Fri Mar 05 18:32:09 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.384465	96.461784	0.000000
-1.603180	87.436951	0.005005
-2.302409	58.858601	0.010010
-4.130964	11.795441	0.015014
-8.335923	5.137986	0.020019
-14.316158	4.249974	0.025024
-18.642240	10.136126	0.030029
-23.380706	19.385507	0.035034
-27.593214	4.112743	0.040038
-31.453254	13.728222	0.045043
-34.262990	5.925733	0.050048
-37.929204	13.225280	0.055053
-41.763242	12.259913	0.060058
-45.484274	16.597212	0.065062
-49.484576	15.060710	0.070067
-53.402070	17.723082	0.075072
-57.199822	14.242998	0.080077
-60.742188	16.112251	0.085082
-64.150853	6.676987	0.090086
-68.426763	22.826007	0.095091
-72.295903	6.084009	0.100096
-75.593159	15.709123	0.105101
-79.527190	16.226348	0.110106
-83.120518	8.667199	0.115110
-86.980492	18.134518	0.120115
-90.428299	9.840952	0.125120
-94.251627	3.553281	0.130125
-98.430778	26.184011	0.135130
-102.125071	5.949575	0.140134
-105.566523	20.670832	0.145139
-109.828009	9.567648	0.150144
-113.376946	13.639469	0.155149
-116.923052	17.262985	0.160154
-120.987821	10.633828	0.165158
-124.839601	10.571872	0.170163
-128.553507	7.605232	0.175168
-131.914853	1.811621	0.180173
-135.886728	14.111745	0.185178
-139.230412	6.484468	0.190182
-143.335212	8.546083	0.195187
-147.448097	-1.598283	0.200192
-151.262657	3.484227	0.205197
-155.376578	6.370492	0.210202
-158.905791	3.336584	0.215206
-162.786910	11.186267	0.220211
-166.543798	13.335910	0.225216
-169.886171	6.120056	0.230221
-173.562679	12.457915	0.235226
-177.028034	8.267390	0.240230
-180.908600	12.379609	0.245235
-184.604812	14.535367	0.250240
-188.383667	12.708290	0.255245
-192.372083	24.276283	0.260250
-196.130963	10.995691	0.265254
-200.404474	18.800820	0.270259
-203.770115	14.868811	0.275264
-207.620357	11.167109	0.280269
-211.549146	23.178203	0.285274
-214.595578	2.840579	0.290278
-218.769162	19.025543	0.295283
-222.996836	6.513681	0.300288
-226.120615	-2.149930	0.305293
-230.124997	20.538250	0.310298
-233.869991	8.772548	0.315302
-237.466950	11.783028	0.320307
-241.180547	15.564341	0.325312
-244.981314	18.583707	0.330317
-249.083480	20.353341	0.335322
-252.609588	10.219586	0.340326
-256.412663	17.230630	0.345331
-259.982110	12.724101	0.350336
-263.711313	6.628268	0.355341
-267.848071	18.592210	0.360346
-271.559102	11.151492	0.365350
-275.642143	14.734779	0.370355
-279.102381	10.512048	0.375360
-282.468643	8.076791	0.380365
-286.586375	16.718221	0.385370
-290.246423	11.611185	0.390374
-293.840331	11.077826	0.395379
-297.552629	10.352058	0.400384
-301.561842	17.758776	0.405389
-305.224128	21.591920	0.410394
-308.940957	10.982493	0.415398
-312.836023	21.963329	0.420403
-316.599632	19.787090	0.425408
-320.286198	16.731229	0.430413
-324.212331	32.212969	0.435418
-327.637067	9.348097	0.440422
-331.289670	30.367047	0.445427
-335.340257	17.093831	0.450432
-339.134732	17.120841	0.455437
-343.392230	23.619510	0.460442
-346.691039	11.279717	0.465446
-350.405263	21.867461	0.470451
-354.258254	15.238019	0.475456
-357.887378	10.402121	0.480461
-361.590659	23.339384	0.485466
-365.519935	6.065038	0.490470
-369.631172	27.221909	0.495475
-372.905400	5.697164	0.500480
-376.821926	22.514698	0.505485
-380.533370	15.405383	0.510490
-384.033277	11.472994	0.515494
-387.985746	21.740860	0.520499
-391.695230	17.058193	0.525504
-395.235465	13.174838	0.530509
-399.483622	14.401906	0.535514
-403.409155	16.534685	0.540518
-407.300558	17.561302	0.545523
-410.690832	4.788359	0.550528
-414.469164	15.608778	0.555533
-418.299630	12.115577	0.560538
-421.966170	3.917370	0.565542
-425.766304	16.286707	0.570547
-429.716901	15.767930	0.575552
-433.167020	2.318602	0.580557
-436.908957	6.924751	0.585562
-440.496352	7.473945	0.590566
-444.198505	8.676984	0.595571
-448.270947	17.784531	0.600576
-452.122112	5.339140	0.605581
-455.774794	24.290862	0.610586
-459.552600	9.217588	0.615590
-463.171632	13.148137	0.620595
-467.375385	10.648188	0.625600
-470.975235	5.508173	0.630605
-474.626119	18.837770	0.635610
-478.370436	5.474918	0.640614
-482.325150	7.437441	0.645619
-485.964707	20.058769	0.650624
-489.652939	5.791266	0.655629
-493.255577	11.945906	0.660634
-496.778961	10.015444	0.665638
-501.199718	17.152313	0.670643
-504.527014	8.490049	0.675648
-507.966352	11.176130	0.680653
-512.473898	7.824338	0.685658
-516.016099	0.774954	0.690662
-519.914903	13.133376	0.695667
-523.559267	14.948628	0.700672
-527.209559	11.154016	0.705677
-531.121082	18.711078	0.710682
-534.368754	14.658204	0.715686
-538.940276	12.543553	0.720691
-542.271650	6.594366	0.725696
-545.892446	14.185437	0.730701
-549.715324	18.505067	0.735706
-553.233037	12.732313	0.740710
-557.048915	16.598249	0.745715
-561.057800	9.629783	0.750720
-565.190888	11.677705	0.755725
-568.822946	9.036156	0.760730
-572.094957	11.336054	0.765734
-576.245285	17.922079	0.770739
-580.189335	21.699716	0.775744
-583.478202	9.435967	0.780749
-587.528669	18.794119	0.785754
-591.238175	12.842327	0.790758
-595.122658	16.705089	0.795763
-598.944574	14.371459	0.800768
-602.653666	20.562190	0.805773
-606.222148	21.411386	0.810778
-610.000929	19.297965	0.815782
-614.031250	19.019312	0.820787
-617.594591	17.459691	0.825792
-620.981640	22.766368	0.830797
-624.965030	32.933890	0.835802
-628.473617	11.484837	0.840806
-632.585306	29.762653	0.845811
-636.279658	21.201798	0.850816
-639.834725	17.846312	0.855821
-644.232064	25.033313	0.860826
-647.749181	9.929759	0.865830
-651.330536	33.374141	0.870835
-655.139155	14.606585	0.875840
-658.713475	19.104292	0.880845
-662.757470	22.177362	0.885850
-666.331201	8.913732	0.890854
-670.148575	20.034080	0.895859
-674.036523	22.875655	0.900864
-677.803918	13.843996	0.905869
-681.396223	15.846712	0.910874
-685.012968	13.299091	0.915878
-689.173182	23.103876	0.920883
-692.853192	18.558910	0.925888
-696.459253	23.621565	0.930893
-700.656175	17.192744	0.935898
-704.189433	20.263120	0.940902
-707.571269	18.614708	0.945907
-711.359770	19.716840	0.950912
-715.293608	14.190605	0.955917
-719.015926	19.651915	0.960922
-722.411436	9.856008	0.965926
-726.836892	24.593378	0.970931
-730.786479	9.284681	0.975936
-734.271553	10.518132	0.980941
-738.115161	22.681989	0.985946
-741.507949	10.745747	0.990950
-745.142207	18.859654	0.995955
-749.206638	22.606341	1.000960
-752.968298	15.541931	1.005965
-756.874797	20.791460	1.010970
-760.500987	5.065285	1.015974
-764.173424	17.859410	1.020979
-768.019341	15.231849	1.025984
-771.570740	20.347378	1.030989
-775.827271	26.957023	1.035994
-779.204057	3.306248	1.040998
-783.321232	24.806881	1.046003
-786.871910	12.293547	1.051008
-790.581179	21.930232	1.056013
-794.808934	18.991582	1.061018
-798.059854	16.303665	1.066022
-801.644118	14.823363	1.071027
-805.543780	24.190880	1.076032
-809.379657	19.242083	1.081037
-813.582815	16.747391	1.086042
-816.519096	13.766359	1.091046
-820.526851	14.714475	1.096051
-824.382763	19.951295	1.101056
-828.209291	10.265447	1.106061
-832.181598	11.991663	1.111066
-835.674811	3.930431	1.116070
-839.588142	22.069615	1.121075
-843.344355	14.400514	1.126080
-846.582305	11.064043	1.131085
-850.543004	20.570695	1.136090
-854.174634	9.705716	1.141094
-858.148813	14.247133	1.146099
-862.319535	18.931941	1.151104
-865.869481	11.043826	1.156109
-869.737798	22.412314	1.161114
-873.269988	12.439793	1.166118
-877.037188	14.319374	1.171123
-881.202545	13.021977	1.176128
-884.674068	7.190318	1.181133
-888.466652	18.623995	1.186138
-891.990896	10.867430	1.191142
-895.741757	21.900212	1.196147
-899.883178	24.459401	1.201152
-903.359461	19.246691	1.206157
-906.796136	19.102286	1.211162
-910.669837	20.875947	1.216166
-914.615807	14.707023	1.221171
-918.533848	22.760899	1.226176
-922.450231	13.780284	1.231181
-926.176055	23.741513	1.236186
-929.836426	19.220597	1.241190
-933.331975	17.472424	1.246195
-937.096011	27.009274	1.251200
-940.756026	12.618179	1.256205
-945.241486	16.837791	1.261210
-948.526554	15.268875	1.266214
-952.271648	21.271922	1.271219
-956.055877	19.371246	1.276224
-960.010678	17.665008	1.281229
-964.076395	11.513743	1.286234
-967.219186	21.664077	1.291238
-970.779505	13.044505	1.296243
-974.593219	10.107789	1.301248
-978.274532	11.234207	1.306253
-981.980597	27.982709	1.311258
-985.758248	18.663052	1.316262
-989.938108	7.919085	1.321267
-993.713636	6.756671	1.326272
-997.502578	5.269979	1.331277
-1001.486729	15.679478	1.336282
-1005.009076	14.627980	1.341286
-1008.875013	22.569588	1.346291
-1012.557623	16.128484	1.351296
-1016.524844	16.280399	1.356301
-1020.238762	20.882964	1.361306
-1023.569143	21.093892	1.366310
-1027.446173	24.653384	1.371315
-1031.203184	21.581534	1.376320
-1035.261129	16.856292	1.381325
-1039.014084	28.794795	1.386330
-1042.412884	18.354932	1.391334
-1046.478571	23.449037	1.396339
-1050.036191	15.289629	1.401344
-1053.833771	13.496906	1.406349
-1057.905431	23.292870	1.411354
-1061.284864	16.085843	1.416358
-1064.904893	5.211480	1.421363
-1068.904791	21.835207	1.426368
-1072.585358	10.011750	1.431373
-1076.711547	17.674968	1.436378
-1080.327308	10.781740	1.441382
-1083.994004	21.263598	1.446387
-1088.135753	13.904160	1.451392
-1091.382888	15.445429	1.456397
-1095.159563	25.429236	1.461402
-1098.514443	21.659240	1.466406
-1102.465075	12.932005	1.471411
-1106.732022	24.905514	1.476416
-1110.382972	16.341665	1.481421
-1114.335582	27.068002	1.486426
-1117.857507	21.503380	1.491430
-1121.572541	10.215375	1.496435
-1125.149769	20.249320	1.501440
-1128.554006	15.396018	1.506445
-1133.030986	21.574772	1.511450
-1136.796569	11.717286	1.516454
-1140.762661	28.206412	1.521459
-1144.114726	14.643186	1.526464
-1147.825276	5.056040	1.531469
-1151.657594	13.815655	1.536474
-1155.297734	15.274807	1.541478
-1159.223356	15.333577	1.546483
-1163.121158	18.667954	1.551488
-1166.787364	18.540154	1.556493
-1170.568172	12.472990	1.561498
-1174.021449	11.617279	1.566502
-1177.554615	18.239621	1.571507
-1181.676663	16.186785	1.576512
-1185.583424	18.237420	1.581517
-1189.611548	19.749240	1.586522
-1193.028030	16.490711	1.591526
-1196.744051	8.792126	1.596531
-1200.842474	17.111851	1.601536
-1204.252381	9.236566	1.606541
-1208.233725	23.883205	1.611546
-1211.716145	14.944053	1.616550
-1215.638687	15.407701	1.621555
-1219.326224	18.107709	1.626560
-1223.185425	12.176180	1.631565
-1227.257176	26.589736	1.636570
-1230.550800	8.589235	1.641574
-1233.988602	7.521405	1.646579
-1238.126267	18.451009	1.651584
-1241.900663	7.093866	1.656589
-1245.858723	17.565812	1.661594
-1249.439102	3.421138	1.666598
-1253.292153	16.437249	1.671603
-1257.112726	13.412216	1.676608
-1260.664589	15.190140	1.681613
-1264.174593	23.338540	1.686618
-1268.105764	12.443342	1.691622
-1271.966806	13.986912	1.696627
-1275.828232	23.618703	1.701632
-1279.340109	7.140272	1.706637
-1283.591655	27.923586	1.711642
-1287.182336	4.123409	1.716646
-1290.703479	20.484775	1.721651
-1294.359101	9.878263	1.726656
-1298.331118	14.648719	1.731661
-1302.286045	21.807097	1.736666
-1306.073151	-4.046317	1.741670
-1309.539060	16.136623	1.746675
-1313.522373	10.649314	1.751680
-1317.103455	11.452718	1.756685
-1320.925781	17.653196	1.761690
-1324.921171	7.802859	1.766694
-1327.959549	8.689727	1.771699
-1331.948977	14.565309	1.776704
-1336.155805	4.442911	1.781709
-1340.055812	13.207345	1.786714
-1343.354232	2.029664	1.791718
-1347.154884	13.219313	1.796723
-1350.954379	6.953601	1.801728
-1354.612859	6.973095	1.806733
-1358.343921	10.905571	1.811738
-1362.357718	9.979018	1.816742
-1366.342494	16.547768	1.821747
-1370.062753	26.609694	1.826752
-1373.265779	13.691602	1.831757
-1377.554081	16.787645	1.836762
-1380.988790	14.615679	1.841766
-1384.487069	16.134479	1.846771
-1388.640320	17.807021	1.851776
-1392.583473	10.165627	1.856781
-1396.503022	23.091683	1.861786
-1399.858758	11.890142	1.866790
-1403.613676	17.371913	1.871795
-1407.239005	7.300060	1.876800
-1410.923460	16.187794	1.881805
-1415.339934	12.835807	1.886810
-1419.135729	4.067014	1.891814
-1422.296173	11.497355	1.896819
-1426.208344	3.653947	1.901824
-1430.031390	14.705385	1.906829
-1433.885299	10.465434	1.911834
-1437.222676	10.777423	1.916838
-1441.118081	14.837267	1.921843
-1445.179945	15.069722	1.926848
-1448.437031	7.646589	1.931853
-1452.889084	22.368972	1.936858
-1456.534125	10.150984	1.941862
-1459.893977	13.705642	1.946867
-1463.993130	23.776335	1.951872
-1467.458682	12.122555	1.956877
-1471.404245	28.940058	1.961882
-1475.089346	11.141407	1.966886
-1478.921865	18.048661	1.971891
-1482.481144	13.638615	1.976896
-1486.048312	20.113888	1.981901
-1489.897766	19.033510	1.986906
-1493.940800	24.824909	1.991910
-1497.787035	15.573894	1.996915
-1501.755608	19.789272	2.006912
-1502.496550	20.413206	2.016909
-1499.892258	16.399319	2.026906
-1497.505978	11.858237	2.036902
-1495.068984	14.807517	2.046899
-1492.917459	19.278841	2.056896
-1491.150904	17.254388	2.066893
-1489.264656	17.097629	2.076890
-1487.851136	16.373931	2.086886
-1485.645217	17.997581	2.096883
-1483.680191	17.068732	2.106880
-1481.630388	19.633181	2.116877
-1480.028659	17.216705	2.126874
-1477.791855	16.222238	2.136870
-1476.246455	16.173751	2.146867
-1474.231114	16.176335	2.156864
-1472.255272	18.670530	2.166861
-1470.228513	19.790772	2.176858
-1468.437630	24.136708	2.186854
-1466.536166	18.539588	2.196851
-1464.741283	18.125897	2.206848
-1462.810187	12.909304	2.216845
-1461.034646	18.674028	2.226842
-1459.065174	14.030772	2.236838
-1457.227835	8.083927	2.246835
-1455.471336	15.945405	2.256832
-1453.647675	13.700257	2.266829
-1451.370107	16.392478	2.276826
-1449.368808	13.840994	2.286822
-1447.668817	20.751521	2.296819
-1446.127130	13.451480	2.306816
-1444.025705	15.690327	2.316813
-1442.119550	12.093021	2.326810
-1440.164177	8.489416	2.336806
-1438.315720	15.434599	2.346803
-1436.274674	16.503636	2.356800
-1434.640569	12.329361	2.366797
-1432.681890	14.887917	2.376794
-1430.826762	15.557248	2.386790
-1429.241296	13.099199	2.396787
-1427.114137	12.206020	2.406784
-1425.160911	19.538657	2.416781
-1423.187668	21.024355	2.426778
-1421.242533	16.271340	2.436774
-1419.410404	17.828581	2.446771
-1417.954456	13.877050	2.456768
-1415.986867	13.104165	2.466765
-1413.781101	16.864245	2.476762
-1412.225153	14.241984	2.486758
-1410.230096	15.975255	2.496755
-1407.983084	12.384987	2.506752
-1406.416838	17.485362	2.516749
-1404.584565	20.372079	2.526746
-1402.587697	17.101336	2.536742
-1400.590591	13.516344	2.546739
-1398.826682	11.347120	2.556736
-1396.950857	15.627409	2.566733
-1395.200689	17.245159	2.576730
-1392.980994	17.559314	2.586726
-1391.398378	21.360753	2.596723
-1389.539196	13.138332	2.606720
-1387.858621	10.355609	2.616717
-1385.596374	17.281967	2.626714
-1383.941212	18.861250	2.636710
-1381.971385	14.276421	2.646707
-1379.994685	9.101541	2.656704
-1378.289022	21.057579	2.666701
-1376.319408	9.593249	2.676698
-1374.344008	11.411804	2.686694
-1372.479065	15.618065	2.696691
-1370.674874	10.458176	2.706688
-1368.893132	17.347784	2.716685
-1366.878416	18.446362	2.726682
-1365.010758	16.262134	2.736678
-1363.333474	17.736838	2.746675
-1361.257106	13.573922	2.756672
-1359.509305	17.078939	2.766669
-1357.805218	13.506150	2.776666
-1355.886119	16.712168	2.786662
-1353.525723	10.272721	2.796659
-1352.025729	14.084255	2.806656
-1349.903022	19.458762	2.816653
-1348.088951	15.708899	2.826650
-1346.205560	13.334271	2.836646
-1344.310190	12.413531	2.846643
-1342.477143	6.931672	2.856640
-1340.942080	14.048684	2.866637
-1338.849784	20.541239	2.876634
-1337.019933	11.461437	2.886630
-1334.848595	15.672373	2.896627
-1333.151742	7.665453	2.906624
-1330.973451	11.224746	2.916621
-1329.118892	7.676841	2.926618
-1327.739674	12.726681	2.936614
-1326.096493	10.369991	2.946611
-1323.564772	8.092140	2.956608
-1321.708266	11.540313	2.966605
-1319.819082	10.764269	2.976602
-1318.145200	17.075914	2.986598
-1316.396523	10.372828	2.996595
-1314.661969	11.652083	3.006592
-1312.290915	13.459474	3.016589
-1310.782589	12.723867	3.026586
-1308.604807	12.744808	3.036582
-1306.908500	7.318019	3.046579
-1305.053787	10.183855	3.056576
-1302.973069	13.101944	3.066573
-1301.273228	19.556293	3.076570
-1299.195026	20.267398	3.086566
-1297.322571	8.652885	3.096563
-1295.402304	12.700355	3.106560
-1293.679673	11.685722	3.116557
-1291.913696	9.857303	3.126554
-1290.128697	17.161724	3.136550
-1288.263303	16.447934	3.146547
-1286.173809	8.934000	3.156544
-1284.324923	11.301834	3.166541
-1282.395605	17.834737	3.176538
-1280.586884	16.310541	3.186534
-1278.603835	17.360580	3.196531
-1276.827346	19.493689	3.206528
-1274.998891	15.102098	3.216525
-1273.047940	9.869844	3.226522
-1271.283238	14.076444	3.236518
-1269.102093	6.355224	3.246515
-1267.439600	8.918692	3.256512
-1265.800158	7.290544	3.266509
-1263.927262	15.324612	3.276506
-1261.780286	8.182030	3.286502
-1259.995713	5.763284	3.296499
-1257.846637	8.997321	3.306496
-1256.178820	17.174743	3.316493
-1254.273027	8.613379	3.326490
-1252.541915	13.944854	3.336486
-1250.584072	13.472092	3.346483
-1248.550404	16.843030	3.356480
-1246.929820	18.461106	3.366477
-1244.745085	14.497266	3.376474
-1243.032853	18.042805	3.386470
-1241.119829	9.835560	3.396467
-1239.561171	12.429875	3.406464
-1237.660954	16.363763	3.416461
-1235.470929	15.637542	3.426458
-1233.597779	21.516313	3.436454
-1231.786559	18.479105	3.446451
-1229.619312	10.812247	3.456448
-1228.167252	12.375195	3.466445
-1226.161035	13.824208	3.476442
-1224.363947	9.109251	3.486438
-1222.457443	12.426347	3.496435
-1220.332467	13.974785	3.506432
-1218.459400	14.197728	3.516429
-1216.985032	11.525489	3.526426
-1215.097870	11.272490	3.536422
-1212.962060	6.383341	3.546419
-1210.861726	13.684741	3.556416
-1209.310390	8.352266	3.566413
-1207.744500	10.369125	3.576410
-1205.444375	8.837412	3.586406
-1203.684978	11.488055	3.596403
-1201.624122	9.069357	3.606400
-1199.672330	17.725604	3.616397
-1198.044182	7.602897	3.626394
-1196.212015	5.416587	3.636390
-1194.122704	12.702397	3.646387
-1192.457146	15.777017	3.656384
-1190.478310	14.271461	3.666381
-1188.443059	14.249003	3.676378
-1186.775475	18.038574	3.686374
-1185.105422	11.998690	3.696371
-1183.056195	9.291339	3.706368
-1181.000698	15.497825	3.716365
-1179.267282	11.503620	3.726362
-1177.328527	14.724017	3.736358
-1175.262503	11.240291	3.746355
-1173.544723	13.916565	3.756352
-1171.872272	14.299539	3.766349
-1169.821008	16.172452	3.776346
-1168.081680	19.366342	3.786342
-1166.225098	16.345611	3.796339
-1164.577658	14.365721	3.806336
-1162.066000	13.065474	3.816333
-1160.503375	14.787622	3.826330
-1158.568900	16.352384	3.836326
-1156.633801	21.914992	3.846323
-1154.848730	13.622488	3.856320
-1152.962189	18.150749	3.866317
-1150.966207	13.634552	3.876314
-1149.257019	20.027528	3.886310
-1147.268617	13.613049	3.896307
-1145.402243	12.131839	3.906304
-1143.611902	16.907606	3.916301
-1142.037415	10.794616	3.926298
-1139.908129	15.187737	3.936294
-1137.739074	13.261789	3.946291
-1136.083032	13.498991	3.956288
-1134.176037	7.050180	3.966285
-1132.299839	20.365483	3.976282
-1130.361947	13.725410	3.986278
-1128.432546	7.748288	3.996275
-1126.522102	9.717978	4.006272
-1124.832309	9.251886	4.016269
-1122.999742	16.621472	4.026266
-1121.066721	15.126461	4.036262
-1119.298716	16.293145	4.046259
-1117.263052	14.911193	4.056256
-1115.666070	15.623652	4.066253
-1113.858729	17.320897	4.076250
-1111.587942	13.804469	4.086246
-1109.658675	19.481737	4.096243
-1107.828523	22.266405	4.106240
-1105.903963	16.789024	4.116237
-1104.238810	20.994316	4.126234
-1102.091815	22.784083	4.136230
-1100.442573	14.423341	4.146227
-1098.729797	16.404148	4.156224
-1096.684959	10.192265	4.166221
-1094.862049	11.980192	4.176218
-1092.858035	11.364386	4.186214
-1091.021652	14.872815	4.196211
-1089.349579	11.336912	4.206208
-1087.355071	15.454796	4.216205
-1085.313008	12.496039	4.226202
-1083.396479	12.345819	4.236198
-1081.702733	15.327590	4.246195
-1079.864994	12.122042	4.256192
-1077.712975	13.044173	4.266189
-1075.939315	10.224672	4.276186
-1074.466777	20.164026	4.286182
-1072.050639	16.790178	4.296179
-1070.317184	11.294445	4.306176
-1068.649033	9.207097	4.316173
-1066.684828	9.489797	4.326170
-1065.018808	10.704414	4.336166
-1062.990054	11.294165	4.346163
-1060.798091	9.713576	4.356160
-1059.192224	5.381432	4.366157
-1057.381082	9.879200	4.376154
-1055.224809	9.826449	4.386150
-1053.512393	10.817335	4.396147
-1051.597571	10.297936	4.406144
-1049.633790	9.165963	4.416141
-1047.831440	11.257220	4.426138
-1046.218758	7.874532	4.436134
-1044.048146	9.665312	4.446131
-1042.005102	12.390718	4.456128
-1040.341238	5.101378	4.466125
-1038.843051	6.211801	4.476122
-1036.766328	8.282869	4.486118
-1034.766143	11.165139	4.496115
-1032.520553	13.627631	4.506112
-1031.010084	13.427131	4.516109
-1029.204541	13.526814	4.526106
-1027.427116	6.017211	4.536102
-1025.204484	12.817649	4.546099
-1023.590182	12.311597	4.556096
-1021.590014	8.176947	4.566093
-1019.396756	14.284185	4.576090
-1017.860886	10.151158	4.586086
-1016.058466	7.908161	4.596083
-1014.113777	2.205002	4.606080
-1011.909092	10.805188	4.616077
-1010.614234	14.037122	4.626074
-1008.729522	13.525731	4.636070
-1006.499723	14.860233	4.646067
-1004.752041	11.209663	4.656064
-1002.773854	10.174901	4.666061
-1000.796675	15.617230	4.676058
-998.942495	10.094346	4.686054
-997.338399	13.292625	4.696051
-995.472614	7.423673	4.706048
-993.484737	12.764822	4.716045
-991.751490	16.542462	4.726042
-989.670175	10.354831	4.736038
-987.594260	11.175531	4.746035
-985.853667	5.167131	4.756032
-984.304870	11.478514	4.766029
-982.338222	11.238256	4.776026
-980.311089	8.904088	4.786022
-978.445787	11.498499	4.796019
-976.462940	10.145640	4.806016
-974.698591	17.417315	4.816013
-972.631789	12.792041	4.826010
-970.914463	15.365909	4.836006
-968.967083	7.843380	4.846003
-967.252785	15.080431	4.856000
-965.435887	6.688230	4.865997
-963.641886	10.955129	4.875994
-961.537363	19.342438	4.885990
-959.762118	7.963173	4.895987
-957.819531	16.540590	4.905984
-956.008005	11.585091	4.915981
-953.792512	10.225052	4.925978
-952.161128	15.852193	4.935974
-950.379852	12.698402	4.945971
-948.432826	20.897747	4.955968
-946.466831	12.664876	4.965965
-944.713501	15.179323	4.975962
-943.158741	14.431790	4.985958
-940.948642	14.220536	4.995955
-939.009825	12.996329	5.005952
-937.083867	15.355283	5.015949
-935.224731	15.973846	5.025946
-933.254905	14.504681	5.035942
-931.679382	16.851776	5.045939
-929.708669	10.441875	5.055936
-927.820174	14.575274	5.065933
-925.918710	13.821267	5.075930
-923.983843	20.149919	5.085926
-921.934626	13.956422	5.095923
-920.278884	13.956981	5.105920
-918.554051	18.481297	5.115917
-916.627538	18.007507	5.125914
-914.713403	14.251439	5.135910
-912.749476	11.153737	5.145907
-910.876892	16.462869	5.155904
-909.059996	12.952882	5.165901
-907.136774	16.453895	5.175898
-905.356245	20.279308	5.185894
-903.834054	19.298583	5.195891
-901.351650	11.156871	5.205888
-899.668390	16.483650	5.215885
-897.630454	16.923654	5.225882
-895.588289	12.232908	5.235878
-893.919521	13.865637	5.245875
-892.152660	11.683681	5.255872
-890.490043	19.022219	5.265869
-888.470024	14.928712	5.275866
-886.510136	12.419054	5.285862
-884.519008	17.835575	5.295859
-882.561534	14.165762	5.305856
-880.751497	10.607945	5.315853
-879.268149	16.153017	5.325850
-877.274187	14.992676	5.335846
-875.165925	18.625191	5.345843
-873.408502	11.497840	5.355840
-871.453410	11.690581	5.365837
-869.474465	11.375819	5.375834
-867.967298	14.161786	5.385830
-865.939307	12.020211	5.395827
-864.039523	11.508105	5.405824
-861.918856	15.080226	5.415821
-860.054550	11.957438	5.425818
-858.386483	21.483585	5.435814
-856.565028	13.409678	5.445811
-854.514558	11.842423	5.455808
-852.748986	12.428639	5.465805
-851.259617	10.565813	5.475802
-849.164723	17.912650	5.485798
-846.882509	15.196760	5.495795
-845.171566	7.884225	5.505792
-843.327485	17.360140	5.515789
-841.308013	13.980454	5.525786
-839.721322	19.516930	5.535782
-837.870802	13.216313	5.545779
-835.791737	12.961366	5.555776
-833.685393	8.249360	5.565773
-831.973448	7.047294	5.575770
-830.279026	12.789188	5.585766
-828.450705	14.548042	5.595763
-826.597139	10.013818	5.605760
-824.717886	8.338165	5.615757
-822.680199	9.716183	5.625754
-820.942175	14.642683	5.635750
-818.961480	11.616588	5.645747
-816.763115	10.300467	5.655744
-815.208377	14.372044	5.665741
-813.277359	13.086026	5.675738
-811.382660	12.852674	5.685734
-809.686983	17.100678	5.695731
-807.781615	10.603420	5.705728
-805.720389	11.096624	5.715725
-803.789299	14.826998	5.725722
-802.101012	18.144596	5.735718
-800.608890	14.219222	5.745715
-798.413229	7.648730	5.755712
-796.228043	14.548548	5.765709
-794.611252	15.835967	5.775706
-792.879012	20.272355	5.785702
-790.705357	16.544378	5.795699
-788.617727	15.506511	5.805696
-787.205111	16.853411	5.815693
-784.952661	11.765982	5.825690
-783.530492	23.257839	5.835686
-781.497499	9.396397	5.845683
-779.334087	12.879657	5.855680
-777.603858	12.075766	5.865677
-775.956458	16.457830	5.875674
-774.159125	13.522656	5.885670
-771.938448	9.022959	5.895667
-770.070637	13.600330	5.905664
-768.525227	9.319085	5.915661
-766.365456	13.732954	5.925658
-764.464614	13.827084	5.935654
-762.622381	9.422615	5.945651
-760.738568	13.293215	5.955648
-758.912293	14.724024	5.965645
-757.214750	19.641256	5.975642
-755.150040	12.385926	5.985638
-753.371816	11.817545	5.995635
-751.402248	11.243849	6.005632
-749.247788	14.310141	6.015629
-747.771337	14.164207	6.025626
-746.063828	12.800277	6.035622
-743.974329	16.159592	6.045619
-742.210018	17.248206	6.055616
-740.023456	14.899814	6.065613
-738.330914	14.255134	6.075610
-736.371408	16.986272	6.085606
-734.538048	16.800679	6.095603
-732.698688	14.934100	6.105600
-730.804573	19.821519	6.115597
-728.779591	21.798504	6.125594
-727.077277	20.081726	6.135590
-725.196214	20.300630	6.145587
-722.924476	13.411722	6.155584
-721.413354	16.471897	6.165581
-719.410201	14.885475	6.175578
-717.778306	13.164168	6.185574
-716.046464	16.070653	6.195571
-713.901192	13.059397	6.205568
-711.560936	14.460218	6.215565
-710.154458	7.944856	6.225562
-708.441807	14.280786	6.235558
-706.608047	12.855656	6.245555
-704.358503	13.052011	6.255552
-702.405871	13.458447	6.265549
-700.835787	12.326512	6.275546
-698.734266	15.772370	6.285542
-696.873029	12.242821	6.295539
-695.003407	8.337717	6.305536
-693.545405	12.500627	6.315533
-691.519449	16.335941	6.325530
-689.441814	18.105596	6.335526
-687.621585	16.696853	6.345523
-685.829619	13.907867	6.355520
-683.754214	8.133543	6.365517
-681.817354	5.866156	6.375514
-680.213816	8.496320	6.385510
-678.371446	10.602001	6.395507
-676.145809	10.890626	6.405504
-674.498272	3.493596	6.415501
-672.543128	5.685474	6.425498
-670.674719	6.602770	6.435494
-668.820592	9.535541	6.445491
-667.414103	11.074549	6.455488
-665.108248	10.552985	6.465485
-663.013464	7.871951	6.475482
-661.243611	19.433082	6.485478
-659.558771	16.028061	6.495475
-657.570457	15.010914	6.505472
-655.931363	18.301744	6.515469
-653.643536	12.214026	6.525466
-651.827313	16.400259	6.535462
-650.206513	14.330237	6.545459
-648.093967	14.600640	6.555456
-646.058150	14.400138	6.565453
-644.661989	13.518662	6.575450
-642.927914	18.202773	6.585446
-640.849752	16.658117	6.595443
-638.747082	14.910597	6.605440
-636.823050	17.109057	6.615437
-635.097763	9.448569	6.625434
-633.306752	10.425630	6.635430
-631.263442	17.660917	6.645427
-629.298142	9.134705	6.655424
-627.283885	7.617640	6.665421
-626.045096	13.116692	6.675418
-624.142307	15.817512	6.685414
-621.928076	15.114835	6.695411
-619.931280	16.865887	6.705408
-618.332449	16.713114	6.715405
-616.232093	14.102284	6.725402
-614.466008	21.269770	6.735398
-612.827688	19.176446	6.745395
-610.545308	12.645945	6.755392
-608.585153	12.384929	6.765389
-606.950954	9.269092	6.775386
-605.275551	19.991135	6.785382
-603.052262	18.344379	6.795379
-601.361403	19.250621	6.805376
-599.392578	9.751217	6.815373
-597.726575	11.498288	6.825370
-595.686492	12.168742	6.835366
-593.714491	11.512681	6.845363
-591.875105	12.609943	6.855360
-589.988358	9.625883	6.865357
-588.059185	12.499363	6.875354
-586.617977	13.173911	6.885350
-584.381505	15.398295	6.895347
-582.575762	16.014614	6.905344
-580.636922	8.097413	6.915341
-578.873536	7.784168	6.925338
-576.890159	12.412715	6.935334
-574.910638	13.089703	6.945331
-573.292022	3.470998	6.955328
-571.207429	4.927008	6.965325
-569.358839	4.857533	6.975322
-567.825480	8.899538	6.985318
-565.385118	6.501288	6.995315
-563.733871	15.270870	7.005312
-561.749964	5.914353	7.015309
-560.246923	11.745450	7.025306
-558.352867	8.215499	7.035302
-556.074367	15.149600	7.045299
-554.343590	4.467707	7.055296
-552.586878	6.190847	7.065293
-550.688874	9.148286	7.075290
-548.824798	10.656908	7.085286
-546.705425	14.133213	7.095283
-545.185153	12.571959	7.105280
-543.148711	10.156140	7.115277
-541.127105	15.503364	7.125274
-539.533797	12.872533	7.135270
-537.505653	14.549173	7.145267
-535.652739	6.186247	7.155264
-533.889707	2.404081	7.165261
-531.817762	7.976959	7.175258
-530.008415	15.301816	7.185254
-528.040372	13.525367	7.195251
-526.313265	8.962612	7.205248
-524.642628	7.557358	7.215245
-522.283401	11.184853	7.225242
-520.809236	14.697916	7.235238
-518.894208	13.476268	7.245235
-516.873747	18.664221	7.255232
-514.852798	10.853955	7.265229
-513.364266	12.413111	7.275226
-511.104211	9.101063	7.285222
-509.041984	15.177632	7.295219
-507.475510	11.952674	7.305216
-505.912823	14.494748	7.315213
-503.873556	13.643277	7.325210
-501.821647	13.374011	7.335206
-500.001270	11.996965	7.345203
-498.021779	9.553963	7.355200
-496.283401	10.661115	7.365197
-494.245317	14.289401	7.375194
-492.353648	13.355721	7.385190
-490.937136	18.578571	7.395187
-488.663182	10.791077	7.405184
-486.766854	11.535111	7.415181
-484.806958	10.773702	7.425178
-483.046992	16.361714	7.435174
-481.298390	12.123983	7.445171
-479.369796	15.836086	7.455168
-477.526663	16.144929	7.465165
-475.657377	13.793756	7.475162
-473.675071	10.101352	7.485158
-471.851570	13.197073	7.495155
-469.856322	14.601125	7.505152
-468.220654	14.335200	7.515149
-466.127121	19.543110	7.525146
-464.240754	12.482282	7.535142
-462.459284	11.755701	7.545139
-460.621992	10.194400	7.555136
-458.549095	11.153423	7.565133
-456.776050	15.921457	7.575130
-455.224008	12.116193	7.585126
-453.083034	19.621848	7.595123
-451.159037	11.227099	7.605120
-449.104278	6.653129	7.615117
-447.363592	8.936287	7.625114
-445.701094	5.375503	7.635110
-443.798321	4.676934	7.645107
-441.646660	8.583977	7.655104
-439.612939	10.255075	7.665101
-438.197901	7.491720	7.675098
-436.382275	12.183494	7.685094
-434.414639	16.836788	7.695091
-432.469850	9.364016	7.705088
-430.444993	16.060848	7.715085
-428.395248	9.722395	7.725082
-426.747579	4.363956	7.735078
-425.409534	8.877781	7.745075
-423.381075	10.281307	7.755072
-421.085905	10.282747	7.765069
-419.137606	7.639521	7.775066
-417.574112	16.704289	7.785062
-415.601221	16.285079	7.795059
-413.682073	16.063929	7.805056
-411.736458	13.957990	7.815053
-410.026130	16.189182	7.825050
-407.865532	13.548383	7.835046
-406.331084	6.482209	7.845043
-404.179852	7.040343	7.855040
-402.233878	10.759208	7.865037
-400.259101	12.755547	7.875034
-398.955367	11.780021	7.885030
-396.880850	8.057165	7.895027
-394.760907	10.685607	7.905024
-392.907773	8.717610	7.915021
-391.481854	7.469942	7.925018
-389.160063	6.156610	7.935014
-387.398235	4.702153	7.945011
-385.715983	11.767941	7.955008
-383.587209	2.519481	7.965005
-381.559269	10.610102	7.975002
-379.896619	9.304119	7.984998
-378.093414	13.090011	7.994995
-375.952970	-0.104596	8.004992
-374.104453	4.090913	8.014989
-372.244194	1.621258	8.024986
-370.689307	8.557388	8.034982
-368.748364	8.329637	8.044979
-367.021395	9.596604	8.054976
-364.803022	10.409322	8.064973
-363.063335	4.804122	8.074970
-361.073899	8.882406	8.084966
-359.323302	12.692502	8.094963
-357.392175	9.109415	8.104960
-355.412383	4.522225	8.114957
-353.451218	7.259739	8.124954
-351.802803	10.808252	8.134950
-349.816851	13.030224	8.144947
-348.266028	12.972140	8.154944
-345.906678	10.113346	8.164941
-344.422852	5.674817	8.174938
-342.691249	20.116076	8.184934
-340.541643	17.312876	8.194931
-338.553454	16.401803	8.204928
-336.486208	11.576449	8.214925
-334.812957	12.315162	8.224922
-332.937363	12.091556	8.234918
-331.274999	4.749210	8.244915
-329.458374	16.317372	8.254912
-327.241202	17.439798	8.264909
-325.211041	11.153500	8.274906
-323.641127	13.413486	8.284902
-321.858402	8.728303	8.294899
-319.751233	15.281042	8.304896
-317.764664	12.368096	8.314893
-316.370604	10.089746	8.324890
-314.197470	4.325385	8.334886
-312.511548	13.405424	8.344883
-310.476580	11.269512	8.354880
-308.709840	11.352254	8.364877
-306.664684	13.586918	8.374874
-304.930030	10.598929	8.384870
-302.897602	12.486673	8.394867
-300.988300	6.241793	8.404864
-299.311424	14.494323	8.414861
-297.422152	11.560608	8.424858
-295.060130	14.651038	8.434854
-293.799390	13.827696	8.444851
-291.389304	14.447247	8.454848
-290.104169	8.761488	8.464845
-287.932001	14.973875	8.474842
-286.315511	11.428431	8.484838
-284.285376	11.060193	8.494835
-282.443685	13.979473	8.504832
-280.578442	12.069628	8.514829
-278.563338	13.652257	8.524826
-276.603544	10.328346	8.534822
-274.900601	14.068743	8.544819
-272.837018	15.060994	8.554816
-270.929367	7.040045	8.564813
-269.206379	11.339364	8.574810
-267.250243	10.068720	8.584807
-265.566099	10.420472	8.594803
-263.585463	15.259738	8.604800
-261.795644	8.441839	8.614797
-259.643789	5.448874	8.624794
-258.162274	9.669897	8.634791
-256.223774	15.640130	8.644787
-254.042714	10.452459	8.654784
-252.024821	14.584721	8.664781
-250.373340	8.002071	8.674778
-248.598983	10.085791	8.684775
-246.991935	19.105842	8.694771
-244.680580	9.079908	8.704768
-243.222552	12.150455	8.714765
-240.781946	4.909751	8.724762
-239.270607	6.187541	8.734759
-237.437711	11.047250	8.744755
-235.061897	2.255280	8.754752
-233.342682	3.111468	8.764749
-231.575170	-1.353323	8.774746
-229.988649	2.086731	8.784743
-228.104272	5.596095	8.794739
-225.974713	5.145721	8.804736
-224.190941	8.255873	8.814733
-222.134533	-2.119355	8.824730
-220.242068	4.102994	8.834727
-218.488150	1.999379	8.844723
-216.821164	-2.780944	8.854720
-214.670626	1.022277	8.864717
-212.933763	-1.029663	8.874714
-211.114608	4.234898	8.884711
-208.917672	4.478012	8.894707
-207.488430	-0.043308	8.904704
-205.693279	3.469261	8.914701
-203.513990	-2.715996	8.924698
-201.618725	-1.568926	8.934695
-199.674693	-1.497029	8.944691
-198.050021	0.219027	8.954688
-195.966943	-5.551387	8.964685
-194.073420	-5.302474	8.974682
-192.508921	0.110110	8.984679
-190.544284	4.936200	8.994675
-188.398581	4.372753	9.004672
-186.676832	-2.631602	9.014669
-184.717053	-1.417443	9.024666
-182.912063	1.221975	9.034663
-181.131251	-0.178521	9.044659
-179.142163	-0.071163	9.054656
-177.191989	-2.641864	9.064653
-175.343522	0.895378	9.074650
-173.701032	3.203884	9.084647
-171.711821	2.059095	9.094643
-169.648979	0.430442	9.104640
-167.882956	-1.735069	9.114637
-165.842239	0.637795	9.124634
-164.092803	-0.992950	9.134631
-162.490297	-0.814419	9.144627
-160.382524	-2.447076	9.154624
-158.298588	2.476850	9.164621
-156.539006	-0.805545	9.174618
-155.004410	-2.471477	9.184615
-152.930540	1.789308	9.194611
-151.205603	1.750938	9.204608
-149.032423	-0.001095	9.214605
-147.137556	0.456066	9.224602
-145.386800	-1.571200	9.234599
-143.499039	10.964740	9.244595
-141.536955	3.476790	9.254592
-139.775872	4.424262	9.264589
-137.806318	7.913795	9.274586
-136.071236	8.843313	9.284583
-134.189247	14.281077	9.294579
-132.209367	9.654569	9.304576
-130.472743	13.293382	9.314573
-128.541769	16.209593	9.324570
-126.511517	13.136667	9.334567
-124.540803	21.336140	9.344563
-122.942433	18.627394	9.354560
-121.103961	17.465641	9.364557
-119.137595	7.690652	9.374554
-117.391553	15.829657	9.384551
-115.579407	21.349637	9.394547
-113.318813	12.686681	9.404544
-111.303946	13.525788	9.414541
-109.852641	16.652757	9.424538
-107.924974	11.453531	9.434535
-105.778773	19.552389	9.444531
-104.100376	10.721795	9.454528
-102.323647	13.397367	9.464525
-100.366130	11.273983	9.474522
-98.392812	11.175497	9.484519
-96.748949	20.245055	9.494515
-94.820646	11.898819	9.504512
-92.745783	9.901987	9.514509
-91.196672	16.978196	9.524506
-88.867429	14.789201	9.534503
-87.338851	14.775887	9.544499
-85.486374	16.591473	9.554496
-83.274145	14.078511	9.564493
-81.618820	14.706575	9.574490
-79.780502	10.934816	9.584487
-77.768533	16.929801	9.594483
-75.870588	15.488588	9.604480
-73.859294	12.718736	9.614477
-72.227978	22.737708	9.624474
-70.336204	17.184224	9.634471
-68.730876	19.727689	9.644467
-66.634670	14.402129	9.654464
-64.596548	15.641786	9.664461
-62.826196	17.661548	9.674458
-60.829934	15.740440	9.684455
-58.978219	16.796676	9.694451
-57.321765	14.932937	9.704448
-55.255332	19.179213	9.714445
-53.229309	16.787563	9.724442
-51.755896	13.302986	9.734439
-49.811265	14.535464	9.744435
-47.757133	15.368361	9.754432
-45.880715	16.313295	9.764429
-44.006550	13.304809	9.774426
-42.305693	13.597208	9.784423
-40.471152	13.895126	9.794419
-38.320676	13.452632	9.804416
-36.645707	9.856964	9.814413
-34.689526	16.149840	9.824410
-32.816348	16.108435	9.834407
-30.774359	14.737440	9.844403
-29.032752	14.057009	9.854400
-26.867023	15.483190	9.864397
-25.479640	14.341356	9.874394
-23.643646	11.550558	9.884391
-21.672125	15.886215	9.894387
-19.683825	15.839088	9.904384
-17.492020	11.332026	9.914381
-15.777460	9.899584	9.924378
-14.237540	14.960947	9.934375
-12.432356	9.677116	9.944371
-10.476005	13.778353	9.954368
-8.552965	12.811622	9.964365
-6.285463	12.467335	9.974362
-4.725036	21.209212	9.984359
-3.494420	44.243026	9.994355
-2.252981	79.307078	10.004352
-0.877095	125.615923	10.014349
0.000000	180.377989	10.019354
0.770090	212.810495	10.024359
1.571890	249.021222	10.029363
2.281156	269.994092	10.034368
2.458208	307.779103	10.039373
2.743912	321.583546	10.044378
3.168867	325.499280	10.049383
3.153298	345.471353	10.054387
3.135288	353.103780	10.059392
3.413662	355.809684	10.064397
3.750551	364.853702	10.069402
3.678739	371.345082	10.074407
3.559597	363.187319	10.079411
3.842741	363.601075	10.084416
3.929521	367.911392	10.089421
3.987730	373.563569	10.094426
3.502273	377.588255	10.099431
3.839191	405.094326	10.104435
4.323803	403.753855	10.109440
4.231740	424.889455	10.114445
4.460446	416.491670	10.119450
4.179581	416.490743	10.124455
4.198538	422.396790	10.129459
4.541034	415.546830	10.134464
4.513967	424.563777	10.139469
4.503940	412.698374	10.144474
4.373410	423.028125	10.149479
4.705448	428.322823	10.154483
4.696465	435.848193	10.159488
4.257265	438.871999	10.164493
4.571176	432.152751	10.169498
4.354561	443.371489	10.174503
4.473728	430.687497	10.179507
4.693042	436.520591	10.184512
4.201667	433.468602	10.189517
4.365401	434.685182	10.194522
4.797629	449.796587	10.199527
5.056629	463.357045	10.204531
5.062852	460.179951	10.209536
5.226872	470.834932	10.214541
5.417788	472.815187	10.219546
4.914211	462.338965	10.224551
4.967993	473.465711	10.229555
5.328357	475.324319	10.234560
5.271581	478.772859	10.239565
5.434928	478.109699	10.244570
5.523906	476.622582	10.249575
5.611941	479.032426	10.254579
5.216080	474.370828	10.259584
5.492099	490.522791	10.264589
5.490932	473.868096	10.269594
5.694102	483.192147	10.274599
5.600689	494.033290	10.279603
5.773161	488.181858	10.284608
5.651052	498.087678	10.289613
5.760426	489.139580	10.294618
5.571605	494.020617	10.299623
5.536289	497.030481	10.304627
5.936158	501.957981	10.309632
5.650008	500.089127	10.314637
5.847285	502.303348	10.319642
5.944334	503.393369	10.324647
5.901225	508.339483	10.329651
5.993223	502.276943	10.334656
5.861576	508.128196	10.339661
6.081446	498.318762	10.344666
6.188564	507.593491	10.349671
6.012775	511.236071	10.354675
6.463566	522.905109	10.359680
6.333128	542.962010	10.364685
6.265946	547.371057	10.369690
6.418890	543.965530	10.374695
6.439949	544.219235	10.379699
6.850058	547.205376	10.384704
6.561000	546.040333	10.389709
6.416696	548.859424	10.394714
6.418952	546.758475	10.399719
6.739501	548.495704	10.404723
6.597901	548.452063	10.409728
6.360177	560.804985	10.414733
6.797104	561.403965	10.419738
6.402812	554.360781	10.424743
6.240153	565.250870	10.429747
6.727213	562.683069	10.434752
6.908183	588.372393	10.439757
6.655906	590.697755	10.444762
7.424554	589.598986	10.449767
7.076375	601.513798	10.454771
7.289849	595.228408	10.459776
7.267967	608.728141	10.464781
7.469966	588.984621	10.469786
7.444760	605.052286	10.474791
6.989203	599.532801	10.479795
7.256210	599.734663	10.484800
7.228013	605.528452	10.489805
7.382372	608.616901	10.494810
7.585887	598.915670	10.499815
7.366913	603.831516	10.504819
7.675316	605.468183	10.509824
6.914996	608.920151	10.514829
7.688717	618.643746	10.519834
7.957223	637.548993	10.524839
7.577846	649.850464	10.529843
7.902398	634.422610	10.534848
7.880099	649.786503	10.539853
7.881027	637.360898	10.544858
7.743669	649.393520	10.549863
7.828374	649.447831	10.554867
7.952568	647.658597	10.559872
7.990757	660.205728	10.564877
8.124685	648.602617	10.569882
8.144809	661.376570	10.574887
7.934039	651.392855	10.579891
8.075735	644.059124	10.584896
7.747965	654.660208	10.589901
8.400718	658.908728	10.594906
8.632804	676.245952	10.599911
8.481449	677.407146	10.604915
8.548842	679.017603	10.609920
8.420262	682.684236	10.614925
8.434430	685.977999	10.619930
8.651215	682.081260	10.624935
8.533698	687.493490	10.629939
8.620626	675.544596	10.634944
8.579840	683.139825	10.639949
8.453668	679.457068	10.644954
8.471585	674.601669	10.649959
8.629914	686.483076	10.654963
8.742665	668.720253	10.659968
8.482399	691.781823	10.664973
8.981251	707.138352	10.669978
9.554990	706.501195	10.674983
9.127913	728.144857	10.679987
9.311613	721.327967	10.684992
9.318920	737.483637	10.689997
9.321564	716.289319	10.695002
9.171709	722.578825	10.700007
9.331311	721.428945	10.705011
9.701475	728.198517	10.710016
9.239466	721.339527	10.715021
9.353964	729.307428	10.720026
9.786193	721.000017	10.725031
9.548165	732.572496	10.730035
9.585840	729.860286	10.735040
9.510239	740.853322	10.740045
9.611397	739.422586	10.745050
9.707908	735.163371	10.750055
9.553625	743.226192	10.755059
9.957600	733.314693	10.760064
9.383428	729.837426	10.765069
9.673347	742.213584	10.770074
9.549102	733.143316	10.775079
9.607715	741.888159	10.780083
9.719257	740.763291	10.785088
10.024013	757.805153	10.790093
10.221867	769.024271	10.795098
10.327406	770.827362	10.800103
10.092981	769.536885	10.805107
10.815826	766.305354	10.810112
10.233220	760.796608	10.815117
10.272318	752.225433	10.820122
10.508365	762.332944	10.825127
10.701169	758.996708	10.830131
10.557313	743.857927	10.835136
10.133550	750.604318	10.840141
10.384598	756.489254	10.845146
10.468096	770.713542	10.850151
10.384410	780.384753	10.855155
10.662891	776.782520	10.860160
10.476367	778.174850	10.865165
10.774286	778.433290	10.870170
10.838011	778.200771	10.875175
10.537929	780.152141	10.880179
10.536904	783.024123	10.885184
10.724250	786.723977	10.890189
10.734465	789.837033	10.895194
11.025324	798.327234	10.900199
10.840644	812.963367	10.905203
11.129425	801.160383	10.910208
11.130667	810.466385	10.915213
11.576604	811.010320	10.920218
11.358505	807.187642	10.925223
11.296943	810.480895	10.930227
11.395989	808.550563	10.935232
11.383552	818.841257	10.940237
11.596410	806.097838	10.945242
11.494143	804.439327	10.950247
11.354609	816.062399	10.955251
11.421875	811.699009	10.960256
11.751105	813.873308	10.965261
11.818586	815.352870	10.970266
11.779235	817.070260	10.975271
11.844117	812.617358	10.980275
12.094682	809.368098	10.985280
12.010472	816.129753	10.990285
12.252470	806.121029	10.995290
12.265086	806.830277	11.000295
11.686198	796.911483	11.005299
12.057282	801.063037	11.010304
11.793025	811.654104	11.015309
12.015527	818.846265	11.020314
11.806249	821.396632	11.025319
11.921993	818.843853	11.030323
12.357952	830.808839	11.035328
12.045350	822.113933	11.040333
12.120753	821.461631	11.045338
11.958166	821.128003	11.050343
12.198354	827.432620	11.055347
12.358929	822.346247	11.060352
12.196217	816.032447	11.065357
12.360142	837.949463	11.070362
12.449264	854.759310	11.075367
12.584536	858.399674	11.080371
12.687446	846.914900	11.085376
12.396651	855.764429	11.090381
12.680714	847.412765	11.095386
12.744780	846.664493	11.100391
12.389682	846.834686	11.105395
12.803262	851.993525	11.110400
12.607890	850.745700	11.115405
12.588451	853.139630	11.120410
13.181994	863.237504	11.125415
13.111428	872.767903	11.130419
13.663914	864.878076	11.135424
13.345950	868.004066	11.140429
13.053697	855.617151	11.145434
13.476240	847.199242	11.150439
13.107083	848.925080	11.155443
13.467588	850.605508	11.160448
13.120131	842.895502	11.165453
12.847998	850.611301	11.170458
13.332393	873.092310	11.175463
13.252623	880.529845	11.180467
13.418555	868.561884	11.185472
13.143955	883.715511	11.190477
13.427016	883.053742	11.195482
13.605946	883.473099	11.200487
13.401481	881.195323	11.205491
14.194620	884.998869	11.210496
13.856199	888.271638	11.215501
13.950211	882.867831	11.220506
14.061084	883.996680	11.225511
13.954458	887.705598	11.230515
14.053441	885.874621	11.235520
13.899827	886.747589	11.240525
13.942018	884.597642	11.245530
13.951133	884.443222	11.250535
13.729915	900.145055	11.255539
14.370581	905.479021	11.260544
14.501621	906.897989	11.265549
14.188922	910.680784	11.270554
14.598229	905.048473	11.275559
14.249173	910.862016	11.280563
14.787647	905.702725	11.285568
14.801026	900.321235	11.290573
14.531365	885.777999	11.295578
14.511171	883.145958	11.300583
14.578819	888.076113	11.305587
14.613264	884.090123	11.310592
14.336383	884.189490	11.315597
14.719307	906.193115	11.320602
15.175803	909.264982	11.325607
14.861598	907.924133	11.330611
15.012941	898.322495	11.335616
14.802851	899.630279	11.340621
14.845613	902.783903	11.345626
14.950122	912.322677	11.350631
15.024571	910.650162	11.355635
14.957783	907.050922	11.360640
15.205816	921.219151	11.365645
15.392741	916.931270	11.370650
15.301388	908.601598	11.375655
15.181923	919.425134	11.380659
15.382668	906.535314	11.385664
15.428185	916.619701	11.390669
15.370177	916.991687	11.395674
15.496213	906.252284	11.400679
15.314734	913.562545	11.405683
15.766489	906.546686	11.410688
15.759258	921.287099	11.415693
15.680028	913.097427	11.420698
15.750427	908.925911	11.425703
15.498870	917.537390	11.430707
15.841781	908.868777	11.435712
15.867984	918.604561	11.440717
15.821943	916.885026	11.445722
15.683596	914.364871	11.450727
15.974166	922.076122	11.455731
16.067115	917.050968	11.460736
15.809166	921.774426	11.465741
15.802354	919.840462	11.470746
16.060880	918.113354	11.475751
15.885274	917.756567	11.480755
16.177784	912.658583	11.485760
16.249932	916.939856	11.490765
15.878237	916.332049	11.495770
15.852550	917.086838	11.500775
15.886284	924.048943	11.505779
16.489083	942.354030	11.510784
16.299075	951.479299	11.515789
16.502174	952.300109	11.520794
16.176833	944.383079	11.525799
16.421988	953.044676	11.530803
16.626543	950.425667	11.535808
16.674815	956.336718	11.540813
16.918821	953.167326	11.545818
16.772228	944.631963	11.550823
16.733211	950.777723	11.555827
16.979320	943.189052	11.560832
16.599018	949.449173	11.565837
16.693823	958.887015	11.570842
17.004758	946.850128	11.575847
16.849528	956.335733	11.580851
17.071452	957.013182	11.585856
16.673999	962.113744	11.590861
16.647817	962.384453	11.595866
16.778181	974.702674	11.600871
17.082259	974.288304	11.605875
17.311786	979.487584	11.610880
17.196344	975.574364	11.615885
17.409374	979.856843	11.620890
17.748263	972.354291	11.625895
17.685523	972.492049	11.630899
17.957519	971.336841	11.635904
17.536072	980.708792	11.640909
17.530101	977.500411	11.645914
17.672770	971.175687	11.650919
17.476823	972.022293	11.655923
17.753113	972.997024	11.660928
17.963716	974.789692	11.665933
18.120274	967.163248	11.670938
18.368273	969.052460	11.675943
17.941432	974.257069	11.680947
17.933697	968.787451	11.685952
17.894409	972.875186	11.690957
18.001288	984.995296	11.695962
18.203992	969.143366	11.700967
17.846855	976.081099	11.705971
18.411912	962.746742	11.710976
17.984586	974.855844	11.715981
17.918546	973.823941	11.720986
18.239079	968.223113	11.725991
17.964442	977.249924	11.730995
18.262962	960.584723	11.736000
17.723178	976.512502	11.741005
17.612999	974.495661	11.746010
18.282305	988.286083	11.751015
18.396541	996.664212	11.756019
18.578701	1004.536311	11.761024
18.592413	1001.119766	11.766029
18.818476	994.295992	11.771034
18.984053	1005.086747	11.776039
18.718722	1016.050322	11.781043
18.969666	1004.843035	11.786048
18.747863	1012.782722	11.791053
18.822782	1010.402014	11.796058
18.793617	1001.617635	11.801063
18.904347	995.566097	11.806067
18.734810	986.009270	11.811072
18.340397	1005.004958	11.816077
18.700272	1003.958743	11.821082
19.566177	1025.882365	11.826087
19.341957	1020.207539	11.831091
19.894364	1018.646454	11.836096
19.516802	1008.403644	11.841101
19.517751	1000.880853	11.846106
19.605799	989.712175	11.851111
19.146626	997.011570	11.856115
19.420718	996.385923	11.861120
19.508336	989.570039	11.866125
19.179955	991.183724	11.871130
19.568828	996.794446	11.876135
19.689959	1010.766944	11.881139
19.615955	1013.163294	11.886144
19.764414	1026.446998	11.891149
20.062088	1022.174540	11.896154
19.842940	997.709633	11.901159
19.374276	1004.581581	11.906163
19.777583	1006.830835	11.911168
20.146103	1018.603291	11.916173
19.820426	1019.819125	11.921178
20.383433	1020.707127	11.926183
19.993242	1023.428319	11.931187
20.138976	1029.737050	11.936192
20.112580	1025.396421	11.941197
19.928058	1020.032256	11.946202
20.123491	1018.903450	11.951207
19.987884	1030.732664	11.956211
20.134359	1023.580921	11.961216
19.964616	1021.736012	11.966221
20.422596	1021.352293	11.971226
20.607914	1025.678632	11.976231
20.294171	1017.449027	11.981235
20.628988	1019.829064	11.986240
20.494155	1034.186211	11.991245
20.623553	1040.570098	11.996250
20.795410	1051.719460	12.001255
20.564641	1069.537863	12.006259
21.207040	1057.490601	12.011264
20.875516	1052.753891	12.016269
20.641198	1050.037690	12.021274
20.366465	1057.968495	12.026279
20.922190	1051.385454	12.031283
20.900818	1050.537248	12.036288
20.962237	1058.740896	12.041293
20.981788	1056.346932	12.046298
21.242224	1057.910872	12.051303
20.713909	1047.805627	12.056307
21.168384	1036.696752	12.061312
20.907431	1034.852194	12.066317
20.878079	1030.053105	12.071322
21.014698	1011.923329	12.076327
20.919432	1016.920515	12.081331
20.956123	1018.171602	12.086336
20.526500	1022.641753	12.091341
20.451880	1014.866059	12.096346
21.039692	1032.467122	12.101351
20.791897	1044.000401	12.106355
21.003589	1044.149588	12.111360
21.045232	1035.429595	12.116365
20.967600	1030.983585	12.121370
20.962172	1020.782347	12.126375
21.024852	1034.480316	12.131379
21.039141	1022.784016	12.136384
21.187192	1028.053083	12.141389
20.808164	1032.365345	12.146394
21.306884	1018.380723	12.151399
20.982546	1028.667690	12.156403
21.144229	1016.982582	12.161408
21.209970	1030.978128	12.166413
20.845585	1029.143759	12.171418
20.953317	1026.402973	12.176423
21.044722	1029.891093	12.181427
21.017222	1014.883292	12.186432
20.852197	1020.695915	12.191437
20.736586	1005.929276	12.196442
20.947011	1010.466088	12.201447
20.880345	1012.847074	12.206451
21.037725	1006.449020	12.211456
20.892271	996.180238	12.216461
20.979349	1003.756819	12.221466
20.865215	996.622998	12.226471
20.838364	997.906296	12.231475
20.811009	998.719707	12.236480
20.766732	1002.961223	12.241485
20.937903	1004.045770	12.246490
20.949516	997.639426	12.251495
20.629518	1000.119167	12.256499
20.782854	1002.313664	12.261504
20.588382	993.516227	12.266509
20.990002	1019.303598	12.271514
21.020308	1011.719345	12.276519
20.856086	1010.146391	12.281523
21.007146	1000.983157	12.286528
20.955643	1003.834846	12.291533
20.715443	1006.328670	12.296538
21.229002	993.305298	12.301543
20.604269	1003.431985	12.306547
21.095706	1000.481761	12.311552
21.090487	1010.941764	12.316557
20.985185	1000.297540	12.321562
20.996269	1005.796618	12.326567
21.074510	1008.255425	12.331571
21.127187	1006.259917	12.336576
20.932523	1001.455662	12.341581
21.396151	1009.793845	12.346586
21.455610	1009.861647	12.351591
21.138694	989.162633	12.356595
20.795891	987.943040	12.361600
20.612304	977.459563	12.366605
20.503940	976.391830	12.371610
20.726847	994.096780	12.376615
20.681826	1004.402266	12.381619
21.063840	1010.539252	12.386624
21.226161	1006.524949	12.391629
20.790119	1007.148056	12.396634
20.966567	984.197152	12.401639
20.648381	983.930917	12.406643
21.109682	988.389860	12.411648
21.052794	998.167337	12.416653
20.804582	984.420156	12.421658
20.938167	975.824317	12.426663
20.705165	990.856295	12.431667
21.180359	973.032140	12.436672
20.532796	975.799104	12.441677
20.461244	984.350371	12.446682
20.951339	995.770657	12.451687
21.001744	1012.025423	12.456691
21.056900	1001.338258	12.461696
20.950415	987.551123	12.466701
20.913459	985.636151	12.471706
20.780190	975.414330	12.476711
20.932441	989.124781	12.481715
21.043619	981.163342	12.486720
21.122802	985.896133	12.491725
20.560901	987.196953	12.496730
20.995985	984.490703	12.501735
20.748113	980.100249	12.506739
20.673335	981.200364	12.511744
20.799825	984.588253	12.516749
20.635348	987.101538	12.521754
20.838907	984.766555	12.526759
20.657197	991.182691	12.531763
21.122917	1003.751826	12.536768
21.004896	1001.274149	12.541773
20.903102	987.782755	12.546778
21.090847	983.497877	12.551783
20.842287	991.255725	12.556787
20.860146	991.424786	12.561792
20.878811	989.141370	12.566797
20.753877	989.733783	12.571802
21.010637	982.059807	12.576807
20.734746	996.679130	12.581811
20.904932	978.279094	12.586816
20.983887	987.058690	12.591821
20.781527	991.446850	12.596826
21.156260	987.639966	12.601831
20.640661	989.117918	12.606835
20.902506	992.246083	12.611840
21.096347	999.699969	12.616845
21.260285	987.066703	12.621850
21.152002	988.342487	12.626855
20.718011	995.729335	12.631859
21.084405	987.284030	12.636864
20.968664	991.221526	12.641869
20.931367	1002.162915	12.646874
20.993120	996.287935	12.651879
21.142082	996.473937	12.656883
21.231032	990.108883	12.661888
20.844199	979.101114	12.666893
21.012593	973.287988	12.671898
20.724309	973.370248	12.676903
20.620080	969.737538	12.681907
21.101891	973.969261	12.686912
20.998164	972.042861	12.691917
20.834683	984.152471	12.696922
20.966257	968.731387	12.701927
20.807178	976.638971	12.706931
20.901324	971.039554	12.711936
20.889673	976.438160	12.716941
20.626953	982.206420	12.721946
21.052988	972.234467	12.726951
20.930115	980.809689	12.731955
20.493682	972.156520	12.736960
20.878832	980.945629	12.741965
20.789064	989.950847	12.746970
21.127719	980.347667	12.751975
20.765400	981.553572	12.756979
20.841366	978.821015	12.761984
20.879777	976.231653	12.766989
20.724377	982.266669	12.771994
20.769816	982.601656	12.776999
20.857183	1002.080361	12.782003
20.799863	1006.341306	12.787008
20.951255	1006.547422	12.792013
20.781435	1006.050927	12.797018
21.002817	1008.794434	12.802023
20.831059	1001.363849	12.807027
20.857651	994.470956	12.812032
21.046105	992.813368	12.817037
20.639357	988.536566	12.822042
21.067198	985.700575	12.827047
20.972666	989.585798	12.832051
20.901480	982.774743	12.837056
20.933163	985.444414	12.842061
21.039755	991.833494	12.847066
20.890311	982.675618	12.852071
20.825061	995.250577	12.857075
20.930476	982.448440	12.862080
20.888173	987.400896	12.867085
20.618795	989.684889	12.872090
20.662636	983.803309	12.877095
20.578321	988.248340	12.882099
20.860638	1001.076976	12.887104
20.860382	996.613906	12.892109
20.834314	1000.412513	12.897114
21.193738	990.187801	12.902119
20.872889	995.189417	12.907123
20.896401	981.859406	12.912128
21.058010	988.794840	12.917133
21.068498	995.197672	12.922138
20.976611	995.075131	12.927143
20.773751	991.582734	12.932147
20.929655	992.355877	12.937152
20.963287	989.603259	12.942157
20.863441	985.499878	12.947162
20.964556	995.252153	12.952167
20.691008	991.515544	12.957171
20.924420	982.198828	12.962176
20.782843	989.501186	12.967181
20.950255	988.876783	12.972186
21.084905	983.602086	12.977191
21.100619	987.023414	12.982195
21.005662	984.147793	12.987200
21.028007	978.755381	12.992205
20.906008	989.708694	12.997210
21.269463	986.950785	13.002215
21.113356	994.056752	13.007219
21.123515	986.150848	13.012224
20.519154	976.518287	13.017229
20.755295	984.042696	13.022234
21.386076	978.493315	13.027239
20.971647	973.514369	13.032243
20.688486	957.195853	13.037248
20.780654	957.061304	13.042253
20.590197	960.688986	13.047258
20.934878	977.737358	13.052263
20.745414	984.795020	13.057267
20.694412	984.419935	13.062272
21.035699	980.700394	13.067277
20.820421	984.918712	13.072282
20.755597	978.340051	13.077287
20.496697	982.022812	13.082291
20.487819	983.219658	13.087296
20.856557	986.027975	13.092301
20.741544	991.331100	13.097306
21.148978	986.099634	13.102311
20.295997	987.934194	13.107315
20.787613	984.709533	13.112320
20.871451	984.857032	13.117325
20.805455	993.628209	13.122330
20.792084	991.761518	13.127335
20.718357	993.736743	13.132339
20.869406	985.824140	13.137344
21.239543	996.385128	13.142349
20.931039	995.021282	13.147354
20.976376	989.341326	13.152359
20.958735	993.944472	13.157363
20.792931	993.534076	13.162368
20.979782	991.835740	13.167373
20.928031	990.128146	13.172378
20.857366	999.803735	13.177383
21.004801	993.665913	13.182387
20.914748	994.465667	13.187392
20.967431	987.526035	13.192397
20.863775	1002.767649	13.197402
20.951115	990.204949	13.202407
20.745743	999.156066	13.207411
20.985169	991.833383	13.212416
21.073834	995.772975	13.217421
20.610334	996.047196	13.222426
21.153877	993.117051	13.227431
20.992283	992.496232	13.232435
20.900591	989.610627	13.237440
21.088829	989.512799	13.242445
21.046626	983.209670	13.247450
20.888614	964.822568	13.252455
20.637403	966.726740	13.257459
20.850642	968.233538	13.262464
20.599374	960.351996	13.267469
20.552622	991.788928	13.272474
20.882626	985.421702	13.277479
20.891452	999.278050	13.282483
20.707925	997.340718	13.287488
20.876680	1003.319312	13.292493
21.100826	995.704151	13.297498
21.002997	984.842687	13.302503
21.025771	994.840864	13.307507
20.864527	985.052462	13.312512
21.007191	968.869460	13.317517
20.736409	973.279567	13.322522
20.573350	965.008610	13.327527
20.749993	983.712904	13.332531
20.925846	987.573928	13.337536
21.011023	995.564000	13.342541
21.060530	998.372768	13.347546
21.088760	981.596098	13.352551
20.627166	978.982396	13.357555
20.556483	966.474884	13.362560
21.022296	978.903623	13.367565
20.823625	993.742457	13.372570
21.090411	989.385043	13.377575
20.731045	981.181659	13.382579
20.667967	974.426089	13.387584
20.995407	984.282619	13.392589
20.982437	997.847529	13.397594
21.147200	976.560737	13.402599
20.756660	972.404367	13.407603
20.908065	970.121861	13.412608
20.701778	971.821735	13.417613
20.689937	971.339472	13.422618
20.846404	973.725868	13.427623
20.887969	988.567385	13.432627
21.009519	987.100255	13.437632
20.755084	971.679227	13.442637
20.734894	976.442058	13.447642
21.001251	985.073484	13.452647
20.745366	980.485596	13.457651
20.877627	988.701562	13.462656
21.043283	994.439354	13.467661
20.741167	988.333807	13.472666
20.663988	983.200136	13.477671
20.976979	996.441800	13.482675
21.124965	989.468042	13.487680
21.122210	973.984792	13.492685
20.748854	979.575140	13.497690
20.929770	960.957354	13.502695
20.463610	975.135458	13.507699
20.333333	977.654327	13.512704
21.079609	989.596764	13.517709
20.833890	997.984992	13.522714
21.166409	1006.315696	13.527719
20.807629	992.288075	13.532723
20.917959	978.207728	13.537728
20.948979	976.945863	13.542733
20.549208	981.840204	13.547738
21.034986	987.463854	13.552743
20.654013	1004.594875	13.557747
21.048716	1008.780573	13.562752
21.073810	1002.924053	13.567757
20.878144	990.999470	13.572762
20.846406	982.412646	13.577767
20.375268	979.455087	13.582771
21.097930	987.692015	13.587776
20.776595	989.728809	13.592781
20.900989	997.524956	13.597786
21.150116	1000.182029	13.602791
20.935266	987.710109	13.607795
20.518983	978.139020	13.612800
20.952071	979.691185	13.617805
20.802619	984.116640	13.622810
20.777977	986.989275	13.627815
20.656883	994.102273	13.632819
20.718028	996.552766	13.637824
20.737451	999.289055	13.642829
20.943533	1014.107513	13.647834
21.068696	1007.165774	13.652839
21.163658	1010.200701	13.657843
20.834395	998.338423	13.662848
20.791955	982.522423	13.667853
20.541465	999.373986	13.672858
21.233451	1005.969352	13.677863
20.841934	1011.930066	13.682867
20.804649	993.238223	13.687872
21.190482	999.760980	13.692877
20.795455	992.530024	13.697882
20.891884	983.471715	13.702887
20.502295	977.875325	13.707891
20.737910	1001.003385	13.712896
21.093447	1005.305724	13.717901
21.041850	997.195182	13.722906
20.664583	977.863670	13.727911
20.620550	984.204225	13.732915
20.703676	1007.638913	13.737920
21.046605	1015.004369	13.742925
21.076855	1016.142933	13.747930
20.893591	986.660373	13.752935
20.707918	995.378093	13.757939
20.866048	995.245641	13.762944
21.008585	994.060613	13.767949
21.069475	1003.067044	13.772954
21.104875	984.063976	13.777959
20.743002	988.294635	13.782963
20.970594	987.797840	13.787968
21.236153	977.895636	13.792973
20.754194	972.823374	13.797978
20.951592	982.292182	13.802983
20.690589	987.926119	13.807987
20.464527	981.338476	13.812992
20.728414	985.075064	13.817997
21.059919	991.240600	13.823002
21.164697	984.338396	13.828007
20.947828	987.265346	13.833011
20.928723	989.149850	13.838016
20.925803	982.553428	13.843021
20.694823	990.821021	13.848026
20.987064	981.209472	13.853031
20.853357	988.925344	13.858035
20.840322	992.718717	13.863040
20.981665	988.408120	13.868045
20.717090	984.648003	13.873050
21.110909	976.602061	13.878055
21.009133	997.631224	13.883059
21.230117	989.871480	13.888064
21.212290	986.119321	13.893069
21.049843	986.791839	13.898074
21.208509	984.612260	13.903079
20.965809	983.491829	13.908083
20.786770	973.520178	13.913088
21.026213	973.575045	13.918093
20.798335	974.674345	13.923098
20.912776	967.937777	13.928103
20.555556	966.353029	13.933107
20.498830	974.651172	13.938112
20.929387	981.270873	13.943117
20.846179	990.208809	13.948122
21.142522	979.319178	13.953127
21.296833	982.505495	13.958131
20.793138	978.285163	13.963136
21.079628	962.580738	13.968141
20.522968	963.344515	13.973146
20.999782	960.338279	13.978151
20.758213	958.738241	13.983155
20.656515	948.803161	13.988160
20.774704	963.533076	13.993165
20.942534	980.784713	13.998170
21.350573	979.573111	14.003175
20.858927	971.901802	14.008179
20.842009	960.603219	14.013184
20.974628	955.937606	14.018189
20.673778	956.276456	14.023207
20.649105	953.129588	14.028224
20.810141	968.905172	14.033242
20.647386	979.286517	14.038259
20.914715	989.086461	14.043277
21.101850	989.934386	14.048295
21.154486	985.342132	14.053312
21.141999	994.499285	14.058330
20.976309	977.327566	14.063347
20.915122	969.198381	14.068365
20.832240	982.864099	14.073383
21.177340	984.366386	14.078400
21.265908	990.561098	14.083418
21.138634	976.719693	14.088435
20.754531	974.175994	14.093453
21.019803	994.476373	14.098471
21.038489	988.403000	14.103488
21.055627	990.827492	14.108506
21.386329	991.990724	14.113523
21.226262	982.297960	14.118541
20.910509	990.652459	14.123559
21.201336	980.850028	14.128576
21.099613	993.524594	14.133594
21.112563	986.294372	14.138611
21.226590	979.760623	14.143629
21.329033	993.241062	14.148647
21.191840	989.504934	14.153664
21.135160	997.931377	14.158682
21.215160	990.031350	14.163699
21.212469	994.194080	14.168717
20.887969	994.878210	14.173735
21.312807	985.101595	14.178752
21.151197	1003.591849	14.183770
21.132497	1014.779242	14.188787
21.680804	1023.463147	14.193805
21.468666	1026.205789	14.198823
21.552685	1028.216919	14.203840
21.297053	1032.860457	14.208858
21.426900	1033.126052	14.213875
21.874857	1024.014272	14.218893
21.690644	1029.981941	14.223911
21.790514	1030.131192	14.228928
21.807369	1030.523350	14.233946
21.624913	1036.290963	14.238963
21.671626	1032.058296	14.243981
21.505467	1042.671468	14.248999
21.561836	1031.193340	14.254016
21.481448	1025.080696	14.259034
21.243420	1032.589104	14.264051
21.499305	1030.191866	14.269069
21.500026	1030.415133	14.274087
21.424647	1032.711240	14.279104
21.738199	1040.169433	14.284122
21.490883	1034.674878	14.289139
21.765921	1034.026967	14.294157
21.779618	1050.280752	14.299175
21.949092	1045.890072	14.304192
21.865368	1053.446241	14.309210
21.719849	1058.632233	14.314227
22.188390	1046.641607	14.319245
22.142244	1063.721367	14.324263
21.919480	1044.408301	14.329280
21.802871	1042.715423	14.334298
21.844176	1052.829890	14.339315
21.760015	1059.818258	14.344333
21.615805	1058.098319	14.349351
22.105756	1061.666533	14.354368
22.084563	1048.324104	14.359386
21.835641	1055.105936	14.364403
21.983704	1056.079649	14.369421
21.990851	1057.642137	14.374439
22.070715	1047.487909	14.379456
21.923102	1057.078794	14.384474
22.005152	1063.304464	14.389491
22.049763	1049.948392	14.394509
22.008300	1059.932916	14.399527
22.128738	1083.070719	14.404544
22.188188	1086.616363	14.409562
22.440750	1081.872640	14.414579
22.751686	1080.990908	14.419597
22.486603	1072.873735	14.424615
22.271050	1062.327730	14.429632
22.156230	1056.690909	14.434650
22.103999	1053.452458	14.439667
22.426482	1071.997727	14.444685
22.403601	1084.595302	14.449703
22.589729	1085.742274	14.454720
22.790443	1082.018298	14.459738
22.225473	1069.204607	14.464755
22.944527	1062.877926	14.469773
22.191596	1065.318281	14.474791
22.078141	1064.998178	14.479808
22.641931	1082.229223	14.484826
22.461038	1089.319552	14.489843
22.933151	1090.381586	14.494861
22.502845	1087.681638	14.499879
22.570357	1082.704727	14.504896
22.652622	1082.452510	14.509914
22.519496	1088.552057	14.514931
22.577785	1082.780649	14.519949
22.570685	1080.083992	14.524967
22.944448	1088.624311	14.529984
23.159594	1082.727209	14.535002
22.714977	1088.171705	14.540019
22.988559	1084.810495	14.545037
22.783696	1086.373766	14.550055
23.140556	1088.525436	14.555072
22.919257	1071.913046	14.560090
22.840193	1079.792535	14.565107
22.939940	1072.743486	14.570125
22.859459	1077.846751	14.575143
22.867175	1083.470792	14.580160
23.220956	1074.289056	14.585178
22.733935	1073.827181	14.590195
22.697833	1074.459025	14.595213
22.965531	1082.475125	14.600231
22.887548	1086.255051	14.605248
22.884943	1097.669608	14.610266
23.018211	1089.062592	14.615283
23.172748	1090.074601	14.620301
22.851471	1093.254670	14.625319
23.133807	1093.860896	14.630336
23.290934	1090.949277	14.635354
23.068054	1090.270663	14.640371
23.204244	1085.852246	14.645389
23.109287	1085.810770	14.650407
23.157598	1085.312278	14.655424
23.361440	1086.697104	14.660442
22.852491	1096.075077	14.665459
23.290457	1091.031214	14.670477
22.932033	1090.185451	14.675495
22.734219	1101.991377	14.680512
23.383113	1096.125767	14.685530
23.168533	1098.871958	14.690547
23.536820	1110.788955	14.695565
23.133303	1104.419493	14.700583
23.754588	1114.543751	14.705600
23.371712	1103.975637	14.710618
23.371080	1117.324762	14.715635
23.786636	1109.316096	14.720653
23.602076	1105.960308	14.725671
23.157803	1093.649602	14.730688
23.568373	1105.501648	14.735706
23.606142	1112.358907	14.740723
23.967944	1111.950419	14.745741
24.253672	1090.190305	14.750759
24.122663	1089.388498	14.755776
23.868634	1078.057368	14.760794
23.824057	1082.914231	14.765811
24.084746	1070.783699	14.770829
23.919550	1078.703667	14.775847
23.922694	1078.946999	14.780864
24.110397	1064.171215	14.785882
24.058031	1070.983054	14.790899
23.733018	1050.279973	14.795917
23.708709	1042.888921	14.800935
23.985660	1040.581131	14.805952
24.293855	1038.933761	14.810970
23.793643	1042.453822	14.815987
23.857122	1044.819022	14.821005
23.909526	1051.656615	14.826023
23.420246	1052.153092	14.831040
23.901307	1065.508717	14.836058
23.874512	1066.807626	14.841075
24.299257	1074.414847	14.846093
23.902913	1060.866392	14.851111
23.716051	1079.459872	14.856128
23.961033	1076.359635	14.861146
24.086408	1085.866100	14.866163
24.213275	1074.650406	14.871181
24.127947	1082.173812	14.876199
24.156838	1074.176496	14.881216
24.331146	1079.695313	14.886234
24.014218	1082.435802	14.891251
24.273763	1078.192772	14.896269
24.204742	1074.546426	14.901287
24.180912	1084.889958	14.906304
24.323306	1069.841390	14.911322
24.150392	1083.301333	14.916339
24.498469	1077.843939	14.921357
24.416833	1088.387034	14.926375
23.943457	1085.706539	14.931392
24.438205	1095.558376	14.936410
24.230241	1082.124578	14.941427
24.366118	1081.873249	14.946445
24.335830	1087.232787	14.951463
24.164493	1083.533541	14.956480
24.227313	1081.974067	14.961498
24.235125	1080.067854	14.966515
24.361666	1079.193509	14.971533
24.310136	1074.891553	14.976551
24.207215	1088.146851	14.981568
24.572371	1085.120256	14.986586
24.471876	1097.160773	14.991603
24.804047	1108.419696	14.996621
24.822984	1110.581220	15.001639
24.708498	1097.050700	15.006656
24.957987	1084.662387	15.011674
24.602914	1077.501826	15.016691
24.419119	1081.602228	15.021709
24.793028	1082.544642	15.026727
24.490847	1098.630204	15.031744
24.952159	1106.222172	15.036762
24.771824	1100.155325	15.041779
24.754100	1104.940270	15.046797
25.010802	1093.930376	15.051815
24.808012	1113.270498	15.056832
24.871254	1099.994780	15.061850
25.208375	1108.677812	15.066867
24.783371	1112.703432	15.071885
24.778788	1102.501285	15.076903
25.034305	1105.594082	15.081920
24.889135	1107.784925	15.086938
25.032375	1107.456915	15.091955
25.125471	1105.563838	15.096973
24.997715	1102.293376	15.101991
24.935593	1109.116228	15.107008
24.985463	1096.410522	15.112026
24.822330	1111.048728	15.117043
24.870767	1106.666323	15.122061
25.371946	1098.164222	15.127079
24.617978	1108.308036	15.132096
25.332003	1107.159090	15.137114
25.258616	1103.974340	15.142131
25.373560	1104.671760	15.147149
25.436685	1111.266992	15.152167
24.950581	1102.019413	15.157184
25.151920	1105.970305	15.162202
25.580052	1109.683675	15.167219
25.082334	1124.186488	15.172237
25.844964	1122.013589	15.177255
25.413071	1113.089273	15.182272
25.296822	1115.767873	15.187290
25.251641	1104.307457	15.192307
25.608863	1124.382562	15.197325
25.509432	1122.502886	15.202343
25.693235	1140.716422	15.207360
25.508560	1119.069043	15.212378
25.392011	1125.895864	15.217395
25.487248	1141.682130	15.222413
25.679440	1131.185878	15.227431
25.367026	1139.388914	15.232448
25.595752	1132.613429	15.237466
25.721989	1145.740993	15.242483
25.491418	1133.323809	15.247501
25.599578	1134.454905	15.252519
25.499712	1140.618385	15.257536
25.520953	1147.904598	15.262554
25.775113	1140.749089	15.267571
25.688511	1137.892064	15.272589
25.962393	1130.393632	15.277607
25.813061	1141.351840	15.282624
25.815505	1136.501696	15.287642
25.911234	1133.082322	15.292659
25.641310	1129.829809	15.297677
25.704736	1135.968816	15.302695
25.771647	1139.289907	15.307712
26.381549	1149.447467	15.312730
26.190780	1153.033035	15.317747
26.046314	1150.463669	15.322765
26.145166	1142.312008	15.327783
26.200846	1142.957532	15.332800
26.147750	1137.334431	15.337818
25.833256	1127.763728	15.342835
25.837903	1158.961632	15.347853
26.317971	1159.065978	15.352871
26.130706	1168.419434	15.357888
26.332661	1165.285140	15.362906
26.384565	1159.343255	15.367923
25.907010	1159.292010	15.372941
26.664371	1150.341597	15.377959
26.480501	1173.010538	15.382976
26.448148	1158.114021	15.387994
26.524345	1168.289073	15.393011
26.404134	1157.276321	15.398029
26.779493	1163.415928	15.403047
26.478025	1151.337234	15.408064
26.570539	1146.636320	15.413082
26.369308	1131.609457	15.418099
26.392424	1134.824272	15.423117
26.353527	1137.226264	15.428135
26.422964	1153.952633	15.433152
26.425590	1153.749297	15.438170
26.615781	1162.287477	15.443187
26.320583	1167.786824	15.448205
26.935908	1162.348126	15.453223
26.638496	1163.816050	15.458240
26.867624	1153.974579	15.463258
27.046698	1158.432418	15.468275
26.888441	1160.755921	15.473293
27.046313	1145.645029	15.478311
27.047441	1140.327892	15.483328
26.850709	1123.407922	15.488346
27.001879	1123.374382	15.493363
26.808131	1131.471970	15.498381
26.888510	1121.772225	15.503399
26.958885	1134.614526	15.508416
26.878510	1123.552973	15.513434
26.782394	1128.957633	15.518451
26.745728	1142.748267	15.523469
26.961570	1148.114191	15.528487
27.278824	1156.138159	15.533504
27.107518	1148.693417	15.538522
27.089963	1140.914263	15.543539
27.057502	1138.487488	15.548557
27.424536	1141.243175	15.553575
26.933582	1130.717447	15.558592
26.841023	1133.192493	15.563610
27.414925	1147.441045	15.568627
27.400615	1158.130760	15.573645
27.280694	1151.601212	15.578663
26.988271	1150.431878	15.583680
27.107923	1157.537229	15.588698
27.267237	1159.934354	15.593715
27.003820	1152.973075	15.598733
27.368783	1157.634081	15.603751
27.117335	1146.075964	15.608768
26.986051	1160.455876	15.613786
27.455192	1148.814292	15.618803
27.170873	1156.289246	15.623821
27.273722	1149.467760	15.628839
27.377298	1158.776397	15.633856
27.813302	1160.421513	15.638874
27.598304	1157.635300	15.643891
27.594918	1154.234875	15.648909
27.215062	1146.458444	15.653927
27.266476	1168.337927	15.658944
27.448014	1181.371758	15.663962
28.065537	1170.148525	15.668979
28.061483	1181.297530	15.673997
27.832379	1177.730174	15.679015
27.922380	1182.991908	15.684032
28.032072	1163.342507	15.689050
28.006304	1154.466654	15.694067
27.800448	1157.522931	15.699085
27.861955	1133.339808	15.704103
28.021032	1134.867062	15.709120
27.612801	1140.541733	15.714138
27.886063	1138.912509	15.719155
27.639192	1151.187207	15.724173
27.781504	1153.498951	15.729191
27.809203	1171.924619	15.734208
28.241318	1167.155378	15.739226
28.213542	1174.861567	15.744243
28.059002	1172.781455	15.749261
28.391732	1165.976782	15.754279
28.196394	1165.402314	15.759296
27.820463	1162.753454	15.764314
28.067238	1159.409088	15.769331
28.356553	1171.614018	15.774349
28.259204	1171.498988	15.779367
28.214325	1170.656697	15.784384
28.524053	1169.163230	15.789402
28.124076	1175.870105	15.794419
28.140314	1174.736486	15.799437
28.204468	1167.466546	15.804455
28.613063	1171.256983	15.809472
28.530645	1176.827793	15.814490
28.499550	1168.640212	15.819507
28.173137	1177.119217	15.824525
28.236243	1175.130238	15.829543
28.501209	1172.533322	15.834560
28.400017	1177.010698	15.839578
28.738993	1169.357142	15.844595
28.188712	1183.481422	15.849613
28.422772	1164.940076	15.854631
28.432907	1168.130226	15.859648
28.308323	1173.588207	15.864666
28.718643	1171.073505	15.869683
28.639567	1171.580069	15.874701
28.634143	1168.806048	15.879719
28.681547	1170.914275	15.884736
28.526560	1185.511930	15.889754
28.944547	1188.613441	15.894771
28.714523	1207.359477	15.899789
29.032894	1202.619377	15.904807
28.986197	1200.839036	15.909824
29.017473	1205.229224	15.914842
29.269144	1183.392603	15.919859
28.860428	1181.181563	15.924877
28.942228	1174.253307	15.929895
29.033294	1175.442191	15.934912
28.727963	1176.593619	15.939930
28.871832	1183.932654	15.944947
29.038373	1191.384485	15.949965
29.064904	1205.426230	15.954983
29.352420	1196.973094	15.960000
29.155029	1203.200919	15.965018
29.145405	1206.789070	15.970035
29.490313	1199.998957	15.975053
29.301445	1194.542210	15.980071
29.528195	1195.695298	15.985088
29.481062	1193.343215	15.990106
29.367229	1166.509059	15.995123
29.139220	1172.356353	16.000141
29.106246	1180.554172	16.005159
29.381371	1173.643848	16.010176
29.280711	1193.314650	16.015194
29.528588	1191.997004	16.020211
29.476551	1203.230760	16.025229
29.526907	1202.097990	16.030247
29.564986	1191.257388	16.035264
29.920772	1207.373416	16.040282
29.846684	1191.706423	16.045299
29.812269	1189.777828	16.050317
29.618242	1176.137220	16.055335
29.801178	1168.595070	16.060352
29.349120	1172.972669	16.065370
29.565026	1179.477498	16.070387
29.839748	1189.182015	16.075405
29.387130	1205.484389	16.080423
29.945754	1198.587830	16.085440
29.521855	1213.224467	16.090458
29.522352	1199.017182	16.095475
29.205940	1210.801996	16.100493
29.874236	1201.435522	16.105511
30.082009	1200.571811	16.110528
29.777148	1208.392211	16.115546
29.762668	1202.107741	16.120563
29.689508	1203.497430	16.125581
29.938117	1207.224514	16.130599
29.954448	1220.721257	16.135616
29.660898	1233.558764	16.140634
30.413254	1232.223580	16.145651
30.047708	1234.754765	16.150669
30.176490	1226.800425	16.155687
30.115085	1225.149059	16.160704
30.025301	1236.955954	16.165722
30.273701	1227.462943	16.170739
30.242539	1227.990183	16.175757
30.241171	1235.071614	16.180775
30.360141	1232.136164	16.185792
29.948909	1238.656094	16.190810
30.133718	1233.201086	16.195827
30.302154	1225.475596	16.200845
30.026917	1238.874135	16.205863
30.813017	1228.262642	16.210880
30.339289	1243.311537	16.215898
30.390422	1237.310752	16.220915
30.399508	1237.166948	16.225933
30.601533	1254.860180	16.230951
30.921245	1255.480903	16.235968
30.593565	1244.947142	16.240986
30.561618	1226.971190	16.246003
30.853401	1236.674591	16.251021
30.403589	1231.488330	16.256039
30.912280	1237.483218	16.261056
30.769451	1250.887393	16.266074
30.786942	1234.316959	16.271091
30.739212	1239.023361	16.276109
30.473221	1254.413528	16.281127
30.663836	1251.240125	16.286144
31.215037	1256.829466	16.291162
31.561729	1259.652131	16.296179
31.235956	1238.841931	16.301197
30.818686	1226.196457	16.306215
31.148322	1220.396662	16.311232
30.999473	1233.075020	16.316250
30.791348	1223.561223	16.321267
30.668081	1230.712431	16.326285
30.820984	1244.059996	16.331303
30.832523	1243.892991	16.336320
31.084016	1253.101804	16.341338
31.226174	1250.728961	16.346355
31.242579	1253.035633	16.351373
31.231692	1252.383764	16.356391
31.254283	1253.933585	16.361408
31.127492	1254.115056	16.366426
31.541965	1252.706339	16.371443
31.339606	1251.684659	16.376461
31.382892	1251.418206	16.381479
31.509616	1252.738267	16.386496
31.286313	1258.834177	16.391514
31.451156	1252.862443	16.396531
31.610864	1253.440256	16.401549
31.360674	1260.886224	16.406567
31.463808	1257.331929	16.411584
31.391625	1259.700709	16.416602
31.348917	1256.798906	16.421619
32.056863	1273.531335	16.426637
31.734626	1270.746472	16.431655
31.953133	1258.548577	16.436672
31.568293	1252.150113	16.441690
31.584838	1254.245184	16.446707
31.962404	1265.678682	16.451725
32.243665	1265.482031	16.456743
32.400572	1253.072947	16.461760
32.133001	1249.927000	16.466778
31.958007	1255.444963	16.471795
32.027812	1251.925086	16.476813
31.619679	1254.971171	16.481831
31.672876	1245.842773	16.486848
31.374959	1250.522225	16.491866
31.699131	1272.695789	16.496883
32.217363	1277.781505	16.501901
32.211302	1285.818569	16.506919
32.214085	1279.223775	16.511936
32.165715	1279.976352	16.516954
31.908402	1285.905445	16.521971
32.211313	1267.675469	16.526989
32.311907	1281.509628	16.532007
32.461500	1272.796863	16.537024
32.183443	1272.000407	16.542042
32.400135	1282.245157	16.547059
32.566080	1270.912964	16.552077
32.378251	1277.414584	16.557095
32.575746	1272.437329	16.562112
32.369955	1276.613654	16.567130
32.188352	1273.683660	16.572147
32.131519	1282.334456	16.577165
32.524872	1282.159255	16.582183
32.843291	1277.360920	16.587200
32.560033	1283.211563	16.592218
32.644819	1288.993285	16.597235
32.639097	1266.977358	16.602253
32.375581	1288.457348	16.607271
32.772416	1279.315024	16.612288
32.674584	1281.158557	16.617306
32.793957	1280.078483	16.622323
32.836477	1271.126385	16.627341
32.259272	1285.400566	16.632359
32.732894	1284.229387	16.637376
32.736561	1298.451053	16.642394
33.081354	1305.388431	16.647411
33.581419	1297.388995	16.652429
33.201011	1284.269599	16.657447
33.074653	1264.097692	16.662464
33.228987	1266.666309	16.667482
33.003148	1263.060656	16.672499
33.173956	1262.824990	16.677517
33.015458	1272.887316	16.682535
33.008255	1259.269532	16.687552
32.858565	1273.219107	16.692570
32.941233	1290.826809	16.697587
33.170901	1286.338365	16.702605
33.343692	1300.328560	16.707623
33.444906	1297.223677	16.712640
33.530765	1296.457272	16.717658
33.450193	1294.303995	16.722675
33.638282	1297.426465	16.727693
33.602195	1291.875313	16.732711
33.547776	1282.098642	16.737728
33.544217	1291.267929	16.742746
33.683148	1285.172108	16.747763
34.088766	1279.960303	16.752781
33.425385	1274.631115	16.757799
33.537276	1266.426967	16.762816
33.747520	1270.444127	16.767834
33.566712	1276.151795	16.772851
33.707772	1292.680491	16.777869
33.608615	1294.068042	16.782887
33.876625	1285.644709	16.787904
33.739250	1285.856970	16.792922
33.881390	1290.901209	16.797939
33.880050	1291.785504	16.802957
33.372504	1290.361019	16.807975
33.739452	1283.426561	16.812992
33.974379	1288.201948	16.818010
33.692020	1290.225927	16.823027
33.835404	1295.847290	16.828045
33.894350	1296.471851	16.833063
33.750911	1284.947521	16.838080
34.414364	1290.338069	16.843098
33.999737	1287.213207	16.848115
34.082639	1294.621013	16.853133
34.049790	1298.934937	16.858151
34.066407	1294.766770	16.863168
34.165386	1312.279084	16.868186
34.060126	1313.066692	16.873203
34.378607	1320.488065	16.878221
34.573215	1322.351033	16.883239
34.562106	1323.265990	16.888256
34.536089	1324.611991	16.893274
34.467223	1315.798756	16.898291
34.568582	1321.090978	16.903309
34.272111	1316.184623	16.908327
34.420487	1317.935408	16.913344
34.627064	1316.433996	16.918362
34.369489	1319.059664	16.923379
34.549633	1308.374076	16.928397
34.724679	1322.643155	16.933415
34.519186	1316.517306	16.938432
34.496476	1310.392196	16.943450
34.640541	1319.906846	16.948467
34.557455	1317.868015	16.953485
34.450976	1314.347923	16.958503
34.487943	1323.657064	16.963520
34.883351	1319.147683	16.968538
35.011539	1330.562801	16.973555
35.239495	1332.365393	16.978573
34.908581	1341.485456	16.983591
35.164396	1331.849617	16.988608
35.281064	1347.180427	16.993626
34.698159	1334.380369	16.998643
35.035430	1331.796277	17.003661
35.256016	1347.227708	17.008679
35.280325	1342.482551	17.013696
35.596858	1347.936315	17.018714
35.438921	1348.528611	17.023731
35.198715	1330.990028	17.028749
35.308766	1329.267259	17.033767
35.679358	1327.897783	17.038784
35.482269	1312.728494	17.043802
35.015584	1319.544390	17.048819
35.371759	1325.245877	17.053837
35.352785	1328.230698	17.058855
35.394349	1342.882896	17.063872
35.434884	1343.094313	17.068890
35.317680	1339.822900	17.073907
35.507395	1335.560259	17.078925
35.652629	1351.921609	17.083943
35.461965	1345.481124	17.088960
35.829169	1335.704030	17.093978
35.356935	1344.771912	17.098995
35.680116	1336.460092	17.104013
35.735827	1334.602051	17.109031
35.397646	1344.885000	17.114048
35.310863	1339.831145	17.119066
35.665235	1356.881981	17.124083
35.986940	1352.039838	17.129101
35.841667	1376.523791	17.134119
35.685620	1371.791658	17.139136
36.159194	1365.787944	17.144154
35.997809	1370.373296	17.149171
35.958880	1366.666232	17.154189
35.953676	1363.557070	17.159207
36.117826	1375.874947	17.164224
36.256388	1369.112160	17.169242
35.801150	1377.043152	17.174259
36.080717	1373.271133	17.179277
36.086238	1383.454461	17.184295
36.327751	1368.410227	17.189312
36.714692	1363.198225	17.194330
36.368639	1376.787516	17.199347
36.320047	1375.413313	17.204365
36.413512	1364.356887	17.209383
36.060836	1371.980498	17.214400
36.569056	1383.646520	17.219418
36.280932	1393.165649	17.224435
36.548509	1391.560114	17.229453
36.826714	1396.007723	17.234471
36.709585	1397.543662	17.239488
36.951562	1390.414358	17.244506
36.722458	1392.977294	17.249523
36.747192	1396.206067	17.254541
37.013722	1390.033221	17.259559
36.788446	1401.566904	17.264576
37.055152	1387.743286	17.269594
36.963964	1384.437825	17.274611
36.881361	1379.204744	17.279629
37.322929	1377.389770	17.284647
36.743822	1382.206920	17.289664
37.314232	1364.885883	17.294682
36.961813	1374.579642	17.299699
36.933743	1364.264648	17.304717
37.150385	1378.291972	17.309735
36.962154	1394.008885	17.314752
37.190880	1386.034586	17.319770
37.265699	1393.383954	17.324787
37.245185	1381.467906	17.329805
37.163531	1387.105531	17.334823
36.873343	1388.670642	17.339840
37.148941	1385.992553	17.344858
36.990772	1396.781681	17.349875
37.042055	1391.786803	17.354893
37.110839	1389.816554	17.359911
37.419204	1402.729680	17.364928
37.590700	1408.844489	17.369946
37.433923	1421.215161	17.374963
37.616776	1418.739055	17.379981
37.511263	1424.830406	17.384999
37.377313	1428.463610	17.390016
38.022465	1416.067760	17.395034
37.917373	1422.750527	17.400051
38.147363	1414.094073	17.405069
38.125970	1413.356565	17.410087
37.763645	1393.742805	17.415104
37.688832	1386.552336	17.420122
37.762697	1402.733209	17.425139
38.261916	1405.890244	17.430157
37.995213	1402.641873	17.435175
37.875517	1408.065340	17.440192
38.414557	1396.430504	17.445210
37.977979	1387.155963	17.450227
38.163918	1398.468324	17.455245
37.985109	1402.370596	17.460263
37.849009	1409.262018	17.465280
38.378836	1409.124043	17.470298
37.864036	1419.895343	17.475315
37.768082	1415.195298	17.480333
38.227193	1410.192003	17.485351
38.003833	1416.357203	17.490368
38.390305	1413.093539	17.495386
38.141571	1414.622939	17.500403
38.271750	1418.102326	17.505421
38.267933	1419.046015	17.510439
38.363306	1445.721570	17.515456
38.503906	1433.413253	17.520474
38.313243	1440.503736	17.525491
38.471983	1442.560425	17.530509
38.611691	1434.065442	17.535527
38.592656	1443.295498	17.540544
39.007909	1434.585889	17.545562
38.643196	1440.742181	17.550579
38.830472	1438.953598	17.555597
38.864195	1445.795143	17.560615
38.746704	1444.182586	17.565632
38.759645	1436.969445	17.570650
38.537164	1447.956066	17.575667
38.756635	1465.085175	17.580685
38.944845	1463.110814	17.585703
38.918887	1472.983818	17.590720
39.361478	1468.397651	17.595738
39.287575	1469.674220	17.600755
39.174742	1470.851601	17.605773
39.102757	1466.760440	17.610791
39.379333	1469.993111	17.615808
39.334743	1465.013498	17.620826
39.583097	1466.694085	17.625843
39.674477	1469.879210	17.630861
39.379864	1443.675871	17.635879
39.285253	1452.941583	17.640896
39.085834	1459.756607	17.645914
39.578741	1457.713202	17.650931
39.547480	1469.466119	17.655949
39.794101	1470.080419	17.660967
39.492453	1463.152616	17.665984
40.049895	1476.575884	17.671002
39.649360	1466.841703	17.676019
40.052665	1457.776891	17.681037
40.024793	1461.931973	17.686055
39.429030	1439.040070	17.691072
39.856508	1445.045639	17.696090
39.669603	1456.286941	17.701107
39.790305	1460.588222	17.706125
39.894556	1461.504454	17.711143
39.868910	1472.134856	17.716160
40.089661	1460.249483	17.721178
40.066609	1466.949861	17.726195
39.850559	1471.881394	17.731213
40.162433	1457.330813	17.736231
40.015928	1462.751497	17.741248
40.159776	1457.832287	17.746266
40.168664	1465.376259	17.751283
39.858364	1464.169634	17.756301
40.316385	1463.290381	17.761319
39.994820	1465.612447	17.766336
40.273525	1463.158802	17.771354
40.006848	1486.945755	17.776371
40.416697	1490.121781	17.781389
40.415998	1493.727457	17.786407
40.376822	1501.470245	17.791424
40.366170	1488.152473	17.796442
40.375033	1495.733433	17.801459
40.658626	1493.260913	17.806477
40.687318	1490.493187	17.811495
40.616254	1498.545455	17.816512
40.861642	1489.951785	17.821530
40.444584	1499.095909	17.826547
40.427655	1492.825075	17.831565
40.653385	1501.707017	17.836583
40.737310	1514.958074	17.841600
41.296550	1528.127833	17.846618
41.520347	1527.630443	17.851635
41.335229	1505.388709	17.856653
41.202259	1490.297888	17.861671
40.830322	1490.159004	17.866688
41.152412	1487.213133	17.871706
41.368110	1491.602311	17.876723
41.153674	1491.623934	17.881741
41.485284	1476.717811	17.886759
40.901033	1485.609365	17.891776
41.037452	1489.485769	17.896794
41.540007	1498.686162	17.901811
41.454874	1512.051486	17.906829
41.640929	1507.193958	17.911847
41.634282	1516.119262	17.916864
41.027959	1496.905303	17.921882
41.732427	1507.908527	17.926899
41.718585	1514.194518	17.931917
41.520471	1517.796289	17.936935
41.262736	1519.414443	17.941952
41.356070	1511.023558	17.946970
41.755873	1510.965311	17.951987
41.580833	1520.227375	17.957005
41.873767	1513.453272	17.962023
41.543885	1518.524104	17.967040
41.596400	1516.587894	17.972058
41.755358	1510.935548	17.977075
41.565953	1514.882800	17.982093
41.657896	1525.832706	17.987111
41.719384	1538.613071	17.992128
41.904599	1544.876768	17.997146
42.151574	1538.806085	18.002163
42.072702	1540.224246	18.007181
42.381610	1526.481861	18.012199
42.174650	1538.561745	18.017216
42.257677	1531.018039	18.022234
42.293999	1536.384423	18.027251
42.230455	1545.351067	18.032269
42.591018	1534.586987	18.037287
42.153651	1541.257516	18.042304
42.222404	1536.875675	18.047322
42.587016	1542.133072	18.052339
42.506849	1539.358316	18.057357
42.588963	1544.275356	18.062375
42.715075	1562.541097	18.067392
42.694150	1567.249623	18.072410
42.821554	1565.093812	18.077427
42.708634	1570.091519	18.082445
42.957485	1563.642979	18.087463
42.859181	1572.344608	18.092480
42.862131	1566.728920	18.097498
43.157212	1570.246542	18.102515
42.930545	1569.101292	18.107533
43.195639	1568.815191	18.112551
42.918848	1570.989338	18.117568
42.960788	1573.999890	18.122586
43.212031	1557.773288	18.127603
42.738155	1576.673525	18.132621
43.269753	1567.728193	18.137639
43.216856	1569.179182	18.142656
42.902352	1573.101567	18.147674
43.058504	1568.008889	18.152691
43.101582	1576.680107	18.157709
43.193792	1563.839819	18.162727
43.289231	1571.957600	18.167744
43.248713	1562.037730	18.172762
43.422726	1576.660388	18.177779
43.265015	1596.591744	18.182797
43.942709	1589.094749	18.187815
43.776001	1596.806014	18.192832
43.666063	1597.284479	18.197850
43.737897	1593.160907	18.202867
43.831255	1601.969635	18.207885
43.973483	1590.895036	18.212903
43.968419	1594.959996	18.217920
44.042184	1581.755312	18.222938
43.968702	1559.000947	18.227955
43.711164	1566.467905	18.232973
44.226306	1568.921616	18.237991
44.113332	1573.999560	18.243008
43.844117	1584.386516	18.248026
44.189484	1581.881319	18.253043
43.730437	1591.849430	18.258061
44.364777	1583.572008	18.263079
44.383658	1590.747129	18.268096
44.347157	1591.972910	18.273114
44.546122	1587.256451	18.278131
44.197916	1589.306702	18.283149
44.124395	1586.307494	18.288167
44.275643	1583.723137	18.293184
44.161565	1594.167947	18.298202
44.223695	1580.127435	18.303219
44.537014	1590.483629	18.308237
44.388992	1578.498874	18.313255
44.407083	1591.795110	18.318272
44.487698	1606.371341	18.323290
44.795330	1605.649781	18.328307
44.793143	1612.740178	18.333325
44.749991	1619.120557	18.338343
45.010822	1615.451358	18.343360
45.318162	1610.251178	18.348378
45.326378	1618.812357	18.353395
45.008778	1615.108770	18.358413
45.059107	1616.487456	18.363431
45.175317	1621.447851	18.368448
44.940523	1619.070569	18.373466
45.502166	1611.391499	18.378483
45.116049	1616.715951	18.383501
45.331349	1620.486997	18.388519
45.540117	1616.922848	18.393536
45.438265	1608.839903	18.398554
45.504082	1601.523861	18.403571
45.138875	1605.942006	18.408589
45.392669	1608.011876	18.413607
45.440626	1614.216478	18.418624
45.442363	1621.516265	18.423642
45.547844	1614.421206	18.428659
45.249060	1625.291134	18.433677
45.182158	1611.031270	18.438695
45.683761	1609.387604	18.443712
45.441283	1617.419295	18.448730
45.519782	1615.508031	18.453747
45.780064	1617.598105	18.458765
45.748472	1621.233123	18.463783
45.905003	1632.805989	18.468800
45.697562	1644.375560	18.473818
45.837091	1639.855764	18.478835
45.893220	1648.450221	18.483853
45.669072	1649.635142	18.488871
46.190491	1642.589360	18.493888
46.029096	1638.554097	18.498906
45.959792	1643.936579	18.503923
45.734832	1641.427155	18.508941
46.090000	1640.082136	18.513959
46.428486	1660.321433	18.518976
46.211228	1679.378304	18.523994
46.773805	1673.986376	18.529011
46.635599	1677.900336	18.534029
46.404882	1670.571772	18.539047
46.372495	1671.719034	18.544064
46.650956	1664.732439	18.549082
46.728739	1665.137707	18.554099
46.582542	1671.310372	18.559117
46.735982	1674.027079	18.564135
46.544335	1670.282154	18.569152
46.386887	1673.806687	18.574170
46.600255	1668.199090	18.579187
46.659791	1676.554691	18.584205
47.015974	1660.135050	18.589223
47.331590	1658.404629	18.594240
47.067913	1651.775078	18.599258
47.393608	1652.006307	18.604275
47.497252	1647.695951	18.609293
47.518493	1652.527562	18.614311
47.812090	1638.613684	18.619328
47.352174	1643.724173	18.624346
47.899648	1630.448617	18.629363
47.884978	1635.525063	18.634381
47.527417	1617.268629	18.639399
47.650566	1598.178885	18.644416
47.642734	1599.050863	18.649434
47.463181	1594.213073	18.654451
47.339253	1609.728830	18.659469
47.437516	1622.188781	18.664487
47.891178	1616.873236	18.669504
47.440088	1644.310387	18.674522
47.894078	1627.420552	18.679539
47.625522	1640.490397	18.684557
47.765782	1639.789235	18.689575
47.896278	1637.879902	18.694592
48.230290	1635.360776	18.699610
47.790080	1635.232777	18.704627
47.608432	1647.110500	18.709645
47.532192	1633.456182	18.714663
48.028616	1626.130446	18.719680
47.580635	1645.164290	18.724698
48.127268	1641.779860	18.729715
48.404098	1661.889771	18.734733
48.477555	1663.927058	18.739751
48.580235	1649.999570	18.744768
48.032058	1638.655130	18.749786
48.396625	1652.622161	18.754803
48.363833	1665.460934	18.759821
48.322309	1659.525093	18.764839
48.836699	1660.681901	18.769856
48.718509	1658.886162	18.774874
48.746582	1660.750564	18.779891
48.891618	1657.739296	18.784909
48.339739	1660.618824	18.789927
48.434123	1656.799970	18.794944
48.550614	1652.721172	18.799962
48.776149	1653.304237	18.804979
48.877677	1649.739091	18.809997
48.795646	1660.861572	18.815015
49.030219	1646.518198	18.820032
48.633045	1662.426822	18.825050
48.889114	1657.367731	18.830067
48.661156	1672.935542	18.835085
48.739300	1686.336338	18.840103
49.373088	1697.396601	18.845120
49.417769	1693.793317	18.850138
49.637754	1686.783788	18.855155
49.350578	1687.438395	18.860173
49.219134	1689.719162	18.865191
49.743403	1684.530768	18.870208
49.625600	1689.533226	18.875226
49.555103	1688.101921	18.880243
49.428988	1693.388083	18.885261
49.640168	1693.564425	18.890279
49.470532	1690.930544	18.895296
49.478755	1692.096501	18.900314
49.584455	1693.290961	18.905331
49.771070	1686.371703	18.910349
49.812312	1700.289663	18.915367
50.191450	1713.114697	18.920384
49.875640	1720.221341	18.925402
50.403621	1709.413129	18.930419
50.509835	1695.057930	18.935437
49.981244	1703.265866	18.940455
50.136246	1687.618435	18.945472
49.994428	1699.461533	18.950490
50.363062	1704.812737	18.955507
50.287074	1710.469247	18.960525
50.161056	1705.759744	18.965543
50.257386	1706.379934	18.970560
50.085037	1701.699845	18.975578
50.126575	1702.860490	18.980595
50.180873	1710.538928	18.985613
50.040555	1706.568716	18.990631
50.529316	1724.409501	18.995648
50.636168	1736.169710	19.000666
50.635521	1745.852447	19.005683
50.854185	1734.690825	19.010701
50.602784	1746.381538	19.015719
50.879339	1745.988994	19.020736
50.911778	1743.701215	19.025754
51.146786	1737.323239	19.030771
51.221126	1738.024020	19.035789
51.515990	1735.743945	19.040807
51.534193	1739.024176	19.045824
51.120998	1738.570160	19.050842
51.461767	1738.136699	19.055859
51.318455	1737.468959	19.060877
50.806834	1732.269560	19.065895
51.199239	1726.228307	19.070912
51.613974	1726.979415	19.075930
51.488300	1726.669109	19.080947
51.605115	1730.721750	19.085965
51.701835	1727.059818	19.090983
51.924023	1725.334851	19.096000
51.629414	1732.320134	19.101018
51.323820	1732.560801	19.106035
51.560125	1725.447971	19.111053
51.534162	1731.632949	19.116071
51.838391	1726.244449	19.121088
51.579968	1720.255865	19.126106
51.470872	1729.297531	19.131123
51.872013	1744.492152	19.136141
51.871543	1760.060745	19.141159
51.572777	1758.572235	19.146176
52.024009	1766.808789	19.151194
52.131639	1762.619682	19.156211
52.089761	1765.833989	19.161229
51.970647	1765.432967	19.166247
52.283312	1769.422136	19.171264
52.065616	1768.201501	19.176282
52.365989	1784.660516	19.181299
52.790690	1781.395395	19.186317
52.410127	1793.046179	19.191335
52.969670	1791.059750	19.196352
52.880746	1786.769052	19.201370
52.782035	1778.842825	19.206387
52.587223	1766.338376	19.211405
52.482738	1772.084405	19.216423
52.631409	1773.420679	19.221440
52.751760	1785.658581	19.226458
52.844363	1788.234778	19.231475
53.025864	1784.146363	19.236493
53.077028	1792.881706	19.241511
53.281311	1777.665224	19.246528
53.137575	1783.791923	19.251546
53.147991	1795.176635	19.256563
53.376778	1784.688236	19.261581
53.032964	1787.434712	19.266599
53.433320	1793.977261	19.271616
53.380953	1784.770973	19.276634
53.499878	1795.476876	19.281651
53.674748	1775.584218	19.286669
53.079835	1783.316676	19.291687
53.695927	1780.594441	19.296704
53.426384	1782.832747	19.301722
53.316208	1779.966769	19.306739
53.571791	1790.430636	19.311757
53.385621	1790.682147	19.316775
53.575559	1808.280448	19.321792
53.387515	1808.908238	19.326810
53.322203	1815.622596	19.331827
53.400570	1807.762502	19.336845
54.077334	1815.293746	19.341863
54.270500	1824.309291	19.346880
54.541024	1819.523926	19.351898
54.523466	1806.817342	19.356915
54.528519	1784.473274	19.361933
54.495205	1789.484316	19.366951
54.655912	1776.280535	19.371968
54.639144	1779.611186	19.376986
54.432991	1786.747568	19.382003
54.646267	1788.683917	19.387021
54.723339	1793.867707	19.392039
54.809005	1786.029271	19.397056
54.893984	1785.387260	19.402074
54.467102	1782.265026	19.407091
54.932685	1788.470746	19.412109
54.578919	1793.979665	19.417127
54.726237	1786.288711	19.422144
54.920974	1789.231678	19.427162
54.739487	1789.771900	19.432179
54.961980	1788.822433	19.437197
54.737106	1789.854100	19.442215
54.713879	1807.895411	19.447232
54.948953	1816.199502	19.452250
54.769475	1814.926361	19.457267
55.079413	1820.595305	19.462285
54.791364	1823.785172	19.467303
54.948466	1832.046646	19.472320
55.297913	1839.408290	19.477338
55.197756	1849.672510	19.482355
55.094017	1853.054803	19.487373
55.109880	1851.263618	19.492391
55.254172	1844.465875	19.497408
55.397943	1874.158079	19.502426
55.509580	1876.212904	19.507443
56.310720	1875.048447	19.512461
55.941347	1886.964168	19.517479
56.327561	1880.477066	19.522496
56.205446	1883.384847	19.527514
56.143002	1874.672504	19.532531
56.206954	1855.417245	19.537549
56.152669	1851.575642	19.542567
56.090306	1848.895521	19.547584
55.840988	1857.414535	19.552602
55.636248	1867.331263	19.557619
56.172102	1870.480202	19.562637
56.190178	1883.801877	19.567655
56.164879	1879.130528	19.572672
56.450015	1882.988828	19.577690
56.315218	1885.416462	19.582707
56.352831	1886.371666	19.587725
56.314360	1881.959626	19.592743
56.601839	1894.579986	19.597760
56.715794	1906.666415	19.602778
56.670113	1907.023735	19.607795
57.164421	1899.264013	19.612813
56.769486	1901.893597	19.617831
56.970489	1896.578131	19.622848
56.851531	1898.396792	19.627866
56.688785	1898.850652	19.632883
57.161866	1902.325026	19.637901
56.953896	1904.821752	19.642919
57.187468	1903.097309	19.647936
57.315833	1897.043035	19.652954
57.204400	1898.538788	19.657971
57.304175	1889.023431	19.662989
57.417777	1900.413793	19.668007
57.439874	1918.722528	19.673024
57.582430	1913.328280	19.678042
57.604263	1938.192399	19.683059
57.795790	1913.998257	19.688077
57.960433	1930.537290	19.693095
58.108431	1923.053025	19.698112
58.136904	1905.848455	19.703130
57.682243	1895.558640	19.708147
58.019972	1905.910382	19.713165
58.083413	1915.745046	19.718183
58.127977	1919.711726	19.723200
58.448197	1904.889575	19.728218
58.213971	1899.152694	19.733235
58.398958	1886.099897	19.738253
58.227912	1897.895903	19.743271
58.246357	1899.579385	19.748288
58.357708	1913.150501	19.753306
58.407694	1913.826072	19.758323
58.467839	1924.962263	19.763341
58.671574	1909.356377	19.768359
58.779413	1914.707563	19.773376
58.635392	1912.639823	19.778394
58.836349	1917.247791	19.783411
58.674482	1910.210956	19.788429
58.642787	1926.310924	19.793447
58.590349	1912.283644	19.798464
58.875826	1910.709024	19.803482
58.420119	1922.926429	19.808499
58.762769	1919.671218	19.813517
59.178563	1928.702452	19.818535
58.821087	1950.894519	19.823552
59.047308	1950.464376	19.828570
59.122897	1955.436084	19.833587
59.135312	1951.482349	19.838605
59.045116	1950.344406	19.843623
59.060735	1956.309686	19.848640
59.643611	1943.633867	19.853658
59.423569	1944.718261	19.858675
59.176942	1951.614192	19.863693
59.572417	1959.423985	19.868711
59.507008	1961.356821	19.873728
59.992537	1979.223607	19.878746
59.501314	1977.539231	19.883763
60.017030	1987.832757	19.888781
59.712344	1984.206459	19.893799
59.471800	1983.113728	19.898816
59.701217	1982.766452	19.903834
59.866055	1980.548765	19.908851
59.887568	1980.045866	19.913869
59.787241	1999.181254	19.918887
59.776539	2008.094134	19.923904
60.303142	2015.436268	19.928922
60.563234	2011.703377	19.933939
60.474710	2012.954794	19.938957
60.378564	2006.058455	19.943975
60.208054	2015.807002	19.948992
60.558504	1998.278032	19.954010
60.498014	2006.298217	19.959027
60.813177	2016.383054	19.964045
60.711207	2026.926136	19.969063
60.911826	2027.127766	19.974080
61.220503	2032.266053	19.979098
60.863365	2036.703489	19.984115
61.341086	2024.551716	19.989133
61.248649	2034.194222	19.994151
61.147139	2037.884542	19.999168
61.542307	2026.471947	20.004186
61.187428	2027.485820	20.009203
61.227045	2025.406869	20.014221
61.716059	2021.998509	20.019239
61.068836	2020.294170	20.024256
61.694612	2020.191238	20.029274
61.209648	2022.555177	20.034291
61.404556	2027.717111	20.039309
61.554085	2025.305213	20.044327
61.326344	2034.356550	20.049344
61.552524	2026.608058	20.054362
61.492671	2031.200235	20.059379
61.561496	2045.191997	20.064397
61.900353	2056.312945	20.069415
61.560088	2054.880576	20.074432
62.173041	2055.743252	20.079450
62.043542	2055.059134	20.084467
61.876481	2057.117528	20.089485
62.055624	2049.232581	20.094503
61.701523	2066.300488	20.099520
62.317480	2081.080498	20.104538
62.568782	2082.052765	20.109555
62.253442	2090.865612	20.114573
62.789107	2086.955823	20.119591
62.761542	2096.796469	20.124608
62.785229	2083.151751	20.129626
62.818283	2093.479062	20.134643
63.148159	2089.897059	20.139661
63.013745	2088.039353	20.144679
62.811921	2091.060569	20.149696
62.799450	2085.416463	20.154714
63.022829	2076.990356	20.159731
62.892521	2084.917102	20.164749
62.953223	2080.438846	20.169767
62.954426	2091.012717	20.174784
62.828016	2077.027751	20.179802
62.802163	2086.736759	20.184819
63.149876	2096.755106	20.189837
63.613992	2107.691721	20.194855
63.240091	2116.589436	20.199872
63.359963	2108.639183	20.204890
63.182657	2106.519303	20.209907
63.080864	2115.561616	20.214925
63.603417	2108.131580	20.219943
63.670528	2141.957478	20.224960
63.920907	2134.483522	20.229978
64.197163	2149.359465	20.234995
64.171956	2151.932490	20.240013
64.382621	2135.689695	20.245031
64.292401	2151.818909	20.250048
64.436806	2132.552028	20.255066
64.504972	2140.158476	20.260083
64.134314	2134.287514	20.265101
64.559862	2140.878120	20.270119
64.206086	2142.668972	20.275136
64.190067	2133.783887	20.280154
64.305317	2143.918784	20.285171
64.170692	2143.610682	20.290189
64.148392	2130.698486	20.295207
63.998715	2139.654060	20.300224
64.525024	2159.779151	20.305242
64.677653	2168.681814	20.310259
64.437816	2166.505036	20.315277
64.701065	2161.693977	20.320295
64.769859	2184.352512	20.325312
65.329926	2189.038592	20.330330
65.221392	2198.442290	20.335347
65.509984	2189.707601	20.340365
65.872825	2182.973172	20.345383
65.317858	2178.111676	20.350400
65.568181	2154.721879	20.355418
65.731131	2161.530567	20.360435
65.691329	2160.363334	20.365453
65.581251	2161.025899	20.370471
65.587125	2169.446976	20.375488
65.793753	2148.243009	20.380506
65.941875	2151.663865	20.385523
65.790039	2163.888071	20.390541
65.690384	2156.145065	20.395559
65.771758	2178.212430	20.400576
66.032279	2180.000499	20.405594
65.895439	2192.894086	20.410611
66.094121	2196.041021	20.415629
66.396512	2178.713001	20.420647
66.327686	2190.743077	20.425664
66.240854	2184.499611	20.430682
66.346876	2191.382678	20.435699
66.084475	2192.610711	20.440717
66.389204	2180.358183	20.445735
66.263014	2198.045126	20.450752
66.363729	2188.346149	20.455770
66.343695	2194.161466	20.460787
66.471887	2214.237639	20.465805
66.538693	2211.594274	20.470823
66.471732	2210.948157	20.475840
66.612178	2212.457262	20.480858
66.915086	2236.207301	20.485875
67.293077	2237.303322	20.490893
67.401146	2227.542578	20.495911
67.322448	2227.443441	20.500928
67.451782	2222.398076	20.505946
68.087130	2233.694484	20.510963
68.060123	2202.058156	20.515981
68.229214	2187.255102	20.520999
68.305384	2183.966818	20.526016
68.145088	2179.456914	20.531034
68.159757	2185.632458	20.536051
67.687563	2177.231480	20.541069
67.866627	2170.708066	20.546087
67.827698	2186.684408	20.551104
67.795136	2188.089739	20.556122
68.151371	2181.523122	20.561139
68.162529	2177.013408	20.566157
68.197834	2180.239096	20.571175
68.266424	2181.049366	20.576192
68.613010	2182.949566	20.581210
68.655295	2180.524069	20.586227
68.424430	2194.291607	20.591245
68.472741	2176.580135	20.596263
68.411351	2183.496976	20.601280
68.245471	2191.140775	20.606298
68.426120	2182.218004	20.611315
68.122738	2185.205093	20.616333
68.513240	2180.892097	20.621351
68.735610	2203.558422	20.626368
68.641473	2220.693600	20.631386
69.179769	2206.678808	20.636403
68.234711	2209.264812	20.641421
69.074075	2214.322468	20.646439
68.928463	2208.492673	20.651456
68.852686	2219.970908	20.656474
69.242811	2233.470335	20.661491
69.387306	2239.930397	20.666509
69.189129	2239.872338	20.671527
69.413739	2240.677395	20.676544
69.561583	2243.295993	20.681562
69.654026	2235.052714	20.686579
69.290265	2243.334558	20.691597
69.503916	2242.277139	20.696615
69.488071	2238.050165	20.701632
69.389345	2268.294702	20.706650
70.108104	2267.725439	20.711667
69.914483	2274.305509	20.716685
69.778393	2274.977734	20.721703
69.921961	2272.993081	20.726720
69.720477	2275.483329	20.731738
69.990179	2273.221345	20.736755
70.079588	2294.199744	20.741773
69.877293	2292.993125	20.746791
70.486804	2299.129706	20.751808
70.590873	2305.283964	20.756826
70.813762	2295.157190	20.761843
70.931147	2290.984468	20.766861
71.109508	2292.922523	20.771879
70.873152	2291.609639	20.776896
71.106257	2294.322412	20.781914
70.937155	2279.756473	20.786931
71.002860	2282.478635	20.791949
71.416670	2287.187286	20.796967
71.157766	2283.100531	20.801984
71.452430	2284.884743	20.807002
71.716639	2282.333380	20.812019
71.636144	2287.413471	20.817037
71.505718	2294.275299	20.822055
71.248395	2282.869809	20.827072
71.425841	2281.267544	20.832090
71.932477	2295.541337	20.837107
71.663540	2307.887382	20.842125
71.890313	2314.040168	20.847143
71.968768	2324.530309	20.852160
71.951947	2318.089983	20.857178
72.024054	2316.036488	20.862195
71.896962	2319.077296	20.867213
72.037171	2317.260718	20.872231
71.810030	2314.296083	20.877248
71.672642	2309.544146	20.882266
72.258745	2319.148640	20.887283
71.884397	2347.154589	20.892301
72.155222	2348.124549	20.897319
72.270481	2343.481765	20.902336
72.084455	2348.398575	20.907354
72.632234	2358.206643	20.912371
72.307577	2378.637647	20.917389
73.387097	2375.686447	20.922407
73.411381	2368.527672	20.927424
73.245981	2353.272794	20.932442
73.363249	2335.737344	20.937459
73.211844	2343.601520	20.942477
73.261180	2326.802158	20.947495
73.579158	2330.205408	20.952512
73.344043	2327.006062	20.957530
73.206030	2325.660974	20.962547
73.308979	2339.671176	20.967565
73.634563	2346.325800	20.972583
73.625339	2350.535582	20.977600
73.832480	2360.583610	20.982618
74.110781	2348.999833	20.987635
73.819176	2350.127917	20.992653
74.049979	2345.255899	20.997671
74.109759	2345.875653	21.002688
74.021541	2351.575265	21.007706
74.244499	2348.741001	21.012723
73.841161	2356.639067	21.017741
74.162380	2352.671375	21.022759
74.276824	2351.728094	21.027776
74.188065	2347.165826	21.032794
74.452732	2339.004362	21.037811
74.083944	2348.727328	21.042829
74.154069	2354.603059	21.047847
74.630640	2373.815273	21.052864
74.254284	2371.609891	21.057882
74.581388	2373.501425	21.062899
74.641374	2379.966373	21.067917
74.562687	2373.686916	21.072935
74.592351	2390.388013	21.077952
74.870952	2400.513559	21.082970
75.339579	2394.828010	21.087987
75.004742	2401.124668	21.093005
75.287000	2402.018868	21.098023
75.410052	2396.653512	21.103040
75.155932	2405.006848	21.108058
75.141692	2408.198797	21.113075
75.208030	2421.045239	21.118093
75.374244	2426.620139	21.123111
75.746200	2425.815133	21.128128
75.769003	2430.749798	21.133146
75.961773	2421.946086	21.138163
75.925081	2425.910917	21.143181
75.852440	2433.863266	21.148199
76.184652	2436.640496	21.153216
76.233413	2452.726641	21.158234
76.721251	2458.572772	21.163251
76.770505	2449.286143	21.168269
76.447256	2438.019260	21.173287
76.623946	2421.567610	21.178304
76.520742	2427.809250	21.183322
76.891002	2435.734235	21.188339
76.887922	2431.867007	21.193357
76.367656	2422.377813	21.198375
76.718097	2445.555835	21.203392
76.508742	2451.336944	21.208410
76.823470	2449.826040	21.213427
77.269988	2453.023970	21.218445
77.018614	2452.286113	21.223463
77.125068	2452.372191	21.228480
77.259911	2459.925697	21.233498
77.429789	2450.103819	21.238515
77.395033	2457.291854	21.243533
77.404252	2455.720330	21.248551
77.465509	2454.105111	21.253568
77.481566	2465.567320	21.258586
77.730485	2468.961952	21.263603
77.889212	2471.111612	21.268621
77.651251	2472.212272	21.273639
77.714798	2473.282942	21.278656
77.689498	2478.455770	21.283674
77.924332	2467.486877	21.288691
77.957899	2474.581431	21.293709
77.972054	2498.775969	21.298727
78.515659	2500.168898	21.303744
77.983961	2505.528681	21.308762
78.143065	2502.181477	21.313779
78.223457	2507.281611	21.318797
78.393731	2510.404042	21.323815
78.693742	2510.267322	21.328832
78.749019	2533.719096	21.333850
79.138255	2535.065850	21.338867
79.039444	2542.035237	21.343885
78.978159	2542.630256	21.348903
78.848485	2537.259527	21.353920
78.824647	2535.292096	21.358938
79.010945	2525.220555	21.363955
78.913885	2538.155298	21.368973
79.412962	2552.845093	21.373991
79.810503	2557.616997	21.379008
79.542183	2566.541408	21.384026
79.995379	2559.636652	21.389043
80.262389	2552.866995	21.394061
79.953673	2552.812402	21.399079
79.917872	2532.031191	21.404096
79.879824	2538.050103	21.409114
79.960781	2547.220075	21.414131
80.128696	2553.921178	21.419149
80.111216	2562.020549	21.424167
80.643831	2554.221341	21.429184
80.199176	2555.738832	21.434202
79.988405	2553.807501	21.439219
80.647925	2555.658637	21.444237
80.251783	2558.781729	21.449255
80.555488	2550.590324	21.454272
80.298212	2563.711107	21.459290
80.675523	2574.514038	21.464307
81.165222	2572.639337	21.469325
80.831849	2570.540341	21.474343
81.652072	2555.468680	21.479360
81.544270	2573.596006	21.484378
81.772251	2553.317822	21.489395
81.819164	2538.961811	21.494413
81.548503	2540.346149	21.499431
81.763665	2532.103586	21.504448
81.716487	2531.023239	21.509466
81.431786	2529.052570	21.514483
81.871144	2530.810594	21.519501
81.568353	2531.622685	21.524519
82.110109	2524.758099	21.529536
81.701833	2531.482639	21.534554
81.670445	2527.409876	21.539571
81.927890	2524.055638	21.544589
81.957991	2531.478788	21.549607
82.210882	2541.182978	21.554624
82.078040	2545.532880	21.559642
82.349562	2544.246748	21.564659
82.678300	2543.693264	21.569677
82.401215	2548.650620	21.574695
82.471445	2539.598931	21.579712
82.274602	2554.729294	21.584730
82.448127	2546.778115	21.589747
82.813960	2557.741758	21.594765
82.859539	2572.496813	21.599783
83.246591	2571.013695	21.604800
82.963713	2581.054277	21.609818
83.372978	2577.929892	21.614835
83.238378	2586.173811	21.619853
82.925373	2579.063212	21.624871
83.193958	2579.766098	21.629888
83.414219	2585.965663	21.634906
83.306753	2582.649150	21.639923
83.557950	2576.453084	21.644941
83.085637	2601.393200	21.649959
83.321454	2608.648287	21.654976
83.416333	2612.735351	21.659994
83.721831	2609.227121	21.665011
84.112650	2619.279076	21.670029
83.986602	2628.109255	21.675047
84.587366	2626.665994	21.680064
84.732925	2640.159178	21.685082
84.686058	2638.604445	21.690099
84.977140	2626.160216	21.695117
84.791559	2610.676235	21.700135
84.709859	2601.563781	21.705152
84.476658	2610.210450	21.710170
84.959064	2619.407698	21.715187
85.093375	2625.317354	21.720205
84.796428	2632.040705	21.725223
84.902341	2626.799136	21.730240
84.996565	2639.266895	21.735258
84.744556	2624.694166	21.740275
85.013113	2624.213206	21.745293
84.980829	2625.190617	21.750311
85.128171	2638.445958	21.755328
85.243770	2639.461930	21.760346
85.119018	2648.789055	21.765363
85.212436	2657.553576	21.770381
85.107257	2665.545851	21.775399
85.505974	2672.257400	21.780416
85.678333	2677.160434	21.785434
85.951265	2681.137316	21.790451
86.183377	2681.700500	21.795469
85.748588	2684.250044	21.800487
86.074331	2678.396025	21.805504
86.178081	2686.283412	21.810522
85.800411	2693.408253	21.815539
86.300894	2704.775309	21.820557
85.967437	2724.947041	21.825575
86.327429	2715.225249	21.830592
86.472166	2720.116969	21.835610
86.437574	2750.449030	21.840627
86.845382	2740.928837	21.845645
87.149631	2749.175235	21.850663
87.114357	2741.137681	21.855680
87.230501	2757.337702	21.860698
87.211584	2744.217543	21.865715
87.583540	2741.000747	21.870733
87.212639	2740.325198	21.875751
87.370353	2744.025488	21.880768
87.751472	2734.314474	21.885786
87.509892	2748.259655	21.890803
87.638960	2747.340762	21.895821
87.657712	2769.498456	21.900839
87.940292	2767.482918	21.905856
87.793948	2771.349695	21.910874
87.864735	2772.539586	21.915891
88.175966	2777.599858	21.920909
88.463354	2770.763137	21.925927
88.733177	2763.451740	21.930944
88.746947	2754.984728	21.935962
88.476569	2754.688032	21.940979
88.816263	2752.333008	21.945997
88.511441	2758.662789	21.951015
88.921079	2769.776146	21.956032
89.232197	2775.011065	21.961050
89.049807	2778.078091	21.966067
89.253292	2775.232693	21.971085
89.180572	2789.450689	21.976103
89.286829	2777.536097	21.981120
89.365578	2783.903837	21.986138
89.286672	2792.718731	21.991155
89.411270	2789.956706	21.996173
89.262330	2792.828038	22.001191
89.175850	2784.797839	22.006208
89.449323	2784.271253	22.011226
89.602615	2797.137984	22.016243
89.594963	2805.123436	22.021261
89.583973	2815.701348	22.026279
89.772376	2804.924465	22.031296
89.556755	2810.317335	22.036314
89.727910	2839.218941	22.041331
90.247752	2842.210186	22.046349
90.208744	2841.059289	22.051367
90.266527	2844.715757	22.056384
90.584400	2852.035757	22.061402
90.299623	2855.076648	22.066419
90.861772	2853.077875	22.071437
90.847664	2872.074796	22.076455
90.918349	2873.422824	22.081472
90.672507	2864.264012	22.086490
91.028198	2869.697954	22.091507
91.466806	2865.251232	22.096525
91.496478	2869.633525	22.101543
91.563192	2869.611096	22.106560
91.641923	2871.081341	22.111578
91.433739	2875.053974	22.116595
91.686729	2863.701164	22.121613
91.488636	2867.159306	22.126631
91.475946	2872.926525	22.131648
91.673470	2890.200835	22.136666
91.640999	2897.616056	22.141683
92.103346	2897.839684	22.146701
91.935756	2890.791485	22.151719
92.192043	2896.611004	22.156736
92.532103	2896.179205	22.161754
92.252436	2901.323520	22.166771
92.476715	2907.615404	22.171789
92.797772	2919.969355	22.176807
92.540748	2922.823336	22.181824
92.681164	2920.726613	22.186842
92.709824	2920.484489	22.191859
93.037163	2918.396504	22.196877
93.009130	2924.012010	22.201895
92.798632	2911.783609	22.206912
93.218514	2920.941463	22.211930
93.532978	2945.751195	22.216947
94.098463	2932.560489	22.221965
94.197230	2943.083234	22.226983
94.044918	2925.195178	22.232000
93.816496	2910.568057	22.237018
93.760584	2903.011188	22.242035
93.959395	2901.101026	22.247053
93.944742	2914.767897	22.252071
94.161630	2913.790153	22.257088
94.076352	2934.719452	22.262106
93.885665	2944.191006	22.267123
94.356221	2933.221150	22.272141
94.309080	2938.234003	22.277159
94.146175	2929.009220	22.282176
94.354694	2940.712499	22.287194
94.248809	2948.533555	22.292211
94.660819	2958.543035	22.297229
94.502230	2958.785443	22.302247
94.459689	2959.290960	22.307264
94.684576	2979.445590	22.312282
94.741051	2991.243951	22.317299
95.300282	2990.000008	22.322317
94.975115	2987.726581	22.327335
95.204603	2991.059144	22.332352
95.394502	2984.184379	22.337370
95.162677	3004.263984	22.342387
95.662677	3009.029141	22.347405
95.564548	3017.409866	22.352423
95.576542	3021.486663	22.357440
95.671817	3016.367007	22.362458
95.246153	3033.365636	22.367475
96.010097	3035.971091	22.372493
95.962204	3040.890490	22.377511
95.941380	3046.666940	22.382528
96.701721	3037.496247	22.387546
96.864017	3044.123741	22.392563
96.815283	3038.002842	22.397581
96.993838	3037.235727	22.402599
97.046704	3045.884233	22.407616
97.339942	3030.212539	22.412634
96.911063	3032.372600	22.417651
97.578199	3047.442004	22.422669
97.402090	3043.437799	22.427687
97.370593	3039.523811	22.432704
97.793617	3041.481952	22.437722
97.782279	3043.967178	22.442739
97.922888	3040.354559	22.447757
97.728072	3030.214437	22.452775
97.707320	3043.268039	22.457792
98.086861	3047.075416	22.462810
97.958466	3058.210284	22.467827
98.030033	3055.765027	22.472845
98.058455	3046.033746	22.477863
97.984008	3046.855074	22.482880
98.230340	3043.145360	22.487898
97.808601	3049.259490	22.492915
98.152311	3069.181332	22.497933
98.499171	3073.246437	22.502951
98.291756	3077.267773	22.507968
98.872352	3078.156925	22.512986
98.351920	3088.490602	22.518003
98.542759	3097.438085	22.523021
98.690912	3113.182653	22.528039
98.554998	3116.006346	22.533056
99.200634	3123.025641	22.538074
99.254475	3141.282074	22.543091
99.603766	3146.595999	22.548109
99.644907	3149.613297	22.553127
99.625697	3155.404479	22.558144
99.542610	3148.379654	22.563162
99.695288	3156.038446	22.568179
99.945408	3163.835887	22.573197
100.194052	3161.555891	22.578215
100.182136	3171.074601	22.583232
100.394827	3164.158358	22.588250
100.543517	3159.388844	22.593267
100.761733	3151.491571	22.598285
101.073161	3152.604577	22.603303
101.037179	3156.715807	22.608320
101.167920	3155.745492	22.613338
100.984162	3143.620402	22.618355
100.810342	3160.770959	22.623373
101.258108	3148.655294	22.628391
101.056859	3155.642880	22.633408
101.331392	3142.463772	22.638426
101.386079	3158.207559	22.643443
101.523939	3153.840175	22.648461
101.487185	3152.964219	22.653479
101.053077	3160.563187	22.658496
101.566354	3158.790856	22.663514
101.640013	3166.724993	22.668531
101.562161	3180.091466	22.673549
102.067229	3180.908498	22.678567
101.627375	3188.590207	22.683584
101.689660	3182.970729	22.688602
101.749531	3199.480712	22.693619
101.935316	3214.862252	22.698637
101.759636	3211.430610	22.703655
102.047581	3230.887217	22.708672
102.683892	3245.905105	22.713690
102.487884	3247.411332	22.718707
102.662124	3250.729953	22.723725
102.761065	3260.998811	22.728743
102.851734	3273.948320	22.733760
102.878743	3282.370601	22.738778
102.860136	3281.091339	22.743795
103.059153	3297.362129	22.748813
104.021752	3301.994621	22.753831
103.861565	3315.725979	22.758848
104.165195	3311.424153	22.763866
104.076032	3318.526100	22.768883
104.395018	3306.968123	22.773901
104.536632	3306.770128	22.778919
104.517205	3303.037434	22.783936
104.184814	3293.203046	22.788954
104.569531	3295.352981	22.793971
104.710254	3310.051129	22.798989
104.534778	3297.684663	22.804007
104.547747	3302.750201	22.809024
104.435228	3307.062474	22.814042
104.372521	3297.478501	22.819059
104.463572	3309.851366	22.824077
104.844256	3315.649644	22.829095
104.932970	3342.648324	22.834112
105.309950	3325.736573	22.839130
105.368639	3337.883347	22.844147
105.071439	3332.605902	22.849165
105.355928	3343.763254	22.854183
105.329033	3367.356904	22.859200
105.721567	3358.898373	22.864218
105.651595	3365.246816	22.869235
105.629010	3372.457744	22.874253
105.912662	3367.643830	22.879271
106.142421	3374.289037	22.884288
106.103574	3387.665212	22.889306
106.491588	3381.134692	22.894323
106.379210	3382.768408	22.899341
106.696979	3380.450610	22.904359
106.420712	3387.788528	22.909376
106.983275	3375.412871	22.914394
106.701969	3385.458467	22.919411
106.695364	3386.930573	22.924429
106.984219	3397.635731	22.929447
106.821199	3400.875220	22.934464
106.865307	3412.946502	22.939482
106.921523	3421.453098	22.944499
106.901809	3429.238642	22.949517
107.249691	3433.022850	22.954535
107.416613	3452.366105	22.959552
107.577419	3440.336079	22.964570
108.009314	3449.837695	22.969587
107.981259	3469.030344	22.974605
108.416058	3465.513884	22.979623
108.704163	3457.656436	22.984640
108.350917	3473.245344	22.989658
108.455467	3468.865086	22.994675
108.577455	3473.778781	22.999693
108.938496	3468.715710	23.004711
109.111307	3469.287597	23.009728
109.096886	3465.358972	23.014746
109.055827	3471.001151	23.019763
109.008041	3467.132912	23.024781
109.022770	3459.678557	23.029799
109.033460	3480.513092	23.034816
109.071131	3483.866917	23.039834
109.122504	3484.931737	23.044851
109.265867	3494.407017	23.049869
109.491567	3498.590683	23.054887
109.084011	3518.876008	23.059904
109.438049	3515.805078	23.064922
109.790470	3522.576326	23.069939
109.821203	3547.525935	23.074957
110.019829	3545.931959	23.079975
110.128247	3545.546522	23.084992
110.344966	3544.865338	23.090010
111.018622	3560.012902	23.095027
110.879812	3574.595408	23.100045
111.539979	3562.153686	23.105063
110.815300	3557.971704	23.110080
111.252264	3562.273527	23.115098
111.555046	3570.366441	23.120115
111.052246	3578.541400	23.125133
111.427377	3574.309911	23.130151
111.552699	3570.480122	23.135168
111.294957	3574.366443	23.140186
111.751989	3567.969583	23.145203
111.661099	3578.912426	23.150221
111.769267	3571.517848	23.155239
111.672734	3572.536246	23.160256
111.913767	3596.600448	23.165274
112.338952	3596.586153	23.170291
111.569577	3603.467086	23.175309
111.999590	3596.135243	23.180327
111.880134	3610.949126	23.185344
112.222044	3633.654464	23.190362
112.408308	3640.943928	23.195379
112.388503	3637.783117	23.200397
112.645958	3651.746340	23.205415
112.910058	3671.652591	23.210432
112.841596	3669.550522	23.215450
113.322828	3669.600451	23.220467
113.059763	3674.157103	23.225485
113.696078	3675.702149	23.230503
114.023442	3698.284826	23.235520
114.166986	3684.094009	23.240538
114.223596	3688.313344	23.245555
114.432713	3685.613196	23.250573
114.486796	3672.724434	23.255591
114.185467	3650.270609	23.260608
114.251790	3666.868983	23.265626
114.739829	3676.318528	23.270643
114.485183	3666.882919	23.275661
114.634130	3667.906235	23.280679
114.431953	3682.427365	23.285696
114.418523	3670.839508	23.290714
114.772516	3683.868539	23.295731
114.677405	3701.204629	23.300749
114.882280	3692.617710	23.305767
115.135177	3688.861949	23.310784
115.148252	3707.315174	23.315802
115.477927	3711.623136	23.320819
115.259706	3719.661541	23.325837
115.447536	3718.427992	23.330855
116.084799	3722.248736	23.335872
116.162059	3725.971546	23.340890
116.388692	3720.138429	23.345907
116.301960	3753.103642	23.350925
116.681665	3738.269377	23.355943
116.495439	3743.397510	23.360960
116.266538	3757.761707	23.365978
116.886928	3744.046257	23.370995
116.590351	3745.176018	23.376013
116.658609	3750.221881	23.381031
116.818258	3758.436057	23.386048
117.025564	3765.876418	23.391066
117.449367	3777.832390	23.396083
117.297315	3787.835623	23.401101
117.699186	3780.063706	23.406119
117.787079	3771.372673	23.411136
117.975736	3784.902522	23.416154
118.082734	3769.433595	23.421171
117.884986	3784.626727	23.426189
117.927824	3781.387455	23.431207
118.002834	3774.972754	23.436224
117.901940	3781.360920	23.441242
118.284439	3786.932536	23.446259
117.990289	3789.305648	23.451277
118.516994	3801.774666	23.456295
118.802656	3795.189485	23.461312
118.294020	3802.311350	23.466330
118.647879	3816.791939	23.471347
118.743977	3831.387590	23.476365
119.094199	3842.759047	23.481383
118.913711	3841.651871	23.486400
119.103052	3847.989854	23.491418
119.307252	3858.909453	23.496435
119.405278	3853.342234	23.501453
119.792491	3861.631105	23.506471
119.788179	3864.552744	23.511488
119.624704	3882.006149	23.516506
120.020666	3884.430506	23.521523
119.955327	3891.138737	23.526541
120.034324	3891.001067	23.531559
120.002161	3899.171959	23.536576
120.311496	3918.305891	23.541594
120.649905	3926.643488	23.546611
120.445369	3925.020142	23.551629
120.642889	3932.515642	23.556647
120.754574	3943.204609	23.561664
120.877606	3963.796925	23.566682
121.012399	3961.642738	23.571699
121.169762	3963.475019	23.576717
121.328544	3975.472624	23.581735
121.631023	3980.366364	23.586752
121.566542	3980.846306	23.591770
122.431471	3974.782298	23.596787
122.791404	3951.748202	23.601805
123.282677	3939.102597	23.606823
123.592631	3938.834486	23.611840
123.395693	3928.154413	23.616858
123.274851	3914.262775	23.621875
123.548279	3905.288768	23.626893
123.710826	3893.111773	23.631911
123.599980	3896.097605	23.636928
123.497800	3869.940246	23.641946
123.827517	3849.583480	23.646963
123.879558	3854.572177	23.651981
123.400363	3852.778656	23.656999
123.869079	3850.911874	23.662016
123.820065	3858.747158	23.667034
123.805510	3858.714874	23.672051
123.663733	3861.759912	23.677069
123.820670	3877.791041	23.682087
124.093610	3892.960368	23.687104
124.132014	3903.832488	23.692122
124.146652	3886.664771	23.697139
124.275822	3900.425270	23.702157
124.113377	3900.298564	23.707175
124.330924	3889.776634	23.712192
124.138757	3914.975599	23.717210
124.291325	3915.454758	23.722227
124.373208	3931.888894	23.727245
124.543495	3937.547114	23.732263
124.650762	3951.238778	23.737280
124.432133	3963.567958	23.742298
124.932653	3982.494487	23.747315
125.189952	3975.793386	23.752333
125.475625	4007.394677	23.757351
126.110630	4004.855492	23.762368
125.988731	4007.340416	23.767386
126.111179	4018.973321	23.772403
125.919450	4017.638997	23.777421
126.119311	4012.979053	23.782439
126.148069	4026.149930	23.787456
126.170975	4049.418913	23.792474
126.427462	4047.646521	23.797491
126.336526	4066.035752	23.802509
126.591841	4070.965364	23.807527
126.945667	4076.909050	23.812544
127.044686	4080.930570	23.817562
126.989974	4076.459096	23.822579
127.415464	4104.385696	23.827597
127.596331	4105.105011	23.832615
128.015272	4094.918208	23.837632
127.834769	4104.901018	23.842650
127.961999	4106.827018	23.847667
128.121601	4115.131872	23.852685
128.143102	4126.981566	23.857703
128.349503	4123.502945	23.862720
128.277001	4139.826618	23.867738
128.374073	4136.946008	23.872755
128.607153	4141.083054	23.877773
128.728570	4148.122717	23.882791
128.900551	4167.234821	23.887808
129.052623	4169.706769	23.892826
128.942057	4167.335211	23.897843
129.494604	4182.595567	23.902861
129.406380	4191.946951	23.907879
129.591338	4200.020455	23.912896
129.414517	4204.421124	23.917914
129.514011	4191.713475	23.922931
129.749093	4202.674034	23.927949
129.614390	4211.004627	23.932967
130.160115	4213.202982	23.937984
129.908752	4227.077170	23.943002
130.531238	4231.222956	23.948019
130.595212	4239.076614	23.953037
130.350415	4245.464325	23.958055
130.866410	4248.369162	23.963072
131.086764	4244.697121	23.968090
131.230732	4244.669454	23.973107
130.842957	4242.277574	23.978125
131.329769	4263.534498	23.983143
131.367942	4268.600284	23.988160
131.106575	4276.689139	23.993178
131.417104	4268.188099	23.998195
131.973242	4287.877122	24.003213
132.247627	4303.348737	24.008231
132.552546	4302.119287	24.013248
132.472331	4300.562612	24.018266
132.311495	4301.677850	24.023283
132.450544	4300.483500	24.028301
132.418416	4307.365992	24.033319
132.921037	4298.521199	24.038336
132.730269	4326.510293	24.043354
132.798486	4335.327826	24.048371
133.073082	4332.004279	24.053389
133.013068	4330.635550	24.058407
133.505682	4344.345596	24.063424
134.294539	4348.957368	24.068442
134.780632	4325.747593	24.073459
135.012498	4303.409148	24.078477
134.960419	4286.321620	24.083495
134.959333	4283.123070	24.088512
135.004817	4277.114076	24.093530
135.352863	4277.068031	24.098547
135.262586	4252.569608	24.103565
135.286859	4245.439813	24.108583
135.314020	4246.252087	24.113600
135.071446	4244.331102	24.118618
135.081077	4244.605707	24.123635
135.290020	4238.522677	24.128653
135.320849	4249.791972	24.133671
135.466700	4260.467857	24.138688
135.245954	4277.211029	24.143706
135.373829	4269.547055	24.148723
135.773421	4271.468986	24.153741
135.589445	4296.554012	24.158759
135.919740	4304.926949	24.163776
135.869102	4313.986845	24.168794
136.027115	4317.323246	24.173811
136.154964	4331.873424	24.178829
136.039896	4344.934566	24.183847
136.369758	4349.040507	24.188864
136.479593	4373.638262	24.193882
136.316870	4377.605619	24.198899
136.809338	4380.470180	24.203917
136.891639	4397.514468	24.208935
137.201644	4400.913192	24.213952
137.510185	4411.458614	24.218970
137.504828	4422.123324	24.223987
137.990033	4433.535083	24.229005
137.873459	4443.950059	24.234023
137.991063	4433.375235	24.239040
137.871057	4442.830971	24.244058
137.986376	4441.877194	24.249075
138.109212	4456.633626	24.254093
138.427386	4464.904741	24.259111
138.326294	4465.412564	24.264128
138.844954	4474.180389	24.269146
139.052286	4489.027228	24.274163
139.295541	4490.095357	24.279181
139.136656	4498.096401	24.284199
139.174874	4492.010593	24.289216
139.632749	4512.814627	24.294234
139.453349	4521.101384	24.299251
139.787967	4514.317696	24.304269
140.170659	4524.620083	24.309287
140.280427	4518.529937	24.314304
140.418975	4520.571409	24.319322
140.473340	4513.427247	24.324339
140.807697	4511.969660	24.329357
140.948027	4540.877175	24.334375
141.007883	4542.658993	24.339392
140.904823	4536.290447	24.344410
141.158515	4543.723022	24.349427
141.598335	4541.386377	24.354445
141.419718	4542.325095	24.359463
141.591945	4537.685915	24.364480
141.531654	4544.122220	24.369498
141.521578	4557.009466	24.374515
141.935060	4567.479265	24.379533
141.992263	4578.209638	24.384551
142.152329	4569.824462	24.389568
142.195228	4573.895189	24.394586
142.232719	4598.477319	24.399603
142.577972	4600.227801	24.404621
142.717784	4594.198918	24.409639
143.191520	4583.597099	24.414656
143.202223	4588.406972	24.419674
143.158198	4602.224851	24.424691
143.903966	4606.918317	24.429709
143.661000	4614.192526	24.434727
143.895872	4600.872900	24.439744
144.138770	4602.495732	24.444762
143.868509	4615.398552	24.449779
144.070169	4603.126623	24.454797
144.284658	4596.054444	24.459815
144.298776	4612.935201	24.464832
144.399708	4628.862005	24.469850
144.690909	4633.675946	24.474867
144.855604	4631.833157	24.479885
144.875624	4641.004716	24.484903
145.003656	4642.970783	24.489920
145.467281	4652.630194	24.494938
145.078328	4658.117453	24.499955
145.528331	4661.313758	24.504973
145.401057	4658.365756	24.509991
145.601890	4653.508777	24.515008
145.889906	4673.008987	24.520026
145.719005	4690.580180	24.525043
145.914181	4700.455503	24.530061
146.090503	4701.940270	24.535079
146.347831	4698.951394	24.540096
146.421405	4711.981996	24.545114
146.327772	4715.961243	24.550131
146.715961	4720.428538	24.555149
146.615969	4727.882195	24.560167
147.060063	4740.040273	24.565184
147.303654	4752.939956	24.570202
147.034645	4751.617884	24.575219
147.143070	4748.803003	24.580237
147.153215	4775.400663	24.585255
147.376963	4778.945400	24.590272
147.928823	4784.277983	24.595290
147.774895	4799.536762	24.600307
148.278081	4804.705606	24.605325
148.109686	4818.476645	24.610343
148.264608	4812.969228	24.615360
148.320228	4831.030793	24.620378
148.476248	4832.481835	24.625395
148.897941	4844.096005	24.630413
149.128547	4864.356165	24.635431
149.004597	4868.685662	24.640448
149.567043	4869.078263	24.645466
149.123747	4880.505453	24.650483
149.790688	4890.116870	24.655501
149.622916	4901.708631	24.660519
149.650801	4907.588189	24.665536
150.014479	4911.017813	24.670554
150.317377	4930.160386	24.675571
150.727843	4926.763122	24.680589
150.954899	4931.464658	24.685607
151.148938	4919.666511	24.690624
151.555790	4914.357270	24.695642
151.109696	4923.854289	24.700659
151.723421	4927.873440	24.705677
151.823850	4931.020119	24.710695
151.648291	4945.783707	24.715712
151.945354	4945.436606	24.720730
152.123639	4950.118388	24.725747
152.331461	4944.543482	24.730765
152.191410	4946.161324	24.735783
152.237820	4943.685151	24.740800
152.381071	4939.852151	24.745818
152.544661	4974.191590	24.750835
152.878399	4970.022957	24.755853
152.721729	4969.716728	24.760871
152.785644	4966.589487	24.765888
152.968999	4990.694280	24.770906
152.690995	5010.376443	24.775923
153.018351	5008.485646	24.780941
152.812496	5038.350149	24.785959
153.271061	5052.021444	24.790976
153.627463	5050.474538	24.795994
153.785966	5078.974251	24.801011
154.088548	5072.735912	24.806029
154.298622	5069.914206	24.811047
154.132936	5083.264937	24.816064
154.487142	5110.920802	24.821082
154.412639	5101.922085	24.826099
155.000124	5101.371329	24.831117
155.074379	5120.770893	24.836135
154.712854	5129.009139	24.841152
155.369394	5126.087130	24.846170
155.206580	5136.317212	24.851187
155.538193	5158.785022	24.856205
155.569853	5167.571118	24.861223
155.791578	5170.507329	24.866240
156.140256	5178.209886	24.871258
156.144256	5187.017712	24.876275
156.589174	5184.424464	24.881293
156.311528	5193.694963	24.886311
156.439645	5212.799683	24.891328
156.748645	5223.951417	24.896346
156.951084	5225.310128	24.901363
157.424708	5237.131114	24.906381
157.815982	5245.597933	24.911399
157.519667	5252.353047	24.916416
157.652783	5252.795231	24.921434
157.444615	5259.051654	24.926451
157.757147	5272.246062	24.931469
157.988598	5283.859442	24.936487
158.414054	5297.211315	24.941504
158.157603	5291.611956	24.946522
158.074113	5312.243018	24.951539
158.368451	5314.814427	24.956557
158.547202	5327.429131	24.961575
158.702289	5348.793230	24.966592
159.268290	5347.557478	24.971610
159.249941	5374.211896	24.976627
159.681254	5370.071655	24.981645
159.870544	5374.112969	24.986663
159.922659	5385.172818	24.991680
160.270493	5392.939351	24.996698
160.096658	5405.074550	25.001715
160.154033	5418.022601	25.006733
160.802662	5423.430471	25.011751
160.334277	5429.693835	25.016768
160.661381	5439.303150	25.021786
160.417715	5448.822514	25.026803
160.697840	5470.473692	25.031821
161.369696	5462.870285	25.036839
161.384126	5459.571447	25.041856
162.309981	5472.473134	25.046874
162.529920	5483.060203	25.051891
162.771573	5487.853217	25.056909
162.564984	5486.776822	25.061927
162.600562	5477.308723	25.066944
162.981815	5476.340806	25.071962
163.316730	5486.446143	25.076979
163.104372	5467.002046	25.081997
163.228642	5469.768179	25.087015
163.329292	5487.378058	25.092032
163.348035	5487.401042	25.097050
163.447501	5487.090942	25.102067
163.406658	5473.902610	25.107085
163.492227	5483.560690	25.112103
163.548982	5498.681959	25.117120
164.105113	5509.969172	25.122138
163.836327	5513.185068	25.127155
164.227718	5512.878778	25.132173
164.462735	5525.267533	25.137191
164.342501	5538.730230	25.142208
164.413120	5542.703179	25.147226
164.617461	5558.447704	25.152243
164.998241	5560.670211	25.157261
165.001664	5562.960750	25.162279
164.993869	5590.872709	25.167296
165.393466	5591.690980	25.172314
165.361774	5612.687919	25.177331
165.744770	5616.485202	25.182349
166.105309	5628.434682	25.187367
165.499120	5637.704335	25.192384
166.087925	5650.013187	25.197402
166.131173	5657.264303	25.202419
166.580475	5669.024999	25.207437
166.684154	5684.513482	25.212455
167.244585	5701.626241	25.217472
167.811588	5711.248627	25.222490
167.365588	5715.592735	25.227507
167.564576	5723.439035	25.232525
168.112706	5716.071592	25.237543
167.844938	5728.821557	25.242560
168.441854	5738.714565	25.247578
168.482958	5746.750485	25.252595
168.779532	5748.434128	25.257613
168.850833	5736.591959	25.262631
168.577236	5759.403434	25.267648
169.069484	5756.623945	25.272666
169.051853	5776.030364	25.277683
169.212515	5770.486272	25.282701
169.662928	5773.187090	25.287719
169.405353	5809.916621	25.292736
169.869072	5807.243167	25.297754
169.864810	5803.928351	25.302771
170.096731	5811.165984	25.307789
170.552108	5818.671694	25.312807
170.498107	5842.664655	25.317824
170.785067	5834.279779	25.322842
170.855219	5835.269394	25.327859
170.593032	5846.947756	25.332877
171.284879	5852.256844	25.337895
171.253348	5880.401300	25.342912
171.678796	5871.652072	25.347930
171.973159	5865.608263	25.352947
172.016783	5867.362932	25.357965
172.162172	5867.715059	25.362983
172.232500	5877.065046	25.368000
172.312405	5886.688887	25.373018
172.376688	5883.016938	25.378035
172.775437	5898.709588	25.383053
172.951017	5884.122095	25.388071
172.732742	5909.352220	25.393088
173.184739	5913.367536	25.398106
173.344436	5924.078612	25.403123
173.320822	5938.995203	25.408141
173.602175	5940.347696	25.413159
173.546146	5971.108374	25.418176
173.716513	5964.422602	25.423194
173.637086	5973.956243	25.428211
173.830263	5994.316762	25.433229
174.219372	5995.049398	25.438247
174.393341	6011.246932	25.443264
174.697971	6017.996279	25.448282
174.738554	6032.985342	25.453299
174.798966	6046.270994	25.458317
175.253529	6050.106550	25.463335
175.090145	6055.002089	25.468352
175.498227	6075.049932	25.473370
175.769976	6077.405562	25.478387
176.134586	6101.713014	25.483405
176.555381	6087.715667	25.488423
176.748694	6101.716624	25.493440
176.823707	6102.738528	25.498458
177.023280	6110.952376	25.503475
177.049103	6108.876625	25.508493
177.201365	6108.680837	25.513511
177.300179	6127.859075	25.518528
177.625191	6125.915014	25.523546
177.435936	6137.968295	25.528563
177.216626	6153.666122	25.533581
177.764786	6163.564044	25.538599
177.979712	6179.324065	25.543616
178.029530	6198.805257	25.548634
178.382598	6198.715932	25.553651
178.944685	6199.841943	25.558669
179.541441	6207.588893	25.563687
179.861881	6211.349098	25.568704
180.610293	6197.567719	25.573722
180.630239	6169.895034	25.578739
180.340841	6168.555620	25.583757
180.863200	6157.186461	25.588775
180.774155	6161.571351	25.593792
180.847909	6154.646759	25.598810
181.057502	6146.455008	25.603827
181.274945	6155.945372	25.608845
181.445734	6153.561681	25.613863
181.572324	6145.446107	25.618880
181.314569	6145.450229	25.623898
181.418259	6152.315860	25.628915
181.362387	6145.869070	25.633933
181.929928	6138.750104	25.638951
181.364976	6148.275500	25.643968
181.615278	6162.197404	25.648986
182.306690	6170.716834	25.654003
182.053993	6186.467227	25.659021
182.147560	6172.936614	25.664039
182.117997	6198.097016	25.669056
182.339300	6210.366579	25.674074
182.622651	6214.881736	25.679092
182.327391	6238.436996	25.684109
182.775934	6251.432780	25.689127
182.781895	6268.362360	25.694144
182.909007	6296.424877	25.699162
183.547547	6291.411824	25.704180
183.775845	6311.571266	25.709197
184.410939	6319.179980	25.714215
184.496595	6336.120537	25.719232
184.523193	6325.479405	25.724250
185.190988	6329.141777	25.729268
184.630160	6338.558843	25.734285
184.832553	6351.143114	25.739303
185.279014	6354.983978	25.744320
185.411748	6369.603839	25.749338
185.658146	6380.827015	25.754356
185.768291	6389.007280	25.759373
185.920843	6399.478287	25.764391
186.059857	6411.977510	25.769408
186.160212	6425.133603	25.774426
186.714172	6420.139500	25.779444
186.395159	6450.096482	25.784461
186.576846	6446.000467	25.789479
186.970818	6464.067522	25.794496
187.039443	6477.240522	25.799514
187.553115	6484.003180	25.804532
187.318550	6493.215686	25.809549
187.642900	6504.634249	25.814567
187.826627	6518.397934	25.819584
188.335922	6539.191128	25.824602
188.465374	6551.394574	25.829620
188.265288	6555.189855	25.834637
188.910635	6567.014437	25.839655
189.121743	6577.495905	25.844672
189.131232	6574.293601	25.849690
189.357267	6592.966689	25.854708
189.434824	6604.932962	25.859725
189.773749	6617.691614	25.864743
189.522961	6620.669613	25.869760
189.554635	6639.308438	25.874778
190.034273	6644.661879	25.879796
189.874352	6673.860624	25.884813
190.274431	6677.760898	25.889831
190.880989	6684.291676	25.894848
191.276770	6704.567368	25.899866
191.531874	6702.616282	25.904884
191.536822	6703.829582	25.909901
191.811079	6713.526839	25.914919
191.759532	6712.844227	25.919936
191.834471	6733.708513	25.924954
192.352068	6723.460135	25.929972
192.463489	6739.576378	25.934989
192.349971	6730.504208	25.940007
192.971537	6735.258309	25.945024
193.180426	6749.112618	25.950042
193.251300	6758.884816	25.955060
193.147078	6759.139851	25.960077
193.648272	6774.985484	25.965095
193.949990	6787.447283	25.970112
193.662958	6786.176675	25.975130
194.246943	6789.960323	25.980148
194.571758	6794.541438	25.985165
194.573414	6805.671764	25.990183
195.045713	6808.617932	25.995200
194.784867	6813.264879	26.000218
195.066004	6818.709829	26.005236
194.695837	6842.343290	26.010253
195.074496	6841.749458	26.015271
195.411145	6864.141948	26.020288
195.672617	6874.736771	26.025306
195.970895	6875.165267	26.030324
195.974585	6900.467908	26.035341
196.294529	6905.039605	26.040359
196.549947	6916.184245	26.045376
196.706491	6930.486126	26.050394
196.796799	6932.998291	26.055412
196.794401	6947.807074	26.060429
197.201298	6954.965444	26.065447
197.250783	6966.339269	26.070464
197.136354	6988.217657	26.075482
197.702620	6985.598470	26.080500
198.036636	7018.151368	26.085517
198.370115	7012.083554	26.090535
198.700097	7021.173338	26.095552
198.835853	7034.933348	26.100570
199.163763	7045.933158	26.105588
198.988704	7057.383765	26.110605
199.457294	7047.487620	26.115623
199.659572	7061.514808	26.120640
199.676590	7075.251294	26.125658
200.307200	7074.982387	26.130676
200.260876	7075.007878	26.135693
200.340074	7099.286930	26.140711
200.691436	7103.104597	26.145728
200.676163	7105.377896	26.150746
201.019079	7105.973178	26.155764
201.092988	7124.709742	26.160781
201.254906	7133.342473	26.165799
201.445207	7142.106023	26.170816
201.585184	7158.100926	26.175834
201.828436	7167.976531	26.180852
202.134574	7160.212622	26.185869
202.126496	7172.537646	26.190887
202.646041	7193.906105	26.195904
202.639712	7206.044393	26.200922
202.833316	7209.806979	26.205940
202.867465	7212.376929	26.210957
202.811336	7235.883837	26.215975
203.313206	7235.973014	26.220992
203.450344	7258.737828	26.226010
203.593242	7261.685454	26.231028
203.864332	7271.290732	26.236045
204.148489	7294.374447	26.241063
204.359960	7303.111898	26.246080
204.371601	7308.974539	26.251098
204.470117	7323.707020	26.256116
204.773668	7323.571296	26.261133
204.931057	7347.699800	26.266151
205.941144	7349.295855	26.271168
205.520170	7362.361988	26.276186
205.838550	7371.804780	26.281204
206.200917	7379.921777	26.286221
206.407067	7396.727090	26.291239
206.615189	7387.127190	26.296256
206.767125	7405.964977	26.301274
206.986290	7414.143378	26.306292
207.118630	7419.535945	26.311309
207.423479	7434.695962	26.316327
207.984135	7448.037676	26.321344
207.731197	7449.292147	26.326362
207.859883	7452.827509	26.331380
208.102773	7462.035315	26.336397
208.122516	7486.436210	26.341415
208.579506	7488.001637	26.346432
208.724439	7510.058193	26.351450
209.273639	7502.559094	26.356468
209.319662	7513.023476	26.361485
209.123522	7532.978405	26.366503
209.603555	7530.447628	26.371520
209.376774	7556.154805	26.376538
210.065676	7561.306047	26.381556
210.192624	7572.408317	26.386573
210.161068	7582.095877	26.391591
210.601424	7590.387834	26.396608
210.752581	7610.412616	26.401626
211.229849	7612.081053	26.406644
211.012726	7628.081453	26.411661
211.146628	7639.740562	26.416679
211.600935	7649.085535	26.421696
211.581011	7675.659346	26.426714
212.093219	7666.298005	26.431732
212.669900	7673.878969	26.436749
212.903407	7678.829800	26.441767
212.957695	7680.472034	26.446784
213.319661	7692.924203	26.451802
213.828120	7694.184007	26.456820
214.154504	7707.553072	26.461837
213.685604	7711.847100	26.466855
214.289064	7701.049291	26.471872
214.244300	7712.260874	26.476890
214.370214	7700.285686	26.481908
214.446320	7705.847059	26.486925
214.338555	7717.607705	26.491943
214.929617	7726.831780	26.496960
214.873795	7748.635053	26.501978
214.820064	7757.409540	26.506996
215.446914	7771.575880	26.512013
215.208859	7773.677056	26.517031
215.599776	7794.041177	26.522048
215.796165	7807.170200	26.527066
215.651083	7824.936515	26.532084
216.280315	7835.499369	26.537101
216.330200	7851.209573	26.542119
216.281476	7870.886105	26.547136
216.498333	7888.749031	26.552154
217.033101	7899.468236	26.557172
217.637140	7928.490206	26.562189
217.371760	7928.846884	26.567207
217.909016	7948.127939	26.572224
218.325418	7957.007405	26.577242
218.349129	7963.074152	26.582260
219.068225	7976.781388	26.587277
218.996906	7982.620533	26.592295
219.411836	7988.806307	26.597312
219.048384	7989.840008	26.602330
219.624782	8007.756321	26.607348
219.727736	8013.319824	26.612365
219.757912	8035.475715	26.617383
220.277832	8050.222002	26.622400
220.222516	8055.231591	26.627418
220.564217	8071.303911	26.632436
220.974696	8073.147119	26.637453
221.131513	8093.244829	26.642471
221.404900	8103.123335	26.647488
221.493101	8119.947085	26.652506
221.752766	8114.873442	26.657524
222.334922	8135.177249	26.662541
222.094945	8143.869517	26.667559
222.154663	8147.150064	26.672576
222.364864	8165.252027	26.677594
222.322453	8175.361123	26.682612
222.846227	8204.006119	26.687629
223.147408	8203.826310	26.692647
224.092934	8201.762618	26.697664
224.389863	8214.809086	26.702682
224.630290	8212.389579	26.707700
225.176019	8202.851804	26.712717
225.410621	8201.248072	26.717735
225.538101	8199.240812	26.722752
225.400084	8200.125669	26.727770
225.552161	8205.224612	26.732788
226.309305	8197.706976	26.737805
226.026087	8200.411492	26.742823
226.009463	8194.250682	26.747840
225.834787	8196.441356	26.752858
226.218580	8198.065746	26.757876
226.151406	8215.491571	26.762893
226.320321	8233.909061	26.767911
226.243304	8236.049156	26.772928
226.626715	8264.139838	26.777946
226.799019	8276.191895	26.782964
226.989634	8300.560980	26.787981
227.180431	8309.862603	26.792999
227.198673	8334.078622	26.798016
227.482782	8349.920414	26.803034
227.776202	8371.993527	26.808052
227.760149	8375.444373	26.813069
227.924757	8409.020406	26.818087
228.268186	8432.981723	26.823104
228.533038	8455.816533	26.828122
228.710147	8480.313971	26.833140
229.893227	8489.419759	26.838157
230.029954	8501.759388	26.843175
230.334925	8512.503472	26.848192
230.405378	8522.331585	26.853210
230.704649	8533.699838	26.858228
230.812023	8546.139007	26.863245
231.144420	8561.558222	26.868263
231.528575	8563.273487	26.873280
231.662164	8573.592450	26.878298
231.922913	8579.231345	26.883316
232.535938	8589.815029	26.888333
232.072837	8622.205755	26.893351
232.545026	8611.962158	26.898368
232.659064	8637.112830	26.903386
233.188887	8648.028526	26.908404
233.486510	8647.112318	26.913421
233.360530	8672.889935	26.918439
233.665260	8682.161825	26.923456
234.038251	8678.614682	26.928474
234.086370	8706.259544	26.933492
234.418455	8708.603626	26.938509
234.628936	8723.230323	26.943527
234.923405	8732.645529	26.948544
235.194036	8744.894764	26.953562
235.161159	8748.564786	26.958580
235.550482	8764.041632	26.963597
235.358103	8779.475078	26.968615
235.968953	8787.831030	26.973632
236.321754	8805.639544	26.978650
236.627997	8816.943947	26.983668
236.920307	8828.404820	26.988685
237.173973	8837.394565	26.993703
237.499182	8840.306757	26.998720
237.717824	8845.660116	27.003738
237.574127	8847.116842	27.008756
238.903855	8828.927566	27.013773
239.027593	8833.225020	27.018791
239.211882	8825.293961	27.023808
239.914925	8835.145388	27.028826
239.568934	8815.185056	27.033844
239.675406	8801.881764	27.038861
239.997208	8822.293721	27.043879
239.687944	8818.804146	27.048896
240.047175	8841.061444	27.053914
239.968731	8829.326077	27.058932
240.414550	8829.491892	27.063949
240.406756	8849.398482	27.068967
240.684844	8859.613554	27.073984
240.650315	8868.250668	27.079002
240.481626	8888.460747	27.084020
241.181706	8896.647117	27.089037
241.098861	8919.931925	27.094055
241.345534	8934.599491	27.099072
241.452143	8950.677969	27.104090
241.866283	8974.810669	27.109108
242.561193	8978.514653	27.114125
242.453061	9009.291467	27.119143
242.336770	9025.309547	27.124160
243.076067	9033.882037	27.129178
242.976467	9064.060700	27.134196
243.820785	9075.632087	27.139213
243.928113	9082.610632	27.144231
244.003300	9105.001344	27.149248
244.370453	9121.439036	27.154266
244.512028	9127.692076	27.159284
245.193618	9138.653196	27.164301
245.551210	9156.020274	27.169319
245.924289	9170.883943	27.174336
246.495864	9167.316446	27.179354
246.394544	9174.824864	27.184372
246.764988	9156.081812	27.189389
246.772173	9174.251591	27.194407
247.250258	9179.810428	27.199424
247.332703	9193.057203	27.204442
247.123780	9198.396212	27.209460
247.570021	9218.918723	27.214477
247.694436	9227.135653	27.219495
247.820328	9228.183112	27.224512
248.102521	9250.695290	27.229530
248.207399	9261.391932	27.234548
248.661337	9279.505186	27.239565
248.851833	9302.873326	27.244583
249.018177	9319.068985	27.249600
249.231944	9313.345140	27.254618
249.019747	9350.147348	27.259636
249.562997	9353.763853	27.264653
249.777933	9385.104958	27.269671
250.068529	9388.110524	27.274688
250.306353	9408.199055	27.279706
250.317899	9418.527822	27.284724
250.717513	9440.056739	27.289741
250.542953	9461.748822	27.294759
251.075957	9467.954959	27.299776
251.757061	9477.855169	27.304794
251.861373	9519.618810	27.309812
252.158120	9521.326876	27.314829
251.938977	9540.907238	27.319847
252.634638	9550.332989	27.324864
253.512833	9554.439959	27.329882
253.975796	9573.084523	27.334900
253.873863	9567.950378	27.339917
254.194354	9578.074583	27.344935
254.727123	9580.343141	27.349952
255.134301	9594.130320	27.354970
255.144684	9598.826569	27.359988
255.540770	9592.434134	27.365005
255.760952	9598.581192	27.370023
255.648062	9591.552156	27.375040
256.259304	9604.390771	27.380058
256.371402	9609.705512	27.385076
256.816285	9620.005484	27.390093
256.666490	9621.423118	27.395111
256.965217	9620.146636	27.400128
257.471154	9631.030663	27.405146
257.560755	9634.062022	27.410164
257.751066	9635.539953	27.415181
258.130277	9639.315284	27.420199
258.281562	9656.770524	27.425216
258.272908	9656.403996	27.430234
258.281332	9678.247444	27.435252
258.779921	9693.490631	27.440269
259.204030	9701.371621	27.445287
259.363989	9717.400313	27.450304
259.553241	9734.047649	27.455322
259.392103	9743.401145	27.460340
259.888440	9758.980409	27.465357
260.127389	9760.746903	27.470375
260.175601	9796.901138	27.475392
260.504155	9808.393583	27.480410
260.404943	9823.171059	27.485428
260.730257	9843.272985	27.490445
261.118053	9861.180276	27.495463
261.296016	9879.524370	27.500480
261.603045	9905.758040	27.505498
261.640640	9936.421049	27.510516
262.077338	9944.354857	27.515533
262.594371	9970.513457	27.520551
262.669532	9994.812798	27.525568
262.958758	10008.569185	27.530586
263.343085	10028.044154	27.535604
263.508627	10049.800136	27.540621
263.767632	10050.164564	27.545639
264.363961	10080.723857	27.550656
264.916743	10090.955407	27.555674
264.979971	10103.129812	27.560692
265.053034	10120.746016	27.565709
265.376109	10134.393631	27.570727
265.083224	10142.371428	27.575744
265.717230	10155.927005	27.580762
265.590251	10183.795309	27.585780
266.287456	10192.842671	27.590797
266.273328	10211.249070	27.595815
266.667850	10227.623408	27.600832
267.496195	10242.666242	27.605850
267.336740	10258.086507	27.610868
267.756834	10273.327055	27.615885
268.150140	10296.480645	27.620903
268.137216	10306.282289	27.625920
268.610722	10315.198533	27.630938
268.651065	10324.441179	27.635956
268.929971	10349.538531	27.640973
269.354213	10359.734481	27.645991
269.379815	10383.298611	27.651008
269.748555	10394.975166	27.656026
269.670156	10412.118845	27.661044
269.691505	10429.178173	27.666061
270.412694	10447.543411	27.671079
270.308834	10474.902902	27.676096
270.831096	10498.123214	27.681114
270.734045	10523.795890	27.686132
271.275321	10547.803821	27.691149
271.472102	10574.651225	27.696167
271.768356	10604.917444	27.701184
272.225060	10624.515052	27.706202
272.309182	10641.412322	27.711220
273.067005	10667.182343	27.716237
273.352095	10677.992148	27.721255
274.184168	10688.685266	27.726272
274.501152	10693.101204	27.731290
274.817549	10694.092038	27.736308
275.265067	10702.960711	27.741325
275.588450	10713.715249	27.746343
275.675605	10715.539501	27.751360
275.662393	10718.378506	27.756378
275.793693	10721.137812	27.761396
276.056100	10747.212420	27.766413
276.563633	10741.611218	27.771431
276.811370	10774.500460	27.776448
277.116804	10773.613585	27.781466
277.479115	10787.050122	27.786484
277.475585	10808.513425	27.791501
277.881107	10811.354969	27.796519
277.837858	10830.108144	27.801536
278.523683	10833.067934	27.806554
278.791587	10840.957109	27.811572
278.670093	10851.249821	27.816589
278.866422	10868.934219	27.821607
278.693455	10881.994550	27.826624
279.193554	10893.836301	27.831642
279.261383	10918.781713	27.836660
279.518817	10933.904826	27.841677
279.449214	10954.976291	27.846695
279.593181	10980.477134	27.851712
279.942306	11018.836129	27.856730
280.228063	11024.959154	27.861748
280.331987	11064.888173	27.866765
281.154442	11085.289917	27.871783
281.249363	11113.581454	27.876800
281.490085	11141.699476	27.881818
281.595644	11168.672269	27.886836
281.995494	11193.076053	27.891853
282.399938	11209.286955	27.896871
282.557847	11255.597676	27.901888
283.141745	11257.031537	27.906906
283.850703	11281.093800	27.911924
283.560900	11307.770557	27.916941
284.070164	11324.252944	27.921959
284.409764	11345.616473	27.926976
284.553593	11370.102668	27.931994
285.062727	11393.571825	27.937012
285.325839	11402.575968	27.942029
285.860923	11420.644438	27.947047
285.702540	11443.657891	27.952064
285.819119	11460.721306	27.957082
286.484692	11494.429802	27.962100
286.517011	11514.606235	27.967117
287.091981	11525.277572	27.972135
287.421186	11546.988375	27.977152
287.609373	11564.082012	27.982170
288.024154	11587.473041	27.987188
288.082754	11610.377194	27.992205
288.917687	11623.046905	27.997223
288.953527	11653.922842	28.002240
289.372943	11661.665514	28.007258
290.191359	11674.090952	28.012276
290.134430	11684.586254	28.017293
290.110273	11708.939794	28.022311
290.008512	11720.766747	28.027328
290.718251	11742.469917	28.032346
290.984747	11756.230342	28.037364
291.126991	11773.880340	28.042381
291.439731	11800.205728	28.047399
291.542158	11825.770103	28.052416
291.836269	11835.307546	28.057434
292.166664	11868.183432	28.062452
292.379037	11881.325277	28.067469
292.700611	11905.369205	28.072487
292.805293	11932.453494	28.077504
293.578621	11942.929600	28.082522
293.654816	11969.395698	28.087540
293.854631	11984.917876	28.092557
294.861450	11996.203537	28.097575
294.790758	12018.299102	28.102592
295.048741	12035.722375	28.107610
295.826807	12048.289348	28.112628
295.574503	12062.511336	28.117645
295.949606	12072.061798	28.122663
296.267550	12078.802728	28.127680
296.830412	12094.319895	28.132698
296.845618	12105.897488	28.137716
297.204365	12112.485133	28.142733
297.599500	12120.057959	28.147751
297.845351	12132.439057	28.152768
298.210183	12155.095495	28.157786
299.023459	12160.593571	28.162804
299.777522	12137.413865	28.167821
300.961975	12129.378945	28.172839
300.952153	12122.145167	28.177856
301.221576	12116.702240	28.182874
301.705260	12106.680768	28.187892
301.780510	12089.568557	28.192909
301.954597	12063.924264	28.197927
301.885966	12074.258178	28.202944
301.668478	12070.245324	28.207962
302.086602	12066.440899	28.212980
302.035254	12082.040398	28.217997
302.282014	12100.455527	28.223015
302.585529	12109.965278	28.228032
302.671917	12112.978561	28.233050
302.939739	12134.636038	28.238068
303.234377	12158.831067	28.243085
303.329637	12165.053004	28.248103
303.485895	12196.642675	28.253120
303.513027	12209.269446	28.258138
303.691214	12229.834262	28.263156
304.062446	12265.635147	28.268173
304.349278	12272.061945	28.273191
304.680113	12310.486751	28.278208
305.207896	12330.489670	28.283226
305.358387	12346.151727	28.288244
305.809019	12383.764793	28.293261
306.148411	12389.498267	28.298279
306.631187	12404.929930	28.303296
306.771586	12437.736776	28.308314
307.473762	12449.454274	28.313332
307.577436	12468.217934	28.318349
308.141915	12498.008727	28.323367
308.019775	12503.074910	28.328384
308.688269	12518.963737	28.333402
309.416395	12535.165803	28.338420
309.072477	12550.013269	28.343437
309.759987	12564.235107	28.348455
309.675475	12578.275178	28.353472
310.562718	12577.885247	28.358490
312.226639	12571.268270	28.363508
312.602498	12563.709715	28.368525
312.831909	12548.620747	28.373543
313.020320	12536.445614	28.378560
313.216411	12540.388621	28.383578
313.432280	12526.699196	28.388596
313.345788	12522.150951	28.393613
313.600348	12529.398869	28.398631
313.998068	12522.026943	28.403648
313.705515	12531.807684	28.408666
313.807434	12532.886158	28.413684
314.133228	12518.549120	28.418701
314.350473	12551.499819	28.423719
314.410204	12569.011583	28.428736
314.689099	12572.078700	28.433754
314.895971	12594.226504	28.438772
314.992365	12615.397004	28.443789
315.063817	12639.820234	28.448807
315.270393	12665.501863	28.453824
315.441850	12695.673491	28.458842
315.810313	12724.004625	28.463860
316.065077	12750.687150	28.468877
316.304439	12782.819930	28.473895
316.691503	12818.127726	28.478912
316.551453	12850.933912	28.483930
317.393520	12860.470083	28.488948
317.502692	12901.754735	28.493965
318.027158	12931.179054	28.498983
318.607925	12964.732546	28.504000
318.644332	13000.318429	28.509018
319.315510	13018.392609	28.514036
319.815686	13051.941917	28.519053
320.135400	13065.959145	28.524071
320.605384	13092.833615	28.529088
320.682739	13116.337456	28.534106
321.115131	13131.710687	28.539124
321.359743	13162.689248	28.544141
321.416284	13186.891289	28.549159
321.785284	13202.718461	28.554176
322.341974	13234.537329	28.559194
323.308252	13239.115726	28.564212
323.892581	13260.525115	28.569229
324.282043	13271.264551	28.574247
324.718171	13282.846902	28.579264
324.646928	13290.954943	28.584282
325.126059	13313.247752	28.589300
325.151893	13319.215259	28.594317
325.304495	13344.052547	28.599335
325.567409	13342.995886	28.604352
326.069379	13375.099971	28.609370
326.532789	13383.596345	28.614388
326.762776	13412.077663	28.619405
327.091712	13417.082791	28.624423
326.887988	13445.196107	28.629440
327.062014	13464.714629	28.634458
327.653027	13484.039789	28.639476
327.881385	13519.929073	28.644493
327.980213	13528.174562	28.649511
328.287721	13550.847434	28.654528
328.241030	13589.601996	28.659546
328.926492	13595.977739	28.664564
329.439624	13636.477752	28.669581
329.592132	13647.279028	28.674599
329.724876	13676.306510	28.679616
330.117967	13695.145408	28.684634
330.423455	13730.137988	28.689652
330.793298	13761.997870	28.694669
330.763944	13785.585083	28.699687
331.637430	13805.638274	28.704704
331.623771	13836.287703	28.709722
332.177702	13860.633734	28.714740
332.243491	13894.270553	28.719757
332.555274	13911.098450	28.724775
333.260090	13946.783312	28.729792
333.471074	13983.105480	28.734810
333.955701	13996.506188	28.739828
334.164051	14024.483555	28.744845
334.601195	14052.465842	28.749863
335.003826	14077.228756	28.754880
335.220388	14100.169337	28.759898
335.627520	14134.768682	28.764916
336.009801	14158.293232	28.769933
336.225853	14187.559922	28.774951
336.815564	14213.858534	28.779968
337.209426	14236.495143	28.784986
338.135847	14236.243998	28.790004
338.352643	14251.436527	28.795021
338.754640	14279.026888	28.800039
339.390962	14277.282850	28.805056
339.989666	14305.397595	28.810074
339.379277	14309.343134	28.815092
340.058275	14322.517923	28.820109
340.396756	14348.271990	28.825127
340.832728	14346.603268	28.830144
340.510667	14382.498055	28.835162
340.831215	14394.095343	28.840180
341.205258	14419.638298	28.845197
341.485571	14451.486724	28.850215
342.142002	14470.495495	28.855232
342.241275	14496.589738	28.860250
342.449830	14516.260562	28.865268
342.877405	14541.511685	28.870285
342.696870	14571.469737	28.875303
343.555345	14594.031656	28.880320
343.861203	14620.495075	28.885338
344.043731	14654.312655	28.890356
344.089916	14687.438298	28.895373
344.384891	14723.609001	28.900391
345.265973	14745.864156	28.905408
345.250551	14776.100763	28.910426
345.949982	14797.226796	28.915444
346.310432	14832.900900	28.920461
346.704038	14841.166249	28.925479
347.063276	14861.408471	28.930496
348.016626	14865.494157	28.935514
348.619492	14883.047192	28.940532
348.840595	14893.591809	28.945549
348.954192	14903.545114	28.950567
349.568988	14897.475610	28.955584
349.854313	14932.247813	28.960602
350.039530	14927.457852	28.965620
350.381576	14938.598569	28.970637
350.557393	14954.221084	28.975655
350.633100	14963.595925	28.980672
350.665958	14997.177723	28.985690
351.014734	15014.781437	28.990708
351.253420	15037.555948	28.995725
351.400198	15068.801748	29.000743
352.079614	15093.159269	29.005760
351.997885	15118.985136	29.010778
353.231760	15139.804765	29.015796
353.402672	15157.929030	29.020813
353.974835	15180.089288	29.025831
354.353921	15191.264438	29.030848
354.360707	15222.401187	29.035866
354.499730	15249.361885	29.040884
355.116048	15264.468135	29.045901
355.093956	15301.727765	29.050919
355.756912	15322.675524	29.055936
355.633144	15358.521204	29.060954
356.160687	15382.906832	29.065972
356.611868	15413.796408	29.070989
356.597887	15445.552572	29.076007
357.291891	15474.995124	29.081024
357.340901	15516.806465	29.086042
357.859045	15542.488737	29.091060
358.098895	15574.008092	29.096077
358.284460	15612.511581	29.101095
358.705442	15641.048087	29.106112
359.114207	15673.908261	29.111130
359.632419	15703.816017	29.116148
359.901056	15737.995730	29.121165
360.082393	15781.675632	29.126183
360.559125	15816.444525	29.131200
360.706589	15854.688974	29.136218
360.925757	15886.090229	29.141236
362.442885	15892.469743	29.146253
364.554271	15876.437939	29.151271
365.976850	15855.847582	29.156288
366.208446	15852.390827	29.161306
366.519236	15834.447043	29.166324
366.897887	15827.209448	29.171341
366.836580	15809.743438	29.176359
367.148542	15792.493327	29.181376
367.445860	15804.220667	29.186394
367.330654	15797.464880	29.191412
367.891366	15801.281155	29.196429
367.506229	15788.894094	29.201447
367.735432	15782.897111	29.206464
367.842358	15793.729307	29.211482
368.056523	15800.645894	29.216500
368.352855	15797.209541	29.221517
368.414089	15826.063922	29.226535
368.675323	15832.618146	29.231552
368.614382	15852.849802	29.236570
368.520054	15874.924183	29.241588
369.134010	15893.710913	29.246605
369.006089	15940.768498	29.251623
369.324722	15962.161917	29.256640
369.455725	16006.237834	29.261658
369.670091	16040.618383	29.266676
370.359860	16077.200964	29.271693
370.607599	16122.102811	29.276711
371.464228	16154.529497	29.281728
371.891752	16192.963404	29.286746
372.620396	16224.343611	29.291764
373.074752	16239.406365	29.296781
373.126476	16269.715508	29.301799
373.531684	16298.162450	29.306816
374.329172	16324.588454	29.311834
374.904229	16336.332765	29.316852
375.623128	16363.376225	29.321869
375.459929	16381.197720	29.326887
376.456262	16408.087809	29.331904
377.543852	16409.022691	29.336922
377.798171	16422.382216	29.341940
378.522542	16423.880641	29.346957
378.241179	16428.833730	29.351975
378.607267	16430.810273	29.356992
379.276325	16451.949733	29.362010
379.547417	16463.964606	29.367028
379.667013	16463.020438	29.372045
379.652944	16489.973648	29.377063
380.276957	16486.815220	29.382080
380.374092	16518.670050	29.387098
380.542612	16528.752061	29.392116
380.952350	16560.243805	29.397133
381.402642	16582.742415	29.402151
381.675755	16606.510538	29.407168
382.214052	16614.764523	29.412186
382.552311	16642.261618	29.417204
382.814765	16645.160545	29.422221
382.817360	16684.506437	29.427239
383.779643	16711.856982	29.432256
383.815307	16730.719365	29.437274
383.844132	16761.176614	29.442292
384.812600	16789.040059	29.447309
384.667386	16817.855174	29.452327
384.976545	16839.470008	29.457344
385.215091	16887.239157	29.462362
385.447449	16906.743604	29.467380
386.346196	16946.468797	29.472397
386.186891	16979.968110	29.477415
386.677433	17006.304438	29.482432
386.974537	17045.575382	29.487450
387.139486	17072.805791	29.492468
387.696635	17103.748404	29.497485
387.995859	17124.383368	29.502503
388.752731	17155.094268	29.507520
389.213165	17177.696063	29.512538
389.835914	17217.249401	29.517556
390.233549	17218.993078	29.522573
390.242958	17262.827980	29.527591
390.685913	17291.556556	29.532608
391.429059	17312.233633	29.537626
391.253350	17347.130801	29.542644
392.202307	17362.678825	29.547661
392.286234	17393.579312	29.552679
392.911046	17428.796345	29.557696
393.530925	17446.191341	29.562714
393.673203	17485.568776	29.567732
394.162503	17500.253975	29.572749
394.394968	17528.261815	29.577767
394.935338	17559.372184	29.582784
395.100517	17583.185775	29.587802
395.220158	17614.903050	29.592820
395.993795	17641.876450	29.597837
396.392091	17678.438795	29.602855
396.573488	17723.967272	29.607872
396.759652	17741.291942	29.612890
396.831601	17776.770297	29.617908
397.744915	17810.591832	29.622925
397.971495	17840.738191	29.627943
398.380181	17872.676474	29.632960
399.080108	17910.768092	29.637978
399.381216	17952.658439	29.642996
399.438193	17985.521508	29.648013
400.052428	18023.858163	29.653031
400.477046	18059.440028	29.658048
400.655550	18100.105398	29.663066
401.162699	18124.198015	29.668084
401.607006	18152.787809	29.673101
402.366236	18175.112736	29.678119
403.236809	18216.974873	29.683136
403.876290	18232.516393	29.688154
404.399143	18263.693172	29.693172
405.066277	18270.054821	29.698189
405.218036	18296.324876	29.703207
405.688892	18319.273144	29.708224
405.834506	18324.613539	29.713242
405.791128	18354.008599	29.718260
406.278999	18376.483750	29.723277
406.522340	18413.968614	29.728295
407.177333	18437.507824	29.733312
407.693438	18455.476028	29.738330
407.392844	18487.621501	29.743348
407.981138	18520.268360	29.748365
408.194167	18559.248635	29.753383
408.631302	18583.313748	29.758400
408.734521	18620.183997	29.763418
408.837810	18662.501887	29.768436
409.262297	18688.453935	29.773453
409.765871	18738.381558	29.778471
410.452811	18755.511814	29.783488
411.904140	18759.381640	29.788506
412.464572	18782.429714	29.793524
413.220570	18791.231130	29.798541
413.619364	18812.927745	29.803559
413.969578	18837.254361	29.808576
414.263766	18845.864409	29.813594
414.372842	18856.586781	29.818612
414.650215	18864.751849	29.823629
414.852800	18894.887141	29.828647
415.051608	18910.994080	29.833664
415.443831	18937.717490	29.838682
415.601141	18983.373176	29.843700
416.430123	18997.039457	29.848717
416.556825	19028.585241	29.853735
417.322545	19063.429171	29.858752
417.461098	19087.512318	29.863770
418.099244	19118.762213	29.868788
418.425443	19142.460005	29.873805
419.040783	19182.347510	29.878823
419.244582	19202.013732	29.883840
419.481243	19226.204702	29.888858
419.476996	19266.055297	29.893876
419.627431	19297.445464	29.898893
420.279599	19342.033098	29.903911
420.771117	19381.285259	29.908928
421.476098	19418.696622	29.913946
421.861789	19457.200793	29.918964
422.427434	19484.760596	29.923981
423.081923	19510.422222	29.928999
423.298393	19555.957541	29.934016
423.916668	19571.684515	29.939034
424.376135	19608.288105	29.944052
424.975389	19637.410334	29.949069
425.264138	19661.090073	29.954087
425.941444	19694.793059	29.959104
426.310761	19708.127642	29.964122
426.469566	19745.985120	29.969140
427.256996	19757.902957	29.974157
427.503204	19796.047064	29.979175
427.744319	19817.217368	29.984192
428.441032	19828.942993	29.989210
428.943357	19864.834356	29.994228
429.521944	19887.647283	29.999245
429.892183	19919.971923	30.004263
429.843564	19958.535889	30.009280
430.470161	19979.600897	30.014298
430.415658	20009.178420	30.019316
430.793914	20034.914844	30.024333
431.541253	20066.874544	30.029351
431.554446	20103.142850	30.034368
432.015941	20123.754363	30.039386
432.189248	20159.404680	30.044404
432.570717	20196.948988	30.049421
433.204831	20236.276260	30.054439
433.534027	20255.491475	30.059456
434.349995	20285.348225	30.064474
434.548394	20326.196558	30.069492
434.979105	20352.725279	30.074509
435.783753	20388.016432	30.079527
435.728174	20419.222732	30.084544
436.552443	20455.041710	30.089562
436.793173	20488.551742	30.094580
437.254532	20526.065996	30.099597
437.683825	20564.016234	30.104615
438.098808	20598.958058	30.109632
438.825556	20620.820328	30.114650
438.688669	20657.928540	30.119668
439.137369	20696.730497	30.124685
439.801909	20718.405139	30.129703
439.868354	20767.825300	30.134720
440.650885	20792.228235	30.139738
441.396131	20836.088224	30.144756
441.826641	20875.304625	30.149773
442.568194	20893.286976	30.154791
442.768040	20925.791650	30.159808
443.547580	20956.603709	30.164826
443.852669	20999.423026	30.169844
444.037991	21036.650123	30.174861
444.943062	21064.334654	30.179879
444.849055	21094.494645	30.184896
445.376799	21124.075222	30.189914
445.776283	21153.523498	30.194932
445.985706	21183.872379	30.199949
446.880018	21220.469521	30.204967
446.956546	21254.004191	30.209984
447.426749	21286.201911	30.215002
448.567073	21301.971111	30.220020
449.487582	21334.711504	30.225037
449.975101	21367.850944	30.230055
450.131405	21382.383757	30.235072
450.891199	21393.791387	30.240090
451.229314	21411.911067	30.245108
451.688548	21434.822052	30.250125
451.922396	21457.195614	30.255143
452.163353	21477.443946	30.260160
452.864616	21505.316882	30.265178
452.970233	21531.828502	30.270196
453.081433	21570.870679	30.275213
453.809489	21598.287432	30.280231
453.985179	21624.820336	30.285248
454.353689	21668.518201	30.290266
454.554744	21700.456420	30.295284
455.157457	21743.074397	30.300301
455.268240	21776.579516	30.305319
455.370672	21810.389265	30.310336
456.113223	21843.647384	30.315354
456.705352	21879.469577	30.320372
456.449759	21922.918659	30.325389
457.526734	21959.466370	30.330407
457.372384	22008.191530	30.335424
458.056039	22062.169860	30.340442
458.600308	22095.197033	30.345460
458.996338	22138.586216	30.350477
459.490053	22184.621338	30.355495
460.290322	22219.992917	30.360512
460.746377	22258.266686	30.365530
461.075306	22305.780011	30.370548
461.513351	22342.945507	30.375565
462.138114	22372.580707	30.380583
462.311709	22420.830356	30.385600
462.937980	22460.536200	30.390618
463.490869	22507.084250	30.395636
463.560207	22550.915700	30.400653
464.273608	22593.836545	30.405671
464.623680	22643.907360	30.410688
465.228034	22687.819364	30.415706
465.345764	22736.746011	30.420724
465.846186	22770.806315	30.425741
466.909189	22820.618399	30.430759
467.430585	22859.956000	30.435776
468.018583	22891.003998	30.440794
468.724177	22929.738225	30.445812
469.301342	22970.417268	30.450829
469.722203	22995.996571	30.455847
469.792646	23023.957717	30.460864
470.567697	23053.795525	30.465882
471.101355	23098.041295	30.470900
471.659461	23133.653564	30.475917
472.241056	23165.788533	30.480935
472.210287	23198.907251	30.485952
472.948589	23230.726736	30.490970
473.254915	23274.255406	30.495988
473.619508	23312.862150	30.501005
474.180040	23350.372040	30.506023
474.313350	23397.938701	30.511040
474.781517	23427.819799	30.516058
475.467699	23479.968822	30.521076
475.745092	23522.266896	30.526093
477.124948	23546.607306	30.531111
477.395204	23578.731267	30.536128
477.626984	23621.603223	30.541146
478.693385	23638.009628	30.546164
479.110258	23669.061992	30.551181
479.647013	23696.320664	30.556199
479.807633	23724.130826	30.561216
480.369426	23744.334886	30.566234
480.975133	23788.163859	30.571252
481.283523	23818.098715	30.576269
481.901111	23840.227037	30.581287
482.308392	23862.362110	30.586304
482.680372	23900.315306	30.591322
483.176557	23934.724588	30.596340
483.133888	23958.701458	30.601357
483.846282	23987.260733	30.606375
484.318861	24024.712181	30.611392
484.796077	24061.317758	30.616410
485.157781	24085.209922	30.621428
485.243033	24129.036879	30.626445
485.907929	24158.562685	30.631463
486.103600	24195.651393	30.636480
486.627000	24240.720421	30.641498
487.191726	24270.729513	30.646516
487.561431	24326.974344	30.651533
488.423383	24353.758542	30.656551
488.563208	24405.067317	30.661568
489.099494	24454.713209	30.666586
489.900137	24484.859214	30.671604
489.649308	24536.441753	30.676621
490.125941	24577.049541	30.681639
490.914799	24630.001287	30.686656
491.483754	24688.834116	30.691674
491.747688	24723.173386	30.696692
492.056982	24777.717644	30.701709
492.937449	24818.490953	30.706727
493.254528	24875.448772	30.711744
494.000850	24926.798101	30.716762
494.526690	24965.133439	30.721780
494.727365	25026.160219	30.726797
495.125324	25067.422237	30.731815
496.000221	25111.727953	30.736832
496.995356	25153.585153	30.741850
497.331223	25197.532668	30.746868
497.641618	25243.019734	30.751885
498.256873	25274.980287	30.756903
498.846562	25326.535463	30.761920
499.541664	25359.811663	30.766938
500.573967	25388.628151	30.771956
500.806408	25417.599675	30.776973
501.215400	25441.558023	30.781991
501.408612	25488.588816	30.787008
502.017346	25532.927068	30.792026
502.581743	25569.716008	30.797044
502.994550	25614.460683	30.802061
503.482337	25651.833953	30.807079
504.332608	25690.920539	30.812096
504.640629	25727.679778	30.817114
505.429517	25767.755564	30.822132
505.333593	25811.267770	30.827149
505.684718	25849.427438	30.832167
506.243832	25891.156708	30.837184
506.498505	25936.488387	30.842202
507.203368	25967.392990	30.847220
507.457385	26037.192116	30.852237
508.182497	26062.747570	30.857255
508.648573	26108.959140	30.862272
509.005449	26152.624670	30.867290
509.580593	26194.177278	30.872308
510.166433	26220.763580	30.877325
510.688425	26268.120862	30.882343
511.317253	26308.025748	30.887360
511.585068	26348.286037	30.892378
512.268531	26386.331803	30.897396
512.491503	26440.184833	30.902413
513.029799	26489.414425	30.907431
513.599056	26529.414435	30.912448
513.776578	26580.483862	30.917466
514.558104	26624.388713	30.922484
514.751611	26669.770802	30.927501
515.114955	26716.636270	30.932519
515.965679	26768.746168	30.937536
516.219037	26819.808998	30.942554
516.820771	26868.686140	30.947572
517.160174	26925.891899	30.952589
518.212522	26974.587287	30.957607
518.787304	27019.224189	30.962624
519.585486	27059.560135	30.967642
520.483311	27102.738688	30.972660
521.223818	27137.201808	30.977677
521.506395	27174.279608	30.982695
522.032722	27203.403713	30.987712
522.585406	27230.278237	30.992730
523.371120	27272.244446	30.997748
523.622250	27317.441117	31.002765
524.288982	27348.815357	31.007783
524.787474	27389.863259	31.012800
524.981788	27435.902887	31.017818
526.093004	27464.688484	31.022836
525.838216	27517.236889	31.027853
526.227591	27545.713722	31.032871
526.952955	27601.317711	31.037888
527.297179	27646.938541	31.042906
527.958307	27680.654361	31.047924
528.574404	27736.890777	31.052941
529.285955	27772.674079	31.057959
529.889679	27811.837394	31.062976
530.060976	27864.347420	31.067994
531.011489	27894.527183	31.073012
531.158218	27945.344237	31.078029
531.479943	27997.272895	31.083047
532.340807	28026.773824	31.088064
532.037184	28097.081951	31.093082
532.892231	28134.166893	31.098100
533.063019	28203.517452	31.103117
533.478066	28251.202505	31.108135
534.485702	28306.072158	31.113152
534.683253	28367.000967	31.118170
535.512597	28433.789281	31.123188
535.670020	28472.120732	31.128205
536.209786	28529.161561	31.133223
536.511379	28573.929784	31.138240
537.599711	28626.420705	31.143258
539.147478	28640.766851	31.148276
540.046092	28671.222656	31.153293
541.440564	28684.962905	31.158311
542.333049	28688.894431	31.163328
542.686034	28710.804513	31.168346
543.454563	28717.214175	31.173364
543.803528	28739.659163	31.178381
544.111576	28749.962141	31.183399
544.516767	28766.918835	31.188416
544.626199	28786.544943	31.193434
545.242332	28803.928241	31.198452
545.012830	28833.561760	31.203469
545.361189	28872.377488	31.208487
546.038610	28913.058778	31.213504
546.401154	28946.449726	31.218522
546.832875	28988.092245	31.223540
547.079993	29040.061332	31.228557
547.505240	29082.250392	31.233575
548.034357	29135.114119	31.238592
548.039502	29174.976492	31.243610
548.762434	29238.165145	31.248628
548.908203	29295.417977	31.253645
549.243349	29370.334052	31.258663
550.268009	29418.133460	31.263680
550.668731	29483.287592	31.268698
551.531912	29537.275084	31.273716
551.978926	29598.408313	31.278733
552.535684	29659.467555	31.283751
553.019464	29718.035984	31.288768
553.792433	29764.153942	31.293786
554.972414	29804.669162	31.298804
555.577346	29864.433912	31.303821
555.818994	29920.393951	31.308839
556.576526	29968.918354	31.313856
557.055617	30021.022249	31.318874
557.369610	30066.237031	31.323892
558.327685	30110.599171	31.328909
558.765609	30157.118326	31.333927
559.717977	30207.054472	31.338944
559.961984	30250.186361	31.343962
561.061236	30298.175052	31.348980
561.253560	30340.527390	31.353997
561.280465	30402.417687	31.359015
562.400158	30429.339595	31.364032
562.675519	30494.180443	31.369050
563.071915	30535.674928	31.374068
563.621513	30584.798507	31.379085
564.291456	30644.374503	31.384103
565.018252	30688.875917	31.389120
565.233359	30751.714726	31.394138
566.114801	30782.512929	31.399156
566.912061	30831.493782	31.404173
567.725013	30870.303307	31.409191
568.997073	30900.030821	31.414208
569.283722	30938.523999	31.419226
569.814373	30955.218695	31.424244
570.039802	30993.780068	31.429261
570.701281	31028.538277	31.434279
570.642053	31060.274873	31.439296
571.406188	31101.401729	31.444314
572.314400	31136.812789	31.449332
572.680891	31178.554811	31.454349
573.057597	31228.919896	31.459367
573.447846	31258.150167	31.464384
573.809934	31317.073104	31.469402
574.146921	31348.524919	31.474420
574.864708	31416.033551	31.479437
575.095053	31474.968577	31.484455
575.630543	31514.649722	31.489472
576.110650	31590.664045	31.494490
576.944271	31640.267260	31.499508
577.242949	31713.710365	31.504525
577.443453	31766.575025	31.509543
578.378059	31827.567979	31.514560
578.651133	31899.641553	31.519578
579.988951	31955.353562	31.524596
580.597725	32015.663019	31.529613
580.937283	32075.383509	31.534631
581.735898	32117.511464	31.539648
581.982760	32176.782100	31.544666
582.836477	32227.514035	31.549684
583.648162	32292.500376	31.554701
584.196628	32346.567735	31.559719
585.168082	32387.034295	31.564736
585.978220	32440.790753	31.569754
586.404224	32493.159986	31.574772
586.906963	32546.075160	31.579789
587.748158	32591.108890	31.584807
588.218248	32634.787934	31.589824
588.361351	32686.892309	31.594842
588.858111	32729.101424	31.599860
589.602171	32788.452699	31.604877
590.250859	32842.128988	31.609895
590.989725	32898.853820	31.614912
591.526301	32960.480239	31.619930
591.941672	33006.741493	31.624948
592.684495	33053.160378	31.629965
593.402711	33117.091384	31.634983
594.364409	33150.814766	31.640000
594.719470	33206.266636	31.645018
595.281280	33260.587068	31.650036
596.350957	33306.875797	31.655053
596.495488	33353.125979	31.660071
597.445399	33387.438117	31.665088
598.043528	33426.305222	31.670106
598.884954	33470.483784	31.675124
599.595274	33497.603617	31.680141
600.378126	33537.215552	31.685159
601.303265	33563.363356	31.690176
601.701072	33601.673218	31.695194
602.060881	33622.767493	31.700212
602.705419	33645.742766	31.705229
602.482278	33679.815124	31.710247
603.289079	33720.870787	31.715264
603.746066	33770.891914	31.720282
604.264597	33808.022817	31.725300
604.489048	33858.672379	31.730317
604.736844	33903.622898	31.735335
605.701383	33949.239711	31.740352
605.791505	34010.572252	31.745370
606.380780	34069.713153	31.750388
607.196981	34128.706202	31.755405
607.585741	34179.516591	31.760423
608.069110	34236.568864	31.765440
608.894784	34304.095748	31.770458
609.322865	34381.876263	31.775476
609.798721	34426.831287	31.780493
610.070827	34507.905176	31.785511
610.970283	34558.856097	31.790528
611.438281	34631.801187	31.795546
611.942302	34702.090829	31.800564
612.516628	34765.384247	31.805581
613.260699	34835.440742	31.810599
614.114766	34909.454320	31.815616
615.012349	34971.941911	31.820634
615.737103	35032.346335	31.825652
616.782213	35093.247009	31.830669
616.974789	35146.487857	31.835687
617.966991	35185.569056	31.840704
618.701780	35256.757575	31.845722
619.269674	35311.298136	31.850740
620.414982	35366.938780	31.855757
620.532594	35428.059313	31.860775
621.335388	35475.980999	31.865792
621.774622	35530.749290	31.870810
622.222893	35588.518059	31.875828
622.991982	35652.286738	31.880845
623.054989	35709.600166	31.885863
623.946810	35769.170299	31.890880
624.302710	35827.194236	31.895898
624.680765	35905.435968	31.900916
625.526494	35956.347683	31.905933
625.827425	36040.790398	31.910951
626.673200	36098.444021	31.915968
627.730170	36162.532992	31.920986
628.685171	36225.960507	31.926004
629.281240	36285.484973	31.931021
629.878086	36330.854685	31.936039
630.847801	36381.286000	31.941056
631.724047	36449.081519	31.946074
632.410766	36482.563775	31.951092
633.364475	36522.035774	31.956109
633.412535	36589.643680	31.961127
634.095189	36614.460071	31.966144
634.833033	36664.473511	31.971162
635.306761	36704.148501	31.976180
635.952315	36751.189146	31.981197
636.257465	36798.987316	31.986215
636.840080	36833.201075	31.991232
637.652719	36888.002626	31.996250
637.892510	36939.004348	32.001268
638.821501	36991.258730	32.006285
639.073241	37043.945910	32.011303
639.963196	37100.951079	32.016320
640.786413	37145.936921	32.021338
641.624908	37186.950337	32.026356
642.399139	37230.126277	32.031373
642.944897	37268.908178	32.036391
644.041570	37319.418275	32.041408
644.764407	37355.160670	32.046426
644.926940	37413.804251	32.051444
645.775098	37443.308317	32.056461
646.184496	37502.608231	32.061479
646.744155	37546.323700	32.066496
647.331184	37595.562945	32.071514
647.721876	37640.549603	32.076532
648.606420	37697.806779	32.081549
649.183934	37755.912447	32.086567
649.607574	37817.147441	32.091584
650.119736	37872.253895	32.096602
650.301625	37943.630127	32.101620
650.901676	37992.952024	32.106637
651.224718	38066.256759	32.111655
652.003134	38138.424975	32.116672
652.763025	38211.462106	32.121690
653.284634	38286.902686	32.126708
654.006251	38367.239264	32.131725
654.458539	38440.129258	32.136743
655.500986	38498.131906	32.141760
656.210292	38573.643215	32.146778
656.685125	38650.105177	32.151796
657.680658	38718.001196	32.156813
658.448091	38783.374591	32.161831
658.895792	38858.909899	32.166848
660.112968	38908.233963	32.171866
660.871192	38964.703457	32.176884
662.046902	39019.991824	32.181901
662.754355	39076.723649	32.186919
663.617741	39117.966437	32.191936
664.672458	39156.873468	32.196954
664.987513	39211.419597	32.201972
665.843704	39258.018962	32.206989
666.196931	39306.680688	32.212007
666.683126	39351.145765	32.217024
667.565636	39412.923712	32.222042
668.069348	39472.909330	32.227060
668.403435	39518.422475	32.232077
668.559904	39576.413763	32.237095
669.103503	39629.153963	32.242112
670.015916	39686.467034	32.247130
670.062528	39746.412855	32.252148
670.714811	39805.792525	32.257165
671.103482	39864.470056	32.262183
671.767317	39937.277586	32.267200
672.231389	40002.927894	32.272218
672.983780	40083.806996	32.277236
674.105961	40140.591452	32.282253
674.243966	40230.283392	32.287271
675.046580	40288.891743	32.292288
676.155499	40362.085965	32.297306
676.872603	40428.438805	32.302324
677.804932	40488.440174	32.307341
678.308397	40548.245099	32.312359
678.815847	40621.807442	32.317376
679.413311	40688.246572	32.322394
679.961050	40760.762265	32.327412
680.767555	40834.558617	32.332429
681.387609	40906.366365	32.337447
681.968973	40982.993712	32.342464
683.334601	41036.563066	32.347482
683.513824	41128.763804	32.352500
684.116072	41181.805404	32.357517
684.725279	41263.889365	32.362535
685.390981	41342.022029	32.367552
686.086318	41416.696515	32.372570
686.598694	41500.162776	32.377588
687.713855	41569.623457	32.382605
688.158742	41660.106712	32.387623
688.703637	41735.137724	32.392640
689.873544	41810.744563	32.397658
690.193226	41891.164859	32.402676
690.964560	41957.738929	32.407693
691.711692	42054.185013	32.412711
692.173079	42132.063598	32.417728
693.127456	42207.697031	32.422746
693.798047	42288.388205	32.427764
694.439431	42355.814090	32.432781
695.316484	42445.955081	32.437799
695.823145	42521.440365	32.442816
696.835004	42592.908876	32.447834
697.071592	42677.405755	32.452852
698.282038	42748.616177	32.457869
698.975451	42831.886566	32.462887
699.400857	42911.127638	32.467904
700.449432	42989.484401	32.472922
700.860338	43067.198586	32.477940
702.105125	43124.165818	32.482957
703.228002	43202.559035	32.487975
703.815482	43265.751102	32.492992
704.869266	43335.651376	32.498010
704.763637	43407.941533	32.503028
705.630066	43463.566354	32.508045
706.326501	43537.372875	32.513063
706.848188	43597.586107	32.518080
707.516873	43672.621593	32.523098
709.352918	43699.887731	32.528116
710.427275	43741.779987	32.533133
711.099115	43781.752183	32.538151
711.398927	43832.982557	32.543168
712.472658	43867.808896	32.548186
713.138044	43917.574362	32.553204
713.693035	43960.776981	32.558221
714.482301	44014.012026	32.563239
714.747886	44058.964470	32.568256
715.163210	44112.120543	32.573274
715.809850	44188.455179	32.578292
716.109327	44242.686908	32.583309
716.957984	44309.891812	32.588327
717.799492	44372.470157	32.593344
718.919043	44429.512101	32.598362
719.274024	44496.786855	32.603380
720.082241	44553.531750	32.608397
721.161463	44628.401899	32.613415
721.380130	44686.310543	32.618432
722.253201	44755.554413	32.623450
722.409673	44819.230865	32.628468
723.206944	44879.600261	32.633485
723.825756	44961.662364	32.638503
724.204458	45037.563842	32.643520
725.012797	45110.876535	32.648538
725.704061	45183.403686	32.653556
726.363212	45264.378674	32.658573
727.306508	45346.062820	32.663591
727.774354	45424.264312	32.668608
728.633029	45504.252714	32.673626
729.242147	45592.383059	32.678644
730.255356	45664.690588	32.683661
731.367192	45741.014745	32.688679
731.652679	45831.971020	32.693696
732.273338	45907.588507	32.698714
733.109257	45989.930057	32.703732
733.756342	46066.354856	32.708749
734.965894	46155.540872	32.713767
735.652680	46222.564361	32.718784
736.514083	46296.646557	32.723802
737.437330	46371.700446	32.728820
738.648043	46430.100561	32.733837
739.469456	46481.892989	32.738855
740.173178	46550.517819	32.743872
740.762229	46612.216773	32.748890
741.439449	46688.831945	32.753908
742.302124	46744.960032	32.758925
742.862276	46806.528597	32.763943
744.007361	46880.908854	32.768960
744.535333	46947.931995	32.773978
745.315987	47020.698616	32.778996
745.760951	47082.939607	32.784013
746.620215	47149.229254	32.789031
747.134669	47214.476024	32.794048
747.815784	47267.299615	32.799066
748.170429	47338.930067	32.804084
748.813171	47409.681963	32.809101
749.635418	47481.348991	32.814119
749.966344	47549.323965	32.819136
750.536011	47626.231686	32.824154
751.308254	47712.418800	32.829172
752.202616	47781.901562	32.834189
753.425193	47839.865883	32.839207
753.827698	47931.211932	32.844224
754.693854	48013.135313	32.849242
755.625997	48082.960334	32.854260
756.201942	48161.535419	32.859277
756.917460	48235.330291	32.864295
757.292958	48316.250877	32.869312
758.529235	48406.135067	32.874330
759.144292	48479.928016	32.879348
759.687610	48566.502826	32.884365
761.001417	48641.680908	32.889383
761.743662	48727.625299	32.894400
762.041396	48810.668380	32.899418
762.870539	48891.825459	32.904436
763.359436	48982.285930	32.909453
764.198486	49065.155678	32.914471
764.809251	49161.586889	32.919488
765.745007	49235.956730	32.924506
766.463685	49337.849800	32.929524
766.893300	49433.986294	32.934541
767.625237	49527.560147	32.939559
768.571736	49632.719424	32.944576
769.557112	49719.213695	32.949594
770.453604	49794.333698	32.954612
771.170597	49891.395703	32.959629
772.082914	49987.117526	32.964647
772.643113	50072.961687	32.969664
773.902954	50162.033667	32.974682
774.950811	50249.236914	32.979700
775.731482	50347.648236	32.984717
776.545637	50419.470413	32.989735
776.901044	50503.080226	32.994752
777.738256	50581.447670	32.999770
778.863574	50664.601170	33.004788
779.715761	50754.962298	33.009805
780.682814	50824.789362	33.014823
781.071773	50908.954313	33.019840
781.966217	50979.876002	33.024858
783.072417	51065.439191	33.029876
783.514444	51157.720145	33.034893
784.560599	51229.057345	33.039911
785.341702	51308.339492	33.044928
785.798575	51396.709099	33.049946
786.751916	51471.290578	33.054964
787.344077	51546.570520	33.059981
788.141718	51635.483540	33.064999
788.967342	51711.717997	33.070016
789.999266	51786.117850	33.075034
790.935189	51847.524107	33.080052
791.799021	51910.463262	33.085069
792.705254	51964.259105	33.090087
793.547338	52039.741190	33.095104
794.332366	52104.495683	33.100122
795.116807	52160.861612	33.105140
796.282464	52209.750206	33.110157
797.192638	52267.526170	33.115175
797.765141	52333.669285	33.120192
798.765835	52400.400964	33.125210
799.735454	52441.181727	33.130228
800.650589	52503.240540	33.135245
801.656054	52546.682784	33.140263
802.310813	52611.415647	33.145280
802.814739	52665.116652	33.150298
803.544036	52728.351510	33.155316
804.202106	52787.463304	33.160333
805.048406	52855.436378	33.165351
805.446834	52934.044875	33.170368
806.105100	53002.780675	33.175386
807.217647	53069.762150	33.180404
807.411126	53153.709875	33.185421
808.299848	53219.348241	33.190439
808.591538	53304.309976	33.195456
809.293560	53394.064352	33.200474
810.270821	53484.678073	33.205492
810.847545	53568.661407	33.210509
811.663566	53660.292756	33.215527
812.033346	53762.531548	33.220544
813.178457	53858.880795	33.225562
813.783071	53944.584812	33.230580
814.445566	54046.605008	33.235597
815.476574	54137.566948	33.240615
816.483051	54241.566233	33.245632
817.327473	54324.894942	33.250650
818.478753	54422.496152	33.255668
819.707865	54505.581386	33.260685
821.304280	54568.952951	33.265703
822.380337	54640.658699	33.270720
823.642087	54693.541186	33.275738
824.692557	54756.368990	33.280756
824.973829	54834.272023	33.285773
826.305465	54885.944456	33.290791
826.835701	54950.702316	33.295808
827.551078	55026.573691	33.300826
828.113386	55081.752982	33.305844
828.618694	55139.094319	33.310861
830.046457	55221.639831	33.315879
830.526024	55290.750471	33.320896
830.749025	55357.897734	33.325914
831.623565	55431.652602	33.330932
832.102251	55525.016879	33.335949
833.198538	55596.549545	33.340967
834.071553	55672.641574	33.345984
834.587801	55744.402869	33.351002
835.338768	55817.194062	33.356020
835.977650	55894.489104	33.361037
836.647249	55966.735097	33.366055
837.136998	56051.419231	33.371072
837.723092	56141.836916	33.376090
838.899795	56207.396013	33.381108
839.627538	56303.029064	33.386125
840.655736	56388.039440	33.391143
841.761859	56475.124476	33.396160
842.302773	56577.061318	33.401178
843.926203	56638.939421	33.406196
844.421446	56724.014069	33.411213
845.716418	56790.673962	33.416231
846.347583	56870.455649	33.421248
847.063569	56966.630690	33.426266
848.064185	57028.501888	33.431284
848.683162	57125.529782	33.436301
849.670637	57202.377063	33.441319
850.441113	57291.574556	33.446336
851.299349	57363.612904	33.451354
851.971576	57454.297975	33.456372
853.040199	57542.618940	33.461389
853.685320	57628.561023	33.466407
854.533795	57720.996762	33.471424
855.381403	57822.806427	33.476442
856.504223	57891.603460	33.481460
857.202808	57992.560106	33.486477
858.281026	58065.791133	33.491495
859.138341	58156.649085	33.496512
860.117615	58239.854114	33.501530
861.164083	58324.068583	33.506548
861.714885	58415.494352	33.511565
862.710413	58497.637143	33.516583
863.525019	58578.931388	33.521600
864.093556	58676.947843	33.526618
865.058413	58759.759687	33.531636
866.092700	58847.009402	33.536653
866.842107	58948.468311	33.541671
867.447760	59035.484023	33.546688
868.230110	59127.918342	33.551706
869.422387	59237.201566	33.556724
869.864908	59329.855145	33.561741
870.382706	59413.748224	33.566759
871.357949	59525.492507	33.571776
871.886735	59634.245854	33.576794
872.998414	59725.721401	33.581812
873.943380	59838.157525	33.586829
874.980507	59946.613932	33.591847
875.594940	60045.785885	33.596864
876.474010	60148.462077	33.601882
877.653821	60257.554331	33.606900
878.156719	60360.976721	33.611917
878.955040	60474.535649	33.616935
880.036162	60565.950700	33.621952
881.056710	60665.538090	33.626970
882.684658	60717.602817	33.631988
884.002162	60805.845971	33.637005
884.562663	60879.640911	33.642023
885.790091	60951.391250	33.647040
886.671062	61036.430528	33.652058
887.380073	61103.274921	33.657076
888.017349	61181.561595	33.662093
888.496552	61275.734610	33.667111
889.435415	61367.245666	33.672128
890.355413	61452.662691	33.677146
891.605400	61536.158240	33.682164
892.239347	61623.857205	33.687181
892.940641	61714.833050	33.692199
894.065426	61800.983235	33.697216
894.529819	61902.146646	33.702234
895.312392	61982.118708	33.707252
895.910243	62098.520266	33.712269
896.937373	62198.244182	33.717287
897.889525	62287.686068	33.722304
899.732043	62364.986939	33.727322
901.263318	62444.936560	33.732340
902.793120	62523.427824	33.737357
903.938960	62593.918472	33.742375
905.237350	62651.980959	33.747392
905.837406	62715.554733	33.752410
906.606556	62777.560759	33.757428
907.227817	62848.666354	33.762445
908.403682	62919.570282	33.767463
909.656834	62976.235689	33.772480
910.017644	63052.287758	33.777498
910.735825	63120.928387	33.782516
911.232146	63194.881529	33.787533
911.718106	63290.730899	33.792551
912.701750	63367.323037	33.797568
913.257894	63462.170491	33.802586
914.320635	63555.241949	33.807604
915.027876	63647.931459	33.812621
915.592881	63736.803853	33.817639
916.497753	63842.954094	33.822656
917.148386	63948.940102	33.827674
918.073820	64049.356281	33.832692
918.931507	64151.435467	33.837709
919.517262	64264.662502	33.842727
920.616599	64372.382764	33.847744
921.817790	64460.869908	33.852762
923.546479	64556.875300	33.857780
924.394363	64654.038265	33.862797
925.209558	64751.788039	33.867815
926.277777	64829.279000	33.872832
926.982622	64941.815228	33.877850
928.095690	65027.593440	33.882868
928.797654	65120.344617	33.887885
929.825516	65219.992653	33.892903
930.624291	65304.877780	33.897920
931.194114	65400.196936	33.902938
932.052609	65486.939940	33.907956
932.969600	65579.870731	33.912973
933.649551	65675.034759	33.917991
934.551683	65781.821536	33.923008
935.004845	65878.560791	33.928026
936.013654	65976.791337	33.933044
937.128520	66085.374678	33.938061
937.616556	66211.707856	33.943079
938.559279	66309.091506	33.948096
939.334805	66425.573261	33.953114
939.944157	66545.960818	33.958132
941.046160	66670.989597	33.963149
941.683479	66797.975621	33.968167
942.888652	66916.059689	33.973184
943.395818	67044.432541	33.978202
944.704931	67176.102595	33.983220
945.798444	67290.511124	33.988237
946.744297	67427.250283	33.993255
947.568040	67559.379201	33.998272
948.561648	67685.758417	34.003290
950.234735	67788.478910	34.008308
951.584234	67898.731323	34.013325
952.719747	68015.291699	34.018343
954.167889	68123.009001	34.023360
954.993805	68230.851166	34.028378
955.673566	68343.227962	34.033396
956.861805	68448.132848	34.038413
957.572864	68555.249597	34.043431
958.578260	68658.933804	34.048448
959.513075	68771.026092	34.053466
960.222391	68884.525861	34.058484
961.286398	68994.267608	34.063501
962.121800	69110.743281	34.068519
963.433758	69212.372568	34.073536
964.936612	69324.775685	34.078554
966.003176	69412.109654	34.083572
966.976699	69518.943520	34.088589
968.070884	69612.181318	34.093607
969.190373	69711.101790	34.098624
969.875126	69825.956666	34.103642
971.219222	69917.443951	34.108660
972.303246	70008.777176	34.113677
973.235633	70107.350321	34.118695
974.230264	70195.305767	34.123712
974.836885	70289.117167	34.128730
975.804855	70395.792410	34.133748
976.543451	70497.930262	34.138765
977.713013	70588.045770	34.143783
978.763618	70706.543810	34.148800
979.436618	70797.137330	34.153818
980.389364	70894.700229	34.158836
981.462066	70995.871331	34.163853
981.939496	71121.830391	34.168871
983.112809	71205.718069	34.173888
983.927824	71304.960363	34.178906
984.913197	71403.973857	34.183924
985.723559	71497.884957	34.188941
986.785509	71600.539423	34.193959
987.993635	71690.021958	34.198976
988.718223	71800.477851	34.203994
989.319843	71898.878763	34.209012
990.272854	72007.315377	34.214029
991.456974	72135.702287	34.219047
992.171647	72232.696723	34.224064
993.095944	72359.875279	34.229082
994.150929	72476.279010	34.234100
994.928212	72588.165295	34.239117
996.071467	72706.622637	34.244135
997.096848	72838.780193	34.249152
997.861726	72949.653110	34.254170
999.026421	73068.526251	34.259188
1000.055116	73189.500741	34.264205
1000.768414	73304.156376	34.269223
1002.441338	73426.154635	34.274240
1003.401747	73535.938066	34.279258
1004.466722	73659.039223	34.284276
1005.662790	73780.692107	34.289293
1006.539245	73897.435850	34.294311
1007.547489	74004.231484	34.299328
1008.295772	74126.709712	34.304346
1009.306111	74261.975595	34.309364
1010.230649	74377.829750	34.314381
1011.432044	74509.477406	34.319399
1012.771679	74630.101466	34.324416
1013.843166	74734.160843	34.329434
1014.485039	74870.355222	34.334452
1015.807546	74976.056958	34.339469
1016.872000	75106.934017	34.344487
1017.957740	75219.215656	34.349504
1018.565886	75347.638938	34.354522
1019.653617	75461.887083	34.359540
1020.931896	75591.279693	34.364557
1021.284519	75721.812610	34.369575
1022.484071	75842.156521	34.374592
1023.606254	75961.925690	34.379610
1024.320619	76098.123123	34.384628
1025.640581	76220.864400	34.389645
1026.709224	76348.626682	34.394663
1028.054751	76462.434971	34.399680
1029.107476	76590.782766	34.404698
1030.242170	76717.114806	34.409716
1031.686150	76828.160164	34.414733
1032.352447	76958.505761	34.419751
1033.508634	77074.022484	34.424768
1034.594222	77196.680526	34.429786
1035.297802	77312.731986	34.434804
1037.157167	77419.612521	34.439821
1038.278572	77528.981197	34.444839
1039.653760	77622.224276	34.449856
1040.704907	77716.524297	34.454874
1043.020447	77768.654817	34.459892
1044.700478	77838.565326	34.464909
1045.409517	77915.425215	34.469927
1046.656178	77969.704633	34.474944
1047.667709	78037.908129	34.479962
1048.466523	78100.330642	34.484980
1049.730375	78171.401973	34.489997
1050.084143	78251.347258	34.495015
1050.922170	78320.742313	34.500032
1051.680421	78403.721032	34.505050
1052.456987	78483.144874	34.510068
1053.265382	78567.070722	34.515085
1053.682184	78669.990215	34.520103
1054.057373	78780.141639	34.525120
1055.165739	78888.407171	34.530138
1056.059900	79003.053605	34.535156
1056.989529	79123.516690	34.540173
1057.636597	79245.378127	34.545191
1058.400537	79369.421433	34.550208
1059.257159	79518.033626	34.555226
1059.994127	79655.047591	34.560244
1061.324765	79785.134800	34.565261
1061.927091	79941.951178	34.570279
1062.856017	80090.220952	34.575296
1063.599472	80241.011901	34.580314
1064.477310	80404.058738	34.585332
1065.698832	80556.261469	34.590349
1066.784627	80721.218405	34.595367
1068.233668	80874.860193	34.600384
1069.550611	81022.733547	34.605402
1071.082268	81182.755602	34.610420
1072.096339	81311.303353	34.615437
1073.209399	81454.888173	34.620455
1074.835467	81594.137839	34.625472
1076.019803	81743.289107	34.630490
1077.126964	81886.561744	34.635508
1078.040744	82023.841351	34.640525
1079.220839	82157.754163	34.645543
1080.475075	82288.532983	34.650560
1081.935574	82429.401363	34.655578
1082.858251	82561.322006	34.660596
1084.466050	82670.128412	34.665613
1085.524207	82804.633738	34.670631
1086.347999	82931.944637	34.675648
1088.087302	83047.541063	34.680666
1089.823795	83167.431375	34.685684
1091.486154	83262.569820	34.690701
1092.515456	83373.261079	34.695719
1093.807613	83475.944975	34.700736
1094.767131	83572.657063	34.705754
1095.484590	83668.219483	34.710772
1096.498203	83769.229417	34.715789
1097.697408	83868.869960	34.720807
1098.686626	83975.846834	34.725824
1100.250835	84065.377511	34.730842
1100.816182	84158.791399	34.735860
1102.062963	84249.075139	34.740877
1102.304057	84358.518600	34.745895
1103.301959	84449.911297	34.750912
1104.421794	84548.916438	34.755930
1105.213467	84672.348186	34.760948
1106.111616	84771.585626	34.765965
1107.141625	84901.866246	34.770983
1107.740272	85030.502789	34.776000
1108.681669	85143.044575	34.781018
1109.844455	85269.499988	34.786036
1111.221952	85403.863576	34.791053
1111.676345	85544.470137	34.796071
1112.877053	85684.870414	34.801088
1114.117570	85807.788431	34.806106
1115.163801	85951.446094	34.811124
1116.256641	86089.033448	34.816141
1117.737392	86233.983376	34.821159
1118.515789	86370.218805	34.826176
1119.679900	86512.805517	34.831194
1120.721281	86655.197704	34.836212
1121.843175	86802.206702	34.841229
1122.891979	86947.034122	34.846247
1123.904904	87092.247629	34.851264
1125.007502	87242.474996	34.856282
1126.142801	87393.438060	34.861300
1127.519688	87524.659630	34.866317
1128.858255	87682.314308	34.871335
1129.912132	87827.614789	34.876352
1131.165126	87966.643129	34.881370
1132.307735	88121.511824	34.886388
1133.965728	88253.900955	34.891405
1135.204009	88401.009853	34.896423
1136.359107	88537.635422	34.901440
1138.191052	88648.586839	34.906458
1139.780053	88763.359148	34.911476
1141.462002	88891.252084	34.916493
1142.563295	88995.909008	34.921511
1143.283842	89125.081869	34.926528
1144.595554	89238.654961	34.931546
1145.723660	89359.207991	34.936564
1146.585614	89488.290957	34.941581
1147.408080	89604.593558	34.946599
1148.537519	89729.992717	34.951616
1149.535603	89847.122448	34.956634
1149.989089	89989.965248	34.961652
1150.943161	90122.281655	34.966669
1152.202256	90263.562523	34.971687
1153.029061	90419.901803	34.976704
1154.126499	90559.730385	34.981722
1154.882974	90718.992211	34.986740
1156.351260	90876.706340	34.991757
1157.260108	91020.514338	34.996775
1158.255605	91175.813925	35.001792
1159.410134	91297.492885	35.006810
1160.460180	91453.348648	35.011828
1161.774405	91584.497133	35.016845
1163.088508	91743.165400	35.021863
1163.700622	91887.222308	35.026880
1165.102206	92038.769722	35.031898
1166.386891	92193.644677	35.036916
1167.014948	92330.333450	35.041933
1168.083036	92489.994935	35.046951
1169.039127	92655.475415	35.051968
1170.325263	92811.322185	35.056986
1171.333066	92982.906890	35.062004
1172.353801	93152.915898	35.067021
1173.846864	93310.036245	35.072039
1174.692210	93480.733466	35.077056
1176.156556	93649.745919	35.082074
1177.535033	93823.485689	35.087092
1178.779295	93990.764624	35.092109
1179.860491	94140.036921	35.097127
1180.801921	94311.737284	35.102144
1182.772011	94481.947041	35.107162
1183.710155	94662.386173	35.112180
1184.665136	94832.848559	35.117197
1186.144781	94990.659698	35.122215
1187.381402	95160.339683	35.127232
1188.973349	95323.132622	35.132250
1190.171754	95488.671457	35.137268
1191.467462	95645.877533	35.142285
1193.103143	95798.988399	35.147303
1194.468438	95961.948510	35.152320
1196.288068	96099.052832	35.157338
1197.407034	96252.185670	35.162356
1198.504740	96392.841592	35.167373
1199.765329	96540.057966	35.172391
1200.886759	96688.265323	35.177408
1202.060949	96835.408785	35.182426
1202.967288	96984.171020	35.187444
1204.042738	97141.239041	35.192461
1205.579426	97289.352665	35.197479
1206.504991	97441.315947	35.202496
1208.246035	97582.876516	35.207514
1208.935496	97744.862416	35.212532
1209.945321	97889.046414	35.217549
1211.797400	98042.530257	35.222567
1213.081340	98196.801383	35.227584
1214.261397	98336.475604	35.232602
1215.392381	98495.872308	35.237620
1216.691872	98647.752526	35.242637
1217.603264	98788.408565	35.247655
1218.331409	98959.558008	35.252672
1219.477712	99117.539393	35.257690
1220.740901	99270.460770	35.262708
1221.635900	99435.380571	35.267725
1222.707550	99600.944122	35.272743
1223.783469	99755.087954	35.277760
1224.951742	99923.333755	35.282778
1226.462033	100070.849495	35.287796
1227.279453	100224.822436	35.292813
1228.836259	100380.159405	35.297831
1229.703914	100544.370164	35.302848
1231.592420	100693.417871	35.307866
1232.641262	100842.125482	35.312884
1233.809204	101004.792187	35.317901
1235.396714	101155.346001	35.322919
1236.424216	101320.909872	35.327936
1237.709762	101466.932655	35.332954
1239.035454	101638.481445	35.337972
1240.048984	101788.618072	35.342989
1241.031095	101954.073427	35.348007
1242.674974	102126.815425	35.353024
1243.809311	102287.129873	35.358042
1245.034963	102449.481084	35.363060
1246.026224	102625.981610	35.368077
1247.378113	102793.383677	35.373095
1248.358863	102959.131087	35.378112
1249.718099	103134.697359	35.383130
1251.060996	103318.892543	35.388148
1252.239102	103485.688035	35.393165
1253.900054	103655.774467	35.398183
1254.604550	103843.853081	35.403200
1256.092968	104009.533490	35.408218
1257.518514	104176.699521	35.413236
1258.418828	104357.600230	35.418253
1260.124830	104541.557364	35.423271
1261.373203	104710.115900	35.428288
1262.890429	104891.909826	35.433306
1264.063441	105068.462967	35.438324
1265.326671	105238.180982	35.443341
1266.745103	105421.880541	35.448359
1267.910743	105592.888624	35.453376
1269.079692	105753.309643	35.458394
1270.493397	105937.406288	35.463412
1271.854534	106109.848906	35.468429
1273.338063	106275.178786	35.473447
1274.756996	106463.854325	35.478464
1275.939578	106624.222044	35.483482
1277.060486	106803.498673	35.488500
1278.364840	106983.804405	35.493517
1279.789553	107131.504472	35.498535
1280.944881	107318.329918	35.503552
1282.476133	107482.350396	35.508570
1284.176740	107643.300769	35.513588
1285.704338	107806.703778	35.518605
1287.166758	107953.940851	35.523623
1288.327453	108116.587808	35.528640
1289.995090	108276.661541	35.533658
1291.059606	108430.357317	35.538676
1292.036380	108594.600049	35.543693
1293.507723	108737.131417	35.548711
1294.599980	108904.142809	35.553728
1295.993938	109032.238120	35.558746
1297.632998	109168.656411	35.563764
1298.332555	109305.604576	35.568781
1300.131638	109436.985940	35.573799
1302.633803	109553.312068	35.578816
1305.136253	109655.605926	35.583834
1306.402071	109769.224309	35.588852
1307.662673	109878.957623	35.593869
1309.114118	109969.880850	35.598887
1310.371952	110091.306525	35.603904
1311.105425	110183.192850	35.608922
1312.364151	110303.296512	35.613940
1313.153750	110415.809914	35.618957
1314.531406	110545.295640	35.623975
1315.386740	110675.067626	35.628992
1316.334052	110808.427399	35.634010
1317.234454	110940.162221	35.639028
1318.283471	111082.274296	35.644045
1319.585483	111212.725048	35.649063
1320.703768	111374.216665	35.654080
1321.482423	111529.496511	35.659098
1322.578267	111678.403100	35.664116
1323.669292	111855.759199	35.669133
1325.133234	112024.359551	35.674151
1325.899648	112203.827052	35.679168
1327.268501	112379.807039	35.684186
1328.763045	112554.939014	35.689204
1329.524810	112739.000620	35.694221
1331.326064	112928.051357	35.699239
1332.083542	113119.257202	35.704256
1333.368950	113308.652354	35.709274
1334.891213	113497.219966	35.714292
1336.059633	113707.280829	35.719309
1337.146664	113900.200165	35.724327
1338.938941	114106.132544	35.729344
1340.172182	114295.119259	35.734362
1341.489396	114499.237445	35.739380
1342.686541	114696.956824	35.744397
1344.667543	114875.034842	35.749415
1346.231079	115070.280484	35.754432
1347.492251	115260.574160	35.759450
1349.030764	115456.491512	35.764468
1350.265886	115655.218972	35.769485
1351.905801	115841.772080	35.774503
1353.671447	116019.379531	35.779520
1355.208379	116207.863720	35.784538
1356.520974	116384.418749	35.789556
1358.018666	116564.649431	35.794573
1359.815642	116736.571325	35.799591
1360.767922	116924.482585	35.804608
1362.483066	117097.356962	35.809626
1363.816941	117267.899774	35.814644
1365.236980	117433.497721	35.819661
1366.535104	117605.409744	35.824679
1367.185715	117776.108834	35.829696
1368.682509	117936.759118	35.834714
1369.943583	118108.908326	35.839732
1370.719322	118280.300016	35.844749
1372.324675	118452.485442	35.849767
1373.418274	118629.122336	35.854784
1374.400259	118819.448786	35.859802
1375.590512	118998.890540	35.864820
1376.842704	119189.582004	35.869837
1377.759342	119388.806817	35.874855
1379.246462	119582.344906	35.879872
1380.424103	119789.674391	35.884890
1381.547603	119988.896235	35.889908
1382.837342	120200.517059	35.894925
1384.356193	120426.908120	35.899943
1385.597857	120638.666765	35.904960
1386.866267	120847.851906	35.909978
1388.949797	121070.637954	35.914996
1390.365398	121273.255313	35.920013
1392.078404	121483.578024	35.925031
1393.620406	121688.749506	35.930048
1395.199580	121895.461842	35.935066
1396.825414	122101.155141	35.940084
1398.098686	122316.835833	35.945101
1399.471441	122520.482787	35.950119
1400.898937	122722.678707	35.955136
1402.038763	122941.615425	35.960154
1403.727614	123145.875549	35.965172
1404.951484	123366.246306	35.970189
1406.142809	123566.294921	35.975207
1408.002375	123783.135572	35.980224
1409.321463	124007.321666	35.985242
1411.000559	124199.773695	35.990260
1412.440441	124420.726770	35.995277
1413.829386	124623.728484	36.000295
1415.483876	124829.298870	36.005312
1416.698019	125051.534317	36.010330
1418.648317	125244.964053	36.015348
1420.065739	125452.818890	36.020365
1421.292058	125669.116641	36.025383
1422.940131	125865.904943	36.030400
1424.350480	126069.002751	36.035418
1425.998717	126276.801874	36.040436
1426.937200	126484.576018	36.045453
1428.678962	126685.700296	36.050471
1430.236455	126884.904513	36.055488
1431.466858	127092.687555	36.060506
1433.704080	127282.184489	36.065524
1435.512576	127466.937040	36.070541
1437.128821	127656.877266	36.075559
1438.777773	127833.372744	36.080576
1439.854844	128017.941179	36.085594
1441.521859	128196.982419	36.090612
1443.414080	128388.796743	36.095629
1444.873045	128547.211227	36.100647
1446.405175	128692.465089	36.105664
1447.199678	128868.558196	36.110682
1448.797382	129023.368149	36.115700
1450.409889	129190.617295	36.120717
1451.432131	129355.148762	36.125735
1452.865010	129510.925108	36.130752
1453.823828	129691.330062	36.135770
1454.948645	129852.288185	36.140788
1456.136411	130042.312822	36.145805
1457.509481	130228.445201	36.150823
1459.534717	130403.871012	36.155840
1460.507231	130602.181339	36.160858
1461.963065	130779.955117	36.165876
1463.396114	130989.166735	36.170893
1464.889673	131161.476358	36.175911
1466.152548	131366.017383	36.180928
1467.463844	131568.144934	36.185946
1468.882011	131765.784478	36.190964
1469.853082	131965.156201	36.195981
1471.361822	132168.092875	36.200999
1473.026455	132370.676804	36.206016
1474.381872	132598.157658	36.211034
1476.070691	132793.404676	36.216052
1477.353905	133021.445199	36.221069
1478.945406	133240.999979	36.226087
1480.568091	133448.184952	36.231104
1481.784388	133673.149658	36.236122
1483.399059	133883.823498	36.241140
1484.834686	134108.186572	36.246157
1486.338470	134325.761570	36.251175
1488.656477	134525.646696	36.256192
1490.299089	134735.194587	36.261210
1491.955972	134938.710197	36.266228
1493.269692	135154.395588	36.271245
1494.923233	135367.392926	36.276263
1496.199398	135574.686218	36.281280
1497.764671	135785.191667	36.286298
1499.269558	135972.088113	36.291316
1500.898894	136188.275898	36.296333
1502.060531	136406.136245	36.301351
1504.036987	136609.891535	36.306368
1505.142462	136820.781608	36.311386
1506.729281	137035.537773	36.316404
1508.216276	137240.376296	36.321421
1509.701130	137459.067480	36.326439
1511.328230	137677.610960	36.331456
1512.465337	137894.827243	36.336474
1514.659423	138112.041945	36.341492
1515.963837	138321.669203	36.346509
1517.048929	138540.583947	36.351527
1518.516784	138755.941765	36.356544
1520.288132	138959.023467	36.361562
1522.276867	139168.269161	36.366580
1524.121095	139384.877053	36.371597
1525.258355	139588.355244	36.376615
1526.661262	139788.358133	36.381632
1528.164522	139982.618014	36.386650
1529.380878	140155.329051	36.391668
1530.834095	140351.386227	36.396685
1532.359286	140559.181744	36.401703
1534.461139	140742.997037	36.406720
1536.054206	140929.568452	36.411738
1537.682595	141109.963208	36.416756
1539.145956	141313.832139	36.421773
1541.027154	141492.237212	36.426791
1543.010985	141670.817141	36.431808
1544.172415	141873.432347	36.436826
1545.686415	142052.989018	36.441844
1547.118566	142239.543330	36.446861
1548.056856	142449.726383	36.451879
1549.760834	142655.910832	36.456896
1551.042484	142848.931432	36.461914
1552.529377	143055.368513	36.466932
1553.829829	143287.186209	36.471949
1554.942946	143498.413334	36.476967
1556.680623	143719.682683	36.481984
1558.011834	143942.323711	36.487002
1559.613401	144157.571793	36.492020
1561.155328	144392.857751	36.497037
1562.576143	144623.639622	36.502055
1564.392231	144840.214613	36.507072
1565.616355	145088.878198	36.512090
1567.649132	145319.669408	36.517108
1569.227722	145541.281179	36.522125
1570.240873	145797.094973	36.527143
1572.019931	146015.775479	36.532160
1573.252271	146267.679444	36.537178
1575.399394	146494.163936	36.542196
1576.938075	146735.298979	36.547213
1578.631340	146980.746597	36.552231
1580.249975	147209.779351	36.557248
1582.103526	147445.964009	36.562266
1583.476507	147685.459279	36.567284
1585.545266	147913.867825	36.572301
1586.954401	148149.709946	36.577319
1589.013118	148369.135509	36.582336
1590.410898	148619.130256	36.587354
1591.864194	148842.331526	36.592372
1593.548808	149083.765349	36.597389
1595.114662	149313.353952	36.602407
1597.067094	149541.437571	36.607424
1598.873057	149767.276803	36.612442
1600.544728	149985.494409	36.617460
1602.254227	150218.679688	36.622477
1603.771937	150443.529836	36.627495
1605.459828	150654.713243	36.632512
1607.085044	150887.396896	36.637530
1608.467381	151101.319414	36.642548
1610.495534	151317.143880	36.647565
1611.932785	151542.597534	36.652583
1613.206732	151750.164408	36.657600
1614.412143	151965.046144	36.662618
1615.929111	152191.252262	36.667636
1617.170641	152393.807701	36.672653
1618.779768	152601.275963	36.677671
1620.282547	152821.035273	36.682688
1621.658626	153058.997361	36.687706
1623.182397	153301.197753	36.692724
1625.087341	153514.697846	36.697741
1626.539838	153754.072774	36.702759
1627.645391	153992.756447	36.707776
1629.012360	154234.062909	36.712794
1630.516235	154487.863730	36.717812
1632.448729	154719.599803	36.722829
1633.573019	154983.557348	36.727847
1635.522866	155225.830707	36.732864
1637.633333	155475.852865	36.737882
1639.226905	155719.137287	36.742900
1640.858064	155968.427680	36.747917
1642.482857	156236.119371	36.752935
1644.675330	156479.199970	36.757952
1646.226954	156733.225498	36.762970
1648.139585	156983.594411	36.767988
1649.595934	157238.120636	36.773005
1651.190268	157489.837151	36.778023
1653.058010	157730.454759	36.783040
1654.652286	157995.413299	36.788058
1655.916684	158262.379055	36.793076
1657.765162	158514.848829	36.798093
1659.210478	158780.039874	36.803111
1660.895342	159044.953948	36.808128
1662.541251	159302.876306	36.813146
1664.338914	159558.341691	36.818164
1666.293521	159805.363715	36.823181
1668.522493	160077.909296	36.828199
1670.624648	160304.621377	36.833216
1672.587606	160557.835817	36.838234
1674.199350	160807.316060	36.843252
1676.086919	161046.469469	36.848269
1677.666842	161291.887358	36.853287
1679.020879	161541.198058	36.858304
1680.657452	161784.974377	36.863322
1681.784281	162041.439147	36.868340
1683.495976	162294.223850	36.873357
1684.948774	162549.803454	36.878375
1687.104174	162799.097054	36.883392
1689.051330	163049.858536	36.888410
1690.854120	163305.628849	36.893428
1693.038897	163547.338847	36.898445
1694.629600	163787.356537	36.903463
1696.148141	164021.439100	36.908480
1698.099351	164261.288505	36.913498
1699.507828	164521.962044	36.918516
1701.678615	164747.701835	36.923533
1702.869522	164999.015270	36.928551
1704.383984	165230.709077	36.933568
1705.609906	165456.438342	36.938586
1706.838800	165697.629336	36.943604
1708.623616	165933.038820	36.948621
1709.992856	166181.046948	36.953639
1711.298402	166423.980765	36.958656
1713.117479	166683.627624	36.963674
1714.761290	166942.073793	36.968692
1716.875585	167191.479642	36.973709
1718.898667	167444.491136	36.978727
1720.997788	167668.370058	36.983744
1722.628979	167923.032455	36.988762
1724.171190	168180.387017	36.993780
1726.053186	168420.426267	36.998797
1727.371255	168685.798138	37.003815
1729.271824	168933.930188	37.008832
1731.359503	169188.503166	37.013850
1732.949857	169441.038485	37.018868
1734.687823	169688.782630	37.023885
1736.346593	169963.039124	37.028903
1737.898517	170226.519823	37.033920
1739.781643	170488.858828	37.038938
1740.954405	170768.880958	37.043956
1742.580413	171040.537149	37.048973
1744.037684	171317.245300	37.053991
1745.550358	171607.304078	37.059008
1747.633638	171887.671657	37.064026
1748.945678	172176.891189	37.069044
1750.581175	172466.137587	37.074061
1752.460756	172754.104156	37.079079
1754.443812	173044.961383	37.084096
1756.234586	173331.017997	37.089114
1757.900422	173638.053441	37.094132
1759.813174	173930.184145	37.099149
1761.624392	174235.272801	37.104167
1763.288648	174523.616076	37.109184
1765.303010	174824.059178	37.114202
1767.172936	175130.122075	37.119220
1768.885859	175420.303485	37.124237
1770.749314	175719.419691	37.129255
1772.707102	176017.838026	37.134272
1775.307636	176281.027185	37.139290
1777.350175	176554.671654	37.144308
1779.651006	176823.062652	37.149325
1781.774110	177097.611365	37.154343
1783.879548	177357.194077	37.159360
1785.992448	177616.751845	37.164378
1788.032102	177864.473086	37.169396
1790.450084	178096.619302	37.174413
1792.555698	178333.079307	37.179431
1794.117321	178572.367458	37.184448
1795.851934	178815.917842	37.189466
1797.424999	179054.775531	37.194484
1799.023813	179297.690489	37.199501
1800.639161	179530.555616	37.204519
1801.885670	179762.782742	37.209536
1803.388800	179982.967779	37.214554
1804.594917	180229.655189	37.219572
1806.252778	180461.224464	37.224589
1807.834321	180701.790170	37.229607
1809.004631	180965.996854	37.234624
1810.536124	181213.209186	37.239642
1812.141794	181494.034834	37.244660
1813.695315	181770.315477	37.249677
1815.201452	182061.653769	37.254695
1816.723014	182339.630624	37.259712
1818.512903	182637.792132	37.264730
1819.854854	182947.789092	37.269748
1821.435060	183253.042894	37.274765
1822.856522	183556.166894	37.279783
1824.850126	183878.336947	37.284800
1826.411409	184183.041800	37.289818
1828.160418	184519.035487	37.294836
1829.958106	184851.813595	37.299853
1831.892813	185176.679694	37.304871
1833.552697	185514.940911	37.309888
1835.964343	185841.017668	37.314906
1838.319112	186161.623909	37.319924
1840.563701	186482.643255	37.324941
1843.034838	186790.545814	37.329959
1845.520518	187103.942785	37.334976
1847.863884	187393.431405	37.339994
1849.606161	187693.930570	37.345012
1851.579403	187994.585356	37.350029
1853.272165	188289.068444	37.355047
1855.044786	188592.385746	37.360064
1856.850006	188885.040010	37.365082
1858.323824	189208.091262	37.370100
1860.102627	189510.893152	37.375117
1862.138852	189816.854109	37.380135
1863.632218	190139.096360	37.385152
1865.639227	190447.604089	37.390170
1867.184407	190778.154770	37.395188
1869.187536	191096.375674	37.400205
1870.997316	191409.908326	37.405223
1872.931297	191723.778626	37.410240
1874.870914	192047.879048	37.415258
1876.826758	192373.654261	37.420276
1879.086403	192684.179296	37.425293
1880.856454	193006.954957	37.430311
1882.493218	193322.633986	37.435328
1884.625908	193652.158856	37.440346
1886.424157	193972.283750	37.445364
1888.052665	194285.609510	37.450381
1889.625732	194612.437313	37.455399
1891.433511	194951.947159	37.460416
1893.694285	195269.290785	37.465434
1895.199324	195626.901029	37.470452
1897.321065	195935.906827	37.475469
1899.530107	196274.371753	37.480487
1901.396036	196579.690504	37.485504
1903.282153	196873.191324	37.490522
1905.276442	197173.263957	37.495540
1907.259547	197467.856953	37.500557
1909.146917	197766.464925	37.505575
1910.891679	198063.942191	37.510592
1913.093027	198354.507332	37.515610
1914.935237	198661.745808	37.520628
1916.776177	198974.698003	37.525645
1918.641244	199272.987940	37.530663
1920.643233	199581.754849	37.535680
1922.706396	199900.274727	37.540698
1924.100805	200205.689106	37.545716
1925.982674	200519.278378	37.550733
1928.031034	200826.026765	37.555751
1930.225985	201149.229486	37.560768
1932.376565	201446.064332	37.565786
1934.338271	201776.250990	37.570804
1936.699910	202080.595627	37.575821
1938.600388	202387.515732	37.580839
1940.379493	202710.412680	37.585856
1942.273857	203024.813779	37.590874
1944.146300	203341.251103	37.595892
1946.160551	203650.812998	37.600909
1948.118207	203973.739554	37.605927
1950.213596	204289.105833	37.610944
1952.365352	204609.047446	37.615962
1953.818532	204930.866157	37.620980
1956.252798	205247.516753	37.625997
1957.950043	205571.191694	37.631015
1960.010265	205899.507724	37.636032
1962.135718	206211.477518	37.641050
1964.267843	206529.008073	37.646068
1966.152152	206854.843788	37.651085
1968.281635	207178.357338	37.656103
1970.358940	207491.674381	37.661120
1972.405315	207813.808106	37.666138
1973.939438	208142.029465	37.671156
1976.099934	208466.230476	37.676173
1978.108081	208779.603192	37.681191
1980.462214	209110.340158	37.686208
1982.664671	209421.108203	37.691226
1984.359157	209743.917220	37.696244
1986.530013	210067.693322	37.701261
1988.613304	210379.284825	37.706279
1989.815378	210715.583157	37.711296
1992.170725	211022.335814	37.716314
1994.270615	211356.400331	37.721332
1996.023630	211683.234385	37.726349
1998.149063	212004.310683	37.731367
1999.601219	212344.792790	37.736384
2001.516829	212663.404583	37.741402
2003.200172	213007.255906	37.746420
2004.911064	213356.259164	37.751437
2007.314792	213702.602453	37.756455
2008.686716	214026.131514	37.761472
2011.150781	214338.646440	37.766490
2013.014473	214662.481419	37.771508
2014.812615	214989.464296	37.776525
2016.924400	215304.858116	37.781543
2018.656892	215649.553096	37.786560
2020.750049	215970.780520	37.791578
2022.721209	216289.464115	37.796596
2024.800010	216620.054065	37.801613
2027.103133	216951.346383	37.806631
2028.524683	217295.641756	37.811648
2030.771124	217626.070164	37.816666
2032.886442	217978.397320	37.821684
2034.514226	218327.756328	37.826701
2036.720175	218686.586011	37.831719
2038.402798	219031.673577	37.836736
2040.367909	219393.706471	37.841754
2042.383347	219757.650410	37.846772
2044.646446	220111.348399	37.851789
2046.596538	220530.665738	37.856807
2048.657309	220914.199815	37.861824
2051.026857	221273.650920	37.866842
2053.615050	221639.366909	37.871860
2055.783981	221999.196079	37.876877
2057.984744	222343.353228	37.881895
2059.776050	222711.727503	37.886912
2061.807525	223069.996243	37.891930
2064.334719	223430.981449	37.896948
2066.529788	223794.001819	37.901965
2069.289469	224133.519655	37.906983
2070.921743	224494.346880	37.912000
2073.684289	224844.673068	37.917018
2075.556197	225196.919748	37.922036
2077.288964	225554.383469	37.927053
2079.603476	225903.058317	37.932071
2081.607072	226259.072627	37.937088
2083.755126	226616.919454	37.942106
2085.731977	226975.429858	37.947124
2087.309378	227339.109814	37.952141
2089.514906	227695.047312	37.957159
2091.371139	228070.800271	37.962176
2093.613280	228427.014320	37.967194
2095.954481	228794.490303	37.972212
2098.190827	229163.990801	37.977229
2100.326119	229519.743645	37.982247
2102.247309	229888.611394	37.987264
2104.325867	230257.912830	37.992282
2106.500028	230619.962339	37.997300
2108.904862	230988.935585	38.002317
2111.057324	231343.346721	38.007335
2112.727993	231712.540862	38.012352
2115.098461	232076.876061	38.017370
2117.302104	232433.314979	38.022388
2119.467574	232805.761981	38.027405
2121.913304	233151.929774	38.032423
2123.525311	233502.066146	38.037440
2125.807405	233839.296771	38.042458
2127.910602	234173.763100	38.047476
2130.013760	234510.846582	38.052493
2131.938396	234844.581504	38.057511
2133.528963	235204.277032	38.062528
2135.234912	235560.526695	38.067546
2137.195580	235905.460140	38.072564
2138.736842	236277.434784	38.077581
2141.107370	236646.205939	38.082599
2142.995256	237025.265311	38.087616
2144.891638	237401.505365	38.092634
2147.141155	237779.951235	38.097652
2149.099032	238175.690757	38.102669
2151.092574	238554.967246	38.107687
2153.541790	238960.613558	38.112704
2155.875408	239355.103856	38.117722
2158.148958	239744.982301	38.122740
2160.010898	240148.135174	38.127757
2162.244003	240549.376376	38.132775
2164.515782	240953.381382	38.137792
2166.831233	241347.576431	38.142810
2169.500026	241748.777927	38.147828
2171.964371	242141.453310	38.152845
2174.504513	242523.195822	38.157863
2176.539105	242917.237193	38.162880
2179.250000	243312.518740	38.167898
2181.687899	243696.770201	38.172916
2183.430733	244098.913364	38.177933
2186.286839	244466.463416	38.182951
2188.289622	244860.210855	38.187968
2190.872682	245229.990736	38.192986
2193.277432	245605.388056	38.198004
2195.660489	245984.320543	38.203021
2198.021420	246358.685387	38.208039
2200.366652	246733.129900	38.213056
2202.590121	247110.693614	38.218074
2205.237645	247476.481137	38.223092
2206.939419	247848.769822	38.228109
2209.099382	248216.998770	38.233127
2211.316536	248582.476192	38.238144
2213.220421	248958.393300	38.243162
2215.386703	249344.125442	38.248180
2217.449290	249721.213052	38.253197
2219.789078	250102.601240	38.258215
2221.321047	250501.594699	38.263232
2223.260863	250885.893080	38.268250
2226.125597	251270.553696	38.273268
2227.600140	251670.956083	38.278285
2230.125851	252069.439970	38.283303
2232.074405	252468.879922	38.288320
2234.525283	252872.000580	38.293338
2236.674709	253278.853199	38.298356
2238.837148	253683.570854	38.303373
2241.007902	254064.486276	38.308391
2242.618234	254462.840958	38.313408
2245.207718	254855.300278	38.318426
2247.270731	255236.285809	38.323444
2248.616122	255630.010755	38.328461
2250.954770	256010.293519	38.333479
2253.217938	256406.744826	38.338496
2254.921202	256809.763233	38.343514
2257.461150	257215.088330	38.348532
2259.216849	257637.024709	38.353549
2261.705080	258050.742274	38.358567
2263.683088	258478.335047	38.363584
2266.143397	258902.575140	38.368602
2268.331744	259327.697340	38.373620
2270.116023	259766.677967	38.378637
2272.558802	260209.543130	38.383655
2274.939716	260647.312838	38.388672
2277.173625	261086.910118	38.393690
2279.735430	261530.571325	38.398708
2281.978163	261978.221209	38.403725
2284.430766	262404.068122	38.408743
2286.835583	262868.586495	38.413760
2288.759265	263315.907728	38.418778
2291.464292	263758.939547	38.423796
2293.838679	264217.189950	38.428813
2296.391475	264668.782402	38.433831
2298.908232	265119.339544	38.438848
2301.102252	265569.973735	38.443866
2303.445674	266017.206074	38.448884
2305.822057	266469.666676	38.453901
2308.629373	266910.450102	38.458919
2310.763786	267356.497440	38.463936
2312.845206	267810.885812	38.468954
2315.515967	268257.814153	38.473972
2317.655068	268718.240042	38.478989
2320.239810	269165.411274	38.484007
2322.817571	269622.618205	38.489024
2324.884800	270075.663973	38.494042
2326.999158	270524.993615	38.499060
2329.733311	270988.451103	38.504077
2332.089152	271435.888419	38.509095
2334.581421	271888.994632	38.514112
2336.756470	272340.576265	38.519130
2340.554359	272764.033230	38.524148
2343.758967	273187.177878	38.529165
2346.288337	273598.210593	38.534183
2349.492868	274020.440853	38.539200
2351.622392	274423.026888	38.544218
2353.978066	274815.618949	38.549236
2356.222552	275224.537626	38.554253
2358.389653	275629.251585	38.559271
2360.419308	276048.721275	38.564288
2362.485667	276449.589797	38.569306
2365.193991	276846.901631	38.574324
2367.539639	277260.097191	38.579341
2369.909243	277664.626293	38.584359
2371.883665	278057.202119	38.589376
2373.669994	278438.503133	38.594394
2375.954228	278816.575077	38.599412
2377.863872	279219.118879	38.604429
2380.126447	279606.948834	38.609447
2382.400916	280003.134421	38.614464
2384.599071	280421.661419	38.619482
2386.609749	280827.338416	38.624500
2388.527480	281242.327502	38.629517
2390.636612	281665.592847	38.634535
2393.101636	282097.286166	38.639552
2395.313604	282542.178130	38.644570
2397.927502	282962.110872	38.649588
2400.217181	283412.832499	38.654605
2402.390137	283861.895588	38.659623
2404.778033	284302.414111	38.664640
2406.901603	284763.144140	38.669658
2409.700936	285217.060134	38.674676
2412.288184	285672.203158	38.679693
2414.778815	286125.303298	38.684711
2417.547687	286586.792558	38.689728
2419.713492	287044.667950	38.694746
2422.464483	287492.060177	38.699764
2425.037758	287956.880915	38.704781
2427.519556	288421.258202	38.709799
2430.159491	288872.984516	38.714816
2432.679813	289334.305921	38.719834
2435.275897	289783.700688	38.724852
2437.385052	290243.917210	38.729869
2439.565824	290711.005689	38.734887
2442.334813	291181.327833	38.739904
2444.534683	291653.466653	38.744922
2446.815188	292125.718784	38.749940
2449.239579	292616.338518	38.754957
2451.361207	293095.650321	38.759975
2454.025827	293571.572742	38.764992
2456.126374	294066.660603	38.770010
2458.333422	294543.364641	38.775028
2460.936055	295050.131820	38.780045
2463.244485	295552.651396	38.785063
2465.765037	296049.166600	38.790080
2468.098520	296548.351964	38.795098
2471.001197	297055.345781	38.800116
2473.234910	297566.051258	38.805133
2475.808388	298066.083516	38.810151
2478.346660	298572.521142	38.815168
2480.858339	299090.493800	38.820186
2483.565384	299591.541907	38.825204
2485.853870	300096.744441	38.830221
2488.287541	300607.129659	38.835239
2490.972934	301116.787505	38.840256
2493.472616	301619.487782	38.845274
2496.603743	302109.843016	38.850292
2499.445174	302610.352143	38.855309
2502.242472	303094.432163	38.860327
2505.135657	303541.181542	38.865344
2507.219840	303997.252775	38.870362
2510.002684	304437.031587	38.875380
2512.551355	304884.923486	38.880397
2515.269183	305336.851183	38.885415
2517.966035	305773.616625	38.890432
2520.389087	306218.933112	38.895450
2522.734908	306658.418251	38.900468
2525.214515	307112.892176	38.905485
2527.460873	307557.088995	38.910503
2529.880054	308011.696235	38.915520
2531.834658	308492.283272	38.920538
2534.238265	308944.908308	38.925556
2537.062172	309403.687959	38.930573
2539.999599	309866.816564	38.935591
2542.389320	310330.690489	38.940608
2544.478799	310821.762032	38.945626
2547.173737	311298.791328	38.950644
2549.811686	311781.339230	38.955661
2551.745260	312271.717923	38.960679
2554.529193	312754.670192	38.965696
2556.877124	313250.312572	38.970714
2559.254022	313746.049640	38.975732
2561.974899	314245.133271	38.980749
2564.551213	314761.965503	38.985767
2566.804939	315267.645572	38.990784
2569.287434	315785.630373	38.995802
2572.309799	316296.288506	39.000820
2574.489119	316810.785638	39.005837
2576.809166	317344.890225	39.010855
2579.719790	317860.129428	39.015872
2582.315061	318380.825452	39.020890
2584.818372	318909.177747	39.025908
2587.613317	319438.725285	39.030925
2589.909624	319971.548774	39.035943
2592.488547	320506.686258	39.040960
2594.944988	321053.674818	39.045978
2597.452483	321589.274225	39.050996
2600.296542	322130.201067	39.056013
2602.400728	322692.193637	39.061031
2605.237912	323240.581054	39.066048
2607.899406	323790.440298	39.071066
2610.631192	324334.926267	39.076084
2613.107355	324890.267650	39.081101
2615.697601	325442.285768	39.086119
2618.297644	326004.024927	39.091136
2620.843221	326566.784553	39.096154
2623.540176	327130.608158	39.101172
2626.183593	327700.327732	39.106189
2628.329376	328276.597517	39.111207
2631.055506	328830.373238	39.116224
2633.955096	329408.902082	39.121242
2636.384605	329979.197090	39.126260
2639.140510	330553.422811	39.131277
2641.722905	331103.776195	39.136295
2644.840670	331647.793835	39.141312
2647.238217	332190.905699	39.146330
2650.096692	332721.218533	39.151348
2652.817259	333250.914395	39.156365
2655.123265	333789.838614	39.161383
2658.258703	334321.415824	39.166400
2660.312258	334846.863005	39.171418
2663.096487	335385.927450	39.176436
2666.357403	335913.536561	39.181453
2669.323976	336449.643511	39.186471
2672.284958	336976.123672	39.191488
2674.701042	337522.135534	39.196506
2677.470077	338050.821067	39.201524
2680.159651	338584.466040	39.206541
2682.728054	339124.727284	39.211559
2685.679946	339662.968131	39.216576
2687.895292	340203.352227	39.221594
2690.615182	340740.401827	39.226612
2693.662343	341285.925847	39.231629
2696.340048	341826.806484	39.236647
2698.961902	342370.763246	39.241664
2701.641995	342938.977717	39.246682
2703.848821	343492.104682	39.251700
2706.792600	344052.218552	39.256717
2708.861783	344620.615219	39.261735
2711.947930	345195.700051	39.266752
2714.507766	345759.412657	39.271770
2717.297157	346334.025376	39.276788
2720.004161	346919.257200	39.281805
2722.154943	347514.497342	39.286823
2725.374300	348090.521935	39.291840
2727.472842	348697.232514	39.296858
2730.253458	349291.262274	39.301876
2733.356124	349891.784132	39.306893
2735.550023	350508.766168	39.311911
2738.728587	351096.265218	39.316928
2741.184960	351704.560934	39.321946
2743.890377	352323.192568	39.326964
2747.000987	352936.092038	39.331981
2749.453656	353549.012337	39.336999
2752.256779	354159.991480	39.342016
2754.953924	354787.149413	39.347034
2757.357590	355406.096565	39.352052
2760.203885	356029.230369	39.357069
2762.810157	356677.497763	39.362087
2765.577654	357300.222068	39.367104
2768.557957	357933.615979	39.372122
2771.505958	358574.595901	39.377140
2774.255142	359210.928710	39.382157
2776.820164	359849.921899	39.387175
2779.627789	360475.188038	39.392192
2782.662754	361125.587119	39.397210
2785.301453	361768.857480	39.402228
2788.639830	362409.698688	39.407245
2790.828948	363033.049135	39.412263
2793.698745	363640.040946	39.417280
2796.435941	364239.406789	39.422298
2799.800003	364841.177928	39.427316
2803.111948	365407.674130	39.432333
2805.634525	366014.536893	39.437351
2808.696443	366595.573579	39.442368
2811.193998	367196.536682	39.447386
2814.102577	367778.825559	39.452404
2816.868406	368368.209236	39.457421
2819.512955	368985.568248	39.462439
2822.019755	369595.505254	39.467456
2824.712288	370186.855023	39.472474
2827.258303	370818.007331	39.477492
2830.069803	371431.067073	39.482509
2832.515431	372066.149655	39.487527
2835.056524	372694.965593	39.492544
2838.006868	373331.166944	39.497562
2841.025064	373969.656678	39.502580
2844.195843	374600.881196	39.507597
2847.209270	375246.836605	39.512615
2850.048098	375891.515407	39.517632
2853.102856	376531.659006	39.522650
2855.683175	377189.119585	39.527668
2858.562048	377840.712220	39.532685
2861.576654	378496.128846	39.537703
2864.778143	379142.016751	39.542720
2867.896571	379787.501202	39.547738
2870.705174	380443.526568	39.552756
2874.115284	381095.640311	39.557773
2876.682502	381751.656171	39.562791
2879.637337	382397.097281	39.567808
2882.726509	383051.029391	39.572826
2885.264492	383706.356429	39.577844
2887.917631	384362.744482	39.582861
2890.832010	385021.489308	39.587879
2893.827254	385676.683827	39.592896
2897.113602	386340.596736	39.597914
2899.908643	387017.612517	39.602932
2903.472509	387675.141446	39.607949
2906.373138	388329.516859	39.612967
2909.348805	388984.781503	39.617984
2912.265007	389639.054373	39.623002
2915.210785	390296.429983	39.628020
2918.313657	390946.743352	39.633037
2920.972970	391616.313053	39.638055
2923.886109	392263.715417	39.643072
2926.974715	392943.538621	39.648090
2929.572344	393604.964441	39.653108
2932.213760	394262.414553	39.658125
2935.197401	394933.643516	39.663143
2938.125160	395609.762092	39.668160
2941.113533	396275.308798	39.673178
2943.248910	396968.210606	39.678196
2946.490080	397642.260673	39.683213
2949.386377	398316.148744	39.688231
2952.125533	398961.472385	39.693248
2954.767631	399623.710367	39.698266
2957.421449	400271.430335	39.703284
2960.590206	400911.069390	39.708301
2963.403443	401565.989375	39.713319
2966.599511	402225.525666	39.718336
2969.969058	402860.200955	39.723354
2972.871970	403524.320124	39.728372
2976.298777	404166.895248	39.733389
2979.399751	404816.226735	39.738407
2982.653651	405446.051559	39.743424
2985.988953	406093.012492	39.748442
2988.794528	406743.465865	39.753460
2992.343521	407384.104671	39.758477
2995.732746	408025.921375	39.763495
2998.589659	408654.323894	39.768512
3001.290880	409300.328887	39.773530
3003.899357	409954.775120	39.778548
3006.807880	410613.544466	39.783565
3010.031137	411267.003001	39.788583
3013.020545	411926.820394	39.793600
3016.141891	412580.722341	39.798618
3018.974045	413253.055054	39.803636
3022.026025	413915.352387	39.808653
3024.940030	414576.566796	39.813671
3028.275967	415252.042925	39.818688
3031.181765	415922.148282	39.823706
3033.773025	416604.958175	39.828724
3036.498266	417295.129902	39.833741
3039.246924	417980.770769	39.838759
3042.075479	418683.334135	39.843776
3045.261385	419380.983852	39.848794
3047.880415	420101.535122	39.853812
3050.994405	420815.832608	39.858829
3054.137012	421531.602050	39.863847
3056.805839	422248.796054	39.868864
3060.308974	422990.920987	39.873882
3062.620573	423716.873718	39.878900
3065.641252	424461.695122	39.883917
3068.330800	425210.247057	39.888935
3071.279750	425963.220974	39.893952
3074.737285	426726.605857	39.898970
3077.386110	427483.029584	39.903988
3080.708613	428253.535329	39.909005
3083.995420	429020.959416	39.914023
3086.890612	429789.866790	39.919040
3090.135078	430564.395061	39.924058
3093.326823	431333.286028	39.929076
3096.212823	432120.260172	39.934093
3098.651284	432902.671853	39.939111
3101.942031	433691.357304	39.944128
3105.557082	434471.306285	39.949146
3108.341892	435268.455770	39.954164
3111.582878	436049.175021	39.959181
3114.570993	436837.101349	39.964199
3117.561500	437588.135428	39.969216
3120.509017	438345.838137	39.974234
3123.560160	439089.651650	39.979252
3126.325158	439837.488319	39.984269
3129.534883	440593.890514	39.989287
3132.392181	441367.793717	39.994304
3136.005894	442123.476935	39.999322
3138.805888	442894.353213	40.004340
3141.943691	443667.632215	40.009357
3145.525728	444437.727743	40.014375
3148.904850	445217.398785	40.019392
3152.116766	445987.806492	40.024410
3155.029993	446774.233031	40.029428
3158.347602	447553.634301	40.034445
3161.452417	448342.407826	40.039463
3164.337212	449125.014175	40.044480
3167.770027	449917.428116	40.049498
3170.864799	450706.679690	40.054516
3173.871599	451503.307470	40.059533
3177.053265	452306.104952	40.064551
3180.090867	453116.184576	40.069568
3183.293869	453922.211193	40.074586
3186.877835	454749.908880	40.079604
3190.098613	455551.977820	40.084621
3193.253648	456375.635121	40.089639
3196.368781	457207.566564	40.094656
3199.295456	458027.656817	40.099674
3202.172167	458869.986521	40.104692
3205.561739	459701.881739	40.109709
3208.820471	460538.015702	40.114727
3212.552108	461373.890986	40.119744
3215.548952	462223.205387	40.124762
3218.523512	463081.190609	40.129780
3221.777911	463932.015580	40.134797
3225.041687	464796.512813	40.139815
3227.922931	465665.132356	40.144832
3231.119208	466524.360194	40.149850
3234.250353	467396.662332	40.154868
3237.377077	468272.013872	40.159885
3240.741483	469151.185109	40.164903
3243.616653	470046.022342	40.169920
3246.849265	470920.234237	40.174938
3249.846884	471824.633265	40.179956
3253.222792	472720.994280	40.184973
3256.570017	473609.888111	40.189991
3259.586557	474527.006646	40.195008
3263.471487	475401.125635	40.200026
3267.022217	476313.225128	40.205044
3270.161147	477213.721459	40.210061
3273.702928	478102.487190	40.215079
3277.229981	478998.595256	40.220096
3281.119637	479874.640351	40.225114
3283.970365	480777.193662	40.230132
3287.284492	481665.885321	40.235149
3291.356431	482516.665180	40.240167
3294.453593	483368.875812	40.245184
3298.075806	484192.414677	40.250202
3301.104650	485012.474982	40.255220
3304.671418	485835.800601	40.260237
3308.133447	486643.241938	40.265255
3311.263004	487475.761720	40.270272
3314.330903	488291.430783	40.275290
3317.456749	489120.998982	40.280308
3320.395453	489958.541988	40.285325
3323.613780	490792.719824	40.290343
3326.396999	491644.002635	40.295360
3330.126345	492494.743280	40.300378
3333.216617	493356.152654	40.305396
3335.994481	494232.318967	40.310413
3339.028474	495104.160657	40.315431
3342.185742	495989.374631	40.320448
3345.297262	496870.209901	40.325466
3349.065240	497761.149359	40.330484
3352.018668	498666.614877	40.335501
3355.473346	499566.855941	40.340519
3358.888534	500477.862583	40.345536
3362.108868	501381.331061	40.350554
3365.508289	502308.957375	40.355572
3368.917350	503237.593612	40.360589
3372.482154	504162.673269	40.365607
3375.590341	505100.950434	40.370624
3378.884418	506033.848168	40.375642
3382.333327	506988.878217	40.380660
3385.345345	507922.425617	40.385677
3388.786749	508898.598050	40.390695
3391.596853	509875.117569	40.395712
3394.924495	510827.632550	40.400730
3398.349553	511800.614404	40.405748
3401.651567	512793.841964	40.410765
3404.899774	513777.837718	40.415783
3408.127737	514781.604747	40.420800
3411.957905	515769.578780	40.425818
3415.415964	516781.108988	40.430836
3418.808040	517789.864339	40.435853
3422.244441	518778.024163	40.440871
3425.424852	519807.569548	40.445888
3428.944858	520822.170598	40.450906
3432.213659	521836.798688	40.455924
3435.838244	522849.239870	40.460941
3440.029474	523853.259393	40.465959
3443.380547	524885.178710	40.470976
3447.206378	525883.734667	40.475994
3450.364208	526889.542354	40.481012
3454.068031	527918.588683	40.486029
3458.101413	528916.467810	40.491047
3461.402678	529921.102717	40.496064
3465.236017	530928.461908	40.501082
3469.254383	531922.523933	40.506100
3472.328209	532916.974180	40.511117
3475.927366	533903.556766	40.516122
3479.301970	534836.983071	40.521127
3482.466373	535705.278834	40.526132
3485.618173	536549.738613	40.531136
3488.476341	537295.209265	40.536141
3491.678174	537977.663239	40.541146
3494.038053	538629.667014	40.546151
3496.733752	539203.923394	40.551156
3499.059188	539708.127256	40.556160
3501.368663	540191.613844	40.561165
3503.851546	540557.154838	40.566170
3505.431582	540925.758211	40.571175
3507.590472	541171.717992	40.576180
3508.902962	541445.375545	40.581184
3510.855493	541597.750590	40.586189
3512.233663	541773.844082	40.591194
3513.512732	541877.145606	40.596199
3514.228181	541956.502675	40.601204
3515.334751	541957.287098	40.606208
3516.353651	541992.417953	40.611213
3517.500977	541958.711893	40.616218
3518.130633	541894.440562	40.621223
3518.660806	541827.609710	40.626228
3519.332098	541716.729086	40.631232
3519.744316	541608.817027	40.636237
3520.264231	541447.316469	40.641242
3520.412259	541305.463598	40.646247
3520.965575	541125.979386	40.651252
3521.440586	540935.599017	40.656256
3521.465691	540738.016318	40.661261
3521.635637	540527.481695	40.666266
3521.900030	540298.953101	40.671271
3522.063739	540080.132087	40.676276
3522.301771	539834.533163	40.681280
3522.436662	539592.228860	40.686285
3522.510560	539328.317210	40.691290
3522.306000	539078.685631	40.696295
3522.423327	538827.837581	40.701300
3521.883376	538553.960035	40.706304
3522.143419	538275.961508	40.711309
3522.012594	538007.413110	40.716314
3522.290138	537748.189037	40.721319
3522.172133	537461.801355	40.726324
3521.607431	537171.589999	40.731328
3521.332560	536904.661108	40.736333
3521.407593	536640.298617	40.741338
3521.353524	536356.809520	40.746343
3520.873072	536098.586400	40.751348
3521.274734	535821.379470	40.756352
3520.473619	535549.863262	40.761357
3520.411001	535265.395658	40.766362
3520.372423	535010.064580	40.771367
3519.949871	534741.403985	40.776372
3519.767813	534474.165607	40.781376
3519.526096	534222.894717	40.786381
3519.714275	533941.343430	40.791386
3519.195810	533697.028383	40.796391
3518.930959	533446.607321	40.801396
3518.854980	533193.474901	40.806400
3518.785820	532944.580870	40.811405
3518.809171	532682.836202	40.816410
3518.358722	532448.544186	40.821415
3518.063595	532198.714036	40.826420
3518.359681	531954.141797	40.831424
3517.685258	531719.065851	40.836429
3517.935751	531478.333105	40.841434
3517.610258	531236.828763	40.846439
3517.202429	530999.729403	40.851444
3517.397318	530774.202708	40.856448
3517.103129	530530.560431	40.861453
3516.830847	530301.867059	40.866458
3516.419744	530103.307106	40.871463
3516.502991	529862.929675	40.876468
3516.266403	529659.334168	40.881472
3516.021920	529439.517061	40.886477
3515.963731	529206.630442	40.891482
3515.413902	529029.200819	40.896487
3515.498896	528800.429167	40.901492
3515.101425	528606.244498	40.906496
3514.859426	528415.923958	40.911501
3514.970497	528200.530893	40.916506
3514.249176	528014.071341	40.921511
3514.172918	527836.755629	40.926516
3514.213236	527629.754865	40.931520
3513.820999	527463.754462	40.936525
3513.892870	527285.903820	40.941530
3514.097087	527106.413066	40.946535
3513.633384	526918.535408	40.951540
3513.485817	526754.257770	40.956544
3512.964062	526593.221555	40.961549
3513.426307	526411.357377	40.966554
3512.810740	526245.834424	40.971559
3512.509596	526081.169799	40.976564
3512.633087	525934.681839	40.981568
3512.226496	525763.207505	40.986573
3512.578826	525617.084806	40.991578
3512.232031	525445.900875	40.996583
3512.162039	525322.434935	41.001588
3511.753941	525155.149424	41.006592
3511.469154	525031.260292	41.011597
3511.623735	524887.386143	41.016602
3511.467406	524737.342781	41.021607
3511.071137	524595.524339	41.026612
3511.067630	524460.314658	41.031616
3510.486747	524339.803029	41.036621
3510.767177	524190.190997	41.041626
3510.339437	524065.659902	41.046631
3510.117714	523963.083530	41.051636
3510.613430	523828.345667	41.056640
3510.363046	523710.607787	41.061645
3510.558384	523606.952267	41.066650
3510.033281	523487.436419	41.071655
3510.101027	523363.023784	41.076660
3509.887452	523249.371234	41.081664
3509.920337	523138.509746	41.086669
3509.551958	523043.432141	41.091674
3509.488684	522922.777564	41.096679
3509.197189	522816.666371	41.101684
3509.413629	522716.186534	41.106688
3508.944483	522608.484403	41.111693
3508.811581	522504.974801	41.116698
3508.941671	522418.155857	41.121703
3508.881584	522312.308103	41.126708
3509.030484	522239.741121	41.131712
3508.673565	522120.340252	41.136717
3508.561443	522038.865667	41.141722
3508.640469	521943.913115	41.146727
3508.245685	521852.118700	41.151732
3508.693506	521758.269525	41.156736
3507.815244	521701.382713	41.161741
3508.584153	521589.079888	41.166746
3508.238808	521523.716085	41.171751
3508.085438	521450.586689	41.176756
3508.121603	521340.774067	41.181760
3507.776832	521278.341426	41.186765
3507.957282	521189.637391	41.191770
3507.672748	521123.655695	41.196775
3507.781317	521045.376874	41.201780
3507.904294	520963.000283	41.206784
3507.203480	520900.420237	41.211789
3507.761921	520821.361441	41.216794
3507.502007	520757.346112	41.221799
3507.405938	520688.602757	41.226804
3507.402373	520600.986321	41.231808
3507.403244	520563.016991	41.236813
3507.237683	520462.128587	41.241818
3506.961617	520433.353821	41.246823
3507.203424	520328.001605	41.251828
3506.940365	520291.236212	41.256832
3506.814546	520220.068753	41.261837
3506.844298	520141.191346	41.266842
3506.721801	520101.723656	41.271847
3506.513284	520047.556558	41.276852
3506.940650	519981.204936	41.281856
3506.782396	519925.613810	41.286861
3506.875328	519873.875946	41.291866
3506.632595	519805.050938	41.296871
3506.607555	519754.089749	41.301876
3506.853934	519688.675642	41.306880
3506.534777	519640.642559	41.311885
3506.545133	519592.102206	41.316890
3506.541701	519530.569604	41.321895
3506.712283	519479.930578	41.326900
3506.529417	519418.880971	41.331904
3506.191750	519388.445564	41.336909
3506.433596	519309.631762	41.341914
3505.970247	519290.390261	41.346919
3506.184276	519218.254623	41.351924
3506.113010	519191.417240	41.356928
3506.119094	519142.067233	41.361933
3506.108101	519090.090511	41.366938
3506.271337	519060.080958	41.371943
3506.094690	518977.893431	41.376948
3506.030923	518962.178375	41.381952
3506.103994	518900.631324	41.386957
3506.034124	518848.562018	41.391962
3505.905854	518827.345602	41.396967
3506.031050	518774.537342	41.401972
3505.527869	518726.985745	41.406976
3504.979382	518705.329945	41.411981
3505.758577	518662.277936	41.416986
3505.503077	518620.400628	41.421991
3505.578803	518604.865442	41.426996
3505.418059	518552.101661	41.432000
3505.204554	518533.679381	41.437005
3505.826334	518460.919773	41.442010
3505.727752	518464.070375	41.447015
3505.749193	518406.018602	41.452020
3505.631838	518350.213423	41.457024
3505.605886	518351.936746	41.462029
3505.635732	518277.348410	41.467034
3505.856390	518265.784655	41.472039
3505.378442	518198.051967	41.477044
3505.538027	518182.755957	41.482048
3505.290033	518143.758490	41.487053
3505.793634	518104.389315	41.492058
3505.503028	518080.871566	41.497063
3505.273254	518043.084563	41.502068
3505.594536	518007.940951	41.507072
3505.689835	517960.848782	41.512077
3505.484626	517955.824597	41.517082
3505.351765	517895.014269	41.522087
3505.086890	517874.627280	41.527092
3505.461914	517825.821821	41.532096
3504.920551	517814.277053	41.537101
3505.155550	517779.399426	41.542106
3505.210535	517746.522286	41.547111
3505.226860	517713.954592	41.552116
3505.748619	517666.389649	41.557120
3505.476369	517652.425578	41.562125
3505.399954	517611.225346	41.567130
3505.517528	517558.566106	41.572135
3505.236509	517564.223518	41.577140
3505.643036	517481.936371	41.582144
3505.035761	517487.291399	41.587149
3505.177179	517439.988188	41.592154
3505.064568	517416.896473	41.597159
3504.827116	517401.510788	41.602164
3504.999971	517368.007452	41.607168
3504.696072	517342.468030	41.612173
3504.727864	517315.914717	41.617178
3505.003623	517295.593272	41.622183
3504.824937	517284.901041	41.627188
3505.217200	517255.256561	41.632192
3504.530057	517227.097404	41.637197
3504.734135	517203.601361	41.642202
3505.056671	517181.755327	41.647207
3504.589041	517161.096090	41.652212
3504.808163	517126.523011	41.657216
3504.876013	517124.186131	41.662221
3504.526399	517080.195903	41.667226
3504.850531	517071.446823	41.672231
3504.580054	517054.801811	41.677236
3504.622787	517018.638176	41.682240
3504.623793	517016.564691	41.687245
3505.062944	516974.775703	41.692250
3504.517023	516952.409223	41.697255
3504.800842	516905.941662	41.702260
3504.508783	516920.096708	41.707264
3504.432911	516911.006207	41.712269
3504.582400	516859.705078	41.717274
3504.463548	516878.687467	41.722279
3504.692388	516833.189213	41.727284
3504.646706	516829.656563	41.732288
3504.639795	516794.612819	41.737293
3504.681394	516807.349842	41.742298
3504.947981	516760.075480	41.747303
3504.402735	516762.336170	41.752308
3504.960937	516722.247108	41.757312
3504.598134	516713.758118	41.762317
3504.657205	516698.122635	41.767322
3504.771229	516667.307399	41.772327
3504.567985	516667.541810	41.777332
3504.939282	516627.229208	41.782336
3504.638769	516606.694578	41.787341
3504.899479	516593.656788	41.792346
3504.719488	516548.525792	41.797351
3504.696339	516546.000931	41.802356
3504.696180	516548.226070	41.807360
3504.669186	516525.878141	41.812365
3504.845508	516496.620432	41.817370
3504.832424	516472.196833	41.822375
3504.318012	516426.157514	41.827380
3504.952067	516390.202481	41.832384
3504.761143	516408.185375	41.837389
3504.766400	516374.655954	41.842394
3504.847433	516317.194296	41.847399
3504.369467	516346.398870	41.852404
3504.284975	516308.888376	41.857408
3504.474729	516263.394742	41.862413
3504.216509	516286.445546	41.867418
3504.407351	516235.186527	41.872423
3504.420055	516241.354251	41.877428
3504.880967	516205.223899	41.882432
3504.421202	516220.468047	41.887437
3504.401512	516188.004194	41.892442
3504.845712	516159.462131	41.897447
3504.491470	516156.686108	41.902452
3504.640439	516103.005856	41.907456
3504.196316	516130.334298	41.912461
3504.624703	516086.167904	41.917466
3504.349879	516096.376310	41.922471
3504.424003	516062.683660	41.927476
3504.965639	516020.774936	41.932480
3504.296372	516056.736348	41.937485
3504.266150	516020.278640	41.942490
3503.989951	516005.656366	41.947495
3503.887396	515998.997050	41.952500
3504.347593	515987.697286	41.957504
3504.383431	515958.814842	41.962509
3504.631415	515932.124006	41.967514
3504.497343	515948.834099	41.972519
3504.058790	515936.058029	41.977524
3504.473513	515896.444811	41.982528
3504.450995	515890.430245	41.987533
3504.464874	515879.302093	41.992538
3504.611336	515874.069976	41.997543
3504.316750	515845.188984	42.002548
3504.793630	515821.597302	42.007552
3504.265343	515804.182617	42.012557
3504.628972	515790.369342	42.017562
3504.486185	515783.868017	42.022567
3504.198965	515746.995173	42.027572
3504.748802	515746.807136	42.032576
3504.358023	515741.761033	42.037581
3504.744739	515696.133576	42.042586
3504.840254	515686.711881	42.047591
3504.186684	515670.075453	42.052596
3504.701923	515627.310170	42.057600
3504.168146	515632.148436	42.062605
3504.635795	515615.891056	42.067610
3504.373703	515589.077994	42.072615
3504.523516	515569.583526	42.077620
3504.404429	515559.791088	42.082624
3504.444740	515551.996395	42.087629
3504.444869	515523.068266	42.092634
3504.499074	515534.438781	42.097639
3504.174200	515492.867977	42.102644
3504.365049	515487.831020	42.107648
3504.190129	515471.118744	42.112653
3504.191384	515453.468278	42.117658
3504.232452	515435.659778	42.122663
3504.149512	515436.330357	42.127668
3504.475718	515408.918287	42.132672
3504.531528	515392.523485	42.137677
3504.352981	515384.156415	42.142682
3504.706213	515387.994801	42.147687
3504.603287	515357.514877	42.152692
3504.663802	515332.723957	42.157696
3504.449176	515335.640619	42.162701
3504.561736	515303.558738	42.167706
3504.421444	515278.394879	42.172711
3504.036168	515273.246614	42.177716
3504.475773	515263.062256	42.182720
3504.317223	515246.246018	42.187725
3504.552264	515232.199734	42.192730
3504.364122	515205.121495	42.197735
3504.088009	515184.985850	42.202740
3504.651377	515181.710614	42.207744
3504.299233	515154.860512	42.212749
3504.176262	515148.102933	42.217754
3504.274132	515129.728808	42.222759
3504.150220	515119.329975	42.227764
3504.322279	515098.111895	42.232768
3504.365800	515096.537202	42.237773
3503.551558	515078.256602	42.242778
3503.917676	515065.099811	42.247783
3503.994309	515060.535952	42.252788
3504.266949	515055.384788	42.257792
3504.215314	515050.740049	42.262797
3504.155979	515025.461864	42.267802
3503.945009	515016.189380	42.272807
3503.483998	515020.662293	42.277812
3504.187965	515010.183124	42.282816
3504.222512	514999.405146	42.287821
3504.109665	514984.907884	42.292826
3504.332524	514978.550757	42.297831
3504.246373	514957.171007	42.302836
3504.526700	514940.689702	42.307840
3504.046309	514946.025480	42.312845
3504.251073	514923.385898	42.317850
3504.184987	514902.002906	42.322855
3503.839079	514894.521826	42.327860
3504.009801	514901.929461	42.332864
3504.166651	514887.288338	42.337869
3503.938011	514866.790778	42.342874
3504.529585	514861.943178	42.347879
3504.274133	514843.118823	42.352884
3504.224104	514825.273496	42.357888
3504.002667	514815.395646	42.362893
3504.077428	514818.418387	42.367898
3504.156334	514791.094968	42.372903
3503.916150	514779.854510	42.377908
3504.154224	514779.260557	42.382912
3504.026659	514783.579680	42.387917
3504.009742	514754.197733	42.392922
3503.960163	514756.886105	42.397927
3504.191820	514745.115867	42.402932
3504.170242	514734.194861	42.407936
3503.897848	514725.842293	42.412941
3504.070980	514714.081283	42.417946
3503.815489	514710.834223	42.422951
3503.419462	514712.161226	42.427956
3504.021218	514707.716582	42.432960
3504.247254	514687.045788	42.437965
3503.710722	514678.330333	42.442970
3503.875865	514677.090412	42.447975
3503.807174	514686.255573	42.452980
3504.275585	514666.305090	42.457984
3503.975893	514635.349186	42.462989
3503.963820	514652.142445	42.467994
3504.237102	514631.767575	42.472999
3503.707210	514623.759110	42.478004
3504.429245	514606.803056	42.483008
3503.890781	514604.814533	42.488013
3503.930491	514619.778889	42.493018
3504.172993	514616.908292	42.498023
3504.113929	514571.904567	42.503028
3504.095399	514572.514423	42.508032
3503.601824	514577.245482	42.513037
3503.949522	514569.199444	42.518042
3503.936998	514543.609674	42.523047
3503.766112	514536.303077	42.528052
3503.586236	514526.469064	42.533056
3503.602763	514534.761035	42.538061
3503.819637	514522.588365	42.543066
3504.071182	514524.065918	42.548071
3503.929427	514526.768896	42.553076
3503.910927	514501.685774	42.558080
3504.152369	514493.454186	42.563085
3504.160234	514493.655259	42.568090
3504.495719	514480.047661	42.573095
3504.397820	514464.434896	42.578100
3504.398033	514449.312379	42.583104
3504.210974	514424.710975	42.588109
3504.046384	514417.049292	42.593114
3504.110280	514402.017822	42.598119
3504.177907	514410.150047	42.603124
3504.220711	514373.879516	42.608128
3503.680421	514367.693349	42.613133
3503.974268	514359.858031	42.618138
3504.544660	514359.869045	42.623143
3503.883686	514341.158795	42.628148
3503.963689	514328.957039	42.633152
3504.046974	514321.913641	42.638157
3504.182064	514316.177063	42.643162
3504.268897	514304.075364	42.648167
3503.860849	514284.667570	42.653172
3504.273590	514290.165861	42.658176
3503.906840	514275.000030	42.663181
3503.945234	514250.160427	42.668186
3504.196070	514246.378055	42.673191
3503.801905	514253.116593	42.678196
3503.876255	514247.895367	42.683200
3503.745404	514235.979756	42.688205
3503.980447	514225.725946	42.693210
3504.045120	514217.117541	42.698215
3503.905964	514218.100518	42.703220
3503.947310	514223.303485	42.708224
3504.508391	514188.973747	42.713229
3504.090041	514183.274016	42.718234
3504.158529	514169.202588	42.723239
3504.096050	514164.205272	42.728244
3504.007236	514145.910152	42.733248
3503.962435	514143.894128	42.738253
3504.315161	514139.943896	42.743258
3504.481009	514118.320937	42.748263
3504.057442	514112.925473	42.753268
3504.218165	514092.416005	42.758272
3504.126765	514078.673240	42.763277
3503.937322	514066.867925	42.768282
3503.865828	514059.697146	42.773287
3504.241755	514070.309714	42.778292
3504.339308	514044.499475	42.783296
3504.348159	514030.538513	42.788301
3504.413235	514015.304197	42.793306
3504.303019	513997.770972	42.798311
3504.184609	513994.552685	42.803316
3504.222234	513976.894915	42.808321
3503.815206	513972.407202	42.813325
3503.671405	513953.513623	42.818330
3504.422260	513932.152015	42.823335
3504.261992	513946.440478	42.828340
3504.297525	513912.951915	42.833345
3504.229488	513909.725650	42.838349
3504.144216	513917.730544	42.843354
3504.260139	513878.969041	42.848359
3504.007492	513898.330008	42.853364
3504.176472	513866.893984	42.858369
3504.292821	513843.002454	42.863373
3503.764599	513845.766620	42.868378
3504.102322	513831.298306	42.873383
3503.786748	513823.457899	42.878388
3504.142181	513810.655870	42.883393
3504.018095	513800.205667	42.888397
3504.153754	513787.590091	42.893402
3504.120617	513786.583759	42.898407
3504.265372	513781.401839	42.903412
3504.301962	513750.745206	42.908417
3504.192829	513751.521148	42.913421
3503.962899	513757.677557	42.918426
3504.384528	513711.078184	42.923431
3503.755878	513706.726584	42.928436
3504.048132	513702.886966	42.933441
3503.834756	513693.462392	42.938445
3503.801801	513706.112403	42.943450
3504.166183	513657.903397	42.948455
3503.491511	513677.685372	42.953460
3503.991657	513665.062678	42.958465
3504.023271	513669.812141	42.963469
3504.046112	513643.203826	42.968474
3504.128620	513628.472199	42.973479
3503.944334	513621.521377	42.978484
3503.987019	513621.211163	42.983489
3503.765081	513625.393759	42.988493
3503.836895	513587.599565	42.993498
3504.158745	513583.249448	42.998503
3503.922749	513600.180307	43.003508
3504.224941	513578.433948	43.008513
3503.978128	513574.072544	43.013517
3504.123821	513548.152776	43.018522
3503.999469	513546.655049	43.023527
3504.225122	513541.763748	43.028532
3504.437319	513526.859797	43.033537
3503.908416	513533.822234	43.038541
3503.968924	513516.008625	43.043546
3504.067569	513495.508242	43.048551
3503.894625	513492.905435	43.053556
3504.239159	513475.400952	43.058561
3503.931905	513475.854161	43.063565
3503.935451	513465.181258	43.068570
3503.934451	513447.781937	43.073575
3503.832484	513442.133108	43.078580
3504.044452	513431.376664	43.083585
3503.872434	513435.601997	43.088589
3503.889796	513442.629876	43.093594
3503.985826	513423.242577	43.098599
3503.606017	513421.532313	43.103604
3504.039788	513408.464698	43.108609
3503.922841	513412.529593	43.113613
3503.854752	513407.482359	43.118618
3503.737902	513377.203357	43.123623
3503.870173	513386.185724	43.128628
3503.824908	513372.839731	43.133633
3503.817555	513372.031619	43.138637
3503.788055	513364.246944	43.143642
3503.876121	513355.027439	43.148647
3503.719105	513346.655946	43.153652
3503.549796	513327.462214	43.158657
3504.027865	513324.857650	43.163661
3504.072827	513311.598509	43.168666
3504.072226	513322.726284	43.173671
3503.961108	513312.577210	43.178676
3504.018282	513281.764729	43.183681
3503.682634	513288.190919	43.188685
3503.602972	513280.414134	43.193690
3504.069383	513275.838768	43.198695
3503.868130	513273.695625	43.203700
3503.785733	513250.745115	43.208705
3503.752827	513254.139219	43.213709
3503.969633	513249.350393	43.218714
3504.028363	513233.914052	43.223719
3503.807870	513244.773148	43.228724
3504.263550	513227.958971	43.233729
3504.169781	513210.523487	43.238733
3504.060549	513212.715727	43.243738
3503.997368	513192.948681	43.248743
3503.820830	513175.526242	43.253748
3504.073189	513166.584152	43.258753
3504.022711	513157.335855	43.263757
3503.732638	513156.774739	43.268762
3503.734400	513157.988409	43.273767
3503.802479	513136.936032	43.278772
3504.154665	513114.169555	43.283777
3503.845147	513123.120724	43.288781
3503.748253	513130.369115	43.293786
3504.184212	513123.168315	43.298791
3504.085184	513105.784135	43.303796
3504.004107	513088.751167	43.308801
3504.092463	513086.056417	43.313805
3503.852495	513085.892028	43.318810
3503.919645	513064.030411	43.323815
3503.883660	513065.755864	43.328820
3504.071965	513044.937276	43.333825
3504.136414	513045.534072	43.338829
3503.827908	513039.968332	43.343834
3504.144747	513010.277683	43.348839
3503.774980	513010.133808	43.353844
3504.061445	513003.664722	43.358849
3503.995266	513002.056590	43.363853
3504.050328	512995.978143	43.368858
3504.091257	512964.763001	43.373863
3503.768457	512975.790183	43.378868
3504.014314	512953.900179	43.383873
3504.134905	512939.414839	43.388877
3503.759626	512943.824164	43.393882
3504.286530	512927.706572	43.398887
3503.765500	512923.691827	43.403892
3503.856850	512928.179151	43.408897
3503.952850	512919.919203	43.413901
3503.718711	512898.256733	43.418906
3503.969381	512888.707785	43.423911
3503.396726	512907.816974	43.428916
3503.917590	512897.365440	43.433921
3503.887847	512895.650376	43.438925
3503.750124	512883.380822	43.443930
3503.939325	512871.970059	43.448935
3503.863967	512863.686584	43.453940
3503.727227	512848.027875	43.458945
3504.201047	512860.092609	43.463949
3503.957226	512838.532756	43.468954
3504.072790	512829.763854	43.473959
3503.755597	512815.195853	43.478964
3503.770741	512798.349711	43.483969
3503.792848	512825.104018	43.488973
3503.824422	512801.730230	43.493978
3504.014123	512804.128186	43.498983
3503.863325	512785.386148	43.503988
3504.118263	512764.303774	43.508993
3504.032028	512771.550633	43.513997
3504.137977	512777.350821	43.519002
3504.153866	512737.843777	43.524007
3503.960202	512740.352915	43.529012
3504.117517	512722.472587	43.534017
3503.761792	512740.637201	43.539021
3503.801019	512704.717716	43.544026
3503.899965	512691.044898	43.549031
3503.680179	512705.900221	43.554036
3504.043778	512691.173933	43.559041
3504.057538	512685.607724	43.564045
3503.745595	512693.800769	43.569050
3504.418607	512653.582685	43.574055
3503.801048	512650.797106	43.579060
3503.717532	512666.591991	43.584065
3504.047107	512640.085362	43.589069
3503.970356	512634.229947	43.594074
3504.022073	512628.151897	43.599079
3503.928577	512615.369334	43.604084
3503.708491	512630.680012	43.609089
3503.967148	512616.627816	43.614093
3503.698982	512586.674805	43.619098
3504.048507	512601.187329	43.624103
3504.173125	512576.483380	43.629108
3504.142543	512588.071620	43.634113
3504.191292	512558.624880	43.639117
3503.751025	512561.122436	43.644122
3503.880499	512527.161032	43.649127
3503.821581	512552.866339	43.654132
3504.110289	512501.833368	43.659137
3503.745365	512533.302920	43.664141
3504.058077	512492.129744	43.669146
3503.741290	512505.129010	43.674151
3503.967637	512494.116784	43.679156
3503.805363	512493.080201	43.684161
3504.226123	512470.909016	43.689165
3503.886062	512454.573917	43.694170
3504.015421	512461.635086	43.699175
3503.957322	512455.068501	43.704180
3503.980075	512430.178107	43.709185
3504.070740	512420.502434	43.714189
3503.993281	512432.502854	43.719194
3504.116176	512407.242518	43.724199
3503.955388	512404.587037	43.729204
3504.101193	512388.630332	43.734209
3503.834265	512390.999350	43.739213
3504.115414	512370.418175	43.744218
3503.930829	512356.638149	43.749223
3503.681435	512360.623063	43.754228
3503.905404	512331.047067	43.759233
3503.904267	512325.887761	43.764237
3504.001332	512335.331501	43.769242
3504.128132	512318.720152	43.774247
3503.922776	512293.663275	43.779252
3503.718743	512318.531955	43.784257
3504.109563	512295.808857	43.789261
3503.761547	512282.661601	43.794266
3503.840170	512294.081033	43.799271
3503.338794	512301.140789	43.804276
3503.655804	512260.421621	43.809281
3503.942814	512264.524114	43.814285
3503.652440	512278.986299	43.819290
3503.625542	512272.010045	43.824295
3503.835725	512242.739574	43.829300
3503.795517	512283.162137	43.834305
3504.017956	512260.971438	43.839309
3504.015657	512263.905652	43.844314
3504.133734	512228.529113	43.849319
3503.682958	512238.717079	43.854324
3504.088046	512228.890436	43.859329
3503.912649	512198.972660	43.864333
3503.587121	512207.168087	43.869338
3503.931352	512181.568931	43.874343
3503.800533	512174.356141	43.879348
3504.004747	512184.845290	43.884353
3504.063400	512183.773771	43.889357
3503.999293	512155.912262	43.894362
3504.121322	512150.328765	43.899367
3503.863835	512145.361671	43.904372
3503.960872	512136.797674	43.909377
3503.683090	512137.246256	43.914381
3503.720259	512121.862892	43.919386
3504.370066	512102.234804	43.924391
3504.004453	512091.366458	43.929396
3503.815292	512122.201986	43.934401
3503.581727	512112.020959	43.939405
3504.007018	512074.116930	43.944410
3503.855292	512077.681801	43.949415
3503.661647	512066.229836	43.954420
3503.626094	512073.317232	43.959425
3504.103126	512041.879710	43.964429
3503.762589	512072.182827	43.969434
3503.843273	512048.496733	43.974439
3504.161748	512024.874192	43.979444
3503.798152	512030.900600	43.984449
3504.056622	512005.415901	43.989453
3503.847314	512038.278135	43.994458
3504.214760	511986.371237	43.999463
3503.620588	512007.052953	44.004468
3503.955442	511969.061815	44.009473
3503.784085	511996.353852	44.014477
3503.836984	511976.769375	44.019482
3504.150337	511964.073771	44.024487
3504.322652	511962.731352	44.029492
3503.956530	511936.485330	44.034497
3504.096132	511937.525549	44.039501
3504.107863	511909.702234	44.044506
3504.067465	511888.665449	44.049511
3503.846589	511900.739496	44.054516
3503.950034	511895.765868	44.059521
3504.100385	511862.153923	44.064525
3503.697209	511882.552680	44.069530
3503.782814	511846.978139	44.074535
3503.661022	511846.036287	44.079540
3503.780669	511864.329045	44.084545
3504.128538	511847.783464	44.089549
3503.862601	511837.253295	44.094554
3504.216984	511820.656073	44.099559
3503.767892	511833.676763	44.104564
3503.883498	511817.876048	44.109569
3503.926124	511800.872817	44.114573
3503.573397	511782.515676	44.119578
3503.702916	511791.549911	44.124583
3503.615759	511771.380314	44.129588
3503.918423	511779.628416	44.134593
3504.022283	511779.409670	44.139597
3503.611443	511770.571663	44.144602
3503.563376	511771.287458	44.149607
3503.765775	511757.294027	44.154612
3503.692282	511739.853822	44.159617
3504.058307	511728.414344	44.164621
3503.747750	511733.876037	44.169626
3503.875497	511743.062334	44.174631
3503.913110	511729.853700	44.179636
3503.997409	511732.673149	44.184641
3503.890473	511713.973577	44.189645
3504.067890	511699.832292	44.194650
3504.012195	511705.456054	44.199655
3503.851969	511711.450432	44.204660
3503.950702	511669.600888	44.209665
3503.945305	511651.896904	44.214669
3503.872265	511660.052688	44.219674
3503.994582	511641.367387	44.224679
3503.913859	511658.629744	44.229684
3504.059046	511635.691658	44.234689
3503.824616	511629.354963	44.239693
3503.968561	511601.965516	44.244698
3503.749466	511621.475539	44.249703
3503.844066	511625.153329	44.254708
3503.757689	511599.368426	44.259713
3503.825735	511578.364703	44.264717
3504.090517	511593.346756	44.269722
3504.028189	511571.655433	44.274727
3503.856903	511579.523270	44.279732
3503.757779	511556.269592	44.284737
3503.583710	511555.690085	44.289741
3503.433291	511529.409341	44.294746
3503.877280	511560.702262	44.299751
3503.621492	511540.811970	44.304756
3503.797318	511524.647366	44.309761
3503.658982	511548.140978	44.314765
3503.928663	511548.098364	44.319770
3503.652263	511524.923246	44.324775
3503.971466	511518.246081	44.329780
3503.953749	511487.543343	44.334785
3503.879782	511521.801587	44.339789
3503.664115	511493.052401	44.344794
3503.812194	511510.379917	44.349799
3503.724032	511487.933784	44.354804
3503.513386	511471.526696	44.359809
3503.712172	511489.605007	44.364813
3503.777636	511461.114849	44.369818
3503.890023	511485.024195	44.374823
3503.865266	511470.054714	44.379828
3503.576123	511470.302764	44.384833
3503.995118	511464.419179	44.389837
3503.811975	511429.139167	44.394842
3504.237562	511427.200232	44.399847
3503.785567	511430.053906	44.404852
3503.704435	511423.237631	44.409857
3503.825163	511412.342569	44.414861
3503.658112	511414.746523	44.419866
3503.720997	511391.112911	44.424871
3503.473603	511387.003961	44.429876
3503.800977	511392.010837	44.434881
3503.751172	511394.092746	44.439885
3503.643097	511381.868003	44.444890
3504.073776	511388.679653	44.449895
3503.939419	511388.093864	44.454900
3503.865593	511363.874788	44.459905
3504.110215	511352.403659	44.464909
3503.779676	511357.109838	44.469914
3503.880724	511347.533086	44.474919
3504.025236	511350.950117	44.479924
3503.967090	511321.973400	44.484929
3504.333401	511303.451511	44.489933
3503.902550	511323.349448	44.494938
3504.318294	511302.442189	44.499943
3504.037082	511282.757959	44.504948
3504.111319	511273.590094	44.509953
3504.039691	511272.640281	44.514957
3503.742560	511253.009118	44.519962
3504.100542	511224.624092	44.524967
3503.822033	511223.959907	44.529972
3504.035377	511211.431308	44.534977
3504.317517	511212.145525	44.539981
3503.833647	511201.548230	44.544986
3503.758769	511186.839354	44.549991
3504.195664	511173.466010	44.554996
3504.069688	511176.015265	44.560001
3504.185354	511152.524740	44.565005
3503.823269	511148.029164	44.570010
3504.061191	511141.010590	44.575015
3504.022839	511150.122286	44.580020
3503.758918	511132.104512	44.585025
3503.938179	511105.669834	44.590029
3503.383929	511125.081635	44.595034
3503.734165	511085.315552	44.600039
3503.542760	511113.219219	44.605044
3503.879132	511095.410052	44.610049
3504.026145	511116.886269	44.615053
3503.939115	511073.091727	44.620058
3503.620398	511078.251397	44.625063
3503.812283	511059.605050	44.630068
3503.738448	511059.464967	44.635073
3504.113739	511083.383913	44.640077
3503.791839	511057.584825	44.645082
3503.607399	511053.718779	44.650087
3503.722343	511026.889448	44.655092
3503.619049	511013.753115	44.660097
3503.744603	511054.759449	44.665101
3503.451435	511025.009978	44.670106
3503.527309	511021.912178	44.675111
3503.517446	511044.222675	44.680116
3503.738255	511030.832783	44.685121
3504.016805	511020.519574	44.690125
3504.001091	511011.163435	44.695130
3504.146122	511007.144133	44.700135
3503.862014	511000.713879	44.705140
3503.784732	511005.481302	44.710145
3504.163495	510999.755678	44.715149
3503.849065	510993.987848	44.720154
3504.124984	510969.611760	44.725159
3504.052017	510959.607007	44.730164
3503.614798	510946.725748	44.735169
3504.068225	510954.849250	44.740173
3503.883659	510941.675120	44.745178
3504.029855	510932.090999	44.750183
3504.006574	510921.218384	44.755188
3504.103545	510929.853522	44.760193
3503.898258	510913.242698	44.765197
3503.623689	510880.960660	44.770202
3503.922167	510884.151101	44.775207
3503.724120	510874.621354	44.780212
3503.827335	510866.511030	44.785217
3503.879228	510851.933592	44.790221
3503.558121	510881.932231	44.795226
3503.736797	510831.366923	44.800231
3503.739742	510853.270944	44.805236
3504.035317	510829.195075	44.810241
3504.049961	510846.038480	44.815245
3503.786512	510838.390795	44.820250
3503.944459	510817.017810	44.825255
3503.805278	510808.541066	44.830260
3503.641322	510796.122382	44.835265
3503.819386	510800.950681	44.840269
3503.837640	510790.476120	44.845274
3503.949842	510789.648990	44.850279
3503.920619	510781.761909	44.855284
3503.828337	510760.175461	44.860289
3503.891791	510769.878325	44.865293
3503.475379	510753.654828	44.870298
3503.800644	510740.956432	44.875303
3503.874492	510743.777697	44.880308
3503.534657	510748.637276	44.885313
3503.628976	510764.456410	44.890317
3503.531150	510751.268422	44.895322
3503.905868	510722.222272	44.900327
3503.655527	510722.261846	44.905332
3503.615205	510700.161230	44.910337
3503.344660	510719.731004	44.915341
3503.427922	510722.854314	44.920346
3503.681745	510724.989493	44.925351
3503.852376	510730.628395	44.930356
3503.711743	510715.170684	44.935361
3504.138218	510716.317403	44.940365
3503.854010	510701.489428	44.945370
3503.548958	510683.730620	44.950375
3504.010584	510672.781208	44.955380
3503.695989	510685.629750	44.960385
3504.178704	510669.011126	44.965389
3503.461998	510659.714997	44.970394
3503.720725	510650.618815	44.975399
3504.135674	510621.414370	44.980404
3503.812685	510634.314866	44.985409
3503.869819	510636.177613	44.990413
3503.688413	510638.482767	44.995418
3504.274521	510612.134788	45.000423
3503.539325	510623.886319	45.005428
3503.663548	510604.845462	45.010433
3503.818480	510586.457380	45.015437
3503.512063	510617.314166	45.020442
3503.786554	510586.867151	45.025447
3503.554002	510601.119267	45.030452
3503.449071	510605.031169	45.035457
3503.700358	510596.442018	45.040461
3503.620211	510578.951086	45.045466
3503.660123	510555.927008	45.050471
3504.157371	510559.086095	45.055476
3503.732410	510564.363888	45.060481
3503.916424	510550.675904	45.065485
3503.558578	510561.609010	45.070490
3503.801697	510552.414066	45.075495
3503.790347	510516.497948	45.080500
3503.563405	510530.799824	45.085505
3503.626453	510527.501607	45.090509
3503.672575	510510.901244	45.095514
3503.676133	510518.893701	45.100519
3503.491362	510525.347672	45.105524
3503.674008	510514.998727	45.110529
3503.848495	510505.612250	45.115533
3503.416090	510549.085655	45.120538
3503.841148	510514.061741	45.125543
3503.704370	510482.313646	45.130548
3503.904099	510490.730411	45.135553
3504.025376	510468.553365	45.140557
3503.928500	510476.409950	45.145562
3503.793472	510481.591356	45.150567
3503.909548	510467.610510	45.155572
3503.518615	510438.431943	45.160577
3503.933631	510427.489741	45.165581
3503.419646	510446.693592	45.170586
3503.857481	510439.491368	45.175591
3503.708662	510439.919608	45.180596
3503.487297	510428.673275	45.185601
3503.680743	510442.807606	45.190605
3503.369304	510441.693292	45.195610
3504.070357	510430.857652	45.200615
3503.823192	510421.335414	45.205620
3503.637523	510398.751489	45.210625
3503.855471	510392.545190	45.215629
3503.995199	510395.609046	45.220634
3503.430780	510394.332356	45.225639
3503.611585	510398.806213	45.230644
3503.942550	510401.536309	45.235649
3503.902308	510376.146974	45.240653
3503.398321	510377.036062	45.245658
3503.655871	510369.407001	45.250663
3503.410971	510375.769353	45.255668
3503.599646	510375.284240	45.260673
3503.998894	510372.084625	45.265677
3503.667165	510372.895899	45.270682
3503.565210	510376.099135	45.275687
3503.754261	510375.361017	45.280692
3503.832023	510362.752047	45.285697
3503.686945	510350.228876	45.290701
3503.549586	510322.527708	45.295706
3503.407368	510327.204405	45.300711
3503.656865	510335.259257	45.305716
3503.602131	510331.827849	45.310721
3503.624520	510325.854790	45.315725
3503.353618	510339.000223	45.320730
3503.421685	510329.681058	45.325735
3503.497588	510331.287926	45.330740
3503.334182	510341.785727	45.335745
3503.605439	510329.854400	45.340749
3503.327353	510341.533877	45.345754
3503.485072	510326.838087	45.350759
3503.369515	510330.701141	45.355764
3503.298304	510328.486478	45.360769
3503.957486	510333.592994	45.365773
3503.690273	510340.515368	45.370778
3504.047122	510326.192818	45.375783
3503.655662	510305.411918	45.380788
3503.862146	510297.892074	45.385793
3504.125346	510288.036153	45.390797
3503.561754	510303.554982	45.395802
3503.671638	510292.306794	45.400807
3503.771531	510297.147591	45.405812
3503.640269	510280.473860	45.410817
3503.779603	510256.270110	45.415821
3503.703447	510259.013985	45.420826
3503.890525	510257.466743	45.425831
3503.953784	510256.697912	45.430836
3503.741650	510263.763380	45.435841
3504.031202	510245.960728	45.440845
3503.800408	510236.334621	45.445850
3504.194184	510220.842589	45.450855
3504.113409	510219.185909	45.455860
3503.956650	510205.045612	45.460865
3503.942894	510178.791774	45.465869
3503.841609	510176.227717	45.470874
3503.681671	510167.855114	45.475879
3503.884271	510180.470525	45.480884
3504.007581	510177.061536	45.485889
3503.980323	510151.315687	45.490893
3503.741805	510143.259030	45.495898
3503.940424	510137.207463	45.500903
3503.779205	510136.474105	45.505908
3503.504192	510143.498970	45.510913
3503.650713	510133.104913	45.515917
3503.267872	510137.263204	45.520922
3503.707009	510136.637320	45.525927
3503.782434	510110.470462	45.530932
3503.344569	510101.737033	45.535937
3503.873900	510093.963715	45.540941
3503.439016	510089.580543	45.545946
3503.498344	510095.085477	45.550951
3503.742586	510098.436408	45.555956
3503.396551	510097.175770	45.560961
3503.851278	510093.512025	45.565965
3503.776803	510096.559200	45.570970
3503.719781	510095.961142	45.575975
3503.669239	510105.176502	45.580980
3503.533563	510087.592662	45.585985
3503.610264	510067.091609	45.590989
3503.568558	510066.086409	45.595994
3503.965998	510053.274916	45.600999
3503.923525	510054.698159	45.606004
3503.663106	510057.977089	45.611009
3503.676703	510065.006962	45.616013
3504.025187	510062.725933	45.621018
3503.508336	510040.042106	45.626023
3503.558890	510024.958272	45.631028
3503.479690	510025.982601	45.636033
3504.063430	510016.834716	45.641037
3503.494933	510016.671624	45.646042
3503.773994	510018.246412	45.651047
3503.579847	510020.857203	45.656052
3503.278368	510022.068433	45.661057
3503.573118	510010.639072	45.666061
3503.315703	510025.199138	45.671066
3503.401333	510022.200796	45.676071
3503.198640	510031.743783	45.681076
3503.212956	510028.503762	45.686081
3503.361786	510020.942319	45.691085
3503.268527	510026.167851	45.696090
3503.442164	510019.968420	45.701095
3503.849639	510018.234553	45.706100
3503.240219	510026.880613	45.711105
3503.401729	510016.888838	45.716109
3503.490424	510027.296397	45.721114
3503.543603	510037.051892	45.726119
3503.593639	510030.669639	45.731124
3503.198678	510027.544894	45.736129
3503.627583	510019.939185	45.741133
3503.709324	510033.282067	45.746138
3503.778099	510020.674266	45.751143
3503.559058	509991.973669	45.756148
3503.182942	509998.609850	45.761153
3503.667126	509990.843621	45.766157
3503.706791	509988.459620	45.771162
3503.717542	509990.936851	45.776167
3503.938679	509989.080661	45.781172
3503.501645	510000.937263	45.786177
3503.598566	509993.181651	45.791181
3503.434874	510002.212589	45.796186
3503.462529	510003.776523	45.801191
3503.911257	509996.218261	45.806196
3503.739984	509981.270629	45.811201
3503.875488	509964.453247	45.816205
3503.807862	509952.372856	45.821210
3504.057126	509952.232289	45.826215
3503.799490	509955.409617	45.831220
3503.849470	509942.147054	45.836225
3503.880851	509924.131920	45.841229
3503.819978	509926.519300	45.846234
3503.718030	509920.211617	45.851239
3503.701913	509917.482289	45.856244
3503.975868	509919.513208	45.861249
3503.820933	509915.591649	45.866253
3503.916199	509899.893554	45.871258
3503.937692	509883.245884	45.876263
3503.505491	509870.363016	45.881268
3503.652903	509874.134020	45.886273
3504.047561	509871.238581	45.891277
3503.796831	509883.268181	45.896282
3503.610872	509871.257026	45.901287
3504.034429	509848.323133	45.906292
3503.347413	509846.610460	45.911297
3503.381108	509835.222242	45.916301
3503.534308	509850.172875	45.921306
3503.631041	509839.533556	45.926311
3503.832926	509839.299295	45.931316
3503.600695	509847.683467	45.936321
3504.057416	509832.130545	45.941325
3503.956662	509832.247659	45.946330
3503.694734	509805.830109	45.951335
3503.708190	509795.659242	45.956340
3503.695434	509800.821529	45.961345
3503.867345	509790.271479	45.966349
3503.678326	509796.827577	45.971354
3503.657650	509790.557593	45.976359
3503.948884	509791.422207	45.981364
3503.699263	509782.456500	45.986369
3503.824616	509763.920437	45.991373
3503.515014	509778.387778	45.996378
3503.982336	509770.522934	46.001383
3504.329102	509764.194866	46.006388
3503.582888	509757.179495	46.011393
3503.754063	509728.113236	46.016397
3503.660766	509719.780472	46.021402
3503.630183	509722.820776	46.026407
3504.127089	509711.612221	46.031412
3503.676761	509731.262131	46.036417
3504.343528	509712.842807	46.041421
3503.863088	509700.220390	46.046426
3503.598067	509691.155886	46.051431
3503.886610	509684.381672	46.056436
3503.712310	509686.685829	46.061441
3503.890849	509682.559738	46.066445
3503.921770	509689.941165	46.071450
3503.654148	509653.153096	46.076455
3503.774875	509659.356744	46.081460
3503.450581	509652.072280	46.086465
3503.873449	509635.563297	46.091469
3503.711746	509643.481101	46.096474
3503.618897	509648.403135	46.101479
3503.730652	509635.585892	46.106484
3503.670143	509642.172330	46.111489
3503.895416	509620.433070	46.116493
3503.777500	509623.436603	46.121498
3503.895407	509608.898263	46.126503
3503.811543	509611.289320	46.131508
3503.680802	509614.092516	46.136513
3504.174758	509604.503281	46.141517
3503.734492	509584.842226	46.146522
3503.859477	509566.862514	46.151527
3503.766998	509556.657657	46.156532
3503.490481	509554.880074	46.161537
3503.610383	509563.917012	46.166541
3503.427374	509558.836204	46.171546
3503.404744	509554.893651	46.176551
3503.570119	509564.378725	46.181556
3503.288626	509570.140061	46.186561
3503.980865	509559.355858	46.191565
3503.740206	509567.842682	46.196570
3503.810986	509536.363575	46.201575
3503.952418	509529.561958	46.206580
3503.796015	509527.866572	46.211585
3504.152427	509511.671523	46.216589
3504.027129	509514.777425	46.221594
3504.119908	509494.930837	46.226599
3504.192528	509481.563156	46.231604
3503.589024	509487.577779	46.236609
3503.993661	509473.044599	46.241613
3503.935242	509471.080762	46.246618
3503.641168	509452.205918	46.251623
3503.561885	509445.439152	46.256628
3503.540939	509437.044223	46.261633
3503.795303	509428.858738	46.266637
3503.860809	509443.368260	46.271642
3503.979298	509434.597149	46.276647
3503.824575	509431.940243	46.281652
3503.572931	509414.323448	46.286657
3503.827952	509393.742814	46.291661
3504.048752	509380.048081	46.296666
3504.231163	509385.887935	46.301671
3503.815095	509396.375655	46.306676
3503.790894	509383.731488	46.311681
3503.892846	509356.952182	46.316685
3503.511367	509358.732614	46.321690
3503.833234	509352.762476	46.326695
3503.816727	509352.208580	46.331700
3503.485992	509358.483691	46.336705
3503.621170	509351.025295	46.341709
3503.966809	509356.535808	46.346714
3503.792482	509329.749533	46.351719
3504.176113	509318.862179	46.356724
3503.754711	509310.834034	46.361729
3504.065169	509306.636411	46.366733
3503.842140	509304.243241	46.371738
3503.797698	509291.551612	46.376743
3503.732120	509277.952653	46.381748
3503.591344	509278.227872	46.386753
3503.808756	509280.116028	46.391757
3504.264724	509280.904042	46.396762
3503.699400	509267.384058	46.401767
3503.935221	509241.696446	46.406772
3503.913500	509235.426424	46.411777
3503.902756	509229.306442	46.416781
3504.074249	509235.856368	46.421786
3503.806157	509224.161293	46.426791
3504.102781	509186.777120	46.431796
3503.784301	509192.847983	46.436801
3503.861457	509193.189946	46.441805
3503.734670	509195.385474	46.446810
3503.969046	509189.935033	46.451815
3503.840806	509166.783886	46.456820
3503.707495	509156.382873	46.461825
3504.192407	509139.914201	46.466829
3503.695924	509153.500935	46.471834
3503.937573	509137.981378	46.476839
3503.868351	509153.018367	46.481844
3503.605687	509123.918467	46.486849
3503.861293	509112.899439	46.491853
3503.671675	509111.816374	46.496858
3503.804114	509108.506917	46.501863
3503.685371	509120.364413	46.506868
3503.439294	509126.929783	46.511873
3503.530289	509112.951797	46.516877
3503.598668	509124.374973	46.521882
3503.487469	509122.267659	46.526887
3503.795214	509114.579516	46.531892
3503.478209	509086.752962	46.536897
3503.566353	509081.527970	46.541901
3503.567137	509074.090695	46.546906
3503.410732	509069.865616	46.551911
3503.417388	509074.114380	46.556916
3503.285241	509083.798523	46.561921
3503.805874	509065.452197	46.566925
3503.530890	509075.917813	46.571930
3503.305773	509083.339968	46.576935
3503.566447	509082.691663	46.581940
3503.478261	509076.432087	46.586945
3503.878803	509074.749817	46.591949
3503.774445	509074.310983	46.596954
3503.749900	509069.154391	46.601959
3503.845118	509073.793901	46.606964
3503.566771	509064.022870	46.611969
3503.919303	509030.272213	46.616973
3503.726160	509032.630029	46.621978
3503.529666	509045.764690	46.626983
3503.736572	509033.488483	46.631988
3504.039026	509035.717376	46.636993
3503.921557	509015.245754	46.641997
3503.921991	509000.421907	46.647002
3503.882038	508996.127811	46.652007
3503.768333	508995.285707	46.657012
3503.814945	509002.007239	46.662017
3503.799643	508993.611202	46.667021
3503.808375	509001.047025	46.672026
3503.628430	508972.642100	46.677031
3503.608698	508965.258613	46.682036
3503.607899	508963.386798	46.687041
3503.607462	508955.899071	46.692045
3503.560974	508963.090672	46.697050
3503.560234	508953.528668	46.702055
3504.105017	508957.490038	46.707060
3503.479527	508964.520182	46.712065
3503.774281	508939.784077	46.717069
3503.946733	508936.012923	46.722074
3503.748572	508927.291601	46.727079
3503.851521	508920.849980	46.732084
3503.541054	508920.797870	46.737089
3503.957866	508919.163607	46.742093
3503.975487	508919.464392	46.747098
3503.735106	508910.749733	46.752103
3504.151098	508880.277325	46.757108
3503.841897	508875.772786	46.762113
3503.898351	508874.549628	46.767117
3503.874955	508874.300367	46.772122
3503.986575	508859.155264	46.777127
3504.055157	508837.338591	46.782132
3503.633798	508838.113506	46.787137
3503.638010	508829.916679	46.792141
3503.704137	508829.552081	46.797146
3503.472810	508829.285089	46.802151
3503.746830	508822.664612	46.807156
3503.677463	508825.255862	46.812161
3504.093217	508799.893308	46.817165
3504.201873	508789.555017	46.822170
3503.925767	508790.003414	46.827175
3504.225015	508778.724306	46.832180
3503.773316	508761.189052	46.837185
3503.798368	508741.048735	46.842189
3504.079389	508738.069881	46.847194
3503.634357	508743.047837	46.852199
3503.970593	508733.988985	46.857204
3503.526004	508728.797491	46.862209
3503.539022	508714.224378	46.867213
3504.050871	508699.370036	46.872218
3503.612241	508701.614913	46.877223
3503.731058	508694.563571	46.882228
3503.690392	508705.599507	46.887233
3504.059942	508694.511609	46.892237
3504.034655	508682.878979	46.897242
3503.449639	508662.784396	46.902247
3503.651042	508657.895534	46.907252
3503.719133	508656.771710	46.912257
3504.009182	508661.329945	46.917261
3504.013488	508665.022646	46.922266
3503.893651	508660.488121	46.927271
3504.014753	508628.442861	46.932276
3503.845332	508616.074052	46.937281
3503.797388	508613.754301	46.942285
3503.839036	508613.747727	46.947290
3503.790363	508617.600594	46.952295
3504.004714	508601.325954	46.957300
3503.811721	508584.457952	46.962305
3503.880527	508569.268766	46.967309
3503.758888	508578.546776	46.972314
3503.737835	508571.264518	46.977319
3503.679636	508572.133830	46.982324
3503.291002	508583.174246	46.987329
3503.537854	508571.802095	46.992333
3503.503009	508575.602192	46.997338
3503.328443	508568.495978	47.002343
3503.875949	508554.394793	47.007348
3503.567342	508540.125337	47.012353
3503.758117	508542.473136	47.017357
3503.822721	508539.983804	47.022362
3503.710572	508531.400469	47.027367
3503.907626	508534.050844	47.032372
3503.881705	508541.745315	47.037377
3503.851174	508519.690932	47.042381
3503.958740	508505.305077	47.047386
3503.506100	508508.513491	47.052391
3503.942504	508493.974465	47.057396
3503.605375	508492.206349	47.062401
3503.749625	508504.882811	47.067405
3503.811471	508485.039947	47.072410
3503.629472	508477.479518	47.077415
3503.731743	508469.216427	47.082420
3503.683184	508470.994925	47.087425
3503.589807	508446.319456	47.092429
3503.522799	508469.401260	47.097434
3503.592507	508471.211662	47.102439
3503.849036	508454.677243	47.107444
3503.574024	508461.702792	47.112449
3503.781592	508460.455721	47.117453
3503.380404	508466.135153	47.122458
3503.751518	508447.609423	47.127463
3503.855466	508426.039614	47.132468
3503.809357	508418.407087	47.137473
3503.876633	508413.134596	47.142477
3503.679247	508419.388971	47.147482
3503.502776	508422.452562	47.152487
3503.707673	508408.152433	47.157492
3503.688553	508412.506624	47.162497
3503.824811	508416.077333	47.167501
3503.856475	508394.468314	47.172506
3503.560468	508381.056848	47.177511
3503.412074	508377.994017	47.182516
3503.436932	508384.112089	47.187521
3503.342529	508380.939535	47.192525
3503.814012	508373.731133	47.197530
3503.685009	508375.168191	47.202535
3503.968023	508376.135369	47.207540
3503.786961	508388.053813	47.212545
3503.714495	508356.392805	47.217549
3503.569167	508350.900921	47.222554
3503.709636	508342.075186	47.227559
3503.730817	508323.048083	47.232564
3503.417995	508333.216559	47.237569
3503.523968	508324.092696	47.242573
3503.594448	508319.983358	47.247578
3503.553119	508348.171377	47.252583
3503.710882	508334.991728	47.257588
3503.711829	508332.057070	47.262593
3503.885128	508331.118977	47.267597
3503.715094	508315.562555	47.272602
3503.654994	508303.479814	47.277607
3503.711258	508287.027482	47.282612
3503.576773	508290.438627	47.287617
3503.706862	508276.757355	47.292621
3504.008467	508284.703748	47.297626
3503.844912	508296.062940	47.302631
3503.874717	508281.385617	47.307636
3503.605011	508266.755619	47.312641
3503.250671	508257.502091	47.317645
3503.704822	508250.903522	47.322650
3503.606444	508242.672035	47.327655
3503.638382	508247.878319	47.332660
3503.470029	508260.806749	47.337665
3503.782065	508255.799098	47.342669
3503.529252	508265.603962	47.347674
3503.619750	508256.178937	47.352679
3503.973720	508249.697391	47.357684
3503.842639	508245.417511	47.362689
3503.811742	508223.919357	47.367693
3503.718302	508222.770438	47.372698
3503.846756	508212.833436	47.377703
3503.985857	508207.347149	47.382708
3503.509484	508232.264813	47.387713
3503.800310	508218.861663	47.392717
3503.972203	508197.887975	47.397722
3503.788341	508182.384214	47.402727
3503.421579	508166.302199	47.407732
3503.629566	508176.135475	47.412737
3503.552480	508175.540521	47.417741
3503.643188	508177.195847	47.422746
3503.537689	508172.152972	47.427751
3503.793079	508171.910234	47.432756
3503.309473	508193.540383	47.437761
3503.695053	508169.244178	47.442765
3503.872810	508160.918413	47.447770
3503.602262	508138.699094	47.452775
3503.615831	508142.289252	47.457780
3503.665016	508137.829067	47.462785
3503.800109	508120.048629	47.467789
3503.636065	508136.265194	47.472794
3503.498936	508147.164946	47.477799
3503.887666	508128.231325	47.482804
3503.571931	508135.212847	47.487809
3503.625960	508134.495976	47.492813
3503.401759	508107.918062	47.497818
3503.449634	508096.577047	47.502823
3503.525749	508093.428085	47.507828
3503.430935	508088.029326	47.512833
3503.709214	508086.669861	47.517837
3503.757635	508096.983765	47.522842
3503.716743	508098.862282	47.527847
3503.856400	508099.497963	47.532852
3503.521685	508094.390101	47.537857
3503.381109	508091.831941	47.542861
3503.368897	508107.569173	47.547866
3503.688633	508095.325062	47.552871
3503.566350	508094.180693	47.557876
3503.424787	508091.217923	47.562881
3503.569033	508100.099996	47.567885
3503.427177	508096.631315	47.572890
3503.118382	508103.864732	47.577895
3503.622893	508094.424780	47.582900
3503.140180	508104.569645	47.587905
3503.203100	508097.982256	47.592909
3503.445455	508088.988501	47.597914
3503.075236	508114.243728	47.602919
3503.387867	508083.634461	47.607924
3503.205488	508109.264774	47.612929
3503.298124	508096.601195	47.617933
3503.446906	508120.458894	47.622938
3503.416606	508112.621350	47.627943
3503.771266	508102.243767	47.632948
3503.589542	508111.683312	47.637953
3503.521757	508106.179095	47.642957
3503.483622	508097.229675	47.647962
3503.291381	508116.587655	47.652967
3503.441866	508108.417962	47.657972
3503.500360	508107.902768	47.662977
3503.570321	508103.945248	47.667981
3503.782268	508091.313403	47.672986
3503.416432	508082.061598	47.677991
3503.695094	508069.672172	47.682996
3503.730330	508069.565420	47.688001
3503.313256	508082.533294	47.693005
3503.769173	508068.193210	47.698010
3503.620227	508065.332793	47.703015
3503.519854	508060.440863	47.708020
3503.582543	508077.633566	47.713025
3503.586591	508082.034775	47.718029
3503.616651	508071.404900	47.723034
3503.345577	508068.664978	47.728039
3503.630222	508071.908732	47.733044
3503.843291	508080.375171	47.738049
3503.750463	508052.966875	47.743053
3503.942835	508036.745772	47.748058
3503.964480	508040.132291	47.753063
3503.703248	508030.712137	47.758068
3503.607563	508032.649917	47.763073
3503.939633	508031.484330	47.768077
3503.977431	508017.362075	47.773082
3504.043252	508001.312729	47.778087
3503.918896	507990.960191	47.783092
3503.871508	507993.497495	47.788097
3503.896472	507987.422023	47.793101
3503.964787	507964.744154	47.798106
3503.575764	507960.859144	47.803111
3503.870426	507946.392657	47.808116
3503.555577	507952.665765	47.813121
3503.578637	507939.658893	47.818125
3503.734591	507942.518240	47.823130
3503.632777	507954.373861	47.828135
3503.868696	507935.818355	47.833140
3503.961807	507911.669205	47.838145
3503.764370	507917.367209	47.843149
3503.790449	507905.169375	47.848154
3503.508156	507903.594916	47.853159
3503.830555	507904.100530	47.858164
3503.549168	507906.219463	47.863169
3503.720908	507900.677323	47.868173
3503.989328	507887.024476	47.873178
3503.770763	507872.487253	47.878183
3503.718124	507864.298951	47.883188
3503.595735	507865.532619	47.888193
3503.967036	507849.890220	47.893197
3503.695545	507848.415241	47.898202
3503.575942	507861.892827	47.903207
3503.689406	507852.818127	47.908212
3503.666154	507844.119207	47.913217
3503.852515	507848.086888	47.918221
3503.979268	507833.444458	47.923226
3503.835735	507844.547800	47.928231
3503.664222	507838.199750	47.933236
3503.810844	507839.998061	47.938241
3503.655031	507803.846117	47.943245
3504.117954	507798.207327	47.948250
3503.514539	507796.177644	47.953255
3504.198799	507786.709116	47.958260
3503.548009	507788.380480	47.963265
3503.674073	507789.979659	47.968269
3503.936711	507789.836965	47.973274
3503.251419	507772.540007	47.978279
3503.521409	507757.773681	47.983284
3503.684347	507755.116903	47.988289
3503.394423	507744.840982	47.993293
3503.596448	507754.523651	47.998298
3503.661115	507748.138240	48.003303
3503.691905	507739.886097	48.008308
3503.522414	507752.005538	48.013313
3503.390110	507753.696152	48.018317
3503.719245	507742.411645	48.023322
3503.553018	507749.268499	48.028327
3503.849148	507749.677076	48.033332
3503.952947	507748.598146	48.038337
3503.718435	507729.408414	48.043341
3503.614618	507706.302039	48.048346
3503.396706	507711.042004	48.053351
3503.597234	507709.694799	48.058356
3503.606990	507702.913274	48.063361
3503.227260	507713.446867	48.068365
3503.644620	507700.529287	48.073370
3503.377641	507704.568652	48.078375
3503.507353	507709.506661	48.083380
3503.621826	507716.319163	48.088385
3503.611033	507710.907006	48.093389
3503.594838	507704.180180	48.098394
3503.447217	507714.828878	48.103399
3503.690167	507715.701234	48.108404
3503.393185	507703.453123	48.113409
3503.608521	507694.868210	48.118413
3503.812684	507682.945655	48.123418
3503.693267	507669.859904	48.128423
3503.627204	507674.727671	48.133428
3503.435079	507673.644910	48.138433
3503.618795	507654.388993	48.143437
3503.735782	507657.709921	48.148442
3503.439697	507668.483306	48.153447
3503.882064	507666.440114	48.158452
3503.611825	507670.985972	48.163457
3503.704814	507670.768896	48.168461
3503.629885	507641.889804	48.173466
3503.435089	507644.855234	48.178471
3503.639176	507632.730268	48.183476
3503.674266	507637.278475	48.188481
3503.684714	507629.130689	48.193485
3503.572968	507621.204600	48.198490
3503.517386	507632.041191	48.203495
3503.615761	507623.980700	48.208500
3503.752074	507634.432781	48.213505
3503.488162	507637.307941	48.218509
3503.704739	507633.175350	48.223514
3503.513757	507619.594900	48.228519
3503.646432	507589.013200	48.233524
3503.441701	507590.563485	48.238529
3503.318985	507599.892788	48.243533
3503.670386	507582.735375	48.248538
3503.365512	507589.411815	48.253543
3503.584613	507604.252794	48.258548
3503.621663	507584.615202	48.263553
3503.403598	507606.052324	48.268557
3503.856923	507591.206283	48.273562
3503.573022	507585.736057	48.278567
3503.611975	507611.028543	48.283572
3503.632554	507580.565739	48.288577
3503.662088	507599.231482	48.293581
3503.721075	507589.102711	48.298586
3503.255800	507568.077171	48.303591
3503.794255	507578.769312	48.308596
3503.848693	507558.116995	48.313601
3503.747050	507553.882887	48.318605
3503.664441	507547.723069	48.323610
3503.459618	507558.279709	48.328615
3503.544676	507551.081444	48.333620
3503.301311	507561.138200	48.338625
3503.320931	507552.078175	48.343629
3503.493943	507549.672761	48.348634
3503.270185	507570.554256	48.353639
3503.657121	507557.186001	48.358644
3503.415304	507539.565731	48.363649
3503.467586	507568.094410	48.368653
3503.514137	507553.059640	48.373658
3503.515333	507566.214779	48.378663
3503.448620	507553.070012	48.383668
3503.213863	507558.318656	48.388673
3503.282458	507560.230523	48.393677
3503.635994	507556.936424	48.398682
3503.393656	507573.671864	48.403687
3503.408503	507567.091871	48.408692
3503.564449	507561.096743	48.413697
3503.614761	507572.979180	48.418701
3503.486936	507572.948794	48.423706
3503.687449	507574.789213	48.428711
3503.910281	507552.946537	48.433716
3503.842291	507523.054202	48.438721
3503.589058	507519.248824	48.443725
3504.120742	507511.069199	48.448730
3504.020918	507523.076594	48.453735
3503.728151	507503.491037	48.458740
3503.793999	507489.616905	48.463745
3503.818579	507483.490720	48.468749
3503.929061	507457.719067	48.473754
3503.733266	507477.078324	48.478759
3503.746484	507480.567480	48.483764
3503.739405	507477.127969	48.488769
3503.736785	507447.933539	48.493773
3503.650605	507449.718088	48.498778
3503.388027	507448.039275	48.503783
3503.705563	507424.562342	48.508788
3503.715462	507437.513813	48.513793
3503.694580	507433.772889	48.518797
3503.882306	507430.606167	48.523802
3503.569713	507435.361171	48.528807
3503.813352	507431.072462	48.533812
3503.624283	507414.911063	48.538817
3503.832005	507400.761448	48.543821
3503.833412	507386.998615	48.548826
3503.493643	507395.249179	48.553831
3503.822285	507385.027073	48.558836
3503.779263	507389.182908	48.563841
3504.049558	507388.836610	48.568845
3503.753071	507368.239530	48.573850
3504.052639	507352.355029	48.578855
3504.323197	507345.279155	48.583860
3504.037078	507346.336345	48.588865
3503.944708	507335.016995	48.593869
3504.211332	507313.318890	48.598874
3503.955015	507301.519450	48.603879
3504.191106	507307.402126	48.608884
3503.948855	507280.623398	48.613889
3503.902697	507263.882690	48.618893
3504.083139	507258.136577	48.623898
3503.426557	507270.485134	48.628903
3503.952027	507231.188421	48.633908
3503.800137	507264.455515	48.638913
3503.726702	507231.730035	48.643917
3504.105519	507217.047245	48.648922
3503.657764	507211.906387	48.653927
3503.734398	507218.421476	48.658932
3503.684894	507218.783498	48.663937
3503.551395	507211.518438	48.668941
3503.900587	507212.272831	48.673946
3503.396863	507200.107637	48.678951
3504.188691	507186.928097	48.683956
3503.976932	507181.395741	48.688961
3503.647850	507183.269306	48.693965
3503.787985	507184.765122	48.698970
3504.014689	507183.970323	48.703975
3503.605260	507150.842407	48.708980
3503.649045	507157.413309	48.713985
3503.688056	507143.037156	48.718989
3504.091472	507130.981533	48.723994
3503.493668	507148.633741	48.728999
3503.840172	507143.013140	48.734004
3503.703862	507133.673949	48.739009
3503.394644	507154.215261	48.744013
3503.948261	507112.485100	48.749018
3503.859362	507101.924030	48.754023
3503.825634	507103.396732	48.759028
3503.568791	507080.364305	48.764033
3503.057125	507117.281057	48.769037
3503.541433	507094.435103	48.774042
3503.506328	507097.678979	48.779047
3503.529677	507080.117528	48.784052
3503.221655	507101.063505	48.789057
3503.323042	507086.222057	48.794061
3503.542658	507108.197805	48.799066
3503.391856	507093.902210	48.804071
3503.656168	507107.370304	48.809076
3503.102726	507114.491002	48.814081
3503.363093	507100.687012	48.819085
3503.340545	507114.352235	48.824090
3503.157743	507102.945829	48.829095
3503.343952	507096.692764	48.834100
3503.420815	507097.793797	48.839105
3503.101754	507094.302321	48.844109
3503.363333	507109.693597	48.849114
3503.197400	507105.975528	48.854119
3503.477499	507113.571670	48.859124
3503.419319	507106.497057	48.864129
3503.457394	507103.353928	48.869133
3503.442327	507094.602738	48.874138
3503.593259	507112.035449	48.879143
3503.471972	507111.599239	48.884148
3503.794763	507102.642859	48.889153
3503.355201	507095.223728	48.894157
3503.459500	507104.466819	48.899162
3503.083137	507119.402327	48.904167
3503.474564	507090.043817	48.909172
3503.209480	507099.446489	48.914177
3502.975013	507111.222456	48.919181
3503.427506	507113.782080	48.924186
3503.143739	507105.579351	48.929191
3503.187783	507091.809544	48.934196
3503.553163	507105.717054	48.939201
3503.515439	507117.360724	48.944205
3503.363765	507118.953264	48.949210
3503.430008	507107.962888	48.954215
3503.792626	507108.006783	48.959220
3503.850259	507098.029735	48.964225
3503.552474	507123.730346	48.969229
3503.777991	507103.202245	48.974234
3503.230263	507116.545680	48.979239
3503.555879	507107.740652	48.984244
3503.785503	507120.252842	48.989249
3503.273276	507116.538908	48.994253
3503.789196	507123.692985	48.999258
3503.803105	507124.550973	49.004263
3503.481925	507088.170675	49.009268
3503.472649	507076.028443	49.014273
3503.159723	507071.473418	49.019277
3503.706738	507063.493556	49.024282
3503.434822	507071.531154	49.029287
3503.019178	507082.020207	49.034292
3503.721156	507069.765557	49.039297
3503.705960	507067.541620	49.044301
3503.497907	507083.310737	49.049306
3503.368401	507071.895888	49.054311
3503.547432	507059.420289	49.059316
3503.587134	507081.677500	49.064321
3503.572276	507082.742432	49.069325
3503.531146	507070.099243	49.074330
3502.872588	507085.129979	49.079335
3503.174049	507064.792224	49.084340
3503.302350	507063.000996	49.089345
3503.552619	507078.748279	49.094349
3503.697613	507083.329860	49.099354
3503.934093	507066.139501	49.104359
3503.845447	507068.177473	49.109364
3503.722900	507081.048945	49.114369
3503.783849	507077.446807	49.119373
3503.987216	507052.165859	49.124378
3503.813778	507033.218694	49.129383
3503.607425	507043.877087	49.134388
3503.776749	507039.144637	49.139393
3503.520496	507052.897444	49.144397
3503.849756	507042.371445	49.149402
3503.655344	507045.387515	49.154407
3503.781758	507016.374359	49.159412
3503.492146	507007.211126	49.164417
3503.444659	507001.349155	49.169421
3503.774952	506986.724439	49.174426
3503.706582	506991.289168	49.179431
3503.635695	506984.469508	49.184436
3503.879548	506996.321752	49.189441
3503.547181	506999.056039	49.194445
3503.915481	506994.292129	49.199450
3503.862317	506967.584230	49.204455
3503.835344	506967.689700	49.209460
3503.812630	506953.424343	49.214465
3503.338665	506955.067835	49.219469
3503.867254	506947.141431	49.224474
3503.571695	506945.720777	49.229479
3503.370202	506948.383788	49.234484
3503.595949	506954.420017	49.239489
3503.619413	506943.335100	49.244493
3503.576429	506953.765331	49.249498
3503.614734	506943.943047	49.254503
3503.287652	506936.455471	49.259508
3503.754763	506894.384264	49.264513
3503.639497	506935.489094	49.269517
3503.921102	506892.991810	49.274522
3503.809855	506911.225150	49.279527
3503.517116	506913.447195	49.284532
3503.593309	506903.214106	49.289537
3503.441132	506904.300751	49.294541
3503.828882	506914.713528	49.299546
3503.381517	506914.683044	49.304551
3503.706324	506898.237547	49.309556
3503.751520	506911.538027	49.314561
3503.538672	506892.141544	49.319565
3503.606401	506868.450344	49.324570
3503.573588	506873.920273	49.329575
3503.510350	506866.593364	49.334580
3503.675112	506866.870929	49.339585
3503.668002	506866.011872	49.344589
3503.870500	506861.678926	49.349594
3503.634794	506882.613736	49.354599
3503.643118	506881.802839	49.359604
3503.885588	506880.550141	49.364609
3503.548738	506859.048045	49.369613
3503.763737	506838.622492	49.374618
3503.725115	506835.795033	49.379623
3503.646781	506821.892555	49.384628
3503.404422	506844.042852	49.389633
3503.385304	506839.846126	49.394637
3503.676634	506830.742780	49.399642
3503.442834	506840.241847	49.404647
3503.480489	506834.568761	49.409652
3503.461897	506829.258760	49.414657
3503.392606	506832.052693	49.419661
3503.529319	506832.081694	49.424666
3503.642868	506844.410032	49.429671
3503.570461	506830.709023	49.434676
3503.658077	506843.699253	49.439681
3503.781627	506827.892692	49.444685
3503.975008	506809.190904	49.449690
3503.540077	506801.720315	49.454695
3503.716445	506793.596512	49.459700
3503.964433	506801.400266	49.464705
3503.667235	506809.745578	49.469709
3503.810056	506795.453929	49.474714
3503.743501	506780.486964	49.479719
3503.352563	506763.041270	49.484724
3503.420238	506764.447375	49.489729
3503.572896	506756.782699	49.494733
3503.755462	506762.066824	49.499738
3503.705269	506759.038783	49.504743
3503.344299	506746.850706	49.509748
3503.942748	506750.551111	49.514753
3503.626397	506759.101874	49.519757
3503.639759	506755.405991	49.524762
3503.654096	506748.016172	49.529767
3503.340317	506751.405356	49.534772
3503.757570	506763.027955	49.539777
3503.477483	506747.032116	49.544781
3503.527625	506716.107722	49.549786
3503.304876	506724.694308	49.554791
3503.561372	506719.290196	49.559796
3503.807809	506703.160500	49.564801
3503.882915	506712.307215	49.569805
3503.879035	506704.970856	49.574810
3503.928404	506710.680847	49.579815
3503.556299	506719.797040	49.584820
3503.649820	506706.423906	49.589825
3503.429168	506702.967397	49.594829
3503.620956	506678.446733	49.599834
3503.370824	506672.161279	49.604839
3503.493051	506665.007372	49.609844
3503.772908	506662.837950	49.614849
3503.589785	506668.382300	49.619853
3503.758951	506665.471373	49.624858
3503.470211	506680.950008	49.629863
3503.361964	506667.406334	49.634868
3503.454075	506666.936384	49.639873
3503.414073	506682.982905	49.644877
3503.816713	506664.500888	49.649882
3503.449139	506683.533979	49.654887
3503.184200	506677.200268	49.659892
3503.405690	506680.504867	49.664897
3503.490900	506676.241012	49.669901
3503.825178	506668.243993	49.674906
3503.671652	506675.807663	49.679911
3503.719281	506659.456348	49.684916
3503.409235	506649.587754	49.689921
3503.522039	506640.563125	49.694925
3503.829233	506636.871377	49.699930
3503.553782	506636.965520	49.704935
3503.227388	506641.419321	49.709940
3503.687736	506629.860354	49.714945
3503.207352	506632.365092	49.719949
3503.580792	506628.359271	49.724954
3503.383408	506635.879290	49.729959
3503.649894	506630.220571	49.734964
3503.654420	506638.012277	49.739969
3503.694768	506632.692901	49.744973
3503.835304	506625.030083	49.749978
3503.914867	506635.339936	49.754983
3503.538855	506612.376321	49.759988
3503.858648	506598.461341	49.764993
3503.467693	506600.041145	49.769997
3503.618264	506596.171742	49.775002
3503.593974	506595.062386	49.780007
3503.546609	506584.899237	49.785012
3503.606150	506596.730285	49.790017
3503.407601	506601.265091	49.795021
3503.804483	506584.858507	49.800026
3503.501080	506590.573693	49.805031
3503.669049	506585.993135	49.810036
3503.800981	506586.933696	49.815041
3503.557081	506575.637800	49.820045
3503.767617	506567.356690	49.825050
3503.937027	506565.660114	49.830055
3503.846625	506557.375962	49.835060
3504.018513	506560.789625	49.840065
3503.752665	506546.967163	49.845069
3504.050264	506525.516180	49.850074
3504.041761	506518.534676	49.855079
3503.880556	506510.818297	49.860084
3504.170589	506510.013460	49.865089
3503.702609	506490.555649	49.870093
3503.656512	506475.939392	49.875098
3503.904198	506463.300714	49.880103
3503.944349	506473.161488	49.885108
3503.864428	506470.846502	49.890113
3503.777670	506470.657821	49.895117
3503.722222	506461.659691	49.900122
3503.663761	506448.360980	49.905127
3503.360702	506434.240706	49.910132
3503.858360	506430.114006	49.915137
3503.504121	506429.259190	49.920141
3503.911206	506428.739453	49.925146
3503.679893	506432.571071	49.930151
3503.819132	506433.206882	49.935156
3503.842976	506426.928638	49.940161
3503.582990	506404.857223	49.945165
3503.661829	506399.481091	49.950170
3503.367387	506393.202539	49.955175
3503.433432	506385.045380	49.960180
3503.419095	506389.753530	49.965185
3503.494598	506404.314629	49.970189
3503.749614	506389.751910	49.975194
3503.676175	506391.230949	49.980199
3503.511482	506390.700378	49.985204
3503.660906	506394.269427	49.990209
3503.254245	506399.697390	49.995213
3503.552239	506392.211987	50.000218
3503.375056	506392.239999	50.005223
3503.578426	506392.916276	50.010228
3503.797969	506397.587459	50.015233
3503.607655	506391.545453	50.020237
3503.922970	506381.881474	50.025242
3503.694581	506373.366038	50.030247
3503.570362	506354.258550	50.035252
3503.906836	506343.882793	50.040257
3503.552011	506351.832625	50.045261
3503.725259	506351.602848	50.050266
3503.613596	506352.733725	50.055271
3503.495056	506357.002945	50.060276
3503.810961	506353.410962	50.065281
3503.557139	506353.349885	50.070285
3503.544188	506335.692217	50.075290
3503.447089	506325.840383	50.080295
3503.501734	506301.391464	50.085300
3504.006713	506304.853734	50.090305
3503.298248	506303.042876	50.095309
3503.516801	506304.779379	50.100314
3503.690023	506314.720413	50.105319
3503.642884	506313.715852	50.110324
3503.742815	506307.729145	50.115329
3503.702863	506313.250980	50.120333
3503.833310	506308.524477	50.125338
3503.639611	506293.678389	50.130343
3503.689403	506263.917070	50.135348
3503.428490	506261.934270	50.140353
3503.402435	506269.832177	50.145357
3503.183730	506263.744012	50.150362
3503.424692	506269.525070	50.155367
3503.415461	506261.430352	50.160372
3503.461875	506262.435049	50.165377
3503.418916	506261.429824	50.170381
3503.363884	506259.718090	50.175386
3503.522897	506263.639858	50.180391
3503.659729	506266.654311	50.185396
3503.816066	506258.482823	50.190401
3503.464283	506265.622594	50.195405
3503.507247	506259.189464	50.200410
3503.694240	506270.747584	50.205415
3503.575335	506258.470304	50.210420
3503.639619	506264.380489	50.215425
3503.521923	506268.953204	50.220429
3503.555653	506267.328645	50.225434
3503.431842	506267.550626	50.230439
3503.480633	506271.287409	50.235444
3503.826159	506247.197249	50.240449
3503.781263	506250.392229	50.245453
3503.956432	506236.803425	50.250458
3503.642334	506230.224313	50.255463
3503.408942	506227.073329	50.260468
3503.635822	506227.594094	50.265473
3503.506402	506229.031393	50.270477
3503.811309	506209.805322	50.275482
3503.623989	506235.641590	50.280487
3503.665237	506205.527313	50.285492
3503.692655	506184.017409	50.290497
3503.358713	506180.275092	50.295501
3503.299024	506188.785568	50.300506
3503.729763	506180.924885	50.305511
3503.337015	506176.989456	50.310516
3503.646563	506180.179031	50.315521
3503.518754	506188.042456	50.320525
3503.469045	506183.648000	50.325530
3503.577843	506183.226002	50.330535
3503.696598	506172.783351	50.335540
3504.114395	506175.348601	50.340545
3503.490440	506179.748346	50.345549
3503.894943	506170.474965	50.350554
3503.840375	506153.177899	50.355559
3503.275105	506150.990181	50.360564
3503.830984	506147.309627	50.365569
3503.732786	506154.004553	50.370573
3503.805610	506133.044026	50.375578
3503.872542	506146.341657	50.380583
3503.562789	506156.612123	50.385588
3503.913022	506132.672865	50.390593
3503.520340	506117.554467	50.395597
3503.756376	506100.717435	50.400602
3503.864337	506099.030526	50.405607
3503.765893	506090.899228	50.410612
3503.890229	506096.698776	50.415617
3503.466652	506107.493277	50.420621
3503.712828	506099.358117	50.425626
3503.653378	506083.124387	50.430631
3503.573679	506065.274587	50.435636
3503.720761	506057.509282	50.440641
3503.781279	506058.359956	50.445645
3503.706020	506063.229627	50.450650
3503.889442	506063.099443	50.455655
3503.769839	506066.761680	50.460660
3504.038097	506060.950692	50.465665
3503.593487	506043.765765	50.470669
3503.738305	506016.316687	50.475674
3503.497760	506017.670362	50.480679
3503.576581	506021.503656	50.485684
3503.563093	506021.758806	50.490689
3503.179656	506024.298908	50.495693
3503.503725	506017.517649	50.500698
3503.573435	506023.123448	50.505703
3503.607304	506007.988140	50.510708
3503.440693	506013.530088	50.515713
3503.460782	506016.107618	50.520717
3503.682964	506008.229218	50.525722
3503.666250	506010.205342	50.530727
3503.622219	505995.942568	50.535732
3503.834945	505965.345356	50.540737
3503.317999	505933.952576	50.545741
3503.490063	505885.802706	50.550746
3503.276055	505846.316127	50.555751
3503.260009	505772.236635	50.560756
3503.402474	505687.555785	50.565761
3502.922295	505608.691080	50.570765
3503.136856	505508.817041	50.575770
3502.960391	505408.650007	50.580775
3502.791851	505296.791632	50.585780
3502.647283	505176.477833	50.590785
3502.407825	505042.565540	50.595789
3502.431018	504892.568888	50.600794
3502.310093	504747.198834	50.605799
3501.836398	504583.159106	50.610804
3501.970593	504400.499771	50.615809
3501.384868	504236.170860	50.620813
3501.237478	504051.426898	50.625818
3500.843285	503857.812972	50.630823
3500.739509	503665.568056	50.635828
3500.502641	503459.981230	50.640833
3500.320095	503248.715113	50.645837
3500.393546	503028.903439	50.650842
3499.991132	502797.726116	50.655847
3499.264868	502558.853339	50.660852
3499.315784	502320.310011	50.665857
3498.819381	502087.164360	50.670861
3498.550992	501815.361176	50.675866
3498.166388	501557.845551	50.680871
3498.051385	501299.979887	50.685876
3497.782869	501020.774704	50.690881
3497.168115	500747.542058	50.695885
3497.156279	500453.051677	50.700890
3496.627029	500145.578590	50.705895
3495.975070	499846.724937	50.710900
3496.018821	499552.868993	50.715905
3495.212617	499242.032586	50.720909
3495.125265	498918.219143	50.725914
3494.698857	498601.540689	50.730919
3494.196678	498270.491424	50.735924
3493.973580	497939.594469	50.740929
3493.057203	497609.864168	50.745933
3492.996667	497261.260659	50.750938
3492.650740	496916.695146	50.755943
3491.967113	496561.392533	50.760948
3491.968619	496209.974434	50.765953
3491.138193	495854.529320	50.770957
3490.292425	495478.016878	50.775962
3490.263419	495119.646025	50.780967
3489.840345	494749.836564	50.785972
3489.695532	494358.607741	50.790977
3489.033979	493986.997734	50.795981
3488.441468	493595.317060	50.800986
3488.141266	493206.518863	50.805991
3487.090370	492825.528277	50.810996
3486.997081	492411.968749	50.816001
3486.329195	492021.178133	50.821005
3485.822677	491615.110418	50.826010
3485.259470	491210.410171	50.831015
3484.619055	490794.166357	50.836020
3484.174019	490378.540775	50.841025
3483.420733	489973.134703	50.846029
3482.806128	489544.399859	50.851034
3482.405523	489128.587587	50.856039
3481.437934	488717.718170	50.861044
3481.581521	488287.821846	50.866049
3480.748685	487871.290393	50.871053
3480.194883	487444.169707	50.876058
3479.480887	487013.164302	50.881063
3478.902944	486581.165155	50.886068
3478.374962	486149.452255	50.891073
3477.619212	485709.558952	50.896077
3477.539719	485273.246780	50.901082
3476.789267	484827.557200	50.906087
3475.603897	484394.743452	50.911092
3475.363014	483944.342636	50.916097
3474.532458	483498.178972	50.921101
3473.956850	483052.572695	50.926106
3473.673010	482610.608702	50.931111
3473.043096	482167.524000	50.936116
3472.394839	481698.743046	50.941121
3471.525875	481264.289282	50.946125
3471.178855	480799.999430	50.951130
3470.830329	480346.542691	50.956135
3469.620738	479888.194916	50.961140
3469.368685	479425.327087	50.966145
3468.745008	478957.338204	50.971149
3468.158831	478501.545487	50.976154
3467.471103	478035.977447	50.981159
3466.437401	477572.024245	50.986164
3465.931368	477097.384576	50.991169
3465.094653	476652.789507	50.996173
3464.883720	476179.247067	51.001178
3463.974295	475707.780540	51.006183
3463.064799	475243.398907	51.011188
3462.792976	474784.582656	51.016193
3462.326508	474313.976538	51.021197
3461.394484	473844.193405	51.026202
3460.473180	473378.757038	51.031207
3459.688500	472901.933609	51.036212
3458.965094	472443.693423	51.041217
3458.030099	471990.495059	51.046221
3457.786595	471520.143993	51.051226
3456.847326	471062.363286	51.056231
3456.126075	470600.583584	51.061236
3455.736090	470136.966754	51.066241
3455.323669	469673.799375	51.071245
3454.649832	469205.085949	51.076250
3453.686029	468730.729234	51.081255
3452.941335	468270.016772	51.086260
3452.488078	467790.893353	51.091265
3451.516752	467343.480670	51.096269
3451.061226	466877.621388	51.101274
3450.564160	466396.850494	51.106279
3449.330744	465944.328082	51.111284
3448.606452	465476.502732	51.116289
3448.145697	465013.848568	51.121293
3447.265683	464546.838713	51.126298
3446.389850	464084.584944	51.131303
3446.065610	463625.885359	51.136308
3445.728375	463169.155880	51.141313
3444.462759	462709.824791	51.146317
3443.780973	462240.958257	51.151322
3443.384423	461782.027892	51.156327
3442.420648	461333.777745	51.161332
3441.924463	460867.590929	51.166337
3441.032766	460404.144865	51.171341
3440.436402	459935.012083	51.176346
3439.705266	459491.607282	51.181351
3439.012483	459028.709276	51.186356
3438.558817	458562.060753	51.191361
3437.769326	458102.354239	51.196365
3436.925697	457644.625086	51.201370
3436.655244	457176.345751	51.206375
3435.170573	456736.149820	51.211380
3434.854489	456275.315966	51.216385
3434.155135	455825.288311	51.221389
3433.193682	455365.450874	51.226394
3432.649258	454916.445843	51.231399
3431.871990	454474.064175	51.236404
3431.295071	454002.164633	51.241409
3430.144941	453562.766715	51.246413
3429.697231	453109.651482	51.251418
3428.771089	452660.306779	51.256423
3428.337392	452220.465184	51.261428
3427.668349	451771.113043	51.266433
3426.990576	451324.239805	51.271437
3426.025620	450876.794346	51.276442
3425.477571	450429.883197	51.281447
3424.235006	449995.860862	51.286452
3423.809253	449548.456610	51.291457
3423.121163	449113.467389	51.296461
3422.391937	448675.634659	51.301466
3421.624090	448235.262373	51.306471
3420.884360	447794.065344	51.311476
3420.314180	447364.607311	51.316481
3419.730491	446931.895466	51.321485
3419.063783	446485.130382	51.326490
3418.368760	446052.166219	51.331495
3417.200594	445616.934237	51.336500
3417.004012	445184.636728	51.341505
3416.208668	444754.050217	51.346509
3415.543036	444330.693670	51.351514
3414.844115	443885.965807	51.356519
3413.923318	443457.558359	51.361524
3413.328298	443020.259570	51.366529
3412.342595	442597.836720	51.371533
3411.623458	442156.887130	51.376538
3410.917820	441749.278312	51.381543
3409.974917	441318.044461	51.386548
3409.500131	440901.095231	51.391553
3408.926859	440477.402692	51.396557
3408.082487	440061.106737	51.401562
3407.520383	439643.286851	51.406567
3406.795232	439221.322694	51.411572
3406.193417	438793.138051	51.416577
3405.376294	438373.560064	51.421581
3404.702180	437942.630588	51.426586
3404.265398	437533.005386	51.431591
3403.053958	437109.203610	51.436596
3402.578345	436688.832405	51.441601
3401.597392	436283.436115	51.446605
3401.063517	435869.737125	51.451610
3400.414051	435457.192057	51.456615
3399.658562	435044.910888	51.461620
3399.280181	434624.667556	51.466625
3397.930895	434223.815561	51.471629
3397.528253	433799.220907	51.476634
3396.874079	433401.445122	51.481639
3396.020095	432986.607186	51.486644
3395.466713	432571.207199	51.491649
3394.391127	432166.648824	51.496653
3393.865032	431763.698438	51.501658
3393.332060	431362.317144	51.506663
3392.706350	430967.647813	51.511668
3392.116116	430552.449725	51.516673
3391.239387	430150.951705	51.521677
3390.191345	429738.580866	51.526682
3389.758552	429334.435392	51.531687
3388.955474	428934.303720	51.536692
3388.366582	428537.357198	51.541697
3387.718494	428144.705795	51.546701
3387.007916	427736.668931	51.551706
3386.161830	427346.703504	51.556711
3385.396619	426939.856630	51.561716
3384.824785	426532.287271	51.566721
3383.973530	426152.082800	51.571725
3383.606324	425755.847011	51.576730
3382.831050	425354.793581	51.581735
3381.667479	424968.323161	51.586740
3381.224805	424571.319953	51.591745
3380.396401	424177.419751	51.596749
3379.851198	423785.856563	51.601754
3379.202481	423402.482699	51.606759
3378.286331	423018.840942	51.611764
3377.815014	422617.826039	51.616769
3376.914876	422231.452925	51.621773
3376.374792	421853.044102	51.626778
3375.992180	421453.014237	51.631783
3374.976613	421074.568330	51.636788
3374.556124	420680.070820	51.641793
3373.220249	420292.317023	51.646797
3372.777336	419908.404845	51.651802
3372.187718	419529.819799	51.656807
3371.526216	419149.462782	51.661812
3370.927272	418760.351899	51.666817
3370.045031	418377.961675	51.671821
3369.370653	417994.999921	51.676826
3368.870615	417594.577860	51.681831
3367.694350	417224.438189	51.686836
3367.433421	416830.496647	51.691841
3366.572809	416465.988018	51.696845
3365.784112	416090.564225	51.701850
3365.557156	415707.780504	51.706855
3364.372595	415338.888104	51.711860
3364.003422	414943.896148	51.716865
3363.022472	414579.611346	51.721869
3362.339719	414196.142887	51.726874
3362.033320	413819.901955	51.731879
3360.942418	413450.208519	51.736884
3360.407575	413067.819824	51.741889
3359.825545	412698.112670	51.746893
3358.919837	412315.391700	51.751898
3358.358177	411952.151334	51.756903
3357.712943	411573.241827	51.761908
3357.247795	411205.454092	51.766913
3356.094640	410828.343301	51.771917
3355.711199	410448.082144	51.776922
3355.091809	410076.213744	51.781927
3353.860565	409720.065543	51.786932
3353.408487	409343.892502	51.791937
3352.918974	408969.423306	51.796941
3352.234952	408606.974891	51.801946
3351.595229	408224.845704	51.806951
3350.160530	407858.923877	51.811956
3349.934409	407486.986902	51.816961
3349.160999	407138.588736	51.821965
3348.340567	406760.891795	51.826970
3347.980203	406393.791454	51.831975
3346.938468	406049.133865	51.836980
3346.653463	405673.473775	51.841985
3345.540835	405323.685534	51.846989
3345.244109	404951.881676	51.851994
3344.460064	404589.935501	51.856999
3343.736421	404227.543519	51.862004
3343.197149	403865.321529	51.867009
3342.280615	403507.475848	51.872013
3341.463542	403147.551617	51.877018
3341.090400	402780.893796	51.882023
3340.305337	402424.972213	51.887028
3339.731413	402065.963134	51.892033
3339.062473	401704.219898	51.897037
3338.607188	401355.173364	51.902042
3337.675570	400983.575814	51.907047
3336.535410	400648.152599	51.912052
3336.443680	400261.747231	51.917057
3335.484562	399915.408382	51.922061
3334.668768	399558.697352	51.927066
3334.017838	399200.075266	51.932071
3333.431880	398850.514007	51.937076
3333.011735	398488.110843	51.942081
3332.106995	398130.254381	51.947085
3331.473266	397768.995591	51.952090
3330.620659	397413.105955	51.957095
3329.943618	397058.684612	51.962100
3329.510922	396700.153345	51.967105
3328.700612	396363.668129	51.972109
3328.124431	395998.084649	51.977114
3327.803117	395640.897227	51.982119
3326.805708	395288.846682	51.987124
3326.125148	394927.157789	51.992129
3325.580723	394588.095863	51.997133
3324.542267	394219.871327	52.002138
3323.776684	393865.633738	52.007143
3323.496806	393517.773442	52.012148
3322.957338	393157.950264	52.017153
3322.164959	392810.824885	52.022157
3321.197166	392456.986098	52.027162
3320.569411	392097.547185	52.032167
3319.684175	391760.901191	52.037172
3319.136182	391414.663908	52.042177
3318.328168	391064.091016	52.047181
3317.784823	390719.676788	52.052186
3316.897058	390357.820130	52.057191
3315.997116	390024.541490	52.062196
3315.481846	389672.382802	52.067201
3314.980635	389334.966264	52.072205
3314.132860	389002.966551	52.077210
3313.605550	388648.205995	52.082215
3312.588037	388310.403698	52.087220
3312.412033	387967.710037	52.092225
3311.993855	387622.737408	52.097229
3310.604122	387275.524813	52.102234
3310.441800	386924.122411	52.107239
3309.632478	386581.337746	52.112244
3308.930430	386237.235980	52.117249
3308.243187	385895.366449	52.122253
3307.249079	385553.796557	52.127258
3306.734195	385215.046749	52.132263
3306.275197	384885.821423	52.137268
3305.528439	384541.227656	52.142273
3304.737660	384205.182449	52.147277
3304.079661	383861.407556	52.152282
3303.642458	383508.032359	52.157287
3302.834931	383184.111391	52.162292
3302.127776	382833.290259	52.167297
3301.672636	382491.937615	52.172301
3300.825140	382159.697852	52.177306
3300.367605	381806.182740	52.182311
3299.337192	381467.277075	52.187316
3298.864722	381129.450079	52.192321
3298.026250	380789.897656	52.197325
3297.501965	380440.195449	52.202330
3296.786928	380101.380428	52.207335
3295.975337	379774.226446	52.212340
3295.586484	379430.470651	52.217345
3294.835816	379096.993657	52.222349
3294.080346	378751.204231	52.227354
3293.659725	378413.879456	52.232359
3292.686087	378073.129210	52.237364
3291.952589	377731.371498	52.242369
3291.341322	377399.740252	52.247373
3290.789719	377052.937131	52.252378
3290.220667	376705.396106	52.257383
3289.348031	376379.800569	52.262388
3288.863576	376031.146553	52.267393
3288.144758	375697.534144	52.272397
3287.171299	375359.126264	52.277402
3286.602474	375025.815264	52.282407
3285.516523	374695.432277	52.287412
3284.929564	374364.331757	52.292417
3284.288824	374029.395985	52.297421
3283.468926	373702.982036	52.302426
3283.002210	373366.690572	52.307431
3282.321914	373046.201834	52.312436
3281.740734	372717.122200	52.317441
3281.064905	372384.824229	52.322445
3280.249632	372062.822940	52.327450
3279.685312	371720.860746	52.332455
3278.878732	371398.980177	52.337460
3278.230104	371060.892710	52.342465
3277.557242	370741.835193	52.347469
3276.669096	370417.161692	52.352474
3276.558465	370086.206267	52.357479
3275.675548	369755.523066	52.362484
3274.652693	369431.473942	52.367489
3274.088353	369106.662963	52.372493
3273.315979	368787.377645	52.377498
3272.971744	368458.990723	52.382503
3272.164050	368137.620051	52.387508
3271.540321	367802.962985	52.392513
3270.973356	367485.950795	52.397517
3269.895405	367160.137983	52.402522
3269.745416	366820.590021	52.407527
3268.776295	366501.802543	52.412532
3268.234110	366174.447532	52.417537
3267.580553	365847.107731	52.422541
3266.673788	365529.931751	52.427546
3266.295622	365206.868961	52.432551
3265.275713	364885.457377	52.437556
3264.764706	364551.343198	52.442561
3264.049294	364243.821761	52.447565
3263.373084	363916.725968	52.452570
3262.907434	363580.892775	52.457575
3261.865984	363269.421681	52.462580
3261.254825	362951.850175	52.467585
3260.788862	362630.411439	52.472589
3260.218405	362309.317779	52.477594
3259.434348	361978.841183	52.482599
3259.035758	361660.871003	52.487604
3258.255098	361323.366480	52.492609
3257.418368	361013.323709	52.497613
3256.527685	360692.778526	52.502618
3256.233460	360362.671116	52.507623
3255.487086	360047.187846	52.512628
3254.905521	359717.070523	52.517633
3254.370136	359403.559857	52.522637
3253.341714	359075.646269	52.527642
3252.712815	358742.705225	52.532647
3251.835925	358431.659670	52.537652
3251.250665	358106.544887	52.542657
3250.764542	357789.198992	52.547661
3250.186246	357468.710196	52.552666
3249.636101	357147.909496	52.557671
3249.055960	356824.541279	52.562676
3247.872526	356495.260769	52.567681
3247.396041	356170.294158	52.572685
3246.873882	355852.610740	52.577690
3246.078846	355528.199309	52.582695
3245.146103	355222.257483	52.587700
3244.395323	354890.836719	52.592705
3244.133457	354571.806214	52.597709
3243.137744	354258.310349	52.602714
3242.624951	353942.903868	52.607719
3241.979289	353616.522526	52.612724
3241.230552	353309.216803	52.617729
3240.375624	352987.165491	52.622733
3239.381517	352675.084921	52.627738
3239.130738	352352.552388	52.632743
3238.066838	352053.992873	52.637748
3237.787051	351743.829753	52.642753
3237.113147	351430.596806	52.647757
3236.223051	351122.715291	52.652762
3235.671499	350799.126512	52.657767
3235.092261	350486.534756	52.662772
3234.208751	350183.864146	52.667777
3233.697632	349867.898549	52.672781
3233.065784	349554.800708	52.677786
3232.452971	349238.771187	52.682791
3231.502679	348933.711782	52.687796
3230.985123	348611.097169	52.692801
3230.305667	348306.984050	52.697805
3229.526168	348002.834184	52.702810
3228.843832	347686.043216	52.707815
3227.937628	347381.833649	52.712820
3227.511398	347075.026756	52.717825
3227.058884	346761.299361	52.722829
3226.424574	346462.743108	52.727834
3225.831753	346146.183845	52.732839
3224.831797	345837.501173	52.737844
3224.068341	345524.274295	52.742849
3223.698527	345218.568398	52.747853
3222.656634	344909.021984	52.752858
3222.208312	344597.827384	52.757863
3221.307981	344294.287700	52.762868
3220.907586	343993.874487	52.767873
3220.049433	343687.092410	52.772877
3219.294726	343381.514153	52.777882
3219.260197	343070.678735	52.782887
3218.274608	342773.177273	52.787892
3217.473575	342455.689166	52.792897
3216.721046	342153.158770	52.797901
3215.725071	341856.901676	52.802906
3215.229477	341549.796758	52.807911
3214.739663	341241.518470	52.812916
3214.182809	340936.278344	52.817921
3213.644504	340631.364683	52.822925
3212.721771	340330.303117	52.827930
3212.418088	340021.760197	52.832935
3211.517211	339718.553992	52.837940
3210.934527	339410.790395	52.842945
3210.489353	339096.817872	52.847949
3209.567256	338792.312340	52.852954
3208.953941	338469.708423	52.857959
3208.054346	338170.923894	52.862964
3207.425807	337863.821920	52.867969
3206.985032	337559.005283	52.872973
3206.075978	337265.105620	52.877978
3205.539096	336951.162574	52.882983
3204.682100	336651.676989	52.887988
3204.209992	336343.193917	52.892993
3203.654423	336044.319762	52.897997
3202.651841	335734.899513	52.903002
3202.420651	335427.748746	52.908007
3201.424035	335128.889354	52.913012
3200.723689	334812.543657	52.918017
3200.567420	334511.893889	52.923021
3199.793774	334205.561649	52.928026
3198.885620	333897.136351	52.933031
3198.363662	333587.808477	52.938036
3197.621305	333284.623929	52.943041
3196.867018	332977.417619	52.948045
3196.197329	332674.677166	52.953050
3195.423824	332368.184049	52.958055
3194.726880	332062.543069	52.963060
3194.073470	331759.159668	52.968065
3193.506224	331459.758306	52.973069
3192.764932	331168.911805	52.978074
3192.567704	330852.672278	52.983079
3191.737238	330549.795508	52.988084
3190.801923	330237.794377	52.993089
3190.405169	329932.096894	52.998093
3189.208011	329632.227577	53.003098
3188.659430	329315.960641	53.008103
3188.211847	329023.506173	53.013108
3187.500961	328720.755758	53.018113
3186.691244	328409.872764	53.023117
3185.753588	328116.015668	53.028122
3185.603600	327809.073906	53.033127
3184.601930	327524.441033	53.038132
3183.633336	327220.019638	53.043137
3183.098528	326921.460573	53.048141
3182.215749	326634.183261	53.053146
3182.200127	326328.283709	53.058151
3181.193334	326045.148397	53.063156
3180.765244	325735.849231	53.068161
3179.914475	325453.781925	53.073165
3178.998355	325145.703405	53.078170
3178.808802	324843.797516	53.083175
3177.989761	324546.522086	53.088180
3177.130839	324253.478364	53.093185
3176.614260	323953.250412	53.098189
3175.782313	323656.610330	53.103194
3175.501077	323350.919797	53.108199
3174.556847	323067.815174	53.113204
3173.676078	322763.083031	53.118209
3173.160515	322470.818954	53.123213
3172.412983	322189.666259	53.128218
3171.669645	321885.749465	53.133223
3171.145540	321596.971982	53.138228
3170.492755	321303.630811	53.143233
3169.993375	321003.924426	53.148237
3169.011134	320705.872044	53.153242
3168.524591	320411.355820	53.158247
3167.827992	320121.913321	53.163252
3167.210486	319836.403990	53.168257
3166.562414	319540.382743	53.173261
3165.756669	319247.109932	53.178266
3165.496739	318944.557949	53.183271
3164.640057	318654.601401	53.188276
3164.092182	318355.810551	53.193281
3163.341600	318067.388595	53.198285
3162.668119	317768.233807	53.203290
3162.347267	317463.293182	53.208295
3161.465152	317174.660154	53.213300
3160.740656	316869.475945	53.218305
3160.365608	316566.476222	53.223309
3159.319394	316270.787770	53.228314
3158.718104	315967.109020	53.233319
3158.047702	315672.810707	53.238324
3157.388793	315378.153221	53.243329
3156.753189	315075.342929	53.248333
3155.744945	314791.000699	53.253338
3155.042596	314480.738425	53.258343
3153.828622	314200.654032	53.263348
3153.417211	313911.758819	53.268353
3153.433633	313623.049751	53.273357
3152.299226	313334.190939	53.278362
3151.631180	313038.917066	53.283367
3151.281261	312752.835421	53.288372
3150.495782	312458.724397	53.293377
3150.066020	312173.035802	53.298381
3149.002316	311883.805398	53.303386
3148.441698	311588.052207	53.308391
3147.811126	311304.226538	53.313396
3147.065707	311005.649044	53.318401
3146.523762	310711.927715	53.323405
3145.710986	310430.191276	53.328410
3145.377366	310132.081075	53.333415
3144.550599	309847.569792	53.338420
3143.940498	309553.601631	53.343425
3143.311104	309261.723886	53.348429
3142.417391	308972.611965	53.353434
3141.806566	308661.453013	53.358439
3141.306591	308389.415178	53.363444
3140.314151	308092.091613	53.368449
3139.512429	307798.735146	53.373453
3139.028898	307521.370598	53.378458
3138.290469	307226.194742	53.383463
3137.908645	306938.041077	53.388468
3137.115286	306643.407314	53.393473
3136.452760	306363.292829	53.398477
3135.648884	306077.037496	53.403482
3135.076221	305781.984863	53.408487
3134.422212	305504.770231	53.413492
3133.595398	305210.367701	53.418497
3133.184086	304921.475729	53.423501
3132.576219	304636.230352	53.428506
3131.720641	304344.402507	53.433511
3130.950458	304072.805753	53.438516
3130.416229	303777.640790	53.443521
3129.792491	303493.745249	53.448525
3128.834959	303207.457233	53.453530
3128.636450	302916.210025	53.458535
3127.754304	302631.233159	53.463540
3126.921487	302342.224304	53.468545
3126.513090	302048.334644	53.473549
3125.654586	301771.119519	53.478554
3124.885886	301475.885111	53.483559
3124.168192	301198.060935	53.488564
3123.764792	300916.188326	53.493569
3123.084812	300625.420305	53.498573
3122.200706	300345.379903	53.503578
3121.748414	300058.700356	53.508583
3120.767601	299780.660644	53.513588
3120.134751	299502.463530	53.518593
3119.786862	299218.567292	53.523597
3118.767854	298928.995854	53.528602
3118.090848	298646.398581	53.533607
3117.504233	298367.606532	53.538612
3116.613375	298079.566835	53.543617
3116.277369	297798.518613	53.548621
3115.571135	297524.888419	53.553626
3115.195980	297233.735194	53.558631
3114.228675	296956.783827	53.563636
3113.375527	296668.455751	53.568641
3113.194944	296391.149845	53.573645
3112.273190	296119.054199	53.578650
3111.562819	295825.226840	53.583655
3110.882349	295546.063311	53.588660
3110.257252	295265.056991	53.593665
3109.584446	294981.867652	53.598669
3108.633790	294717.007281	53.603674
3108.274245	294426.866001	53.608679
3107.395474	294152.825346	53.613684
3106.624824	293872.756954	53.618689
3105.906651	293581.346954	53.623693
3105.386460	293313.105946	53.628698
3104.898048	293027.643662	53.633703
3104.171848	292746.522622	53.638708
3103.576122	292480.406352	53.643713
3102.719573	292191.690501	53.648717
3102.104476	291925.907732	53.653722
3101.545540	291639.410710	53.658727
3100.725577	291369.126525	53.663732
3099.933720	291094.762786	53.668737
3099.670076	290813.362511	53.673741
3098.545531	290542.005050	53.678746
3098.088363	290271.738673	53.683751
3097.248335	289998.451015	53.688756
3096.507578	289712.337123	53.693761
3096.066258	289437.636014	53.698765
3095.099011	289162.763178	53.703770
3094.709517	288885.277340	53.708775
3094.066466	288622.169718	53.713780
3093.249304	288350.888777	53.718785
3092.981815	288067.779939	53.723789
3092.398097	287803.770830	53.728794
3091.537893	287518.845191	53.733799
3090.773023	287244.091367	53.738804
3090.191669	286971.473042	53.743809
3089.740412	286689.792787	53.748813
3088.893899	286412.555335	53.753818
3088.712795	286129.838619	53.758823
3087.359025	285860.168587	53.763828
3086.649316	285585.812192	53.768833
3086.254100	285302.542951	53.773837
3085.518210	285033.793265	53.778842
3084.697045	284752.908620	53.783847
3084.190163	284475.412237	53.788852
3083.515896	284198.502455	53.793857
3082.966855	283921.165186	53.798861
3082.160778	283659.098364	53.803866
3081.394832	283370.308947	53.808871
3080.917256	283093.240012	53.813876
3080.070979	282828.377586	53.818881
3079.548743	282554.626277	53.823885
3078.681313	282279.554166	53.828890
3077.994199	282007.025669	53.833895
3077.250402	281736.467061	53.838900
3076.757778	281463.932991	53.843905
3076.447306	281177.897262	53.848909
3075.620490	280910.738696	53.853914
3074.755740	280633.551522	53.858919
3074.499271	280366.659035	53.863924
3073.571821	280096.154261	53.868929
3073.039770	279815.246683	53.873933
3071.987074	279539.565998	53.878938
3071.779069	279259.829424	53.883943
3070.885014	278994.285319	53.888948
3070.124625	278721.818066	53.893953
3069.594913	278434.873680	53.898957
3068.508863	278171.295334	53.903962
3068.153895	277885.851253	53.908967
3067.804745	277602.953022	53.913972
3066.935815	277325.892843	53.918977
3066.002155	277044.080270	53.923981
3065.457480	276786.783076	53.928986
3064.671768	276499.751454	53.933991
3063.938497	276235.480231	53.938996
3063.064337	275972.071734	53.944001
3062.794348	275689.135219	53.949005
3061.923827	275431.583833	53.954010
3061.389568	275155.387292	53.959015
3060.695500	274893.580206	53.964020
3059.805657	274628.111181	53.969025
3059.272785	274358.663529	53.974029
3058.507715	274092.792736	53.979034
3058.322378	273809.689977	53.984039
3057.286713	273546.281529	53.989044
3056.520159	273283.314409	53.994049
3056.327530	273008.744772	53.999053
3055.362208	272745.401666	54.004058
3054.754286	272466.058825	54.009063
3054.112876	272197.086953	54.014068
3052.947769	271933.673705	54.019073
3052.650498	271665.004015	54.024077
3052.053279	271406.059824	54.029082
3051.209098	271129.556138	54.034087
3050.546164	270876.200030	54.039092
3049.822577	270611.290952	54.044097
3049.599051	270337.516226	54.049101
3048.832192	270079.516058	54.054106
3048.108676	269802.535206	54.059111
3047.332582	269531.420477	54.064116
3046.372721	269257.406068	54.069121
3045.913094	269001.369609	54.074125
3045.169720	268736.846272	54.079130
3044.475092	268471.016438	54.084135
3043.967702	268216.082963	54.089140
3043.238655	267945.012329	54.094145
3042.601556	267667.101774	54.099149
3041.858932	267406.526448	54.104154
3041.001719	267142.327422	54.109159
3040.378666	266884.789602	54.114164
3039.790602	266625.336255	54.119169
3039.201590	266352.818014	54.124173
3038.492090	266104.539218	54.129178
3037.994661	265840.869690	54.134183
3037.438728	265585.741397	54.139188
3036.626887	265310.253783	54.144193
3036.133718	265040.777316	54.149197
3035.142378	264786.864463	54.154202
3034.335919	264516.495596	54.159207
3033.972510	264252.270994	54.164212
3033.167407	263995.629548	54.169217
3032.748984	263730.879177	54.174221
3031.824099	263477.873498	54.179226
3031.436632	263198.398101	54.184231
3030.774474	262937.761757	54.189236
3029.958678	262682.854745	54.194241
3029.146324	262408.235200	54.199245
3028.468269	262159.724699	54.204250
3027.994623	261893.532786	54.209255
3027.496844	261631.114158	54.214260
3026.969268	261367.172394	54.219265
3026.501903	261099.044602	54.224269
3025.179047	260841.112232	54.229274
3024.582813	260560.755307	54.234279
3024.163886	260305.660068	54.239284
3023.040875	260051.491464	54.244289
3022.478683	259777.598723	54.249293
3021.590941	259523.953654	54.254298
3020.956596	259262.271871	54.259303
3020.564553	259011.248400	54.264308
3019.749658	258750.054119	54.269313
3019.446089	258488.600898	54.274317
3018.416945	258233.553275	54.279322
3017.779257	257963.723722	54.284327
3017.117066	257712.107608	54.289332
3016.318574	257457.635505	54.294337
3015.978989	257195.272532	54.299341
3015.140176	256946.410199	54.304346
3014.306471	256691.078609	54.309351
3013.983382	256430.853152	54.314356
3013.154962	256170.682513	54.319361
3012.611209	255907.411046	54.324365
3011.481275	255658.239677	54.329370
3011.088327	255398.561311	54.334375
3010.480236	255140.088806	54.339380
3009.744990	254886.984854	54.344385
3009.313251	254630.598844	54.349389
3008.439185	254380.369808	54.354394
3007.744562	254119.340103	54.359399
3007.002735	253869.931186	54.364404
3006.327722	253616.411820	54.369409
3006.053068	253355.367587	54.374413
3004.866031	253102.643015	54.379418
3004.330216	252855.163755	54.384423
3004.004856	252596.547947	54.389428
3003.044508	252332.710437	54.394433
3002.609434	252079.537158	54.399437
3001.761447	251834.018689	54.404442
3000.923699	251568.583945	54.409447
3000.575849	251319.472611	54.414452
2999.724164	251066.341247	54.419457
2999.174454	250811.583523	54.424461
2998.634379	250557.996115	54.429466
2998.001040	250296.911215	54.434471
2997.145927	250038.917806	54.439476
2996.421932	249787.830924	54.444481
2995.625598	249535.380688	54.449485
2995.139906	249283.289134	54.454490
2994.482793	249025.469712	54.459495
2993.799667	248772.391558	54.464500
2992.981525	248520.226501	54.469505
2992.686147	248260.390164	54.474509
2991.636617	248017.710518	54.479514
2991.323091	247761.417694	54.484519
2990.440067	247507.965787	54.489524
2989.532097	247259.535070	54.494529
2989.120113	247008.046731	54.499533
2988.341976	246753.331667	54.504538
2987.800959	246502.526731	54.509543
2986.884862	246247.528797	54.514548
2986.256274	246007.103198	54.519553
2985.653376	245756.131096	54.524557
2984.802477	245505.147763	54.529562
2983.969315	245251.258981	54.534567
2983.410592	245008.404785	54.539572
2983.098571	244773.839221	54.544577
2982.295168	244520.278126	54.549581
2981.363045	244279.547041	54.554586
2980.986758	244026.988813	54.559591
2980.305362	243772.060144	54.564596
2979.635437	243533.173341	54.569601
2979.338718	243281.749880	54.574605
2978.409645	243028.873620	54.579610
2977.710499	242780.061361	54.584615
2977.177693	242529.517086	54.589620
2976.300821	242284.579168	54.594625
2975.697774	242032.035249	54.599629
2974.835020	241785.899208	54.604634
2974.394278	241532.693979	54.609639
2973.481803	241298.866364	54.614644
2972.909242	241047.440081	54.619649
2972.613158	240793.831505	54.624653
2971.778427	240547.515261	54.629658
2971.084355	240298.019631	54.634663
2970.609127	240052.335046	54.639668
2969.910275	239804.420019	54.644673
2969.375151	239550.520891	54.649677
2968.552003	239303.084966	54.654682
2967.798392	239046.751467	54.659687
2967.295157	238800.029913	54.664692
2966.383512	238565.036215	54.669697
2965.892597	238305.963575	54.674701
2965.077968	238055.116794	54.679706
2964.274332	237804.014194	54.684711
2964.008266	237561.077438	54.689716
2962.899698	237318.758405	54.694721
2962.480074	237061.383475	54.699725
2961.694368	236822.859497	54.704730
2961.077818	236581.457312	54.709735
2960.487895	236325.562535	54.714740
2959.915382	236090.571369	54.719745
2959.288244	235828.037636	54.724749
2958.428532	235594.519006	54.729754
2957.710748	235336.966262	54.734759
2957.286864	235087.974303	54.739764
2956.417499	234838.849757	54.744769
2955.908409	234589.745172	54.749773
2955.257309	234353.471738	54.754778
2954.549053	234095.385868	54.759783
2953.634304	233854.546484	54.764788
2952.956285	233608.653960	54.769793
2952.510244	233363.641991	54.774797
2951.928946	233111.777022	54.779802
2950.802861	232868.452645	54.784807
2950.270803	232628.981585	54.789812
2949.468495	232394.952020	54.794817
2949.057185	232137.053425	54.799821
2948.380558	231906.748176	54.804826
2947.564438	231648.914979	54.809831
2946.616820	231411.957150	54.814836
2946.267391	231169.990950	54.819841
2945.942391	230923.158178	54.824845
2944.945068	230682.747163	54.829850
2944.501911	230447.290579	54.834855
2943.845095	230199.621075	54.839860
2943.093852	229955.735590	54.844865
2942.915881	229707.380517	54.849869
2941.900863	229464.200119	54.854874
2941.182095	229215.881081	54.859879
2940.815157	228967.074177	54.864884
2939.483983	228721.425112	54.869889
2939.047812	228482.356941	54.874893
2938.379116	228244.548388	54.879898
2937.773981	228005.610103	54.884903
2937.328961	227741.516566	54.889908
2936.346014	227512.849524	54.894913
2936.058188	227258.280626	54.899917
2935.333610	227023.870618	54.904922
2934.823226	226766.817734	54.909927
2933.924196	226523.219739	54.914932
2932.894218	226276.995218	54.919937
2932.597147	226035.823975	54.924941
2931.662632	225792.450124	54.929946
2930.862410	225554.848075	54.934951
2930.392328	225312.395071	54.939956
2929.778606	225073.937395	54.944961
2929.078199	224827.550401	54.949965
2928.466410	224593.740384	54.954970
2927.701946	224348.001491	54.959975
2926.984064	224107.946376	54.964980
2925.918517	223871.600579	54.969985
2925.896723	223626.790174	54.974989
2924.833851	223396.492174	54.979994
2924.088815	223155.387607	54.984999
2923.605628	222926.539532	54.990004
2922.838970	222685.439819	54.995009
2922.185123	222443.571918	55.000013
2921.774993	222217.476740	55.005018
2921.128829	221980.993811	55.010023
2920.561291	221730.623626	55.015028
2919.515491	221494.701918	55.020033
2919.068373	221251.570213	55.025037
2918.425968	221017.610139	55.030042
2917.750101	220777.011186	55.035047
2916.940704	220545.281240	55.040052
2916.282597	220306.144881	55.045057
2915.777588	220058.749016	55.050061
2914.893446	219829.388080	55.055066
2914.185859	219593.406024	55.060071
2913.951817	219359.551938	55.065076
2912.683571	219127.428048	55.070081
2912.571068	218882.087043	55.075085
2911.632770	218651.643612	55.080090
2910.637822	218412.528510	55.085095
2910.356924	218179.742137	55.090100
2909.117218	217953.587478	55.095105
2909.033010	217704.452666	55.100109
2907.949877	217479.267583	55.105114
2907.416419	217247.949873	55.110119
2906.989848	217004.650704	55.115124
2905.986856	216790.389350	55.120129
2905.645026	216551.024311	55.125133
2904.951360	216323.031787	55.130138
2904.275804	216090.289272	55.135143
2903.725034	215850.577840	55.140148
2902.904603	215618.088961	55.145153
2902.742151	215374.740905	55.150157
2901.583808	215152.082763	55.155162
2900.922240	214917.712704	55.160167
2900.696686	214676.731912	55.165172
2900.136330	214441.494647	55.170177
2899.311035	214202.557962	55.175181
2898.585409	213970.759741	55.180186
2897.609589	213740.020206	55.185191
2896.831594	213500.009338	55.190196
2896.110583	213274.475157	55.195201
2895.315326	213035.436049	55.200205
2894.763612	212799.121271	55.205210
2894.351112	212568.614813	55.210215
2893.664105	212323.718896	55.215220
2892.666040	212113.519062	55.220225
2892.313239	211878.257992	55.225229
2891.773327	211650.549659	55.230234
2891.274331	211412.513258	55.235239
2890.528677	211172.085754	55.240244
2889.642197	210945.325736	55.245249
2889.205693	210698.932588	55.250253
2888.549951	210477.279740	55.255258
2887.781317	210239.570398	55.260263
2886.913348	210004.957777	55.265268
2886.304096	209771.476007	55.270273
2885.459739	209538.274154	55.275277
2885.041716	209310.529422	55.280282
2884.402950	209079.574956	55.285287
2883.752044	208851.270581	55.290292
2883.077007	208629.296392	55.295297
2882.642554	208389.924775	55.300301
2882.101915	208152.059997	55.305306
2881.031406	207923.901855	55.310311
2880.372929	207680.012113	55.315316
2879.764351	207446.831723	55.320321
2879.124542	207214.357164	55.325325
2878.539911	206986.481962	55.330330
2877.810953	206757.434132	55.335335
2877.377692	206513.144345	55.340340
2876.544240	206283.058531	55.345345
2875.876288	206044.751291	55.350349
2875.277254	205820.459054	55.355354
2874.414992	205594.363962	55.360359
2874.124908	205355.528767	55.365364
2873.529420	205120.840887	55.370369
2872.795127	204875.994625	55.375373
2872.063984	204644.651780	55.380378
2871.236327	204406.478267	55.385383
2870.537953	204164.556403	55.390388
2869.477169	203935.063011	55.395393
2869.251687	203709.867043	55.400397
2868.685001	203470.637951	55.405402
2867.605234	203235.919839	55.410407
2867.198860	203008.286372	55.415412
2866.551212	202785.922470	55.420417
2866.018099	202544.350329	55.425421
2865.230785	202311.893147	55.430426
2864.129873	202086.587690	55.435431
2863.675498	201849.192912	55.440436
2862.813570	201635.330231	55.445441
2862.362992	201400.380127	55.450445
2861.500697	201168.194076	55.455450
2861.005095	200949.821991	55.460455
2860.606917	200721.152979	55.465460
2859.720639	200496.354445	55.470465
2859.276679	200250.769533	55.475469
2858.532478	200031.167893	55.480474
2857.730750	199797.959980	55.485479
2857.243274	199565.415927	55.490484
2856.289484	199356.030535	55.495489
2855.475946	199113.028892	55.500493
2855.249994	198891.759125	55.505498
2853.912887	198660.435147	55.510503
2853.414945	198432.440526	55.515508
2852.847507	198215.274219	55.520513
2852.456723	197975.455681	55.525517
2851.574531	197755.274353	55.530522
2850.917414	197546.777971	55.535527
2850.505674	197309.752520	55.540532
2849.261478	197090.153004	55.545537
2849.195421	196864.081801	55.550541
2848.167930	196638.621908	55.555546
2847.627412	196425.428806	55.560551
2847.058940	196190.354655	55.565556
2846.291010	195973.458377	55.570561
2845.867978	195741.607989	55.575565
2845.244163	195511.050156	55.580570
2844.587866	195295.704149	55.585575
2843.991150	195064.406009	55.590580
2843.012872	194842.547131	55.595585
2842.551697	194607.425030	55.600589
2841.499811	194388.162801	55.605594
2840.971022	194164.810587	55.610599
2840.434853	193938.788472	55.615604
2839.592789	193717.154693	55.620609
2839.298345	193486.375719	55.625613
2838.190749	193265.294936	55.630618
2837.474952	193048.224710	55.635623
2837.311078	192816.104864	55.640628
2836.519050	192604.341731	55.645633
2835.841263	192372.521637	55.650637
2835.304151	192155.528795	55.655642
2834.379452	191919.360280	55.660647
2833.895897	191689.243033	55.665652
2832.637838	191469.517318	55.670657
2832.603031	191250.298659	55.675661
2831.945288	191025.301458	55.680666
2831.092525	190806.125260	55.685671
2830.682547	190572.235530	55.690676
2829.815656	190358.738132	55.695681
2828.999159	190135.017062	55.700685
2828.502535	189905.851812	55.705690
2827.776876	189672.970651	55.710695
2826.925192	189457.248320	55.715700
2825.855295	189242.833804	55.720705
2825.662338	189021.449239	55.725709
2825.178280	188803.496047	55.730714
2824.364227	188584.311124	55.735719
2823.946966	188357.723432	55.740724
2822.986548	188140.561192	55.745729
2822.464482	187915.989658	55.750733
2821.986042	187692.697251	55.755738
2821.472061	187471.625227	55.760743
2820.430933	187244.556467	55.765748
2819.627868	187030.186079	55.770753
2819.274103	186802.501728	55.775757
2818.543927	186580.972000	55.780762
2817.735124	186352.649481	55.785767
2817.321794	186130.855456	55.790772
2816.487991	185915.871715	55.795777
2815.957510	185692.139177	55.800781
2815.337328	185469.579622	55.805786
2814.550330	185242.887555	55.810791
2814.235638	185020.256365	55.815796
2813.013865	184800.034367	55.820801
2812.721868	184566.321268	55.825805
2811.970002	184350.021609	55.830810
2811.133666	184130.123475	55.835815
2811.033612	183900.886809	55.840820
2810.035514	183683.064619	55.845825
2809.227951	183464.297382	55.850829
2808.795862	183225.652141	55.855834
2808.105386	183010.188814	55.860839
2807.516908	182783.108770	55.865844
2806.473600	182571.507046	55.870849
2806.480689	182335.455717	55.875853
2805.797872	182102.746009	55.880858
2804.634732	181875.672587	55.885863
2804.187413	181645.026935	55.890868
2803.332568	181421.786860	55.895873
2802.688084	181193.986075	55.900877
2801.951901	180976.695443	55.905882
2801.348941	180760.911254	55.910887
2801.188443	180525.074302	55.915892
2800.033350	180307.916963	55.920897
2799.348167	180076.337825	55.925901
2798.996111	179854.374527	55.930906
2797.914560	179635.364500	55.935911
2797.431692	179406.377275	55.940916
2796.716096	179182.503416	55.945921
2796.046567	178955.570650	55.950925
2795.312065	178736.433944	55.955930
2794.559767	178519.717950	55.960935
2794.041050	178290.933193	55.965940
2793.105951	178080.506511	55.970945
2792.825153	177848.188557	55.975949
2791.839412	177627.634630	55.980954
2791.124368	177411.796072	55.985959
2790.829069	177182.574926	55.990964
2789.985019	176960.768284	55.995969
2789.617808	176738.531161	56.000973
2788.789220	176515.974000	56.005978
2787.735266	176300.627318	56.010983
2787.571222	176067.067016	56.015988
2786.786174	175855.991821	56.020993
2785.805626	175636.465140	56.025997
2785.094403	175418.677616	56.031002
2784.505337	175193.952873	56.036007
2783.905198	174969.014898	56.041012
2783.428464	174756.650085	56.046017
2782.803181	174544.640589	56.051021
2781.967722	174316.207713	56.056026
2781.438606	174095.727509	56.061031
2780.473776	173869.454338	56.066036
2779.582715	173658.572628	56.071041
2778.972211	173442.458539	56.076045
2778.743925	173221.922738	56.081050
2777.848188	173020.036865	56.086055
2777.527500	172792.217860	56.091060
2776.624227	172577.846295	56.096065
2775.865582	172361.507135	56.101069
2775.324732	172153.820936	56.106074
2774.533567	171933.266932	56.111079
2773.830109	171708.236351	56.116084
2773.111412	171491.196131	56.121089
2772.656972	171282.267203	56.126093
2771.950083	171059.936980	56.131098
2771.196440	170839.217813	56.136103
2770.433023	170620.726970	56.141108
2770.088311	170412.357567	56.146113
2769.011016	170203.062494	56.151117
2768.671374	169987.649219	56.156122
2768.126001	169774.914871	56.161127
2767.437506	169544.273391	56.166132
2766.703196	169337.739107	56.171137
2765.989168	169120.622289	56.176141
2765.428345	168889.150613	56.181146
2764.789924	168684.626602	56.186151
2764.103088	168454.652637	56.191156
2763.446085	168239.273936	56.196161
2762.759350	168027.410908	56.201165
2762.232131	167816.172326	56.206170
2761.282663	167590.797631	56.211175
2760.988147	167363.069753	56.216180
2760.037695	167160.599776	56.221185
2759.559600	166941.664969	56.226189
2758.788893	166728.054940	56.231194
2758.392470	166506.846256	56.236199
2757.736304	166280.186740	56.241204
2756.819526	166068.905164	56.246209
2755.843730	165848.249894	56.251213
2755.796946	165625.948323	56.256218
2754.993454	165403.526336	56.261223
2754.301567	165181.304161	56.266228
2753.639097	164971.158342	56.271233
2752.781364	164755.424437	56.276237
2752.269033	164522.967305	56.281242
2751.376903	164315.315636	56.286247
2750.992743	164093.826867	56.291252
2750.198133	163885.691709	56.296257
2750.040130	163631.797294	56.301261
2749.229503	163373.684939	56.306266
2748.383104	163159.713243	56.311271
2747.563795	162929.247466	56.316276
2746.865692	162714.631867	56.321281
2746.367610	162493.984557	56.326285
2745.630587	162269.129782	56.331290
2744.633597	162049.276217	56.336295
2744.146835	161839.184093	56.341300
2743.423253	161633.631567	56.346305
2742.803421	161407.441304	56.351309
2742.396176	161188.262425	56.356314
2741.366586	160980.092135	56.361319
2740.925446	160763.197041	56.366324
2739.936481	160547.610574	56.371329
2739.408893	160330.820796	56.376333
2738.997107	160111.623806	56.381338
2738.104311	159907.036103	56.386343
2737.881608	159682.001656	56.391348
2736.702623	159482.534467	56.396353
2736.158176	159249.785762	56.401357
2735.624735	159032.458169	56.406362
2734.889777	158829.758705	56.411367
2734.062738	158606.759263	56.416372
2733.537402	158399.821000	56.421377
2732.594470	158173.105009	56.426381
2731.943603	157956.285778	56.431386
2731.393615	157759.029795	56.436391
2730.469839	157553.024141	56.441396
2729.648920	157335.905175	56.446401
2729.379538	157121.230024	56.451405
2728.732772	156917.103880	56.456410
2727.911556	156709.892005	56.461415
2727.311351	156496.264714	56.466420
2726.498170	156288.850697	56.471425
2725.909406	156078.033623	56.476429
2725.419736	155858.646825	56.481434
2724.601368	155664.775911	56.486439
2724.176959	155449.703523	56.491444
2723.363201	155253.266376	56.496449
2722.578701	155028.236639	56.501453
2722.207060	154830.117485	56.506458
2721.528768	154618.459197	56.511463
2720.876086	154394.429717	56.516468
2720.388248	154199.358031	56.521473
2719.572930	153976.386721	56.526477
2719.151272	153760.955961	56.531482
2718.254721	153550.978707	56.536487
2717.633578	153335.188221	56.541492
2716.670811	153126.152036	56.546497
2716.065448	152904.082498	56.551501
2715.841559	152692.898196	56.556506
2714.964057	152489.330938	56.561511
2714.224646	152269.689224	56.566516
2713.746208	152066.086760	56.571521
2712.863869	151846.597593	56.576525
2712.250742	151634.439391	56.581530
2711.470503	151423.211472	56.586535
2711.128565	151216.643761	56.591540
2710.108596	151011.951496	56.596545
2709.392461	150803.017974	56.601549
2709.057044	150584.696168	56.606554
2708.297393	150382.572181	56.611559
2707.682505	150158.654185	56.616564
2707.163452	149948.068005	56.621569
2706.473523	149744.754890	56.626573
2705.376135	149524.692516	56.631578
2704.754809	149310.555204	56.636583
2704.387441	149105.441045	56.641588
2703.649964	148898.709153	56.646593
2703.030642	148686.583755	56.651597
2702.518801	148470.769709	56.656602
2701.451543	148262.988412	56.661607
2701.018722	148055.158787	56.666612
2700.104614	147840.556523	56.671617
2699.703941	147626.802117	56.676621
2699.262469	147411.962629	56.681626
2698.349627	147211.191745	56.686631
2698.013955	146990.174519	56.691636
2697.113150	146790.052529	56.696641
2696.363794	146572.458841	56.701645
2695.956162	146356.693373	56.706650
2694.545875	146139.105693	56.711655
2694.371944	145936.611826	56.716660
2693.744064	145716.780803	56.721665
2693.148811	145507.277915	56.726669
2692.051796	145299.431719	56.731674
2691.328353	145089.176727	56.736679
2691.156329	144876.256070	56.741684
2690.148235	144679.011039	56.746689
2689.459330	144464.878861	56.751693
2689.132545	144256.866725	56.756698
2687.929910	144052.489326	56.761703
2687.459283	143856.117418	56.766708
2686.938359	143641.608472	56.771713
2686.490532	143433.341451	56.776717
2685.819256	143220.841582	56.781722
2684.719148	143020.305044	56.786727
2684.664876	142805.740662	56.791732
2683.777311	142606.481973	56.796737
2682.605590	142390.572670	56.801741
2682.325168	142182.795839	56.806746
2681.370719	141974.834941	56.811751
2680.806512	141777.525363	56.816756
2680.123933	141580.947379	56.821761
2680.095351	141362.691384	56.826765
2679.071751	141152.612340	56.831770
2678.282051	140945.394734	56.836775
2677.725807	140744.850455	56.841780
2677.408971	140533.151674	56.846785
2676.456008	140328.035251	56.851789
2675.981047	140115.043010	56.856794
2675.176384	139904.747332	56.861799
2674.770826	139689.752268	56.866804
2673.934301	139484.978887	56.871809
2673.298990	139268.422309	56.876813
2672.696523	139053.678982	56.881818
2671.773010	138852.430426	56.886823
2671.196742	138624.421530	56.891828
2670.729002	138429.456292	56.896833
2669.897140	138211.375750	56.901837
2669.698214	138004.707342	56.906842
2668.448261	137784.294905	56.911847
2667.632514	137577.041124	56.916852
2667.093409	137380.175625	56.921857
2666.670654	137155.444213	56.926861
2666.199374	136962.102665	56.931866
2665.209834	136741.491573	56.936871
2664.827509	136525.321422	56.941876
2664.071069	136316.923683	56.946881
2663.030202	136109.334742	56.951885
2662.399978	135897.121406	56.956890
2661.905124	135684.189434	56.961895
2661.082659	135478.387048	56.966900
2660.558934	135275.879913	56.971905
2660.035290	135066.336248	56.976909
2659.689603	134850.655399	56.981914
2658.677521	134646.680157	56.986919
2658.231948	134423.878852	56.991924
2657.313115	134216.982746	56.996929
2656.454491	134018.856607	57.001933
2656.056073	133803.230014	57.006938
2655.014264	133594.668312	57.011943
2654.432124	133382.618160	57.016948
2653.918935	133177.405563	57.021953
2653.351060	132973.308249	57.026957
2652.858795	132756.522996	57.031962
2651.822038	132561.102712	57.036967
2651.450905	132343.780581	57.041972
2650.548256	132139.488201	57.046977
2649.740299	131935.728487	57.051981
2649.070787	131720.287535	57.056986
2648.663866	131516.962672	57.061991
2648.195011	131301.213654	57.066996
2647.241707	131107.060347	57.072001
2646.469795	130887.081901	57.077005
2645.999637	130692.816782	57.082010
2645.246656	130481.894942	57.087015
2644.308288	130266.406038	57.092020
2643.963515	130065.152146	57.097025
2642.855862	129872.898930	57.102029
2642.631631	129666.954632	57.107034
2641.758723	129455.437128	57.112039
2641.312324	129256.643795	57.117044
2640.346434	129057.756369	57.122049
2639.598638	128850.986551	57.127053
2639.309362	128643.637579	57.132058
2638.366425	128435.149035	57.137063
2637.665156	128238.384684	57.142068
2637.477256	128027.087007	57.147073
2636.626788	127830.044377	57.152077
2636.079700	127613.459818	57.157082
2635.163779	127423.809442	57.162087
2634.987795	127208.299597	57.167092
2634.034644	127006.541902	57.172097
2633.252307	126795.589136	57.177101
2632.756670	126574.635751	57.182106
2631.858987	126393.231902	57.187111
2631.296374	126181.347350	57.192116
2630.859938	125976.962689	57.197121
2629.672285	125770.946036	57.202125
2628.968700	125568.346615	57.207130
2628.396292	125372.585621	57.212135
2628.192435	125164.754042	57.217140
2627.487932	124967.962844	57.222145
2626.669806	124756.612429	57.227149
2626.451276	124546.502059	57.232154
2625.163240	124344.283759	57.237159
2624.463718	124140.602244	57.242164
2623.861911	123932.843174	57.247169
2623.308343	123732.468696	57.252173
2622.797213	123529.409582	57.257178
2621.950542	123323.014673	57.262183
2621.525515	123120.897392	57.267188
2620.982702	122906.762312	57.272193
2619.820929	122715.126644	57.277197
2619.487604	122502.955221	57.282202
2618.539602	122307.428385	57.287207
2617.825147	122104.437696	57.292212
2617.536466	121903.844467	57.297217
2616.430095	121706.899587	57.302221
2615.951493	121497.984414	57.307226
2614.982745	121306.277519	57.312231
2614.890237	121097.634460	57.317236
2614.042838	120907.523800	57.322241
2613.191223	120708.095398	57.327245
2612.820941	120488.467261	57.332250
2612.107522	120291.508753	57.337255
2611.236983	120089.345475	57.342260
2610.449235	119897.531266	57.347265
2609.841624	119693.031247	57.352269
2609.337315	119484.770943	57.357274
2608.321360	119289.873968	57.362279
2607.918226	119094.906734	57.367284
2607.336223	118901.918193	57.372289
2606.759937	118697.128988	57.377293
2606.422311	118492.805074	57.382298
2605.303779	118299.366432	57.387303
2605.007190	118091.960369	57.392308
2604.278691	117894.673192	57.397313
2603.409282	117684.606154	57.402317
2602.545869	117478.037531	57.407322
2601.788692	117281.483231	57.412327
2601.823607	117075.924425	57.417332
2600.844145	116886.809823	57.422337
2599.943392	116685.934651	57.427341
2599.564644	116480.471542	57.432346
2598.352820	116281.407112	57.437351
2598.229436	116085.021777	57.442356
2597.681568	115883.138505	57.447361
2596.862021	115676.171184	57.452365
2596.339789	115480.710591	57.457370
2595.481160	115274.520752	57.462375
2594.911543	115064.757719	57.467380
2594.313572	114869.675611	57.472385
2593.019740	114673.016932	57.477389
2592.523048	114457.744385	57.482394
2592.147322	114269.746760	57.487399
2591.234407	114066.037996	57.492404
2590.822715	113868.433366	57.497409
2590.277387	113674.075680	57.502413
2589.999569	113469.731602	57.507418
2589.172863	113273.701601	57.512423
2588.371708	113064.734425	57.517428
2587.773006	112864.533414	57.522433
2586.766973	112665.585371	57.527437
2586.225160	112457.762631	57.532442
2585.355682	112266.247015	57.537447
2585.235579	112060.531264	57.542452
2584.197399	111852.506626	57.547457
2583.349630	111659.545242	57.552461
2582.971740	111453.513608	57.557466
2582.078338	111254.920709	57.562471
2581.581942	111056.882071	57.567476
2581.299017	110844.608445	57.572481
2580.194593	110645.254254	57.577485
2579.473439	110442.750398	57.582490
2578.746705	110246.195306	57.587495
2578.191985	110046.682683	57.592500
2577.442638	109842.925371	57.597505
2576.905982	109642.448582	57.602509
2576.271384	109450.232160	57.607514
2575.363886	109260.509955	57.612519
2574.851040	109055.395432	57.617524
2574.528313	108857.588081	57.622529
2573.436956	108668.070937	57.627533
2573.061193	108460.763130	57.632538
2572.375079	108259.915227	57.637543
2571.503915	108061.065395	57.642548
2570.887896	107862.113301	57.647553
2570.010079	107657.652142	57.652557
2569.614421	107462.913433	57.657562
2568.708402	107278.574540	57.662567
2567.997547	107072.524579	57.667572
2567.501986	106876.467579	57.672577
2566.611716	106684.630758	57.677581
2566.228493	106481.757220	57.682586
2565.274296	106288.138037	57.687591
2564.670939	106098.963374	57.692596
2563.964662	105908.639049	57.697601
2563.233417	105712.793835	57.702605
2563.024772	105507.458082	57.707610
2562.178641	105322.947010	57.712615
2561.675843	105126.588182	57.717620
2561.127421	104934.641369	57.722625
2560.350310	104733.545391	57.727629
2560.030660	104532.410333	57.732634
2559.057209	104329.718334	57.737639
2558.306876	104130.171256	57.742644
2557.698168	103937.855018	57.747649
2556.734991	103742.874803	57.752653
2556.407003	103543.709822	57.757658
2555.467355	103350.797334	57.762663
2554.804376	103150.254961	57.767668
2554.366197	102964.745910	57.772673
2553.415241	102766.999429	57.777677
2552.981820	102562.352788	57.782682
2552.153295	102376.415397	57.787687
2551.727878	102183.526118	57.792692
2550.795666	101985.688073	57.797697
2550.277745	101796.622938	57.802701
2549.929495	101598.035860	57.807706
2549.266128	101400.020589	57.812711
2548.628570	101194.320769	57.817716
2547.836747	100995.549017	57.822721
2546.899132	100810.973491	57.827725
2546.387049	100601.154756	57.832730
2545.631051	100403.416361	57.837735
2544.943477	100215.101381	57.842740
2544.226858	100018.026078	57.847745
2543.617287	99834.053335	57.852749
2543.226732	99637.405334	57.857754
2542.420132	99442.861092	57.862759
2541.454657	99245.907918	57.867764
2540.936910	99051.625659	57.872769
2540.078261	98856.809166	57.877773
2539.371676	98665.312948	57.882778
2538.663959	98486.218843	57.887783
2538.388388	98286.265831	57.892788
2537.787380	98096.907833	57.897793
2536.794921	97900.693526	57.902797
2536.485629	97698.442227	57.907802
2535.527871	97518.773722	57.912807
2534.669629	97324.033602	57.917812
2534.335240	97124.639167	57.922817
2533.658559	96941.917961	57.927821
2533.063971	96740.360948	57.932826
2532.479053	96563.108074	57.937831
2531.627127	96361.347853	57.942836
2530.940016	96175.609178	57.947841
2530.311419	95979.746953	57.952845
2529.804248	95772.666966	57.957850
2528.746619	95586.725472	57.962855
2527.989159	95393.901228	57.967860
2527.721178	95205.744847	57.972865
2527.213399	95019.080340	57.977869
2526.582018	94831.238355	57.982874
2525.688221	94645.246946	57.987879
2525.363177	94447.447355	57.992884
2524.462335	94252.042804	57.997889
2523.913345	94063.141455	58.002893
2523.486906	93863.822053	58.007898
2522.542232	93665.125595	58.012903
2521.875854	93463.139953	58.017908
2521.626349	93272.143171	58.022913
2520.690184	93079.424198	58.027917
2519.968948	92886.450881	58.032922
2519.233719	92690.818122	58.037927
2518.666624	92484.164785	58.042932
2518.091302	92289.981367	58.047937
2517.155281	92105.882089	58.052941
2516.656536	91901.842211	58.057946
2515.828839	91706.898589	58.062951
2515.043206	91508.532258	58.067956
2514.186968	91319.163912	58.072961
2513.436640	91130.763229	58.077965
2513.144357	90942.437394	58.082970
2512.298567	90764.269945	58.087975
2511.882409	90568.294683	58.092980
2511.241765	90380.181048	58.097985
2510.450003	90196.176289	58.102989
2510.142120	89997.582991	58.107994
2508.987090	89801.845812	58.112999
2508.251069	89611.293802	58.118004
2507.503019	89407.570173	58.123009
2507.119214	89238.605105	58.128013
2506.565111	89034.981015	58.133018
2505.781301	88865.359455	58.138023
2504.926780	88670.358291	58.143028
2504.721320	88472.998938	58.148033
2503.422794	88298.803447	58.153037
2503.190517	88096.861604	58.158042
2502.566995	87914.288593	58.163047
2502.048698	87725.538126	58.168052
2501.335234	87536.053128	58.173057
2500.422672	87341.745125	58.178061
2499.777027	87141.843022	58.183066
2498.948533	86953.325978	58.188071
2498.401139	86768.493681	58.193076
2497.887347	86585.508777	58.198081
2496.855745	86401.409351	58.203085
2496.360486	86214.849219	58.208090
2495.941372	86028.481498	58.213095
2495.225741	85833.547322	58.218100
2494.684749	85644.698242	58.223105
2494.174760	85454.096306	58.228109
2493.496266	85257.551343	58.233114
2492.476901	85073.182474	58.238119
2491.762979	84885.743086	58.243124
2490.917532	84687.835257	58.248129
2490.255394	84505.474831	58.253133
2489.738228	84316.988702	58.258138
2488.942633	84137.143746	58.263143
2488.215464	83950.342238	58.268148
2487.881789	83765.197779	58.273153
2487.257958	83580.088252	58.278157
2486.590377	83389.054400	58.283162
2485.558580	83207.917341	58.288167
2485.330962	83021.602632	58.293172
2484.704864	82827.391728	58.298177
2483.932275	82639.746979	58.303181
2483.254478	82459.827897	58.308186
2482.602331	82274.962484	58.313191
2481.870527	82074.525808	58.318196
2481.428207	81898.294701	58.323201
2480.536940	81712.787626	58.328205
2480.145782	81512.422746	58.333210
2479.335489	81338.625078	58.338215
2478.366950	81149.028273	58.343220
2477.864472	80957.844574	58.348225
2477.192402	80777.470031	58.353229
2476.527207	80586.683116	58.358234
2475.809942	80403.840930	58.363239
2475.025019	80219.280914	58.368244
2474.453601	80032.109318	58.373249
2473.686357	79855.313208	58.378253
2473.229856	79664.831219	58.383258
2472.623090	79487.905066	58.388263
2472.190157	79296.256652	58.393268
2471.463101	79115.106760	58.398273
2470.869838	78935.318754	58.403277
2469.998163	78733.440830	58.408282
2469.162009	78541.172590	58.413287
2468.688483	78361.446649	58.418292
2467.793179	78177.815862	58.423297
2467.304284	78002.550376	58.428301
2466.744077	77809.757284	58.433306
2466.093216	77628.747793	58.438311
2465.279856	77440.288312	58.443316
2464.676428	77252.722439	58.448321
2464.057375	77071.256590	58.453325
2463.393968	76877.886644	58.458330
2462.291094	76702.419115	58.463335
2462.126617	76501.528247	58.468340
2461.666886	76315.392908	58.473345
2461.035113	76131.250803	58.478349
2460.275814	75944.444001	58.483354
2459.547698	75759.370094	58.488359
2458.679600	75576.696122	58.493364
2458.449383	75378.735052	58.498369
2457.340897	75196.146968	58.503373
2456.802287	75003.991567	58.508378
2455.937020	74817.059883	58.513383
2455.189232	74640.489446	58.518388
2454.796350	74452.941361	58.523393
2454.083920	74278.687388	58.528397
2453.379904	74079.762406	58.533402
2452.492417	73890.124823	58.538407
2451.984908	73712.409354	58.543412
2451.653271	73522.490717	58.548417
2450.676917	73347.608747	58.553421
2450.347973	73156.128290	58.558426
2449.771647	72970.320993	58.563431
2449.078812	72778.984185	58.568436
2448.456122	72588.727745	58.573441
2447.513955	72408.545981	58.578445
2446.966204	72211.483628	58.583450
2446.178255	72033.707143	58.588455
2445.363794	71850.906471	58.593460
2444.974927	71649.174611	58.598465
2443.967842	71473.230653	58.603469
2443.586822	71290.379087	58.608474
2442.993084	71104.015469	58.613479
2442.240066	70910.393965	58.618484
2441.835529	70717.986032	58.623489
2440.617166	70543.927187	58.628493
2440.389959	70355.295406	58.633498
2439.627745	70178.145910	58.638503
2439.099776	69980.051051	58.643508
2438.602206	69802.444903	58.648513
2437.631410	69609.269733	58.653517
2436.920636	69420.121795	58.658522
2436.158583	69237.742340	58.663527
2435.517960	69050.917799	58.668532
2434.899800	68858.941912	58.673537
2434.217427	68680.146395	58.678541
2433.719449	68484.361076	58.683546
2432.924238	68303.294015	58.688551
2432.050528	68121.905384	58.693556
2431.579466	67947.497709	58.698561
2430.661150	67753.363446	58.703565
2430.630257	67573.651385	58.708570
2429.546436	67385.487948	58.713575
2429.026455	67201.733716	58.718580
2428.294591	67015.753777	58.723585
2427.565911	66841.276509	58.728589
2427.194945	66645.172844	58.733594
2426.345121	66457.791956	58.738599
2425.518039	66277.388443	58.743604
2424.918218	66087.216567	58.748609
2424.090770	65911.778524	58.753613
2423.546057	65729.761584	58.758618
2422.890677	65545.325719	58.763623
2422.397190	65361.024272	58.768628
2421.513638	65169.567007	58.773633
2420.792536	64993.091373	58.778637
2420.009584	64823.716629	58.783642
2419.403726	64642.739214	58.788647
2418.750895	64463.895534	58.793652
2418.188518	64274.163059	58.798657
2417.241704	64101.407433	58.803661
2417.062633	63911.491127	58.808666
2416.310158	63741.171247	58.813671
2415.218531	63558.137583	58.818676
2414.815432	63376.275623	58.823681
2414.257787	63201.373625	58.828685
2413.588440	63016.847131	58.833690
2413.112734	62835.799678	58.838695
2412.016254	62662.048676	58.843700
2411.745042	62469.289761	58.848705
2410.874032	62295.360729	58.853709
2410.181480	62112.762071	58.858714
2409.398113	61934.089426	58.863719
2408.520575	61761.290211	58.868724
2408.554561	61576.200812	58.873729
2407.570689	61405.115418	58.878733
2407.118272	61223.968842	58.883738
2406.394170	61038.374910	58.888743
2406.119672	60855.642953	58.893748
2405.653589	60675.130615	58.898753
2404.507015	60497.057803	58.903757
2404.002907	60297.605626	58.908762
2403.122993	60115.293395	58.913767
2402.227258	59931.858510	58.918772
2401.965137	59744.827070	58.923777
2401.130364	59569.451778	58.928781
2400.754301	59388.760250	58.933786
2399.711013	59199.233948	58.938791
2399.207976	59017.021415	58.943796
2398.545325	58830.651365	58.948801
2397.888585	58654.158046	58.953805
2397.346943	58457.656157	58.958810
2396.566384	58284.908346	58.963815
2395.929792	58104.890929	58.968820
2395.565845	57909.639066	58.973825
2394.404615	57726.942105	58.978829
2393.912759	57549.163882	58.983834
2393.285381	57359.603004	58.988839
2392.721303	57181.444115	58.993844
2392.085727	56999.294494	58.998849
2391.330840	56813.434033	59.003853
2390.503754	56624.649785	59.008858
2389.838562	56447.859103	59.013863
2389.169739	56267.791834	59.018868
2388.598096	56081.675474	59.023873
2387.839976	55897.612901	59.028877
2387.223893	55711.700378	59.033882
2386.458358	55534.494452	59.038887
2385.679965	55351.051363	59.043892
2385.028205	55175.289814	59.048897
2384.188815	55006.474569	59.053901
2383.694365	54823.289213	59.058906
2383.389383	54641.047190	59.063911
2382.918288	54453.855392	59.068916
2382.264947	54271.102655	59.073921
2381.030044	54098.586318	59.078925
2380.422731	53919.522822	59.083930
2379.888221	53743.101376	59.088935
2379.515776	53554.545584	59.093940
2379.013194	53360.499962	59.098945
2377.881162	53197.190627	59.103949
2377.577374	53000.620618	59.108954
2376.850819	52809.005478	59.113959
2375.716763	52634.363767	59.118964
2375.506915	52444.800108	59.123969
2374.763511	52269.324728	59.128973
2374.231823	52085.533614	59.133978
2373.541716	51897.080198	59.138983
2372.531302	51716.475948	59.143988
2371.954330	51534.181595	59.148993
2371.206950	51358.491032	59.153997
2370.683964	51167.190056	59.159002
2370.268716	50994.604916	59.164007
2368.906532	50823.146082	59.169012
2368.366233	50638.016892	59.174017
2368.107812	50462.475851	59.179021
2367.286254	50283.776514	59.184026
2366.521169	50104.845368	59.189031
2365.866895	49926.167361	59.194036
2365.359053	49744.585710	59.199041
2364.464483	49565.493818	59.204045
2364.072634	49375.687583	59.209050
2363.247990	49205.471931	59.214055
2362.362169	49031.971072	59.219060
2362.030594	48846.213549	59.224065
2361.422785	48674.342478	59.229069
2360.601337	48497.432586	59.234074
2359.933773	48321.379513	59.239079
2358.865648	48143.079180	59.244084
2358.556832	47957.362116	59.249089
2357.524847	47785.804150	59.254093
2357.024528	47614.217317	59.259098
2356.476031	47442.231707	59.264103
2355.503721	47278.150574	59.269108
2355.437496	47091.882151	59.274113
2354.856787	46917.274871	59.279117
2353.729706	46736.783740	59.284122
2352.875102	46563.773378	59.289127
2352.502144	46398.738649	59.294132
2351.773245	46210.930244	59.299137
2350.977484	46045.393335	59.304141
2350.576434	45876.512102	59.309146
2350.154862	45695.442136	59.314151
2349.262409	45522.109560	59.319156
2348.982970	45343.997087	59.324161
2347.753127	45171.879128	59.329165
2347.553680	44994.269920	59.334170
2346.875834	44815.099988	59.339175
2346.040273	44636.526215	59.344180
2345.908530	44455.454715	59.349185
2344.662682	44284.426550	59.354189
2344.054582	44102.482239	59.359194
2343.949352	43920.763705	59.364199
2342.909675	43742.870310	59.369204
2342.209326	43557.695045	59.374209
2341.489035	43382.667507	59.379213
2341.036697	43203.108330	59.384218
2340.475170	43027.157850	59.389223
2339.531454	42842.541129	59.394228
2339.059925	42665.729313	59.399233
2338.348556	42489.760603	59.404237
2337.770342	42300.224637	59.409242
2336.902707	42120.799440	59.414247
2336.297213	41951.909539	59.419252
2335.270677	41765.502225	59.424257
2334.461718	41590.661796	59.429261
2333.985067	41411.608874	59.434266
2333.590659	41228.376921	59.439271
2332.577765	41066.498269	59.444276
2332.341045	40889.597815	59.449281
2331.605317	40712.971203	59.454285
2330.869437	40525.291649	59.459290
2330.279533	40347.257498	59.464295
2329.521240	40172.853480	59.469300
2328.951786	40001.478966	59.474305
2328.273113	39825.620808	59.479309
2327.425768	39651.942917	59.484314
2326.929919	39475.058607	59.489319
2326.131017	39307.025321	59.494324
2325.466437	39117.993421	59.499329
2324.926827	38947.219165	59.504333
2324.087815	38773.496713	59.509338
2323.466696	38602.677177	59.514343
2322.680175	38435.363493	59.519348
2322.286604	38244.034502	59.524353
2321.371683	38073.722152	59.529357
2320.799803	37901.698830	59.534362
2320.162311	37714.949843	59.539367
2319.375122	37549.938724	59.544372
2319.090124	37371.612208	59.549377
2318.280236	37198.985640	59.554381
2317.534493	37035.166430	59.559386
2317.003331	36845.381471	59.564391
2315.809705	36674.092014	59.569396
2315.496155	36490.752671	59.574401
2314.828083	36335.334020	59.579405
2314.087500	36163.105374	59.584410
2313.536678	35991.847358	59.589415
2312.870085	35822.289646	59.594420
2312.430950	35640.481055	59.599425
2311.989003	35471.716326	59.604429
2310.898662	35289.504274	59.609434
2310.480960	35114.744170	59.614439
2309.498293	34938.102968	59.619444
2309.186856	34757.239914	59.624449
2307.781861	34593.403607	59.629453
2307.297202	34414.759145	59.634458
2307.141225	34242.930047	59.639463
2306.242614	34072.546493	59.644468
2306.155900	33900.501308	59.649473
2305.054089	33727.601086	59.654477
2304.352560	33539.568393	59.659482
2303.764538	33357.653318	59.664487
2302.960887	33182.644314	59.669492
2302.481673	33013.344524	59.674497
2301.516417	32844.916871	59.679501
2301.035809	32672.722423	59.684506
2300.680848	32493.259372	59.689511
2299.594992	32321.346292	59.694516
2299.122390	32135.780552	59.699521
2298.177892	31968.553195	59.704525
2297.674563	31798.199790	59.709530
2296.880810	31620.174794	59.714535
2296.047583	31459.326955	59.719540
2295.625748	31279.009072	59.724545
2295.090238	31111.660734	59.729549
2294.141362	30939.203045	59.734554
2293.691178	30759.840268	59.739559
2293.021034	30593.965950	59.744564
2292.547457	30426.854924	59.749569
2291.749941	30251.450908	59.754573
2290.910543	30081.201721	59.759578
2290.504093	29902.686696	59.764583
2289.935616	29742.063297	59.769588
2289.323874	29561.099135	59.774593
2288.537971	29389.453479	59.779597
2287.818128	29213.657979	59.784602
2287.020797	29038.025175	59.789607
2286.153920	28871.843978	59.794612
2285.921547	28692.317580	59.799617
2285.257906	28526.695401	59.804621
2284.426004	28346.416310	59.809626
2284.129274	28179.763076	59.814631
2283.239886	28000.700807	59.819636
2282.643934	27816.560535	59.824641
2281.642731	27660.220767	59.829645
2280.884045	27488.172142	59.834650
2280.317658	27312.548164	59.839655
2279.329374	27149.203230	59.844660
2279.047351	26974.711595	59.849665
2278.782324	26806.444980	59.854669
2277.853265	26634.263399	59.859674
2277.236293	26457.566683	59.864679
2276.399248	26292.067458	59.869684
2275.722400	26115.823132	59.874689
2274.952343	25942.258059	59.879693
2274.387503	25772.487452	59.884698
2274.112581	25596.038146	59.889703
2272.552924	25445.867863	59.894708
2272.274903	25267.852492	59.899713
2271.780918	25104.847895	59.904718
2271.095477	24934.771161	59.909722
2270.711939	24757.400527	59.914727
2269.619355	24589.214840	59.919732
2269.119406	24410.189028	59.924737
2268.311447	24255.880490	59.929742
2267.531891	24084.247396	59.934746
2267.084779	23921.096544	59.939751
2266.525881	23749.910618	59.944756
2265.813514	23574.291304	59.949761
2264.881821	23410.022936	59.954766
2264.318202	23244.125574	59.959770
2263.838263	23085.599549	59.964775
2262.770374	22918.334882	59.969780
2262.628826	22746.727099	59.974785
2261.647331	22585.864433	59.979790
2261.058975	22416.101528	59.984794
2260.397421	22247.546005	59.989799
2259.625063	22088.912035	59.994804
2259.023342	21919.982520	59.999809
2258.272404	21752.728802	60.004814
2257.721598	21590.039134	60.009818
2256.964285	21413.652480	60.014823
2256.300258	21257.657221	60.019828
2255.919337	21081.423812	60.024833
2255.010158	20922.657402	60.029838
2254.399847	20758.632358	60.034842
2254.206034	20582.871475	60.039847
2253.489956	20428.040698	60.044852
2252.836418	20251.798196	60.049857
2251.925441	20078.241116	60.054862
2251.078219	19917.164779	60.059866
2250.471463	19754.055617	60.064871
2249.665422	19581.372437	60.069876
2249.008682	19415.030568	60.074881
2248.629792	19257.701244	60.079886
2247.511945	19093.007044	60.084890
2247.002732	18928.807390	60.089895
2246.179849	18766.009618	60.094900
2245.635104	18604.259685	60.099905
2244.916004	18452.209251	60.104910
2244.481405	18285.293478	60.109914
2244.011410	18113.091446	60.114919
2243.220600	17953.754037	60.119924
2242.661646	17778.456246	60.124929
2241.793602	17616.440988	60.129934
2240.905430	17473.650140	60.134938
2240.785878	17301.374239	60.139943
2239.505991	17131.603945	60.144948
2238.911975	16975.613294	60.149953
2238.629680	16806.740172	60.154958
2237.735334	16648.897233	60.159962
2237.365427	16487.423716	60.164967
2236.463972	16327.832577	60.169972
2236.169003	16162.504006	60.174977
2235.280539	16001.419333	60.179982
2234.326660	15837.300670	60.184986
2233.825831	15670.522502	60.189991
2233.441258	15505.595410	60.194996
2232.573890	15341.409087	60.200001
2231.981522	15188.620420	60.205006
2231.263793	15013.318450	60.210010
2230.395592	14842.272207	60.215015
2229.371486	14696.251010	60.220020
2229.205177	14527.165520	60.225025
2228.347806	14370.442773	60.230030
2227.576683	14218.418489	60.235034
2227.412930	14059.880645	60.240039
2226.326354	13900.132740	60.245044
2225.954792	13741.231891	60.250049
2225.077412	13575.379922	60.255054
2224.469406	13409.998795	60.260058
2223.940854	13246.442333	60.265063
2222.709810	13097.575058	60.270068
2222.259406	12934.068625	60.275073
2221.955110	12775.420416	60.280078
2220.820758	12615.443512	60.285082
2220.466153	12463.466440	60.290087
2219.672089	12303.670736	60.295092
2219.032050	12145.510266	60.300097
2218.312978	11996.183955	60.305102
2217.749681	11838.317722	60.310106
2217.359312	11682.894456	60.315111
2216.211829	11533.479264	60.320116
2215.511533	11377.037063	60.325121
2214.975457	11216.174956	60.330126
2214.312683	11059.918462	60.335130
2213.708935	10900.082244	60.340135
2213.012986	10746.477854	60.345140
2212.496001	10594.934099	60.350145
2211.601449	10445.859163	60.355150
2210.850721	10285.663730	60.360154
2210.454625	10125.798786	60.365159
2209.537799	9985.431479	60.370164
2209.309169	9826.870082	60.375169
2208.371041	9678.061322	60.380174
2207.451218	9521.581172	60.385178
2206.919175	9370.961789	60.390183
2206.116654	9215.977136	60.395188
2205.357829	9059.959887	60.400193
2204.860108	8921.265446	60.405198
2204.315762	8767.374660	60.410202
2203.533683	8617.160270	60.415207
2202.719134	8474.170665	60.420212
2202.199191	8317.783963	60.425217
2201.639625	8166.923789	60.430222
2200.746086	8021.452065	60.435226
2200.543061	7866.736888	60.440231
2199.629479	7722.198622	60.445236
2199.294669	7576.684782	60.450241
2198.647354	7419.076837	60.455246
2197.811046	7267.127290	60.460250
2197.320586	7104.954157	60.465255
2196.424015	6956.608314	60.470260
2195.777402	6802.975177	60.475265
2195.123949	6653.443610	60.480270
2193.894844	6502.717854	60.485274
2193.670320	6346.140789	60.490279
2192.928804	6206.003062	60.495284
2192.152402	6052.317782	60.500289
2191.334140	5900.664837	60.505294
2190.704302	5759.877014	60.510298
2190.072185	5609.389399	60.515303
2189.380671	5471.841079	60.520308
2188.784081	5325.176362	60.525313
2187.728745	5180.035648	60.530318
2187.281429	5044.031686	60.535322
2186.900856	4899.628289	60.540327
2185.929868	4767.676637	60.545332
2185.243495	4616.739169	60.550337
2184.837682	4486.156397	60.555342
2184.027577	4337.884478	60.560346
2183.438906	4196.806024	60.565351
2182.643663	4062.995041	60.570356
2181.895646	3914.645743	60.575361
2181.198302	3774.729826	60.580366
2180.358714	3646.735307	60.585370
2179.691069	3503.179778	60.590375
2178.576673	3374.349466	60.595380
2178.114342	3239.226511	60.600385
2177.423781	3113.498566	60.605390
2176.427643	2986.565410	60.610394
2176.118514	2862.397433	60.615399
2175.388763	2744.070937	60.620404
2174.413281	2611.550160	60.625409
2173.803476	2493.171955	60.630414
2173.217603	2362.343177	60.635418
2172.724423	2245.179519	60.640423
2171.354412	2130.382959	60.645428
2170.796897	2012.985315	60.650433
2170.253669	1898.374849	60.655438
2169.318887	1788.190715	60.660442
2168.710841	1664.055058	60.665447
2167.848992	1563.030796	60.670452
2167.144776	1448.685178	60.675457
2166.537154	1347.102402	60.680462
2165.584396	1240.393399	60.685466
2164.828516	1133.563256	60.690471
2163.884461	1050.019906	60.695476
2163.278231	948.856037	60.700481
2162.179905	864.802008	60.705486
2160.861436	784.205673	60.710490
2159.745022	718.818639	60.715495
2158.743664	658.887672	60.720500
2157.929950	602.791001	60.725505
2156.619760	557.943658	60.730510
2155.259042	490.705513	60.735514
2154.819319	458.644361	60.740519
2153.591720	432.138067	60.745524
2153.263358	393.580868	60.750529
2152.512613	359.880265	60.755534
2151.621237	327.556728	60.760538
2150.854143	294.839788	60.765543
2150.657442	281.037254	60.770548
2149.919635	249.049092	60.775553
2149.360067	213.828203	60.780558
2148.913151	180.792628	60.785562
2148.019201	149.900258	60.790567
2146.897166	131.392188	60.795572
2146.492827	108.392478	60.800577
2146.025122	89.332775	60.805582
2145.034070	71.559392	60.810586
2144.549411	44.374523	60.815591
2143.403350	32.249396	60.820596
2142.782094	22.892241	60.825601
2142.209824	1.322881	60.830606
2141.374459	-3.657216	60.835610
2140.729383	-13.236079	60.840615
2139.525456	-8.410243	60.845620
2138.756754	-10.409339	60.850625
2137.976398	-1.632502	60.855630
2136.615397	19.513453	60.860634
2136.254320	16.181766	60.865639
2135.873804	26.648811	60.870644
2135.690018	28.382724	60.875649
2135.208216	25.098576	60.880654
2134.407190	32.028886	60.885658
2133.975715	17.005404	60.890663
2133.156591	26.942778	60.895668
2132.568436	25.741384	60.900673
2132.030208	35.948021	60.905678
2131.066244	46.791514	60.910682
2130.708360	40.522926	60.915687
2129.915572	46.906292	60.920692
2129.411657	43.964706	60.925697
2128.675179	44.575172	60.930702
2127.946599	47.001099	60.935706
2127.892750	42.877890	60.940711
2126.902430	63.009428	60.945716
2126.115055	44.940411	60.950721
2125.915969	49.833925	60.955726
2125.315975	57.221224	60.960730
2124.535712	50.308420	60.965735
2123.429237	59.849849	60.970740
2122.759212	60.640591	60.975745
2122.365748	68.859328	60.980750
2121.985156	66.970540	60.985754
2121.540690	56.658037	60.990759
2120.480370	60.175854	60.995764
2119.576397	62.896129	61.000769
2119.045005	65.946810	61.005774
2117.973904	66.414825	61.010778
2118.120401	61.826144	61.015783
2117.531975	73.650901	61.020788
2116.646245	73.807219	61.025793
2115.963546	63.789566	61.030798
2115.331486	65.969940	61.035802
2115.157116	67.251340	61.040807
2114.013010	74.428506	61.045812
2113.313079	66.744409	61.050817
2112.677955	58.556429	61.055822
2111.952189	73.118588	61.060826
2111.442821	74.150357	61.065831
2110.882634	80.171970	61.070836
2110.127682	71.342229	61.075841
2109.506081	66.481170	61.080846
2109.010750	80.696103	61.085850
2108.724043	73.738096	61.090855
2107.868949	77.649151	61.095860
2107.050350	78.242691	61.100865
2106.008805	73.508192	61.105870
2104.846406	83.463808	61.110874
2104.819592	76.587569	61.115879
2104.568600	80.022710	61.120884
2103.878724	80.964847	61.125889
2102.929877	76.695050	61.130894
2101.764052	75.597937	61.135898
2102.103713	79.483424	61.140903
2101.417408	78.163561	61.145908
2100.847363	80.395604	61.150913
2099.952265	78.618420	61.155918
2099.110677	83.429386	61.160922
2098.607004	80.908824	61.165927
2097.584996	87.986200	61.170932
2096.920821	83.847859	61.175937
2096.272153	88.150380	61.180942
2095.782501	94.452556	61.185946
2095.529223	87.599631	61.190951
2094.717761	88.127386	61.195956
2094.061385	84.713233	61.200961
2093.503054	87.397599	61.205966
2092.256507	86.005781	61.210970
2091.705890	79.517022	61.215975
2090.975913	79.952996	61.220980
2090.726465	89.222839	61.225985
2090.416710	87.816417	61.230990
2089.693197	92.868860	61.235994
2089.168991	89.577242	61.240999
2087.685239	88.901181	61.246004
2087.261610	84.740442	61.251009
2086.735030	86.311132	61.256014
2085.890900	89.454028	61.261018
2085.558861	82.384939	61.266023
2084.858806	88.867162	61.271028
2083.589714	88.565487	61.276033
2083.106180	88.792040	61.281038
2082.805371	90.759006	61.286042
2082.809178	85.074859	61.291047
2081.356126	90.569509	61.296052
2080.963376	87.230226	61.301057
2080.657926	94.982411	61.306062
2079.362506	88.299591	61.311066
2078.938906	81.626670	61.316071
2078.601343	94.845142	61.321076
2077.215077	90.613224	61.326081
2077.126180	91.418999	61.331086
2076.590350	102.677174	61.336090
2075.549268	88.805395	61.341095
2074.855698	89.916867	61.346100
2074.461110	88.135964	61.351105
2073.937569	87.048908	61.356110
2072.814409	89.266224	61.361114
2072.337899	90.171357	61.366119
2071.788187	91.815109	61.371124
2070.993025	93.510428	61.376129
2070.453524	92.209854	61.381134
2069.549606	90.304765	61.386138
2069.054119	82.419492	61.391143
2068.437298	93.116480	61.396148
2067.669879	97.248613	61.401153
2066.806908	87.161794	61.406158
2066.190653	94.510698	61.411162
2065.596572	85.792637	61.416167
2065.036662	89.781448	61.421172
2063.856325	91.722402	61.426177
2063.524782	99.626970	61.431182
2062.819168	109.057527	61.436186
2062.670986	102.676797	61.441191
2061.786806	96.602109	61.446196
2060.789127	100.381262	61.451201
2061.155663	95.951625	61.456206
2060.025078	100.803737	61.461210
2059.245771	89.213366	61.466215
2058.338084	97.504263	61.471220
2057.721106	98.490040	61.476225
2057.401919	91.450453	61.481230
2056.234138	95.116246	61.486234
2055.740523	84.464599	61.491239
2055.693239	92.344554	61.496244
2054.609559	90.037473	61.501249
2053.996691	89.201149	61.506254
2052.746503	98.841128	61.511258
2052.428414	98.290774	61.516263
2052.432038	98.517297	61.521268
2051.707886	96.056963	61.526273
2050.961093	97.235237	61.531278
2050.246863	109.169882	61.536282
2049.507704	92.534582	61.541287
2048.718513	98.508972	61.546292
2048.068381	100.968211	61.551297
2047.739011	98.123517	61.556302
2046.945979	98.665708	61.561306
2045.804917	102.030789	61.566311
2045.071080	104.905451	61.571316
2044.886591	101.615125	61.576321
2044.556597	97.223481	61.581326
2042.962979	105.971763	61.586330
2042.275406	98.855014	61.591335
2042.293715	96.860350	61.596340
2041.694858	101.785787	61.601345
2040.807689	102.935876	61.606350
2039.505940	105.123200	61.611354
2039.887992	93.378490	61.616359
2038.728885	99.134033	61.621364
2037.772868	96.352518	61.626369
2037.357988	90.419415	61.631374
2037.025169	97.217122	61.636378
2036.154280	100.656029	61.641383
2035.426332	97.809934	61.646388
2034.979325	96.754896	61.651393
2034.407335	87.930832	61.656398
2033.426886	100.931203	61.661402
2033.080035	98.336876	61.666407
2032.282325	104.834615	61.671412
2031.784061	92.587769	61.676417
2031.424894	94.892021	61.681422
2030.629796	95.568591	61.686426
2029.572960	95.425651	61.691431
2028.641294	97.142645	61.696436
2027.855981	107.423249	61.701441
2027.778775	92.438121	61.706446
2026.934305	92.228362	61.711450
2025.804633	90.461622	61.716455
2025.539757	103.245926	61.721460
2025.292844	90.065028	61.726465
2024.791831	92.033810	61.731470
2023.399793	92.311514	61.736474
2023.304058	87.256625	61.741479
2022.797281	96.091054	61.746484
2022.007503	96.287370	61.751489
2021.625917	90.041469	61.756494
2019.758570	95.258114	61.761498
2019.280510	93.766444	61.766503
2018.793815	102.857897	61.771508
2018.806495	88.736905	61.776513
2018.321761	86.724305	61.781518
2016.902588	95.668843	61.786522
2016.748154	85.691956	61.791527
2015.682519	86.517126	61.796532
2015.291854	90.297729	61.801537
2014.837286	93.284199	61.806542
2014.021715	95.705044	61.811546
2012.712235	91.820533	61.816551
2012.346519	87.221671	61.821556
2011.472373	97.068498	61.826561
2011.206777	89.705013	61.831566
2010.363003	92.964573	61.836570
2009.854722	91.004599	61.841575
2009.081834	95.124997	61.846580
2008.273911	92.264795	61.851585
2007.927981	99.629157	61.856590
2007.305819	98.778548	61.861594
2006.860658	95.058073	61.866599
2006.317176	93.264540	61.871604
2005.538572	96.688808	61.876609
2005.056439	88.924437	61.881614
2003.341402	91.447038	61.886618
2002.811211	90.808924	61.891623
2002.291282	90.268533	61.896628
2002.194850	94.426655	61.901633
2001.449536	92.494841	61.906638
2000.805450	92.992905	61.911642
2000.390945	91.032242	61.916647
1999.572821	92.439477	61.921652
1998.978383	95.937023	61.926657
1998.016392	88.835462	61.931662
1996.667272	93.922561	61.936666
1996.328334	85.728597	61.941671
1996.075829	87.353578	61.946676
1995.393478	90.805149	61.951681
1994.890857	82.225567	61.956686
1994.173878	87.472541	61.961690
1993.727923	83.138740	61.966695
1993.391535	85.481958	61.971700
1991.812278	94.582807	61.976705
1990.860337	84.839739	61.981710
1990.575289	97.622508	61.986714
1990.495015	97.955391	61.991719
1989.523581	99.614053	61.996724
1988.856184	96.722090	62.001729
1988.254531	95.576485	62.006734
1988.011075	88.518585	62.011738
1986.934433	97.577512	62.016743
1985.765127	95.643608	62.021748
1984.902183	93.760432	62.026753
1984.796438	85.767587	62.031758
1984.052446	100.111899	62.036762
1983.669777	97.534304	62.041767
1983.159069	93.761157	62.046772
1982.208620	100.611167	62.051777
1982.087901	90.285142	62.056782
1981.218943	96.295862	62.061786
1979.943922	89.442697	62.066791
1978.969302	94.159691	62.071796
1978.147058	90.727741	62.076801
1978.933879	93.570798	62.081806
1977.762987	92.260070	62.086810
1977.173296	90.576385	62.091815
1976.601662	91.566021	62.096820
1975.962768	95.624158	62.101825
1974.936710	90.734283	62.106830
1973.395025	92.630124	62.111834
1973.101658	82.408783	62.116839
1973.035967	89.438491	62.121844
1972.375771	99.521038	62.126849
1971.925484	89.340370	62.131854
1970.804543	99.387234	62.136858
1970.792404	90.963200	62.141863
1970.374172	96.656368	62.146868
1968.928057	90.196232	62.151873
1968.346731	89.654554	62.156878
1967.842050	96.224068	62.161882
1967.291151	91.500059	62.166887
1966.881720	92.005041	62.171892
1965.779936	98.106340	62.176897
1964.857449	91.534706	62.181902
1964.127280	101.349231	62.186906
1963.601104	90.466224	62.191911
1962.937243	98.658517	62.196916
1962.646514	88.227014	62.201921
1962.484011	91.818437	62.206926
1961.027194	101.065456	62.211930
1960.052079	92.959860	62.216935
1959.336130	91.900215	62.221940
1958.485823	101.755888	62.226945
1958.794740	90.415464	62.231950
1957.884342	94.994534	62.236954
1957.534389	94.244239	62.241959
1956.966419	87.922277	62.246964
1956.011936	99.264259	62.251969
1955.181524	89.639115	62.256974
1954.136794	95.122634	62.261978
1953.412860	81.183241	62.266983
1952.936868	90.649898	62.271988
1952.364630	92.071736	62.276993
1952.130355	86.207760	62.281998
1951.464827	91.375611	62.287002
1950.764554	88.518843	62.292007
1950.116046	93.553103	62.297012
1948.898184	99.335353	62.302017
1948.358964	91.411317	62.307022
1947.722737	95.992603	62.312026
1947.279591	91.995844	62.317031
1946.983910	85.988646	62.322036
1946.255429	100.259535	62.327041
1945.468740	95.776393	62.332046
1944.267390	92.234314	62.337050
1943.561819	88.075778	62.342055
1943.212302	86.716690	62.347060
1942.527550	89.175138	62.352065
1942.319550	85.429649	62.357070
1941.763988	93.546403	62.362074
1940.905606	91.399157	62.367079
1939.841413	87.748574	62.372084
1939.047165	88.514925	62.377089
1938.722712	79.843998	62.382094
1937.944105	94.447703	62.387098
1937.549804	80.910171	62.392103
1937.101053	86.704380	62.397108
1935.962062	83.221798	62.402113
1935.054223	79.134800	62.407118
1934.294993	88.800965	62.412122
1933.674336	85.518388	62.417127
1933.262053	82.357282	62.422132
1932.511732	91.047442	62.427137
1932.291554	91.389919	62.432142
1931.918005	93.338483	62.437146
1931.358535	83.670343	62.442151
1930.449464	77.740020	62.447156
1929.312162	81.785813	62.452161
1928.804157	72.954789	62.457166
1928.110105	93.359501	62.462170
1927.713742	92.991905	62.467175
1926.991096	89.810677	62.472180
1925.755996	91.358246	62.477185
1925.272368	88.763572	62.482190
1924.824986	86.286152	62.487194
1924.558564	86.046169	62.492199
1923.721868	81.837491	62.497204
1923.164280	97.508445	62.502209
1921.853712	90.878582	62.507214
1921.288557	91.133892	62.512218
1920.584954	85.413813	62.517223
1920.328200	95.550595	62.522228
1919.356504	95.186019	62.527233
1919.097895	90.626943	62.532238
1918.615339	94.571960	62.537242
1917.100723	94.500159	62.542247
1916.555119	92.675444	62.547252
1916.107402	93.248015	62.552257
1915.414102	90.088941	62.557262
1914.844350	92.970703	62.562266
1914.503578	86.596917	62.567271
1914.339896	88.302425	62.572276
1913.310446	92.960332	62.577281
1912.395653	82.113808	62.582286
1911.626330	82.862017	62.587290
1911.161242	91.642525	62.592295
1910.500063	89.251088	62.597300
1909.173054	95.823414	62.602305
1908.703741	86.631418	62.607310
1908.397931	94.213348	62.612314
1907.802499	89.772401	62.617319
1907.175574	83.027714	62.622324
1906.709561	91.980264	62.627329
1905.727916	79.315026	62.632334
1905.013431	92.697412	62.637338
1904.425374	93.361652	62.642343
1903.844915	85.016810	62.647348
1903.035798	95.479409	62.652353
1902.571766	92.695541	62.657358
1901.327596	87.039205	62.662362
1900.555599	85.048578	62.667367
1900.259330	89.454472	62.672372
1899.814229	91.141576	62.677377
1899.310094	84.733802	62.682382
1898.925198	95.873404	62.687386
1898.177119	85.173889	62.692391
1897.205170	86.667078	62.697396
1896.239922	92.398204	62.702401
1895.714679	79.849756	62.707406
1895.131739	89.073189	62.712410
1894.624028	88.109819	62.717415
1894.190614	81.493694	62.722420
1893.292401	95.102378	62.727425
1892.833772	86.681424	62.732430
1892.159445	90.582769	62.737434
1891.296556	85.703300	62.742439
1890.217906	81.996687	62.747444
1889.463441	86.669295	62.752449
1888.694641	86.182630	62.757454
1888.380792	84.750076	62.762458
1887.508428	94.886816	62.767463
1887.405639	83.777344	62.772468
1887.146736	86.628685	62.777473
1886.514375	89.506198	62.782478
1885.138764	95.021769	62.787482
1884.202981	91.240433	62.792487
1883.952853	90.182554	62.797492
1883.608437	96.316612	62.802497
1883.099343	87.506266	62.807502
1881.650751	82.360230	62.812506
1880.847091	85.988785	62.817511
1880.692574	88.869287	62.822516
1879.802328	89.907949	62.827521
1879.705993	82.784135	62.832526
1879.117380	92.571463	62.837530
1877.522512	87.178982	62.842535
1877.164298	84.859309	62.847540
1876.090102	88.317921	62.852545
1876.028533	84.785743	62.857550
1875.767529	87.099658	62.862554
1875.052838	81.635254	62.867559
1874.023129	82.727599	62.872564
1872.952131	83.875386	62.877569
1872.447590	85.728055	62.882574
1871.955866	91.917039	62.887578
1871.581702	93.154477	62.892583
1871.379758	89.139942	62.897588
1869.752404	95.589652	62.902593
1869.112826	88.886408	62.907598
1868.218475	89.375350	62.912602
1868.380380	89.825910	62.917607
1867.871338	91.020105	62.922612
1867.121246	96.117819	62.927617
1866.285131	89.029449	62.932622
1865.549824	94.241514	62.937626
1864.605510	89.198357	62.942631
1864.482447	91.957168	62.947636
1863.170915	103.217085	62.952641
1862.427932	88.828146	62.957646
1861.953658	86.132650	62.962650
1861.042360	86.110180	62.967655
1860.497642	83.261860	62.972660
1860.312046	95.757587	62.977665
1859.978783	93.829784	62.982670
1859.465447	91.571012	62.987674
1858.423648	84.895362	62.992679
1857.561864	82.397015	62.997684
1856.674783	93.229980	63.002689
1856.433049	89.527704	63.007694
1855.889274	89.027400	63.012698
1854.565988	90.084359	63.017703
1854.131081	88.412400	63.022708
1853.446064	91.279356	63.027713
1853.314213	96.740980	63.032718
1852.409080	91.835114	63.037722
1851.230233	92.239915	63.042727
1851.090562	75.798139	63.047732
1850.051980	93.716998	63.052737
1849.667247	86.052327	63.057742
1849.108595	90.004704	63.062746
1848.440518	84.741071	63.067751
1847.584001	85.602494	63.072756
1846.707359	95.087041	63.077761
1846.348890	84.518082	63.082766
1845.910337	88.408812	63.087770
1845.164537	87.798655	63.092775
1844.046977	85.437119	63.097780
1843.187132	93.255255	63.102785
1842.763916	87.047544	63.107790
1842.255894	89.955789	63.112794
1841.637770	91.556828	63.117799
1841.483436	86.096507	63.122804
1840.896693	85.158312	63.127809
1840.060688	83.132134	63.132814
1839.241844	80.114448	63.137818
1838.384889	90.471107	63.142823
1837.269291	82.091401	63.147828
1836.273398	90.476783	63.152833
1836.411052	88.243970	63.157838
1835.815398	87.712482	63.162842
1835.009351	89.715535	63.167847
1834.657914	86.036989	63.172852
1834.152327	90.922416	63.177857
1833.758983	90.119102	63.182862
1832.739309	96.450268	63.187866
1831.828737	93.104935	63.192871
1831.174812	83.395053	63.197876
1829.873204	85.069923	63.202881
1829.329470	89.658622	63.207886
1828.920811	94.579125	63.212890
1828.064716	92.474135	63.217895
1827.967758	85.724175	63.222900
1827.431282	101.199390	63.227905
1827.078445	75.296297	63.232910
1825.784257	84.533314	63.237914
1824.745844	86.218438	63.242919
1824.672635	78.485389	63.247924
1823.873755	84.719992	63.252929
1823.811956	75.949040	63.257934
1822.692403	79.981016	63.262938
1821.482549	87.110382	63.267943
1821.102588	79.829753	63.272948
1820.603249	88.443811	63.277953
1820.552511	78.537232	63.282958
1818.920283	83.857025	63.287962
1818.186566	79.521645	63.292967
1817.768053	76.298471	63.297972
1817.014844	83.383715	63.302977
1817.077295	80.707089	63.307982
1816.672698	87.650246	63.312986
1815.422867	86.060381	63.317991
1814.792443	88.973873	63.322996
1813.747769	85.891124	63.328001
1813.471299	86.185776	63.333006
1812.400063	87.743648	63.338010
1811.420324	85.033802	63.343015
1811.005548	79.927089	63.348020
1810.278259	88.410180	63.353025
1809.948865	80.793507	63.358030
1809.907664	82.064817	63.363034
1809.267318	86.299839	63.368039
1808.541914	86.315681	63.373044
1807.375321	99.935460	63.378049
1806.902889	77.225881	63.383054
1805.751769	84.293884	63.388058
1804.800819	88.021544	63.393063
1804.315736	80.743418	63.398068
1803.672614	84.847990	63.403073
1803.532298	88.204073	63.408078
1803.188333	89.566039	63.413082
1802.729136	79.941947	63.418087
1802.111683	82.030182	63.423092
1800.761707	86.152376	63.428097
1800.172737	78.214212	63.433102
1799.120450	77.454034	63.438106
1798.134816	83.186846	63.443111
1797.651532	70.718513	63.448116
1797.182709	83.204004	63.453121
1796.872870	76.620324	63.458126
1796.215857	83.076842	63.463130
1795.799336	89.427364	63.468135
1795.559873	83.688820	63.473140
1794.196931	83.804325	63.478145
1793.717897	84.285691	63.483150
1793.030548	84.867948	63.488154
1792.078519	89.106734	63.493159
1791.090116	90.359714	63.498164
1790.479514	83.393268	63.503169
1789.997153	82.686100	63.508174
1789.790886	84.770549	63.513178
1789.391309	83.596058	63.518183
1788.398726	83.088186	63.523188
1787.417114	87.834736	63.528193
1786.922874	82.649179	63.533198
1786.238892	81.926718	63.538202
1785.781027	82.237561	63.543207
1785.154494	78.200574	63.548212
1783.966738	81.683559	63.553217
1783.502137	84.714231	63.558222
1782.673951	83.213551	63.563226
1782.455610	87.364219	63.568231
1781.942504	78.925142	63.573236
1780.832674	91.204914	63.578241
1780.082363	75.445192	63.583246
1779.514624	87.321901	63.588250
1778.947808	90.305727	63.593255
1778.737428	82.403646	63.598260
1777.573276	83.938437	63.603265
1776.784447	78.459031	63.608270
1776.629971	92.064751	63.613274
1775.921668	86.408546	63.618279
1775.460229	80.937076	63.623284
1774.415286	81.815828	63.628289
1773.808801	86.211066	63.633294
1773.435510	81.509371	63.638298
1771.535819	77.436436	63.643303
1771.124863	82.959723	63.648308
1770.476760	89.209823	63.653313
1770.841761	82.887999	63.658318
1770.069663	82.102262	63.663322
1769.004292	82.755594	63.668327
1768.860469	78.981012	63.673332
1768.216879	85.280858	63.678337
1766.862875	90.359374	63.683342
1766.289204	86.313995	63.688346
1765.700746	92.182451	63.693351
1765.242653	80.441851	63.698356
1764.311758	89.791521	63.703361
1763.629356	87.461845	63.708366
1763.515437	85.239018	63.713370
1762.361242	91.862813	63.718375
1761.879683	90.081581	63.723380
1760.561125	89.019916	63.728385
1760.092140	84.437501	63.733390
1759.734982	83.456559	63.738394
1758.960565	84.399592	63.743399
1759.035292	85.573642	63.748404
1758.272454	86.469104	63.753409
1757.474095	83.721015	63.758414
1756.720419	83.864367	63.763418
1756.090862	80.226850	63.768423
1755.229070	71.789539	63.773428
1753.922442	90.845423	63.778433
1753.613699	85.866965	63.783438
1753.378232	92.920471	63.788442
1752.716670	83.453111	63.793447
1752.425283	82.789742	63.798452
1751.115118	79.758646	63.803457
1750.527543	76.887196	63.808462
1749.956930	82.672390	63.813466
1749.373217	88.945385	63.818471
1748.873980	78.413005	63.823476
1747.592285	71.646197	63.828481
1747.076883	78.118080	63.833486
1746.634467	77.694747	63.838490
1745.878163	74.410110	63.843495
1745.806911	80.639566	63.848500
1744.624273	90.596943	63.853505
1743.972549	80.027276	63.858510
1743.407791	82.602336	63.863514
1742.826463	77.181455	63.868519
1742.127799	75.910963	63.873524
1740.849273	81.297634	63.878529
1740.260104	81.526832	63.883534
1739.954275	82.171519	63.888538
1739.520664	85.302936	63.893543
1739.081391	72.032820	63.898548
1737.997647	80.883200	63.903553
1737.142387	76.453605	63.908558
1736.570158	81.020033	63.913562
1735.676879	89.862248	63.918567
1735.762394	85.291128	63.923572
1735.043162	88.379595	63.928577
1733.883269	86.491626	63.933582
1733.462110	90.770704	63.938586
1732.804809	89.351714	63.943591
1732.681937	81.369510	63.948596
1731.521498	85.332320	63.953601
1730.603747	85.085408	63.958606
1730.091647	81.025530	63.963610
1729.493571	85.449403	63.968615
1729.302257	79.996548	63.973620
1727.905092	87.942623	63.978625
1727.268279	86.122976	63.983630
1726.858349	88.405359	63.988634
1726.163964	82.016808	63.993639
1725.873423	74.529608	63.998644
1724.702291	82.288391	64.003649
1724.197118	84.625326	64.008654
1723.672582	81.956766	64.013658
1723.025233	90.506029	64.018663
1722.017240	82.186567	64.023668
1720.974535	84.627796	64.028673
1720.624489	83.634691	64.033678
1720.345273	82.737572	64.038682
1719.759130	87.252596	64.043687
1719.354131	85.842427	64.048692
1717.905906	88.865321	64.053697
1717.190437	83.888387	64.058702
1716.967764	82.884515	64.063706
1716.454255	87.277613	64.068711
1715.956848	74.768966	64.073716
1714.879290	75.130932	64.078721
1713.792957	78.809156	64.083726
1713.423469	77.325538	64.088730
1712.871701	79.756609	64.093735
1712.852876	77.140203	64.098740
1711.411619	88.436539	64.103745
1710.704427	88.452669	64.108750
1710.468465	81.371552	64.113754
1709.787437	86.712228	64.118759
1709.342610	78.874205	64.123764
1707.972346	83.818129	64.128769
1707.255053	85.425486	64.133774
1707.178539	82.796164	64.138778
1706.206163	86.244974	64.143783
1706.366591	86.787225	64.148788
1705.066011	92.346157	64.153793
1704.114437	94.271433	64.158798
1703.999570	86.686940	64.163802
1703.303225	83.435372	64.168807
1702.490803	76.852683	64.173812
1701.656665	86.322621	64.178817
1701.126634	90.229475	64.183822
1700.548103	80.829375	64.188826
1699.740262	87.935940	64.193831
1699.044378	80.270262	64.198836
1698.203070	95.637768	64.203841
1697.584448	85.185863	64.208846
1697.482078	86.148334	64.213850
1696.095882	87.929747	64.218855
1695.415627	79.712791	64.223860
1694.637401	88.196108	64.228865
1694.061366	83.796298	64.233870
1694.293243	77.213332	64.238874
1693.585332	85.936224	64.243879
1693.075717	78.310353	64.248884
1692.004826	86.936352	64.253889
1691.269362	92.468612	64.258894
1690.742284	87.589501	64.263898
1689.566154	80.246118	64.268903
1689.238699	81.353153	64.273908
1688.418154	95.315405	64.278913
1687.646060	88.945514	64.283918
1687.631882	73.674486	64.288922
1686.552511	86.468277	64.293927
1685.612973	79.081011	64.298932
1684.836186	82.341061	64.303937
1684.478950	84.258677	64.308942
1684.306225	80.700011	64.313946
1682.986889	77.517440	64.318951
1682.553624	76.636909	64.323956
1681.814676	78.156245	64.328961
1681.302268	72.328609	64.333966
1680.896977	80.889890	64.338970
1679.500517	84.103283	64.343975
1678.880373	74.831234	64.348980
1678.015754	77.621096	64.353985
1677.853005	81.434919	64.358990
1677.502544	78.106343	64.363994
1677.143480	78.450399	64.368999
1676.698263	74.479264	64.374004
1675.354896	79.094067	64.379009
1674.961945	77.098501	64.384014
1674.578624	73.000837	64.389018
1673.029834	86.733392	64.394023
1672.654557	79.196578	64.399028
1672.127572	74.902530	64.404033
1671.540189	75.972003	64.409038
1670.465181	79.839262	64.414042
1669.680403	74.729849	64.419047
1669.518454	79.218502	64.424052
1668.884265	83.176598	64.429057
1668.386676	75.566172	64.434062
1667.216987	72.476538	64.439066
1666.177179	86.109325	64.444071
1666.005747	78.753030	64.449076
1665.963727	83.198980	64.454081
1664.703015	75.096315	64.459086
1663.911975	68.909231	64.464090
1662.962682	82.146002	64.469095
1662.681130	76.841536	64.474100
1662.252515	85.863856	64.479105
1661.668974	79.924515	64.484110
1661.310183	76.168320	64.489114
1660.154068	79.439742	64.494119
1659.928397	79.366784	64.499124
1658.767985	86.669714	64.504129
1657.800297	86.004969	64.509134
1657.385887	81.014928	64.514138
1656.855561	84.989646	64.519143
1656.502452	75.139005	64.524148
1655.470924	89.451748	64.529153
1654.285771	83.732553	64.534158
1654.013245	77.888896	64.539162
1653.253650	83.447073	64.544167
1653.129346	69.625467	64.549172
1652.808389	74.744946	64.554177
1651.661982	82.760035	64.559182
1650.893433	73.191438	64.564186
1650.261386	76.523125	64.569191
1649.630583	74.229444	64.574196
1648.255838	73.088451	64.579201
1647.501197	73.683010	64.584206
1647.651543	76.918803	64.589210
1646.747137	78.480201	64.594215
1646.748941	70.837766	64.599220
1646.335861	80.734430	64.604225
1645.286162	80.868065	64.609230
1644.483087	66.238047	64.614234
1643.865724	77.949172	64.619239
1642.894685	76.270952	64.624244
1642.255467	77.414900	64.629249
1641.290013	74.155636	64.634254
1640.866523	68.017411	64.639258
1640.086891	72.206778	64.644263
1639.758025	74.372211	64.649268
1638.919717	69.482632	64.654273
1638.169635	81.344158	64.659278
1637.742431	76.477585	64.664282
1637.200045	71.995175	64.669287
1636.650283	73.076026	64.674292
1635.453678	78.702048	64.679297
1634.711070	77.394411	64.684302
1634.377426	69.966119	64.689306
1634.018529	80.204271	64.694311
1633.050959	69.626476	64.699316
1632.244676	70.571453	64.704321
1631.767973	75.198418	64.709326
1631.494354	78.563061	64.714330
1630.415798	74.526959	64.719335
1629.679320	64.593725	64.724340
1629.003580	77.474798	64.729345
1628.509107	75.963737	64.734350
1628.151118	70.494797	64.739354
1626.934757	71.211596	64.744359
1626.321301	73.371776	64.749364
1625.709409	73.164626	64.754369
1625.428236	80.504517	64.759374
1624.896435	79.401522	64.764378
1623.638811	72.782352	64.769383
1622.889883	64.916972	64.774388
1622.252524	68.369359	64.779393
1621.693866	79.270045	64.784398
1621.726882	67.397864	64.789402
1620.416162	85.729009	64.794407
1619.936994	74.177893	64.799412
1619.504935	75.501832	64.804417
1618.395156	72.104651	64.809422
1617.645344	61.875489	64.814426
1616.426163	68.872361	64.819431
1616.470800	73.714561	64.824436
1615.869058	70.049012	64.829441
1615.388616	70.436013	64.834446
1615.048685	69.482319	64.839450
1613.960060	74.025141	64.844455
1613.682746	74.302600	64.849460
1612.867945	72.094932	64.854465
1611.605966	72.858410	64.859470
1611.219472	71.953116	64.864474
1610.500152	77.982733	64.869479
1610.123965	72.696465	64.874484
1609.320384	70.367164	64.879489
1608.146906	80.608563	64.884494
1607.560499	73.105308	64.889498
1607.012978	78.448447	64.894503
1607.028246	69.752016	64.899508
1606.528624	69.916555	64.904513
1605.420381	69.960155	64.909518
1604.582153	65.878003	64.914522
1604.261893	71.973538	64.919527
1603.817710	67.401418	64.924532
1602.638168	80.659010	64.929537
1601.814555	75.049572	64.934542
1601.627416	72.267516	64.939546
1600.579498	79.555746	64.944551
1599.355269	67.586825	64.949556
1598.825671	72.652718	64.954561
1598.319133	67.740411	64.959566
1598.195430	69.310265	64.964570
1597.420747	74.460828	64.969575
1597.214562	76.210948	64.974580
1596.768746	71.027211	64.979585
1595.464416	78.144860	64.984590
1594.766942	73.031066	64.989594
1593.985709	73.159919	64.994599
1593.143264	72.448493	64.999604
1592.547692	73.934035	65.004609
1591.831310	77.523568	65.009614
1591.416474	68.477564	65.014618
1591.011002	72.698967	65.019623
1590.413109	70.228181	65.024628
1589.389073	66.410526	65.029633
1588.733211	68.798230	65.034638
1588.707739	71.287640	65.039642
1587.509879	81.914555	65.044647
1586.510192	77.424382	65.049652
1585.882245	78.713213	65.054657
1585.161337	78.605396	65.059662
1585.044451	67.991828	65.064666
1584.176846	81.147827	65.069671
1583.889695	72.084691	65.074676
1582.890446	76.327888	65.079681
1581.751697	70.461011	65.084686
1581.988374	70.686778	65.089690
1581.002459	76.582132	65.094695
1580.107829	72.699764	65.099700
1579.310897	81.763257	65.104705
1578.803753	72.881734	65.109710
1578.700028	71.034206	65.114714
1577.320524	72.513407	65.119719
1577.092651	71.606572	65.124724
1576.286113	75.284551	65.129729
1575.903969	70.426604	65.134734
1574.936562	60.821040	65.139738
1574.396676	72.252558	65.144743
1573.802931	64.848258	65.149748
1573.264242	78.213781	65.154753
1572.370532	71.139419	65.159758
1571.722707	70.824447	65.164762
1570.715642	81.422631	65.169767
1570.330822	76.899434	65.174772
1569.814710	71.050338	65.179777
1568.818734	76.720206	65.184782
1568.426632	71.386012	65.189786
1567.443270	72.930017	65.194791
1567.245971	61.904230	65.199796
1566.709272	68.549043	65.204801
1565.169981	69.635732	65.209806
1564.920923	63.427234	65.214810
1564.132705	70.641093	65.219815
1563.958780	64.756559	65.224820
1563.203228	67.399811	65.229825
1562.026118	69.987035	65.234830
1561.662586	58.822078	65.239834
1561.073436	65.744891	65.244839
1560.692371	66.800531	65.249844
1559.723021	63.413397	65.254849
1558.826047	67.027685	65.259854
1558.492870	71.638163	65.264858
1557.893467	72.906695	65.269863
1557.407536	66.310041	65.274868
1556.284298	71.555417	65.279873
1555.527368	72.606120	65.284878
1555.241285	68.874665	65.289882
1554.632356	73.994171	65.294887
1554.311755	67.672457	65.299892
1552.978356	78.246797	65.304897
1552.233649	71.407398	65.309902
1552.073402	71.018116	65.314906
1550.888600	73.546641	65.319911
1550.187161	76.017292	65.324916
1549.392938	70.620833	65.329921
1548.911893	77.872629	65.334926
1549.002742	69.424401	65.339930
1548.097535	78.751113	65.344935
1547.481108	67.830556	65.349940
1546.753310	71.592228	65.354945
1545.743154	70.920080	65.359950
1545.533843	66.914647	65.364954
1544.573460	71.304649	65.369959
1543.696672	72.543139	65.374964
1543.528689	67.673250	65.379969
1542.942257	76.827884	65.384974
1541.895422	67.527485	65.389978
1540.773812	70.489111	65.394983
1540.642034	73.764988	65.399988
1540.110217	69.419701	65.404993
1539.378323	81.314623	65.409998
1538.343514	68.177047	65.415002
1537.216832	77.619378	65.420007
1536.909493	77.460056	65.425012
1536.606442	74.548185	65.430017
1536.169248	75.921840	65.435022
1536.082953	68.917906	65.440026
1535.096434	76.204285	65.445031
1534.404355	73.341612	65.450036
1533.367520	73.307663	65.455041
1531.829698	78.945364	65.460046
1531.671625	72.802837	65.465050
1530.953815	77.767756	65.470055
1530.813439	72.879288	65.475060
1530.187960	75.164404	65.480065
1529.829452	72.102070	65.485070
1528.831198	63.556441	65.490074
1528.006389	75.993630	65.495079
1527.797993	69.393886	65.500084
1526.532738	70.637334	65.505089
1525.708344	74.357588	65.510094
1525.532589	67.576824	65.515098
1524.944415	73.867114	65.520103
1524.223436	69.965062	65.525108
1523.265777	73.559831	65.530113
1522.255660	76.197811	65.535118
1522.309335	69.169273	65.540122
1521.661045	73.018457	65.545127
1520.996141	68.993164	65.550132
1519.753931	77.819115	65.555137
1519.330261	83.101588	65.560142
1519.344359	69.932186	65.565146
1518.277384	72.075350	65.570151
1517.438757	63.756683	65.575156
1516.572454	68.070241	65.580161
1515.681537	74.761887	65.585166
1515.489307	62.404316	65.590170
1514.939437	70.586439	65.595175
1514.607968	72.762549	65.600180
1513.876672	74.592960	65.605185
1512.768235	71.646637	65.610190
1512.629218	72.209647	65.615194
1511.305703	66.519616	65.620199
1510.530959	76.834097	65.625204
1510.092318	67.425245	65.630209
1509.400264	76.556453	65.635214
1509.037477	64.468841	65.640218
1508.236361	67.366937	65.645223
1507.281321	68.403400	65.650228
1506.882767	58.758731	65.655233
1506.333099	63.567619	65.660238
1506.456002	62.636592	65.665242
1504.860961	67.482280	65.670247
1504.433120	64.184956	65.675252
1503.906152	67.662405	65.680257
1502.668108	69.152283	65.685262
1501.925287	54.866018	65.690266
1501.482981	73.498383	65.695271
1500.793458	63.891275	65.700276
1500.564422	70.543192	65.705281
1499.997452	78.531703	65.710286
1499.010752	67.760678	65.715290
1498.102206	68.903301	65.720295
1497.618109	73.555113	65.725300
1497.073691	70.462400	65.730305
1496.249468	67.944023	65.735310
1495.566587	64.524798	65.740314
1494.610994	75.878876	65.745319
1494.277203	64.184065	65.750324
1493.906915	65.390970	65.755329
1493.280008	65.094772	65.760334
1492.243900	62.539103	65.765338
1491.420437	65.768769	65.770343
1491.093113	69.228689	65.775348
1490.746756	72.221687	65.780353
1489.775380	78.856739	65.785358
1489.031570	71.158544	65.790362
1488.196914	74.541384	65.795367
1487.816114	68.006891	65.800372
1487.700571	69.824618	65.805377
1486.482520	67.420868	65.810382
1486.166409	65.753758	65.815386
1485.130259	73.939042	65.820391
1484.139435	73.937226	65.825396
1483.329804	74.983708	65.830401
1482.561021	73.377493	65.835406
1482.255119	65.607348	65.840410
1481.824644	67.650168	65.845415
1481.310620	72.216848	65.850420
1481.008212	70.378821	65.855425
1480.157825	78.339830	65.860430
1479.643451	70.352858	65.865434
1478.885122	75.380999	65.870439
1477.963722	74.371489	65.875444
1477.498453	71.796075	65.880449
1476.586329	74.825365	65.885454
1475.307712	70.816397	65.890458
1474.621552	71.269233	65.895463
1474.057700	73.440485	65.900468
1474.105985	68.943103	65.905473
1473.333149	75.422813	65.910478
1473.064303	72.010338	65.915482
1471.950903	75.193045	65.920487
1471.307565	71.882662	65.925492
1471.054885	70.166048	65.930497
1470.045640	73.284894	65.935502
1469.159058	62.000435	65.940506
1468.629960	72.018044	65.945511
1467.819717	69.137899	65.950516
1467.396142	71.390943	65.955521
1466.332284	76.254746	65.960526
1465.540744	72.485354	65.965530
1465.063113	74.986693	65.970535
1465.073516	66.166467	65.975540
1464.501546	68.227044	65.980545
1463.209870	77.310833	65.985550
1462.552621	70.202094	65.990554
1461.853371	71.879187	65.995559
1461.399428	72.793454	66.000564
1461.129609	71.513240	66.005569
1459.526157	69.295334	66.010574
1459.391620	70.628787	66.015578
1458.430729	70.425099	66.020583
1458.400931	67.036141	66.025588
1457.741023	68.353735	66.030593
1456.612898	63.483476	66.035598
1456.285133	61.496515	66.040602
1455.623981	67.207825	66.045607
1454.429931	65.629779	66.050612
1453.814855	65.746461	66.055617
1453.233069	67.788099	66.060622
1453.106660	66.787879	66.065626
1452.260193	70.929565	66.070631
1451.554989	69.237560	66.075636
1450.663302	71.473534	66.080641
1450.115708	69.724941	66.085646
1449.844317	59.637441	66.090650
1448.364063	72.903439	66.095655
1447.682690	68.793262	66.100660
1447.261338	62.156413	66.105665
1446.654250	71.408958	66.110670
1446.528732	70.938468	66.115674
1445.981188	75.371706	66.120679
1445.128829	62.325042	66.125684
1444.233703	62.352188	66.130689
1443.440803	63.946395	66.135694
1442.783590	55.052502	66.140698
1441.825027	64.580105	66.145703
1441.496019	59.541852	66.150708
1440.998412	63.760564	66.155713
1440.438507	68.254114	66.160718
1439.612501	62.700319	66.165722
1438.537002	69.308562	66.170727
1437.916332	68.032070	66.175732
1437.790564	64.834990	66.180737
1437.247945	68.712341	66.185742
1436.162489	60.517307	66.190746
1435.499724	68.812001	66.195751
1435.009667	59.751189	66.200756
1434.615161	63.605000	66.205761
1433.420947	60.670772	66.210766
1433.021511	59.535745	66.215770
1432.304373	69.212646	66.220775
1431.543030	66.722146	66.225780
1431.049522	62.287220	66.230785
1430.139431	68.293573	66.235790
1429.834148	62.251734	66.240794
1429.379491	65.025400	66.245799
1428.342183	69.974883	66.250804
1427.502743	64.937328	66.255809
1426.613154	71.076047	66.260814
1426.528157	62.211064	66.265818
1425.750816	70.293729	66.270823
1425.122839	72.071471	66.275828
1424.464424	65.128517	66.280833
1423.589490	65.917306	66.285838
1423.279652	64.304402	66.290842
1422.586771	73.449158	66.295847
1421.512320	64.328259	66.300852
1420.739141	64.900598	66.305857
1420.131964	66.979395	66.310862
1420.279359	56.871077	66.315866
1419.110403	63.211896	66.320871
1418.397579	63.967036	66.325876
1417.813242	68.221615	66.330881
1417.324172	68.975887	66.335886
1416.673505	52.218053	66.340890
1415.297206	63.663450	66.345895
1415.074761	60.532202	66.350900
1414.600568	65.556197	66.355905
1413.914216	67.988211	66.360910
1412.942083	59.108108	66.365914
1412.046280	62.335102	66.370919
1411.592392	58.419024	66.375924
1411.371147	62.202720	66.380929
1410.705763	60.930189	66.385934
1409.994375	60.194840	66.390938
1408.887346	68.175362	66.395943
1408.313382	60.510921	66.400948
1408.075299	60.526693	66.405953
1407.180779	64.970926	66.410958
1406.475268	59.719700	66.415962
1405.586889	55.498935	66.420967
1405.168586	58.765156	66.425972
1404.982031	58.607154	66.430977
1403.909261	61.472758	66.435982
1403.465440	54.806377	66.440986
1402.524074	58.616219	66.445991
1402.059163	63.346995	66.450996
1400.926496	59.171366	66.456001
1399.932360	66.939975	66.461006
1399.742534	59.909938	66.466010
1399.675761	67.698312	66.471015
1399.176700	68.107236	66.476020
1398.379050	64.815094	66.481025
1397.108547	73.250549	66.486030
1397.077403	60.082845	66.491034
1395.763445	63.967681	66.496039
1394.508625	69.860099	66.501044
1394.076469	61.141766	66.506049
1393.520256	70.911372	66.511054
1393.431791	65.464298	66.516058
1393.111551	66.004077	66.521063
1392.299890	65.923355	66.526068
1391.887962	54.604496	66.531073
1390.585365	66.270009	66.536078
1390.532280	67.033838	66.541082
1389.129577	70.267291	66.546087
1388.560343	59.296717	66.551092
1388.098718	63.479755	66.556097
1387.283256	76.676386	66.561102
1387.116325	63.643807	66.566106
1385.758317	68.989642	66.571111
1385.024183	64.277574	66.576116
1384.671872	63.595547	66.581121
1384.268164	66.646558	66.586126
1384.000411	62.456465	66.591130
1383.250430	59.962599	66.596135
1382.284141	62.483272	66.601140
1381.510107	65.296671	66.606145
1380.383025	67.858673	66.611150
1379.915027	59.308473	66.616154
1379.516439	63.345870	66.621159
1379.074104	63.266374	66.626164
1378.387877	63.897445	66.631169
1376.932640	65.294167	66.636174
1376.756740	57.146984	66.641178
1376.321315	64.676977	66.646183
1375.370489	71.875724	66.651188
1374.605307	60.709213	66.656193
1373.786530	65.963033	66.661198
1373.327146	68.068812	66.666202
1373.168353	62.666037	66.671207
1372.778763	62.442536	66.676212
1371.571678	62.352133	66.681217
1370.670227	69.544609	66.686222
1370.499544	63.473500	66.691226
1369.404497	61.860834	66.696231
1368.176327	60.742429	66.701236
1367.937001	55.890214	66.706241
1367.377268	67.407691	66.711246
1367.080196	53.492192	66.716250
1366.725354	61.072455	66.721255
1365.856647	66.044046	66.726260
1365.046478	62.692404	66.731265
1364.281900	75.614437	66.736270
1364.014385	61.776237	66.741274
1362.543553	68.958294	66.746279
1361.800064	66.144849	66.751284
1361.550858	61.950234	66.756289
1360.862863	59.157931	66.761294
1360.712181	64.535796	66.766298
1359.869835	64.507272	66.771303
1358.836323	60.107738	66.776308
1358.936438	53.022159	66.781313
1357.534885	60.590606	66.786318
1356.503518	55.459007	66.791322
1356.072979	65.645464	66.796327
1355.706008	64.237200	66.801332
1355.127168	54.321602	66.806337
1354.520737	61.296867	66.811342
1353.819563	56.723079	66.816346
1353.019593	57.954149	66.821351
1352.860464	58.078804	66.826356
1352.085147	56.226082	66.831361
1351.177332	54.560008	66.836366
1350.758780	51.592411	66.841370
1349.198079	61.848129	66.846375
1347.878530	56.185164	66.851380
1348.281815	55.032938	66.856385
1347.461599	58.957583	66.861390
1346.783741	63.334276	66.866394
1346.621809	52.144430	66.871399
1346.143708	59.695400	66.876404
1345.899096	60.417133	66.881409
1344.417778	62.592324	66.886414
1343.986041	52.225982	66.891418
1343.233924	53.288594	66.896423
1342.070207	65.723699	66.901428
1341.908667	50.835736	66.906433
1341.039512	66.057878	66.911438
1340.786323	57.364729	66.916442
1339.837639	52.954875	66.921447
1338.834507	55.065092	66.926452
1338.660610	53.922614	66.931457
1337.898160	63.209328	66.936462
1337.575365	51.616113	66.941466
1336.289657	60.861424	66.946471
1335.455181	63.452625	66.951476
1335.626361	56.417251	66.956481
1334.498137	63.751443	66.961486
1334.022866	56.486088	66.966490
1333.154042	56.953805	66.971495
1332.406349	60.119430	66.976500
1332.096792	52.777270	66.981505
1331.401589	56.141137	66.986510
1330.276760	51.529048	66.991514
1329.704768	53.816740	66.996519
1329.091194	56.831731	67.001524
1328.994011	52.199784	67.006529
1327.867882	49.587533	67.011534
1327.320511	50.084577	67.016538
1327.011128	48.101022	67.021543
1326.183926	56.566952	67.026548
1325.062157	52.364397	67.031553
1324.513346	62.533385	67.036558
1324.036938	56.419421	67.041562
1323.657588	63.927888	67.046567
1322.630140	60.080932	67.051572
1321.641630	63.262765	67.056577
1320.975551	70.528228	67.061582
1320.849462	61.127305	67.066586
1320.424510	58.651175	67.071591
1319.234924	53.268773	67.076596
1318.603653	60.746323	67.081601
1317.661511	65.332198	67.086606
1317.561678	62.236665	67.091610
1316.909352	59.279428	67.096615
1315.358407	55.936758	67.101620
1315.129420	57.974377	67.106625
1314.842513	59.339942	67.111630
1314.084489	55.885410	67.116634
1313.804866	50.577552	67.121639
1312.698923	48.075643	67.126644
1312.319201	57.438712	67.131649
1311.409389	56.069444	67.136654
1311.113129	56.673231	67.141658
1309.629889	61.062848	67.146663
1309.147202	62.049521	67.151668
1308.670726	49.890950	67.156673
1308.174551	61.977081	67.161678
1307.743480	60.110647	67.166682
1306.580276	48.543815	67.171687
1306.091548	58.698519	67.176692
1305.921974	52.311847	67.181697
1305.011325	62.860069	67.186702
1304.029259	62.689768	67.191706
1303.437537	51.442100	67.196711
1302.764203	52.394425	67.201716
1302.693101	62.446466	67.206721
1301.293091	67.267570	67.211726
1300.725901	56.228894	67.216730
1300.321023	59.543458	67.221735
1299.891347	59.958716	67.226740
1299.059491	57.034758	67.231745
1298.061088	64.245820	67.236750
1297.450507	61.062749	67.241754
1297.009402	58.884091	67.246759
1295.926490	64.648291	67.251764
1295.192937	51.043488	67.256769
1294.336509	54.880861	67.261774
1294.142294	54.096441	67.266778
1293.921110	59.305735	67.271783
1293.381931	66.890079	67.276788
1292.659802	50.940045	67.281793
1291.295181	60.817678	67.286798
1290.746025	56.137739	67.291802
1290.444184	60.281192	67.296807
1289.500220	58.570423	67.301812
1289.181315	48.102580	67.306817
1288.350249	60.264032	67.311822
1288.054253	49.956553	67.316826
1286.875216	48.926573	67.321831
1286.235073	56.987448	67.326836
1286.034645	55.670991	67.331841
1285.015352	60.428418	67.336846
1284.151599	53.666401	67.341850
1283.276883	61.032847	67.346855
1282.506228	62.029036	67.351860
1282.496477	58.832449	67.356865
1282.323338	65.361937	67.361870
1281.452691	57.240068	67.366874
1280.658712	59.350170	67.371879
1279.665071	60.785524	67.376884
1278.996085	54.695882	67.381889
1277.750250	59.114004	67.386894
1277.314364	67.796864	67.391898
1277.125429	64.027929	67.396903
1276.439940	56.190446	67.401908
1276.057971	59.763152	67.406913
1275.444902	64.230487	67.411918
1274.444975	65.906546	67.416922
1273.966350	55.315857	67.421927
1272.956754	62.320542	67.426932
1272.043603	43.981785	67.431937
1271.263718	64.035844	67.436942
1270.724698	62.170810	67.441946
1270.604330	62.847564	67.446951
1270.218709	66.373543	67.451956
1269.876401	59.060255	67.456961
1268.745981	63.658733	67.461966
1267.961690	63.647818	67.466970
1267.250736	65.202239	67.471975
1265.991072	67.072566	67.476980
1265.511494	56.724888	67.481985
1265.195942	63.048353	67.486990
1264.846514	55.956979	67.491994
1264.223303	60.922681	67.496999
1262.874239	65.694702	67.502004
1262.736192	55.194950	67.507009
1261.934413	61.187282	67.512014
1261.468849	54.527547	67.517018
1260.208151	59.287094	67.522023
1259.377807	63.762170	67.527028
1259.281345	58.112950	67.532033
1258.763994	63.323604	67.537038
1258.205560	56.708598	67.542042
1257.254383	56.292124	67.547047
1256.336650	57.499368	67.552052
1256.022632	63.396802	67.557057
1255.631722	58.811562	67.562062
1254.273447	57.120949	67.567066
1253.692520	64.071675	67.572071
1253.127518	71.795754	67.577076
1253.077827	68.116648	67.582081
1252.272549	64.554527	67.587086
1251.390951	65.836455	67.592090
1250.685108	63.509082	67.597095
1249.923920	63.500807	67.602100
1249.821827	51.454620	67.607105
1248.306562	66.120326	67.612110
1247.579354	62.575757	67.617114
1247.289946	62.957682	67.622119
1246.783305	65.701793	67.627124
1246.510870	56.552818	67.632129
1245.204314	58.793318	67.637134
1244.486549	60.260515	67.642138
1244.033223	54.439377	67.647143
1243.621905	57.174638	67.652148
1242.999405	64.316484	67.657153
1241.884433	69.484968	67.662158
1241.706941	59.653827	67.667162
1241.087352	59.285563	67.672167
1239.637495	63.993194	67.677172
1239.334261	57.340769	67.682177
1238.620236	61.276946	67.687182
1238.399349	56.828682	67.692186
1237.509699	49.280730	67.697191
1236.469670	54.240170	67.702196
1236.048275	41.156639	67.707201
1235.450438	50.190103	67.712206
1235.050140	49.958864	67.717210
1234.300346	43.394800	67.722215
1233.079279	55.689236	67.727220
1232.834995	46.250358	67.732225
1232.344673	59.199753	67.737230
1231.955523	53.915631	67.742234
1231.032044	47.273525	67.747239
1230.042718	55.143919	67.752244
1229.764574	53.450308	67.757249
1228.630838	47.999149	67.762254
1227.780340	49.060090	67.767258
1227.354318	45.516527	67.772263
1226.798990	58.033123	67.777268
1226.816366	51.083712	67.782273
1225.705353	56.669471	67.787278
1224.862401	56.902869	67.792282
1224.406512	51.951068	67.797287
1223.716129	47.561695	67.802292
1222.965804	52.473496	67.807297
1221.823290	51.068723	67.812302
1221.621975	46.879133	67.817306
1221.437134	50.089329	67.822311
1220.121153	58.248219	67.827316
1219.441973	61.808266	67.832321
1219.023459	59.996624	67.837326
1218.404455	57.024656	67.842330
1218.048986	56.775252	67.847335
1216.666037	57.543963	67.852340
1216.280583	57.926972	67.857345
1215.874698	65.619443	67.862350
1214.796617	53.797844	67.867354
1214.157865	51.527626	67.872359
1213.294596	55.891250	67.877364
1213.089998	54.203293	67.882369
1212.661970	49.411072	67.887374
1211.910573	51.057094	67.892378
1210.851329	55.544925	67.897383
1209.889472	50.634160	67.902388
1209.668825	42.779562	67.907393
1209.351094	48.234448	67.912398
1208.482910	55.109427	67.917402
1207.490551	56.613991	67.922407
1206.584435	60.620146	67.927412
1206.649133	49.793270	67.932417
1206.009489	59.508344	67.937422
1205.335547	54.613299	67.942426
1204.654455	48.112437	67.947431
1203.865961	57.494780	67.952436
1203.327391	52.224963	67.957441
1201.998333	56.806167	67.962446
1201.477093	58.891845	67.967450
1201.240571	48.977062	67.972455
1200.881728	59.503791	67.977460
1199.810918	54.261840	67.982465
1198.961403	57.207141	67.987470
1198.785268	54.115867	67.992474
1197.908323	51.341046	67.997479
1196.888572	61.482431	68.002484
1196.258282	49.624330	68.007489
1196.007571	51.889345	68.012494
1195.582814	52.174524	68.017498
1195.094386	53.734577	68.022503
1193.499655	56.533452	68.027508
1193.129749	53.364179	68.032513
1192.733875	54.699775	68.037518
1191.777974	57.128973	68.042522
1190.800810	49.475106	68.047527
1190.430712	60.918282	68.052532
1189.753502	51.131929	68.057537
1189.117676	53.311526	68.062542
1188.975836	47.428254	68.067546
1188.320634	46.616224	68.072551
1187.294289	53.164691	68.077556
1186.890376	50.527544	68.082561
1185.406348	53.720413	68.087566
1184.890992	56.937439	68.092570
1184.318634	47.599629	68.097575
1183.728223	55.042314	68.102580
1183.377302	52.388856	68.107585
1183.036007	49.461047	68.112590
1182.061337	45.586840	68.117594
1181.690578	48.733561	68.122599
1180.546002	55.934783	68.127604
1180.327202	48.464680	68.132609
1179.451144	50.740831	68.137614
1178.623102	50.576048	68.142618
1178.149720	47.470545	68.147623
1177.217846	54.082841	68.152628
1176.497544	42.494542	68.157633
1175.486464	53.416736	68.162638
1175.148561	55.955822	68.167642
1174.889376	49.340564	68.172647
1174.406415	52.680175	68.177652
1173.651243	48.532939	68.182657
1172.585948	53.911168	68.187662
1172.148324	58.246539	68.192666
1171.941948	51.878354	68.197671
1170.502730	62.688867	68.202676
1170.085789	45.649545	68.207681
1169.332722	48.923300	68.212686
1168.864429	46.864113	68.217690
1168.128901	42.858839	68.222695
1166.978717	54.369298	68.227700
1166.560044	51.166785	68.232705
1166.031161	52.588193	68.237710
1165.781813	47.890573	68.242714
1165.320891	53.965916	68.247719
1164.118290	59.083705	68.252724
1163.866879	48.808590	68.257729
1162.552399	55.499085	68.262734
1161.434101	55.467203	68.267738
1161.252492	53.277266	68.272743
1160.467422	62.189133	68.277748
1160.502656	48.700252	68.282753
1160.064629	56.189671	68.287758
1159.157655	57.601824	68.292762
1158.278680	50.810741	68.297767
1157.762067	56.082792	68.302772
1156.630391	50.874197	68.307777
1155.499905	55.072172	68.312782
1154.919514	52.489907	68.317786
1154.730735	49.356493	68.322791
1154.070844	52.158106	68.327796
1154.004232	46.802206	68.332801
1153.224525	55.113960	68.337806
1151.862750	52.129250	68.342810
1152.157245	47.644768	68.347815
1151.305087	45.074187	68.352820
1150.832993	47.620423	68.357825
1149.750260	57.909033	68.362830
1149.233453	54.190684	68.367834
1148.023347	48.494661	68.372839
1147.007195	61.809972	68.377844
1146.388021	52.110602	68.382849
1146.400385	59.585164	68.387854
1145.907162	52.496186	68.392858
1145.581260	45.666036	68.397863
1144.257100	64.171328	68.402868
1143.683255	48.008544	68.407873
1143.156005	56.414194	68.412878
1142.363802	54.516916	68.417882
1141.495479	55.382019	68.422887
1140.655744	55.233301	68.427892
1140.584901	53.188179	68.432897
1140.152984	53.379888	68.437902
1139.156403	57.029857	68.442906
1138.257684	53.600916	68.447911
1137.641436	63.160890	68.452916
1137.203837	52.071699	68.457921
1135.889499	52.703381	68.462926
1135.277561	53.884110	68.467930
1134.733716	54.517831	68.472935
1134.629420	60.870783	68.477940
1134.325066	61.237751	68.482945
1133.348914	66.336886	68.487950
1132.365628	63.599501	68.492954
1131.836164	55.521207	68.497959
1131.064455	56.874008	68.502964
1130.553947	52.422937	68.507969
1129.573727	57.506948	68.512974
1128.938145	49.775127	68.517978
1128.834888	58.291544	68.522983
1127.647536	58.188656	68.527988
1127.196840	45.846271	68.532993
1126.429353	55.144860	68.537998
1125.692501	64.675133	68.543002
1125.655438	46.908337	68.548007
1124.509499	58.727229	68.553012
1123.841450	51.092038	68.558017
1123.335053	59.108013	68.563022
1122.776918	52.234374	68.568026
1121.706161	52.164985	68.573031
1120.874975	56.033089	68.578036
1120.697608	53.091833	68.583041
1120.051264	53.642509	68.588046
1118.868980	54.056073	68.593050
1118.614017	46.178561	68.598055
1117.416991	54.645010	68.603060
1117.625994	55.832368	68.608065
1116.933230	54.600543	68.613070
1116.099532	54.854583	68.618074
1115.493298	46.900475	68.623079
1114.433367	53.520541	68.628084
1113.967577	49.811434	68.633089
1112.973726	37.788845	68.638094
1112.632204	44.792970	68.643098
1112.195367	51.324969	68.648103
1111.407058	49.387658	68.653108
1110.454525	43.814696	68.658113
1109.619077	48.020954	68.663118
1108.829076	46.804599	68.668122
1108.835303	47.402874	68.673127
1107.817736	48.362690	68.678132
1107.875500	44.871516	68.683137
1106.940153	51.848669	68.688142
1106.028762	48.032239	68.693146
1105.656127	44.995886	68.698151
1104.487628	58.283396	68.703156
1103.935351	56.327468	68.708161
1103.613147	53.369826	68.713166
1103.112164	47.696658	68.718170
1102.138055	54.380350	68.723175
1101.318426	54.591155	68.728180
1100.535947	47.023062	68.733185
1100.231746	47.889915	68.738190
1099.256831	49.606215	68.743194
1098.481410	46.905172	68.748199
1097.991220	47.290664	68.753204
1097.687581	44.826824	68.758209
1097.071522	54.367844	68.763214
1096.066460	49.566506	68.768218
1095.502180	41.597849	68.773223
1094.332311	52.736138	68.778228
1094.402896	52.816385	68.783233
1093.345125	55.159316	68.788238
1092.465999	56.062425	68.793242
1091.996263	48.493476	68.798247
1091.479650	57.238071	68.803252
1091.384675	52.001806	68.808257
1090.222941	52.109331	68.813262
1089.194310	50.140867	68.818266
1088.727559	48.013640	68.823271
1088.021917	57.184127	68.828276
1087.821481	51.953599	68.833281
1086.878026	54.008683	68.838286
1086.118436	55.402148	68.843290
1085.777659	48.317325	68.848295
1084.882408	51.962234	68.853300
1083.881500	45.972767	68.858305
1083.531898	44.186462	68.863310
1082.916680	48.815024	68.868314
1082.572589	44.277571	68.873319
1081.725115	53.278225	68.878324
1081.049535	47.415210	68.883329
1080.202215	47.493228	68.888334
1079.445917	55.143669	68.893338
1078.783569	46.657592	68.898343
1077.873029	57.371430	68.903348
1077.436808	46.345122	68.908353
1076.840191	52.672300	68.913358
1076.445192	60.012955	68.918362
1076.341207	58.496669	68.923367
1074.964408	55.779327	68.928372
1074.395550	56.118988	68.933377
1073.728310	51.350656	68.938382
1072.734734	45.563460	68.943386
1072.034763	43.774541	68.948391
1071.383801	54.145883	68.953396
1071.076911	52.344899	68.958401
1070.870830	47.623063	68.963406
1069.918085	54.599841	68.968410
1069.220492	49.229198	68.973415
1068.720238	59.422025	68.978420
1067.279154	54.754713	68.983425
1066.471508	52.036729	68.988430
1065.491154	57.997589	68.993434
1065.251397	54.582126	68.998439
1064.734870	52.153732	69.003444
1064.783911	50.043811	69.008449
1064.340064	49.390586	69.013454
1063.623318	46.973542	69.018458
1063.012553	38.148101	69.023463
1062.010273	50.015118	69.028468
1061.032315	46.176180	69.033473
1060.204461	45.536732	69.038478
1059.571849	46.835886	69.043482
1059.686880	41.709727	69.048487
1058.348220	55.423295	69.053492
1057.480454	43.174088	69.058497
1057.035229	52.102874	69.063502
1056.706171	54.099657	69.068506
1056.490806	47.937931	69.073511
1054.848708	53.392189	69.078516
1054.343465	56.303269	69.083521
1054.002769	42.375882	69.088526
1052.985428	54.160142	69.093530
1052.404274	43.429718	69.098535
1051.526258	54.848033	69.103540
1051.416506	44.072582	69.108545
1051.060213	51.302995	69.113550
1049.720732	55.818118	69.118554
1049.164400	47.278915	69.123559
1048.266097	57.143970	69.128564
1048.053424	50.030891	69.133569
1047.332312	41.301857	69.138574
1046.212255	47.806927	69.143578
1045.665914	50.256179	69.148583
1044.881793	54.348634	69.153588
1044.743222	43.117288	69.158593
1044.427214	51.489342	69.163598
1043.440892	48.698862	69.168602
1042.403630	43.544696	69.173607
1042.211802	51.477516	69.178612
1041.104774	34.573265	69.183617
1040.552363	44.384865	69.188622
1039.558936	47.428802	69.193626
1039.651870	42.197346	69.198631
1038.860212	50.922618	69.203636
1037.967755	42.704981	69.208641
1037.174123	50.706730	69.213646
1036.386503	57.685636	69.218650
1036.619099	44.696825	69.223655
1035.462859	50.217306	69.228660
1034.654828	42.766850	69.233665
1034.213775	46.104545	69.238670
1033.284918	63.873611	69.243674
1032.392374	49.007394	69.248679
1031.606557	52.672757	69.253684
1031.208727	45.226432	69.258689
1031.000773	45.920282	69.263694
1030.364031	59.269880	69.268698
1029.467732	48.255274	69.273703
1028.409211	50.609388	69.278708
1028.057517	47.229087	69.283713
1028.007338	50.007849	69.288718
1027.022237	46.785088	69.293722
1026.242717	47.170890	69.298727
1025.412879	52.333513	69.303732
1024.871785	52.548917	69.308737
1023.575623	52.707822	69.313742
1022.847220	53.353581	69.318746
1022.804160	50.320004	69.323751
1022.023328	47.757046	69.328756
1021.681461	59.963727	69.333761
1021.421456	53.162539	69.338766
1020.023035	56.054868	69.343770
1019.707450	47.712345	69.348775
1018.633789	55.094738	69.353780
1017.723300	50.781448	69.358785
1017.124458	51.539063	69.363790
1016.410579	58.192422	69.368794
1016.309167	50.982797	69.373799
1015.910168	54.695438	69.378804
1015.340519	51.625787	69.383809
1014.730809	45.250832	69.388814
1013.515155	47.852306	69.393818
1013.132608	49.021799	69.398823
1011.990779	52.261248	69.403828
1011.510682	55.832247	69.408833
1011.120806	50.713872	69.413838
1010.495646	55.970097	69.418842
1009.860661	48.775975	69.423847
1008.839941	46.274841	69.428852
1007.947790	47.828193	69.433857
1008.022935	49.011604	69.438862
1006.803248	52.840621	69.443866
1006.180409	47.153748	69.448871
1005.474320	51.408843	69.453876
1005.236888	43.385060	69.458881
1004.159877	49.175229	69.463886
1003.086761	50.318970	69.468890
1002.905579	47.171749	69.473895
1002.282508	54.288489	69.478900
1001.978945	50.160926	69.483905
1001.248249	50.100565	69.488910
1000.350396	52.910110	69.493914
999.962092	49.185546	69.498919
998.760722	57.677965	69.503924
997.650542	54.771588	69.508929
997.336751	52.486000	69.513934
996.666500	55.322414	69.518938
996.625227	47.109722	69.523943
996.030191	57.148896	69.528948
995.367074	47.320952	69.533953
994.441864	52.492449	69.538958
993.858657	56.428370	69.543962
993.426489	48.361450	69.548967
992.261712	49.956605	69.553972
991.793711	52.076429	69.558977
991.010834	55.358128	69.563982
990.523687	53.565334	69.568986
990.124245	49.361563	69.573991
988.620437	60.184008	69.578996
988.313653	54.147224	69.584001
987.978454	46.432317	69.589006
987.335449	53.408725	69.594010
986.615854	46.584473	69.599015
985.285923	48.742084	69.604020
985.246912	56.366734	69.609025
984.827152	55.012661	69.614030
983.723806	58.074109	69.619034
983.190754	50.696616	69.624039
982.400309	53.093254	69.629044
981.798817	53.122730	69.634049
981.513260	56.572893	69.639054
979.906042	64.552717	69.644058
979.875661	52.890990	69.649063
979.013082	57.752901	69.654068
978.719610	49.596106	69.659073
978.527266	45.392504	69.664078
977.062486	53.803834	69.669082
976.485876	51.580567	69.674087
975.802511	59.526941	69.679092
975.230093	53.444113	69.684097
974.894809	55.845606	69.689102
973.884168	57.717450	69.694106
973.296993	49.157946	69.699111
972.578185	54.296610	69.704116
971.470426	54.250519	69.709121
971.048937	43.775423	69.714126
970.445053	61.171084	69.719130
970.342503	45.177818	69.724135
969.542977	52.745272	69.729140
968.838452	42.485526	69.734145
968.243746	50.337364	69.739150
967.382048	58.942910	69.744154
966.474003	48.945784	69.749159
965.894062	49.351890	69.754164
965.176690	48.024674	69.759169
964.747839	49.354509	69.764174
964.361091	57.089682	69.769178
963.572645	57.238798	69.774183
962.609126	57.411040	69.779188
962.145836	55.026238	69.784193
960.764313	49.360745	69.789198
960.219796	52.656566	69.794202
959.870696	46.227546	69.799207
959.293797	48.276390	69.804212
959.023415	54.270976	69.809217
958.531985	40.500069	69.814222
957.411962	47.399413	69.819226
957.062258	42.519093	69.824231
956.353756	56.394213	69.829236
955.210514	51.294795	69.834241
954.810925	41.875957	69.839246
954.151074	48.517573	69.844250
953.579048	43.218457	69.849255
952.461943	47.622544	69.854260
951.348234	49.376752	69.859265
950.948870	48.331684	69.864270
950.610603	55.340036	69.869274
950.629277	58.806450	69.874279
949.882555	69.770234	69.879284
949.103133	53.884667	69.884289
948.292544	48.584085	69.889294
947.648688	62.092525	69.894298
946.926318	52.330796	69.899303
945.726933	49.804500	69.904308
945.254858	49.015436	69.909313
945.045748	56.000084	69.914318
944.282200	64.552173	69.919322
943.932558	46.584414	69.924327
942.953559	49.298076	69.929332
942.410442	48.712710	69.934337
941.896125	51.076460	69.939342
940.444517	53.772284	69.944346
940.003603	41.198165	69.949351
939.347489	56.567819	69.954356
938.940634	54.502056	69.959361
938.251617	51.413571	69.964366
937.483408	52.797411	69.969370
936.956024	48.902598	69.974375
936.158337	55.212909	69.979380
935.768360	56.779419	69.984385
935.485929	48.179320	69.989390
934.097671	53.739917	69.994394
933.762472	43.738390	69.999399
933.173395	51.359098	70.004404
931.942447	52.740877	70.009409
931.128015	51.550544	70.014414
930.359488	59.065768	70.019418
930.490002	48.955437	70.024423
929.717380	52.123555	70.029428
929.186547	55.981766	70.034433
928.676550	46.905360	70.039438
927.561064	51.638791	70.044442
927.328368	48.443003	70.049447
926.388458	60.419989	70.054452
925.729920	53.474074	70.059457
925.094062	51.293365	70.064462
924.642731	52.715095	70.069466
923.901680	39.146354	70.074471
922.632898	45.810755	70.079476
921.993257	51.867255	70.084481
921.678718	49.731611	70.089486
920.903215	54.232744	70.094490
920.959340	43.178601	70.099495
920.035672	56.070808	70.104500
919.542123	60.005092	70.109505
918.831318	42.877004	70.114510
917.941913	55.419975	70.119514
916.955867	51.077748	70.124519
916.570229	52.359713	70.129524
915.398418	46.951043	70.134529
915.079997	48.234927	70.139534
913.991225	54.261973	70.144538
913.814291	55.411376	70.149543
913.172664	55.223324	70.154548
912.535381	49.701207	70.159553
911.955158	50.250875	70.164558
911.231377	59.053689	70.169562
910.941743	47.161990	70.174567
909.700683	55.468365	70.179572
908.743127	57.722880	70.184577
908.441307	54.369355	70.189582
907.669077	61.472003	70.194586
907.485085	54.078408	70.199591
907.090421	56.658095	70.204596
905.786563	55.225526	70.209601
905.528984	55.014207	70.214606
904.502130	55.510371	70.219610
903.545973	61.287656	70.224615
902.613712	58.810337	70.229620
902.141240	48.288176	70.234625
902.215508	46.989545	70.239630
901.328602	60.249655	70.244634
901.268575	56.904962	70.249639
900.044783	63.391907	70.254644
899.560528	57.697201	70.259649
898.619142	47.353746	70.264654
897.625536	63.365335	70.269658
897.025754	50.802310	70.274663
896.467416	56.785953	70.279668
895.832681	56.210445	70.284673
895.744892	60.163741	70.289678
894.615481	57.831343	70.294682
894.017880	50.055709	70.299687
893.358100	55.779522	70.304692
893.006696	61.790161	70.309697
891.855474	56.529614	70.314702
891.351994	65.726317	70.319706
890.899528	52.267774	70.324711
890.556728	53.943480	70.329716
889.104375	58.574416	70.334721
888.330425	52.924241	70.339726
887.704828	56.564147	70.344730
887.869883	46.213352	70.349735
886.797158	57.427721	70.354740
885.665717	64.489768	70.359745
885.526536	48.847707	70.364750
884.824143	57.733856	70.369754
884.292816	57.630761	70.374759
883.266383	52.137467	70.379764
882.209494	56.172448	70.384769
882.243206	48.015644	70.389774
881.762444	50.779350	70.394778
881.107027	52.463807	70.399783
879.849014	51.468667	70.404788
879.066372	60.307664	70.409793
879.198619	57.437009	70.414798
878.342829	57.294087	70.419802
877.629316	52.042739	70.424807
876.749367	50.030202	70.429812
876.081469	55.761618	70.434817
875.804098	47.132342	70.439822
874.679122	61.294535	70.444826
874.176094	55.000415	70.449831
873.533174	65.739528	70.454836
873.102276	58.801556	70.459841
871.914498	55.789313	70.464846
871.267488	67.774899	70.469850
871.036344	59.265995	70.474855
870.482755	58.832124	70.479860
869.720101	58.570302	70.484865
868.749026	52.547798	70.489870
868.230238	57.749273	70.494874
867.689689	49.989800	70.499879
867.281042	59.026326	70.504884
866.034875	55.789985	70.509889
865.476537	54.511607	70.514894
864.460733	57.953417	70.519898
864.892170	56.132728	70.524903
864.162357	60.164549	70.529908
862.840723	62.063854	70.534913
862.518401	60.129733	70.539918
861.151586	62.228622	70.544922
860.621255	57.028549	70.549927
859.889964	62.091956	70.554932
859.380324	57.207143	70.559937
859.109790	52.547633	70.564942
858.514986	65.594106	70.569946
858.092047	60.323323	70.574951
856.827563	60.757976	70.579956
856.228482	53.608652	70.584961
856.068324	46.208121	70.589966
855.212311	52.206028	70.594970
854.274194	55.367389	70.599975
853.740868	60.333056	70.604980
852.884089	57.580386	70.609985
852.616877	60.940906	70.614990
851.383850	60.339204	70.619994
851.427055	58.892547	70.624999
850.828157	56.467849	70.630004
849.368622	53.984583	70.635009
848.676280	56.605348	70.640014
848.194442	57.450038	70.645018
847.789069	47.958026	70.650023
847.535832	48.157616	70.655028
846.400481	57.279841	70.660033
846.293356	50.231999	70.665038
845.013157	58.502051	70.670042
844.183876	47.683453	70.675047
843.585169	50.601558	70.680052
842.848934	62.670732	70.685057
842.490993	53.950200	70.690062
841.747442	60.354424	70.695066
841.503055	57.092695	70.700071
840.524382	56.674448	70.705076
839.537454	58.843774	70.710081
839.436977	48.558898	70.715086
838.827794	56.208054	70.720090
838.019997	50.132769	70.725095
837.087143	53.562963	70.730100
836.502665	56.068789	70.735105
836.008965	58.815639	70.740110
835.102088	60.764063	70.745114
834.591445	46.365457	70.750119
833.761443	55.353928	70.755124
833.145561	60.779026	70.760129
833.195195	54.548344	70.765134
831.965163	55.874830	70.770138
831.086620	60.237844	70.775143
830.588905	52.339096	70.780148
830.094622	58.482868	70.785153
829.414368	58.447645	70.790158
828.594291	60.511569	70.795162
828.078238	50.002674	70.800167
827.220325	54.173165	70.805172
826.254852	64.315481	70.810177
826.054147	59.449313	70.815182
825.492074	65.313714	70.820186
825.018577	63.572399	70.825191
823.847105	55.714658	70.830196
822.959426	59.722729	70.835201
822.729203	58.631836	70.840206
821.964155	59.912703	70.845210
821.415424	48.068574	70.850215
820.474539	48.320847	70.855220
819.820070	57.071643	70.860225
819.674548	54.864956	70.865230
818.991432	58.622843	70.870234
818.123223	58.000938	70.875239
817.600808	55.329104	70.880244
816.764431	59.855725	70.885249
816.276741	59.185869	70.890254
815.144395	63.519899	70.895258
814.396638	55.418097	70.900263
814.327950	54.085447	70.905268
813.340996	58.437336	70.910273
812.663419	54.470264	70.915278
811.674248	64.679436	70.920282
811.296419	50.847910	70.925287
811.050771	52.060297	70.930292
810.480955	51.752028	70.935297
809.676203	52.482541	70.940302
808.554535	58.711987	70.945306
808.327476	57.827178	70.950311
807.791952	59.561957	70.955316
806.447727	59.271297	70.960321
806.091673	49.075994	70.965326
805.373049	63.921020	70.970330
805.052990	55.658101	70.975335
803.789563	54.599205	70.980340
803.170098	63.792300	70.985345
802.990074	48.738668	70.990350
802.431824	57.636580	70.995354
801.700272	52.388129	71.000359
800.779023	60.938540	71.005364
799.853381	60.644334	71.010369
799.817632	52.225773	71.015374
799.039574	62.861823	71.020378
798.415097	54.861832	71.025383
797.676023	53.596469	71.030388
796.858118	63.819384	71.035393
796.288874	50.324269	71.040398
794.787279	52.873585	71.045402
794.498662	54.089659	71.050407
793.815038	56.942443	71.055412
793.139107	58.690113	71.060417
793.114932	55.074787	71.065422
792.485800	65.956798	71.070426
792.442565	60.819558	71.075431
791.641789	63.129585	71.080436
790.559304	62.325751	71.085441
789.561224	51.527736	71.090446
788.339270	72.219931	71.095450
788.005175	64.810818	71.100455
787.728890	59.769024	71.105460
787.285215	57.707573	71.110465
786.400912	50.129003	71.115470
785.317341	55.376238	71.120474
785.356678	46.731259	71.125479
784.705027	57.662583	71.130484
783.534222	56.134782	71.135489
782.975288	55.640280	71.140494
782.455229	50.840727	71.145498
782.211156	53.465844	71.150503
781.071779	51.500948	71.155508
780.150339	53.722950	71.160513
779.796591	55.028243	71.165518
779.246217	54.614382	71.170522
778.459962	52.407190	71.175527
777.461937	59.028559	71.180532
777.031092	61.770145	71.185537
776.792156	54.144037	71.190542
775.623138	61.797168	71.195546
774.869242	56.498663	71.200551
774.400728	58.634375	71.205556
773.912222	62.528455	71.210561
773.386288	54.895993	71.215566
772.246932	61.073075	71.220570
771.813543	56.527814	71.225575
771.340369	52.712724	71.230580
770.585052	54.564501	71.235585
769.663257	48.745515	71.240590
768.415709	48.928352	71.245594
768.248983	54.739283	71.250599
767.865490	58.356443	71.255604
767.589689	57.607133	71.260609
767.055573	51.862053	71.265614
766.020496	65.122128	71.270618
765.633848	52.436911	71.275623
764.405879	52.783793	71.280628
763.335407	54.570623	71.285633
763.201473	50.405057	71.290638
762.229579	51.095959	71.295642
762.142586	45.282858	71.300647
761.577039	43.772259	71.305652
760.320190	56.916242	71.310657
759.819393	50.975045	71.315662
759.588687	56.356184	71.320666
758.779377	52.033201	71.325671
757.745357	50.138278	71.330676
756.853934	59.836728	71.335681
756.610116	48.497603	71.340686
756.129145	59.056400	71.345690
755.285046	47.929535	71.350695
754.463377	51.826190	71.355700
753.644806	52.896395	71.360705
753.631255	46.220031	71.365710
752.962394	58.021441	71.370714
752.076374	50.275998	71.375719
751.445079	52.308314	71.380724
750.225247	64.085476	71.385729
750.197073	54.137613	71.390734
749.079792	65.609863	71.395738
748.413993	63.500200	71.400743
747.880054	63.181503	71.405748
747.249498	61.643407	71.410753
747.414815	52.514738	71.415758
746.083111	62.046737	71.420762
745.577932	60.342022	71.425767
745.057589	54.325090	71.430772
743.975984	58.321479	71.435777
743.223755	47.656243	71.440782
742.313398	55.793340	71.445786
742.089331	50.539814	71.450791
741.828864	45.240043	71.455796
740.496800	57.259003	71.460801
739.962324	57.181671	71.465806
739.213856	57.597311	71.470810
739.404630	42.752756	71.475815
738.650646	50.910689	71.480820
737.459802	51.805195	71.485825
737.019831	46.235953	71.490830
736.057306	52.853257	71.495834
734.878156	62.731566	71.500839
734.454127	53.485406	71.505844
734.073396	60.500534	71.510849
734.035903	57.235844	71.515854
732.967612	58.552398	71.520858
732.180058	58.710905	71.525863
731.840220	58.970026	71.530868
731.069352	67.345128	71.535873
730.011793	58.016898	71.540878
729.038124	64.229122	71.545882
728.791478	58.490324	71.550887
728.510449	56.477108	71.555892
727.773233	56.681221	71.560897
726.417985	59.382323	71.565902
725.861748	56.389460	71.570906
725.709263	53.102078	71.575911
725.041787	58.044966	71.580916
724.506126	58.612814	71.585921
723.799690	53.141190	71.590926
722.835606	57.918408	71.595930
722.289712	56.639659	71.600935
721.957211	63.181900	71.605940
720.571300	61.577986	71.610945
720.057962	54.392976	71.615950
719.594598	60.787313	71.620954
719.442471	57.588184	71.625959
718.395094	55.911451	71.630964
717.315524	60.238694	71.635969
717.097871	52.770062	71.640974
716.288101	55.102043	71.645978
715.566884	56.587277	71.650983
714.717522	53.811401	71.655988
714.094671	60.048200	71.660993
714.086004	49.081661	71.665998
713.215049	57.953676	71.671002
712.138654	51.329834	71.676007
711.520488	57.307261	71.681012
710.940951	59.326616	71.686017
710.740103	49.972390	71.691022
709.877422	58.122408	71.696026
708.836658	55.835909	71.701031
708.474313	58.661217	71.706036
708.264381	60.596494	71.711041
707.319464	50.136995	71.716046
706.019747	57.669031	71.721050
705.803497	49.962054	71.726055
705.502679	48.240582	71.731060
703.941541	63.749628	71.736065
703.633010	48.919911	71.741070
703.022334	53.525747	71.746074
702.627882	46.738141	71.751079
702.477831	52.822389	71.756084
701.184222	56.127137	71.761089
700.560851	50.224395	71.766094
699.636379	64.668539	71.771098
699.047904	55.503765	71.776103
698.309989	51.424909	71.781108
697.447921	56.282088	71.786113
697.113111	55.250440	71.791118
696.607287	54.173479	71.796122
696.196363	51.291532	71.801127
695.467371	56.036059	71.806132
694.212191	59.492390	71.811137
694.338060	52.382236	71.816142
692.940350	57.296317	71.821146
692.208210	60.014922	71.826151
691.983865	52.828063	71.831156
691.347413	58.127148	71.836161
690.754896	56.381158	71.841166
689.469486	59.828112	71.846170
688.767819	54.843028	71.851175
688.446129	49.464702	71.856180
688.168520	58.513491	71.861185
687.917647	48.131157	71.866190
686.529146	57.788919	71.871194
685.926044	60.952190	71.876199
685.663539	61.381934	71.881204
684.187707	58.325764	71.886209
683.460881	57.402268	71.891214
682.847218	54.890078	71.896218
682.160749	51.725572	71.901223
681.873670	49.104611	71.906228
681.674155	58.875841	71.911233
681.349730	49.607531	71.916238
680.360160	51.911379	71.921242
679.605723	48.839699	71.926247
678.523707	47.411355	71.931252
677.445256	53.611890	71.936257
677.057718	41.418869	71.941262
676.503824	53.774424	71.946266
675.930082	54.053450	71.951271
675.975814	49.936557	71.956276
674.517496	58.313892	71.961281
674.093730	48.952590	71.966286
673.239576	59.403656	71.971290
673.265707	55.228381	71.976295
672.234808	52.670664	71.981300
671.145104	53.060232	71.986305
670.797126	54.101264	71.991310
670.319968	54.987820	71.996314
669.471798	57.026302	72.001319
668.535734	51.534490	72.006324
667.661958	55.193458	72.011329
667.857710	46.924136	72.016334
667.202293	50.751764	72.021338
665.728578	52.224366	72.026343
665.162987	58.196584	72.031348
664.453737	53.729967	72.036353
664.507693	42.106905	72.041358
663.581829	57.782895	72.046362
662.853197	51.083202	72.051367
662.542438	51.549017	72.056372
661.456345	54.021210	72.061377
660.893688	51.234394	72.066382
659.788988	57.125297	72.071386
659.511490	55.553084	72.076391
659.081422	50.233022	72.081396
658.128064	57.413454	72.086401
657.793291	43.455275	72.091406
656.655058	61.762377	72.096410
656.130331	55.460732	72.101415
655.981319	52.606474	72.106420
654.559902	51.878748	72.111425
653.950464	44.398399	72.116430
653.021435	53.819002	72.121434
653.074914	44.771230	72.126439
652.857640	48.041805	72.131444
651.887538	52.146632	72.136449
651.172375	43.727467	72.141454
650.588371	55.994779	72.146458
649.095702	48.647189	72.151463
648.743667	37.325329	72.156468
648.008353	45.827241	72.161473
647.537650	40.772281	72.166478
647.224119	38.672790	72.171482
646.678970	40.435939	72.176487
646.018034	49.060053	72.181492
645.417384	43.817623	72.186497
644.383815	46.860210	72.191502
643.205829	54.910638	72.196506
643.162493	48.762583	72.201511
642.785015	46.886167	72.206516
641.351066	44.898859	72.211521
640.749075	45.437862	72.216526
640.122046	50.450020	72.221530
639.614711	51.358734	72.226535
639.413666	41.227106	72.231540
638.351022	45.009198	72.236545
637.646443	42.350649	72.241550
637.268538	54.157779	72.246554
636.561295	42.531353	72.251559
635.909697	46.374149	72.256564
634.553789	53.293830	72.261569
634.625891	51.964000	72.266574
633.860095	57.187497	72.271578
633.240633	50.781097	72.276583
632.182520	48.390162	72.281588
631.537416	58.536704	72.286593
631.022235	52.790224	72.291598
630.858200	53.530727	72.296602
629.949972	52.737063	72.301607
629.388716	52.361239	72.306612
628.232087	54.273810	72.311617
627.988090	44.797162	72.316622
627.117614	54.998516	72.321626
626.312662	53.925050	72.326631
626.046677	58.559592	72.331636
625.379247	49.285993	72.336641
624.494515	42.691603	72.341646
623.553851	38.435324	72.346650
623.208761	46.436698	72.351655
622.935834	37.431450	72.356660
621.850757	48.129032	72.361665
621.200549	46.253473	72.366670
620.560251	51.054856	72.371674
620.015538	44.880991	72.376679
619.163720	44.858953	72.381684
617.962519	51.848623	72.386689
617.542106	46.968590	72.391694
617.338834	53.274206	72.396698
616.912898	49.948379	72.401703
616.564020	46.364272	72.406708
614.968549	52.199302	72.411713
614.522279	44.995761	72.416718
614.130114	47.521469	72.421722
613.731683	44.052489	72.426727
612.483239	45.241660	72.431732
611.642835	52.779437	72.436737
611.211098	41.541241	72.441742
611.166603	51.418665	72.446746
610.084722	50.597468	72.451751
609.394577	43.637775	72.456756
608.888189	58.772302	72.461761
607.842437	39.174535	72.466766
606.922088	55.117741	72.471770
606.566204	42.358293	72.476775
606.007099	44.445377	72.481780
605.698710	50.187403	72.486785
604.759927	40.178003	72.491790
603.691933	48.751830	72.496794
603.232844	51.732907	72.501799
602.810342	48.848092	72.506804
602.148549	52.889643	72.511809
601.288250	46.057977	72.516814
600.868565	51.923386	72.521818
599.883701	56.642452	72.526823
599.846310	47.705349	72.531828
598.660373	59.082918	72.536833
597.870827	52.884968	72.541838
597.158377	53.173486	72.546842
596.513051	55.849904	72.551847
596.727421	53.297331	72.556852
595.328229	59.468553	72.561857
594.963016	62.750079	72.566862
594.238837	57.910540	72.571866
593.270792	48.987609	72.576871
592.586252	49.153410	72.581876
591.355441	53.653022	72.586881
591.141970	51.305786	72.591886
590.912342	48.659919	72.596890
590.478259	54.086069	72.601895
590.317810	53.800965	72.606900
588.909349	61.105940	72.611905
588.479975	53.830324	72.616910
587.075252	53.640883	72.621914
586.153208	59.351334	72.626919
585.806315	47.301675	72.631924
585.384337	56.712507	72.636929
585.370780	49.460558	72.641934
584.777170	48.820234	72.646938
583.909946	52.025589	72.651943
583.197444	53.741288	72.656948
582.258587	52.750665	72.661953
581.467819	55.981694	72.666958
580.616078	48.768619	72.671962
580.103310	50.807329	72.676967
579.942645	36.621173	72.681972
578.936346	56.697148	72.686977
578.192962	47.013033	72.691982
577.258406	58.140834	72.696986
576.995404	51.584637	72.701991
576.786279	51.979081	72.706996
575.449454	52.543669	72.712001
575.250653	42.873751	72.717006
574.088666	54.829417	72.722010
573.311709	50.834093	72.727015
573.385834	54.443047	72.732020
572.375402	60.412011	72.737025
571.687940	50.294783	72.742030
571.285973	46.176658	72.747034
570.036204	49.953887	72.752039
569.440017	48.984388	72.757044
568.674080	56.824136	72.762049
568.459285	47.246652	72.767054
568.246903	46.400532	72.772058
567.337105	52.328235	72.777063
566.693018	45.285526	72.782068
565.980538	55.154220	72.787073
564.774768	48.707181	72.792078
563.714888	46.691880	72.797082
562.890362	48.583123	72.802087
562.794309	48.024410	72.807092
562.269291	50.760522	72.812097
562.251313	42.777562	72.817102
561.771430	53.935450	72.822106
560.433987	60.612528	72.827111
560.012914	56.380749	72.832116
559.157308	65.136819	72.837121
558.398034	52.438472	72.842126
557.890959	55.266347	72.847130
557.058002	55.119899	72.852135
556.562505	53.418416	72.857140
556.255526	55.952642	72.862145
555.495369	53.906952	72.867150
554.835066	62.228208	72.872154
553.776772	49.873964	72.877159
552.667475	46.062473	72.882164
552.139852	54.662218	72.887169
551.837910	58.250644	72.892174
551.409785	54.215536	72.897178
550.594211	51.325528	72.902183
549.908959	50.412798	72.907188
549.172500	63.918685	72.912193
548.848174	58.696923	72.917198
548.038680	55.288696	72.922202
546.816282	58.172161	72.927207
546.335865	49.781876	72.932212
545.499866	52.491829	72.937217
545.677293	48.816020	72.942222
545.226055	50.721931	72.947226
543.817863	62.650595	72.952231
543.184065	61.860560	72.957236
542.709093	65.058648	72.962241
541.999640	58.141472	72.967246
541.063268	58.145545	72.972250
540.102567	66.535154	72.977255
539.994943	53.805560	72.982260
539.466114	61.208574	72.987265
539.080508	53.500213	72.992270
537.721158	59.641463	72.997274
537.048014	54.104674	73.002279
536.758707	54.699554	73.007284
536.251780	66.713331	73.012289
535.194703	56.449978	73.017294
534.529731	55.890420	73.022298
534.041303	59.084343	73.027303
533.894582	51.104541	73.032308
532.773167	60.322432	73.037313
532.157842	58.250525	73.042318
531.564081	51.994607	73.047322
530.936894	57.375828	73.052327
529.705059	51.874417	73.057332
529.141767	57.679131	73.062337
528.732830	52.544970	73.067342
528.265579	55.264003	73.072346
527.218668	52.603243	73.077351
526.599690	51.150098	73.082356
525.742457	55.252760	73.087361
525.658060	55.029665	73.092366
525.091023	49.815032	73.097370
524.085870	54.512123	73.102375
523.504326	47.137761	73.107380
522.676681	54.738185	73.112385
522.232734	49.426674	73.117390
521.307988	45.642573	73.122394
520.455701	59.020250	73.127399
520.336056	57.717807	73.132404
519.410267	66.060859	73.137409
518.990076	51.395638	73.142414
518.103019	53.698988	73.147418
517.492512	53.094488	73.152423
517.324886	50.192745	73.157428
516.412861	43.284198	73.162433
515.271928	51.330348	73.167438
514.548778	52.998875	73.172442
513.725918	59.622390	73.177447
513.634779	49.194149	73.182452
513.517635	52.160194	73.187457
512.456796	57.151595	73.192462
511.795282	52.757851	73.197466
510.884850	52.778304	73.202471
510.033873	48.168734	73.207476
509.326738	59.049010	73.212481
509.118058	58.924562	73.217486
508.526012	53.318093	73.222490
507.593840	53.496555	73.227495
506.948765	50.235621	73.232500
506.191364	51.857566	73.237505
505.609006	53.260812	73.242510
505.214042	56.162303	73.247514
504.251308	55.006777	73.252519
503.705945	45.567121	73.257524
502.954608	54.744990	73.262529
502.591752	54.205125	73.267534
501.514059	52.046030	73.272538
500.719952	54.845520	73.277543
500.551826	55.827961	73.282548
499.834808	61.942603	73.287553
498.845975	52.097340	73.292558
498.135185	54.981331	73.297562
497.441858	58.032855	73.302567
497.321323	46.965893	73.307572
496.638228	53.712227	73.312577
495.446990	57.745102	73.317582
495.098046	53.490809	73.322586
494.348096	65.590611	73.327591
493.800889	46.623130	73.332596
492.805009	56.808224	73.337601
492.057663	58.171524	73.342606
491.594376	58.169639	73.347610
491.101120	60.241529	73.352615
491.047170	53.540078	73.357620
489.861829	56.758293	73.362625
489.120510	54.585043	73.367630
488.751632	54.558658	73.372634
487.531180	54.051331	73.377639
486.735623	54.837252	73.382644
486.224752	60.102180	73.387649
485.712546	50.057993	73.392654
485.498846	58.213494	73.397658
484.587135	64.150994	73.402663
483.883725	43.582538	73.407668
483.180502	58.023014	73.412673
482.563686	56.689386	73.417678
482.227751	52.584413	73.422682
480.960827	53.246728	73.427687
480.385414	53.574950	73.432692
479.613284	61.021462	73.437697
479.415008	48.916616	73.442702
478.230031	43.688474	73.447706
477.517548	51.773618	73.452711
477.311449	45.337689	73.457716
476.429420	56.523379	73.462721
476.389673	46.881756	73.467726
475.534778	44.201471	73.472730
474.041854	50.026552	73.477735
473.854939	48.575554	73.482740
473.312160	52.738525	73.487745
472.626671	52.768889	73.492750
471.699797	47.146388	73.497754
471.192582	52.525853	73.502759
471.090035	35.906646	73.507764
470.117585	49.834909	73.512769
469.090334	51.484084	73.517774
468.812722	57.478266	73.522778
468.083839	51.491480	73.527783
467.587865	40.478030	73.532788
466.382320	41.192076	73.537793
465.798402	52.022761	73.542798
465.531998	45.996994	73.547802
464.602599	54.176624	73.552807
463.991259	49.005337	73.557812
463.422806	55.608835	73.562817
463.137710	51.295490	73.567822
462.173859	54.755979	73.572826
461.155544	57.190648	73.577831
460.821644	44.512894	73.582836
460.144522	54.241930	73.587841
459.536914	51.493867	73.592846
458.598028	49.350525	73.597850
457.610058	57.219364	73.602855
457.562825	49.028179	73.607860
456.763497	53.314028	73.612865
456.041768	48.963013	73.617870
455.447619	49.986520	73.622874
454.697826	58.460822	73.627879
454.645880	49.365202	73.632884
453.238657	64.938153	73.637889
452.518099	53.889514	73.642894
452.377496	50.392104	73.647898
451.598111	49.264161	73.652903
450.659705	57.617123	73.657908
449.624507	57.911369	73.662913
449.153623	51.689518	73.667918
448.604951	50.075379	73.672922
448.425068	51.636870	73.677927
448.262438	49.339899	73.682932
447.005483	54.558113	73.687937
446.198960	53.748313	73.692942
445.775239	52.825486	73.697946
444.347036	48.337867	73.702951
444.286148	52.178059	73.707956
443.504616	51.279122	73.712961
442.924415	45.484706	73.717966
442.418271	46.927864	73.722970
441.591141	52.008213	73.727975
441.082431	51.157275	73.732980
440.347880	52.744058	73.737985
439.254943	51.527300	73.742990
438.756251	53.456558	73.747994
438.155732	57.437921	73.752999
437.903832	49.940101	73.758004
436.878208	55.678138	73.763009
435.889570	48.706136	73.768014
435.519735	52.821059	73.773018
435.075502	48.372222	73.778023
434.819097	50.803782	73.783028
433.712128	49.254943	73.788033
432.709546	45.499049	73.793038
432.026446	52.119239	73.798042
431.724404	53.780620	73.803047
431.209806	40.246983	73.808052
430.129258	51.309765	73.813057
429.809647	54.845821	73.818062
429.488831	50.306357	73.823066
427.942243	55.280562	73.828071
427.351696	46.699699	73.833076
426.703969	46.791869	73.838081
426.114896	49.599714	73.843086
426.124560	49.891501	73.848090
425.551526	50.676680	73.853095
424.416879	47.246189	73.858100
423.527434	49.761264	73.863105
423.543786	44.250281	73.868110
422.034859	51.665959	73.873114
420.903200	46.227498	73.878119
420.825754	47.944560	73.883124
420.384634	51.846911	73.888129
420.230565	48.384768	73.893134
419.596821	50.236197	73.898138
418.321524	57.035903	73.903143
418.096627	48.281664	73.908148
417.496311	50.235002	73.913153
416.289045	56.079259	73.918158
415.537951	58.184358	73.923162
414.929834	60.837544	73.928167
414.755069	46.051256	73.933172
413.560285	51.581282	73.938177
413.001074	53.777235	73.943182
412.511189	43.125537	73.948186
411.787596	48.760262	73.953191
411.597505	49.156417	73.958196
410.288609	46.343486	73.963201
409.730885	46.306201	73.968206
409.190986	48.342957	73.973210
408.462622	51.333851	73.978215
408.068282	39.481045	73.983220
407.095872	54.639364	73.988225
406.415374	45.754291	73.993230
406.098794	45.399459	73.998234
405.234492	50.212923	74.003239
404.604179	46.970169	74.008244
403.589225	45.580150	74.013249
403.527972	46.288520	74.018254
402.994341	46.908151	74.023258
401.715225	59.729379	74.028263
401.082156	48.313582	74.033268
400.326858	53.201144	74.038273
400.204382	54.493290	74.043278
399.262309	54.085156	74.048282
398.409964	55.077276	74.053287
398.135463	41.723016	74.058292
397.569927	52.978142	74.063297
396.556321	55.811060	74.068302
395.989016	56.764070	74.073306
395.301747	53.891521	74.078311
394.977701	51.278069	74.083316
393.821625	53.479243	74.088321
392.852013	45.991713	74.093326
392.514769	49.773435	74.098330
391.855013	57.824966	74.103335
391.771519	52.028689	74.108340
390.716359	62.210646	74.113345
390.019467	56.018512	74.118350
389.440671	54.010212	74.123354
388.759140	60.433041	74.128359
388.147462	48.249006	74.133364
386.756677	60.356315	74.138369
386.270248	56.986557	74.143374
386.201107	51.099682	74.148378
385.487485	56.682364	74.153383
385.612896	42.431738	74.158388
384.370116	56.116094	74.163393
383.828478	52.278887	74.168398
382.541371	51.496801	74.173402
381.748130	55.882628	74.178407
380.940927	59.160487	74.183412
380.339497	58.718582	74.188417
380.032231	57.334078	74.193422
379.738847	48.524526	74.198426
378.761959	68.296240	74.203431
378.092876	50.989861	74.208436
377.473784	54.441176	74.213441
377.259076	55.095151	74.218446
376.121888	46.844265	74.223450
375.204141	53.128113	74.228455
374.918168	47.952317	74.233460
374.280600	47.872568	74.238465
373.634541	58.189614	74.243470
372.787319	49.805789	74.248474
372.085274	47.850250	74.253479
371.897153	52.149116	74.258484
371.186153	48.923959	74.263489
370.116070	54.740067	74.268494
369.436515	49.655374	74.273498
369.065201	51.952284	74.278503
368.322568	48.434120	74.283508
367.558015	45.351543	74.288513
366.684525	52.703840	74.293518
366.425707	52.178956	74.298522
365.699492	61.535783	74.303527
364.846100	48.349468	74.308532
364.010399	55.992218	74.313537
363.590575	53.879742	74.318542
363.389900	51.860081	74.323546
362.328917	55.731905	74.328551
361.497420	47.132688	74.333556
360.837784	57.701062	74.338561
360.520090	50.535444	74.343566
359.697961	50.023056	74.348570
358.927307	55.021888	74.353575
358.742225	52.887776	74.358580
357.640886	56.113164	74.363585
356.265573	55.761470	74.368590
355.862851	60.551860	74.373594
355.483048	63.397337	74.378599
355.206415	54.026867	74.383604
354.888444	57.196809	74.388609
354.243688	56.399109	74.393614
353.203747	53.235838	74.398618
352.486996	53.924086	74.403623
351.679398	51.258387	74.408628
350.557946	49.793897	74.413633
350.151301	42.618805	74.418638
349.843796	40.461627	74.423642
349.122866	46.890738	74.428647
348.749354	48.271776	74.433652
347.630509	50.932245	74.438657
346.766206	50.122225	74.443662
346.480560	48.251727	74.448666
346.141814	60.046319	74.453671
345.369854	47.350094	74.458676
344.355037	53.840235	74.463681
344.022770	53.970466	74.468686
343.404998	50.090208	74.473690
342.233057	60.293943	74.478695
341.807857	52.823757	74.483700
341.132397	47.315791	74.488705
340.361048	51.669754	74.493710
339.778311	46.057125	74.498714
338.674159	55.630303	74.503719
338.316869	54.119734	74.508724
337.675529	59.397591	74.513729
337.608345	50.585115	74.518734
336.903895	45.745679	74.523738
335.598895	48.626633	74.528743
335.496640	45.957346	74.533748
334.786010	54.827559	74.538753
333.534894	58.340182	74.543758
332.907106	53.628878	74.548762
332.274145	54.906185	74.553767
332.460085	49.669381	74.558772
331.562688	52.152638	74.563777
330.438003	51.507124	74.568782
330.241616	44.301683	74.573786
329.248660	61.122280	74.578791
329.005039	56.231480	74.583796
328.038008	49.243470	74.588801
327.375911	50.180062	74.593806
326.784517	44.166689	74.598810
325.246387	54.777296	74.603815
325.017582	44.762117	74.608820
324.486076	53.756752	74.613825
324.057542	53.896019	74.618830
323.685170	51.181469	74.623834
322.327607	56.606588	74.628839
321.830007	55.053727	74.633844
321.064576	55.551043	74.638849
320.656146	54.307252	74.643854
320.691996	47.064799	74.648858
319.401548	50.391304	74.653863
318.796872	43.533213	74.658868
318.319284	44.446710	74.663873
317.301418	48.440990	74.668878
316.562745	54.806706	74.673882
315.612907	51.581784	74.678887
315.378429	42.767592	74.683892
314.986273	45.332761	74.688897
313.937285	50.765475	74.693902
313.428538	45.126869	74.698906
312.857930	53.463830	74.703911
312.183217	51.368332	74.708916
311.635541	50.315472	74.713921
310.601292	46.440098	74.718926
310.117512	48.742323	74.723930
309.452047	56.149794	74.728935
308.743636	53.824699	74.733940
307.697158	45.635090	74.738945
307.148526	47.912957	74.743950
306.852634	37.582045	74.748954
306.326896	47.217587	74.753959
305.954987	41.401056	74.758964
305.049306	43.098730	74.763969
304.325524	44.313244	74.768974
303.806027	43.889840	74.773978
302.433210	49.851992	74.778983
301.796441	41.657015	74.783988
301.117286	48.849043	74.788993
300.814171	45.155197	74.793998
300.703940	36.064162	74.799002
299.568801	46.698860	74.804007
298.971806	39.464233	74.809012
298.244037	43.059041	74.814017
297.422026	46.028618	74.819022
296.783284	42.714699	74.824026
295.690254	47.706577	74.829031
295.585447	45.241129	74.834036
294.930334	49.434650	74.839041
294.625815	52.834269	74.844046
293.911238	40.803873	74.849050
292.852234	43.732374	74.854055
292.762759	44.620288	74.859060
291.762939	41.960017	74.864065
290.666588	53.282410	74.869070
290.169211	49.712568	74.874074
289.593692	43.999455	74.879079
289.220925	47.589725	74.884084
287.945256	49.374761	74.889089
287.360656	50.634908	74.894094
286.993985	44.998897	74.899098
286.293501	46.911458	74.904103
286.142012	41.627511	74.909108
285.046626	41.046736	74.914113
284.550724	38.362923	74.919118
284.044706	36.792490	74.924122
283.225169	43.562187	74.929127
282.685574	44.040866	74.934132
282.046491	51.855726	74.939137
280.703035	44.569764	74.944142
280.224451	31.123491	74.949146
279.383129	46.210474	74.954151
279.091736	40.899940	74.959156
278.611033	47.981493	74.964161
277.772685	48.685989	74.969166
276.937233	47.483460	74.974170
276.459037	47.687422	74.979175
276.009860	41.629320	74.984180
274.917642	47.497874	74.989185
273.994396	45.836247	74.994190
273.608976	43.319332	74.999194
272.870085	52.227176	75.004199
272.866047	37.415296	75.009204
272.244295	43.145784	75.014209
271.094689	47.008112	75.019214
270.634702	40.049705	75.024218
270.040976	45.360982	75.029223
269.282310	47.177164	75.034228
268.224490	44.273831	75.039233
267.786974	52.728358	75.044238
267.531620	43.532719	75.049242
266.378709	46.900406	75.054247
265.515386	52.803447	75.059252
265.138155	53.986390	75.064257
264.427818	46.894418	75.069262
264.215611	34.138983	75.074266
262.847534	57.626906	75.079271
262.115822	42.767003	75.084276
261.819336	42.139324	75.089281
261.222636	46.452853	75.094286
260.929610	41.205662	75.099290
259.695747	52.975766	75.104295
259.417457	46.418912	75.109300
259.006863	43.790893	75.114305
258.374491	44.694379	75.119310
257.506911	45.383040	75.124314
256.331976	46.402972	75.129319
256.308327	45.856386	75.134324
254.794432	45.052169	75.139329
253.890782	44.805127	75.144334
253.920080	41.905139	75.149338
253.058258	49.979437	75.154343
252.846671	36.930587	75.159348
252.374607	32.296996	75.164353
251.175284	41.292423	75.169358
250.647313	44.126834	75.174362
250.071676	51.207754	75.179367
249.730865	39.295999	75.184372
248.813338	40.968772	75.189377
247.889344	47.505968	75.194382
247.602107	41.563987	75.199386
246.732042	48.594066	75.204391
245.686488	47.764087	75.209396
245.593326	39.455672	75.214401
244.687873	43.269631	75.219406
244.307526	49.261272	75.224410
243.103455	45.163837	75.229415
242.544384	44.496015	75.234420
241.824012	47.227054	75.239425
241.421656	54.442784	75.244430
241.370743	48.245509	75.249434
239.924515	45.891387	75.254439
239.191557	47.938449	75.259444
238.631246	47.937886	75.264449
238.300371	48.823280	75.269454
237.685143	47.995674	75.274458
236.581646	54.734957	75.279463
236.294404	50.073481	75.284468
235.721315	43.498968	75.289473
234.671053	53.021011	75.294478
234.006561	49.006306	75.299482
233.381485	48.918295	75.304487
232.833653	46.111881	75.309492
232.438559	47.308715	75.314497
231.023252	48.297589	75.319502
230.732498	37.852332	75.324506
230.184391	50.926101	75.329511
229.646155	41.015464	75.334516
229.236113	46.955067	75.339521
227.858038	47.192098	75.344526
227.731707	39.729500	75.349530
227.017492	48.696496	75.354535
226.311123	51.961480	75.359540
225.173220	53.508541	75.364545
224.759512	49.576865	75.369550
224.528432	45.743813	75.374554
223.923930	42.353494	75.379559
223.033692	38.161890	75.384564
222.453582	37.984711	75.389569
221.431958	46.902939	75.394574
221.301493	46.330803	75.399578
219.786232	54.364195	75.404583
219.375183	50.753800	75.409588
218.666857	45.304732	75.414593
218.054057	50.202740	75.419598
218.190103	43.100445	75.424602
216.881322	52.816671	75.429607
216.121486	48.203727	75.434612
215.559957	52.663049	75.439617
214.780403	54.460500	75.444622
214.676935	48.826700	75.449626
213.694614	52.033173	75.454631
212.931949	50.498937	75.459636
212.540246	46.027586	75.464641
211.972951	48.743692	75.469646
210.935240	46.939485	75.474650
209.861232	56.897416	75.479655
209.841106	44.229637	75.484660
209.540093	45.692178	75.489665
208.546606	49.810348	75.494670
207.953610	46.392966	75.499674
207.414838	52.256900	75.504679
206.204838	53.315562	75.509684
205.029834	54.494803	75.514689
204.777190	51.879461	75.519694
204.652370	48.336982	75.524698
204.122646	55.336474	75.529703
203.358416	49.459500	75.534708
202.266647	58.000988	75.539713
201.679124	51.275816	75.544718
201.387312	48.709298	75.549722
200.374352	61.418785	75.554727
199.546345	50.893593	75.559732
198.723804	51.862104	75.564737
198.298184	56.835935	75.569742
198.420266	53.566336	75.574746
197.421830	57.893461	75.579751
196.620820	55.909596	75.584756
195.866905	60.412210	75.589761
195.397007	59.594562	75.594766
194.245194	48.017112	75.599770
193.600438	57.641685	75.604775
193.173970	49.097820	75.609780
192.664712	49.865000	75.614785
192.087055	52.964391	75.619790
191.637768	50.588561	75.624794
190.754241	56.316647	75.629799
190.176333	52.395385	75.634804
188.950725	53.863403	75.639809
188.291861	54.014182	75.644814
188.147004	42.558487	75.649818
187.441765	53.681364	75.654823
187.068318	48.841248	75.659828
186.096021	48.280318	75.664833
185.161222	56.391504	75.669838
184.930427	42.964097	75.674842
183.683168	50.130023	75.679847
183.140322	46.250485	75.684852
182.496830	50.331789	75.689857
182.078478	55.488970	75.694862
181.294138	48.150201	75.699866
180.381163	49.186753	75.704871
179.889352	53.239146	75.709876
179.408257	47.235040	75.714881
178.753274	62.577781	75.719886
177.746651	51.115966	75.724890
176.828254	60.402541	75.729895
176.434864	52.470003	75.734900
176.260624	50.964971	75.739905
175.868925	62.708084	75.744910
175.109286	55.057865	75.749914
174.194235	54.361655	75.754919
173.557467	50.790410	75.759924
172.492757	47.106039	75.764929
171.867752	62.781475	75.769934
171.422264	51.045695	75.774938
170.648552	54.874948	75.779943
170.391753	52.474741	75.784948
169.477391	53.252894	75.789953
168.474625	64.462642	75.794958
168.714295	57.156159	75.799962
167.409988	60.812961	75.804967
166.483244	56.912627	75.809972
166.235708	54.077276	75.814977
165.445221	56.193456	75.819982
165.143556	52.617672	75.824986
163.800466	54.564910	75.829991
163.093885	44.443008	75.834996
162.561885	48.960710	75.840001
162.073564	47.822727	75.845006
162.139500	36.935837	75.850010
160.898856	51.687537	75.855015
159.571139	52.638831	75.860020
159.768625	51.172307	75.865025
159.168187	56.885231	75.870030
158.336068	51.739775	75.875034
157.568706	55.941762	75.880039
156.999296	48.005755	75.885044
156.414921	49.161815	75.890049
155.119440	59.386891	75.895054
154.810199	52.503824	75.900058
153.902768	62.700149	75.905063
153.761571	45.757577	75.910068
153.012474	47.025057	75.915073
152.112629	51.923113	75.920078
151.466405	48.015909	75.925082
150.747503	55.425622	75.930087
150.446653	54.369715	75.935092
149.784599	55.933983	75.940097
148.743002	58.269981	75.945102
148.507370	49.799782	75.950106
147.905767	52.412561	75.955111
147.336528	57.865042	75.960116
146.493907	57.627233	75.965121
145.729879	61.819232	75.970126
145.467393	55.758198	75.975130
143.826955	56.518085	75.980135
143.411489	55.012093	75.985140
142.943357	57.969451	75.990145
142.437053	58.252039	75.995150
141.662456	46.381085	76.000154
140.385832	57.888393	76.005159
140.178054	46.754977	76.010164
139.851741	50.971802	76.015169
139.392762	58.603430	76.020174
138.734947	43.947847	76.025178
137.684076	48.114615	76.030183
137.127978	34.956718	76.035188
136.536063	43.962577	76.040193
135.521887	55.538427	76.045198
135.061596	39.247573	76.050202
134.462917	52.340452	76.055207
133.716954	42.847748	76.060212
132.969723	46.396817	76.065217
131.810615	49.152108	76.070222
131.815528	43.026369	76.075226
131.153103	46.525645	76.080231
130.692211	47.222046	76.085236
130.300811	46.358779	76.090241
128.866042	46.962878	76.095246
128.470981	31.897981	76.100250
127.936248	49.404069	76.105255
126.901159	42.135269	76.110260
126.107154	33.875542	76.115265
125.351971	44.597950	76.120270
125.229708	38.530339	76.125274
124.643960	46.912314	76.130279
124.410209	43.065510	76.135284
123.540736	36.806378	76.140289
122.773049	39.328946	76.145294
122.309610	35.285376	76.150298
120.790071	45.916772	76.155303
120.175379	35.209378	76.160308
119.773309	39.446166	76.165313
119.054969	49.964006	76.170318
119.049302	37.642452	76.175322
117.588364	49.677475	76.180327
116.785114	45.632893	76.185332
116.667869	41.851093	76.190337
115.928587	43.377219	76.195342
115.844402	42.600588	76.200346
114.839794	51.025701	76.205351
113.973794	49.476435	76.210356
113.621924	40.651039	76.215361
112.174842	54.005362	76.220366
111.891988	48.039050	76.225370
111.108924	45.561916	76.230375
111.007635	48.479707	76.235380
110.124682	46.724985	76.240385
108.992675	46.990655	76.245390
108.557316	43.685363	76.250394
107.966705	52.137506	76.255399
107.338996	45.191691	76.260404
106.401124	42.726629	76.265409
105.584771	52.462153	76.270414
105.355018	40.138485	76.275418
104.726872	48.689653	76.280423
104.543083	44.508450	76.285428
103.404126	41.793176	76.290433
102.306536	40.616740	76.295438
102.521243	42.561612	76.300442
101.763707	49.638443	76.305447
100.540730	49.566958	76.310452
100.569875	35.121984	76.315457
99.563397	47.787875	76.320462
98.506738	36.493367	76.325466
97.544778	42.222943	76.330471
97.196308	41.893738	76.335476
97.274266	31.268296	76.340481
96.545931	41.059167	76.345486
95.325757	36.811416	76.350490
94.601685	40.159679	76.355495
94.143817	43.870775	76.360500
93.708188	37.343776	76.365505
92.521851	43.594841	76.370510
92.137128	40.190014	76.375514
91.528444	44.035548	76.380519
91.067432	46.353103	76.385524
90.460835	34.698247	76.390529
89.101947	50.594783	76.395534
88.853811	37.775728	76.400538
88.543234	47.963618	76.405543
87.390036	37.402032	76.410548
86.550438	44.261712	76.415553
85.822927	49.187500	76.420558
85.946572	40.929688	76.425562
84.836027	42.313174	76.430567
84.096553	45.627626	76.435572
83.761110	42.894617	76.440577
82.742017	46.469705	76.445582
82.431034	36.308412	76.450586
81.439147	41.881915	76.455591
80.833184	45.380084	76.460596
80.171527	34.514613	76.465601
79.710712	47.702205	76.470606
79.404945	41.991871	76.475610
78.346555	34.796202	76.480615
77.485285	44.950480	76.485620
77.121194	33.804167	76.490625
76.097534	49.311354	76.495630
75.759590	49.164979	76.500634
74.988419	40.095795	76.505639
74.281502	43.537523	76.510644
74.094437	40.681505	76.515649
72.796010	38.043718	76.520654
72.156193	45.991194	76.525658
71.946220	45.755025	76.530663
70.966576	50.175392	76.535668
70.278217	39.107596	76.540673
69.226210	43.332919	76.545678
69.233770	38.134023	76.550682
68.590284	40.556375	76.555687
67.485398	43.457590	76.560692
67.008430	34.279994	76.565697
65.818443	46.415334	76.570702
65.550706	37.440915	76.575706
65.347910	46.094569	76.580711
64.762331	53.377380	76.585716
63.686627	47.904951	76.590721
62.969649	46.931188	76.595726
62.551924	49.226076	76.600730
61.568668	43.177504	76.605735
60.913265	42.728516	76.610740
60.481263	49.384431	76.615745
59.712669	48.887262	76.620750
59.642426	48.021676	76.625754
58.702979	42.275206	76.630759
57.730668	50.540643	76.635764
57.298748	36.106124	76.640769
56.227053	41.928909	76.645774
55.539018	47.764629	76.650778
55.255602	35.425879	76.655783
54.817877	44.610589	76.660788
54.340968	50.221827	76.665793
52.950191	52.039531	76.670798
52.743635	44.203390	76.675802
52.267999	47.898403	76.680807
51.268908	44.974766	76.685812
50.346036	48.760028	76.690817
49.595811	55.074031	76.695822
49.316532	43.892114	76.700826
48.467473	48.165505	76.705831
47.313041	49.869825	76.710836
47.087608	41.030589	76.715841
46.207234	47.109876	76.720846
46.261996	37.033766	76.725850
45.825357	45.849293	76.730855
44.860129	50.928122	76.735860
44.121893	37.889192	76.740865
43.374657	50.833882	76.745870
42.153678	47.302231	76.750874
41.360555	45.872258	76.755879
40.945249	45.837576	76.760884
40.766286	43.115888	76.765889
40.195427	49.235702	76.770894
39.731359	35.468645	76.775898
38.725170	45.909400	76.780903
37.881740	42.989329	76.785908
37.944777	42.583465	76.790913
36.550659	43.548568	76.795918
35.861654	36.197814	76.800922
35.311902	43.687802	76.805927
34.634272	46.259113	76.810932
33.767525	45.388094	76.815937
32.653160	44.573914	76.820942
32.669121	46.388049	76.825946
31.938179	45.845459	76.830951
31.374408	43.749700	76.835956
31.203967	41.709483	76.840961
29.538634	44.039347	76.845966
29.107481	42.157407	76.850970
28.819025	40.009854	76.855975
28.476921	36.473663	76.860980
27.536340	43.880904	76.865985
26.576740	59.139774	76.870990
25.995615	38.951032	76.875994
25.512078	48.589336	76.880999
24.834789	50.719044	76.886004
23.875087	39.014869	76.891009
22.984780	43.099300	76.896014
22.851282	45.561752	76.901018
22.677076	41.839508	76.906023
21.573329	53.454907	76.911028
21.116252	42.768138	76.916033
20.098473	45.068847	76.921038
19.623680	53.828965	76.926042
18.471734	49.672874	76.931047
17.451785	55.291881	76.936052
17.312454	34.520170	76.941057
16.746460	45.756480	76.946062
16.723163	46.591268	76.951066
15.781124	42.761251	76.956071
14.804607	49.229624	76.961076
14.325964	36.707554	76.966081
13.818884	37.662080	76.971086
12.925525	44.003647	76.976090
11.985116	40.211220	76.981095
11.384309	42.538468	76.986100
11.360088	37.371454	76.991105
10.346653	48.007341	76.996110
9.687360	56.296989	77.001114
9.329511	48.314671	77.006119
8.299255	46.212894	77.011124
7.395840	37.002405	77.016129
6.633213	42.727027	77.021134
6.539229	40.863854	77.026139
5.929459	42.003498	77.031143
4.796803	44.576428	77.036148
4.302093	40.414868	77.041153
3.673896	47.283432	77.046158