.393764	125509.115942	36.025383
1422.326887	125717.848111	36.030400
1423.889569	125932.562119	36.035418
1425.105618	126144.368741	36.040436
1426.943378	126363.501339	36.045453
1428.410159	126568.709676	36.050471
1429.681821	126792.749333	36.055488
1431.759484	126997.496456	36.060506
1433.575229	127197.878322	36.065524
1435.072975	127401.707183	36.070541
1436.854545	127593.597191	36.075559
1438.738295	127782.507965	36.080576
1440.491844	127966.538137	36.085594
1441.824385	128138.348215	36.090612
1443.402724	128317.898668	36.095629
1445.115282	128499.430570	36.100647
1445.822394	128670.127157	36.105664
1447.265383	128838.934265	36.110682
1448.953955	128998.404586	36.115700
1449.912166	129183.772740	36.120717
1451.243179	129349.965646	36.125735
1452.594251	129524.365797	36.130752
1453.936648	129706.952572	36.135770
1454.721388	129897.623322	36.140788
1456.011303	130084.477705	36.145805
1457.938740	130266.747132	36.150823
1459.323034	130463.724430	36.155840
1460.552251	130651.149680	36.160858
1461.969635	130849.682761	36.165876
1463.015498	131062.947645	36.170893
1464.697497	131261.948368	36.175911
1466.003932	131469.359539	36.180928
1467.115468	131680.249398	36.185946
1468.802139	131889.060263	36.190964
1470.371651	132093.089332	36.195981
1472.507441	132286.716405	36.200999
1473.722508	132500.142597	36.206016
1475.582751	132719.296229	36.211034
1476.827267	132913.664675	36.216052
1478.622683	133104.158438	36.221069
1480.358385	133311.109371	36.226087
1481.942472	133513.815870	36.231104
1482.923452	133715.504592	36.236122
1484.969889	133910.411268	36.241140
1485.982774	134126.656610	36.246157
1487.637183	134326.861488	36.251175
1488.972149	134544.325891	36.256192
1490.384753	134744.382010	36.261210
1492.123358	134947.808970	36.266228
1493.315395	135170.293271	36.271245
1494.762116	135382.842375	36.276263
1496.209994	135596.153142	36.281280
1497.456714	135814.895562	36.286298
1499.408133	136030.271019	36.291316
1500.713669	136254.557623	36.296333
1502.510202	136458.201345	36.301351
1504.168305	136674.312425	36.306368
1505.410792	136881.544590	36.311386
1507.745383	137106.016364	36.316404
1509.343618	137302.765729	36.321421
1510.917790	137509.239965	36.326439
1512.412686	137702.650223	36.331456
1513.786847	137905.965536	36.336474
1515.418174	138114.323128	36.341492
1516.737673	138320.209841	36.346509
1518.696576	138513.500982	36.351527
1519.767700	138732.216899	36.356544
1521.214716	138936.706266	36.361562
1523.149485	139129.941874	36.366580
1524.065869	139341.006930	36.371597
1525.733768	139546.453884	36.376615
1527.372704	139730.450854	36.381632
1529.062139	139914.542317	36.386650
1531.083632	140081.777091	36.391668
1532.445590	140259.700000	36.396685
1534.139812	140438.509027	36.401703
1535.378789	140634.095404	36.406720
1536.359815	140809.002345	36.411738
1538.205937	140994.330212	36.416756
1539.344325	141189.226414	36.421773
1541.012232	141376.295910	36.426791
1542.166906	141574.575963	36.431808
1543.664697	141787.213375	36.436826
1545.048489	141980.833586	36.441844
1546.136694	142198.317131	36.446861
1547.815012	142413.338354	36.451879
1548.833012	142635.741174	36.456896
1550.354462	142854.998363	36.461914
1552.264846	143070.925250	36.466932
1553.213865	143298.274287	36.471949
1554.348381	143533.504684	36.476967
1555.945685	143777.421802	36.481984
1557.701290	144013.165586	36.487002
1559.717493	144238.932392	36.492020
1560.896605	144485.773425	36.497037
1562.717474	144736.697361	36.502055
1564.230419	144966.618190	36.507072
1566.003523	145209.656667	36.512090
1567.306969	145453.164576	36.517108
1569.033862	145692.804371	36.522125
1570.673606	145941.218883	36.527143
1571.976544	146188.066322	36.532160
1573.784685	146428.636829	36.537178
1575.365732	146672.667810	36.542196
1577.036954	146917.738479	36.547213
1578.813030	147160.918278	36.552231
1580.825881	147409.728718	36.557248
1582.102664	147655.894518	36.562266
1583.374065	147902.139127	36.567284
1585.250553	148147.782450	36.572301
1587.021594	148396.284024	36.577319
1588.390481	148643.140003	36.582336
1589.717070	148894.314797	36.587354
1591.424571	149136.417573	36.592372
1592.779702	149396.719304	36.597389
1594.895111	149643.717902	36.602407
1596.289570	149892.455604	36.607424
1598.170084	150142.892867	36.612442
1599.785475	150390.192071	36.617460
1601.224013	150646.978843	36.622477
1602.847245	150888.689679	36.627495
1604.226498	151148.773363	36.632512
1606.186777	151393.160142	36.637530
1608.428379	151634.943070	36.642548
1609.820034	151888.171750	36.647565
1611.737402	152120.463019	36.652583
1613.429392	152341.064181	36.657600
1614.602210	152558.402143	36.662618
1616.373887	152770.460876	36.667636
1617.719333	152997.904473	36.672653
1619.530054	153211.303750	36.677671
1621.450742	153431.317949	36.682688
1622.960369	153648.077006	36.687706
1624.814613	153862.310330	36.692724
1625.642292	154097.489056	36.697741
1627.659852	154324.137560	36.702759
1629.787268	154526.438677	36.707776
1631.150701	154758.633378	36.712794
1632.500308	154981.271593	36.717812
1634.144932	155214.882894	36.722829
1635.860447	155447.039070	36.727847
1637.493986	155681.314673	36.732864
1638.766626	155904.161344	36.737882
1640.713140	156139.709081	36.742900
1642.372014	156382.430237	36.747917
1644.139269	156605.532598	36.752935
1645.795907	156836.135229	36.757952
1647.000632	157085.374956	36.762970
1648.798210	157316.846031	36.767988
1650.944480	157556.556232	36.773005
1652.805837	157789.313734	36.778023
1654.379308	158020.229115	36.783040
1655.099782	158269.237236	36.788058
1657.323999	158499.443781	36.793076
1658.771883	158748.111545	36.798093
1660.944137	158993.584589	36.803111
1662.320129	159234.709417	36.808128
1663.827452	159493.746054	36.813146
1665.588417	159739.936354	36.818164
1666.941586	159995.158761	36.823181
1668.534301	160240.199904	36.828199
1670.159054	160489.080120	36.833216
1671.549274	160754.307736	36.838234
1673.076169	161013.162138	36.843252
1674.175816	161296.143437	36.848269
1676.074681	161571.708021	36.853287
1677.520115	161838.773763	36.858304
1679.380124	162118.444958	36.863322
1680.740648	162395.800720	36.868340
1682.342038	162685.320622	36.873357
1683.828675	162967.987255	36.878375
1685.882745	163253.584387	36.883392
1687.611698	163550.015497	36.888410
1689.531751	163822.473939	36.893428
1690.892902	164109.658968	36.898445
1693.161826	164377.830121	36.903463
1695.212236	164647.394992	36.908480
1697.150995	164919.744446	36.913498
1699.140835	165190.172652	36.918516
1700.901957	165453.739516	36.923533
1703.279051	165706.036515	36.928551
1705.239884	165937.029941	36.933568
1706.843289	166175.995983	36.938586
1708.343652	166404.668253	36.943604
1710.051150	166641.210874	36.948621
1711.486166	166870.454430	36.953639
1713.086423	167108.082436	36.958656
1714.560276	167359.582698	36.963674
1716.237180	167588.373639	36.968692
1717.896074	167833.264739	36.973709
1719.558435	168091.639987	36.978727
1721.018479	168341.741014	36.983744
1722.304367	168603.857895	36.988762
1723.910593	168863.211269	36.993780
1725.597352	169127.145349	36.998797
1726.845821	169397.404266	37.003815
1729.011154	169663.295545	37.008832
1730.501610	169928.598149	37.013850
1732.110859	170205.984930	37.018868
1733.452077	170490.456317	37.023885
1735.439161	170781.550233	37.028903
1737.002219	171063.555066	37.033920
1738.533674	171367.283827	37.038938
1740.538079	171655.958627	37.043956
1742.257638	171952.241194	37.048973
1744.259585	172242.861520	37.053991
1745.905311	172533.236079	37.059008
1747.441863	172831.292172	37.064026
1749.485458	173133.773398	37.069044
1751.005916	173427.599478	37.074061
1752.931834	173733.858897	37.079079
1754.927044	174019.368123	37.084096
1756.255236	174335.203404	37.089114
1758.140585	174638.824742	37.094132
1760.035540	174946.645964	37.099149
1761.689119	175248.532571	37.104167
1763.931771	175546.648824	37.109184
1765.749766	175851.469708	37.114202
1767.917564	176134.010389	37.119220
1769.544954	176448.926426	37.124237
1771.182863	176742.948047	37.129255
1773.864525	177017.344386	37.134272
1776.725797	177284.774262	37.139290
1779.397320	177551.005336	37.144308
1781.520229	177803.369381	37.149325
1783.234578	178054.797516	37.154343
1785.176486	178298.312241	37.159360
1786.318118	178561.125975	37.164378
1788.024348	178816.226576	37.169396
1789.643222	179076.468323	37.174413
1791.377278	179331.897478	37.179431
1793.284984	179590.624759	37.184448
1794.631679	179863.500657	37.189466
1796.498064	180122.529528	37.194484
1798.329600	180383.874685	37.199501
1799.843155	180650.435900	37.204519
1801.453958	180890.084702	37.209536
1802.940602	181142.582202	37.214554
1804.481572	181385.163083	37.219572
1806.590051	181638.833567	37.224589
1808.132556	181897.251979	37.229607
1810.003877	182154.731530	37.234624
1811.267688	182432.445623	37.239642
1813.104696	182696.442974	37.244660
1814.471445	182959.869431	37.249677
1816.234476	183233.080975	37.254695
1818.102304	183509.145227	37.259712
1819.669326	183789.915745	37.264730
1821.336321	184074.605726	37.269748
1823.061563	184367.789908	37.274765
1824.508893	184660.296833	37.279783
1826.060051	184951.507562	37.284800
1827.680359	185266.514250	37.289818
1829.664505	185578.140754	37.294836
1831.460066	185892.882854	37.299853
1832.979494	186219.205731	37.304871
1834.378140	186534.497432	37.309888
1836.017303	186852.938224	37.314906
1838.465161	187190.414437	37.319924
1840.528913	187514.616993	37.324941
1842.164733	187842.620578	37.329959
1844.446503	188157.351642	37.334976
1846.988578	188477.144936	37.339994
1848.957994	188794.099849	37.345012
1851.160771	189106.387877	37.350029
1852.847988	189430.384195	37.355047
1854.201715	189738.585225	37.360064
1856.348241	190072.589236	37.365082
1858.614666	190388.505039	37.370100
1860.336311	190704.813954	37.375117
1862.090471	191029.939895	37.380135
1864.191685	191337.943655	37.385152
1865.920866	191661.681773	37.390170
1867.874757	191992.023795	37.395188
1869.728314	192306.532704	37.400205
1871.259850	192638.367497	37.405223
1873.511228	192959.404166	37.410240
1875.153210	193290.007412	37.415258
1877.199985	193610.306566	37.420276
1879.126770	193932.060955	37.425293
1881.385378	194256.099997	37.430311
1883.346775	194572.332106	37.435328
1884.973835	194892.046032	37.440346
1886.763829	195219.617764	37.445364
1888.906553	195530.927968	37.450381
1890.896153	195859.550921	37.455399
1893.069870	196174.578865	37.460416
1895.040126	196492.661757	37.465434
1896.762477	196811.204781	37.470452
1898.853287	197125.274332	37.475469
1900.190400	197442.613097	37.480487
1902.337380	197736.597964	37.485504
1903.865443	198046.878411	37.490522
1905.724641	198334.337511	37.495540
1907.733985	198628.476085	37.500557
1909.187212	198932.998379	37.505575
1910.945384	199226.926240	37.510592
1913.156650	199541.803281	37.515610
1914.942569	199853.094070	37.520628
1916.722459	200154.829714	37.525645
1918.517525	200483.562932	37.530663
1920.655188	200787.783917	37.535680
1922.685996	201102.228943	37.540698
1924.618981	201418.201790	37.545716
1927.455689	201717.480787	37.550733
1929.147494	202016.828836	37.555751
1931.414589	202318.803614	37.560768
1933.245989	202631.537194	37.565786
1935.152446	202941.747241	37.570804
1937.159303	203256.005058	37.575821
1938.668852	203568.794875	37.580839
1940.834604	203874.081719	37.585856
1942.678278	204200.912203	37.590874
1944.583553	204527.506268	37.595892
1946.565929	204839.123563	37.600909
1948.149678	205163.956961	37.605927
1949.918169	205483.088509	37.610944
1952.010554	205818.025613	37.615962
1953.925391	206145.972781	37.620980
1956.251816	206468.677104	37.625997
1958.122364	206800.747915	37.631015
1960.275025	207118.900589	37.636032
1962.512936	207450.980172	37.641050
1964.053362	207786.815643	37.646068
1966.007198	208105.309721	37.651085
1967.812171	208456.391458	37.656103
1969.770714	208787.837121	37.661120
1971.505056	209127.965447	37.666138
1973.522189	209474.423702	37.671156
1975.825934	209804.575895	37.676173
1977.552581	210170.241095	37.681191
1979.422393	210499.564423	37.686208
1981.473299	210858.148949	37.691226
1983.295362	211204.939645	37.696244
1985.331078	211552.282308	37.701261
1987.387894	211903.317907	37.706279
1989.343211	212255.133249	37.711296
1991.414285	212607.160644	37.716314
1993.189350	212959.795508	37.721332
1995.088842	213316.995716	37.726349
1996.626788	213691.610535	37.731367
1999.055113	214037.355154	37.736384
2000.976841	214421.612900	37.741402
2002.204839	214780.501760	37.746420
2004.999542	215144.247811	37.751437
2006.998330	215508.744193	37.756455
2008.618262	215852.480633	37.761472
2010.599007	216191.298816	37.766490
2012.964531	216527.023149	37.771508
2015.200380	216859.963737	37.776525
2016.959682	217210.159966	37.781543
2018.993643	217546.665468	37.786560
2021.184674	217887.693054	37.791578
2023.024977	218235.900785	37.796596
2025.338264	218573.649162	37.801613
2026.961175	218925.132384	37.806631
2029.351069	219278.158914	37.811648
2031.279617	219614.716147	37.816666
2032.961438	219972.683193	37.821684
2035.310198	220326.343407	37.826701
2037.451021	220729.519183	37.831719
2039.679324	221072.079282	37.836736
2041.955624	221426.352918	37.841754
2043.747142	221783.968324	37.846772
2045.832971	222135.075714	37.851789
2048.008539	222490.271742	37.856807
2049.839427	222849.003191	37.861824
2051.620808	223207.160040	37.866842
2054.037114	223570.284147	37.871860
2055.861227	223933.173713	37.876877
2057.927664	224299.607246	37.881895
2060.215585	224651.798445	37.886912
2062.768526	225017.561247	37.891930
2064.320639	225386.468459	37.896948
2066.708898	225751.841616	37.901965
2068.777234	226106.930921	37.906983
2071.021953	226472.380792	37.912000
2072.968121	226840.774780	37.917018
2075.069525	227207.190213	37.922036
2077.990478	227559.712297	37.927053
2080.541815	227918.465829	37.932071
2082.837812	228253.439222	37.937088
2085.245128	228586.110525	37.942106
2087.195122	228931.554076	37.947124
2089.336814	229271.685983	37.952141
2091.954656	229609.432515	37.957159
2093.491763	229955.402651	37.962176
2095.585211	230295.647652	37.967194
2097.568985	230647.060765	37.972212
2099.801352	230982.638547	37.977229
2101.134474	231335.833704	37.982247
2103.347279	231689.271619	37.987264
2105.426670	232040.446215	37.992282
2107.505813	232400.181219	37.997300
2109.152054	232755.566988	38.002317
2110.865288	233117.038959	38.007335
2112.882967	233495.633117	38.012352
2115.046026	233865.367077	38.017370
2116.971045	234241.261161	38.022388
2119.273945	234610.594713	38.027405
2121.462749	234979.642923	38.032423
2123.665410	235334.009868	38.037440
2125.300842	235682.981877	38.042458
2127.290624	236038.553327	38.047476
2129.220467	236387.430184	38.052493
2131.628131	236742.226549	38.057511
2133.411914	237093.617974	38.062528
2135.892122	237453.078593	38.067546
2137.293264	237830.821162	38.072564
2138.898991	238200.074612	38.077581
2141.109296	238584.625409	38.082599
2143.258114	238965.453549	38.087616
2145.283602	239350.569642	38.092634
2146.952085	239750.627820	38.097652
2149.286929	240143.114171	38.102669
2151.345827	240543.443328	38.107687
2153.227261	240944.995768	38.112704
2155.448163	241353.302893	38.117722
2157.454421	241766.623833	38.122740
2159.621907	242176.542365	38.127757
2161.623260	242598.655288	38.132775
2163.838199	243036.255324	38.137792
2166.218966	243457.879106	38.142810
2168.355531	243889.245956	38.147828
2171.067006	244304.774697	38.152845
2173.457215	244727.950464	38.157863
2176.143707	245138.964424	38.162880
2179.165060	245541.950662	38.167898
2181.289792	245963.445071	38.172916
2183.834185	246361.657733	38.177933
2185.947185	246764.766100	38.182951
2188.524849	247160.892803	38.187968
2191.254015	247542.162283	38.192986
2193.575288	247937.747486	38.198004
2195.920365	248319.232245	38.203021
2198.491472	248695.576437	38.208039
2200.867170	249067.100858	38.213056
2203.514995	249432.486651	38.218074
2205.474111	249818.354484	38.223092
2207.977202	250187.295734	38.228109
2209.897641	250566.795661	38.233127
2212.183611	250940.065871	38.238144
2214.056171	251308.982551	38.243162
2215.953402	251696.261581	38.248180
2218.031583	252072.259754	38.253197
2219.546351	252460.871180	38.258215
2221.855753	252849.611443	38.263232
2224.829003	253227.044977	38.268250
2226.769648	253612.644641	38.273268
2229.025703	253995.426233	38.278285
2231.110689	254388.371149	38.283303
2233.348800	254791.580439	38.288320
2236.097773	255164.379252	38.293338
2238.382691	255546.879777	38.298356
2240.727586	255923.071704	38.303373
2243.107953	256294.406808	38.308391
2244.787778	256653.762067	38.313408
2247.299911	256995.204216	38.318426
2249.407165	257356.143969	38.323444
2251.765895	257703.555664	38.328461
2253.756718	258047.596853	38.333479
2255.703846	258412.196151	38.338496
2258.112971	258772.328075	38.343514
2260.035689	259137.084705	38.348532
2262.363124	259492.785119	38.353549
2264.763719	259851.014679	38.358567
2266.975150	260221.722056	38.363584
2269.181273	260589.890484	38.368602
2271.144327	260978.318574	38.373620
2272.982990	261353.049347	38.378637
2274.706823	261751.550494	38.383655
2276.543516	262153.768482	38.388672
2278.696563	262558.172272	38.393690
2280.397901	262981.497185	38.398708
2282.526535	263405.466152	38.403725
2284.818272	263836.573419	38.408743
2287.307167	264275.829716	38.413760
2289.462157	264702.006039	38.418778
2291.478219	265158.409160	38.423796
2293.457626	265602.777480	38.428813
2296.033907	266051.420963	38.433831
2298.397682	266512.165088	38.438848
2300.929581	266956.828144	38.443866
2302.770512	267415.877748	38.448884
2305.350331	267871.990826	38.453901
2307.890517	268328.745619	38.458919
2309.908277	268802.476761	38.463936
2312.829017	269258.308153	38.468954
2314.940706	269731.389935	38.473972
2317.346994	270199.065179	38.478989
2319.939506	270655.838504	38.484007
2322.309750	271108.760556	38.489024
2324.610860	271571.931314	38.494042
2327.142811	272037.402756	38.499060
2329.541415	272502.692253	38.504077
2331.864578	272965.859941	38.509095
2334.672440	273433.802937	38.514112
2337.350676	273890.919294	38.519130
2339.583135	274346.429733	38.524148
2341.828286	274802.192214	38.529165
2344.489881	275257.202784	38.534183
2346.735541	275729.248742	38.539200
2349.377495	276177.225602	38.544218
2351.808788	276623.736985	38.549236
2354.099902	277083.505666	38.554253
2356.625783	277530.306685	38.559271
2358.753509	277984.054996	38.564288
2361.296348	278434.130064	38.569306
2363.377318	278894.947572	38.574324
2365.782438	279342.706966	38.579341
2368.563483	279790.457354	38.584359
2370.533866	280217.911719	38.589376
2372.871572	280641.471715	38.594394
2374.971307	281072.918788	38.599412
2376.981832	281496.733327	38.604429
2379.383423	281929.579947	38.609447
2381.059748	282381.796844	38.614464
2383.436189	282820.921347	38.619482
2385.316494	283280.599075	38.624500
2387.681144	283745.864496	38.629517
2389.466760	284206.877279	38.634535
2391.559073	284690.754559	38.639552
2393.979288	285171.657942	38.644570
2395.999920	285662.124804	38.649588
2398.269078	286149.579478	38.654605
2400.620742	286652.465417	38.659623
2402.872727	287159.811930	38.664640
2405.553183	287667.902641	38.669658
2408.088254	288191.435107	38.674676
2410.235044	288702.961875	38.679693
2412.965341	289215.385974	38.684711
2414.940892	289742.078071	38.689728
2417.838043	290257.572927	38.694746
2419.981824	290786.471737	38.699764
2422.524672	291306.847147	38.704781
2425.393091	291834.816014	38.709799
2427.707347	292374.531260	38.714816
2430.446751	292897.590111	38.719834
2433.128310	293418.751737	38.724852
2435.786549	293943.370524	38.729869
2438.729386	294456.232497	38.734887
2441.023927	294985.478710	38.739904
2443.670927	295506.081777	38.744922
2446.186901	296024.697470	38.749940
2448.785543	296541.012485	38.754957
2451.531689	297069.012958	38.759975
2453.803860	297588.653624	38.764992
2456.992866	298098.469434	38.770010
2459.424821	298601.875505	38.775028
2461.585550	299113.172157	38.780045
2464.482179	299626.789174	38.785063
2467.104426	300136.790259	38.790080
2469.992716	300624.369001	38.795098
2472.459494	301133.731094	38.800116
2474.839466	301628.601202	38.805133
2478.134662	302123.832689	38.810151
2480.204391	302627.435839	38.815168
2482.894746	303112.523255	38.820186
2485.386902	303599.520102	38.825204
2488.029215	304084.205413	38.830221
2490.404744	304562.454144	38.835239
2493.072323	305052.923393	38.840256
2495.784773	305532.563149	38.845274
2498.201337	306023.500416	38.850292
2500.786232	306508.440099	38.855309
2503.200555	306980.349289	38.860327
2504.938724	307437.606410	38.865344
2507.811656	307888.992454	38.870362
2509.880646	308336.821242	38.875380
2512.049525	308793.293884	38.880397
2514.623192	309254.932987	38.885415
2516.719280	309729.625154	38.890432
2519.296081	310189.177320	38.895450
2521.688964	310679.718652	38.900468
2523.906496	311158.144791	38.905485
2526.309291	311636.945920	38.910503
2528.236589	312123.694023	38.915520
2531.062633	312623.124024	38.920538
2533.447825	313116.271851	38.925556
2535.705491	313629.578768	38.930573
2538.260322	314136.842026	38.935591
2540.317006	314656.830153	38.940608
2543.187657	315180.699608	38.945626
2545.525328	315724.893136	38.950644
2547.523066	316255.346409	38.955661
2550.200516	316786.755842	38.960679
2552.250629	317338.986329	38.965696
2555.184766	317889.448128	38.970714
2557.782040	318433.432942	38.975732
2560.395494	318985.615356	38.980749
2563.141587	319543.970358	38.985767
2565.561686	320100.671982	38.990784
2567.931395	320663.524179	38.995802
2570.264495	321230.467475	39.000820
2572.718748	321802.162459	39.005837
2576.464755	322355.058904	39.010855
2579.197118	322924.746863	39.015872
2582.041702	323470.083829	39.020890
2585.017914	324038.862153	39.025908
2587.321482	324610.282692	39.030925
2590.048509	325155.804941	39.035943
2592.951739	325707.441266	39.040960
2595.536487	326265.396841	39.045978
2598.265760	326829.141037	39.050996
2600.801220	327395.425958	39.056013
2603.802488	327943.272660	39.061031
2606.325272	328510.744939	39.066048
2608.724554	329060.812102	39.071066
2611.580343	329613.469294	39.076084
2614.108354	330177.042864	39.081101
2616.983808	330722.070504	39.086119
2619.899648	331272.547263	39.091136
2623.024377	331801.656386	39.096154
2626.084416	332337.881902	39.101172
2628.597104	332890.619255	39.106189
2631.754259	333414.251720	39.111207
2633.865163	333958.842418	39.116224
2635.862707	334500.729790	39.121242
2638.587661	335040.415490	39.126260
2641.098840	335595.848319	39.131277
2643.323743	336135.604443	39.136295
2645.540438	336661.493739	39.141312
2648.265482	337173.129986	39.146330
2650.523619	337699.156744	39.151348
2652.733190	338237.933134	39.156365
2655.441491	338760.122090	39.161383
2657.701471	339294.869869	39.166400
2660.321063	339836.106839	39.171418
2663.144500	340390.687374	39.176436
2665.401524	340946.469818	39.181453
2668.160803	341502.370813	39.186471
2671.398411	342056.388348	39.191488
2673.920295	342601.069438	39.196506
2676.541227	343163.425923	39.201524
2679.399230	343722.108984	39.206541
2682.183753	344276.050779	39.211559
2684.907657	344849.088800	39.216576
2686.859750	345422.268798	39.221594
2689.782614	345993.588386	39.226612
2692.353603	346583.795406	39.231629
2695.250832	347156.478309	39.236647
2698.211715	347745.875219	39.241664
2700.684827	348321.989829	39.246682
2703.491056	348905.356943	39.251700
2706.641282	349496.482280	39.256717
2709.831047	350073.048917	39.261735
2712.591765	350666.025596	39.266752
2715.128764	351250.704814	39.271770
2718.038825	351827.398444	39.276788
2720.740541	352410.185704	39.281805
2723.407355	352998.835802	39.286823
2725.622363	353582.372446	39.291840
2728.251351	354180.762601	39.296858
2731.054857	354774.904484	39.301876
2733.320497	355389.380375	39.306893
2736.299011	355999.370056	39.311911
2738.943061	356622.426524	39.316928
2741.688408	357230.940520	39.321946
2744.326449	357841.926057	39.326964
2746.591379	358475.476532	39.331981
2749.201915	359103.177106	39.336999
2752.005607	359737.387214	39.342016
2755.055596	360371.752975	39.347034
2758.137740	361008.414789	39.352052
2760.884763	361647.126095	39.357069
2763.675485	362276.279068	39.362087
2766.569743	362915.812617	39.367104
2769.576425	363546.614564	39.372122
2772.333684	364184.680203	39.377140
2774.939148	364827.861946	39.382157
2778.001828	365448.299781	39.387175
2781.063583	366076.545441	39.392192
2784.168124	366695.385956	39.397210
2787.278848	367310.638726	39.402228
2789.579213	367945.855518	39.407245
2792.779533	368550.647016	39.412263
2795.324473	369137.897769	39.417280
2798.127179	369714.315205	39.422298
2800.984795	370295.004569	39.427316
2803.776325	370871.585793	39.432333
2806.282478	371441.911527	39.437351
2809.373666	372022.895463	39.442368
2811.678723	372610.821294	39.447386
2814.643082	373199.370257	39.452404
2817.145511	373799.579375	39.457421
2819.539589	374398.705865	39.462439
2822.763555	374999.062276	39.467456
2825.168841	375605.273434	39.472474
2827.451073	376228.265429	39.477492
2830.287038	376851.007859	39.482509
2832.896157	377474.918150	39.487527
2835.708781	378108.706124	39.492544
2838.362346	378749.079840	39.497562
2841.387867	379388.699220	39.502580
2844.273468	380041.750375	39.507597
2847.260097	380686.453648	39.512615
2850.308553	381327.508685	39.517632
2852.962607	381985.256542	39.522650
2855.784335	382644.970461	39.527668
2858.748991	383307.060051	39.532685
2861.228456	383966.779592	39.537703
2864.375483	384626.939824	39.542720
2867.880855	385293.905570	39.547738
2871.016070	385947.702712	39.552756
2873.723269	386627.529108	39.557773
2876.690489	387292.083260	39.562791
2879.609793	387949.480273	39.567808
2882.269077	388629.885321	39.572826
2885.698671	389287.303824	39.577844
2888.235204	389956.416626	39.582861
2891.627667	390617.519168	39.587879
2894.697142	391288.221523	39.592896
2897.531051	391945.481783	39.597914
2901.227058	392594.300365	39.602932
2904.199786	393257.853761	39.607949
2907.190563	393909.269781	39.612967
2910.310972	394564.431292	39.617984
2913.071225	395227.548921	39.623002
2916.166313	395872.241542	39.628020
2919.225685	396532.167123	39.633037
2921.926506	397176.187034	39.638055
2924.904202	397829.862067	39.643072
2927.614361	398493.277748	39.648090
2930.546048	399138.237089	39.653108
2932.779896	399805.657000	39.658125
2935.320801	400484.195798	39.663143
2938.222933	401161.649038	39.668160
2941.170564	401836.342669	39.673178
2943.810896	402515.532752	39.678196
2946.745131	403200.670246	39.683213
2949.800637	403860.118019	39.688231
2953.151212	404516.868777	39.693248
2955.727106	405161.332005	39.698266
2958.865260	405800.369438	39.703284
2961.347845	406450.473732	39.708301
2964.171856	407098.127501	39.713319
2967.203646	407741.957825	39.718336
2970.366232	408384.714619	39.723354
2973.628946	409041.408300	39.728372
2976.240563	409702.296924	39.733389
2979.063202	410356.978536	39.738407
2981.769139	411031.864714	39.743424
2984.665872	411700.369173	39.748442
2987.794747	412361.547979	39.753460
2990.743866	413052.874230	39.758477
2993.654486	413735.294826	39.763495
2996.594811	414412.474199	39.768512
2999.634318	415099.378789	39.773530
3002.946911	415776.771498	39.778548
3006.007869	416489.335816	39.783565
3008.706788	417179.589648	39.788583
3011.640563	417881.116395	39.793600
3014.088732	418591.393890	39.798618
3017.382689	419297.009455	39.803636
3020.172243	420029.773059	39.808653
3023.227142	420751.580554	39.813671
3026.714411	421468.157615	39.818688
3029.614505	422194.335233	39.823706
3033.050185	422919.471549	39.828724
3035.823039	423653.560555	39.833741
3038.788727	424373.260434	39.838759
3041.870903	425113.670478	39.843776
3044.917340	425851.051320	39.848794
3048.409516	426588.240056	39.853812
3051.496088	427325.523287	39.858829
3054.186597	428074.221976	39.863847
3057.265421	428815.923103	39.868864
3060.102160	429562.428765	39.873882
3063.752140	430308.708499	39.878900
3066.685228	431055.586838	39.883917
3069.840263	431798.204354	39.888935
3073.357429	432550.924188	39.893952
3076.065713	433305.598675	39.898970
3079.033885	434050.814454	39.903988
3082.250636	434806.250451	39.909005
3085.437169	435557.844951	39.914023
3088.413429	436311.957191	39.919040
3091.462328	437071.403383	39.924058
3094.835187	437832.724902	39.929076
3097.536286	438604.105345	39.934093
3100.604339	439361.984640	39.939111
3104.315192	440128.802808	39.944128
3107.005944	440892.264559	39.949146
3110.347030	441641.928575	39.954164
3113.337864	442412.738215	39.959181
3116.155365	443160.260904	39.964199
3119.602841	443887.105558	39.969216
3122.656656	444602.548738	39.974234
3126.016493	445301.165020	39.979252
3129.550813	446012.794120	39.984269
3132.757873	446713.822860	39.989287
3136.149942	447424.520676	39.994304
3138.669613	448147.129259	39.999322
3142.073241	448840.571652	40.004340
3145.290994	449566.872733	40.009357
3148.034714	450283.052469	40.014375
3151.347005	451001.853132	40.019392
3153.992515	451730.302340	40.024410
3157.011383	452449.002799	40.029428
3160.098809	453184.319857	40.034445
3163.030415	453932.744829	40.039463
3166.185149	454666.535486	40.044480
3168.914740	455428.201237	40.049498
3171.888596	456195.520414	40.054516
3175.007225	456972.404233	40.059533
3177.686866	457744.523496	40.064551
3181.155011	458522.815593	40.069568
3184.128144	459311.884466	40.074586
3187.509096	460110.371816	40.079604
3190.549873	460914.448714	40.084621
3193.807592	461709.557910	40.089639
3197.356436	462511.926927	40.094656
3199.912180	463327.575216	40.099674
3203.003257	464155.551234	40.104692
3206.219386	464972.600422	40.109709
3209.361346	465819.572752	40.114727
3212.850744	466638.335365	40.119744
3215.616568	467491.824523	40.124762
3219.344219	468311.799193	40.129780
3222.670615	469161.085744	40.134797
3225.650222	469998.104174	40.139815
3229.065082	470839.115830	40.144832
3232.306961	471693.924702	40.149850
3235.400688	472553.272018	40.154868
3238.714567	473412.143865	40.159885
3241.662091	474264.363647	40.164903
3245.524178	475115.240116	40.169920
3248.505662	475991.951966	40.174938
3251.225137	476836.920328	40.179956
3254.753498	477713.975796	40.184973
3257.719878	478597.551533	40.189991
3261.296126	479466.687090	40.195008
3264.868966	480347.460300	40.200026
3268.102456	481220.312746	40.205044
3271.599031	482088.283443	40.210061
3274.804678	482959.141990	40.215079
3278.333845	483833.548678	40.220096
3281.826712	484698.775234	40.225114
3284.902040	485586.160709	40.230132
3288.573598	486445.267175	40.235149
3291.280816	487303.982126	40.240167
3294.759354	488124.644325	40.245184
3297.561111	488970.941197	40.250202
3300.796489	489789.346489	40.255220
3304.467210	490619.568961	40.260237
3307.458160	491455.923629	40.265255
3310.988060	492277.103073	40.270272
3314.188816	493116.986526	40.275290
3317.365172	493934.663105	40.280308
3320.824016	494776.248313	40.285325
3323.724718	495625.054392	40.290343
3327.545441	496466.353017	40.295360
3330.564694	497313.748591	40.300378
3334.263876	498160.946479	40.305396
3337.487943	499007.826204	40.310413
3340.769527	499876.872634	40.315431
3344.249587	500734.384698	40.320448
3346.962292	501606.718540	40.325466
3350.495035	502463.583511	40.330484
3354.039837	503331.056409	40.335501
3356.875726	504215.609708	40.340519
3360.645424	505088.512833	40.345536
3363.514960	505993.665842	40.350554
3366.697983	506877.474236	40.355572
3370.355362	507778.069212	40.360589
3373.364088	508697.745014	40.365607
3377.208517	509594.581942	40.370624
3380.552082	510504.015504	40.375642
3383.741946	511419.530142	40.380660
3387.428886	512349.699909	40.385677
3390.052028	513270.955900	40.390695
3393.549447	514198.178041	40.395712
3396.533231	515143.338385	40.400730
3399.968653	516095.032343	40.405748
3403.637571	517035.941693	40.410765
3407.181399	517973.034621	40.415783
3411.314655	518912.250726	40.420800
3415.211613	519846.003941	40.425818
3419.280324	520772.616774	40.430836
3422.927465	521689.662731	40.435853
3426.326182	522636.596937	40.440871
3429.708073	523539.713961	40.445888
3433.364413	524477.423972	40.450906
3437.061553	525384.118532	40.455924
3440.374766	526301.459189	40.460941
3443.713812	527226.858732	40.465959
3447.209772	528150.869020	40.470976
3450.576140	529072.124102	40.475994
3453.791629	529997.280357	40.481012
3457.325667	530929.437676	40.486029
3460.435567	531852.535664	40.491047
3464.254994	532778.339106	40.496064
3467.816356	533718.538964	40.501082
3470.965112	534648.266935	40.506100
3474.241300	535588.146112	40.511117
3477.513280	536496.688511	40.516122
3480.956306	537384.742729	40.521127
3483.781806	538227.189531	40.526132
3486.689707	539004.433152	40.531136
3489.989017	539717.949539	40.536141
3492.402743	540373.554295	40.541146
3495.357143	540979.007281	40.546151
3497.576934	541514.673273	40.551156
3499.938378	542006.170556	40.556160
3501.989633	542430.552603	40.561165
3504.017020	542794.545007	40.566170
3505.863904	543115.341870	40.571175
3507.521649	543405.063530	40.576180
3509.084170	543637.647574	40.581184
3511.050414	543800.195203	40.586189
3512.641265	543949.372099	40.591194
3514.596633	544045.483937	40.596199
3515.630166	544080.001683	40.601204
3516.257202	544120.994766	40.606208
3517.689346	544089.116407	40.611213
3518.205693	544031.434986	40.616218
3519.126833	543967.984883	40.621223
3519.830089	543864.687776	40.626228
3520.585482	543753.354929	40.631232
3521.377648	543605.314025	40.636237
3521.487226	543453.138874	40.641242
3521.948385	543262.740301	40.646247
3522.057139	543069.365876	40.651252
3522.469800	542872.305932	40.656256
3522.687234	542649.526063	40.661261
3522.770255	542421.967812	40.666266
3522.880095	542182.284687	40.671271
3522.991044	541943.455865	40.676276
3523.105179	541677.307699	40.681280
3522.925078	541430.286839	40.686285
3522.825736	541175.574427	40.691290
3522.896418	540910.328388	40.696295
3523.355723	540632.140433	40.701300
3522.948070	540364.031745	40.706304
3522.950898	540070.454286	40.711309
3522.682173	539802.818623	40.716314
3522.557157	539533.792087	40.721319
3522.956291	539240.337866	40.726324
3522.282775	538950.279419	40.731328
3522.201691	538700.218776	40.736333
3521.802668	538386.421692	40.741338
3521.767515	538118.719376	40.746343
3521.335789	537845.923743	40.751348
3521.422061	537563.395161	40.756352
3520.843124	537289.703768	40.761357
3520.687786	537013.415246	40.766362
3520.968754	536751.699631	40.771367
3520.505633	536494.491261	40.776372
3520.564710	536201.537309	40.781376
3520.406640	535956.949253	40.786381
3519.943364	535688.261833	40.791386
3520.091336	535421.847118	40.796391
3519.630773	535162.039957	40.801396
3519.475383	534905.160415	40.806400
3519.452160	534652.650359	40.811405
3518.955970	534405.969522	40.816410
3519.079968	534149.588898	40.821415
3518.435718	533902.670847	40.826420
3518.301190	533658.850837	40.831424
3518.269589	533407.635194	40.836429
3517.792356	533189.575261	40.841434
3517.720291	532961.344476	40.846439
3517.689498	532724.111337	40.851444
3517.346779	532495.461806	40.856448
3517.187186	532262.384643	40.861453
3517.224266	532054.079099	40.866458
3516.811112	531815.275840	40.871463
3516.741310	531598.190181	40.876468
3515.978712	531386.819145	40.881472
3515.917194	531173.970286	40.886477
3515.960800	530982.069890	40.891482
3515.546596	530769.574420	40.896487
3515.160311	530591.429685	40.901492
3515.502393	530385.024231	40.906496
3514.789488	530184.846128	40.911501
3514.759813	530001.989786	40.916506
3514.472023	529818.414175	40.921511
3514.574870	529633.359857	40.926516
3514.104964	529454.912269	40.931520
3514.123914	529271.231268	40.936525
3514.365418	529107.624395	40.941530
3514.008637	528936.732743	40.946535
3513.950709	528741.890204	40.951540
3513.855013	528597.937899	40.956544
3513.696701	528414.881343	40.961549
3513.266159	528250.917009	40.966554
3513.287769	528075.559788	40.971559
3513.234024	527921.892071	40.976564
3512.830827	527759.889196	40.981568
3512.658989	527601.132944	40.986573
3512.443910	527461.333130	40.991578
3512.504174	527311.027422	40.996583
3512.298570	527165.108530	41.001588
3512.172241	527008.663886	41.006592
3512.193190	526860.280572	41.011597
3511.685636	526735.732649	41.016602
3511.858975	526586.716237	41.021607
3511.492882	526457.190930	41.026612
3511.170877	526323.260615	41.031616
3511.582612	526191.841320	41.036621
3511.305332	526068.060435	41.041626
3511.193389	525921.812109	41.046631
3510.854726	525813.757310	41.051636
3510.642895	525690.266403	41.056640
3510.856768	525567.566486	41.061645
3510.809494	525449.708473	41.066650
3510.211398	525314.448679	41.071655
3510.559555	525207.140473	41.076660
3510.030978	525086.272691	41.081664
3509.977952	524992.016252	41.086669
3510.009442	524877.073150	41.091674
3509.604374	524772.408310	41.096679
3509.686978	524678.836227	41.101684
3509.533448	524579.134356	41.106688
3509.894845	524462.215413	41.111693
3509.653973	524383.047779	41.116698
3509.460819	524275.919995	41.121703
3509.375263	524178.378398	41.126708
3508.773570	524087.539459	41.131712
3509.330966	523984.031601	41.136717
3509.043863	523900.167983	41.141722
3508.967635	523814.147585	41.146727
3508.816784	523708.171941	41.151732
3508.471877	523634.931225	41.156736
3508.917584	523554.640038	41.161741
3508.914617	523472.902890	41.166746
3508.414878	523384.369130	41.171751
3508.511797	523297.610923	41.176756
3508.564827	523217.177921	41.181760
3508.398115	523131.117633	41.186765
3508.514171	523061.289421	41.191770
3508.527699	522976.413032	41.196775
3508.522203	522896.290988	41.201780
3508.186449	522828.504661	41.206784
3508.478265	522746.060086	41.211789
3508.012147	522678.799248	41.216794
3508.027942	522603.474786	41.221799
3507.906711	522520.083305	41.226804
3507.804226	522455.797194	41.231808
3507.646568	522370.590819	41.236813
3507.553896	522314.239338	41.241818
3507.640088	522252.601894	41.246823
3507.992218	522195.320303	41.251828
3507.454254	522114.671911	41.256832
3507.503263	522059.965415	41.261837
3507.352943	522007.666258	41.266842
3507.306465	521930.730798	41.271847
3507.218003	521870.535016	41.276852
3506.791433	521822.222139	41.281856
3507.134907	521775.202939	41.286861
3507.287979	521712.946225	41.291866
3507.002272	521645.349260	41.296871
3506.998335	521586.301827	41.301876
3506.757270	521538.161006	41.306880
3506.984011	521475.133414	41.311885
3507.136538	521433.653933	41.316890
3507.021300	521371.589985	41.321895
3506.786080	521323.144271	41.326900
3506.926693	521266.145618	41.331904
3506.572431	521216.909506	41.336909
3506.620737	521165.486260	41.341914
3506.702340	521113.653137	41.346919
3506.494230	521059.287252	41.351924
3506.235930	521036.628174	41.356928
3506.778662	520980.019978	41.361933
3506.605231	520942.786981	41.366938
3506.491704	520883.198193	41.371943
3506.499870	520852.053701	41.376948
3506.535484	520801.490786	41.381952
3506.679712	520745.349218	41.386957
3506.072478	520712.026629	41.391962
3506.514669	520673.785685	41.396967
3506.262158	520635.705004	41.401972
3506.115721	520576.575319	41.406976
3506.197038	520546.075937	41.411981
3505.726040	520518.848961	41.416986
3506.247283	520469.775574	41.421991
3506.079183	520428.900356	41.426996
3505.852861	520395.163009	41.432000
3506.132891	520353.053928	41.437005
3506.058699	520314.944316	41.442010
3506.158816	520285.098743	41.447015
3506.352442	520237.087617	41.452020
3506.240825	520205.960826	41.457024
3506.111901	520148.798636	41.462029
3505.868168	520118.956544	41.467034
3505.902475	520088.109822	41.472039
3505.801962	520050.610470	41.477044
3505.913829	520016.262735	41.482048
3506.164020	519983.258184	41.487053
3505.991947	519951.887664	41.492058
3506.085023	519905.155458	41.497063
3506.278050	519870.086747	41.502068
3505.949709	519844.605709	41.507072
3506.058542	519799.336961	41.512077
3506.038145	519768.397162	41.517082
3505.943672	519720.480617	41.522087
3505.851313	519695.012611	41.527092
3505.679636	519677.292915	41.532096
3505.922594	519603.941127	41.537101
3505.318741	519601.609655	41.542106
3505.589641	519560.662888	41.547111
3505.808642	519539.443135	41.552116
3505.508486	519510.215586	41.557120
3505.757649	519465.783283	41.562125
3505.375583	519443.798856	41.567130
3505.535903	519418.694979	41.572135
3505.602371	519393.909267	41.577140
3505.485969	519365.916463	41.582144
3505.582035	519327.322589	41.587149
3505.011727	519316.289118	41.592154
3505.630609	519278.573179	41.597159
3505.829668	519262.867487	41.602164
3505.525981	519238.038917	41.607168
3505.624407	519206.320847	41.612173
3505.489082	519172.162100	41.617178
3505.298845	519143.927775	41.622183
3505.243220	519123.610451	41.627188
3505.171956	519090.250411	41.632192
3505.352395	519070.451902	41.637197
3505.252780	519068.647411	41.642202
3505.298560	519026.116885	41.647207
3505.254953	519000.892911	41.652212
3505.222560	518988.762944	41.657216
3505.242014	518955.084914	41.662221
3505.223297	518933.952513	41.667226
3505.566462	518906.391926	41.672231
3505.460264	518879.407945	41.677236
3505.746677	518850.743841	41.682240
3505.602028	518821.844433	41.687245
3505.106668	518810.950465	41.692250
3504.905780	518777.003513	41.697255
3505.190009	518765.581795	41.702260
3505.358341	518729.604409	41.707264
3505.310629	518698.565786	41.712269
3504.875031	518704.803446	41.717274
3505.096791	518653.749415	41.722279
3505.251331	518650.387790	41.727284
3505.078097	518617.295726	41.732288
3505.166721	518614.045640	41.737293
3505.257697	518588.546944	41.742298
3505.143996	518559.945570	41.747303
3505.434897	518553.933031	41.752308
3504.832898	518528.847150	41.757312
3505.051171	518507.777876	41.762317
3505.153822	518477.574668	41.767322
3505.076137	518455.844199	41.772327
3505.201553	518440.553880	41.777332
3505.230756	518429.475624	41.782336
3505.274911	518401.759192	41.787341
3505.109784	518371.901500	41.792346
3505.054836	518344.857979	41.797351
3505.124249	518338.728672	41.802356
3505.266625	518307.558140	41.807360
3504.987151	518289.752854	41.812365
3504.844816	518263.683748	41.817370
3505.005984	518264.214517	41.822375
3505.154241	518223.182678	41.827380
3504.875033	518209.725882	41.832384
3505.220545	518192.226237	41.837389
3505.192195	518164.470300	41.842394
3504.997832	518144.072564	41.847399
3505.287135	518120.210464	41.852404
3505.072769	518116.502509	41.857408
3505.428152	518077.713029	41.862413
3504.790512	518055.008649	41.867418
3505.063447	518035.042582	41.872423
3505.184969	518033.253593	41.877428
3505.212717	518022.478689	41.882432
3505.031740	517989.083193	41.887437
3505.016803	517973.308964	41.892442
3504.902881	517952.645447	41.897447
3504.926970	517938.230303	41.902452
3504.911660	517931.254609	41.907456
3505.212469	517901.676391	41.912461
3504.619084	517899.646412	41.917466
3504.969331	517872.436945	41.922471
3504.988770	517845.431415	41.927476
3505.049839	517851.944863	41.932480
3505.099106	517814.265041	41.937485
3504.850725	517804.140434	41.942490
3504.808393	517774.767921	41.947495
3505.083054	517762.639090	41.952500
3504.891031	517753.264046	41.957504
3504.942238	517727.214072	41.962509
3504.610245	517720.895142	41.967514
3504.629621	517690.501389	41.972519
3505.000106	517683.616318	41.977524
3504.776059	517667.975981	41.982528
3505.109663	517644.763565	41.987533
3504.676255	517636.286246	41.992538
3504.397414	517614.990999	41.997543
3504.755532	517602.140920	42.002548
3505.109534	517593.943669	42.007552
3504.682398	517579.447825	42.012557
3504.827253	517562.889440	42.017562
3505.054134	517550.312899	42.022567
3504.676480	517527.667837	42.027572
3504.639019	517519.734689	42.032576
3504.866074	517493.909393	42.037581
3505.171188	517475.859134	42.042586
3505.066273	517461.817936	42.047591
3505.336463	517439.677177	42.052596
3505.102199	517430.966006	42.057600
3505.174909	517408.755281	42.062605
3504.807149	517387.271523	42.067610
3504.758738	517357.292415	42.072615
3505.076910	517355.876817	42.077620
3504.609697	517340.982553	42.082624
3504.893828	517308.169558	42.087629
3505.054626	517314.010070	42.092634
3505.257490	517287.783731	42.097639
3504.932140	517278.682331	42.102644
3504.919990	517258.052430	42.107648
3504.923469	517232.110356	42.112653
3504.740688	517216.968753	42.117658
3504.865668	517195.052891	42.122663
3505.254252	517185.130646	42.127668
3504.865022	517165.773870	42.132672
3505.161931	517145.904081	42.137677
3504.913539	517126.929550	42.142682
3504.867416	517113.435020	42.147687
3504.774048	517080.630668	42.152692
3504.804820	517061.156821	42.157696
3505.018662	517059.150862	42.162701
3504.917066	517038.180842	42.167706
3504.926069	517022.553630	42.172711
3505.080633	516993.502596	42.177716
3505.083498	516983.691762	42.182720
3505.342691	516960.793565	42.187725
3505.038437	516943.799851	42.192730
3504.920265	516926.726140	42.197735
3505.123252	516904.746997	42.202740
3504.940353	516895.167747	42.207744
3504.870113	516854.875022	42.212749
3504.573670	516851.382032	42.217754
3504.708717	516828.149287	42.222759
3505.076165	516815.094847	42.227764
3504.560015	516809.108090	42.232768
3504.698289	516773.384050	42.237773
3505.006737	516765.800430	42.242778
3504.758537	516765.536262	42.247783
3504.562899	516745.490991	42.252788
3504.588492	516724.045343	42.257792
3505.162125	516718.139167	42.262797
3504.622402	516698.148220	42.267802
3504.647799	516679.534464	42.272807
3504.633691	516670.737528	42.277812
3504.679483	516671.893427	42.282816
3504.769418	516648.920411	42.287821
3504.545544	516642.836830	42.292826
3504.788683	516620.193553	42.297831
3504.442350	516619.135768	42.302836
3504.620992	516619.158129	42.307840
3504.576149	516593.273264	42.312845
3504.827462	516581.046121	42.317850
3505.126768	516571.795036	42.322855
3504.949426	516533.844697	42.327860
3504.615767	516537.336247	42.332864
3504.770052	516525.174969	42.337869
3504.516957	516502.559389	42.342874
3504.757711	516485.428497	42.347879
3504.758590	516477.994498	42.352884
3504.275272	516467.552209	42.357888
3504.593416	516451.926172	42.362893
3504.420546	516456.606025	42.367898
3504.436339	516440.825480	42.372903
3504.459485	516414.221601	42.377908
3504.241106	516415.014701	42.382912
3504.704410	516407.153590	42.387917
3504.688647	516404.981557	42.392922
3504.572607	516380.877595	42.397927
3504.842538	516371.479329	42.402932
3504.778955	516369.871131	42.407936
3504.638717	516346.327223	42.412941
3504.223305	516335.924690	42.417946
3504.190145	516329.709710	42.422951
3504.786286	516317.883015	42.427956
3504.311009	516304.759081	42.432960
3504.577378	516296.322189	42.437965
3504.327132	516296.311192	42.442970
3504.462209	516283.798775	42.447975
3504.957814	516262.783961	42.452980
3504.583743	516253.082840	42.457984
3504.707672	516239.409010	42.462989
3504.774911	516226.755557	42.467994
3504.698184	516212.759419	42.472999
3504.654770	516210.996303	42.478004
3504.699992	516179.129125	42.483008
3504.575224	516168.882838	42.488013
3504.880623	516164.333722	42.493018
3504.828423	516145.478775	42.498023
3505.008145	516127.396301	42.503028
3504.857382	516112.198057	42.508032
3504.692448	516085.218803	42.513037
3504.704062	516090.021316	42.518042
3504.737255	516073.529668	42.523047
3504.773943	516050.159667	42.528052
3504.592180	516044.878362	42.533056
3504.894130	516024.652435	42.538061
3504.761541	516018.655341	42.543066
3504.389373	516006.071167	42.548071
3504.776197	515988.360387	42.553076
3504.535542	515982.683792	42.558080
3504.451571	515978.398454	42.563085
3504.361531	515976.339249	42.568090
3504.215742	515952.340512	42.573095
3504.483089	515937.986329	42.578100
3504.179832	515932.471328	42.583104
3504.296496	515926.637097	42.588109
3504.751066	515940.877242	42.593114
3504.318245	515923.599368	42.598119
3504.742205	515894.908418	42.603124
3504.515733	515902.580670	42.608128
3504.554163	515881.637632	42.613133
3504.297983	515864.331779	42.618138
3504.538278	515854.229891	42.623143
3504.361768	515843.839863	42.628148
3504.329255	515852.796370	42.633152
3504.508802	515835.927349	42.638157
3504.394557	515822.088529	42.643162
3503.983763	515812.291808	42.648167
3504.349856	515812.689127	42.653172
3503.787124	515823.448920	42.658176
3504.301743	515816.692020	42.663181
3504.078177	515821.228344	42.668186
3504.404463	515811.315130	42.673191
3504.740136	515784.964288	42.678196
3504.457055	515773.579604	42.683200
3504.605997	515768.245945	42.688205
3504.336030	515752.509911	42.693210
3504.615400	515743.059228	42.698215
3504.047225	515741.480144	42.703220
3504.138917	515744.348332	42.708224
3504.655636	515731.876329	42.713229
3504.672223	515727.878471	42.718234
3504.352195	515718.320214	42.723239
3504.404961	515713.659185	42.728244
3504.340768	515711.393571	42.733248
3504.526347	515697.102677	42.738253
3504.307081	515684.038937	42.743258
3504.289520	515675.090301	42.748263
3504.337191	515661.680916	42.753268
3504.688206	515667.188507	42.758272
3504.614377	515636.451716	42.763277
3504.638191	515628.153968	42.768282
3504.610907	515620.319451	42.773287
3504.522851	515619.372500	42.778292
3504.384692	515599.013322	42.783296
3504.782512	515582.058974	42.788301
3504.521183	515585.539289	42.793306
3504.666877	515558.206648	42.798311
3504.531212	515545.787041	42.803316
3504.511776	515541.895978	42.808321
3504.178251	515530.620247	42.813325
3504.152062	515516.059227	42.818330
3504.393858	515515.717595	42.823335
3504.453637	515502.963625	42.828340
3504.271865	515509.415225	42.833345
3504.337730	515501.060194	42.838349
3504.292342	515505.770738	42.843354
3504.023454	515475.418494	42.848359
3504.196485	515457.336351	42.853364
3504.457447	515471.658070	42.858369
3504.480990	515467.254460	42.863373
3504.666962	515472.636480	42.868378
3504.550277	515446.660040	42.873383
3504.319484	515436.177190	42.878388
3504.090686	515435.657062	42.883393
3504.563211	515421.421730	42.888397
3504.147361	515425.937977	42.893402
3504.206833	515420.618347	42.898407
3504.528639	515399.124179	42.903412
3504.342647	515401.834016	42.908417
3504.386520	515393.229538	42.913421
3504.390800	515397.426522	42.918426
3504.335532	515384.488349	42.923431
3504.319204	515371.139420	42.928436
3504.316797	515370.583510	42.933441
3504.692199	515360.358823	42.938445
3504.359215	515360.613770	42.943450
3504.495609	515332.169600	42.948455
3504.317608	515318.340439	42.953460
3503.951150	515322.444314	42.958465
3504.537127	515315.878232	42.963469
3504.719263	515316.304638	42.968474
3504.242518	515296.858365	42.973479
3504.400594	515288.134635	42.978484
3504.126691	515279.630895	42.983489
3504.351079	515294.261993	42.988493
3504.309654	515291.385832	42.993498
3504.285629	515255.178448	42.998503
3504.266853	515230.652854	43.003508
3504.436454	515243.421402	43.008513
3504.693457	515248.539395	43.013517
3504.634929	515236.107366	43.018522
3504.319321	515216.686107	43.023527
3504.626080	515205.005514	43.028532
3504.145091	515214.791861	43.033537
3504.489717	515194.507612	43.038541
3504.482699	515183.837512	43.043546
3504.344262	515168.333012	43.048551
3504.418432	515161.645462	43.053556
3504.205276	515165.927444	43.058561
3504.488226	515151.367823	43.063565
3504.536016	515132.394778	43.068570
3504.029286	515138.746156	43.073575
3504.174992	515127.546135	43.078580
3503.999916	515139.054294	43.083585
3504.130570	515120.573887	43.088589
3504.385413	515130.547436	43.093594
3504.270677	515117.770179	43.098599
3504.484140	515101.451379	43.103604
3504.215879	515097.700688	43.108609
3504.209258	515083.894821	43.113613
3504.478009	515095.282290	43.118618
3504.523940	515074.691079	43.123623
3504.389002	515060.854898	43.128628
3504.386487	515054.128850	43.133633
3504.475326	515049.917110	43.138637
3504.868403	515038.880234	43.143642
3504.104151	515025.295210	43.148647
3504.413930	515008.404771	43.153652
3504.216428	515013.038344	43.158657
3504.542718	515006.917787	43.163661
3504.131272	514988.927513	43.168666
3504.267967	514973.328773	43.173671
3504.683153	514976.297691	43.178676
3504.431689	514971.482238	43.183681
3504.117339	514967.890527	43.188685
3504.418398	514951.861189	43.193690
3504.395867	514926.374812	43.198695
3504.347042	514930.276855	43.203700
3504.039594	514929.212813	43.208705
3504.487985	514920.190131	43.213709
3504.396956	514941.800214	43.218714
3504.214848	514913.607972	43.223719
3504.425700	514896.176726	43.228724
3504.379082	514906.552081	43.233729
3504.591136	514893.318402	43.238733
3504.207511	514877.194902	43.243738
3504.100189	514861.735776	43.248743
3504.272282	514855.841836	43.253748
3504.160804	514853.330700	43.258753
3504.434020	514851.618549	43.263757
3504.421542	514861.887385	43.268762
3503.962315	514840.920546	43.273767
3504.575644	514816.345018	43.278772
3504.309160	514822.253939	43.283777
3504.553672	514814.628966	43.288781
3504.429246	514816.216501	43.293786
3504.092048	514801.956892	43.298791
3504.047008	514789.674126	43.303796
3504.051991	514788.054938	43.308801
3504.223049	514783.728985	43.313805
3504.220594	514777.862605	43.318810
3504.215769	514775.587480	43.323815
3504.493326	514781.865613	43.328820
3503.998176	514787.456655	43.333825
3504.262261	514772.343352	43.338829
3504.243734	514758.842554	43.343834
3504.701736	514746.025070	43.348839
3504.651091	514752.051630	43.353844
3504.181015	514756.070866	43.358849
3504.525006	514735.482707	43.363853
3504.426805	514725.838245	43.368858
3504.309625	514723.732598	43.373863
3504.580302	514711.298725	43.378868
3504.040647	514699.448098	43.383873
3504.377389	514680.024265	43.388877
3504.067064	514678.252595	43.393882
3504.287787	514670.884197	43.398887
3504.621059	514678.569695	43.403892
3504.035399	514680.685325	43.408897
3504.561126	514658.045304	43.413901
3504.225050	514645.252092	43.418906
3504.070295	514637.690141	43.423911
3504.348157	514634.004761	43.428916
3504.323828	514628.344091	43.433921
3504.603692	514620.359409	43.438925
3504.268951	514605.542904	43.443930
3504.847723	514594.375236	43.448935
3504.571941	514594.418846	43.453940
3504.401139	514593.434338	43.458945
3504.116418	514557.620681	43.463949
3504.338115	514561.126019	43.468954
3504.447658	514557.214342	43.473959
3504.767852	514551.145159	43.478964
3504.343047	514535.027838	43.483969
3504.584088	514520.626023	43.488973
3504.368721	514514.641470	43.493978
3504.362830	514516.513760	43.498983
3504.527650	514497.572077	43.503988
3504.538017	514488.112626	43.508993
3504.620519	514477.984272	43.513997
3504.619004	514481.777788	43.519002
3504.454848	514465.973242	43.524007
3504.279895	514449.108274	43.529012
3504.498279	514450.034743	43.534017
3504.535715	514435.665034	43.539021
3504.196480	514417.207540	43.544026
3504.568185	514393.579967	43.549031
3504.303128	514397.010539	43.554036
3504.344250	514401.758297	43.559041
3504.648270	514386.941798	43.564045
3504.247353	514369.151501	43.569050
3504.374526	514361.646022	43.574055
3504.617332	514348.053013	43.579060
3504.396978	514366.093303	43.584065
3504.818376	514328.296205	43.589069
3504.661889	514321.139003	43.594074
3504.287284	514308.452777	43.599079
3504.579499	514308.356040	43.604084
3504.250392	514297.989167	43.609089
3504.426301	514267.311545	43.614093
3504.350247	514268.132827	43.619098
3504.243987	514259.298607	43.624103
3504.230798	514269.062146	43.629108
3504.325667	514258.881127	43.634113
3504.304276	514235.467193	43.639117
3504.344895	514239.709302	43.644122
3504.199124	514228.352439	43.649127
3504.496143	514231.744787	43.654132
3504.258068	514227.230467	43.659137
3504.231601	514202.957472	43.664141
3504.250852	514197.138035	43.669146
3504.231684	514206.143892	43.674151
3503.946147	514200.069162	43.679156
3504.152295	514206.864573	43.684161
3504.406753	514190.184365	43.689165
3504.368429	514199.395563	43.694170
3504.082459	514174.657765	43.699175
3504.250372	514155.462320	43.704180
3504.590982	514167.547152	43.709185
3504.630004	514151.406731	43.714189
3504.651220	514152.111490	43.719194
3504.391161	514139.103566	43.724199
3504.517525	514133.772956	43.729204
3504.179130	514131.145841	43.734209
3504.190500	514121.433136	43.739213
3504.322866	514100.675335	43.744218
3504.486499	514082.896663	43.749223
3504.338749	514087.522627	43.754228
3504.105199	514097.371670	43.759233
3504.244362	514082.783271	43.764237
3504.565953	514078.079301	43.769242
3504.106014	514061.360140	43.774247
3504.536496	514062.050797	43.779252
3504.400311	514060.555006	43.784257
3504.704085	514049.278707	43.789261
3504.439743	514021.856631	43.794266
3504.561328	514012.682803	43.799271
3504.359622	514004.369315	43.804276
3504.383032	514014.734155	43.809281
3504.629286	513982.932178	43.814285
3504.628679	513969.832538	43.819290
3504.336390	513974.936581	43.824295
3504.179386	513973.949855	43.829300
3504.326278	513955.566755	43.834305
3504.214917	513931.660834	43.839309
3504.622775	513940.346451	43.844314
3504.321864	513937.612224	43.849319
3504.424200	513920.551166	43.854324
3504.326566	513908.781851	43.859329
3504.193092	513894.944476	43.864333
3504.379099	513889.503206	43.869338
3504.485644	513889.182920	43.874343
3504.281839	513887.849535	43.879348
3504.319723	513863.616458	43.884353
3504.482071	513854.436102	43.889357
3504.393176	513856.979105	43.894362
3504.037836	513850.257758	43.899367
3504.815695	513839.563913	43.904372
3504.029447	513838.727207	43.909377
3504.217148	513823.119338	43.914381
3504.156917	513805.982699	43.919386
3504.103984	513807.559029	43.924391
3504.162881	513811.343149	43.929396
3504.396959	513812.874118	43.934401
3504.507875	513803.398390	43.939405
3504.271490	513778.905066	43.944410
3504.365207	513777.120020	43.949415
3504.434622	513752.932379	43.954420
3504.109158	513773.468282	43.959425
3503.663653	513764.333366	43.964429
3504.033276	513762.858764	43.969434
3504.364848	513776.917882	43.974439
3504.308337	513744.960991	43.979444
3504.050377	513738.274788	43.984449
3504.246365	513723.727675	43.989453
3504.081658	513728.710470	43.994458
3503.832858	513732.846712	43.999463
3504.302477	513737.577514	44.004468
3503.964444	513736.619384	44.009473
3504.234373	513735.767484	44.014477
3504.251510	513730.302273	44.019482
3504.079256	513703.016859	44.024487
3504.185257	513695.919062	44.029492
3504.204592	513696.624137	44.034497
3504.006380	513687.450096	44.039501
3504.226586	513696.064340	44.044506
3504.255359	513701.471776	44.049511
3504.701813	513689.363421	44.054516
3504.282784	513683.815392	44.059521
3504.555406	513668.750329	44.064525
3504.101401	513663.308979	44.069530
3504.557819	513656.054625	44.074535
3504.288963	513642.440755	44.079540
3504.009566	513630.548235	44.084545
3504.222313	513611.193346	44.089549
3504.153567	513618.993449	44.094554
3504.223424	513628.339599	44.099559
3504.227426	513616.806914	44.104564
3504.115781	513620.567451	44.109569
3504.203751	513610.387131	44.114573
3504.384459	513607.273256	44.119578
3504.350159	513590.435775	44.124583
3504.236256	513573.863755	44.129588
3504.017156	513591.904676	44.134593
3504.376761	513575.207242	44.139597
3504.011680	513595.597884	44.144602
3503.768454	513582.738605	44.149607
3504.347338	513578.044412	44.154612
3504.178474	513553.540088	44.159617
3504.322960	513543.553113	44.164621
3504.318942	513552.405187	44.169626
3504.376152	513543.544755	44.174631
3504.390182	513541.519380	44.179636
3504.425993	513545.762424	44.184641
3504.601858	513519.585023	44.189645
3504.263640	513517.008362	44.194650
3504.252404	513517.161901	44.199655
3504.509059	513512.670356	44.204660
3504.446905	513487.997332	44.209665
3504.269710	513475.481594	44.214669
3504.400672	513483.452515	44.219674
3504.440050	513469.941529	44.224679
3504.592489	513446.954241	44.229684
3504.094049	513439.800127	44.234689
3504.361319	513431.260495	44.239693
3504.277414	513432.892336	44.244698
3503.955115	513436.281568	44.249703
3504.230141	513424.857656	44.254708
3504.151079	513427.702649	44.259713
3504.257883	513406.088174	44.264717
3504.294143	513401.732592	44.269722
3504.525994	513386.370241	44.274727
3504.342654	513381.897622	44.279732
3504.076866	513394.989290	44.284737
3504.350601	513388.370654	44.289741
3504.438977	513368.074122	44.294746
3504.326045	513351.299410	44.299751
3504.161749	513357.243271	44.304756
3504.409636	513355.585555	44.309761
3504.676995	513358.628709	44.314765
3504.134431	513337.571997	44.319770
3504.238650	513321.774538	44.324775
3504.445936	513316.076819	44.329780
3503.958479	513318.885215	44.334785
3503.874197	513312.221972	44.339789
3504.187411	513309.441162	44.344794
3504.175691	513309.695939	44.349799
3504.298755	513299.863947	44.354804
3504.369322	513293.884347	44.359809
3504.519061	513278.787777	44.364813
3504.379521	513281.743514	44.369818
3504.392079	513279.414858	44.374823
3504.711808	513248.712651	44.379828
3504.280863	513249.185428	44.384833
3504.049759	513233.794946	44.389837
3504.640252	513231.779587	44.394842
3504.469861	513224.472373	44.399847
3504.680009	513205.572653	44.404852
3504.314797	513200.825246	44.409857
3504.499711	513190.072965	44.414861
3504.645892	513184.486020	44.419866
3503.794717	513159.785477	44.424871
3504.407880	513131.970359	44.429876
3504.243686	513153.594304	44.434881
3504.502909	513142.678506	44.439885
3504.415320	513132.475063	44.444890
3504.364769	513126.008739	44.449895
3504.159064	513115.520469	44.454900
3504.039378	513107.395897	44.459905
3504.267080	513091.983354	44.464909
3504.195614	513104.538726	44.469914
3504.206963	513112.275823	44.474919
3504.378087	513093.280984	44.479924
3504.325097	513074.675611	44.484929
3504.111887	513067.324515	44.489933
3504.232989	513066.799590	44.494938
3503.805258	513068.738711	44.499943
3504.454607	513052.601939	44.504948
3504.063261	513071.935163	44.509953
3504.095878	513054.732504	44.514957
3504.335395	513032.186117	44.519962
3504.178448	513022.246475	44.524967
3504.177992	513024.118072	44.529972
3504.222793	513029.624352	44.534977
3504.400250	513027.320181	44.539981
3504.540550	513026.842802	44.544986
3504.134754	513002.830353	44.549991
3504.680814	512987.063911	44.554996
3504.265801	512989.051612	44.560001
3504.718987	512985.742815	44.565005
3504.029346	512972.498394	44.570010
3503.798822	512953.061064	44.575015
3504.056173	512943.713454	44.580020
3504.204880	512946.016716	44.585025
3504.130457	512940.565719	44.590029
3504.551691	512941.966027	44.595034
3504.247233	512950.309506	44.600039
3504.290982	512942.209605	44.605044
3503.991182	512929.561094	44.610049
3504.629315	512909.834682	44.615053
3504.497789	512909.197934	44.620058
3504.224747	512918.396348	44.625063
3504.611394	512903.160837	44.630068
3504.533320	512891.842953	44.635073
3504.213317	512878.135385	44.640077
3504.419997	512875.573668	44.645082
3504.448746	512875.316241	44.650087
3504.470719	512866.005788	44.655092
3503.754748	512851.804383	44.660097
3503.678430	512840.992004	44.665101
3504.183510	512848.044210	44.670106
3504.051822	512851.454014	44.675111
3504.258785	512834.527066	44.680116
3504.342469	512848.575557	44.685121
3504.196800	512837.065993	44.690125
3504.190247	512845.008369	44.695130
3504.322836	512835.629836	44.700135
3504.263493	512811.764685	44.705140
3504.067692	512811.289837	44.710145
3504.181727	512802.470617	44.715149
3503.987594	512798.201874	44.720154
3503.861715	512807.377089	44.725159
3504.130039	512800.405007	44.730164
3504.190885	512798.068654	44.735169
3504.701382	512801.983954	44.740173
3504.351510	512772.094853	44.745178
3504.313450	512765.070016	44.750183
3504.417985	512762.726753	44.755188
3504.283250	512763.152726	44.760193
3504.639043	512754.447018	44.765197
3504.254216	512736.348954	44.770202
3504.322057	512722.782290	44.775207
3504.461887	512714.464767	44.780212
3504.459650	512716.184933	44.785217
3504.594345	512691.580797	44.790221
3504.379021	512684.583942	44.795226
3504.228185	512673.934979	44.800231
3504.466106	512658.874501	44.805236
3504.192030	512663.621984	44.810241
3504.498419	512645.212250	44.815245
3504.546771	512633.621300	44.820250
3504.093009	512634.148281	44.825255
3504.325933	512622.224659	44.830260
3504.148329	512623.314981	44.835265
3504.502630	512597.866684	44.840269
3504.321700	512593.545220	44.845274
3504.078445	512590.548748	44.850279
3504.375661	512586.354042	44.855284
3503.938475	512589.002864	44.860289
3503.798183	512585.180799	44.865293
3504.482461	512586.741894	44.870298
3504.363266	512576.290198	44.875303
3504.398898	512556.102192	44.880308
3504.362489	512551.960206	44.885313
3504.254383	512557.642555	44.890317
3503.931623	512566.798434	44.895322
3504.310888	512545.645621	44.900327
3504.165565	512514.610921	44.905332
3504.054863	512524.542629	44.910337
3504.109709	512511.028431	44.915341
3504.272907	512514.492863	44.920346
3504.144832	512511.478172	44.925351
3504.280861	512512.721263	44.930356
3504.413490	512509.614785	44.935361
3504.279765	512501.542723	44.940365
3504.328663	512477.407080	44.945370
3504.478418	512461.652202	44.950375
3504.554964	512463.714022	44.955380
3504.003282	512479.279555	44.960385
3504.290055	512460.822138	44.965389
3504.290439	512437.351681	44.970394
3504.148425	512426.954082	44.975399
3504.168258	512424.371245	44.980404
3504.496326	512432.969089	44.985409
3504.429420	512418.664734	44.990413
3503.912785	512415.964352	44.995418
3503.973204	512406.040575	45.000423
3504.275251	512392.942460	45.005428
3504.261681	512391.882387	45.010433
3504.113506	512382.902057	45.015437
3504.717915	512383.868799	45.020442
3504.062955	512396.618083	45.025447
3504.659638	512376.037692	45.030452
3504.332830	512361.875532	45.035457
3504.330297	512345.992867	45.040461
3504.298389	512351.814991	45.045466
3504.105582	512351.238490	45.050471
3504.078972	512331.616468	45.055476
3504.029196	512323.025221	45.060481
3504.212857	512306.253177	45.065485
3504.599369	512304.522867	45.070490
3504.363176	512306.027135	45.075495
3504.617690	512302.243774	45.080500
3504.487734	512284.661360	45.085505
3504.300750	512273.360275	45.090509
3504.189362	512275.148320	45.095514
3503.788676	512271.266172	45.100519
3504.094455	512260.747115	45.105524
3504.107999	512264.842250	45.110529
3503.874503	512277.777928	45.115533
3504.241236	512265.478824	45.120538
3504.244728	512268.968547	45.125543
3504.086398	512248.456746	45.130548
3504.067926	512245.323519	45.135553
3504.602453	512228.344194	45.140557
3504.130607	512244.554909	45.145562
3504.310945	512246.752101	45.150567
3504.475236	512226.391618	45.155572
3504.478711	512200.138252	45.160577
3504.342577	512212.502173	45.165581
3504.433397	512200.853632	45.170586
3504.231444	512202.099579	45.175591
3504.604418	512192.379197	45.180596
3504.242804	512166.031729	45.185601
3504.282888	512171.083782	45.190605
3504.315601	512149.934664	45.195610
3504.110711	512162.916492	45.200615
3504.606592	512139.569645	45.205620
3504.319460	512140.980810	45.210625
3504.448449	512112.987626	45.215629
3504.364105	512110.218870	45.220634
3504.195160	512130.175607	45.225639
3504.235407	512102.044679	45.230644
3503.916983	512084.997683	45.235649
3504.285764	512072.445196	45.240653
3503.865041	512073.270474	45.245658
3503.858261	512080.606237	45.250663
3503.943275	512058.437060	45.255668
3503.664517	512084.531866	45.260673
3503.877461	512069.626564	45.265677
3504.235517	512066.990217	45.270682
3503.981534	512071.380601	45.275687
3504.016944	512076.231086	45.280692
3503.979890	512077.501564	45.285697
3504.544462	512063.451193	45.290701
3504.249435	512062.890838	45.295706
3503.798270	512072.471949	45.300711
3504.128468	512043.637506	45.305716
3503.947867	512033.751604	45.310721
3503.638212	512043.006862	45.315725
3504.199691	512015.906260	45.320730
3503.938919	512035.017692	45.325735
3504.288869	512029.145242	45.330740
3503.731834	512035.404558	45.335745
3503.817696	512046.468912	45.340749
3503.967713	512032.534619	45.345754
3503.600253	512040.382661	45.350759
3503.597450	512044.227514	45.355764
3503.586332	512037.552204	45.360769
3503.756624	512060.035193	45.365773
3504.250188	512037.346163	45.370778
3503.950877	512033.144434	45.375783
3504.280397	512047.458241	45.380788
3504.171248	512025.269124	45.385793
3504.135850	512057.597931	45.390797
3504.123077	512036.961701	45.395802
3503.774109	512063.978147	45.400807
3504.382498	512030.091903	45.405812
3504.123565	512034.381910	45.410817
3504.058136	512016.890188	45.415821
3504.269267	512003.148548	45.420826
3504.231374	512010.438675	45.425831
3504.475998	512000.738469	45.430836
3504.239568	512006.087194	45.435841
3504.327261	512002.026628	45.440845
3504.060873	511986.893506	45.445850
3503.862635	511952.426413	45.450855
3503.976659	511971.175176	45.455860
3504.300969	511962.979880	45.460865
3504.134765	511959.465274	45.465869
3504.015998	511972.433636	45.470874
3503.536971	511972.610538	45.475879
3504.311070	511963.484223	45.480884
3503.939575	511967.943790	45.485889
3504.235992	511967.492293	45.490893
3504.233229	511970.325470	45.495898
3504.227999	511957.579090	45.500903
3504.070651	511925.128850	45.505908
3503.980274	511947.653186	45.510913
3503.969696	511923.374400	45.515917
3503.708285	511945.672849	45.520922
3503.897588	511936.183687	45.525927
3504.107851	511923.757313	45.530932
3503.738361	511948.298552	45.535937
3503.837946	511924.002356	45.540941
3503.962058	511931.266913	45.545946
3504.125104	511927.042666	45.550951
3503.842658	511952.075986	45.555956
3503.961747	511932.430474	45.560961
3504.059705	511925.484959	45.565965
3504.134267	511941.002592	45.570970
3503.957045	511946.898406	45.575975
3504.251192	511928.034570	45.580980
3504.247617	511929.249184	45.585985
3504.090291	511909.748500	45.590989
3504.217591	511904.265288	45.595994
3503.808158	511899.069240	45.600999
3504.186184	511884.542361	45.606004
3503.967470	511911.184372	45.611009
3504.190912	511899.059404	45.616013
3504.208813	511897.184974	45.621018
3504.003874	511903.591028	45.626023
3504.028598	511901.513182	45.631028
3503.936316	511866.118648	45.636033
3503.715213	511871.363824	45.641037
3504.055618	511854.617146	45.646042
3504.073191	511865.591242	45.651047
3504.069657	511858.509987	45.656052
3503.812750	511856.881324	45.661057
3504.297547	511845.574949	45.666061
3504.413860	511862.755346	45.671066
3504.325068	511874.960277	45.676071
3504.253563	511853.372000	45.681076
3504.055312	511851.228220	45.686081
3504.242276	511835.466881	45.691085
3504.177978	511821.009855	45.696090
3504.139738	511816.159793	45.701095
3504.000610	511821.341444	45.706100
3504.118795	511822.385067	45.711105
3504.343859	511803.683766	45.716109
3504.393897	511812.022360	45.721114
3504.091529	511817.836828	45.726119
3504.309803	511783.455317	45.731124
3504.140610	511783.836175	45.736129
3504.066245	511791.283915	45.741133
3504.329823	511765.848709	45.746138
3504.174432	511793.138500	45.751143
3504.095657	511790.166473	45.756148
3504.041229	511785.774224	45.761153
3503.972317	511764.691272	45.766157
3504.379105	511741.105035	45.771162
3504.369373	511740.246654	45.776167
3504.025676	511748.192243	45.781172
3504.074777	511726.281234	45.786177
3504.233218	511746.136094	45.791181
3504.094529	511747.169736	45.796186
3504.485299	511740.886056	45.801191
3504.333084	511700.340986	45.806196
3504.033899	511718.750654	45.811201
3504.237351	511702.076056	45.816205
3504.172859	511700.265211	45.821210
3503.965639	511693.974855	45.826215
3504.275441	511699.844366	45.831220
3503.816461	511705.430699	45.836225
3504.096555	511688.541635	45.841229
3504.296406	511689.673529	45.846234
3504.108145	511671.442088	45.851239
3504.421146	511658.847528	45.856244
3503.972490	511676.977353	45.861249
3504.124157	511658.641588	45.866253
3504.176080	511662.224952	45.871258
3504.112120	511658.340028	45.876263
3504.319940	511659.116569	45.881268
3503.941284	511644.658492	45.886273
3504.062334	511629.008549	45.891277
3504.150455	511633.800244	45.896282
3504.135478	511645.639576	45.901287
3504.044632	511629.921954	45.906292
3503.681850	511649.049942	45.911297
3504.016907	511628.054730	45.916301
3504.388752	511627.641888	45.921306
3504.230404	511642.943678	45.926311
3504.691505	511622.889657	45.931316
3504.371911	511606.348216	45.936321
3504.380519	511585.303375	45.941325
3504.688784	511584.951166	45.946330
3504.266127	511583.955697	45.951335
3504.471902	511549.828616	45.956340
3503.974583	511546.366256	45.961345
3504.230476	511550.625603	45.966349
3504.390816	511547.969841	45.971354
3504.012401	511555.313982	45.976359
3504.475882	511549.069325	45.981364
3504.326394	511530.679848	45.986369
3503.942488	511502.007935	45.991373
3503.687390	511509.990219	45.996378
3503.819055	511520.693578	46.001383
3504.094419	511499.252371	46.006388
3504.314070	511508.070164	46.011393
3503.981484	511514.698880	46.016397
3504.271595	511513.034314	46.021402
3504.237887	511486.431622	46.026407
3504.285443	511518.798930	46.031412
3504.039864	511484.490126	46.036417
3503.789060	511481.848747	46.041421
3504.093272	511461.667576	46.046426
3503.795928	511481.088925	46.051431
3504.346208	511458.288988	46.056436
3504.003900	511474.581134	46.061441
3504.028033	511489.550707	46.066445
3504.316065	511483.434928	46.071450
3503.989463	511480.046744	46.076455
3504.597203	511479.444859	46.081460
3504.231555	511463.011728	46.086465
3504.036871	511443.111727	46.091469
3504.186719	511435.449610	46.096474
3504.374693	511447.611105	46.101479
3504.422148	511433.894874	46.106484
3504.302314	511435.178483	46.111489
3504.298552	511411.656676	46.116493
3504.201216	511410.205093	46.121498
3504.397689	511402.839108	46.126503
3504.292112	511389.804645	46.131508
3504.230065	511390.623851	46.136513
3504.031348	511406.286336	46.141517
3504.640008	511383.072385	46.146522
3504.344080	511360.760161	46.151527
3504.272729	511349.389597	46.156532
3504.258636	511359.256132	46.161537
3503.948669	511358.849871	46.166541
3504.355636	511353.676383	46.171546
3504.050522	511334.198395	46.176551
3504.332167	511314.324132	46.181556
3504.017464	511318.876064	46.186561
3504.403318	511313.705901	46.191565
3503.948517	511316.762390	46.196570
3504.156048	511313.542685	46.201575
3504.132701	511310.511227	46.206580
3504.150678	511323.407886	46.211585
3503.876565	511315.863307	46.216589
3504.106982	511306.468468	46.221594
3504.370823	511291.402682	46.226599
3504.567525	511272.604107	46.231604
3504.106901	511287.650473	46.236609
3504.376773	511267.879189	46.241613
3503.986506	511278.614605	46.246618
3504.300978	511266.323040	46.251623
3504.021475	511253.012443	46.256628
3504.182939	511239.783901	46.261633
3503.970352	511233.393049	46.266637
3504.286900	511238.856963	46.271642
3503.973538	511237.894785	46.276647
3504.610205	511226.715757	46.281652
3504.295050	511238.602815	46.286657
3504.132638	511215.409329	46.291661
3504.499537	511195.572040	46.296666
3504.021175	511192.207783	46.301671
3504.110791	511181.115186	46.306676
3504.035227	511192.913822	46.311681
3503.827784	511211.663644	46.316685
3504.375100	511200.954000	46.321690
3504.536050	511190.406586	46.326695
3504.224478	511160.761520	46.331700
3503.986263	511162.165032	46.336705
3504.192091	511146.956527	46.341709
3504.179684	511146.351472	46.346714
3503.582916	511165.314638	46.351719
3504.068677	511165.844928	46.356724
3504.140951	511153.793907	46.361729
3504.151497	511154.196958	46.366733
3504.038999	511150.066655	46.371738
3503.930499	511161.415239	46.376743
3504.160596	511134.770303	46.381748
3503.995628	511136.668108	46.386753
3504.175355	511116.354442	46.391757
3504.136515	511106.395007	46.396762
3504.263476	511120.741612	46.401767
3504.534127	511108.659206	46.406772
3504.145493	511121.670869	46.411777
3503.978350	511107.229490	46.416781
3504.154123	511096.072633	46.421786
3504.088479	511080.805801	46.426791
3504.341741	511072.267200	46.431796
3503.881755	511074.312813	46.436801
3504.109982	511080.903649	46.441805
3504.176854	511076.087349	46.446810
3504.065334	511079.342560	46.451815
3504.478097	511052.719212	46.456820
3504.195478	511058.379056	46.461825
3504.219882	511046.335525	46.466829
3504.002362	511047.735776	46.471834
3504.090060	511032.899949	46.476839
3504.243019	511025.591265	46.481844
3503.931628	511030.193337	46.486849
3504.377762	511027.745260	46.491853
3504.132099	511023.332451	46.496858
3504.145859	511026.466697	46.501863
3504.269089	511007.831203	46.506868
3504.345884	511001.596876	46.511873
3503.894080	511007.081127	46.516877
3504.300689	510996.747703	46.521882
3504.167689	511000.562782	46.526887
3504.357891	510994.462290	46.531892
3504.219458	511008.092127	46.536897
3504.262070	510991.897538	46.541901
3504.421268	510955.500205	46.546906
3504.364235	510962.338521	46.551911
3504.188578	510960.798103	46.556916
3504.202988	510969.598027	46.561921
3504.227421	510960.994361	46.566925
3504.301882	510937.712472	46.571930
3504.127145	510922.108628	46.576935
3504.000309	510911.201827	46.581940
3503.942760	510928.005950	46.586945
3503.936849	510910.908380	46.591949
3504.249197	510914.501330	46.596954
3504.036446	510918.177269	46.601959
3503.934579	510925.174448	46.606964
3503.758790	510925.101081	46.611969
3503.836204	510927.112363	46.616973
3504.071977	510922.269326	46.621978
3503.964294	510924.461625	46.626983
3504.255656	510905.698272	46.631988
3504.355217	510896.323889	46.636993
3504.047464	510886.862114	46.641997
3504.040101	510872.597633	46.647002
3504.208939	510873.532135	46.652007
3504.312003	510872.150007	46.657012
3504.004852	510884.896034	46.662017
3504.112316	510877.796827	46.667021
3504.365819	510883.776695	46.672026
3504.319342	510878.421793	46.677031
3504.442937	510849.415631	46.682036
3504.360332	510845.280530	46.687041
3504.315105	510859.249868	46.692045
3504.318960	510842.555387	46.697050
3503.903437	510825.370707	46.702055
3504.203623	510816.672799	46.707060
3504.089905	510805.207392	46.712065
3504.360263	510793.883626	46.717069
3504.162613	510806.662992	46.722074
3504.223470	510798.609953	46.727079
3504.226374	510791.274297	46.732084
3504.206706	510787.736287	46.737089
3504.168096	510773.628425	46.742093
3504.357988	510759.130322	46.747098
3504.030393	510756.298615	46.752103
3503.917940	510754.950540	46.757108
3503.622341	510763.496040	46.762113
3503.822770	510759.316184	46.767117
3503.981137	510765.665245	46.772122
3503.978443	510762.377486	46.777127
3504.023854	510752.708056	46.782132
3504.032097	510757.866737	46.787137
3503.883550	510750.403237	46.792141
3504.321814	510754.178672	46.797146
3503.620406	510754.340140	46.802151
3504.066388	510758.771995	46.807156
3504.128744	510761.746846	46.812161
3503.909361	510740.635818	46.817165
3504.300874	510734.806944	46.822170
3504.004217	510724.685681	46.827175
3504.581217	510715.235741	46.832180
3504.236622	510727.077219	46.837185
3504.028287	510717.093757	46.842189
3503.979428	510712.497998	46.847194
3504.105780	510720.167423	46.852199
3504.234224	510705.982514	46.857204
3503.947431	510693.583214	46.862209
3504.357695	510668.527892	46.867213
3504.426629	510668.820550	46.872218
3503.810278	510680.401482	46.877223
3503.911332	510675.731432	46.882228
3504.087612	510677.423590	46.887233
3504.124277	510683.538976	46.892237
3503.803540	510674.433250	46.897242
3504.128903	510682.374767	46.902247
3504.484363	510669.418651	46.907252
3504.202582	510653.224421	46.912257
3504.105012	510643.577527	46.917261
3504.078350	510636.701771	46.922266
3504.224041	510643.255233	46.927271
3504.237776	510638.194268	46.932276
3504.170853	510646.400155	46.937281
3504.251283	510638.141593	46.942285
3504.016737	510621.636339	46.947290
3503.848152	510610.331237	46.952295
3503.942934	510598.377443	46.957300
3503.818739	510601.837101	46.962305
3503.818219	510590.505424	46.967309
3504.422563	510599.161713	46.972314
3503.922890	510597.368941	46.977319
3503.957130	510595.441198	46.982324
3503.966332	510597.564477	46.987329
3503.905263	510605.769458	46.992333
3504.295295	510599.333713	46.997338
3504.187394	510601.222558	47.002343
3504.210443	510596.615403	47.007348
3504.108933	510600.223240	47.012353
3504.126788	510578.467456	47.017357
3504.220657	510563.782010	47.022362
3503.811295	510559.749071	47.027367
3504.112119	510562.433326	47.032372
3504.207538	510566.617107	47.037377
3504.172931	510557.213155	47.042381
3504.207844	510552.047640	47.047386
3504.210750	510561.810773	47.052391
3504.403204	510543.113242	47.057396
3504.056309	510530.571557	47.062401
3503.934437	510516.577818	47.067405
3503.991323	510518.339451	47.072410
3503.910693	510523.562838	47.077415
3504.171765	510523.774543	47.082420
3504.205307	510518.153938	47.087425
3504.460388	510522.059554	47.092429
3504.289126	510525.577254	47.097434
3504.255206	510502.463666	47.102439
3504.377189	510482.866612	47.107444
3504.355197	510479.683027	47.112449
3504.136273	510481.943552	47.117453
3504.376170	510478.769164	47.122458
3503.980180	510476.959993	47.127463
3504.422633	510449.369828	47.132468
3504.272724	510443.019361	47.137473
3504.461508	510440.965997	47.142477
3504.145710	510436.412352	47.147482
3504.151825	510445.112680	47.152487
3504.374928	510429.698451	47.157492
3504.233944	510418.692393	47.162497
3504.181204	510397.807546	47.167501
3504.277846	510387.472156	47.172506
3504.217059	510394.614826	47.177511
3504.147391	510400.645941	47.182516
3504.218440	510400.584147	47.187521
3504.513205	510381.414970	47.192525
3504.370737	510374.557411	47.197530
3504.140214	510374.442102	47.202535
3504.264419	510360.662289	47.207540
3503.754207	510361.855909	47.212545
3503.950202	510370.728621	47.217549
3504.211987	510365.426015	47.222554
3504.441466	510362.202663	47.227559
3504.192467	510342.259369	47.232564
3504.282485	510330.559086	47.237569
3504.367365	510331.709244	47.242573
3504.286463	510324.993703	47.247578
3504.250203	510327.275968	47.252583
3504.279823	510320.947670	47.257588
3504.405153	510295.329765	47.262593
3503.988617	510291.399073	47.267597
3504.395410	510281.419314	47.272602
3504.062028	510285.772114	47.277607
3504.274002	510278.352606	47.282612
3504.149851	510268.760289	47.287617
3504.351359	510271.814412	47.292621
3504.288546	510244.657898	47.297626
3503.874853	510240.220852	47.302631
3504.237206	510232.018716	47.307636
3503.798288	510230.013944	47.312641
3503.837878	510226.314684	47.317645
3504.292935	510235.045344	47.322650
3504.014926	510233.723393	47.327655
3504.034510	510240.701657	47.332660
3503.869805	510245.685470	47.337665
3504.295725	510240.609831	47.342669
3504.068158	510220.814776	47.347674
3504.055277	510198.759829	47.352679
3504.309669	510200.540869	47.357684
3504.172413	510204.154440	47.362689
3504.185384	510196.766348	47.367693
3504.493577	510192.721092	47.372698
3504.133198	510206.943131	47.377703
3503.985709	510195.027346	47.382708
3504.051798	510186.011990	47.387713
3504.221760	510159.273856	47.392717
3504.282907	510165.031431	47.397722
3503.813464	510156.707775	47.402727
3503.972592	510148.284770	47.407732
3504.164405	510155.893513	47.412737
3504.187084	510156.598208	47.417741
3504.003046	510160.472129	47.422746
3503.904878	510161.550051	47.427751
3504.267757	510160.784468	47.432756
3504.356695	510156.419729	47.437761
3504.218595	510136.610436	47.442765
3504.320996	510116.914878	47.447770
3504.073107	510117.459978	47.452775
3504.457231	510115.223933	47.457780
3504.243870	510119.507217	47.462785
3504.350762	510116.758501	47.467789
3504.503698	510087.948768	47.472794
3504.234334	510078.278115	47.477799
3504.249488	510063.149371	47.482804
3504.201803	510077.676227	47.487809
3504.330172	510071.838128	47.492813
3504.412419	510057.659983	47.497818
3504.113921	510045.262060	47.502823
3504.409629	510032.264316	47.507828
3504.203455	510040.543092	47.512833
3504.046512	510031.866444	47.517837
3504.463922	510044.751530	47.522842
3504.361292	510017.752719	47.527847
3504.356954	510000.805759	47.532852
3504.465919	510005.999339	47.537857
3504.468515	509991.530188	47.542861
3504.554643	509986.356408	47.547866
3504.219171	509966.325161	47.552871
3504.063283	509950.666858	47.557876
3504.297354	509949.668674	47.562881
3504.347769	509951.734929	47.567885
3504.085273	509937.358219	47.572890
3504.153900	509947.617219	47.577895
3504.443482	509929.966062	47.582900
3504.029677	509914.297899	47.587905
3503.964427	509906.669093	47.592909
3503.978372	509902.872636	47.597914
3503.757416	509904.728835	47.602919
3504.057941	509893.298525	47.607924
3504.231843	509892.259256	47.612929
3504.191499	509897.881191	47.617933
3503.636262	509899.840813	47.622938
3503.743479	509896.282565	47.627943
3504.211863	509895.905019	47.632948
3504.327884	509907.826035	47.637953
3504.277466	509899.891340	47.642957
3504.268318	509873.130477	47.647962
3503.885675	509872.634482	47.652967
3504.023391	509865.934798	47.657972
3503.588953	509876.779253	47.662977
3504.028232	509878.379335	47.667981
3504.013370	509872.310854	47.672986
3503.847364	509871.982982	47.677991
3504.229394	509867.217713	47.682996
3503.884678	509873.545437	47.688001
3503.939011	509879.810089	47.693005
3504.165422	509870.465686	47.698010
3503.930165	509885.123531	47.703015
3504.000331	509879.749880	47.708020
3504.225477	509876.122398	47.713025
3504.135758	509857.114582	47.718029
3504.233868	509836.002845	47.723034
3504.030493	509826.422801	47.728039
3504.470280	509816.488149	47.733044
3504.285047	509829.772187	47.738049
3503.991823	509829.970327	47.743053
3504.461037	509831.818635	47.748058
3503.890229	509808.283056	47.753063
3503.927062	509791.025837	47.758068
3504.378926	509784.327062	47.763073
3504.151708	509786.487808	47.768077
3504.185052	509783.700072	47.773082
3503.789627	509793.071283	47.778087
3504.176486	509784.156791	47.783092
3503.859374	509777.478366	47.788097
3503.951837	509785.507703	47.793101
3504.068532	509778.355991	47.798106
3503.898189	509781.114837	47.803111
3504.025280	509784.180809	47.808116
3504.123527	509791.045642	47.813121
3504.085400	509765.756322	47.818125
3504.263962	509751.006202	47.823130
3504.030624	509762.122491	47.828135
3504.264643	509743.468109	47.833140
3504.317018	509748.265985	47.838145
3503.888404	509747.119570	47.843149
3504.128421	509748.194658	47.848154
3503.886350	509738.974817	47.853159
3504.152359	509743.738930	47.858164
3504.330671	509745.835587	47.863169
3504.133518	509721.127834	47.868173
3504.018148	509720.083683	47.873178
3503.920838	509718.277814	47.878183
3504.199746	509712.365210	47.883188
3504.242753	509714.887983	47.888193
3504.185018	509721.524542	47.893197
3504.375147	509717.750789	47.898202
3504.034665	509704.043890	47.903207
3504.437819	509676.458692	47.908212
3504.295211	509663.479353	47.913217
3504.090566	509670.392106	47.918221
3504.242436	509670.115172	47.923226
3503.882170	509678.469067	47.928231
3503.674598	509676.832394	47.933236
3503.789050	509668.011485	47.938241
3503.712301	509673.689838	47.943245
3504.089980	509666.648604	47.948250
3503.976727	509666.514755	47.953255
3504.091715	509666.698970	47.958260
3504.371589	509672.624505	47.963265
3503.989006	509657.153536	47.968269
3504.297261	509633.377599	47.973274
3504.102130	509631.890728	47.978279
3504.396809	509626.785061	47.983284
3504.468185	509627.178534	47.988289
3504.219798	509623.727022	47.993293
3504.021069	509602.358366	47.998298
3503.550353	509589.633192	48.003303
3504.021857	509583.892469	48.008308
3504.010055	509594.720897	48.013313
3503.817119	509588.326320	48.018317
3504.260989	509582.337008	48.023322
3503.828074	509594.041453	48.028327
3503.938598	509595.288791	48.033332
3504.340822	509582.729193	48.038337
3504.372925	509592.589447	48.043341
3504.266342	509582.032734	48.048346
3503.924999	509584.515090	48.053351
3504.098689	509572.396335	48.058356
3504.342269	509565.224480	48.063361
3504.286734	509557.442208	48.068365
3504.209447	509552.850630	48.073370
3504.096446	509554.234482	48.078375
3504.249452	509560.787205	48.083380
3504.158754	509548.963176	48.088385
3503.992434	509552.277928	48.093389
3504.274375	509536.701823	48.098394
3504.364940	509521.004175	48.103399
3504.403481	509513.510564	48.108404
3504.200675	509495.785008	48.113409
3503.948304	509504.071343	48.118413
3504.274918	509493.648476	48.123418
3504.019714	509511.294696	48.128423
3504.275166	509495.318007	48.133428
3504.065597	509478.655925	48.138433
3503.905090	509475.696411	48.143437
3504.331437	509463.638830	48.148442
3503.808212	509469.033673	48.153447
3503.864694	509460.323004	48.158452
3503.561002	509459.915701	48.163457
3503.749837	509459.683513	48.168461
3504.274548	509456.615698	48.173466
3503.757587	509462.970795	48.178471
3504.266128	509452.417966	48.183476
3504.009772	509463.892228	48.188481
3503.572689	509462.595357	48.193485
3504.334904	509458.478172	48.198490
3504.109115	509467.974524	48.203495
3504.189932	509461.030717	48.208500
3504.119743	509447.584442	48.213505
3503.740632	509441.421602	48.218509
3504.140806	509420.565163	48.223514
3503.824415	509423.245966	48.228519
3503.845095	509423.495680	48.233524
3504.010397	509426.302719	48.238529
3503.786558	509412.577150	48.243533
3503.961545	509417.811067	48.248538
3503.874707	509427.690214	48.253543
3503.869925	509426.932118	48.258548
3503.723905	509428.624748	48.263553
3504.097947	509429.628083	48.268557
3504.202841	509419.139029	48.273562
3503.891500	509430.318453	48.278567
3503.801138	509427.803170	48.283572
3503.862634	509423.847316	48.288577
3504.012492	509426.302653	48.293581
3504.206769	509423.843566	48.298586
3503.958982	509425.501689	48.303591
3504.272169	509417.053977	48.308596
3504.080484	509423.964781	48.313601
3503.815332	509418.998124	48.318605
3504.113534	509393.351547	48.323610
3504.066389	509396.293351	48.328615
3504.288452	509385.937534	48.333620
3504.348729	509391.746099	48.338625
3504.366053	509397.713226	48.343629
3504.226925	509393.080787	48.348634
3504.139494	509395.624223	48.353639
3504.305472	509356.237495	48.358644
3504.301729	509349.155231	48.363649
3504.169974	509351.402126	48.368653
3504.566163	509341.018762	48.373658
3504.217483	509347.650857	48.378663
3504.247216	509336.718304	48.383668
3504.191026	509316.945708	48.388673
3504.222200	509310.161462	48.393677
3504.321690	509297.092990	48.398682
3503.976164	509312.881778	48.403687
3503.938337	509294.421649	48.408692
3504.154429	509300.711540	48.413697
3504.281813	509304.283474	48.418701
3504.437310	509294.393452	48.423706
3504.083222	509284.836924	48.428711
3504.364556	509263.847302	48.433716
3504.344420	509252.467246	48.438721
3504.133559	509263.732082	48.443725
3504.000334	509259.655188	48.448730
3504.092139	509262.979792	48.453735
3504.360950	509252.414138	48.458740
3504.016372	509237.948628	48.463745
3503.876097	509232.203295	48.468749
3504.338481	509227.931074	48.473754
3504.224846	509231.541115	48.478759
3504.335304	509224.339566	48.483764
3504.069576	509228.479570	48.488769
3504.208261	509221.577112	48.493773
3504.249115	509210.895683	48.498778
3503.974068	509186.401839	48.503783
3504.103517	509173.227352	48.508788
3504.142961	509166.897075	48.513793
3504.141142	509168.617533	48.518797
3504.379396	509170.148271	48.523802
3504.124784	509169.480240	48.528807
3504.380799	509164.684102	48.533812
3503.983461	509150.985745	48.538817
3503.892016	509136.176586	48.543821
3503.906853	509129.445444	48.548826
3503.959923	509128.121671	48.553831
3503.739549	509133.215790	48.558836
3504.044265	509124.617495	48.563841
3503.959605	509130.246685	48.568845
3504.165182	509131.883776	48.573850
3504.216461	509120.289975	48.578855
3504.154523	509121.261049	48.583860
3504.126914	509136.089086	48.588865
3503.870596	509126.921758	48.593869
3504.292796	509131.914320	48.598874
3503.995327	509134.743954	48.603879
3504.146001	509101.126619	48.608884
3503.991169	509095.585911	48.613889
3503.942225	509089.218983	48.618893
3504.259213	509077.229009	48.623898
3503.829736	509098.292914	48.628903
3503.936652	509095.189882	48.633908
3503.932038	509086.893421	48.638913
3503.896097	509097.877756	48.643917
3504.149276	509091.361892	48.648922
3504.042746	509100.991376	48.653927
3504.372133	509096.183623	48.658932
3504.134500	509100.825145	48.663937
3503.736952	509101.697484	48.668941
3504.095749	509084.945190	48.673946
3503.749887	509090.160340	48.678951
3504.089857	509083.883721	48.683956
3503.931457	509071.715913	48.688961
3503.727754	509074.986073	48.693965
3504.275999	509061.593532	48.698970
3503.650435	509070.040244	48.703975
3503.964049	509071.710858	48.708980
3503.872957	509066.817775	48.713985
3503.983485	509080.409798	48.718989
3504.140922	509070.114599	48.723994
3503.930220	509073.537643	48.728999
3503.889070	509076.579740	48.734004
3503.866736	509073.598318	48.739009
3503.737667	509085.710420	48.744013
3504.009345	509066.998759	48.749018
3503.920072	509074.551224	48.754023
3504.012323	509072.765919	48.759028
3503.855047	509071.880130	48.764033
3503.869778	509077.341850	48.769037
3504.305769	509077.272966	48.774042
3503.892975	509083.510553	48.779047
3503.991533	509075.653116	48.784052
3504.096700	509071.083165	48.789057
3503.835840	509051.696761	48.794061
3504.066582	509034.205762	48.799066
3503.842626	509044.410359	48.804071
3504.004881	509035.682757	48.809076
3504.088051	509024.539188	48.814081
3504.040426	509041.191816	48.819085
3504.150806	509023.972795	48.824090
3503.968097	509034.069694	48.829095
3504.142610	509034.952809	48.834100
3504.007217	509035.429568	48.839105
3503.878223	509039.193856	48.844109
3504.642509	509016.103885	48.849114
3504.349370	509018.072772	48.854119
3504.010455	508996.927888	48.859124
3504.467147	508987.344238	48.864129
3504.153571	508987.343229	48.869133
3504.528191	508980.504572	48.874138
3504.039358	508987.310735	48.879143
3504.073635	508972.026227	48.884148
3503.924279	508948.372260	48.889153
3503.999083	508949.271139	48.894157
3504.251524	508941.338726	48.899162
3504.002466	508942.389978	48.904167
3504.279354	508940.170732	48.909172
3504.588369	508949.127507	48.914177
3504.094953	508938.176196	48.919181
3504.195977	508937.350762	48.924186
3503.941231	508919.784598	48.929191
3504.032082	508905.553548	48.934196
3503.945508	508911.233705	48.939201
3504.229067	508899.856011	48.944205
3504.396414	508899.880180	48.949210
3503.729872	508909.294720	48.954215
3503.527229	508910.642197	48.959220
3503.575711	508903.602089	48.964225
3503.835112	508907.608580	48.969229
3504.008813	508898.322573	48.974234
3503.754899	508909.898004	48.979239
3503.803452	508906.551197	48.984244
3503.877380	508909.726915	48.989249
3503.948781	508911.031080	48.994253
3504.209701	508919.388352	48.999258
3503.962303	508916.341287	49.004263
3503.996373	508912.136683	49.009268
3504.350771	508909.652217	49.014273
3504.171570	508908.415731	49.019277
3504.366351	508900.441819	49.024282
3504.177422	508886.710312	49.029287
3504.486766	508865.715777	49.034292
3504.197554	508872.186875	49.039297
3503.860975	508879.171391	49.044301
3503.941584	508874.757049	49.049306
3503.984954	508871.664021	49.054311
3504.099867	508872.910718	49.059316
3504.233105	508869.196365	49.064321
3503.905066	508854.373763	49.069325
3504.094302	508836.433782	49.074330
3503.569404	508830.749104	49.079335
3503.537020	508828.426943	49.084340
3503.993101	508836.551036	49.089345
3503.820082	508837.033747	49.094349
3504.009049	508826.784012	49.099354
3503.806103	508826.057208	49.104359
3504.027774	508826.426946	49.109364
3503.852127	508825.189892	49.114369
3503.897022	508834.036690	49.119373
3503.919333	508826.747719	49.124378
3503.881608	508835.051045	49.129383
3503.822552	508833.239036	49.134388
3504.309090	508828.153403	49.139393
3503.974138	508840.905340	49.144397
3503.977649	508837.717418	49.149402
3503.650755	508838.578604	49.154407
3503.654627	508828.509904	49.159412
3503.821999	508829.444752	49.164417
3503.618770	508829.780458	49.169421
3504.216825	508834.340565	49.174426
3503.867856	508842.996640	49.179431
3503.685709	508830.073512	49.184436
3503.974125	508843.637608	49.189441
3503.717303	508838.720059	49.194445
3503.985562	508829.621444	49.199450
3503.746689	508839.626146	49.204455
3503.998938	508832.300836	49.209460
3504.050642	508844.131570	49.214465
3503.826948	508840.321843	49.219469
3504.042075	508834.773173	49.224474
3503.988112	508842.977875	49.229479
3504.061667	508840.386005	49.234484
3504.118464	508836.582539	49.239489
3503.514404	508851.400741	49.244493
3503.864798	508842.946867	49.249498
3503.866712	508848.511873	49.254503
3504.093868	508840.886971	49.259508
3504.053147	508854.047738	49.264513
3504.019534	508844.086158	49.269517
3504.131611	508826.512517	49.274522
3504.187027	508812.135209	49.279527
3503.890235	508814.256478	49.284532
3504.164459	508799.288048	49.289537
3504.007130	508805.131204	49.294541
3504.086167	508799.300470	49.299546
3503.656109	508807.311662	49.304551
3503.579405	508808.487461	49.309556
3503.859118	508806.419533	49.314561
3503.404973	508807.857361	49.319565
3504.254502	508793.050968	49.324570
3503.990961	508810.345069	49.329575
3504.147709	508796.660043	49.334580
3504.196166	508797.259532	49.339585
3504.287032	508806.756796	49.344589
3504.008923	508804.321687	49.349594
3503.915515	508798.821770	49.354599
3504.124391	508780.575065	49.359604
3504.027478	508765.817045	49.364609
3503.736695	508772.136648	49.369613
3503.810928	508754.265351	49.374618
3503.695849	508759.747689	49.379623
3503.861363	508766.349333	49.384628
3504.200321	508768.572503	49.389633
3504.200504	508765.992218	49.394637
3504.424202	508768.992510	49.399642
3504.181462	508766.804775	49.404647
3504.587151	508767.044243	49.409652
3504.573315	508742.002544	49.414657
3503.963123	508730.007086	49.419661
3504.100315	508717.134589	49.424666
3503.920991	508726.219255	49.429671
3504.035447	508721.192399	49.434676
3504.230306	508715.950458	49.439681
3504.153844	508725.625993	49.444685
3504.101210	508716.932193	49.449690
3503.671909	508728.231902	49.454695
3503.931135	508716.351994	49.459700
3504.475722	508706.602515	49.464705
3503.882021	508704.773805	49.469709
3504.300203	508681.333335	49.474714
3504.037099	508683.398702	49.479719
3504.156157	508682.165653	49.484724
3503.873390	508677.606316	49.489729
3503.792445	508677.922697	49.494733
3503.900207	508676.387870	49.499738
3503.891011	508684.534978	49.504743
3504.142124	508669.114742	49.509748
3504.019666	508678.494010	49.514753
3504.186285	508687.220457	49.519757
3504.060413	508677.070986	49.524762
3503.948222	508643.342520	49.529767
3504.017348	508634.477651	49.534772
3504.041522	508642.417128	49.539777
3503.950400	508641.369078	49.544781
3503.966746	508630.134627	49.549786
3503.926796	508637.375923	49.554791
3503.942773	508633.983617	49.559796
3503.839465	508636.833239	49.564801
3503.549227	508636.626164	49.569805
3503.632827	508638.130798	49.574810
3503.733774	508644.388536	49.579815
3503.973512	508634.484820	49.584820
3503.864026	508639.409777	49.589825
3503.957230	508628.264365	49.594829
3504.211443	508628.730152	49.599834
3503.686503	508647.178801	49.604839
3504.184988	508633.490229	49.609844
3504.339710	508634.275306	49.614849
3504.333697	508647.734309	49.619853
3504.794812	508629.548767	49.624858
3504.386574	508609.881592	49.629863
3504.202785	508610.214228	49.634868
3503.864023	508616.389688	49.639873
3504.153317	508604.555545	49.644877
3504.138235	508604.203794	49.649882
3503.865858	508606.068258	49.654887
3504.013878	508594.205842	49.659892
3504.170025	508598.532290	49.664897
3503.901001	508592.149366	49.669901
3504.406063	508556.147621	49.674906
3504.133944	508565.854169	49.679911
3503.904769	508556.732841	49.684916
3504.104054	508555.234132	49.689921
3503.778979	508559.990807	49.694925
3503.845410	508549.507302	49.699930
3503.570456	508566.044537	49.704935
3503.642132	508557.432197	49.709940
3503.952002	508553.689860	49.714945
3503.645478	508563.907791	49.719949
3503.835166	508564.282589	49.724954
3503.873673	508556.839161	49.729959
3503.986048	508560.666594	49.734964
3503.757570	508563.788982	49.739969
3504.080635	508559.690401	49.744973
3504.141440	508551.079776	49.749978
3503.810183	508561.402806	49.754983
3504.055644	508564.045535	49.759988
3504.086608	508563.281750	49.764993
3503.797974	508570.461190	49.769997
3504.038736	508573.256443	49.775002
3503.735143	508571.432460	49.780007
3504.110430	508556.296064	49.785012
3504.011905	508559.499103	49.790017
3504.086512	508573.046611	49.795021
3504.164415	508545.814572	49.800026
3503.580497	508542.466465	49.805031
3503.797281	508521.739112	49.810036
3504.089531	508523.160185	49.815041
3503.675186	508523.832829	49.820045
3503.674453	508524.541291	49.825050
3503.604649	508545.346648	49.830055
3504.065441	508557.416490	49.835060
3503.770226	508554.933456	49.840065
3503.703811	508552.869608	49.845069
3504.013871	508563.091278	49.850074
3503.983553	508544.022024	49.855079
3503.801608	508540.610386	49.860084
3503.840688	508528.815737	49.865089
3503.801737	508532.009366	49.870093
3503.754305	508532.219264	49.875098
3503.805968	508536.511648	49.880103
3504.066112	508539.708598	49.885108
3503.985700	508528.135211	49.890113
3503.927230	508535.885422	49.895117
3504.123235	508531.756321	49.900122
3504.006048	508526.816613	49.905127
3504.056346	508538.243024	49.910132
3504.011994	508524.285999	49.915137
3504.295731	508541.139713	49.920141
3504.416769	508528.674384	49.925146
3504.180729	508537.869301	49.930151
3504.092407	508509.145644	49.935156
3503.907413	508500.219680	49.940161
3503.538557	508495.623306	49.945165
3504.147307	508485.559995	49.950170
3503.998438	508497.270885	49.955175
3503.932226	508488.882682	49.960180
3504.097690	508496.192761	49.965185
3503.963127	508498.895562	49.970189
3503.835124	508489.758208	49.975194
3504.140216	508499.272378	49.980199
3504.115000	508490.523535	49.985204
3503.972710	508500.816735	49.990209
3503.679570	508491.705482	49.995213
3504.179773	508490.614559	50.000218
3504.197496	508493.445076	50.005223
3504.013843	508504.655513	50.010228
3503.930015	508497.939717	50.015233
3503.802455	508479.897650	50.020237
3504.043587	508476.115566	50.025242
3503.734908	508471.863836	50.030247
3504.263279	508468.947055	50.035252
3504.416543	508466.241342	50.040257
3503.826010	508470.382267	50.045261
3504.091803	508470.087310	50.050266
3503.985296	508468.282762	50.055271
3503.821520	508472.811589	50.060276
3503.975312	508472.787307	50.065281
3504.086576	508477.980988	50.070285
3504.195323	508467.035393	50.075290
3503.950904	508474.359669	50.080295
3503.950945	508463.127685	50.085300
3503.902816	508451.093793	50.090305
3503.998689	508467.572513	50.095309
3504.002726	508447.435236	50.100314
3503.850151	508431.825616	50.105319
3503.919044	508433.130215	50.110324
3504.140639	508433.297595	50.115329
3504.120481	508423.536024	50.120333
3504.265321	508425.992298	50.125338
3503.870085	508439.512980	50.130343
3503.938304	508426.954736	50.135348
3503.903133	508430.754922	50.140353
3504.054699	508436.954140	50.145357
3504.111731	508416.960235	50.150362
3504.032087	508438.425008	50.155367
3503.942720	508426.802374	50.160372
3503.891748	508423.825366	50.165377
3503.838424	508426.312959	50.170381
3504.214509	508423.268455	50.175386
3504.077188	508411.147442	50.180391
3503.786517	508387.211469	50.185396
3503.720763	508385.096902	50.190401
3503.941992	508387.085755	50.195405
3504.201448	508378.342458	50.200410
3504.075805	508388.430715	50.205415
3504.008393	508392.944333	50.210420
3503.895927	508384.968149	50.215425
3504.048580	508382.869657	50.220429
3504.295531	508386.422885	50.225434
3503.666115	508396.590758	50.230439
3503.997574	508392.440215	50.235444
3504.141152	508386.042598	50.240449
3503.946452	508395.939386	50.245453
3504.037083	508387.425155	50.250458
3503.971319	508392.292677	50.255463
3503.722597	508385.552303	50.260468
3504.176617	508381.281198	50.265473
3503.910996	508381.778556	50.270477
3504.088852	508364.295237	50.275482
3504.000913	508351.458049	50.280487
3503.860681	508345.965386	50.285492
3503.999830	508343.110100	50.290497
3503.965552	508343.975656	50.295501
3504.175938	508348.141811	50.300506
3504.175697	508347.787708	50.305511
3503.992587	508341.391112	50.310516
3504.239399	508348.637803	50.315521
3504.033417	508356.310218	50.320525
3504.110169	508340.006537	50.325530
3503.976132	508341.596189	50.330535
3503.787678	508343.295632	50.335540
3504.020424	508322.767897	50.340545
3503.665194	508323.178230	50.345549
3503.864224	508317.631939	50.350554
3503.804853	508326.748452	50.355559
3503.832776	508329.324408	50.360564
3504.272363	508323.487124	50.365569
3503.993108	508328.489596	50.370573
3503.948789	508314.481801	50.375578
3504.084202	508321.088374	50.380583
3504.015592	508314.117126	50.385588
3504.290893	508314.933755	50.390593
3503.820104	508319.106385	50.395597
3504.073295	508317.953302	50.400602
3504.241677	508316.408862	50.405607
3504.148988	508311.718195	50.410612
3504.192274	508308.119129	50.415617
3504.231871	508277.806420	50.420621
3504.155416	508269.419729	50.425626
3503.755239	508273.328234	50.430631
3503.747403	508270.546762	50.435636
3504.327803	508271.770530	50.440641
3504.249328	508275.628190	50.445645
3503.860278	508277.561723	50.450650
3503.978421	508272.331773	50.455655
3504.031941	508269.692389	50.460660
3503.954159	508262.368403	50.465665
3503.668668	508277.136747	50.470669
3503.998385	508270.557883	50.475674
3503.975905	508280.781683	50.480679
3503.856639	508278.675561	50.485684
3503.887195	508263.643987	50.490689
3503.645699	508284.274414	50.495693
3503.428527	508279.451628	50.500698
3503.754250	508267.206735	50.505703
3504.110972	508274.183110	50.510708
3503.938294	508281.749104	50.515713
3504.022874	508276.069103	50.520717
3504.194386	508269.464647	50.525722
3503.804766	508253.892331	50.530727
3503.720712	508245.304448	50.535732
3503.850355	508218.215499	50.540737
3503.791714	508195.507471	50.545741
3504.010274	508152.770380	50.550746
3503.669395	508087.100565	50.555751
3503.843857	508017.756740	50.560756
3503.772882	507951.031830	50.565761
3503.445655	507863.096697	50.570765
3503.585090	507774.935570	50.575770
3503.309579	507670.395577	50.580775
3503.182394	507560.265810	50.585780
3502.974498	507432.135348	50.590785
3502.912963	507299.173992	50.595789
3502.803826	507154.733294	50.600794
3502.570196	507025.693117	50.605799
3502.736722	506862.282441	50.610804
3502.706614	506676.637386	50.615809
3501.934462	506513.574181	50.620813
3502.018184	506314.751176	50.625818
3501.643787	506122.222284	50.630823
3501.083477	505922.889369	50.635828
3500.996364	505708.349193	50.640833
3500.682191	505492.982007	50.645837
3500.157447	505258.770173	50.650842
3500.215322	505043.692868	50.655847
3499.906042	504810.149428	50.660852
3499.606233	504570.174419	50.665857
3499.084689	504324.158367	50.670861
3499.149030	504070.151510	50.675866
3498.955501	503811.019706	50.680871
3498.596251	503548.063997	50.685876
3498.162929	503276.056933	50.690881
3497.606308	502983.770347	50.695885
3497.548153	502696.866160	50.700890
3496.801907	502408.800764	50.705895
3496.774086	502099.055975	50.710900
3496.378898	501803.485118	50.715905
3495.634400	501498.853888	50.720909
3495.571525	501172.243728	50.725914
3495.395131	500855.819453	50.730919
3494.663350	500533.200767	50.735924
3494.314649	500192.546145	50.740929
3493.730933	499854.908719	50.745933
3493.522452	499515.231417	50.750938
3493.153298	499178.660975	50.755943
3492.745423	498808.932706	50.760948
3492.388988	498469.562736	50.765953
3491.486490	498105.466755	50.770957
3491.229052	497739.287075	50.775962
3490.875237	497360.812983	50.780967
3490.026729	497001.698237	50.785972
3489.673980	496614.652343	50.790977
3489.228570	496235.966730	50.795981
3488.841092	495847.087316	50.800986
3487.931006	495475.547626	50.805991
3487.748578	495072.999367	50.810996
3487.750068	494684.995747	50.816001
3486.711800	494283.831256	50.821005
3486.021833	493885.944926	50.826010
3485.570839	493472.061493	50.831015
3485.243901	493069.694703	50.836020
3484.610037	492655.214186	50.841025
3484.135881	492237.812625	50.846029
3483.421709	491819.325482	50.851034
3482.963399	491406.105970	50.856039
3482.533108	490976.717409	50.861044
3481.767283	490554.512969	50.866049
3481.019304	490142.324138	50.871053
3480.510129	489695.698852	50.876058
3480.493130	489273.043266	50.881063
3479.739337	488834.539948	50.886068
3479.209145	488392.546809	50.891073
3478.273229	487962.156151	50.896077
3477.543984	487505.484589	50.901082
3477.022113	487079.719193	50.906087
3476.368344	486618.252823	50.911092
3476.090239	486179.967434	50.916097
3475.344535	485727.055038	50.921101
3474.842126	485282.908177	50.926106
3473.910812	484837.704287	50.931111
3473.108377	484377.068555	50.936116
3472.813287	483932.249749	50.941121
3472.034976	483479.086838	50.946125
3471.975960	483021.037074	50.951130
3471.304180	482561.604016	50.956135
3470.180970	482098.228700	50.961140
3469.672539	481636.670590	50.966145
3468.940718	481184.662839	50.971149
3468.448084	480719.128287	50.976154
3467.662362	480260.165748	50.981159
3467.561136	479794.547392	50.986164
3466.488164	479323.193350	50.991169
3465.658603	478857.870696	50.996173
3465.097569	478388.693857	51.001178
3464.275529	477940.173280	51.006183
3463.505749	477470.095513	51.011188
3463.225726	477007.277946	51.016193
3462.516979	476535.597402	51.021197
3461.533176	476063.138289	51.026202
3460.973695	475597.037883	51.031207
3460.416866	475135.792060	51.036212
3459.639211	474667.575833	51.041217
3458.964093	474207.037094	51.046221
3458.323402	473735.178801	51.051226
3457.718877	473268.676980	51.056231
3456.940558	472802.141245	51.061236
3456.330544	472333.844692	51.066241
3455.183684	471869.880540	51.071245
3454.973150	471404.084947	51.076250
3454.062286	470940.265250	51.081255
3453.866793	470469.731408	51.086260
3453.153932	470007.583135	51.091265
3452.318555	469537.991106	51.096269
3451.662506	469068.917806	51.101274
3450.575669	468605.580606	51.106279
3449.968048	468132.473129	51.111284
3449.528589	467661.914260	51.116289
3448.593393	467201.817722	51.121293
3447.763408	466736.471740	51.126298
3447.097196	466264.497641	51.131303
3446.361088	465796.834252	51.136308
3446.130753	465332.934499	51.141313
3445.128204	464876.195450	51.146317
3444.557461	464403.302720	51.151322
3443.880768	463939.341710	51.156327
3442.905348	463483.633506	51.161332
3442.368758	463023.586179	51.166337
3441.316835	462563.864044	51.171341
3440.690125	462091.943471	51.176346
3439.769857	461647.041103	51.181351
3439.394861	461186.523288	51.186356
3438.768536	460723.854454	51.191361
3437.760349	460289.082209	51.196365
3437.519611	459819.485819	51.201370
3436.667765	459364.330715	51.206375
3435.528688	458908.907217	51.211380
3434.803729	458458.379922	51.216385
3434.118672	458016.714268	51.221389
3433.894932	457558.733994	51.226394
3432.951961	457116.380938	51.231399
3432.027097	456665.595064	51.236404
3431.575890	456216.500752	51.241409
3430.997200	455782.079032	51.246413
3430.156980	455322.070168	51.251418
3429.388214	454868.686698	51.256423
3428.481877	454423.433402	51.261428
3428.080931	453969.111165	51.266433
3427.312540	453537.973877	51.271437
3426.621491	453083.020123	51.276442
3425.781623	452644.063507	51.281447
3425.249524	452194.495891	51.286452
3424.487555	451753.987620	51.291457
3423.801406	451323.607228	51.296461
3422.859164	450873.672556	51.301466
3422.176709	450425.058088	51.306471
3421.488970	449992.369558	51.311476
3420.873943	449552.049585	51.316481
3419.820892	449114.683048	51.321485
3419.319102	448686.660165	51.326490
3418.799961	448246.960009	51.331495
3418.250924	447809.844518	51.336500
3417.334774	447373.946161	51.341505
3416.327544	446935.567289	51.346509
3415.625682	446511.697866	51.351514
3415.114572	446077.589283	51.356519
3414.723464	445644.874874	51.361524
3414.101114	445222.695413	51.366529
3413.165621	444793.705910	51.371533
3412.473734	444346.854514	51.376538
3411.555310	443918.607928	51.381543
3411.028634	443487.246228	51.386548
3410.439296	443059.389099	51.391553
3409.332177	442633.890448	51.396557
3408.826063	442199.558317	51.401562
3407.902277	441778.228810	51.406567
3407.329466	441363.334180	51.411572
3406.925648	440934.445649	51.416577
3406.259298	440498.027105	51.421581
3405.636277	440069.056502	51.426586
3404.540671	439653.098620	51.431591
3403.960024	439233.346250	51.436596
3403.276242	438815.151473	51.441601
3402.135065	438391.716541	51.446605
3401.759390	437970.539540	51.451610
3400.810375	437557.493247	51.456615
3400.406101	437138.845233	51.461620
3399.556565	436721.580686	51.466625
3398.718641	436306.033646	51.471629
3398.474990	435884.800587	51.476634
3397.677918	435472.863679	51.481639
3396.753523	435060.229309	51.486644
3396.059296	434638.970523	51.491649
3395.394393	434240.677018	51.496653
3394.807132	433814.284481	51.501658
3393.663969	433402.876448	51.506663
3393.319698	432996.515062	51.511668
3392.653423	432586.414961	51.516673
3391.645289	432178.622153	51.521677
3390.924861	431764.226447	51.526682
3390.241301	431366.424434	51.531687
3389.677074	430954.225523	51.536692
3389.288589	430548.137266	51.541697
3388.186603	430150.052671	51.546701
3387.877568	429739.698649	51.551706
3387.098558	429328.066636	51.556711
3385.983818	428917.395435	51.561716
3385.675407	428514.970508	51.566721
3384.637145	428120.679610	51.571725
3384.375999	427713.714725	51.576730
3383.353684	427324.386915	51.581735
3382.574859	426922.977213	51.586740
3382.090753	426515.368947	51.591745
3381.083346	426123.735573	51.596749
3380.621112	425720.962531	51.601754
3380.052545	425333.794330	51.606759
3379.371123	424930.358380	51.611764
3378.437546	424530.029464	51.616769
3377.500486	424131.828666	51.621773
3377.211869	423735.221237	51.626778
3376.590171	423351.411172	51.631783
3376.087818	422953.480006	51.636788
3374.975954	422553.836024	51.641793
3374.319387	422164.680822	51.646797
3373.937246	421773.470065	51.651802
3373.359636	421376.035986	51.656807
3372.376434	420982.038735	51.661812
3371.988299	420579.051140	51.666817
3370.923989	420187.138400	51.671821
3370.472214	419785.063870	51.676826
3369.566729	419395.451956	51.681831
3368.678292	419012.284382	51.686836
3368.257242	418622.508946	51.691841
3367.475860	418229.609598	51.696845
3366.593528	417842.284315	51.701850
3365.916586	417456.267718	51.706855
3365.349958	417067.586314	51.711860
3364.410620	416680.635305	51.716865
3363.928115	416305.572932	51.721869
3363.182725	415910.069924	51.726874
3362.628561	415537.955966	51.731879
3361.877976	415149.709573	51.736884
3361.346257	414759.416200	51.741889
3360.518089	414379.937203	51.746893
3360.072580	413995.666904	51.751898
3359.107368	413622.068896	51.756903
3358.272441	413228.194997	51.761908
3357.821622	412845.663611	51.766913
3356.644899	412466.189487	51.771917
3356.247889	412077.414386	51.776922
3355.884993	411710.328709	51.781927
3354.905230	411337.339257	51.786932
3354.501207	410949.719347	51.791937
3353.278267	410575.183356	51.796941
3352.937679	410201.519592	51.801946
3352.038047	409824.178693	51.806951
3351.651724	409447.082244	51.811956
3351.155770	409071.014896	51.816961
3349.741656	408687.667665	51.821965
3349.390870	408311.771233	51.826970
3348.855617	407951.629926	51.831975
3347.993388	407572.704871	51.836980
3347.832132	407193.638866	51.841985
3346.603574	406821.420792	51.846989
3346.005332	406459.975802	51.851994
3345.341577	406080.162284	51.856999
3344.587810	405705.187144	51.862004
3344.073908	405331.084486	51.867009
3343.551804	404965.619858	51.872013
3342.461150	404575.536809	51.877018
3342.134435	404209.397049	51.882023
3341.167540	403845.590883	51.887028
3340.587293	403468.324833	51.892033
3339.830979	403110.551449	51.897037
3339.357110	402728.964303	51.902042
3338.541057	402358.635792	51.907047
3337.811277	401992.940784	51.912052
3337.177484	401621.583601	51.917057
3336.377498	401264.253906	51.922061
3335.961627	400891.582895	51.927066
3335.260361	400521.926721	51.932071
3334.548224	400149.776953	51.937076
3334.081661	399783.100114	51.942081
3333.218400	399405.322578	51.947085
3332.747556	399029.334278	51.952090
3331.870989	398667.310766	51.957095
3330.991589	398296.310212	51.962100
3330.915812	397925.051289	51.967105
3329.780423	397558.073994	51.972109
3329.344234	397184.626681	51.977114
3328.434514	396819.766356	51.982119
3327.575218	396447.445389	51.987124
3327.068762	396072.979841	51.992129
3326.363676	395709.854598	51.997133
3325.538276	395339.956539	52.002138
3324.629026	394983.923323	52.007143
3324.526358	394628.140159	52.012148
3323.710302	394257.389806	52.017153
3322.633445	393897.024227	52.022157
3322.151089	393544.899989	52.027162
3321.413751	393168.099802	52.032167
3321.166800	392809.625499	52.037172
3320.198206	392449.990332	52.042177
3319.298581	392088.306487	52.047181
3318.606141	391720.026296	52.052186
3317.830383	391366.705794	52.057191
3317.199991	391014.452047	52.062196
3316.630685	390649.955001	52.067201
3315.685864	390297.998038	52.072205
3315.034859	389941.592237	52.077210
3314.441560	389593.869799	52.082215
3313.855099	389240.218281	52.087220
3313.311108	388879.131650	52.092225
3312.635150	388524.520921	52.097229
3311.901250	388161.600827	52.102234
3311.354651	387812.073647	52.107239
3310.134373	387455.199010	52.112244
3309.736053	387108.006418	52.117249
3308.905305	386757.191655	52.122253
3308.494566	386399.110557	52.127258
3307.542504	386048.765876	52.132263
3307.182024	385699.900933	52.137268
3306.602494	385343.412841	52.142273
3305.639322	384993.492145	52.147277
3305.315717	384631.133129	52.152282
3304.343823	384283.699294	52.157287
3303.715275	383932.596691	52.162292
3303.140957	383575.836443	52.167297
3302.382282	383225.917614	52.172301
3301.826708	382859.737889	52.177306
3301.049849	382520.318713	52.182311
3300.128585	382169.576515	52.187316
3299.548634	381810.638676	52.192321
3298.625660	381475.785672	52.197325
3298.310173	381117.613322	52.202330
3297.554263	380775.581081	52.207335
3296.686616	380431.528786	52.212340
3296.273248	380077.533298	52.217345
3295.463997	379735.423951	52.222349
3294.812892	379375.609838	52.227354
3294.489499	379041.454731	52.232359
3293.694097	378693.560424	52.237364
3292.679263	378336.770104	52.242369
3291.972677	378010.475294	52.247373
3291.548187	377655.671106	52.252378
3290.504091	377307.218861	52.257383
3289.859350	376963.736668	52.262388
3289.546801	376614.450453	52.267393
3288.560727	376280.529399	52.272397
3287.944378	375937.669798	52.277402
3287.175944	375588.192377	52.282407
3286.635229	375242.008137	52.287412
3285.901218	374902.973875	52.292417
3285.374223	374563.827732	52.297421
3284.826082	374221.960307	52.302426
3284.319967	373864.464654	52.307431
3283.126485	373527.552095	52.312436
3282.670358	373181.565956	52.317441
3282.148184	372846.525837	52.322445
3281.650223	372488.711720	52.327450
3280.725243	372157.163950	52.332455
3279.946207	371808.673584	52.337460
3279.276965	371467.667502	52.342465
3278.669964	371130.973501	52.347469
3278.046571	370779.931505	52.352474
3277.435393	370443.258131	52.357479
3276.601206	370102.521531	52.362484
3276.277390	369757.758267	52.367489
3275.319429	369414.949672	52.372493
3274.524492	369068.500000	52.377498
3273.841562	368733.758024	52.382503
3273.179170	368393.820257	52.387508
3272.708814	368042.935200	52.392513
3271.955070	367714.378778	52.397517
3271.157731	367356.441788	52.402522
3270.301870	367020.187523	52.407527
3269.885496	366688.033665	52.412532
3269.374174	366339.202286	52.417537
3268.353248	366009.734066	52.422541
3267.735800	365658.013709	52.427546
3266.919718	365332.324477	52.432551
3265.957356	365000.117194	52.437556
3265.836179	364660.624907	52.442561
3264.755837	364332.120622	52.447565
3264.648979	364005.699017	52.452570
3264.124894	363667.407994	52.457575
3263.142194	363327.507715	52.462580
3262.569862	362981.433448	52.467585
3261.719100	362650.845266	52.472589
3261.154931	362303.161645	52.477594
3260.425376	361969.699667	52.482599
3259.875317	361630.354618	52.487604
3259.211623	361292.551784	52.492609
3258.270362	360961.355272	52.497613
3257.896202	360616.529830	52.502618
3257.306854	360284.916687	52.507623
3256.143364	359956.140180	52.512628
3255.740985	359607.953066	52.517633
3255.062791	359283.319192	52.522637
3254.450113	358942.845226	52.527642
3254.112146	358608.305314	52.532647
3253.032127	358276.348784	52.537652
3252.521695	357929.489900	52.542657
3251.664041	357598.740484	52.547661
3251.228738	357255.605648	52.552666
3250.971228	356918.623990	52.557671
3249.915580	356578.865276	52.562676
3249.274540	356241.608872	52.567681
3248.357338	355911.392012	52.572685
3247.991383	355576.963218	52.577690
3247.156697	355236.753279	52.582695
3246.012659	354902.697573	52.587700
3245.726901	354565.577339	52.592705
3244.919446	354237.851592	52.597709
3244.155335	353905.128932	52.602714
3243.567407	353570.874764	52.607719
3242.901936	353236.579801	52.612724
3242.326045	352910.641326	52.617729
3241.578415	352580.783314	52.622733
3240.913605	352244.878570	52.627738
3240.315141	351922.831299	52.632743
3239.586588	351581.155310	52.637748
3239.038874	351243.520526	52.642753
3237.910226	350924.834115	52.647757
3237.202589	350585.617099	52.652762
3237.058330	350259.110451	52.657767
3236.338882	349936.535865	52.662772
3235.421706	349600.781643	52.667777
3235.136562	349279.228840	52.672781
3234.305355	348938.977568	52.677786
3233.783790	348609.797432	52.682791
3232.835890	348275.770636	52.687796
3232.437663	347944.861782	52.692801
3231.202279	347612.988956	52.697805
3230.762344	347284.627959	52.702810
3229.974229	346954.334856	52.707815
3229.330418	346628.445677	52.712820
3229.357224	346305.630091	52.717825
3228.294262	345973.516723	52.722829
3227.760457	345639.561490	52.727834
3226.652296	345313.407367	52.732839
3226.193982	344991.450154	52.737844
3225.643041	344651.255942	52.742849
3225.173856	344333.776549	52.747853
3224.333212	343997.849592	52.752858
3223.636975	343664.901389	52.757863
3223.255576	343334.472327	52.762868
3222.257753	342997.902754	52.767873
3221.317187	342672.521961	52.772877
3221.019832	342337.339650	52.777882
3220.087237	342015.695791	52.782887
3219.172997	341694.683678	52.787892
3218.745060	341352.669351	52.792897
3218.137096	341048.405354	52.797901
3217.313156	340709.377361	52.802906
3216.529195	340386.861413	52.807911
3215.989749	340062.828717	52.812916
3215.407820	339743.153890	52.817921
3214.300766	339424.375071	52.822925
3213.688103	339098.847110	52.827930
3213.176047	338775.668926	52.832935
3212.650188	338444.981859	52.837940
3212.148893	338123.198729	52.842945
3211.148097	337804.573173	52.847949
3210.621534	337474.339428	52.852954
3209.931258	337152.734095	52.857959
3208.962673	336835.244214	52.862964
3208.480742	336508.791514	52.867969
3207.889845	336186.987531	52.872973
3207.120866	335865.897487	52.877978
3206.634354	335551.456353	52.882983
3205.562113	335230.614883	52.887988
3205.393573	334896.824028	52.892993
3204.509278	334587.507273	52.897997
3203.871288	334263.817694	52.903002
3203.201051	333949.830958	52.908007
3202.480038	333628.137191	52.913012
3202.060419	333314.718899	52.918017
3200.958566	332990.180248	52.923021
3200.332970	332665.437460	52.928026
3199.844971	332348.257887	52.933031
3198.738159	332047.060642	52.938036
3198.644581	331724.164183	52.943041
3197.649212	331408.893674	52.948045
3196.924729	331097.575903	52.953050
3196.247633	330776.371378	52.958055
3195.564038	330461.862090	52.963060
3195.261790	330141.842943	52.968065
3194.481363	329826.887990	52.973069
3193.933081	329520.245519	52.978074
3193.064410	329198.784358	52.983079
3192.223352	328889.817915	52.988084
3191.788948	328571.722358	52.993089
3191.180212	328262.589296	52.998093
3190.384382	327937.546919	53.003098
3189.560200	327620.731106	53.008103
3188.858313	327304.327457	53.013108
3188.307960	326986.981990	53.018113
3187.570528	326680.867199	53.023117
3186.750943	326360.913950	53.028122
3186.214621	326058.329324	53.033127
3185.375737	325751.845075	53.038132
3184.733689	325438.301458	53.043137
3184.321797	325123.421723	53.048141
3183.677003	324814.051621	53.053146
3182.866747	324506.539684	53.058151
3181.853322	324199.287880	53.063156
3181.677918	323876.014801	53.068161
3181.041828	323580.642122	53.073165
3180.015422	323259.614534	53.078170
3179.647643	322952.459664	53.083175
3178.913597	322638.792635	53.088180
3178.183162	322327.873696	53.093185
3177.643612	322020.157023	53.098189
3177.106928	321697.365606	53.103194
3175.995222	321390.068207	53.108199
3175.484152	321082.165468	53.113204
3175.009927	320766.439066	53.118209
3173.889006	320469.350063	53.123213
3173.492604	320161.400515	53.128218
3173.342779	319841.723838	53.133223
3172.330883	319537.357825	53.138228
3171.813498	319214.427013	53.143233
3170.754802	318893.210288	53.148237
3170.109931	318587.891871	53.153242
3169.813277	318283.561319	53.158247
3168.910084	317975.582746	53.163252
3168.263876	317660.942230	53.168257
3167.540589	317353.213254	53.173261
3166.832327	317042.934633	53.178266
3166.392789	316737.246735	53.183271
3165.232850	316431.850089	53.188276
3164.745584	316126.498841	53.193281
3164.091403	315812.617454	53.198285
3163.769286	315502.069138	53.203290
3163.224157	315197.258908	53.208295
3162.122249	314887.977908	53.213300
3161.760928	314580.641330	53.218305
3161.185261	314270.969635	53.223309
3160.271038	313953.304089	53.228314
3159.653227	313635.514282	53.233319
3158.940590	313326.905450	53.238324
3158.054227	313019.469072	53.243329
3157.275821	312718.966357	53.248333
3156.705259	312408.549911	53.253338
3156.145373	312100.906459	53.258343
3155.399511	311813.000756	53.263348
3155.040612	311493.202897	53.268353
3154.468816	311195.413416	53.273357
3153.294462	310894.382655	53.278362
3153.013010	310578.491420	53.283367
3152.219186	310276.787663	53.288372
3151.551047	309963.986172	53.293377
3150.729620	309660.553580	53.298381
3149.655369	309350.615790	53.303386
3149.165260	309038.343868	53.308391
3148.496383	308739.952235	53.313396
3148.359357	308439.514918	53.318401
3147.201246	308129.765473	53.323405
3146.510612	307834.685479	53.328410
3145.779754	307531.105829	53.333415
3145.216746	307229.561550	53.338420
3144.550502	306931.012298	53.343425
3143.932710	306644.295987	53.348429
3143.274972	306331.610799	53.353434
3142.419276	306035.381297	53.358439
3141.783819	305741.357226	53.363444
3140.930118	305433.284647	53.368449
3140.387126	305138.709827	53.373453
3139.797126	304844.651107	53.378458
3138.879363	304555.380206	53.383463
3138.409541	304249.714336	53.388468
3137.689849	303958.984761	53.393473
3136.818496	303666.979820	53.398477
3136.492860	303370.151287	53.403482
3135.719988	303074.156872	53.408487
3135.199798	302789.275936	53.413492
3134.929025	302474.992719	53.418497
3133.875438	302177.563863	53.423501
3133.340762	301891.919493	53.428506
3132.748290	301584.000870	53.433511
3131.608189	301291.422505	53.438516
3131.506872	300982.406304	53.443521
3130.734330	300689.131980	53.448525
3129.882925	300394.774534	53.453530
3129.417421	300087.062039	53.458535
3128.412977	299790.384786	53.463540
3127.941527	299483.487004	53.468545
3127.600879	299196.839289	53.473549
3126.844259	298899.688281	53.478554
3126.290469	298591.936018	53.483559
3125.717258	298288.362800	53.488564
3125.080104	297977.515693	53.493569
3123.820519	297682.403092	53.498573
3123.180911	297377.820128	53.503578
3122.650978	297085.086827	53.508583
3121.796592	296785.884879	53.513588
3121.026705	296482.390635	53.518593
3120.462577	296194.143502	53.523597
3119.838312	295892.229679	53.528602
3119.421793	295592.447205	53.533607
3118.393412	295315.146625	53.538612
3117.918051	295000.372462	53.543617
3116.743146	294718.484690	53.548621
3116.647831	294423.157307	53.553626
3116.054922	294128.061040	53.558631
3115.133237	293833.703996	53.563636
3114.566520	293529.867485	53.568641
3113.758087	293245.729554	53.573645
3113.504513	292942.759494	53.578650
3112.980555	292648.006834	53.583655
3112.090124	292349.262461	53.588660
3111.440787	292047.550794	53.593665
3110.701037	291747.126418	53.598669
3109.868820	291460.570618	53.603674
3109.453862	291150.925801	53.608679
3108.129776	290864.829146	53.613684
3107.880944	290564.172829	53.618689
3107.123238	290270.167329	53.623693
3106.518592	289972.750079	53.628698
3106.148279	289678.173263	53.633703
3105.068033	289384.981851	53.638708
3104.746139	289095.948706	53.643713
3103.558436	288800.226909	53.648717
3102.779184	288500.416265	53.653722
3102.626555	288221.287892	53.658727
3101.599176	287921.897944	53.663732
3101.318471	287633.595407	53.668737
3100.236883	287348.195337	53.673741
3099.851899	287051.275159	53.678746
3098.992545	286768.106054	53.683751
3098.416349	286476.894967	53.688756
3097.840505	286174.426733	53.693761
3097.220836	285884.087940	53.698765
3096.502741	285593.306064	53.703770
3095.925676	285293.969852	53.708775
3095.171091	285013.049431	53.713780
3094.393192	284716.342294	53.718785
3093.655829	284424.492929	53.723789
3093.021397	284133.212837	53.728794
3092.585809	283848.013430	53.733799
3091.767737	283560.454891	53.738804
3091.342586	283263.869202	53.743809
3090.541519	282985.272406	53.748813
3089.695424	282682.767949	53.753818
3089.307284	282387.551150	53.758823
3088.474134	282098.899002	53.763828
3087.894344	281804.399851	53.768833
3086.988231	281520.292292	53.773837
3086.268762	281232.971528	53.778842
3085.685521	280941.197594	53.783847
3085.069472	280653.070683	53.788852
3084.453943	280362.269396	53.793857
3083.666806	280084.738660	53.798861
3083.080117	279784.331029	53.803866
3082.178693	279495.077275	53.808871
3081.646949	279219.976244	53.813876
3081.059579	278924.407390	53.818881
3080.237462	278644.385812	53.823885
3079.390617	278343.152936	53.828890
3078.965777	278055.657041	53.833895
3078.293369	277765.908101	53.838900
3077.629542	277473.891053	53.843905
3076.635882	277198.888077	53.848909
3075.990723	276901.952566	53.853914
3075.227080	276612.905486	53.858919
3074.363506	276350.335827	53.863924
3073.956636	276062.785782	53.868929
3073.314833	275798.652867	53.873933
3072.556416	275516.863322	53.878938
3072.022481	275244.537945	53.883943
3071.595914	274965.395503	53.888948
3071.026173	274674.763998	53.893953
3070.643938	274396.607797	53.898957
3069.708537	274105.371983	53.903962
3068.922937	273821.905800	53.908967
3068.372903	273539.930454	53.913972
3067.525804	273251.227551	53.918977
3066.775553	272971.015788	53.923981
3066.285220	272686.942665	53.928986
3065.648082	272400.677063	53.933991
3064.502863	272124.551920	53.938996
3063.841963	271844.020552	53.944001
3063.477609	271562.168889	53.949005
3062.808488	271287.165567	53.954010
3062.502458	271019.796286	53.959015
3061.774159	270738.562710	53.964020
3061.009106	270442.359641	53.969025
3060.154183	270163.081856	53.974029
3059.508742	269879.364982	53.979034
3058.991605	269599.371738	53.984039
3057.753255	269317.455264	53.989044
3057.573109	269037.307011	53.994049
3056.954688	268759.367562	53.999053
3055.993240	268476.872752	54.004058
3055.416783	268202.874470	54.009063
3054.678496	267923.604519	54.014068
3054.109169	267648.281002	54.019073
3053.339172	267377.955676	54.024077
3052.658949	267096.537596	54.029082
3052.439361	266823.807822	54.034087
3051.335692	266545.513231	54.039092
3050.962703	266257.272436	54.044097
3050.127402	265989.403103	54.049101
3049.418654	265710.231502	54.054106
3048.742349	265427.336588	54.059111
3048.113231	265167.584903	54.064116
3047.701986	264869.825954	54.069121
3046.896364	264590.466650	54.074125
3045.886625	264307.472440	54.079130
3045.434591	264033.049302	54.084135
3044.594178	263764.163451	54.089140
3044.440451	263476.220913	54.094145
3043.553852	263211.086568	54.099149
3042.879846	262943.066359	54.104154
3042.238924	262658.359610	54.109159
3041.333841	262384.671583	54.114164
3040.917637	262097.000928	54.119169
3039.826633	261823.673873	54.124173
3039.339522	261548.825274	54.129178
3038.737069	261268.952538	54.134183
3038.057261	261007.250854	54.139188
3037.393411	260723.899245	54.144193
3036.844581	260455.530221	54.149197
3035.911868	260178.359427	54.154202
3035.518346	259903.675806	54.159207
3034.745025	259633.560349	54.164212
3034.137860	259352.671503	54.169217
3033.419265	259084.814554	54.174221
3032.659166	258814.876101	54.179226
3032.359606	258529.686354	54.184231
3031.392125	258268.669486	54.189236
3030.966875	257986.581820	54.194241
3029.888514	257704.979859	54.199245
3029.312529	257436.821944	54.204250
3028.762375	257171.792738	54.209255
3028.351208	256887.310191	54.214260
3027.714614	256605.028401	54.219265
3026.854626	256338.903156	54.224269
3026.005618	256064.983488	54.229274
3026.044579	255787.307260	54.234279
3024.817535	255521.648573	54.239284
3024.091961	255237.345234	54.244289
3023.284010	254974.422294	54.249293
3022.659003	254689.772706	54.254298
3022.238202	254419.301848	54.259303
3021.324058	254149.520645	54.264308
3020.583630	253871.995793	54.269313
3019.790969	253607.391379	54.274317
3019.236548	253335.669793	54.279322
3018.883658	253067.660334	54.284327
3018.125054	252796.888642	54.289332
3017.276993	252526.691770	54.294337
3016.549359	252263.887083	54.299341
3016.004455	251991.019929	54.304346
3015.469211	251723.703413	54.309351
3014.324953	251457.043958	54.314356
3013.988570	251177.931158	54.319361
3013.209053	250920.611995	54.324365
3012.471007	250649.662014	54.329370
3012.243281	250376.849028	54.334375
3011.380162	250115.036728	54.339380
3010.935188	249838.388090	54.344385
3010.079370	249574.359903	54.349389
3009.250465	249305.514732	54.354394
3008.733414	249034.659736	54.359399
3007.980394	248769.419673	54.364404
3007.387298	248496.489391	54.369409
3006.577564	248240.885448	54.374413
3005.896479	247972.630331	54.379418
3005.680856	247697.910005	54.384423
3004.540792	247434.516117	54.389428
3004.142067	247161.633839	54.394433
3003.537635	246894.565405	54.399437
3002.848438	246627.281677	54.404442
3002.100304	246349.031958	54.409447
3000.857066	246090.036938	54.414452
3000.577455	245809.498569	54.419457
2999.906206	245553.520815	54.424461
2998.992648	245295.137171	54.429466
2998.396391	245030.235499	54.434471
2997.965373	244773.533576	54.439476
2997.344763	244516.531091	54.444481
2996.430071	244248.549067	54.449485
2995.923010	243980.324795	54.454490
2995.593789	243711.920118	54.459495
2994.582170	243445.151923	54.464500
2993.903123	243177.720461	54.469505
2993.287877	242918.937641	54.474509
2992.370828	242657.732987	54.479514
2991.876703	242387.600042	54.484519
2991.342797	242126.666874	54.489524
2990.730567	241864.600718	54.494529
2990.048556	241598.548150	54.499533
2989.299390	241332.099345	54.504538
2989.070618	241066.663733	54.509543
2987.841923	240805.410424	54.514548
2987.293285	240539.721018	54.519553
2986.414483	240269.831852	54.524557
2985.665650	240020.574575	54.529562
2985.051454	239750.822958	54.534567
2984.693022	239500.893832	54.539572
2984.193939	239228.247702	54.544577
2983.190957	238970.629608	54.549581
2982.849295	238712.958339	54.554586
2982.546993	238444.204437	54.559591
2981.077818	238176.043313	54.564596
2980.575476	237908.366390	54.569601
2979.811929	237651.833825	54.574605
2979.205865	237383.690767	54.579610
2978.574584	237115.297714	54.584615
2978.150990	236864.518972	54.589620
2977.287072	236595.527429	54.594625
2976.237890	236343.066454	54.599629
2975.735913	236079.289927	54.604634
2975.062453	235818.724166	54.609639
2974.217855	235565.265035	54.614644
2973.909033	235297.614876	54.619649
2972.961510	235053.212857	54.624653
2972.631834	234790.685475	54.629658
2971.610984	234531.934907	54.634663
2970.821582	234278.113709	54.639668
2970.641969	234022.770672	54.644673
2969.654845	233774.736737	54.649677
2969.262852	233507.664626	54.654682
2968.703448	233251.517930	54.659687
2967.679471	233000.716284	54.664692
2967.182311	232737.278650	54.669697
2966.504878	232479.039227	54.674701
2965.736780	232218.217638	54.679706
2965.044704	231963.266612	54.684711
2964.505678	231704.650874	54.689716
2964.082252	231454.980375	54.694721
2963.273305	231194.295359	54.699725
2962.449019	230936.057889	54.704730
2961.929691	230678.511266	54.709735
2961.093399	230427.763048	54.714740
2960.680821	230170.506482	54.719745
2959.986162	229913.218905	54.724749
2959.214936	229654.059975	54.729754
2958.775220	229391.284619	54.734759
2957.758134	229141.536106	54.739764
2957.258410	228877.651420	54.744769
2956.410485	228626.935471	54.749773
2955.959086	228373.687667	54.754778
2955.493600	228105.853281	54.759783
2954.456386	227858.912342	54.764788
2953.743696	227598.120580	54.769793
2953.154234	227346.679905	54.774797
2952.155626	227091.078144	54.779802
2951.900336	226836.377921	54.784807
2950.637046	226589.731010	54.789812
2950.369660	226335.085120	54.794817
2949.803091	226090.595405	54.799821
2949.029317	225833.523276	54.804826
2948.394349	225576.060779	54.809831
2947.779939	225325.279293	54.814836
2947.330921	225069.749410	54.819841
2946.562862	224821.068829	54.824845
2945.947213	224569.029533	54.829850
2945.247145	224309.378951	54.834855
2944.494931	224060.036205	54.839860
2944.097431	223800.224782	54.844865
2943.174805	223553.176554	54.849869
2942.298490	223296.485069	54.854874
2941.947676	223047.896647	54.859879
2941.289613	222790.828531	54.864884
2940.538031	222538.053332	54.869889
2939.860634	222290.753807	54.874893
2939.260747	222032.546000	54.879898
2938.732116	221781.100053	54.884903
2937.751004	221533.863748	54.889908
2937.391091	221265.054764	54.894913
2936.543950	221021.592371	54.899917
2935.926040	220761.100329	54.904922
2935.442940	220506.876283	54.909927
2934.748714	220256.136239	54.914932
2933.995391	219997.246740	54.919937
2933.679058	219736.175854	54.924941
2932.746916	219477.214632	54.929946
2932.188753	219228.340461	54.934951
2930.842509	218977.262419	54.939956
2930.514217	218717.940945	54.944961
2929.891364	218471.930950	54.949965
2929.037921	218229.917092	54.954970
2928.617115	217971.491241	54.959975
2927.867659	217721.939658	54.964980
2927.504070	217458.134884	54.969985
2926.911351	217218.807178	54.974989
2926.095141	216954.452201	54.979994
2925.399807	216698.556573	54.984999
2924.564886	216455.005583	54.990004
2924.180553	216186.728239	54.995009
2923.230227	215935.279958	55.000013
2922.658187	215688.609638	55.005018
2922.042140	215431.102266	55.010023
2921.262678	215178.560463	55.015028
2920.724320	214921.208170	55.020033
2919.863696	214673.174294	55.025037
2919.063168	214421.695094	55.030042
2918.705906	214169.790247	55.035047
2917.804821	213926.996924	55.040052
2917.117748	213675.057042	55.045057
2916.427849	213428.668126	55.050061
2915.543886	213183.278198	55.055066
2914.911995	212928.417609	55.060071
2914.334471	212680.677204	55.065076
2913.918350	212431.015674	55.070081
2913.095488	212194.542200	55.075085
2912.335184	211942.696870	55.080090
2911.749009	211696.743483	55.085095
2910.946727	211447.388686	55.090100
2910.303574	211203.966332	55.095105
2909.770268	210967.413299	55.100109
2908.660383	210717.193621	55.105114
2908.723914	210469.296515	55.110119
2907.731351	210232.271619	55.115124
2907.015328	209980.821523	55.120129
2906.271127	209740.564493	55.125133
2905.577334	209491.365622	55.130138
2905.122135	209242.371788	55.135143
2903.950823	209014.721801	55.140148
2903.891072	208766.469088	55.145153
2903.210852	208522.566559	55.150157
2902.320207	208273.607368	55.155162
2901.772817	208032.625763	55.160167
2900.937243	207794.134366	55.165172
2900.513017	207543.615200	55.170177
2899.756229	207306.118685	55.175181
2899.154790	207066.396715	55.180186
2898.373372	206809.522676	55.185191
2897.547190	206569.443725	55.190196
2897.120521	206323.282634	55.195201
2896.297738	206082.479661	55.200205
2895.510187	205845.642857	55.205210
2895.162817	205604.104750	55.210215
2894.400480	205360.584328	55.215220
2893.866137	205114.394388	55.220225
2892.833688	204876.263945	55.225229
2892.457562	204633.576248	55.230234
2892.239371	204384.094042	55.235239
2891.052754	204143.929302	55.240244
2890.680225	203896.433505	55.245249
2890.126752	203652.798054	55.250253
2889.380435	203409.003273	55.255258
2888.643890	203158.603055	55.260263
2887.928552	202917.032559	55.265268
2887.365038	202657.762434	55.270273
2886.650561	202424.351353	55.275277
2885.729078	202176.339071	55.280282
2885.587981	201930.418636	55.285287
2884.647608	201688.990824	55.290292
2883.994594	201440.608407	55.295297
2883.575121	201198.133071	55.300301
2882.408134	200952.939309	55.305306
2881.966331	200702.096127	55.310311
2881.240536	200461.950414	55.315316
2880.477230	200216.276057	55.320321
2879.528466	199970.619441	55.325325
2879.213048	199733.058847	55.330330
2878.794839	199485.551563	55.335335
2877.688924	199246.183999	55.340340
2877.355502	198996.222252	55.345345
2876.681364	198764.169129	55.350349
2875.964997	198516.726213	55.355354
2875.321941	198274.133831	55.360359
2874.125883	198026.501908	55.365364
2873.701842	197789.756030	55.370369
2873.088458	197559.556366	55.375373
2872.562244	197317.611538	55.380378
2872.078131	197070.469417	55.385383
2871.458164	196831.990095	55.390388
2870.678594	196587.760104	55.395393
2869.825362	196349.943423	55.400397
2869.356919	196101.759966	55.405402
2868.644683	195861.365545	55.410407
2867.818779	195618.076331	55.415412
2867.227844	195379.115534	55.420417
2866.696503	195140.579038	55.425421
2865.941219	194899.292486	55.430426
2864.800775	194651.336932	55.435431
2864.119769	194423.515845	55.440436
2863.919566	194180.299788	55.445441
2863.230307	193942.315585	55.450445
2862.737565	193702.023785	55.455450
2862.149503	193466.316122	55.460455
2860.997267	193226.207366	55.465460
2860.699841	192970.314095	55.470465
2859.966272	192740.918452	55.475469
2859.490741	192497.881362	55.480474
2858.821112	192257.917147	55.485479
2858.145381	192019.647296	55.490484
2857.402939	191769.708967	55.495489
2856.623012	191535.631267	55.500493
2856.113031	191290.646157	55.505498
2855.394868	191045.517112	55.510503
2854.651289	190810.559212	55.515508
2854.372958	190559.154008	55.520513
2853.720228	190324.502150	55.525517
2852.676825	190073.322401	55.530522
2852.343497	189835.339786	55.535527
2851.713006	189586.540007	55.540532
2850.797141	189348.117687	55.545537
2849.927124	189100.706985	55.550541
2849.399450	188854.871867	55.555546
2849.013267	188606.292958	55.560551
2848.022774	188380.202861	55.565556
2847.742153	188137.971004	55.570561
2847.077704	187892.798664	55.575565
2846.129244	187643.359673	55.580570
2845.551474	187388.430861	55.585575
2844.776090	187156.422132	55.590580
2844.156767	186908.410725	55.595585
2843.557024	186673.564975	55.600589
2842.799625	186426.926553	55.605594
2842.385190	186181.520059	55.610599
2841.415506	185943.517925	55.615604
2840.928184	185688.889455	55.620609
2839.939141	185451.897963	55.625613
2839.040544	185220.847160	55.630618
2838.586868	184979.498828	55.635623
2837.992927	184749.140029	55.640628
2837.399584	184501.506425	55.645633
2836.632978	184265.109246	55.650637
2836.176069	184024.898719	55.655642
2835.431687	183780.664163	55.660647
2834.620025	183551.465432	55.665652
2833.940237	183309.513046	55.670657
2833.179329	183069.559316	55.675661
2832.546435	182838.440481	55.680666
2832.219407	182599.222005	55.685671
2831.471879	182369.243217	55.690676
2830.636338	182122.742413	55.695681
2829.895736	181891.734623	55.700685
2829.363375	181660.097194	55.705690
2828.986547	181405.666344	55.710695
2827.863037	181177.356134	55.715700
2827.319314	180937.761227	55.720705
2826.709136	180701.879818	55.725709
2826.212095	180465.243991	55.730714
2825.498616	180217.119114	55.735719
2824.526274	179995.342150	55.740724
2823.927269	179748.855471	55.745729
2823.200978	179520.796374	55.750733
2822.480312	179282.332597	55.755738
2822.098078	179044.325352	55.760743
2821.157713	178818.224620	55.765748
2820.626799	178575.651649	55.770753
2820.055654	178341.774037	55.775757
2819.135255	178108.118382	55.780762
2818.562425	177872.399275	55.785767
2817.669760	177646.488039	55.790772
2817.298146	177412.571256	55.795777
2816.490638	177187.997266	55.800781
2815.834914	176951.329780	55.805786
2815.459292	176713.423663	55.810791
2814.878334	176487.532915	55.815796
2814.430908	176235.637055	55.820801
2813.578543	176006.650282	55.825805
2813.032309	175775.390472	55.830810
2812.179088	175533.865535	55.835815
2810.886105	175303.171802	55.840820
2810.666670	175061.625580	55.845825
2810.210017	174831.298083	55.850829
2809.587996	174600.298549	55.855834
2809.228500	174367.592617	55.860839
2808.216083	174131.201314	55.865844
2807.626865	173887.037013	55.870849
2807.102449	173644.809826	55.875853
2806.212644	173404.638725	55.880858
2805.212684	173162.006458	55.885863
2804.601485	172927.250180	55.890868
2804.298722	172691.098317	55.895873
2803.659883	172463.598408	55.900877
2802.781824	172232.118833	55.905882
2802.465959	171990.644398	55.910887
2801.404032	171754.440267	55.915892
2800.984206	171515.605039	55.920897
2800.294279	171279.917119	55.925901
2799.487832	171045.749724	55.930906
2799.128394	170806.095307	55.935911
2797.978783	170580.022447	55.940916
2797.887778	170336.602201	55.945921
2796.636145	170112.137861	55.950925
2796.074368	169875.611465	55.955930
2795.760232	169634.074923	55.960935
2795.059407	169397.954966	55.965940
2794.336879	169161.356643	55.970945
2793.330731	168921.345719	55.975949
2792.857618	168690.903861	55.980954
2792.368920	168448.194286	55.985959
2791.534877	168227.604190	55.990964
2790.994512	167982.604043	55.995969
2790.447452	167754.048851	56.000973
2789.204027	167523.570704	56.005978
2789.046640	167281.286568	56.010983
2787.903846	167053.859952	56.015988
2787.453439	166814.867830	56.020993
2786.736055	166581.260232	56.025997
2786.522280	166353.283778	56.031002
2785.809917	166119.004305	56.036007
2784.841912	165888.683247	56.041012
2784.358486	165648.750072	56.046017
2783.667764	165415.069211	56.051021
2782.871849	165182.767038	56.056026
2782.067888	164937.485096	56.061031
2781.530750	164707.192097	56.066036
2780.756276	164474.534926	56.071041
2779.901041	164250.309491	56.076045
2779.381778	164016.241539	56.081050
2778.619704	163793.148492	56.086055
2778.047258	163567.280326	56.091060
2777.621702	163330.366455	56.096065
2776.900500	163104.537416	56.101069
2776.186060	162884.837214	56.106074
2775.806028	162580.850710	56.111079
2775.093858	162346.391690	56.116084
2774.229229	162109.402721	56.121089
2774.036135	161879.734153	56.126093
2773.290877	161638.775181	56.131098
2772.518278	161405.259978	56.136103
2771.785200	161168.523350	56.141108
2771.115164	160929.438909	56.146113
2770.565454	160696.884707	56.151117
2769.860062	160464.801663	56.156122
2769.228454	160231.716763	56.161127
2768.378057	159988.344489	56.166132
2767.932879	159754.165235	56.171137
2767.087317	159516.071599	56.176141
2766.582723	159285.693495	56.181146
2766.043401	159040.587567	56.186151
2764.759741	158817.989380	56.191156
2764.699322	158584.977413	56.196161
2764.381137	158348.498991	56.201165
2763.120137	158114.256441	56.206170
2762.810331	157865.092327	56.211175
2761.639924	157632.084535	56.216180
2761.118198	157393.089532	56.221185
2760.061080	157168.470062	56.226189
2759.449291	156928.106840	56.231194
2758.853773	156702.120593	56.236199
2758.447252	156483.707940	56.241204
2757.705152	156241.285294	56.246209
2757.080425	156009.218989	56.251213
2756.262191	155777.057782	56.256218
2755.660770	155553.749575	56.261223
2755.094017	155321.348231	56.266228
2754.435518	155086.979938	56.271233
2753.856069	154865.643103	56.276237
2753.130512	154630.932640	56.281242
2752.751653	154381.347062	56.286247
2751.612720	154166.268575	56.291252
2751.063014	153921.289628	56.296257
2750.288659	153689.428092	56.301261
2749.507264	153458.802267	56.306266
2749.060792	153223.574349	56.311271
2748.354096	153005.651051	56.316276
2747.934735	152770.892328	56.321281
2747.158287	152532.797984	56.326285
2746.476870	152319.387557	56.331290
2745.802450	152071.467534	56.336295
2744.915840	151853.046414	56.341300
2744.586273	151611.900858	56.346305
2743.884681	151385.661897	56.351309
2742.597731	151161.512749	56.356314
2742.183461	150928.520290	56.361319
2741.631914	150708.439448	56.366324
2741.125778	150474.308123	56.371329
2740.186415	150242.738273	56.376333
2739.168863	150023.295091	56.381338
2739.028020	149794.525231	56.386343
2738.277281	149579.249756	56.391348
2737.805264	149340.647285	56.396353
2736.984401	149124.025989	56.401357
2736.314461	148885.775954	56.406362
2735.600411	148667.170810	56.411367
2734.935406	148436.561704	56.416372
2734.363484	148211.544306	56.421377
2733.691074	147992.797334	56.426381
2732.750157	147768.082964	56.431386
2732.400069	147527.898640	56.436391
2731.541193	147304.750444	56.441396
2730.829808	147084.045961	56.446401
2730.135946	146863.225850	56.451405
2729.398099	146642.986129	56.456410
2728.850367	146417.863134	56.461415
2728.026102	146201.465449	56.466420
2727.975717	145975.999927	56.471425
2727.024083	145758.163981	56.476429
2726.111058	145529.661210	56.481434
2725.604450	145290.077757	56.486439
2724.694203	145078.149242	56.491444
2724.599253	144857.921783	56.496449
2723.667165	144626.874294	56.501453
2722.981354	144407.772935	56.506458
2722.286713	144177.517158	56.511463
2721.577897	143947.354279	56.516468
2721.080563	143723.958115	56.521473
2720.343192	143512.533843	56.526477
2719.582505	143286.107352	56.531482
2719.286214	143055.097882	56.536487
2718.409126	142834.538460	56.541492
2717.402603	142606.872465	56.546497
2717.163023	142382.441294	56.551501
2716.114050	142166.259663	56.556506
2715.890100	141931.994193	56.561511
2715.285011	141715.872486	56.566516
2714.501339	141484.062550	56.571521
2713.817345	141266.075948	56.576525
2713.073985	141034.860242	56.581530
2712.659326	140813.987974	56.586535
2711.778716	140595.071644	56.591540
2711.264518	140362.071295	56.596545
2710.658732	140143.902465	56.601549
2709.701441	139919.768282	56.606554
2709.373892	139682.067823	56.611559
2708.839861	139467.183323	56.616564
2707.904680	139235.999040	56.621569
2706.959016	138998.058851	56.626573
2706.255703	138783.625342	56.631578
2705.862801	138549.336550	56.636583
2705.345714	138332.716862	56.641588
2704.534793	138105.815999	56.646593
2703.617836	137884.193559	56.651597
2703.248392	137662.193820	56.656602
2702.539481	137431.114715	56.661607
2701.777637	137219.852543	56.666612
2701.008494	136994.490833	56.671617
2700.259836	136761.377801	56.676621
2699.289352	136547.307666	56.681626
2699.214382	136322.044394	56.686631
2698.768319	136109.215623	56.691636
2697.942122	135889.181809	56.696641
2697.407386	135660.363047	56.701645
2696.275474	135429.849414	56.706650
2696.058076	135195.813483	56.711655
2695.338354	134987.482591	56.716660
2694.419819	134760.192627	56.721665
2693.840903	134537.322309	56.726669
2693.016826	134321.682736	56.731674
2692.554415	134083.972437	56.736679
2692.155435	133870.936593	56.741684
2691.431887	133645.796749	56.746689
2690.858885	133424.687110	56.751693
2689.515254	133200.538202	56.756698
2689.149010	132973.149388	56.761703
2688.220072	132754.781611	56.766708
2688.098995	132547.199165	56.771713
2687.175909	132322.495091	56.776717
2686.348593	132104.294017	56.781722
2686.154852	131868.426759	56.786727
2685.308655	131659.974851	56.791732
2684.636661	131429.763327	56.796737
2683.988983	131204.859313	56.801741
2683.307815	130988.561673	56.806746
2682.700604	130756.452750	56.811751
2681.740878	130539.529474	56.816756
2681.101576	130310.769885	56.821761
2680.633512	130094.292914	56.826765
2679.696593	129872.404823	56.831770
2679.177132	129656.447430	56.836775
2678.620535	129437.004713	56.841780
2677.971692	129214.555435	56.846785
2676.949405	128996.879217	56.851789
2676.386174	128776.185327	56.856794
2675.767964	128558.918449	56.861799
2674.598174	128347.138517	56.866804
2674.238617	128134.241175	56.871809
2673.716608	127915.897221	56.876813
2673.076737	127694.995450	56.881818
2672.695969	127485.942017	56.886823
2672.043128	127269.605164	56.891828
2671.401992	127042.460239	56.896833
2670.825016	126823.143014	56.901837
2669.953276	126597.600416	56.906842
2669.489365	126377.430633	56.911847
2668.248764	126157.944467	56.916852
2668.108473	125948.089935	56.921857
2667.325040	125721.486484	56.926861
2666.674174	125502.839220	56.931866
2666.282798	125286.628989	56.936871
2665.603314	125068.586620	56.941876
2665.167135	124839.763904	56.946881
2664.108223	124612.984748	56.951885
2663.340595	124393.298190	56.956890
2662.696594	124172.463626	56.961895
2662.109493	123950.326574	56.966900
2661.445434	123731.594100	56.971905
2660.994965	123503.699268	56.976909
2659.828247	123286.243726	56.981914
2659.379662	123072.485685	56.986919
2658.785436	122844.822398	56.991924
2658.500813	122614.077129	56.996929
2657.644007	122400.020890	57.001933
2656.450847	122179.289735	57.006938
2656.126368	121955.489569	57.011943
2655.382643	121738.665292	57.016948
2654.825447	121518.448352	57.021953
2654.235787	121295.229064	57.026957
2653.280757	121083.522643	57.031962
2652.802605	120866.815790	57.036967
2652.292534	120645.024179	57.041972
2651.188327	120417.259342	57.046977
2650.443302	120205.602875	57.051981
2649.577011	120000.353879	57.056986
2649.156463	119780.663059	57.061991
2648.224823	119559.366394	57.066996
2647.554082	119347.121034	57.072001
2647.162693	119134.198310	57.077005
2646.417599	118928.348128	57.082010
2646.220810	118717.391306	57.087015
2645.514108	118498.029576	57.092020
2644.895178	118272.707672	57.097025
2644.008348	118051.486536	57.102029
2642.934687	117840.447241	57.107034
2643.013560	117627.481384	57.112039
2641.940949	117411.722594	57.117044
2641.506279	117189.586575	57.122049
2640.539892	116985.196090	57.127053
2639.877591	116767.155978	57.132058
2639.457348	116552.729244	57.137063
2638.487846	116332.964158	57.142068
2638.183573	116113.863601	57.147073
2637.402607	115897.068407	57.152077
2636.757584	115686.835771	57.157082
2635.970096	115464.218364	57.162087
2635.212661	115258.323269	57.167092
2634.510933	115043.484088	57.172097
2634.038786	114826.623674	57.177101
2633.359907	114609.874033	57.182106
2632.741984	114400.745781	57.187111
2631.720537	114198.157170	57.192116
2631.395175	113980.868175	57.197121
2630.871312	113766.309944	57.202125
2630.042950	113552.246067	57.207130
2629.923223	113331.483728	57.212135
2628.763867	113110.913444	57.217140
2627.837757	112898.482696	57.222145
2627.040430	112685.842943	57.227149
2626.711305	112480.569022	57.232154
2626.138659	112263.257890	57.237159
2625.364040	112057.099706	57.242164
2625.053488	111833.753345	57.247169
2624.364457	111628.702113	57.252173
2623.221768	111403.086190	57.257178
2622.789108	111190.610823	57.262183
2621.957601	110977.007385	57.267188
2621.202932	110759.528798	57.272193
2620.773604	110561.508511	57.277197
2620.065573	110339.393566	57.282202
2619.838044	110126.082533	57.287207
2618.719583	109917.896086	57.292212
2618.182228	109689.934367	57.297217
2617.632785	109477.777796	57.302221
2616.892117	109266.167366	57.307226
2616.266064	109055.048259	57.312231
2615.572488	108843.770337	57.317236
2614.970735	108623.506992	57.322241
2614.389012	108411.878760	57.327245
2613.338283	108197.966156	57.332250
2613.186772	107978.265494	57.337255
2612.098926	107770.942749	57.342260
2611.679039	107549.879806	57.347265
2611.014179	107330.342488	57.352269
2609.849478	107125.086965	57.357274
2609.688984	106910.207067	57.362279
2608.901380	106697.503301	57.367284
2608.516011	106481.996606	57.372289
2607.594724	106263.778617	57.377293
2606.789963	106057.605870	57.382298
2606.413241	105834.039183	57.387303
2605.382499	105630.190070	57.392308
2605.027532	105411.388837	57.397313
2604.416337	105190.441278	57.402317
2603.401167	104983.771801	57.407322
2603.222054	104766.953504	57.412327
2602.149525	104562.974180	57.417332
2601.652076	104348.234042	57.422337
2600.701865	104136.213214	57.427341
2599.963058	103917.562629	57.432346
2599.528785	103711.465611	57.437351
2598.714924	103511.628882	57.442356
2598.003044	103294.946491	57.447361
2597.842587	103083.196925	57.452365
2596.737492	102873.952607	57.457370
2596.180734	102658.602761	57.462375
2595.362164	102457.138935	57.467380
2594.756446	102244.953588	57.472385
2594.167192	102033.598593	57.477389
2593.372566	101827.308688	57.482394
2592.863337	101607.228455	57.487399
2591.934747	101410.333172	57.492404
2591.432389	101193.053315	57.497409
2590.988171	100975.683798	57.502413
2589.948219	100775.950554	57.507418
2589.197854	100561.729051	57.512423
2588.549591	100369.435204	57.517428
2587.978562	100159.432730	57.522433
2587.376491	99955.615450	57.527437
2586.734724	99750.353648	57.532442
2586.262082	99533.344649	57.537447
2585.310151	99340.473135	57.542452
2584.598233	99139.071811	57.547457
2584.188355	98923.771219	57.552461
2583.491429	98724.806854	57.557466
2582.838131	98506.884685	57.562471
2582.350624	98297.970520	57.567476
2581.452428	98096.011609	57.572481
2580.948674	97890.985510	57.577485
2580.040780	97684.255683	57.582490
2579.937372	97464.695966	57.587495
2578.907904	97263.691219	57.592500
2577.932330	97061.487311	57.597505
2577.936311	96846.400667	57.602509
2576.941507	96644.438175	57.607514
2576.405213	96432.187318	57.612519
2575.511094	96229.781274	57.617524
2574.492694	96017.724852	57.622529
2574.270753	95810.605234	57.627533
2573.382238	95615.446531	57.632538
2572.912598	95404.672435	57.637543
2571.816281	95200.728464	57.642548
2571.317988	95007.612367	57.647553
2570.843007	94796.775030	57.652557
2570.317218	94591.281185	57.657562
2569.510862	94383.550647	57.662567
2569.067518	94180.095880	57.667572
2568.446656	93964.070253	57.672577
2567.776966	93767.358212	57.677581
2567.172151	93560.338982	57.682586
2566.454103	93351.443515	57.687591
2565.711399	93133.409606	57.692596
2565.065959	92927.632909	57.697601
2563.991874	92712.743866	57.702605
2563.532716	92523.232144	57.707610
2563.023622	92315.752729	57.712615
2562.298451	92118.949881	57.717620
2561.627620	91908.944431	57.722625
2561.420499	91697.650012	57.727629
2560.334362	91493.535352	57.732634
2559.943094	91274.081676	57.737639
2558.929038	91073.256730	57.742644
2558.472523	90860.297820	57.747649
2557.780190	90660.915721	57.752653
2556.838731	90454.435354	57.757658
2556.398192	90245.563230	57.762663
2555.480927	90048.314727	57.767668
2554.829948	89839.086710	57.772673
2554.398004	89631.658354	57.777677
2553.281023	89442.962111	57.782682
2553.092357	89227.617984	57.787687
2552.243319	89031.344240	57.792692
2551.453082	88824.531930	57.797697
2551.036524	88626.487786	57.802701
2550.604346	88418.183384	57.807706
2549.937650	88211.452422	57.812711
2548.728796	88012.480663	57.817716
2548.120452	87812.863990	57.822721
2548.035781	87597.056709	57.827725
2546.846985	87397.884546	57.832730
2546.261311	87191.581578	57.837735
2545.549715	86991.976166	57.842740
2545.004194	86800.873003	57.847745
2544.006603	86589.759607	57.852749
2543.689120	86389.932483	57.857754
2542.932946	86188.154478	57.862759
2542.305772	85987.587754	57.867764
2541.604791	85783.250058	57.872769
2541.103543	85582.901715	57.877773
2540.121620	85380.774058	57.882778
2539.849500	85176.323472	57.887783
2539.095280	84979.165070	57.892788
2538.298090	84772.982264	57.897793
2537.543718	84574.813390	57.902797
2536.659763	84374.454639	57.907802
2536.354600	84169.194899	57.912807
2535.804155	83976.203431	57.917812
2534.964105	83778.454904	57.922817
2534.875192	83574.136460	57.927821
2533.649646	83371.800285	57.932826
2532.787003	83161.815016	57.937831
2532.303370	82967.516424	57.942836
2531.766889	82764.709224	57.947841
2531.229295	82566.733943	57.952845
2530.155087	82365.093330	57.957850
2529.829004	82150.101937	57.962855
2528.987226	81959.437809	57.967860
2528.457154	81763.281607	57.972865
2527.913475	81553.192114	57.977869
2527.201018	81354.451048	57.982874
2526.336976	81152.947226	57.987879
2526.099155	80950.623580	57.992884
2525.275587	80751.886841	57.997889
2524.658700	80542.180365	58.002893
2523.485492	80349.916630	58.007898
2523.078220	80137.988176	58.012903
2522.384075	79946.729626	58.017908
2521.848441	79743.976914	58.022913
2521.765438	79547.073568	58.027917
2520.328169	79347.877158	58.032922
2519.809609	79129.949831	58.037927
2519.321631	78937.932790	58.042932
2518.464007	78726.172534	58.047937
2517.830439	78536.146820	58.052941
2517.127289	78339.739826	58.057946
2516.437245	78136.045118	58.062951
2516.080157	77935.442755	58.067956
2515.006446	77737.040757	58.072961
2514.527174	77531.240151	58.077965
2513.841353	77324.942064	58.082970
2513.263357	77129.908204	58.087975
2512.504232	76932.300572	58.092980
2511.832998	76715.227778	58.097985
2511.194426	76512.744982	58.102989
2509.947182	76327.969534	58.107994
2509.496171	76125.239082	58.112999
2508.795464	75947.198365	58.118004
2508.206355	75745.805193	58.123009
2507.808552	75551.036664	58.128013
2506.782120	75353.353659	58.133018
2506.320400	75158.079472	58.138023
2505.834885	74971.852382	58.143028
2505.414493	74771.753687	58.148033
2504.752081	74565.251767	58.153037
2503.863940	74364.730710	58.158042
2503.596251	74165.678225	58.163047
2503.016463	73965.910559	58.168052
2502.214276	73762.682874	58.173057
2501.277188	73559.725711	58.178061
2500.626708	73352.144622	58.183066
2500.528448	73150.148337	58.188071
2499.380381	72964.139855	58.193076
2498.466327	72760.236827	58.198081
2497.925626	72548.395684	58.203085
2497.106672	72356.182855	58.208090
2496.369655	72156.027349	58.213095
2495.755091	71956.880716	58.218100
2495.238537	71762.490768	58.223105
2494.364147	71561.976569	58.228109
2493.819347	71371.452876	58.233114
2493.026576	71170.391228	58.238119
2492.527631	70976.348252	58.243124
2492.030589	70779.424603	58.248129
2491.138162	70578.017348	58.253133
2490.512001	70393.350106	58.258138
2489.879008	70191.405234	58.263143
2489.346381	69998.175328	58.268148
2488.759860	69796.170122	58.273153
2487.608989	69602.028602	58.278157
2487.443597	69404.438991	58.283162
2486.724187	69214.761863	58.288167
2486.000286	69007.402495	58.293172
2485.162129	68809.881164	58.298177
2484.373986	68618.231810	58.303181
2483.729112	68438.741713	58.308186
2483.487350	68231.903171	58.313191
2482.852978	68028.973649	58.318196
2482.185028	67830.453483	58.323201
2481.775027	67629.842345	58.328205
2480.802522	67436.853061	58.333210
2480.124643	67228.276542	58.338215
2479.349210	67036.894030	58.343220
2478.815178	66835.829388	58.348225
2478.271734	66633.330655	58.353229
2477.160317	66448.650850	58.358234
2476.798898	66249.819555	58.363239
2476.386874	66051.679132	58.368244
2475.270480	65848.193295	58.373249
2474.912667	65647.049718	58.378253
2474.289477	65449.237094	58.383258
2473.421686	65249.027118	58.388263
2472.750155	65055.396389	58.393268
2472.068036	64853.951521	58.398273
2471.595772	64654.178983	58.403277
2470.528904	64459.242734	58.408282
2470.182964	64257.092238	58.413287
2469.354386	64074.755540	58.418292
2468.869047	63870.323029	58.423297
2468.095088	63678.713961	58.428301
2467.262778	63475.683127	58.433306
2466.561033	63281.422866	58.438311
2465.547598	63097.275784	58.443316
2465.107243	62901.948974	58.448321
2464.705344	62703.613524	58.453325
2463.772384	62520.003818	58.458330
2463.016567	62324.821584	58.463335
2462.451638	62132.400267	58.468340
2461.824922	61952.600419	58.473345
2461.266768	61762.480211	58.478349
2460.819559	61578.194766	58.483354
2460.035448	61374.428419	58.488359
2459.489177	61182.016957	58.493364
2458.565970	60984.323463	58.498369
2458.366430	60799.648614	58.503373
2457.523808	60601.680435	58.508378
2456.908616	60410.743965	58.513383
2456.158514	60219.533252	58.518388
2455.517562	60018.664871	58.523393
2454.985621	59827.809755	58.528397
2453.707776	59635.704165	58.533402
2453.486368	59432.695810	58.538407
2452.687761	59250.973721	58.543412
2451.882440	59059.340421	58.548417
2451.173814	58853.057096	58.553421
2450.947613	58676.786068	58.558426
2450.443762	58478.565014	58.563431
2449.546272	58284.716403	58.568436
2448.777207	58089.668815	58.573441
2448.379665	57891.744176	58.578445
2447.129692	57704.607578	58.583450
2447.013777	57506.908261	58.588455
2446.051657	57316.852826	58.593460
2445.461500	57120.733063	58.598465
2445.029792	56916.209235	58.603469
2444.016710	56736.216829	58.608474
2443.516478	56537.588629	58.613479
2442.779678	56348.339802	58.618484
2442.077382	56153.903327	58.623489
2441.763593	55967.240371	58.628493
2440.684245	55770.297837	58.633498
2440.337010	55578.444288	58.638503
2439.631136	55389.453586	58.643508
2438.783557	55194.822403	58.648513
2438.422070	54997.578123	58.653517
2437.256157	54803.776907	58.658522
2436.949471	54614.537849	58.663527
2436.183029	54425.696424	58.668532
2435.827093	54238.889980	58.673537
2435.333714	54044.379418	58.678541
2434.339667	53848.235136	58.683546
2433.687010	53645.216231	58.688551
2433.351602	53451.177437	58.693556
2432.277411	53253.451052	58.698561
2431.907919	53073.395708	58.703565
2430.757942	52878.150467	58.708570
2430.552769	52667.591019	58.713575
2429.843264	52475.412936	58.718580
2429.029782	52277.570405	58.723585
2428.393124	52093.048608	58.728589
2427.824402	51905.407541	58.733594
2427.210554	51701.401164	58.738599
2426.241963	51501.949517	58.743604
2425.695887	51320.816320	58.748609
2424.906919	51120.403849	58.753613
2424.213251	50935.045465	58.758618
2423.480888	50748.688981	58.763623
2423.189105	50552.633558	58.768628
2422.290928	50360.163030	58.773633
2421.992073	50159.136205	58.778637
2421.085632	49975.435019	58.783642
2420.472553	49773.462562	58.788647
2419.706297	49576.357222	58.793652
2419.142949	49392.572818	58.798657
2418.590970	49197.845274	58.803661
2417.651455	48998.391512	58.808666
2417.097813	48799.290072	58.813671
2416.593701	48612.394461	58.818676
2416.031370	48428.350914	58.823681
2415.492775	48222.784052	58.828685
2414.326000	48032.532370	58.833690
2413.884071	47833.664440	58.838695
2413.360979	47637.892773	58.843700
2412.196784	47446.274043	58.848705
2412.039594	47251.590609	58.853709
2411.078261	47065.194999	58.858714
2410.642061	46866.457214	58.863719
2409.846519	46679.938154	58.868724
2409.120437	46481.076685	58.873729
2408.548175	46291.429544	58.878733
2407.731671	46103.430044	58.883738
2406.977641	45901.745363	58.888743
2406.793368	45713.596012	58.893748
2405.956584	45519.314614	58.898753
2405.290255	45325.356269	58.903757
2404.118672	45135.642643	58.908762
2403.757960	44943.079218	58.913767
2403.107780	44753.543256	58.918772
2402.442454	44559.975929	58.923777
2402.009946	44375.786418	58.928781
2400.917172	44186.589287	58.933786
2400.329573	43983.847065	58.938791
2400.271171	43792.658962	58.943796
2399.014398	43607.210321	58.948801
2398.457703	43408.495998	58.953805
2397.698739	43231.960701	58.958810
2397.161231	43037.447539	58.963815
2396.533773	42846.179784	58.968820
2395.727145	42659.670512	58.973825
2395.156096	42463.904084	58.978829
2394.241964	42287.168973	58.983834
2393.891871	42094.262169	58.988839
2393.628677	41899.598100	58.993844
2392.625031	41711.033624	58.998849
2391.974846	41515.334746	59.003853
2391.410858	41328.984759	59.008858
2390.503197	41133.078058	59.013863
2389.860611	40940.319060	59.018868
2388.791757	40755.219022	59.023873
2388.878117	40566.241267	59.028877
2387.732777	40381.577944	59.033882
2387.187715	40187.294113	59.038887
2386.423935	40001.230504	59.043892
2385.681728	39815.747301	59.048897
2385.281326	39620.049356	59.053901
2384.348566	39437.775074	59.058906
2383.776886	39241.179011	59.063911
2383.024609	39066.588769	59.068916
2382.236565	38875.289401	59.073921
2381.843067	38686.721479	59.078925
2380.879337	38510.627501	59.083930
2380.336390	38316.332975	59.088935
2379.823412	38128.716559	59.093940
2378.987041	37949.810098	59.098945
2378.499620	37758.621045	59.103949
2377.584981	37585.371163	59.108954
2377.048780	37392.802866	59.113959
2376.402886	37210.200279	59.118964
2375.992427	37027.288860	59.123969
2374.995334	36835.308981	59.128973
2374.037831	36661.790816	59.133978
2373.551387	36475.432504	59.138983
2373.215021	36291.336524	59.143988
2372.484674	36118.766357	59.148993
2371.816677	35920.754011	59.153997
2370.971365	35742.936078	59.159002
2370.338515	35552.547406	59.164007
2369.896224	35382.140895	59.169012
2369.102026	35201.565619	59.174017
2368.190199	35004.092707	59.179021
2367.693695	34827.371894	59.184026
2367.439187	34646.650632	59.189031
2366.739515	34460.915855	59.194036
2365.790941	34278.995221	59.199041
2365.178109	34089.065685	59.204045
2364.426807	33908.171976	59.209050
2363.989651	33717.475997	59.214055
2363.274796	33541.604670	59.219060
2362.233418	33360.427851	59.224065
2362.045725	33176.370937	59.229069
2360.934318	32993.404425	59.234074
2360.352795	32816.310640	59.239079
2360.007692	32626.704571	59.244084
2359.457356	32443.146283	59.249089
2358.945215	32251.913236	59.254093
2357.822880	32079.903624	59.259098
2357.340658	31885.384671	59.264103
2356.548508	31702.471848	59.269108
2355.971990	31517.832859	59.274113
2355.340318	31328.933389	59.279117
2354.275238	31143.628619	59.284122
2353.833464	30973.799648	59.289127
2353.043820	30794.655707	59.294132
2352.675738	30606.030846	59.299137
2352.026826	30424.460491	59.304141
2351.139066	30248.452461	59.309146
2350.963549	30052.888891	59.314151
2350.439603	29871.451774	59.319156
2349.528191	29691.150956	59.324161
2348.893792	29496.404662	59.329165
2347.899432	29315.078318	59.334170
2347.247991	29132.366092	59.339175
2346.758236	28954.984799	59.344180
2346.484152	28768.260542	59.349185
2345.837505	28582.690816	59.354189
2345.071440	28394.257201	59.359194
2344.356005	28207.535088	59.364199
2343.789745	28016.865447	59.369204
2342.675531	27829.640566	59.374209
2342.365976	27636.457442	59.379213
2341.410352	27458.005122	59.384218
2340.680897	27271.859970	59.389223
2340.155158	27090.082792	59.394228
2339.404007	26902.322870	59.399233
2338.650446	26713.203756	59.404237
2338.077255	26541.865071	59.409242
2337.683091	26367.755830	59.414247
2336.482025	26171.077635	59.419252
2335.720126	25989.605385	59.424257
2335.489822	25811.872092	59.429261
2334.815689	25631.039199	59.434266
2334.088038	25447.875013	59.439271
2333.355816	25277.916068	59.444276
2332.572628	25083.568513	59.449281
2331.979331	24900.717804	59.454285
2331.050529	24721.902876	59.459290
2330.799315	24544.509116	59.464295
2330.142092	24368.835467	59.469300
2329.317424	24192.210210	59.474305
2328.906984	24004.554005	59.479309
2328.006387	23826.321896	59.484314
2327.727334	23639.061381	59.489319
2326.721856	23472.983225	59.494324
2325.706644	23290.933276	59.499329
2325.261634	23106.754390	59.504333
2324.211452	22937.566416	59.509338
2324.005052	22762.550432	59.514343
2323.471670	22582.447435	59.519348
2322.688584	22405.616601	59.524353
2322.095479	22226.948498	59.529357
2320.760983	22053.933840	59.534362
2320.396272	21875.444305	59.539367
2319.875857	21704.572989	59.544372
2319.054174	21523.542252	59.549377
2318.680506	21354.242528	59.554381
2318.082817	21181.927522	59.559386
2317.298332	20999.121846	59.564391
2316.533997	20828.440790	59.569396
2315.838377	20653.374830	59.574401
2315.181009	20478.686106	59.579405
2314.263832	20306.299457	59.584410
2313.537509	20129.484243	59.589415
2312.741378	19966.880470	59.594420
2312.270637	19798.570529	59.599425
2311.878502	19621.542610	59.604429
2311.057961	19460.820696	59.609434
2310.502518	19286.022056	59.614439
2309.760359	19115.678554	59.619444
2309.136257	18950.220147	59.624449
2308.461815	18773.868278	59.629453
2307.486423	18614.513427	59.634458
2307.113463	18435.428989	59.639463
2306.534458	18266.258573	59.644468
2305.800294	18098.265613	59.649473
2305.187111	17918.179171	59.654477
2304.259486	17759.238339	59.659482
2303.774083	17591.880419	59.664487
2303.329427	17423.618291	59.669492
2302.412502	17252.877168	59.674497
2301.860521	17084.817283	59.679501
2300.962524	16914.262776	59.684506
2300.540750	16735.179141	59.689511
2299.962761	16574.557771	59.694516
2299.172483	16411.383793	59.699521
2298.943649	16228.439870	59.704525
2298.129480	16068.868605	59.709530
2297.282570	15881.154550	59.714535
2296.836388	15713.365047	59.719540
2296.028484	15544.951769	59.724545
2295.218010	15375.422671	59.729549
2294.279228	15205.290061	59.734554
2293.630790	15036.707851	59.739559
2293.163466	14868.997164	59.744564
2292.522076	14704.168557	59.749569
2291.815733	14534.922135	59.754573
2291.137263	14378.003395	59.759578
2290.656303	14206.515592	59.764583
2289.735417	14044.439790	59.769588
2289.004011	13876.826972	59.774593
2288.700477	13706.153889	59.779597
2287.566747	13550.566255	59.784602
2287.155721	13375.349348	59.789607
2286.454826	13211.067850	59.794612
2285.867351	13049.258354	59.799617
2285.069539	12884.482754	59.804621
2284.114745	12721.807462	59.809626
2283.579329	12558.890440	59.814631
2283.033339	12398.829942	59.819636
2282.480804	12233.016281	59.824641
2281.723800	12071.028881	59.829645
2281.046308	11914.603068	59.834650
2280.803407	11746.151897	59.839655
2280.209866	11586.682731	59.844660
2279.274528	11425.941177	59.849665
2278.725828	11248.077262	59.854669
2277.840122	11091.780517	59.859674
2277.109791	10923.283982	59.864679
2276.532806	10766.347439	59.869684
2275.571616	10605.321778	59.874689
2274.915737	10437.523070	59.879693
2274.042663	10282.194129	59.884698
2273.415060	10124.232687	59.889703
2273.173628	9965.499539	59.894708
2272.272239	9817.355928	59.899713
2272.186332	9648.061630	59.904718
2271.077758	9493.472870	59.909722
2270.758125	9319.067886	59.914727
2269.840411	9167.475643	59.919732
2269.002150	9000.210987	59.924737
2268.567969	8840.130045	59.929742
2267.608212	8685.183554	59.934746
2267.279053	8530.871977	59.939751
2266.727868	8365.642616	59.944756
2265.746594	8203.824061	59.949761
2264.874141	8041.391979	59.954766
2264.292526	7894.077092	59.959770
2263.484372	7728.902593	59.964775
2262.879430	7573.058083	59.969780
2261.865744	7422.155826	59.974785
2261.372777	7266.558264	59.979790
2260.806834	7125.616781	59.984794
2259.950651	6958.649481	59.989799
2259.245664	6812.113052	59.994804
2258.579848	6665.160061	59.999809
2258.410655	6516.143806	60.004814
2257.391647	6379.005404	60.009818
2256.700372	6224.881501	60.014823
2255.925140	6074.476063	60.019828
2255.316457	5935.019032	60.024833
2254.911729	5772.400550	60.029838
2253.712717	5629.709644	60.034842
2253.430445	5483.412660	60.039847
2252.594150	5337.798953	60.044852
2251.877726	5185.466948	60.049857
2250.924370	5036.699911	60.054862
2250.169280	4901.594341	60.059866
2249.358180	4751.690704	60.064871
2248.871619	4616.562490	60.069876
2248.216058	4485.506213	60.074881
2247.626518	4330.271327	60.079886
2246.778814	4208.902913	60.084890
2246.060946	4070.095145	60.089895
2245.350106	3935.062362	60.094900
2244.480499	3799.891945	60.099905
2244.120673	3668.342493	60.104910
2243.813462	3533.547485	60.109914
2242.977718	3392.216514	60.114919
2241.689296	3271.721499	60.119924
2240.946611	3134.835072	60.124929
2240.440104	3006.164270	60.129934
2240.054574	2886.001605	60.134938
2239.310144	2754.908543	60.139943
2238.574134	2624.855538	60.144948
2237.564160	2503.742993	60.149953
2236.818502	2380.800902	60.154958
2236.108552	2263.936064	60.159962
2235.475088	2137.115523	60.164967
2234.757691	2025.277278	60.169972
2233.967410	1911.683389	60.174977
2233.273647	1794.761366	60.179982
2232.172182	1691.996364	60.184986
2231.218150	1578.336405	60.189991
2230.567049	1481.411138	60.194996
2229.560404	1387.317924	60.200001
2228.732235	1294.826989	60.205006
2228.200822	1205.855478	60.210010
2227.291116	1111.569659	60.215015
2226.467320	1018.743850	60.220020
2225.374974	937.974869	60.225025
2225.180913	856.195648	60.230030
2224.207026	775.204543	60.235034
2223.437388	693.106706	60.240039
2222.983261	619.934422	60.245044
2221.897274	538.974242	60.250049
2221.253780	460.052848	60.255054
2220.324378	396.310622	60.260058
2219.668321	325.155783	60.265063
2218.822248	261.142297	60.270068
2217.799017	211.743159	60.275073
2217.201377	137.954212	60.280078
2216.217973	95.913857	60.285082
2215.413502	53.503028	60.290087
2215.113098	8.791931	60.295092
2213.501796	-35.682690	60.300097
2212.378447	-74.957935	60.305102
2211.295302	-93.666721	60.310106
2210.415959	-114.711017	60.315111
2209.336009	-125.704808	60.320116
2208.252197	-120.182106	60.325121
2207.788038	-130.447233	60.330126
2206.231405	-117.885510	60.335130
2203.659936	-56.576192	60.340135
2201.947000	4.883415	60.345140
2202.054584	26.338952	60.350145
2202.547554	51.035652	60.355150
2203.094444	57.329521	60.360154
2203.246588	55.763089	60.365159
2203.293736	57.875142	60.370164
2202.874152	49.026863	60.375169
2202.371962	38.759765	60.380174
2202.429528	28.845440	60.385178
2201.740429	21.670563	60.390183
2201.048900	-1.244059	60.395188
2199.748988	11.587721	60.400193
2198.247711	13.716742	60.405198
2196.253561	24.498163	60.410202
2195.602619	30.986775	60.415207
2195.556935	37.147550	60.420212
2195.266428	38.915759	60.425217
2195.658119	44.086176	60.430222
2194.983786	50.928604	60.435226
2194.419644	41.832017	60.440231
2193.774571	33.800143	60.445236
2192.819283	37.126242	60.450241
2191.763564	34.101873	60.455246
2191.001765	47.551668	60.460250
2190.152793	37.694417	60.465255
2190.097309	48.054760	60.470260
2189.337976	51.513786	60.475265
2188.744901	44.307899	60.480270
2188.660908	50.244513	60.485274
2187.521823	48.887656	60.490279
2187.200791	56.828414	60.495284
2186.234251	49.697543	60.500289
2185.612442	50.332399	60.505294
2184.809195	57.080161	60.510298
2183.990257	60.666922	60.515303
2183.388732	60.656715	60.520308
2183.323603	63.705981	60.525313
2183.256091	54.700920	60.530318
2182.395588	56.742492	60.535322
2181.063194	56.381439	60.540327
2180.509641	57.636273	60.545332
2179.177145	68.106179	60.550337
2178.879245	66.713648	60.555342
2178.417762	64.438708	60.560346
2177.889820	55.099823	60.565351
2177.200727	61.872059	60.570356
2176.726762	66.615242	60.575361
2176.459626	58.714220	60.580366
2175.387783	62.128210	60.585370
2174.701825	64.796556	60.590375
2173.828794	68.354056	60.595380
2173.091704	65.804285	60.600385
2172.705041	60.461221	60.605390
2172.042823	72.286686	60.610394
2171.144323	71.853646	60.615399
2171.153928	70.062233	60.620404
2170.143536	75.027724	60.625409
2169.848033	69.403679	60.630414
2168.744224	66.819045	60.635418
2167.779700	64.335322	60.640423
2167.558781	71.637284	60.645428
2166.840549	76.274140	60.650433
2166.605536	71.102564	60.655438
2165.810432	73.811885	60.660442
2165.103193	71.828259	60.665447
2164.304138	69.887587	60.670452
2163.507043	72.501026	60.675457
2162.934328	73.445079	60.680462
2161.849195	74.590282	60.685466
2161.582405	75.605652	60.690471
2161.712411	69.303795	60.695476
2160.584812	66.521081	60.700481
2159.879192	65.880817	60.705486
2159.154654	70.103918	60.710490
2158.420182	64.327162	60.715495
2157.907004	64.675120	60.720500
2156.540954	76.803076	60.725505
2155.943408	74.065582	60.730510
2155.700484	80.281322	60.735514
2155.237061	81.682719	60.740519
2154.394895	68.717659	60.745524
2153.460428	75.334862	60.750529
2153.164629	78.354493	60.755534
2152.435223	78.727296	60.760538
2152.026196	74.777131	60.765543
2151.787171	76.974013	60.770548
2150.539996	76.326630	60.775553
2149.727242	73.336265	60.780558
2149.734818	77.749156	60.785562
2148.748934	79.003202	60.790567
2148.326316	70.604855	60.795572
2146.965164	84.214439	60.800577
2146.939243	68.595073	60.805582
2145.925921	75.745205	60.810586
2145.424390	80.437575	60.815591
2144.797200	74.451402	60.820596
2143.643995	83.727471	60.825601
2143.408983	74.225409	60.830606
2142.331458	75.336295	60.835610
2141.739105	83.610288	60.840615
2141.236021	81.280449	60.845620
2140.480915	84.978531	60.850625
2140.891784	79.035824	60.855630
2139.825114	83.144476	60.860634
2138.690947	81.171820	60.865639
2137.824753	78.450145	60.870644
2137.026440	85.630828	60.875649
2137.248658	87.402856	60.880654
2136.591711	84.589631	60.885658
2135.921382	81.387430	60.890663
2134.638519	75.513176	60.895668
2133.667211	83.645438	60.900673
2133.527006	82.724651	60.905678
2133.423523	86.294114	60.910682
2132.247829	79.045044	60.915687
2131.455020	87.951688	60.920692
2131.046799	94.769273	60.925697
2130.630609	84.225158	60.930702
2129.448532	87.934215	60.935706
2128.498328	86.064845	60.940711
2128.631585	87.945608	60.945716
2127.811769	90.203106	60.950721
2127.186686	81.764339	60.955726
2126.129340	88.806345	60.960730
2125.766850	83.352210	60.965735
2125.112252	84.572625	60.970740
2124.029409	88.306942	60.975745
2124.045103	86.680148	60.980750
2122.592089	77.600012	60.985754
2122.525146	80.930277	60.990759
2121.968029	82.907964	60.995764
2120.801370	83.402195	61.000769
2120.572110	85.283705	61.005774
2119.731838	91.045429	61.010778
2119.092181	87.205980	61.015783
2118.054888	89.004381	61.020788
2117.883162	98.287170	61.025793
2117.725108	89.987195	61.030798
2115.994183	91.245924	61.035802
2115.656416	89.075947	61.040807
2115.574732	85.938052	61.045812
2114.496073	87.823446	61.050817
2113.628608	80.979658	61.055822
2112.548718	89.761542	61.060826
2112.663103	90.781094	61.065831
2112.402338	83.427861	61.070836
2111.231073	87.258218	61.075841
2110.542022	86.295204	61.080846
2109.519084	90.857418	61.085850
2109.020896	96.306236	61.090855
2109.148696	94.530761	61.095860
2107.727109	88.782610	61.100865
2107.274451	92.262394	61.105870
2106.210615	88.688959	61.110874
2105.260692	94.135335	61.115879
2105.819020	93.195178	61.120884
2105.006565	97.640415	61.125889
2104.380977	80.722113	61.130894
2103.712602	92.316758	61.135898
2102.611865	91.463227	61.140903
2102.361851	87.260746	61.145908
2101.719022	88.968175	61.150913
2100.883847	90.926907	61.155918
2099.591493	93.007070	61.160922
2098.829661	91.565155	61.165927
2099.312373	84.926617	61.170932
2098.221249	92.727808	61.175937
2097.295987	88.438501	61.180942
2096.139551	88.768688	61.185946
2095.592863	92.001608	61.190951
2095.707941	83.811271	61.195956
2094.770420	85.598579	61.200961
2094.025924	84.852534	61.205966
2093.383523	89.723392	61.210970
2092.511226	91.642283	61.215975
2092.091424	88.617968	61.220980
2091.482839	96.115504	61.225985
2091.124086	80.744499	61.230990
2090.567903	87.121919	61.235994
2090.055991	90.292550	61.240999
2089.649852	79.726353	61.246004
2087.660906	96.108629	61.251009
2087.111206	83.289575	61.256014
2086.736558	90.767334	61.261018
2085.949608	91.792709	61.266023
2085.867750	83.934833	61.271028
2084.626034	88.383531	61.276033
2084.119131	89.006485	61.281038
2083.266911	85.634457	61.286042
2082.508845	88.632828	61.291047
2082.909476	78.548919	61.296052
2081.756381	84.631536	61.301057
2081.606977	90.209520	61.306062
2080.749603	90.911744	61.311066
2079.993124	92.151491	61.316071
2078.939528	92.769731	61.321076
2077.472449	91.277301	61.326081
2077.650461	84.132002	61.331086
2076.996385	91.773957	61.336090
2076.145869	92.143921	61.341095
2075.506861	91.365371	61.346100
2074.799514	90.829487	61.351105
2074.496789	84.545828	61.356110
2073.795855	82.439796	61.361114
2073.174598	92.347447	61.366119
2072.557506	89.687193	61.371124
2071.966943	92.539134	61.376129
2071.594436	90.568650	61.381134
2070.362340	90.642761	61.386138
2068.932156	90.350899	61.391143
2069.264536	84.702925	61.396148
2068.777664	91.993483	61.401153
2068.085941	91.623862	61.406158
2066.825068	87.137080	61.411162
2066.230570	90.350782	61.416167
2065.849550	86.902409	61.421172
2065.102213	89.430708	61.426177
2064.814181	77.819139	61.431182
2064.253134	84.202064	61.436186
2063.797554	85.425606	61.441191
2062.228843	77.882535	61.446196
2061.262267	82.071528	61.451201
2061.134156	79.833596	61.456206
2060.593564	87.173680	61.461210
2059.969915	81.380941	61.466215
2059.534395	81.653513	61.471220
2058.892852	82.947568	61.476225
2057.917075	84.832427	61.481230
2056.648756	88.629320	61.486234
2056.294538	92.188109	61.491239
2056.513245	79.687115	61.496244
2055.379109	92.413857	61.501249
2054.492046	87.624899	61.506254
2053.889878	95.023646	61.511258
2053.408640	89.471668	61.516263
2053.002172	90.827773	61.521268
2052.267344	88.274521	61.526273
2051.531364	79.959039	61.531278
2050.653712	84.108692	61.536282
2049.551172	90.970231	61.541287
2049.321614	84.082008	61.546292
2048.372199	89.939920	61.551297
2047.954931	86.396373	61.556302
2047.503351	86.017035	61.561306
2047.102964	91.328908	61.566311
2046.692437	81.334298	61.571316
2044.671665	88.597034	61.576321
2044.339478	87.613676	61.581326
2043.469107	81.421686	61.586330
2043.796483	87.651009	61.591335
2043.225482	86.076321	61.596340
2042.012963	93.154021	61.601345
2041.524055	84.886066	61.606350
2041.434383	89.533593	61.611354
2040.217251	89.851358	61.616359
2039.422513	83.648943	61.621364
2038.507339	87.798247	61.626369
2037.989761	84.805230	61.631374
2037.421176	83.987127	61.636378
2036.731092	94.501818	61.641383
2036.377818	92.946196	61.646388
2035.482761	87.300618	61.651393
2035.001252	79.121383	61.656398
2033.868049	93.188446	61.661402
2032.972451	92.139956	61.666407
2032.732081	87.276762	61.671412
2032.370101	94.544350	61.676417
2031.402454	83.751875	61.681422
2031.099670	90.839749	61.686426
2029.988824	92.358107	61.691431
2029.969002	86.319730	61.696436
2029.028260	89.239869	61.701441
2028.775854	88.852579	61.706446
2027.392691	86.153060	61.711450
2026.649922	97.702753	61.716455
2026.250941	87.200090	61.721460
2025.310717	91.875367	61.726465
2025.178628	85.074184	61.731470
2024.850302	88.319772	61.736474
2023.600248	94.916139	61.741479
2022.688366	92.349993	61.746484
2021.891827	90.273341	61.751489
2021.433491	84.604192	61.756494
2020.810543	90.520692	61.761498
2020.138844	88.944643	61.766503
2020.189679	86.631003	61.771508
2019.372646	89.965191	61.776513
2019.073474	85.984998	61.781518
2017.894034	85.801609	61.786522
2016.637209	90.855154	61.791527
2016.465824	81.019725	61.796532
2015.453745	90.770203	61.801537
2015.311189	81.691898	61.806542
2014.425464	85.257770	61.811546
2013.545764	84.709832	61.816551
2012.738275	81.149374	61.821556
2011.976664	93.823314	61.826561
2011.918847	85.904858	61.831566
2010.931140	94.446632	61.836570
2010.181868	95.322540	61.841575
2010.027249	88.258419	61.846580
2009.602153	84.225671	61.851585
2009.123628	83.547829	61.856590
2008.295047	83.195214	61.861594
2007.614629	85.528396	61.866599
2007.095678	85.407348	61.871604
2005.293151	83.856232	61.876609
2004.676341	84.957132	61.881614
2004.104321	89.537705	61.886618
2003.115276	89.549618	61.891623
2003.509693	87.932106	61.896628
2002.510529	90.765328	61.901633
2002.148767	80.917538	61.906638
2001.710504	86.858346	61.911642
2001.269835	78.923384	61.916647
2000.108168	85.819554	61.921652
1999.044021	92.654517	61.926657
1998.495061	89.863616	61.931662
1997.967207	84.508293	61.936666
1997.276603	87.330392	61.941671
1997.066167	72.244981	61.946676
1995.566370	77.136812	61.951681
1994.976901	86.307689	61.956686
1994.641176	80.843024	61.961690
1993.525795	78.386464	61.966695
1993.405678	76.642451	61.971700
1992.584778	84.810807	61.976705
1992.496457	78.693417	61.981710
1991.381610	83.587236	61.986714
1990.378425	87.632247	61.991719
1990.077391	79.679856	61.996724
1988.906079	91.313338	62.001729
1988.690145	88.330805	62.006734
1988.342046	84.117100	62.011738
1987.722797	86.517852	62.016743
1986.751391	81.243972	62.021748
1985.244565	91.940343	62.026753
1985.195276	89.888609	62.031758
1984.566861	89.928448	62.036762
1983.643055	87.651226	62.041767
1983.991857	83.112436	62.046772
1983.068269	88.644557	62.051777
1982.556299	81.206637	62.056782
1981.335560	85.226254	62.061786
1980.684755	91.686521	62.066791
1980.401281	76.554353	62.071796
1979.757223	84.685181	62.076801
1979.021043	78.479803	62.081806
1977.843794	76.091419	62.086810
1976.888695	85.627849	62.091815
1976.849022	72.139664	62.096820
1976.328008	77.812897	62.101825
1975.973638	79.389409	62.106830
1975.236353	81.144974	62.111834
1973.925259	85.764009	62.116839
1973.408820	83.269163	62.121844
1972.449244	86.493518	62.126849
1971.720335	83.718571	62.131854
1971.535270	92.189729	62.136858
1970.889702	87.026568	62.141863
1970.899753	77.034614	62.146868
1969.484563	76.764082	62.151873
1969.111952	81.604754	62.156878
1968.233220	80.001655	62.161882
1967.617512	89.053695	62.166887
1967.336107	72.077676	62.171892
1965.723738	80.324352	62.176897
1965.154978	77.068231	62.181902
1964.395598	77.972565	62.186906
1963.736535	83.293961	62.191911
1963.582871	74.859276	62.196916
1963.221688	80.549722	62.201921
1962.847969	72.077424	62.206926
1962.466980	79.001083	62.211930
1961.048262	78.570260	62.216935
1960.583539	72.235068	62.221940
1959.604214	74.855410	62.226945
1959.384120	76.366454	62.231950
1957.906727	76.047452	62.236954
1956.811602	80.860879	62.241959
1956.887817	74.466633	62.246964
1956.137233	79.625931	62.251969
1955.841671	77.879806	62.256974
1955.278549	74.271119	62.261978
1954.797006	82.188489	62.266983
1954.421600	76.930413	62.271988
1952.772517	79.087768	62.276993
1952.520932	76.404225	62.281998
1951.703231	81.321857	62.287002
1951.315326	86.882501	62.292007
1950.396643	81.540342	62.297012
1949.135408	76.009699	62.302017
1948.600978	73.383670	62.307022
1948.243696	75.094693	62.312026
1947.419599	79.104981	62.317031
1947.110724	71.283163	62.322036
1946.909954	82.328915	62.327041
1946.883332	81.609316	62.332046
1945.396309	74.804018	62.337050
1944.261253	82.710002	62.342055
1944.252310	73.971639	62.347060
1943.182581	73.613168	62.352065
1942.347290	74.609985	62.357070
1941.387469	84.144018	62.362074
1940.924961	78.302082	62.367079
1940.855304	69.601746	62.372084
1940.127533	79.102096	62.377089
1939.400287	80.307277	62.382094
1938.654357	83.554502	62.387098
1937.375317	81.385729	62.392103
1936.915261	77.476824	62.397108
1936.565837	85.464691	62.402113
1936.156225	82.066615	62.407118
1935.807710	75.544240	62.412122
1934.631690	85.582545	62.417127
1933.812016	76.752094	62.422132
1933.071414	83.852695	62.427137
1932.567031	80.824491	62.432142
1932.072890	77.293172	62.437146
1931.371196	74.244250	62.442151
1930.473726	80.735792	62.447156
1929.789370	86.455464	62.452161
1929.061970	81.090835	62.457166
1928.760181	79.479747	62.462170
1927.769384	89.171675	62.467175
1927.756273	77.994332	62.472180
1927.019504	88.716727	62.477185
1925.836634	83.596294	62.482190
1925.361985	78.084308	62.487194
1924.739067	85.196192	62.492199
1924.232012	73.751898	62.497204
1923.011523	87.511131	62.502209
1922.525896	86.138970	62.507214
1921.779769	82.934669	62.512218
1921.485175	80.451929	62.517223
1921.208647	85.622720	62.522228
1920.298428	83.381215	62.527233
1919.489171	82.030466	62.532238
1918.516405	82.634360	62.537242
1917.684238	82.864261	62.542247
1917.813697	83.327877	62.547252
1917.178761	86.182159	62.552257
1916.192364	80.570055	62.557262
1915.204751	80.561272	62.562266
1914.451868	85.150069	62.567271
1913.841026	80.288933	62.572276
1913.543393	86.812998	62.577281
1913.060231	83.630036	62.582286
1912.330318	81.574385	62.587290
1911.276763	80.828567	62.592295
1910.526276	84.317806	62.597300
1909.959877	81.562813	62.602305
1909.432166	78.353808	62.607310
1909.522628	79.107477	62.612314
1908.406591	81.131352	62.617319
1907.465098	76.989785	62.622324
1906.685973	83.875725	62.627329
1906.002490	79.685315	62.632334
1905.667935	79.013023	62.637338
1904.766019	85.599901	62.642343
1903.912180	78.135847	62.647348
1903.040070	82.727803	62.652353
1902.588565	93.543696	62.657358
1902.259264	80.546212	62.662362
1901.181087	82.822710	62.667367
1901.248948	80.916392	62.672372
1900.733002	81.816793	62.677377
1900.050968	76.724104	62.682382
1899.225766	81.568820	62.687386
1898.454904	85.379853	62.692391
1897.959508	70.793886	62.697396
1896.558452	84.572328	62.702401
1896.155408	86.401014	62.707406
1895.721394	80.751691	62.712410
1894.968860	88.089170	62.717415
1894.974357	78.115294	62.722420
1893.460219	85.056419	62.727425
1892.811698	86.767952	62.732430
1892.420579	79.298255	62.737434
1891.541928	87.652429	62.742439
1891.510767	72.565392	62.747444
1890.202918	89.661270	62.752449
1889.634606	81.169412	62.757454
1889.038562	87.811819	62.762458
1887.811242	89.227296	62.767463
1887.687763	76.452620	62.772468
1887.271562	86.373469	62.777473
1886.728500	87.164633	62.782478
1885.994912	82.747207	62.787482
1884.937562	82.413603	62.792487
1884.754994	69.755552	62.797492
1883.672453	80.091278	62.802497
1882.634670	83.274460	62.807502
1882.397672	76.182437	62.812506
1882.054350	82.623866	62.817511
1881.438244	83.443974	62.822516
1880.649187	83.703314	62.827521
1879.612015	81.616025	62.832526
1878.938611	77.979131	62.837530
1878.076050	94.589571	62.842535
1878.181181	85.593392	62.847540
1877.456891	84.036771	62.852545
1876.593768	83.379010	62.857550
1875.976478	84.151997	62.862554
1874.989387	83.140166	62.867559
1875.064683	81.830355	62.872564
1873.781475	78.069495	62.877569
1872.882978	75.395623	62.882574
1872.127424	79.358778	62.887578
1871.078488	80.182948	62.892583
1871.067813	75.955121	62.897588
1870.267581	93.230626	62.902593
1869.932414	85.483956	62.907598
1869.674606	87.445712	62.912602
1868.894526	83.578166	62.917607
1868.296097	82.081993	62.922612
1867.125458	81.034649	62.927617
1866.867620	85.551169	62.932622
1866.369513	78.363403	62.937626
1865.103691	84.637469	62.942631
1864.756923	76.979382	62.947636
1863.617291	77.759604	62.952641
1863.478462	80.773261	62.957646
1862.952768	82.891093	62.962650
1861.431894	80.535241	62.967655
1861.115026	78.854014	62.972660
1860.362006	77.193147	62.977665
1860.157583	75.815778	62.982670
1859.972473	73.937008	62.987674
1858.472549	84.898851	62.992679
1858.052567	71.288133	62.997684
1857.303601	66.010539	63.002689
1856.548895	72.559858	63.007694
1856.282006	72.688991	63.012698
1855.253806	86.652690	63.017703
1854.141610	79.109823	63.022708
1853.233579	77.937209	63.027713
1853.129189	79.423582	63.032718
1853.091579	81.000281	63.037722
1852.849342	82.546389	63.042727
1852.300333	70.662486	63.047732
1851.112062	90.898145	63.052737
1850.260363	80.669269	63.057742
1849.194471	76.791914	63.062746
1848.014947	80.062270	63.067751
1848.026088	71.539934	63.072756
1847.143988	84.272446	63.077761
1846.623714	74.516101	63.082766
1846.320896	74.098986	63.087770
1845.972319	76.127195	63.092775
1845.452810	73.971924	63.097780
1844.300469	86.110233	63.102785
1843.512275	79.115192	63.107790
1843.301229	83.433466	63.112794
1841.455924	77.248112	63.117799
1841.050374	69.976273	63.122804
1840.588551	86.710747	63.127809
1840.118275	81.248550	63.132814
1839.831594	73.904217	63.137818
1839.036634	77.197099	63.142823
1838.722900	71.465614	63.147828
1837.567726	78.600515	63.152833
1836.794182	76.968146	63.157838
1836.657197	82.851671	63.162842
1835.391641	79.736180	63.167847
1834.271849	77.682529	63.172852
1833.786066	84.495100	63.177857
1833.305984	73.921794	63.182862
1833.159419	69.948945	63.187866
1832.558789	76.385494	63.192871
1831.859385	73.721029	63.197876
1830.839598	77.073265	63.202881
1830.611794	74.933185	63.207886
1830.074641	77.090689	63.212890
1828.662056	87.444146	63.217895
1828.047294	74.693870	63.222900
1827.398217	86.438451	63.227905
1827.172139	82.941866	63.232910
1826.755942	83.738130	63.237914
1825.828969	88.398746	63.242919
1825.224892	81.353977	63.247924
1824.153939	79.172723	63.252929
1823.387252	76.007992	63.257934
1822.960133	76.493742	63.262938
1822.516276	76.715635	63.267943
1822.046849	78.182696	63.272948
1820.869853	82.955554	63.277953
1820.450667	77.056304	63.282958
1820.092878	73.760414	63.287962
1818.790292	75.720901	63.292967
1818.191039	74.535544	63.297972
1817.247420	68.875693	63.302977
1816.968899	65.488369	63.307982
1816.977202	61.888339	63.312986
1816.114871	78.074517	63.317991
1815.336645	65.583607	63.322996
1814.006262	72.225921	63.328001
1813.822018	75.372949	63.333006
1813.438921	74.823500	63.338010
1812.100152	77.322766	63.343015
1811.275099	66.444689	63.348020
1810.762228	77.541564	63.353025
1810.178937	82.221732	63.358030
1809.735937	76.829332	63.363034
1809.633182	85.259026	63.368039
1809.391170	70.948258	63.373044
1808.157906	69.887231	63.378049
1807.501800	78.666569	63.383054
1806.927354	74.963521	63.388058
1805.295045	82.350823	63.393063
1805.119669	76.452288	63.398068
1804.269741	75.201078	63.403073
1804.174771	78.091073	63.408078
1803.639773	69.631807	63.413082
1801.998181	87.391007	63.418087
1801.573362	83.861325	63.423092
1800.773785	83.843228	63.428097
1800.354771	85.272325	63.433102
1800.309493	74.740376	63.438106
1799.824908	82.409076	63.443111
1798.851280	76.779227	63.448116
1797.701941	81.801601	63.453121
1797.049015	78.333374	63.458126
1796.684026	74.161814	63.463130
1796.235678	80.060085	63.468135
1795.186808	72.863599	63.473140
1794.510727	84.500503	63.478145
1793.904090	67.784350	63.483150
1793.414960	74.247356	63.488154
1792.817364	80.085746	63.493159
1792.058359	72.406402	63.498164
1791.114245	75.879104	63.503169
1790.212592	74.388522	63.508174
1790.338860	75.141231	63.513178
1789.455205	79.506384	63.518183
1788.803034	74.951481	63.523188
1787.605727	86.535532	63.528193
1787.300455	88.148426	63.533198
1787.272662	76.126580	63.538202
1786.152826	83.449863	63.543207
1785.574808	71.540625	63.548212
1784.730054	76.369551	63.553217
1783.917213	79.092832	63.558222
1783.860432	66.629303	63.563226
1782.174382	73.979415	63.568231
1782.075285	70.645607	63.573236
1781.231781	81.110569	63.578241
1780.867192	82.016920	63.583246
1780.590897	78.485736	63.588250
1779.502932	80.710217	63.593255
1778.676833	74.197480	63.598260
1777.995003	75.291408	63.603265
1777.197039	66.151641	63.608270
1777.041932	69.584212	63.613274
1775.787214	83.325268	63.618279
1775.494622	75.136608	63.623284
1774.698732	77.871393	63.628289
1774.121701	73.284061	63.633294
1774.107182	80.518559	63.638298
1772.615357	79.918092	63.643303
1772.439389	78.102535	63.648308
1771.583365	80.129331	63.653313
1771.080270	78.499768	63.658318
1770.299531	77.683876	63.663322
1769.280314	86.448344	63.668327
1769.008577	77.294396	63.673332
1768.188349	83.221763	63.678337
1767.780246	73.882884	63.683342
1766.830758	68.867407	63.688346
1765.895730	72.565763	63.693351
1765.217832	71.539570	63.698356
1764.948513	73.104176	63.703361
1764.414257	76.238978	63.708366
1763.908590	74.169840	63.713370
1762.758454	79.566104	63.718375
1762.243062	74.123709	63.723380
1761.643266	74.739397	63.728385
1761.029508	77.773280	63.733390
1760.551946	67.499232	63.738394
1759.351152	85.967490	63.743399
1758.541078	71.592398	63.748404
1758.163895	77.298015	63.753409
1757.607485	75.927666	63.758414
1757.409563	71.792663	63.763418
1756.462444	75.784689	63.768423
1755.690195	75.968855	63.773428
1755.212268	75.021298	63.778433
1754.949239	78.953575	63.783438
1753.693941	79.493584	63.788442
1752.535814	81.502128	63.793447
1752.195883	72.644454	63.798452
1751.931667	76.509109	63.803457
1751.288504	72.306037	63.808462
1750.470889	70.675963	63.813466
1749.284012	78.801561	63.818471
1749.382634	76.410947	63.823476
1748.695219	74.928936	63.828481
1747.888218	74.106183	63.833486
1747.047321	69.049813	63.838490
1746.076273	68.795604	63.843495
1745.696819	70.494402	63.848500
1745.317847	77.711078	63.853505
1744.399951	70.028601	63.858510
1743.577259	66.155253	63.863514
1742.637927	75.976248	63.868519
1742.485048	66.718277	63.873524
1742.141785	71.689928	63.878529
1741.414167	74.953217	63.883534
1740.412624	73.486402	63.888538
1739.395152	79.300014	63.893543
1739.040172	69.553725	63.898548
1738.261924	69.596918	63.903553
1738.268784	75.675222	63.908558
1737.512028	68.148513	63.913562
1736.491996	79.743847	63.918567
1735.845245	70.461803	63.923572
1735.604053	69.470346	63.928577
1734.795372	73.177033	63.933582
1733.660488	68.930630	63.938586
1732.841068	62.066760	63.943591
1732.310933	59.760234	63.948596
1732.166705	76.138316	63.953601
1731.589189	71.294021	63.958606
1730.529541	70.520860	63.963610
1729.547637	75.015177	63.968615
1729.569203	67.555680	63.973620
1728.995472	71.359100	63.978625
1727.851577	75.213647	63.983630
1727.193818	65.804043	63.988634
1726.442272	77.954424	63.993639
1726.158054	63.476916	63.998644
1725.353390	68.047167	64.003649
1724.308088	73.089314	64.008654
1724.011370	68.189387	64.013658
1723.308260	78.177883	64.018663
1723.038646	70.315182	64.023668
1721.877540	73.459657	64.028673
1721.106205	74.411691	64.033678
1720.377865	73.308362	64.038682
1719.849637	79.424339	64.043687
1719.697772	71.790527	64.048692
1718.788288	72.220434	64.053697
1717.690477	74.451233	64.058702
1717.194809	70.595343	64.063706
1716.687526	68.102257	64.068711
1716.639219	70.325650	64.073716
1715.777229	73.771140	64.078721
1714.457883	73.811966	64.083726
1714.073144	73.024664	64.088730
1713.352588	77.043802	64.093735
1713.138800	62.692313	64.098740
1711.601427	77.720958	64.103745
1711.225728	83.858446	64.108750
1710.584491	76.387516	64.113754
1710.103021	81.658676	64.118759
1710.051833	67.016421	64.123764
1709.031074	71.261440	64.128769
1707.806775	75.396857	64.133774
1707.566954	71.148662	64.138778
1706.897589	78.217490	64.143783
1706.598287	70.417857	64.148788
1705.458856	80.265914	64.153793
1704.540764	75.138237	64.158798
1704.358219	64.054080	64.163802
1703.940589	76.298090	64.168807
1702.579948	75.995384	64.173812
1701.825161	78.884516	64.178817
1701.109336	74.577877	64.183822
1701.431758	80.889922	64.188826
1700.233297	72.827809	64.193831
1699.387865	76.311677	64.198836
1698.633555	76.628632	64.203841
1698.112646	79.267723	64.208846
1697.953347	74.191425	64.213850
1697.267242	72.969428	64.218855
1696.466048	72.524251	64.223860
1695.702134	77.423942	64.228865
1694.894050	66.201010	64.233870
1694.058474	76.030770	64.238874
1693.033537	83.654414	64.243879
1692.493344	71.830668	64.248884
1692.174033	74.410930	64.253889
1691.693643	74.391057	64.258894
1691.757506	75.275102	64.263898
1690.261152	73.454798	64.268903
1689.594786	72.977169	64.273908
1688.991489	81.852222	64.278913
1688.380867	76.852340	64.283918
1688.056650	69.394148	64.288922
1686.668572	79.043576	64.293927
1686.211433	75.668868	64.298932
1685.768902	70.145534	64.303937
1684.981311	67.919335	64.308942
1684.593523	77.491888	64.313946
1683.437110	80.861147	64.318951
1683.233984	77.898695	64.323956
1682.397332	75.724445	64.328961
1681.727156	84.821443	64.333966
1681.012321	77.917318	64.338970
1679.833081	78.453166	64.343975
1679.487354	69.897640	64.348980
1679.201744	75.158194	64.353985
1678.476874	69.116716	64.358990
1678.377055	65.737298	64.363994
1677.141107	74.178230	64.368999
1676.316115	74.995292	64.374004
1675.990514	75.920696	64.379009
1675.208796	78.613832	64.384014
1674.706481	77.558197	64.389018
1673.801478	79.119700	64.394023
1673.362633	78.058714	64.399028
1672.315004	72.208856	64.404033
1671.270726	73.155371	64.409038
1671.018744	74.315095	64.414042
1670.556862	82.573157	64.419047
1669.943951	74.914808	64.424052
1669.567525	86.062570	64.429057
1668.523701	83.230501	64.434062
1667.700918	78.901436	64.439066
1667.018122	83.496505	64.444071
1666.751586	80.496816	64.449076
1665.933321	79.327359	64.454081
1664.911033	78.866846	64.459086
1664.699523	74.912213	64.464090
1663.886482	80.204506	64.469095
1663.376044	74.660422	64.474100
1662.259041	77.886229	64.479105
1661.623474	70.895404	64.484110
1661.327366	77.130641	64.489114
1660.449930	80.752073	64.494119
1660.105912	72.177355	64.499124
1659.288971	69.683004	64.504129
1658.602424	81.894040	64.509134
1658.142481	75.411500	64.514138
1657.318659	80.863209	64.519143
1656.762491	66.603962	64.524148
1655.924252	77.053918	64.529153
1654.995601	73.421366	64.534158
1655.030604	78.052233	64.539162
1654.162052	71.393319	64.544167
1653.195409	63.537273	64.549172
1652.283886	73.308138	64.554177
1651.947389	82.084044	64.559182
1651.657630	74.358600	64.564186
1651.054080	73.241777	64.569191
1649.851555	66.978129	64.574196
1649.050178	70.954923	64.579201
1648.582418	81.357073	64.584206
1648.330841	73.846346	64.589210
1647.022957	75.557012	64.594215
1646.344607	68.568259	64.599220
1645.969808	79.840342	64.604225
1645.369808	75.253539	64.609230
1645.268085	67.928754	64.614234
1644.582038	80.731088	64.619239
1643.721443	76.469542	64.624244
1642.739596	77.396689	64.629249
1642.044299	81.760351	64.634254
1640.847474	75.088930	64.639258
1640.010359	80.230506	64.644263
1639.574557	72.842089	64.649268
1639.269117	73.308540	64.654273
1638.755391	74.126632	64.659278
1638.582467	70.443428	64.664282
1637.803403	76.911507	64.669287
1637.193350	68.257627	64.674292
1636.255205	79.816325	64.679297
1635.907113	81.872867	64.684302
1634.811888	68.651770	64.689306
1633.749948	80.540804	64.694311
1633.264757	66.243483	64.699316
1632.667928	71.913034	64.704321
1632.643112	81.655021	64.709326
1632.086830	69.587840	64.714330
1630.980331	74.740669	64.719335
1630.432869	66.173047	64.724340
1629.520004	77.570028	64.729345
1628.269690	77.199371	64.734350
1628.319900	69.389966	64.739354
1627.258470	80.578729	64.744359
1627.255358	73.041153	64.749364
1626.583815	77.727484	64.754369
1625.399597	83.357882	64.759374
1625.190997	68.841575	64.764378
1624.382847	78.293244	64.769383
1623.973034	67.801886	64.774388
1622.636813	72.210592	64.779393
1621.771789	74.858627	64.784398
1621.426511	73.327032	64.789402
1621.059204	77.088218	64.794407
1620.626309	79.738573	64.799412
1619.450535	78.266366	64.804417
1618.970186	76.678955	64.809422
1618.110666	71.644516	64.814426
1617.690747	76.492733	64.819431
1617.304066	74.046744	64.824436
1616.266528	72.874289	64.829441
1615.586701	77.082528	64.834446
1615.061278	70.162534	64.839450
1614.420178	74.993847	64.844455
1613.784972	69.650953	64.849460
1612.907310	75.300464	64.854465
1612.125738	78.288495	64.859470
1611.591555	68.433507	64.864474
1611.210472	75.630025	64.869479
1610.511211	73.121727	64.874484
1609.830805	69.511260	64.879489
1609.170260	77.002919	64.884494
1609.171817	66.138699	64.889498
1607.766429	75.074947	64.894503
1606.870550	72.184709	64.899508
1606.218452	77.508220	64.904513
1606.132835	75.779253	64.909518
1605.005481	66.027964	64.914522
1603.715066	76.811548	64.919527
1603.412987	64.811234	64.924532
1603.202493	71.938071	64.929537
1602.910210	81.916518	64.934542
1602.374133	74.359530	64.939546
1600.923002	81.560459	64.944551
1600.532459	71.304172	64.949556
1599.984319	74.550021	64.954561
1599.326359	73.200572	64.959566
1598.522857	68.340175	64.964570
1597.193460	83.983984	64.969575
1596.783579	79.955214	64.974580
1596.512460	78.479652	64.979585
1595.939529	72.507106	64.984590
1595.842666	67.857734	64.989594
1594.383148	81.002158	64.994599
1593.929412	72.291916	64.999604
1593.315462	77.314469	65.004609
1592.469632	73.612012	65.009614
1591.803689	65.066379	65.014618
1591.034329	74.060866	65.019623
1590.608600	75.350706	65.024628
1590.271737	74.286150	65.029633
1589.409199	77.206622	65.034638
1588.671243	71.711319	65.039642
1587.685256	79.480198	65.044647
1587.449273	68.473938	65.049652
1586.698902	69.949399	65.054657
1585.712465	74.676303	65.059662
1585.154719	72.593400	65.064666
1584.703907	76.345778	65.069671
1584.316454	69.588383	65.074676
1583.409418	73.216116	65.079681
1582.484880	72.172384	65.084686
1582.189236	70.457862	65.089690
1581.314726	75.990184	65.094695
1580.772137	61.575844	65.099700
1579.413934	71.818251	65.104705
1578.854855	75.535789	65.109710
1578.603347	63.741921	65.114714
1578.282450	77.839318	65.119719
1577.704734	67.995988	65.124724
1577.228782	74.308687	65.129729
1576.154669	78.450263	65.134734
1576.023519	81.472168	65.139738
1574.612642	79.870171	65.144743
1573.943926	76.275204	65.149748
1573.346878	82.023654	65.154753
1572.688660	81.249860	65.159758
1572.298647	77.172206	65.164762
1570.773091	80.920291	65.169767
1570.073919	77.328586	65.174772
1570.145887	90.182400	65.179777
1569.633950	80.552549	65.184782
1569.543683	75.296559	65.189786
1568.335898	73.044114	65.194791
1567.334916	70.675232	65.199796
1567.040185	75.112467	65.204801
1566.176194	81.067338	65.209806
1565.290042	79.430866	65.214810
1564.362574	81.754515	65.219815
1564.127673	80.399363	65.224820
1563.770433	75.367146	65.229825
1563.183225	73.131228	65.234830
1562.153505	79.421524	65.239834
1561.257961	80.820706	65.244839
1560.809149	81.032392	65.249844
1560.865385	78.410382	65.254849
1559.248551	84.011766	65.259854
1558.861690	70.848481	65.264858
1558.383442	80.733467	65.269863
1557.734360	72.459563	65.274868
1556.799683	72.679056	65.279873
1555.916591	77.099382	65.284878
1555.708319	62.243990	65.289882
1554.897862	70.787680	65.294887
1554.754700	64.589166	65.299892
1553.504215	66.708663	65.304897
1552.471039	78.962167	65.309902
1552.405477	72.475344	65.314906
1551.648537	74.822366	65.319911
1550.781686	72.772812	65.324916
1549.969000	76.625271	65.329921
1549.201017	77.632016	65.334926
1549.101147	67.607114	65.339930
1548.608492	74.416073	65.344935
1548.226365	74.087292	65.349940
1547.376331	73.413370	65.354945
1546.454096	74.222267	65.359950
1545.914394	64.368180	65.364954
1544.399389	76.882750	65.369959
1543.967301	67.429469	65.374964
1543.627183	71.463894	65.379969
1543.014735	73.286473	65.384974
1542.976908	64.707292	65.389978
1541.936852	75.648245	65.394983
1541.170651	73.395039	65.399988
1540.509878	71.725921	65.404993
1539.799353	76.202414	65.409998
1538.932218	73.444835	65.415002
1537.884916	76.069816	65.420007
1537.739587	74.427613	65.425012
1537.205175	78.442448	65.430017
1536.924197	85.839121	65.435022
1535.723681	76.731867	65.440026
1535.089341	78.091132	65.445031
1534.338774	73.414741	65.450036
1534.173369	78.492195	65.455041
1532.844008	81.251885	65.460046
1532.215998	74.288286	65.465050
1531.530488	82.715938	65.470055
1531.485875	81.305322	65.475060
1530.702281	73.054376	65.480065
1529.726396	77.344370	65.485070
1529.379385	69.418308	65.490074
1528.654291	77.962638	65.495079
1527.680308	76.272325	65.500084
1526.466333	74.575990	65.505089
1525.897493	72.185770	65.510094
1525.558954	67.030740	65.515098
1525.190036	79.214976	65.520103
1524.513351	69.956687	65.525108
1524.384022	65.922782	65.530113
1523.548079	67.191077	65.535118
1522.851688	66.595256	65.540122
1521.907151	71.495301	65.545127
1521.685488	72.642335	65.550132
1520.948711	75.869285	65.555137
1519.695474	76.989415	65.560142
1519.100294	70.266618	65.565146
1518.470508	87.914056	65.570151
1517.570208	83.210995	65.575156
1516.677135	80.041214	65.580161
1516.123979	79.518832	65.585166
1516.025719	69.586721	65.590170
1515.356836	79.757477	65.595175
1515.103827	73.529107	65.600180
1514.217081	76.387214	65.605185
1513.247139	66.852244	65.610190
1512.925634	72.107470	65.615194
1512.143140	71.700381	65.620199
1511.287171	69.740580	65.625204
1510.129910	74.004204	65.630209
1509.455445	68.350603	65.635214
1509.485973	65.983424	65.640218
1509.061059	71.392281	65.645223
1508.311509	63.509690	65.650228
1507.731183	67.407239	65.655233
1506.548052	79.104246	65.660238
1506.067455	70.981789	65.665242
1505.216218	68.767340	65.670247
1504.280839	68.073878	65.675252
1503.925641	69.527570	65.680257
1503.803447	74.046205	65.685262
1503.106603	59.938691	65.690266
1501.739151	80.311702	65.695271
1501.005153	75.117007	65.700276
1500.622794	67.223379	65.705281
1500.179996	71.081730	65.710286
1499.823724	59.835981	65.715290
1498.642711	72.787943	65.720295
1498.258384	65.391386	65.725300
1497.569933	67.916778	65.730305
1496.981972	75.964643	65.735310
1495.817807	69.660286	65.740314
1495.157148	68.759164	65.745319
1494.950585	65.797282	65.750324
1494.382677	62.186323	65.755329
1493.712096	61.985391	65.760334
1493.249473	65.358021	65.765338
1492.173147	75.047879	65.770343
1491.452958	68.335494	65.775348
1490.702069	73.225278	65.780353
1489.246719	74.801754	65.785358
1488.907982	71.949187	65.790362
1488.518414	72.533106	65.795367
1488.694276	66.960437	65.800372
1488.357574	65.392807	65.805377
1487.297689	77.664764	65.810382
1486.486461	63.638511	65.815386
1485.619702	66.411444	65.820391
1485.057582	62.192421	65.825396
1483.986684	68.115531	65.830401
1483.247612	69.500913	65.835406
1483.007372	68.331129	65.840410
1482.580191	71.057865	65.845415
1482.032842	69.418050	65.850420
1481.018729	74.762841	65.855425
1480.413611	67.753045	65.860430
1480.149533	62.803818	65.865434
1478.680367	69.263321	65.870439
1477.849993	74.343941	65.875444
1477.631043	68.990136	65.880449
1477.403684	71.388643	65.885454
1476.239025	63.579915	65.890458
1474.911013	78.203218	65.895463
1474.894491	73.537935	65.900468
1474.461003	74.010559	65.905473
1473.754876	83.539093	65.910478
1473.460377	71.701610	65.915482
1472.211089	73.078186	65.920487
1471.661190	73.492038	65.925492
1471.006248	73.449481	65.930497
1470.753889	81.322591	65.935502
1469.592961	72.306860	65.940506
1468.871399	74.708208	65.945511
1468.362735	73.765592	65.950516
1467.846251	70.334129	65.955521
1467.091592	76.132873	65.960526
1466.509042	74.922869	65.965530
1465.697757	73.008023	65.970535
1465.102009	76.217305	65.975540
1464.909114	74.434429	65.980545
1463.362481	77.553543	65.985550
1462.923879	73.357473	65.990554
1462.466510	77.024174	65.995559
1462.207836	73.288381	66.000564
1461.242813	73.668854	66.005569
1460.194026	82.520115	66.010574
1459.718222	72.359418	66.015578
1459.243393	73.817935	66.020583
1458.657604	80.681133	66.025588
1457.792647	77.238816	66.030593
1457.234284	74.350191	66.035598
1456.917322	71.664485	66.040602
1455.782485	74.409067	66.045607
1454.937378	70.842169	66.050612
1454.526314	70.470690	66.055617
1453.829811	67.435282	66.060622
1453.724214	64.949384	66.065626
1452.018130	79.178604	66.070631
1451.212822	80.801610	66.075636
1450.944249	74.640382	66.080641
1450.468202	75.495101	66.085646
1450.137782	65.790716	66.090650
1449.700135	70.807352	66.095655
1449.069315	73.643730	66.100660
1448.191897	74.830327	66.105665
1447.106206	72.415031	66.110670
1446.528413	67.236535	66.115674
1445.450585	69.133095	66.120679
1445.128443	65.607673	66.125684
1445.332683	72.439933	66.130689
1444.139751	79.191459	66.135694
1443.593055	69.928311	66.140698
1442.434429	75.215655	66.145703
1442.101256	69.712846	66.150708
1441.823286	67.218072	66.155713
1440.470216	74.157478	66.160718
1440.179265	70.141381	66.165722
1439.427155	76.661994	66.170727
1438.408303	68.448476	66.175732
1437.479691	65.019440	66.180737
1436.895784	72.281320	66.185742
1436.487581	67.030142	66.190746
1436.268837	72.059300	66.195751
1436.012711	66.405471	66.200756
1435.460552	71.077598	66.205761
1434.160161	73.091538	66.210766
1433.786612	62.096140	66.215770
1432.465753	64.602204	66.220775
1431.787471	70.899764	66.225780
1431.308497	68.181463	66.230785
1430.755878	71.084265	66.235790
1430.283081	65.868587	66.240794
1428.986812	73.552778	66.245799
1428.604215	65.067829	66.250804
1427.529644	66.598013	66.255809
1427.251071	68.176736	66.260814
1427.243862	67.487178	66.265818
1426.606718	65.718140	66.270823
1425.426417	61.047009	66.275828
1424.897968	57.281559	66.280833
1423.942568	76.497814	66.285838
1423.850499	69.130519	66.290842
1422.534298	67.210778	66.295847
1422.280477	68.075916	66.300852
1421.873061	71.668448	66.305857
1421.165312	71.579101	66.310862
1420.004313	72.634155	66.315866
1419.316924	75.365986	66.320871
1418.743181	74.195595	66.325876
1418.562397	75.350333	66.330881
1417.318793	71.957174	66.335886
1416.631070	61.502162	66.340890
1416.071480	70.067514	66.345895
1415.477621	74.465566	66.350900
1415.089510	72.521327	66.355905
1413.970122	76.044088	66.360910
1413.359563	63.378469	66.365914
1412.796484	66.653532	66.370919
1412.723801	69.811229	66.375924
1412.049124	60.193112	66.380929
1410.661429	65.174663	66.385934
1410.304336	59.880676	66.390938
1409.746562	73.209864	66.395943
1408.849745	64.891808	66.400948
1408.145850	64.046469	66.405953
1407.474828	69.488145	66.410958
1406.937265	66.544187	66.415962
1406.395995	66.728015	66.420967
1405.704109	63.909515	66.425972
1404.838407	62.082190	66.430977
1403.998379	67.479762	66.435982
1403.764996	65.471509	66.440986
1403.165760	66.252773	66.445991
1402.732438	62.439091	66.450996
1401.760655	60.582895	66.456001
1400.915081	73.164596	66.461006
1400.561721	64.121480	66.466010
1399.721859	64.942567	66.471015
1398.646493	69.251567	66.476020
1398.062815	67.057709	66.481025
1397.489026	74.187097	66.486030
1397.511662	63.179200	66.491034
1396.830521	70.942256	66.496039
1395.829118	68.534088	66.501044
1395.621816	64.419546	66.506049
1394.481471	71.260502	66.511054
1393.413410	65.808277	66.516058
1392.663683	64.727368	66.521063
1392.307288	66.543974	66.526068
1391.979642	65.932158	66.531073
1391.408818	71.099283	66.536078
1390.781369	65.476097	66.541082
1389.864569	71.415750	66.546087
1389.491140	61.041684	66.551092
1388.277102	64.331907	66.556097
1387.562402	65.057408	66.561102
1387.325228	60.110228	66.566106
1387.205273	71.352842	66.571111
1385.739317	73.766872	66.576116
1384.975539	65.372485	66.581121
1384.185004	71.978066	66.586126
1383.999001	64.904837	66.591130
1383.321456	72.301461	66.596135
1382.094912	70.941519	66.601140
1381.634299	64.959070	66.606145
1381.241863	72.822901	66.611150
1380.921883	63.749252	66.616154
1380.286773	69.804987	66.621159
1378.888639	63.654581	66.626164
1378.740173	63.274491	66.631169
1377.809140	58.494375	66.636174
1377.584930	60.722070	66.641178
1376.463741	74.896201	66.646183
1375.720091	72.841321	66.651188
1375.412056	74.973528	66.656193
1374.587102	71.501230	66.661198
1374.230096	61.851555	66.666202
1373.059650	72.188786	66.671207
1372.392028	64.629125	66.676212
1372.122487	60.784685	66.681217
1371.431972	70.471600	66.686222
1370.468445	70.760403	66.691226
1369.925803	81.332174	66.696231
1369.109077	77.278231	66.701236
1368.977705	69.704294	66.706241
1367.958351	69.246588	66.711246
1367.322326	64.315500	66.716250
1366.543111	76.968666	66.721255
1365.910953	70.548270	66.726260
1365.533276	64.838079	66.731265
1365.105332	69.872106	66.736270
1364.302271	70.077055	66.741274
1363.507853	69.031645	66.746279
1362.912087	71.040851	66.751284
1361.898789	67.081241	66.756289
1361.002266	74.973162	66.761294
1360.621607	63.210913	66.766298
1360.314332	68.601085	66.771303
1359.574376	66.685976	66.776308
1358.575930	62.686159	66.781313
1357.875486	80.038889	66.786318
1357.647274	66.572896	66.791322
1357.011904	66.948317	66.796327
1355.746427	71.344325	66.801332
1355.453475	62.525015	66.806337
1354.861557	68.723703	66.811342
1354.577842	70.208629	66.816346
1353.465216	72.303151	66.821351
1352.542985	76.240888	66.826356
1352.133131	67.630975	66.831361
1351.453527	70.274849	66.836366
1351.388171	59.263601	66.841370
1349.863801	67.264787	66.846375
1349.179517	67.048724	66.851380
1348.592088	68.353265	66.856385
1348.031515	68.839804	66.861390
1348.041035	67.106767	66.866394
1347.017548	70.022932	66.871399
1346.338625	62.950794	66.876404
1345.862546	59.397819	66.881409
1344.446519	67.788651	66.886414
1343.874802	63.381951	66.891418
1343.386937	65.862878	66.896423
1342.819103	69.283795	66.901428
1342.793226	58.887611	66.906433
1341.984514	71.583314	66.911438
1341.241363	71.537465	66.916442
1340.366033	80.531505	66.921447
1339.526115	73.876052	66.926452
1338.475187	65.514715	66.931457
1337.570210	73.980437	66.936462
1337.621597	75.462559	66.941466
1336.883801	78.550941	66.946471
1336.400921	76.005173	66.951476
1336.303929	75.564862	66.956481
1334.862193	78.202158	66.961486
1334.316247	68.443748	66.966490
1333.892223	70.794677	66.971495
1332.966873	78.405753	66.976500
1331.904332	65.911365	66.981505
1331.348345	69.514909	66.986510
1331.090540	63.580660	66.991514
1330.396678	66.179494	66.996519
1329.738579	65.672260	67.001524
1329.234055	71.043328	67.006529
1328.367045	73.770617	67.011534
1328.158387	64.385961	67.016538
1327.252212	73.520524	67.021543
1326.019858	74.221098	67.026548
1325.580825	72.567253	67.031553
1324.557494	69.885048	67.036558
1324.562056	60.090384	67.041562
1324.262267	67.334708	67.046567
1323.320826	69.523458	67.051572
1322.509812	62.204236	67.056577
1321.907868	74.455477	67.061582
1321.235866	67.046344	67.066586
1319.968069	66.095127	67.071591
1319.468185	66.978890	67.076596
1319.208832	64.668836	67.081601
1318.638732	68.553756	67.086606
1318.116225	68.220517	67.091610
1316.978334	70.412114	67.096615
1316.571506	71.698989	67.101620
1316.316030	63.521876	67.106625
1314.976171	72.793198	67.111630
1314.082687	63.448028	67.116634
1313.498053	61.982130	67.121639
1312.978632	73.818906	67.126644
1312.890625	63.524066	67.131649
1311.758239	73.006842	67.136654
1311.012924	67.760396	67.141658
1310.608829	71.160019	67.146663
1310.163635	69.571815	67.151668
1309.798308	69.664612	67.156673
1308.211121	71.377267	67.161678
1307.871673	64.651730	67.166682
1307.240065	70.872506	67.171687
1306.950574	71.910487	67.176692
1306.041349	68.431110	67.181697
1304.787258	71.830244	67.186702
1304.328575	63.304594	67.191706
1304.331006	68.570625	67.196711
1303.408567	72.058963	67.201716
1302.761685	65.956331	67.206721
1301.720700	73.458060	67.211726
1301.544365	74.323506	67.216730
1300.867152	64.369140	67.221735
1299.831381	72.709793	67.226740
1299.290817	68.080524	67.231745
1298.778031	74.299760	67.236750
1298.303696	68.346320	67.241754
1297.490475	64.587538	67.246759
1296.542787	72.772258	67.251764
1295.998452	65.780455	67.256769
1295.236646	72.568364	67.261774
1294.718592	62.505117	67.266778
1294.102527	67.683392	67.271783
1293.519312	78.515515	67.276788
1292.998774	67.243889	67.281793
1291.467532	67.917879	67.286798
1290.743999	70.929884	67.291802
1290.301135	72.131027	67.296807
1290.152775	61.766148	67.301812
1289.595253	66.074862	67.306817
1289.084668	68.388306	67.311822
1288.380585	66.234909	67.316826
1287.468583	72.124153	67.321831
1286.803104	73.759671	67.326836
1286.375935	64.899421	67.331841
1285.020360	75.992326	67.336846
1284.676286	56.434691	67.341850
1284.094704	67.963581	67.346855
1283.963656	68.739035	67.351860
1283.449026	67.873891	67.356865
1282.049404	75.384547	67.361870
1281.669476	64.085053	67.366874
1280.680506	65.860314	67.371879
1279.195274	72.365840	67.376884
1278.830886	57.458857	67.381889
1278.228587	66.166635	67.386894
1278.340279	64.038876	67.391898
1277.856026	73.215972	67.396903
1277.364683	72.590772	67.401908
1276.728201	66.476244	67.406913
1275.707102	62.815966	67.411918
1275.313683	59.530571	67.416922
1273.948824	69.282136	67.421927
1273.025625	67.372534	67.426932
1272.953742	65.065797	67.431937
1272.369726	71.014865	67.436942
1272.122098	70.371419	67.441946
1271.019326	69.718062	67.446951
1270.252866	73.797431	67.451956
1270.149704	62.849764	67.456961
1268.548237	70.681107	67.461966
1267.742345	66.662542	67.466970
1266.999901	63.021043	67.471975
1266.934377	62.913210	67.476980
1266.536209	61.257611	67.481985
1265.996013	63.734255	67.486990
1265.051453	59.402628	67.491994
1264.271049	62.866817	67.496999
1264.063366	63.358768	67.502004
1263.153518	63.730543	67.507009
1262.170406	68.655725	67.512014
1261.661884	62.389179	67.517018
1261.250630	66.885960	67.522023
1260.092581	71.047304	67.527028
1259.413407	59.384590	67.532033
1258.323612	64.744640	67.537038
1258.403058	66.626009	67.542042
1257.835807	65.940341	67.547047
1257.345547	68.759141	67.552052
1256.831428	65.398319	67.557057
1255.443711	69.585143	67.562062
1254.906189	66.830456	67.567066
1254.450421	70.321882	67.572071
1253.642351	68.479139	67.577076
1252.838345	69.822867	67.582081
1252.070726	72.072316	67.587086
1251.987944	58.903364	67.592090
1251.502491	71.279594	67.597095
1250.616947	63.584309	67.602100
1250.193545	64.124754	67.607105
1249.270473	69.726389	67.612110
1248.676923	67.855847	67.617114
1247.613621	67.438295	67.622119
1246.834879	72.264754	67.627124
1246.627339	65.731150	67.632129
1246.046199	67.485735	67.637134
1245.443330	58.589568	67.642138
1244.137349	71.075764	67.647143
1243.897450	61.286072	67.652148
1243.622262	51.431033	67.657153
1242.176573	58.367901	67.662158
1242.079375	55.847567	67.667162
1241.074914	58.480038	67.672167
1240.753028	60.873087	67.677172
1239.942178	55.268073	67.682177
1238.745181	58.945170	67.687182
1238.288603	58.762318	67.692186
1237.662046	62.154742	67.697191
1237.267072	55.162078	67.702196
1237.228320	51.236808	67.707201
1235.786359	55.115287	67.712206
1235.375151	62.144721	67.717210
1234.803253	53.078051	67.722215
1233.774196	55.706551	67.727220
1233.096832	52.699710	67.732225
1232.270314	50.361579	67.737230
1231.918211	48.771205	67.742234
1231.641582	59.187131	67.747239
1230.539534	57.290214	67.752244
1229.973508	59.897131	67.757249
1228.958196	61.671868	67.762254
1228.856191	49.020087	67.767258
1228.281362	55.638708	67.772263
1227.130504	50.554557	67.777268
1226.632347	53.674245	67.782273
1225.764225	55.297841	67.787278
1225.544342	46.350252	67.792282
1224.620057	50.920724	67.797287
1223.719424	58.253493	67.802292
1223.224485	53.402522	67.807297
1222.634694	57.205429	67.812302
1222.371420	57.371900	67.817306
1221.175561	58.303269	67.822311
1220.148938	56.772843	67.827316
1220.098152	57.395972	67.832321
1219.434715	65.752348	67.837326
1219.297325	52.576320	67.842330
1218.179898	56.078341	67.847335
1217.499563	58.930525	67.852340
1216.981746	52.678088	67.857345
1216.153587	61.059078	67.862350
1215.444520	49.577766	67.867354
1214.500736	50.804955	67.872359
1213.885227	59.399718	67.877364
1213.620213	53.512372	67.882369
1212.531848	64.705526	67.887374
1212.026092	53.275464	67.892378
1211.093473	56.913685	67.897383
1210.352972	53.891659	67.902388
1210.771491	56.053430	67.907393
1209.791803	58.204143	67.912398
1208.452098	55.067659	67.917402
1208.050839	53.988167	67.922407
1207.683933	55.625111	67.927412
1207.395659	52.015495	67.932417
1206.357596	54.899334	67.937422
1205.820471	49.958880	67.942426
1205.161992	56.504072	67.947431
1204.315272	55.771392	67.952436
1203.470569	54.478557	67.957441
1202.873247	51.148329	67.962446
1202.300104	47.279655	67.967450
1201.184451	63.231796	67.972455
1200.633224	61.017059	67.977460
1200.871640	60.955515	67.982465
1199.905097	60.096807	67.987470
1199.254444	56.691478	67.992474
1198.301208	61.824823	67.997479
1197.422564	56.006673	68.002484
1197.330933	53.810318	68.007489
1195.814476	57.916713	68.012494
1195.154391	53.274943	68.017498
1194.640374	52.590287	68.022503
1194.003718	52.906025	68.027508
1194.199850	49.064836	68.032513
1193.074208	54.733389	68.037518
1192.271853	55.963328	68.042522
1191.864113	46.727065	68.047527
1190.885747	51.429154	68.052532
1190.538551	53.140237	68.057537
1189.648944	56.538230	68.062542
1188.897295	50.042282	68.067546
1188.386675	59.180203	68.072551
1187.857299	60.647438	68.077556
1186.976922	50.708875	68.082561
1185.963345	59.653959	68.087566
1185.781880	52.953793	68.092570
1185.244986	57.114158	68.097575
1184.813631	55.689363	68.102580
1184.040737	58.396996	68.107585
1182.769867	59.603671	68.112590
1182.630353	45.970665	68.117594
1181.653472	51.629758	68.122599
1180.390388	59.739289	68.127604
1180.216360	61.069589	68.132609
1179.635854	62.896627	68.137614
1179.473026	59.703893	68.142618
1179.164456	50.221619	68.147623
1177.691925	55.267235	68.152628
1177.164819	52.111933	68.157633
1176.650683	64.773429	68.162638
1176.038240	54.658213	68.167642
1174.897559	57.198828	68.172647
1174.261463	58.045930	68.177652
1174.092887	56.727585	68.182657
1173.002539	62.048328	68.187662
1172.188143	58.050864	68.192666
1171.536629	49.924153	68.197671
1171.027048	51.981193	68.202676
1170.891890	49.187773	68.207681
1170.300043	52.079511	68.212686
1169.096518	51.605442	68.217690
1168.342669	61.051714	68.222695
1167.823215	56.310314	68.227700
1167.676577	52.249236	68.232705
1166.451670	63.052522	68.237710
1165.914781	58.607216	68.242714
1165.395410	55.619424	68.247719
1164.667464	60.067228	68.252724
1163.671301	55.311753	68.257729
1162.892588	55.812522	68.262734
1162.366165	54.194687	68.267738
1162.103702	61.389711	68.272743
1161.584320	60.928271	68.277748
1160.637790	55.661842	68.282753
1159.725247	65.477141	68.287758
1159.223395	50.911406	68.292762
1159.160814	55.130387	68.297767
1157.910666	57.007155	68.302772
1157.341840	59.318056	68.307777
1156.621984	53.436822	68.312782
1156.077385	53.264830	68.317786
1155.224589	58.450025	68.322791
1154.345289	59.632286	68.327796
1154.148086	53.820900	68.332801
1153.326029	62.218281	68.337806
1153.403886	47.754326	68.342810
1152.501036	62.239146	68.347815
1151.496838	61.078930	68.352820
1150.267915	56.404635	68.357825
1149.212839	58.950570	68.362830
1148.998113	55.439656	68.367834
1148.254841	58.973665	68.372839
1147.740550	61.452518	68.377844
1147.821806	53.652409	68.382849
1146.920611	62.573325	68.387854
1146.604626	58.214320	68.392858
1145.459906	51.683128	68.397863
1144.970447	55.742913	68.402868
1144.696344	56.360558	68.407873
1143.135653	61.158434	68.412878
1142.498775	55.942116	68.417882
1142.068318	54.597612	68.422887
1141.779497	57.619364	68.427892
1141.323777	57.854298	68.432897
1139.969613	55.213753	68.437902
1139.297222	52.196687	68.442906
1138.696267	47.939781	68.447911
1138.117178	64.051037	68.452916
1137.107871	54.613983	68.457921
1136.594636	57.419108	68.462926
1136.656472	54.775714	68.467930
1136.294275	52.669705	68.472935
1134.848421	59.024740	68.477940
1134.323611	51.388836	68.482945
1133.602299	59.088935	68.487950
1132.670135	60.952989	68.492954
1132.151968	53.839591	68.497959
1131.347976	61.182247	68.502964
1130.900877	53.382591	68.507969
1130.244514	55.380981	68.512974
1129.926242	48.324105	68.517978
1128.660201	51.658981	68.522983
1128.113043	62.368678	68.527988
1127.869562	50.226708	68.532993
1126.896410	48.943291	68.537998
1125.668054	55.552326	68.543002
1125.519050	52.655453	68.548007
1124.666881	57.170333	68.553012
1124.647050	51.996233	68.558017
1123.936196	59.473891	68.563022
1123.047181	50.792020	68.568026
1122.485530	52.395291	68.573031
1121.712822	57.203471	68.578036
1121.353717	45.494646	68.583041
1120.105375	61.311788	68.588046
1119.695338	49.656795	68.593050
1119.356013	56.498179	68.598055
1118.011186	55.579818	68.603060
1117.128066	51.705273	68.608065
1116.619615	56.700087	68.613070
1116.404624	53.044136	68.618074
1116.200541	52.764375	68.623079
1115.166632	59.074400	68.628084
1114.509828	50.656805	68.633089
1113.597586	61.085516	68.638094
1113.019419	49.832591	68.643098
1112.611098	53.644502	68.648103
1111.411191	55.896511	68.653108
1111.053793	52.837238	68.658113
1110.319186	59.714687	68.663118
1110.278353	52.159511	68.668122
1108.981881	56.467512	68.673127
1108.439875	55.132872	68.678132
1107.946334	58.106762	68.683137
1107.262223	60.641019	68.688142
1106.315182	59.812362	68.693146
1105.517005	59.810028	68.698151
1105.132594	57.901528	68.703156
1104.966085	57.306700	68.708161
1103.751476	65.142042	68.713166
1103.061313	57.598679	68.718170
1102.531507	57.712936	68.723175
1101.727077	52.293041	68.728180
1101.760847	52.352351	68.733185
1100.281870	60.920466	68.738190
1099.642384	47.513662	68.743194
1099.467026	48.520893	68.748199
1098.766423	55.583750	68.753204
1097.845262	56.671761	68.758209
1096.783430	62.584101	68.763214
1096.399854	56.958489	68.768218
1096.302962	59.724206	68.773223
1095.127000	60.106828	68.778228
1094.146830	52.387243	68.783233
1093.294272	57.777426	68.788238
1093.334803	63.755704	68.793242
1093.102265	55.027772	68.798247
1092.374538	57.218877	68.803252
1091.444166	61.754091	68.808257
1090.817414	59.584511	68.813262
1090.068477	60.350232	68.818266
1088.991791	53.413999	68.823271
1088.281572	58.956589	68.828276
1088.104493	53.266594	68.833281
1087.207799	65.891174	68.838286
1086.999418	56.019231	68.843290
1086.008857	57.288601	68.848295
1085.190198	56.783316	68.853300
1085.062047	50.338044	68.858305
1083.855209	65.311216	68.863310
1083.001900	59.498543	68.868314
1082.439824	56.389827	68.873319
1082.091955	51.439802	68.878324
1082.093562	49.236509	68.883329
1080.530502	60.536748	68.888334
1080.002566	53.593657	68.893338
1079.523191	59.504818	68.898343
1078.597799	60.975142	68.903348
1078.091267	50.215473	68.908353
1076.908737	62.022902	68.913358
1076.702352	60.966052	68.918362
1076.159041	55.578748	68.923367
1075.628583	61.808704	68.928372
1074.829111	57.815210	68.933377
1073.616184	67.845475	68.938382
1074.009812	48.660237	68.943386
1073.156054	54.186237	68.948391
1071.978443	59.847335	68.953396
1071.366824	48.558745	68.958401
1070.382472	54.887709	68.963406
1070.341387	50.841392	68.968410
1069.595707	49.947602	68.973415
1068.412003	51.828035	68.978420
1067.904934	46.289888	68.983425
1067.452502	58.692405	68.988430
1067.342856	50.969979	68.993434
1066.420310	54.466292	68.998439
1065.387045	55.378176	69.003444
1065.254434	45.771743	69.008449
1064.267968	52.881656	69.013454
1063.212672	54.246490	69.018458
1063.015855	48.047117	69.023463
1062.368201	45.409350	69.028468
1061.943886	46.320564	69.033473
1060.596651	51.125530	69.038478
1060.134955	54.595845	69.043482
1059.378492	60.795521	69.048487
1059.223117	59.577589	69.053492
1058.471101	52.831004	69.058497
1057.493174	57.641882	69.063502
1056.858876	55.943456	69.068506
1056.356524	50.160127	69.073511
1055.116160	59.727968	69.078516
1054.524172	52.998506	69.083521
1053.838177	57.535859	69.088526
1053.774840	59.239652	69.093530
1053.403816	55.288399	69.098535
1052.705020	54.984836	69.103540
1051.643743	56.841072	69.108545
1051.096184	60.523750	69.113550
1050.284287	52.566099	69.118554
1049.445693	58.957042	69.123559
1048.345744	61.008670	69.128564
1048.148427	53.114107	69.133569
1047.274244	58.742715	69.138574
1047.046548	55.227569	69.143578
1047.340946	51.386511	69.148583
1045.756101	58.356651	69.153588
1045.412355	51.649205	69.158593
1044.330661	55.927801	69.163598
1043.797751	47.403789	69.168602
1042.824173	47.645426	69.173607
1042.016211	54.933537	69.178612
1041.758647	51.309600	69.183617
1041.114030	53.542691	69.188622
1040.932435	51.679210	69.193626
1039.756902	54.599173	69.198631
1039.141410	58.716872	69.203636
1038.619631	51.384874	69.208641
1037.141155	52.115276	69.213646
1036.536845	51.118579	69.218650
1036.160365	49.287680	69.223655
1035.571792	53.667607	69.228660
1035.793123	43.017676	69.233665
1034.532317	55.859459	69.238670
1033.930068	59.216517	69.243674
1033.380381	51.931539	69.248679
1032.593958	56.502219	69.253684
1031.764323	45.126901	69.258689
1030.861764	55.987762	69.263694
1030.204814	52.741185	69.268698
1029.783842	58.057995	69.273703
1029.447118	52.581068	69.278708
1028.490495	49.038382	69.283713
1027.663175	57.811952	69.288718
1027.191966	49.752803	69.293722
1027.038755	59.606607	69.298727
1025.957643	56.380200	69.303732
1025.315320	51.518033	69.308737
1024.559496	53.924942	69.313742
1024.034079	45.972194	69.318746
1023.273304	51.540185	69.323751
1022.150423	58.192410	69.328756
1021.802159	48.473630	69.333761
1021.415197	56.371300	69.338766
1020.658037	58.346327	69.343770
1020.100464	56.875408	69.348775
1019.080057	54.356879	69.353780
1019.125970	50.903867	69.358785
1018.241275	55.950668	69.363790
1017.427789	56.906456	69.368794
1016.843602	57.243854	69.373799
1015.859044	61.975376	69.378804
1015.020950	57.973854	69.383809
1014.119228	59.648598	69.388814
1013.875438	56.363103	69.393818
1013.421374	54.714865	69.398823
1012.470422	58.903285	69.403828
1012.680296	53.750997	69.408833
1011.778570	59.183719	69.413838
1010.960185	55.188526	69.418842
1009.885150	53.506615	69.423847
1008.708150	54.690554	69.428852
1008.545594	53.252990	69.433857
1007.761895	66.335862	69.438862
1007.346725	57.991825	69.443866
1006.880270	54.640828	69.448871
1006.293896	62.089245	69.453876
1005.494692	62.017718	69.458881
1004.799263	61.322539	69.463886
1004.285385	57.129087	69.468890
1002.933723	56.426347	69.473895
1002.110164	69.048773	69.478900
1001.805316	50.176519	69.483905
1001.208685	58.282595	69.488910
1000.935487	54.224323	69.493914
1000.306199	54.021683	69.498919
999.820695	59.684664	69.503924
999.080645	55.798441	69.508929
998.169650	59.870119	69.513934
997.755230	55.403796	69.518938
996.708676	54.843333	69.523943
995.702818	63.475003	69.528948
995.775434	51.864682	69.533953
995.175270	62.876146	69.538958
994.280981	64.045076	69.543962
993.617893	59.796516	69.548967
993.117293	67.860511	69.553972
992.295822	52.549304	69.558977
990.992594	60.037655	69.563982
990.796634	60.154015	69.568986
990.138713	61.149718	69.573991
989.599397	60.782952	69.578996
989.349764	59.580022	69.584001
988.505620	60.015558	69.589006
987.592882	58.132787	69.594010
987.053729	51.320822	69.599015
985.735472	57.420658	69.604020
985.428557	49.814787	69.609025
984.753756	66.483767	69.614030
984.379115	61.456013	69.619034
983.993169	55.540636	69.624039
982.672228	63.265206	69.629044
982.231395	55.393627	69.634049
981.727625	59.622875	69.639054
981.075241	56.643675	69.644058
980.242498	52.926752	69.649063
979.500769	54.227536	69.654068
979.032247	60.364069	69.659073
978.545137	58.008294	69.664078
977.880145	59.863010	69.669082
976.858517	60.903969	69.674087
976.075052	57.742193	69.679092
975.775285	52.387133	69.684097
975.106259	55.404735	69.689102
974.586570	62.665922	69.694106
973.952911	52.491076	69.699111
972.886274	57.153667	69.704116
972.570981	56.694488	69.709121
971.302341	59.271318	69.714126
970.921524	61.793622	69.719130
970.469201	51.506344	69.724135
969.857303	59.955485	69.729140
968.934510	55.475437	69.734145
967.633158	59.205524	69.739150
967.510610	56.865865	69.744154
967.322502	51.969292	69.749159
966.640431	54.930623	69.754164
966.271270	47.888186	69.759169
965.174588	54.052124	69.764174
964.386665	57.123341	69.769178
964.107565	52.797925	69.774183
963.015021	55.824568	69.779188
962.441702	58.677131	69.784193
961.852194	56.241456	69.789198
961.267073	51.512136	69.794202
960.502015	58.490659	69.799207
959.273270	69.745655	69.804212
958.944847	54.434861	69.809217
958.515198	72.597679	69.814222
958.224677	58.260164	69.819226
957.535699	57.466198	69.824231
956.303289	64.374004	69.829236
956.250248	58.618556	69.834241
955.037775	63.911502	69.839246
953.985964	58.753379	69.844250
953.679519	53.648550	69.849255
953.015281	61.994056	69.854260
952.863434	51.884483	69.859265
952.333346	57.631835	69.864270
951.656279	57.471504	69.869274
950.489662	56.709385	69.874279
950.046374	62.651092	69.879284
949.684741	56.694005	69.884289
948.355772	62.782949	69.889294
947.371700	56.942251	69.894298
947.082601	56.015272	69.899303
946.669438	57.330017	69.904308
946.715326	54.501499	69.909313
944.991965	53.780662	69.914318
944.465204	58.880920	69.919322
944.412404	47.177021	69.924327
942.860824	55.193776	69.929332
942.235438	50.716880	69.934337
941.418000	54.600219	69.939342
941.269756	48.367902	69.944346
940.912876	55.741960	69.949351
940.139727	60.860924	69.954356
939.817197	57.190566	69.959361
938.725972	57.883059	69.964366
938.219371	52.970936	69.969370
937.864324	50.125790	69.974375
936.100799	61.975253	69.979380
935.716132	50.598557	69.984385
935.145726	56.659841	69.989390
935.136415	52.364042	69.994394
934.254443	55.327226	69.999399
933.095310	60.837203	70.004404
932.807765	43.936622	70.009409
932.263803	55.292390	70.014414
931.698212	47.868046	70.019418
930.712634	53.183243	70.024423
929.567425	58.758815	70.029428
929.544360	54.807412	70.034433
929.226780	61.065016	70.039438
928.199448	58.863026	70.044442
927.859318	57.677658	70.049447
926.789600	56.360799	70.054452
925.996923	50.811365	70.059457
925.102858	59.762741	70.064462
924.750788	59.290497	70.069466
924.247554	51.838883	70.074471
923.569286	63.018906	70.079476
923.237015	54.912442	70.084481
922.191807	59.366633	70.089486
921.348578	55.922643	70.094490
921.096644	54.664893	70.099495
920.338045	48.460317	70.104500
919.392997	42.794783	70.109505
918.886250	50.011333	70.114510
917.938732	54.934115	70.119514
917.981490	46.275957	70.124519
916.696635	59.265118	70.129524
916.140933	45.026598	70.134529
915.493840	56.852954	70.139534
915.221219	59.007955	70.144538
914.258571	55.840021	70.149543
913.288338	69.143410	70.154548
913.056937	54.805965	70.159553
912.317998	52.417739	70.164558
911.814464	52.941027	70.169562
910.768753	52.697441	70.174567
909.874720	65.473026	70.179572
909.415325	52.540696	70.184577
909.370441	62.400913	70.189582
908.704328	60.862135	70.194586
907.622445	51.495097	70.199591
906.878428	55.600157	70.204596
906.433083	50.583675	70.209601
905.290964	58.609411	70.214606
904.410796	57.882156	70.219610
904.443478	45.853993	70.224615
903.875667	58.112446	70.229620
903.738606	51.145053	70.234625
902.469839	55.478704	70.239630
901.850024	49.047040	70.244634
901.417017	53.304462	70.249639
899.891343	52.597930	70.254644
899.488467	55.303529	70.259649
898.777397	55.508177	70.264654
898.643771	55.141527	70.269658
898.081043	54.144555	70.274663
897.028826	59.566567	70.279668
896.197190	54.931689	70.284673
895.817803	61.184938	70.289678
895.218879	57.296792	70.294682
894.470932	55.037741	70.299687
893.357192	56.227435	70.304692
893.240396	45.893096	70.309697
892.382550	60.514309	70.314702
892.019563	54.973777	70.319706
891.126565	56.426395	70.324711
890.243513	50.268444	70.329716
889.918001	49.429271	70.334721
889.448715	51.584030	70.339726
888.508489	51.970233	70.344730
887.603879	40.624263	70.349735
886.890510	53.096694	70.354740
886.681113	55.164362	70.359745
886.124698	51.504427	70.364750
884.928022	54.893034	70.369754
884.403182	51.213881	70.374759
883.864360	51.335927	70.379764
883.615382	39.492948	70.384769
882.689681	51.459840	70.389774
881.745253	44.619364	70.394778
881.113127	47.667384	70.399783
880.905273	55.481363	70.404788
880.165177	52.620233	70.409793
879.589179	60.666273	70.414798
878.968219	46.188987	70.419802
877.654562	43.130551	70.424807
876.815714	51.461274	70.429812
876.164539	49.256216	70.434817
875.932514	49.622758	70.439822
875.788700	48.582778	70.444826
874.925838	44.888037	70.449831
873.524436	57.490474	70.454836
873.069682	47.023838	70.459841
872.727511	54.723572	70.464846
872.177183	54.964149	70.469850
871.271493	51.003404	70.474855
870.218381	58.086139	70.479860
870.047950	48.337517	70.484865
869.498228	53.263239	70.489870
868.818135	62.019724	70.494874
867.968694	51.713674	70.499879
867.037585	62.096563	70.504884
867.005241	52.354348	70.509889
866.246961	47.975898	70.514894
865.161699	58.507900	70.519898
865.008370	55.759975	70.524903
863.976872	56.241140	70.529908
863.885692	46.866270	70.534913
862.754536	55.568381	70.539918
861.710784	60.982751	70.544922
861.759409	53.345550	70.549927
860.396862	56.320587	70.554932
859.574588	52.732933	70.559937
859.056938	58.790565	70.564942
858.365480	50.078948	70.569946
858.100873	57.020422	70.574951
857.734234	55.287337	70.579956
857.777473	44.635791	70.584961
856.389410	53.426100	70.589966
855.766968	53.769623	70.594970
854.881466	49.802519	70.599975
853.652510	56.566307	70.604980
853.161618	51.911909	70.609985
852.945181	51.686177	70.614990
852.468879	49.762384	70.619994
851.922228	55.105523	70.624999
850.714766	58.517940	70.630004
850.243054	55.858538	70.635009
849.528519	50.519051	70.640014
848.719079	51.173042	70.645018
847.928566	44.262352	70.650023
847.335861	46.162364	70.655028
846.996374	54.233842	70.660033
846.761218	48.244034	70.665038
845.412442	59.128651	70.670042
844.732494	51.702031	70.675047
844.079592	56.685182	70.680052
843.723495	46.485135	70.685057
842.951025	58.832939	70.690062
842.077967	58.481476	70.695066
841.435878	47.100048	70.700071
841.034517	50.246970	70.705076
840.535389	41.380171	70.710081
839.472009	48.852486	70.715086
838.575895	53.672492	70.720090
838.291165	44.605984	70.725095
837.996703	52.769645	70.730100
837.471032	52.481167	70.735105
836.397689	55.220946	70.740110
835.487592	57.671385	70.745114
835.554183	50.111755	70.750119
834.386913	58.635118	70.755124
833.777331	59.503315	70.760129
833.181140	59.949900	70.765134
832.184660	54.279970	70.770138
831.497557	46.621102	70.775143
830.721078	58.939584	70.780148
830.343301	55.571358	70.785153
829.902918	58.305015	70.790158
829.287147	61.132821	70.795162
828.227935	58.074912	70.800167
827.523706	62.118465	70.805172
827.465456	45.094684	70.810177
826.530842	57.469875	70.815182
825.638100	58.547151	70.820186
825.331399	53.019752	70.825191
824.489481	57.167224	70.830196
823.619525	54.151736	70.835201
822.538279	59.718747	70.840206
821.880384	59.391392	70.845210
821.617641	53.060617	70.850215
821.039079	57.905780	70.855220
820.830378	54.723539	70.860225
820.067161	51.381973	70.865230
818.939941	52.173289	70.870234
818.643611	51.435139	70.875239
817.777342	62.749183	70.880244
817.166228	53.636851	70.885249
815.996726	49.637694	70.890254
815.373398	57.803241	70.895258
815.379649	54.768140	70.900263
814.398739	57.974198	70.905268
814.658861	46.994812	70.910273
813.427315	59.459850	70.915278
812.609763	52.862564	70.920282
812.092129	49.849349	70.925287
810.789280	58.056825	70.930292
810.327975	55.348465	70.935297
809.946862	58.359702	70.940302
809.700814	57.178300	70.945306
808.627213	53.807293	70.950311
807.523187	54.347335	70.955316
806.910373	60.292386	70.960321
806.597230	49.694414	70.965326
806.141384	54.250381	70.970330
805.429714	50.500060	70.975335
804.664561	54.562776	70.980340
804.408707	45.912735	70.985345
803.564049	53.782344	70.990350
802.179949	45.592597	70.995354
801.744759	44.936479	71.000359
801.319500	55.920119	71.005364
800.908034	44.144022	71.010369
799.902015	47.694709	71.015374
798.936147	53.716458	71.020378
798.146515	49.002392	71.025383
798.097791	52.317120	71.030388
797.832333	50.790295	71.035393
796.956414	52.719631	71.040398
795.850972	55.546539	71.045402
795.317955	49.254061	71.050407
794.678671	49.466235	71.055412
794.220404	39.134232	71.060417
793.245369	56.000820	71.065422
792.631802	56.975319	71.070426
792.215736	43.522040	71.075431
791.744987	47.149955	71.080436
790.663063	44.810057	71.085441
789.809073	53.914361	71.090446
789.323902	53.345050	71.095450
789.088189	47.729087	71.100455
788.349598	45.189455	71.105460
787.319837	53.824988	71.110465
786.654609	52.450111	71.115470
786.157153	57.481071	71.120474
785.426515	52.221441	71.125479
784.868187	55.798644	71.130484
784.448487	48.508821	71.135489
783.994263	46.373365	71.140494
782.691966	47.315571	71.145498
782.037378	59.015403	71.150503
781.305999	57.392431	71.155508
780.956438	49.325026	71.160513
780.026423	50.237935	71.165518
779.168249	52.129758	71.170522
778.929951	49.835348	71.175527
778.138257	55.244315	71.180532
777.830011	55.939973	71.185537
776.859880	56.864001	71.190542
775.972155	55.164992	71.195546
775.642420	49.961399	71.200551
774.964888	60.488451	71.205556
774.246265	54.487303	71.210561
773.439760	60.042137	71.215566
772.663352	69.635587	71.220570
772.556863	48.189725	71.225575
771.679098	52.535310	71.230580
770.722882	46.089430	71.235585
770.333364	53.933904	71.240590
769.997401	51.983056	71.245594
769.307895	49.053984	71.250599
767.755269	57.872111	71.255604
767.631629	48.150752	71.260609
766.868929	51.913460	71.265614
766.374765	50.822024	71.270618
765.651202	46.168418	71.275623
764.427061	63.576159	71.280628
764.296817	52.077004	71.285633
763.607359	54.080749	71.290638
763.296635	44.313481	71.295642
762.804429	36.552653	71.300647
761.469781	47.729943	71.305652
761.098234	43.272619	71.310657
760.272634	49.958039	71.315662
759.359029	41.105206	71.320666
758.839890	45.016802	71.325671
758.346956	42.726662	71.330676
758.155710	44.879758	71.335681
757.198002	43.316481	71.340686
756.457786	45.356692	71.345690
755.927128	36.341974	71.350695
754.961518	44.913681	71.355700
754.720214	36.691856	71.360705
753.334499	41.615059	71.365710
752.780493	43.179339	71.370714
752.459590	39.567107	71.375719
752.145666	42.129249	71.380724
751.462310	41.802813	71.385729
750.490354	53.212538	71.390734
749.719131	49.561604	71.395738
749.069831	43.555742	71.400743
747.889276	47.869110	71.405748
747.230558	38.778583	71.410753
746.798251	43.319768	71.415758
746.627644	40.278134	71.420762
746.531339	40.654620	71.425767
745.480249	40.514464	71.430772
744.777662	37.740453	71.435777
744.168039	48.568933	71.440782
743.178748	44.763481	71.445786
742.905335	48.005165	71.450791
741.824986	46.336836	71.455796
741.536883	43.928932	71.460801
740.485703	43.981186	71.465806
739.433953	46.151425	71.470810
739.076956	45.170626	71.475815
738.142659	48.653146	71.480820
738.469753	35.234546	71.485825
737.402229	38.377144	71.490830
736.461956	43.488066	71.495834
736.167230	39.966288	71.500839
734.953134	41.304494	71.505844
734.202568	43.699604	71.510849
733.504177	46.439654	71.515854
733.046116	39.826175	71.520858
732.781431	34.216416	71.525863
732.256669	49.278215	71.530868
731.739288	43.237163	71.535873
730.430957	50.341650	71.540878
729.937871	52.776198	71.545882
729.760826	47.116210	71.550887
728.482869	58.467428	71.555892
727.835754	56.745900	71.560897
727.298017	53.661787	71.565902
726.621749	50.842587	71.570906
726.426926	45.456673	71.575911
724.992209	54.349090	71.580916
724.994627	47.815265	71.585921
724.334926	49.681815	71.590926
722.958830	54.133562	71.595930
722.408628	48.257012	71.600935
721.620464	43.842371	71.605940
721.350165	41.190357	71.610945
721.101710	50.095764	71.615950
720.374994	49.337837	71.620954
719.506172	43.113039	71.625959
718.849935	47.833386	71.630964
718.618324	46.108790	71.635969
717.208445	49.116665	71.640974
716.399230	51.834940	71.645978
716.281536	42.480086	71.650983
715.478763	44.128137	71.655988
715.099899	43.504068	71.660993
713.917338	54.393812	71.665998
712.995871	47.996042	71.671002
712.734201	42.838399	71.676007
712.294571	44.373439	71.681012
711.683108	42.701436	71.686017
710.998310	53.543470	71.691022
710.259143	45.684773	71.696026
709.923872	36.705194	71.701031
708.438711	51.588737	71.706036
707.946868	46.057723	71.711041
707.372626	50.651476	71.716046
706.694170	47.575581	71.721050
706.959490	44.548125	71.726055
705.085540	48.278036	71.731060
704.737951	38.138177	71.736065
704.241894	43.971608	71.741070
703.474280	50.745584	71.746074
703.370775	44.712762	71.751079
702.145672	55.101494	71.756084
702.246808	43.478784	71.761089
700.951485	43.697661	71.766094
699.507412	52.279335	71.771098
699.026538	41.958842	71.776103
698.685765	53.758529	71.781108
698.621658	46.326954	71.786113
698.372535	47.623502	71.791118
697.313927	55.085647	71.796122
696.665218	45.458941	71.801127
695.439154	52.430495	71.806132
694.417526	50.402746	71.811137
693.865455	54.972472	71.816142
693.316653	52.112485	71.821146
693.510944	48.773053	71.826151
692.887143	57.859656	71.831156
692.150183	54.245864	71.836161
691.058242	51.518090	71.841166
689.952505	47.385840	71.846170
689.464489	50.417265	71.851175
688.355981	56.703041	71.856180
687.996189	50.856108	71.861185
687.546841	51.733519	71.866190
687.121337	51.826525	71.871194
686.855222	47.898065	71.876199
685.998957	57.688748	71.881204
685.220757	51.512611	71.886209
684.578899	52.672993	71.891214
683.930319	53.481201	71.896218
682.707385	48.441923	71.901223
682.026358	56.884765	71.906228
681.916348	53.294156	71.911233
681.166188	48.067636	71.916238
680.601162	45.684910	71.921242
679.729941	45.334789	71.926247
678.641721	52.618723	71.931252
678.320474	49.788741	71.936257
678.168729	51.777854	71.941262
677.309166	56.726135	71.946266
676.408461	49.000405	71.951271
675.653340	51.956089	71.956276
675.690844	51.781404	71.961281
674.415683	55.307182	71.966286
673.695322	50.870721	71.971290
673.533738	44.214778	71.976295
672.609740	43.300617	71.981300
671.813621	41.449865	71.986305
671.153518	49.269617	71.991310
670.477824	41.657880	71.996314
670.239933	40.891520	72.001319
668.481528	55.052177	72.006324
668.192403	40.785502	72.011329
667.402840	50.117699	72.016334
666.857753	49.848119	72.021338
667.199709	55.199607	72.026343
666.574013	51.836196	72.031348
665.398801	48.495629	72.036353
664.545581	40.234058	72.041358
663.991826	46.295883	72.046362
663.534219	41.205718	72.051367
662.307188	54.425463	72.056372
661.627815	49.976171	72.061377
661.390419	49.102498	72.066382
660.758012	42.308635	72.071386
659.875885	45.653561	72.076391
659.090844	56.265557	72.081396
658.433278	46.074137	72.086401
657.984201	42.345131	72.091406
657.308500	54.060953	72.096410
656.594600	38.731221	72.101415
655.727865	51.649161	72.106420
655.269804	46.669458	72.111425
655.015372	44.349247	72.116430
654.299172	45.540398	72.121434
653.473969	37.706466	72.126439
652.524190	53.741141	72.131444
652.314336	47.114964	72.136449
651.410291	39.738297	72.141454
650.726431	50.225366	72.146458
650.427932	45.881014	72.151463
649.364254	49.180734	72.156468
648.591539	49.264379	72.161473
647.911010	51.626284	72.166478
647.233839	57.584765	72.171482
647.039889	46.707651	72.176487
646.152256	48.610516	72.181492
645.287683	51.531596	72.186497
644.679673	45.077636	72.191502
644.145367	47.203363	72.196506
643.662482	39.603512	72.201511
642.587305	44.909415	72.206516
641.652154	35.173805	72.211521
641.179029	46.892059	72.216526
641.136877	47.766138	72.221530
640.971110	46.267613	72.226535
639.592932	47.069008	72.231540
639.252387	48.823253	72.236545
638.022936	44.340138	72.241550
636.884508	42.657451	72.246554
636.473355	40.458396	72.251559
635.463148	47.196899	72.256564
635.684124	43.593014	72.261569
635.139113	40.916947	72.266574
634.320092	41.864274	72.271578
634.072069	39.189802	72.276583
633.117658	32.691663	72.281588
632.561415	38.373833	72.286593
631.169830	37.922087	72.291598
630.318623	36.848113	72.296602
630.182197	32.440112	72.301607
629.630093	45.503494	72.306612
629.742809	37.334128	72.311617
628.465133	41.592047	72.316622
627.367681	45.497986	72.321626
627.023650	34.606938	72.326631
625.971003	40.678826	72.331636
625.101583	38.120658	72.336641
624.804122	41.583803	72.341646
623.980229	36.990381	72.346650
624.011092	36.941335	72.351655
623.566515	40.820578	72.356660
622.500370	35.775292	72.361665
622.168005	33.875938	72.366670
620.736607	48.664220	72.371674
620.051502	33.998567	72.376679
619.298690	40.737084	72.381684
618.929241	36.162760	72.386689
618.963917	28.475769	72.391694
617.881857	40.781434	72.396698
617.126172	34.540243	72.401703
616.338789	37.909516	72.406708
615.724016	37.558003	72.411713
615.097378	44.031996	72.416718
613.916406	40.788571	72.421722
613.523003	33.488302	72.426727
613.066255	38.506489	72.431732
612.739583	31.115168	72.436737
611.933863	34.419552	72.441742
610.805142	35.086617	72.446746
610.243787	33.775676	72.451751
610.041972	36.758379	72.456756
609.456764	31.932984	72.461761
608.451091	29.002276	72.466766
607.712583	38.952411	72.471770
607.302227	31.339447	72.476775
606.375286	39.272665	72.481780
605.548690	34.603986	72.486785
604.933603	35.421071	72.491790
604.341183	40.935540	72.496794
604.272552	31.754249	72.501799
602.864929	52.936583	72.506804
602.338902	34.706846	72.511809
601.728757	40.451223	72.516814
601.247861	42.458063	72.521818
600.881971	37.522046	72.526823
599.975843	49.306108	72.531828
599.341323	43.045624	72.536833
598.815222	50.355183	72.541838
597.611003	46.606101	72.546842
596.951625	40.226572	72.551847
596.146007	44.754687	72.556852
595.831528	47.452554	72.561857
595.448884	44.378470	72.566862
594.817462	43.368857	72.571866
594.004390	42.479638	72.576871
593.314308	45.472294	72.581876
592.712628	40.928651	72.586881
591.697114	44.417845	72.591886
590.910107	50.535756	72.596890
590.563420	38.232158	72.601895
589.998557	44.220067	72.606900
589.740544	49.369040	72.611905
588.693681	44.006878	72.616910
587.741876	40.234949	72.621914
587.560581	46.251660	72.626919
586.830806	55.530200	72.631924
585.696461	45.823180	72.636929
584.743449	49.486932	72.641934
584.412725	48.336388	72.646938
584.498840	40.147605	72.651943
583.877943	48.669195	72.656948
582.714967	39.009319	72.661953
582.190706	44.866183	72.666958
581.356093	49.466732	72.671962
580.646766	43.919925	72.676967
579.650791	39.625168	72.681972
579.146063	41.922819	72.686977
578.588002	43.870989	72.691982
578.330783	49.707401	72.696986
578.063335	41.923442	72.701991
576.771745	48.159565	72.706996
575.815917	44.413513	72.712001
575.778097	43.090162	72.717006
574.458234	50.688575	72.722010
573.891217	43.313457	72.727015
573.028176	52.652648	72.732020
572.964142	34.672623	72.737025
572.557889	40.206333	72.742030
571.412089	38.742475	72.747034
571.064712	31.896943	72.752039
570.015211	44.377216	72.757044
569.638818	43.092019	72.762049
568.524506	34.222359	72.767054
567.654276	47.689661	72.772058
567.368291	38.287517	72.777063
566.951595	47.899399	72.782068
566.435883	35.936550	72.787073
565.472252	43.500304	72.792078
564.793730	49.017457	72.797082
564.439120	33.952253	72.802087
563.740700	44.227181	72.807092
562.673855	42.184614	72.812097
561.952519	41.969938	72.817102
561.607005	43.490012	72.822106
561.249165	35.190589	72.827111
560.191083	42.201673	72.832116
559.905753	42.362263	72.837121
559.144207	44.245073	72.842126
558.153145	49.468225	72.847130
557.449221	46.446896	72.852135
556.195078	53.227434	72.857140
556.057257	54.763316	72.862145
555.993166	48.033512	72.867150
555.328059	54.355949	72.872154
554.323648	41.439589	72.877159
553.497372	52.865587	72.882164
553.136801	46.258701	72.887169
552.201730	44.141532	72.892174
551.397247	51.060190	72.897178
550.484522	41.117617	72.902183
550.396676	52.422847	72.907188
549.939021	43.024392	72.912193
549.643430	46.996613	72.917198
548.277085	52.927684	72.922202
547.656380	45.299345	72.927207
547.051815	50.385244	72.932212
546.100390	44.616808	72.937217
545.387255	46.974469	72.942222
544.215981	49.763079	72.947226
544.596596	38.193645	72.952231
543.964647	44.531299	72.957236
543.521926	42.269480	72.962241
542.565000	44.252802	72.967246
541.770534	47.228981	72.972250
541.498864	31.086112	72.977255
540.042994	48.909288	72.982260
539.436747	37.392962	72.987265
539.101896	33.371396	72.992270
538.467763	40.578315	72.997274
538.216974	41.118190	73.002279
536.801643	41.545505	73.007284
536.142611	44.377108	73.012289
535.637119	38.783659	73.017294
535.142689	44.922789	73.022298
535.141992	36.919729	73.027303
533.782248	46.692863	73.032308
532.957005	41.875758	73.037313
532.818740	41.640757	73.042318
531.399951	48.630460	73.047322
530.852828	36.775130	73.052327
530.234181	42.251211	73.057332
529.640991	41.366415	73.062337
529.296483	35.909755	73.067342
528.787620	44.752558	73.072346
527.836092	36.853643	73.077351
527.049161	53.934753	73.082356
526.416544	40.347317	73.087361
526.042101	37.527413	73.092366
525.022498	47.336259	73.097370
524.377256	38.648952	73.102375
524.021463	43.498104	73.107380
523.401368	33.255043	73.112385
522.958582	46.056589	73.117390
521.965914	54.105966	73.122394
521.304551	40.758082	73.127399
520.706179	44.067314	73.132404
520.314235	46.731795	73.137409
519.098732	46.258372	73.142414
518.416200	49.524240	73.147418
518.202899	41.004677	73.152423
517.173069	50.296329	73.157428
516.502051	49.136922	73.162433
515.699829	50.467972	73.167438
515.406832	46.283618	73.172442
515.032675	44.933419	73.177447
513.999354	47.783647	73.182452
513.293171	45.432911	73.187457
513.089044	37.888043	73.192462
511.789290	48.126304	73.197466
511.088179	39.346974	73.202471
510.309337	45.551912	73.207476
510.387388	40.226644	73.212481
509.956137	39.946851	73.217486
508.656922	40.125446	73.222490
508.142007	42.771669	73.227495
507.569046	49.153553	73.232500
506.621430	44.840084	73.237505
505.998930	42.695221	73.242510
505.207135	48.753989	73.247514
504.897609	41.784163	73.252519
504.183199	43.919683	73.257524
503.406730	45.350716	73.262529
502.775218	45.736771	73.267534
501.975161	51.959287	73.272538
501.772706	39.429306	73.277543
500.708986	43.288920	73.282548
499.874935	51.499119	73.287553
499.265126	42.555434	73.292558
498.562941	43.550426	73.297562
498.534527	40.393124	73.302567
497.612385	50.208533	73.307572
496.808245	42.847558	73.312577
496.341207	46.702011	73.317582
495.719772	48.587753	73.322586
494.689403	42.850840	73.327591
493.631096	46.020453	73.332596
493.334848	45.596151	73.337601
493.194444	45.566501	73.342606
492.250024	50.802746	73.347610
491.685046	41.473446	73.352615
490.997780	47.783653	73.357620
490.513326	41.526107	73.362625
489.343642	42.612921	73.367630
488.638035	48.249525	73.372634
488.266968	43.566670	73.377639
487.484571	36.161237	73.382644
487.315931	42.393555	73.387649
486.013389	38.649158	73.392654
485.240612	45.166956	73.397658
485.140048	38.031380	73.402663
484.432738	39.471901	73.407668
483.310209	36.673405	73.412673
482.465394	42.778470	73.417678
481.591646	39.484594	73.422682
481.930416	34.102025	73.427687
481.142489	40.082908	73.432692
480.619410	39.156992	73.437697
479.609564	35.928954	73.442702
479.029901	48.930508	73.447706
478.518268	44.295280	73.452711
478.008358	42.004753	73.457716
476.690379	40.115775	73.462721
476.192948	44.930724	73.467726
475.832290	44.956664	73.472730
475.485842	35.836993	73.477735
474.112501	36.147265	73.482740
473.912811	37.446996	73.487745
473.098705	37.351205	73.492750
472.081249	38.926295	73.497754
471.646470	39.842424	73.502759
470.658532	35.712019	73.507764
470.390871	40.335819	73.512769
470.190443	41.523702	73.517774
469.322568	43.688411	73.522778
468.712416	40.425087	73.527783
467.820698	45.302852	73.532788
467.652300	37.585140	73.537793
466.598691	41.999830	73.542798
465.661098	44.595124	73.547802
465.136136	38.564818	73.552807
464.039388	45.228852	73.557812
463.270574	43.452670	73.562817
462.816998	45.652305	73.567822
462.154498	46.845992	73.572826
461.973993	40.150517	73.577831
461.806841	48.508373	73.582836
461.057651	45.492710	73.587841
460.094892	40.468879	73.592846
459.064059	45.745708	73.597850
457.998275	35.898532	73.602855
457.251584	49.555914	73.607860
457.086766	44.480655	73.612865
457.139876	42.855810	73.617870
456.260466	44.672270	73.622874
455.451081	34.486198	73.627879
454.352920	48.360427	73.632884
453.776345	45.080718	73.637889
453.375809	44.338716	73.642894
452.116230	47.789574	73.647898
451.538347	44.030672	73.652903
450.860545	40.018025	73.657908
450.606878	32.782267	73.662913
450.390951	40.785184	73.667918
449.300551	41.104010	73.672922
448.760431	33.377715	73.677927
448.233839	42.914067	73.682932
447.268078	47.527663	73.687937
446.356302	40.297401	73.692942
445.504506	49.275277	73.697946
445.866023	39.623340	73.702951
444.992635	36.756784	73.707956
443.903300	41.098325	73.712961
443.054020	40.717983	73.717966
442.412994	47.274727	73.722970
442.142601	31.363500	73.727975
441.385381	45.009942	73.732980
440.466303	40.855963	73.737985
439.970406	41.687215	73.742990
439.491723	49.243134	73.747994
439.190654	39.589526	73.752999
437.784222	38.599350	73.758004
437.509445	34.296990	73.763009
437.155088	31.738836	73.768014
435.579039	42.689784	73.773018
435.099344	40.041209	73.778023
434.398957	48.711107	73.783028
434.102973	36.322204	73.788033
433.518159	36.372825	73.793038
432.946099	41.239094	73.798042
432.060482	33.509502	73.803047
431.126129	35.885090	73.808052
430.865594	43.444098	73.813057
430.438609	40.793434	73.818062
429.163587	47.539504	73.823066
428.594404	38.791226	73.828071
428.081014	47.007123	73.833076
427.523745	38.780506	73.838081
427.128371	36.522207	73.843086
426.128916	46.614883	73.848090
425.495648	34.110985	73.853095
424.992468	38.631960	73.858100
424.147705	38.392834	73.863105
423.393430	42.774041	73.868110
422.671268	45.540034	73.873114
422.277711	36.836319	73.878119
421.870756	48.435232	73.883124
420.727253	43.537988	73.888129
420.266574	41.860962	73.893134
419.445115	50.293106	73.898138
418.982365	36.908892	73.903143
417.806662	36.900696	73.908148
417.022008	41.570601	73.913153
416.261946	44.260631	73.918158
416.097681	48.945235	73.923162
416.066297	47.840064	73.928167
415.704490	44.278560	73.933172
414.447808	39.533397	73.938177
414.164802	40.963104	73.943182
412.734124	48.634438	73.948186
412.515267	43.219282	73.953191
411.718472	47.148366	73.958196
411.094947	49.067577	73.963201
409.800394	36.792052	73.968206
408.576951	43.645030	73.973210
408.234735	42.606733	73.978215
408.126582	42.109893	73.983220
407.615364	55.193595	73.988225
407.869262	43.237483	73.993230
406.908618	41.764702	73.998234
406.183263	38.980231	74.003239
405.156672	55.766801	74.008244
404.057845	40.936918	74.013249
403.380766	50.418409	74.018254
402.482107	51.602431	74.023258
402.218955	43.406228	74.028263
402.026111	45.628984	74.033268
401.321771	43.836242	74.038273
400.473799	44.968032	74.043278
399.700881	48.093786	74.048282
399.731862	42.220923	74.053287
398.196663	44.520370	74.058292
397.420328	37.993962	74.063297
397.103835	42.571931	74.068302
396.525837	46.146029	74.073306
396.128244	43.055441	74.078311
395.107288	60.080822	74.083316
394.301510	46.218245	74.088321
394.259956	42.588370	74.093326
392.886688	41.547203	74.098330
392.164130	43.299267	74.103335
391.490502	48.259002	74.108340
391.156182	37.796982	74.113345
391.002301	47.209299	74.118350
389.949968	48.725323	74.123354
389.115335	39.032165	74.128359
388.401189	38.587731	74.133364
387.803161	44.106287	74.138369
386.929033	45.398371	74.143374
385.723352	38.640754	74.148378
385.745605	42.275328	74.153383
385.147608	45.907810	74.158388
384.820480	49.320509	74.163393
384.352651	44.430739	74.168398
383.244159	56.873166	74.173402
382.658815	48.775613	74.178407
382.209289	51.430364	74.183412
380.946888	46.536316	74.188417
380.448124	43.376695	74.193422
379.868785	48.469644	74.198426
379.636791	41.388140	74.203431
378.637851	48.747840	74.208436
377.925578	46.166300	74.213441
377.502301	46.191194	74.218446
376.277591	50.450255	74.223450
375.898348	46.248128	74.228455
375.131862	46.024931	74.233460
374.482220	45.699535	74.238465
374.405139	44.562222	74.243470
373.312172	50.924486	74.248474
372.708378	38.677688	74.253479
371.946414	54.520064	74.258484
371.252017	44.702059	74.263489
370.703093	47.692778	74.268494
369.645191	50.458668	74.273498
369.196370	40.975279	74.278503
368.871157	42.779152	74.283508
368.164310	51.849070	74.288513
367.477111	43.526478	74.293518
366.403298	52.498752	74.298522
366.129304	47.847761	74.303527
365.537744	47.424801	74.308532
365.027993	44.295320	74.313537
364.153381	40.974818	74.318542
363.079652	48.622414	74.323546
363.145741	42.742381	74.328551
361.955569	46.207453	74.333556
361.040287	38.969904	74.338561
360.534486	44.107908	74.343566
359.849542	52.221841	74.348570
359.591347	41.591574	74.353575
359.222087	48.313188	74.358580
358.213875	42.112332	74.363585
357.504947	40.809198	74.368590
357.066029	49.164627	74.373594
356.278344	37.923291	74.378599
355.028986	39.609500	74.383604
354.536324	44.668140	74.388609
354.640008	36.870817	74.393614
353.310435	45.688303	74.398618
352.820911	36.723927	74.403623
351.609381	48.563022	74.408628
351.150536	43.223966	74.413633
351.209077	40.730917	74.418638
350.098387	48.248786	74.423642
349.524404	41.710649	74.428647
348.638956	43.206403	74.433652
348.068795	42.019933	74.438657
348.118388	48.135473	74.443662
346.572049	44.687052	74.448666
346.135616	48.093519	74.453671
345.536853	54.384924	74.458676
345.044303	37.059875	74.463681
344.999911	43.319702	74.468686
343.514477	45.366820	74.473690
343.061558	40.367450	74.478695
341.874522	43.675910	74.483700
340.888981	43.520749	74.488705
340.404809	46.305609	74.493710
339.752646	51.287167	74.498714
339.513491	47.739247	74.503719
338.991242	50.706797	74.508724
338.750698	43.079449	74.513729
338.482268	38.741398	74.518734
337.264141	40.977736	74.523738
336.756223	36.468114	74.528743
335.240862	40.084369	74.533748
334.684523	45.252509	74.538753
334.285155	50.690531	74.543758
333.806568	49.995681	74.548762
333.540173	39.497618	74.553767
332.379147	43.719739	74.558772
331.816181	48.433190	74.563777
331.504258	48.170681	74.568782
329.866121	46.186147	74.573786
329.426359	48.533415	74.578791
328.761675	44.118163	74.583796
328.639160	48.162168	74.588801
328.251471	50.154202	74.593806
326.946951	54.178419	74.598810
326.170709	49.364621	74.603815
325.686569	54.035550	74.608820
325.375050	45.760335	74.613825
324.321995	44.188772	74.618830
323.109216	47.170178	74.623834
322.909672	40.542413	74.628839
322.489715	46.926750	74.633844
322.278923	45.593126	74.638849
321.713920	50.362097	74.643854
320.439405	51.686474	74.648858
320.016672	43.736497	74.653863
319.188812	51.644552	74.658868
318.009900	44.811740	74.663873
317.836474	40.053267	74.668878
317.150146	48.112232	74.673882
316.481236	37.824982	74.678887
315.555802	46.432994	74.683892
314.807853	35.332006	74.688897
314.653091	40.021401	74.693902
314.241648	45.292611	74.698906
313.367310	46.379746	74.703911
312.093074	46.163372	74.708916
311.830691	47.583494	74.713921
311.549614	42.701827	74.718926
310.583757	48.917698	74.723930
309.970078	49.602163	74.728935
309.369513	45.260278	74.733940
308.888222	37.664998	74.738945
307.910186	42.577069	74.743950
306.793197	46.566675	74.748954
306.461959	37.939791	74.753959
305.858078	43.591760	74.758964
305.386625	47.697685	74.763969
304.747913	37.498669	74.768974
304.232040	40.900455	74.773978
303.668102	37.986210	74.778983
302.596737	43.387828	74.783988
301.838852	44.360212	74.788993
300.818453	38.719577	74.793998
300.467449	36.567772	74.799002
300.053635	43.641849	74.804007
299.298850	39.937992	74.809012
298.769774	41.115187	74.814017
297.989926	42.009069	74.819022
297.205683	47.095265	74.824026
296.843622	39.452600	74.829031
295.822858	44.316291	74.834036
295.055330	39.551582	74.839041
294.697099	48.371981	74.844046
294.004607	52.962578	74.849050
293.928764	48.781497	74.854055
292.565568	53.176211	74.859060
291.617808	47.631236	74.864065
291.411049	42.732996	74.869070
291.218377	46.785028	74.874074
290.335049	41.933120	74.879079
289.603165	45.035016	74.884084
288.904890	41.115572	74.889089
287.940899	46.602587	74.894094
287.136411	51.539047	74.899098
286.691303	46.737144	74.904103
286.310616	44.484413	74.909108
285.885319	44.908620	74.914113
285.317908	35.625513	74.919118
284.243316	49.844548	74.924122
283.403695	36.950963	74.929127
282.062979	42.682529	74.934132
281.696814	41.936655	74.939137
281.208303	39.868272	74.944142
280.784520	44.822901	74.949146
280.652663	42.066880	74.954151
279.980171	42.426407	74.959156
279.275628	36.333311	74.964161
278.352313	40.255788	74.969166
277.655248	51.282772	74.974170
276.551492	41.779217	74.979175
275.909080	35.539022	74.984180
275.098790	42.573790	74.989185
275.269918	45.009781	74.994190
274.541913	47.920250	74.999194
273.600740	44.332843	75.004199
273.052521	43.139740	75.009204
272.495010	43.665449	75.014209
271.444581	39.970877	75.019214
270.322489	44.109547	75.024218
270.069946	38.160456	75.029223
269.646634	42.454257	75.034228
269.265407	49.127322	75.039233
268.427560	46.050160	75.044238
267.541798	46.965664	75.049242
267.145478	41.280767	75.054247
266.329055	44.706809	75.059252
265.444019	43.923791	75.064257
264.885282	37.082049	75.069262
263.974863	47.575327	75.074266
263.544288	44.977309	75.079271
263.322251	46.603897	75.084276
262.534202	39.213646	75.089281
261.411812	41.442645	75.094286
260.847850	53.669000	75.099290
260.613594	38.583126	75.104295
259.956391	37.560364	75.109300
258.402203	45.669360	75.114305
258.385289	38.768064	75.119310
257.513741	42.969308	75.124314
257.489846	40.464167	75.129319
256.371900	52.092837	75.134324
255.794655	36.883438	75.139329
255.218439	38.661100	75.144334
254.424920	48.284179	75.149338
253.720677	40.084197	75.154343
252.790005	41.200833	75.159348
251.927485	34.251398	75.164353
251.871371	34.826502	75.169358
251.491999	36.910261	75.174362
250.589021	40.589805	75.179367
249.646377	37.628705	75.184372
249.058531	40.379641	75.189377
248.764639	44.605506	75.194382
247.587977	47.035554	75.199386
246.780894	41.430330	75.204391
246.482425	40.238424	75.209396
245.902392	36.733817	75.214401
245.825398	42.374352	75.219406
244.375612	49.523682	75.224410
243.894324	37.333102	75.229415
243.492456	47.576585	75.234420
242.063494	49.168475	75.239425
241.544326	39.379365	75.244430
240.721893	52.760269	75.249434
240.358771	45.720189	75.254439
240.148785	43.976430	75.259444
239.481023	46.743261	75.264449
238.638702	44.543624	75.269454
237.985266	47.863269	75.274458
237.600604	45.041891	75.279463
236.435618	52.174214	75.284468
235.560848	44.785179	75.289473
235.220210	43.868083	75.294478
234.629757	50.662815	75.299482
234.456369	36.742097	75.304487
233.373141	41.782926	75.309492
232.282620	48.617946	75.314497
232.018643	45.271121	75.319502
231.329826	49.099464	75.324506
230.880825	40.587563	75.329511
229.683359	47.581559	75.334516
229.015325	53.310006	75.339521
228.903925	46.207725	75.344526
228.081579	49.683610	75.349530
227.348984	40.773786	75.354535
226.737021	46.223629	75.359540
226.099068	49.036176	75.364545
225.393808	48.779611	75.369550
224.047596	56.286188	75.374554
223.767769	47.316802	75.379559
223.744523	46.309688	75.384564
223.073298	49.501284	75.389569
222.246211	37.351642	75.394574
221.139610	48.292527	75.399578
220.995025	39.574405	75.404583
220.106695	51.027709	75.409588
218.984193	52.102397	75.414593
218.473276	42.305668	75.419598
217.882769	42.494445	75.424602
217.929643	42.146369	75.429607
217.238964	39.018959	75.434612
215.978403	40.454706	75.439617
215.265197	30.073635	75.444622
214.662563	38.772141	75.449626
214.612515	43.156259	75.454631
213.510210	42.739061	75.459636
212.779431	54.060019	75.464641
212.202647	46.470524	75.469646
211.240399	42.104322	75.474650
210.516012	43.140779	75.479655
209.631455	43.419012	75.484660
209.360637	45.561167	75.489665
208.979412	39.509596	75.494670
208.443112	47.221383	75.499674
207.535586	44.631599	75.504679
206.393243	52.446311	75.509684
206.042206	51.333754	75.514689
206.102344	45.093547	75.519694
205.220252	50.330987	75.524698
204.414903	35.686262	75.529703
203.453961	47.341957	75.534708
203.125372	55.477961	75.539713
202.404927	41.340099	75.544718
201.266103	57.480702	75.549722
200.873260	44.971673	75.554727
200.398532	48.409497	75.559732
199.610293	44.953862	75.564737
198.928708	40.544500	75.569742
198.169942	49.286829	75.574746
198.179087	37.514828	75.579751
196.723549	42.408441	75.584756
195.989701	46.776989	75.589761
195.795924	47.763555	75.594766
195.354618	50.631493	75.599770
194.519086	48.446559	75.604775
193.465042	48.672968	75.609780
193.184494	52.631780	75.614785
192.440776	51.596020	75.619790
191.184380	50.159437	75.624794
190.667471	46.513890	75.629799
190.096592	52.979075	75.634804
189.527798	43.932762	75.639809
189.239620	49.580157	75.644814
188.638292	52.765349	75.649818
187.922060	48.424591	75.654823
186.920602	53.688953	75.659828
186.617819	54.290768	75.664833
186.001934	53.603644	75.669838
184.823133	59.479763	75.674842
184.332667	49.164109	75.679847
184.114476	50.100950	75.684852
183.223738	54.445630	75.689857
182.415098	45.604716	75.694862
181.538765	54.086669	75.699866
181.372320	53.226966	75.704871
180.405226	52.211052	75.709876
179.199004	51.523426	75.714881
178.831418	46.557799	75.719886
178.237216	55.076777	75.724890
178.207942	34.183352	75.729895
177.368480	48.614092	75.734900
176.441055	43.132161	75.739905
176.025394	39.361666	75.744910
175.224090	46.652075	75.749914
174.591032	38.705708	75.754919
173.471650	42.418202	75.759924
172.761592	43.670009	75.764929
172.816554	38.457243	75.769934
172.091813	44.664679	75.774938
170.940988	39.219945	75.779943
170.253417	38.541100	75.784948
169.480421	48.700252	75.789953
169.435617	41.458051	75.794958
168.670989	46.358224	75.799962
167.990302	32.794376	75.804967
167.134616	39.782789	75.809972
166.410170	41.883729	75.814977
166.299292	40.865356	75.819982
165.250156	45.724156	75.824986
164.588526	44.080797	75.829991
164.170109	43.305425	75.834996
163.450166	39.843646	75.840001
162.661750	40.070297	75.845006
161.721192	44.758820	75.850010
161.303380	41.844970	75.855015
160.850045	51.991009	75.860020
159.829336	44.726201	75.865025
159.232607	43.611823	75.870030
158.467816	42.669322	75.875034
158.117436	37.659957	75.880039
157.311967	37.832558	75.885044
156.384671	45.952048	75.890049
155.797806	41.032428	75.895054
155.336845	41.761969	75.900058
155.058892	34.495443	75.905063
153.888860	41.079810	75.910068
153.331972	41.402016	75.915073
152.831158	35.823694	75.920078
152.403687	46.351965	75.925082
151.324651	47.266786	75.930087
150.681234	47.776256	75.935092
150.265583	44.111421	75.940097
150.060082	34.549881	75.945102
148.350796	50.425048	75.950106
147.964030	45.002008	75.955111
147.303020	52.429334	75.960116
146.981926	56.205377	75.965121
146.076308	41.467850	75.970126
145.104522	50.412891	75.975130
144.393112	40.351683	75.980135
143.949882	45.153309	75.985140
143.654887	51.393161	75.990145
142.698410	49.520847	75.995150
141.505752	44.846054	76.000154
141.700629	36.362409	76.005159
141.276462	35.761425	76.010164
140.498256	46.653130	76.015169
139.650975	38.698353	76.020174
138.914056	51.273997	76.025178
138.180040	43.400509	76.030183
137.278210	41.539986	76.035188
136.172440	42.386534	76.040193
135.902794	42.355434	76.045198
135.317282	52.812714	76.050202
135.256614	41.217432	76.055207
134.668619	48.030710	76.060212
133.369365	45.650074	76.065217
133.023649	44.790574	76.070222
132.193150	46.060019	76.075226
131.608264	50.652419	76.080231
130.499614	44.817775	76.085236
130.108461	43.650125	76.090241
129.732259	32.180857	76.095246
129.413136	39.209885	76.100250
128.496061	34.601550	76.105255
127.643773	38.052275	76.110260
126.954586	40.153910	76.115265
126.542577	33.552172	76.120270
125.054309	41.037283	76.125274
124.695506	35.336976	76.130279
124.297720	38.070248	76.135284
123.791116	43.899131	76.140289
123.022048	42.331264	76.145294
122.300549	40.323720	76.150298
121.638629	35.733052	76.155303
121.048120	39.034803	76.160308
120.293337	34.370632	76.165313
119.770125	39.449944	76.170318
118.724110	50.005883	76.175322
118.647672	36.383552	76.180327
117.763753	42.160633	76.185332
117.074701	40.430196	76.190337
116.300442	41.846799	76.195342
115.555958	48.785960	76.200346
115.649881	42.548255	76.205351
114.502218	44.156865	76.210356
113.656566	43.861217	76.215361
113.075773	41.137370	76.220366
112.150127	45.979653	76.225370
111.094461	45.313787	76.230375
110.705851	50.258100	76.235380
110.170232	43.321251	76.240385
109.828151	39.513806	76.245390
109.260432	41.703312	76.250394
109.209286	47.806508	76.255399
108.013375	37.396789	76.260404
107.332205	43.557866	76.265409
106.691707	46.134299	76.270414
105.484531	50.357570	76.275418
105.009850	43.732709	76.280423
104.655160	50.406288	76.285428
103.964829	47.010770	76.290433
103.212584	43.585701	76.295438
102.551561	45.186105	76.300442
102.136868	42.765363	76.305447
101.160440	43.167095	76.310452
100.106159	43.002492	76.315457
99.603723	41.417347	76.320462
98.932101	49.226424	76.325466
98.576752	42.104713	76.330471
98.430180	43.394421	76.335476
97.326305	44.319534	76.340481
96.756544	38.570868	76.345486
96.028808	57.337847	76.350490
95.201754	38.916618	76.355495
94.207883	47.302213	76.360500
93.557583	48.774752	76.365505
93.595006	42.927686	76.370510
92.534996	39.185840	76.375514
91.656584	36.876894	76.380519
91.013668	43.230574	76.385524
90.281432	44.168967	76.390529
89.947116	36.080374	76.395534
89.570380	41.645698	76.400538
89.415692	40.430886	76.405543
88.349539	42.341905	76.410548
87.229534	45.608250	76.415553
86.503568	38.312251	76.420558
85.278433	42.856942	76.425562
84.993908	32.189941	76.430567
84.794377	38.430337	76.435572
84.440795	39.800367	76.440577
83.570894	35.786933	76.445582
82.839974	44.669924	76.450586
82.534776	39.407361	76.455591
81.168348	37.094239	76.460596
80.087064	42.276745	76.465601
79.789402	44.123567	76.470606
79.190136	46.154105	76.475610
78.972534	41.516249	76.480615
78.356604	51.517908	76.485620
77.078785	44.641078	76.490625
76.955523	35.339254	76.495630
75.826356	48.925220	76.500634
75.406750	42.961800	76.505639
74.408351	42.379859	76.510644
73.819797	46.734730	76.515649
73.662858	36.613517	76.520654
73.077143	39.140219	76.525658
72.341501	39.214978	76.530663
71.280280	42.498764	76.535668
70.803513	35.514698	76.540673
70.324985	42.313682	76.545678
69.690038	41.683245	76.550682
68.704255	38.098310	76.555687
67.925347	44.508375	76.560692
67.572094	40.508751	76.565697
67.048865	32.343057	76.570702
65.694504	45.315222	76.575706
65.354684	37.019351	76.580711
64.912207	39.835453	76.585716
64.075736	43.381449	76.590721
63.854147	34.946874	76.595726
62.713371	42.833926	76.600730
62.390223	32.742377	76.605735
61.954249	39.299605	76.610740
61.064983	38.925774	76.615745
59.944257	34.985467	76.620750
59.543198	49.138153	76.625754
59.432774	43.863455	76.630759
58.276953	36.336394	76.635764
57.202727	49.617133	76.640769
57.067093	41.809101	76.645774
56.121605	45.200594	76.650778
56.120956	40.242710	76.655783
54.859324	44.957241	76.660788
54.430989	44.913610	76.665793
53.470347	39.202062	76.670798
52.408947	44.215827	76.675802
51.865330	41.110747	76.680807
51.065327	42.600862	76.685812
50.800654	41.465096	76.690817
50.776120	43.072817	76.695822
49.960878	55.318766	76.700826
49.513989	46.380792	76.705831
48.669235	42.872724	76.710836
47.708322	47.507761	76.715841
46.763667	43.566186	76.720846
45.720741	40.417735	76.725850
45.679464	37.773446	76.730855
44.957278	48.542695	76.735860
44.551277	49.266645	76.740865
44.023361	47.105248	76.745870
43.147008	45.858873	76.750874
42.447377	40.988810	76.755879
42.107909	43.356397	76.760884
40.937470	50.800331	76.765889
40.006053	42.917361	76.770894
39.408195	38.144611	76.775898
39.245335	40.760002	76.780903
38.921151	44.667434	76.785908
37.528260	38.690512	76.790913
37.250772	43.435756	76.795918
36.561461	43.955728	76.800922
36.271055	38.656121	76.805927
35.144598	40.010646	76.810932
34.318067	42.350256	76.815937
34.015588	34.370141	76.820942
32.680464	38.441957	76.825946
31.849366	32.914768	76.830951
31.599283	43.052048	76.835956
30.580163	42.270001	76.840961
30.744087	50.830516	76.845966
30.237598	43.436452	76.850970
29.875570	41.775313	76.855975
28.838888	47.876412	76.860980
28.093784	45.375915	76.865985
27.080002	36.545713	76.870990
25.773327	48.214018	76.875994
25.322713	42.575682	76.880999
25.406174	48.397205	76.886004
24.959071	46.079419	76.891009
24.183292	35.788828	76.896014
22.986980	40.710578	76.901018
22.405824	37.896926	76.906023
22.294660	38.726822	76.911028
21.439494	46.317600	76.916033
20.656175	37.609919	76.921038
20.362319	48.697215	76.926042
19.557058	43.627960	76.931047
18.422164	44.403511	76.936052
17.354150	41.345808	76.941057
17.203485	35.396282	76.946062
16.521578	42.128360	76.951066
16.226271	38.151043	76.956071
15.390881	39.282532	76.961076
14.434168	46.550459	76.966081
14.156630	39.104117	76.971086
13.577202	38.665116	76.976090
12.667638	46.084797	76.981095
11.919844	40.391360	76.986100
11.051392	39.831299	76.991105
11.001435	40.484274	76.996110
9.746913	49.871848	77.001114
8.841391	47.504177	77.006119
8.465914	47.799058	77.011124
8.010613	49.350905	77.016129
7.767837	47.248118	77.021134
6.850282	40.922583	77.026139
6.231188	43.872522	77.031143
5.350928	42.751366	77.036148
5.021474	48.596168	77.041153
4.354714	46.045336	77.046158