Fri Mar 05 18:35:23 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-0.695900	101.849820	0.000000
-1.393622	87.432476	0.005005
-2.104846	52.773713	0.010010
-4.162442	19.089885	0.015014
-8.651000	18.889655	0.020019
-13.656382	8.895333	0.025024
-18.749863	8.099325	0.030029
-22.969909	5.099757	0.035034
-27.223470	8.683065	0.040038
-30.592522	6.687911	0.045043
-34.299630	2.770751	0.050048
-38.161972	8.538846	0.055053
-41.462373	11.460772	0.060058
-45.358334	5.588355	0.065062
-49.391085	13.551979	0.070067
-52.689585	5.381245	0.075072
-56.650793	10.086497	0.080077
-60.468626	12.272547	0.085082
-64.457934	11.817734	0.090086
-68.285526	15.564973	0.095091
-71.812203	14.780900	0.100096
-75.495011	17.689761	0.105101
-78.772935	3.974327	0.110106
-82.803385	8.741129	0.115110
-87.213652	14.714988	0.120115
-90.560158	6.731741	0.125120
-94.529181	11.414645	0.130125
-97.893980	15.401910	0.135130
-101.648531	4.839211	0.140134
-105.982167	9.042560	0.145139
-109.696440	-1.807246	0.150144
-113.514113	12.288090	0.155149
-117.051612	12.453565	0.160154
-120.426066	13.439861	0.165158
-124.516992	3.285688	0.170163
-127.790299	-2.042534	0.175168
-131.620685	9.914916	0.180173
-135.632274	0.837788	0.185178
-139.758304	6.380027	0.190182
-143.598186	4.903286	0.195187
-147.230681	-6.278050	0.200192
-151.030575	15.768702	0.205197
-154.831542	2.643049	0.210202
-158.700275	11.039569	0.215206
-162.517714	4.721153	0.220211
-165.897560	4.530382	0.225216
-169.796653	10.134231	0.230221
-173.320392	8.955598	0.235226
-177.006708	0.474769	0.240230
-180.821434	10.551630	0.245235
-184.733155	5.153474	0.250240
-188.865042	23.099548	0.255245
-192.007844	13.354009	0.260250
-195.886164	4.651535	0.265254
-200.117592	12.587178	0.270259
-203.646122	7.567873	0.275264
-207.376165	9.957763	0.280269
-210.976784	15.928786	0.285274
-214.801726	10.934724	0.290278
-218.535580	8.488696	0.295283
-222.004703	1.635395	0.300288
-226.355456	10.600957	0.305293
-229.627898	15.141366	0.310298
-233.596688	7.262375	0.315302
-237.662646	19.959332	0.320307
-240.807539	12.667951	0.325312
-244.906069	14.716161	0.330317
-248.628786	21.302819	0.335322
-252.407844	12.452129	0.340326
-256.443712	9.977093	0.345331
-259.703178	13.212900	0.350336
-263.771801	16.382319	0.355341
-267.799089	6.353865	0.360346
-271.384312	17.324638	0.365350
-275.194080	17.827118	0.370355
-278.504776	11.983098	0.375360
-282.461176	17.088491	0.380365
-286.106529	17.601014	0.385370
-289.863985	5.947836	0.390374
-294.240230	15.051626	0.395379
-297.606430	5.409712	0.400384
-301.605996	12.781808	0.405389
-304.959621	7.753662	0.410394
-308.676577	10.622589	0.415398
-312.649052	14.372832	0.420403
-316.296339	4.304306	0.425408
-320.201831	12.741632	0.430413
-323.882075	9.853548	0.435418
-327.893674	18.200594	0.440422
-331.421246	11.954453	0.445427
-334.909246	9.876217	0.450432
-338.826552	16.126639	0.455437
-342.733458	9.255097	0.460442
-346.513669	7.450610	0.465446
-350.577320	21.883607	0.470451
-354.009076	15.321003	0.475456
-357.768056	7.670508	0.480461
-361.331797	10.686943	0.485466
-365.203775	7.260253	0.490470
-369.153650	21.161024	0.495475
-372.789539	14.637348	0.500480
-376.979157	16.960522	0.505485
-380.413254	19.904248	0.510490
-383.795620	11.020405	0.515494
-387.891942	15.189514	0.520499
-391.817916	12.350232	0.525504
-395.666620	13.139818	0.530509
-398.842630	9.491673	0.535514
-402.960585	10.250144	0.540518
-407.151288	16.895988	0.545523
-410.162776	-0.728186	0.550528
-414.379768	19.042162	0.555533
-418.044719	16.632755	0.560538
-421.577814	7.646882	0.565542
-425.414234	13.272663	0.570547
-428.901065	10.724445	0.575552
-433.250326	8.033248	0.580557
-437.025781	10.326661	0.585562
-440.466145	5.459220	0.590566
-444.617246	16.607326	0.595571
-447.619334	2.023657	0.600576
-451.897110	12.435061	0.605581
-455.691781	2.853925	0.610586
-459.443098	2.738657	0.615590
-463.154039	12.905019	0.620595
-466.346154	10.308215	0.625600
-470.335680	20.028647	0.630605
-474.442050	15.220304	0.635610
-478.276297	12.508444	0.640614
-482.435719	13.484986	0.645619
-485.583613	1.132398	0.650624
-489.217641	10.176335	0.655629
-493.108498	6.634600	0.660634
-496.935241	5.667265	0.665638
-500.917482	14.355247	0.670643
-504.427686	12.156228	0.675648
-508.426280	10.328531	0.680653
-512.100108	10.588901	0.685658
-515.817223	2.867329	0.690662
-519.749432	17.710098	0.695667
-523.067241	6.136908	0.700672
-527.010907	12.864920	0.705677
-530.960848	12.079744	0.710682
-534.431943	9.584363	0.715686
-538.346419	15.601256	0.720691
-541.790469	12.965948	0.725696
-545.941939	13.539206	0.730701
-549.699180	7.874140	0.735706
-553.317882	13.577306	0.740710
-557.001236	10.521351	0.745715
-560.770985	13.233516	0.750720
-564.983870	15.647464	0.755725
-568.443603	16.953937	0.760730
-572.109049	13.201283	0.765734
-576.249918	21.274484	0.770739
-579.640751	20.575117	0.775744
-583.528253	24.608695	0.780749
-587.449382	15.905840	0.785754
-590.755973	16.952915	0.790758
-594.755867	17.397965	0.795763
-598.182469	6.536129	0.800768
-602.419901	19.723095	0.805773
-606.180777	10.969444	0.810778
-610.121046	11.422341	0.815782
-613.913016	18.194068	0.820787
-617.446835	24.435706	0.825792
-620.715258	14.228298	0.830797
-624.675792	20.266880	0.835802
-628.231005	12.710433	0.840806
-632.457773	16.121776	0.845811
-636.042856	2.583998	0.850816
-640.126691	16.916583	0.855821
-644.071866	23.898917	0.860826
-647.294004	13.313569	0.865830
-651.128915	15.585276	0.870835
-654.780522	11.560884	0.875840
-658.764683	16.911012	0.880845
-662.564710	17.160238	0.885850
-666.164197	15.655394	0.890854
-669.811446	16.711277	0.895859
-673.646424	9.040334	0.900864
-677.818625	12.996547	0.905869
-681.693866	7.781061	0.910874
-685.131046	10.273122	0.915878
-688.861472	8.082761	0.920883
-692.423805	9.057301	0.925888
-696.462120	13.531471	0.930893
-700.188377	11.651121	0.935898
-703.800601	15.068467	0.940902
-707.769367	14.081590	0.945907
-711.389611	4.203357	0.950912
-714.987287	11.813089	0.955917
-718.579766	17.834007	0.960922
-722.336709	11.879016	0.965926
-726.746562	12.694153	0.970931
-730.193702	9.994964	0.975936
-734.088386	16.972523	0.980941
-738.056167	13.440336	0.985946
-741.594866	11.310883	0.990950
-745.362380	18.700222	0.995955
-748.922068	5.743621	1.000960
-752.557738	12.389654	1.005965
-756.288189	11.937206	1.010970
-760.028650	17.002546	1.015974
-764.296350	18.993519	1.020979
-767.634905	7.805640	1.025984
-771.690848	10.636413	1.030989
-775.325652	10.802644	1.035994
-779.061203	10.483512	1.040998
-783.024991	20.149859	1.046003
-786.397479	13.283550	1.051008
-790.892416	23.687663	1.056013
-794.319098	10.962186	1.061018
-797.715496	13.793243	1.066022
-801.956342	19.886375	1.071027
-805.269864	6.568821	1.076032
-808.988788	10.561619	1.081037
-812.909461	22.485626	1.086042
-816.527835	20.346943	1.091046
-820.683300	27.948222	1.096051
-823.994829	4.982583	1.101056
-827.843153	17.071663	1.106061
-831.816813	13.305612	1.111066
-835.475219	7.656758	1.116070
-839.340719	19.319671	1.121075
-843.138995	16.326695	1.126080
-846.859182	18.974615	1.131085
-850.723653	23.463832	1.136090
-854.089080	15.924713	1.141094
-858.366877	19.518074	1.146099
-861.672103	14.203884	1.151104
-865.638853	21.147441	1.156109
-869.556531	21.322768	1.161114
-873.039662	9.055874	1.166118
-876.869289	23.203118	1.171123
-880.354089	3.961650	1.176128
-884.541993	17.253123	1.181133
-888.352627	15.389718	1.186138
-891.980496	17.355898	1.191142
-895.858880	22.913429	1.196147
-899.269141	1.775623	1.201152
-903.281721	13.749149	1.206157
-907.116791	12.996701	1.211162
-911.028582	12.281756	1.216166
-914.846366	17.536315	1.221171
-918.075236	11.418372	1.226176
-921.778812	14.211985	1.231181
-925.635691	20.389020	1.236186
-929.300059	6.974791	1.241190
-933.486254	13.950388	1.246195
-937.263895	14.503983	1.251200
-940.598123	5.979149	1.256205
-944.515731	10.716705	1.261210
-948.203767	10.708788	1.266214
-952.253648	21.491457	1.271219
-956.037222	6.150380	1.276224
-959.633010	7.698372	1.281229
-963.467135	4.378594	1.286234
-966.949257	4.225817	1.291238
-970.938400	13.257847	1.296243
-974.426964	9.703056	1.301248
-978.326501	16.779547	1.306253
-982.126225	7.480815	1.311258
-986.048343	-1.074513	1.316262
-990.056724	11.067209	1.321267
-993.117422	8.871163	1.326272
-997.218075	9.348777	1.331277
-1001.012965	13.160054	1.336282
-1004.892381	13.003061	1.341286
-1008.899753	17.158991	1.346291
-1012.319011	8.080162	1.351296
-1016.165709	6.604357	1.356301
-1019.950175	17.500803	1.361306
-1023.592590	10.394173	1.366310
-1027.519780	18.785609	1.371315
-1031.027095	16.593231	1.376320
-1034.982438	19.029895	1.381325
-1038.873442	18.403304	1.386330
-1042.013844	10.232397	1.391334
-1046.062434	16.181663	1.396339
-1049.925226	12.475530	1.401344
-1053.974387	11.101556	1.406349
-1057.573761	18.559094	1.411354
-1061.227799	13.551724	1.416358
-1065.045273	14.064587	1.421363
-1068.657344	4.524682	1.426368
-1072.174370	10.185540	1.431373
-1076.270085	15.568385	1.436378
-1080.169336	10.981891	1.441382
-1084.172031	17.724969	1.446387
-1087.351425	11.594626	1.451392
-1091.116419	14.510290	1.456397
-1094.890519	19.158904	1.461402
-1098.668811	11.976361	1.466406
-1103.125487	24.893301	1.471411
-1106.617723	22.558277	1.476416
-1110.067530	19.683463	1.481421
-1113.347751	9.516534	1.486426
-1117.295960	6.212110	1.491430
-1121.553776	13.557452	1.496435
-1125.028905	6.854736	1.501440
-1129.164800	16.973360	1.506445
-1132.930059	16.038229	1.511450
-1136.431782	2.405954	1.516454
-1140.199080	8.553224	1.521459
-1143.852770	2.923043	1.526464
-1147.653825	16.528371	1.531469
-1151.396591	20.243241	1.536474
-1155.111323	14.660686	1.541478
-1159.276494	15.587297	1.546483
-1162.653430	5.934233	1.551488
-1166.427728	7.963684	1.556493
-1169.931500	9.833164	1.561498
-1173.645912	7.029169	1.566502
-1178.437747	17.046243	1.571507
-1181.895649	4.925629	1.576512
-1185.308115	2.339848	1.581517
-1189.044305	13.653019	1.586522
-1192.912135	3.340538	1.591526
-1196.442898	15.426670	1.596531
-1200.233926	12.537206	1.601536
-1203.990777	17.925973	1.606541
-1207.855598	14.742402	1.611546
-1211.932069	3.654366	1.616550
-1215.643012	9.669734	1.621555
-1219.392411	13.008880	1.626560
-1222.952680	7.362301	1.631565
-1226.688044	12.981051	1.636570
-1230.518237	8.475230	1.641574
-1234.162621	9.774376	1.646579
-1237.706256	11.322332	1.651584
-1241.935119	10.198216	1.656589
-1245.650540	18.212338	1.661594
-1249.088749	4.680471	1.666598
-1253.206744	15.748911	1.671603
-1256.378996	3.956442	1.676608
-1260.206143	7.186669	1.681613
-1264.400021	12.828393	1.686618
-1268.260990	6.588193	1.691622
-1272.368459	9.976841	1.696627
-1275.555979	7.385156	1.701632
-1279.102035	9.460261	1.706637
-1283.122940	14.142361	1.711642
-1286.669664	7.777784	1.716646
-1290.788855	13.948492	1.721651
-1294.086435	17.593912	1.726656
-1297.993687	12.007716	1.731661
-1301.914583	6.515175	1.736666
-1305.668143	5.354529	1.741670
-1309.892283	7.828366	1.746675
-1313.743559	6.093596	1.751680
-1316.907648	8.653244	1.756685
-1320.697525	10.680705	1.761690
-1323.900619	6.661295	1.766694
-1328.119074	16.093303	1.771699
-1331.953263	2.740071	1.776704
-1335.748192	3.334925	1.781709
-1339.846802	11.257557	1.786714
-1343.269378	7.213382	1.791718
-1347.168031	7.988859	1.796723
-1350.682678	7.012393	1.801728
-1354.379137	15.521956	1.806733
-1358.446350	14.629221	1.811738
-1362.056237	10.722289	1.816742
-1366.084015	10.264799	1.821747
-1369.449133	5.683191	1.826752
-1373.196893	7.308182	1.831757
-1377.185227	9.875279	1.836762
-1380.976147	5.227812	1.841766
-1384.723614	15.469183	1.846771
-1388.491339	10.195122	1.851776
-1392.184092	3.775247	1.856781
-1396.026410	10.565702	1.861786
-1399.560213	7.718971	1.866790
-1403.517312	14.251850	1.871795
-1407.687693	8.547125	1.876800
-1411.000212	8.926099	1.881805
-1414.762788	10.458913	1.886810
-1418.555117	3.555134	1.891814
-1422.283619	7.488916	1.896819
-1425.703574	7.733726	1.901824
-1429.300780	7.044986	1.906829
-1433.994943	6.880385	1.911834
-1437.053830	-1.448072	1.916838
-1440.932788	4.364308	1.921843
-1444.976419	7.336185	1.926848
-1448.899216	0.645736	1.931853
-1452.526822	5.544266	1.936858
-1455.978058	9.291782	1.941862
-1459.927721	8.452945	1.946867
-1463.895111	6.607713	1.951872
-1467.428767	6.416632	1.956877
-1471.148787	14.321445	1.961882
-1474.760196	12.722002	1.966886
-1478.755412	11.057867	1.971891
-1482.135199	10.080508	1.976896
-1486.058425	3.353923	1.981901
-1490.075270	8.176069	1.986906
-1493.364336	3.123582	1.991910
-1497.679484	6.649957	1.996915
-1501.773066	8.363359	2.006912
-1502.367418	9.802307	2.016909
-1499.606943	13.386678	2.026906
-1496.955722	11.661141	2.036902
-1494.923881	5.860024	2.046899
-1492.972143	11.583922	2.056896
-1491.187906	11.063021	2.066893
-1489.457674	9.374445	2.076890
-1487.216977	7.229917	2.086886
-1485.285080	7.785910	2.096883
-1483.604042	3.826779	2.106880
-1481.593947	12.981894	2.116877
-1479.695930	13.713845	2.126874
-1477.752093	9.786846	2.136870
-1475.942770	6.997714	2.146867
-1473.630283	12.458600	2.156864
-1472.086955	9.776799	2.166861
-1470.434246	8.705392	2.176858
-1468.542599	4.688864	2.186854
-1466.318455	6.203874	2.196851
-1464.304200	4.589840	2.206848
-1462.617865	7.683084	2.216845
-1460.886919	6.728631	2.226842
-1458.975108	7.794708	2.236838
-1456.952873	1.595685	2.246835
-1455.006441	4.039390	2.256832
-1453.364902	6.795600	2.266829
-1451.447210	8.894960	2.276826
-1449.563925	5.764003	2.286822
-1447.473088	7.003532	2.296819
-1445.744387	1.214678	2.306816
-1443.966018	2.046341	2.316813
-1442.177337	4.392156	2.326810
-1439.805582	4.055123	2.336806
-1438.006676	3.214544	2.346803
-1436.254725	12.477350	2.356800
-1434.385760	5.732880	2.366797
-1432.633045	2.921264	2.376794
-1430.503891	10.053666	2.386790
-1428.818126	11.031222	2.396787
-1426.829387	3.782841	2.406784
-1425.155359	5.513863	2.416781
-1423.136690	3.093889	2.426778
-1421.302243	7.404513	2.436774
-1419.339994	9.927823	2.446771
-1417.134410	9.112151	2.456768
-1415.779649	7.291109	2.466765
-1413.817946	11.993477	2.476762
-1411.831707	12.555043	2.486758
-1409.993980	9.701411	2.496755
-1407.934321	9.078059	2.506752
-1406.388590	7.636978	2.516749
-1404.480301	6.737860	2.526746
-1402.415201	15.112136	2.536742
-1400.384269	0.770648	2.546739
-1398.646039	4.733534	2.556736
-1396.687792	6.523288	2.566733
-1394.743292	8.413140	2.576730
-1393.077802	16.391922	2.586726
-1391.458642	11.506435	2.596723
-1389.286473	9.508760	2.606720
-1387.189046	12.051512	2.616717
-1385.594740	4.608935	2.626714
-1383.499938	11.222669	2.636710
-1381.913914	13.954664	2.646707
-1380.111777	11.910443	2.656704
-1378.024339	12.708472	2.666701
-1376.066998	7.798859	2.676698
-1374.335846	2.214926	2.686694
-1372.344228	10.233094	2.696691
-1370.388096	3.619982	2.706688
-1368.680387	9.229898	2.716685
-1366.579674	12.200041	2.726682
-1364.920712	9.856643	2.736678
-1363.114542	5.733879	2.746675
-1360.958812	9.824176	2.756672
-1359.108310	9.510666	2.766669
-1357.657978	12.949668	2.776666
-1355.834717	14.868435	2.786662
-1353.615872	6.639057	2.796659
-1351.594601	11.783528	2.806656
-1349.667734	7.211975	2.816653
-1348.066660	8.564730	2.826650
-1346.013489	13.184622	2.836646
-1344.127439	11.908583	2.846643
-1342.104524	6.233758	2.856640
-1340.548191	7.061569	2.866637
-1338.791201	8.296215	2.876634
-1336.472612	8.318328	2.886630
-1334.955356	10.998204	2.896627
-1333.127537	2.839330	2.906624
-1331.079039	5.126278	2.916621
-1329.153154	7.406011	2.926618
-1327.595974	9.635814	2.936614
-1325.426063	9.048572	2.946611
-1323.080131	7.138410	2.956608
-1321.751829	5.357973	2.966605
-1319.962671	8.378026	2.976602
-1317.961035	11.073544	2.986598
-1315.888350	6.429731	2.996595
-1314.197565	8.227628	3.006592
-1312.562630	4.197046	3.016589
-1310.177076	12.311699	3.026586
-1308.636343	9.243572	3.036582
-1306.932853	13.949469	3.046579
-1304.664507	6.602745	3.056576
-1302.958696	6.648757	3.066573
-1301.131070	8.039496	3.076570
-1299.118084	11.107428	3.086566
-1297.231135	7.077573	3.096563
-1295.394268	6.819981	3.106560
-1293.640074	12.016725	3.116557
-1291.746327	14.931641	3.126554
-1289.600433	16.195663	3.136550
-1287.732358	7.956164	3.146547
-1285.773354	9.973264	3.156544
-1284.157152	16.532641	3.166541
-1282.632675	15.335044	3.176538
-1280.717096	13.550641	3.186534
-1278.480213	8.106889	3.196531
-1276.428880	12.326084	3.206528
-1274.332373	8.085866	3.216525
-1273.046643	12.869699	3.226522
-1271.176638	9.411002	3.236518
-1269.172386	12.977733	3.246515
-1267.168582	6.262332	3.256512
-1265.424543	7.863847	3.266509
-1263.371346	13.249610	3.276506
-1261.564689	13.022143	3.286502
-1260.025888	12.550171	3.296499
-1257.987432	12.266663	3.306496
-1255.986034	5.793238	3.316493
-1253.961268	14.117272	3.326490
-1252.302043	12.378653	3.336486
-1250.261551	11.644822	3.346483
-1248.534229	15.682208	3.356480
-1246.633824	15.645015	3.366477
-1244.726666	15.207266	3.376474
-1242.876582	14.423384	3.386470
-1240.913528	10.127180	3.396467
-1238.865946	7.491153	3.406464
-1237.285114	14.713074	3.416461
-1235.684703	11.877024	3.426458
-1233.745730	13.646320	3.436454
-1231.350559	9.434136	3.446451
-1229.644031	12.331694	3.456448
-1227.862006	13.442419	3.466445
-1225.842105	13.910337	3.476442
-1224.383382	17.955987	3.486438
-1222.254167	7.056825	3.496435
-1219.933476	12.009822	3.506432
-1218.460939	6.241584	3.516429
-1216.677465	10.288957	3.526426
-1214.762175	11.668897	3.536422
-1212.687334	5.079543	3.546419
-1210.817179	11.301493	3.556416
-1209.420082	7.410088	3.566413
-1207.504738	11.321104	3.576410
-1205.355636	7.429374	3.586406
-1203.276777	13.340041	3.596403
-1201.455081	5.079604	3.606400
-1199.625704	9.697546	3.616397
-1197.717431	13.530754	3.626394
-1196.061263	8.964739	3.636390
-1193.997667	7.633570	3.646387
-1192.239708	6.798152	3.656384
-1190.398493	7.143111	3.666381
-1188.377663	15.669947	3.676378
-1186.280314	13.569164	3.686374
-1184.598279	16.548047	3.696371
-1182.991565	17.402643	3.706368
-1180.962201	15.625377	3.716365
-1179.236244	17.035640	3.726362
-1177.116626	13.246548	3.736358
-1175.254423	11.500770	3.746355
-1173.132319	19.959314	3.756352
-1171.657293	10.011182	3.766349
-1169.550524	18.535341	3.776346
-1167.820563	16.561250	3.786342
-1166.043357	17.713847	3.796339
-1163.941098	16.074935	3.806336
-1162.158128	14.697111	3.816333
-1160.320659	22.598044	3.826330
-1158.644785	15.842030	3.836326
-1156.800552	18.469718	3.846323
-1154.513095	15.593277	3.856320
-1152.649700	11.314666	3.866317
-1150.879873	14.172158	3.876314
-1148.983647	18.998927	3.886310
-1147.255169	17.244564	3.896307
-1145.094300	11.751512	3.906304
-1143.496532	10.995443	3.916301
-1141.550947	13.441136	3.926298
-1139.651133	16.713637	3.936294
-1137.906340	13.695077	3.946291
-1135.684875	13.360293	3.956288
-1133.981561	12.047340	3.966285
-1132.487808	14.813221	3.976282
-1130.090959	10.935608	3.986278
-1128.413215	17.862634	3.996275
-1126.507098	9.432423	4.006272
-1124.537609	-0.681621	4.016269
-1122.655893	14.475498	4.026266
-1121.042568	13.840115	4.036262
-1119.078476	13.254411	4.046259
-1117.053649	10.091595	4.056256
-1115.300686	11.079159	4.066253
-1113.353341	6.610306	4.076250
-1111.567632	11.947421	4.086246
-1109.265213	10.893915	4.096243
-1107.635532	12.676479	4.106240
-1106.085744	9.392292	4.116237
-1104.182550	14.465881	4.126234
-1101.839420	13.170603	4.136230
-1100.179820	18.756854	4.146227
-1098.400180	12.745344	4.156224
-1096.407684	17.417810	4.166221
-1094.792189	13.995222	4.176218
-1092.759899	14.803911	4.186214
-1090.684955	12.277317	4.196211
-1088.816038	10.838432	4.206208
-1087.079558	14.113419	4.216205
-1085.166718	11.124860	4.226202
-1083.325439	5.133504	4.236198
-1081.631314	12.672161	4.246195
-1079.522404	9.180134	4.256192
-1077.525113	13.157103	4.266189
-1075.964373	9.754339	4.276186
-1074.159752	8.054167	4.286182
-1071.891202	10.332996	4.296179
-1070.267856	12.632922	4.306176
-1068.312447	14.131306	4.316173
-1066.264665	12.930674	4.326170
-1064.392264	6.749614	4.336166
-1062.750421	8.122892	4.346163
-1060.732000	3.759555	4.356160
-1058.993448	5.696847	4.366157
-1057.122620	9.411426	4.376154
-1055.490577	7.394656	4.386150
-1053.569658	17.382357	4.396147
-1051.369908	17.857979	4.406144
-1049.484908	19.872911	4.416141
-1047.535330	12.307395	4.426138
-1045.985760	14.126500	4.436134
-1043.923969	15.521048	4.446131
-1041.989773	16.683369	4.456128
-1040.079360	14.713667	4.466125
-1038.185700	11.210312	4.476122
-1036.581573	8.965911	4.486118
-1034.887691	11.682481	4.496115
-1032.583559	12.570905	4.506112
-1030.742026	15.912820	4.516109
-1029.159078	12.809695	4.526106
-1027.108847	17.422463	4.536102
-1025.054256	19.154499	4.546099
-1023.184268	18.763928	4.556096
-1021.473830	16.272005	4.566093
-1019.539784	13.272211	4.576090
-1017.768084	20.981678	4.586086
-1015.692597	18.243480	4.596083
-1013.959623	17.300083	4.606080
-1012.068845	15.069856	4.616077
-1010.151996	12.600195	4.626074
-1008.430921	24.896775	4.636070
-1006.286180	13.058968	4.646067
-1004.628435	15.977133	4.656064
-1002.824980	17.561454	4.666061
-1000.689319	17.171046	4.676058
-998.975880	19.166087	4.686054
-997.037723	17.803042	4.696051
-995.286879	17.133121	4.706048
-993.115660	18.218106	4.716045
-991.383566	19.068575	4.726042
-989.640395	20.334122	4.736038
-987.624974	16.124481	4.746035
-985.658796	10.567963	4.756032
-983.763633	13.355017	4.766029
-981.836997	13.858589	4.776026
-980.243141	13.527999	4.786022
-978.467933	10.615218	4.796019
-976.463894	17.785452	4.806016
-974.310046	7.665716	4.816013
-972.588064	13.186824	4.826010
-971.140317	12.495914	4.836006
-968.850578	13.625127	4.846003
-966.626753	11.696947	4.856000
-965.256817	10.072682	4.865997
-963.395800	9.876226	4.875994
-961.494204	11.997524	4.885990
-959.529782	10.930315	4.895987
-957.464229	9.949570	4.905984
-955.654733	14.416158	4.915981
-953.866779	14.776137	4.925978
-952.241579	16.526371	4.935974
-950.414030	15.823692	4.945971
-947.812634	6.374530	4.955968
-946.302670	11.163760	4.965965
-944.727714	16.836297	4.975962
-942.779304	18.343802	4.985958
-940.596009	17.189505	4.995955
-938.691153	11.200718	5.005952
-937.056025	8.010361	5.015949
-935.046224	8.653834	5.025946
-933.089913	8.222689	5.035942
-931.427113	8.588486	5.045939
-929.511272	7.011168	5.055936
-927.669799	4.094145	5.065933
-925.871861	14.442684	5.075930
-923.716838	8.724966	5.085926
-922.088622	10.162103	5.095923
-920.283114	9.158230	5.105920
-918.110263	9.685647	5.115917
-915.966100	8.352891	5.125914
-914.473137	11.256414	5.135910
-912.785873	14.169927	5.145907
-910.888988	12.292492	5.155904
-908.757011	14.885429	5.165901
-906.654095	14.950348	5.175898
-905.215166	12.794025	5.185894
-903.191581	11.704772	5.195891
-901.338140	10.849568	5.205888
-899.684259	14.308435	5.215885
-897.462938	9.391731	5.225882
-895.698426	15.821903	5.235878
-893.840160	7.819517	5.245875
-892.003564	10.609696	5.255872
-890.274387	9.349624	5.265869
-888.043353	8.363009	5.275866
-886.312773	6.284810	5.285862
-884.452875	13.190801	5.295859
-882.672079	13.619874	5.305856
-880.439588	14.305163	5.315853
-879.025697	11.265478	5.325850
-876.797434	12.317767	5.335846
-874.925084	11.606404	5.345843
-873.257413	2.044483	5.355840
-871.520688	10.587039	5.365837
-869.427314	2.714458	5.375834
-867.534081	7.335100	5.385830
-865.728517	9.853941	5.395827
-863.629964	11.455933	5.405824
-861.711821	11.591483	5.415821
-860.372334	9.929512	5.425818
-858.295241	12.272319	5.435814
-856.188745	9.384036	5.445811
-854.528625	11.629290	5.455808
-852.498072	12.226885	5.465805
-850.477806	12.505595	5.475802
-849.035902	11.695692	5.485798
-846.760892	8.969956	5.495795
-845.060929	9.937777	5.505792
-843.225162	11.351266	5.515789
-841.410852	8.497071	5.525786
-839.588023	3.819386	5.535782
-837.291853	6.103506	5.545779
-835.541331	14.111775	5.555776
-833.765298	4.366763	5.565773
-831.944659	5.624781	5.575770
-830.011494	5.805325	5.585766
-828.117818	4.490582	5.595763
-826.222576	4.527189	5.605760
-824.357431	7.248120	5.615757
-822.617001	11.173216	5.625754
-820.941421	12.740225	5.635750
-818.903194	13.556099	5.645747
-816.687764	8.613566	5.655744
-814.984496	8.852975	5.665741
-813.211981	7.319186	5.675738
-811.368005	5.571867	5.685734
-809.347261	11.007454	5.695731
-807.379871	7.716705	5.705728
-805.558770	7.608861	5.715725
-803.830406	6.873200	5.725722
-801.973593	3.064860	5.735718
-799.917428	6.615818	5.745715
-798.155009	10.869002	5.755712
-796.087105	10.230658	5.765709
-794.455833	21.747552	5.775706
-792.692295	19.507833	5.785702
-790.810054	16.699659	5.795699
-788.753851	11.867864	5.805696
-786.788625	12.329113	5.815693
-784.818194	17.226442	5.825690
-783.090800	14.695660	5.835686
-781.268521	18.230334	5.845683
-779.247001	12.151965	5.855680
-777.445062	12.205102	5.865677
-775.929827	18.165207	5.875674
-773.618118	14.577870	5.885670
-771.725495	16.103910	5.895667
-769.933182	12.482745	5.905664
-768.204782	11.183411	5.915661
-766.499951	10.017321	5.925658
-764.176163	15.396623	5.935654
-762.632455	14.063652	5.945651
-760.700242	8.653265	5.955648
-758.598127	7.433161	5.965645
-756.723915	11.398508	5.975642
-755.092525	14.891078	5.985638
-753.094116	13.742816	5.995635
-751.245409	12.260054	6.005632
-749.370484	10.392572	6.015629
-747.498127	3.859640	6.025626
-745.701583	15.211208	6.035622
-743.632990	12.336974	6.045619
-742.070769	16.483249	6.055616
-740.251639	13.378880	6.065613
-738.097286	25.628559	6.075610
-736.051998	14.031070	6.085606
-734.218391	13.684437	6.095603
-732.505457	10.742311	6.105600
-730.629923	16.959084	6.115597
-728.605615	9.075545	6.125594
-726.792108	13.546416	6.135590
-724.902575	13.418224	6.145587
-722.795980	16.113287	6.155584
-721.488046	11.607968	6.165581
-719.452860	9.566475	6.175578
-717.373471	13.077482	6.185574
-715.517540	12.474660	6.195571
-713.951934	15.690399	6.205568
-711.832342	13.701741	6.215565
-709.555725	12.180632	6.225562
-708.301656	12.093998	6.235558
-706.094449	7.721307	6.245555
-704.257918	9.725319	6.255552
-702.507994	12.763189	6.265549
-700.539636	12.909794	6.275546
-698.812014	19.098126	6.285542
-696.484998	11.592562	6.295539
-695.144973	14.151190	6.305536
-693.335516	15.636899	6.315533
-690.869482	12.664464	6.325530
-689.243315	13.036286	6.335526
-687.610742	16.020287	6.345523
-685.887725	12.244463	6.355520
-683.634105	13.076565	6.365517
-681.779094	8.450693	6.375514
-679.970128	19.561912	6.385510
-677.991003	21.113682	6.395507
-675.793855	11.868330	6.405504
-674.388982	18.490363	6.415501
-672.803220	15.263855	6.425498
-670.694213	11.893743	6.435494
-668.512222	6.135618	6.445491
-666.542542	8.743659	6.455488
-664.879641	11.677039	6.465485
-663.006615	17.027416	6.475482
-661.276981	24.609693	6.485478
-659.507299	15.791079	6.495475
-657.199210	9.753863	6.505472
-655.371007	13.129794	6.515469
-653.815936	13.738794	6.525466
-651.598222	10.818706	6.535462
-650.100983	20.459207	6.545459
-648.016616	9.501343	6.555456
-646.271127	14.256309	6.565453
-644.086595	11.411005	6.575450
-642.278609	17.427065	6.585446
-640.716010	16.699058	6.595443
-638.606334	13.099915	6.605440
-636.455948	11.788519	6.615437
-634.997672	14.350397	6.625434
-633.361605	11.840627	6.635430
-631.309870	12.621348	6.645427
-629.331484	12.722199	6.655424
-627.258451	10.832634	6.665421
-625.389083	11.478283	6.675418
-623.693698	13.931233	6.685414
-621.670921	14.561849	6.695411
-619.858372	11.676519	6.705408
-618.039978	15.954064	6.715405
-616.114441	12.835945	6.725402
-614.225749	13.950629	6.735398
-612.371067	15.001273	6.745395
-610.502870	9.138587	6.755392
-608.584805	15.050245	6.765389
-607.030097	17.051989	6.775386
-605.219325	15.936984	6.785382
-602.845299	18.412590	6.795379
-601.027022	20.766977	6.805376
-599.207254	15.982579	6.815373
-597.415404	9.273137	6.825370
-595.393743	15.897743	6.835366
-593.714335	18.556956	6.845363
-591.612744	13.598068	6.855360
-590.012565	20.788968	6.865357
-587.778363	8.049815	6.875354
-586.012637	9.187323	6.885350
-584.149139	4.863330	6.895347
-582.200755	10.921747	6.905344
-581.030533	10.606991	6.915341
-578.604458	12.359031	6.925338
-576.711635	17.872111	6.935334
-574.435771	13.679622	6.945331
-573.107648	14.034397	6.955328
-571.332932	21.527437	6.965325
-568.940334	9.093002	6.975322
-567.720520	11.296691	6.985318
-565.732408	7.957033	6.995315
-563.403222	9.353506	7.005312
-561.442336	6.776109	7.015309
-559.832745	2.724802	7.025306
-558.249865	8.426353	7.035302
-555.957503	10.469779	7.045299
-554.106958	7.970014	7.055296
-552.620054	7.906272	7.065293
-550.401271	10.881999	7.075290
-548.314949	4.278717	7.085286
-546.718996	5.143366	7.095283
-545.179058	7.265933	7.105280
-542.882180	5.274369	7.115277
-541.312460	7.853242	7.125274
-539.178376	7.829824	7.135270
-537.066581	9.644737	7.145267
-535.276354	11.597858	7.155264
-533.659389	5.470614	7.165261
-531.719723	6.193531	7.175258
-529.656544	14.191590	7.185254
-528.116217	16.028314	7.195251
-526.457539	8.343856	7.205248
-524.535724	11.670204	7.215245
-522.167397	11.462542	7.225242
-520.388889	14.255983	7.235238
-518.450122	9.256846	7.245235
-516.603936	3.088266	7.255232
-514.914133	9.980688	7.265229
-513.179803	17.110744	7.275226
-511.053617	18.672326	7.285222
-509.242927	6.154038	7.295219
-506.989236	5.336268	7.305216
-505.284087	10.081998	7.315213
-503.575990	7.935027	7.325210
-501.710264	11.849836	7.335206
-500.073181	9.087356	7.345203
-497.880239	13.186756	7.355200
-495.755947	11.840178	7.365197
-494.387544	7.745324	7.375194
-492.442222	15.544344	7.385190
-490.360855	11.687737	7.395187
-488.169877	10.393676	7.405184
-486.615144	13.290777	7.415181
-485.060891	16.942707	7.425178
-482.808710	9.195071	7.435174
-480.907932	13.366410	7.445171
-479.225436	3.721827	7.455168
-477.091428	9.032258	7.465165
-475.288984	8.482376	7.475162
-473.927790	4.554477	7.485158
-471.784232	10.294448	7.495155
-469.859750	3.407595	7.505152
-467.577212	7.904827	7.515149
-466.081718	11.078249	7.525146
-464.141304	12.178478	7.535142
-462.249280	9.098989	7.545139
-460.323215	8.639904	7.555136
-458.493177	7.247190	7.565133
-456.802856	14.488531	7.575130
-454.661638	10.657134	7.585126
-452.872061	14.064661	7.595123
-450.939321	8.624423	7.605120
-448.906365	10.177264	7.615117
-447.104674	8.888561	7.625114
-445.473281	9.621302	7.635110
-443.672833	5.364323	7.645107
-441.775816	9.935776	7.655104
-439.622139	10.986180	7.665101
-438.079434	7.124053	7.675098
-435.984809	10.332879	7.685094
-434.068281	5.207881	7.695091
-432.284399	5.357323	7.705088
-430.476805	7.781444	7.715085
-428.395999	11.180381	7.725082
-426.761966	5.800492	7.735078
-424.522364	7.538255	7.745075
-422.810409	9.748702	7.755072
-420.852500	8.700343	7.765069
-419.381711	9.480852	7.775066
-417.562348	6.653004	7.785062
-415.414400	5.901153	7.795059
-413.248125	3.291078	7.805056
-411.571851	10.534696	7.815053
-409.912621	10.388263	7.825050
-407.779892	9.488845	7.835046
-405.937535	10.235298	7.845043
-404.271876	9.075717	7.855040
-402.079988	8.571077	7.865037
-400.278936	16.607957	7.875034
-398.307315	10.067317	7.885030
-396.867554	8.981706	7.895027
-394.643278	3.922866	7.905024
-392.609752	4.695649	7.915021
-391.024959	8.090129	7.925018
-389.423379	9.478208	7.935014
-387.384504	7.194819	7.945011
-385.349200	7.904165	7.955008
-383.518013	8.808738	7.965005
-381.555978	9.780843	7.975002
-379.291063	10.044579	7.984998
-378.083726	10.418747	7.994995
-375.972221	11.665420	8.004992
-374.153983	12.677859	8.014989
-372.327639	13.764796	8.024986
-370.237460	14.206442	8.034982
-368.350274	8.178264	8.044979
-366.506705	6.690299	8.054976
-364.734302	12.064886	8.064973
-362.958477	13.524640	8.074970
-360.884434	18.930024	8.084966
-359.148557	12.013357	8.094963
-357.297130	12.363655	8.104960
-355.040920	7.969238	8.114957
-353.264427	9.844163	8.124954
-351.664217	10.305626	8.134950
-349.876088	11.866059	8.144947
-347.678069	9.598349	8.154944
-345.972592	8.350345	8.164941
-344.107338	13.901182	8.174938
-342.239381	12.931984	8.184934
-340.147223	8.630086	8.194931
-338.532273	7.942866	8.204928
-336.852390	16.084407	8.214925
-334.824747	19.725607	8.224922
-332.782420	14.716391	8.234918
-330.927831	12.066143	8.244915
-329.044388	11.325014	8.254912
-326.848675	6.913437	8.264909
-325.203778	16.541655	8.274906
-323.448615	16.842609	8.284902
-321.758955	15.390299	8.294899
-319.590065	9.909303	8.304896
-317.863920	8.699073	8.314893
-315.869072	13.182382	8.324890
-313.711754	17.987135	8.334886
-312.250332	13.817525	8.344883
-310.244359	8.965714	8.354880
-308.596116	12.604340	8.364877
-306.692242	9.729923	8.374874
-304.715310	4.644328	8.384870
-302.846467	9.335660	8.394867
-300.728504	6.311808	8.404864
-299.033019	13.724557	8.414861
-297.422040	12.417458	8.424858
-295.327107	17.306399	8.434854
-293.446963	18.632710	8.444851
-291.375966	14.283701	8.454848
-289.673593	6.511886	8.464845
-287.754328	15.237373	8.474842
-285.583786	10.559843	8.484838
-284.058276	13.284900	8.494835
-282.509535	9.185056	8.504832
-280.450839	15.104552	8.514829
-278.224740	11.476077	8.524826
-276.439637	12.959679	8.534822
-274.797924	3.711736	8.544819
-272.635583	6.848320	8.554816
-270.610565	7.327296	8.564813
-269.027577	9.509493	8.574810
-267.248303	3.988098	8.584807
-265.366275	7.992079	8.594803
-263.320465	4.255023	8.604800
-261.585842	1.170810	8.614797
-259.679824	0.997722	8.624794
-257.453286	-2.769752	8.634791
-256.222847	4.965151	8.644787
-253.931922	-2.580042	8.654784
-252.298597	7.463767	8.664781
-250.207524	0.788912	8.674778
-248.547810	9.137426	8.684775
-246.308761	2.723172	8.694771
-244.628642	2.420357	8.704768
-242.567485	3.035697	8.714765
-240.972140	7.960209	8.724762
-239.031151	9.497908	8.734759
-237.151393	3.985759	8.744755
-235.140758	4.882333	8.754752
-233.328130	4.994177	8.764749
-231.386348	1.801130	8.774746
-229.623452	-0.337028	8.784743
-227.525781	-7.838721	8.794739
-225.804824	-4.307962	8.804736
-224.129015	-10.019657	8.814733
-221.928766	2.284794	8.824730
-220.114619	-2.098951	8.834727
-218.477865	-0.318468	8.844723
-216.452248	-10.593972	8.854720
-214.676488	-4.795063	8.864717
-212.585786	1.084644	8.874714
-211.047510	3.002431	8.884711
-208.873874	0.463994	8.894707
-207.045204	-2.224656	8.904704
-205.289709	-0.060473	8.914701
-203.246985	-2.655383	8.924698
-201.483550	-2.579876	8.934695
-199.798257	-7.399368	8.944691
-197.823172	-4.813898	8.954688
-195.762026	-6.783307	8.964685
-193.851749	-3.345895	8.974682
-192.214285	1.548244	8.984679
-190.131542	1.522275	8.994675
-188.238403	-4.719881	9.004672
-186.436120	-2.766839	9.014669
-184.622662	-1.674544	9.024666
-182.816300	-2.128517	9.034663
-180.939006	-5.173861	9.044659
-178.942927	-4.371236	9.054656
-177.080364	-5.985249	9.064653
-175.034589	-1.448367	9.074650
-173.378845	-2.929899	9.084647
-171.812383	-1.092376	9.094643
-169.607604	-6.673706	9.104640
-167.590875	-1.127951	9.114637
-165.851987	2.314729	9.124634
-163.607143	-4.608808	9.134631
-162.015713	2.748013	9.144627
-160.325484	-2.626464	9.154624
-158.456318	-1.514617	9.164621
-156.435620	-5.427581	9.174618
-154.409043	2.770883	9.184615
-152.630843	-0.040730	9.194611
-151.049085	-1.270436	9.204608
-148.826099	3.092928	9.214605
-147.093893	4.694018	9.224602
-145.387831	0.289675	9.234599
-143.357691	-1.591058	9.244595
-141.413714	-1.190623	9.254592
-139.709509	-7.606285	9.264589
-137.584758	-8.346294	9.274586
-135.909271	-2.022890	9.284583
-133.851769	-1.957938	9.294579
-132.055929	-8.871385	9.304576
-130.288990	-0.339361	9.314573
-128.084114	-2.562179	9.324570
-126.350824	0.270358	9.334567
-124.787987	9.671818	9.344563
-122.820599	8.326915	9.354560
-120.854274	11.104907	9.364557
-118.778283	-1.684416	9.374554
-117.256859	7.662075	9.384551
-115.237541	8.017352	9.394547
-113.046109	4.326659	9.404544
-111.389700	4.234567	9.414541
-109.706752	8.392021	9.424538
-107.618063	0.073938	9.434535
-105.899380	4.460960	9.444531
-103.679337	3.315768	9.454528
-102.091290	5.776751	9.464525
-100.117481	6.316148	9.474522
-98.356610	8.639032	9.484519
-96.446656	13.445559	9.494515
-94.551769	11.499600	9.504512
-92.511556	12.806848	9.514509
-90.870886	13.495719	9.524506
-89.117770	9.238645	9.534503
-87.041783	7.074321	9.544499
-85.190089	5.354739	9.554496
-83.156648	10.965805	9.564493
-81.508869	8.464001	9.574490
-79.337283	8.523431	9.584487
-77.569363	6.752481	9.594483
-75.702757	-2.550169	9.604480
-74.047529	8.489783	9.614477
-72.099352	6.521129	9.624474
-70.161036	8.425717	9.634471
-68.484761	13.604292	9.644467
-66.501981	9.943766	9.654464
-64.211986	7.500578	9.664461
-62.433750	7.685933	9.674458
-60.898099	10.030564	9.684455
-58.800676	13.086123	9.694451
-57.044691	10.055483	9.704448
-55.321088	6.739477	9.714445
-53.232523	8.533267	9.724442
-51.448360	11.068792	9.734439
-49.567357	7.666101	9.744435
-47.785342	12.295705	9.754432
-45.543083	7.347984	9.764429
-43.791696	14.016209	9.774426
-42.214873	12.334190	9.784423
-40.150786	13.249245	9.794419
-38.123235	14.004335	9.804416
-36.397951	8.509075	9.814413
-34.523781	9.602853	9.824410
-32.800410	12.015455	9.834407
-30.732340	13.288312	9.844403
-28.802803	8.409437	9.854400
-26.929056	7.835882	9.864397
-24.865889	6.796312	9.874394
-23.196568	13.491855	9.884391
-21.353458	14.999556	9.894387
-19.453394	11.758060	9.904384
-17.749443	4.369855	9.914381
-15.877417	9.106707	9.924378
-13.805482	19.739187	9.934375
-12.143551	5.730685	9.944371
-10.012849	11.389462	9.954368
-8.078910	1.526627	9.964365
-6.298679	8.461863	9.974362
-5.035625	20.938152	9.984359
-3.334395	48.826543	9.994355
-2.113191	96.348969	10.004352
-0.637122	148.023144	10.014349
0.000000	199.171110	10.019354
0.656814	238.071621	10.024359
1.378370	281.267107	10.029363
2.001728	303.024892	10.034368
2.472398	334.090077	10.039373
2.615804	358.953919	10.044378
3.080434	368.335566	10.049383
3.460998	391.603555	10.054387
3.449403	394.735803	10.059392
3.635992	398.580789	10.064397
3.682652	408.432844	10.069402
3.972919	404.451947	10.074407
4.005505	413.424702	10.079411
4.196633	419.028912	10.084416
4.023026	420.919091	10.089421
4.114676	431.684960	10.094426
4.297956	435.609334	10.099431
4.254597	447.394997	10.104435
4.150418	451.412536	10.109440
4.379699	438.682625	10.114445
4.312673	454.253744	10.119450
4.572060	445.253396	10.124455
4.399288	453.279605	10.129459
4.306599	455.923310	10.134464
4.480250	457.168302	10.139469
4.613905	456.101462	10.144474
4.817986	448.248537	10.149479
4.734840	463.571493	10.154483
4.766483	460.404570	10.159488
4.693931	462.143012	10.164493
4.631162	461.396095	10.169498
4.587042	464.464157	10.174503
4.591671	468.920103	10.179507
4.743542	464.924993	10.184512
4.850000	475.459865	10.189517
4.580988	477.573434	10.194522
5.161821	493.470210	10.199527
5.292767	505.144536	10.204531
5.485812	511.548026	10.209536
5.472161	507.926250	10.214541
5.015277	501.098124	10.219546
5.210451	504.274690	10.224551
5.223744	504.237913	10.229555
5.548198	510.144183	10.234560
5.517616	509.970896	10.239565
5.073873	519.005497	10.244570
5.389631	514.648328	10.249575
5.555029	524.700729	10.254579
5.451188	519.568355	10.259584
5.558858	527.034188	10.264589
5.347259	521.105257	10.269594
5.756716	519.111290	10.274599
5.440217	529.024505	10.279603
5.819476	525.907782	10.284608
6.021534	522.357257	10.289613
5.530707	529.946939	10.294618
5.805429	544.591553	10.299623
6.104465	556.939309	10.304627
6.109480	557.108866	10.309632
5.961885	568.927024	10.314637
6.035027	576.896730	10.319642
6.114749	568.730823	10.324647
5.943925	575.034675	10.329651
6.009823	575.478387	10.334656
6.247833	572.966107	10.339661
5.960203	581.078519	10.344666
6.374733	577.569788	10.349671
6.217591	579.179804	10.354675
6.369435	573.994012	10.359680
6.567286	585.454295	10.364685
6.256070	591.059845	10.369690
6.724281	593.803355	10.374695
6.586618	621.410773	10.379699
6.688934	620.954501	10.384704
6.793235	616.255695	10.389709
6.791131	617.342644	10.394714
6.891063	614.330384	10.399719
6.463147	620.348816	10.404723
6.806669	615.873642	10.409728
6.837481	618.899822	10.414733
6.807936	622.088601	10.419738
6.905915	615.867391	10.424743
6.918660	627.764106	10.429747
7.131002	622.202776	10.434752
6.988220	629.194496	10.439757
6.787591	636.245911	10.444762
7.111830	638.783724	10.449767
6.924766	658.589621	10.454771
7.289086	659.610243	10.459776
7.775471	658.261613	10.464781
7.351627	663.041439	10.469786
7.681307	667.204314	10.474791
7.811373	669.113901	10.479795
7.615160	671.939746	10.484800
8.021500	662.343361	10.489805
7.605504	672.501212	10.494810
8.002214	667.626434	10.499815
7.453153	673.385075	10.504819
7.614202	669.058844	10.509824
7.738353	677.462040	10.514829
7.404979	674.693931	10.519834
7.511430	669.206247	10.524839
7.616630	676.716708	10.529843
7.840274	687.340281	10.534848
7.996486	694.044632	10.539853
8.013188	704.881008	10.544858
8.378679	707.833323	10.549863
8.322423	716.952907	10.554867
8.340404	711.047208	10.559872
8.540155	706.061899	10.564877
8.232091	700.717593	10.569882
8.323373	702.177605	10.574887
8.301064	717.842805	10.579891
8.477870	710.613868	10.584896
8.335184	711.289560	10.589901
8.012498	729.333551	10.594906
8.376727	713.227504	10.599911
8.399492	719.811219	10.604915
8.682701	722.839743	10.609920
8.789998	722.240739	10.614925
8.706350	722.284083	10.619930
9.031046	711.798619	10.624935
8.955783	723.810380	10.629939
8.860485	723.000825	10.634944
9.032026	724.985810	10.639949
8.591837	727.383775	10.644954
9.027626	717.582372	10.649959
8.804965	725.938405	10.654963
9.022936	730.357249	10.659968
9.537915	744.906971	10.664973
9.130617	744.345886	10.669978
8.939252	733.655696	10.674983
9.360016	752.789152	10.679987
9.227282	765.524516	10.684992
9.789470	764.059700	10.689997
9.733758	763.718520	10.695002
9.367972	744.670981	10.700007
9.451951	748.560813	10.705011
9.510860	753.427683	10.710016
9.958726	756.172893	10.715021
9.549685	763.185067	10.720026
9.958070	767.769106	10.725031
9.765057	759.575626	10.730035
9.583724	753.422563	10.735040
9.853182	764.953573	10.740045
9.715597	762.830771	10.745050
9.712671	768.865062	10.750055
9.934108	772.969534	10.755059
9.739061	769.091179	10.760064
9.829560	777.906680	10.765069
9.892121	776.005858	10.770074
10.121990	774.737558	10.775079
9.915258	776.226186	10.780083
9.497261	770.902542	10.785088
10.167935	786.411551	10.790093
10.123359	795.103518	10.795098
10.399186	806.854332	10.800103
10.344036	809.362795	10.805107
10.080100	806.235056	10.810112
10.797762	788.796719	10.815117
10.756885	804.220531	10.820122
11.062863	804.832551	10.825127
10.632200	802.657135	10.830131
10.568860	808.939213	10.835136
10.899971	803.544964	10.840141
10.859971	811.471340	10.845146
10.955186	799.573103	10.850151
10.680253	805.702837	10.855155
10.800355	810.377028	10.860160
10.831396	804.421896	10.865165
10.797836	813.694049	10.870170
10.748904	812.948061	10.875175
10.777979	818.608238	10.880179
10.770440	819.295497	10.885184
10.906264	812.484657	10.890189
10.451379	826.037905	10.895194
11.254307	827.449083	10.900199
11.160663	845.103424	10.905203
11.348287	842.461932	10.910208
11.529075	831.674461	10.915213
11.234923	843.483098	10.920218
11.209051	841.105908	10.925223
11.284731	851.404673	10.930227
11.462691	847.369025	10.935232
11.486973	847.953433	10.940237
11.229848	854.241206	10.945242
11.432442	847.422855	10.950247
11.287213	858.114850	10.955251
11.275247	860.573854	10.960256
11.820398	871.367070	10.965261
11.684828	883.461127	10.970266
12.297432	873.475289	10.975271
12.220488	885.563151	10.980275
12.047117	880.911703	10.985280
12.527051	879.493114	10.990285
12.059435	883.953542	10.995290
12.324656	855.033748	11.000295
11.939791	864.882394	11.005299
11.916033	850.665891	11.010304
12.592015	865.552779	11.015309
12.457082	866.810753	11.020314
12.327875	859.393993	11.025319
12.237912	861.600491	11.030323
12.105294	879.089190	11.035328
12.568904	885.134279	11.040333
12.281464	890.471204	11.045338
12.689956	881.336412	11.050343
12.540407	889.934783	11.055347
12.413525	891.331834	11.060352
12.693007	886.450449	11.065357
12.515581	892.875347	11.070362
12.459139	891.171700	11.075367
12.686443	892.562725	11.080371
12.341904	896.822163	11.085376
12.748268	893.379321	11.090381
12.662812	901.093785	11.095386
12.947221	910.953994	11.100391
13.184605	925.447243	11.105395
13.142632	931.427900	11.110400
13.440634	921.927478	11.115405
13.169296	912.733929	11.120410
13.077737	898.853068	11.125415
13.051387	899.666342	11.130419
13.221405	916.304092	11.135424
13.134045	920.733845	11.140429
13.519839	925.020318	11.145434
13.640720	914.948867	11.150439
13.719266	923.373673	11.155443
13.475273	923.327466	11.160448
14.049590	920.785144	11.165453
13.686519	921.043379	11.170458
13.742928	906.262062	11.175463
13.360844	895.852923	11.180467
13.679543	908.041714	11.185472
13.519339	920.445680	11.190477
13.426779	929.053910	11.195482
13.718534	925.318659	11.200487
13.578099	918.873553	11.205491
13.735609	921.154138	11.210496
13.743941	920.000013	11.215501
13.183783	921.563951	11.220506
13.976511	938.455668	11.225511
14.160574	946.150824	11.230515
14.329668	953.086647	11.235520
14.329427	951.350372	11.240525
14.257177	956.324968	11.245530
14.480342	952.889254	11.250535
14.637859	958.861760	11.255539
14.444199	957.804510	11.260544
14.405335	950.437952	11.265549
14.554199	953.483222	11.270554
14.594675	949.272342	11.275559
14.634223	963.738831	11.280563
14.549200	952.288718	11.285568
14.876876	950.881792	11.290573
14.585017	959.204836	11.295578
14.748878	949.397762	11.300583
14.828091	948.177132	11.305587
14.803979	951.768846	11.310592
15.068172	949.086735	11.315597
14.933944	951.740309	11.320602
14.978355	955.138155	11.325607
14.882766	953.529059	11.330611
14.863725	949.436489	11.335616
15.138309	945.815943	11.340621
15.040396	956.363258	11.345626
15.180125	955.979862	11.350631
15.245689	954.468074	11.355635
15.059494	953.201460	11.360640
14.984017	953.196189	11.365645
15.074721	967.875313	11.370650
15.460801	950.765658	11.375655
15.337774	951.252132	11.380659
15.236817	952.840609	11.385664
15.292580	960.010570	11.390669
15.347883	970.345788	11.395674
16.059688	972.927509	11.400679
15.890728	977.622625	11.405683
15.665549	970.036598	11.410688
15.608775	961.431737	11.415693
15.647417	969.869243	11.420698
15.912400	979.563852	11.425703
15.890122	990.245796	11.430707
16.036134	985.276849	11.435712
16.070053	984.833052	11.440717
15.818202	994.218989	11.445722
15.985197	992.001839	11.450727
16.240058	986.192298	11.455731
16.093783	984.889350	11.460736
16.367323	976.685993	11.465741
16.403026	992.044170	11.470746
16.202545	993.916628	11.475751
16.028238	993.141738	11.480755
15.932925	993.581211	11.485760
16.206920	992.089796	11.490765
15.715635	999.083657	11.495770
16.116070	994.769616	11.500775
15.997316	998.649270	11.505779
16.419702	1019.061827	11.510784
16.594693	1018.300615	11.515789
16.444310	1021.988186	11.520794
16.662162	1021.672758	11.525799
16.777565	1022.371960	11.530803
16.747788	1025.909398	11.535808
17.095810	1023.291180	11.540813
16.598608	1030.609301	11.545818
16.535620	1024.016167	11.550823
16.970849	1023.738614	11.555827
16.707523	1017.197939	11.560832
17.018084	1021.991643	11.565837
17.154621	1035.081718	11.570842
17.039276	1039.963861	11.575847
17.365798	1045.248652	11.580851
17.253999	1054.626485	11.585856
17.431127	1048.162213	11.590861
17.346553	1055.769376	11.595866
17.275652	1046.360831	11.600871
17.568335	1044.934245	11.605875
17.343819	1054.844183	11.610880
17.474010	1056.578746	11.615885
17.898298	1051.909195	11.620890
18.030874	1037.692808	11.625895
17.612582	1035.244124	11.630899
17.499997	1027.307344	11.635904
17.636734	1024.058876	11.640909
17.497100	1046.002558	11.645914
17.760336	1042.311253	11.650919
18.258571	1042.805882	11.655923
17.758807	1047.829771	11.660928
18.308456	1040.744647	11.665933
18.348208	1046.267581	11.670938
18.603891	1033.050356	11.675943
18.019164	1017.527448	11.680947
17.988742	1023.276048	11.685952
18.133641	1010.126979	11.690957
17.882423	1013.614571	11.695962
18.143096	1007.638502	11.700967
18.127049	1015.048620	11.705971
17.945289	1039.132793	11.710976
18.373184	1037.637329	11.715981
18.200093	1044.884837	11.720986
18.856454	1040.201932	11.725991
18.499634	1040.839246	11.730995
18.388177	1047.231612	11.736000
18.638388	1037.369701	11.741005
18.428910	1049.168153	11.746010
18.547980	1048.013704	11.751015
18.378665	1049.540549	11.756019
18.616877	1043.055498	11.761024
18.797104	1041.768283	11.766029
18.620113	1054.924153	11.771034
18.874434	1048.706210	11.776039
18.917675	1052.645204	11.781043
18.864994	1066.210223	11.786048
19.021819	1073.239531	11.791053
18.947007	1083.325901	11.796058
19.456997	1080.820623	11.801063
19.261866	1089.383801	11.806067
19.318618	1090.123903	11.811072
19.457931	1079.273473	11.816077
19.159702	1067.623865	11.821082
19.271854	1069.550557	11.826087
19.812671	1082.025793	11.831091
19.309607	1078.470893	11.836096
19.352370	1073.262896	11.841101
19.300561	1078.104953	11.846106
19.371360	1082.236694	11.851111
19.341551	1078.420218	11.856115
19.412286	1083.881449	11.861120
19.499276	1080.751299	11.866125
19.210103	1088.692335	11.871130
19.433452	1086.223311	11.876135
19.545639	1088.096379	11.881139
19.227643	1098.994317	11.886144
19.928790	1100.484843	11.891149
19.568445	1105.224719	11.896154
19.853308	1108.251485	11.901159
19.883360	1108.734050	11.906163
19.970775	1107.428514	11.911168
20.330449	1101.972825	11.916173
20.122300	1104.351187	11.921178
20.100225	1108.554524	11.926183
20.186365	1110.415978	11.931187
19.875313	1109.557226	11.936192
20.388370	1118.449053	11.941197
20.532011	1135.586467	11.946202
20.770898	1123.149343	11.951207
20.437386	1119.307172	11.956211
20.318783	1113.082443	11.961216
20.880972	1124.024534	11.966221
20.793962	1134.086074	11.971226
20.894657	1115.127662	11.976231
20.793590	1105.774356	11.981235
20.586870	1094.881326	11.986240
20.511127	1094.040243	11.991245
20.639081	1110.271728	11.996250
20.937828	1126.810334	12.001255
20.939590	1135.610241	12.006259
20.851526	1136.165266	12.011264
21.091917	1130.086718	12.016269
21.147458	1126.493178	12.021274
21.331064	1131.195195	12.026279
21.369746	1128.470165	12.031283
21.388924	1118.285473	12.036288
21.368248	1103.098323	12.041293
20.893679	1099.540450	12.046298
20.746645	1099.380998	12.051303
20.844438	1095.924242	12.056307
21.160313	1106.251116	12.061312
21.158270	1097.375649	12.066317
21.082176	1102.000796	12.071322
21.019735	1105.679092	12.076327
21.429433	1109.561230	12.081331
21.055770	1111.033934	12.086336
21.350492	1107.763404	12.091341
21.262277	1111.013692	12.096346
21.020506	1110.047688	12.101351
21.108724	1105.059530	12.106355
20.958285	1110.057689	12.111360
21.081958	1104.399924	12.116365
21.215667	1108.212530	12.121370
21.135585	1109.009152	12.126375
21.448194	1102.078511	12.131379
21.023013	1111.285570	12.136384
21.214173	1099.606772	12.141389
20.902147	1115.025270	12.146394
21.026414	1115.869732	12.151399
21.071087	1100.367785	12.156403
20.970974	1114.241636	12.161408
21.116237	1103.014894	12.166413
21.014683	1109.203840	12.171418
21.105719	1111.048742	12.176423
21.383865	1102.051307	12.181427
20.966977	1109.796663	12.186432
21.022796	1108.248564	12.191437
21.090824	1115.345677	12.196442
20.922720	1115.033454	12.201447
21.514292	1112.303830	12.206451
20.888509	1103.447411	12.211456
21.204282	1099.124764	12.216461
21.106772	1104.120787	12.221466
20.891518	1096.288662	12.226471
21.143447	1106.039059	12.231475
20.928496	1106.382489	12.236480
21.513153	1111.663985	12.241485
21.166466	1096.937303	12.246490
21.332334	1091.503067	12.251495
21.348100	1095.123152	12.256499
20.956091	1099.718253	12.261504
21.317924	1092.229363	12.266509
21.224158	1098.954848	12.271514
21.356477	1092.535554	12.276519
21.289667	1085.561347	12.281523
21.001545	1090.669776	12.286528
21.424840	1091.222095	12.291533
20.893317	1102.401694	12.296538
20.916473	1092.359900	12.301543
21.421148	1089.281411	12.306547
20.923092	1094.167836	12.311552
21.286955	1095.940835	12.316557
21.000210	1097.729286	12.321562
20.955248	1099.599032	12.326567
21.144140	1086.420798	12.331571
21.017184	1091.617072	12.336576
21.252055	1086.499866	12.341581
21.076932	1073.381279	12.346586
21.040404	1063.705445	12.351591
20.851846	1058.605316	12.356595
21.074842	1081.350723	12.361600
21.323199	1076.772308	12.366605
21.016623	1071.596373	12.371610
20.750692	1057.886685	12.376615
20.848584	1071.552283	12.381619
20.758462	1086.328183	12.386624
21.357833	1090.287305	12.391629
21.130833	1102.717851	12.396634
21.272229	1088.714490	12.401639
21.106272	1074.044169	12.406643
20.910801	1076.950404	12.411648
21.112306	1071.803828	12.416653
21.013465	1066.479636	12.421658
20.779743	1076.760094	12.426663
20.973025	1080.370787	12.431667
21.093624	1095.409579	12.436672
21.263252	1092.914427	12.441677
21.091513	1082.071025	12.446682
21.081435	1081.668938	12.451687
21.169013	1069.013122	12.456691
20.811137	1074.943290	12.461696
21.086185	1075.572874	12.466701
21.093840	1084.081627	12.471706
20.908802	1077.348650	12.476711
21.057600	1075.569664	12.481715
21.586632	1088.639768	12.486720
21.259386	1075.299418	12.491725
20.712025	1077.167283	12.496730
20.747302	1074.666752	12.501735
21.080056	1071.756047	12.506739
20.779692	1078.142282	12.511744
21.081293	1086.654620	12.516749
21.065556	1100.996012	12.521754
21.142151	1102.515184	12.526759
20.980478	1093.691990	12.531763
20.986259	1096.403690	12.536768
21.254035	1098.180975	12.541773
20.564489	1094.643197	12.546778
21.192805	1099.157571	12.551783
21.432975	1103.284383	12.556787
21.151076	1095.262598	12.561792
21.181322	1091.748802	12.566797
20.938857	1075.795896	12.571802
21.124070	1078.062625	12.576807
21.037900	1074.513780	12.581811
21.110537	1083.262923	12.586816
21.084889	1078.075298	12.591821
21.079483	1081.698757	12.596826
21.050268	1083.151217	12.601831
21.211674	1074.606115	12.606835
20.679178	1081.092459	12.611840
21.187737	1073.362539	12.616845
20.954774	1082.491611	12.621850
20.622130	1082.268715	12.626855
20.793492	1083.313838	12.631859
21.017733	1105.406172	12.636864
21.661036	1103.254974	12.641869
21.195147	1096.415382	12.646874
20.984912	1087.145737	12.651879
21.445115	1074.958808	12.656883
20.919667	1084.336397	12.661888
20.980768	1076.020199	12.666893
20.939760	1081.768934	12.671898
20.939636	1084.790682	12.676903
21.182696	1091.940298	12.681907
20.881508	1087.236623	12.686912
21.234277	1074.975358	12.691917
21.156298	1082.455317	12.696922
20.899176	1087.476792	12.701927
21.185585	1084.463080	12.706931
20.959379	1082.120957	12.711936
20.951723	1078.050191	12.716941
20.974226	1081.333280	12.721946
21.058885	1086.672434	12.726951
21.149285	1074.676961	12.731955
21.151834	1087.220705	12.736960
21.191038	1076.302658	12.741965
21.021495	1079.405048	12.746970
21.086170	1085.412917	12.751975
21.204994	1094.504813	12.756979
20.877017	1085.976253	12.761984
21.099975	1084.103430	12.766989
21.366874	1085.977055	12.771994
20.797370	1088.081861	12.776999
21.145402	1078.062384	12.782003
21.036400	1091.835122	12.787008
21.150067	1086.532226	12.792013
21.185222	1095.322051	12.797018
20.868122	1099.922553	12.802023
21.220874	1091.386350	12.807027
21.067606	1090.802080	12.812032
21.110874	1083.597411	12.817037
21.100328	1091.306336	12.822042
20.837279	1101.607260	12.827047
21.146896	1085.637258	12.832051
20.915193	1094.091145	12.837056
20.883912	1082.635511	12.842061
21.095937	1089.925705	12.847066
20.711955	1092.229599	12.852071
21.266798	1089.628849	12.857075
21.171256	1091.643868	12.862080
21.298367	1088.179283	12.867085
21.166932	1090.293074	12.872090
20.920637	1083.844277	12.877095
21.225534	1079.961799	12.882099
20.862466	1092.524434	12.887104
21.204094	1088.505198	12.892109
20.866186	1099.958291	12.897114
20.967994	1102.755611	12.902119
21.235449	1098.850712	12.907123
21.056437	1097.792691	12.912128
21.472004	1094.017148	12.917133
20.982733	1095.462554	12.922138
20.890532	1094.882738	12.927143
21.345282	1092.190711	12.932147
20.989814	1095.704412	12.937152
21.190280	1090.898646	12.942157
21.010670	1099.383654	12.947162
21.144347	1099.542159	12.952167
21.288531	1093.650872	12.957171
21.182533	1101.638400	12.962176
21.451862	1080.090375	12.967181
20.958485	1079.120344	12.972186
20.570576	1066.401586	12.977191
21.239731	1070.726495	12.982195
20.919156	1084.293255	12.987200
20.996058	1080.412445	12.992205
21.215503	1085.096114	12.997210
20.924578	1073.478455	13.002215
21.070065	1075.481839	13.007219
21.203866	1082.855474	13.012224
21.060252	1076.279908	13.017229
20.967802	1072.375644	13.022234
20.716045	1072.969392	13.027239
20.750193	1088.219100	13.032243
20.910304	1093.973611	13.037248
21.108626	1098.584954	13.042253
20.924833	1102.303106	13.047258
21.134308	1094.950488	13.052263
21.193001	1098.920148	13.057267
21.339122	1109.833963	13.062272
21.210102	1099.650842	13.067277
20.924176	1097.731437	13.072282
21.003521	1103.719626	13.077287
21.386044	1099.427337	13.082291
21.132729	1088.809848	13.087296
20.701075	1078.216078	13.092301
20.716052	1089.201261	13.097306
21.072955	1100.284895	13.102311
21.278249	1102.967930	13.107315
21.028529	1100.475000	13.112320
21.145075	1094.512421	13.117325
21.178341	1107.396664	13.122330
21.388171	1100.741057	13.127335
21.551730	1086.467636	13.132339
21.229570	1076.526665	13.137344
20.999245	1068.088204	13.142349
20.773125	1076.719400	13.147354
20.957714	1074.996213	13.152359
21.097356	1068.583646	13.157363
21.064313	1077.068921	13.162368
21.077309	1075.018258	13.167373
21.117692	1078.352115	13.172378
21.197709	1077.153426	13.177383
21.165453	1070.875516	13.182387
21.030134	1070.237918	13.187392
21.025724	1072.351949	13.192397
20.919145	1072.583469	13.197402
21.020932	1076.645606	13.202407
21.151570	1070.305444	13.207411
20.892809	1083.977471	13.212416
21.073327	1078.553520	13.217421
21.148648	1077.066973	13.222426
20.852904	1085.087909	13.227431
21.382264	1066.815035	13.232435
21.023254	1069.528138	13.237440
21.058519	1076.915909	13.242445
21.155526	1078.351391	13.247450
20.628421	1084.071992	13.252455
21.460129	1078.982608	13.257459
20.927175	1083.694809	13.262464
20.859889	1074.973277	13.267469
20.978462	1077.044037	13.272474
20.919678	1078.881289	13.277479
21.132162	1073.139979	13.282483
20.879839	1077.058305	13.287488
21.204041	1080.936724	13.292493
20.946185	1087.070159	13.297498
20.673770	1079.485299	13.302503
21.165496	1071.349600	13.307507
20.862585	1087.763331	13.312512
21.053119	1073.331067	13.317517
20.789346	1085.961444	13.322522
20.803922	1081.516517	13.327527
20.710564	1093.793265	13.332531
20.783578	1114.308992	13.337536
21.391741	1117.282619	13.342541
21.573060	1119.281871	13.347546
21.396629	1105.676144	13.352551
21.216620	1093.791599	13.357555
20.878789	1084.154345	13.362560
21.122045	1086.071168	13.367565
21.078095	1086.407827	13.372570
21.172374	1088.274288	13.377575
21.336716	1076.516200	13.382579
21.291860	1084.393032	13.387584
21.293074	1087.856151	13.392589
21.261006	1087.462303	13.397594
21.027071	1085.727011	13.402599
21.219336	1082.242574	13.407603
21.055502	1090.264553	13.412608
21.115050	1083.068328	13.417613
21.259160	1078.522310	13.422618
20.885706	1088.315665	13.427623
21.080128	1081.563169	13.432627
20.930244	1090.656916	13.437632
20.788895	1083.117387	13.442637
20.962882	1090.054073	13.447642
20.768578	1097.361765	13.452647
20.789108	1087.596383	13.457651
20.881737	1089.496227	13.462656
21.176571	1093.456610	13.467661
20.953979	1095.509241	13.472666
20.970374	1096.943388	13.477671
20.976508	1092.952426	13.482675
20.976269	1094.914395	13.487680
20.562141	1096.013475	13.492685
20.859149	1092.979146	13.497690
20.812766	1098.235117	13.502695
21.233506	1105.126146	13.507699
20.802028	1107.836620	13.512704
21.340427	1106.711488	13.517709
21.315701	1098.894709	13.522714
20.959050	1104.200168	13.527719
21.053271	1096.285564	13.532723
21.313077	1099.035603	13.537728
21.346584	1097.984691	13.542733
21.230633	1095.142393	13.547738
21.084080	1091.786116	13.552743
21.109616	1099.110790	13.557747
21.016061	1096.881560	13.562752
21.401850	1093.807837	13.567757
21.388717	1090.632147	13.572762
21.148220	1092.671863	13.577767
21.007493	1092.825245	13.582771
21.394587	1096.411338	13.587776
21.410803	1100.584909	13.592781
21.406339	1089.208578	13.597786
20.985613	1069.459685	13.602791
21.066768	1065.302212	13.607795
20.943167	1070.351275	13.612800
20.847630	1067.423718	13.617805
21.101748	1057.818235	13.622810
20.601422	1069.847610	13.627815
21.282766	1072.976726	13.632819
21.219819	1082.356247	13.637824
20.825020	1071.439611	13.642829
20.863878	1074.617579	13.647834
20.964932	1093.360897	13.652839
21.224770	1094.828762	13.657843
21.293731	1099.277795	13.662848
21.223017	1082.180913	13.667853
21.096447	1070.753103	13.672858
20.779493	1080.069048	13.677863
21.473881	1072.071350	13.682867
21.168106	1070.615623	13.687872
20.801528	1065.054990	13.692877
21.011437	1068.148900	13.697882
20.816187	1070.720758	13.702887
20.972877	1066.854036	13.707891
20.951246	1079.021553	13.712896
20.997561	1080.771074	13.717901
21.375726	1089.250700	13.722906
21.019772	1077.462045	13.727911
21.017946	1076.894625	13.732915
21.041121	1074.225700	13.737920
20.771283	1066.435415	13.742925
21.050736	1083.831827	13.747930
20.932250	1097.169231	13.752935
20.956906	1105.826684	13.757939
21.108691	1109.391960	13.762944
21.259986	1106.297283	13.767949
21.139165	1099.732264	13.772954
20.765056	1087.075946	13.777959
21.306262	1085.399967	13.782963
20.889934	1091.063474	13.787968
20.887929	1087.065927	13.792973
21.321227	1095.902647	13.797978
21.240377	1089.228747	13.802983
21.379109	1075.558588	13.807987
21.142153	1073.465783	13.812992
20.601364	1081.415404	13.817997
20.924595	1069.491619	13.823002
20.788369	1073.929212	13.828007
21.120990	1078.623215	13.833011
21.169983	1092.353407	13.838016
21.037426	1083.829952	13.843021
20.827230	1076.970090	13.848026
20.954100	1097.311610	13.853031
21.050985	1092.763658	13.858035
21.120927	1105.596314	13.863040
20.888337	1111.692611	13.868045
21.029852	1102.442554	13.873050
21.173648	1109.477113	13.878055
21.252462	1105.165448	13.883059
21.160633	1100.321135	13.888064
21.173909	1085.507088	13.893069
21.201277	1077.718284	13.898074
20.725291	1078.776762	13.903079
20.922880	1075.862381	13.908083
21.145453	1083.209241	13.913088
20.886268	1079.019307	13.918093
21.235828	1081.488501	13.923098
21.020687	1075.952600	13.928103
20.935744	1075.478868	13.933107
20.781331	1087.733808	13.938112
20.844234	1095.192880	13.943117
21.218577	1102.058189	13.948122
21.014559	1110.512401	13.953127
21.362449	1109.345108	13.958131
21.160353	1101.315322	13.963136
21.189541	1093.236036	13.968141
21.342857	1077.210541	13.973146
20.894655	1086.754022	13.978151
21.170674	1080.977342	13.983155
20.965246	1089.100579	13.988160
21.200715	1083.076456	13.993165
20.958209	1077.056023	13.998170
21.089599	1084.379578	14.003175
21.189572	1077.620068	14.008179
21.082037	1079.299502	14.013184
20.949091	1081.235322	14.018189
21.181024	1078.885914	14.023207
20.768027	1076.178521	14.028224
21.220511	1070.246750	14.033242
21.060901	1083.559871	14.038259
20.939953	1078.902496	14.043277
21.137144	1075.836654	14.048295
21.122467	1088.598116	14.053312
21.191049	1079.809545	14.058330
21.024699	1073.798717	14.063347
21.204463	1076.217763	14.068365
21.166044	1081.882222	14.073383
20.988850	1078.765977	14.078400
21.357145	1095.795422	14.083418
21.191960	1110.171273	14.088435
21.273831	1112.011321	14.093453
21.385845	1111.252582	14.098471
21.136234	1118.180873	14.103488
21.350357	1110.380551	14.108506
21.503624	1111.108068	14.113523
21.303107	1122.409510	14.118541
21.317816	1121.411454	14.123559
21.349650	1117.846573	14.128576
21.359403	1123.127403	14.133594
21.202759	1127.022162	14.138611
21.374788	1123.933581	14.143629
21.411274	1117.012615	14.148647
21.131011	1123.621747	14.153664
21.192050	1122.569109	14.158682
21.168098	1119.849995	14.163699
20.865662	1126.829189	14.168717
21.200255	1140.776138	14.173735
21.269570	1155.487448	14.178752
21.892487	1146.061424	14.183770
21.626721	1151.623740	14.188787
21.501372	1156.093977	14.193805
21.543439	1150.562696	14.198823
21.407572	1158.663676	14.203840
21.482823	1150.846155	14.208858
21.443735	1142.755857	14.213875
21.492203	1154.598073	14.218893
21.706903	1154.540273	14.223911
21.682688	1150.987470	14.228928
21.625882	1152.514578	14.233946
21.780715	1163.174195	14.238963
21.922845	1179.546087	14.243981
22.103114	1186.124268	14.248999
21.601905	1174.316559	14.254016
22.010131	1184.993980	14.259034
21.989069	1179.125109	14.264051
21.954854	1175.957723	14.269069
22.097671	1162.983910	14.274087
21.655984	1169.285319	14.279104
22.110841	1185.605766	14.284122
22.196699	1190.021878	14.289139
21.720272	1178.814272	14.294157
22.189452	1180.817504	14.299175
22.148919	1184.761402	14.304192
22.321244	1182.456150	14.309210
22.092592	1158.857301	14.314227
21.953075	1157.721814	14.319245
22.145152	1163.637413	14.324263
21.741308	1172.898021	14.329280
22.272351	1180.848599	14.334298
22.419923	1175.438912	14.339315
22.395657	1184.269314	14.344333
22.493557	1165.516912	14.349351
22.099624	1158.529291	14.354368
22.241591	1152.997806	14.359386
22.038390	1147.444295	14.364403
22.260512	1168.135641	14.369421
22.515946	1172.812573	14.374439
22.411538	1183.702320	14.379456
22.452517	1168.743800	14.384474
22.824051	1157.490630	14.389491
22.448908	1154.028405	14.394509
22.524018	1142.732860	14.399527
21.986877	1150.910421	14.404544
22.041061	1145.477885	14.409562
22.343345	1162.849854	14.414579
22.402684	1179.142140	14.419597
22.867575	1183.955560	14.424615
22.670052	1194.408695	14.429632
22.757519	1181.619878	14.434650
22.538984	1167.302089	14.439667
22.223022	1170.158876	14.444685
22.702296	1177.792085	14.449703
22.644593	1185.599034	14.454720
22.618113	1186.709164	14.459738
22.735143	1186.965825	14.464755
22.721008	1184.138165	14.469773
22.768590	1189.939964	14.474791
22.945953	1192.309074	14.479808
22.718086	1178.593676	14.484826
22.982037	1167.906658	14.489843
22.344516	1166.963860	14.494861
22.622454	1180.614709	14.499879
22.469757	1192.064311	14.504896
22.461461	1191.464760	14.509914
22.744848	1194.400570	14.514931
22.653105	1197.175982	14.519949
22.783020	1191.446624	14.524967
22.749639	1193.166635	14.529984
22.691869	1187.539575	14.535002
22.761805	1179.161299	14.540019
22.868434	1191.485068	14.545037
22.871825	1178.100884	14.550055
23.071012	1189.244244	14.555072
23.050354	1196.299655	14.560090
23.127055	1197.361868	14.565107
23.213647	1201.896633	14.570125
23.222269	1181.817406	14.575143
22.836303	1183.675449	14.580160
22.738173	1187.513700	14.585178
22.933301	1201.114852	14.590195
22.845703	1216.069121	14.595213
23.281475	1204.705779	14.600231
23.373557	1204.614051	14.605248
23.278128	1208.050743	14.610266
23.436272	1198.930055	14.615283
23.383975	1209.622742	14.620301
23.658284	1199.240799	14.625319
23.749243	1189.775318	14.630336
23.510555	1186.300760	14.635354
23.642954	1171.886095	14.640371
23.190702	1180.651046	14.645389
23.187442	1183.497288	14.650407
23.667923	1175.769282	14.655424
23.531168	1182.751965	14.660442
23.498020	1174.275300	14.665459
23.302955	1179.772867	14.670477
23.846863	1178.084771	14.675495
23.393861	1176.908043	14.680512
23.273141	1175.594946	14.685530
23.534858	1175.677515	14.690547
23.314261	1180.480711	14.695565
23.605670	1176.185412	14.700583
23.765165	1182.246218	14.705600
23.486795	1179.827228	14.710618
23.519560	1184.698558	14.715635
23.532799	1182.234630	14.720653
23.914496	1187.583579	14.725671
23.848072	1182.761740	14.730688
23.582778	1183.911533	14.735706
24.070622	1177.335413	14.740723
23.724700	1177.587257	14.745741
23.834671	1181.156355	14.750759
23.789238	1178.986512	14.755776
23.611157	1182.132778	14.760794
23.810079	1185.063180	14.765811
23.833350	1195.706051	14.770829
23.866960	1200.526913	14.775847
24.175656	1204.497703	14.780864
23.685469	1201.822260	14.785882
23.728602	1206.982175	14.790899
23.897192	1215.261937	14.795917
23.825621	1208.392769	14.800935
23.867078	1201.324674	14.805952
23.644381	1206.847894	14.810970
24.055052	1206.446583	14.815987
23.920780	1210.897023	14.821005
23.741745	1210.565383	14.826023
23.908200	1215.926649	14.831040
23.658996	1214.847193	14.836058
23.857844	1206.816440	14.841075
23.927335	1233.570464	14.846093
24.113926	1242.880094	14.851111
24.310060	1241.422857	14.856128
23.874469	1239.706928	14.861146
24.339193	1236.167360	14.866163
24.225017	1244.625950	14.871181
24.411307	1239.625355	14.876199
24.349043	1234.653393	14.881216
24.309078	1250.040561	14.886234
24.698144	1240.536153	14.891251
24.493230	1243.725252	14.896269
24.511203	1242.703857	14.901287
24.374365	1236.275322	14.906304
24.449926	1243.988687	14.911322
24.480619	1242.154342	14.916339
24.352424	1241.087831	14.921357
24.772824	1229.640403	14.926375
24.997259	1230.837937	14.931392
24.179912	1229.146716	14.936410
24.811376	1226.479569	14.941427
24.962183	1233.400682	14.946445
24.511567	1223.681772	14.951463
24.785264	1206.847171	14.956480
24.437722	1209.550909	14.961498
24.621218	1221.089277	14.966515
24.546358	1231.509504	14.971533
24.838518	1238.386838	14.976551
24.902002	1236.095005	14.981568
24.749769	1230.839296	14.986586
24.939870	1229.909216	14.991603
24.582343	1234.204142	14.996621
24.661115	1230.899171	15.001639
24.942900	1228.884777	15.006656
24.449977	1235.271465	15.011674
24.794906	1232.340908	15.016691
24.660949	1226.468786	15.021709
24.515466	1236.831066	15.026727
24.747431	1236.462976	15.031744
24.624209	1237.706520	15.036762
24.735730	1236.468065	15.041779
24.872192	1245.434111	15.046797
24.865290	1258.721463	15.051815
25.305726	1255.067783	15.056832
25.134824	1270.714177	15.061850
25.340224	1260.142614	15.066867
25.314741	1248.664823	15.071885
25.014706	1233.533315	15.076903
25.112079	1238.963812	15.081920
25.231338	1261.689168	15.086938
25.572338	1253.639650	15.091955
25.189367	1242.336075	15.096973
25.243793	1237.768658	15.101991
25.223265	1231.090333	15.107008
25.113129	1238.350377	15.112026
25.171914	1250.560700	15.117043
25.224414	1262.449554	15.122061
25.504213	1256.062315	15.127079
25.644302	1244.766552	15.132096
25.410078	1261.596551	15.137114
25.920090	1264.515108	15.142131
25.618902	1241.282422	15.147149
25.504829	1237.278299	15.152167
25.519173	1234.372939	15.157184
25.596680	1234.215893	15.162202
25.407335	1231.042563	15.167219
25.563306	1228.909018	15.172237
25.316036	1228.587474	15.177255
25.442998	1226.104615	15.182272
25.351504	1246.960141	15.187290
25.402552	1254.896078	15.192307
25.844499	1264.953895	15.197325
25.341441	1254.697470	15.202343
25.486371	1255.755884	15.207360
25.430590	1258.188933	15.212378
25.530490	1258.560802	15.217395
25.769189	1266.451873	15.222413
25.550211	1265.104100	15.227431
25.960211	1259.573872	15.232448
25.697459	1261.789026	15.237466
25.781569	1259.010964	15.242483
26.012992	1261.929121	15.247501
25.903252	1264.896185	15.252519
26.281806	1254.095655	15.257536
25.836796	1274.026003	15.262554
25.796873	1267.198165	15.267571
26.120193	1269.939639	15.272589
26.134546	1263.328097	15.277607
26.056851	1255.892001	15.282624
26.390833	1268.323511	15.287642
26.090715	1263.157446	15.292659
26.310541	1257.805419	15.297677
26.186478	1268.935900	15.302695
26.677297	1262.788718	15.307712
26.248439	1260.704398	15.312730
26.331703	1259.210104	15.317747
26.281679	1255.380597	15.322765
26.361814	1263.547862	15.327783
26.418967	1258.541901	15.332800
26.376026	1267.362749	15.337818
26.261467	1260.402881	15.342835
26.518262	1266.721134	15.347853
26.195658	1263.629614	15.352871
26.135174	1268.264151	15.357888
26.160259	1265.082570	15.362906
26.358116	1258.558170	15.367923
26.460742	1260.953370	15.372941
26.659981	1270.795848	15.377959
26.831713	1269.396772	15.382976
26.636489	1275.128788	15.387994
26.412366	1271.728966	15.393011
26.406752	1264.605425	15.398029
26.274320	1268.725243	15.403047
26.200299	1263.105464	15.408064
26.730267	1277.634886	15.413082
26.386657	1275.603037	15.418099
26.655334	1282.378741	15.423117
26.495394	1303.565386	15.428135
26.824617	1298.596246	15.433152
26.526215	1303.135815	15.438170
26.550016	1304.360636	15.443187
26.880307	1294.082173	15.448205
26.603166	1302.096435	15.453223
26.971300	1300.934242	15.458240
26.681152	1294.198999	15.463258
27.073076	1293.911578	15.468275
27.108650	1298.218548	15.473293
26.734181	1298.638548	15.478311
27.063705	1293.214741	15.483328
26.969623	1301.991854	15.488346
26.764656	1296.641494	15.493363
27.401629	1293.029609	15.498381
27.277273	1300.910960	15.503399
27.414172	1294.452111	15.508416
27.042889	1297.426288	15.513434
26.936674	1296.282332	15.518451
27.073054	1291.838686	15.523469
26.891586	1300.109832	15.528487
27.147780	1297.494660	15.533504
27.210776	1304.558018	15.538522
27.109228	1297.571675	15.543539
27.066759	1288.449106	15.548557
27.270205	1296.839764	15.553575
27.094183	1295.628288	15.558592
27.275130	1304.881441	15.563610
27.437707	1302.588738	15.568627
27.592634	1305.733830	15.573645
27.194345	1306.554045	15.578663
27.332111	1313.548065	15.583680
27.758912	1318.259063	15.588698
27.216828	1324.048779	15.593715
27.614527	1324.858450	15.598733
27.729754	1329.084296	15.603751
27.704286	1331.120824	15.608768
27.752281	1325.223575	15.613786
27.455895	1313.169144	15.618803
27.676495	1316.491747	15.623821
27.434204	1325.849384	15.628839
27.847945	1322.044211	15.633856
27.995414	1326.644028	15.638874
27.823713	1323.806076	15.643891
27.840345	1298.974693	15.648909
27.570820	1302.830084	15.653927
27.874166	1313.691076	15.658944
27.939241	1316.373070	15.663962
27.857585	1322.320594	15.668979
28.013590	1312.756567	15.673997
27.540450	1322.380691	15.679015
27.764349	1318.243987	15.684032
27.980390	1319.860522	15.689050
27.814659	1337.511846	15.694067
28.138842	1324.185694	15.699085
27.844137	1323.119778	15.704103
28.087697	1324.882940	15.709120
28.007350	1320.231596	15.714138
27.968905	1317.317335	15.719155
27.940490	1309.051416	15.724173
28.098544	1319.765692	15.729191
28.204069	1319.001686	15.734208
28.090155	1315.982266	15.739226
27.752105	1322.750933	15.744243
28.365777	1318.762071	15.749261
28.244230	1308.849042	15.754279
28.404337	1315.222064	15.759296
28.376254	1313.836762	15.764314
28.320386	1312.707585	15.769331
28.341887	1310.033885	15.774349
28.152611	1309.211500	15.779367
28.404165	1311.169234	15.784384
28.457962	1307.558331	15.789402
28.276212	1315.022538	15.794419
28.337159	1325.190716	15.799437
28.389131	1334.189168	15.804455
28.633746	1342.970491	15.809472
28.825406	1343.380426	15.814490
28.752971	1341.508246	15.819507
28.844716	1343.162698	15.824525
28.777382	1332.332548	15.829543
28.578488	1322.699271	15.834560
28.648538	1322.766791	15.839578
28.512889	1337.912113	15.844595
28.560824	1341.951273	15.849613
28.618027	1341.794318	15.854631
28.697774	1340.707219	15.859648
28.711844	1346.831403	15.864666
28.630647	1343.466973	15.869683
29.123876	1339.835528	15.874701
28.890649	1341.609453	15.879719
28.956078	1340.064510	15.884736
28.894625	1346.166131	15.889754
28.865793	1349.607965	15.894771
28.844096	1347.161380	15.899789
28.847436	1349.851652	15.904807
28.985678	1343.822021	15.909824
29.067921	1342.644858	15.914842
28.974929	1342.383651	15.919859
29.399414	1333.383215	15.924877
29.209428	1345.940833	15.929895
28.885642	1345.860373	15.934912
29.394319	1338.513979	15.939930
29.128762	1343.738121	15.944947
29.345110	1338.738991	15.949965
29.126113	1339.872759	15.954983
29.335050	1339.950377	15.960000
29.140143	1339.041582	15.965018
29.276072	1352.514674	15.970035
29.452903	1355.702689	15.975053
29.531556	1366.119765	15.980071
29.406453	1366.514152	15.985088
29.799923	1372.510979	15.990106
29.342483	1363.261057	15.995123
29.620103	1361.417990	16.000141
29.720513	1354.868190	16.005159
29.484971	1344.149019	16.010176
29.728025	1344.221982	16.015194
29.407327	1354.229243	16.020211
29.820752	1352.141926	16.025229
29.972434	1350.362993	16.030247
29.698546	1346.055553	16.035264
29.835920	1342.571317	16.040282
29.346146	1342.930266	16.045299
30.038775	1347.310215	16.050317
30.100573	1350.036784	16.055335
29.910050	1340.023832	16.060352
30.273614	1328.569661	16.065370
30.002257	1336.425712	16.070387
30.146223	1330.338541	16.075405
29.989556	1336.714116	16.080423
29.766162	1334.663085	16.085440
30.247000	1328.891863	16.090458
29.944052	1332.924059	16.095475
29.998170	1331.288896	16.100493
29.811580	1333.775854	16.105511
29.654713	1337.994761	16.110528
30.106257	1338.456059	16.115546
30.046238	1358.383323	16.120563
29.989937	1364.063328	16.125581
30.294160	1363.757646	16.130599
29.904968	1369.242198	16.135616
30.259207	1359.611129	16.140634
30.417033	1364.521564	16.145651
30.291519	1368.000059	16.150669
30.458728	1364.847700	16.155687
30.307755	1368.748697	16.160704
30.215412	1360.120123	16.165722
30.138787	1368.286492	16.170739
30.243242	1366.685770	16.175757
30.487566	1362.374330	16.180775
30.643748	1371.007746	16.185792
30.612492	1357.198683	16.190810
30.663088	1362.130939	16.195827
30.541026	1359.148991	16.200845
30.502914	1360.650329	16.205863
30.379440	1362.269106	16.210880
30.432593	1358.403453	16.215898
30.107106	1371.972177	16.220915
30.259239	1390.430990	16.225933
30.635769	1391.330562	16.230951
30.572607	1396.328952	16.235968
30.735635	1392.128001	16.240986
30.768852	1401.239603	16.246003
30.857499	1402.668030	16.251021
31.191281	1404.345238	16.256039
30.894845	1402.200449	16.261056
30.852909	1394.727904	16.266074
30.705872	1397.587680	16.271091
30.989493	1397.734402	16.276109
31.217818	1393.052681	16.281127
30.795118	1403.767618	16.286144
31.266844	1389.654925	16.291162
30.989345	1399.429588	16.296179
30.953766	1404.478640	16.301197
31.613058	1402.770545	16.306215
31.040780	1403.826950	16.311232
31.367502	1395.279388	16.316250
31.312983	1394.565286	16.321267
31.031299	1400.835767	16.326285
31.272888	1399.440482	16.331303
31.047624	1395.297526	16.336320
31.096863	1396.132103	16.341338
31.733689	1412.465473	16.346355
31.465955	1413.595221	16.351373
31.850741	1398.299260	16.356391
31.531128	1398.039588	16.361408
31.691784	1398.665265	16.366426
31.293856	1402.612737	16.371443
31.381463	1389.619212	16.376461
31.554734	1395.743982	16.381479
31.514002	1402.446389	16.386496
31.535225	1403.886356	16.391514
31.635907	1414.155229	16.396531
31.732785	1424.036160	16.401549
31.837755	1435.193163	16.406567
31.719331	1439.002468	16.411584
32.176666	1422.085632	16.416602
32.069332	1423.860724	16.421619
31.621043	1408.117148	16.426637
31.900378	1397.530548	16.431655
31.713451	1405.447891	16.436672
31.815037	1418.040082	16.441690
31.873445	1419.750199	16.446707
31.953205	1432.183854	16.451725
32.084937	1426.176464	16.456743
31.945586	1424.773503	16.461760
31.883644	1418.075740	16.466778
32.118693	1429.054682	16.471795
32.014694	1427.006619	16.476813
32.091781	1425.030352	16.481831
31.887430	1427.348692	16.486848
32.026055	1426.896379	16.491866
32.120818	1430.135254	16.496883
31.874674	1429.320359	16.501901
32.215639	1426.271628	16.506919
32.073692	1431.262145	16.511936
32.217411	1446.474713	16.516954
32.392098	1451.686097	16.521971
32.512200	1449.762744	16.526989
32.472260	1457.726676	16.532007
32.541061	1457.228080	16.537024
32.448894	1454.482816	16.542042
32.505023	1455.955762	16.547059
32.379821	1456.496465	16.552077
32.896737	1453.918339	16.557095
32.698521	1459.247404	16.562112
32.947477	1456.540546	16.567130
32.814780	1431.516452	16.572147
32.388790	1427.517190	16.577165
33.043553	1432.682675	16.582183
32.700756	1434.316776	16.587200
32.508429	1430.723860	16.592218
32.924732	1445.213374	16.597235
32.599056	1447.982883	16.602253
32.817556	1448.346854	16.607271
32.912653	1460.925959	16.612288
33.017219	1451.774331	16.617306
33.070538	1455.044205	16.622323
32.941771	1448.679572	16.627341
32.896367	1452.614880	16.632359
32.965688	1453.789979	16.637376
33.055111	1454.045543	16.642394
33.514190	1451.722045	16.647411
33.257574	1454.463236	16.652429
33.273759	1445.076372	16.657447
33.095690	1459.260343	16.662464
33.098365	1455.576543	16.667482
33.172210	1446.205651	16.672499
32.912088	1455.489133	16.677517
33.337708	1448.479204	16.682535
33.157006	1453.115669	16.687552
33.013050	1452.535384	16.692570
33.303615	1455.703709	16.697587
33.354665	1453.796875	16.702605
33.258216	1446.461205	16.707623
33.339908	1475.659897	16.712640
33.539143	1474.448334	16.717658
33.570226	1480.641436	16.722675
33.468526	1486.185577	16.727693
34.053650	1478.723884	16.732711
33.924639	1485.034548	16.737728
33.662165	1475.727502	16.742746
33.623371	1469.645826	16.747763
33.463064	1480.301666	16.752781
33.780145	1483.910170	16.757799
33.616302	1482.691229	16.762816
33.699126	1474.485343	16.767834
33.775210	1471.569302	16.772851
33.621376	1492.107130	16.777869
33.837979	1480.579534	16.782887
33.532188	1485.214723	16.787904
33.587016	1475.121646	16.792922
33.748615	1482.936252	16.797939
34.052765	1501.215224	16.802957
34.298404	1505.999224	16.807975
34.007624	1492.811900	16.812992
34.100863	1494.671421	16.818010
34.141347	1503.850359	16.823027
34.046962	1511.847386	16.828045
34.267650	1508.900410	16.833063
34.042898	1505.203315	16.838080
33.965027	1517.716457	16.843098
34.054896	1516.066919	16.848115
33.877215	1513.662487	16.853133
34.297688	1508.302752	16.858151
34.212279	1507.622673	16.863168
34.312973	1514.185379	16.868186
34.608780	1513.108642	16.873203
34.191118	1512.482340	16.878221
34.415886	1523.045334	16.883239
34.703468	1534.430492	16.888256
34.419317	1538.274119	16.893274
34.920019	1529.505240	16.898291
34.605739	1547.000388	16.903309
34.958642	1539.412097	16.908327
34.806349	1545.306481	16.913344
34.590894	1538.596965	16.918362
34.886482	1521.854470	16.923379
35.002909	1534.117189	16.928397
35.299539	1533.026948	16.933415
35.182084	1521.826318	16.938432
35.091611	1507.895989	16.943450
35.017056	1504.307868	16.948467
34.921725	1502.661912	16.953485
34.817394	1490.038701	16.958503
34.687237	1500.545021	16.963520
34.924276	1510.977055	16.968538
35.479181	1514.851246	16.973555
34.836851	1513.720414	16.978573
35.027671	1524.030047	16.983591
35.104126	1530.397628	16.988608
35.083711	1526.006448	16.993626
35.511778	1525.146155	16.998643
35.161304	1527.326572	17.003661
35.294367	1529.152217	17.008679
35.585882	1527.196796	17.013696
35.423795	1534.392124	17.018714
35.509647	1521.600120	17.023731
35.300990	1526.742888	17.028749
35.603657	1520.197724	17.033767
35.429736	1518.248106	17.038784
35.306945	1522.516689	17.043802
35.561377	1526.288574	17.048819
35.022339	1526.184237	17.053837
35.542076	1524.269500	17.058855
35.647877	1519.403564	17.063872
35.618995	1529.071804	17.068890
35.672839	1521.701901	17.073907
35.480261	1535.711286	17.078925
35.923362	1551.456693	17.083943
36.111304	1556.283735	17.088960
36.005700	1538.202779	17.093978
35.943857	1530.122974	17.098995
35.820853	1529.791041	17.104013
35.695639	1534.037203	17.109031
36.062325	1542.491636	17.114048
36.217814	1560.799899	17.119066
36.432595	1547.115806	17.124083
36.132626	1530.613798	17.129101
35.926831	1531.419055	17.134119
36.299985	1536.229135	17.139136
35.655825	1555.092811	17.144154
35.959584	1550.587783	17.149171
36.220792	1549.017886	17.154189
35.977341	1550.264900	17.159207
36.583056	1557.158450	17.164224
36.171722	1561.702737	17.169242
36.461458	1557.524005	17.174259
36.468466	1558.350382	17.179277
36.479816	1555.059237	17.184295
36.557635	1551.977726	17.189312
36.282783	1545.416900	17.194330
36.507850	1549.379101	17.199347
36.582392	1551.262062	17.204365
36.372392	1554.745423	17.209383
36.463451	1541.448389	17.214400
36.689198	1557.917491	17.219418
36.729376	1549.100919	17.224435
36.482991	1559.713913	17.229453
36.650596	1571.973221	17.234471
36.874536	1572.718594	17.239488
36.919312	1575.396794	17.244506
37.355476	1575.814148	17.249523
37.136597	1582.902933	17.254541
37.363663	1570.299162	17.259559
37.157068	1545.238677	17.264576
37.017781	1554.805773	17.269594
37.204672	1546.460547	17.274611
37.246454	1540.135530	17.279629
36.791193	1544.774126	17.284647
37.009546	1547.833646	17.289664
37.140442	1567.714230	17.294682
37.336215	1563.140686	17.299699
37.606354	1580.042417	17.304717
37.753410	1561.900685	17.309735
37.517661	1540.396943	17.314752
37.156123	1547.024733	17.319770
37.180228	1536.716278	17.324787
37.483937	1539.675662	17.329805
37.518861	1554.818388	17.334823
37.467733	1546.502470	17.339840
37.537648	1544.320468	17.344858
37.841177	1552.476650	17.349875
37.426196	1541.619988	17.354893
37.648383	1542.562278	17.359911
37.576401	1552.305052	17.364928
37.437898	1569.299474	17.369946
37.653418	1569.268286	17.374963
38.049010	1573.317347	17.379981
37.873825	1575.737243	17.384999
37.690902	1572.652480	17.390016
37.682957	1570.290185	17.395034
37.823797	1568.951067	17.400051
37.942016	1567.426783	17.405069
37.845807	1575.723028	17.410087
38.008807	1560.500812	17.415104
37.839558	1573.619278	17.420122
37.853959	1566.936800	17.425139
37.968352	1561.363152	17.430157
37.739437	1579.963207	17.435175
38.276044	1573.427116	17.440192
38.382828	1569.537122	17.445210
38.441195	1566.390281	17.450227
38.327726	1567.608701	17.455245
38.310069	1565.190537	17.460263
38.700020	1561.790242	17.465280
38.204474	1574.537582	17.470298
38.530483	1564.636373	17.475315
38.208234	1563.423812	17.480333
38.111081	1578.072432	17.485351
38.474855	1589.718417	17.490368
38.604868	1594.939337	17.495386
38.867449	1593.757776	17.500403
38.943276	1597.389055	17.505421
38.511808	1596.738208	17.510439
39.018924	1591.813748	17.515456
38.825363	1601.151991	17.520474
38.649124	1594.090895	17.525491
39.164624	1599.848121	17.530509
38.717162	1595.123097	17.535527
38.810858	1602.446773	17.540544
38.693608	1598.315634	17.545562
38.904996	1600.855575	17.550579
39.149897	1599.387381	17.555597
39.278896	1588.915073	17.560615
39.274696	1588.262153	17.565632
39.318062	1591.846695	17.570650
39.333996	1582.841262	17.575667
39.430130	1593.857430	17.580685
39.124797	1574.394839	17.585703
39.455249	1563.917950	17.590720
39.277186	1567.005303	17.595738
39.724941	1568.334000	17.600755
39.415061	1555.760031	17.605773
39.080997	1555.214780	17.610791
39.676528	1546.791009	17.615808
39.284351	1545.681628	17.620826
39.225103	1564.435512	17.625843
39.729364	1571.224906	17.630861
39.561761	1585.538686	17.635879
39.792186	1575.236626	17.640896
39.785595	1579.437140	17.645914
39.453384	1565.006519	17.650931
39.837637	1570.244301	17.655949
39.779414	1584.982680	17.660967
39.872500	1582.156719	17.665984
39.877121	1581.677008	17.671002
39.693745	1585.428279	17.676019
39.536267	1580.708923	17.681037
39.328622	1585.540074	17.686055
39.570695	1583.435221	17.691072
39.603414	1578.535300	17.696090
39.926202	1582.134267	17.701107
40.083716	1582.611794	17.706125
39.709611	1597.194487	17.711143
40.143195	1597.842715	17.716160
40.382771	1608.138340	17.721178
40.005609	1603.967636	17.726195
40.197610	1603.883567	17.731213
40.011744	1606.484507	17.736231
40.582760	1601.980100	17.741248
39.990865	1608.086200	17.746266
40.357678	1615.135863	17.751283
40.595769	1609.219194	17.756301
40.212536	1614.245895	17.761319
40.581341	1614.585899	17.766336
40.505952	1607.334097	17.771354
40.246456	1610.724686	17.776371
40.369590	1602.987380	17.781389
40.193960	1620.846704	17.786407
40.614429	1626.600219	17.791424
40.363898	1637.330341	17.796442
40.274061	1640.892878	17.801459
40.711911	1633.849449	17.806477
40.599081	1645.171918	17.811495
40.621547	1644.731833	17.816512
40.753943	1648.806375	17.821530
40.812603	1662.450176	17.826547
41.298519	1668.736784	17.831565
41.213717	1660.976765	17.836583
41.466315	1655.237099	17.841600
41.491312	1649.729588	17.846618
41.245618	1632.207291	17.851635
41.568037	1622.832824	17.856653
40.946159	1633.744871	17.861671
41.106763	1629.542666	17.866688
41.000174	1633.870049	17.871706
41.504533	1654.060086	17.876723
41.873219	1652.123805	17.881741
41.475820	1639.223927	17.886759
41.457581	1631.534323	17.891776
41.588410	1630.599515	17.896794
41.396508	1627.573590	17.901811
41.627178	1620.597031	17.906829
41.685105	1632.889615	17.911847
41.478815	1628.277921	17.916864
41.710997	1642.395855	17.921882
41.461644	1652.569703	17.926899
42.123734	1649.161381	17.931917
41.940052	1653.371282	17.936935
42.109587	1646.717512	17.941952
41.818526	1632.697924	17.946970
41.783898	1637.532960	17.951987
42.089689	1633.660764	17.957005
41.758675	1651.868970	17.962023
41.936312	1645.246944	17.967040
41.822078	1653.771064	17.972058
41.968989	1658.010831	17.977075
42.229385	1646.611408	17.982093
42.134667	1650.183378	17.987111
42.134718	1650.472863	17.992128
42.169845	1648.080875	17.997146
42.222076	1654.234498	18.002163
42.376811	1644.158405	18.007181
42.182905	1657.704049	18.012199
42.192612	1644.596084	18.017216
42.066379	1644.223762	18.022234
42.181546	1667.021196	18.027251
42.594027	1670.117426	18.032269
42.627743	1676.016805	18.037287
42.312951	1668.413019	18.042304
42.805479	1675.766726	18.047322
43.118495	1679.414470	18.052339
43.253919	1665.366946	18.057357
43.160110	1674.944959	18.062375
42.889017	1655.283305	18.067392
42.966166	1640.913956	18.072410
42.674584	1647.374895	18.077427
42.733540	1648.262209	18.082445
42.796629	1665.042110	18.087463
42.911587	1670.926170	18.092480
43.009925	1679.838786	18.097498
42.773658	1676.335405	18.102515
43.150071	1667.620089	18.107533
42.728010	1674.849082	18.112551
42.953853	1667.804840	18.117568
43.304678	1664.629426	18.122586
42.953277	1676.797766	18.127603
43.124366	1678.867493	18.132621
43.420132	1693.883028	18.137639
43.585571	1697.129569	18.142656
43.704859	1693.991862	18.147674
43.680708	1700.182069	18.152691
43.786243	1677.266873	18.157709
43.489032	1671.330938	18.162727
43.430340	1659.700806	18.167744
43.861428	1669.072399	18.172762
43.475240	1684.715030	18.177779
44.027974	1685.779229	18.182797
44.254975	1683.137971	18.187815
44.002084	1664.202545	18.192832
44.161084	1656.282514	18.197850
43.772041	1657.788725	18.202867
44.107563	1653.186573	18.207885
43.936505	1660.419575	18.212903
44.042293	1656.813665	18.217920
44.078907	1652.167944	18.222938
43.679367	1654.810049	18.227955
43.705674	1657.165574	18.232973
44.128135	1666.070537	18.237991
44.146878	1681.118441	18.243008
44.372031	1675.123580	18.248026
44.521578	1680.295795	18.253043
44.939227	1669.418722	18.258061
44.491276	1656.787242	18.263079
44.215696	1657.459694	18.268096
44.426817	1655.493482	18.273114
44.462856	1668.951337	18.278131
44.637714	1666.543354	18.283149
44.854110	1675.048578	18.288167
44.607884	1676.783713	18.293184
44.849591	1672.785652	18.298202
44.580100	1686.385065	18.303219
44.832192	1675.266960	18.308237
44.915447	1675.033484	18.313255
44.803515	1677.606126	18.318272
44.913408	1667.781003	18.323290
44.711591	1676.078417	18.328307
44.835234	1674.959123	18.333325
44.902433	1673.206211	18.338343
44.863606	1684.402071	18.343360
44.953930	1674.687823	18.348378
44.607278	1674.732135	18.353395
44.840620	1672.331342	18.358413
45.128680	1680.566362	18.363431
45.077735	1696.582642	18.368448
45.358339	1695.191334	18.373466
45.613443	1696.743477	18.378483
45.643528	1693.375375	18.383501
45.663283	1700.736065	18.388519
45.610161	1688.051027	18.393536
45.743694	1678.102570	18.398554
45.109002	1678.862184	18.403571
45.542482	1680.924672	18.408589
45.829188	1699.828849	18.413607
45.598724	1710.911351	18.418624
45.881482	1692.719497	18.423642
45.678466	1702.830144	18.428659
45.411078	1698.471220	18.433677
45.804646	1695.775079	18.438695
45.719993	1700.093477	18.443712
45.945860	1688.097021	18.448730
45.706964	1695.954379	18.453747
45.827655	1699.309524	18.458765
46.096362	1697.484356	18.463783
45.931188	1694.567420	18.468800
46.180880	1694.475724	18.473818
45.991614	1704.675420	18.478835
45.873631	1697.953430	18.483853
46.081124	1706.412112	18.488871
46.113087	1717.429956	18.493888
46.540406	1723.909203	18.498906
46.417949	1733.811955	18.503923
46.287920	1737.953545	18.508941
46.416720	1733.948305	18.513959
46.254158	1728.303925	18.518976
46.400387	1732.352687	18.523994
46.396819	1733.203572	18.529011
46.353710	1731.192160	18.534029
46.355198	1731.768514	18.539047
46.212217	1729.688082	18.544064
46.607928	1748.365711	18.549082
46.427473	1753.830485	18.554099
46.703522	1763.037302	18.559117
47.069878	1756.038253	18.564135
46.858017	1764.778582	18.569152
47.213885	1758.899702	18.574170
47.142792	1761.133128	18.579187
46.864594	1766.994194	18.584205
47.057680	1765.281759	18.589223
47.063929	1757.412779	18.594240
47.083656	1752.508579	18.599258
47.068653	1762.069362	18.604275
47.295994	1769.997129	18.609293
47.376379	1760.575439	18.614311
47.463772	1787.305604	18.619328
47.765372	1784.881322	18.624346
47.793505	1762.317347	18.629363
47.442600	1754.023950	18.634381
47.558872	1761.615472	18.639399
46.777180	1762.311225	18.644416
47.440283	1772.177601	18.649434
47.423982	1786.166192	18.654451
47.713698	1784.516214	18.659469
48.031223	1781.348446	18.664487
47.645429	1782.837633	18.669504
47.723102	1783.680283	18.674522
47.790834	1784.813188	18.679539
47.897481	1789.757888	18.684557
47.827640	1776.554732	18.689575
47.928236	1796.821160	18.694592
48.442778	1804.084114	18.699610
48.426897	1822.359472	18.704627
48.262400	1803.642591	18.709645
48.513912	1787.260778	18.714663
48.187623	1787.209028	18.719680
48.580942	1775.056012	18.724698
48.686167	1771.078118	18.729715
48.425148	1775.522200	18.734733
48.745612	1767.904357	18.739751
48.580396	1781.048323	18.744768
48.597001	1772.258185	18.749786
48.540345	1767.386613	18.754803
48.374487	1769.193103	18.759821
48.348158	1767.606117	18.764839
48.568177	1782.938227	18.769856
48.965217	1789.766063	18.774874
49.160059	1791.552787	18.779891
48.980538	1784.520437	18.784909
48.980704	1764.944370	18.789927
48.439299	1772.036703	18.794944
48.863190	1784.953003	18.799962
49.154800	1795.206641	18.804979
48.845165	1805.613594	18.809997
49.116759	1798.193092	18.815015
49.013223	1805.269882	18.820032
49.034818	1795.074123	18.825050
49.240506	1797.659057	18.830067
49.423926	1790.903900	18.835085
49.534901	1795.445975	18.840103
49.111773	1795.646425	18.845120
49.299898	1792.840663	18.850138
49.259268	1799.381203	18.855155
49.307891	1811.005265	18.860173
49.499125	1823.183147	18.865191
49.497348	1828.705189	18.870208
49.741704	1821.937153	18.875226
49.772219	1820.380423	18.880243
49.896772	1832.660977	18.885261
49.899731	1828.545996	18.890279
49.822775	1829.813673	18.895296
49.831812	1822.644260	18.900314
50.178521	1829.422723	18.905331
49.758318	1831.342936	18.910349
50.086243	1821.041672	18.915367
49.886572	1829.767510	18.920384
49.988595	1820.795395	18.925402
50.158023	1820.471876	18.930419
49.982981	1826.344044	18.935437
50.177794	1818.330118	18.940455
50.207540	1846.248652	18.945472
50.373305	1845.321631	18.950490
50.767172	1843.425359	18.955507
50.348720	1848.843174	18.960525
50.674651	1852.643858	18.965543
50.610808	1848.812466	18.970560
50.451892	1847.483373	18.975578
50.759607	1848.111575	18.980595
50.750557	1848.652644	18.985613
50.706135	1842.474961	18.990631
50.563094	1854.018718	18.995648
50.924506	1840.985057	19.000666
51.254442	1837.488084	19.005683
51.060292	1842.770232	19.010701
50.755612	1846.893298	19.015719
51.089393	1843.724498	19.020736
50.977416	1840.203613	19.025754
51.014313	1843.747561	19.030771
50.911170	1840.381795	19.035789
51.234782	1837.850167	19.040807
50.962607	1851.804117	19.045824
50.908060	1860.967760	19.050842
51.334783	1859.757642	19.055859
51.104448	1866.937274	19.060877
51.230166	1866.377674	19.065895
51.324462	1875.268245	19.070912
51.415129	1874.888068	19.075930
51.251059	1880.135541	19.080947
51.311250	1890.236590	19.085965
51.965944	1889.492733	19.090983
51.636536	1904.001742	19.096000
51.765283	1903.775166	19.101018
51.945467	1898.235732	19.106035
51.495722	1910.442761	19.111053
51.597151	1896.217952	19.116071
51.946270	1909.200561	19.121088
51.906581	1910.622764	19.126106
51.906713	1905.866367	19.131123
52.206865	1910.574165	19.136141
52.313934	1900.114571	19.141159
51.802328	1911.270378	19.146176
52.034306	1930.649235	19.151194
52.514910	1929.044310	19.156211
52.413418	1935.482924	19.161229
52.730686	1935.184593	19.166247
52.891146	1933.684212	19.171264
52.456148	1929.696469	19.176282
52.654299	1928.938897	19.181299
52.764542	1939.518101	19.186317
52.685233	1933.270431	19.191335
52.881083	1933.538135	19.196352
52.558209	1929.527003	19.201370
52.975254	1924.526345	19.206387
52.824493	1930.530759	19.211405
52.721283	1928.494296	19.216423
53.057136	1928.347170	19.221440
52.998445	1930.247496	19.226458
53.024619	1921.731044	19.231475
52.709774	1935.094868	19.236493
53.227992	1940.508852	19.241511
53.234489	1953.189038	19.246528
53.419709	1949.870075	19.251546
54.189313	1939.975740	19.256563
54.043990	1924.199013	19.261581
54.068362	1919.642469	19.266599
53.852088	1907.972770	19.271616
54.033141	1910.968313	19.276634
54.217657	1902.561910	19.281651
53.608799	1893.659074	19.286669
53.858018	1879.534989	19.291687
54.101566	1870.310594	19.296704
53.953988	1873.952401	19.301722
54.115791	1871.649508	19.306739
53.693690	1872.732329	19.311757
53.531076	1883.156005	19.316775
53.798389	1883.465797	19.321792
53.741537	1904.735197	19.326810
53.813362	1909.519523	19.331827
53.992997	1910.971247	19.336845
54.035359	1907.466634	19.341863
54.309693	1911.911114	19.346880
54.134739	1913.950326	19.351898
54.193094	1909.602314	19.356915
53.907394	1912.037529	19.361933
54.218154	1921.603883	19.366951
54.492837	1924.289531	19.371968
54.608088	1938.361902	19.376986
54.716756	1926.712731	19.382003
54.641686	1942.350854	19.387021
54.742688	1939.854711	19.392039
54.841743	1929.231980	19.397056
54.407255	1938.000837	19.402074
54.620613	1926.516669	19.407091
55.036549	1933.052102	19.412109
54.698444	1932.415448	19.417127
54.975932	1934.545328	19.422144
54.922218	1939.982092	19.427162
55.153440	1929.742583	19.432179
55.092848	1941.907239	19.437197
55.403639	1942.815763	19.442215
55.463072	1947.913563	19.447232
55.473544	1955.802081	19.452250
55.596315	1948.633345	19.457267
55.553473	1943.753218	19.462285
55.204857	1931.959876	19.467303
55.874354	1934.665938	19.472320
55.783576	1937.176258	19.477338
56.271589	1930.521124	19.482355
55.787932	1935.004692	19.487373
55.699757	1917.570195	19.492391
55.914485	1912.627763	19.497408
55.393944	1920.069224	19.502426
55.841110	1939.605700	19.507443
55.705728	1939.536087	19.512461
55.751353	1931.090465	19.517479
55.972917	1935.485163	19.522496
55.821640	1943.497006	19.527514
56.073298	1940.454549	19.532531
55.981609	1949.268639	19.537549
56.130734	1945.253020	19.542567
56.378866	1946.321773	19.547584
56.418257	1969.477860	19.552602
56.474260	1966.232987	19.557619
56.422551	1978.479635	19.562637
56.485620	1980.530450	19.567655
56.811027	1977.760966	19.572672
56.510906	1986.034903	19.577690
56.523092	1971.632327	19.582707
56.669375	1980.540629	19.587725
56.480052	1976.034665	19.592743
56.836948	1976.022621	19.597760
56.412557	1978.101622	19.602778
56.403406	1978.794522	19.607795
56.447833	1980.779878	19.612813
56.687771	1995.496291	19.617831
57.096981	2007.308416	19.622848
56.788271	2005.209539	19.627866
56.882584	1999.310924	19.632883
56.857170	2011.103482	19.637901
57.080048	2019.665295	19.642919
57.334778	2024.281266	19.647936
57.524485	2033.866213	19.652954
57.673255	2029.160797	19.657971
57.894333	2025.681142	19.662989
57.723435	2035.107289	19.668007
57.797321	2028.154755	19.673024
58.116634	2028.470417	19.678042
58.186189	2024.388022	19.683059
57.981104	2024.065233	19.688077
57.706135	2026.231317	19.693095
58.179734	2016.808106	19.698112
58.094035	2028.853346	19.703130
58.101405	2006.975842	19.708147
58.075045	2025.126487	19.713165
58.045650	2024.488577	19.718183
58.458032	2016.730881	19.723200
58.165390	2021.053440	19.728218
58.405054	2021.419560	19.733235
58.412911	2016.036563	19.738253
58.088925	2018.613980	19.743271
58.313349	2019.912268	19.748288
57.967147	2017.992416	19.753306
58.244722	2017.537592	19.758323
58.495582	2032.943706	19.763341
58.628770	2040.770224	19.768359
59.073676	2040.360294	19.773376
58.819349	2049.404892	19.778394
58.863756	2042.805507	19.783411
58.769234	2047.293910	19.788429
58.844640	2049.117018	19.793447
59.226156	2041.354006	19.798464
59.110123	2045.198482	19.803482
58.992041	2036.145710	19.808499
59.123378	2038.160475	19.813517
58.946097	2044.946307	19.818535
58.996662	2048.712301	19.823552
59.037287	2062.614207	19.828570
59.230782	2068.925604	19.833587
59.488489	2078.883589	19.838605
59.538164	2087.690949	19.843623
59.596386	2073.699394	19.848640
59.713175	2070.678420	19.853658
59.409447	2081.945934	19.858675
59.546813	2082.212742	19.863693
59.654785	2074.085100	19.868711
59.822250	2075.523836	19.873728
59.692700	2082.614347	19.878746
59.931267	2089.569857	19.883763
60.281750	2093.133074	19.888781
59.839242	2106.642481	19.893799
60.467813	2102.459901	19.898816
60.585972	2108.441952	19.903834
60.575712	2102.198143	19.908851
60.132095	2082.919745	19.913869
60.271249	2097.710542	19.918887
60.487827	2098.593986	19.923904
60.474034	2106.319699	19.928922
60.488502	2104.462664	19.933939
60.499301	2100.777404	19.938957
60.367962	2113.040010	19.943975
60.464573	2099.969691	19.948992
60.353271	2106.491750	19.954010
60.552808	2109.806099	19.959027
60.886667	2122.558506	19.964045
60.965880	2127.233177	19.969063
61.321390	2129.339632	19.974080
61.256324	2143.356793	19.979098
61.414691	2131.500527	19.984115
61.627482	2128.277024	19.989133
61.142675	2124.626747	19.994151
61.236730	2114.198179	19.999168
61.352213	2129.159540	20.004186
61.298286	2131.223528	20.009203
61.369569	2119.601404	20.014221
61.194411	2128.089894	20.019239
61.286968	2122.394448	20.024256
61.068529	2131.220995	20.029274
61.419673	2141.173561	20.034291
61.881721	2136.960894	20.039309
61.829582	2153.548142	20.044327
61.767237	2156.057112	20.049344
61.958095	2154.059458	20.054362
61.818771	2151.337312	20.059379
62.007372	2156.453129	20.064397
61.857132	2159.190855	20.069415
62.268297	2158.219173	20.074432
61.899972	2162.721386	20.079450
61.930545	2164.774263	20.084467
62.302779	2171.087877	20.089485
62.130968	2188.044281	20.094503
62.329459	2189.254689	20.099520
62.575702	2184.587167	20.104538
62.294244	2180.567786	20.109555
62.408106	2174.598336	20.114573
62.166878	2188.406871	20.119591
62.617308	2191.954961	20.124608
62.697802	2203.306813	20.129626
63.350573	2211.716804	20.134643
63.335933	2215.801583	20.139661
63.067459	2214.264963	20.144679
62.944026	2209.620204	20.149696
63.333380	2203.539161	20.154714
63.383911	2214.745561	20.159731
63.585108	2205.703906	20.164749
63.131294	2190.780768	20.169767
63.509618	2191.566057	20.174784
63.248124	2208.995369	20.179802
63.263683	2212.870818	20.184819
63.646981	2209.812819	20.189837
63.601220	2206.887747	20.194855
63.699666	2205.812548	20.199872
63.774356	2207.494991	20.204890
63.662474	2211.199622	20.209907
63.737464	2203.810271	20.214925
63.664242	2215.411611	20.219943
63.925931	2197.191815	20.224960
63.853280	2206.696795	20.229978
63.697830	2219.786895	20.234995
64.212906	2225.103953	20.240013
64.106834	2234.775533	20.245031
64.501076	2237.298227	20.250048
64.620156	2228.349099	20.255066
64.555045	2235.045551	20.260083
64.307901	2229.498629	20.265101
64.334361	2232.861060	20.270119
64.402493	2238.324913	20.275136
64.650499	2235.915399	20.280154
64.570150	2228.771053	20.285171
64.530945	2228.222011	20.290189
64.917278	2241.497890	20.295207
64.910203	2248.893025	20.300224
65.200208	2248.092473	20.305242
65.144302	2256.844406	20.310259
65.253051	2241.391009	20.315277
64.938568	2251.703085	20.320295
64.769681	2250.682316	20.325312
65.197070	2244.838247	20.330330
65.229967	2255.681726	20.335347
65.542814	2249.817379	20.340365
65.157062	2261.013946	20.345383
65.243738	2250.692647	20.350400
65.619022	2246.244437	20.355418
65.604343	2246.695175	20.360435
65.674412	2251.687555	20.365453
65.385714	2273.400347	20.370471
65.732068	2270.931881	20.375488
65.948501	2280.664542	20.380506
65.485272	2293.536349	20.385523
65.891173	2280.860185	20.390541
65.653061	2282.552404	20.395559
65.680827	2276.550234	20.400576
66.151744	2287.235784	20.405594
66.216716	2304.875082	20.410611
66.301981	2305.309883	20.415629
66.141703	2307.246123	20.420647
66.213483	2308.415395	20.425664
66.459064	2310.916974	20.430682
66.505974	2314.068501	20.435699
66.700647	2300.147787	20.440717
66.816117	2305.288691	20.445735
66.936361	2308.119390	20.450752
66.854189	2302.504442	20.455770
67.039490	2306.475555	20.460787
67.181096	2297.868894	20.465805
67.217103	2306.461466	20.470823
67.296124	2297.891531	20.475840
67.238314	2292.294726	20.480858
66.933588	2303.817425	20.485875
67.423789	2297.603059	20.490893
67.427008	2288.168950	20.495911
67.177641	2297.061097	20.500928
67.364314	2289.107994	20.505946
67.217691	2314.669024	20.510963
67.541720	2323.876414	20.515981
67.782458	2322.639288	20.520999
67.683543	2321.464194	20.526016
68.068681	2324.254225	20.531034
67.653496	2339.412127	20.536051
67.964531	2327.684742	20.541069
68.100998	2331.789505	20.546087
68.140127	2328.267215	20.551104
68.133535	2327.543850	20.556122
67.990337	2326.987790	20.561139
67.849125	2318.497800	20.566157
67.825745	2327.208405	20.571175
67.943463	2335.098903	20.576192
68.353375	2328.668428	20.581210
68.115317	2342.581220	20.586227
68.217993	2347.412687	20.591245
68.399881	2345.480152	20.596263
68.766301	2374.172720	20.601280
68.681330	2374.026630	20.606298
68.806021	2382.432051	20.611315
68.975067	2375.338321	20.616333
68.924282	2380.022006	20.621351
68.808424	2383.588873	20.626368
69.061213	2367.789079	20.631386
68.786551	2382.996982	20.636403
68.836594	2374.017872	20.641421
69.014511	2380.565510	20.646439
69.135980	2397.546966	20.651456
69.238885	2399.569463	20.656474
69.360809	2403.553069	20.661491
69.639463	2396.576358	20.666509
69.449043	2401.089600	20.671527
69.492592	2411.799347	20.676544
70.111103	2392.151359	20.681562
69.921260	2399.482899	20.686579
69.795410	2393.567320	20.691597
70.103461	2393.754212	20.696615
69.841333	2398.584878	20.701632
69.955185	2398.795661	20.706650
69.749183	2404.759522	20.711667
70.051171	2407.977369	20.716685
70.476223	2425.395777	20.721703
70.481671	2429.820371	20.726720
70.857011	2432.696153	20.731738
70.555189	2423.803803	20.736755
70.940139	2418.273996	20.741773
70.585708	2407.844374	20.746791
70.476389	2426.122016	20.751808
70.589450	2421.375760	20.756826
70.779217	2428.437540	20.761843
70.786670	2423.668008	20.766861
70.844890	2424.459523	20.771879
70.908823	2426.443403	20.776896
71.274717	2420.242516	20.781914
71.170881	2421.594764	20.786931
70.973945	2426.130292	20.791949
71.396821	2417.304867	20.796967
70.994906	2427.114999	20.801984
71.600487	2430.761117	20.807002
71.556186	2441.623338	20.812019
71.264084	2437.697614	20.817037
71.579856	2437.272086	20.822055
71.447234	2442.844331	20.827072
71.891644	2435.864766	20.832090
71.823578	2438.415599	20.837107
71.684371	2445.348932	20.842125
71.808246	2441.454409	20.847143
71.660574	2452.595848	20.852160
72.071366	2463.314715	20.857178
72.029548	2466.720339	20.862195
72.169455	2475.468708	20.867213
72.115553	2478.718154	20.872231
71.813713	2483.389993	20.877248
72.346729	2468.959718	20.882266
72.523251	2486.244780	20.887283
72.401354	2500.187966	20.892301
72.973009	2501.080886	20.897319
72.988284	2496.770247	20.902336
73.240957	2491.006648	20.907354
73.242130	2499.445994	20.912371
73.122653	2487.562167	20.917389
73.539849	2484.892011	20.922407
73.171073	2483.873997	20.927424
73.200454	2458.192218	20.932442
73.086293	2461.643201	20.937459
73.040273	2468.954986	20.942477
73.467141	2482.406328	20.947495
73.352572	2488.937729	20.952512
73.486488	2489.529178	20.957530
73.456484	2489.808527	20.962547
73.572095	2484.895083	20.967565
73.858288	2489.899489	20.972583
73.507620	2495.914775	20.977600
73.607168	2493.181215	20.982618
73.702094	2492.526605	20.987635
74.002452	2496.997009	20.992653
73.831097	2480.002231	20.997671
73.935336	2505.861829	21.002688
74.086514	2513.539424	21.007706
74.279635	2519.220219	21.012723
74.280103	2518.878796	21.017741
74.674838	2507.158372	21.022759
74.261644	2519.268828	21.027776
74.413364	2519.969923	21.032794
74.654391	2522.006594	21.037811
74.344797	2524.877566	21.042829
74.689387	2515.268521	21.047847
74.847521	2534.567140	21.052864
75.142924	2533.006637	21.057882
75.206342	2535.774862	21.062899
75.194842	2537.562334	21.067917
75.383322	2530.580275	21.072935
75.384819	2537.296920	21.077952
75.664295	2535.250473	21.082970
75.784370	2534.656353	21.087987
75.256529	2529.651214	21.093005
75.722147	2531.182466	21.098023
75.569178	2534.338385	21.103040
75.862431	2533.576632	21.108058
75.545516	2538.917149	21.113075
75.715289	2529.502734	21.118093
76.129368	2518.025426	21.123111
76.163526	2534.349203	21.128128
76.254281	2536.322527	21.133146
76.235017	2535.100889	21.138163
75.984114	2533.985413	21.143181
76.441225	2532.406201	21.148199
75.726170	2541.445126	21.153216
75.760845	2534.825834	21.158234
75.911871	2548.891517	21.163251
76.072233	2561.123712	21.168269
76.525741	2563.771525	21.173287
76.162085	2573.452154	21.178304
76.116349	2574.175302	21.183322
76.402120	2589.676338	21.188339
76.640702	2600.348042	21.193357
76.846518	2599.110170	21.198375
76.944469	2596.338302	21.203392
77.084949	2594.376155	21.208410
77.088444	2593.142230	21.213427
76.881782	2596.396398	21.218445
77.046660	2604.250418	21.223463
76.874777	2624.980715	21.228480
77.396951	2627.007965	21.233498
77.801919	2621.955511	21.238515
77.591242	2630.060582	21.243533
77.832763	2621.509380	21.248551
77.706300	2627.590438	21.253568
77.766731	2632.422443	21.258586
77.998720	2626.004481	21.263603
77.924133	2618.733954	21.268621
78.554405	2610.871193	21.273639
78.360108	2608.928607	21.278656
78.263800	2607.484839	21.283674
78.551988	2610.712799	21.288691
78.577884	2613.702554	21.293709
78.587252	2614.649753	21.298727
78.640390	2614.528046	21.303744
78.321900	2611.164977	21.308762
78.683875	2612.164498	21.313779
78.636410	2621.662585	21.318797
78.921903	2624.050089	21.323815
79.028784	2637.296955	21.328832
79.113404	2633.795655	21.333850
79.458883	2633.939613	21.338867
79.215477	2630.073720	21.343885
79.478495	2629.582659	21.348903
79.581523	2625.276081	21.353920
79.563052	2619.159218	21.358938
79.542846	2610.744941	21.363955
79.399664	2619.995562	21.368973
79.770549	2612.423521	21.373991
79.417009	2625.230141	21.379008
79.647576	2622.200350	21.384026
79.935621	2625.648588	21.389043
79.600878	2622.285749	21.394061
79.733888	2630.413886	21.399079
79.996629	2631.576330	21.404096
79.994216	2622.057951	21.409114
80.163472	2634.363517	21.414131
80.062485	2657.241809	21.419149
80.215263	2656.349848	21.424167
80.401222	2655.660262	21.429184
80.270941	2662.598567	21.434202
80.382063	2654.647089	21.439219
80.415116	2655.411953	21.444237
80.471839	2663.402031	21.449255
80.433830	2669.650708	21.454272
80.606608	2674.159604	21.459290
80.677052	2673.671721	21.464307
80.755352	2685.904521	21.469325
81.082482	2680.615103	21.474343
80.690773	2692.151977	21.479360
80.661097	2701.781004	21.484378
81.082508	2709.995346	21.489395
81.107578	2714.236762	21.494413
81.437213	2715.001529	21.499431
81.388416	2716.666753	21.504448
81.616981	2714.213853	21.509466
81.784427	2728.035600	21.514483
81.968760	2745.816867	21.519501
82.007369	2734.470849	21.524519
82.306246	2735.058027	21.529536
82.156489	2740.722792	21.534554
82.404206	2733.876714	21.539571
82.572540	2736.504747	21.544589
82.428451	2721.270513	21.549607
82.275103	2720.063949	21.554624
82.063835	2731.516229	21.559642
82.180227	2729.125265	21.564659
81.914731	2739.023188	21.569677
82.297470	2738.123656	21.574695
82.649207	2749.727661	21.579712
82.711840	2758.613594	21.584730
82.729432	2768.031392	21.589747
82.593812	2770.743301	21.594765
82.584864	2768.663368	21.599783
83.032116	2767.283148	21.604800
82.909813	2778.132885	21.609818
83.287334	2783.913383	21.614835
83.146697	2790.533244	21.619853
83.217560	2801.725053	21.624871
83.507044	2793.156665	21.629888
83.399123	2795.758753	21.634906
83.753342	2799.911520	21.639923
83.862176	2818.823493	21.644941
84.020171	2817.420959	21.649959
84.245129	2815.514535	21.654976
84.606481	2810.095327	21.659994
84.591927	2805.429081	21.665011
84.661766	2787.394112	21.670029
84.383186	2780.174127	21.675047
84.444345	2766.671505	21.680064
84.324512	2784.858451	21.685082
84.694101	2789.120464	21.690099
84.952411	2800.704797	21.695117
84.544602	2808.300992	21.700135
84.515669	2804.492099	21.705152
84.954238	2807.658365	21.710170
85.337220	2799.017639	21.715187
84.999973	2805.582332	21.720205
84.941673	2800.713822	21.725223
85.343578	2797.875353	21.730240
85.034672	2810.746599	21.735258
85.196674	2790.961638	21.740275
85.095398	2801.961431	21.745293
85.367530	2814.765982	21.750311
85.410357	2835.195672	21.755328
85.436196	2837.042517	21.760346
85.421738	2829.768589	21.765363
85.350650	2847.969078	21.770381
85.428345	2840.192742	21.775399
85.713392	2856.821412	21.780416
85.624534	2868.705015	21.785434
86.127621	2863.998681	21.790451
85.905185	2865.276273	21.795469
85.627563	2868.913104	21.800487
86.029547	2883.193957	21.805504
86.142530	2895.822582	21.810522
86.467613	2902.272257	21.815539
86.555472	2904.951699	21.820557
86.527937	2902.715813	21.825575
86.559671	2911.636659	21.830592
86.470430	2932.718421	21.835610
86.970204	2930.573860	21.840627
86.926180	2934.854677	21.845645
87.066337	2929.704328	21.850663
87.324151	2929.734837	21.855680
87.068497	2929.629331	21.860698
87.440250	2936.780333	21.865715
87.552002	2945.120493	21.870733
87.637424	2957.648944	21.875751
88.232079	2954.572825	21.880768
87.831649	2959.593279	21.885786
87.999732	2940.450611	21.890803
88.363565	2944.830797	21.895821
89.079839	2917.546438	21.900839
89.153198	2896.643511	21.905856
88.956543	2883.476094	21.910874
89.000508	2873.866772	21.915891
89.027073	2880.770728	21.920909
88.967902	2872.294077	21.925927
89.139477	2846.630631	21.930944
88.893787	2844.966806	21.935962
88.996464	2837.509004	21.940979
89.084229	2836.639987	21.945997
88.969715	2843.068489	21.951015
89.203162	2839.393949	21.956032
88.957696	2839.853189	21.961050
89.077667	2838.204997	21.966067
89.077052	2838.272783	21.971085
89.230120	2849.269024	21.976103
89.596192	2866.268658	21.981120
89.512775	2871.135481	21.986138
89.601157	2870.562135	21.991155
89.631043	2877.359365	21.996173
89.807075	2875.725828	22.001191
89.652224	2871.858334	22.006208
89.570316	2887.982333	22.011226
89.777565	2869.829381	22.016243
89.674355	2875.136726	22.021261
89.842593	2901.317202	22.026279
89.923277	2900.096114	22.031296
90.191910	2898.517818	22.036314
90.230931	2896.398752	22.041331
90.447786	2892.011015	22.046349
90.551713	2893.741580	22.051367
90.647619	2895.313739	22.056384
90.920051	2923.686490	22.061402
91.319272	2912.628945	22.066419
91.062765	2907.649626	22.071437
90.764389	2909.471879	22.076455
91.126134	2912.101354	22.081472
90.918736	2921.363978	22.086490
90.933759	2923.593287	22.091507
91.260476	2926.354998	22.096525
91.093154	2930.300705	22.101543
91.364576	2926.961485	22.106560
91.314516	2950.234867	22.111578
91.460832	2948.071152	22.116595
91.933657	2951.082530	22.121613
91.421672	2956.429130	22.126631
91.784830	2959.384054	22.131648
91.929792	2965.429047	22.136666
91.860432	2984.701610	22.141683
92.152414	2980.994102	22.146701
92.188303	2987.316873	22.151719
92.228285	2992.360717	22.156736
92.134564	2993.137161	22.161754
92.352258	2999.795944	22.166771
92.583203	3013.464668	22.171789
92.590361	3020.224684	22.176807
92.925454	3011.533261	22.181824
93.004544	3011.497875	22.186842
92.922715	3013.955820	22.191859
92.892111	3015.137543	22.196877
93.125201	3030.482258	22.201895
93.451746	3023.662022	22.206912
93.569270	3034.346270	22.211930
93.454237	3041.556070	22.216947
93.900279	3038.368332	22.221965
93.803272	3034.272886	22.226983
93.788572	3032.288229	22.232000
93.624769	3030.896086	22.237018
93.446661	3026.555558	22.242035
93.994918	3049.492978	22.247053
94.245383	3059.447286	22.252071
94.394156	3065.878739	22.257088
94.557238	3071.562181	22.262106
94.406535	3063.865412	22.267123
94.626900	3065.251763	22.272141
94.418590	3069.729517	22.277159
94.580411	3068.705509	22.282176
94.746505	3072.287364	22.287194
94.682558	3069.812615	22.292211
94.969247	3088.910542	22.297229
95.004232	3102.759273	22.302247
95.173370	3100.499860	22.307264
95.216277	3103.576679	22.312282
95.166232	3099.737250	22.317299
95.142854	3096.125627	22.322317
94.975996	3104.286114	22.327335
95.343032	3103.842171	22.332352
95.479121	3114.720177	22.337370
95.479613	3125.423940	22.342387
95.750408	3110.735146	22.347405
95.649729	3119.587557	22.352423
95.944871	3109.874309	22.357440
95.871591	3132.620702	22.362458
96.079320	3146.999657	22.367475
96.502715	3153.514005	22.372493
96.291754	3157.081277	22.377511
96.207044	3147.893482	22.382528
96.633542	3150.939036	22.387546
96.724185	3155.566590	22.392563
96.637682	3142.939101	22.397581
96.622565	3162.518691	22.402599
97.463031	3163.836847	22.407616
97.438018	3170.090745	22.412634
97.214041	3165.055805	22.417651
97.314893	3164.066686	22.422669
97.253915	3165.708730	22.427687
97.435211	3157.346177	22.432704
97.485010	3165.988973	22.437722
97.259314	3167.252163	22.442739
97.875662	3170.774044	22.447757
97.848750	3190.986439	22.452775
97.892963	3197.011410	22.457792
98.053434	3198.038388	22.462810
98.060616	3203.530415	22.467827
98.024543	3192.065369	22.472845
97.922601	3204.059886	22.477863
98.083795	3202.760644	22.482880
97.993790	3218.832019	22.487898
98.366643	3228.056586	22.492915
98.794055	3228.496641	22.497933
98.875247	3232.671833	22.502951
99.137140	3224.094222	22.507968
99.066478	3221.939108	22.512986
98.973109	3233.255768	22.518003
99.480524	3246.694976	22.523021
99.264661	3250.293731	22.528039
99.017770	3259.039745	22.533056
99.341404	3251.727427	22.538074
99.123023	3259.140249	22.543091
99.624418	3253.381531	22.548109
99.730728	3267.520330	22.553127
99.838377	3274.704961	22.558144
100.082235	3277.449274	22.563162
99.952178	3284.018110	22.568179
100.207474	3285.439032	22.573197
100.038609	3290.474588	22.578215
100.280706	3286.037084	22.583232
100.341849	3277.493814	22.588250
100.248285	3291.568537	22.593267
100.391429	3294.226649	22.598285
100.397652	3311.022229	22.603303
100.255289	3309.149144	22.608320
100.884309	3307.036629	22.613338
101.080711	3311.501051	22.618355
101.103686	3302.915867	22.623373
101.199809	3321.410447	22.628391
101.071005	3328.541558	22.633408
101.619473	3324.119693	22.638426
101.780191	3330.937177	22.643443
101.472747	3327.990675	22.648461
101.459101	3328.103021	22.653479
101.852241	3327.537700	22.658496
101.945671	3323.022413	22.663514
101.849656	3335.882981	22.668531
102.020278	3348.627097	22.673549
102.073648	3359.250227	22.678567
102.093566	3356.528419	22.683584
102.160942	3354.550298	22.688602
102.399397	3350.711210	22.693619
102.585889	3344.334805	22.698637
102.280822	3350.098514	22.703655
102.986679	3368.260715	22.708672
103.193653	3375.181762	22.713690
103.112376	3385.413389	22.718707
103.138211	3376.189730	22.723725
103.319885	3380.809920	22.728743
103.259765	3377.455029	22.733760
103.174606	3373.866562	22.738778
103.273921	3381.368810	22.743795
103.687326	3389.510084	22.748813
103.843754	3399.137426	22.753831
103.559987	3400.944820	22.758848
103.960898	3404.621472	22.763866
104.129283	3413.370583	22.768883
103.949668	3407.597682	22.773901
104.016125	3410.706210	22.778919
103.976863	3408.995242	22.783936
104.440572	3419.728407	22.788954
104.284867	3426.980281	22.793971
104.827300	3421.871026	22.798989
104.548720	3433.056109	22.804007
104.560669	3431.327532	22.809024
104.817341	3423.288711	22.814042
104.759781	3440.681456	22.819059
104.660263	3451.458831	22.824077
104.638110	3457.070482	22.829095
105.001638	3459.519631	22.834112
105.511711	3472.660481	22.839130
105.503831	3484.969051	22.844147
105.528280	3482.770413	22.849165
105.401449	3491.832536	22.854183
105.497690	3491.683496	22.859200
105.866143	3496.524884	22.864218
105.926876	3494.763347	22.869235
105.937913	3520.275377	22.874253
106.056030	3517.764439	22.879271
106.336306	3515.832586	22.884288
106.103772	3517.583051	22.889306
106.235758	3522.380342	22.894323
106.490694	3514.514027	22.899341
106.776133	3523.233525	22.904359
106.768947	3525.868451	22.909376
107.137027	3518.967419	22.914394
107.070688	3526.264090	22.919411
107.542228	3525.149758	22.924429
107.839354	3523.551909	22.929447
107.585344	3523.359600	22.934464
108.029777	3521.450343	22.939482
108.097233	3524.280258	22.944499
107.888486	3522.002374	22.949517
108.065863	3524.522910	22.954535
107.733435	3531.087939	22.959552
108.016601	3519.858076	22.964570
108.017704	3525.942762	22.969587
108.151295	3519.691930	22.974605
108.760791	3521.358473	22.979623
108.612648	3522.071250	22.984640
108.533746	3517.616423	22.989658
108.267595	3523.503792	22.994675
108.603846	3541.438016	22.999693
108.537860	3551.892306	23.004711
108.403255	3550.563896	23.009728
109.040934	3553.862207	23.014746
108.897217	3554.024402	23.019763
108.736147	3576.786268	23.024781
109.056721	3582.764969	23.029799
108.908686	3577.156098	23.034816
109.300001	3594.166716	23.039834
109.642546	3603.799914	23.044851
109.754514	3601.990862	23.049869
110.134027	3596.249876	23.054887
110.058262	3610.437705	23.059904
110.451182	3597.930043	23.064922
110.242478	3610.357275	23.069939
110.228817	3610.490079	23.074957
110.460918	3612.604638	23.079975
110.634583	3625.682057	23.084992
110.920605	3622.446555	23.090010
110.796512	3629.816207	23.095027
111.009273	3629.219066	23.100045
111.066923	3625.975139	23.105063
110.988983	3629.913072	23.110080
111.235561	3617.483796	23.115098
111.599443	3623.118128	23.120115
111.460664	3621.952430	23.125133
111.815096	3617.278221	23.130151
111.815104	3621.327230	23.135168
111.895369	3617.068046	23.140186
111.487810	3627.856909	23.145203
112.216904	3640.440641	23.150221
112.396876	3643.964572	23.155239
112.004865	3652.128224	23.160256
112.409148	3648.272845	23.165274
112.159018	3642.187774	23.170291
112.467082	3646.197895	23.175309
112.384942	3652.803308	23.180327
112.314185	3655.707994	23.185344
112.581023	3666.768523	23.190362
112.501858	3673.791192	23.195379
112.653808	3676.672957	23.200397
113.016943	3679.751542	23.205415
112.894482	3693.264856	23.210432
113.370252	3707.937530	23.215450
113.265901	3713.715000	23.220467
113.308429	3724.764927	23.225485
113.823010	3721.273477	23.230503
113.486792	3721.245314	23.235520
113.753726	3732.164275	23.240538
113.677487	3753.223902	23.245555
114.045573	3753.730865	23.250573
114.290858	3758.046817	23.255591
113.778438	3747.913610	23.260608
114.329170	3761.074985	23.265626
114.459657	3771.851319	23.270643
114.400646	3777.891415	23.275661
114.646905	3774.574899	23.280679
114.573292	3781.804417	23.285696
114.939283	3797.803713	23.290714
115.082302	3794.517816	23.295731
115.238136	3796.445535	23.300749
115.358292	3790.857538	23.305767
115.347759	3805.952418	23.310784
115.563903	3816.250200	23.315802
115.712961	3822.288603	23.320819
115.556242	3832.287914	23.325837
115.782961	3826.563336	23.330855
115.872513	3826.708004	23.335872
116.276565	3826.914232	23.340890
116.013576	3842.763708	23.345907
116.416192	3848.842719	23.350925
116.697448	3846.690398	23.355943
116.549772	3866.385677	23.360960
116.756247	3863.012552	23.365978
116.864191	3850.067884	23.370995
116.721705	3853.279052	23.376013
116.986992	3874.092444	23.381031
117.168493	3881.467774	23.386048
117.465842	3874.638430	23.391066
117.792252	3877.964425	23.396083
117.657870	3878.746611	23.401101
117.961702	3865.791148	23.406119
117.653222	3872.978706	23.411136
117.921267	3874.838982	23.416154
118.048601	3868.230274	23.421171
118.161597	3866.106355	23.426189
118.220049	3861.650761	23.431207
118.219388	3874.104042	23.436224
118.372645	3887.331272	23.441242
118.828875	3891.000803	23.446259
118.456070	3894.666432	23.451277
118.998375	3886.143634	23.456295
119.083317	3894.506704	23.461312
118.885419	3896.699311	23.466330
119.025909	3892.325816	23.471347
119.006434	3901.265657	23.476365
118.937007	3915.696642	23.481383
119.234337	3919.985462	23.486400
119.179089	3921.552728	23.491418
119.281147	3924.918441	23.496435
119.312195	3944.745024	23.501453
119.793577	3933.709805	23.506471
119.921989	3942.711839	23.511488
120.102146	3944.739542	23.516506
120.376496	3961.684277	23.521523
120.303140	3969.751665	23.526541
120.462000	3975.724060	23.531559
120.253067	3979.853685	23.536576
120.641136	3977.205223	23.541594
120.795108	3979.500646	23.546611
120.783117	3991.879524	23.551629
121.344984	4006.686668	23.556647
121.294343	4006.198382	23.561664
121.178857	4006.669967	23.566682
121.304882	4004.512483	23.571699
121.132562	4014.742543	23.576717
121.479587	4028.719397	23.581735
121.766184	4030.805662	23.586752
121.706921	4040.918591	23.591770
121.503497	4042.856426	23.596787
121.389765	4060.374504	23.601805
122.001176	4055.538033	23.606823
121.893914	4071.872698	23.611840
122.202724	4087.103392	23.616858
122.729910	4091.660062	23.621875
122.793559	4102.733652	23.626893
123.094457	4093.009403	23.631911
123.268502	4101.842200	23.636928
123.328262	4104.029154	23.641946
123.680365	4106.625775	23.646963
123.406640	4117.785426	23.651981
123.823434	4122.119766	23.656999
123.633234	4116.331752	23.662016
123.724328	4119.074624	23.667034
124.071211	4120.960123	23.672051
124.404032	4108.439587	23.677069
124.849287	4088.129408	23.682087
124.829039	4089.618736	23.687104
125.233741	4086.420066	23.692122
125.494073	4070.432372	23.697139
125.140296	4056.322108	23.702157
125.367285	4045.285676	23.707175
125.392853	4047.555956	23.712192
125.194008	4041.315430	23.717210
125.701799	4038.329259	23.722227
125.445221	4040.744436	23.727245
125.484450	4044.482859	23.732263
125.376616	4049.366551	23.737280
125.604458	4051.816985	23.742298
125.771736	4042.581368	23.747315
125.154752	4049.182557	23.752333
125.533056	4051.497290	23.757351
125.940358	4066.528960	23.762368
125.603449	4071.195084	23.767386
126.165897	4062.986011	23.772403
126.109100	4093.990723	23.777421
126.139513	4101.234491	23.782439
126.449138	4111.551404	23.787456
126.461280	4111.996348	23.792474
126.849984	4118.264925	23.797491
126.502811	4134.783452	23.802509
127.010975	4133.704150	23.807527
127.215384	4139.641815	23.812544
127.225223	4152.196714	23.817562
127.652544	4155.379240	23.822579
127.699497	4148.647912	23.827597
127.635257	4157.676863	23.832615
127.666301	4160.270405	23.837632
127.704769	4165.164635	23.842650
127.899767	4164.427129	23.847667
127.824652	4186.237703	23.852685
128.114073	4182.835547	23.857703
128.233472	4205.506461	23.862720
128.623863	4211.689846	23.867738
129.094977	4219.956912	23.872755
128.957394	4219.414826	23.877773
128.886910	4220.659646	23.882791
129.049594	4218.390868	23.887808
129.102113	4242.638820	23.892826
129.476586	4240.923147	23.897843
129.362134	4260.753688	23.902861
129.485438	4245.489391	23.907879
129.749377	4256.068581	23.912896
129.796281	4276.508282	23.917914
129.746484	4283.356631	23.922931
129.742488	4284.852827	23.927949
129.878322	4283.856483	23.932967
129.894038	4315.835051	23.937984
130.467142	4321.066545	23.943002
130.570388	4311.560904	23.948019
130.355181	4325.173761	23.953037
130.630844	4347.551712	23.958055
131.050379	4351.463225	23.963072
130.847945	4359.269766	23.968090
131.230392	4350.405589	23.973107
131.112395	4359.595855	23.978125
131.105719	4366.383084	23.983143
131.434970	4365.456594	23.988160
131.687270	4372.740639	23.993178
132.119356	4369.956859	23.998195
132.072422	4386.013986	24.003213
132.052344	4395.866017	24.008231
132.614427	4395.641119	24.013248
132.454948	4396.246390	24.018266
132.336034	4394.506311	24.023283
132.387835	4396.443618	24.028301
132.719208	4414.474882	24.033319
133.027042	4420.138917	24.038336
132.945174	4434.935066	24.043354
133.380383	4422.498639	24.048371
133.097990	4423.360309	24.053389
133.157957	4432.631597	24.058407
133.784530	4446.780623	24.063424
133.619842	4456.507850	24.068442
134.158122	4460.335163	24.073459
134.091299	4458.493151	24.078477
134.125028	4457.022170	24.083495
134.197216	4462.556225	24.088512
134.291997	4481.891901	24.093530
134.418091	4483.344560	24.098547
134.328292	4494.143961	24.103565
134.339575	4487.270265	24.108583
134.746863	4504.828522	24.113600
134.915020	4516.447474	24.118618
134.990464	4514.585131	24.123635
135.066978	4518.492380	24.128653
135.310672	4536.364697	24.133671
135.566080	4550.035678	24.138688
135.546990	4553.462548	24.143706
135.774176	4539.691879	24.148723
135.943979	4556.208691	24.153741
136.118068	4567.464848	24.158759
136.293820	4570.042470	24.163776
136.302665	4574.251608	24.168794
136.271931	4575.615208	24.173811
136.619957	4579.515371	24.178829
136.944999	4598.533627	24.183847
136.849196	4593.794802	24.188864
137.268731	4596.504277	24.193882
137.153107	4587.310281	24.198899
137.364870	4599.374709	24.203917
137.298732	4618.662271	24.208935
137.512290	4623.081092	24.213952
137.804362	4621.852908	24.218970
137.572911	4618.183614	24.223987
138.144133	4633.706606	24.229005
138.641269	4642.013820	24.234023
138.861589	4633.726031	24.239040
138.608992	4630.069546	24.244058
138.791991	4632.756951	24.249075
138.753492	4645.884844	24.254093
138.914536	4648.583620	24.259111
138.962913	4639.699372	24.264128
138.591508	4642.389424	24.269146
138.967736	4642.980880	24.274163
139.145277	4658.865623	24.279181
139.381973	4662.718261	24.284199
139.610380	4668.044966	24.289216
139.487855	4675.462879	24.294234
139.570049	4674.463262	24.299251
139.839735	4687.452366	24.304269
139.996196	4700.791532	24.309287
140.314127	4703.499920	24.314304
140.171084	4707.517752	24.319322
140.014424	4709.996562	24.324339
140.684244	4730.107848	24.329357
140.525702	4728.046769	24.334375
140.869525	4732.172647	24.339392
140.934298	4755.106443	24.344410
141.026303	4758.950708	24.349427
141.006156	4763.978786	24.354445
141.220583	4776.942950	24.359463
142.077736	4782.969549	24.364480
141.919862	4802.065068	24.369498
141.676694	4801.356486	24.374515
141.870218	4794.263201	24.379533
141.655968	4805.166852	24.384551
142.267283	4817.860861	24.389568
142.466769	4818.978506	24.394586
142.615608	4818.004443	24.399603
142.440913	4829.328999	24.404621
142.879634	4844.874915	24.409639
142.936877	4849.658597	24.414656
143.072309	4856.682228	24.419674
143.007894	4861.037660	24.424691
143.289013	4877.654307	24.429709
143.151594	4878.071983	24.434727
143.659486	4887.355532	24.439744
143.867142	4906.890121	24.444762
143.549615	4916.609763	24.449779
143.783099	4909.327529	24.454797
143.917036	4934.631236	24.459815
144.914774	4923.523186	24.464832
145.025784	4925.672982	24.469850
145.222847	4925.541685	24.474867
145.646944	4922.611173	24.479885
145.577972	4928.942845	24.484903
145.723105	4913.882077	24.489920
145.611230	4923.630299	24.494938
145.780671	4918.545398	24.499955
146.282236	4916.490759	24.504973
145.968701	4918.919877	24.509991
146.100503	4917.898960	24.515008
146.363597	4912.567828	24.520026
146.166453	4913.555970	24.525043
146.154044	4921.639335	24.530061
146.382650	4934.073478	24.535079
146.708064	4940.247865	24.540096
146.815782	4946.158005	24.545114
146.730264	4951.691427	24.550131
147.077330	4939.843728	24.555149
146.754559	4955.032052	24.560167
146.986564	4970.940704	24.565184
147.011809	4982.328694	24.570202
147.503018	4981.189889	24.575219
147.688290	5002.624215	24.580237
147.542547	5011.951482	24.585255
147.984026	5011.027517	24.590272
148.033427	5021.536830	24.595290
147.832427	5028.364001	24.600307
148.422502	5038.794988	24.605325
148.106221	5037.987906	24.610343
148.383504	5062.896850	24.615360
148.711298	5063.010627	24.620378
148.801951	5066.447655	24.625395
149.108344	5074.352821	24.630413
149.323382	5096.266384	24.635431
149.465062	5102.455186	24.640448
149.708677	5108.171427	24.645466
149.728437	5104.467464	24.650483
149.806753	5117.974456	24.655501
149.834471	5124.385205	24.660519
150.508489	5128.357846	24.665536
150.555347	5125.477215	24.670554
150.494664	5127.869198	24.675571
150.835455	5142.788272	24.680589
150.659107	5162.760491	24.685607
151.008081	5149.268016	24.690624
150.998347	5161.922091	24.695642
150.720203	5166.142539	24.700659
151.504190	5174.722170	24.705677
151.759600	5188.440949	24.710695
151.859825	5182.304882	24.715712
151.730041	5190.850048	24.720730
151.913798	5207.197787	24.725747
151.765553	5221.541122	24.730765
151.827565	5224.032358	24.735783
152.328079	5235.922242	24.740800
152.509317	5247.466518	24.745818
152.438184	5250.908142	24.750835
153.197637	5244.940731	24.755853
153.006647	5271.080428	24.760871
153.369189	5270.298849	24.765888
153.386931	5277.043265	24.770906
153.154216	5277.710598	24.775923
153.801540	5288.897362	24.780941
154.071538	5296.532300	24.785959
154.188802	5295.378354	24.790976
154.264487	5299.326067	24.795994
154.235599	5296.654168	24.801011
154.576925	5283.678116	24.806029
154.451868	5293.679658	24.811047
154.582816	5284.110756	24.816064
155.268332	5294.104222	24.821082
155.352524	5308.570294	24.826099
155.662495	5303.686295	24.831117
155.452477	5304.449928	24.836135
155.686119	5309.278803	24.841152
155.876478	5297.155263	24.846170
155.932864	5305.709364	24.851187
156.105671	5299.239105	24.856205
155.888140	5310.153878	24.861223
156.169439	5324.077934	24.866240
156.339382	5339.193600	24.871258
156.033556	5343.457062	24.876275
156.532585	5332.985251	24.881293
156.442695	5352.525386	24.886311
156.829407	5361.946573	24.891328
157.146213	5368.884885	24.896346
156.622194	5380.998817	24.901363
157.361523	5388.311931	24.906381
157.448955	5400.333898	24.911399
157.471177	5406.452184	24.916416
157.795191	5414.789803	24.921434
157.779122	5433.345837	24.926451
157.967494	5440.251159	24.931469
158.084273	5462.010991	24.936487
158.429788	5462.412265	24.941504
158.948779	5456.199089	24.946522
158.464945	5470.240553	24.951539
158.878254	5481.257070	24.956557
158.823219	5491.099669	24.961575
158.841654	5507.881644	24.966592
159.407246	5516.063577	24.971610
159.581661	5524.410161	24.976627
159.927752	5522.712249	24.981645
159.935543	5529.754192	24.986663
160.242338	5534.627339	24.991680
160.533412	5534.986155	24.996698
160.921292	5534.034517	25.001715
161.162510	5528.631124	25.006733
161.019870	5533.235256	25.011751
161.781207	5525.719077	25.016768
161.759355	5537.022164	25.021786
161.779169	5530.774464	25.026803
162.254127	5514.920937	25.031821
162.179090	5513.183956	25.036839
162.572608	5509.855383	25.041856
162.765163	5509.201602	25.046874
162.454327	5513.643720	25.051891
162.467860	5511.985456	25.056909
162.726963	5517.675785	25.061927
162.529955	5522.117853	25.066944
162.872241	5508.948694	25.071962
162.736667	5509.004966	25.076979
162.986527	5508.991131	25.081997
162.747530	5535.165698	25.087015
162.734657	5551.343756	25.092032
163.025265	5541.329885	25.097050
162.981512	5567.337268	25.102067
163.259225	5585.487100	25.107085
163.498396	5594.278941	25.112103
163.705350	5606.304049	25.117120
163.896951	5620.648661	25.122138
163.879565	5632.576594	25.127155
164.257545	5639.247219	25.132173
164.462044	5636.515232	25.137191
164.912033	5651.116865	25.142208
165.177184	5667.363232	25.147226
165.029607	5675.745504	25.152243
165.258675	5677.675175	25.157261
165.721754	5677.374791	25.162279
165.646166	5691.252240	25.167296
165.894079	5694.196997	25.172314
165.848500	5704.491414	25.177331
166.105280	5700.161003	25.182349
166.000628	5716.187864	25.187367
166.147367	5730.755313	25.192384
166.450755	5729.724294	25.197402
166.556170	5757.627182	25.202419
166.459617	5750.295663	25.207437
166.808551	5766.492590	25.212455
167.019386	5784.965680	25.217472
167.037278	5785.326360	25.222490
167.183704	5811.457272	25.227507
167.515646	5817.675837	25.232525
167.942290	5829.474913	25.237543
168.000872	5847.029002	25.242560
168.216660	5846.913598	25.247578
168.438688	5858.286624	25.252595
168.708672	5858.596885	25.257613
169.143324	5869.355373	25.262631
169.225792	5875.360392	25.267648
169.714051	5870.192078	25.272666
169.464315	5880.590764	25.277683
169.667075	5873.113115	25.282701
169.673466	5877.350553	25.287719
169.865866	5892.962029	25.292736
169.935677	5895.969054	25.297754
170.371914	5903.101011	25.302771
170.570607	5895.627933	25.307789
170.638992	5899.564382	25.312807
170.585785	5923.879158	25.317824
171.032636	5927.250943	25.322842
171.011412	5936.368534	25.327859
171.272479	5935.414275	25.332877
171.527237	5926.771728	25.337895
171.313287	5950.702258	25.342912
171.765484	5957.066936	25.347930
171.652263	5963.896275	25.352947
171.684866	5966.608693	25.357965
172.105397	5976.601602	25.362983
172.120054	5981.865303	25.368000
172.561960	5987.810701	25.373018
172.211432	5993.220748	25.378035
172.612451	6013.068228	25.383053
172.826311	6022.044536	25.388071
172.711368	6033.945858	25.393088
173.331286	6042.449093	25.398106
173.586773	6053.652495	25.403123
173.257328	6057.915203	25.408141
173.579151	6070.865745	25.413159
173.712676	6084.522964	25.418176
174.242311	6081.986115	25.423194
174.082102	6089.781322	25.428211
174.280613	6109.697411	25.433229
174.587133	6116.269495	25.438247
174.344489	6120.836248	25.443264
174.809906	6140.450968	25.448282
175.177718	6147.790653	25.453299
176.540774	6116.994395	25.458317
177.118716	6105.347363	25.463335
177.252984	6106.798096	25.468352
177.531369	6088.245897	25.473370
177.166603	6077.017480	25.478387
177.417903	6073.630419	25.483405
177.594203	6061.908978	25.488423
177.444428	6067.442045	25.493440
177.431803	6057.370742	25.498458
177.561403	6062.196784	25.503475
177.390379	6062.964464	25.508493
177.606380	6057.619978	25.513511
177.457072	6068.605469	25.518528
177.779161	6063.918351	25.523546
177.778832	6070.945324	25.528563
178.001954	6093.006209	25.533581
178.280473	6096.431624	25.538599
177.894346	6102.779741	25.543616
178.074680	6113.284692	25.548634
178.396762	6132.019008	25.553651
178.249977	6130.556183	25.558669
178.572887	6152.967111	25.563687
178.508598	6171.890538	25.568704
178.985714	6186.121729	25.573722
178.573175	6200.451495	25.578739
179.116182	6224.501760	25.583757
179.589795	6240.347298	25.588775
179.665168	6270.665928	25.593792
179.715411	6272.526624	25.598810
179.901513	6282.920622	25.603827
179.989879	6309.569948	25.608845
180.398512	6317.916622	25.613863
180.574608	6332.383992	25.618880
180.967154	6346.628033	25.623898
181.545580	6360.150846	25.628915
181.355855	6364.603017	25.633933
181.865101	6362.203132	25.638951
181.673866	6365.246363	25.643968
182.033444	6372.771588	25.648986
182.020237	6388.221236	25.654003
182.356347	6390.646153	25.659021
182.530313	6397.256019	25.664039
182.587251	6411.153926	25.669056
183.357520	6417.397284	25.674074
183.033064	6422.688453	25.679092
182.793620	6432.240841	25.684109
183.380023	6442.313843	25.689127
183.571044	6441.567425	25.694144
183.509800	6453.410952	25.699162
184.167478	6468.850506	25.704180
183.899182	6475.294083	25.709197
184.297737	6481.680919	25.714215
184.484745	6499.336475	25.719232
184.823704	6498.686852	25.724250
184.713931	6503.971362	25.729268
185.042604	6532.460129	25.734285
186.201683	6529.947963	25.739303
186.189148	6523.434336	25.744320
186.017054	6527.037125	25.749338
186.385441	6522.465229	25.754356
186.406729	6526.311002	25.759373
186.586158	6523.418407	25.764391
186.390571	6534.277859	25.769408
186.505854	6534.936972	25.774426
186.456010	6547.988101	25.779444
186.873562	6560.102369	25.784461
187.536081	6575.624666	25.789479
187.382566	6580.647083	25.794496
187.419194	6589.589046	25.799514
187.803165	6584.821088	25.804532
188.017704	6597.735693	25.809549
188.665540	6594.852599	25.814567
188.302061	6605.036234	25.819584
188.449494	6596.413559	25.824602
188.719656	6600.212592	25.829620
188.771887	6626.175842	25.834637
188.901462	6628.592811	25.839655
189.087143	6640.876298	25.844672
189.310807	6654.754148	25.849690
189.653728	6655.512310	25.854708
189.563595	6661.837865	25.859725
189.962931	6683.085495	25.864743
190.145846	6697.098133	25.869760
190.127539	6687.007639	25.874778
190.526498	6702.668082	25.879796
190.380692	6716.951098	25.884813
190.942345	6726.378320	25.889831
191.059247	6725.822316	25.894848
190.858127	6749.984199	25.899866
191.311010	6748.018131	25.904884
191.340157	6755.975485	25.909901
192.046416	6763.171824	25.914919
192.322399	6771.716941	25.919936
192.743996	6776.498239	25.924954
192.762387	6769.948100	25.929972
192.574197	6773.284417	25.934989
192.932824	6763.811242	25.940007
193.035529	6768.749599	25.945024
193.179770	6793.312071	25.950042
193.404921	6797.553451	25.955060
193.308477	6814.669167	25.960077
193.401185	6811.344206	25.965095
193.503972	6833.408854	25.970112
193.653101	6834.547277	25.975130
194.007594	6851.058455	25.980148
193.892268	6869.673810	25.985165
194.305870	6886.576893	25.990183
194.663364	6896.080048	25.995200
194.746993	6902.814700	26.000218
195.247540	6921.065983	26.005236
195.108882	6931.905239	26.010253
195.549494	6931.303129	26.015271
195.743737	6945.414912	26.020288
195.836234	6960.894727	26.025306
196.056429	6955.402114	26.030324
196.203126	6991.034627	26.035341
196.458365	6990.360565	26.040359
196.818335	7004.746559	26.045376
196.846541	7027.685768	26.050394
196.962903	7026.723039	26.055412
196.865193	7046.985039	26.060429
197.104974	7052.483118	26.065447
197.412434	7071.266591	26.070464
197.662713	7091.665166	26.075482
197.971974	7092.935451	26.080500
198.028170	7115.362027	26.085517
198.428678	7122.552207	26.090535
198.387710	7127.076884	26.095552
198.580332	7154.742668	26.100570
199.040135	7164.512167	26.105588
199.564580	7174.922096	26.110605
199.596696	7178.383899	26.115623
199.495480	7190.401196	26.120640
199.808883	7195.259681	26.125658
200.166198	7206.289566	26.130676
199.997310	7223.491263	26.135693
200.238483	7221.959398	26.140711
200.861604	7235.667097	26.145728
201.115995	7247.382250	26.150746
201.181824	7245.357436	26.155764
201.294585	7267.108753	26.160781
201.385277	7275.470461	26.165799
201.719391	7276.067183	26.170816
201.622882	7284.646012	26.175834
202.150890	7293.369214	26.180852
202.127738	7311.564405	26.185869
202.385075	7313.890301	26.190887
202.442683	7323.091385	26.195904
202.473719	7346.674287	26.200922
202.966824	7342.976141	26.205940
202.852518	7364.964450	26.210957
203.483333	7367.033312	26.215975
203.362301	7378.263120	26.220992
203.766549	7394.599370	26.226010
204.223640	7401.111043	26.231028
204.393839	7398.687152	26.236045
204.700119	7419.284194	26.241063
204.716423	7424.524537	26.246080
204.839098	7436.189232	26.251098
205.027534	7438.172042	26.256116
205.178678	7449.832209	26.261133
205.444988	7460.753253	26.266151
205.436924	7461.015818	26.271168
205.523497	7489.180694	26.276186
206.066087	7499.247244	26.281204
206.094349	7514.712695	26.286221
206.121080	7532.498110	26.291239
206.350781	7538.506298	26.296256
206.690526	7562.629697	26.301274
206.703175	7563.548364	26.306292
207.142238	7580.140510	26.311309
207.033911	7589.367424	26.316327
206.998544	7602.656378	26.321344
207.008208	7626.583061	26.326362
207.922534	7646.453195	26.331380
207.938052	7662.743907	26.336397
208.371559	7680.366291	26.341415
208.700085	7684.526137	26.346432
208.715767	7693.173085	26.351450
209.308969	7707.910514	26.356468
209.729586	7714.262108	26.361485
209.532642	7713.571183	26.366503
209.721024	7732.899326	26.371520
209.954807	7752.450028	26.376538
210.350094	7752.819052	26.381556
210.616826	7766.813042	26.386573
210.260068	7786.440617	26.391591
210.339745	7776.997112	26.396608
210.928199	7810.030531	26.401626
211.227971	7813.402600	26.406644
211.285122	7828.230324	26.411661
211.651579	7845.174671	26.416679
211.784124	7850.520567	26.421696
211.840985	7873.184243	26.426714
212.308332	7882.686258	26.431732
212.457018	7886.991684	26.436749
212.152234	7901.805178	26.441767
212.731231	7912.209292	26.446784
212.970161	7930.132109	26.451802
213.030237	7941.762719	26.456820
213.076842	7950.388755	26.461837
213.214149	7969.472753	26.466855
213.628898	7979.804736	26.471872
213.672378	8001.792040	26.476890
214.128500	8012.290961	26.481908
214.240989	8018.452196	26.486925
214.481683	8036.171445	26.491943
214.908512	8052.854989	26.496960
214.861912	8060.976986	26.501978
215.118152	8078.558854	26.506996
215.701402	8092.398428	26.512013
215.894062	8106.492679	26.517031
215.990064	8109.290203	26.522048
215.904002	8116.814966	26.527066
216.136418	8129.827989	26.532084
216.384500	8143.754091	26.537101
216.460280	8175.960778	26.542119
216.680098	8167.392548	26.547136
216.846841	8193.645196	26.552154
217.016394	8200.849112	26.557172
217.505950	8222.329683	26.562189
217.789907	8231.199365	26.567207
218.521928	8239.018708	26.572224
218.303026	8260.485971	26.577242
218.851250	8260.864862	26.582260
219.095489	8271.995404	26.587277
219.197720	8291.239246	26.592295
219.425215	8290.766282	26.597312
219.688127	8295.789775	26.602330
220.227018	8305.389251	26.607348
220.313967	8321.909303	26.612365
220.501490	8321.613077	26.617383
220.794528	8317.966264	26.622400
220.751284	8333.325923	26.627418
221.197915	8348.382841	26.632436
221.526088	8350.660627	26.637453
221.248869	8364.349612	26.642471
221.709122	8366.163704	26.647488
221.569444	8383.438406	26.652506
221.948580	8393.541460	26.657524
221.820538	8411.670902	26.662541
222.101174	8423.121933	26.667559
222.418725	8424.244256	26.672576
222.588470	8454.586906	26.677594
222.641703	8464.267839	26.682612
223.066555	8474.126402	26.687629
223.066971	8494.817363	26.692647
223.488832	8499.349728	26.697664
223.282962	8522.011807	26.702682
223.598246	8541.362473	26.707700
224.065503	8553.530649	26.712717
224.248590	8583.380390	26.717735
224.732153	8584.403865	26.722752
224.986096	8596.868522	26.727770
225.198434	8614.445822	26.732788
225.378986	8623.491182	26.737805
225.343686	8609.556758	26.742823
225.836584	8618.625509	26.747840
225.862188	8633.197799	26.752858
226.312563	8642.608576	26.757876
226.392942	8654.300245	26.762893
226.620675	8669.508061	26.767911
226.903117	8672.077270	26.772928
227.600948	8694.800548	26.777946
227.532499	8699.046390	26.782964
227.868458	8692.015907	26.787981
227.690968	8714.806351	26.792999
228.092391	8723.213376	26.798016
228.541501	8727.159135	26.803034
228.749329	8750.346601	26.808052
228.997691	8752.791412	26.813069
228.886542	8771.200319	26.818087
229.328080	8779.226792	26.823104
229.236587	8786.339611	26.828122
229.570745	8790.673573	26.833140
229.980639	8812.138577	26.838157
230.096907	8828.617921	26.843175
230.297887	8831.370910	26.848192
230.314610	8854.469779	26.853210
230.746497	8859.871017	26.858228
230.930516	8874.766511	26.863245
231.006527	8896.778273	26.868263
231.338178	8906.150696	26.873280
231.436063	8915.974716	26.878298
231.356594	8940.611006	26.883316
232.267574	8952.254314	26.888333
232.187043	8971.104784	26.893351
232.360034	8976.828276	26.898368
232.525831	8998.383608	26.903386
232.806675	9024.346059	26.908404
233.110899	9039.537336	26.913421
233.249100	9052.371411	26.918439
233.779663	9064.814005	26.923456
234.379702	9086.622108	26.928474
233.909213	9100.985513	26.933492
234.551309	9103.444741	26.938509
235.087078	9120.334037	26.943527
235.003819	9119.895634	26.948544
235.228304	9135.117426	26.953562
235.058027	9156.825322	26.958580
235.689366	9159.568793	26.963597
235.342214	9190.426188	26.968615
235.727110	9201.724660	26.973632
235.898802	9221.749914	26.978650
236.209707	9241.620793	26.983668
236.650223	9250.000243	26.988685
236.668006	9271.496144	26.993703
236.925657	9285.774346	26.998720
237.073903	9304.349528	27.003738
237.044664	9319.436458	27.008756
237.780007	9328.549235	27.013773
237.963372	9353.080165	27.018791
238.559039	9358.122983	27.023808
238.505967	9383.435338	27.028826
238.529625	9392.332646	27.033844
239.464063	9399.325108	27.038861
239.690677	9418.730392	27.043879
239.847131	9424.873000	27.048896
239.914997	9429.651741	27.053914
240.102549	9447.227280	27.058932
240.631430	9448.702404	27.063949
240.564351	9461.340541	27.068967
240.807315	9477.545028	27.073984
241.350630	9483.040484	27.079002
241.301595	9489.909594	27.084020
241.631912	9502.575709	27.089037
241.467716	9518.755428	27.094055
241.821814	9529.288606	27.099072
241.854229	9550.187616	27.104090
242.014244	9565.730979	27.109108
242.621501	9569.881949	27.114125
242.735029	9601.009480	27.119143
242.813608	9617.910438	27.124160
243.217028	9637.537689	27.129178
243.086550	9652.550194	27.134196
243.350480	9662.883778	27.139213
243.456366	9682.785562	27.144231
244.185207	9714.747432	27.149248
244.346321	9729.248029	27.154266
244.602803	9751.485292	27.159284
244.933232	9762.145964	27.164301
244.890141	9780.345358	27.169319
244.885580	9808.578304	27.174336
245.485213	9816.290524	27.179354
246.122856	9849.621242	27.184372
246.342285	9860.206811	27.189389
246.617281	9882.750607	27.194407
246.702727	9887.402346	27.199424
246.882352	9905.292908	27.204442
246.788678	9923.706733	27.209460
247.425824	9942.390503	27.214477
247.621362	9962.676982	27.219495
247.707568	9982.202963	27.224512
248.167489	9996.372867	27.229530
248.118964	10019.106554	27.234548
248.693607	10028.338638	27.239565
249.016778	10051.860731	27.244583
249.101054	10060.136480	27.249600
249.836576	10075.860939	27.254618
250.166545	10079.842581	27.259636
250.352986	10078.785070	27.264653
250.736115	10096.526551	27.269671
251.230409	10102.394830	27.274688
251.665815	10106.269167	27.279706
251.538912	10107.222827	27.284724
251.805285	10108.333768	27.289741
251.977073	10104.209649	27.294759
251.766988	10111.005943	27.299776
252.291504	10133.958937	27.304794
252.276004	10143.634987	27.309812
252.342940	10141.820134	27.314829
252.546471	10162.334235	27.319847
252.539695	10177.900488	27.324864
252.870670	10198.859055	27.329882
252.970506	10209.450161	27.334900
253.293216	10222.593257	27.339917
253.357767	10251.512524	27.344935
253.737337	10269.113901	27.349952
254.219836	10284.241427	27.354970
254.149434	10321.010810	27.359988
254.833398	10329.219845	27.365005
255.603557	10320.868432	27.370023
256.052924	10341.209797	27.375040
256.894225	10338.492339	27.380058
257.387539	10334.785972	27.385076
257.566819	10335.348094	27.390093
257.614056	10333.181411	27.395111
257.802928	10331.537559	27.400128
258.066515	10328.258174	27.405146
258.027968	10334.636863	27.410164
258.415254	10333.171125	27.415181
258.141296	10336.256273	27.420199
258.412094	10340.543731	27.425216
258.976593	10343.640047	27.430234
258.774703	10362.042141	27.435252
258.755566	10363.051438	27.440269
259.162774	10386.261986	27.445287
259.319834	10390.291342	27.450304
259.580087	10403.779629	27.455322
259.677755	10438.621846	27.460340
260.004556	10450.522366	27.465357
259.931271	10462.686179	27.470375
260.264768	10489.716275	27.475392
260.557708	10499.912805	27.480410
260.839405	10534.540958	27.485428
260.900658	10548.741482	27.490445
261.257439	10570.082492	27.495463
261.542357	10604.149137	27.500480
261.915637	10620.221539	27.505498
261.810893	10647.378436	27.510516
262.308599	10659.236927	27.515533
262.531478	10676.966466	27.520551
262.333421	10706.196842	27.525568
262.646148	10717.857015	27.530586
262.994067	10757.566097	27.535604
263.256092	10777.627819	27.540621
263.629856	10800.987577	27.545639
263.697398	10830.934570	27.550656
264.377708	10846.604498	27.555674
264.425492	10869.501986	27.560692
264.658697	10888.236369	27.565709
265.541706	10895.764282	27.570727
265.654382	10930.684338	27.575744
266.243516	10927.323815	27.580762
266.449417	10949.829456	27.585780
266.464342	10951.008876	27.590797
266.839829	10968.073771	27.595815
267.081054	10978.977773	27.600832
267.686376	10988.702983	27.605850
267.494627	11010.831346	27.610868
267.826603	11022.934949	27.615885
267.971562	11040.999241	27.620903
268.063168	11064.079917	27.625920
268.818975	11079.439169	27.630938
268.823916	11096.978249	27.635956
268.838578	11114.582897	27.640973
269.406460	11126.802065	27.645991
269.587373	11152.037783	27.651008
269.652708	11166.223676	27.656026
270.240467	11189.016690	27.661044
270.560953	11201.280468	27.666061
270.889286	11217.066702	27.671079
271.036307	11233.245871	27.676096
271.414160	11252.910986	27.681114
271.520351	11271.773524	27.686132
271.771560	11293.454296	27.691149
272.045410	11295.628455	27.696167
272.057274	11324.870638	27.701184
272.545944	11347.397521	27.706202
272.749380	11368.106108	27.711220
273.064613	11393.270052	27.716237
273.404094	11405.737773	27.721255
273.391518	11438.106206	27.726272
273.811127	11440.751439	27.731290
274.180130	11457.810051	27.736308
274.847269	11481.191003	27.741325
274.996475	11498.381505	27.746343
275.091239	11506.204591	27.751360
275.743543	11532.342773	27.756378
275.719363	11539.139587	27.761396
276.090378	11552.541197	27.766413
276.391743	11563.591288	27.771431
276.312305	11590.614200	27.776448
276.926589	11607.169506	27.781466
277.342931	11616.631662	27.786484
277.885731	11626.221248	27.791501
277.997036	11634.878044	27.796519
278.186782	11659.081129	27.801536
278.419874	11669.393264	27.806554
278.421777	11695.236733	27.811572
278.468742	11712.603947	27.816589
279.073490	11733.144977	27.821607
279.195742	11733.848475	27.826624
279.181100	11758.866470	27.831642
279.756662	11771.230749	27.836660
279.724802	11787.813285	27.841677
279.925872	11798.560957	27.846695
280.149225	11829.184423	27.851712
280.846921	11843.920697	27.856730
280.918050	11870.915190	27.861748
281.093534	11889.607867	27.866765
281.758672	11895.115108	27.871783
281.950022	11916.279545	27.876800
282.281655	11936.974380	27.881818
282.619135	11943.264099	27.886836
282.940124	11969.608740	27.891853
283.208977	11977.538327	27.896871
283.192002	12005.475886	27.901888
283.666207	12020.390814	27.906906
283.734148	12042.355711	27.911924
284.178264	12051.075602	27.916941
284.525106	12065.997297	27.921959
284.850741	12087.776556	27.926976
285.323417	12101.318888	27.931994
285.330354	12117.686818	27.937012
285.471262	12136.372127	27.942029
285.645644	12153.045373	27.947047
285.965125	12182.919065	27.952064
286.287331	12201.267598	27.957082
286.863268	12222.975672	27.962100
286.920828	12231.695293	27.967117
287.251036	12259.501042	27.972135
287.411943	12285.497864	27.977152
287.516263	12301.668055	27.982170
288.215677	12323.727132	27.987188
288.672314	12336.928062	27.992205
288.880591	12357.740736	27.997223
288.928473	12386.673030	28.002240
289.364130	12402.071478	28.007258
289.578653	12407.255592	28.012276
289.723112	12437.831463	28.017293
290.159639	12456.848855	28.022311
290.580000	12469.533618	28.027328
290.932136	12486.327077	28.032346
291.673567	12490.993727	28.037364
291.982368	12498.229857	28.042381
292.322705	12515.642931	28.047399
292.167674	12538.809827	28.052416
292.633857	12537.567850	28.057434
293.092638	12550.625761	28.062452
293.041937	12574.789127	28.067469
293.400213	12582.905893	28.072487
293.283204	12600.254208	28.077504
293.881104	12615.245449	28.082522
294.402654	12637.406142	28.087540
294.280714	12653.592107	28.092557
294.915085	12666.972213	28.097575
294.745371	12685.869068	28.102592
295.134454	12691.093546	28.107610
295.769752	12712.940845	28.112628
295.538420	12735.177005	28.117645
295.886651	12748.042045	28.122663
295.791845	12774.906273	28.127680
295.848442	12793.722226	28.132698
296.370165	12821.183423	28.137716
296.707739	12844.032682	28.142733
297.268375	12864.332458	28.147751
297.338227	12883.414729	28.152768
297.414106	12903.846525	28.157786
297.993830	12925.441947	28.162804
297.936995	12955.813810	28.167821
298.481130	12980.159502	28.172839
298.951697	13003.139529	28.177856
299.295149	13019.559585	28.182874
299.591158	13038.807421	28.187892
300.366467	13052.645181	28.192909
300.503886	13064.311394	28.197927
300.982559	13092.283923	28.202944
301.261377	13106.754756	28.207962
301.731688	13125.204681	28.212980
301.579608	13153.750052	28.217997
302.093646	13168.226822	28.223015
302.007641	13195.315319	28.228032
302.568312	13217.447599	28.233050
302.696558	13232.533098	28.238068
302.916230	13255.231343	28.243085
303.500413	13271.958874	28.248103
303.334940	13301.063185	28.253120
303.580124	13316.556188	28.258138
304.215498	13328.487138	28.263156
304.387096	13353.734687	28.268173
304.850861	13382.120539	28.273191
305.107078	13396.316563	28.278208
305.500036	13422.847079	28.283226
305.656678	13444.860079	28.288244
306.172471	13470.268456	28.293261
306.251365	13481.824565	28.298279
306.865469	13505.653197	28.303296
306.787678	13528.925096	28.308314
307.345716	13551.379554	28.313332
307.476505	13579.267909	28.318349
307.966663	13593.580531	28.323367
308.700451	13624.773918	28.328384
308.824260	13630.559465	28.333402
308.995524	13654.473472	28.338420
309.324185	13672.998297	28.343437
309.467470	13696.140360	28.348455
309.907990	13721.541866	28.353472
309.851770	13739.877783	28.358490
310.122572	13765.906944	28.363508
310.406212	13786.667640	28.368525
310.868765	13811.373639	28.373543
310.990047	13832.090507	28.378560
310.860271	13854.577982	28.383578
311.501965	13884.120561	28.388596
312.013407	13914.307226	28.393613
312.045306	13926.158073	28.398631
312.217991	13959.025822	28.403648
312.572900	13985.275162	28.408666
313.522314	14000.598864	28.413684
313.200541	14035.874346	28.418701
313.632649	14061.091975	28.423719
314.005016	14086.178846	28.428736
314.183030	14112.826490	28.433754
314.917185	14130.569009	28.438772
315.122435	14154.802911	28.443789
315.546481	14170.661984	28.448807
315.635077	14205.760866	28.453824
315.608909	14230.360926	28.458842
316.127060	14257.807766	28.463860
316.550934	14283.799046	28.468877
317.157737	14300.265598	28.473895
317.763622	14336.011801	28.478912
317.823276	14350.214454	28.483930
318.056825	14374.127825	28.488948
318.412522	14404.758988	28.493965
318.649444	14425.415620	28.498983
318.913590	14449.224155	28.504000
319.065953	14480.214477	28.509018
319.573377	14491.251476	28.514036
319.808600	14521.268740	28.519053
320.287012	14546.666464	28.524071
320.812380	14566.906429	28.529088
320.644212	14589.581671	28.534106
321.226581	14611.030668	28.539124
321.464385	14635.291533	28.544141
321.948538	14652.616131	28.549159
322.540402	14678.188966	28.554176
322.543584	14704.572252	28.559194
323.262957	14713.947905	28.564212
323.483591	14744.495878	28.569229
323.835130	14754.931164	28.574247
324.124397	14777.081112	28.579264
324.246488	14799.677341	28.584282
324.535029	14827.862351	28.589300
324.857480	14856.474606	28.594317
325.310814	14871.176411	28.599335
325.652711	14901.780949	28.604352
325.465001	14923.835699	28.609370
326.299578	14942.467424	28.614388
326.451400	14979.842821	28.619405
326.589522	15002.822845	28.624423
327.009836	15026.860789	28.629440
327.010474	15056.481817	28.634458
327.753003	15067.198056	28.639476
328.010287	15100.200115	28.644493
328.236333	15122.561095	28.649511
328.627977	15137.625881	28.654528
328.681470	15174.740302	28.659546
329.422576	15190.710311	28.664564
329.841627	15210.509781	28.669581
330.011147	15234.027578	28.674599
330.682325	15255.432721	28.679616
331.047722	15259.703949	28.684634
331.627862	15273.500445	28.689652
331.707591	15289.983965	28.694669
332.208177	15303.438892	28.699687
332.644388	15326.239633	28.704704
332.518697	15341.892301	28.709722
333.039717	15356.461955	28.714740
333.209014	15371.690535	28.719757
333.290613	15390.893525	28.724775
333.994129	15406.500123	28.729792
333.941998	15430.345625	28.734810
334.059594	15456.068361	28.739828
334.227132	15487.533520	28.744845
334.415962	15511.406879	28.749863
335.099982	15533.125279	28.754880
334.993460	15572.772100	28.759898
335.786585	15597.561155	28.764916
335.889876	15627.073331	28.769933
336.144545	15658.513538	28.774951
336.839471	15693.944525	28.779968
336.893236	15720.784224	28.784986
337.260720	15748.441381	28.790004
337.532838	15787.987670	28.795021
337.848593	15816.926655	28.800039
338.260807	15843.427392	28.805056
338.244779	15884.733023	28.810074
338.727719	15921.879808	28.815092
339.191080	15943.670367	28.820109
339.657586	15982.900777	28.825127
340.032391	16009.346745	28.830144
340.317893	16044.043087	28.835162
340.386565	16064.337044	28.840180
340.992809	16102.792226	28.845197
341.440280	16137.568074	28.850215
342.323660	16160.747957	28.855232
342.286886	16195.245825	28.860250
342.932175	16223.901193	28.865268
343.183201	16230.042903	28.870285
343.502455	16253.086665	28.875303
344.091038	16274.531785	28.880320
344.277357	16297.917241	28.885338
344.785733	16307.662315	28.890356
344.945186	16340.914391	28.895373
345.080303	16362.929096	28.900391
345.833807	16378.144699	28.905408
346.152514	16414.364399	28.910426
346.010824	16433.884560	28.915444
346.579410	16451.720035	28.920461
346.950528	16483.166197	28.925479
347.662855	16489.854725	28.930496
347.820838	16511.769352	28.935514
348.193908	16516.825279	28.940532
348.725982	16536.948971	28.945549
348.759036	16558.787125	28.950567
349.075270	16571.624956	28.955584
349.129953	16594.617106	28.960602
349.502839	16617.227701	28.965620
349.678808	16628.550446	28.970637
349.854888	16669.929520	28.975655
350.295660	16694.547969	28.980672
350.339805	16726.723458	28.985690
350.798023	16757.602397	28.990708
351.298340	16793.784597	28.995725
351.202696	16821.868444	29.000743
352.004469	16850.362646	29.005760
351.920615	16892.657505	29.010778
352.579589	16925.325947	29.015796
352.971188	16949.208386	29.020813
353.293431	16993.668612	29.025831
353.618295	17016.271302	29.030848
354.141611	17055.252284	29.035866
354.349876	17079.336967	29.040884
354.973327	17119.582807	29.045901
355.045058	17153.144096	29.050919
356.111810	17155.860253	29.055936
356.569292	17194.056437	29.060954
356.791412	17206.407646	29.065972
357.073773	17232.969256	29.070989
357.535760	17261.876621	29.076007
357.874660	17285.436886	29.081024
358.307217	17320.693348	29.086042
358.709992	17338.157465	29.091060
359.035592	17354.729986	29.096077
359.261353	17378.226139	29.101095
359.628845	17393.016872	29.106112
359.869574	17417.894920	29.111130
360.303187	17442.310391	29.116148
360.575112	17466.805602	29.121165
360.950790	17500.043227	29.126183
361.302371	17524.143952	29.131200
361.353141	17556.158688	29.136218
361.895356	17586.295197	29.141236
362.127890	17608.791025	29.146253
362.147186	17655.183687	29.151271
362.652875	17678.360493	29.156288
363.051459	17712.681926	29.161306
363.234858	17747.320402	29.166324
363.543135	17775.969754	29.171341
364.044816	17815.099796	29.176359
364.810904	17847.814928	29.181376
365.089731	17883.460554	29.186394
365.527566	17910.142643	29.191412
366.080754	17932.933517	29.196429
366.046000	17965.601707	29.201447
366.679610	17984.990820	29.206464
367.044503	18011.155170	29.211482
367.553128	18036.082072	29.216500
367.615163	18050.418161	29.221517
367.888916	18087.592652	29.226535
368.442185	18098.555555	29.231552
368.382349	18130.975720	29.236570
369.036171	18153.689858	29.241588
370.059260	18167.212659	29.246605
370.361202	18201.167096	29.251623
370.706405	18210.911230	29.256640
371.075626	18230.535701	29.261658
371.158878	18249.743151	29.266676
371.676055	18272.225685	29.271693
372.021332	18292.968654	29.276711
372.366478	18318.228763	29.281728
372.880444	18338.797664	29.286746
372.909586	18365.959455	29.291764
373.429721	18395.691983	29.296781
373.561403	18422.343812	29.301799
373.575036	18451.411455	29.306816
374.106661	18477.312610	29.311834
374.390696	18516.204281	29.316852
374.948381	18539.644181	29.321869
375.011990	18584.915957	29.326887
375.386396	18610.277001	29.331904
375.992884	18648.619562	29.336922
375.758913	18675.885633	29.341940
376.755694	18709.607616	29.346957
376.733348	18740.748586	29.351975
377.529577	18768.631813	29.356992
378.087018	18789.993253	29.362010
378.680197	18834.332099	29.367028
379.043278	18863.911007	29.372045
379.212283	18893.251585	29.377063
379.729565	18915.624789	29.382080
380.219105	18942.399237	29.387098
380.449306	18972.801555	29.392116
380.770089	18997.376042	29.397133
381.174082	19042.716569	29.402151
381.371755	19070.579562	29.407168
382.173674	19096.672950	29.412186
382.203583	19133.166678	29.417204
382.579166	19148.137732	29.422221
382.862235	19189.141658	29.427239
383.197527	19216.420726	29.432256
384.196818	19236.555180	29.437274
384.539795	19265.770302	29.442292
385.560679	19290.840448	29.447309
385.555379	19309.727846	29.452327
385.796007	19325.581290	29.457344
386.093649	19341.429997	29.462362
386.209150	19374.727650	29.467380
386.752905	19394.669907	29.472397
386.958975	19425.250197	29.477415
387.074669	19443.448326	29.482432
387.297145	19472.618068	29.487450
387.504873	19500.686153	29.492468
388.160943	19525.696684	29.497485
388.252193	19562.421823	29.502503
388.418538	19601.982662	29.507520
388.962697	19634.902292	29.512538
389.293808	19670.393651	29.517556
390.091414	19703.095853	29.522573
389.996308	19736.499888	29.527591
390.733087	19768.818564	29.532608
391.162901	19801.618557	29.537626
391.401747	19839.933244	29.542644
391.874179	19866.165866	29.547661
392.441526	19912.104227	29.552679
392.661298	19941.683203	29.557696
393.171973	19969.831828	29.562714
393.559736	20000.952480	29.567732
393.674532	20040.883715	29.572749
393.921764	20083.158868	29.577767
394.581115	20111.886904	29.582784
395.276401	20139.239374	29.587802
395.363529	20195.177462	29.592820
395.902116	20217.457392	29.597837
396.252608	20255.080786	29.602855
396.777091	20285.161945	29.607872
397.266124	20317.123921	29.612890
397.380386	20351.698855	29.617908
397.811385	20382.122709	29.622925
398.197331	20428.977069	29.627943
398.230031	20463.720390	29.632960
399.025279	20503.784185	29.637978
398.880519	20550.090284	29.642996
399.744953	20577.276385	29.648013
400.084599	20630.116178	29.653031
400.428259	20661.449141	29.658048
400.840542	20696.180534	29.663066
401.162294	20737.878144	29.668084
401.700780	20777.010922	29.673101
402.336229	20818.566619	29.678119
402.892992	20848.526369	29.683136
403.359402	20876.542702	29.688154
403.684676	20905.510893	29.693172
404.266052	20931.510179	29.698189
404.976525	20961.233012	29.703207
405.126808	20988.758071	29.708224
405.672779	21023.364140	29.713242
405.949837	21051.343224	29.718260
406.230001	21084.490676	29.723277
406.189811	21116.130639	29.728295
406.932951	21158.702582	29.733312
406.896952	21186.462436	29.738330
407.468815	21231.217455	29.743348
407.801962	21261.847620	29.748365
408.346486	21304.216904	29.753383
408.611962	21339.263724	29.758400
409.219885	21359.015543	29.763418
409.520045	21393.349708	29.768436
409.903276	21425.861627	29.773453
410.678395	21455.189965	29.778471
410.867690	21479.158433	29.783488
411.134424	21513.540715	29.788506
411.857950	21542.059129	29.793524
412.333055	21560.038230	29.798541
412.711716	21588.379336	29.803559
413.108719	21621.021779	29.808576
413.772778	21644.619507	29.813594
413.960721	21669.409155	29.818612
414.440840	21705.107012	29.823629
415.049400	21725.170292	29.828647
415.420029	21755.201594	29.833664
415.882087	21782.476737	29.838682
416.095529	21812.455219	29.843700
416.379297	21832.155317	29.848717
416.968249	21859.106359	29.853735
417.199925	21900.340954	29.858752
417.536398	21933.378041	29.863770
417.769975	21967.414532	29.868788
418.143591	21999.104534	29.873805
418.428697	22042.703282	29.878823
418.532446	22070.406978	29.883840
419.215445	22112.872151	29.888858
419.664797	22162.506584	29.893876
419.791711	22188.438584	29.898893
420.551158	22233.580061	29.903911
420.323446	22287.045868	29.908928
421.254056	22322.192102	29.913946
421.523241	22370.176664	29.918964
422.160522	22417.132356	29.923981
422.377001	22457.339020	29.928999
422.944601	22500.021316	29.934016
423.494131	22536.140829	29.939034
424.080878	22586.234373	29.944052
424.479507	22608.444685	29.949069
425.120686	22647.049834	29.954087
425.518407	22691.008918	29.959104
426.040802	22720.734318	29.964122
426.766568	22746.604900	29.969140
426.976657	22779.841898	29.974157
427.450012	22808.582047	29.979175
427.645392	22849.294014	29.984192
428.688846	22878.339651	29.989210
428.678984	22913.399955	29.994228
429.147502	22951.331550	29.999245
429.433854	22976.418692	30.004263
429.854747	23026.025706	30.009280
430.493830	23049.947733	30.014298
430.435316	23088.979715	30.019316
430.611514	23121.729747	30.024333
431.138516	23168.580785	30.029351
431.366358	23211.964232	30.034368
432.252135	23236.773543	30.039386
432.224974	23272.739283	30.044404
432.643428	23313.712278	30.049421
433.117673	23343.605629	30.054439
433.453910	23385.091297	30.059456
434.350021	23415.252336	30.064474
434.785084	23445.267912	30.069492
435.293981	23477.604911	30.074509
435.682048	23514.020977	30.079527
436.017092	23539.424203	30.084544
436.716507	23570.124149	30.089562
436.839130	23617.400123	30.094580
437.235478	23653.004650	30.099597
438.203025	23680.518395	30.104615
438.383546	23717.231084	30.109632
438.929159	23750.746702	30.114650
439.235265	23795.936498	30.119668
439.747006	23827.077233	30.124685
440.286736	23863.343904	30.129703
440.797751	23892.506165	30.134720
441.137451	23917.048287	30.139738
441.303447	23954.171081	30.144756
441.775112	24000.368557	30.149773
442.347781	24022.542094	30.154791
442.439541	24067.209893	30.159808
442.803834	24111.902930	30.164826
443.475351	24157.768901	30.169844
443.632652	24195.108688	30.174861
444.164298	24235.007320	30.179879
444.273592	24287.677805	30.184896
444.860190	24333.208846	30.189914
445.346050	24379.524105	30.194932
445.868491	24424.121923	30.199949
446.640557	24464.582293	30.204967
446.677186	24506.983546	30.209984
447.292359	24545.038942	30.215002
447.770080	24593.825685	30.220020
448.250329	24640.017342	30.225037
448.762830	24680.558999	30.230055
448.833470	24724.518299	30.235072
449.257549	24764.462175	30.240090
450.049382	24815.745563	30.245108
450.398508	24868.641285	30.250125
450.878396	24907.988173	30.255143
451.457593	24943.174933	30.260160
452.064317	24984.808365	30.265178
452.604329	25028.136774	30.270196
452.895556	25062.589788	30.275213
454.128794	25095.774959	30.280231
454.444079	25136.376763	30.285248
454.868380	25165.519716	30.290266
455.413758	25189.005349	30.295284
455.642944	25219.930703	30.300301
456.433548	25243.504968	30.305319
456.377413	25280.156536	30.310336
456.690439	25308.757369	30.315354
457.135101	25341.633041	30.320372
457.442293	25377.222530	30.325389
458.116866	25408.701215	30.330407
458.287334	25447.110844	30.335424
458.742998	25483.079472	30.340442
459.015269	25520.964937	30.345460
459.520410	25567.784748	30.350477
460.139538	25599.944627	30.355495
460.381043	25646.171706	30.360512
460.981845	25686.349700	30.365530
461.158696	25722.501934	30.370548
461.549505	25758.593379	30.375565
462.321561	25786.248265	30.380583
462.553922	25845.721892	30.385600
463.085801	25887.242757	30.390618
463.815823	25923.037100	30.395636
464.044211	25974.951248	30.400653
464.216410	26020.630312	30.405671
464.895997	26062.470009	30.410688
465.288927	26104.624915	30.415706
465.680104	26158.699126	30.420724
466.148169	26208.642536	30.425741
466.685208	26243.604097	30.430759
467.218293	26299.994435	30.435776
467.670661	26337.920887	30.440794
468.814785	26381.012537	30.445812
468.721304	26425.469817	30.450829
469.397376	26457.237881	30.455847
469.968837	26497.483241	30.460864
470.599755	26547.050383	30.465882
470.928409	26583.514410	30.470900
471.420125	26621.113823	30.475917
471.975198	26669.534509	30.480935
472.166154	26710.273543	30.485952
472.712600	26747.691206	30.490970
473.815621	26780.272708	30.495988
474.279021	26820.043682	30.501005
474.743649	26847.461021	30.506023
475.303594	26880.494804	30.511040
475.658154	26911.686277	30.516058
476.221142	26946.906801	30.521076
476.395427	26988.835708	30.526093
477.184129	27016.723272	30.531111
477.145688	27057.428818	30.536128
478.033773	27093.425130	30.541146
478.106556	27123.057806	30.546164
478.224089	27173.180589	30.551181
478.773325	27207.028252	30.556199
478.724460	27261.058865	30.561216
479.214542	27307.356683	30.566234
479.868917	27367.761414	30.571252
480.097287	27412.960377	30.576269
480.751889	27467.472101	30.581287
481.483590	27517.550112	30.586304
481.988148	27567.246881	30.591322
482.479751	27596.441822	30.596340
482.681437	27640.708083	30.601357
483.512304	27678.864185	30.606375
483.870341	27727.669256	30.611392
484.294467	27767.726159	30.616410
484.828412	27803.789926	30.621428
485.099786	27852.385414	30.626445
485.660760	27899.986278	30.631463
486.161652	27941.679678	30.636480
486.464278	27990.475457	30.641498
487.412794	28033.188251	30.646516
487.402982	28084.237081	30.651533
487.915466	28144.809139	30.656551
488.384033	28182.390658	30.661568
489.032296	28231.752983	30.666586
489.563203	28275.538327	30.671604
489.785525	28326.842471	30.676621
490.910808	28374.083788	30.681639
491.261488	28421.101947	30.686656
491.358839	28461.690103	30.691674
492.484678	28508.109122	30.696692
492.856440	28564.565360	30.701709
493.556271	28600.052918	30.706727
494.538224	28640.350898	30.711744
495.004428	28676.610200	30.716762
495.815344	28701.890627	30.721780
496.131593	28740.580337	30.726797
496.739882	28764.117112	30.731815
497.080581	28800.347829	30.736832
497.475761	28833.076182	30.741850
498.247436	28859.169966	30.746868
498.242640	28905.092590	30.751885
498.952606	28930.825982	30.756903
499.277607	28970.471421	30.761920
499.904469	29009.118594	30.766938
500.682407	29038.095595	30.771956
500.726268	29093.047316	30.776973
501.122686	29125.153569	30.781991
501.556021	29168.022337	30.787008
501.722132	29223.013331	30.792026
502.247989	29254.152082	30.797044
502.415050	29304.617103	30.802061
503.338934	29349.631865	30.807079
503.716594	29405.231186	30.812096
504.249022	29448.040778	30.817114
504.965998	29487.907133	30.822132
505.074424	29538.908589	30.827149
506.222979	29577.648944	30.832167
506.697332	29626.330867	30.837184
507.118904	29664.818452	30.842202
507.674035	29705.366727	30.847220
508.209370	29749.974846	30.852237
508.436521	29787.223444	30.857255
508.704311	29827.129084	30.862272
509.297039	29872.481721	30.867290
509.819351	29915.215351	30.872308
509.773694	29971.174012	30.877325
510.396157	30012.861235	30.882343
510.930641	30053.834459	30.887360
511.536788	30109.133432	30.892378
512.186128	30146.550426	30.897396
512.960590	30191.408496	30.902413
513.494394	30235.282178	30.907431
513.924811	30276.461661	30.912448
514.382175	30328.078234	30.917466
515.165058	30367.608424	30.922484
515.321429	30421.331552	30.927501
515.935596	30453.394700	30.932519
516.232856	30498.085336	30.937536
516.540928	30558.509793	30.942554
517.465829	30594.112422	30.947572
517.904232	30651.006557	30.952589
518.113030	30705.592256	30.957607
518.793815	30746.679454	30.962624
518.906368	30799.479334	30.967642
519.788288	30844.025773	30.972660
520.114834	30904.885140	30.977677
520.755810	30961.834770	30.982695
521.283330	31010.958379	30.987712
522.067595	31068.843831	30.992730
522.495735	31115.989799	30.997748
522.896790	31172.059498	31.002765
523.223255	31224.408996	31.007783
524.071805	31278.177556	31.012800
524.239129	31330.767095	31.017818
524.960756	31379.818332	31.022836
525.769108	31428.422462	31.027853
526.230489	31490.696813	31.032871
526.752708	31535.534120	31.037888
527.172178	31594.606482	31.042906
527.858868	31643.498574	31.047924
528.009758	31700.613939	31.052941
528.721207	31752.148806	31.057959
529.324840	31801.508536	31.062976
529.472958	31872.091854	31.067994
530.333296	31922.271657	31.073012
530.833293	31984.745054	31.078029
531.147486	32031.014934	31.083047
531.825489	32083.837621	31.088064
532.176770	32138.775784	31.093082
532.749472	32191.169518	31.098100
533.068116	32259.733411	31.103117
533.888587	32307.351487	31.108135
534.742391	32370.565987	31.113152
535.014428	32433.159353	31.118170
535.872480	32476.979491	31.123188
536.131771	32538.503437	31.128205
536.636952	32596.865877	31.133223
537.609506	32638.324310	31.138240
537.898531	32690.014508	31.143258
538.590194	32730.844846	31.148276
538.714299	32779.147385	31.153293
539.485233	32827.748993	31.158311
539.929386	32868.023257	31.163328
540.298310	32919.740854	31.168346
541.089219	32968.978092	31.173364
541.506288	33022.499504	31.178381
542.062410	33077.841642	31.183399
543.033829	33116.758877	31.188416
543.514316	33160.070342	31.193434
543.928913	33210.555200	31.198452
544.669226	33264.828256	31.203469
545.016306	33295.918029	31.208487
545.490865	33342.664153	31.213504
546.080953	33402.169781	31.218522
546.375888	33451.113858	31.223540
547.077118	33505.319838	31.228557
547.514987	33560.718678	31.233575
548.283770	33602.776320	31.238592
548.554291	33667.715474	31.243610
549.164303	33720.532149	31.248628
549.568015	33775.800001	31.253645
550.008236	33836.915310	31.258663
550.889572	33890.709227	31.263680
551.281627	33942.027499	31.268698
552.234420	33987.649396	31.273716
552.466694	34032.711479	31.278733
552.901103	34102.030675	31.283751
553.560580	34157.156593	31.288768
553.989198	34216.106006	31.293786
554.268941	34271.418895	31.298804
555.225902	34326.204779	31.303821
555.884029	34383.395199	31.308839
556.915117	34438.948404	31.313856
557.230878	34497.773332	31.318874
558.126165	34541.009720	31.323892
558.611674	34582.362997	31.328909
558.789384	34633.507870	31.333927
559.748240	34674.972009	31.338944
560.037179	34731.200879	31.343962
560.555482	34777.863669	31.348980
561.397448	34827.785630	31.353997
562.003171	34890.284654	31.359015
562.471762	34939.993686	31.364032
562.633811	34990.163150	31.369050
563.019566	35039.344936	31.374068
563.990165	35093.957760	31.379085
564.157278	35151.285769	31.384103
565.013881	35190.806310	31.389120
565.763997	35256.985343	31.394138
565.991204	35309.147555	31.399156
566.708793	35358.507601	31.404173
567.045393	35415.457957	31.409191
567.925105	35465.716343	31.414208
568.378667	35508.573129	31.419226
568.771166	35555.597082	31.424244
569.607843	35610.526161	31.429261
569.930292	35662.978579	31.434279
570.829984	35692.263221	31.439296
571.156901	35751.544829	31.444314
571.604988	35801.480404	31.449332
572.294560	35854.412559	31.454349
572.892513	35893.547131	31.459367
573.762820	35940.816113	31.464384
573.946111	35992.809293	31.469402
574.166271	36051.349050	31.474420
574.871730	36100.621775	31.479437
575.187501	36165.068374	31.484455
576.003049	36211.913278	31.489472
576.770617	36277.084537	31.494490
577.182946	36329.944101	31.499508
578.045435	36384.160554	31.504525
578.599888	36441.048163	31.509543
579.181010	36485.957236	31.514560
579.969568	36540.365703	31.519578
580.497514	36589.231406	31.524596
581.142098	36636.249773	31.529613
581.931295	36686.619261	31.534631
582.343891	36733.539254	31.539648
582.922437	36791.028066	31.544666
583.444993	36844.989544	31.549684
584.303625	36892.754986	31.554701
584.497133	36954.632044	31.559719
585.026097	37000.747491	31.564736
585.592304	37052.233608	31.569754
586.035236	37110.678503	31.574772
586.821805	37165.076695	31.579789
586.916446	37229.065924	31.584807
587.536347	37288.815560	31.589824
588.342416	37345.199448	31.594842
589.298184	37404.041429	31.599860
589.705915	37455.281244	31.604877
590.096020	37525.812066	31.609895
591.037692	37577.605792	31.614912
591.570663	37639.940583	31.619930
591.918123	37708.353521	31.624948
592.375756	37755.683867	31.629965
592.536684	37825.539747	31.634983
593.238325	37886.319135	31.640000
593.901563	37952.760705	31.645018
594.192541	38028.277789	31.650036
595.055231	38086.693899	31.655053
595.472472	38158.162792	31.660071
596.367499	38218.892079	31.665088
597.208946	38281.706753	31.670106
597.772781	38343.670249	31.675124
598.718725	38394.641134	31.680141
599.411151	38458.311172	31.685159
600.008366	38496.906334	31.690176
600.828400	38552.650264	31.695194
601.347047	38594.109049	31.700212
602.078192	38635.600322	31.705229
602.509735	38680.491749	31.710247
603.293584	38723.100701	31.715264
603.413580	38778.983661	31.720282
603.582411	38834.420665	31.725300
604.696975	38879.661134	31.730317
604.906697	38947.929129	31.735335
605.181425	39002.375319	31.740352
606.052275	39060.285738	31.745370
606.324278	39129.990530	31.750388
607.123531	39183.289381	31.755405
607.620330	39251.711564	31.760423
608.111107	39307.012108	31.765440
608.688567	39374.367000	31.770458
609.112855	39450.682851	31.775476
610.185295	39512.232157	31.780493
610.375226	39591.342392	31.785511
611.076733	39661.748919	31.790528
612.072535	39717.679988	31.795546
612.469129	39786.530275	31.800564
613.294076	39857.204953	31.805581
613.415158	39917.640942	31.810599
614.658496	39976.818219	31.815616
615.446050	40051.014678	31.820634
615.855686	40120.518671	31.825652
616.495569	40173.084325	31.830669
617.013615	40243.369500	31.835687
617.643945	40303.001924	31.840704
618.613639	40363.337468	31.845722
619.473544	40435.502380	31.850740
620.118102	40486.576419	31.855757
620.828612	40548.991372	31.860775
621.072966	40608.102833	31.865792
621.663363	40657.186359	31.870810
622.111500	40735.764009	31.875828
622.866802	40791.523998	31.880845
623.382549	40854.825828	31.885863
624.041179	40929.116015	31.890880
624.639465	40990.377131	31.895898
625.108048	41051.592884	31.900916
625.800155	41115.971529	31.905933
626.377935	41194.098520	31.910951
626.975057	41254.666857	31.915968
627.835837	41322.504738	31.920986
628.373466	41394.718699	31.926004
629.228447	41456.520969	31.931021
629.767064	41514.267092	31.936039
630.425418	41570.483483	31.941056
631.276801	41636.523057	31.946074
631.871010	41707.104905	31.951092
632.432497	41763.599152	31.956109
632.988948	41817.835952	31.961127
633.449458	41883.295250	31.966144
634.178607	41931.805179	31.971162
634.740366	41992.230342	31.976180
635.449144	42044.415404	31.981197
635.885486	42106.942765	31.986215
636.563325	42172.633515	31.991232
637.154917	42230.528166	31.996250
637.610580	42290.993350	32.001268
638.749057	42349.914796	32.006285
638.986147	42418.237985	32.011303
639.882680	42470.977997	32.016320
640.776654	42526.368247	32.021338
641.231289	42592.121372	32.026356
641.633539	42642.041738	32.031373
642.148837	42712.327981	32.036391
642.959376	42773.605808	32.041408
643.997108	42819.558188	32.046426
644.533297	42884.173309	32.051444
645.432706	42936.324407	32.056461
645.720092	42996.468713	32.061479
646.680116	43056.329471	32.066496
647.636257	43107.248121	32.071514
648.059733	43167.081137	32.076532
648.606008	43212.112847	32.081549
649.437860	43269.600493	32.086567
650.134866	43329.239100	32.091584
650.799096	43384.753858	32.096602
651.386663	43440.814117	32.101620
652.064344	43485.850851	32.106637
652.852556	43550.759558	32.111655
653.268670	43599.516447	32.116672
654.101496	43650.629834	32.121690
654.497411	43719.488070	32.126708
655.085428	43758.199075	32.131725
655.899559	43816.016280	32.136743
656.395134	43887.218956	32.141760
657.064446	43940.031177	32.146778
657.632255	44006.907315	32.151796
658.310481	44061.680672	32.156813
658.758419	44134.589145	32.161831
659.082367	44199.362837	32.166848
660.026851	44260.047291	32.171866
660.494258	44337.474175	32.176884
661.118148	44398.547711	32.181901
661.816399	44471.237919	32.186919
662.861260	44538.156865	32.191936
663.201479	44597.462294	32.196954
663.703228	44680.380798	32.201972
664.343015	44751.399997	32.206989
664.751745	44825.626834	32.212007
665.677350	44903.232502	32.217024
666.550138	44965.650196	32.222042
667.296377	45041.117682	32.227060
667.932376	45098.118863	32.232077
668.644242	45160.133819	32.237095
669.036660	45217.669484	32.242112
670.040587	45276.827376	32.247130
670.548654	45344.033641	32.252148
671.126387	45404.007528	32.257165
671.998878	45464.458403	32.262183
672.458356	45533.566073	32.267200
673.231795	45587.045013	32.272218
673.674528	45663.598325	32.277236
674.193588	45729.012314	32.282253
674.942902	45791.234927	32.287271
676.004526	45865.078274	32.292288
676.241849	45930.077245	32.297306
676.943411	45997.883052	32.302324
677.900494	46069.365038	32.307341
678.771389	46133.544545	32.312359
679.196510	46209.604550	32.317376
680.049214	46262.400910	32.322394
680.427858	46339.008388	32.327412
681.184395	46413.224435	32.332429
681.957105	46470.981310	32.337447
682.336255	46542.503604	32.342464
682.985715	46613.238545	32.347482
683.504289	46687.490482	32.352500
684.350176	46765.502020	32.357517
685.041884	46839.651310	32.362535
685.653312	46924.124760	32.367552
686.397990	46999.042457	32.372570
687.129924	47077.196571	32.377588
687.878194	47152.868440	32.382605
688.226302	47221.978393	32.387623
689.184124	47297.421896	32.392640
690.165527	47371.161292	32.397658
691.000263	47445.728939	32.402676
691.765383	47510.132246	32.407693
692.757977	47583.028291	32.412711
693.364989	47661.883269	32.417728
694.214562	47722.661095	32.422746
694.782944	47784.604036	32.427764
695.177006	47856.479521	32.432781
696.299873	47924.998729	32.437799
697.264072	47987.781791	32.442816
697.970814	48043.591696	32.447834
698.346721	48112.684927	32.452852
698.901757	48172.611913	32.457869
699.720247	48242.196844	32.462887
700.092961	48317.990292	32.467904
701.114934	48386.675657	32.472922
701.502669	48457.655292	32.477940
702.088682	48523.861005	32.482957
702.835624	48597.974169	32.487975
703.404612	48677.615966	32.492992
703.935360	48739.123313	32.498010
704.533554	48826.476289	32.503028
705.663046	48902.404187	32.508045
706.394615	48965.824145	32.513063
706.845175	49046.789681	32.518080
707.583036	49113.677103	32.523098
707.994363	49165.643621	32.528116
709.257540	49232.668747	32.533133
710.066207	49288.169717	32.538151
710.475427	49360.042563	32.543168
711.760852	49416.282175	32.548186
712.243845	49487.727251	32.553204
713.084483	49547.392512	32.558221
713.589487	49619.516228	32.563239
713.743788	49687.953462	32.568256
714.578779	49749.387465	32.573274
715.331185	49816.575000	32.578292
715.998998	49895.647956	32.583309
716.987665	49951.280122	32.588327
718.048459	50023.831368	32.593344
719.232890	50078.561790	32.598362
720.166341	50143.661049	32.603380
720.864236	50195.752201	32.608397
721.673084	50246.143826	32.613415
722.186233	50305.980526	32.618432
723.103842	50356.143711	32.623450
723.653036	50414.577030	32.628468
724.038108	50477.950234	32.633485
724.821162	50540.234669	32.638503
725.481070	50612.186253	32.643520
725.805483	50673.445941	32.648538
726.263148	50744.379361	32.653556
726.810609	50821.544198	32.658573
727.817679	50893.962360	32.663591
728.169395	50981.295688	32.668608
728.913859	51052.598089	32.673626
729.852579	51122.197219	32.678644
730.674960	51196.713124	32.683661
731.719175	51270.433445	32.688679
732.290865	51354.230482	32.693696
733.012057	51426.188197	32.698714
733.736045	51506.906733	32.703732
734.096489	51586.610470	32.708749
735.252839	51654.419133	32.713767
735.643891	51738.486572	32.718784
736.637809	51817.948467	32.723802
737.423944	51885.583392	32.728820
738.062823	51967.229636	32.733837
738.923431	52038.353342	32.738855
739.377765	52119.360567	32.743872
740.610534	52182.200854	32.748890
741.328288	52265.009955	32.753908
741.928407	52333.645098	32.758925
743.019844	52410.203078	32.763943
743.742931	52480.002751	32.768960
744.675752	52550.047048	32.773978
745.187655	52614.395462	32.778996
745.843514	52692.030794	32.784013
746.670754	52756.872380	32.789031
747.080452	52818.315156	32.794048
747.988252	52881.758793	32.799066
748.370558	52957.488271	32.804084
748.695398	53031.191438	32.809101
749.490365	53097.317658	32.814119
750.263799	53186.178959	32.819136
751.007298	53246.771516	32.824154
751.903252	53329.446653	32.829172
752.412818	53409.756477	32.834189
753.102076	53488.204230	32.839207
754.023663	53568.569108	32.844224
754.722457	53649.288599	32.849242
755.354682	53720.736191	32.854260
756.051440	53813.214173	32.859277
757.037790	53884.590257	32.864295
758.015843	53980.925609	32.869312
758.251469	54057.424775	32.874330
759.646114	54133.310490	32.879348
760.288937	54222.153460	32.884365
761.508248	54298.269787	32.889383
761.644460	54379.375620	32.894400
762.106696	54458.444486	32.899418
763.082444	54535.437044	32.904436
763.889048	54637.289155	32.909453
764.483650	54713.216259	32.914471
765.285223	54794.858799	32.919488
765.975058	54887.393836	32.924506
766.991047	54976.484106	32.929524
767.642118	55067.122809	32.934541
768.395459	55156.899711	32.939559
769.277423	55251.063224	32.944576
769.766201	55341.325070	32.949594
770.651626	55422.833957	32.954612
771.177391	55526.992731	32.959629
772.377667	55616.022057	32.964647
773.027708	55710.742546	32.969664
773.228133	55813.398478	32.974682
774.351534	55907.542715	32.979700
774.987966	56006.190716	32.984717
775.921625	56100.697605	32.989735
776.686017	56192.375034	32.994752
777.536288	56274.000627	32.999770
778.619197	56359.005225	33.004788
779.162847	56468.302621	33.009805
780.314553	56545.016761	33.014823
781.728928	56626.039561	33.019840
782.649637	56711.775587	33.024858
783.330257	56785.623509	33.029876
784.295132	56858.302625	33.034893
784.669414	56927.186720	33.039911
785.719171	57021.048474	33.044928
786.251045	57096.869142	33.049946
787.382274	57177.475369	33.054964
787.872456	57265.725979	33.059981
788.373141	57336.211004	33.064999
789.719302	57411.174089	33.070016
790.205992	57471.928853	33.075034
790.944659	57552.586574	33.080052
791.471036	57625.632110	33.085069
792.176824	57699.795384	33.090087
792.740277	57777.328088	33.095104
793.474941	57860.361892	33.100122
794.769213	57932.326664	33.105140
795.063942	58020.908749	33.110157
796.067832	58092.794080	33.115175
796.664798	58169.094973	33.120192
797.159448	58259.300705	33.125210
798.076795	58336.687862	33.130228
799.012814	58439.645409	33.135245
799.217002	58532.348659	33.140263
800.549165	58618.795229	33.145280
800.956750	58704.767391	33.150298
802.400274	58792.734608	33.155316
802.874883	58896.630047	33.160333
803.807117	58983.713430	33.165351
804.688923	59064.269690	33.170368
805.302938	59169.893593	33.175386
805.999279	59251.064278	33.180404
806.973561	59352.470546	33.185421
807.740056	59444.975169	33.190439
808.620590	59520.690248	33.195456
809.470766	59642.413302	33.200474
810.352454	59723.209228	33.205492
810.763689	59822.276476	33.210509
811.849683	59923.475461	33.215527
812.875380	60010.810826	33.220544
813.505629	60114.189387	33.225562
814.424452	60197.573718	33.230580
814.731365	60303.060292	33.235597
815.697920	60400.804479	33.240615
816.610800	60498.169343	33.245632
817.555378	60598.901912	33.250650
818.583629	60685.535886	33.255668
819.350866	60787.551238	33.260685
820.110078	60883.161691	33.265703
821.433840	60976.485092	33.270720
821.856060	61071.970156	33.275738
822.706575	61155.559071	33.280756
823.841231	61254.382957	33.285773
824.706367	61347.414906	33.290791
825.391425	61434.706907	33.295808
826.026662	61524.438660	33.300826
827.024844	61605.353613	33.305844
827.899670	61712.835464	33.310861
829.060054	61781.416577	33.315879
830.125166	61875.496090	33.320896
831.095146	61953.376117	33.325914
831.714829	62028.334437	33.330932
832.825961	62115.252314	33.335949
833.528539	62197.119978	33.340967
834.401073	62270.996945	33.345984
834.800552	62343.430576	33.351002
836.221778	62410.668282	33.356020
836.490778	62497.538787	33.361037
837.075716	62562.649110	33.366055
838.032771	62643.477162	33.371072
838.260237	62738.180591	33.376090
839.117735	62808.266265	33.381108
839.966285	62907.396964	33.386125
840.836032	63002.283702	33.391143
841.763131	63097.584952	33.396160
842.051080	63189.202001	33.401178
843.047293	63272.676033	33.406196
843.549408	63372.303249	33.411213
844.506745	63468.261565	33.416231
845.519921	63573.123430	33.421248
845.961364	63679.245337	33.426266
847.308742	63776.213709	33.431284
848.112860	63886.406637	33.436301
849.067451	63985.339747	33.441319
849.746429	64084.531984	33.446336
850.301323	64191.545062	33.451354
851.243202	64288.713214	33.456372
852.060475	64396.971050	33.461389
853.070966	64509.092786	33.466407
853.965363	64610.119952	33.471424
854.880458	64721.285388	33.476442
856.032704	64823.011666	33.481460
856.783984	64925.418152	33.486477
857.546149	65037.967811	33.491495
858.751271	65133.926642	33.496512
859.416067	65236.733864	33.501530
860.401118	65328.044928	33.506548
861.504259	65434.892422	33.511565
861.940336	65530.043910	33.516583
863.553359	65631.647456	33.521600
864.227955	65730.792055	33.526618
865.268808	65818.120164	33.531636
866.036646	65911.009862	33.536653
866.828795	66008.564295	33.541671
867.996827	66093.352988	33.546688
868.265013	66198.919456	33.551706
869.613641	66298.695634	33.556724
870.399538	66395.229671	33.561741
871.435342	66492.763570	33.566759
872.581122	66584.083440	33.571776
873.050070	66684.614354	33.576794
873.576825	66779.312218	33.581812
874.572366	66874.100189	33.586829
875.161146	66975.782216	33.591847
876.285512	67072.970138	33.596864
877.297956	67181.199936	33.601882
878.126684	67272.371357	33.606900
879.308247	67383.891940	33.611917
879.575971	67475.336790	33.616935
880.879628	67563.540663	33.621952
881.475864	67654.592942	33.626970
882.522699	67733.697193	33.631988
883.282062	67829.064397	33.637005
883.986119	67919.664855	33.642023
885.154249	68002.693007	33.647040
885.771922	68091.646508	33.652058
886.766096	68194.230666	33.657076
887.572171	68286.996160	33.662093
888.282637	68384.648200	33.667111
889.352918	68474.150551	33.672128
890.331055	68582.494691	33.677146
891.073232	68671.146727	33.682164
892.004746	68774.584165	33.687181
892.819771	68873.662460	33.692199
893.593015	68960.485025	33.697216
894.237898	69077.654067	33.702234
895.160566	69182.762984	33.707252
896.139904	69291.218264	33.712269
896.747896	69406.695622	33.717287
897.852262	69518.379695	33.722304
898.767433	69620.023571	33.727322
899.630321	69727.798494	33.732340
900.538241	69844.165773	33.737357
901.201718	69959.858689	33.742375
902.364942	70067.909911	33.747392
903.314970	70179.356938	33.752410
904.140073	70291.159340	33.757428
905.226968	70398.441062	33.762445
905.931203	70510.649358	33.767463
906.813008	70618.956889	33.772480
907.697273	70725.407020	33.777498
909.176945	70843.483647	33.782516
910.003558	70954.916785	33.787533
910.467548	71060.715293	33.792551
911.804493	71172.074770	33.797568
912.629166	71284.615816	33.802586
913.715954	71392.174654	33.807604
915.145906	71492.766896	33.812621
915.741830	71606.237094	33.817639
916.864166	71709.539541	33.822656
917.736928	71815.561379	33.827674
918.724169	71905.503281	33.832692
919.954601	72008.625799	33.837709
920.731836	72111.347052	33.842727
922.071603	72207.445634	33.847744
922.683875	72317.264997	33.852762
923.796664	72417.779701	33.857780
924.770288	72503.644458	33.862797
925.736165	72602.496313	33.867815
926.425751	72693.715025	33.872832
927.045788	72798.619618	33.877850
928.021970	72898.615049	33.882868
929.031383	73002.175987	33.887885
929.580197	73109.684380	33.892903
930.668430	73190.497507	33.897920
931.481349	73292.543020	33.902938
932.330072	73382.482039	33.907956
933.485801	73471.974502	33.912973
934.223755	73572.384046	33.917991
934.724764	73665.615135	33.923008
935.555052	73773.606812	33.928026
936.581843	73875.096760	33.933044
937.469331	73984.426500	33.938061
937.930351	74102.949974	33.943079
939.092414	74210.189754	33.948096
939.832640	74328.897638	33.953114
940.500041	74445.797777	33.958132
941.854065	74561.515018	33.963149
942.592115	74679.207860	33.968167
943.714992	74785.161418	33.973184
945.108555	74894.933801	33.978202
946.077938	75005.450485	33.983220
947.034282	75109.706958	33.988237
947.730477	75233.855860	33.993255
948.841344	75340.104957	33.998272
949.953107	75458.646624	34.003290
950.850267	75567.724304	34.008308
952.103787	75669.193545	34.013325
952.807611	75784.307098	34.018343
954.027818	75901.576432	34.023360
954.715189	76013.129415	34.028378
955.896342	76133.206086	34.033396
956.719459	76242.368700	34.038413
957.668111	76359.645968	34.043431
958.609807	76462.685631	34.048448
959.801442	76576.853884	34.053466
960.410317	76692.739800	34.058484
961.885198	76808.494917	34.063501
962.533372	76913.814629	34.068519
963.175782	77022.915378	34.073536
964.340763	77134.771429	34.078554
965.711935	77249.692302	34.083572
966.934795	77358.177902	34.088589
967.724844	77492.767088	34.093607
968.746258	77594.756912	34.098624
970.239707	77691.204855	34.103642
970.663573	77807.347754	34.108660
971.665989	77905.929027	34.113677
972.483931	78014.419325	34.118695
973.604820	78135.572935	34.123712
974.393007	78249.498697	34.128730
975.441444	78354.635738	34.133748
977.379572	78448.709427	34.138765
978.269772	78554.384652	34.143783
979.160731	78652.721774	34.148800
980.277934	78744.222093	34.153818
981.233584	78853.655696	34.158836
982.210398	78939.092167	34.163853
983.042630	79034.096674	34.168871
984.198450	79122.925082	34.173888
985.117960	79219.597948	34.178906
985.749463	79298.921515	34.183924
986.457752	79391.456889	34.188941
987.247436	79491.463935	34.193959
988.106156	79581.100118	34.198976
989.493173	79682.947336	34.203994
990.011566	79786.772715	34.209012
990.834623	79885.840822	34.214029
991.736166	79994.315614	34.219047
992.669335	80106.332197	34.224064
993.434119	80214.374763	34.229082
994.204070	80339.389968	34.234100
995.048999	80446.276824	34.239117
995.889406	80581.099431	34.244135
996.910879	80708.769786	34.249152
997.964501	80822.458912	34.254170
998.624133	80947.912549	34.259188
1000.118940	81076.938540	34.264205
1001.030687	81207.872397	34.269223
1001.958374	81335.125322	34.274240
1002.973775	81464.015038	34.279258
1003.855286	81601.739385	34.284276
1005.037385	81713.661809	34.289293
1005.835627	81859.783807	34.294311
1006.656932	81997.008266	34.299328
1007.967294	82132.240284	34.304346
1008.600476	82269.338407	34.309364
1010.122014	82405.784025	34.314381
1010.959772	82537.344890	34.319399
1012.272811	82665.492914	34.324416
1013.373675	82798.322233	34.329434
1014.056482	82937.155405	34.334452
1015.571582	83059.899854	34.339469
1016.467759	83189.805416	34.344487
1017.415759	83331.102609	34.349504
1018.852351	83453.817589	34.354522
1019.568960	83592.946855	34.359540
1020.449932	83717.414534	34.364557
1021.491886	83845.992213	34.369575
1022.966899	83970.088700	34.374592
1023.925014	84104.820412	34.379610
1024.702006	84243.033909	34.384628
1025.919257	84365.245338	34.389645
1026.591759	84497.483300	34.394663
1027.822011	84642.809812	34.399680
1029.090396	84761.379855	34.404698
1029.904104	84905.402397	34.409716
1030.879930	85033.846057	34.414733
1032.256785	85162.979118	34.419751
1033.409114	85295.619933	34.424768
1034.467148	85423.566009	34.429786
1035.539473	85554.058726	34.434804
1036.423437	85668.591385	34.439821
1037.526021	85789.849185	34.444839
1038.401811	85926.711104	34.449856
1039.349273	86031.264153	34.454874
1040.420122	86160.338116	34.459892
1041.226610	86270.769974	34.464909
1042.141734	86391.485598	34.469927
1043.136585	86522.262125	34.474944
1044.289213	86639.103165	34.479962
1044.929542	86770.639480	34.484980
1046.350244	86895.590017	34.489997
1047.177935	87024.809036	34.495015
1048.263585	87169.391648	34.500032
1049.757594	87278.214358	34.505050
1050.504348	87406.689731	34.510068
1051.504337	87535.365884	34.515085
1052.645645	87666.998727	34.520103
1053.565157	87795.461585	34.525120
1054.404910	87926.328229	34.530138
1055.407011	88072.321387	34.535156
1056.784670	88205.614668	34.540173
1057.937574	88344.560022	34.545191
1058.547753	88484.060553	34.550208
1059.862518	88618.428779	34.555226
1060.609299	88764.947829	34.560244
1061.622323	88903.153821	34.565261
1062.750155	89048.526459	34.570279
1064.085738	89198.559444	34.575296
1065.079706	89345.213836	34.580314
1065.879991	89494.448633	34.585332
1067.255621	89637.819001	34.590349
1068.565600	89771.518434	34.595367
1069.845082	89911.750131	34.600384
1071.360973	90033.712295	34.605402
1072.638994	90169.999550	34.610420
1073.825499	90297.960416	34.615437
1074.869828	90427.981090	34.620455
1075.912932	90556.149681	34.625472
1077.111681	90678.633891	34.630490
1077.830830	90816.943016	34.635508
1079.189689	90945.607568	34.640525
1080.025910	91087.062032	34.645543
1081.059572	91214.717357	34.650560
1082.229633	91337.323647	34.655578
1083.487604	91477.486566	34.660596
1084.365438	91615.490863	34.665613
1085.504542	91743.486667	34.670631
1086.444682	91879.541010	34.675648
1087.598171	92003.140307	34.680666
1088.451428	92158.576795	34.685684
1089.484309	92292.487450	34.690701
1090.576447	92417.895097	34.695719
1091.605569	92561.870959	34.700736
1092.771126	92700.759717	34.705754
1093.974211	92836.778125	34.710772
1094.975794	92971.652945	34.715789
1096.135054	93107.104396	34.720807
1097.151258	93234.122668	34.725824
1098.768206	93344.923177	34.730842
1099.722155	93476.962298	34.735860
1100.633680	93591.399383	34.740877
1101.966608	93703.897748	34.745895
1102.876244	93826.805926	34.750912
1104.227065	93943.869551	34.755930
1105.755950	94057.945183	34.760948
1106.944973	94163.966241	34.765965
1108.318099	94275.841206	34.770983
1109.067881	94391.604838	34.776000
1110.439681	94504.904398	34.781018
1110.654692	94630.565211	34.786036
1111.779763	94759.099309	34.791053
1113.121356	94879.743268	34.796071
1113.771510	95005.659585	34.801088
1115.134918	95132.993997	34.806106
1116.135876	95266.598653	34.811124
1116.767070	95410.099500	34.816141
1118.066337	95542.216072	34.821159
1118.572186	95690.122430	34.826176
1120.150403	95825.276995	34.831194
1120.853051	95978.442397	34.836212
1121.756140	96123.897214	34.841229
1123.326089	96270.398252	34.846247
1124.018941	96429.748794	34.851264
1125.259871	96579.011712	34.856282
1126.481418	96730.359999	34.861300
1127.514803	96885.098429	34.866317
1128.915156	97037.356605	34.871335
1129.687581	97189.133641	34.876352
1131.077736	97343.230109	34.881370
1132.142001	97505.230467	34.886388
1133.229867	97658.168801	34.891405
1134.886539	97801.331907	34.896423
1135.845424	97961.701061	34.901440
1136.810002	98116.560019	34.906458
1138.102559	98270.336636	34.911476
1139.232815	98436.704772	34.916493
1140.455798	98586.091242	34.921511
1141.596161	98745.247610	34.926528
1142.852917	98889.423801	34.931546
1144.419288	99049.824174	34.936564
1145.313086	99191.010460	34.941581
1146.711635	99347.554921	34.946599
1148.006001	99499.371824	34.951616
1148.912976	99641.115542	34.956634
1150.058751	99778.538781	34.961652
1151.089587	99928.141674	34.966669
1152.519982	100079.358674	34.971687
1153.528460	100228.732965	34.976704
1154.803559	100376.958570	34.981722
1155.725033	100530.328423	34.986740
1156.950304	100683.328292	34.991757
1158.318653	100823.765747	34.996775
1159.090886	100963.716728	35.001792
1160.226107	101091.829298	35.006810
1161.134289	101225.679652	35.011828
1162.219197	101377.915488	35.016845
1163.748973	101514.066753	35.021863
1164.384362	101664.648541	35.026880
1165.850670	101798.312193	35.031898
1166.883908	101954.413479	35.036916
1167.843158	102099.106206	35.041933
1169.084024	102239.838223	35.046951
1169.894262	102407.355128	35.051968
1171.026035	102563.191694	35.056986
1172.121460	102724.457992	35.062004
1173.530874	102883.631579	35.067021
1174.766556	103031.064016	35.072039
1175.467276	103195.731096	35.077056
1176.956506	103361.286422	35.082074
1178.257136	103523.968343	35.087092
1179.059344	103693.818056	35.092109
1180.095218	103847.963467	35.097127
1181.196551	104029.582582	35.102144
1182.210082	104204.572451	35.107162
1183.572613	104375.363124	35.112180
1184.699831	104546.369633	35.117197
1186.391718	104726.621872	35.122215
1187.468286	104909.846399	35.127232
1188.518312	105076.185992	35.132250
1189.618199	105249.562401	35.137268
1191.001916	105430.596742	35.142285
1192.448351	105599.199518	35.147303
1193.611283	105781.410763	35.152320
1194.973235	105942.099645	35.157338
1196.384765	106099.712307	35.162356
1198.181640	106261.454359	35.167373
1199.657613	106412.128866	35.172391
1200.943139	106574.473291	35.177408
1202.142382	106722.902716	35.182426
1203.781528	106880.364066	35.187444
1204.831477	107031.515242	35.192461
1206.497345	107169.652000	35.197479
1207.911772	107324.936845	35.202496
1209.282130	107460.710901	35.207514
1210.673559	107601.836777	35.212532
1211.444588	107743.517812	35.217549
1212.558186	107875.948943	35.222567
1213.385923	108021.141596	35.227584
1214.598572	108171.179077	35.232602
1216.021330	108317.709309	35.237620
1217.342078	108476.003847	35.242637
1217.988421	108609.203161	35.247655
1219.108515	108761.689472	35.252672
1220.383652	108919.595395	35.257690
1221.574974	109076.591563	35.262708
1222.991717	109231.116041	35.267725
1224.304177	109367.929015	35.272743
1225.226298	109507.482227	35.277760
1226.462131	109646.790139	35.282778
1227.636654	109782.133571	35.287796
1228.454097	109923.832558	35.292813
1229.890251	110068.940666	35.297831
1230.833665	110225.356971	35.302848
1231.526632	110374.351248	35.307866
1232.514797	110529.433111	35.312884
1233.495831	110707.133768	35.317901
1234.639431	110869.561051	35.322919
1235.867182	111032.438113	35.327936
1236.795464	111203.782778	35.332954
1238.152735	111376.642942	35.337972
1239.253158	111567.294767	35.342989
1240.658105	111740.004294	35.348007
1242.203721	111920.086332	35.353024
1243.343802	112099.151675	35.358042
1244.425343	112281.221840	35.363060
1245.730491	112459.276005	35.368077
1247.224075	112636.307615	35.373095
1248.722223	112823.221552	35.378112
1249.664825	113007.186578	35.383130
1251.117183	113176.568697	35.388148
1251.957740	113375.423038	35.393165
1253.609729	113543.003340	35.398183
1254.776432	113731.591053	35.403200
1255.904342	113920.585181	35.408218
1257.429827	114099.787161	35.413236
1258.955930	114282.427939	35.418253
1260.595812	114457.936090	35.423271
1261.693311	114640.293068	35.428288
1263.194556	114809.741723	35.433306
1265.127882	114964.992107	35.438324
1265.986087	115149.688937	35.443341
1267.559779	115309.461968	35.448359
1268.732618	115475.915719	35.453376
1270.683763	115636.599465	35.458394
1272.119540	115796.074594	35.463412
1273.494035	115957.105281	35.468429
1274.926082	116096.190057	35.473447
1275.915721	116247.723577	35.478464
1277.144966	116409.596946	35.483482
1278.942101	116548.493194	35.488500
1279.867410	116723.617754	35.493517
1281.234580	116867.300977	35.498535
1282.618839	117017.421399	35.503552
1283.866662	117166.779280	35.508570
1284.879732	117321.443196	35.513588
1286.036136	117480.745305	35.518605
1287.356715	117632.373699	35.523623
1288.590633	117785.479375	35.528640
1289.864825	117955.865107	35.533658
1291.092208	118112.696807	35.538676
1292.165180	118284.800938	35.543693
1293.203370	118439.410577	35.548711
1294.816884	118594.670515	35.553728
1295.747227	118736.261769	35.558746
1297.283833	118876.997595	35.563764
1298.562858	119022.802709	35.568781
1300.132463	119168.891716	35.573799
1301.067776	119316.684373	35.578816
1302.327835	119478.857047	35.583834
1303.751089	119610.642313	35.588852
1304.839242	119761.781880	35.593869
1305.796482	119923.011302	35.598887
1307.161366	120074.944541	35.603904
1308.407039	120252.796557	35.608922
1309.678279	120410.572312	35.613940
1310.658530	120578.007762	35.618957
1311.883203	120756.664405	35.623975
1313.365081	120922.831830	35.628992
1314.044969	121110.417534	35.634010
1315.450949	121279.765509	35.639028
1316.632509	121470.376961	35.644045
1318.049676	121648.299805	35.649063
1319.388424	121840.662069	35.654080
1320.692912	122021.569010	35.659098
1322.402379	122205.376533	35.664116
1323.436786	122393.459593	35.669133
1325.076720	122576.406814	35.674151
1326.601236	122759.006331	35.679168
1327.846314	122937.446466	35.684186
1329.500839	123112.668909	35.689204
1331.200218	123297.030209	35.694221
1332.006918	123485.929791	35.699239
1333.231422	123657.715653	35.704256
1334.442736	123841.423638	35.709274
1336.070227	124032.881857	35.714292
1337.222098	124223.416389	35.719309
1338.908871	124399.693434	35.724327
1340.890375	124566.386856	35.729344
1342.398618	124739.135191	35.734362
1343.822808	124913.709336	35.739380
1345.387294	125078.990197	35.744397
1346.758371	125259.503087	35.749415
1348.620913	125418.911880	35.754432
1350.033142	125578.773192	35.759450
1351.138686	125735.897422	35.764468
1352.207263	125903.668882	35.769485
1353.306155	126064.064202	35.774503
1355.135756	126221.937537	35.779520
1356.480465	126399.054670	35.784538
1357.719292	126566.296453	35.789556
1358.835908	126734.103388	35.794573
1359.853345	126903.003866	35.799591
1361.431074	127077.744842	35.804608
1362.515899	127244.039823	35.809626
1363.803912	127415.801386	35.814644
1364.870219	127609.565544	35.819661
1366.256954	127779.742859	35.824679
1367.729660	127942.775395	35.829696
1368.727514	128111.623065	35.834714
1370.060351	128274.008371	35.839732
1371.439330	128446.078602	35.844749
1372.634494	128611.946237	35.849767
1374.020270	128785.575715	35.854784
1375.331570	128963.272070	35.859802
1376.567628	129134.381132	35.864820
1377.500980	129319.006253	35.869837
1379.147125	129502.341115	35.874855
1380.510720	129685.443368	35.879872
1381.468922	129875.363836	35.884890
1382.453129	130065.066084	35.889908
1384.278578	130261.591315	35.894925
1385.447582	130462.935219	35.899943
1386.705893	130650.849506	35.904960
1388.014301	130861.739490	35.909978
1389.825119	131055.067221	35.914996
1391.572367	131268.272384	35.920013
1392.641585	131466.712630	35.925031
1394.347367	131662.595162	35.930048
1395.720727	131880.286124	35.935066
1397.153459	132077.063797	35.940084
1398.774576	132266.388218	35.945101
1399.933853	132473.981676	35.950119
1401.293998	132668.887118	35.955136
1402.640508	132883.853246	35.960154
1404.208994	133079.032469	35.965172
1405.455425	133279.649183	35.970189
1407.052284	133481.643396	35.975207
1408.609821	133688.523508	35.980224
1409.906927	133897.005004	35.985242
1411.526047	134097.074042	35.990260
1413.028252	134292.107322	35.995277
1414.880578	134490.266725	36.000295
1416.513440	134680.808980	36.005312
1418.154242	134881.120758	36.010330
1419.947866	135065.722530	36.015348
1421.497581	135246.144657	36.020365
1422.850478	135436.229510	36.025383
1424.440249	135623.807008	36.030400
1425.455176	135817.268003	36.035418
1427.172177	135989.380894	36.040436
1428.606990	136179.837729	36.045453
1429.572902	136364.275133	36.050471
1431.148348	136553.787006	36.055488
1432.442489	136744.117799	36.060506
1433.929911	136933.329308	36.065524
1435.615708	137122.421807	36.070541
1437.045313	137305.993091	36.075559
1438.718209	137490.439271	36.080576
1439.692682	137686.288738	36.085594
1441.236893	137870.453598	36.090612
1442.650058	138057.263657	36.095629
1443.917550	138252.702801	36.100647
1445.165621	138424.093384	36.105664
1445.984622	138603.663753	36.110682
1447.507236	138785.214437	36.115700
1448.930223	138969.696847	36.120717
1449.601597	139168.949910	36.125735
1451.247276	139371.255801	36.130752
1452.308458	139572.122466	36.135770
1453.415903	139785.022804	36.140788
1454.829533	139995.607452	36.145805
1456.044214	140208.430379	36.150823
1457.441120	140424.495646	36.155840
1458.794499	140656.145366	36.160858
1460.493946	140877.957693	36.165876
1461.925676	141091.107212	36.170893
1463.300940	141312.695401	36.175911
1465.182699	141526.511564	36.180928
1466.615613	141760.970722	36.185946
1468.224503	141984.529199	36.190964
1469.703718	142207.374802	36.195981
1471.270487	142435.708829	36.200999
1473.017215	142653.965049	36.206016
1474.472360	142879.772532	36.211034
1476.044770	143093.433327	36.216052
1477.801945	143315.875244	36.221069
1478.956816	143553.104678	36.226087
1480.722074	143766.473319	36.231104
1482.199292	143984.490251	36.236122
1483.281388	144218.808397	36.241140
1485.388900	144434.510191	36.246157
1486.504872	144663.591417	36.251175
1488.381866	144882.058138	36.256192
1489.792526	145106.481928	36.261210
1491.520429	145330.641440	36.266228
1493.782681	145544.830597	36.271245
1494.784948	145763.987499	36.276263
1496.684490	145971.506336	36.281280
1498.636715	146181.388579	36.286298
1499.911484	146390.353087	36.291316
1501.497898	146596.987758	36.296333
1503.009184	146815.424606	36.301351
1504.635175	147011.940065	36.306368
1505.796220	147228.394511	36.311386
1506.955116	147440.033707	36.316404
1508.589657	147642.344852	36.321421
1509.746739	147870.466722	36.326439
1511.519493	148085.600165	36.331456
1512.784244	148311.198075	36.336474
1514.361604	148529.940406	36.341492
1516.338465	148741.508964	36.346509
1517.507874	148968.495746	36.351527
1519.395721	149181.818097	36.356544
1520.786213	149393.788339	36.361562
1522.270730	149610.828641	36.366580
1524.118705	149817.455207	36.371597
1524.897587	150042.483168	36.376615
1526.604616	150238.029308	36.381632
1527.927776	150444.464321	36.386650
1529.307435	150649.344980	36.391668
1530.700316	150841.686463	36.396685
1532.201522	151055.412145	36.401703
1533.610122	151266.314064	36.406720
1535.067233	151474.078150	36.411738
1536.478744	151681.242240	36.416756
1538.669447	151894.280648	36.421773
1539.780016	152109.292334	36.426791
1541.247157	152328.115679	36.431808
1542.757845	152546.971586	36.436826
1544.355714	152773.827929	36.441844
1545.910220	152991.716233	36.446861
1547.150800	153225.237975	36.451879
1548.414239	153449.045748	36.456896
1550.046908	153689.900195	36.461914
1551.635996	153928.341607	36.466932
1553.478721	154155.422006	36.471949
1554.879542	154379.112723	36.476967
1556.841297	154609.575290	36.481984
1558.416707	154847.708399	36.487002
1559.715704	155079.458622	36.492020
1561.361164	155318.598265	36.497037
1562.530528	155553.808462	36.502055
1564.548915	155791.421356	36.507072
1566.162267	156025.765462	36.512090
1567.727258	156263.060583	36.517108
1569.937166	156482.705864	36.522125
1571.641275	156719.741128	36.527143
1573.454256	156948.138255	36.532160
1575.590255	157165.973707	36.537178
1577.108627	157374.461837	36.542196
1578.719262	157597.607731	36.547213
1580.113267	157821.486893	36.552231
1582.109348	158027.950290	36.557248
1583.518960	158253.148527	36.562266
1584.637186	158469.657519	36.567284
1586.431518	158690.486043	36.572301
1587.763022	158920.151927	36.577319
1589.363905	159150.816362	36.582336
1590.815823	159378.678111	36.587354
1591.953186	159615.493412	36.592372
1593.445999	159851.810004	36.597389
1594.953151	160088.227348	36.602407
1596.376357	160332.293766	36.607424
1597.843408	160572.854824	36.612442
1599.697363	160815.740180	36.617460
1602.228554	161052.660732	36.622477
1603.575575	161285.243577	36.627495
1605.318655	161518.132799	36.632512
1606.901846	161752.913158	36.637530
1608.453910	161990.046150	36.642548
1610.221422	162212.181719	36.647565
1611.448729	162450.650201	36.652583
1613.414101	162654.583643	36.657600
1615.090932	162869.724423	36.662618
1616.615175	163085.638968	36.667636
1618.422134	163279.949851	36.672653
1619.709912	163498.555017	36.677671
1620.978060	163705.813750	36.682688
1622.638139	163913.480667	36.687706
1623.994229	164139.523495	36.692724
1625.754761	164369.460499	36.697741
1627.129212	164601.996821	36.702759
1628.989661	164828.864262	36.707776
1630.751674	165049.191626	36.712794
1631.834023	165282.121058	36.717812
1634.199906	165501.391294	36.722829
1635.743047	165731.396655	36.727847
1637.519501	165950.547534	36.732864
1639.371936	166177.957188	36.737882
1641.031555	166405.386163	36.742900
1642.501208	166624.767283	36.747917
1643.952103	166858.891000	36.752935
1645.535746	167083.786743	36.757952
1647.029421	167314.824364	36.762970
1648.235205	167564.681185	36.767988
1650.416075	167803.704942	36.773005
1652.023859	168038.254978	36.778023
1653.559678	168292.782618	36.783040
1655.113928	168541.220630	36.788058
1656.521087	168788.262978	36.793076
1658.388937	169039.483005	36.798093
1660.090849	169294.193869	36.803111
1661.545915	169542.882429	36.808128
1663.349685	169795.982183	36.813146
1664.696556	170059.126287	36.818164
1666.419176	170314.373334	36.823181
1668.207928	170574.761591	36.828199
1669.581801	170831.348572	36.833216
1671.405182	171092.927164	36.838234
1672.667173	171362.689729	36.843252
1674.603032	171622.782521	36.848269
1676.527810	171894.726810	36.853287
1678.362132	172153.596070	36.858304
1679.831176	172410.736382	36.863322
1681.352503	172685.274560	36.868340
1683.357228	172949.043919	36.873357
1685.106559	173221.557946	36.878375
1686.687003	173488.265197	36.883392
1688.162620	173756.792253	36.888410
1689.731525	174027.336035	36.893428
1691.584143	174298.673855	36.898445
1693.325106	174578.442106	36.903463
1695.139663	174845.209947	36.908480
1696.970166	175112.788926	36.913498
1698.611857	175391.018115	36.918516
1700.694580	175653.587536	36.923533
1702.591426	175913.638165	36.928551
1703.935113	176156.740182	36.933568
1705.507622	176396.584885	36.938586
1707.191319	176648.744832	36.943604
1709.115158	176886.126107	36.948621
1710.514974	177127.195019	36.953639
1712.111979	177384.904680	36.958656
1713.807936	177625.485407	36.963674
1714.839170	177889.669590	36.968692
1716.651678	178155.672523	36.973709
1718.207833	178421.172288	36.978727
1720.205391	178688.620926	36.983744
1722.069418	178946.500757	36.988762
1723.734056	179202.954749	36.993780
1725.475456	179472.796190	36.998797
1727.095157	179744.422245	37.003815
1728.840184	180020.064829	37.008832
1730.791717	180288.939156	37.013850
1732.203500	180572.733028	37.018868
1733.957492	180848.620562	37.023885
1735.993196	181119.757849	37.028903
1737.630785	181408.761519	37.033920
1739.469468	181678.017656	37.038938
1740.974754	181956.831932	37.043956
1743.157429	182234.893325	37.048973
1744.846259	182519.975480	37.053991
1746.397924	182796.579921	37.059008
1748.489283	183079.723874	37.064026
1750.119317	183363.602690	37.069044
1752.109359	183649.469056	37.074061
1754.205191	183929.724660	37.079079
1755.991087	184209.510979	37.084096
1757.880345	184489.853636	37.089114
1759.422311	184765.824672	37.094132
1761.182016	185036.154202	37.099149
1763.270837	185309.186663	37.104167
1764.836235	185592.785260	37.109184
1766.467309	185869.192979	37.114202
1768.434558	186158.200428	37.119220
1770.235575	186432.858793	37.124237
1771.848547	186711.863130	37.129255
1773.067285	186995.817286	37.134272
1775.109831	187276.914085	37.139290
1776.860052	187576.928854	37.144308
1779.217081	187864.311528	37.149325
1780.952159	188144.954770	37.154343
1782.601722	188437.338935	37.159360
1784.513687	188709.480461	37.164378
1785.835519	189000.206961	37.169396
1787.737942	189290.627337	37.174413
1789.165533	189573.967462	37.179431
1790.861679	189873.903883	37.184448
1792.897361	190165.234826	37.189466
1794.693070	190458.471155	37.194484
1796.636272	190747.193331	37.199501
1798.899676	191024.825394	37.204519
1800.519844	191291.647001	37.209536
1802.966088	191544.340821	37.214554
1804.936148	191805.043421	37.219572
1806.614889	192049.980573	37.224589
1808.536559	192295.514938	37.229607
1810.086238	192546.452570	37.234624
1811.836772	192799.364811	37.239642
1813.504303	193060.807398	37.244660
1815.456181	193308.144153	37.249677
1817.479482	193560.217402	37.254695
1818.975481	193826.539361	37.259712
1820.846050	194086.165570	37.264730
1822.351188	194359.913478	37.269748
1824.136035	194628.478317	37.274765
1825.674532	194905.396806	37.279783
1827.586998	195172.192789	37.284800
1829.240558	195448.270985	37.289818
1830.886303	195746.207531	37.294836
1832.912585	196031.583702	37.299853
1834.171938	196315.496666	37.304871
1835.777120	196611.985040	37.309888
1837.917260	196902.158275	37.314906
1839.631503	197201.932682	37.319924
1841.433333	197503.801842	37.324941
1843.338719	197798.548492	37.329959
1845.068816	198107.489519	37.334976
1847.077716	198403.340049	37.339994
1848.640965	198719.330143	37.345012
1850.464757	199030.559026	37.350029
1852.409835	199340.260009	37.355047
1854.205712	199668.289670	37.360064
1856.328288	199969.969531	37.365082
1858.571208	200282.179916	37.370100
1860.199207	200600.760106	37.375117
1862.063922	200904.542344	37.380135
1864.068023	201221.822498	37.385152
1866.122848	201529.068654	37.390170
1868.139999	201844.776321	37.395188
1869.854684	202150.785160	37.400205
1872.342321	202439.562042	37.405223
1874.367987	202751.262292	37.410240
1876.334519	203044.021927	37.415258
1878.313394	203358.068585	37.420276
1880.003056	203659.773673	37.425293
1881.908150	203954.642220	37.430311
1883.941271	204260.281844	37.435328
1885.936318	204559.378999	37.440346
1887.696802	204858.794194	37.445364
1889.710633	205165.723756	37.450381
1891.629472	205468.709400	37.455399
1893.187881	205779.827390	37.460416
1894.721872	206081.163528	37.465434
1896.755438	206382.713884	37.470452
1898.349300	206696.395330	37.475469
1900.378444	206987.260667	37.480487
1902.588489	207279.355471	37.485504
1904.562291	207567.414186	37.490522
1906.498845	207853.906033	37.495540
1908.140016	208127.941718	37.500557
1910.373256	208410.072860	37.505575
1911.945318	208700.257250	37.510592
1913.863925	208976.664732	37.515610
1915.556248	209265.740924	37.520628
1917.337920	209563.056096	37.525645
1918.978494	209854.453739	37.530663
1920.724859	210154.151315	37.535680
1922.849338	210449.093058	37.540698
1924.461103	210753.664435	37.545716
1926.533694	211064.892702	37.550733
1928.829349	211374.081203	37.555751
1930.175970	211689.680690	37.560768
1932.701271	211989.415623	37.565786
1934.711996	212293.448554	37.570804
1936.691138	212597.932264	37.575821
1938.582131	212911.153366	37.580839
1940.506778	213227.747707	37.585856
1942.457972	213539.756134	37.590874
1944.430418	213858.326456	37.595892
1946.280404	214170.798253	37.600909
1948.650306	214483.569882	37.605927
1950.475293	214807.792457	37.610944
1952.203722	215120.376806	37.615962
1954.278451	215443.445512	37.620980
1955.980955	215774.789310	37.625997
1957.988734	216089.492111	37.631015
1959.790372	216423.083231	37.636032
1961.751926	216749.845255	37.641050
1963.525680	217085.805500	37.646068
1965.378630	217429.207680	37.651085
1967.430482	217752.938223	37.656103
1969.663027	218098.962393	37.661120
1971.419697	218433.509667	37.666138
1973.464091	218769.320607	37.671156
1975.261039	219124.116131	37.676173
1977.186555	219457.777931	37.681191
1979.197344	219814.053793	37.686208
1981.386112	220148.667308	37.691226
1983.678676	220522.817430	37.696244
1985.434367	220898.514777	37.701261
1987.794370	221238.057884	37.706279
1989.731030	221581.377292	37.711296
1991.875069	221925.338295	37.716314
1994.282348	222258.402765	37.721332
1996.282927	222589.984102	37.726349
1998.410163	222919.604029	37.731367
1999.984807	223262.620084	37.736384
2001.988159	223595.767026	37.741402
2004.251732	223938.854463	37.746420
2006.039588	224269.409982	37.751437
2008.290717	224594.611067	37.756455
2010.023333	224908.378772	37.761472
2012.118758	225218.471219	37.766490
2014.099875	225515.021569	37.771508
2015.902026	225825.391390	37.776525
2018.174667	226135.141708	37.781543
2019.974670	226444.485629	37.786560
2021.809719	226750.752178	37.791578
2023.950197	227075.358333	37.796596
2025.630453	227405.702143	37.801613
2027.977466	227714.252791	37.806631
2030.142494	228045.563399	37.811648
2031.953899	228369.769489	37.816666
2033.985791	228694.221161	37.821684
2035.611535	229030.522627	37.826701
2037.729109	229362.709208	37.831719
2039.726315	229695.500249	37.836736
2041.685897	230029.111193	37.841754
2044.143926	230371.126980	37.846772
2046.101239	230720.156965	37.851789
2048.231627	231063.827336	37.856807
2050.296028	231403.801397	37.861824
2051.986272	231749.575916	37.866842
2054.370277	232086.581002	37.871860
2056.200541	232439.015425	37.876877
2058.418835	232787.249716	37.881895
2060.274196	233148.622820	37.886912
2062.658146	233487.207476	37.891930
2064.889977	233830.109723	37.896948
2066.573602	234186.231038	37.901965
2068.691666	234541.624340	37.906983
2070.854390	234891.906709	37.912000
2072.840725	235258.879720	37.917018
2074.927822	235614.484851	37.922036
2076.911374	235985.778648	37.927053
2079.268611	236345.331015	37.932071
2081.454961	236698.231793	37.937088
2083.718451	237054.321772	37.942106
2086.067848	237412.202633	37.947124
2087.808697	237778.969311	37.952141
2089.804953	238132.590681	37.957159
2092.139603	238492.991917	37.962176
2093.929286	238862.167353	37.967194
2096.093213	239223.817174	37.972212
2098.078100	239604.876411	37.977229
2100.277828	239965.532296	37.982247
2102.410381	240341.134991	37.987264
2104.323683	240708.290116	37.992282
2106.944073	241067.536443	37.997300
2108.668481	241449.684328	38.002317
2110.869746	241804.554318	38.007335
2113.082877	242168.389686	38.012352
2114.650337	242549.651457	38.017370
2117.295500	242921.091334	38.022388
2119.148869	243301.268595	38.027405
2121.492697	243663.004678	38.032423
2123.541900	244015.415712	38.037440
2125.457794	244360.406467	38.042458
2127.997589	244690.515997	38.047476
2129.782881	245040.914138	38.052493
2131.784708	245382.159964	38.057511
2134.108972	245727.013204	38.062528
2135.808349	246081.415523	38.067546
2138.122434	246424.925837	38.072564
2140.549061	246783.075491	38.077581
2142.853921	247125.064872	38.082599
2145.597209	247478.822426	38.087616
2147.106273	247827.289918	38.092634
2149.374174	248180.438690	38.097652
2151.043798	248538.356998	38.102669
2152.769809	248895.301936	38.107687
2155.079278	249263.179353	38.112704
2157.381297	249640.533543	38.117722
2159.346836	250009.940497	38.122740
2161.254839	250399.653262	38.127757
2163.297536	250766.077678	38.132775
2165.719511	251157.056967	38.137792
2167.221735	251550.062737	38.142810
2169.750884	251933.888883	38.147828
2171.676844	252334.805357	38.152845
2173.926547	252725.612216	38.157863
2176.144746	253126.687290	38.162880
2178.072721	253519.706000	38.167898
2180.413319	253926.224783	38.172916
2182.222477	254343.624593	38.177933
2184.693612	254750.149772	38.182951
2186.789454	255165.524448	38.187968
2189.001264	255580.398920	38.192986
2191.389186	255991.232706	38.198004
2193.502603	256420.197290	38.203021
2195.543768	256833.577074	38.208039
2198.083946	257244.135009	38.213056
2200.314815	257670.492275	38.218074
2202.986024	258086.619454	38.223092
2204.968247	258496.963197	38.228109
2207.418610	258911.272395	38.233127
2209.782063	259327.831479	38.238144
2211.674974	259739.156668	38.243162
2214.062644	260154.189035	38.248180
2216.498566	260572.516732	38.253197
2219.019946	260970.306002	38.258215
2222.141458	261364.266425	38.263232
2225.022157	261760.297778	38.268250
2227.380151	262138.097010	38.273268
2229.693639	262527.081041	38.278285
2232.313762	262902.070668	38.283303
2234.924935	263260.042110	38.288320
2237.339540	263636.208252	38.293338
2239.512900	263986.857558	38.298356
2241.951559	264355.501311	38.303373
2244.146650	264709.018378	38.308391
2246.590868	265041.843513	38.313408
2248.462636	265362.185125	38.318426
2250.607783	265687.665872	38.323444
2252.731188	266014.852316	38.328461
2254.512090	266341.585233	38.333479
2256.613144	266682.086958	38.338496
2258.486813	267039.213278	38.343514
2260.751654	267373.872152	38.348532
2262.869561	267725.930360	38.353549
2264.527535	268085.174624	38.358567
2266.597172	268444.125200	38.363584
2268.600008	268819.217668	38.368602
2270.609136	269196.722660	38.373620
2272.733363	269580.153978	38.378637
2274.606028	269970.484272	38.383655
2276.895795	270355.464717	38.388672
2278.339925	270758.590384	38.393690
2280.787508	271172.480568	38.398708
2282.723934	271595.978216	38.403725
2284.980423	272022.854718	38.408743
2287.060052	272441.071420	38.413760
2289.088644	272875.325863	38.418778
2291.299766	273321.668882	38.423796
2293.318005	273767.966342	38.428813
2295.709023	274207.930107	38.433831
2298.363364	274654.050586	38.438848
2300.756059	275111.034409	38.443866
2302.964790	275562.585645	38.448884
2305.903296	276000.379516	38.453901
2307.998244	276455.428960	38.458919
2310.541097	276904.335898	38.463936
2312.969672	277358.671772	38.468954
2315.483164	277806.516190	38.473972
2317.897122	278263.115001	38.478989
2320.056285	278723.259692	38.484007
2322.621709	279170.917534	38.489024
2324.704371	279633.766680	38.494042
2327.046120	280077.953860	38.499060
2329.742937	280532.779292	38.504077
2332.157732	280996.692713	38.509095
2334.429334	281445.310331	38.514112
2336.430521	281907.307197	38.519130
2339.194778	282367.988775	38.524148
2341.589332	282820.904375	38.529165
2344.016454	283283.416815	38.534183
2346.689927	283730.978100	38.539200
2349.185372	284187.204235	38.544218
2351.660209	284629.639268	38.549236
2354.735654	285066.542363	38.554253
2356.806932	285511.809340	38.559271
2359.439521	285952.846128	38.564288
2361.719241	286388.705302	38.569306
2364.642934	286813.513181	38.574324
2367.013695	287253.141875	38.579341
2369.368098	287670.646649	38.584359
2372.043979	288060.283780	38.589376
2374.312828	288462.864171	38.594394
2376.327934	288853.443314	38.599412
2379.078403	289234.912794	38.604429
2381.086648	289634.128898	38.609447
2383.224395	290023.239029	38.614464
2385.567815	290428.421276	38.619482
2387.802141	290828.565066	38.624500
2389.999799	291234.836059	38.629517
2392.037316	291657.643412	38.634535
2394.284404	292066.826481	38.639552
2395.982775	292497.383055	38.644570
2398.207164	292941.699753	38.649588
2400.368305	293376.652135	38.654605
2402.345916	293819.075614	38.659623
2405.138347	294270.056598	38.664640
2407.451059	294734.321776	38.669658
2409.915295	295188.375636	38.674676
2412.326022	295649.016079	38.679693
2414.225503	296123.656759	38.684711
2416.958749	296588.282766	38.689728
2419.298208	297066.890256	38.694746
2421.504176	297534.772689	38.699764
2424.183887	298014.339823	38.704781
2426.389190	298500.915489	38.709799
2428.617991	298984.539471	38.714816
2431.402107	299479.123716	38.719834
2433.420371	299972.303770	38.724852
2436.228247	300463.020258	38.729869
2438.407698	300964.046140	38.734887
2440.948293	301454.420877	38.739904
2443.346136	301966.255207	38.744922
2445.556799	302477.228420	38.749940
2448.473968	302970.129434	38.754957
2451.150069	303487.426389	38.759975
2454.204702	303977.838276	38.764992
2456.738685	304480.624875	38.770010
2459.018742	304975.220089	38.775028
2461.951215	305466.738248	38.780045
2464.471492	305976.125582	38.785063
2466.946714	306451.684891	38.790080
2469.231640	306966.160294	38.795098
2471.826448	307449.367797	38.800116
2474.466057	307943.767728	38.805133
2477.078848	308445.662888	38.810151
2479.502622	308940.016789	38.815168
2481.917597	309439.627772	38.820186
2484.638797	309939.264309	38.825204
2487.271125	310420.675968	38.830221
2489.602907	310913.664533	38.835239
2492.472538	311403.721006	38.840256
2494.983373	311890.784282	38.845274
2497.037272	312379.314751	38.850292
2500.110974	312868.925975	38.855309
2502.395260	313349.618081	38.860327
2504.530515	313805.999694	38.865344
2506.897629	314269.174789	38.870362
2509.707247	314727.883761	38.875380
2512.086980	315183.382406	38.880397
2514.556645	315645.036513	38.885415
2517.233018	316105.233440	38.890432
2519.646615	316566.714359	38.895450
2521.718975	317035.460157	38.900468
2524.062372	317499.970109	38.905485
2526.480063	317978.663294	38.910503
2528.834774	318458.786289	38.915520
2530.911642	318946.036698	38.920538
2533.248680	319444.291100	38.925556
2535.816630	319934.556917	38.930573
2538.377891	320440.059290	38.935591
2540.998840	320937.371584	38.940608
2543.556615	321445.814815	38.945626
2545.834073	321963.848581	38.950644
2548.749196	322464.788068	38.955661
2551.204172	322987.485866	38.960679
2553.793531	323495.454848	38.965696
2556.368566	324018.939894	38.970714
2559.306339	324532.993148	38.975732
2562.072426	325041.940480	38.980749
2564.609353	325567.605695	38.985767
2567.549053	326077.788762	38.990784
2570.337038	326577.682198	38.995802
2572.629202	327095.554414	39.000820
2575.778262	327605.008758	39.005837
2578.585186	328122.919541	39.010855
2581.500856	328624.227056	39.015872
2584.157662	329135.145884	39.020890
2586.546789	329637.012571	39.025908
2589.305318	330138.284080	39.030925
2591.948003	330652.038837	39.035943
2594.582086	331146.289118	39.040960
2597.461582	331655.301468	39.045978
2599.851298	332162.330947	39.050996
2602.174651	332668.961035	39.056013
2605.111879	333181.762256	39.061031
2607.542259	333674.478267	39.066048
2609.898545	334200.466593	39.071066
2612.240446	334718.200693	39.076084
2614.938377	335238.134347	39.081101
2617.231025	335764.755464	39.086119
2619.723974	336281.031700	39.091136
2623.012258	336803.551183	39.096154
2625.284033	337331.915170	39.101172
2627.939789	337855.948360	39.106189
2630.686537	338383.416040	39.111207
2633.483430	338899.648787	39.116224
2636.523944	339415.280166	39.121242
2639.093190	339937.075627	39.126260
2642.168026	340449.874768	39.131277
2644.689757	340950.951035	39.136295
2647.597562	341430.812554	39.141312
2650.712963	341908.834782	39.146330
2653.072524	342374.049869	39.151348
2655.392307	342839.343837	39.156365
2658.194519	343318.877059	39.161383
2660.941381	343788.208970	39.166400
2662.952095	344257.476031	39.171418
2665.232395	344743.960603	39.176436
2668.601037	345209.983750	39.181453
2670.488875	345708.048546	39.186471
2673.154226	346195.830868	39.191488
2675.653538	346684.777748	39.196506
2678.421056	347195.612384	39.201524
2680.914262	347694.604778	39.206541
2683.573352	348204.152674	39.211559
2686.195669	348723.043911	39.216576
2688.437700	349233.029179	39.221594
2691.038521	349762.677732	39.226612
2693.527845	350294.953506	39.231629
2695.638765	350832.386429	39.236647
2698.127674	351379.882776	39.241664
2701.055846	351924.384661	39.246682
2703.537971	352492.381580	39.251700
2706.052457	353052.244235	39.256717
2708.689223	353627.870394	39.261735
2711.384946	354205.943032	39.266752
2714.058157	354790.587048	39.271770
2716.466418	355377.347734	39.276788
2719.081374	355951.834321	39.281805
2721.657412	356557.744162	39.286823
2724.218005	357171.441444	39.291840
2727.477797	357758.369314	39.296858
2729.938089	358369.097876	39.301876
2732.959944	358968.181346	39.306893
2735.788373	359580.943027	39.311911
2738.519622	360194.702130	39.316928
2741.699496	360795.895148	39.321946
2744.193217	361409.828460	39.326964
2746.937406	362012.445498	39.331981
2750.015890	362630.660911	39.336999
2752.592651	363244.683851	39.342016
2755.689706	363860.113560	39.347034
2758.297290	364474.115170	39.352052
2761.777041	365085.381816	39.357069
2764.571557	365694.667713	39.362087
2767.754736	366289.393320	39.367104
2770.491640	366896.971655	39.372122
2773.242074	367508.650516	39.377140
2776.205168	368101.051953	39.382157
2778.961908	368706.521264	39.387175
2781.810166	369316.053101	39.392192
2784.754160	369906.301350	39.397210
2787.810047	370496.777493	39.402228
2791.039785	371084.731210	39.407245
2794.333052	371649.449304	39.412263
2796.901929	372192.072373	39.417280
2799.959842	372725.273504	39.422298
2802.859745	373261.715213	39.427316
2805.976739	373775.381474	39.432333
2808.944917	374299.087050	39.437351
2811.477011	374822.499755	39.442368
2814.499489	375333.268981	39.447386
2816.893959	375868.665536	39.452404
2820.042963	376389.676862	39.457421
2822.609851	376919.805628	39.462439
2825.397937	377444.843574	39.467456
2827.961087	377971.381653	39.472474
2830.308928	378516.872750	39.477492
2832.810236	379058.704122	39.482509
2835.811559	379619.298127	39.487527
2838.212467	380175.767867	39.492544
2840.936787	380733.852706	39.497562
2843.358335	381317.041038	39.502580
2846.186031	381884.631142	39.507597
2848.793934	382474.799102	39.512615
2851.460780	383066.901767	39.517632
2854.289241	383656.255302	39.522650
2856.926652	384261.711896	39.527668
2859.888326	384860.664412	39.532685
2862.864392	385470.613470	39.537703
2865.783542	386088.323060	39.542720
2868.637196	386697.865238	39.547738
2871.426998	387322.524239	39.552756
2874.164379	387938.683958	39.557773
2876.927081	388558.075588	39.562791
2880.196629	389189.296706	39.567808
2883.360766	389811.849428	39.572826
2885.869119	390450.980142	39.577844
2888.792099	391080.726012	39.582861
2891.988764	391718.481967	39.587879
2894.419501	392362.307155	39.592896
2897.450754	392992.457761	39.597914
2900.289013	393642.838837	39.602932
2903.571571	394291.793200	39.607949
2906.170547	394934.529133	39.612967
2909.117870	395588.532735	39.617984
2912.414676	396228.217410	39.623002
2914.895463	396879.886098	39.628020
2917.945187	397521.841870	39.633037
2921.320043	398175.093228	39.638055
2923.857082	398826.106182	39.643072
2927.483224	399469.352680	39.648090
2930.418749	400116.879287	39.653108
2933.731394	400753.583185	39.658125
2936.853084	401388.504644	39.663143
2939.966310	402030.082722	39.668160
2943.365670	402657.836228	39.673178
2946.596289	403300.460299	39.678196
2949.088618	403921.284495	39.683213
2952.332473	404524.586729	39.688231
2955.012083	405126.699119	39.693248
2957.715709	405712.648119	39.698266
2960.108197	406304.541742	39.703284
2962.965765	406893.359232	39.708301
2965.516214	407497.752722	39.713319
2967.973121	408111.832039	39.718336
2970.812704	408726.928362	39.723354
2973.165899	409354.230406	39.728372
2976.077954	409984.928786	39.733389
2978.867725	410616.647115	39.738407
2981.866688	411274.450096	39.743424
2984.736167	411912.718163	39.748442
2987.398911	412568.568782	39.753460
2990.272582	413240.337962	39.758477
2992.880260	413918.773749	39.763495
2995.756455	414588.813583	39.768512
2999.127258	415269.783432	39.773530
3001.874976	415971.717090	39.778548
3004.452921	416660.990133	39.783565
3007.391826	417365.469528	39.788583
3010.236958	418074.938207	39.793600
3013.442887	418798.014982	39.798618
3016.340983	419508.655548	39.803636
3019.868696	420226.577033	39.808653
3023.254590	420934.190386	39.813671
3026.577878	421648.053660	39.818688
3029.884855	422360.963657	39.823706
3033.331574	423075.049134	39.828724
3036.417692	423791.757127	39.833741
3039.839866	424496.106300	39.838759
3043.182950	425203.970955	39.843776
3046.469385	425900.857130	39.848794
3049.463662	426608.664029	39.853812
3053.072401	427303.512174	39.858829
3056.638539	427989.407317	39.863847
3059.347157	428687.173311	39.868864
3062.856018	429373.244218	39.873882
3066.070241	430064.510769	39.878900
3069.339305	430742.706624	39.883917
3072.857943	431421.959688	39.888935
3075.691393	432109.990253	39.893952
3079.122983	432767.137187	39.898970
3082.072876	433440.804739	39.903988
3084.817146	434125.123268	39.909005
3088.224123	434796.656737	39.914023
3090.622398	435476.435335	39.919040
3093.910503	436159.549307	39.924058
3097.005686	436854.221852	39.929076
3099.762901	437545.915388	39.934093
3103.057251	438218.691858	39.939111
3106.058535	438914.916941	39.944128
3109.412947	439588.279650	39.949146
3112.300289	440284.180242	39.954164
3115.207838	440969.728386	39.959181
3118.956295	441642.314007	39.964199
3121.757363	442311.182847	39.969216
3124.783214	442948.859868	39.974234
3127.811954	443606.214297	39.979252
3130.356081	444254.615636	39.984269
3133.407709	444905.855433	39.989287
3136.293420	445566.064285	39.994304
3139.244381	446238.394089	39.999322
3142.058216	446911.333913	40.004340
3145.111408	447585.229036	40.009357
3148.268995	448257.316591	40.014375
3150.624706	448957.503233	40.019392
3153.830261	449664.873694	40.024410
3157.125137	450376.915566	40.029428
3159.776620	451086.051049	40.034445
3162.941260	451799.081763	40.039463
3165.799295	452528.789380	40.044480
3168.907997	453260.660723	40.049498
3171.995663	454006.884028	40.054516
3175.006634	454750.969399	40.059533
3177.967639	455507.233412	40.064551
3180.877198	456267.831741	40.069568
3184.176460	457036.134832	40.074586
3187.647408	457807.875429	40.079604
3191.038219	458580.816058	40.084621
3194.652236	459355.414441	40.089639
3197.633676	460129.377196	40.094656
3200.877853	460911.264285	40.099674
3204.358879	461685.497429	40.104692
3207.462971	462468.766991	40.109709
3210.712718	463243.891389	40.114727
3213.877519	464040.701510	40.119744
3217.487257	464821.579511	40.124762
3220.983931	465619.492075	40.129780
3224.054382	466417.846609	40.134797
3227.893968	467194.503961	40.139815
3231.285933	467982.582529	40.144832
3234.710496	468767.440203	40.149850
3237.926328	469542.136704	40.154868
3241.284493	470325.125530	40.159885
3245.029637	471095.027917	40.164903
3248.212628	471872.625633	40.169920
3251.887813	472629.688717	40.174938
3255.408880	473402.270231	40.179956
3259.200596	474166.589059	40.184973
3262.399578	474922.428657	40.189991
3265.867855	475682.140638	40.195008
3269.391822	476432.664977	40.200026
3272.592274	477184.172807	40.205044
3275.513036	477930.136123	40.210061
3279.112268	478669.847903	40.215079
3282.109779	479437.882123	40.220096
3285.384755	480185.473513	40.225114
3288.850172	480929.721130	40.230132
3292.457542	481665.275704	40.235149
3296.311864	482381.912862	40.240167
3299.415567	483090.000618	40.245184
3302.262262	483777.636768	40.250202
3305.366878	484461.872493	40.255220
3308.382705	485158.073669	40.260237
3311.441220	485852.474301	40.265255
3314.256807	486564.976735	40.270272
3317.496026	487269.048895	40.275290
3320.513016	487994.551859	40.280308
3323.377368	488719.293302	40.285325
3326.340793	489451.114408	40.290343
3329.366213	490200.780267	40.295360
3332.483761	490951.664399	40.300378
3335.328206	491719.634881	40.305396
3338.554714	492499.989403	40.310413
3341.913219	493271.653146	40.315431
3345.000773	494043.883005	40.320448
3348.163651	494848.492395	40.325466
3351.789238	495638.650613	40.330484
3355.250301	496454.252632	40.335501
3358.682190	497249.219549	40.340519
3361.844598	498057.625976	40.345536
3365.473921	498878.091221	40.350554
3368.314630	499690.817573	40.355572
3371.785957	500520.321022	40.360589
3375.008954	501349.168818	40.365607
3378.424937	502196.878887	40.370624
3381.200988	503041.166296	40.375642
3384.828716	503883.259468	40.380660
3388.364835	504748.192629	40.385677
3391.926324	505599.148170	40.390695
3395.632535	506463.262835	40.395712
3399.089124	507312.536035	40.400730
3402.285375	508174.223469	40.405748
3405.773915	509038.193413	40.410765
3409.341582	509910.887655	40.415783
3412.867684	510776.025544	40.420800
3416.488783	511642.264967	40.425818
3420.409020	512500.491634	40.430836
3423.420909	513374.105030	40.435853
3427.012985	514240.619497	40.440871
3430.216451	515101.702474	40.445888
3433.997573	515974.100431	40.450906
3438.023463	516841.067275	40.455924
3441.479854	517713.374831	40.460941
3445.314719	518566.764111	40.465959
3448.735838	519427.487329	40.470976
3452.356601	520283.595129	40.475994
3456.022030	521143.231398	40.481012
3459.305092	522001.117874	40.486029
3462.821211	522856.501912	40.491047
3466.304613	523707.308127	40.496064
3469.626847	524558.699907	40.501082
3473.465069	525407.746776	40.506100
3476.698562	526274.538624	40.511117
3480.075686	527104.923775	40.516122
3483.314937	527910.267000	40.521127
3486.255927	528651.591421	40.526132
3489.622474	529341.575790	40.531136
3492.342966	529986.307962	40.536141
3495.244268	530544.938221	40.541146
3497.452640	531066.572701	40.546151
3499.674669	531520.081915	40.551156
3502.086637	531936.009919	40.556160
3503.989171	532301.233709	40.561165
3505.886681	532585.769207	40.566170
3507.724509	532847.726804	40.571175
3509.072817	533073.080891	40.576180
3510.818850	533229.411818	40.581184
3512.097435	533362.223319	40.586189
3513.238233	533449.539381	40.591194
3514.272748	533515.503008	40.596199
3515.315611	533532.413016	40.601204
3515.997874	533516.190268	40.606208
3516.847918	533498.779091	40.611213
3517.152022	533437.706171	40.616218
3518.157542	533363.337059	40.621223
3518.397715	533270.245368	40.626228
3519.121701	533145.856348	40.631232
3519.719639	533017.697348	40.636237
3519.766444	532867.345418	40.641242
3520.592257	532698.883881	40.646247
3520.278777	532533.581276	40.651252
3520.313508	532342.304653	40.656256
3520.486752	532160.299758	40.661261
3520.621951	531954.553329	40.666266
3520.658893	531749.476512	40.671271
3520.695418	531544.397068	40.676276
3520.941781	531301.641191	40.681280
3520.743491	531089.115283	40.686285
3520.855110	530864.310286	40.691290
3520.739688	530622.813678	40.696295
3520.683598	530384.840885	40.701300
3520.816561	530141.630215	40.706304
3520.418261	529915.477427	40.711309
3520.375601	529674.257905	40.716314
3520.208123	529429.618351	40.721319
3519.787586	529199.163703	40.726324
3519.927871	528947.393672	40.731328
3519.611041	528721.311928	40.736333
3519.414160	528465.494360	40.741338
3519.227690	528233.169420	40.746343
3518.846282	528016.588231	40.751348
3518.834353	527769.978073	40.756352
3518.492424	527534.433175	40.761357
3518.577497	527308.368819	40.766362
3518.479904	527082.936570	40.771367
3517.886481	526851.615939	40.776372
3517.757431	526624.767092	40.781376
3517.487705	526398.897510	40.786381
3517.106970	526188.912053	40.791386
3517.042576	525979.682500	40.796391
3516.764978	525776.195148	40.801396
3516.768348	525543.143883	40.806400
3516.430777	525350.729449	40.811405
3516.383546	525150.331419	40.816410
3515.945291	524946.757829	40.821415
3515.583921	524751.458922	40.826420
3515.596148	524556.604053	40.831424
3515.183606	524370.760672	40.836429
3515.001125	524174.213364	40.841434
3515.152005	523992.522519	40.846439
3514.533631	523822.476180	40.851444
3514.752390	523632.935592	40.856448
3514.191712	523453.373078	40.861453
3513.981771	523286.087293	40.866458
3514.105450	523119.960257	40.871463
3513.657395	522940.121487	40.876468
3513.656849	522779.823943	40.881472
3513.528796	522617.977856	40.886477
3513.323625	522453.918034	40.891482
3513.667399	522287.747678	40.896487
3512.970185	522146.612419	40.901492
3512.977326	521978.469966	40.906496
3512.714023	521832.511332	40.911501
3512.506024	521672.741182	40.916506
3512.407459	521527.967095	40.921511
3512.115332	521386.103989	40.926516
3511.987176	521249.117679	40.931520
3511.781849	521118.866439	40.936525
3511.901060	520969.957893	40.941530
3511.810501	520830.788176	40.946535
3511.260952	520714.188055	40.951540
3511.215297	520579.812093	40.956544
3511.291958	520449.460386	40.961549
3510.917925	520323.729183	40.966554
3510.674610	520201.009917	40.971559
3510.491106	520091.526935	40.976564
3510.653886	519978.247046	40.981568
3510.500412	519867.594939	40.986573
3510.638995	519733.031226	40.991578
3510.169658	519628.848654	40.996583
3509.956694	519523.158618	41.001588
3510.016291	519393.964126	41.006592
3510.007543	519315.442749	41.011597
3509.826900	519215.560269	41.016602
3509.722015	519106.968415	41.021607
3509.532336	519000.512895	41.026612
3509.379764	518896.730683	41.031616
3509.142469	518810.810194	41.036621
3509.173942	518717.262186	41.041626
3509.289444	518625.267858	41.046631
3508.750333	518537.522768	41.051636
3509.045953	518445.246146	41.056640
3508.850281	518368.772389	41.061645
3508.734109	518281.717568	41.066650
3508.873961	518186.076240	41.071655
3508.763483	518099.575780	41.076660
3508.847488	518015.724133	41.081664
3508.365851	517928.927478	41.086669
3508.597908	517847.782164	41.091674
3508.874611	517762.634613	41.096679
3508.473959	517682.953796	41.101684
3508.563730	517596.065082	41.106688
3508.304884	517511.455987	41.111693
3508.440242	517430.222775	41.116698
3508.556257	517351.065516	41.121703
3507.965209	517284.712290	41.126708
3508.274988	517202.641302	41.131712
3507.987219	517132.092906	41.136717
3507.908721	517057.617318	41.141722
3508.309277	516985.240161	41.146727
3507.774157	516909.824694	41.151732
3507.751684	516838.171158	41.156736
3507.637936	516773.409248	41.161741
3507.370774	516707.103659	41.166746
3507.643919	516637.475910	41.171751
3507.662492	516571.074048	41.176756
3507.509746	516499.540783	41.181760
3507.442333	516457.982275	41.186765
3507.128536	516379.697450	41.191770
3507.345019	516318.977836	41.196775
3506.763016	516265.211348	41.201780
3507.058598	516201.798518	41.206784
3506.658031	516156.195606	41.211789
3506.633262	516091.821553	41.216794
3506.785396	516035.510837	41.221799
3506.629425	515991.031975	41.226804
3506.334577	515936.915607	41.231808
3506.205245	515903.052510	41.236813
3506.494497	515860.626979	41.241818
3506.492921	515820.320790	41.246823
3505.921065	515775.249635	41.251828
3506.394414	515723.337516	41.256832
3506.255901	515687.553655	41.261837
3506.372729	515635.343598	41.266842
3506.106964	515585.924816	41.271847
3506.085727	515553.561131	41.276852
3506.325785	515499.864539	41.281856
3506.322163	515468.357659	41.286861
3506.320747	515421.475877	41.291866
3506.057777	515380.805349	41.296871
3505.761260	515341.252656	41.301876
3506.132250	515303.212751	41.306880
3506.005783	515265.959425	41.311885
3506.222558	515233.608077	41.316890
3506.350308	515191.762694	41.321895
3506.218435	515142.119139	41.326900
3506.505577	515089.273561	41.331904
3505.712896	515062.796402	41.336909
3505.624351	515019.062918	41.341914
3505.649271	514980.722950	41.346919
3505.571874	514940.679500	41.351924
3506.039834	514923.207608	41.356928
3505.934515	514875.126905	41.361933
3505.877760	514844.335306	41.366938
3505.656126	514806.893695	41.371943
3505.566250	514768.975993	41.376948
3505.684632	514722.326199	41.381952
3505.180317	514718.359853	41.386957
3505.602028	514675.657502	41.391962
3505.691424	514642.212466	41.396967
3505.478512	514622.268478	41.401972
3505.705362	514591.431591	41.406976
3505.365101	514566.551164	41.411981
3505.426778	514534.577016	41.416986
3505.501548	514496.379791	41.421991
3505.629119	514482.349886	41.426996
3505.817124	514430.580013	41.432000
3505.899142	514415.596289	41.437005
3505.951025	514363.948879	41.442010
3505.764321	514335.958631	41.447015
3505.651156	514305.781885	41.452020
3505.663994	514272.449368	41.457024
3505.510220	514244.908960	41.462029
3505.678902	514205.634102	41.467034
3505.373273	514168.811274	41.472039
3505.080639	514144.276737	41.477044
3505.401183	514112.058559	41.482048
3505.434560	514085.601026	41.487053
3505.413759	514059.860108	41.492058
3505.229497	514031.970122	41.497063
3505.386755	514003.672065	41.502068
3505.054569	513983.341542	41.507072
3505.357808	513958.661978	41.512077
3505.351851	513930.693065	41.517082
3505.757347	513906.857098	41.522087
3505.406420	513880.409403	41.527092
3505.403303	513842.121843	41.532096
3505.576852	513828.084125	41.537101
3505.303555	513795.149936	41.542106
3505.482188	513766.443471	41.547111
3505.171928	513736.954381	41.552116
3505.214649	513699.822573	41.557120
3505.176188	513686.273458	41.562125
3505.227605	513651.163337	41.567130
3505.650464	513626.666698	41.572135
3505.402696	513608.244397	41.577140
3505.273706	513560.568305	41.582144
3505.229047	513543.428901	41.587149
3505.207682	513513.792601	41.592154
3505.384864	513480.634859	41.597159
3505.420905	513458.374047	41.602164
3505.293363	513428.450898	41.607168
3505.090467	513406.632422	41.612173
3505.052345	513380.539142	41.617178
3505.548191	513355.322452	41.622183
3505.207908	513346.625888	41.627188
3505.383244	513321.965608	41.632192
3504.929869	513294.015771	41.637197
3505.131329	513277.899387	41.642202
3505.371005	513249.789360	41.647207
3505.136019	513221.501403	41.652212
3505.274608	513183.493434	41.657216
3505.127676	513164.902967	41.662221
3505.004885	513136.647716	41.667226
3505.024589	513104.626904	41.672231
3504.815802	513092.368756	41.677236
3504.986933	513068.062837	41.682240
3505.251978	513045.208893	41.687245
3504.907852	513028.723270	41.692250
3504.986916	513003.015534	41.697255
3504.806194	512984.329046	41.702260
3504.983637	512960.274881	41.707264
3504.546419	512952.807388	41.712269
3504.616235	512932.563802	41.717274
3505.102207	512899.507858	41.722279
3504.786866	512885.951279	41.727284
3504.845289	512858.273901	41.732288
3505.181652	512845.777667	41.737293
3505.024774	512828.958764	41.742298
3505.127100	512799.352241	41.747303
3504.671526	512785.817745	41.752308
3505.281108	512756.080393	41.757312
3505.128710	512730.257079	41.762317
3505.071592	512709.830959	41.767322
3505.507190	512693.575848	41.772327
3505.188886	512676.276484	41.777332
3505.287565	512636.047971	41.782336
3505.389536	512611.094755	41.787341
3505.419603	512591.868693	41.792346
3505.330545	512556.829080	41.797351
3504.626484	512537.314324	41.802356
3505.025457	512504.676021	41.807360
3504.893520	512482.996883	41.812365
3504.742567	512471.133806	41.817370
3504.946917	512436.705149	41.822375
3504.455698	512430.004703	41.827380
3504.896357	512419.059744	41.832384
3504.750046	512394.145449	41.837389
3504.724405	512374.472696	41.842394
3505.109578	512352.610495	41.847399
3505.020533	512346.048784	41.852404
3504.864191	512312.587381	41.857408
3504.539404	512288.965723	41.862413
3504.284557	512284.757032	41.867418
3504.669144	512253.334522	41.872423
3504.773553	512260.146834	41.877428
3504.944844	512219.450604	41.882432
3504.612777	512222.689894	41.887437
3504.823112	512195.341508	41.892442
3504.682888	512178.620492	41.897447
3504.571477	512151.171135	41.902452
3504.666477	512135.829248	41.907456
3504.778593	512124.632523	41.912461
3504.265605	512106.908090	41.917466
3504.537609	512097.254180	41.922471
3504.258575	512090.115390	41.927476
3504.532330	512060.075808	41.932480
3504.394141	512063.385654	41.937485
3504.581445	512054.149779	41.942490
3504.640380	512037.093642	41.947495
3504.385799	512031.215567	41.952500
3504.970925	512017.313633	41.957504
3504.655938	512003.857458	41.962509
3504.599323	511982.671617	41.967514
3504.937385	511965.065447	41.972519
3504.700442	511949.877024	41.977524
3504.973082	511914.880086	41.982528
3504.894505	511918.736968	41.987533
3504.564410	511894.609753	41.992538
3504.989281	511871.172536	41.997543
3504.723541	511866.054937	42.002548
3505.045729	511831.657012	42.007552
3504.699348	511823.972321	42.012557
3504.451582	511801.754184	42.017562
3504.593868	511790.754811	42.022567
3504.645664	511765.201260	42.027572
3504.444464	511755.065512	42.032576
3504.578206	511726.615605	42.037581
3504.579706	511721.860405	42.042586
3504.527918	511695.260834	42.047591
3504.591897	511690.192239	42.052596
3504.906311	511665.355810	42.057600
3504.785970	511652.070932	42.062605
3504.482058	511644.632373	42.067610
3504.801630	511628.445168	42.072615
3504.388370	511608.428106	42.077620
3504.536924	511594.898342	42.082624
3504.495669	511577.351723	42.087629
3504.539580	511575.776669	42.092634
3504.505358	511552.006887	42.097639
3504.292578	511530.288722	42.102644
3504.561834	511515.930447	42.107648
3504.703359	511503.868708	42.112653
3504.601081	511488.860930	42.117658
3504.632059	511477.120159	42.122663
3504.692713	511465.374690	42.127668
3504.305816	511440.244088	42.132672
3504.503150	511446.839697	42.137677
3504.175645	511436.521376	42.142682
3504.420127	511408.407536	42.147687
3504.175288	511404.551145	42.152692
3504.522994	511411.274760	42.157696
3504.537671	511382.438407	42.162701
3504.420337	511374.413793	42.167706
3504.702035	511362.734489	42.172711
3504.495619	511334.540033	42.177716
3504.560941	511326.486528	42.182720
3504.349622	511312.052277	42.187725
3503.920104	511299.574784	42.192730
3504.130213	511281.431681	42.197735
3504.181061	511287.392881	42.202740
3504.122397	511282.292962	42.207744
3504.250730	511262.038133	42.212749
3504.260216	511260.063799	42.217754
3504.448520	511246.780408	42.222759
3504.123701	511247.590582	42.227764
3504.498010	511230.787310	42.232768
3504.275294	511230.771962	42.237773
3504.154523	511221.938434	42.242778
3504.553092	511214.287485	42.247783
3504.135488	511195.788221	42.252788
3504.429509	511185.067995	42.257792
3504.701053	511176.425371	42.262797
3504.477723	511163.409321	42.267802
3504.765034	511145.759740	42.272807
3504.472211	511125.318378	42.277812
3504.579116	511109.670162	42.282816
3504.545065	511107.803865	42.287821
3504.659167	511083.150007	42.292826
3504.870110	511062.477188	42.297831
3504.536118	511051.856136	42.302836
3504.265278	511036.419316	42.307840
3504.538002	511028.838762	42.312845
3504.448549	511005.481643	42.317850
3504.400906	510986.215457	42.322855
3504.356880	510989.965914	42.327860
3504.644727	510965.486775	42.332864
3504.614475	510949.000103	42.337869
3504.356209	510943.324581	42.342874
3504.764505	510913.969936	42.347879
3504.499787	510910.470686	42.352884
3504.738133	510899.253205	42.357888
3504.938735	510878.733560	42.362893
3504.790124	510867.121928	42.367898
3504.901062	510829.214230	42.372903
3504.503312	510827.810088	42.377908
3504.668295	510807.751277	42.382912
3504.348391	510798.898415	42.387917
3504.217585	510794.821509	42.392922
3504.612964	510764.456891	42.397927
3504.388968	510772.080526	42.402932
3504.312055	510757.270446	42.407936
3504.562556	510728.901594	42.412941
3504.214605	510728.349569	42.417946
3504.343054	510706.019950	42.422951
3504.236940	510699.359124	42.427956
3504.391252	510666.654789	42.432960
3504.554494	510672.345499	42.437965
3503.965579	510670.566851	42.442970
3504.213500	510645.790034	42.447975
3504.328634	510634.136558	42.452980
3504.369066	510640.049042	42.457984
3504.365365	510633.675534	42.462989
3504.377671	510616.979461	42.467994
3504.504266	510605.374742	42.472999
3504.486873	510600.116331	42.478004
3504.731195	510578.577646	42.483008
3504.841935	510561.865962	42.488013
3504.619899	510536.758556	42.493018
3504.647989	510511.662169	42.498023
3504.654069	510506.298841	42.503028
3504.590141	510493.661795	42.508032
3504.698935	510488.130462	42.513037
3504.916965	510447.220251	42.518042
3504.762586	510434.850401	42.523047
3504.842360	510424.214150	42.528052
3504.481543	510413.394582	42.533056
3504.674701	510388.322513	42.538061
3504.348232	510366.620830	42.543066
3504.874382	510347.718537	42.548071
3504.420881	510344.350185	42.553076
3504.472066	510307.057842	42.558080
3504.444428	510315.105949	42.563085
3504.417428	510289.259103	42.568090
3504.499986	510278.521141	42.573095
3504.337779	510271.363119	42.578100
3504.565322	510248.966651	42.583104
3504.540609	510237.385597	42.588109
3504.298912	510231.302501	42.593114
3504.540019	510204.502540	42.598119
3504.274396	510197.310242	42.603124
3504.427801	510196.375421	42.608128
3504.397661	510182.569242	42.613133
3504.170037	510171.627290	42.618138
3504.385410	510159.755288	42.623143
3504.275778	510164.123373	42.628148
3504.213548	510134.032320	42.633152
3504.119160	510133.035480	42.638157
3503.948119	510137.362687	42.643162
3504.256238	510122.693561	42.648167
3504.097213	510112.297217	42.653172
3504.246796	510100.688522	42.658176
3504.080225	510091.912236	42.663181
3504.050388	510089.994572	42.668186
3504.178704	510077.680963	42.673191
3504.220733	510066.291604	42.678196
3504.269257	510052.978788	42.683200
3504.498685	510054.004957	42.688205
3504.244223	510047.316732	42.693210
3504.487285	510019.453780	42.698215
3503.986869	510030.814515	42.703220
3503.972299	510013.363248	42.708224
3504.311703	510022.213515	42.713229
3504.354179	509995.899933	42.718234
3504.234051	509975.328715	42.723239
3504.037005	509989.929899	42.728244
3504.247158	509966.018101	42.733248
3504.010466	509955.836299	42.738253
3504.043028	509948.343815	42.743258
3504.537259	509938.855925	42.748263
3504.350184	509941.516232	42.753268
3504.377376	509911.764788	42.758272
3504.495511	509900.312700	42.763277
3504.518931	509906.986985	42.768282
3504.552550	509883.963013	42.773287
3504.220359	509883.914373	42.778292
3504.155159	509870.669980	42.783296
3504.297492	509856.431554	42.788301
3504.117605	509838.702694	42.793306
3504.393923	509822.824160	42.798311
3504.325144	509827.034101	42.803316
3504.143255	509805.055899	42.808321
3504.142344	509796.354460	42.813325
3504.396672	509784.981951	42.818330
3504.376832	509781.848491	42.823335
3504.224003	509772.513369	42.828340
3504.317178	509752.970580	42.833345
3504.496113	509743.431234	42.838349
3504.567648	509737.045500	42.843354
3504.741001	509719.817187	42.848359
3504.526425	509715.702672	42.853364
3504.675105	509674.750984	42.858369
3504.610029	509669.550414	42.863373
3504.270040	509661.054271	42.868378
3504.316811	509641.215142	42.873383
3504.320851	509635.143585	42.878388
3504.554575	509625.544923	42.883393
3504.690380	509602.200874	42.888397
3504.416401	509597.539213	42.893402
3504.193834	509584.319471	42.898407
3504.311376	509574.081453	42.903412
3504.396605	509569.110054	42.908417
3504.554115	509559.422217	42.913421
3504.401413	509532.481081	42.918426
3504.711268	509515.180397	42.923431
3504.505335	509519.816824	42.928436
3504.385085	509492.465763	42.933441
3504.550414	509477.262145	42.938445
3504.435196	509468.882156	42.943450
3504.534934	509441.293877	42.948455
3504.541270	509441.242322	42.953460
3504.661999	509432.825024	42.958465
3504.573551	509417.762646	42.963469
3504.557809	509398.287260	42.968474
3504.630605	509370.045428	42.973479
3504.319061	509368.475759	42.978484
3504.431788	509348.119945	42.983489
3504.350269	509333.005806	42.988493
3504.042377	509328.754169	42.993498
3504.513001	509320.838029	42.998503
3504.435688	509306.633862	43.003508
3504.189720	509278.846999	43.008513
3504.561415	509278.029405	43.013517
3504.518246	509277.631527	43.018522
3504.686385	509253.421823	43.023527
3504.387629	509248.308651	43.028532
3504.398362	509228.930073	43.033537
3504.335435	509203.694376	43.038541
3504.192941	509196.431602	43.043546
3504.342192	509197.672866	43.048551
3504.401674	509182.637494	43.053556
3504.319456	509151.485429	43.058561
3504.506303	509155.604540	43.063565
3504.276492	509146.078872	43.068570
3504.505755	509121.707543	43.073575
3504.244820	509120.079259	43.078580
3504.411405	509106.139935	43.083585
3504.745960	509086.558237	43.088589
3504.522367	509085.025234	43.093594
3504.742573	509055.697135	43.098599
3504.410599	509044.872139	43.103604
3504.453631	509031.964143	43.108609
3504.449704	509005.352816	43.113613
3504.411129	509009.709963	43.118618
3504.663057	508987.409181	43.123623
3504.604151	508972.544117	43.128628
3504.120812	508951.067803	43.133633
3504.320549	508955.286112	43.138637
3504.348927	508942.734518	43.143642
3504.240846	508921.957758	43.148647
3504.307631	508923.718010	43.153652
3504.361439	508911.263561	43.158657
3504.410543	508892.637441	43.163661
3503.968359	508881.627387	43.168666
3504.555881	508872.630102	43.173671
3504.399020	508858.640511	43.178676
3503.873876	508846.682268	43.183681
3503.874504	508838.182475	43.188685
3504.151238	508841.933299	43.193690
3504.386244	508827.224030	43.198695
3504.227813	508814.347712	43.203700
3504.496778	508793.460610	43.208705
3504.298042	508796.375905	43.213709
3503.698219	508799.101623	43.218714
3503.986014	508774.062831	43.223719
3503.864877	508764.519775	43.228724
3504.070310	508753.457876	43.233729
3504.164293	508751.368710	43.238733
3504.114179	508762.760296	43.243738
3504.264524	508742.397819	43.248743
3504.246445	508736.278847	43.253748
3504.155982	508720.153702	43.258753
3504.410858	508704.783466	43.263757
3504.150889	508717.523695	43.268762
3504.391031	508677.617648	43.273767
3504.393489	508688.191469	43.278772
3504.252941	508688.112533	43.283777
3504.423491	508658.032693	43.288781
3504.249669	508653.911480	43.293786
3504.438622	508639.006952	43.298791
3504.094072	508631.725280	43.303796
3504.298150	508609.735137	43.308801
3504.378649	508607.496301	43.313805
3503.990232	508603.358399	43.318810
3504.062767	508604.004700	43.323815
3503.916734	508582.474613	43.328820
3504.129750	508562.456179	43.333825
3504.197706	508564.975200	43.338829
3503.932430	508558.844640	43.343834
3504.447759	508550.313949	43.348839
3504.073872	508539.039908	43.353844
3504.155855	508531.387211	43.358849
3504.442953	508512.470091	43.363853
3504.128672	508524.864884	43.368858
3504.237740	508506.886599	43.373863
3504.040173	508487.135349	43.378868
3504.279589	508479.356558	43.383873
3504.253704	508474.301215	43.388877
3504.102324	508465.622883	43.393882
3504.315693	508448.235189	43.398887
3504.019060	508441.805974	43.403892
3503.923807	508434.838980	43.408897
3504.418291	508431.927552	43.413901
3504.014311	508420.658189	43.418906
3504.592485	508401.441968	43.423911
3504.264941	508396.889635	43.428916
3504.129287	508391.295072	43.433921
3504.349677	508372.135367	43.438925
3504.160238	508376.162353	43.443930
3504.513696	508350.100668	43.448935
3504.237942	508350.346670	43.453940
3504.150269	508320.813005	43.458945
3504.205758	508309.926305	43.463949
3503.971866	508327.165674	43.468954
3504.285123	508320.538830	43.473959
3504.552295	508305.216889	43.478964
3504.455337	508288.485224	43.483969
3504.595424	508287.147644	43.488973
3504.222829	508261.251174	43.493978
3504.508286	508238.488766	43.498983
3504.370730	508237.043278	43.503988
3504.334695	508230.269223	43.508993
3504.670982	508202.995739	43.513997
3504.269529	508205.943172	43.519002
3504.367916	508181.034647	43.524007
3504.365267	508161.353408	43.529012
3504.093585	508162.711873	43.534017
3504.314240	508150.432886	43.539021
3504.360404	508154.625069	43.544026
3504.514891	508119.436665	43.549031
3504.084448	508121.983928	43.554036
3504.041830	508120.118659	43.559041
3504.296591	508087.191150	43.564045
3503.812163	508089.848142	43.569050
3504.048864	508084.599395	43.574055
3504.311613	508088.959746	43.579060
3504.083367	508058.385336	43.584065
3503.932938	508046.367310	43.589069
3504.192152	508042.784659	43.594074
3504.116633	508042.644845	43.599079
3504.244204	508039.690153	43.604084
3504.244168	508026.181058	43.609089
3504.415736	508014.820462	43.614093
3504.411712	508000.704825	43.619098
3504.383814	507987.301295	43.624103
3503.999809	507981.543467	43.629108
3504.161915	507970.589107	43.634113
3504.177125	507965.324735	43.639117
3503.741903	507970.048412	43.644122
3504.564708	507952.513300	43.649127
3504.444172	507940.794053	43.654132
3504.335718	507932.614630	43.659137
3504.371911	507918.037202	43.664141
3504.245558	507897.717461	43.669146
3504.242427	507891.747616	43.674151
3504.232298	507884.665752	43.679156
3504.231506	507877.683603	43.684161
3504.188489	507846.978349	43.689165
3503.754095	507841.582613	43.694170
3504.097530	507837.986610	43.699175
3503.984078	507840.230830	43.704180
3503.844908	507838.380790	43.709185
3504.279267	507831.582828	43.714189
3504.190947	507817.277978	43.719194
3504.027610	507804.553470	43.724199
3504.071199	507808.847337	43.729204
3504.269226	507809.322044	43.734209
3504.239034	507781.346867	43.739213
3503.845252	507778.373337	43.744218
3504.024713	507757.903903	43.749223
3504.012855	507763.572660	43.754228
3504.135861	507760.568045	43.759233
3504.503850	507758.081274	43.764237
3504.091981	507737.553487	43.769242
3503.998933	507718.695581	43.774247
3503.750779	507723.035580	43.779252
3503.918779	507724.678764	43.784257
3504.234265	507715.622684	43.789261
3503.866808	507702.525586	43.794266
3504.225028	507684.760050	43.799271
3504.329895	507682.011274	43.804276
3504.075573	507688.730318	43.809281
3503.952717	507671.344385	43.814285
3503.690058	507664.099955	43.819290
3504.025602	507649.980959	43.824295
3503.844536	507648.289312	43.829300
3503.909155	507649.847649	43.834305
3504.003783	507649.630342	43.839309
3503.892063	507653.999393	43.844314
3504.290219	507650.445299	43.849319
3504.196542	507627.792607	43.854324
3504.222354	507614.380299	43.859329
3504.468424	507606.650662	43.864333
3503.963311	507614.370720	43.869338
3504.052111	507590.373610	43.874343
3504.126034	507581.001458	43.879348
3503.927268	507575.416605	43.884353
3504.378811	507565.377592	43.889357
3503.914330	507579.921891	43.894362
3504.111666	507563.395995	43.899367
3504.247366	507543.692186	43.904372
3503.848328	507542.034979	43.909377
3504.151740	507531.007409	43.914381
3503.814907	507532.932792	43.919386
3504.001375	507515.143631	43.924391
3503.970287	507526.836611	43.929396
3503.640150	507506.902801	43.934401
3504.112064	507486.892800	43.939405
3504.004571	507497.838911	43.944410
3504.054915	507492.214658	43.949415
3504.196072	507491.787606	43.954420
3504.087852	507494.334629	43.959425
3503.886496	507469.877235	43.964429
3504.146252	507463.258519	43.969434
3504.168968	507457.385634	43.974439
3503.868725	507461.177356	43.979444
3504.160053	507453.895877	43.984449
3504.306497	507437.226111	43.989453
3504.241391	507422.259494	43.994458
3504.403857	507412.974451	43.999463
3504.262605	507419.979315	44.004468
3504.094818	507392.784224	44.009473
3504.395471	507369.158106	44.014477
3504.362989	507373.464105	44.019482
3504.640850	507354.294189	44.024487
3504.546049	507347.276086	44.029492
3504.354279	507352.619226	44.034497
3504.611233	507312.251986	44.039501
3503.949103	507306.487291	44.044506
3503.929556	507302.594360	44.049511
3504.035938	507293.115725	44.054516
3503.778077	507284.301833	44.059521
3504.076769	507287.391752	44.064525
3504.096769	507260.622157	44.069530
3504.098516	507260.874910	44.074535
3503.918004	507251.694589	44.079540
3504.065126	507257.743170	44.084545
3504.054759	507245.955441	44.089549
3503.933602	507240.560606	44.094554
3503.816978	507216.899035	44.099559
3504.180597	507218.814941	44.104564
3503.892108	507210.815427	44.109569
3504.594407	507210.906859	44.114573
3504.227017	507208.789231	44.119578
3504.258436	507181.815316	44.124583
3504.139159	507176.420164	44.129588
3503.991447	507174.217213	44.134593
3503.768303	507166.308547	44.139597
3504.078717	507172.533744	44.144602
3504.247168	507140.883040	44.149607
3503.998623	507137.582851	44.154612
3504.134443	507133.209939	44.159617
3504.387089	507132.613461	44.164621
3503.882053	507118.373894	44.169626
3504.184094	507095.809758	44.174631
3504.583471	507092.305957	44.179636
3504.280066	507092.657542	44.184641
3504.355430	507065.271709	44.189645
3504.065268	507046.191230	44.194650
3504.191442	507043.135391	44.199655
3503.989294	507052.173985	44.204660
3504.291205	507045.953239	44.209665
3504.441507	507024.070778	44.214669
3504.166463	507009.946568	44.219674
3504.147725	507014.958870	44.224679
3503.996123	507020.548759	44.229684
3504.200978	506997.696261	44.234689
3504.259859	506972.488646	44.239693
3504.212815	506976.695847	44.244698
3504.041471	506964.073183	44.249703
3503.939019	506943.950940	44.254708
3504.192193	506934.954901	44.259713
3504.447791	506924.187500	44.264717
3503.962595	506925.478607	44.269722
3504.326138	506927.192160	44.274727
3504.609276	506900.026224	44.279732
3504.059631	506893.535219	44.284737
3504.293311	506884.947031	44.289741
3503.974642	506884.997435	44.294746
3503.979065	506864.099217	44.299751
3503.997540	506864.652929	44.304756
3504.078787	506856.847810	44.309761
3504.503411	506845.800648	44.314765
3504.185190	506842.005420	44.319770
3504.127747	506823.343309	44.324775
3504.341888	506820.931322	44.329780
3503.782574	506816.111602	44.334785
3503.880282	506810.277244	44.339789
3503.976810	506813.196803	44.344794
3504.173272	506791.660950	44.349799
3504.230918	506779.406756	44.354804
3504.354951	506774.529620	44.359809
3504.127814	506770.770579	44.364813
3503.949684	506759.565631	44.369818
3504.286682	506734.060714	44.374823
3504.067897	506731.261741	44.379828
3503.637850	506743.979702	44.384833
3503.751088	506735.511676	44.389837
3503.986655	506724.696717	44.394842
3504.046889	506731.315814	44.399847
3503.817790	506717.234704	44.404852
3503.783849	506704.438334	44.409857
3504.144274	506695.678220	44.414861
3503.771227	506705.300604	44.419866
3504.478484	506697.244672	44.424871
3504.411198	506696.344546	44.429876
3504.210137	506684.738374	44.434881
3504.269983	506664.084155	44.439885
3504.137827	506661.423279	44.444890
3504.036623	506654.608307	44.449895
3504.122573	506630.812719	44.454900
3503.948260	506626.488696	44.459905
3504.290695	506617.124185	44.464909
3504.022559	506618.178605	44.469914
3503.915083	506618.651032	44.474919
3503.877950	506617.341335	44.479924
3503.729991	506599.047490	44.484929
3503.935483	506567.946489	44.489933
3503.843563	506579.042519	44.494938
3504.448002	506574.797802	44.499943
3504.242831	506577.967485	44.504948
3504.330252	506564.291626	44.509953
3504.572134	506545.177104	44.514957
3504.208936	506536.075877	44.519962
3504.430199	506523.188438	44.524967
3504.504825	506502.936494	44.529972
3504.096189	506498.092870	44.534977
3504.157977	506491.909879	44.539981
3503.939995	506478.079819	44.544986
3504.164227	506466.709886	44.549991
3504.027625	506453.372951	44.554996
3504.174853	506457.043566	44.560001
3504.661937	506445.075467	44.565005
3503.910128	506424.802251	44.570010
3504.169657	506417.575966	44.575015
3504.380187	506416.834319	44.580020
3504.288508	506403.186640	44.585025
3504.367210	506390.372236	44.590029
3503.896157	506376.885699	44.595034
3504.245485	506374.806490	44.600039
3504.354064	506383.846921	44.605044
3503.853333	506367.835025	44.610049
3504.457515	506344.665550	44.615053
3504.035238	506341.493869	44.620058
3504.313414	506331.026138	44.625063
3504.198762	506327.805833	44.630068
3504.161341	506310.152026	44.635073
3503.832805	506293.809240	44.640077
3503.854177	506300.738250	44.645082
3504.176260	506284.849236	44.650087
3503.922704	506297.691431	44.655092
3503.887549	506292.434511	44.660097
3504.221558	506261.009042	44.665101
3504.043530	506263.263671	44.670106
3504.041991	506250.765453	44.675111
3504.326941	506245.862736	44.680116
3504.009881	506237.462476	44.685121
3504.056845	506217.012167	44.690125
3504.083633	506223.333136	44.695130
3503.765927	506211.795685	44.700135
3504.150020	506208.648334	44.705140
3503.902059	506223.463152	44.710145
3504.055882	506215.241464	44.715149
3504.268869	506179.432659	44.720154
3504.185680	506172.867658	44.725159
3504.487796	506172.668142	44.730164
3503.939970	506158.991163	44.735169
3504.251199	506137.385760	44.740173
3503.782630	506135.334591	44.745178
3504.033870	506123.251743	44.750183
3504.219605	506132.533118	44.755188
3504.171876	506126.063697	44.760193
3504.200717	506105.211308	44.765197
3504.052017	506088.991710	44.770202
3503.893066	506081.021801	44.775207
3503.918096	506084.306994	44.780212
3503.605924	506083.698550	44.785217
3504.283550	506083.490285	44.790221
3503.915859	506078.032849	44.795226
3504.074763	506056.097208	44.800231
3504.021216	506049.578077	44.805236
3503.801706	506046.930913	44.810241
3504.007393	506042.445481	44.815245
3503.783236	506052.854321	44.820250
3504.039518	506042.946498	44.825255
3504.268523	506043.972980	44.830260
3504.006102	506015.475038	44.835265
3504.361598	506012.281571	44.840269
3504.131218	506007.106022	44.845274
3503.681353	505997.613394	44.850279
3503.835407	505997.589083	44.855284
3503.877977	505991.712564	44.860289
3504.281718	505970.193536	44.865293
3504.095007	505975.789309	44.870298
3504.020398	505962.239790	44.875303
3504.042048	505961.780988	44.880308
3503.933262	505954.106703	44.885313
3503.913514	505938.170196	44.890317
3503.537993	505934.130813	44.895322
3503.925031	505911.956525	44.900327
3503.946054	505922.579702	44.905332
3503.599469	505925.670650	44.910337
3503.888344	505915.453991	44.915341
3503.713680	505922.110523	44.920346
3503.898945	505918.488524	44.925351
3503.953035	505925.867932	44.930356
3503.780777	505919.063901	44.935361
3503.828918	505906.962402	44.940365
3504.016443	505905.617143	44.945370
3504.026084	505886.943424	44.950375
3504.127625	505887.332231	44.955380
3504.019053	505885.983168	44.960385
3504.177360	505882.365423	44.965389
3503.677797	505871.868534	44.970394
3503.983061	505845.051670	44.975399
3503.801225	505851.810567	44.980404
3503.841719	505855.093360	44.985409
3504.179460	505839.859297	44.990413
3503.863585	505852.458657	44.995418
3504.088767	505848.830335	45.000423
3504.024101	505840.794810	45.005428
3503.986297	505824.355029	45.010433
3504.025432	505809.117532	45.015437
3504.012379	505803.300343	45.020442
3503.898355	505800.079841	45.025447
3504.073295	505805.770315	45.030452
3503.748586	505807.693968	45.035457
3503.949693	505793.999536	45.040461
3503.969332	505786.456687	45.045466
3503.921205	505772.042591	45.050471
3504.165173	505772.560698	45.055476
3503.631321	505773.808973	45.060481
3503.673880	505765.098633	45.065485
3503.649593	505772.186878	45.070490
3503.878322	505773.314626	45.075495
3504.263611	505770.571829	45.080500
3503.910521	505749.323956	45.085505
3504.327323	505743.793026	45.090509
3503.984092	505738.635234	45.095514
3504.076131	505741.707491	45.100519
3504.256750	505740.059695	45.105524
3503.904959	505722.859800	45.110529
3503.838289	505705.513619	45.115533
3503.690682	505708.218936	45.120538
3503.884140	505706.113683	45.125543
3503.778747	505707.547257	45.130548
3503.563424	505703.937925	45.135553
3504.126609	505691.906681	45.140557
3503.710671	505712.061781	45.145562
3503.908555	505702.618421	45.150567
3503.978359	505696.636292	45.155572
3503.723202	505678.662038	45.160577
3504.005609	505660.197979	45.165581
3503.803836	505666.454069	45.170586
3503.977690	505649.727655	45.175591
3504.353435	505663.027486	45.180596
3503.891616	505665.630663	45.185601
3504.144579	505643.021798	45.190605
3503.942394	505623.622231	45.195610
3503.886409	505620.797347	45.200615
3503.925570	505617.552599	45.205620
3503.666493	505622.299670	45.210625
3503.803172	505616.306945	45.215629
3503.962299	505614.611931	45.220634
3503.885060	505617.710964	45.225639
3503.964984	505617.293546	45.230644
3503.780747	505598.245335	45.235649
3503.986760	505583.133075	45.240653
3503.725913	505580.745388	45.245658
3504.001998	505582.624711	45.250663
3503.785219	505587.871138	45.255668
3503.712869	505587.680199	45.260673
3504.190546	505574.447913	45.265677
3503.749569	505579.982793	45.270682
3503.928988	505548.175648	45.275687
3503.589954	505542.359291	45.280692
3503.523743	505547.430122	45.285697
3503.681270	505540.877440	45.290701
3503.473027	505547.438215	45.295706
3503.936412	505538.762455	45.300711
3503.815058	505549.813189	45.305716
3503.860146	505546.769905	45.310721
3504.165959	505550.466251	45.315725
3504.067970	505550.178157	45.320730
3504.192887	505543.327010	45.325735
3504.318411	505519.726062	45.330740
3503.739707	505515.162057	45.335745
3503.878659	505508.258074	45.340749
3503.835922	505502.141856	45.345754
3504.081196	505507.011658	45.350759
3503.940913	505511.284552	45.355764
3503.668951	505501.358706	45.360769
3504.063050	505475.134475	45.365773
3503.942976	505474.748664	45.370778
3503.725932	505459.500748	45.375783
3503.837571	505459.786762	45.380788
3503.714823	505472.001647	45.385793
3504.195950	505468.737622	45.390797
3504.161065	505466.870844	45.395802
3504.104709	505458.277191	45.400807
3503.739276	505440.218913	45.405812
3503.878094	505433.517337	45.410817
3504.122400	505427.507536	45.415821
3503.879943	505436.199112	45.420826
3504.123782	505432.162926	45.425831
3504.209284	505423.293817	45.430836
3503.943399	505401.626907	45.435841
3503.877170	505380.130829	45.440845
3503.681866	505386.082374	45.445850
3503.986920	505381.429257	45.450855
3504.012419	505386.536243	45.455860
3504.227208	505392.321763	45.460865
3504.263671	505367.520196	45.465869
3504.017690	505345.141617	45.470874
3503.992944	505354.507278	45.475879
3504.157499	505345.220804	45.480884
3503.781276	505340.978977	45.485889
3504.136872	505351.245999	45.490893
3504.144305	505329.586405	45.495898
3504.280569	505315.041579	45.500903
3504.389768	505291.797132	45.505908
3503.956337	505306.793852	45.510913
3504.499482	505289.350875	45.515917
3504.109209	505277.267627	45.520922
3504.278608	505260.642753	45.525927
3504.155930	505254.387271	45.530932
3504.049949	505253.543790	45.535937
3504.166258	505236.623659	45.540941
3504.098512	505223.123085	45.545946
3504.093168	505218.923818	45.550951
3504.236045	505219.053087	45.555956
3504.077861	505206.123440	45.560961
3504.300918	505188.933370	45.565965
3504.069664	505188.565124	45.570970
3504.134833	505176.308614	45.575975
3504.307955	505175.572829	45.580980
3504.165333	505159.958658	45.585985
3504.147524	505142.351172	45.590989
3504.012473	505145.661844	45.595994
3503.788016	505145.444336	45.600999
3504.035439	505138.826691	45.606004
3503.933366	505130.796751	45.611009
3503.916390	505109.393764	45.616013
3503.662488	505114.848618	45.621018
3504.015276	505103.406875	45.626023
3504.022221	505100.217728	45.631028
3503.941832	505105.240323	45.636033
3504.357661	505096.116421	45.641037
3504.060460	505081.690517	45.646042
3503.854835	505066.238033	45.651047
3503.958368	505071.838825	45.656052
3503.808652	505059.059545	45.661057
3504.454864	505049.140135	45.666061
3503.761184	505053.196979	45.671066
3503.916149	505028.679830	45.676071
3504.301513	505016.321996	45.681076
3503.867930	505013.506088	45.686081
3504.033313	505017.528373	45.691085
3503.917478	505018.002162	45.696090
3504.005109	505017.937745	45.701095
3503.976651	504989.552962	45.706100
3503.857290	504981.120847	45.711105
3503.957214	504976.044600	45.716109
3503.856763	504981.070402	45.721114
3503.962729	504972.855694	45.726119
3504.209053	504972.968615	45.731124
3503.886055	504982.432219	45.736129
3504.042008	504960.849904	45.741133
3503.945900	504948.213885	45.746138
3503.721622	504939.494702	45.751143
3503.842634	504943.625226	45.756148
3503.937619	504928.934789	45.761153
3504.246684	504934.351325	45.766157
3504.057975	504938.227173	45.771162
3504.087249	504938.880450	45.776167
3504.030393	504907.615534	45.781172
3503.961659	504915.875070	45.786177
3504.011956	504902.406196	45.791181
3503.969971	504908.131250	45.796186
3504.516088	504898.531207	45.801191
3504.556230	504874.487437	45.806196
3504.021825	504873.408019	45.811201
3504.090269	504858.721718	45.816205
3504.323584	504842.136950	45.821210
3504.105883	504831.999725	45.826215
3504.377957	504811.461585	45.831220
3504.191370	504814.021384	45.836225
3504.306284	504799.530110	45.841229
3503.906455	504784.512915	45.846234
3504.064909	504776.239214	45.851239
3504.300678	504781.262538	45.856244
3503.795297	504779.267628	45.861249
3504.243840	504764.268145	45.866253
3504.039489	504740.870100	45.871258
3504.039033	504746.993488	45.876263
3504.164148	504724.960306	45.881268
3504.236964	504734.361484	45.886273
3504.249570	504709.613361	45.891277
3503.706500	504711.217404	45.896282
3504.117383	504683.622982	45.901287
3504.106026	504688.533574	45.906292
3504.259555	504679.805154	45.911297
3504.346253	504672.605467	45.916301
3504.335330	504650.897328	45.921306
3504.207245	504646.818534	45.926311
3504.167536	504644.345160	45.931316
3504.208150	504638.266072	45.936321
3504.241628	504611.338457	45.941325
3503.888455	504611.748557	45.946330
3504.110171	504602.604473	45.951335
3504.428130	504596.127293	45.956340
3503.713780	504588.446907	45.961345
3503.988254	504557.938696	45.966349
3504.214202	504564.228788	45.971354
3503.996186	504557.735094	45.976359
3504.418202	504562.982075	45.981364
3504.066970	504540.821525	45.986369
3504.163452	504527.345063	45.991373
3504.102596	504527.152295	45.996378
3504.185143	504512.311656	46.001383
3504.221678	504508.611662	46.006388
3504.066637	504494.719473	46.011393
3504.407254	504481.457421	46.016397
3504.052351	504482.272648	46.021402
3503.828113	504470.010779	46.026407
3504.454161	504473.859167	46.031412
3503.922233	504461.747136	46.036417
3504.187035	504443.993068	46.041421
3503.974529	504450.048862	46.046426
3504.066161	504446.137720	46.051431
3504.407387	504432.268258	46.056436
3504.074214	504414.406245	46.061441
3504.103214	504404.077960	46.066445
3503.985079	504402.021800	46.071450
3503.811533	504403.820498	46.076455
3503.840979	504399.463716	46.081460
3503.535417	504391.060746	46.086465
3503.900547	504361.549998	46.091469
3503.495309	504353.466404	46.096474
3503.794956	504354.785463	46.101479
3503.817111	504358.628111	46.106484
3503.506890	504359.183247	46.111489
3503.712368	504358.492922	46.116493
3503.787305	504365.313021	46.121498
3503.292126	504351.980545	46.126503
3503.789578	504350.889825	46.131508
3503.453723	504370.021675	46.136513
3503.825850	504353.971179	46.141517
3503.538634	504355.129961	46.146522
3503.643825	504365.184108	46.151527
3503.969154	504354.505319	46.156532
3503.409488	504362.893314	46.161537
3503.784043	504351.397035	46.166541
3503.854037	504366.972878	46.171546
3503.470917	504358.936397	46.176551
3503.648655	504350.254594	46.181556
3503.731999	504367.447741	46.186561
3503.966108	504365.487724	46.191565
3503.936005	504363.974319	46.196570
3503.770021	504360.964189	46.201575
3504.095602	504328.372627	46.206580
3504.025603	504331.268316	46.211585
3503.995018	504333.651707	46.216589
3504.042411	504327.115979	46.221594
3503.980028	504330.820173	46.226599
3504.099761	504322.957233	46.231604
3503.590690	504312.309083	46.236609
3503.774598	504292.695194	46.241613
3504.170381	504286.711669	46.246618
3503.823537	504286.715920	46.251623
3504.226070	504285.387164	46.256628
3503.866475	504295.211170	46.261633
3504.143201	504281.554211	46.266637
3504.231222	504265.700360	46.271642
3504.059192	504259.502929	46.276647
3504.113736	504245.931665	46.281652
3503.860947	504241.467631	46.286657
3503.878511	504255.432433	46.291661
3503.725377	504256.063959	46.296666
3503.835850	504237.220720	46.301671
3504.180762	504224.413259	46.306676
3503.499902	504217.284093	46.311681
3503.892125	504201.179674	46.316685
3503.577627	504205.682850	46.321690
3503.456672	504211.066363	46.326695
3503.587910	504194.952582	46.331700
3503.634504	504207.040369	46.336705
3504.150857	504206.756367	46.341709
3504.028875	504202.929541	46.346714
3503.971939	504202.179471	46.351719
3504.119551	504219.514427	46.356724
3503.473228	504194.566080	46.361729
3503.929866	504162.864426	46.366733
3504.005262	504168.672383	46.371738
3503.890311	504165.907190	46.376743
3504.227269	504169.902552	46.381748
3504.023668	504168.163516	46.386753
3504.130509	504168.753955	46.391757
3503.819466	504153.772792	46.396762
3503.914715	504132.350874	46.401767
3504.285881	504127.889407	46.406772
3503.874446	504129.826947	46.411777
3503.808253	504123.157273	46.416781
3503.853383	504133.980156	46.421786
3503.641636	504124.954942	46.426791
3503.841977	504128.567047	46.431796
3503.718213	504120.793109	46.436801
3504.150947	504093.649774	46.441805
3503.866350	504100.020727	46.446810
3503.870837	504096.123281	46.451815
3503.900029	504086.452676	46.456820
3503.971690	504082.089143	46.461825
3503.788116	504088.950208	46.466829
3503.648411	504093.931861	46.471834
3503.772402	504091.331320	46.476839
3504.158374	504075.835066	46.481844
3503.832197	504067.637628	46.486849
3504.082235	504047.557546	46.491853
3504.101986	504043.961322	46.496858
3504.065847	504054.442846	46.501863
3504.321369	504047.266827	46.506868
3503.971057	504036.694631	46.511873
3504.086516	504011.878660	46.516877
3503.916675	504002.998583	46.521882
3503.841312	504010.854730	46.526887
3504.092189	504008.183515	46.531892
3503.741537	504012.692454	46.536897
3503.997975	504000.961576	46.541901
3504.236048	503988.879339	46.546906
3504.223255	503971.269884	46.551911
3504.171565	503963.838740	46.556916
3503.985959	503970.295309	46.561921
3504.193539	503960.090362	46.566925
3503.961436	503936.948669	46.571930
3503.994148	503927.328028	46.576935
3504.239742	503911.448953	46.581940
3504.117503	503921.944165	46.586945
3504.057628	503913.299701	46.591949
3504.265777	503892.416334	46.596954
3504.138300	503882.669163	46.601959
3504.213587	503888.325407	46.606964
3504.206507	503875.674542	46.611969
3504.201368	503866.414107	46.616973
3503.859923	503850.324111	46.621978
3503.732838	503839.665907	46.626983
3504.464753	503840.461212	46.631988
3503.746054	503840.321801	46.636993
3503.833505	503833.880774	46.641997
3504.088006	503826.350569	46.647002
3503.648599	503823.181129	46.652007
3503.936990	503804.511739	46.657012
3503.859971	503796.831485	46.662017
3503.866980	503803.358889	46.667021
3503.803768	503804.836559	46.672026
3503.670758	503808.855676	46.677031
3504.334420	503812.698267	46.682036
3503.763141	503818.102467	46.687041
3503.755229	503798.164086	46.692045
3503.827970	503769.052815	46.697050
3503.577826	503768.181438	46.702055
3503.787747	503760.759468	46.707060
3503.519574	503760.295808	46.712065
3503.971974	503768.574733	46.717069
3503.711701	503771.652412	46.722074
3503.961191	503770.449025	46.727079
3504.106198	503768.300591	46.732084
3503.673577	503776.061483	46.737089
3503.777791	503762.583213	46.742093
3504.016869	503766.391705	46.747098
3503.632491	503749.498667	46.752103
3503.991046	503738.814253	46.757108
3503.766691	503738.444883	46.762113
3503.864520	503725.777330	46.767117
3503.839391	503725.275255	46.772122
3503.613857	503736.191771	46.777127
3503.635931	503719.892374	46.782132
3503.822694	503720.014720	46.787137
3503.574366	503721.774698	46.792141
3503.679505	503728.742097	46.797146
3503.515023	503734.537503	46.802151
3503.841546	503724.263011	46.807156
3503.752176	503735.613484	46.812161
3504.264751	503723.639505	46.817165
3504.055993	503709.451532	46.822170
3503.846143	503697.237457	46.827175
3504.189363	503678.761702	46.832180
3503.585340	503693.887976	46.837185
3503.805380	503679.682815	46.842189
3503.858100	503676.789827	46.847194
3504.062476	503677.769736	46.852199
3503.867628	503675.118311	46.857204
3503.785387	503658.885954	46.862209
3504.110291	503651.698808	46.867213
3503.917675	503649.148243	46.872218
3503.744371	503650.896370	46.877223
3503.856805	503641.111146	46.882228
3503.640457	503651.722611	46.887233
3503.721923	503645.484896	46.892237
3503.743274	503649.277217	46.897242
3503.943630	503650.966286	46.902247
3504.152284	503647.998038	46.907252
3503.635634	503626.672216	46.912257
3503.820081	503612.573844	46.917261
3504.283898	503616.852937	46.922266
3503.593321	503603.550772	46.927271
3503.793125	503604.177147	46.932276
3503.684470	503602.321829	46.937281
3503.719210	503615.272248	46.942285
3503.378046	503617.755433	46.947290
3503.577844	503610.790479	46.952295
3503.945787	503600.762414	46.957300
3503.348095	503619.278547	46.962305
3503.596387	503602.791461	46.967309
3503.774315	503604.585297	46.972314
3503.861703	503604.571523	46.977319
3504.237046	503611.192609	46.982324
3503.684698	503596.147890	46.987329
3504.047800	503570.026932	46.992333
3504.104542	503570.220438	46.997338
3503.509115	503575.173047	47.002343
3504.397379	503562.279228	47.007348
3503.922570	503572.223065	47.012353
3503.900418	503572.277213	47.017357
3503.860773	503551.027734	47.022362
3503.991275	503547.110250	47.027367
3504.170540	503533.265679	47.032372
3504.001982	503531.622258	47.037377
3504.003525	503525.852615	47.042381
3503.820854	503533.877763	47.047386
3503.714571	503528.428817	47.052391
3504.082461	503512.783099	47.057396
3503.818114	503496.073282	47.062401
3504.110409	503491.118029	47.067405
3503.972046	503490.583235	47.072410
3503.591044	503485.987444	47.077415
3503.688920	503481.164135	47.082420
3503.855344	503495.004796	47.087425
3503.774201	503481.859262	47.092429
3504.048074	503479.487989	47.097434
3504.149763	503464.137348	47.102439
3504.004543	503460.060986	47.107444
3503.531122	503454.923091	47.112449
3503.717849	503438.951675	47.117453
3503.806914	503447.794272	47.122458
3503.874411	503455.121994	47.127463
3504.011951	503451.304595	47.132468
3503.894812	503449.956696	47.137473
3503.751738	503441.679416	47.142477
3504.001431	503431.619335	47.147482
3503.596301	503421.156650	47.152487
3503.758224	503414.906137	47.157492
3503.602812	503406.327134	47.162497
3503.705346	503406.159138	47.167501
3503.682551	503406.871312	47.172506
3503.755506	503400.229980	47.177511
3503.694529	503406.869495	47.182516
3503.980133	503409.203037	47.187521
3503.863575	503401.275813	47.192525
3503.801979	503406.953846	47.197530
3503.742697	503410.708353	47.202535
3504.157569	503413.476948	47.207540
3503.751675	503398.155865	47.212545
3504.107028	503372.693762	47.217549
3504.065391	503373.459525	47.222554
3504.002923	503375.392599	47.227559
3503.819713	503361.757012	47.232564
3503.799125	503376.538296	47.237569
3503.949075	503366.898820	47.242573
3503.942342	503346.757303	47.247578
3503.815157	503334.985397	47.252583
3504.433536	503325.120031	47.257588
3504.042968	503329.635452	47.262593
3504.038714	503317.135569	47.267597
3504.429018	503319.452575	47.272602
3504.055858	503302.658553	47.277607
3504.193482	503285.733174	47.282612
3504.067631	503281.754929	47.287617
3504.022412	503276.549302	47.292621
3504.163645	503267.771516	47.297626
3504.178204	503250.511286	47.302631
3504.327423	503232.166946	47.307636
3503.794599	503240.095739	47.312641
3503.817265	503246.013556	47.317645
3503.704228	503240.666809	47.322650
3503.720255	503244.611888	47.327655
3504.290263	503228.883363	47.332660
3503.943430	503218.107684	47.337665
3504.144477	503202.285621	47.342669
3504.142193	503199.148197	47.347674
3503.838342	503198.285279	47.352679
3504.249246	503192.501436	47.357684
3503.973811	503184.042514	47.362689
3503.784731	503167.269879	47.367693
3503.943457	503168.712524	47.372698
3503.837738	503169.690864	47.377703
3503.979437	503157.673901	47.382708
3504.036719	503179.528464	47.387713
3503.978419	503147.602712	47.392717
3504.188920	503132.335804	47.397722
3503.952688	503133.182943	47.402727
3504.308231	503116.931503	47.407732
3503.963226	503127.766058	47.412737
3504.087501	503111.753607	47.417741
3504.003059	503103.922393	47.422746
3503.933649	503085.663066	47.427751
3504.050172	503076.332377	47.432756
3503.754215	503081.237790	47.437761
3504.054140	503073.902527	47.442765
3504.149376	503071.812486	47.447770
3503.684549	503067.584106	47.452775
3504.055338	503037.412310	47.457780
3503.552946	503035.011838	47.462785
3503.508804	503039.573799	47.467789
3503.803170	503032.745503	47.472794
3503.671850	503025.022884	47.477799
3503.833200	503025.655358	47.482804
3503.940372	503036.823384	47.487809
3503.926136	503023.616323	47.492813
3503.905891	503024.581162	47.497818
3503.652997	503036.109762	47.502823
3503.918683	503028.729281	47.507828
3503.770674	503014.632367	47.512833
3503.847400	502995.944966	47.517837
3503.900876	502998.871968	47.522842
3503.785958	502994.790709	47.527847
3504.261949	502992.336815	47.532852
3503.970485	502989.801777	47.537857
3503.961593	502993.194134	47.542861
3503.831946	502988.001767	47.547866
3503.574367	502991.433430	47.552871
3503.774741	502955.417593	47.557876
3504.159953	502957.533010	47.562881
3503.807492	502955.918601	47.567885
3503.939401	502942.587159	47.572890
3503.945735	502952.354075	47.577895
3504.027391	502942.978215	47.582900
3503.987425	502957.358027	47.587905
3503.948138	502931.451555	47.592909
3503.760480	502915.690672	47.597914
3503.386324	502908.006383	47.602919
3503.966535	502888.530738	47.607924
3503.814932	502902.675184	47.612929
3503.986897	502900.522385	47.617933
3504.075278	502912.300791	47.622938
3504.063001	502904.356861	47.627943
3504.290755	502900.626307	47.632948
3503.780709	502876.261875	47.637953
3504.059987	502869.182846	47.642957
3503.727550	502858.758948	47.647962
3503.863746	502870.276770	47.652967
3503.902619	502861.768015	47.657972
3503.921283	502857.918666	47.662977
3504.044931	502869.134806	47.667981
3504.119662	502840.173520	47.672986
3503.728030	502822.875848	47.677991
3503.893438	502816.725796	47.682996
3503.734307	502823.279822	47.688001
3503.797877	502819.777645	47.693005
3503.991309	502819.291610	47.698010
3503.993051	502825.567153	47.703015
3503.827766	502828.781815	47.708020
3503.765888	502810.824680	47.713025
3503.792543	502806.265500	47.718029
3503.994513	502796.010156	47.723034
3503.787184	502791.690399	47.728039
3503.784541	502774.533644	47.733044
3503.551789	502793.853352	47.738049
3504.177770	502778.166192	47.743053
3504.260562	502781.948989	47.748058
3503.920423	502780.028948	47.753063
3503.843037	502745.676145	47.758068
3503.897707	502746.477324	47.763073
3503.886448	502748.706041	47.768077
3503.781631	502733.438014	47.773082
3503.386945	502738.814629	47.778087
3503.482094	502732.422595	47.783092
3503.736487	502740.885136	47.788097
3503.351110	502740.389360	47.793101
3503.701953	502737.904601	47.798106
3503.708204	502749.696096	47.803111
3504.132405	502741.176993	47.808116
3503.645140	502746.568237	47.813121
3503.830237	502744.463955	47.818125
3504.047336	502747.061470	47.823130
3503.661206	502733.457469	47.828135
3504.037780	502718.265178	47.833140
3503.784217	502714.661270	47.838145
3503.678498	502699.494580	47.843149
3503.740020	502697.511046	47.848154
3503.690384	502698.682994	47.853159
3503.835555	502693.750773	47.858164
3503.678902	502705.416211	47.863169
3503.774535	502698.922866	47.868173
3503.959545	502703.600530	47.873178
3503.615868	502698.492517	47.878183
3503.861098	502689.495561	47.883188
3503.869367	502707.410758	47.888193
3503.846388	502695.419508	47.893197
3503.748770	502668.610863	47.898202
3503.684706	502670.746713	47.903207
3503.996665	502657.842103	47.908212
3504.226638	502661.196771	47.913217
3504.070433	502655.401164	47.918221
3503.997136	502663.611865	47.923226
3503.868755	502663.784029	47.928231
3504.305845	502640.484252	47.933236
3504.039125	502623.571535	47.938241
3503.903199	502629.160343	47.943245
3504.010439	502629.143432	47.948250
3503.926734	502621.463723	47.953255
3504.247579	502608.709508	47.958260
3503.765916	502602.762876	47.963265
3504.054439	502582.624433	47.968269
3503.689079	502590.425824	47.973274
3503.863441	502586.855478	47.978279
3503.879457	502571.821272	47.983284
3503.656450	502587.141329	47.988289
3503.551360	502577.035613	47.993293
3504.091976	502576.393476	47.998298
3504.024615	502586.374689	48.003303
3503.807247	502553.258319	48.008308
3503.645467	502547.362334	48.013313
3504.158497	502545.459257	48.018317
3504.083376	502537.120200	48.023322
3503.581291	502544.386489	48.028327
3504.004296	502535.462581	48.033332
3503.840443	502543.788875	48.038337
3503.854559	502539.231608	48.043341
3503.979813	502539.464909	48.048346
3503.733758	502537.783031	48.053351
3503.584543	502517.916148	48.058356
3503.828769	502524.052248	48.063361
3503.608135	502522.163903	48.068365
3504.102541	502507.003420	48.073370
3503.566251	502515.439204	48.078375
3504.003577	502495.580815	48.083380
3503.604515	502507.588370	48.088385
3503.627352	502507.230514	48.093389
3503.937500	502515.431292	48.098394
3503.830964	502505.933108	48.103399
3503.766260	502513.788237	48.108404
3503.806059	502515.907689	48.113409
3503.587091	502475.402072	48.118413
3503.829834	502475.869866	48.123418
3503.412128	502467.686146	48.128423
3503.876893	502469.890273	48.133428
3503.902248	502472.366299	48.138433
3503.956646	502465.980609	48.143437
3503.892550	502471.963011	48.148442
3503.959609	502473.622651	48.153447
3504.000422	502465.973805	48.158452
3503.865540	502469.031891	48.163457
3503.748583	502464.242260	48.168461
3503.960443	502442.799859	48.173466
3503.758570	502433.063644	48.178471
3504.077886	502436.556070	48.183476
3504.061828	502422.943950	48.188481
3504.060136	502430.940993	48.193485
3504.001074	502423.915262	48.198490
3503.794744	502425.365055	48.203495
3503.782196	502381.739249	48.208500
3503.537474	502385.320834	48.213505
3503.851525	502378.742237	48.218509
3504.170551	502385.524525	48.223514
3503.774483	502387.611658	48.228519
3503.840035	502385.222554	48.233524
3503.827785	502379.454716	48.238529
3503.971756	502380.140573	48.243533
3503.850549	502382.741000	48.248538
3503.964640	502376.143394	48.253543
3504.131048	502349.798660	48.258548
3503.831757	502355.008475	48.263553
3503.590270	502344.822960	48.268557
3504.432428	502328.645724	48.273562
3503.937033	502340.972292	48.278567
3504.023816	502336.808388	48.283572
3503.821130	502308.041914	48.288577
3503.864156	502310.970683	48.293581
3503.889035	502298.971600	48.298586
3503.753844	502304.712232	48.303591
3504.064039	502292.263149	48.308596
3503.662991	502296.831099	48.313601
3503.761508	502287.553452	48.318605
3504.177864	502303.582502	48.323610
3503.656511	502294.453444	48.328615
3504.076860	502275.306069	48.333620
3503.592679	502263.994774	48.338625
3503.578876	502259.947975	48.343629
3503.887991	502246.284325	48.348634
3503.723368	502266.859158	48.353639
3504.191871	502255.802184	48.358644
3503.773865	502265.484710	48.363649
3503.485980	502247.714562	48.368653
3503.958610	502262.064534	48.373658
3503.561097	502264.759263	48.378663
3504.024472	502262.104814	48.383668
3504.076129	502257.339090	48.388673
3503.978678	502245.156855	48.393677
3504.097186	502228.385324	48.398682
3503.715181	502218.981138	48.403687
3504.121010	502214.868005	48.408692
3503.962150	502213.729055	48.413697
3503.979144	502213.675795	48.418701
3503.891830	502210.197345	48.423706
3503.982385	502195.252264	48.428711
3503.990852	502179.307886	48.433716
3503.927794	502186.251866	48.438721
3503.784671	502177.417257	48.443725
3503.833341	502169.260912	48.448730
3503.665420	502181.535832	48.453735
3504.001356	502174.093281	48.458740
3503.799175	502180.654348	48.463745
3503.682010	502162.249776	48.468749
3503.596315	502154.418339	48.473754
3503.397477	502143.567997	48.478759
3503.824117	502150.029689	48.483764
3503.643930	502155.878706	48.488769
3504.068813	502143.158327	48.493773
3503.924921	502136.753246	48.498778
3503.570363	502132.304758	48.503783
3503.673239	502131.934244	48.508788
3503.832780	502141.323102	48.513793
3503.475285	502132.775418	48.518797
3503.861247	502134.384686	48.523802
3503.364895	502134.868079	48.528807
3503.687388	502127.528859	48.533812
3503.623758	502142.621657	48.538817
3503.469740	502127.816401	48.543821
3503.807480	502120.171089	48.548826
3503.545142	502132.714032	48.553831
3503.662852	502139.629459	48.558836
3503.695688	502143.116610	48.563841
3503.613784	502142.522237	48.568845
3503.513018	502135.047465	48.573850
3503.651474	502139.024054	48.578855
3503.965958	502129.256672	48.583860
3504.032422	502143.215419	48.588865
3503.891249	502124.460310	48.593869
3503.796652	502103.521453	48.598874
3503.902665	502092.066152	48.603879
3503.762672	502089.253976	48.608884
3504.335989	502089.720146	48.613889
3503.989579	502097.619983	48.618893
3504.128189	502094.713161	48.623898
3503.989674	502075.097155	48.628903
3504.088182	502050.635399	48.633908
3504.098896	502061.363768	48.638913
3503.896302	502060.636628	48.643917
3504.134187	502044.402801	48.648922
3504.071246	502051.802336	48.653927
3503.869575	502028.147193	48.658932
3504.101225	502026.744057	48.663937
3503.836758	502016.865664	48.668941
3503.933484	502004.601960	48.673946
3503.608081	502012.650355	48.678951
3503.892880	502013.668262	48.683956
3503.814241	502021.424585	48.688961
3503.977584	502014.920287	48.693965
3504.298350	501982.021475	48.698970
3503.715775	501988.085987	48.703975
3503.791512	501977.546441	48.708980
3504.080305	501976.944085	48.713985
3504.166362	501974.197390	48.718989
3503.762612	501974.311856	48.723994
3503.765392	501969.199485	48.728999
3504.100575	501960.997760	48.734004
3503.911180	501946.602853	48.739009
3503.880396	501936.940550	48.744013
3504.366761	501923.198023	48.749018
3503.690660	501924.064127	48.754023
3503.931451	501931.921843	48.759028
3503.814160	501942.518674	48.764033
3504.034800	501909.989849	48.769037
3503.955793	501888.542137	48.774042
3504.015800	501882.205965	48.779047
3503.841565	501889.167633	48.784052
3503.787245	501886.038201	48.789057
3504.089170	501885.484381	48.794061
3503.997227	501885.853248	48.799066
3503.900113	501876.960603	48.804071
3503.852410	501866.339273	48.809076
3503.927081	501863.746202	48.814081
3503.435447	501856.130635	48.819085
3504.024158	501851.634216	48.824090
3503.810177	501864.675844	48.829095
3503.945055	501852.861529	48.834100
3503.992763	501857.561119	48.839105
3503.793937	501853.341015	48.844109
3503.953974	501839.498159	48.849114
3503.473005	501827.123183	48.854119
3503.476420	501806.168483	48.859124
3503.548924	501815.723112	48.864129
3503.593372	501819.664017	48.869133
3503.678054	501810.135238	48.874138
3503.612156	501806.501481	48.879143
3503.894825	501796.182191	48.884148
3503.787434	501812.041397	48.889153
3503.709876	501808.662554	48.894157
3503.748018	501808.859020	48.899162
3503.522513	501809.603297	48.904167
3503.768906	501806.122638	48.909172
3503.912312	501812.730448	48.914177
3503.793642	501808.953190	48.919181
3504.009327	501810.842472	48.924186
3503.784896	501820.089732	48.929191
3503.990911	501810.035635	48.934196
3504.011413	501788.521460	48.939201
3503.669347	501776.225722	48.944205
3503.903223	501764.800614	48.949210
3503.346290	501777.289141	48.954215
3503.690714	501778.196410	48.959220
3503.780631	501772.766526	48.964225
3503.586682	501776.036522	48.969229
3503.854254	501780.043399	48.974234
3503.581135	501782.009941	48.979239
3504.061884	501774.240649	48.984244
3503.923376	501782.158381	48.989249
3503.753772	501789.068743	48.994253
3503.992141	501785.083207	48.999258
3503.929237	501768.997898	49.004263
3503.957606	501749.810683	49.009268
3503.700810	501732.743702	49.014273
3503.788880	501743.409423	49.019277
3503.849461	501732.720284	49.024282
3503.775722	501743.816493	49.029287
3504.054110	501731.118974	49.034292
3503.803127	501735.005363	49.039297
3503.748649	501733.698042	49.044301
3503.968898	501720.756633	49.049306
3503.943418	501702.742006	49.054311
3503.579872	501694.498752	49.059316
3503.799392	501694.059179	49.064321
3503.862526	501689.949476	49.069325
3503.928758	501693.178365	49.074330
3503.707012	501690.125975	49.079335
3503.886141	501690.097702	49.084340
3504.035368	501688.201422	49.089345
3503.938397	501696.821228	49.094349
3504.018719	501678.384940	49.099354
3503.937277	501652.078343	49.104359
3504.104158	501647.496702	49.109364
3504.036922	501642.091616	49.114369
3503.645185	501643.317703	49.119373
3503.819105	501641.366902	49.124378
3503.490761	501650.073914	49.129383
3503.663692	501642.656905	49.134388
3503.634546	501647.925457	49.139393
3503.535792	501650.066912	49.144397
3504.146847	501647.490261	49.149402
3503.686213	501632.479981	49.154407
3503.671574	501613.552489	49.159412
3503.902315	501618.273828	49.164417
3503.666047	501610.314105	49.169421
3504.063626	501608.884711	49.174426
3503.876521	501607.800800	49.179431
3504.002384	501606.161278	49.184436
3504.053389	501600.484418	49.189441
3503.891107	501606.432016	49.194445
3504.152366	501594.040793	49.199450
3503.859080	501571.158740	49.204455
3503.814135	501560.789865	49.209460
3503.961686	501566.182358	49.214465
3503.813986	501564.282381	49.219469
3503.896469	501570.748066	49.224474
3503.577489	501566.850573	49.229479
3503.861194	501556.227292	49.234484
3503.763512	501564.341126	49.239489
3503.753466	501566.316727	49.244493
3504.015015	501549.370102	49.249498
3503.623344	501531.818098	49.254503
3503.552591	501530.159030	49.259508
3503.635890	501529.690369	49.264513
3503.721155	501517.377525	49.269517
3503.956787	501523.869636	49.274522
3503.586275	501525.547910	49.279527
3503.560518	501521.249758	49.284532
3503.875383	501521.351875	49.289537
3503.412900	501530.991214	49.294541
3503.952639	501522.807571	49.299546
3503.659022	501521.639261	49.304551
3503.638185	501526.349772	49.309556
3503.604433	501530.050028	49.314561
3503.789039	501519.189313	49.319565
3503.816392	501522.120689	49.324570
3503.894124	501538.001496	49.329575
3503.888010	501517.554110	49.334580
3503.685937	501505.590361	49.339585
3503.747473	501496.621836	49.344589
3503.962304	501483.023116	49.349594
3503.929317	501479.232246	49.354599
3504.146116	501486.081653	49.359604
3504.029922	501484.885297	49.364609
3503.644695	501479.732881	49.369613
3503.868971	501478.735787	49.374618
3503.745415	501496.926118	49.379623
3503.808382	501475.657927	49.384628
3503.925617	501457.013115	49.389633
3503.847433	501456.165055	49.394637
3504.014672	501449.457475	49.399642
3504.108192	501445.849063	49.404647
3503.824335	501438.757241	49.409652
3503.770291	501451.672662	49.414657
3503.891150	501454.133735	49.419661
3504.014256	501425.010645	49.424666
3503.528828	501421.291273	49.429671
3503.728600	501398.533528	49.434676
3503.847455	501406.562595	49.439681
3503.835149	501404.995508	49.444685
3503.626939	501405.180300	49.449690
3503.680344	501401.881911	49.454695
3503.812308	501397.963722	49.459700
3503.758143	501402.831379	49.464705
3503.539310	501406.763374	49.469709
3504.014274	501398.893604	49.474714
3503.709678	501407.394520	49.479719
3503.908664	501400.074522	49.484724
3504.031899	501407.799205	49.489729
3503.872571	501388.691881	49.494733
3503.810483	501365.671791	49.499738
3503.767023	501364.767623	49.504743
3504.110817	501360.613484	49.509748
3503.902104	501359.026820	49.514753
3503.859392	501366.170367	49.519757
3504.258806	501355.629909	49.524762
3503.890007	501357.561003	49.529767
3503.919457	501327.237789	49.534772
3503.955775	501321.968085	49.539777
3503.925407	501324.655539	49.544781
3504.049022	501308.692180	49.549786
3503.730518	501319.270569	49.554791
3503.861898	501318.136303	49.559796
3503.789841	501317.186037	49.564801
3503.859529	501312.012287	49.569805
3503.926932	501287.503781	49.574810
3503.715644	501284.753360	49.579815
3503.536251	501275.468494	49.584820
3503.820217	501269.197937	49.589825
3503.845148	501276.432059	49.594829
3503.806067	501272.692724	49.599834
3503.707620	501270.886162	49.604839
3504.187804	501270.304150	49.609844
3504.121188	501267.125937	49.614849
3503.770317	501263.739572	49.619853
3504.141360	501240.144705	49.624858
3503.924487	501235.724844	49.629863
3503.893018	501226.467188	49.634868
3504.028942	501233.329475	49.639873
3503.937587	501222.360349	49.644877
3503.839705	501230.778062	49.649882
3503.593088	501237.548962	49.654887
3503.908670	501218.518241	49.659892
3503.997725	501197.296209	49.664897
3503.429811	501195.715688	49.669901
3503.734528	501181.748221	49.674906
3503.911092	501184.656070	49.679911
3503.664848	501186.112270	49.684916
3503.954290	501181.359291	49.689921
3504.046060	501171.221659	49.694925
3503.836904	501186.135807	49.699930
3503.806701	501183.508597	49.704935
3503.886230	501184.002224	49.709940
3503.830627	501156.222951	49.714945
3503.826262	501153.389189	49.719949
3504.174274	501127.013938	49.724954
3503.909680	501141.076415	49.729959
3503.833961	501139.974870	49.734964
3504.207378	501146.344111	49.739969
3504.099129	501136.592384	49.744973
3504.256048	501120.826056	49.749978
3503.819448	501105.811530	49.754983
3503.821407	501096.244827	49.759988
3503.849582	501088.749234	49.764993
3503.637940	501096.982525	49.769997
3503.555074	501093.098225	49.775002
3503.851123	501095.430426	49.780007
3503.572664	501098.207743	49.785012
3503.591968	501104.784815	49.790017
3503.460545	501088.355407	49.795021
3503.625020	501088.683762	49.800026
3503.595653	501102.202930	49.805031
3503.744982	501087.804405	49.810036
3503.749498	501092.409793	49.815041
3503.791192	501090.074902	49.820045
3503.603977	501085.042922	49.825050
3503.599975	501088.941031	49.830055
3503.358595	501086.195336	49.835060
3503.541804	501090.114471	49.840065
3503.462928	501091.898539	49.845069
3503.827893	501101.255479	49.850074
3503.494523	501104.598250	49.855079
3503.916236	501090.662837	49.860084
3503.832234	501089.765063	49.865089
3503.790176	501069.322843	49.870093
3503.784891	501049.836494	49.875098
3503.491882	501057.880200	49.880103
3503.681316	501040.337095	49.885108
3503.660605	501047.072363	49.890113
3503.556490	501044.355582	49.895117
3503.888490	501043.189590	49.900122
3503.862649	501054.531739	49.905127
3503.957632	501049.657612	49.910132
3504.331874	501053.192249	49.915137
3503.994824	501054.510963	49.920141
3503.883852	501030.840155	49.925146
3503.649709	501025.360030	49.930151
3503.665025	501013.918369	49.935156
3503.833313	501017.333716	49.940161
3503.785514	501014.456181	49.945165
3503.881522	501003.912854	49.950170
3503.589898	501009.223081	49.955175
3503.724097	501011.732723	49.960180
3503.699279	501012.344080	49.965185
3503.738545	501017.804471	49.970189
3503.961255	501011.897820	49.975194
3503.876375	501012.012506	49.980199
3503.968021	501003.646369	49.985204
3503.768235	500967.639128	49.990209
3503.710961	500974.683900	49.995213
3503.897851	500967.011321	50.000218
3503.842031	500971.221345	50.005223
3503.782997	500968.902358	50.010228
3503.976186	500970.997752	50.015233
3503.754372	500964.250248	50.020237
3503.837856	500966.666680	50.025242
3503.797452	500974.113717	50.030247
3503.895011	500958.052929	50.035252
3503.948219	500945.238591	50.040257
3503.569296	500941.299817	50.045261
3503.897026	500926.974198	50.050266
3503.951847	500930.711195	50.055271
3503.625557	500934.407194	50.060276
3503.989373	500933.792949	50.065281
3503.831942	500928.908066	50.070285
3503.991857	500921.897747	50.075290
3503.744267	500921.278902	50.080295
3503.895818	500920.293273	50.085300
3504.290874	500892.290510	50.090305
3503.926401	500899.383866	50.095309
3503.933828	500874.884271	50.100314
3503.988393	500884.391620	50.105319
3503.834024	500884.365440	50.110324
3504.008914	500883.477353	50.115329
3503.891935	500866.691141	50.120333
3504.032393	500847.687703	50.125338
3503.590746	500850.136533	50.130343
3503.639654	500847.952321	50.135348
3503.729224	500836.397576	50.140353
3503.374340	500842.578337	50.145357
3503.913419	500854.388110	50.150362
3503.753285	500842.518520	50.155367
3503.632945	500840.006739	50.160372
3503.884862	500850.950800	50.165377
3503.964035	500842.485325	50.170381
3503.922630	500837.835163	50.175386
3503.666095	500852.352144	50.180391
3503.875434	500839.158736	50.185396
3503.834265	500806.922358	50.190401
3503.762396	500796.506676	50.195405
3503.908353	500792.282441	50.200410
3503.632616	500805.182754	50.205415
3503.632153	500798.653286	50.210420
3504.026139	500787.151630	50.215425
3503.834970	500797.608969	50.220429
3504.140773	500781.363257	50.225434
3503.519438	500798.671254	50.230439
3503.930212	500794.658249	50.235444
3503.843291	500789.002931	50.240449
3503.622602	500775.168806	50.245453
3503.619737	500763.729858	50.250458
3503.920182	500747.687430	50.255463
3503.812269	500756.106952	50.260468
3503.937920	500764.287087	50.265473
3503.706900	500752.175555	50.270477
3503.725261	500744.985071	50.275482
3503.369498	500749.647490	50.280487
3503.691349	500764.174360	50.285492
3503.928210	500756.139474	50.290497
3503.725043	500761.030857	50.295501
3503.924298	500758.367318	50.300506
3503.962820	500763.372352	50.305511
3504.044441	500735.368265	50.310516
3503.869580	500727.449057	50.315521
3503.888995	500721.827528	50.320525
3503.939028	500712.556723	50.325530
3504.166728	500705.738073	50.330535
3503.993569	500707.587698	50.335540
3504.029838	500706.822746	50.340545
3503.897897	500690.544904	50.345549
3503.826176	500675.472344	50.350554
3503.603203	500673.331082	50.355559
3503.732602	500672.348940	50.360564
3503.556319	500678.299059	50.365569
3503.595851	500682.089142	50.370573
3503.849672	500672.735490	50.375578
3504.046290	500679.132843	50.380583
3503.951280	500679.400984	50.385588
3503.648901	500672.514251	50.390593
3503.645704	500682.790095	50.395597
3504.001352	500665.422821	50.400602
3503.755226	500651.187681	50.405607
3503.654668	500639.915947	50.410612
3503.773881	500629.672435	50.415617
3503.453884	500629.216876	50.420621
3503.754636	500626.638510	50.425626
3503.489796	500630.628564	50.430631
3503.723690	500626.137304	50.435636
3503.770069	500630.634959	50.440641
3503.650169	500637.588528	50.445645
3504.033525	500633.326734	50.450650
3503.690360	500638.847686	50.455655
3503.753872	500622.133951	50.460660
3504.009450	500631.963985	50.465665
3503.656825	500644.218540	50.470669
3503.550475	500635.073647	50.475674
3503.775678	500633.620804	50.480679
3503.729885	500630.236716	50.485684
3503.940917	500625.242896	50.490689
3503.304183	500606.362040	50.495693
3503.742774	500598.193963	50.500698
3503.533739	500601.213471	50.505703
3503.711886	500596.022371	50.510708
3503.885604	500593.109756	50.515713
3503.905389	500590.727645	50.520717
3503.801828	500591.604549	50.525722
3503.707512	500593.036784	50.530727
3504.082694	500572.983605	50.535732
3503.983274	500547.639950	50.540737
3503.746819	500532.998247	50.545741
3503.765130	500474.278814	50.550746
3503.815669	500407.252741	50.555751
3503.537968	500353.793352	50.560756
3503.516386	500270.985293	50.565761
3502.883795	500187.261050	50.570765
3503.131049	500085.275785	50.575770
3503.020710	499999.544598	50.580775
3502.896719	499876.559234	50.585780
3502.961103	499756.580443	50.590785
3502.297469	499631.248933	50.595789
3502.609646	499486.931454	50.600794
3501.776901	499350.943757	50.605799
3501.791400	499191.940237	50.610804
3501.772264	499034.509904	50.615809
3501.190395	498878.382070	50.620813
3501.333374	498679.210152	50.625818
3500.789172	498513.505467	50.630823
3500.148912	498322.705004	50.635828
3499.818241	498125.373659	50.640833
3499.698768	497930.335524	50.645837
3499.559383	497729.375241	50.650842
3499.446151	497518.232735	50.655847
3499.180718	497288.228038	50.660852
3498.714779	497060.631600	50.665857
3498.240250	496829.590953	50.670861
3498.028929	496586.304236	50.675866
3497.419665	496350.469054	50.680871
3496.681528	496096.525610	50.685876
3496.859656	495833.016465	50.690881
3496.282291	495587.799652	50.695885
3496.031394	495317.110556	50.700890
3495.540789	495056.632574	50.705895
3495.099775	494773.256590	50.710900
3494.430423	494499.330339	50.715905
3494.102679	494224.789014	50.720909
3493.909511	493918.878570	50.725914
3493.428648	493635.744504	50.730919
3492.913511	493337.116359	50.735924
3492.586181	493031.566849	50.740929
3491.887190	492724.703766	50.745933
3491.366779	492412.236934	50.750938
3490.854525	492103.561626	50.755943
3490.376304	491794.926444	50.760948
3489.857542	491466.997626	50.765953
3489.189840	491160.559505	50.770957
3488.979528	490822.087330	50.775962
3488.173206	490503.151094	50.780967
3487.855791	490177.548113	50.785972
3487.141657	489840.505251	50.790977
3486.620339	489504.134927	50.795981
3485.905270	489170.422955	50.800986
3485.422464	488830.792952	50.805991
3484.959031	488482.391159	50.810996
3484.622156	488141.662010	50.816001
3483.479670	487795.583562	50.821005
3483.148679	487438.986509	50.826010
3482.676743	487091.776142	50.831015
3481.657399	486737.047619	50.836020
3481.244251	486380.545000	50.841025
3480.828232	486044.856378	50.846029
3480.547918	485664.358409	50.851034
3479.638856	485318.248663	50.856039
3479.071783	484946.191199	50.861044
3478.243626	484592.101886	50.866049
3477.810271	484215.601609	50.871053
3477.385645	483853.734265	50.876058
3476.475740	483482.361318	50.881063
3475.788226	483119.052505	50.886068
3475.524516	482753.947241	50.891073
3474.610973	482387.164481	50.896077
3474.136623	482001.912888	50.901082
3473.316138	481641.333526	50.906087
3472.650389	481263.444593	50.911092
3472.141290	480883.699439	50.916097
3470.906259	480507.152658	50.921101
3470.772364	480142.890116	50.926106
3470.189853	479765.516551	50.931111
3469.779079	479389.375477	50.936116
3468.912769	479000.174217	50.941121
3468.138174	478632.488417	50.946125
3467.495005	478245.770882	50.951130
3467.037608	477876.044482	50.956135
3466.181544	477494.464516	50.961140
3465.788085	477103.833646	50.966145
3464.730998	476737.576512	50.971149
3464.262815	476339.593685	50.976154
3463.966729	475953.993221	50.981159
3463.037776	475576.240119	50.986164
3462.420908	475188.344185	50.991169
3461.849374	474811.838064	50.996173
3461.256597	474414.039582	51.001178
3460.262731	474037.839242	51.006183
3459.409619	473645.237022	51.011188
3459.116413	473261.003986	51.016193
3457.866569	472888.168373	51.021197
3457.557948	472490.591453	51.026202
3456.778196	472108.086452	51.031207
3456.025861	471727.090794	51.036212
3455.552368	471348.629428	51.041217
3454.806695	470958.189176	51.046221
3454.256262	470563.401418	51.051226
3453.228685	470179.530890	51.056231
3452.458446	469810.518008	51.061236
3451.738073	469423.238770	51.066241
3451.409442	469051.911795	51.071245
3450.815368	468666.322312	51.076250
3450.071741	468285.819590	51.081255
3449.444403	467896.215637	51.086260
3448.815358	467519.331503	51.091265
3447.566529	467142.944215	51.096269
3447.138024	466750.194519	51.101274
3446.529295	466374.199350	51.106279
3445.843286	465995.370048	51.111284
3445.338846	465609.152457	51.116289
3444.262252	465232.298181	51.121293
3443.817243	464844.333133	51.126298
3443.115338	464469.688088	51.131303
3442.304876	464086.128204	51.136308
3441.806320	463700.838579	51.141313
3440.663226	463340.950392	51.146317
3440.354832	462945.372820	51.151322
3439.619944	462577.394284	51.156327
3438.704861	462196.403667	51.161332
3438.209725	461818.940910	51.166337
3437.345004	461448.681344	51.171341
3436.896875	461073.734103	51.176346
3436.312434	460694.592131	51.181351
3435.427104	460315.085347	51.186356
3435.100013	459936.802487	51.191361
3434.022498	459573.544331	51.196365
3433.727914	459186.518970	51.201370
3432.682564	458807.772189	51.206375
3432.079792	458422.912541	51.211380
3431.421426	458050.787363	51.216385
3430.387796	457682.164710	51.221389
3429.885586	457306.958669	51.226394
3428.714563	456931.699823	51.231399
3428.330659	456562.347083	51.236404
3427.854883	456190.770579	51.241409
3426.883525	455837.326741	51.246413
3426.593381	455453.431538	51.251418
3426.010100	455084.035138	51.256423
3424.859071	454715.889304	51.261428
3424.304371	454351.296096	51.266433
3423.541609	453974.502525	51.271437
3422.981693	453612.130581	51.276442
3422.279247	453238.562364	51.281447
3421.364846	452872.936697	51.286452
3420.875537	452513.072955	51.291457
3419.798323	452148.019509	51.296461
3419.348274	451776.772172	51.301466
3418.828296	451414.358916	51.306471
3417.639288	451059.910779	51.311476
3417.227802	450689.096412	51.316481
3416.518601	450325.833262	51.321485
3415.754684	449961.964103	51.326490
3415.293068	449597.838441	51.331495
3414.511462	449238.324826	51.336500
3413.936420	448877.453557	51.341505
3412.890015	448528.475495	51.346509
3412.784052	448162.038197	51.351514
3411.813382	447793.549630	51.356519
3410.969207	447439.042364	51.361524
3410.256196	447071.821220	51.366529
3409.420044	446721.311190	51.371533
3408.872315	446370.039807	51.376538
3407.964508	446013.288004	51.381543
3407.331792	445663.948193	51.386548
3406.812218	445307.682677	51.391553
3406.147190	444961.129150	51.396557
3405.208537	444595.478665	51.401562
3404.643713	444255.598886	51.406567
3404.105230	443907.132026	51.411572
3403.550691	443551.048838	51.416577
3402.585578	443194.213131	51.421581
3402.252597	442841.231482	51.426586
3401.367205	442488.890374	51.431591
3400.568670	442133.383173	51.436596
3400.073971	441772.391139	51.441601
3399.111010	441443.347011	51.446605
3398.544236	441090.985970	51.451610
3397.949321	440731.923360	51.456615
3397.244588	440383.635080	51.461620
3396.665235	440035.169722	51.466625
3395.653841	439687.833823	51.471629
3395.194447	439330.328399	51.476634
3394.669334	438981.941070	51.481639
3393.637474	438635.913545	51.486644
3393.055032	438282.676991	51.491649
3392.264977	437935.306820	51.496653
3391.454791	437587.452650	51.501658
3390.877469	437256.844578	51.506663
3390.095626	436909.712658	51.511668
3389.540557	436559.950634	51.516673
3388.655086	436226.255110	51.521677
3388.399486	435886.438786	51.526682
3387.412625	435543.179232	51.531687
3386.946948	435204.123162	51.536692
3386.239993	434851.111751	51.541697
3385.635488	434521.259039	51.546701
3385.021497	434165.303692	51.551706
3384.382134	433821.864312	51.556711
3383.604405	433473.643537	51.561716
3382.970731	433132.352102	51.566721
3382.084339	432788.760165	51.571725
3381.442934	432439.589724	51.576730
3380.872874	432101.245230	51.581735
3380.206651	431766.288551	51.586740
3379.535635	431406.342864	51.591745
3378.457210	431067.862085	51.596749
3378.082139	430721.901893	51.601754
3377.690009	430388.509186	51.606759
3376.799743	430054.657724	51.611764
3376.312999	429702.708912	51.616769
3375.310385	429359.470795	51.621773
3374.633580	429028.594348	51.626778
3373.814166	428691.794013	51.631783
3373.293783	428347.831586	51.636788
3372.803605	428001.117245	51.641793
3371.991841	427667.299249	51.646797
3371.220414	427320.442708	51.651802
3370.497761	426985.078311	51.656807
3369.806070	426652.777751	51.661812
3369.550160	426307.223311	51.666817
3368.533354	425976.108598	51.671821
3368.142610	425638.160537	51.676826
3367.730934	425306.002186	51.681831
3366.655579	424961.169549	51.686836
3366.164827	424611.592200	51.691841
3365.031459	424276.893898	51.696845
3364.562202	423931.444342	51.701850
3363.848901	423595.274288	51.706855
3362.945014	423260.120805	51.711860
3362.408207	422912.687868	51.716865
3361.340850	422590.607526	51.721869
3360.930147	422253.865145	51.726874
3360.290836	421925.791035	51.731879
3359.449943	421597.694096	51.736884
3359.150994	421262.395201	51.741889
3358.099456	420937.270294	51.746893
3357.846863	420598.145800	51.751898
3356.901611	420264.410366	51.756903
3356.420464	419925.034398	51.761908
3355.914964	419596.632193	51.766913
3354.786978	419262.177011	51.771917
3354.241326	418925.695105	51.776922
3353.636314	418598.846584	51.781927
3352.816550	418262.857380	51.786932
3352.181122	417939.105332	51.791937
3351.605481	417613.307765	51.796941
3350.847967	417266.499948	51.801946
3350.112844	416945.216625	51.806951
3349.560856	416617.117460	51.811956
3348.988411	416286.502595	51.816961
3347.832376	415959.253589	51.821965
3347.646852	415629.865696	51.826970
3347.206566	415307.704414	51.831975
3345.904930	414972.819827	51.836980
3345.441741	414640.161658	51.841985
3344.727750	414307.793414	51.846989
3344.261404	413971.393185	51.851994
3343.367578	413647.836960	51.856999
3342.774443	413317.648832	51.862004
3342.328480	412982.631471	51.867009
3341.564806	412668.038528	51.872013
3340.984345	412332.577673	51.877018
3340.493529	411995.980813	51.882023
3339.586244	411667.577127	51.887028
3339.065257	411331.180767	51.892033
3337.873996	411010.056599	51.897037
3337.098718	410673.896309	51.902042
3336.637522	410352.522568	51.907047
3335.818134	410033.260330	51.912052
3335.543270	409691.343186	51.917057
3334.480266	409366.267746	51.922061
3333.838687	409043.815840	51.927066
3333.385120	408726.718178	51.932071
3332.386493	408404.036389	51.937076
3332.185704	408073.829867	51.942081
3330.986508	407755.366040	51.947085
3330.509914	407421.968614	51.952090
3329.799173	407097.499374	51.957095
3329.203974	406783.224834	51.962100
3328.843843	406456.736516	51.967105
3327.738994	406128.786814	51.972109
3327.359230	405806.767679	51.977114
3326.577096	405487.451990	51.982119
3325.887835	405162.094919	51.987124
3325.190154	404841.285163	51.992129
3324.567953	404513.597914	51.997133
3323.984378	404193.144704	52.002138
3323.161949	403875.496373	52.007143
3322.406155	403555.521392	52.012148
3322.272760	403223.778420	52.017153
3320.786010	402900.531962	52.022157
3320.592317	402578.602765	52.027162
3319.933330	402254.227550	52.032167
3318.869417	401932.048171	52.037172
3318.422402	401611.471001	52.042177
3317.675527	401295.742115	52.047181
3317.163261	400974.787629	52.052186
3315.941610	400655.213072	52.057191
3315.496730	400337.113915	52.062196
3315.388808	400017.382346	52.067201
3314.356400	399715.816334	52.072205
3313.786517	399379.145823	52.077210
3313.177727	399054.018728	52.082215
3312.081195	398740.913108	52.087220
3311.761808	398419.826629	52.092225
3310.533929	398109.786236	52.097229
3310.187476	397789.892675	52.102234
3309.675899	397481.868476	52.107239
3308.728378	397173.147710	52.112244
3308.357231	396836.318080	52.117249
3307.397627	396536.440110	52.122253
3306.740263	396202.166125	52.127258
3306.203787	395892.707520	52.132263
3305.218430	395581.944223	52.137268
3304.844011	395262.107112	52.142273
3304.048885	394946.324958	52.147277
3303.544648	394631.027746	52.152282
3302.894164	394325.564292	52.157287
3302.118334	394005.855078	52.162292
3301.816789	393686.245830	52.167297
3301.032034	393373.752583	52.172301
3299.998927	393054.507379	52.177306
3299.717713	392742.666070	52.182311
3298.791348	392419.101285	52.187316
3298.063238	392109.943727	52.192321
3297.586454	391795.455141	52.197325
3296.764559	391474.814388	52.202330
3296.288324	391168.354611	52.207335
3295.491947	390846.992125	52.212340
3294.984021	390525.352233	52.217345
3294.085768	390224.366792	52.222349
3293.273910	389898.675535	52.227354
3293.085505	389584.045217	52.232359
3292.051351	389278.521742	52.237364
3291.575573	388954.345153	52.242369
3290.942737	388642.497544	52.247373
3290.440968	388331.796177	52.252378
3289.789829	388009.139003	52.257383
3288.732449	387692.086604	52.262388
3288.542581	387370.215319	52.267393
3287.274491	387061.480479	52.272397
3286.675706	386753.705180	52.277402
3286.087356	386437.076185	52.282407
3285.318132	386118.311526	52.287412
3284.925852	385809.885283	52.292417
3283.820626	385493.355288	52.297421
3283.404317	385183.427207	52.302426
3282.481564	384883.697957	52.307431
3281.554324	384577.507586	52.312436
3281.261758	384251.378183	52.317441
3280.291942	383947.147526	52.322445
3279.847522	383655.190923	52.327450
3279.475049	383340.179679	52.332455
3278.516816	383036.753589	52.337460
3278.088368	382730.723494	52.342465
3277.265037	382415.674083	52.347469
3276.664725	382099.569478	52.352474
3276.069286	381801.366015	52.357479
3275.414365	381491.546835	52.362484
3275.301220	381172.305536	52.367489
3273.992129	380855.794049	52.372493
3273.380592	380550.411196	52.377498
3272.636691	380233.881493	52.382503
3271.960682	379923.188238	52.387508
3271.294278	379607.429596	52.392513
3270.418610	379309.836099	52.397517
3269.516315	378997.619737	52.402522
3269.207766	378687.570653	52.407527
3268.421208	378392.118012	52.412532
3267.843033	378080.478946	52.417537
3267.132472	377776.692406	52.422541
3266.240689	377469.447539	52.427546
3265.576406	377174.551456	52.432551
3265.193771	376860.506343	52.437556
3264.506849	376555.689287	52.442561
3263.606864	376262.171843	52.447565
3263.228633	375947.788197	52.452570
3262.522059	375655.075127	52.457575
3261.654941	375350.964218	52.462580
3261.136427	375033.670410	52.467585
3260.290843	374734.231870	52.472589
3259.927465	374440.336512	52.477594
3259.156442	374127.781493	52.482599
3258.320043	373819.507968	52.487604
3257.955050	373512.276838	52.492609
3256.928657	373212.601397	52.497613
3256.559117	372905.951552	52.502618
3256.080740	372603.081550	52.507623
3255.068417	372303.600824	52.512628
3254.489053	371989.473010	52.517633
3253.718921	371684.480189	52.522637
3252.968753	371370.730903	52.527642
3252.570527	371084.194657	52.532647
3251.876482	370772.619837	52.537652
3251.516462	370456.003700	52.542657
3250.558243	370157.389555	52.547661
3249.866672	369841.457294	52.552666
3249.132748	369545.474612	52.557671
3248.380204	369240.436021	52.562676
3247.579212	368934.258104	52.567681
3247.312775	368632.572821	52.572685
3246.494903	368328.606646	52.577690
3246.141731	368018.713367	52.582695
3244.999081	367722.884645	52.587700
3244.918039	367406.303782	52.592705
3244.115176	367101.741552	52.597709
3242.807885	366796.366540	52.602714
3242.614565	366492.594162	52.607719
3241.684661	366200.487004	52.612724
3241.137535	365883.765435	52.617729
3240.212455	365586.895760	52.622733
3239.907803	365279.977855	52.627738
3239.288097	364982.267155	52.632743
3238.043469	364682.490675	52.637748
3237.858423	364365.573931	52.642753
3236.967393	364072.123753	52.647757
3236.379002	363771.219721	52.652762
3235.435223	363464.212526	52.657767
3235.183967	363166.762442	52.662772
3234.534830	362868.839049	52.667777
3233.952581	362568.129727	52.672781
3233.083107	362257.235216	52.677786
3232.560780	361953.560882	52.682791
3231.289457	361657.712823	52.687796
3231.037431	361351.345566	52.692801
3230.117097	361066.379590	52.697805
3229.609717	360763.458548	52.702810
3229.119996	360459.056941	52.707815
3228.542909	360166.372178	52.712820
3227.699995	359855.737521	52.717825
3226.836155	359567.343889	52.722829
3226.278802	359259.942724	52.727834
3225.465009	358965.226940	52.732839
3224.773744	358659.853390	52.737844
3224.513901	358360.313274	52.742849
3223.609847	358065.300948	52.747853
3222.761798	357772.619092	52.752858
3222.155302	357474.019023	52.757863
3221.579083	357171.875199	52.762868
3220.976971	356876.120900	52.767873
3220.328991	356593.019483	52.772877
3219.855469	356281.209402	52.777882
3218.917788	355976.570729	52.782887
3217.932997	355690.896359	52.787892
3217.573085	355385.730093	52.792897
3216.791783	355101.903355	52.797901
3216.135140	354795.966131	52.802906
3215.722730	354503.399801	52.807911
3214.828247	354214.852597	52.812916
3214.258635	353914.138748	52.817921
3213.622039	353623.333380	52.822925
3212.835420	353315.397417	52.827930
3212.214929	353021.048693	52.832935
3211.564117	352735.381342	52.837940
3211.181316	352423.253422	52.842945
3210.280984	352126.577122	52.847949
3209.855843	351826.184655	52.852954
3208.902571	351530.785871	52.857959
3208.146702	351236.321319	52.862964
3207.896824	350933.147461	52.867969
3207.077487	350643.906982	52.872973
3206.019399	350342.511912	52.877978
3205.462406	350043.606403	52.882983
3204.832790	349752.422328	52.887988
3204.275306	349446.692791	52.892993
3203.241559	349156.460243	52.897997
3202.596431	348862.906923	52.903002
3202.187976	348574.557575	52.908007
3201.458658	348278.469324	52.913012
3200.976074	347986.234558	52.918017
3200.281125	347699.351269	52.923021
3199.552237	347397.582521	52.928026
3198.759318	347113.893218	52.933031
3198.099679	346815.215535	52.938036
3197.359798	346504.866366	52.943041
3196.299725	346226.839832	52.948045
3195.752363	345934.273786	52.953050
3195.142006	345642.428886	52.958055
3194.550471	345365.647587	52.963060
3194.013263	345076.028092	52.968065
3193.075610	344796.346284	52.973069
3192.663846	344504.871476	52.978074
3192.470610	344211.324378	52.983079
3191.414640	343921.475777	52.988084
3190.939517	343621.810599	52.993089
3190.255668	343333.376548	52.998093
3189.624439	343039.740195	53.003098
3188.835472	342748.290936	53.008103
3188.101231	342450.977169	53.013108
3187.512320	342160.817022	53.018113
3186.928523	341869.229232	53.023117
3186.103216	341577.932794	53.028122
3185.181291	341280.846612	53.033127
3184.440679	341000.174022	53.038132
3184.134699	340707.620372	53.043137
3183.488405	340416.035552	53.048141
3182.644801	340122.826000	53.053146
3182.044645	339835.863976	53.058151
3181.459295	339549.840140	53.063156
3180.862162	339253.889270	53.068161
3179.970784	338970.584035	53.073165
3179.177985	338680.007091	53.078170
3178.419064	338384.205039	53.083175
3177.733449	338103.001677	53.088180
3177.119897	337821.862053	53.093185
3176.585930	337530.017069	53.098189
3175.733817	337247.894453	53.103194
3175.244774	336959.349105	53.108199
3174.550216	336678.471919	53.113204
3174.111834	336385.792100	53.118209
3173.332483	336107.115157	53.123213
3172.495748	335816.888769	53.128218
3172.316728	335522.738538	53.133223
3171.297013	335236.993531	53.138228
3170.700072	334951.587738	53.143233
3170.162069	334669.073534	53.148237
3169.482339	334375.888526	53.153242
3168.738268	334094.957439	53.158247
3168.079630	333800.137359	53.163252
3167.572406	333507.634163	53.168257
3166.542456	333222.315132	53.173261
3165.850569	332935.592185	53.178266
3165.824526	332632.571491	53.183271
3164.722705	332355.152250	53.188276
3164.114905	332067.954221	53.193281
3163.513838	331769.297769	53.198285
3162.886450	331477.696190	53.203290
3162.087993	331190.219298	53.208295
3161.030815	330905.200756	53.213300
3160.654736	330608.515118	53.218305
3159.931249	330348.900227	53.223309
3159.339880	330053.901218	53.228314
3158.926060	329759.483952	53.233319
3157.800650	329478.773217	53.238324
3157.516927	329193.702044	53.243329
3156.901822	328898.702203	53.248333
3156.306168	328617.802588	53.253338
3155.202503	328325.652869	53.258343
3154.434545	328033.728969	53.263348
3153.836720	327750.458761	53.268353
3153.079930	327482.666693	53.273357
3152.003422	327190.457432	53.278362
3151.426403	326903.463700	53.283367
3151.095674	326639.776737	53.288372
3150.351517	326364.238997	53.293377
3149.458729	326083.479022	53.298381
3148.923780	325797.162027	53.303386
3148.443024	325522.801783	53.308391
3147.789439	325242.637512	53.313396
3147.328988	324947.623700	53.318401
3146.437741	324683.509752	53.323405
3145.506808	324399.363680	53.328410
3144.951463	324126.309012	53.333415
3144.331795	323842.137229	53.338420
3143.830660	323560.186280	53.343425
3143.233775	323290.114363	53.348429
3142.667568	323003.868926	53.353434
3141.716431	322721.349834	53.358439
3140.823532	322445.924281	53.363444
3140.492922	322158.136503	53.368449
3139.859126	321885.316134	53.373453
3138.804009	321613.299950	53.378458
3138.145415	321330.093460	53.383463
3137.829993	321059.078821	53.388468
3137.208064	320777.774372	53.393473
3136.356920	320500.375496	53.398477
3135.841220	320218.466845	53.403482
3135.140460	319933.531149	53.408487
3134.410969	319667.517420	53.413492
3134.119504	319380.427331	53.418497
3133.427428	319098.135702	53.423501
3132.507993	318820.105922	53.428506
3131.739044	318538.792311	53.433511
3131.155763	318259.587318	53.438516
3130.713418	317988.405354	53.443521
3129.822520	317705.046068	53.448525
3129.276790	317418.830425	53.453530
3128.533668	317134.402088	53.458535
3127.582264	316868.899290	53.463540
3127.303817	316581.060164	53.468545
3126.601119	316306.731772	53.473549
3125.727398	316031.487540	53.478554
3125.146146	315748.633716	53.483559
3124.188686	315469.632630	53.488564
3123.914052	315191.184767	53.493569
3123.240413	314916.415064	53.498573
3122.869297	314628.890508	53.503578
3122.033164	314352.286164	53.508583
3121.228716	314081.965559	53.513588
3120.371858	313795.126657	53.518593
3120.006008	313519.209584	53.523597
3119.205049	313244.888460	53.528602
3118.619563	312964.726780	53.533607
3117.652227	312669.855734	53.538612
3116.956998	312399.462606	53.543617
3116.316858	312124.502028	53.548621
3115.584191	311852.152732	53.553626
3115.438792	311567.283335	53.558631
3114.252066	311304.451730	53.563636
3114.193877	311015.569238	53.568641
3113.451491	310738.406003	53.573645
3112.304700	310466.220707	53.578650
3111.739276	310191.701897	53.583655
3110.989469	309918.866800	53.588660
3110.205972	309635.239413	53.593665
3109.795284	309376.838726	53.598669
3109.356441	309091.678537	53.603674
3108.785780	308809.976264	53.608679
3107.759506	308533.234665	53.613684
3107.071222	308253.688742	53.618689
3106.525039	307971.522269	53.623693
3105.622532	307695.981496	53.628698
3104.832221	307425.897339	53.633703
3104.292188	307154.627063	53.638708
3103.703547	306876.233651	53.643713
3102.912171	306611.571990	53.648717
3102.290912	306330.865213	53.653722
3101.734441	306055.495289	53.658727
3100.913975	305785.081373	53.663732
3100.298067	305512.062523	53.668737
3099.943588	305246.819641	53.673741
3099.110845	304972.942704	53.678746
3098.471233	304689.790645	53.683751
3097.531754	304427.465399	53.688756
3096.959229	304150.591616	53.693761
3096.205020	303882.073321	53.698765
3095.475440	303610.953104	53.703770
3095.113821	303342.677242	53.708775
3094.233968	303072.089090	53.713780
3093.666806	302799.108082	53.718785
3092.776292	302527.654756	53.723789
3092.119269	302269.686431	53.728794
3091.679425	301984.918461	53.733799
3090.939812	301726.529340	53.738804
3090.588773	301450.455710	53.743809
3089.436755	301187.827153	53.748813
3088.948028	300914.677492	53.753818
3088.343858	300640.399638	53.758823
3087.210548	300376.595301	53.763828
3087.043040	300093.792577	53.768833
3086.060616	299832.331835	53.773837
3085.547797	299574.259797	53.778842
3084.960971	299300.868233	53.783847
3084.351111	299032.725971	53.788852
3083.716460	298759.875885	53.793857
3083.010349	298494.982253	53.798861
3081.934255	298222.812364	53.803866
3081.834682	297954.460319	53.808871
3080.730462	297696.529941	53.813876
3080.506472	297416.049132	53.818881
3079.611242	297151.285264	53.823885
3079.140367	296883.346901	53.828890
3078.485767	296615.539089	53.833895
3077.707800	296344.745317	53.838900
3077.359254	296071.922243	53.843905
3076.295879	295800.128713	53.848909
3075.422283	295528.508505	53.853914
3075.275235	295260.185528	53.858919
3074.531738	294995.878511	53.863924
3073.874606	294716.812008	53.868929
3072.870610	294446.586187	53.873933
3072.264036	294183.045928	53.878938
3071.801573	293913.777870	53.883943
3071.156615	293657.934132	53.888948
3070.622152	293374.109513	53.893953
3069.512026	293107.642474	53.898957
3068.919655	292837.756954	53.903962
3068.160567	292559.289515	53.908967
3067.663303	292297.359592	53.913972
3067.094673	292042.622486	53.918977
3066.247637	291761.162846	53.923981
3065.745759	291489.835253	53.928986
3065.415828	291224.847029	53.933991
3064.100988	290968.342280	53.938996
3063.828037	290688.318605	53.944001
3063.198122	290419.225786	53.949005
3062.219693	290150.162374	53.954010
3061.891437	289880.766584	53.959015
3061.111724	289615.338527	53.964020
3060.157195	289341.635401	53.969025
3059.579483	289084.324533	53.974029
3058.693351	288819.931267	53.979034
3058.309749	288549.880783	53.984039
3057.495701	288290.467314	53.989044
3056.950104	288021.740844	53.994049
3056.424742	287762.102959	53.999053
3055.385821	287490.168747	54.004058
3055.140214	287227.430002	54.009063
3054.475315	286966.642027	54.014068
3053.616237	286697.913114	54.019073
3052.950045	286429.637353	54.024077
3052.324727	286172.611760	54.029082
3051.984144	285902.399433	54.034087
3050.935033	285642.817328	54.039092
3050.318499	285370.610842	54.044097
3049.584468	285112.430183	54.049101
3048.558390	284843.216965	54.054106
3048.376682	284568.852720	54.059111
3047.814546	284317.699003	54.064116
3046.817744	284048.939057	54.069121
3046.217810	283781.898904	54.074125
3045.365786	283517.725453	54.079130
3045.014912	283254.949688	54.084135
3044.220254	282993.441018	54.089140
3043.574061	282720.193345	54.094145
3043.008144	282460.303624	54.099149
3041.969455	282207.772507	54.104154
3041.255301	281947.320227	54.109159
3040.825450	281691.330709	54.114164
3040.012869	281430.537215	54.119169
3039.638930	281166.159566	54.124173
3038.900066	280905.328713	54.129178
3038.374209	280645.966673	54.134183
3037.338543	280391.447790	54.139188
3036.717105	280124.281918	54.144193
3036.371040	279868.151080	54.149197
3035.596829	279602.257151	54.154202
3034.932810	279339.707515	54.159207
3034.165376	279075.544194	54.164212
3033.533546	278814.695687	54.169217
3033.070399	278560.645929	54.174221
3032.276052	278299.440985	54.179226
3031.707029	278027.962039	54.184231
3030.747651	277775.264059	54.189236
3030.173097	277500.194835	54.194241
3029.452066	277237.679180	54.199245
3028.539034	276982.274077	54.204250
3027.949834	276713.650531	54.209255
3027.337332	276465.201595	54.214260
3026.577795	276212.497215	54.219265
3026.013248	275955.101233	54.224269
3025.517240	275700.444968	54.229274
3024.879186	275442.805898	54.234279
3023.941856	275186.436665	54.239284
3023.403203	274920.733829	54.244289
3022.880097	274666.794924	54.249293
3022.150670	274413.296168	54.254298
3021.343626	274151.277790	54.259303
3020.504922	273899.400850	54.264308
3020.146167	273638.635895	54.269313
3019.617091	273378.636496	54.274317
3019.023612	273124.148484	54.279322
3018.661058	272859.691275	54.284327
3017.410155	272606.810006	54.289332
3016.692273	272345.337965	54.294337
3016.279319	272090.414007	54.299341
3015.663484	271835.776885	54.304346
3015.196399	271571.438285	54.309351
3014.207337	271318.541244	54.314356
3013.362771	271052.301435	54.319361
3012.831322	270799.739567	54.324365
3012.356882	270542.151473	54.329370
3011.727376	270276.107033	54.334375
3010.858804	270031.137346	54.339380
3010.184947	269768.614704	54.344385
3009.700586	269507.793995	54.349389
3009.058006	269250.232889	54.354394
3008.338650	268986.673505	54.359399
3007.163895	268734.621558	54.364404
3007.112888	268481.220293	54.369409
3006.175387	268232.289046	54.374413
3005.450766	267983.044050	54.379418
3005.166365	267708.719660	54.384423
3004.156574	267457.737243	54.389428
3003.645638	267184.263941	54.394433
3002.816906	266928.847101	54.399437
3002.272315	266678.631856	54.404442
3001.397695	266425.922154	54.409447
3000.690861	266175.630966	54.414452
3000.658463	265916.752258	54.419457
2999.745081	265656.586925	54.424461
2998.752607	265405.297167	54.429466
2998.692762	265140.718384	54.434471
2997.502063	264878.305274	54.439476
2996.849692	264623.090989	54.444481
2996.361707	264372.282286	54.449485
2995.376565	264114.344978	54.454490
2994.896530	263850.241029	54.459495
2994.258745	263610.153103	54.464500
2993.866396	263351.282036	54.469505
2993.043597	263086.366976	54.474509
2991.942476	262833.338770	54.479514
2991.704964	262575.054992	54.484519
2990.764240	262320.499168	54.489524
2990.204131	262073.727404	54.494529
2989.674512	261815.439519	54.499533
2988.991868	261567.083064	54.504538
2988.259093	261300.117749	54.509543
2987.465170	261058.350019	54.514548
2986.919020	260797.391478	54.519553
2985.810669	260552.261245	54.524557
2985.192873	260305.932987	54.529562
2984.760798	260046.790742	54.534567
2984.071541	259801.569348	54.539572
2983.188055	259550.546817	54.544577
2982.730086	259304.805371	54.549581
2982.074389	259053.518037	54.554586
2981.574487	258796.297797	54.559591
2980.796603	258555.522943	54.564596
2980.389656	258298.059280	54.569601
2979.311428	258050.889157	54.574605
2978.527809	257798.655548	54.579610
2978.218522	257542.017644	54.584615
2977.550608	257305.505140	54.589620
2977.186187	257050.455477	54.594625
2976.297470	256788.536486	54.599629
2975.507574	256537.654992	54.604634
2974.835153	256282.782276	54.609639
2974.024017	256038.882754	54.614644
2973.102322	255776.537222	54.619649
2972.994167	255537.951512	54.624653
2971.980339	255291.028847	54.629658
2971.605996	255037.180033	54.634663
2970.781019	254796.009109	54.639668
2970.135578	254535.607827	54.644673
2969.776672	254289.270295	54.649677
2968.998047	254042.821237	54.654682
2968.257855	253791.731399	54.659687
2967.364051	253540.156860	54.664692
2966.802690	253283.513028	54.669697
2966.378081	253043.452337	54.674701
2965.403027	252791.458706	54.679706
2965.052386	252541.454852	54.684711
2964.240269	252290.964118	54.689716
2963.822417	252035.012352	54.694721
2963.004115	251790.125984	54.699725
2961.940762	251533.920580	54.704730
2961.413376	251285.729112	54.709735
2960.657418	251046.003644	54.714740
2959.998378	250790.550258	54.719745
2959.770752	250549.595845	54.724749
2958.721661	250305.868629	54.729754
2958.354146	250044.283711	54.734759
2957.386144	249801.257457	54.739764
2956.513228	249542.758384	54.744769
2956.054570	249304.567257	54.749773
2955.601864	249059.881619	54.754778
2954.950505	248805.448737	54.759783
2954.386095	248567.402781	54.764788
2953.540578	248316.592171	54.769793
2952.558527	248062.773102	54.774797
2951.905052	247824.182130	54.779802
2951.733302	247579.912725	54.784807
2950.845258	247333.694357	54.789812
2950.063236	247075.592441	54.794817
2949.370867	246837.340250	54.799821
2948.848367	246605.173381	54.804826
2948.298972	246346.322872	54.809831
2947.474950	246108.398305	54.814836
2946.540656	245852.894713	54.819841
2946.375063	245608.143771	54.824845
2945.118427	245366.469070	54.829850
2944.711260	245115.263471	54.834855
2943.937690	244884.132324	54.839860
2943.452865	244630.851720	54.844865
2942.664837	244393.280897	54.849869
2942.232690	244149.058587	54.854874
2941.738801	243901.332263	54.859879
2940.773313	243662.288368	54.864884
2940.079698	243415.307604	54.869889
2939.774660	243170.735925	54.874893
2938.667362	242920.332843	54.879898
2938.282732	242672.209569	54.884903
2937.479182	242427.336244	54.889908
2936.972630	242188.120557	54.894913
2936.349765	241937.337134	54.899917
2935.297381	241691.384171	54.904922
2935.118955	241440.913362	54.909927
2934.258922	241203.512611	54.914932
2933.743647	240954.853201	54.919937
2933.067380	240703.087617	54.924941
2932.354646	240468.771691	54.929946
2931.990709	240212.654144	54.934951
2930.809480	239972.301836	54.939956
2930.524607	239722.437138	54.944961
2929.696606	239480.043677	54.949965
2928.805557	239236.769447	54.954970
2928.325318	238977.922849	54.959975
2927.527454	238729.592980	54.964980
2926.917172	238503.948135	54.969985
2926.375561	238247.990382	54.974989
2925.690408	238003.463905	54.979994
2925.231816	237754.063906	54.984999
2924.203420	237519.192825	54.990004
2923.828612	237256.284710	54.995009
2923.145571	237014.255566	55.000013
2922.211373	236767.759609	55.005018
2921.620155	236522.101150	55.010023
2920.882772	236277.994224	55.015028
2920.128336	236032.006239	55.020033
2919.500338	235794.834710	55.025037
2918.576110	235549.664107	55.030042
2918.080359	235313.771374	55.035047
2917.157016	235069.798548	55.040052
2917.248868	234818.204777	55.045057
2916.285431	234587.735074	55.050061
2915.298989	234350.547213	55.055066
2914.901111	234106.900902	55.060071
2914.011168	233860.252037	55.065076
2913.555625	233625.222592	55.070081
2913.077068	233384.111664	55.075085
2911.996515	233133.929943	55.080090
2912.183368	232893.402364	55.085095
2911.029196	232650.184922	55.090100
2910.551050	232399.018502	55.095105
2909.801005	232149.016144	55.100109
2908.772891	231915.201820	55.105114
2908.545331	231662.418960	55.110119
2907.387666	231424.552328	55.115124
2906.622580	231185.401938	55.120129
2906.343447	230943.985447	55.125133
2905.492614	230697.414843	55.130138
2904.790863	230464.392704	55.135143
2903.845434	230235.789241	55.140148
2903.471179	229996.121710	55.145153
2902.774928	229748.485218	55.150157
2902.224360	229519.540945	55.155162
2901.545462	229272.717789	55.160167
2901.039351	229040.686790	55.165172
2900.059426	228798.877673	55.170177
2899.790529	228552.067974	55.175181
2899.251937	228308.153373	55.180186
2898.390652	228065.538160	55.185191
2897.709462	227821.596563	55.190196
2897.151801	227582.652005	55.195201
2896.509906	227344.077902	55.200205
2895.374556	227107.874109	55.205210
2894.906677	226851.985555	55.210215
2894.287430	226618.807671	55.215220
2893.611965	226383.245981	55.220225
2893.202771	226137.993040	55.225229
2892.434505	225902.561959	55.230234
2891.913950	225650.911900	55.235239
2890.608012	225412.435638	55.240244
2890.529100	225165.720177	55.245249
2889.735825	224918.443852	55.250253
2888.907032	224684.044239	55.255258
2888.392450	224447.940613	55.260263
2887.798101	224211.748459	55.265268
2886.965838	223966.250697	55.270273
2886.556948	223719.324520	55.275277
2885.806178	223490.848263	55.280282
2885.215050	223242.870351	55.285287
2884.355055	223000.995285	55.290292
2883.398242	222764.088262	55.295297
2883.157540	222514.962365	55.300301
2882.194608	222282.933340	55.305306
2881.574660	222047.159029	55.310311
2881.292260	221803.897754	55.315316
2880.448964	221560.076835	55.320321
2879.664599	221321.466564	55.325325
2878.991858	221092.004769	55.330330
2878.265152	220844.157802	55.335335
2877.641224	220603.742217	55.340340
2877.101827	220373.204919	55.345345
2876.330556	220131.172050	55.350349
2875.390709	219893.863853	55.355354
2875.053679	219650.261698	55.360359
2874.020554	219411.314975	55.365364
2873.529321	219179.640819	55.370369
2872.831002	218950.571514	55.375373
2872.171947	218717.448781	55.380378
2871.901896	218471.905059	55.385383
2871.085007	218238.579722	55.390388
2869.989116	218002.829851	55.395393
2869.723672	217761.653924	55.400397
2868.935918	217530.821180	55.405402
2868.123763	217294.137670	55.410407
2867.868258	217065.627948	55.415412
2867.185101	216816.794831	55.420417
2866.337661	216583.836144	55.425421
2865.785467	216343.181405	55.430426
2865.230184	216105.952046	55.435431
2864.179049	215876.171997	55.440436
2863.533593	215633.866997	55.445441
2862.884307	215392.963612	55.450445
2862.246950	215173.672496	55.455450
2861.517931	214929.512085	55.460455
2861.060862	214703.485929	55.465460
2860.144286	214463.875538	55.470465
2859.849955	214226.840451	55.475469
2858.931705	213999.858655	55.480474
2858.280690	213757.841221	55.485479
2857.722946	213537.002647	55.490484
2857.044057	213289.365374	55.495489
2856.405317	213053.330867	55.500493
2855.457641	212813.667656	55.505498
2855.093789	212580.595172	55.510503
2854.442644	212343.852385	55.515508
2853.828685	212105.564464	55.520513
2853.400526	211875.470318	55.525517
2852.199444	211648.223176	55.530522
2851.878814	211405.105636	55.535527
2850.744712	211163.937919	55.540532
2850.244139	210942.819017	55.545537
2849.791154	210695.575827	55.550541
2849.074041	210471.298158	55.555546
2848.453693	210225.737906	55.560551
2847.855561	209991.235447	55.565556
2847.245797	209758.619393	55.570561
2846.536036	209519.452594	55.575565
2845.706026	209291.824180	55.580570
2845.382519	209046.806988	55.585575
2844.402775	208816.836704	55.590580
2843.626229	208578.129553	55.595585
2843.347228	208352.593710	55.600589
2842.644184	208110.847617	55.605594
2842.029911	207871.888414	55.610599
2840.953655	207643.986884	55.615604
2840.208404	207401.983006	55.620609
2840.312809	207164.185486	55.625613
2839.006242	206933.255863	55.630618
2838.882130	206691.576457	55.635623
2837.772346	206457.219388	55.640628
2836.904066	206217.785138	55.645633
2836.572014	205976.319723	55.650637
2835.934367	205751.423077	55.655642
2835.370872	205509.894396	55.660647
2834.316528	205272.822420	55.665652
2833.590254	205045.588056	55.670657
2833.298344	204805.660996	55.675661
2832.293914	204584.924857	55.680666
2831.695848	204341.026598	55.685671
2830.717418	204122.477057	55.690676
2830.337662	203887.212851	55.695681
2829.934402	203651.673346	55.700685
2829.458001	203431.876095	55.705690
2828.647034	203186.934694	55.710695
2827.841628	202953.727014	55.715700
2827.535894	202720.924753	55.720705
2826.842968	202484.163319	55.725709
2825.585293	202248.026805	55.730714
2825.138565	202002.192918	55.735719
2824.597409	201778.543627	55.740724
2823.966836	201543.672438	55.745729
2823.478861	201308.716026	55.750733
2822.661446	201074.245453	55.755738
2821.961794	200839.540884	55.760743
2821.063980	200611.053366	55.765748
2820.522869	200371.629910	55.770753
2820.315336	200125.448303	55.775757
2818.934297	199895.640476	55.780762
2818.453661	199669.750441	55.785767
2817.774069	199436.804808	55.790772
2817.124510	199198.027216	55.795777
2816.360149	198961.317628	55.800781
2815.880227	198741.921240	55.805786
2815.371562	198507.527320	55.810791
2814.348164	198278.636841	55.815796
2813.861098	198044.266979	55.820801
2813.474510	197808.762435	55.825805
2812.352893	197586.431139	55.830810
2811.936020	197352.753084	55.835815
2811.141591	197115.700150	55.840820
2810.400934	196890.359291	55.845825
2809.701294	196659.541272	55.850829
2809.122848	196433.973092	55.855834
2808.419471	196203.793911	55.860839
2807.515497	195982.923723	55.865844
2806.847285	195747.956558	55.870849
2806.289075	195512.527684	55.875853
2805.431059	195301.374607	55.880858
2805.022284	195061.139758	55.885863
2804.199034	194841.394142	55.890868
2803.860642	194607.843244	55.895873
2803.424699	194391.155660	55.900877
2802.635069	194157.003913	55.905882
2802.290484	193917.107838	55.910887
2801.244071	193686.765253	55.915892
2800.491290	193464.164265	55.920897
2800.194863	193223.080540	55.925901
2799.674396	192999.770454	55.930906
2798.765914	192765.071435	55.935911
2798.206034	192527.837190	55.940916
2797.204801	192293.307771	55.945921
2796.717614	192069.958416	55.950925
2795.648420	191840.849427	55.955930
2795.206125	191596.704877	55.960935
2794.236904	191382.328680	55.965940
2793.458063	191155.225372	55.970945
2793.343585	190927.432628	55.975949
2792.334979	190700.367827	55.980954
2791.926117	190467.280107	55.985959
2791.067709	190238.641453	55.990964
2790.233079	190019.936812	55.995969
2789.597453	189791.163210	56.000973
2789.015794	189574.418036	56.005978
2788.382568	189353.979655	56.010983
2787.728259	189123.316491	56.015988
2787.012066	188902.079076	56.020993
2786.890418	188673.840106	56.025997
2785.663782	188445.497344	56.031002
2785.324261	188220.692004	56.036007
2784.554748	187994.034739	56.041012
2784.061989	187769.154041	56.046017
2783.285868	187533.009104	56.051021
2782.246917	187311.779374	56.056026
2781.728108	187079.807060	56.061031
2781.192065	186865.140815	56.066036
2780.397365	186637.667171	56.071041
2779.886658	186411.689035	56.076045
2779.354112	186192.369074	56.081050
2778.963289	185957.214325	56.086055
2777.882793	185732.907282	56.091060
2776.944145	185498.248752	56.096065
2776.689645	185282.514815	56.101069
2775.975960	185069.551627	56.106074
2775.562190	184823.872769	56.111079
2774.857006	184606.852201	56.116084
2773.985631	184374.784008	56.121089
2773.431684	184143.251918	56.126093
2772.662996	183918.624572	56.131098
2772.175225	183691.943888	56.136103
2771.587607	183459.835470	56.141108
2770.791121	183226.998068	56.146113
2770.364629	183001.888602	56.151117
2769.374322	182777.632839	56.156122
2768.731184	182537.154848	56.161127
2767.955530	182313.694298	56.166132
2767.144411	182089.222828	56.171137
2766.928756	181856.847622	56.176141
2766.249161	181635.130768	56.181146
2765.659655	181399.013704	56.186151
2764.838811	181167.908305	56.191156
2763.793255	180948.771573	56.196161
2763.495148	180723.653424	56.201165
2762.500433	180492.324744	56.206170
2762.174102	180269.070603	56.211175
2761.438311	180039.407858	56.216180
2760.558946	179817.095908	56.221185
2760.186165	179589.972982	56.226189
2759.286139	179359.334994	56.231194
2758.800166	179133.809702	56.236199
2758.480057	178903.667438	56.241204
2757.650745	178676.036563	56.246209
2757.392630	178440.074015	56.251213
2756.360121	178213.864262	56.256218
2755.503503	177982.323768	56.261223
2754.939396	177755.647969	56.266228
2753.916206	177526.680279	56.271233
2753.570938	177290.636209	56.276237
2752.871975	177064.417963	56.281242
2752.187474	176840.208302	56.286247
2751.532785	176616.770996	56.291252
2751.004338	176389.588182	56.296257
2750.396781	176152.014928	56.301261
2749.726684	175939.356779	56.306266
2749.000004	175694.135457	56.311271
2748.033137	175464.864948	56.316276
2747.524310	175237.558174	56.321281
2746.860126	175015.339325	56.326285
2746.243807	174781.641867	56.331290
2745.555926	174560.103336	56.336295
2744.767199	174342.868127	56.341300
2744.258046	174103.497842	56.346305
2744.050117	173880.284468	56.351309
2743.096505	173656.796174	56.356314
2742.418671	173416.922501	56.361319
2741.638838	173182.471631	56.366324
2740.495594	172953.751961	56.371329
2740.099500	172731.248820	56.376333
2739.013681	172513.701709	56.381338
2738.711711	172285.132400	56.386343
2737.852194	172065.122777	56.391348
2737.650213	171838.587761	56.396353
2737.115687	171611.292786	56.401357
2736.388527	171402.800791	56.406362
2735.756670	171168.834325	56.411367
2734.920326	170933.884245	56.416372
2734.235570	170698.288407	56.421377
2733.742925	170481.179930	56.426381
2732.532635	170250.985860	56.431386
2732.069657	170026.689981	56.436391
2731.665024	169812.776000	56.441396
2730.950449	169583.384831	56.446401
2730.644459	169355.291008	56.451405
2729.295589	169136.303675	56.456410
2728.652504	168903.687847	56.461415
2728.298563	168679.051860	56.466420
2727.497043	168458.748156	56.471425
2726.895756	168236.430215	56.476429
2726.192049	168017.677688	56.481434
2725.747611	167774.775035	56.486439
2725.012768	167556.653187	56.491444
2724.150781	167338.667176	56.496449
2723.788962	167102.088426	56.501453
2722.740798	166881.209816	56.506458
2722.199921	166652.965855	56.511463
2721.921311	166426.843440	56.516468
2720.695489	166210.943404	56.521473
2720.386290	165990.283571	56.526477
2719.783167	165767.039441	56.531482
2719.202526	165538.045607	56.536487
2718.168978	165310.816095	56.541492
2717.757040	165096.739046	56.546497
2717.424110	164857.321594	56.551501
2716.198869	164638.099128	56.556506
2715.491643	164407.174148	56.561511
2715.155836	164182.193342	56.566516
2714.449150	163958.010136	56.571521
2713.809116	163734.758650	56.576525
2712.992992	163507.810934	56.581530
2712.518318	163277.479237	56.586535
2711.665576	163058.219893	56.591540
2711.211329	162837.207682	56.596545
2710.285530	162602.844852	56.601549
2709.965047	162386.760181	56.606554
2709.356280	162152.032174	56.611559
2708.557633	161926.337563	56.616564
2707.650133	161710.833064	56.621569
2707.198771	161406.219823	56.626573
2706.211143	161185.073339	56.631578
2705.522783	160962.151696	56.636583
2704.838059	160740.019132	56.641588
2704.252276	160515.176928	56.646593
2703.704670	160287.850897	56.651597
2703.097549	160072.702794	56.656602
2702.332791	159845.426705	56.661607
2701.620370	159625.034541	56.666612
2701.018553	159394.951254	56.671617
2700.827861	159167.194456	56.676621
2699.326947	158956.453728	56.681626
2699.254206	158727.371613	56.686631
2698.372524	158506.835267	56.691636
2697.528336	158286.739328	56.696641
2697.284273	158067.528604	56.701645
2696.334458	157844.579040	56.706650
2695.709158	157619.303891	56.711655
2695.034549	157404.589616	56.716660
2694.129287	157182.094901	56.721665
2693.695114	156954.696190	56.726669
2693.134047	156745.968362	56.731674
2692.535110	156509.712618	56.736679
2691.971359	156287.449233	56.741684
2690.805589	156073.520220	56.746689
2690.747578	155844.785297	56.751693
2689.606916	155631.198295	56.756698
2689.061025	155398.882550	56.761703
2688.665476	155176.523451	56.766708
2687.656478	154960.339263	56.771713
2687.100203	154729.936505	56.776717
2686.372663	154516.888496	56.781722
2685.937352	154295.672801	56.786727
2684.943056	154066.055801	56.791732
2684.334998	153843.065398	56.796737
2683.531427	153621.976017	56.801741
2682.341487	153409.580267	56.806746
2681.851276	153199.248622	56.811751
2681.432623	152990.559408	56.816756
2680.837750	152777.183613	56.821761
2680.406709	152558.342930	56.826765
2679.536573	152340.043551	56.831770
2679.033347	152121.153623	56.836775
2678.496440	151898.584364	56.841780
2677.593643	151688.289485	56.846785
2677.269657	151467.634116	56.851789
2676.561427	151251.845651	56.856794
2675.751532	151025.334433	56.861799
2675.287528	150808.048488	56.866804
2674.071270	150585.354218	56.871809
2673.650824	150366.856823	56.876813
2673.098307	150163.583021	56.881818
2672.480963	149938.421487	56.886823
2671.969978	149713.104848	56.891828
2671.221107	149494.805127	56.896833
2670.750519	149277.466849	56.901837
2669.990457	149054.126112	56.906842
2669.032169	148828.657701	56.911847
2668.851981	148612.790306	56.916852
2667.961776	148399.260981	56.921857
2667.327410	148180.443609	56.926861
2666.371271	147959.302087	56.931866
2665.795865	147727.883658	56.936871
2665.466919	147499.719481	56.941876
2664.641215	147291.004019	56.946881
2663.715173	147070.829743	56.951885
2663.534364	146860.324649	56.956890
2663.009567	146627.711547	56.961895
2662.181010	146405.111786	56.966900
2661.265576	146182.730688	56.971905
2660.947995	145948.691801	56.976909
2659.787160	145736.582969	56.981914
2659.491348	145508.554918	56.986919
2658.870882	145278.190829	56.991924
2657.702869	145062.529405	56.996929
2657.316730	144840.582235	57.001933
2656.519444	144626.631474	57.006938
2655.954477	144398.349142	57.011943
2655.395605	144180.957979	57.016948
2654.703851	143966.842526	57.021953
2654.194506	143741.072293	57.026957
2652.908809	143522.708043	57.031962
2652.423883	143292.019445	57.036967
2651.979035	143085.495333	57.041972
2651.287264	142872.696279	57.046977
2650.507243	142647.116686	57.051981
2649.816372	142442.402135	57.056986
2649.304268	142206.389036	57.061991
2648.728254	142000.566441	57.066996
2647.853434	141784.728878	57.072001
2647.464385	141555.308768	57.077005
2646.413491	141338.422194	57.082010
2645.747905	141123.102533	57.087015
2645.211469	140905.756334	57.092020
2644.373644	140691.750354	57.097025
2643.905573	140470.800572	57.102029
2643.457918	140263.558987	57.107034
2642.646897	140041.027599	57.112039
2642.104567	139825.723031	57.117044
2640.695526	139611.497552	57.122049
2640.926373	139385.324543	57.127053
2639.803904	139175.757863	57.132058
2639.310851	138961.887400	57.137063
2638.555005	138744.451766	57.142068
2637.605489	138527.493085	57.147073
2637.383006	138314.219645	57.152077
2636.393991	138096.139594	57.157082
2635.611837	137884.647690	57.162087
2635.579566	137673.635605	57.167092
2634.252484	137459.831833	57.172097
2633.939054	137237.890402	57.177101
2633.228138	137025.364253	57.182106
2632.235289	136815.666608	57.187111
2631.664635	136602.498754	57.192116
2631.256811	136389.687776	57.197121
2630.454644	136177.144089	57.202125
2629.856069	135966.691287	57.207130
2629.384156	135749.156434	57.212135
2628.889664	135535.031454	57.217140
2627.621698	135324.816373	57.222145
2627.493008	135109.035860	57.227149
2626.381315	134895.292857	57.232154
2625.783085	134685.611458	57.237159
2625.451357	134462.525199	57.242164
2624.576671	134256.828806	57.247169
2623.558007	134041.730785	57.252173
2622.839794	133836.596945	57.257178
2622.517422	133616.323153	57.262183
2622.330676	133413.089807	57.267188
2620.826536	133194.975474	57.272193
2620.673158	132987.077851	57.277197
2619.980326	132773.690677	57.282202
2619.450816	132564.293272	57.287207
2618.614068	132353.993387	57.292212
2618.136449	132142.672752	57.297217
2617.605854	131925.506253	57.302221
2616.617365	131705.644856	57.307226
2615.831360	131484.495554	57.312231
2615.557000	131276.375515	57.317236
2614.535717	131074.802598	57.322241
2614.162560	130856.095086	57.327245
2613.632342	130632.104776	57.332250
2612.882125	130422.135742	57.337255
2612.036386	130213.593296	57.342260
2611.686715	130006.459874	57.347265
2611.137203	129781.552173	57.352269
2610.355834	129562.868583	57.357274
2609.754684	129337.642391	57.362279
2609.306033	129120.840128	57.367284
2608.167178	128912.074390	57.372289
2607.696407	128684.800632	57.377293
2606.659858	128466.242276	57.382298
2605.905676	128247.272574	57.387303
2605.412053	128039.554214	57.392308
2604.598121	127835.076016	57.397313
2604.191507	127608.042219	57.402317
2603.511422	127403.164991	57.407322
2602.725951	127197.696370	57.412327
2601.648186	126975.663744	57.417332
2600.974689	126766.484843	57.422337
2600.692834	126552.825876	57.427341
2599.775661	126348.959270	57.432346
2599.100952	126146.033646	57.437351
2598.362968	125940.312918	57.442356
2597.736286	125728.111999	57.447361
2597.689550	125521.497512	57.452365
2596.673525	125321.006919	57.457370
2595.694666	125106.326768	57.462375
2595.420506	124893.606617	57.467380
2594.547728	124686.646804	57.472385
2594.097109	124471.049832	57.477389
2593.421761	124274.805262	57.482394
2592.996044	124054.166192	57.487399
2592.095380	123842.353615	57.492404
2591.243694	123648.097154	57.497409
2590.580147	123426.459627	57.502413
2589.803316	123223.127626	57.507418
2589.384719	123013.721385	57.512423
2588.981439	122796.822394	57.517428
2588.108354	122596.062753	57.522433
2587.823198	122384.329232	57.527437
2586.801339	122169.565047	57.532442
2586.066011	121961.207690	57.537447
2585.631314	121754.226471	57.542452
2584.656813	121543.777069	57.547457
2584.018808	121334.406094	57.552461
2583.356459	121122.336079	57.557466
2582.888904	120911.113011	57.562471
2582.487120	120700.160548	57.567476
2581.411846	120499.791638	57.572481
2580.985962	120282.002585	57.577485
2580.072084	120072.139371	57.582490
2579.665920	119864.698652	57.587495
2578.736515	119655.755401	57.592500
2578.419752	119444.202798	57.597505
2577.588152	119230.987722	57.602509
2576.695311	119026.366873	57.607514
2576.289392	118810.408828	57.612519
2575.546223	118602.104703	57.617524
2574.956767	118395.295074	57.622529
2574.232245	118180.116430	57.627533
2573.775926	117977.700892	57.632538
2573.078924	117761.054989	57.637543
2572.101514	117552.669456	57.642548
2571.380526	117345.990614	57.647553
2570.996603	117130.671506	57.652557
2570.393345	116922.822108	57.657562
2569.422319	116709.199186	57.662567
2568.752937	116501.014557	57.667572
2568.230347	116294.744355	57.672577
2567.350393	116082.654671	57.677581
2566.844824	115890.190821	57.682586
2566.200428	115671.192941	57.687591
2565.685932	115470.900991	57.692596
2564.836718	115259.390880	57.697601
2564.346814	115048.238154	57.702605
2563.312683	114850.515205	57.707610
2562.986980	114642.538808	57.712615
2562.371771	114421.452506	57.717620
2561.608447	114223.101255	57.722625
2561.353172	114013.354389	57.727629
2560.269603	113806.387199	57.732634
2559.737291	113590.410648	57.737639
2559.024888	113379.649836	57.742644
2558.112792	113171.765786	57.747649
2557.839048	112965.514941	57.752653
2557.020454	112764.251759	57.757658
2556.192398	112545.919327	57.762663
2555.752100	112338.836897	57.767668
2554.796762	112129.286515	57.772673
2554.195156	111925.361901	57.777677
2553.629811	111728.071536	57.782682
2552.644672	111515.954399	57.787687
2552.257025	111303.883997	57.792692
2551.534942	111105.354157	57.797697
2550.980633	110894.506759	57.802701
2550.084185	110687.516710	57.807706
2549.562592	110483.654716	57.812711
2548.904983	110281.072472	57.817716
2548.440528	110077.972640	57.822721
2547.523342	109860.344276	57.827725
2547.076363	109671.612183	57.832730
2546.303971	109453.869280	57.837735
2545.599059	109243.205823	57.842740
2544.668404	109036.596784	57.847745
2544.418712	108828.523595	57.852749
2543.474478	108623.658903	57.857754
2542.531637	108431.144140	57.862759
2542.261391	108229.094892	57.867764
2541.533537	108026.218792	57.872769
2541.178504	107815.689868	57.877773
2540.269392	107619.216659	57.882778
2539.685020	107409.412899	57.887783
2539.020865	107204.909173	57.892788
2538.180130	107007.256221	57.897793
2537.604951	106792.335796	57.902797
2536.942497	106591.555226	57.907802
2536.187309	106383.665577	57.912807
2535.823413	106180.943950	57.917812
2535.130833	105985.623523	57.922817
2534.295014	105773.659460	57.927821
2533.508734	105563.910096	57.932826
2532.703410	105368.574491	57.937831
2532.472540	105162.820279	57.942836
2531.289433	104970.783589	57.947841
2530.970583	104754.489361	57.952845
2530.515348	104552.627123	57.957850
2529.651249	104360.322730	57.962855
2529.305176	104152.622353	57.967860
2528.101957	103954.049609	57.972865
2527.428805	103744.444232	57.977869
2526.904914	103557.434327	57.982874
2526.348823	103346.982813	57.987879
2526.004284	103136.975451	57.992884
2525.198133	102937.326893	57.997889
2524.726448	102733.420914	58.002893
2523.711029	102522.351705	58.007898
2523.084681	102318.505551	58.012903
2522.543287	102109.686790	58.017908
2521.882583	101916.450180	58.022913
2521.175727	101694.535980	58.027917
2520.371761	101497.912584	58.032922
2519.408563	101290.062442	58.037927
2518.864000	101086.074481	58.042932
2517.951267	100892.226541	58.047937
2517.483076	100691.871114	58.052941
2516.547317	100495.873337	58.057946
2516.102020	100299.152449	58.062951
2515.463914	100105.654479	58.067956
2514.988010	99917.632032	58.072961
2514.455590	99709.099746	58.077965
2513.580654	99508.914140	58.082970
2513.324258	99308.632228	58.087975
2512.878504	99101.950208	58.092980
2511.645242	98912.108660	58.097985
2511.045757	98695.305854	58.102989
2510.385765	98503.613472	58.107994
2509.915457	98305.892301	58.112999
2509.509171	98088.423966	58.118004
2508.473693	97897.912483	58.123009
2507.968136	97688.296938	58.128013
2506.732352	97496.704236	58.133018
2506.322659	97300.117461	58.138023
2505.982249	97090.252890	58.143028
2505.065993	96896.255172	58.148033
2504.770791	96685.099647	58.153037
2504.093704	96484.826620	58.158042
2503.484800	96274.828192	58.163047
2502.816776	96069.001568	58.168052
2502.054071	95869.730581	58.173057
2501.594201	95660.024988	58.178061
2500.613063	95454.488236	58.183066
2499.662039	95256.089654	58.188071
2499.138009	95046.273087	58.193076
2498.761342	94849.309104	58.198081
2498.029815	94649.942468	58.203085
2497.319113	94450.428438	58.208090
2496.691434	94240.680200	58.213095
2495.950713	94037.052498	58.218100
2494.532533	93833.147193	58.223105
2494.558537	93630.841189	58.228109
2494.142685	93441.784626	58.233114
2493.161098	93241.423812	58.238119
2492.617865	93035.009072	58.243124
2491.693871	92835.321303	58.248129
2491.565201	92627.493928	58.253133
2490.683112	92434.030216	58.258138
2490.033884	92231.247867	58.263143
2489.252468	92020.276640	58.268148
2488.628241	91822.325960	58.273153
2487.966052	91623.501675	58.278157
2487.241999	91427.364842	58.283162
2486.357630	91227.989630	58.288167
2486.285235	91022.197455	58.293172
2484.998638	90821.298143	58.298177
2484.600652	90623.442823	58.303181
2483.872622	90425.204097	58.308186
2483.046356	90230.140327	58.313191
2482.556722	90028.621029	58.318196
2481.701003	89836.754696	58.323201
2481.473318	89632.052664	58.328205
2481.045051	89434.891283	58.333210
2479.991938	89225.036076	58.338215
2479.532439	89021.834766	58.343220
2478.660549	88825.624158	58.348225
2477.904093	88620.913983	58.353229
2477.209882	88425.503029	58.358234
2476.521917	88219.378293	58.363239
2475.791008	88026.214759	58.368244
2475.032346	87830.527743	58.373249
2474.613260	87629.545654	58.378253
2474.005303	87440.983221	58.383258
2473.602422	87233.662501	58.388263
2472.922037	87039.320589	58.393268
2471.809487	86841.784059	58.398273
2471.702763	86640.324231	58.403277
2470.757471	86439.899419	58.408282
2470.322909	86234.767763	58.413287
2469.839482	86019.547267	58.418292
2468.780437	85832.655259	58.423297
2468.396428	85631.305902	58.428301
2467.713097	85425.784016	58.433306
2466.785971	85217.348738	58.438311
2466.069739	85016.488894	58.443316
2465.168253	84815.685664	58.448321
2464.712353	84619.694651	58.453325
2464.138606	84417.683200	58.458330
2463.369515	84215.951847	58.463335
2462.847001	84018.569723	58.468340
2461.987703	83817.293832	58.473345
2461.730287	83620.684735	58.478349
2460.840809	83422.459913	58.483354
2459.875042	83223.691257	58.488359
2459.710668	83021.095787	58.493364
2458.738854	82828.993496	58.498369
2457.905189	82624.086681	58.503373
2457.123221	82432.515683	58.508378
2456.722525	82240.201462	58.513383
2455.989543	82033.433687	58.518388
2455.299896	81844.509092	58.523393
2454.942458	81638.769482	58.528397
2454.129426	81451.610942	58.533402
2453.305640	81248.737794	58.538407
2452.828628	81064.102639	58.543412
2451.918703	80857.418893	58.548417
2451.156487	80656.075485	58.553421
2450.297262	80471.151258	58.558426
2449.962968	80269.921199	58.563431
2449.703723	80078.022720	58.568436
2448.633018	79892.135836	58.573441
2447.954781	79677.207370	58.578445
2447.394951	79486.895662	58.583450
2446.600174	79304.177013	58.588455
2446.046602	79101.256628	58.593460
2445.075841	78917.156093	58.598465
2444.711967	78713.696129	58.603469
2444.047043	78519.436613	58.608474
2443.440866	78333.471090	58.613479
2442.998508	78139.084822	58.618484
2441.907410	77938.371299	58.623489
2441.745215	77745.091316	58.628493
2440.888287	77550.522865	58.633498
2440.048365	77347.772882	58.638503
2439.328667	77154.320708	58.643508
2438.839782	76966.435310	58.648513
2438.219568	76759.727641	58.653517
2437.324739	76561.740210	58.658522
2436.491313	76362.997272	58.663527
2436.348719	76168.284377	58.668532
2435.163288	75982.552432	58.673537
2434.721792	75781.896502	58.678541
2434.020118	75593.202108	58.683546
2433.460832	75409.714176	58.688551
2432.823829	75212.174217	58.693556
2432.154090	75024.069308	58.698561
2431.690821	74816.881311	58.703565
2430.918783	74631.894529	58.708570
2429.967055	74426.688730	58.713575
2429.723507	74226.162554	58.718580
2428.710647	74037.025155	58.723585
2428.125112	73842.512545	58.728589
2427.756503	73651.350607	58.733594
2426.677003	73460.277849	58.738599
2426.205624	73264.162531	58.743604
2425.578962	73076.753198	58.748609
2425.109091	72868.319228	58.753613
2424.163334	72677.992961	58.758618
2423.374077	72486.541373	58.763623
2423.050346	72290.171450	58.768628
2422.205051	72107.069401	58.773633
2421.346333	71897.870974	58.778637
2420.748519	71710.102458	58.783642
2420.241948	71527.813584	58.788647
2419.535458	71327.731908	58.793652
2418.848049	71143.935867	58.798657
2418.159764	70943.272383	58.803661
2417.422027	70759.177486	58.808666
2416.770916	70563.079228	58.813671
2416.308278	70360.067425	58.818676
2415.468591	70173.568028	58.823681
2414.787261	69977.461366	58.828685
2414.204806	69794.719060	58.833690
2413.508408	69601.373957	58.838695
2413.141406	69400.960240	58.843700
2412.154915	69222.303184	58.848705
2411.828334	69021.525879	58.853709
2411.259939	68826.293218	58.858714
2410.325926	68633.413356	58.863719
2410.112469	68439.471068	58.868724
2408.952841	68244.553294	58.873729
2408.435290	68043.847949	58.878733
2407.732140	67857.652916	58.883738
2406.695609	67655.735436	58.888743
2406.281505	67462.094338	58.893748
2405.403237	67282.082460	58.898753
2404.760075	67082.838294	58.903757
2404.337417	66900.287670	58.908762
2403.476704	66711.272223	58.913767
2403.010846	66512.607458	58.918772
2402.462152	66326.503921	58.923777
2401.489827	66132.172932	58.928781
2400.830351	65945.761297	58.933786
2400.622893	65754.064555	58.938791
2400.210772	65558.713222	58.943796
2399.050232	65364.704776	58.948801
2398.591858	65165.400374	58.953805
2397.929987	64977.627414	58.958810
2396.852267	64794.959878	58.963815
2396.855848	64586.595799	58.968820
2395.756559	64396.466140	58.973825
2395.117758	64201.373497	58.978829
2394.504406	64005.376432	58.983834
2393.741125	63811.915929	58.988839
2393.146929	63614.514042	58.993844
2392.096816	63432.127408	58.998849
2391.872934	63230.212874	59.003853
2391.408317	63041.674077	59.008858
2390.706505	62849.856756	59.013863
2390.159947	62645.558567	59.018868
2389.556466	62459.121278	59.023873
2388.618989	62256.082823	59.028877
2387.828001	62060.118081	59.033882
2387.034963	61866.640890	59.038887
2386.611787	61670.561703	59.043892
2385.728455	61490.304186	59.048897
2385.281121	61291.307558	59.053901
2384.489281	61101.690734	59.058906
2383.462103	60912.910886	59.063911
2383.200797	60725.698794	59.068916
2382.430969	60534.124633	59.073921
2381.890943	60337.564975	59.078925
2381.216664	60146.790000	59.083930
2380.613721	59953.340264	59.088935
2380.210748	59751.161996	59.093940
2379.227115	59566.105065	59.098945
2378.527010	59369.315019	59.103949
2377.893272	59178.632091	59.108954
2377.052676	58985.173049	59.113959
2376.578581	58787.887971	59.118964
2375.929998	58610.931795	59.123969
2375.121652	58421.331999	59.128973
2374.403929	58228.063898	59.133978
2373.828222	58032.933127	59.138983
2373.295087	57837.294387	59.143988
2372.386853	57654.149896	59.148993
2371.897121	57459.888253	59.153997
2371.178699	57273.985917	59.159002
2370.499004	57083.993217	59.164007
2370.000323	56885.111702	59.169012
2369.252011	56703.112810	59.174017
2368.732159	56503.067710	59.179021
2368.001114	56321.895887	59.184026
2367.138727	56133.340818	59.189031
2366.655301	55933.327764	59.194036
2366.346254	55751.404690	59.199041
2365.628629	55554.942673	59.204045
2365.012018	55360.384581	59.209050
2363.932347	55171.114279	59.214055
2363.470904	54977.339480	59.219060
2362.634073	54779.600803	59.224065
2362.220782	54578.743237	59.229069
2361.348369	54386.001901	59.234074
2360.879356	54197.442302	59.239079
2360.409597	54003.742411	59.244084
2359.238061	53808.823604	59.249089
2358.941991	53608.534045	59.254093
2358.269115	53413.347361	59.259098
2357.542712	53229.012457	59.264103
2356.842306	53035.406892	59.269108
2356.020796	52842.759233	59.274113
2355.273709	52647.760242	59.279117
2354.509352	52454.471619	59.284122
2353.600285	52269.688122	59.289127
2353.475089	52082.130617	59.294132
2352.658519	51905.246652	59.299137
2351.894545	51715.797651	59.304141
2351.497396	51526.934779	59.309146
2350.882824	51333.805237	59.314151
2350.259184	51128.076887	59.319156
2349.281085	50941.308769	59.324161
2348.927021	50742.379463	59.329165
2348.318335	50552.272616	59.334170
2347.170263	50364.018763	59.339175
2346.744320	50166.126004	59.344180
2346.092100	49978.648641	59.349185
2345.163437	49789.163778	59.354189
2344.833716	49601.670856	59.359194
2343.729417	49416.140851	59.364199
2343.465783	49223.234614	59.369204
2342.399376	49051.186036	59.374209
2341.984910	48854.125348	59.379213
2341.332412	48672.131633	59.384218
2340.732999	48478.078205	59.389223
2340.365765	48285.983092	59.394228
2339.456027	48104.273239	59.399233
2338.625095	47911.676783	59.404237
2338.217228	47727.847602	59.409242
2337.413339	47541.957328	59.414247
2337.187820	47348.404210	59.419252
2336.174175	47152.950499	59.424257
2335.706914	46956.899850	59.429261
2334.820115	46761.816267	59.434266
2334.092126	46588.905953	59.439271
2333.555533	46391.300454	59.444276
2332.766084	46204.906348	59.449281
2332.238461	46017.552227	59.454285
2331.780241	45836.053450	59.459290
2330.937691	45636.063040	59.464295
2330.422797	45447.624880	59.469300
2329.470174	45263.284633	59.474305
2328.755010	45064.726012	59.479309
2328.591357	44879.698511	59.484314
2327.758227	44678.642130	59.489319
2327.287008	44484.887433	59.494324
2326.345729	44303.468467	59.499329
2325.949547	44103.896015	59.504333
2325.086055	43915.010934	59.509338
2324.561984	43715.437903	59.514343
2323.661803	43522.581052	59.519348
2322.927289	43337.723665	59.524353
2322.442275	43145.462981	59.529357
2321.612772	42954.033883	59.534362
2320.645769	42767.767812	59.539367
2320.232020	42579.170630	59.544372
2319.302931	42396.305380	59.549377
2318.850165	42216.038776	59.554381
2318.146480	42020.890500	59.559386
2317.344677	41835.199627	59.564391
2316.977268	41639.120033	59.569396
2315.913839	41459.176364	59.574401
2315.352379	41273.684262	59.579405
2314.851915	41087.330683	59.584410
2314.196167	40910.515609	59.589415
2313.412491	40714.335465	59.594420
2312.672744	40534.375426	59.599425
2312.089132	40352.375100	59.604429
2311.956179	40158.513937	59.609434
2311.331105	39977.890163	59.614439
2310.810257	39786.709708	59.619444
2309.227291	39601.448251	59.624449
2308.552232	39407.544013	59.629453
2308.302076	39227.614907	59.634458
2307.391846	39042.662284	59.639463
2307.005895	38856.551922	59.644468
2306.237848	38678.781720	59.649473
2305.610786	38483.664660	59.654477
2305.089596	38300.572824	59.659482
2304.167264	38118.947198	59.664487
2303.472721	37925.143531	59.669492
2302.796575	37751.124475	59.674497
2302.000542	37565.641805	59.679501
2301.466079	37385.758282	59.684506
2300.663610	37196.246554	59.689511
2300.229517	37009.762536	59.694516
2299.366399	36827.513802	59.699521
2298.641697	36654.999582	59.704525
2297.814867	36467.945224	59.709530
2297.229788	36302.715218	59.714535
2296.719574	36113.714610	59.719540
2295.885132	35936.336194	59.724545
2295.589350	35769.167196	59.729549
2294.953371	35580.134039	59.734554
2294.213586	35399.796868	59.739559
2293.424516	35216.396830	59.744564
2293.132887	35038.559300	59.749569
2292.333686	34851.712936	59.754573
2291.622432	34657.641244	59.759578
2290.786035	34485.791292	59.764583
2290.208123	34299.728366	59.769588
2289.444024	34132.455550	59.774593
2288.992678	33949.617978	59.779597
2288.386301	33767.829534	59.784602
2287.425075	33588.920384	59.789607
2286.991198	33402.824063	59.794612
2286.001190	33219.269188	59.799617
2285.494753	33037.171012	59.804621
2284.878987	32860.234604	59.809626
2283.884142	32685.917170	59.814631
2283.973587	32501.235021	59.819636
2283.008097	32322.575640	59.824641
2282.336386	32141.404783	59.829645
2281.771368	31959.073298	59.834650
2280.892501	31777.710138	59.839655
2280.605559	31592.206556	59.844660
2279.823277	31414.344898	59.849665
2279.055680	31224.898471	59.854669
2278.807689	31043.075132	59.859674
2277.638687	30863.779583	59.864679
2277.430324	30676.459813	59.869684
2276.271901	30497.455741	59.874689
2275.626943	30307.158213	59.879693
2275.052505	30123.483303	59.884698
2274.498925	29958.360256	59.889703
2273.703616	29770.213243	59.894708
2272.985270	29588.328899	59.899713
2272.396436	29403.294448	59.904718
2272.017164	29219.816744	59.909722
2271.023868	29047.713201	59.914727
2270.841776	28855.719087	59.919732
2269.962324	28665.345099	59.924737
2269.042828	28487.386816	59.929742
2268.812995	28309.438002	59.934746
2267.777619	28121.526568	59.939751
2266.903672	27939.773731	59.944756
2266.146080	27761.633391	59.949761
2265.677504	27582.496521	59.954766
2265.157820	27409.339866	59.959770
2264.170312	27227.932125	59.964775
2263.928433	27043.809403	59.969780
2263.187298	26863.331910	59.974785
2262.420873	26684.825646	59.979790
2261.726770	26503.932384	59.984794
2260.828711	26330.577924	59.989799
2260.631664	26148.743322	59.994804
2259.684423	25970.944989	59.999809
2258.840281	25786.123308	60.004814
2258.628485	25619.123710	60.009818
2257.253112	25445.698870	60.014823
2257.064358	25260.088970	60.019828
2256.330018	25086.309639	60.024833
2255.563585	24916.036826	60.029838
2255.013144	24732.523294	60.034842
2254.350227	24565.247626	60.039847
2253.671715	24389.015537	60.044852
2252.610399	24220.561203	60.049857
2252.295839	24041.942270	60.054862
2251.709398	23856.593311	60.059866
2250.802801	23686.268129	60.064871
2250.498307	23514.971881	60.069876
2249.724449	23345.355030	60.074881
2249.179994	23166.607811	60.079886
2248.259087	22988.539055	60.084890
2247.711745	22819.191952	60.089895
2247.169915	22637.109889	60.094900
2246.256765	22466.116497	60.099905
2245.662274	22294.895146	60.104910
2245.089115	22115.174047	60.109914
2244.091398	21946.365670	60.114919
2243.576137	21757.898899	60.119924
2242.784224	21594.403481	60.124929
2242.137830	21420.381629	60.129934
2241.675852	21259.618354	60.134938
2240.869811	21092.480797	60.139943
2240.430935	20914.897343	60.144948
2239.765400	20744.203819	60.149953
2238.985424	20568.303324	60.154958
2238.378556	20392.082823	60.159962
2237.177041	20226.954746	60.164967
2236.932942	20057.592996	60.169972
2236.447047	19881.088203	60.174977
2235.615180	19704.885418	60.179982
2235.198215	19542.392372	60.184986
2234.344697	19372.062497	60.189991
2233.904030	19189.089823	60.194996
2232.837855	19025.768752	60.200001
2232.314970	18859.593684	60.205006
2231.829995	18685.487611	60.210010
2231.034312	18510.286449	60.215015
2230.575951	18337.850930	60.220020
2229.704252	18166.922442	60.225025
2228.904412	17997.414106	60.230030
2228.468710	17825.127878	60.235034
2227.529073	17654.391031	60.240039
2227.240328	17477.520475	60.245044
2226.587387	17315.439263	60.250049
2225.671697	17139.147222	60.255054
2225.100708	16966.957457	60.260058
2224.331658	16805.990512	60.265063
2223.831292	16634.584580	60.270068
2222.589242	16468.439132	60.275073
2221.967526	16296.685178	60.280078
2221.718784	16130.037877	60.285082
2220.515456	15974.810044	60.290087
2220.452946	15799.824602	60.295092
2219.723752	15638.671640	60.300097
2218.991683	15471.856886	60.305102
2218.191363	15298.181087	60.310106
2217.732219	15134.539944	60.315111
2216.942435	14961.205463	60.320116
2216.473723	14800.790462	60.325121
2215.651113	14635.225356	60.330126
2214.950203	14467.608595	60.335130
2214.185185	14300.012312	60.340135
2213.911086	14127.957293	60.345140
2213.081547	13967.907726	60.350145
2212.499851	13800.137755	60.355150
2211.646476	13631.104877	60.360154
2210.953543	13470.236707	60.365159
2210.215909	13310.063011	60.370164
2209.532292	13140.730710	60.375169
2208.618611	12975.389320	60.380174
2208.109133	12809.131903	60.385178
2207.233072	12661.365983	60.390183
2206.748895	12493.122434	60.395188
2205.780299	12335.209082	60.400193
2204.903455	12184.894812	60.405198
2204.968556	12025.851508	60.410202
2203.948175	11871.866574	60.415207
2203.697895	11710.132394	60.420212
2202.964769	11544.453826	60.425217
2202.225482	11382.479136	60.430222
2201.511937	11230.376840	60.435226
2200.347207	11072.739589	60.440231
2200.040409	10915.834678	60.445236
2199.346340	10758.050672	60.450241
2198.414013	10599.782165	60.455246
2198.105815	10447.514123	60.460250
2197.225633	10296.082816	60.465255
2196.613592	10132.446647	60.470260
2196.272929	9993.666695	60.475265
2195.433564	9832.411879	60.480270
2194.673576	9669.925781	60.485274
2194.284576	9525.459920	60.490279
2193.410668	9363.313952	60.495284
2192.324846	9204.015310	60.500289
2191.867869	9056.685692	60.505294
2191.571087	8904.693318	60.510298
2190.685429	8749.106292	60.515303
2190.007383	8590.311983	60.520308
2189.294558	8436.609656	60.525313
2188.447912	8290.221543	60.530318
2187.926419	8128.535521	60.535322
2186.969166	7985.622670	60.540327
2186.598189	7829.552087	60.545332
2186.150903	7697.018602	60.550337
2185.187773	7542.986851	60.555342
2184.690212	7386.408452	60.560346
2183.865174	7235.521034	60.565351
2183.147020	7084.313673	60.570356
2182.705413	6935.054292	60.575361
2181.810069	6781.091025	60.580366
2181.256890	6633.636765	60.585370
2180.231300	6483.473879	60.590375
2179.504651	6332.017529	60.595380
2179.119560	6189.858560	60.600385
2178.235271	6044.242263	60.605390
2177.569146	5894.435713	60.610394
2177.032220	5759.344345	60.615399
2176.389073	5609.184422	60.620404
2175.341522	5475.447404	60.625409
2174.764917	5328.459393	60.630414
2174.109923	5193.136334	60.635418
2173.098359	5053.133712	60.640423
2172.519175	4910.696732	60.645428
2171.669470	4780.404367	60.650433
2171.214647	4641.844338	60.655438
2170.921865	4508.943579	60.660442
2169.974210	4378.004596	60.665447
2169.298565	4243.320532	60.670452
2168.174219	4112.037291	60.675457
2167.849529	3983.023678	60.680462
2167.261881	3850.946975	60.685466
2166.251084	3726.781436	60.690471
2165.519041	3594.280380	60.695476
2164.980259	3468.978175	60.700481
2163.988635	3346.481662	60.705486
2163.396173	3221.728745	60.710490
2162.778402	3109.021501	60.715495
2161.891315	2980.356679	60.720500
2161.188223	2871.671981	60.725505
2160.290516	2755.358017	60.730510
2159.710524	2635.538731	60.735514
2158.486847	2540.903589	60.740519
2157.915093	2425.525532	60.745524
2156.649497	2326.788862	60.750529
2155.775331	2241.869710	60.755534
2155.010494	2150.383448	60.760538
2154.125565	2057.989403	60.765543
2153.572199	1968.641774	60.770548
2152.469886	1895.000860	60.775553
2151.732178	1821.310355	60.780558
2150.726205	1742.630757	60.785562
2150.047318	1673.772851	60.790567
2149.559500	1604.753260	60.795572
2148.763631	1527.151030	60.800577
2148.089982	1462.897040	60.805582
2147.626986	1400.118457	60.810586
2146.828860	1332.842459	60.815591
2146.315404	1263.234754	60.820596
2145.615716	1193.988914	60.825601
2144.833599	1121.263152	60.830606
2144.401702	1058.977107	60.835610
2143.402144	1002.600933	60.840615
2142.547641	934.365008	60.845620
2141.861441	878.530222	60.850625
2140.871425	825.260105	60.855630
2140.308093	756.110627	60.860634
2139.263213	717.727831	60.865639
2139.102367	663.096625	60.870644
2138.392073	614.988820	60.875649
2137.833588	572.954017	60.880654
2137.291648	505.229581	60.885658
2136.271883	458.259567	60.890663
2135.382391	420.562576	60.895668
2134.712230	369.287236	60.900673
2133.720748	336.476555	60.905678
2133.066350	299.527944	60.910682
2131.830645	284.228112	60.915687
2130.902239	254.815579	60.920692
2130.097477	236.567765	60.925697
2129.142221	220.302521	60.930702
2128.538925	195.500214	60.935706
2127.860543	191.797803	60.940711
2126.933913	174.760058	60.945716
2126.677758	156.862135	60.950721
2126.030260	140.191744	60.955726
2125.897314	125.341609	60.960730
2124.537458	109.145421	60.965735
2124.322271	91.171690	60.970740
2123.858634	85.219532	60.975745
2123.137559	70.472235	60.980750
2122.610991	52.178939	60.985754
2121.696271	38.435415	60.990759
2120.816601	11.668174	60.995764
2119.833079	8.895775	61.000769
2119.182689	12.305988	61.005774
2118.909651	-15.051849	61.010778
2117.715958	-11.173010	61.015783
2117.211647	-12.442864	61.020788
2116.707496	-3.935335	61.025793
2115.979526	-20.077878	61.030798
2115.302343	-24.255096	61.035802
2114.311412	-25.138642	61.040807
2113.742636	-25.136665	61.045812
2112.967481	-26.112797	61.050817
2112.435720	-22.707221	61.055822
2112.018286	-25.979454	61.060826
2111.219340	-24.076940	61.065831
2110.457168	-32.181591	61.070836
2110.053849	-20.518726	61.075841
2109.219030	-21.848100	61.080846
2108.845447	-15.791452	61.085850
2107.799319	-11.235836	61.090855
2107.347715	-20.314682	61.095860
2106.702109	-8.417026	61.100865
2106.100744	-4.069968	61.105870
2105.629425	-13.320738	61.110874
2104.514764	1.822704	61.115879
2103.847306	-12.002577	61.120884
2103.341429	-5.819273	61.125889
2102.887782	7.001235	61.130894
2102.585005	-4.674116	61.135898
2102.141902	-6.575018	61.140903
2100.940013	-3.219223	61.145908
2100.020259	-6.623068	61.150913
2099.578546	-11.871374	61.155918
2098.905905	-8.417417	61.160922
2098.138935	5.242885	61.165927
2097.833975	-1.231166	61.170932
2097.276686	0.871135	61.175937
2096.619068	4.741406	61.180942
2095.667148	-0.593894	61.185946
2094.450902	10.196597	61.190951
2094.168253	9.367827	61.195956
2093.801645	10.548866	61.200961
2093.022933	6.982286	61.205966
2092.839585	13.459783	61.210970
2092.397541	14.381548	61.215975
2091.684951	8.924688	61.220980
2091.051208	14.219939	61.225985
2089.710460	7.752547	61.230990
2089.065621	6.083938	61.235994
2088.051672	13.426545	61.240999
2087.933859	12.011782	61.246004
2087.246489	11.570522	61.251009
2086.260947	15.328826	61.256014
2086.102647	14.540251	61.261018
2085.453200	14.242788	61.266023
2085.157087	13.810406	61.271028
2084.996159	8.240776	61.276033
2083.950882	27.412732	61.281038
2082.786227	9.006290	61.286042
2081.440128	20.776216	61.291047
2081.325974	24.467211	61.296052
2080.824727	18.743417	61.301057
2079.827049	22.177211	61.306062
2079.209329	21.423692	61.311066
2079.083567	25.178033	61.316071
2078.422443	20.086756	61.321076
2077.731728	34.796310	61.326081
2076.966914	24.698725	61.331086
2076.362206	13.012931	61.336090
2075.440791	25.502394	61.341095
2074.560440	30.240680	61.346100
2074.326354	23.492016	61.351105
2073.896250	40.833243	61.356110
2073.690227	12.848916	61.361114
2072.480929	15.888925	61.366119
2071.521705	17.476256	61.371124
2071.226148	21.251233	61.376129
2070.512997	31.824711	61.381134
2070.260717	28.242405	61.386138
2068.995260	31.915825	61.391143
2068.179073	27.748048	61.396148
2067.610483	27.112895	61.401153
2067.035013	28.767067	61.406158
2066.149064	24.537821	61.411162
2065.008229	40.984130	61.416167
2065.169686	31.430281	61.421172
2064.763370	38.430467	61.426177
2063.799544	35.175550	61.431182
2063.798383	35.423362	61.436186
2063.004742	35.317527	61.441191
2061.890992	27.033681	61.446196
2060.667197	37.792284	61.451201
2060.442783	37.077281	61.456206
2060.059710	28.281653	61.461210
2059.603837	45.298957	61.466215
2058.781688	38.976359	61.471220
2058.233897	36.298839	61.476225
2057.285930	38.496269	61.481230
2056.679661	33.680149	61.486234
2056.053571	40.123838	61.491239
2055.534772	39.846650	61.496244
2054.991515	32.194538	61.501249
2053.979712	43.526652	61.506254
2053.822166	37.265749	61.511258
2052.448578	39.141205	61.516263
2051.743945	46.958317	61.521268
2051.137232	44.102485	61.526273
2050.354744	54.111379	61.531278
2049.936179	47.188550	61.536282
2049.335240	47.485814	61.541287
2048.355722	44.378475	61.546292
2047.815596	50.172994	61.551297
2047.146550	49.788761	61.556302
2047.107349	46.969025	61.561306
2046.278773	52.995408	61.566311
2045.539929	48.233444	61.571316
2045.013981	39.444716	61.576321
2043.902617	52.787552	61.581326
2043.572693	50.517019	61.586330
2042.817138	50.442993	61.591335
2042.317322	49.011581	61.596340
2042.013528	44.704142	61.601345
2040.999643	47.434029	61.606350
2040.422698	40.217786	61.611354
2039.484820	52.332988	61.616359
2039.200651	48.337835	61.621364
2038.409787	48.605316	61.626369
2037.255535	56.291935	61.631374
2037.245803	46.374148	61.636378
2036.355531	58.980136	61.641383
2035.653577	51.589756	61.646388
2035.186705	50.966852	61.651393
2034.355751	54.440444	61.656398
2033.861545	57.691852	61.661402
2033.113827	62.090555	61.666407
2032.181956	61.421597	61.671412
2031.710016	58.481297	61.676417
2031.105226	57.216362	61.681422
2030.519623	52.540471	61.686426
2029.149655	65.531690	61.691431
2029.042529	59.259624	61.696436
2028.657052	52.356779	61.701441
2028.202811	58.284334	61.706446
2026.904274	53.183832	61.711450
2025.675538	61.230798	61.716455
2025.526823	59.158596	61.721460
2025.633411	61.969292	61.726465
2024.331395	62.174394	61.731470
2023.990490	50.954516	61.736474
2022.882358	47.124830	61.741479
2022.247594	53.787533	61.746484
2021.794310	51.413575	61.751489
2020.726353	62.448685	61.756494
2020.673052	49.718123	61.761498
2019.818051	58.465891	61.766503
2019.246297	62.283140	61.771508
2018.813801	52.202205	61.776513
2017.815204	58.914771	61.781518
2017.403806	57.545026	61.786522
2016.880169	54.168220	61.791527
2016.144197	59.672120	61.796532
2015.986176	58.574409	61.801537
2014.348600	56.777934	61.806542
2013.605287	50.274096	61.811546
2013.166362	67.477976	61.816551
2012.659560	56.762260	61.821556
2011.923860	54.376354	61.826561
2010.833970	58.709516	61.831566
2011.030576	56.503658	61.836570
2010.097552	58.419605	61.841575
2009.204352	60.067448	61.846580
2008.588603	56.779381	61.851585
2007.714899	58.307432	61.856590
2007.731703	48.229312	61.861594
2007.188525	51.365490	61.866599
2006.479924	61.143466	61.871604
2006.143003	57.090453	61.876609
2004.403591	58.353770	61.881614
2003.576143	58.029383	61.886618
2002.745077	66.948408	61.891623
2002.724420	63.578506	61.896628
2002.487755	62.791333	61.901633
2001.590340	69.019477	61.906638
2000.970442	58.302790	61.911642
2000.186530	67.744206	61.916647
1999.502895	63.517556	61.921652
1998.876856	57.114960	61.926657
1998.342858	68.912184	61.931662
1997.963199	53.317536	61.936666
1996.557336	58.593439	61.941671
1995.531963	57.308532	61.946676
1995.629754	63.405526	61.951681
1994.632783	64.139411	61.956686
1994.080327	50.127122	61.961690
1993.404624	63.329868	61.966695
1992.724986	58.725683	61.971700
1992.219168	57.889764	61.976705
1991.447988	65.627570	61.981710
1991.236460	61.188791	61.986714
1990.434658	68.412624	61.991719
1989.888684	61.492678	61.996724
1989.609471	55.765190	62.001729
1988.242545	67.850742	62.006734
1987.357697	65.803916	62.011738
1986.464573	57.538692	62.016743
1985.918668	61.798137	62.021748
1985.148190	59.138628	62.026753
1984.757745	70.574013	62.031758
1984.451938	58.864427	62.036762
1983.736993	58.402337	62.041767
1983.269334	67.979646	62.046772
1982.865286	63.752781	62.051777
1982.372062	63.277577	62.056782
1981.250078	62.148363	62.061786
1980.356290	69.957676	62.066791
1979.609337	64.227155	62.071796
1978.892780	55.609046	62.076801
1978.164494	64.767236	62.081806
1977.782052	65.980770	62.086810
1977.229290	61.287062	62.091815
1976.657364	58.110324	62.096820
1975.914430	61.956328	62.101825
1974.571378	66.834331	62.106830
1974.025624	58.420930	62.111834
1973.706028	64.511632	62.116839
1973.180351	64.465795	62.121844
1972.958305	56.612893	62.126849
1971.944332	75.836736	62.131854
1971.298223	62.492191	62.136858
1970.740696	71.311035	62.141863
1970.216829	64.158918	62.146868
1969.086695	64.261068	62.151873
1968.214725	68.523387	62.156878
1967.443355	58.600334	62.161882
1967.102294	61.583009	62.166887
1966.553305	61.867314	62.171892
1966.152183	59.530820	62.176897
1965.593488	62.016589	62.181902
1965.017179	63.674073	62.186906
1963.727266	66.373685	62.191911
1962.813781	63.533449	62.196916
1962.519268	55.423962	62.201921
1961.760389	69.152445	62.206926
1961.419491	73.158575	62.211930
1961.076240	68.847943	62.216935
1960.323854	65.868591	62.221940
1959.155748	69.206483	62.226945
1957.976057	80.104812	62.231950
1957.549348	64.661141	62.236954
1957.061162	72.317765	62.241959
1956.640212	62.537793	62.246964
1956.205735	60.121436	62.251969
1955.402532	61.627274	62.256974
1954.906624	67.861086	62.261978
1954.472255	62.785879	62.266983
1953.140248	67.488668	62.271988
1952.337914	66.452234	62.276993
1951.586404	67.844209	62.281998
1951.431707	54.937354	62.287002
1950.572716	58.456422	62.292007
1950.060902	68.176366	62.297012
1949.684736	56.239831	62.302017
1948.824938	72.255226	62.307022
1948.805547	66.980101	62.312026
1947.669553	67.455364	62.317031
1946.809816	67.134543	62.322036
1946.287996	60.765882	62.327041
1945.292835	71.776849	62.332046
1944.886201	55.366453	62.337050
1944.449134	72.562157	62.342055
1942.964415	69.891455	62.347060
1942.387945	66.299114	62.352065
1941.584057	72.083484	62.357070
1941.704325	67.205674	62.362074
1940.926923	76.642920	62.367079
1940.447684	75.829601	62.372084
1940.175266	70.583601	62.377089
1938.927003	69.917590	62.382094
1938.040420	60.321929	62.387098
1937.241512	66.102354	62.392103
1936.338581	66.283573	62.397108
1935.943696	64.630513	62.402113
1935.328671	66.967531	62.407118
1934.837686	63.342699	62.412122
1934.462106	69.339786	62.417127
1933.918589	64.020127	62.422132
1933.636067	66.597685	62.427137
1932.479182	65.762625	62.432142
1931.678060	64.938902	62.437146
1930.841755	66.151947	62.442151
1930.022839	69.164751	62.447156
1930.186306	63.228221	62.452161
1928.744068	66.447210	62.457166
1928.308898	59.579081	62.462170
1927.259669	61.399958	62.467175
1926.691813	68.611900	62.472180
1926.356468	64.328406	62.477185
1925.615584	67.330400	62.482190
1925.371231	63.999167	62.487194
1924.562736	63.775879	62.492199
1923.710885	67.344287	62.497204
1923.109288	68.799206	62.502209
1922.076599	78.756393	62.507214
1921.714812	65.779905	62.512218
1920.993215	71.483405	62.517223
1920.366524	75.334628	62.522228
1920.071544	63.061921	62.527233
1918.805738	66.103091	62.532238
1918.134203	67.258443	62.537242
1917.296356	62.797671	62.542247
1916.831802	69.863901	62.547252
1916.405348	65.476597	62.552257
1915.841148	74.089920	62.557262
1915.667104	64.922065	62.562266
1915.181434	70.853050	62.567271
1913.777406	69.549436	62.572276
1913.036261	67.416744	62.577281
1912.305022	73.413523	62.582286
1912.138561	69.019638	62.587290
1911.341460	66.023746	62.592295
1909.877129	74.863549	62.597300
1909.501608	66.487796	62.602305
1908.724896	72.635302	62.607310
1908.209605	62.834048	62.612314
1907.857371	67.949039	62.617319
1907.350786	66.843590	62.622324
1906.988796	59.859767	62.627329
1906.118208	71.341415	62.632334
1905.585001	63.690888	62.637338
1904.802956	67.946834	62.642343
1903.787935	71.336142	62.647348
1903.424556	60.842124	62.652353
1902.634290	70.070096	62.657358
1901.360480	64.210348	62.662362
1900.826384	64.184786	62.667367
1900.170081	64.268515	62.672372
1899.594945	55.161191	62.677377
1898.824518	71.247563	62.682382
1898.643325	62.314244	62.687386
1898.539027	60.662369	62.692391
1897.735748	57.136013	62.697396
1897.282688	56.884691	62.702401
1895.910172	63.112591	62.707406
1895.240037	53.555134	62.712410
1894.800038	64.783911	62.717415
1894.260259	64.653594	62.722420
1893.686212	52.056188	62.727425
1892.094109	70.963377	62.732430
1891.704864	64.696688	62.737434
1890.937510	59.308495	62.742439
1890.720264	66.258190	62.747444
1890.302800	64.619762	62.752449
1889.712566	68.444700	62.757454
1889.328256	57.835735	62.762458
1888.354198	71.839675	62.767463
1887.413640	66.977312	62.772468
1887.201391	71.365160	62.777473
1885.708439	73.925150	62.782478
1884.720315	66.143417	62.787482
1884.164451	64.812401	62.792487
1884.156215	63.279321	62.797492
1883.694611	64.786142	62.802497
1882.917669	68.989242	62.807502
1882.353929	63.347944	62.812506
1881.799875	73.039909	62.817511
1880.825037	62.671358	62.822516
1879.722932	66.986008	62.827521
1878.953526	71.055444	62.832526
1878.758834	67.612250	62.837530
1878.286406	68.666613	62.842535
1877.722868	76.499219	62.847540
1877.284294	66.271040	62.852545
1875.923962	69.950155	62.857550
1875.264730	60.889303	62.862554
1874.760380	72.197691	62.867559
1874.181830	60.290151	62.872564
1874.122507	64.279968	62.877569
1873.083004	72.582391	62.882574
1872.022095	67.073646	62.887578
1871.019659	64.241259	62.892583
1870.604700	62.643439	62.897588
1870.622268	67.020030	62.902593
1869.626355	73.695950	62.907598
1869.441643	70.777891	62.912602
1868.184042	70.178054	62.917607
1867.290388	74.453308	62.922612
1866.786583	73.725907	62.927617
1866.205666	75.453532	62.932622
1865.996747	63.591389	62.937626
1865.347180	73.708541	62.942631
1864.097246	74.045807	62.947636
1863.732573	58.789449	62.952641
1862.659027	73.157709	62.957646
1862.496912	72.891740	62.962650
1862.050148	70.767519	62.967655
1861.335741	73.524045	62.972660
1860.344275	66.682750	62.977665
1859.397328	76.151661	62.982670
1859.264653	65.660446	62.987674
1858.659118	65.359221	62.992679
1857.389672	65.970832	62.997684
1856.778434	59.947564	63.002689
1856.055024	75.133896	63.007694
1855.659249	68.909252	63.012698
1855.234264	57.568716	63.017703
1854.709980	68.558559	63.022708
1854.340196	62.957439	63.027713
1852.626206	77.192416	63.032718
1852.075783	67.802045	63.037722
1851.522104	73.348008	63.042727
1851.275313	71.401781	63.047732
1850.632462	69.567325	63.052737
1849.927802	67.014107	63.057742
1849.087230	64.778946	63.062746
1848.512733	64.386060	63.067751
1847.524579	73.284331	63.072756
1847.533201	56.213504	63.077761
1846.853352	69.213495	63.082766
1845.626431	66.170748	63.087770
1844.609167	69.833255	63.092775
1844.156702	62.056382	63.097780
1843.984058	63.400631	63.102785
1843.336968	74.911466	63.107790
1842.997670	71.286224	63.112794
1842.209287	68.779418	63.117799
1841.031230	69.253521	63.122804
1840.666023	69.895038	63.127809
1839.986953	70.513847	63.132814
1839.284746	63.699177	63.137818
1838.187672	70.241351	63.142823
1837.414969	61.513930	63.147828
1837.304108	64.248749	63.152833
1836.437444	71.036624	63.157838
1836.112696	66.011848	63.162842
1835.781527	70.716633	63.167847
1834.573705	81.373458	63.172852
1833.688630	63.588212	63.177857
1833.071320	70.664512	63.182862
1832.536497	73.996524	63.187866
1832.504392	77.390645	63.192871
1831.547441	74.793909	63.197876
1830.605828	59.589742	63.202881
1829.788443	64.884255	63.207886
1829.566945	65.290059	63.212890
1829.057783	71.626920	63.217895
1827.911603	74.579750	63.222900
1827.313196	71.798348	63.227905
1826.734101	74.129684	63.232910
1826.260790	71.777866	63.237914
1825.580350	77.698788	63.242919
1824.296571	66.098789	63.247924
1823.516725	68.307454	63.252929
1822.984825	72.887991	63.257934
1822.626880	64.470043	63.262938
1822.226359	73.073157	63.267943
1821.511263	74.670704	63.272948
1821.563395	57.909949	63.277953
1820.280269	71.617615	63.282958
1819.229386	69.625599	63.287962
1818.845815	65.058036	63.292967
1818.313985	65.808018	63.297972
1817.381253	60.398800	63.302977
1816.234137	70.531881	63.307982
1815.874711	70.631571	63.312986
1815.553227	60.733339	63.317991
1814.701842	76.432022	63.322996
1814.468554	67.868120	63.328001
1813.600425	68.958518	63.333006
1812.828520	64.845293	63.338010
1812.106457	68.946653	63.343015
1811.497879	71.678501	63.348020
1811.322037	62.305940	63.353025
1810.035978	74.971679	63.358030
1809.145545	68.658429	63.363034
1808.388706	68.620946	63.368039
1807.855541	72.077281	63.373044
1807.637136	62.847101	63.378049
1806.990951	73.230238	63.383054
1806.947329	69.089681	63.388058
1805.933612	65.912171	63.393063
1804.948276	75.349343	63.398068
1804.579531	67.745270	63.403073
1803.781168	69.430162	63.408078
1802.753331	70.186367	63.413082
1802.081529	68.809122	63.418087
1801.680017	70.877290	63.423092
1801.311300	67.616284	63.428097
1800.060263	72.333096	63.433102
1799.407154	66.392187	63.438106
1798.350082	72.131637	63.443111
1797.866835	71.232247	63.448116
1798.037649	66.439455	63.453121
1797.436966	69.792968	63.458126
1796.724693	62.300223	63.463130
1795.654601	65.930132	63.468135
1794.818423	70.633109	63.473140
1794.706198	60.488757	63.478145
1793.900997	65.120579	63.483150
1792.810406	70.478988	63.488154
1792.028220	67.744126	63.493159
1790.986264	69.403046	63.498164
1791.005894	65.015897	63.503169
1790.483838	64.855978	63.508174
1790.082707	65.145226	63.513178
1789.635992	66.409994	63.518183
1788.217796	67.794336	63.523188
1787.658026	70.441165	63.528193
1787.171923	76.421123	63.533198
1786.516474	68.491986	63.538202
1785.562292	75.904075	63.543207
1784.626220	71.503103	63.548212
1784.502877	61.973972	63.553217
1783.744255	70.455752	63.558222
1783.359945	67.775986	63.563226
1782.866573	71.672298	63.568231
1781.587609	72.093063	63.573236
1781.050983	58.453657	63.578241
1780.241032	63.524644	63.583246
1779.840888	63.611880	63.588250
1779.698703	63.897858	63.593255
1778.549499	63.900613	63.598260
1777.743045	61.820913	63.603265
1777.088938	57.545489	63.608270
1776.780036	69.318022	63.613274
1776.399838	67.932325	63.618279
1775.067237	68.501964	63.623284
1774.418804	66.892349	63.628289
1773.779364	67.276217	63.633294
1773.597050	60.287544	63.638298
1772.560564	71.349272	63.643303
1771.382238	68.713597	63.648308
1771.225821	68.714820	63.653313
1770.678777	70.918071	63.658318
1770.124008	71.088213	63.663322
1769.989834	62.999031	63.668327
1768.415960	72.562791	63.673332
1768.247791	65.388937	63.678337
1767.463678	67.022689	63.683342
1766.343319	67.191186	63.688346
1765.492844	68.203099	63.693351
1764.794800	67.497103	63.698356
1764.547022	56.653595	63.703361
1764.268718	63.953619	63.708366
1763.739267	72.020529	63.713370
1762.540557	60.403909	63.718375
1761.612247	66.954002	63.723380
1761.376071	64.772703	63.728385
1760.521549	63.216323	63.733390
1760.101839	62.425125	63.738394
1759.896691	66.324554	63.743399
1758.511356	74.573121	63.748404
1758.025817	61.733034	63.753409
1757.484920	75.934729	63.758414
1756.876337	75.897371	63.763418
1756.198949	73.313040	63.768423
1754.704972	79.465680	63.773428
1754.557453	71.008018	63.778433
1754.039559	72.859702	63.783438
1753.770763	72.028768	63.788442
1753.235902	62.118703	63.793447
1751.878937	70.574084	63.798452
1751.295797	65.748059	63.803457
1750.537918	75.863505	63.808462
1750.171929	83.655297	63.813466
1749.989152	66.171735	63.818471
1748.799374	66.802286	63.823476
1748.124187	57.193641	63.828481
1747.294397	74.491137	63.833486
1746.936348	63.395472	63.838490
1746.189038	63.775976	63.843495
1745.081405	64.896546	63.848500
1744.594352	64.412523	63.853505
1744.166944	71.608494	63.858510
1743.572884	67.139031	63.863514
1743.296905	71.601662	63.868519
1742.202275	72.414230	63.873524
1741.335164	64.498225	63.878529
1740.440529	69.565326	63.883534
1740.326272	59.444960	63.888538
1739.993315	66.564426	63.893543
1738.801093	71.022756	63.898548
1738.019081	66.592606	63.903553
1737.490738	67.504481	63.908558
1736.768234	69.092186	63.913562
1736.446757	66.948093	63.918567
1735.723751	68.679386	63.923572
1734.973324	63.255441	63.928577
1734.426461	69.763886	63.933582
1733.749049	73.620047	63.938586
1733.334316	65.405110	63.943591
1732.097201	69.898959	63.948596
1731.412682	62.684112	63.953601
1730.799991	68.412934	63.958606
1730.610394	68.171839	63.963610
1729.935104	63.843019	63.968615
1728.613100	70.236446	63.973620
1728.045996	69.358273	63.978625
1727.422475	62.168434	63.983630
1727.308917	62.869350	63.988634
1726.830143	61.172877	63.993639
1725.578461	72.834942	63.998644
1725.021605	68.935180	64.003649
1724.257170	67.959034	64.008654
1723.877446	60.445039	64.013658
1723.139159	59.199805	64.018663
1722.119023	63.517264	64.023668
1721.354560	63.231851	64.028673
1720.797983	70.796856	64.033678
1720.290495	63.309460	64.038682
1720.045482	65.877924	64.043687
1719.469542	72.193865	64.048692
1718.881996	64.876885	64.053697
1717.813224	63.006030	64.058702
1717.314118	65.936559	64.063706
1716.148429	66.691036	64.068711
1715.298956	67.881007	64.073716
1715.063610	67.678720	64.078721
1714.373570	70.199591	64.083726
1713.760538	65.315245	64.088730
1713.721799	60.065288	64.093735
1712.647138	67.174820	64.098740
1712.145405	67.245085	64.103745
1711.124313	72.504174	64.108750
1710.472165	75.083686	64.113754
1709.329960	65.938744	64.118759
1708.280133	67.938001	64.123764
1708.281461	65.044030	64.128769
1707.486027	69.962916	64.133774
1707.391603	69.793442	64.138778
1707.256961	71.246784	64.143783
1706.431156	75.987564	64.148788
1705.484520	75.259565	64.153793
1704.751855	77.500196	64.158798
1703.970093	80.464585	64.163802
1702.782833	73.482562	64.168807
1702.093523	67.493815	64.173812
1701.815535	70.124291	64.178817
1701.051360	80.803739	64.183822
1700.716986	68.352830	64.188826
1700.681114	68.754394	64.193831
1699.129884	69.494418	64.198836
1698.671533	62.592178	64.203841
1698.008573	71.025664	64.208846
1697.505142	71.872086	64.213850
1696.311675	69.382359	64.218855
1695.717015	71.115355	64.223860
1695.255520	67.120028	64.228865
1694.439818	69.143607	64.233870
1694.265804	75.953973	64.238874
1693.744849	64.666570	64.243879
1692.607234	66.247678	64.248884
1692.262107	64.501598	64.253889
1691.512512	65.027565	64.258894
1690.693738	64.870639	64.263898
1689.577997	63.313195	64.268903
1688.735462	77.947594	64.273908
1688.842042	67.905698	64.278913
1688.016397	75.685341	64.283918
1687.551224	66.688348	64.288922
1687.161692	67.939318	64.293927
1686.092192	73.146177	64.298932
1685.467403	69.403878	64.303937
1684.707060	78.150891	64.308942
1684.042024	72.347533	64.313946
1683.293298	70.372238	64.318951
1682.459900	75.588908	64.323956
1682.215591	60.956903	64.328961
1681.765624	69.525298	64.333966
1681.193680	63.773392	64.338970
1680.141133	65.833018	64.343975
1679.313010	71.200241	64.348980
1679.041215	75.124454	64.353985
1678.412335	81.996035	64.358990
1677.096007	72.386739	64.363994
1676.395357	65.664920	64.368999
1675.584626	82.166175	64.374004
1675.512029	70.179908	64.379009
1675.136844	73.462934	64.384014
1674.819241	74.396542	64.389018
1673.798328	76.036395	64.394023
1672.743341	73.136740	64.399028
1672.488269	74.837878	64.404033
1671.281065	74.124472	64.409038
1670.133082	71.085043	64.414042
1669.778393	68.302818	64.419047
1669.163239	71.915707	64.424052
1668.863735	71.662112	64.429057
1668.607530	72.593854	64.434062
1668.390280	71.929789	64.439066
1667.226985	77.145247	64.444071
1666.489131	81.924110	64.449076
1665.874419	70.531751	64.454081
1664.580942	72.662771	64.459086
1663.743124	64.142885	64.464090
1663.613157	73.553037	64.469095
1662.945344	77.098596	64.474100
1662.810132	70.737985	64.479105
1661.613943	69.062440	64.484110
1660.924149	67.852099	64.489114
1660.367719	69.929124	64.494119
1659.521239	73.944625	64.499124
1659.189855	72.716777	64.504129
1658.295449	71.964729	64.509134
1657.448897	63.001519	64.514138
1657.252759	67.199151	64.519143
1656.271447	73.935897	64.524148
1656.146275	64.856519	64.529153
1654.923964	75.381658	64.534158
1654.295938	81.117665	64.539162
1654.084632	70.855021	64.544167
1653.032411	74.592537	64.549172
1652.218625	74.699767	64.554177
1651.396763	80.807197	64.559182
1650.875461	77.147817	64.564186
1650.658514	72.320421	64.569191
1649.840818	78.994910	64.574196
1649.205224	60.656034	64.579201
1648.195205	76.021962	64.584206
1647.412617	73.209938	64.589210
1647.615580	61.881675	64.594215
1646.682512	78.626297	64.599220
1645.725952	57.954773	64.604225
1644.993532	55.292485	64.609230
1644.443468	60.920692	64.614234
1644.174011	65.771810	64.619239
1642.884304	67.478028	64.624244
1642.198069	64.754783	64.629249
1641.595446	70.778498	64.634254
1640.836360	68.609314	64.639258
1640.946725	60.270776	64.644263
1640.259354	64.275986	64.649268
1639.201964	64.141212	64.654273
1638.422901	61.679516	64.659278
1637.615391	68.003079	64.664282
1637.366527	65.385404	64.669287
1636.157569	72.144126	64.674292
1635.496900	63.184513	64.679297
1635.153602	70.731418	64.684302
1634.593800	74.945821	64.689306
1634.182230	66.121684	64.694311
1633.576087	70.040663	64.699316
1632.931796	63.742004	64.704321
1631.772905	66.460381	64.709326
1631.541364	71.933125	64.714330
1630.649479	66.996903	64.719335
1629.421395	67.248804	64.724340
1629.032703	68.714121	64.729345
1628.439312	64.575754	64.734350
1627.960078	62.824968	64.739354
1627.698471	63.939714	64.744359
1626.411756	66.951221	64.749364
1626.136157	62.438298	64.754369
1625.484389	67.519678	64.759374
1624.608816	67.876437	64.764378
1624.402174	61.848101	64.769383
1623.063376	64.572195	64.774388
1622.549263	58.911259	64.779393
1621.830084	61.324814	64.784398
1621.633245	66.657209	64.789402
1620.911587	62.224610	64.794407
1619.400617	64.415434	64.799412
1619.444449	56.400503	64.804417
1618.980777	67.931897	64.809422
1618.147180	63.403538	64.814426
1617.267246	64.196243	64.819431
1616.612603	66.206085	64.824436
1616.341601	62.867299	64.829441
1615.739035	60.231699	64.834446
1614.902044	62.121483	64.839450
1614.355981	54.998229	64.844455
1613.366679	65.547861	64.849460
1612.911171	59.123024	64.854465
1611.704904	63.985770	64.859470
1610.817784	67.615855	64.864474
1610.761308	61.208840	64.869479
1610.250714	69.002314	64.874484
1609.849757	54.810759	64.879489
1609.310437	65.577497	64.884494
1607.982108	61.385578	64.889498
1607.332003	63.447531	64.894503
1606.610795	64.058901	64.899508
1606.702180	64.474942	64.904513
1605.569306	69.896119	64.909518
1604.512544	76.682716	64.914522
1604.046287	70.988158	64.919527
1603.727583	65.715663	64.924532
1603.039096	68.561964	64.929537
1601.815830	71.853571	64.934542
1601.366215	71.529213	64.939546
1601.350321	66.030409	64.944551
1600.441475	76.471863	64.949556
1599.208685	67.400509	64.954561
1598.802135	71.712787	64.959566
1598.095777	71.101202	64.964570
1598.098108	62.320920	64.969575
1597.034744	72.331167	64.974580
1596.299033	66.919913	64.979585
1595.571332	67.469238	64.984590
1595.092885	68.436293	64.989594
1594.534783	65.943449	64.994599
1593.047089	66.976225	64.999604
1592.798737	70.561606	65.004609
1592.010834	66.902808	65.009614
1591.841535	62.386406	65.014618
1591.396338	59.158092	65.019623
1589.898483	72.515952	65.024628
1589.250880	67.790890	65.029633
1588.978059	68.534461	65.034638
1588.258899	65.557835	65.039642
1588.256576	60.710545	65.044647
1586.804932	68.356266	65.049652
1586.185332	61.772995	65.054657
1585.649468	65.564119	65.059662
1585.321057	70.071359	65.064666
1584.890313	66.809208	65.069671
1583.570504	67.518841	65.074676
1583.056381	73.940892	65.079681
1582.402255	71.037515	65.084686
1581.729822	67.803512	65.089690
1581.073632	54.935407	65.094695
1580.304372	68.665592	65.099700
1579.753810	74.174041	65.104705
1579.229192	72.189982	65.109710
1578.168007	70.375541	65.114714
1577.533800	66.642654	65.119719
1576.560741	71.676529	65.124724
1576.236080	69.285376	65.129729
1575.584926	69.410947	65.134734
1575.364240	82.898655	65.139738
1575.381552	66.391841	65.144743
1574.036982	74.808271	65.149748
1573.566677	59.180055	65.154753
1572.415215	70.080328	65.159758
1571.346166	77.760683	65.164762
1571.170948	67.278640	65.169767
1570.410441	80.926232	65.174772
1570.048482	70.820797	65.179777
1569.275811	69.846006	65.184782
1568.180390	67.619893	65.189786
1567.765833	65.484306	65.194791
1567.060354	70.633370	65.199796
1566.885514	70.191242	65.204801
1566.783095	74.789527	65.209806
1565.429169	70.681335	65.214810
1564.971200	60.732304	65.219815
1563.440970	71.164466	65.224820
1562.662709	71.229808	65.229825
1562.218430	69.866943	65.234830
1561.657538	71.171965	65.239834
1561.458609	67.942374	65.244839
1560.829226	68.864029	65.249844
1560.435461	61.454807	65.254849
1559.204688	70.432708	65.259854
1558.386378	73.831886	65.264858
1558.249794	69.704538	65.269863
1557.289671	69.056011	65.274868
1556.354015	65.027240	65.279873
1555.806790	69.984000	65.284878
1555.130763	63.652561	65.289882
1555.128041	60.659888	65.294887
1554.170954	66.670547	65.299892
1553.435024	61.301136	65.304897
1552.580868	70.414747	65.309902
1551.924908	63.638561	65.314906
1551.436942	64.903612	65.319911
1550.199065	64.802282	65.324916
1549.918584	61.673964	65.329921
1549.497260	64.257836	65.334926
1548.803882	71.787828	65.339930
1548.767782	63.238380	65.344935
1547.474079	70.422197	65.349940
1547.078419	67.187596	65.354945
1546.586196	65.572147	65.359950
1545.049973	71.659060	65.364954
1544.702739	67.405908	65.369959
1543.972720	70.617590	65.374964
1543.396814	66.714595	65.379969
1542.463204	71.571897	65.384974
1541.346609	71.178480	65.389978
1540.965776	66.085395	65.394983
1540.254512	67.100492	65.399988
1539.881938	63.841724	65.404993
1539.631643	64.897120	65.409998
1539.121191	67.865751	65.415002
1538.900649	62.507495	65.420007
1537.846526	71.025238	65.425012
1537.331509	66.576390	65.430017
1536.301410	71.138357	65.435022
1534.905398	73.236843	65.440026
1534.673619	66.207176	65.445031
1534.057087	70.908439	65.450036
1533.725550	69.727943	65.455041
1532.900886	66.135722	65.460046
1531.654145	80.332102	65.465050
1531.510690	62.958263	65.470055
1530.495538	71.127607	65.475060
1530.571777	66.980639	65.480065
1530.124990	58.345060	65.485070
1528.530560	68.082519	65.490074
1528.286941	65.288978	65.495079
1527.439864	70.760180	65.500084
1527.094126	65.552709	65.505089
1526.076988	73.660869	65.510094
1525.507758	69.730008	65.515098
1524.924315	66.135731	65.520103
1523.955362	71.720920	65.525108
1524.060006	72.546448	65.530113
1523.230146	71.300053	65.535118
1522.348849	61.320527	65.540122
1522.194483	64.234156	65.545127
1521.278302	71.577199	65.550132
1520.314857	73.220594	65.555137
1519.677516	70.883865	65.560142
1519.049147	73.664651	65.565146
1518.600985	62.800991	65.570151
1517.215212	67.107234	65.575156
1516.813727	64.095922	65.580161
1516.443698	70.167856	65.585166
1515.770517	67.289605	65.590170
1515.408549	61.775625	65.595175
1514.063858	64.362720	65.600180
1513.499279	59.693091	65.605185
1513.178593	60.225072	65.610190
1512.402552	64.822370	65.615194
1511.879113	57.063173	65.620199
1510.991432	73.073605	65.625204
1510.601394	60.227887	65.630209
1510.033029	63.808138	65.635214
1508.812366	68.096034	65.640218
1508.021450	65.338999	65.645223
1507.500149	68.703610	65.650228
1507.094126	64.505540	65.655233
1506.637275	69.359635	65.660238
1505.785785	68.616592	65.665242
1504.890410	60.180039	65.670247
1503.971262	64.702306	65.675252
1503.616484	60.809918	65.680257
1503.520501	59.464260	65.685262
1502.805810	73.436531	65.690266
1502.023920	60.170522	65.695271
1501.616265	62.832656	65.700276
1500.918719	62.686489	65.705281
1499.439550	65.364350	65.710286
1498.733127	66.837595	65.715290
1498.933787	59.316583	65.720295
1497.807625	63.958483	65.725300
1497.489100	60.646978	65.730305
1496.412712	62.833468	65.735310
1495.475354	64.480610	65.740314
1495.151085	68.632374	65.745319
1494.470681	63.135883	65.750324
1494.241535	62.191443	65.755329
1492.990700	63.770126	65.760334
1492.328764	65.841870	65.765338
1492.306137	54.981566	65.770343
1491.255952	66.152782	65.775348
1490.424314	61.031997	65.780353
1489.914118	63.253098	65.785358
1488.799973	68.497083	65.790362
1488.854265	62.035417	65.795367
1488.155953	63.144666	65.800372
1487.680377	63.420558	65.805377
1486.740871	62.798745	65.810382
1485.894987	63.715396	65.815386
1485.488710	64.981670	65.820391
1484.215282	62.881657	65.825396
1483.690356	63.141738	65.830401
1483.358178	60.616173	65.835406
1482.662129	60.830906	65.840410
1482.501437	54.069084	65.845415
1481.487687	58.144330	65.850420
1480.509580	64.953158	65.855425
1480.021194	57.871239	65.860430
1479.350843	68.420687	65.865434
1478.754166	51.501322	65.870439
1477.928006	61.878401	65.875444
1477.013598	58.857143	65.880449
1476.781740	66.428923	65.885454
1476.226838	65.397476	65.890458
1475.933972	62.553419	65.895463
1474.960838	63.753656	65.900468
1474.115449	63.403903	65.905473
1473.212297	62.689583	65.910478
1472.443667	73.215228	65.915482
1471.975676	67.063649	65.920487
1471.179895	71.987382	65.925492
1470.891030	69.953265	65.930497
1470.581052	65.626395	65.935502
1469.621621	67.313325	65.940506
1468.858983	59.439184	65.945511
1467.948476	62.439863	65.950516
1467.595670	62.551165	65.955521
1466.666508	51.442262	65.960526
1465.768948	59.779017	65.965530
1465.443416	59.712515	65.970535
1464.961949	64.042231	65.975540
1464.394276	59.991290	65.980545
1463.361631	62.347465	65.985550
1462.613449	59.422802	65.990554
1462.294865	53.827822	65.995559
1461.777792	53.531556	66.000564
1461.301016	57.628707	66.005569
1460.137772	54.079283	66.010574
1459.314434	55.355069	66.015578
1459.526067	57.928250	66.020583
1457.980703	56.215254	66.025588
1457.261503	59.906220	66.030593
1456.760691	54.321278	66.035598
1456.141065	64.840587	66.040602
1456.163249	56.526325	66.045607
1454.918213	69.767577	66.050612
1454.346955	58.743724	66.055617
1453.614797	56.541936	66.060622
1452.978566	67.934389	66.065626
1452.611682	60.762202	66.070631
1451.333647	56.737425	66.075636
1450.732230	58.399003	66.080641
1450.319268	62.465514	66.085646
1449.579781	61.428715	66.090650
1449.327766	69.691271	66.095655
1448.091219	68.913247	66.100660
1447.644449	61.269618	66.105665
1447.085725	59.969120	66.110670
1446.140884	60.978784	66.115674
1445.527228	59.404733	66.120679
1444.896942	68.074346	66.125684
1444.378590	53.607392	66.130689
1444.143522	58.643869	66.135694
1443.313300	56.777799	66.140698
1442.515661	51.670556	66.145703
1441.607640	62.997390	66.150708
1441.258062	55.824034	66.155713
1439.995942	52.143675	66.160718
1439.038711	59.534261	66.165722
1438.857184	51.388001	66.170727
1438.147301	58.557921	66.175732
1437.577068	61.663805	66.180737
1437.695423	52.213018	66.185742
1436.843620	60.668668	66.190746
1436.288479	54.625574	66.195751
1435.191732	59.690188	66.200756
1434.576070	57.488815	66.205761
1433.514323	53.164739	66.210766
1432.894927	59.746252	66.215770
1432.592319	53.103190	66.220775
1432.073366	55.196378	66.225780
1430.938181	54.985741	66.230785
1430.704108	56.677251	66.235790
1429.837584	57.587739	66.240794
1429.434798	49.443531	66.245799
1428.150356	51.702538	66.250804
1427.157298	50.557811	66.255809
1426.889742	48.152877	66.260814
1426.095064	57.392678	66.265818
1426.104613	52.638132	66.270823
1425.780296	58.346402	66.275828
1424.919027	51.964026	66.280833
1424.509972	57.078620	66.285838
1423.552692	59.091662	66.290842
1422.511930	51.137165	66.295847
1421.648932	55.503869	66.300852
1421.025488	55.211902	66.305857
1420.745403	50.623243	66.310862
1420.062567	64.927931	66.315866
1418.698645	46.916254	66.320871
1418.142973	59.232635	66.325876
1417.837937	52.577346	66.330881
1417.753828	48.906891	66.335886
1416.813537	63.257229	66.340890
1416.220238	47.229937	66.345895
1415.447458	51.419873	66.350900
1414.602113	62.129607	66.355905
1414.225712	60.804868	66.360910
1412.936569	60.424739	66.365914
1412.433385	54.308737	66.370919
1412.001765	72.481300	66.375924
1411.642990	61.284912	66.380929
1410.807247	52.495143	66.385934
1409.553219	61.263896	66.390938
1409.098646	60.019394	66.395943
1408.557136	62.149289	66.400948
1408.208134	66.689778	66.405953
1407.841725	55.235981	66.410958
1406.629481	59.301801	66.415962
1405.993079	63.165705	66.420967
1405.255302	61.131986	66.425972
1404.793573	52.683329	66.430977
1404.095198	52.639825	66.435982
1403.087788	59.787655	66.440986
1402.748291	61.782937	66.445991
1402.036573	60.166135	66.450996
1401.681009	57.849310	66.456001
1400.904789	58.024767	66.461006
1399.969479	64.369488	66.466010
1399.848981	61.647860	66.471015
1398.976604	64.235635	66.476020
1397.787437	63.976822	66.481025
1397.325336	61.736857	66.486030
1396.633533	66.120516	66.491034
1396.687264	62.953290	66.496039
1395.718305	66.122561	66.501044
1394.567552	56.919228	66.506049
1394.141743	54.529990	66.511054
1393.387467	58.275433	66.516058
1393.337853	51.579550	66.521063
1392.010558	55.091213	66.526068
1391.368643	56.193099	66.531073
1391.021938	56.691382	66.536078
1390.495188	64.597047	66.541082
1389.616999	62.371180	66.546087
1388.624175	61.901385	66.551092
1388.131602	61.020905	66.556097
1387.819800	56.617069	66.561102
1386.870223	64.774452	66.566106
1386.235438	56.353305	66.571111
1385.428459	57.161300	66.576116
1385.016169	61.117322	66.581121
1384.178103	52.971347	66.586126
1382.786709	65.895252	66.591130
1382.698092	65.972457	66.596135
1382.079128	59.773936	66.601140
1381.750319	59.977632	66.606145
1381.718967	61.750466	66.611150
1380.546073	60.102895	66.616154
1379.914748	55.827123	66.621159
1379.215220	57.717205	66.626164
1378.223490	57.567370	66.631169
1377.722972	55.076467	66.636174
1376.820329	65.727508	66.641178
1376.552097	50.164236	66.646183
1376.099951	63.467137	66.651188
1374.829872	57.771098	66.656193
1374.131421	52.460451	66.661198
1373.688873	61.822492	66.666202
1373.281625	50.715832	66.671207
1372.234370	65.616207	66.676212
1371.537803	51.240690	66.681217
1371.216624	51.756996	66.686222
1370.428243	67.494610	66.691226
1370.262035	50.599907	66.696231
1369.075319	60.695268	66.701236
1368.376317	53.146953	66.706241
1368.282393	53.182423	66.711246
1366.505358	63.267540	66.716250
1366.130418	51.826153	66.721255
1365.505410	52.403372	66.726260
1365.173366	64.419279	66.731265
1364.919721	55.440800	66.736270
1363.700021	62.012092	66.741274
1363.105140	56.199269	66.746279
1362.384038	58.512266	66.751284
1362.103949	59.711188	66.756289
1361.337611	59.564956	66.761294
1360.060104	65.323825	66.766298
1359.735572	56.634166	66.771303
1359.505345	60.148076	66.776308
1358.373080	61.373651	66.781313
1357.569280	63.207773	66.786318
1357.036976	61.027863	66.791322
1356.755693	57.824005	66.796327
1356.327913	56.725068	66.801332
1355.208093	58.439111	66.806337
1354.375812	64.838432	66.811342
1353.595010	69.233096	66.816346
1353.597620	50.696717	66.821351
1352.681694	61.774084	66.826356
1351.433654	59.748955	66.831361
1350.729123	46.385572	66.836366
1349.903486	58.328546	66.841370
1349.943562	59.009784	66.846375
1349.545258	58.746701	66.851380
1348.883062	47.893472	66.856385
1348.177733	50.705448	66.861390
1347.118246	61.373542	66.866394
1347.253488	56.745678	66.871399
1346.056292	60.588353	66.876404
1345.057310	51.848216	66.881409
1344.911577	42.592390	66.886414
1343.977296	55.407365	66.891418
1343.551231	56.749346	66.896423
1342.364838	53.612103	66.901428
1341.894939	59.100663	66.906433
1341.554461	55.330615	66.911438
1340.574228	63.070250	66.916442
1339.562163	51.168744	66.921447
1339.156002	55.380845	66.926452
1338.690385	49.415015	66.931457
1338.412002	54.950402	66.936462
1337.312205	62.037244	66.941466
1336.608611	52.966294	66.946471
1336.103488	52.068896	66.951476
1335.412262	56.649599	66.956481
1335.316490	53.913007	66.961486
1333.933197	60.887219	66.966490
1333.339598	57.679396	66.971495
1332.974634	52.430868	66.976500
1332.036875	58.801228	66.981505
1331.360198	61.294833	66.986510
1330.406648	60.471878	66.991514
1330.254311	48.167193	66.996519
1329.773361	54.892296	67.001524
1328.442120	54.069460	67.006529
1327.883594	53.800312	67.011534
1326.932540	62.306462	67.016538
1326.748173	58.063731	67.021543
1326.390954	57.295790	67.026548
1325.797105	52.648215	67.031553
1325.323631	54.917123	67.036558
1324.163615	60.616326	67.041562
1323.745079	54.376501	67.046567
1322.709895	59.007157	67.051572
1321.755328	56.075926	67.056577
1321.404653	54.130508	67.061582
1320.964604	56.837239	67.066586
1320.424865	54.923455	67.071591
1319.109491	50.117768	67.076596
1318.427474	58.928086	67.081601
1318.324195	53.883969	67.086606
1317.565365	65.759563	67.091610
1317.560074	54.839755	67.096615
1316.211189	65.979657	67.101620
1315.207900	51.632426	67.106625
1315.222666	57.646349	67.111630
1314.373435	61.440025	67.116634
1313.702930	50.974492	67.121639
1312.828812	58.243088	67.126644
1312.002117	62.779101	67.131649
1311.856670	55.011910	67.136654
1310.907507	70.776674	67.141658
1309.811737	59.006759	67.146663
1309.427545	58.702014	67.151668
1308.942892	59.935041	67.156673
1308.781773	54.748729	67.161678
1307.655129	61.142818	67.166682
1306.913935	48.871829	67.171687
1306.284987	58.925845	67.176692
1305.595726	66.974056	67.181697
1305.366435	51.768897	67.186702
1303.727311	61.412644	67.191706
1302.993610	63.970518	67.196711
1302.973574	59.206487	67.201716
1302.260002	63.645669	67.206721
1302.510447	49.394020	67.211726
1301.065534	60.558653	67.216730
1300.656521	61.785964	67.221735
1300.094542	57.576462	67.226740
1299.301287	52.648352	67.231745
1298.581054	52.889057	67.236750
1297.417173	56.057809	67.241754
1297.058880	51.426409	67.246759
1296.584547	60.121708	67.251764
1295.722013	55.602015	67.256769
1295.291819	54.703752	67.261774
1294.413101	62.264830	67.266778
1294.079644	51.764641	67.271783
1292.584420	50.262979	67.276788
1291.823919	54.914630	67.281793
1291.577409	49.025943	67.286798
1291.111937	58.642374	67.291802
1290.850805	48.761487	67.296807
1290.350815	54.030903	67.301812
1289.032457	65.375702	67.306817
1288.839218	55.351549	67.311822
1287.886206	60.369710	67.316826
1286.927254	53.854683	67.321831
1286.362316	56.078214	67.326836
1285.721459	60.034316	67.331841
1285.475320	51.108280	67.336846
1284.438253	62.126074	67.341850
1283.647119	62.833807	67.346855
1283.613839	55.731625	67.351860
1282.945130	65.176942	67.356865
1282.633771	55.475930	67.361870
1281.239825	56.954459	67.366874
1280.390274	56.559701	67.371879
1279.926624	56.622417	67.376884
1278.988974	59.621164	67.381889
1278.371752	47.735765	67.386894
1277.516316	59.396480	67.391898
1277.619506	56.546254	67.396903
1276.788304	54.527430	67.401908
1275.632225	56.726676	67.406913
1274.972435	57.072898	67.411918
1274.259004	54.041844	67.416922
1274.103241	58.229911	67.421927
1273.658295	57.996334	67.426932
1272.539513	59.125182	67.431937
1271.760425	64.090465	67.436942
1271.050011	58.379618	67.441946
1271.087280	59.543860	67.446951
1270.487444	58.095394	67.451956
1269.326227	55.085074	67.456961
1268.710951	49.654003	67.461966
1267.944813	61.172786	67.466970
1267.114896	53.557011	67.471975
1266.416173	53.821113	67.476980
1265.844157	58.177869	67.481985
1265.400379	48.743930	67.486990
1264.844366	61.227541	67.491994
1264.442341	56.382320	67.496999
1263.198834	61.735268	67.502004
1262.649806	61.158688	67.507009
1262.300462	51.815392	67.512014
1261.651194	59.966061	67.517018
1260.609557	53.273376	67.522023
1259.974730	60.093921	67.527028
1259.190683	60.850999	67.532033
1259.186568	48.779810	67.537038
1257.715988	55.310605	67.542042
1257.278801	54.601123	67.547047
1256.338073	46.930433	67.552052
1256.010302	55.961984	67.557057
1255.690147	59.056525	67.562062
1255.177504	56.297910	67.567066
1254.197701	60.550770	67.572071
1253.535693	52.583442	67.577076
1252.923839	57.008036	67.582081
1252.226125	52.115215	67.587086
1251.102792	56.037650	67.592090
1250.725868	47.449394	67.597095
1250.283167	55.750148	67.602100
1249.578856	60.872283	67.607105
1249.181366	61.047491	67.612110
1248.180953	59.870887	67.617114
1247.926655	52.206173	67.622119
1247.270676	56.931105	67.627124
1245.902985	57.741564	67.632129
1245.045187	47.137102	67.637134
1244.395004	54.925209	67.642138
1244.364279	49.568358	67.647143
1243.762324	51.499731	67.652148
1242.955766	56.007327	67.657153
1242.339006	45.530125	67.662158
1241.419670	55.384310	67.667162
1241.143893	52.898703	67.672167
1240.699556	55.634512	67.677172
1239.648479	49.165697	67.682177
1239.169861	45.971159	67.687182
1238.468913	49.815395	67.692186
1237.820490	50.626608	67.697191
1236.703267	45.464602	67.702196
1236.140327	53.674086	67.707201
1235.964483	48.523243	67.712206
1234.767731	53.734721	67.717210
1234.168893	49.761341	67.722215
1233.830199	54.883689	67.727220
1233.425966	56.630657	67.732225
1232.422670	42.565763	67.737230
1231.134082	45.708637	67.742234
1230.877210	55.682995	67.747239
1230.765071	51.094470	67.752244
1230.059702	51.121514	67.757249
1229.099398	53.472580	67.762254
1228.204237	59.186477	67.767258
1227.734200	53.628240	67.772263
1227.214046	57.424807	67.777268
1226.362290	57.751103	67.782273
1225.730282	50.575397	67.787278
1224.786390	60.461880	67.792282
1224.346596	62.613483	67.797287
1223.944291	63.346140	67.802292
1222.832920	65.039971	67.807297
1222.412315	61.148639	67.812302
1221.433658	58.407364	67.817306
1221.092953	56.666962	67.822311
1221.060179	61.267569	67.827316
1219.798728	58.295290	67.832321
1219.392507	60.003151	67.837326
1218.792034	57.983927	67.842330
1217.738251	55.240408	67.847335
1216.915490	58.386489	67.852340
1216.122522	65.555475	67.857345
1216.065160	53.279862	67.862350
1215.408038	56.226135	67.867354
1214.596987	59.695216	67.872359
1213.593416	55.584345	67.877364
1213.253513	57.011995	67.882369
1213.046903	53.722166	67.887374
1211.573677	58.763149	67.892378
1210.654578	59.224742	67.897383
1210.365041	54.659697	67.902388
1209.861850	57.117857	67.907393
1209.884997	53.521827	67.912398
1208.516396	58.125117	67.917402
1207.773252	59.558543	67.922407
1207.283145	58.382810	67.927412
1206.471338	62.444963	67.932417
1206.295871	48.691570	67.937422
1205.265990	53.425505	67.942426
1204.709158	54.436632	67.947431
1204.217389	52.683986	67.952436
1203.170378	53.531784	67.957441
1202.370700	54.185705	67.962446
1201.591189	58.507658	67.967450
1201.222973	54.349374	67.972455
1200.930910	56.128972	67.977460
1200.134959	58.619497	67.982465
1199.583288	54.329535	67.987470
1198.560720	56.767787	67.992474
1198.248830	58.112134	67.997479
1197.268866	58.849922	68.002484
1196.205177	55.183870	68.007489
1195.863759	46.526901	68.012494
1195.540374	57.831779	68.017498
1195.514809	44.674312	68.022503
1194.385169	47.635805	68.027508
1192.989763	55.129258	68.032513
1192.932156	54.439851	68.037518
1191.965368	55.798457	68.042522
1190.927681	49.501005	68.047527
1190.725716	50.419431	68.052532
1190.536307	58.443362	68.057537
1190.002177	48.785688	68.062542
1188.734132	54.979949	68.067546
1188.230143	46.322028	68.072551
1187.696598	38.900441	68.077556
1186.469040	47.857457	68.082561
1186.013437	41.170968	68.087566
1185.515727	48.518507	68.092570
1184.515855	50.316050	68.097575
1184.759398	48.706674	68.102580
1183.406759	58.107800	68.107585
1182.880816	51.016167	68.112590
1182.329900	45.062366	68.117594
1181.701886	46.442795	68.122599
1180.631334	52.108900	68.127604
1179.804809	61.286008	68.132609
1179.536172	48.788530	68.137614
1179.296142	53.288050	68.142618
1178.316586	43.030999	68.147623
1177.440311	51.716107	68.152628
1176.643947	59.387122	68.157633
1176.327534	55.838786	68.162638
1175.465222	55.827724	68.167642
1174.732536	53.496794	68.172647
1173.880559	53.391046	68.177652
1173.380873	61.308202	68.182657
1173.297630	47.223175	68.187662
1172.590727	55.605377	68.192666
1171.593795	48.732160	68.197671
1170.932593	53.819068	68.202676
1170.127384	56.285842	68.207681
1169.682711	46.804764	68.212686
1168.816471	59.025474	68.217690
1168.090207	55.725251	68.222695
1167.626527	53.282154	68.227700
1167.085219	63.339599	68.232705
1166.669619	48.386466	68.237710
1165.490353	57.223850	68.242714
1164.544587	56.871241	68.247719
1164.473655	52.752420	68.252724
1163.625123	56.229052	68.257729
1162.568923	47.198479	68.262734
1161.921685	51.095693	68.267738
1161.791019	46.675707	68.272743
1161.400299	45.673417	68.277748
1160.397356	59.846106	68.282753
1159.867886	45.166561	68.287758
1159.168509	53.443487	68.292762
1158.754453	52.981085	68.297767
1157.692411	55.345204	68.302772
1156.638862	59.780139	68.307777
1156.216046	52.698921	68.312782
1155.910329	49.185159	68.317786
1155.296822	58.616981	68.322791
1154.616364	51.945756	68.327796
1153.647283	54.066427	68.332801
1153.300843	43.849048	68.337806
1152.444844	53.142811	68.342810
1151.591296	49.403934	68.347815
1150.743266	54.723992	68.352820
1149.740224	55.478084	68.357825
1149.860887	54.624703	68.362830
1149.252692	57.914879	68.367834
1148.997616	54.191208	68.372839
1148.062337	60.506034	68.377844
1147.228594	57.894710	68.382849
1146.727438	47.657781	68.387854
1145.538904	59.593856	68.392858
1145.013924	59.343068	68.397863
1144.629871	55.773954	68.402868
1144.319959	61.142475	68.407873
1143.294431	43.794715	68.412878
1142.373852	55.878986	68.417882
1141.761048	56.250886	68.422887
1141.527678	51.377292	68.427892
1140.515298	58.292599	68.432897
1139.780337	46.624680	68.437902
1139.035080	62.379116	68.442906
1138.619349	52.727856	68.447911
1138.293278	50.882635	68.452916
1137.040598	53.155654	68.457921
1136.441461	45.913249	68.462926
1135.701989	47.953251	68.467930
1135.626014	49.632252	68.472935
1134.837221	51.162846	68.477940
1133.714784	60.733967	68.482945
1133.348729	57.925256	68.487950
1132.813441	59.680466	68.492954
1131.719710	51.900122	68.497959
1130.860666	49.838468	68.502964
1130.263048	68.939457	68.507969
1130.211445	52.351446	68.512974
1129.542075	54.560078	68.517978
1129.002335	51.889383	68.522983
1128.161595	51.345038	68.527988
1127.171468	54.536688	68.532993
1127.110296	51.206391	68.537998
1125.820737	57.894546	68.543002
1124.841638	53.108025	68.548007
1124.484023	54.957982	68.553012
1123.523793	62.013239	68.558017
1123.595372	47.821593	68.563022
1123.052310	52.083877	68.568026
1121.993414	51.332953	68.573031
1121.537468	45.483915	68.578036
1120.839885	61.278078	68.583041
1120.140312	50.867705	68.588046
1119.259315	50.462233	68.593050
1118.579997	51.033956	68.598055
1118.083428	50.169937	68.603060
1117.343325	53.312361	68.608065
1117.043068	46.006653	68.613070
1115.637739	56.012290	68.618074
1115.159210	48.348574	68.623079
1115.129390	49.129234	68.628084
1114.457163	53.289060	68.633089
1113.385079	42.772363	68.638094
1112.782631	56.865589	68.643098
1112.087272	53.809633	68.648103
1111.720451	48.515713	68.653108
1110.545059	62.124475	68.658113
1110.073749	49.768064	68.663118
1109.587144	56.235466	68.668122
1108.970263	59.891317	68.673127
1108.354394	50.825424	68.678132
1107.377215	59.479294	68.683137
1106.935690	56.723595	68.688142
1106.174444	60.902315	68.693146
1105.817585	50.486323	68.698151
1104.745205	47.356296	68.703156
1103.729589	50.870560	68.708161
1103.864107	44.509704	68.713166
1103.129055	48.815146	68.718170
1102.280466	59.776201	68.723175
1101.528242	52.808895	68.728180
1100.517896	54.590789	68.733185
1100.508366	46.393573	68.738190
1099.948313	52.289172	68.743194
1098.826682	55.463903	68.748199
1098.590314	41.564105	68.753204
1098.038607	49.745009	68.758209
1097.248388	44.428553	68.763214
1096.033674	51.899617	68.768218
1095.273180	47.567205	68.773223
1095.146963	50.178314	68.778228
1094.597353	51.473750	68.783233
1093.502923	45.825630	68.788238
1092.590664	53.253316	68.793242
1092.209260	49.617559	68.798247
1091.995447	59.998241	68.803252
1090.823268	55.931591	68.808257
1090.168260	50.961066	68.813262
1089.559020	59.330905	68.818266
1089.102568	56.274802	68.823271
1088.878610	50.328942	68.828276
1087.726926	55.656318	68.833281
1087.274096	48.365422	68.838286
1086.560803	57.131866	68.843290
1085.836539	56.419193	68.848295
1084.900883	52.748596	68.853300
1084.029937	59.827509	68.858305
1083.984302	49.768880	68.863310
1083.099992	46.645218	68.868314
1081.768378	51.770976	68.873319
1081.941291	48.124318	68.878324
1080.925891	51.559707	68.883329
1080.648729	52.895389	68.888334
1080.045640	57.600903	68.893338
1079.095896	56.685974	68.898343
1078.629823	50.232991	68.903348
1078.007904	46.807389	68.908353
1077.077931	49.524275	68.913358
1076.403773	53.774305	68.918362
1075.597790	52.636231	68.923367
1075.250705	50.531006	68.928372
1074.541769	60.869020	68.933377
1073.686815	38.842053	68.938382
1072.734588	48.592695	68.943386
1072.093074	52.518981	68.948391
1072.027881	44.128770	68.953396
1071.096364	49.865838	68.958401
1070.901546	47.053556	68.963406
1069.603453	51.289296	68.968410
1069.130645	53.223817	68.973415
1068.779971	48.499785	68.978420
1068.186862	63.023629	68.983425
1067.142380	54.732422	68.988430
1066.154558	51.352413	68.993434
1065.499568	55.231958	68.998439
1065.365171	51.009698	69.003444
1064.898539	52.309287	69.008449
1064.186905	42.574236	69.013454
1063.257319	52.300781	69.018458
1063.333952	48.434467	69.023463
1062.142575	49.578106	69.028468
1061.109922	50.780077	69.033473
1060.751426	47.372500	69.038478
1059.746030	55.149333	69.043482
1059.046007	49.615110	69.048487
1058.157788	54.517376	69.053492
1057.608974	54.202588	69.058497
1057.397129	44.276065	69.063502
1057.172318	47.159908	69.068506
1056.189235	52.865760	69.073511
1055.540980	43.502260	69.078516
1054.546735	58.678131	69.083521
1054.260534	45.820774	69.088526
1053.142880	51.600075	69.093530
1052.529472	48.501139	69.098535
1052.493285	50.870840	69.103540
1051.636840	60.519525	69.108545
1050.825789	47.389262	69.113550
1049.781081	62.631514	69.118554
1049.394098	49.602525	69.123559
1048.939897	54.522484	69.128564
1048.103703	58.380397	69.133569
1047.328057	46.326319	69.138574
1046.590384	52.562426	69.143578
1046.430792	52.983677	69.148583
1045.385331	48.286599	69.153588
1044.686080	52.876526	69.158593
1044.023143	44.710723	69.163598
1043.446897	50.621522	69.168602
1042.917696	47.400381	69.173607
1042.118793	52.605417	69.178612
1041.051228	54.104693	69.183617
1041.118807	52.753540	69.188622
1040.428015	54.501966	69.193626
1039.349823	60.315999	69.198631
1038.666881	52.047718	69.203636
1037.645232	54.859630	69.208641
1037.688192	49.172520	69.213646
1037.190699	50.764036	69.218650
1036.009248	47.768090	69.223655
1035.328036	52.438730	69.228660
1034.788027	53.833579	69.233665
1034.532151	51.639731	69.238670
1033.644029	47.308721	69.243674
1032.566731	51.845251	69.248679
1032.200561	50.854846	69.253684
1031.670126	52.052626	69.258689
1031.349089	46.686783	69.263694
1030.579450	50.529380	69.268698
1029.830897	53.498125	69.273703
1029.285739	45.327782	69.278708
1027.599574	45.949320	69.283713
1027.240843	43.027500	69.288718
1026.660012	51.017501	69.293722
1026.008103	56.098230	69.298727
1026.098308	40.339267	69.303732
1025.316016	54.074747	69.308737
1024.393965	50.908224	69.313742
1023.771073	53.051138	69.318746
1022.783413	43.675413	69.323751
1022.079227	44.727368	69.328756
1021.253341	48.121589	69.333761
1020.625776	44.316847	69.338766
1020.428914	47.194669	69.343770
1020.085364	57.958694	69.348775
1019.357160	51.929061	69.353780
1018.231297	53.167955	69.358785
1017.796030	49.433547	69.363790
1017.460640	52.814390	69.368794
1016.343984	52.553682	69.373799
1015.825359	44.647210	69.378804
1015.020107	53.492952	69.383809
1014.585262	49.755323	69.388814
1013.094518	51.544291	69.393818
1012.297120	56.589822	69.398823
1012.429523	45.850006	69.403828
1011.452960	51.468100	69.408833
1011.473044	46.879062	69.413838
1011.013773	41.025851	69.418842
1009.945431	52.758336	69.423847
1009.121675	39.363610	69.428852
1008.782505	53.474879	69.433857
1008.000944	56.928286	69.438862
1007.337458	52.343921	69.443866
1006.642820	51.473590	69.448871
1005.791063	43.878749	69.453876
1004.659234	50.595477	69.458881
1004.049826	58.533260	69.463886
1003.811222	53.242616	69.468890
1003.341896	52.099890	69.473895
1002.839244	44.296539	69.478900
1002.224484	47.929993	69.483905
1001.607555	42.429881	69.488910
1000.572370	47.521129	69.493914
999.595688	45.990761	69.498919
998.863642	42.216842	69.503924
998.350651	51.344100	69.508929
998.115673	46.787759	69.513934
997.282873	55.901246	69.518938
996.418779	50.312721	69.523943
995.780381	46.937074	69.528948
994.960845	54.611815	69.533953
994.908611	49.010817	69.538958
994.075322	57.029954	69.543962
992.965788	48.124651	69.548967
992.741499	49.128646	69.553972
991.876936	53.610843	69.558977
991.486413	44.952274	69.563982
990.608478	51.691691	69.568986
989.694929	52.762773	69.573991
989.585329	42.141892	69.578996
988.887868	51.894603	69.584001
988.080693	50.840328	69.589006
987.306875	58.889430	69.594010
986.778885	43.594691	69.599015
986.053935	52.154843	69.604020
984.702710	58.567437	69.609025
984.174000	47.484946	69.614030
984.013152	48.053060	69.619034
983.049679	52.152020	69.624039
983.307904	54.482762	69.629044
982.303267	54.491257	69.634049
981.556595	44.441683	69.639054
980.996200	47.840982	69.644058
980.358610	53.288456	69.649063
979.266666	48.333871	69.654068
978.740736	52.948276	69.659073
978.097147	42.032307	69.664078
977.557318	56.531904	69.669082
976.481231	52.431100	69.674087
975.705942	43.548322	69.679092
975.172685	51.209055	69.684097
974.998825	41.692831	69.689102
974.382121	53.426007	69.694106
973.467896	48.848433	69.699111
973.020610	48.629475	69.704116
972.084735	53.264953	69.709121
971.423560	43.575526	69.714126
970.324427	48.375755	69.719130
969.878278	47.070073	69.724135
969.623880	46.546029	69.729140
969.247148	45.658242	69.734145
968.433253	55.577721	69.739150
967.533388	52.906019	69.744154
966.604458	50.179017	69.749159
966.675332	45.646556	69.754164
965.096008	48.260217	69.759169
964.399968	44.862211	69.764174
964.281995	48.825066	69.769178
963.596555	52.353078	69.774183
963.435280	45.529923	69.779188
962.138277	54.586390	69.784193
961.522394	49.633336	69.789198
961.052067	50.222310	69.794202
960.053841	52.560581	69.799207
959.346390	55.932822	69.804212
958.383729	64.647508	69.809217
958.335196	54.083140	69.814222
958.103246	56.220634	69.819226
957.019670	58.104122	69.824231
956.622865	44.206232	69.829236
955.595195	58.288283	69.834241
955.072083	53.178539	69.839246
953.949060	52.138263	69.844250
952.826840	56.106371	69.849255
952.839699	46.304965	69.854260
952.143994	52.430334	69.859265
951.743885	52.875669	69.864270
951.507152	52.340931	69.869274
950.125297	57.845339	69.874279
949.780077	49.039217	69.879284
948.999696	58.033986	69.884289
948.710928	56.853078	69.889294
947.732701	52.001840	69.894298
946.753964	61.595890	69.899303
946.690760	54.635700	69.904308
945.456877	64.547902	69.909313
944.692208	52.878479	69.914318
944.206104	51.997061	69.919322
943.704470	60.983748	69.924327
943.630371	53.145333	69.929332
942.462931	63.652526	69.934337
941.757505	55.397318	69.939342
940.994970	53.566385	69.944346
940.586268	51.554567	69.949351
940.470087	43.516268	69.954356
938.889017	53.568869	69.959361
938.138226	50.113350	69.964366
937.922636	53.596565	69.969370
936.967935	53.578208	69.974375
935.918184	44.822700	69.979380
935.191671	54.906481	69.984385
934.986694	51.630618	69.989390
934.650123	54.615834	69.994394
934.045609	61.806936	69.999399
933.542672	47.984286	70.004404
932.561642	57.476198	70.009409
932.117069	50.862133	70.014414
931.499137	49.834534	70.019418
930.116146	50.529321	70.024423
929.669667	48.676485	70.029428
929.232084	63.151935	70.034433
928.894907	54.658356	70.039438
927.633397	58.232316	70.044442
926.750425	62.031475	70.049447
926.654896	48.178690	70.054452
926.271702	57.878251	70.059457
925.286005	54.028021	70.064462
924.273780	50.642494	70.069466
923.551058	51.967090	70.074471
923.208478	48.575929	70.079476
922.770918	54.354290	70.084481
922.125598	51.422897	70.089486
921.220565	58.895216	70.094490
920.144733	63.138239	70.099495
920.247682	50.952284	70.104500
919.742420	55.632798	70.109505
918.456244	58.830633	70.114510
918.020397	57.688904	70.119514
917.335247	53.049666	70.124519
916.909470	52.179154	70.129524
915.824383	58.697664	70.134529
915.424960	49.569009	70.139534
915.041486	54.772626	70.144538
913.659276	58.255411	70.149543
913.017358	47.749212	70.154548
911.984725	56.173837	70.159553
911.984016	55.751356	70.164558
911.500327	54.487929	70.169562
910.902291	56.981735	70.174567
910.532647	52.423180	70.179572
909.612639	64.693506	70.184577
908.854559	53.275368	70.189582
908.086036	56.442870	70.194586
906.923102	48.774584	70.199591
906.604711	57.842501	70.204596
906.024928	58.786379	70.209601
906.045375	54.869082	70.214606
904.541796	53.643379	70.219610
904.001413	58.230135	70.224615
903.876189	58.973939	70.229620
902.910102	59.176608	70.234625
901.792406	51.322925	70.239630
901.170247	54.419826	70.244634
900.317304	60.155485	70.249639
900.663073	51.293025	70.254644
899.988443	62.505568	70.259649
898.877205	62.285051	70.264654
898.217030	48.504783	70.269658
897.570791	59.555107	70.274663
896.588289	49.309701	70.279668
895.937747	58.198661	70.284673
895.346230	54.640534	70.289678
894.696991	51.632501	70.294682
894.673710	53.129651	70.299687
893.783273	58.620537	70.304692
892.965389	47.931034	70.309697
892.440863	52.769161	70.314702
891.212461	44.546743	70.319706
890.177937	54.215917	70.324711
889.572021	50.164911	70.329716
889.213582	56.030034	70.334721
889.004749	55.594943	70.339726
888.632275	46.104032	70.344730
888.083337	51.950584	70.349735
887.096456	50.923366	70.354740
886.405863	66.557170	70.359745
885.459048	55.123344	70.364750
884.524127	46.165080	70.369754
883.942798	53.935980	70.374759
883.591775	54.173237	70.379764
882.989932	60.753628	70.384769
882.845734	53.651789	70.389774
881.990365	54.540182	70.394778
881.075941	58.632948	70.399783
880.457104	56.837513	70.404788
879.169103	60.243821	70.409793
878.342886	52.380031	70.414798
878.076045	52.958712	70.419802
877.432822	61.441227	70.424807
876.997980	51.523416	70.429812
876.500184	54.438101	70.434817
875.992101	59.284655	70.439822
875.408616	59.823843	70.444826
874.568274	65.947021	70.449831
874.183600	53.893869	70.454836
872.759996	56.154790	70.459841
872.182273	56.674139	70.464846
871.755002	48.966061	70.469850
870.943855	56.817697	70.474855
870.701944	50.680759	70.479860
869.787931	64.814137	70.484865
869.253865	52.582909	70.489870
869.053960	58.528461	70.494874
867.469946	52.540469	70.499879
867.182302	55.498981	70.504884
866.246392	55.673206	70.509889
865.750040	60.801753	70.514894
864.791345	60.134340	70.519898
863.897682	57.767626	70.524903
863.926643	51.494535	70.529908
863.264923	60.170811	70.534913
862.729695	55.324798	70.539918
862.012781	51.436548	70.544922
860.634638	57.000334	70.549927
860.486449	49.153222	70.554932
859.927243	58.311509	70.559937
859.387945	62.134839	70.564942
858.805733	52.782971	70.569946
857.523364	60.372136	70.574951
857.646562	48.473131	70.579956
856.502350	56.521287	70.584961
855.532374	48.839664	70.589966
855.223222	52.771446	70.594970
854.547450	61.079368	70.599975
854.245067	49.173981	70.604980
853.257447	55.216520	70.609985
852.597986	53.097969	70.614990
852.172762	58.516400	70.619994
851.220619	57.994610	70.624999
850.220993	52.470293	70.630004
849.329219	60.415195	70.635009
849.141434	46.799465	70.640014
848.938925	49.906856	70.645018
848.430292	46.430172	70.650023
847.360859	50.514501	70.655028
846.740139	49.936809	70.660033
846.358178	54.372200	70.665038
845.376092	56.458781	70.670042
844.102525	54.001151	70.675047
843.761058	44.256153	70.680052
843.237911	55.972878	70.685057
842.829428	55.306212	70.690062
842.301846	52.026512	70.695066
841.075525	53.735645	70.700071
840.793197	54.927089	70.705076
840.644787	55.516887	70.710081
839.336008	52.487688	70.715086
838.712370	52.042928	70.720090
837.941303	51.582210	70.725095
837.608405	49.976247	70.730100
836.145039	62.164334	70.735105
835.505704	53.876569	70.740110
834.931241	53.412945	70.745114
834.550409	54.325172	70.750119
834.881555	45.657433	70.755124
834.067468	46.496692	70.760129
832.609429	46.326673	70.765134
832.214545	41.235980	70.770138
831.559974	49.236168	70.775143
830.623218	44.228570	70.780148
829.970941	50.624600	70.785153
829.211050	46.334764	70.790158
829.084785	49.999312	70.795162
828.021170	51.698322	70.800167
826.944244	47.517298	70.805172
826.339928	52.007006	70.810177
825.901784	49.820119	70.815182
826.095271	41.210565	70.820186
825.070947	47.322031	70.825191
824.643765	44.665036	70.830196
823.756232	53.877162	70.835201
823.240528	56.290071	70.840206
821.865754	44.919674	70.845210
821.187428	51.135346	70.850215
820.714071	42.761247	70.855220
820.533452	56.195983	70.860225
819.605206	50.196686	70.865230
818.710997	47.856886	70.870234
817.910173	54.803278	70.875239
817.976294	54.259771	70.880244
817.245141	51.821475	70.885249
816.176321	50.375233	70.890254
815.712577	47.936952	70.895258
815.179543	52.454741	70.900263
814.539886	51.627753	70.905268
813.279389	55.852899	70.910273
812.532630	49.797908	70.915278
812.230873	44.531542	70.920282
812.099999	55.821545	70.925287
811.150130	46.685918	70.930292
810.118522	54.072755	70.935297
809.104494	53.448866	70.940302
809.276413	50.805321	70.945306
808.266167	59.349422	70.950311
807.237470	51.191457	70.955316
806.674468	57.735713	70.960321
806.372676	54.402735	70.965326
806.248367	52.653184	70.970330
805.356788	52.662677	70.975335
804.732322	41.915620	70.980340
803.784281	49.938872	70.985345
802.923921	52.922321	70.990350
801.826759	45.574791	70.995354
801.224365	57.863965	71.000359
801.003574	51.553362	71.005364
800.344408	54.949495	71.010369
799.933583	46.234279	71.015374
799.456295	45.788312	71.020378
798.214043	57.318306	71.025383
797.990052	49.038560	71.030388
797.182104	58.274297	71.035393
796.364120	54.805865	71.040398
795.623478	45.824601	71.045402
794.886319	51.423580	71.050407
794.651198	56.915837	71.055412
794.113401	50.162102	71.060417
792.838136	55.331067	71.065422
792.381150	50.215571	71.070426
791.811840	54.622442	71.075431
791.616605	48.074380	71.080436
790.541443	52.194338	71.085441
789.849177	54.949178	71.090446
789.506500	49.724022	71.095450
788.251164	58.259834	71.100455
787.725615	57.799473	71.105460
787.004241	54.432362	71.110465
786.369266	52.291009	71.115470
786.208982	51.728347	71.120474
784.896777	56.529452	71.125479
784.299928	53.082594	71.130484
783.608913	47.786732	71.135489
783.342238	53.351821	71.140494
783.046347	49.839708	71.145498
781.832820	59.005969	71.150503
781.488433	53.921437	71.155508
780.846907	54.301149	71.160513
779.961217	53.078089	71.165518
779.138799	45.937575	71.170522
778.511749	51.071166	71.175527
778.436298	49.766434	71.180532
777.301272	48.600414	71.185537
776.045898	55.499326	71.190542
775.865720	47.261496	71.195546
775.155689	53.472763	71.200551
774.856413	47.051655	71.205556
774.037528	47.629917	71.210561
773.219962	50.559252	71.215566
772.692230	54.112667	71.220570
771.733259	56.697077	71.225575
771.801254	50.800986	71.230580
770.743176	45.394826	71.235585
770.108553	45.312962	71.240590
769.582444	50.146629	71.245594
768.574749	62.084007	71.250599
767.884906	50.789113	71.255604
767.441281	57.186635	71.260609
766.584865	58.255009	71.265614
766.430588	53.588078	71.270618
765.146023	57.107435	71.275623
764.706787	53.146626	71.280628
764.021332	51.357098	71.285633
763.614126	51.590699	71.290638
762.653944	51.142764	71.295642
761.597296	53.599222	71.300647
761.666102	48.327489	71.305652
761.078169	46.408894	71.310657
760.174118	50.249304	71.315662
759.584755	44.304898	71.320666
758.760264	50.412962	71.325671
758.446058	44.341172	71.330676
757.392324	46.152180	71.335681
756.528594	49.714931	71.340686
756.222046	51.892700	71.345690
755.709335	54.491228	71.350695
754.831104	47.791702	71.355700
753.828776	54.238746	71.360705
753.178829	57.027860	71.365710
752.963076	51.883431	71.370714
752.255139	55.099678	71.375719
751.461766	45.131750	71.380724
750.567095	52.840588	71.385729
749.888555	49.982345	71.390734
749.812503	52.713211	71.395738
749.257792	56.348198	71.400743
748.131452	44.864182	71.405748
747.602380	45.009952	71.410753
746.736766	49.039794	71.415758
746.722573	43.625155	71.420762
745.370174	54.078276	71.425767
744.975813	49.194100	71.430772
744.405054	49.888990	71.435777
743.687940	52.192050	71.440782
742.865721	46.937591	71.445786
741.966605	55.263741	71.450791
741.675532	43.965301	71.455796
741.089268	54.529845	71.460801
740.110203	56.884072	71.465806
739.609164	48.088615	71.470810
738.875993	57.396039	71.475815
738.328826	42.845631	71.480820
738.187773	47.335718	71.485825
736.796762	51.927035	71.490830
736.547542	47.923366	71.495834
735.355802	50.115907	71.500839
735.371058	50.931972	71.505844
734.085219	59.915795	71.510849
733.517764	62.493081	71.515854
733.246748	48.736082	71.520858
732.763216	59.959224	71.525863
731.838949	51.303690	71.530868
730.881839	55.836970	71.535873
730.689434	58.775600	71.540878
729.812863	53.521912	71.545882
728.523550	49.247012	71.550887
727.883467	53.390767	71.555892
727.602389	49.316476	71.560897
727.205811	57.791284	71.565902
726.984946	44.333818	71.570906
725.792403	50.967274	71.575911
725.200416	49.222802	71.580916
724.586579	47.104909	71.585921
723.851955	54.392451	71.590926
723.251532	61.101955	71.595930
722.157367	52.653251	71.600935
722.030405	49.458035	71.605940
721.271524	55.697593	71.610945
719.988896	47.614796	71.615950
719.792424	44.957360	71.620954
719.128503	52.419729	71.625959
718.775010	50.831256	71.630964
717.769570	54.326694	71.635969
716.736351	60.240919	71.640974
716.252797	48.022207	71.645978
715.876303	58.974413	71.650983
715.596079	47.444010	71.655988
714.422241	44.484862	71.660993
713.536683	48.666125	71.665998
713.217756	41.224699	71.671002
712.760089	44.981436	71.676007
712.030268	51.905508	71.681012
711.588130	47.639240	71.686017
710.712854	54.867176	71.691022
710.116739	46.455881	71.696026
709.036439	54.355138	71.701031
708.385163	48.316523	71.706036
708.080072	49.688227	71.711041
707.386138	58.691361	71.716046
706.589987	50.226757	71.721050
705.497404	55.079664	71.726055
705.057243	45.369338	71.731060
704.457630	49.733738	71.736065
704.026912	46.180027	71.741070
703.788811	40.297985	71.746074
702.534402	47.978954	71.751079
701.841208	49.704194	71.756084
701.244773	47.414800	71.761089
700.577943	48.260617	71.766094
700.143887	46.062066	71.771098
698.952499	63.073478	71.776103
698.960237	43.038293	71.781108
698.183080	51.122679	71.786113
697.240607	52.427132	71.791118
696.628186	40.913362	71.796122
695.807951	53.535277	71.801127
695.280651	48.200762	71.806132
695.116397	46.995331	71.811137
693.859867	64.207933	71.816142
693.394708	49.657093	71.821146
692.902647	59.752476	71.826151
692.377511	51.154837	71.831156
691.335899	49.617585	71.836161
690.540432	53.273569	71.841166
690.073852	43.993240	71.846170
689.651162	48.179659	71.851175
689.131150	49.194493	71.856180
688.138794	44.348777	71.861185
687.655097	51.098044	71.866190
686.816795	50.263296	71.871194
685.805782	55.114261	71.876199
685.056632	45.669186	71.881204
684.826433	46.461254	71.886209
684.189994	52.827982	71.891214
683.902359	38.988494	71.896218
682.583421	51.115796	71.901223
681.975763	48.601109	71.906228
681.663464	48.586218	71.911233
680.804989	44.280593	71.916238
679.932327	32.964394	71.921242
679.047985	43.694674	71.926247
678.755563	42.083867	71.931252
678.317421	39.362414	71.936257
677.855472	54.120865	71.941262
677.514517	46.711337	71.946266
676.218855	56.513623	71.951271
675.596461	50.336375	71.956276
674.681615	49.062802	71.961281
673.746156	61.676267	71.966286
673.523074	54.812527	71.971290
673.132677	53.532717	71.976295
672.872374	49.761061	71.981300
671.513779	53.336405	71.986305
670.567029	47.759598	71.991310
670.565392	40.070535	71.996314
670.025712	49.921179	72.001319
669.057537	48.312318	72.006324
668.453037	50.400342	72.011329
667.695610	56.119276	72.016334
666.724844	42.967320	72.021338
665.567001	57.928050	72.026343
665.328006	48.545252	72.031348
664.965963	46.483478	72.036353
664.452408	54.590554	72.041358
664.390217	50.022516	72.046362
662.920370	51.852514	72.051367
662.384071	48.567940	72.056372
661.822553	48.171682	72.061377
661.127292	54.576168	72.066382
659.906698	46.313216	72.071386
659.170201	56.335557	72.076391
658.964899	47.977165	72.081396
658.649048	44.745801	72.086401
658.163476	47.672767	72.091406
656.941628	43.208968	72.096410
656.370293	49.663105	72.101415
655.922169	47.920974	72.106420
655.283340	41.375763	72.111425
653.969537	57.909927	72.116430
653.459240	42.549419	72.121434
652.965475	55.437907	72.126439
652.566510	57.933184	72.131444
652.386296	48.761806	72.136449
651.080536	59.346318	72.141454
650.825733	52.263702	72.146458
649.979754	52.863665	72.151463
648.843234	50.601940	72.156468
648.119089	54.391661	72.161473
647.217895	56.257273	72.166478
647.087391	53.578300	72.171482
646.552435	59.506246	72.176487
646.188798	48.162611	72.181492
645.584504	49.470001	72.186497
644.800209	47.131688	72.191502
644.025395	49.645815	72.196506
642.994430	49.879416	72.201511
642.459280	51.169488	72.206516
642.121369	52.913862	72.211521
641.412688	49.439121	72.216526
640.670284	49.350799	72.221530
639.752786	61.120880	72.226535
639.440889	53.205249	72.231540
638.575205	47.826863	72.236545
637.922060	40.788765	72.241550
637.236861	43.283891	72.246554
636.596444	62.823793	72.251559
636.121048	52.308523	72.256564
634.937853	51.538177	72.261569
634.099157	54.264335	72.266574
634.136292	42.979889	72.271578
633.497096	48.918125	72.276583
633.079708	52.148057	72.281588
632.052526	50.491836	72.286593
631.211858	59.329114	72.291598
630.993751	51.849566	72.296602
629.703169	55.852501	72.301607
629.092551	48.263572	72.306612
628.752182	55.021563	72.311617
627.959629	51.090242	72.316622
627.566795	37.589228	72.321626
626.420450	44.295791	72.326631
625.588435	43.173052	72.331636
625.372154	42.234536	72.336641
624.978871	45.534747	72.341646
624.335239	45.246194	72.346650
623.195515	43.201039	72.351655
622.674623	44.069367	72.356660
622.120784	39.098653	72.361665
621.435499	41.223206	72.366670
620.656506	35.397356	72.371674
620.026493	49.821440	72.376679
619.845211	46.671155	72.381684
618.928037	42.050044	72.386689
617.135830	52.879194	72.391694
617.196773	45.169128	72.396698
616.615927	51.411895	72.401703
616.227778	43.252947	72.406708
615.937989	40.954166	72.411713
615.002491	46.789780	72.416718
614.220059	44.370755	72.421722
613.525114	49.420572	72.426727
612.782492	50.508721	72.431732
612.015333	47.891719	72.436737
611.225890	61.078043	72.441742
611.077121	48.332954	72.446746
610.229656	49.696426	72.451751
609.637129	47.663482	72.456756
608.466984	44.811033	72.461761
607.630949	51.182753	72.466766
607.697224	34.148735	72.471770
607.203556	46.515223	72.476775
606.256640	42.482337	72.481780
605.681828	44.608224	72.486785
604.941478	46.654818	72.491790
604.914078	34.641056	72.496794
603.449379	46.974529	72.501799
602.766897	46.231691	72.506804
602.573603	39.634466	72.511809
601.517439	54.977994	72.516814
600.852665	37.950012	72.521818
599.857540	45.698541	72.526823
599.441368	46.619583	72.531828
599.583445	46.057667	72.536833
598.173449	55.506026	72.541838
597.329319	45.740216	72.546842
596.732989	52.650939	72.551847
596.402393	52.774593	72.556852
595.859397	44.544115	72.561857
594.721255	52.228691	72.566862
594.073154	50.253488	72.571866
593.542487	54.329382	72.576871
593.078808	48.590516	72.581876
592.605168	48.035197	72.586881
591.471525	49.562526	72.591886
591.082225	48.213169	72.596890
590.768534	49.997846	72.601895
589.888552	44.449867	72.606900
589.248619	44.381511	72.611905
588.111365	50.183034	72.616910
587.810227	43.489442	72.621914
586.909029	51.533684	72.626919
585.944927	53.309985	72.631924
585.593142	49.652262	72.636929
584.921975	56.056080	72.641934
585.016801	44.682024	72.646938
583.748315	51.163628	72.651943
582.786967	56.233805	72.656948
582.703531	50.467497	72.661953
581.915733	49.643665	72.666958
581.087872	42.634990	72.671962
580.292167	50.089987	72.676967
579.443635	44.685239	72.681972
579.307672	42.324116	72.686977
578.700512	50.895548	72.691982
577.916945	38.742020	72.696986
576.680715	46.618845	72.701991
576.080816	44.825208	72.706996
576.331227	47.314839	72.712001
575.775269	48.934673	72.717006
574.897369	44.714186	72.722010
573.942170	46.135830	72.727015
573.036101	44.354688	72.732020
572.061122	39.842154	72.737025
571.127006	43.414595	72.742030
571.108875	44.620756	72.747034
570.240687	51.741942	72.752039
570.245385	43.752251	72.757044
569.583923	42.996613	72.762049
568.477238	43.603433	72.767054
568.144737	39.903219	72.772058
567.304144	41.164683	72.777063
566.336269	42.671928	72.782068
566.006162	40.926788	72.787073
565.477719	45.511694	72.792078
564.743430	39.322346	72.797082
563.666962	47.467048	72.802087
563.090026	50.602551	72.807092
562.332244	44.107855	72.812097
561.827170	52.323980	72.817102
561.746663	48.331312	72.822106
560.342898	49.543705	72.827111
559.677719	44.582855	72.832116
559.435962	37.812004	72.837121
558.358325	50.266780	72.842126
558.465807	41.986325	72.847130
557.383854	52.942083	72.852135
556.381406	53.062366	72.857140
556.228728	45.715918	72.862145
555.622028	50.646035	72.867150
554.806200	41.129634	72.872154
554.066875	46.371038	72.877159
553.814739	43.575828	72.882164
553.057570	45.517879	72.887169
551.879724	51.349537	72.892174
551.536097	42.893349	72.897178
550.815454	45.865659	72.902183
549.824134	44.060257	72.907188
549.098129	41.545534	72.912193
548.239608	39.802561	72.917198
548.129058	42.330758	72.922202
547.712077	44.715374	72.927207
546.943886	42.973783	72.932212
546.107229	40.943471	72.937217
545.397704	46.309443	72.942222
545.123797	39.368670	72.947226
544.223321	47.978941	72.952231
543.058199	42.695601	72.957236
542.928494	35.241420	72.962241
542.439765	46.044339	72.967246
541.235546	43.673600	72.972250
540.410242	51.120705	72.977255
539.809212	55.614677	72.982260
539.696299	46.252824	72.987265
539.179609	44.329247	72.992270
538.631606	41.554358	72.997274
537.430163	45.554174	73.002279
536.850144	44.859689	73.007284
536.174615	48.323143	73.012289
535.195738	47.638574	73.017294
534.569330	37.987931	73.022298
533.868304	42.330668	73.027303
533.579593	45.473882	73.032308
533.514578	32.277081	73.037313
532.189505	42.863129	73.042318
531.781590	38.394331	73.047322
531.133716	43.955492	73.052327
530.107564	46.227407	73.057332
529.364950	46.746289	73.062337
528.435289	47.722327	73.067342
528.529016	43.531595	73.072346
528.002237	50.147393	73.077351
526.949875	46.967135	73.082356
525.985486	39.289515	73.087361
525.250922	44.982760	73.092366
525.295050	40.402531	73.097370
524.692919	44.808367	73.102375
523.706550	59.932642	73.107380
523.366188	42.923977	73.112385
522.143391	38.618101	73.117390
521.133930	44.180091	73.122394
520.469689	43.659878	73.127399
519.848852	43.626346	73.132404
519.817154	45.586888	73.137409
519.325041	49.257675	73.142414
518.752785	46.822550	73.147418
517.769107	38.741146	73.152423
517.157690	42.407283	73.157428
516.849009	48.001150	73.162433
515.498160	50.832581	73.167438
515.018693	45.271296	73.172442
514.560594	43.863525	73.177447
513.695919	57.963879	73.182452
513.598941	39.970263	73.187457
511.978043	52.707139	73.192462
511.454587	51.905877	73.197466
511.228634	47.321360	73.202471
510.551973	35.357419	73.207476
509.909360	38.670551	73.212481
509.168504	50.311590	73.217486
508.480926	42.522071	73.222490
508.028079	50.523297	73.227495
507.146316	45.384074	73.232500
506.595479	42.146012	73.237505
505.928327	52.332377	73.242510
504.970819	48.074135	73.247514
504.020187	43.929919	73.252519
503.112123	49.584576	73.257524
503.126665	50.205205	73.262529
502.708394	49.797204	73.267534
502.499550	47.788323	73.272538
501.239314	49.110351	73.277543
500.400786	49.718639	73.282548
500.185596	41.235696	73.287553
498.994686	57.021771	73.292558
497.974791	52.652041	73.297562
497.644074	48.984670	73.302567
497.113148	42.253585	73.307572
497.132202	52.748536	73.312577
496.188655	54.666679	73.317582
495.368528	45.392263	73.322586
494.617340	53.617641	73.327591
494.184593	48.564589	73.332596
493.131734	47.770396	73.337601
492.133829	46.049646	73.342606
491.554021	44.707001	73.347610
491.635133	48.450481	73.352615
490.884462	47.876235	73.357620
489.937543	48.777764	73.362625
489.102303	47.603546	73.367630
488.651504	40.217869	73.372634
488.292524	55.888762	73.377639
487.037211	56.137667	73.382644
486.472216	41.667468	73.387649
485.790183	51.028292	73.392654
485.692903	44.666526	73.397658
485.356414	47.315877	73.402663
483.926669	51.935571	73.407668
483.535750	49.168786	73.412673
482.730427	49.145729	73.417678
481.424707	50.336238	73.422682
480.864546	45.289296	73.427687
480.090608	48.490892	73.432692
480.077661	48.668038	73.437697
479.344135	51.301793	73.442702
479.244970	47.804121	73.447706
478.330666	51.401824	73.452711
477.297956	48.732553	73.457716
477.174183	37.339720	73.462721
475.949556	48.192072	73.467726
475.048231	39.583474	73.472730
474.901410	44.549152	73.477735
474.194709	48.665724	73.482740
473.807685	34.469964	73.487745
472.688707	54.253261	73.492750
472.082411	49.226286	73.497754
471.704079	42.912452	73.502759
471.321945	49.787492	73.507764
470.219240	49.895396	73.512769
469.123020	53.189342	73.517774
468.715352	47.395852	73.522778
468.173240	54.070874	73.527783
467.020494	55.771615	73.532788
467.031941	41.271091	73.537793
466.208226	46.981708	73.542798
465.722318	56.394873	73.547802
464.834121	41.613468	73.552807
463.886622	50.474108	73.557812
463.398620	47.601367	73.562817
462.584097	46.225158	73.567822
462.263793	41.146318	73.572826
461.945549	49.036216	73.577831
461.134634	52.109666	73.582836
460.773220	40.630112	73.587841
459.377932	52.840632	73.592846
458.772162	47.723690	73.597850
458.104586	46.525925	73.602855
457.446259	47.409875	73.607860
457.354193	47.413542	73.612865
456.213612	55.574808	73.617870
455.427952	47.662158	73.622874
455.071025	57.255052	73.627879
454.524733	49.922441	73.632884
453.733275	48.334399	73.637889
452.702699	51.378192	73.642894
452.183589	49.286282	73.647898
451.438296	43.365236	73.652903
450.920211	52.105426	73.657908
450.270662	45.927848	73.662913
449.801201	55.257967	73.667918
449.386399	49.222763	73.672922
448.722502	48.707246	73.677927
447.615798	58.246129	73.682932
446.919319	45.850117	73.687937
446.854648	51.384613	73.692942
445.726311	47.932641	73.697946
444.750163	49.042275	73.702951
443.945843	46.607872	73.707956
443.794366	45.682704	73.712961
442.734439	50.614088	73.717966
442.470634	49.104411	73.722970
441.746031	47.185595	73.727975
440.989655	48.244446	73.732980
440.829519	45.592290	73.737985
439.685836	53.091724	73.742990
438.899617	57.927463	73.747994
438.543694	45.644355	73.752999
437.822161	49.624525	73.758004
437.394782	44.138541	73.763009
436.203227	49.966122	73.768014
435.405717	44.095980	73.773018
435.017963	54.069104	73.778023
434.492421	58.112670	73.783028
434.339566	48.772965	73.788033
433.228822	47.901286	73.793038
432.458018	44.286699	73.798042
431.983600	42.656037	73.803047
430.985797	51.975718	73.808052
430.166493	47.619793	73.813057
429.742800	54.526692	73.818062
429.011568	46.048709	73.823066
428.620161	42.403637	73.828071
427.673821	50.505577	73.833076
427.131339	48.704407	73.838081
426.429472	57.007099	73.843086
425.889826	49.059993	73.848090
425.585352	44.875937	73.853095
424.108144	59.247373	73.858100
423.530735	47.281836	73.863105
422.919846	49.544399	73.868110
422.784177	50.069111	73.873114
422.321637	41.628746	73.878119
421.427161	53.497709	73.883124
420.873259	48.621676	73.888129
420.130176	51.367358	73.893134
419.633861	47.097172	73.898138
418.527036	59.028360	73.903143
417.496585	57.953080	73.908148
417.349471	50.460681	73.913153
417.092366	55.577978	73.918158
416.089402	52.464017	73.923162
415.570563	48.937023	73.928167
414.816347	50.034961	73.933172
414.026554	55.552530	73.938177
412.831745	64.761686	73.943182
412.252820	52.692311	73.948186
411.913186	53.572802	73.953191
411.296401	55.568222	73.958196
411.085774	50.905581	73.963201
409.901580	54.587312	73.968206
409.253549	53.212978	73.973210
408.804478	46.087246	73.978215
408.402861	56.144585	73.983220
407.466893	49.359788	73.988225
406.663400	57.759103	73.993230
406.011232	55.871334	73.998234
405.600441	44.581013	74.003239
404.317016	54.550196	74.008244
404.279989	47.303615	74.013249
403.213268	54.951653	74.018254
402.811472	55.406805	74.023258
402.160145	44.848682	74.028263
400.998508	60.245344	74.033268
400.590523	56.479911	74.038273
400.194561	47.488037	74.043278
400.123487	55.952001	74.048282
399.120273	50.314924	74.053287
398.158031	53.125495	74.058292
397.860565	40.891436	74.063297
396.396648	49.184668	74.068302
395.713433	51.731579	74.073306
395.221317	46.181802	74.078311
394.509073	50.660405	74.083316
394.815744	50.908049	74.088321
394.126843	55.277276	74.093326
392.902352	54.671326	74.098330
392.541928	48.775706	74.103335
391.179946	56.723114	74.108340
390.388658	44.919408	74.113345
389.926948	54.563692	74.118350
389.201193	49.864865	74.123354
388.804280	49.169624	74.128359
388.383712	50.916159	74.133364
387.867217	43.378548	74.138369
386.794611	55.187593	74.143374
385.858522	46.956738	74.148378
385.669817	54.291405	74.153383
385.490911	54.201678	74.158388
384.726281	49.062763	74.163393
383.909544	61.649494	74.168398
383.021252	54.630023	74.173402
381.933277	53.291108	74.178407
381.025698	58.196664	74.183412
380.675260	39.693104	74.188417
380.415125	42.699310	74.193422
380.114911	48.296568	74.198426
379.369550	41.221213	74.203431
378.035514	46.607890	74.208436
377.705432	39.329165	74.213441
377.436197	45.618509	74.218446
376.327467	46.109044	74.223450
375.335086	52.154074	74.228455
374.936767	48.702504	74.233460
374.663067	49.395872	74.238465
373.991212	55.304671	74.243470
373.045530	46.900306	74.248474
372.400572	41.753367	74.253479
372.110710	47.770028	74.258484
370.897355	43.577847	74.263489
370.305755	56.552906	74.268494
369.944318	47.334762	74.273498
369.464183	50.368144	74.278503
368.013543	41.476540	74.283508
367.531307	42.136906	74.288513
366.824830	47.371544	74.293518
366.254232	47.722712	74.298522
366.469180	45.846589	74.303527
365.296058	54.364739	74.308532
364.737886	43.936869	74.313537
363.880378	51.069024	74.318542
362.430170	47.799275	74.323546
361.791526	49.858114	74.328551
361.332156	52.393017	74.333556
361.140590	37.521159	74.338561
360.640416	46.226962	74.343566
360.140271	39.431087	74.348570
359.811453	46.382795	74.353575
358.660801	49.385834	74.358580
358.093525	39.807832	74.363585
357.169365	47.195041	74.368590
355.958207	45.442100	74.373594
355.884661	49.027287	74.378599
355.236811	50.240758	74.383604
355.024696	44.255281	74.388609
353.855537	50.008363	74.393614
353.206546	49.873702	74.398618
352.924692	46.293189	74.403623
351.711798	42.898895	74.408628
351.017315	46.778580	74.413633
350.064512	45.077512	74.418638
349.649941	39.155841	74.423642
349.614692	37.896763	74.428647
348.736423	49.422530	74.433652
348.361437	42.890567	74.438657
347.430006	50.881343	74.443662
346.822224	51.426102	74.448666
345.759584	48.621309	74.453671
344.555961	54.772556	74.458676
344.419527	36.168675	74.463681
344.153679	52.882868	74.468686
343.574267	47.563061	74.473690
343.441212	37.444352	74.478695
341.870194	51.841805	74.483700
341.378470	36.721316	74.488705
340.760207	35.873699	74.493710
339.967809	41.038454	74.498714
339.040535	43.436613	74.503719
338.379013	46.319130	74.508724
338.069119	42.607469	74.513729
337.634619	42.203660	74.518734
336.383474	39.471493	74.523738
335.871256	32.556126	74.528743
335.452731	39.492165	74.533748
335.411035	35.023394	74.538753
333.941299	46.343798	74.543758
333.106720	46.232411	74.548762
332.949179	36.133376	74.553767
332.138650	39.161067	74.558772
331.533149	43.770907	74.563777
330.547241	49.775496	74.568782
330.057256	41.975053	74.573786
329.501467	44.233586	74.578791
328.928346	48.642723	74.583796
328.440700	37.307907	74.588801
327.586470	46.618927	74.593806
326.834143	44.354478	74.598810
326.252486	38.839492	74.603815
325.176932	48.425487	74.608820
325.299015	51.763451	74.613825
324.335037	47.482664	74.618830
323.392492	52.158840	74.623834
322.738124	46.172886	74.628839
321.686728	43.926139	74.633844
321.857602	42.574286	74.638849
321.225363	51.290105	74.643854
319.833302	45.303448	74.648858
319.676078	46.493929	74.653863
318.804227	53.530611	74.658868
318.613886	42.462230	74.663873
317.345359	54.586377	74.668878
316.658836	46.052425	74.673882
316.257858	41.327096	74.678887
315.593584	46.692216	74.683892
314.868297	39.413412	74.688897
314.106154	44.092376	74.693902
313.366083	49.335535	74.698906
313.389695	46.072202	74.703911
312.542183	50.911433	74.708916
311.524679	43.177722	74.713921
310.745141	35.295702	74.718926
309.941573	50.230030	74.723930
309.640162	41.800287	74.728935
309.004036	54.637365	74.733940
308.248056	41.372523	74.738945
307.733292	47.130137	74.743950
307.246309	42.943650	74.748954
306.633929	39.598753	74.753959
305.548121	46.410912	74.758964
304.861069	39.387796	74.763969
304.414129	43.776825	74.768974
303.759356	47.197600	74.773978
302.855144	39.133599	74.778983
301.747590	49.886932	74.783988
301.804838	41.398451	74.788993
301.266378	40.446661	74.793998
300.513878	46.701067	74.799002
299.540183	47.520202	74.804007
298.900393	43.727083	74.809012
298.697351	45.763818	74.814017
297.940509	46.874825	74.819022
297.307615	49.333314	74.824026
296.380326	44.777031	74.829031
295.978647	48.004502	74.834036
295.325668	45.676920	74.839041
294.259830	48.327418	74.844046
293.500311	45.494838	74.849050
293.161157	41.770501	74.854055
292.684841	49.933185	74.859060
291.844111	39.127749	74.864065
291.059919	47.740055	74.869070
290.646502	55.178347	74.874074
289.984011	37.016299	74.879079
288.831732	43.995178	74.884084
288.192624	39.246309	74.889089
287.787482	49.611721	74.894094
287.100908	42.618496	74.899098
287.000788	45.111920	74.904103
285.633643	43.932665	74.909108
285.339462	40.701062	74.914113
284.542579	44.494580	74.919118
283.772425	44.880728	74.924122
283.084437	40.678975	74.929127
282.014656	45.123127	74.934132
281.569070	47.573842	74.939137
281.384372	42.870819	74.944142
281.113227	38.741401	74.949146
280.561546	45.583553	74.954151
279.475780	51.410108	74.959156
279.022160	48.123493	74.964161
277.815535	47.972076	74.969166
276.998143	53.859936	74.974170
276.829648	43.775268	74.979175
275.961577	44.262181	74.984180
274.908727	46.622030	74.989185
274.143639	50.539797	74.994190
273.812858	49.651106	74.999194
273.800737	39.954683	75.004199
273.011805	56.525166	75.009204
272.077726	47.057695	75.014209
270.952354	41.307687	75.019214
270.575578	43.378424	75.024218
270.431786	43.461307	75.029223
268.935146	55.817378	75.034228
268.662920	47.184290	75.039233
268.019506	47.249039	75.044238
267.424582	52.331877	75.049242
267.109505	44.360067	75.054247
265.836444	46.773944	75.059252
265.435272	48.132624	75.064257
265.012112	48.821441	75.069262
263.886576	51.443621	75.074266
263.245882	40.005485	75.079271
262.652090	53.291564	75.084276
262.278871	51.860852	75.089281
261.543723	46.980638	75.094286
260.484746	40.873118	75.099290
260.111302	39.174357	75.104295
259.124703	49.479488	75.109300
259.126436	41.040860	75.114305
258.228115	41.187244	75.119310
257.206198	50.648017	75.124314
256.722465	46.755917	75.129319
256.219691	48.234874	75.134324
256.022672	52.983049	75.139329
254.810264	44.602335	75.144334
254.086021	46.742653	75.149338
253.739379	47.715746	75.154343
252.492008	52.175603	75.159348
251.731029	46.968345	75.164353
251.206911	36.943527	75.169358
250.495908	51.800032	75.174362
250.411747	38.185275	75.179367
249.969869	50.622381	75.184372
249.076897	47.699123	75.189377
248.157455	48.437089	75.194382
247.635372	48.944556	75.199386
247.397583	48.134086	75.204391
246.150712	49.454110	75.209396
245.451150	53.194281	75.214401
245.244142	47.149657	75.219406
244.116579	49.384232	75.224410
243.277784	43.520746	75.229415
242.663989	54.498174	75.234420
242.314144	49.247459	75.239425
241.742707	43.626788	75.244430
240.832207	51.279940	75.249434
240.105579	42.935341	75.254439
239.151220	50.330553	75.259444
239.340149	50.505482	75.264449
239.121069	48.556610	75.269454
237.889890	49.076187	75.274458
237.459300	47.560005	75.279463
236.045615	55.250794	75.284468
235.213791	44.461308	75.289473
234.820240	44.295420	75.294478
233.998099	47.266646	75.299482
234.138212	44.166096	75.304487
233.270075	43.930781	75.309492
231.971348	44.319201	75.314497
231.495144	43.985138	75.319502
230.888566	50.285687	75.324506
230.811706	49.722382	75.329511
229.741687	47.735692	75.334516
229.056833	45.381671	75.339521
228.410537	47.626267	75.344526
228.022610	52.560996	75.349530
227.204127	47.580537	75.354535
226.033262	52.636922	75.359540
225.689410	56.287277	75.364545
225.145575	46.637770	75.369550
224.391878	49.781016	75.374554
223.656261	44.069826	75.379559
222.665242	49.733063	75.384564
222.695106	44.388707	75.389569
222.368010	46.139290	75.394574
221.138271	53.974229	75.399578
220.313684	43.478490	75.404583
219.792934	54.483667	75.409588
219.243660	53.110989	75.414593
218.532606	43.585916	75.419598
217.406519	45.154784	75.424602
217.106180	47.153417	75.429607
216.774435	49.791002	75.434612
216.136585	47.976701	75.439617
215.208546	47.251040	75.444622
213.990301	50.122990	75.449626
214.018134	37.971165	75.454631
213.569641	50.723145	75.459636
212.658734	45.069865	75.464641
211.791230	40.377930	75.469646
211.086893	49.149414	75.474650
210.906392	42.559670	75.479655
209.986294	47.153454	75.484660
209.322376	36.703076	75.489665
208.582758	49.533005	75.494670
208.034123	48.496124	75.499674
206.924456	43.850681	75.504679
206.187299	50.500062	75.509684
205.647414	46.104410	75.514689
205.261233	42.315045	75.519694
204.986474	51.306633	75.524698
203.977996	44.096670	75.529703
202.845648	59.040860	75.534708
202.342833	51.619391	75.539713
202.484296	52.601410	75.544718
201.458701	60.236656	75.549722
200.910113	49.290062	75.554727
199.746903	57.913932	75.559732
199.442232	44.301217	75.564737
198.972511	48.523580	75.569742
197.771366	54.119399	75.574746
197.542657	48.950308	75.579751
196.640973	51.722912	75.584756
196.062464	47.847513	75.589761
195.465373	52.366154	75.594766
194.526738	55.557818	75.599770
194.218811	40.718741	75.604775
193.396807	47.561425	75.609780
192.499301	53.927288	75.614785
191.905086	47.934941	75.619790
191.302852	47.920603	75.624794
191.087893	45.404946	75.629799
190.013286	58.256752	75.634804
189.509766	47.036471	75.639809
189.220523	50.845281	75.644814
188.314375	50.582925	75.649818
187.444107	49.081656	75.654823
186.455211	58.103523	75.659828
186.104812	57.001926	75.664833
185.901704	47.660814	75.669838
184.699496	52.572401	75.674842
184.193293	41.740488	75.679847
183.359895	57.291465	75.684852
182.962766	50.424017	75.689857
182.111435	51.160610	75.694862
181.253625	49.371925	75.699866
180.574070	48.007412	75.704871
180.044846	49.846997	75.709876
180.004654	49.353543	75.714881
179.180225	50.117387	75.719886
178.266998	48.332808	75.724890
177.753568	44.782934	75.729895
176.342098	50.675648	75.734900
175.761357	45.373450	75.739905
174.916340	42.789512	75.744910
174.165873	56.281933	75.749914
174.121838	48.028805	75.754919
173.810305	53.547456	75.759924
173.635684	46.770695	75.764929
172.891328	44.839344	75.769934
171.853678	51.317443	75.774938
171.157413	40.760269	75.779943
169.899048	55.617322	75.784948
169.446834	43.348067	75.789953
169.017385	52.165622	75.794958
168.429237	47.019150	75.799962
167.929805	42.077735	75.804967
166.720142	35.060721	75.809972
166.386059	41.426644	75.814977
166.000367	38.302692	75.819982
164.839798	52.022925	75.824986
163.994703	45.953891	75.829991
163.093273	47.445963	75.834996
162.841664	51.128926	75.840001
162.893609	53.066668	75.845006
161.707079	64.171699	75.850010
161.187212	51.946342	75.855015
160.348848	50.533038	75.860020
159.770839	53.545788	75.865025
159.422031	56.313835	75.870030
158.303647	58.070739	75.875034
157.648117	45.177882	75.880039
157.068469	61.806483	75.885044
156.264601	63.738750	75.890049
155.583002	52.076930	75.895054
154.664387	57.462139	75.900058
154.270131	52.544956	75.905063
153.897024	55.103986	75.910068
153.433847	55.822857	75.915073
152.522602	53.768308	75.920078
151.531980	54.675356	75.925082
151.624739	42.927927	75.930087
150.267820	59.196326	75.935092
149.914636	53.813695	75.940097
149.424239	47.636072	75.945102
148.255598	50.337715	75.950106
147.937501	49.838108	75.955111
146.725063	54.707189	75.960116
146.216839	45.920942	75.965121
145.956781	51.339922	75.970126
145.389827	57.452820	75.975130
144.791906	47.513914	75.980135
143.966283	54.117492	75.985140
143.337928	44.610801	75.990145
142.769169	52.241032	75.995150
141.583752	56.987534	76.000154
141.235586	46.505753	76.005159
140.605380	53.406183	76.010164
140.013673	42.726691	76.015169
139.170876	39.587318	76.020174
138.189435	48.958093	76.025178
138.089934	30.920825	76.030183
137.432485	47.016184	76.035188
136.937335	51.813476	76.040193
135.750727	43.625840	76.045198
135.076633	49.150262	76.050202
134.868514	37.641627	76.055207
133.746746	43.598555	76.060212
132.904609	45.693049	76.065217
132.754305	45.368543	76.070222
131.817712	47.359825	76.075226
131.588923	41.249307	76.080231
130.807656	46.207339	76.085236
129.859399	39.963957	76.090241
129.463812	47.050905	76.095246
128.612069	51.392541	76.100250
128.003089	45.976588	76.105255
127.114132	51.156799	76.110260
126.668267	49.242524	76.115265
126.117723	46.665265	76.120270
125.398570	45.220349	76.125274
124.625589	45.086596	76.130279
124.085423	45.316270	76.135284
123.436314	36.532001	76.140289
123.143281	31.480418	76.145294
121.851315	38.658254	76.150298
121.460878	37.979374	76.155303
121.081757	51.021497	76.160308
120.070543	40.266979	76.165313
119.148858	38.321345	76.170318
118.566279	49.760591	76.175322
118.179603	42.161357	76.180327
117.670395	43.674483	76.185332
116.574880	38.463851	76.190337
115.811316	41.422616	76.195342
115.339069	49.909526	76.200346
115.201485	45.158009	76.205351
113.986714	49.067098	76.210356
112.908553	46.004689	76.215361
112.896709	43.328918	76.220366
111.872120	45.526629	76.225370
111.899905	39.597556	76.230375
111.329669	50.897638	76.235380
110.429911	46.683978	76.240385
109.749162	40.262329	76.245390
108.575626	47.197361	76.250394
107.909806	36.687400	76.255399
107.153515	41.045358	76.260404
106.599426	45.194454	76.265409
106.347833	47.776690	76.270414
105.930586	38.406666	76.275418
105.072858	38.461477	76.280423
104.272776	38.828798	76.285428
103.760134	33.279221	76.290433
103.000112	39.621604	76.295438
101.587288	42.575095	76.300442
101.662675	38.584414	76.305447
101.130632	36.521460	76.310452
100.444205	41.243598	76.315457
99.861408	43.257322	76.320462
99.133063	43.606897	76.325466
98.659910	36.272200	76.330471
97.672622	46.306246	76.335476
96.891362	45.379028	76.340481
96.548813	37.673416	76.345486
95.472980	49.809494	76.350490
94.666346	44.144369	76.355495
93.931884	43.930366	76.360500
93.544953	40.529078	76.365505
93.442218	42.261244	76.370510
92.396494	47.080106	76.375514
91.431078	43.791568	76.380519
90.668786	51.209815	76.385524
90.184234	43.911627	76.390529
90.384561	43.165352	76.395534
88.756920	53.342522	76.400538
88.351533	35.962751	76.405543
87.886882	46.660939	76.410548
87.285721	45.723928	76.415553
86.403138	40.417853	76.420558
85.461589	41.764961	76.425562
85.062373	36.031718	76.430567
84.724481	43.533673	76.435572
83.661522	44.947452	76.440577
82.669488	48.759533	76.445582
82.157212	48.951653	76.450586
81.957634	39.442843	76.455591
81.490719	46.198967	76.460596
80.563553	46.788414	76.465601
79.821723	41.808406	76.470606
78.907730	44.672899	76.475610
78.884920	38.870169	76.480615
77.503891	42.165536	76.485620
76.661942	42.038066	76.490625
76.264049	36.809245	76.495630
75.708818	47.816774	76.500634
75.473278	36.036556	76.505639
74.673349	38.906513	76.510644
73.462882	39.315635	76.515649
73.063910	38.204457	76.520654
72.336736	41.936454	76.525658
72.243732	32.650355	76.530663
71.089963	47.153282	76.535668
70.163821	41.362146	76.540673
69.525050	43.227106	76.545678
69.330734	47.989046	76.550682
69.022987	38.260945	76.555687
67.941585	48.059271	76.560692
67.235382	48.443171	76.565697
66.914972	31.992890	76.570702
65.980031	39.577443	76.575706
64.827200	44.101156	76.580711
64.757070	45.826546	76.585716
64.129560	44.244031	76.590721
63.547298	41.982510	76.595726
62.191598	42.927314	76.600730
61.720516	38.823509	76.605735
61.277535	47.679498	76.610740
60.564380	46.309340	76.615745
60.478698	37.048880	76.620750
59.110374	48.528286	76.625754
58.659870	46.581648	76.630759
58.666909	43.688399	76.635764
57.284071	42.634782	76.640769
56.751553	39.089561	76.645774
56.035818	47.836083	76.650778
55.407722	37.329588	76.655783
54.461991	46.576419	76.660788
53.838464	46.434623	76.665793
53.671724	40.298453	76.670798
52.771364	54.857175	76.675802
51.826741	53.814097	76.680807
51.315225	36.990588	76.685812
50.465445	37.870482	76.690817
50.265709	43.481696	76.695822
49.172296	44.558144	76.700826
48.922086	42.738839	76.705831
48.370745	33.213600	76.710836
47.899967	42.296372	76.715841
46.772920	32.665829	76.720846
45.796154	42.136807	76.725850
45.424973	48.399846	76.730855
45.050335	33.989357	76.735860
43.988924	40.933337	76.740865
43.245311	38.964064	76.745870
42.768502	47.339742	76.750874
42.340333	37.547273	76.755879
41.981909	43.004021	76.760884
40.273994	39.966391	76.765889
40.319687	38.964074	76.770894
39.281099	50.868723	76.775898
39.025022	40.693988	76.780903
37.887859	41.567681	76.785908
36.882577	47.455608	76.790913
36.840524	48.613542	76.795918
36.069262	44.177567	76.800922
35.844125	40.187508	76.805927
35.326057	43.255377	76.810932
34.269492	36.805385	76.815937
33.620280	39.941480	76.820942
33.206297	42.013451	76.825946
32.134381	48.976462	76.830951
31.288188	40.901753	76.835956
30.703207	42.977343	76.840961
30.616529	37.724127	76.845966
29.157247	49.293748	76.850970
28.614494	35.517208	76.855975
27.889448	30.219152	76.860980
27.376383	44.260354	76.865985
27.339275	32.995710	76.870990
26.351741	38.019781	76.875994
25.715441	38.923983	76.880999
24.829743	38.950166	76.886004
24.403279	45.168406	76.891009
23.788533	36.869129	76.896014
22.748870	40.725098	76.901018
22.345433	30.569146	76.906023
21.925137	36.089378	76.911028
21.054705	40.165939	76.916033
20.277808	32.067572	76.921038
19.474569	35.515244	76.926042
19.202779	35.634327	76.931047
18.785968	38.356462	76.936052
17.671861	37.867139	76.941057
16.840101	33.970685	76.946062
16.269610	40.092046	76.951066
15.904371	35.006266	76.956071
15.005336	39.301858	76.961076
13.937068	39.723022	76.966081
13.789827	38.661591	76.971086
13.275538	38.600154	76.976090
12.886653	38.513984	76.981095
11.735329	43.909543	76.986100
10.935165	41.540864	76.991105
10.434042	36.350601	76.996110
9.638262	44.621036	77.001114
9.022451	38.039255	77.006119
8.620366	38.234314	77.011124
8.116647	44.392337	77.016129
7.405631	38.975352	77.021134
6.155677	39.685698	77.026139
5.693858	39.115994	77.031143
5.075127	40.686034	77.036148
4.340315	40.509961	77.041153
4.239294	37.279133	77.046158