Fri Mar 05 18:38:36 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.577605	106.549005	0.000000
-1.718585	84.571127	0.005005
-2.532909	60.284765	0.010010
-4.925674	28.565650	0.015014
-8.961924	9.161489	0.020019
-14.276340	11.179284	0.025024
-19.168315	9.830698	0.030029
-23.652519	8.773471	0.035034
-27.357483	17.324978	0.040038
-30.825794	11.523056	0.045043
-35.303538	18.532571	0.050048
-38.606636	13.041776	0.055053
-42.239333	16.300523	0.060058
-46.015526	17.645654	0.065062
-49.613351	7.828969	0.070067
-53.433965	18.843257	0.075072
-57.079806	10.570206	0.080077
-60.905564	9.974139	0.085082
-64.993805	18.891198	0.090086
-68.422389	14.784538	0.095091
-72.560121	21.367714	0.100096
-76.307092	11.784599	0.105101
-79.576371	16.989745	0.110106
-83.418791	19.190752	0.115110
-86.962241	7.403708	0.120115
-91.267652	17.459329	0.125120
-94.955968	8.546561	0.130125
-98.931737	10.089195	0.135130
-102.831700	15.276719	0.140134
-106.069793	8.720662	0.145139
-109.917772	16.801515	0.150144
-113.773201	10.457504	0.155149
-117.326369	8.453962	0.160154
-121.204342	18.105543	0.165158
-125.014002	6.988666	0.170163
-128.893232	18.881323	0.175168
-132.262739	9.075649	0.180173
-135.799496	5.133007	0.185178
-140.050094	10.914278	0.190182
-143.785779	-1.810249	0.195187
-147.693213	8.054225	0.200192
-151.892769	6.067142	0.205197
-155.639801	2.415129	0.210202
-159.283397	7.289016	0.215206
-162.663417	8.418145	0.220211
-166.686899	8.927708	0.225216
-170.374239	9.087169	0.230221
-174.120996	8.268940	0.235226
-177.610741	12.383441	0.240230
-180.986352	8.766814	0.245235
-185.157816	20.002863	0.250240
-189.135599	16.349875	0.255245
-192.949045	7.755280	0.260250
-196.649492	15.327016	0.265254
-199.968058	4.833646	0.270259
-204.219134	10.741259	0.275264
-207.782415	20.322250	0.280269
-211.691886	17.637691	0.285274
-215.426929	16.841310	0.290278
-218.904019	12.040864	0.295283
-222.850034	18.428108	0.300288
-226.664462	17.712224	0.305293
-230.427405	14.266293	0.310298
-234.371172	21.459025	0.315302
-237.692518	26.456644	0.320307
-241.439651	24.154657	0.325312
-245.449237	19.527545	0.330317
-249.011008	22.335304	0.335322
-253.092728	15.316430	0.340326
-256.773965	11.086368	0.345331
-260.450931	14.082841	0.350336
-264.063732	12.339772	0.355341
-267.571107	15.962049	0.360346
-272.149260	18.482634	0.365350
-275.694659	3.725213	0.370355
-279.592682	16.264489	0.375360
-283.049789	10.811242	0.380365
-286.725950	8.766085	0.385370
-290.543595	16.935409	0.390374
-294.098325	8.446344	0.395379
-298.074084	11.591492	0.400384
-301.689931	19.708121	0.405389
-305.600500	5.647707	0.410394
-309.734954	11.024372	0.415398
-313.400614	4.035390	0.420403
-316.738309	8.494821	0.425408
-320.784580	11.220752	0.430413
-324.457771	13.644281	0.435418
-328.350480	14.149007	0.440422
-331.852553	4.930928	0.445427
-335.382556	18.485446	0.450432
-339.351442	5.711739	0.455437
-343.111021	6.934829	0.460442
-347.317425	14.836716	0.465446
-351.010262	6.316174	0.470451
-354.771967	12.492848	0.475456
-358.306752	5.923014	0.480461
-361.990576	19.885328	0.485466
-365.893111	16.037698	0.490470
-369.459346	19.439281	0.495475
-373.353104	17.387996	0.500480
-376.981006	18.591693	0.505485
-380.748164	8.320024	0.510490
-384.781190	21.000863	0.515494
-388.256353	7.714750	0.520499
-392.419496	14.966406	0.525504
-395.961756	17.561527	0.530509
-399.425257	6.728896	0.535514
-403.833582	12.162061	0.540518
-406.886530	11.659196	0.545523
-410.757350	14.645845	0.550528
-414.543858	8.103676	0.555533
-418.445217	10.976941	0.560538
-422.729077	24.289252	0.565542
-425.944099	5.666237	0.570547
-429.774186	10.488297	0.575552
-433.524468	15.046885	0.580557
-437.072835	10.125685	0.585562
-441.166988	12.298065	0.590566
-444.517691	9.389049	0.595571
-448.609920	15.143981	0.600576
-452.689080	12.352879	0.605581
-456.036362	5.933028	0.610586
-459.938665	12.097619	0.615590
-464.032764	6.661213	0.620595
-467.606451	11.850819	0.625600
-470.935331	10.081650	0.630605
-474.597930	4.011804	0.635610
-478.807089	13.825620	0.640614
-482.630385	0.853883	0.645619
-486.338372	9.972659	0.650624
-489.850622	10.246574	0.655629
-493.473089	3.154790	0.660634
-497.720222	16.122307	0.665638
-500.699694	13.267623	0.670643
-504.650170	14.554569	0.675648
-509.032302	8.979741	0.680653
-512.705614	10.921024	0.685658
-516.553961	5.454924	0.690662
-520.316798	8.208457	0.695667
-524.159473	14.144429	0.700672
-527.645596	16.907394	0.705677
-531.158677	6.598554	0.710682
-535.294674	13.954921	0.715686
-538.656540	5.794986	0.720691
-542.598436	13.011552	0.725696
-546.578660	12.146043	0.730701
-549.731364	8.117454	0.735706
-554.057452	18.175579	0.740710
-557.738611	3.206918	0.745715
-561.645652	11.294733	0.750720
-565.213688	13.168817	0.755725
-568.767991	9.120825	0.760730
-572.766136	10.820775	0.765734
-576.631791	9.689434	0.770739
-580.114220	11.423709	0.775744
-583.953985	16.831030	0.780749
-587.767353	11.886162	0.785754
-591.649224	11.435526	0.790758
-594.995463	8.808289	0.795763
-599.302228	7.812107	0.800768
-603.069517	8.628404	0.805773
-606.298852	8.581327	0.810778
-610.567534	9.381541	0.815782
-614.067585	10.943638	0.820787
-617.717090	18.102575	0.825792
-621.760429	4.604836	0.830797
-625.428201	9.074839	0.835802
-629.327203	11.720986	0.840806
-632.812271	10.984673	0.845811
-636.696475	11.185766	0.850816
-640.630826	15.116487	0.855821
-644.341226	6.417884	0.860826
-648.134552	5.689844	0.865830
-651.458418	0.813534	0.870835
-655.429604	4.770663	0.875840
-658.894955	7.125220	0.880845
-662.650829	5.520741	0.885850
-666.866412	18.248530	0.890854
-670.730207	1.333325	0.895859
-674.565764	16.665453	0.900864
-678.140743	9.181598	0.905869
-681.556523	9.744734	0.910874
-685.679283	15.279433	0.915878
-689.353154	8.394870	0.920883
-693.246830	9.543741	0.925888
-697.001123	10.725539	0.930893
-700.457074	1.737214	0.935898
-704.406689	13.304502	0.940902
-707.986265	-0.694532	0.945907
-711.877780	5.385150	0.950912
-715.829084	12.674456	0.955917
-719.517726	1.244377	0.960922
-723.466658	5.289524	0.965926
-727.058223	12.705864	0.970931
-730.648325	9.468088	0.975936
-734.529330	8.008300	0.980941
-737.875638	8.584069	0.985946
-741.680638	22.307657	0.990950
-745.580131	17.469854	0.995955
-749.700772	15.504338	1.000960
-753.633496	14.776667	1.005965
-757.033996	1.318373	1.010970
-760.928275	12.580438	1.015974
-764.439357	1.404331	1.020979
-768.306483	11.102462	1.025984
-772.167658	13.184554	1.030989
-775.818145	7.680959	1.035994
-780.099665	19.173682	1.040998
-783.632873	12.880223	1.046003
-787.042119	11.414507	1.051008
-790.830339	25.185951	1.056013
-794.356237	10.711692	1.061018
-798.419161	16.818912	1.066022
-802.243321	14.440249	1.071027
-806.175379	17.566628	1.076032
-809.791430	18.955166	1.081037
-813.337532	6.455362	1.086042
-817.307818	10.396844	1.091046
-820.895520	14.658802	1.096051
-824.648136	10.300706	1.101056
-828.572704	16.590864	1.106061
-832.342798	7.183026	1.111066
-836.249235	9.643039	1.116070
-840.121283	7.973837	1.121075
-843.577773	9.256495	1.126080
-847.510411	12.709463	1.131085
-850.641511	17.614410	1.136090
-854.989750	17.511572	1.141094
-858.459859	9.393077	1.146099
-862.248097	10.416559	1.151104
-866.073125	10.982306	1.156109
-869.795676	12.070993	1.161114
-873.932108	10.603385	1.166118
-877.295849	6.279403	1.171123
-881.158411	5.578577	1.176128
-885.068331	8.195344	1.181133
-888.540387	0.575527	1.186138
-892.580187	12.873459	1.191142
-896.077226	7.884842	1.196147
-899.754428	15.077004	1.201152
-903.944254	4.085330	1.206157
-907.397216	8.729571	1.211162
-911.453424	2.680785	1.216166
-915.077140	6.664787	1.221171
-918.480910	5.821284	1.226176
-922.457077	14.985156	1.231181
-926.144129	16.189681	1.236186
-930.244652	10.815060	1.241190
-933.828790	10.744738	1.246195
-937.633041	-1.038645	1.251200
-941.721185	19.473534	1.256205
-945.338742	4.391294	1.261210
-948.866973	14.543293	1.266214
-952.116476	9.083098	1.271219
-956.362609	16.186544	1.276224
-960.230950	11.907100	1.281229
-964.009729	14.140329	1.286234
-968.220569	25.912232	1.291238
-971.419309	-4.298361	1.296243
-974.877858	11.547921	1.301248
-978.811215	9.899793	1.306253
-982.550896	7.586768	1.311258
-986.688490	20.703159	1.316262
-990.200526	8.029465	1.321267
-993.875400	7.185271	1.326272
-998.182453	15.642090	1.331277
-1001.391120	8.953302	1.336282
-1005.364195	12.405110	1.341286
-1009.062745	5.249054	1.346291
-1012.905000	10.359401	1.351296
-1016.719365	5.207256	1.356301
-1020.156870	8.141352	1.361306
-1024.127349	9.763517	1.366310
-1027.966721	13.633948	1.371315
-1031.446711	10.413725	1.376320
-1035.542432	12.639410	1.381325
-1039.179252	13.616882	1.386330
-1042.863846	16.160025	1.391334
-1046.839362	15.463346	1.396339
-1050.630597	9.832896	1.401344
-1054.657543	15.233046	1.406349
-1057.754985	-6.116962	1.411354
-1061.490237	0.576943	1.416358
-1065.199980	1.821584	1.421363
-1069.027078	10.977614	1.426368
-1073.190696	17.572904	1.431373
-1076.951278	7.050641	1.436378
-1080.842034	3.087225	1.441382
-1084.112037	-1.729255	1.446387
-1087.936710	11.945940	1.451392
-1091.993798	15.860761	1.456397
-1095.703345	10.803944	1.461402
-1099.256065	12.928688	1.466406
-1102.820265	3.240801	1.471411
-1106.806457	4.413036	1.476416
-1110.977385	10.489166	1.481421
-1113.958038	0.157598	1.486426
-1118.154545	24.550899	1.491430
-1122.064560	13.754570	1.496435
-1125.612016	6.565075	1.501440
-1129.315582	1.261357	1.506445
-1132.969625	3.017586	1.511450
-1137.459692	9.698324	1.516454
-1141.024997	8.190287	1.521459
-1144.611742	12.417879	1.526464
-1148.153732	-0.881533	1.531469
-1151.478906	2.252399	1.536474
-1155.727028	1.563250	1.541478
-1159.406062	1.981540	1.546483
-1163.491016	2.646126	1.551488
-1167.441129	7.031234	1.556493
-1170.588005	4.831828	1.561498
-1174.200468	8.942154	1.566502
-1178.307914	-2.049553	1.571507
-1182.342014	1.934279	1.576512
-1186.114041	9.955740	1.581517
-1189.618111	4.509816	1.586522
-1193.313520	16.551277	1.591526
-1196.814492	4.267238	1.596531
-1200.758462	7.017705	1.601536
-1204.634621	1.314376	1.606541
-1208.706827	-2.922558	1.611546
-1212.180835	9.351579	1.616550
-1216.188031	7.188973	1.621555
-1219.836850	4.793987	1.626560
-1223.734891	11.130997	1.631565
-1226.815015	10.097386	1.636570
-1230.763113	3.401100	1.641574
-1235.018949	12.291682	1.646579
-1238.622569	4.545235	1.651584
-1242.242430	20.338842	1.656589
-1245.946444	4.963450	1.661594
-1249.964738	18.783417	1.666598
-1253.600495	10.282047	1.671603
-1257.055144	15.843263	1.676608
-1261.141065	4.387796	1.681613
-1264.668829	3.766493	1.686618
-1268.469756	5.516477	1.691622
-1272.191218	3.079586	1.696627
-1276.152058	12.940156	1.701632
-1280.012112	16.852149	1.706637
-1283.783403	3.707928	1.711642
-1287.372680	12.966583	1.716646
-1291.028668	8.650566	1.721651
-1294.925882	13.371193	1.726656
-1298.930382	1.303531	1.731661
-1302.517365	7.734383	1.736666
-1306.621033	10.732936	1.741670
-1310.253244	7.867085	1.746675
-1313.583221	10.029041	1.751680
-1317.275775	10.976442	1.756685
-1320.641499	-2.019734	1.761690
-1325.153497	11.269090	1.766694
-1328.910783	7.022965	1.771699
-1332.616950	3.631252	1.776704
-1336.383899	9.479108	1.781709
-1339.870581	1.056527	1.786714
-1343.868784	4.796771	1.791718
-1347.672741	11.066881	1.796723
-1351.356524	8.772319	1.801728
-1355.525224	15.042481	1.806733
-1358.786310	4.954836	1.811738
-1362.234865	5.614095	1.816742
-1366.353794	7.809377	1.821747
-1369.919220	1.553551	1.826752
-1373.876091	11.235447	1.831757
-1377.525755	7.221332	1.836762
-1381.380624	3.066611	1.841766
-1385.067242	8.996299	1.846771
-1388.845609	6.436245	1.851776
-1393.138262	10.786678	1.856781
-1396.354641	0.330818	1.861786
-1400.081752	7.260483	1.866790
-1404.257909	7.733515	1.871795
-1407.738343	-3.657754	1.876800
-1411.643617	1.625741	1.881805
-1414.934045	-4.511612	1.886810
-1419.195843	2.014832	1.891814
-1422.882604	0.069368	1.896819
-1426.687688	10.422478	1.901824
-1430.278437	8.515269	1.906829
-1433.725470	1.281811	1.911834
-1437.845699	6.535111	1.916838
-1441.669898	7.495903	1.921843
-1445.431760	-4.088362	1.926848
-1449.381988	14.961184	1.931853
-1452.599881	1.654544	1.936858
-1456.951201	5.476750	1.941862
-1460.241099	3.986614	1.946867
-1464.203489	9.233612	1.951872
-1468.119325	8.772530	1.956877
-1471.582577	5.730076	1.961882
-1475.750757	7.457202	1.966886
-1479.033751	8.444936	1.971891
-1482.987660	9.052831	1.976896
-1486.680927	13.693807	1.981901
-1490.210169	6.541408	1.986906
-1494.671341	15.377016	1.991910
-1498.060262	-6.512242	1.996915
-1502.307092	6.951313	2.006912
-1502.788345	9.726818	2.016909
-1500.118873	13.452000	2.026906
-1497.404359	13.724686	2.036902
-1495.435689	8.696250	2.046899
-1493.461411	11.089595	2.056896
-1491.723958	8.510834	2.066893
-1489.591455	8.126723	2.076890
-1487.930782	4.747097	2.086886
-1486.016285	9.982671	2.096883
-1483.859764	6.321541	2.106880
-1482.114531	6.807876	2.116877
-1480.051025	3.756912	2.126874
-1478.340488	12.934651	2.136870
-1476.625121	8.723637	2.146867
-1474.610186	8.576262	2.156864
-1472.682580	6.469175	2.166861
-1470.686758	9.732254	2.176858
-1468.533733	5.659590	2.186854
-1467.105217	10.076149	2.196851
-1465.210185	7.427965	2.206848
-1463.237200	10.055230	2.216845
-1461.366515	13.853096	2.226842
-1459.214514	7.909538	2.236838
-1457.370563	12.000636	2.246835
-1455.968892	10.874622	2.256832
-1453.769548	9.060359	2.266829
-1452.165148	8.606103	2.276826
-1449.683747	13.114620	2.286822
-1447.958426	6.626754	2.296819
-1446.368550	14.854361	2.306816
-1444.258046	11.101159	2.316813
-1442.412743	9.812543	2.326810
-1440.557746	9.755543	2.336806
-1438.716463	14.638143	2.346803
-1436.732462	13.418904	2.356800
-1435.024952	7.311269	2.366797
-1432.856917	9.512593	2.376794
-1431.304287	8.499793	2.386790
-1429.430591	7.233484	2.396787
-1427.476787	6.789620	2.406784
-1425.632869	6.748616	2.416781
-1423.612662	7.178340	2.426778
-1421.334372	6.322528	2.436774
-1419.984244	11.820624	2.446771
-1418.269494	19.518259	2.456768
-1416.113116	10.496644	2.466765
-1414.141786	10.689464	2.476762
-1412.361309	12.993908	2.486758
-1410.275051	7.741449	2.496755
-1408.719313	9.770821	2.506752
-1406.793947	7.694146	2.516749
-1404.865294	9.235921	2.526746
-1403.107664	21.919374	2.536742
-1400.977187	17.100371	2.546739
-1399.456910	10.717994	2.556736
-1397.052010	1.969248	2.566733
-1395.245652	4.525352	2.576730
-1393.646598	9.633085	2.586726
-1391.877471	13.687270	2.596723
-1389.768360	9.755917	2.606720
-1387.727187	12.280754	2.616717
-1386.116468	9.633936	2.626714
-1384.307688	9.979119	2.636710
-1382.854699	15.422879	2.646707
-1380.372091	18.947592	2.656704
-1378.014530	9.150114	2.666701
-1376.530739	8.363109	2.676698
-1374.887044	9.738945	2.686694
-1372.904390	10.856836	2.696691
-1371.191054	11.889946	2.706688
-1369.157736	9.660230	2.716685
-1367.064952	15.153164	2.726682
-1365.258922	12.745097	2.736678
-1363.591959	14.532483	2.746675
-1361.504903	10.509947	2.756672
-1359.858513	11.766941	2.766669
-1358.142995	10.983907	2.776666
-1355.878779	10.016727	2.786662
-1354.226490	13.445430	2.796659
-1352.381489	15.828016	2.806656
-1350.296380	12.590544	2.816653
-1348.160674	12.194998	2.826650
-1346.677235	10.026478	2.836646
-1344.710691	15.441745	2.846643
-1342.865379	18.785877	2.856640
-1340.938204	11.818924	2.866637
-1339.173608	11.632790	2.876634
-1337.359773	12.670366	2.886630
-1335.542797	16.322199	2.896627
-1333.571182	11.872897	2.906624
-1331.283791	15.577333	2.916621
-1329.833105	11.986685	2.926618
-1327.842279	10.349601	2.936614
-1326.017491	15.820733	2.946611
-1324.125861	15.416907	2.956608
-1322.131059	14.004982	2.966605
-1320.141054	7.681681	2.976602
-1318.404063	15.525838	2.986598
-1316.763294	15.143223	2.996595
-1314.908091	15.121028	3.006592
-1312.591044	14.751755	3.016589
-1310.861109	16.325416	3.026586
-1309.379231	15.958763	3.036582
-1307.297397	11.417631	3.046579
-1305.202274	8.803865	3.056576
-1303.357127	18.160739	3.066573
-1301.661132	19.992474	3.076570
-1299.317359	14.956262	3.086566
-1297.811459	12.637334	3.096563
-1296.167209	13.498398	3.106560
-1294.159589	16.563959	3.116557
-1292.089696	17.041111	3.126554
-1290.182346	16.821115	3.136550
-1288.414981	18.399856	3.146547
-1286.520053	11.403368	3.156544
-1284.827988	12.192050	3.166541
-1282.816733	13.692288	3.176538
-1280.837221	10.746516	3.186534
-1279.111450	14.392465	3.196531
-1277.066951	13.357892	3.206528
-1275.095923	16.064586	3.216525
-1273.487319	9.003404	3.226522
-1271.444209	7.763793	3.236518
-1269.609489	9.202294	3.246515
-1267.998269	6.844425	3.256512
-1265.826757	17.900171	3.266509
-1263.854026	10.951250	3.276506
-1262.086297	6.417792	3.286502
-1260.492312	15.639633	3.296499
-1258.531830	17.590128	3.306496
-1256.389835	11.229920	3.316493
-1254.785694	2.726297	3.326490
-1252.650040	12.183566	3.336486
-1250.596876	13.343965	3.346483
-1248.959582	14.660918	3.356480
-1247.322925	23.091201	3.366477
-1245.524728	16.781280	3.376474
-1243.183633	8.807103	3.386470
-1241.400360	15.410750	3.396467
-1239.635182	11.545617	3.406464
-1237.790157	20.087826	3.416461
-1236.072824	9.267127	3.426458
-1234.019817	12.293899	3.436454
-1232.307555	12.904123	3.446451
-1230.294412	12.801459	3.456448
-1228.292850	14.388560	3.466445
-1226.244630	17.517160	3.476442
-1224.409965	13.910921	3.486438
-1222.804848	15.548833	3.496435
-1220.977196	18.971683	3.506432
-1219.141328	17.326326	3.516429
-1216.923812	6.442973	3.526426
-1215.254394	8.687975	3.536422
-1213.354613	11.892444	3.546419
-1211.591056	12.293947	3.556416
-1209.927534	11.342498	3.566413
-1207.692209	7.981640	3.576410
-1205.686925	10.586596	3.586406
-1203.913321	10.610704	3.596403
-1202.132323	19.049505	3.606400
-1200.019287	12.722400	3.616397
-1198.271732	8.277479	3.626394
-1196.615936	10.728361	3.636390
-1194.525569	14.409199	3.646387
-1192.629006	8.271477	3.656384
-1190.927770	11.744576	3.666381
-1188.875846	12.619437	3.676378
-1186.926037	15.279077	3.686374
-1185.519968	14.466733	3.696371
-1183.594240	18.196029	3.706368
-1181.333663	11.543752	3.716365
-1179.484465	10.148928	3.726362
-1177.687990	12.792056	3.736358
-1175.592946	14.754251	3.746355
-1173.999720	16.979896	3.756352
-1172.151359	10.895690	3.766349
-1170.151196	8.643028	3.776346
-1168.361909	8.910973	3.786342
-1166.654280	17.877862	3.796339
-1164.627670	11.182506	3.806336
-1162.518059	9.758663	3.816333
-1160.683330	9.889869	3.826330
-1159.186724	11.894138	3.836326
-1157.023516	11.418577	3.846323
-1155.217937	15.437123	3.856320
-1153.296857	8.539184	3.866317
-1151.259690	8.205373	3.876314
-1149.564195	11.418894	3.886310
-1147.869329	13.171976	3.896307
-1145.587192	12.762664	3.906304
-1143.857844	13.769698	3.916301
-1141.826183	17.109448	3.926298
-1140.136807	13.867571	3.936294
-1138.584738	17.906161	3.946291
-1136.531937	18.728823	3.956288
-1134.307288	15.123421	3.966285
-1132.723854	6.029490	3.976282
-1130.663279	14.805732	3.986278
-1128.788898	11.876903	3.996275
-1127.302369	11.346989	4.006272
-1125.298447	14.256975	4.016269
-1123.295918	13.203986	4.026266
-1121.271376	3.335280	4.036262
-1119.381445	11.339875	4.046259
-1117.612239	13.722146	4.056256
-1115.734607	11.054915	4.066253
-1114.068704	5.937846	4.076250
-1111.897891	11.015906	4.086246
-1110.055162	11.149030	4.096243
-1108.300011	8.079815	4.106240
-1106.775618	10.550204	4.116237
-1104.378533	12.217830	4.126234
-1102.561982	8.088786	4.136230
-1100.743388	11.925291	4.146227
-1099.031759	13.754676	4.156224
-1096.932439	9.967250	4.166221
-1095.086049	9.777691	4.176218
-1093.224660	10.174688	4.186214
-1091.392899	13.860673	4.196211
-1089.638001	11.562046	4.206208
-1087.487646	10.295965	4.216205
-1085.626748	9.153556	4.226202
-1083.545914	-0.589911	4.236198
-1082.280933	8.308899	4.246195
-1080.239767	3.629201	4.256192
-1078.272854	8.608854	4.266189
-1076.588206	4.000396	4.276186
-1074.146517	1.416663	4.286182
-1072.672872	5.445735	4.296179
-1070.800246	5.234630	4.306176
-1068.939911	10.212392	4.316173
-1066.901810	8.048485	4.326170
-1064.805205	1.820443	4.336166
-1063.330553	9.386241	4.346163
-1061.746751	9.636608	4.356160
-1059.253687	9.271012	4.366157
-1057.547680	4.532833	4.376154
-1055.942609	5.744550	4.386150
-1053.984899	10.531485	4.396147
-1052.006549	12.270876	4.406144
-1050.011140	11.487512	4.416141
-1048.256917	14.745403	4.426138
-1046.168223	8.711272	4.436134
-1044.582356	13.505584	4.446131
-1042.706137	10.922320	4.456128
-1040.485201	4.382303	4.466125
-1038.646429	3.489789	4.476122
-1036.780860	6.145661	4.486118
-1035.081986	7.765553	4.496115
-1033.288951	8.891959	4.506112
-1031.533021	8.685339	4.516109
-1029.726969	6.094361	4.526106
-1027.379253	11.223161	4.536102
-1025.515662	2.419229	4.546099
-1023.771086	9.771358	4.556096
-1022.088151	8.842200	4.566093
-1019.761561	11.875941	4.576090
-1018.320215	5.741678	4.586086
-1016.384616	8.135312	4.596083
-1014.524719	10.072103	4.606080
-1012.811761	6.730227	4.616077
-1010.571931	7.886251	4.626074
-1008.578483	7.373239	4.636070
-1006.970064	13.018191	4.646067
-1005.374284	14.558276	4.656064
-1003.222253	10.440390	4.666061
-1001.193874	13.555000	4.676058
-999.529263	12.646157	4.686054
-997.605083	15.610063	4.696051
-995.577094	13.321516	4.706048
-993.972218	14.776469	4.716045
-991.741102	6.343263	4.726042
-990.061445	4.885698	4.736038
-988.194157	9.685573	4.746035
-986.167918	0.467234	4.756032
-984.430665	2.564188	4.766029
-982.454749	8.388813	4.776026
-980.703540	7.805613	4.786022
-978.982697	5.457249	4.796019
-977.123424	9.159454	4.806016
-975.031040	7.864851	4.816013
-972.825997	2.655346	4.826010
-971.184446	5.366042	4.836006
-969.338480	12.237789	4.846003
-967.781779	3.812974	4.856000
-965.697468	10.076604	4.865997
-964.026214	9.605676	4.875994
-961.713272	6.712639	4.885990
-959.943732	10.659737	4.895987
-958.158986	8.768543	4.905984
-955.985143	7.129348	4.915981
-954.266060	12.851382	4.925978
-952.814690	15.933562	4.935974
-950.858155	2.813712	4.945971
-948.828522	10.185061	4.955968
-946.929824	7.539856	4.965965
-945.184017	1.158002	4.975962
-942.967386	8.591036	4.985958
-941.146723	6.591479	4.995955
-939.417688	9.799797	5.005952
-937.499325	4.546160	5.015949
-935.452028	7.545695	5.025946
-933.807769	5.650140	5.035942
-932.039208	12.887985	5.045939
-929.827620	7.457993	5.055936
-927.997581	5.022731	5.065933
-926.533634	12.798764	5.075930
-924.372757	10.762192	5.085926
-922.313508	14.364575	5.095923
-920.924634	10.889839	5.105920
-918.910710	12.116810	5.115917
-916.621248	11.682864	5.125914
-914.730542	9.599495	5.135910
-913.025335	6.519458	5.145907
-911.469612	10.415515	5.155904
-909.430187	12.478428	5.165901
-907.474102	4.712960	5.175898
-905.521566	10.956663	5.185894
-903.611744	13.272410	5.195891
-902.050973	7.240696	5.205888
-899.870968	11.188534	5.215885
-898.124395	14.420923	5.225882
-896.116752	8.530929	5.235878
-894.508845	10.951794	5.245875
-892.400311	15.432127	5.255872
-890.486294	8.006558	5.265869
-888.644310	5.492047	5.275866
-886.817165	3.418862	5.285862
-885.151928	5.025295	5.295859
-883.133974	4.671104	5.305856
-881.106767	3.841746	5.315853
-879.330408	2.814068	5.325850
-877.433821	6.140912	5.335846
-875.459480	-0.334273	5.345843
-873.823090	12.075342	5.355840
-872.165991	6.636150	5.365837
-869.967327	11.296306	5.375834
-867.884308	3.512155	5.385830
-866.257321	5.776830	5.395827
-864.538714	7.900543	5.405824
-862.371568	2.844037	5.415821
-860.487629	6.079758	5.425818
-858.789281	-0.248661	5.435814
-856.978855	0.335095	5.445811
-854.958315	7.772723	5.455808
-852.909743	8.370519	5.465805
-851.096831	2.859065	5.475802
-849.539455	4.154340	5.485798
-847.428966	8.013866	5.495795
-845.512597	10.301771	5.505792
-843.950682	12.185281	5.515789
-841.872378	12.178326	5.525786
-839.814755	5.513009	5.535782
-838.006505	3.659200	5.545779
-836.158508	10.347576	5.555776
-834.366757	2.887910	5.565773
-832.232574	8.039996	5.575770
-830.716576	6.100275	5.585766
-828.639696	4.890385	5.595763
-826.748480	5.208615	5.605760
-825.011331	3.355129	5.615757
-823.002403	4.597191	5.625754
-821.361279	7.161222	5.635750
-819.340765	11.800957	5.645747
-817.536053	4.694498	5.655744
-815.733133	13.842237	5.665741
-813.356118	9.949085	5.675738
-811.548326	10.575930	5.685734
-809.908310	7.675334	5.695731
-808.080534	8.783731	5.705728
-806.178899	13.410900	5.715725
-804.126359	9.166983	5.725722
-802.326276	10.620869	5.735718
-800.754707	13.398141	5.745715
-798.842158	11.472426	5.755712
-796.873392	10.346161	5.765709
-795.060779	7.699043	5.775706
-793.053176	9.197137	5.785702
-790.996147	14.424755	5.795699
-789.341204	11.398626	5.805696
-787.496838	16.047597	5.815693
-785.503610	13.722150	5.825690
-783.422246	16.637432	5.835686
-781.679133	13.990379	5.845683
-780.130355	16.073404	5.855680
-778.138634	14.975064	5.865677
-776.061414	14.524649	5.875674
-773.893630	15.651365	5.885670
-772.554082	11.968275	5.895667
-770.442860	11.706645	5.905664
-768.754338	9.770968	5.915661
-766.495293	4.193008	5.925658
-764.900001	15.889276	5.935654
-763.198729	11.935219	5.945651
-761.187039	11.670556	5.955648
-759.454570	10.869459	5.965645
-757.117763	11.741805	5.975642
-755.377411	11.357877	5.985638
-753.782921	10.968841	5.995635
-751.892724	13.256271	6.005632
-749.911338	13.735420	6.015629
-747.905441	12.735893	6.025626
-746.102430	9.706656	6.035622
-744.196757	9.594742	6.045619
-742.634214	9.919777	6.055616
-740.932818	13.587409	6.065613
-738.377357	14.047457	6.075610
-736.383928	6.416676	6.085606
-734.928691	12.259998	6.095603
-732.997548	16.792515	6.105600
-731.179803	12.631969	6.115597
-729.378212	7.193462	6.125594
-727.306316	7.392898	6.135590
-725.409978	15.699987	6.145587
-723.773024	10.486742	6.155584
-721.685789	14.602739	6.165581
-719.689862	14.629582	6.175578
-717.900422	8.187220	6.185574
-716.178075	7.626195	6.195571
-714.474936	9.177747	6.205568
-712.410523	10.019455	6.215565
-710.037720	5.542857	6.225562
-708.618444	9.811393	6.235558
-706.805351	5.844244	6.245555
-705.071916	7.133589	6.255552
-702.867648	5.143967	6.265549
-701.203561	8.388110	6.275546
-699.097676	9.366888	6.285542
-697.254257	7.565986	6.295539
-695.518989	6.268691	6.305536
-693.403975	10.756069	6.315533
-691.806998	5.291862	6.325530
-689.862920	8.396536	6.335526
-688.046836	5.205777	6.345523
-686.188746	15.814837	6.355520
-684.179767	10.404802	6.365517
-682.363992	9.031493	6.375514
-680.317548	5.923934	6.385510
-678.436411	12.498202	6.395507
-676.737243	9.755612	6.405504
-674.835600	9.914402	6.415501
-673.175587	10.045485	6.425498
-670.949156	4.783879	6.435494
-669.081386	-0.133044	6.445491
-667.340160	6.086211	6.455488
-665.249619	6.565358	6.465485
-663.732200	9.109794	6.475482
-661.894174	6.405030	6.485478
-659.930585	11.346115	6.495475
-657.825828	15.044102	6.505472
-656.116798	12.513112	6.515469
-654.176720	11.424705	6.525466
-652.270022	15.482768	6.535462
-650.410125	15.526667	6.545459
-648.481054	12.807365	6.555456
-646.715408	9.482587	6.565453
-644.806052	5.992742	6.575450
-642.783919	2.510145	6.585446
-640.864851	6.514133	6.595443
-639.360998	14.064518	6.605440
-637.064837	12.186591	6.615437
-635.542083	9.601690	6.625434
-633.559599	8.640738	6.635430
-631.609142	13.228677	6.645427
-629.740877	4.725855	6.655424
-628.378960	16.102670	6.665421
-625.937281	10.378811	6.675418
-623.791180	8.810664	6.685414
-622.233426	12.435018	6.695411
-620.491049	6.794465	6.705408
-618.865061	12.812696	6.715405
-616.471773	6.918154	6.725402
-614.600503	8.940296	6.735398
-612.848068	12.801980	6.745395
-611.156439	8.022186	6.755392
-609.324053	8.836313	6.765389
-607.388435	3.262795	6.775386
-605.300012	4.718139	6.785382
-603.673041	7.074585	6.795379
-601.717662	11.028595	6.805376
-599.748839	8.182980	6.815373
-597.928589	6.725334	6.825370
-595.738977	10.010341	6.835366
-594.145214	12.451048	6.845363
-592.487996	12.222628	6.855360
-590.421492	11.592505	6.865357
-588.502627	12.152831	6.875354
-586.699436	9.728428	6.885350
-584.671098	10.500220	6.895347
-582.914686	10.173854	6.905344
-581.200891	8.054267	6.915341
-579.253083	9.233671	6.925338
-577.033957	13.772425	6.935334
-575.133077	11.136632	6.945331
-573.559024	15.538431	6.955328
-571.736459	11.126173	6.965325
-569.895463	12.028958	6.975322
-567.781929	8.317080	6.985318
-565.781995	7.067602	6.995315
-564.163521	8.283835	7.005312
-562.313393	6.579860	7.015309
-560.190567	6.193403	7.025306
-558.567959	8.631106	7.035302
-556.745898	8.985863	7.045299
-554.869253	9.079267	7.055296
-552.874017	11.556929	7.065293
-550.731601	10.006805	7.075290
-549.151422	5.571702	7.085286
-547.479846	2.899926	7.095283
-545.184060	4.031670	7.105280
-543.630122	9.936726	7.115277
-541.459176	7.208875	7.125274
-539.636826	6.257788	7.135270
-537.835893	3.352196	7.145267
-536.052223	11.879556	7.155264
-534.252488	8.402568	7.165261
-532.105474	6.498036	7.175258
-530.136893	1.912486	7.185254
-528.604575	2.711445	7.195251
-526.929457	11.061936	7.205248
-524.735631	12.221039	7.215245
-522.663175	4.189371	7.225242
-520.965950	4.993575	7.235238
-519.158924	6.776577	7.245235
-517.338656	5.757943	7.255232
-515.475487	4.978779	7.265229
-513.380728	5.204751	7.275226
-511.502666	6.551669	7.285222
-509.586129	-2.374047	7.295219
-508.005543	-0.524872	7.305216
-505.806234	3.879743	7.315213
-503.925223	-0.308109	7.325210
-502.228997	2.376827	7.335206
-500.265264	7.044865	7.345203
-498.814770	11.766454	7.355200
-496.337144	4.448532	7.365197
-494.445768	0.756408	7.375194
-492.880466	0.200099	7.385190
-490.840001	5.714853	7.395187
-489.070950	9.060812	7.405184
-487.219944	7.629916	7.415181
-485.262381	9.679434	7.425178
-483.273603	5.087537	7.435174
-481.713264	2.406728	7.445171
-479.853702	5.397180	7.455168
-477.717252	8.539208	7.465165
-475.817183	4.387807	7.475162
-474.196970	8.344926	7.485158
-472.434001	13.861383	7.495155
-470.298176	5.825950	7.505152
-468.593901	6.818544	7.515149
-466.426340	6.173968	7.525146
-464.579636	5.590108	7.535142
-462.703315	6.938922	7.545139
-460.975744	7.245683	7.555136
-458.979810	4.675330	7.565133
-457.199229	2.278318	7.575130
-455.117331	1.243215	7.585126
-453.527583	-2.411763	7.595123
-451.335566	8.268917	7.605120
-449.302861	4.364781	7.615117
-447.923439	5.614531	7.625114
-446.327088	8.088086	7.635110
-444.048432	9.541618	7.645107
-442.256270	9.598074	7.655104
-440.255200	9.523276	7.665101
-438.428758	2.034653	7.675098
-436.462134	2.535368	7.685094
-434.682033	2.557440	7.695091
-432.890119	11.800425	7.705088
-430.786468	7.933923	7.715085
-429.001433	6.752031	7.725082
-427.094842	8.557101	7.735078
-425.176753	4.061802	7.745075
-423.332618	2.090463	7.755072
-421.719471	10.345142	7.765069
-420.060057	2.700040	7.775066
-417.748129	-1.247076	7.785062
-415.723051	1.031723	7.795059
-413.946732	9.670887	7.805056
-412.145355	6.236357	7.815053
-410.148227	12.825495	7.825050
-408.259804	6.863337	7.835046
-406.551516	5.455291	7.845043
-404.479626	8.482957	7.855040
-402.832597	12.543217	7.865037
-400.694552	15.162422	7.875034
-399.234566	9.631843	7.885030
-397.035016	7.809042	7.895027
-395.214429	11.326850	7.905024
-393.560722	12.832845	7.915021
-391.415663	13.673011	7.925018
-389.703814	5.967447	7.935014
-387.817937	8.000071	7.945011
-385.703781	10.239412	7.955008
-384.055696	14.286886	7.965005
-382.199388	9.518844	7.975002
-380.280857	0.416054	7.984998
-378.276626	0.669230	7.994995
-376.502089	5.386531	8.004992
-374.943769	11.373115	8.014989
-372.403896	4.402222	8.024986
-370.463584	0.691325	8.034982
-368.783800	2.568970	8.044979
-367.560824	-0.500020	8.054976
-365.566944	4.644910	8.064973
-363.552040	5.077977	8.074970
-361.225424	2.543331	8.084966
-359.288554	3.064651	8.094963
-357.845914	7.263364	8.104960
-356.149451	6.283565	8.114957
-353.843226	2.815848	8.124954
-351.867664	6.466845	8.134950
-350.257292	7.935577	8.144947
-348.141355	5.924060	8.154944
-346.409490	3.231742	8.164941
-344.622927	3.925493	8.174938
-342.689962	8.268575	8.184934
-340.833977	6.101192	8.194931
-339.226086	10.301959	8.204928
-337.472210	8.929315	8.214925
-335.184194	3.977125	8.224922
-333.099386	5.145915	8.234918
-331.495801	4.924658	8.244915
-329.683201	5.898480	8.254912
-327.581556	10.023591	8.264909
-325.624859	3.426899	8.274906
-324.150911	2.635805	8.284902
-322.180948	8.049861	8.294899
-320.113529	3.840281	8.304896
-318.285490	9.997011	8.314893
-316.379248	9.823768	8.324890
-314.686642	3.172924	8.334886
-312.621661	1.602212	8.344883
-310.996110	7.904957	8.354880
-309.021197	8.579722	8.364877
-307.181919	5.333431	8.374874
-305.089440	1.707244	8.384870
-303.009751	1.492113	8.394867
-301.499749	5.602740	8.404864
-299.917990	10.688777	8.414861
-297.692104	4.735991	8.424858
-295.664628	9.867728	8.434854
-293.616030	7.691740	8.444851
-292.375817	0.506796	8.454848
-290.417049	2.649444	8.464845
-288.099827	-3.422122	8.474842
-286.369921	-1.959795	8.484838
-284.681183	2.757061	8.494835
-282.859834	3.770576	8.504832
-280.745253	10.374241	8.514829
-278.833469	-1.075342	8.524826
-276.994758	-0.364600	8.534822
-275.352834	6.443988	8.544819
-273.134266	10.970496	8.554816
-271.296264	3.014341	8.564813
-269.458269	4.967859	8.574810
-267.611281	1.963530	8.584807
-265.736470	3.679064	8.594803
-263.865563	5.186799	8.604800
-262.100875	4.966717	8.614797
-260.212223	-0.611676	8.624794
-258.466344	-3.077218	8.634791
-256.538970	-0.683210	8.644787
-254.518813	-0.764058	8.654784
-252.343186	-0.912350	8.664781
-250.867251	5.149050	8.674778
-249.212213	1.207456	8.684775
-246.952284	-2.030137	8.694771
-244.819993	3.264918	8.704768
-243.316552	3.528660	8.714765
-241.464422	0.678269	8.724762
-239.437010	1.047864	8.734759
-237.599923	0.113599	8.744755
-235.849190	-1.858481	8.754752
-233.962125	4.162577	8.764749
-232.067693	-3.404651	8.774746
-229.619351	-11.800817	8.784743
-228.173507	-1.684525	8.794739
-226.546926	-6.467893	8.804736
-224.639166	1.687806	8.814733
-222.573903	0.579766	8.824730
-220.576136	-5.484967	8.834727
-218.775180	-4.299198	8.844723
-216.931529	-8.580350	8.854720
-215.251154	-2.183654	8.864717
-213.223832	-3.538267	8.874714
-211.415431	-3.618443	8.884711
-209.638341	-8.010548	8.894707
-207.341423	-9.548710	8.904704
-205.697200	-8.615820	8.914701
-203.918305	-8.228641	8.924698
-202.253608	-4.955811	8.934695
-200.020350	-6.036956	8.944691
-198.310158	-6.262505	8.954688
-196.380685	-0.792932	8.964685
-194.537053	-8.276234	8.974682
-192.493185	-12.024044	8.984679
-190.780034	-3.020930	8.994675
-188.827978	-3.236121	9.004672
-187.383247	-3.090873	9.014669
-184.975354	0.475486	9.024666
-183.141554	0.727601	9.034663
-181.375711	-0.853687	9.044659
-179.623509	-3.931248	9.054656
-177.499118	-3.531286	9.064653
-175.779911	-5.875669	9.074650
-174.027641	-0.311483	9.084647
-172.111072	-5.592680	9.094643
-170.268884	-4.212924	9.104640
-168.054944	-3.582501	9.114637
-166.329773	0.021766	9.124634
-164.439750	3.058139	9.134631
-162.582177	2.258033	9.144627
-160.691013	2.412589	9.154624
-158.924391	7.502385	9.164621
-157.155590	0.692638	9.174618
-155.105357	-4.429872	9.184615
-153.054735	-1.460170	9.194611
-151.260706	2.969981	9.204608
-149.436580	2.544704	9.214605
-147.696191	-0.504108	9.224602
-145.768567	0.243075	9.234599
-143.755129	-0.681363	9.244595
-142.089182	4.304507	9.254592
-140.071555	-2.882832	9.264589
-138.310234	-4.150729	9.274586
-136.360168	-5.121892	9.284583
-134.467543	2.017860	9.294579
-132.461792	6.829517	9.304576
-130.610938	4.546265	9.314573
-128.839117	3.598811	9.324570
-126.865695	3.230257	9.334567
-125.217161	-3.329747	9.344563
-123.030460	10.090073	9.354560
-121.363917	5.928825	9.364557
-119.637533	6.144442	9.374554
-117.458629	8.072109	9.384551
-115.841667	-1.069225	9.394547
-113.911172	8.365081	9.404544
-111.780048	6.319763	9.414541
-110.126435	4.685378	9.424538
-108.097757	6.164906	9.434535
-106.457099	-0.453833	9.444531
-104.322439	4.664130	9.454528
-102.503371	5.469722	9.464525
-100.771855	1.981821	9.474522
-98.750805	-6.980806	9.484519
-96.713591	-2.128350	9.494515
-94.982819	1.794032	9.504512
-93.506008	-0.696365	9.514509
-91.725573	-1.608849	9.524506
-89.258816	-0.685523	9.534503
-87.290179	2.144156	9.544499
-85.798363	5.435180	9.554496
-83.827971	4.451342	9.564493
-81.834094	9.891795	9.574490
-79.964676	3.996065	9.584487
-78.322277	6.369367	9.594483
-76.344763	0.931670	9.604480
-74.190664	3.248605	9.614477
-72.693177	-1.831450	9.624474
-70.574685	-2.257838	9.634471
-68.758172	3.114601	9.644467
-66.998862	1.378117	9.654464
-64.968304	-1.467449	9.664461
-63.391160	1.299965	9.674458
-61.367343	1.343434	9.684455
-59.441123	-6.239796	9.694451
-57.581177	2.687905	9.704448
-55.560077	4.511326	9.714445
-53.677109	2.095111	9.724442
-51.954371	1.750818	9.734439
-50.236588	0.306767	9.744435
-47.959937	-4.643351	9.754432
-46.141322	4.183583	9.764429
-44.569177	3.749632	9.774426
-42.584800	3.483612	9.784423
-40.890565	5.798144	9.794419
-38.587405	2.902797	9.804416
-37.006251	2.535310	9.814413
-35.099695	4.285439	9.824410
-33.081492	4.839839	9.834407
-31.344869	2.379088	9.844403
-29.211176	5.842503	9.854400
-27.480555	2.673749	9.864397
-25.542056	0.684497	9.874394
-23.862782	5.000419	9.884391
-22.004506	-0.078736	9.894387
-20.000380	-0.125251	9.904384
-18.071532	6.497235	9.914381
-16.030355	4.736354	9.924378
-14.528189	2.194589	9.934375
-12.395040	0.712731	9.944371
-10.725891	-1.609344	9.954368
-8.718400	-2.793254	9.964365
-7.049976	-3.948344	9.974362
-5.419351	13.916714	9.984359
-3.875315	38.271031	9.994355
-2.651045	79.072632	10.004352
-1.231866	140.744443	10.014349
0.000000	196.793294	10.019354
0.331829	226.884467	10.024359
1.156303	255.564567	10.029363
1.299430	286.638466	10.034368
1.938678	315.972720	10.039373
2.636245	342.059359	10.044378
2.754737	357.422534	10.049383
3.141021	356.824741	10.054387
3.068739	365.200694	10.059392
3.074778	362.222349	10.064397
3.378880	367.728051	10.069402
3.186538	381.622175	10.074407
3.629189	389.367212	10.079411
3.787035	394.445228	10.084416
3.702542	396.652321	10.089421
3.599748	390.816446	10.094426
3.791598	406.046543	10.099431
3.997549	407.314725	10.104435
3.569013	401.625423	10.109440
3.616559	402.366918	10.114445
3.735721	414.249592	10.119450
3.474434	412.955541	10.124455
3.940525	409.858075	10.129459
4.056382	416.879362	10.134464
3.830340	423.858988	10.139469
3.925669	415.110307	10.144474
3.921442	421.519946	10.149479
4.022846	422.069919	10.154483
3.829873	425.817711	10.159488
3.929106	432.124118	10.164493
4.207379	439.761354	10.169498
4.174421	460.099033	10.174503
4.607968	453.272381	10.179507
4.442474	467.190691	10.184512
4.537093	463.220448	10.189517
4.657420	465.937376	10.194522
4.429322	471.095901	10.199527
4.821832	470.940252	10.204531
4.408313	474.565532	10.209536
4.919718	466.958449	10.214541
4.855774	473.800276	10.219546
4.615539	485.013327	10.224551
4.580747	474.823470	10.229555
4.780846	482.492122	10.234560
4.761747	478.129989	10.239565
4.973716	486.317165	10.244570
4.943881	489.586349	10.249575
4.866459	484.779335	10.254579
4.834483	487.591525	10.259584
4.722413	487.174144	10.264589
5.105257	485.630686	10.269594
4.713560	509.231727	10.274599
5.469961	514.043998	10.279603
4.983703	519.327299	10.284608
5.077316	521.815099	10.289613
5.137321	524.648896	10.294618
5.163427	531.973149	10.299623
5.381529	527.167874	10.304627
5.133635	530.247910	10.309632
5.234715	532.523200	10.314637
5.569588	545.688388	10.319642
5.843213	559.142490	10.324647
5.965132	553.281748	10.329651
5.753304	554.755358	10.334656
5.653808	542.686499	10.339661
5.637529	545.152405	10.344666
5.838665	563.587273	10.349671
5.967398	562.204191	10.354675
5.821549	573.493723	10.359680
6.099177	575.947451	10.364685
6.329377	571.318436	10.369690
5.862786	578.869538	10.374695
6.262876	577.104113	10.379699
6.111179	576.283023	10.384704
6.323244	578.160555	10.389709
6.348161	582.351472	10.394714
6.346704	572.228773	10.399719
6.683100	574.457075	10.404723
6.210860	583.165040	10.409728
6.187746	588.585816	10.414733
6.513085	585.362523	10.419738
6.153216	581.702870	10.424743
6.139481	581.548935	10.429747
6.258581	584.893738	10.434752
6.500622	590.694865	10.439757
6.744691	599.591379	10.444762
6.627361	620.709176	10.449767
6.784220	608.783886	10.454771
6.871921	617.765279	10.459776
7.033629	616.996706	10.464781
7.172789	624.487486	10.469786
6.649962	628.426719	10.474791
6.915642	619.382649	10.479795
6.915312	623.587067	10.484800
7.015549	628.376295	10.489805
7.065595	627.799005	10.494810
6.913797	630.830617	10.499815
7.054144	632.822102	10.504819
7.238595	633.368300	10.509824
7.045518	637.265980	10.514829
7.419674	635.326480	10.519834
7.041401	636.110672	10.524839
7.098701	641.811970	10.529843
7.508901	659.273702	10.534848
7.249188	662.984888	10.539853
7.577007	663.408867	10.544858
7.756833	674.663879	10.549863
7.516145	661.884119	10.554867
7.328548	678.449268	10.559872
7.611722	676.205712	10.564877
7.728143	673.744314	10.569882
7.516979	672.973706	10.574887
7.990419	676.031765	10.579891
8.115637	675.043493	10.584896
7.694953	677.174934	10.589901
8.054228	685.449119	10.594906
7.931251	684.284379	10.599911
8.120153	679.321276	10.604915
8.134474	688.465812	10.609920
8.306500	701.671309	10.614925
8.591018	697.394733	10.619930
8.485491	689.526370	10.624935
8.686242	681.413608	10.629939
8.178857	680.450537	10.634944
7.944209	679.488122	10.639949
8.156748	702.855899	10.644954
8.399608	714.821596	10.649959
8.635819	704.791792	10.654963
8.315171	714.477076	10.659968
8.287612	719.231521	10.664973
8.982022	718.083071	10.669978
8.645844	716.758357	10.674983
8.956326	716.317730	10.679987
8.829779	727.960714	10.684992
9.004685	719.535067	10.689997
8.864072	730.287691	10.695002
8.878630	734.138086	10.700007
8.959526	727.526836	10.705011
8.675220	725.321743	10.710016
9.166297	726.334731	10.715021
9.348327	719.451873	10.720026
8.982588	727.141515	10.725031
9.130626	723.651565	10.730035
8.847207	725.035679	10.735040
8.867398	721.586622	10.740045
9.073849	741.845507	10.745050
9.522473	752.906311	10.750055
9.876706	758.960864	10.755059
9.410979	754.081646	10.760064
9.456040	763.525696	10.765069
9.810693	761.541980	10.770074
9.551000	765.215339	10.775079
9.704274	767.362486	10.780083
9.669677	769.211572	10.785088
9.537419	768.537190	10.790093
9.413761	763.466207	10.795098
9.348503	769.830537	10.800103
9.677245	766.396915	10.805107
9.660666	777.951432	10.810112
9.667673	769.806441	10.815117
9.724273	771.636251	10.820122
9.680787	788.186424	10.825127
9.754608	797.228492	10.830131
9.876163	806.728183	10.835136
9.987476	802.140135	10.840141
10.405815	804.815903	10.845146
10.323451	807.491103	10.850151
10.654404	799.478941	10.855155
10.243979	803.323017	10.860160
10.083387	809.803502	10.865165
10.615126	810.895172	10.870170
10.170765	815.580500	10.875175
10.524416	805.249603	10.880179
10.194583	810.340890	10.885184
10.374297	816.836490	10.890189
10.612585	828.336204	10.895194
10.512706	843.979166	10.900199
10.765937	836.539236	10.905203
10.882407	842.641209	10.910208
10.892918	836.588374	10.915213
10.945908	836.486876	10.920218
11.016786	838.888465	10.925223
10.790786	842.084930	10.930227
10.769971	850.189584	10.935232
10.526717	844.989404	10.940237
11.215381	832.827713	10.945242
10.977605	842.764809	10.950247
11.151246	837.493407	10.955251
10.859871	842.289970	10.960256
11.082681	848.870181	10.965261
11.287690	844.180438	10.970266
11.079087	851.857699	10.975271
11.249614	861.172984	10.980275
11.645267	872.322758	10.985280
11.786755	872.593525	10.990285
11.874803	872.418622	10.995290
11.681934	866.122228	11.000295
11.478663	858.318252	11.005299
11.705774	853.448351	11.010304
11.853570	854.030368	11.015309
11.752962	847.339196	11.020314
11.817304	852.243040	11.025319
11.720057	845.393628	11.030323
11.833046	871.575251	11.035328
11.948944	872.378414	11.040333
12.055132	874.324915	11.045338
11.889378	883.690696	11.050343
11.967023	878.306849	11.055347
11.944184	888.242813	11.060352
12.190431	888.921100	11.065357
12.200903	876.760302	11.070362
12.048788	879.028719	11.075367
12.317138	873.355819	11.080371
12.306068	886.432982	11.085376
12.296312	881.480994	11.090381
12.397502	886.066715	11.095386
12.369370	890.453852	11.100391
12.256078	880.776159	11.105395
12.533019	884.292989	11.110400
12.392265	880.450066	11.115405
12.653461	886.850695	11.120410
12.276594	886.716826	11.125415
12.468370	889.744158	11.130419
12.859451	912.760499	11.135424
12.822872	917.611071	11.140429
13.022305	910.272731	11.145434
12.805667	922.717194	11.150439
12.941911	923.534462	11.155443
13.162908	919.296339	11.160448
13.062688	914.483357	11.165453
13.416746	914.649253	11.170458
13.223985	922.989545	11.175463
13.083533	912.519745	11.180467
13.098253	921.060349	11.185472
13.111832	916.527280	11.190477
13.168651	920.493995	11.195482
13.065411	926.424451	11.200487
13.459408	917.888047	11.205491
13.276275	921.508230	11.210496
13.250265	923.914247	11.215501
13.429058	912.075104	11.220506
13.225856	921.431112	11.225511
13.538854	918.428927	11.230515
13.387300	917.379120	11.235520
13.779553	918.887313	11.240525
13.760798	918.934462	11.245530
13.380212	921.963198	11.250535
13.760361	929.474051	11.255539
13.817358	936.874011	11.260544
13.942523	942.141949	11.265549
13.949129	949.408017	11.270554
14.016404	946.169033	11.275559
14.183801	944.194657	11.280563
14.094976	940.619423	11.285568
14.083117	942.554797	11.290573
14.288181	943.957221	11.295578
14.316327	948.193464	11.300583
14.143695	938.369067	11.305587
14.165347	938.875006	11.310592
14.241419	935.875912	11.315597
14.651998	935.528132	11.320602
14.521627	940.620768	11.325607
14.420584	940.753587	11.330611
14.454336	946.364137	11.335616
14.286186	947.020206	11.340621
14.384458	937.524790	11.345626
14.378310	946.843076	11.350631
14.532947	951.868179	11.355635
14.227316	943.714604	11.360640
14.853972	957.685245	11.365645
15.280398	960.466994	11.370650
14.845374	963.318327	11.375655
14.840470	951.016406	11.380659
14.784745	952.801072	11.385664
14.815753	967.503861	11.390669
15.218834	978.518483	11.395674
15.134769	984.999456	11.400679
15.234641	975.547918	11.405683
15.265812	980.135374	11.410688
15.477908	980.754453	11.415693
15.830431	957.349724	11.420698
15.103757	961.693744	11.425703
15.381024	946.221074	11.430707
15.387202	946.732635	11.435712
15.130169	951.295082	11.440717
15.587074	960.944828	11.445722
15.420672	977.453315	11.450727
15.497450	977.086229	11.455731
15.592302	990.044082	11.460736
15.573716	978.733143	11.465741
16.089403	970.871210	11.470746
15.880776	984.741696	11.475751
16.000022	981.710473	11.480755
16.070665	979.537043	11.485760
15.678868	974.869901	11.490765
15.992811	972.911575	11.495770
16.145945	980.217371	11.500775
16.021253	971.769973	11.505779
15.564173	968.559418	11.510784
15.867945	980.777414	11.515789
15.954508	980.389843	11.520794
15.734831	988.797548	11.525799
15.897523	980.386316	11.530803
16.099258	988.070746	11.535808
15.928590	992.537423	11.540813
16.038257	994.152201	11.545818
16.291287	1008.002696	11.550823
16.392007	1008.369861	11.555827
16.505912	1019.600961	11.560832
16.538947	1020.130321	11.565837
16.886737	1012.536437	11.570842
16.616551	1013.584127	11.575847
16.683468	1014.589089	11.580851
16.657804	1017.703173	11.585856
16.587882	1017.558195	11.590861
16.495925	1016.259160	11.595866
16.689312	1021.789080	11.600871
16.743508	1014.929626	11.605875
16.654411	1025.333603	11.610880
16.734197	1022.877989	11.615885
16.654878	1024.634885	11.620890
16.628047	1045.554346	11.625895
17.329564	1049.741571	11.630899
17.381827	1049.512445	11.635904
17.628128	1046.423094	11.640909
17.415815	1031.331218	11.645914
17.428486	1019.538985	11.650919
17.269037	1015.640657	11.655923
17.420719	1022.680180	11.660928
17.127749	1024.939544	11.665933
17.440751	1020.711951	11.670938
17.457019	1038.011450	11.675943
17.517326	1044.097233	11.680947
18.134794	1044.874028	11.685952
17.724712	1039.526907	11.690957
17.709197	1029.731010	11.695962
17.478334	1034.111098	11.700967
17.798491	1041.248349	11.705971
17.944498	1043.317843	11.710976
17.872567	1043.748818	11.715981
18.125308	1043.240116	11.720986
18.067487	1049.431481	11.725991
17.978463	1043.686194	11.730995
17.755179	1053.852953	11.736000
18.025627	1049.953863	11.741005
18.183240	1050.475971	11.746010
18.160859	1053.550112	11.751015
18.061926	1040.611779	11.756019
17.937303	1055.497187	11.761024
18.139567	1056.215617	11.766029
18.385906	1056.772463	11.771034
18.063836	1051.305636	11.776039
18.580959	1047.450789	11.781043
18.599010	1050.945868	11.786048
18.074212	1057.803121	11.791053
18.129287	1061.948363	11.796058
18.111579	1061.643657	11.801063
18.734590	1068.828820	11.806067
19.003600	1062.176375	11.811072
18.733153	1064.846924	11.816077
19.342239	1058.592863	11.821082
18.860939	1053.820113	11.826087
18.762347	1050.233792	11.831091
18.915149	1046.944871	11.836096
18.812677	1043.068989	11.841101
19.121029	1050.826342	11.846106
18.944262	1059.594703	11.851111
19.261144	1056.896248	11.856115
19.275021	1063.014677	11.861120
19.054719	1057.556849	11.866125
19.258023	1053.001364	11.871130
19.191856	1060.736447	11.876135
19.336411	1060.073098	11.881139
19.538496	1059.832693	11.886144
19.337820	1064.114927	11.891149
19.722328	1057.647507	11.896154
19.425835	1055.367029	11.901159
19.638017	1055.866240	11.906163
19.648477	1056.058553	11.911168
19.577477	1053.844620	11.916173
19.666412	1044.930987	11.921178
19.570413	1052.219780	11.926183
19.694315	1055.709018	11.931187
19.463024	1063.199181	11.936192
19.666415	1064.682315	11.941197
20.081158	1064.218743	11.946202
19.853014	1069.405872	11.951207
19.510424	1060.483779	11.956211
20.103895	1055.687853	11.961216
19.833978	1064.953660	11.966221
19.802538	1065.715673	11.971226
19.634432	1058.891654	11.976231
19.668006	1066.008389	11.981235
20.153947	1088.435824	11.986240
20.050606	1092.043322	11.991245
20.483515	1093.664908	11.996250
20.276021	1104.573567	12.001255
20.123144	1098.114561	12.006259
20.195200	1098.738634	12.011264
19.996429	1105.067630	12.016269
20.110532	1099.964915	12.021274
20.146736	1100.629402	12.026279
20.677434	1114.462524	12.031283
20.664604	1116.634639	12.036288
20.722228	1116.920364	12.041293
20.949294	1103.507321	12.046298
20.738395	1102.302948	12.051303
20.820686	1096.055615	12.056307
21.037797	1094.024401	12.061312
20.680179	1095.529201	12.066317
20.984114	1091.481245	12.071322
21.217818	1088.983724	12.076327
20.682938	1077.791326	12.081331
20.639227	1070.005945	12.086336
20.822729	1069.550866	12.091341
20.818074	1055.635464	12.096346
20.570184	1066.066374	12.101351
20.523128	1062.115411	12.106355
20.872158	1064.994687	12.111360
20.451541	1076.829944	12.116365
20.738400	1060.410951	12.121370
20.246637	1064.081971	12.126375
20.557533	1059.354769	12.131379
20.655070	1064.549882	12.136384
20.859068	1070.049741	12.141389
20.868688	1069.048338	12.146394
20.579202	1079.586825	12.151399
20.624157	1066.992979	12.156403
20.835264	1053.085747	12.161408
20.835737	1054.840960	12.166413
20.491482	1041.034934	12.171418
20.455189	1049.150053	12.176423
20.559748	1040.003678	12.181427
20.650479	1046.876303	12.186432
20.528026	1051.067204	12.191437
20.481307	1041.668967	12.196442
20.532986	1052.195601	12.201447
20.397972	1049.512447	12.206451
20.455497	1048.713157	12.211456
20.452169	1048.825661	12.216461
20.595687	1046.035000	12.221466
20.369644	1055.440472	12.226471
20.646322	1048.278992	12.231475
20.497647	1042.853903	12.236480
20.439216	1049.967956	12.241485
21.017311	1037.634483	12.246490
20.425163	1051.531505	12.251495
20.019822	1050.093200	12.256499
20.483326	1048.536822	12.261504
20.401677	1048.885762	12.266509
20.702607	1051.856293	12.271514
20.769778	1059.882371	12.276519
20.627150	1055.164422	12.281523
20.359940	1056.626411	12.286528
20.426814	1051.531246	12.291533
20.416520	1057.263990	12.296538
20.348416	1053.127137	12.301543
20.365671	1047.959456	12.306547
20.581380	1045.584669	12.311552
20.399803	1057.936916	12.316557
20.479600	1060.401780	12.321562
20.630275	1068.974407	12.326567
20.863381	1064.914099	12.331571
20.795835	1052.529035	12.336576
20.783238	1056.815966	12.341581
20.855314	1051.242117	12.346586
20.955870	1050.629944	12.351591
20.526014	1057.959371	12.356595
20.801244	1051.758561	12.361600
20.768287	1054.818618	12.366605
20.464060	1059.317656	12.371610
20.520033	1063.338165	12.376615
20.483723	1056.674491	12.381619
20.729174	1057.349760	12.386624
20.495188	1059.050898	12.391629
20.916333	1052.591830	12.396634
21.165261	1051.700506	12.401639
20.926397	1034.884383	12.406643
20.988837	1026.638936	12.411648
20.588532	1027.437700	12.416653
20.543614	1019.012246	12.421658
20.412237	1035.491556	12.426663
20.422485	1026.136287	12.431667
20.538008	1023.818487	12.436672
20.537122	1022.698906	12.441677
20.611785	1023.073382	12.446682
20.423623	1034.299050	12.451687
20.233554	1026.209004	12.456691
20.555442	1024.566397	12.461696
20.214005	1027.462743	12.466701
20.469931	1023.368843	12.471706
20.234161	1025.306822	12.476711
20.193115	1020.884943	12.481715
20.504893	1029.624256	12.486720
20.401024	1035.266252	12.491725
20.672506	1031.042125	12.496730
20.792626	1035.329961	12.501735
20.388566	1029.481949	12.506739
20.573023	1027.578965	12.511744
20.265455	1034.674394	12.516749
20.298927	1028.374947	12.521754
20.175888	1039.623352	12.526759
20.633748	1051.553461	12.531763
20.577517	1066.437435	12.536768
20.563125	1068.508859	12.541773
20.900393	1050.966842	12.546778
20.376430	1046.675598	12.551783
20.164278	1047.371808	12.556787
20.409219	1053.751448	12.561792
20.286159	1066.264693	12.566797
20.677397	1064.407578	12.571802
20.623733	1071.700668	12.576807
20.572456	1061.807942	12.581811
20.580961	1062.495769	12.586816
20.437006	1073.359574	12.591821
20.572081	1066.089773	12.596826
20.539206	1066.558678	12.601831
20.420162	1074.220194	12.606835
20.557530	1068.411979	12.611840
20.326781	1072.610696	12.616845
20.538979	1064.453315	12.621850
20.699756	1076.224230	12.626855
20.574483	1074.818530	12.631859
20.622457	1071.219867	12.636864
20.595320	1070.396229	12.641869
20.356507	1042.401752	12.646874
20.735793	1057.419697	12.651879
20.564481	1057.918567	12.656883
20.512318	1043.200136	12.661888
20.352105	1046.621137	12.666893
20.473010	1057.120963	12.671898
20.689425	1075.882078	12.676903
20.662490	1063.649813	12.681907
20.744624	1051.472708	12.686912
20.353425	1050.811223	12.691917
20.601878	1043.236322	12.696922
20.585374	1044.806569	12.701927
20.438850	1039.824297	12.706931
20.430386	1047.717341	12.711936
20.295117	1050.355287	12.716941
20.379460	1044.699053	12.721946
20.574006	1059.585604	12.726951
20.301686	1071.256843	12.731955
20.691354	1066.843531	12.736960
20.430346	1081.113578	12.741965
20.628701	1072.956824	12.746970
20.264867	1076.481276	12.751975
20.425733	1072.077644	12.756979
20.780520	1084.740214	12.761984
20.571071	1081.338738	12.766989
21.033928	1067.194205	12.771994
20.426398	1058.751220	12.776999
20.543256	1047.008585	12.782003
20.586421	1045.762118	12.787008
20.493520	1052.056859	12.792013
20.747534	1047.158947	12.797018
20.149744	1048.632656	12.802023
20.151924	1053.970717	12.807027
20.264586	1064.621686	12.812032
20.288195	1069.565219	12.817037
20.636473	1074.816545	12.822042
20.393653	1083.735816	12.827047
20.324539	1083.597017	12.832051
20.810888	1090.606853	12.837056
20.493129	1090.935100	12.842061
20.754480	1090.959654	12.847066
20.556612	1090.983328	12.852071
20.243141	1087.284602	12.857075
20.620684	1079.036181	12.862080
20.249289	1092.781330	12.867085
20.667184	1082.610316	12.872090
20.794995	1087.581394	12.877095
20.617934	1086.920450	12.882099
21.060886	1078.262596	12.887104
20.679308	1061.790928	12.892109
21.067140	1061.394731	12.897114
20.754179	1058.153283	12.902119
20.850916	1048.523988	12.907123
20.598482	1054.736932	12.912128
20.723427	1065.283432	12.917133
20.750755	1058.425089	12.922138
20.687029	1058.758554	12.927143
20.555257	1057.330237	12.932147
20.797347	1053.227495	12.937152
20.573600	1049.284214	12.942157
20.286705	1028.758588	12.947162
20.401101	1041.718101	12.952167
20.365124	1046.887190	12.957171
20.575385	1058.934072	12.962176
20.307496	1056.489746	12.967181
20.500222	1059.329291	12.972186
20.307599	1064.977569	12.977191
20.655648	1052.072022	12.982195
20.475927	1060.377193	12.987200
20.244487	1052.054015	12.992205
20.601320	1059.145998	12.997210
20.351554	1063.784597	13.002215
20.179578	1066.524603	13.007219
20.757767	1052.812734	13.012224
20.382135	1064.342738	13.017229
20.590007	1054.102731	13.022234
20.586724	1057.848817	13.027239
20.419113	1068.777897	13.032243
20.714580	1050.417735	13.037248
20.704069	1070.049311	13.042253
20.694834	1060.607234	13.047258
20.473409	1063.014477	13.052263
20.558814	1060.685704	13.057267
20.620955	1060.294140	13.062272
20.535840	1057.259223	13.067277
20.713797	1070.140810	13.072282
20.698459	1062.541734	13.077287
20.396859	1064.296238	13.082291
21.094379	1060.999288	13.087296
20.521360	1043.444758	13.092301
20.573819	1033.049766	13.097306
20.492159	1034.649329	13.102311
20.540845	1041.074459	13.107315
20.659063	1026.038688	13.112320
20.099004	1041.897196	13.117325
20.451470	1048.204487	13.122330
20.535784	1057.396443	13.127335
20.284237	1065.966984	13.132339
20.592825	1067.204663	13.137344
20.527581	1067.371200	13.142349
20.732471	1059.183446	13.147354
20.510948	1071.608313	13.152359
20.629964	1067.698676	13.157363
20.862262	1045.125177	13.162368
20.096872	1046.404827	13.167373
20.378758	1043.686723	13.172378
20.758785	1055.115121	13.177383
20.784748	1060.193905	13.182387
20.696060	1042.833384	13.187392
20.126915	1040.383489	13.192397
20.853676	1037.192277	13.197402
20.372898	1041.489215	13.202407
20.260148	1038.381433	13.207411
20.419486	1037.528055	13.212416
20.247302	1057.852503	13.217421
20.877833	1069.696735	13.222426
20.506656	1059.672091	13.227431
20.455151	1050.124790	13.232435
20.875017	1048.070707	13.237440
20.447845	1048.865871	13.242445
20.527355	1035.728757	13.247450
20.407109	1039.044026	13.252455
20.327101	1043.075178	13.257459
20.759798	1052.421318	13.262464
20.435210	1053.228509	13.267469
20.677970	1043.175349	13.272474
20.615194	1048.238317	13.277479
20.441899	1044.340612	13.282483
20.215947	1041.271386	13.287488
20.407908	1050.204876	13.292493
20.755251	1058.107413	13.297498
20.485343	1058.721365	13.302503
20.326216	1049.394672	13.307507
20.472241	1056.375186	13.312512
20.824385	1069.339386	13.317517
20.577150	1052.871535	13.322522
20.547943	1041.614284	13.327527
20.249329	1049.947875	13.332531
20.762304	1058.558914	13.337536
20.649143	1049.904610	13.342541
20.610976	1047.288018	13.347546
20.634377	1040.209519	13.352551
20.297141	1036.741695	13.357555
20.376551	1042.261415	13.362560
20.222748	1047.073951	13.367565
20.406790	1060.604315	13.372570
20.617209	1068.711638	13.377575
20.658418	1070.428814	13.382579
20.957195	1063.091900	13.387584
20.571078	1060.899838	13.392589
20.611248	1046.918943	13.397594
20.490786	1045.626028	13.402599
20.307606	1041.901802	13.407603
20.646515	1035.441664	13.412608
20.516850	1049.326428	13.417613
20.744278	1043.999060	13.422618
20.637810	1046.176637	13.427623
20.696079	1044.251196	13.432627
20.675479	1035.990601	13.437632
20.618182	1041.387033	13.442637
20.739034	1039.629819	13.447642
20.443288	1051.019328	13.452647
20.472364	1048.912447	13.457651
20.710960	1046.403112	13.462656
20.502780	1047.248511	13.467661
20.733631	1046.604517	13.472666
20.352892	1052.301719	13.477671
20.444312	1040.858059	13.482675
20.592201	1045.015303	13.487680
20.591762	1053.086856	13.492685
20.809991	1043.192163	13.497690
20.791900	1042.233032	13.502695
20.542804	1052.025407	13.507699
21.269042	1052.097250	13.512704
21.009123	1035.106275	13.517709
20.555031	1019.942577	13.522714
20.244252	1024.501001	13.527719
20.293201	1023.125870	13.532723
20.580575	1015.793953	13.537728
20.322797	1027.637893	13.542733
20.299548	1014.755326	13.547738
20.408627	1029.603435	13.552743
20.692280	1041.480889	13.557747
20.560679	1038.559054	13.562752
20.378350	1034.779496	13.567757
20.388792	1037.466746	13.572762
20.850114	1041.685971	13.577767
20.607961	1033.555338	13.582771
20.524772	1021.433013	13.587776
20.354863	1024.742005	13.592781
20.713111	1024.757413	13.597786
20.619174	1028.920103	13.602791
20.180715	1030.781593	13.607795
20.368575	1032.358671	13.612800
20.493068	1052.224176	13.617805
20.456994	1056.306677	13.622810
20.685824	1066.126924	13.627815
20.720309	1054.591401	13.632819
20.596876	1033.128146	13.637824
20.266635	1028.930599	13.642829
20.485313	1028.225465	13.647834
20.550083	1037.420526	13.652839
20.480961	1040.995744	13.657843
20.837636	1047.095766	13.662848
20.465615	1051.919452	13.667853
20.367595	1024.025567	13.672858
20.227271	1039.257266	13.677863
20.369681	1045.547591	13.682867
20.750761	1055.379820	13.687872
20.353297	1058.043815	13.692877
20.555269	1060.445035	13.697882
20.552449	1061.021119	13.702887
20.790939	1059.905937	13.707891
20.552241	1037.904350	13.712896
20.460290	1031.656447	13.717901
20.479445	1033.479646	13.722906
20.448015	1042.861956	13.727911
20.522787	1045.538947	13.732915
20.772702	1044.385671	13.737920
20.410751	1038.885782	13.742925
20.822195	1036.022426	13.747930
20.580502	1024.728111	13.752935
20.285159	1031.805818	13.757939
20.461794	1023.248824	13.762944
20.470587	1027.201149	13.767949
20.340492	1023.233476	13.772954
20.433215	1043.124538	13.777959
20.611572	1060.333553	13.782963
20.757187	1055.599595	13.787968
20.633020	1043.882788	13.792973
20.486673	1031.229590	13.797978
20.512997	1032.059665	13.802983
20.457978	1031.536967	13.807987
20.335374	1029.788620	13.812992
20.353511	1044.256979	13.817997
20.794822	1045.486105	13.823002
20.809349	1049.387055	13.828007
20.683029	1034.764045	13.833011
20.506891	1033.938940	13.838016
20.556842	1035.981172	13.843021
20.328554	1030.283335	13.848026
20.174034	1039.883987	13.853031
20.289553	1042.505589	13.858035
20.565666	1060.872357	13.863040
20.282998	1069.717544	13.868045
20.695348	1067.946954	13.873050
20.522823	1071.518169	13.878055
20.651747	1073.568313	13.883059
20.990818	1059.462456	13.888064
20.773635	1052.975877	13.893069
20.721580	1040.559965	13.898074
20.440904	1037.750224	13.903079
20.706314	1052.595501	13.908083
20.677905	1036.428684	13.913088
20.453831	1032.982239	13.918093
20.544454	1031.381248	13.923098
20.334115	1036.731119	13.928103
20.174532	1037.964612	13.933107
20.509562	1033.679882	13.938112
20.096803	1037.313061	13.943117
20.279974	1033.658149	13.948122
20.575652	1047.053992	13.953127
20.619560	1058.252128	13.958131
20.870356	1047.126847	13.963136
20.434347	1047.742057	13.968141
20.662543	1031.382920	13.973146
20.305198	1038.643998	13.978151
20.339574	1037.143447	13.983155
20.677699	1035.572372	13.988160
20.694857	1035.486050	13.993165
20.540575	1037.322718	13.998170
20.616413	1040.852737	14.003175
20.181807	1036.876853	14.008179
20.544656	1036.087218	14.013184
20.476275	1037.306165	14.018189
20.279275	1038.275550	14.023207
20.789407	1054.111922	14.028224
20.749766	1057.574247	14.033242
20.817934	1046.581880	14.038259
20.566618	1047.139499	14.043277
20.650723	1042.764007	14.048295
21.079567	1037.793975	14.053312
20.657350	1041.345629	14.058330
20.673386	1036.740318	14.063347
20.191150	1036.482172	14.068365
20.420374	1048.485765	14.073383
20.794848	1042.220342	14.078400
20.482856	1042.421116	14.083418
20.539631	1042.539478	14.088435
21.001592	1063.684735	14.093453
20.705899	1063.801111	14.098471
21.162677	1076.803506	14.103488
21.048424	1053.035548	14.108506
20.883308	1039.884409	14.113523
20.507280	1058.358558	14.118541
20.586807	1041.231042	14.123559
20.676563	1059.055165	14.128576
20.685395	1072.748784	14.133594
20.881430	1061.210611	14.138611
20.683112	1074.986036	14.143629
20.913024	1069.953338	14.148647
20.818162	1082.022806	14.153664
20.849234	1074.324027	14.158682
21.194972	1074.684171	14.163699
20.754385	1083.917503	14.168717
20.801284	1081.772238	14.173735
20.683759	1086.341840	14.178752
20.819084	1085.573054	14.183770
20.846920	1082.778010	14.188787
20.784891	1102.935644	14.193805
20.850993	1112.300543	14.198823
21.327160	1111.924144	14.203840
21.087327	1112.308469	14.208858
21.351302	1112.269514	14.213875
21.130300	1109.962474	14.218893
21.404401	1113.039711	14.223911
21.680551	1111.782837	14.228928
21.462719	1121.899333	14.233946
21.469696	1116.254074	14.238963
21.221497	1112.087295	14.243981
21.119888	1115.921321	14.248999
21.414802	1115.764170	14.254016
21.357012	1118.423997	14.259034
21.391402	1111.850980	14.264051
21.147660	1110.774556	14.269069
21.161749	1111.582436	14.274087
21.555838	1108.823355	14.279104
21.019199	1118.386640	14.284122
21.298800	1115.590761	14.289139
21.268189	1122.598916	14.294157
21.460651	1115.245617	14.299175
21.354127	1122.833754	14.304192
21.022501	1115.867644	14.309210
21.871815	1105.082562	14.314227
21.530375	1106.831206	14.319245
21.383984	1112.067678	14.324263
21.708066	1112.017563	14.329280
21.477806	1118.815307	14.334298
21.735039	1125.300916	14.339315
21.655977	1128.196950	14.344333
21.861167	1133.551965	14.349351
21.719131	1119.884255	14.354368
21.501562	1128.372594	14.359386
22.031669	1136.099878	14.364403
21.887499	1123.204879	14.369421
21.406984	1121.562161	14.374439
22.034267	1124.793860	14.379456
21.914194	1133.222606	14.384474
21.712782	1128.304301	14.389491
21.815245	1137.952861	14.394509
21.896122	1142.160493	14.399527
22.031173	1135.656357	14.404544
21.971428	1143.738851	14.409562
22.242465	1128.079820	14.414579
22.055178	1116.525661	14.419597
21.751231	1108.225903	14.424615
21.921700	1108.352874	14.429632
21.996645	1130.162437	14.434650
21.975499	1138.827098	14.439667
22.237565	1136.760768	14.444685
22.352558	1128.655309	14.449703
22.243263	1118.292102	14.454720
21.883188	1117.509517	14.459738
21.982269	1111.363494	14.464755
22.131156	1134.347358	14.469773
21.965422	1138.128695	14.474791
22.186350	1136.866469	14.479808
22.405048	1142.675522	14.484826
22.339233	1137.804801	14.489843
22.296103	1141.631081	14.494861
22.269962	1145.556900	14.499879
22.397793	1138.918631	14.504896
22.330678	1142.169848	14.509914
22.443012	1140.553698	14.514931
22.564128	1133.015137	14.519949
22.141715	1133.164308	14.524967
22.670720	1130.259434	14.529984
22.255995	1122.450828	14.535002
21.939642	1130.486151	14.540019
22.560598	1137.154432	14.545037
22.383829	1141.657994	14.550055
22.448869	1150.172059	14.555072
22.318286	1152.376301	14.560090
22.339132	1134.331500	14.565107
22.401445	1138.364336	14.570125
22.144071	1150.557310	14.575143
22.517446	1138.580222	14.580160
22.417114	1147.860001	14.585178
22.307808	1153.510582	14.590195
22.311795	1141.321839	14.595213
22.436660	1151.482801	14.600231
22.596447	1162.874629	14.605248
22.974317	1167.470640	14.610266
23.042880	1162.034198	14.615283
22.864847	1148.762322	14.620301
22.832939	1146.659504	14.625319
22.646429	1146.233063	14.630336
22.538137	1142.962630	14.635354
22.709237	1144.598070	14.640371
22.730557	1150.446472	14.645389
22.663387	1164.855460	14.650407
22.878172	1159.365809	14.655424
22.494829	1167.995444	14.660442
22.797835	1162.966787	14.665459
22.783874	1161.974836	14.670477
22.591693	1172.600095	14.675495
22.896931	1162.958849	14.680512
22.954529	1165.523200	14.685530
23.097364	1158.302067	14.690547
22.847049	1164.719202	14.695565
22.937748	1171.273866	14.700583
22.991865	1164.345312	14.705600
23.182950	1164.003369	14.710618
23.230818	1160.390266	14.715635
23.011753	1160.066547	14.720653
22.879936	1165.368356	14.725671
23.309613	1156.687287	14.730688
23.125828	1155.821525	14.735706
23.005561	1162.082634	14.740723
23.207742	1176.922167	14.745741
23.268944	1188.792222	14.750759
23.645945	1179.940211	14.755776
23.271432	1172.726077	14.760794
23.071215	1181.990348	14.765811
23.239217	1190.780606	14.770829
23.158144	1193.030442	14.775847
23.380181	1190.091143	14.780864
23.567098	1192.373744	14.785882
23.494241	1196.940975	14.790899
23.735370	1197.069263	14.795917
23.494268	1206.753788	14.800935
23.803327	1195.018153	14.805952
23.716197	1191.676692	14.810970
23.463583	1172.042612	14.815987
23.473989	1167.354785	14.821005
23.270201	1168.494728	14.826023
23.787819	1174.237241	14.831040
23.971852	1193.194832	14.836058
23.585490	1179.322207	14.841075
23.726757	1158.480131	14.846093
23.557179	1165.620584	14.851111
23.384086	1162.089915	14.856128
23.826219	1181.300488	14.861146
23.911220	1185.413091	14.866163
23.894797	1163.540629	14.871181
23.569516	1162.947552	14.876199
23.844518	1178.201773	14.881216
23.899090	1182.890252	14.886234
23.805615	1191.624684	14.891251
23.812929	1175.625407	14.896269
23.563522	1197.892655	14.901287
24.036132	1195.536326	14.906304
23.922829	1194.934607	14.911322
24.079707	1194.741268	14.916339
24.465039	1191.727159	14.921357
24.147077	1182.504629	14.926375
23.938875	1168.178871	14.931392
23.780404	1165.874434	14.936410
23.633977	1172.392983	14.941427
23.949367	1178.137864	14.946445
24.033431	1194.745506	14.951463
23.932331	1192.883386	14.956480
24.132743	1198.099184	14.961498
24.080343	1199.973204	14.966515
24.221834	1187.406977	14.971533
24.054044	1191.838334	14.976551
24.230933	1193.318696	14.981568
24.439452	1187.483958	14.986586
24.155484	1190.741457	14.991603
24.409992	1190.290295	14.996621
24.201926	1191.756546	15.001639
24.287504	1191.304011	15.006656
24.498141	1197.026280	15.011674
24.103330	1193.491639	15.016691
24.448365	1193.697738	15.021709
24.048296	1189.515831	15.026727
24.469506	1196.131053	15.031744
24.737958	1188.087604	15.036762
24.490888	1196.967663	15.041779
24.625410	1196.191135	15.046797
24.192424	1195.121290	15.051815
24.421878	1188.329933	15.056832
24.426375	1192.595381	15.061850
24.172579	1184.594329	15.066867
24.460800	1182.284714	15.071885
24.624764	1193.504437	15.076903
24.761392	1198.151518	15.081920
24.664741	1195.700360	15.086938
24.488532	1199.349672	15.091955
24.677211	1205.117919	15.096973
24.748750	1213.632558	15.101991
24.987068	1220.483820	15.107008
25.359607	1204.862788	15.112026
24.595191	1207.583421	15.117043
25.089797	1186.672365	15.122061
24.770054	1192.449335	15.127079
24.678205	1192.566234	15.132096
24.854058	1189.465982	15.137114
24.592762	1191.596694	15.142131
24.860266	1202.217873	15.147149
25.118652	1219.272808	15.152167
25.023536	1219.416971	15.157184
25.275622	1221.406029	15.162202
25.048455	1209.972991	15.167219
25.264876	1199.549911	15.172237
24.872439	1193.644274	15.177255
25.038522	1193.042042	15.182272
25.314277	1189.932148	15.187290
24.822307	1193.321926	15.192307
25.163136	1194.982213	15.197325
24.945466	1206.075618	15.202343
25.265032	1219.032383	15.207360
25.544259	1219.278867	15.212378
25.320694	1220.844338	15.217395
25.062751	1195.743862	15.222413
25.046264	1201.039874	15.227431
25.007381	1219.348766	15.232448
25.655560	1214.326389	15.237466
25.340658	1223.843366	15.242483
25.655761	1217.723408	15.247501
25.694756	1220.171183	15.252519
25.626306	1209.446669	15.257536
25.540634	1194.050531	15.262554
25.291143	1195.520244	15.267571
25.376482	1189.278850	15.272589
25.733366	1205.994007	15.277607
25.115235	1204.875037	15.282624
25.518006	1208.667970	15.287642
25.456725	1223.997897	15.292659
25.419048	1218.329832	15.297677
25.476462	1227.326519	15.302695
25.607471	1220.799394	15.307712
25.990723	1214.792055	15.312730
25.683724	1228.330120	15.317747
25.506356	1220.198091	15.322765
25.493467	1226.194343	15.327783
25.519569	1219.875078	15.332800
25.818665	1218.319585	15.337818
25.549919	1220.659921	15.342835
25.627247	1221.635478	15.347853
25.778792	1230.754012	15.352871
25.520955	1226.411765	15.357888
25.934848	1212.125175	15.362906
25.779051	1227.914573	15.367923
26.062110	1239.582540	15.372941
26.286337	1239.486215	15.377959
25.861405	1228.665167	15.382976
25.771632	1225.635588	15.387994
25.881087	1240.692116	15.393011
26.354511	1246.960036	15.398029
26.315440	1259.400650	15.403047
26.045058	1232.224847	15.408064
26.262754	1214.950030	15.413082
25.908519	1223.762251	15.418099
26.022852	1226.504761	15.423117
26.346268	1242.247632	15.428135
26.239577	1246.393186	15.433152
26.287695	1242.403271	15.438170
26.246222	1237.563242	15.443187
26.543405	1238.909589	15.448205
26.218588	1220.375527	15.453223
26.065587	1225.774334	15.458240
26.456349	1229.309631	15.463258
26.420323	1244.520717	15.468275
26.626240	1241.403075	15.473293
26.767097	1233.492427	15.478311
26.502855	1227.775547	15.483328
26.117270	1215.173807	15.488346
26.199493	1230.883561	15.493363
26.583673	1232.086253	15.498381
26.546962	1248.334894	15.503399
26.496419	1249.854682	15.508416
26.581242	1249.318106	15.513434
26.567566	1257.737820	15.518451
26.496897	1254.064946	15.523469
26.625586	1241.210482	15.528487
26.259895	1257.534413	15.533504
26.733534	1257.325948	15.538522
26.423828	1256.503859	15.543539
26.574739	1257.971067	15.548557
26.708975	1255.170818	15.553575
26.422737	1254.477912	15.558592
26.555979	1248.260314	15.563610
26.605513	1260.583761	15.568627
26.699231	1267.491142	15.573645
27.021192	1273.135123	15.578663
26.760964	1279.792997	15.583680
27.197105	1279.795799	15.588698
27.131474	1282.025882	15.593715
27.184437	1286.693415	15.598733
27.172568	1278.838562	15.603751
27.052734	1280.745370	15.608768
27.452269	1272.223203	15.613786
26.959975	1272.398464	15.618803
26.899748	1267.672318	15.623821
27.301739	1270.194345	15.628839
26.981254	1277.089139	15.633856
27.441572	1273.686302	15.638874
27.443805	1277.691005	15.643891
27.327662	1256.776580	15.648909
27.190850	1245.029432	15.653927
27.143511	1262.613753	15.658944
27.276446	1270.399737	15.663962
27.151814	1283.267737	15.668979
27.318122	1282.328040	15.673997
27.684962	1269.199608	15.679015
27.397382	1275.459134	15.684032
27.425183	1275.180985	15.689050
27.395192	1280.016695	15.694067
27.209341	1273.658850	15.699085
27.636917	1270.643493	15.704103
27.312216	1279.001923	15.709120
27.639669	1272.635359	15.714138
27.148273	1268.987110	15.719155
27.151269	1274.297345	15.724173
27.329049	1275.665099	15.729191
27.324263	1275.537657	15.734208
27.565218	1277.170623	15.739226
27.490741	1290.342101	15.744243
27.999938	1296.561864	15.749261
27.745055	1279.121662	15.754279
27.440891	1292.050553	15.759296
27.878276	1295.093135	15.764314
27.954480	1311.309680	15.769331
28.070739	1308.675889	15.774349
28.240111	1301.864959	15.779367
27.924161	1278.503981	15.784384
28.029850	1275.887612	15.789402
27.856150	1273.267825	15.794419
27.945032	1276.428122	15.799437
27.959201	1267.269760	15.804455
27.774697	1277.329136	15.809472
28.144055	1287.459063	15.814490
28.371246	1297.643921	15.819507
28.046782	1284.720115	15.824525
28.063593	1288.787779	15.829543
28.052616	1299.270968	15.834560
28.281541	1296.981805	15.839578
28.488398	1309.672686	15.844595
28.445627	1287.109724	15.849613
28.529146	1276.244515	15.854631
28.215146	1278.231842	15.859648
28.298912	1271.915156	15.864666
28.334578	1264.642634	15.869683
28.081003	1277.215006	15.874701
28.125813	1286.852410	15.879719
28.282293	1303.266150	15.884736
28.492832	1295.609419	15.889754
28.236127	1299.387215	15.894771
28.118770	1298.771195	15.899789
28.653874	1294.046049	15.904807
28.196939	1304.631043	15.909824
28.533651	1306.389531	15.914842
28.697564	1301.696842	15.919859
28.658904	1299.978911	15.924877
28.575890	1297.779612	15.929895
28.432210	1303.821138	15.934912
28.484517	1299.637051	15.939930
28.532433	1302.107799	15.944947
28.429026	1304.966064	15.949965
28.821307	1302.517921	15.954983
28.522688	1310.732991	15.960000
28.701503	1322.840810	15.965018
29.415408	1331.476445	15.970035
29.060069	1325.950242	15.975053
29.006074	1304.395030	15.980071
29.114343	1304.025392	15.985088
28.803189	1295.543411	15.990106
28.829625	1298.565017	15.995123
28.791858	1301.645629	16.000141
28.947001	1300.397815	16.005159
28.935188	1318.300592	16.010176
29.190551	1325.180647	16.015194
29.245584	1319.328650	16.020211
29.118202	1322.824695	16.025229
29.302970	1318.531383	16.030247
28.994379	1320.933148	16.035264
29.165400	1319.008733	16.040282
29.466261	1320.943621	16.045299
28.994345	1333.303890	16.050317
29.525234	1322.663822	16.055335
29.130373	1317.950130	16.060352
29.447567	1319.751061	16.065370
29.422903	1321.438195	16.070387
29.491720	1323.005022	16.075405
29.398116	1325.777568	16.080423
29.734019	1328.765554	16.085440
29.417283	1320.125568	16.090458
29.513441	1314.723994	16.095475
29.563024	1333.129036	16.100493
29.763271	1325.071221	16.105511
29.528409	1316.669872	16.110528
29.745452	1323.775483	16.115546
29.848117	1324.513404	16.120563
29.396477	1314.762315	16.125581
29.559714	1318.480219	16.130599
29.613800	1323.908171	16.135616
29.565330	1313.671196	16.140634
29.736090	1324.449473	16.145651
29.564553	1334.546933	16.150669
29.657208	1325.839290	16.155687
29.652679	1324.091529	16.160704
29.628881	1334.310937	16.165722
29.705130	1323.387862	16.170739
29.355642	1331.145423	16.175757
30.128490	1329.236711	16.180775
29.891622	1337.410486	16.185792
30.059949	1349.415390	16.190810
30.134005	1355.351422	16.195827
30.146134	1351.745545	16.200845
30.320892	1339.239165	16.205863
29.892022	1326.981658	16.210880
30.077445	1327.850316	16.215898
30.331791	1342.428433	16.220915
30.334211	1341.226996	16.225933
30.368196	1330.349197	16.230951
30.265540	1325.913741	16.235968
30.057786	1318.279665	16.240986
30.375159	1330.887656	16.246003
30.113313	1337.526937	16.251021
30.278221	1342.405518	16.256039
30.464192	1344.905381	16.261056
30.296916	1344.853406	16.266074
30.364482	1347.085851	16.271091
30.293452	1343.957300	16.276109
30.542470	1349.379341	16.281127
30.567672	1351.808888	16.286144
30.487822	1350.969010	16.291162
30.620719	1347.741864	16.296179
30.541766	1355.387075	16.301197
30.834427	1353.753941	16.306215
30.626896	1353.163311	16.311232
30.805485	1352.080860	16.316250
31.059111	1345.600979	16.321267
30.385942	1344.153347	16.326285
30.623281	1345.120696	16.331303
30.509095	1344.618217	16.336320
30.645463	1349.668886	16.341338
31.036286	1348.209653	16.346355
30.608268	1359.271439	16.351373
30.827781	1347.869300	16.356391
30.760983	1348.172548	16.361408
30.755040	1357.181781	16.366426
30.783846	1352.919626	16.371443
30.822735	1371.529350	16.376461
31.014917	1367.081465	16.381479
31.229438	1381.702941	16.386496
31.278050	1373.274438	16.391514
31.314605	1370.809870	16.396531
31.701580	1381.335832	16.401549
31.320162	1362.398466	16.406567
31.096896	1348.729336	16.411584
30.974697	1351.753422	16.416602
31.550214	1347.344297	16.421619
31.373740	1362.457565	16.426637
31.417608	1355.064922	16.431655
31.373147	1351.058281	16.436672
31.304693	1362.484310	16.441690
31.467587	1365.494391	16.446707
31.289846	1380.065950	16.451725
31.523071	1367.580110	16.456743
31.602151	1368.365841	16.461760
31.377170	1375.755129	16.466778
31.656248	1367.631234	16.471795
31.474044	1370.504438	16.476813
31.499798	1372.097803	16.481831
31.357193	1371.583338	16.486848
31.238719	1373.885573	16.491866
31.382801	1367.248541	16.496883
31.392136	1376.490525	16.501901
31.462264	1377.304426	16.506919
31.456424	1384.926194	16.511936
31.323037	1401.209302	16.516954
31.627257	1407.907778	16.521971
31.742311	1408.336187	16.526989
31.760832	1407.352410	16.532007
31.825564	1399.113239	16.537024
31.689025	1412.787103	16.542042
31.900253	1397.941958	16.547059
31.697970	1402.934968	16.552077
31.971083	1403.849423	16.557095
32.087543	1416.915841	16.562112
31.958126	1430.874889	16.567130
32.199062	1425.164667	16.572147
31.999785	1429.294363	16.577165
32.407821	1432.526495	16.582183
32.395149	1430.809910	16.587200
32.348875	1435.704113	16.592218
32.713947	1427.734790	16.597235
32.512123	1422.184851	16.602253
32.257819	1407.546084	16.607271
32.403491	1402.194786	16.612288
32.385604	1407.149736	16.617306
32.108340	1402.685473	16.622323
31.815483	1423.080148	16.627341
32.139991	1423.653698	16.632359
32.804376	1428.587147	16.637376
32.595442	1421.503001	16.642394
33.027271	1424.375817	16.647411
32.725118	1428.086960	16.652429
32.804076	1424.136123	16.657447
33.081385	1419.928701	16.662464
32.884517	1424.097339	16.667482
32.800683	1420.675858	16.672499
33.039634	1422.899072	16.677517
32.730064	1410.773483	16.682535
32.777677	1416.167107	16.687552
32.811663	1427.438416	16.692570
33.008919	1425.151925	16.697587
33.018707	1422.631839	16.702605
33.042715	1420.718274	16.707623
33.161346	1420.650588	16.712640
32.835921	1416.549521	16.717658
33.310015	1415.686575	16.722675
32.844090	1407.872608	16.727693
33.093823	1412.219350	16.732711
33.286111	1418.691066	16.737728
33.073315	1427.302305	16.742746
33.376151	1416.413811	16.747763
33.104726	1428.944327	16.752781
33.003456	1423.636338	16.757799
33.327745	1418.393406	16.762816
33.306948	1425.296317	16.767834
33.464032	1416.191362	16.772851
33.419107	1419.041109	16.777869
33.388342	1421.355319	16.782887
33.291248	1422.026785	16.787904
33.312774	1418.951099	16.792922
33.188198	1416.959767	16.797939
33.393693	1424.341774	16.802957
33.520614	1411.713968	16.807975
33.824172	1415.731216	16.812992
33.729488	1426.287624	16.818010
33.613535	1417.382738	16.823027
33.563065	1421.248802	16.828045
33.754915	1413.618587	16.833063
33.628680	1410.446913	16.838080
33.283872	1424.636158	16.843098
33.453510	1418.662019	16.848115
33.587834	1431.737399	16.853133
34.056595	1445.111826	16.858151
33.752889	1457.324243	16.863168
33.937112	1460.019469	16.868186
34.372932	1443.315237	16.873203
33.867821	1435.796954	16.878221
33.869567	1439.309400	16.883239
34.302240	1447.063406	16.888256
34.164786	1458.429725	16.893274
34.184447	1439.720099	16.898291
34.192816	1423.351490	16.903309
33.910717	1433.591713	16.908327
34.224516	1447.938648	16.913344
34.270276	1448.755653	16.918362
34.305567	1448.206520	16.923379
34.357142	1452.519595	16.928397
34.596314	1451.951316	16.933415
34.723901	1443.238818	16.938432
34.273038	1429.825358	16.943450
34.313880	1425.787787	16.948467
34.318031	1445.346217	16.953485
34.339667	1448.256930	16.958503
34.568973	1449.100507	16.963520
34.672007	1449.283858	16.968538
34.691168	1449.792846	16.973555
34.725217	1456.047560	16.978573
34.829464	1445.779055	16.983591
35.087864	1440.692136	16.988608
34.510513	1433.097281	16.993626
34.826811	1430.121664	16.998643
34.962586	1442.230942	17.003661
34.614968	1439.752125	17.008679
35.066554	1432.390375	17.013696
34.906465	1444.822133	17.018714
34.709511	1435.580927	17.023731
34.736517	1452.506291	17.028749
34.600480	1453.110034	17.033767
35.085452	1444.390089	17.038784
34.680447	1445.176735	17.043802
34.736842	1447.108943	17.048819
34.813987	1444.677216	17.053837
34.715123	1450.490635	17.058855
34.728726	1447.112598	17.063872
35.003653	1462.518936	17.068890
35.183460	1468.214768	17.073907
35.354162	1470.477977	17.078925
34.999039	1484.289807	17.083943
35.490752	1472.741908	17.088960
35.358891	1469.478306	17.093978
35.348215	1473.351408	17.098995
35.325085	1472.713272	17.104013
35.355382	1479.730762	17.109031
35.492973	1476.782064	17.114048
35.651491	1474.124986	17.119066
35.631904	1469.348246	17.124083
35.761377	1467.623930	17.129101
35.329929	1477.706310	17.134119
35.799985	1463.285458	17.139136
35.607073	1477.452888	17.144154
35.573593	1470.343095	17.149171
35.458455	1468.815888	17.154189
35.559225	1474.892433	17.159207
35.550662	1474.334562	17.164224
35.371721	1472.255934	17.169242
35.590811	1484.888387	17.174259
36.013791	1493.800193	17.179277
36.122614	1507.366584	17.184295
36.532106	1489.951523	17.189312
36.259014	1482.846117	17.194330
36.090990	1467.917449	17.199347
36.091182	1465.170787	17.204365
35.927111	1470.096374	17.209383
36.140809	1463.825739	17.214400
35.737401	1469.571327	17.219418
35.916551	1482.418583	17.224435
36.041374	1486.509976	17.229453
36.055258	1507.319913	17.234471
36.420692	1487.742571	17.239488
36.721067	1495.361965	17.244506
36.488139	1504.933693	17.249523
36.590825	1494.571017	17.254541
36.661339	1497.265508	17.259559
36.652808	1499.119198	17.264576
36.495746	1498.347471	17.269594
36.693848	1502.171553	17.274611
36.700283	1498.579133	17.279629
36.263463	1503.258779	17.284647
36.589537	1497.783502	17.289664
36.456959	1504.219762	17.294682
36.322510	1498.721972	17.299699
36.637916	1505.719173	17.304717
36.409644	1505.773670	17.309735
36.571811	1502.511146	17.314752
36.443534	1503.660307	17.319770
36.711351	1519.998330	17.324787
37.111190	1528.288540	17.329805
36.791144	1530.789697	17.334823
37.102787	1533.645522	17.339840
37.122636	1533.112220	17.344858
36.905268	1533.873663	17.349875
37.329926	1519.327068	17.354893
37.117696	1523.380201	17.359911
37.122653	1529.410699	17.364928
37.006185	1531.127443	17.369946
36.835212	1528.050186	17.374963
37.145422	1523.231842	17.379981
37.100567	1533.355642	17.384999
37.163958	1525.922044	17.390016
37.326674	1523.058997	17.395034
37.348284	1529.701923	17.400051
37.325438	1522.479505	17.405069
37.248319	1523.647251	17.410087
37.532874	1514.628090	17.415104
37.356937	1526.455227	17.420122
37.094808	1522.426623	17.425139
37.799873	1534.679576	17.430157
38.071928	1534.754957	17.435175
38.398512	1517.438820	17.440192
38.331733	1509.093140	17.445210
37.960208	1515.746847	17.450227
38.015720	1503.022593	17.455245
38.170362	1509.932172	17.460263
38.115397	1507.070024	17.465280
38.376660	1491.501042	17.470298
38.012967	1496.134416	17.475315
38.185067	1467.979132	17.480333
37.851783	1475.765647	17.485351
38.035779	1471.429154	17.490368
37.961854	1475.141663	17.495386
37.869814	1474.304508	17.500403
38.328235	1488.600890	17.505421
38.111623	1500.521013	17.510439
38.349924	1498.820238	17.515456
38.208198	1499.423317	17.520474
38.398398	1506.609595	17.525491
38.473291	1498.977538	17.530509
38.232686	1501.715357	17.535527
38.355091	1508.243093	17.540544
38.447499	1503.610509	17.545562
38.191947	1506.842308	17.550579
38.489888	1504.619188	17.555597
38.120661	1510.253942	17.560615
38.125715	1496.446794	17.565632
38.463771	1509.744595	17.570650
38.403299	1509.071512	17.575667
38.728607	1503.535004	17.580685
38.695573	1509.286035	17.585703
38.541301	1506.745694	17.590720
38.772177	1503.990549	17.595738
38.536584	1506.516774	17.600755
38.698056	1517.848836	17.605773
38.979492	1532.019322	17.610791
38.784920	1551.156533	17.615808
38.853338	1542.260707	17.620826
38.641663	1546.699169	17.625843
38.892192	1542.472387	17.630861
38.905312	1543.519558	17.635879
39.084561	1545.146666	17.640896
38.966840	1542.605209	17.645914
38.832704	1537.860873	17.650931
38.978033	1535.500058	17.655949
38.867054	1539.973584	17.660967
38.951539	1544.883938	17.665984
39.441978	1546.363884	17.671002
39.104923	1553.707425	17.676019
39.450807	1551.456202	17.681037
39.272413	1563.310503	17.686055
39.504876	1555.690254	17.691072
39.591622	1553.483506	17.696090
39.332531	1560.845292	17.701107
39.691743	1556.860735	17.706125
39.865476	1563.156142	17.711143
39.856936	1553.946162	17.716160
39.751293	1555.257680	17.721178
39.693740	1562.467768	17.726195
39.888111	1554.721453	17.731213
39.817244	1557.491203	17.736231
39.462348	1558.636396	17.741248
39.443375	1561.542596	17.746266
39.484977	1562.510504	17.751283
39.879716	1549.002971	17.756301
39.766326	1558.359030	17.761319
39.623262	1554.832913	17.766336
39.905829	1559.909106	17.771354
39.794106	1576.585378	17.776371
39.910795	1581.931079	17.781389
39.917445	1592.781350	17.786407
39.947626	1583.978118	17.791424
40.322972	1588.779960	17.796442
40.309015	1597.623869	17.801459
40.169347	1586.490413	17.806477
40.157844	1591.616663	17.811495
40.243118	1591.640818	17.816512
40.595787	1588.960621	17.821530
40.078310	1590.296922	17.826547
40.433783	1584.598262	17.831565
40.134796	1588.408831	17.836583
40.251548	1603.504686	17.841600
40.849590	1601.948671	17.846618
40.926361	1616.088170	17.851635
41.039501	1610.812774	17.856653
40.818846	1598.085288	17.861671
40.389212	1591.855850	17.866688
40.864724	1596.270465	17.871706
40.506133	1605.470594	17.876723
41.089517	1616.280028	17.881741
41.027085	1609.960556	17.886759
40.764116	1610.885013	17.891776
41.241600	1603.698383	17.896794
41.319557	1609.887169	17.901811
41.394032	1610.276436	17.906829
41.328243	1591.812277	17.911847
40.790035	1591.326287	17.916864
41.178829	1579.449420	17.921882
41.024165	1600.881008	17.926899
41.175578	1597.921430	17.931917
41.230435	1594.805782	17.936935
41.048568	1604.533821	17.941952
41.620886	1602.575259	17.946970
41.386207	1603.709934	17.951987
41.494680	1600.584161	17.957005
41.421953	1606.171664	17.962023
41.330728	1605.325720	17.967040
41.693727	1605.458175	17.972058
41.251317	1605.045000	17.977075
41.610904	1605.423405	17.982093
41.487146	1604.642427	17.987111
41.595575	1604.043869	17.992128
42.016823	1599.609722	17.997146
41.614810	1598.292644	18.002163
41.608766	1597.607730	18.007181
41.622288	1596.816658	18.012199
41.763248	1601.080912	18.017216
41.822842	1611.709597	18.022234
41.552855	1635.571999	18.027251
42.183303	1636.615110	18.032269
42.387511	1623.816696	18.037287
41.962889	1630.908384	18.042304
42.411140	1629.867855	18.047322
42.699166	1624.220051	18.052339
42.259361	1614.932512	18.057357
42.327528	1610.111054	18.062375
42.222567	1610.384212	18.067392
42.487296	1615.420795	18.072410
42.411608	1626.723122	18.077427
42.223578	1624.865371	18.082445
42.552996	1621.730312	18.087463
41.966168	1627.214973	18.092480
42.490038	1627.287163	18.097498
42.646315	1630.498928	18.102515
42.657729	1632.900832	18.107533
42.421014	1626.040466	18.112551
42.382408	1627.925711	18.117568
42.472250	1622.262322	18.122586
42.584988	1627.443492	18.127603
42.481809	1627.479612	18.132621
42.670435	1630.904882	18.137639
42.472397	1651.593871	18.142656
42.838827	1647.763091	18.147674
42.975680	1652.098806	18.152691
42.911414	1655.940389	18.157709
42.889409	1646.211009	18.162727
43.133646	1651.529315	18.167744
42.901265	1651.640313	18.172762
42.859823	1652.899126	18.177779
43.053687	1653.312615	18.182797
43.302849	1648.707685	18.187815
43.041925	1652.681311	18.192832
43.498917	1648.248528	18.197850
43.385498	1657.643983	18.202867
43.155101	1647.364210	18.207885
43.326721	1659.327945	18.212903
43.658501	1683.387054	18.217920
43.635903	1674.554430	18.222938
43.420415	1677.374010	18.227955
43.862176	1686.175182	18.232973
43.990215	1673.099418	18.237991
43.741435	1663.592608	18.243008
43.443727	1667.916618	18.248026
43.714467	1668.770906	18.253043
43.649697	1678.300197	18.258061
43.914160	1668.974240	18.263079
43.802223	1676.123841	18.268096
43.962313	1669.868747	18.273114
43.643418	1675.523852	18.278131
43.777280	1684.391433	18.283149
44.308220	1672.533509	18.288167
43.980814	1672.621907	18.293184
44.156111	1679.016222	18.298202
44.259767	1674.576857	18.303219
44.162108	1667.477990	18.308237
44.520093	1675.218076	18.313255
44.146874	1675.799088	18.318272
44.571356	1667.707684	18.323290
44.232219	1665.877958	18.328307
44.315408	1667.835812	18.333325
44.591909	1659.964652	18.338343
44.181970	1673.105815	18.343360
44.630139	1682.046757	18.348378
44.572975	1698.510749	18.353395
44.595839	1694.641936	18.358413
44.947553	1700.809911	18.363431
44.898488	1692.694909	18.368448
45.057541	1690.474248	18.373466
44.926272	1673.990766	18.378483
44.609196	1671.963240	18.383501
44.909687	1680.666596	18.388519
45.008768	1689.313984	18.393536
44.819728	1704.980204	18.398554
45.308566	1699.073028	18.403571
44.892894	1701.206408	18.408589
45.282434	1699.292715	18.413607
45.196680	1704.922448	18.418624
45.304641	1697.653911	18.423642
45.151662	1696.833541	18.428659
45.036715	1698.696363	18.433677
45.308650	1694.053965	18.438695
45.110013	1693.491004	18.443712
45.309622	1690.128080	18.448730
45.206264	1695.353964	18.453747
45.316094	1695.100480	18.458765
45.321083	1687.544758	18.463783
45.218559	1696.430382	18.468800
45.528158	1699.951999	18.473818
45.764449	1717.316232	18.478835
45.599750	1724.408199	18.483853
46.023423	1721.241570	18.488871
46.466346	1713.525536	18.493888
45.743459	1704.830534	18.498906
45.376767	1697.978278	18.503923
45.597211	1706.123371	18.508941
45.910523	1711.404727	18.513959
45.753392	1727.951552	18.518976
46.090767	1727.541433	18.523994
46.076709	1716.847198	18.529011
45.735311	1729.514193	18.534029
46.213225	1715.548048	18.539047
45.981831	1726.462339	18.544064
46.354193	1721.044096	18.549082
46.496214	1717.554274	18.554099
46.164274	1719.580701	18.559117
46.423999	1710.057261	18.564135
46.043440	1719.290067	18.569152
46.275518	1715.964434	18.574170
46.791533	1725.503384	18.579187
46.550209	1732.999284	18.584205
46.684802	1728.456649	18.589223
47.228600	1730.364649	18.594240
47.034797	1711.396903	18.599258
46.672781	1710.992926	18.604275
46.612397	1712.641754	18.609293
47.034730	1707.819627	18.614311
46.756052	1710.374780	18.619328
46.652262	1707.637577	18.624346
46.966684	1716.163329	18.629363
46.886104	1738.568081	18.634381
47.425128	1730.478038	18.639399
47.288676	1726.767555	18.644416
47.335746	1730.530836	18.649434
47.377115	1723.239084	18.654451
47.059480	1713.434889	18.659469
47.302388	1717.086705	18.664487
47.144098	1725.541551	18.669504
47.287351	1731.262982	18.674522
47.514898	1733.574587	18.679539
47.425165	1735.385411	18.684557
47.333526	1729.006833	18.689575
46.956086	1734.738942	18.694592
46.984869	1736.670873	18.699610
47.342371	1735.310522	18.704627
47.468337	1737.686308	18.709645
47.781735	1756.381742	18.714663
47.848814	1771.675256	18.719680
47.978408	1768.554732	18.724698
48.287819	1755.139275	18.729715
47.754421	1751.015432	18.734733
47.573812	1737.900739	18.739751
47.896819	1749.423526	18.744768
47.939008	1760.582093	18.749786
47.818361	1756.308260	18.754803
48.035891	1765.182998	18.759821
48.157684	1759.113310	18.764839
48.054784	1757.488946	18.769856
48.172370	1770.101654	18.774874
48.178211	1761.255003	18.779891
47.957635	1764.389250	18.784909
48.165749	1757.992744	18.789927
48.274014	1766.267454	18.794944
48.442183	1784.700563	18.799962
48.347086	1787.253195	18.804979
48.255439	1790.731067	18.809997
48.472920	1787.373136	18.815015
48.422778	1789.504865	18.820032
48.404754	1788.510373	18.825050
48.432107	1785.224453	18.830067
48.378101	1793.209645	18.835085
48.643546	1809.487808	18.840103
48.859936	1816.399484	18.845120
48.616150	1816.544551	18.850138
49.005774	1821.904232	18.855155
48.873484	1831.577321	18.860173
49.427866	1817.462808	18.865191
49.440495	1819.255744	18.870208
49.247550	1826.058875	18.875226
49.564730	1818.107992	18.880243
49.373878	1820.510722	18.885261
49.594349	1811.393839	18.890279
49.499882	1821.605982	18.895296
49.698101	1812.974028	18.900314
49.760981	1810.013582	18.905331
49.678141	1803.840435	18.910349
49.691743	1793.081953	18.915367
49.754321	1786.887195	18.920384
49.471105	1790.155715	18.925402
49.727279	1797.099580	18.930419
49.859377	1804.957563	18.935437
49.208160	1816.874891	18.940455
49.514407	1815.641479	18.945472
49.674123	1813.654305	18.950490
50.038469	1801.934539	18.955507
49.931959	1807.007585	18.960525
49.859874	1816.538919	18.965543
50.222960	1805.498160	18.970560
49.840815	1813.424789	18.975578
50.175012	1812.922360	18.980595
50.132608	1813.174533	18.985613
49.891872	1807.463111	18.990631
50.202419	1813.257788	18.995648
50.465297	1823.583628	19.000666
50.683356	1824.278788	19.005683
50.481261	1838.790190	19.010701
50.593971	1826.793548	19.015719
50.400197	1816.389041	19.020736
50.079428	1837.169444	19.025754
50.570841	1837.235802	19.030771
50.414639	1837.598939	19.035789
50.704969	1835.870951	19.040807
50.799976	1831.005811	19.045824
50.449430	1837.822283	19.050842
50.555383	1828.678819	19.055859
50.556454	1839.368130	19.060877
50.579685	1841.098026	19.065895
50.919797	1858.715664	19.070912
50.985257	1865.385573	19.075930
51.096856	1863.690020	19.080947
51.284439	1868.714612	19.085965
51.195493	1863.174817	19.090983
51.377625	1862.920025	19.096000
51.081849	1865.521193	19.101018
51.394662	1856.808012	19.106035
51.337305	1867.408340	19.111053
51.460094	1858.603544	19.116071
51.492528	1857.466497	19.121088
51.498801	1863.967293	19.126106
51.715648	1856.655355	19.131123
51.296322	1865.523961	19.136141
51.546844	1861.342710	19.141159
51.742159	1854.654812	19.146176
51.508156	1875.661336	19.151194
51.899437	1874.832027	19.156211
51.661541	1885.736461	19.161229
51.798827	1890.660535	19.166247
52.155465	1885.704885	19.171264
51.930172	1897.206686	19.176282
52.419281	1882.313588	19.181299
52.186077	1888.569421	19.186317
52.199200	1892.074656	19.191335
52.437580	1887.831622	19.196352
52.041810	1883.161147	19.201370
52.561816	1885.457598	19.206387
52.332267	1898.482883	19.211405
52.261671	1890.984731	19.216423
52.485310	1885.692401	19.221440
51.950860	1897.905801	19.226458
52.184073	1886.721299	19.231475
52.071501	1899.746021	19.236493
52.410378	1914.316739	19.241511
52.469568	1915.719200	19.246528
52.512175	1917.631647	19.251546
52.720957	1912.694848	19.256563
52.543032	1926.274325	19.261581
52.427261	1923.221215	19.266599
53.325206	1921.521380	19.271616
52.996997	1941.255400	19.276634
52.861086	1934.254532	19.281651
53.031923	1944.964041	19.286669
53.139962	1938.816242	19.291687
53.354430	1936.343656	19.296704
53.548587	1942.490455	19.301722
53.771569	1933.272415	19.306739
53.688356	1941.198632	19.311757
53.580917	1931.674611	19.316775
53.622341	1919.379351	19.321792
53.305059	1923.786786	19.326810
53.537692	1927.023410	19.331827
53.842018	1928.717139	19.336845
53.758300	1932.484026	19.341863
54.049347	1933.373635	19.346880
53.626871	1929.773213	19.351898
54.089802	1926.243963	19.356915
53.804035	1930.901225	19.361933
53.936252	1931.201062	19.366951
54.069801	1925.790154	19.371968
53.649248	1930.353285	19.376986
54.099923	1920.777232	19.382003
54.104655	1927.150877	19.387021
53.891493	1936.267453	19.392039
53.976605	1924.242882	19.397056
53.890982	1932.127791	19.402074
53.819500	1924.739883	19.407091
54.037520	1943.965190	19.412109
54.069675	1949.405526	19.417127
54.393481	1954.819016	19.422144
54.528535	1966.821872	19.427162
54.438437	1958.099736	19.432179
54.476938	1965.003671	19.437197
54.517228	1960.580618	19.442215
54.451089	1958.637311	19.447232
55.046568	1972.138323	19.452250
55.141818	1961.985731	19.457267
55.535763	1958.367580	19.462285
55.533032	1942.816624	19.467303
56.047448	1926.524060	19.472320
55.812425	1929.372760	19.477338
55.772728	1919.365211	19.482355
55.887525	1902.982235	19.487373
55.579978	1897.555947	19.492391
55.715363	1886.903038	19.497408
55.849734	1892.559091	19.502426
55.999259	1888.792732	19.507443
55.946573	1894.772795	19.512461
55.412955	1878.627760	19.517479
55.636882	1866.751784	19.522496
55.643694	1878.589390	19.527514
55.312806	1887.603578	19.532531
55.657123	1886.559945	19.537549
55.796397	1889.709982	19.542567
55.863818	1886.029083	19.547584
55.714058	1890.160449	19.552602
55.856439	1888.601566	19.557619
56.077640	1888.241435	19.562637
55.706574	1890.434584	19.567655
56.152484	1886.857717	19.572672
55.877538	1892.344648	19.577690
55.788955	1885.020054	19.582707
56.183948	1884.739181	19.587725
55.830443	1884.941074	19.592743
56.250861	1905.218736	19.597760
56.206342	1919.749923	19.602778
56.330611	1922.248716	19.607795
56.595337	1915.024289	19.612813
56.335502	1932.077760	19.617831
56.723765	1922.303217	19.622848
56.646355	1923.896578	19.627866
56.539396	1922.257110	19.632883
56.566991	1924.760309	19.637901
56.333910	1925.895539	19.642919
56.695011	1928.966946	19.647936
56.739954	1943.342305	19.652954
57.067555	1947.937936	19.657971
56.921458	1942.824897	19.662989
56.601772	1950.862771	19.668007
57.146639	1951.212426	19.673024
56.999936	1947.017416	19.678042
56.744760	1949.626282	19.683059
56.941959	1952.402909	19.688077
56.998478	1968.932453	19.693095
57.278376	1969.493480	19.698112
57.122966	1974.797771	19.703130
57.516815	1973.795001	19.708147
57.350237	1982.481784	19.713165
57.224465	1978.574461	19.718183
57.431784	1972.172483	19.723200
57.235844	1989.651595	19.728218
57.173810	2007.334334	19.733235
57.688089	2004.797405	19.738253
57.320908	2009.713875	19.743271
57.889238	2020.058788	19.748288
57.765062	2038.350062	19.753306
58.045407	2037.005923	19.758323
58.234809	2029.443424	19.763341
58.246208	2039.255771	19.768359
58.784297	2028.959357	19.773376
58.700232	2035.709825	19.778394
58.360693	2039.358648	19.783411
58.629939	2031.445972	19.788429
58.492133	2035.923141	19.793447
58.731296	2026.818089	19.798464
59.014827	2041.573957	19.803482
58.660904	2021.471920	19.808499
58.807870	2006.817320	19.813517
58.602377	2020.304531	19.818535
58.668285	2020.149290	19.823552
58.790249	2024.912245	19.828570
59.186692	2027.372371	19.833587
59.223612	2019.441691	19.838605
58.888983	2032.880290	19.843623
59.008498	2029.047102	19.848640
59.099122	2028.367990	19.853658
59.161174	2024.208885	19.858675
59.313442	2018.754056	19.863693
59.046663	2022.934797	19.868711
59.201696	2024.367606	19.873728
59.581301	2021.569770	19.878746
59.400171	2019.066657	19.883763
59.518553	2019.412751	19.888781
59.262302	2021.180946	19.893799
59.305153	2020.264827	19.898816
59.608299	2026.228312	19.903834
59.660301	2045.911277	19.908851
59.702076	2044.164698	19.913869
59.537822	2056.710908	19.918887
59.621115	2056.062067	19.923904
59.924409	2047.031726	19.928922
59.743678	2045.154664	19.933939
59.918818	2039.509759	19.938957
59.749614	2049.708023	19.943975
59.987250	2066.307902	19.948992
60.108125	2077.646877	19.954010
60.146069	2080.473311	19.959027
60.671987	2077.552235	19.964045
60.357173	2084.350536	19.969063
60.549558	2085.812004	19.974080
60.758636	2077.984410	19.979098
60.712604	2080.035294	19.984115
60.818314	2076.196430	19.989133
60.753119	2077.739878	19.994151
60.700504	2067.610007	19.999168
60.804766	2072.118588	20.004186
60.715809	2075.200447	20.009203
60.686160	2061.045122	20.014221
60.645246	2079.960302	20.019239
60.763055	2099.639137	20.024256
60.926865	2103.778763	20.029274
60.672867	2103.359905	20.034291
61.205623	2099.928814	20.039309
60.948544	2105.409829	20.044327
60.952963	2111.026124	20.049344
61.037156	2123.787623	20.054362
61.266235	2137.354303	20.059379
61.536346	2133.062090	20.064397
61.567746	2137.188232	20.069415
61.649215	2135.614653	20.074432
61.941144	2127.808430	20.079450
61.502284	2135.453238	20.084467
61.846449	2129.741228	20.089485
61.713906	2134.855509	20.094503
61.794765	2140.359728	20.099520
62.306358	2146.844564	20.104538
62.121464	2156.192744	20.109555
62.249260	2153.357170	20.114573
62.198371	2152.919291	20.119591
62.194542	2156.262896	20.124608
62.243917	2155.311118	20.129626
62.782650	2160.065861	20.134643
62.849129	2157.815846	20.139661
62.654773	2142.111961	20.144679
62.580748	2125.029684	20.149696
62.700154	2116.443158	20.154714
62.345574	2126.862965	20.159731
62.860671	2129.271936	20.164749
62.866931	2146.871587	20.169767
62.772876	2149.060712	20.174784
62.967678	2150.558771	20.179802
63.167087	2153.692982	20.184819
63.270118	2145.299404	20.189837
62.985388	2150.818668	20.194855
63.053666	2149.537442	20.199872
63.299683	2143.599597	20.204890
63.069864	2145.929147	20.209907
63.309937	2142.842839	20.214925
63.204232	2145.449140	20.219943
63.112384	2146.755363	20.224960
63.229312	2149.308854	20.229978
62.843586	2168.759742	20.234995
63.128763	2156.416757	20.240013
63.110269	2175.826395	20.245031
63.013126	2181.462847	20.250048
63.362404	2187.704573	20.255066
63.352114	2204.530570	20.260083
63.863972	2209.391872	20.265101
63.939607	2201.886757	20.270119
63.776534	2207.712289	20.275136
64.439341	2212.816960	20.280154
64.603269	2214.323095	20.285171
64.510982	2195.366844	20.290189
64.496667	2199.827515	20.295207
64.659645	2197.849210	20.300224
64.793625	2193.032797	20.305242
64.477196	2194.875896	20.310259
64.717772	2188.570777	20.315277
64.872292	2192.022071	20.320295
64.671928	2184.184205	20.325312
64.681946	2187.472908	20.330330
64.562042	2189.435691	20.335347
64.620806	2192.723700	20.340365
65.252266	2207.170182	20.345383
65.259535	2220.779393	20.350400
65.536452	2211.113660	20.355418
65.270641	2203.961114	20.360435
65.392719	2183.943406	20.365453
65.311853	2187.072767	20.370471
65.417891	2182.741418	20.375488
65.272196	2175.772670	20.380506
65.223757	2180.237991	20.385523
65.634992	2199.704984	20.390541
65.782356	2205.383471	20.395559
65.499416	2209.413457	20.400576
65.653765	2197.122765	20.405594
65.456822	2214.873679	20.410611
65.808842	2204.660306	20.415629
66.181788	2210.750390	20.420647
65.863479	2203.128756	20.425664
66.141611	2206.392798	20.430682
66.045703	2213.847660	20.435699
66.383953	2204.806143	20.440717
66.276418	2202.796251	20.445735
66.269787	2204.231262	20.450752
66.225708	2207.012593	20.455770
66.128189	2213.215462	20.460787
66.206277	2204.458490	20.465805
66.724374	2206.037144	20.470823
66.624414	2206.090842	20.475840
66.527910	2210.754979	20.480858
66.502565	2206.078025	20.485875
66.721140	2203.569344	20.490893
66.592366	2209.121179	20.495911
66.606541	2227.038234	20.500928
66.973818	2226.948986	20.505946
66.811048	2236.001864	20.510963
66.964007	2231.975295	20.515981
67.374342	2234.349077	20.520999
67.259579	2240.827654	20.526016
67.057317	2233.398304	20.531034
66.785458	2240.330627	20.536051
66.944784	2235.272607	20.541069
67.347163	2255.855687	20.546087
67.100503	2265.227945	20.551104
67.584588	2270.339114	20.556122
67.391720	2275.756463	20.561139
67.516380	2269.062340	20.566157
67.575859	2261.420544	20.571175
67.412110	2281.804478	20.576192
67.737083	2280.573549	20.581210
67.510311	2294.277573	20.586227
68.110984	2281.535708	20.591245
68.331121	2284.050740	20.596263
68.231335	2280.145483	20.601280
68.750319	2274.238781	20.606298
68.377582	2276.447196	20.611315
68.110902	2280.451011	20.616333
68.134802	2283.634478	20.621351
68.226429	2288.831838	20.626368
68.840989	2291.983253	20.631386
68.633187	2305.252422	20.636403
68.847158	2302.339362	20.641421
68.599684	2308.016355	20.646439
69.046745	2317.532873	20.651456
69.157546	2299.834115	20.656474
69.046295	2308.374614	20.661491
68.931365	2311.411896	20.666509
69.152614	2298.703780	20.671527
69.380189	2304.722696	20.676544
69.514057	2306.236781	20.681562
69.442300	2306.638376	20.686579
69.019051	2300.441431	20.691597
69.382027	2298.262101	20.696615
69.212292	2306.785181	20.701632
69.273375	2302.869210	20.706650
69.427998	2304.941614	20.711667
69.195427	2297.885191	20.716685
69.281547	2308.964806	20.721703
69.530624	2324.258195	20.726720
69.645012	2325.745498	20.731738
69.365365	2334.620426	20.736755
69.622971	2330.836719	20.741773
69.731985	2340.466943	20.746791
69.790523	2360.102093	20.751808
70.171863	2357.184357	20.756826
70.296757	2373.528044	20.761843
69.853576	2371.676273	20.766861
70.159105	2367.910085	20.771879
70.305863	2378.208430	20.776896
70.471463	2383.347618	20.781914
70.377577	2401.274253	20.786931
70.700334	2394.796260	20.791949
70.768080	2388.170940	20.796967
70.894886	2399.156823	20.801984
70.990855	2397.779914	20.807002
71.122921	2389.716657	20.812019
71.040766	2389.868987	20.817037
71.012680	2388.112270	20.822055
70.973352	2392.311119	20.827072
71.080158	2386.823286	20.832090
71.114270	2404.076635	20.837107
71.651766	2411.993008	20.842125
71.897158	2408.257638	20.847143
71.679877	2421.109951	20.852160
71.917268	2415.956827	20.857178
71.950620	2415.898020	20.862195
71.817576	2406.985812	20.867213
72.105129	2395.995200	20.872231
71.973407	2387.541382	20.877248
72.108906	2385.357412	20.882266
72.123494	2385.416441	20.887283
72.263674	2393.374139	20.892301
72.690858	2389.940942	20.897319
71.992489	2393.117692	20.902336
72.044214	2388.610880	20.907354
72.194001	2404.171112	20.912371
71.949269	2409.376533	20.917389
72.467149	2407.625566	20.922407
72.712853	2404.650791	20.927424
72.759653	2402.681546	20.932442
72.585804	2405.121774	20.937459
72.454055	2407.786549	20.942477
73.109694	2399.197722	20.947495
72.602127	2406.255024	20.952512
72.692683	2400.769778	20.957530
72.938858	2410.622021	20.962547
72.898103	2420.674989	20.967565
73.401723	2429.457315	20.972583
73.005070	2439.570198	20.977600
73.101035	2430.813386	20.982618
73.217561	2433.989981	20.987635
73.301071	2437.949791	20.992653
73.260807	2430.024118	20.997671
73.275163	2443.976151	21.002688
73.426267	2453.850664	21.007706
73.689392	2460.181763	21.012723
73.639929	2467.424831	21.017741
73.743376	2458.411163	21.022759
73.626598	2464.242786	21.027776
73.801876	2467.033236	21.032794
74.205973	2472.736961	21.037811
74.236618	2494.015236	21.042829
74.452191	2487.458330	21.047847
74.455450	2494.833806	21.052864
74.394790	2491.959785	21.057882
74.554444	2499.959273	21.062899
74.457503	2497.891801	21.067917
74.769574	2490.385805	21.072935
74.889990	2495.055556	21.077952
74.864931	2486.249576	21.082970
74.809067	2482.263320	21.087987
74.456437	2482.295170	21.093005
75.190119	2483.499665	21.098023
74.867325	2487.563613	21.103040
74.907804	2487.788420	21.108058
75.116576	2491.536337	21.113075
74.863965	2496.360755	21.118093
75.004358	2506.462767	21.123111
75.255949	2511.810111	21.128128
75.649787	2503.519407	21.133146
75.568139	2510.285440	21.138163
75.669067	2516.170466	21.143181
76.191048	2511.922932	21.148199
75.637624	2518.273360	21.153216
75.717210	2510.946803	21.158234
75.992505	2500.076060	21.163251
75.701573	2513.719725	21.168269
76.151948	2513.327755	21.173287
76.227126	2528.684488	21.178304
76.437768	2532.065559	21.183322
76.400659	2534.130029	21.188339
76.121400	2542.395398	21.193357
76.093259	2539.490225	21.198375
76.194608	2534.890501	21.203392
76.252574	2544.318190	21.208410
76.330673	2534.321325	21.213427
76.250423	2547.586890	21.218445
76.528273	2561.161134	21.223463
76.691407	2570.048186	21.228480
76.697125	2563.849581	21.233498
77.034333	2565.044942	21.238515
76.719166	2572.318635	21.243533
76.848095	2570.248171	21.248551
76.706366	2578.179345	21.253568
76.951511	2600.684505	21.258586
77.327294	2587.750123	21.263603
77.619456	2601.801955	21.268621
77.627008	2597.750492	21.273639
77.355049	2596.182882	21.278656
77.655110	2600.728839	21.283674
77.468179	2582.355898	21.288691
77.469280	2600.388768	21.293709
78.224638	2611.865321	21.298727
78.317354	2622.808825	21.303744
78.117896	2630.801937	21.308762
78.634080	2603.343170	21.313779
78.909558	2610.671361	21.318797
79.009427	2584.926183	21.323815
78.751204	2577.316794	21.328832
78.690536	2563.370447	21.333850
78.789916	2566.681955	21.338867
78.411442	2576.308268	21.343885
78.744172	2570.753661	21.348903
78.786539	2569.348314	21.353920
78.606424	2570.191178	21.358938
78.798462	2583.299295	21.363955
78.849968	2593.900882	21.368973
79.012846	2593.331360	21.373991
79.256296	2604.869877	21.379008
78.911118	2613.288962	21.384026
79.302295	2596.735278	21.389043
79.467987	2595.596588	21.394061
79.923255	2584.116564	21.399079
79.965271	2579.551459	21.404096
79.622760	2591.313985	21.409114
79.849040	2583.319765	21.414131
79.985228	2587.490680	21.419149
79.796910	2583.524731	21.424167
79.990780	2582.780360	21.429184
79.658160	2579.555600	21.434202
80.212410	2583.066742	21.439219
79.852329	2585.748295	21.444237
80.261637	2588.509314	21.449255
80.428813	2598.664543	21.454272
80.225495	2613.732254	21.459290
80.483143	2614.841194	21.464307
80.729827	2620.252289	21.469325
80.760852	2615.106047	21.474343
80.708186	2616.118163	21.479360
80.703963	2618.827928	21.484378
81.259204	2613.458073	21.489395
80.567551	2616.239704	21.494413
80.660362	2613.500868	21.499431
80.722778	2617.420827	21.504448
80.623249	2620.498193	21.509466
80.678966	2621.026564	21.514483
80.680290	2639.953825	21.519501
81.087102	2653.885952	21.524519
80.983167	2653.790827	21.529536
81.141158	2658.166738	21.534554
81.747355	2658.077149	21.539571
81.372229	2674.930403	21.544589
81.557607	2669.820883	21.549607
81.476687	2675.477749	21.554624
81.511482	2676.930585	21.559642
81.430026	2678.475901	21.564659
81.744661	2694.192650	21.569677
81.785507	2696.325732	21.574695
82.235001	2707.148690	21.579712
81.962043	2712.005527	21.584730
82.320818	2691.622933	21.589747
82.426016	2704.587685	21.594765
82.541495	2727.829540	21.599783
82.560979	2718.010233	21.604800
82.635084	2722.688229	21.609818
83.185841	2721.662753	21.614835
83.192755	2719.809167	21.619853
83.248185	2712.155983	21.624871
83.606292	2718.644318	21.629888
83.340861	2724.402208	21.634906
83.410104	2719.212864	21.639923
83.261061	2718.518451	21.644941
83.431013	2723.242518	21.649959
83.699227	2714.507626	21.654976
83.427967	2709.400116	21.659994
83.811706	2711.523357	21.665011
83.607499	2710.695363	21.670029
83.448667	2706.365195	21.675047
83.673949	2709.740827	21.680064
83.437265	2721.187666	21.685082
83.819619	2726.640096	21.690099
83.856215	2745.062366	21.695117
84.072410	2747.433371	21.700135
84.131942	2744.647114	21.705152
83.837750	2755.816034	21.710170
84.230597	2752.759516	21.715187
84.180196	2771.267274	21.720205
84.447862	2771.981319	21.725223
84.567422	2776.731532	21.730240
84.318024	2782.818056	21.735258
84.468328	2768.070128	21.740275
84.822855	2793.529994	21.745293
84.684267	2807.768708	21.750311
85.303101	2809.485549	21.755328
85.156299	2806.622843	21.760346
85.487343	2799.954563	21.765363
85.469009	2810.502155	21.770381
85.632995	2798.417878	21.775399
85.677817	2800.683280	21.780416
85.503378	2806.455011	21.785434
85.477831	2807.001068	21.790451
85.503321	2797.931187	21.795469
85.329927	2802.119280	21.800487
85.575213	2801.044971	21.805504
85.927594	2818.679912	21.810522
85.835356	2818.092069	21.815539
86.167420	2830.809154	21.820557
86.240364	2827.400096	21.825575
86.549084	2827.473579	21.830592
86.151249	2836.856148	21.835610
86.397071	2843.589780	21.840627
86.679582	2826.744023	21.845645
86.158659	2837.953882	21.850663
86.750806	2830.869518	21.855680
86.081057	2853.358132	21.860698
86.724179	2855.218204	21.865715
86.944315	2851.625197	21.870733
86.672227	2860.074458	21.875751
87.074083	2847.072762	21.880768
87.368615	2874.803095	21.885786
87.656994	2877.385225	21.890803
88.045386	2876.170884	21.895821
87.480040	2864.806197	21.900839
87.972789	2844.593178	21.905856
87.755592	2854.819319	21.910874
87.544477	2849.674636	21.915891
87.250537	2855.526799	21.920909
87.711502	2872.390116	21.925927
88.248363	2867.827034	21.930944
87.880517	2869.930132	21.935962
88.051082	2878.659650	21.940979
88.039079	2877.152816	21.945997
88.112539	2890.199097	21.951015
88.512493	2886.242304	21.956032
88.897215	2889.359712	21.961050
88.963730	2896.925894	21.966067
89.304107	2895.827762	21.971085
89.193029	2895.463962	21.976103
89.484432	2870.079480	21.981120
89.218370	2870.619841	21.986138
89.305733	2855.215591	21.991155
89.218760	2852.802724	21.996173
88.960749	2855.920357	22.001191
89.298476	2867.455848	22.006208
89.296260	2881.898650	22.011226
89.437131	2878.989269	22.016243
89.485549	2881.964434	22.021261
89.178871	2882.486888	22.026279
89.516341	2878.408695	22.031296
89.337098	2881.602661	22.036314
89.368424	2901.856448	22.041331
90.065954	2907.484450	22.046349
89.671567	2910.395719	22.051367
89.747966	2917.759746	22.056384
89.835488	2910.733002	22.061402
90.159053	2912.950827	22.066419
90.252025	2938.296115	22.071437
90.357346	2940.005972	22.076455
90.536785	2932.833193	22.081472
90.334202	2945.533375	22.086490
90.520188	2941.983550	22.091507
90.907166	2941.692146	22.096525
90.671658	2953.799746	22.101543
90.943219	2959.713592	22.106560
91.188644	2973.217875	22.111578
91.489699	2963.993821	22.116595
91.487854	2964.332367	22.121613
91.485994	2969.616462	22.126631
91.732986	2959.818137	22.131648
91.694025	2957.296121	22.136666
91.687413	2961.161890	22.141683
91.983491	2959.481633	22.146701
92.020026	2953.377064	22.151719
91.880796	2961.191625	22.156736
92.016541	2957.433485	22.161754
91.811705	2956.309017	22.166771
92.003377	2951.534287	22.171789
91.753310	2967.229679	22.176807
92.155020	2976.634298	22.181824
92.173369	2989.466052	22.186842
92.522684	2994.538403	22.191859
92.779185	2983.877185	22.196877
92.644204	2992.640549	22.201895
92.760291	2981.734268	22.206912
92.713880	2999.117581	22.211930
92.842265	3015.131046	22.216947
93.008551	3018.043392	22.221965
92.978838	3029.825610	22.226983
93.151642	3024.092599	22.232000
93.031580	3029.948568	22.237018
93.144031	3040.557280	22.242035
93.404087	3045.443291	22.247053
93.482235	3055.085202	22.252071
93.788619	3055.032413	22.257088
93.654789	3054.662010	22.262106
93.851988	3055.060067	22.267123
93.994028	3045.462495	22.272141
93.919143	3051.813928	22.277159
94.376236	3061.036710	22.282176
94.260939	3076.908961	22.287194
94.379355	3076.018485	22.292211
94.372783	3067.512849	22.297229
94.108896	3074.593751	22.302247
94.764714	3072.050600	22.307264
94.855622	3068.517480	22.312282
94.607250	3070.556716	22.317299
94.870945	3063.777129	22.322317
94.708523	3074.715246	22.327335
94.965526	3089.157035	22.332352
95.152966	3096.956548	22.337370
94.917950	3104.614972	22.342387
95.029152	3090.031857	22.347405
95.033983	3102.415909	22.352423
95.329974	3104.571297	22.357440
95.267149	3122.198871	22.362458
95.538895	3124.152815	22.367475
96.073728	3123.943241	22.372493
95.777570	3123.277772	22.377511
96.319250	3115.157453	22.382528
96.276997	3116.389774	22.387546
96.324175	3116.322467	22.392563
96.542618	3115.319282	22.397581
96.415425	3124.589651	22.402599
96.528458	3107.233324	22.407616
96.547296	3116.863495	22.412634
96.426278	3134.013435	22.417651
96.506803	3133.902264	22.422669
96.932102	3137.136759	22.427687
97.116781	3134.349352	22.432704
97.624770	3124.341745	22.437722
97.518019	3130.954739	22.442739
97.493379	3122.736715	22.447757
97.486460	3117.217974	22.452775
97.755292	3121.132686	22.457792
97.574898	3128.515741	22.462810
97.949077	3124.254635	22.467827
97.979081	3114.504182	22.472845
97.980887	3125.316246	22.477863
97.938055	3117.574682	22.482880
98.408008	3118.414604	22.487898
97.977503	3109.525014	22.492915
98.135641	3117.403941	22.497933
98.213663	3117.393074	22.502951
98.117860	3120.960812	22.507968
98.318726	3134.281984	22.512986
98.354401	3152.875615	22.518003
98.533790	3148.257749	22.523021
98.449708	3161.153973	22.528039
98.635314	3150.809942	22.533056
98.562399	3161.560003	22.538074
98.783695	3188.252445	22.543091
98.705020	3184.336499	22.548109
98.917067	3191.799389	22.553127
98.887825	3205.328807	22.558144
99.170735	3216.235348	22.563162
98.982535	3228.055585	22.568179
99.383629	3212.571039	22.573197
99.322583	3234.887650	22.578215
99.875085	3241.173734	22.583232
100.821565	3219.367264	22.588250
100.917395	3221.925884	22.593267
100.752573	3194.627314	22.598285
100.727522	3193.187820	22.603303
100.774357	3176.405990	22.608320
101.174033	3174.157754	22.613338
100.695099	3173.376685	22.618355
100.998349	3174.402096	22.623373
100.931653	3178.191759	22.628391
100.638656	3173.951283	22.633408
101.327400	3168.358564	22.638426
101.045137	3166.322907	22.643443
101.285918	3167.193084	22.648461
101.198598	3173.911554	22.653479
101.444427	3165.901316	22.658496
101.587418	3174.574838	22.663514
101.437560	3166.464074	22.668531
101.766280	3157.222115	22.673549
101.685528	3173.688382	22.678567
101.445130	3167.320307	22.683584
101.725665	3175.677693	22.688602
101.623629	3192.380221	22.693619
101.721695	3189.089791	22.698637
102.030486	3197.729808	22.703655
101.982794	3196.118502	22.708672
102.073954	3206.985603	22.713690
102.097695	3238.738652	22.718707
102.450671	3225.991425	22.723725
102.312591	3228.353711	22.728743
102.416348	3233.677698	22.733760
102.691926	3243.393663	22.738778
102.454636	3252.014593	22.743795
102.823932	3263.790799	22.748813
102.932482	3264.317063	22.753831
102.920958	3276.857267	22.758848
103.152573	3291.619537	22.763866
103.080446	3301.174657	22.768883
103.353069	3298.130908	22.773901
103.487142	3306.775251	22.778919
103.274545	3326.000251	22.783936
103.719493	3324.122365	22.788954
103.602448	3335.243023	22.793971
103.842280	3330.170218	22.798989
103.889185	3352.684550	22.804007
104.228963	3361.173406	22.809024
104.619470	3361.751471	22.814042
104.207093	3369.691616	22.819059
104.486519	3357.575099	22.824077
104.633557	3356.428314	22.829095
104.422921	3371.448409	22.834112
104.596183	3383.512419	22.839130
104.610526	3395.029884	22.844147
104.298714	3392.197307	22.849165
104.861408	3406.467947	22.854183
105.007761	3419.903483	22.859200
105.410445	3413.117307	22.864218
105.392247	3425.918299	22.869235
105.557623	3420.383770	22.874253
105.656616	3426.774504	22.879271
105.250808	3433.374748	22.884288
106.327395	3439.825147	22.889306
105.749139	3445.439681	22.894323
106.211094	3447.357046	22.899341
106.385023	3452.259289	22.904359
106.551834	3451.938481	22.909376
107.250785	3439.544962	22.914394
107.031709	3437.795760	22.919411
107.422412	3428.240886	22.924429
107.586647	3423.206064	22.929447
107.180437	3407.011472	22.934464
107.429121	3390.999598	22.939482
107.218509	3389.969627	22.944499
107.136239	3384.104873	22.949517
107.481110	3387.351464	22.954535
107.249854	3396.667705	22.959552
107.605789	3406.545602	22.964570
107.635723	3422.762435	22.969587
107.906489	3422.545409	22.974605
108.006830	3423.202787	22.979623
108.101031	3423.312057	22.984640
108.190547	3414.513208	22.989658
107.874048	3421.232150	22.994675
107.801673	3421.308197	22.999693
108.204925	3429.682347	23.004711
108.134692	3441.287280	23.009728
108.097967	3448.914263	23.014746
108.416258	3451.802459	23.019763
108.538482	3445.162469	23.024781
109.181229	3451.450776	23.029799
108.585663	3475.885708	23.034816
109.018053	3473.360814	23.039834
109.038679	3474.128451	23.044851
108.856269	3482.079971	23.049869
109.090321	3479.622890	23.054887
108.896360	3493.993031	23.059904
109.462148	3506.068498	23.064922
109.569818	3509.167288	23.069939
109.361753	3505.503953	23.074957
109.749504	3510.282441	23.079975
109.607327	3532.385883	23.084992
109.971802	3535.490929	23.090010
109.902030	3531.621457	23.095027
109.897726	3552.922577	23.100045
110.344801	3555.244315	23.105063
110.514853	3570.953599	23.110080
110.652196	3559.878300	23.115098
110.531439	3574.152674	23.120115
110.321740	3585.277281	23.125133
110.812042	3592.293236	23.130151
111.206600	3604.003542	23.135168
111.429836	3603.162402	23.140186
111.414082	3602.409716	23.145203
111.104043	3589.478405	23.150221
111.206337	3592.105286	23.155239
111.283686	3611.595157	23.160256
111.514925	3614.636506	23.165274
111.467102	3625.532372	23.170291
111.677578	3630.482341	23.175309
111.988116	3631.585290	23.180327
111.553949	3650.342577	23.185344
111.963319	3655.621133	23.190362
111.651406	3663.996962	23.195379
112.162245	3670.687146	23.200397
112.639534	3692.504037	23.205415
112.534526	3693.997361	23.210432
112.641904	3692.616941	23.215450
112.843068	3699.364384	23.220467
112.692078	3705.262526	23.225485
113.202130	3710.688676	23.230503
112.963622	3722.358422	23.235520
113.354455	3720.020263	23.240538
113.368472	3725.877155	23.245555
113.434885	3721.303086	23.250573
113.830999	3740.519672	23.255591
113.672266	3760.610642	23.260608
113.936648	3749.153076	23.265626
113.829759	3759.650963	23.270643
114.079972	3759.810094	23.275661
114.279671	3751.541786	23.280679
113.686911	3764.302527	23.285696
114.237129	3765.521457	23.290714
114.788792	3773.174361	23.295731
114.424390	3776.103041	23.300749
115.162997	3775.108912	23.305767
115.093383	3790.696165	23.310784
115.417713	3793.081569	23.315802
115.705158	3805.792461	23.320819
115.564247	3803.803401	23.325837
115.646030	3791.950899	23.330855
116.097739	3792.206916	23.335872
116.310528	3789.968724	23.340890
116.086078	3768.015397	23.345907
115.896979	3762.691451	23.350925
115.821200	3774.074901	23.355943
115.779776	3783.893694	23.360960
115.852299	3784.839513	23.365978
115.834049	3792.794132	23.370995
115.950068	3809.110160	23.376013
116.863685	3818.797931	23.381031
116.601746	3827.785784	23.386048
116.817135	3826.534451	23.391066
116.886711	3819.633644	23.396083
116.652858	3824.239950	23.401101
117.023100	3835.878013	23.406119
117.195911	3848.652849	23.411136
117.499509	3841.820918	23.416154
117.440214	3844.234460	23.421171
117.391863	3847.307853	23.426189
117.844347	3851.324069	23.431207
117.694350	3845.858549	23.436224
117.625327	3840.847405	23.441242
117.988513	3858.253745	23.446259
117.857216	3874.942046	23.451277
118.461545	3868.086537	23.456295
117.988753	3881.300257	23.461312
118.250448	3871.463584	23.466330
118.743581	3873.003152	23.471347
118.720939	3883.916435	23.476365
118.863415	3889.705708	23.481383
118.991442	3895.221163	23.486400
118.777013	3892.557042	23.491418
118.899027	3893.638152	23.496435
118.925616	3895.223794	23.501453
119.262242	3901.158331	23.506471
119.212741	3919.518710	23.511488
119.580855	3903.605240	23.516506
119.907642	3910.903881	23.521523
119.643391	3917.229241	23.526541
120.133132	3917.759256	23.531559
120.349462	3939.720397	23.536576
120.742066	3921.186495	23.541594
121.507532	3907.872580	23.546611
121.835204	3879.356664	23.551629
122.194592	3866.823414	23.556647
122.187682	3852.668236	23.561664
122.082193	3842.562872	23.566682
122.439409	3827.164135	23.571699
121.777276	3815.679609	23.576717
121.956691	3807.374383	23.581735
121.851845	3808.609662	23.586752
121.745818	3801.783278	23.591770
121.810987	3802.793992	23.596787
121.858113	3811.440698	23.601805
122.208613	3801.290188	23.606823
121.972143	3813.544182	23.611840
121.856323	3800.619474	23.616858
122.243311	3802.915435	23.621875
122.083375	3811.269473	23.626893
122.165830	3813.182109	23.631911
121.855098	3818.501600	23.636928
121.968168	3828.212401	23.641946
122.026692	3839.292071	23.646963
122.160356	3851.049684	23.651981
122.713196	3858.199760	23.656999
122.507790	3875.105202	23.662016
122.445125	3897.400264	23.667034
123.052599	3903.050105	23.672051
122.718869	3914.889376	23.677069
122.682231	3927.303551	23.682087
122.874006	3951.995266	23.687104
123.129981	3966.847950	23.692122
123.533435	3972.525628	23.697139
123.769656	3992.680596	23.702157
123.916884	3988.814949	23.707175
123.971766	3995.563041	23.712192
124.173832	4000.969968	23.717210
124.768764	4008.395041	23.722227
124.593318	4019.309974	23.727245
124.972233	4005.525807	23.732263
125.271679	4016.095184	23.737280
125.263842	4013.195919	23.742298
125.313747	4001.622885	23.747315
125.496479	4011.697949	23.752333
126.035851	4007.256850	23.757351
125.776997	4007.848805	23.762368
125.573926	4006.432109	23.767386
125.921117	4005.005556	23.772403
125.605324	4006.897542	23.777421
125.881231	4016.188373	23.782439
125.884266	4033.760912	23.787456
125.975225	4047.422196	23.792474
126.037699	4035.279143	23.797491
126.173433	4061.147422	23.802509
126.283395	4053.406176	23.807527
126.500521	4076.639471	23.812544
126.548645	4072.693628	23.817562
126.761377	4082.881961	23.822579
126.820989	4096.010979	23.827597
126.826138	4114.074958	23.832615
127.182996	4096.774564	23.837632
127.297792	4122.350494	23.842650
127.442820	4124.286234	23.847667
127.547575	4145.371790	23.852685
127.732792	4131.981844	23.857703
127.764938	4138.697439	23.862720
127.776676	4164.020824	23.867738
128.144028	4157.917290	23.872755
128.066400	4170.860570	23.877773
128.411058	4168.356634	23.882791
128.252569	4194.211485	23.887808
128.377115	4193.932017	23.892826
129.032942	4189.170205	23.897843
128.679686	4207.171868	23.902861
129.128332	4226.913311	23.907879
129.413822	4221.696825	23.912896
128.997424	4229.455553	23.917914
129.560635	4234.484010	23.922931
129.296282	4231.081996	23.927949
129.641873	4248.103763	23.932967
129.885791	4250.458011	23.937984
129.922347	4254.188218	23.943002
130.260777	4248.810661	23.948019
130.240498	4254.910030	23.953037
130.241544	4270.571488	23.958055
130.521776	4280.714581	23.963072
130.297486	4294.195070	23.968090
130.810459	4280.520652	23.973107
130.779716	4286.465148	23.978125
130.969043	4291.484797	23.983143
130.974225	4297.185199	23.988160
131.021315	4309.584771	23.993178
131.394359	4312.113543	23.998195
131.489373	4320.868557	24.003213
131.521230	4315.709787	24.008231
131.833631	4323.914065	24.013248
131.370048	4347.733854	24.018266
131.754428	4338.014197	24.023283
132.027369	4337.040794	24.028301
131.836269	4344.565409	24.033319
132.063334	4356.449355	24.038336
132.326797	4371.069963	24.043354
132.622119	4365.745653	24.048371
132.989400	4390.559595	24.053389
133.143478	4388.645359	24.058407
133.468239	4394.139074	24.063424
133.322163	4411.031735	24.068442
133.495724	4399.304146	24.073459
133.849736	4396.194489	24.078477
133.755278	4397.686987	24.083495
134.070482	4390.568953	24.088512
134.096108	4392.386880	24.093530
134.145863	4385.973581	24.098547
134.099125	4385.361895	24.103565
134.258925	4395.717800	24.108583
134.367782	4405.670387	24.113600
134.571898	4421.542720	24.118618
134.678824	4409.791132	24.123635
134.897024	4409.251274	24.128653
134.792306	4410.277318	24.133671
135.199082	4420.828300	24.138688
135.148176	4438.847333	24.143706
135.421965	4441.525694	24.148723
135.278049	4445.289445	24.153741
135.444499	4448.035272	24.158759
135.936765	4464.533557	24.163776
135.376967	4480.165082	24.168794
135.490311	4473.467043	24.173811
136.034828	4484.693922	24.178829
136.056147	4496.734301	24.183847
136.063932	4505.879383	24.188864
136.192528	4510.559490	24.193882
136.788092	4514.646699	24.198899
136.799662	4531.605621	24.203917
136.510829	4540.640676	24.208935
137.301712	4538.217366	24.213952
136.992463	4546.163720	24.218970
137.353706	4553.049671	24.223987
137.210971	4562.409960	24.229005
137.260141	4566.736926	24.234023
137.491163	4566.482171	24.239040
137.642736	4570.836081	24.244058
138.647099	4573.809433	24.249075
138.901342	4579.019444	24.254093
138.670964	4575.838504	24.259111
138.849169	4557.084671	24.264128
138.771654	4547.680833	24.269146
138.749535	4554.103171	24.274163
138.929105	4565.302549	24.279181
138.888028	4578.280482	24.284199
139.046378	4576.062654	24.289216
138.892398	4580.289848	24.294234
139.056760	4575.120087	24.299251
139.333020	4597.468374	24.304269
139.539224	4604.031341	24.309287
139.605108	4603.973634	24.314304
139.585246	4613.134991	24.319322
139.871102	4630.797676	24.324339
140.263695	4641.924599	24.329357
140.376909	4646.515156	24.334375
140.429299	4645.965539	24.339392
140.483606	4648.669494	24.344410
140.411057	4656.371258	24.349427
140.601928	4670.158013	24.354445
140.746601	4676.349263	24.359463
140.832942	4672.392446	24.364480
141.158697	4693.651246	24.369498
141.278236	4707.134720	24.374515
141.144897	4708.411592	24.379533
141.394129	4726.147102	24.384551
141.909887	4731.719061	24.389568
141.744577	4743.255211	24.394586
141.920966	4738.343095	24.399603
141.828504	4744.191408	24.404621
142.039799	4772.607322	24.409639
142.451929	4762.764955	24.414656
142.489400	4782.356356	24.419674
142.624182	4796.148239	24.424691
142.449055	4800.387521	24.429709
142.690640	4805.079603	24.434727
142.807463	4818.986086	24.439744
143.061695	4832.845497	24.444762
143.113788	4838.905245	24.449779
143.621040	4848.755274	24.454797
143.434382	4865.535341	24.459815
143.673450	4853.107771	24.464832
144.160558	4871.309824	24.469850
144.193555	4880.438530	24.474867
144.317944	4873.030490	24.479885
144.367189	4892.027750	24.484903
144.870093	4896.154231	24.489920
144.965682	4905.285561	24.494938
145.346779	4911.684676	24.499955
145.186222	4917.243381	24.504973
145.284504	4918.600564	24.509991
145.468772	4911.610941	24.515008
145.515417	4912.379225	24.520026
145.639773	4917.337856	24.525043
145.626867	4918.421675	24.530061
145.839181	4932.987272	24.535079
145.829689	4936.289143	24.540096
145.625572	4943.799615	24.545114
146.283808	4958.919595	24.550131
146.220060	4969.293452	24.555149
146.355730	4989.135388	24.560167
146.375002	4979.647396	24.565184
146.725097	4991.146406	24.570202
146.806637	5011.712935	24.575219
147.071598	5005.634823	24.580237
147.046079	5013.512584	24.585255
147.511370	5021.681863	24.590272
147.726005	5032.734393	24.595290
147.991195	5038.628074	24.600307
148.095474	5035.829531	24.605325
147.976221	5037.922395	24.610343
148.513890	5041.128396	24.615360
148.526634	5064.933182	24.620378
148.644225	5057.976151	24.625395
148.919205	5055.199165	24.630413
148.783497	5061.284227	24.635431
149.072217	5047.543372	24.640448
149.177442	5058.091756	24.645466
149.356979	5071.827196	24.650483
149.893036	5073.788833	24.655501
149.595879	5083.076515	24.660519
149.701795	5083.956516	24.665536
150.037552	5080.243052	24.670554
150.080295	5090.619683	24.675571
149.952014	5085.451560	24.680589
150.079684	5105.103749	24.685607
150.365382	5118.115809	24.690624
149.937949	5119.091077	24.695642
150.349295	5132.644854	24.700659
151.037039	5136.348561	24.705677
150.918801	5134.437524	24.710695
151.407667	5145.091593	24.715712
151.411717	5163.593676	24.720730
151.113504	5170.780177	24.725747
151.374754	5165.410665	24.730765
151.649774	5187.215615	24.735783
152.032396	5193.797137	24.740800
152.186600	5196.652055	24.745818
152.266092	5206.778229	24.750835
152.490026	5203.754449	24.755853
152.378488	5207.702050	24.760871
152.632254	5225.993673	24.765888
152.951748	5225.992299	24.770906
152.594528	5237.587754	24.775923
153.205921	5241.209252	24.780941
153.512109	5247.820293	24.785959
153.561633	5249.157744	24.790976
153.488588	5252.673587	24.795994
153.403437	5252.359875	24.801011
153.581332	5243.958105	24.806029
153.759633	5266.968164	24.811047
154.144109	5273.211908	24.816064
154.177208	5274.800595	24.821082
154.244350	5283.933548	24.826099
154.563321	5294.583343	24.831117
154.742703	5315.956855	24.836135
154.932766	5311.294133	24.841152
154.917353	5311.247812	24.846170
154.900666	5324.217790	24.851187
155.445845	5335.796113	24.856205
155.419583	5343.564022	24.861223
155.405170	5346.929710	24.866240
155.453685	5359.650935	24.871258
155.406334	5367.346691	24.876275
155.819047	5372.696152	24.881293
156.335165	5396.285892	24.886311
156.436385	5403.057925	24.891328
156.551499	5401.097060	24.896346
156.498537	5411.135133	24.901363
156.798458	5419.864425	24.906381
157.058449	5438.589611	24.911399
157.198251	5436.177137	24.916416
157.289879	5441.470030	24.921434
157.305906	5467.694237	24.926451
157.480726	5468.887423	24.931469
157.215563	5481.408573	24.936487
157.637575	5492.385113	24.941504
158.461792	5488.920965	24.946522
158.540605	5484.069007	24.951539
158.950788	5482.181461	24.956557
159.058363	5485.486819	24.961575
159.009817	5497.454969	24.966592
159.596213	5510.664118	24.971610
159.445976	5509.183775	24.976627
159.495026	5507.545775	24.981645
159.702505	5517.153733	24.986663
159.447416	5521.796204	24.991680
159.828104	5515.328080	24.996698
159.730534	5528.899633	25.001715
160.199279	5536.831047	25.006733
159.977473	5547.705716	25.011751
160.275826	5550.200198	25.016768
160.448258	5552.552682	25.021786
160.351983	5574.014576	25.026803
160.485007	5575.717181	25.031821
160.674580	5592.748859	25.036839
160.759670	5605.488854	25.041856
160.809035	5610.765729	25.046874
160.754419	5636.858306	25.051891
161.289081	5638.539368	25.056909
161.895176	5651.481936	25.061927
162.013660	5670.289772	25.066944
162.724278	5670.225255	25.071962
162.964281	5677.372608	25.076979
162.936725	5667.390466	25.081997
163.067124	5678.002155	25.087015
162.831231	5676.954015	25.092032
163.231049	5667.384454	25.097050
162.988083	5673.358622	25.102067
162.880813	5669.594485	25.107085
163.361503	5668.067820	25.112103
163.252509	5691.551564	25.117120
163.208348	5691.948059	25.122138
163.210467	5702.292258	25.127155
163.686191	5715.682100	25.132173
164.000320	5720.154415	25.137191
164.085270	5735.573522	25.142208
164.516515	5742.450449	25.147226
163.853340	5761.782708	25.152243
164.643524	5764.364823	25.157261
164.764273	5787.136245	25.162279
164.466492	5791.159327	25.167296
164.979447	5806.043708	25.172314
165.293964	5816.093490	25.177331
165.447328	5821.477385	25.182349
165.478486	5838.329252	25.187367
165.412290	5856.095956	25.192384
165.964625	5848.276163	25.197402
166.171180	5877.779148	25.202419
166.468084	5878.794760	25.207437
166.944712	5880.977633	25.212455
166.725819	5891.118017	25.217472
167.052680	5892.326338	25.222490
167.230873	5914.296502	25.227507
167.313149	5918.988377	25.232525
167.472143	5923.236863	25.237543
167.403875	5926.895299	25.242560
167.449572	5943.893671	25.247578
167.816191	5945.227052	25.252595
167.689333	5956.353603	25.257613
168.422582	5968.856819	25.262631
168.401396	5970.163909	25.267648
168.669604	5975.245519	25.272666
168.963625	5988.028851	25.277683
169.150629	5992.958974	25.282701
169.139078	6000.609224	25.287719
169.014587	5998.291512	25.292736
169.595032	6015.657903	25.297754
169.621626	6030.804950	25.302771
169.635272	6034.771365	25.307789
169.803706	6033.344804	25.312807
169.887536	6060.322440	25.317824
169.896946	6054.692992	25.322842
169.890065	6079.905394	25.327859
170.135985	6087.963901	25.332877
170.718742	6099.371609	25.337895
170.464008	6113.298421	25.342912
170.973464	6121.200845	25.347930
171.096137	6134.908573	25.352947
171.487232	6138.593748	25.357965
171.407716	6140.812613	25.362983
171.588324	6159.133577	25.368000
172.333883	6149.324476	25.373018
172.739820	6151.469881	25.378035
172.975676	6145.218130	25.383053
172.656906	6141.593809	25.388071
172.579622	6153.980925	25.393088
173.514888	6156.106457	25.398106
173.391055	6176.192779	25.403123
173.421439	6173.278343	25.408141
173.785601	6177.126756	25.413159
173.416408	6172.286202	25.418176
173.815043	6162.093368	25.423194
173.745064	6168.339925	25.428211
173.993500	6171.364909	25.433229
174.040971	6196.767119	25.438247
174.007758	6205.206944	25.443264
174.182283	6203.184573	25.448282
174.266106	6227.713196	25.453299
174.494599	6228.926214	25.458317
174.522361	6242.304553	25.463335
174.533860	6266.772385	25.468352
175.082543	6274.398763	25.473370
175.236858	6290.679958	25.478387
175.493336	6296.307233	25.483405
175.675948	6312.833359	25.488423
175.872048	6332.330708	25.493440
176.023019	6330.273523	25.498458
176.533476	6337.924912	25.503475
176.458519	6352.942130	25.508493
176.878574	6352.196931	25.513511
176.743636	6368.161606	25.518528
177.128321	6382.816815	25.523546
177.221461	6395.695472	25.528563
177.081098	6396.472404	25.533581
177.554362	6400.115434	25.538599
177.226186	6423.045165	25.543616
177.930713	6426.174522	25.548634
178.297723	6438.047278	25.553651
178.373857	6448.360526	25.558669
178.768051	6444.919880	25.563687
178.908126	6453.214983	25.568704
179.225451	6462.757262	25.573722
179.330393	6477.468966	25.578739
179.341444	6480.442163	25.583757
179.846310	6473.177241	25.588775
179.620430	6477.855477	25.593792
180.054889	6495.956993	25.598810
180.387249	6502.434603	25.603827
180.228396	6509.044033	25.608845
180.350346	6504.149459	25.613863
180.235060	6511.275965	25.618880
180.424666	6512.287486	25.623898
180.936668	6522.553327	25.628915
180.874660	6535.196403	25.633933
180.889727	6541.939417	25.638951
180.876885	6551.546194	25.643968
181.066767	6555.836360	25.648986
181.327462	6574.804428	25.654003
181.595797	6595.750951	25.659021
181.859180	6593.399633	25.664039
181.770774	6609.077825	25.669056
181.957573	6625.435252	25.674074
181.949515	6635.183735	25.679092
182.390372	6647.299818	25.684109
182.885414	6661.096592	25.689127
183.027138	6676.757837	25.694144
183.441216	6676.475445	25.699162
183.713815	6686.039162	25.704180
183.388692	6685.839997	25.709197
183.727290	6698.896163	25.714215
183.828067	6716.228909	25.719232
184.452254	6717.935174	25.724250
184.610554	6720.802327	25.729268
184.656640	6735.991834	25.734285
184.812625	6742.367841	25.739303
184.549072	6762.224656	25.744320
184.611302	6759.112254	25.749338
185.119656	6772.466383	25.754356
185.097404	6785.241028	25.759373
185.460510	6801.827836	25.764391
185.912401	6807.099190	25.769408
185.928669	6826.809978	25.774426
186.027082	6837.871373	25.779444
186.238262	6850.561649	25.784461
186.730825	6842.263822	25.789479
187.255933	6857.351119	25.794496
187.350894	6863.786478	25.799514
187.564238	6860.882081	25.804532
187.421704	6868.626049	25.809549
187.882310	6868.096251	25.814567
187.885920	6874.951400	25.819584
188.102352	6880.922051	25.824602
188.547916	6888.401528	25.829620
188.587745	6899.519519	25.834637
188.779252	6881.651335	25.839655
188.515259	6903.396034	25.844672
188.841191	6913.485661	25.849690
189.220350	6921.783827	25.854708
189.349446	6927.018560	25.859725
189.760115	6939.324211	25.864743
189.851741	6953.280780	25.869760
189.613714	6960.321630	25.874778
189.737717	6958.488188	25.879796
189.758734	6983.324710	25.884813
190.170680	6983.842089	25.889831
190.348132	7004.521987	25.894848
190.299872	7017.275012	25.899866
190.396447	7022.501587	25.904884
190.372947	7035.933662	25.909901
190.775433	7050.786555	25.914919
191.094390	7081.311078	25.919936
191.563627	7078.811988	25.924954
191.995727	7089.459997	25.929972
191.943180	7097.618569	25.934989
192.441446	7081.942980	25.940007
192.456354	7107.412523	25.945024
192.968637	7112.395028	25.950042
193.333796	7113.584761	25.955060
193.067493	7108.012245	25.960077
193.254331	7112.014285	25.965095
193.528681	7120.188425	25.970112
193.489919	7135.798669	25.975130
193.567636	7130.174449	25.980148
193.590987	7152.707765	25.985165
194.268332	7162.654985	25.990183
194.021132	7168.797235	25.995200
193.974641	7177.636302	26.000218
194.632575	7196.050051	26.005236
194.783709	7211.028156	26.010253
194.835137	7215.664772	26.015271
195.090397	7236.750410	26.020288
195.375173	7241.454486	26.025306
195.494202	7253.326515	26.030324
195.431597	7273.026862	26.035341
195.757695	7274.266112	26.040359
196.138529	7297.307622	26.045376
196.114531	7307.796375	26.050394
196.657641	7319.076013	26.055412
196.429381	7334.711166	26.060429
196.705782	7339.788795	26.065447
196.877933	7362.355360	26.070464
197.117735	7364.975160	26.075482
197.663270	7381.211706	26.080500
197.693660	7406.636801	26.085517
198.081199	7401.044922	26.090535
198.071813	7418.967314	26.095552
198.027556	7436.739486	26.100570
198.503432	7440.237579	26.105588
198.595940	7459.029003	26.110605
198.767288	7461.869827	26.115623
198.999932	7475.340151	26.120640
199.118229	7493.255653	26.125658
199.727620	7495.311386	26.130676
199.949221	7510.730222	26.135693
200.094248	7530.040567	26.140711
200.640925	7517.459448	26.145728
200.901752	7514.109069	26.150746
201.222522	7508.656841	26.155764
201.243123	7503.323286	26.160781
201.849397	7503.954492	26.165799
201.981937	7495.365117	26.170816
201.872488	7499.781178	26.175834
202.264962	7490.428019	26.180852
202.158276	7491.889723	26.185869
202.261208	7494.891753	26.190887
202.752970	7502.683648	26.195904
202.655959	7522.756492	26.200922
203.237345	7522.908527	26.205940
202.926624	7525.458744	26.210957
202.942135	7529.071167	26.215975
202.960344	7529.826023	26.220992
203.164822	7539.160369	26.226010
203.434863	7551.430327	26.231028
203.135903	7565.734585	26.236045
203.400594	7578.718326	26.241063
204.265701	7585.201976	26.246080
203.997166	7592.836569	26.251098
204.434120	7602.354220	26.256116
204.540207	7614.132601	26.261133
205.039462	7629.068220	26.266151
204.930542	7642.537279	26.271168
205.141430	7652.021754	26.276186
205.560933	7665.805543	26.281204
205.692130	7677.740495	26.286221
205.688381	7684.657779	26.291239
206.140551	7701.934082	26.296256
206.141849	7712.295546	26.301274
206.575862	7720.118796	26.306292
206.693874	7738.476868	26.311309
206.957311	7742.281163	26.316327
207.081415	7753.874225	26.321344
207.449134	7777.120799	26.326362
207.600169	7778.717708	26.331380
207.617107	7786.329317	26.336397
207.886894	7802.696056	26.341415
208.281853	7806.854353	26.346432
208.195480	7835.449492	26.351450
208.363505	7839.646729	26.356468
208.586471	7860.414201	26.361485
208.786336	7865.660804	26.366503
208.987353	7874.090987	26.371520
209.228301	7905.814695	26.376538
209.444259	7896.537032	26.381556
209.791198	7918.007975	26.386573
209.902709	7941.292895	26.391591
210.231311	7940.026332	26.396608
210.109909	7966.239866	26.401626
210.490276	7966.640745	26.406644
210.550840	7983.322351	26.411661
210.719339	8001.593221	26.416679
211.192981	8020.869127	26.421696
211.220953	8035.177584	26.426714
211.740892	8050.852770	26.431732
211.999224	8067.336513	26.436749
211.996974	8074.447710	26.441767
212.536200	8080.621950	26.446784
212.734865	8091.393666	26.451802
212.994391	8097.445285	26.456820
213.124159	8098.000218	26.461837
212.986034	8099.024359	26.466855
213.660956	8100.473656	26.471872
213.294548	8123.280672	26.476890
213.641529	8122.522260	26.481908
213.919921	8138.193946	26.486925
214.379867	8146.199391	26.491943
214.681810	8147.138431	26.496960
214.915344	8149.447363	26.501978
215.375918	8162.666362	26.506996
215.380215	8167.250983	26.512013
215.785461	8171.878709	26.517031
215.923963	8171.530064	26.522048
216.055243	8175.959884	26.527066
216.300267	8175.651702	26.532084
216.499464	8185.623904	26.537101
217.531217	8165.266210	26.542119
218.140242	8155.680999	26.547136
218.141166	8151.821471	26.552154
218.138729	8128.405521	26.557172
218.356981	8116.907105	26.562189
218.386041	8114.780979	26.567207
218.564365	8119.414174	26.572224
218.044713	8124.220800	26.577242
218.585655	8121.670770	26.582260
218.747040	8139.645888	26.587277
218.531332	8155.925553	26.592295
218.807871	8155.934193	26.597312
218.726005	8160.439692	26.602330
219.468589	8175.255236	26.607348
219.337280	8185.660988	26.612365
219.089336	8197.789390	26.617383
219.058117	8206.892212	26.622400
219.358418	8244.842648	26.627418
219.879505	8253.897982	26.632436
219.828860	8280.109441	26.637453
219.897021	8303.774440	26.642471
219.867065	8315.891795	26.647488
220.313353	8358.179148	26.652506
220.421849	8384.813965	26.657524
220.589162	8411.064879	26.662541
221.036219	8432.471814	26.667559
221.533971	8444.852577	26.672576
221.587482	8480.857156	26.677594
221.898412	8501.480081	26.682612
222.158364	8519.238096	26.687629
222.119660	8533.517524	26.692647
222.787947	8554.950749	26.697664
223.208090	8566.619619	26.702682
223.643169	8576.611532	26.707700
223.874872	8596.506325	26.712717
223.958645	8597.752845	26.717735
224.252709	8605.734619	26.722752
224.278763	8630.349194	26.727770
224.587886	8621.677515	26.732788
224.864767	8635.977165	26.737805
224.682230	8661.138908	26.742823
225.277231	8653.132633	26.747840
225.000789	8686.240094	26.752858
225.483763	8692.689543	26.757876
225.659636	8702.282571	26.762893
225.721461	8720.764518	26.767911
226.371361	8733.110250	26.772928
226.156465	8762.930872	26.777946
226.518830	8773.423591	26.782964
227.103218	8786.440052	26.787981
226.679964	8797.961823	26.792999
227.211911	8812.792300	26.798016
227.384780	8840.498134	26.803034
227.598228	8854.786464	26.808052
228.045109	8864.173498	26.813069
228.209272	8887.818606	26.818087
228.481814	8892.682549	26.823104
228.479856	8916.606005	26.828122
228.974780	8935.780549	26.833140
229.024684	8951.375010	26.838157
228.938455	8972.340080	26.843175
229.682846	8983.276877	26.848192
229.520488	8998.806068	26.853210
229.781282	9017.778018	26.858228
230.171221	9045.665253	26.863245
230.459124	9061.771577	26.868263
230.968779	9066.032353	26.873280
230.997842	9091.021794	26.878298
231.663742	9090.257751	26.883316
232.958449	9074.691584	26.888333
232.944374	9082.464218	26.893351
233.149402	9072.548960	26.898368
233.361688	9072.591456	26.903386
233.096091	9083.080223	26.908404
233.399180	9087.279106	26.913421
233.537962	9085.301007	26.918439
233.902214	9086.803869	26.923456
234.041088	9097.010971	26.928474
233.888974	9094.548047	26.933492
234.346169	9115.454629	26.938509
234.128235	9127.674216	26.943527
234.242681	9130.525613	26.948544
234.858086	9154.527711	26.953562
234.703013	9160.243323	26.958580
234.888647	9169.857523	26.963597
235.478624	9190.486496	26.968615
235.686851	9197.917233	26.973632
235.765321	9225.697849	26.978650
235.991851	9232.512642	26.983668
236.433355	9237.764101	26.988685
236.506241	9253.054593	26.993703
236.666320	9258.253729	26.998720
236.857338	9276.970350	27.003738
236.840439	9285.324320	27.008756
237.340396	9287.060548	27.013773
237.458591	9316.281442	27.018791
237.824384	9315.464891	27.023808
238.227227	9326.304109	27.028826
238.361603	9345.799893	27.033844
238.714409	9340.014131	27.038861
238.791226	9365.373374	27.043879
238.830784	9384.324786	27.048896
239.010943	9397.312962	27.053914
238.938300	9411.242530	27.058932
239.480680	9422.668692	27.063949
239.610014	9443.642947	27.068967
239.957839	9466.362541	27.073984
240.178498	9483.316986	27.079002
240.166267	9509.248237	27.084020
240.835080	9520.164427	27.089037
240.758486	9542.545709	27.094055
241.135965	9552.386130	27.099072
241.534579	9575.813158	27.104090
241.837958	9590.694617	27.109108
241.798117	9604.227217	27.114125
242.221969	9622.695456	27.119143
242.540040	9635.042893	27.124160
242.958869	9643.869838	27.129178
242.924398	9655.427085	27.134196
243.292146	9677.556732	27.139213
243.681027	9698.483675	27.144231
243.639442	9715.889811	27.149248
243.626282	9725.972834	27.154266
243.920605	9744.723938	27.159284
244.125610	9758.288084	27.164301
244.570042	9786.264811	27.169319
244.871390	9807.932645	27.174336
244.977463	9823.484430	27.179354
244.971725	9851.904890	27.184372
245.592125	9861.022108	27.189389
246.019719	9891.098270	27.194407
246.129816	9899.321763	27.199424
246.556155	9917.743143	27.204442
246.284718	9934.574672	27.209460
247.027984	9946.134091	27.214477
246.899554	9976.789748	27.219495
247.080944	9986.698701	27.224512
247.630519	10008.229669	27.229530
247.481509	10033.702765	27.234548
247.891591	10048.412630	27.239565
247.905564	10068.539651	27.244583
248.737481	10085.082144	27.249600
249.377433	10098.501321	27.254618
249.824570	10093.440026	27.259636
250.315772	10104.819779	27.264653
250.042814	10123.328481	27.269671
250.488045	10123.006850	27.274688
250.992770	10111.434494	27.279706
251.108431	10121.711709	27.284724
251.339613	10117.821663	27.289741
251.053059	10129.808631	27.294759
251.290953	10143.483573	27.299776
251.320680	10139.740536	27.304794
251.586196	10153.474832	27.309812
252.119587	10157.645966	27.314829
252.039513	10174.196202	27.319847
252.610263	10198.191744	27.324864
253.029162	10207.578578	27.329882
253.025865	10216.276000	27.334900
253.170424	10238.241951	27.339917
253.527300	10236.828253	27.344935
254.104154	10247.885952	27.349952
254.607679	10263.423634	27.354970
254.429490	10257.902785	27.359988
254.832707	10259.625041	27.365005
254.922180	10280.001600	27.370023
254.987154	10290.039098	27.375040
255.598855	10298.849461	27.380058
255.295219	10321.912263	27.385076
255.779853	10332.796234	27.390093
255.768548	10352.394850	27.395111
255.911109	10371.229560	27.400128
256.052404	10385.820473	27.405146
256.186269	10406.736320	27.410164
256.649584	10420.958375	27.415181
257.212425	10440.325893	27.420199
257.408778	10460.869036	27.425216
257.722134	10469.939553	27.430234
257.752368	10499.331018	27.435252
258.348738	10511.666693	27.440269
258.189187	10529.056759	27.445287
258.517843	10551.312372	27.450304
258.737076	10575.408227	27.455322
258.706669	10601.143165	27.460340
258.944467	10605.739319	27.465357
259.331763	10644.549263	27.470375
259.383393	10655.702001	27.475392
259.687049	10671.462032	27.480410
259.901456	10708.420645	27.485428
260.340890	10729.260294	27.490445
260.879774	10741.804048	27.495463
261.033329	10767.413927	27.500480
261.234431	10785.085623	27.505498
261.688991	10812.601043	27.510516
261.988294	10830.034406	27.515533
262.077279	10851.775764	27.520551
262.509074	10870.023898	27.525568
263.011163	10879.158631	27.530586
263.116685	10902.965004	27.535604
263.397608	10919.898475	27.540621
263.672645	10936.504703	27.545639
263.780209	10949.822185	27.550656
264.215340	10964.257815	27.555674
264.144674	10984.420010	27.560692
264.678948	10991.028747	27.565709
264.985105	11020.895128	27.570727
264.936935	11029.778438	27.575744
265.635298	11041.114865	27.580762
265.324033	11055.979259	27.585780
265.753438	11079.097949	27.590797
266.127864	11092.443463	27.595815
266.204466	11116.308104	27.600832
266.494650	11145.725700	27.605850
266.409064	11159.521205	27.610868
266.805695	11191.005082	27.615885
267.606907	11193.231095	27.620903
267.993130	11214.600539	27.625920
268.553855	11212.593676	27.630938
268.667236	11224.500051	27.635956
269.074942	11228.119129	27.640973
269.364036	11237.623321	27.645991
269.664807	11255.941999	27.651008
270.157584	11265.050315	27.656026
270.173856	11273.686393	27.661044
270.607534	11268.780928	27.666061
270.785584	11282.570139	27.671079
271.009014	11298.489812	27.676096
271.586901	11290.225161	27.681114
271.846863	11283.466676	27.686132
272.328974	11297.650754	27.691149
272.634988	11306.804014	27.696167
272.657402	11315.998351	27.701184
272.890956	11313.502512	27.706202
272.807400	11321.133304	27.711220
273.031257	11322.234352	27.716237
273.309127	11349.375344	27.721255
273.226665	11347.952079	27.726272
273.702107	11363.619144	27.731290
273.884914	11376.986402	27.736308
274.015670	11403.876447	27.741325
274.367075	11418.234558	27.746343
274.824101	11434.070901	27.751360
275.553907	11435.450027	27.756378
275.928409	11450.573068	27.761396
275.896223	11461.739760	27.766413
276.425072	11468.010738	27.771431
276.272835	11475.521702	27.776448
276.773087	11482.587669	27.781466
276.797172	11500.964322	27.786484
276.707557	11507.293947	27.791501
277.096320	11516.841658	27.796519
277.344409	11543.500345	27.801536
277.667022	11560.192946	27.806554
277.845895	11594.942174	27.811572
278.146255	11605.283443	27.816589
278.401455	11611.308843	27.821607
278.592349	11642.639915	27.826624
278.927805	11644.195257	27.831642
278.992043	11678.791756	27.836660
279.360940	11677.763855	27.841677
279.641752	11700.468772	27.846695
279.434748	11710.196568	27.851712
279.800289	11744.462430	27.856730
280.296207	11764.280141	27.861748
280.492085	11780.051426	27.866765
280.989414	11805.134437	27.871783
280.766625	11825.213376	27.876800
281.371904	11835.308641	27.881818
281.965884	11858.827721	27.886836
282.120000	11880.545614	27.891853
282.325419	11894.811939	27.896871
282.384722	11927.025857	27.901888
282.776934	11948.019544	27.906906
283.099891	11972.227422	27.911924
283.135645	12000.668522	27.916941
283.866266	12013.828995	27.921959
283.840670	12048.915871	27.926976
284.426288	12065.395127	27.931994
284.562182	12079.587896	27.937012
284.757067	12109.819899	27.942029
285.135783	12125.380185	27.947047
285.300764	12152.220055	27.952064
285.637514	12191.296654	27.957082
285.787974	12201.915477	27.962100
286.123787	12235.015562	27.967117
286.659097	12242.040289	27.972135
286.617850	12268.166650	27.977152
287.275658	12280.709266	27.982170
287.561255	12315.302237	27.987188
287.651713	12336.075359	27.992205
288.018866	12349.440068	27.997223
288.276424	12380.282283	28.002240
289.067689	12389.146731	28.007258
289.067990	12415.821647	28.012276
289.628333	12421.311112	28.017293
290.343973	12441.812749	28.022311
290.305395	12459.578912	28.027328
290.796126	12462.658470	28.032346
291.345412	12475.664062	28.037364
291.639171	12484.340824	28.042381
292.017672	12486.078308	28.047399
291.889278	12496.894880	28.052416
292.367060	12508.505093	28.057434
292.744571	12516.060833	28.062452
292.665906	12526.129004	28.067469
293.034071	12532.433124	28.072487
293.160992	12554.686843	28.077504
293.199263	12574.387085	28.082522
293.730013	12574.802523	28.087540
293.457928	12615.286846	28.092557
294.290323	12624.767506	28.097575
294.208701	12646.712978	28.102592
294.512996	12655.466284	28.107610
294.913618	12676.106410	28.112628
294.824302	12697.993753	28.117645
294.922371	12704.778054	28.122663
295.733900	12733.556671	28.127680
295.781655	12756.153903	28.132698
296.720426	12769.100328	28.137716
296.651833	12782.400365	28.142733
296.930158	12794.135176	28.147751
297.014147	12828.419529	28.152768
297.199721	12837.647227	28.157786
297.637331	12866.994289	28.162804
297.736084	12886.309036	28.167821
298.025124	12896.609404	28.172839
297.999042	12935.515598	28.177856
298.291215	12955.867677	28.182874
298.860929	12984.829261	28.187892
299.125900	13010.022832	28.192909
299.876168	13028.696096	28.197927
299.743714	13063.533522	28.202944
300.482275	13070.970893	28.207962
300.921500	13097.890142	28.212980
301.362495	13103.015335	28.217997
302.046997	13117.152459	28.223015
301.810852	13136.453890	28.228032
302.133919	13164.885121	28.233050
302.758857	13163.225554	28.238068
302.836714	13194.476391	28.243085
302.888457	13209.185643	28.248103
303.466331	13222.731846	28.253120
303.855351	13236.946850	28.258138
303.723907	13262.231469	28.263156
304.118318	13277.528899	28.268173
304.932383	13294.537982	28.273191
304.927397	13315.046236	28.278208
304.979970	13321.716543	28.283226
305.587864	13339.119750	28.288244
305.717184	13356.525649	28.293261
305.983142	13386.410372	28.298279
306.074661	13390.800050	28.303296
306.412832	13427.809711	28.308314
306.704644	13438.256027	28.313332
306.623352	13469.557292	28.318349
307.112906	13484.378281	28.323367
307.421146	13507.549506	28.328384
307.987786	13530.132785	28.333402
308.571445	13553.446159	28.338420
308.706804	13571.572305	28.343437
309.163623	13600.857599	28.348455
309.393769	13617.804636	28.353472
309.398901	13639.630551	28.358490
309.823234	13662.029970	28.363508
309.883035	13691.048483	28.368525
310.482988	13708.187701	28.373543
310.880463	13726.888630	28.378560
310.784429	13747.843357	28.383578
311.422397	13756.101126	28.388596
311.674394	13778.794451	28.393613
311.993763	13806.702505	28.398631
312.031042	13820.518816	28.403648
312.294470	13859.191013	28.408666
312.730520	13863.234948	28.413684
312.633014	13892.584053	28.418701
313.288509	13917.464486	28.423719
313.517409	13936.928059	28.428736
313.755545	13971.379436	28.433754
314.406889	13985.293456	28.438772
314.554012	14015.820441	28.443789
315.134478	14027.986086	28.448807
315.119906	14061.784309	28.453824
315.603267	14079.255738	28.458842
316.008519	14104.081794	28.463860
316.259419	14122.901427	28.468877
316.759221	14143.834259	28.473895
317.299690	14167.284067	28.478912
317.564111	14182.888293	28.483930
317.918829	14197.957989	28.488948
317.804348	14222.805860	28.493965
318.478464	14238.012053	28.498983
318.964441	14263.872901	28.504000
318.946392	14287.523198	28.509018
319.251339	14294.761840	28.514036
319.434840	14331.230256	28.519053
319.666831	14338.627855	28.524071
320.246625	14373.428354	28.529088
320.266073	14396.999828	28.534106
321.059971	14408.954538	28.539124
321.057970	14442.206734	28.544141
321.433062	14465.888725	28.549159
321.532849	14486.133573	28.554176
321.600611	14507.418965	28.559194
322.450449	14537.612900	28.564212
322.545719	14557.920755	28.569229
322.772792	14583.261316	28.574247
323.167224	14618.965848	28.579264
323.274545	14648.765349	28.584282
323.651233	14685.455835	28.589300
323.905090	14714.619929	28.594317
324.428303	14735.277650	28.599335
325.089386	14769.051331	28.604352
325.039822	14791.734582	28.609370
325.470917	14807.667146	28.614388
325.713322	14852.338837	28.619405
326.096242	14863.565457	28.624423
326.340109	14902.322028	28.629440
326.522490	14918.919130	28.634458
326.956081	14948.346507	28.639476
327.479299	14981.967266	28.644493
327.844466	14992.965061	28.649511
327.995133	15019.998041	28.654528
327.968015	15048.756348	28.659546
328.673041	15072.715183	28.664564
328.807228	15095.118165	28.669581
329.114690	15122.017005	28.674599
329.300797	15140.992383	28.679616
329.695522	15178.134440	28.684634
330.166379	15194.284261	28.689652
330.591084	15217.458999	28.694669
331.324387	15238.064728	28.699687
331.571511	15262.036999	28.704704
331.543855	15290.993450	28.709722
332.229860	15300.630408	28.714740
332.875293	15318.707346	28.719757
333.166625	15327.506966	28.724775
334.190698	15335.582435	28.729792
334.560519	15338.941468	28.734810
335.529887	15339.259158	28.739828
335.782074	15338.303562	28.744845
335.903396	15327.788631	28.749863
336.594772	15332.406450	28.754880
336.385105	15328.767999	28.759898
337.013043	15336.995955	28.764916
337.148214	15362.855618	28.769933
336.998539	15370.080718	28.774951
337.389481	15366.120399	28.779968
337.498690	15372.726184	28.784986
337.592622	15398.781230	28.790004
337.541067	15415.841578	28.795021
337.751911	15431.275917	28.800039
338.117852	15450.396418	28.805056
337.953881	15484.215179	28.810074
338.548386	15510.422694	28.815092
339.002371	15537.382464	28.820109
339.123208	15574.479967	28.825127
339.482591	15598.609653	28.830144
339.722360	15632.515361	28.835162
340.224350	15655.207053	28.840180
340.560994	15694.057218	28.845197
340.911902	15719.932503	28.850215
341.419256	15746.221426	28.855232
341.587885	15770.120986	28.860250
341.984544	15798.223470	28.865268
342.475438	15829.106112	28.870285
342.636339	15856.698113	28.875303
343.221252	15877.737160	28.880320
343.716292	15910.362990	28.885338
344.041281	15929.880528	28.890356
343.959080	15966.233665	28.895373
344.246134	15993.887294	28.900391
344.611530	16016.330451	28.905408
344.617309	16051.986184	28.910426
345.216800	16083.639542	28.915444
345.323203	16111.162541	28.920461
345.691680	16150.527821	28.925479
345.980124	16176.083349	28.930496
346.095196	16207.741133	28.935514
346.575363	16241.949403	28.940532
346.991468	16273.303076	28.945549
347.332942	16303.014924	28.950567
348.059140	16333.913043	28.955584
348.293129	16373.520185	28.960602
348.724863	16390.454990	28.965620
349.739894	16417.351104	28.970637
349.310997	16446.698632	28.975655
349.827036	16464.815062	28.980672
350.060052	16497.265796	28.985690
350.194693	16531.354980	28.990708
350.762601	16560.941484	28.995725
351.290359	16590.300209	29.000743
352.146490	16600.156335	29.005760
352.539592	16640.485994	29.010778
353.352627	16646.568387	29.015796
354.181753	16640.615226	29.020813
354.628234	16637.702157	29.025831
355.333597	16653.970663	29.030848
355.227035	16671.095487	29.035866
355.599394	16658.979326	29.040884
356.161843	16658.628694	29.045901
356.068649	16674.002893	29.050919
356.443210	16670.273975	29.055936
356.622806	16691.774565	29.060954
356.691693	16705.837426	29.065972
356.966577	16706.946694	29.070989
356.950626	16728.651712	29.076007
357.638987	16754.044082	29.081024
358.335122	16761.495064	29.086042
358.334750	16787.970997	29.091060
358.189049	16802.092549	29.096077
358.395577	16843.858879	29.101095
358.974782	16845.896771	29.106112
358.982649	16893.199883	29.111130
359.519390	16919.485338	29.116148
359.971068	16940.802767	29.121165
360.219398	16977.221150	29.126183
360.658856	16996.700932	29.131200
361.031410	17028.726629	29.136218
362.416725	17032.016343	29.141236
363.165157	17038.608971	29.146253
363.595240	17040.848992	29.151271
364.135873	17031.657363	29.156288
364.629394	17035.248627	29.161306
364.827344	17028.342605	29.166324
365.278273	17043.420041	29.171341
365.433979	17058.572881	29.176359
365.745158	17068.255928	29.181376
365.871378	17070.716019	29.186394
365.597902	17079.174580	29.191412
365.918137	17098.578219	29.196429
365.843422	17118.638887	29.201447
366.115474	17136.406619	29.206464
366.337082	17158.429488	29.211482
366.373236	17180.765000	29.216500
366.839355	17206.764573	29.221517
366.973867	17240.461260	29.226535
367.375358	17278.638958	29.231552
367.546511	17317.275095	29.236570
367.980316	17345.975249	29.241588
368.364691	17387.265700	29.246605
368.298967	17422.695042	29.251623
368.532573	17461.708979	29.256640
368.882246	17507.463462	29.261658
369.465491	17557.737885	29.266676
369.705067	17588.326499	29.271693
370.028471	17630.087936	29.276711
370.473842	17680.758347	29.281728
370.913571	17720.856225	29.286746
371.345002	17758.723639	29.291764
371.668853	17804.133109	29.296781
371.849435	17845.150163	29.301799
372.539498	17887.827100	29.306816
372.673782	17929.284040	29.311834
373.439734	17968.028985	29.316852
374.318373	18010.013208	29.321869
374.293000	18052.779796	29.326887
374.891658	18087.142559	29.331904
375.427641	18119.616129	29.336922
375.613285	18157.290997	29.341940
376.280066	18187.772559	29.346957
376.673670	18220.672582	29.351975
377.758268	18233.186355	29.356992
378.124929	18261.263842	29.362010
378.421180	18288.058854	29.367028
379.162706	18302.789235	29.372045
379.276827	18322.368197	29.377063
379.373569	18346.685169	29.382080
379.830450	18360.227450	29.387098
380.053441	18390.681303	29.392116
380.322131	18411.739352	29.397133
380.593676	18443.895879	29.402151
380.821964	18468.792894	29.407168
381.653059	18502.070672	29.412186
381.547390	18529.536077	29.417204
381.972739	18558.165799	29.422221
382.342444	18592.754755	29.427239
383.149677	18627.652045	29.432256
383.375830	18647.773044	29.437274
383.709694	18670.657776	29.442292
384.285085	18708.259667	29.447309
384.484825	18734.469608	29.452327
385.172548	18756.735450	29.457344
385.460580	18787.990002	29.462362
385.677789	18811.179375	29.467380
386.195103	18839.926466	29.472397
386.365693	18872.055077	29.477415
386.727181	18897.519783	29.482432
387.034368	18913.330264	29.487450
387.142109	18938.267709	29.492468
387.669086	18962.254074	29.497485
387.543483	18998.321778	29.502503
388.016324	19029.063470	29.507520
388.420548	19059.502743	29.512538
388.618388	19096.623165	29.517556
389.567583	19126.880845	29.522573
389.825942	19166.091184	29.527591
390.235487	19187.243201	29.532608
390.603005	19225.799231	29.537626
391.109388	19262.501558	29.542644
391.206565	19296.664193	29.547661
391.305599	19328.631111	29.552679
391.787346	19363.793746	29.557696
392.283142	19409.139542	29.562714
392.714131	19450.258724	29.567732
393.466734	19482.882924	29.572749
393.725175	19519.513537	29.577767
394.956156	19533.811551	29.582784
395.412793	19564.467105	29.587802
395.718952	19589.272386	29.592820
396.218302	19607.044523	29.597837
396.383062	19635.688607	29.602855
396.857709	19658.807898	29.607872
397.182460	19669.023150	29.612890
397.332165	19703.819720	29.617908
397.880613	19726.807654	29.622925
398.419313	19756.546458	29.627943
398.473285	19786.458629	29.632960
398.671374	19818.289881	29.637978
399.057371	19854.802517	29.642996
399.694622	19878.382511	29.648013
399.914133	19907.994878	29.653031
399.989058	19946.268549	29.658048
401.019218	19976.153905	29.663066
400.889666	20006.465081	29.668084
401.779562	20041.556726	29.673101
401.974151	20070.060610	29.678119
402.499379	20095.556698	29.683136
402.854088	20131.980462	29.688154
403.211006	20172.464426	29.693172
403.693830	20195.574546	29.698189
403.869660	20233.378437	29.703207
404.324147	20260.552865	29.708224
404.797540	20289.320647	29.713242
404.629906	20331.046264	29.718260
405.475421	20364.927397	29.723277
405.704594	20394.109936	29.728295
405.713819	20446.779606	29.733312
406.771333	20486.507759	29.738330
406.862784	20521.346529	29.743348
407.223691	20551.484134	29.748365
407.714675	20596.193466	29.753383
408.018289	20627.368877	29.758400
408.583039	20664.603871	29.763418
409.368449	20693.944056	29.768436
409.602610	20711.261183	29.773453
410.171770	20734.418984	29.778471
410.755974	20751.447268	29.783488
411.600276	20777.971394	29.788506
412.060107	20797.708251	29.793524
412.813403	20799.218466	29.798541
413.048431	20826.338272	29.803559
413.400688	20843.691071	29.808576
413.645621	20851.485083	29.813594
413.536621	20880.260898	29.818612
413.790366	20889.514446	29.823629
414.621537	20919.301398	29.828647
414.752166	20955.884059	29.833664
415.223720	20978.241070	29.838682
415.079477	21016.599518	29.843700
415.668304	21045.788182	29.848717
415.964429	21080.317568	29.853735
416.377718	21115.673424	29.858752
416.856764	21151.372503	29.863770
417.247094	21189.428828	29.868788
417.691032	21222.169234	29.873805
418.261923	21249.546561	29.878823
418.280119	21291.716869	29.883840
418.790173	21322.409484	29.888858
418.971608	21365.951149	29.893876
419.749513	21393.799797	29.898893
420.288238	21437.837619	29.903911
420.451748	21481.387184	29.908928
421.116362	21508.103418	29.913946
421.106242	21557.383792	29.918964
421.697924	21589.079127	29.923981
422.347771	21640.648896	29.928999
422.400318	21673.357298	29.934016
423.262724	21706.510897	29.939034
423.742051	21743.675420	29.944052
424.449315	21781.090402	29.949069
424.852883	21809.000214	29.954087
425.043765	21848.734425	29.959104
426.004505	21863.761689	29.964122
426.406129	21900.179708	29.969140
426.695817	21924.135168	29.974157
427.237211	21950.596910	29.979175
427.327904	21979.824139	29.984192
427.871543	22001.036956	29.989210
428.073567	22036.239508	29.994228
428.444421	22070.532321	29.999245
429.141303	22103.349249	30.004263
429.570128	22128.194127	30.009280
430.586860	22149.778351	30.014298
431.084350	22174.279198	30.019316
431.278531	22198.537773	30.024333
431.587721	22215.181421	30.029351
431.836579	22248.558359	30.034368
432.449958	22261.650230	30.039386
432.545068	22292.213148	30.044404
432.701596	22311.805684	30.049421
433.151613	22340.356467	30.054439
433.642259	22386.969123	30.059456
434.110498	22405.196766	30.064474
434.418494	22435.386572	30.069492
434.589016	22470.811709	30.074509
434.908104	22499.010298	30.079527
434.977014	22541.500362	30.084544
435.797176	22577.068767	30.089562
436.110341	22622.886519	30.094580
436.416862	22660.874676	30.099597
437.313995	22707.596797	30.104615
436.892163	22751.746419	30.109632
437.537976	22782.391100	30.114650
438.087479	22840.460790	30.119668
438.157978	22883.632050	30.124685
438.880912	22929.522455	30.129703
439.324457	22980.875835	30.134720
439.968865	23016.136896	30.139738
440.295049	23060.764464	30.144756
440.754490	23107.791434	30.149773
441.349024	23146.415412	30.154791
441.616822	23198.036158	30.159808
441.985267	23237.275317	30.164826
442.760763	23280.714996	30.169844
443.275336	23326.316797	30.174861
443.570663	23362.157261	30.179879
444.233367	23406.766845	30.184896
445.343260	23434.282640	30.189914
445.980424	23472.543012	30.194932
445.886747	23501.523573	30.199949
446.706251	23520.295970	30.204967
447.001699	23562.756609	30.209984
447.530816	23592.519543	30.215002
448.213877	23618.661395	30.220020
448.510105	23645.748712	30.225037
449.058449	23675.402399	30.230055
449.282535	23716.738959	30.235072
449.711491	23739.636788	30.240090
449.983006	23777.631616	30.245108
450.597485	23810.792896	30.250125
450.962298	23833.352914	30.255143
451.190837	23873.503676	30.260160
451.485585	23911.486456	30.265178
452.418630	23947.786703	30.270196
452.524354	23994.394505	30.275213
452.511881	24033.050387	30.280231
453.058635	24083.659097	30.285248
453.623294	24120.105075	30.290266
453.992785	24165.838736	30.295284
454.391086	24214.220992	30.300301
455.330244	24230.797903	30.305319
455.710999	24269.350749	30.310336
455.902538	24301.994364	30.315354
456.717556	24324.573157	30.320372
457.663586	24348.664821	30.325389
458.087610	24375.375390	30.330407
458.249586	24400.345112	30.335424
458.760220	24428.553631	30.340442
459.299760	24456.798558	30.345460
459.654909	24492.806913	30.350477
459.955359	24512.302821	30.355495
460.441802	24541.989253	30.360512
460.977760	24578.140723	30.365530
461.555028	24609.116523	30.370548
461.895185	24640.686305	30.375565
462.539482	24660.859432	30.380583
462.689869	24692.902262	30.385600
463.316471	24720.135711	30.390618
463.868620	24749.676570	30.395636
464.258352	24785.780119	30.400653
464.912336	24808.577467	30.405671
464.741496	24849.508797	30.410688
465.363296	24870.450684	30.415706
465.907623	24911.857483	30.420724
466.114988	24966.849428	30.425741
466.651100	25000.334471	30.430759
466.666450	25036.965372	30.435776
467.236235	25079.318593	30.440794
467.529497	25126.403986	30.445812
468.057919	25167.228668	30.450829
468.747245	25206.270301	30.455847
469.094928	25265.362540	30.460864
469.650927	25311.334459	30.465882
470.212524	25351.298011	30.470900
470.636294	25397.596113	30.475917
471.323695	25435.254479	30.480935
471.514848	25487.042934	30.485952
472.499467	25518.275446	30.490970
473.337350	25543.413425	30.495988
473.693501	25590.928174	30.501005
474.493387	25610.675945	30.506023
474.785945	25644.036486	30.511040
475.635116	25669.380844	30.516058
476.347086	25690.228300	30.521076
476.679158	25726.700816	30.526093
476.953924	25749.366120	30.531111
477.210576	25788.980717	30.536128
477.604455	25815.778064	30.541146
478.333019	25840.517967	30.546164
478.350103	25888.725732	30.551181
479.045514	25908.137578	30.556199
479.009828	25951.715333	30.561216
479.426163	25992.654510	30.566234
479.908582	26028.551505	30.571252
479.911262	26077.593272	30.576269
480.605486	26110.546521	30.581287
480.744364	26158.211005	30.586304
481.062508	26200.987003	30.591322
481.811294	26251.303311	30.596340
482.190379	26298.068852	30.601357
482.655852	26331.872032	30.606375
482.886649	26385.983519	30.611392
483.220531	26430.237952	30.616410
484.214953	26478.860607	30.621428
484.562159	26521.456352	30.626445
485.276571	26560.289297	30.631463
485.720552	26604.447099	30.636480
486.576538	26641.804122	30.641498
487.442233	26668.164535	30.646516
487.797868	26709.116780	30.651533
488.464491	26740.734018	30.656551
488.892168	26776.268750	30.661568
489.083675	26815.216334	30.666586
489.713063	26842.749183	30.671604
489.944593	26892.684273	30.676621
490.376306	26927.052669	30.681639
490.797080	26977.378591	30.686656
491.243125	27012.264872	30.691674
491.780023	27057.689387	30.696692
492.066804	27108.511355	30.701709
492.858806	27153.345572	30.706727
493.347303	27198.018687	30.711744
493.729937	27244.401138	30.716762
494.190404	27279.681212	30.721780
494.605857	27337.471842	30.726797
495.251337	27368.452349	30.731815
495.548993	27416.394647	30.736832
495.922564	27467.255916	30.741850
496.820425	27511.666143	30.746868
497.267106	27556.118422	30.751885
497.815277	27603.028629	30.756903
498.546387	27651.874833	30.761920
498.971633	27692.381989	30.766938
499.456164	27728.281645	30.771956
499.932258	27774.496300	30.776973
500.502390	27806.676225	30.781991
501.306946	27849.241225	30.787008
501.669213	27888.852819	30.792026
502.534666	27922.527070	30.797044
502.613422	27958.819643	30.802061
503.408951	27989.147114	30.807079
503.884243	28031.661040	30.812096
504.545121	28067.788642	30.817114
505.022452	28105.366958	30.822132
505.013549	28147.266527	30.827149
505.530649	28186.962917	30.832167
506.175015	28231.448595	30.837184
506.606522	28266.213830	30.842202
507.013167	28314.566901	30.847220
507.180063	28360.589799	30.852237
507.791293	28403.420278	30.857255
508.272680	28444.136262	30.862272
508.619146	28486.104590	30.867290
508.917175	28526.739677	30.872308
509.157180	28572.538787	30.877325
510.118173	28607.278720	30.882343
510.816346	28657.967523	30.887360
511.349582	28712.776910	30.892378
511.587716	28739.803269	30.897396
511.989186	28796.640032	30.902413
512.548548	28843.986994	30.907431
512.959229	28892.430966	30.912448
513.339209	28941.693141	30.917466
514.154161	28993.335149	30.922484
514.324360	29047.957648	30.927501
514.841043	29090.816030	30.932519
515.720842	29149.208913	30.937536
516.201764	29202.409802	30.942554
516.920033	29238.760956	30.947572
517.197124	29293.242751	30.952589
517.313506	29338.009399	30.957607
518.017997	29394.010429	30.962624
518.564394	29453.012242	30.967642
519.304924	29501.358206	30.972660
519.857617	29561.946404	30.977677
520.306226	29598.048182	30.982695
520.744277	29650.147876	30.987712
521.495155	29711.245621	30.992730
522.316136	29755.069061	30.997748
522.548421	29811.372106	31.002765
523.155607	29856.121883	31.007783
523.448416	29908.426775	31.012800
524.173531	29954.850664	31.017818
525.122990	29992.414872	31.022836
525.789665	30055.751068	31.027853
526.128726	30083.075627	31.032871
526.793336	30126.698027	31.037888
527.311378	30174.369061	31.042906
528.289793	30211.949652	31.047924
528.343603	30260.746093	31.052941
528.874898	30301.318501	31.057959
529.681592	30333.508302	31.062976
530.015526	30379.735660	31.067994
530.436790	30412.852259	31.073012
530.935918	30454.616936	31.078029
531.597173	30496.565512	31.083047
532.214572	30541.966453	31.088064
532.825503	30584.818475	31.093082
533.090506	30625.553882	31.098100
533.656290	30667.637885	31.103117
534.110369	30712.822597	31.108135
534.850802	30752.188633	31.113152
535.095824	30794.174323	31.118170
535.401268	30849.000367	31.123188
536.144185	30890.174117	31.128205
536.387357	30933.731825	31.133223
537.163777	30968.625984	31.138240
537.384627	31022.534604	31.143258
538.096738	31060.987022	31.148276
538.573615	31095.125343	31.153293
539.103483	31155.839708	31.158311
539.653057	31182.376034	31.163328
539.931741	31235.760749	31.168346
540.412289	31282.879877	31.173364
541.264161	31333.208907	31.178381
541.616382	31376.484052	31.183399
542.133015	31418.355573	31.188416
542.541749	31468.049484	31.193434
542.909421	31515.100567	31.198452
543.658063	31571.759274	31.203469
544.087381	31623.630207	31.208487
544.793106	31671.814748	31.213504
545.212204	31732.999670	31.218522
545.827597	31784.631841	31.223540
546.084071	31844.511205	31.228557
546.492727	31902.374241	31.233575
547.445786	31955.122700	31.238592
547.839077	32025.153710	31.243610
548.443064	32081.115307	31.248628
549.074649	32124.300635	31.253645
549.294741	32191.748151	31.258663
550.202678	32246.796555	31.263680
550.775358	32294.613205	31.268698
551.569084	32350.370534	31.273716
551.839458	32402.182536	31.278733
552.023229	32464.749031	31.283751
553.344403	32512.710332	31.288768
553.672834	32582.820238	31.293786
554.246652	32623.993737	31.298804
555.393020	32677.383631	31.303821
556.341186	32716.024576	31.308839
557.681186	32747.267230	31.313856
558.414335	32760.195703	31.318874
558.832423	32790.240708	31.323892
560.014018	32798.964792	31.328909
560.649124	32817.750613	31.333927
561.514392	32822.660054	31.338944
561.944573	32847.988586	31.343962
562.358524	32854.662843	31.348980
562.828768	32864.395587	31.353997
563.197363	32890.988716	31.359015
563.614210	32909.962304	31.364032
563.865458	32935.809695	31.369050
564.341568	32956.430580	31.374068
564.538549	32999.632249	31.379085
564.978791	33025.794889	31.384103
565.510873	33049.348351	31.389120
565.554593	33104.820995	31.394138
566.065538	33146.193392	31.399156
566.920096	33190.242921	31.404173
566.892473	33235.189700	31.409191
567.465617	33270.061218	31.414208
567.827226	33323.942323	31.419226
568.335530	33362.533462	31.424244
568.674430	33419.933714	31.429261
568.796706	33472.538753	31.434279
569.657106	33517.652253	31.439296
569.852926	33580.544192	31.444314
570.323092	33641.099075	31.449332
570.959793	33696.469796	31.454349
571.102506	33767.541191	31.459367
571.985098	33823.539978	31.464384
572.337177	33894.969514	31.469402
573.026155	33954.560625	31.474420
573.647520	34017.124761	31.479437
574.427251	34098.631157	31.484455
574.781416	34145.904685	31.489472
575.238216	34210.057972	31.494490
575.753535	34282.555626	31.499508
576.516026	34345.098518	31.504525
576.889650	34424.686468	31.509543
577.873184	34479.804352	31.514560
578.975173	34542.675416	31.519578
579.849692	34583.184773	31.524596
580.791553	34647.721241	31.529613
581.170043	34695.241533	31.534631
581.963951	34745.453034	31.539648
582.550963	34795.874200	31.544666
583.279743	34845.295528	31.549684
583.919838	34878.324748	31.554701
584.848640	34921.911447	31.559719
585.629036	34969.149382	31.564736
585.819898	34999.433210	31.569754
586.655214	35041.327776	31.574772
587.265744	35082.101100	31.579789
587.509769	35126.382268	31.584807
588.587502	35166.192248	31.589824
589.115843	35215.955591	31.594842
589.496443	35259.081853	31.599860
589.977999	35290.136545	31.604877
590.155993	35342.398078	31.609895
590.413851	35383.649233	31.614912
591.345492	35442.161783	31.619930
591.631173	35493.167486	31.624948
591.949440	35548.563541	31.629965
592.634920	35615.473128	31.634983
592.850434	35662.183402	31.640000
593.577117	35729.704890	31.645018
594.174635	35790.245715	31.650036
594.408586	35848.575978	31.655053
595.178308	35926.908228	31.660071
595.794322	35989.100650	31.665088
596.155142	36062.228148	31.670106
596.897672	36136.666811	31.675124
597.393072	36186.958559	31.680141
597.918874	36264.110941	31.685159
598.783989	36319.685747	31.690176
599.605907	36370.269747	31.695194
599.711205	36433.823781	31.700212
600.345778	36497.594904	31.705229
600.950045	36546.724184	31.710247
601.862934	36607.813700	31.715264
602.783741	36657.534587	31.720282
603.295178	36710.756326	31.725300
604.325161	36763.790020	31.730317
604.483151	36824.149147	31.735335
605.213981	36865.714902	31.740352
605.596571	36933.095788	31.745370
606.042128	36987.270162	31.750388
606.835358	37036.895815	31.755405
607.699870	37095.949858	31.760423
608.258727	37155.842704	31.765440
609.071995	37210.356564	31.770458
609.777645	37265.392283	31.775476
610.684131	37314.650692	31.780493
611.044039	37376.252038	31.785511
611.418776	37409.826747	31.790528
612.647297	37455.716885	31.795546
613.045301	37510.286808	31.800564
613.652470	37566.857576	31.805581
614.101832	37613.457186	31.810599
614.666913	37659.638007	31.815616
615.396293	37715.850814	31.820634
615.560610	37779.011060	31.825652
616.591290	37831.757887	31.830669
616.812512	37899.556206	31.835687
617.036850	37958.926500	31.840704
618.145662	38008.271397	31.845722
618.660891	38066.969771	31.850740
619.406023	38126.547846	31.855757
620.019334	38186.221231	31.860775
620.681337	38253.711105	31.865792
621.274650	38309.698421	31.870810
621.546168	38367.441686	31.875828
622.224955	38428.672839	31.880845
622.839591	38489.450846	31.885863
623.751430	38550.519182	31.890880
624.234162	38610.899195	31.895898
624.725458	38680.556124	31.900916
625.209311	38738.006660	31.905933
626.146419	38807.173679	31.910951
626.744705	38864.939136	31.915968
627.310605	38921.092096	31.920986
627.386971	39005.042793	31.926004
628.643561	39056.235795	31.931021
629.154454	39134.551606	31.936039
629.611856	39193.783453	31.941056
630.743220	39247.450594	31.946074
630.953272	39314.909425	31.951092
631.531731	39368.136733	31.956109
632.461597	39432.277160	31.961127
633.023548	39484.564474	31.966144
633.881164	39537.651670	31.971162
634.132906	39599.442307	31.976180
634.819289	39640.616694	31.981197
635.593482	39709.472712	31.986215
636.375368	39766.060837	31.991232
637.094775	39812.233981	31.996250
637.785308	39860.745719	32.001268
638.319433	39921.231005	32.006285
638.742631	39980.412684	32.011303
639.351974	40023.990922	32.016320
639.932647	40091.849548	32.021338
640.427627	40152.931670	32.026356
641.244368	40208.064904	32.031373
641.492025	40277.305102	32.036391
642.052393	40341.944612	32.041408
643.013717	40399.960246	32.046426
643.491749	40471.905355	32.051444
644.422279	40535.792777	32.056461
644.977838	40599.702298	32.061479
645.300895	40664.134798	32.066496
646.315628	40724.104833	32.071514
646.932983	40785.892004	32.076532
648.485544	40840.235147	32.081549
649.214815	40887.641289	32.086567
649.757537	40944.451183	32.091584
650.693377	40983.671412	32.096602
651.365575	41036.584626	32.101620
651.677007	41088.981400	32.106637
652.635851	41142.208865	32.111655
652.962096	41187.005322	32.116672
653.980334	41228.774140	32.121690
654.209145	41283.953991	32.126708
655.491470	41317.574840	32.131725
656.069482	41369.179336	32.136743
656.343859	41428.279320	32.141760
657.385380	41466.342021	32.146778
657.666161	41531.819080	32.151796
658.345251	41579.291902	32.156813
659.207936	41612.595338	32.161831
660.079921	41662.731365	32.166848
661.151578	41706.495768	32.171866
661.324709	41752.081398	32.176884
662.186848	41790.570815	32.181901
662.647838	41845.172971	32.186919
662.793960	41898.298775	32.191936
663.448027	41939.209425	32.196954
663.958098	41996.740862	32.201972
664.816920	42062.541111	32.206989
665.237117	42102.297068	32.212007
665.853674	42167.909184	32.217024
667.244294	42203.946503	32.222042
667.814677	42275.231519	32.227060
668.427222	42323.445641	32.232077
669.116011	42378.571533	32.237095
669.548349	42420.357685	32.242112
669.978247	42462.753117	32.247130
670.293426	42526.241233	32.252148
670.881123	42573.169873	32.257165
671.031903	42643.368717	32.262183
671.647460	42702.503913	32.267200
672.227732	42766.256678	32.272218
672.580092	42843.291391	32.277236
673.747817	42911.701722	32.282253
673.862521	42979.680641	32.287271
674.347200	43054.108575	32.292288
675.106240	43135.786296	32.297306
675.388461	43214.606643	32.302324
676.024537	43300.809335	32.307341
676.867043	43385.894433	32.312359
677.339017	43470.934844	32.317376
678.131338	43556.012994	32.322394
678.635945	43649.743037	32.327412
679.497101	43733.186492	32.332429
680.443137	43810.471670	32.337447
680.848820	43899.508994	32.342464
681.803102	43977.301495	32.347482
682.440921	44076.993813	32.352500
682.981528	44155.165284	32.357517
683.747948	44239.348670	32.362535
685.287732	44315.585695	32.367552
686.600659	44380.612652	32.372570
687.425482	44455.497187	32.377588
688.306421	44505.968130	32.382605
689.201476	44567.838190	32.387623
689.910765	44627.327819	32.392640
690.982464	44676.977046	32.397658
691.433081	44738.186568	32.402676
692.078363	44787.071141	32.407693
692.713327	44842.935882	32.412711
692.918816	44918.728638	32.417728
694.021491	44970.957555	32.422746
694.359745	45037.927773	32.427764
694.977210	45106.099953	32.432781
695.779025	45165.217035	32.437799
696.030304	45229.772603	32.442816
696.887304	45290.632269	32.447834
697.305152	45376.788493	32.452852
698.333556	45450.076909	32.457869
699.115554	45516.987777	32.462887
699.569704	45588.352212	32.467904
700.502082	45640.178022	32.472922
700.847635	45726.423193	32.477940
701.127420	45790.480963	32.482957
702.747648	45855.858874	32.487975
702.926943	45930.549629	32.492992
703.383772	45996.021790	32.498010
704.210008	46080.687242	32.503028
704.937240	46166.312218	32.508045
705.459381	46237.362431	32.513063
706.108225	46308.175061	32.518080
706.841724	46369.477761	32.523098
707.388956	46447.674200	32.528116
707.921067	46504.873131	32.533133
709.255745	46574.410265	32.538151
709.578090	46653.801345	32.543168
710.178621	46720.534303	32.548186
711.072496	46793.707774	32.553204
711.937184	46866.580146	32.558221
712.794677	46938.611537	32.563239
713.298354	47011.093949	32.568256
713.973678	47077.103281	32.573274
714.772616	47149.425668	32.578292
715.115899	47228.661398	32.583309
716.162198	47297.329136	32.588327
716.669281	47370.238436	32.593344
717.416339	47452.534578	32.598362
718.103053	47534.105532	32.603380
718.648739	47617.816510	32.608397
719.362628	47691.625022	32.613415
720.147476	47781.637696	32.618432
721.076539	47849.234507	32.623450
721.793137	47935.661759	32.628468
722.532589	48024.581681	32.633485
723.493259	48088.854942	32.638503
724.003844	48178.774461	32.643520
724.800491	48253.430406	32.648538
725.892808	48326.726946	32.653556
726.920832	48392.909079	32.658573
727.743206	48453.974530	32.663591
728.449132	48528.175916	32.668608
729.088771	48592.088748	32.673626
730.003341	48665.661113	32.678644
730.427246	48745.916324	32.683661
731.238612	48794.003037	32.688679
731.729075	48883.531739	32.693696
732.353329	48965.213890	32.698714
733.006955	49035.184697	32.703732
733.692514	49113.689612	32.708749
734.580416	49191.222304	32.713767
734.761870	49274.481570	32.718784
735.577158	49358.116816	32.723802
736.630694	49444.535642	32.728820
736.807625	49534.653981	32.733837
737.557594	49614.583503	32.738855
738.283292	49705.312740	32.743872
738.917828	49798.688780	32.748890
739.574605	49884.974094	32.753908
740.317863	49973.862134	32.758925
741.436414	50069.481980	32.763943
741.805860	50146.940419	32.768960
742.951210	50244.046439	32.773978
743.944387	50323.646935	32.778996
744.543983	50414.327263	32.784013
745.908214	50500.310425	32.789031
746.424574	50564.306758	32.794048
747.199595	50647.203369	32.799066
747.996555	50706.147254	32.804084
748.799023	50782.737930	32.809101
749.797906	50840.151086	32.814119
750.010434	50922.772435	32.819136
750.690003	50982.660586	32.824154
751.505780	51063.242530	32.829172
751.872563	51143.546004	32.834189
752.765099	51219.205837	32.839207
753.508336	51293.400154	32.844224
754.061831	51374.189353	32.849242
755.066980	51445.685299	32.854260
755.534686	51533.343618	32.859277
756.430137	51614.527611	32.864295
757.135899	51707.173218	32.869312
757.424152	51791.405531	32.874330
758.684206	51868.385619	32.879348
759.353790	51960.798430	32.884365
760.362576	52037.986512	32.889383
761.222022	52130.464653	32.894400
762.003493	52204.350499	32.899418
762.984194	52287.616446	32.904436
763.580560	52368.488493	32.909453
765.082045	52423.794165	32.914471
766.021308	52516.046960	32.919488
766.832194	52573.255713	32.924506
767.621337	52639.283288	32.929524
768.063708	52728.277035	32.934541
768.533140	52785.553437	32.939559
769.487624	52869.637384	32.944576
770.222192	52944.123933	32.949594
770.629882	53026.275663	32.954612
771.240816	53116.690042	32.959629
771.920040	53189.033844	32.964647
772.394259	53291.060662	32.969664
772.967076	53371.792594	32.974682
773.918629	53464.082982	32.979700
774.414694	53565.198844	32.984717
775.382502	53661.963328	32.989735
776.584290	53761.285614	32.994752
777.022867	53857.317880	32.999770
778.002435	53940.626328	33.004788
778.878591	54014.163595	33.009805
779.827627	54100.435191	33.014823
780.868886	54192.415139	33.019840
781.552077	54269.970738	33.024858
782.455652	54347.797765	33.029876
783.139089	54446.653921	33.034893
784.112549	54517.011779	33.039911
785.742990	54593.281641	33.044928
786.619679	54660.524203	33.049946
787.315543	54723.259859	33.054964
787.929126	54799.269464	33.059981
788.729263	54851.938533	33.064999
789.517808	54932.699866	33.070016
789.936364	54990.445856	33.075034
790.984247	55049.619647	33.080052
791.511663	55124.387998	33.085069
792.353101	55186.306611	33.090087
793.236622	55246.981341	33.095104
793.861581	55313.227846	33.100122
794.326373	55373.354100	33.105140
795.060868	55461.175154	33.110157
795.893264	55520.119609	33.115175
796.196124	55601.560966	33.120192
796.966328	55686.665827	33.125210
798.663478	55740.716212	33.130228
799.240720	55834.119885	33.135245
799.796656	55905.345041	33.140263
800.522833	55976.110902	33.145280
801.097461	56078.440357	33.150298
802.243619	56146.684067	33.155316
802.865775	56240.148948	33.160333
803.481650	56313.424373	33.165351
804.463923	56399.139613	33.170368
805.196896	56473.268319	33.175386
806.260242	56559.340752	33.180404
806.968442	56634.500025	33.185421
807.499237	56732.111116	33.190439
808.506889	56809.133350	33.195456
808.935501	56896.309117	33.200474
809.944122	56993.545633	33.205492
810.346941	57083.908566	33.210509
811.120151	57176.975321	33.215527
811.962601	57287.701080	33.220544
812.429735	57388.953132	33.225562
813.255249	57488.213454	33.230580
813.922286	57581.854777	33.235597
814.663683	57694.063908	33.240615
815.787959	57789.461434	33.245632
816.456156	57898.700037	33.250650
817.440257	57993.565279	33.255668
817.908256	58113.968916	33.260685
819.111554	58212.869909	33.265703
819.849509	58321.058043	33.270720
820.343365	58429.538229	33.275738
821.475956	58535.940993	33.280756
822.114453	58641.943109	33.285773
822.763804	58748.837594	33.290791
823.666534	58872.356268	33.295808
824.247343	58972.307546	33.300826
825.636877	59072.035929	33.305844
826.162986	59193.592861	33.310861
826.952107	59302.327920	33.315879
828.307400	59401.362592	33.320896
829.155339	59518.194412	33.325914
830.402698	59608.078423	33.330932
831.407885	59718.218116	33.335949
831.773260	59797.950346	33.340967
832.944358	59894.459459	33.345984
833.494066	59984.026902	33.351002
834.526614	60064.512906	33.356020
834.993503	60170.611001	33.361037
836.076903	60260.742108	33.366055
837.343771	60334.172917	33.371072
837.846581	60425.486551	33.376090
838.643703	60515.405529	33.381108
839.350399	60599.943109	33.386125
840.241596	60700.264697	33.391143
841.069988	60792.977616	33.396160
841.736481	60885.824115	33.401178
842.734330	60979.363530	33.406196
843.249891	61077.397662	33.411213
844.077950	61169.408342	33.416231
845.183464	61265.161328	33.421248
845.878098	61370.510006	33.426266
846.698268	61470.787010	33.431284
847.168702	61572.828519	33.436301
848.031631	61683.251835	33.441319
849.228477	61783.088470	33.446336
849.829704	61899.352288	33.451354
850.778736	61998.847415	33.456372
851.396903	62116.701386	33.461389
852.075828	62233.523294	33.466407
853.174006	62333.691162	33.471424
853.745816	62458.643946	33.476442
854.688428	62560.483007	33.481460
855.541020	62686.652594	33.486477
856.325735	62801.121174	33.491495
857.270699	62908.715421	33.496512
858.064157	63034.723045	33.501530
859.567033	63136.062345	33.506548
860.517924	63247.718697	33.511565
861.170092	63356.862114	33.516583
862.414580	63446.632264	33.521600
863.011978	63570.040858	33.526618
863.931539	63667.904095	33.531636
865.322604	63766.608637	33.536653
866.231839	63883.858797	33.541671
867.308348	63966.890374	33.546688
867.573968	64074.709853	33.551706
868.788801	64182.262035	33.556724
869.647061	64273.367111	33.561741
871.029242	64372.006723	33.566759
872.322559	64444.296565	33.571776
873.487268	64535.587830	33.576794
874.298094	64620.581549	33.581812
875.727176	64707.069000	33.586829
875.901955	64790.301342	33.591847
876.858649	64859.298604	33.596864
877.203261	64962.660555	33.601882
878.047614	65050.155341	33.606900
878.826818	65139.754836	33.611917
879.635384	65222.654484	33.616935
880.856665	65306.989012	33.621952
881.801295	65388.127493	33.626970
882.633449	65453.277763	33.631988
883.192359	65544.117526	33.637005
884.089848	65618.053967	33.642023
884.855044	65695.492273	33.647040
885.423512	65800.977121	33.652058
886.364433	65887.168569	33.657076
887.235435	65983.930134	33.662093
887.733073	66066.064864	33.667111
888.752377	66162.348910	33.672128
889.537986	66257.833631	33.677146
890.158868	66366.313773	33.682164
890.886229	66462.734212	33.687181
891.750405	66577.939178	33.692199
892.541839	66679.492573	33.697216
893.269844	66787.348432	33.702234
894.112688	66911.983908	33.707252
895.305590	67016.614810	33.712269
896.016720	67142.011835	33.717287
897.162887	67249.967977	33.722304
897.993530	67366.496959	33.727322
898.904578	67462.172972	33.732340
900.317582	67580.259392	33.737357
901.326509	67685.611773	33.742375
902.484056	67785.691290	33.747392
903.011417	67888.550203	33.752410
903.715053	68005.551766	33.757428
904.745107	68114.245066	33.762445
905.172978	68236.541770	33.767463
906.488218	68332.517852	33.772480
907.123333	68453.639452	33.777498
908.021659	68577.367032	33.782516
909.039377	68688.080836	33.787533
909.905866	68814.228353	33.792551
911.060502	68921.320567	33.797568
911.771065	69034.094265	33.802586
913.444766	69147.062844	33.807604
914.358396	69250.151770	33.812621
915.020814	69360.944870	33.817639
915.976058	69469.145859	33.822656
916.778557	69578.957570	33.827674
917.403595	69694.989818	33.832692
918.662528	69807.712302	33.837709
919.458008	69917.034209	33.842727
920.496279	70024.631145	33.847744
921.368942	70149.604774	33.852762
922.657363	70247.445747	33.857780
923.361454	70350.308423	33.862797
924.546621	70454.699937	33.867815
925.798005	70561.002239	33.872832
926.732965	70654.838795	33.877850
927.292313	70771.355396	33.882868
928.623554	70869.464338	33.887885
929.081727	70970.770816	33.892903
930.444708	71075.958726	33.897920
931.004120	71163.905439	33.902938
931.731999	71258.681361	33.907956
932.788075	71353.708810	33.912973
933.288344	71451.978135	33.917991
934.310139	71560.552817	33.923008
935.288305	71650.362249	33.928026
936.107180	71760.960697	33.933044
936.701898	71860.512354	33.938061
937.343589	71975.019892	33.943079
938.614862	72088.562242	33.948096
939.527372	72194.876692	33.953114
940.365460	72321.019568	33.958132
941.549525	72426.710714	33.963149
942.070410	72542.750963	33.968167
943.410991	72644.917664	33.973184
944.555830	72756.796776	33.978202
945.474841	72879.353745	33.983220
946.485986	72976.336058	33.988237
946.993415	73100.406941	33.993255
947.930231	73204.068872	33.998272
948.855949	73339.430230	34.003290
950.047881	73448.196675	34.008308
951.563937	73555.414474	34.013325
952.193310	73677.554792	34.018343
953.182434	73783.821283	34.023360
954.323139	73913.256365	34.028378
955.298609	74016.688857	34.033396
956.399609	74129.473664	34.038413
957.370966	74233.584111	34.043431
958.302857	74343.591172	34.048448
960.138177	74428.903632	34.053466
961.524878	74535.850241	34.058484
962.862952	74608.047287	34.063501
963.563042	74712.993328	34.068519
964.305518	74806.399772	34.073536
965.257804	74897.359145	34.078554
965.838898	74989.888398	34.083572
966.997559	75087.337754	34.088589
967.657615	75189.764742	34.093607
968.469506	75289.589607	34.098624
969.227698	75393.935883	34.103642
969.662718	75512.598099	34.108660
970.872106	75618.150367	34.113677
971.788089	75734.443233	34.118695
972.749874	75845.806205	34.123712
974.076167	75957.724841	34.128730
974.820720	76067.916468	34.133748
975.766144	76183.651063	34.138765
976.386885	76304.816408	34.143783
977.295160	76412.398922	34.148800
978.155009	76536.965783	34.153818
978.631508	76663.490468	34.158836
979.665938	76791.305001	34.163853
980.529218	76926.194730	34.168871
981.351101	77045.101404	34.173888
982.151650	77157.293580	34.178906
982.746566	77295.325439	34.183924
984.021086	77418.295850	34.188941
984.713286	77554.601133	34.193959
985.623225	77691.991426	34.198976
986.833767	77820.207862	34.203994
987.562119	77953.830117	34.209012
988.502443	78084.265497	34.214029
989.547611	78228.792896	34.219047
990.054702	78368.546236	34.224064
991.106984	78512.233835	34.229082
992.110053	78677.193659	34.234100
993.254374	78812.866499	34.239117
994.294837	78953.430210	34.244135
995.404408	79099.634859	34.249152
996.455029	79248.390982	34.254170
997.089967	79400.286355	34.259188
998.697547	79535.833370	34.264205
999.643580	79691.227548	34.269223
1000.487282	79831.209064	34.274240
1001.931142	79975.603116	34.279258
1002.818888	80134.423378	34.284276
1003.961021	80269.846967	34.289293
1005.022789	80398.109441	34.294311
1006.324970	80545.235559	34.299328
1007.578969	80686.655764	34.304346
1008.255537	80827.024591	34.309364
1009.470164	80960.557340	34.314381
1010.738851	81097.129360	34.319399
1011.885338	81237.849753	34.324416
1013.018860	81359.791419	34.329434
1013.924527	81510.186211	34.334452
1015.074361	81629.762534	34.339469
1015.871538	81775.308732	34.344487
1017.019307	81899.900128	34.349504
1018.056084	82039.543375	34.354522
1019.068955	82171.402736	34.359540
1019.837479	82302.125909	34.364557
1020.852244	82442.919624	34.369575
1022.125098	82585.759507	34.374592
1023.032779	82715.849883	34.379610
1024.493146	82860.438317	34.384628
1025.288854	82979.787861	34.389645
1026.292872	83131.354566	34.394663
1027.463187	83257.897686	34.399680
1029.602514	83364.650387	34.404698
1030.540597	83486.584941	34.409716
1031.921211	83585.973819	34.414733
1032.824374	83711.860382	34.419751
1033.640258	83828.006068	34.424768
1034.488576	83934.081874	34.429786
1035.643819	84055.055768	34.434804
1036.646028	84166.709995	34.439821
1038.025811	84277.381659	34.444839
1039.443678	84381.839057	34.449856
1040.397739	84463.558727	34.454874
1040.795712	84569.329994	34.459892
1041.941830	84662.052907	34.464909
1043.051625	84761.458781	34.469927
1043.552650	84879.152473	34.474944
1044.952783	84986.391357	34.479962
1045.256158	85094.753655	34.484980
1045.682246	85213.143978	34.489997
1046.734626	85343.783919	34.495015
1048.073504	85460.171499	34.500032
1049.170415	85580.423587	34.505050
1050.316007	85716.849135	34.510068
1051.236451	85834.746959	34.515085
1052.124498	85961.433318	34.520103
1053.102086	86093.853884	34.525120
1054.190010	86231.512250	34.530138
1055.474024	86361.071933	34.535156
1056.231615	86490.735101	34.540173
1057.248907	86620.104816	34.545191
1058.203458	86758.344228	34.550208
1059.234792	86886.309542	34.555226
1060.177732	87045.887594	34.560244
1061.386133	87176.615085	34.565261
1062.374511	87316.990026	34.570279
1062.948940	87458.177895	34.575296
1063.982329	87609.759156	34.580314
1065.044320	87761.431787	34.585332
1066.245842	87910.098535	34.590349
1067.644601	88063.224748	34.595367
1068.678417	88207.398786	34.600384
1070.527935	88336.279666	34.605402
1071.255357	88487.612209	34.610420
1072.387199	88630.926086	34.615437
1073.328140	88767.024101	34.620455
1073.876780	88905.816116	34.625472
1075.388395	89054.928346	34.630490
1076.596773	89210.730043	34.635508
1077.644493	89351.943513	34.640525
1078.826327	89507.681993	34.645543
1079.690720	89636.404751	34.650560
1081.356246	89766.423790	34.655578
1082.443467	89926.006433	34.660596
1083.315597	90047.387965	34.665613
1084.784757	90192.150998	34.670631
1085.737341	90342.391810	34.675648
1087.041989	90470.967249	34.680666
1088.357441	90612.968462	34.685684
1089.064795	90741.532970	34.690701
1090.175139	90884.795509	34.695719
1091.726915	91011.203459	34.700736
1093.027148	91139.739251	34.705754
1093.771151	91261.824615	34.710772
1095.134700	91393.716514	34.715789
1096.701830	91501.916205	34.720807
1097.408896	91630.372112	34.725824
1098.583553	91738.964273	34.730842
1099.522902	91865.999491	34.735860
1100.343939	91973.169046	34.740877
1101.486504	92099.407986	34.745895
1101.967718	92222.697909	34.750912
1103.087176	92353.571788	34.755930
1103.967981	92475.686384	34.760948
1104.860236	92624.510271	34.765965
1106.051283	92754.907087	34.770983
1106.621727	92891.304657	34.776000
1107.874982	93036.664683	34.781018
1108.777806	93183.169317	34.786036
1109.398026	93340.953409	34.791053
1110.763313	93495.293050	34.796071
1111.372615	93657.850355	34.801088
1112.795263	93801.626090	34.806106
1114.193738	93970.885202	34.811124
1115.275400	94136.242589	34.816141
1116.651049	94279.946649	34.821159
1117.938987	94429.997413	34.826176
1119.379972	94570.302476	34.831194
1120.432333	94728.008660	34.836212
1121.848717	94871.507620	34.841229
1123.345844	95013.685243	34.846247
1124.507009	95169.156912	34.851264
1125.867226	95297.928619	34.856282
1126.932613	95442.809129	34.861300
1127.862635	95578.109486	34.866317
1129.170522	95709.902968	34.871335
1130.413199	95855.510715	34.876352
1131.778833	95985.481089	34.881370
1132.912619	96134.777001	34.886388
1134.153659	96258.721119	34.891405
1135.082634	96391.970563	34.896423
1135.896538	96543.205203	34.901440
1137.223892	96682.864606	34.906458
1138.312975	96824.264501	34.911476
1139.366255	96957.870746	34.916493
1140.901988	97103.933366	34.921511
1141.921612	97242.645600	34.926528
1142.782082	97376.145786	34.931546
1143.838771	97535.673874	34.936564
1144.807554	97681.330572	34.941581
1146.254881	97821.192986	34.946599
1147.059054	97972.394385	34.951616
1148.632123	98111.061853	34.956634
1150.123734	98251.539862	34.961652
1151.032204	98389.359388	34.966669
1152.342529	98533.347591	34.971687
1153.747584	98667.882216	34.976704
1154.677173	98805.397204	34.981722
1155.862874	98937.804553	34.986740
1156.813545	99086.225209	34.991757
1158.177843	99218.042687	34.996775
1159.184306	99362.021137	35.001792
1160.452082	99477.513130	35.006810
1161.622604	99605.073993	35.011828
1162.443761	99732.564576	35.016845
1163.444158	99862.823902	35.021863
1164.499825	99992.524721	35.026880
1165.228416	100134.299743	35.031898
1166.317138	100271.665304	35.036916
1167.199140	100416.878600	35.041933
1168.820065	100570.320895	35.046951
1169.546117	100723.431956	35.051968
1170.798596	100867.848876	35.056986
1171.853232	101015.347926	35.062004
1172.568337	101182.592680	35.067021
1174.057973	101340.781162	35.072039
1175.269661	101496.173885	35.077056
1176.196518	101665.394236	35.082074
1177.513694	101826.726570	35.087092
1178.436155	101998.291224	35.092109
1179.480839	102156.005479	35.097127
1180.903420	102325.290988	35.102144
1182.185478	102487.766118	35.107162
1183.524991	102653.219946	35.112180
1184.302141	102833.963776	35.117197
1185.860616	103006.016829	35.122215
1186.952208	103170.355715	35.127232
1187.704040	103350.386152	35.132250
1189.033213	103522.289595	35.137268
1190.418828	103703.057245	35.142285
1192.037672	103861.982567	35.147303
1193.509849	104033.329103	35.152320
1194.526294	104196.782154	35.157338
1196.492808	104350.510665	35.162356
1197.583423	104511.511398	35.167373
1199.176339	104670.129852	35.172391
1200.140144	104825.875067	35.177408
1201.317560	104992.617730	35.182426
1202.488074	105141.275980	35.187444
1203.581888	105318.001501	35.192461
1205.061640	105471.251420	35.197479
1206.065025	105621.116338	35.202496
1207.107003	105786.405198	35.207514
1208.233853	105947.289621	35.212532
1209.363050	106125.122994	35.217549
1210.738289	106280.989483	35.222567
1211.910706	106449.875887	35.227584
1212.990338	106617.177038	35.232602
1214.462618	106771.987028	35.237620
1215.303160	106940.828382	35.242637
1216.906225	107121.675966	35.247655
1217.996360	107279.341044	35.252672
1219.084751	107452.703453	35.257690
1220.115068	107614.101704	35.262708
1221.491040	107785.806862	35.267725
1222.979639	107948.337015	35.272743
1223.927245	108101.599688	35.277760
1225.131958	108255.904756	35.282778
1226.578357	108402.336715	35.287796
1227.419585	108559.093968	35.292813
1228.849963	108703.137798	35.297831
1230.032451	108875.045983	35.302848
1231.650907	109009.890406	35.307866
1233.908244	109143.045305	35.312884
1235.290330	109272.187919	35.317901
1236.322268	109412.710452	35.322919
1237.537876	109556.280773	35.327936
1238.573760	109695.823218	35.332954
1239.968625	109837.353868	35.337972
1240.736502	109976.839245	35.342989
1242.155175	110117.734759	35.348007
1243.464937	110268.408905	35.353024
1244.572956	110419.837647	35.358042
1245.702047	110556.122969	35.363060
1246.619796	110708.317996	35.368077
1248.004044	110871.042427	35.373095
1248.804368	111025.416583	35.378112
1250.000279	111200.883708	35.383130
1251.212346	111356.238923	35.388148
1252.341985	111529.053959	35.393165
1253.722323	111694.075922	35.398183
1254.801075	111870.737492	35.403200
1256.025204	112033.976116	35.408218
1257.589587	112202.814650	35.413236
1258.706198	112377.448115	35.418253
1260.007359	112567.512202	35.423271
1260.902837	112728.775579	35.428288
1262.140769	112914.053912	35.433306
1263.491276	113086.553445	35.438324
1264.388793	113265.266799	35.443341
1265.990505	113434.234337	35.448359
1267.428291	113629.849355	35.453376
1268.429480	113812.411808	35.458394
1269.830104	113997.912851	35.463412
1271.074128	114172.861444	35.468429
1272.020274	114363.084204	35.473447
1273.136057	114550.983328	35.478464
1274.493445	114736.230778	35.483482
1276.370648	114907.304257	35.488500
1277.298482	115101.112466	35.493517
1279.198158	115277.958747	35.498535
1280.680373	115461.165723	35.503552
1281.844488	115642.430280	35.508570
1283.729985	115816.015700	35.513588
1285.273907	115966.693284	35.518605
1286.696619	116133.934589	35.523623
1288.159452	116303.779107	35.528640
1289.255870	116467.199710	35.533658
1290.471549	116623.270666	35.538676
1291.868486	116789.273078	35.543693
1293.213743	116956.563734	35.548711
1294.653703	117092.841430	35.553728
1295.552738	117242.280434	35.558746
1296.776852	117389.395603	35.563764
1297.948858	117538.438371	35.568781
1299.105103	117679.069763	35.573799
1300.142731	117843.489876	35.578816
1301.284220	118010.237262	35.583834
1303.090283	118145.563237	35.588852
1304.074220	118309.368008	35.593869
1305.353993	118476.666283	35.598887
1306.550855	118622.969679	35.603904
1307.782827	118801.839642	35.608922
1309.241842	118962.938953	35.613940
1310.431381	119121.637951	35.618957
1311.417777	119302.317017	35.623975
1312.352525	119477.376330	35.628992
1313.602003	119653.425259	35.634010
1315.138422	119838.408770	35.639028
1315.982267	120022.617164	35.644045
1317.392707	120205.267713	35.649063
1318.567541	120408.119015	35.654080
1319.714765	120595.031427	35.659098
1321.364050	120781.878033	35.664116
1322.788673	120974.828149	35.669133
1323.795461	121173.861948	35.674151
1324.987541	121367.459817	35.679168
1326.161866	121567.470494	35.684186
1327.723878	121771.714583	35.689204
1329.001107	121983.022116	35.694221
1330.299728	122190.528298	35.699239
1331.883144	122382.931500	35.704256
1333.172145	122584.552812	35.709274
1334.649643	122795.176360	35.714292
1335.935038	122996.712703	35.719309
1337.633079	123197.653013	35.724327
1338.964309	123400.641701	35.729344
1340.339171	123600.319136	35.734362
1341.783600	123787.219462	35.739380
1343.779000	123979.024043	35.744397
1345.167245	124163.478658	35.749415
1347.237323	124338.554316	35.754432
1348.579378	124512.872830	35.759450
1350.618339	124680.482397	35.764468
1352.050554	124852.508785	35.769485
1353.781228	125008.072683	35.774503
1355.539833	125164.861722	35.779520
1356.470682	125333.310132	35.784538
1358.277885	125476.818313	35.789556
1359.572631	125636.597216	35.794573
1360.530862	125791.579022	35.799591
1361.966150	125945.447182	35.804608
1363.004204	126096.377197	35.809626
1364.964889	126247.427431	35.814644
1366.457751	126405.519939	35.819661
1367.721011	126542.267114	35.824679
1368.813608	126682.120314	35.829696
1369.916776	126823.999368	35.834714
1371.257117	126947.828016	35.839732
1372.180586	127107.129828	35.844749
1373.425960	127246.822285	35.849767
1374.708470	127386.838917	35.854784
1375.734572	127549.826008	35.859802
1376.963251	127709.272824	35.864820
1378.139186	127872.187338	35.869837
1378.945180	128036.111720	35.874855
1380.488628	128201.744106	35.879872
1381.638465	128388.089429	35.884890
1383.309503	128551.942737	35.889908
1384.521624	128729.754617	35.894925
1385.607009	128916.823172	35.899943
1387.343351	129098.075969	35.904960
1388.379301	129289.829628	35.909978
1389.513065	129472.042095	35.914996
1390.958126	129658.868445	35.920013
1392.133081	129859.535518	35.925031
1393.707703	130056.529824	35.930048
1394.869650	130256.428994	35.935066
1396.004767	130458.449622	35.940084
1397.140929	130665.741995	35.945101
1398.778641	130886.005748	35.950119
1400.237079	131092.527889	35.955136
1401.170839	131309.333997	35.960154
1402.771819	131525.642975	35.965172
1403.946961	131743.617679	35.970189
1405.117115	131977.875748	35.975207
1406.432612	132189.673972	35.980224
1407.630814	132438.058490	35.985242
1409.340223	132664.951178	35.990260
1410.573881	132892.618141	35.995277
1411.774924	133135.522007	36.000295
1413.465162	133368.543166	36.005312
1414.800398	133610.897572	36.010330
1416.221967	133847.462422	36.015348
1418.006763	134076.609709	36.020365
1419.743463	134311.506421	36.025383
1421.178623	134537.519839	36.030400
1422.638326	134791.052963	36.035418
1424.030936	135009.448763	36.040436
1425.733396	135237.896073	36.045453
1427.208625	135468.611470	36.050471
1429.018714	135694.510966	36.055488
1430.109489	135923.174894	36.060506
1431.688800	136138.698367	36.065524
1433.366855	136365.726481	36.070541
1435.060207	136593.248130	36.075559
1436.637203	136803.670053	36.080576
1437.927056	137038.685105	36.085594
1439.558575	137242.435939	36.090612
1441.057193	137466.586447	36.095629
1442.262216	137672.220163	36.100647
1443.831354	137879.140742	36.105664
1445.486950	138071.412150	36.110682
1446.903294	138271.047643	36.115700
1448.397285	138468.758548	36.120717
1449.539730	138676.639578	36.125735
1451.410125	138858.946419	36.130752
1452.421054	139071.438706	36.135770
1454.018273	139264.626883	36.140788
1455.530940	139467.765538	36.145805
1456.535938	139682.455567	36.150823
1457.962360	139888.791774	36.155840
1459.580815	140087.862332	36.160858
1460.537389	140306.303180	36.165876
1461.959931	140524.189973	36.170893
1463.269564	140738.370196	36.175911
1464.747005	140966.441144	36.180928
1465.958101	141190.614532	36.185946
1467.303890	141430.331881	36.190964
1468.845677	141653.683024	36.195981
1470.013063	141889.401959	36.200999
1471.568848	142122.082537	36.206016
1473.143205	142360.871002	36.211034
1474.743203	142599.416439	36.216052
1476.481096	142831.883355	36.221069
1478.036316	143072.391469	36.226087
1479.894628	143299.798253	36.231104
1481.485924	143528.643375	36.236122
1483.160628	143759.314813	36.241140
1485.073578	143972.496529	36.246157
1486.565609	144209.360428	36.251175
1488.147123	144416.450390	36.256192
1489.758545	144629.900002	36.261210
1491.326785	144855.919293	36.266228
1492.842769	145063.454929	36.271245
1494.605186	145282.804485	36.276263
1496.279768	145498.379497	36.281280
1497.863463	145717.912599	36.286298
1499.230927	145929.698599	36.291316
1500.854866	146139.962191	36.296333
1501.979367	146350.914979	36.301351
1503.567743	146569.692706	36.306368
1505.179799	146785.603359	36.311386
1506.519813	147010.482818	36.316404
1507.891876	147225.407809	36.321421
1509.263546	147449.043053	36.326439
1510.593904	147666.842531	36.331456
1511.956856	147900.623577	36.336474
1513.299688	148122.594798	36.341492
1514.975537	148355.936481	36.346509
1516.311750	148588.611229	36.351527
1517.943680	148812.632986	36.356544
1519.564144	149041.614870	36.361562
1521.074661	149272.910417	36.366580
1522.875992	149490.558692	36.371597
1524.713648	149712.956673	36.376615
1526.481570	149919.064051	36.381632
1527.514425	150114.272737	36.386650
1529.050412	150322.688795	36.391668
1531.043971	150517.519084	36.396685
1532.309741	150711.553352	36.401703
1533.629953	150915.861845	36.406720
1535.341018	151116.813265	36.411738
1536.832374	151311.461823	36.416756
1539.023202	151513.835464	36.421773
1539.905203	151721.159888	36.426791
1541.635621	151928.401553	36.431808
1543.206084	152124.690517	36.436826
1544.148657	152351.711356	36.441844
1545.965990	152553.719635	36.446861
1547.403361	152774.959460	36.451879
1548.602109	153000.460645	36.456896
1550.053188	153209.694515	36.461914
1551.039642	153452.488208	36.466932
1552.828605	153667.757098	36.471949
1554.183847	153920.182268	36.476967
1555.468344	154148.466938	36.481984
1557.277658	154397.121271	36.487002
1558.173684	154640.685976	36.492020
1560.100660	154887.309226	36.497037
1561.492336	155126.994894	36.502055
1563.169722	155380.191284	36.507072
1565.071680	155632.466314	36.512090
1566.549791	155875.757219	36.517108
1568.513139	156114.167137	36.522125
1569.889557	156364.045806	36.527143
1572.126833	156606.511246	36.532160
1574.022627	156840.942754	36.537178
1575.444820	157081.334677	36.542196
1577.668640	157300.133297	36.547213
1579.567267	157528.533237	36.552231
1580.939099	157758.780934	36.557248
1583.060437	157981.695912	36.562266
1584.402046	158201.756236	36.567284
1586.108965	158417.537270	36.572301
1587.757520	158645.819423	36.577319
1589.264003	158863.980986	36.582336
1591.164511	159078.594080	36.587354
1592.550141	159295.610881	36.592372
1594.584089	159520.464380	36.597389
1596.075184	159726.574074	36.602407
1597.681427	159947.554402	36.607424
1598.725009	160157.973208	36.612442
1600.577512	160393.855748	36.617460
1602.163526	160608.211060	36.622477
1603.365041	160828.500270	36.627495
1605.039208	161041.373133	36.632512
1606.679012	161273.338627	36.637530
1608.111016	161510.043556	36.642548
1609.547499	161735.627369	36.647565
1611.038885	161962.129657	36.652583
1612.166270	162175.920420	36.657600
1613.737471	162396.135175	36.662618
1615.157232	162622.247155	36.667636
1616.856574	162840.820952	36.672653
1618.097557	163080.014183	36.677671
1619.319305	163301.659625	36.682688
1621.137982	163529.476743	36.687706
1622.547835	163778.831751	36.692724
1624.287045	164001.933847	36.697741
1625.388178	164254.448362	36.702759
1627.232724	164508.609451	36.707776
1628.843224	164752.422185	36.712794
1630.154379	165006.328975	36.717812
1632.164432	165257.120627	36.722829
1633.881329	165497.420848	36.727847
1635.198069	165769.735203	36.732864
1637.088229	166017.304117	36.737882
1638.428068	166282.706140	36.742900
1639.996857	166538.243980	36.747917
1641.689540	166821.008204	36.752935
1643.197715	167086.845782	36.757952
1645.069347	167355.202314	36.762970
1646.553881	167620.793726	36.767988
1648.814256	167881.456575	36.773005
1650.385262	168151.287082	36.778023
1652.163654	168414.059565	36.783040
1654.056363	168679.974066	36.788058
1655.609393	168940.388638	36.793076
1657.487016	169213.666121	36.798093
1658.927021	169472.199585	36.803111
1660.622903	169741.805810	36.808128
1662.293491	170003.667616	36.813146
1664.197222	170276.174701	36.818164
1666.187837	170534.843456	36.823181
1668.171350	170799.958980	36.828199
1669.649707	171046.065631	36.833216
1671.943658	171313.824554	36.838234
1673.550135	171559.660380	36.843252
1675.348672	171817.353292	36.848269
1676.929233	172054.544997	36.853287
1678.529782	172321.926151	36.858304
1680.401351	172564.415244	36.863322
1682.300722	172816.542410	36.868340
1683.991281	173067.296226	36.873357
1685.622356	173308.508729	36.878375
1687.277695	173574.684440	36.883392
1688.867638	173815.969954	36.888410
1690.246893	174069.291262	36.893428
1691.988954	174326.933224	36.898445
1693.947736	174575.941241	36.903463
1695.525688	174834.906472	36.908480
1697.149818	175094.982410	36.913498
1698.509366	175361.483245	36.918516
1700.459783	175598.396075	36.923533
1702.009203	175860.835730	36.928551
1703.458609	176101.586219	36.933568
1705.466495	176348.770371	36.938586
1706.798550	176587.893067	36.943604
1708.223652	176816.941746	36.948621
1709.607078	177071.143661	36.953639
1711.325760	177325.991677	36.958656
1712.898904	177576.385841	36.963674
1714.774503	177830.400049	36.968692
1716.705357	178083.011433	36.973709
1718.625008	178331.452011	36.978727
1720.601547	178588.487024	36.983744
1722.316796	178825.709313	36.988762
1724.019987	179078.121740	36.993780
1726.048229	179337.360706	36.998797
1727.978524	179575.504603	37.003815
1729.582631	179833.545164	37.008832
1731.123987	180070.129545	37.013850
1732.364755	180343.900251	37.018868
1734.517823	180598.115331	37.023885
1736.234899	180849.698590	37.028903
1737.682026	181111.984145	37.033920
1739.801669	181370.852903	37.038938
1741.520419	181644.949272	37.043956
1743.073502	181895.790637	37.048973
1744.759835	182172.318922	37.053991
1746.615428	182438.062267	37.059008
1748.156994	182703.336841	37.064026
1749.624398	182983.127858	37.069044
1751.361561	183253.856156	37.074061
1753.276932	183538.287052	37.079079
1755.101742	183835.283410	37.084096
1756.949051	184108.207267	37.089114
1758.723847	184395.026068	37.094132
1760.492849	184660.111214	37.099149
1762.208058	184950.001074	37.104167
1764.131068	185224.366235	37.109184
1765.844455	185500.885447	37.114202
1767.491281	185776.655541	37.119220
1769.194604	186059.143747	37.124237
1771.214003	186349.755584	37.129255
1772.615474	186633.856059	37.134272
1774.673339	186918.653527	37.139290
1776.554983	187209.229195	37.144308
1778.022674	187497.854708	37.149325
1780.112723	187777.056097	37.154343
1781.518636	188068.930880	37.159360
1783.913875	188352.274956	37.164378
1785.742859	188638.667442	37.169396
1787.408495	188921.902342	37.174413
1789.651837	189199.831501	37.179431
1791.399522	189480.442502	37.184448
1793.137466	189759.013533	37.189466
1795.257597	190032.944228	37.194484
1796.987153	190304.349603	37.199501
1799.369728	190557.441711	37.204519
1801.123364	190808.667921	37.209536
1802.969127	191048.827111	37.214554
1804.480027	191292.441800	37.219572
1806.089177	191538.161497	37.224589
1807.749052	191791.882398	37.229607
1809.255220	192047.748420	37.234624
1811.148137	192295.863552	37.239642
1812.544501	192559.732385	37.244660
1814.189997	192823.525004	37.249677
1815.895747	193085.253462	37.254695
1817.466486	193365.699163	37.259712
1819.190973	193645.893585	37.264730
1820.931295	193932.699354	37.269748
1822.395135	194212.405262	37.274765
1824.371447	194496.663837	37.279783
1825.447568	194803.087106	37.284800
1827.417118	195102.034517	37.289818
1829.176000	195400.826737	37.294836
1831.052707	195715.771591	37.299853
1832.904682	196017.078324	37.304871
1834.609405	196332.549231	37.309888
1836.853795	196642.643739	37.314906
1838.441118	196962.020918	37.319924
1840.011807	197282.303844	37.324941
1842.162332	197595.020832	37.329959
1843.568627	197926.135041	37.334976
1845.585598	198246.022971	37.339994
1847.100745	198571.996115	37.345012
1849.058710	198910.251016	37.350029
1851.351238	199230.177257	37.355047
1853.094351	199565.881044	37.360064
1854.827503	199896.752461	37.365082
1856.702634	200232.172861	37.370100
1858.619872	200571.853535	37.375117
1860.631381	200895.413644	37.380135
1862.343869	201234.051980	37.385152
1864.426330	201565.017637	37.390170
1866.712317	201901.538080	37.395188
1868.508814	202235.954953	37.400205
1870.248386	202569.925882	37.405223
1872.220980	202905.943567	37.410240
1874.448342	203234.788919	37.415258
1876.880840	203569.277754	37.420276
1878.067375	203897.022732	37.425293
1880.463670	204209.090929	37.430311
1882.213253	204556.870242	37.435328
1884.157944	204870.562356	37.440346
1886.180863	205197.458388	37.445364
1887.938067	205536.940342	37.450381
1889.886054	205848.276039	37.455399
1892.129093	206173.213023	37.460416
1894.262725	206480.485764	37.465434
1896.678167	206805.843149	37.470452
1898.711251	207113.287436	37.475469
1900.819313	207411.416211	37.480487
1902.773445	207692.534575	37.485504
1904.616035	207972.300908	37.490522
1906.384718	208240.502568	37.495540
1907.849650	208536.403073	37.500557
1909.616096	208813.684441	37.505575
1911.400533	209111.809399	37.510592
1913.007661	209401.470927	37.515610
1914.995178	209691.606630	37.520628
1916.423676	209997.929889	37.525645
1918.876302	210276.353000	37.530663
1920.580975	210581.302266	37.535680
1922.380989	210892.280860	37.540698
1924.744797	211183.722109	37.545716
1926.353711	211490.303236	37.550733
1928.653420	211789.704782	37.555751
1930.356648	212098.305119	37.560768
1932.485173	212395.603768	37.565786
1934.387825	212704.924375	37.570804
1936.188394	212998.519872	37.575821
1938.906672	213297.709566	37.580839
1940.884841	213600.776043	37.585856
1943.092230	213907.476655	37.590874
1944.947434	214210.895509	37.595892
1946.666861	214506.541893	37.600909
1948.377366	214813.871417	37.605927
1949.760654	215131.246147	37.610944
1951.458539	215454.019117	37.615962
1953.428846	215772.433633	37.620980
1954.728820	216118.100804	37.625997
1956.882829	216447.370055	37.631015
1959.035238	216787.864805	37.636032
1960.588009	217135.261702	37.641050
1962.717301	217469.669071	37.646068
1964.277329	217813.640054	37.651085
1966.192680	218164.437937	37.656103
1967.717884	218525.025176	37.661120
1969.949588	218876.817458	37.666138
1971.915649	219238.976180	37.671156
1973.812681	219613.971592	37.676173
1975.677407	219966.144748	37.681191
1977.488925	220362.133027	37.686208
1979.314696	220767.174222	37.691226
1981.472681	221137.310949	37.696244
1983.054701	221517.051144	37.701261
1984.990892	221889.829661	37.706279
1987.405334	222258.788358	37.711296
1990.179409	222635.678467	37.716314
1992.689930	222986.010857	37.721332
1995.118769	223346.503150	37.726349
1997.442243	223693.693959	37.731367
1999.879432	224039.179443	37.736384
2001.690999	224391.317721	37.741402
2003.632424	224741.011645	37.746420
2005.473935	225089.097594	37.751437
2007.191339	225421.002157	37.756455
2009.395206	225746.748542	37.761472
2011.222955	226060.226097	37.766490
2013.553498	226379.059830	37.771508
2015.311530	226705.807644	37.776525
2017.523432	227017.729439	37.781543
2019.281173	227340.009981	37.786560
2021.044921	227658.227335	37.791578
2023.136740	227989.193704	37.796596
2024.808835	228328.913597	37.801613
2026.973536	228663.883639	37.806631
2028.389383	229004.586472	37.811648
2029.915099	229361.908217	37.816666
2031.917372	229709.454082	37.821684
2033.496387	230071.062293	37.826701
2035.270755	230445.364997	37.831719
2037.405427	230811.129326	37.836736
2039.318826	231199.178426	37.841754
2041.257320	231574.246969	37.846772
2043.179081	231959.097780	37.851789
2045.424565	232350.883191	37.856807
2047.659192	232737.312959	37.861824
2049.460776	233127.571874	37.866842
2051.989233	233504.459209	37.871860
2054.076395	233900.796836	37.876877
2056.107100	234284.623619	37.881895
2058.512326	234669.713170	37.886912
2060.388792	235065.504641	37.891930
2062.717479	235456.704946	37.896948
2064.814617	235855.715464	37.901965
2066.659552	236238.817058	37.906983
2068.849073	236644.825981	37.912000
2071.119613	237035.634994	37.917018
2073.594233	237410.411626	37.922036
2076.191774	237815.268066	37.927053
2078.028838	238196.193521	37.932071
2080.939106	238567.374486	37.937088
2082.726690	238952.755248	37.942106
2084.949845	239330.753161	37.947124
2087.244209	239709.680807	37.952141
2089.069745	240087.083875	37.957159
2091.222746	240463.420220	37.962176
2093.439347	240835.963093	37.967194
2095.961775	241200.254438	37.972212
2098.046381	241571.017122	37.977229
2100.170133	241955.033554	37.982247
2102.337250	242322.788200	37.987264
2104.085732	242701.024416	37.992282
2105.934621	243082.827272	37.997300
2108.290385	243456.854550	38.002317
2110.797117	243815.390088	38.007335
2113.520871	244188.395873	38.012352
2114.947219	244567.958634	38.017370
2117.275674	244930.487941	38.022388
2119.150255	245310.565897	38.027405
2121.239984	245661.679273	38.032423
2123.163631	246013.150083	38.037440
2125.033107	246357.340296	38.042458
2126.926465	246709.782862	38.047476
2128.705903	247061.685528	38.052493
2130.778926	247412.729637	38.057511
2132.974176	247775.592124	38.062528
2134.597903	248147.842975	38.067546
2136.525935	248521.138722	38.072564
2138.420557	248901.959460	38.077581
2140.369092	249279.927611	38.082599
2142.819295	249665.716944	38.087616
2144.465389	250064.945123	38.092634
2146.529580	250454.175938	38.097652
2148.517128	250852.030968	38.102669
2150.719669	251257.498742	38.107687
2153.219105	251652.810477	38.112704
2154.899792	252078.023878	38.117722
2157.483481	252472.765234	38.122740
2159.738512	252873.376608	38.127757
2161.774300	253289.163196	38.132775
2164.139410	253701.977233	38.137792
2165.977226	254123.893519	38.142810
2167.891692	254552.301500	38.147828
2170.344192	254970.489585	38.152845
2172.127712	255392.264721	38.157863
2174.890760	255818.533983	38.162880
2176.742551	256257.065526	38.167898
2179.121327	256674.023937	38.172916
2181.519252	257101.445892	38.177933
2183.610309	257544.158802	38.182951
2186.382847	257965.832773	38.187968
2188.229001	258400.050849	38.192986
2190.370110	258822.156658	38.198004
2192.705134	259263.284416	38.203021
2194.878100	259692.296117	38.208039
2197.581058	260122.824827	38.213056
2199.500076	260562.648927	38.218074
2201.873723	260986.194603	38.223092
2204.264092	261418.883266	38.228109
2206.439454	261850.844550	38.233127
2209.260205	262267.208296	38.238144
2211.455817	262691.775250	38.243162
2213.615990	263121.301943	38.248180
2215.936725	263551.616600	38.253197
2217.936906	263974.666518	38.258215
2220.226502	264403.488323	38.263232
2222.268657	264834.382083	38.268250
2224.443881	265257.049981	38.273268
2227.032900	265674.140197	38.278285
2229.187050	266105.093687	38.283303
2231.899409	266521.301411	38.288320
2233.689199	266946.292869	38.293338
2236.288279	267375.347887	38.298356
2238.397240	267801.813611	38.303373
2240.571638	268219.301912	38.308391
2242.929047	268619.258602	38.313408
2244.803524	269020.079610	38.318426
2247.208368	269401.484819	38.323444
2249.404022	269792.017785	38.328461
2251.448601	270195.606812	38.333479
2253.455687	270590.971278	38.338496
2255.633984	271001.093522	38.343514
2257.463992	271411.398161	38.348532
2259.560450	271823.591351	38.353549
2261.667870	272242.387810	38.358567
2264.018796	272670.951485	38.363584
2266.010189	273105.440446	38.368602
2268.270532	273529.928707	38.373620
2270.223931	273962.010502	38.378637
2272.184681	274403.033173	38.383655
2274.816584	274848.725296	38.388672
2276.859641	275300.988647	38.393690
2279.070172	275749.313294	38.398708
2281.340490	276209.771245	38.403725
2283.613551	276669.898444	38.408743
2286.207787	277117.958819	38.413760
2289.038140	277582.697078	38.418778
2291.450272	278040.795002	38.423796
2293.960745	278478.300436	38.428813
2296.043536	278929.718334	38.433831
2298.729110	279385.663872	38.438848
2301.198387	279838.239421	38.443866
2303.290271	280291.103177	38.448884
2305.798979	280737.295717	38.453901
2308.674107	281184.979479	38.458919
2310.902547	281640.259413	38.463936
2313.075392	282089.679663	38.468954
2315.604432	282540.440261	38.473972
2318.379923	282976.021095	38.478989
2320.541693	283433.037515	38.484007
2322.829227	283869.253772	38.489024
2325.345216	284318.185764	38.494042
2327.610300	284755.370020	38.499060
2330.155259	285198.758600	38.504077
2332.480492	285649.522992	38.509095
2335.462038	286088.472014	38.514112
2337.892109	286523.951506	38.519130
2339.869624	286960.721534	38.524148
2342.335677	287396.930896	38.529165
2344.744214	287837.695904	38.534183
2347.236187	288258.582039	38.539200
2349.766713	288696.913211	38.544218
2352.108935	289131.285343	38.549236
2354.476169	289567.913691	38.554253
2356.940750	289999.292964	38.559271
2359.112286	290423.173408	38.564288
2361.259193	290861.257127	38.569306
2363.430655	291302.282896	38.574324
2365.546156	291734.832308	38.579341
2367.588240	292175.953214	38.584359
2369.841936	292596.539992	38.589376
2371.653356	293024.588194	38.594394
2373.859790	293442.361230	38.599412
2376.016467	293874.823873	38.604429
2378.018683	294308.351617	38.609447
2380.805429	294736.572068	38.614464
2382.925917	295188.978438	38.619482
2385.326944	295630.467236	38.624500
2387.464654	296084.469160	38.629517
2389.361482	296535.764778	38.634535
2391.704787	296995.371167	38.639552
2393.664229	297467.179314	38.644570
2396.159825	297931.737955	38.649588
2398.635819	298415.425943	38.654605
2400.941203	298900.816123	38.659623
2403.594201	299378.986587	38.664640
2406.062590	299874.432521	38.669658
2408.141297	300362.648514	38.674676
2410.803133	300843.963044	38.679693
2413.202653	301343.733556	38.684711
2416.205084	301827.988400	38.689728
2419.485302	302302.519863	38.694746
2422.263457	302787.188165	38.699764
2424.630947	303255.002948	38.704781
2427.053506	303735.330076	38.709799
2429.957567	304203.082105	38.714816
2432.198459	304672.436294	38.719834
2434.995045	305138.398734	38.724852
2437.856500	305601.428228	38.729869
2440.248780	306065.368670	38.734887
2442.820199	306529.329874	38.739904
2445.320879	307001.530275	38.744922
2447.744697	307460.533051	38.749940
2450.475890	307922.076230	38.754957
2452.424369	308405.738031	38.759975
2455.359347	308862.038391	38.764992
2457.945431	309319.941685	38.770010
2460.210990	309778.427391	38.775028
2462.623354	310238.945390	38.780045
2464.875437	310718.612694	38.785063
2467.234913	311184.189748	38.790080
2469.791376	311664.795370	38.795098
2471.695908	312132.167700	38.800116
2474.365525	312607.595259	38.805133
2476.610661	313098.759079	38.810151
2479.178679	313582.224452	38.815168
2481.703571	314073.441014	38.820186
2483.661384	314569.469232	38.825204
2486.310258	315050.400510	38.830221
2488.825641	315545.599076	38.835239
2491.002044	316044.150662	38.840256
2493.357683	316548.309688	38.845274
2495.612585	317063.479346	38.850292
2498.299001	317560.037546	38.855309
2500.714097	318053.334468	38.860327
2503.232144	318531.170843	38.865344
2505.873590	318997.683408	38.870362
2508.002343	319484.897376	38.875380
2510.803730	319948.763855	38.880397
2513.040391	320419.346032	38.885415
2515.833852	320897.278771	38.890432
2518.379165	321383.197402	38.895450
2520.636717	321856.206708	38.900468
2523.352212	322335.896312	38.905485
2525.502946	322826.034380	38.910503
2527.897279	323304.601201	38.915520
2530.562224	323799.045678	38.920538
2533.084621	324292.570160	38.925556
2535.721258	324782.416616	38.930573
2538.735832	325282.358445	38.935591
2541.104460	325773.307998	38.940608
2543.509134	326266.788344	38.945626
2546.207623	326778.046361	38.950644
2548.575709	327277.570189	38.955661
2550.772934	327792.684812	38.960679
2553.380854	328312.835216	38.965696
2555.753269	328820.449190	38.970714
2558.387970	329340.334363	38.975732
2561.244253	329855.152811	38.980749
2563.926449	330379.162422	38.985767
2566.499061	330903.693526	38.990784
2569.180343	331431.149266	38.995802
2572.104856	331955.896320	39.000820
2575.170810	332459.667835	39.005837
2577.920543	332977.807442	39.010855
2580.803288	333487.110884	39.015872
2583.656159	333980.925898	39.020890
2586.355813	334495.557958	39.025908
2589.156191	334989.424814	39.030925
2592.019751	335491.809756	39.035943
2594.461652	336000.097842	39.040960
2597.092426	336497.738459	39.045978
2599.433716	337005.526952	39.050996
2602.083190	337501.354233	39.056013
2604.582665	338011.826698	39.061031
2607.002930	338523.170957	39.066048
2609.763452	339038.621285	39.071066
2612.166038	339547.421071	39.076084
2614.422716	340072.794239	39.081101
2616.879871	340600.721006	39.086119
2619.356168	341128.589464	39.091136
2621.994589	341638.071098	39.096154
2624.452937	342179.491335	39.101172
2626.935033	342710.112618	39.106189
2629.583675	343255.199851	39.111207
2631.777051	343798.551620	39.116224
2634.620392	344342.531702	39.121242
2636.978679	344891.610416	39.126260
2639.625909	345436.042973	39.131277
2642.539232	345959.635766	39.136295
2645.052061	346481.306991	39.141312
2647.734422	346999.773180	39.146330
2650.062520	347518.417656	39.151348
2652.725779	348025.199423	39.156365
2655.220134	348552.591768	39.161383
2657.502770	349072.549061	39.166400
2660.660689	349593.429007	39.171418
2663.527443	350105.490461	39.176436
2666.203269	350639.510394	39.181453
2669.187301	351158.016584	39.186471
2671.764175	351677.673779	39.191488
2674.275884	352208.886269	39.196506
2677.017799	352739.193866	39.201524
2679.425444	353275.057407	39.206541
2682.061005	353822.911327	39.211559
2684.223273	354368.448318	39.216576
2686.907951	354923.669383	39.221594
2689.436253	355490.509251	39.226612
2692.150114	356039.367686	39.231629
2694.681164	356614.773866	39.236647
2697.429886	357178.183870	39.241664
2700.342642	357746.206385	39.246682
2702.778052	358329.273129	39.251700
2706.145928	358897.413262	39.256717
2708.928699	359459.243356	39.261735
2711.572374	360039.134667	39.266752
2714.699625	360606.734348	39.271770
2717.251133	361191.448522	39.276788
2719.864342	361780.104934	39.281805
2722.760430	362359.141064	39.286823
2725.322562	362936.192535	39.291840
2728.211620	363521.686966	39.296858
2730.501311	364123.561892	39.301876
2732.845273	364706.716517	39.306893
2735.877497	365309.853955	39.311911
2738.267892	365921.434167	39.316928
2741.368945	366519.113647	39.321946
2744.503456	367118.353151	39.326964
2747.110537	367718.480084	39.331981
2749.812766	368323.405209	39.336999
2752.585146	368934.578653	39.342016
2755.456374	369534.283474	39.347034
2758.607767	370139.289716	39.352052
2761.608702	370732.410451	39.357069
2765.141867	371329.650775	39.362087
2767.389170	371924.624966	39.367104
2770.699707	372519.549230	39.372122
2773.327926	373103.611761	39.377140
2776.507838	373690.623459	39.382157
2779.643728	374269.692131	39.387175
2782.185823	374850.089870	39.392192
2784.945891	375439.604068	39.397210
2787.320159	376022.498054	39.402228
2790.248297	376604.484020	39.407245
2793.782772	377163.303473	39.412263
2796.174230	377712.883615	39.417280
2799.053339	378246.319645	39.422298
2802.134514	378778.473333	39.427316
2804.593679	379309.931816	39.432333
2808.083076	379841.524362	39.437351
2810.258986	380370.603120	39.442368
2813.170046	380909.553359	39.447386
2815.447822	381447.835247	39.452404
2817.956550	381993.860844	39.457421
2820.402336	382547.346530	39.462439
2822.561218	383117.662406	39.467456
2825.420426	383688.492914	39.472474
2827.738908	384275.457051	39.477492
2830.504353	384861.580187	39.482509
2832.891598	385458.280501	39.487527
2835.293112	386065.495293	39.492544
2838.586444	386679.889140	39.497562
2840.915126	387302.719351	39.502580
2843.627166	387924.970876	39.507597
2846.508427	388545.510880	39.512615
2849.146559	389187.535430	39.517632
2852.096338	389840.252631	39.522650
2854.669880	390485.408823	39.527668
2857.231604	391136.616394	39.532685
2860.283131	391807.109940	39.537703
2862.657077	392467.655141	39.542720
2865.835997	393144.645605	39.547738
2868.516461	393820.027924	39.552756
2871.474738	394497.711286	39.557773
2874.679327	395173.896717	39.562791
2877.440970	395861.777949	39.567808
2880.538042	396542.035536	39.572826
2883.460212	397218.300590	39.577844
2886.693521	397909.944560	39.582861
2889.835110	398596.694917	39.587879
2893.075200	399276.442652	39.592896
2896.121522	399951.212048	39.597914
2899.673962	400632.124424	39.602932
2902.614106	401303.890665	39.607949
2905.897578	401966.233244	39.612967
2908.859292	402636.370898	39.617984
2912.072509	403312.970075	39.623002
2915.077268	403970.954464	39.628020
2917.667437	404637.711428	39.633037
2920.659145	405298.078391	39.638055
2923.553559	405971.375163	39.643072
2926.328655	406630.581988	39.648090
2929.427911	407308.227982	39.653108
2931.934250	407985.496577	39.658125
2935.135648	408642.590171	39.663143
2938.010250	409321.291607	39.668160
2941.037631	409993.819761	39.673178
2943.945308	410667.923256	39.678196
2946.880646	411333.567173	39.683213
2949.924270	411994.414241	39.688231
2952.377170	412641.983643	39.693248
2955.678593	413272.931133	39.698266
2958.250286	413906.160048	39.703284
2961.304124	414549.461297	39.708301
2964.326300	415179.195333	39.713319
2967.213781	415814.309368	39.718336
2970.259090	416450.119302	39.723354
2973.000531	417095.313806	39.728372
2975.737776	417736.896139	39.733389
2978.636700	418388.447373	39.738407
2981.221719	419055.743193	39.743424
2983.950405	419714.993653	39.748442
2986.850571	420383.221570	39.753460
2989.724834	421063.117821	39.758477
2992.946106	421730.857158	39.763495
2996.015013	422413.729775	39.768512
2999.098942	423102.283404	39.773530
3002.214670	423774.246069	39.778548
3005.103363	424468.724347	39.783565
3008.079303	425165.805657	39.788583
3010.655944	425880.158112	39.793600
3013.579217	426574.804703	39.798618
3016.977549	427287.444381	39.803636
3019.166297	428008.235408	39.808653
3022.550191	428729.780225	39.813671
3025.283602	429459.513456	39.818688
3028.233202	430196.663985	39.823706
3031.324715	430932.302246	39.828724
3033.934412	431674.175635	39.833741
3037.210699	432417.771058	39.838759
3040.240589	433173.489448	39.843776
3043.131300	433925.535500	39.848794
3046.388576	434682.591430	39.853812
3049.391682	435459.113026	39.858829
3052.443938	436207.875132	39.863847
3055.485125	436987.382227	39.868864
3058.615637	437750.037965	39.873882
3061.806125	438523.320496	39.878900
3064.626701	439299.979517	39.883917
3067.833382	440072.907134	39.888935
3071.088103	440858.815965	39.893952
3074.282105	441628.557061	39.898970
3077.598730	442407.216173	39.903988
3081.045779	443181.728530	39.909005
3084.183475	443945.886060	39.914023
3087.371518	444720.794758	39.919040
3090.628796	445492.326048	39.924058
3093.785757	446256.659579	39.929076
3097.003056	447023.540547	39.934093
3100.854086	447792.067951	39.939111
3104.085520	448556.719890	39.944128
3106.950510	449306.725795	39.949146
3110.175540	450061.813258	39.954164
3113.475404	450813.877993	39.959181
3116.515557	451543.234418	39.964199
3119.554238	452268.012909	39.969216
3122.985104	452960.569689	39.974234
3126.445152	453665.752572	39.979252
3129.584647	454352.189437	39.984269
3132.387410	455046.249298	39.989287
3135.469196	455749.807463	39.994304
3138.677366	456437.131154	39.999322
3141.709504	457130.482820	40.004340
3144.593903	457844.935514	40.009357
3147.692892	458539.295044	40.014375
3150.340500	459270.638164	40.019392
3152.873124	459987.910245	40.024410
3156.058423	460720.688230	40.029428
3158.658136	461471.341665	40.034445
3161.788507	462220.165167	40.039463
3164.337237	462968.245304	40.044480
3167.076933	463752.841556	40.049498
3170.563079	464514.326599	40.054516
3173.264851	465320.065246	40.059533
3176.137393	466120.486121	40.064551
3179.118475	466929.862133	40.069568
3182.125237	467744.563851	40.074586
3185.354074	468554.394352	40.079604
3188.054044	469394.922865	40.084621
3191.450069	470232.778834	40.089639
3194.351711	471074.269259	40.094656
3197.368218	471927.134672	40.099674
3200.960778	472778.356608	40.104692
3203.505576	473649.730563	40.109709
3207.070024	474507.912469	40.114727
3210.606165	475375.111920	40.119744
3213.636663	476255.346262	40.124762
3217.142274	477138.853745	40.129780
3220.241483	478012.327096	40.134797
3223.679652	478877.924203	40.139815
3227.218848	479776.574216	40.144832
3230.297730	480656.049912	40.149850
3233.791196	481541.081077	40.154868
3237.108845	482418.418163	40.159885
3240.241188	483303.679022	40.164903
3244.008222	484188.900068	40.169920
3246.688516	485074.656540	40.174938
3250.771151	485957.421801	40.179956
3253.814076	486848.849599	40.184973
3256.969848	487745.977479	40.189991
3260.645160	488620.296573	40.195008
3263.986196	489518.877136	40.200026
3267.918957	490386.859567	40.205044
3270.912226	491270.357131	40.210061
3274.234090	492141.688458	40.215079
3277.936742	493015.141042	40.220096
3281.391748	493874.247421	40.225114
3285.092233	494746.911148	40.230132
3288.391997	495598.739153	40.235149
3291.685758	496443.407816	40.240167
3295.100669	497259.183811	40.245184
3298.384347	498069.591259	40.250202
3301.881930	498867.002174	40.255220
3304.973519	499674.489618	40.260237
3307.739469	500468.663085	40.265255
3311.171662	501281.678791	40.270272
3314.558461	502091.080098	40.275290
3317.818955	502880.675452	40.280308
3321.169850	503698.085946	40.285325
3324.641009	504520.790001	40.290343
3327.973495	505331.060504	40.295360
3331.081662	506143.196333	40.300378
3334.507715	506957.717006	40.305396
3337.950602	507781.583729	40.310413
3340.901843	508601.603022	40.315431
3344.444893	509436.779928	40.320448
3347.467158	510266.801030	40.325466
3350.923362	511091.263706	40.330484
3353.810782	511954.223471	40.335501
3356.881582	512798.795889	40.340519
3360.130697	513644.660035	40.345536
3362.932465	514529.851246	40.350554
3366.656080	515400.422661	40.355572
3369.778115	516280.224323	40.360589
3372.556256	517174.762244	40.365607
3376.098661	518076.444429	40.370624
3379.329736	518976.663984	40.375642
3382.667363	519881.255388	40.380660
3386.260694	520791.454861	40.385677
3389.354421	521714.339434	40.390695
3392.899240	522630.192359	40.395712
3396.471409	523555.266463	40.400730
3400.038922	524485.985395	40.405748
3403.014169	525427.683937	40.410765
3406.321974	526362.418582	40.415783
3409.452161	527277.618475	40.420800
3412.940635	528244.122514	40.425818
3416.801163	529196.295266	40.430836
3419.995282	530141.963929	40.435853
3423.219010	531099.414063	40.440871
3426.938743	532056.777574	40.445888
3430.101026	533022.081593	40.450906
3433.543459	533986.072006	40.455924
3436.785465	534948.623246	40.460941
3439.921439	535936.220567	40.465959
3443.723016	536916.898556	40.470976
3447.387981	537886.906277	40.475994
3451.713580	538838.362404	40.481012
3455.599290	539802.974309	40.486029
3458.960913	540762.067359	40.491047
3463.012661	541720.184431	40.496064
3466.353891	542683.035862	40.501082
3469.990413	543636.916121	40.506100
3473.541471	544600.466589	40.511117
3476.468760	545534.437415	40.516122
3480.133196	546425.055164	40.521127
3483.375244	547270.362757	40.526132
3486.574751	548039.370659	40.531136
3489.346165	548761.825739	40.536141
3491.888473	549425.592068	40.541146
3494.933779	550026.777262	40.546151
3497.139999	550572.362729	40.551156
3499.891459	551041.397660	40.556160
3502.379443	551453.745837	40.561165
3504.450764	551815.390044	40.566170
3506.083875	552136.781524	40.571175
3507.561807	552391.541594	40.576180
3509.338460	552594.939672	40.581184
3510.786314	552776.894284	40.586189
3512.050395	552898.787902	40.591194
3513.523787	552997.439848	40.596199
3514.340689	553059.365655	40.601204
3515.481971	553059.235743	40.606208
3515.763520	553066.506646	40.611213
3516.891289	553036.511841	40.616218
3517.832008	552975.468551	40.621223
3518.109193	552890.868072	40.626228
3518.848249	552789.242249	40.631232
3519.158035	552674.565935	40.636237
3519.455781	552542.030315	40.641242
3520.068095	552379.726732	40.646247
3519.891226	552208.464321	40.651252
3520.222223	552023.648227	40.656256
3520.396148	551834.868619	40.661261
3520.598583	551647.545261	40.666266
3520.703064	551429.708662	40.671271
3520.769002	551230.998251	40.676276
3521.044327	550994.357923	40.681280
3521.174543	550758.745843	40.686285
3521.010532	550518.281821	40.691290
3521.527326	550262.870755	40.696295
3521.095818	550028.042033	40.701300
3521.041827	549777.960656	40.706304
3521.173611	549514.321436	40.711309
3520.673042	549239.725691	40.716314
3521.045059	548995.922067	40.721319
3520.843108	548748.975252	40.726324
3520.601073	548481.692421	40.731328
3520.724760	548207.836548	40.736333
3520.194097	547959.212430	40.741338
3520.253036	547686.871108	40.746343
3519.980365	547435.926202	40.751348
3519.602523	547163.189951	40.756352
3519.386985	546918.788472	40.761357
3519.234843	546667.003825	40.766362
3519.379490	546416.177450	40.771367
3519.143041	546151.526422	40.776372
3518.739558	545897.698876	40.781376
3518.352861	545653.909175	40.786381
3517.791345	545420.390010	40.791386
3518.193452	545171.520900	40.796391
3518.099793	544922.019251	40.801396
3517.605179	544712.859770	40.806400
3517.582587	544473.485794	40.811405
3517.534007	544235.172178	40.816410
3517.441712	544001.657468	40.821415
3517.153962	543774.530849	40.826420
3516.717399	543537.277027	40.831424
3516.418890	543321.706004	40.836429
3516.317086	543102.920201	40.841434
3515.818799	542877.176282	40.846439
3515.905384	542684.556843	40.851444
3515.815730	542459.398361	40.856448
3515.711075	542254.434159	40.861453
3515.323021	542056.428918	40.866458
3515.334375	541864.113745	40.871463
3514.850146	541656.979818	40.876468
3514.985165	541447.977984	40.881472
3514.535705	541254.667519	40.886477
3514.429993	541067.460291	40.891482
3514.636834	540868.386010	40.896487
3514.221177	540690.362282	40.901492
3513.869890	540514.245050	40.906496
3513.731178	540327.639769	40.911501
3513.675956	540154.501227	40.916506
3513.411718	539959.226040	40.921511
3513.167009	539796.111523	40.926516
3513.200353	539613.863422	40.931520
3513.092352	539446.279784	40.936525
3512.426697	539287.013625	40.941530
3512.975553	539107.101864	40.946535
3512.429256	538962.054068	40.951540
3512.165936	538790.094284	40.956544
3511.916245	538648.784102	40.961549
3511.894859	538491.831782	40.966554
3511.802810	538342.514707	40.971559
3511.973859	538204.315479	40.976564
3511.466706	538045.566757	40.981568
3511.629599	537900.093725	40.986573
3511.230720	537769.505533	40.991578
3511.260693	537625.616486	40.996583
3511.249736	537482.944650	41.001588
3510.843804	537351.646935	41.006592
3510.785358	537219.182061	41.011597
3511.010655	537076.368078	41.016602
3510.840931	536946.898254	41.021607
3510.634465	536822.433269	41.026612
3510.411023	536686.959479	41.031616
3510.201657	536557.391610	41.036621
3510.244295	536437.379265	41.041626
3510.039144	536315.990917	41.046631
3509.750474	536215.070699	41.051636
3509.652443	536083.056822	41.056640
3509.461872	535968.078028	41.061645
3509.214718	535860.936291	41.066650
3509.728849	535739.631743	41.071655
3509.222592	535648.894676	41.076660
3509.376752	535536.282656	41.081664
3509.223245	535424.678145	41.086669
3508.916209	535325.623887	41.091674
3509.136193	535218.403842	41.096679
3509.582885	535114.733572	41.101684
3509.001650	535008.093298	41.106688
3508.816406	534915.129137	41.111693
3508.535942	534815.713810	41.116698
3508.569175	534716.601857	41.121703
3508.405227	534623.986168	41.126708
3508.299496	534532.775111	41.131712
3508.190448	534438.987815	41.136717
3508.070406	534352.677829	41.141722
3507.867637	534247.639457	41.146727
3507.769992	534195.473017	41.151732
3507.629437	534110.478309	41.156736
3507.799208	534026.141305	41.161741
3507.548070	533952.276615	41.166746
3507.600058	533861.794406	41.171751
3507.750011	533801.151321	41.176756
3507.268536	533732.727224	41.181760
3507.547472	533642.258382	41.186765
3507.342530	533566.161809	41.191770
3507.198931	533495.915169	41.196775
3506.946517	533430.636121	41.201780
3507.086131	533358.424434	41.206784
3507.264810	533302.068861	41.211789
3506.996906	533224.161916	41.216794
3507.165769	533153.864344	41.221799
3506.749326	533099.319714	41.226804
3506.930519	533019.522097	41.231808
3507.108410	532952.960580	41.236813
3506.886215	532889.392125	41.241818
3506.947017	532824.818814	41.246823
3506.695476	532764.235131	41.251828
3506.844654	532694.948987	41.256832
3506.811185	532628.823646	41.261837
3506.722022	532562.858386	41.266842
3506.499382	532497.116025	41.271847
3506.485007	532457.156532	41.276852
3506.538115	532385.560245	41.281856
3506.494723	532327.821653	41.286861
3506.236312	532289.365409	41.291866
3506.331051	532216.751343	41.296871
3506.209391	532162.662050	41.301876
3506.226962	532109.763086	41.306880
3506.505121	532063.845305	41.311885
3506.065229	532011.270916	41.316890
3506.256458	531955.211614	41.321895
3506.166045	531908.240136	41.326900
3505.979037	531845.823872	41.331904
3506.115502	531800.230845	41.336909
3506.170583	531745.910082	41.341914
3506.169271	531694.073675	41.346919
3506.195652	531644.607313	41.351924
3506.020659	531596.284135	41.356928
3506.018106	531537.778313	41.361933
3505.969739	531487.262270	41.366938
3506.090618	531435.203597	41.371943
3506.022612	531393.228898	41.376948
3505.769193	531339.612292	41.381952
3505.830449	531297.465333	41.386957
3505.855152	531244.208639	41.391962
3506.055877	531186.427244	41.396967
3505.746660	531159.091681	41.401972
3505.552952	531106.829010	41.406976
3505.448598	531060.716112	41.411981
3505.277588	531026.941780	41.416986
3505.379664	530978.673954	41.421991
3505.653223	530955.237437	41.426996
3505.815934	530906.606128	41.432000
3505.396333	530860.340360	41.437005
3505.334756	530813.057878	41.442010
3505.665841	530775.919464	41.447015
3505.363990	530743.125194	41.452020
3505.511985	530702.226078	41.457024
3505.609264	530659.010656	41.462029
3505.192779	530625.122674	41.467034
3505.332327	530577.706642	41.472039
3504.987308	530545.727208	41.477044
3505.167987	530502.801335	41.482048
3505.469551	530465.111055	41.487053
3505.455687	530423.428361	41.492058
3505.572310	530384.150246	41.497063
3505.522527	530354.144853	41.502068
3505.369332	530305.410026	41.507072
3505.599639	530269.296893	41.512077
3505.147504	530237.182175	41.517082
3505.452470	530194.336872	41.522087
3505.335090	530160.046917	41.527092
3505.287757	530125.695287	41.532096
3504.860546	530079.883171	41.537101
3505.109167	530051.800643	41.542106
3505.647174	530012.707644	41.547111
3504.915695	529977.655361	41.552116
3504.741448	529941.504356	41.557120
3505.090406	529909.262358	41.562125
3505.211180	529891.558162	41.567130
3505.273737	529841.423515	41.572135
3505.165342	529810.617883	41.577140
3504.589863	529776.045785	41.582144
3504.810111	529748.523023	41.587149
3504.487932	529719.620586	41.592154
3504.568187	529679.083221	41.597159
3504.744191	529659.702558	41.602164
3504.529190	529633.056858	41.607168
3504.929745	529605.909588	41.612173
3504.574860	529585.400023	41.617178
3504.815181	529548.677295	41.622183
3504.586461	529541.235000	41.627188
3504.460449	529508.309299	41.632192
3504.426560	529483.352745	41.637197
3504.588703	529464.075093	41.642202
3504.639088	529427.634754	41.647207
3504.603826	529416.473105	41.652212
3504.592852	529391.310663	41.657216
3504.904921	529361.448309	41.662221
3504.723457	529338.131829	41.667226
3504.614221	529308.285429	41.672231
3504.647242	529291.503982	41.677236
3504.620975	529269.880921	41.682240
3504.567008	529231.334323	41.687245
3504.521135	529208.703656	41.692250
3504.454376	529179.406141	41.697255
3504.524777	529159.182523	41.702260
3504.290612	529134.661321	41.707264
3505.024167	529122.872642	41.712269
3504.604803	529097.471087	41.717274
3504.847983	529060.847836	41.722279
3504.701425	529043.538659	41.727284
3504.684712	529016.304729	41.732288
3505.002042	528987.653599	41.737293
3504.706362	528961.979618	41.742298
3504.963495	528915.297975	41.747303
3504.917478	528896.052529	41.752308
3504.585454	528862.753781	41.757312
3504.615848	528834.754109	41.762317
3504.543604	528814.400998	41.767322
3504.708679	528788.148590	41.772327
3504.525405	528756.493680	41.777332
3505.011613	528737.618718	41.782336
3505.051288	528705.372610	41.787341
3504.690774	528672.179029	41.792346
3504.602614	528637.628477	41.797351
3504.520005	528622.532180	41.802356
3504.492215	528600.049382	41.807360
3504.727969	528576.261571	41.812365
3504.548224	528549.709533	41.817370
3504.639387	528522.407169	41.822375
3504.533143	528491.194352	41.827380
3504.510742	528476.694802	41.832384
3504.479986	528449.209446	41.837389
3504.347713	528430.836135	41.842394
3504.665888	528397.736848	41.847399
3504.506791	528375.678752	41.852404
3504.347136	528359.533172	41.857408
3504.654429	528328.355744	41.862413
3504.441488	528317.271933	41.867418
3504.516440	528283.503372	41.872423
3504.556073	528271.267861	41.877428
3504.537931	528233.218507	41.882432
3504.379862	528210.553608	41.887437
3504.175199	528195.476194	41.892442
3504.569575	528158.372149	41.897447
3504.329937	528139.611194	41.902452
3504.461559	528120.033521	41.907456
3504.516986	528098.749688	41.912461
3504.191581	528072.523078	41.917466
3504.465878	528062.524381	41.922471
3504.279316	528037.438069	41.927476
3504.091767	528017.961249	41.932480
3504.412027	527997.848262	41.937485
3504.311119	527977.549140	41.942490
3504.538894	527957.299114	41.947495
3504.343225	527941.259869	41.952500
3504.298812	527925.600984	41.957504
3504.251688	527913.732655	41.962509
3504.215705	527884.983765	41.967514
3504.219382	527856.936051	41.972519
3504.023088	527846.910523	41.977524
3503.950995	527825.697014	41.982528
3504.078109	527815.165533	41.987533
3503.675268	527809.063862	41.992538
3504.205826	527778.709172	41.997543
3504.200363	527774.010218	42.002548
3503.751260	527753.462625	42.007552
3504.057620	527724.962554	42.012557
3504.311146	527721.738727	42.017562
3504.156979	527707.410905	42.022567
3504.369989	527696.865770	42.027572
3504.224697	527675.107732	42.032576
3504.357305	527645.169435	42.037581
3504.298795	527628.703907	42.042586
3504.283680	527610.765954	42.047591
3504.378686	527596.954549	42.052596
3504.020909	527567.851653	42.057600
3504.173602	527561.308332	42.062605
3504.096555	527537.467329	42.067610
3504.201504	527525.372529	42.072615
3503.985382	527510.245737	42.077620
3504.042579	527492.296221	42.082624
3504.315058	527474.919101	42.087629
3503.926502	527452.239008	42.092634
3504.179267	527453.967845	42.097639
3504.146893	527423.549837	42.102644
3504.088772	527398.897046	42.107648
3504.456560	527385.295030	42.112653
3504.348708	527366.967163	42.117658
3504.184782	527345.262155	42.122663
3504.122040	527326.977649	42.127668
3504.051499	527308.795430	42.132672
3504.388522	527284.181084	42.137677
3504.175348	527278.200843	42.142682
3504.026340	527263.972879	42.147687
3503.967656	527242.705934	42.152692
3503.829218	527230.194540	42.157696
3504.182383	527210.883957	42.162701
3503.880064	527196.225326	42.167706
3504.157406	527187.943875	42.172711
3503.884726	527164.790220	42.177716
3504.443287	527148.681507	42.182720
3504.422225	527128.671905	42.187725
3503.864204	527123.706324	42.192730
3503.901473	527102.070261	42.197735
3503.916838	527073.412863	42.202740
3504.106992	527073.433348	42.207744
3503.970382	527054.351597	42.212749
3504.067966	527036.951102	42.217754
3503.953947	527024.486225	42.222759
3504.039964	527003.398242	42.227764
3503.877048	526991.244296	42.232768
3504.004043	526985.008029	42.237773
3503.918519	526970.213848	42.242778
3504.243300	526949.896671	42.247783
3503.941651	526946.255049	42.252788
3504.016287	526923.096688	42.257792
3504.048488	526910.406458	42.262797
3504.087284	526896.906561	42.267802
3504.211676	526862.318548	42.272807
3504.084069	526864.107567	42.277812
3503.636920	526839.970241	42.282816
3504.081649	526815.540304	42.287821
3503.854322	526829.423839	42.292826
3504.073794	526808.769355	42.297831
3504.131535	526785.562925	42.302836
3504.033402	526780.372935	42.307840
3503.841278	526752.000445	42.312845
3503.865283	526731.781065	42.317850
3504.045855	526730.489052	42.322855
3503.823187	526709.449467	42.327860
3503.491114	526713.595615	42.332864
3504.111149	526696.162715	42.337869
3503.960384	526680.165638	42.342874
3503.971537	526663.587022	42.347879
3504.046267	526662.766585	42.352884
3503.993040	526644.631409	42.357888
3503.860405	526632.826177	42.362893
3504.140728	526622.876166	42.367898
3504.167648	526595.075249	42.372903
3503.730361	526596.205689	42.377908
3503.561601	526577.077907	42.382912
3504.228620	526549.883299	42.387917
3504.007311	526552.748493	42.392922
3504.075716	526533.330477	42.397927
3504.080263	526509.980435	42.402932
3503.882371	526508.394441	42.407936
3503.833834	526474.287775	42.412941
3503.698863	526481.536299	42.417946
3503.846144	526473.376114	42.422951
3503.731039	526455.907520	42.427956
3503.678319	526436.053671	42.432960
3503.928768	526422.924241	42.437965
3503.644811	526425.091798	42.442970
3503.934973	526409.732322	42.447975
3504.153022	526392.817485	42.452980
3504.114013	526378.470265	42.457984
3504.183639	526359.102384	42.462989
3503.774328	526352.040908	42.467994
3504.198292	526333.425638	42.472999
3503.869881	526322.207061	42.478004
3503.713423	526311.668864	42.483008
3504.320655	526295.905385	42.488013
3503.894564	526281.973036	42.493018
3503.937549	526268.775188	42.498023
3503.966718	526241.680866	42.503028
3503.728032	526224.332632	42.508032
3503.958907	526208.881251	42.513037
3503.840022	526212.336805	42.518042
3503.984485	526187.549039	42.523047
3504.243389	526176.490240	42.528052
3504.067733	526163.377400	42.533056
3504.162421	526143.398808	42.538061
3503.795584	526145.124634	42.543066
3503.846645	526116.207169	42.548071
3503.881410	526101.848040	42.553076
3504.236221	526087.640480	42.558080
3504.112425	526061.176520	42.563085
3503.991937	526076.560057	42.568090
3503.851042	526047.824429	42.573095
3504.124907	526018.214539	42.578100
3504.025695	526017.825889	42.583104
3504.259141	525988.980451	42.588109
3503.698160	525981.538450	42.593114
3503.792639	525972.324986	42.598119
3503.877939	525946.939701	42.603124
3503.545699	525934.559002	42.608128
3503.824110	525931.937382	42.613133
3503.521340	525931.580902	42.618138
3503.833113	525911.972044	42.623143
3503.879540	525897.358180	42.628148
3503.973986	525888.195214	42.633152
3503.634752	525861.714432	42.638157
3503.846960	525863.146604	42.643162
3503.822937	525857.439183	42.648167
3503.609896	525854.743598	42.653172
3503.475978	525850.266545	42.658176
3503.932996	525816.078572	42.663181
3503.759559	525815.752191	42.668186
3503.658993	525820.266314	42.673191
3503.627856	525798.740379	42.678196
3503.805158	525791.636482	42.683200
3503.823149	525784.962098	42.688205
3503.735689	525782.600447	42.693210
3504.011048	525746.924777	42.698215
3504.022544	525734.893933	42.703220
3503.562404	525746.591348	42.708224
3503.949577	525718.176005	42.713229
3503.469738	525711.277017	42.718234
3503.691057	525695.422314	42.723239
3504.122158	525698.285632	42.728244
3503.706829	525679.448454	42.733248
3503.892520	525652.985448	42.738253
3503.287043	525656.922365	42.743258
3503.763852	525652.904699	42.748263
3503.763418	525629.503615	42.753268
3503.406138	525636.383316	42.758272
3504.111609	525609.181036	42.763277
3503.762607	525607.315578	42.768282
3503.792578	525589.772566	42.773287
3503.981368	525578.876063	42.778292
3503.391361	525574.572102	42.783296
3503.757096	525565.972588	42.788301
3503.704981	525541.720317	42.793306
3503.939967	525525.105144	42.798311
3503.580197	525538.606388	42.803316
3503.554394	525527.996481	42.808321
3504.008643	525498.003320	42.813325
3504.038341	525504.619745	42.818330
3503.925877	525485.683930	42.823335
3504.082860	525469.788629	42.828340
3503.660891	525465.761337	42.833345
3503.842257	525448.699673	42.838349
3503.694747	525428.404666	42.843354
3503.958490	525411.279399	42.848359
3503.777682	525412.622098	42.853364
3503.814683	525394.875588	42.858369
3503.968197	525379.486178	42.863373
3503.792718	525366.423199	42.868378
3503.768842	525358.592757	42.873383
3504.162779	525341.143579	42.878388
3504.031493	525346.926275	42.883393
3503.854903	525329.213450	42.888397
3503.888168	525306.362545	42.893402
3504.141505	525290.755099	42.898407
3503.938829	525275.522972	42.903412
3503.648225	525265.915070	42.908417
3503.934989	525242.720748	42.913421
3503.749399	525254.476216	42.918426
3503.712802	525226.025890	42.923431
3503.925112	525201.023700	42.928436
3503.879052	525200.525542	42.933441
3503.995149	525180.087470	42.938445
3503.786709	525178.654640	42.943450
3503.932266	525159.172220	42.948455
3503.849011	525145.690133	42.953460
3503.605727	525137.843716	42.958465
3503.779362	525128.061272	42.963469
3503.488587	525131.695857	42.968474
3503.703820	525116.195352	42.973479
3503.715489	525096.936193	42.978484
3503.475522	525098.945342	42.983489
3503.710445	525090.972779	42.988493
3503.421066	525088.693482	42.993498
3503.571675	525059.657288	42.998503
3503.481084	525059.823238	43.003508
3503.354711	525058.478516	43.008513
3503.678134	525041.798322	43.013517
3503.631369	525044.585652	43.018522
3503.885259	525030.039297	43.023527
3503.866868	525011.997852	43.028532
3503.671459	525009.501514	43.033537
3503.854696	524996.886984	43.038541
3503.693222	524968.304304	43.043546
3503.642650	524963.561107	43.048551
3503.830429	524958.628604	43.053556
3503.648959	524963.509566	43.058561
3503.926038	524931.875378	43.063565
3503.935367	524935.159308	43.068570
3503.608009	524932.481634	43.073575
3503.615116	524903.670016	43.078580
3503.725962	524894.352257	43.083585
3503.773966	524882.416093	43.088589
3503.826096	524885.440544	43.093594
3503.758579	524864.576187	43.098599
3503.756282	524852.546861	43.103604
3503.737237	524855.127662	43.108609
3503.757279	524844.712237	43.113613
3503.486621	524822.616307	43.118618
3503.457899	524805.031167	43.123623
3503.591471	524809.407479	43.128628
3503.666870	524804.088330	43.133633
3503.913807	524785.195974	43.138637
3503.606789	524783.677598	43.143642
3503.798911	524786.730488	43.148647
3503.913808	524763.360457	43.153652
3503.664767	524740.806091	43.158657
3503.638059	524723.018362	43.163661
3503.667981	524716.948191	43.168666
3503.678339	524720.889092	43.173671
3503.506818	524715.760575	43.178676
3503.758314	524693.127033	43.183681
3503.917537	524694.416050	43.188685
3503.807707	524697.769407	43.193690
3503.793798	524668.505780	43.198695
3503.764180	524650.061339	43.203700
3503.345895	524648.055079	43.208705
3503.622435	524642.249177	43.213709
3503.850607	524630.890898	43.218714
3503.546102	524615.118234	43.223719
3503.616959	524602.116790	43.228724
3503.858215	524608.295784	43.233729
3503.872770	524590.046475	43.238733
3503.370031	524568.138511	43.243738
3503.835054	524560.129319	43.248743
3503.562170	524558.504435	43.253748
3503.625571	524557.432952	43.258753
3503.853835	524534.853405	43.263757
3503.569334	524530.248143	43.268762
3503.246772	524530.754037	43.273767
3503.646596	524511.028462	43.278772
3503.436694	524543.158320	43.283777
3503.938219	524503.905930	43.288781
3503.603895	524494.051744	43.293786
3503.685922	524481.857175	43.298791
3504.068488	524480.684698	43.303796
3503.791957	524461.470326	43.308801
3503.825618	524446.250604	43.313805
3503.734800	524450.561385	43.318810
3503.995496	524419.686973	43.323815
3503.823772	524401.567984	43.328820
3503.270349	524396.297537	43.333825
3503.872063	524395.848614	43.338829
3503.535085	524388.117730	43.343834
3503.275586	524376.027604	43.348839
3503.585314	524359.197228	43.353844
3503.770598	524357.095539	43.358849
3503.532700	524361.985601	43.363853
3503.734627	524359.679096	43.368858
3503.810454	524337.881563	43.373863
3503.748270	524315.903626	43.378868
3503.672810	524321.324040	43.383873
3503.542235	524298.800876	43.388877
3503.537681	524303.805717	43.393882
3503.494808	524276.315087	43.398887
3503.951244	524295.248514	43.403892
3503.753674	524278.296044	43.408897
3503.569421	524249.715686	43.413901
3503.784762	524239.117361	43.418906
3503.920135	524234.748936	43.423911
3503.807857	524238.962071	43.428916
3503.868520	524211.960437	43.433921
3503.626246	524202.900275	43.438925
3503.803228	524206.410592	43.443930
3503.803809	524178.306363	43.448935
3503.734869	524155.166693	43.453940
3503.635772	524152.705546	43.458945
3503.595912	524172.576857	43.463949
3503.718136	524140.005194	43.468954
3503.581632	524122.031964	43.473959
3503.878912	524132.296612	43.478964
3503.839935	524104.602885	43.483969
3503.851771	524107.886588	43.488973
3503.826515	524070.485553	43.493978
3503.608447	524075.726399	43.498983
3504.169122	524067.802942	43.503988
3503.901863	524054.803947	43.508993
3503.714337	524051.446907	43.513997
3503.400644	524051.496485	43.519002
3503.898397	524022.706839	43.524007
3504.073325	524004.633711	43.529012
3503.641293	523999.394494	43.534017
3503.753079	523986.436632	43.539021
3503.845135	523966.961224	43.544026
3503.561451	523971.252068	43.549031
3504.192863	523951.135373	43.554036
3503.777852	523940.687026	43.559041
3504.131165	523915.761650	43.564045
3503.743808	523923.253407	43.569050
3504.050416	523898.487030	43.574055
3503.782754	523883.567139	43.579060
3503.869825	523879.560087	43.584065
3504.095180	523856.322927	43.589069
3503.897670	523840.229303	43.594074
3503.339888	523843.148153	43.599079
3504.000020	523826.059650	43.604084
3503.867624	523804.395401	43.609089
3503.960090	523790.631664	43.614093
3503.959013	523789.418676	43.619098
3503.973638	523761.564243	43.624103
3504.267774	523754.744274	43.629108
3503.642191	523737.858881	43.634113
3503.811930	523722.263129	43.639117
3503.700595	523713.333642	43.644122
3503.669900	523706.969380	43.649127
3503.901538	523687.825415	43.654132
3503.687881	523673.402279	43.659137
3503.745874	523667.226179	43.664141
3503.650094	523662.590841	43.669146
3503.799886	523640.174090	43.674151
3503.807358	523631.074134	43.679156
3503.473696	523627.184064	43.684161
3503.621167	523618.415816	43.689165
3503.800305	523603.778892	43.694170
3503.432170	523583.415325	43.699175
3503.736369	523587.310063	43.704180
3503.787903	523595.035899	43.709185
3503.928238	523570.800788	43.714189
3503.748046	523545.251474	43.719194
3503.423419	523557.434545	43.724199
3503.916840	523526.976585	43.729204
3503.420484	523523.263850	43.734209
3503.695685	523510.936918	43.739213
3503.529465	523499.994021	43.744218
3503.694924	523501.332699	43.749223
3503.486829	523505.712817	43.754228
3503.390750	523473.983098	43.759233
3503.856288	523458.542539	43.764237
3503.458674	523453.398801	43.769242
3503.231331	523472.694014	43.774247
3503.522698	523465.318320	43.779252
3503.390065	523464.277747	43.784257
3503.858577	523436.098270	43.789261
3503.902327	523425.223236	43.794266
3503.566646	523417.744425	43.799271
3503.615765	523414.248751	43.804276
3503.484337	523395.869514	43.809281
3503.616971	523376.336431	43.814285
3503.246002	523396.362129	43.819290
3503.598898	523390.745908	43.824295
3503.616808	523384.828783	43.829300
3503.579631	523381.953335	43.834305
3503.726109	523350.943282	43.839309
3503.666249	523351.407690	43.844314
3503.782519	523340.521137	43.849319
3503.828026	523342.182085	43.854324
3503.362742	523320.519248	43.859329
3503.556458	523299.308277	43.864333
3503.373576	523298.730584	43.869338
3503.297686	523301.320618	43.874343
3503.673016	523293.375528	43.879348
3503.100728	523299.279206	43.884353
3503.331891	523275.787544	43.889357
3503.465545	523274.654323	43.894362
3503.644930	523251.726859	43.899367
3503.785074	523252.159659	43.904372
3503.189103	523264.183636	43.909377
3503.556809	523250.375938	43.914381
3503.494937	523246.291170	43.919386
3502.778430	523228.813013	43.924391
3503.339239	523224.478176	43.929396
3503.433925	523226.030263	43.934401
3503.446070	523217.131535	43.939405
3503.510956	523214.442126	43.944410
3503.634099	523215.939167	43.949415
3503.605226	523214.730529	43.954420
3503.295692	523193.598956	43.959425
3503.775059	523174.617431	43.964429
3504.009887	523182.617797	43.969434
3503.684821	523173.620690	43.974439
3503.795188	523156.163419	43.979444
3503.856409	523144.779932	43.984449
3503.865707	523138.611327	43.989453
3503.597368	523139.917495	43.994458
3503.836230	523098.428440	43.999463
3504.044974	523099.406458	44.004468
3503.798391	523097.827816	44.009473
3503.593976	523080.167461	44.014477
3503.810262	523064.968124	44.019482
3503.641146	523062.214572	44.024487
3503.933070	523052.412176	44.029492
3503.592864	523036.593056	44.034497
3503.781126	523013.512199	44.039501
3503.702412	523017.214841	44.044506
3503.524084	522997.073288	44.049511
3503.433088	522988.039083	44.054516
3503.519509	522985.649538	44.059521
3503.451575	522963.519015	44.064525
3503.623003	522971.327303	44.069530
3503.616476	522970.772276	44.074535
3503.935072	522952.220307	44.079540
3503.868025	522942.676783	44.084545
3503.789585	522938.998963	44.089549
3503.482325	522924.236094	44.094554
3503.689316	522915.205304	44.099559
3503.767613	522895.680229	44.104564
3503.500809	522888.645246	44.109569
3503.664061	522884.777561	44.114573
3503.722623	522872.989895	44.119578
3503.318930	522847.929762	44.124583
3503.544482	522835.155203	44.129588
3503.444328	522846.646164	44.134593
3503.427954	522846.446547	44.139597
3503.648365	522850.961322	44.144602
3503.301939	522822.404065	44.149607
3503.362503	522813.598565	44.154612
3503.087944	522814.198024	44.159617
3503.424092	522806.410543	44.164621
3503.573401	522785.357571	44.169626
3503.309081	522796.722859	44.174631
3503.811403	522795.834647	44.179636
3503.324722	522792.979586	44.184641
3503.545494	522757.053168	44.189645
3503.605509	522767.760598	44.194650
3503.648555	522767.450486	44.199655
3503.824598	522763.833508	44.204660
3503.583248	522756.541687	44.209665
3503.963972	522737.575242	44.214669
3503.890652	522731.520642	44.219674
3503.739251	522723.456316	44.224679
3503.646469	522704.463566	44.229684
3503.659403	522691.520291	44.234689
3503.882937	522688.451859	44.239693
3503.842393	522685.930682	44.244698
3503.570671	522671.465276	44.249703
3503.759404	522650.203691	44.254708
3503.633437	522644.764001	44.259713
3503.531493	522643.769077	44.264717
3503.666166	522617.663015	44.269722
3503.591391	522610.648112	44.274727
3503.893662	522593.715977	44.279732
3503.590465	522596.544257	44.284737
3503.655627	522575.706521	44.289741
3503.299921	522581.475122	44.294746
3503.604060	522561.711743	44.299751
3504.190564	522554.541751	44.304756
3503.322507	522556.448270	44.309761
3503.698327	522534.145922	44.314765
3503.293305	522532.946130	44.319770
3503.535873	522535.233195	44.324775
3503.835907	522520.424528	44.329780
3503.518466	522517.289908	44.334785
3503.645371	522502.003065	44.339789
3503.497137	522486.608036	44.344794
3503.386523	522478.486589	44.349799
3503.689396	522473.939560	44.354804
3503.867901	522485.588944	44.359809
3503.663701	522465.703581	44.364813
3503.804894	522444.600898	44.369818
3503.617504	522442.305100	44.374823
3503.747843	522431.314609	44.379828
3503.501726	522409.717016	44.384833
3503.823588	522413.760906	44.389837
3503.524463	522398.389640	44.394842
3503.539386	522397.628993	44.399847
3503.603691	522379.672639	44.404852
3503.473627	522367.459443	44.409857
3503.591082	522355.409330	44.414861
3503.729008	522359.836173	44.419866
3503.611448	522352.423499	44.424871
3503.619271	522337.408085	44.429876
3503.547689	522323.972346	44.434881
3503.722899	522316.867255	44.439885
3503.887904	522316.992835	44.444890
3503.539868	522308.605510	44.449895
3503.951580	522271.181805	44.454900
3503.616428	522275.885652	44.459905
3503.742151	522270.304951	44.464909
3504.056200	522252.308985	44.469914
3503.761484	522246.086982	44.474919
3503.603359	522235.546374	44.479924
3503.496760	522228.940761	44.484929
3503.609844	522205.466212	44.489933
3503.521121	522207.552916	44.494938
3503.114134	522186.536536	44.499943
3503.713549	522189.879423	44.504948
3503.523698	522184.348569	44.509953
3503.748324	522179.308292	44.514957
3503.688730	522154.041040	44.519962
3503.693587	522140.036980	44.524967
3503.560797	522139.552434	44.529972
3503.624412	522142.272265	44.534977
3503.607415	522120.536968	44.539981
3503.439845	522104.992971	44.544986
3503.588324	522105.778362	44.549991
3503.559811	522098.958140	44.554996
3503.295536	522093.792892	44.560001
3502.978205	522102.841579	44.565005
3503.631668	522097.430178	44.570010
3503.260074	522087.378194	44.575015
3503.555256	522083.085039	44.580020
3503.178908	522080.869609	44.585025
3503.528515	522067.569304	44.590029
3503.700318	522069.109314	44.595034
3503.573942	522069.988700	44.600039
3503.798268	522041.339860	44.605044
3503.631636	522032.923721	44.610049
3503.709599	522031.950878	44.615053
3503.758019	522030.780489	44.620058
3503.590181	522014.377034	44.625063
3503.718590	521986.046579	44.630068
3503.528551	521989.665941	44.635073
3503.736667	521978.612297	44.640077
3503.556302	521971.057713	44.645082
3502.990956	521959.165775	44.650087
3503.316926	521930.702891	44.655092
3503.555496	521938.096633	44.660097
3503.311875	521949.762565	44.665101
3503.333258	521947.130377	44.670106
3503.373740	521942.473009	44.675111
3503.494553	521934.516929	44.680116
3503.585770	521948.607090	44.685121
3503.447384	521920.824228	44.690125
3503.602833	521908.515007	44.695130
3503.572534	521897.751760	44.700135
3503.493957	521897.764179	44.705140
3503.375946	521902.433815	44.710145
3503.416263	521893.277137	44.715149
3503.334960	521874.938805	44.720154
3503.188034	521873.394846	44.725159
3503.486689	521866.371156	44.730164
3503.345868	521873.622672	44.735169
3503.373477	521863.456901	44.740173
3503.278609	521871.055036	44.745178
3503.397906	521867.295166	44.750183
3503.489311	521866.219081	44.755188
3503.554641	521845.127609	44.760193
3503.586384	521826.164704	44.765197
3503.431294	521821.790982	44.770202
3503.401268	521820.430759	44.775207
3503.782077	521816.528437	44.780212
3503.851191	521823.898460	44.785217
3503.392533	521796.317666	44.790221
3503.642208	521787.835603	44.795226
3503.498203	521777.747456	44.800231
3503.692578	521786.563780	44.805236
3503.729269	521772.453263	44.810241
3503.677255	521751.531880	44.815245
3503.909031	521741.990975	44.820250
3503.434494	521742.268194	44.825255
3504.010974	521711.338710	44.830260
3503.433372	521705.666756	44.835265
3503.520139	521687.554424	44.840269
3503.626235	521688.599307	44.845274
3503.543803	521687.803459	44.850279
3503.757754	521658.093932	44.855284
3503.434131	521662.745578	44.860289
3503.576210	521648.213858	44.865293
3503.594421	521649.120969	44.870298
3503.828234	521649.791785	44.875303
3503.970934	521612.156307	44.880308
3503.550309	521619.401604	44.885313
3503.787414	521606.219815	44.890317
3503.882098	521588.460006	44.895322
3503.192287	521570.116394	44.900327
3503.485401	521564.205664	44.905332
3503.367243	521564.982668	44.910337
3503.688030	521560.836996	44.915341
3503.653892	521554.624098	44.920346
3503.179066	521531.595380	44.925351
3503.520597	521524.514212	44.930356
3503.528282	521523.956889	44.935361
3503.710917	521518.265826	44.940365
3503.778065	521519.114655	44.945370
3503.600298	521503.824471	44.950375
3503.485228	521482.508265	44.955380
3503.365494	521480.606081	44.960385
3503.242954	521480.423227	44.965389
3503.394075	521482.269895	44.970394
3503.576488	521485.779948	44.975399
3503.679165	521462.558749	44.980404
3503.297455	521444.722411	44.985409
3503.529718	521443.624035	44.990413
3503.369677	521430.605983	44.995418
3503.462765	521438.376836	45.000423
3503.207071	521442.057251	45.005428
3503.471800	521438.628187	45.010433
3503.417928	521428.121133	45.015437
3503.678587	521432.124387	45.020442
3503.321499	521422.575253	45.025447
3503.624862	521410.950059	45.030452
3503.651333	521418.023670	45.035457
3503.200946	521410.208167	45.040461
3503.632771	521398.663773	45.045466
3503.474646	521380.842583	45.050471
3503.282182	521377.687987	45.055476
3503.598617	521376.020190	45.060481
3503.455525	521366.133866	45.065485
3503.432024	521368.817040	45.070490
3503.167875	521376.442160	45.075495
3503.503692	521353.638960	45.080500
3503.552122	521340.739555	45.085505
3503.353603	521329.345292	45.090509
3503.337080	521323.988973	45.095514
3503.253060	521316.418857	45.100519
3503.607701	521317.020035	45.105524
3503.263151	521331.533495	45.110529
3503.414910	521322.914999	45.115533
3503.403377	521298.599386	45.120538
3503.444512	521300.867906	45.125543
3504.056210	521270.083689	45.130548
3503.589715	521276.224152	45.135553
3503.283355	521268.335261	45.140557
3503.310585	521249.877959	45.145562
3503.361380	521236.876986	45.150567
3503.657800	521233.240645	45.155572
3503.638020	521236.934377	45.160577
3503.607781	521239.062518	45.165581
3503.797538	521226.696805	45.170586
3503.477862	521219.669451	45.175591
3503.897717	521189.218740	45.180596
3503.676414	521193.348783	45.185601
3503.553682	521193.772632	45.190605
3503.834617	521162.939376	45.195610
3503.689991	521156.642676	45.200615
3503.805595	521148.029802	45.205620
3503.635816	521160.847426	45.210625
3503.685201	521131.617958	45.215629
3503.710456	521117.104229	45.220634
3503.759745	521109.866844	45.225639
3503.939334	521095.177034	45.230644
3503.760465	521087.571245	45.235649
3503.553445	521082.093284	45.240653
3503.577877	521071.674737	45.245658
3503.409338	521074.380882	45.250663
3503.465556	521040.498951	45.255668
3503.045618	521034.043488	45.260673
3503.515502	521028.155185	45.265677
3503.692404	521024.183789	45.270682
3503.497551	521027.500783	45.275687
3503.596246	521020.761119	45.280692
3503.768061	521013.099871	45.285697
3503.494225	520990.443076	45.290701
3503.864600	520985.884966	45.295706
3503.621224	520980.716059	45.300711
3503.600650	520971.366259	45.305716
3503.434466	520953.090861	45.310721
3503.552000	520949.786073	45.315725
3503.676053	520945.469112	45.320730
3503.358720	520939.957980	45.325735
3503.616008	520929.755327	45.330740
3503.713568	520924.734746	45.335745
3503.586425	520901.447957	45.340749
3503.610711	520894.416657	45.345754
3503.721701	520892.477938	45.350759
3503.782477	520878.918972	45.355764
3503.672555	520875.447889	45.360769
3503.673073	520853.455345	45.365773
3503.844345	520846.299679	45.370778
3503.242229	520854.029014	45.375783
3503.495815	520826.637351	45.380788
3503.414501	520817.499293	45.385793
3503.190251	520817.231390	45.390797
3503.539612	520814.749413	45.395802
3503.332892	520808.816295	45.400807
3503.719180	520807.693535	45.405812
3503.405663	520811.282114	45.410817
3503.398699	520789.543455	45.415821
3503.611219	520771.814692	45.420826
3503.518493	520767.936407	45.425831
3503.624763	520761.751573	45.430836
3503.638714	520771.962021	45.435841
3503.387497	520753.345935	45.440845
3503.409376	520746.163278	45.445850
3503.374924	520742.326334	45.450855
3503.776966	520725.882070	45.455860
3503.869275	520739.265296	45.460865
3503.499089	520723.600329	45.465869
3503.575541	520699.269917	45.470874
3503.348973	520697.131736	45.475879
3503.589244	520683.898145	45.480884
3503.410302	520689.386684	45.485889
3503.575277	520693.354686	45.490893
3503.154613	520669.001681	45.495898
3502.980607	520664.478963	45.500903
3503.236810	520643.254654	45.505908
3503.147394	520645.442783	45.510913
3503.423588	520639.837744	45.515917
3503.604543	520641.123655	45.520922
3503.521333	520645.939823	45.525927
3503.868700	520639.514606	45.530932
3503.671487	520641.972563	45.535937
3503.920582	520618.221442	45.540941
3503.577634	520604.978847	45.545946
3503.325073	520607.394998	45.550951
3503.378951	520605.869738	45.555956
3503.152840	520607.472779	45.560961
3503.324954	520599.356266	45.565965
3503.377124	520576.040672	45.570970
3503.169421	520572.231070	45.575975
3503.529151	520565.753312	45.580980
3503.819872	520565.050107	45.585985
3503.601515	520571.050498	45.590989
3503.720175	520565.723123	45.595994
3503.532539	520546.388935	45.600999
3503.798949	520525.213418	45.606004
3503.716321	520527.248815	45.611009
3503.442867	520527.443710	45.616013
3503.588358	520494.759940	45.621018
3503.316653	520483.123858	45.626023
3503.419429	520477.798965	45.631028
3503.505143	520478.695473	45.636033
3503.383856	520477.248444	45.641037
3503.650285	520477.256894	45.646042
3503.355287	520469.568054	45.651047
3503.821021	520447.804790	45.656052
3503.869777	520441.376132	45.661057
3503.547365	520444.511169	45.666061
3503.813270	520420.302075	45.671066
3503.408917	520403.529908	45.676071
3503.847076	520396.635217	45.681076
3503.580412	520385.908329	45.686081
3503.665118	520389.282385	45.691085
3503.494341	520373.535007	45.696090
3503.397525	520348.624751	45.701095
3503.578418	520347.787218	45.706100
3503.636730	520349.041977	45.711105
3503.573408	520347.788011	45.716109
3503.462865	520334.811819	45.721114
3503.399487	520303.879685	45.726119
3503.600398	520300.258234	45.731124
3503.262545	520301.777847	45.736129
3503.262623	520301.980071	45.741133
3503.324350	520299.644596	45.746138
3503.280061	520303.746885	45.751143
3503.569539	520298.594663	45.756148
3503.624062	520291.659443	45.761153
3503.511064	520268.470634	45.766157
3503.569523	520260.321357	45.771162
3503.142940	520254.119430	45.776167
3503.631279	520252.879386	45.781172
3503.456323	520257.710168	45.786177
3503.308210	520256.065122	45.791181
3503.294473	520232.557219	45.796186
3503.315707	520230.784286	45.801191
3503.093812	520215.550428	45.806196
3503.293345	520219.715321	45.811201
3503.268015	520210.921991	45.816205
3503.485693	520218.623175	45.821210
3503.052992	520218.843241	45.826215
3502.784288	520219.441863	45.831220
3503.066207	520220.357935	45.836225
3503.180235	520221.098304	45.841229
3503.822498	520213.969042	45.846234
3503.214502	520224.278129	45.851239
3503.335393	520219.051408	45.856244
3503.538353	520197.127105	45.861249
3503.313035	520191.196701	45.866253
3503.356736	520181.027338	45.871258
3503.195444	520188.586194	45.876263
3503.617558	520173.705548	45.881268
3503.391805	520181.729630	45.886273
3503.291623	520177.751264	45.891277
3503.357579	520181.987838	45.896282
3502.949050	520166.480074	45.901287
3503.100988	520167.720049	45.906292
3503.402403	520175.509138	45.911297
3503.192639	520160.576669	45.916301
3503.440416	520146.734743	45.921306
3503.421101	520141.176238	45.926311
3503.313355	520138.210250	45.931316
3503.444478	520132.678526	45.936321
3503.517675	520137.975720	45.941325
3503.923456	520130.428761	45.946330
3503.484816	520115.582983	45.951335
3503.629291	520092.353231	45.956340
3503.675881	520105.036366	45.961345
3503.570591	520101.513825	45.966349
3503.705747	520092.088350	45.971354
3503.394439	520076.817934	45.976359
3503.861498	520064.761436	45.981364
3503.610370	520069.755991	45.986369
3503.461096	520068.920067	45.991373
3503.567872	520053.735232	45.996378
3503.380432	520042.338318	46.001383
3503.478912	520024.525650	46.006388
3503.365731	520027.577137	46.011393
3503.288423	520032.948712	46.016397
3503.222998	520027.599697	46.021402
3503.440999	520033.227958	46.026407
3503.481547	520015.171637	46.031412
3503.656989	520000.430940	46.036417
3503.469921	519986.253125	46.041421
3503.491531	519978.210652	46.046426
3503.318344	519986.378202	46.051431
3503.267162	519993.009664	46.056436
3503.418334	519989.396006	46.061441
3503.479580	519977.656382	46.066445
3503.440041	519950.815183	46.071450
3503.194278	519953.382036	46.076455
3503.510038	519941.652721	46.081460
3503.389805	519934.492169	46.086465
3503.385608	519938.638773	46.091469
3503.675491	519936.671669	46.096474
3503.189083	519939.428238	46.101479
3503.364584	519912.249628	46.106484
3503.565288	519903.875452	46.111489
3503.485546	519894.888310	46.116493
3503.472645	519903.991216	46.121498
3503.276764	519900.634631	46.126503
3503.315701	519896.735329	46.131508
3503.121715	519904.754526	46.136513
3503.125707	519912.641308	46.141517
3503.495866	519904.290910	46.146522
3503.441450	519872.446459	46.151527
3503.260337	519866.660631	46.156532
3503.646405	519865.234482	46.161537
3503.440122	519867.188382	46.166541
3503.670537	519866.039636	46.171546
3503.529070	519858.124000	46.176551
3503.735913	519825.884243	46.181556
3503.763368	519818.801420	46.186561
3503.400366	519823.914853	46.191565
3503.684450	519817.752121	46.196570
3503.033176	519806.883396	46.201575
3503.148187	519786.185900	46.206580
3503.216941	519775.102234	46.211585
3503.197808	519774.650211	46.216589
3503.053283	519780.234735	46.221594
3503.166056	519780.975323	46.226599
3503.201901	519778.593304	46.231604
3503.198027	519779.402888	46.236609
3502.960953	519784.951477	46.241613
3503.272732	519778.936036	46.246618
3503.095042	519775.879914	46.251623
3503.314591	519769.980168	46.256628
3503.082070	519772.747199	46.261633
3503.074060	519782.355006	46.266637
3503.443252	519782.751703	46.271642
3503.257180	519782.578869	46.276647
3503.354162	519782.866906	46.281652
3503.190407	519779.909704	46.286657
3503.258826	519775.348425	46.291661
3503.223568	519774.949512	46.296666
3503.173921	519771.974274	46.301671
3503.619104	519749.050435	46.306676
3503.495684	519746.086853	46.311681
3503.472367	519741.843428	46.316685
3503.137490	519736.638025	46.321690
3503.375391	519746.308110	46.326695
3503.408198	519733.966076	46.331700
3503.555713	519741.274087	46.336705
3503.435779	519719.096813	46.341709
3503.462210	519709.132132	46.346714
3503.393945	519692.255555	46.351719
3503.342945	519697.977008	46.356724
3503.257522	519697.282656	46.361729
3503.361642	519697.519005	46.366733
3503.582716	519693.742552	46.371738
3503.142881	519684.508841	46.376743
3503.317807	519659.150100	46.381748
3503.460770	519649.925381	46.386753
3503.425312	519655.846637	46.391757
3503.584338	519643.181220	46.396762
3503.366943	519655.956986	46.401767
3503.586897	519659.259256	46.406772
3503.525760	519667.358694	46.411777
3503.376929	519639.573599	46.416781
3503.435299	519627.126322	46.421786
3502.928077	519617.094244	46.426791
3503.508757	519618.418184	46.431796
3503.179307	519621.453365	46.436801
3503.294904	519613.800350	46.441805
3503.445447	519602.905885	46.446810
3503.755616	519605.030999	46.451815
3503.299222	519590.490918	46.456820
3503.145835	519576.256863	46.461825
3502.947463	519572.243306	46.466829
3503.573787	519562.032039	46.471834
3503.408512	519580.058011	46.476839
3503.582400	519573.053061	46.481844
3503.447925	519567.209195	46.486849
3503.304183	519578.254293	46.491853
3503.327578	519559.593445	46.496858
3503.298731	519545.996979	46.501863
3503.568645	519525.527480	46.506868
3503.501417	519536.206582	46.511873
3503.305887	519525.670132	46.516877
3503.624971	519525.366894	46.521882
3503.305030	519538.057835	46.526887
3503.597970	519527.343062	46.531892
3503.460297	519504.814371	46.536897
3503.329946	519494.621531	46.541901
3503.646154	519500.891755	46.546906
3503.312396	519494.624305	46.551911
3503.420193	519493.090420	46.556916
3503.248505	519496.454622	46.561921
3502.915354	519500.349958	46.566925
3503.168849	519486.708819	46.571930
3503.116667	519496.121529	46.576935
3503.237386	519480.074412	46.581940
3503.476777	519484.637687	46.586945
3503.306795	519462.619662	46.591949
3503.320145	519447.145661	46.596954
3503.276905	519461.056973	46.601959
3503.383554	519437.832274	46.606964
3503.267096	519446.800115	46.611969
3503.257076	519447.105069	46.616973
3503.382687	519446.124544	46.621978
3503.203911	519450.096616	46.626983
3503.314409	519443.202753	46.631988
3503.357504	519449.465601	46.636993
3503.186804	519433.919553	46.641997
3503.393292	519425.645343	46.647002
3503.230286	519419.654248	46.652007
3503.193485	519415.261184	46.657012
3503.103850	519415.882093	46.662017
3503.106102	519422.606463	46.667021
3503.072287	519413.055618	46.672026
3503.081198	519417.604778	46.677031
3503.069867	519418.314435	46.682036
3503.380394	519407.546242	46.687041
3503.425511	519412.645861	46.692045
3503.179170	519414.505022	46.697050
3503.046207	519427.267621	46.702055
3503.499932	519422.746470	46.707060
3503.475380	519414.357084	46.712065
3503.343685	519398.602591	46.717069
3503.578216	519380.767723	46.722074
3503.431004	519377.757272	46.727079
3503.147885	519382.150348	46.732084
3503.615596	519371.003354	46.737089
3503.447128	519376.136741	46.742093
3503.453931	519359.500767	46.747098
3503.117586	519335.941442	46.752103
3503.138723	519336.848220	46.757108
3503.322847	519333.330335	46.762113
3503.238213	519341.888706	46.767117
3503.820597	519322.583058	46.772122
3503.482832	519327.136472	46.777127
3503.515986	519331.681824	46.782132
3503.133466	519324.259086	46.787137
3503.399522	519307.733772	46.792141
3503.591950	519292.585258	46.797146
3503.282727	519292.836379	46.802151
3503.181441	519281.981504	46.807156
3503.634524	519285.398692	46.812161
3503.299541	519288.586495	46.817165
3503.561140	519276.915829	46.822170
3503.291103	519301.380073	46.827175
3503.225134	519281.974601	46.832180
3503.393395	519261.015216	46.837185
3503.177931	519259.785211	46.842189
3503.614321	519250.817268	46.847194
3503.429241	519260.857865	46.852199
3503.397020	519242.559383	46.857204
3503.663349	519257.281502	46.862209
3503.248045	519237.476127	46.867213
3503.840149	519209.775451	46.872218
3503.636381	519203.487344	46.877223
3503.485281	519205.735976	46.882228
3503.639759	519205.660999	46.887233
3503.717288	519199.328432	46.892237
3503.511770	519177.012264	46.897242
3503.259878	519184.434212	46.902247
3503.521386	519161.184647	46.907252
3503.637069	519168.599070	46.912257
3503.525573	519175.746020	46.917261
3503.752319	519148.810861	46.922266
3503.742056	519128.587401	46.927271
3503.719482	519123.534694	46.932276
3503.927243	519123.147919	46.937281
3503.694142	519097.347172	46.942285
3503.919136	519079.715737	46.947290
3503.584916	519085.229351	46.952295
3503.568101	519079.366715	46.957300
3503.736578	519036.867205	46.962305
3503.356805	519032.882186	46.967309
3503.504708	519029.471087	46.972314
3503.430986	519027.510780	46.977319
3503.404732	519041.015259	46.982324
3503.503714	519023.707058	46.987329
3503.465446	519002.223791	46.992333
3503.411703	518986.456582	46.997338
3503.262126	518996.845671	47.002343
3503.317704	518991.477193	47.007348
3503.471368	518982.503225	47.012353
3503.293298	518989.205709	47.017357
3503.683931	518983.076389	47.022362
3503.485282	518964.601650	47.027367
3503.761219	518954.951020	47.032372
3503.530564	518952.358184	47.037377
3503.557530	518948.865056	47.042381
3503.675681	518937.975272	47.047386
3503.425481	518935.233833	47.052391
3503.206005	518920.453458	47.057396
3503.686791	518911.023243	47.062401
3503.402840	518911.927699	47.067405
3503.544631	518900.680210	47.072410
3503.394986	518903.889358	47.077415
3503.244678	518884.041675	47.082420
3503.833155	518870.701028	47.087425
3503.515336	518855.481065	47.092429
3503.593049	518855.519347	47.097434
3503.203508	518867.918422	47.102439
3503.479770	518864.739820	47.107444
3503.285421	518855.264587	47.112449
3503.235616	518833.530106	47.117453
3503.321876	518823.150922	47.122458
3503.091948	518820.406260	47.127463
3503.150323	518811.750642	47.132468
3503.313953	518824.719650	47.137473
3503.198478	518824.282828	47.142477
3503.257865	518822.958787	47.147482
3503.236316	518829.333215	47.152487
3503.129340	518826.467994	47.157492
3503.377039	518824.456863	47.162497
3503.263144	518830.491941	47.167501
3503.527000	518827.113037	47.172506
3503.323681	518803.683615	47.177511
3503.484194	518790.663361	47.182516
3503.509452	518784.692842	47.187521
3503.219198	518778.367678	47.192525
3503.536257	518776.699525	47.197530
3503.529822	518782.970455	47.202535
3503.578844	518768.855401	47.207540
3503.632234	518757.621787	47.212545
3503.071563	518754.170928	47.217549
3503.807275	518740.958598	47.222554
3503.529001	518749.092806	47.227559
3503.522640	518754.301893	47.232564
3503.721835	518743.146352	47.237569
3503.293865	518714.038583	47.242573
3503.721630	518700.723199	47.247578
3503.658094	518708.975180	47.252583
3503.527308	518704.192268	47.257588
3503.531445	518688.112241	47.262593
3503.203289	518674.309539	47.267597
3503.356092	518665.689484	47.272602
3503.245811	518660.549369	47.277607
3503.129229	518650.707778	47.282612
3503.105560	518652.380138	47.287617
3502.911365	518666.417108	47.292621
3503.292411	518655.182202	47.297626
3503.400164	518659.412564	47.302631
3503.019453	518666.349462	47.307636
3503.284621	518662.565805	47.312641
3503.140313	518661.172817	47.317645
3503.320973	518661.953291	47.322650
3503.340637	518668.574089	47.327655
3503.310803	518666.606802	47.332660
3503.408212	518640.601410	47.337665
3503.324934	518630.956800	47.342669
3503.271130	518613.065544	47.347674
3502.913296	518624.600196	47.352679
3503.065124	518618.407356	47.357684
3503.324096	518626.861228	47.362689
3503.441269	518623.151517	47.367693
3503.476988	518612.729625	47.372698
3502.750017	518630.440897	47.377703
3503.162856	518621.375206	47.382708
3503.633008	518618.873813	47.387713
3503.114056	518625.984270	47.392717
3503.407545	518621.083713	47.397722
3503.040684	518599.752984	47.402727
3503.085396	518601.667363	47.407732
3503.633746	518588.332831	47.412737
3503.293660	518594.504873	47.417741
3503.460964	518583.859908	47.422746
3503.460946	518586.742082	47.427751
3503.609534	518576.909102	47.432756
3503.508338	518577.632998	47.437761
3503.273161	518567.961794	47.442765
3503.414679	518546.045002	47.447770
3503.547310	518543.293556	47.452775
3503.197181	518539.354295	47.457780
3503.464209	518545.733788	47.462785
3503.418242	518544.780328	47.467789
3503.608244	518542.171507	47.472794
3503.479301	518520.347991	47.477799
3503.549427	518503.701145	47.482804
3503.598006	518495.957073	47.487809
3503.458469	518506.648271	47.492813
3503.715107	518499.326399	47.497818
3503.760517	518491.633391	47.502823
3503.514863	518466.490980	47.507828
3503.688574	518458.170901	47.512833
3503.519666	518451.624172	47.517837
3503.653056	518454.687544	47.522842
3503.392745	518433.390324	47.527847
3503.327052	518413.882654	47.532852
3503.631475	518401.597823	47.537857
3503.000295	518413.479214	47.542861
3503.416929	518410.379470	47.547866
3503.285600	518413.383558	47.552871
3503.339797	518413.273863	47.557876
3503.509566	518408.392797	47.562881
3502.946854	518408.987383	47.567885
3503.490401	518392.164470	47.572890
3503.489058	518385.338407	47.577895
3503.387405	518381.056446	47.582900
3503.425586	518375.134302	47.587905
3503.381724	518379.540394	47.592909
3503.795178	518366.378698	47.597914
3503.314830	518366.606312	47.602919
3503.251600	518344.317092	47.607924
3503.365437	518326.348464	47.612929
3503.171777	518326.277942	47.617933
3503.207908	518325.362058	47.622938
3503.242095	518327.075872	47.627943
3503.546196	518319.392463	47.632948
3503.462634	518330.125494	47.637953
3503.507228	518331.584837	47.642957
3503.181112	518324.506687	47.647962
3503.356752	518328.776970	47.652967
3503.251136	518302.954828	47.657972
3503.205140	518277.982835	47.662977
3503.372216	518278.765475	47.667981
3503.500038	518282.032020	47.672986
3503.364278	518277.502597	47.677991
3503.337320	518276.242724	47.682996
3503.674337	518278.212073	47.688001
3503.106525	518278.301816	47.693005
3503.502337	518256.091621	47.698010
3503.587056	518250.263208	47.703015
3503.307290	518254.959444	47.708020
3503.299531	518251.522222	47.713025
3503.251070	518254.664938	47.718029
3503.331329	518245.145952	47.723034
3503.147590	518250.939452	47.728039
3503.360146	518248.984372	47.733044
3503.427590	518239.568539	47.738049
3503.571351	518233.882485	47.743053
3503.365951	518210.755941	47.748058
3503.450157	518208.871707	47.753063
3503.346234	518200.747075	47.758068
3503.264825	518208.850434	47.763073
3503.399615	518208.525737	47.768077
3503.504037	518209.571111	47.773082
3503.480080	518193.950133	47.778087
3503.428668	518176.867075	47.783092
3503.801245	518156.935874	47.788097
3503.407836	518164.431212	47.793101
3503.642797	518156.708089	47.798106
3503.553186	518149.693616	47.803111
3503.634175	518135.269573	47.808116
3503.565223	518116.267725	47.813121
3503.312105	518112.565857	47.818125
3503.812872	518105.154662	47.823130
3503.291758	518114.591708	47.828135
3503.443091	518099.650858	47.833140
3503.491809	518089.479411	47.838145
3503.230800	518092.352355	47.843149
3503.354812	518083.028624	47.848154
3503.493335	518079.264851	47.853159
3503.539378	518076.628144	47.858164
3503.663435	518083.384376	47.863169
3503.252707	518063.930825	47.868173
3503.863196	518032.432820	47.873178
3503.218725	518037.540721	47.878183
3503.236700	518030.256363	47.883188
3503.299974	518035.707502	47.888193
3503.209315	518039.463721	47.893197
3503.527436	518032.384756	47.898202
3503.105149	518042.160187	47.903207
3503.168487	518038.964514	47.908212
3503.298838	518017.503881	47.913217
3503.228525	518006.896100	47.918221
3503.690949	517987.607856	47.923226
3503.014588	517985.944935	47.928231
3503.316649	517998.134222	47.933236
3503.304057	517986.505981	47.938241
3503.304578	517993.635738	47.943245
3503.413449	517989.522667	47.948250
3503.292481	517995.508601	47.953255
3503.464246	517988.553881	47.958260
3503.488994	517968.475163	47.963265
3503.062814	517966.418736	47.968269
3503.401931	517943.357455	47.973274
3503.580083	517944.138361	47.978279
3503.119719	517947.649634	47.983284
3503.430791	517946.184612	47.988289
3503.072821	517955.393699	47.993293
3503.450110	517941.933984	47.998298
3503.222865	517951.274111	48.003303
3503.643052	517942.156323	48.008308
3503.631786	517920.920212	48.013313
3503.091477	517927.781509	48.018317
3503.130058	517912.706612	48.023322
3503.405437	517912.764222	48.028327
3503.213458	517906.979420	48.033332
3503.335056	517913.028179	48.038337
3503.052255	517909.027558	48.043341
3503.209805	517906.828299	48.048346
3503.189038	517908.854241	48.053351
3503.127599	517908.863952	48.058356
3503.050159	517908.421093	48.063361
3503.310447	517912.981505	48.068365
3503.421943	517902.041523	48.073370
3503.295136	517890.279566	48.078375
3502.947742	517879.664929	48.083380
3503.461872	517870.683954	48.088385
3503.296167	517864.035352	48.093389
3503.407707	517869.175518	48.098394
3503.155807	517876.294653	48.103399
3503.368591	517876.210457	48.108404
3503.509252	517864.456775	48.113409
3503.265166	517869.552014	48.118413
3503.611259	517863.783288	48.123418
3503.553102	517847.105488	48.128423
3503.555191	517837.295222	48.133428
3503.696625	517828.170861	48.138433
3503.449913	517832.811426	48.143437
3503.517456	517821.979471	48.148442
3503.237988	517795.830047	48.153447
3503.431092	517787.253732	48.158452
3503.630966	517777.917839	48.163457
3503.334713	517787.016131	48.168461
3503.481868	517780.621449	48.173466
3503.435668	517780.021949	48.178471
3503.077619	517771.937270	48.183476
3503.586669	517751.023241	48.188481
3503.391626	517734.366962	48.193485
3503.345581	517730.682848	48.198490
3503.412425	517744.021972	48.203495
3503.459532	517735.974375	48.208500
3503.580990	517729.887137	48.213505
3503.056852	517746.758221	48.218509
3503.170593	517732.733187	48.223514
3503.090573	517720.053508	48.228519
3503.137780	517704.572522	48.233524
3503.477384	517689.955516	48.238529
3503.061292	517706.809564	48.243533
3503.351307	517678.041592	48.248538
3503.266990	517686.752472	48.253543
3503.209187	517686.003101	48.258548
3503.432118	517677.826552	48.263553
3503.234808	517687.718336	48.268557
3503.304590	517690.589635	48.273562
3503.208146	517686.964043	48.278567
3503.282159	517690.390912	48.283572
3503.098416	517692.392071	48.288577
3503.168184	517697.184923	48.293581
3503.284178	517693.677459	48.298586
3503.268409	517674.514995	48.303591
3502.969634	517670.971946	48.308596
3503.154497	517649.552787	48.313601
3503.162337	517653.192391	48.318605
3503.329991	517648.665407	48.323610
3503.261630	517649.030183	48.328615
3503.347913	517637.032098	48.333620
3503.627566	517652.461490	48.338625
3503.061179	517654.826534	48.343629
3503.301324	517642.096193	48.348634
3503.245335	517648.729357	48.353639
3502.834313	517654.103882	48.358644
3503.313558	517638.453416	48.363649
3503.002462	517649.779090	48.368653
3503.050369	517646.535213	48.373658
3503.164986	517652.079498	48.378663
3503.265161	517653.226713	48.383668
3503.281819	517648.571892	48.388673
3503.091291	517631.409123	48.393677
3503.607962	517622.377045	48.398682
3503.405698	517613.812561	48.403687
3502.974515	517614.588652	48.408692
3503.479522	517603.282875	48.413697
3503.180992	517609.499281	48.418701
3502.978535	517613.576671	48.423706
3503.254580	517611.358645	48.428711
3503.264907	517611.862687	48.433716
3503.336094	517615.138316	48.438721
3503.085541	517608.503021	48.443725
3503.200417	517607.321816	48.448730
3502.851868	517608.590521	48.453735
3502.880583	517613.844992	48.458740
3502.964103	517612.365338	48.463745
3502.884120	517609.445071	48.468749
3503.079642	517617.150979	48.473754
3503.055417	517615.233248	48.478759
3503.045137	517607.700332	48.483764
3503.316144	517608.365444	48.488769
3503.002559	517621.562524	48.493773
3503.150131	517607.886009	48.498778
3503.400586	517610.880469	48.503783
3503.083860	517611.739606	48.508788
3503.395472	517614.522130	48.513793
3503.146885	517609.656383	48.518797
3503.447099	517602.478931	48.523802
3503.378770	517579.683811	48.528807
3503.160524	517571.273532	48.533812
3503.298782	517570.442601	48.538817
3503.124437	517573.403072	48.543821
3503.479292	517562.272701	48.548826
3503.265094	517569.891684	48.553831
3502.998851	517578.479672	48.558836
3503.290966	517579.141449	48.563841
3503.319073	517586.267021	48.568845
3503.281542	517572.215192	48.573850
3503.186452	517568.437658	48.578855
3503.169095	517570.361967	48.583860
3503.191016	517541.585563	48.588865
3503.001241	517525.181078	48.593869
3503.161058	517524.296170	48.598874
3503.293657	517516.841766	48.603879
3502.952680	517530.700628	48.608884
3503.309266	517527.711347	48.613889
3503.360595	517527.197559	48.618893
3503.419719	517522.788829	48.623898
3503.473260	517533.804113	48.628903
3503.251266	517536.772122	48.633908
3503.601535	517528.474239	48.638913
3503.361871	517533.518314	48.643917
3503.536632	517522.972624	48.648922
3503.459302	517494.818637	48.653927
3503.020536	517487.454524	48.658932
3503.400778	517483.450141	48.663937
3503.421544	517488.402501	48.668941
3503.106972	517493.913537	48.673946
3503.380719	517492.960053	48.678951
3503.107226	517498.919704	48.683956
3503.403466	517481.932685	48.688961
3503.016880	517489.224977	48.693965
3503.035722	517493.924800	48.698970
3503.082430	517487.748152	48.703975
3503.211941	517498.903156	48.708980
3503.135814	517498.055537	48.713985
3503.334527	517482.246990	48.718989
3503.414354	517454.068095	48.723994
3503.417076	517449.314285	48.728999
3503.289501	517452.014546	48.734004
3503.211865	517454.403507	48.739009
3502.911417	517449.596477	48.744013
3503.291485	517446.805742	48.749018
3503.457161	517452.240889	48.754023
3503.291808	517439.675618	48.759028
3503.332218	517451.906662	48.764033
3503.196980	517464.317161	48.769037
3503.079231	517441.681365	48.774042
3503.398541	517437.231491	48.779047
3503.255543	517425.623466	48.784052
3503.595417	517413.130029	48.789057
3503.053224	517423.481021	48.794061
3503.439524	517416.947267	48.799066
3503.386737	517417.461290	48.804071
3503.155976	517421.998312	48.809076
3503.305467	517419.345151	48.814081
3503.278119	517427.541484	48.819085
3503.361855	517425.100988	48.824090
3503.597469	517418.287642	48.829095
3502.936997	517391.287571	48.834100
3503.574835	517380.719171	48.839105
3503.349013	517377.771344	48.844109
3503.190820	517375.571350	48.849114
3503.092199	517376.193755	48.854119
3503.145469	517383.821118	48.859124
3503.112613	517378.516662	48.864129
3503.076707	517395.563778	48.869133
3503.321394	517391.783070	48.874138
3503.203259	517389.677883	48.879143
3503.434227	517384.837413	48.884148
3503.694804	517372.811590	48.889153
3503.385370	517361.988348	48.894157
3503.127578	517348.274549	48.899162
3503.620659	517347.438096	48.904167
3503.669812	517351.172374	48.909172
3503.717633	517338.876743	48.914177
3503.947051	517323.720580	48.919181
3503.756572	517305.849510	48.924186
3503.892229	517304.209883	48.929191
3503.592448	517291.109494	48.934196
3503.834559	517264.320542	48.939201
3503.690599	517260.500093	48.944205
3503.701842	517257.717051	48.949210
3503.681875	517251.247442	48.954215
3503.291117	517229.716443	48.959220
3503.334798	517215.145790	48.964225
3503.460672	517218.513992	48.969229
3503.335550	517209.583126	48.974234
3503.562282	517200.394370	48.979239
3503.416840	517208.002652	48.984244
3503.722545	517191.873507	48.989249
3503.070974	517177.665548	48.994253
3503.177188	517174.412364	48.999258
3503.312958	517176.717067	49.004263
3503.154772	517173.556239	49.009268
3503.732187	517168.104694	49.014273
3503.722412	517170.887520	49.019277
3503.671007	517151.578378	49.024282
3503.774895	517138.869188	49.029287
3503.422857	517131.491208	49.034292
3503.559609	517114.579590	49.039297
3503.683537	517119.313480	49.044301
3503.398715	517109.194146	49.049306
3503.633023	517101.824619	49.054311
3503.270793	517083.929885	49.059316
3503.554339	517077.311101	49.064321
3503.615200	517078.818553	49.069325
3503.628820	517078.765831	49.074330
3503.783521	517048.905637	49.079335
3503.480773	517042.834624	49.084340
3503.687700	517031.676709	49.089345
3503.191378	517029.833525	49.094349
3503.507107	517030.491593	49.099354
3503.401610	517019.686463	49.104359
3503.433959	516993.789904	49.109364
3503.300939	516986.377243	49.114369
3503.405965	516997.587024	49.119373
3503.498390	516990.846704	49.124378
3503.263528	516998.115229	49.129383
3503.374147	516995.468145	49.134388
3503.820081	516986.598611	49.139393
3503.217188	516973.040183	49.144397
3503.391805	516953.846797	49.149402
3503.483657	516950.191283	49.154407
3503.533916	516935.467637	49.159412
3503.567393	516945.222247	49.164417
3503.304487	516940.206857	49.169421
3503.326842	516932.617907	49.174426
3503.429805	516915.610288	49.179431
3503.248455	516912.402501	49.184436
3503.726066	516906.511520	49.189441
3503.492661	516909.987138	49.194445
3503.565511	516905.677214	49.199450
3503.463334	516902.507483	49.204455
3503.373142	516883.709854	49.209460
3503.723363	516862.819812	49.214465
3503.513764	516864.420599	49.219469
3503.409127	516851.996994	49.224474
3503.662355	516854.586597	49.229479
3503.256582	516852.324523	49.234484
3503.367495	516828.336937	49.239489
3503.469018	516816.993259	49.244493
3503.272990	516814.495750	49.249498
3503.391907	516815.741202	49.254503
3503.585148	516810.754818	49.259508
3503.141633	516801.722344	49.264513
3502.874030	516818.705532	49.269517
3502.990381	516813.073894	49.274522
3503.405589	516816.244739	49.279527
3502.983279	516819.092825	49.284532
3503.377054	516807.247821	49.289537
3503.107709	516814.521877	49.294541
3503.100578	516825.648361	49.299546
3502.985407	516827.284797	49.304551
3502.884285	516825.682546	49.309556
3503.010780	516823.993752	49.314561
3503.128222	516815.125475	49.319565
3502.685599	516810.441868	49.324570
3503.136259	516806.122776	49.329575
3503.176169	516798.530990	49.334580
3503.329646	516802.501753	49.339585
3502.867972	516819.717892	49.344589
3503.259715	516814.750707	49.349594
3502.992823	516817.675368	49.354599
3503.169829	516812.590411	49.359604
3503.253210	516791.691883	49.364609
3503.269384	516788.402284	49.369613
3503.151153	516781.695173	49.374618
3503.193802	516771.220457	49.379623
3502.796029	516775.834620	49.384628
3502.860848	516773.245309	49.389633
3502.967688	516784.556087	49.394637
3503.324385	516791.528928	49.399642
3503.398911	516783.729385	49.404647
3503.065874	516774.477155	49.409652
3503.105690	516786.658214	49.414657
3503.467312	516779.521272	49.419661
3503.294973	516775.958046	49.424666
3503.176898	516774.712459	49.429671
3503.309026	516778.737172	49.434676
3503.125355	516769.865892	49.439681
3503.361414	516781.055109	49.444685
3503.336737	516770.641603	49.449690
3502.960463	516774.342109	49.454695
3502.882898	516780.422761	49.459700
3503.344296	516772.814918	49.464705
3503.142096	516774.920243	49.469709
3503.031483	516777.567363	49.474714
3503.494106	516773.802640	49.479719
3503.420753	516756.721585	49.484724
3503.311828	516745.411119	49.489729
3503.124783	516739.119427	49.494733
3503.338854	516732.966616	49.499738
3503.253518	516728.024237	49.504743
3503.086084	516743.626278	49.509748
3503.311809	516730.897519	49.514753
3503.079977	516734.524635	49.519757
3503.087236	516742.210136	49.524762
3503.399096	516736.699282	49.529767
3503.201797	516748.159294	49.534772
3503.496332	516738.504437	49.539777
3503.353080	516745.960874	49.544781
3503.012182	516711.576529	49.549786
3503.058264	516699.381840	49.554791
3502.821855	516698.862933	49.559796
3503.416143	516698.870147	49.564801
3503.295549	516702.075128	49.569805
3503.348284	516703.229907	49.574810
3503.435333	516703.367860	49.579815
3503.089914	516699.579121	49.584820
3503.240011	516686.508291	49.589825
3503.287392	516698.941069	49.594829
3503.150727	516698.001836	49.599834
3503.195515	516694.100854	49.604839
3503.330645	516699.591647	49.609844
3503.270383	516698.134636	49.614849
3503.356913	516697.160128	49.619853
3503.313798	516689.985976	49.624858
3503.204000	516660.369168	49.629863
3503.391291	516649.517522	49.634868
3503.252039	516653.130024	49.639873
3503.257836	516653.533671	49.644877
3503.462733	516644.499770	49.649882
3503.324127	516664.547518	49.654887
3502.976296	516656.814668	49.659892
3503.295682	516646.548987	49.664897
3503.336636	516637.692705	49.669901
3503.442694	516644.806361	49.674906
3503.114668	516624.478349	49.679911
3503.503786	516604.492101	49.684916
3503.540815	516599.682055	49.689921
3503.270039	516612.923739	49.694925
3503.236029	516613.485390	49.699930
3503.277164	516609.736677	49.704935
3503.051684	516605.322115	49.709940
3503.363319	516607.750814	49.714945
3503.379202	516612.501925	49.719949
3503.102956	516601.420087	49.724954
3503.196387	516604.237267	49.729959
3503.551047	516605.748898	49.734964
3503.171284	516577.691723	49.739969
3503.214110	516575.813845	49.744973
3503.325490	516572.964292	49.749978
3503.755544	516567.889837	49.754983
3503.277547	516566.144844	49.759988
3503.179149	516563.581297	49.764993
3503.266934	516571.153008	49.769997
3503.029942	516580.697727	49.775002
3503.190976	516577.334621	49.780007
3503.269753	516580.508115	49.785012
3503.298429	516573.474278	49.790017
3503.237809	516551.030519	49.795021
3503.000427	516539.639074	49.800026
3503.332185	516529.624218	49.805031
3503.064743	516534.015566	49.810036
3503.128041	516524.548844	49.815041
3503.112653	516530.771471	49.820045
3503.114912	516530.518261	49.825050
3503.279621	516531.402502	49.830055
3503.282316	516531.756071	49.835060
3503.481848	516531.168258	49.840065
3503.315476	516532.812815	49.845069
3503.290598	516529.984790	49.850074
3503.312306	516526.542552	49.855079
3503.079033	516534.569589	49.860084
3503.420497	516524.098060	49.865089
3503.384663	516516.973254	49.870093
3503.302418	516494.684549	49.875098
3503.496572	516491.164479	49.880103
3503.168710	516489.901457	49.885108
3503.301163	516471.270456	49.890113
3503.261169	516489.128282	49.895117
3503.177031	516485.854478	49.900122
3503.523460	516482.108056	49.905127
3503.309599	516484.468115	49.910132
3503.719100	516474.440939	49.915137
3503.578614	516452.060240	49.920141
3503.337619	516432.527372	49.925146
3503.262460	516437.495206	49.930151
3502.987891	516437.488031	49.935156
3503.095438	516445.511816	49.940161
3503.398613	516448.093588	49.945165
3503.272091	516442.550782	49.950170
3503.512773	516438.821063	49.955175
3503.255442	516439.923725	49.960180
3503.425429	516422.045301	49.965185
3503.326376	516410.025052	49.970189
3503.346526	516403.245346	49.975194
3503.608466	516392.634590	49.980199
3503.068037	516408.548752	49.985204
3503.462052	516402.670806	49.990209
3503.225627	516395.527080	49.995213
3503.206727	516393.456653	50.000218
3503.275769	516392.383748	50.005223
3503.151398	516397.511086	50.010228
3503.237899	516385.815490	50.015233
3503.256319	516364.876121	50.020237
3503.369894	516351.102803	50.025242
3503.468842	516339.860349	50.030247
3503.153695	516360.492648	50.035252
3503.229508	516352.642129	50.040257
3503.325278	516347.165300	50.045261
3503.125668	516347.247420	50.050266
3503.341482	516344.785892	50.055271
3503.175384	516352.347258	50.060276
3503.486700	516353.360051	50.065281
3503.608146	516351.722578	50.070285
3503.467497	516324.840894	50.075290
3503.491215	516310.120889	50.080295
3503.009582	516315.153003	50.085300
3503.346436	516309.132345	50.090305
3503.304849	516315.156908	50.095309
3503.103387	516311.395899	50.100314
3503.642733	516308.529232	50.105319
3503.108418	516320.245088	50.110324
3503.228949	516307.330347	50.115329
3503.335653	516279.903783	50.120333
3503.346590	516272.518622	50.125338
3503.404741	516273.065718	50.130343
3503.047339	516280.151638	50.135348
3503.287148	516273.944020	50.140353
3503.404258	516266.845505	50.145357
3503.235971	516259.994380	50.150362
3503.569549	516262.419662	50.155367
3503.358519	516277.270457	50.160372
3503.063485	516275.344801	50.165377
3503.162736	516273.457971	50.170381
3502.833295	516257.175448	50.175386
3503.211364	516255.193978	50.180391
3503.245838	516266.921118	50.185396
3503.082888	516264.013726	50.190401
3503.341881	516241.721322	50.195405
3502.964071	516239.201885	50.200410
3503.488288	516222.531551	50.205415
3503.231289	516236.428787	50.210420
3503.440697	516224.359652	50.215425
3503.282844	516233.993204	50.220429
3503.331294	516222.960939	50.225434
3503.578363	516241.532235	50.230439
3503.301975	516237.631336	50.235444
3503.266817	516221.251695	50.240449
3503.444238	516190.526652	50.245453
3503.092622	516184.412474	50.250458
3503.296358	516190.752312	50.255463
3503.112397	516183.903633	50.260468
3503.462765	516182.735680	50.265473
3503.251647	516178.723307	50.270477
3503.155271	516174.996230	50.275482
3503.495815	516172.565535	50.280487
3503.337422	516185.233507	50.285492
3503.270514	516182.766067	50.290497
3503.336701	516185.385337	50.295501
3503.203406	516163.508831	50.300506
3503.315628	516136.586877	50.305511
3503.209358	516143.734306	50.310516
3503.098943	516144.813767	50.315521
3503.268596	516142.005501	50.320525
3503.109284	516132.320881	50.325530
3503.402427	516142.186638	50.330535
3503.291822	516145.137287	50.335540
3503.532979	516132.456205	50.340545
3503.354288	516158.781810	50.345549
3503.036900	516134.051767	50.350554
3503.303586	516144.427424	50.355559
3502.926871	516141.199793	50.360564
3503.379961	516112.302195	50.365569
3503.235026	516109.644788	50.370573
3503.225741	516094.272373	50.375578
3503.289482	516100.280367	50.380583
3503.078743	516097.279355	50.385588
3503.058129	516094.956302	50.390593
3503.212076	516100.747750	50.395597
3503.309035	516097.900395	50.400602
3503.224567	516097.660886	50.405607
3503.200623	516100.698990	50.410612
3503.261085	516089.513021	50.415617
3503.100423	516098.337944	50.420621
3502.993908	516095.725035	50.425626
3503.278104	516103.316489	50.430631
3503.062724	516100.063351	50.435636
3502.977256	516095.323092	50.440641
3503.284359	516090.369070	50.445645
3503.159934	516098.429685	50.450650
3503.628196	516099.417689	50.455655
3503.259444	516086.023815	50.460660
3503.128233	516080.936777	50.465665
3503.307250	516057.291321	50.470669
3502.945735	516064.276837	50.475674
3503.274746	516072.670376	50.480679
3503.296918	516072.009436	50.485684
3503.297159	516060.883538	50.490689
3503.125291	516080.987817	50.495693
3503.124397	516078.863933	50.500698
3503.415750	516065.163425	50.505703
3503.018863	516069.069632	50.510708
3503.413938	516077.098722	50.515713
3503.391277	516090.857899	50.520717
3503.134401	516064.044735	50.525722
3503.418156	516058.689817	50.530727
3503.021345	516048.233530	50.535732
3503.362904	515996.140727	50.540737
3503.341693	515991.238565	50.545741
3503.487503	515911.209918	50.550746
3503.215859	515864.978893	50.555751
3502.983887	515808.980907	50.560756
3503.424734	515715.047717	50.565761
3502.998961	515631.011638	50.570765
3502.859986	515527.509508	50.575770
3502.872829	515420.037966	50.580775
3502.759184	515309.500687	50.585780
3502.512416	515173.342314	50.590785
3502.231916	515057.266510	50.595789
3502.164330	514895.941692	50.600794
3502.342965	514740.847843	50.605799
3501.922305	514573.405437	50.610804
3501.732667	514401.979829	50.615809
3501.672823	514228.610005	50.620813
3501.187371	514038.716012	50.625818
3501.155924	513847.331909	50.630823
3500.927899	513632.760752	50.635828
3500.333107	513422.695874	50.640833
3499.857482	513215.391480	50.645837
3499.788585	512996.538291	50.650842
3499.309089	512764.393507	50.655847
3499.023795	512533.074745	50.660852
3498.576302	512296.770695	50.665857
3498.253672	512043.194409	50.670861
3498.286194	511800.484543	50.675866
3498.171134	511531.591148	50.680871
3497.477094	511258.232219	50.685876
3497.282050	510992.125192	50.690881
3496.876943	510705.862536	50.695885
3496.385802	510417.939234	50.700890
3495.938762	510131.268852	50.705895
3495.404908	509848.553458	50.710900
3495.223242	509530.211831	50.715905
3494.656720	509229.885482	50.720909
3493.844305	508910.519007	50.725914
3493.773609	508613.999215	50.730919
3493.718338	508285.242688	50.735924
3493.162612	507967.943150	50.740929
3492.427948	507629.567020	50.745933
3492.026358	507297.810585	50.750938
3491.842441	506961.054665	50.755943
3491.004218	506637.146862	50.760948
3490.568500	506273.852305	50.765953
3490.030289	505930.048214	50.770957
3489.458627	505585.331764	50.775962
3489.107165	505217.852394	50.780967
3488.681609	504866.722519	50.785972
3488.253774	504509.867445	50.790977
3487.563764	504142.520211	50.795981
3487.217420	503768.886131	50.800986
3486.729135	503387.776335	50.805991
3486.058069	503023.085022	50.810996
3485.731169	502640.263406	50.816001
3485.126801	502256.515711	50.821005
3484.372488	501859.067028	50.826010
3483.855614	501476.351497	50.831015
3483.335044	501085.630959	50.836020
3482.840845	500696.112488	50.841025
3482.558027	500300.022328	50.846029
3481.971138	499902.807199	50.851034
3481.310800	499489.953088	50.856039
3480.657979	499081.542998	50.861044
3480.095156	498671.945066	50.866049
3479.730222	498259.117213	50.871053
3478.558672	497850.406799	50.876058
3478.283216	497436.229720	50.881063
3477.624367	497023.065687	50.886068
3477.061972	496610.636423	50.891073
3476.397027	496187.733618	50.896077
3475.858070	495765.763063	50.901082
3475.477484	495345.985529	50.906087
3474.416470	494922.761566	50.911092
3474.024095	494496.485322	50.916097
3473.488373	494063.942996	50.921101
3472.628062	493647.797533	50.926106
3472.069591	493216.504804	50.931111
3471.333506	492792.572767	50.936116
3470.893366	492360.836243	50.941121
3470.135811	491925.139144	50.946125
3469.047236	491498.194708	50.951130
3468.917932	491060.149743	50.956135
3467.908731	490637.984217	50.961140
3467.527903	490194.590310	50.966145
3466.850184	489767.743923	50.971149
3466.178920	489340.937451	50.976154
3465.264357	488900.129746	50.981159
3464.623454	488467.220675	50.986164
3464.522998	488038.977549	50.991169
3463.937203	487593.478016	50.996173
3462.890327	487164.554263	51.001178
3462.538650	486708.055565	51.006183
3461.602520	486287.959273	51.011188
3460.568448	485836.511929	51.016193
3460.188748	485401.921309	51.021197
3459.325313	484969.828992	51.026202
3458.679068	484518.187952	51.031207
3458.008646	484089.895612	51.036212
3457.524666	483652.242156	51.041217
3456.945692	483213.580505	51.046221
3455.823318	482789.991962	51.051226
3455.490692	482334.754353	51.056231
3454.547461	481906.862186	51.061236
3453.838713	481473.400588	51.066241
3453.389501	481035.327991	51.071245
3452.543342	480593.305272	51.076250
3451.996505	480151.579986	51.081255
3451.225213	479723.359535	51.086260
3450.624867	479279.494827	51.091265
3450.127666	478842.647833	51.096269
3449.198474	478412.244827	51.101274
3448.912663	477963.030428	51.106279
3447.938959	477529.523933	51.111284
3447.031664	477088.446082	51.116289
3446.701889	476649.851963	51.121293
3445.494184	476212.400672	51.126298
3445.310261	475776.551936	51.131303
3444.303772	475349.744360	51.136308
3443.701855	474898.534408	51.141313
3443.096393	474467.893989	51.146317
3442.152934	474028.528741	51.151322
3441.539449	473588.544225	51.156327
3440.848833	473153.732816	51.161332
3440.282866	472735.113748	51.166337
3439.670288	472299.156564	51.171341
3438.808061	471860.492091	51.176346
3438.239448	471418.375261	51.181351
3437.361306	471000.682600	51.186356
3436.925614	470560.959736	51.191361
3436.193131	470131.109849	51.196365
3434.678095	469700.411456	51.201370
3434.486639	469257.377536	51.206375
3433.850675	468844.267468	51.211380
3433.339283	468404.105227	51.216385
3432.687920	467981.752695	51.221389
3431.891449	467555.256825	51.226394
3431.042907	467117.808154	51.231399
3430.050542	466698.323182	51.236404
3429.892123	466260.950426	51.241409
3429.077400	465841.268204	51.246413
3428.076681	465426.880844	51.251418
3427.614139	464983.951741	51.256423
3427.088253	464563.285783	51.261428
3426.256434	464132.213110	51.266433
3425.528719	463716.481476	51.271437
3424.607598	463290.071583	51.276442
3423.985265	462870.351142	51.281447
3422.990285	462458.745342	51.286452
3422.440902	462048.734910	51.291457
3422.073136	461611.908656	51.296461
3421.034890	461207.995066	51.301466
3420.682898	460782.713629	51.306471
3419.639672	460368.336810	51.311476
3419.291918	459955.313112	51.316481
3418.350646	459524.419391	51.321485
3417.572135	459117.737669	51.326490
3416.954794	458694.334337	51.331495
3415.940655	458284.986017	51.336500
3415.697267	457863.181554	51.341505
3415.323990	457444.889818	51.346509
3414.322254	457042.719920	51.351514
3413.777567	456612.721183	51.356519
3412.997110	456203.043799	51.361524
3412.182173	455795.951669	51.366529
3411.636707	455382.975253	51.371533
3410.789178	454964.864142	51.376538
3409.778460	454551.387904	51.381543
3408.930343	454152.540952	51.386548
3408.441709	453742.062200	51.391553
3408.014685	453329.029390	51.396557
3406.915381	452928.982878	51.401562
3406.396596	452520.871488	51.406567
3405.477472	452120.528578	51.411572
3405.147109	451706.892901	51.416577
3404.252695	451307.089990	51.421581
3403.668447	450902.664221	51.426586
3403.290503	450494.392944	51.431591
3402.157835	450101.964581	51.436596
3401.819454	449698.290720	51.441601
3400.901912	449294.041686	51.446605
3399.921700	448893.347823	51.451610
3399.331782	448493.448069	51.456615
3398.602732	448087.372080	51.461620
3397.990705	447686.193270	51.466625
3397.170362	447298.895465	51.471629
3396.622801	446901.905354	51.476634
3396.093741	446504.093584	51.481639
3395.032210	446109.658254	51.486644
3394.227030	445720.301974	51.491649
3394.007754	445315.569432	51.496653
3393.179733	444933.005008	51.501658
3392.401394	444533.372367	51.506663
3391.394485	444133.413871	51.511668
3390.982965	443746.703985	51.516673
3390.546934	443360.448572	51.521677
3389.319656	442973.702935	51.526682
3389.135654	442569.324445	51.531687
3388.002123	442186.053848	51.536692
3387.378626	441789.092225	51.541697
3387.095182	441404.456567	51.546701
3386.330741	441016.743510	51.551706
3385.600674	440632.623155	51.556711
3385.079915	440239.427390	51.561716
3384.069111	439846.759693	51.566721
3383.285900	439447.043851	51.571725
3382.507094	439069.760304	51.576730
3382.173622	438690.115980	51.581735
3381.461792	438302.453286	51.586740
3380.676527	437913.476111	51.591745
3380.236412	437518.954986	51.596749
3379.226345	437139.800100	51.601754
3378.397314	436755.178149	51.606759
3377.913875	436373.821312	51.611764
3377.659505	435989.477552	51.616769
3376.909876	435604.749252	51.621773
3375.625918	435214.336504	51.626778
3374.988582	434823.307719	51.631783
3374.318583	434457.108219	51.636788
3373.515478	434071.857294	51.641793
3372.859246	433696.199921	51.646797
3372.259548	433314.586861	51.651802
3371.760621	432939.045825	51.656807
3371.151407	432563.008917	51.661812
3370.575285	432178.582263	51.666817
3370.188485	431800.772468	51.671821
3369.113909	431415.803871	51.676826
3368.497730	431026.948258	51.681831
3367.492888	430652.088735	51.686836
3366.758157	430268.953829	51.691841
3366.075937	429891.645428	51.696845
3365.340030	429512.207015	51.701850
3364.920841	429140.508966	51.706855
3364.005749	428768.223822	51.711860
3363.573564	428397.888631	51.716865
3362.734173	428016.540419	51.721869
3362.089586	427648.666242	51.726874
3361.499175	427267.013926	51.731879
3360.562615	426900.115197	51.736884
3359.874666	426522.708785	51.741889
3359.493113	426147.788279	51.746893
3358.753143	425767.636599	51.751898
3358.011523	425396.318131	51.756903
3357.299521	425023.135821	51.761908
3356.651677	424656.465546	51.766913
3355.861361	424286.231641	51.771917
3354.860368	423919.658039	51.776922
3354.400953	423541.335620	51.781927
3353.190340	423181.897020	51.786932
3352.509161	422817.086801	51.791937
3351.976741	422457.074251	51.796941
3351.515024	422106.926625	51.801946
3351.047410	421730.307755	51.806951
3350.045541	421375.257678	51.811956
3349.646649	421003.291868	51.816961
3349.337124	420647.056125	51.821965
3348.206689	420281.953243	51.826970
3347.631763	419907.028561	51.831975
3347.038635	419539.138337	51.836980
3346.300027	419184.272746	51.841985
3345.296335	418808.664487	51.846989
3344.725398	418454.601504	51.851994
3343.961302	418084.636192	51.856999
3343.540206	417740.041748	51.862004
3342.979662	417378.469341	51.867009
3342.164130	417016.907259	51.872013
3341.219657	416661.661547	51.877018
3340.752630	416288.043749	51.882023
3340.238155	415928.147905	51.887028
3339.510233	415568.560783	51.892033
3338.873516	415204.838860	51.897037
3337.982632	414848.749273	51.902042
3337.464131	414472.219694	51.907047
3336.907623	414129.254850	51.912052
3336.103535	413764.347188	51.917057
3335.650831	413398.159805	51.922061
3334.715564	413039.183988	51.927066
3334.055588	412679.143893	51.932071
3333.191205	412320.275139	51.937076
3332.696739	411961.750082	51.942081
3332.066437	411601.031504	51.947085
3331.380018	411246.314225	51.952090
3330.959543	410876.228132	51.957095
3330.131394	410517.509734	51.962100
3329.297601	410152.181037	51.967105
3328.526717	409797.129574	51.972109
3327.564695	409442.129559	51.977114
3327.107701	409086.943855	51.982119
3326.453678	408736.308532	51.987124
3325.885484	408378.285927	51.992129
3325.143255	408017.796163	51.997133
3324.533929	407670.267272	52.002138
3324.050195	407304.416850	52.007143
3323.049973	406961.846541	52.012148
3322.456999	406602.841345	52.017153
3321.801861	406246.993182	52.022157
3320.803189	405889.467051	52.027162
3320.275627	405533.158459	52.032167
3319.597215	405191.737560	52.037172
3319.040008	404839.898803	52.042177
3318.430448	404487.733958	52.047181
3317.489335	404147.359825	52.052186
3317.164379	403783.755662	52.057191
3316.357154	403440.938157	52.062196
3315.843777	403089.733706	52.067201
3314.860385	402730.644099	52.072205
3314.214312	402380.113625	52.077210
3313.710915	402020.762175	52.082215
3312.815666	401670.390398	52.087220
3312.253735	401320.089170	52.092225
3311.495321	400972.916267	52.097229
3310.508077	400630.478307	52.102234
3310.124909	400273.579353	52.107239
3309.524180	399929.623957	52.112244
3308.699705	399578.277745	52.117249
3308.137258	399235.122383	52.122253
3307.060266	398889.019780	52.127258
3306.495895	398551.322905	52.132263
3305.985204	398204.360905	52.137268
3305.215829	397858.071687	52.142273
3304.616605	397518.208945	52.147277
3303.939868	397182.651222	52.152282
3303.511302	396833.907774	52.157287
3302.558841	396493.887044	52.162292
3301.845761	396153.367392	52.167297
3301.167444	395801.271490	52.172301
3300.499626	395464.881581	52.177306
3300.164751	395120.223988	52.182311
3299.331424	394775.463746	52.187316
3298.640579	394439.219810	52.192321
3297.960232	394086.445350	52.197325
3297.161676	393746.550563	52.202330
3296.868894	393394.394111	52.207335
3295.708805	393058.719277	52.212340
3295.111912	392719.850256	52.217345
3294.665802	392376.275827	52.222349
3294.134589	392037.135469	52.227354
3293.216227	391688.569246	52.232359
3292.429604	391354.674884	52.237364
3291.924234	391009.265642	52.242369
3291.482092	390660.969806	52.247373
3290.504245	390320.408669	52.252378
3290.168517	389975.852364	52.257383
3289.563484	389629.784233	52.262388
3288.528902	389282.941551	52.267393
3288.013355	388946.667586	52.272397
3287.238759	388599.675415	52.277402
3286.619652	388262.953684	52.282407
3285.588544	387929.853925	52.287412
3284.972928	387579.012474	52.292417
3284.225923	387238.283653	52.297421
3283.556074	386913.381752	52.302426
3283.246702	386571.916295	52.307431
3282.595364	386235.409626	52.312436
3281.796352	385897.041406	52.317441
3281.218474	385545.309741	52.322445
3280.517861	385214.599537	52.327450
3279.914082	384867.366647	52.332455
3279.257838	384535.804135	52.337460
3278.662084	384187.800680	52.342465
3278.177746	383839.725485	52.347469
3277.020457	383508.360216	52.352474
3276.503697	383151.916796	52.357479
3275.679911	382822.094910	52.362484
3274.910483	382490.811906	52.367489
3274.388206	382150.331258	52.372493
3273.824150	381819.442246	52.377498
3273.226739	381482.222861	52.382503
3272.604906	381137.145549	52.387508
3271.743023	380803.802394	52.392513
3271.358079	380461.911560	52.397517
3270.314553	380120.070987	52.402522
3269.722277	379783.954955	52.407527
3269.097662	379454.504872	52.412532
3268.298176	379111.345097	52.417537
3267.810496	378770.956227	52.422541
3267.017286	378439.158818	52.427546
3266.575929	378095.577407	52.432551
3265.548121	377764.752509	52.437556
3265.387080	377433.100994	52.442561
3264.480595	377078.341834	52.447565
3263.687956	376754.567870	52.452570
3263.151025	376420.601831	52.457575
3262.613563	376079.231122	52.462580
3261.523534	375743.540949	52.467585
3260.908076	375393.986202	52.472589
3260.071353	375069.442531	52.477594
3259.390716	374727.040125	52.482599
3258.982730	374413.208763	52.487604
3258.044012	374081.474576	52.492609
3257.754093	373745.463289	52.497613
3256.734203	373416.051403	52.502618
3256.110440	373077.238418	52.507623
3255.513910	372745.820928	52.512628
3254.844533	372418.635124	52.517633
3254.296614	372082.447646	52.522637
3253.312870	371748.870303	52.527642
3252.776752	371418.195895	52.532647
3252.185972	371087.578416	52.537652
3251.238871	370757.905098	52.542657
3250.892652	370425.106840	52.547661
3250.232158	370102.836967	52.552666
3249.428992	369757.920021	52.557671
3248.506245	369436.246294	52.562676
3247.965078	369102.527293	52.567681
3247.573415	368776.058127	52.572685
3246.615868	368452.805248	52.577690
3246.208519	368118.523240	52.582695
3245.096844	367790.634092	52.587700
3244.725342	367466.492525	52.592705
3244.218279	367131.048441	52.597709
3243.120029	366810.019117	52.602714
3242.680871	366481.632213	52.607719
3242.212767	366159.200955	52.612724
3241.228342	365840.741733	52.617729
3240.810563	365494.508999	52.622733
3239.889654	365172.701992	52.627738
3239.207463	364847.420118	52.632743
3238.435139	364529.834011	52.637748
3237.914579	364206.684642	52.642753
3237.563147	363874.931744	52.647757
3236.748486	363547.600594	52.652762
3236.118569	363210.747295	52.657767
3235.423859	362884.893646	52.662772
3234.562294	362562.957070	52.667777
3233.905751	362235.515267	52.672781
3233.289588	361913.230041	52.677786
3232.866315	361582.337172	52.682791
3232.103294	361262.106282	52.687796
3231.307499	360932.794468	52.692801
3230.553571	360600.700193	52.697805
3229.754403	360282.834806	52.702810
3228.931823	359951.179428	52.707815
3228.646701	359630.200343	52.712820
3227.612274	359304.324766	52.717825
3227.097253	358989.942857	52.722829
3226.178545	358677.633025	52.727834
3225.900495	358356.695248	52.732839
3225.183642	358040.506967	52.737844
3224.229119	357716.796512	52.742849
3223.828428	357389.662753	52.747853
3222.919548	357073.880330	52.752858
3222.155509	356750.260634	52.757863
3221.737114	356431.648217	52.762868
3220.984754	356120.670011	52.767873
3220.453269	355793.393748	52.772877
3219.473129	355485.196004	52.777882
3218.893922	355158.864745	52.782887
3218.398045	354855.981580	52.787892
3217.536662	354535.264137	52.792897
3217.267354	354221.347607	52.797901
3216.478745	353900.920061	52.802906
3215.999000	353579.932682	52.807911
3215.039739	353251.537118	52.812916
3214.525795	352938.796697	52.817921
3213.823760	352616.082521	52.822925
3212.886074	352304.296062	52.827930
3212.576089	351965.508067	52.832935
3211.695671	351656.660886	52.837940
3211.068007	351346.982971	52.842945
3210.517932	351018.915928	52.847949
3209.587786	350700.807188	52.852954
3208.842640	350374.624932	52.857959
3208.326262	350068.154233	52.862964
3207.568104	349749.070993	52.867969
3207.057388	349425.823680	52.872973
3206.066528	349118.913667	52.877978
3205.924041	348790.386871	52.882983
3205.078769	348477.011072	52.887988
3204.306866	348155.426492	52.892993
3203.789139	347839.042889	52.897997
3202.989636	347523.923755	52.903002
3202.580496	347209.759175	52.908007
3201.682602	346895.950131	52.913012
3200.820206	346567.524127	52.918017
3200.130521	346245.202932	52.923021
3199.517770	345944.629680	52.928026
3199.075560	345619.338762	52.933031
3198.476530	345314.407628	52.938036
3197.776188	345003.840352	52.943041
3197.229766	344684.262120	52.948045
3196.315382	344362.042301	52.953050
3195.773211	344044.877957	52.958055
3194.942744	343736.360800	52.963060
3194.300673	343419.641606	52.968065
3194.077825	343097.992728	52.973069
3192.809828	342786.179948	52.978074
3192.378148	342462.040748	52.983079
3191.669187	342142.499969	52.988084
3190.884372	341832.438511	52.993089
3190.454970	341515.599269	52.998093
3189.368778	341196.775011	53.003098
3188.892612	340884.496271	53.008103
3188.240975	340574.127368	53.013108
3187.407546	340266.407532	53.018113
3187.228014	339948.629782	53.023117
3185.834760	339641.708170	53.028122
3185.323184	339317.437756	53.033127
3184.952273	339007.373040	53.038132
3183.998895	338704.628348	53.043137
3183.321221	338388.296154	53.048141
3182.681687	338084.276997	53.053146
3181.982718	337771.178025	53.058151
3181.334866	337469.041027	53.063156
3180.583864	337161.547683	53.068161
3180.507034	336846.054771	53.073165
3179.459552	336541.991115	53.078170
3178.940181	336222.644933	53.083175
3178.353606	335914.203311	53.088180
3177.406409	335607.242896	53.093185
3176.773312	335283.429807	53.098189
3176.332628	334978.117455	53.103194
3175.498732	334664.948756	53.108199
3174.754226	334362.838391	53.113204
3173.810890	334055.132064	53.118209
3173.389388	333741.613862	53.123213
3172.712627	333441.067094	53.128218
3172.324532	333129.348327	53.133223
3171.547956	332822.832115	53.138228
3170.612382	332519.827459	53.143233
3170.132942	332208.882796	53.148237
3169.700187	331903.606557	53.153242
3168.736186	331576.773515	53.158247
3168.046502	331275.023028	53.163252
3166.977925	330974.705983	53.168257
3167.036972	330662.371037	53.173261
3166.019258	330357.613597	53.178266
3165.435518	330049.425665	53.183271
3164.794850	329742.263809	53.188276
3164.209463	329422.693382	53.193281
3163.377201	329122.993319	53.198285
3162.623091	328820.428258	53.203290
3162.042506	328510.018509	53.208295
3161.420431	328203.763945	53.213300
3160.385960	327902.385253	53.218305
3160.108225	327593.375053	53.223309
3159.277459	327289.568523	53.228314
3158.413373	326980.699564	53.233319
3157.989596	326675.171353	53.238324
3157.208512	326379.449686	53.243329
3156.555612	326075.126560	53.248333
3155.449999	325778.079144	53.253338
3155.101859	325473.501820	53.258343
3154.799321	325169.909084	53.263348
3154.070563	324872.595013	53.268353
3153.483697	324561.686892	53.273357
3152.755560	324262.817402	53.278362
3152.004421	323955.879388	53.283367
3151.302656	323652.420570	53.288372
3150.803541	323349.361422	53.293377
3150.137098	323044.163460	53.298381
3149.467583	322737.946433	53.303386
3149.161609	322425.076312	53.308391
3148.355570	322114.881227	53.313396
3146.988847	321812.106634	53.318401
3146.552402	321498.719098	53.323405
3145.818755	321212.697797	53.328410
3145.408814	320909.030299	53.333415
3144.640094	320601.675636	53.338420
3144.153818	320296.897798	53.343425
3143.636849	319991.283533	53.348429
3142.626008	319682.156220	53.353434
3142.089528	319371.399607	53.358439
3141.497993	319074.629420	53.363444
3140.682230	318769.796734	53.368449
3140.125707	318463.547057	53.373453
3139.422138	318167.377323	53.378458
3138.599968	317855.234926	53.383463
3137.934323	317559.693846	53.388468
3137.572367	317261.022807	53.393473
3137.107968	316947.776855	53.398477
3135.926856	316645.515945	53.403482
3135.241719	316334.721913	53.408487
3134.669975	316036.436776	53.413492
3133.590229	315740.955672	53.418497
3133.460557	315440.052480	53.423501
3132.514529	315144.599378	53.428506
3131.950991	314842.744516	53.433511
3131.286508	314539.835265	53.438516
3130.348892	314231.035338	53.443521
3129.967415	313932.331924	53.448525
3129.066118	313648.682530	53.453530
3128.541907	313339.661762	53.458535
3128.003140	313044.494699	53.463540
3127.013654	312746.800820	53.468545
3126.422542	312445.121633	53.473549
3126.030818	312149.979770	53.478554
3125.205269	311853.861724	53.483559
3124.665339	311559.225535	53.488564
3123.683039	311258.267040	53.493569
3123.263630	310955.232453	53.498573
3122.526924	310662.127424	53.503578
3121.707433	310358.135967	53.508583
3121.119818	310054.998270	53.513588
3120.098522	309767.105269	53.518593
3119.789841	309464.838615	53.523597
3118.958083	309177.576251	53.528602
3118.377502	308883.372501	53.533607
3117.606048	308592.483187	53.538612
3116.931518	308300.533775	53.543617
3116.426592	307993.328799	53.548621
3115.377551	307711.572277	53.553626
3115.064428	307417.959280	53.558631
3114.560071	307121.269109	53.563636
3113.758728	306832.799550	53.568641
3113.053889	306528.754814	53.573645
3112.654361	306244.905945	53.578650
3111.777487	305947.839080	53.583655
3111.115898	305653.385874	53.588660
3110.532495	305358.486726	53.593665
3109.853136	305055.631404	53.598669
3108.880652	304769.679987	53.603674
3108.517138	304471.051590	53.608679
3107.839845	304173.923737	53.613684
3107.048372	303874.368604	53.618689
3106.534177	303585.082594	53.623693
3105.432968	303299.224905	53.628698
3105.092593	303007.210834	53.633703
3104.258098	302712.294846	53.638708
3103.303948	302420.733240	53.643713
3102.686301	302130.467507	53.648717
3102.190843	301841.225983	53.653722
3101.654957	301557.083525	53.658727
3101.468772	301254.855142	53.663732
3100.225535	300975.407447	53.668737
3099.858606	300684.539020	53.673741
3099.289726	300389.831130	53.678746
3098.326535	300091.848994	53.683751
3097.723295	299794.318674	53.688756
3096.710413	299520.536444	53.693761
3096.559777	299219.368152	53.698765
3095.613930	298934.267213	53.703770
3094.786940	298641.354204	53.708775
3094.362209	298351.025568	53.713780
3093.818367	298065.757694	53.718785
3092.960749	297776.999132	53.723789
3091.830778	297492.663480	53.728794
3091.791314	297202.271977	53.733799
3090.711403	296912.146522	53.738804
3089.796871	296634.575079	53.743809
3089.494750	296343.383374	53.748813
3088.923973	296057.327125	53.753818
3088.438563	295773.803638	53.758823
3087.709760	295480.487975	53.763828
3086.915254	295199.661138	53.768833
3086.163208	294906.246432	53.773837
3085.485272	294628.634670	53.778842
3085.027816	294334.332104	53.783847
3084.245197	294050.038259	53.788852
3083.491846	293766.834491	53.793857
3083.221086	293476.117531	53.798861
3082.544908	293195.243789	53.803866
3081.809672	292896.602823	53.808871
3080.958591	292602.512986	53.813876
3080.184263	292316.432859	53.818881
3079.827326	292020.659631	53.823885
3078.770934	291749.980318	53.828890
3078.412800	291452.245574	53.833895
3077.682699	291166.691879	53.838900
3076.879394	290894.901925	53.843905
3076.512002	290595.435820	53.848909
3075.915844	290311.999237	53.853914
3075.040101	290011.823406	53.858919
3074.445584	289725.915570	53.863924
3073.645031	289441.797309	53.868929
3072.774538	289152.621746	53.873933
3071.933976	288876.149561	53.878938
3071.078139	288592.548548	53.883943
3070.925876	288307.205978	53.888948
3069.980397	288035.792230	53.893953
3069.734381	287741.728495	53.898957
3068.895855	287463.471933	53.903962
3068.406416	287179.913495	53.908967
3067.964364	286893.953327	53.913972
3067.010101	286603.718955	53.918977
3066.330724	286312.727731	53.923981
3065.640639	286030.397076	53.928986
3065.316591	285747.346103	53.933991
3064.550596	285457.030061	53.938996
3063.574166	285172.044453	53.944001
3063.102989	284878.523278	53.949005
3062.386642	284596.908814	53.954010
3061.563522	284307.390476	53.959015
3061.173884	284022.183854	53.964020
3060.297939	283738.913180	53.969025
3059.460216	283446.314937	53.974029
3058.715443	283179.424645	53.979034
3058.142543	282892.463548	53.984039
3057.502261	282611.090482	53.989044
3056.756288	282335.948232	53.994049
3056.238736	282058.503017	53.999053
3055.450379	281781.991909	54.004058
3054.842226	281500.536776	54.009063
3054.041604	281205.410049	54.014068
3053.446873	280925.709837	54.019073
3052.712745	280633.297425	54.024077
3052.012213	280349.284107	54.029082
3051.567741	280067.751514	54.034087
3050.790422	279784.666989	54.039092
3049.789588	279514.148150	54.044097
3049.308575	279226.814265	54.049101
3048.562675	278952.918552	54.054106
3047.938579	278682.441710	54.059111
3047.097402	278405.326444	54.064116
3046.643423	278124.991753	54.069121
3046.152325	277844.764742	54.074125
3045.381025	277572.808297	54.079130
3044.822773	277284.594730	54.084135
3043.832666	277012.418128	54.089140
3043.337554	276737.667241	54.094145
3042.891960	276459.164626	54.099149
3042.160621	276184.094495	54.104154
3041.474412	275904.356479	54.109159
3040.631218	275628.489011	54.114164
3040.215594	275358.207836	54.119169
3039.489831	275070.937380	54.124173
3038.647455	274802.684792	54.129178
3037.968399	274522.869171	54.134183
3037.501669	274246.789269	54.139188
3036.415813	273972.844835	54.144193
3036.313498	273688.913950	54.149197
3035.664022	273416.021089	54.154202
3034.537727	273133.372921	54.159207
3033.953090	272862.532788	54.164212
3033.179847	272591.773474	54.169217
3033.118999	272316.291670	54.174221
3032.364340	272046.395419	54.179226
3031.532548	271762.198200	54.184231
3030.968526	271489.164737	54.189236
3029.884347	271210.890771	54.194241
3029.367698	270931.049881	54.199245
3028.632538	270657.508860	54.204250
3028.146378	270381.305262	54.209255
3027.559459	270103.895212	54.214260
3026.776017	269826.592756	54.219265
3026.430088	269551.717039	54.224269
3025.631074	269276.582039	54.229274
3024.876363	268994.869307	54.234279
3024.508872	268713.579295	54.239284
3023.378943	268450.492546	54.244289
3022.932903	268163.994199	54.249293
3021.890515	267896.309534	54.254298
3021.743924	267613.304134	54.259303
3021.025463	267341.035103	54.264308
3019.961892	267061.333172	54.269313
3019.366366	266781.277156	54.274317
3018.754064	266516.555794	54.279322
3017.977863	266237.216313	54.284327
3017.573125	265953.132057	54.289332
3016.882686	265693.313397	54.294337
3016.318150	265415.519926	54.299341
3015.523049	265137.100952	54.304346
3014.789926	264860.633392	54.309351
3014.004255	264585.600545	54.314356
3013.373013	264319.992091	54.319361
3012.924939	264034.133197	54.324365
3011.935657	263769.371297	54.329370
3011.421774	263502.522365	54.334375
3010.884567	263225.617464	54.339380
3009.885532	262952.962622	54.344385
3009.418993	262680.605728	54.349389
3008.553779	262412.030471	54.354394
3007.942292	262139.875231	54.359399
3007.245656	261864.957695	54.364404
3006.372074	261603.413563	54.369409
3006.123406	261333.264477	54.374413
3005.496902	261063.710258	54.379418
3004.940944	260795.724117	54.384423
3004.186991	260513.736816	54.389428
3003.528714	260245.054278	54.394433
3002.798377	259965.763359	54.399437
3002.013756	259707.568567	54.404442
3001.344164	259437.768019	54.409447
3000.932421	259160.006490	54.414452
2999.884296	258886.217062	54.419457
2999.390801	258622.629040	54.424461
2998.834675	258347.387058	54.429466
2997.715049	258072.260041	54.434471
2997.487496	257807.994091	54.439476
2996.560391	257546.971659	54.444481
2995.827138	257275.961053	54.449485
2995.139496	257015.920000	54.454490
2994.476696	256750.399816	54.459495
2994.006070	256481.207688	54.464500
2993.249254	256214.404178	54.469505
2992.764206	255941.853294	54.474509
2992.009481	255677.571367	54.479514
2991.084777	255415.506852	54.484519
2991.118445	255143.842624	54.489524
2989.823211	254878.322953	54.494529
2989.390546	254600.824864	54.499533
2988.432866	254345.261038	54.504538
2987.872243	254077.563292	54.509543
2987.308753	253811.063310	54.514548
2986.418587	253552.841244	54.519553
2985.792303	253281.258525	54.524557
2985.404155	253020.818481	54.529562
2984.336499	252758.576339	54.534567
2983.821627	252502.919383	54.539572
2982.665501	252243.620663	54.544577
2982.556949	251969.334814	54.549581
2981.708291	251712.585796	54.554586
2981.044613	251454.840132	54.559591
2980.575344	251189.373132	54.564596
2979.750865	250933.207157	54.569601
2979.077818	250666.983748	54.574605
2978.626507	250413.408005	54.579610
2977.695858	250144.144741	54.584615
2977.212324	249886.449318	54.589620
2976.611929	249624.901896	54.594625
2975.611702	249357.077051	54.599629
2974.901369	249103.264192	54.604634
2974.420744	248840.553093	54.609639
2973.722940	248586.051484	54.614644
2972.789330	248335.840478	54.619649
2972.245522	248078.106575	54.624653
2972.026807	247817.596763	54.629658
2971.004928	247561.212715	54.634663
2970.564774	247304.660618	54.639668
2969.980241	247041.205058	54.644673
2969.469318	246768.341369	54.649677
2968.824963	246507.290035	54.654682
2967.934829	246249.894233	54.659687
2967.497428	245984.150826	54.664692
2966.729576	245724.291890	54.669697
2966.118437	245453.280095	54.674701
2965.424820	245200.719043	54.679706
2964.450638	244930.784362	54.684711
2963.864724	244662.545874	54.689716
2963.353051	244407.258124	54.694721
2962.645041	244139.345583	54.699725
2961.931031	243883.683409	54.704730
2961.212836	243622.394536	54.709735
2960.621532	243359.201658	54.714740
2959.906229	243109.932992	54.719745
2959.227894	242837.434648	54.724749
2958.902819	242578.046463	54.729754
2958.011947	242326.311522	54.734759
2957.328716	242056.209346	54.739764
2956.536790	241796.387368	54.744769
2955.934176	241531.468433	54.749773
2955.200057	241276.094766	54.754778
2954.686192	241024.200917	54.759783
2954.169498	240760.212248	54.764788
2953.333809	240498.668343	54.769793
2952.706021	240235.997115	54.774797
2951.834222	239981.284604	54.779802
2951.398281	239717.234531	54.784807
2950.684409	239444.469251	54.789812
2949.940696	239193.608788	54.794817
2949.250151	238927.741908	54.799821
2948.504106	238665.933265	54.804826
2947.936452	238420.597856	54.809831
2947.367116	238158.278592	54.814836
2946.647087	237897.409792	54.819841
2946.001145	237633.321395	54.824845
2945.324496	237376.062862	54.829850
2944.562260	237113.623824	54.834855
2943.888661	236864.361711	54.839860
2942.971490	236604.774930	54.844865
2943.041708	236338.946607	54.849869
2942.140460	236082.974434	54.854874
2941.379738	235831.513171	54.859879
2940.724669	235566.183563	54.864884
2939.780793	235305.509256	54.869889
2938.997200	235047.763997	54.874893
2938.589759	234797.344232	54.879898
2937.913266	234538.666608	54.884903
2937.486936	234277.174535	54.889908
2936.642668	234028.837417	54.894913
2936.051895	233761.923575	54.899917
2935.359418	233499.762689	54.904922
2934.712717	233250.173998	54.909927
2934.222084	232987.829733	54.914932
2933.147194	232729.143476	54.919937
2932.505111	232467.537546	54.924941
2931.856049	232215.252808	54.929946
2931.450103	231967.029740	54.934951
2930.738880	231706.226168	54.939956
2929.991568	231459.153359	54.944961
2929.577102	231187.304394	54.949965
2928.747444	230930.162852	54.954970
2928.116239	230682.997313	54.959975
2927.559551	230421.230732	54.964980
2926.683565	230158.064096	54.969985
2926.071802	229908.555025	54.974989
2925.121063	229642.728178	54.979994
2924.806625	229390.118005	54.984999
2923.992278	229135.041489	54.990004
2923.192728	228879.606889	54.995009
2922.741030	228624.525337	55.000013
2922.115670	228369.191933	55.005018
2920.935458	228107.709008	55.010023
2920.433530	227847.468938	55.015028
2920.011552	227605.345576	55.020033
2919.342931	227336.196437	55.025037
2918.619452	227081.493408	55.030042
2917.925130	226845.627863	55.035047
2917.386837	226582.545698	55.040052
2916.334614	226336.400979	55.045057
2915.717172	226071.652496	55.050061
2915.033569	225826.507538	55.055066
2914.333302	225572.594658	55.060071
2913.618853	225321.905591	55.065076
2912.920950	225078.916538	55.070081
2912.590424	224829.963161	55.075085
2911.938241	224581.978048	55.080090
2911.545728	224328.033006	55.085095
2910.787976	224073.051787	55.090100
2910.001332	223832.244634	55.095105
2909.622971	223570.101499	55.100109
2908.733540	223311.159014	55.105114
2907.935519	223058.631575	55.110119
2907.557459	222806.127561	55.115124
2906.584367	222558.046756	55.120129
2905.799136	222295.615819	55.125133
2905.091025	222051.797384	55.130138
2904.493170	221795.283326	55.135143
2903.941979	221551.861704	55.140148
2902.970068	221303.300988	55.145153
2902.328233	221053.594063	55.150157
2901.881101	220804.353587	55.155162
2901.074024	220561.217499	55.160167
2900.775397	220301.173159	55.165172
2900.010118	220058.350316	55.170177
2899.260257	219801.625190	55.175181
2898.345534	219558.458479	55.180186
2897.821899	219301.686532	55.185191
2897.575569	219053.769411	55.190196
2896.494906	218810.695086	55.195201
2895.902263	218558.964751	55.200205
2895.054421	218309.630604	55.205210
2894.212902	218064.586059	55.210215
2893.952191	217817.057301	55.215220
2893.023503	217576.852573	55.220225
2892.648097	217317.276488	55.225229
2891.633245	217066.534713	55.230234
2891.070870	216823.792362	55.235239
2890.637824	216579.121026	55.240244
2889.718805	216343.208601	55.245249
2889.302793	216086.596572	55.250253
2888.703723	215845.301777	55.255258
2887.950154	215600.620972	55.260263
2887.500755	215346.104483	55.265268
2886.537374	215105.009971	55.270273
2886.008871	214837.448269	55.275277
2885.392631	214599.520914	55.280282
2884.527602	214348.014250	55.285287
2883.940798	214093.218702	55.290292
2883.023797	213855.596153	55.295297
2882.381189	213607.888293	55.300301
2881.764626	213362.926549	55.305306
2881.063150	213113.091483	55.310311
2880.483883	212868.952993	55.315316
2879.768176	212626.835338	55.320321
2879.411400	212373.766434	55.325325
2878.540546	212139.350221	55.330330
2877.949521	211889.744143	55.335335
2877.582981	211642.661807	55.340340
2876.493827	211397.642212	55.345345
2876.167365	211141.493132	55.350349
2875.203845	210905.174142	55.355354
2874.520060	210653.169236	55.360359
2874.256457	210398.158678	55.365364
2873.234061	210155.335171	55.370369
2872.810325	209910.546835	55.375373
2872.134280	209660.695622	55.380378
2871.283429	209417.478693	55.385383
2870.915451	209165.060616	55.390388
2869.932654	208925.901118	55.395393
2869.554284	208670.343006	55.400397
2869.039854	208421.285724	55.405402
2868.313187	208180.153992	55.410407
2867.675211	207926.205531	55.415412
2866.942956	207682.849369	55.420417
2866.150281	207430.276551	55.425421
2865.596815	207178.672348	55.430426
2864.844196	206932.815174	55.435431
2864.273641	206663.028862	55.440436
2863.441526	206429.938788	55.445441
2862.581582	206178.565473	55.450445
2862.029589	205932.947896	55.455450
2861.096138	205685.902704	55.460455
2860.740642	205440.459680	55.465460
2859.818063	205201.521725	55.470465
2859.482198	204950.274266	55.475469
2858.771768	204697.241842	55.480474
2858.079219	204452.390839	55.485479
2857.541977	204209.654322	55.490484
2856.611851	203974.006018	55.495489
2856.125491	203718.422548	55.500493
2855.411245	203475.615333	55.505498
2854.396306	203232.474974	55.510503
2854.310531	202979.554782	55.515508
2853.139806	202745.133164	55.520513
2852.727336	202492.864997	55.525517
2852.214065	202262.973562	55.530522
2851.306925	202013.980101	55.535527
2850.949838	201759.046716	55.540532
2850.422427	201522.886667	55.545537
2849.563527	201268.836711	55.550541
2848.915391	201019.132199	55.555546
2847.973049	200779.439624	55.560551
2847.588131	200530.802770	55.565556
2846.718069	200281.734839	55.570561
2846.379129	200031.451362	55.575565
2845.895106	199789.412657	55.580570
2844.726852	199538.791921	55.585575
2844.318149	199284.654393	55.590580
2843.327650	199044.315331	55.595585
2842.729722	198799.830371	55.600589
2842.376026	198557.445677	55.605594
2841.257194	198311.340255	55.610599
2840.478218	198064.762221	55.615604
2839.782994	197831.711473	55.620609
2839.122718	197591.682939	55.625613
2838.744634	197348.493207	55.630618
2837.586537	197117.860281	55.635623
2837.349398	196859.469756	55.640628
2836.498109	196630.571852	55.645633
2835.722521	196388.989199	55.650637
2835.250463	196152.831178	55.655642
2834.586072	195920.343906	55.660647
2834.250295	195669.749592	55.665652
2833.630226	195443.785103	55.670657
2832.843560	195190.057966	55.675661
2832.507452	194941.235935	55.680666
2831.374689	194700.023126	55.685671
2830.630851	194453.838333	55.690676
2829.977548	194214.040627	55.695681
2829.340197	193973.376292	55.700685
2828.922164	193729.077478	55.705690
2828.133044	193494.865078	55.710695
2827.466635	193244.729487	55.715700
2826.803542	193008.463579	55.720705
2826.241825	192757.117807	55.725709
2825.543538	192518.785818	55.730714
2824.792308	192280.717831	55.735719
2823.992371	192033.981227	55.740724
2823.910637	191797.069175	55.745729
2823.122841	191551.465454	55.750733
2822.304868	191307.521781	55.755738
2821.457777	191066.154045	55.760743
2821.089084	190810.741609	55.765748
2820.116812	190573.963783	55.770753
2819.561533	190333.698554	55.775757
2818.943065	190085.301765	55.780762
2818.131982	189849.227174	55.785767
2817.718395	189605.825995	55.790772
2816.763889	189367.359129	55.795777
2816.085700	189125.745328	55.800781
2815.377284	188887.127381	55.805786
2814.869068	188644.216830	55.810791
2814.118486	188395.213606	55.815796
2813.387292	188167.836953	55.820801
2812.782322	187931.153990	55.825805
2812.066024	187682.479885	55.830810
2811.279018	187454.072283	55.835815
2810.958220	187207.997033	55.840820
2810.013334	186978.967922	55.845825
2809.358440	186734.233031	55.850829
2808.924990	186503.992992	55.855834
2808.032718	186258.852932	55.860839
2807.212098	186015.954615	55.865844
2806.562310	185786.172244	55.870849
2806.009689	185541.999964	55.875853
2805.477018	185314.186016	55.880858
2804.671556	185081.086015	55.885863
2804.097978	184839.096224	55.890868
2803.481082	184609.238238	55.895873
2802.920921	184362.669099	55.900877
2802.086300	184136.639004	55.905882
2801.445008	183895.924405	55.910887
2801.354400	183647.974510	55.915892
2800.192986	183416.046228	55.920897
2799.545108	183171.482030	55.925901
2799.265584	182939.734583	55.930906
2798.287822	182691.434380	55.935911
2797.956435	182448.261510	55.940916
2797.210370	182207.712550	55.945921
2796.390956	181961.859218	55.950925
2795.639906	181722.585778	55.955930
2794.940925	181486.256595	55.960935
2794.516837	181244.453450	55.965940
2793.526318	181013.032271	55.970945
2792.575732	180769.585153	55.975949
2792.285492	180526.416426	55.980954
2791.613061	180288.919260	55.985959
2791.031735	180043.051760	55.990964
2790.088587	179803.475859	55.995969
2789.638028	179574.749857	56.000973
2788.984370	179334.011355	56.005978
2788.040409	179102.618490	56.010983
2787.593382	178860.374414	56.015988
2786.771456	178627.883607	56.020993
2786.406141	178389.610580	56.025997
2785.711089	178154.978070	56.031002
2784.982134	177921.369803	56.036007
2784.344756	177686.221981	56.041012
2783.419544	177447.254340	56.046017
2782.982831	177204.522063	56.051021
2782.072516	176966.915779	56.056026
2781.381639	176732.926522	56.061031
2780.965875	176494.341536	56.066036
2780.180850	176256.999284	56.071041
2779.550801	176026.527568	56.076045
2779.117121	175793.075232	56.081050
2778.261772	175551.538189	56.086055
2777.724341	175321.729845	56.091060
2776.815107	175080.038764	56.096065
2776.240580	174834.073496	56.101069
2775.652437	174604.340804	56.106074
2774.593348	174380.788896	56.111079
2773.972435	174141.563262	56.116084
2773.572593	173909.744280	56.121089
2773.066027	173679.151770	56.126093
2772.283137	173440.553696	56.131098
2771.644711	173207.746357	56.136103
2771.324296	172960.696608	56.141108
2770.263537	172735.335394	56.146113
2769.676200	172492.476885	56.151117
2769.211138	172265.739457	56.156122
2768.189474	172033.406627	56.161127
2767.721089	171791.576412	56.166132
2766.749534	171558.856894	56.171137
2766.280343	171322.663587	56.176141
2765.526344	171089.454545	56.181146
2764.867389	170858.241183	56.186151
2763.972144	170619.436206	56.191156
2763.525707	170385.915564	56.196161
2762.940021	170163.901992	56.201165
2762.374748	169924.807368	56.206170
2761.802056	169704.511166	56.211175
2760.884937	169461.761745	56.216180
2760.376765	169230.559583	56.221185
2759.673067	168996.083405	56.226189
2759.375818	168758.683009	56.231194
2758.352959	168523.268357	56.236199
2757.947082	168274.900970	56.241204
2757.177424	168040.339337	56.246209
2756.344629	167795.107361	56.251213
2756.120449	167560.907347	56.256218
2754.841509	167332.852482	56.261223
2754.563071	167091.517421	56.266228
2753.951090	166857.828235	56.271233
2753.068795	166626.599355	56.276237
2752.593768	166392.433580	56.281242
2751.886119	166162.769376	56.286247
2751.564447	165917.112566	56.291252
2750.490434	165693.879869	56.296257
2749.912965	165438.768088	56.301261
2749.385729	165200.676191	56.306266
2748.807531	164968.074248	56.311271
2748.274425	164732.592945	56.316276
2747.350074	164491.542237	56.321281
2746.750880	164239.175924	56.326285
2745.765224	164010.497246	56.331290
2744.813349	163780.352409	56.336295
2744.516915	163548.719261	56.341300
2743.943744	163237.447316	56.346305
2743.288833	162995.918715	56.351309
2742.861336	162762.798245	56.356314
2741.700811	162536.762987	56.361319
2741.233910	162294.776960	56.366324
2740.538387	162064.475194	56.371329
2740.054488	161828.750482	56.376333
2739.244898	161597.643325	56.381338
2738.468799	161351.033739	56.386343
2738.247823	161115.208476	56.391348
2737.140870	160885.462556	56.396353
2736.611557	160653.770375	56.401357
2736.162991	160400.402484	56.406362
2735.076810	160174.446579	56.411367
2734.549647	159930.706097	56.416372
2733.732023	159692.963265	56.421377
2733.081145	159470.591692	56.426381
2732.646182	159235.016189	56.431386
2731.740123	158997.914999	56.436391
2731.293708	158762.713153	56.441396
2730.490824	158544.198198	56.446401
2729.817105	158308.654004	56.451405
2729.401020	158067.146318	56.456410
2728.531660	157831.102387	56.461415
2727.818746	157592.683395	56.466420
2727.451624	157371.996414	56.471425
2726.844420	157130.067841	56.476429
2726.010633	156897.406189	56.481434
2725.105266	156664.376067	56.486439
2724.591811	156423.225764	56.491444
2723.933309	156194.253113	56.496449
2723.126663	155967.682644	56.501453
2722.441618	155721.695655	56.506458
2721.730934	155491.286777	56.511463
2721.243989	155262.839792	56.516468
2720.457563	155041.522307	56.521473
2719.856593	154805.939648	56.526477
2719.239134	154571.441731	56.531482
2718.334451	154345.011982	56.536487
2717.811556	154105.010885	56.541492
2717.463977	153880.567978	56.546497
2716.577053	153644.237883	56.551501
2715.896141	153409.669105	56.556506
2715.147863	153183.451187	56.561511
2714.646747	152949.479995	56.566516
2713.764441	152723.172019	56.571521
2713.344620	152493.728977	56.576525
2712.831399	152254.209894	56.581530
2712.031150	152030.029050	56.586535
2711.439097	151794.224604	56.591540
2710.576363	151556.545417	56.596545
2710.024104	151334.681453	56.601549
2709.601451	151102.007309	56.606554
2708.795228	150863.014994	56.611559
2708.160563	150631.420010	56.616564
2707.119167	150399.675021	56.621569
2706.434777	150168.586879	56.626573
2706.092939	149932.997620	56.631578
2704.959599	149719.828557	56.636583
2704.586988	149482.442627	56.641588
2703.841393	149244.736226	56.646593
2703.319890	149015.956330	56.651597
2702.865637	148789.696589	56.656602
2701.686680	148564.557282	56.661607
2701.151037	148333.318830	56.666612
2700.719381	148108.687076	56.671617
2699.928939	147868.532316	56.676621
2699.339957	147639.505985	56.681626
2698.439040	147412.030366	56.686631
2697.961815	147181.617038	56.691636
2697.238403	146943.708069	56.696641
2696.428186	146723.492411	56.701645
2695.898220	146493.130543	56.706650
2694.979601	146271.765998	56.711655
2694.290006	146043.656673	56.716660
2693.569576	145823.280541	56.721665
2692.972114	145593.952574	56.726669
2692.418272	145367.720153	56.731674
2691.760134	145150.465059	56.736679
2691.266441	144914.237840	56.741684
2690.404139	144693.765015	56.746689
2689.802569	144471.320854	56.751693
2689.297943	144238.468029	56.756698
2688.551151	144026.012875	56.761703
2687.961792	143792.630378	56.766708
2687.156165	143569.970828	56.771713
2686.552550	143343.735529	56.776717
2686.037852	143111.706007	56.781722
2685.421486	142893.481573	56.786727
2684.755506	142654.846325	56.791732
2684.050557	142435.012668	56.796737
2683.464273	142207.702858	56.801741
2682.930370	141976.498164	56.806746
2681.942166	141747.540028	56.811751
2681.646239	141510.456085	56.816756
2680.728687	141297.093793	56.821761
2679.845358	141059.560036	56.826765
2679.480912	140827.574807	56.831770
2678.440569	140619.179466	56.836775
2677.838916	140376.219000	56.841780
2677.170224	140157.488728	56.846785
2676.384586	139931.078787	56.851789
2676.025493	139713.014213	56.856794
2675.132929	139480.729098	56.861799
2674.857779	139265.653013	56.866804
2673.847594	139051.876535	56.871809
2673.127989	138815.376339	56.876813
2672.777649	138592.871609	56.881818
2671.603649	138372.658921	56.886823
2671.282704	138144.613387	56.891828
2670.559614	137927.254736	56.896833
2669.944091	137696.578539	56.901837
2669.475100	137475.917758	56.906842
2668.606329	137253.568700	56.911847
2668.264160	137023.743764	56.916852
2667.282856	136803.397850	56.921857
2666.769163	136575.661719	56.926861
2666.178010	136345.195476	56.931866
2665.334641	136123.384501	56.936871
2664.932077	135892.028044	56.941876
2664.072277	135681.923563	56.946881
2663.489830	135452.123572	56.951885
2662.947057	135219.435322	56.956890
2662.296071	135001.693025	56.961895
2661.869436	134759.042983	56.966900
2660.926329	134533.728262	56.971905
2660.038007	134306.526496	56.976909
2659.372436	134076.331332	56.981914
2658.496784	133860.132199	56.986919
2658.149296	133632.138660	56.991924
2657.633849	133420.967026	56.996929
2657.017407	133193.692833	57.001933
2656.341533	132953.358576	57.006938
2655.102001	132737.136617	57.011943
2654.886969	132518.467483	57.016948
2654.057849	132291.551709	57.021953
2653.453156	132055.939078	57.026957
2652.857750	131834.553603	57.031962
2652.040923	131614.183009	57.036967
2651.388267	131393.419749	57.041972
2650.614927	131172.563011	57.046977
2650.161203	130952.178136	57.051981
2649.408804	130729.784593	57.056986
2648.726143	130504.841393	57.061991
2647.923435	130278.216982	57.066996
2647.535302	130061.575671	57.072001
2646.983402	129827.764152	57.077005
2646.258727	129608.664763	57.082010
2645.435129	129394.231436	57.087015
2644.648599	129161.364447	57.092020
2644.261733	128946.598632	57.097025
2643.704819	128722.297566	57.102029
2643.335778	128498.133651	57.107034
2642.482308	128275.559692	57.112039
2642.056369	128037.653559	57.117044
2641.393964	127813.528954	57.122049
2640.395495	127577.444769	57.127053
2639.768666	127349.724056	57.132058
2638.821004	127130.349328	57.137063
2638.331665	126896.120746	57.142068
2637.855085	126673.995283	57.147073
2636.652721	126431.946106	57.152077
2636.278868	126225.174930	57.157082
2635.498010	126002.049038	57.162087
2635.067146	125772.913384	57.167092
2634.283488	125542.730695	57.172097
2633.213351	125334.870133	57.177101
2632.832641	125104.563805	57.182106
2632.114587	124894.441143	57.187111
2631.664169	124666.041765	57.192116
2631.009776	124439.937057	57.197121
2630.414284	124227.057168	57.202125
2629.793577	124001.471447	57.207130
2628.987761	123778.520178	57.212135
2628.473015	123547.664207	57.217140
2627.839550	123327.597344	57.222145
2627.046847	123101.144835	57.227149
2626.767410	122867.666959	57.232154
2625.778932	122650.595209	57.237159
2625.148685	122418.764111	57.242164
2624.742375	122200.270481	57.247169
2623.448458	121970.186482	57.252173
2622.952141	121742.250985	57.257178
2622.003328	121529.245368	57.262183
2621.858329	121297.639197	57.267188
2621.052564	121084.131986	57.272193
2619.974927	120855.775635	57.277197
2619.554136	120636.002063	57.282202
2618.772125	120418.585735	57.287207
2617.873927	120198.713700	57.292212
2617.755231	119977.551875	57.297217
2616.981808	119751.543916	57.302221
2616.400162	119531.640007	57.307226
2615.455695	119314.652164	57.312231
2614.851157	119086.077531	57.317236
2614.457862	118875.589109	57.322241
2613.272384	118664.910510	57.327245
2613.042636	118436.040961	57.332250
2612.100040	118228.831543	57.337255
2611.421253	117998.399217	57.342260
2610.709483	117781.495205	57.347265
2610.275374	117563.108051	57.352269
2609.561737	117348.417021	57.357274
2608.549077	117139.310398	57.362279
2607.956570	116920.852215	57.367284
2607.366853	116703.830012	57.372289
2606.529008	116493.844004	57.377293
2606.222247	116274.850921	57.382298
2605.420937	116069.858107	57.387303
2604.513390	115847.352164	57.392308
2604.024122	115631.510095	57.397313
2603.799172	115422.438643	57.402317
2603.403667	115210.342896	57.407322
2602.131131	114987.204096	57.412327
2601.767848	114768.404269	57.417332
2600.964614	114551.294556	57.422337
2600.264896	114330.063758	57.427341
2599.317089	114117.721921	57.432346
2598.763860	113897.652233	57.437351
2598.408637	113675.458615	57.442356
2597.828559	113468.427088	57.447361
2596.573193	113252.047571	57.452365
2596.181084	113043.022258	57.457370
2595.202492	112827.732256	57.462375
2594.602776	112618.432392	57.467380
2594.465879	112411.098184	57.472385
2593.213979	112184.496673	57.477389
2592.686433	111972.696600	57.482394
2592.126602	111762.686781	57.487399
2591.857862	111530.782134	57.492404
2590.998087	111332.843450	57.497409
2590.249916	111126.061038	57.502413
2589.378245	110899.664827	57.507418
2588.656603	110692.291635	57.512423
2588.255011	110475.693041	57.517428
2587.854434	110268.869052	57.522433
2587.006096	110059.306491	57.527437
2586.333742	109836.346990	57.532442
2585.189184	109633.872607	57.537447
2584.911168	109416.058029	57.542452
2584.038803	109198.948762	57.547457
2583.438513	108986.849471	57.552461
2583.063005	108773.491687	57.557466
2582.373118	108566.455018	57.562471
2581.717446	108355.340856	57.567476
2581.017062	108142.858639	57.572481
2580.040545	107912.692955	57.577485
2579.839418	107708.473282	57.582490
2578.900849	107506.910312	57.587495
2578.486322	107287.981512	57.592500
2577.549864	107075.070156	57.597505
2576.895290	106862.338082	57.602509
2576.587747	106649.089694	57.607514
2575.593537	106441.396041	57.612519
2574.689684	106216.190438	57.617524
2574.486564	106010.614904	57.622529
2573.587130	105791.922453	57.627533
2573.178786	105582.512743	57.632538
2572.283296	105371.056575	57.637543
2571.786223	105156.607890	57.642548
2571.073603	104951.458446	57.647553
2570.392715	104731.535565	57.652557
2569.972023	104513.210362	57.657562
2568.852044	104314.589670	57.662567
2568.415281	104102.405875	57.667572
2567.867847	103883.243697	57.672577
2567.248532	103667.444719	57.677581
2566.724676	103457.177435	57.682586
2565.892347	103247.487472	57.687591
2565.131017	103021.331475	57.692596
2564.395571	102814.396037	57.697601
2563.439755	102602.098592	57.702605
2563.053164	102374.874366	57.707610
2562.465900	102171.499075	57.712615
2561.878340	101960.411493	57.717620
2560.995445	101756.401517	57.722625
2560.526414	101538.504766	57.727629
2559.885005	101318.556642	57.732634
2558.876806	101120.979158	57.737639
2558.399396	100904.485236	57.742644
2557.531149	100697.798859	57.747649
2557.113994	100483.627356	57.752653
2556.515319	100264.297715	57.757658
2555.946244	100064.204719	57.762663
2555.435709	99853.948614	57.767668
2554.451748	99637.927360	57.772673
2553.836544	99422.306386	57.777677
2553.004298	99206.360266	57.782682
2552.269975	99003.505330	57.787687
2551.992110	98795.683065	57.792692
2551.193659	98578.811392	57.797697
2550.453541	98366.537426	57.802701
2549.871005	98142.290634	57.807706
2549.001038	97945.853709	57.812711
2548.725344	97729.103834	57.817716
2547.932751	97519.097677	57.822721
2546.998658	97313.054602	57.827725
2546.350352	97096.147792	57.832730
2545.470866	96900.355609	57.837735
2545.143538	96687.733700	57.842740
2544.113292	96477.280095	57.847745
2543.593213	96279.064267	57.852749
2543.159533	96064.270619	57.857754
2542.285514	95862.746811	57.862759
2541.740522	95650.156429	57.867764
2540.952801	95452.320039	57.872769
2540.249647	95243.195936	57.877773
2539.869659	95031.244790	57.882778
2538.987205	94827.467488	57.887783
2538.727511	94611.023874	57.892788
2537.947579	94410.842581	57.897793
2536.594658	94200.080828	57.902797
2536.236740	93997.426496	57.907802
2535.638818	93789.079255	57.912807
2535.268875	93578.896830	57.917812
2534.372331	93382.078844	57.922817
2533.709722	93173.145156	57.927821
2533.228039	92952.637180	57.932826
2532.645041	92753.111690	57.937831
2531.843332	92541.396787	57.942836
2530.799612	92339.614462	57.947841
2530.342288	92136.238190	57.952845
2530.006990	91927.613083	57.957850
2529.359263	91731.347304	57.962855
2528.723474	91525.164165	57.967860
2527.932327	91298.120774	57.972865
2526.975564	91108.472298	57.977869
2526.854794	90885.721075	57.982874
2525.970340	90679.483800	57.987879
2525.275984	90467.860503	57.992884
2524.474128	90257.080557	57.997889
2523.900703	90057.571540	58.002893
2523.107457	89848.835794	58.007898
2522.392902	89647.748746	58.012903
2521.693081	89435.020379	58.017908
2521.360854	89232.469000	58.022913
2520.596423	89035.370839	58.027917
2519.781373	88821.398675	58.032922
2518.930856	88616.582974	58.037927
2518.501457	88409.920908	58.042932
2518.383201	88200.973483	58.047937
2517.132555	88002.034404	58.052941
2516.834014	87799.966514	58.057946
2516.065900	87587.774223	58.062951
2515.651073	87374.754572	58.067956
2514.679463	87166.313750	58.072961
2513.921475	86960.782656	58.077965
2513.664416	86745.493650	58.082970
2512.791162	86542.545990	58.087975
2511.903088	86332.546825	58.092980
2511.618629	86121.103756	58.097985
2510.551391	85918.192742	58.102989
2510.307446	85712.566749	58.107994
2509.204128	85503.427582	58.112999
2508.697833	85296.534961	58.118004
2508.130194	85084.627204	58.123009
2507.037911	84880.779150	58.128013
2506.599590	84673.900808	58.133018
2506.164905	84477.844338	58.138023
2505.378206	84263.158679	58.143028
2504.472347	84054.452491	58.148033
2503.784329	83850.398108	58.153037
2503.317750	83649.308756	58.158042
2502.846351	83445.477482	58.163047
2502.233108	83238.666209	58.168052
2501.654369	83037.980756	58.173057
2500.428925	82829.394354	58.178061
2500.371414	82614.495747	58.183066
2499.424047	82417.252951	58.188071
2498.538986	82213.530841	58.193076
2498.105807	82005.828456	58.198081
2497.373196	81790.912172	58.203085
2496.664932	81588.093466	58.208090
2495.804179	81384.622736	58.213095
2495.240043	81178.818996	58.218100
2494.815603	80973.597230	58.223105
2493.991788	80774.461650	58.228109
2493.674053	80563.294871	58.233114
2492.887774	80358.161868	58.238119
2492.498121	80155.503042	58.243124
2491.551465	79942.217773	58.248129
2490.804830	79737.319101	58.253133
2490.418749	79519.842657	58.258138
2489.657838	79319.006299	58.263143
2488.937807	79104.584698	58.268148
2488.230662	78915.226823	58.273153
2487.190708	78700.828439	58.278157
2486.870161	78493.333366	58.283162
2486.220946	78287.172551	58.288167
2485.443761	78080.901011	58.293172
2484.725953	77875.084720	58.298177
2484.033057	77677.992317	58.303181
2483.281486	77455.538811	58.308186
2482.921185	77256.813551	58.313191
2481.862343	77054.158192	58.318196
2481.553103	76846.513214	58.323201
2480.540036	76663.675195	58.328205
2479.800057	76448.809243	58.333210
2479.177166	76251.801860	58.338215
2478.480745	76045.037468	58.343220
2478.193208	75855.381557	58.348225
2477.161380	75658.951638	58.353229
2476.438465	75455.308507	58.358234
2475.734076	75259.388130	58.363239
2475.322062	75061.839302	58.368244
2474.292963	74856.920164	58.373249
2473.330395	74662.959936	58.378253
2473.255211	74470.508212	58.383258
2472.510630	74283.410431	58.388263
2471.954219	74080.540382	58.393268
2471.374564	73880.248322	58.398273
2470.502412	73688.703343	58.403277
2470.207710	73489.225305	58.408282
2469.458207	73291.411538	58.413287
2468.791226	73082.201982	58.418292
2468.196402	72876.670317	58.423297
2467.173633	72684.861042	58.428301
2466.652440	72492.080836	58.433306
2466.152724	72291.247150	58.438311
2465.285308	72093.216851	58.443316
2464.858450	71892.489660	58.448321
2463.977051	71688.041926	58.453325
2463.367323	71488.184009	58.458330
2462.733970	71299.018655	58.463335
2462.378688	71090.300027	58.468340
2461.771989	70890.891072	58.473345
2460.893566	70696.411182	58.478349
2460.482092	70478.053967	58.483354
2459.460453	70283.385466	58.488359
2458.702733	70084.325304	58.493364
2458.073966	69889.509724	58.498369
2457.477855	69689.788154	58.503373
2457.115274	69484.628497	58.508378
2456.139112	69291.406785	58.513383
2455.722985	69093.943025	58.518388
2455.277036	68888.308745	58.523393
2454.362504	68692.125169	58.528397
2453.650357	68481.191492	58.533402
2452.766386	68278.267953	58.538407
2452.598993	68075.555941	58.543412
2452.072164	67876.994582	58.548417
2451.042967	67674.436022	58.553421
2450.555083	67467.094243	58.558426
2449.946033	67263.193970	58.563431
2448.935629	67059.809134	58.568436
2448.925228	66855.254554	58.573441
2447.588030	66655.554778	58.578445
2447.179144	66450.313973	58.583450
2446.161884	66252.961587	58.588455
2445.730614	66041.474654	58.593460
2445.151041	65850.073438	58.598465
2444.203050	65648.849914	58.603469
2443.964892	65432.250485	58.608474
2443.479277	65232.196085	58.613479
2442.665825	65027.370164	58.618484
2441.779283	64822.830316	58.623489
2441.028092	64624.739974	58.628493
2440.617352	64426.116427	58.633498
2439.986704	64219.883296	58.638503
2439.264452	64007.464284	58.643508
2438.497226	63805.452504	58.648513
2437.648309	63612.995421	58.653517
2437.273685	63401.097936	58.658522
2436.409409	63205.566761	58.663527
2435.735091	63000.265535	58.668532
2435.200445	62794.852561	58.673537
2434.658705	62600.194607	58.678541
2434.062445	62388.983036	58.683546
2433.190468	62193.862381	58.688551
2432.672390	61977.802300	58.693556
2431.714760	61783.190159	58.698561
2431.063173	61585.542968	58.703565
2430.624160	61384.638208	58.708570
2429.846928	61182.820483	58.713575
2428.923118	60983.443593	58.718580
2428.479233	60777.382782	58.723585
2427.516376	60570.662573	58.728589
2426.691285	60382.400467	58.733594
2426.499510	60179.699759	58.738599
2425.799183	59985.663655	58.743604
2425.573108	59782.849206	58.748609
2424.510968	59591.042918	58.753613
2423.871345	59380.986120	58.758618
2423.245682	59185.553659	58.763623
2422.418197	58978.376867	58.768628
2421.956803	58780.064263	58.773633
2420.779047	58583.380357	58.778637
2420.536534	58381.647236	58.783642
2419.647471	58186.849396	58.788647
2419.011865	57983.929466	58.793652
2418.277736	57787.215284	58.798657
2417.452097	57592.986502	58.803661
2417.137816	57392.699790	58.808666
2416.304455	57201.400889	58.813671
2415.734468	57008.903800	58.818676
2415.477572	56813.298508	58.823681
2414.732362	56623.998210	58.828685
2414.005957	56409.352018	58.833690
2412.974677	56209.232927	58.838695
2412.408696	56023.246180	58.843700
2412.198340	55814.870656	58.848705
2410.958732	55626.719196	58.853709
2410.666010	55412.000031	58.858714
2409.897849	55222.385463	58.863719
2409.096518	55018.407203	58.868724
2408.695771	54826.187726	58.873729
2407.884539	54628.440274	58.878733
2407.317290	54425.592916	58.883738
2406.671263	54224.146375	58.888743
2406.157928	54019.937370	58.893748
2405.433869	53826.298655	58.898753
2404.716713	53634.129211	58.903757
2404.200185	53420.968826	58.908762
2403.041946	53223.861197	58.913767
2402.306370	53021.976966	58.918772
2401.759739	52827.466364	58.923777
2401.168141	52627.054087	58.928781
2400.897755	52433.133602	58.933786
2399.807100	52247.869651	58.938791
2399.526737	52053.385250	58.943796
2398.680246	51848.304198	58.948801
2397.705538	51646.134638	58.953805
2397.518629	51453.116350	58.958810
2396.672838	51250.763081	58.963815
2396.076206	51049.865990	58.968820
2395.434100	50856.388379	58.973825
2394.584945	50657.902354	58.978829
2393.899577	50457.206292	58.983834
2393.256888	50273.416601	58.988839
2392.814929	50070.335510	58.993844
2392.195155	49868.148629	58.998849
2391.303083	49670.104283	59.003853
2390.769994	49472.732866	59.008858
2390.094842	49276.673778	59.013863
2389.311542	49077.596872	59.018868
2388.876589	48872.712317	59.023873
2387.893707	48683.061103	59.028877
2387.321193	48478.323107	59.033882
2386.552211	48291.460876	59.038887
2385.758039	48093.839251	59.043892
2385.235661	47893.459323	59.048897
2384.281860	47708.726731	59.053901
2383.863960	47515.053611	59.058906
2383.342327	47319.833196	59.063911
2382.584935	47126.746430	59.068916
2382.180685	46929.968003	59.073921
2381.387743	46738.687852	59.078925
2380.611477	46531.559446	59.083930
2379.913179	46338.674366	59.088935
2379.276254	46147.534044	59.093940
2378.674081	45955.814600	59.098945
2377.582431	45774.894508	59.103949
2377.217783	45582.132453	59.108954
2376.382920	45386.673116	59.113959
2375.539184	45190.866274	59.118964
2375.035533	44998.575480	59.123969
2374.261678	44811.073989	59.128973
2373.789575	44618.042251	59.133978
2373.262981	44440.455898	59.138983
2372.495571	44248.854054	59.143988
2371.870299	44053.926687	59.148993
2371.074818	43872.881237	59.153997
2370.751501	43681.518825	59.159002
2369.905883	43480.475042	59.164007
2369.319703	43294.715352	59.169012
2368.803187	43109.420989	59.174017
2367.915771	42917.157050	59.179021
2367.251287	42723.348206	59.184026
2366.475207	42530.520617	59.189031
2365.751688	42342.117434	59.194036
2365.588648	42150.692703	59.199041
2364.977791	41964.097320	59.204045
2364.198366	41767.581935	59.209050
2363.700877	41569.806590	59.214055
2362.777736	41371.519148	59.219060
2362.171855	41174.900774	59.224065
2361.660487	40988.132566	59.229069
2361.092039	40788.122789	59.234074
2360.128257	40591.858745	59.239079
2359.361548	40401.219519	59.244084
2358.864680	40207.557799	59.249089
2357.970168	40014.878306	59.254093
2357.237524	39822.826681	59.259098
2356.582197	39631.553858	59.264103
2355.879102	39443.667676	59.269108
2355.351784	39260.417884	59.274113
2354.516838	39077.256781	59.279117
2354.228206	38874.200657	59.284122
2353.248669	38688.099298	59.289127
2352.754385	38500.602996	59.294132
2352.148899	38299.085244	59.299137
2351.583535	38111.416377	59.304141
2350.744731	37919.719173	59.309146
2349.946704	37728.966148	59.314151
2349.340104	37544.214018	59.319156
2349.090796	37343.692854	59.324161
2348.254868	37153.938704	59.329165
2347.938774	36963.674290	59.334170
2346.985951	36775.439873	59.339175
2346.312334	36578.109064	59.344180
2345.857326	36374.431101	59.349185
2345.123272	36190.915274	59.354189
2344.455779	35993.103493	59.359194
2343.649126	35796.677017	59.364199
2342.766584	35603.611002	59.369204
2342.623792	35407.300340	59.374209
2341.749697	35218.381701	59.379213
2341.171602	35019.987122	59.384218
2340.368338	34827.870524	59.389223
2339.365963	34640.184685	59.394228
2338.948722	34443.927234	59.399233
2338.222468	34256.189270	59.404237
2337.996358	34058.828142	59.409242
2336.829268	33873.029330	59.414247
2336.209464	33673.279190	59.419252
2335.546357	33483.959475	59.424257
2334.732912	33294.789022	59.429261
2334.428697	33102.902333	59.434266
2333.521289	32914.387993	59.439271
2332.649530	32722.665229	59.444276
2332.016017	32534.318791	59.449281
2330.953301	32359.157416	59.454285
2330.595812	32171.503000	59.459290
2329.977198	31990.701457	59.464295
2329.372298	31802.921363	59.469300
2329.297415	31606.605151	59.474305
2328.072634	31421.187415	59.479309
2327.678109	31232.602975	59.484314
2326.961005	31048.674880	59.489319
2326.201531	30854.331295	59.494324
2325.681437	30667.266475	59.499329
2325.053266	30471.516067	59.504333
2324.298095	30296.383108	59.509338
2323.492577	30111.632571	59.514343
2322.811001	29921.572829	59.519348
2322.489653	29721.848340	59.524353
2321.244222	29545.883133	59.529357
2320.691752	29344.580368	59.534362
2320.172454	29166.385296	59.539367
2319.381006	28985.445095	59.544372
2318.924906	28799.288846	59.549377
2318.229179	28606.887739	59.554381
2317.914494	28420.291540	59.559386
2316.855931	28233.396774	59.564391
2316.288541	28047.213037	59.569396
2315.788243	27859.074399	59.574401
2315.178299	27676.554292	59.579405
2314.336343	27483.788360	59.584410
2313.699322	27298.417310	59.589415
2312.987912	27113.527792	59.594420
2312.288379	26926.325713	59.599425
2311.782614	26743.992302	59.604429
2311.024436	26546.593966	59.609434
2310.489965	26361.367445	59.614439
2309.679473	26171.142844	59.619444
2309.307373	25986.941411	59.624449
2308.315953	25806.278435	59.629453
2307.855220	25617.189639	59.634458
2307.121311	25418.798955	59.639463
2306.024007	25228.687034	59.644468
2305.806506	25034.720270	59.649473
2304.744120	24866.956675	59.654477
2304.096036	24676.490979	59.659482
2303.648773	24502.758492	59.664487
2302.811978	24316.729157	59.669492
2302.364119	24121.337059	59.674497
2301.764208	23943.797451	59.679501
2301.038331	23751.481820	59.684506
2300.268382	23572.033728	59.689511
2299.669192	23390.283828	59.694516
2299.030187	23205.545388	59.699521
2298.001320	23025.333479	59.704525
2297.429853	22834.198423	59.709530
2296.928292	22650.623612	59.714535
2296.151176	22475.181598	59.719540
2295.296314	22297.804184	59.724545
2294.610262	22122.950965	59.729549
2294.360376	21945.501274	59.734554
2293.785923	21752.651954	59.739559
2293.325512	21580.104655	59.744564
2292.731691	21393.414724	59.749569
2291.704792	21207.802426	59.754573
2291.083627	21013.031826	59.759578
2290.444125	20835.394211	59.764583
2289.654435	20655.878744	59.769588
2289.172372	20467.895793	59.774593
2287.973387	20296.078923	59.779597
2287.222986	20114.732396	59.784602
2287.100349	19928.814857	59.789607
2286.559956	19742.093732	59.794612
2286.108092	19567.302691	59.799617
2284.929996	19387.705373	59.804621
2284.266882	19196.376147	59.809626
2283.698149	19013.753061	59.814631
2283.143461	18830.539337	59.819636
2282.581559	18649.484562	59.824641
2281.637774	18467.838771	59.829645
2280.705602	18283.027522	59.834650
2280.340295	18109.391214	59.839655
2279.739576	17938.280512	59.844660
2279.306191	17753.088143	59.849665
2278.268159	17564.471870	59.854669
2277.906144	17377.087132	59.859674
2276.743373	17193.828001	59.864679
2276.014100	17027.600927	59.869684
2275.681276	16843.638421	59.874689
2274.926218	16671.986694	59.879693
2274.673741	16484.758528	59.884698
2273.810066	16301.556610	59.889703
2272.860297	16134.103796	59.894708
2272.259573	15946.767053	59.899713
2271.304767	15785.712648	59.904718
2270.791097	15601.249900	59.909722
2270.120216	15430.598835	59.914727
2269.304306	15259.693638	59.919732
2268.957867	15084.488404	59.924737
2268.043552	14903.493471	59.929742
2267.430045	14727.418289	59.934746
2266.922791	14555.828572	59.939751
2266.193534	14381.527284	59.944756
2265.631542	14205.762242	59.949761
2264.857462	14037.338556	59.954766
2264.287646	13854.635320	59.959770
2263.376751	13678.544824	59.964775
2262.961119	13514.196398	59.969780
2262.324756	13330.805280	59.974785
2261.487140	13161.536806	59.979790
2260.645285	12988.047440	59.984794
2259.849975	12816.745094	59.989799
2259.419177	12649.701710	59.994804
2258.886758	12472.428050	59.999809
2258.175356	12315.653471	60.004814
2257.633948	12138.222056	60.009818
2256.919479	11966.051525	60.014823
2256.008977	11792.588498	60.019828
2255.480281	11625.994937	60.024833
2254.798736	11452.844899	60.029838
2254.221457	11286.546838	60.034842
2253.470583	11122.564915	60.039847
2252.438391	10944.886929	60.044852
2252.173232	10776.349717	60.049857
2251.242108	10612.255919	60.054862
2250.942447	10449.624487	60.059866
2250.139015	10277.574184	60.064871
2248.978264	10118.629658	60.069876
2248.654429	9945.007492	60.074881
2248.033480	9779.124835	60.079886
2247.652094	9618.759661	60.084890
2246.871797	9445.531633	60.089895
2246.174544	9284.983405	60.094900
2245.594685	9115.770970	60.099905
2244.606159	8956.012910	60.104910
2244.089309	8784.090772	60.109914
2243.248499	8618.616900	60.114919
2242.459143	8461.667229	60.119924
2242.000387	8288.844495	60.124929
2241.238492	8122.887828	60.129934
2240.552879	7960.422543	60.134938
2239.919666	7803.793033	60.139943
2239.102721	7633.536316	60.144948
2238.744224	7473.006949	60.149953
2237.930682	7333.327751	60.154958
2237.350698	7159.985813	60.159962
2236.380691	6994.833160	60.164967
2235.655534	6839.692077	60.169972
2235.032014	6669.044883	60.174977
2233.818765	6521.568216	60.179982
2233.040727	6356.969606	60.184986
2232.982038	6211.545676	60.189991
2232.330355	6059.155659	60.194996
2231.429198	5895.644222	60.200001
2230.645741	5754.319304	60.205006
2229.865943	5600.566789	60.210010
2229.277069	5449.532945	60.215015
2228.717543	5317.321931	60.220020
2228.371747	5162.668988	60.225025
2227.100927	5008.536690	60.230030
2226.651118	4862.362934	60.235034
2225.909180	4713.317780	60.240039
2225.165787	4571.497697	60.245044
2224.562043	4426.741639	60.250049
2223.590461	4291.705732	60.255054
2223.076949	4144.329788	60.260058
2222.664729	3995.738030	60.265063
2221.463763	3858.035600	60.270068
2220.866833	3711.130717	60.275073
2220.014462	3584.106612	60.280078
2219.346393	3445.379434	60.285082
2218.875014	3322.537913	60.290087
2217.737562	3200.807060	60.295092
2217.358459	3065.975461	60.300097
2216.308841	2938.369901	60.305102
2215.528740	2812.788964	60.310106
2214.668926	2692.086904	60.315111
2213.572038	2576.616638	60.320116
2212.784581	2457.822209	60.325121
2211.879648	2366.041328	60.330126
2211.034976	2260.652439	60.335130
2209.778130	2166.436586	60.340135
2208.701183	2077.826654	60.345140
2208.250275	1992.948217	60.350145
2207.047389	1924.144613	60.355150
2206.239836	1847.763249	60.360154
2205.464263	1771.173754	60.365159
2204.650354	1716.967864	60.370164
2204.094579	1653.176124	60.375169
2202.927961	1589.617203	60.380174
2202.030903	1518.584975	60.385178
2201.203859	1468.649116	60.390183
2200.103109	1433.124744	60.395188
2199.375287	1392.615061	60.400193
2198.185625	1357.768172	60.405198
2197.330463	1317.896353	60.410202
2196.503525	1299.164113	60.415207
2195.972983	1271.113659	60.420212
2195.373841	1243.016576	60.425217
2194.540754	1228.607547	60.430222
2193.943081	1196.414502	60.435226
2193.679341	1179.452509	60.440231
2192.952967	1162.482708	60.445236
2192.864830	1130.027606	60.450241
2192.242426	1104.621902	60.455246
2191.788822	1071.524668	60.460250
2191.179412	1037.088811	60.465255
2190.923268	994.843918	60.470260
2190.363207	962.064261	60.475265
2189.395268	915.239054	60.480270
2188.635441	869.438426	60.485274
2187.906564	840.641971	60.490279
2187.032005	818.978998	60.495284
2186.291577	790.784558	60.500289
2185.495012	766.221644	60.505294
2185.190100	739.629921	60.510298
2184.661230	702.220321	60.515303
2183.874832	682.311472	60.520308
2183.137914	646.318119	60.525313
2182.426657	627.197000	60.530318
2182.098960	587.535266	60.535322
2181.775584	559.491171	60.540327
2180.549059	527.482173	60.545332
2180.146315	485.030192	60.550337
2179.396989	465.987871	60.555342
2178.522063	439.324694	60.560346
2177.974108	412.081383	60.565351
2177.048103	385.156735	60.570356
2176.809120	345.763878	60.575361
2176.149126	341.094889	60.580366
2175.586431	306.132935	60.585370
2174.779588	269.049266	60.590375
2173.948560	244.188341	60.595380
2173.184419	216.952887	60.600385
2172.492401	196.942999	60.605390
2172.176047	172.700742	60.610394
2171.391606	145.547494	60.615399
2170.681536	135.991456	60.620404
2170.004674	114.332873	60.625409
2169.473196	93.490229	60.630414
2168.635714	77.203257	60.635418
2167.962268	67.292936	60.640423
2167.152085	47.235770	60.645428
2166.415950	15.200577	60.650433
2165.409640	13.612912	60.655438
2164.634150	3.643129	60.660442
2163.903646	-4.963370	60.665447
2162.928503	-9.279456	60.670452
2162.197922	-21.513822	60.675457
2161.663048	-22.763103	60.680462
2161.208234	-29.448385	60.685466
2160.759228	-40.548601	60.690471
2160.201936	-24.731202	60.695476
2159.854083	-35.650345	60.700481
2158.842913	-52.977236	60.705486
2157.969885	-40.364680	60.710490
2156.704781	-51.813237	60.715495
2155.706260	-43.181611	60.720500
2155.399544	-43.140833	60.725505
2154.976741	-34.419189	60.730510
2154.456297	-40.583104	60.735514
2153.879234	-42.995819	60.740519
2153.137109	-27.024514	60.745524
2152.640306	-37.685049	60.750529
2151.653927	-38.641911	60.755534
2151.157021	-34.735699	60.760538
2150.642772	-43.374903	60.765543
2149.691068	-35.477695	60.770548
2149.413440	-36.906562	60.775553
2148.694815	-23.317093	60.780558
2148.196014	-30.301330	60.785562
2147.901092	-37.461418	60.790567
2146.413937	-29.830921	60.795572
2146.180027	-26.728123	60.800577
2145.721316	-19.295488	60.805582
2144.596303	-26.174062	60.810586
2143.935341	-24.771322	60.815591
2143.181767	-20.810189	60.820596
2143.031704	-16.993695	60.825601
2142.168553	-14.194769	60.830606
2141.654286	-18.377381	60.835610
2140.540791	-26.379027	60.840615
2140.207835	-10.327539	60.845620
2139.747846	-13.454288	60.850625
2139.180918	-2.332430	60.855630
2138.436375	-12.017722	60.860634
2137.635540	-21.567127	60.865639
2136.684200	-15.346312	60.870644
2136.393608	-7.113997	60.875649
2135.917660	-1.697966	60.880654
2135.117939	-6.026106	60.885658
2134.577511	-6.851076	60.890663
2133.540910	2.096505	60.895668
2132.909518	-10.547847	60.900673
2132.339766	-7.003815	60.905678
2131.827555	-4.855884	60.910682
2131.296010	-4.093435	60.915687
2130.547472	-9.542267	60.920692
2129.942495	-9.592937	60.925697
2129.081737	-10.930858	60.930702
2128.215031	-0.745480	60.935706
2127.572132	0.949299	60.940711
2127.365975	12.139299	60.945716
2127.024631	-6.016965	60.950721
2126.549244	7.987328	60.955726
2125.922169	2.622515	60.960730
2125.103760	-0.857385	60.965735
2123.719359	-3.307585	60.970740
2123.324180	10.027163	60.975745
2122.634668	14.758763	60.980750
2121.637637	8.332977	60.985754
2120.965710	9.598689	60.990759
2120.174855	7.612569	60.995764
2120.146990	10.392515	61.000769
2119.889335	16.351888	61.005774
2118.980854	9.773277	61.010778
2118.372087	13.659408	61.015783
2117.393336	17.771408	61.020788
2116.952417	13.406839	61.025793
2116.316864	12.184579	61.030798
2115.272956	17.997465	61.035802
2114.867007	6.362098	61.040807
2113.958533	15.473084	61.045812
2113.229663	14.166280	61.050817
2112.445358	17.971453	61.055822
2111.835681	16.388686	61.060826
2111.621550	16.528322	61.065831
2110.959045	31.760063	61.070836
2110.842445	21.236295	61.075841
2109.471899	16.153459	61.080846
2108.466199	23.624026	61.085850
2108.787824	23.393214	61.090855
2107.978386	32.132093	61.095860
2107.074371	15.769043	61.100865
2105.820430	26.262691	61.105870
2106.001619	23.442645	61.110874
2105.363401	18.191567	61.115879
2104.270110	24.445971	61.120884
2103.775975	18.760433	61.125889
2102.959568	31.214261	61.130894
2102.394782	33.669387	61.135898
2101.870221	30.896668	61.140903
2101.177608	32.966787	61.145908
2100.637596	25.440278	61.150913
2099.478533	29.360119	61.155918
2099.019726	39.659796	61.160922
2098.528281	32.429939	61.165927
2097.592596	44.733967	61.170932
2097.355174	35.748018	61.175937
2096.514762	43.310645	61.180942
2095.752113	33.843473	61.185946
2095.147146	37.125019	61.190951
2094.542471	40.592606	61.195956
2093.716282	36.645572	61.200961
2093.082378	33.702543	61.205966
2092.493416	34.660199	61.210970
2092.124081	42.764684	61.215975
2091.226938	42.430789	61.220980
2090.805724	33.368348	61.225985
2090.043338	37.945940	61.230990
2089.500205	48.982851	61.235994
2088.193881	31.403104	61.240999
2087.508856	37.095979	61.246004
2087.322219	29.432969	61.251009
2086.740719	40.401842	61.256014
2086.129505	38.806706	61.261018
2085.552062	37.376528	61.266023
2084.064251	38.812721	61.271028
2083.778573	39.753793	61.276033
2083.619082	46.052429	61.281038
2082.852848	37.738619	61.286042
2082.285985	40.954195	61.291047
2080.832783	39.451669	61.296052
2080.668917	38.613475	61.301057
2079.876776	45.165472	61.306062
2079.677331	40.649039	61.311066
2078.493389	28.058450	61.316071
2077.698753	46.544034	61.321076
2077.761840	39.844368	61.326081
2076.823058	37.635719	61.331086
2075.553517	47.742348	61.336090
2075.825268	36.592380	61.341095
2074.503040	45.797437	61.346100
2074.271661	46.490189	61.351105
2073.174864	44.008561	61.356110
2072.657151	50.422393	61.361114
2072.745001	48.762059	61.366119
2071.344692	48.003376	61.371124
2070.904056	32.781087	61.376129
2069.936901	37.952591	61.381134
2069.432995	34.104239	61.386138
2069.010182	39.452723	61.391143
2067.818519	44.323956	61.396148
2067.688755	35.024452	61.401153
2066.841769	45.292693	61.406158
2066.460625	39.466218	61.411162
2065.835409	41.689660	61.416167
2065.159948	52.451098	61.421172
2064.388458	53.499230	61.426177
2063.888198	50.413567	61.431182
2062.939989	48.854567	61.436186
2062.035093	41.135221	61.441191
2061.133098	55.941357	61.446196
2061.198680	47.954455	61.451201
2060.845990	41.596746	61.456206
2059.676623	47.833285	61.461210
2058.848417	40.981739	61.466215
2057.965397	50.848837	61.471220
2057.432667	44.423501	61.476225
2056.988271	40.595669	61.481230
2056.432322	49.329037	61.486234
2055.914301	46.910114	61.491239
2055.134211	51.675038	61.496244
2054.625125	45.739553	61.501249
2054.029210	42.445139	61.506254
2053.366641	46.896512	61.511258
2052.172701	46.649156	61.516263
2051.256166	55.414519	61.521268
2051.145433	57.980534	61.526273
2050.545657	59.305782	61.531278
2049.474555	45.697466	61.536282
2048.703876	53.151268	61.541287
2048.389967	55.041451	61.546292
2048.171867	58.830915	61.551297
2047.323530	48.785973	61.556302
2046.455697	58.275340	61.561306
2045.717931	47.175183	61.566311
2045.006361	61.471698	61.571316
2044.621098	45.076787	61.576321
2044.405255	50.461819	61.581326
2043.600677	57.378515	61.586330
2042.543946	38.969100	61.591335
2041.436414	59.369956	61.596340
2040.768507	44.461285	61.601345
2040.466760	59.238403	61.606350
2040.305801	52.812417	61.611354
2039.874509	39.846920	61.616359
2038.604372	58.847970	61.621364
2038.221754	54.114595	61.626369
2037.745707	50.148280	61.631374
2036.635262	50.613103	61.636378
2035.725831	55.018501	61.641383
2034.549915	52.082651	61.646388
2034.396311	53.920585	61.651393
2034.426445	58.326688	61.656398
2033.101672	60.061900	61.661402
2032.755095	52.679744	61.666407
2031.872696	59.339126	61.671412
2031.526014	52.747068	61.676417
2031.262869	50.361819	61.681422
2030.629746	57.908919	61.686426
2029.724434	49.872670	61.691431
2028.245681	57.214919	61.696436
2027.927846	53.855876	61.701441
2027.345570	65.100872	61.706446
2026.519847	61.648962	61.711450
2026.181895	59.993122	61.716455
2025.543866	63.745152	61.721460
2024.816249	54.321321	61.726465
2024.463866	58.895368	61.731470
2023.150416	59.879709	61.736474
2022.491227	51.911637	61.741479
2021.497319	59.307833	61.746484
2021.544714	56.952150	61.751489
2020.909857	54.676361	61.756494
2019.819348	59.541025	61.761498
2019.458291	60.382101	61.766503
2018.992552	65.917190	61.771508
2018.624010	54.950834	61.776513
2017.961469	62.105201	61.781518
2017.027462	62.001116	61.786522
2016.071145	53.165539	61.791527
2015.071064	66.225746	61.796532
2014.796815	66.319737	61.801537
2014.362685	65.276849	61.806542
2013.238218	62.230337	61.811546
2013.058498	54.870590	61.816551
2012.436223	71.751851	61.821556
2012.064244	54.757145	61.826561
2011.106487	66.296712	61.831566
2009.878959	66.157210	61.836570
2009.468743	43.920311	61.841575
2008.423997	67.788514	61.846580
2008.356218	55.998537	61.851585
2007.779430	65.301371	61.856590
2007.043128	66.668799	61.861594
2006.699407	68.193122	61.866599
2006.305414	72.064126	61.871604
2005.250491	61.963669	61.876609
2004.562756	71.720947	61.881614
2003.754521	61.358981	61.886618
2003.510598	63.709586	61.891623
2001.680855	58.977231	61.896628
2001.567488	58.708210	61.901633
2000.933724	58.662137	61.906638
1999.851400	61.984776	61.911642
1999.815201	51.773106	61.916647
1998.975477	60.385940	61.921652
1997.980965	56.426226	61.926657
1997.617306	58.161878	61.931662
1997.008238	69.518370	61.936666
1996.708681	57.337812	61.941671
1996.256028	68.177452	61.946676
1995.669696	69.491116	61.951681
1994.449265	63.174940	61.956686
1993.391903	64.405665	61.961690
1993.126276	55.252307	61.966695
1992.324990	60.731842	61.971700
1992.087871	59.682921	61.976705
1991.431280	57.377472	61.981710
1990.814316	65.721558	61.986714
1990.095317	57.892301	61.991719
1988.835475	66.947150	61.996724
1988.344075	67.720605	62.001729
1988.035874	57.403866	62.006734
1987.140322	65.006821	62.011738
1986.979368	65.544895	62.016743
1985.886940	59.936985	62.021748
1984.442552	58.414188	62.026753
1984.168465	54.597185	62.031758
1983.349142	70.591905	62.036762
1983.037189	70.354404	62.041767
1982.461664	69.761333	62.046772
1981.957634	70.311282	62.051777
1981.584857	74.664640	62.056782
1981.224314	74.244034	62.061786
1980.621052	63.144619	62.066791
1979.285326	68.450360	62.071796
1978.657927	62.033756	62.076801
1978.226068	68.345668	62.081806
1977.575829	62.765349	62.086810
1976.836459	64.008688	62.091815
1975.626021	69.685641	62.096820
1975.038542	68.484167	62.101825
1974.321656	68.831353	62.106830
1973.762134	75.942573	62.111834
1973.556507	71.007642	62.116839
1972.895653	65.905263	62.121844
1972.074443	67.339795	62.126849
1971.592853	68.971165	62.131854
1970.432862	68.332090	62.136858
1969.723318	63.843012	62.141863
1968.867683	68.678302	62.146868
1968.290443	66.388648	62.151873
1968.283279	67.241369	62.156878
1967.099330	67.916590	62.161882
1967.172898	67.785061	62.166887
1966.558560	67.926730	62.171892
1966.151584	68.491240	62.176897
1964.948232	66.693644	62.181902
1963.997827	71.933499	62.186906
1963.657155	70.866323	62.191911
1962.949271	69.542033	62.196916
1961.900386	66.404697	62.201921
1961.081596	66.768061	62.206926
1960.204704	72.614435	62.211930
1959.905300	61.569304	62.216935
1959.005199	73.823581	62.221940
1958.889720	66.172933	62.226945
1958.573072	66.248427	62.231950
1957.675336	68.677585	62.236954
1957.808742	69.186284	62.241959
1956.359743	70.692085	62.246964
1955.738799	67.154074	62.251969
1955.043523	63.668865	62.256974
1954.233205	74.393391	62.261978
1953.020628	68.586938	62.266983
1952.481365	78.896269	62.271988
1952.567891	68.501103	62.276993
1951.826219	67.795635	62.281998
1950.489835	65.115538	62.287002
1950.378389	65.748261	62.292007
1949.762144	77.642085	62.297012
1949.135420	76.024209	62.302017
1948.391766	60.837415	62.307022
1947.360633	75.988953	62.312026
1947.071726	64.715067	62.317031
1946.082715	67.338495	62.322036
1945.672287	68.215803	62.327041
1945.193221	65.528936	62.332046
1944.555679	69.075894	62.337050
1943.214367	58.328627	62.342055
1942.299010	71.965207	62.347060
1941.928506	70.524288	62.352065
1941.689506	64.944934	62.357070
1940.956165	67.333808	62.362074
1940.670164	59.180360	62.367079
1940.351040	66.195070	62.372084
1939.641698	72.877476	62.377089
1938.616443	67.334618	62.382094
1937.891582	73.782937	62.387098
1937.098184	74.646920	62.392103
1936.059454	70.787290	62.397108
1934.900198	61.334233	62.402113
1934.880629	67.851947	62.407118
1934.566892	69.223281	62.412122
1934.236276	63.655317	62.417127
1933.315041	78.152306	62.422132
1932.857340	71.920093	62.427137
1931.563853	68.914640	62.432142
1930.607119	74.693270	62.437146
1930.520551	66.419850	62.442151
1929.543334	70.102736	62.447156
1929.456794	72.417325	62.452161
1929.158664	63.917284	62.457166
1928.191402	68.787652	62.462170
1927.588569	68.629450	62.467175
1926.470448	68.234493	62.472180
1925.704343	57.853257	62.477185
1925.533456	69.791501	62.482190
1923.973316	79.483852	62.487194
1923.676970	62.671132	62.492199
1922.881325	78.312015	62.497204
1922.403523	74.448504	62.502209
1922.068831	73.222683	62.507214
1921.459785	81.264323	62.512218
1921.007373	77.079803	62.517223
1919.838649	79.028426	62.522228
1918.959410	69.422108	62.527233
1918.677215	71.824529	62.532238
1918.061381	78.293394	62.537242
1917.604842	61.619651	62.542247
1916.356565	79.729437	62.547252
1915.630170	72.410746	62.552257
1915.099162	70.419704	62.557262
1914.423596	72.379931	62.562266
1914.422026	65.384586	62.567271
1913.503262	76.951111	62.572276
1913.187692	66.790099	62.577281
1912.005218	64.656465	62.582286
1910.955961	76.393521	62.587290
1910.872061	73.475187	62.592295
1910.110558	71.251069	62.597300
1909.383789	75.800983	62.602305
1908.266922	74.342932	62.607310
1907.443944	80.256461	62.612314
1906.945427	72.844825	62.617319
1906.665574	72.359379	62.622324
1906.152528	63.835111	62.627329
1905.641176	69.626623	62.632334
1905.004513	78.353914	62.637338
1904.946828	71.980931	62.642343
1903.607805	66.448476	62.647348
1903.050776	67.063626	62.652353
1902.286119	77.183230	62.657358
1900.846505	70.931859	62.662362
1900.042939	67.501706	62.667367
1899.747157	83.668812	62.672372
1899.621087	70.259047	62.677377
1898.780244	66.429522	62.682382
1898.258990	82.260249	62.687386
1898.070562	70.185069	62.692391
1897.288896	78.608941	62.697396
1896.172843	74.807336	62.702401
1895.609338	67.148971	62.707406
1894.792882	77.666320	62.712410
1894.605034	60.342784	62.717415
1892.974333	69.297269	62.722420
1892.125484	70.154298	62.727425
1891.653247	71.766849	62.732430
1891.155181	77.507370	62.737434
1891.246405	73.697036	62.742439
1890.870678	75.366808	62.747444
1890.162152	76.174752	62.752449
1888.983716	79.459077	62.757454
1888.034763	71.369879	62.762458
1887.793695	72.810108	62.767463
1887.163693	72.812353	62.772468
1886.345322	70.674544	62.777473
1885.489260	73.142842	62.782478
1884.539834	65.179885	62.787482
1884.201496	61.483485	62.792487
1883.643346	73.286085	62.797492
1883.275778	81.376128	62.802497
1882.404265	78.527642	62.807502
1881.249563	74.074568	62.812506
1880.884898	79.650405	62.817511
1880.322519	79.127811	62.822516
1879.877478	75.221260	62.827521
1879.683638	72.632629	62.832526
1878.203531	84.318250	62.837530
1877.605933	80.290833	62.842535
1876.929307	70.992999	62.847540
1876.166666	77.013653	62.852545
1875.889730	74.698421	62.857550
1874.865993	68.787909	62.862554
1874.098323	79.318019	62.867559
1873.189423	70.069679	62.872564
1872.234681	84.660317	62.877569
1871.991365	61.419205	62.882574
1871.605961	79.075031	62.887578
1871.468087	71.088890	62.892583
1870.520448	72.433135	62.897588
1870.401736	74.792258	62.902593
1869.367440	68.686299	62.907598
1868.383824	75.809669	62.912602
1868.182220	74.382948	62.917607
1867.337114	73.537803	62.922612
1866.149074	76.653345	62.927617
1865.627042	77.586232	62.932622
1864.890790	73.713303	62.937626
1864.864297	74.482357	62.942631
1863.914896	65.436003	62.947636
1863.370910	82.770070	62.952641
1862.763446	75.659603	62.957646
1861.622341	73.967293	62.962650
1861.541432	69.059886	62.967655
1860.466155	82.018538	62.972660
1859.366198	68.632514	62.977665
1858.950430	67.969950	62.982670
1858.344470	62.358982	62.987674
1857.931401	71.359869	62.992679
1857.757735	67.000217	62.997684
1857.047960	64.320035	63.002689
1856.148478	65.339661	63.007694
1855.076946	69.557957	63.012698
1854.974470	64.210839	63.017703
1853.881603	77.643805	63.022708
1852.785014	65.481009	63.027713
1852.171701	66.674404	63.032718
1851.555081	84.758044	63.037722
1851.429067	76.330035	63.042727
1850.487044	67.487525	63.047732
1850.555259	76.628050	63.052737
1849.526405	83.739689	63.057742
1848.690141	79.037368	63.062746
1848.376707	76.480344	63.067751
1847.516027	79.409874	63.072756
1846.445286	80.026172	63.077761
1845.668906	70.233238	63.082766
1844.552423	80.807698	63.087770
1844.293367	75.865495	63.092775
1843.872596	78.474435	63.097780
1843.773386	79.439544	63.102785
1843.124654	76.237145	63.107790
1842.187365	79.677173	63.112794
1841.367794	78.492080	63.117799
1840.898448	81.596027	63.122804
1840.070822	78.253294	63.127809
1839.784154	71.416764	63.132814
1838.465278	74.387505	63.137818
1837.886404	74.734892	63.142823
1837.044510	77.413852	63.147828
1836.522889	78.507534	63.152833
1836.347595	80.402541	63.157838
1835.674108	82.889177	63.162842
1834.744460	62.327569	63.167847
1833.653528	78.680845	63.172852
1833.174806	73.533818	63.177857
1832.981983	73.249034	63.182862
1832.553447	79.549398	63.187866
1832.080857	74.489710	63.192871
1830.668475	73.023420	63.197876
1830.034351	78.396032	63.202881
1830.132687	78.124943	63.207886
1828.301182	79.361954	63.212890
1827.731672	78.703305	63.217895
1827.390335	82.252146	63.222900
1826.606821	75.300534	63.227905
1826.652786	77.518389	63.232910
1825.837364	83.927497	63.237914
1824.820289	77.205365	63.242919
1823.778057	84.866357	63.247924
1823.006670	80.814509	63.252929
1822.965516	75.066555	63.257934
1822.517016	84.166120	63.262938
1822.148015	81.535919	63.267943
1820.871931	77.397047	63.272948
1820.078928	86.127101	63.277953
1819.776192	83.700851	63.282958
1819.065616	88.139404	63.287962
1818.568662	73.824993	63.292967
1817.505353	83.498436	63.297972
1816.526818	75.328807	63.302977
1816.254565	72.339459	63.307982
1815.880003	73.160627	63.312986
1815.061821	75.094636	63.317991
1814.461709	74.647436	63.322996
1813.444991	76.877907	63.328001
1813.002921	67.531814	63.333006
1812.324265	74.890638	63.338010
1812.050326	67.594763	63.343015
1811.009750	83.506377	63.348020
1809.983143	85.762075	63.353025
1809.685349	71.507511	63.358030
1808.927133	83.225195	63.363034
1808.736626	76.357629	63.368039
1807.692815	72.216578	63.373044
1806.954244	79.799391	63.378049
1806.542271	69.866605	63.383054
1805.745071	68.827787	63.388058
1805.245507	58.538322	63.393063
1804.427279	63.757235	63.398068
1803.517367	62.953942	63.403073
1803.254096	65.760233	63.408078
1802.667522	71.738751	63.413082
1801.663828	65.605887	63.418087
1800.719137	71.294331	63.423092
1799.640286	79.722835	63.428097
1799.713259	70.369078	63.433102
1799.374516	65.089445	63.438106
1798.987535	59.803280	63.443111
1798.058913	73.656469	63.448116
1797.069228	75.084689	63.453121
1796.718938	66.693885	63.458126
1796.014342	80.358537	63.463130
1795.353495	73.348035	63.468135
1794.612982	70.849376	63.473140
1793.828050	72.563638	63.478145
1793.373471	69.142761	63.483150
1792.097576	68.850188	63.488154
1791.270582	75.593885	63.493159
1790.782805	66.887435	63.498164
1790.235106	65.889430	63.503169
1790.071260	61.143440	63.508174
1788.957336	67.235662	63.513178
1788.995556	63.678184	63.518183
1788.418515	64.045791	63.523188
1787.275978	69.156932	63.528193
1786.793777	60.768156	63.533198
1786.356155	66.046488	63.538202
1785.081142	63.888184	63.543207
1784.095947	74.888102	63.548212
1783.513922	71.591547	63.553217
1783.321202	62.505500	63.558222
1782.513406	70.845229	63.563226
1782.532632	73.576699	63.568231
1781.775675	69.232408	63.573236
1780.325176	66.919041	63.578241
1779.958602	66.396917	63.583246
1779.322849	67.699550	63.588250
1779.069109	66.751064	63.593255
1777.776268	70.462044	63.598260
1776.747677	71.707209	63.603265
1776.750615	62.888146	63.608270
1776.140202	72.041805	63.613274
1775.609445	67.320963	63.618279
1774.399875	67.337997	63.623284
1773.439740	71.084458	63.628289
1773.094258	70.486442	63.633294
1772.421751	68.183578	63.638298
1772.251959	64.982419	63.643303
1771.702306	65.803011	63.648308
1771.147450	69.511922	63.653313
1770.394480	63.590001	63.658318
1769.296057	63.912672	63.663322
1768.831867	60.182660	63.668327
1768.301853	66.868158	63.673332
1767.307080	65.693566	63.678337
1766.718166	69.190259	63.683342
1766.056678	67.101696	63.688346
1765.811033	60.793274	63.693351
1764.879303	59.063029	63.698356
1763.628342	63.842878	63.703361
1763.288048	57.294015	63.708366
1762.619704	65.617907	63.713370
1762.026430	60.758761	63.718375
1761.955332	62.933698	63.723380
1761.230475	70.077508	63.728385
1760.291765	50.861794	63.733390
1759.494599	67.020972	63.738394
1758.954105	59.657052	63.743399
1757.912981	66.354331	63.748404
1756.903068	71.365572	63.753409
1756.663480	64.646167	63.758414
1756.270532	73.572901	63.763418
1756.101387	63.798694	63.768423
1755.214041	72.357650	63.773428
1753.952120	72.636905	63.778433
1753.449489	62.272244	63.783438
1752.906763	67.068938	63.788442
1752.616819	60.464769	63.793447
1751.865190	66.396963	63.798452
1750.378843	74.511715	63.803457
1749.968072	70.497244	63.808462
1749.347092	77.720761	63.813466
1749.106933	66.265708	63.818471
1748.582836	70.340333	63.823476
1747.348132	76.931164	63.828481
1747.030108	74.792791	63.833486
1746.294390	72.274461	63.838490
1746.011925	77.465080	63.843495
1745.223409	73.141582	63.848500
1744.059560	70.465734	63.853505
1743.594946	65.627161	63.858510
1743.104123	72.397907	63.863514
1742.484192	78.075796	63.868519
1741.420288	77.624997	63.873524
1740.383818	68.717109	63.878529
1740.162878	72.503886	63.883534
1739.884853	77.230161	63.888538
1739.471757	69.915396	63.893543
1739.057525	71.192320	63.898548
1737.506696	74.792900	63.903553
1736.827886	67.928780	63.908558
1736.196257	74.510572	63.913562
1735.814379	72.366571	63.918567
1735.323326	70.159483	63.923572
1734.276216	74.941667	63.928577
1733.694814	72.255326	63.933582
1733.021166	82.574983	63.938586
1732.716771	74.197400	63.943591
1731.719251	73.810182	63.948596
1730.877249	71.964770	63.953601
1730.548099	66.133251	63.958606
1729.842369	68.885235	63.963610
1729.470636	69.504110	63.968615
1728.283321	65.109912	63.973620
1727.448901	73.037553	63.978625
1727.379296	66.106647	63.983630
1726.456262	75.303657	63.988634
1725.895780	74.061683	63.993639
1724.845828	67.018385	63.998644
1723.904101	77.088870	64.003649
1723.783792	68.309884	64.008654
1723.103442	72.619071	64.013658
1722.688325	67.190726	64.018663
1722.799001	64.971655	64.023668
1721.419498	69.000786	64.028673
1720.809503	67.881799	64.033678
1720.137065	78.330576	64.038682
1718.995858	72.251127	64.043687
1718.029454	76.684598	64.048692
1717.736385	73.048845	64.053697
1717.319993	66.455300	64.058702
1716.451967	69.826016	64.063706
1716.411201	63.540257	64.068711
1715.093190	79.385561	64.073716
1714.598198	82.629222	64.078721
1714.027800	70.882837	64.083726
1713.561618	81.677339	64.088730
1712.412930	69.529201	64.093735
1711.683506	64.609687	64.098740
1711.010043	69.807210	64.103745
1710.448142	68.309992	64.108750
1709.970987	70.148864	64.113754
1709.902721	62.452903	64.118759
1709.016561	68.393859	64.123764
1708.113502	69.978668	64.128769
1707.703323	67.123210	64.133774
1706.459060	68.746442	64.138778
1705.569956	65.443486	64.143783
1704.935892	67.804036	64.148788
1704.360844	70.029053	64.153793
1704.168013	63.149262	64.158798
1703.391739	73.712305	64.163802
1703.247607	72.337974	64.168807
1702.106087	72.552398	64.173812
1701.529434	72.232390	64.178817
1701.322384	65.674988	64.183822
1700.235239	67.184956	64.188826
1699.523121	68.602242	64.193831
1698.750607	67.887553	64.198836
1698.177636	71.372266	64.203841
1697.704455	65.379122	64.208846
1696.324418	74.949932	64.213850
1695.988933	66.351789	64.218855
1695.274616	65.512737	64.223860
1694.782280	69.828338	64.228865
1694.726492	61.342685	64.233870
1693.470120	70.867831	64.238874
1692.571935	72.081277	64.243879
1692.249769	69.536704	64.248884
1691.542596	71.636048	64.253889
1690.603900	65.578069	64.258894
1689.696005	67.173114	64.263898
1689.292159	70.410185	64.268903
1688.746184	69.255805	64.273908
1688.026153	71.511739	64.278913
1688.116885	68.882660	64.283918
1687.110105	81.117673	64.288922
1686.333501	62.355647	64.293927
1685.928208	72.168252	64.298932
1684.851945	68.601709	64.303937
1683.803665	67.593348	64.308942
1683.112943	73.544272	64.313946
1682.668860	70.981217	64.318951
1682.529185	71.623164	64.323956
1681.953552	69.875813	64.328961
1681.252100	68.377112	64.333966
1680.159355	79.223827	64.338970
1679.282170	79.956110	64.343975
1679.000225	72.694645	64.348980
1678.393751	76.498507	64.353985
1677.447052	65.219565	64.358990
1676.445906	77.769872	64.363994
1676.126584	69.721114	64.368999
1676.173169	69.052952	64.374004
1675.239776	76.337142	64.379009
1674.106416	72.014826	64.384014
1673.015972	75.711053	64.389018
1672.813886	74.804837	64.394023
1672.717471	72.959291	64.399028
1672.222049	72.703660	64.404033
1671.479170	64.760821	64.409038
1670.162286	77.019072	64.414042
1669.776660	78.323003	64.419047
1669.487621	71.851168	64.424052
1668.174488	69.714749	64.429057
1667.626858	69.940512	64.434062
1666.802679	72.241380	64.439066
1666.328440	69.881821	64.444071
1666.029414	66.692526	64.449076
1665.228902	76.839157	64.454081
1664.373132	66.484093	64.459086
1663.874783	73.827706	64.464090
1663.222246	77.615233	64.469095
1662.039998	66.993474	64.474100
1660.936401	78.899296	64.479105
1660.706874	69.040074	64.484110
1660.307624	78.541845	64.489114
1659.966147	70.413029	64.494119
1659.562998	78.336841	64.499124
1658.939892	78.129880	64.504129
1658.036311	74.113281	64.509134
1657.312856	80.540936	64.514138
1656.715840	75.769144	64.519143
1655.799080	79.259589	64.524148
1654.786263	79.762681	64.529153
1654.467581	70.818089	64.534158
1653.768824	77.297015	64.539162
1653.230487	79.752762	64.544167
1652.986742	79.597510	64.549172
1651.986739	73.820526	64.554177
1651.560999	66.700975	64.559182
1650.644535	69.169476	64.564186
1649.497958	67.691028	64.569191
1648.793576	68.375370	64.574196
1648.059866	79.799804	64.579201
1647.879293	66.945181	64.584206
1647.761107	64.412369	64.589210
1647.021488	61.707029	64.594215
1645.975741	63.517957	64.599220
1645.322225	67.039128	64.604225
1644.852395	61.226821	64.609230
1643.789509	69.059881	64.614234
1642.902123	74.350539	64.619239
1642.370895	69.215843	64.624244
1641.684669	73.022130	64.629249
1641.645624	64.163226	64.634254
1640.870370	70.565991	64.639258
1639.997187	76.206066	64.644263
1639.205457	72.638499	64.649268
1638.760787	76.787261	64.654273
1638.373404	66.526542	64.659278
1637.356737	73.047297	64.664282
1636.475961	75.246775	64.669287
1636.011149	71.859885	64.674292
1635.279124	67.724579	64.679297
1634.830336	65.025083	64.684302
1633.795780	70.606422	64.689306
1633.011062	66.452678	64.694311
1632.581588	70.069153	64.699316
1632.082236	72.857765	64.704321
1631.740109	63.945293	64.709326
1630.976728	69.910922	64.714330
1630.030539	67.694154	64.719335
1629.710328	68.639181	64.724340
1628.950684	68.335643	64.729345
1628.223136	67.456133	64.734350
1626.867570	73.399139	64.739354
1626.792153	68.489303	64.744359
1626.185888	67.940620	64.749364
1625.479444	76.911644	64.754369
1624.989622	67.170265	64.759374
1623.803478	72.914466	64.764378
1623.430139	72.011804	64.769383
1623.292298	63.098422	64.774388
1622.345173	77.975697	64.779393
1621.463882	70.486959	64.784398
1620.847460	62.274097	64.789402
1620.261994	68.935307	64.794407
1619.739747	72.159656	64.799412
1618.362581	82.872585	64.804417
1618.046756	77.835353	64.809422
1617.504122	71.403026	64.814426
1616.774883	73.173148	64.819431
1616.431511	64.954756	64.824436
1615.680707	78.816797	64.829441
1614.892766	71.584477	64.834446
1614.072681	80.617714	64.839450
1613.726926	71.652988	64.844455
1613.106528	70.762768	64.849460
1611.590105	70.448568	64.854465
1611.469862	69.828986	64.859470
1610.862832	68.665399	64.864474
1610.287253	68.518711	64.869479
1610.037809	68.996745	64.874484
1609.064773	71.478978	64.879489
1608.612950	67.887387	64.884494
1607.956823	71.877350	64.889498
1606.750188	63.958535	64.894503
1605.964163	65.128958	64.899508
1605.461225	66.002089	64.904513
1605.214162	62.885764	64.909518
1604.602561	69.311425	64.914522
1603.692122	71.214419	64.919527
1602.973935	66.326273	64.924532
1602.300336	69.375967	64.929537
1602.102034	69.749680	64.934542
1601.020780	70.952814	64.939546
1600.203626	67.551732	64.944551
1599.646227	64.254469	64.949556
1599.047172	76.038361	64.954561
1598.922586	64.546057	64.959566
1597.591753	73.982932	64.964570
1596.984076	64.530742	64.969575
1596.784153	71.114936	64.974580
1595.620631	66.639752	64.979585
1594.924253	61.833303	64.984590
1593.979138	66.458977	64.989594
1593.615848	62.302953	64.994599
1593.012361	65.866650	64.999604
1592.433970	67.592311	65.004609
1591.943304	58.053726	65.009614
1590.987237	80.550910	65.014618
1590.592107	66.631217	65.019623
1590.132886	64.978938	65.024628
1589.368491	69.071263	65.029633
1588.372315	64.407066	65.034638
1587.605148	72.089082	65.039642
1586.943932	76.447300	65.044647
1586.578302	70.249432	65.049652
1585.824534	70.744512	65.054657
1585.338072	61.109062	65.059662
1584.119258	68.813945	65.064666
1583.979279	70.061513	65.069671
1583.702163	63.879548	65.074676
1582.497974	70.654835	65.079681
1581.841878	62.924542	65.084686
1581.143822	65.129700	65.089690
1580.270511	67.141923	65.094695
1580.168429	69.611952	65.099700
1578.900979	76.219092	65.104705
1578.628581	69.765132	65.109710
1577.837313	71.002631	65.114714
1577.448912	62.537506	65.119719
1576.821434	70.116904	65.124724
1575.700144	69.891340	65.129729
1575.281571	61.615519	65.134734
1574.391076	73.500910	65.139738
1573.992185	63.479377	65.144743
1573.332716	60.296112	65.149748
1571.933424	72.766978	65.154753
1571.761341	65.289381	65.159758
1570.955094	67.447075	65.164762
1570.817121	63.804052	65.169767
1570.686844	65.964737	65.174772
1569.696993	64.387306	65.179777
1569.211109	57.702337	65.184782
1568.494797	64.581466	65.189786
1566.920588	67.708023	65.194791
1566.413566	70.611408	65.199796
1565.702059	67.736040	65.204801
1565.558414	61.466640	65.209806
1565.070482	63.520142	65.214810
1563.916262	68.418753	65.219815
1563.176478	72.231200	65.224820
1562.505910	71.594975	65.229825
1562.294041	62.669709	65.234830
1561.461754	71.929613	65.239834
1560.584765	72.835374	65.244839
1560.190755	64.833205	65.249844
1559.205539	65.697812	65.254849
1559.037498	67.713107	65.259854
1557.768549	76.249163	65.264858
1557.064132	69.557910	65.269863
1556.880336	69.251212	65.274868
1556.255502	69.218021	65.279873
1556.224450	63.258748	65.284878
1555.196188	68.889577	65.289882
1554.242628	67.371042	65.294887
1553.735124	65.458352	65.299892
1552.623548	63.260007	65.304897
1551.963579	65.348731	65.309902
1551.186534	77.064712	65.314906
1550.848679	68.213080	65.319911
1550.510859	59.309408	65.324916
1549.195167	66.438322	65.329921
1548.721359	67.131788	65.334926
1547.804060	63.748214	65.339930
1547.624811	60.313608	65.344935
1547.418412	51.240821	65.349940
1546.055270	56.093780	65.354945
1545.502694	62.647269	65.359950
1544.813553	58.470487	65.364954
1544.651723	64.195469	65.369959
1543.703309	65.588837	65.374964
1542.593572	75.066302	65.379969
1542.473266	63.404590	65.384974
1541.495948	63.712846	65.389978
1540.738382	65.955855	65.394983
1540.087945	54.308997	65.399988
1539.132308	62.949816	65.404993
1538.829693	61.237970	65.409998
1538.503040	63.519747	65.415002
1538.021429	64.864178	65.420007
1536.922911	63.646235	65.425012
1535.772923	74.322307	65.430017
1535.883435	65.278009	65.435022
1535.144480	66.805260	65.440026
1534.608382	75.893528	65.445031
1533.499179	60.970015	65.450036
1532.815461	66.125047	65.455041
1532.762145	52.751121	65.460046
1531.886664	58.496453	65.465050
1530.764039	55.213325	65.470055
1530.468698	56.848289	65.475060
1529.718191	66.568301	65.480065
1529.236671	67.196762	65.485070
1527.723759	67.892910	65.490074
1527.204777	63.559781	65.495079
1526.757472	69.725953	65.500084
1526.312481	66.153796	65.505089
1526.084176	54.778921	65.510094
1525.625468	56.405151	65.515098
1524.531012	54.786011	65.520103
1523.895822	61.303742	65.525108
1523.250251	62.978589	65.530113
1522.200603	60.838229	65.535118
1521.251359	61.220881	65.540122
1520.475945	60.738527	65.545127
1520.451988	55.888337	65.550132
1519.862007	56.286445	65.555137
1519.786692	54.429673	65.560142
1518.579502	69.054173	65.565146
1517.854070	65.815170	65.570151
1517.496074	60.789393	65.575156
1516.501929	71.262505	65.580161
1515.496574	66.932543	65.585166
1514.647996	61.380731	65.590170
1514.057987	62.482186	65.595175
1513.980463	56.494031	65.600180
1513.194490	68.328128	65.605185
1513.255187	58.668837	65.610190
1511.745878	66.631225	65.615194
1510.924509	74.753969	65.620199
1510.866865	60.469222	65.625204
1510.083005	70.998809	65.630209
1509.370380	54.031591	65.635214
1508.334189	65.948026	65.640218
1507.931755	59.707140	65.645223
1507.684611	59.464130	65.650228
1506.290217	69.220231	65.655233
1505.983519	63.200681	65.660238
1505.294457	64.805170	65.665242
1505.053651	61.823486	65.670247
1504.210673	60.973393	65.675252
1503.165299	74.389443	65.680257
1503.162650	62.821009	65.685262
1501.803942	55.979856	65.690266
1500.634688	61.983198	65.695271
1500.514654	66.799498	65.700276
1499.512641	64.433952	65.705281
1499.621351	58.080305	65.710286
1499.371526	57.557016	65.715290
1498.067605	58.156891	65.720295
1497.354487	58.238671	65.725300
1496.640088	61.512497	65.730305
1496.366972	59.504225	65.735310
1494.868906	62.546180	65.740314
1494.370546	60.813405	65.745319
1493.996093	70.213464	65.750324
1493.278283	69.329291	65.755329
1493.417474	51.072361	65.760334
1491.788509	63.601828	65.765338
1490.839026	60.286471	65.770343
1490.832378	61.635860	65.775348
1490.109632	67.631334	65.780353
1489.945776	54.699192	65.785358
1488.847192	57.879524	65.790362
1487.890593	62.257889	65.795367
1487.601177	63.776796	65.800372
1486.683113	65.263134	65.805377
1486.025561	59.785059	65.810382
1485.167868	70.802637	65.815386
1484.475331	62.862119	65.820391
1484.458157	58.343600	65.825396
1483.882614	64.519114	65.830401
1482.991645	56.780450	65.835406
1482.515504	70.068194	65.840410
1481.973787	64.275235	65.845415
1480.748134	53.744857	65.850420
1479.987712	58.931010	65.855425
1479.741187	60.316942	65.860430
1478.632680	65.559991	65.865434
1477.426446	68.661239	65.870439
1476.814243	66.844054	65.875444
1476.331557	76.988313	65.880449
1476.469632	63.516160	65.885454
1475.580776	66.360387	65.890458
1475.142084	70.315823	65.895463
1474.791326	57.602623	65.900468
1473.592267	70.451726	65.905473
1473.070412	68.900889	65.910478
1472.657659	70.343201	65.915482
1471.512082	70.126273	65.920487
1470.782177	61.560901	65.925492
1470.036043	72.603333	65.930497
1469.810592	72.003632	65.935502
1468.745257	71.788146	65.940506
1467.842918	70.200002	65.945511
1467.310016	62.980042	65.950516
1466.516219	69.600264	65.955521
1466.456307	61.276936	65.960526
1465.769072	63.518250	65.965530
1465.300560	67.200875	65.970535
1464.610550	61.188631	65.975540
1463.767300	65.473296	65.980545
1463.256491	65.314771	65.985550
1462.283071	71.755378	65.990554
1461.345669	69.753327	65.995559
1461.110773	69.150397	66.000564
1460.532296	74.925828	66.005569
1460.290670	58.344260	66.010574
1459.020636	67.973381	66.015578
1458.171729	72.154866	66.020583
1457.935470	64.897226	66.025588
1456.380407	68.897614	66.030593
1455.709278	63.636176	66.035598
1455.246772	68.240391	66.040602
1454.959837	69.216420	66.045607
1454.774546	52.677948	66.050612
1454.152436	63.525619	66.055617
1453.696643	53.604634	66.060622
1452.795342	66.169870	66.065626
1451.818386	70.595640	66.070631
1450.830505	56.682679	66.075636
1449.884437	71.666261	66.080641
1449.474376	59.158039	66.085646
1449.067057	60.572681	66.090650
1448.819932	68.555287	66.095655
1448.181572	69.164532	66.100660
1446.859618	67.256720	66.105665
1446.398244	59.594879	66.110670
1445.801643	64.878013	66.115674
1445.388625	59.361087	66.120679
1444.898084	63.493505	66.125684
1443.506609	68.502411	66.130689
1442.870148	69.384176	66.135694
1442.403527	71.562050	66.140698
1442.053667	71.324332	66.145703
1441.483061	60.305079	66.150708
1440.345309	73.538701	66.155713
1440.043451	69.126928	66.160718
1439.144758	70.392580	66.165722
1438.306532	71.032015	66.170727
1437.321125	61.614682	66.175732
1437.214907	68.010514	66.180737
1436.847641	64.875466	66.185742
1436.241050	73.514463	66.190746
1435.503253	72.817992	66.195751
1434.322171	62.040848	66.200756
1433.743667	77.992647	66.205761
1433.794361	66.619174	66.210766
1432.764796	65.579557	66.215770
1431.520988	68.868152	66.220775
1431.093771	66.234657	66.225780
1430.580311	75.254680	66.230785
1430.565544	63.984656	66.235790
1429.362842	66.085549	66.240794
1428.369817	70.799317	66.245799
1427.945878	68.198418	66.250804
1427.650979	80.077496	66.255809
1426.645445	66.373931	66.260814
1425.772502	66.760261	66.265818
1425.099089	73.902272	66.270823
1424.980318	66.928747	66.275828
1424.305731	73.361296	66.280833
1423.726034	63.764366	66.285838
1422.801275	70.406991	66.290842
1422.075542	74.592566	66.295847
1421.291764	67.035587	66.300852
1420.386826	69.839808	66.305857
1419.888654	66.347091	66.310862
1419.300140	75.120417	66.315866
1418.901447	78.549096	66.320871
1418.542719	61.926221	66.325876
1417.250750	79.180473	66.330881
1416.993391	65.367463	66.335886
1416.360703	64.450860	66.340890
1414.881438	65.196920	66.345895
1414.258713	53.559898	66.350900
1413.601739	65.781948	66.355905
1413.084383	68.338484	66.360910
1412.759386	61.691062	66.365914
1412.418054	62.349303	66.370919
1412.113632	63.782290	66.375924
1411.107253	69.594198	66.380929
1410.455740	60.480211	66.385934
1409.985985	65.697457	66.390938
1408.760051	58.403159	66.395943
1408.406944	63.832105	66.400948
1407.600610	68.759064	66.405953
1407.022843	66.931692	66.410958
1405.793653	65.856005	66.415962
1404.842201	69.506586	66.420967
1404.767902	56.856700	66.425972
1404.316552	64.744027	66.430977
1403.913968	64.161447	66.435982
1403.021624	64.872576	66.440986
1402.143169	69.468791	66.445991
1401.877229	61.223950	66.450996
1401.057168	68.938066	66.456001
1399.693721	67.013219	66.461006
1399.093998	62.991008	66.466010
1398.678104	62.662864	66.471015
1398.554919	63.657027	66.476020
1398.191423	68.045233	66.481025
1397.144728	69.053718	66.486030
1396.457205	74.103726	66.491034
1395.822652	68.674061	66.496039
1394.831773	60.520793	66.501044
1393.996955	69.473621	66.506049
1393.414118	62.952343	66.511054
1392.909232	68.530000	66.516058
1392.502189	66.030504	66.521063
1392.057023	62.114619	66.526068
1390.542897	72.454367	66.531073
1390.236680	62.971679	66.536078
1390.008762	64.431933	66.541082
1389.388219	62.116189	66.546087
1388.586814	65.342368	66.551092
1387.558233	65.176269	66.556097
1387.122340	64.053346	66.561102
1386.668992	63.836816	66.566106
1385.164603	65.739670	66.571111
1384.942256	56.279927	66.576116
1384.156682	72.934859	66.581121
1383.928469	71.118164	66.586126
1383.206215	60.364316	66.591130
1382.508437	62.988959	66.596135
1381.909670	63.856862	66.601140
1381.035310	61.822745	66.606145
1380.833883	61.165617	66.611150
1379.362437	65.572236	66.616154
1378.799878	60.810821	66.621159
1378.589978	53.061719	66.626164
1377.962849	67.029494	66.631169
1377.337726	56.159285	66.636174
1376.467945	57.817763	66.641178
1375.716171	54.475759	66.646183
1375.168935	53.304304	66.651188
1374.662490	53.865789	66.656193
1373.329688	47.626165	66.661198
1372.753713	50.770779	66.666202
1372.322774	54.666643	66.671207
1372.298587	47.715947	66.676212
1371.415749	54.878632	66.681217
1370.563328	52.713296	66.686222
1369.881435	48.180597	66.691226
1369.558328	55.639096	66.696231
1368.908635	47.171410	66.701236
1367.455199	51.259770	66.706241
1367.049284	45.293873	66.711246
1366.903674	56.638254	66.716250
1365.500434	58.200179	66.721255
1365.152784	46.801738	66.726260
1364.018915	51.331324	66.731265
1363.648916	53.246260	66.736270
1363.390973	55.417781	66.741274
1362.844245	59.776766	66.746279
1362.589488	50.271720	66.751284
1361.075485	57.160991	66.756289
1360.285686	57.991454	66.761294
1360.075252	49.849771	66.766298
1359.485434	55.986568	66.771303
1358.738951	51.615529	66.776308
1357.755232	66.638227	66.781313
1357.565757	61.000628	66.786318
1357.113217	55.966258	66.791322
1355.763277	58.505337	66.796327
1355.187272	58.686789	66.801332
1354.502701	60.192827	66.806337
1354.152703	51.770546	66.811342
1353.923691	58.712606	66.816346
1352.289660	68.858536	66.821351
1352.064450	63.193501	66.826356
1351.675855	65.928279	66.831361
1350.904063	64.466087	66.836366
1349.985823	51.980334	66.841370
1348.938000	60.839290	66.846375
1348.661184	59.262145	66.851380
1347.883813	63.787111	66.856385
1347.489463	54.085053	66.861390
1346.575591	59.924852	66.866394
1345.952182	63.483879	66.871399
1345.833137	61.388054	66.876404
1344.935115	56.306229	66.881409
1343.878845	56.846312	66.886414
1343.401146	61.974939	66.891418
1342.664960	60.811449	66.896423
1342.416669	51.530888	66.901428
1341.537903	59.653325	66.906433
1340.466572	64.991442	66.911438
1340.155256	64.023771	66.916442
1339.548762	69.396809	66.921447
1339.200352	57.380304	66.926452
1338.104490	66.286329	66.931457
1337.401424	59.818875	66.936462
1336.739831	58.397519	66.941466
1336.233863	59.689084	66.946471
1335.818452	53.924978	66.951476
1334.564041	67.707040	66.956481
1334.201242	56.962306	66.961486
1333.333819	64.165134	66.966490
1333.237176	63.638012	66.971495
1332.244627	54.318067	66.976500
1331.456716	66.231351	66.981505
1330.826774	57.993928	66.986510
1330.361162	52.346616	66.991514
1329.240349	63.041764	66.996519
1329.111801	57.309327	67.001524
1328.443499	64.242375	67.006529
1327.650615	65.040222	67.011534
1327.309292	54.162764	67.016538
1325.905312	66.153487	67.021543
1325.384950	55.687700	67.026548
1324.719204	60.021457	67.031553
1324.492178	60.287789	67.036558
1324.102730	59.447662	67.041562
1322.831851	57.864543	67.046567
1322.557821	58.991502	67.051572
1321.725966	55.998146	67.056577
1321.069397	52.055961	67.061582
1320.068618	62.184813	67.066586
1319.316805	54.373634	67.071591
1319.138240	48.474107	67.076596
1318.627917	55.213300	67.081601
1317.770506	57.975302	67.086606
1317.195425	52.632409	67.091610
1316.398486	60.292401	67.096615
1316.197675	55.104479	67.101620
1314.715501	58.719608	67.106625
1314.127077	58.046736	67.111630
1313.697032	54.007038	67.116634
1313.107601	55.488499	67.121639
1312.612541	57.191506	67.126644
1311.476194	71.710191	67.131649
1310.976084	56.790910	67.136654
1310.568878	61.744327	67.141658
1309.718006	60.898709	67.146663
1309.120162	58.964164	67.151668
1308.301331	60.015307	67.156673
1307.732035	57.172607	67.161678
1307.364978	60.454337	67.166682
1306.389949	63.466861	67.171687
1305.725442	49.868437	67.176692
1305.046666	62.876152	67.181697
1304.695763	62.862552	67.186702
1304.193865	59.405150	67.191706
1303.006933	64.752197	67.196711
1302.527597	57.626275	67.201716
1301.564207	61.729806	67.206721
1301.358630	60.682249	67.211726
1300.581473	57.803210	67.216730
1299.305021	61.869779	67.221735
1299.013777	56.152173	67.226740
1298.636998	58.634336	67.231745
1298.338703	57.377588	67.236750
1297.300138	57.140571	67.241754
1296.481561	69.115511	67.246759
1296.132773	59.702694	67.251764
1295.479366	64.223735	67.256769
1294.554913	59.830547	67.261774
1293.745870	61.741176	67.266778
1293.032618	59.837600	67.271783
1292.867442	57.980931	67.276788
1291.482616	59.517890	67.281793
1290.972569	57.895829	67.286798
1290.499003	54.538008	67.291802
1289.774556	59.661715	67.296807
1289.639064	63.259878	67.301812
1289.076007	61.660437	67.306817
1288.001700	55.919094	67.311822
1287.656901	59.791813	67.316826
1286.657963	49.433671	67.321831
1285.543371	53.712636	67.326836
1284.707277	54.981001	67.331841
1284.192874	51.902494	67.336846
1283.656587	49.615963	67.341850
1283.375670	52.578062	67.346855
1283.449938	54.594266	67.351860
1282.180400	55.264478	67.356865
1281.531812	55.071124	67.361870
1281.033450	48.870777	67.366874
1280.029233	53.428670	67.371879
1278.975231	45.659249	67.376884
1278.247246	61.833504	67.381889
1277.906003	53.507621	67.386894
1277.807014	56.592187	67.391898
1277.094045	64.962679	67.396903
1276.111374	53.725145	67.401908
1275.140856	56.449948	67.406913
1274.784033	56.180244	67.411918
1274.624765	57.855101	67.416922
1273.399990	59.913839	67.421927
1272.936762	61.523481	67.426932
1272.029950	62.992333	67.431937
1271.627843	49.183466	67.436942
1270.911441	54.088271	67.441946
1269.478296	64.426235	67.446951
1269.480433	54.968671	67.451956
1269.112201	56.446512	67.456961
1268.276407	67.364454	67.461966
1267.301880	60.061801	67.466970
1266.535357	58.781729	67.471975
1266.441854	54.188625	67.476980
1265.765551	55.016841	67.481985
1264.945087	55.808053	67.486990
1264.137829	52.780845	67.491994
1263.518913	50.699849	67.496999
1263.158752	45.573544	67.502004
1262.127756	61.021676	67.507009
1261.236463	58.998180	67.512014
1260.772587	56.670177	67.517018
1259.995774	60.453889	67.522023
1259.967446	60.433162	67.527028
1258.756989	65.263560	67.532033
1258.077316	58.183696	67.537038
1257.901380	63.357397	67.542042
1257.129030	69.114798	67.547047
1256.316172	66.548962	67.552052
1255.517225	67.806700	67.557057
1254.919968	63.464007	67.562062
1254.583844	56.181283	67.567066
1253.589815	62.388678	67.572071
1252.695045	58.246260	67.577076
1251.826193	58.408065	67.582081
1251.644372	64.418508	67.587086
1251.524061	55.027726	67.592090
1250.288233	64.799723	67.597095
1249.717455	48.997554	67.602100
1249.196486	52.327416	67.607105
1248.824618	53.170309	67.612110
1247.391725	54.751205	67.617114
1246.403733	53.755519	67.622119
1246.370687	52.175898	67.627124
1245.884078	52.005684	67.632129
1245.466591	57.258792	67.637134
1244.396161	56.102746	67.642138
1243.543191	65.260347	67.647143
1243.216831	54.426263	67.652148
1242.190818	57.563613	67.657153
1241.399034	54.936084	67.662158
1240.692877	52.637148	67.667162
1240.255383	58.979986	67.672167
1239.905142	45.758988	67.677172
1239.421356	55.657415	67.682177
1238.392778	50.899177	67.687182
1237.979752	54.404269	67.692186
1236.786336	63.568694	67.697191
1236.923268	49.010212	67.702196
1236.051410	60.094743	67.707201
1234.901009	55.136674	67.712206
1234.556467	60.059634	67.717210
1234.014895	56.108650	67.722215
1232.613964	59.892260	67.727220
1231.475391	58.212455	67.732225
1231.403513	53.869811	67.737230
1231.331406	50.497054	67.742234
1230.692555	60.170977	67.747239
1230.387983	50.596606	67.752244
1229.646236	58.747746	67.757249
1228.618015	49.200133	67.762254
1228.428140	56.258976	67.767258
1226.954412	60.908893	67.772263
1226.278772	49.818113	67.777268
1225.665501	51.257651	67.782273
1225.202586	50.140632	67.787278
1225.038856	48.080309	67.792282
1223.995445	55.377379	67.797287
1223.590629	50.240834	67.802292
1222.670812	65.046812	67.807297
1222.046576	61.345523	67.812302
1221.227760	52.557841	67.817306
1220.053714	59.963998	67.822311
1220.168368	56.736589	67.827316
1219.474049	61.552740	67.832321
1218.346996	55.021860	67.837326
1217.742184	58.008660	67.842330
1217.077485	62.138841	67.847335
1216.876614	55.392874	67.852340
1216.416077	61.914425	67.857345
1214.991987	58.119551	67.862350
1214.632266	54.382512	67.867354
1213.870569	58.665316	67.872359
1213.854114	60.580824	67.877364
1212.495465	69.042965	67.882369
1211.703531	64.404804	67.887374
1211.347566	59.344070	67.892378
1210.349563	70.787728	67.897383
1210.252800	58.748588	67.902388
1209.691822	60.077309	67.907393
1208.483662	63.320910	67.912398
1208.209277	56.610288	67.917402
1207.468337	56.870041	67.922407
1207.090537	53.801369	67.927412
1205.943825	49.210170	67.932417
1205.196999	57.784756	67.937422
1205.115123	51.814672	67.942426
1203.992990	56.667316	67.947431
1203.094791	48.865271	67.952436
1202.556317	60.934454	67.957441
1202.335101	51.449338	67.962446
1201.874022	46.421096	67.967450
1200.609656	60.893926	67.972455
1200.171821	47.407739	67.977460
1199.524608	58.141155	67.982465
1198.734161	49.494055	67.987470
1198.077637	51.949751	67.992474
1196.740857	53.635240	67.997479
1196.522435	51.129443	68.002484
1196.218359	55.224357	68.007489
1195.375136	53.783037	68.012494
1195.255934	56.473416	68.017498
1194.259350	57.228000	68.022503
1193.522082	55.146920	68.027508
1192.840760	47.310390	68.032513
1192.520267	53.273494	68.037518
1191.783713	52.611592	68.042522
1190.821226	53.374948	68.047527
1190.580541	55.376577	68.052532
1189.107839	51.603644	68.057537
1188.654617	50.910879	68.062542
1188.117785	50.620926	68.067546
1187.651625	58.338732	68.072551
1187.360768	46.789377	68.077556
1186.189281	50.743106	68.082561
1185.176241	57.865044	68.087566
1185.319623	48.392916	68.092570
1184.422873	51.016131	68.097575
1183.747241	50.177383	68.102580
1182.593968	54.571351	68.107585
1182.124950	52.338803	68.112590
1181.888178	52.166717	68.117594
1181.191699	62.404914	68.122599
1180.445306	48.748600	68.127604
1179.691643	56.687174	68.132609
1178.806955	52.286134	68.137614
1178.873112	44.113115	68.142618
1177.510300	56.280275	68.147623
1176.870520	52.174610	68.152628
1176.187301	54.177230	68.157633
1175.957392	52.952201	68.162638
1175.435678	50.355864	68.167642
1174.095604	53.623610	68.172647
1173.632088	56.160584	68.177652
1172.946324	59.554515	68.182657
1172.398871	54.921646	68.187662
1171.454601	50.675169	68.192666
1170.690560	60.104075	68.197671
1170.397784	52.760860	68.202676
1169.908007	52.187454	68.207681
1169.177801	57.014053	68.212686
1168.292448	49.989012	68.217690
1167.505165	55.474408	68.222695
1167.263668	49.436672	68.227700
1166.927563	51.775184	68.232705
1165.733105	55.958085	68.237710
1165.241480	56.343785	68.242714
1164.630294	55.647760	68.247719
1164.007446	46.502501	68.252724
1162.725384	57.819445	68.257729
1162.462821	47.639154	68.262734
1161.791323	50.646032	68.267738
1161.419123	58.558637	68.272743
1160.497027	49.435738	68.277748
1159.431646	52.800156	68.282753
1158.712199	52.602333	68.287758
1158.584446	50.880077	68.292762
1158.213937	58.732488	68.297767
1157.477310	39.171966	68.302772
1156.407080	48.673219	68.307777
1155.857267	52.688943	68.312782
1155.577106	51.156510	68.317786
1154.300752	50.829634	68.322791
1153.785172	40.927715	68.327796
1153.158292	49.781281	68.332801
1152.932605	46.568577	68.337806
1152.391447	44.954650	68.342810
1151.042636	54.328322	68.347815
1150.700694	46.910929	68.352820
1150.031056	49.051746	68.357825
1148.950847	53.856741	68.362830
1148.383763	45.525809	68.367834
1147.440506	54.913832	68.372839
1147.266994	43.560296	68.377844
1146.893193	52.089756	68.382849
1146.114821	43.631577	68.387854
1145.165549	39.146207	68.392858
1144.677265	54.479658	68.397863
1144.454378	42.692420	68.402868
1143.438423	46.599351	68.407873
1142.560296	53.745576	68.412878
1142.158269	49.092742	68.417882
1141.327068	52.312686	68.422887
1140.900963	43.725941	68.427892
1139.460940	50.302352	68.432897
1138.784280	55.699196	68.437902
1138.454062	50.464070	68.442906
1137.867127	54.864179	68.447911
1137.811338	43.009364	68.452916
1136.995797	50.525690	68.457921
1135.797566	48.992617	68.462926
1135.643961	42.944064	68.467930
1135.106741	51.009072	68.472935
1134.437368	50.994107	68.477940
1133.195429	51.048130	68.482945
1132.846929	43.062493	68.487950
1132.425205	47.154043	68.492954
1131.230654	45.700814	68.497959
1130.938221	40.450221	68.502964
1130.193724	44.848580	68.507969
1129.683085	47.492405	68.512974
1128.667942	50.951348	68.517978
1127.698085	46.122320	68.522983
1127.419740	48.140981	68.527988
1127.212621	52.302482	68.532993
1126.100679	52.597612	68.537998
1125.524449	49.560517	68.543002
1124.608326	45.426281	68.548007
1124.481631	43.393194	68.553012
1123.597558	46.668861	68.558017
1122.415984	46.186574	68.563022
1121.995278	48.781402	68.568026
1121.132681	60.578861	68.573031
1121.058582	44.767138	68.578036
1120.475947	55.818305	68.583041
1119.765963	57.128166	68.588046
1119.015147	51.292875	68.593050
1118.167717	55.682380	68.598055
1117.812727	51.991917	68.603060
1116.613606	57.028732	68.608065
1115.670920	55.302054	68.613070
1115.766365	47.479201	68.618074
1115.222591	53.775874	68.623079
1114.579657	42.443393	68.628084
1113.177882	54.271414	68.633089
1112.480023	51.565911	68.638094
1112.395269	49.418917	68.643098
1111.816948	58.340467	68.648103
1111.233206	58.069031	68.653108
1110.235519	52.689334	68.658113
1109.592206	45.696787	68.663118
1109.282446	54.955672	68.668122
1108.088850	66.652819	68.673127
1107.695515	55.819959	68.678132
1107.173600	61.993309	68.683137
1106.522706	61.535432	68.688142
1105.534944	57.955079	68.693146
1104.469957	60.728087	68.698151
1104.293548	55.090023	68.703156
1103.981003	56.150587	68.708161
1103.274294	61.328288	68.713166
1102.433566	56.948671	68.718170
1101.535664	49.679644	68.723175
1101.497716	51.229553	68.728180
1100.447327	54.932239	68.733185
1099.160819	54.584927	68.738190
1098.897265	49.818610	68.743194
1098.488443	63.734336	68.748199
1098.210969	58.303164	68.753204
1097.357779	56.065506	68.758209
1096.239242	68.577062	68.763214
1095.835283	57.726970	68.768218
1095.109339	61.647718	68.773223
1094.644237	51.438153	68.778228
1093.529892	61.361198	68.783233
1092.705494	65.275530	68.788238
1092.708814	57.140890	68.793242
1091.838421	64.235440	68.798247
1091.309849	55.718617	68.803252
1090.630305	63.347372	68.808257
1090.005642	66.775761	68.813262
1089.167227	55.904891	68.818266
1087.738810	61.235242	68.823271
1087.191944	53.109271	68.828276
1086.992487	61.290879	68.833281
1086.675315	62.582422	68.838286
1086.513843	56.103026	68.843290
1085.527784	61.967000	68.848295
1084.745099	60.560244	68.853300
1084.088682	66.141545	68.858305
1083.258420	60.997006	68.863310
1082.296729	57.324205	68.868314
1081.253294	61.274958	68.873319
1081.284285	58.458257	68.878324
1080.887420	61.790485	68.883329
1080.402060	58.104995	68.888334
1079.603726	55.588952	68.893338
1078.549898	61.020575	68.898343
1078.058365	56.132825	68.903348
1076.921284	59.054508	68.908353
1076.253830	57.793432	68.913358
1075.992019	51.697439	68.918362
1075.374156	58.595699	68.923367
1074.892973	57.934211	68.928372
1073.908543	65.802285	68.933377
1072.833044	63.109554	68.938382
1072.555448	56.697519	68.943386
1071.992831	64.446453	68.948391
1071.712014	62.917288	68.953396
1070.739743	60.477804	68.958401
1069.967571	68.750518	68.963406
1069.883195	55.504614	68.968410
1068.640416	54.587378	68.973415
1067.794069	60.279319	68.978420
1067.193753	68.614585	68.983425
1066.624845	57.957901	68.988430
1066.409791	51.900205	68.993434
1065.295620	55.679283	68.998439
1064.583212	57.975163	69.003444
1064.230817	53.044783	69.008449
1063.855670	58.349524	69.013454
1062.804177	51.098639	69.018458
1061.772206	59.031047	69.023463
1061.349811	47.056358	69.028468
1061.060345	52.449972	69.033473
1059.906941	51.721954	69.038478
1059.510276	47.383682	69.043482
1058.742941	57.745132	69.048487
1058.295601	53.747664	69.053492
1057.456044	51.110452	69.058497
1056.408445	52.947134	69.063502
1056.053587	51.781419	69.068506
1055.318047	59.985225	69.073511
1055.367427	50.428706	69.078516
1054.205369	53.560956	69.083521
1053.139865	60.191379	69.088526
1052.813256	42.338216	69.093530
1052.202224	45.876406	69.098535
1051.774253	52.960506	69.103540
1050.750153	45.981244	69.108545
1049.655587	63.125340	69.113550
1049.441649	38.014304	69.118554
1049.063302	50.091134	69.123559
1048.771512	42.263655	69.128564
1047.344267	45.196815	69.133569
1046.560990	52.468328	69.138574
1046.389556	48.726601	69.143578
1045.701627	53.227949	69.148583
1044.725931	46.928557	69.153588
1044.027097	51.187207	69.158593
1043.495129	44.984387	69.163598
1043.450786	46.301918	69.168602
1042.126144	52.322270	69.173607
1041.552969	48.907810	69.178612
1041.095335	58.105065	69.183617
1040.397355	50.533018	69.188622
1039.790660	57.524126	69.193626
1038.797742	59.360001	69.198631
1038.419542	55.720553	69.203636
1037.965181	56.868342	69.208641
1037.096599	56.136025	69.213646
1036.491950	45.134956	69.218650
1035.261019	60.269586	69.223655
1035.297070	55.362572	69.228660
1034.449903	57.008100	69.233665
1033.374820	59.735431	69.238670
1032.899835	56.735869	69.243674
1032.109270	59.635561	69.248679
1031.945217	49.709290	69.253684
1031.400374	60.598336	69.258689
1030.244285	68.034830	69.263694
1030.044182	55.565876	69.268698
1029.032087	69.164410	69.273703
1028.002126	58.890178	69.278708
1027.507297	62.993375	69.283713
1026.584248	67.836497	69.288718
1026.523369	53.829910	69.293722
1026.315002	55.753868	69.298727
1025.363481	54.039670	69.303732
1024.379974	57.304381	69.308737
1023.684298	64.386923	69.313742
1023.384878	63.852650	69.318746
1022.468817	72.440012	69.323751
1021.636354	68.078031	69.328756
1020.836520	72.068903	69.333761
1020.608929	64.611259	69.338766
1020.263128	57.314354	69.343770
1019.119811	64.800859	69.348775
1018.701320	51.458310	69.353780
1018.004471	57.254215	69.358785
1016.700318	58.067262	69.363790
1016.123550	54.662841	69.368794
1015.482620	59.628241	69.373799
1015.014714	59.043502	69.378804
1014.749019	57.142924	69.383809
1014.453986	62.416001	69.388814
1013.396055	56.162818	69.393818
1012.369349	59.770305	69.398823
1011.920866	58.972737	69.403828
1011.416894	54.649968	69.408833
1009.911577	68.964080	69.413838
1009.848528	59.499564	69.418842
1009.358862	63.333855	69.423847
1008.653010	69.793535	69.428852
1007.948533	54.914765	69.433857
1006.937555	67.680477	69.438862
1006.486058	58.429155	69.443866
1005.659072	55.853040	69.448871
1005.744404	57.033244	69.453876
1004.979456	60.490276	69.458881
1003.729923	66.948143	69.463886
1003.453080	57.121820	69.468890
1003.070505	70.817330	69.473895
1001.584467	59.163266	69.478900
1000.935701	58.086898	69.483905
1000.608948	57.415048	69.488910
1000.009499	48.095808	69.493914
999.441041	58.917649	69.498919
998.607903	53.923417	69.503924
997.882508	55.284649	69.508929
997.388278	61.748505	69.513934
996.936997	52.837784	69.518938
996.309059	58.752044	69.523943
995.540210	60.743101	69.528948
994.678116	58.033800	69.533953
994.114336	58.694369	69.538958
993.294693	54.421829	69.543962
992.456333	68.576215	69.548967
992.205326	58.774169	69.553972
991.726451	57.531999	69.558977
990.978036	66.494824	69.563982
989.863015	56.937483	69.568986
989.182557	59.855940	69.573991
988.708754	59.641159	69.578996
988.626956	62.448597	69.584001
987.306229	63.940824	69.589006
986.599732	59.120414	69.594010
986.020629	67.516972	69.599015
985.711798	56.516156	69.604020
984.764409	55.171909	69.609025
983.760347	65.164181	69.614030
983.595540	64.543838	69.619034
982.948555	62.136214	69.624039
982.241997	58.063308	69.629044
981.417938	57.481625	69.634049
980.654656	61.720584	69.639054
980.399973	60.005920	69.644058
979.781161	71.460271	69.649063
978.633026	69.972919	69.654068
978.184075	57.004239	69.659073
977.563498	64.935877	69.664078
977.115671	48.406187	69.669082
976.177378	60.698279	69.674087
975.299994	54.627705	69.679092
974.753570	58.302293	69.684097
974.156304	64.478189	69.689102
974.081595	59.662917	69.694106
972.778032	67.654341	69.699111
972.053333	57.605965	69.704116
971.575267	53.380011	69.709121
971.018571	57.113005	69.714126
970.428275	50.266611	69.719130
969.351672	55.419613	69.724135
968.994855	57.554857	69.729140
968.840380	56.213766	69.734145
967.574296	57.180056	69.739150
966.763583	53.898029	69.744154
966.237808	58.012467	69.749159
965.675959	54.679804	69.754164
965.126007	50.712877	69.759169
964.354620	53.082823	69.764174
963.477721	47.631935	69.769178
963.053840	51.408453	69.774183
962.583773	50.015074	69.779188
961.714793	51.835987	69.784193
960.527964	55.789099	69.789198
960.426543	51.709803	69.794202
959.886455	59.537168	69.799207
959.322148	56.860924	69.804212
958.223513	46.460467	69.809217
957.684296	51.736127	69.814222
957.603015	46.335268	69.819226
956.239156	57.726808	69.824231
955.474142	58.588143	69.829236
954.995739	54.337014	69.834241
954.334213	61.120815	69.839246
954.085502	51.051906	69.844250
953.185917	52.746802	69.849255
952.176505	51.932843	69.854260
951.741565	56.370303	69.859265
951.110899	58.650051	69.864270
950.915857	52.352639	69.869274
949.364940	53.521960	69.874279
948.876408	52.850628	69.879284
948.349737	52.213750	69.884289
947.759249	50.773302	69.889294
947.824215	56.053754	69.894298
946.749450	58.063540	69.899303
946.095732	56.180558	69.904308
945.336459	52.152325	69.909313
943.952026	62.605686	69.914318
943.609377	57.654854	69.919322
942.862795	58.637842	69.924327
942.470612	56.087181	69.929332
942.279753	55.890465	69.934337
941.572968	49.368552	69.939342
940.747182	58.597588	69.944346
939.805411	62.242051	69.949351
939.236095	57.343057	69.954356
938.430791	52.946828	69.959361
937.337664	61.152365	69.964366
937.492613	56.764187	69.969370
936.988128	53.004503	69.974375
936.186616	56.543066	69.979380
935.375439	51.135347	69.984385
934.744489	60.166222	69.989390
934.087045	52.215593	69.994394
932.761949	61.106186	69.999399
932.369672	66.192889	70.004404
931.904494	56.306664	70.009409
931.156242	50.600346	70.014414
931.067303	50.616076	70.019418
929.899870	52.896085	70.024423
929.074064	51.702827	70.029428
928.685452	52.493234	70.034433
928.310261	58.408288	70.039438
927.709935	46.545535	70.044442
926.340393	48.979135	70.049447
926.144435	46.608569	70.054452
925.977873	47.507148	70.059457
924.712799	61.191690	70.064462
923.946749	45.256723	70.069466
923.307817	62.112295	70.074471
922.790227	55.934024	70.079476
921.980885	58.420411	70.084481
920.723240	56.556268	70.089486
920.535167	50.942165	70.094490
919.689721	65.930337	70.099495
919.566595	56.910644	70.104500
919.218674	56.313137	70.109505
918.098118	54.151208	70.114510
917.372682	51.240415	70.119514
916.723306	56.645579	70.124519
916.283454	42.615749	70.129524
915.290247	53.043130	70.134529
914.410012	58.702657	70.139534
914.256286	43.900303	70.144538
913.779525	57.866260	70.149543
912.864084	61.005060	70.154548
912.137512	54.890011	70.159553
911.417996	58.577963	70.164558
911.134406	56.151956	70.169562
910.297857	61.470212	70.174567
909.266127	60.174109	70.179572
908.533600	52.555566	70.184577
907.807869	56.996729	70.189582
908.063772	47.979804	70.194586
907.171061	61.436359	70.199591
906.012790	57.585176	70.204596
905.557104	52.698074	70.209601
904.785901	62.735313	70.214606
904.487129	53.532259	70.219610
902.983408	62.815575	70.224615
902.701200	61.425428	70.229620
902.546346	52.699378	70.234625
901.677029	52.492361	70.239630
901.356168	56.282456	70.244634
900.540653	60.859338	70.249639
899.931545	54.414935	70.254644
898.525960	46.689040	70.259649
897.771556	58.024616	70.264654
897.664420	44.673563	70.269658
897.003817	51.088209	70.274663
896.478858	55.603081	70.279668
895.845785	52.594015	70.284673
894.681062	63.629035	70.289678
894.252383	53.262341	70.294682
893.679801	59.801758	70.299687
893.272289	53.993916	70.304692
892.256041	49.295378	70.309697
891.220636	56.875141	70.314702
891.226555	51.635454	70.319706
890.705557	53.285891	70.324711
889.512454	56.483079	70.329716
888.973193	59.122040	70.334721
888.430146	56.327310	70.339726
888.058955	51.377879	70.344730
886.973289	54.460196	70.349735
885.806471	52.641542	70.354740
885.686096	47.568616	70.359745
885.049966	49.887094	70.364750
884.979401	53.145337	70.369754
883.899365	52.700620	70.374759
883.012492	53.198163	70.379764
882.646393	49.867486	70.384769
881.812432	55.866594	70.389774
881.087124	50.565082	70.394778
880.403530	55.311788	70.399783
879.899910	46.210733	70.404788
879.404356	41.650113	70.409793
877.946882	50.167544	70.414798
877.419651	49.543387	70.419802
876.927705	47.598409	70.424807
876.438646	56.800678	70.429812
876.623798	48.135642	70.434817
875.393794	61.494492	70.439822
874.576282	47.602049	70.444826
874.065046	51.934963	70.449831
872.939552	46.632489	70.454836
872.313991	51.645932	70.459841
871.385720	55.395502	70.464846
871.134582	51.715364	70.469850
871.095011	48.987171	70.474855
869.959592	49.448579	70.479860
869.411544	48.137017	70.484865
868.373233	55.409738	70.489870
868.275951	48.887042	70.494874
866.771490	55.535348	70.499879
866.225841	56.814392	70.504884
865.568258	47.084973	70.509889
865.232859	56.890426	70.514894
865.024338	46.996495	70.519898
864.327001	54.684891	70.524903
863.063358	54.007625	70.529908
862.752862	45.951343	70.534913
862.120561	53.176793	70.539918
861.374190	52.016648	70.544922
860.314080	51.447342	70.549927
859.644003	46.416175	70.554932
859.473878	42.904501	70.559937
858.764064	53.403490	70.564942
857.714122	46.146154	70.569946
857.280980	48.301442	70.574951
856.653879	56.995816	70.579956
856.392757	46.761745	70.584961
855.720798	52.058548	70.589966
854.955696	45.818767	70.594970
854.283302	48.061021	70.599975
853.684811	50.662104	70.604980
852.862240	40.287159	70.609985
851.861523	46.016338	70.614990
851.279904	45.410305	70.619994
850.329480	55.632196	70.624999
849.608184	51.948042	70.630004
848.901747	52.440533	70.635009
848.441807	57.385043	70.640014
848.137463	54.951309	70.645018
847.907692	61.160200	70.650023
847.243325	53.773686	70.655028
846.551110	51.352801	70.660033
845.811014	60.049393	70.665038
844.820237	50.795643	70.670042
844.084733	53.167796	70.675047
843.339955	58.428884	70.680052
842.925255	53.808091	70.685057
841.893267	53.038771	70.690062
840.966105	41.762672	70.695066
840.668246	55.589766	70.700071
840.178735	56.358398	70.705076
840.113307	40.076992	70.710081
838.766891	57.794238	70.715086
838.265718	50.181478	70.720090
837.538020	56.292997	70.725095
837.203892	53.723654	70.730100
835.977317	57.446597	70.735105
835.295266	56.463883	70.740110
834.965443	42.416568	70.745114
834.326274	49.069092	70.750119
833.836154	50.793474	70.755124
832.726373	46.997693	70.760129
832.132720	52.335654	70.765134
831.750166	49.319849	70.770138
830.700717	50.313227	70.775143
829.680648	51.478552	70.780148
829.347963	54.196609	70.785153
828.593806	52.071022	70.790158
828.365481	46.829200	70.795162
828.163311	50.977307	70.800167
826.931715	53.120915	70.805172
826.368752	48.604152	70.810177
825.690077	57.469169	70.815182
825.353848	43.236791	70.820186
824.272266	47.695188	70.825191
823.514133	57.217839	70.830196
822.796753	43.468761	70.835201
822.221142	50.076478	70.840206
821.868838	44.080093	70.845210
820.807754	49.784199	70.850215
820.011589	45.608916	70.855220
820.027559	43.753419	70.860225
819.138431	55.108874	70.865230
818.279002	53.736499	70.870234
817.611231	54.205496	70.875239
817.190242	51.165849	70.880244
816.916592	45.139598	70.885249
815.610514	52.951706	70.890254
815.172733	44.341673	70.895258
814.301820	52.341562	70.900263
814.011418	44.406675	70.905268
813.269127	46.762568	70.910273
812.002383	50.865659	70.915278
811.832567	53.179316	70.920282
811.116400	51.333122	70.925287
810.603909	52.335657	70.930292
810.046505	51.903978	70.935297
809.532731	50.512857	70.940302
808.179484	52.349402	70.945306
807.530611	55.278643	70.950311
806.464131	61.259590	70.955316
806.266734	49.537750	70.960321
806.055080	55.696445	70.965326
805.695714	44.952889	70.970330
804.360808	46.352846	70.975335
803.522251	53.199544	70.980340
803.508710	51.386592	70.985345
802.704753	56.065740	70.990350
802.020077	41.317968	70.995354
800.766841	42.480995	71.000359
800.316366	48.212493	71.005364
800.514285	47.972827	71.010369
799.053745	61.141314	71.015374
798.387227	54.267680	71.020378
798.157792	45.201855	71.025383
797.178907	48.223053	71.030388
796.600836	48.171566	71.035393
795.579139	49.699869	71.040398
795.081226	36.764292	71.045402
794.608556	50.098801	71.050407
794.210398	57.856285	71.055412
793.125613	52.025387	71.060417
792.139150	59.138491	71.065422
791.702763	46.669361	71.070426
791.201146	43.708788	71.075431
791.124868	45.769432	71.080436
790.378897	48.302539	71.085441
789.284978	50.153007	71.090446
788.729106	48.151991	71.095450
788.096891	47.688070	71.100455
787.134533	48.107774	71.105460
786.682410	45.237096	71.110465
785.936416	54.045024	71.115470
785.658630	49.416643	71.120474
784.469494	59.749095	71.125479
783.701335	47.572482	71.130484
783.411987	49.304338	71.135489
782.743331	53.230233	71.140494
782.230893	48.106185	71.145498
781.212335	48.140592	71.150503
780.425436	50.740143	71.155508
780.337827	38.962992	71.160513
779.486947	53.534141	71.165518
778.349192	47.501946	71.170522
777.706233	54.705452	71.175527
777.261607	52.308254	71.180532
777.229768	48.452868	71.185537
776.440795	56.709390	71.190542
775.516094	46.711861	71.195546
774.521821	52.821673	71.200551
774.060314	62.372813	71.205556
773.912361	42.794466	71.210561
772.524241	55.197633	71.215566
772.033599	56.180928	71.220570
771.288632	56.108706	71.225575
770.797373	56.172718	71.230580
770.487316	61.413507	71.235585
769.375213	61.283033	71.240590
768.916712	42.115255	71.245594
768.396898	42.663215	71.250599
767.474676	48.838830	71.255604
766.732648	48.692023	71.260609
765.614967	53.957298	71.265614
765.655702	50.539799	71.270618
765.065810	54.953063	71.275623
764.399693	54.545009	71.280628
763.758166	49.132428	71.285633
763.137745	49.578132	71.290638
762.395783	46.884490	71.295642
761.326847	56.489747	71.300647
760.767267	60.896611	71.305652
760.435082	46.362402	71.310657
759.363121	50.650555	71.315662
758.523501	48.354090	71.320666
758.070426	52.029624	71.325671
757.374244	48.231114	71.330676
757.341349	46.602598	71.335681
756.705537	53.667773	71.340686
756.012581	49.953907	71.345690
754.749961	47.357347	71.350695
754.484083	60.130657	71.355700
753.556773	49.349792	71.360705
752.637994	60.378820	71.365710
752.252471	55.373348	71.370714
751.663262	57.597654	71.375719
751.105988	52.367209	71.380724
749.895508	55.797463	71.385729
748.978408	63.079316	71.390734
749.108128	58.157400	71.395738
748.648314	53.487038	71.400743
748.166185	57.203470	71.405748
747.407849	52.154849	71.410753
746.609025	53.888968	71.415758
746.037435	50.537414	71.420762
744.433005	49.424021	71.425767
743.766549	51.539199	71.430772
743.778309	42.406601	71.435777
743.012241	63.371541	71.440782
742.949750	55.122828	71.445786
742.008970	49.365227	71.450791
741.071183	58.925959	71.455796
740.556851	45.125666	71.460801
740.188193	51.823453	71.465806
739.112572	44.530841	71.470810
737.998545	52.038012	71.475815
737.196470	49.476951	71.480820
737.218474	49.006662	71.485825
736.785821	59.048381	71.490830
735.884118	47.473380	71.495834
735.225453	47.147728	71.500839
734.322571	51.014727	71.505844
734.144232	45.302906	71.510849
732.740617	53.879645	71.515854
732.339391	49.810253	71.520858
731.463912	50.009561	71.525863
731.189748	49.360915	71.530868
731.250192	49.549992	71.535873
729.734715	52.808035	71.540878
729.213989	54.340186	71.545882
728.634478	48.838894	71.550887
727.909361	55.624974	71.555892
726.904205	49.596926	71.560897
726.264594	55.188233	71.565902
725.996768	54.253145	71.570906
725.349145	54.007740	71.575911
724.553377	55.023853	71.580916
723.713527	52.154991	71.585921
723.106830	59.359045	71.590926
722.425583	47.458787	71.595930
722.266211	53.952941	71.600935
721.125816	48.914695	71.605940
720.788179	52.089298	71.610945
719.922719	50.858269	71.615950
719.457195	54.367054	71.620954
718.514847	43.787304	71.625959
717.799136	56.860891	71.630964
717.860386	50.860184	71.635969
716.721716	56.283365	71.640974
715.621280	42.849217	71.645978
714.874001	48.598018	71.650983
714.325262	55.460099	71.655988
714.199551	54.365188	71.660993
713.801839	67.990564	71.665998
712.922645	58.496754	71.671002
712.129183	54.887214	71.676007
711.269662	55.899289	71.681012
711.123953	47.909843	71.686017
709.738056	54.791671	71.691022
709.325290	46.609776	71.696026
708.950973	46.508522	71.701031
708.047076	58.370990	71.706036
707.438434	51.887150	71.711041
706.555983	55.449702	71.716046
706.532120	45.734564	71.721050
705.964349	47.386175	71.726055
704.487826	51.554256	71.731060
703.975449	44.299718	71.736065
703.355648	54.129955	71.741070
702.927460	48.886857	71.746074
702.106225	53.348005	71.751079
701.119703	47.889447	71.756084
700.586420	41.953443	71.761089
700.350771	48.753058	71.766094
699.932454	47.165410	71.771098
698.812061	51.153786	71.776103
697.784011	55.960108	71.781108
697.438709	49.136293	71.786113
696.963706	60.302838	71.791118
695.934530	48.858541	71.796122
695.305287	50.732835	71.801127
694.461564	52.141375	71.806132
694.282849	45.839828	71.811137
693.502501	55.995257	71.816142
693.313531	42.915899	71.821146
691.928638	49.166781	71.826151
691.412768	55.954246	71.831156
691.352134	40.589911	71.836161
690.123679	51.589407	71.841166
689.521867	54.091704	71.846170
688.870225	51.517747	71.851175
688.238755	51.235086	71.856180
687.790166	46.600801	71.861185
686.584169	53.993323	71.866190
686.176533	52.400822	71.871194
685.544624	53.422395	71.876199
685.086252	46.269653	71.881204
684.343550	47.810347	71.886209
683.214372	55.384608	71.891214
682.859524	53.783702	71.896218
682.313609	49.738935	71.901223
681.953024	47.536537	71.906228
681.275866	47.108186	71.911233
680.054360	48.952205	71.916238
679.306461	51.591308	71.921242
679.060534	48.604240	71.926247
678.370932	56.513795	71.931252
677.643774	46.335046	71.936257
676.805074	52.692936	71.941262
676.351710	51.011522	71.946266
675.748996	43.195779	71.951271
674.732331	53.942359	71.956276
674.643881	50.367234	71.961281
673.398628	46.755530	71.966286
673.476196	48.851603	71.971290
672.626924	40.896923	71.976295
671.818029	50.484454	71.981300
671.605434	45.358425	71.986305
670.368619	46.976225	71.991310
669.698784	40.495837	71.996314
668.740812	44.810028	72.001319
668.404931	47.995395	72.006324
668.506104	32.294644	72.011329
667.256499	59.530953	72.016334
666.488701	42.224418	72.021338
665.990971	45.219510	72.026343
664.946572	51.614887	72.031348
664.291974	45.638284	72.036353
663.414100	46.399402	72.041358
663.027173	47.000342	72.046362
662.709645	45.948595	72.051367
661.888541	58.009205	72.056372
661.116829	44.199463	72.061377
660.479747	48.894653	72.066382
660.068943	46.641907	72.071386
659.792728	51.175555	72.076391
658.660697	45.402713	72.081396
657.858350	39.613648	72.086401
657.050580	50.725942	72.091406
655.616954	53.278699	72.096410
655.226980	45.515820	72.101415
654.977524	44.842748	72.106420
654.632340	39.863995	72.111425
654.242585	49.744338	72.116430
653.907956	51.704194	72.121434
652.778866	45.886731	72.126439
652.039649	40.551247	72.131444
651.806793	34.565843	72.136449
650.607526	42.769447	72.141454
649.773392	41.837813	72.146458
649.389492	41.007952	72.151463
648.478813	51.338684	72.156468
647.866076	40.304354	72.161473
646.602449	58.700777	72.166478
646.333449	52.962400	72.171482
646.054187	47.280854	72.176487
645.505892	48.924645	72.181492
645.205478	52.367724	72.186497
643.829200	55.586303	72.191502
643.383764	47.015382	72.196506
642.698554	47.297964	72.201511
641.678156	54.153161	72.206516
641.065373	40.756524	72.211521
640.372691	51.759030	72.216526
639.831160	51.862613	72.221530
639.934703	38.739845	72.226535
638.950423	44.188929	72.231540
638.168228	42.741240	72.236545
637.336969	46.861796	72.241550
636.996550	45.264909	72.246554
635.974296	46.940022	72.251559
634.805476	48.875023	72.256564
634.615933	45.465814	72.261569
634.157725	51.953937	72.266574
633.665112	46.752655	72.271578
632.683271	46.715041	72.276583
631.803857	54.452977	72.281588
631.539227	49.571786	72.286593
631.299859	51.029187	72.291598
630.329730	48.141683	72.296602
629.334209	46.562386	72.301607
628.613976	39.918148	72.306612
628.531154	42.732053	72.311617
627.494127	56.351993	72.316622
626.588374	52.621592	72.321626
626.231657	49.116001	72.326631
625.864942	56.425357	72.331636
624.622782	46.314450	72.336641
623.668640	55.832084	72.341646
623.116978	56.514458	72.346650
622.809943	45.899813	72.351655
622.199385	54.042798	72.356660
622.062275	46.182887	72.361665
620.753025	59.713718	72.366670
620.183478	54.677654	72.371674
619.926139	43.741279	72.376679
618.696844	48.295818	72.381684
617.818323	42.422702	72.386689
616.969105	49.157603	72.391694
616.746813	47.081428	72.396698
616.456033	50.890410	72.401703
616.040663	58.852501	72.406708
615.369879	45.537647	72.411713
614.351059	45.969562	72.416718
613.717068	47.546581	72.421722
612.727354	53.458598	72.426727
611.540777	57.815526	72.431732
611.444446	48.277521	72.436737
610.699623	44.340147	72.441742
610.792483	42.417214	72.446746
610.370938	41.795208	72.451751
609.331857	54.396750	72.456756
608.823957	44.615205	72.461761
607.573962	59.000788	72.466766
606.420815	54.278448	72.471770
606.083110	44.348371	72.476775
605.550662	43.903303	72.481780
605.269526	52.339185	72.486785
604.332497	51.616345	72.491790
603.589084	49.935406	72.496794
603.099615	46.332688	72.501799
602.409904	53.739216	72.506804
602.194127	47.404159	72.511809
600.933982	53.718800	72.516814
600.019959	52.252694	72.521818
599.776872	53.851041	72.526823
599.302963	55.806277	72.531828
598.706012	41.631259	72.536833
597.426674	48.579748	72.541838
597.170729	48.606317	72.546842
596.913760	46.467857	72.551847
595.462474	50.707673	72.556852
594.879212	40.594356	72.561857
594.302418	49.798003	72.566862
593.907024	46.175573	72.571866
593.365842	44.788865	72.576871
592.070332	50.300151	72.581876
591.973941	48.927760	72.586881
591.210685	60.690587	72.591886
590.761458	50.689960	72.596890
589.697798	46.866451	72.601895
589.073376	54.555902	72.606900
588.556640	42.791930	72.611905
588.269655	56.424893	72.616910
586.972763	49.856737	72.621914
586.314388	45.211732	72.626919
585.661228	54.347119	72.631924
585.449533	46.204197	72.636929
584.780315	48.088036	72.641934
583.825124	49.698872	72.646938
583.136802	40.280392	72.651943
582.413703	43.920105	72.656948
582.403135	45.691159	72.661953
581.403741	44.930951	72.666958
580.506742	47.596981	72.671962
580.483578	45.534828	72.676967
578.963405	46.022951	72.681972
578.533961	46.987073	72.686977
577.540661	45.707070	72.691982
577.311126	49.129402	72.696986
576.792812	50.971862	72.701991
575.586278	55.686804	72.706996
575.137210	52.336282	72.712001
574.365368	56.190347	72.717006
574.158070	47.603594	72.722010
573.744915	39.394991	72.727015
572.515239	51.342488	72.732020
572.101538	45.825873	72.737025
571.423206	47.373694	72.742030
571.001399	42.375620	72.747034
569.623338	41.366641	72.752039
568.910883	45.707995	72.757044
568.865537	42.577030	72.762049
568.051398	51.115151	72.767054
567.408827	45.576642	72.772058
566.618741	44.934493	72.777063
565.834261	48.811073	72.782068
565.518244	39.617158	72.787073
565.080376	50.312581	72.792078
564.411938	50.545205	72.797082
563.467582	50.815467	72.802087
562.819556	51.716633	72.807092
562.062656	39.229244	72.812097
561.110634	47.423468	72.817102
560.613690	44.848564	72.822106
560.480724	45.669271	72.827111
559.261578	56.703606	72.832116
558.551263	44.877434	72.837121
557.726861	51.718787	72.842126
557.442416	51.070222	72.847130
556.994022	47.408932	72.852135
556.363965	52.713317	72.857140
555.445567	39.745444	72.862145
554.494455	43.535023	72.867150
554.025501	40.077287	72.872154
553.566301	50.328247	72.877159
552.929663	42.715071	72.882164
552.428630	45.759594	72.887169
551.445565	47.217183	72.892174
550.832522	37.927078	72.897178
550.491086	45.626652	72.902183
549.358790	50.906953	72.907188
548.964894	40.258856	72.912193
548.555822	43.317118	72.917198
547.575340	45.236351	72.922202
546.736074	48.691147	72.927207
546.018934	51.021030	72.932212
545.780264	46.071063	72.937217
545.498377	51.491883	72.942222
544.375143	50.533792	72.947226
543.486739	45.496502	72.952231
542.780649	44.112417	72.957236
542.383981	42.645932	72.962241
541.175179	53.110911	72.967246
540.390430	50.182878	72.972250
540.022548	39.786111	72.977255
539.687900	43.433348	72.982260
539.454147	38.481024	72.987265
538.490758	47.416667	72.992270
537.700326	43.215343	72.997274
537.141131	45.926929	73.002279
536.565888	50.667489	73.007284
535.668914	45.688339	73.012289
535.011933	49.830051	73.017294
534.630708	47.908513	73.022298
534.101027	43.071136	73.027303
532.750788	38.235152	73.032308
532.279637	40.076415	73.037313
531.840827	46.165636	73.042318
530.854507	43.488915	73.047322
530.005837	47.725818	73.052327
529.405342	45.572699	73.057332
529.154345	47.580749	73.062337
528.297830	57.527567	73.067342
528.301934	46.360328	73.072346
527.133521	52.775508	73.077351
525.913026	50.822075	73.082356
525.597430	48.560496	73.087361
525.344572	42.873190	73.092366
524.543686	49.054782	73.097370
523.759851	52.936003	73.102375
522.871446	49.340078	73.107380
522.756881	46.480343	73.112385
521.888568	50.837074	73.117390
520.653939	50.557493	73.122394
520.519344	40.904174	73.127399
519.879098	44.562244	73.132404
519.635374	39.291385	73.137409
518.185005	48.946436	73.142414
517.229787	37.678124	73.147418
517.376205	41.184076	73.152423
516.563469	48.056696	73.157428
516.103147	41.621836	73.162433
514.711014	42.338765	73.167438
514.109007	46.293526	73.172442
514.046386	43.983767	73.177447
513.392080	43.610170	73.182452
512.913394	40.871518	73.187457
512.173839	50.192568	73.192462
511.184356	47.569976	73.197466
510.769908	42.230116	73.202471
509.822955	48.231549	73.207476
509.148477	37.595044	73.212481
508.480079	50.560193	73.217486
508.077379	49.097827	73.222490
507.671677	41.663926	73.227495
506.477061	52.140851	73.232500
506.094661	42.216343	73.237505
505.589855	40.711896	73.242510
504.225529	42.171888	73.247514
503.595057	45.374236	73.252519
502.798819	44.704702	73.257524
502.644754	40.436713	73.262529
502.105953	42.176793	73.267534
501.734161	39.720741	73.272538
500.878069	35.665512	73.277543
499.688983	45.900277	73.282548
499.595995	37.613883	73.287553
498.552758	49.724097	73.292558
497.267879	41.714304	73.297562
497.168556	38.697600	73.302567
496.524876	42.772544	73.307572
496.269075	46.577539	73.312577
495.902316	45.186722	73.317582
494.877976	39.228077	73.322586
494.262882	42.716563	73.327591
493.644522	42.491789	73.332596
492.906008	40.488403	73.337601
491.661476	46.322777	73.342606
491.219127	43.732884	73.347610
490.735775	43.849309	73.352615
490.180133	46.418410	73.357620
489.748698	28.536417	73.362625
489.138079	38.278477	73.367630
488.432144	38.939723	73.372634
487.522599	34.918247	73.377639
486.443696	41.166212	73.382644
486.115483	41.448737	73.387649
485.453692	50.142383	73.392654
484.724317	38.070121	73.397658
484.129726	36.557904	73.402663
483.313005	44.812597	73.407668
482.795585	40.268176	73.412673
482.525523	44.676271	73.417678
481.265666	35.500273	73.422682
480.723114	34.385050	73.427687
480.147527	37.526618	73.432692
480.014323	39.444941	73.437697
478.608720	35.750079	73.442702
477.945786	43.135014	73.447706
477.479690	42.551668	73.452711
476.874193	45.852547	73.457716
476.656686	43.061255	73.462721
475.146165	43.661447	73.467726
474.750772	41.179197	73.472730
474.421886	39.429108	73.477735
473.869565	43.254533	73.482740
472.955759	48.310819	73.487745
471.944888	44.485264	73.492750
471.606313	41.954538	73.497754
471.329932	39.879113	73.502759
470.038095	44.658150	73.507764
469.306260	35.820668	73.512769
468.859322	38.437111	73.517774
468.341244	49.205242	73.522778
468.071155	45.033011	73.527783
466.874486	41.194481	73.532788
466.496411	31.693508	73.537793
465.760504	43.287980	73.542798
465.103470	41.208543	73.547802
464.248685	37.996802	73.552807
463.346887	41.663436	73.557812
462.967555	31.607570	73.562817
462.402404	43.184300	73.567822
461.443239	45.297292	73.572826
460.612715	38.776344	73.577831
459.983463	41.670996	73.582836
459.685884	32.764336	73.587841
459.265829	38.013200	73.592846
458.757187	38.251933	73.597850
457.943269	35.062070	73.602855
457.143720	46.617799	73.607860
456.570080	35.201994	73.612865
455.557285	42.519667	73.617870
454.391707	40.625334	73.622874
454.303090	38.761274	73.627879
453.596908	42.543405	73.632884
453.765502	42.666358	73.637889
452.524796	43.242501	73.642894
451.656323	47.894173	73.647898
451.324187	36.301119	73.652903
450.497735	51.549685	73.657908
450.010325	42.562877	73.662913
448.916911	52.061744	73.667918
448.262544	44.826748	73.672922
447.987292	46.680971	73.677927
447.018765	43.331236	73.682932
446.386745	34.425822	73.687937
445.866733	33.401635	73.692942
445.393107	35.112417	73.697946
445.022382	39.935526	73.702951
443.601309	47.231519	73.707956
443.262602	33.868572	73.712961
442.923856	36.653863	73.717966
442.079520	40.095304	73.722970
441.192591	36.923387	73.727975
440.163376	45.779657	73.732980
439.867426	41.277233	73.737985
439.183729	45.754387	73.742990
437.802206	43.952814	73.747994
437.553213	43.795363	73.752999
436.968804	51.297111	73.758004
437.064509	36.844646	73.763009
436.622968	39.485465	73.768014
435.498409	38.174394	73.773018
434.559740	38.596765	73.778023
433.962328	48.494433	73.783028
433.455501	39.319911	73.788033
432.673353	42.667867	73.793038
431.486444	39.359242	73.798042
431.831441	31.400475	73.803047
430.730263	42.982186	73.808052
430.070099	36.618615	73.813057
429.198362	36.532000	73.818062
428.753123	41.102051	73.823066
428.332857	32.583958	73.828071
427.132884	42.938755	73.833076
426.506940	37.342451	73.838081
425.891131	42.996253	73.843086
425.646282	41.541869	73.848090
424.946723	43.556739	73.853095
423.744153	45.519290	73.858100
423.321346	44.586853	73.863105
422.926543	37.107083	73.868110
421.929452	39.566758	73.873114
421.276978	31.516180	73.878119
420.452480	43.457517	73.883124
420.039778	35.890713	73.888129
419.740290	36.815229	73.893134
418.538336	41.625700	73.898138
418.110597	31.486094	73.903143
417.479515	33.737640	73.908148
417.238184	33.780823	73.913153
416.117959	36.662248	73.918158
415.315382	45.130749	73.923162
415.245372	36.765010	73.928167
414.035889	36.339548	73.933172
413.122704	26.211062	73.938177
412.689028	37.465642	73.943182
411.920387	37.849892	73.948186
411.804443	32.273260	73.953191
410.730532	42.376161	73.958196
409.703185	38.849732	73.963201
409.116628	42.360498	73.968206
408.790824	36.799956	73.973210
408.867223	33.014083	73.978215
408.000035	49.127019	73.983220
406.822526	33.757777	73.988225
406.501638	34.983753	73.993230
405.565804	30.793033	73.998234
404.836846	36.062737	74.003239
403.669096	38.114366	74.008244
403.527849	34.391558	74.013249
403.002075	35.539792	74.018254
402.167898	42.516781	74.023258
401.704821	42.081205	74.028263
400.693138	38.430857	74.033268
400.510763	37.028024	74.038273
399.966502	40.224541	74.043278
398.864659	43.303321	74.048282
398.632818	39.535022	74.053287
397.503397	48.538163	74.058292
397.047505	42.807536	74.063297
395.988715	37.595606	74.068302
395.391398	35.850454	74.073306
395.238599	40.984201	74.078311
394.528528	50.502428	74.083316
393.303520	39.239320	74.088321
392.716502	45.410520	74.093326
392.380608	40.971240	74.098330
392.026093	43.718050	74.103335
391.051116	33.422794	74.108340
390.286730	40.532169	74.113345
389.644592	43.648090	74.118350
389.082010	36.940973	74.123354
388.716244	36.953523	74.128359
387.526760	47.404439	74.133364
387.026490	42.165017	74.138369
386.677876	40.320313	74.143374
385.606077	42.571129	74.148378
384.718077	40.960610	74.153383
383.674883	44.424294	74.158388
383.457212	43.963810	74.163393
383.197948	47.767786	74.168398
382.730377	41.868710	74.173402
382.301437	44.236291	74.178407
381.137986	48.105499	74.183412
380.527610	40.888750	74.188417
379.947074	41.031720	74.193422
378.984844	36.293275	74.198426
378.675691	35.918333	74.203431
377.976286	44.867149	74.208436
377.444361	44.351084	74.213441
376.016838	44.545442	74.218446
375.356303	41.003156	74.223450
375.107974	39.393212	74.228455
374.643620	51.545261	74.233460
374.075739	39.974021	74.238465
373.174749	43.315699	74.243470
371.912720	41.438353	74.248474
371.870710	32.736995	74.253479
371.322316	44.842505	74.258484
371.041926	37.401287	74.263489
369.877985	42.776588	74.268494
369.044879	48.436643	74.273498
369.037415	41.196363	74.278503
367.769086	44.593427	74.283508
366.841328	38.464909	74.288513
366.451821	41.146333	74.293518
365.805749	39.877319	74.298522
365.836769	34.315120	74.303527
364.657804	44.587745	74.308532
364.274077	42.231391	74.313537
363.444804	47.081849	74.318542
362.098742	40.327699	74.323546
361.592303	37.776433	74.328551
360.891563	49.496212	74.333556
360.356224	44.979908	74.338561
360.227496	40.909750	74.343566
359.680316	48.153259	74.348570
358.842256	42.862015	74.353575
357.962249	52.284327	74.358580
357.783676	40.879715	74.363585
356.423420	40.875705	74.368590
355.624220	37.335022	74.373594
355.065289	39.532507	74.378599
354.257349	48.009764	74.383604
354.233393	40.407833	74.388609
353.722265	45.005741	74.393614
352.966016	47.521681	74.398618
352.817592	38.058255	74.403623
351.409183	54.202261	74.408628
350.600748	43.057297	74.413633
349.473762	42.787457	74.418638
349.364535	49.377695	74.423642
349.214764	39.488700	74.428647
347.996823	44.725956	74.433652
347.430331	41.731671	74.438657
346.911022	40.831974	74.443662
346.024999	45.264121	74.448666
345.543313	43.014846	74.453671
344.367785	42.779552	74.458676
344.113655	36.442768	74.463681
343.472763	44.800362	74.468686
342.836428	43.783696	74.473690
341.974819	39.705753	74.478695
341.135993	44.396887	74.483700
340.470066	43.097928	74.488705
340.358796	43.519366	74.493710
339.733019	41.985348	74.498714
338.895957	34.749547	74.503719
337.993182	47.331013	74.508724
337.914444	39.889204	74.513729
337.203100	41.272032	74.518734
336.011948	52.453375	74.523738
335.602665	43.189218	74.528743
334.953594	46.068133	74.533748
334.219316	48.837624	74.538753
333.061918	45.391879	74.543758
332.358861	44.769054	74.548762
331.762913	35.189294	74.553767
331.583949	51.015944	74.558772
331.444992	42.702201	74.563777
330.536869	43.674839	74.568782
329.628251	39.844092	74.573786
329.298482	44.291674	74.578791
328.455454	48.048337	74.583796
327.496919	41.355453	74.588801
326.729805	42.005994	74.593806
326.246034	43.637989	74.598810
325.970620	36.836239	74.603815
324.585549	44.001971	74.608820
324.035170	38.379463	74.613825
323.478380	43.711638	74.618830
322.770145	44.825889	74.623834
323.072103	37.992047	74.628839
321.706103	39.179588	74.633844
320.755963	35.293961	74.638849
320.429289	42.502331	74.643854
320.096460	42.963811	74.648858
319.143830	39.159007	74.653863
318.106718	41.584098	74.658868
317.954864	42.324246	74.663873
317.037688	39.223431	74.668878
315.515860	47.264107	74.673882
315.090533	37.057909	74.678887
314.790215	42.060624	74.683892
314.635771	47.967352	74.688897
314.379744	47.680146	74.693902
313.261536	45.073424	74.698906
312.592429	38.291842	74.703911
311.841097	42.975348	74.708916
311.554493	39.573761	74.713921
310.454870	43.459634	74.718926
309.347086	39.942917	74.723930
309.415304	37.344232	74.728935
308.400285	41.024230	74.733940
307.253133	49.585524	74.738945
307.253981	44.595842	74.743950
306.436564	43.133377	74.748954
306.323425	31.593773	74.753959
305.075809	48.994243	74.758964
304.553788	43.176405	74.763969
304.168209	45.120765	74.768974
302.921917	48.181606	74.773978
302.188673	48.410436	74.778983
301.694834	45.030840	74.783988
301.311640	39.663970	74.788993
300.754127	42.521992	74.793998
300.078269	51.624772	74.799002
299.197272	43.957587	74.804007
298.517196	60.081733	74.809012
298.095493	48.174974	74.814017
297.139027	42.998823	74.819022
296.393447	57.638435	74.824026
296.080148	48.376334	74.829031
295.439173	51.635597	74.834036
294.852506	41.839898	74.839041
293.657329	53.496568	74.844046
292.662879	50.292957	74.849050
292.754257	41.023134	74.854055
292.069631	40.602389	74.859060
291.558934	41.806591	74.864065
290.701017	45.608216	74.869070
289.917256	47.691738	74.874074
289.576611	42.185622	74.879079
288.462263	46.400285	74.884084
287.306380	44.340483	74.889089
287.175349	40.775330	74.894094
286.520318	50.562352	74.899098
286.543002	45.862508	74.904103
285.565598	49.667411	74.909108
284.798361	46.536401	74.914113
283.921916	48.809741	74.919118
283.167419	42.458098	74.924122
282.541924	42.750185	74.929127
281.578993	43.827771	74.934132
281.128657	44.484607	74.939137
280.456491	43.814295	74.944142
280.004931	43.241286	74.949146
280.103603	34.031808	74.954151
279.093199	49.590421	74.959156
278.578847	44.665512	74.964161
277.346404	40.075837	74.969166
275.898366	40.806540	74.974170
275.473344	37.745571	74.979175
274.803452	45.413932	74.984180
274.811242	33.615356	74.989185
274.539769	50.048109	74.994190
273.992777	45.782847	74.999194
273.563208	37.878141	75.004199
272.335981	46.466401	75.009204
271.436195	41.585583	75.014209
270.121641	42.856416	75.019214
269.445217	42.541605	75.024218
269.271057	39.464305	75.029223
268.794509	45.291485	75.034228
268.689241	36.707454	75.039233
267.816251	38.846204	75.044238
266.842046	46.041094	75.049242
266.573243	36.205782	75.054247
265.420226	46.769202	75.059252
264.400716	39.830597	75.064257
263.919215	34.649720	75.069262
263.479091	42.787666	75.074266
263.292737	36.569405	75.079271
262.463583	53.291327	75.084276
261.581706	47.947180	75.089281
261.079114	37.045252	75.094286
260.507369	48.121580	75.099290
259.430676	41.988462	75.104295
258.613281	42.164485	75.109300
258.361663	49.570635	75.114305
257.914678	40.323549	75.119310
256.536879	37.516957	75.124314
256.058682	29.227345	75.129319
255.217394	44.009941	75.134324
255.012583	44.766418	75.139329
254.664412	39.056504	75.144334
253.981645	55.882832	75.149338
252.946980	34.345453	75.154343
251.874627	44.588509	75.159348
251.675131	43.478581	75.164353
251.530458	37.775655	75.169358
250.339767	48.769292	75.174362
249.828549	43.586845	75.179367
248.989376	47.808124	75.184372
248.201650	43.287927	75.189377
247.395551	38.190333	75.194382
246.691498	55.811694	75.199386
246.412143	38.547367	75.204391
245.497304	44.996354	75.209396
245.293165	39.195673	75.214401
244.033757	31.437449	75.219406
243.266131	45.315740	75.224410
243.222945	31.051027	75.229415
242.792660	47.859177	75.234420
242.447965	31.988279	75.239425
241.273712	37.349505	75.244430
240.218536	41.475905	75.249434
239.667000	35.039889	75.254439
238.644374	43.001029	75.259444
238.187108	42.017348	75.264449
237.803052	34.523296	75.269454
237.409721	40.466524	75.274458
236.960168	32.744791	75.279463
235.575331	45.250155	75.284468
235.157864	42.672120	75.289473
234.835019	38.825308	75.294478
233.691035	42.287770	75.299482
233.119807	46.575153	75.304487
232.751011	44.400948	75.309492
231.964277	40.374192	75.314497
231.047984	41.141584	75.319502
229.923084	41.683606	75.324506
229.971833	43.196037	75.329511
229.402003	49.096441	75.334516
228.824589	45.485754	75.339521
227.931342	45.962465	75.344526
226.823974	54.575797	75.349530
226.872099	44.675774	75.354535
226.079319	41.212962	75.359540
225.007745	46.272397	75.364545
224.426562	40.987569	75.369550
223.558555	41.567491	75.374554
223.395085	34.738454	75.379559
222.718411	41.949005	75.384564
222.023849	34.261602	75.389569
221.260309	35.958714	75.394574
220.739635	35.387273	75.399578
220.452348	34.548390	75.404583
219.117018	42.718659	75.409588
218.519878	36.941208	75.414593
218.071760	41.349317	75.419598
217.296601	42.152563	75.424602
216.723243	41.124314	75.429607
216.068470	41.146692	75.434612
215.635810	44.383802	75.439617
214.455384	41.534732	75.444622
213.583299	44.682618	75.449626
213.541412	35.262159	75.454631
212.990767	41.848641	75.459636
212.287423	36.424017	75.464641
211.106233	43.424837	75.469646
210.410096	41.919416	75.474650
210.234489	32.502929	75.479655
209.474512	51.139311	75.484660
208.493896	37.177006	75.489665
207.859564	39.643588	75.494670
207.239444	47.758196	75.499674
207.067190	44.385704	75.504679
205.999650	44.795589	75.509684
205.199268	46.859708	75.514689
204.953726	40.882703	75.519694
204.355409	48.101270	75.524698
203.896338	44.470147	75.529703
202.434226	52.269551	75.534708
201.824738	49.253772	75.539713
201.297623	43.731669	75.544718
200.793597	56.345800	75.549722
200.426088	43.708182	75.554727
199.225150	56.080174	75.559732
198.650103	47.843855	75.564737
198.268970	45.974402	75.569742
197.402275	48.525340	75.574746
196.479458	41.002066	75.579751
196.037534	52.194905	75.584756
195.770347	44.450411	75.589761
195.160667	43.006906	75.594766
194.218160	50.518471	75.599770
193.580405	39.743768	75.604775
192.847793	35.585395	75.609780
192.229693	37.036976	75.614785
191.367764	37.365203	75.619790
190.214131	53.531732	75.624794
190.123477	38.960770	75.629799
189.498814	45.434477	75.634804
188.830001	45.930615	75.639809
188.813567	46.130357	75.644814
187.633452	46.870438	75.649818
187.288135	46.365666	75.654823
186.432103	43.983716	75.659828
185.261846	43.403878	75.664833
184.390753	37.922428	75.669838
183.706652	46.799455	75.674842
183.573207	42.723758	75.679847
183.238738	44.324091	75.684852
182.894859	41.658639	75.689857
181.901111	40.476645	75.694862
181.060230	43.597490	75.699866
180.329784	33.790065	75.704871
179.430568	40.089921	75.709876
178.570499	40.193925	75.714881
178.208178	37.080402	75.719886
177.495604	42.210353	75.724890
177.536933	36.409973	75.729895
176.477124	43.984395	75.734900
175.501443	42.670212	75.739905
175.084606	40.655067	75.744910
174.507590	44.205360	75.749914
173.488291	41.073575	75.754919
172.931085	36.849396	75.759924
172.324586	40.622011	75.764929
172.079185	43.168521	75.769934
171.315244	47.133398	75.774938
170.465233	30.841611	75.779943
169.910073	40.827190	75.784948
169.362199	42.245504	75.789953
168.314753	46.004843	75.794958
167.424164	49.232968	75.799962
167.366909	39.658841	75.804967
166.756275	42.323506	75.809972
165.591253	43.952180	75.814977
165.037518	34.517138	75.819982
164.205035	42.362830	75.824986
164.164697	40.502128	75.829991
163.165189	44.550296	75.834996
162.152343	47.826300	75.840001
161.913353	43.157144	75.845006
161.241136	50.251882	75.850010
160.898545	43.247978	75.855015
159.716016	44.310160	75.860020
159.356933	46.247162	75.865025
159.088291	42.054248	75.870030
157.430528	48.178585	75.875034
156.573490	43.902864	75.880039
155.876495	51.532993	75.885044
155.620895	42.409964	75.890049
155.404096	42.417722	75.895054
154.816026	46.788230	75.900058
154.397521	37.517711	75.905063
153.417970	44.779722	75.910068
152.666061	46.727316	75.915073
151.891926	42.842084	75.920078
150.604090	47.988069	75.925082
150.377654	37.912635	75.930087
149.770870	42.270356	75.935092
149.454864	40.720116	75.940097
149.154994	40.654386	75.945102
147.546969	48.160109	75.950106
147.165092	40.228907	75.955111
146.698143	46.358928	75.960116
146.545203	44.711724	75.965121
145.531820	32.937211	75.970126
144.464461	43.685713	75.975130
144.233366	41.918505	75.980135
143.072423	47.537853	75.985140
142.085771	40.988311	75.990145
141.758825	35.049531	75.995150
141.062674	46.456370	76.000154
140.945129	35.641324	76.005159
140.387028	46.559368	76.010164
139.211569	39.648844	76.015169
138.578274	41.035052	76.020174
138.158534	46.059974	76.025178
137.911690	41.008871	76.030183
137.008913	42.016996	76.035188
136.062151	38.064677	76.040193
135.645632	40.690513	76.045198
134.832716	41.386263	76.050202
133.728975	41.947033	76.055207
132.922720	46.148905	76.060212
132.603489	44.607066	76.065217
132.401241	43.611129	76.070222
131.481498	34.576660	76.075226
130.859965	39.184321	76.080231
130.276171	40.942688	76.085236
129.830931	41.430001	76.090241
128.873876	35.864510	76.095246
127.569042	33.762305	76.100250
127.580361	36.370386	76.105255
126.834618	26.724701	76.110260
126.299785	37.044512	76.115265
125.526683	36.762504	76.120270
124.770902	42.342485	76.125274
124.733744	34.446213	76.130279
123.403513	40.020019	76.135284
122.632565	40.202874	76.140289
122.392204	30.309445	76.145294
121.458653	38.595466	76.150298
120.865377	35.028342	76.155303
119.732996	35.946926	76.160308
118.889889	39.322036	76.165313
118.869965	39.885038	76.170318
118.380526	41.965834	76.175322
118.142457	34.786004	76.180327
116.969182	39.675612	76.185332
116.436216	36.114642	76.190337
116.002732	34.907995	76.195342
114.596099	41.563174	76.200346
114.219687	37.838467	76.205351
113.134448	45.188307	76.210356
112.965362	44.606559	76.215361
112.738767	36.104975	76.220366
111.651877	41.036005	76.225370
110.910030	37.965665	76.230375
109.940260	44.462876	76.235380
109.427529	43.615800	76.240385
109.516492	39.681267	76.245390
108.111565	50.024714	76.250394
107.447665	39.982773	76.255399
107.052942	50.455298	76.260404
106.566163	48.571168	76.265409
105.722780	45.081775	76.270414
104.790734	46.323239	76.275418
104.534138	45.031616	76.280423
103.903068	42.057155	76.285428
102.844871	44.356383	76.290433
101.922328	41.105122	76.295438
101.136132	50.998245	76.300442
101.404311	37.207454	76.305447
101.096341	47.107896	76.310452
99.897360	44.263419	76.315457
99.117573	43.230270	76.320462
98.467741	44.034068	76.325466
97.771525	41.060536	76.330471
96.904987	48.050652	76.335476
95.884767	45.969311	76.340481
95.622506	43.412286	76.345486
95.161766	44.105507	76.350490
94.912374	38.097596	76.355495
93.583727	44.183681	76.360500
92.960999	44.694573	76.365505
92.441996	37.401848	76.370510
92.187039	49.708179	76.375514
91.347816	41.286942	76.380519
90.279175	43.513722	76.385524
89.719206	39.061346	76.390529
89.673681	33.986034	76.395534
88.276577	37.725466	76.400538
87.358042	34.722735	76.405543
87.016073	43.111552	76.410548
86.659086	40.929182	76.415553
86.416799	40.226644	76.420558
84.910368	45.510021	76.425562
84.734130	41.007491	76.430567
83.796197	40.280267	76.435572
83.269433	42.332327	76.440577
82.529379	39.252249	76.445582
81.869816	40.111220	76.450586
81.551381	38.780576	76.455591
80.964026	37.615820	76.460596
80.082242	38.248452	76.465601
79.272050	35.323065	76.470606
78.474636	46.367589	76.475610
77.816621	38.740641	76.480615
76.965791	41.870989	76.485620
76.085833	28.668583	76.490625
76.322794	36.187629	76.495630
75.363327	38.556278	76.500634
74.881850	33.749188	76.505639
73.651441	41.853904	76.510644
73.117915	45.572326	76.515649
72.861736	40.038592	76.520654
71.996084	45.927849	76.525658
70.999616	38.996704	76.530663
70.155686	42.845052	76.535668
69.698059	45.124212	76.540673
69.554519	35.537053	76.545678
68.830843	43.545192	76.550682
68.329774	37.605808	76.555687
67.461595	43.665781	76.560692
66.843539	40.982571	76.565697
66.720229	37.772604	76.570702
65.036917	42.363524	76.575706
64.688555	43.245412	76.580711
64.227845	42.818985	76.585716
63.414928	42.932857	76.590721
62.738815	36.925195	76.595726
61.898390	40.476516	76.600730
61.649671	44.649418	76.605735
61.399287	43.943442	76.610740
59.971074	38.495698	76.615745
59.412901	36.449499	76.620750
58.697244	47.197135	76.625754
58.481451	39.745676	76.630759
57.227269	40.906066	76.635764
56.459992	45.972230	76.640769
56.034069	33.601025	76.645774
55.324408	43.928230	76.650778
54.985584	41.503270	76.655783
53.808898	47.456329	76.660788
53.019201	45.800295	76.665793
52.975863	34.963968	76.670798
52.342253	43.609034	76.675802
51.914736	36.142458	76.680807
50.995853	41.447268	76.685812
50.240846	41.548755	76.690817
49.903062	28.930107	76.695822
48.484238	41.522971	76.700826
47.831260	36.360035	76.705831
47.224287	39.230725	76.710836
47.075795	35.952235	76.715841
46.612904	36.454994	76.720846
45.400901	49.141039	76.725850
44.924437	36.902476	76.730855
44.465620	37.412470	76.735860
43.496122	40.516022	76.740865
42.729953	29.214657	76.745870
41.852105	42.771508	76.750874
41.378665	42.009644	76.755879
40.677897	45.147611	76.760884
40.708156	40.020790	76.765889
40.115794	33.141910	76.770894
38.944160	43.974884	76.775898
38.775369	41.855550	76.780903
37.828854	43.512513	76.785908
36.927498	40.913919	76.790913
36.231834	35.119122	76.795918
35.867872	42.476957	76.800922
35.151348	43.620995	76.805927
34.239938	48.882043	76.810932
33.468389	38.409442	76.815937
33.475482	43.705349	76.820942
32.386034	48.543780	76.825946
31.679029	43.928786	76.830951
31.179321	38.607367	76.835956
30.454530	43.679376	76.840961
29.854022	44.276628	76.845966
28.414720	40.100133	76.850970
28.166894	40.546517	76.855975
27.687963	37.074724	76.860980
27.314539	39.064491	76.865985
26.816780	29.579569	76.870990
25.470234	37.893640	76.875994
24.985757	39.137867	76.880999
24.448099	42.005392	76.886004
23.821175	35.788047	76.891009
22.775527	38.531587	76.896014
22.196011	48.084252	76.901018
21.819665	47.122401	76.906023
21.487140	51.318136	76.911028
20.754305	51.386133	76.916033
19.910693	44.124698	76.921038
19.269514	47.201127	76.926042
18.829210	43.232736	76.931047
17.499666	45.644664	76.936052
16.731292	37.910759	76.941057
16.607520	42.872719	76.946062
15.903434	42.597084	76.951066
15.214064	48.403048	76.956071
14.390147	42.195045	76.961076
13.611096	38.329572	76.966081
13.274754	31.069242	76.971086
12.638386	45.407609	76.976090
12.282293	38.470550	76.981095
11.387137	34.141045	76.986100
10.501627	41.108977	76.991105
10.049243	43.150765	76.996110
8.716822	37.717738	77.001114
8.255089	39.131807	77.006119
7.536265	34.116583	77.011124
7.532894	40.461263	77.016129
7.110552	42.641765	77.021134
5.677165	39.741685	77.026139
5.013982	39.254523	77.031143
4.538912	41.159581	77.036148
4.222877	38.937578	77.041153
4.017907	38.661185	77.046158