Fri Mar 05 18:28:58 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.233179	91.133370	0.000000
-0.048270	86.866780	0.005005
-1.027839	47.519744	0.010010
-2.651216	11.702269	0.015014
-6.656816	-2.638438	0.020019
-11.866858	-13.547902	0.025024
-17.329126	-8.281580	0.030029
-21.789104	-5.630472	0.035034
-25.356238	-1.472276	0.040038
-29.224246	1.183762	0.045043
-32.692507	-3.586831	0.050048
-36.740778	-6.169099	0.055053
-40.421828	-7.606716	0.060058
-44.069997	-8.155432	0.065062
-47.966625	-4.472924	0.070067
-51.197815	-10.140756	0.075072
-55.168502	-4.899417	0.080077
-58.788531	-9.256246	0.085082
-62.899795	-2.734047	0.090086
-66.909957	-12.360349	0.095091
-70.022328	-6.276627	0.100096
-74.256733	-3.735529	0.105101
-77.615439	-12.475412	0.110106
-81.691383	-11.749442	0.115110
-85.686149	-5.635304	0.120115
-89.031951	-12.535331	0.125120
-93.053222	-7.839378	0.130125
-96.534992	-11.822388	0.135130
-100.067291	-10.594919	0.140134
-103.966556	-11.541877	0.145139
-107.503444	-19.086326	0.150144
-111.698929	-14.561245	0.155149
-115.661406	-14.111945	0.160154
-119.314168	-23.079231	0.165158
-123.303639	-14.660360	0.170163
-127.307893	-12.006084	0.175168
-130.855596	-0.994189	0.180173
-134.585020	-9.006201	0.185178
-138.231829	-11.422119	0.190182
-142.126391	-4.253122	0.195187
-145.218967	-11.959880	0.200192
-149.571405	1.766680	0.205197
-152.906192	-7.074683	0.210202
-156.758128	-5.938051	0.215206
-160.758672	-8.616034	0.220211
-164.377621	-11.506293	0.225216
-168.452584	0.365661	0.230221
-171.786448	-6.695426	0.235226
-175.526988	-1.056958	0.240230
-179.565491	-10.653308	0.245235
-183.022714	-12.686247	0.250240
-187.308430	-7.039607	0.255245
-191.216610	-7.860421	0.260250
-194.522697	-4.412279	0.265254
-198.036057	-0.856934	0.270259
-201.894246	-10.439443	0.275264
-205.560685	-7.416327	0.280269
-209.507190	-9.702303	0.285274
-213.164898	-7.276661	0.290278
-217.030650	-1.039401	0.295283
-220.708760	-12.951410	0.300288
-225.080480	-4.452442	0.305293
-228.865186	-5.972574	0.310298
-231.948985	-9.148418	0.315302
-236.000178	-6.770326	0.320307
-239.520897	-19.956375	0.325312
-243.618440	-11.024898	0.330317
-247.046344	-9.405445	0.335322
-250.736171	-12.151793	0.340326
-254.622062	-3.293501	0.345331
-258.125696	-3.453375	0.350336
-262.604941	-4.984018	0.355341
-266.125574	-9.843673	0.360346
-269.920943	-8.208110	0.365350
-273.567354	-10.533996	0.370355
-277.315669	-8.476997	0.375360
-280.877012	-8.914634	0.380365
-284.639867	-12.824109	0.385370
-288.540490	-8.451453	0.390374
-292.693795	-11.202598	0.395379
-295.848400	-15.614432	0.400384
-300.234736	-9.533641	0.405389
-303.728301	-12.049462	0.410394
-307.284409	-8.267941	0.415398
-311.014526	-11.420928	0.420403
-314.535342	-17.747053	0.425408
-318.846261	-9.330173	0.430413
-322.873249	-14.999887	0.435418
-326.355639	-20.007479	0.440422
-329.987305	-15.251918	0.445427
-333.538158	-18.365677	0.450432
-337.587376	-10.591369	0.455437
-341.260616	-12.506011	0.460442
-345.008622	-11.708951	0.465446
-348.868464	-9.845349	0.470451
-352.876571	-20.594264	0.475456
-356.222737	-14.294670	0.480461
-359.733921	-13.708864	0.485466
-363.553747	-16.468972	0.490470
-367.708345	-8.775561	0.495475
-371.473734	-14.945854	0.500480
-375.164187	-13.952932	0.505485
-378.881926	-12.050471	0.510490
-382.628950	-13.585835	0.515494
-386.403479	-6.492399	0.520499
-389.762651	-17.329097	0.525504
-394.016701	-16.350233	0.530509
-397.600957	-12.977252	0.535514
-401.560660	-8.740065	0.540518
-405.519971	-14.754757	0.545523
-409.026439	-19.327869	0.550528
-412.793027	-14.517527	0.555533
-416.331174	-13.835869	0.560538
-420.044916	-6.397273	0.565542
-423.911704	-2.983866	0.570547
-427.678009	-15.170028	0.575552
-431.835968	-9.166476	0.580557
-435.594333	-19.516729	0.585562
-438.886297	-23.324531	0.590566
-443.053847	-2.253151	0.595571
-446.488932	-15.124537	0.600576
-450.349801	-7.211390	0.605581
-453.937420	-19.780855	0.610586
-457.911061	-7.844211	0.615590
-461.351401	-13.392906	0.620595
-465.070574	-15.471907	0.625600
-469.523233	-6.104880	0.630605
-473.121372	-10.544985	0.635610
-476.750263	-12.488576	0.640614
-480.590946	-11.693849	0.645619
-484.018503	-13.590736	0.650624
-488.052890	-13.930434	0.655629
-491.716493	-13.039392	0.660634
-495.264417	-18.909897	0.665638
-499.301847	-11.657609	0.670643
-503.218184	-25.491246	0.675648
-507.090612	-4.916343	0.680653
-510.678041	-9.280830	0.685658
-514.155034	-11.264394	0.690662
-517.864987	-7.849082	0.695667
-521.414638	-10.032344	0.700672
-525.429857	-4.502443	0.705677
-528.975271	-12.795509	0.710682
-533.234180	-9.928003	0.715686
-537.149868	-10.922091	0.720691
-540.895300	-24.016560	0.725696
-544.627130	-9.648895	0.730701
-548.232961	-11.600790	0.735706
-552.264626	-11.846195	0.740710
-555.985810	-4.522904	0.745715
-559.370159	-18.543931	0.750720
-563.128057	-11.787203	0.755725
-567.094337	-13.378712	0.760730
-570.344224	-10.855257	0.765734
-574.239552	-12.771903	0.770739
-578.113834	-20.611802	0.775744
-582.339476	-15.380935	0.780749
-586.170056	-17.848801	0.785754
-589.449560	-22.535167	0.790758
-593.489134	-11.332107	0.795763
-596.768398	-12.421464	0.800768
-600.853439	-8.116621	0.805773
-604.527723	-19.423042	0.810778
-608.370573	-9.681686	0.815782
-612.389144	-14.685185	0.820787
-615.817731	-17.169919	0.825792
-619.908199	-17.244965	0.830797
-623.135326	-4.250925	0.835802
-627.059609	-7.795009	0.840806
-630.914981	-2.631098	0.845811
-634.630292	-6.960768	0.850816
-638.575761	-7.341225	0.855821
-642.279571	-5.443737	0.860826
-646.002511	-8.772377	0.865830
-649.766027	-5.693659	0.870835
-653.322412	-15.577500	0.875840
-657.060826	-18.302827	0.880845
-660.961945	-13.667728	0.885850
-665.125046	-18.143413	0.890854
-668.911676	-17.254519	0.895859
-672.316365	-14.428647	0.900864
-676.106260	-9.502211	0.905869
-679.273387	-12.918035	0.910874
-683.347162	-4.598347	0.915878
-687.492777	-5.035049	0.920883
-691.087738	-12.578771	0.925888
-695.196951	-5.221651	0.930893
-698.799376	-10.950668	0.935898
-702.626362	-14.913872	0.940902
-705.914316	-13.407595	0.945907
-709.649362	-14.042334	0.950912
-713.700978	-9.643296	0.955917
-717.512307	-14.585112	0.960922
-721.140102	-16.512729	0.965926
-725.146869	-10.829314	0.970931
-728.466221	-18.543175	0.975936
-732.472288	-9.898338	0.980941
-735.916637	-20.515885	0.985946
-740.068170	-19.264207	0.990950
-744.099223	-10.243198	0.995955
-747.725076	-17.671502	1.000960
-751.421599	-14.759452	1.005965
-754.859447	-16.069247	1.010970
-758.768978	-12.651632	1.015974
-763.106037	-6.350813	1.020979
-766.470459	-12.980357	1.025984
-769.951679	-20.321353	1.030989
-773.733870	-19.087648	1.035994
-777.638000	-15.637751	1.040998
-781.650227	-16.212301	1.046003
-784.998150	-23.814275	1.051008
-788.667576	-13.761324	1.056013
-792.689265	-19.099897	1.061018
-795.905692	-19.531967	1.066022
-800.323240	-14.451398	1.071027
-803.904686	-11.996055	1.076032
-807.858241	-11.971235	1.081037
-811.840712	-18.211753	1.086042
-815.271246	-7.339084	1.091046
-819.199156	-3.967318	1.096051
-822.738306	-8.422613	1.101056
-826.509779	-7.614737	1.106061
-830.142950	-9.043008	1.111066
-834.279749	-12.068641	1.116070
-838.031566	-9.891941	1.121075
-841.492098	-12.574662	1.126080
-845.175946	-8.891786	1.131085
-849.139885	-3.481518	1.136090
-852.769538	-6.826315	1.141094
-856.617754	-1.160144	1.146099
-860.629800	-5.658050	1.151104
-863.936864	-3.451487	1.156109
-867.686399	-10.782555	1.161114
-871.229681	-13.094033	1.166118
-875.554939	-3.051215	1.171123
-879.225222	-9.876118	1.176128
-883.285152	-5.696240	1.181133
-887.066878	-6.283809	1.186138
-890.421098	-10.014782	1.191142
-894.446019	-6.892310	1.196147
-897.936141	-10.232536	1.201152
-901.417068	-6.534710	1.206157
-905.204692	-5.957516	1.211162
-909.039028	-15.283991	1.216166
-913.431141	-1.250190	1.221171
-916.763016	-15.750550	1.226176
-920.744563	-7.285949	1.231181
-924.235957	-10.070844	1.236186
-928.019903	-10.377294	1.241190
-931.824630	-9.647512	1.246195
-935.314163	-11.123817	1.251200
-939.326295	-8.113702	1.256205
-943.199744	-12.972667	1.261210
-946.987415	-16.588511	1.266214
-950.449432	-10.151322	1.271219
-954.399603	-9.691558	1.276224
-958.137131	-9.190098	1.281229
-961.743339	-16.477694	1.286234
-965.711620	-18.664291	1.291238
-969.552447	-11.753337	1.296243
-972.996595	-11.882242	1.301248
-977.257968	-2.876059	1.306253
-980.857978	-10.172502	1.311258
-984.728309	-11.740799	1.316262
-988.207918	-5.270779	1.321267
-991.853246	-13.215967	1.326272
-995.920525	-9.673390	1.331277
-999.734990	-3.394226	1.336282
-1003.370358	-13.693799	1.341286
-1007.164535	-4.770170	1.346291
-1010.369075	-9.005875	1.351296
-1014.570345	-7.187520	1.356301
-1018.633460	0.926013	1.361306
-1022.250484	-9.431659	1.366310
-1026.145571	-2.199697	1.371315
-1029.344908	-14.825582	1.376320
-1033.350698	-2.301005	1.381325
-1037.144962	-0.473591	1.386330
-1040.939353	-1.953017	1.391334
-1044.906246	6.023746	1.396339
-1048.544480	-7.784014	1.401344
-1052.155457	-6.446363	1.406349
-1055.723232	-8.010897	1.411354
-1059.775267	-2.480537	1.416358
-1063.760979	3.081801	1.421363
-1067.183727	-6.072122	1.426368
-1071.225787	-0.426644	1.431373
-1074.455407	-9.504213	1.436378
-1078.241771	-12.911892	1.441382
-1082.521781	-2.193133	1.446387
-1086.247150	-7.132313	1.451392
-1090.048358	-3.422403	1.456397
-1093.731558	-5.868852	1.461402
-1097.201736	-15.335255	1.466406
-1100.653035	-4.337453	1.471411
-1104.716667	-10.886170	1.476416
-1108.965298	-7.237117	1.481421
-1112.887068	-4.513977	1.486426
-1116.270889	-8.284035	1.491430
-1120.107719	-9.176223	1.496435
-1123.563678	-19.534255	1.501440
-1127.514991	-11.727016	1.506445
-1131.052779	-15.191721	1.511450
-1134.586033	-19.264270	1.516454
-1138.731110	-7.158791	1.521459
-1142.255603	-14.402397	1.526464
-1146.128729	-9.250601	1.531469
-1150.292390	-3.880425	1.536474
-1153.629810	-7.985857	1.541478
-1157.441032	-4.411432	1.546483
-1161.267000	-8.886538	1.551488
-1165.091519	-12.939247	1.556493
-1168.918301	-13.388261	1.561498
-1172.549129	-11.061657	1.566502
-1176.343298	-12.911476	1.571507
-1179.837844	-24.838609	1.576512
-1183.940419	-17.459663	1.581517
-1187.620601	-16.711547	1.586522
-1191.678205	-18.422993	1.591526
-1195.336757	-10.999958	1.596531
-1198.743156	-18.804837	1.601536
-1202.565516	-15.868800	1.606541
-1206.388837	-7.638791	1.611546
-1209.976908	-13.485979	1.616550
-1214.033805	-9.080524	1.621555
-1217.788944	-26.647631	1.626560
-1221.713847	-16.561052	1.631565
-1225.183972	-15.944262	1.636570
-1228.850311	-22.149473	1.641574
-1232.851027	-12.758791	1.646579
-1236.188292	-17.490169	1.651584
-1240.302685	-17.561880	1.656589
-1244.166556	-10.932232	1.661594
-1247.757433	-17.023335	1.666598
-1252.000555	-5.961685	1.671603
-1255.229651	-17.450214	1.676608
-1258.703785	-13.040179	1.681613
-1262.532985	-14.119430	1.686618
-1266.317737	-13.961578	1.691622
-1270.623877	-13.975738	1.696627
-1274.046545	-22.168977	1.701632
-1278.112356	-8.494281	1.706637
-1281.799647	-20.947063	1.711642
-1285.454617	-16.252581	1.716646
-1289.446288	-14.210240	1.721651
-1292.696577	-21.454911	1.726656
-1296.706939	-10.288518	1.731661
-1300.555951	-11.366111	1.736666
-1303.852475	-17.734471	1.741670
-1308.222859	-12.510707	1.746675
-1311.910632	-16.799517	1.751680
-1315.474252	-14.883994	1.756685
-1319.034671	-17.666696	1.761690
-1322.860415	-16.341559	1.766694
-1326.947426	-10.917116	1.771699
-1330.470810	-24.151404	1.776704
-1334.692313	-12.364530	1.781709
-1338.143701	-15.932626	1.786714
-1341.628544	-11.396177	1.791718
-1345.659564	-9.319056	1.796723
-1349.177570	-20.144606	1.801728
-1353.204248	-19.397530	1.806733
-1356.801538	-18.419567	1.811738
-1360.409350	-13.551171	1.816742
-1364.536259	-6.872913	1.821747
-1367.970182	-19.801344	1.826752
-1372.094346	-13.246516	1.831757
-1375.723430	-10.883608	1.836762
-1379.332729	-10.267961	1.841766
-1383.436903	-7.811634	1.846771
-1386.603836	-18.098821	1.851776
-1390.869012	-10.534219	1.856781
-1394.908991	-13.252640	1.861786
-1398.254747	-13.302049	1.866790
-1402.114043	-12.428724	1.871795
-1405.319263	-17.684034	1.876800
-1409.434901	-14.883631	1.881805
-1413.179181	-20.599821	1.886810
-1417.272706	-13.092618	1.891814
-1421.166755	-7.486021	1.896819
-1424.271011	-18.579543	1.901824
-1428.288408	-11.194895	1.906829
-1432.117376	-12.184014	1.911834
-1435.986577	-10.594690	1.916838
-1439.887828	-4.179513	1.921843
-1443.213649	-10.672285	1.926848
-1447.249930	-4.257552	1.931853
-1450.995005	-5.848273	1.936858
-1454.497566	-13.672051	1.941862
-1458.319732	-7.905016	1.946867
-1462.054817	-13.157401	1.951872
-1466.097070	-11.417315	1.956877
-1469.689641	-13.942320	1.961882
-1473.273347	-19.986895	1.966886
-1477.349927	-4.715862	1.971891
-1480.793147	-14.755242	1.976896
-1484.518928	-8.705559	1.981901
-1488.553726	-8.633455	1.986906
-1492.153770	-14.716386	1.991910
-1496.355846	-2.252678	1.996915
-1500.287689	-14.176447	2.006912
-1500.973355	-13.474578	2.016909
-1498.204089	-16.095500	2.026906
-1495.577143	-11.763569	2.036902
-1493.295682	-14.991634	2.046899
-1491.455163	-17.924871	2.056896
-1489.505096	-13.421378	2.066893
-1487.843979	-13.065329	2.076890
-1485.989553	-17.412379	2.086886
-1483.719158	-13.380182	2.096883
-1481.888679	-17.983923	2.106880
-1480.062690	-20.627453	2.116877
-1478.208463	-15.952285	2.126874
-1476.420456	-12.253361	2.136870
-1474.601098	-15.721623	2.146867
-1472.610240	-11.568859	2.156864
-1470.585396	-17.345305	2.166861
-1468.711097	-12.340182	2.176858
-1466.745376	-10.261300	2.186854
-1465.092038	-6.212377	2.196851
-1462.879563	-9.105680	2.206848
-1460.998486	-15.418050	2.216845
-1459.377593	-10.947082	2.226842
-1457.506654	-7.926164	2.236838
-1455.654421	-9.497028	2.246835
-1453.598522	-14.282109	2.256832
-1451.734215	-15.738059	2.266829
-1449.744285	-19.404141	2.276826
-1448.014051	-15.495416	2.286822
-1446.177680	-17.248470	2.296819
-1444.103042	-14.771742	2.306816
-1442.264881	-10.600816	2.316813
-1440.757425	-13.441210	2.326810
-1438.615626	-16.092645	2.336806
-1436.502865	-18.665217	2.346803
-1434.572054	-21.562340	2.356800
-1432.916460	-19.070612	2.366797
-1431.461697	-11.530364	2.376794
-1429.366693	-15.113781	2.386790
-1427.072638	-13.621125	2.396787
-1425.333314	-16.906006	2.406784
-1423.386924	-13.829246	2.416781
-1421.644289	-17.166760	2.426778
-1420.007068	-12.234163	2.436774
-1417.790013	-13.541300	2.446771
-1415.986858	-13.168467	2.456768
-1413.920241	-12.444653	2.466765
-1411.921477	-10.266802	2.476762
-1410.660659	-13.936117	2.486758
-1408.830916	-8.489592	2.496755
-1406.627388	-15.881452	2.506752
-1404.583514	-11.012371	2.516749
-1402.683601	-12.783460	2.526746
-1400.875853	-12.933986	2.536742
-1399.015505	-9.657110	2.546739
-1397.350130	-9.058517	2.556736
-1395.527603	-5.826109	2.566733
-1393.426393	-14.243693	2.576730
-1391.454893	-13.030941	2.586726
-1389.534667	-11.066288	2.596723
-1387.781530	-13.724928	2.606720
-1386.122546	-14.216366	2.616717
-1384.053520	-12.738167	2.626714
-1382.244553	-11.887811	2.636710
-1380.377165	-6.641500	2.646707
-1378.545653	-17.873817	2.656704
-1376.161292	-13.716067	2.666701
-1374.688435	-9.377653	2.676698
-1372.794040	-9.440975	2.686694
-1371.066923	-6.542223	2.696691
-1369.247804	-7.348236	2.706688
-1367.307455	-10.919472	2.716685
-1365.040119	-14.899898	2.726682
-1363.127634	-9.153946	2.736678
-1361.412970	-9.186907	2.746675
-1359.844356	-11.564932	2.756672
-1357.702825	-20.288941	2.766669
-1355.800344	-17.550885	2.776666
-1353.778500	-14.724566	2.786662
-1352.346809	-11.178502	2.796659
-1350.235589	-8.009640	2.806656
-1348.332080	-12.770239	2.816653
-1346.621821	-11.937212	2.826650
-1344.503279	-13.605882	2.836646
-1342.612020	-13.122356	2.846643
-1340.931524	-14.750902	2.856640
-1339.134888	-10.173763	2.866637
-1337.339593	-8.416437	2.876634
-1335.318778	0.083285	2.886630
-1333.503758	-8.405285	2.896627
-1331.312557	-9.806098	2.906624
-1329.547268	-10.095036	2.916621
-1327.686028	-13.914106	2.926618
-1325.915294	-12.594949	2.936614
-1324.000418	-8.352517	2.946611
-1321.820019	-7.809466	2.956608
-1320.158394	-9.769717	2.966605
-1318.431330	-9.370416	2.976602
-1316.364599	-7.628100	2.986598
-1314.549803	-8.030742	2.996595
-1312.680329	-1.982591	3.006592
-1311.086703	0.228622	3.016589
-1308.865000	-8.896612	3.026586
-1306.992380	-6.267418	3.036582
-1305.395047	-4.672592	3.046579
-1303.448447	0.884798	3.056576
-1301.250374	-5.250825	3.066573
-1299.226514	-6.605876	3.076570
-1297.508414	-10.534645	3.086566
-1295.802051	-3.981946	3.096563
-1294.053023	-4.563522	3.106560
-1291.885889	-6.377292	3.116557
-1290.209822	-10.059327	3.126554
-1288.580922	-7.057947	3.136550
-1286.597979	-1.143198	3.146547
-1284.543666	-9.150554	3.156544
-1282.453175	-13.219441	3.166541
-1280.508381	-5.613827	3.176538
-1279.189600	-4.626513	3.186534
-1277.225898	-7.247720	3.196531
-1275.110958	-4.150435	3.206528
-1273.297570	-8.863395	3.216525
-1271.447012	-9.925419	3.226522
-1269.291666	-5.524054	3.236518
-1267.890843	3.430231	3.246515
-1265.887191	1.699491	3.256512
-1263.954486	-0.127263	3.266509
-1261.957419	-5.242248	3.276506
-1260.123899	-1.032528	3.286502
-1258.396955	-5.329006	3.296499
-1256.345045	-5.336915	3.306496
-1254.538927	1.370384	3.316493
-1252.199026	-10.421643	3.326490
-1250.854917	-6.995706	3.336486
-1249.102570	-10.446760	3.346483
-1246.890693	-11.607641	3.356480
-1245.079239	-9.112293	3.366477
-1243.383856	-9.320504	3.376474
-1241.241648	-8.760212	3.386470
-1239.472990	-7.361707	3.396467
-1237.754139	-5.089957	3.406464
-1235.757390	-7.877473	3.416461
-1233.877839	-11.667823	3.426458
-1232.182175	-8.405504	3.436454
-1230.158788	-0.035567	3.446451
-1228.073580	-2.087224	3.456448
-1226.300387	-7.284777	3.466445
-1224.266871	-9.225525	3.476442
-1222.710887	-4.582936	3.486438
-1220.959692	-5.700072	3.496435
-1218.733759	-1.723642	3.506432
-1216.839329	-5.652152	3.516429
-1215.086092	-8.519106	3.526426
-1213.491120	-10.162297	3.536422
-1211.527145	-9.215030	3.546419
-1209.441733	-6.220327	3.556416
-1207.449618	-9.880247	3.566413
-1205.764135	-2.894654	3.576410
-1203.847709	-0.700282	3.586406
-1201.987025	-2.112824	3.596403
-1199.998476	-3.864776	3.606400
-1198.010844	-5.404997	3.616397
-1196.168544	-8.205662	3.626394
-1194.455795	-4.368145	3.636390
-1192.652385	-0.791453	3.646387
-1190.830913	-4.960903	3.656384
-1188.971904	-5.995793	3.666381
-1186.846458	-6.800153	3.676378
-1185.189094	-8.200674	3.686374
-1183.352338	-5.991959	3.696371
-1181.310710	-6.947115	3.706368
-1179.336366	-1.376684	3.716365
-1177.371006	-5.401778	3.726362
-1175.772827	-1.397491	3.736358
-1173.883518	0.951247	3.746355
-1171.821627	-3.547188	3.756352
-1170.021284	-5.854798	3.766349
-1168.101940	-7.265645	3.776346
-1166.416813	-5.072129	3.786342
-1164.574320	-5.025922	3.796339
-1162.306818	-2.556105	3.806336
-1160.982868	-3.870105	3.816333
-1158.575394	-6.500639	3.826330
-1156.844604	-4.747059	3.836326
-1155.158045	-6.946451	3.846323
-1153.157636	-5.974963	3.856320
-1151.016746	-3.566983	3.866317
-1149.642277	-6.569081	3.876314
-1147.570768	-6.682661	3.886310
-1145.603018	-8.693348	3.896307
-1143.922347	-7.868067	3.906304
-1141.740167	-2.896126	3.916301
-1139.839466	-7.248743	3.926298
-1138.453951	-7.216246	3.936294
-1136.577154	-7.110768	3.946291
-1134.471207	-3.986647	3.956288
-1132.533230	-4.658332	3.966285
-1130.662841	-4.507612	3.976282
-1128.905198	-7.359419	3.986278
-1126.691752	-6.515151	3.996275
-1125.152556	-5.240900	4.006272
-1123.023265	-1.689444	4.016269
-1121.218522	-2.275067	4.026266
-1119.408817	-2.992537	4.036262
-1117.488366	2.417624	4.046259
-1115.474278	-1.749429	4.056256
-1113.673934	-4.080681	4.066253
-1112.057829	-11.330942	4.076250
-1110.113411	-4.104062	4.086246
-1108.354213	-6.435044	4.096243
-1106.232201	-9.801446	4.106240
-1104.314868	-7.938720	4.116237
-1102.451174	-10.491679	4.126234
-1100.537933	-13.365198	4.136230
-1098.662307	-6.968894	4.146227
-1096.929758	-7.876111	4.156224
-1095.109026	-10.084292	4.166221
-1093.021248	-2.891382	4.176218
-1091.026175	-7.060108	4.186214
-1089.551883	-2.331721	4.196211
-1087.670318	-9.588117	4.206208
-1085.659366	-11.967249	4.216205
-1083.847843	-9.779680	4.226202
-1081.936833	-3.952712	4.236198
-1079.902862	-10.450313	4.246195
-1078.040333	-7.025093	4.256192
-1076.293535	-8.275631	4.266189
-1074.430973	-7.269393	4.276186
-1072.282915	-6.373559	4.286182
-1070.469301	-3.392091	4.296179
-1068.994285	-0.624884	4.306176
-1066.783382	-5.383913	4.316173
-1065.043287	-2.370154	4.326170
-1062.889751	-3.411004	4.336166
-1061.112606	-2.550567	4.346163
-1059.487248	-3.216397	4.356160
-1057.639485	-11.272639	4.366157
-1055.324056	-11.161466	4.376154
-1053.582171	-11.850668	4.386150
-1052.106361	-7.542505	4.396147
-1049.947934	-5.863561	4.406144
-1048.138909	-5.249795	4.416141
-1045.977784	-5.106037	4.426138
-1044.293745	-3.725425	4.436134
-1042.494121	-9.577610	4.446131
-1040.482163	-11.183170	4.456128
-1038.729220	-3.815070	4.466125
-1036.714256	-8.659574	4.476122
-1035.140985	-9.585481	4.486118
-1033.468084	-9.493098	4.496115
-1031.465351	-4.260237	4.506112
-1029.228566	-11.717092	4.516109
-1027.077630	-9.133758	4.526106
-1025.613297	-9.031695	4.536102
-1023.769743	-3.844421	4.546099
-1021.817942	-6.994050	4.556096
-1019.961830	-9.722578	4.566093
-1018.097819	-7.222820	4.576090
-1016.031614	-7.106485	4.586086
-1014.432646	-9.817566	4.596083
-1012.564956	-10.318434	4.606080
-1010.514453	-9.561680	4.616077
-1008.879155	-14.514387	4.626074
-1006.797696	-16.449986	4.636070
-1004.808343	-5.019085	4.646067
-1003.081607	-11.132747	4.656064
-1001.196876	-9.013663	4.666061
-999.236797	-9.477191	4.676058
-997.387754	-8.356621	4.686054
-995.599648	-0.665681	4.696051
-993.625672	-4.897272	4.706048
-991.866866	-2.990149	4.716045
-989.809349	-17.263133	4.726042
-988.084441	-11.722116	4.736038
-985.973968	0.505764	4.746035
-984.310440	-6.295683	4.756032
-982.566960	-6.716663	4.766029
-980.812913	-8.400928	4.776026
-978.598212	-10.487287	4.786022
-976.495280	-9.890468	4.796019
-975.008163	-7.884620	4.806016
-972.968297	-3.589236	4.816013
-971.141564	-8.548851	4.826010
-969.369765	-7.471169	4.836006
-967.629835	-7.109980	4.846003
-965.398296	-9.844818	4.856000
-963.443162	-10.572792	4.865997
-961.709953	-4.810444	4.875994
-959.829159	-4.389668	4.885990
-957.922070	-10.663195	4.895987
-956.533808	-9.359958	4.905984
-954.405030	1.666590	4.915981
-952.389170	-7.441213	4.925978
-950.299380	-9.580204	4.935974
-948.543378	-4.978875	4.945971
-946.989854	-3.779429	4.955968
-944.801100	-9.813772	4.965965
-942.922762	-5.296739	4.975962
-941.111058	-5.234379	4.985958
-939.398389	-7.134633	4.995955
-937.466941	-8.166698	5.005952
-935.588837	-4.358579	5.015949
-933.347984	-6.875400	5.025946
-931.767426	-8.342412	5.035942
-930.190470	-1.871357	5.045939
-928.343960	-0.312951	5.055936
-925.915688	-2.087617	5.065933
-924.068705	-4.833560	5.075930
-922.335801	-7.616525	5.085926
-920.449741	-0.812776	5.095923
-918.589753	-2.294459	5.105920
-916.664398	-5.886625	5.115917
-914.946247	-10.696203	5.125914
-913.015704	-13.480761	5.135910
-911.135297	-10.168788	5.145907
-908.967894	-8.690098	5.155904
-907.592409	-3.175249	5.165901
-905.488964	-4.051628	5.175898
-903.669339	-2.927858	5.185894
-901.699682	-4.616539	5.195891
-899.895164	-3.828250	5.205888
-898.230326	-6.028727	5.215885
-895.977491	-7.317410	5.225882
-894.095675	-6.991483	5.235878
-892.472074	-5.477936	5.245875
-890.337383	-5.482968	5.255872
-888.667929	-5.903095	5.265869
-886.543033	-8.147119	5.275866
-884.558363	-11.331893	5.285862
-883.059077	-5.299973	5.295859
-881.233625	-1.484968	5.305856
-879.382323	0.007974	5.315853
-877.493592	-3.643045	5.325850
-875.652103	-4.376462	5.335846
-873.414121	-2.193746	5.345843
-871.472127	1.921587	5.355840
-870.096389	-4.607984	5.365837
-867.882125	-3.150957	5.375834
-866.111205	-7.181032	5.385830
-864.271053	-5.643664	5.395827
-862.471611	2.400847	5.405824
-859.984246	-7.276485	5.415821
-858.545770	-1.927993	5.425818
-856.690512	-5.936808	5.435814
-854.951030	-3.821223	5.445811
-852.820484	-6.422969	5.455808
-851.277089	-5.310261	5.465805
-849.102294	-7.372752	5.475802
-847.021720	-11.423895	5.485798
-845.534538	-6.026339	5.495795
-843.610242	-2.683428	5.505792
-841.716058	-3.988937	5.515789
-839.988717	-2.806152	5.525786
-837.988936	-2.034820	5.535782
-835.729699	-0.387579	5.545779
-834.282393	-3.099562	5.555776
-832.406882	-4.133652	5.565773
-830.257740	-13.485301	5.575770
-828.451284	-7.985612	5.585766
-826.707290	-4.767026	5.595763
-824.961739	-6.325081	5.605760
-823.117585	-3.828303	5.615757
-821.249739	-6.503292	5.625754
-818.846963	-7.103754	5.635750
-817.239925	-8.521238	5.645747
-815.435097	-2.733904	5.655744
-813.843641	-8.710550	5.665741
-811.296603	-3.054487	5.675738
-809.915679	-6.655859	5.685734
-807.920540	-5.511121	5.695731
-806.331888	-8.327788	5.705728
-804.052417	-2.129991	5.715725
-802.126781	-1.111509	5.725722
-800.344494	2.322036	5.735718
-798.599610	-5.054414	5.745715
-796.733382	-5.971727	5.755712
-794.814827	-1.424679	5.765709
-792.854665	-4.632306	5.775706
-790.957882	-6.295038	5.785702
-789.263795	-8.948543	5.795699
-787.066431	-4.345000	5.805696
-785.509676	-2.642268	5.815693
-783.502652	-7.886359	5.825690
-781.335391	-7.861761	5.835686
-780.166744	-3.657476	5.845683
-777.989679	-6.124483	5.855680
-775.783858	0.688284	5.865677
-773.923588	-6.665538	5.875674
-772.498168	-2.184916	5.885670
-770.438911	-1.544613	5.895667
-768.678384	3.594570	5.905664
-766.540887	-1.251935	5.915661
-764.783873	-4.218646	5.925658
-763.056690	-3.698948	5.935654
-760.900990	-4.059331	5.945651
-758.988965	-7.235552	5.955648
-757.275062	-2.441022	5.965645
-755.325990	-1.495722	5.975642
-753.420456	-9.447299	5.985638
-751.791709	-9.374500	5.995635
-749.686843	-2.428728	6.005632
-747.480331	-2.072470	6.015629
-746.210876	-7.686554	6.025626
-744.257935	-3.754443	6.035622
-742.220605	-3.600093	6.045619
-740.274719	-8.537531	6.055616
-738.538817	-3.541236	6.065613
-736.601960	-8.226171	6.075610
-734.416492	-2.668553	6.085606
-733.011347	-2.428950	6.095603
-731.026109	4.453856	6.105600
-729.198768	0.059589	6.115597
-727.144189	1.458586	6.125594
-725.558752	-7.272357	6.135590
-723.386909	-9.040574	6.145587
-721.397232	-2.518478	6.155584
-720.026149	-0.817608	6.165581
-717.923214	0.006817	6.175578
-716.038200	-3.049790	6.185574
-714.140325	0.243769	6.195571
-712.397956	-6.484841	6.205568
-710.065706	-10.190820	6.215565
-708.505519	-6.146964	6.225562
-706.808931	-8.505544	6.235558
-704.621977	-1.983380	6.245555
-702.874509	2.180556	6.255552
-700.751326	-5.139439	6.265549
-699.200240	-8.022667	6.275546
-697.158937	-7.905230	6.285542
-695.054317	-7.845278	6.295539
-693.283655	-7.913540	6.305536
-691.930606	-5.469232	6.315533
-689.911283	-2.589805	6.325530
-687.767048	-4.629899	6.335526
-685.685452	-6.314186	6.345523
-684.106692	-5.394916	6.355520
-682.367660	-4.003878	6.365517
-680.198140	-6.076427	6.375514
-678.415324	-9.509838	6.385510
-676.578978	-8.000134	6.395507
-674.806566	-6.653899	6.405504
-672.910378	-10.950174	6.415501
-670.780221	-9.668996	6.425498
-668.947694	-12.039798	6.435494
-667.358714	-7.866302	6.445491
-665.674317	-2.002756	6.455488
-663.276960	1.365774	6.465485
-661.505998	-4.647359	6.475482
-659.721583	-7.659426	6.485478
-657.774825	-2.221486	6.495475
-656.035629	-5.463172	6.505472
-653.937431	-5.727427	6.515469
-652.242027	-3.986757	6.525466
-650.261107	-3.439623	6.535462
-648.397985	-6.257412	6.545459
-646.675405	-0.110999	6.555456
-644.597324	-6.537935	6.565453
-642.684453	-7.179944	6.575450
-640.770071	-7.610609	6.585446
-639.127544	-11.531586	6.595443
-637.280683	-2.990769	6.605440
-635.157159	-1.839553	6.615437
-633.508288	-0.516180	6.625434
-631.166026	-11.108022	6.635430
-629.861994	-5.940006	6.645427
-627.935539	-12.086907	6.655424
-626.017951	-8.442735	6.665421
-623.974068	-3.122917	6.675418
-622.069159	-3.536265	6.685414
-620.249396	-5.200768	6.695411
-618.409405	-6.743762	6.705408
-616.337009	-2.649042	6.715405
-614.791676	-8.818728	6.725402
-612.924485	-8.430238	6.735398
-611.040277	-3.051740	6.745395
-609.191673	-3.925037	6.755392
-607.215265	-6.615629	6.765389
-605.061036	-10.675178	6.775386
-603.310406	-6.819573	6.785382
-601.623713	-5.638012	6.795379
-599.703704	-6.306390	6.805376
-597.784516	-4.459325	6.815373
-595.937447	-10.099299	6.825370
-593.812581	-7.503497	6.835366
-591.895078	-6.660387	6.845363
-590.384042	-5.922870	6.855360
-588.482756	-6.253505	6.865357
-586.791689	-7.720577	6.875354
-584.763520	-3.482971	6.885350
-582.763766	-1.639290	6.895347
-580.789813	-4.924742	6.905344
-579.198013	-2.166396	6.915341
-577.038918	1.854510	6.925338
-575.111291	-1.200902	6.935334
-573.169154	-4.064416	6.945331
-571.438586	1.322872	6.955328
-569.969759	-3.722967	6.965325
-567.678953	-5.960057	6.975322
-566.139967	-5.334360	6.985318
-563.671326	-2.670285	6.995315
-562.038971	-9.390695	7.005312
-560.192058	-6.654141	7.015309
-558.610926	-5.799903	7.025306
-556.718143	-8.535517	7.035302
-554.322640	-12.857780	7.045299
-552.559990	-7.734557	7.055296
-551.010071	-3.726845	7.065293
-548.987866	-5.600479	7.075290
-547.129174	-5.671640	7.085286
-545.198728	-0.033623	7.095283
-543.264482	-0.110534	7.105280
-541.380151	-8.154892	7.115277
-539.769590	-3.575795	7.125274
-537.743890	-11.712205	7.135270
-535.598059	-8.698110	7.145267
-534.001024	0.492190	7.155264
-532.530240	-4.424464	7.165261
-530.356765	-5.032219	7.175258
-528.171096	-1.920268	7.185254
-526.506270	-7.965303	7.195251
-524.774717	-6.824010	7.205248
-522.616838	-10.672489	7.215245
-520.785313	-8.381876	7.225242
-519.047188	-9.703256	7.235238
-517.161200	-6.200789	7.245235
-515.087785	-4.908827	7.255232
-513.204532	-8.249213	7.265229
-511.502815	-5.926806	7.275226
-509.427593	-6.007259	7.285222
-507.827048	-0.420729	7.295219
-506.032854	-7.694334	7.305216
-504.310139	-7.517949	7.315213
-501.962378	0.426657	7.325210
-499.939694	-10.871939	7.335206
-498.375057	-8.532365	7.345203
-496.451778	-9.403292	7.355200
-494.242872	-7.419253	7.365197
-492.763742	-8.312399	7.375194
-491.075577	-9.665254	7.385190
-488.916482	-16.978176	7.395187
-486.981562	-8.204975	7.405184
-485.193268	-6.109538	7.415181
-483.343996	-10.227648	7.425178
-481.247081	-5.585657	7.435174
-479.644146	-8.020704	7.445171
-477.987929	-16.090160	7.455168
-475.621920	-9.236362	7.465165
-474.090128	-14.533784	7.475162
-471.932388	-16.910587	7.485158
-469.947504	-4.698437	7.495155
-468.244340	-3.718361	7.505152
-466.473144	-3.636536	7.515149
-464.727232	-4.591219	7.525146
-462.682206	-5.800518	7.535142
-460.936373	-0.406107	7.545139
-459.244416	-6.886494	7.555136
-456.688835	-2.436153	7.565133
-454.715743	-5.238200	7.575130
-453.470168	-4.837155	7.585126
-451.645238	-3.401241	7.595123
-449.542835	-1.382781	7.605120
-447.554676	-1.004005	7.615117
-445.722457	-5.563058	7.625114
-443.952101	-12.365434	7.635110
-442.214063	-8.324531	7.645107
-439.829190	-10.612840	7.655104
-438.676294	-0.056775	7.665101
-436.274104	-6.328456	7.675098
-434.457780	-9.956522	7.685094
-432.426713	-9.000363	7.695091
-430.791615	-7.562539	7.705088
-429.031602	-9.469995	7.715085
-426.802920	-9.881205	7.725082
-424.944980	-16.042276	7.735078
-423.457051	-9.389261	7.745075
-421.631086	-10.123007	7.755072
-419.643761	-10.303034	7.765069
-417.458087	-6.868866	7.775066
-415.939832	-9.099293	7.785062
-413.697561	-11.296909	7.795059
-411.895767	-10.907291	7.805056
-410.297962	-4.292337	7.815053
-408.435894	-10.199842	7.825050
-406.072450	-1.258143	7.835046
-404.325016	-0.844049	7.845043
-402.786663	1.179255	7.855040
-401.112847	-1.311272	7.865037
-398.579215	-2.530640	7.875034
-397.214608	-5.590751	7.885030
-395.187358	-6.599781	7.895027
-393.033982	-5.333110	7.905024
-391.618877	-1.082703	7.915021
-389.623436	-0.561353	7.925018
-387.539378	-11.116494	7.935014
-385.491662	-5.966021	7.945011
-383.733222	-0.879885	7.955008
-382.408241	-0.317793	7.965005
-379.845534	-1.941266	7.975002
-378.047306	7.013346	7.984998
-376.226186	-5.130895	7.994995
-374.328525	2.263597	8.004992
-372.998766	-3.039407	8.014989
-370.797642	-5.830428	8.024986
-368.760392	-7.829475	8.034982
-367.100893	-7.680793	8.044979
-365.161792	-6.218829	8.054976
-363.216665	-6.453651	8.064973
-361.276954	-2.133824	8.074970
-359.371804	-6.991835	8.084966
-357.640236	-6.237271	8.094963
-355.850871	-3.101356	8.104960
-353.575559	-2.079912	8.114957
-351.908260	-7.302582	8.124954
-350.300876	-7.938217	8.134950
-348.086961	-7.364870	8.144947
-346.184945	-4.723786	8.154944
-344.575239	-11.235178	8.164941
-342.702031	-5.519952	8.174938
-340.685667	-7.247214	8.184934
-339.198700	-5.084609	8.194931
-336.985147	-2.449043	8.204928
-335.021976	-3.523584	8.214925
-332.940663	-3.693280	8.224922
-331.266400	-1.825839	8.234918
-329.449767	-2.502762	8.244915
-327.746677	-1.126248	8.254912
-325.643840	1.995963	8.264909
-324.067547	-1.563704	8.274906
-321.783493	-4.334762	8.284902
-319.799916	-3.951989	8.294899
-318.216636	-0.742090	8.304896
-316.485577	1.601042	8.314893
-314.756341	0.579653	8.324890
-312.584185	3.717653	8.334886
-310.573148	0.900188	8.344883
-308.708370	-3.292906	8.354880
-306.928741	-4.117066	8.364877
-305.073527	2.562669	8.374874
-303.201753	1.441164	8.384870
-301.242662	-5.015452	8.394867
-299.303008	-4.159850	8.404864
-297.605863	1.883530	8.414861
-295.574522	-7.939953	8.424858
-293.706519	-3.144401	8.434854
-292.015667	-7.175503	8.444851
-290.110281	-14.578817	8.454848
-288.179407	-7.568512	8.464845
-286.424169	-3.059696	8.474842
-284.565112	-1.768049	8.484838
-282.632454	-5.964063	8.494835
-280.622224	-5.639198	8.504832
-278.714328	-7.971214	8.514829
-276.885757	-3.461465	8.524826
-275.194134	-2.173084	8.534822
-273.117760	-4.525674	8.544819
-271.126017	-9.250596	8.554816
-269.442124	-7.231488	8.564813
-267.672309	-2.246552	8.574810
-265.395196	-10.287095	8.584807
-263.967576	-8.133916	8.594803
-261.978743	-7.008234	8.604800
-260.169871	-1.884259	8.614797
-258.311385	-1.634630	8.624794
-256.157866	-7.069063	8.634791
-254.399088	-6.048762	8.644787
-252.512440	-5.202031	8.654784
-250.472578	0.227722	8.664781
-248.913533	0.732001	8.674778
-247.026663	0.129194	8.684775
-244.968472	-7.292166	8.694771
-243.009501	-4.870092	8.704768
-241.276024	-5.934738	8.714765
-239.350934	-8.806322	8.724762
-237.499775	-9.341841	8.734759
-235.630586	-11.266584	8.744755
-233.853879	-17.274024	8.754752
-231.927577	-5.791260	8.764749
-229.853836	-1.896932	8.774746
-228.319188	-2.280871	8.784743
-226.332935	-12.465008	8.794739
-224.266196	-7.694802	8.804736
-222.280918	-8.911731	8.814733
-220.850272	-6.943750	8.824730
-218.784199	-8.430945	8.834727
-216.647106	-1.571910	8.844723
-214.921276	-7.792280	8.854720
-213.142467	-3.001372	8.864717
-211.224239	-9.656665	8.874714
-209.412077	-8.468004	8.884711
-207.501830	-16.513103	8.894707
-205.315378	-17.574225	8.904704
-203.635904	-14.993826	8.914701
-201.872072	-13.180065	8.924698
-200.029846	-16.654196	8.934695
-198.137125	-15.206799	8.944691
-196.321423	-17.879308	8.954688
-194.277234	-7.831672	8.964685
-192.477920	-10.258400	8.974682
-190.609643	-12.309282	8.984679
-188.725033	-14.402244	8.994675
-186.693918	-10.267387	9.004672
-184.962648	-16.742818	9.014669
-183.006540	-16.042910	9.024666
-181.470594	-12.642202	9.034663
-179.332021	-16.981526	9.044659
-177.645101	-15.318107	9.054656
-175.896801	-14.116072	9.064653
-173.855428	-12.894488	9.074650
-171.723487	-14.401629	9.084647
-169.720821	-19.808754	9.094643
-168.152283	-17.450632	9.104640
-166.056718	-19.212495	9.114637
-164.488417	-16.429586	9.124634
-162.524544	-12.236609	9.134631
-160.637240	-12.874155	9.144627
-158.449376	-18.610833	9.154624
-156.853950	-18.549678	9.164621
-155.049288	-15.978169	9.174618
-152.884450	-17.528438	9.184615
-151.415767	-14.079082	9.194611
-149.556921	-7.137689	9.204608
-147.200188	-13.089205	9.214605
-145.715546	-9.050272	9.224602
-143.802125	-14.354714	9.234599
-141.663881	-6.178921	9.244595
-140.153922	-9.562095	9.254592
-138.052945	-5.286759	9.264589
-136.153648	-6.297261	9.274586
-134.265133	-8.206064	9.284583
-132.326833	-7.774858	9.294579
-130.741175	-12.180656	9.304576
-128.841233	-12.777561	9.314573
-126.854469	-11.626172	9.324570
-125.108381	-17.167590	9.334567
-123.131466	-12.112955	9.344563
-121.149851	-9.200171	9.354560
-119.275725	-6.260759	9.364557
-117.431228	-8.980440	9.374554
-115.759411	-9.160400	9.384551
-113.597103	-8.379650	9.394547
-111.596556	-12.959006	9.404544
-110.187795	-11.813274	9.414541
-108.103152	-6.755286	9.424538
-106.029658	-8.200938	9.434535
-104.290386	-11.642785	9.444531
-102.562154	-6.962146	9.454528
-100.563964	-7.718393	9.464525
-98.303820	-3.004194	9.474522
-96.868193	-13.967247	9.484519
-95.111707	-11.222210	9.494515
-93.292963	-6.507056	9.504512
-90.961840	-6.710085	9.514509
-89.172672	-2.762331	9.524506
-87.708440	2.323611	9.534503
-85.317704	-6.593878	9.544499
-83.516107	-13.958382	9.554496
-81.923304	-6.096568	9.564493
-80.134428	-1.523482	9.574490
-78.261394	-12.101566	9.584487
-76.057970	-9.748355	9.594483
-74.201893	-8.127639	9.604480
-72.234858	-9.178901	9.614477
-70.496513	-5.613035	9.624474
-68.785278	-5.376083	9.634471
-66.984598	-4.842340	9.644467
-64.984924	-4.574032	9.654464
-63.012709	-3.393425	9.664461
-60.955219	-1.752725	9.674458
-59.238192	-11.341146	9.684455
-57.348061	-7.878436	9.694451
-55.676156	-3.349829	9.704448
-53.619335	-6.697036	9.714445
-51.794996	-8.368164	9.724442
-50.119481	-7.969181	9.734439
-48.046177	-4.061988	9.744435
-45.965151	-3.163995	9.754432
-43.982551	-7.416745	9.764429
-42.337067	-11.988353	9.774426
-40.727615	-11.323029	9.784423
-38.750050	-9.064808	9.794419
-36.628665	-1.189384	9.804416
-35.056422	-11.951567	9.814413
-32.947351	-8.789033	9.824410
-31.428651	-3.803326	9.834407
-29.253800	-7.613038	9.844403
-27.518042	-1.750878	9.854400
-25.336585	-1.892073	9.864397
-23.404725	3.280372	9.874394
-21.781607	-5.301446	9.884391
-19.658578	-6.919142	9.894387
-18.099376	-12.440153	9.904384
-16.385562	-7.687673	9.914381
-14.102981	-11.347182	9.924378
-12.511049	-12.025920	9.934375
-10.658766	-0.851674	9.944371
-8.649613	-17.375784	9.954368
-6.490418	-9.256888	9.964365
-5.351862	0.359068	9.974362
-4.059972	28.371076	9.984359
-2.569052	71.006048	9.994355
-1.141372	126.738000	10.004352
0.000000	177.379004	10.009357
0.928388	219.825415	10.014362
1.344038	250.967820	10.019367
1.957562	278.336508	10.024371
2.591163	286.392449	10.029376
2.648572	321.296524	10.034381
2.949263	321.868299	10.039386
3.168008	342.987334	10.044391
3.081188	337.387016	10.049395
3.136560	335.906813	10.054400
3.054095	349.613092	10.059405
3.621252	352.268170	10.064410
3.164388	375.705984	10.069415
3.657298	369.975332	10.074419
3.931916	374.282474	10.079424
3.850888	384.577484	10.084429
3.769688	377.862884	10.089434
3.629961	389.517182	10.094439
4.328403	380.752688	10.099443
4.390412	391.419139	10.104448
3.887072	382.890499	10.109453
4.309613	392.504348	10.114458
4.130796	395.541786	10.119463
4.149133	392.201880	10.124467
4.347758	395.702680	10.129472
3.785498	399.969850	10.134477
4.055508	408.792725	10.139482
3.994751	415.509433	10.144487
4.184630	400.189974	10.149491
4.204569	398.122460	10.154496
3.889567	410.142213	10.159501
4.468381	413.643877	10.164506
4.478657	439.785980	10.169511
4.760871	438.755304	10.174515
5.016952	437.847073	10.179520
4.474889	426.310904	10.184525
4.611158	423.142998	10.189530
4.624406	429.980378	10.194535
5.029562	437.568988	10.199539
5.021979	441.429134	10.204544
4.666779	432.939915	10.209549
4.958506	438.464957	10.214554
5.140312	458.817315	10.219559
4.835672	458.832767	10.224563
4.932745	454.612926	10.229568
4.903361	459.433805	10.234573
5.297132	458.369563	10.239578
5.144698	475.704803	10.244583
5.290709	472.581066	10.249587
5.273759	468.431451	10.254592
5.253777	471.342640	10.259597
5.294616	472.146691	10.264602
5.351676	473.044352	10.269607
5.414896	470.775950	10.274611
5.464061	477.468846	10.279616
5.348506	472.231043	10.284621
5.696807	474.686078	10.289626
5.134137	483.266489	10.294631
5.629417	481.358118	10.299635
5.845908	477.527671	10.304640
5.646635	479.484976	10.309645
5.650078	477.741794	10.314650
5.573319	485.266945	10.319655
5.549732	483.772513	10.324659
5.868511	493.953362	10.329664
6.111104	506.084534	10.334669
6.434986	509.768818	10.339674
5.922793	503.539243	10.344679
6.049047	484.709926	10.349683
6.580996	501.259489	10.354688
6.212935	496.213349	10.359693
6.432834	487.222337	10.364698
6.167199	497.212544	10.369703
6.008625	490.544929	10.374707
6.001183	505.294415	10.379712
5.921033	513.021981	10.384717
6.387010	517.276563	10.389722
5.752614	528.445301	10.394727
6.339126	526.464021	10.399731
6.345332	526.702716	10.404736
6.383851	532.255567	10.409741
6.550770	534.460412	10.414746
6.454516	546.852257	10.419751
6.687275	554.148291	10.424755
7.053708	552.574292	10.429760
6.917086	564.452173	10.434765
7.236311	555.459468	10.439770
6.825193	574.943001	10.444775
6.881839	564.132855	10.449779
7.120420	577.412804	10.454784
7.010205	578.884384	10.459789
7.258269	564.227288	10.464794
6.999389	571.380967	10.469799
7.029489	574.888191	10.474803
7.274531	583.313013	10.479808
7.000348	574.179974	10.484813
7.074311	576.606243	10.489818
6.963705	586.071863	10.494823
7.074803	585.273487	10.499827
7.213365	577.402470	10.504832
6.915316	593.329132	10.509837
7.392142	607.055256	10.514842
7.675672	616.376021	10.519847
7.840849	615.054904	10.524851
7.783646	626.253080	10.529856
7.839533	620.293980	10.534861
7.924820	610.497997	10.539866
7.500188	624.549288	10.544871
7.789495	620.182035	10.549875
7.671891	624.214329	10.554880
7.606324	630.815203	10.559885
7.801290	630.000293	10.564890
7.556977	634.817664	10.569895
7.592093	633.192421	10.574899
7.989007	645.882598	10.579904
8.309144	663.882314	10.584909
8.326597	658.181656	10.589914
8.201756	673.178710	10.594919
8.157249	668.841034	10.599923
8.254849	669.992453	10.604928
8.098037	675.453507	10.609933
8.147723	673.956830	10.614938
8.294934	677.655145	10.619943
8.516718	665.812429	10.624947
8.496487	675.268423	10.629952
7.988782	680.728676	10.634957
8.247440	668.525241	10.639962
8.185910	699.848809	10.644967
8.475297	697.829742	10.649971
8.636344	705.235068	10.654976
8.704027	718.411512	10.659981
8.884288	709.040309	10.664986
8.687152	712.686321	10.669991
8.517580	711.574717	10.674995
8.513594	722.321328	10.680000
8.522376	722.357753	10.685005
9.047160	732.509064	10.690010
8.860887	748.066384	10.695015
9.154690	745.527756	10.700019
9.492824	746.133004	10.705024
9.054336	750.331641	10.710029
9.363015	751.157643	10.715034
9.189836	753.044586	10.720039
9.101316	752.481481	10.725043
9.209615	747.291456	10.730048
8.724321	757.033009	10.735053
9.158252	761.748544	10.740058
9.276608	778.329700	10.745063
9.298118	784.984568	10.750067
9.771819	783.723039	10.755072
9.737854	800.418409	10.760077
9.463225	791.952398	10.765082
9.423784	792.274076	10.770087
9.671961	795.956317	10.775091
9.428100	798.849662	10.780096
9.566065	806.689258	10.785101
9.975111	815.808769	10.790106
10.017604	828.912055	10.795111
9.903255	826.776008	10.800115
10.196339	827.796904	10.805120
10.004825	831.557173	10.810125
10.266046	832.745589	10.815130
10.328916	832.245071	10.820135
10.481674	827.541546	10.825139
10.501816	832.569129	10.830144
10.295026	838.503448	10.835149
10.140043	835.022341	10.840154
10.251461	839.912356	10.845159
10.406787	837.485693	10.850163
10.385257	837.806092	10.855168
10.062609	840.417103	10.860173
10.340404	830.063527	10.865178
10.420332	838.257773	10.870183
10.457130	839.019908	10.875187
10.697080	851.468780	10.880192
10.470049	864.632437	10.885197
10.714177	867.050537	10.890202
10.829068	871.611979	10.895207
10.689328	878.341499	10.900211
10.656587	879.611504	10.905216
10.907400	884.238008	10.910221
10.904595	879.625517	10.915226
10.853727	876.288653	10.920231
10.994200	874.163996	10.925235
10.957112	884.488622	10.930240
10.941649	900.288536	10.935245
11.299099	901.240819	10.940250
11.348900	915.607825	10.945255
11.209337	915.899741	10.950259
11.451762	907.330686	10.955264
11.382637	915.619719	10.960269
11.936542	918.672864	10.965274
11.756014	920.586233	10.970279
11.351139	919.486913	10.975283
11.676050	908.062823	10.980288
11.585549	922.835443	10.985293
12.085759	917.194886	10.990298
12.034570	918.045182	10.995303
11.836095	917.543767	11.000307
11.868481	923.758538	11.005312
11.735564	922.614261	11.010317
12.097462	915.596906	11.015322
11.916601	925.416176	11.020327
11.839674	920.853344	11.025331
12.125894	912.543826	11.030336
11.634117	914.820677	11.035341
11.924845	926.818358	11.040346
11.764241	928.149765	11.045351
11.768376	921.657863	11.050355
11.796174	933.588670	11.055360
11.904331	943.421781	11.060365
12.216795	943.458655	11.065370
11.885740	964.967513	11.070375
12.379425	953.178973	11.075379
12.474783	951.564587	11.080384
11.971344	959.173812	11.085389
12.122268	965.886973	11.090394
12.436628	974.154297	11.095399
12.703841	988.475657	11.100403
12.595197	993.728858	11.105408
12.730387	992.209047	11.110413
12.993003	986.358760	11.115418
12.873583	995.603684	11.120423
13.175846	997.529948	11.125427
12.833890	986.209013	11.130432
12.674811	992.629409	11.135437
12.905991	993.701195	11.140442
12.752252	995.730159	11.145447
12.802153	986.508893	11.150451
12.662939	994.905352	11.155456
12.801333	997.166861	11.160461
13.351317	997.534886	11.165466
13.198203	1019.587920	11.170471
13.301523	1015.780117	11.175475
13.368256	1010.662866	11.180480
13.330937	1023.804291	11.185485
13.433297	1020.217430	11.190490
13.366937	1021.847652	11.195495
13.270692	1018.182076	11.200499
13.402833	1027.451554	11.205504
13.348886	1028.778575	11.210509
13.755880	1020.053884	11.215514
13.414572	1029.954014	11.220519
13.262854	1031.388101	11.225523
13.541609	1044.263068	11.230528
13.559618	1057.457205	11.235533
13.916462	1053.170523	11.240538
13.609885	1058.557829	11.245543
13.756936	1058.805608	11.250547
13.744150	1059.447920	11.255552
13.847627	1060.336637	11.260557
14.112980	1055.277583	11.265562
13.940787	1067.995823	11.270567
14.267007	1064.467870	11.275571
14.199729	1066.254375	11.280576
14.147655	1070.911904	11.285581
14.346269	1085.554987	11.290586
14.488249	1088.554016	11.295591
14.555739	1095.859337	11.300595
14.682656	1098.242551	11.305600
14.552002	1083.796743	11.310605
14.665659	1072.964509	11.315610
14.485416	1074.439423	11.320615
14.357363	1084.425433	11.325619
14.847078	1086.067898	11.330624
14.878790	1093.304802	11.335629
14.915592	1082.959523	11.340634
15.038742	1098.453667	11.345639
14.976031	1087.152772	11.350643
14.807819	1076.567363	11.355648
14.405149	1089.382314	11.360653
14.968643	1086.562471	11.365658
15.053145	1100.165545	11.370663
15.234106	1093.448225	11.375667
15.297172	1102.522171	11.380672
14.690059	1100.660241	11.385677
14.849728	1099.062392	11.390682
14.715517	1099.875474	11.395687
14.937794	1098.404845	11.400691
14.924040	1105.447139	11.405696
15.169042	1127.525151	11.410701
15.123474	1129.724553	11.415706
15.289945	1126.458630	11.420711
15.288384	1135.997896	11.425715
15.331773	1140.345304	11.430720
15.121249	1138.355450	11.435725
15.502569	1133.998603	11.440730
15.656151	1149.026647	11.445735
15.687521	1162.950519	11.450739
15.863367	1161.516466	11.455744
15.941463	1166.323589	11.460749
16.401518	1154.933738	11.465754
16.057623	1147.770996	11.470759
15.790832	1140.979192	11.475763
15.957778	1136.994036	11.480768
15.891861	1145.353657	11.485773
16.153258	1153.695770	11.490778
16.147175	1171.319969	11.495783
16.258122	1158.426840	11.500787
16.614480	1162.289844	11.505792
16.264754	1149.157939	11.510797
16.466819	1143.774605	11.515802
16.169239	1135.520230	11.520807
16.170047	1150.105036	11.525811
16.137915	1160.320247	11.530816
16.447792	1171.694489	11.535821
16.494345	1163.845719	11.540826
16.384071	1170.330954	11.545831
16.146070	1165.559539	11.550835
16.391450	1169.798248	11.555840
16.177923	1184.691690	11.560845
16.563097	1176.967113	11.565850
16.648889	1196.021308	11.570855
17.150076	1202.498920	11.575859
17.057242	1196.128817	11.580864
16.636245	1197.225791	11.585869
17.158363	1192.962385	11.590874
16.953985	1211.264083	11.595879
17.165163	1203.176124	11.600883
16.898218	1196.614576	11.605888
16.974323	1200.738356	11.610893
16.710635	1201.578404	11.615898
17.042308	1213.236234	11.620903
16.924709	1204.912895	11.625907
17.310525	1208.555151	11.630912
17.374420	1202.805080	11.635917
17.556812	1205.027274	11.640922
17.210833	1208.419579	11.645927
17.015803	1205.154524	11.650931
17.295045	1225.937945	11.655936
17.547646	1230.341905	11.660941
17.874712	1234.180425	11.665946
17.605981	1237.724434	11.670951
17.886582	1234.246299	11.675955
18.081920	1234.123646	11.680960
17.715872	1243.249566	11.685965
17.921479	1239.904040	11.690970
17.939776	1234.158864	11.695975
18.070482	1235.741905	11.700979
18.176567	1235.152472	11.705984
17.892969	1239.015062	11.710989
18.246977	1231.641602	11.715994
18.064174	1222.184465	11.720999
18.088224	1233.629580	11.726003
18.405849	1232.036487	11.731008
18.183049	1236.303368	11.736013
18.241772	1227.287932	11.741018
18.365608	1234.345404	11.746023
18.222275	1234.169528	11.751027
18.541617	1229.974729	11.756032
18.399427	1239.169817	11.761037
18.416699	1231.276791	11.766042
18.260475	1241.997601	11.771047
18.966094	1237.282250	11.776051
18.762500	1233.418466	11.781056
18.521012	1245.027382	11.786061
18.815189	1238.254087	11.791066
18.781154	1235.314251	11.796071
18.477775	1242.006956	11.801075
18.723518	1237.065307	11.806080
18.471555	1237.405911	11.811085
18.385583	1237.907714	11.816090
18.446893	1250.878267	11.821095
18.555862	1265.658056	11.826099
18.900772	1269.604137	11.831104
18.864446	1271.370748	11.836109
19.022368	1265.025279	11.841114
19.216640	1272.690549	11.846119
19.167955	1268.508706	11.851123
19.295122	1263.117562	11.856128
19.219853	1270.840807	11.861133
19.151538	1266.794572	11.866138
19.026343	1282.312753	11.871143
19.080770	1295.843529	11.876147
19.859570	1302.385727	11.881152
19.805132	1306.919905	11.886157
20.028211	1303.014858	11.891162
19.828397	1304.525247	11.896167
19.826754	1301.852282	11.901171
19.705624	1296.406893	11.906176
19.559573	1299.112829	11.911181
19.813163	1304.491307	11.916186
19.966271	1309.142996	11.921191
19.791094	1300.465262	11.926195
20.088604	1302.216479	11.931200
19.942782	1308.275317	11.936205
20.113093	1294.264678	11.941210
20.071262	1300.668873	11.946215
20.035850	1304.749751	11.951219
20.042456	1305.616873	11.956224
20.170753	1307.151417	11.961229
20.047632	1303.488478	11.966234
20.184903	1307.462957	11.971239
20.073965	1308.780957	11.976243
20.248609	1303.008450	11.981248
19.918781	1312.759479	11.986253
20.089327	1316.897405	11.991258
20.241606	1338.843857	11.996263
20.428844	1336.195958	12.001267
20.547740	1333.469853	12.006272
20.402736	1340.757147	12.011277
20.615948	1338.232851	12.016282
20.728723	1342.313759	12.021287
20.733650	1345.724249	12.026291
20.611593	1331.812254	12.031296
20.745696	1341.821286	12.036301
21.060271	1334.990283	12.041306
20.646494	1334.998693	12.046311
20.741122	1332.032796	12.051315
20.789049	1329.507266	12.056320
20.690000	1332.547944	12.061325
20.921130	1333.717546	12.066330
20.881759	1341.330225	12.071335
20.901053	1329.140763	12.076339
21.004087	1313.438343	12.081344
20.510097	1309.147725	12.086349
21.026942	1301.793992	12.091354
20.910736	1307.392322	12.096359
20.784860	1304.201378	12.101363
21.020907	1300.388101	12.106368
20.783528	1308.231061	12.111373
20.740479	1307.845991	12.116378
20.679863	1315.573231	12.121383
20.922243	1313.265871	12.126387
21.153866	1307.520548	12.131392
20.746068	1305.870461	12.136397
20.687311	1277.471338	12.141402
20.481190	1279.901396	12.146407
20.706060	1284.386285	12.151411
20.731721	1271.185718	12.156416
20.492710	1283.970003	12.161421
20.846990	1281.129874	12.166426
20.829504	1277.788381	12.171431
20.613727	1280.043342	12.176435
20.990889	1280.776445	12.181440
20.388828	1288.490675	12.186445
20.771946	1283.900086	12.191450
20.855544	1276.673824	12.196455
20.407471	1281.768359	12.201459
20.789384	1280.237553	12.206464
20.506753	1283.859492	12.211469
20.655515	1281.528430	12.216474
20.462662	1284.826147	12.221479
20.894171	1282.168472	12.226483
20.747459	1276.005643	12.231488
21.006149	1281.062359	12.236493
21.093842	1288.605063	12.241498
21.086568	1291.996196	12.246503
20.743222	1293.852785	12.251507
20.853606	1284.284970	12.256512
20.958880	1289.862160	12.261517
21.346369	1279.885048	12.266522
20.615517	1265.610493	12.271527
20.680539	1265.559093	12.276531
20.906060	1254.253099	12.281536
20.588855	1260.914897	12.286541
20.794149	1255.583053	12.291546
20.528194	1257.379191	12.296551
20.574486	1252.396016	12.301555
20.521336	1256.213179	12.306560
20.356198	1260.696396	12.311565
20.721152	1256.485641	12.316570
20.696443	1257.921570	12.321575
20.611337	1260.809397	12.326579
20.820026	1255.268044	12.331584
20.654143	1258.413994	12.336589
20.796704	1260.541615	12.341594
20.781191	1261.613343	12.346599
20.604365	1260.366434	12.351603
20.813499	1265.255201	12.356608
20.548652	1260.436779	12.361613
20.984783	1255.712363	12.366618
20.878408	1258.751041	12.371623
20.637320	1262.346634	12.376627
20.711504	1257.046741	12.381632
20.435757	1269.978025	12.386637
20.361276	1265.404443	12.391642
20.568669	1266.760770	12.396647
20.440855	1265.272630	12.401651
20.985986	1260.706674	12.406656
20.552714	1268.047796	12.411661
20.767063	1260.099663	12.416666
20.394155	1262.335526	12.421671
20.247535	1262.202755	12.426675
20.862851	1261.089718	12.431680
20.591213	1267.794719	12.436685
20.385080	1266.540655	12.441690
20.605037	1272.302203	12.446695
20.400114	1267.981262	12.451699
20.563580	1268.043482	12.456704
20.468917	1280.477490	12.461709
20.890641	1285.244037	12.466714
21.083136	1282.034647	12.471719
20.450538	1276.800957	12.476723
20.505503	1267.312174	12.481728
20.411249	1271.724159	12.486733
20.624887	1284.591590	12.491738
20.704099	1295.114020	12.496743
20.841827	1297.164351	12.501747
20.898723	1273.647658	12.506752
20.344405	1279.343457	12.511757
20.660676	1267.473355	12.516762
20.616210	1277.871195	12.521767
20.468377	1279.574371	12.526771
20.875396	1281.947635	12.531776
20.755207	1281.244466	12.536781
20.907692	1269.570815	12.541786
20.878680	1277.524828	12.546791
20.653020	1271.313875	12.551795
20.797965	1262.428970	12.556800
20.654457	1279.785821	12.561805
20.582596	1268.774066	12.566810
20.951242	1271.307217	12.571815
20.626995	1280.001461	12.576819
21.085637	1278.179269	12.581824
20.829461	1281.195321	12.586829
20.973967	1272.975230	12.591834
21.113022	1277.949303	12.596839
20.587833	1278.986411	12.601843
20.841060	1272.580790	12.606848
20.515754	1275.479332	12.611853
20.815226	1273.026453	12.616858
20.357627	1267.879193	12.621863
20.485617	1278.515269	12.626867
21.117776	1271.622599	12.631872
20.176741	1279.733125	12.636877
20.529724	1275.155231	12.641882
20.577304	1284.257782	12.646887
20.321847	1280.018233	12.651891
20.708402	1275.154258	12.656896
20.357926	1287.814386	12.661901
20.832291	1278.205867	12.666906
20.717341	1286.834401	12.671911
20.567798	1287.428355	12.676915
20.663478	1281.634544	12.681920
20.892892	1287.870877	12.686925
20.721151	1285.087839	12.691930
21.140390	1286.218758	12.696935
20.962259	1284.480785	12.701939
20.950392	1267.691189	12.706944
20.733737	1267.576686	12.711949
20.726259	1254.005280	12.716954
20.456039	1257.328736	12.721959
20.092256	1263.012274	12.726963
20.493819	1267.483169	12.731968
20.437235	1287.605816	12.736973
20.914575	1282.124903	12.741978
21.100988	1288.131529	12.746983
20.561397	1271.512054	12.751987
20.636160	1257.933835	12.756992
20.339754	1263.922836	12.761997
20.688569	1274.297372	12.767002
20.786370	1286.261462	12.772007
20.834301	1276.329050	12.777011
20.853688	1267.699946	12.782016
20.734942	1258.639461	12.787021
20.865265	1250.937359	12.792026
20.732927	1258.771423	12.797031
20.612085	1262.757096	12.802035
20.411691	1263.911936	12.807040
20.560939	1260.842714	12.812045
20.706905	1260.279249	12.817050
20.885443	1263.412845	12.822055
20.577338	1261.220897	12.827059
20.866595	1250.804478	12.832064
20.638211	1265.993715	12.837069
20.752069	1261.031302	12.842074
20.654263	1262.190280	12.847079
20.417050	1268.550713	12.852083
20.804091	1255.548798	12.857088
20.876457	1264.107225	12.862093
20.671348	1261.301126	12.867098
20.660213	1268.076550	12.872103
20.917580	1267.735825	12.877107
20.969151	1262.156447	12.882112
20.669932	1276.107136	12.887117
20.802070	1271.823114	12.892122
20.904699	1270.305314	12.897127
20.637559	1267.728325	12.902131
20.806150	1264.960399	12.907136
20.589701	1273.168256	12.912141
20.643484	1267.937852	12.917146
20.614562	1276.989518	12.922151
20.692932	1271.516259	12.927155
20.819717	1266.707127	12.932160
20.734578	1277.046004	12.937165
20.897561	1264.270650	12.942170
20.854065	1244.824757	12.947175
20.159343	1238.728063	12.952179
20.658547	1250.698279	12.957184
20.429793	1263.981642	12.962189
20.492039	1263.199696	12.967194
20.779636	1266.401850	12.972199
20.459605	1271.176307	12.977203
20.738570	1280.055851	12.982208
20.434469	1276.731687	12.987213
20.682070	1267.747606	12.992218
20.791066	1271.386719	12.997223
20.667064	1281.393509	13.002227
20.844442	1264.078519	13.007232
20.593926	1273.323238	13.012237
20.410370	1274.872035	13.017242
20.726431	1268.255312	13.022247
20.682516	1270.415832	13.027251
20.750578	1271.925283	13.032256
20.681800	1283.382090	13.037261
20.597071	1277.064280	13.042266
20.665377	1276.970563	13.047271
20.563207	1273.637848	13.052275
20.964933	1266.760644	13.057280
20.820401	1275.799207	13.062285
20.727380	1263.538608	13.067290
20.570891	1247.515708	13.072295
20.427341	1250.132130	13.077299
20.293057	1258.447521	13.082304
20.545225	1277.086528	13.087309
20.928603	1267.167645	13.092314
20.877796	1272.368350	13.097319
20.689526	1281.058255	13.102323
20.819919	1267.082397	13.107328
20.484347	1255.926617	13.112333
20.603808	1252.344069	13.117338
20.596727	1257.910779	13.122343
20.909961	1267.914846	13.127347
20.823919	1263.585983	13.132352
20.402267	1259.488865	13.137357
20.468523	1255.098651	13.142362
20.485798	1262.005961	13.147367
20.480789	1269.367880	13.152371
20.813739	1271.704855	13.157376
20.824890	1281.723207	13.162381
20.816265	1274.825500	13.167386
20.992565	1260.377869	13.172391
20.827640	1259.602981	13.177395
20.918891	1242.016299	13.182400
20.549375	1247.748058	13.187405
20.406914	1248.713866	13.192410
20.645415	1243.648780	13.197415
20.282292	1247.098238	13.202419
20.393415	1246.279321	13.207424
20.354795	1261.389394	13.212429
20.822821	1274.955115	13.217434
20.569017	1279.313695	13.222439
20.597803	1283.583043	13.227443
20.874596	1277.249362	13.232448
20.695268	1289.662186	13.237453
20.726686	1272.673273	13.242458
20.828734	1264.632652	13.247463
20.622423	1262.415004	13.252467
20.493679	1254.934801	13.257472
20.464137	1262.457552	13.262477
20.545246	1272.573559	13.267482
20.942568	1274.836394	13.272487
20.519309	1267.005729	13.277491
20.772931	1264.937092	13.282496
20.367472	1270.848076	13.287501
20.514043	1266.900043	13.292506
20.836670	1268.840444	13.297511
20.372994	1285.239021	13.302515
20.630614	1280.812756	13.307520
20.545426	1287.526666	13.312525
20.704553	1285.527509	13.317530
20.702926	1284.064187	13.322535
20.500346	1282.362445	13.327539
20.816573	1281.662213	13.332544
20.485224	1285.081379	13.337549
20.647663	1286.699581	13.342554
20.846141	1284.292773	13.347559
20.495545	1295.901784	13.352563
21.004309	1289.689597	13.357568
20.955162	1288.673869	13.362573
20.875673	1271.947886	13.367578
20.785864	1263.456850	13.372583
20.767182	1255.759587	13.377587
20.621228	1242.279672	13.382592
20.743074	1249.887879	13.387597
20.486308	1243.928716	13.392602
20.769747	1244.795837	13.397607
20.514995	1257.991080	13.402611
20.669119	1253.702768	13.407616
20.450134	1260.819666	13.412621
20.448403	1248.410465	13.417626
20.437778	1249.477470	13.422631
20.028963	1261.708445	13.427635
20.860087	1266.700661	13.432640
20.760923	1283.487416	13.437645
20.969327	1284.547875	13.442650
20.809154	1285.208186	13.447655
20.501808	1265.829585	13.452659
20.795865	1270.346805	13.457664
20.651285	1262.186235	13.462669
20.695260	1259.480769	13.467674
20.354206	1262.800543	13.472679
20.593354	1274.025282	13.477683
20.903904	1278.227607	13.482688
20.614999	1272.851568	13.487693
20.715297	1263.761662	13.492698
20.670564	1254.825006	13.497703
20.453839	1263.450835	13.502707
20.711078	1258.368560	13.507712
20.518204	1267.866670	13.512717
20.911389	1273.930992	13.517722
20.694654	1267.768296	13.522727
20.355536	1266.920258	13.527731
20.857505	1264.834088	13.532736
20.640683	1267.438544	13.537741
20.600830	1264.677843	13.542746
20.647783	1272.264099	13.547751
20.716721	1273.680362	13.552755
20.815142	1261.266214	13.557760
20.717043	1269.037259	13.562765
20.893730	1261.404245	13.567770
20.825222	1258.883105	13.572775
20.452614	1266.831987	13.577779
20.667427	1255.713798	13.582784
20.440924	1265.584736	13.587789
20.479722	1263.320895	13.592794
20.615139	1263.937211	13.597799
20.418773	1267.623453	13.602803
20.809029	1262.087045	13.607808
20.438024	1271.309977	13.612813
20.817043	1276.631377	13.617818
20.786091	1272.720332	13.622823
20.333191	1277.726528	13.627827
20.757770	1270.764457	13.632832
20.451546	1279.294173	13.637837
20.572504	1290.715202	13.642842
20.604462	1291.412683	13.647847
20.816077	1298.710100	13.652851
21.000601	1291.539491	13.657856
20.328373	1274.800018	13.662861
20.653912	1276.027892	13.667866
20.849785	1280.037176	13.672871
20.717519	1279.126178	13.677875
21.067676	1259.093877	13.682880
20.760140	1265.907904	13.687885
20.669531	1259.862301	13.692890
20.709863	1256.508437	13.697895
20.550946	1266.369384	13.702899
20.876566	1260.074447	13.707904
20.260231	1272.146124	13.712909
20.489944	1270.526045	13.717914
20.635158	1259.998540	13.722919
20.542402	1273.243659	13.727923
20.850222	1270.478758	13.732928
20.878890	1267.526549	13.737933
20.712265	1265.626666	13.742938
20.894672	1262.898330	13.747943
20.828577	1264.121643	13.752947
21.216284	1255.048195	13.757952
20.784101	1264.437014	13.762957
20.611503	1266.654333	13.767962
20.664861	1267.003012	13.772967
20.983775	1273.335461	13.777971
20.831856	1267.660004	13.782976
20.773536	1271.906969	13.787981
20.445348	1275.469933	13.792986
20.548457	1274.458308	13.797991
20.745818	1277.445389	13.802995
20.979617	1269.636087	13.808000
20.610699	1264.593756	13.813005
20.650239	1259.971235	13.818010
20.582480	1246.445725	13.823015
20.455053	1260.409214	13.828019
21.046298	1269.862687	13.833024
20.726115	1262.530508	13.838029
20.575961	1245.544565	13.843034
20.499004	1250.889796	13.848039
20.536343	1255.770477	13.853043
20.983241	1263.106049	13.858048
20.871414	1257.134802	13.863053
20.375261	1251.187797	13.868058
20.733935	1250.323874	13.873063
20.504061	1257.900656	13.878067
20.799252	1247.129233	13.883072
20.589778	1248.470041	13.888077
20.511934	1250.225134	13.893082
20.574537	1250.136269	13.898087
20.544761	1254.313226	13.903091
20.733074	1264.841890	13.908096
20.680100	1263.456942	13.913101
20.631793	1256.233593	13.918106
20.980914	1251.340900	13.923111
20.699913	1247.558852	13.928115
20.800928	1250.953205	13.933120
20.467389	1247.820631	13.938125
20.475196	1245.634283	13.943130
20.339308	1250.212189	13.948135
20.545524	1261.987062	13.953139
20.833815	1270.307605	13.958144
20.560888	1272.797208	13.963149
20.586052	1273.919224	13.968154
21.176072	1279.061876	13.973159
20.796174	1270.915180	13.978163
20.921080	1262.784962	13.983168
20.815432	1256.085684	13.988173
20.669797	1260.626508	13.993178
21.166507	1256.641555	13.998183
20.512517	1252.977352	14.003187
20.684906	1248.155432	14.008192
20.767306	1257.560574	14.013210
20.774781	1262.003316	14.018227
20.789676	1260.126588	14.023245
20.822358	1253.448336	14.028263
21.191135	1251.891130	14.033280
20.715618	1258.444905	14.038298
20.827188	1256.521296	14.043315
20.933949	1247.118451	14.048333
21.098660	1245.892680	14.053351
20.770266	1232.566773	14.058368
20.647950	1235.551515	14.063386
20.549866	1247.347937	14.068403
20.692037	1240.897627	14.073421
20.807359	1254.207141	14.078439
20.912269	1250.069695	14.083456
20.936648	1264.585334	14.088474
20.928658	1262.928555	14.093491
20.850673	1259.038938	14.098509
20.701258	1268.627091	14.103527
20.958805	1257.174843	14.108544
20.889765	1261.880697	14.113562
20.604735	1261.606800	14.118579
20.755546	1255.600288	14.123597
20.627187	1251.743091	14.128615
21.044782	1247.588020	14.133632
21.009404	1264.047293	14.138650
21.145784	1262.679743	14.143667
21.104968	1265.228332	14.148685
21.264815	1284.908839	14.153703
21.207570	1276.665542	14.158720
20.959936	1282.486104	14.163738
20.740573	1282.387357	14.168755
21.175093	1283.353115	14.173773
21.018651	1291.282013	14.178791
21.281880	1285.987470	14.183808
21.023196	1292.553080	14.188826
20.973987	1288.131095	14.193843
21.343337	1278.322963	14.198861
21.075001	1295.821484	14.203879
21.303266	1278.286046	14.208896
21.527055	1285.989906	14.213914
21.052830	1294.276245	14.218931
21.102218	1285.665923	14.223949
20.871056	1297.291696	14.228967
20.971559	1320.750833	14.233984
21.248908	1330.978061	14.239002
21.417998	1329.271006	14.244019
21.535625	1319.400746	14.249037
21.237151	1333.341073	14.254055
21.634767	1326.237263	14.259072
21.446027	1336.341414	14.264090
21.348458	1331.361603	14.269107
21.667442	1322.805003	14.274125
21.308002	1319.602870	14.279143
21.597606	1322.336302	14.284160
21.298716	1327.063107	14.289178
21.009040	1332.596226	14.294195
21.553041	1338.724714	14.299213
21.526618	1367.456725	14.304231
21.514988	1361.470573	14.309248
21.782045	1360.222177	14.314266
21.634038	1360.291380	14.319283
21.986564	1347.675553	14.324301
21.798432	1364.242678	14.329319
22.028041	1349.593568	14.334336
22.045103	1359.200061	14.339354
22.044704	1352.192757	14.344371
22.340775	1352.515973	14.349389
21.801707	1340.913858	14.354407
22.337287	1333.964224	14.359424
21.905085	1332.718034	14.364442
21.671744	1331.646200	14.369459
21.924356	1326.443788	14.374477
21.611286	1332.965393	14.379495
22.232868	1339.681641	14.384512
22.257680	1352.311161	14.389530
21.871817	1343.609773	14.394547
22.525513	1337.355482	14.399565
22.018562	1338.616137	14.404583
22.041746	1331.563395	14.409600
21.900545	1336.087292	14.414618
21.836260	1340.972531	14.419635
22.115399	1349.719994	14.424653
21.971597	1353.263489	14.429671
22.441531	1344.875502	14.434688
22.267102	1349.292227	14.439706
22.288152	1357.777254	14.444723
22.467918	1349.740728	14.449741
22.537805	1358.062229	14.454759
22.051148	1349.494111	14.459776
22.295013	1344.009145	14.464794
21.952895	1355.165789	14.469811
22.032213	1347.968013	14.474829
22.133290	1359.483424	14.479847
22.368415	1357.397729	14.484864
22.550565	1351.900581	14.489882
22.418477	1348.768361	14.494899
22.954147	1352.761925	14.499917
22.585040	1351.895797	14.504935
22.624949	1355.187396	14.509952
22.586394	1356.771334	14.514970
22.784796	1354.952631	14.519987
22.804198	1345.017793	14.525005
22.483451	1337.326173	14.530023
22.280502	1335.734303	14.535040
22.462242	1340.703788	14.540058
22.484461	1353.570474	14.545075
22.692745	1351.546479	14.550093
22.713522	1362.906380	14.555111
22.491501	1360.678874	14.560128
22.798830	1358.711442	14.565146
22.889747	1359.779991	14.570163
22.559751	1353.798217	14.575181
22.646930	1360.530498	14.580199
22.738357	1362.057523	14.585216
22.751388	1363.003996	14.590234
22.569087	1369.503973	14.595251
22.916063	1359.147986	14.600269
22.642028	1359.434714	14.605287
22.659856	1362.957936	14.610304
22.891593	1358.624044	14.615322
22.791592	1356.096279	14.620339
22.531865	1364.238327	14.625357
22.603533	1368.630749	14.630375
22.426381	1371.020196	14.635392
22.600614	1384.902478	14.640410
22.441467	1395.698045	14.645427
23.057701	1394.526091	14.650445
22.640975	1401.820133	14.655463
22.735901	1406.659550	14.660480
23.028029	1399.423085	14.665498
22.868073	1407.751387	14.670515
23.016073	1403.546461	14.675533
23.040536	1401.937975	14.680551
23.000022	1412.643057	14.685568
23.461516	1417.049610	14.690586
23.357264	1418.500882	14.695603
23.364145	1410.307845	14.700621
23.255970	1404.167968	14.705639
22.996284	1403.632824	14.710656
23.231694	1412.191449	14.715674
23.348620	1420.614814	14.720691
23.788828	1420.356590	14.725709
23.434913	1408.774441	14.730727
23.292200	1404.511273	14.735744
23.597444	1395.861649	14.740762
23.349105	1402.742638	14.745779
23.600387	1395.868997	14.750797
23.624918	1390.466978	14.755815
23.175739	1396.477827	14.760832
23.319634	1392.341202	14.765850
23.392186	1397.856683	14.770867
23.552715	1417.738618	14.775885
23.661455	1423.797349	14.780903
23.682543	1422.381317	14.785920
23.876904	1400.847601	14.790938
23.480110	1405.011147	14.795955
23.709500	1390.699460	14.800973
23.517325	1394.928685	14.805991
23.268825	1395.902717	14.811008
23.877599	1406.038594	14.816026
23.886695	1415.409643	14.821043
23.439689	1420.587986	14.826061
23.702082	1420.259019	14.831079
23.799453	1422.626711	14.836096
24.461804	1418.039278	14.841114
23.866969	1418.316611	14.846131
23.937635	1402.078800	14.851149
23.925797	1391.485853	14.856167
23.724990	1395.257897	14.861184
23.693815	1395.505102	14.866202
23.464191	1406.024828	14.871219
24.047647	1420.066825	14.876237
23.798591	1416.958753	14.881255
23.702317	1424.780594	14.886272
23.935002	1414.090424	14.891290
23.601420	1429.534032	14.896307
23.596342	1418.541993	14.901325
23.883788	1418.401734	14.906343
23.808851	1430.810481	14.911360
23.916907	1421.909923	14.916378
24.025439	1429.515833	14.921395
23.972469	1443.095406	14.926413
24.242027	1450.371248	14.931431
24.208406	1454.323504	14.936448
24.619163	1449.471009	14.941466
24.231396	1451.028070	14.946483
24.517774	1446.355871	14.951501
24.453796	1426.161133	14.956519
24.161109	1421.479840	14.961536
24.089421	1417.891212	14.966554
24.210424	1431.212566	14.971571
24.536178	1451.787101	14.976589
24.560109	1448.524576	14.981607
24.344478	1436.609660	14.986624
24.786975	1423.044996	14.991642
24.698085	1423.368264	14.996659
24.622993	1410.170900	15.001677
24.519441	1406.868154	15.006695
24.203658	1413.799233	15.011712
24.176652	1416.342499	15.016730
24.597971	1428.712205	15.021747
24.703073	1429.211394	15.026765
24.560221	1425.157464	15.031783
24.395696	1446.558202	15.036800
24.856758	1441.781061	15.041818
24.511441	1452.852555	15.046835
25.064998	1442.063205	15.051853
25.221992	1432.848865	15.056871
24.797057	1420.576431	15.061888
24.973381	1402.992497	15.066906
24.597450	1416.148483	15.071923
24.655100	1412.249775	15.076941
24.845392	1407.957874	15.081959
24.969931	1403.617471	15.086976
25.296996	1402.519169	15.091994
24.824635	1405.499214	15.097011
24.839013	1408.097228	15.102029
25.044256	1409.455874	15.107047
24.940698	1414.775284	15.112064
25.085555	1403.031783	15.117082
25.093099	1406.139784	15.122099
25.009030	1409.003625	15.127117
25.112210	1403.799851	15.132135
24.756199	1407.692612	15.137152
24.984776	1404.459593	15.142170
25.083456	1409.767195	15.147187
24.927945	1411.356422	15.152205
25.274794	1408.585120	15.157223
25.154963	1409.028159	15.162240
25.107545	1404.351798	15.167258
25.145263	1413.424111	15.172275
24.943928	1413.073151	15.177293
25.286377	1423.120952	15.182311
25.181081	1434.766085	15.187328
25.618408	1431.499765	15.192346
25.381039	1427.907671	15.197363
25.209322	1415.903966	15.202381
25.433772	1420.155625	15.207399
25.497645	1438.822842	15.212416
25.577425	1421.082816	15.217434
25.172138	1425.801454	15.222451
25.015982	1428.367682	15.227469
25.774941	1437.387108	15.232487
25.412445	1442.489055	15.237504
25.695417	1436.827135	15.242522
25.690094	1440.973084	15.247539
25.323069	1444.322531	15.252557
25.548396	1439.863790	15.257575
25.238336	1443.042908	15.262592
25.508712	1440.468637	15.267610
25.782477	1448.757672	15.272627
25.769104	1444.179692	15.277645
26.072602	1436.953194	15.282663
25.484659	1441.545233	15.287680
25.885722	1440.312424	15.292698
25.791885	1438.286267	15.297715
25.881680	1447.210289	15.302733
25.673096	1441.843073	15.307751
25.803432	1439.796105	15.312768
26.084825	1448.834293	15.317786
25.833527	1446.655489	15.322803
25.861078	1451.444316	15.327821
25.934889	1437.827541	15.332839
26.097600	1448.254830	15.337856
25.998219	1443.553709	15.342874
25.908983	1445.631042	15.347891
25.682016	1449.658182	15.352909
25.975718	1444.968299	15.357927
25.875262	1445.587583	15.362944
26.072035	1437.630884	15.367962
25.768726	1449.037825	15.372979
26.074436	1442.151548	15.377997
26.392557	1429.997338	15.383015
26.074764	1444.890219	15.388032
25.933277	1437.535700	15.393050
26.066225	1441.375649	15.398067
26.298822	1461.589086	15.403085
26.506130	1462.282770	15.408103
26.025011	1457.605564	15.413120
26.065697	1463.413245	15.418138
26.044494	1464.547665	15.423155
26.270623	1472.410921	15.428173
26.410027	1459.085700	15.433191
26.262848	1467.738417	15.438208
26.346511	1467.496948	15.443226
26.636527	1469.623911	15.448243
26.435320	1472.765223	15.453261
26.742415	1474.858000	15.458279
26.531755	1475.094508	15.463296
26.674100	1468.390013	15.468314
26.494497	1472.023407	15.473331
26.184591	1466.351430	15.478349
26.821379	1464.827750	15.483367
26.594338	1471.426148	15.488384
26.505197	1464.745207	15.493402
26.777831	1456.292668	15.498419
26.852799	1463.072564	15.503437
27.162969	1455.585430	15.508455
26.916137	1461.404361	15.513472
27.059999	1452.400540	15.518490
27.362171	1457.032303	15.523507
27.070473	1470.531211	15.528525
26.983802	1446.570903	15.533543
26.825994	1444.253700	15.538560
26.636985	1435.067017	15.543578
27.348831	1444.109694	15.548595
26.837602	1450.594528	15.553613
27.147633	1435.934077	15.558631
26.885748	1441.178859	15.563648
26.957932	1439.871872	15.568666
26.973688	1446.535356	15.573683
26.883658	1467.043305	15.578701
26.781097	1463.467454	15.583719
27.039488	1465.520806	15.588736
26.756016	1462.864975	15.593754
27.133368	1458.186128	15.598771
26.978431	1457.671242	15.603789
27.041118	1460.909680	15.608807
26.776499	1465.375433	15.613824
27.080473	1466.045047	15.618842
27.520361	1477.367292	15.623859
27.034085	1481.728398	15.628877
27.318300	1487.725345	15.633895
27.326108	1495.356795	15.638912
27.184775	1497.611554	15.643930
27.515464	1493.491514	15.648947
27.415007	1499.033055	15.653965
27.739545	1489.467110	15.658983
27.680487	1496.272332	15.664000
27.689744	1489.402642	15.669018
27.608084	1493.534826	15.674035
27.339252	1506.843706	15.679053
27.493938	1490.055179	15.684071
27.849568	1494.909674	15.689088
27.674528	1495.319835	15.694106
28.010872	1485.095236	15.699123
27.582905	1473.712045	15.704141
27.796194	1460.424591	15.709159
27.314056	1465.898791	15.714176
27.421158	1473.213928	15.719194
27.687852	1486.070839	15.724211
27.953825	1496.328315	15.729229
27.888333	1489.500437	15.734247
27.607444	1490.312891	15.739264
27.649350	1496.733116	15.744282
27.801411	1493.767912	15.749299
27.825268	1496.771079	15.754317
27.810656	1487.917575	15.759335
27.678842	1491.746283	15.764352
27.705213	1486.019088	15.769370
28.340172	1489.737291	15.774387
28.243378	1502.034749	15.779405
28.246712	1491.832585	15.784423
27.988727	1498.549195	15.789440
27.986657	1502.688350	15.794458
28.248705	1489.360057	15.799475
27.735819	1497.119392	15.804493
28.081245	1494.054130	15.809511
27.998486	1499.851625	15.814528
28.251730	1508.476680	15.819546
28.097231	1512.219344	15.824563
28.256274	1518.364477	15.829581
28.631074	1513.866141	15.834599
28.425742	1517.100934	15.839616
28.186375	1517.757322	15.844634
28.666161	1511.704526	15.849651
28.081656	1528.298090	15.854669
28.366389	1518.746340	15.859687
28.293383	1524.534424	15.864704
28.465025	1520.204564	15.869722
28.521843	1520.029515	15.874739
28.401897	1526.794909	15.879757
28.273867	1516.273890	15.884775
28.412346	1512.967911	15.889792
28.142062	1528.475464	15.894810
28.290698	1527.006829	15.899827
28.418476	1548.528630	15.904845
28.583333	1545.865773	15.909863
28.869755	1549.753635	15.914880
28.720444	1553.018041	15.919898
28.954674	1547.383518	15.924915
28.936801	1547.163749	15.929933
28.761188	1543.516942	15.934951
29.065979	1547.877741	15.939968
29.044504	1545.730696	15.944986
29.163209	1540.390683	15.950003
29.061190	1550.758805	15.955021
29.263606	1546.564822	15.960039
28.985584	1547.951009	15.965056
28.889154	1548.619995	15.970074
29.245817	1537.147786	15.975091
29.032438	1540.266670	15.980109
29.226374	1545.231135	15.985127
29.216397	1544.122084	15.990144
29.207549	1532.688514	15.995162
29.244898	1530.016895	16.000179
29.147328	1525.029152	16.005197
29.100323	1527.108413	16.010215
29.212440	1532.980237	16.015232
29.485631	1544.612283	16.020250
29.595916	1533.571080	16.025267
29.111240	1529.344327	16.030285
29.433000	1527.686835	16.035303
29.454354	1527.099781	16.040320
29.052962	1536.972920	16.045338
29.405073	1542.243294	16.050355
29.463974	1540.143995	16.055373
29.500498	1538.722343	16.060391
29.658573	1545.105970	16.065408
29.422350	1545.919168	16.070426
30.036543	1534.351613	16.075443
29.433601	1540.722119	16.080461
29.331952	1540.684036	16.085479
29.786195	1540.112883	16.090496
29.605974	1544.676103	16.095514
29.631659	1544.911096	16.100531
29.529544	1546.809589	16.105549
29.302680	1543.287368	16.110567
29.621086	1544.248856	16.115584
29.440145	1540.059389	16.120602
29.985934	1534.918687	16.125619
29.768826	1544.916603	16.130637
29.611224	1545.975252	16.135655
29.852098	1552.425904	16.140672
29.877879	1569.744126	16.145690
30.165833	1565.162880	16.150707
30.184203	1575.250680	16.155725
30.153057	1561.913240	16.160743
29.836570	1562.507994	16.165760
29.984819	1575.166786	16.170778
30.245958	1581.679503	16.175795
30.230744	1578.661520	16.180813
29.910160	1571.926990	16.185831
30.258964	1566.213620	16.190848
30.224689	1573.615069	16.195866
30.404489	1570.464517	16.200883
30.204453	1573.054286	16.205901
30.372502	1572.942510	16.210919
30.131610	1575.904546	16.215936
30.086804	1574.650815	16.220954
30.499019	1563.926394	16.225971
30.394028	1566.489204	16.230989
30.183280	1579.156493	16.236007
30.199784	1572.380782	16.241024
30.507795	1573.099312	16.246042
30.247064	1576.586786	16.251059
30.090636	1582.017730	16.256077
30.099700	1582.824056	16.261095
30.497295	1584.405310	16.266112
30.271024	1608.285142	16.271130
30.444366	1606.306801	16.276147
30.902415	1614.741941	16.281165
30.679691	1618.479782	16.286183
30.823887	1608.976345	16.291200
30.736343	1614.637788	16.296218
31.005391	1599.326146	16.301235
30.743329	1604.827433	16.306253
30.742661	1608.073649	16.311271
31.091092	1607.850513	16.316288
30.599352	1606.934709	16.321306
30.866873	1608.703464	16.326323
30.699534	1606.053466	16.331341
30.613122	1606.308699	16.336359
30.894829	1607.503362	16.341376
30.574678	1609.954983	16.346394
30.932090	1613.352525	16.351411
30.993469	1625.958360	16.356429
30.912632	1637.456599	16.361447
31.346634	1626.951254	16.366464
31.069753	1636.445142	16.371482
31.138206	1629.720111	16.376499
31.434954	1629.047439	16.381517
31.219730	1628.804087	16.386535
31.281288	1632.524119	16.391552
30.994020	1631.915495	16.396570
31.403843	1628.510365	16.401587
31.623967	1623.334268	16.406605
31.687175	1625.786885	16.411623
31.811767	1622.606586	16.416640
31.760525	1627.411185	16.421658
31.856971	1621.343190	16.426675
31.651516	1611.219866	16.431693
31.254079	1606.476563	16.436711
31.854102	1610.239700	16.441728
31.746906	1613.680671	16.446746
31.608193	1602.112808	16.451763
31.538457	1607.865008	16.456781
31.639074	1616.398061	16.461799
31.963948	1616.184188	16.466816
31.558318	1630.006600	16.471834
31.731769	1624.172516	16.476851
31.592787	1627.779805	16.481869
31.817677	1621.537158	16.486887
31.977444	1624.131686	16.491904
31.843377	1622.752180	16.496922
32.185036	1620.488212	16.501939
31.845856	1618.541277	16.506957
32.021889	1622.332715	16.511975
31.969886	1617.214969	16.516992
31.720036	1631.283898	16.522010
31.723669	1629.243741	16.527027
31.767782	1628.631816	16.532045
31.780984	1624.397987	16.537063
31.773711	1619.192090	16.542080
31.710670	1627.107058	16.547098
31.825627	1642.217425	16.552115
31.999201	1659.579825	16.557133
31.719155	1659.101404	16.562151
32.076806	1657.219509	16.567168
32.115357	1657.650665	16.572186
32.101757	1654.645781	16.577203
32.470283	1663.361873	16.582221
32.216130	1675.336914	16.587239
32.702840	1682.195967	16.592256
32.490662	1677.334998	16.597274
32.577779	1663.251031	16.602291
32.490405	1668.654474	16.607309
32.782314	1672.856121	16.612327
32.662569	1667.005073	16.617344
32.450857	1660.207516	16.622362
32.664031	1676.640195	16.627379
32.948723	1678.241828	16.632397
32.776267	1667.342369	16.637415
32.820408	1656.843339	16.642432
32.872180	1661.854902	16.647450
32.777390	1652.651481	16.652467
33.038489	1648.158655	16.657485
32.583350	1648.384605	16.662503
32.992392	1659.706407	16.667520
32.961894	1681.075099	16.672538
33.090875	1671.247625	16.677555
32.870861	1665.950579	16.682573
33.112522	1673.681685	16.687591
33.077729	1674.483999	16.692608
32.879506	1685.396132	16.697626
32.978956	1679.699679	16.702643
33.034329	1680.486826	16.707661
32.917043	1679.523877	16.712679
33.370375	1676.660032	16.717696
33.229259	1685.959253	16.722714
33.168452	1686.797180	16.727731
33.559228	1687.648815	16.732749
33.039677	1680.861807	16.737767
33.247929	1682.603056	16.742784
33.259907	1680.225698	16.747802
33.162589	1677.311245	16.752819
33.155087	1674.913398	16.757837
32.969072	1684.557215	16.762855
33.374094	1692.127772	16.767872
33.592884	1703.746598	16.772890
33.512021	1714.050896	16.777907
34.003283	1706.637792	16.782925
33.683666	1704.576031	16.787943
33.816282	1681.857743	16.792960
33.465552	1690.019206	16.797978
33.773652	1689.384049	16.802995
33.981997	1683.602582	16.808013
33.582111	1687.480390	16.813031
33.913399	1683.709436	16.818048
34.001138	1677.299079	16.823066
33.783306	1674.848257	16.828083
34.161446	1671.464689	16.833101
34.029002	1678.699366	16.838119
34.004703	1674.677584	16.843136
33.838230	1686.707866	16.848154
33.654055	1684.947784	16.853171
34.090887	1688.628425	16.858189
34.216021	1716.625897	16.863207
34.250836	1703.028466	16.868224
34.072734	1690.835989	16.873242
33.999478	1704.382073	16.878259
34.208362	1703.936572	16.883277
34.213592	1710.553090	16.888295
34.049809	1704.968617	16.893312
34.183465	1713.901538	16.898330
34.483062	1713.845863	16.903347
34.404383	1702.380824	16.908365
34.126589	1716.941176	16.913383
34.557585	1703.621924	16.918400
34.416746	1710.039927	16.923418
34.423832	1716.304557	16.928435
34.739158	1703.492211	16.933453
34.401014	1714.731870	16.938471
34.658707	1710.482617	16.943488
34.762783	1716.239387	16.948506
34.734844	1712.808886	16.953523
35.018819	1713.042799	16.958541
34.435670	1716.462960	16.963559
34.809871	1705.514036	16.968576
34.703149	1709.464648	16.973594
34.756171	1706.430249	16.978611
34.989154	1713.777344	16.983629
34.768567	1713.036949	16.988647
34.617990	1709.595333	16.993664
34.773862	1703.328264	16.998682
34.676644	1710.105850	17.003699
35.002469	1704.769710	17.008717
34.699006	1706.534374	17.013735
35.027074	1707.646141	17.018752
35.636637	1722.824003	17.023770
35.475144	1708.844930	17.028787
36.032987	1691.630048	17.033805
35.473692	1693.360791	17.038823
35.374022	1684.163634	17.043840
35.463921	1690.480328	17.048858
35.278516	1688.118720	17.053875
35.741581	1685.287143	17.058893
35.657385	1692.025675	17.063911
35.528243	1688.102414	17.068928
35.765077	1687.153774	17.073946
35.613369	1664.502885	17.078963
35.620025	1660.343240	17.083981
35.419088	1649.519913	17.088999
35.494786	1652.740587	17.094016
35.362899	1652.975544	17.099034
35.424650	1661.329980	17.104051
35.656496	1670.400593	17.109069
35.509636	1681.015862	17.114087
35.522620	1677.113982	17.119104
35.863141	1676.589281	17.124122
35.740333	1683.988389	17.129139
35.525234	1673.699807	17.134157
35.605727	1689.345863	17.139175
35.760418	1682.408838	17.144192
35.863916	1681.659229	17.149210
35.850342	1687.230245	17.154227
36.006037	1673.848743	17.159245
35.621267	1686.813673	17.164263
35.692182	1675.128940	17.169280
35.750358	1691.362189	17.174298
36.043065	1705.441400	17.179315
36.332691	1706.962807	17.184333
36.310299	1711.125713	17.189351
36.243129	1706.834675	17.194368
36.556106	1709.894026	17.199386
36.341871	1699.525058	17.204403
36.180265	1683.255550	17.209421
36.320790	1691.629688	17.214439
36.244719	1706.978243	17.219456
36.660791	1700.282684	17.224474
36.294845	1708.104428	17.229491
36.532974	1705.197819	17.234509
36.507722	1708.772043	17.239527
36.500022	1711.596232	17.244544
36.510399	1717.796625	17.249562
36.089270	1709.548195	17.254579
36.455627	1706.798898	17.259597
36.209127	1713.320278	17.264615
36.399609	1712.456899	17.269632
36.564555	1708.443465	17.274650
36.483664	1715.095745	17.279667
36.428007	1726.586892	17.284685
36.729109	1743.948718	17.289703
36.910781	1739.205819	17.294720
36.858383	1745.760753	17.299738
36.475597	1752.022296	17.304755
37.017005	1743.717860	17.309773
36.743912	1748.686880	17.314791
36.752350	1746.748980	17.319808
36.707278	1742.203492	17.324826
37.029937	1747.824730	17.329843
37.122942	1740.822793	17.334861
36.938444	1765.389971	17.339879
37.126091	1765.132700	17.344896
37.388409	1771.112807	17.349914
37.162685	1780.609640	17.354931
37.149271	1773.631740	17.359949
37.160793	1773.176028	17.364967
37.027309	1783.212682	17.369984
36.985714	1772.166420	17.375002
37.073980	1776.037969	17.380019
37.276064	1776.057627	17.385037
37.223626	1782.671576	17.390055
37.301104	1788.119562	17.395072
37.799258	1804.743691	17.400090
37.630178	1810.871279	17.405107
37.814301	1812.262436	17.410125
37.748936	1801.542437	17.415143
37.957895	1805.916241	17.420160
37.763303	1787.933219	17.425178
37.621436	1788.519007	17.430195
38.138317	1789.077596	17.435213
37.932043	1777.718584	17.440231
37.959330	1782.912646	17.445248
38.082742	1765.530211	17.450266
37.768610	1774.833487	17.455283
38.320615	1783.708378	17.460301
38.009488	1776.152638	17.465319
37.900098	1774.295667	17.470336
38.144667	1787.478082	17.475354
38.393572	1789.171172	17.480371
38.477242	1784.006557	17.485389
38.087959	1770.569520	17.490407
38.282290	1767.571563	17.495424
38.404182	1767.260281	17.500442
37.973044	1780.320784	17.505459
38.335918	1781.626794	17.510477
38.449152	1784.589022	17.515495
38.481660	1788.025842	17.520512
38.701212	1787.426830	17.525530
38.414352	1798.481395	17.530547
38.447818	1784.468007	17.535565
38.231963	1802.392163	17.540583
38.283440	1799.240006	17.545600
38.582616	1793.682339	17.550618
38.218236	1797.893524	17.555635
38.480152	1787.256626	17.560653
38.486850	1796.570883	17.565671
38.658163	1803.835044	17.570688
38.793204	1806.985722	17.575706
39.058902	1823.848311	17.580723
39.148127	1822.574755	17.585741
39.003218	1817.922462	17.590759
38.797844	1813.811536	17.595776
39.219484	1812.230112	17.600794
38.756370	1810.969929	17.605811
38.780838	1816.742582	17.610829
39.117526	1815.884981	17.615847
38.759452	1825.306204	17.620864
39.194847	1817.651825	17.625882
38.957894	1825.699254	17.630899
38.815944	1825.177563	17.635917
38.936201	1819.960692	17.640935
38.861408	1828.447122	17.645952
39.259101	1836.073198	17.650970
38.831568	1846.127691	17.655987
38.889913	1858.415649	17.661005
39.351638	1857.632492	17.666023
39.257879	1854.243919	17.671040
39.452983	1858.690740	17.676058
39.364898	1857.780541	17.681075
39.612303	1849.441921	17.686093
39.628938	1859.699308	17.691111
39.485556	1865.037819	17.696128
39.854179	1861.332444	17.701146
39.865339	1861.425029	17.706163
39.673831	1858.455558	17.711181
40.084681	1873.227151	17.716199
39.809011	1875.937583	17.721216
39.932258	1876.037461	17.726234
40.032486	1895.015668	17.731251
40.037700	1883.194945	17.736269
40.161150	1882.988026	17.741287
39.843386	1890.403388	17.746304
40.397993	1870.734698	17.751322
40.002473	1875.354384	17.756339
39.948183	1878.618651	17.761357
40.073033	1883.673695	17.766375
40.114184	1888.784566	17.771392
40.393962	1878.165204	17.776410
40.342755	1885.373654	17.781427
40.237250	1885.010542	17.786445
40.362712	1879.293345	17.791463
40.137728	1879.048398	17.796480
40.373489	1869.893586	17.801498
39.971295	1880.932785	17.806515
40.383223	1871.919774	17.811533
40.130694	1886.333108	17.816551
40.468321	1897.594909	17.821568
40.812731	1902.272780	17.826586
41.015992	1909.133891	17.831603
41.081262	1910.929436	17.836621
41.341494	1906.544432	17.841639
40.845917	1894.153862	17.846656
41.191442	1877.454011	17.851674
40.927628	1879.427106	17.856691
41.052013	1879.033620	17.861709
41.057183	1872.203730	17.866727
40.994745	1885.351823	17.871744
41.055610	1872.900838	17.876762
40.840031	1871.940181	17.881779
41.159912	1874.403030	17.886797
41.470091	1862.030276	17.891815
41.092966	1875.694203	17.896832
41.395146	1875.439900	17.901850
41.117687	1877.164253	17.906867
40.762938	1879.080273	17.911885
40.876754	1877.470855	17.916903
41.087808	1897.137732	17.921920
41.023591	1905.598136	17.926938
41.232505	1911.277695	17.931955
41.400626	1912.308802	17.936973
41.621898	1901.727071	17.941991
40.985051	1912.622022	17.947008
41.552791	1903.830338	17.952026
41.740056	1910.314084	17.957043
41.636716	1907.901595	17.962061
41.628899	1909.671828	17.967079
41.572170	1917.862036	17.972096
41.856865	1926.871680	17.977114
41.855708	1934.550411	17.982131
41.867015	1936.882360	17.987149
42.168796	1927.389765	17.992167
41.983405	1938.532080	17.997184
42.039309	1933.596802	18.002202
42.139972	1930.996816	18.007219
41.996958	1932.081481	18.012237
42.109165	1932.912278	18.017255
42.253250	1933.441451	18.022272
42.285204	1926.642660	18.027290
42.433712	1931.546858	18.032307
42.274303	1924.242144	18.037325
42.567652	1928.758267	18.042343
41.838188	1942.134718	18.047360
41.893748	1918.029817	18.052378
42.339942	1927.257542	18.057395
42.037450	1936.141390	18.062413
42.293015	1927.752656	18.067431
42.475344	1930.641754	18.072448
42.306176	1930.739504	18.077466
42.371103	1931.826400	18.082483
42.468640	1952.423101	18.087501
43.083024	1954.195570	18.092519
42.656010	1969.598801	18.097536
42.767022	1962.395668	18.102554
42.815408	1960.237419	18.107571
42.779154	1966.941687	18.112589
43.077387	1959.136065	18.117607
42.772438	1959.431665	18.122624
43.157987	1949.785684	18.127642
43.253703	1957.143784	18.132659
43.042221	1951.201064	18.137677
43.381741	1944.838529	18.142695
42.902290	1959.693216	18.147712
42.968104	1956.974503	18.152730
43.409673	1948.600139	18.157747
43.237713	1950.465776	18.162765
43.484471	1944.349290	18.167783
43.285760	1957.209271	18.172800
43.257035	1947.582958	18.177818
43.189139	1950.538714	18.182835
43.447985	1955.643990	18.187853
43.335338	1945.177626	18.192871
43.381460	1950.142208	18.197888
43.229539	1957.335294	18.202906
43.508570	1955.242515	18.207923
43.253863	1949.563115	18.212941
43.850913	1966.527977	18.217959
44.162465	1977.930078	18.222976
44.047300	1961.431036	18.227994
43.874501	1954.720736	18.233011
43.642989	1955.741647	18.238029
43.618744	1951.633256	18.243047
43.740469	1972.505363	18.248064
43.964049	1983.047608	18.253082
43.950653	1979.733498	18.258099
44.197248	1986.172420	18.263117
44.512468	1973.555714	18.268135
44.093051	1979.903427	18.273152
44.072759	1978.421576	18.278170
44.159571	1974.656506	18.283187
43.757561	1984.169001	18.288205
43.855168	1978.817249	18.293223
44.185331	1976.788676	18.298240
43.879726	1982.996318	18.303258
44.271005	1995.441307	18.308275
44.477094	2001.718368	18.313293
44.633185	2009.905360	18.318311
44.747298	2020.159898	18.323328
44.532701	2009.086776	18.328346
44.987638	2006.312284	18.333363
44.781003	2015.176172	18.338381
45.131524	1997.073699	18.343399
44.949699	1989.267542	18.348416
44.688464	1973.784448	18.353434
45.040279	1986.950726	18.358451
45.207306	1990.876630	18.363469
45.188060	1971.811396	18.368487
45.133166	1966.142595	18.373504
45.191406	1963.824672	18.378522
45.242935	1963.058953	18.383539
45.184022	1967.171124	18.388557
45.410438	1967.266347	18.393575
44.911688	1964.583403	18.398592
44.967726	1961.909511	18.403610
45.263867	1967.126830	18.408627
45.107427	1977.473258	18.413645
45.293965	1998.604075	18.418663
45.509532	1999.137581	18.423680
45.255283	1992.758820	18.428698
45.350034	1992.967073	18.433715
45.319597	1998.240423	18.438733
45.577656	1995.929954	18.443751
45.393103	1998.409565	18.448768
45.154024	2004.738751	18.453786
45.521451	1990.560992	18.458803
45.253209	1999.230186	18.463821
46.004432	2001.687187	18.468839
45.850367	2009.664075	18.473856
45.461786	2003.744074	18.478874
46.021268	2008.725122	18.483891
45.643320	2021.154381	18.488909
45.735838	2019.822076	18.493927
46.107702	2016.155476	18.498944
45.787207	2020.302303	18.503962
45.995053	2022.689443	18.508979
45.899861	2027.617597	18.513997
46.300787	2018.071375	18.519015
45.878726	2028.416155	18.524032
46.077922	2025.448047	18.529050
46.376013	2037.560266	18.534067
46.140785	2050.358506	18.539085
46.507857	2056.416416	18.544103
46.422436	2048.999942	18.549120
46.286159	2058.331664	18.554138
46.731772	2051.232437	18.559155
46.528080	2056.863020	18.564173
46.563938	2051.535248	18.569191
46.237670	2054.582575	18.574208
46.274013	2053.442500	18.579226
46.811369	2048.875602	18.584243
46.803408	2052.094763	18.589261
47.194318	2040.496353	18.594279
47.084822	2038.788815	18.599296
46.873843	2046.844021	18.604314
47.317598	2032.716975	18.609331
47.195108	2039.619090	18.614349
47.223152	2037.515203	18.619367
47.006361	2045.761688	18.624384
46.764098	2037.217890	18.629402
47.400900	2046.899827	18.634419
47.270924	2068.837135	18.639437
47.450816	2061.889619	18.644455
47.481273	2053.668863	18.649472
47.524980	2053.679173	18.654490
47.586119	2046.970062	18.659507
47.126603	2051.290881	18.664525
47.690618	2056.798234	18.669543
47.548551	2069.977285	18.674560
47.422487	2068.756923	18.679578
47.803671	2053.436361	18.684595
47.505485	2070.545703	18.689613
47.500917	2058.777526	18.694631
47.586575	2064.149585	18.699648
47.608176	2073.038460	18.704666
47.550109	2062.329690	18.709683
47.617104	2070.132129	18.714701
47.930746	2068.534868	18.719719
47.963878	2072.259547	18.724736
47.817570	2089.403681	18.729754
48.285648	2088.889301	18.734771
48.300122	2098.731883	18.739789
48.005396	2104.442291	18.744807
48.535144	2090.490255	18.749824
48.445268	2097.207068	18.754842
48.723327	2097.833654	18.759859
48.315847	2084.843648	18.764877
48.144173	2086.266408	18.769895
48.583668	2087.214130	18.774912
48.607908	2097.028410	18.779930
48.876190	2089.085124	18.784947
48.453133	2087.387475	18.789965
48.519712	2094.591401	18.794983
48.843988	2090.422665	18.800000
48.602201	2095.920900	18.805018
48.965378	2089.427889	18.810035
48.936742	2096.895564	18.815053
48.754162	2092.687319	18.820071
48.956737	2088.298872	18.825088
48.921903	2092.849298	18.830106
49.143218	2084.682249	18.835123
48.974070	2088.429755	18.840141
48.920271	2090.945948	18.845159
49.155253	2090.379073	18.850176
49.013283	2089.872320	18.855194
49.152796	2085.031419	18.860211
49.274129	2092.966789	18.865229
49.206342	2084.675946	18.870247
48.989571	2086.732808	18.875264
49.188879	2106.987063	18.880282
49.479870	2111.407657	18.885299
49.592663	2115.051208	18.890317
49.388449	2114.082428	18.895335
49.726780	2107.082878	18.900352
49.141649	2112.177299	18.905370
49.656784	2111.757669	18.910387
49.339997	2122.582061	18.915405
49.360168	2118.869272	18.920423
49.777920	2130.614812	18.925440
49.740620	2142.592617	18.930458
49.965664	2144.778814	18.935475
50.362161	2156.730706	18.940493
50.077979	2156.304839	18.945511
50.098884	2157.633964	18.950528
50.062877	2157.808800	18.955546
50.597519	2148.761103	18.960563
50.266089	2150.998298	18.965581
50.193758	2145.899340	18.970599
50.565366	2145.100653	18.975616
50.017661	2156.253724	18.980634
50.465663	2146.784863	18.985651
50.390657	2148.200864	18.990669
50.364388	2152.080555	18.995687
50.379392	2143.889744	19.000704
50.368813	2146.151278	19.005722
50.381666	2136.295604	19.010739
50.330011	2145.408585	19.015757
50.375078	2155.667939	19.020775
50.655883	2170.601377	19.025792
50.640670	2171.270022	19.030810
50.512600	2175.544306	19.035827
50.795720	2170.971511	19.040845
50.610167	2179.878545	19.045863
50.779340	2171.947875	19.050880
50.744962	2185.654175	19.055898
51.024781	2197.159047	19.060915
51.294465	2206.791095	19.065933
51.394135	2211.859709	19.070951
51.712704	2194.193929	19.075968
51.245354	2206.669854	19.080986
51.355140	2198.872923	19.086003
51.599926	2200.689429	19.091021
51.549525	2199.287084	19.096039
51.495820	2189.350745	19.101056
51.558222	2196.731585	19.106074
52.014964	2202.336336	19.111091
51.875870	2190.079797	19.116109
51.916469	2196.033303	19.121127
52.070032	2198.217537	19.126144
51.959230	2182.481329	19.131162
51.901993	2168.050201	19.136179
52.145749	2166.506553	19.141197
51.925581	2170.010507	19.146215
52.371030	2171.804444	19.151232
51.947152	2170.102983	19.156250
52.124614	2173.002345	19.161267
52.063185	2178.461620	19.166285
52.258829	2179.658261	19.171303
52.602588	2184.138895	19.176320
52.478699	2188.230813	19.181338
52.307468	2187.742882	19.186355
52.249447	2179.423684	19.191373
52.287475	2192.963484	19.196391
52.487951	2184.378090	19.201408
52.518604	2190.631299	19.206426
52.359377	2181.802798	19.211443
52.324125	2177.139192	19.216461
52.401060	2183.423559	19.221479
52.820894	2179.720951	19.226496
52.569832	2186.953559	19.231514
52.858519	2192.413633	19.236531
53.212721	2209.383691	19.241549
52.596028	2208.119645	19.246567
53.013477	2205.569770	19.251584
53.000236	2215.557651	19.256602
53.085988	2212.176547	19.261619
53.252813	2218.886298	19.266637
53.191749	2217.637464	19.271655
53.350559	2213.104934	19.276672
52.908110	2214.921713	19.281690
53.182298	2216.503846	19.286707
53.328859	2214.530483	19.291725
52.745077	2218.786216	19.296743
53.255997	2216.159291	19.301760
53.462451	2218.211597	19.306778
53.711102	2235.102555	19.311795
53.929865	2233.276566	19.316813
53.682318	2233.949232	19.321831
53.383123	2235.335709	19.326848
53.492213	2244.596165	19.331866
53.600985	2250.647371	19.336883
53.757648	2239.522726	19.341901
53.727689	2246.530530	19.346919
53.969631	2240.354909	19.351936
53.629359	2243.668802	19.356954
53.712980	2248.440296	19.361971
53.604148	2264.180093	19.366989
53.861184	2274.520566	19.372007
54.228364	2271.831603	19.377024
54.107393	2275.192333	19.382042
53.942335	2273.964800	19.387059
54.527394	2269.785885	19.392077
54.484391	2275.633982	19.397095
54.709071	2272.229919	19.402112
54.574697	2278.666018	19.407130
54.820238	2283.041212	19.412147
54.781584	2267.530171	19.417165
54.589848	2272.258277	19.422183
54.852817	2272.382284	19.427200
54.909216	2288.860326	19.432218
55.106045	2291.961139	19.437235
55.172379	2287.231741	19.442253
55.165807	2290.807061	19.447271
54.994305	2282.108672	19.452288
55.407207	2295.075918	19.457306
54.995723	2297.966979	19.462323
55.361330	2280.433608	19.467341
54.994258	2292.346928	19.472359
55.344192	2289.943887	19.477376
55.120928	2293.206879	19.482394
54.887283	2290.045029	19.487411
55.184310	2286.569643	19.492429
55.196443	2285.189567	19.497447
55.258317	2294.603892	19.502464
55.362753	2302.302946	19.507482
55.752793	2309.292564	19.512499
55.938653	2308.090866	19.517517
55.804444	2317.968322	19.522535
55.995787	2314.612043	19.527552
55.764474	2318.991721	19.532570
55.731924	2318.848221	19.537587
55.981735	2313.064614	19.542605
56.128130	2322.425361	19.547623
56.082227	2321.589424	19.552640
56.301481	2322.716238	19.557658
55.914951	2319.796652	19.562675
56.119871	2306.947901	19.567693
55.998097	2320.139673	19.572711
56.222028	2315.411874	19.577728
56.302288	2312.970034	19.582746
56.187846	2322.436096	19.587763
56.097705	2334.471255	19.592781
56.323793	2344.937850	19.597799
56.595716	2349.963308	19.602816
56.722410	2343.632186	19.607834
56.516002	2345.970606	19.612851
56.928763	2346.850245	19.617869
56.233752	2352.215556	19.622887
56.509835	2342.321694	19.627904
56.562051	2355.293031	19.632922
57.036341	2366.337537	19.637939
57.513343	2364.661491	19.642957
57.308476	2374.508564	19.647975
57.186859	2372.690436	19.652992
57.239558	2371.389621	19.658010
57.244554	2378.362809	19.663027
57.223212	2371.083832	19.668045
57.322463	2379.256501	19.673063
57.397521	2371.158242	19.678080
57.395589	2366.471956	19.683098
57.472766	2373.625561	19.688115
57.364671	2363.626984	19.693133
57.440958	2374.591813	19.698151
57.542070	2373.789061	19.703168
57.237417	2379.741071	19.708186
57.547564	2394.550497	19.713203
57.708898	2394.817358	19.718221
57.685636	2408.911463	19.723239
58.273328	2392.152740	19.728256
58.391908	2393.194931	19.733274
58.273325	2401.547875	19.738291
58.544979	2387.293764	19.743309
58.308820	2386.699763	19.748327
58.616440	2388.109824	19.753344
58.701808	2387.777611	19.758362
58.707580	2383.728812	19.763379
58.425557	2381.235403	19.768397
58.459994	2390.374136	19.773415
58.767745	2381.739267	19.778432
58.847204	2379.282599	19.783450
58.691989	2385.287864	19.788467
58.693322	2385.501583	19.793485
58.685800	2386.823464	19.798503
59.150196	2383.330015	19.803520
58.960645	2389.662478	19.808538
59.020703	2384.598170	19.813555
59.143826	2377.527411	19.818573
58.801634	2376.345425	19.823591
59.240413	2382.126164	19.828608
59.259367	2370.412193	19.833626
58.838972	2384.324979	19.838643
59.295012	2375.030103	19.843661
58.990800	2381.537384	19.848679
59.266741	2374.328982	19.853696
59.282258	2373.978019	19.858714
59.225875	2376.710202	19.863731
59.091829	2377.718742	19.868749
59.377976	2391.973506	19.873767
59.272482	2401.417741	19.878784
59.467587	2397.293905	19.883802
59.500176	2403.078081	19.888819
59.974018	2402.509285	19.893837
59.914019	2402.104290	19.898855
59.738606	2406.706339	19.903872
59.855613	2403.980166	19.908890
59.427986	2415.308571	19.913907
60.420702	2426.179195	19.918925
60.267488	2438.996945	19.923943
60.029754	2435.860886	19.928960
60.115165	2434.234700	19.933978
59.938700	2440.431375	19.938995
60.499949	2432.980791	19.944013
60.354529	2436.450075	19.949031
60.419314	2435.303861	19.954048
60.707843	2438.567067	19.959066
60.538699	2438.594020	19.964083
60.917046	2428.859203	19.969101
60.988292	2436.386635	19.974119
60.934216	2434.392540	19.979136
60.562923	2435.443641	19.984154
60.721991	2442.843798	19.989171
61.064120	2455.982944	19.994189
61.029187	2469.294722	19.999207
60.955180	2469.187724	20.004224
61.196791	2462.303330	20.009242
61.099718	2473.756834	20.014259
61.176832	2467.470536	20.019277
61.035431	2468.541610	20.024295
61.092750	2472.553578	20.029312
61.358727	2463.215805	20.034330
61.113583	2466.381638	20.039347
61.413555	2478.158832	20.044365
61.419389	2492.478066	20.049383
61.651994	2501.701682	20.054400
61.796879	2494.895628	20.059418
61.574695	2517.431978	20.064435
61.600514	2501.472264	20.069453
61.710392	2500.932408	20.074471
61.423537	2508.213359	20.079488
61.787467	2511.710765	20.084506
61.719446	2529.612232	20.089523
62.159705	2535.627207	20.094541
62.280943	2525.263141	20.099559
61.891013	2529.928546	20.104576
62.213491	2527.304090	20.109594
61.995422	2526.372102	20.114611
62.281041	2531.588158	20.119629
62.195302	2534.484734	20.124647
62.539321	2550.920347	20.129664
62.517972	2557.190659	20.134682
62.688598	2556.929012	20.139699
62.546599	2556.442698	20.144717
62.646802	2560.716871	20.149735
62.946421	2563.187006	20.154752
63.100166	2562.655097	20.159770
62.547044	2564.703525	20.164787
62.930537	2559.490033	20.169805
63.059995	2557.598014	20.174823
62.791759	2563.742515	20.179840
63.344493	2561.827039	20.184858
62.789620	2582.530253	20.189875
62.977636	2581.769480	20.194893
63.139429	2591.199526	20.199911
63.640887	2585.735160	20.204928
63.781410	2585.542030	20.209946
63.691657	2592.057676	20.214963
63.577859	2590.692149	20.219981
63.629297	2582.689575	20.224999
63.423889	2585.957649	20.230016
63.951540	2587.585141	20.235034
63.835669	2583.204858	20.240051
63.850788	2583.457286	20.245069
64.281399	2604.101686	20.250087
64.305454	2604.354262	20.255104
64.408225	2589.968779	20.260122
63.994480	2587.626133	20.265139
64.277226	2593.509718	20.270157
64.803087	2605.240762	20.275175
64.554863	2600.754151	20.280192
64.611428	2581.291376	20.285210
64.508474	2579.496203	20.290227
64.796805	2585.535430	20.295245
64.684975	2584.879901	20.300263
64.382793	2594.447662	20.305280
64.786962	2598.534924	20.310298
64.359956	2607.667152	20.315315
64.563030	2600.096621	20.320333
64.721498	2604.719424	20.325351
64.593887	2599.662160	20.330368
64.899981	2603.407943	20.335386
65.036867	2614.882453	20.340403
65.317219	2629.320082	20.345421
65.323544	2639.203659	20.350439
65.195738	2635.672449	20.355456
65.177593	2626.009390	20.360474
65.474391	2631.532053	20.365491
65.538611	2634.938058	20.370509
65.549751	2627.678945	20.375527
65.113727	2632.006408	20.380544
65.345870	2633.323126	20.385562
65.717109	2633.148262	20.390579
65.450894	2628.838353	20.395597
65.828105	2645.464647	20.400615
65.650316	2662.273081	20.405632
65.919927	2654.828781	20.410650
65.993841	2654.624247	20.415667
66.102435	2659.729352	20.420685
66.384055	2651.324253	20.425703
66.098460	2660.373391	20.430720
66.130594	2665.618124	20.435738
66.234882	2666.170191	20.440755
66.345543	2661.988955	20.445773
66.562913	2653.687708	20.450791
66.233337	2662.902758	20.455808
66.587803	2664.758469	20.460826
66.808271	2682.537811	20.465843
66.536501	2679.253737	20.470861
67.134785	2683.435138	20.475879
67.018266	2689.880368	20.480896
66.627650	2683.254813	20.485914
66.868978	2687.892746	20.490931
66.791507	2685.644336	20.495949
67.100421	2683.893590	20.500967
66.967053	2687.555305	20.505984
67.177124	2674.312889	20.511002
67.043674	2685.485244	20.516019
67.391846	2705.496336	20.521037
67.678913	2709.768283	20.526055
67.338895	2718.798605	20.531072
67.554132	2719.885974	20.536090
67.517747	2724.318065	20.541107
67.833939	2716.466702	20.546125
67.727633	2714.822291	20.551143
67.697205	2711.460387	20.556160
67.640513	2704.807525	20.561178
67.670838	2720.179506	20.566195
67.834149	2728.549034	20.571213
68.495631	2726.844315	20.576231
67.941226	2734.496854	20.581248
68.051460	2745.735798	20.586266
68.261632	2742.190777	20.591283
68.316815	2744.520578	20.596301
68.242154	2741.705344	20.601319
68.010383	2745.514920	20.606336
68.309866	2742.055556	20.611354
68.050025	2752.699058	20.616371
68.486827	2765.214538	20.621389
68.707448	2775.381826	20.626407
68.791924	2767.794725	20.631424
69.007824	2774.035945	20.636442
68.806350	2773.793521	20.641459
68.802979	2772.518133	20.646477
68.986833	2770.689780	20.651495
68.609416	2784.680258	20.656512
69.319166	2791.091297	20.661530
69.807366	2792.211441	20.666547
69.726140	2783.339457	20.671565
69.913812	2767.112148	20.676583
70.042942	2747.260787	20.681600
70.217562	2750.809683	20.686618
70.245726	2734.991719	20.691635
70.312806	2740.221466	20.696653
70.233841	2725.461298	20.701671
69.918599	2725.254325	20.706688
70.028378	2705.181921	20.711706
70.054710	2698.293207	20.716723
70.407726	2697.435318	20.721741
70.300611	2697.015017	20.726759
70.269546	2692.153137	20.731776
70.494645	2694.308733	20.736794
70.362025	2698.063939	20.741811
70.151644	2700.234711	20.746829
70.469665	2705.624226	20.751847
70.425181	2716.171213	20.756864
70.537683	2720.284575	20.761882
70.835704	2728.896925	20.766899
70.290052	2735.581311	20.771917
70.794578	2723.048620	20.776935
70.563549	2736.807251	20.781952
70.971509	2726.562506	20.786970
71.062418	2717.847177	20.791987
71.018571	2718.811463	20.797005
71.392729	2715.469989	20.802023
71.348684	2725.350645	20.807040
71.482649	2714.180489	20.812058
71.354533	2719.726116	20.817075
71.239837	2719.711346	20.822093
71.372873	2716.102331	20.827111
71.052460	2720.033804	20.832128
71.503596	2731.773724	20.837146
71.623235	2734.922341	20.842163
71.714702	2733.979517	20.847181
72.114884	2746.603084	20.852199
71.851242	2751.916258	20.857216
71.697615	2743.181704	20.862234
71.706621	2745.311201	20.867251
71.684604	2745.205348	20.872269
72.051460	2736.927412	20.877287
72.055101	2765.649514	20.882304
72.248638	2761.468405	20.887322
72.876281	2775.368593	20.892339
72.449020	2778.692543	20.897357
72.694975	2766.488170	20.902375
72.600729	2774.879137	20.907392
72.441115	2772.752368	20.912410
72.936589	2761.637009	20.917427
72.767792	2779.579240	20.922445
72.812159	2761.368902	20.927463
73.031719	2766.999117	20.932480
72.829731	2765.063177	20.937498
72.896726	2769.194823	20.942515
72.868511	2771.092700	20.947533
72.944223	2774.326994	20.952551
73.020775	2775.056547	20.957568
72.858788	2776.524237	20.962586
73.110555	2781.365844	20.967603
73.336100	2798.856616	20.972621
73.333196	2800.567177	20.977639
73.559629	2789.630004	20.982656
73.523877	2790.638627	20.987674
73.639289	2795.271505	20.992691
73.410809	2799.005840	20.997709
73.694799	2812.883782	21.002727
73.818938	2816.602789	21.007744
73.700562	2820.929204	21.012762
74.315671	2816.901101	21.017779
74.142607	2821.609886	21.022797
74.578069	2811.566792	21.027815
74.413372	2814.675817	21.032832
74.585307	2816.146894	21.037850
74.657566	2809.841559	21.042867
74.245460	2812.354449	21.047885
74.776332	2810.396806	21.052903
74.519261	2811.900116	21.057920
74.290361	2808.882133	21.062938
74.748401	2812.639923	21.067955
74.668331	2826.632577	21.072973
74.967227	2832.702475	21.077991
74.848817	2830.923107	21.083008
74.912928	2840.656012	21.088026
75.170323	2836.976005	21.093043
74.866888	2837.327224	21.098061
74.928097	2834.223637	21.103079
75.287812	2846.625623	21.108096
75.628694	2864.174382	21.113114
75.661667	2858.304004	21.118131
75.467395	2874.216981	21.123149
75.642232	2874.985141	21.128167
75.452448	2874.249208	21.133184
75.811763	2876.180477	21.138202
75.726881	2870.380020	21.143219
75.457492	2875.771245	21.148237
76.041115	2883.761540	21.153255
76.400181	2889.765229	21.158272
76.103071	2902.687354	21.163290
76.559249	2892.042276	21.168307
76.385638	2898.805848	21.173325
76.362124	2900.967300	21.178343
76.449376	2896.567114	21.183360
76.444860	2901.950717	21.188378
76.448175	2897.932060	21.193395
76.341093	2902.377052	21.198413
76.267762	2896.308862	21.203431
76.847798	2919.586329	21.208448
76.870053	2931.187138	21.213466
76.870623	2930.096753	21.218483
76.959321	2933.353396	21.223501
77.038117	2926.994264	21.228519
76.785611	2936.346653	21.233536
76.574709	2930.673252	21.238554
77.228358	2944.595415	21.243571
77.162282	2965.695552	21.248589
77.549163	2956.644185	21.253607
77.367415	2965.886980	21.258624
77.129115	2968.485451	21.263642
77.483124	2958.767541	21.268659
77.475821	2978.221340	21.273677
77.359731	2980.310251	21.278695
77.422753	2994.158315	21.283712
77.836331	2998.823156	21.288730
78.123765	2989.032460	21.293747
77.884578	3006.514999	21.298765
78.420049	3008.691155	21.303783
78.397466	3003.287401	21.308800
78.239695	3026.671692	21.313818
78.635892	3018.281937	21.318835
78.389015	3017.869756	21.323853
78.522791	3026.692549	21.328871
78.483177	3015.084945	21.333888
78.436654	3023.792537	21.338906
78.853867	3025.418031	21.343923
78.883112	3036.276796	21.348941
79.006477	3046.101078	21.353959
79.207124	3036.085840	21.358976
79.385598	3047.355826	21.363994
79.388475	3041.538159	21.369011
79.483867	3042.042102	21.374029
79.464537	3046.481796	21.379047
79.515486	3035.535455	21.384064
79.603874	3049.114429	21.389082
79.925631	3035.336269	21.394099
79.601678	3044.598645	21.399117
79.624289	3039.658079	21.404135
79.871505	3045.259606	21.409152
79.743382	3045.880219	21.414170
79.767158	3051.483557	21.419187
79.839270	3056.485277	21.424205
80.058147	3075.479135	21.429223
80.190248	3072.069203	21.434240
80.240118	3075.069333	21.439258
80.417453	3067.138453	21.444275
80.152014	3075.148627	21.449293
80.240989	3073.065553	21.454311
80.385106	3079.764377	21.459328
80.286041	3105.297969	21.464346
80.704524	3098.851551	21.469363
80.765342	3104.960318	21.474381
80.726241	3096.267859	21.479399
80.731561	3103.983143	21.484416
80.524120	3112.753423	21.489434
81.355584	3128.127863	21.494451
80.959890	3136.517551	21.499469
81.244949	3130.336257	21.504487
81.345721	3130.077090	21.509504
81.214644	3132.708835	21.514522
81.463401	3132.286831	21.519539
81.210376	3135.026916	21.524557
81.721940	3147.594523	21.529575
81.639851	3157.252623	21.534592
81.763482	3165.447017	21.539610
82.234282	3153.606081	21.544627
82.107522	3162.006387	21.549645
82.076705	3161.689540	21.554663
82.518717	3152.840870	21.559680
82.430977	3162.443237	21.564698
82.128122	3149.579545	21.569715
82.395515	3152.933604	21.574733
82.486372	3149.231306	21.579751
82.560790	3148.279376	21.584768
82.460344	3167.283373	21.589786
83.098248	3169.405461	21.594803
82.940428	3175.621497	21.599821
82.821539	3191.792614	21.604839
82.963128	3178.935896	21.609856
82.869257	3186.748067	21.614874
83.401609	3180.138711	21.619891
83.479075	3173.337590	21.624909
83.517484	3174.006381	21.629927
83.650913	3174.745764	21.634944
83.573548	3172.320267	21.639962
83.560317	3162.593138	21.644979
83.586519	3171.909882	21.649997
83.777444	3176.634675	21.655015
83.880066	3167.420053	21.660032
83.658932	3174.771087	21.665050
83.672068	3189.111077	21.670067
83.827323	3198.636957	21.675085
83.912391	3197.553528	21.680103
83.814535	3196.628282	21.685120
83.586414	3214.565558	21.690138
84.086710	3222.060370	21.695155
84.113942	3224.891866	21.700173
84.045251	3230.252785	21.705191
84.271355	3229.689649	21.710208
84.610082	3250.540776	21.715226
84.668974	3257.110103	21.720243
84.688262	3257.203761	21.725261
84.800192	3265.896452	21.730279
85.286608	3257.495322	21.735296
84.970979	3265.206809	21.740314
85.160489	3258.536457	21.745331
85.276167	3264.012729	21.750349
84.828415	3265.083943	21.755367
84.906853	3271.584081	21.760384
85.485130	3282.814088	21.765402
85.520303	3282.231840	21.770419
85.250270	3282.413330	21.775437
85.575501	3284.320986	21.780455
85.719914	3277.038723	21.785472
85.654609	3296.966318	21.790490
86.073708	3303.154121	21.795507
86.169639	3305.311530	21.800525
86.368301	3310.632201	21.805543
86.465772	3301.838389	21.810560
86.796272	3304.383967	21.815578
86.743810	3307.314720	21.820595
86.992004	3307.762052	21.825613
86.909080	3303.906500	21.830631
87.113781	3288.998261	21.835648
87.011392	3282.626964	21.840666
86.946740	3263.398157	21.845683
86.939543	3269.150475	21.850701
86.708209	3285.791951	21.855719
87.104396	3292.228839	21.860736
87.062054	3301.986107	21.865754
87.132775	3298.020309	21.870771
87.203636	3303.692540	21.875789
87.200731	3306.635056	21.880807
87.455121	3295.232858	21.885824
87.247016	3314.843418	21.890842
87.255366	3320.430439	21.895859
87.592161	3326.985372	21.900877
87.462621	3339.589307	21.905895
87.775278	3331.010529	21.910912
87.373131	3357.766580	21.915930
87.579376	3363.911263	21.920947
87.714440	3363.409840	21.925965
87.581315	3372.829212	21.930983
87.899943	3388.443832	21.936000
88.118485	3393.194185	21.941018
88.330910	3393.670037	21.946035
88.225578	3402.836413	21.951053
88.560092	3427.623321	21.956071
89.049085	3432.574420	21.961088
88.776392	3435.545040	21.966106
89.174705	3435.076366	21.971123
89.127510	3439.874619	21.976141
89.148096	3436.772664	21.981159
89.328259	3429.499572	21.986176
89.053539	3433.077814	21.991194
89.387134	3443.256659	21.996211
89.477849	3455.782302	22.001229
89.481580	3456.057801	22.006247
89.847325	3448.304348	22.011264
89.794881	3452.437142	22.016282
89.748276	3458.801546	22.021299
90.189184	3459.052165	22.026317
89.640807	3462.358605	22.031335
90.056255	3447.013041	22.036352
90.182810	3452.021160	22.041370
89.998946	3450.901148	22.046387
90.379175	3461.834055	22.051405
90.014395	3483.671685	22.056423
90.509012	3483.803608	22.061440
90.559558	3482.091615	22.066458
90.735477	3477.558330	22.071475
90.756478	3479.984165	22.076493
90.775664	3488.851472	22.081511
90.844693	3475.141526	22.086528
90.882007	3479.935755	22.091546
91.050416	3495.400594	22.096563
91.338778	3503.944145	22.101581
91.254079	3510.162033	22.106599
91.488102	3506.239363	22.111616
91.114704	3507.888731	22.116634
91.359611	3507.171548	22.121651
91.267199	3505.377725	22.126669
91.383141	3528.930776	22.131687
91.954528	3529.713614	22.136704
92.055938	3537.118016	22.141722
92.054900	3543.387870	22.146739
92.233108	3531.695561	22.151757
92.075835	3535.835655	22.156775
92.282950	3535.749896	22.161792
91.819738	3542.972158	22.166810
92.072063	3558.105082	22.171827
92.673476	3558.951572	22.176845
92.287980	3571.539885	22.181863
92.292207	3574.755863	22.186880
92.572263	3577.422029	22.191898
92.327032	3588.019748	22.196915
92.883416	3591.841516	22.201933
92.949689	3604.469517	22.206951
92.971209	3595.028415	22.211968
93.422626	3602.764073	22.216986
93.414766	3621.833346	22.222003
93.938051	3615.484060	22.227021
93.632800	3623.445025	22.232039
94.189973	3617.462427	22.237056
94.202616	3619.008550	22.242074
94.252763	3609.285179	22.247091
94.149262	3595.971582	22.252109
94.082003	3594.231163	22.257127
94.428304	3597.490141	22.262144
94.288810	3604.236008	22.267162
94.389519	3612.707282	22.272179
94.260173	3613.927554	22.277197
94.142933	3618.967529	22.282215
94.528263	3611.109388	22.287232
94.422813	3615.522868	22.292250
94.401724	3617.698985	22.297267
94.848729	3627.203791	22.302285
94.933167	3640.628182	22.307303
94.869180	3645.009885	22.312320
95.018156	3648.065129	22.317338
95.169713	3653.366692	22.322355
95.322526	3654.302822	22.327373
95.146990	3654.097151	22.332391
95.369008	3644.979616	22.337408
95.633330	3644.408012	22.342426
95.128973	3648.700249	22.347443
95.534840	3655.284435	22.352461
95.467995	3673.845553	22.357479
95.412836	3671.006576	22.362496
95.549315	3680.686805	22.367514
95.885217	3691.088083	22.372531
95.886171	3705.421080	22.377549
95.836724	3714.858006	22.382567
96.323648	3699.592822	22.387584
96.331514	3715.763967	22.392602
96.063381	3721.652475	22.397619
96.399180	3718.670114	22.402637
96.312799	3722.505526	22.407655
96.609789	3732.770651	22.412672
96.926481	3745.196784	22.417690
97.118341	3763.310048	22.422707
97.548300	3755.561928	22.427725
97.466155	3761.597794	22.432743
97.883476	3753.301018	22.437760
97.677142	3750.505014	22.442778
97.867677	3754.621958	22.447795
97.911969	3751.308473	22.452813
97.615650	3754.341924	22.457831
97.796686	3749.456883	22.462848
98.146571	3742.376053	22.467866
98.186611	3745.506904	22.472883
98.596290	3742.634691	22.477901
98.406525	3750.438853	22.482919
98.062483	3748.209976	22.487936
98.186965	3745.288843	22.492954
98.098889	3759.080697	22.497971
98.600099	3764.043337	22.502989
98.552145	3781.067560	22.508007
98.493728	3780.700820	22.513024
98.659751	3782.557625	22.518042
98.496440	3789.678686	22.523059
98.975045	3800.576492	22.528077
98.654759	3810.368981	22.533095
98.715254	3807.132355	22.538112
99.056475	3814.412907	22.543130
99.078708	3835.905350	22.548147
98.905596	3844.331529	22.553165
99.212344	3853.364028	22.558183
99.324964	3864.724600	22.563200
99.677907	3880.103775	22.568218
99.745478	3880.920566	22.573235
100.143135	3877.804013	22.578253
99.803457	3889.886532	22.583271
99.954797	3885.674862	22.588288
100.401863	3890.191478	22.593306
100.782025	3891.422562	22.598323
101.166453	3875.109161	22.603341
101.650024	3855.103021	22.608359
101.714990	3842.630830	22.613376
101.596592	3842.028209	22.618394
102.015603	3841.039376	22.623411
101.855172	3814.239953	22.628429
101.593358	3798.224790	22.633447
102.038321	3799.778297	22.638464
101.923445	3793.839868	22.643482
101.854319	3804.771531	22.648499
102.042084	3797.087974	22.653517
101.890972	3783.256297	22.658535
101.859821	3783.439030	22.663552
102.115641	3777.299891	22.668570
102.033576	3790.598357	22.673587
101.890516	3784.267154	22.678605
102.143156	3782.945345	22.683623
102.110511	3794.010424	22.688640
102.432758	3784.496068	22.693658
102.133799	3798.902945	22.698675
102.190316	3793.074852	22.703693
102.625505	3787.278417	22.708711
102.444681	3816.001312	22.713728
102.587845	3829.107347	22.718746
102.429607	3833.460082	22.723763
102.829050	3823.954631	22.728781
102.622034	3830.798690	22.733799
102.609024	3850.283662	22.738816
102.686205	3843.929898	22.743834
102.519767	3864.399892	22.748851
102.666396	3879.644406	22.753869
102.885598	3894.513915	22.758887
103.377110	3905.578879	22.763904
103.809476	3904.064768	22.768922
104.036093	3916.322115	22.773939
104.121401	3906.275120	22.778957
104.216033	3911.651149	22.783975
104.220835	3915.229772	22.788992
104.497274	3902.481508	22.794010
104.592194	3903.728974	22.799027
104.428896	3907.125930	22.804045
104.915904	3917.637010	22.809063
104.804797	3935.533689	22.814080
105.054238	3932.911986	22.819098
105.118442	3943.760342	22.824115
105.361301	3931.409964	22.829133
105.060096	3943.053714	22.834151
104.892173	3939.912486	22.839168
105.420975	3937.584508	22.844186
105.302385	3940.962542	22.849203
105.194579	3944.006876	22.854221
105.445415	3947.891627	22.859239
105.454504	3967.138010	22.864256
106.033806	3960.946423	22.869274
105.778017	3976.422775	22.874291
105.890030	3969.010815	22.879309
106.096191	3961.782091	22.884327
105.907477	3965.515095	22.889344
106.438099	3972.749790	22.894362
106.565478	3986.383989	22.899379
106.644663	3988.078451	22.904397
107.056051	3991.277579	22.909415
107.004713	3990.030188	22.914432
107.165026	3990.705538	22.919450
106.872782	3998.615855	22.924467
107.064456	3992.407401	22.929485
106.953854	3994.761479	22.934503
106.865156	3994.709517	22.939520
107.187214	3991.655346	22.944538
107.335515	4010.531870	22.949555
107.230496	4025.358812	22.954573
107.091728	4023.597491	22.959591
107.406287	4036.831357	22.964608
107.721714	4046.289766	22.969626
107.647388	4060.170966	22.974643
107.938976	4047.876442	22.979661
108.033379	4056.066555	22.984679
107.996280	4065.259436	22.989696
108.049619	4075.332369	22.994714
108.320449	4079.715877	22.999731
108.350242	4082.368551	23.004749
108.743358	4089.864387	23.009767
108.596470	4107.792941	23.014784
108.636887	4111.586993	23.019802
108.607704	4123.561187	23.024819
108.759828	4123.103435	23.029837
109.364281	4131.773955	23.034855
109.169811	4141.756646	23.039872
109.348566	4137.889827	23.044890
109.136668	4147.190089	23.049907
109.576003	4158.541270	23.054925
109.958202	4162.882656	23.059943
109.803781	4178.676614	23.064960
109.875786	4180.171635	23.069978
109.620233	4182.965807	23.074995
109.984493	4184.934231	23.080013
110.312954	4190.661704	23.085031
110.124606	4204.912090	23.090048
110.460054	4200.051840	23.095066
110.443937	4202.080137	23.100083
110.528606	4210.245928	23.105101
110.791837	4231.075090	23.110119
111.075117	4236.304723	23.115136
111.526080	4228.815768	23.120154
111.492367	4227.951029	23.125171
111.461850	4227.169958	23.130189
111.597489	4228.297674	23.135207
111.504737	4224.533130	23.140224
111.382929	4222.927207	23.145242
111.655855	4220.449609	23.150259
111.447648	4225.384718	23.155277
111.727682	4239.227672	23.160295
111.479004	4247.606342	23.165312
112.154552	4249.548736	23.170330
112.104329	4247.840924	23.175347
112.189668	4269.769210	23.180365
112.414722	4279.491566	23.185383
112.661419	4282.280402	23.190400
112.707838	4285.602307	23.195418
112.644367	4287.959142	23.200435
112.740064	4285.575092	23.205453
113.113921	4287.792959	23.210471
113.136155	4304.362892	23.215488
113.713856	4295.723985	23.220506
113.335572	4307.142728	23.225523
113.325889	4311.735460	23.230541
113.599942	4307.557598	23.235559
113.489652	4314.354987	23.240576
113.717307	4321.370690	23.245594
113.974704	4341.198675	23.250611
114.197973	4348.705209	23.255629
114.310037	4342.457381	23.260647
114.026943	4345.100207	23.265664
114.208259	4347.212686	23.270682
114.145911	4346.634148	23.275699
114.252575	4364.577650	23.280717
114.672645	4370.665845	23.285735
114.484111	4377.800652	23.290752
114.656198	4371.732837	23.295770
114.904094	4394.876813	23.300787
114.984501	4405.811037	23.305805
115.420888	4403.188550	23.310823
115.217279	4413.460031	23.315840
115.534320	4406.956851	23.320858
115.455189	4412.103518	23.325875
115.796197	4423.468225	23.330893
116.257851	4424.433830	23.335911
116.146074	4423.631877	23.340928
116.543051	4427.776669	23.345946
116.389976	4424.280521	23.350963
116.464003	4419.023689	23.355981
116.861708	4413.446975	23.360999
116.599673	4426.041499	23.366016
116.689425	4421.586964	23.371034
116.555488	4417.415915	23.376051
116.308585	4444.026449	23.381069
116.733062	4445.910570	23.386087
116.924115	4452.978588	23.391104
116.915605	4454.562788	23.396122
117.068099	4467.103831	23.401139
117.153354	4484.239791	23.406157
117.467604	4485.665532	23.411175
117.633567	4491.344298	23.416192
117.589247	4489.309030	23.421210
117.661558	4482.958916	23.426227
117.849315	4507.337574	23.431245
117.864385	4513.829487	23.436263
118.085209	4512.736116	23.441280
118.229492	4516.785127	23.446298
118.477283	4522.859163	23.451315
118.206193	4520.845104	23.456333
118.734751	4528.820707	23.461351
118.880883	4537.458349	23.466368
118.977276	4534.027028	23.471386
119.137077	4533.037006	23.476403
119.045155	4530.469635	23.481421
119.444366	4522.623749	23.486439
119.300395	4549.660981	23.491456
119.522658	4557.473816	23.496474
119.550031	4563.797004	23.501491
119.443043	4568.048949	23.506509
119.645089	4559.697942	23.511527
119.856445	4570.491825	23.516544
119.976590	4580.331023	23.521562
120.559806	4570.768257	23.526579
120.843843	4573.650322	23.531597
120.982430	4577.715993	23.536615
121.098250	4574.405866	23.541632
121.343333	4564.886795	23.546650
121.301386	4576.495208	23.551667
121.310664	4569.597323	23.556685
121.391300	4560.487611	23.561703
121.289388	4564.434284	23.566720
121.581728	4558.434543	23.571738
121.592161	4559.639682	23.576755
121.390557	4566.859269	23.581773
121.689314	4562.219526	23.586791
121.693695	4572.594840	23.591808
121.615222	4570.583101	23.596826
121.847103	4582.300477	23.601843
121.904371	4603.670445	23.606861
122.048613	4595.474179	23.611879
121.896175	4599.624026	23.616896
122.015888	4622.436351	23.621914
122.302362	4617.936226	23.626931
122.247765	4629.006219	23.631949
122.967261	4645.722608	23.636967
122.870412	4655.542175	23.641984
122.979222	4657.929814	23.647002
123.205616	4664.418778	23.652019
123.056231	4662.709422	23.657037
123.221088	4670.076744	23.662055
123.403752	4686.174665	23.667072
123.471043	4687.436046	23.672090
123.683908	4688.563285	23.677107
123.564649	4691.698497	23.682125
123.965548	4707.175531	23.687143
124.175780	4712.293469	23.692160
124.113855	4725.845252	23.697178
124.195149	4725.593099	23.702195
124.326463	4724.672120	23.707213
124.385392	4723.825621	23.712231
124.469036	4736.021485	23.717248
124.402552	4754.018248	23.722266
124.711366	4744.002702	23.727283
124.383806	4763.493408	23.732301
125.101699	4781.424132	23.737319
125.065592	4786.643528	23.742336
125.035090	4780.908383	23.747354
125.850344	4797.876378	23.752371
125.254034	4816.934823	23.757389
125.739449	4811.506043	23.762407
126.055722	4806.203365	23.767424
125.779215	4813.605736	23.772442
126.746059	4823.800216	23.777459
126.718834	4827.878236	23.782477
127.140229	4820.935760	23.787495
127.468994	4822.571639	23.792512
127.580095	4795.634295	23.797530
127.917889	4772.507961	23.802547
127.835254	4776.796205	23.807565
128.070117	4770.465677	23.812583
127.928373	4779.338181	23.817600
128.037047	4777.013349	23.822618
128.377150	4746.695975	23.827635
127.846957	4744.377826	23.832653
127.886041	4736.656126	23.837671
128.071902	4726.985116	23.842688
128.036085	4752.701080	23.847706
128.414911	4761.002006	23.852723
128.278458	4764.321710	23.857741
128.505668	4768.355994	23.862759
128.494517	4765.319399	23.867776
128.554998	4771.974905	23.872794
128.518569	4765.366653	23.877811
128.451090	4784.867839	23.882829
128.789256	4789.506740	23.887847
128.490799	4800.600799	23.892864
128.743056	4806.095207	23.897882
129.142803	4819.647412	23.902899
129.136325	4828.003521	23.907917
129.319088	4841.502232	23.912935
129.464805	4865.565627	23.917952
129.521661	4862.936710	23.922970
129.771666	4864.456915	23.927987
129.722925	4886.354002	23.933005
130.058146	4897.923766	23.938023
130.156566	4902.516752	23.943040
130.297597	4907.819662	23.948058
130.756821	4927.322016	23.953075
130.518494	4932.281043	23.958093
130.733680	4929.909307	23.963111
130.876472	4932.544115	23.968128
130.608505	4944.232914	23.973146
130.994113	4936.113623	23.978163
131.108099	4951.605983	23.983181
131.144615	4952.702358	23.988199
131.917782	4948.517898	23.993216
132.299008	4956.895652	23.998234
132.362104	4937.424000	24.003251
132.289897	4939.455048	24.008269
132.499241	4934.856198	24.013287
132.964065	4940.960314	24.018304
132.666370	4942.264968	24.023322
132.967554	4937.681369	24.028339
133.004062	4944.947351	24.033357
132.740842	4960.521897	24.038375
132.784725	4960.308750	24.043392
132.891544	4960.799927	24.048410
133.267574	4953.655351	24.053427
133.423870	4964.159344	24.058445
133.355098	4969.605874	24.063463
133.358309	4978.061227	24.068480
133.499463	4995.497271	24.073498
133.607365	4986.959631	24.078515
133.618736	5005.218858	24.083533
133.611271	5018.764586	24.088551
133.883181	5025.285789	24.093568
134.191693	5031.771262	24.098586
134.446844	5045.212986	24.103603
134.346815	5058.608294	24.108621
134.313587	5050.842102	24.113639
134.945739	5064.522691	24.118656
134.619956	5084.978872	24.123674
134.739757	5078.119773	24.128691
134.809788	5088.783158	24.133709
135.167431	5109.505675	24.138727
135.406626	5108.947469	24.143744
135.633126	5109.150500	24.148762
136.178326	5116.649365	24.153779
136.241526	5131.507239	24.158797
136.693427	5128.885303	24.163815
136.848692	5129.873854	24.168832
136.652357	5134.003312	24.173850
137.111080	5129.668323	24.178867
136.959623	5137.232653	24.183885
137.314493	5121.522100	24.188903
137.329124	5116.368902	24.193920
137.141018	5126.502296	24.198938
137.455550	5117.719997	24.203955
137.523735	5117.636720	24.208973
137.629378	5118.684321	24.213991
137.852291	5113.243792	24.219008
137.245052	5126.613041	24.224026
137.518742	5139.070032	24.229043
137.946085	5149.030564	24.234061
137.518210	5146.810112	24.239079
137.698730	5157.567647	24.244096
137.610587	5175.119142	24.249114
138.275570	5173.565460	24.254131
138.161007	5190.504373	24.259149
138.520267	5207.558932	24.264167
138.478402	5216.571549	24.269184
138.732261	5231.983680	24.274202
138.671560	5242.439863	24.279219
138.935322	5247.776039	24.284237
139.120504	5250.241288	24.289255
139.664589	5261.915717	24.294272
139.610352	5278.588628	24.299290
139.831806	5270.437111	24.304307
139.854277	5273.111623	24.309325
140.015607	5280.928266	24.314343
140.456219	5294.198242	24.319360
140.599103	5305.330875	24.324378
140.658380	5303.967388	24.329395
140.844055	5305.689868	24.334413
140.970405	5306.159061	24.339431
140.745962	5308.527564	24.344448
140.829135	5321.454886	24.349466
141.235637	5328.523590	24.354483
141.566246	5331.115148	24.359501
141.313427	5333.369379	24.364519
142.055713	5341.578849	24.369536
141.941383	5364.317920	24.374554
141.929961	5370.310907	24.379571
141.991630	5373.945330	24.384589
142.220286	5364.740713	24.389607
142.252086	5369.291754	24.394624
142.164520	5384.733310	24.399642
142.674576	5383.938363	24.404659
142.423728	5383.202589	24.409677
142.514895	5404.958547	24.414695
142.749786	5414.636028	24.419712
142.832563	5425.702021	24.424730
143.205382	5437.013664	24.429747
143.578401	5443.095651	24.434765
143.688696	5446.956009	24.439783
143.690186	5444.470354	24.444800
143.757995	5459.741662	24.449818
144.133177	5457.622846	24.454835
144.089950	5469.928452	24.459853
144.522295	5480.965496	24.464871
144.623578	5470.151728	24.469888
145.008838	5476.169624	24.474906
144.824446	5478.195817	24.479923
145.054016	5488.553176	24.484941
145.122351	5506.723688	24.489959
145.325725	5505.041382	24.494976
145.417142	5507.945694	24.499994
145.370433	5502.123947	24.505011
145.306153	5504.451993	24.510029
145.462558	5534.520182	24.515047
145.749499	5529.391082	24.520064
145.901590	5538.900104	24.525082
145.953755	5543.389731	24.530099
145.893221	5553.588832	24.535117
146.094898	5566.795659	24.540135
146.270663	5567.533139	24.545152
146.365610	5592.188024	24.550170
146.501020	5598.644703	24.555187
146.987398	5600.495509	24.560205
146.706483	5614.510241	24.565223
147.076001	5623.449642	24.570240
147.084257	5641.504802	24.575258
147.314784	5647.954991	24.580275
147.473238	5663.839116	24.585293
147.849402	5663.943549	24.590311
147.811309	5664.774141	24.595328
147.818958	5692.371499	24.600346
148.128814	5701.797248	24.605363
148.196259	5701.611018	24.610381
148.174870	5723.937710	24.615399
148.764694	5737.806638	24.620416
148.886033	5739.721175	24.625434
149.015512	5735.459754	24.630451
149.220209	5744.099782	24.635469
149.053537	5766.074408	24.640487
149.488051	5756.606197	24.645504
149.265167	5771.371069	24.650522
149.671102	5791.658048	24.655539
149.976813	5793.821716	24.660557
149.922891	5796.464443	24.665575
150.553239	5796.982323	24.670592
150.755496	5822.872256	24.675610
150.742509	5831.236263	24.680627
151.002228	5825.489842	24.685645
150.882346	5822.140703	24.690663
151.244900	5817.015184	24.695680
150.933425	5815.734371	24.700698
151.049645	5830.334295	24.705715
151.898616	5834.647392	24.710733
151.653167	5847.875410	24.715751
152.049052	5845.215079	24.720768
152.194722	5850.916490	24.725786
152.376785	5849.515280	24.730803
152.207462	5845.938770	24.735821
152.355183	5860.849989	24.740839
152.705342	5860.960145	24.745856
152.472249	5862.856467	24.750874
152.618974	5859.567878	24.755891
153.455747	5865.133923	24.760909
153.518318	5879.728288	24.765927
153.572624	5880.978467	24.770944
153.713129	5887.115811	24.775962
153.810985	5886.433773	24.780979
154.003220	5885.635192	24.785997
153.864640	5876.124531	24.791015
154.165047	5885.108156	24.796032
153.991022	5878.799082	24.801050
154.030955	5887.044533	24.806067
154.561818	5897.906466	24.811085
154.568144	5916.424114	24.816103
154.716819	5910.186313	24.821120
155.023042	5907.897470	24.826138
154.637246	5914.508991	24.831155
155.149790	5924.800293	24.836173
155.187703	5945.961281	24.841191
155.463729	5943.851916	24.846208
155.476941	5954.399885	24.851226
155.598206	5966.289425	24.856243
156.050914	5961.313136	24.861261
155.957296	5969.899365	24.866279
155.884731	5966.294022	24.871296
156.187270	5994.226517	24.876314
156.448226	5996.477604	24.881331
156.912105	6001.679864	24.886349
156.753761	6015.950022	24.891367
157.252593	6017.466083	24.896384
157.176715	6028.734066	24.901402
157.181755	6036.883667	24.906419
157.398601	6024.671027	24.911437
157.563461	6054.273140	24.916455
157.978444	6055.961508	24.921472
158.082780	6063.941866	24.926490
158.183996	6058.172634	24.931507
158.365415	6071.309183	24.936525
158.469728	6087.946709	24.941543
158.756027	6092.455820	24.946560
158.768918	6086.245103	24.951578
158.661993	6087.890803	24.956595
159.303119	6100.473346	24.961613
159.262266	6119.031028	24.966631
159.618866	6106.947891	24.971648
159.622501	6115.993926	24.976666
159.625389	6120.013210	24.981683
159.795406	6134.414450	24.986701
159.906614	6140.607712	24.991719
159.993309	6146.987424	24.996736
160.150520	6156.155342	25.001754
160.210104	6169.121785	25.006771
160.565635	6169.748019	25.011789
160.579311	6175.898624	25.016807
160.998171	6190.206739	25.021824
161.479574	6195.982216	25.026842
161.273945	6207.978361	25.031859
161.634156	6203.981365	25.036877
161.698022	6215.387716	25.041895
162.211769	6220.202863	25.046912
162.371523	6220.595948	25.051930
162.570540	6216.933079	25.056947
162.992592	6210.399786	25.061965
162.894807	6219.131595	25.066983
162.909705	6209.881859	25.072000
162.976430	6216.957962	25.077018
162.945391	6216.947938	25.082035
163.057622	6212.973169	25.087053
162.971525	6211.387295	25.092071
163.383342	6212.973116	25.097088
163.360298	6221.790574	25.102106
163.522934	6231.369174	25.107123
163.595010	6236.497085	25.112141
163.728419	6239.853555	25.117159
163.780380	6259.445429	25.122176
164.106136	6271.939925	25.127194
164.203093	6273.861567	25.132211
164.503280	6281.983127	25.137229
164.584867	6297.339651	25.142247
164.738289	6299.939179	25.147264
164.661042	6319.435286	25.152282
164.750331	6326.816273	25.157299
164.910911	6332.122088	25.162317
165.074313	6355.325888	25.167335
165.371951	6363.617064	25.172352
165.555221	6382.587825	25.177370
165.776716	6392.916421	25.182387
166.384907	6391.396862	25.187405
166.470025	6412.491977	25.192423
167.276555	6412.274447	25.197440
167.355021	6412.651387	25.202458
167.221383	6416.572136	25.207475
167.486718	6414.683933	25.212493
167.752197	6415.042857	25.217511
167.398998	6416.557907	25.222528
167.446533	6425.612081	25.227546
167.561433	6441.003569	25.232563
167.880803	6449.638316	25.237581
167.671521	6462.227722	25.242599
167.800176	6465.400886	25.247616
168.422471	6475.787593	25.252634
168.206757	6482.107085	25.257651
168.844713	6489.709107	25.262669
168.869201	6500.421685	25.267687
169.353697	6502.787494	25.272704
169.497060	6500.925810	25.277722
169.462313	6510.228413	25.282739
169.670642	6522.037638	25.287757
169.921822	6530.517285	25.292775
170.234599	6530.671179	25.297792
170.754642	6529.692833	25.302810
170.754859	6527.904326	25.307827
171.098789	6520.279442	25.312845
171.146288	6517.071050	25.317863
171.378336	6517.584804	25.322880
171.411264	6516.743138	25.327898
171.456016	6516.466098	25.332915
171.557273	6503.257283	25.337933
171.734210	6507.197778	25.342951
171.456152	6521.736143	25.347968
171.716044	6534.266541	25.352986
172.303707	6546.644763	25.358003
172.475783	6529.617978	25.363021
172.601707	6528.313782	25.368039
172.609236	6530.229258	25.373056
173.010566	6525.574920	25.378074
172.851101	6530.428268	25.383091
173.162994	6538.091746	25.388109
173.223914	6547.811873	25.393127
173.299935	6558.059133	25.398144
173.478185	6542.766297	25.403162
173.264179	6563.733072	25.408179
173.710759	6571.828304	25.413197
173.557622	6590.499684	25.418215
173.724160	6589.258247	25.423232
173.961765	6602.302120	25.428250
173.600598	6629.417114	25.433267
174.538299	6632.561247	25.438285
174.150510	6655.659052	25.443303
174.369999	6669.050504	25.448320
174.827004	6676.140922	25.453338
174.862949	6695.367688	25.458355
174.996058	6713.980207	25.463373
175.157516	6727.830246	25.468391
175.377777	6737.590399	25.473408
175.719140	6743.729908	25.478426
175.731958	6762.270394	25.483443
175.836082	6784.146696	25.488461
176.332911	6788.807362	25.493479
176.595370	6809.785068	25.498496
176.983683	6808.855249	25.503514
176.983624	6816.108309	25.508531
177.194199	6830.694174	25.513549
177.443394	6838.507075	25.518567
177.751865	6845.211314	25.523584
177.846898	6850.064317	25.528602
177.990169	6864.372177	25.533619
178.493819	6867.335352	25.538637
178.277763	6881.539216	25.543655
178.474696	6881.069523	25.548672
178.552018	6890.582287	25.553690
178.902201	6904.314274	25.558707
179.034008	6911.353578	25.563725
179.002033	6913.989857	25.568743
179.049863	6927.530871	25.573760
179.326338	6940.832437	25.578778
179.381985	6949.922619	25.583795
179.422196	6971.313673	25.588813
179.881653	6980.874546	25.593831
179.619310	7003.607461	25.598848
180.121934	7014.295322	25.603866
180.103737	7024.389538	25.608883
180.804599	7024.241576	25.613901
181.262925	7036.757285	25.618919
181.109001	7033.199275	25.623936
181.498387	7029.432680	25.628954
181.564998	7033.000628	25.633971
181.834684	7049.205276	25.638989
182.092736	7053.468183	25.644007
181.756121	7060.598766	25.649024
182.298245	7059.497270	25.654042
182.444274	7068.402366	25.659059
182.469162	7085.907408	25.664077
182.651159	7093.292880	25.669095
182.697087	7096.166203	25.674112
182.939028	7108.827419	25.679130
182.948955	7128.054958	25.684148
183.268222	7128.279430	25.689165
183.431855	7130.225962	25.694183
183.468429	7168.216592	25.699200
183.877705	7162.662202	25.704218
184.168965	7184.377850	25.709236
184.023116	7189.526672	25.714253
184.500250	7199.434234	25.719271
184.584906	7212.625779	25.724288
184.568338	7220.252278	25.729306
184.789472	7225.017629	25.734324
184.967364	7241.092340	25.739341
185.549653	7241.990923	25.744359
185.406030	7258.548113	25.749376
185.587577	7270.318139	25.754394
185.757923	7279.346957	25.759412
186.030090	7285.645655	25.764429
186.326382	7305.905769	25.769447
186.654047	7314.363442	25.774464
186.748787	7309.812826	25.779482
187.172516	7320.569356	25.784500
187.297671	7329.075849	25.789517
187.607935	7334.331406	25.794535
187.282505	7344.207288	25.799552
187.728322	7352.299924	25.804570
187.847947	7361.794835	25.809588
187.966499	7363.057717	25.814605
188.144859	7374.733910	25.819623
188.141563	7393.051918	25.824640
188.422337	7388.782432	25.829658
188.719165	7410.703682	25.834676
188.724446	7425.883114	25.839693
189.556969	7424.685722	25.844711
189.248464	7436.015463	25.849728
189.745836	7447.322956	25.854746
189.677464	7464.442793	25.859764
189.752409	7464.013778	25.864781
190.055765	7477.281638	25.869799
190.019093	7489.494230	25.874816
190.633165	7490.322453	25.879834
190.629235	7498.514415	25.884852
190.807009	7520.939524	25.889869
191.208065	7521.713581	25.894887
191.334549	7529.444117	25.899904
190.884185	7530.229593	25.904922
191.596584	7538.563105	25.909940
191.584966	7558.402102	25.914957
191.975909	7558.484534	25.919975
192.008328	7573.206548	25.924992
192.060790	7582.203197	25.930010
192.179753	7593.938606	25.935028
192.300710	7610.046398	25.940045
192.714695	7618.343337	25.945063
192.887888	7620.609458	25.950080
192.957676	7653.872384	25.955098
193.096585	7662.494907	25.960116
193.204204	7665.544995	25.965133
193.612756	7680.846096	25.970151
193.651696	7701.707253	25.975168
193.833447	7711.954187	25.980186
194.149320	7723.519812	25.985204
194.187227	7737.322423	25.990221
194.246030	7744.105040	25.995239
194.517353	7771.423820	26.000256
194.895995	7780.299339	26.005274
195.229789	7791.823996	26.010292
195.497471	7801.252697	26.015309
196.112775	7807.646420	26.020327
195.578006	7819.239148	26.025344
196.285900	7841.830059	26.030362
196.345689	7847.120224	26.035380
196.357409	7850.082163	26.040397
196.696276	7858.854693	26.045415
196.935555	7879.285596	26.050432
197.142064	7879.136188	26.055450
197.497367	7895.045219	26.060468
197.728517	7903.152317	26.065485
198.051745	7904.820915	26.070503
198.042702	7907.205840	26.075520
198.567016	7912.245704	26.080538
198.692574	7923.855598	26.085556
198.673310	7936.796413	26.090573
199.347890	7929.796802	26.095591
199.173771	7935.858859	26.100608
199.140708	7929.045642	26.105626
200.231355	7944.707260	26.110644
200.067514	7949.981180	26.115661
200.460448	7947.084498	26.120679
200.550843	7950.364411	26.125696
200.874335	7944.252125	26.130714
201.108853	7949.728899	26.135732
200.943347	7948.897543	26.140749
201.166003	7939.078914	26.145767
201.305672	7941.634500	26.150784
201.451173	7939.049927	26.155802
201.206655	7950.732613	26.160820
201.250744	7956.403425	26.165837
201.753302	7972.246177	26.170855
201.390638	7976.873891	26.175872
201.767276	7999.906584	26.180890
201.970167	8001.553066	26.185908
201.924355	8022.680779	26.190925
202.195956	8033.585231	26.195943
202.621164	8047.104475	26.200960
202.612384	8076.198477	26.205978
202.674459	8081.727580	26.210996
202.804850	8098.343917	26.216013
203.375037	8115.234821	26.221031
203.335211	8137.149434	26.226048
203.442309	8148.396140	26.231066
203.818195	8155.326300	26.236084
203.816400	8181.229264	26.241101
204.321325	8184.875942	26.246119
204.347519	8201.643173	26.251136
204.952561	8218.720645	26.256154
205.561826	8226.938791	26.261172
205.285758	8228.496406	26.266189
205.862409	8229.449076	26.271207
206.397229	8245.728041	26.276224
206.405751	8251.071377	26.281242
206.699627	8251.652458	26.286260
206.648071	8249.443524	26.291277
207.175821	8254.257902	26.296295
207.034523	8266.028250	26.301312
207.370565	8271.730147	26.306330
208.100563	8265.855887	26.311348
207.977071	8264.201390	26.316365
208.170423	8258.133726	26.321383
208.458740	8257.285872	26.326400
208.726098	8285.729154	26.331418
209.255928	8287.404992	26.336436
208.952829	8299.102009	26.341453
209.252969	8290.200148	26.346471
209.310538	8293.935092	26.351488
209.483440	8294.210466	26.356506
209.875149	8290.746943	26.361524
209.747223	8305.666002	26.366541
210.269774	8303.589410	26.371559
210.206762	8317.502289	26.376576
210.174579	8321.674518	26.381594
210.734570	8317.093885	26.386612
210.787254	8341.786820	26.391629
211.085167	8336.265889	26.396647
211.000590	8347.116793	26.401664
211.249734	8366.198407	26.406682
211.224528	8377.050097	26.411700
211.112751	8388.448342	26.416717
211.683566	8403.210461	26.421735
211.930788	8412.881643	26.426752
212.004605	8427.737577	26.431770
212.394372	8430.925015	26.436788
212.448505	8446.029232	26.441805
212.752125	8466.371990	26.446823
212.636315	8476.483929	26.451840
212.971256	8485.108727	26.456858
213.396577	8504.673145	26.461876
213.421207	8520.116584	26.466893
213.573461	8541.826469	26.471911
213.955913	8546.245856	26.476928
213.757762	8567.741724	26.481946
214.292561	8574.243051	26.486964
214.484855	8599.369786	26.491981
214.703497	8607.988801	26.496999
214.803970	8621.893998	26.502016
215.080602	8641.236383	26.507034
215.475544	8650.153501	26.512052
215.524653	8679.034054	26.517069
215.732460	8685.586773	26.522087
216.117200	8690.246247	26.527104
216.036242	8714.095470	26.532122
216.580203	8716.587523	26.537140
216.766282	8738.812861	26.542157
216.749465	8743.114175	26.547175
216.907195	8758.998968	26.552192
217.137061	8778.962013	26.557210
217.702302	8796.049249	26.562228
217.329444	8813.590605	26.567245
217.449985	8821.739445	26.572263
218.103537	8846.746631	26.577280
217.972231	8866.773666	26.582298
218.828445	8889.116279	26.587316
218.957421	8905.436665	26.592333
219.009824	8912.076427	26.597351
219.257606	8930.780454	26.602368
219.413657	8945.516373	26.607386
219.790970	8963.910981	26.612404
219.996467	8983.833721	26.617421
220.289195	8997.292712	26.622439
220.698149	9003.488886	26.627456
220.541510	9019.995007	26.632474
221.046559	9027.249670	26.637492
221.106361	9043.630812	26.642509
221.533127	9052.420726	26.647527
221.634109	9071.724384	26.652544
221.928065	9079.630487	26.657562
222.224367	9087.681414	26.662580
222.253716	9107.069330	26.667597
222.273464	9118.822147	26.672615
222.895526	9131.189970	26.677632
222.735925	9134.926694	26.682650
223.439107	9141.469106	26.687668
223.782304	9148.718547	26.692685
224.052905	9151.348297	26.697703
224.604760	9169.044448	26.702720
224.820445	9188.331938	26.707738
224.892513	9184.899891	26.712756
225.031043	9191.685406	26.717773
225.019654	9182.832290	26.722791
225.341143	9183.540828	26.727808
225.161989	9189.787159	26.732826
225.798744	9194.702515	26.737844
225.526084	9210.752408	26.742861
225.924054	9204.037914	26.747879
226.286701	9212.638257	26.752896
226.405501	9227.135251	26.757914
226.502570	9238.819174	26.762932
226.758817	9248.417059	26.767949
226.938996	9261.117888	26.772967
226.938184	9263.351799	26.777984
227.251740	9285.948749	26.783002
227.275273	9296.896426	26.788020
227.746246	9312.684258	26.793037
227.475951	9330.074504	26.798055
227.991746	9353.130776	26.803072
227.871148	9369.246705	26.808090
228.354076	9384.177661	26.813108
228.492694	9411.787377	26.818125
228.627368	9429.350451	26.823143
229.065644	9451.551593	26.828160
228.756113	9476.622862	26.833178
229.301445	9486.977532	26.838196
229.652942	9508.790052	26.843213
229.790612	9536.606731	26.848231
229.974438	9558.578266	26.853248
230.334726	9576.933057	26.858266
230.836776	9593.718061	26.863284
231.164872	9615.251940	26.868301
231.262930	9636.534090	26.873319
231.953219	9640.494711	26.878336
231.724047	9662.119855	26.883354
232.325518	9676.173994	26.888372
232.402399	9692.570435	26.893389
232.771814	9698.339571	26.898407
232.886299	9707.059246	26.903424
233.181626	9725.253405	26.908442
233.790322	9724.674707	26.913460
234.166326	9726.628653	26.918477
234.595323	9723.476022	26.923495
234.808184	9716.256445	26.928512
234.742852	9752.158768	26.933530
234.812606	9754.703776	26.938548
235.256404	9753.778724	26.943565
235.188584	9755.241906	26.948583
235.688296	9768.203483	26.953600
235.590787	9782.602887	26.958618
235.783252	9789.033011	26.963636
236.082246	9800.448295	26.968653
235.861378	9820.573117	26.973671
236.548827	9825.176431	26.978688
236.371883	9853.934336	26.983706
236.402330	9858.108418	26.988724
236.827247	9869.775982	26.993741
237.014721	9891.166617	26.998759
237.457314	9904.404997	27.003776
237.588422	9919.990693	27.008794
237.911919	9920.170084	27.013812
238.342427	9945.560158	27.018829
238.627341	9946.271811	27.023847
238.824239	9944.759260	27.028864
239.080665	9955.357064	27.033882
239.383240	9966.287896	27.038900
239.776719	9968.905682	27.043917
239.576621	9993.296918	27.048935
240.188075	9993.514617	27.053952
240.337538	10009.643268	27.058970
240.801903	10018.259341	27.063988
240.775918	10030.286955	27.069005
240.709817	10046.396099	27.074023
241.216365	10057.661229	27.079040
241.313776	10070.075693	27.084058
241.432279	10078.882301	27.089076
241.907378	10098.358626	27.094093
241.765806	10101.861725	27.099111
241.927066	10123.539012	27.104128
241.992874	10150.558839	27.109146
242.496592	10168.582588	27.114164
242.881776	10185.017186	27.119181
243.036581	10205.382879	27.124199
243.496165	10205.234826	27.129216
243.251061	10231.247397	27.134234
243.441432	10248.263834	27.139252
244.073441	10265.436945	27.144269
244.432899	10267.854402	27.149287
244.704269	10290.339173	27.154304
244.922657	10314.212072	27.159322
244.971477	10320.134476	27.164340
245.137486	10332.158877	27.169357
245.247368	10357.731010	27.174375
245.653749	10369.177617	27.179392
246.188926	10382.701124	27.184410
246.432070	10394.338654	27.189428
246.977098	10416.362078	27.194445
247.198655	10415.718364	27.199463
247.983665	10417.428156	27.204480
247.894678	10438.625564	27.209498
248.658031	10440.489921	27.214516
248.792273	10445.182405	27.219533
248.956102	10448.806898	27.224551
248.808621	10440.912482	27.229568
249.069533	10439.195676	27.234586
248.966510	10457.623434	27.239604
249.370523	10475.140072	27.244621
249.638607	10483.513816	27.249639
250.236352	10499.642366	27.254656
249.888299	10514.596731	27.259674
250.197673	10520.195135	27.264692
250.206015	10531.365320	27.269709
249.943557	10542.360278	27.274727
250.544597	10557.197235	27.279744
250.855654	10581.819997	27.284762
250.697130	10595.585713	27.289780
251.141341	10615.688211	27.294797
251.376064	10636.402210	27.299815
251.816569	10639.935423	27.304832
251.760384	10673.062984	27.309850
251.890722	10689.224138	27.314868
252.432133	10710.598868	27.319885
252.379461	10734.706500	27.324903
252.657637	10756.766665	27.329920
253.160309	10773.974749	27.334938
253.340753	10794.344627	27.339956
253.605193	10811.950410	27.344973
254.057134	10840.696124	27.349991
254.414757	10848.400581	27.355008
254.429967	10868.271542	27.360026
255.035808	10876.482265	27.365044
255.377468	10892.968060	27.370061
255.401026	10909.436893	27.375079
256.102998	10923.626514	27.380096
256.190380	10945.707924	27.385114
256.573914	10951.143554	27.390132
256.727424	10962.403858	27.395149
256.616384	10988.038640	27.400167
256.927667	10989.537530	27.405184
257.319929	11014.420375	27.410202
257.497076	11028.700446	27.415220
258.154824	11047.658548	27.420237
258.093902	11056.526598	27.425255
258.596068	11076.999640	27.430272
258.614086	11087.687207	27.435290
259.110553	11104.470464	27.440308
259.270689	11112.476894	27.445325
259.804106	11131.834876	27.450343
259.833696	11139.781652	27.455360
260.138992	11154.678149	27.460378
260.351268	11171.828693	27.465396
260.659272	11172.761044	27.470413
260.472058	11182.517433	27.475431
261.103454	11202.594025	27.480448
261.362985	11218.417372	27.485466
261.595974	11231.307624	27.490484
261.784720	11253.910895	27.495501
261.691662	11268.937708	27.500519
262.336131	11274.147490	27.505536
262.928812	11293.724682	27.510554
262.907190	11296.054101	27.515572
263.839268	11292.663746	27.520589
263.874096	11316.715066	27.525607
264.164320	11318.710450	27.530624
264.294906	11312.941216	27.535642
264.401794	11314.724979	27.540660
264.980756	11322.432965	27.545677
264.927625	11339.832613	27.550695
265.168825	11338.444307	27.555712
265.285552	11353.674871	27.560730
265.400194	11363.434813	27.565748
265.677595	11365.756523	27.570765
265.813244	11384.987567	27.575783
266.245106	11409.086331	27.580800
266.468274	11412.215184	27.585818
266.692372	11429.963498	27.590836
266.957583	11443.360199	27.595853
266.913565	11470.377065	27.600871
267.488844	11473.202267	27.605888
267.732679	11492.484285	27.610906
267.818822	11501.663860	27.615924
268.308049	11519.607519	27.620941
268.672095	11537.981815	27.625959
268.616428	11554.907895	27.630976
268.853366	11574.164356	27.635994
269.191437	11590.597373	27.641012
269.804457	11602.212888	27.646029
269.805967	11612.641553	27.651047
270.506924	11627.253687	27.656064
270.677112	11640.392787	27.661082
270.640849	11664.904633	27.666100
271.318734	11670.714307	27.671117
271.210854	11694.011327	27.676135
271.776319	11701.257275	27.681152
272.398950	11701.409875	27.686170
272.640193	11716.621349	27.691188
272.628760	11714.605627	27.696205
273.012700	11732.446291	27.701223
273.653256	11734.421702	27.706240
273.919696	11747.829104	27.711258
273.825696	11751.942475	27.716276
274.092423	11746.420563	27.721293
274.537090	11773.970074	27.726311
274.789288	11778.135707	27.731328
274.886025	11780.517764	27.736346
274.900439	11800.369216	27.741364
275.378896	11807.547621	27.746381
275.250028	11829.352114	27.751399
275.660916	11848.292134	27.756416
275.903872	11852.902006	27.761434
275.871422	11879.648567	27.766452
276.144301	11889.471782	27.771469
276.271444	11911.745825	27.776487
276.766092	11939.401406	27.781504
277.338814	11957.263603	27.786522
277.097602	11984.689249	27.791540
277.576619	11998.429585	27.796557
277.668972	12019.168565	27.801575
278.062331	12032.006586	27.806592
278.503133	12053.103894	27.811610
278.669621	12079.881082	27.816628
278.797340	12091.423206	27.821645
279.375845	12111.016510	27.826663
279.393447	12127.887470	27.831680
279.579323	12141.318491	27.836698
280.057314	12151.695978	27.841716
280.794622	12171.112922	27.846733
280.843142	12186.143656	27.851751
281.505379	12190.466603	27.856768
281.919507	12203.294769	27.861786
281.814072	12214.861752	27.866804
282.121052	12227.902617	27.871821
282.617966	12236.130666	27.876839
282.729044	12250.082975	27.881856
283.074848	12245.607550	27.886874
283.240820	12264.544035	27.891892
283.681755	12263.889289	27.896909
283.772457	12292.686293	27.901927
283.766008	12303.463429	27.906944
284.443260	12310.335289	27.911962
284.273081	12334.919937	27.916980
284.774957	12349.205773	27.921997
284.821028	12359.934434	27.927015
285.167066	12387.787690	27.932032
285.398757	12402.710925	27.937050
285.381939	12424.266009	27.942068
285.701949	12445.319164	27.947085
286.058681	12468.069458	27.952103
286.312105	12492.606125	27.957120
286.746771	12521.810982	27.962138
286.818471	12543.645530	27.967156
287.387386	12569.193883	27.972173
287.581677	12587.770863	27.977191
287.927756	12597.694250	27.982208
288.796940	12612.802600	27.987226
289.100403	12626.265095	27.992244
289.438495	12633.499526	27.997261
289.587315	12663.024535	28.002279
289.902354	12676.213370	28.007296
290.309367	12669.036329	28.012314
290.203644	12691.512161	28.017332
290.533721	12699.180929	28.022349
290.738191	12728.236419	28.027367
290.836264	12740.942737	28.032384
291.484021	12764.815413	28.037402
291.404307	12781.790966	28.042420
291.656752	12796.112849	28.047437
292.112915	12828.533036	28.052455
292.239484	12846.770942	28.057472
292.710196	12862.082086	28.062490
293.066355	12877.716723	28.067508
293.413152	12895.820995	28.072525
293.402243	12920.754705	28.077543
293.647745	12936.971137	28.082560
293.821152	12955.763345	28.087578
294.172342	12977.697132	28.092596
294.384885	12997.614008	28.097613
294.918598	13014.894285	28.102631
295.144043	13036.227128	28.107648
295.679044	13050.945322	28.112666
296.070910	13072.294320	28.117684
295.984175	13077.091426	28.122701
296.444949	13103.783069	28.127719
296.678930	13126.366765	28.132736
297.016091	13139.357750	28.137754
297.265803	13163.386793	28.142772
298.129450	13163.551288	28.147789
298.518457	13185.544486	28.152807
298.913759	13201.701410	28.157824
299.235311	13201.356618	28.162842
299.175917	13219.598437	28.167860
299.453134	13227.856635	28.172877
299.757108	13231.951348	28.177895
299.705646	13261.604391	28.182912
300.282253	13263.870937	28.187930
300.184526	13292.716787	28.192948
300.577399	13307.012735	28.197965
300.846846	13322.731218	28.202983
300.749483	13339.926382	28.208000
301.381724	13355.940518	28.213018
301.473514	13388.044094	28.218036
301.932244	13410.463882	28.223053
302.462449	13424.476215	28.228071
302.645345	13448.022200	28.233088
302.745536	13470.482297	28.238106
302.951444	13500.474797	28.243124
303.494716	13522.441040	28.248141
303.620303	13542.801308	28.253159
303.636087	13575.382719	28.258176
304.344505	13598.083962	28.263194
304.626824	13630.074532	28.268212
304.947867	13653.335992	28.273229
305.325896	13672.264633	28.278247
305.497870	13701.268017	28.283264
305.849599	13715.652185	28.288282
305.693159	13752.679178	28.293300
306.491168	13770.371814	28.298317
307.103447	13792.010108	28.303335
306.745249	13827.661626	28.308352
307.549667	13847.368474	28.313370
307.839300	13871.988183	28.318388
307.931909	13891.760495	28.323405
308.687454	13910.302473	28.328423
308.976504	13922.861058	28.333440
309.589826	13930.605355	28.338458
309.754416	13955.390860	28.343476
310.331869	13965.075166	28.348493
310.701205	13975.000276	28.353511
310.773071	13987.358448	28.358528
311.249861	13997.263593	28.363546
311.587980	14007.012837	28.368564
311.944609	13997.964922	28.373581
312.146585	14016.057495	28.378599
312.149538	14031.703167	28.383616
312.605593	14034.185655	28.388634
313.038689	14051.724530	28.393652
313.068953	14059.288757	28.398669
313.349711	14067.776420	28.403687
313.656030	14092.417540	28.408704
313.982014	14097.745305	28.413722
313.952232	14119.210280	28.418740
314.045975	14140.970485	28.423757
314.624313	14155.508967	28.428775
314.797587	14177.013887	28.433792
315.262696	14191.690797	28.438810
315.634404	14220.860334	28.443828
316.028443	14237.776951	28.448845
316.165903	14254.351888	28.453863
316.587193	14280.547076	28.458880
317.350280	14292.670553	28.463898
317.555822	14309.073514	28.468916
317.667826	14329.686152	28.473933
318.037673	14341.336633	28.478951
318.231954	14365.552347	28.483968
318.748151	14375.607429	28.488986
319.236811	14384.221547	28.494004
319.551796	14390.203883	28.499021
319.752798	14404.239477	28.504039
319.960278	14421.412164	28.509056
320.119391	14440.333942	28.514074
320.602899	14457.380017	28.519092
320.909431	14481.722974	28.524109
320.896249	14492.217942	28.529127
321.477793	14522.912261	28.534144
321.636655	14537.285334	28.539162
321.883478	14562.067178	28.544180
322.124770	14584.130610	28.549197
322.466874	14609.467407	28.554215
322.845902	14628.811757	28.559232
323.260758	14651.838274	28.564250
323.759619	14673.390602	28.569268
323.876952	14695.189066	28.574285
324.029303	14718.198182	28.579303
324.129610	14747.294874	28.584320
324.654023	14759.120313	28.589338
324.934450	14790.965016	28.594356
324.966367	14829.946888	28.599373
325.558786	14842.959756	28.604391
325.898912	14878.707493	28.609408
326.233550	14904.888726	28.614426
326.612417	14918.327355	28.619444
326.871293	14951.379840	28.624461
327.117286	14976.202733	28.629479
327.616225	15011.844480	28.634496
328.143849	15034.861276	28.639514
328.156415	15056.295715	28.644532
328.360254	15085.789271	28.649549
328.841136	15090.826898	28.654567
329.340972	15116.484413	28.659584
329.461357	15134.901495	28.664602
329.939782	15159.085181	28.669620
330.318208	15189.858574	28.674637
330.497182	15202.145348	28.679655
330.640215	15222.634967	28.684672
330.899704	15239.971710	28.689690
331.562387	15272.373713	28.694708
331.409412	15305.344295	28.699725
332.354537	15321.776902	28.704743
332.229857	15350.110517	28.709760
332.460729	15379.975665	28.714778
332.763729	15406.632410	28.719796
333.125241	15438.994391	28.724813
333.597344	15464.762209	28.729831
333.638755	15494.298770	28.734848
334.374529	15520.207112	28.739866
334.970726	15544.211832	28.744884
335.092362	15568.758888	28.749901
335.477192	15589.237817	28.754919
335.598110	15611.173602	28.759936
336.264084	15633.693721	28.764954
336.764841	15659.235084	28.769972
337.232223	15680.456586	28.774989
337.820237	15692.828151	28.780007
338.105161	15716.054705	28.785024
338.535888	15741.631969	28.790042
338.780188	15745.619665	28.795060
338.780228	15767.533801	28.800077
339.377570	15775.033494	28.805095
339.417717	15810.191027	28.810112
339.642421	15835.853243	28.815130
340.491914	15852.951981	28.820148
340.881366	15860.285462	28.825165
341.679667	15861.828289	28.830183
342.058129	15877.183442	28.835200
342.366478	15888.986817	28.840218
342.876126	15894.308086	28.845236
342.658649	15896.087005	28.850253
343.315742	15925.333381	28.855271
343.531331	15925.960143	28.860288
343.714825	15940.678792	28.865306
344.201823	15959.972973	28.870324
344.380646	15958.948696	28.875341
344.480349	15990.220028	28.880359
344.496891	16007.487115	28.885376
344.782101	16024.135285	28.890394
345.168196	16054.460613	28.895412
344.969657	16076.265116	28.900429
345.649136	16102.451301	28.905447
345.606058	16135.420507	28.910464
345.847589	16169.527182	28.915482
346.396645	16189.175110	28.920500
346.676546	16219.425568	28.925517
347.325974	16250.449597	28.930535
347.316196	16279.223252	28.935552
347.581338	16305.317166	28.940570
348.002316	16328.445213	28.945588
348.353179	16365.289572	28.950605
348.765089	16388.592367	28.955623
349.136808	16414.195111	28.960640
349.225662	16442.174085	28.965658
350.118885	16470.211520	28.970676
350.510910	16495.894228	28.975693
350.985954	16510.518142	28.980711
351.313806	16547.083947	28.985728
351.710681	16570.358312	28.990746
351.874993	16578.383088	28.995764
352.258107	16615.107951	29.000781
352.555789	16632.008710	29.005799
352.954947	16661.699530	29.010816
353.280587	16687.436440	29.015834
353.477366	16719.057136	29.020852
353.607606	16744.783748	29.025869
354.359317	16767.691843	29.030887
354.704063	16802.730062	29.035904
355.108607	16830.438772	29.040922
355.514097	16850.546619	29.045940
355.480724	16886.080694	29.050957
355.926604	16906.676638	29.055975
356.287569	16938.736751	29.060992
356.620973	16972.463841	29.066010
357.433712	17000.392042	29.071028
357.615461	17028.270463	29.076045
358.094237	17042.214790	29.081063
358.319748	17069.791443	29.086080
358.735062	17103.406556	29.091098
359.305784	17116.835136	29.096116
359.621121	17140.937891	29.101133
359.772465	17168.009628	29.106151
360.321992	17188.268183	29.111168
360.640114	17211.239145	29.116186
360.873658	17226.652201	29.121204
361.497607	17271.716755	29.126221
362.389212	17267.174376	29.131239
362.591365	17296.843284	29.136256
362.708061	17314.732070	29.141274
363.480187	17329.611380	29.146292
363.371503	17352.178139	29.151309
363.584432	17371.073678	29.156327
364.157090	17392.089427	29.161344
364.359691	17414.914538	29.166362
364.816992	17435.526297	29.171380
365.238933	17456.048839	29.176397
365.897181	17472.618455	29.181415
366.427403	17495.024551	29.186432
366.738979	17500.793692	29.191450
367.304075	17509.229486	29.196468
367.631129	17525.479896	29.201485
367.888535	17530.048640	29.206503
368.449380	17538.763472	29.211520
368.528779	17536.060667	29.216538
368.690767	17559.359387	29.221556
368.842821	17579.205423	29.226573
369.307815	17587.567056	29.231591
369.332822	17606.204642	29.236608
369.582097	17639.138722	29.241626
370.176937	17642.006885	29.246644
370.108883	17669.012491	29.251661
370.400933	17694.510366	29.256679
370.781414	17725.442226	29.261696
371.048466	17752.419378	29.266714
371.292979	17779.002529	29.271732
371.408457	17831.445049	29.276749
372.022877	17849.077968	29.281767
372.553785	17889.605956	29.286784
372.716669	17922.660704	29.291802
373.779411	17943.333748	29.296820
374.225702	17960.319955	29.301837
374.538300	17992.329717	29.306855
374.904739	18020.497424	29.311872
375.190676	18041.701089	29.316890
375.437996	18060.958924	29.321908
375.757359	18098.148258	29.326925
376.420514	18128.956740	29.331943
376.899556	18143.221321	29.336960
376.773815	18177.427752	29.341978
377.343416	18198.845491	29.346996
377.714355	18230.693686	29.352013
378.275960	18253.128163	29.357031
378.469374	18279.421483	29.362048
378.954468	18314.140345	29.367066
379.131865	18333.240363	29.372084
379.476361	18363.209503	29.377101
379.850191	18395.006783	29.382119
380.037125	18424.336159	29.387136
380.169388	18464.935472	29.392154
380.740449	18493.417901	29.397172
380.801821	18539.016356	29.402189
381.193957	18577.631534	29.407207
381.710047	18610.442075	29.412224
381.857181	18650.105193	29.417242
383.109902	18679.802254	29.422260
384.043259	18690.575439	29.427277
384.832223	18706.666467	29.432295
385.768979	18703.671319	29.437312
385.852766	18713.460145	29.442330
386.189779	18731.352069	29.447348
386.744847	18738.450680	29.452365
387.015454	18751.458793	29.457383
387.590261	18757.653421	29.462400
387.622005	18771.643378	29.467418
388.137315	18777.909703	29.472436
388.448648	18781.040995	29.477453
388.432533	18787.954644	29.482471
389.120244	18789.678231	29.487488
388.948803	18807.967429	29.492506
389.479986	18813.637498	29.497524
389.946495	18829.072113	29.502541
389.918349	18841.256585	29.507559
390.627294	18862.647920	29.512576
390.468276	18876.919175	29.517594
391.054699	18890.216869	29.522612
391.019125	18924.761382	29.527629
391.001542	18949.323962	29.532647
391.978743	18975.813666	29.537664
391.997643	19012.350642	29.542682
392.611379	19037.338396	29.547700
392.859162	19070.754128	29.552717
393.187406	19109.981647	29.557735
393.454946	19135.676751	29.562752
393.938579	19175.782512	29.567770
394.145679	19205.440882	29.572788
394.757196	19235.656581	29.577805
395.039260	19273.903977	29.582823
395.549337	19292.463133	29.587840
395.710511	19338.031084	29.592858
396.420677	19363.173698	29.597876
396.806670	19397.597348	29.602893
397.293340	19423.865160	29.607911
398.089034	19440.988277	29.612928
398.458306	19473.605898	29.617946
399.126926	19485.824349	29.622964
399.477889	19519.654569	29.627981
399.862359	19535.420712	29.632999
400.507821	19563.609354	29.638016
400.822188	19588.722476	29.643034
400.840125	19606.978097	29.648052
401.397712	19631.334335	29.653069
401.714549	19652.708519	29.658087
402.292353	19669.887084	29.663104
402.441258	19705.056758	29.668122
403.272364	19722.873059	29.673140
403.433068	19750.657724	29.678157
403.781011	19769.952826	29.683175
404.349930	19790.734596	29.688192
404.438215	19815.325371	29.693210
405.023546	19836.545197	29.698228
405.576716	19855.279284	29.703245
406.097653	19873.491686	29.708263
406.715337	19893.833480	29.713280
407.049770	19911.397596	29.718298
407.212117	19941.637408	29.723316
407.832586	19954.064325	29.728333
407.656368	19980.793082	29.733351
408.437234	19996.410690	29.738368
408.552072	20016.565800	29.743386
408.614596	20038.232252	29.748404
409.206059	20070.551894	29.753421
409.195923	20099.258628	29.758439
409.347570	20118.562599	29.763456
409.837642	20161.965253	29.768474
410.376754	20191.540693	29.773492
410.573722	20226.720416	29.778509
410.809088	20263.580202	29.783527
411.101865	20294.291329	29.788544
411.567735	20335.497168	29.793562
412.133452	20372.291182	29.798580
412.766959	20406.345664	29.803597
412.738791	20450.649156	29.808615
413.764731	20473.273914	29.813632
414.061334	20509.924485	29.818650
414.642283	20530.444252	29.823668
415.223721	20574.294988	29.828685
415.328134	20599.146672	29.833703
415.924467	20625.987328	29.838720
416.095249	20661.361995	29.843738
416.520574	20694.911591	29.848756
417.111955	20726.795902	29.853773
417.417904	20765.343582	29.858791
418.037500	20795.213695	29.863808
418.367760	20831.490288	29.868826
419.041610	20869.881946	29.873844
419.275856	20886.864574	29.878861
419.632476	20935.043559	29.883879
420.090496	20960.422268	29.888896
420.146656	21002.233044	29.893914
420.582644	21019.645971	29.898932
421.505279	21064.353350	29.903949
421.547376	21102.787170	29.908967
421.925835	21130.231242	29.913984
422.005494	21169.764993	29.919002
422.968768	21214.010316	29.924020
423.604140	21234.831065	29.929037
423.936366	21268.768456	29.934055
424.593045	21305.450139	29.939072
424.980871	21329.207182	29.944090
425.466702	21367.403977	29.949108
425.899952	21388.994315	29.954125
426.114153	21419.703619	29.959143
426.895148	21442.085279	29.964160
427.448060	21473.081745	29.969178
428.477055	21482.616159	29.974196
428.958355	21507.330466	29.979213
429.088014	21525.425987	29.984231
429.987540	21533.646879	29.989248
430.410902	21548.023870	29.994266
430.743989	21567.105386	29.999284
430.956178	21586.681896	30.004301
431.254083	21604.141889	30.009319
431.631861	21612.912212	30.014336
431.995887	21636.965712	30.019354
432.321113	21655.620134	30.024372
432.578955	21668.982402	30.029389
432.654019	21698.209313	30.034407
433.377852	21715.297552	30.039424
433.361606	21732.279259	30.044442
433.416217	21768.425506	30.049460
434.116453	21792.882485	30.054477
434.422591	21831.209062	30.059495
435.147261	21856.920058	30.064512
435.350671	21892.894810	30.069530
435.493404	21914.645574	30.074548
436.145635	21942.727940	30.079565
436.245170	21991.047201	30.084583
437.109089	22027.370687	30.089600
437.378787	22062.902073	30.094618
437.873088	22090.806660	30.099636
438.481456	22129.816718	30.104653
438.799689	22165.882488	30.109671
439.340860	22193.761673	30.114688
439.640179	22222.070892	30.119706
439.871552	22256.426591	30.124724
440.712162	22292.303877	30.129741
440.961140	22334.552156	30.134759
441.086714	22370.585290	30.139776
441.865572	22399.429627	30.144794
442.188298	22448.451950	30.149812
442.721030	22478.646278	30.154829
442.904107	22520.759052	30.159847
444.093332	22539.540721	30.164864
445.274722	22559.716216	30.169882
445.463204	22578.214721	30.174900
446.369433	22591.264164	30.179917
446.604638	22627.239456	30.184935
447.009273	22635.508279	30.189952
447.459209	22666.493568	30.194970
447.592126	22692.645988	30.199988
448.077902	22714.392030	30.205005
448.391010	22736.657107	30.210023
448.846661	22760.225127	30.215040
448.811725	22790.092250	30.220058
448.935583	22820.095598	30.225076
449.732706	22837.386050	30.230093
450.176831	22881.513191	30.235111
450.751014	22907.594874	30.240128
451.315379	22941.148362	30.245146
451.752895	22981.099855	30.250164
452.146720	23008.238343	30.255181
452.455144	23048.726495	30.260199
452.971171	23075.901553	30.265216
453.372993	23113.153420	30.270234
453.243713	23152.630100	30.275252
453.995672	23182.834166	30.280269
454.386928	23222.520314	30.285287
454.752341	23259.387636	30.290304
455.580431	23294.012056	30.295322
455.795851	23326.657832	30.300340
456.484035	23352.277044	30.305357
456.697764	23386.871943	30.310375
456.901370	23415.197754	30.315392
457.278088	23458.405404	30.320410
457.393222	23495.468322	30.325428
457.760360	23527.267201	30.330445
458.245577	23568.438221	30.335463
458.856089	23616.078428	30.340480
459.998424	23637.606131	30.345498
460.549864	23679.077239	30.350516
460.973101	23704.291031	30.355533
461.486331	23744.398585	30.360551
462.106928	23773.695216	30.365568
462.584447	23796.307383	30.370586
462.771504	23842.933427	30.375604
463.235285	23859.818087	30.380621
463.667608	23899.676615	30.385639
463.965912	23935.788178	30.390656
464.622770	23967.574864	30.395674
464.825406	24009.121308	30.400692
465.307426	24040.363324	30.405709
465.185637	24092.553326	30.410727
466.140135	24137.626677	30.415744
466.378944	24171.904983	30.420762
466.583861	24226.669645	30.425780
467.585347	24257.362204	30.430797
468.180857	24303.725226	30.435815
468.643647	24353.010747	30.440832
469.235476	24387.672041	30.445850
470.126090	24419.694945	30.450868
471.175598	24434.467144	30.455885
471.754870	24465.946577	30.460903
472.694704	24477.132386	30.465920
472.968381	24488.852075	30.470938
473.544858	24505.439819	30.475956
474.003539	24512.206673	30.480973
474.085015	24524.972407	30.485991
474.449863	24549.202710	30.491008
474.594913	24578.009410	30.496026
475.218452	24604.179760	30.501044
475.618077	24626.965430	30.506061
475.875843	24667.124671	30.511079
476.215676	24697.775397	30.516096
476.543110	24729.310439	30.521114
476.528510	24764.169997	30.526132
477.195263	24802.053985	30.531149
477.530642	24835.137484	30.536167
478.128130	24881.044969	30.541184
478.947495	24918.006874	30.546202
478.961663	24962.374494	30.551220
479.675489	24996.871153	30.556237
479.520511	25045.000742	30.561255
479.806042	25085.704894	30.566272
480.559468	25134.300552	30.571290
480.607765	25183.761805	30.576308
481.479916	25221.033473	30.581325
481.925088	25260.660957	30.586343
482.104308	25309.947336	30.591360
482.743959	25353.749238	30.596378
483.556623	25396.587022	30.601396
485.080049	25415.250348	30.606413
485.725167	25437.823964	30.611431
486.368853	25464.424222	30.616448
486.977289	25472.197270	30.621466
487.363357	25503.231340	30.626484
487.595659	25519.648089	30.631501
488.261053	25547.331390	30.636519
488.271194	25570.020531	30.641536
488.808977	25605.204356	30.646554
489.104605	25638.054781	30.651572
489.699834	25654.125518	30.656589
489.780663	25697.525801	30.661607
489.967222	25727.067696	30.666624
490.773040	25767.999513	30.671642
491.008107	25812.962171	30.676660
491.443938	25849.504405	30.681677
491.726853	25894.833876	30.686695
492.124309	25938.891821	30.691712
493.022856	25984.452776	30.696730
493.221115	26034.559246	30.701748
494.040524	26070.365718	30.706765
494.548587	26112.952209	30.711783
495.128178	26160.164536	30.716800
495.811149	26186.594294	30.721818
495.941960	26231.458918	30.726836
496.409702	26274.635252	30.731853
497.230763	26311.674161	30.736871
497.852554	26359.188391	30.741888
498.283737	26398.487660	30.746906
498.861111	26439.823138	30.751924
499.458201	26467.346374	30.756941
499.833613	26507.173977	30.761959
500.207832	26551.282208	30.766976
500.988048	26584.790062	30.771994
500.908649	26630.143868	30.777012
501.728317	26673.661494	30.782029
502.391487	26699.269588	30.787047
502.686117	26750.354043	30.792064
503.435773	26785.725724	30.797082
503.983332	26823.488512	30.802100
504.451600	26846.770630	30.807117
505.124774	26883.795025	30.812135
505.345453	26925.283114	30.817152
506.135363	26955.883786	30.822170
506.852330	26984.001767	30.827188
507.063620	27010.077847	30.832205
508.101125	27039.783619	30.837223
508.215362	27079.522668	30.842240
508.987380	27097.118789	30.847258
509.639159	27127.691370	30.852276
510.219782	27141.332989	30.857293
510.865534	27177.959041	30.862311
510.665201	27194.101330	30.867328
511.307869	27208.231058	30.872346
511.843830	27253.735191	30.877364
511.947049	27265.710186	30.882381
512.290035	27310.261950	30.887399
512.568347	27351.524499	30.892416
512.885265	27383.699880	30.897434
513.484742	27428.086624	30.902452
513.889798	27465.058944	30.907469
514.631170	27503.200575	30.912487
515.171873	27546.482935	30.917504
515.688442	27587.429219	30.922522
516.374141	27629.653415	30.927540
516.822084	27659.714254	30.932557
517.266411	27703.901133	30.937575
518.063594	27735.945558	30.942592
518.476720	27779.242560	30.947610
519.204825	27821.468382	30.952628
519.513422	27850.836357	30.957645
520.143167	27886.465928	30.962663
520.463339	27934.738808	30.967680
520.943731	27984.828444	30.972698
521.490631	28018.763313	30.977716
522.032388	28042.583839	30.982733
522.612313	28082.692398	30.987751
523.128908	28129.820458	30.992768
523.872846	28155.509401	30.997786
524.361603	28207.768322	31.002804
524.671324	28250.893955	31.007821
525.583187	28290.833542	31.012839
525.609345	28339.293135	31.017856
526.150270	28384.782322	31.022874
526.728492	28423.175884	31.027892
526.973171	28462.949548	31.032909
527.735289	28507.450445	31.037927
527.842161	28557.145919	31.042944
528.631912	28610.432938	31.047962
528.898234	28648.303094	31.052980
529.406945	28713.593039	31.057997
529.900189	28757.234464	31.063015
530.297794	28809.902239	31.068032
530.692402	28863.407467	31.073050
531.787321	28919.444122	31.078068
531.921215	28981.939297	31.083085
532.582357	29026.917869	31.088103
533.177678	29075.273229	31.093120
534.069396	29122.974786	31.098138
535.290664	29159.948605	31.103156
535.956983	29196.490846	31.108173
537.000149	29207.472850	31.113191
537.975714	29236.886806	31.118208
538.726201	29243.517001	31.123226
539.137937	29250.111329	31.128244
539.430399	29288.560334	31.133261
540.000440	29288.171657	31.138279
540.508854	29316.303279	31.143296
540.834375	29334.935875	31.148314
540.959850	29351.523251	31.153332
541.188969	29371.061659	31.158349
541.912494	29399.422345	31.163367
542.153589	29437.879885	31.168384
542.421641	29468.848964	31.173402
542.546815	29515.545384	31.178420
543.095770	29551.451516	31.183437
543.656193	29594.693645	31.188455
544.149817	29625.488406	31.193472
545.032424	29673.520836	31.198490
545.746307	29715.288936	31.203508
545.689563	29760.267261	31.208525
546.413303	29785.252810	31.213543
546.780252	29851.094700	31.218560
547.135156	29893.799845	31.223578
547.822953	29938.045423	31.228596
548.427099	29989.201084	31.233613
548.958166	30042.983162	31.238631
549.477331	30090.091272	31.243648
550.038209	30133.922614	31.248666
550.758111	30190.089573	31.253684
551.050587	30244.621108	31.258701
552.064857	30283.505946	31.263719
553.011701	30331.898877	31.268736
553.297220	30368.562715	31.273754
553.814672	30407.791760	31.278772
554.563199	30442.241733	31.283789
554.954126	30490.942754	31.288807
555.388951	30539.851271	31.293824
555.981651	30582.458871	31.298842
556.363941	30632.515532	31.303860
556.813655	30677.406247	31.308877
557.440934	30725.085266	31.313895
557.569314	30780.543088	31.318912
558.097963	30841.136884	31.323930
558.592065	30891.682454	31.328948
558.797945	30962.542823	31.333965
559.649202	31008.190061	31.338983
560.210318	31076.442613	31.344000
560.621440	31126.697932	31.349018
561.338837	31195.402075	31.354036
561.822399	31243.403379	31.359053
562.756113	31299.445516	31.364071
563.362068	31365.271175	31.369088
563.601512	31403.207155	31.374106
564.598351	31461.239924	31.379124
565.381404	31502.785636	31.384141
565.945992	31558.403569	31.389159
566.713379	31607.017989	31.394176
567.003405	31652.348181	31.399194
567.632836	31691.285051	31.404212
568.165301	31734.425372	31.409229
568.756856	31769.591929	31.414247
569.076896	31809.615488	31.419264
569.731440	31853.148061	31.424282
570.619727	31884.814165	31.429300
571.525638	31930.564021	31.434317
571.834721	31965.574234	31.439335
572.133564	32005.596916	31.444352
572.698486	32043.455735	31.449370
573.657959	32097.663358	31.454388
573.718078	32142.274931	31.459405
574.684543	32190.224150	31.464423
575.095066	32238.990273	31.469440
575.257793	32282.602314	31.474458
576.074364	32319.185919	31.479476
576.545989	32379.799188	31.484493
577.100730	32428.790372	31.489511
577.761406	32478.541921	31.494528
578.225920	32530.169084	31.499546
578.697962	32577.189371	31.504564
579.314588	32636.234173	31.509581
580.365175	32674.190478	31.514599
581.410318	32701.252529	31.519616
582.535922	32738.029016	31.524634
583.321763	32758.217332	31.529652
583.909930	32805.421538	31.534669
584.335917	32841.308742	31.539687
584.541823	32866.479200	31.544704
585.411020	32888.914801	31.549722
586.009486	32914.350679	31.554740
586.010232	32962.424427	31.559757
586.774529	32991.188376	31.564775
587.311058	33038.798701	31.569792
587.770932	33080.827046	31.574810
588.356777	33117.986693	31.579828
588.524744	33174.697844	31.584845
588.942941	33224.266420	31.589863
589.554310	33269.106921	31.594880
589.846105	33321.728775	31.599898
590.417609	33376.308196	31.604916
590.637966	33445.099291	31.609933
591.309534	33494.524282	31.614951
592.292660	33552.654872	31.619968
592.714760	33604.363075	31.624986
593.358168	33667.427007	31.630004
593.986113	33729.825259	31.635021
594.184570	33788.552979	31.640039
594.687466	33853.184843	31.645056
595.177211	33921.060109	31.650074
596.075989	33975.412821	31.655092
596.480670	34043.645788	31.660109
597.107710	34101.877575	31.665127
597.938556	34167.101602	31.670144
598.512385	34218.215310	31.675162
599.217469	34266.360362	31.680180
600.018916	34319.293579	31.685197
600.604319	34367.716518	31.690215
601.317624	34415.165484	31.695232
601.906087	34451.545788	31.700250
603.208335	34497.816605	31.705268
603.495568	34548.131996	31.710285
604.190243	34591.078941	31.715303
604.998066	34631.928631	31.720320
605.686290	34667.357104	31.725338
606.473401	34704.374744	31.730356
606.696394	34737.087117	31.735373
607.413058	34767.755075	31.740391
607.666027	34827.359020	31.745408
608.009802	34869.891202	31.750426
609.016813	34906.864813	31.755444
609.154735	34957.851575	31.760461
610.001219	35005.683019	31.765479
610.655190	35048.552496	31.770496
611.303573	35098.659110	31.775514
612.024419	35144.043736	31.780532
612.857454	35190.030188	31.785549
613.255055	35234.467032	31.790567
613.522286	35293.494939	31.795584
614.136016	35338.649640	31.800602
614.796819	35384.180062	31.805620
615.407054	35445.764611	31.810637
616.091377	35490.897445	31.815655
616.185675	35546.190588	31.820672
616.397842	35617.582199	31.825690
617.442042	35668.149322	31.830708
618.688211	35724.840898	31.835725
619.527501	35776.869347	31.840743
620.128001	35820.482422	31.845760
620.421437	35876.295161	31.850778
621.223503	35918.607250	31.855796
621.400881	35975.971237	31.860813
622.098392	36032.696052	31.865831
622.853226	36077.360451	31.870848
622.896991	36142.474743	31.875866
623.742298	36195.938239	31.880884
624.070026	36263.472009	31.885901
624.755586	36325.345772	31.890919
625.503992	36393.992382	31.895936
626.134331	36458.574607	31.900954
627.163001	36518.578165	31.905972
627.742547	36576.069349	31.910989
628.179306	36629.861010	31.916007
629.059723	36688.283761	31.921024
629.759090	36750.295634	31.926042
630.350239	36797.025054	31.931060
630.978526	36864.754602	31.936077
631.478921	36917.955260	31.941095
632.108425	36971.487124	31.946112
632.180777	37027.912799	31.951130
633.817772	37068.770417	31.956148
634.354685	37121.054577	31.961165
634.804513	37165.589122	31.966183
635.702967	37214.061888	31.971200
636.220705	37258.322555	31.976218
636.926363	37291.700940	31.981236
637.349985	37346.901828	31.986253
637.824270	37393.340901	31.991271
638.617220	37446.540787	31.996288
639.146998	37504.104555	32.001306
639.994699	37549.778221	32.006324
640.386595	37600.521267	32.011341
641.137856	37650.765752	32.016359
641.755535	37693.852743	32.021376
642.582591	37748.577592	32.026394
643.116814	37797.578333	32.031412
643.757098	37845.993116	32.036429
644.579477	37888.661702	32.041447
645.014173	37936.396786	32.046464
645.420297	38007.643068	32.051482
646.228145	38052.562860	32.056500
646.757288	38103.101076	32.061517
647.696736	38160.683836	32.066535
648.590918	38208.966198	32.071552
649.245309	38265.724320	32.076570
649.840538	38313.830681	32.081588
650.244172	38365.383050	32.086605
651.133977	38420.943676	32.091623
652.059109	38469.354305	32.096640
652.130722	38526.925131	32.101658
652.663836	38577.667540	32.106676
653.514058	38632.022582	32.111693
653.879103	38694.457501	32.116711
654.946398	38737.702620	32.121728
656.065612	38790.086860	32.126746
656.878025	38838.082860	32.131764
657.368817	38888.063434	32.136781
658.055566	38935.433210	32.141799
658.878718	38978.306261	32.146816
659.055064	39038.564884	32.151834
659.926975	39080.525307	32.156852
660.369670	39136.626229	32.161869
660.580990	39190.886111	32.166887
661.322994	39246.066140	32.171904
662.054214	39307.699135	32.176922
662.315723	39370.004792	32.181940
662.715489	39433.663722	32.186957
663.385844	39492.315689	32.191975
664.036195	39567.060321	32.196992
664.241868	39644.725592	32.202010
665.160577	39707.342563	32.207028
665.888052	39775.921072	32.212045
666.296405	39850.082589	32.217063
667.159286	39911.985385	32.222080
667.910476	39982.986298	32.227098
668.458373	40049.768388	32.232116
669.207537	40113.339524	32.237133
669.952707	40187.297483	32.242151
670.800532	40235.569335	32.247168
671.403988	40305.374530	32.252186
672.767435	40351.505065	32.257204
673.759340	40394.206576	32.262221
674.132719	40453.385385	32.267239
674.692603	40487.826215	32.272256
674.988529	40546.260717	32.277274
675.807889	40604.321901	32.282292
676.322949	40664.024525	32.287309
676.705901	40734.062130	32.292327
677.673521	40790.728329	32.297344
678.095047	40851.796437	32.302362
678.695790	40921.437411	32.307380
679.384833	40980.350145	32.312397
679.809552	41051.429555	32.317415
681.018684	41113.221641	32.322432
681.537248	41188.055846	32.327450
682.366072	41249.158294	32.332468
683.008897	41313.198707	32.337485
683.611502	41381.292560	32.342503
684.330529	41444.904980	32.347520
684.593904	41527.341865	32.352538
685.599357	41585.524990	32.357556
686.542098	41657.729331	32.362573
687.341716	41724.793288	32.367591
688.021435	41782.445412	32.372608
689.390483	41829.014333	32.377626
690.608604	41879.799422	32.382644
691.084384	41934.797100	32.387661
691.258433	41983.155925	32.392679
692.485343	42040.441059	32.397696
693.008474	42099.153784	32.402714
693.695304	42149.169448	32.407732
694.135565	42201.725891	32.412749
694.422467	42264.631029	32.417767
695.154247	42332.515664	32.422784
695.650729	42398.845081	32.427802
696.618927	42455.475677	32.432820
697.191157	42512.178969	32.437837
697.499265	42591.822197	32.442855
698.422839	42648.056769	32.447872
698.722883	42722.607529	32.452890
699.445162	42796.268076	32.457908
700.430715	42875.505077	32.462925
701.071604	42950.043555	32.467943
701.587291	43019.473124	32.472960
702.125212	43091.088640	32.477978
702.964346	43160.278006	32.482996
703.674352	43223.504113	32.488013
703.798650	43314.495139	32.493031
705.121599	43380.453832	32.498048
705.766924	43458.205105	32.503066
706.198492	43527.091744	32.508084
706.997961	43609.418500	32.513101
707.922353	43676.271431	32.518119
708.196389	43736.458399	32.523136
708.733230	43818.414707	32.528154
709.438265	43882.420041	32.533172
710.158763	43965.679054	32.538189
711.212300	44032.960756	32.543207
712.003533	44090.085457	32.548224
712.500210	44162.412294	32.553242
713.599817	44240.946503	32.558260
714.724977	44299.334233	32.563277
715.374639	44358.220596	32.568295
716.272509	44429.478315	32.573312
716.889822	44491.619644	32.578330
717.831367	44544.346292	32.583348
718.768775	44610.156525	32.588365
719.638373	44661.194570	32.593383
720.327859	44724.110774	32.598400
721.158775	44771.300165	32.603418
721.903042	44831.640042	32.608436
722.911850	44874.674919	32.613453
723.824917	44932.884019	32.618471
723.948440	44973.750762	32.623488
724.371313	45042.922408	32.628506
725.101898	45094.949235	32.633524
725.885770	45157.173684	32.638541
726.186030	45229.652948	32.643559
727.632509	45283.238441	32.648576
728.180960	45345.261271	32.653594
728.939902	45414.977158	32.658612
729.864493	45464.453434	32.663629
730.303272	45533.062913	32.668647
730.910275	45597.323618	32.673664
731.501048	45653.393753	32.678682
732.357479	45711.522973	32.683700
732.898099	45776.164033	32.688717
733.107813	45849.767670	32.693735
733.882013	45924.250330	32.698752
734.836951	45996.467633	32.703770
736.000031	46064.496939	32.708788
736.602124	46127.577239	32.713805
737.216603	46206.541426	32.718823
738.218846	46273.934592	32.723840
738.499473	46346.516248	32.728858
739.038788	46413.794346	32.733876
740.012429	46483.716935	32.738893
740.635596	46569.338615	32.743911
741.533500	46638.964678	32.748928
742.140094	46711.353964	32.753946
742.968279	46782.077060	32.758964
743.823034	46861.425570	32.763981
744.823175	46937.652912	32.768999
745.546823	46989.235279	32.774016
745.927499	47061.210777	32.779034
746.805573	47131.242656	32.784052
747.656153	47186.023704	32.789069
748.079833	47265.855996	32.794087
748.823243	47320.313759	32.799104
749.722408	47388.737285	32.804122
750.308699	47464.108299	32.809140
750.422589	47523.948827	32.814157
751.073999	47612.025880	32.819175
752.210138	47678.412347	32.824192
752.878012	47760.738555	32.829210
753.418839	47838.816203	32.834228
754.045830	47913.800859	32.839245
755.037619	48000.333179	32.844263
755.788959	48085.531612	32.849280
756.822120	48157.041674	32.854298
757.277437	48240.962716	32.859316
758.296646	48315.687843	32.864333
758.886265	48404.024796	32.869351
760.009490	48471.523856	32.874368
760.918859	48545.645817	32.879386
761.724711	48622.555072	32.884404
762.482298	48679.788426	32.889421
763.305656	48767.932206	32.894439
764.330350	48838.133678	32.899456
765.090116	48906.320201	32.904474
765.760068	48980.037161	32.909492
767.363323	49038.083710	32.914509
767.996053	49098.295038	32.919527
768.857437	49157.343633	32.924544
769.497850	49222.631469	32.929562
770.000169	49292.958919	32.934580
770.881491	49347.808035	32.939597
771.983962	49416.592015	32.944615
772.824023	49477.049315	32.949632
773.435959	49540.342183	32.954650
773.988139	49607.548325	32.959668
774.976286	49667.660823	32.964685
775.196620	49735.819636	32.969703
776.319287	49800.051407	32.974720
776.735787	49876.068735	32.979738
777.333273	49952.622448	32.984756
778.581334	50015.632710	32.989773
779.057078	50085.440509	32.994791
779.675242	50160.385552	32.999808
780.881036	50228.682859	33.004826
781.317309	50301.375835	33.009844
782.242369	50379.807408	33.014861
782.594479	50453.783025	33.019879
783.139693	50524.799617	33.024896
784.459996	50601.591342	33.029914
784.688970	50688.867238	33.034932
785.914726	50759.173664	33.039949
786.579407	50839.191908	33.044967
787.245495	50919.560588	33.049984
788.413988	50994.973800	33.055002
789.463816	51052.158783	33.060020
790.863428	51106.050305	33.065037
791.553460	51166.884356	33.070055
792.235512	51210.728347	33.075072
792.881500	51262.802562	33.080090
793.082978	51329.259917	33.085108
793.967743	51376.041795	33.090125
794.692796	51439.541136	33.095143
796.255212	51506.167541	33.100160
796.895187	51555.624098	33.105178
797.571894	51630.509160	33.110196
798.112512	51686.928259	33.115213
798.817573	51751.665887	33.120231
799.210963	51820.114360	33.125248
800.244448	51887.959394	33.130266
800.529391	51980.231828	33.135284
801.534547	52034.075311	33.140301
801.853567	52116.189928	33.145319
803.011249	52203.855565	33.150336
803.843042	52274.678805	33.155354
804.821244	52352.072172	33.160372
805.643450	52428.774257	33.165389
806.471641	52507.558779	33.170407
807.173629	52576.406017	33.175424
808.343220	52660.956842	33.180442
808.671974	52745.064317	33.185460
809.927615	52811.911670	33.190477
810.575485	52881.699766	33.195495
811.143910	52967.875327	33.200512
811.986908	53055.229062	33.205530
812.712999	53140.218846	33.210548
813.395258	53222.918231	33.215565
813.936870	53310.744111	33.220583
814.807676	53402.419219	33.225600
815.863083	53489.861179	33.230618
816.104044	53586.315145	33.235636
817.176104	53673.922627	33.240653
818.384931	53768.496977	33.245671
819.406827	53854.762387	33.250688
820.245335	53943.434170	33.255706
820.719555	54018.897933	33.260724
821.417732	54110.976550	33.265741
822.400870	54204.623222	33.270759
823.606803	54286.328722	33.275776
825.696056	54335.871539	33.280794
826.482669	54402.332254	33.285812
827.634846	54462.160045	33.290829
828.364078	54527.673934	33.295847
829.135896	54591.814506	33.300864
830.022219	54659.522898	33.305882
830.404047	54727.693779	33.310900
831.177848	54785.133379	33.315917
831.899826	54865.384424	33.320935
832.339151	54930.642871	33.325952
833.268584	55006.739028	33.330970
833.700752	55087.182375	33.335988
834.344230	55140.909575	33.341005
835.010621	55226.786668	33.346023
835.229183	55303.385467	33.351040
836.683872	55369.926459	33.356058
837.285931	55464.764017	33.361076
838.061978	55537.439713	33.366093
839.601062	55601.837358	33.371111
840.576007	55675.302685	33.376128
841.410601	55740.406405	33.381146
842.215499	55823.890401	33.386164
842.851418	55890.374198	33.391181
843.970272	55965.626598	33.396199
844.018457	56050.889359	33.401216
844.997379	56135.098384	33.406234
845.629851	56211.780307	33.411252
846.583550	56302.648643	33.416269
847.481490	56384.519874	33.421287
848.013320	56485.545475	33.426304
848.910069	56561.807974	33.431322
849.512491	56652.475082	33.436340
850.901292	56746.651058	33.441357
851.531775	56828.869893	33.446375
852.130272	56931.696233	33.451392
853.265581	57020.531405	33.456410
854.015157	57111.177347	33.461428
855.206166	57208.522014	33.466445
855.742130	57299.622753	33.471463
856.685125	57398.160191	33.476480
858.022190	57479.202400	33.481498
858.718461	57567.683882	33.486516
859.823260	57656.397531	33.491533
861.445650	57724.388393	33.496551
862.179675	57797.183878	33.501568
863.388716	57866.705929	33.506586
864.216024	57938.745211	33.511604
865.701125	58010.484346	33.516621
866.429730	58071.714150	33.521639
867.254330	58139.836667	33.526656
868.123570	58202.875655	33.531674
868.723717	58274.841897	33.536692
869.993550	58343.380506	33.541709
871.118017	58399.345392	33.546727
871.906014	58451.139691	33.551744
872.675870	58518.659820	33.556762
873.637413	58572.567413	33.561780
874.517263	58623.930826	33.566797
875.355062	58683.282519	33.571815
876.280124	58754.719015	33.576832
877.041949	58803.484365	33.581850
877.870497	58879.972498	33.586868
878.447823	58933.329779	33.591885
879.361451	59002.306383	33.596903
879.954536	59076.385910	33.601920
880.773746	59145.996901	33.606938
881.349744	59205.720284	33.611956
881.873373	59266.143644	33.616973
882.894162	59342.486262	33.621991
883.215677	59412.499499	33.627008
884.207318	59492.146790	33.632026
884.696111	59573.784653	33.637044
885.349544	59661.133635	33.642061
886.508144	59743.003483	33.647079
887.291341	59840.613141	33.652096
888.017381	59921.403309	33.657114
888.605031	60015.549726	33.662132
889.465467	60110.111037	33.667149
890.114776	60201.889955	33.672167
890.890488	60312.736242	33.677184
892.153876	60403.761667	33.682202
892.958246	60513.941505	33.687220
893.491233	60614.146288	33.692237
894.625433	60715.758929	33.697255
895.152697	60827.124579	33.702272
896.124905	60936.361328	33.707290
897.314681	61038.661542	33.712308
898.239630	61148.298586	33.717325
899.485931	61247.363840	33.722343
900.306705	61351.347507	33.727360
901.953840	61443.943104	33.732378
903.034294	61542.865790	33.737396
903.643552	61638.453646	33.742413
905.862034	61693.606982	33.747431
907.227716	61755.612689	33.752448
908.100808	61822.525181	33.757466
909.413367	61897.537096	33.762484
910.082305	61969.029767	33.767501
911.100058	62022.445748	33.772519
911.521274	62103.192748	33.777536
912.334973	62162.265625	33.782554
913.269847	62240.310496	33.787572
913.900820	62320.418744	33.792589
914.846648	62394.894164	33.797607
915.147742	62476.779746	33.802624
915.683550	62562.332512	33.807642
917.024370	62658.450159	33.812660
917.685113	62743.661758	33.817677
918.773406	62829.055180	33.822695
919.278080	62938.264221	33.827712
920.067499	63029.245114	33.832730
920.856245	63123.112928	33.837748
921.585694	63233.731086	33.842765
922.597678	63322.047367	33.847783
923.621546	63433.876721	33.852800
924.251177	63538.404936	33.857818
925.088634	63648.338812	33.862836
925.986133	63764.573588	33.867853
927.097090	63869.017550	33.872871
927.838197	63978.138082	33.877888
928.781703	64078.595887	33.882906
929.887452	64168.047567	33.887924
930.727003	64258.761071	33.892941
931.543384	64349.273410	33.897959
932.279330	64454.484518	33.902976
933.100347	64547.902587	33.907994
934.266406	64638.348021	33.913012
935.416412	64738.261645	33.918029
936.934741	64817.913902	33.923047
938.094543	64911.696728	33.928064
938.954978	64990.677456	33.933082
940.385431	65078.382580	33.938100
941.012138	65162.691335	33.943117
942.101541	65251.048435	33.948135
942.744166	65342.853284	33.953152
943.441247	65429.602874	33.958170
944.084002	65518.742902	33.963188
944.946793	65623.340148	33.968205
946.359748	65708.536872	33.973223
947.229363	65815.831343	33.978240
948.028057	65901.707808	33.983258
949.190376	66007.323869	33.988276
949.731862	66104.953652	33.993293
950.942596	66196.103653	33.998311
951.682711	66302.612870	34.003328
953.419312	66399.466506	34.008346
954.480225	66488.399193	34.013364
955.885668	66575.224426	34.018381
956.659384	66650.697689	34.023399
957.779637	66740.853928	34.028416
959.084056	66814.108206	34.033434
960.439125	66902.351648	34.038452
960.926729	66978.831925	34.043469
961.692574	67053.265675	34.048487
962.602044	67138.138210	34.053504
963.452358	67226.513980	34.058522
964.462095	67311.314466	34.063540
965.170269	67412.430425	34.068557
965.983606	67488.690317	34.073575
966.686035	67587.369601	34.078592
967.649694	67683.152349	34.083610
968.422187	67784.759088	34.088628
969.227831	67873.947228	34.093645
970.051165	67985.920235	34.098663
971.148252	68104.540620	34.103680
971.897470	68198.685872	34.108698
972.944897	68306.430190	34.113716
973.574847	68426.365111	34.118733
974.784915	68524.450326	34.123751
975.517786	68642.778143	34.128768
976.600740	68754.998555	34.133786
977.435813	68867.233779	34.138804
978.439059	68981.875259	34.143821
979.225702	69090.038142	34.148839
980.417416	69217.874333	34.153856
981.337415	69329.151005	34.158874
982.411313	69429.138857	34.163892
983.146927	69532.226324	34.168909
984.737292	69629.416281	34.173927
985.472236	69734.160243	34.178944
986.396947	69835.254293	34.183962
987.574464	69926.446018	34.188980
988.489720	70041.891143	34.193997
989.605961	70143.518625	34.199015
990.796721	70230.805001	34.204032
991.586116	70331.822040	34.209050
993.278682	70426.800929	34.214068
993.847745	70525.724749	34.219085
995.545854	70601.192590	34.224103
996.514648	70698.215038	34.229120
997.467685	70791.228273	34.234138
998.391541	70877.637492	34.239156
999.553279	70972.450728	34.244173
1000.662334	71056.600844	34.249191
1001.189799	71159.098091	34.254208
1002.142739	71254.173365	34.259226
1003.146371	71342.499089	34.264244
1003.969565	71444.495826	34.269261
1005.438824	71537.127152	34.274279
1006.373329	71639.726415	34.279296
1006.800799	71737.554094	34.284314
1007.961035	71845.299861	34.289332
1008.846327	71953.683920	34.294349
1009.614784	72066.143844	34.299367
1010.465215	72169.094115	34.304384
1011.315307	72286.824865	34.309402
1012.912882	72391.603648	34.314420
1013.919583	72502.069266	34.319437
1015.768629	72589.166546	34.324455
1016.919723	72699.730352	34.329472
1017.672312	72789.814909	34.334490
1018.764119	72897.861624	34.339508
1019.677292	73007.517123	34.344525
1020.366276	73102.245128	34.349543
1021.030779	73211.751732	34.354560
1021.887880	73328.274231	34.359578
1022.944631	73444.234830	34.364596
1023.568527	73573.131056	34.369613
1024.471201	73690.691099	34.374631
1025.417249	73810.741085	34.379648
1026.661429	73918.042343	34.384666
1028.337462	74021.420615	34.389684
1029.478784	74131.469379	34.394701
1030.761113	74237.451827	34.399719
1031.580258	74345.246393	34.404736
1032.610585	74458.588131	34.409754
1033.865233	74555.097290	34.414772
1034.848119	74682.066600	34.419789
1035.906908	74778.987170	34.424807
1036.841074	74879.972647	34.429824
1037.921018	74985.169669	34.434842
1038.993133	75086.121595	34.439860
1039.738934	75185.457505	34.444877
1040.734721	75276.829061	34.449895
1041.607748	75369.433973	34.454912
1042.582638	75470.169451	34.459930
1043.757488	75578.602896	34.464948
1044.697877	75682.030889	34.469965
1045.832390	75787.122288	34.474983
1046.703917	75882.674907	34.480000
1047.780365	75995.158414	34.485018
1048.986912	76091.606736	34.490036
1050.177715	76193.942053	34.495053
1051.665609	76285.195643	34.500071
1052.499728	76386.640650	34.505088
1053.439824	76493.093875	34.510106
1054.806091	76586.991060	34.515124
1055.486021	76698.220608	34.520141
1056.574295	76809.025550	34.525159
1057.513129	76903.794871	34.530176
1058.282982	77031.975743	34.535194
1058.924104	77145.603009	34.540212
1059.585121	77266.919736	34.545229
1061.029627	77387.493147	34.550247
1061.897171	77508.468752	34.555264
1063.071685	77646.834695	34.560282
1064.044782	77772.870494	34.565300
1064.922870	77895.888270	34.570317
1066.041704	78015.714468	34.575335
1067.318631	78154.016984	34.580352
1068.208256	78283.779471	34.585370
1069.527838	78417.026682	34.590388
1070.434028	78545.903277	34.595405
1071.595804	78672.685738	34.600423
1072.758267	78799.064332	34.605440
1073.920444	78925.273082	34.610458
1075.443615	79054.674182	34.615476
1076.272658	79182.043670	34.620493
1077.249765	79303.404329	34.625511
1078.748796	79421.686476	34.630528
1079.497353	79557.535061	34.635546
1080.664707	79677.236799	34.640564
1081.915534	79814.378881	34.645581
1083.053646	79930.041143	34.650599
1084.650887	80057.173735	34.655616
1085.559822	80173.379515	34.660634
1086.649733	80293.893629	34.665652
1087.467836	80421.828774	34.670669
1088.627993	80526.497911	34.675687
1089.920075	80642.196552	34.680704
1090.781937	80773.338220	34.685722
1091.546050	80896.278224	34.690740
1093.044799	81034.476252	34.695757
1093.795783	81148.797164	34.700775
1094.759708	81280.418879	34.705792
1095.507036	81412.082198	34.710810
1097.182173	81525.025448	34.715828
1097.824693	81641.819155	34.720845
1099.443277	81737.520390	34.725863
1100.565706	81855.478038	34.730880
1101.969114	81968.321506	34.735898
1102.738374	82075.507173	34.740916
1103.864666	82191.379868	34.745933
1104.945117	82306.621974	34.750951
1106.150861	82400.160245	34.755968
1106.976771	82533.841172	34.760986
1108.053833	82641.853224	34.766004
1109.131283	82764.179068	34.771021
1109.968089	82897.512859	34.776039
1111.378287	83003.950147	34.781056
1112.333601	83137.664911	34.786074
1113.538639	83252.234879	34.791092
1114.270305	83387.333443	34.796109
1115.313336	83512.261260	34.801127
1116.760678	83650.611178	34.806144
1117.521970	83776.217606	34.811162
1118.935707	83911.546134	34.816180
1120.224003	84034.699355	34.821197
1120.886274	84172.633816	34.826215
1122.267468	84302.109016	34.831232
1122.503985	84450.425143	34.836250
1124.108049	84587.219865	34.841268
1125.519862	84719.373558	34.846285
1127.207074	84858.059941	34.851303
1128.311893	84991.294762	34.856320
1129.172055	85132.877534	34.861338
1130.574507	85245.795609	34.866356
1131.791585	85384.585489	34.871373
1133.209136	85506.316686	34.876391
1134.287052	85633.236857	34.881408
1135.528531	85766.758300	34.886426
1136.597910	85886.789241	34.891444
1137.651307	86003.124388	34.896461
1139.167402	86128.295873	34.901479
1140.535304	86244.089111	34.906496
1141.830068	86362.746371	34.911514
1143.066717	86488.185717	34.916532
1144.389358	86596.292681	34.921549
1145.079627	86721.181633	34.926567
1146.314745	86839.060604	34.931584
1147.387534	86956.548694	34.936602
1148.434648	87080.061398	34.941620
1149.053945	87210.124381	34.946637
1150.096077	87345.552783	34.951655
1151.580883	87464.369293	34.956672
1152.733539	87608.615737	34.961690
1153.380725	87729.969872	34.966708
1154.626277	87865.679048	34.971725
1155.545513	87997.482347	34.976743
1156.676478	88143.000546	34.981760
1157.752032	88282.501989	34.986778
1158.660726	88399.903887	34.991796
1160.005015	88540.629017	34.996813
1160.811753	88666.067200	35.001831
1162.124622	88786.783869	35.006848
1162.608996	88945.747412	35.011866
1164.037124	89073.707251	35.016884
1165.019210	89212.799507	35.021901
1165.752358	89367.242828	35.026919
1166.802863	89503.859672	35.031936
1167.938688	89675.069623	35.036954
1168.941291	89817.261316	35.041972
1170.449074	89985.397904	35.046989
1172.404142	90110.193801	35.052007
1173.605221	90253.994767	35.057024
1175.079852	90396.722306	35.062042
1176.038748	90535.086722	35.067060
1177.207308	90686.004341	35.072077
1178.476697	90836.242892	35.077095
1179.478562	90980.927790	35.082112
1180.517524	91132.729226	35.087130
1181.653245	91280.708896	35.092148
1182.562746	91443.715012	35.097165
1183.825242	91596.413826	35.102183
1185.074262	91752.790530	35.107200
1186.021716	91927.235687	35.112218
1186.728692	92086.154971	35.117236
1187.880095	92253.296680	35.122253
1188.455359	92432.396885	35.127271
1190.127282	92615.410109	35.132288
1190.925154	92805.496100	35.137306
1192.182407	92971.861060	35.142324
1193.427409	93168.602653	35.147341
1194.276616	93343.023962	35.152359
1195.790501	93528.467094	35.157376
1196.652095	93726.362523	35.162394
1197.963638	93911.752460	35.167412
1199.587417	94101.484137	35.172429
1200.648983	94289.459779	35.177447
1202.085061	94476.200898	35.182464
1203.164841	94662.690272	35.187482
1204.562551	94845.525026	35.192500
1205.895277	95035.582893	35.197517
1207.170755	95214.929327	35.202535
1208.742306	95402.649750	35.207552
1209.970260	95580.165842	35.212570
1211.147380	95771.393314	35.217588
1212.159989	95936.851330	35.222605
1213.603677	96127.792721	35.227623
1214.776593	96296.264358	35.232640
1216.025719	96490.225636	35.237658
1217.409372	96659.817819	35.242676
1218.832803	96850.502822	35.247693
1219.729288	97021.256946	35.252711
1221.174233	97186.838802	35.257728
1222.085399	97368.284637	35.262746
1223.359938	97534.414876	35.267764
1224.920464	97701.285332	35.272781
1225.896995	97863.840303	35.277799
1227.151105	98010.687815	35.282816
1228.886049	98158.016558	35.287834
1230.626867	98318.833645	35.292852
1232.532596	98443.437211	35.297869
1233.946857	98578.735766	35.302887
1235.378019	98717.638663	35.307904
1236.892972	98850.702136	35.312922
1238.144394	98968.877055	35.317940
1239.406218	99101.741811	35.322957
1240.413338	99246.694178	35.327975
1241.853116	99365.821854	35.332992
1242.937148	99502.949889	35.338010
1244.052983	99624.199314	35.343028
1245.453716	99758.456688	35.348045
1246.229234	99903.513275	35.353063
1247.292964	100042.893845	35.358080
1248.600266	100179.655065	35.363098
1249.952949	100327.172375	35.368116
1251.433506	100462.313276	35.373133
1252.698830	100609.953838	35.378151
1253.587602	100748.069383	35.383168
1254.891690	100902.222734	35.388186
1255.883270	101047.315398	35.393204
1257.120836	101195.470281	35.398221
1258.000814	101355.034382	35.403239
1258.989492	101506.426168	35.408256
1260.217196	101675.162643	35.413274
1261.032311	101849.812608	35.418292
1262.622181	102015.178310	35.423309
1263.556032	102177.030054	35.428327
1264.707686	102356.717736	35.433344
1265.904086	102541.917485	35.438362
1266.626682	102722.644325	35.443380
1268.000372	102903.857532	35.448397
1269.251386	103107.606338	35.453415
1270.810567	103285.470839	35.458432
1271.966576	103469.849019	35.463450
1272.629112	103659.021492	35.468468
1274.051598	103854.611601	35.473485
1275.117705	104051.639521	35.478503
1276.507948	104245.814149	35.483520
1277.932991	104445.053776	35.488538
1279.414970	104640.672553	35.493556
1281.072035	104821.380776	35.498573
1282.133130	105033.555099	35.503591
1283.675070	105210.462208	35.508608
1285.846764	105384.315099	35.513626
1287.334464	105562.714318	35.518644
1289.234623	105727.499744	35.523661
1291.295386	105882.577940	35.528679
1292.597995	106020.329473	35.533696
1294.056141	106170.942354	35.538714
1295.155896	106314.778089	35.543732
1296.733450	106437.349913	35.548749
1297.424759	106586.878507	35.553767
1298.543585	106713.670052	35.558784
1299.451400	106864.457041	35.563802
1300.694613	107012.185407	35.568820
1301.769081	107168.953980	35.573837
1303.072886	107324.320044	35.578855
1303.891591	107475.352860	35.583872
1305.085690	107639.162378	35.588890
1306.109620	107806.082352	35.593908
1307.254752	107973.288010	35.598925
1308.612096	108143.309245	35.603943
1309.785736	108320.171186	35.608960
1311.259385	108492.340992	35.613978
1312.227917	108673.687628	35.618996
1313.464366	108843.669683	35.624013
1315.374524	109020.628505	35.629031
1316.747002	109195.199240	35.634048
1318.474684	109358.530430	35.639066
1319.809256	109537.768192	35.644084
1321.279250	109710.687739	35.649101
1322.488668	109875.161811	35.654119
1323.723662	110054.963536	35.659136
1325.229105	110234.521034	35.664154
1326.303476	110400.469608	35.669172
1327.886987	110575.510350	35.674189
1329.104772	110747.913926	35.679207
1330.567055	110914.665170	35.684224
1332.006780	111097.600611	35.689242
1333.013375	111274.358493	35.694260
1334.376193	111449.573442	35.699277
1335.625819	111637.221026	35.704295
1336.538670	111811.263015	35.709312
1338.170893	112000.947824	35.714330
1339.466782	112188.788457	35.719348
1340.743409	112371.031228	35.724365
1341.852679	112568.836675	35.729383
1343.179696	112749.972718	35.734400
1344.932792	112939.373250	35.739418
1345.817808	113140.782923	35.744436
1347.834183	113316.673115	35.749453
1348.986262	113494.468161	35.754471
1350.546617	113675.206633	35.759488
1352.405397	113858.779443	35.764506
1353.734570	114043.659607	35.769524
1355.214714	114221.711527	35.774541
1356.715141	114395.785714	35.779559
1357.621499	114572.456222	35.784576
1358.869011	114758.703082	35.789594
1360.100193	114952.930937	35.794612
1361.717175	115128.270499	35.799629
1363.024219	115307.053985	35.804647
1363.860963	115499.765952	35.809664
1365.045622	115688.106229	35.814682
1365.906582	115862.798619	35.819700
1367.360405	116046.768224	35.824717
1368.919149	116230.304614	35.829735
1369.891861	116420.963254	35.834752
1371.345180	116611.363318	35.839770
1372.407553	116805.448514	35.844788
1373.540315	116991.115782	35.849805
1374.884222	117180.138201	35.854823
1375.734467	117396.042041	35.859840
1377.736742	117594.036023	35.864858
1378.531297	117799.238976	35.869876
1380.160272	118000.296624	35.874893
1381.340772	118213.837405	35.879911
1382.832527	118433.871264	35.884928
1384.671632	118632.456341	35.889946
1385.443344	118858.667855	35.894964
1387.118465	119073.257853	35.899981
1388.713256	119279.035522	35.904999
1389.891409	119503.725342	35.910016
1392.033959	119702.162716	35.915034
1393.987401	119903.671106	35.920052
1395.450435	120117.720844	35.925069
1396.483783	120311.349315	35.930087
1397.779540	120522.110818	35.935104
1399.291604	120720.390153	35.940122
1400.639609	120948.408868	35.945140
1402.153775	121146.045167	35.950157
1403.588458	121346.621211	35.955175
1405.124243	121564.407356	35.960192
1406.757836	121760.876745	35.965210
1408.331601	121969.680510	35.970228
1409.562372	122168.420713	35.975245
1410.528401	122384.024354	35.980263
1411.912687	122605.148835	35.985280
1413.475323	122819.103307	35.990298
1414.589369	123033.726081	35.995316
1415.904865	123245.975358	36.000333
1417.383712	123470.055815	36.005351
1418.909537	123688.278900	36.010368
1420.104950	123917.753274	36.015386
1421.442271	124146.155744	36.020404
1422.781814	124358.777325	36.025421
1424.558102	124579.450475	36.030439
1426.063998	124802.511741	36.035456
1427.797910	125023.410588	36.040474
1428.869837	125258.527389	36.045492
1430.345204	125486.881254	36.050509
1431.855171	125695.179465	36.055527
1433.231731	125922.171971	36.060544
1434.994141	126143.582093	36.065562
1436.326529	126355.460428	36.070580
1438.096290	126572.021229	36.075597
1439.329602	126800.348557	36.080615
1440.671928	127016.524762	36.085632
1442.378636	127221.117034	36.090650
1443.426997	127439.902187	36.095668
1444.897615	127635.920865	36.100685
1446.363632	127830.852210	36.105703
1447.739569	128038.518129	36.110720
1449.193397	128235.797889	36.115738
1450.894561	128439.019236	36.120756
1452.415229	128647.046776	36.125773
1453.673390	128850.392207	36.130791
1454.905852	129062.218553	36.135808
1456.616451	129264.950369	36.140826
1457.759600	129476.540683	36.145844
1459.257164	129697.311959	36.150861
1461.296876	129897.259577	36.155879
1462.519325	130110.691772	36.160896
1463.741033	130325.265941	36.165914
1464.976942	130535.759964	36.170932
1466.468281	130756.147817	36.175949
1468.091351	130974.172598	36.180967
1469.427672	131197.451850	36.185984
1471.119371	131414.822978	36.191002
1472.300610	131653.524211	36.196020
1473.993043	131865.488658	36.201037
1476.004728	132070.321415	36.206055
1477.522797	132297.698218	36.211072
1479.274169	132499.483916	36.216090
1480.908006	132713.275837	36.221108
1483.619194	132889.963952	36.226125
1485.359758	133089.588907	36.231143
1486.978851	133283.532797	36.236160
1488.731739	133459.578453	36.241178
1490.148800	133660.424485	36.246196
1491.232323	133840.899554	36.251213
1492.935406	134034.011566	36.256231
1494.137659	134217.561830	36.261248
1495.759934	134401.882816	36.266266
1497.123444	134595.635410	36.271284
1498.276056	134784.772467	36.276301
1499.694547	134984.867216	36.281319
1501.232364	135172.817855	36.286336
1502.572452	135371.039682	36.291354
1503.967051	135582.521337	36.296372
1505.132340	135788.642828	36.301389
1506.678225	136003.676908	36.306407
1507.797943	136219.147762	36.311424
1509.042024	136432.268804	36.316442
1510.551690	136656.830065	36.321460
1511.646113	136880.191801	36.326477
1513.610790	137097.435675	36.331495
1515.082304	137330.726635	36.336512
1516.575681	137557.058801	36.341530
1517.819596	137774.929070	36.346548
1519.271237	138011.650137	36.351565
1520.662214	138240.741080	36.356583
1521.889221	138478.071824	36.361600
1523.463114	138695.807712	36.366618
1524.935349	138924.460125	36.371636
1526.298708	139149.443712	36.376653
1527.394787	139361.810929	36.381671
1528.290058	139609.582706	36.386688
1530.054997	139829.881844	36.391706
1532.018244	140067.792586	36.396724
1533.533178	140312.822948	36.401741
1535.212659	140532.633859	36.406759
1536.477823	140764.045330	36.411776
1538.445811	140994.307655	36.416794
1539.790367	141230.589516	36.421812
1541.484489	141474.409452	36.426829
1543.313494	141706.232815	36.431847
1544.410193	141947.781375	36.436864
1546.082428	142176.933596	36.441882
1547.977642	142414.987608	36.446900
1548.987113	142658.672266	36.451917
1550.809187	142899.301915	36.456935
1552.629379	143130.998037	36.461952
1554.695054	143371.136383	36.466970
1556.536016	143610.044799	36.471988
1558.107342	143831.734472	36.477005
1559.893043	144066.675224	36.482023
1561.276902	144300.426740	36.487040
1562.767406	144529.498547	36.492058
1564.340276	144767.026139	36.497076
1565.862663	144993.295016	36.502093
1567.888474	145228.181029	36.507111
1569.310258	145455.039627	36.512128
1570.992348	145695.307538	36.517146
1572.443779	145920.884532	36.522164
1574.047865	146162.359931	36.527181
1575.435248	146399.739197	36.532199
1576.654707	146637.552555	36.537216
1578.052651	146883.883156	36.542234
1580.227433	147117.504626	36.547252
1581.409997	147373.938277	36.552269
1582.845746	147610.393524	36.557287
1584.733352	147857.731382	36.562304
1586.535046	148088.338798	36.567322
1588.238350	148344.152411	36.572340
1589.600204	148574.389497	36.577357
1591.398126	148811.442595	36.582375
1592.871697	149061.137356	36.587392
1594.353038	149306.560582	36.592410
1596.256494	149544.477026	36.597428
1597.734056	149799.425259	36.602445
1599.123719	150040.000464	36.607463
1600.837018	150292.151413	36.612480
1602.378464	150542.556727	36.617498
1603.772302	150796.194891	36.622516
1605.597630	151053.696634	36.627533
1607.218232	151293.242818	36.632551
1608.597948	151548.435751	36.637568
1610.519864	151786.124692	36.642586
1612.048473	152019.427736	36.647604
1613.681208	152250.687347	36.652621
1615.287701	152458.839911	36.657639
1616.974593	152686.582026	36.662656
1618.260030	152929.717927	36.667674
1620.149704	153149.849182	36.672692
1621.470977	153380.468783	36.677709
1623.276786	153618.125873	36.682727
1624.706722	153856.059889	36.687744
1625.870692	154094.646428	36.692762
1627.847413	154336.909317	36.697780
1629.053507	154590.821787	36.702797
1630.720258	154826.949946	36.707815
1631.952474	155085.553334	36.712832
1633.186880	155337.121199	36.717850
1635.084526	155600.960904	36.722868
1636.443120	155871.215453	36.727885
1638.612914	156119.572030	36.732903
1640.537385	156389.614000	36.737920
1642.122943	156650.582304	36.742938
1644.732774	156885.814121	36.747956
1646.375926	157142.453090	36.752973
1648.038165	157389.517310	36.757991
1649.884090	157639.255042	36.763008
1651.887684	157876.897721	36.768026
1653.754813	158117.645074	36.773044
1655.141190	158376.033142	36.778061
1657.012385	158611.317896	36.783079
1658.373303	158840.433629	36.788096
1660.130881	159104.652025	36.793114
1662.082926	159339.662529	36.798132
1663.514980	159586.931027	36.803149
1665.191477	159833.934176	36.808167
1666.679851	160082.528722	36.813184
1668.412794	160332.544526	36.818202
1670.207325	160593.331539	36.823220
1671.501251	160851.904604	36.828237
1673.263642	161090.431580	36.833255
1675.323494	161328.152006	36.838272
1677.204679	161572.446190	36.843290
1679.095620	161811.972099	36.848308
1680.681243	162063.025270	36.853325
1682.033632	162307.966430	36.858343
1683.423009	162571.660263	36.863360
1685.088475	162815.857622	36.868378
1686.593935	163071.343931	36.873396
1687.640295	163346.372442	36.878413
1689.706572	163610.866765	36.883431
1691.236592	163880.952408	36.888448
1692.367254	164156.062392	36.893466
1694.191573	164425.851653	36.898484
1695.984618	164715.648764	36.903501
1697.513785	164977.181635	36.908519
1698.806200	165273.404101	36.913536
1700.587617	165544.781035	36.918554
1702.304225	165811.566214	36.923572
1703.426315	166081.136577	36.928589
1705.565909	166351.498564	36.933607
1707.091250	166614.654325	36.938624
1708.527887	166891.334071	36.943642
1710.393164	167149.924222	36.948660
1712.457925	167419.176910	36.953677
1714.052761	167684.371185	36.958695
1715.962225	167957.787306	36.963712
1717.801197	168225.242386	36.968730
1719.514468	168503.691099	36.973748
1721.325091	168777.407837	36.978765
1722.850641	169049.903359	36.983783
1724.823191	169322.063459	36.988800
1726.344468	169602.973349	36.993818
1728.268043	169878.367015	36.998836
1729.792432	170157.745596	37.003853
1731.478240	170435.679854	37.008871
1733.109201	170728.808614	37.013888
1734.807882	171022.842137	37.018906
1736.927736	171298.392255	37.023924
1737.909768	171599.292344	37.028941
1739.790067	171890.043422	37.033959
1741.487489	172189.248753	37.038976
1743.270244	172496.345832	37.043994
1745.370778	172795.783491	37.049012
1747.039369	173093.909245	37.054029
1748.672831	173384.824609	37.059047
1750.636300	173693.830429	37.064064
1752.251832	173990.791483	37.069082
1754.274037	174282.590370	37.074100
1755.998888	174579.830171	37.079117
1758.035108	174878.545054	37.084135
1759.703085	175188.471855	37.089152
1761.422473	175479.147578	37.094170
1763.604846	175782.260729	37.099188
1765.052350	176075.952482	37.104205
1766.878426	176385.913965	37.109223
1768.935672	176686.097631	37.114240
1770.494296	176997.336767	37.119258
1772.803746	177272.770634	37.124276
1774.715732	177580.570607	37.129293
1776.396561	177870.761749	37.134311
1778.427560	178157.334194	37.139328
1779.950922	178455.471188	37.144346
1781.896699	178749.660880	37.149364
1783.778538	179030.401354	37.154381
1786.058955	179318.401124	37.159399
1787.999882	179597.638827	37.164416
1789.276441	179890.128312	37.169434
1791.282834	180165.045493	37.174452
1792.992803	180451.976173	37.179469
1794.650024	180760.867338	37.184487
1796.423202	181041.904674	37.189504
1797.878680	181332.865644	37.194522
1799.480660	181608.312966	37.199540
1801.328820	181880.005268	37.204557
1802.917784	182153.415270	37.209575
1804.789339	182435.892429	37.214592
1806.269729	182736.666945	37.219610
1808.270135	183004.243612	37.224628
1809.891675	183292.057088	37.229645
1811.684686	183580.187801	37.234663
1813.711431	183865.999271	37.239680
1815.478827	184137.515217	37.244698
1817.611069	184429.493051	37.249716
1818.639097	184724.173203	37.254733
1820.370739	185001.943078	37.259751
1822.196739	185313.935345	37.264768
1824.031792	185611.005618	37.269786
1826.452357	185899.267227	37.274804
1828.438159	186202.573308	37.279821
1830.420223	186483.522893	37.284839
1832.539633	186779.121663	37.289856
1834.316806	187065.563880	37.294874
1836.188474	187370.443897	37.299892
1837.872160	187658.249727	37.304909
1839.585916	187962.917572	37.309927
1841.529270	188266.611883	37.314944
1843.092070	188561.764625	37.319962
1845.256681	188853.473456	37.324980
1846.734132	189159.480945	37.329997
1848.199114	189489.401120	37.335015
1850.223974	189793.346078	37.340032
1851.843824	190103.309133	37.345050
1853.777018	190420.204311	37.350068
1855.712461	190740.603856	37.355085
1857.735887	191051.904920	37.360103
1859.491401	191366.118648	37.365120
1861.459602	191685.694307	37.370138
1863.697389	191997.436940	37.375156
1865.867916	192317.555694	37.380173
1867.884119	192614.476061	37.385191
1870.092554	192924.071694	37.390208
1871.847526	193230.022653	37.395226
1873.996747	193533.971114	37.400244
1875.894452	193837.161773	37.405261
1877.747109	194135.018238	37.410279
1879.466368	194440.334962	37.415296
1881.454795	194754.723492	37.420314
1883.425732	195042.616166	37.425332
1885.459534	195335.158418	37.430349
1887.194179	195652.905343	37.435367
1889.133307	195942.953067	37.440384
1891.126011	196248.605243	37.445402
1892.462697	196549.717991	37.450420
1894.150380	196865.131746	37.455437
1896.031047	197171.530578	37.460455
1898.198271	197482.556534	37.465472
1900.158854	197785.303529	37.470490
1902.402168	198062.914152	37.475508
1904.337299	198340.663990	37.480525
1906.250302	198599.557426	37.485543
1908.975728	198870.279761	37.490560
1911.535701	199119.629614	37.495578
1913.659822	199365.292704	37.500596
1915.961057	199615.434798	37.505613
1917.413597	199863.161449	37.510631
1919.833474	200097.192213	37.515648
1921.311177	200352.431384	37.520666
1923.162376	200601.113565	37.525684
1925.280816	200851.937695	37.530701
1926.520970	201109.502864	37.535719
1928.123204	201369.080784	37.540736
1929.678880	201639.304382	37.545754
1931.684046	201918.965366	37.550772
1933.299706	202194.513391	37.555789
1934.840603	202481.613113	37.560807
1936.630856	202762.391360	37.565824
1938.243827	203070.211388	37.570842
1940.074947	203355.949337	37.575860
1942.056006	203652.416620	37.580877
1943.660755	203970.309038	37.585895
1946.015043	204256.412739	37.590912
1948.320532	204572.191619	37.595930
1950.380898	204867.954393	37.600948
1952.308737	205171.013470	37.605965
1954.373832	205478.444548	37.610983
1956.107797	205774.390640	37.616000
1957.745421	206091.464270	37.621018
1959.971430	206411.861032	37.626036
1961.682678	206724.242095	37.631053
1963.399510	207050.054779	37.636071
1964.898450	207371.346418	37.641088
1966.880919	207703.137743	37.646106
1968.535510	208049.061442	37.651124
1970.164256	208387.970934	37.656141
1972.036017	208744.007297	37.661159
1974.054020	209083.341253	37.666176
1975.617384	209458.358928	37.671194
1977.428022	209808.469788	37.676212
1979.472664	210176.902778	37.681229
1981.330657	210547.157573	37.686247
1983.091047	210913.583312	37.691264
1985.450769	211280.043006	37.696282
1987.672550	211655.718243	37.701300
1989.800468	212014.411146	37.706317
1991.758417	212387.110934	37.711335
1994.145485	212746.122223	37.716352
1995.934867	213124.502553	37.721370
1998.275587	213483.283989	37.726388
2000.741940	213830.417934	37.731405
2002.618905	214194.926479	37.736423
2004.789962	214551.125181	37.741440
2006.506256	214911.194062	37.746458
2008.648336	215245.817550	37.751476
2010.678216	215569.973352	37.756493
2012.818566	215913.576633	37.761511
2015.100147	216229.404886	37.766528
2016.691359	216556.834399	37.771546
2018.624823	216892.971733	37.776564
2021.355242	217211.082053	37.781581
2023.367284	217528.228570	37.786599
2026.003451	217838.116545	37.791616
2028.353898	218162.423904	37.796634
2030.791956	218456.513150	37.801652
2033.383058	218761.193871	37.806669
2035.505246	219074.190553	37.811687
2037.864067	219350.469542	37.816704
2039.939095	219662.562037	37.821722
2042.006055	219942.571680	37.826740
2043.920657	220231.672277	37.831757
2045.644958	220594.841280	37.836775
2047.494356	220900.346832	37.841792
2049.598193	221196.531551	37.846810
2051.615387	221502.203362	37.851828
2053.795923	221801.006602	37.856845
2055.042887	222119.056019	37.861863
2057.145541	222422.229230	37.866880
2059.387326	222755.855580	37.871898
2060.887482	223078.427147	37.876916
2063.099847	223394.246187	37.881933
2065.493842	223706.761671	37.886951
2067.729583	224032.280553	37.891968
2069.196516	224364.106534	37.896986
2071.292941	224692.710346	37.902004
2073.335334	225025.742914	37.907021
2075.130654	225371.958385	37.912039
2077.086058	225706.899500	37.917056
2078.669111	226053.583222	37.922074
2080.819737	226410.311408	37.927092
2082.541279	226764.112412	37.932109
2084.470581	227126.288131	37.937127
2086.496817	227496.018157	37.942144
2088.556842	227863.357126	37.947162
2090.368043	228235.867253	37.952180
2092.707169	228610.453944	37.957197
2094.407736	228996.927691	37.962215
2096.268267	229372.964952	37.967232
2098.259208	229761.478491	37.972250
2100.091305	230165.688994	37.977268
2102.564251	230554.713590	37.982285
2104.360900	230945.853507	37.987303
2106.609263	231343.983936	37.992320
2108.715548	231746.786365	37.997338
2110.856957	232143.311677	38.002356
2113.155424	232537.604101	38.007373
2115.111410	232953.261380	38.012391
2117.294145	233346.737311	38.017408
2119.151826	233742.653806	38.022426
2121.003026	234135.931479	38.027444
2123.276139	234507.047159	38.032461
2125.400251	234891.420445	38.037479
2127.529189	235269.165378	38.042496
2130.087163	235636.506378	38.047514
2132.095737	236022.934093	38.052532
2134.306072	236404.454642	38.057549
2136.164782	236786.718103	38.062567
2138.672376	237168.143428	38.067584
2140.729950	237550.581241	38.072602
2142.472259	237942.417305	38.077620
2144.738539	238325.129490	38.082637
2146.681122	238726.258086	38.087655
2148.885871	239129.784871	38.092672
2151.316311	239534.090066	38.097690
2153.228617	239932.484532	38.102708
2155.493009	240325.871557	38.107725
2157.748610	240743.899119	38.112743
2160.001194	241145.926665	38.117760
2162.191015	241552.435897	38.122778
2164.301890	241961.676803	38.127796
2166.728531	242362.207515	38.132813
2168.976938	242762.691568	38.137831
2171.399903	243175.188948	38.142848
2173.588229	243586.785044	38.147866
2176.044759	243999.228913	38.152884
2178.422290	244388.216471	38.157901
2180.797129	244781.980902	38.162919
2183.669822	245169.545943	38.167936
2186.334897	245557.170403	38.172954
2188.761847	245940.388556	38.177972
2191.124634	246312.060505	38.182989
2193.413288	246692.914928	38.188007
2195.486018	247078.224375	38.193024
2198.295179	247434.333765	38.198042
2200.520068	247798.157016	38.203060
2203.270775	248159.179822	38.208077
2205.477946	248529.967567	38.213095
2207.327623	248888.213821	38.218112
2210.078757	249239.434148	38.223130
2211.832504	249606.130499	38.228148
2214.244774	249954.180139	38.233165
2216.221035	250320.410979	38.238183
2218.382288	250686.054449	38.243200
2220.282119	251045.567556	38.248218
2221.788807	251421.451670	38.253236
2223.733900	251800.061265	38.258253
2225.810909	252185.941074	38.263271
2227.752476	252580.632242	38.268288
2229.729937	252975.420169	38.273306
2231.379510	253389.033005	38.278324
2233.361383	253793.500102	38.283341
2235.590864	254201.408863	38.288359
2237.433590	254620.963178	38.293376
2239.655244	255041.474360	38.298394
2242.099194	255450.621734	38.303412
2244.074225	255829.437688	38.308429
2246.103625	256236.061266	38.313447
2248.392620	256627.377585	38.318464
2250.675394	257025.681243	38.323482
2252.690235	257428.879951	38.328500
2254.753455	257838.930360	38.333517
2257.148484	258258.835858	38.338535
2258.991708	258668.770127	38.343552
2261.088545	259105.032804	38.348570
2263.110404	259534.169939	38.353588
2265.389430	259959.863015	38.358605
2267.492444	260396.330032	38.363623
2269.793249	260842.978290	38.368640
2272.127698	261285.659046	38.373658
2273.871467	261740.246452	38.378676
2276.234477	262191.103709	38.383693
2278.978508	262644.949534	38.388711
2280.956779	263116.191425	38.393728
2283.798127	263571.725043	38.398746
2285.957246	264036.360084	38.403764
2288.567932	264489.772135	38.408781
2290.906997	264953.566839	38.413799
2293.062143	265418.788392	38.418816
2296.177458	265869.683232	38.423834
2298.389817	266319.730953	38.428852
2301.138661	266777.696048	38.433869
2303.429820	267228.062337	38.438887
2305.845124	267681.965773	38.443904
2308.490093	268126.662568	38.448922
2311.170375	268569.906098	38.453940
2313.645574	269013.436472	38.458957
2315.555554	269458.199883	38.463975
2317.974784	269904.025963	38.468992
2321.206324	270331.306060	38.474010
2323.700939	270767.645173	38.479028
2326.443243	271180.040624	38.484045
2329.139100	271605.297703	38.489063
2331.847439	272026.132751	38.494080
2334.370070	272440.392474	38.499098
2336.505401	272854.815308	38.504116
2338.898794	273261.525480	38.509133
2340.893914	273681.864274	38.514151
2342.870590	274105.152834	38.519168
2345.435549	274515.748065	38.524186
2347.878678	274923.771472	38.529204
2350.539241	275336.841085	38.534221
2352.829865	275756.269366	38.539239
2355.030018	276165.042513	38.544256
2357.543396	276580.904304	38.549274
2359.525536	277005.106337	38.554292
2362.027873	277407.150258	38.559309
2364.600431	277821.249550	38.564327
2367.011113	278232.046531	38.569344
2369.562572	278637.562556	38.574362
2371.427227	279033.381599	38.579380
2373.656868	279408.642118	38.584397
2375.963410	279792.095564	38.589415
2378.047556	280181.223619	38.594432
2380.337827	280570.039363	38.599450
2381.926229	280969.381497	38.604468
2384.450798	281371.013707	38.609485
2386.500385	281783.288703	38.614503
2388.098155	282211.791485	38.619520
2390.530654	282630.965650	38.624538
2392.716112	283063.058057	38.629556
2394.594927	283511.278898	38.634573
2397.275279	283946.035603	38.639591
2399.587002	284391.240190	38.644608
2402.249118	284833.746848	38.649626
2404.341287	285295.370258	38.654644
2407.057671	285746.656753	38.659661
2409.274636	286202.899235	38.664679
2411.453986	286671.086491	38.669696
2414.157773	287124.786518	38.674714
2416.532281	287599.419294	38.679732
2418.944614	288063.808013	38.684749
2420.938440	288549.575326	38.689767
2423.609266	289030.357205	38.694784
2426.330555	289500.562738	38.699802
2428.299779	289988.084293	38.704820
2431.025431	290473.148026	38.709837
2432.928395	290964.056826	38.714855
2435.238249	291459.523441	38.719872
2437.792688	291949.818982	38.724890
2440.392228	292460.225092	38.729908
2443.002714	292962.906012	38.734925
2445.303733	293475.821182	38.739943
2447.699961	293988.694651	38.744960
2450.143535	294485.683002	38.749978
2452.513603	295010.141516	38.754996
2455.116705	295518.151996	38.760013
2458.101778	296025.999018	38.765031
2460.771204	296535.241022	38.770048
2463.127669	297050.551480	38.775066
2465.753645	297558.730676	38.780084
2468.227031	298068.786935	38.785101
2470.533654	298580.239823	38.790119
2472.606983	299096.097224	38.795136
2475.262138	299621.818213	38.800154
2477.474129	300142.095643	38.805172
2480.342791	300665.442488	38.810189
2483.025724	301186.327705	38.815207
2484.707819	301709.173250	38.820224
2487.456921	302240.916075	38.825242
2490.219814	302768.158839	38.830260
2493.004071	303290.087526	38.835277
2495.640934	303810.996232	38.840295
2497.927199	304327.792851	38.845312
2501.013927	304827.442291	38.850330
2503.606017	305316.144456	38.855348
2506.218188	305797.704136	38.860365
2508.957094	306271.037665	38.865383
2510.798365	306752.690575	38.870400
2513.344635	307223.358698	38.875418
2515.725439	307714.066499	38.880436
2518.026838	308193.481969	38.885453
2520.324460	308676.807727	38.890471
2522.501253	309182.121447	38.895488
2525.150653	309680.017637	38.900506
2527.465525	310185.076572	38.905524
2530.112554	310689.242481	38.910541
2532.953774	311187.736741	38.915559
2535.284203	311707.086229	38.920576
2537.827608	312209.229778	38.925594
2540.614153	312728.756146	38.930612
2542.778921	313242.206612	38.935629
2545.368120	313769.912192	38.940647
2547.935557	314293.046819	38.945664
2550.982835	314811.759636	38.950682
2553.005974	315336.880057	38.955700
2555.443409	315877.856728	38.960717
2558.624252	316402.102367	38.965735
2560.885686	316936.446836	38.970752
2563.786482	317466.217051	38.975770
2566.685170	317993.013145	38.980788
2569.394218	318506.782055	38.985805
2572.362547	319022.361057	38.990823
2575.271182	319553.845256	38.995840
2578.206804	320060.229827	39.000858
2580.733395	320577.952564	39.005876
2583.103297	321089.754281	39.010893
2585.971667	321613.004094	39.015911
2588.546457	322131.979882	39.020928
2590.621792	322649.914233	39.025946
2593.228049	323179.087986	39.030964
2595.809208	323694.929517	39.035981
2598.379045	324236.165437	39.040999
2600.358218	324780.234105	39.046016
2603.219816	325311.867949	39.051034
2605.789973	325840.319259	39.056052
2608.188169	326384.691653	39.061069
2610.754976	326917.758233	39.066087
2613.602825	327469.975093	39.071104
2615.910077	328017.474077	39.076122
2618.478727	328573.104730	39.081140
2620.900677	329123.929650	39.086157
2623.644287	329688.869429	39.091175
2625.936634	330246.080493	39.096192
2628.834905	330802.785047	39.101210
2631.498286	331373.463544	39.106228
2634.122153	331947.622650	39.111245
2636.656807	332498.886758	39.116263
2639.328463	333071.734153	39.121280
2641.857193	333624.615508	39.126298
2644.004166	334166.024765	39.131316
2646.500261	334707.628371	39.136333
2648.917127	335243.196915	39.141351
2651.360050	335800.873341	39.146368
2653.931594	336338.871643	39.151386
2656.703677	336892.601860	39.156404
2659.139911	337448.107202	39.161421
2662.197102	338001.909810	39.166439
2664.348945	338565.397980	39.171456
2666.971235	339138.048807	39.176474
2669.590047	339716.687111	39.181492
2671.924993	340293.613129	39.186509
2674.666833	340876.232832	39.191527
2677.207152	341467.968408	39.196544
2679.799390	342058.344398	39.201562
2682.891962	342642.846680	39.206580
2685.748234	343239.567328	39.211597
2688.983184	343839.624081	39.216615
2691.652705	344417.524143	39.221632
2694.263456	345014.240344	39.226650
2696.990180	345613.648532	39.231668
2699.596947	346205.910196	39.236685
2702.762431	346806.302688	39.241703
2705.354720	347399.975880	39.246720
2707.957259	348008.974737	39.251738
2710.752474	348614.356927	39.256756
2713.144696	349218.806241	39.261773
2716.238273	349831.362821	39.266791
2718.448401	350447.504842	39.271808
2721.219843	351060.403141	39.276826
2724.304322	351673.879454	39.281844
2726.733098	352316.949512	39.286861
2729.809167	352936.479414	39.291879
2732.041383	353571.061424	39.296896
2734.752835	354195.583935	39.301914
2737.708229	354821.786285	39.306932
2740.522081	355467.852952	39.311949
2743.562103	356089.787253	39.316967
2746.517039	356718.275989	39.321984
2749.350877	357343.806243	39.327002
2752.094778	357982.592130	39.332020
2755.206461	358595.650728	39.337037
2758.517390	359213.492467	39.342055
2761.055746	359834.240530	39.347072
2764.465385	360447.253791	39.352090
2767.535493	361060.972799	39.357108
2769.783804	361677.326568	39.362125
2772.833691	362278.545986	39.367143
2775.873182	362891.865173	39.372160
2778.715710	363499.649433	39.377178
2781.600857	364090.085344	39.382196
2784.345485	364701.904323	39.387213
2787.614049	365290.284423	39.392231
2789.983319	365906.181597	39.397248
2792.294733	366495.458766	39.402266
2795.251590	367062.573412	39.407284
2797.977637	367640.197829	39.412301
2800.538633	368205.964702	39.417319
2803.189005	368781.555920	39.422336
2806.022939	369346.807952	39.427354
2808.842315	369914.110259	39.432372
2811.274155	370500.599056	39.437389
2814.240349	371075.018388	39.442407
2816.870887	371659.759597	39.447424
2819.578517	372241.537101	39.452442
2822.626504	372824.318296	39.457460
2825.395504	373428.322017	39.462477
2827.874179	374016.022829	39.467495
2830.796877	374612.347639	39.472512
2833.591383	375218.223887	39.477530
2836.161950	375825.978658	39.482548
2838.441049	376442.371246	39.487565
2841.469025	377062.492142	39.492583
2844.138750	377698.161414	39.497600
2846.685467	378322.296591	39.502618
2849.631032	378960.743272	39.507636
2852.150317	379615.939921	39.512653
2855.030934	380258.079509	39.517671
2857.782562	380926.662612	39.522688
2860.323272	381586.135014	39.527706
2863.210364	382247.063208	39.532724
2865.879613	382921.940821	39.537741
2868.819332	383597.017175	39.542759
2871.906992	384268.100813	39.547776
2874.546119	384955.604145	39.552794
2877.808968	385640.636979	39.557812
2880.667943	386327.851589	39.562829
2883.565278	387024.330457	39.567847
2886.635073	387713.641447	39.572864
2889.630301	388399.729922	39.577882
2892.503627	389100.230555	39.582900
2894.830669	389806.053844	39.587917
2897.755844	390516.232015	39.592935
2900.636423	391223.663886	39.597952
2903.444968	391941.617496	39.602970
2906.663448	392642.905846	39.607988
2909.017634	393374.088919	39.613005
2912.227207	394094.140531	39.618023
2915.236825	394813.523898	39.623040
2918.763632	395521.728682	39.628058
2922.611564	396209.581771	39.633076
2925.691741	396902.968635	39.638093
2929.564193	397596.773488	39.643111
2932.834438	398277.321921	39.648128
2935.829172	398962.818828	39.653146
2938.664897	399630.197842	39.658164
2941.668682	400309.757351	39.663181
2944.715366	400993.631300	39.668199
2947.547958	401662.312668	39.673216
2950.164576	402334.360816	39.678234
2953.276947	402958.679553	39.683252
2955.465443	403617.154196	39.688269
2958.353910	404242.471736	39.693287
2961.193648	404882.589317	39.698304
2963.876394	405539.221560	39.703322
2966.937403	406178.364885	39.708340
2969.918571	406822.830937	39.713357
2972.875086	407474.562419	39.718375
2975.653756	408139.159604	39.723392
2978.351555	408787.963632	39.728410
2981.278122	409451.418765	39.733428
2983.431606	410138.604423	39.738445
2986.263125	410812.867441	39.743463
2988.811250	411520.818442	39.748480
2991.250482	412234.016119	39.753498
2994.320854	412947.527542	39.758516
2996.959705	413673.102653	39.763533
3000.203494	414395.953727	39.768551
3002.976523	415134.294622	39.773568
3005.640594	415881.123271	39.778586
3008.746837	416636.529077	39.783604
3011.479052	417394.862895	39.788621
3014.718907	418148.839166	39.793639
3017.893842	418918.236873	39.798656
3020.756745	419686.598742	39.803674
3023.966359	420455.948830	39.808692
3027.521407	421227.629980	39.813709
3030.297421	421993.306974	39.818727
3033.463688	422769.567042	39.823744
3036.641015	423544.308649	39.828762
3040.258484	424307.609097	39.833780
3043.027024	425102.080643	39.838797
3046.131219	425874.715300	39.843815
3049.574462	426651.251117	39.848832
3052.379734	427436.376443	39.853850
3055.641709	428221.532953	39.858868
3058.394614	429003.757837	39.863885
3061.689171	429798.360699	39.868903
3065.217578	430576.262100	39.873920
3068.218872	431359.643625	39.878938
3071.599167	432128.657497	39.883956
3074.881598	432917.645684	39.888973
3077.943841	433696.590533	39.893991
3081.812305	434466.900523	39.899008
3084.654425	435248.415732	39.904026
3087.743653	436005.760782	39.909044
3090.341768	436793.850482	39.914061
3093.756561	437560.060910	39.919079
3096.808350	438352.460746	39.924096
3099.586834	439122.648231	39.929114
3103.167902	439897.444536	39.934132
3106.386557	440671.058466	39.939149
3109.466377	441441.024233	39.944167
3112.775318	442216.043191	39.949184
3115.630614	442988.223158	39.954202
3118.821530	443723.771290	39.959220
3121.762710	444452.349797	39.964237
3124.782226	445187.070009	39.969255
3127.916159	445916.737611	39.974272
3130.606130	446655.261274	39.979290
3133.779232	447397.633790	39.984308
3136.239218	448145.916849	39.989325
3138.969143	448899.802414	39.994343
3141.888799	449660.517304	39.999360
3144.656768	450432.568811	40.004378
3147.525383	451201.541769	40.009396
3150.908116	452008.163378	40.014413
3153.832870	452794.382854	40.019431
3157.139632	453590.383147	40.024448
3160.353973	454389.203969	40.029466
3163.738376	455180.632010	40.034484
3167.109419	455986.152188	40.039501
3170.145360	456793.568513	40.044519
3173.487561	457599.591501	40.049536
3176.468535	458423.755787	40.054554
3179.628240	459244.420531	40.059572
3182.554527	460069.138886	40.064589
3185.690312	460899.206143	40.069607
3188.821672	461725.397637	40.074624
3191.989005	462570.319584	40.079642
3195.325757	463416.446191	40.084660
3198.541996	464265.694581	40.089677
3201.579202	465119.742651	40.094695
3204.771255	465983.847620	40.099712
3208.148894	466854.311136	40.104730
3211.222504	467719.779845	40.109748
3214.048968	468594.253769	40.114765
3217.489578	469485.079780	40.119783
3220.445635	470350.660130	40.124800
3223.354175	471246.753568	40.129818
3226.572502	472137.550890	40.134836
3230.023918	473016.997342	40.139853
3233.482207	473914.555542	40.144871
3237.416910	474791.472472	40.149888
3240.706515	475682.052599	40.154906
3244.615621	476562.182530	40.159924
3248.052580	477435.979045	40.164941
3251.308720	478319.723820	40.169959
3254.393627	479205.174848	40.174976
3257.469481	480096.905552	40.179994
3261.033308	480958.143229	40.185012
3264.405473	481836.910411	40.190029
3267.717125	482719.235644	40.195047
3270.980003	483599.304934	40.200064
3273.893546	484490.455936	40.205082
3277.302913	485369.562170	40.210100
3281.191219	486240.821573	40.215117
3284.199329	487124.053799	40.220135
3287.704609	488005.246444	40.225152
3290.565000	488886.146350	40.230170
3293.783302	489721.229395	40.235188
3296.841423	490576.507001	40.240205
3299.250416	491419.522734	40.245223
3302.502050	492252.416256	40.250240
3305.354693	493117.257218	40.255258
3308.761326	493978.283051	40.260276
3312.178221	494838.105314	40.265293
3315.065746	495712.919481	40.270311
3318.154564	496599.527230	40.275328
3320.859049	497495.797385	40.280346
3324.214831	498387.577599	40.285364
3327.459356	499294.781785	40.290381
3330.622965	500219.371704	40.295399
3333.876265	501123.654363	40.300416
3336.902527	502054.734042	40.305434
3340.108829	502982.555960	40.310452
3343.738645	503926.263880	40.315469
3346.489722	504876.571426	40.320487
3350.321255	505825.394656	40.325504
3353.509586	506788.601499	40.330522
3357.274434	507746.061751	40.335540
3360.785250	508706.839735	40.340557
3363.927655	509675.090648	40.345575
3367.483389	510643.221435	40.350592
3370.551805	511636.148315	40.355610
3373.631704	512611.810696	40.360628
3377.374118	513589.128215	40.365645
3380.693952	514586.836549	40.370663
3384.188871	515562.716221	40.375680
3387.511514	516563.736354	40.380698
3390.723714	517565.621520	40.385716
3394.558667	518562.959674	40.390733
3397.676866	519571.244121	40.395751
3401.869353	520564.067132	40.400768
3405.241822	521579.399036	40.405786
3408.669893	522568.085855	40.410804
3412.207262	523580.392388	40.415821
3415.906344	524586.156476	40.420839
3419.554084	525584.354070	40.425856
3423.096599	526591.277406	40.430874
3426.577449	527589.527199	40.435892
3430.131445	528576.865732	40.440909
3433.325331	529583.755030	40.445927
3437.356512	530573.866709	40.450944
3440.958866	531577.791691	40.455962
3444.617016	532569.650162	40.460980
3448.073867	533567.070229	40.465997
3451.459227	534573.204284	40.471015
3454.943195	535552.907593	40.476032
3458.137240	536546.750535	40.481050
3461.479272	537541.009278	40.486068
3465.207286	538535.696231	40.491085
3467.961730	539546.841598	40.496103
3471.436496	540546.322285	40.501120
3474.676221	541547.206972	40.506125
3477.627967	542492.446947	40.511130
3480.582553	543398.047147	40.516135
3483.368597	544263.738789	40.521140
3486.529861	545050.826672	40.526144
3489.203911	545778.993743	40.531149
3492.185364	546466.091682	40.536154
3495.334090	547063.241309	40.541159
3497.562361	547623.921596	40.546164
3500.366222	548093.091944	40.551168
3502.195142	548521.826188	40.556173
3504.307096	548883.384273	40.561178
3506.568527	549196.161310	40.566183
3508.106704	549454.394144	40.571188
3510.308450	549663.266003	40.576192
3511.342595	549826.752156	40.581197
3512.591864	549956.595027	40.586202
3513.909195	550036.216967	40.591207
3514.946118	550093.881717	40.596212
3515.800572	550108.178548	40.601216
3516.913440	550092.914748	40.606221
3517.544061	550050.831273	40.611226
3518.366416	549976.977057	40.616231
3518.755125	549892.594007	40.621236
3519.511689	549775.604179	40.626240
3519.937006	549641.457969	40.631245
3520.428961	549487.417463	40.636250
3521.097951	549309.629327	40.641255
3521.342492	549136.498377	40.646260
3521.316755	548933.633638	40.651264
3521.776239	548728.721222	40.656269
3521.813868	548507.117671	40.661274
3522.332388	548270.395447	40.666279
3521.950321	548041.180102	40.671284
3522.304373	547778.131436	40.676288
3522.279935	547537.193292	40.681293
3521.909264	547284.697607	40.686298
3521.929485	547028.350417	40.691303
3521.872228	546760.503230	40.696308
3521.662514	546490.252527	40.701312
3521.879392	546215.891479	40.706317
3521.902867	545954.931898	40.711322
3521.739520	545674.917155	40.716327
3521.598506	545406.351935	40.721332
3521.615303	545129.226069	40.726336
3521.609538	544855.884525	40.731341
3521.288701	544571.280178	40.736346
3521.033482	544297.462963	40.741351
3521.050820	544036.621985	40.746356
3520.771485	543744.877278	40.751360
3520.720661	543477.423995	40.756365
3520.566893	543187.970791	40.761370
3520.417771	542930.115350	40.766375
3519.970861	542662.053731	40.771380
3520.113005	542374.254532	40.776384
3519.938886	542109.623543	40.781389
3519.453795	541848.116880	40.786394
3519.268067	541588.729424	40.791399
3518.862656	541318.920534	40.796404
3518.804045	541068.339952	40.801408
3518.202860	540812.690675	40.806413
3518.223381	540549.566708	40.811418
3518.003066	540323.589729	40.816423
3517.674874	540079.296618	40.821428
3518.180026	539832.393533	40.826432
3517.461043	539593.102944	40.831437
3516.955099	539359.733631	40.836442
3516.786483	539108.632915	40.841447
3516.740854	538912.805356	40.846452
3516.927275	538678.255637	40.851456
3516.734261	538438.156676	40.856461
3516.102148	538237.312514	40.861466
3516.189198	538010.191904	40.866471
3515.461130	537806.226077	40.871476
3515.712626	537575.992323	40.876480
3515.263269	537382.936070	40.881485
3515.265870	537172.937281	40.886490
3515.099027	536947.659152	40.891495
3514.949679	536778.841089	40.896500
3514.753251	536564.824897	40.901504
3514.911582	536372.518453	40.906509
3514.566705	536174.430166	40.911514
3514.410810	535977.218612	40.916519
3513.929396	535789.046677	40.921524
3514.236650	535587.059520	40.926528
3513.802934	535429.535320	40.931533
3513.778078	535246.891278	40.936538
3513.385917	535063.141345	40.941543
3513.123039	534884.268504	40.946548
3513.067023	534719.706611	40.951552
3513.108305	534541.034279	40.956557
3512.899615	534377.907253	40.961562
3512.892322	534197.470626	40.966567
3512.189054	534047.804694	40.971572
3512.364527	533898.554099	40.976576
3512.584496	533710.700571	40.981581
3511.788129	533584.939098	40.986586
3512.240098	533425.233781	40.991591
3511.887169	533271.665654	40.996596
3511.637212	533110.906130	41.001600
3511.601297	532983.655593	41.006605
3511.267775	532824.118756	41.011610
3511.401024	532682.794657	41.016615
3510.938014	532546.565010	41.021620
3511.134655	532406.087220	41.026624
3511.023394	532275.205307	41.031629
3510.634411	532148.407906	41.036634
3510.631107	532011.646227	41.041639
3510.254247	531883.581706	41.046644
3510.205791	531751.270842	41.051648
3510.009814	531630.956159	41.056653
3509.915384	531515.424233	41.061658
3510.058072	531406.977840	41.066663
3509.833429	531285.452454	41.071668
3509.857952	531175.557929	41.076672
3509.682649	531056.852345	41.081677
3509.487913	530944.161450	41.086682
3509.287974	530825.104324	41.091687
3509.140342	530726.854774	41.096692
3509.213926	530626.851746	41.101696
3508.985092	530523.712697	41.106701
3508.723265	530427.500387	41.111706
3508.911914	530319.392888	41.116711
3508.802608	530235.585021	41.121716
3508.288700	530125.515596	41.126720
3508.406845	530043.489762	41.131725
3508.214555	529953.377471	41.136730
3508.504597	529859.146124	41.141735
3508.249402	529781.068649	41.146740
3508.292073	529685.157368	41.151744
3508.187397	529598.768374	41.156749
3508.241108	529514.627720	41.161754
3508.309850	529429.877878	41.166759
3508.084388	529342.849678	41.171764
3507.907350	529252.427780	41.176768
3508.189890	529180.326029	41.181773
3507.912688	529088.099904	41.186778
3508.071882	529005.304205	41.191783
3507.349528	528924.517082	41.196788
3507.710268	528842.850909	41.201792
3507.622047	528774.595812	41.206797
3507.535465	528687.390448	41.211802
3507.754025	528614.386639	41.216807
3507.554658	528541.650680	41.221812
3507.512045	528460.652681	41.226816
3507.645972	528384.477587	41.231821
3507.001528	528312.619458	41.236826
3507.295025	528248.293926	41.241831
3506.773324	528180.761720	41.246836
3506.962432	528097.602801	41.251840
3507.093226	528063.218620	41.256845
3506.828182	527977.907331	41.261850
3507.020055	527903.540021	41.266855
3506.563055	527845.951572	41.271860
3506.615499	527790.960774	41.276864
3506.855099	527721.537542	41.281869
3506.579330	527666.092829	41.286874
3506.591373	527601.708088	41.291879
3506.400060	527548.119449	41.296884
3506.697751	527466.355074	41.301888
3506.539153	527434.441021	41.306893
3506.327743	527380.905530	41.311898
3506.580088	527318.452594	41.316903
3506.132426	527269.199172	41.321908
3506.198039	527209.453788	41.326912
3506.042266	527160.911955	41.331917
3505.919592	527113.830333	41.336922
3505.993231	527059.339028	41.341927
3505.924663	527017.352885	41.346932
3506.064106	526959.414259	41.351936
3505.964242	526898.986330	41.356941
3505.967154	526869.016608	41.361946
3506.062397	526825.487915	41.366951
3506.230909	526778.915203	41.371956
3505.942132	526731.151161	41.376960
3506.205385	526683.198646	41.381965
3506.112379	526634.544209	41.386970
3505.644825	526580.288420	41.391975
3505.479465	526546.908015	41.396980
3505.489186	526487.623611	41.401984
3505.860397	526449.609630	41.406989
3505.539629	526418.022407	41.411994
3505.614095	526372.726869	41.416999
3505.443079	526336.516678	41.422004
3505.562970	526294.903164	41.427008
3505.676115	526253.694931	41.432013
3505.499894	526208.590170	41.437018
3505.557303	526161.275108	41.442023
3505.167490	526138.997719	41.447028
3505.412611	526102.367440	41.452032
3505.430236	526071.635781	41.457037
3505.101444	526028.778427	41.462042
3505.266650	525995.445701	41.467047
3505.246918	525966.539227	41.472052
3505.216839	525923.230046	41.477056
3505.363028	525895.914543	41.482061
3505.258680	525852.414743	41.487066
3505.592749	525804.498939	41.492071
3505.076448	525784.212175	41.497076
3505.053437	525747.926715	41.502080
3505.175788	525713.033375	41.507085
3504.747235	525683.281247	41.512090
3504.987178	525644.679594	41.517095
3504.878063	525615.685528	41.522100
3505.111508	525581.229222	41.527104
3504.942754	525556.793297	41.532109
3505.008222	525536.212097	41.537114
3505.209036	525494.836424	41.542119
3504.918810	525456.874085	41.547124
3504.779830	525435.769097	41.552128
3505.084931	525414.644436	41.557133
3504.835676	525376.978689	41.562138
3505.069343	525345.352256	41.567143
3505.146346	525323.758095	41.572148
3504.778847	525299.656449	41.577152
3504.827058	525277.359169	41.582157
3504.801792	525253.354992	41.587162
3504.947112	525210.572139	41.592167
3504.633495	525199.502079	41.597172
3504.597999	525171.051552	41.602176
3504.562430	525138.911285	41.607181
3504.686943	525118.471847	41.612186
3504.931700	525095.688354	41.617191
3504.569515	525080.632912	41.622196
3504.628530	525038.166503	41.627200
3504.945814	525019.162252	41.632205
3504.579713	524990.409849	41.637210
3504.894577	524957.657842	41.642215
3504.629903	524944.305371	41.647220
3504.634985	524909.782628	41.652224
3504.771447	524885.802884	41.657229
3504.913077	524856.211821	41.662234
3504.862293	524835.092102	41.667239
3504.596828	524806.475097	41.672244
3504.509257	524776.819024	41.677248
3504.656853	524767.950293	41.682253
3504.255426	524740.163380	41.687258
3504.388097	524718.761787	41.692263
3504.373811	524702.185191	41.697268
3504.283122	524694.668258	41.702272
3504.301569	524658.575960	41.707277
3504.351799	524644.617467	41.712282
3504.637907	524630.419498	41.717287
3504.006855	524613.030475	41.722292
3504.355826	524597.306176	41.727296
3504.527701	524568.114166	41.732301
3504.161053	524563.622982	41.737306
3504.460992	524529.103364	41.742311
3504.372375	524514.964521	41.747316
3503.998488	524487.880459	41.752320
3504.223854	524473.894136	41.757325
3504.456448	524468.903845	41.762330
3504.327944	524447.442079	41.767335
3504.222276	524429.059987	41.772340
3504.458261	524405.316527	41.777344
3503.931921	524408.483011	41.782349
3503.987282	524387.699750	41.787354
3504.433336	524367.360174	41.792359
3504.531077	524360.571498	41.797364
3504.413843	524322.983502	41.802368
3504.607582	524312.590835	41.807373
3504.320346	524281.499558	41.812378
3504.553627	524271.353347	41.817383
3504.299639	524246.878351	41.822388
3504.577982	524227.980414	41.827392
3504.522204	524197.964420	41.832397
3504.467552	524188.722963	41.837402
3504.388327	524148.955038	41.842407
3504.254280	524138.108597	41.847412
3504.196267	524140.291264	41.852416
3504.289727	524115.609511	41.857421
3504.281025	524104.187218	41.862426
3504.411577	524068.581349	41.867431
3504.328921	524054.592800	41.872436
3504.177313	524039.958022	41.877440
3504.375019	524027.037178	41.882445
3504.354432	524017.790239	41.887450
3504.466365	523986.332016	41.892455
3504.406414	523978.152773	41.897460
3504.149245	523955.649189	41.902464
3504.447148	523934.978652	41.907469
3504.036680	523913.611287	41.912474
3504.165103	523897.061853	41.917479
3503.847162	523898.881254	41.922484
3504.258196	523867.324976	41.927488
3504.370671	523868.924707	41.932493
3503.987752	523843.812353	41.937498
3504.255483	523822.944250	41.942503
3503.825593	523816.440931	41.947508
3504.084442	523809.980395	41.952512
3504.190067	523786.812657	41.957517
3503.931931	523794.587293	41.962522
3504.658418	523750.192256	41.967527
3504.446769	523745.474150	41.972532
3504.460512	523722.523035	41.977536
3504.527218	523701.332710	41.982541
3504.249496	523681.157216	41.987546
3504.363889	523662.436176	41.992551
3504.051486	523649.848398	41.997556
3504.251881	523630.001660	42.002560
3504.178859	523623.896795	42.007565
3504.206012	523606.908133	42.012570
3504.441546	523571.183475	42.017575
3504.359996	523570.084268	42.022580
3504.017394	523543.094767	42.027584
3504.166831	523536.499768	42.032589
3504.239356	523516.622552	42.037594
3504.427172	523497.788619	42.042599
3504.044555	523490.266715	42.047604
3504.321097	523463.330869	42.052608
3504.334891	523445.687010	42.057613
3504.217966	523429.479171	42.062618
3504.262754	523415.217178	42.067623
3504.093842	523411.604303	42.072628
3504.009382	523387.050655	42.077632
3504.109357	523375.610669	42.082637
3503.976575	523372.345921	42.087642
3504.107434	523346.090048	42.092647
3504.046606	523343.673262	42.097652
3504.108914	523322.179838	42.102656
3503.922730	523300.725660	42.107661
3504.039098	523312.889701	42.112666
3504.201355	523291.936485	42.117671
3503.970286	523268.517922	42.122676
3503.949864	523251.738604	42.127680
3503.995980	523242.430127	42.132685
3503.661845	523225.093769	42.137690
3504.073141	523213.402262	42.142695
3503.554450	523219.550209	42.147700
3503.984716	523191.780815	42.152704
3503.875758	523187.248514	42.157709
3503.721193	523178.679419	42.162714
3504.053555	523165.635504	42.167719
3503.957963	523171.564945	42.172724
3503.924758	523141.543418	42.177728
3504.215148	523129.719310	42.182733
3503.821514	523127.810046	42.187738
3503.992389	523106.147524	42.192743
3503.992755	523098.716555	42.197748
3504.092794	523085.911496	42.202752
3504.245095	523065.161761	42.207757
3503.944615	523058.890432	42.212762
3504.198830	523045.201616	42.217767
3504.070754	523034.808443	42.222772
3504.079002	523020.501327	42.227776
3504.108692	523017.716332	42.232781
3503.868866	522991.417371	42.237786
3504.295258	522977.751835	42.242791
3504.024698	522966.673429	42.247796
3504.201816	522938.084251	42.252800
3504.221431	522927.768767	42.257805
3504.073848	522920.967709	42.262810
3504.175434	522896.636665	42.267815
3504.027680	522898.328174	42.272820
3504.018086	522876.542217	42.277824
3504.226917	522856.895401	42.282829
3503.905137	522851.233970	42.287834
3504.128374	522827.490206	42.292839
3504.015885	522814.061360	42.297844
3503.970095	522811.338811	42.302848
3504.200584	522784.206909	42.307853
3503.768715	522771.839533	42.312858
3503.996852	522760.934920	42.317863
3504.010246	522761.943805	42.322868
3503.906106	522746.946493	42.327872
3504.053163	522748.389215	42.332877
3504.112749	522741.150927	42.337882
3504.191438	522710.352643	42.342887
3504.050427	522704.359280	42.347892
3504.269929	522687.541456	42.352896
3504.214403	522668.542814	42.357901
3504.013299	522653.864050	42.362906
3504.068642	522631.208121	42.367911
3504.240041	522625.215901	42.372916
3504.031777	522613.470234	42.377920
3504.205478	522597.973902	42.382925
3504.030163	522588.548393	42.387930
3504.078819	522577.924785	42.392935
3503.868446	522558.293313	42.397940
3503.952035	522534.318433	42.402944
3504.233097	522529.977062	42.407949
3503.926338	522528.155098	42.412954
3503.865378	522497.125721	42.417959
3503.891896	522497.879788	42.422964
3503.931014	522481.444127	42.427968
3504.089557	522464.534602	42.432973
3504.071377	522460.189958	42.437978
3504.243863	522448.434543	42.442983
3504.148075	522440.411842	42.447988
3504.161722	522412.858622	42.452992
3504.223757	522404.760406	42.457997
3503.850988	522389.603011	42.463002
3504.325578	522374.463329	42.468007
3504.382670	522353.272758	42.473012
3504.081567	522343.513119	42.478016
3503.921859	522314.874974	42.483021
3503.922671	522303.601563	42.488026
3504.380818	522294.379076	42.493031
3504.132219	522282.639544	42.498036
3503.802259	522266.261999	42.503040
3504.152023	522251.546355	42.508045
3503.963725	522241.212743	42.513050
3504.291812	522214.064463	42.518055
3504.273648	522221.094179	42.523060
3503.977788	522199.908642	42.528064
3503.916165	522178.433288	42.533069
3503.794613	522169.555121	42.538074
3504.345121	522157.486982	42.543079
3503.596053	522143.197683	42.548084
3504.062862	522130.030580	42.553088
3504.120416	522128.403755	42.558093
3503.679568	522113.812947	42.563098
3503.911754	522099.621284	42.568103
3503.761293	522107.632474	42.573108
3503.945518	522092.336211	42.578112
3504.068582	522074.724141	42.583117
3503.888410	522058.727139	42.588122
3503.931535	522044.767524	42.593127
3504.094428	522036.147647	42.598132
3503.961307	522016.301094	42.603136
3504.258144	522017.821316	42.608141
3503.667573	521995.468805	42.613146
3503.636083	521977.729397	42.618151
3504.027019	521970.286732	42.623156
3503.940827	521960.391786	42.628160
3503.922205	521944.369138	42.633165
3503.641520	521941.986892	42.638170
3504.074662	521926.954454	42.643175
3504.064963	521919.575089	42.648180
3503.887024	521897.662763	42.653184
3503.861393	521890.993659	42.658189
3504.050970	521888.486524	42.663194
3503.984395	521858.366786	42.668199
3503.548113	521863.137253	42.673204
3503.714729	521844.759739	42.678208
3504.019027	521844.155523	42.683213
3503.430424	521829.587813	42.688218
3503.605205	521809.287907	42.693223
3503.407538	521806.184760	42.698228
3503.705694	521801.587723	42.703232
3504.081651	521801.326060	42.708237
3503.655386	521806.752166	42.713242
3503.865175	521785.334503	42.718247
3503.923741	521777.742066	42.723252
3504.060866	521767.002836	42.728256
3504.084150	521761.893135	42.733261
3503.573570	521737.707664	42.738266
3503.857385	521735.842820	42.743271
3503.760071	521723.168988	42.748276
3503.637286	521717.425151	42.753280
3503.918903	521697.360993	42.758285
3503.829033	521693.988013	42.763290
3503.791068	521690.809047	42.768295
3503.910808	521694.379477	42.773300
3503.758972	521663.312316	42.778304
3504.034068	521649.012368	42.783309
3503.710831	521651.894502	42.788314
3504.006559	521637.995722	42.793319
3503.855120	521627.858112	42.798324
3503.566631	521615.770517	42.803329
3503.925659	521609.495494	42.808333
3504.006849	521609.735412	42.813338
3503.612702	521585.177427	42.818343
3503.688897	521582.536501	42.823348
3503.758848	521568.774457	42.828353
3503.673724	521575.309486	42.833357
3503.407514	521563.976656	42.838362
3503.794400	521541.772356	42.843367
3503.725311	521543.957122	42.848372
3503.560729	521532.203766	42.853377
3503.813444	521535.348773	42.858381
3503.598412	521536.393839	42.863386
3503.728286	521510.994590	42.868391
3503.143331	521503.250962	42.873396
3503.652294	521495.233319	42.878401
3504.075482	521500.980262	42.883405
3503.613412	521499.233283	42.888410
3503.869877	521487.514456	42.893415
3503.949089	521472.385874	42.898420
3503.720269	521477.224773	42.903425
3503.987702	521471.368617	42.908429
3503.691912	521463.377044	42.913434
3503.835278	521431.150563	42.918439
3503.637195	521429.311295	42.923444
3504.030454	521427.530228	42.928449
3503.816156	521415.430758	42.933453
3503.430187	521403.813411	42.938458
3503.516196	521388.835345	42.943463
3503.558534	521392.215854	42.948468
3503.837838	521393.385018	42.953473
3503.720847	521388.044593	42.958477
3503.544292	521368.153558	42.963482
3503.663739	521347.154043	42.968487
3503.573346	521352.173323	42.973492
3503.455918	521344.962391	42.978497
3503.621316	521341.093989	42.983501
3503.808092	521351.377813	42.988506
3503.818351	521346.371151	42.993511
3503.818780	521323.014298	42.998516
3503.888788	521313.599828	43.003521
3503.755543	521306.290268	43.008525
3503.753589	521319.788959	43.013530
3504.140254	521294.753232	43.018535
3503.671953	521278.699891	43.023540
3503.883837	521279.121381	43.028545
3503.904421	521262.586305	43.033549
3503.510762	521245.206677	43.038554
3503.697028	521230.617067	43.043559
3503.991641	521233.603843	43.048564
3503.798573	521218.467505	43.053569
3503.678964	521205.695682	43.058573
3503.864341	521195.302342	43.063578
3503.727990	521196.183325	43.068583
3503.450741	521193.345419	43.073588
3503.612394	521190.084248	43.078593
3503.750087	521178.485085	43.083597
3503.441117	521172.416589	43.088602
3503.504789	521157.087946	43.093607
3503.664275	521158.377178	43.098612
3503.630644	521164.145888	43.103617
3503.956647	521160.100390	43.108621
3503.888868	521141.304124	43.113626
3504.094051	521113.566760	43.118631
3503.923726	521121.278235	43.123636
3503.662872	521113.230411	43.128641
3503.984859	521082.340033	43.133645
3503.574889	521082.708147	43.138650
3503.974537	521076.628726	43.143655
3504.078173	521065.338205	43.148660
3504.154446	521046.114608	43.153665
3504.075313	521045.469855	43.158669
3503.725414	521026.060810	43.163674
3504.009017	521003.619319	43.168679
3503.474784	521005.776562	43.173684
3503.551415	521011.022331	43.178689
3503.994308	521005.593287	43.183693
3503.792928	520982.470070	43.188698
3503.928368	520967.635474	43.193703
3503.743805	520961.142781	43.198708
3503.457313	520960.278014	43.203713
3503.461062	520962.603016	43.208717
3503.625011	520937.500830	43.213722
3504.165507	520923.815541	43.218727
3504.101937	520920.488800	43.223732
3503.685866	520909.836441	43.228737
3504.267599	520894.779569	43.233741
3503.807393	520880.392939	43.238746
3503.834848	520874.978958	43.243751
3504.009069	520873.889697	43.248756
3503.971650	520853.419913	43.253761
3504.169818	520843.277113	43.258765
3503.796094	520843.184487	43.263770
3503.848111	520813.852990	43.268775
3503.717829	520809.020049	43.273780
3503.491348	520805.567362	43.278785
3503.827929	520798.790004	43.283789
3503.781561	520774.782515	43.288794
3503.848927	520771.586721	43.293799
3503.807123	520772.958358	43.298804
3504.187030	520770.825429	43.303809
3504.373476	520739.500809	43.308813
3503.857748	520733.565943	43.313818
3504.243449	520712.523529	43.318823
3504.064283	520703.552552	43.323828
3503.791860	520696.568062	43.328833
3504.112438	520667.497201	43.333837
3503.763453	520656.834074	43.338842
3503.809413	520649.344220	43.343847
3503.748730	520654.308460	43.348852
3503.691351	520622.921038	43.353857
3503.719078	520608.861511	43.358861
3503.499519	520606.317731	43.363866
3503.736985	520602.488323	43.368871
3503.501220	520602.019983	43.373876
3503.748924	520608.957815	43.378881
3503.831087	520587.457636	43.383885
3503.899411	520569.195337	43.388890
3503.705681	520564.877934	43.393895
3503.839638	520566.221807	43.398900
3503.573920	520552.562520	43.403905
3503.872479	520537.853427	43.408909
3503.212570	520539.828360	43.413914
3503.958404	520521.509482	43.418919
3503.711569	520520.082282	43.423924
3503.323066	520525.603957	43.428929
3503.621302	520518.984219	43.433933
3503.926957	520502.706666	43.438938
3503.657512	520490.261315	43.443943
3503.595867	520488.450933	43.448948
3503.526338	520492.253778	43.453953
3503.689661	520487.728244	43.458957
3503.569566	520460.496210	43.463962
3504.183898	520450.186273	43.468967
3503.481348	520441.095642	43.473972
3503.593813	520443.656327	43.478977
3503.852456	520434.969914	43.483981
3503.686760	520414.772647	43.488986
3503.985780	520400.316151	43.493991
3503.700283	520412.191973	43.498996
3503.773991	520406.669409	43.504001
3503.748190	520390.444133	43.509005
3503.854175	520379.708913	43.514010
3503.847366	520375.867502	43.519015
3503.766099	520366.425838	43.524020
3503.830984	520364.140415	43.529025
3503.863167	520330.665366	43.534029
3503.659828	520330.141334	43.539034
3503.923006	520318.066697	43.544039
3503.710067	520327.655961	43.549044
3503.885928	520308.567432	43.554049
3503.987129	520288.934533	43.559053
3503.625273	520292.075802	43.564058
3504.190808	520280.661174	43.569063
3503.965372	520257.894645	43.574068
3503.736890	520258.739680	43.579073
3503.770038	520247.864209	43.584077
3503.883857	520230.959438	43.589082
3503.921005	520216.240815	43.594087
3503.762016	520217.226546	43.599092
3503.877071	520211.747940	43.604097
3503.893139	520193.190126	43.609101
3503.592973	520192.782512	43.614106
3504.273315	520179.023940	43.619111
3504.080686	520165.757251	43.624116
3503.755583	520140.124427	43.629121
3503.715845	520135.833129	43.634125
3503.588260	520127.864873	43.639130
3504.196444	520121.802700	43.644135
3503.754347	520107.210286	43.649140
3503.518079	520098.955836	43.654145
3503.807028	520086.775837	43.659149
3503.288678	520099.699881	43.664154
3503.456465	520088.095189	43.669159
3503.950756	520087.106966	43.674164
3503.679524	520069.453935	43.679169
3503.779196	520049.922110	43.684173
3503.603810	520066.887311	43.689178
3503.845120	520056.282169	43.694183
3503.742999	520042.343798	43.699188
3503.767805	520018.778988	43.704193
3504.077933	520009.022455	43.709197
3503.799563	520004.718281	43.714202
3503.894503	519979.372733	43.719207
3503.907162	519968.196955	43.724212
3503.910289	519968.297557	43.729217
3503.901594	519966.680988	43.734221
3503.777862	519944.959709	43.739226
3504.036624	519931.975405	43.744231
3503.754342	519934.548003	43.749236
3503.667464	519916.511747	43.754241
3503.862616	519902.071229	43.759245
3503.870729	519898.732950	43.764250
3504.049214	519884.851214	43.769255
3504.129621	519882.158788	43.774260
3503.773002	519861.535973	43.779265
3503.964310	519847.854420	43.784269
3503.663141	519841.683073	43.789274
3503.923473	519827.586110	43.794279
3503.820105	519818.703787	43.799284
3503.774356	519807.688812	43.804289
3503.879533	519805.144140	43.809293
3503.933766	519788.602255	43.814298
3503.633208	519775.807354	43.819303
3503.634079	519764.127693	43.824308
3503.921715	519764.385571	43.829313
3503.713144	519763.558982	43.834317
3503.231505	519746.191661	43.839322
3503.659792	519716.343680	43.844327
3503.608593	519737.334453	43.849332
3503.473621	519731.692963	43.854337
3503.676407	519718.666777	43.859341
3503.479564	519723.501138	43.864346
3503.676509	519719.324004	43.869351
3503.799422	519701.304913	43.874356
3503.605106	519688.695395	43.879361
3503.924990	519680.302268	43.884365
3503.440438	519686.345014	43.889370
3503.870762	519686.024170	43.894375
3503.633241	519658.455436	43.899380
3503.344245	519658.855016	43.904385
3503.666581	519640.096485	43.909389
3503.467155	519652.009813	43.914394
3503.627761	519653.501233	43.919399
3503.591937	519650.877702	43.924404
3503.691860	519618.300589	43.929409
3503.814734	519615.854212	43.934413
3503.621092	519614.570207	43.939418
3503.547887	519593.548331	43.944423
3503.440757	519603.980833	43.949428
3503.422067	519612.124100	43.954433
3503.712555	519607.426542	43.959437
3502.999860	519596.617963	43.964442
3503.517866	519577.423944	43.969447
3503.328696	519568.099997	43.974452
3503.312388	519575.484487	43.979457
3503.593786	519568.411979	43.984461
3503.612836	519573.515626	43.989466
3503.349275	519571.787618	43.994471
3503.466295	519574.094914	43.999476
3503.558885	519586.821675	44.004481
3503.649521	519561.981774	44.009485
3503.600482	519560.068174	44.014490
3503.687969	519543.166857	44.019495
3503.469673	519539.662045	44.024500
3503.595458	519525.838896	44.029505
3503.514070	519525.447246	44.034509
3503.275628	519542.018464	44.039514
3503.570600	519533.376394	44.044519
3503.620931	519505.964151	44.049524
3503.564447	519499.501193	44.054529
3503.653930	519495.088180	44.059533
3503.698912	519500.794490	44.064538
3503.415958	519499.322346	44.069543
3503.507938	519499.358345	44.074548
3503.295738	519497.066035	44.079553
3503.549737	519473.565339	44.084557
3503.413294	519473.637443	44.089562
3503.229013	519463.554240	44.094567
3503.580442	519459.605431	44.099572
3503.338050	519466.014474	44.104577
3503.572478	519460.769558	44.109581
3503.540681	519462.493653	44.114586
3503.801759	519463.413034	44.119591
3503.605748	519465.719260	44.124596
3503.656190	519445.739444	44.129601
3503.755926	519430.858539	44.134605
3503.365287	519438.352819	44.139610
3503.502630	519421.898551	44.144615
3503.709323	519417.517554	44.149620
3503.423719	519423.225580	44.154625
3503.093338	519412.558697	44.159629
3503.221429	519430.386699	44.164634
3503.690233	519418.936203	44.169639
3503.681783	519412.516180	44.174644
3503.450063	519390.406741	44.179649
3503.865479	519381.644431	44.184653
3503.236935	519394.990939	44.189658
3503.559660	519386.091596	44.194663
3503.492714	519390.096534	44.199668
3503.584574	519373.851655	44.204673
3503.592658	519353.777298	44.209677
3503.453948	519359.816061	44.214682
3503.700449	519349.260205	44.219687
3503.491820	519348.838100	44.224692
3503.510902	519352.627202	44.229697
3503.906837	519341.087046	44.234701
3503.409104	519341.772435	44.239706
3503.427969	519319.926665	44.244711
3503.601483	519302.809256	44.249716
3503.428852	519310.218574	44.254721
3503.454061	519306.624662	44.259725
3503.525327	519314.298801	44.264730
3503.647229	519303.509799	44.269735
3503.577876	519307.363452	44.274740
3503.655068	519287.379215	44.279745
3504.062713	519267.595534	44.284749
3503.776588	519278.208220	44.289754
3503.826025	519276.531833	44.294759
3503.714854	519244.644651	44.299764
3503.624031	519233.535291	44.304769
3503.647561	519238.183274	44.309773
3503.443752	519234.574983	44.314778
3503.703490	519227.708000	44.319783
3503.655209	519236.361754	44.324788
3503.659611	519206.984344	44.329793
3503.721380	519193.272159	44.334797
3503.539532	519190.267135	44.339802
3503.679979	519182.407741	44.344807
3503.800193	519198.872054	44.349812
3503.762388	519175.821553	44.354817
3503.776262	519146.341413	44.359821
3503.453837	519160.347601	44.364826
3503.642102	519147.474946	44.369831
3503.658762	519153.034165	44.374836
3503.234944	519146.528002	44.379841
3503.815813	519112.508682	44.384845
3503.714552	519117.530362	44.389850
3503.663516	519116.426028	44.394855
3503.676568	519111.620492	44.399860
3503.619614	519123.916184	44.404865
3504.160248	519101.785406	44.409869
3503.688799	519091.140611	44.414874
3503.798789	519080.353345	44.419879
3503.616658	519078.410162	44.424884
3503.328831	519077.039875	44.429889
3503.677683	519044.068340	44.434893
3503.587356	519041.706140	44.439898
3503.468142	519035.303476	44.444903
3503.750089	519040.062360	44.449908
3503.505986	519035.449136	44.454913
3503.599277	519033.816355	44.459917
3503.590605	519024.564695	44.464922
3503.606189	518998.825674	44.469927
3503.637740	519000.185864	44.474932
3503.234309	519004.901398	44.479937
3503.695640	518994.007981	44.484941
3503.632024	518993.916886	44.489946
3503.730934	518986.620157	44.494951
3503.706245	518983.590255	44.499956
3503.648531	518976.773344	44.504961
3503.856634	518957.273645	44.509965
3503.493352	518974.926991	44.514970
3503.718168	518963.666433	44.519975
3503.642090	518951.745542	44.524980
3503.309094	518934.910060	44.529985
3503.507855	518918.799524	44.534989
3503.299995	518924.495434	44.539994
3503.112602	518918.811386	44.544999
3503.827059	518921.428851	44.550004
3503.560632	518926.577822	44.555009
3504.086198	518921.893478	44.560013
3503.849451	518904.233740	44.565018
3503.821550	518886.439847	44.570023
3503.806684	518883.408374	44.575028
3503.748081	518880.788319	44.580033
3503.929221	518858.764599	44.585037
3503.715653	518845.247333	44.590042
3503.841738	518836.985537	44.595047
3503.663221	518850.463607	44.600052
3503.654550	518841.211843	44.605057
3503.808307	518814.136044	44.610061
3503.478798	518819.244455	44.615066
3503.793356	518803.722267	44.620071
3503.783383	518796.442663	44.625076
3503.825947	518800.430436	44.630081
3503.893319	518775.694152	44.635085
3503.717571	518763.131551	44.640090
3503.759544	518769.597045	44.645095
3503.905993	518754.859837	44.650100
3503.796679	518736.623577	44.655105
3503.747259	518723.889287	44.660109
3503.488080	518723.121207	44.665114
3503.683990	518713.230270	44.670119
3503.774971	518716.047442	44.675124
3503.615231	518696.959522	44.680129
3503.797793	518681.963722	44.685133
3503.873211	518680.182039	44.690138
3503.761298	518676.963611	44.695143
3503.872508	518658.945229	44.700148
3503.671351	518643.403274	44.705153
3503.934742	518629.102547	44.710157
3503.641426	518643.964162	44.715162
3503.830414	518627.146989	44.720167
3503.762529	518608.196141	44.725172
3503.376718	518598.245388	44.730177
3503.747449	518587.214331	44.735181
3503.580111	518603.067355	44.740186
3503.634345	518593.805510	44.745191
3503.338473	518582.778684	44.750196
3503.445722	518559.047057	44.755201
3503.551872	518552.810843	44.760205
3503.480976	518559.951596	44.765210
3503.317178	518558.409967	44.770215
3503.615689	518558.969534	44.775220
3503.478495	518560.811510	44.780225
3503.638623	518548.145092	44.785229
3503.419078	518561.731012	44.790234
3503.376133	518539.186075	44.795239
3503.657954	518522.606945	44.800244
3503.628138	518524.179131	44.805249
3503.721807	518517.540361	44.810253
3503.370975	518516.331677	44.815258
3503.367434	518512.287056	44.820263
3503.634185	518504.609634	44.825268
3503.425891	518510.963093	44.830273
3503.126830	518489.570988	44.835277
3503.610149	518481.454808	44.840282
3503.482063	518478.997366	44.845287
3503.508769	518483.897884	44.850292
3503.361101	518471.532879	44.855297
3503.660779	518470.322503	44.860301
3503.547612	518473.121419	44.865306
3503.879245	518474.788175	44.870311
3503.311194	518455.056607	44.875316
3503.115207	518435.165078	44.880321
3503.690847	518426.478069	44.885325
3503.287886	518425.732700	44.890330
3503.618329	518426.034401	44.895335
3503.735805	518439.364893	44.900340
3503.174802	518440.616528	44.905345
3503.597400	518427.301756	44.910349
3503.560707	518438.027251	44.915354
3503.375420	518424.404039	44.920359
3503.702087	518413.329267	44.925364
3503.487972	518396.525008	44.930369
3503.250917	518405.613554	44.935373
3503.274585	518400.553309	44.940378
3503.417324	518400.935242	44.945383
3503.504946	518398.393129	44.950388
3503.245045	518407.586414	44.955393
3503.578410	518398.078081	44.960397
3503.138162	518407.603260	44.965402
3503.294003	518397.313949	44.970407
3503.869067	518395.200439	44.975412
3503.557875	518386.805273	44.980417
3503.713188	518360.537522	44.985421
3503.398051	518366.351709	44.990426
3503.720145	518360.940894	44.995431
3503.654075	518363.934644	45.000436
3503.186205	518364.969304	45.005441
3503.647198	518358.070152	45.010445
3503.608609	518350.137529	45.015450
3503.691120	518338.241693	45.020455
3503.406124	518327.516366	45.025460
3503.317396	518333.497040	45.030465
3503.740676	518317.249300	45.035469
3503.543128	518339.933635	45.040474
3503.673859	518323.681576	45.045479
3503.937177	518317.723822	45.050484
3503.760068	518292.974891	45.055489
3503.929821	518290.419779	45.060493
3503.557171	518282.691621	45.065498
3503.446812	518270.472264	45.070503
3503.761246	518249.437967	45.075508
3503.460942	518244.176053	45.080513
3503.211721	518237.186844	45.085517
3503.435708	518252.826657	45.090522
3503.511700	518249.224488	45.095527
3503.691704	518248.235273	45.100532
3503.659004	518242.779367	45.105537
3503.740942	518213.387930	45.110541
3503.775740	518211.410356	45.115546
3503.705684	518207.780697	45.120551
3503.763069	518205.142202	45.125556
3503.519089	518204.776218	45.130561
3503.892196	518181.912206	45.135565
3503.397180	518181.333072	45.140570
3503.660858	518169.762438	45.145575
3503.844251	518171.553786	45.150580
3503.619303	518175.280599	45.155585
3503.511928	518156.638866	45.160589
3503.409013	518134.406248	45.165594
3503.624191	518130.782054	45.170599
3503.505619	518122.457439	45.175604
3503.406606	518126.922843	45.180609
3503.596162	518129.825666	45.185613
3503.313874	518132.095148	45.190618
3503.622374	518126.383012	45.195623
3503.852306	518116.233512	45.200628
3503.185950	518089.994070	45.205633
3503.836938	518085.239102	45.210637
3503.352659	518093.406144	45.215642
3503.302175	518092.099390	45.220647
3503.617792	518089.217799	45.225652
3503.533497	518096.714830	45.230657
3503.762314	518084.138331	45.235661
3503.214638	518065.515522	45.240666
3503.283311	518065.403513	45.245671
3503.805639	518046.308166	45.250676
3503.386771	518053.200741	45.255681
3503.647708	518049.265902	45.260685
3503.631409	518050.937129	45.265690
3503.546312	518052.366400	45.270695
3503.597542	518047.655651	45.275700
3503.583605	518024.852598	45.280705
3503.524838	518010.450557	45.285709
3503.461106	518011.168531	45.290714
3503.482766	518011.367348	45.295719
3503.594722	518008.366234	45.300724
3503.726288	518018.711445	45.305729
3503.682610	518004.559844	45.310733
3503.495899	517995.942539	45.315738
3503.407657	517975.224369	45.320743
3503.537168	517979.501994	45.325748
3503.444749	517981.893185	45.330753
3503.736016	517965.564834	45.335757
3503.474032	517973.797932	45.340762
3503.530988	517962.310393	45.345767
3503.784513	517933.194734	45.350772
3503.602931	517934.538133	45.355777
3503.533168	517931.414029	45.360781
3503.387806	517938.667953	45.365786
3503.544186	517931.361674	45.370791
3503.562356	517934.948981	45.375796
3503.559713	517933.027858	45.380801
3503.600128	517909.558694	45.385805
3503.310968	517896.912224	45.390810
3503.145865	517893.550350	45.395815
3503.801629	517884.091898	45.400820
3503.561484	517888.680806	45.405825
3503.344441	517889.928680	45.410829
3503.285337	517894.084441	45.415834
3503.470008	517895.521653	45.420839
3503.122285	517899.419632	45.425844
3503.069788	517899.579605	45.430849
3503.645919	517889.830345	45.435853
3503.228700	517891.059292	45.440858
3503.555364	517884.737405	45.445863
3503.544479	517862.692141	45.450868
3503.164202	517864.623182	45.455873
3503.412049	517854.875223	45.460877
3503.251725	517856.619800	45.465882
3503.618500	517844.931511	45.470887
3503.599508	517844.985055	45.475892
3503.390820	517849.720701	45.480897
3503.635798	517845.586070	45.485901
3503.421635	517851.333911	45.490906
3503.434745	517831.560305	45.495911
3503.498595	517817.543248	45.500916
3503.285707	517826.426025	45.505921
3503.275481	517823.646456	45.510925
3503.524595	517817.994167	45.515930
3503.508084	517809.855529	45.520935
3503.623926	517813.629692	45.525940
3503.538191	517826.790532	45.530945
3503.630988	517804.374836	45.535949
3503.325064	517788.949768	45.540954
3503.443645	517789.841202	45.545959
3503.774131	517778.360869	45.550964
3503.571025	517780.971850	45.555969
3503.483759	517765.107666	45.560973
3503.335212	517786.369145	45.565978
3503.433400	517776.998761	45.570983
3503.358156	517762.548542	45.575988
3503.449186	517793.784361	45.580993
3503.749376	517752.221603	45.585997
3503.549419	517752.910553	45.591002
3503.269611	517731.160452	45.596007
3503.353295	517763.712228	45.601012
3503.557306	517733.946677	45.606017
3503.874728	517730.862471	45.611021
3503.555221	517744.565994	45.616026
3503.544748	517738.044505	45.621031
3503.517038	517725.659981	45.626036
3503.541058	517720.700606	45.631041
3503.704096	517708.690455	45.636045
3503.657535	517716.636796	45.641050
3503.505090	517707.710523	45.646055
3503.623333	517712.596802	45.651060
3503.722266	517697.663894	45.656065
3503.440306	517679.807722	45.661069
3503.083648	517670.964273	45.666074
3503.313528	517673.557401	45.671079
3503.463636	517663.723644	45.676084
3503.123325	517672.222107	45.681089
3503.328869	517666.728354	45.686093
3503.343752	517675.929180	45.691098
3503.403922	517667.171548	45.696103
3503.750868	517662.413950	45.701108
3503.306781	517676.491190	45.706113
3503.386383	517672.483789	45.711117
3503.530442	517650.919423	45.716122
3503.332102	517633.960192	45.721127
3503.629257	517627.390036	45.726132
3503.323947	517635.731284	45.731137
3503.557098	517633.368320	45.736141
3503.481878	517639.144840	45.741146
3503.437761	517635.156985	45.746151
3503.532140	517642.322578	45.751156
3503.469132	517625.797053	45.756161
3503.346565	517603.263424	45.761165
3503.183907	517609.812283	45.766170
3503.730257	517596.426718	45.771175
3503.734895	517594.554972	45.776180
3503.412190	517604.871108	45.781185
3503.635378	517581.827695	45.786189
3503.826378	517584.123579	45.791194
3503.794706	517578.060483	45.796199
3503.717642	517565.734207	45.801204
3503.551888	517562.726340	45.806209
3504.030590	517545.457738	45.811213
3503.760476	517564.109210	45.816218
3503.585489	517536.779875	45.821223
3503.626556	517520.237794	45.826228
3503.497830	517520.966062	45.831233
3503.457265	517515.713429	45.836237
3503.594384	517521.759833	45.841242
3503.220581	517512.615604	45.846247
3503.305710	517516.698095	45.851252
3503.503978	517514.947438	45.856257
3503.607122	517482.871272	45.861261
3503.552900	517473.929348	45.866266
3503.505733	517470.447611	45.871271
3503.637807	517473.056230	45.876276
3503.331030	517477.605215	45.881281
3503.638731	517482.916725	45.886285
3503.518614	517475.350542	45.891290
3503.352373	517463.897936	45.896295
3503.567565	517445.052713	45.901300
3503.448774	517441.177749	45.906305
3503.613460	517430.785305	45.911309
3503.364079	517436.387152	45.916314
3503.264066	517435.088174	45.921319
3503.921312	517434.781997	45.926324
3503.632079	517439.024812	45.931329
3503.809052	517419.831628	45.936333
3503.778166	517407.194528	45.941338
3504.099583	517395.209686	45.946343
3503.874350	517398.734445	45.951348
3503.845144	517386.400472	45.956353
3503.844320	517360.509787	45.961357
3503.615890	517360.647004	45.966362
3503.456093	517355.261461	45.971367
3503.374241	517358.106183	45.976372
3503.365624	517351.938224	45.981377
3503.681061	517330.649762	45.986381
3503.573545	517319.187773	45.991386
3503.842849	517308.273035	45.996391
3503.514763	517305.847028	46.001396
3503.325411	517310.731476	46.006401
3503.535925	517308.473180	46.011405
3503.523970	517307.362547	46.016410
3503.581596	517288.845460	46.021415
3503.781049	517264.086038	46.026420
3503.629979	517272.706498	46.031425
3503.775227	517259.788606	46.036429
3503.818481	517261.147090	46.041434
3503.862323	517244.199749	46.046439
3503.928854	517227.703920	46.051444
3503.592865	517236.303059	46.056449
3503.689683	517227.741676	46.061453
3503.286655	517225.833186	46.066458
3503.221371	517228.270764	46.071463
3503.374075	517200.889080	46.076468
3503.509024	517188.377307	46.081473
3503.407404	517192.995080	46.086477
3503.310228	517187.397311	46.091482
3503.144589	517189.597914	46.096487
3503.130341	517193.544485	46.101492
3503.287030	517186.086124	46.106497
3503.186579	517181.651947	46.111501
3503.511415	517192.978498	46.116506
3503.396197	517192.238158	46.121511
3503.443363	517179.436842	46.126516
3503.393654	517190.569751	46.131521
3503.359567	517192.597855	46.136525
3503.251087	517192.412704	46.141530
3503.507480	517192.827272	46.146535
3503.391141	517191.884835	46.151540
3503.153761	517193.237112	46.156545
3503.572894	517185.484427	46.161549
3503.449670	517172.811175	46.166554
3503.519565	517166.731875	46.171559
3503.724915	517159.316379	46.176564
3503.504434	517158.491538	46.181569
3503.622998	517152.758521	46.186573
3503.456506	517161.634319	46.191578
3503.496262	517160.060385	46.196583
3503.917201	517122.977570	46.201588
3503.615189	517121.255376	46.206593
3503.638476	517104.108867	46.211597
3503.810512	517116.774409	46.216602
3503.694318	517111.179620	46.221607
3503.663596	517095.760975	46.226612
3503.719567	517077.850740	46.231617
3503.535650	517069.434785	46.236621
3503.500769	517078.997790	46.241626
3503.354440	517087.718735	46.246631
3503.499529	517089.920807	46.251636
3503.327466	517074.625620	46.256641
3503.495680	517057.304449	46.261645
3503.200565	517041.017302	46.266650
3503.311227	517040.291822	46.271655
3503.644642	517038.620892	46.276660
3503.369913	517034.821049	46.281665
3503.606826	517025.175469	46.286669
3503.349445	517037.200979	46.291674
3503.295043	517044.997175	46.296679
3503.666861	517036.746210	46.301684
3503.618810	517035.236711	46.306689
3503.719242	517014.234672	46.311693
3503.303876	516997.460798	46.316698
3503.177733	516998.390956	46.321703
3503.566782	516990.946351	46.326708
3503.398928	516993.653021	46.331713
3504.047337	516986.470834	46.336717
3503.853182	516987.866865	46.341722
3503.511973	516985.695730	46.346727
3503.718530	516945.106562	46.351732
3503.434259	516952.281734	46.356737
3503.573852	516951.096554	46.361741
3503.732448	516950.565771	46.366746
3503.489976	516951.716595	46.371751
3503.695436	516938.434951	46.376756
3503.524167	516915.604668	46.381761
3503.680292	516911.534419	46.386765
3503.494572	516913.131399	46.391770
3503.362937	516920.484737	46.396775
3503.763851	516901.710682	46.401780
3503.478325	516914.903824	46.406785
3503.585499	516890.967540	46.411789
3503.441313	516880.926988	46.416794
3503.322119	516869.112547	46.421799
3503.464271	516868.483221	46.426804
3503.301160	516866.536768	46.431809
3503.396843	516852.412725	46.436813
3503.228529	516869.430662	46.441818
3503.043275	516875.073131	46.446823
3503.425908	516872.281878	46.451828
3503.166186	516876.773019	46.456833
3503.182887	516875.303841	46.461837
3503.296719	516868.509515	46.466842
3503.418960	516876.834134	46.471847
3503.653726	516876.139601	46.476852
3503.562691	516874.535743	46.481857
3503.575032	516861.941965	46.486861
3503.324540	516845.799281	46.491866
3503.199425	516838.840432	46.496871
3503.562309	516832.411283	46.501876
3503.395155	516840.073687	46.506881
3503.419697	516838.754976	46.511885
3503.450422	516841.683131	46.516890
3503.376953	516835.626370	46.521895
3503.725761	516837.543428	46.526900
3503.404390	516836.026543	46.531905
3503.568353	516815.014210	46.536909
3503.306335	516800.188115	46.541914
3503.551333	516806.470579	46.546919
3503.826147	516789.739115	46.551924
3503.412033	516785.000420	46.556929
3503.681011	516796.740629	46.561933
3503.642080	516795.027389	46.566938
3503.614297	516776.422091	46.571943
3503.563712	516759.438610	46.576948
3503.206606	516766.473664	46.581953
3503.348880	516748.246014	46.586957
3503.674766	516764.629677	46.591962
3503.806476	516755.759117	46.596967
3503.689439	516758.407223	46.601972
3503.838849	516730.317306	46.606977
3503.558237	516720.551069	46.611981
3503.543220	516717.114663	46.616986
3503.796645	516702.712710	46.621991
3503.633067	516716.038445	46.626996
3503.554343	516705.279460	46.632001
3503.927246	516680.188333	46.637005
3504.072081	516679.609147	46.642010
3503.817367	516677.778290	46.647015
3503.856597	516661.488494	46.652020
3503.823663	516649.103991	46.657025
3503.602479	516624.966374	46.662029
3503.754562	516624.487180	46.667034
3503.283010	516619.706945	46.672039
3503.599974	516626.180384	46.677044
3503.381598	516616.151397	46.682049
3503.685901	516589.250447	46.687053
3503.594295	516585.977829	46.692058
3503.638993	516585.465037	46.697063
3503.977509	516592.845349	46.702068
3503.857013	516575.721019	46.707073
3503.337575	516560.227412	46.712077
3503.339481	516545.713367	46.717082
3503.444335	516539.223748	46.722087
3503.793362	516542.708492	46.727092
3503.533874	516546.845691	46.732097
3503.770577	516537.199863	46.737101
3503.849269	516532.990049	46.742106
3503.408371	516506.459601	46.747111
3503.561791	516505.221634	46.752116
3503.600371	516513.660800	46.757121
3503.686156	516513.900070	46.762125
3503.333616	516514.967180	46.767130
3503.348336	516506.367831	46.772135
3504.113200	516492.441137	46.777140
3503.621552	516487.714610	46.782145
3503.587796	516464.861972	46.787149
3503.591637	516460.714542	46.792154
3503.337641	516471.728510	46.797159
3503.564594	516467.040109	46.802164
3503.440942	516460.080870	46.807169
3503.370405	516444.516201	46.812173
3503.274888	516449.386069	46.817178
3503.690680	516436.879913	46.822183
3503.722123	516432.070692	46.827188
3503.713406	516440.618513	46.832193
3503.630687	516444.778368	46.837197
3503.456672	516425.791224	46.842202
3503.429954	516416.338674	46.847207
3503.485663	516402.625134	46.852212
3503.640497	516396.076989	46.857217
3503.534688	516384.563513	46.862221
3503.470352	516389.681325	46.867226
3503.464142	516398.228771	46.872231
3503.656031	516396.327293	46.877236
3503.359997	516379.533932	46.882241
3503.584250	516359.624057	46.887245
3503.707332	516349.894937	46.892250
3503.595389	516355.273139	46.897255
3503.588488	516350.621668	46.902260
3503.486010	516358.122358	46.907265
3503.692129	516350.807524	46.912269
3503.686257	516324.966593	46.917274
3503.595261	516306.522474	46.922279
3503.905590	516307.535396	46.927284
3503.559274	516305.820118	46.932289
3503.640702	516304.745228	46.937293
3503.808897	516300.116640	46.942298
3503.454131	516284.293318	46.947303
3503.812496	516273.313255	46.952308
3503.787674	516263.202891	46.957313
3504.085111	516270.134698	46.962317
3503.932540	516244.620257	46.967322
3503.492698	516226.939186	46.972327
3503.583258	516213.927983	46.977332
3503.320991	516221.959705	46.982337
3503.364641	516218.918494	46.987341
3503.578306	516224.548703	46.992346
3503.578681	516223.436048	46.997351
3503.437446	516191.193728	47.002356
3503.206499	516181.217037	47.007361
3503.298986	516179.533533	47.012365
3503.447196	516184.921242	47.017370
3503.787900	516183.603079	47.022375
3503.910255	516174.025685	47.027380
3503.419739	516179.615495	47.032385
3503.599934	516170.736960	47.037389
3503.533020	516151.580860	47.042394
3503.595173	516136.652363	47.047399
3503.737717	516135.112657	47.052404
3503.242723	516135.140299	47.057409
3503.835665	516127.460797	47.062413
3503.585457	516140.648969	47.067418
3503.347286	516114.389282	47.072423
3503.851068	516093.625759	47.077428
3503.462832	516100.969444	47.082433
3503.523907	516094.638287	47.087437
3503.749153	516094.754377	47.092442
3503.392061	516107.150320	47.097447
3503.568382	516088.309705	47.102452
3503.617684	516078.288656	47.107457
3503.352097	516055.573242	47.112461
3503.506114	516058.178617	47.117466
3503.141721	516051.560689	47.122471
3503.506225	516044.574691	47.127476
3503.098252	516058.394727	47.132481
3503.367911	516051.373151	47.137485
3503.331901	516053.148838	47.142490
3503.404684	516050.608712	47.147495
3503.174234	516059.191774	47.152500
3502.689203	516064.072748	47.157505
3503.197829	516048.315024	47.162509
3503.087775	516052.732158	47.167514
3503.210264	516058.781409	47.172519
3503.367220	516058.200286	47.177524
3503.010855	516054.615407	47.182529
3503.188075	516062.274310	47.187533
3503.193116	516062.324061	47.192538
3503.231208	516059.789419	47.197543
3503.422559	516056.168542	47.202548
3502.954829	516065.547685	47.207553
3503.284119	516054.926077	47.212557
3503.352012	516067.710025	47.217562
3503.203951	516068.289694	47.222567
3503.406772	516065.021010	47.227572
3503.546392	516073.292713	47.232577
3503.742272	516059.961312	47.237581
3503.400737	516048.788294	47.242586
3503.336243	516039.897792	47.247591
3503.382361	516024.567153	47.252596
3503.176955	516031.932542	47.257601
3503.341900	516022.095469	47.262605
3503.435817	516020.462295	47.267610
3503.125643	516029.209691	47.272615
3503.286059	516013.254111	47.277620
3503.171272	516023.892366	47.282625
3503.356078	516020.373660	47.287629
3503.392546	516015.866957	47.292634
3503.132452	516008.575089	47.297639
3503.493782	516025.712462	47.302644
3503.156385	516030.114962	47.307649
3503.498823	516017.620087	47.312653
3503.169862	516030.770221	47.317658
3502.884159	516034.102537	47.322663
3503.432754	516027.441439	47.327668
3503.401421	516033.211580	47.332673
3503.106970	516032.701804	47.337677
3503.187928	516029.806379	47.342682
3503.430948	516032.751694	47.347687
3503.535668	516026.464185	47.352692
3503.220491	516016.197276	47.357697
3503.210909	515999.459399	47.362701
3503.594927	515995.201190	47.367706
3503.386750	515992.199742	47.372711
3503.381203	515994.678630	47.377716
3503.447629	515996.387560	47.382721
3503.531171	515986.411617	47.387725
3503.155552	515987.937556	47.392730
3503.195627	515987.779481	47.397735
3503.420818	515992.093070	47.402740
3503.105483	515998.211545	47.407745
3503.180117	515998.250297	47.412749
3503.331649	515984.672984	47.417754
3503.179570	515994.507998	47.422759
3503.314944	515995.599164	47.427764
3503.288443	516001.014548	47.432769
3503.585040	515998.135605	47.437773
3503.334169	516000.299264	47.442778
3503.456355	515989.710349	47.447783
3503.488515	515968.616636	47.452788
3503.006389	515969.097394	47.457793
3503.313838	515953.573667	47.462797
3503.468132	515957.342176	47.467802
3503.083768	515964.837025	47.472807
3503.424725	515951.735468	47.477812
3503.218612	515962.388197	47.482817
3503.191908	515951.013635	47.487821
3503.390387	515967.620512	47.492826
3503.223189	515965.219448	47.497831
3503.419994	515950.168356	47.502836
3503.052528	515968.786431	47.507841
3503.006184	515961.207896	47.512845
3503.351040	515973.543562	47.517850
3503.492853	515969.627063	47.522855
3503.405293	515958.009263	47.527860
3503.117286	515972.113843	47.532865
3503.147982	515957.038441	47.537869
3503.090892	515968.274479	47.542874
3503.238669	515967.037364	47.547879
3503.534366	515966.788315	47.552884
3503.312567	515967.329070	47.557889
3502.972727	515969.102217	47.562893
3503.311860	515970.161179	47.567898
3503.009726	515976.227004	47.572903
3503.282365	515966.271732	47.577908
3502.725304	515980.873981	47.582913
3503.253947	515961.067235	47.587917
3503.535038	515973.766985	47.592922
3502.932304	515968.602718	47.597927
3503.449775	515961.289073	47.602932
3503.366798	515966.157100	47.607937
3503.377175	515976.168736	47.612941
3503.194307	515977.563065	47.617946
3503.019714	515971.167966	47.622951
3503.444058	515966.599944	47.627956
3503.137306	515978.077725	47.632961
3503.093194	515985.164780	47.637965
3503.107728	515974.946876	47.642970
3503.070647	515990.377230	47.647975
3503.279363	515974.059973	47.652980
3503.152124	515980.452158	47.657985
3503.018887	515975.668835	47.662989
3503.260628	515986.250762	47.667994
3503.167079	515994.154782	47.672999
3503.158215	515991.526407	47.678004
3503.214117	515993.034712	47.683009
3503.206946	515986.259152	47.688013
3503.422794	515993.962552	47.693018
3503.322716	515994.028919	47.698023
3503.342002	515986.743456	47.703028
3503.070034	515997.760577	47.708033
3503.233392	515996.976151	47.713037
3503.401306	515987.391449	47.718042
3503.001896	515981.588183	47.723047
3503.357879	515987.195977	47.728052
3502.976573	515993.223737	47.733057
3503.249363	515983.673029	47.738061
3503.536577	515992.477739	47.743066
3503.278045	515976.487197	47.748071
3503.439544	515956.991337	47.753076
3503.471918	515954.255294	47.758081
3503.131050	515956.635472	47.763085
3503.405841	515957.350599	47.768090
3503.753527	515950.518937	47.773095
3503.389266	515958.263472	47.778100
3503.307000	515956.354705	47.783105
3503.549850	515949.741902	47.788109
3503.396739	515949.108639	47.793114
3503.196145	515954.248120	47.798119
3503.280397	515952.060172	47.803124
3503.484314	515942.065176	47.808129
3503.315403	515933.393411	47.813133
3503.345588	515924.791317	47.818138
3503.510655	515910.655509	47.823143
3503.575262	515915.753086	47.828148
3503.158952	515919.409502	47.833153
3503.291586	515914.837000	47.838157
3503.809867	515905.348591	47.843162
3503.315650	515919.081229	47.848167
3503.531702	515914.444970	47.853172
3503.518119	515914.851672	47.858177
3503.472216	515898.372296	47.863181
3503.511368	515879.350836	47.868186
3503.132797	515872.684504	47.873191
3503.296215	515864.213039	47.878196
3503.231743	515875.551451	47.883201
3503.382315	515869.762361	47.888205
3503.560639	515878.280907	47.893210
3503.475762	515881.278076	47.898215
3503.438316	515869.399431	47.903220
3503.461660	515880.976823	47.908225
3503.545925	515867.056039	47.913229
3503.468922	515870.153111	47.918234
3503.655666	515857.682724	47.923239
3503.506546	515845.619423	47.928244
3503.590258	515853.748355	47.933249
3503.544573	515837.572320	47.938253
3503.687539	515839.825467	47.943258
3503.731480	515843.308009	47.948263
3503.721376	515807.099556	47.953268
3503.569967	515811.169280	47.958273
3503.790327	515801.272747	47.963277
3503.640802	515800.588338	47.968282
3503.581281	515806.009004	47.973287
3503.424503	515785.602369	47.978292
3503.591445	515766.408863	47.983297
3503.744039	515759.456240	47.988301
3503.732416	515756.575400	47.993306
3503.271421	515763.981305	47.998311
3503.686248	515756.734368	48.003316
3503.396770	515763.253425	48.008321
3503.444847	515749.388836	48.013325
3503.421878	515728.556398	48.018330
3502.932581	515715.838748	48.023335
3503.184808	515707.049728	48.028340
3503.368661	515718.905301	48.033345
3503.299950	515706.272886	48.038349
3503.518671	515710.891010	48.043354
3503.407362	515715.308430	48.048359
3503.382064	515704.338062	48.053364
3503.427827	515715.507440	48.058369
3503.232819	515715.032509	48.063373
3503.283786	515714.518700	48.068378
3503.442254	515720.511814	48.073383
3503.678394	515715.518314	48.078388
3503.196726	515730.816886	48.083393
3503.436796	515712.269208	48.088397
3503.386103	515718.244810	48.093402
3503.167024	515698.201926	48.098407
3503.312191	515695.852597	48.103412
3503.225109	515693.641123	48.108417
3503.114846	515690.775862	48.113421
3503.403519	515695.787518	48.118426
3503.143430	515685.005966	48.123431
3503.199225	515688.891251	48.128436
3503.263638	515692.067150	48.133441
3503.135950	515685.209370	48.138445
3503.599907	515687.108364	48.143450
3503.253734	515676.947290	48.148455
3503.147170	515692.540621	48.153460
3503.104764	515686.276239	48.158465
3503.391858	515677.532265	48.163469
3503.340613	515682.445932	48.168474
3502.931553	515680.184201	48.173479
3503.153955	515688.089000	48.178484
3503.286202	515682.201595	48.183489
3503.171501	515680.045058	48.188493
3503.119053	515685.515218	48.193498
3503.173991	515685.000780	48.198503
3503.562692	515682.511811	48.203508
3503.575039	515682.256970	48.208513
3503.476318	515677.417532	48.213517
3503.489833	515682.674975	48.218522
3503.320477	515687.657882	48.223527
3503.592440	515678.410569	48.228532
3503.081435	515666.606629	48.233537
3503.143191	515647.530759	48.238541
3503.170119	515641.963426	48.243546
3502.933656	515663.140369	48.248551
3503.496938	515671.901613	48.253556
3503.281127	515674.767795	48.258561
3503.392043	515654.976139	48.263565
3503.481966	515640.396821	48.268570
3503.385725	515655.229956	48.273575
3503.542775	515642.157225	48.278580
3503.460029	515636.860091	48.283585
3503.401817	515646.629899	48.288589
3503.505246	515652.429445	48.293594
3503.383448	515650.577465	48.298599
3503.397207	515657.048634	48.303604
3503.171297	515651.470694	48.308609
3503.373146	515645.875714	48.313613
3503.303001	515636.682452	48.318618
3502.956597	515629.404059	48.323623
3503.480773	515629.978638	48.328628
3503.411293	515617.245131	48.333633
3503.336759	515615.335103	48.338637
3503.284124	515617.922636	48.343642
3502.963334	515618.377902	48.348647
3503.562147	515607.814557	48.353652
3503.233883	515616.109868	48.358657
3503.175212	515611.061787	48.363661
3503.487119	515619.812218	48.368666
3503.263809	515613.778695	48.373671
3503.395997	515607.031527	48.378676
3503.551252	515610.294230	48.383681
3503.211423	515614.899516	48.388685
3503.553950	515615.249940	48.393690
3503.371435	515610.727167	48.398695
3503.429172	515609.453684	48.403700
3503.308982	515610.231257	48.408705
3503.213837	515580.660857	48.413709
3502.987890	515578.623036	48.418714
3503.112140	515597.517819	48.423719
3503.241619	515612.922195	48.428724
3503.687766	515603.495590	48.433729
3503.309948	515581.758162	48.438733
3503.500031	515587.341741	48.443738
3503.350374	515588.123972	48.448743
3503.445124	515569.396811	48.453748
3503.125739	515586.085921	48.458753
3503.351147	515583.420454	48.463757
3503.083094	515588.823577	48.468762
3503.192415	515593.610745	48.473767
3503.522679	515572.014253	48.478772
3503.378741	515588.827350	48.483777
3503.325975	515586.863305	48.488781
3503.852418	515587.488100	48.493786
3503.080421	515573.146102	48.498791
3503.374197	515544.778502	48.503796
3503.188506	515555.832851	48.508801
3503.260311	515545.909073	48.513805
3503.613996	515536.952206	48.518810
3503.316421	515553.840196	48.523815
3503.692262	515548.672845	48.528820
3503.470292	515545.673495	48.533825
3503.579537	515548.994055	48.538829
3503.377836	515550.745411	48.543834
3503.247032	515554.306206	48.548839
3503.459884	515551.035836	48.553844
3503.559737	515528.059648	48.558849
3503.524135	515512.438013	48.563853
3503.714941	515506.794160	48.568858
3503.499156	515517.853290	48.573863
3503.580349	515501.302859	48.578868
3503.295977	515506.101705	48.583873
3503.192124	515493.525257	48.588877
3503.183946	515506.321659	48.593882
3503.306580	515500.435710	48.598887
3503.732999	515490.506424	48.603892
3503.413195	515491.366126	48.608897
3503.551343	515468.940114	48.613901
3503.523654	515472.990366	48.618906
3503.228861	515465.400302	48.623911
3503.844527	515470.461489	48.628916
3503.307580	515463.769452	48.633921
3503.288337	515470.852795	48.638925
3503.560466	515461.352467	48.643930
3503.400824	515473.464802	48.648935
3503.729010	515446.153644	48.653940
3503.781432	515430.770889	48.658945
3503.499516	515419.183433	48.663949
3503.968512	515419.463298	48.668954
3503.619815	515425.789550	48.673959
3503.760018	515386.319699	48.678964
3503.536028	515393.030844	48.683969
3503.878044	515376.742510	48.688973
3503.846744	515382.462296	48.693978
3503.492429	515387.171083	48.698983
3503.436452	515361.892893	48.703988
3503.386439	515355.123848	48.708993
3503.077022	515328.216720	48.713997
3503.853799	515341.192625	48.719002
3503.507448	515336.999117	48.724007
3503.554665	515346.600715	48.729012
3503.642574	515348.053446	48.734017
3503.755267	515340.449492	48.739021
3503.646220	515318.011775	48.744026
3503.511523	515315.757202	48.749031
3503.728167	515294.077162	48.754036
3503.643417	515306.380077	48.759041
3503.286274	515293.843514	48.764045
3503.737249	515296.098626	48.769050
3503.388674	515298.126094	48.774055
3503.603240	515271.995818	48.779060
3503.253263	515261.582220	48.784065
3503.320411	515258.081951	48.789069
3503.531342	515257.087675	48.794074
3503.168722	515264.882845	48.799079
3503.317699	515253.277742	48.804084
3503.409125	515260.798850	48.809089
3503.489655	515256.335553	48.814093
3503.475531	515258.512460	48.819098
3503.448471	515265.091382	48.824103
3503.683824	515252.107118	48.829108
3503.267918	515250.402727	48.834113
3503.329073	515224.954093	48.839117
3503.664629	515226.367692	48.844122
3503.239227	515232.402693	48.849127
3503.743538	515221.601171	48.854132
3503.594861	515232.295861	48.859137
3503.313980	515226.423020	48.864141
3503.380083	515222.922909	48.869146
3503.368400	515233.747668	48.874151
3503.696623	515226.008448	48.879156
3503.556462	515210.504206	48.884161
3503.512817	515193.770905	48.889165
3503.742160	515188.626599	48.894170
3503.504552	515195.390550	48.899175
3503.735155	515180.738021	48.904180
3503.563860	515184.861615	48.909185
3503.348415	515170.077279	48.914189
3503.574671	515155.678288	48.919194
3503.175127	515147.548314	48.924199
3503.661102	515142.363431	48.929204
3503.491086	515138.850048	48.934209
3503.539925	515141.876789	48.939213
3503.781778	515133.291407	48.944218
3503.663954	515133.967478	48.949223
3503.834186	515111.687641	48.954228
3503.604536	515103.227343	48.959233
3503.811027	515100.413065	48.964237
3503.942775	515095.284156	48.969242
3503.500405	515071.937870	48.974247
3503.654885	515062.759362	48.979252
3503.580549	515073.847003	48.984257
3503.892539	515051.443530	48.989261
3504.023362	515049.298678	48.994266
3503.647481	515031.909678	48.999271
3503.824583	515016.001084	49.004276
3503.694259	515022.950448	49.009281
3503.570824	515006.482446	49.014285
3503.479381	515013.729119	49.019290
3503.522121	515011.749910	49.024295
3503.862878	514991.668266	49.029300
3503.503228	514979.131862	49.034305
3503.564076	514970.929033	49.039309
3503.867365	514973.106382	49.044314
3503.331487	514972.078403	49.049319
3503.577436	514964.250916	49.054324
3503.508593	514944.537407	49.059329
3503.535907	514931.737503	49.064333
3503.514887	514919.349833	49.069338
3503.400091	514929.685332	49.074343
3503.316991	514914.475249	49.079348
3503.281576	514917.565923	49.084353
3503.324643	514924.589073	49.089357
3503.664746	514918.162793	49.094362
3503.244669	514931.328191	49.099367
3503.417817	514916.027032	49.104372
3503.344996	514904.557896	49.109377
3503.151895	514889.162874	49.114381
3503.270057	514882.771660	49.119386
3503.328956	514889.235992	49.124391
3503.442397	514885.880055	49.129396
3503.473211	514894.371843	49.134401
3503.446519	514885.828780	49.139405
3503.891544	514882.218131	49.144410
3503.230766	514894.713545	49.149415
3503.261897	514878.979620	49.154420
3503.584306	514890.813882	49.159425
3503.337857	514877.096272	49.164429
3503.282598	514880.493543	49.169434
3503.080469	514872.129928	49.174439
3503.257761	514886.010152	49.179444
3503.232026	514888.998150	49.184449
3503.237350	514872.155637	49.189453
3503.325741	514855.148250	49.194458
3503.474310	514845.110772	49.199463
3503.355960	514846.899601	49.204468
3503.210388	514844.343230	49.209473
3503.390440	514835.362858	49.214477
3503.348561	514852.362866	49.219482
3503.182563	514845.611947	49.224487
3503.543421	514846.364097	49.229492
3503.037003	514846.292390	49.234497
3503.080905	514852.051047	49.239501
3503.555652	514846.463244	49.244506
3503.489870	514852.188662	49.249511
3503.533453	514840.701083	49.254516
3503.025829	514854.487286	49.259521
3503.375926	514837.033912	49.264525
3503.287244	514847.061881	49.269530
3503.309834	514849.334190	49.274535
3503.366089	514837.642303	49.279540
3502.812311	514848.856448	49.284545
3502.906839	514840.597656	49.289549
3503.121255	514846.986847	49.294554
3503.283995	514839.223029	49.299559
3503.246896	514838.217356	49.304564
3503.451873	514850.677115	49.309569
3503.451417	514846.074782	49.314573
3503.508508	514850.212936	49.319578
3503.019002	514811.852772	49.324583
3503.267652	514811.965175	49.329588
3503.456812	514808.496103	49.334593
3503.150797	514811.578991	49.339597
3503.284160	514802.100224	49.344602
3503.514152	514809.903089	49.349607
3503.508777	514809.903915	49.354612
3503.253167	514819.250225	49.359617
3503.170431	514815.520676	49.364621
3503.587247	514808.424745	49.369626
3503.454112	514820.583937	49.374631
3503.443987	514810.369219	49.379636
3503.508128	514817.439658	49.384641
3503.246749	514818.745340	49.389645
3503.567601	514812.676093	49.394650
3503.305663	514792.031986	49.399655
3503.237035	514770.092903	49.404660
3503.031074	514773.868046	49.409665
3503.227593	514764.632155	49.414669
3503.237839	514770.092705	49.419674
3503.104213	514767.483857	49.424679
3503.499249	514764.892602	49.429684
3503.396798	514766.021440	49.434689
3503.367942	514765.823674	49.439693
3503.601686	514773.322508	49.444698
3503.036164	514769.719832	49.449703
3503.879619	514764.933514	49.454708
3503.386296	514776.997941	49.459713
3503.362952	514764.964554	49.464717
3503.459854	514764.190576	49.469722
3503.324893	514764.869371	49.474727
3503.473476	514744.362622	49.479732
3503.843476	514726.197923	49.484737
3503.548055	514740.456440	49.489741
3503.475938	514739.001112	49.494746
3503.445952	514738.297765	49.499751
3503.489164	514739.403582	49.504756
3503.570984	514737.418164	49.509761
3503.467956	514714.725806	49.514765
3503.688339	514695.927235	49.519770
3503.282594	514704.791577	49.524775
3503.493575	514679.975923	49.529780
3503.488239	514676.436413	49.534785
3503.441185	514692.729335	49.539789
3503.617481	514690.071490	49.544794
3503.244732	514684.718739	49.549799
3503.539895	514677.996014	49.554804
3503.431232	514678.721231	49.559809
3503.410670	514664.057373	49.564813
3503.629748	514651.985588	49.569818
3503.202396	514654.329041	49.574823
3503.084809	514649.896896	49.579828
3503.519763	514649.828124	49.584833
3503.410087	514647.974115	49.589837
3503.444947	514649.384716	49.594842
3503.452477	514654.845733	49.599847
3503.512805	514645.530150	49.604852
3503.630454	514644.348278	49.609857
3503.439464	514624.805427	49.614861
3503.690673	514609.643380	49.619866
3503.339196	514610.052944	49.624871
3503.382119	514607.163285	49.629876
3503.429944	514607.610889	49.634881
3503.136384	514611.450490	49.639885
3503.298911	514614.459357	49.644890
3503.337557	514606.967928	49.649895
3503.510973	514608.356632	49.654900
3503.577166	514603.136782	49.659905
3503.289683	514606.317931	49.664909
3503.471241	514598.854486	49.669914
3503.431647	514594.662881	49.674919
3503.526300	514578.615175	49.679924
3503.571143	514564.901845	49.684929
3503.229305	514573.503273	49.689933
3503.206779	514575.428715	49.694938
3503.249212	514576.130054	49.699943
3503.601008	514568.133924	49.704948
3503.438736	514575.998898	49.709953
3503.664969	514570.500860	49.714957
3503.677697	514559.220271	49.719962
3503.419281	514539.890285	49.724967
3503.497673	514537.399620	49.729972
3503.448187	514530.781887	49.734977
3503.363871	514535.144775	49.739981
3503.441043	514532.603726	49.744986
3503.036707	514529.835322	49.749991
3503.345320	514524.577131	49.754996
3503.302514	514526.202324	49.760001
3503.115508	514526.585894	49.765005
3503.489811	514522.480582	49.770010
3503.608386	514535.409421	49.775015
3503.462644	514530.577082	49.780020
3503.261466	514504.309016	49.785025
3503.339195	514499.340193	49.790029
3503.350678	514488.363213	49.795034
3503.345921	514495.343525	49.800039
3503.410201	514491.438937	49.805044
3503.316123	514489.380138	49.810049
3503.093964	514488.251964	49.815053
3503.272984	514491.915744	49.820058
3503.313398	514496.309504	49.825063
3503.031050	514492.662010	49.830068
3502.981286	514492.164085	49.835073
3503.279298	514492.521571	49.840077
3503.469426	514494.868601	49.845082
3503.250380	514489.339763	49.850087
3503.580073	514480.639010	49.855092
3503.272172	514495.759511	49.860097
3503.252427	514502.337575	49.865101
3503.644935	514489.327882	49.870106
3503.417232	514494.067481	49.875111
3503.298875	514480.986798	49.880116
3503.241794	514460.866247	49.885121
3503.143276	514465.534858	49.890125
3503.260989	514454.439912	49.895130
3503.068429	514451.840330	49.900135
3503.026494	514454.679236	49.905140
3503.086083	514465.796687	49.910145
3503.034755	514487.299891	49.915149
3503.150028	514500.482163	49.920154
3503.164705	514506.194982	49.925159
3503.104371	514501.450289	49.930164
3502.692380	514498.885397	49.935169
3502.751333	514493.868964	49.940173
3503.229228	514493.641675	49.945178
3502.995126	514510.925295	49.950183
3503.167710	514499.012479	49.955188
3503.156498	514497.092314	49.960193
3503.149063	514509.080133	49.965197
3503.401295	514498.065108	49.970202
3503.431502	514493.862445	49.975207
3503.301627	514505.515583	49.980212
3503.321091	514500.808853	49.985217
3503.392802	514496.093865	49.990221
3503.192385	514509.831794	49.995226
3503.183939	514514.486155	50.000231
3503.156387	514499.014031	50.005236
3503.249322	514502.033919	50.010241
3503.419597	514512.931537	50.015245
3503.274843	514501.220611	50.020250
3503.329953	514514.058345	50.025255
3503.390992	514512.531374	50.030260
3503.181296	514518.481960	50.035265
3503.442935	514501.446831	50.040269
3503.548494	514474.573892	50.045274
3503.205806	514469.266897	50.050279
3503.419768	514465.894988	50.055284
3503.644790	514469.197465	50.060289
3503.336770	514474.050918	50.065293
3503.533058	514460.414719	50.070298
3503.144784	514468.770656	50.075303
3503.314842	514472.081819	50.080308
3503.324145	514470.107832	50.085313
3503.352099	514469.951659	50.090317
3503.526332	514460.921431	50.095322
3503.257628	514475.226526	50.100327
3503.282852	514455.143536	50.105332
3503.355963	514454.322728	50.110337
3503.219591	514448.275041	50.115341
3503.384457	514434.441480	50.120346
3503.249093	514449.028983	50.125351
3503.090814	514429.632465	50.130356
3503.305916	514421.050947	50.135361
3503.302473	514437.438378	50.140365
3503.545592	514432.949163	50.145370
3503.279873	514439.566130	50.150375
3503.478479	514436.348373	50.155380
3503.495828	514430.731575	50.160385
3503.282259	514434.002227	50.165389
3503.499746	514435.738018	50.170394
3503.158978	514435.437818	50.175399
3503.131683	514417.993081	50.180404
3503.126506	514438.275207	50.185409
3503.162567	514436.600447	50.190413
3503.601372	514434.811454	50.195418
3503.176671	514445.803157	50.200423
3503.242782	514434.058854	50.205428
3503.249615	514437.092362	50.210433
3503.249485	514440.228124	50.215437
3503.271913	514431.980527	50.220442
3503.172107	514428.152436	50.225447
3503.159302	514413.133094	50.230452
3502.986190	514421.910239	50.235457
3502.990570	514436.576819	50.240461
3503.276923	514432.434808	50.245466
3503.058936	514439.550000	50.250471
3503.323720	514432.629672	50.255476
3503.478811	514439.938780	50.260481
3503.199038	514421.623570	50.265485
3503.341291	514407.540676	50.270490
3503.430474	514396.298470	50.275495
3503.372001	514388.417677	50.280500
3503.396083	514394.129048	50.285505
3503.204871	514393.602900	50.290509
3503.598660	514382.767732	50.295514
3503.378131	514397.217010	50.300519
3503.324190	514390.701081	50.305524
3503.195232	514391.783557	50.310529
3503.013715	514396.515883	50.315533
3503.491706	514399.626659	50.320538
3503.486208	514401.397698	50.325543
3503.439660	514390.328672	50.330548
3503.582992	514392.025612	50.335553
3503.395834	514383.457078	50.340557
3503.512883	514360.071954	50.345562
3503.248217	514359.709146	50.350567
3503.145658	514352.138768	50.355572
3503.381755	514348.156411	50.360577
3503.213494	514359.714564	50.365581
3503.289269	514348.525022	50.370586
3503.185277	514354.206072	50.375591
3503.330111	514346.343703	50.380596
3503.405371	514354.929894	50.385601
3503.416948	514353.309573	50.390605
3503.475586	514350.670271	50.395610
3503.353182	514351.954022	50.400615
3503.082352	514355.233740	50.405620
3503.242657	514360.974168	50.410625
3503.350496	514355.343042	50.415629
3503.278710	514350.853001	50.420634
3503.288066	514360.511726	50.425639
3503.361644	514358.982760	50.430644
3503.629752	514357.473624	50.435649
3503.290975	514342.758627	50.440653
3503.411562	514329.842367	50.445658
3503.343118	514324.087362	50.450663
3503.148033	514320.881231	50.455668
3503.480046	514309.297123	50.460673
3503.262885	514314.844342	50.465677
3503.469888	514306.820396	50.470682
3502.999332	514322.067916	50.475687
3503.167485	514309.902780	50.480692
3503.398482	514312.698571	50.485697
3502.988276	514323.890371	50.490701
3503.606171	514320.505166	50.495706
3503.233757	514323.194020	50.500711
3503.032933	514315.386270	50.505716
3503.539329	514326.433193	50.510721
3503.184955	514321.734924	50.515725
3503.382971	514313.712401	50.520730
3503.382750	514301.472718	50.525735
3503.527449	514275.453088	50.530740
3503.678982	514230.212905	50.535745
3503.054264	514197.891425	50.540749
3503.586868	514123.002812	50.545754
3503.282726	514062.458540	50.550759
3503.101764	513989.098299	50.555764
3503.059967	513899.277743	50.560769
3502.850273	513800.429647	50.565773
3503.058867	513689.628769	50.570778
3502.433901	513581.386727	50.575783
3502.864458	513451.834800	50.580788
3502.449456	513304.712443	50.585793
3502.005464	513170.491458	50.590797
3501.801968	513010.333864	50.595802
3501.612935	512867.521953	50.600807
3501.526450	512694.393979	50.605812
3501.474607	512539.063826	50.610817
3501.340460	512339.687385	50.615821
3501.186564	512132.875904	50.620826
3500.890370	511958.357200	50.625831
3500.530615	511738.623862	50.630836
3500.137147	511515.200258	50.635841
3499.766812	511299.155653	50.640845
3499.779717	511083.401835	50.645850
3499.677678	510839.182643	50.650855
3499.227166	510587.275012	50.655860
3498.925097	510336.503745	50.660865
3498.628600	510075.711120	50.665869
3498.311464	509810.415209	50.670874
3497.924279	509547.099324	50.675879
3497.811180	509257.276314	50.680884
3497.426202	508963.393336	50.685889
3497.047844	508671.831609	50.690893
3496.667415	508365.997502	50.695898
3496.472453	508056.485749	50.700903
3496.219190	507732.102208	50.705908
3495.650042	507431.088046	50.710913
3494.723189	507103.156135	50.715917
3494.902964	506777.674273	50.720922
3494.342161	506465.611296	50.725927
3493.459030	506119.893098	50.730932
3493.607484	505773.802560	50.735937
3492.839260	505419.247446	50.740941
3492.565749	505075.233882	50.745946
3491.968194	504729.291150	50.750951
3491.608653	504369.690798	50.755956
3491.040554	504010.470289	50.760961
3490.568889	503643.484065	50.765965
3490.612897	503261.276362	50.770970
3489.978895	502893.338574	50.775975
3489.465370	502506.850117	50.780980
3488.951418	502119.745922	50.785985
3488.118347	501731.823266	50.790989
3488.134094	501330.395528	50.795994
3487.576612	500933.604811	50.800999
3487.060299	500526.675234	50.806004
3486.662958	500127.209136	50.811009
3485.779275	499719.458711	50.816013
3485.705890	499302.408512	50.821018
3484.637444	498885.607151	50.826023
3484.125927	498468.910580	50.831028
3483.732546	498042.263279	50.836033
3483.406672	497620.961550	50.841037
3482.985835	497184.325047	50.846042
3481.959560	496760.025739	50.851047
3481.703581	496318.937687	50.856052
3481.151424	495897.378530	50.861057
3480.534888	495454.351932	50.866061
3480.110584	495007.486720	50.871066
3479.302678	494561.633283	50.876071
3478.531408	494109.028690	50.881076
3477.798431	493673.117014	50.886081
3477.468526	493215.559543	50.891085
3476.776255	492755.971798	50.896090
3475.925288	492323.186509	50.901095
3475.753917	491869.166129	50.906100
3475.125298	491406.850852	50.911105
3474.417559	490964.085232	50.916109
3473.841765	490495.813634	50.921114
3473.349736	490048.130235	50.926119
3472.825905	489575.522429	50.931124
3472.264396	489116.330699	50.936129
3471.196824	488639.277528	50.941133
3471.064135	488170.675283	50.946138
3470.085004	487721.696581	50.951143
3469.380009	487236.547529	50.956148
3468.921646	486763.858979	50.961153
3468.001292	486308.151034	50.966157
3467.800470	485819.998737	50.971162
3466.932198	485357.876977	50.976167
3466.174994	484880.984342	50.981172
3465.776317	484398.602391	50.986177
3464.801775	483930.738312	50.991181
3464.323340	483443.886734	50.996186
3463.487876	482975.470885	51.001191
3463.012664	482496.093440	51.006196
3462.580972	482021.358734	51.011201
3461.769855	481540.136118	51.016205
3461.205458	481053.491574	51.021210
3460.108631	480577.306780	51.026215
3459.677204	480088.590380	51.031220
3459.070752	479616.003874	51.036225
3458.199184	479131.488566	51.041229
3457.557908	478658.833963	51.046234
3456.702334	478182.705188	51.051239
3456.249948	477692.868602	51.056244
3455.752504	477217.825714	51.061249
3454.569258	476750.532822	51.066253
3454.029972	476261.688453	51.071258
3453.493138	475787.175310	51.076263
3452.858560	475297.156782	51.081268
3452.437718	474826.657453	51.086273
3451.588518	474340.957950	51.091277
3450.683731	473864.176787	51.096282
3450.062808	473378.823644	51.101287
3449.524463	472902.215423	51.106292
3448.677249	472411.653822	51.111297
3447.775156	471926.411941	51.116301
3447.205411	471450.890101	51.121306
3446.410379	470988.573785	51.126311
3445.932183	470506.627970	51.131316
3445.358789	470024.635257	51.136321
3443.911967	469544.290380	51.141325
3443.559341	469068.932849	51.146330
3442.446009	468612.089414	51.151335
3441.930639	468140.944664	51.156340
3441.561036	467667.281760	51.161345
3440.460946	467197.374398	51.166349
3439.985448	466725.329531	51.171354
3439.189540	466269.196126	51.176359
3438.779194	465797.170889	51.181364
3438.219873	465329.063313	51.186369
3437.009493	464854.202398	51.191373
3436.390017	464378.223225	51.196378
3435.887948	463921.485773	51.201383
3435.151127	463441.700808	51.206388
3434.416204	462972.656414	51.211393
3433.589537	462516.701070	51.216397
3432.892658	462042.558761	51.221402
3432.125699	461592.660520	51.226407
3431.341731	461121.402727	51.231412
3430.471541	460670.690158	51.236417
3429.695351	460201.592171	51.241421
3429.418589	459746.201712	51.246426
3428.617289	459288.906474	51.251431
3427.900853	458834.023071	51.256436
3427.227974	458375.166751	51.261441
3426.623117	457917.659749	51.266445
3426.024144	457466.432607	51.271450
3424.976276	457000.910939	51.276455
3424.166115	456540.972965	51.281460
3423.394603	456085.128596	51.286465
3422.831250	455643.244066	51.291469
3422.356736	455188.247625	51.296474
3421.276060	454732.323107	51.301479
3420.350352	454284.583940	51.306484
3419.656814	453838.777884	51.311489
3419.050094	453390.513926	51.316493
3418.595034	452944.043697	51.321498
3418.046078	452505.393370	51.326503
3417.121697	452063.292883	51.331508
3416.121810	451623.935792	51.336513
3415.440435	451180.003864	51.341517
3414.888253	450725.082420	51.346522
3414.134594	450305.907645	51.351527
3413.517477	449855.749238	51.356532
3413.111344	449404.483046	51.361537
3411.719284	448970.059700	51.366541
3411.115074	448534.539459	51.371546
3410.395089	448093.497761	51.376551
3410.152660	447659.629454	51.381556
3409.228217	447225.657940	51.386561
3408.473966	446789.113915	51.391565
3407.868880	446349.899076	51.396570
3407.265628	445927.525949	51.401575
3406.525967	445491.361645	51.406580
3406.089098	445053.517277	51.411585
3405.283657	444635.112031	51.416589
3404.370932	444186.312846	51.421594
3403.445743	443747.557325	51.426599
3402.787437	443315.654811	51.431604
3402.373396	442889.441794	51.436609
3401.501315	442464.511922	51.441613
3400.852823	442027.254877	51.446618
3399.938148	441599.829224	51.451623
3399.258629	441178.602786	51.456628
3398.710081	440751.256621	51.461633
3397.689515	440333.115367	51.466637
3397.224757	439910.411663	51.471642
3396.401405	439482.579138	51.476647
3395.946680	439071.256619	51.481652
3395.278259	438644.654244	51.486657
3394.212983	438232.322763	51.491661
3393.719588	437796.742649	51.496666
3392.762489	437388.797089	51.501671
3392.146920	436956.166326	51.506676
3391.694653	436545.588552	51.511681
3390.523757	436125.089829	51.516685
3390.099409	435702.587358	51.521690
3389.343738	435308.945343	51.526695
3388.540581	434877.831718	51.531700
3388.338213	434478.300774	51.536705
3387.139314	434062.976805	51.541709
3386.734770	433638.964211	51.546714
3385.920356	433234.432629	51.551719
3384.953472	432818.670874	51.556724
3384.625923	432417.807177	51.561729
3383.801951	432001.222484	51.566733
3382.881928	431592.923873	51.571738
3382.265696	431204.427218	51.576743
3381.485480	430780.401516	51.581748
3380.803645	430388.221141	51.586753
3380.210141	429983.654487	51.591757
3379.743029	429572.281535	51.596762
3379.034903	429173.154672	51.601767
3378.164543	428763.686554	51.606772
3377.678145	428361.947506	51.611777
3376.615874	427956.128626	51.616781
3375.894441	427546.211763	51.621786
3375.374318	427152.586228	51.626791
3374.577214	426746.656139	51.631796
3373.861018	426350.967287	51.636801
3372.875153	425959.734288	51.641805
3372.391780	425561.685850	51.646810
3371.627197	425162.812469	51.651815
3371.066648	424769.132923	51.656820
3370.330972	424370.751237	51.661825
3369.571207	423986.108243	51.666829
3369.124648	423593.028571	51.671834
3367.971145	423202.264776	51.676839
3367.679015	422806.685614	51.681844
3367.083228	422409.523148	51.686849
3366.225138	422020.854817	51.691853
3365.430909	421627.141520	51.696858
3364.574145	421232.060831	51.701863
3364.295962	420847.627923	51.706868
3363.418881	420464.376688	51.711873
3362.591401	420075.549218	51.716877
3361.863058	419676.285544	51.721882
3361.038956	419305.127123	51.726887
3360.376892	418921.820750	51.731892
3359.983351	418539.559059	51.736897
3359.069496	418163.395242	51.741901
3358.390334	417771.870440	51.746906
3357.907976	417382.544739	51.751911
3356.901065	417002.594941	51.756916
3356.034042	416624.447158	51.761921
3355.651463	416254.703307	51.766925
3355.041824	415860.956400	51.771930
3354.087674	415495.332740	51.776935
3353.778247	415101.400950	51.781940
3353.212706	414737.611760	51.786945
3352.213736	414350.765763	51.791949
3351.701779	413962.084470	51.796954
3350.798523	413586.113129	51.801959
3350.062332	413202.056055	51.806964
3349.426973	412834.696990	51.811969
3348.528347	412464.707015	51.816973
3347.887053	412089.284906	51.821978
3347.478340	411726.322846	51.826983
3346.794807	411345.358665	51.831988
3346.227512	410964.066297	51.836993
3345.324552	410591.207669	51.841997
3344.679777	410215.406707	51.847002
3343.996181	409849.746297	51.852007
3343.361302	409480.465284	51.857012
3343.019361	409102.366299	51.862017
3342.165292	408719.972662	51.867021
3341.407248	408346.377190	51.872026
3340.442378	407976.977552	51.877031
3339.728906	407609.846284	51.882036
3339.529757	407228.499357	51.887041
3338.496523	406864.078137	51.892045
3338.025024	406499.589179	51.897050
3337.167655	406126.693931	51.902055
3336.174946	405759.076440	51.907060
3335.810837	405380.477546	51.912065
3335.116370	405013.693596	51.917069
3334.697205	404644.548972	51.922074
3333.931247	404275.454837	51.927079
3332.986592	403903.995493	51.932084
3332.700903	403531.156725	51.937089
3331.630363	403167.104815	51.942093
3331.114108	402799.682249	51.947098
3330.265712	402442.373257	51.952103
3329.423375	402058.192771	51.957108
3328.950291	401706.306402	51.962113
3328.124142	401333.654422	51.967117
3327.940197	400966.641156	51.972122
3327.053439	400603.649363	51.977127
3326.395476	400239.193834	51.982132
3325.956911	399862.218557	51.987137
3324.933156	399489.983267	51.992141
3324.341609	399127.970486	51.997146
3323.720005	398766.619376	52.002151
3323.147885	398404.265055	52.007156
3322.524867	398045.702500	52.012161
3321.798432	397669.357595	52.017165
3321.443239	397291.907418	52.022170
3320.639639	396930.081962	52.027175
3319.877098	396561.687200	52.032180
3319.294374	396180.040345	52.037185
3318.424260	395812.188205	52.042189
3317.483545	395447.012601	52.047194
3316.650157	395088.019306	52.052199
3316.141846	394727.674192	52.057204
3315.441223	394366.033632	52.062209
3314.591244	394000.599255	52.067213
3314.360710	393631.554455	52.072218
3313.563770	393271.112454	52.077223
3312.638133	392913.509166	52.082228
3312.449314	392547.014004	52.087233
3311.441313	392184.636278	52.092237
3310.899113	391818.799494	52.097242
3309.911336	391458.673857	52.102247
3309.454016	391097.621544	52.107252
3308.747951	390739.884839	52.112257
3307.796168	390389.099378	52.117261
3307.244633	390025.431987	52.122266
3306.743996	389664.931187	52.127271
3305.747777	389310.709372	52.132276
3305.042383	388945.046453	52.137281
3304.171976	388606.918837	52.142285
3303.855347	388245.128577	52.147290
3303.132739	387905.572411	52.152295
3302.437259	387543.250143	52.157300
3301.705375	387189.321519	52.162305
3300.818092	386841.415281	52.167309
3300.372464	386486.747935	52.172314
3299.556984	386131.830475	52.177319
3298.739534	385783.699646	52.182324
3298.187734	385430.640918	52.187329
3297.470212	385086.607347	52.192333
3296.785158	384733.206981	52.197338
3296.012450	384388.743317	52.202343
3295.259193	384048.316915	52.207348
3294.661820	383703.666584	52.212353
3294.015924	383359.859987	52.217357
3293.590490	383007.521162	52.222362
3292.728912	382658.706767	52.227367
3292.154085	382324.797933	52.232372
3291.551237	381976.470392	52.237377
3290.604732	381627.431026	52.242381
3290.263077	381279.640739	52.247386
3289.315709	380933.825140	52.252391
3288.816567	380592.717000	52.257396
3288.140752	380243.749363	52.262401
3287.182037	379900.622225	52.267405
3286.748512	379554.280591	52.272410
3286.376849	379207.748043	52.277415
3285.227773	378876.265422	52.282420
3284.992792	378526.780242	52.287425
3283.854140	378180.792291	52.292429
3283.458829	377811.970118	52.297434
3282.681792	377474.871956	52.302439
3281.824560	377140.479785	52.307444
3281.400547	376793.044008	52.312449
3280.557671	376469.148925	52.317453
3279.946550	376111.994815	52.322458
3279.328269	375777.070148	52.327463
3278.823474	375437.037409	52.332468
3278.102569	375091.414435	52.337473
3277.243221	374745.759540	52.342477
3276.830866	374392.705054	52.347482
3276.170269	374054.313378	52.352487
3275.468822	373719.054214	52.357492
3274.778287	373365.373498	52.362497
3273.596862	373025.605773	52.367501
3272.957006	372689.946935	52.372506
3272.538701	372351.630167	52.377511
3271.697887	372006.407250	52.382516
3270.841644	371666.246291	52.387521
3270.208210	371333.526465	52.392525
3269.618101	370998.990962	52.397530
3269.031207	370670.964846	52.402535
3268.417375	370338.895526	52.407540
3268.046898	369994.497595	52.412545
3266.994710	369664.400363	52.417549
3266.729951	369312.119195	52.422554
3265.986431	368983.850502	52.427559
3265.213870	368625.029482	52.432564
3264.561070	368289.490536	52.437569
3263.772035	367963.231158	52.442573
3263.017260	367613.506938	52.447578
3262.382320	367280.628768	52.452583
3261.653145	366951.528371	52.457588
3261.332141	366605.518356	52.462593
3260.141763	366278.928340	52.467597
3259.514278	365937.312210	52.472602
3259.006221	365620.099446	52.477607
3258.138017	365283.706684	52.482612
3257.980448	364935.876886	52.487617
3257.024658	364615.318501	52.492621
3256.237578	364272.926238	52.497626
3255.193458	363945.329292	52.502631
3254.923227	363607.099336	52.507636
3254.208304	363279.241996	52.512641
3253.830308	362946.978091	52.517645
3252.782361	362605.632395	52.522650
3252.174595	362279.710215	52.527655
3251.629525	361942.198537	52.532660
3250.999025	361603.349360	52.537665
3249.879802	361280.961605	52.542669
3249.471055	360949.833350	52.547674
3248.790128	360622.969754	52.552679
3248.259683	360293.026641	52.557684
3247.747776	359959.007000	52.562689
3246.699577	359632.042021	52.567693
3246.080097	359297.398635	52.572698
3245.490513	358977.481546	52.577703
3244.799296	358644.142734	52.582708
3244.296596	358309.474038	52.587713
3243.472846	357991.852237	52.592717
3242.751123	357647.900155	52.597722
3242.008666	357324.001232	52.602727
3241.175276	356993.218367	52.607732
3240.543096	356674.718003	52.612737
3239.826254	356349.307256	52.617741
3239.278144	356017.785688	52.622746
3238.974846	355700.066855	52.627751
3238.111718	355365.740651	52.632756
3237.690574	355037.068169	52.637761
3236.822506	354717.193051	52.642765
3236.066981	354386.635180	52.647770
3235.595027	354062.316147	52.652775
3234.633825	353729.445291	52.657780
3234.009678	353400.107282	52.662785
3233.025815	353076.957338	52.667789
3232.705736	352746.803607	52.672794
3232.184324	352422.278530	52.677799
3231.459078	352100.226859	52.682804
3230.962796	351764.801287	52.687809
3229.740889	351445.470969	52.692813
3229.203274	351117.097481	52.697818
3228.655239	350792.515715	52.702823
3227.824374	350463.141137	52.707828
3227.281289	350144.968185	52.712833
3226.562510	349830.231554	52.717837
3225.979821	349506.385597	52.722842
3225.045192	349185.825673	52.727847
3224.273316	348860.606005	52.732852
3224.237981	348526.079958	52.737857
3222.728343	348218.992769	52.742861
3222.260448	347886.745565	52.747866
3221.782463	347576.106550	52.752871
3221.006356	347263.654981	52.757876
3220.704999	346933.640992	52.762881
3219.752926	346618.744828	52.767885
3219.446000	346297.178144	52.772890
3218.416881	345978.396406	52.777895
3217.966664	345659.826742	52.782900
3217.488302	345334.005717	52.787905
3216.626147	345009.872556	52.792909
3215.590043	344684.034292	52.797914
3215.390421	344372.341130	52.802919
3214.274332	344047.708268	52.807924
3214.005703	343717.416136	52.812929
3213.206682	343414.517816	52.817933
3212.494506	343079.837910	52.822938
3211.612371	342760.149913	52.827943
3210.829068	342442.939070	52.832948
3210.628374	342120.263554	52.837953
3209.758890	341816.171951	52.842957
3209.038175	341498.258983	52.847962
3208.467476	341177.266078	52.852967
3207.690395	340849.405916	52.857972
3207.143792	340540.547769	52.862977
3205.863561	340229.182281	52.867981
3205.724464	339914.885555	52.872986
3205.040731	339598.458806	52.877991
3204.424382	339282.885286	52.882996
3203.890318	338962.638817	52.888001
3202.721722	338653.971595	52.893005
3202.342440	338327.206260	52.898010
3201.576848	338018.014005	52.903015
3200.869669	337706.214515	52.908020
3200.306461	337397.318196	52.913025
3199.532236	337074.707433	52.918029
3199.219546	336759.480771	52.923034
3198.218954	336443.266798	52.928039
3197.636536	336135.716763	52.933044
3197.133891	335814.660626	52.938049
3196.606263	335505.571607	52.943053
3195.561121	335195.010164	52.948058
3195.160656	334872.609590	52.953063
3194.543172	334557.598942	52.958068
3193.728694	334243.636296	52.963073
3192.727905	333925.908530	52.968077
3192.284440	333610.585962	52.973082
3191.554651	333292.736033	52.978087
3190.594632	332978.943404	52.983092
3190.508343	332673.106741	52.988097
3189.722586	332361.778653	52.993101
3189.028197	332047.787095	52.998106
3188.376356	331731.852595	53.003111
3187.671345	331417.554443	53.008116
3187.250462	331100.893246	53.013121
3186.132048	330792.258629	53.018125
3185.432097	330476.631740	53.023130
3184.882237	330157.135467	53.028135
3184.015100	329847.311460	53.033140
3183.821330	329539.543631	53.038145
3182.875593	329230.747841	53.043149
3182.335816	328915.572666	53.048154
3181.613895	328612.441777	53.053159
3180.749635	328294.514821	53.058164
3180.271454	327989.586181	53.063169
3179.640453	327678.162844	53.068173
3178.968687	327362.212867	53.073178
3178.371183	327048.668533	53.078183
3177.122727	326733.902012	53.083188
3176.747788	326433.584612	53.088193
3176.213095	326127.180916	53.093197
3175.644319	325810.546422	53.098202
3175.134040	325501.259447	53.103207
3174.268556	325194.115233	53.108212
3173.578472	324876.936118	53.113217
3172.798949	324577.210433	53.118221
3172.375122	324265.129852	53.123226
3171.606591	323947.501250	53.128231
3170.744685	323638.772055	53.133236
3170.405638	323335.891399	53.138241
3169.211073	323022.960577	53.143245
3168.459213	322710.416849	53.148250
3168.096945	322409.904432	53.153255
3167.542037	322102.012183	53.158260
3166.861656	321792.305459	53.163265
3166.012793	321487.869362	53.168269
3165.580856	321176.135131	53.173274
3164.584349	320875.081194	53.178279
3163.946249	320571.423343	53.183284
3163.540000	320268.135159	53.188289
3162.652539	319965.405863	53.193293
3162.200201	319651.148775	53.198298
3161.510431	319350.677726	53.203303
3160.578732	319045.558916	53.208308
3160.229019	318731.129650	53.213313
3159.571628	318428.969951	53.218317
3158.582361	318117.669827	53.223322
3158.169365	317822.751771	53.228327
3157.254872	317504.868448	53.233332
3156.820207	317199.232105	53.238337
3155.869130	316895.764449	53.243341
3155.261529	316587.021599	53.248346
3154.632145	316291.089092	53.253351
3153.839949	315990.598103	53.258356
3153.430676	315687.550225	53.263361
3152.599197	315394.829898	53.268365
3151.793833	315082.752491	53.273370
3151.379548	314781.001289	53.278375
3150.427273	314484.477931	53.283380
3150.125555	314184.515057	53.288385
3149.386080	313881.845048	53.293389
3148.509313	313575.732824	53.298394
3147.879457	313266.066643	53.303399
3147.038594	312976.905839	53.308404
3146.499020	312669.337125	53.313409
3145.919317	312373.971108	53.318413
3145.344644	312067.832212	53.323418
3144.586770	311766.585084	53.328423
3143.690897	311485.068219	53.333428
3143.225680	311174.071325	53.338433
3142.405074	310885.207336	53.343437
3141.972292	310578.099693	53.348442
3141.510480	310280.264862	53.353447
3140.449532	309980.639687	53.358452
3139.830536	309677.327836	53.363457
3138.906966	309382.925076	53.368461
3138.412554	309082.749583	53.373466
3137.709636	308778.481032	53.378471
3137.333296	308491.934469	53.383476
3136.713624	308191.572839	53.388481
3135.677878	307900.545540	53.393485
3135.128225	307597.624877	53.398490
3134.535073	307296.238258	53.403495
3133.868200	307003.673509	53.408500
3133.567293	306704.480156	53.413505
3132.450233	306409.209565	53.418509
3131.838301	306111.057183	53.423514
3131.121060	305817.835592	53.428519
3130.281314	305526.568100	53.433524
3130.061204	305223.003958	53.438529
3128.979639	304928.921287	53.443533
3128.535965	304628.956349	53.448538
3127.818264	304336.470077	53.453543
3127.235672	304039.352512	53.458548
3126.848459	303737.797821	53.463553
3125.568346	303453.012939	53.468557
3125.227010	303152.646629	53.473562
3124.495341	302851.068159	53.478567
3123.728894	302553.594582	53.483572
3123.203485	302259.494703	53.488577
3122.418921	301970.553923	53.493581
3121.964859	301669.973208	53.498586
3121.319828	301383.581296	53.503591
3120.641945	301085.123064	53.508596
3119.928149	300782.391607	53.513601
3118.881551	300489.134758	53.518605
3118.338153	300190.780865	53.523610
3118.084334	299898.594391	53.528615
3117.167819	299603.278018	53.533620
3116.391072	299311.402436	53.538625
3115.659471	299019.289996	53.543629
3115.326011	298719.677801	53.548634
3114.667189	298426.483219	53.553639
3113.576214	298135.546655	53.558644
3113.255283	297846.626950	53.563649
3112.164347	297560.069693	53.568653
3111.626127	297267.185147	53.573658
3111.090987	296975.318311	53.578663
3110.261332	296687.954317	53.583668
3109.711466	296391.275645	53.588673
3108.647566	296095.365456	53.593677
3108.262773	295801.639367	53.598682
3107.491266	295518.339108	53.603687
3106.900097	295230.629565	53.608692
3106.669073	294934.891408	53.613697
3105.304523	294654.103135	53.618701
3104.753384	294366.971763	53.623706
3104.082201	294075.580499	53.628711
3103.371705	293792.650175	53.633716
3102.973654	293511.478208	53.638721
3102.484468	293222.629169	53.643725
3101.997566	292934.110464	53.648730
3101.095096	292642.346390	53.653735
3099.959567	292346.569504	53.658740
3099.827062	292056.822097	53.663745
3099.120484	291770.526884	53.668749
3098.307386	291484.732067	53.673754
3097.713340	291203.995752	53.678759
3097.087311	290909.257020	53.683764
3096.563475	290609.229978	53.688769
3095.455986	290330.356670	53.693773
3094.962826	290033.711295	53.698778
3094.349845	289744.470176	53.703783
3093.484029	289469.836284	53.708788
3093.182644	289176.037466	53.713793
3092.364253	288895.181374	53.718797
3091.547335	288603.271758	53.723802
3090.892961	288319.995178	53.728807
3090.204247	288027.555346	53.733812
3089.769804	287731.585897	53.738817
3088.763617	287456.437499	53.743821
3088.392114	287169.218508	53.748826
3087.971059	286881.370407	53.753831
3087.022828	286592.255685	53.758836
3086.451472	286301.858612	53.763841
3085.547037	286025.903421	53.768845
3084.820169	285727.609944	53.773850
3084.393284	285445.466413	53.778855
3083.555484	285163.846126	53.783860
3083.121173	284874.037467	53.788865
3082.371699	284592.988557	53.793869
3081.360875	284303.525407	53.798874
3080.791732	284016.768181	53.803879
3079.848845	283736.691629	53.808884
3079.600638	283451.360395	53.813889
3078.630224	283177.680358	53.818893
3077.911712	282900.241945	53.823898
3077.529301	282621.425837	53.828903
3076.826371	282341.208614	53.833908
3076.170572	282049.523085	53.838913
3075.180549	281770.904563	53.843917
3074.639217	281488.751211	53.848922
3074.281548	281205.906484	53.853927
3073.097983	280932.259039	53.858932
3072.800905	280654.141571	53.863937
3072.013956	280375.108255	53.868941
3071.307564	280079.380344	53.873946
3070.835270	279804.321001	53.878951
3069.986091	279514.880673	53.883956
3069.461240	279239.345556	53.888961
3069.038774	278961.349188	53.893965
3068.028505	278671.246433	53.898970
3067.746118	278393.609757	53.903975
3066.674284	278114.799066	53.908980
3066.265680	277822.130428	53.913985
3065.567347	277550.213356	53.918989
3065.324521	277270.685502	53.923994
3064.316769	276983.765489	53.928999
3063.485763	276697.785252	53.934004
3063.103561	276412.447057	53.939009
3062.163242	276137.562790	53.944013
3061.464731	275853.344263	53.949018
3060.695752	275570.563093	53.954023
3060.166040	275295.537363	53.959028
3059.322011	275012.309608	53.964033
3058.672891	274735.290752	53.969037
3058.211359	274457.274405	53.974042
3057.554100	274169.891201	53.979047
3056.679260	273898.689402	53.984052
3056.125720	273618.802980	53.989057
3055.267420	273349.050291	53.994061
3054.847485	273069.219169	53.999066
3054.138234	272788.109511	54.004071
3053.489811	272511.982062	54.009076
3052.959455	272234.842698	54.014081
3052.011636	271954.433095	54.019085
3051.460064	271667.822951	54.024090
3050.700951	271399.226376	54.029095
3049.765740	271121.820211	54.034100
3049.301179	270848.465491	54.039105
3048.608485	270573.236822	54.044109
3047.884903	270306.341261	54.049114
3047.298864	270028.472624	54.054119
3046.612905	269754.414668	54.059124
3046.101919	269475.108103	54.064129
3045.096703	269212.383319	54.069133
3044.563144	268933.233331	54.074138
3043.979301	268661.528147	54.079143
3043.212146	268393.850603	54.084148
3042.813151	268108.872883	54.089153
3042.070552	267846.259864	54.094157
3041.496283	267574.579090	54.099162
3040.887011	267301.070271	54.104167
3040.039118	267020.162635	54.109172
3039.445468	266747.593942	54.114177
3038.473761	266472.665752	54.119181
3038.059256	266203.023303	54.124186
3037.252983	265927.203314	54.129191
3036.326450	265658.278919	54.134196
3036.210690	265386.934221	54.139201
3035.285875	265119.206877	54.144205
3034.511810	264851.379435	54.149210
3033.978798	264579.693797	54.154215
3033.058988	264308.196904	54.159220
3032.535779	264027.978285	54.164225
3031.585231	263766.495573	54.169229
3031.037368	263494.634761	54.174234
3030.216116	263237.181368	54.179239
3029.323783	262970.137985	54.184244
3029.270958	262704.362662	54.189249
3028.734601	262437.161471	54.194253
3027.699036	262168.333159	54.199258
3027.288539	261904.677981	54.204263
3026.542674	261642.145753	54.209268
3026.053068	261369.717124	54.214273
3024.932332	261111.421406	54.219277
3024.238569	260837.446560	54.224282
3023.807785	260574.916310	54.229287
3023.073477	260310.677064	54.234292
3022.657522	260039.562319	54.239297
3021.899834	259779.860524	54.244301
3021.404136	259508.504241	54.249306
3020.638582	259243.710664	54.254311
3019.660504	258974.290413	54.259316
3019.293427	258703.551281	54.264321
3018.784102	258440.882705	54.269325
3017.952070	258165.862783	54.274330
3017.546717	257898.899767	54.279335
3016.584867	257629.529315	54.284340
3015.842442	257361.907154	54.289345
3015.416277	257101.900934	54.294349
3014.869462	256836.795150	54.299354
3013.928434	256566.811400	54.304359
3013.141052	256297.975149	54.309364
3012.427565	256023.117236	54.314369
3011.749068	255760.198287	54.319373
3011.166537	255486.186208	54.324378
3010.864539	255231.026755	54.329383
3009.666623	254971.374397	54.334388
3009.383871	254695.889728	54.339393
3008.574711	254432.993114	54.344397
3007.954329	254169.073742	54.349402
3006.905756	253903.872743	54.354407
3006.401389	253641.361862	54.359412
3006.172358	253370.250841	54.364417
3004.996354	253117.830046	54.369421
3004.336070	252851.983282	54.374426
3004.020166	252580.734335	54.379431
3003.243049	252332.402556	54.384436
3002.688106	252055.131108	54.389441
3001.748326	251794.143337	54.394445
3000.993262	251530.707367	54.399450
3000.925311	251263.343016	54.404455
3000.027184	251004.208885	54.409460
2999.499093	250734.829916	54.414465
2998.447185	250472.919598	54.419469
2998.054500	250208.969875	54.424474
2997.464069	249941.384694	54.429479
2996.545120	249676.016597	54.434484
2996.168423	249399.205069	54.439489
2995.268781	249143.690285	54.444493
2994.391818	248882.824388	54.449498
2993.785083	248617.281276	54.454503
2992.929453	248361.939047	54.459508
2992.432169	248096.379492	54.464513
2991.217089	247847.283301	54.469517
2990.928181	247583.754406	54.474522
2990.482620	247321.167547	54.479527
2989.547382	247069.227069	54.484532
2989.087602	246818.739712	54.489537
2988.434784	246554.353466	54.494541
2987.636914	246294.778250	54.499546
2987.103791	246031.239850	54.504551
2985.989069	245779.584673	54.509556
2985.878627	245520.538685	54.514561
2985.187415	245268.970169	54.519565
2984.626969	245014.070870	54.524570
2984.073537	244751.072862	54.529575
2982.866482	244487.440329	54.534580
2982.187881	244231.924550	54.539585
2981.882745	243972.861365	54.544589
2980.996345	243703.144289	54.549594
2980.680195	243451.952678	54.554599
2980.003108	243191.014536	54.559604
2979.256514	242933.907711	54.564609
2978.412922	242672.487666	54.569613
2977.955697	242413.171529	54.574618
2977.245868	242160.898819	54.579623
2976.289769	241901.662706	54.584628
2976.085076	241640.474696	54.589633
2975.261228	241381.957215	54.594637
2974.496514	241116.428065	54.599642
2973.845714	240865.523750	54.604647
2972.798921	240601.924778	54.609652
2972.566520	240349.325553	54.614657
2971.787369	240095.616576	54.619661
2971.190816	239838.186864	54.624666
2970.489482	239581.309059	54.629671
2969.777848	239327.438264	54.634676
2969.341784	239057.558179	54.639681
2968.424036	238810.290983	54.644685
2967.676610	238547.642354	54.649690
2967.165079	238288.751169	54.654695
2966.341304	238047.251154	54.659700
2965.659803	237775.503158	54.664705
2965.138643	237529.958482	54.669709
2964.313768	237273.130928	54.674714
2964.103595	237014.627893	54.679719
2962.869557	236759.445091	54.684724
2962.299202	236509.046888	54.689729
2961.412117	236258.903123	54.694733
2960.801246	236008.767143	54.699738
2960.122012	235759.482879	54.704743
2959.474123	235509.353944	54.709748
2959.362206	235248.853469	54.714753
2958.272384	234995.205367	54.719757
2957.764221	234760.283296	54.724762
2957.277465	234501.753808	54.729767
2956.365157	234254.598064	54.734772
2956.005870	233986.348178	54.739777
2955.347753	233731.590883	54.744781
2954.743073	233479.066533	54.749786
2954.174396	233215.486154	54.754791
2952.903173	232965.767723	54.759796
2952.552509	232714.096318	54.764801
2951.864234	232460.951241	54.769805
2951.271709	232210.210631	54.774810
2950.590186	231951.260299	54.779815
2949.881595	231702.449094	54.784820
2949.511222	231438.434746	54.789825
2948.373127	231184.345752	54.794829
2947.972911	230925.226369	54.799834
2947.035942	230669.553718	54.804839
2946.291906	230427.218942	54.809844
2945.983918	230161.976125	54.814849
2944.789265	229918.644614	54.819853
2944.370650	229671.040562	54.824858
2943.934949	229413.407846	54.829863
2943.239107	229162.997323	54.834868
2942.585289	228901.224839	54.839873
2941.676819	228660.423057	54.844877
2941.094888	228408.850830	54.849882
2940.382500	228157.070816	54.854887
2939.640442	227909.293694	54.859892
2939.405262	227647.204024	54.864897
2938.630397	227402.514380	54.869901
2937.702665	227148.097919	54.874906
2937.109550	226897.753964	54.879911
2936.464503	226651.110842	54.884916
2935.916317	226395.719919	54.889921
2935.445321	226156.969097	54.894925
2934.336586	225898.320292	54.899930
2934.181877	225644.142398	54.904935
2932.988064	225397.844435	54.909940
2932.313221	225137.156077	54.914945
2931.520965	224888.020829	54.919949
2930.933941	224647.408613	54.924954
2930.433080	224403.537243	54.929959
2929.357926	224160.877790	54.934964
2929.010286	223907.295940	54.939969
2927.952895	223664.838849	54.944973
2927.423627	223424.335694	54.949978
2927.027608	223172.864294	54.954983
2926.020393	222935.697188	54.959988
2925.776472	222686.290978	54.964993
2924.936037	222445.330859	54.969997
2924.389865	222203.370147	54.975002
2923.624286	221957.384091	54.980007
2922.816660	221714.626123	54.985012
2922.483413	221468.891413	54.990017
2921.595675	221215.212802	54.995021
2920.923597	220969.355123	55.000026
2920.558824	220720.992754	55.005031
2919.348851	220484.285343	55.010036
2919.065958	220242.925610	55.015041
2918.120069	219999.902218	55.020045
2917.455779	219751.730492	55.025050
2917.087687	219502.748927	55.030055
2916.301224	219262.655936	55.035060
2915.815255	219018.391825	55.040065
2914.921766	218779.182954	55.045069
2914.427377	218526.265859	55.050074
2913.972988	218282.050122	55.055079
2913.083365	218048.978541	55.060084
2912.395381	217791.397579	55.065089
2911.749717	217549.085796	55.070093
2911.142623	217303.153664	55.075098
2910.279490	217060.852511	55.080103
2909.673970	216814.438116	55.085108
2909.255558	216567.409421	55.090113
2908.579348	216331.089240	55.095117
2907.727383	216088.280504	55.100122
2907.422529	215842.458355	55.105127
2906.408104	215595.705667	55.110132
2905.428199	215344.544251	55.115137
2904.891603	215112.813908	55.120141
2904.442504	214863.174017	55.125146
2903.969066	214620.806921	55.130151
2903.109213	214374.886963	55.135156
2902.600939	214127.983047	55.140161
2901.741113	213889.600125	55.145165
2901.207110	213643.262110	55.150170
2900.494895	213389.761693	55.155175
2899.796108	213143.642537	55.160180
2899.119984	212904.139405	55.165185
2898.672261	212658.758719	55.170189
2897.659588	212410.108162	55.175194
2896.998749	212163.846638	55.180199
2896.158278	211943.452495	55.185204
2895.736004	211689.772694	55.190209
2894.942206	211445.291408	55.195213
2894.391138	211201.561743	55.200218
2893.878854	210960.805187	55.205223
2892.746391	210730.571842	55.210228
2892.559892	210491.967379	55.215233
2891.729960	210248.730970	55.220237
2890.803028	210004.441726	55.225242
2890.536201	209765.979988	55.230247
2889.648442	209529.755712	55.235252
2888.935114	209279.326207	55.240257
2888.142861	209044.552308	55.245261
2887.736692	208808.101771	55.250266
2887.383800	208563.370882	55.255271
2886.394068	208329.254602	55.260276
2885.544819	208082.606020	55.265281
2884.994223	207849.580216	55.270285
2884.677952	207603.549166	55.275290
2883.853294	207370.683131	55.280295
2882.643617	207127.213638	55.285300
2882.414244	206879.288149	55.290305
2881.837545	206651.196448	55.295309
2880.953564	206409.358245	55.300314
2880.549609	206170.232201	55.305319
2879.763990	205934.323811	55.310324
2879.098205	205690.697665	55.315329
2878.286198	205450.697345	55.320333
2877.785644	205214.975762	55.325338
2877.164133	204963.493230	55.330343
2876.596577	204737.341886	55.335348
2875.963452	204495.280889	55.340353
2875.080804	204252.127752	55.345357
2874.238123	204016.452453	55.350362
2873.831598	203769.929797	55.355367
2873.011980	203534.596425	55.360372
2872.277714	203289.616707	55.365377
2871.343684	203063.899002	55.370381
2870.868511	202831.975509	55.375386
2870.747753	202594.626413	55.380391
2869.709996	202357.932565	55.385396
2869.088431	202116.057942	55.390401
2868.674032	201885.910344	55.395405
2867.717385	201653.571619	55.400410
2867.176206	201405.171662	55.405415
2866.887380	201169.305942	55.410420
2866.254905	200920.057252	55.415425
2865.493516	200687.907974	55.420429
2864.941964	200438.241419	55.425434
2864.319653	200184.947685	55.430439
2863.200806	199952.183662	55.435444
2862.687933	199701.241783	55.440449
2862.050130	199457.587049	55.445453
2861.419657	199217.317191	55.450458
2861.005720	198973.298322	55.455463
2860.172636	198742.148521	55.460468
2859.460873	198492.185408	55.465473
2858.633217	198249.049752	55.470477
2857.855298	198003.616814	55.475482
2857.359590	197760.087242	55.480487
2856.255918	197536.556884	55.485492
2855.623733	197299.566215	55.490497
2855.240639	197058.605188	55.495501
2854.481602	196816.088752	55.500506
2853.643559	196576.156342	55.505511
2853.187519	196346.865979	55.510516
2852.306359	196097.971708	55.515521
2851.662945	195873.624798	55.520525
2851.195620	195634.999544	55.525530
2850.643561	195397.559458	55.530535
2849.651904	195168.766309	55.535540
2849.291522	194933.104873	55.540545
2848.549966	194695.023654	55.545549
2847.790399	194458.422405	55.550554
2847.078565	194223.812386	55.555559
2846.496191	193993.929031	55.560564
2845.918746	193752.174427	55.565569
2844.848724	193519.393036	55.570573
2844.232153	193288.449497	55.575578
2844.190914	193053.496964	55.580583
2843.150526	192820.548714	55.585588
2842.822852	192579.447288	55.590593
2842.233236	192345.462868	55.595597
2841.369560	192110.517790	55.600602
2840.787053	191861.368001	55.605607
2840.102766	191630.430159	55.610612
2839.585227	191386.120131	55.615617
2838.304887	191162.938381	55.620621
2837.831100	190919.094518	55.625626
2837.245414	190677.941473	55.630631
2836.541232	190441.923105	55.635636
2835.945547	190207.746276	55.640641
2835.331083	189976.843379	55.645645
2834.506365	189732.068664	55.650650
2833.982676	189503.418353	55.655655
2833.368097	189265.152321	55.660660
2832.514937	189025.716595	55.665665
2831.874925	188797.037193	55.670669
2830.753749	188563.269689	55.675674
2830.605177	188326.015982	55.680679
2829.610542	188105.792997	55.685684
2828.975290	187868.669554	55.690689
2828.383159	187640.509783	55.695693
2827.516923	187411.503968	55.700698
2826.919658	187179.174324	55.705703
2826.424776	186956.676631	55.710708
2825.965307	186717.673735	55.715713
2825.116600	186493.618580	55.720717
2824.537017	186269.776327	55.725722
2824.141781	186020.347502	55.730727
2823.142836	185799.818053	55.735732
2822.358751	185564.765442	55.740737
2821.558702	185336.281008	55.745741
2820.973995	185109.531932	55.750746
2820.591380	184878.146736	55.755751
2819.686232	184655.941417	55.760756
2819.101926	184421.677244	55.765761
2818.352212	184196.917975	55.770765
2817.467535	183969.535149	55.775770
2816.968596	183744.445828	55.780775
2816.621524	183520.300400	55.785780
2815.845459	183288.909339	55.790785
2814.980704	183061.591570	55.795789
2814.671057	182834.263370	55.800794
2813.932536	182602.666390	55.805799
2813.117829	182380.750610	55.810804
2812.819571	182144.990148	55.815809
2812.108143	181908.876598	55.820813
2811.242902	181679.823250	55.825818
2810.623937	181448.416928	55.830823
2809.768114	181212.037421	55.835828
2809.164483	180990.146117	55.840833
2808.335161	180760.214181	55.845837
2807.764578	180529.809988	55.850842
2807.372717	180299.302392	55.855847
2806.456332	180085.479067	55.860852
2806.021529	179845.135196	55.865857
2805.301012	179624.121660	55.870861
2804.225820	179394.744743	55.875866
2803.990483	179163.785954	55.880871
2803.038036	178938.551487	55.885876
2802.683299	178708.479028	55.890881
2802.034669	178486.849436	55.895885
2801.754262	178253.689474	55.900890
2801.065909	178014.833398	55.905895
2800.207849	177793.291488	55.910900
2799.447749	177546.079935	55.915905
2798.662982	177317.367831	55.920909
2797.582013	177091.807421	55.925914
2797.138993	176854.534448	55.930919
2796.487811	176634.937390	55.935924
2795.907986	176411.717941	55.940929
2795.006199	176187.253337	55.945933
2794.308385	175958.395012	55.950938
2794.052855	175729.124489	55.955943
2793.011599	175513.957765	55.960948
2792.426268	175282.745096	55.965953
2791.979718	175057.782097	55.970957
2791.562886	174832.484941	55.975962
2790.924528	174589.736010	55.980967
2790.112074	174366.564505	55.985972
2789.388058	174142.210117	55.990977
2788.524536	173917.128680	55.995981
2787.917853	173691.244713	56.000986
2787.078099	173452.197369	56.005991
2786.349694	173229.489397	56.010996
2786.092278	173006.262923	56.016001
2785.726056	172781.109063	56.021005
2784.649858	172553.550765	56.026010
2784.213327	172325.421883	56.031015
2783.471164	172095.269710	56.036020
2783.150040	171860.333892	56.041025
2782.242979	171633.326365	56.046029
2781.326047	171406.181810	56.051034
2780.945409	171174.578784	56.056039
2780.042388	170952.178282	56.061044
2779.667415	170712.628662	56.066049
2778.850160	170485.537220	56.071053
2778.042634	170243.083135	56.076058
2777.473714	170021.754111	56.081063
2776.782298	169802.264290	56.086068
2776.366779	169569.417293	56.091073
2775.435787	169342.884641	56.096077
2774.805256	169107.314901	56.101082
2774.177311	168877.901112	56.106087
2773.346645	168659.864106	56.111092
2772.753091	168417.374834	56.116097
2772.268876	168192.355040	56.121101
2771.261704	167973.688630	56.126106
2770.639319	167747.841332	56.131111
2770.045804	167521.049790	56.136116
2769.331063	167289.777246	56.141121
2768.593398	167078.143530	56.146125
2768.078408	166846.295253	56.151130
2767.735718	166614.548266	56.156135
2766.586537	166392.747167	56.161140
2766.047627	166165.064983	56.166145
2765.420735	165943.577995	56.171149
2764.866099	165721.483231	56.176154
2763.932175	165493.880409	56.181159
2763.135561	165273.454241	56.186164
2762.494995	165043.137430	56.191169
2761.768131	164829.683651	56.196173
2761.196011	164613.345633	56.201178
2760.805636	164378.377645	56.206183
2759.663556	164167.320350	56.211188
2759.332786	163938.957619	56.216193
2758.619330	163708.368217	56.221197
2757.947839	163440.633237	56.226202
2757.499211	163211.518085	56.231207
2756.971329	162991.113838	56.236212
2756.611453	162762.190882	56.241217
2755.855157	162536.765109	56.246221
2754.659371	162308.371574	56.251226
2754.363883	162071.254599	56.256231
2753.422610	161854.927783	56.261236
2753.032526	161623.346775	56.266241
2751.997524	161406.846779	56.271245
2751.318932	161184.544830	56.276250
2750.929249	160953.629204	56.281255
2749.891165	160729.874044	56.286260
2749.333500	160503.692108	56.291265
2748.873003	160288.849669	56.296269
2748.094748	160072.240792	56.301274
2747.444344	159837.470562	56.306279
2746.580019	159623.560642	56.311284
2746.037446	159398.451289	56.316289
2745.485632	159177.908956	56.321293
2744.701176	158958.777899	56.326298
2744.315241	158730.406087	56.331303
2743.288763	158511.811970	56.336308
2742.917460	158285.818100	56.341313
2742.304581	158067.224804	56.346317
2741.546421	157851.071353	56.351322
2740.930599	157613.043259	56.356327
2740.221925	157391.761530	56.361332
2739.517142	157182.837352	56.366337
2738.632892	156964.611788	56.371341
2738.285852	156732.712781	56.376346
2737.615445	156505.697292	56.381351
2736.738448	156291.606383	56.386356
2736.132763	156068.460801	56.391361
2735.375698	155841.908350	56.396365
2734.720985	155620.082810	56.401370
2734.281517	155399.279711	56.406375
2733.488094	155181.279897	56.411380
2732.949748	154954.279185	56.416385
2732.363896	154735.092563	56.421389
2731.333689	154508.477830	56.426394
2730.806517	154289.729699	56.431399
2729.764945	154080.356624	56.436404
2729.588866	153857.475259	56.441409
2729.321104	153642.656205	56.446413
2728.226542	153418.601262	56.451418
2727.723069	153188.505320	56.456423
2726.805647	152971.619855	56.461428
2726.578526	152745.563454	56.466433
2726.014150	152509.622031	56.471437
2725.104638	152291.468633	56.476442
2724.149068	152064.477246	56.481447
2723.403914	151853.978006	56.486452
2723.052076	151623.779865	56.491457
2722.072262	151399.580500	56.496461
2721.412456	151181.827005	56.501466
2721.143209	150955.458994	56.506471
2720.296064	150742.262976	56.511476
2719.516156	150517.783738	56.516481
2719.426876	150302.449592	56.521485
2718.466345	150072.358728	56.526490
2717.633968	149848.769381	56.531495
2717.051455	149633.466941	56.536500
2716.229016	149400.499222	56.541505
2715.886840	149183.382317	56.546509
2714.935481	148961.457469	56.551514
2714.511826	148731.303747	56.556519
2713.643440	148515.774403	56.561524
2713.230796	148302.284049	56.566529
2712.601524	148073.578327	56.571533
2711.950460	147848.334576	56.576538
2711.203378	147616.359101	56.581543
2710.150584	147399.112607	56.586548
2709.960323	147164.459561	56.591553
2709.267417	146952.318898	56.596557
2708.242146	146724.219322	56.601562
2707.558887	146501.252316	56.606567
2706.962247	146286.686203	56.611572
2706.421047	146055.426568	56.616577
2705.520591	145852.107672	56.621581
2704.768802	145622.930609	56.626586
2704.481091	145401.980129	56.631591
2703.201073	145192.612985	56.636596
2702.808100	144963.854072	56.641601
2702.301528	144751.863854	56.646605
2701.577668	144540.786336	56.651610
2701.013516	144322.962543	56.656615
2700.051795	144102.471110	56.661620
2699.675851	143881.265763	56.666625
2698.861352	143669.179190	56.671629
2698.272299	143454.516870	56.676634
2697.699368	143226.752256	56.681639
2696.812647	143015.939616	56.686644
2696.532369	142798.234025	56.691649
2695.841731	142580.277307	56.696653
2695.012098	142355.317215	56.701658
2694.477859	142134.365453	56.706663
2693.446854	141922.083751	56.711668
2693.077343	141706.267918	56.716673
2692.296234	141492.094433	56.721677
2691.509091	141266.944999	56.726682
2691.215255	141044.654248	56.731687
2690.217749	140843.924847	56.736692
2689.773198	140614.787002	56.741697
2689.171249	140395.218119	56.746701
2687.922277	140186.871116	56.751706
2688.020995	139969.151041	56.756711
2686.753807	139766.413146	56.761716
2686.484413	139531.639762	56.766721
2685.741519	139328.186462	56.771725
2684.675577	139106.705677	56.776730
2684.593123	138875.465361	56.781735
2683.577794	138674.791334	56.786740
2682.849419	138452.512284	56.791745
2682.271110	138239.320748	56.796749
2681.719001	138030.459032	56.801754
2681.237433	137815.336729	56.806759
2680.622905	137605.471483	56.811764
2679.967815	137379.720384	56.816769
2679.141166	137155.459233	56.821773
2677.932612	136944.523951	56.826778
2677.908124	136729.235475	56.831783
2676.837583	136517.353948	56.836788
2676.151024	136296.558155	56.841793
2675.850208	136084.926214	56.846797
2675.107913	135872.501861	56.851802
2674.536244	135661.894110	56.856807
2673.533705	135448.269067	56.861812
2673.188410	135229.841004	56.866817
2672.424741	135013.361029	56.871821
2671.593296	134800.856965	56.876826
2671.130302	134580.305491	56.881831
2670.574778	134368.535794	56.886836
2669.697727	134150.327127	56.891841
2669.222606	133941.876112	56.896845
2668.420624	133731.928592	56.901850
2667.816832	133509.057487	56.906855
2667.031254	133297.535340	56.911860
2666.497648	133071.455329	56.916865
2665.593486	132863.562809	56.921869
2664.927099	132652.560049	56.926874
2664.558260	132447.850342	56.931879
2663.877239	132227.592774	56.936884
2663.474865	132013.339144	56.941889
2662.582885	131793.944013	56.946893
2661.804159	131577.759015	56.951898
2661.564705	131370.686616	56.956903
2660.706502	131151.697564	56.961908
2659.887844	130929.388714	56.966913
2659.081051	130713.633921	56.971917
2658.674921	130505.730527	56.976922
2657.830809	130282.401956	56.981927
2657.527081	130075.908100	56.986932
2656.780523	129856.936811	56.991937
2656.183963	129633.904408	56.996941
2655.269995	129414.594757	57.001946
2654.429991	129186.968503	57.006951
2653.549340	128983.215965	57.011956
2653.253195	128757.081981	57.016961
2652.461951	128555.566486	57.021965
2651.670045	128341.859744	57.026970
2651.123356	128128.814334	57.031975
2650.473936	127920.536879	57.036980
2649.623135	127704.926581	57.041985
2648.878034	127500.807826	57.046989
2648.520628	127286.418060	57.051994
2648.335342	127069.005426	57.056999
2647.421591	126861.412857	57.062004
2646.723896	126633.899325	57.067009
2646.103981	126421.196202	57.072013
2645.194316	126211.842605	57.077018
2644.916227	125989.830470	57.082023
2644.206997	125779.191149	57.087028
2643.695306	125557.816424	57.092033
2643.024196	125345.383776	57.097037
2642.014299	125126.999673	57.102042
2641.334936	124901.313678	57.107047
2640.582172	124698.207582	57.112052
2640.231277	124475.889153	57.117057
2639.637105	124263.846453	57.122061
2638.667119	124046.645740	57.127066
2638.082677	123829.931731	57.132071
2637.484012	123605.856505	57.137076
2637.074354	123398.413681	57.142081
2635.845646	123182.873653	57.147085
2635.280542	122980.258705	57.152090
2634.671009	122762.617606	57.157095
2634.004403	122548.479310	57.162100
2633.288267	122326.414306	57.167105
2632.901102	122113.835171	57.172109
2631.967213	121906.779039	57.177114
2631.226034	121692.507065	57.182119
2630.588246	121485.026368	57.187124
2629.993204	121263.700212	57.192129
2629.319441	121056.050809	57.197133
2628.508366	120840.222323	57.202138
2628.055393	120628.694003	57.207143
2627.054373	120416.555883	57.212148
2626.366995	120211.962591	57.217153
2625.809515	120005.420375	57.222157
2625.027357	119791.703592	57.227162
2624.236605	119588.502796	57.232167
2623.887035	119383.760857	57.237172
2623.252364	119174.139449	57.242177
2622.589136	118966.308095	57.247181
2621.883756	118761.379837	57.252186
2621.433229	118547.449278	57.257191
2620.660778	118340.446436	57.262196
2619.944070	118122.530539	57.267201
2619.424483	117919.598142	57.272205
2618.321534	117712.424160	57.277210
2618.070951	117494.128636	57.282215
2617.237017	117294.209057	57.287220
2616.759395	117082.396010	57.292225
2616.065870	116871.507595	57.297229
2615.026927	116666.083840	57.302234
2614.693469	116457.096841	57.307239
2613.707015	116252.613869	57.312244
2613.142263	116042.740157	57.317249
2612.776830	115830.672103	57.322253
2612.153797	115627.406024	57.327258
2611.391872	115412.725673	57.332263
2610.875166	115213.038639	57.337268
2610.100382	114990.829656	57.342273
2609.381388	114787.801289	57.347277
2608.410913	114578.035667	57.352282
2607.986894	114374.944819	57.357287
2607.198666	114166.226382	57.362292
2606.331586	113970.146292	57.367297
2605.791460	113761.988492	57.372301
2605.042319	113561.316759	57.377306
2604.892112	113351.259966	57.382311
2603.851646	113142.647094	57.387316
2603.352141	112932.668192	57.392321
2602.682957	112728.398197	57.397325
2601.898937	112530.329663	57.402330
2601.709930	112311.827685	57.407335
2600.910152	112110.623428	57.412340
2600.041866	111901.365308	57.417345
2599.589470	111692.309587	57.422349
2598.774829	111483.484378	57.427354
2598.288060	111267.444001	57.432359
2597.200019	111069.422564	57.437364
2596.582579	110855.938627	57.442369
2596.079445	110647.743781	57.447373
2595.358043	110447.251340	57.452378
2594.871329	110238.695609	57.457383
2593.981705	110035.447266	57.462388
2593.572575	109828.748423	57.467393
2593.117006	109623.289772	57.472397
2592.373500	109413.588700	57.477402
2591.654677	109187.862470	57.482407
2590.706200	108989.619868	57.487412
2590.232015	108779.710202	57.492417
2589.291609	108576.171055	57.497421
2588.574858	108369.330205	57.502426
2588.069668	108159.913040	57.507431
2587.391281	107960.309785	57.512436
2586.474768	107763.963015	57.517441
2586.085754	107550.084572	57.522445
2585.456617	107350.028006	57.527450
2584.750895	107138.455957	57.532455
2584.189232	106937.345143	57.537460
2583.579542	106734.232211	57.542465
2582.724750	106519.821208	57.547469
2581.861236	106328.058820	57.552474
2581.732320	106116.613694	57.557479
2580.672410	105914.543454	57.562484
2580.197313	105702.319307	57.567489
2579.540116	105500.848589	57.572493
2578.792444	105298.232817	57.577498
2578.214007	105089.913447	57.582503
2577.533570	104880.317753	57.587508
2576.872760	104674.292782	57.592513
2576.202657	104466.646866	57.597517
2575.385014	104269.551607	57.602522
2574.964722	104062.294706	57.607527
2574.076261	103855.018644	57.612532
2573.380850	103660.611758	57.617537
2572.786973	103454.999121	57.622541
2572.117884	103253.397031	57.627546
2571.615008	103049.397608	57.632551
2570.947850	102842.996200	57.637556
2570.249603	102634.698317	57.642561
2569.546556	102433.051517	57.647565
2568.557439	102230.703201	57.652570
2568.482507	102021.696594	57.657575
2567.723584	101821.795767	57.662580
2567.164264	101616.650445	57.667585
2566.489887	101392.957164	57.672589
2565.541133	101197.348370	57.677594
2564.937942	100990.838919	57.682599
2564.041443	100793.981881	57.687604
2563.356867	100583.257804	57.692609
2562.693713	100386.576561	57.697613
2562.083609	100178.629106	57.702618
2561.815108	99970.787954	57.707623
2560.838846	99776.711508	57.712628
2560.428441	99570.279263	57.717633
2559.649670	99360.329713	57.722637
2558.981584	99157.963537	57.727642
2558.280993	98959.619422	57.732647
2557.761620	98759.364429	57.737652
2556.779571	98545.211066	57.742657
2556.385393	98346.887091	57.747661
2555.233611	98145.545216	57.752666
2555.020352	97943.872417	57.757671
2554.550464	97739.654248	57.762676
2553.589026	97531.380410	57.767681
2552.997987	97317.246308	57.772685
2552.361720	97120.759919	57.777690
2551.725579	96920.317504	57.782695
2550.614899	96725.875873	57.787700
2550.125325	96530.785676	57.792705
2549.772851	96322.083878	57.797709
2548.914630	96112.646006	57.802714
2548.318638	95911.711423	57.807719
2547.554486	95707.386868	57.812724
2546.932356	95520.311104	57.817729
2546.033940	95307.107178	57.822733
2545.205427	95104.212545	57.827738
2544.996266	94913.334600	57.832743
2543.961381	94712.194861	57.837748
2543.472803	94511.877206	57.842753
2542.654718	94325.876122	57.847757
2541.880265	94135.963187	57.852762
2541.625411	93934.554574	57.857767
2540.892108	93735.069001	57.862772
2540.065984	93534.268201	57.867777
2539.388878	93338.220701	57.872781
2538.770622	93147.232374	57.877786
2538.310624	92940.709666	57.882791
2537.763969	92744.259886	57.887796
2536.914564	92540.453269	57.892801
2536.402272	92344.711788	57.897805
2535.631252	92148.410635	57.902810
2535.084860	91946.558892	57.907815
2534.129220	91742.319885	57.912820
2533.484921	91537.450049	57.917825
2532.942801	91359.920508	57.922829
2532.103551	91165.281179	57.927834
2531.659455	90954.811419	57.932839
2530.905996	90762.730060	57.937844
2530.131022	90565.568574	57.942849
2529.767512	90364.913369	57.947853
2528.755917	90185.857190	57.952858
2528.123732	89983.409297	57.957863
2527.422899	89787.625274	57.962868
2526.987658	89580.102901	57.967873
2526.701920	89394.153936	57.972877
2525.598529	89189.670406	57.977882
2525.125447	88997.414248	57.982887
2524.588340	88787.861321	57.987892
2523.782433	88598.698368	57.992897
2523.146869	88388.854223	57.997901
2522.683276	88199.196684	58.002906
2522.100717	87996.981257	58.007911
2521.195148	87801.209495	58.012916
2520.245444	87595.068242	58.017921
2519.904474	87392.978654	58.022925
2518.915673	87193.966955	58.027930
2518.355478	86986.787113	58.032935
2517.421507	86805.204278	58.037940
2516.449168	86607.659822	58.042945
2516.448616	86417.348606	58.047949
2515.603454	86219.927020	58.052954
2515.022194	86013.292398	58.057959
2514.298494	85824.654196	58.062964
2513.553455	85631.932238	58.067969
2513.328146	85434.876051	58.072973
2512.457901	85239.071288	58.077978
2511.971988	85037.464222	58.082983
2511.435910	84837.134809	58.087988
2510.455710	84645.302115	58.092993
2509.553233	84447.500290	58.097997
2508.978226	84249.654735	58.103002
2508.124825	84047.849060	58.108007
2507.524263	83851.684694	58.113012
2507.070513	83659.156264	58.118017
2506.239265	83460.230412	58.123021
2505.460308	83285.701447	58.128026
2504.887621	83083.118859	58.133031
2504.374838	82889.624329	58.138036
2503.687822	82697.636028	58.143041
2503.299345	82509.221316	58.148045
2502.351658	82310.305747	58.153050
2502.034040	82110.614000	58.158055
2501.405899	81923.009448	58.163060
2500.610006	81720.817610	58.168065
2499.863999	81519.031784	58.173069
2498.850926	81335.714611	58.178074
2498.577314	81132.159064	58.183079
2497.929331	80938.228606	58.188084
2496.949329	80742.508295	58.193089
2496.099842	80547.472616	58.198093
2495.762040	80357.047503	58.203098
2495.242857	80163.274954	58.208103
2494.704409	79977.974196	58.213108
2493.794549	79782.765132	58.218113
2493.233907	79568.940295	58.223117
2492.277867	79382.183741	58.228122
2492.118403	79184.034908	58.233127
2491.506635	78996.200623	58.238132
2490.649417	78797.874586	58.243137
2490.220014	78600.597968	58.248141
2489.241458	78410.951370	58.253146
2488.519340	78198.205588	58.258151
2487.898241	78006.332470	58.263156
2487.291423	77822.335598	58.268161
2486.775437	77613.739180	58.273165
2485.965540	77422.883646	58.278170
2485.227047	77221.797505	58.283175
2484.591788	77032.571796	58.288180
2483.965253	76831.389368	58.293185
2483.378278	76626.153629	58.298189
2482.451244	76444.551731	58.303194
2482.233304	76248.392097	58.308199
2481.355360	76052.700150	58.313204
2480.408463	75856.013551	58.318209
2479.996256	75657.235520	58.323213
2479.207450	75467.776223	58.328218
2478.330335	75268.980652	58.333223
2478.029539	75069.043892	58.338228
2477.382590	74886.296384	58.343233
2476.911357	74695.355706	58.348237
2475.929846	74497.179840	58.353242
2475.301905	74293.811563	58.358247
2474.635409	74107.431137	58.363252
2474.171789	73909.369018	58.368257
2473.804601	73705.205066	58.373261
2472.781386	73519.406153	58.378266
2472.291282	73325.072938	58.383271
2471.499174	73122.496445	58.388276
2470.697055	72929.445594	58.393281
2470.040130	72734.884797	58.398285
2469.371472	72541.784851	58.403290
2468.508595	72337.231933	58.408295
2468.081958	72142.190601	58.413300
2467.435539	71954.965430	58.418305
2467.004116	71746.466798	58.423309
2466.097510	71557.348114	58.428314
2465.445873	71353.563667	58.433319
2464.855833	71168.199402	58.438324
2464.446993	70972.583909	58.443329
2463.447908	70777.348978	58.448333
2462.651955	70586.974073	58.453338
2462.256225	70385.319099	58.458343
2461.356010	70187.204777	58.463348
2460.429633	69989.191607	58.468353
2460.348566	69797.292068	58.473357
2459.412161	69603.813408	58.478362
2458.716376	69418.019910	58.483367
2458.080885	69221.228850	58.488372
2457.170723	69023.799224	58.493377
2456.584469	68832.141202	58.498381
2455.790354	68642.823570	58.503386
2455.356104	68448.731955	58.508391
2454.202717	68273.985824	58.513396
2453.721050	68080.817448	58.518401
2453.409928	67891.006151	58.523405
2452.571931	67694.769225	58.528410
2451.575016	67508.332208	58.533415
2450.950397	67319.614881	58.538420
2450.705259	67138.433058	58.543425
2449.937502	66956.949439	58.548429
2449.070010	66769.035968	58.553434
2448.885891	66568.849712	58.558439
2448.180920	66383.897184	58.563444
2447.256657	66195.402946	58.568449
2446.639185	66012.213382	58.573453
2445.901421	65824.244172	58.578458
2445.348868	65629.325471	58.583463
2444.555084	65450.928419	58.588468
2444.083611	65248.033892	58.593473
2443.463777	65064.058922	58.598477
2442.516774	64885.599570	58.603482
2442.319086	64686.540022	58.608487
2441.738780	64499.806299	58.613492
2440.965462	64313.035335	58.618497
2440.134434	64112.033571	58.623501
2439.611949	63925.581232	58.628506
2438.875425	63729.529954	58.633511
2438.316473	63543.109284	58.638516
2437.561157	63342.907795	58.643521
2436.918793	63154.215043	58.648525
2436.148058	62957.933318	58.653530
2435.479749	62774.045010	58.658535
2434.976460	62578.000240	58.663540
2434.034552	62391.930146	58.668545
2433.485989	62198.593861	58.673549
2432.661308	62013.794252	58.678554
2432.167090	61818.461874	58.683559
2431.481527	61645.063070	58.688564
2430.668927	61449.512712	58.693569
2430.328869	61254.712555	58.698573
2429.461896	61075.035196	58.703578
2429.025785	60880.174983	58.708583
2428.471376	60688.206804	58.713588
2427.590114	60499.448546	58.718593
2427.284975	60304.475380	58.723597
2426.451283	60109.553215	58.728602
2425.892331	59906.916235	58.733607
2425.135016	59723.055873	58.738612
2424.880171	59524.062628	58.743617
2424.074194	59319.809276	58.748621
2422.821741	59134.988592	58.753626
2422.382256	58939.639398	58.758631
2421.549759	58752.375546	58.763636
2421.155030	58559.508026	58.768641
2420.358790	58364.389173	58.773645
2419.561727	58177.429340	58.778650
2419.021347	57978.089504	58.783655
2418.251662	57790.451860	58.788660
2417.367941	57603.033594	58.793665
2417.127387	57411.289808	58.798669
2416.207001	57233.629655	58.803674
2415.405728	57035.525041	58.808679
2414.644519	56856.418991	58.813684
2414.179682	56668.788666	58.818689
2413.816893	56474.636905	58.823693
2413.010397	56286.982337	58.828698
2412.083543	56095.955993	58.833703
2411.103181	55922.008219	58.838708
2410.740930	55742.118633	58.843713
2410.423290	55553.624963	58.848717
2409.390460	55374.484584	58.853722
2408.861158	55184.167374	58.858727
2408.299145	54999.493664	58.863732
2407.550063	54808.363891	58.868737
2406.848405	54624.450302	58.873741
2406.130308	54446.626711	58.878746
2405.726401	54246.428932	58.883751
2405.017029	54069.829146	58.888756
2403.804263	53881.662311	58.893761
2403.983252	53693.064718	58.898765
2403.123014	53512.279160	58.903770
2402.482062	53309.844502	58.908775
2401.671554	53132.159122	58.913780
2401.112978	52943.591301	58.918785
2400.629301	52760.759960	58.923789
2399.806411	52572.367638	58.928794
2399.432796	52375.881491	58.933799
2398.574764	52183.651050	58.938804
2397.802626	51998.696147	58.943809
2397.402386	51807.425472	58.948813
2396.291294	51617.168144	58.953818
2396.038826	51425.374985	58.958823
2395.141293	51233.429858	58.963828
2394.739305	51045.451814	58.968833
2394.103814	50853.643202	58.973837
2393.017329	50672.580156	58.978842
2392.698064	50467.193298	58.983847
2392.177158	50288.755913	58.988852
2391.092653	50095.938207	58.993857
2390.726517	49896.956283	58.998861
2389.868663	49706.441723	59.003866
2389.326593	49523.076648	59.008871
2388.657086	49334.548326	59.013876
2387.783878	49141.599827	59.018881
2387.105295	48951.779873	59.023885
2386.488040	48766.915927	59.028890
2385.825311	48577.556166	59.033895
2385.137618	48397.794260	59.038900
2384.406152	48205.940654	59.043905
2384.192539	48019.321653	59.048909
2383.132391	47831.747456	59.053914
2382.653542	47642.359002	59.058919
2381.661648	47445.496604	59.063924
2381.092361	47266.420152	59.068929
2380.779189	47080.725199	59.073933
2379.886453	46900.520658	59.078938
2379.092066	46703.682641	59.083943
2378.684315	46515.756385	59.088948
2377.812256	46327.459746	59.093953
2377.206518	46141.539532	59.098957
2376.331109	45961.474686	59.103962
2375.964302	45781.789678	59.108967
2375.065509	45588.864934	59.113972
2374.518232	45400.333764	59.118977
2374.098567	45212.296786	59.123981
2373.120084	45037.258429	59.128986
2372.697778	44844.449758	59.133991
2371.859258	44654.337563	59.138996
2371.017951	44470.967903	59.144001
2370.598231	44284.291428	59.149005
2369.840319	44101.921353	59.154010
2369.163308	43915.539478	59.159015
2368.644463	43741.061109	59.164020
2367.841611	43550.272130	59.169025
2367.393744	43355.453503	59.174029
2366.339835	43173.722006	59.179034
2365.944670	42987.507775	59.184039
2365.221677	42815.632745	59.189044
2364.300921	42636.045779	59.194049
2363.838448	42440.800134	59.199053
2362.936481	42252.207427	59.204058
2362.456684	42073.182532	59.209063
2361.677113	41900.506487	59.214068
2361.288738	41710.933794	59.219073
2360.960413	41533.247114	59.224077
2359.634421	41350.499548	59.229082
2359.006879	41165.157635	59.234087
2358.808424	40975.746311	59.239092
2358.107250	40800.991266	59.244097
2357.406966	40609.842132	59.249101
2356.506695	40435.694721	59.254106
2355.760832	40240.860412	59.259111
2355.161238	40061.505446	59.264116
2354.585783	39886.350839	59.269121
2353.996222	39693.686071	59.274125
2352.877524	39526.260629	59.279130
2352.686726	39337.188683	59.284135
2351.744712	39155.470745	59.289140
2351.204651	38976.892363	59.294145
2350.617353	38789.609395	59.299149
2349.558157	38612.987359	59.304154
2349.261442	38433.881253	59.309159
2348.325864	38256.881288	59.314164
2347.848597	38075.384137	59.319169
2347.391466	37890.977019	59.324173
2346.464334	37715.000986	59.329178
2345.917380	37531.228534	59.334183
2345.166960	37354.701813	59.339188
2344.413320	37179.924175	59.344193
2344.204113	36996.824778	59.349197
2343.146047	36814.819895	59.354202
2342.604255	36636.422880	59.359207
2341.938509	36455.186362	59.364212
2341.302751	36267.401483	59.369217
2340.860876	36084.383644	59.374221
2340.124755	35907.566286	59.379226
2339.480442	35730.880062	59.384231
2338.688420	35542.195482	59.389236
2337.652087	35356.814090	59.394241
2337.378841	35172.311064	59.399245
2336.732154	35005.517705	59.404250
2336.356054	34823.838716	59.409255
2335.549816	34645.441521	59.414260
2334.518222	34457.940358	59.419265
2334.148977	34268.397003	59.424269
2333.100053	34104.665098	59.429274
2332.845997	33915.565810	59.434279
2332.466549	33735.220425	59.439284
2331.326759	33558.683097	59.444289
2330.676646	33370.171176	59.449293
2329.969665	33192.575019	59.454298
2329.371053	33005.056283	59.459303
2328.609648	32836.565960	59.464308
2327.936359	32653.720307	59.469313
2327.139962	32483.078811	59.474317
2326.522065	32307.873733	59.479322
2326.297072	32125.561735	59.484327
2325.378555	31940.559928	59.489332
2324.829494	31768.928921	59.494337
2324.367379	31590.979219	59.499341
2323.774171	31396.576965	59.504346
2323.171783	31207.309330	59.509351
2322.224527	31035.791754	59.514356
2321.539280	30844.161685	59.519361
2321.139783	30668.553785	59.524365
2320.477726	30484.437782	59.529370
2319.544798	30300.651217	59.534375
2318.866455	30115.518021	59.539380
2317.988943	29939.962109	59.544385
2317.606683	29761.458575	59.549389
2316.793727	29588.430588	59.554394
2316.174437	29390.973516	59.559399
2315.645849	29224.763118	59.564404
2314.786502	29046.805974	59.569409
2314.361037	28852.896991	59.574413
2313.630850	28686.172633	59.579418
2312.791452	28504.345783	59.584423
2312.313159	28329.047183	59.589428
2311.496196	28138.324369	59.594433
2310.851549	27959.896334	59.599437
2310.289028	27794.980836	59.604442
2309.534797	27603.908344	59.609447
2308.727383	27428.843838	59.614452
2308.304324	27252.021966	59.619457
2307.620912	27069.660331	59.624461
2306.791827	26887.325431	59.629466
2306.232601	26708.671685	59.634471
2305.456821	26522.078161	59.639476
2304.632736	26356.017383	59.644481
2304.051022	26175.716750	59.649485
2303.277464	26008.977781	59.654490
2302.813257	25826.823649	59.659495
2302.197589	25654.099263	59.664500
2301.233663	25477.384938	59.669505
2301.041467	25298.776240	59.674509
2300.077386	25135.479810	59.679514
2299.470078	24957.007087	59.684519
2298.997258	24771.004177	59.689524
2298.258087	24597.356663	59.694529
2297.595268	24420.878664	59.699533
2296.955694	24252.446545	59.704538
2296.224061	24072.413593	59.709543
2295.533240	23898.887596	59.714548
2294.658019	23725.780487	59.719553
2294.538513	23546.771458	59.724557
2293.603786	23370.427926	59.729562
2292.854963	23180.113827	59.734567
2292.511556	23010.599084	59.739572
2291.804899	22839.787862	59.744577
2290.781884	22659.330602	59.749581
2289.783401	22487.480480	59.754586
2289.310166	22308.442741	59.759591
2288.688662	22135.273963	59.764596
2288.005473	21970.316522	59.769601
2287.669197	21791.277098	59.774605
2286.920040	21637.262933	59.779610
2286.153726	21449.698895	59.784615
2285.535091	21278.479895	59.789620
2285.026418	21102.391624	59.794625
2284.271684	20922.376639	59.799629
2283.647122	20757.646768	59.804634
2282.798221	20571.758048	59.809639
2282.262010	20404.816509	59.814644
2281.285371	20233.206088	59.819649
2281.142163	20060.057575	59.824653
2280.398871	19883.435054	59.829658
2279.407919	19706.580620	59.834663
2278.858388	19534.146200	59.839668
2278.336281	19371.566015	59.844673
2277.587269	19191.101319	59.849677
2276.994644	19021.292232	59.854682
2276.220135	18843.116835	59.859687
2275.319434	18665.594273	59.864692
2275.189314	18508.362868	59.869697
2274.484942	18338.647585	59.874701
2273.313185	18161.273999	59.879706
2272.523543	17987.888512	59.884711
2272.044354	17816.740729	59.889716
2271.577809	17642.736271	59.894721
2270.834637	17470.416071	59.899725
2269.796069	17318.825218	59.904730
2269.114066	17142.845938	59.909735
2268.773227	16980.225147	59.914740
2267.891873	16813.593695	59.919745
2267.346675	16649.729574	59.924750
2266.421765	16489.564824	59.929754
2266.004274	16317.115158	59.934759
2265.274639	16157.559676	59.939764
2264.339942	16000.340486	59.944769
2264.233009	15828.690600	59.949774
2263.191252	15670.738711	59.954778
2262.856418	15495.916100	59.959783
2262.339231	15328.509566	59.964788
2261.250992	15158.904677	59.969793
2260.859232	14988.240077	59.974798
2259.908395	14834.848568	59.979802
2259.336595	14656.823554	59.984807
2258.386515	14501.676538	59.989812
2257.604961	14343.147730	59.994817
2257.592044	14174.470305	59.999822
2256.673734	14018.840885	60.004826
2255.902446	13853.547737	60.009831
2255.455096	13692.562990	60.014836
2254.451395	13536.607529	60.019841
2254.049283	13364.746481	60.024846
2252.781017	13204.808806	60.029850
2252.414508	13047.951934	60.034855
2251.900289	12893.672916	60.039860
2251.220174	12740.699619	60.044865
2250.608798	12573.826710	60.049870
2249.673072	12414.588239	60.054874
2249.070516	12256.299028	60.059879
2248.857125	12104.983466	60.064884
2247.565411	11947.443124	60.069889
2247.002876	11780.548844	60.074894
2246.513959	11635.601178	60.079898
2246.163560	11473.171048	60.084903
2245.538340	11312.276861	60.089908
2244.096263	11165.785733	60.094913
2244.002639	10992.824436	60.099918
2242.984569	10845.630962	60.104922
2242.411954	10684.645516	60.109927
2241.863366	10539.900827	60.114932
2241.157070	10385.954531	60.119937
2240.262023	10224.728431	60.124942
2239.286015	10078.397377	60.129946
2238.803582	9933.077122	60.134951
2238.219505	9782.599374	60.139956
2237.139340	9631.181820	60.144961
2236.860157	9474.320809	60.149966
2236.179562	9342.263812	60.154970
2235.264862	9186.436050	60.159975
2234.811476	9047.261228	60.164980
2234.371762	8894.896574	60.169985
2233.743462	8741.903797	60.174990
2232.754079	8605.894668	60.179994
2231.918196	8456.634800	60.184999
2231.605654	8318.384017	60.190004
2230.407780	8183.739580	60.195009
2230.316901	8033.596907	60.200014
2229.162448	7892.083700	60.205018
2228.240786	7754.405331	60.210023
2227.829948	7617.229012	60.215028
2226.951493	7481.145815	60.220033
2226.439422	7346.352772	60.225038
2225.548034	7212.336640	60.230042
2224.708352	7070.165145	60.235047
2224.252751	6935.667407	60.240052
2223.296397	6800.483539	60.245057
2222.628842	6658.189259	60.250062
2222.133687	6544.161995	60.255066
2220.940063	6409.485917	60.260071
2219.992459	6284.266900	60.265076
2219.612726	6163.290334	60.270081
2218.994608	6038.225422	60.275086
2217.864903	5928.297368	60.280090
2217.229838	5812.635061	60.285095
2216.744894	5699.459829	60.290100
2215.669129	5601.188975	60.295105
2215.178794	5482.409432	60.300110
2214.622687	5376.200415	60.305114
2213.532389	5274.914532	60.310119
2212.720480	5181.635481	60.315124
2211.607158	5080.800239	60.320129
2210.883554	4981.552389	60.325134
2209.498979	4903.295809	60.330138
2208.397652	4819.411847	60.335143
2207.523553	4753.373468	60.340148
2206.192671	4699.066451	60.345153
2205.731953	4632.576540	60.350158
2204.856513	4583.005932	60.355162
2204.137850	4535.218428	60.360167
2203.466565	4471.407319	60.365172
2202.924683	4415.143135	60.370177
2202.260911	4367.524143	60.375182
2201.424678	4328.119747	60.380186
2201.051551	4277.415936	60.385191
2200.832757	4219.030816	60.390196
2199.960083	4175.966589	60.395201
2199.504830	4110.001090	60.400206
2198.801659	4054.446905	60.405210
2198.348079	4007.252400	60.410215
2197.623169	3944.551552	60.415220
2196.714470	3897.841312	60.420225
2196.140866	3825.784121	60.425230
2195.535243	3785.958912	60.430234
2194.905798	3730.861165	60.435239
2194.589355	3671.980255	60.440244
2193.242484	3620.791972	60.445249
2192.732039	3563.315399	60.450254
2192.262159	3530.827876	60.455258
2191.386813	3471.223296	60.460263
2190.844760	3420.303950	60.465268
2190.161805	3369.893753	60.470273
2189.921908	3308.434193	60.475278
2188.626109	3278.280263	60.480282
2188.388875	3222.186034	60.485287
2188.063528	3168.050868	60.490292
2186.929099	3115.170488	60.495297
2186.761238	3069.857229	60.500302
2185.920080	3023.652479	60.505306
2185.229280	2956.977916	60.510311
2184.501615	2907.329575	60.515316
2183.984877	2865.704078	60.520321
2183.493065	2798.214739	60.525326
2182.725428	2756.527622	60.530330
2181.865777	2706.434808	60.535335
2181.396345	2655.788139	60.540340
2180.596227	2600.694108	60.545345
2180.091078	2542.157597	60.550350
2179.465150	2498.129340	60.555354
2178.653095	2455.502974	60.560359
2178.191494	2399.270040	60.565364
2177.086305	2362.343376	60.570369
2176.574829	2303.391637	60.575374
2176.150348	2268.597703	60.580378
2175.540879	2209.680816	60.585383
2175.146240	2166.630242	60.590388
2174.322455	2109.870726	60.595393
2173.651931	2051.401846	60.600398
2172.467071	2013.733214	60.605402
2171.953372	1951.914272	60.610407
2171.514569	1909.402984	60.615412
2170.690137	1860.548748	60.620417
2170.336528	1809.844044	60.625422
2169.387657	1767.908549	60.630426
2168.955207	1718.290744	60.635431
2168.026089	1669.614631	60.640436
2167.629708	1622.973889	60.645441
2166.936457	1566.421313	60.650446
2165.991895	1525.509420	60.655450
2165.612054	1475.738992	60.660455
2164.610507	1430.365140	60.665460
2164.000606	1388.467643	60.670465
2163.468178	1344.429607	60.675470
2162.580970	1308.092432	60.680474
2162.179966	1264.724576	60.685479
2161.544693	1207.423724	60.690484
2160.793338	1176.327445	60.695489
2160.411026	1119.676799	60.700494
2159.650351	1082.042639	60.705498
2159.111658	1038.129538	60.710503
2158.754802	981.121327	60.715508
2157.531190	940.986348	60.720513
2157.348301	894.705183	60.725518
2156.478690	848.048167	60.730522
2155.180456	807.028030	60.735527
2155.115667	749.651868	60.740532
2153.993696	716.512331	60.745537
2153.251760	669.954700	60.750542
2152.449226	647.581833	60.755546
2152.149557	597.891575	60.760551
2151.370068	558.774578	60.765556
2150.676359	522.455981	60.770561
2150.095488	484.263372	60.775566
2149.416194	444.902111	60.780570
2148.772594	400.936613	60.785575
2148.041614	357.860373	60.790580
2147.240484	335.911991	60.795585
2146.811841	279.383148	60.800590
2145.592092	256.099324	60.805594
2145.271376	223.920360	60.810599
2144.530827	182.219755	60.815604
2143.372003	164.969580	60.820609
2143.155090	131.448073	60.825614
2142.348498	105.919493	60.830618
2141.591939	74.724688	60.835623
2140.933282	45.487257	60.840628
2140.166394	29.327853	60.845633
2139.458446	0.894725	60.850638
2138.429422	-16.962471	60.855642
2137.673185	-32.957909	60.860647
2136.917222	-54.998019	60.865652
2135.428706	-45.386579	60.870657
2134.139912	-49.069414	60.875662
2132.718865	-18.286357	60.880666
2131.836257	0.692582	60.885671
2131.858624	12.286324	60.890676
2131.485862	8.920187	60.895681
2131.679406	21.011918	60.900686
2130.888355	17.116041	60.905690
2130.481213	6.360768	60.910695
2130.355484	12.540487	60.915700
2129.352922	22.939065	60.920705
2128.502583	17.475588	60.925710
2127.423520	19.826213	60.930714
2126.128564	30.594481	60.935719
2125.961017	27.509602	60.940724
2125.106685	30.630422	60.945729
2124.874147	39.612102	60.950734
2124.680341	39.999235	60.955738
2123.890985	32.967990	60.960743
2123.026588	35.076391	60.965748
2122.483896	47.530981	60.970753
2122.587808	47.017710	60.975758
2121.281736	35.873605	60.980762
2120.425642	40.453443	60.985767
2119.952817	47.240208	60.990772
2118.660073	50.372252	60.995777
2118.548610	38.708990	61.000782
2118.167072	57.457101	61.005786
2117.499513	55.020862	61.010791
2116.732704	45.189992	61.015796
2115.650467	54.358553	61.020801
2115.335017	61.262284	61.025806
2115.008479	56.794357	61.030810
2114.543429	55.582862	61.035815
2113.808559	44.340231	61.040820
2112.960707	57.784730	61.045825
2112.332524	50.817795	61.050830
2111.356693	52.828762	61.055834
2110.140466	54.086217	61.060839
2109.835793	55.322030	61.065844
2109.462893	60.388196	61.070849
2108.964098	50.230934	61.075854
2108.449952	48.309692	61.080858
2107.701951	63.269630	61.085863
2106.737669	48.453619	61.090868
2105.975837	55.584306	61.095873
2105.190742	46.005510	61.100878
2104.794670	57.400747	61.105882
2104.892463	49.236782	61.110887
2104.356046	49.151563	61.115892
2102.604452	62.204872	61.120897
2102.589271	48.044108	61.125902
2101.836026	57.220395	61.130906
2101.171743	55.565838	61.135911
2100.272501	51.201412	61.140916
2099.477287	60.130462	61.145921
2099.042928	55.687533	61.150926
2097.947412	57.001534	61.155930
2097.371933	57.920764	61.160935
2097.253164	59.231161	61.165940
2096.860512	66.729064	61.170945
2096.088223	59.731379	61.175950
2095.119735	63.925351	61.180954
2094.063497	60.860065	61.185959
2094.275664	63.436329	61.190964
2093.446938	65.599009	61.195969
2092.945729	59.181228	61.200974
2091.841979	59.894120	61.205978
2090.882815	67.530811	61.210983
2090.922637	61.427735	61.215988
2090.026362	66.433451	61.220993
2089.575858	56.449884	61.225998
2088.648362	64.327563	61.231002
2087.912201	60.246353	61.236007
2087.328191	59.752358	61.241012
2086.603851	60.931765	61.246017
2085.641232	65.091692	61.251022
2084.958230	66.873268	61.256026
2084.426109	70.405040	61.261031
2083.532949	72.628413	61.266036
2082.974572	72.133505	61.271041
2082.766836	64.916916	61.276046
2082.321113	70.256428	61.281050
2081.505878	63.972064	61.286055
2080.841558	72.528680	61.291060
2079.683472	71.203236	61.296065
2079.523783	66.934346	61.301070
2078.904012	69.973807	61.306074
2078.198952	71.422981	61.311079
2077.552480	59.844613	61.316084
2076.357795	66.441585	61.321089
2076.303612	68.191182	61.326094
2075.492296	61.027803	61.331098
2074.681020	58.191743	61.336103
2074.798219	53.144029	61.341108
2073.837169	59.424790	61.346113
2073.191031	58.636294	61.351118
2071.992563	65.385261	61.356122
2071.221638	71.542812	61.361127
2070.928030	64.272041	61.366132
2069.954814	70.247221	61.371137
2069.701441	63.358012	61.376142
2068.905230	70.916809	61.381146
2068.027744	73.945131	61.386151
2067.962318	60.186588	61.391156
2066.799390	70.107599	61.396161
2066.341834	59.025977	61.401166
2065.875784	63.318424	61.406170
2064.817868	73.754226	61.411175
2064.638026	64.995625	61.416180
2063.941714	74.572918	61.421185
2063.323188	66.437468	61.426190
2062.577533	66.920070	61.431194
2061.701924	62.780572	61.436199
2061.277994	60.856059	61.441204
2059.691154	64.134158	61.446209
2059.804914	60.523646	61.451214
2059.090312	57.793678	61.456218
2058.283589	65.093936	61.461223
2058.168487	57.141959	61.466228
2056.785094	57.001926	61.471233
2055.945980	60.203939	61.476238
2055.619773	62.318417	61.481242
2055.436437	72.014579	61.486247
2054.775702	69.684508	61.491252
2053.519017	65.987127	61.496257
2052.546952	67.262631	61.501262
2052.547198	65.411156	61.506266
2051.952615	59.246333	61.511271
2051.265932	59.331635	61.516276
2050.004489	66.644136	61.521281
2049.873027	60.960922	61.526286
2049.181750	69.898725	61.531290
2048.556672	71.158587	61.536295
2048.518424	68.805422	61.541300
2047.135811	66.370716	61.546305
2047.095767	71.745200	61.551310
2046.345527	66.784686	61.556314
2045.290896	73.080313	61.561319
2044.332258	65.984481	61.566324
2043.543243	74.737520	61.571329
2043.485150	70.539244	61.576334
2042.532408	62.665012	61.581338
2041.615737	68.981322	61.586343
2041.293930	60.724671	61.591348
2040.292387	67.988042	61.596353
2040.192617	63.110383	61.601358
2039.610251	62.291274	61.606362
2038.445467	69.730371	61.611367
2038.297882	64.712061	61.616372
2037.307900	73.263598	61.621377
2036.682437	62.670696	61.626382
2036.513596	65.455663	61.631386
2035.749807	69.216607	61.636391
2035.196403	65.216798	61.641396
2033.979624	71.393078	61.646401
2033.145007	63.597876	61.651406
2032.730390	68.337923	61.656410
2031.713184	70.639349	61.661415
2031.457439	69.946604	61.666420
2030.856857	75.506252	61.671425
2030.036832	61.271369	61.676430
2029.624738	63.454677	61.681434
2028.825697	69.996759	61.686439
2028.698797	73.073127	61.691444
2027.408010	73.203851	61.696449
2026.501142	65.435888	61.701454
2025.998771	68.012009	61.706458
2025.484047	69.910398	61.711463
2024.796350	64.211386	61.716468
2023.824639	70.244690	61.721473
2023.280599	70.895585	61.726478
2022.708726	56.157683	61.731482
2022.261047	66.611759	61.736487
2022.082422	59.844741	61.741492
2021.113912	74.196279	61.746497
2020.694322	67.751366	61.751502
2020.017328	65.266185	61.756506
2018.354019	75.586768	61.761511
2017.787768	65.498578	61.766516
2017.714885	66.833236	61.771521
2016.843317	64.484598	61.776526
2016.281535	57.019854	61.781530
2015.579087	63.100311	61.786535
2015.257693	58.683625	61.791540
2014.507240	71.811485	61.796545
2013.916584	63.687399	61.801550
2013.549785	64.254968	61.806554
2012.042311	68.187574	61.811559
2011.436772	66.985780	61.816564
2010.895797	72.447656	61.821569
2010.249527	69.777821	61.826574
2009.716579	63.084390	61.831578
2008.899832	66.587230	61.836583
2008.558572	59.134796	61.841588
2007.983856	75.068656	61.846593
2007.512531	71.366496	61.851598
2006.308790	65.643737	61.856602
2005.171171	66.732639	61.861607
2004.990317	73.384773	61.866612
2004.084681	69.592271	61.871617
2003.689449	66.357448	61.876622
2003.046318	67.736884	61.881626
2002.232713	73.418660	61.886631
2002.154830	66.072659	61.891636
2001.518855	68.507557	61.896641
2000.972479	63.440582	61.901646
2000.194510	66.443665	61.906650
1999.057176	74.053470	61.911655
1998.605486	62.541987	61.916660
1997.781547	67.025296	61.921665
1997.123782	56.836524	61.926670
1996.523153	69.558966	61.931674
1995.996104	68.392029	61.936679
1995.516812	63.057354	61.941684
1994.382974	69.179482	61.946689
1993.462330	66.956917	61.951694
1992.849510	66.894887	61.956698
1991.795610	69.536478	61.961703
1992.139441	66.947621	61.966708
1991.509023	72.289650	61.971713
1990.963518	62.206064	61.976718
1990.077820	68.996884	61.981722
1989.276238	70.332086	61.986727
1988.848494	55.112410	61.991732
1987.467666	60.210836	61.996737
1987.011523	58.628932	62.001742
1986.622540	57.880067	62.006746
1985.617156	66.523949	62.011751
1985.450500	59.206237	62.016756
1984.658668	64.572310	62.021761
1984.442620	53.901830	62.026766
1983.914249	64.811854	62.031770
1982.577528	67.580346	62.036775
1981.850929	53.575101	62.041780
1980.952474	54.756940	62.046785
1980.586656	56.466114	62.051790
1980.139230	49.215053	62.056794
1979.153862	54.495145	62.061799
1979.016064	51.004993	62.066804
1978.342906	49.880177	62.071809
1977.869555	51.895012	62.076814
1976.535674	55.448405	62.081818
1975.535842	61.413641	62.086823
1975.125983	52.309938	62.091828
1973.971141	54.216900	62.096833
1974.091575	58.536114	62.101838
1974.203947	56.930203	62.106842
1973.330054	60.374311	62.111847
1972.730125	60.923697	62.116852
1971.407387	63.928102	62.121857
1970.907955	51.701943	62.126862
1970.184251	57.792089	62.131866
1969.508263	62.267689	62.136871
1969.146182	47.099108	62.141876
1968.217774	56.255914	62.146881
1967.318593	54.287007	62.151886
1966.594385	48.658473	62.156890
1965.778362	57.682319	62.161895
1965.421230	50.666096	62.166900
1964.688125	54.778587	62.171905
1964.390251	46.169642	62.176910
1964.099007	55.036064	62.181914
1963.220421	62.555915	62.186919
1962.360508	56.174609	62.191924
1961.438001	60.208354	62.196929
1961.122645	58.083692	62.201934
1960.879242	50.136328	62.206938
1959.437955	56.551704	62.211943
1958.456729	48.887050	62.216948
1957.608705	62.060360	62.221953
1957.741853	54.600443	62.226958
1957.048203	52.777116	62.231962
1956.230503	60.044443	62.236967
1955.907474	49.548655	62.241972
1955.210862	54.727722	62.246977
1954.636763	53.778005	62.251982
1953.902253	57.600553	62.256986
1952.499080	57.026883	62.261991
1952.127934	54.408013	62.266996
1951.444699	62.485081	62.272001
1951.005371	55.609644	62.277006
1950.770882	53.569922	62.282010
1950.273013	61.598640	62.287015
1949.210920	49.600586	62.292020
1947.889907	57.816744	62.297025
1947.391194	53.380909	62.302030
1946.980613	56.125403	62.307034
1946.098310	53.171347	62.312039
1945.874626	59.161622	62.317044
1945.495720	52.691350	62.322049
1944.794562	54.827512	62.327054
1943.922317	56.041475	62.332058
1942.688739	55.046635	62.337063
1942.564564	49.103651	62.342068
1941.865787	60.160580	62.347073
1941.323704	57.682392	62.352078
1940.865100	55.670364	62.357082
1939.404892	59.783166	62.362087
1939.011226	47.562309	62.367092
1937.951390	59.159120	62.372097
1937.536065	46.618416	62.377102
1937.071244	53.418125	62.382106
1936.470081	57.314129	62.387111
1936.357216	57.379332	62.392116
1935.518209	49.580143	62.397121
1934.939584	51.226907	62.402126
1934.084472	48.457782	62.407130
1933.074225	51.256471	62.412135
1932.629260	39.873273	62.417140
1931.775766	62.186220	62.422145
1930.500202	48.050524	62.427150
1930.600309	58.099081	62.432154
1929.534234	59.231851	62.437159
1929.269231	47.200314	62.442164
1928.538698	48.316087	62.447169
1928.033797	49.605784	62.452174
1927.946219	44.507001	62.457178
1927.164916	45.645028	62.462183
1926.141668	47.581582	62.467188
1925.374232	53.986195	62.472193
1924.748769	49.751845	62.477198
1924.158979	54.625367	62.482202
1922.589222	56.776421	62.487207
1922.031804	52.632198	62.492212
1921.560017	55.053662	62.497217
1921.575464	58.309287	62.502222
1921.079657	54.609461	62.507226
1920.014094	61.323190	62.512231
1919.827964	53.615907	62.517236
1918.515956	54.216847	62.522241
1917.510779	53.248840	62.527246
1917.138348	55.839042	62.532250
1916.461247	60.496185	62.537255
1916.194440	48.734605	62.542260
1915.421745	49.429706	62.547265
1915.062869	55.249047	62.552270
1914.896293	57.939037	62.557274
1913.380867	51.699668	62.562279
1912.821653	42.201791	62.567284
1912.071954	54.974703	62.572289
1911.341955	59.162411	62.577294
1911.188210	54.922563	62.582298
1909.766022	70.651909	62.587303
1909.053056	60.303189	62.592308
1908.611263	62.358760	62.597313
1908.190258	53.551743	62.602318
1907.802487	56.286312	62.607322
1907.104723	64.807258	62.612327
1906.680680	59.984248	62.617332
1905.590285	61.967743	62.622337
1905.228736	61.868995	62.627342
1904.269975	63.859979	62.632346
1902.807727	61.616198	62.637351
1902.948956	45.588690	62.642356
1901.961225	71.490158	62.647361
1901.189301	57.378595	62.652366
1900.854004	62.533429	62.657370
1900.195564	67.163960	62.662375
1899.836065	58.353486	62.667380
1899.083776	67.021867	62.672385
1898.282598	62.873767	62.677390
1897.532748	61.608178	62.682394
1896.416531	74.062394	62.687399
1896.491161	58.283575	62.692404
1895.675034	55.552429	62.697409
1895.343271	53.496617	62.702414
1894.703623	53.446754	62.707418
1893.916690	57.758626	62.712423
1893.315844	50.814229	62.717428
1892.183574	54.507546	62.722433
1891.066021	57.794813	62.727438
1890.741069	54.187720	62.732442
1890.262737	52.301841	62.737447
1889.619913	53.346927	62.742452
1889.043148	59.953099	62.747457
1888.544198	59.934517	62.752462
1888.201464	45.770600	62.757466
1886.904602	58.860635	62.762471
1886.373451	54.507238	62.767476
1885.352235	62.548088	62.772481
1884.947565	59.723232	62.777486
1884.401932	57.319740	62.782490
1883.900498	66.090227	62.787495
1883.415485	51.231356	62.792500
1881.967532	55.774341	62.797505
1881.746395	53.051239	62.802510
1881.283764	49.298846	62.807514
1880.357785	55.615096	62.812519
1880.201316	53.678117	62.817524
1878.691522	53.204996	62.822529
1877.891648	59.127476	62.827534
1877.412840	56.776457	62.832538
1876.938451	61.485005	62.837543
1876.638013	61.412830	62.842548
1876.239392	61.335742	62.847553
1875.631960	67.607731	62.852558
1874.685627	61.688049	62.857562
1873.611704	62.828395	62.862567
1873.074888	55.881721	62.867572
1872.632202	60.705088	62.872577
1872.036204	61.550349	62.877582
1870.907421	55.210192	62.882586
1870.034972	66.777276	62.887591
1869.892867	58.719219	62.892596
1869.248708	60.672880	62.897601
1869.031177	66.892425	62.902606
1868.513596	62.702461	62.907610
1866.845113	63.464109	62.912615
1866.499549	59.917064	62.917620
1865.920423	62.738794	62.922625
1865.342580	62.370031	62.927630
1864.827141	51.830694	62.932634
1863.484035	57.172355	62.937639
1863.149571	54.320587	62.942644
1862.428470	62.897286	62.947649
1861.718948	58.934927	62.952654
1861.547749	58.096308	62.957658
1861.068514	58.973497	62.962663
1860.294630	49.413519	62.967668
1859.387857	56.832209	62.972673
1858.771755	58.220001	62.977678
1858.256511	54.920681	62.982682
1857.165820	61.026542	62.987687
1856.351729	56.793774	62.992692
1855.609102	66.786894	62.997697
1855.032593	65.083771	63.002702
1854.810834	52.114946	63.007706
1854.152631	61.074334	63.012711
1854.057578	52.997773	63.017716
1852.876037	55.558752	63.022721
1852.035279	55.518753	63.027726
1851.843667	56.254077	63.032730
1850.327050	57.814820	63.037735
1849.829492	55.261772	63.042740
1848.738787	58.358706	63.047745
1848.100633	58.855839	63.052750
1848.348955	51.104817	63.057754
1847.748005	68.353336	63.062759
1847.040617	58.140956	63.067764
1846.975840	56.694062	63.072769
1845.357614	62.298621	63.077774
1844.994311	53.835708	63.082778
1844.015708	68.991577	63.087783
1843.839422	59.644226	63.092788
1842.333309	61.039297	63.097793
1841.385815	58.459920	63.102798
1841.324780	52.596810	63.107802
1840.592940	61.358150	63.112807
1840.599552	55.487452	63.117812
1839.939102	62.322969	63.122817
1838.977868	56.837771	63.127822
1837.910333	51.823633	63.132826
1837.394027	49.620508	63.137831
1837.265280	47.619204	63.142836
1836.565887	54.117115	63.147841
1835.575098	57.827414	63.152846
1834.974843	55.979830	63.157850
1834.299517	54.773392	63.162855
1833.891871	60.423860	63.167860
1832.903776	55.080130	63.172865
1831.705862	47.090384	63.177870
1831.562711	55.674664	63.182874
1830.754799	61.043326	63.187879
1830.863558	46.624799	63.192884
1829.955639	53.556382	63.197889
1828.849829	52.896135	63.202894
1827.985930	49.388827	63.207898
1827.207215	58.039335	63.212903
1827.012456	41.096910	63.217908
1826.719460	45.525912	63.222913
1825.792103	51.329868	63.227918
1824.922728	47.399215	63.232922
1823.913214	57.105119	63.237927
1823.876870	43.211126	63.242932
1823.004596	47.438791	63.247937
1822.616425	48.621657	63.252942
1821.483643	54.548125	63.257946
1820.273374	62.297305	63.262951
1820.026884	56.266519	63.267956
1819.781641	56.471024	63.272961
1819.244017	59.174204	63.277966
1818.858704	51.668883	63.282970
1817.978601	61.556099	63.287975
1817.247759	44.613641	63.292980
1816.207453	54.193543	63.297985
1815.828622	59.374220	63.302990
1815.220416	51.576276	63.307994
1813.826433	65.970180	63.312999
1813.326701	58.777927	63.318004
1812.489731	55.845108	63.323009
1812.234894	57.484637	63.328014
1812.085114	52.397316	63.333018
1811.528559	62.583251	63.338023
1811.323994	50.534257	63.343028
1810.271950	59.844783	63.348033
1809.336836	53.194774	63.353038
1808.716027	50.789046	63.358042
1807.283592	50.437728	63.363047
1806.848962	46.480625	63.368052
1806.306311	48.749350	63.373057
1805.703101	55.936916	63.378062
1805.618511	50.799820	63.383066
1804.934904	50.477829	63.388071
1803.894482	41.624125	63.393076
1802.752858	53.669210	63.398081
1802.442800	54.659897	63.403086
1802.306222	45.829823	63.408090
1801.340163	51.781862	63.413095
1800.178688	38.333064	63.418100
1799.583927	55.246261	63.423105
1798.937161	47.877086	63.428110
1798.552532	43.792193	63.433114
1797.998704	51.798267	63.438119
1797.893534	45.989482	63.443124
1796.549316	48.953222	63.448129
1796.063379	44.690445	63.453134
1795.654545	43.556820	63.458138
1794.694929	51.682530	63.463143
1793.960669	49.471447	63.468148
1793.160319	48.696474	63.473153
1792.177983	45.043979	63.478158
1792.220034	49.195843	63.483162
1791.630509	50.729245	63.488167
1790.580253	45.676115	63.493172
1789.765023	44.361017	63.498177
1788.779605	47.911199	63.503182
1788.629596	47.581748	63.508186
1788.219871	48.452641	63.513191
1787.738457	36.130650	63.518196
1786.733886	45.608683	63.523201
1785.623701	48.328675	63.528206
1785.424731	47.224804	63.533210
1784.934626	51.208857	63.538215
1784.497935	39.231435	63.543220
1783.154480	47.474874	63.548225
1782.357289	45.127128	63.553230
1781.942960	38.634137	63.558234
1781.522759	48.535051	63.563239
1781.094084	38.795707	63.568244
1780.009524	47.105269	63.573249
1779.411896	53.493985	63.578254
1779.165243	44.694013	63.583258
1778.294437	52.100702	63.588263
1777.602169	43.232722	63.593268
1776.400988	52.756179	63.598273
1775.819238	46.352854	63.603278
1775.552609	38.472299	63.608282
1774.928643	51.064406	63.613287
1774.848539	41.033154	63.618292
1773.329652	49.124680	63.623297
1772.633245	46.565382	63.628302
1772.073910	42.451467	63.633306
1771.442580	56.853574	63.638311
1771.170353	48.097088	63.643316
1769.967574	49.503952	63.648321
1769.172673	46.919295	63.653326
1768.819958	53.313274	63.658330
1768.084427	46.980107	63.663335
1767.653443	50.167847	63.668340
1767.158348	48.686792	63.673345
1766.163094	54.257113	63.678350
1765.755428	37.113548	63.683354
1765.049455	52.850613	63.688359
1764.593760	41.653677	63.693364
1763.168078	41.723949	63.698369
1762.164868	31.282626	63.703374
1762.025415	30.615599	63.708378
1761.601343	50.215707	63.713383
1761.227544	43.612200	63.718388
1760.543903	42.410258	63.723393
1759.867768	43.578939	63.728398
1759.225423	37.276714	63.733402
1758.558732	37.887213	63.738407
1757.937834	40.944259	63.743412
1756.864423	50.109950	63.748417
1755.906804	46.229610	63.753422
1755.420597	35.714062	63.758426
1755.042544	50.571119	63.763431
1754.828349	47.616687	63.768436
1753.554198	49.321909	63.773441
1753.121557	46.966739	63.778446
1752.293827	41.802591	63.783450
1751.530245	54.366412	63.788455
1751.643980	41.694433	63.793460
1750.519903	44.635847	63.798465
1749.453076	36.414015	63.803470
1749.373811	40.747572	63.808474
1748.485262	47.202996	63.813479
1747.444152	43.755403	63.818484
1746.611029	41.191019	63.823489
1745.635068	45.845194	63.828494
1745.591572	42.824228	63.833498
1745.168644	52.019082	63.838503
1744.957640	41.130232	63.843508
1744.733389	35.950670	63.848513
1743.147138	47.288922	63.853518
1742.457304	37.488561	63.858522
1741.821163	43.760390	63.863527
1740.900006	44.113255	63.868532
1739.980230	39.258632	63.873537
1739.270217	48.814480	63.878542
1738.835630	40.105870	63.883546
1738.607475	52.095781	63.888551
1738.352435	45.495494	63.893556
1737.885004	45.963961	63.898561
1736.685865	46.644839	63.903566
1736.021904	43.900621	63.908570
1735.106674	55.310509	63.913575
1734.463886	46.100359	63.918580
1733.447225	51.972144	63.923585
1732.398555	53.274121	63.928590
1732.302231	46.000477	63.933594
1731.567538	49.296384	63.938599
1731.514311	51.659284	63.943604
1731.134773	49.500694	63.948609
1730.422306	57.219728	63.953614
1729.584059	49.455197	63.958618
1728.957152	53.684921	63.963623
1727.884696	52.361809	63.968628
1726.934734	52.156263	63.973633
1726.468384	60.410239	63.978638
1726.299829	49.563531	63.983642
1725.546145	51.706512	63.988647
1724.933618	45.415328	63.993652
1723.932190	51.410857	63.998657
1723.395401	62.751183	64.003662
1722.814311	51.302924	64.008666
1721.837022	53.839402	64.013671
1720.936576	53.599184	64.018676
1720.476813	56.271091	64.023681
1719.575273	53.955708	64.028686
1719.652992	49.612883	64.033690
1719.098581	58.330292	64.038695
1718.217208	48.572971	64.043700
1717.139645	50.737434	64.048705
1716.569333	52.341919	64.053710
1716.522417	50.146271	64.058714
1715.458381	54.312960	64.063719
1714.499047	54.071059	64.068724
1713.631192	55.718074	64.073729
1713.001601	58.500538	64.078734
1712.878925	51.215309	64.083738
1712.685116	54.307036	64.088743
1711.689728	50.030575	64.093748
1710.518806	56.986619	64.098753
1710.120510	51.489337	64.103758
1709.959963	44.773118	64.108762
1708.587886	55.593234	64.113767
1707.577253	56.352997	64.118772
1707.087269	59.300951	64.123777
1706.409292	53.650967	64.128782
1706.173823	48.701854	64.133786
1705.877085	57.917672	64.138791
1705.273374	56.502769	64.143796
1704.397348	56.878441	64.148801
1703.627413	60.716138	64.153806
1703.336673	47.742538	64.158810
1701.748380	58.489766	64.163815
1700.933228	54.692476	64.168820
1700.684204	53.438862	64.173825
1700.020321	48.330710	64.178830
1699.644480	47.562457	64.183834
1699.555609	58.374304	64.188839
1698.589712	47.633751	64.193844
1697.396474	49.231526	64.198849
1696.618785	56.759070	64.203854
1696.647609	52.189037	64.208858
1695.280229	51.713904	64.213863
1694.420049	48.773776	64.218868
1694.290566	43.087140	64.223873
1693.813892	44.042800	64.228878
1693.401360	48.948130	64.233882
1692.383317	59.221571	64.238887
1691.756725	52.606188	64.243892
1690.949126	53.682225	64.248897
1690.449063	56.381038	64.253902
1689.480314	49.430486	64.258906
1688.388296	53.219994	64.263911
1687.871032	49.531516	64.268916
1687.484991	43.666430	64.273921
1686.889597	59.729732	64.278926
1687.199136	48.707738	64.283930
1685.757316	50.663559	64.288935
1685.032314	46.498708	64.293940
1684.539417	58.970660	64.298945
1684.191299	49.969193	64.303950
1682.658896	53.133197	64.308954
1681.643564	56.915258	64.313959
1681.301361	49.573439	64.318964
1681.257215	56.307930	64.323969
1680.388365	48.529356	64.328974
1680.345626	44.391754	64.333978
1679.082424	49.227201	64.338983
1678.529999	50.175973	64.343988
1678.032084	49.059672	64.348993
1677.168521	47.031597	64.353998
1676.173859	51.390713	64.359002
1675.460079	57.137133	64.364007
1675.332650	51.486442	64.369012
1674.670575	45.064367	64.374017
1674.199397	47.775940	64.379022
1672.933515	48.014849	64.384026
1672.281912	50.084856	64.389031
1672.129212	44.652654	64.394036
1671.322517	52.016069	64.399041
1669.599197	48.167506	64.404046
1669.156586	50.067116	64.409050
1668.665506	56.120371	64.414055
1668.543843	49.856887	64.419060
1668.677917	46.848720	64.424065
1668.065719	51.038271	64.429070
1667.127126	44.190177	64.434074
1666.006944	50.959973	64.439079
1665.163413	50.523070	64.444084
1663.771024	51.565850	64.449089
1663.285619	54.043135	64.454094
1662.932716	45.502921	64.459098
1662.274652	62.426188	64.464103
1662.246429	54.403691	64.469108
1662.023354	53.880844	64.474113
1660.640280	55.210738	64.479118
1660.023795	46.598851	64.484122
1659.100603	50.823613	64.489127
1658.849998	53.946442	64.494132
1657.881306	51.602325	64.499137
1656.884831	55.163773	64.504142
1656.465210	46.003356	64.509146
1655.671977	56.818277	64.514151
1655.272806	48.509348	64.519156
1655.334461	44.113883	64.524161
1653.973453	49.556254	64.529166
1653.348772	43.419993	64.534170
1652.858425	52.188732	64.539175
1652.006664	51.231152	64.544180
1651.322233	53.255916	64.549185
1650.352267	49.798639	64.554190
1650.138922	50.162101	64.559194
1649.545054	50.412541	64.564199
1648.569464	43.012074	64.569204
1647.708109	50.387330	64.574209
1647.046450	53.513957	64.579214
1647.244364	46.113154	64.584218
1646.330930	53.149745	64.589223
1645.387493	54.480771	64.594228
1644.655862	48.810946	64.599233
1644.161323	48.998298	64.604238
1643.833510	49.946089	64.609242
1642.632737	54.282765	64.614247
1641.639823	52.607998	64.619252
1641.006860	54.108907	64.624257
1640.616403	50.133782	64.629262
1640.444542	45.701294	64.634266
1639.574644	45.501985	64.639271
1639.139443	46.296520	64.644276
1638.322406	45.268772	64.649281
1637.511700	49.633371	64.654286
1636.986460	40.835106	64.659290
1635.494199	49.460228	64.664295
1634.712805	47.501118	64.669300
1634.321296	37.656558	64.674305
1633.566337	44.330494	64.679310
1633.555872	41.238053	64.684314
1633.039866	47.799910	64.689319
1632.727032	53.547299	64.694324
1632.156514	44.111232	64.699329
1631.034038	46.032119	64.704334
1630.697410	41.036011	64.709338
1629.143410	52.821798	64.714343
1628.540685	44.158849	64.719348
1628.194231	47.195978	64.724353
1627.496149	52.602434	64.729358
1627.492107	41.652342	64.734362
1626.837155	51.603176	64.739367
1625.928538	47.793954	64.744372
1625.217407	43.661614	64.749377
1623.707591	43.500893	64.754382
1623.363558	43.511369	64.759386
1622.249415	44.140947	64.764391
1622.406652	45.282926	64.769396
1621.919438	46.342778	64.774401
1621.345144	48.933541	64.779406
1620.568138	38.573046	64.784410
1619.277330	51.083446	64.789415
1619.040031	49.126212	64.794420
1618.754922	47.851532	64.799425
1617.838924	51.559484	64.804430
1616.992765	48.043127	64.809434
1616.086533	52.567993	64.814439
1615.728926	48.213904	64.819444
1615.239284	42.379486	64.824449
1613.962138	47.989908	64.829454
1613.511651	38.993688	64.834458
1612.767922	46.910100	64.839463
1612.374347	42.782508	64.844468
1612.140311	43.385810	64.849473
1610.972927	48.694935	64.854478
1610.271401	41.977943	64.859482
1609.785375	45.043555	64.864487
1609.445299	43.474825	64.869492
1608.254323	40.890069	64.874497
1607.056610	44.158640	64.879502
1606.768356	40.823319	64.884506
1606.075223	51.991361	64.889511
1605.440692	49.240926	64.894516
1605.453038	54.640177	64.899521
1605.087511	53.592747	64.904526
1604.290833	41.975355	64.909530
1603.108931	45.670361	64.914535
1602.669024	43.157098	64.919540
1602.019002	41.440486	64.924545
1600.618353	52.180025	64.929550
1600.214039	44.411264	64.934554
1599.745664	44.491962	64.939559
1599.518414	47.320915	64.944564
1598.663498	47.877778	64.949569
1597.610452	39.199654	64.954574
1597.285158	36.489982	64.959578
1596.584496	45.408835	64.964583
1596.256626	49.725118	64.969588
1595.110028	41.203788	64.974593
1594.633822	41.944918	64.979598
1593.969072	40.140760	64.984602
1593.626574	39.804056	64.989607
1592.785072	34.438725	64.994612
1591.958138	45.686371	64.999617
1591.202286	56.542675	65.004622
1590.338705	50.964797	65.009626
1589.138457	52.685163	65.014631
1588.569897	41.796381	65.019636
1588.001584	48.003844	65.024641
1587.852792	57.374358	65.029646
1587.769685	52.061998	65.034650
1587.126839	47.062507	65.039655
1586.543772	44.441101	65.044660
1585.508883	44.569232	65.049665
1584.937867	49.900313	65.054670
1583.990873	41.632712	65.059674
1582.937759	55.679211	65.064679
1582.501635	43.160845	65.069684
1582.069572	46.946463	65.074689
1581.234753	50.272509	65.079694
1580.905159	43.529549	65.084698
1579.484450	49.416693	65.089703
1578.872856	55.757198	65.094708
1578.683234	42.794377	65.099713
1578.200508	54.119811	65.104718
1578.064316	55.019817	65.109722
1576.880769	52.175265	65.114727
1576.339489	59.909710	65.119732
1575.898550	47.231252	65.124737
1574.326955	60.369781	65.129742
1573.521525	46.680029	65.134746
1572.693504	51.632464	65.139751
1572.048790	50.189415	65.144756
1572.054739	47.185833	65.149761
1571.442958	47.618916	65.154766
1571.675277	50.934687	65.159770
1570.691973	55.400847	65.164775
1569.691008	47.965020	65.169780
1569.036853	48.371719	65.174785
1567.614522	56.892724	65.179790
1567.267347	48.767949	65.184794
1566.601929	51.909383	65.189799
1566.221752	40.150135	65.194804
1565.652569	50.927892	65.199809
1564.708476	50.309875	65.204814
1564.155249	50.642190	65.209818
1563.630236	58.126461	65.214823
1563.142038	52.246090	65.219828
1562.504081	53.102816	65.224833
1561.298503	59.509319	65.229838
1560.450367	49.514968	65.234842
1560.074681	46.568871	65.239847
1559.609854	53.321310	65.244852
1559.269949	39.201201	65.249857
1557.984273	54.120468	65.254862
1557.745838	48.424349	65.259866
1556.929858	53.355952	65.264871
1556.493360	47.139354	65.269876
1555.400444	49.446672	65.274881
1554.452091	51.019792	65.279886
1554.244442	45.462290	65.284890
1553.753830	50.772715	65.289895
1553.130423	43.992865	65.294900
1551.988193	48.711371	65.299905
1551.410710	46.577957	65.304910
1551.223313	44.644343	65.309914
1550.302468	48.860880	65.314919
1549.732408	49.834558	65.319924
1548.785821	41.929619	65.324929
1548.082891	57.133199	65.329934
1547.971107	49.158688	65.334938
1547.237442	49.819308	65.339943
1546.634035	45.209390	65.344948
1545.733261	36.521291	65.349953
1544.754161	39.876580	65.354958
1544.385302	39.121434	65.359962
1543.190651	46.040304	65.364967
1542.600061	41.991342	65.369972
1542.005034	40.928349	65.374977
1541.274507	48.730711	65.379982
1541.493951	39.049300	65.384986
1540.791577	49.100723	65.389991
1540.204706	45.044861	65.394996
1539.175144	47.584977	65.400001
1538.459814	47.350103	65.405006
1538.257991	41.731752	65.410010
1536.939846	48.134068	65.415015
1536.121851	46.944075	65.420020
1535.481369	47.443229	65.425025
1535.338310	47.582636	65.430030
1534.954127	45.763874	65.435034
1533.444881	46.175567	65.440039
1532.989336	44.606272	65.445044
1532.728788	44.417408	65.450049
1531.728914	52.566935	65.455054
1531.090964	43.647834	65.460058
1529.986038	40.125320	65.465063
1529.908879	42.067806	65.470068
1529.351479	38.948736	65.475073
1528.572958	50.347982	65.480078
1528.021591	43.085169	65.485082
1527.446983	46.718398	65.490087
1526.966369	43.252802	65.495092
1526.074856	44.417918	65.500097
1525.191594	48.677378	65.505102
1524.780199	39.492038	65.510106
1523.763410	52.152901	65.515111
1523.020790	54.098630	65.520116
1522.037415	43.588033	65.525121
1521.417517	54.772837	65.530126
1521.147266	39.386376	65.535130
1520.720754	47.511027	65.540135
1520.566939	39.652017	65.545140
1519.561081	35.797578	65.550145
1518.549792	42.675490	65.555150
1518.136702	40.451305	65.560154
1517.029504	48.004436	65.565159
1516.519865	49.288651	65.570164
1515.779852	50.458082	65.575169
1515.372357	50.992760	65.580174
1515.131211	38.914169	65.585178
1513.892603	48.580074	65.590183
1512.676435	44.838695	65.595188
1512.293915	39.966599	65.600193
1512.141830	48.829834	65.605198
1511.656075	43.256607	65.610202
1511.003428	51.130181	65.615207
1510.080405	56.542446	65.620212
1509.432878	52.929905	65.625217
1508.853966	41.998639	65.630222
1508.250909	45.209025	65.635226
1507.017569	47.606488	65.640231
1506.413467	49.918151	65.645236
1506.183334	50.478263	65.650241
1505.405671	50.792638	65.655246
1504.910850	39.662714	65.660250
1503.966494	45.661068	65.665255
1503.134324	51.893129	65.670260
1502.898517	52.954053	65.675265
1502.121171	48.450638	65.680270
1500.986438	43.046781	65.685274
1500.091411	46.661546	65.690279
1499.806476	49.223697	65.695284
1499.786483	43.128588	65.700289
1499.389187	45.735403	65.705294
1498.608935	49.404472	65.710298
1497.636265	52.230462	65.715303
1497.099333	44.473339	65.720308
1496.011713	40.687097	65.725313
1494.652634	47.355353	65.730318
1494.497193	35.769366	65.735322
1493.707596	45.532661	65.740327
1493.181499	43.201855	65.745332
1492.892370	47.150856	65.750337
1492.774440	44.815111	65.755342
1491.912939	38.856101	65.760346
1490.859194	38.041067	65.765351
1490.513170	47.782758	65.770356
1489.782650	39.137802	65.775361
1488.676472	44.228293	65.780366
1488.069166	33.433233	65.785370
1487.665357	42.216615	65.790375
1486.883820	45.435657	65.795380
1486.194775	41.302217	65.800385
1485.152441	44.455469	65.805390
1484.774601	38.839080	65.810394
1484.568243	36.470081	65.815399
1483.878518	30.889856	65.820404
1482.921809	34.618508	65.825409
1482.089137	39.926528	65.830414
1481.824094	35.467868	65.835418
1481.113087	45.322757	65.840423
1480.587994	37.176608	65.845428
1480.048666	31.902075	65.850433
1479.202607	36.947286	65.855438
1478.061089	33.995179	65.860442
1477.156654	38.991320	65.865447
1476.631045	37.884193	65.870452
1476.523276	33.263341	65.875457
1475.921862	39.799363	65.880462
1475.340983	36.420680	65.885466
1474.153030	45.901924	65.890471
1473.479012	40.909789	65.895476
1473.087842	37.461531	65.900481
1472.389269	45.372370	65.905486
1472.000275	39.253905	65.910490
1470.835232	38.999055	65.915495
1470.615208	31.809765	65.920500
1470.349218	31.934018	65.925505
1468.743960	45.461143	65.930510
1468.007877	37.309893	65.935514
1467.251463	38.153927	65.940519
1467.008925	32.050038	65.945524
1467.188092	33.365143	65.950529
1465.780691	41.981586	65.955534
1465.078253	30.246782	65.960538
1464.430161	35.900795	65.965543
1463.754342	41.187045	65.970548
1463.252634	31.987694	65.975553
1462.225828	38.044106	65.980558
1461.964872	35.552896	65.985562
1461.277379	42.962066	65.990567
1460.341910	39.045212	65.995572
1459.745629	37.283828	66.000577
1458.927030	42.039245	66.005582
1458.532037	31.354748	66.010586
1457.933141	39.800118	66.015591
1457.419210	43.541991	66.020596
1456.366351	40.522184	66.025601
1455.824640	45.228865	66.030606
1455.473049	41.719124	66.035610
1454.384157	39.092987	66.040615
1453.244681	40.204494	66.045620
1452.988739	35.749123	66.050625
1452.082012	40.094335	66.055630
1451.970372	38.875688	66.060634
1451.704246	39.881507	66.065639
1450.940545	35.070008	66.070644
1450.013432	39.161410	66.075649
1449.103676	44.385494	66.080654
1448.923070	44.209165	66.085658
1447.672259	36.458286	66.090663
1446.913846	44.856471	66.095668
1446.448513	28.621082	66.100673
1445.769941	42.568650	66.105678
1445.661171	38.878388	66.110682
1444.815867	43.709019	66.115687
1444.027093	36.435080	66.120692
1443.205714	31.828300	66.125697
1442.659283	39.399561	66.130702
1442.072400	37.220360	66.135706
1441.027859	37.971420	66.140711
1440.158112	35.633744	66.145716
1439.973485	31.594409	66.150721
1439.391688	36.059872	66.155726
1439.340003	38.115008	66.160730
1437.757932	35.106781	66.165735
1437.273651	45.134594	66.170740
1437.064967	38.292021	66.175745
1436.136400	47.215586	66.180750
1435.643341	35.654097	66.185754
1434.836960	34.569528	66.190759
1434.270434	39.608171	66.195764
1433.606122	37.644711	66.200769
1432.513768	36.779066	66.205774
1432.144783	30.422460	66.210778
1431.573597	37.551365	66.215783
1430.740339	34.228577	66.220788
1429.856435	35.364130	66.225793
1428.921200	46.982270	66.230798
1428.977008	38.843944	66.235802
1428.437541	34.698578	66.240807
1427.556520	33.356208	66.245812
1426.797095	35.971702	66.250817
1425.854028	42.040050	66.255822
1425.399876	34.517385	66.260826
1424.761574	40.565678	66.265831
1424.311445	39.415025	66.270836
1423.388386	34.510591	66.275841
1422.545365	33.587972	66.280846
1422.218339	40.339018	66.285850
1421.665035	34.767092	66.290855
1420.984049	33.854990	66.295860
1420.450802	30.924504	66.300865
1419.707496	48.427461	66.305870
1419.219278	32.733472	66.310874
1417.899853	36.499298	66.315879
1417.144888	36.171406	66.320884
1416.820926	37.675291	66.325889
1416.313167	39.142156	66.330894
1415.744154	37.467915	66.335898
1414.947993	36.022172	66.340903
1414.138216	42.752178	66.345908
1413.880709	36.414125	66.350913
1412.895778	34.389666	66.355918
1412.467428	30.827479	66.360922
1411.264628	46.146788	66.365927
1411.204974	42.846125	66.370932
1410.677934	38.665669	66.375937
1409.306926	42.824488	66.380942
1408.550042	36.751898	66.385946
1408.451241	40.429369	66.390951
1407.627089	36.597348	66.395956
1407.369686	40.088711	66.400961
1406.158627	36.209377	66.405966
1405.253004	34.970277	66.410970
1404.825172	40.627140	66.415975
1404.203973	45.821141	66.420980
1404.259124	34.926330	66.425985
1403.036886	41.171527	66.430990
1402.532201	36.186406	66.435994
1401.951061	39.886928	66.440999
1400.968944	34.345321	66.446004
1400.109778	36.281220	66.451009
1399.328497	41.081185	66.456014
1399.025746	29.197718	66.461018
1398.597759	44.463256	66.466023
1398.109451	31.510114	66.471028
1397.236759	37.767561	66.476033
1396.179912	41.464852	66.481038
1395.849429	35.475880	66.486042
1395.572131	39.238496	66.491047
1394.033887	37.221570	66.496052
1393.570429	34.609589	66.501057
1392.920749	43.159239	66.506062
1392.448948	37.620097	66.511066
1392.005439	36.561442	66.516071
1391.050379	36.852008	66.521076
1390.733829	42.789237	66.526081
1389.503170	39.542249	66.531086
1389.258381	29.578240	66.536090
1388.357204	32.977965	66.541095
1387.435421	32.722333	66.546100
1387.294666	34.578732	66.551105
1386.718854	40.888342	66.556110
1386.235822	31.217677	66.561114
1384.906393	40.633915	66.566119
1384.219615	35.059561	66.571124
1383.925768	32.160416	66.576129
1383.233945	39.220194	66.581134
1383.068029	43.698411	66.586138
1381.964455	41.107757	66.591143
1381.094766	41.096166	66.596148
1380.751572	36.979537	66.601153
1379.480700	40.598888	66.606158
1378.695971	33.974056	66.611162
1378.278137	40.797888	66.616167
1377.631453	42.420889	66.621172
1377.759740	39.054082	66.626177
1377.114486	41.627786	66.631182
1376.192422	37.547982	66.636186
1375.352077	37.355104	66.641191
1374.487549	38.306240	66.646196
1374.134074	40.445621	66.651201
1372.923482	43.140735	66.656206
1372.276468	37.824998	66.661210
1372.487418	33.158222	66.666215
1371.175348	45.743051	66.671220
1370.593031	37.715632	66.676225
1369.658136	45.042721	66.681230
1369.503184	44.766122	66.686234
1368.940497	36.904322	66.691239
1367.939337	41.876447	66.696244
1367.075133	32.438274	66.701249
1366.294270	48.089503	66.706254
1365.897298	39.553213	66.711258
1365.834001	34.950534	66.716263
1365.026001	38.784900	66.721268
1364.227626	43.614400	66.726273
1363.046231	44.552833	66.731278
1362.905063	34.613355	66.736282
1362.388117	37.833734	66.741287
1361.134015	38.714337	66.746292
1360.876627	36.080642	66.751297
1360.247312	40.156271	66.756302
1359.715816	36.785538	66.761306
1358.625729	35.834406	66.766311
1357.776685	34.031226	66.771316
1357.577627	32.091600	66.776321
1356.899170	34.662700	66.781326
1356.270532	35.248327	66.786330
1355.293160	34.829651	66.791335
1354.597428	38.679289	66.796340
1354.092126	34.891220	66.801345
1353.591970	41.370163	66.806350
1352.923528	33.154588	66.811354
1351.951777	36.087715	66.816359
1351.486676	33.682590	66.821364
1351.216427	38.106427	66.826369
1350.079352	40.562776	66.831374
1349.175172	35.185425	66.836378
1348.601860	44.167655	66.841383
1347.984218	38.735290	66.846388
1347.712284	38.869962	66.851393
1347.224434	44.798156	66.856398
1346.164581	44.268012	66.861402
1345.478338	40.656946	66.866407
1345.037790	43.431510	66.871412
1344.676963	35.025104	66.876417
1343.527094	45.113003	66.881422
1342.708037	32.885838	66.886426
1342.419371	39.081994	66.891431
1341.689925	44.288484	66.896436
1340.931540	37.921258	66.901441
1339.932904	41.858481	66.906446
1339.351849	39.585335	66.911450
1339.125238	39.577182	66.916455
1338.604746	48.300276	66.921460
1337.514930	38.464304	66.926465
1336.988041	43.189148	66.931470
1336.707015	44.676755	66.936474
1335.979985	46.889721	66.941479
1334.766966	36.937717	66.946484
1334.464052	42.328717	66.951489
1333.758512	36.905599	66.956494
1332.748452	33.319211	66.961498
1331.739126	34.857945	66.966503
1330.947452	40.402345	66.971508
1331.012163	38.024960	66.976513
1330.418959	44.875102	66.981518
1330.304313	40.882999	66.986522
1329.527421	41.478009	66.991527
1328.476893	44.453633	66.996532
1328.255451	40.998919	67.001537
1326.810493	53.789408	67.006542
1326.002695	43.331422	67.011546
1325.575961	45.190710	67.016551
1324.805427	43.042312	67.021556
1324.866225	39.116938	67.026561
1323.725808	46.333208	67.031566
1322.785201	36.626492	67.036570
1322.630059	36.715791	67.041575
1321.589340	49.814182	67.046580
1321.299859	34.892899	67.051585
1320.646055	40.845901	67.056590
1319.632690	39.917283	67.061594
1319.079980	37.786297	67.066599
1318.560538	37.558189	67.071604
1318.318513	29.820475	67.076609
1317.084090	38.207626	67.081614
1316.500706	34.625951	67.086618
1316.225185	35.928174	67.091623
1315.014406	42.764537	67.096628
1314.279987	42.018659	67.101633
1313.431398	44.908565	67.106638
1312.914679	46.810548	67.111642
1312.995082	48.664907	67.116647
1312.128476	42.128810	67.121652
1311.425930	37.943166	67.126657
1310.275177	43.549392	67.131662
1310.537194	42.310769	67.136666
1309.305481	42.336259	67.141671
1308.040570	43.491427	67.146676
1308.017421	37.869935	67.151681
1307.407449	50.346320	67.156686
1307.020181	39.812022	67.161690
1305.780034	40.211026	67.166695
1304.857744	42.778328	67.171700
1304.659776	39.299384	67.176705
1304.042902	50.426958	67.181710
1303.074262	48.529266	67.186714
1302.243138	38.131774	67.191719
1301.400603	41.918031	67.196724
1301.446317	43.401002	67.201729
1300.763957	51.045939	67.206734
1300.172974	46.628087	67.211738
1299.632158	46.513771	67.216743
1298.950063	48.788990	67.221748
1298.490599	41.219890	67.226753
1297.109828	44.372615	67.231758
1296.363392	47.033390	67.236762
1295.876532	39.896012	67.241767
1295.363305	45.943369	67.246772
1294.860662	42.803035	67.251777
1293.915544	53.919721	67.256782
1293.112513	42.126852	67.261786
1292.982370	38.627664	67.266791
1292.243388	44.345050	67.271796
1291.448979	42.537936	67.276801
1290.589354	46.169216	67.281806
1290.134004	41.745573	67.286810
1289.853738	44.089372	67.291815
1288.750866	53.359246	67.296820
1288.030821	50.961550	67.301825
1287.203286	48.956271	67.306830
1286.953418	46.960072	67.311834
1286.517920	47.336806	67.316839
1284.970349	49.409007	67.321844
1284.905736	53.082623	67.326849
1284.078787	56.442198	67.331854
1283.684738	45.696086	67.336858
1282.588675	45.345196	67.341863
1281.727989	45.062540	67.346868
1281.238464	41.418638	67.351873
1280.939417	52.325366	67.356878
1280.546241	44.629030	67.361882
1279.870064	42.432527	67.366887
1278.657084	49.337068	67.371892
1278.354467	43.873556	67.376897
1277.572640	52.999344	67.381902
1276.544686	50.363596	67.386906
1275.837331	44.395143	67.391911
1275.362857	51.589127	67.396916
1275.244095	39.584962	67.401921
1274.336452	46.404683	67.406926
1273.456741	36.431258	67.411930
1272.434531	45.055932	67.416935
1272.122827	39.688487	67.421940
1272.026709	31.971736	67.426945
1271.286265	43.182036	67.431950
1270.022341	43.977509	67.436954
1269.512845	41.398105	67.441959
1269.005589	47.255276	67.446964
1269.215018	38.439658	67.451969
1267.743056	45.746513	67.456974
1266.843235	45.764984	67.461978
1266.534073	42.166525	67.466983
1265.191957	45.727870	67.471988
1264.339345	40.217770	67.476993
1263.416669	45.645820	67.481998
1263.449568	48.476005	67.487002
1263.542905	37.535709	67.492007
1263.014777	45.794810	67.497012
1262.151775	49.824039	67.502017
1261.095355	41.941426	67.507022
1260.555112	39.939362	67.512026
1259.284618	40.876238	67.517031
1258.513328	42.285686	67.522036
1258.068706	41.056916	67.527041
1257.841794	47.301608	67.532046
1257.446594	43.391971	67.537050
1256.849169	46.519508	67.542055
1255.635341	52.515844	67.547060
1255.372383	43.053074	67.552065
1254.631797	50.874440	67.557070
1253.620582	51.759052	67.562074
1252.759236	42.161191	67.567079
1251.816253	44.241357	67.572084
1251.662789	41.282058	67.577089
1251.655625	48.176225	67.582094
1250.980562	35.166091	67.587098
1250.221768	38.248323	67.592103
1249.012232	42.805755	67.597108
1248.919214	45.353178	67.602113
1247.721805	43.999679	67.607118
1246.934094	41.134928	67.612122
1246.433444	35.236124	67.617127
1245.774022	42.129924	67.622132
1245.192543	32.995362	67.627137
1244.422988	41.226620	67.632142
1244.004501	42.784980	67.637146
1243.706933	38.498689	67.642151
1242.385796	44.206154	67.647156
1241.957937	41.927597	67.652161
1241.137851	41.490261	67.657166
1240.392744	40.093228	67.662170
1239.627822	47.566796	67.667175
1238.654826	45.467967	67.672180
1238.289611	32.924247	67.677185
1237.626348	46.938795	67.682190
1237.516454	47.063482	67.687194
1237.335039	37.318086	67.692199
1236.120944	43.970499	67.697204
1235.398831	42.623429	67.702209
1234.834416	45.658986	67.707214
1234.025127	46.970401	67.712218
1233.118296	44.867362	67.717223
1232.468789	46.787321	67.722228
1232.318707	40.604107	67.727233
1230.754204	45.580704	67.732238
1229.997057	41.351727	67.737242
1229.715168	40.734192	67.742247
1229.268015	47.833945	67.747252
1228.948469	36.446786	67.752257
1228.412564	46.105923	67.757262
1227.451800	47.368886	67.762266
1226.720569	45.591171	67.767271
1225.966495	58.517852	67.772276
1225.643386	45.697763	67.777281
1224.290331	41.528856	67.782286
1223.691430	34.658484	67.787290
1223.586431	41.695940	67.792295
1222.497473	46.838199	67.797300
1222.695211	40.702180	67.802305
1221.412718	45.398963	67.807310
1220.945409	43.877333	67.812314
1220.192479	37.695370	67.817319
1218.774262	37.138688	67.822324
1217.925400	36.948793	67.827329
1217.292614	47.239943	67.832334
1217.752300	35.571170	67.837338
1217.175681	39.781954	67.842343
1216.749616	29.924081	67.847348
1215.589619	38.873463	67.852353
1215.063210	36.085444	67.857358
1214.353396	43.020381	67.862362
1213.254063	39.102877	67.867367
1212.317055	40.614387	67.872372
1211.964609	35.583026	67.877377
1211.326227	39.459848	67.882382
1211.158772	42.834415	67.887386
1210.481669	38.190583	67.892391
1209.302447	45.238019	67.897396
1208.799916	43.636834	67.902401
1208.153101	47.868248	67.907406
1207.671937	45.629713	67.912410
1206.878679	35.953238	67.917415
1206.044812	46.749466	67.922420
1205.584426	39.793988	67.927425
1204.973958	44.347636	67.932430
1204.218358	44.207571	67.937434
1203.612477	46.798708	67.942439
1202.687837	52.687574	67.947444
1202.654833	38.384717	67.952449
1201.626885	39.675720	67.957454
1200.555284	48.016528	67.962458
1199.963276	40.809164	67.967463
1199.531049	47.209514	67.972468
1199.565053	39.632928	67.977473
1198.127904	42.566005	67.982478
1197.381321	42.504935	67.987482
1197.002853	42.118810	67.992487
1196.150085	52.400795	67.997492
1196.119321	37.818456	68.002497
1195.118294	41.940618	68.007502
1194.099280	42.219349	68.012506
1193.855545	40.512354	68.017511
1192.902404	48.621432	68.022516
1192.020745	30.552063	68.027521
1191.258091	44.314332	68.032526
1191.065228	33.965200	68.037530
1190.804973	38.012132	68.042535
1189.435539	38.636762	68.047540
1188.922004	40.129819	68.052545
1187.798103	47.610025	68.057550
1187.728373	43.547712	68.062554
1187.447489	40.913044	68.067559
1186.601443	47.317706	68.072564
1185.749672	38.142567	68.077569
1185.361713	45.341722	68.082574
1184.802768	39.146267	68.087578
1183.736242	48.076070	68.092583
1182.915802	53.040020	68.097588
1182.585960	43.108495	68.102593
1181.909000	45.297767	68.107598
1180.561075	32.747923	68.112602
1180.362072	32.347452	68.117607
1179.256571	49.996349	68.122612
1179.144519	44.128799	68.127617
1178.866659	50.621301	68.132622
1178.057861	47.942856	68.137626
1177.697355	49.033100	68.142631
1176.749248	52.167540	68.147636
1175.543562	38.155275	68.152641
1174.532644	45.043489	68.157646
1173.982229	37.184528	68.162650
1173.897069	41.583670	68.167655
1173.464225	52.771881	68.172660
1172.865329	41.246229	68.177665
1171.635542	37.677508	68.182670
1170.766520	49.179521	68.187674
1170.457018	42.684192	68.192679
1169.713929	42.526378	68.197684
1169.745481	38.033209	68.202689
1168.555264	44.215062	68.207694
1167.620205	37.623680	68.212698
1167.162335	33.888037	68.217703
1166.628006	36.532457	68.222708
1166.288013	43.906916	68.227713
1165.251328	40.176595	68.232718
1164.256904	47.685103	68.237722
1164.094740	41.260962	68.242727
1163.246222	47.889956	68.247732
1162.462460	43.487035	68.252737
1161.382522	47.490869	68.257742
1160.983379	45.613047	68.262746
1161.073313	49.063378	68.267751
1160.475427	47.904735	68.272756
1159.377495	43.122840	68.277761
1158.749756	45.537685	68.282766
1158.218811	47.456153	68.287770
1157.274815	44.559516	68.292775
1156.468545	42.590326	68.297780
1156.192123	39.508664	68.302785
1155.557828	38.194960	68.307790
1154.503378	42.221551	68.312794
1153.606407	45.231167	68.317799
1152.911266	45.324359	68.322804
1152.905626	50.534046	68.327809
1152.148550	49.941634	68.332814
1151.776976	51.109337	68.337818
1151.139408	42.967767	68.342823
1150.430803	53.529617	68.347828
1149.619256	41.580467	68.352833
1148.600375	45.265504	68.357838
1147.894971	46.642426	68.362842
1147.290657	42.870152	68.367847
1146.700183	42.386865	68.372852
1145.761077	43.392516	68.377857
1144.910180	44.462988	68.382862
1144.598427	45.818302	68.387866
1144.353000	44.316590	68.392871
1143.700975	55.022411	68.397876
1143.105352	41.840404	68.402881
1142.345307	45.203569	68.407886
1141.499243	43.336910	68.412890
1140.955302	44.522567	68.417895
1139.700199	46.152509	68.422900
1139.144166	40.174228	68.427905
1138.483378	44.292757	68.432910
1138.161558	32.316189	68.437914
1138.273673	33.851671	68.442919
1136.831880	50.983197	68.447924
1136.177026	35.557093	68.452929
1135.777994	51.652262	68.457934
1134.866494	44.519388	68.462938
1133.942491	36.440734	68.467943
1133.063927	49.070246	68.472948
1133.228872	38.334619	68.477953
1132.513938	47.426139	68.482958
1131.727616	42.809164	68.487962
1130.920024	36.847245	68.492967
1130.077071	43.428052	68.497972
1129.873430	46.431476	68.502977
1129.062598	51.613114	68.507982
1127.725264	48.036288	68.512986
1127.603608	39.372685	68.517991
1126.955010	41.272024	68.522996
1126.693243	35.970783	68.528001
1125.314270	35.824237	68.533006
1124.727631	37.753145	68.538010
1124.265981	39.335735	68.543015
1123.807195	44.663230	68.548020
1123.308677	39.931093	68.553025
1122.359790	41.690535	68.558030
1121.824571	37.856816	68.563034
1121.537852	33.691826	68.568039
1120.207525	36.393480	68.573044
1119.645557	33.929693	68.578049
1118.766509	40.585630	68.583054
1118.383930	33.067432	68.588058
1117.536874	29.813187	68.593063
1116.280211	39.717868	68.598068
1115.883181	37.940647	68.603073
1115.397462	48.055450	68.608078
1115.013280	39.250676	68.613082
1114.959157	38.333566	68.618087
1113.985261	33.304880	68.623092
1113.086928	26.955272	68.628097
1112.552753	39.001707	68.633102
1112.052097	36.947649	68.638106
1111.096064	35.349236	68.643111
1110.361780	44.084282	68.648116
1110.041540	36.031028	68.653121
1109.406814	40.659516	68.658126
1108.281060	41.953498	68.663130
1107.426074	42.723427	68.668135
1106.690970	42.162227	68.673140
1106.747461	39.030771	68.678145
1106.017929	36.871192	68.683150
1105.179419	43.784043	68.688154
1104.836188	40.741401	68.693159
1103.993244	46.300322	68.698164
1103.313919	42.696115	68.703169
1102.043955	39.994860	68.708174
1101.810557	39.030572	68.713178
1101.455997	37.623499	68.718183
1100.582098	47.839476	68.723188
1099.765785	33.604472	68.728193
1099.155809	39.968447	68.733198
1098.380516	41.302881	68.738202
1098.525670	35.006490	68.743207
1097.015650	33.652328	68.748212
1096.362351	28.586846	68.753217
1095.986711	33.651949	68.758222
1095.412889	34.374002	68.763226
1094.329931	30.674732	68.768231
1093.562189	35.529390	68.773236
1093.139704	32.631826	68.778241
1092.639317	34.004535	68.783246
1092.229717	38.940998	68.788250
1091.835833	30.634532	68.793255
1090.716844	43.649232	68.798260
1090.328750	30.929418	68.803265
1088.718552	37.894062	68.808270
1088.080125	38.328342	68.813274
1087.856164	31.182322	68.818279
1087.154231	35.220670	68.823284
1086.870745	28.751187	68.828289
1086.299547	35.500088	68.833294
1085.142099	36.608305	68.838298
1084.750519	31.058057	68.843303
1083.922739	41.796566	68.848308
1083.545004	35.786786	68.853313
1082.728924	39.376505	68.858318
1081.556340	40.461899	68.863322
1081.360254	31.502635	68.868327
1080.814788	35.971844	68.873332
1080.566451	34.076356	68.878337
1079.026099	39.810881	68.883342
1078.430018	37.688430	68.888346
1078.076199	38.356564	68.893351
1077.477245	38.729373	68.898356
1077.031539	40.008228	68.903361
1075.882085	45.281594	68.908366
1075.302477	40.597063	68.913370
1074.950955	32.823192	68.918375
1074.133103	41.659848	68.923380
1073.248330	26.961079	68.928385
1072.538167	26.794902	68.933390
1072.087917	37.468621	68.938394
1071.972435	38.176115	68.943399
1070.985577	36.454884	68.948404
1070.258368	35.406727	68.953409
1069.329421	32.979255	68.958414
1068.925999	29.279129	68.963418
1068.205730	29.541926	68.968423
1067.215524	32.312503	68.973428
1066.875891	32.661407	68.978433
1066.487582	37.771108	68.983438
1065.216689	40.089588	68.988442
1064.456634	37.887568	68.993447
1063.845850	39.490738	68.998452
1063.595704	29.814661	69.003457
1062.912148	39.754350	69.008462
1062.905945	42.087685	69.013466
1061.981865	29.252870	69.018471
1061.023263	40.762843	69.023476
1060.408443	42.289384	69.028481
1059.532715	39.500202	69.033486
1058.868784	42.729824	69.038490
1058.582196	39.183003	69.043495
1057.449599	39.653328	69.048500
1056.838124	39.241214	69.053505
1055.885912	41.122637	69.058510
1055.537728	43.283291	69.063514
1055.541484	32.391961	69.068519
1054.097653	38.969027	69.073524
1053.781996	34.113199	69.078529
1052.980431	37.101359	69.083534
1052.105518	35.633570	69.088538
1051.956116	28.095640	69.093543
1050.534745	40.472464	69.098548
1050.318116	35.982514	69.103553
1049.675036	39.380711	69.108558
1049.199490	43.124427	69.113562
1048.036519	31.933001	69.118567
1047.382675	41.090509	69.123572
1047.029596	40.134229	69.128577
1046.641268	42.868987	69.133582
1046.059416	33.690395	69.138586
1045.129855	34.920073	69.143591
1044.212319	44.042263	69.148596
1043.710066	37.318999	69.153601
1043.063170	35.980521	69.158606
1042.102474	40.914778	69.163610
1041.849481	28.156140	69.168615
1040.944462	41.958424	69.173620
1040.970508	36.445823	69.178625
1039.404045	40.142320	69.183630
1038.403899	37.773496	69.188634
1038.293224	34.966688	69.193639
1037.647384	46.357525	69.198644
1037.733942	28.079010	69.203649
1036.655947	33.071353	69.208654
1035.750018	37.116936	69.213658
1035.380027	27.652326	69.218663
1034.875668	33.490139	69.223668
1033.590934	30.491643	69.228673
1032.904188	38.646689	69.233678
1032.277207	41.386301	69.238682
1032.221059	34.265631	69.243687
1030.975108	45.865488	69.248692
1030.423798	34.005885	69.253697
1029.880797	37.523785	69.258702
1029.160618	45.409758	69.263706
1028.835758	30.972019	69.268711
1027.607544	34.384465	69.273716
1027.158060	37.277192	69.278721
1026.409701	32.578523	69.283726
1025.945490	32.314880	69.288730
1025.688269	32.841493	69.293735
1024.443464	40.929207	69.298740
1023.961752	32.395450	69.303745
1023.371328	36.969596	69.308750
1022.537640	40.426512	69.313754
1021.851979	36.455900	69.318759
1020.911107	36.427371	69.323764
1020.703936	36.938137	69.328769
1020.239585	32.566454	69.333774
1019.253872	39.603674	69.338778
1018.728082	32.021550	69.343783
1017.865950	45.063216	69.348788
1017.452620	33.610607	69.353793
1016.615351	36.954550	69.358798
1015.604569	34.171103	69.363802
1015.572138	26.542028	69.368807
1014.608766	37.679022	69.373812
1014.265030	27.040113	69.378817
1013.301173	37.683587	69.383822
1012.695174	46.663177	69.388826
1012.721925	33.240274	69.393831
1010.889426	37.896923	69.398836
1010.453427	37.212468	69.403841
1009.924964	38.701625	69.408846
1009.375999	42.677807	69.413850
1009.206025	35.937956	69.418855
1007.849906	35.836726	69.423860
1007.070549	35.392986	69.428865
1006.488484	45.426929	69.433870
1006.310386	41.060165	69.438874
1005.850547	35.516062	69.443879
1004.472045	43.284428	69.448884
1003.799903	35.739785	69.453889
1003.462978	37.187429	69.458894
1003.088555	35.189006	69.463898
1002.247460	40.730312	69.468903
1001.169812	37.531722	69.473908
1000.588471	42.776226	69.478913
1000.225667	40.580407	69.483918
999.434426	49.510625	69.488922
998.882743	43.998480	69.493927
998.154584	43.092424	69.498932
997.553292	37.583445	69.503937
997.109054	38.885735	69.508942
995.808735	39.524703	69.513946
995.476600	31.880233	69.518951
994.558800	46.238088	69.523956
994.378698	36.856812	69.528961
993.774014	30.921012	69.533966
992.501282	45.097215	69.538970
992.105983	34.393969	69.543975
991.674316	38.417722	69.548980
991.097533	36.815784	69.553985
990.245493	37.929066	69.558990
989.378264	29.761022	69.563994
988.976607	28.705244	69.568999
988.435593	36.908074	69.574004
987.505682	36.762693	69.579009
986.433567	44.608476	69.584014
985.902912	44.585652	69.589018
985.765621	43.035213	69.594023
985.256613	37.549401	69.599028
984.172970	39.904359	69.604033
983.543977	37.323534	69.609038
982.784020	38.128846	69.614042
982.955658	36.253278	69.619047
981.509806	40.186089	69.624052
981.024646	32.755210	69.629057
979.903521	33.561220	69.634062
979.789230	36.925756	69.639066
979.529814	29.104136	69.644071
978.281188	39.871782	69.649076
977.551040	42.142109	69.654081
977.326711	35.204326	69.659086
976.040639	40.624051	69.664090
975.269099	33.574641	69.669095
974.313242	43.679103	69.674100
973.983837	38.188370	69.679105
973.846477	34.896946	69.684110
973.303723	34.022898	69.689114
972.946688	31.267913	69.694119
971.780452	40.271993	69.699124
971.088793	32.724161	69.704129
970.859247	34.329768	69.709134
969.688492	39.649142	69.714138
969.106136	37.932975	69.719143
968.232370	39.868180	69.724148
967.724372	33.571641	69.729153
967.184334	42.903446	69.734158
966.526085	36.941481	69.739162
966.211616	36.176193	69.744167
965.452485	38.356515	69.749172
964.475854	34.698734	69.754177
963.606445	37.528977	69.759182
963.333390	32.407760	69.764186
962.559828	31.633522	69.769191
961.626398	41.426904	69.774196
960.863972	32.489968	69.779201
960.656494	32.358953	69.784206
959.963575	39.846351	69.789210
958.832264	30.256894	69.794215
958.194240	39.668947	69.799220
957.683315	40.346328	69.804225
957.317153	35.954303	69.809230
957.063379	39.522389	69.814234
956.055965	32.909500	69.819239
954.970365	32.982875	69.824244
954.730324	35.003325	69.829249
954.136891	36.501254	69.834254
952.379921	43.391560	69.839258
952.016625	30.951699	69.844263
951.328191	42.265741	69.849268
951.360248	35.697181	69.854273
951.044063	39.447091	69.859278
950.388299	41.013289	69.864282
949.743647	31.959844	69.869287
948.837679	32.566045	69.874292
948.331980	32.827848	69.879297
947.168112	37.313483	69.884302
946.092355	39.343918	69.889306
945.561889	26.845507	69.894311
945.166599	36.827651	69.899316
944.768743	33.309594	69.904321
944.218480	38.394617	69.909326
943.238136	33.135214	69.914330
942.834182	32.035654	69.919335
942.284741	40.233524	69.924340
941.176191	34.254915	69.929345
940.273616	40.982456	69.934350
939.835885	45.740483	69.939354
939.638495	40.927355	69.944359
938.976325	49.176287	69.949364
938.100432	44.684025	69.954369
937.179577	35.048470	69.959374
936.999152	41.796713	69.964378
936.345827	40.388323	69.969383
934.954665	46.015607	69.974388
934.606595	40.382768	69.979393
934.427175	44.369543	69.984398
933.308266	44.867707	69.989402
932.403448	38.926067	69.994407
931.637725	47.024317	69.999412
931.095017	45.707136	70.004417
930.579406	45.562079	70.009422
930.259800	48.356881	70.014426
930.101648	37.514983	70.019431
929.004240	34.671240	70.024436
928.196100	30.691765	70.029441
927.790550	37.043738	70.034446
926.430253	44.467036	70.039450
925.755085	43.320751	70.044455
925.013201	42.054193	70.049460
924.708760	40.517742	70.054465
924.345312	42.701341	70.059470
923.862332	38.479303	70.064474
923.445708	36.170634	70.069479
922.031720	36.838768	70.074484
921.696529	37.819357	70.079489
920.827312	33.310273	70.084494
919.822444	44.968000	70.089498
919.754077	33.462098	70.094503
919.081883	38.413561	70.099508
918.789593	36.491970	70.104513
917.482593	34.075835	70.109518
916.866147	44.604126	70.114522
916.656768	35.654888	70.119527
915.285578	42.983728	70.124532
914.471629	27.437964	70.129537
914.151271	40.740364	70.134542
913.517166	44.520373	70.139546
913.136469	38.113699	70.144551
911.930282	43.832984	70.149556
911.289470	31.714849	70.154561
911.008497	40.609606	70.159566
910.738354	38.063157	70.164570
909.988931	36.543908	70.169575
908.724517	49.195448	70.174580
908.014348	40.989821	70.179585
907.800281	36.680836	70.184590
907.296209	48.982707	70.189594
906.232952	31.916975	70.194599
905.335298	40.840488	70.199604
904.940257	38.818554	70.204609
904.787384	39.268647	70.209614
903.602233	44.886814	70.214618
903.018997	38.712653	70.219623
902.276815	39.944102	70.224628
901.683139	36.559722	70.229633
901.264811	40.037303	70.234638
900.140757	41.905128	70.239642
899.672301	31.945276	70.244647
899.188434	31.680053	70.249652
898.784802	34.630157	70.254657
897.726177	41.065570	70.259662
896.850655	40.749136	70.264666
896.558788	38.877944	70.269671
896.063102	42.259026	70.274676
895.413417	42.455443	70.279681
894.232715	39.588701	70.284686
893.532533	46.780797	70.289690
893.426876	30.959884	70.294695
892.293698	45.505005	70.299700
891.590010	42.503997	70.304705
891.235657	43.452946	70.309710
890.662662	36.119649	70.314714
890.043744	35.051156	70.319719
888.606516	37.303151	70.324724
888.448000	37.019265	70.329729
888.098012	41.919455	70.334734
887.416542	40.670103	70.339738
886.382731	41.916430	70.344743
885.610263	36.406343	70.349748
885.021199	36.074285	70.354753
884.812506	41.057645	70.359758
883.833682	45.302541	70.364762
883.171735	36.851125	70.369767
882.370995	40.063136	70.374772
881.809409	35.361599	70.379777
881.415563	39.699476	70.384782
880.661051	37.439862	70.389786
879.794944	37.918315	70.394791
879.118114	39.631389	70.399796
878.840417	39.934189	70.404801
878.397998	35.946987	70.409806
876.781513	45.562096	70.414810
876.600743	31.221319	70.419815
876.093614	33.426213	70.424820
875.716770	35.615102	70.429825
874.853209	45.315385	70.434830
873.873188	40.928035	70.439834
873.657917	34.799400	70.444839
872.492098	32.007575	70.449844
871.859699	38.454006	70.454849
871.354177	40.111431	70.459854
870.762008	42.093314	70.464858
870.364405	31.688521	70.469863
868.891207	38.472208	70.474868
868.226748	33.313953	70.479873
867.931674	30.807750	70.484878
867.825935	35.005152	70.489882
867.115879	30.667881	70.494887
866.057774	42.884463	70.499892
865.613902	34.332112	70.504897
865.184362	36.961484	70.509902
863.757312	44.040613	70.514906
863.190444	28.217422	70.519911
862.407806	36.449263	70.524916
861.861061	32.347781	70.529921
861.578443	36.434561	70.534926
860.442846	36.415007	70.539930
860.161866	29.334873	70.544935
859.415485	45.961566	70.549940
858.849696	41.563484	70.554945
858.257682	35.942682	70.559950
856.958767	43.857724	70.564954
856.802845	34.113072	70.569959
855.933756	47.400313	70.574964
855.865458	44.531577	70.579969
854.987071	34.058229	70.584974
854.238894	41.656948	70.589978
854.087328	39.589961	70.594983
853.052218	35.110463	70.599988
851.902319	33.904140	70.604993
851.573073	37.922648	70.609998
850.924815	46.199341	70.615002
850.183145	35.902933	70.620007
849.391571	37.304688	70.625012
848.667429	40.800990	70.630017
848.438227	34.740810	70.635022
847.489202	46.348667	70.640026
846.677242	35.222914	70.645031
845.892066	51.163491	70.650036
845.108612	41.539222	70.655041
845.210576	37.618345	70.660046
844.363943	49.260370	70.665050
844.072269	31.750157	70.670055
842.897797	48.028669	70.675060
842.486342	37.635547	70.680065
842.169478	32.235888	70.685070
840.699489	43.915629	70.690074
840.539369	41.801118	70.695079
839.648666	46.413634	70.700084
838.836187	41.107055	70.705089
837.968337	39.655566	70.710094
837.164729	48.846412	70.715098
837.211528	45.349062	70.720103
836.781203	43.715964	70.725108
835.612243	45.529462	70.730113
835.060454	43.646033	70.735118
834.002244	47.080395	70.740122
834.100965	37.511259	70.745127
832.745288	39.933234	70.750132
831.913380	38.685765	70.755137
831.560983	40.623182	70.760142
830.657140	44.133900	70.765146
830.689604	32.569385	70.770151
830.297740	39.086349	70.775156
829.330591	35.526466	70.780161
828.785006	41.033396	70.785166
827.686659	47.648628	70.790170
826.662327	39.546658	70.795175
826.161959	48.534692	70.800180
825.260269	42.012266	70.805185
825.151645	33.874927	70.810190
824.657708	49.879536	70.815194
824.133803	43.041502	70.820199
822.940590	45.776674	70.825204
822.789042	43.734918	70.830209
822.062221	44.673778	70.835214
820.692160	43.630251	70.840218
820.373898	33.599204	70.845223
819.586214	39.911088	70.850228
819.058903	44.467342	70.855233
818.619086	40.549125	70.860238
817.894408	50.061734	70.865242
817.188598	39.679202	70.870247
816.536775	44.911304	70.875252
816.006591	40.810349	70.880257
814.960227	39.541829	70.885262
813.967414	43.388421	70.890266
813.656582	32.670203	70.895271
813.341568	41.319639	70.900276
813.018184	45.898627	70.905281
812.091340	36.051191	70.910286
810.985212	45.346969	70.915290
810.606404	38.988903	70.920295
810.294727	43.211204	70.925300
809.040183	39.788544	70.930305
808.219824	35.525622	70.935310
807.481069	36.050060	70.940314
807.269031	30.144856	70.945319
806.747119	40.859964	70.950324
806.331940	37.515006	70.955329
805.614649	34.691238	70.960334
804.710084	40.791492	70.965338
804.144751	37.902532	70.970343
802.805049	40.757228	70.975348
802.136567	40.313250	70.980353
801.736759	32.930335	70.985358
801.313124	44.281097	70.990362
801.146262	39.422127	70.995367
800.017352	43.664134	71.000372
799.137348	37.422128	71.005377
798.551442	35.960465	71.010382
797.945678	46.600614	71.015386
797.546332	32.953830	71.020391
796.643395	41.009292	71.025396
795.852350	39.589747	71.030401
795.574487	37.293707	71.035406
794.820281	47.061759	71.040410
794.196677	42.575126	71.045415
793.479718	53.611460	71.050420
793.068414	35.148877	71.055425
792.247011	36.954375	71.060430
791.196303	45.642082	71.065434
790.707518	30.446745	71.070439
790.122568	37.516432	71.075444
789.459493	25.252081	71.080449
788.646131	25.450927	71.085454
787.559936	38.323294	71.090458
787.362448	28.408652	71.095463
786.812804	37.831891	71.100468
786.670244	37.739442	71.105473
785.428918	33.841595	71.110478
784.736967	37.449485	71.115482
784.249636	18.846061	71.120487
783.753434	32.916052	71.125492
782.962619	35.601372	71.130497
782.483967	39.834487	71.135502
781.656015	31.806939	71.140506
780.703753	29.156207	71.145511
780.056964	27.639585	71.150516
779.420167	33.317162	71.155521
779.257594	35.027242	71.160526
777.971500	32.071680	71.165530
777.141313	23.751174	71.170535
776.512792	29.935222	71.175540
776.147211	26.629687	71.180545
775.860639	27.044300	71.185550
775.051434	35.332429	71.190554
774.504605	25.678415	71.195559
773.685556	37.727648	71.200564
773.301104	36.355348	71.205569
772.193452	32.920363	71.210574
771.249695	39.809051	71.215578
770.896373	47.100496	71.220583
769.929152	37.455054	71.225588
769.773413	35.648942	71.230593
769.030045	34.169776	71.235598
768.046077	41.854939	71.240602
767.725021	35.003555	71.245607
767.351492	42.534763	71.250612
766.096898	34.813267	71.255617
765.631471	35.841418	71.260622
764.718025	44.007375	71.265626
764.398876	31.797086	71.270631
763.734164	38.945710	71.275636
762.637782	40.876999	71.280641
762.348526	34.857933	71.285646
761.775936	37.644139	71.290650
761.526866	35.239439	71.295655
760.655466	39.897791	71.300660
759.544660	32.091906	71.305665
759.294634	36.104117	71.310670
758.081806	36.530576	71.315674
757.194758	33.303333	71.320679
756.526124	35.283220	71.325684
756.079936	41.939730	71.330689
756.268382	29.680172	71.335694
755.342356	37.154257	71.340698
754.842681	37.415139	71.345703
753.717521	34.063376	71.350708
753.036616	33.575657	71.355713
752.890527	25.239289	71.360718
751.225088	36.190075	71.365722
751.031128	26.591854	71.370727
750.665237	36.260237	71.375732
750.121753	31.607897	71.380737
749.378049	27.695501	71.385742
748.135128	36.022726	71.390746
748.301403	32.534745	71.395751
747.451973	36.897859	71.400756
746.228073	41.235438	71.405761
745.327887	35.704735	71.410766
744.589260	43.981640	71.415770
744.289886	33.507624	71.420775
744.214506	34.631376	71.425780
743.390680	36.205458	71.430785
742.667712	41.236007	71.435790
742.093195	40.863819	71.440794
741.641188	39.663132	71.445799
740.634856	36.259340	71.450804
739.699736	31.626777	71.455809
739.530826	35.566149	71.460814
738.575313	40.138549	71.465818
737.698998	34.479467	71.470823
736.892976	38.278998	71.475828
736.459664	38.541933	71.480833
736.561386	34.248927	71.485838
735.687073	34.876972	71.490842
734.882142	38.901839	71.495847
734.300724	40.973505	71.500852
732.937022	47.727216	71.505857
732.301486	30.738575	71.510862
731.352941	39.709659	71.515866
731.333996	34.704143	71.520871
730.796499	37.216679	71.525876
730.063995	33.234696	71.530881
729.161848	29.593544	71.535886
728.584082	38.568673	71.540890
728.000264	33.776100	71.545895
727.502282	32.240530	71.550900
726.666501	37.196002	71.555905
725.833776	38.148596	71.560910
725.187616	47.847419	71.565914
725.087406	34.526773	71.570919
724.069328	43.523126	71.575924
723.127330	30.259242	71.580929
722.530782	33.629600	71.585934
721.737037	43.140602	71.590938
721.877990	40.151824	71.595943
720.986594	45.103538	71.600948
719.391510	43.652763	71.605953
719.379477	38.717110	71.610958
718.845200	46.340151	71.615962
718.754817	33.017944	71.620967
717.450438	41.258773	71.625972
716.839926	39.162368	71.630977
716.401503	36.724743	71.635982
714.874578	29.420388	71.640986
714.546836	38.467675	71.645991
713.734057	44.647962	71.650996
713.429756	31.823452	71.656001
713.243980	29.746155	71.661006
712.364263	43.744757	71.666010
711.709783	38.865665	71.671015
710.820464	37.668382	71.676020
710.267030	37.169839	71.681025
709.194029	39.032771	71.686030
708.460808	36.309343	71.691034
707.842373	33.260126	71.696039
707.329637	41.169902	71.701044
707.323224	38.259782	71.706049
706.899806	29.251626	71.711054
705.499322	41.308298	71.716058
704.869702	29.808219	71.721063
704.485282	31.156225	71.726068
703.568100	31.951960	71.731073
702.473995	31.772904	71.736078
701.832393	44.027295	71.741082
701.710116	37.513287	71.746087
701.094468	31.525705	71.751092
700.425559	41.150877	71.756097
699.872818	30.367126	71.761102
698.711252	40.080205	71.766106
698.333279	31.686145	71.771111
697.190182	34.511164	71.776116
696.491808	42.936213	71.781121
696.587552	32.779348	71.786126
695.342950	38.168939	71.791130
695.356021	39.213953	71.796135
694.465721	35.943095	71.801140
693.464203	34.443556	71.806145
692.928443	34.546189	71.811150
692.776652	38.668921	71.816154
692.141148	27.494645	71.821159
690.994496	33.923643	71.826164
690.528424	42.510403	71.831169
690.009781	34.052009	71.836174
688.752872	34.621142	71.841178
688.675717	27.322501	71.846183
687.599918	32.439206	71.851188
686.828413	31.489682	71.856193
686.205745	31.281297	71.861198
685.332985	39.335136	71.866202
685.108422	30.380477	71.871207
684.710246	38.396594	71.876212
683.905426	40.221563	71.881217
683.191756	26.673758	71.886222
682.095056	28.191960	71.891226
682.006467	35.124275	71.896231
681.400886	31.994170	71.901236
680.315248	32.267947	71.906241
679.885664	28.390713	71.911246
679.148537	37.400686	71.916250
678.606546	35.250802	71.921255
677.489731	30.732357	71.926260
676.653788	41.347669	71.931265
676.444253	28.859748	71.936270
675.942555	33.855076	71.941274
675.513055	27.391574	71.946279
674.554605	34.602757	71.951284
673.658666	33.261459	71.956289
673.281895	25.010724	71.961294
672.616084	32.623170	71.966298
671.929855	27.790151	71.971303
670.815547	31.951034	71.976308
670.566453	39.128111	71.981313
670.208921	32.109088	71.986318
669.201895	36.123576	71.991322
668.749868	29.116448	71.996327
668.167662	30.942242	72.001332
667.234920	27.788545	72.006337
666.276509	20.152418	72.011342
665.464473	24.394478	72.016346
664.989691	30.192935	72.021351
664.806254	31.488441	72.026356
664.309208	30.119897	72.031361
663.498692	35.175443	72.036366
662.512280	37.778403	72.041370
661.985707	30.959770	72.046375
661.759895	27.054822	72.051380
660.469799	31.197969	72.056385
659.835489	25.259106	72.061390
659.400799	33.552278	72.066394
658.755678	39.043545	72.071399
657.619076	30.044891	72.076404
656.917337	34.572174	72.081409
656.764343	30.040605	72.086414
656.066885	31.805906	72.091418
655.677456	34.132447	72.096423
654.677128	36.833822	72.101428
653.556425	34.161079	72.106433
653.537145	29.062581	72.111438
652.987798	32.633598	72.116442
652.132916	30.027336	72.121447
651.621346	30.283825	72.126452
650.625144	33.594837	72.131457
650.353360	28.728942	72.136462
648.963446	31.208502	72.141466
648.575317	29.735882	72.146471
648.181889	33.195336	72.151476
647.696604	34.546797	72.156481
647.100316	28.098825	72.161486
645.869065	31.281686	72.166490
645.557154	29.599806	72.171495
645.133099	33.001058	72.176500
643.684575	36.991245	72.181505
643.200494	31.585136	72.186510
642.327902	34.215710	72.191514
641.965326	35.571285	72.196519
641.558418	38.414710	72.201524
641.033244	30.838908	72.206529
640.349789	22.662254	72.211534
639.527736	31.159043	72.216538
639.202808	28.152993	72.221543
637.982503	37.783981	72.226548
636.957992	30.847531	72.231553
636.574229	29.626535	72.236558
636.295656	31.372441	72.241562
635.805117	28.353342	72.246567
635.252064	27.733329	72.251572
634.047446	31.618443	72.256577
633.442765	37.976923	72.261582
632.829016	40.110530	72.266586
632.461549	35.901707	72.271591
631.418084	37.919241	72.276596
630.648186	36.868552	72.281601
630.436993	32.578071	72.286606
629.835797	31.820644	72.291610
628.774728	30.180802	72.296615
628.170514	35.246081	72.301620
627.459421	26.291647	72.306625
627.576931	32.656539	72.311630
626.329740	32.992339	72.316634
625.310438	31.926177	72.321639
625.140085	33.924514	72.326644
624.348819	36.802344	72.331649
623.324513	35.285962	72.336654
622.312057	30.695729	72.341658
622.123832	23.222395	72.346663
621.813613	30.208927	72.351668
621.084624	31.690670	72.356673
620.905078	27.179105	72.361678
619.616701	27.436310	72.366682
619.263874	22.165429	72.371687
618.592381	22.049994	72.376692
617.095362	26.213499	72.381697
616.735198	23.394418	72.386702
615.977350	34.568169	72.391706
615.648401	27.826888	72.396711
615.223002	25.349364	72.401716
614.720610	34.828175	72.406721
613.648869	23.513669	72.411726
612.973625	28.503527	72.416730
612.716701	23.539078	72.421735
612.054222	29.018922	72.426740
610.992925	27.931069	72.431745
610.627156	17.522865	72.436750
609.712547	34.565880	72.441754
609.299451	32.061164	72.446759
608.426109	23.143619	72.451764
607.471530	31.385551	72.456769
607.254022	28.665179	72.461774
606.619579	28.875012	72.466778
605.887106	23.986303	72.471783
605.204295	28.110027	72.476788
604.176988	31.355045	72.481793
604.144083	13.459932	72.486798
602.723683	30.004747	72.491802
602.042482	29.233261	72.496807
601.688427	22.794034	72.501812
601.357497	25.920256	72.506817
600.984761	21.770631	72.511822
600.017654	31.107409	72.516826
599.402842	23.925952	72.521831
599.282839	25.876844	72.526836
597.575567	33.000730	72.531841
597.143644	24.386629	72.536846
596.440818	26.688974	72.541850
596.061099	23.847780	72.546855
595.160838	19.298042	72.551860
593.931236	26.878867	72.556865
593.739035	21.773223	72.561870
593.069405	26.456256	72.566874
593.008717	22.788375	72.571879
592.368542	29.925233	72.576884
591.317651	32.502218	72.581889
590.915093	26.502810	72.586894
590.301392	27.609801	72.591898
589.144426	31.741240	72.596903
588.263049	28.379117	72.601908
587.596477	24.752542	72.606913
587.647633	26.920607	72.611918
586.624690	37.378059	72.616922
585.747123	29.506733	72.621927
585.068644	29.073869	72.626932
584.538613	33.521778	72.631937
584.366400	24.166135	72.636942
583.486000	32.377336	72.641946
582.364893	20.665428	72.646951
581.968737	31.019891	72.651956
581.438479	33.351526	72.656961
581.046674	27.206902	72.661966
579.838568	22.228377	72.666970
579.292163	36.030403	72.671975
578.818797	33.314515	72.676980
578.299697	24.952429	72.681985
577.869215	29.731418	72.686990
576.492475	29.460238	72.691994
576.323229	33.587327	72.696999
575.294309	32.171051	72.702004
573.986576	24.000813	72.707009
573.754841	32.387823	72.712014
573.113375	36.659516	72.717018
572.826131	27.580820	72.722023
572.844009	28.755955	72.727028
571.847521	37.695294	72.732033
571.109260	28.232688	72.737038
570.176634	30.852346	72.742042
569.715915	30.080443	72.747047
568.626621	29.173691	72.752052
567.986421	29.086401	72.757057
567.783203	25.865431	72.762062
567.165423	28.974268	72.767066
565.854723	24.179251	72.772071
565.417107	27.439167	72.777076
564.891897	26.554533	72.782081
564.346417	20.464357	72.787086
563.454846	32.168780	72.792090
562.745519	22.905003	72.797095
562.360016	31.447395	72.802100
561.667163	37.485611	72.807105
560.879784	26.974255	72.812110
560.215127	33.652965	72.817114
559.441071	20.307231	72.822119
559.408219	27.125002	72.827124
558.218598	26.010303	72.832129
557.411548	29.232871	72.837134
556.966196	31.869536	72.842138
556.382361	23.872590	72.847143
556.069343	27.890113	72.852148
554.607071	25.021086	72.857153
554.261958	34.944791	72.862158
553.588120	28.953909	72.867162
553.128353	39.208122	72.872167
551.999982	33.305410	72.877172
551.154487	29.193250	72.882177
550.929788	23.879895	72.887182
550.514141	37.273158	72.892186
550.054002	27.671640	72.897191
549.197199	28.945100	72.902196
548.308198	33.186840	72.907201
547.978169	27.090732	72.912206
546.796102	28.304038	72.917210
546.011578	29.696875	72.922215
545.310595	28.362419	72.927220
544.751882	30.056761	72.932225
544.402764	21.935698	72.937230
544.067885	22.583539	72.942234
543.403247	28.117358	72.947239
542.489207	34.439974	72.952244
541.732638	39.333993	72.957249
541.118548	27.740040	72.962254
540.041067	32.808181	72.967258
539.389741	27.488667	72.972263
539.103659	27.285051	72.977268
538.428648	33.091766	72.982273
537.912813	28.064489	72.987278
537.158273	38.592744	72.992282
536.092502	27.821387	72.997287
535.873001	27.053644	73.002292
535.260617	35.204819	73.007297
534.722885	25.604628	73.012302
533.493099	34.898114	73.017306
532.973469	32.553889	73.022311
532.845365	27.051680	73.027316
532.169146	36.592884	73.032321
531.259213	32.472071	73.037326
530.522093	31.520274	73.042330
530.059900	31.324213	73.047335
528.772682	32.969024	73.052340
527.912845	35.944539	73.057345
527.756327	22.114085	73.062350
527.021197	36.129108	73.067354
526.832022	28.441468	73.072359
526.595303	21.589321	73.077364
525.445322	33.901054	73.082369
524.729229	25.283355	73.087374
523.781456	34.612346	73.092378
522.965538	25.573724	73.097383
522.403634	21.094697	73.102388
521.651596	36.008139	73.107393
521.567748	21.046453	73.112398
521.081988	23.172310	73.117402
520.006349	30.638753	73.122407
519.274242	31.468151	73.127412
518.681218	42.590436	73.132417
517.978557	26.675476	73.137422
516.832592	25.582229	73.142426
516.586014	26.884648	73.147431
516.031360	20.128883	73.152436
515.639170	30.331327	73.157441
514.692337	21.614770	73.162446
513.481417	26.737293	73.167450
513.155636	19.285892	73.172455
512.842655	22.776699	73.177460
512.173627	29.618542	73.182465
511.632419	21.707862	73.187470
510.242572	26.204444	73.192474
509.929473	29.264756	73.197479
509.720704	33.347679	73.202484
508.875002	36.134865	73.207489
508.152872	28.128423	73.212494
507.182143	30.935526	73.217498
507.110535	20.967772	73.222503
505.991002	28.866997	73.227508
505.008977	27.764985	73.232513
504.928783	22.141606	73.237518
504.293008	29.418131	73.242522
503.725572	22.295392	73.247527
502.690724	23.256603	73.252532
501.993570	29.454789	73.257537
501.643351	16.360115	73.262542
500.641861	22.513740	73.267546
499.586610	24.091648	73.272551
499.233056	22.249264	73.277556
498.593564	27.149870	73.282561
498.432944	22.682616	73.287566
497.735620	32.268186	73.292570
496.765702	31.481222	73.297575
496.193172	31.506175	73.302580
495.649388	33.784787	73.307585
495.277959	27.472930	73.312590
493.977324	32.608179	73.317594
493.554441	25.033474	73.322599
493.189358	26.446239	73.327604
491.773338	35.600674	73.332609
491.223069	25.448974	73.337614
490.349177	35.838552	73.342618
489.859424	39.228215	73.347623
489.673034	30.494597	73.352628
489.556596	35.234607	73.357633
488.670051	22.102371	73.362638
487.803844	32.014474	73.367642
487.058083	22.225089	73.372647
486.128362	25.020934	73.377652
485.281715	20.174112	73.382657
485.217556	19.364280	73.387662
484.442081	29.859603	73.392666
483.645646	28.794266	73.397671
482.806375	26.412667	73.402676
481.795941	28.994287	73.407681
481.831791	23.964291	73.412686
481.471161	31.055057	73.417690
480.038827	31.686935	73.422695
479.747242	24.536025	73.427700
478.915490	36.792345	73.432705
478.549452	24.237942	73.437710
477.288466	35.143364	73.442714
476.745304	28.548206	73.447719
476.451272	25.114630	73.452724
475.701017	33.368204	73.457729
475.262493	22.347139	73.462734
473.997626	31.751893	73.467738
473.397587	23.470545	73.472743
473.088242	24.682041	73.477748
472.655892	28.455227	73.482753
472.118564	19.236626	73.487758
470.967902	25.221636	73.492762
470.440549	33.701478	73.497767
470.083825	30.586978	73.502772
468.734777	26.507768	73.507777
468.528167	23.082343	73.512782
467.883234	28.396992	73.517786
467.294202	27.614013	73.522791
466.259244	16.781022	73.527796
465.443559	28.333023	73.532801
464.855216	16.001709	73.537806
464.229059	18.268217	73.542810
464.102932	20.391979	73.547815
463.474407	21.299508	73.552820
462.443548	26.577872	73.557825
462.252244	22.872461	73.562830
461.232661	19.123971	73.567834
460.132665	24.596280	73.572839
459.667042	20.056198	73.577844
458.863248	30.358917	73.582849
458.771711	27.112281	73.587854
458.081908	22.510143	73.592858
457.020582	26.361466	73.597863
456.474136	21.151429	73.602868
455.825177	20.895250	73.607873
455.505845	24.921671	73.612878
454.332887	25.914369	73.617882
453.777601	22.356839	73.622887
453.467353	24.385356	73.627892
452.687986	29.290912	73.632897
451.889903	24.813263	73.637902
451.200524	27.047269	73.642906
450.232615	22.478406	73.647911
450.082804	30.805053	73.652916
449.434678	37.375494	73.657921
448.706408	29.250202	73.662926
447.713739	30.047018	73.667930
447.462846	23.223951	73.672935
446.813779	24.432806	73.677940
445.453748	34.866734	73.682945
445.365249	27.650354	73.687950
444.582622	27.664639	73.692954
444.061442	33.749644	73.697959
443.618568	30.711955	73.702964
442.493165	31.580384	73.707969
442.027777	19.350913	73.712974
441.559658	23.636012	73.717978
440.655502	20.337503	73.722983
439.892486	24.709013	73.727988
439.207102	32.736212	73.732993
439.129402	22.775746	73.737998
437.987233	25.592842	73.743002
437.034798	26.801150	73.748007
436.531042	19.521628	73.753012
435.647060	25.924639	73.758017
435.857977	19.199884	73.763022
435.228199	22.203425	73.768026
433.958052	18.510642	73.773031
433.573518	21.792080	73.778036
432.863132	18.871138	73.783041
431.662950	18.715412	73.788046
431.077937	31.878611	73.793050
430.419885	24.544824	73.798055
430.253728	26.115138	73.803060
429.922787	26.786021	73.808065
429.112354	23.281769	73.813070
428.036145	28.368672	73.818074
427.580159	27.334264	73.823079
427.223919	28.606855	73.828084
425.569729	30.300729	73.833089
425.368225	26.043427	73.838094
424.959484	21.494289	73.843098
424.310381	30.961799	73.848103
423.578430	24.904527	73.853108
422.537025	29.292016	73.858113
422.303764	24.284402	73.863118
421.740816	26.346880	73.868122
420.690139	15.726157	73.873127
420.062430	20.650132	73.878132
419.244949	27.293292	73.883137
418.829708	18.391152	73.888142
418.686907	23.570604	73.893146
417.772567	20.466119	73.898151
417.317495	18.717197	73.903156
416.303176	24.824009	73.908161
415.540663	21.834106	73.913166
414.352356	31.753396	73.918170
413.910843	28.037395	73.923175
413.770845	24.027342	73.928180
413.384799	26.593076	73.933185
412.480201	28.577530	73.938190
411.764381	30.344243	73.943194
410.930198	28.963241	73.948199
410.597032	19.466119	73.953204
409.032333	27.532509	73.958209
408.830678	24.159919	73.963214
408.184810	28.840784	73.968218
407.655889	36.346310	73.973223
407.401106	27.489563	73.978228
406.031764	26.021948	73.983233
405.672767	31.555980	73.988238
405.216204	35.840823	73.993242
404.521616	31.474433	73.998247
403.681538	20.536301	74.003252
402.531349	31.003041	74.008257
401.992866	25.192496	74.013262
401.425962	25.953024	74.018266
401.449990	31.383443	74.023271
401.139873	19.783690	74.028276
399.693325	28.378470	74.033281
399.354259	17.966066	74.038286
398.310601	29.139663	74.043290
397.487488	29.048449	74.048295
396.887664	18.478898	74.053300
396.461498	26.234556	74.058305
395.992935	26.479512	74.063310
395.017382	29.137610	74.068314
394.297627	26.489412	74.073319
394.184362	24.066274	74.078324
393.489574	27.512277	74.083329
392.613354	26.284639	74.088334
391.719351	29.123712	74.093338
390.893130	29.472972	74.098343
390.961874	30.856044	74.103348
389.463930	31.512622	74.108353
389.079851	21.922690	74.113358
388.537610	23.743751	74.118362
388.015255	27.600677	74.123367
386.898699	26.890742	74.128372
385.922982	32.370087	74.133377
385.513405	32.359636	74.138382
385.099251	31.246029	74.143386
384.798730	23.099911	74.148391
384.566654	28.146932	74.153396
383.284547	28.445838	74.158401
382.639761	28.576951	74.163406
382.097037	24.984321	74.168410
381.109338	23.930574	74.173415
380.431182	14.027962	74.178420
379.617232	32.376482	74.183425
379.448507	23.088130	74.188430
378.653764	25.332637	74.193434
377.604751	30.632849	74.198439
377.068494	24.692645	74.203444
376.520471	31.635082	74.208449
376.227008	31.997220	74.213454
375.655690	27.237453	74.218458
374.759564	31.606540	74.223463
373.987813	24.412319	74.228468
373.424169	34.014456	74.233473
372.457785	31.681538	74.238478
371.952832	30.910415	74.243482
371.541474	35.516070	74.248487
371.240480	29.989390	74.253492
369.651935	27.866012	74.258497
369.260883	22.743200	74.263502
368.920457	23.166441	74.268506
368.226097	28.630914	74.273511
366.939298	16.481909	74.278516
366.216686	28.282453	74.283521
365.632401	30.247417	74.288526
365.610751	26.956534	74.293530
365.145011	29.266888	74.298535
364.324266	27.128388	74.303540
363.189257	34.263723	74.308545
362.884056	24.008356	74.313550
362.389312	27.610147	74.318554
361.442210	25.863952	74.323559
360.587564	20.706213	74.328564
360.112156	22.850948	74.333569
359.785426	28.528077	74.338574
358.548212	26.090091	74.343578
357.875830	28.015479	74.348583
357.429807	24.609298	74.353588
356.904468	33.784279	74.358593
355.990179	28.757472	74.363598
354.953475	27.418227	74.368602
354.226453	29.300283	74.373607
354.161987	30.285106	74.378612
353.312397	32.994110	74.383617
353.108349	19.768946	74.388622
352.626478	21.233457	74.393626
351.602825	24.274557	74.398631
351.000555	7.828024	74.403636
350.560936	22.578143	74.408641
349.676344	15.901822	74.413646
348.886091	22.736204	74.418650
348.197189	20.704434	74.423655
347.493880	15.153571	74.428660
346.184033	12.873829	74.433665
345.578487	16.266194	74.438670
345.402065	18.087310	74.443674
344.922441	26.081731	74.448679
344.858274	21.673240	74.453684
343.744802	26.718804	74.458689
342.892031	21.362074	74.463694
342.425639	12.412916	74.468698
341.853218	24.378761	74.473703
340.913100	14.740266	74.478708
339.746029	23.140719	74.483713
339.410982	17.999528	74.488718
338.909898	25.770285	74.493722
339.016212	22.742866	74.498727
338.013088	16.473377	74.503732
337.120880	25.790405	74.508737
336.695156	20.171648	74.513742
335.326378	25.726267	74.518746
334.420284	18.394201	74.523751
334.182285	21.414173	74.528756
333.406845	20.777633	74.533761
333.280561	28.884479	74.538766
332.784458	22.959966	74.543770
331.643334	21.210014	74.548775
330.981122	24.620877	74.553780
330.550868	31.459394	74.558785
329.895066	13.419184	74.563790
328.913753	28.610464	74.568794
328.170045	23.835608	74.573799
327.951224	19.451768	74.578804
326.934606	28.189378	74.583809
326.113632	18.090345	74.588814
325.628658	29.346812	74.593818
325.322368	35.090074	74.598823
325.130507	20.776435	74.603828
323.618200	31.925400	74.608833
322.991026	25.583379	74.613838
322.559681	29.167188	74.618842
321.592780	23.836540	74.623847
320.951897	24.678263	74.628852
320.203940	29.498421	74.633857
319.848943	29.310546	74.638862
319.675364	24.402246	74.643866
318.803591	30.756038	74.648871
317.821818	19.562982	74.653876
317.450309	32.039294	74.658881
316.649900	31.051918	74.663886
315.563746	24.727860	74.668890
314.761832	29.127681	74.673895
314.149477	20.793157	74.678900
313.958826	22.597619	74.683905
313.618557	20.519756	74.688910
312.434000	28.568189	74.693914
311.500942	24.613584	74.698919
311.513489	17.120918	74.703924
310.963564	24.251325	74.708929
309.850130	20.385396	74.713934
309.366847	28.547565	74.718938
308.722680	27.651985	74.723943
308.342205	22.842897	74.728948
307.182264	28.279088	74.733953
306.516559	20.471896	74.738958
306.037789	17.485693	74.743962
304.637114	16.821081	74.748967
304.210970	16.321268	74.753972
303.337927	16.712713	74.758977
303.237827	9.912953	74.763982
303.098108	17.399027	74.768986
302.466282	18.248774	74.773991
301.101286	13.030477	74.778996
300.478761	19.581089	74.784001
299.789076	15.396886	74.789006
299.542971	19.663963	74.794010
298.934649	23.249173	74.799015
298.312245	15.414584	74.804020
297.432756	18.831700	74.809025
296.672728	11.230365	74.814030
295.774775	12.970944	74.819034
294.888022	22.473194	74.824039
294.513639	13.436843	74.829044
294.091851	14.420272	74.834049
293.831409	10.139269	74.839054
292.573499	20.187964	74.844058
291.780850	21.262046	74.849063
291.382569	18.162090	74.854068
290.954706	22.801920	74.859073
290.336540	12.311031	74.864078
289.334869	16.747427	74.869082
288.373982	21.205709	74.874087
288.291163	9.870965	74.879092
287.683123	19.286212	74.884097
287.008940	20.760888	74.889102
286.089168	13.011551	74.894106
285.301482	14.039111	74.899111
285.195946	13.024567	74.904116
284.031916	23.717479	74.909121
282.991089	12.770407	74.914126
282.678591	21.264902	74.919130
282.214681	24.320887	74.924135
282.152418	10.894949	74.929140
280.751340	27.282263	74.934145
280.610717	12.687658	74.939150
279.843938	14.222827	74.944154
278.294113	13.142030	74.949159
277.880751	15.649054	74.954164
277.226165	21.495141	74.959169
276.796234	26.245693	74.964174
276.647678	28.622199	74.969178
275.465758	24.507002	74.974183
274.895492	16.943234	74.979188
273.863173	24.729290	74.984193
273.798420	19.407829	74.989198
273.066102	25.643207	74.994202
271.775148	21.159034	74.999207
271.436863	11.292177	75.004212
271.006693	18.903398	75.009217
270.590667	14.355458	75.014222
269.546014	28.519198	75.019226
268.919557	18.997897	75.024231
268.398198	14.619714	75.029236
267.979394	14.293782	75.034241
266.899831	16.495411	75.039246
266.078321	17.031622	75.044250
265.122568	18.904430	75.049255
265.101401	24.176458	75.054260
264.535371	24.473246	75.059265
263.443061	27.490631	75.064270
262.707632	18.749960	75.069274
262.322055	33.608174	75.074279
262.066135	18.860055	75.079284
260.988818	36.886296	75.084289
260.341717	20.391739	75.089294
259.707180	25.031403	75.094298
259.637655	25.715831	75.099303
258.616141	29.661811	75.104308
257.065516	28.306759	75.109313
257.020201	28.149953	75.114318
256.639858	29.539950	75.119322
256.080978	29.562783	75.124327
255.462655	21.405851	75.129332
254.359762	28.209670	75.134337
253.761851	24.359363	75.139342
252.755842	17.855404	75.144346
251.897426	29.333834	75.149351
251.637161	16.876184	75.154356
251.009245	25.138685	75.159361
250.616846	22.577124	75.164366
250.149699	30.703612	75.169370
248.609369	28.105843	75.174375
248.493394	20.089612	75.179380
247.845917	27.737058	75.184385
247.587936	26.658506	75.189390
246.351835	34.584295	75.194394
245.604964	24.784146	75.199399
245.804467	26.885968	75.204404
244.481678	27.163046	75.209409
243.801744	21.613221	75.214414
243.033643	30.409013	75.219418
242.323564	27.912289	75.224423
242.382887	19.357173	75.229428
240.883140	33.252847	75.234433
240.345266	17.609804	75.239438
239.966837	19.259699	75.244442
239.673358	28.123334	75.249447
238.779755	17.663752	75.254452
237.598164	30.849530	75.259457
237.216876	15.837551	75.264462
237.050755	14.618199	75.269466
235.896637	27.596166	75.274471
235.458179	12.717885	75.279476
234.782140	25.428822	75.284481
233.943561	24.321402	75.289486
232.716792	23.236441	75.294490
232.116203	27.295103	75.299495
231.701114	18.419797	75.304500
231.173827	22.624470	75.309505
231.232106	18.116043	75.314510
230.332775	26.305120	75.319514
229.055513	22.697164	75.324519
229.037680	30.957032	75.329524
227.941126	26.627974	75.334529
227.350912	26.118060	75.339534
226.578704	22.125233	75.344538
225.500314	22.429592	75.349543
225.707232	20.046888	75.354548
224.951030	30.118137	75.359553
224.444982	23.185974	75.364558
223.708310	32.095034	75.369562
222.763668	33.644385	75.374567
221.787743	17.121845	75.379572
220.809648	32.314217	75.384577
220.479155	32.456769	75.389582
220.289438	21.925980	75.394586
219.547751	26.111218	75.399591
218.863911	19.256289	75.404596
217.812529	33.093109	75.409601
217.482196	25.592030	75.414606
217.190060	17.048794	75.419610
216.108546	24.670821	75.424615
215.502971	25.275127	75.429620
215.034155	31.168886	75.434625
214.269562	20.687170	75.439630
213.158672	29.613313	75.444634
212.255066	32.105464	75.449639
212.307599	22.701441	75.454644
211.502193	29.606086	75.459649
211.298771	31.210738	75.464654
210.117854	26.440970	75.469658
209.188834	32.879615	75.474663
208.974586	23.713669	75.479668
208.318396	24.461666	75.484673
206.974430	25.877562	75.489678
206.848856	28.136864	75.494682
206.074351	31.508889	75.499687
205.843302	19.393525	75.504692
205.327956	27.893558	75.509697
204.253701	27.129654	75.514702
203.659381	20.643663	75.519706
202.652874	25.960816	75.524711
202.269427	24.872309	75.529716
201.096434	29.216204	75.534721
200.516311	24.711784	75.539726
200.095556	31.982468	75.544730
199.482790	28.766911	75.549735
199.459060	21.259535	75.554740
198.415904	26.563609	75.559745
197.668839	27.961618	75.564750
197.604567	26.292362	75.569754
196.476284	32.130412	75.574759
195.482390	25.829553	75.579764
194.492415	24.719475	75.584769
194.628690	19.361240	75.589774
193.851419	17.148062	75.594778
192.520646	29.671654	75.599783
191.971665	22.506645	75.604788
191.240953	27.590595	75.609793
191.133731	24.300748	75.614798
190.864214	33.453884	75.619802
189.802820	26.965090	75.624807
189.413577	18.656540	75.629812
188.352686	34.891888	75.634817
187.584093	26.993904	75.639822
187.177212	24.422049	75.644826
186.177452	28.347240	75.649831
185.847474	22.897759	75.654836
185.313222	37.923185	75.659841
183.859216	32.253937	75.664846
183.556372	25.224730	75.669850
183.248821	27.800056	75.674855
182.867970	22.861742	75.679860
181.454744	34.493306	75.684865
180.628455	25.144245	75.689870
180.346957	27.778496	75.694874
179.662102	31.409052	75.699879
179.645596	16.666941	75.704884
178.564165	35.729929	75.709889
177.714774	34.239469	75.714894
177.445055	30.152348	75.719898
176.593365	33.390029	75.724903
175.789878	31.531124	75.729908
174.846263	34.501184	75.734913
174.032900	27.860885	75.739918
174.089373	28.523649	75.744922
173.461066	28.037168	75.749927
172.597883	30.201185	75.754932
171.855825	35.343722	75.759937
171.203285	30.833509	75.764942
170.854454	30.539015	75.769946
169.557163	24.783290	75.774951
168.997705	31.164600	75.779956
168.125609	38.231282	75.784961
168.200220	26.228037	75.789966
167.744453	20.006975	75.794970
166.474679	26.946246	75.799975
166.099897	23.998687	75.804980
165.373621	27.512846	75.809985
164.066894	25.019814	75.814990
163.739169	28.588699	75.819994
163.151026	26.599268	75.824999
163.329005	25.930614	75.830004
161.896746	30.894615	75.835009
160.769761	27.805214	75.840014
160.594955	28.154765	75.845018
159.751518	26.458356	75.850023
159.536202	22.739464	75.855028
158.945102	28.961814	75.860033
157.912758	25.765860	75.865038
157.540375	25.396275	75.870042
156.872606	24.305801	75.875047
155.924639	30.364278	75.880052
154.794807	30.429285	75.885057
154.550731	25.841334	75.890062
154.236089	23.205891	75.895066
153.620501	20.877058	75.900071
152.766886	21.084107	75.905076
151.756994	25.927148	75.910081
151.344511	23.360924	75.915086
151.040775	28.909819	75.920090
149.857802	24.348573	75.925095
149.260107	27.045860	75.930100
148.628958	21.161855	75.935105
148.289494	27.754096	75.940110
147.785027	20.099450	75.945114
146.706225	19.508187	75.950119
146.157294	19.959973	75.955124
145.682442	26.717307	75.960129
144.878027	20.368914	75.965134
144.187888	21.163342	75.970138
143.510158	24.152517	75.975143
143.276755	20.710904	75.980148
142.107239	25.498976	75.985153
141.415657	29.736171	75.990158
140.822574	27.969886	75.995162
140.278483	27.299672	76.000167
139.073514	15.461050	76.005172
138.254012	18.449177	76.010177
137.836898	24.199079	76.015182
137.778337	21.328838	76.020186
137.190531	30.113250	76.025191
136.439503	18.271631	76.030196
135.571774	25.211462	76.035201
134.960255	27.958267	76.040206
134.423288	15.294030	76.045210
133.120943	22.665867	76.050215
132.714233	22.552498	76.055220
132.085751	25.092270	76.060225
131.634444	23.412192	76.065230
131.578086	22.148537	76.070234
129.905031	28.234332	76.075239
129.686595	19.436506	76.080244
129.082169	18.884727	76.085249
128.003187	28.669993	76.090254
127.594971	18.514693	76.095258
126.189011	21.241521	76.100263
126.369643	18.949736	76.105268
125.825769	25.445261	76.110273
125.479938	24.486389	76.115278
124.521453	19.652814	76.120282
123.500762	26.361571	76.125287
123.466753	19.636445	76.130292
122.261392	28.374253	76.135297
121.679195	21.353337	76.140302
121.089714	21.669666	76.145306
120.191461	21.920115	76.150311
119.416378	19.507914	76.155316
118.493668	29.670392	76.160321
118.228496	23.813192	76.165326
117.658452	25.566200	76.170330
117.329965	36.630574	76.175335
116.618810	27.506034	76.180340
115.467637	29.540950	76.185345
115.035406	22.497698	76.190350
114.655602	17.500885	76.195354
113.474933	25.980865	76.200359
112.989367	18.280638	76.205364
112.208960	20.295853	76.210369
111.791374	19.473007	76.215374
111.596762	16.597656	76.220378
110.275151	23.865342	76.225383
109.732391	21.364056	76.230388
109.308057	25.839342	76.235393
108.456021	17.905815	76.240398
107.526939	21.786646	76.245402
106.651544	24.573960	76.250407
106.479867	22.757830	76.255412
106.272037	21.404789	76.260417
105.298051	18.043434	76.265422
104.607812	18.062018	76.270426
103.845138	22.908230	76.275431
103.392701	14.442623	76.280436
102.084790	23.292985	76.285441
101.328208	22.634589	76.290446
101.182788	20.546187	76.295450
100.461198	19.956329	76.300455
99.831616	25.623422	76.305460
99.493872	23.622462	76.310465
98.587988	28.245507	76.315470
98.078722	17.035565	76.320474
97.547594	25.375698	76.325479
96.674911	17.980063	76.330484
95.501523	28.009056	76.335489
94.892431	24.884408	76.340494
94.832043	24.812011	76.345498
94.231424	24.901462	76.350503
93.609990	17.032094	76.355508
92.334589	28.610174	76.360513
91.619355	32.039012	76.365518
91.295216	30.439588	76.370522
90.228230	33.612281	76.375527
89.937475	17.229712	76.380532
89.052995	20.376452	76.385537
88.781040	24.885787	76.390542
88.420720	27.508962	76.395546
87.327190	26.500600	76.400551
86.876441	26.670232	76.405556
86.342655	20.589368	76.410561
85.173751	32.599908	76.415566
84.543000	22.866464	76.420570
83.482687	32.055828	76.425575
83.661597	27.349966	76.430580
83.029920	31.372616	76.435585
81.974904	31.318491	76.440590
81.223050	21.199081	76.445594
80.602034	27.599682	76.450599
80.345770	23.169807	76.455604
79.124241	34.770845	76.460609
78.170004	30.171579	76.465614
77.997931	29.011536	76.470618
77.237783	36.427824	76.475623
77.171321	29.526521	76.480628
76.528708	34.120204	76.485633
75.579073	27.512717	76.490638
75.250099	19.721293	76.495642
73.812796	37.440710	76.500647
72.771315	26.861281	76.505652
72.296448	26.623173	76.510657
71.908996	17.355568	76.515662
71.528699	20.696298	76.520666
71.302001	30.733594	76.525671
70.424558	20.935421	76.530676
69.580582	34.485312	76.535681
68.796434	20.334005	76.540686
68.384353	23.716076	76.545690
67.144897	26.853204	76.550695
66.653469	20.885440	76.555700
66.110027	29.555553	76.560705
65.525218	24.395899	76.565710
65.189408	23.296664	76.570714
64.321472	41.112943	76.575719
63.866721	21.547389	76.580724
62.847142	23.561340	76.585729
61.735972	33.552040	76.590734
61.290422	37.081380	76.595738
60.687505	29.770466	76.600743
60.459433	23.407459	76.605748
59.913551	35.813815	76.610753
58.718761	28.157323	76.615758
58.015451	17.490858	76.620762
57.292655	36.353172	76.625767
57.466338	29.643809	76.630772
56.303496	25.442105	76.635777
55.332226	25.918691	76.640782
54.982092	23.115457	76.645786
54.541211	30.709489	76.650791
54.077139	24.084497	76.655796
52.981926	27.282206	76.660801
52.573861	29.588144	76.665806
51.869282	15.957176	76.670810
50.419578	25.694358	76.675815
50.052714	29.750473	76.680820
49.917099	30.166322	76.685825
49.252263	27.908451	76.690830
48.462415	33.679967	76.695834
47.080618	35.594000	76.700839
46.872970	22.998691	76.705844
46.240772	28.071694	76.710849
45.790203	36.813735	76.715854
45.478157	20.759428	76.720858
44.278231	30.951948	76.725863
43.779380	30.189384	76.730868
43.284145	26.417378	76.735873
42.215262	29.338077	76.740878
41.341430	29.165184	76.745882
40.679709	38.290992	76.750887
40.909828	32.410000	76.755892
40.387494	25.295979	76.760897
39.229778	23.422657	76.765902
38.372892	29.681112	76.770906
37.717268	29.591690	76.775911
37.244010	22.168643	76.780916
36.206350	25.972199	76.785921
35.544933	32.208942	76.790926
35.136655	34.915468	76.795930
34.805326	30.844504	76.800935
34.281018	24.289050	76.805940
33.396550	26.737209	76.810945
32.530782	30.470772	76.815950
31.572272	26.678043	76.820954
30.535572	30.328483	76.825959
30.131969	23.507769	76.830964
29.831004	26.499957	76.835969
29.411779	27.314285	76.840974
29.182020	24.821443	76.845978
27.637353	29.529051	76.850983
27.147528	12.716205	76.855988
26.525563	29.565984	76.860993
25.943446	20.588062	76.865998
25.142118	25.454653	76.871002
24.271715	30.124104	76.876007
23.972002	27.536763	76.881012
23.484845	19.040443	76.886017
22.437387	18.111496	76.891022
22.153106	20.523850	76.896026
21.459621	27.339726	76.901031
20.705466	24.922644	76.906036
19.678213	29.189754	76.911041
18.956436	20.907478	76.916046
18.547629	20.792886	76.921050
18.064805	21.797134	76.926055
17.781384	25.388928	76.931060
16.615403	23.997911	76.936065
15.706959	24.705768	76.941070
15.586764	25.248471	76.946074
14.808419	34.861244	76.951079
13.874417	27.435998	76.956084
13.058268	27.727006	76.961089
12.464273	29.434972	76.966094
12.200658	27.706056	76.971098
11.415620	30.218788	76.976103
10.435298	18.995701	76.981108
9.690741	23.101025	76.986113
9.060333	28.192674	76.991118
9.222037	12.401869	76.996122
8.387072	20.274805	77.001127
7.803142	24.032806	77.006132
7.089350	24.720656	77.011137
5.929447	24.129778	77.016142
5.028362	22.431582	77.021147
4.417224	29.196480	77.026151
4.117819	20.044159	77.031156
3.891535	24.688142	77.036161