Fri Mar 05 18:41:50 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.088292	97.962267	0.000000
-0.984776	89.286609	0.005005
-1.806886	58.248907	0.010010
-3.623926	7.493889	0.015014
-7.368494	-9.272792	0.020019
-12.805615	1.250178	0.025024
-17.676155	-0.196472	0.030029
-22.091778	-11.027635	0.035034
-26.368998	3.003602	0.040038
-29.987096	-5.851090	0.045043
-33.804411	-1.309241	0.050048
-37.321452	-1.416860	0.055053
-41.164359	-4.646919	0.060058
-44.479867	-8.910429	0.065062
-48.472110	-6.302397	0.070067
-52.245105	-10.158604	0.075072
-56.072119	-5.993646	0.080077
-59.895287	1.141702	0.085082
-63.513645	-13.344222	0.090086
-67.456562	-5.702483	0.095091
-71.177972	-9.229419	0.100096
-74.924106	-5.963587	0.105101
-78.585618	-6.231026	0.110106
-82.046722	-4.242260	0.115110
-86.002343	-9.813398	0.120115
-90.003532	-4.105143	0.125120
-93.601646	-17.209671	0.130125
-97.508502	-6.159520	0.135130
-101.079046	-2.792349	0.140134
-105.062301	-2.620487	0.145139
-108.929605	-4.151311	0.150144
-112.329558	-7.346266	0.155149
-116.590963	0.633371	0.160154
-120.038811	-11.044289	0.165158
-123.795828	-5.239318	0.170163
-127.519733	-1.379284	0.175168
-130.916658	-19.536890	0.180173
-135.080887	-0.150809	0.185178
-138.716881	-4.544404	0.190182
-142.384243	-9.322497	0.195187
-146.411920	-0.361386	0.200192
-149.851765	4.112529	0.205197
-153.787817	2.739403	0.210202
-157.561750	-11.212186	0.215206
-161.514379	-11.767365	0.220211
-165.673302	-7.604473	0.225216
-169.295235	-1.239089	0.230221
-173.361592	4.724129	0.235226
-176.980090	-1.190813	0.240230
-180.255377	-2.156819	0.245235
-184.075093	-1.039515	0.250240
-187.901750	-1.559558	0.255245
-191.531800	3.234926	0.260250
-194.742534	3.550168	0.265254
-198.634000	0.682928	0.270259
-203.246800	-9.040933	0.275264
-206.687588	-3.382495	0.280269
-210.517190	6.471209	0.285274
-214.462424	2.016691	0.290278
-217.816398	-8.882588	0.295283
-221.667294	4.161563	0.300288
-225.013445	-2.304547	0.305293
-229.417943	7.487967	0.310298
-232.975979	-3.987434	0.315302
-236.768692	0.375756	0.320307
-240.346950	-3.556962	0.325312
-244.069499	4.406279	0.330317
-247.854021	1.763326	0.335322
-251.742380	6.392542	0.340326
-255.460698	-12.503636	0.345331
-259.405214	-1.250109	0.350336
-262.776338	-12.760017	0.355341
-266.894529	0.957641	0.360346
-270.114052	-7.277458	0.365350
-273.881082	2.864395	0.370355
-278.156083	-2.598674	0.375360
-281.955472	-2.172014	0.380365
-286.092014	0.858407	0.385370
-289.569687	-0.824201	0.390374
-293.339352	-15.397555	0.395379
-296.953270	-12.225032	0.400384
-300.230295	-2.388438	0.405389
-304.445425	2.419174	0.410394
-308.179323	-5.396298	0.415398
-311.963424	-2.217086	0.420403
-315.542684	-4.020636	0.425408
-319.319983	-13.290997	0.430413
-323.310591	2.984709	0.435418
-326.992475	4.539131	0.440422
-330.893869	4.124286	0.445427
-334.841546	-4.745118	0.450432
-338.079280	-2.574027	0.455437
-342.082733	-7.820127	0.460442
-346.211902	5.336438	0.465446
-349.602300	-10.533704	0.470451
-353.292915	-4.485100	0.475456
-356.700073	-3.297766	0.480461
-360.762174	-3.718446	0.485466
-364.462169	-7.592114	0.490470
-368.236089	-0.180313	0.495475
-372.234052	-6.209408	0.500480
-375.618470	-1.833919	0.505485
-379.611131	0.434097	0.510490
-383.532711	-2.718190	0.515494
-387.031323	-4.469852	0.520499
-391.525663	4.443149	0.525504
-394.408174	-1.841269	0.530509
-398.544709	-7.032908	0.535514
-402.118451	-0.121372	0.540518
-405.790994	-5.707201	0.545523
-409.716685	9.615255	0.550528
-413.505778	-2.300783	0.555533
-417.449365	-1.327336	0.560538
-421.457886	1.061552	0.565542
-424.691834	-7.901152	0.570547
-428.722463	1.264302	0.575552
-432.148071	0.152332	0.580557
-436.171235	-4.106439	0.585562
-439.925325	4.639563	0.590566
-443.351696	-8.400358	0.595571
-447.454666	0.581134	0.600576
-451.010059	-6.008927	0.605581
-454.832567	4.998337	0.610586
-458.392089	-4.869544	0.615590
-462.583306	-0.387181	0.620595
-466.252667	-7.012634	0.625600
-469.933632	-0.817165	0.630605
-473.582788	-3.326828	0.635610
-477.559729	1.736356	0.640614
-480.788847	-13.683087	0.645619
-485.215227	8.945039	0.650624
-488.914360	-6.924467	0.655629
-492.655758	-1.615023	0.660634
-496.100448	0.436365	0.665638
-499.653137	-15.633118	0.670643
-504.037425	9.312744	0.675648
-507.560631	0.513045	0.680653
-511.245954	6.456962	0.685658
-515.266446	-4.332268	0.690662
-518.874610	-3.145719	0.695667
-522.679841	-6.734247	0.700672
-526.432701	-4.720331	0.705677
-530.385567	3.146071	0.710682
-533.992275	-2.159910	0.715686
-537.240960	5.573536	0.720691
-541.547460	-0.675648	0.725696
-545.179113	4.021837	0.730701
-549.133783	-10.322832	0.735706
-552.907619	1.276043	0.740710
-556.467345	-6.710342	0.745715
-560.225741	12.523270	0.750720
-563.683443	-2.335999	0.755725
-567.686256	0.605730	0.760730
-571.026667	-8.647262	0.765734
-575.038796	-8.447931	0.770739
-578.968203	-1.974497	0.775744
-582.990839	-7.595583	0.780749
-586.519778	-3.264529	0.785754
-590.468613	0.006083	0.790758
-593.986281	-6.296467	0.795763
-598.053476	-0.195229	0.800768
-601.824380	-0.732977	0.805773
-605.503013	-0.919606	0.810778
-609.127563	-1.846575	0.815782
-612.623793	-7.942784	0.820787
-616.604295	-3.388164	0.825792
-620.306760	-3.671887	0.830797
-624.344411	0.649026	0.835802
-628.139976	-8.032850	0.840806
-631.787470	-2.711390	0.845811
-635.460078	-3.384636	0.850816
-639.145013	-3.638014	0.855821
-642.736874	-1.119783	0.860826
-646.950384	-5.510203	0.865830
-650.432551	-5.601994	0.870835
-654.401435	-4.632001	0.875840
-658.077645	-13.613589	0.880845
-662.075119	-5.798204	0.885850
-665.536536	0.105435	0.890854
-668.991908	-9.147964	0.895859
-672.918515	-1.421153	0.900864
-676.848286	-5.902584	0.905869
-680.582019	-6.543916	0.910874
-684.393914	-2.732060	0.915878
-688.275844	-6.770107	0.920883
-691.983426	-3.586763	0.925888
-695.506507	-3.679835	0.930893
-699.560044	6.142570	0.935898
-703.102567	-10.812871	0.940902
-706.853625	-7.378131	0.945907
-710.934851	4.438827	0.950912
-714.530135	-9.404726	0.955917
-718.267956	-0.990498	0.960922
-721.793705	0.355075	0.965926
-725.494752	-9.827226	0.970931
-729.631022	-0.832071	0.975936
-733.174225	-4.473163	0.980941
-737.174279	-6.440639	0.985946
-740.915182	2.720015	0.990950
-744.477113	-7.653220	0.995955
-748.476619	2.340399	1.000960
-751.819811	-1.816752	1.005965
-755.527253	-8.374150	1.010970
-759.631695	-4.457078	1.015974
-763.660225	-3.748606	1.020979
-767.412804	-0.274104	1.025984
-770.856202	-5.173725	1.030989
-774.579227	2.892873	1.035994
-778.030319	-6.004651	1.040998
-781.831283	-3.399178	1.046003
-786.077828	-1.200301	1.051008
-789.444857	-3.338245	1.056013
-793.661605	3.140454	1.061018
-797.623080	-0.507806	1.066022
-800.959552	0.556897	1.071027
-804.682469	6.086213	1.076032
-808.489132	-6.013988	1.081037
-812.306476	-0.535802	1.086042
-815.890335	0.764004	1.091046
-819.785391	-5.637146	1.096051
-823.766318	0.554753	1.101056
-827.097177	-0.962869	1.106061
-830.913542	-9.623728	1.111066
-835.102803	-3.524667	1.116070
-838.725946	-1.813272	1.121075
-842.220234	2.165685	1.126080
-845.873073	-14.565297	1.131085
-850.000338	-6.063393	1.136090
-854.013489	-10.925427	1.141094
-857.220395	-1.745884	1.146099
-861.333612	-7.853469	1.151104
-864.637176	-7.595026	1.156109
-868.281506	-11.748020	1.161114
-872.312695	1.775336	1.166118
-876.210345	-7.927430	1.171123
-880.233768	15.034316	1.176128
-883.714364	-12.289695	1.181133
-887.285912	1.533942	1.186138
-891.298655	11.283905	1.191142
-894.804027	-6.229089	1.196147
-898.752992	1.585233	1.201152
-902.489707	7.769760	1.206157
-906.346198	2.018600	1.211162
-910.124571	7.946449	1.216166
-913.839755	2.831875	1.221171
-917.719769	3.835408	1.226176
-921.311460	-0.630271	1.231181
-925.092068	5.671694	1.236186
-929.123388	2.471641	1.241190
-932.420634	-1.768284	1.246195
-936.147366	-1.886783	1.251200
-939.867027	-1.531745	1.256205
-944.049281	-1.935366	1.261210
-948.071349	-3.558341	1.266214
-951.492308	1.566527	1.271219
-955.387926	-1.465942	1.276224
-958.541883	-1.352714	1.281229
-962.579881	-2.646688	1.286234
-966.462852	-3.516014	1.291238
-970.161110	-10.998616	1.296243
-974.504555	7.778755	1.301248
-977.796282	0.609622	1.306253
-981.444227	-3.022223	1.311258
-984.954729	-9.039879	1.316262
-988.649794	-8.311807	1.321267
-992.709845	-4.147549	1.326272
-996.623518	-9.767980	1.331277
-1000.142764	-9.254085	1.336282
-1004.079765	-4.896598	1.341286
-1007.930923	-4.326460	1.346291
-1011.814267	-1.335288	1.351296
-1015.436959	-8.714783	1.356301
-1019.396067	-3.202565	1.361306
-1023.013416	-1.217427	1.366310
-1026.444814	-15.208082	1.371315
-1030.391356	-4.965448	1.376320
-1034.293094	-0.003271	1.381325
-1038.035827	-5.682510	1.386330
-1041.711792	-8.330493	1.391334
-1045.228493	-6.132761	1.396339
-1049.227677	-0.924742	1.401344
-1053.219820	-1.301803	1.406349
-1056.974810	0.189740	1.411354
-1060.655071	4.873689	1.416358
-1063.866926	-8.615864	1.421363
-1068.394910	-6.467664	1.426368
-1071.632062	-10.699649	1.431373
-1075.460708	-13.029845	1.436378
-1079.458489	2.489634	1.441382
-1082.884351	-12.703450	1.446387
-1086.955818	3.477528	1.451392
-1090.111769	-17.861484	1.456397
-1094.330483	-10.675487	1.461402
-1098.273502	-3.837927	1.466406
-1102.342931	-1.017115	1.471411
-1105.872112	12.818977	1.476416
-1109.237718	-5.748910	1.481421
-1112.557097	-0.034518	1.486426
-1116.749789	-4.247632	1.491430
-1120.461031	-6.290608	1.496435
-1124.735192	-0.420316	1.501440
-1128.389390	-6.597687	1.506445
-1132.202219	-8.310581	1.511450
-1135.736890	-20.378010	1.516454
-1139.178457	-9.489018	1.521459
-1143.457100	-5.664849	1.526464
-1146.951029	-12.955915	1.531469
-1150.774582	-1.250439	1.536474
-1154.776486	3.281683	1.541478
-1157.841825	-17.076666	1.546483
-1161.891038	-9.004620	1.551488
-1165.870242	-10.217758	1.556493
-1169.861799	-10.867523	1.561498
-1173.884071	-2.690954	1.566502
-1177.269612	-26.233917	1.571507
-1180.799712	-12.771334	1.576512
-1184.660025	-17.187304	1.581517
-1188.127206	-9.506375	1.586522
-1192.174622	0.963967	1.591526
-1195.866533	-11.158636	1.596531
-1199.694708	1.206817	1.601536
-1203.439992	-9.169446	1.606541
-1207.102410	-4.368283	1.611546
-1211.279156	-1.151647	1.616550
-1214.616779	-7.786380	1.621555
-1218.217028	-6.253108	1.626560
-1221.863649	-1.522258	1.631565
-1225.881511	-6.103762	1.636570
-1230.225447	-7.718897	1.641574
-1233.504152	-6.328514	1.646579
-1237.312940	-4.520572	1.651584
-1241.084945	-2.060925	1.656589
-1244.963467	3.106036	1.661594
-1248.545263	-1.248743	1.666598
-1252.055543	-3.839323	1.671603
-1256.013141	0.684300	1.676608
-1259.681767	-3.593487	1.681613
-1263.522160	-0.361198	1.686618
-1267.641910	1.154359	1.691622
-1271.201051	-7.237821	1.696627
-1274.883114	-3.928350	1.701632
-1278.652790	-4.533011	1.706637
-1282.733382	-2.970078	1.711642
-1286.216180	-1.794539	1.716646
-1290.091569	-10.285885	1.721651
-1293.375604	-3.370546	1.726656
-1297.285995	-8.577820	1.731661
-1300.853786	-7.489582	1.736666
-1305.240835	-2.192256	1.741670
-1308.711537	-11.081070	1.746675
-1312.805248	-7.719852	1.751680
-1316.518102	-1.119046	1.756685
-1319.814279	-8.968188	1.761690
-1323.543703	-5.037632	1.766694
-1327.141731	-7.085777	1.771699
-1330.969553	-2.718417	1.776704
-1335.032782	-10.264995	1.781709
-1338.981871	-8.617357	1.786714
-1342.818126	-4.363746	1.791718
-1346.348627	-4.114030	1.796723
-1350.244350	-7.093768	1.801728
-1353.733909	-9.961893	1.806733
-1357.405764	-8.729180	1.811738
-1361.608676	-8.447504	1.816742
-1365.090365	-14.220014	1.821747
-1369.042476	-10.237973	1.826752
-1372.855535	-9.233366	1.831757
-1376.661698	-6.296530	1.836762
-1380.505539	-14.455298	1.841766
-1383.994338	-5.004461	1.846771
-1387.639308	-6.562452	1.851776
-1391.342527	-8.803389	1.856781
-1395.255473	-1.896045	1.861786
-1399.156280	-7.096791	1.866790
-1402.543695	-4.031407	1.871795
-1406.631592	-1.229191	1.876800
-1410.436953	-7.731978	1.881805
-1413.903596	-3.756617	1.886810
-1417.735699	2.524395	1.891814
-1421.323743	-10.596880	1.896819
-1425.127046	1.195659	1.901824
-1428.888770	-1.029544	1.906829
-1432.752866	-9.033595	1.911834
-1436.802330	2.900873	1.916838
-1440.533130	0.710162	1.921843
-1444.617496	-2.417407	1.926848
-1447.819842	0.243102	1.931853
-1451.326203	-2.366721	1.936858
-1455.513736	-2.360147	1.941862
-1459.246468	-6.884383	1.946867
-1462.998940	0.369535	1.951872
-1466.800454	-10.607540	1.956877
-1470.369625	-0.195971	1.961882
-1474.357491	1.956419	1.966886
-1477.834589	-7.282759	1.971891
-1481.832442	-9.156254	1.976896
-1485.346507	-9.637502	1.981901
-1489.043264	-11.229616	1.986906
-1493.262743	-3.605987	1.991910
-1496.647099	-18.424985	1.996915
-1501.050735	-7.282865	2.006912
-1501.865697	-1.804417	2.016909
-1498.970048	-7.795983	2.026906
-1496.202190	-4.448088	2.036902
-1494.131882	-1.588498	2.046899
-1492.259513	-1.608805	2.056896
-1490.340546	-9.911878	2.066893
-1488.522823	-16.195040	2.076890
-1486.814124	-7.454358	2.086886
-1484.665489	-2.140972	2.096883
-1482.777901	-1.803707	2.106880
-1480.898126	-11.568925	2.116877
-1478.789037	-6.026570	2.126874
-1477.082969	-5.311287	2.136870
-1475.329818	-6.285128	2.146867
-1473.229762	-6.455561	2.156864
-1471.268670	-9.752179	2.166861
-1469.604053	-10.809736	2.176858
-1467.581488	-9.453539	2.186854
-1465.852935	-7.156575	2.196851
-1463.811664	-2.296508	2.206848
-1462.186565	-8.064074	2.216845
-1460.052940	-9.907247	2.226842
-1458.179436	-7.216641	2.236838
-1456.588378	-11.376112	2.246835
-1454.246437	-7.456286	2.256832
-1452.228213	-12.585729	2.266829
-1450.673111	-9.793614	2.276826
-1449.138213	-11.784076	2.286822
-1446.892508	-12.094647	2.296819
-1445.049728	-6.531728	2.306816
-1443.269550	-0.140883	2.316813
-1440.980243	-4.052134	2.326810
-1439.377376	-8.674540	2.336806
-1437.527290	-3.021203	2.346803
-1435.527774	-5.056043	2.356800
-1433.956096	-9.963980	2.366797
-1431.668478	-8.618605	2.376794
-1429.908978	-6.039198	2.386790
-1428.118499	-7.601615	2.396787
-1426.040470	-8.638484	2.406784
-1424.126048	-12.199172	2.416781
-1422.533687	-5.465610	2.426778
-1420.929937	-4.962853	2.436774
-1418.737540	-4.383804	2.446771
-1416.756169	-11.466804	2.456768
-1414.888599	-3.698867	2.466765
-1412.793560	-9.405843	2.476762
-1411.269821	-9.678169	2.486758
-1409.365814	-14.225604	2.496755
-1407.508887	-4.829632	2.506752
-1405.391574	-8.664367	2.516749
-1403.336180	-7.832844	2.526746
-1401.461053	-6.325089	2.536742
-1399.859427	-7.086721	2.546739
-1398.416684	-4.159738	2.556736
-1396.266480	-1.385478	2.566733
-1394.067942	-5.796894	2.576730
-1392.141403	-3.763674	2.586726
-1390.518188	-6.505610	2.596723
-1388.694468	-8.701743	2.606720
-1386.671999	-7.681775	2.616717
-1384.901343	-3.946743	2.626714
-1382.971869	-2.482409	2.636710
-1381.124374	-6.316563	2.646707
-1379.044632	-6.335237	2.656704
-1377.446356	0.853735	2.666701
-1375.456764	-1.818944	2.676698
-1373.654700	-5.099501	2.686694
-1371.816631	-5.445802	2.696691
-1369.866632	-6.665812	2.706688
-1368.040481	-4.761766	2.716685
-1365.840938	-3.842755	2.726682
-1364.080483	-1.321870	2.736678
-1362.379464	-1.611488	2.746675
-1360.519530	0.610844	2.756672
-1358.457040	-3.316129	2.766669
-1356.597658	1.052099	2.776666
-1354.616822	-2.528641	2.786662
-1352.987167	-5.740534	2.796659
-1351.209751	-5.421842	2.806656
-1349.281027	-4.489468	2.816653
-1347.292211	0.795952	2.826650
-1345.179152	-1.181196	2.836646
-1343.475415	-2.759665	2.846643
-1341.713008	-7.615967	2.856640
-1339.763889	-5.578421	2.866637
-1337.849909	-4.048411	2.876634
-1335.988854	-7.870490	2.886630
-1334.022463	-6.194128	2.896627
-1332.078751	-9.233639	2.906624
-1330.543455	-3.536142	2.916621
-1328.548549	-2.140655	2.926618
-1326.590404	-7.359856	2.936614
-1324.970135	-5.588614	2.946611
-1322.810210	-3.425318	2.956608
-1320.877514	-4.187779	2.966605
-1319.147680	-9.351485	2.976602
-1317.390617	-8.045818	2.986598
-1315.314031	-4.143375	2.996595
-1313.561802	-0.324808	3.006592
-1311.492712	-4.535431	3.016589
-1309.788131	-6.707699	3.026586
-1307.589254	-5.693789	3.036582
-1305.968889	2.413815	3.046579
-1304.254793	3.058470	3.056576
-1302.301921	-0.940914	3.066573
-1300.247828	1.949874	3.076570
-1298.416726	0.317895	3.086566
-1296.550510	-1.888127	3.096563
-1294.847610	-3.654324	3.106560
-1292.974521	0.928082	3.116557
-1290.779434	-2.882685	3.126554
-1288.766512	-3.376903	3.136550
-1287.365431	-7.569021	3.146547
-1285.550024	-4.709497	3.156544
-1283.328610	-1.736524	3.166541
-1281.494720	-8.446868	3.176538
-1279.708029	-5.985379	3.186534
-1277.668563	-6.066990	3.196531
-1276.039793	-6.444458	3.206528
-1274.337427	-4.541053	3.216525
-1272.260137	1.808707	3.226522
-1270.338667	-1.576147	3.236518
-1268.179327	-3.233787	3.246515
-1266.451245	-7.104009	3.256512
-1264.881828	-2.968778	3.266509
-1262.864157	-3.920053	3.276506
-1260.817006	-1.778125	3.286502
-1259.204884	-4.742410	3.296499
-1257.222421	0.075157	3.306496
-1255.183682	-4.474775	3.316493
-1253.383331	-8.692870	3.326490
-1251.522842	-2.444190	3.336486
-1249.720347	-4.938403	3.346483
-1248.060910	2.594570	3.356480
-1246.114974	-4.272629	3.366477
-1243.776616	-7.375220	3.376474
-1242.020720	-6.392995	3.386470
-1240.236977	-3.518893	3.396467
-1238.596711	-3.459223	3.406464
-1236.543901	0.488152	3.416461
-1234.629922	-2.966527	3.426458
-1232.601703	-8.160551	3.436454
-1230.922354	0.131886	3.446451
-1228.937498	1.991703	3.456448
-1227.297467	-1.043344	3.466445
-1225.324482	-12.926471	3.476442
-1223.385240	-9.126705	3.486438
-1221.602827	-2.617610	3.496435
-1219.914526	-5.221424	3.506432
-1217.870078	-4.056401	3.516429
-1215.654691	-3.622943	3.526426
-1213.709989	-9.095696	3.536422
-1212.181401	-2.078607	3.546419
-1210.432381	-3.479488	3.556416
-1208.386043	-0.053687	3.566413
-1206.301777	-5.089288	3.576410
-1204.410261	-4.419262	3.586406
-1202.654216	-2.840183	3.596403
-1201.177998	-5.620053	3.606400
-1199.072153	-1.557969	3.616397
-1197.167827	-6.670562	3.626394
-1195.213450	-9.241140	3.636390
-1193.200271	-4.163164	3.646387
-1191.208210	-6.209237	3.656384
-1189.551242	-3.572183	3.666381
-1187.928373	-9.214478	3.676378
-1186.090946	-4.518908	3.686374
-1183.713376	-7.834557	3.696371
-1182.194709	-6.048536	3.706368
-1180.086108	-2.015297	3.716365
-1178.389721	-9.919368	3.726362
-1176.654115	2.358884	3.736358
-1174.932167	-6.255073	3.746355
-1172.523139	0.618030	3.756352
-1170.858509	-7.985174	3.766349
-1168.912349	-3.616460	3.776346
-1167.014569	-5.476901	3.786342
-1165.088092	-1.804515	3.796339
-1163.216723	-2.738614	3.806336
-1161.594194	-2.462892	3.816333
-1159.592929	3.104921	3.826330
-1157.860169	-1.953354	3.836326
-1155.795156	-2.282105	3.846323
-1153.848357	-2.206676	3.856320
-1151.791635	-4.567800	3.866317
-1150.345334	-2.757548	3.876314
-1148.692663	-3.825599	3.886310
-1146.372259	-10.081566	3.896307
-1144.489808	-10.250049	3.906304
-1142.827065	-8.097046	3.916301
-1140.840634	-7.770576	3.926298
-1138.855933	-9.674900	3.936294
-1137.169763	-9.841977	3.946291
-1135.064015	-7.707731	3.956288
-1133.287871	-4.522852	3.966285
-1131.603975	-4.807984	3.976282
-1129.596432	-5.590154	3.986278
-1127.578723	-2.134436	3.996275
-1125.956646	1.960893	4.006272
-1124.149003	2.923879	4.016269
-1122.023321	-0.326155	4.026266
-1120.140517	-5.384720	4.036262
-1118.183127	-3.389359	4.046259
-1116.293177	-2.043214	4.056256
-1114.600367	-2.023440	4.066253
-1112.882247	-1.126653	4.076250
-1110.722668	-4.011042	4.086246
-1108.905279	-7.690174	4.096243
-1106.913971	-0.481757	4.106240
-1105.032330	-2.217988	4.116237
-1103.376132	-1.619187	4.126234
-1101.146440	-3.927408	4.136230
-1099.631094	-4.198188	4.146227
-1097.888027	-1.596942	4.156224
-1095.738496	1.326136	4.166221
-1093.791265	-5.219045	4.176218
-1092.355763	-6.879168	4.186214
-1090.129372	-11.245817	4.196211
-1088.105072	-2.133696	4.206208
-1086.379752	0.644084	4.216205
-1084.521325	-3.439494	4.226202
-1082.712881	-6.479275	4.236198
-1080.658275	-11.254232	4.246195
-1079.024537	-10.449715	4.256192
-1077.117062	-2.929439	4.266189
-1075.098415	-4.542295	4.276186
-1073.389443	-3.683489	4.286182
-1071.491404	-11.142898	4.296179
-1069.498782	-2.592539	4.306176
-1067.471355	-6.298919	4.316173
-1065.626338	-1.902884	4.326170
-1063.754823	-5.758010	4.336166
-1061.898438	-6.250681	4.346163
-1060.235889	-7.078668	4.356160
-1058.265252	-1.712709	4.366157
-1056.472677	-3.428340	4.376154
-1054.558923	-4.912296	4.386150
-1052.406309	-10.460807	4.396147
-1050.623616	-14.236979	4.406144
-1049.014508	-12.296384	4.416141
-1047.312196	-15.526008	4.426138
-1045.114089	-12.618548	4.436134
-1043.140456	-4.085655	4.446131
-1041.466814	-5.422251	4.456128
-1039.402657	-4.062850	4.466125
-1037.565004	-2.602486	4.476122
-1035.826348	-3.069993	4.486118
-1033.914206	-4.095775	4.496115
-1031.963819	-2.975544	4.506112
-1029.834474	-4.560275	4.516109
-1028.224765	-4.361358	4.526106
-1026.469608	-12.479995	4.536102
-1024.331392	-5.307629	4.546099
-1022.735333	3.421460	4.556096
-1020.755310	-5.786307	4.566093
-1018.919265	-10.065204	4.576090
-1016.930352	-11.815361	4.586086
-1015.125488	-17.796126	4.596083
-1013.269798	-8.818027	4.606080
-1011.101806	-8.428901	4.616077
-1009.287560	-2.759990	4.626074
-1007.627069	-8.019763	4.636070
-1006.089433	-13.422521	4.646067
-1003.903499	-13.066257	4.656064
-1002.008961	-6.315960	4.666061
-999.970871	-2.501804	4.676058
-997.925714	-8.119928	4.686054
-996.222956	-6.097955	4.696051
-994.478577	-7.033719	4.706048
-993.081036	-5.888209	4.716045
-990.804495	-7.627497	4.726042
-988.772176	-9.512468	4.736038
-986.654784	-2.938320	4.746035
-985.003639	-7.080256	4.756032
-983.317058	1.321753	4.766029
-981.314550	-6.708513	4.776026
-979.719469	0.634434	4.786022
-977.503459	-2.214649	4.796019
-975.683582	2.997071	4.806016
-973.931837	-1.322000	4.816013
-971.760151	-0.620792	4.826010
-970.205728	-7.515179	4.836006
-968.267581	-7.229789	4.846003
-966.359800	-7.485863	4.856000
-964.603568	-7.375068	4.865997
-962.690353	-4.747240	4.875994
-960.344172	-9.412403	4.885990
-958.801490	-4.440563	4.895987
-956.937959	-9.788032	4.905984
-954.892806	-3.330197	4.915981
-953.442315	-8.183722	4.925978
-951.215901	-1.587496	4.935974
-949.483568	-7.875572	4.945971
-947.534907	-2.201259	4.955968
-945.507411	-3.101728	4.965965
-943.958444	-0.025639	4.975962
-942.093565	-3.412239	4.985958
-939.910240	-2.363911	4.995955
-938.162070	-0.530735	5.005952
-936.400106	-2.391384	5.015949
-934.353969	-4.289572	5.025946
-932.421843	-7.557441	5.035942
-930.627578	-3.047388	5.045939
-928.739792	-2.828124	5.055936
-926.948202	-1.546624	5.065933
-924.995092	-4.549418	5.075930
-923.304090	-10.238756	5.085926
-921.243370	-6.933415	5.095923
-919.451520	-8.340930	5.105920
-917.715407	-7.446875	5.115917
-915.759358	-3.651105	5.125914
-913.849601	-9.405410	5.135910
-911.576438	-7.588253	5.145907
-909.941779	-1.246329	5.155904
-908.227718	-4.774582	5.165901
-906.114227	-5.001916	5.175898
-904.335753	-2.999872	5.185894
-902.482288	-2.948787	5.195891
-900.794763	-1.697999	5.205888
-898.904872	-4.006973	5.215885
-896.871027	-4.783677	5.225882
-894.895929	-3.607280	5.235878
-893.221532	-3.172292	5.245875
-891.362721	-8.525275	5.255872
-889.562181	-2.843020	5.265869
-887.315165	-13.519173	5.275866
-885.713664	-8.002468	5.285862
-883.688854	-5.818734	5.295859
-882.049097	-0.530774	5.305856
-880.220184	-3.284728	5.315853
-877.798868	-4.184936	5.325850
-876.005477	-9.470606	5.335846
-874.386197	-4.912009	5.345843
-872.579918	-2.658593	5.355840
-870.689567	-6.267108	5.365837
-868.765709	-7.837794	5.375834
-866.763110	-4.729957	5.385830
-864.944730	-9.605924	5.395827
-863.416809	-6.308519	5.405824
-861.055750	-2.563232	5.415821
-859.476600	-10.547835	5.425818
-857.462179	-3.046036	5.435814
-855.353958	-2.623526	5.445811
-853.719721	-8.062163	5.455808
-852.078376	-2.149164	5.465805
-849.994966	-6.955380	5.475802
-848.115760	-9.133130	5.485798
-846.260337	-7.146500	5.495795
-844.444746	0.003406	5.505792
-842.346113	-1.907833	5.515789
-840.650847	1.077047	5.525786
-838.790257	0.307560	5.535782
-836.804586	-4.601445	5.545779
-834.870293	-4.035851	5.555776
-833.061544	-1.007525	5.565773
-831.178080	-3.127522	5.575770
-829.643332	-12.025547	5.585766
-827.428185	-4.761071	5.595763
-825.445570	-3.547921	5.605760
-823.647179	-1.811107	5.615757
-821.837771	-0.769219	5.625754
-820.050231	-7.066033	5.635750
-818.187245	-4.881640	5.645747
-816.132513	2.670601	5.655744
-814.148013	0.060777	5.665741
-812.450591	-2.116313	5.675738
-810.927034	-3.545603	5.685734
-808.717692	5.635114	5.695731
-806.750140	3.094322	5.705728
-804.954985	0.306345	5.715725
-803.018880	-2.382578	5.725722
-801.071004	-5.673387	5.735718
-799.487136	-0.060638	5.745715
-797.465367	-1.046909	5.755712
-795.434560	2.735441	5.765709
-793.615227	2.841016	5.775706
-791.799603	0.010303	5.785702
-789.982959	-1.873190	5.795699
-787.689996	-3.430171	5.805696
-786.428422	2.060412	5.815693
-784.385631	-3.457690	5.825690
-782.607138	-2.635044	5.835686
-780.585649	-7.710783	5.845683
-778.631923	-2.166603	5.855680
-776.818789	-7.047986	5.865677
-774.998749	-0.250842	5.875674
-772.971327	-3.085389	5.885670
-771.082030	-2.900977	5.895667
-769.017424	-7.948860	5.905664
-767.637692	-1.915039	5.915661
-765.523196	-7.559847	5.925658
-763.386593	0.020411	5.935654
-761.908298	-3.187429	5.945651
-760.014050	-9.032301	5.955648
-758.406540	4.504703	5.965645
-756.032677	-0.881545	5.975642
-754.196543	-0.833889	5.985638
-752.347647	-0.431424	5.995635
-750.575273	-5.639437	6.005632
-748.715175	-3.708739	6.015629
-746.753202	-6.247011	6.025626
-744.831728	-3.877691	6.035622
-743.072472	1.118117	6.045619
-741.283291	2.570675	6.055616
-739.265582	-4.405508	6.065613
-737.445397	-3.171063	6.075610
-735.273158	-3.436053	6.085606
-733.574548	-5.854860	6.095603
-732.236227	-7.751875	6.105600
-730.122669	3.635837	6.115597
-727.912339	1.121051	6.125594
-726.119262	-1.783380	6.135590
-724.038503	-15.486555	6.145587
-722.249033	-4.246004	6.155584
-720.661578	2.304138	6.165581
-718.542096	-6.054099	6.175578
-716.969861	-0.944701	6.185574
-714.847670	-7.174916	6.195571
-712.910222	-6.181825	6.205568
-711.105444	-15.446620	6.215565
-709.267634	-8.377523	6.225562
-707.490354	-7.846736	6.235558
-705.515755	-7.688534	6.245555
-703.516977	-2.344121	6.255552
-701.833789	2.029129	6.265549
-699.912044	-3.610091	6.275546
-697.980455	0.453467	6.285542
-695.910598	-14.482702	6.295539
-694.098871	-6.888364	6.305536
-692.754678	-4.780450	6.315533
-690.246054	-13.478737	6.325530
-688.556636	-9.682800	6.335526
-686.771550	-11.949599	6.345523
-684.879877	-11.010751	6.355520
-682.876269	-6.361839	6.365517
-681.031938	-8.568625	6.375514
-679.405478	-6.283168	6.385510
-677.425122	-4.371627	6.395507
-675.397553	-2.672893	6.405504
-673.724627	-4.321755	6.415501
-671.644894	-13.977828	6.425498
-669.742756	-8.900582	6.435494
-667.983903	-6.671007	6.445491
-666.060607	-8.989874	6.455488
-664.445900	-0.904550	6.465485
-662.357400	-6.414066	6.475482
-660.416598	-8.093084	6.485478
-658.483463	-10.400885	6.495475
-656.866446	-8.131272	6.505472
-654.824875	-5.038948	6.515469
-652.953043	-5.293764	6.525466
-651.342976	-4.680955	6.535462
-649.188631	-5.160905	6.545459
-647.095759	-2.177824	6.555456
-645.325119	-8.740243	6.565453
-643.664202	-3.902334	6.575450
-641.772142	-13.667351	6.585446
-639.734339	-9.424923	6.595443
-638.207624	-7.660351	6.605440
-636.011612	-5.792702	6.615437
-634.114702	-4.298851	6.625434
-632.219932	-3.208873	6.635430
-630.456118	-2.813247	6.645427
-628.448258	-7.027727	6.655424
-627.028749	-2.448085	6.665421
-625.110279	-1.459784	6.675418
-622.662728	-0.488107	6.685414
-620.927102	-10.052856	6.695411
-619.346505	-13.370112	6.705408
-617.350545	-11.590488	6.715405
-615.232822	-2.454941	6.725402
-613.662502	-7.308471	6.735398
-611.668546	-3.591124	6.745395
-609.936009	1.579587	6.755392
-608.023272	3.028300	6.765389
-605.990364	-10.337146	6.775386
-604.159313	-10.452774	6.785382
-602.279261	-6.079320	6.795379
-600.439157	-8.766957	6.805376
-598.838744	-10.993139	6.815373
-596.807031	-6.347060	6.825370
-594.463762	-6.427660	6.835366
-592.866489	-13.622358	6.845363
-591.163095	-11.876505	6.855360
-589.361918	-8.226242	6.865357
-586.959387	-6.895227	6.875354
-585.445771	-10.174920	6.885350
-583.613445	-14.247637	6.895347
-581.670096	-13.095905	6.905344
-579.524151	-12.639700	6.915341
-578.072961	-15.901521	6.925338
-575.873257	-4.570052	6.935334
-574.214264	-13.926736	6.945331
-572.474690	-6.366560	6.955328
-570.536288	-8.539341	6.965325
-568.519493	-8.911983	6.975322
-566.736518	-7.958835	6.985318
-564.603806	-6.761544	6.995315
-563.081100	-8.664234	7.005312
-560.835688	-4.702792	7.015309
-559.509868	0.259760	7.025306
-557.315127	-6.245602	7.035302
-555.283063	-6.074348	7.045299
-553.639794	0.176472	7.055296
-551.458430	-0.672449	7.065293
-549.876482	0.151766	7.075290
-547.789031	-2.234281	7.085286
-545.927305	-9.461719	7.095283
-544.405247	-7.593708	7.105280
-542.433918	-4.899018	7.115277
-540.056793	-10.519270	7.125274
-538.373272	-10.838657	7.135270
-536.694952	-13.086715	7.145267
-535.000272	-13.024192	7.155264
-533.090441	-6.746459	7.165261
-530.719978	-8.167150	7.175258
-528.931226	-6.576991	7.185254
-527.233521	-3.563845	7.195251
-525.432155	-5.019957	7.205248
-523.448460	-8.327322	7.215245
-521.699601	-1.509123	7.225242
-519.619715	-6.519769	7.235238
-517.887941	-10.650593	7.245235
-516.152569	-11.584571	7.255232
-514.294049	-4.663879	7.265229
-512.140437	-10.463148	7.275226
-510.370771	-9.102035	7.285222
-508.597972	-7.531419	7.295219
-506.360909	-11.656088	7.305216
-504.729014	-5.701843	7.315213
-502.959495	-7.658123	7.325210
-500.883483	-5.120645	7.335206
-499.235541	-11.069676	7.345203
-497.252017	-11.057991	7.355200
-495.334596	-8.064122	7.365197
-493.628492	-7.273908	7.375194
-491.578021	-7.656600	7.385190
-489.614869	-11.061711	7.395187
-487.771237	-9.319230	7.405184
-485.908251	-1.172363	7.415181
-484.131238	-1.794016	7.425178
-482.155630	-6.672714	7.435174
-480.086023	-7.470565	7.445171
-478.618832	-1.314730	7.455168
-476.685186	-7.723065	7.465165
-474.840818	-0.667444	7.475162
-472.671217	-5.097106	7.485158
-470.827334	-10.761615	7.495155
-469.091086	-5.927709	7.505152
-467.264507	-6.222522	7.515149
-465.367056	-9.235011	7.525146
-463.727798	-3.815603	7.535142
-461.557047	-9.712305	7.545139
-459.647108	-10.595169	7.555136
-457.787581	-5.218826	7.565133
-455.719158	-8.566509	7.575130
-454.115562	-10.482048	7.585126
-452.127534	-10.109460	7.595123
-450.399948	-9.013167	7.605120
-448.550813	-1.235115	7.615117
-446.434737	-3.931968	7.625114
-444.606850	-8.194934	7.635110
-442.759030	-4.455683	7.645107
-440.874878	-11.405569	7.655104
-439.279428	-1.936975	7.665101
-437.348815	-9.031649	7.675098
-435.653799	-7.540138	7.685094
-433.070582	-8.547855	7.695091
-431.855215	-11.568251	7.705088
-429.830666	-8.154057	7.715085
-427.489685	-8.875191	7.725082
-425.886949	-15.124857	7.735078
-424.266896	-8.181804	7.745075
-422.214762	-2.060906	7.755072
-420.278436	-8.815422	7.765069
-418.411098	-9.505133	7.775066
-416.203232	-7.710223	7.785062
-414.750828	-8.853163	7.795059
-412.764249	-9.080321	7.805056
-411.240565	-7.340379	7.815053
-409.286608	-4.854385	7.825050
-406.915604	-8.643503	7.835046
-405.327313	-2.481691	7.845043
-403.234482	-13.241775	7.855040
-401.539437	-4.971707	7.865037
-399.591609	-7.760080	7.875034
-397.572513	-2.721799	7.885030
-396.235016	-9.259108	7.895027
-393.966685	-3.684290	7.905024
-392.285550	-0.021018	7.915021
-389.914245	-3.805433	7.925018
-388.344378	-7.596104	7.935014
-386.786094	-7.356959	7.945011
-384.752654	-5.281535	7.955008
-382.837888	-5.636154	7.965005
-381.010379	-4.298389	7.975002
-379.131876	-3.821410	7.984998
-376.959341	-6.620377	7.994995
-375.204140	-5.225273	8.004992
-373.454244	-1.917182	8.014989
-371.552951	-1.317518	8.024986
-369.406200	-10.437736	8.034982
-367.747751	-12.578296	8.044979
-365.960670	-10.029308	8.054976
-364.104484	-7.442402	8.064973
-362.244281	-3.510849	8.074970
-360.269297	-7.146700	8.084966
-358.182336	-10.399365	8.094963
-356.632435	-6.776697	8.104960
-354.906991	-4.236808	8.114957
-352.767192	-4.878383	8.124954
-350.562677	-2.503392	8.134950
-349.000148	-3.093863	8.144947
-346.943379	-0.987392	8.154944
-345.299314	-6.779391	8.164941
-343.330179	-8.563735	8.174938
-341.494711	-6.137717	8.184934
-339.592484	-12.417773	8.194931
-337.726921	-4.995941	8.204928
-335.806668	-10.168853	8.214925
-334.050273	-4.828049	8.224922
-332.130071	-9.843052	8.234918
-330.219806	-12.080627	8.244915
-328.390404	-7.580436	8.254912
-326.853639	-8.168359	8.264909
-324.596688	-6.957524	8.274906
-322.839641	-4.844242	8.284902
-320.694059	-15.928479	8.294899
-318.692514	-8.348335	8.304896
-316.885764	-3.790832	8.314893
-315.608575	-7.675269	8.324890
-313.515585	-4.210316	8.334886
-311.370162	-7.432800	8.344883
-309.536932	-8.338039	8.354880
-307.673118	-8.714465	8.364877
-305.874214	-11.758472	8.374874
-304.095909	-8.202227	8.384870
-302.077264	-7.665451	8.394867
-300.411018	-11.716193	8.404864
-298.335898	-5.459901	8.414861
-296.372016	-4.391738	8.424858
-294.409014	-4.409768	8.434854
-292.602504	-6.379697	8.444851
-291.080096	-11.702235	8.454848
-288.918390	-2.069692	8.464845
-287.031418	-5.048794	8.474842
-285.455802	-7.078182	8.484838
-283.200597	1.543112	8.494835
-281.281868	-9.986479	8.504832
-279.646968	-11.755320	8.514829
-277.538706	-4.683231	8.524826
-276.027112	-9.383497	8.534822
-273.926858	-9.815003	8.544819
-272.167630	-8.755209	8.554816
-270.259818	-3.503259	8.564813
-268.374349	-6.268946	8.574810
-266.371946	-8.652233	8.584807
-264.532871	-11.309457	8.594803
-262.772112	-8.681976	8.604800
-260.723079	-8.854239	8.614797
-258.882020	-5.769035	8.624794
-257.126977	-7.928096	8.634791
-255.247722	-8.395369	8.644787
-253.657912	-9.166978	8.654784
-251.308013	-7.584058	8.664781
-249.182373	-2.736336	8.674778
-247.263584	-21.012876	8.684775
-245.726159	-13.780183	8.694771
-243.969568	-13.089427	8.704768
-242.258327	-22.563199	8.714765
-240.236512	-21.706345	8.724762
-238.152951	-10.783894	8.734759
-236.337567	-17.643710	8.744755
-234.275947	-19.006928	8.754752
-232.788671	-15.712085	8.764749
-230.930459	-8.435834	8.774746
-229.025953	-9.606603	8.784743
-226.990919	-17.374640	8.794739
-225.084874	-19.560933	8.804736
-223.499594	-14.156422	8.814733
-221.328156	-22.532021	8.824730
-219.613525	-15.738123	8.834727
-217.982925	-16.009367	8.844723
-215.619064	-22.293524	8.854720
-213.941788	-15.518924	8.864717
-212.252570	-14.473178	8.874714
-210.128195	-21.559128	8.884711
-208.058260	-20.106757	8.894707
-205.999927	-12.128198	8.904704
-204.747321	-12.920176	8.914701
-202.696142	-16.223844	8.924698
-200.801987	-14.667625	8.934695
-198.936635	-13.829978	8.944691
-196.955226	-17.357776	8.954688
-195.321720	-15.444163	8.964685
-193.555788	-13.098514	8.974682
-191.522909	-15.549763	8.984679
-189.409759	-12.530029	8.994675
-187.309371	-20.959002	9.004672
-185.980748	-15.781935	9.014669
-183.941453	-11.743024	9.024666
-181.880835	-15.294502	9.034663
-180.155981	-15.817607	9.044659
-178.389200	-10.753082	9.054656
-176.271437	-20.574319	9.064653
-174.391187	-14.651566	9.074650
-172.730515	-17.704999	9.084647
-171.053398	-14.803573	9.094643
-168.747531	-19.548405	9.104640
-166.982855	-8.597105	9.114637
-165.241459	-14.153464	9.124634
-163.180694	-21.191332	9.134631
-161.243048	-13.123999	9.144627
-159.609082	-21.113784	9.154624
-157.535543	-11.596524	9.164621
-155.733999	-13.098183	9.174618
-154.045744	-18.112359	9.184615
-151.732232	-17.955669	9.194611
-150.239208	-12.100586	9.204608
-148.387775	-15.013911	9.214605
-146.360206	-7.142492	9.224602
-144.425140	-12.069726	9.234599
-142.518718	-13.038624	9.244595
-140.761097	-13.082182	9.254592
-139.050962	-13.942390	9.264589
-136.898376	-12.653146	9.274586
-135.145093	-9.713317	9.284583
-133.334107	-10.256447	9.294579
-131.282616	-18.540205	9.304576
-129.770375	-11.838683	9.314573
-127.494701	-11.713829	9.324570
-125.515417	-21.522407	9.334567
-123.797980	-12.172515	9.344563
-122.118256	-9.819373	9.354560
-120.110356	0.073148	9.364557
-118.396030	-10.438439	9.374554
-116.140429	-10.461953	9.384551
-114.459013	-8.058548	9.394547
-112.605805	-12.909539	9.404544
-110.789493	-11.187666	9.414541
-108.937649	-8.958293	9.424538
-107.088338	-7.789587	9.434535
-105.065070	-9.730802	9.444531
-103.172480	-8.640053	9.454528
-101.368489	-10.271539	9.464525
-99.555825	-5.258481	9.474522
-97.492880	-6.661271	9.484519
-95.575318	1.191432	9.494515
-93.994098	-17.009063	9.504512
-92.103686	-4.975628	9.514509
-89.990468	-12.015496	9.524506
-88.242717	-7.167341	9.534503
-86.261882	-7.339629	9.544499
-84.368532	-6.995843	9.554496
-82.733602	-6.386616	9.564493
-80.740845	-10.918786	9.574490
-78.832623	-8.302059	9.584487
-76.904460	-12.402334	9.594483
-75.253270	-10.366719	9.604480
-72.973402	-9.018772	9.614477
-71.080339	-4.253784	9.624474
-69.561262	-15.517367	9.634471
-67.783453	-5.188614	9.644467
-65.772449	-6.166241	9.654464
-63.771046	-12.305601	9.664461
-61.817065	-8.279814	9.674458
-60.165207	-10.678071	9.684455
-58.049444	-9.701835	9.694451
-56.296566	-15.692594	9.704448
-54.705874	-14.211010	9.714445
-52.667524	-3.232210	9.724442
-50.711134	-5.079027	9.734439
-48.887958	-8.780422	9.744435
-46.911886	-16.905242	9.754432
-44.954634	-11.288351	9.764429
-43.190387	-12.019752	9.774426
-41.403495	-11.218416	9.784423
-39.437719	-4.811809	9.794419
-37.476144	-8.048945	9.804416
-35.539407	-5.716210	9.814413
-33.886174	-7.238335	9.824410
-31.822059	-3.943788	9.834407
-30.013745	-8.200179	9.844403
-28.255976	-12.404294	9.854400
-26.299560	-12.517374	9.864397
-24.350225	-10.504015	9.874394
-22.478234	-12.289978	9.884391
-20.866703	-13.368064	9.894387
-18.974490	-16.079374	9.904384
-16.440276	-14.552464	9.914381
-14.729404	-12.891071	9.924378
-13.476132	-10.742995	9.934375
-11.575050	-6.972418	9.944371
-9.090143	-13.280435	9.954368
-7.443865	-9.946066	9.964365
-6.018211	-3.323804	9.974362
-4.234570	5.624050	9.984359
-3.169585	41.227702	9.994355
-1.776343	85.913551	10.004352
-0.669061	161.217715	10.014349
0.000000	237.384164	10.019354
1.017351	271.422119	10.024359
1.873117	306.037875	10.029363
2.300540	356.803501	10.034368
3.127745	375.489959	10.039373
3.251416	407.831985	10.044378
3.742353	427.756476	10.049383
4.018377	427.882783	10.054387
3.883669	459.405086	10.059392
4.463935	464.884141	10.064397
3.943245	481.666209	10.069402
4.491702	481.059910	10.074407
4.768799	490.665490	10.079411
4.553090	487.006536	10.084416
4.948552	488.752314	10.089421
4.705550	491.902539	10.094426
4.904771	503.537553	10.099431
4.972785	504.245839	10.104435
4.750907	507.465241	10.109440
5.236580	506.999847	10.114445
5.043228	520.045837	10.119450
5.312501	525.468856	10.124455
5.067579	524.124886	10.129459
5.081455	531.608804	10.134464
5.141192	527.587349	10.139469
5.005850	548.964977	10.144474
5.380195	543.231159	10.149479
5.448160	547.716424	10.154483
5.285132	553.060162	10.159488
5.516397	546.986446	10.164493
5.304175	556.547105	10.169498
5.600755	555.140423	10.174503
5.400075	553.380945	10.179507
5.427601	558.686407	10.184512
5.795330	553.109765	10.189517
5.701011	564.145066	10.194522
5.615906	556.286149	10.199527
5.955547	567.359476	10.204531
5.958998	559.795530	10.209536
5.936792	566.432051	10.214541
5.878126	569.093977	10.219546
5.913245	575.232481	10.224551
5.986733	570.115943	10.229555
6.264134	579.265773	10.234560
6.143369	564.986159	10.239565
5.823547	575.962812	10.244570
5.951950	581.402012	10.249575
6.252577	601.006994	10.254579
6.359848	611.324171	10.259584
6.644054	608.930659	10.264589
6.442837	615.384431	10.269594
6.552534	610.922879	10.274599
6.463407	611.623116	10.279603
6.485631	621.261548	10.284608
6.432963	613.602440	10.289613
6.447407	623.926546	10.294618
6.355607	622.509257	10.299623
6.534169	627.205577	10.304627
6.471205	624.042647	10.309632
6.822498	622.398562	10.314637
6.474044	623.706314	10.319642
6.728937	629.950144	10.324647
6.502509	624.020362	10.329651
6.578947	644.044378	10.334656
6.852013	641.258379	10.339661
6.962846	652.347763	10.344666
7.273705	650.285903	10.349671
7.319757	655.897544	10.354675
7.002267	657.167243	10.359680
7.263783	658.313054	10.364685
7.015513	663.269860	10.369690
7.234653	666.937803	10.374695
7.210898	658.649554	10.379699
6.908428	663.069350	10.384704
7.215947	667.301969	10.389709
7.092430	665.825076	10.394714
7.326472	690.093054	10.399719
7.419656	684.744664	10.404723
7.284422	698.552716	10.409728
7.878314	698.215145	10.414733
7.816651	707.885938	10.419738
7.948390	699.635948	10.424743
7.933332	705.312552	10.429747
7.784803	702.253142	10.434752
8.155582	701.933809	10.439757
8.212418	713.413495	10.444762
8.052681	701.429825	10.449767
8.109166	710.972961	10.454771
8.092784	714.954462	10.459776
8.029345	712.509141	10.464781
8.051309	716.374133	10.469786
8.025419	710.085884	10.474791
8.191600	706.403814	10.479795
7.663930	725.103378	10.484800
8.372700	711.091886	10.489805
8.020842	723.718613	10.494810
8.156652	719.172434	10.499815
8.403039	707.466204	10.504819
8.352248	721.636146	10.509824
8.717936	726.564442	10.514829
8.463079	735.329303	10.519834
8.679062	752.419990	10.524839
8.927718	739.745068	10.529843
8.985673	743.361462	10.534848
8.739769	728.690036	10.539853
8.567768	732.817794	10.544858
8.912332	745.081140	10.549863
8.963977	752.089188	10.554867
8.834986	766.306339	10.559872
9.024785	755.216260	10.564877
8.879776	759.159936	10.569882
9.002442	760.958720	10.574887
8.955330	749.813384	10.579891
8.871914	757.898019	10.584896
9.021074	756.565295	10.589901
8.958246	766.764623	10.594906
8.876158	755.564933	10.599911
9.145812	761.658224	10.604915
9.097170	761.467288	10.609920
9.496689	775.592272	10.614925
9.562184	792.459411	10.619930
9.637965	782.638096	10.624935
9.767356	787.820156	10.629939
9.760176	782.792108	10.634944
9.957701	773.568007	10.639949
9.628143	770.908061	10.644954
9.324722	770.592170	10.649959
9.609520	775.948148	10.654963
9.523366	799.283300	10.659968
9.904407	800.695506	10.664973
9.747260	799.586684	10.669978
9.823138	800.722689	10.674983
10.120156	798.667747	10.679987
10.157614	804.965256	10.684992
10.379065	802.671615	10.689997
10.211436	811.275943	10.695002
9.952819	807.227911	10.700007
10.190869	805.691760	10.705011
10.126062	812.719987	10.710016
10.010967	814.517272	10.715021
9.945816	808.497032	10.720026
10.211292	815.989857	10.725031
10.476938	814.588084	10.730035
10.038833	807.370418	10.735040
10.553006	821.737374	10.740045
10.680164	834.003928	10.745050
10.675393	835.196956	10.750055
10.834108	831.727371	10.755059
10.333670	823.955052	10.760064
11.210074	828.630031	10.765069
10.600925	826.416815	10.770074
11.109953	827.609903	10.775079
11.230100	820.891435	10.780083
10.698895	817.785794	10.785088
10.820460	811.385668	10.790093
10.468744	833.657717	10.795098
10.741098	834.431207	10.800103
11.247994	840.089276	10.805107
11.332147	839.790421	10.810112
11.662525	827.909840	10.815117
11.848019	831.983763	10.820122
11.524132	821.956487	10.825127
11.727958	811.826129	10.830131
11.446245	809.456608	10.835136
11.729966	805.347311	10.840141
11.387413	807.564095	10.845146
11.395756	812.327050	10.850151
11.473879	807.594490	10.855155
11.212221	810.618440	10.860160
11.401435	811.521890	10.865165
11.286662	812.830237	10.870170
11.825686	819.161307	10.875175
11.885513	827.346144	10.880179
11.853861	824.851577	10.885184
12.193659	835.712184	10.890189
11.640182	823.166697	10.895194
11.743158	827.660659	10.900199
12.149716	832.366418	10.905203
12.125991	828.965357	10.910208
12.046423	831.215900	10.915213
11.959623	833.320931	10.920218
12.242645	840.142299	10.925223
12.474891	833.834905	10.930227
11.948122	840.039480	10.935232
12.485126	833.398034	10.940237
12.243899	840.006528	10.945242
12.387271	846.214619	10.950247
12.340445	829.700881	10.955251
12.266127	847.437261	10.960256
12.343823	835.950234	10.965261
12.197141	843.657051	10.970266
12.163048	839.926460	10.975271
12.443017	847.674050	10.980275
12.589442	851.725822	10.985280
12.906211	833.326283	10.990285
12.501567	845.720245	10.995290
12.619194	840.353706	11.000295
13.026545	856.201240	11.005299
12.782912	862.751778	11.010304
12.921155	865.629951	11.015309
12.844872	872.772009	11.020314
12.677535	877.228668	11.025319
12.774761	879.332742	11.030323
12.929078	877.595458	11.035328
13.206426	864.641443	11.040333
12.888361	880.333446	11.045338
12.945934	872.192964	11.050343
13.168005	864.030983	11.055347
13.174008	868.639778	11.060352
13.438854	865.992253	11.065357
13.258219	869.621499	11.070362
13.431281	872.795339	11.075367
13.522077	892.044648	11.080371
13.614614	901.254131	11.085376
14.058191	884.425558	11.090381
13.549463	880.557752	11.095386
13.736913	870.568746	11.100391
13.936803	868.874661	11.105395
13.309718	875.312884	11.110400
13.842055	876.983262	11.115405
13.861688	905.354609	11.120410
14.208472	894.534296	11.125415
14.651860	887.865176	11.130419
13.903166	881.152777	11.135424
14.155424	874.138806	11.140429
13.808221	871.054272	11.145434
13.995196	875.356644	11.150439
14.016311	875.574079	11.155443
14.031678	878.331494	11.160448
14.445621	906.404973	11.165453
14.471452	910.581658	11.170458
14.527955	900.362764	11.175463
14.322050	897.862858	11.180467
14.593802	897.092505	11.185472
14.664967	883.165193	11.190477
14.444622	880.336410	11.195482
14.306562	878.677298	11.200487
14.652477	887.680770	11.205491
14.443416	908.468247	11.210496
14.647885	907.240238	11.215501
14.480363	909.506397	11.220506
14.792387	904.471555	11.225511
14.677924	906.540004	11.230515
14.531711	912.297535	11.235520
14.750977	897.286802	11.240525
14.859334	913.371333	11.245530
14.727563	903.415869	11.250535
15.192614	903.407950	11.255539
15.177702	908.860667	11.260544
15.410534	907.842615	11.265549
15.110281	905.174815	11.270554
15.083675	907.371188	11.275559
15.044889	908.284199	11.280563
15.047727	912.751577	11.285568
15.456871	916.023401	11.290573
15.136808	926.098276	11.295578
15.242144	938.123954	11.300583
15.609040	935.083223	11.305587
15.443642	934.128681	11.310592
15.844343	939.090894	11.315597
16.156617	946.019620	11.320602
15.939056	920.461728	11.325607
16.233035	903.292690	11.330611
15.726086	911.522235	11.335616
16.115900	903.369751	11.340621
15.747543	908.886724	11.345626
15.857936	909.550422	11.350631
15.798606	910.745849	11.355635
15.587867	908.163127	11.360640
15.890040	902.019606	11.365645
15.551044	922.272699	11.370650
15.767784	928.363461	11.375655
16.047833	940.936906	11.380659
15.729853	946.619335	11.385664
16.058605	938.451338	11.390669
16.099345	952.116438	11.395674
16.210637	946.482769	11.400679
16.628509	948.873207	11.405683
16.338625	944.062091	11.410688
16.595913	950.408188	11.415693
16.640647	954.321655	11.420698
16.259228	947.549072	11.425703
16.601476	942.376922	11.430707
16.490510	947.780314	11.435712
16.367198	947.213326	11.440717
16.453617	959.527488	11.445722
16.738921	961.672547	11.450727
16.957555	969.832137	11.455731
16.990688	981.451444	11.460736
17.186699	965.901838	11.465741
17.160610	958.678311	11.470746
16.923950	950.952169	11.475751
17.050140	937.552231	11.480755
16.531860	949.374581	11.485760
16.844138	952.598780	11.490765
16.944510	961.043751	11.495770
16.777392	976.265473	11.500775
17.111318	980.001928	11.505779
17.164893	970.519943	11.510784
17.542626	967.106866	11.515789
17.377249	980.923147	11.520794
17.460263	967.550569	11.525799
17.722495	965.176276	11.530803
17.581259	976.959017	11.535808
17.690625	970.544996	11.540813
17.646437	961.133807	11.545818
17.462113	980.214207	11.550823
17.699456	967.432074	11.555827
17.248276	971.352092	11.560832
17.705808	971.643439	11.565837
17.556824	976.660214	11.570842
17.736104	975.357363	11.575847
17.824080	969.273208	11.580851
17.755653	989.185176	11.585856
18.055223	994.395367	11.590861
18.118267	1000.177910	11.595866
18.272548	1002.206666	11.600871
18.333966	999.348693	11.605875
18.031821	988.433096	11.610880
18.217941	989.105223	11.615885
17.880396	998.514257	11.620890
18.165575	1004.554709	11.625895
18.227756	994.371116	11.630899
18.025745	1002.001679	11.635904
18.308195	1001.073486	11.640909
18.724961	998.980494	11.645914
18.885360	991.739825	11.650919
18.662303	999.178186	11.655923
18.803359	1002.738811	11.660928
19.013137	991.009806	11.665933
18.853376	1003.716532	11.670938
18.769710	994.896711	11.675943
18.894757	996.803963	11.680947
18.702563	999.428912	11.685952
18.946910	994.543615	11.690957
18.827060	1007.236093	11.695962
18.799872	993.040488	11.700967
19.121734	999.026199	11.705971
18.904100	1009.351319	11.710976
19.415468	999.643327	11.715981
18.847029	1009.720022	11.720986
18.915469	1006.094470	11.725991
19.081923	999.549897	11.730995
18.908548	1002.039372	11.736000
19.280148	994.353402	11.741005
19.065881	1005.745660	11.746010
18.869507	1001.132515	11.751015
19.115080	1005.494972	11.756019
19.494026	1032.331545	11.761024
19.917662	1028.471129	11.766029
19.503172	1012.569373	11.771034
19.441597	1028.266363	11.776039
20.137618	1023.796337	11.781043
19.801848	1009.534804	11.786048
19.880507	1001.529670	11.791053
19.716760	994.364352	11.796058
19.464678	1000.126185	11.801063
20.088123	1009.381962	11.806067
19.992563	1021.050212	11.811072
19.938331	1010.815782	11.816077
19.722660	1018.164659	11.821082
19.685044	1029.640735	11.826087
19.986939	1018.996237	11.831091
19.974039	1023.868314	11.836096
19.927498	1019.254923	11.841101
20.188647	1024.696774	11.846106
19.964634	1016.306208	11.851111
20.439968	1022.953480	11.856115
20.098937	1028.999190	11.861120
19.987928	1014.722307	11.866125
20.153287	1030.815226	11.871130
20.441573	1042.024852	11.876135
20.416045	1056.159549	11.881139
20.624507	1056.298217	11.886144
20.899318	1058.315644	11.891149
20.990288	1057.569385	11.896154
20.881695	1049.501041	11.901159
20.994081	1027.410375	11.906163
20.386954	1024.534431	11.911168
20.777206	1028.077398	11.916173
20.820268	1048.097832	11.921178
20.895466	1055.207935	11.926183
21.258459	1061.805327	11.931187
21.211010	1054.865879	11.936192
20.896379	1045.584505	11.941197
20.592771	1041.811684	11.946202
20.563595	1062.707897	11.951207
21.084410	1053.503028	11.956211
20.953831	1063.940469	11.961216
20.984973	1062.539802	11.966221
20.877170	1045.871526	11.971226
21.010679	1068.273143	11.976231
21.140222	1074.475653	11.981235
21.132456	1091.309089	11.986240
21.389738	1097.678909	11.991245
21.341129	1082.625546	11.996250
21.079758	1092.587086	12.001255
21.803558	1075.652096	12.006259
21.683693	1080.960754	12.011264
21.937569	1082.621949	12.016269
22.107835	1077.710589	12.021274
21.800544	1085.682865	12.026279
21.878078	1071.981455	12.031283
22.088620	1085.012425	12.036288
21.955195	1070.149234	12.041293
21.921942	1087.351036	12.046298
22.180844	1090.034956	12.051303
22.177713	1066.532241	12.056307
21.984245	1063.678633	12.061312
22.005615	1048.705614	12.066317
22.005794	1051.033366	12.071322
21.875220	1049.123862	12.076327
21.920043	1056.606269	12.081331
21.528077	1052.219859	12.086336
21.740458	1053.826162	12.091341
21.537486	1062.904667	12.096346
21.863376	1054.159852	12.101351
21.611233	1061.241732	12.106355
21.324226	1058.224834	12.111360
21.683942	1054.983358	12.116365
21.612902	1059.109298	12.121370
21.705545	1060.764663	12.126375
21.877103	1053.895951	12.131379
21.637575	1059.138524	12.136384
21.556661	1060.952466	12.141389
21.785370	1067.430916	12.146394
21.758450	1054.063175	12.151399
22.047968	1049.840914	12.156403
21.931814	1058.162767	12.161408
21.883934	1050.641448	12.166413
22.017482	1054.477695	12.171418
21.762396	1064.785171	12.176423
21.791542	1055.303873	12.181427
21.716569	1051.817885	12.186432
21.983941	1051.538696	12.191437
21.750449	1045.166707	12.196442
21.814961	1063.534119	12.201447
21.847648	1057.324694	12.206451
21.974623	1056.314052	12.211456
21.850354	1060.891641	12.216461
21.832193	1058.929512	12.221466
21.720965	1056.086445	12.226471
22.034388	1050.191823	12.231475
21.696423	1040.480478	12.236480
22.026344	1031.798115	12.241485
22.015142	1030.396319	12.246490
21.867516	1029.645533	12.251495
21.813835	1023.511402	12.256499
21.674520	1027.443203	12.261504
21.752064	1022.363709	12.266509
21.585130	1022.491279	12.271514
21.711103	1027.934189	12.276519
21.626024	1026.187756	12.281523
21.433836	1027.563666	12.286528
21.745495	1023.107628	12.291533
21.740321	1032.312276	12.296538
21.378014	1026.172168	12.301543
21.931211	1038.235321	12.306547
21.754323	1049.743087	12.311552
21.813144	1040.950979	12.316557
21.907074	1030.785953	12.321562
21.712079	1032.712710	12.326567
21.924018	1030.054670	12.331571
21.661928	1023.829188	12.336576
21.834828	1027.266460	12.341581
22.017214	1036.070585	12.346586
21.530838	1034.072737	12.351591
21.794562	1031.915832	12.356595
21.670823	1040.625269	12.361600
21.759962	1032.784039	12.366605
21.917462	1029.940700	12.371610
21.715356	1040.175050	12.376615
21.820983	1039.431185	12.381619
21.974175	1035.713256	12.386624
21.966534	1019.044807	12.391629
21.889771	1041.713325	12.396634
21.762258	1032.698608	12.401639
21.922617	1036.628353	12.406643
21.914113	1032.371619	12.411648
21.926681	1035.670447	12.416653
21.874443	1033.519776	12.421658
22.013796	1037.197385	12.426663
21.964366	1039.427382	12.431667
21.894313	1044.526217	12.436672
21.960271	1023.687274	12.441677
21.986328	1012.717738	12.446682
21.674400	1014.144285	12.451687
21.450396	1009.439342	12.456691
21.556922	1015.968798	12.461696
21.650818	1015.725161	12.466701
21.703768	1029.401004	12.471706
21.929925	1044.681511	12.476711
21.822885	1035.493202	12.481715
21.428272	1020.310568	12.486720
21.949103	1034.528432	12.491725
22.007092	1022.061882	12.496730
21.447844	1020.665484	12.501735
21.835433	1013.440614	12.506739
21.928943	1019.951646	12.511744
21.792497	1015.835179	12.516749
21.253221	1019.958508	12.521754
21.280858	1020.167020	12.526759
22.335942	1034.304409	12.531763
22.012738	1035.541930	12.536768
21.907890	1011.927782	12.541773
21.902784	1022.263175	12.546778
21.685963	1012.843211	12.551783
21.610711	1017.182716	12.556787
21.695661	1016.920004	12.561792
21.733902	1018.336440	12.566797
21.905029	1013.353996	12.571802
21.686055	1020.768061	12.576807
21.828252	1020.136646	12.581811
21.795113	1024.827433	12.586816
21.853038	1022.329585	12.591821
21.949282	1012.358183	12.596826
22.102544	1017.172215	12.601831
21.881303	1014.447635	12.606835
21.671925	1017.192031	12.611840
21.816548	1020.288432	12.616845
21.862432	1021.227373	12.621850
21.731737	1021.970531	12.626855
22.044570	1013.267248	12.631859
21.802615	1023.421203	12.636864
21.850326	1017.890694	12.641869
21.993708	1027.801832	12.646874
21.855510	1015.235680	12.651879
22.238617	1014.803981	12.656883
21.985100	990.653717	12.661888
21.687389	990.281711	12.666893
21.591226	986.822775	12.671898
21.273367	989.833644	12.676903
21.657707	996.168962	12.681907
21.655576	1008.166103	12.686912
21.636295	1007.901090	12.691917
21.857361	1022.258220	12.696922
21.570650	1028.662725	12.701927
21.807425	1016.751184	12.706931
21.846747	1027.633048	12.711936
22.124874	1020.928719	12.716941
21.824820	1001.895579	12.721946
21.415634	998.923412	12.726951
21.559677	1000.430212	12.731955
21.482731	1019.674903	12.736960
21.797533	1019.093237	12.741965
22.081521	1024.482557	12.746970
21.684644	1025.067878	12.751975
21.640176	1021.014018	12.756979
21.589907	1020.813875	12.761984
21.756039	1023.400605	12.766989
21.875799	1028.385577	12.771994
21.773558	1040.304087	12.776999
21.791269	1030.875094	12.782003
22.050768	1032.653667	12.787008
21.963666	1019.166236	12.792013
21.648988	1006.252894	12.797018
21.374960	1005.779332	12.802023
21.870441	1007.818332	12.807027
21.569958	1011.646513	12.812032
21.547228	1021.541558	12.817037
21.949997	1022.163363	12.822042
21.895289	1021.285786	12.827047
21.929148	1004.664356	12.832051
21.523180	1010.387653	12.837056
21.474730	1006.197226	12.842061
22.222778	1022.854845	12.847066
21.587646	1022.919880	12.852071
22.045337	1009.421271	12.857075
21.723914	1010.428254	12.862080
21.775974	1003.244284	12.867085
21.431163	1006.374582	12.872090
21.374960	1011.464888	12.877095
21.586644	1021.529144	12.882099
21.732351	1031.619700	12.887104
21.781696	1035.951956	12.892109
21.901942	1037.733813	12.897114
21.872484	1038.082328	12.902119
22.020249	1022.846309	12.907123
21.685757	1018.977485	12.912128
21.626182	1009.434667	12.917133
21.690221	1002.608360	12.922138
21.554110	1009.088194	12.927143
22.180484	1002.817225	12.932147
21.582888	1001.531032	12.937152
21.814330	1011.271984	12.942157
21.966189	1007.106385	12.947162
21.796172	1006.969499	12.952167
22.121380	1000.492655	12.957171
21.658695	1011.949770	12.962176
21.621964	1006.044773	12.967181
21.758235	1009.456341	12.972186
21.498900	1010.163240	12.977191
21.791902	1000.660397	12.982195
21.858314	1000.108884	12.987200
21.894064	997.895296	12.992205
22.076467	1004.207626	12.997210
21.710785	1013.050256	13.002215
21.906542	1004.062853	13.007219
21.892350	1020.763182	13.012224
21.653914	1007.077530	13.017229
22.055888	1010.139193	13.022234
21.836292	1009.857238	13.027239
22.109788	1007.701933	13.032243
21.973010	1013.957931	13.037248
21.786171	1014.632766	13.042253
22.015091	1008.453570	13.047258
21.868367	1010.039864	13.052263
21.851713	983.584004	13.057267
21.367580	992.994334	13.062272
21.516728	986.766365	13.067277
21.971356	995.181668	13.072282
21.822290	1000.315168	13.077287
21.953067	986.141688	13.082291
21.633770	985.162798	13.087296
21.709801	983.608312	13.092301
21.954718	988.972308	13.097306
21.737239	981.782448	13.102311
21.711586	985.002199	13.107315
21.715885	990.959700	13.112320
21.373989	983.504231	13.117325
21.705090	986.604003	13.122330
21.696345	1004.921519	13.127335
21.853831	1013.206014	13.132339
21.710543	1008.350993	13.137344
21.726649	1001.354122	13.142349
21.455219	996.943774	13.147354
21.466020	1006.620557	13.152359
21.827998	1001.186601	13.157363
21.684711	1011.137139	13.162368
21.707160	1016.738492	13.167373
21.530955	1017.340662	13.172378
21.405612	1024.780801	13.177383
21.901260	1015.461689	13.182387
21.747429	1014.243503	13.187392
21.936257	1018.223900	13.192397
22.020577	1023.851660	13.197402
21.712721	1027.745681	13.202407
21.954618	1015.476905	13.207411
21.935040	1021.830918	13.212416
21.696714	1016.614131	13.217421
21.820771	1005.218931	13.222426
21.755524	1012.908119	13.227431
22.022808	1001.655672	13.232435
21.434006	1004.321797	13.237440
21.687882	992.409125	13.242445
21.785260	1002.930024	13.247450
21.764668	1004.649177	13.252455
22.043553	990.627127	13.257459
21.701340	995.990140	13.262464
21.523773	992.487411	13.267469
21.705015	996.855394	13.272474
21.324769	1001.855441	13.277479
21.695893	1004.772201	13.282483
21.619381	1022.125916	13.287488
21.578552	1019.960811	13.292493
21.827819	1027.371170	13.297498
21.817043	1022.854584	13.302503
21.891470	1016.329412	13.307507
21.840976	1020.171345	13.312512
21.673445	1026.138917	13.317517
21.861427	1014.126342	13.322522
21.951304	1027.375216	13.327527
21.821761	1009.097101	13.332531
21.425914	1010.590652	13.337536
21.549098	1016.557591	13.342541
21.992200	1015.293092	13.347546
21.719309	1029.136028	13.352551
21.820566	1027.609055	13.357555
21.639374	1038.235913	13.362560
21.873043	1029.796002	13.367565
21.880718	1014.598104	13.372570
21.457098	1017.455522	13.377575
21.753136	1016.925738	13.382579
21.640648	1022.160653	13.387584
21.897075	1019.956025	13.392589
21.815307	1019.361906	13.397594
21.646499	1028.498024	13.402599
21.741815	1022.401637	13.407603
21.585550	1029.805705	13.412608
21.791977	1033.031035	13.417613
22.076659	1027.499002	13.422618
21.567019	1023.733811	13.427623
21.859733	1017.135975	13.432627
21.663022	1013.025966	13.437632
21.731121	1023.490044	13.442637
21.857621	1009.627907	13.447642
21.284769	1010.335918	13.452647
21.871392	1011.235931	13.457651
21.419370	1026.280775	13.462656
21.674193	1031.441342	13.467661
22.000970	1033.690193	13.472666
21.676972	1037.366000	13.477671
22.004993	1029.093982	13.482675
21.789819	1038.152339	13.487680
21.956181	1039.157228	13.492685
21.834216	1014.333035	13.497690
21.715925	1018.490156	13.502695
21.764748	1007.573767	13.507699
21.687178	1009.256272	13.512704
22.033881	1005.991649	13.517709
21.938463	1011.272727	13.522714
21.698829	1006.805262	13.527719
21.884919	1003.829626	13.532723
21.450924	1021.172539	13.537728
21.759917	1005.948673	13.542733
21.864305	1008.314995	13.547738
21.613856	1012.830685	13.552743
21.670886	1004.286486	13.557747
21.822060	1009.794761	13.562752
21.808181	1007.511809	13.567757
21.844814	1003.960722	13.572762
21.889132	1004.805287	13.577767
22.163895	1006.899991	13.582771
21.683829	1016.314418	13.587776
21.883115	1010.617801	13.592781
22.053871	1006.198434	13.597786
21.606266	1012.081348	13.602791
21.713734	1006.080808	13.607795
21.630968	1011.933923	13.612800
21.740840	1003.523233	13.617805
21.924997	1005.944647	13.622810
21.750877	1012.023659	13.627815
21.823387	1010.868731	13.632819
21.756105	1011.770521	13.637824
21.815807	1006.578752	13.642829
21.963097	1003.166147	13.647834
21.869487	1014.346766	13.652839
22.115145	1013.653116	13.657843
21.998785	1007.481676	13.662848
21.754333	996.741388	13.667853
21.720431	980.379969	13.672858
21.535632	974.262039	13.677863
21.742323	980.788121	13.682867
21.655562	992.694660	13.687872
21.850061	1000.419692	13.692877
21.814100	989.646159	13.697882
21.270165	990.958306	13.702887
21.642078	1007.485070	13.707891
21.560352	1021.633427	13.712896
21.871968	1014.773938	13.717901
21.906157	1014.926207	13.722906
21.758468	1016.739753	13.727911
21.994367	1013.559037	13.732915
21.841927	1017.636442	13.737920
21.340637	1003.688340	13.742925
21.413950	1005.018750	13.747930
21.182151	1014.590716	13.752935
21.350779	1013.395225	13.757939
21.596988	1018.035149	13.762944
21.647255	1017.268574	13.767949
21.737464	1016.442008	13.772954
21.857246	1022.628704	13.777959
21.971565	1017.350944	13.782963
21.905223	1019.295031	13.787968
21.784461	1023.493551	13.792973
21.918790	1013.809410	13.797978
21.837110	1020.485587	13.802983
21.902482	1017.808343	13.807987
21.836926	1017.326765	13.812992
22.063637	1015.729319	13.817997
22.018349	1019.086261	13.823002
21.823560	1029.338360	13.828007
22.135296	1013.661429	13.833011
21.652324	1004.036317	13.838016
21.609851	990.790972	13.843021
21.829722	988.451820	13.848026
21.508950	992.174413	13.853031
21.558042	998.124773	13.858035
21.687279	1009.725621	13.863040
22.006183	1014.033805	13.868045
21.897442	1002.486487	13.873050
21.548943	992.698000	13.878055
21.965850	994.107662	13.883059
22.006598	994.192647	13.888064
21.864123	991.808774	13.893069
21.571030	985.673414	13.898074
21.766900	985.151721	13.903079
21.979576	981.375429	13.908083
21.447803	987.703874	13.913088
21.489310	985.404208	13.918093
21.753855	991.873755	13.923098
21.517782	994.349571	13.928103
21.773256	996.056236	13.933107
21.583885	1001.801760	13.938112
21.696440	1021.405767	13.943117
21.909697	1021.684030	13.948122
21.633045	1015.314207	13.953127
21.893786	1011.509739	13.958131
21.761625	1009.537411	13.963136
21.706282	1009.621950	13.968141
21.949794	992.438778	13.973146
21.556304	995.296118	13.978151
21.635414	975.503899	13.983155
21.441261	995.898010	13.988160
21.654161	1006.588159	13.993165
22.055376	1023.137078	13.998170
21.847854	1020.602711	14.003175
21.724881	1004.709668	14.008179
21.930506	1006.681347	14.013184
21.952699	999.098413	14.018189
21.745278	996.231138	14.023207
21.644978	999.421560	14.028224
21.701302	990.517004	14.033242
21.495308	996.321384	14.038259
21.646114	1007.942628	14.043277
21.894271	1022.206812	14.048295
22.007044	1024.998310	14.053312
22.105804	1018.253060	14.058330
21.908109	1010.252609	14.063347
21.778651	996.087513	14.068365
22.251208	997.714199	14.073383
21.802001	995.432575	14.078400
21.840441	987.781445	14.083418
21.606262	1004.291769	14.088435
21.621123	1018.829115	14.093453
22.112515	1023.915085	14.098471
21.766987	1026.995184	14.103488
22.281029	1023.608235	14.108506
21.688932	1032.302553	14.113523
22.000972	1021.153349	14.118541
21.996665	1024.119251	14.123559
21.747308	1036.553111	14.128576
22.136982	1023.461388	14.133594
21.933082	1029.784555	14.138611
22.024640	1032.722585	14.143629
21.831086	1022.140088	14.148647
21.769503	1033.123533	14.153664
22.089421	1040.805652	14.158682
22.062739	1051.829163	14.163699
22.205680	1056.907796	14.168717
22.617773	1051.693479	14.173735
22.563183	1059.466798	14.178752
22.277902	1058.640837	14.183770
22.327468	1059.976335	14.188787
22.229991	1067.503236	14.193805
22.461590	1056.398295	14.198823
22.420417	1058.610299	14.203840
22.476253	1056.598909	14.208858
22.612880	1067.552341	14.213875
22.260911	1057.007668	14.218893
22.435273	1051.400249	14.223911
22.482502	1057.507194	14.228928
22.566098	1061.431232	14.233946
22.604774	1055.883205	14.238963
22.427860	1064.391775	14.243981
22.544833	1058.359343	14.248999
22.361865	1067.425741	14.254016
22.485236	1060.313172	14.259034
22.532663	1064.889506	14.264051
22.309292	1066.254376	14.269069
22.655113	1054.382446	14.274087
22.823991	1069.392363	14.279104
22.881746	1064.473658	14.284122
22.705805	1070.276421	14.289139
22.546091	1065.030596	14.294157
22.617934	1060.919769	14.299175
22.443168	1066.173346	14.304192
22.682396	1061.969756	14.309210
22.672286	1057.730425	14.314227
22.444843	1062.802063	14.319245
22.727322	1065.678190	14.324263
22.505694	1061.939790	14.329280
22.539520	1060.048316	14.334298
22.789083	1083.261449	14.339315
22.830668	1090.534944	14.344333
22.841329	1089.284249	14.349351
22.794932	1105.564961	14.354368
22.718851	1091.748343	14.359386
23.025887	1093.107277	14.364403
22.763395	1094.671876	14.369421
22.832073	1094.126097	14.374439
22.992946	1107.726296	14.379456
22.781637	1101.889351	14.384474
22.891510	1101.692513	14.389491
22.745543	1097.770573	14.394509
23.098102	1099.073482	14.399527
22.873626	1103.342400	14.404544
23.164651	1101.886539	14.409562
23.063320	1099.252108	14.414579
23.070776	1112.702171	14.419597
23.349557	1116.260033	14.424615
23.302021	1121.958965	14.429632
23.113417	1116.179742	14.434650
23.209089	1115.346506	14.439667
23.317406	1131.044135	14.444685
23.489924	1124.540336	14.449703
23.067553	1118.513670	14.454720
23.260528	1131.471683	14.459738
23.171990	1130.376808	14.464755
23.029187	1135.197439	14.469773
23.807230	1120.717598	14.474791
23.626199	1133.000640	14.479808
23.466797	1135.895344	14.484826
23.700293	1125.612760	14.489843
23.339294	1131.204382	14.494861
23.515195	1128.190670	14.499879
23.279986	1137.642978	14.504896
23.477181	1130.671188	14.509914
23.749376	1126.979859	14.514931
23.489257	1132.330444	14.519949
23.822278	1123.858316	14.524967
23.557765	1124.790868	14.529984
23.599735	1122.866626	14.535002
23.755934	1126.321342	14.540019
23.594766	1130.661971	14.545037
23.800916	1121.198598	14.550055
23.664217	1125.384309	14.555072
23.999837	1121.590055	14.560090
24.128976	1119.277522	14.565107
23.730277	1109.378927	14.570125
23.667198	1091.861971	14.575143
23.789766	1109.350590	14.580160
23.586283	1115.038210	14.585178
23.869335	1113.357098	14.590195
23.848025	1127.318288	14.595213
24.010129	1123.056192	14.600231
23.897912	1123.377704	14.605248
23.856324	1127.449144	14.610266
23.883530	1129.434743	14.615283
23.965290	1129.989593	14.620301
23.848385	1130.028701	14.625319
23.986755	1119.883992	14.630336
23.946204	1119.923507	14.635354
23.881499	1114.714423	14.640371
23.930840	1120.083292	14.645389
24.163017	1122.876215	14.650407
24.141297	1128.841600	14.655424
24.208873	1129.965014	14.660442
23.938384	1126.413719	14.665459
23.919767	1132.600412	14.670477
23.891343	1125.342129	14.675495
23.921955	1125.859517	14.680512
24.096672	1123.409151	14.685530
24.337166	1129.598564	14.690547
24.094259	1127.329635	14.695565
24.100872	1132.211381	14.700583
24.080518	1133.646128	14.705600
24.191284	1144.403964	14.710618
24.125489	1158.076541	14.715635
24.122806	1158.581937	14.720653
24.474972	1160.487399	14.725671
24.314976	1159.358300	14.730688
24.266673	1158.834321	14.735706
24.616409	1161.960870	14.740723
24.421481	1160.838914	14.745741
24.771581	1152.337303	14.750759
24.539038	1157.747996	14.755776
24.650432	1161.400207	14.760794
25.176613	1153.175689	14.765811
24.453354	1156.284595	14.770829
24.715506	1137.043546	14.775847
24.541000	1128.362914	14.780864
24.205624	1133.281898	14.785882
24.565412	1148.252012	14.790899
24.810271	1153.984550	14.795917
24.713573	1157.866581	14.800935
24.706336	1162.810323	14.805952
24.873184	1161.207515	14.810970
25.126636	1147.767736	14.815987
24.612122	1145.963702	14.821005
24.788868	1153.978609	14.826023
24.681694	1158.965030	14.831040
24.767164	1158.822421	14.836058
25.103868	1158.312547	14.841075
25.133942	1167.030418	14.846093
25.249839	1146.631309	14.851111
24.705226	1139.972880	14.856128
24.603412	1134.378014	14.861146
24.958469	1136.827292	14.866163
24.568517	1153.054307	14.871181
24.696726	1160.767065	14.876199
24.658167	1157.787549	14.881216
24.799995	1154.710050	14.886234
25.275197	1156.039025	14.891251
25.039889	1157.021979	14.896269
25.137891	1147.737863	14.901287
24.802805	1149.752930	14.906304
25.159918	1149.088787	14.911322
25.517013	1142.299134	14.916339
25.193951	1154.401920	14.921357
25.441296	1153.906298	14.926375
25.082128	1149.334063	14.931392
25.171864	1158.726696	14.936410
25.107789	1148.870663	14.941427
24.836026	1149.706843	14.946445
25.014434	1152.742735	14.951463
25.134059	1150.079348	14.956480
25.092732	1162.370023	14.961498
25.620393	1171.596866	14.966515
25.638188	1181.688418	14.971533
25.558990	1162.747174	14.976551
25.477259	1151.335046	14.981568
25.193971	1159.786703	14.986586
25.360726	1155.865211	14.991603
25.576698	1170.907049	14.996621
25.682289	1174.739519	15.001639
25.540982	1166.212449	15.006656
25.506041	1162.673917	15.011674
25.629736	1158.767157	15.016691
25.712161	1180.468644	15.021709
25.627222	1173.917792	15.026727
25.720921	1160.077178	15.031744
25.584745	1159.774858	15.036762
25.772654	1166.878760	15.041779
25.850925	1169.029258	15.046797
25.600316	1169.810154	15.051815
26.020773	1159.323120	15.056832
25.608074	1162.012827	15.061850
25.656523	1152.735037	15.066867
25.787064	1177.839252	15.071885
25.816071	1180.788862	15.076903
26.210832	1183.392269	15.081920
26.310446	1170.434766	15.086938
26.039097	1152.180150	15.091955
25.869060	1151.493111	15.096973
25.886535	1149.763112	15.101991
26.060010	1155.351303	15.107008
25.607189	1148.681377	15.112026
26.038359	1153.961048	15.117043
26.062985	1163.549690	15.122061
26.623373	1171.193528	15.127079
26.329385	1152.778922	15.132096
26.030200	1147.162045	15.137114
26.301761	1141.977975	15.142131
26.393140	1150.113463	15.147149
26.246432	1144.846657	15.152167
26.292015	1139.912565	15.157184
25.985503	1151.550229	15.162202
26.121822	1139.593662	15.167219
26.428288	1151.674700	15.172237
26.191391	1158.753536	15.177255
26.416604	1147.489092	15.182272
26.128596	1155.705539	15.187290
26.636003	1148.858876	15.192307
26.451076	1146.116643	15.197325
26.410834	1146.915900	15.202343
26.289373	1141.549112	15.207360
26.108358	1150.110297	15.212378
26.379097	1148.632497	15.217395
26.070107	1152.949516	15.222413
26.284978	1159.814727	15.227431
26.734902	1171.144573	15.232448
26.771642	1175.916134	15.237466
26.591230	1158.947933	15.242483
26.280294	1158.827645	15.247501
26.255233	1177.239685	15.252519
26.587399	1168.843174	15.257536
26.409615	1173.738611	15.262554
26.819256	1174.720958	15.267571
26.889125	1174.834101	15.272589
26.563958	1177.813453	15.277607
26.787234	1170.714784	15.282624
26.647052	1171.559869	15.287642
26.658167	1169.620092	15.292659
26.550392	1170.592146	15.297677
26.713599	1181.893792	15.302695
26.894114	1181.740745	15.307712
26.722739	1179.388038	15.312730
26.804730	1170.979513	15.317747
26.640495	1170.115364	15.322765
26.728350	1179.898432	15.327783
27.323455	1181.714815	15.332800
26.913112	1178.366713	15.337818
27.144836	1169.545762	15.342835
27.163797	1171.718304	15.347853
27.017611	1180.428112	15.352871
27.206476	1179.930804	15.357888
26.725716	1178.664091	15.362906
27.137659	1193.389974	15.367923
27.312864	1196.360316	15.372941
27.155584	1205.880468	15.377959
27.441489	1202.348959	15.382976
27.331619	1190.496110	15.387994
27.530132	1177.842161	15.393011
27.418077	1184.067374	15.398029
27.089297	1170.366490	15.403047
27.507217	1158.808601	15.408064
27.091864	1177.819302	15.413082
27.081207	1171.945608	15.418099
27.045173	1176.215955	15.423117
27.287530	1201.744411	15.428135
27.773628	1200.114280	15.433152
27.851598	1205.184450	15.438170
27.732721	1190.976576	15.443187
27.510326	1178.542343	15.448205
27.057398	1181.872415	15.453223
27.195952	1186.221890	15.458240
27.003846	1202.971127	15.463258
27.312876	1205.015613	15.468275
27.487978	1204.451284	15.473293
27.584821	1204.310008	15.478311
27.961086	1202.944365	15.483328
27.620874	1207.793358	15.488346
27.859331	1201.080802	15.493363
28.100783	1204.599021	15.498381
27.542548	1214.870556	15.503399
27.934673	1215.320854	15.508416
27.743509	1214.641900	15.513434
27.933940	1201.927870	15.518451
28.084434	1205.418122	15.523469
27.845939	1209.992910	15.528487
27.949284	1209.845877	15.533504
27.942996	1205.967700	15.538522
27.883143	1211.865266	15.543539
28.064423	1206.863890	15.548557
28.394294	1199.488651	15.553575
28.724808	1192.371296	15.558592
28.509130	1193.140331	15.563610
28.207962	1176.982621	15.568627
28.040448	1167.545777	15.573645
27.947311	1174.644167	15.578663
28.116714	1169.177497	15.583680
28.056473	1176.893576	15.588698
28.037486	1188.564067	15.593715
28.315868	1197.665511	15.598733
28.110726	1200.934047	15.603751
28.483449	1192.630158	15.608768
28.007067	1201.954226	15.613786
28.067265	1204.414360	15.618803
28.147495	1191.291612	15.623821
27.927115	1205.339682	15.628839
28.035014	1190.908446	15.633856
27.747641	1193.235242	15.638874
28.401875	1216.234609	15.643891
28.670035	1218.672592	15.648909
28.471327	1218.344849	15.653927
28.733133	1218.101756	15.658944
28.432033	1207.993252	15.663962
28.385336	1214.881329	15.668979
28.755791	1214.938669	15.673997
28.648405	1219.010403	15.679015
28.959194	1214.704905	15.684032
28.539106	1200.268199	15.689050
28.489530	1194.287441	15.694067
28.779282	1197.239516	15.699085
28.661490	1226.924875	15.704103
28.792368	1209.677301	15.709120
28.743563	1220.988407	15.714138
28.657443	1223.607951	15.719155
28.807487	1222.858849	15.724173
28.759330	1230.726404	15.729191
28.933999	1220.974609	15.734208
28.796684	1228.547273	15.739226
28.803623	1216.936903	15.744243
29.026153	1229.435672	15.749261
28.671531	1229.036051	15.754279
28.983054	1229.771346	15.759296
28.861955	1230.006184	15.764314
28.750058	1227.374988	15.769331
28.824216	1224.684231	15.774349
28.952245	1227.753343	15.779367
29.165033	1221.781857	15.784384
28.649135	1235.591573	15.789402
28.720043	1224.284823	15.794419
29.375016	1247.403676	15.799437
29.140731	1264.056674	15.804455
29.330845	1255.519168	15.809472
29.547897	1259.088485	15.814490
29.296328	1262.545343	15.819507
29.564482	1260.071400	15.824525
29.451953	1249.780205	15.829543
29.281946	1234.273217	15.834560
29.359103	1231.960305	15.839578
29.228030	1255.921853	15.844595
29.632114	1253.029032	15.849613
29.197915	1256.278267	15.854631
29.796246	1256.914338	15.859648
29.882244	1258.438319	15.864666
29.312988	1238.628926	15.869683
29.520427	1245.685706	15.874701
29.723892	1251.380839	15.879719
29.704454	1253.889077	15.884736
29.682478	1260.241533	15.889754
29.560238	1251.126974	15.894771
29.704476	1257.945293	15.899789
29.549089	1258.438079	15.904807
29.763430	1252.578021	15.909824
30.123842	1254.320155	15.914842
29.901754	1253.720851	15.919859
30.094255	1252.644856	15.924877
29.621244	1255.621846	15.929895
29.547035	1256.192137	15.934912
29.681500	1259.356972	15.939930
29.757399	1256.491321	15.944947
30.115105	1256.177876	15.949965
29.851115	1258.760510	15.954983
30.069463	1256.675983	15.960000
30.218892	1251.936869	15.965018
29.875486	1255.463429	15.970035
29.991357	1246.185839	15.975053
29.801382	1259.699773	15.980071
30.163029	1259.570536	15.985088
30.128076	1257.278645	15.990106
30.004490	1258.817961	15.995123
30.399149	1243.132031	16.000141
29.999041	1258.723687	16.005159
30.077754	1257.746852	16.010176
30.086891	1260.035808	16.015194
30.251569	1266.655024	16.020211
30.541371	1264.614157	16.025229
30.480430	1263.543186	16.030247
30.168508	1259.979588	16.035264
30.211621	1268.635663	16.040282
30.579725	1274.724561	16.045299
30.658422	1278.695846	16.050317
30.258503	1275.537974	16.055335
30.569377	1276.031908	16.060352
30.596675	1277.880655	16.065370
30.309650	1283.363006	16.070387
30.497207	1283.624127	16.075405
30.423641	1281.990433	16.080423
30.231656	1277.627455	16.085440
30.343858	1278.832644	16.090458
29.995651	1289.631537	16.095475
30.841290	1286.025686	16.100493
30.517829	1304.867735	16.105511
31.122010	1322.495316	16.110528
31.224052	1307.096666	16.115546
31.061465	1293.880411	16.120563
30.917061	1286.344805	16.125581
30.847803	1284.337603	16.130599
30.930603	1277.169262	16.135616
31.136392	1269.499947	16.140634
30.952999	1277.962482	16.145651
31.015755	1269.164486	16.150669
30.755708	1275.615479	16.155687
31.028384	1289.678595	16.160704
31.229177	1292.041601	16.165722
31.002115	1321.131077	16.170739
31.403057	1305.776785	16.175757
31.362167	1307.555397	16.180775
31.443399	1289.224714	16.185792
31.457323	1280.568997	16.190810
31.420476	1271.298442	16.195827
31.460240	1262.875363	16.200845
31.301637	1275.622152	16.205863
31.195486	1264.282258	16.210880
31.442516	1264.282203	16.215898
31.321206	1259.909532	16.220915
31.352692	1252.951526	16.225933
31.551408	1267.076754	16.230951
31.382922	1264.029059	16.235968
31.604335	1260.995476	16.240986
31.541341	1266.726819	16.246003
31.670333	1263.418529	16.251021
31.316344	1266.973522	16.256039
31.358784	1259.419143	16.261056
31.888527	1274.143626	16.266074
31.657311	1286.140634	16.271091
31.573599	1276.493719	16.276109
31.781850	1288.481207	16.281127
31.701562	1290.877242	16.286144
31.819189	1293.710491	16.291162
31.665486	1287.956308	16.296179
31.854349	1293.627044	16.301197
31.860195	1295.977881	16.306215
32.036682	1299.478170	16.311232
32.032166	1294.145373	16.316250
32.033098	1303.941601	16.321267
32.065023	1291.396709	16.326285
31.980919	1290.957875	16.331303
31.831579	1293.361776	16.336320
32.025813	1287.202093	16.341338
31.942417	1302.922618	16.346355
32.349536	1290.521604	16.351373
32.284840	1297.599787	16.356391
31.995352	1287.116555	16.361408
32.644296	1291.086566	16.366426
32.221909	1293.655140	16.371443
32.171080	1300.646166	16.376461
31.993455	1301.597907	16.381479
32.131427	1284.684179	16.386496
32.299818	1294.295599	16.391514
32.017813	1294.628461	16.396531
32.374412	1284.925477	16.401549
31.878812	1298.730443	16.406567
32.093541	1293.518416	16.411584
32.224871	1291.591698	16.416602
31.916210	1306.466441	16.421619
32.638411	1312.671922	16.426637
32.523722	1320.420356	16.431655
32.407874	1323.770637	16.436672
32.917028	1320.466989	16.441690
32.612509	1327.831981	16.446707
32.893848	1325.082995	16.451725
32.834364	1323.034115	16.456743
32.857311	1325.323239	16.461760
32.942846	1321.396566	16.466778
32.791058	1326.277684	16.471795
32.912840	1316.663253	16.476813
32.816061	1324.352202	16.481831
32.555735	1332.451857	16.486848
33.037796	1316.044809	16.491866
32.730936	1326.956689	16.496883
32.701515	1326.127661	16.501901
32.916403	1316.984464	16.506919
32.959937	1318.848717	16.511936
33.007794	1324.011038	16.516954
32.744216	1335.807175	16.521971
32.611115	1317.297485	16.526989
32.774405	1330.946275	16.532007
32.702425	1333.061769	16.537024
33.070882	1336.164136	16.542042
33.015350	1356.435143	16.547059
33.201124	1356.943525	16.552077
33.534544	1355.286603	16.557095
33.481909	1362.552450	16.562112
33.420364	1361.165378	16.567130
33.425854	1361.595542	16.572147
33.514485	1355.440087	16.577165
33.382190	1359.093459	16.582183
33.102647	1364.307221	16.587200
33.541644	1354.074291	16.592218
33.375469	1358.597477	16.597235
33.591515	1350.161964	16.602253
33.586490	1361.601483	16.607271
33.646018	1360.156561	16.612288
33.831030	1353.204698	16.617306
33.557603	1351.612308	16.622323
33.481392	1356.444415	16.627341
33.634777	1349.411078	16.632359
33.592577	1348.250592	16.637376
33.951405	1351.177525	16.642394
33.915146	1359.477424	16.647411
33.905666	1355.512410	16.652429
33.857779	1354.352830	16.657447
33.823778	1354.309501	16.662464
33.989492	1358.134005	16.667482
33.875317	1360.178364	16.672499
33.940645	1361.024506	16.677517
33.858866	1349.677513	16.682535
33.805880	1356.244176	16.687552
33.955949	1356.696116	16.692570
33.886153	1361.654622	16.697587
33.871243	1374.531957	16.702605
33.952663	1376.841652	16.707623
34.143422	1380.876108	16.712640
33.881537	1381.487346	16.717658
34.202664	1393.536360	16.722675
34.268863	1383.216566	16.727693
34.591736	1377.851191	16.732711
34.497439	1384.240404	16.737728
34.388170	1385.004275	16.742746
34.445823	1387.631594	16.747763
33.870113	1382.493684	16.752781
34.284432	1383.807222	16.757799
34.040103	1387.358126	16.762816
34.378640	1396.414707	16.767834
34.094284	1403.995181	16.772851
34.840905	1401.528284	16.777869
34.652339	1409.204387	16.782887
34.628773	1414.273519	16.787904
35.124242	1416.947430	16.792922
35.050006	1415.094380	16.797939
35.052232	1392.161498	16.802957
34.503096	1381.217791	16.807975
34.572582	1385.609016	16.812992
34.963587	1389.020057	16.818010
34.864993	1389.609973	16.823027
34.603523	1393.282380	16.828045
35.046458	1402.935822	16.833063
34.678712	1413.781968	16.838080
35.131162	1404.096655	16.843098
34.898747	1406.824509	16.848115
34.953271	1409.269852	16.853133
34.811066	1402.090141	16.858151
34.907943	1411.750798	16.863168
35.290827	1407.773535	16.868186
35.009880	1408.954913	16.873203
35.137481	1411.451527	16.878221
35.093199	1406.060534	16.883239
34.956537	1410.173171	16.888256
35.000914	1402.146481	16.893274
35.085327	1408.539453	16.898291
35.257996	1420.290467	16.903309
35.551920	1425.560666	16.908327
35.395709	1434.676510	16.913344
35.738399	1434.983684	16.918362
35.642991	1423.361942	16.923379
35.572209	1413.812765	16.928397
35.537110	1405.584808	16.933415
35.532726	1411.129100	16.938432
35.790026	1411.580458	16.943450
35.621725	1418.090818	16.948467
35.279149	1412.953470	16.953485
35.481779	1422.388048	16.958503
35.939690	1432.741508	16.963520
35.969325	1424.897277	16.968538
35.878507	1419.858208	16.973555
35.817692	1424.746087	16.978573
36.214488	1423.080623	16.983591
35.824546	1431.858557	16.988608
36.003523	1427.899650	16.993626
36.250684	1435.099632	16.998643
36.074824	1419.830130	17.003661
36.177338	1416.028931	17.008679
35.787676	1420.690028	17.013696
35.950435	1424.073767	17.018714
36.246261	1426.463327	17.023731
36.235255	1429.732415	17.028749
36.135931	1424.042653	17.033767
35.940073	1421.842468	17.038784
35.967456	1423.563800	17.043802
36.503111	1426.898296	17.048819
36.167335	1429.916357	17.053837
36.413400	1426.469018	17.058855
36.562225	1428.811232	17.063872
36.432163	1427.844871	17.068890
36.699345	1420.710764	17.073907
36.563072	1425.462806	17.078925
36.646321	1423.773411	17.083943
36.306691	1435.092524	17.088960
36.621771	1420.618581	17.093978
36.515505	1425.446852	17.098995
36.442347	1428.113131	17.104013
36.634722	1417.395647	17.109031
36.641357	1429.630133	17.114048
36.779370	1423.736560	17.119066
36.551268	1426.079895	17.124083
36.478429	1418.416397	17.129101
36.691556	1426.719823	17.134119
36.393789	1426.303261	17.139136
36.618691	1426.611916	17.144154
36.540816	1445.040583	17.149171
36.907605	1460.533746	17.154189
37.004294	1453.250626	17.159207
37.007650	1467.992398	17.164224
37.166534	1461.247581	17.169242
36.861582	1456.947398	17.174259
37.023787	1468.556969	17.179277
37.252083	1453.878172	17.184295
36.849326	1466.067861	17.189312
37.130314	1460.171922	17.194330
37.207430	1464.083732	17.199347
37.055241	1467.101625	17.204365
37.178366	1457.920276	17.209383
37.187246	1460.599433	17.214400
37.276047	1468.960464	17.219418
37.466819	1469.290294	17.224435
37.410504	1482.128708	17.229453
37.706228	1479.754944	17.234471
37.354156	1492.689300	17.239488
37.529179	1484.879268	17.244506
37.943230	1487.847762	17.249523
37.483091	1489.741237	17.254541
37.357563	1485.596484	17.259559
37.445781	1488.686944	17.264576
37.571593	1482.819676	17.269594
37.717922	1484.022586	17.274611
37.585554	1485.317922	17.279629
37.824387	1480.523576	17.284647
37.556345	1480.606452	17.289664
37.189728	1487.269598	17.294682
37.729850	1493.691396	17.299699
37.803032	1518.334203	17.304717
38.155658	1510.981136	17.309735
37.808116	1523.203753	17.314752
38.353477	1520.460606	17.319770
37.995917	1514.629512	17.324787
37.813240	1528.146462	17.329805
38.430430	1511.345606	17.334823
38.028273	1511.543469	17.339840
38.238939	1511.271561	17.344858
38.501457	1518.594197	17.349875
38.652185	1518.057342	17.354893
38.584815	1504.566147	17.359911
38.241614	1515.133948	17.364928
38.815719	1509.459458	17.369946
39.009673	1506.200532	17.374963
38.391190	1496.913261	17.379981
38.909235	1480.172299	17.384999
38.519007	1475.833797	17.390016
38.286061	1478.125214	17.395034
38.597287	1474.421282	17.400051
38.276826	1477.613884	17.405069
38.636171	1490.854014	17.410087
38.593678	1503.673725	17.415104
38.862570	1512.419000	17.420122
38.966800	1509.712384	17.425139
38.550879	1513.530581	17.430157
39.000265	1508.507583	17.435175
38.769476	1516.145642	17.440192
38.968201	1513.044837	17.445210
39.184266	1508.286362	17.450227
39.169998	1512.805819	17.455245
39.214572	1500.789652	17.460263
39.149767	1510.490318	17.465280
39.286858	1513.384218	17.470298
39.221667	1503.977243	17.475315
39.042722	1509.375583	17.480333
39.091339	1503.542641	17.485351
38.796741	1511.856297	17.490368
38.622754	1510.974804	17.495386
38.567928	1506.788094	17.500403
38.857916	1513.108212	17.505421
39.194115	1526.957712	17.510439
39.375259	1533.261376	17.515456
39.307032	1538.300706	17.520474
39.654987	1534.339205	17.525491
39.231262	1548.748026	17.530509
39.602235	1538.219061	17.535527
39.705854	1537.671627	17.540544
39.538205	1539.494079	17.545562
39.775563	1527.091623	17.550579
39.776311	1535.938667	17.555597
40.023819	1526.621028	17.560615
39.911633	1540.415413	17.565632
39.648560	1525.577368	17.570650
39.872584	1529.687576	17.575667
39.835278	1532.186912	17.580685
39.684687	1527.855798	17.585703
39.719852	1535.019635	17.590720
39.702750	1532.755530	17.595738
39.858275	1528.644598	17.600755
39.966795	1535.441216	17.605773
40.065647	1521.191216	17.610791
40.268286	1530.624290	17.615808
39.841503	1538.586216	17.620826
40.143370	1547.836727	17.625843
40.037051	1566.280308	17.630861
40.363773	1564.952425	17.635879
40.777274	1550.303774	17.640896
40.295829	1562.308666	17.645914
40.036643	1560.043836	17.650931
40.113574	1566.699993	17.655949
40.492580	1553.850185	17.660967
40.222193	1569.786445	17.665984
40.181840	1570.747773	17.671002
40.520294	1556.568859	17.676019
40.351427	1571.311458	17.681037
40.547595	1569.625275	17.686055
40.746277	1561.669063	17.691072
40.364342	1565.681639	17.696090
40.705719	1559.381179	17.701107
40.515420	1570.903109	17.706125
40.635457	1573.789515	17.711143
40.726026	1584.400666	17.716160
40.692630	1594.514040	17.721178
41.020205	1590.665105	17.726195
40.891576	1593.675334	17.731213
40.834784	1593.696203	17.736231
41.124074	1582.619418	17.741248
41.146770	1595.137787	17.746266
41.221654	1580.278825	17.751283
40.888613	1596.367472	17.756301
41.214150	1590.683040	17.761319
41.306661	1587.272737	17.766336
41.120854	1593.218860	17.771354
41.274908	1581.490350	17.776371
41.280673	1590.121111	17.781389
41.220302	1588.178520	17.786407
41.492580	1583.186101	17.791424
41.213464	1588.957542	17.796442
41.616476	1588.975087	17.801459
41.287594	1597.529439	17.806477
41.299052	1585.225884	17.811495
41.700535	1604.791962	17.816512
41.718215	1611.370281	17.821530
41.717926	1607.017533	17.826547
42.171122	1599.929971	17.831565
41.965422	1594.163507	17.836583
41.876188	1578.102905	17.841600
41.559591	1568.042240	17.846618
41.952400	1577.365575	17.851635
41.496491	1586.369638	17.856653
41.927242	1591.132771	17.861671
42.037142	1592.148794	17.866688
42.069714	1605.703852	17.871706
42.067137	1601.124155	17.876723
42.071099	1592.793116	17.881741
42.342885	1600.856039	17.886759
42.751146	1600.310359	17.891776
42.303897	1590.033760	17.896794
42.208925	1574.050374	17.901811
42.171539	1577.901034	17.906829
42.327550	1581.672872	17.911847
42.425207	1588.930596	17.916864
41.878743	1597.278960	17.921882
42.605525	1602.781445	17.926899
42.974954	1599.529122	17.931917
42.433664	1607.418892	17.936935
42.645501	1589.382412	17.941952
42.362163	1596.625390	17.946970
42.404517	1594.127625	17.951987
42.502417	1598.556857	17.957005
42.529887	1597.685705	17.962023
42.989772	1586.622612	17.967040
42.614278	1607.944708	17.972058
42.771342	1599.044952	17.977075
42.764599	1592.161311	17.982093
42.830540	1601.931641	17.987111
42.951533	1595.988014	17.992128
42.940583	1604.096029	17.997146
43.317493	1587.048672	18.002163
43.084568	1604.066802	18.007181
43.105507	1592.169166	18.012199
43.360679	1578.633544	18.017216
42.879601	1593.762602	18.022234
42.779115	1578.746768	18.027251
43.120944	1590.234191	18.032269
42.930858	1584.196239	18.037287
42.962710	1592.689126	18.042304
43.305657	1606.176597	18.047322
43.490601	1616.579228	18.052339
43.569654	1611.406817	18.057357
43.578618	1626.267412	18.062375
43.715149	1611.553538	18.067392
43.670986	1628.132583	18.072410
43.713431	1610.728741	18.077427
43.977292	1609.879668	18.082445
43.443601	1606.249883	18.087463
43.608695	1604.879342	18.092480
43.519861	1615.288665	18.097498
43.592711	1621.976961	18.102515
43.711422	1617.030258	18.107533
43.571101	1620.520583	18.112551
44.213745	1608.273662	18.117568
43.792449	1623.902906	18.122586
44.090642	1614.117779	18.127603
44.153684	1620.894946	18.132621
43.939132	1618.689846	18.137639
44.084768	1614.799130	18.142656
43.861689	1619.359787	18.147674
43.780980	1617.458190	18.152691
43.940462	1625.822198	18.157709
43.857601	1639.490870	18.162727
44.468433	1645.904607	18.167744
44.063170	1648.319490	18.172762
44.486019	1650.297125	18.177779
44.449414	1650.501976	18.182797
44.166431	1651.045011	18.187815
44.571235	1650.823157	18.192832
44.556365	1653.792445	18.197850
44.612551	1650.033182	18.202867
44.539113	1650.654491	18.207885
44.534727	1657.433777	18.212903
44.874004	1653.100799	18.217920
44.719570	1649.661433	18.222938
44.732476	1652.395829	18.227955
44.501845	1651.163116	18.232973
44.561124	1640.256684	18.237991
44.719274	1654.332127	18.243008
44.732779	1664.775504	18.248026
45.095884	1663.728906	18.253043
45.380804	1675.289183	18.258061
45.107158	1680.147377	18.263079
45.185122	1671.703025	18.268096
45.111813	1679.514267	18.273114
44.996568	1675.779191	18.278131
45.299270	1670.244670	18.283149
45.078949	1664.467925	18.288167
45.453980	1666.278571	18.293184
45.082533	1669.149775	18.298202
45.064942	1672.548963	18.303219
45.326221	1671.923682	18.308237
45.068903	1670.505661	18.313255
45.348910	1673.507371	18.318272
45.514597	1682.319548	18.323290
45.719324	1689.833184	18.328307
45.867207	1688.694270	18.333325
45.853528	1684.935128	18.338343
45.768188	1678.970886	18.343360
45.910920	1665.941569	18.348378
45.588816	1676.520279	18.353395
45.642077	1684.579557	18.358413
45.616999	1701.784105	18.363431
45.861168	1685.232100	18.368448
46.075754	1691.349591	18.373466
46.135433	1704.456011	18.378483
46.178235	1692.665711	18.383501
46.282739	1695.708785	18.388519
46.231983	1691.504068	18.393536
46.277528	1698.945561	18.398554
46.329343	1690.732684	18.403571
46.452161	1699.260680	18.408589
46.104586	1700.423603	18.413607
46.442892	1693.875023	18.418624
46.188073	1689.898703	18.423642
46.287539	1706.728656	18.428659
46.497048	1693.458989	18.433677
46.382810	1691.890726	18.438695
46.401677	1702.824877	18.443712
46.366807	1694.245126	18.448730
46.461038	1707.930454	18.453747
46.838642	1702.155087	18.458765
46.661507	1722.029904	18.463783
46.804778	1711.879283	18.468800
47.192319	1724.284520	18.473818
46.820008	1709.993850	18.478835
46.976416	1707.019311	18.483853
46.806387	1718.587678	18.488871
47.007177	1708.681946	18.493888
47.123483	1724.616485	18.498906
46.931735	1722.318851	18.503923
47.231183	1714.334687	18.508941
46.857899	1723.674104	18.513959
46.982569	1725.704021	18.518976
47.241092	1714.489675	18.523994
46.975450	1729.371357	18.529011
47.211232	1716.914719	18.534029
47.123081	1721.362648	18.539047
47.218755	1714.398119	18.544064
47.280089	1722.536360	18.549082
47.181115	1733.535734	18.554099
47.875697	1747.249635	18.559117
47.653394	1758.009129	18.564135
47.754418	1758.941630	18.569152
47.818005	1747.663172	18.574170
47.553355	1752.423994	18.579187
47.825435	1748.981084	18.584205
47.317008	1747.668387	18.589223
47.461793	1748.765379	18.594240
47.794764	1747.843925	18.599258
47.821825	1737.748001	18.604275
47.911557	1742.248584	18.609293
47.504327	1750.089520	18.614311
48.067526	1758.536309	18.619328
48.181323	1765.964592	18.624346
47.867369	1772.801951	18.629363
48.291519	1766.673047	18.634381
47.900270	1782.301601	18.639399
47.990010	1774.482205	18.644416
48.088551	1784.098797	18.649434
48.211772	1777.248616	18.654451
48.488588	1778.941224	18.659469
48.147732	1785.917382	18.664487
48.496430	1794.404693	18.669504
48.625329	1803.571260	18.674522
48.664454	1799.814680	18.679539
48.997595	1794.947773	18.684557
49.066692	1798.709932	18.689575
48.880904	1791.070543	18.694592
48.898034	1778.787944	18.699610
48.842037	1772.676616	18.704627
49.096584	1762.566420	18.709645
48.841570	1769.955986	18.714663
49.045780	1773.337131	18.719680
48.956709	1782.870376	18.724698
48.869816	1789.103631	18.729715
49.229568	1796.847448	18.734733
49.163748	1795.771709	18.739751
48.949159	1797.302782	18.744768
49.172318	1795.360569	18.749786
48.957466	1802.213600	18.754803
49.349706	1798.893885	18.759821
49.303292	1793.032722	18.764839
49.157641	1792.278835	18.769856
49.498481	1788.058834	18.774874
49.428336	1795.996272	18.779891
49.830780	1784.603181	18.784909
49.701918	1796.570913	18.789927
49.761875	1788.332299	18.794944
49.405145	1798.429733	18.799962
49.230999	1803.921805	18.804979
49.748967	1802.132364	18.809997
49.718336	1821.594602	18.815015
50.141672	1819.170545	18.820032
50.217134	1818.213069	18.825050
49.852753	1818.974385	18.830067
50.351330	1820.719728	18.835085
50.225621	1819.291716	18.840103
50.047776	1803.307923	18.845120
50.068346	1803.046662	18.850138
50.042832	1819.681157	18.855155
50.183037	1800.639594	18.860173
50.298864	1817.304246	18.865191
50.336007	1811.628751	18.870208
50.403704	1817.514086	18.875226
50.252381	1811.812014	18.880243
50.564027	1813.669757	18.885261
50.420113	1815.206079	18.890279
50.261691	1811.644605	18.895296
50.028887	1812.460448	18.900314
50.142597	1827.409157	18.905331
50.593880	1831.878854	18.910349
50.491432	1850.601410	18.915367
50.810301	1847.670153	18.920384
51.257671	1838.377077	18.925402
51.210986	1836.618687	18.930419
51.225914	1837.520875	18.935437
50.882065	1846.559925	18.940455
51.170780	1835.155042	18.945472
51.136655	1847.602460	18.950490
51.134311	1840.207517	18.955507
51.620049	1842.947562	18.960525
51.385957	1843.249195	18.965543
51.263068	1843.702993	18.970560
51.425605	1832.680842	18.975578
51.344325	1839.024130	18.980595
51.563174	1839.925261	18.985613
51.541658	1829.575092	18.990631
51.577620	1844.153159	18.995648
51.569235	1836.063853	19.000666
51.261172	1837.656244	19.005683
51.445111	1832.366348	19.010701
51.683606	1835.506855	19.015719
51.245062	1845.230377	19.020736
51.440363	1836.264599	19.025754
51.247665	1835.396294	19.030771
51.746716	1846.279146	19.035789
51.749897	1855.131502	19.040807
51.828195	1856.034598	19.045824
52.080749	1858.800821	19.050842
52.005459	1862.223413	19.055859
52.260114	1858.113099	19.060877
52.034546	1867.654795	19.065895
52.013231	1870.540206	19.070912
52.319999	1860.099121	19.075930
52.221824	1860.035347	19.080947
52.495008	1867.242408	19.085965
52.533495	1863.224771	19.090983
52.132292	1864.374234	19.096000
52.724215	1862.567487	19.101018
52.288880	1860.036522	19.106035
52.768972	1870.108315	19.111053
52.757549	1887.547663	19.116071
52.544617	1891.483033	19.121088
52.824287	1888.866355	19.126106
52.951320	1886.093107	19.131123
53.017520	1880.707917	19.136141
53.040667	1890.084900	19.141159
52.666203	1882.723321	19.146176
52.669267	1888.061312	19.151194
52.970918	1890.299787	19.156211
53.181200	1891.875595	19.161229
53.418099	1886.360926	19.166247
52.966025	1900.573250	19.171264
53.201066	1888.024556	19.176282
53.099222	1894.749488	19.181299
53.323523	1888.626448	19.186317
52.841818	1881.260734	19.191335
53.067922	1901.949304	19.196352
53.460213	1918.265580	19.201370
53.282442	1915.701396	19.206387
53.580176	1911.567679	19.211405
53.465550	1922.886680	19.216423
53.231247	1923.502978	19.221440
53.580689	1924.728595	19.226458
53.489511	1920.215628	19.231475
53.488072	1929.914333	19.236493
53.683299	1950.611043	19.241511
53.632634	1961.034976	19.246528
54.053760	1943.512142	19.251546
54.022197	1961.923851	19.256563
54.109499	1949.187076	19.261581
54.487481	1949.027704	19.266599
54.460391	1949.582640	19.271616
55.020333	1932.236686	19.276634
54.741923	1934.433953	19.281651
55.048035	1921.302844	19.286669
55.026299	1914.978336	19.291687
54.726874	1907.162723	19.296704
54.880193	1899.035010	19.301722
54.761587	1900.380101	19.306739
54.889726	1894.704221	19.311757
54.617896	1896.780875	19.316775
54.490368	1898.103790	19.321792
54.429065	1902.488500	19.326810
54.154780	1902.131889	19.331827
54.704273	1894.460138	19.336845
54.392753	1904.971251	19.341863
54.794883	1916.233797	19.346880
55.083597	1930.695345	19.351898
54.624350	1933.608918	19.356915
54.966194	1935.273870	19.361933
55.580899	1928.511208	19.366951
55.163887	1940.059357	19.371968
54.921492	1934.466935	19.376986
54.664093	1935.604482	19.382003
55.278548	1925.526449	19.387021
55.254876	1928.289541	19.392039
55.508050	1944.897828	19.397056
56.030191	1934.360991	19.402074
55.855801	1932.825104	19.407091
55.773721	1926.835857	19.412109
55.959209	1924.131151	19.417127
55.914657	1925.292961	19.422144
56.026762	1914.368461	19.427162
55.962844	1921.483004	19.432179
55.911728	1921.512407	19.437197
56.140368	1918.669463	19.442215
55.902116	1922.800017	19.447232
56.047836	1911.414732	19.452250
56.176212	1913.998619	19.457267
56.101215	1926.820740	19.462285
56.093076	1923.282467	19.467303
55.720532	1921.614574	19.472320
56.114753	1942.404604	19.477338
55.759389	1947.944506	19.482355
56.039186	1954.993241	19.487373
56.364029	1950.416281	19.492391
56.545963	1951.866831	19.497408
56.676941	1939.430650	19.502426
56.715177	1950.565621	19.507443
56.639767	1950.473046	19.512461
56.519279	1943.587714	19.517479
56.479410	1951.194766	19.522496
56.971760	1966.105260	19.527514
56.913622	1971.847903	19.532531
57.025387	1968.826157	19.537549
57.276583	1973.664463	19.542567
57.020240	1976.889420	19.547584
57.392045	1975.022588	19.552602
57.141082	1971.327169	19.557619
57.038396	1974.397836	19.562637
57.317150	1970.720985	19.567655
57.431212	1977.759979	19.572672
57.280773	1973.168349	19.577690
57.291612	1977.805866	19.582707
57.554590	1970.949039	19.587725
57.854991	1957.864429	19.592743
57.350977	1970.734552	19.597760
57.503300	1970.274511	19.602778
57.448069	1962.994914	19.607795
57.547073	1965.768340	19.612813
57.821893	1959.434277	19.617831
58.077339	1965.222872	19.622848
58.005378	1954.978194	19.627866
57.301645	1971.317505	19.632883
57.415340	1964.139966	19.637901
57.830422	1975.489376	19.642919
57.953316	1987.612188	19.647936
58.213064	1996.731267	19.652954
58.209764	1999.401454	19.657971
58.635273	1996.186513	19.662989
58.446338	1996.985929	19.668007
58.458396	1994.852394	19.673024
58.524545	1999.396934	19.678042
58.233723	2000.693198	19.683059
58.318109	1994.840198	19.688077
58.922107	1987.088915	19.693095
58.527927	1997.264823	19.698112
58.593670	1997.500552	19.703130
58.753512	1989.341858	19.708147
58.723340	1995.796624	19.713165
58.492179	1992.869674	19.718183
58.323083	1993.155438	19.723200
58.912814	2005.790606	19.728218
58.875219	2022.261291	19.733235
58.802193	2022.247780	19.738253
58.961180	2036.312447	19.743271
58.735158	2035.446297	19.748288
58.883061	2029.375497	19.753306
59.252773	2030.688349	19.758323
59.163373	2028.400300	19.763341
59.382738	2045.773143	19.768359
59.344427	2043.633474	19.773376
59.757600	2045.572594	19.778394
59.561551	2050.994311	19.783411
59.691259	2042.948155	19.788429
59.809710	2037.185668	19.793447
59.769105	2048.368683	19.798464
59.973703	2040.107648	19.803482
59.986657	2036.616325	19.808499
59.563632	2044.943682	19.813517
59.861550	2035.627121	19.818535
60.026787	2043.918088	19.823552
60.153748	2037.572174	19.828570
59.721606	2037.553791	19.833587
59.675509	2044.748143	19.838605
60.087582	2040.970570	19.843623
60.050631	2078.623060	19.848640
60.189994	2068.258865	19.853658
60.353917	2065.001460	19.858675
60.243755	2078.165977	19.863693
60.273241	2073.015466	19.868711
60.166280	2080.099195	19.873728
60.299123	2070.997716	19.878746
60.682268	2067.966496	19.883763
60.635118	2086.602664	19.888781
60.826931	2089.097809	19.893799
60.791630	2091.013276	19.898816
60.822308	2096.368178	19.903834
60.979955	2105.081998	19.908851
60.720963	2098.767716	19.913869
61.009540	2099.914958	19.918887
61.148738	2097.189286	19.923904
61.069520	2097.937388	19.928922
61.527111	2096.599604	19.933939
61.151290	2096.181307	19.938957
61.652596	2088.931671	19.943975
61.370471	2101.662694	19.948992
61.427732	2097.516146	19.954010
61.533950	2085.669008	19.959027
61.571332	2094.409080	19.964045
61.934817	2089.162826	19.969063
61.646264	2084.548350	19.974080
61.736275	2088.641547	19.979098
62.309189	2099.696874	19.984115
62.011109	2095.974326	19.989133
61.908504	2082.914543	19.994151
62.075560	2093.377790	19.999168
62.071090	2095.359921	20.004186
62.325159	2100.784602	20.009203
62.178218	2110.582143	20.014221
62.368222	2104.741359	20.019239
62.251435	2108.245352	20.024256
62.520072	2108.832581	20.029274
62.643428	2105.490391	20.034291
62.609087	2117.030356	20.039309
62.544806	2112.380107	20.044327
62.538674	2119.341586	20.049344
62.447151	2103.031422	20.054362
62.838064	2109.168168	20.059379
62.576702	2100.284491	20.064397
62.577512	2105.344470	20.069415
62.626561	2112.410415	20.074432
62.516483	2102.054510	20.079450
62.900211	2119.077945	20.084467
62.658203	2132.575025	20.089485
62.980130	2134.901550	20.094503
63.013168	2136.681845	20.099520
63.098834	2133.817611	20.104538
63.279701	2130.743910	20.109555
63.115160	2141.353674	20.114573
63.425831	2141.041426	20.119591
63.165309	2137.037574	20.124608
63.109294	2132.174409	20.129626
63.347257	2148.462854	20.134643
63.425284	2160.866697	20.139661
63.833914	2156.167764	20.144679
63.845288	2164.919105	20.149696
64.052164	2147.060498	20.154714
64.208185	2143.471609	20.159731
64.119190	2152.876084	20.164749
63.907200	2145.508125	20.169767
64.284543	2148.820847	20.174784
64.839065	2148.365883	20.179802
64.246323	2151.597327	20.184819
64.194303	2154.221824	20.189837
64.422503	2145.911344	20.194855
64.597166	2149.778681	20.199872
64.640444	2152.048175	20.204890
64.667218	2148.546755	20.209907
64.472478	2158.129346	20.214925
64.574616	2152.467739	20.219943
64.522987	2144.651024	20.224960
64.608007	2140.303391	20.229978
64.812137	2135.224904	20.234995
64.574850	2142.794318	20.240013
64.891924	2141.403426	20.245031
64.816237	2131.874224	20.250048
64.637522	2140.565406	20.255066
65.098344	2138.044865	20.260083
65.091809	2154.234655	20.265101
65.032273	2159.628350	20.270119
65.211609	2161.340483	20.275136
65.087535	2164.801602	20.280154
65.452202	2162.704629	20.285171
65.176384	2169.559687	20.290189
65.612310	2159.213422	20.295207
65.349842	2161.845522	20.300224
65.378137	2168.350034	20.305242
65.626643	2173.595502	20.310259
66.110631	2185.224340	20.315277
65.847069	2187.049580	20.320295
65.799892	2188.491068	20.325312
65.772697	2192.894809	20.330330
66.175538	2189.590624	20.335347
66.073004	2198.578822	20.340365
66.228643	2189.415427	20.345383
66.601448	2186.072770	20.350400
65.977015	2196.681973	20.355418
66.295368	2184.739572	20.360435
66.198317	2189.113549	20.365453
66.179437	2182.149760	20.370471
66.585378	2188.923640	20.375488
66.402510	2198.981037	20.380506
66.557152	2190.098613	20.385523
66.813763	2217.537994	20.390541
66.691213	2223.611936	20.395559
67.074132	2217.258165	20.400576
67.129616	2223.193594	20.405594
67.214067	2217.250036	20.410611
66.813913	2208.125705	20.415629
66.870576	2213.507183	20.420647
67.065634	2209.868004	20.425664
66.728758	2215.666991	20.430682
67.187740	2209.790352	20.435699
67.082750	2222.497167	20.440717
67.061050	2221.036796	20.445735
67.232519	2216.207333	20.450752
67.272016	2238.979142	20.455770
67.441752	2246.623716	20.460787
67.450304	2242.417248	20.465805
67.651658	2252.631297	20.470823
67.830759	2251.011475	20.475840
67.560011	2251.409417	20.480858
67.793927	2249.220800	20.485875
67.706756	2252.164770	20.490893
67.681388	2251.338188	20.495911
68.111919	2263.950988	20.500928
67.863937	2270.479938	20.505946
67.709933	2274.965280	20.510963
68.358076	2271.798157	20.515981
68.193769	2264.807963	20.520999
68.005013	2270.241184	20.526016
68.127592	2280.394661	20.531034
68.782703	2296.219522	20.536051
68.415544	2306.037365	20.541069
68.648315	2301.892662	20.546087
69.053189	2309.064785	20.551104
68.893576	2302.349134	20.556122
68.962520	2296.510274	20.561139
69.293421	2309.887053	20.566157
69.274811	2302.513347	20.571175
69.377001	2294.316483	20.576192
69.276604	2301.293081	20.581210
69.416708	2293.513359	20.586227
69.135030	2300.617976	20.591245
69.439721	2297.075349	20.596263
69.529114	2299.651364	20.601280
69.655875	2292.390562	20.606298
69.810455	2299.612034	20.611315
69.519585	2300.944513	20.616333
69.881737	2294.058350	20.621351
69.783120	2290.949738	20.626368
69.770930	2296.010283	20.631386
69.918214	2293.356439	20.636403
69.906240	2293.164860	20.641421
69.509763	2295.692499	20.646439
69.729762	2297.359621	20.651456
69.660440	2296.649382	20.656474
70.187271	2308.635681	20.661491
70.123573	2315.408212	20.666509
69.959903	2314.837300	20.671527
70.259852	2316.020504	20.676544
70.129630	2322.632955	20.681562
70.289909	2311.371680	20.686579
70.188769	2314.549149	20.691597
70.316110	2328.571164	20.696615
70.745035	2338.705721	20.701632
70.516487	2346.560954	20.706650
70.670756	2353.024222	20.711667
70.709899	2360.330992	20.716685
70.658515	2353.368371	20.721703
70.812047	2342.482569	20.726720
70.723414	2362.411790	20.731738
71.037133	2374.742834	20.736755
70.944160	2381.549168	20.741773
71.033950	2399.529899	20.746791
71.335403	2393.512336	20.751808
70.930420	2387.992861	20.756826
71.166008	2386.972844	20.761843
71.412213	2406.801535	20.766861
71.661166	2415.081724	20.771879
71.789217	2415.718917	20.776896
71.763492	2421.587143	20.781914
72.229300	2417.705728	20.786931
72.239678	2413.194505	20.791949
72.016758	2426.060316	20.796967
72.163268	2414.735083	20.801984
71.852338	2413.213051	20.807002
72.265648	2413.774077	20.812019
72.375362	2421.265488	20.817037
71.944966	2407.460071	20.822055
72.613048	2398.736345	20.827072
72.411115	2411.812752	20.832090
72.538579	2408.416351	20.837107
72.505193	2406.194036	20.842125
72.582953	2423.936017	20.847143
72.811010	2419.556839	20.852160
72.957758	2425.108094	20.857178
73.229308	2421.315864	20.862195
73.165031	2424.038329	20.867213
73.361878	2430.015015	20.872231
73.608770	2421.724210	20.877248
73.276176	2406.236390	20.882266
73.192037	2404.579869	20.887283
73.310317	2402.788024	20.892301
73.339928	2409.764394	20.897319
73.454322	2407.704938	20.902336
73.164793	2411.916958	20.907354
73.480992	2410.650465	20.912371
73.462747	2408.880391	20.917389
73.506279	2424.311292	20.922407
73.593631	2416.440018	20.927424
73.471922	2423.692237	20.932442
73.427227	2432.449533	20.937459
73.695744	2441.871124	20.942477
73.388671	2441.887068	20.947495
73.769309	2447.635442	20.952512
73.831681	2452.988567	20.957530
73.792649	2453.165498	20.962547
73.931079	2473.783124	20.967565
74.155447	2477.460130	20.972583
74.704818	2476.253989	20.977600
74.496778	2475.186718	20.982618
74.121067	2488.090321	20.987635
74.367970	2495.789582	20.992653
74.595108	2501.427159	20.997671
74.914660	2496.316771	21.002688
75.056234	2508.479515	21.007706
75.090768	2505.536050	21.012723
75.251523	2507.104879	21.017741
75.078108	2510.208961	21.022759
75.487749	2506.494588	21.027776
75.256889	2505.527707	21.032794
75.179047	2509.103458	21.037811
75.495301	2502.836496	21.042829
75.184686	2509.442400	21.047847
75.140266	2503.007197	21.052864
74.961571	2515.342942	21.057882
75.279288	2529.020149	21.062899
75.549044	2537.802092	21.067917
75.472057	2551.161543	21.072935
75.710370	2534.945395	21.077952
75.900960	2539.327097	21.082970
76.053073	2553.992757	21.087987
76.244925	2560.155932	21.093005
76.188284	2564.850807	21.098023
76.347043	2564.521087	21.103040
76.499531	2565.074942	21.108058
76.843639	2551.083741	21.113075
76.882208	2558.031222	21.118093
76.675673	2562.065649	21.123111
77.039655	2540.124184	21.128128
77.038558	2553.000357	21.133146
76.828124	2521.081149	21.138163
76.931199	2522.633220	21.143181
76.974049	2537.868485	21.148199
77.147700	2538.370195	21.153216
77.115121	2557.084087	21.158234
77.285885	2552.109891	21.163251
77.239902	2550.505477	21.168269
77.012094	2552.296741	21.173287
77.199499	2552.889865	21.178304
76.997300	2549.122804	21.183322
77.243497	2548.050743	21.188339
77.332179	2549.247992	21.193357
77.560363	2574.238361	21.198375
77.563184	2575.021388	21.203392
77.461715	2583.613200	21.208410
77.367395	2583.835920	21.213427
77.786151	2579.865214	21.218445
77.408516	2590.744480	21.223463
78.020224	2600.992451	21.228480
78.038694	2610.075663	21.233498
77.968448	2613.219952	21.238515
78.315516	2611.987065	21.243533
78.484928	2610.294808	21.248551
78.663795	2609.050985	21.253568
78.697534	2618.393709	21.258586
78.406372	2599.208295	21.263603
78.819427	2600.186275	21.268621
78.658902	2605.914816	21.273639
78.498841	2609.709794	21.278656
78.914221	2614.552026	21.283674
78.705774	2610.398933	21.288691
79.257771	2615.091162	21.293709
79.063331	2626.649979	21.298727
79.472618	2637.034087	21.303744
79.264531	2627.409255	21.308762
79.174948	2637.688847	21.313779
79.596917	2631.320019	21.318797
79.392860	2630.363801	21.323815
79.827211	2634.784537	21.328832
79.970446	2625.971317	21.333850
79.763660	2634.072588	21.338867
79.874502	2616.472573	21.343885
80.091292	2621.797204	21.348903
80.020400	2617.299663	21.353920
79.674588	2635.357227	21.358938
79.723680	2626.363153	21.363955
80.195443	2630.738591	21.368973
80.130469	2649.287072	21.373991
80.225504	2649.479597	21.379008
80.356166	2652.329915	21.384026
80.293744	2658.392875	21.389043
80.368417	2652.501831	21.394061
80.445918	2659.562717	21.399079
80.343180	2652.837048	21.404096
80.599993	2686.169015	21.409114
80.593657	2673.739949	21.414131
80.798327	2672.805866	21.419149
80.874107	2677.549669	21.424167
80.835403	2671.068643	21.429184
81.573869	2678.893350	21.434202
81.156964	2685.232313	21.439219
81.451195	2700.043006	21.444237
81.116933	2711.676889	21.449255
81.559871	2708.020873	21.454272
81.428853	2714.591937	21.459290
81.393705	2710.112267	21.464307
81.663458	2700.448160	21.469325
81.351867	2722.055879	21.474343
81.523952	2713.857074	21.479360
81.931426	2724.538088	21.484378
81.814982	2737.344716	21.489395
82.060739	2730.797064	21.494413
81.857383	2732.465670	21.499431
82.013510	2731.209731	21.504448
82.335989	2737.697478	21.509466
82.295607	2738.684844	21.514483
82.225090	2732.385853	21.519501
82.469104	2756.798993	21.524519
82.466436	2765.899832	21.529536
82.720303	2766.766337	21.534554
82.553686	2765.711317	21.539571
82.697083	2772.662637	21.544589
82.643695	2773.656012	21.549607
82.659550	2770.695807	21.554624
82.737464	2783.290559	21.559642
82.977296	2793.109475	21.564659
83.796208	2782.490104	21.569677
83.980704	2787.505296	21.574695
84.186715	2787.009140	21.579712
84.089282	2779.628884	21.584730
84.137255	2776.024820	21.589747
84.162389	2762.700992	21.594765
84.030389	2747.362531	21.599783
84.000342	2742.539858	21.604800
84.098683	2746.347157	21.609818
84.286628	2746.137065	21.614835
84.157692	2740.930560	21.619853
84.109694	2744.836708	21.624871
84.047892	2746.264064	21.629888
84.679899	2757.815484	21.634906
84.412965	2762.231667	21.639923
84.501043	2774.203362	21.644941
84.377764	2777.663711	21.649959
84.597596	2773.464303	21.654976
84.725047	2777.492728	21.659994
84.851760	2785.101969	21.665011
85.001289	2771.685141	21.670029
84.765942	2776.259908	21.675047
84.973398	2768.651690	21.680064
85.072794	2773.324896	21.685082
85.304551	2801.541801	21.690099
85.308694	2795.397641	21.695117
85.363036	2806.769830	21.700135
85.320396	2808.713307	21.705152
85.731170	2798.405218	21.710170
85.954649	2793.610538	21.715187
86.141569	2785.105692	21.720205
86.237453	2788.944858	21.725223
86.179117	2793.737617	21.730240
86.561974	2786.331114	21.735258
86.195957	2782.031614	21.740275
86.178963	2794.368553	21.745293
86.167673	2785.750575	21.750311
86.158300	2792.697946	21.755328
86.085175	2791.579246	21.760346
85.925734	2796.883699	21.765363
86.134428	2776.320419	21.770381
86.304536	2783.438181	21.775399
86.271961	2799.682395	21.780416
86.828283	2808.952137	21.785434
86.156272	2801.623373	21.790451
86.430454	2798.808399	21.795469
86.516302	2817.853787	21.800487
86.838326	2825.047246	21.805504
86.965963	2841.109420	21.810522
86.782149	2843.939912	21.815539
87.199853	2842.839696	21.820557
87.358801	2844.705408	21.825575
86.875864	2864.875178	21.830592
87.269024	2866.487225	21.835610
87.536830	2863.486038	21.840627
87.350674	2873.556220	21.845645
87.745419	2869.074027	21.850663
87.603943	2896.407467	21.855680
87.863636	2903.237256	21.860698
88.133760	2897.957622	21.865715
88.706208	2903.737738	21.870733
88.388226	2896.833888	21.875751
88.700708	2890.173265	21.880768
89.038701	2895.342583	21.885786
88.726071	2892.641615	21.890803
88.899381	2889.989808	21.895821
88.918264	2887.368132	21.900839
89.209691	2897.834939	21.905856
89.238164	2883.147245	21.910874
88.787813	2883.484950	21.915891
88.941521	2887.137931	21.920909
88.946436	2885.980821	21.925927
89.043332	2893.214146	21.930944
89.348878	2884.750897	21.935962
89.036490	2884.145464	21.940979
89.347977	2896.232667	21.945997
89.415608	2904.711174	21.951015
89.393996	2914.194281	21.956032
89.841557	2912.195690	21.961050
89.493129	2916.940351	21.966067
89.704453	2913.333805	21.971085
89.714394	2911.947769	21.976103
89.876986	2937.849123	21.981120
90.341477	2940.984516	21.986138
90.117431	2948.125092	21.991155
90.742088	2940.074251	21.996173
90.464920	2945.201659	22.001191
90.510578	2941.415426	22.006208
90.520042	2939.522088	22.011226
90.493415	2940.596163	22.016243
90.267228	2937.436171	22.021261
90.866759	2948.985058	22.026279
90.659627	2968.668905	22.031296
91.367223	2965.476430	22.036314
91.101357	2962.098569	22.041331
91.266248	2967.281356	22.046349
91.116643	2963.829893	22.051367
90.837630	2971.752502	22.056384
91.143017	2963.537022	22.061402
91.414430	2976.013770	22.066419
91.469982	2985.557775	22.071437
91.640447	2990.915101	22.076455
91.626890	2988.193958	22.081472
92.155117	3001.894682	22.086490
92.044356	2996.228940	22.091507
92.106339	2983.715559	22.096525
92.039619	2990.126246	22.101543
91.871555	2994.939714	22.106560
92.306070	2975.779682	22.111578
92.146232	3003.839164	22.116595
92.397703	3002.207722	22.121613
92.989142	3003.868405	22.126631
92.908104	3008.576750	22.131648
93.214713	3003.442294	22.136666
92.967970	3004.329643	22.141683
93.352457	2994.481856	22.146701
93.701998	3001.874754	22.151719
93.520077	2995.667356	22.156736
93.532749	2979.061917	22.161754
93.491286	2974.292905	22.166771
93.464977	2977.346883	22.171789
93.567181	2982.700931	22.176807
93.573284	2987.131067	22.181824
93.857491	2987.619885	22.186842
94.014260	2994.031909	22.191859
94.218292	2991.631627	22.196877
94.245511	2988.696311	22.201895
94.162361	3000.297459	22.206912
94.115863	2990.844064	22.211930
94.120562	2980.162446	22.216947
93.890124	2990.821877	22.221965
93.938464	2990.361083	22.226983
93.970819	2993.187812	22.232000
94.262161	2997.643265	22.237018
94.387044	3017.890170	22.242035
94.715020	3016.096281	22.247053
94.809461	3014.742386	22.252071
94.595437	3022.694778	22.257088
95.001758	3042.571174	22.262106
95.032865	3038.669240	22.267123
95.022530	3047.072946	22.272141
95.240510	3050.633124	22.277159
94.982021	3049.610824	22.282176
95.301714	3049.285326	22.287194
95.321453	3063.840452	22.292211
95.425562	3072.466634	22.297229
95.645208	3084.585158	22.302247
95.508351	3092.595293	22.307264
95.630029	3072.139084	22.312282
95.724392	3084.449858	22.317299
96.190922	3110.385650	22.322317
96.162544	3100.565081	22.327335
96.161209	3115.035515	22.332352
95.975356	3104.926972	22.337370
95.810238	3120.046543	22.342387
96.249274	3127.302519	22.347405
96.380289	3140.725310	22.352423
96.341999	3153.312165	22.357440
96.703910	3144.437807	22.362458
96.789046	3142.408087	22.367475
96.844013	3142.990890	22.372493
97.420172	3157.982861	22.377511
97.173295	3166.450312	22.382528
97.838313	3169.948676	22.387546
97.654951	3167.145233	22.392563
97.482317	3172.717022	22.397581
98.132947	3157.380772	22.402599
98.143334	3157.783463	22.407616
97.923144	3161.524452	22.412634
98.015056	3161.543636	22.417651
98.376900	3145.388928	22.422669
98.704996	3148.353391	22.427687
98.341386	3128.042923	22.432704
98.360919	3110.893459	22.437722
98.378991	3132.899958	22.442739
98.376344	3143.200654	22.447757
98.518645	3143.219670	22.452775
98.371627	3143.225034	22.457792
98.623600	3147.007154	22.462810
98.658894	3156.464037	22.467827
98.637345	3146.149125	22.472845
98.746125	3163.709278	22.477863
98.706360	3172.374193	22.482880
98.873011	3178.599075	22.487898
99.084945	3190.097469	22.492915
98.962772	3189.397973	22.497933
99.642751	3197.332196	22.502951
99.227624	3214.437098	22.507968
99.099130	3206.077487	22.512986
99.283773	3213.363843	22.518003
99.740358	3226.065366	22.523021
99.866763	3240.320467	22.528039
99.864998	3235.738555	22.533056
99.960605	3243.706199	22.538074
100.225976	3237.045066	22.543091
100.720658	3252.367145	22.548109
101.133050	3238.446216	22.553127
100.932245	3233.743433	22.558144
100.986241	3222.255335	22.563162
100.943357	3224.560761	22.568179
100.812134	3219.101149	22.573197
101.199618	3214.597199	22.578215
101.260187	3219.010067	22.583232
101.472789	3218.419238	22.588250
101.701517	3213.098107	22.593267
101.602113	3218.534734	22.598285
101.647810	3209.770543	22.603303
101.687390	3215.197594	22.608320
101.682598	3207.814148	22.613338
101.303567	3212.087075	22.618355
101.555617	3221.919281	22.623373
102.187335	3229.109186	22.628391
102.042300	3243.343854	22.633408
102.117859	3241.053695	22.638426
102.497606	3243.352306	22.643443
102.056422	3244.510599	22.648461
102.486388	3238.449390	22.653479
102.309796	3246.313336	22.658496
102.342939	3233.171878	22.663514
102.754574	3245.034942	22.668531
102.615330	3260.345621	22.673549
102.795477	3268.294291	22.678567
102.525692	3275.745177	22.683584
102.873697	3267.031079	22.688602
102.979138	3274.880748	22.693619
102.691119	3297.641924	22.698637
103.003372	3288.916208	22.703655
103.331744	3300.099557	22.708672
102.968173	3310.495679	22.713690
103.478532	3307.007340	22.718707
103.528469	3334.918368	22.723725
104.117355	3318.357543	22.728743
103.923852	3330.906368	22.733760
104.239120	3323.772330	22.738778
104.347482	3329.661232	22.743795
104.265081	3322.877731	22.748813
104.654009	3312.507478	22.753831
104.939668	3332.999004	22.758848
105.000511	3325.915760	22.763866
104.867324	3318.499239	22.768883
104.579121	3318.136936	22.773901
104.949177	3330.204149	22.778919
104.932422	3348.334408	22.783936
105.220851	3342.463282	22.788954
105.267565	3344.473607	22.793971
105.089435	3353.430513	22.798989
105.487643	3337.624576	22.804007
105.242640	3349.387111	22.809024
104.958277	3350.594351	22.814042
105.372850	3372.795223	22.819059
105.432061	3373.111470	22.824077
105.808227	3372.231025	22.829095
105.864021	3377.723203	22.834112
105.912638	3396.553445	22.839130
106.072059	3398.970599	22.844147
106.119553	3404.724492	22.849165
106.477736	3401.538085	22.854183
106.362633	3397.506759	22.859200
106.445525	3414.895917	22.864218
106.613098	3419.738603	22.869235
106.788189	3439.051406	22.874253
106.785351	3427.475450	22.879271
106.963559	3435.908314	22.884288
106.580519	3428.992557	22.889306
106.688778	3436.271538	22.894323
107.229568	3460.584256	22.899341
107.659700	3453.066046	22.904359
107.553403	3457.856441	22.909376
107.766411	3457.898010	22.914394
107.994577	3458.369823	22.919411
107.984772	3459.812556	22.924429
108.058502	3449.215562	22.929447
108.003889	3461.900470	22.934464
108.119245	3463.353926	22.939482
108.390822	3448.544304	22.944499
108.293008	3478.657416	22.949517
108.489727	3479.981475	22.954535
108.603154	3479.432409	22.959552
108.680384	3483.235400	22.964570
108.760848	3484.603170	22.969587
108.847490	3483.997015	22.974605
108.750773	3477.965410	22.979623
108.673062	3497.323319	22.984640
108.894643	3499.156317	22.989658
109.445607	3511.763589	22.994675
109.194846	3507.609117	22.999693
109.396564	3503.825389	23.004711
109.510888	3520.389961	23.009728
109.117122	3533.408273	23.014746
109.670446	3547.368256	23.019763
109.606500	3536.015930	23.024781
109.849039	3546.735651	23.029799
109.952996	3560.537593	23.034816
109.839270	3566.728681	23.039834
110.112876	3568.554966	23.044851
109.971744	3575.631490	23.049869
110.731528	3594.507498	23.054887
110.730685	3602.073783	23.059904
110.489739	3603.981331	23.064922
110.858414	3609.546427	23.069939
110.888752	3604.353549	23.074957
111.277962	3602.205270	23.079975
111.191379	3626.381510	23.084992
111.438468	3624.054502	23.090010
111.630194	3615.710465	23.095027
111.716375	3629.354040	23.100045
111.545338	3617.699340	23.105063
111.439820	3622.536865	23.110080
111.398008	3620.751521	23.115098
112.051615	3640.414664	23.120115
111.897123	3656.647012	23.125133
112.268371	3653.394748	23.130151
112.466485	3647.688943	23.135168
112.057254	3660.727139	23.140186
112.555947	3645.409893	23.145203
112.123766	3666.127263	23.150221
112.658031	3670.806152	23.155239
112.645194	3682.999215	23.160256
112.634559	3677.078096	23.165274
112.774630	3692.814329	23.170291
112.952823	3695.125485	23.175309
112.995462	3700.851162	23.180327
112.987994	3718.456475	23.185344
112.882550	3721.948026	23.190362
113.540919	3718.399020	23.195379
113.501544	3741.245529	23.200397
113.442759	3747.932189	23.205415
113.718298	3738.220856	23.210432
113.754329	3747.800724	23.215450
114.179280	3760.479438	23.220467
113.977977	3772.509891	23.225485
114.322874	3772.244870	23.230503
114.779946	3769.509116	23.235520
114.676589	3771.069063	23.240538
115.284183	3764.413702	23.245555
115.383327	3763.346912	23.250573
115.486854	3761.795620	23.255591
115.755675	3757.341896	23.260608
115.411532	3764.114183	23.265626
115.596366	3755.137108	23.270643
115.798408	3760.728045	23.275661
115.884758	3759.341546	23.280679
115.935078	3750.967272	23.285696
115.621628	3760.495885	23.290714
115.760476	3754.690141	23.295731
115.489245	3754.439973	23.300749
115.666582	3750.664789	23.305767
115.838503	3776.031988	23.310784
115.849272	3780.784942	23.315802
116.286909	3787.798392	23.320819
116.145077	3788.536894	23.325837
116.523425	3805.333453	23.330855
116.671572	3821.155071	23.335872
116.649369	3817.982026	23.340890
116.759269	3822.787629	23.345907
116.763735	3824.774862	23.350925
117.078059	3830.200814	23.355943
117.341482	3847.478312	23.360960
117.242470	3842.452297	23.365978
117.305833	3846.337048	23.370995
117.056091	3857.859233	23.376013
117.316252	3868.994894	23.381031
117.659195	3874.166135	23.386048
117.278656	3884.349815	23.391066
117.750127	3902.918187	23.396083
117.760537	3914.373762	23.401101
118.080188	3909.269170	23.406119
118.521687	3925.222702	23.411136
118.604730	3925.154408	23.416154
119.026990	3939.470792	23.421171
118.940650	3942.337083	23.426189
119.224776	3929.483032	23.431207
119.261084	3943.573819	23.436224
118.951480	3936.178821	23.441242
119.623520	3936.593252	23.446259
119.095779	3933.336371	23.451277
119.393910	3933.748272	23.456295
119.610320	3927.432124	23.461312
119.507106	3932.463693	23.466330
119.759249	3931.124692	23.471347
119.678136	3951.932809	23.476365
119.942547	3956.636725	23.481383
120.543344	3956.622761	23.486400
120.054213	3960.134638	23.491418
120.484819	3960.582058	23.496435
120.451621	3953.128819	23.501453
120.684218	3967.859373	23.506471
120.807981	3978.761194	23.511488
120.753823	3983.359362	23.516506
120.842393	3986.003463	23.521523
120.866640	3981.420317	23.526541
120.915799	3985.891877	23.531559
121.299717	3997.965300	23.536576
120.962468	4018.901673	23.541594
121.339098	4023.542090	23.546611
121.343763	4035.082064	23.551629
121.462414	4036.486278	23.556647
121.684967	4054.122185	23.561664
121.617390	4053.187374	23.566682
121.908528	4054.351682	23.571699
122.032148	4061.776423	23.576717
122.043373	4069.533764	23.581735
122.485237	4065.248243	23.586752
122.537848	4074.345014	23.591770
122.637048	4067.042105	23.596787
122.979790	4075.003052	23.601805
122.641523	4090.085143	23.606823
123.338582	4092.034359	23.611840
123.132009	4098.480414	23.616858
123.519419	4094.188621	23.621875
123.279671	4105.330220	23.626893
123.826425	4114.555127	23.631911
123.973241	4121.322458	23.636928
124.001472	4127.946642	23.641946
124.041904	4128.400425	23.646963
124.443922	4117.989761	23.651981
124.170253	4130.028109	23.656999
124.540019	4121.681361	23.662016
124.603066	4116.199092	23.667034
125.190856	4114.985137	23.672051
124.865866	4105.016876	23.677069
124.716455	4120.918515	23.682087
125.009253	4106.029328	23.687104
124.887975	4127.340500	23.692122
125.114067	4133.463483	23.697139
125.526395	4132.070603	23.702157
125.745536	4145.032636	23.707175
125.603755	4151.836556	23.712192
125.581992	4154.151347	23.717210
125.409884	4150.249266	23.722227
126.000557	4142.210282	23.727245
125.728048	4135.243522	23.732263
126.193115	4140.159380	23.737280
126.218716	4160.621940	23.742298
126.078130	4176.700024	23.747315
126.719357	4163.504049	23.752333
126.423647	4175.676540	23.757351
126.839751	4167.335752	23.762368
126.838217	4161.170685	23.767386
127.277635	4161.847210	23.772403
127.333633	4164.582286	23.777421
127.109814	4184.833692	23.782439
127.680530	4178.715836	23.787456
127.655842	4190.389630	23.792474
127.613186	4187.410147	23.797491
127.947147	4179.135945	23.802509
127.773580	4183.599022	23.807527
127.782633	4179.867082	23.812544
127.770008	4202.823326	23.817562
128.053417	4202.170823	23.822579
128.181638	4211.254050	23.827597
128.301017	4212.796624	23.832615
128.884120	4199.004129	23.837632
128.514646	4214.543673	23.842650
128.626500	4227.489057	23.847667
129.256388	4236.419150	23.852685
129.290648	4236.372793	23.857703
129.485459	4230.783723	23.862720
129.344877	4246.850082	23.867738
129.579367	4231.638866	23.872755
129.447543	4235.667339	23.877773
129.549739	4250.930324	23.882791
129.644583	4262.552075	23.887808
129.733487	4262.235822	23.892826
129.679474	4273.999321	23.897843
130.203479	4279.550924	23.902861
130.142174	4299.900875	23.907879
130.135960	4290.973603	23.912896
130.264255	4311.033728	23.917914
130.709595	4310.145353	23.922931
130.835754	4311.272264	23.927949
130.874793	4326.156766	23.932967
131.087663	4315.378837	23.937984
130.999700	4320.692106	23.943002
131.194668	4344.428137	23.948019
131.678326	4345.841841	23.953037
131.599268	4351.210344	23.958055
131.750065	4335.947855	23.963072
131.958400	4364.066873	23.968090
132.036529	4346.822448	23.973107
132.233098	4349.660232	23.978125
132.033777	4351.256781	23.983143
132.320801	4367.310951	23.988160
132.650479	4371.701714	23.993178
132.782223	4374.224143	23.998195
132.977658	4380.012260	24.003213
132.846807	4366.549000	24.008231
132.999104	4372.417944	24.013248
133.052939	4379.665949	24.018266
133.340676	4386.020729	24.023283
133.681643	4393.018418	24.028301
133.539907	4402.204594	24.033319
133.768926	4398.989797	24.038336
134.039318	4397.139633	24.043354
133.761249	4396.106980	24.048371
133.889667	4391.352118	24.053389
133.944287	4388.789773	24.058407
134.198799	4410.999648	24.063424
134.083122	4413.958032	24.068442
134.440165	4424.931556	24.073459
134.716237	4413.244272	24.078477
134.887935	4426.673556	24.083495
135.151867	4440.772583	24.088512
135.368730	4441.198246	24.093530
134.889260	4453.393969	24.098547
135.271352	4451.052391	24.103565
135.201352	4450.083325	24.108583
135.599820	4468.505141	24.113600
135.681218	4469.713939	24.118618
135.569005	4479.738810	24.123635
135.633389	4474.701474	24.128653
135.874442	4497.600424	24.133671
136.129244	4500.901768	24.138688
136.408773	4501.226969	24.143706
136.381871	4510.094379	24.148723
136.659341	4520.930400	24.153741
136.809712	4529.724715	24.158759
137.239203	4523.320844	24.163776
136.826379	4536.762392	24.168794
136.596293	4539.387381	24.173811
137.239982	4549.637148	24.178829
137.268013	4571.349195	24.183847
137.343472	4565.545373	24.188864
137.590441	4584.413956	24.193882
137.663226	4593.746206	24.198899
137.893774	4591.921254	24.203917
138.261953	4602.049774	24.208935
138.409181	4594.668930	24.213952
138.146850	4615.352679	24.218970
138.380011	4626.813417	24.223987
138.535780	4622.504909	24.229005
138.368074	4619.298247	24.234023
138.714850	4648.309117	24.239040
138.715501	4649.919444	24.244058
138.694038	4657.936417	24.249075
139.019236	4664.212180	24.254093
139.267913	4679.265802	24.259111
139.537011	4679.392843	24.264128
139.685951	4685.433166	24.269146
139.502972	4695.510376	24.274163
140.021920	4696.466125	24.279181
140.026483	4718.015343	24.284199
140.040648	4717.626817	24.289216
140.276618	4714.982792	24.294234
140.231630	4720.457712	24.299251
140.400757	4736.562551	24.304269
140.612022	4749.179427	24.309287
141.062375	4749.371192	24.314304
140.981728	4752.211557	24.319322
140.768410	4776.228942	24.324339
141.399005	4768.163592	24.329357
141.543460	4779.770762	24.334375
141.746909	4769.741396	24.339392
141.733173	4793.151105	24.344410
141.980549	4799.097107	24.349427
142.135608	4805.725763	24.354445
141.727131	4806.398258	24.359463
142.328920	4803.798954	24.364480
142.494134	4820.909949	24.369498
142.681214	4836.916054	24.374515
142.605147	4832.816743	24.379533
142.683195	4835.411538	24.384551
142.983038	4845.629795	24.389568
143.127772	4866.671469	24.394586
142.982908	4874.422650	24.399603
143.220873	4862.604984	24.404621
143.633087	4889.801920	24.409639
144.025649	4895.039569	24.414656
144.070006	4890.787298	24.419674
143.938316	4910.604892	24.424691
144.329859	4893.981730	24.429709
144.320803	4906.604760	24.434727
144.415778	4914.349192	24.439744
144.416421	4929.522075	24.444762
144.705128	4933.213840	24.449779
144.545164	4935.509090	24.454797
144.223327	4950.253499	24.459815
144.891006	4955.007521	24.464832
145.028387	4973.643893	24.469850
145.022780	4990.894823	24.474867
145.603567	4985.649102	24.479885
145.313735	5002.400938	24.484903
145.684343	5012.578132	24.489920
145.735613	5023.720440	24.494938
146.120205	5017.638214	24.499955
146.329947	5019.028001	24.504973
146.296906	5033.499081	24.509991
146.896858	5044.801750	24.515008
147.483623	5040.364614	24.520026
146.958972	5039.647372	24.525043
147.249941	5043.615737	24.530061
147.076242	5039.616902	24.535079
147.347764	5037.326694	24.540096
147.528638	5029.488680	24.545114
147.435553	5030.227336	24.550131
147.640604	5048.581588	24.555149
147.750976	5055.176571	24.560167
147.910131	5066.695082	24.565184
148.365636	5056.655233	24.570202
147.934044	5071.380285	24.575219
148.214126	5079.528001	24.580237
148.596959	5095.832037	24.585255
148.711539	5094.819339	24.590272
148.698614	5091.130010	24.595290
148.791277	5113.470598	24.600307
149.216651	5114.594713	24.605325
149.072003	5139.256310	24.610343
149.207965	5124.325021	24.615360
149.824865	5134.607008	24.620378
149.696642	5160.250242	24.625395
149.869689	5159.347803	24.630413
149.883377	5164.610551	24.635431
149.995807	5165.624853	24.640448
150.217638	5165.952191	24.645466
150.265358	5188.637573	24.650483
150.505382	5184.805615	24.655501
150.423050	5186.495318	24.660519
150.751939	5216.789413	24.665536
151.227008	5220.238329	24.670554
151.059608	5220.238283	24.675571
151.156119	5233.054822	24.680589
151.757231	5235.242940	24.685607
151.812765	5239.928648	24.690624
151.996927	5250.524389	24.695642
151.591669	5249.969053	24.700659
152.041167	5261.368258	24.705677
151.744585	5277.241103	24.710695
152.058301	5284.948496	24.715712
152.378803	5290.998693	24.720730
152.472379	5307.033591	24.725747
152.647597	5311.469721	24.730765
152.877205	5317.267710	24.735783
153.101944	5336.603413	24.740800
153.317955	5350.684990	24.745818
153.047900	5346.070454	24.750835
153.198386	5355.951757	24.755853
153.227461	5374.859238	24.760871
153.515455	5378.428495	24.765888
153.912052	5377.597402	24.770906
154.181081	5402.512909	24.775923
154.472796	5409.070484	24.780941
154.903829	5406.576982	24.785959
154.956650	5400.593914	24.790976
155.426521	5389.765579	24.795994
155.419585	5391.784738	24.801011
155.410467	5388.484961	24.806029
155.667522	5385.966486	24.811047
155.787181	5380.962514	24.816064
156.238471	5376.117311	24.821082
155.912070	5387.879491	24.826099
156.411072	5374.805043	24.831117
156.397272	5367.511642	24.836135
156.291050	5375.826537	24.841152
156.380733	5373.124684	24.846170
156.764575	5383.008926	24.851187
156.811586	5385.829846	24.856205
156.708472	5384.506448	24.861223
156.859315	5396.317643	24.866240
157.062008	5387.470483	24.871258
157.127418	5401.835750	24.876275
157.635302	5408.571287	24.881293
157.905147	5419.943399	24.886311
157.484369	5426.860831	24.891328
157.673414	5425.140741	24.896346
157.760809	5433.299705	24.901363
158.209962	5444.021706	24.906381
158.184516	5453.142000	24.911399
157.855642	5460.019619	24.916416
158.441099	5466.261316	24.921434
158.542508	5482.754627	24.926451
158.816091	5488.465423	24.931469
158.774785	5493.280732	24.936487
159.174431	5511.260719	24.941504
159.320996	5501.222621	24.946522
159.626003	5502.443062	24.951539
159.728267	5520.104625	24.956557
160.204566	5526.665870	24.961575
160.167029	5531.930622	24.966592
160.485588	5528.635220	24.971610
160.297604	5532.702894	24.976627
160.651912	5535.608601	24.981645
160.891832	5541.819662	24.986663
160.929147	5555.637247	24.991680
161.171623	5559.207512	24.996698
161.133952	5562.210335	25.001715
161.592902	5558.107349	25.006733
161.472436	5552.270649	25.011751
161.438769	5565.221526	25.016768
161.619695	5590.596709	25.021786
161.639000	5593.510990	25.026803
161.746406	5598.456044	25.031821
162.066281	5617.813928	25.036839
162.236222	5629.033759	25.041856
162.683682	5614.009043	25.046874
162.599634	5635.535174	25.051891
162.651581	5650.592042	25.056909
163.025397	5653.518267	25.061927
162.879435	5661.669714	25.066944
163.120309	5667.673755	25.071962
163.252005	5687.562906	25.076979
163.401316	5680.762618	25.081997
163.632409	5691.731994	25.087015
163.417512	5702.073037	25.092032
163.685810	5717.038833	25.097050
163.909285	5734.622320	25.102067
164.273281	5746.273141	25.107085
164.458743	5754.924907	25.112103
164.324467	5757.688254	25.117120
164.496340	5767.217880	25.122138
164.677182	5777.943562	25.127155
164.939028	5794.063885	25.132173
165.241975	5799.656825	25.137191
164.992425	5820.610081	25.142208
165.635821	5820.428056	25.147226
165.626614	5835.742699	25.152243
165.586915	5857.833286	25.157261
166.195377	5853.912523	25.162279
165.932361	5873.089867	25.167296
166.320932	5874.619600	25.172314
166.438824	5874.772338	25.177331
166.673754	5897.184270	25.182349
167.236100	5905.238665	25.187367
167.018926	5907.931856	25.192384
167.398978	5907.589610	25.197402
167.732122	5929.040214	25.202419
167.787818	5928.564783	25.207437
168.308031	5933.932734	25.212455
168.258688	5936.136542	25.217472
168.578498	5922.351390	25.222490
168.893452	5919.620606	25.227507
168.481574	5931.481814	25.232525
168.752189	5938.024108	25.237543
168.626787	5947.048130	25.242560
169.102320	5958.516899	25.247578
169.402117	5962.735881	25.252595
169.133805	5964.055631	25.257613
169.560803	5976.371657	25.262631
169.727934	5978.312791	25.267648
169.800383	5973.398760	25.272666
170.001177	5989.634460	25.277683
170.451873	5989.458766	25.282701
170.530627	6000.866511	25.287719
170.713081	6010.393033	25.292736
170.841020	6013.810149	25.297754
171.302236	5998.931557	25.302771
171.127981	6009.279709	25.307789
171.617684	6028.861257	25.312807
171.495194	6042.093433	25.317824
171.582122	6033.725407	25.322842
171.946506	6032.501301	25.327859
171.496459	6041.806880	25.332877
172.009720	6061.427203	25.337895
172.085622	6072.228838	25.342912
172.121877	6067.946049	25.347930
172.080168	6077.062238	25.352947
172.180552	6103.749355	25.357965
172.656760	6100.660802	25.362983
172.544407	6109.623046	25.368000
172.571010	6126.124278	25.373018
172.847848	6136.803445	25.378035
173.174476	6154.595224	25.383053
173.652961	6159.151639	25.388071
173.441039	6169.889079	25.393088
173.884524	6180.658157	25.398106
174.187349	6186.466848	25.403123
174.314630	6192.117841	25.408141
174.415830	6196.627410	25.413159
174.477244	6215.829008	25.418176
174.586577	6222.800771	25.423194
174.991324	6230.663312	25.428211
175.159650	6249.284557	25.433229
175.235729	6257.357657	25.438247
175.441962	6257.972335	25.443264
175.793730	6251.237862	25.448282
176.000459	6281.905318	25.453299
176.043901	6287.679867	25.458317
176.177959	6279.368708	25.463335
176.289669	6286.438473	25.468352
176.723977	6311.124592	25.473370
176.960207	6315.578838	25.478387
177.360307	6308.314981	25.483405
177.328190	6310.289497	25.488423
177.105064	6324.440437	25.493440
176.949667	6332.079968	25.498458
177.227452	6335.178217	25.503475
177.008848	6362.192821	25.508493
177.623292	6376.395185	25.513511
177.763672	6391.776250	25.518528
178.163876	6404.072515	25.523546
178.225721	6406.608012	25.528563
178.246737	6435.272264	25.533581
178.481035	6431.568367	25.538599
178.664238	6458.460079	25.543616
178.650153	6468.844387	25.548634
178.969515	6481.650872	25.553651
179.061839	6509.470659	25.558669
179.724594	6504.704687	25.563687
180.023705	6528.483489	25.568704
180.359724	6530.843113	25.573722
180.468835	6522.140025	25.578739
180.667674	6530.273959	25.583757
180.768395	6521.962472	25.588775
180.980479	6553.154443	25.593792
181.387901	6552.065852	25.598810
181.513124	6554.685689	25.603827
181.228635	6563.227945	25.608845
181.488998	6560.701669	25.613863
181.675497	6569.051607	25.618880
181.812242	6577.625859	25.623898
182.257027	6588.932429	25.628915
181.900531	6594.445110	25.633933
182.029594	6599.872517	25.638951
182.269057	6616.692858	25.643968
182.701339	6619.838138	25.648986
182.967800	6614.236755	25.654003
182.670917	6647.714747	25.659021
183.296452	6650.080954	25.664039
183.479990	6655.529597	25.669056
183.354540	6667.071122	25.674074
183.623607	6683.398986	25.679092
183.310906	6687.857450	25.684109
183.980601	6700.948973	25.689127
183.905284	6711.692563	25.694144
184.081643	6721.859422	25.699162
184.757342	6734.484213	25.704180
184.605726	6757.328879	25.709197
184.981041	6761.776825	25.714215
185.379914	6779.819854	25.719232
185.344480	6773.262539	25.724250
185.453436	6777.122698	25.729268
185.833178	6804.440068	25.734285
186.118959	6812.703502	25.739303
186.327077	6816.650152	25.744320
186.104562	6818.763671	25.749338
186.791611	6825.298986	25.754356
186.590307	6843.329188	25.759373
186.809141	6850.755892	25.764391
187.011557	6859.647162	25.769408
186.772447	6863.490442	25.774426
187.149005	6873.458679	25.779444
187.467654	6889.840239	25.784461
188.034484	6896.166568	25.789479
187.642810	6914.291724	25.794496
188.037879	6938.111751	25.799514
188.849990	6935.081215	25.804532
188.507911	6937.207517	25.809549
188.802636	6955.340932	25.814567
189.323248	6959.000177	25.819584
189.222703	6961.139909	25.824602
189.538152	6966.359125	25.829620
189.409058	6985.877711	25.834637
189.645289	6996.526204	25.839655
189.647153	7001.228894	25.844672
189.715763	7012.005622	25.849690
189.899683	7023.050389	25.854708
189.980410	7037.649278	25.859725
190.251967	7055.155851	25.864743
190.157401	7066.718727	25.869760
190.648258	7090.824305	25.874778
190.686006	7095.375737	25.879796
190.341882	7125.237311	25.884813
191.114474	7132.816656	25.889831
191.270809	7141.297623	25.894848
191.415129	7165.519152	25.899866
192.193805	7173.747490	25.904884
192.071003	7197.284602	25.909901
192.180411	7205.397755	25.914919
192.821756	7203.595921	25.919936
193.172933	7208.916539	25.924954
193.741526	7210.143109	25.929972
194.162494	7210.770809	25.934989
194.236421	7197.476123	25.940007
194.822213	7198.528415	25.945024
194.333287	7186.527355	25.950042
194.741064	7171.406687	25.955060
194.560245	7173.170539	25.960077
194.545508	7187.006595	25.965095
195.184365	7193.921155	25.970112
195.345196	7194.364496	25.975130
195.138579	7190.852664	25.980148
195.184239	7195.742000	25.985165
195.445902	7191.286830	25.990183
195.592543	7209.535832	25.995200
195.618227	7222.509377	26.000218
196.041575	7222.005198	26.005236
196.029362	7233.248201	26.010253
195.898801	7252.516362	26.015271
196.593254	7256.536679	26.020288
196.247029	7266.146714	26.025306
196.600703	7280.019336	26.030324
196.876729	7299.403720	26.035341
196.839338	7309.361128	26.040359
197.251564	7313.390256	26.045376
197.278592	7340.349376	26.050394
197.748585	7345.581860	26.055412
197.701832	7351.239008	26.060429
198.292758	7367.950665	26.065447
198.585658	7365.470216	26.070464
198.652526	7372.732560	26.075482
198.748978	7388.161790	26.080500
198.771143	7407.701665	26.085517
198.947969	7409.796458	26.090535
199.596878	7426.161373	26.095552
199.507889	7435.426778	26.100570
199.924037	7440.920465	26.105588
200.226218	7460.120696	26.110605
199.860790	7471.699523	26.115623
200.004903	7475.301675	26.120640
200.089871	7489.646959	26.125658
200.339175	7500.235501	26.130676
200.510861	7526.142669	26.135693
200.863346	7531.977025	26.140711
201.074177	7557.729288	26.145728
201.264155	7575.639769	26.150746
201.596866	7583.093539	26.155764
201.923853	7600.455002	26.160781
202.177922	7608.758559	26.165799
202.443611	7608.083571	26.170816
202.394518	7633.304552	26.175834
202.896315	7633.510998	26.180852
202.757841	7632.717880	26.185869
203.135273	7642.663679	26.190887
203.348818	7658.146128	26.195904
203.434879	7672.072006	26.200922
204.023501	7655.342754	26.205940
204.806449	7646.120059	26.210957
204.870000	7652.251536	26.215975
205.293295	7644.477376	26.220992
204.992684	7633.004617	26.226010
205.635182	7638.176659	26.231028
205.558538	7642.287743	26.236045
205.976315	7649.039468	26.241063
206.235408	7646.046596	26.246080
205.914379	7650.717553	26.251098
206.569873	7646.064913	26.256116
206.574688	7645.064036	26.261133
206.301286	7655.213526	26.266151
206.627160	7647.164536	26.271168
206.465705	7652.839295	26.276186
206.804581	7663.296431	26.281204
206.892903	7676.264320	26.286221
206.945447	7681.821568	26.291239
207.180875	7699.898067	26.296256
207.196490	7715.808717	26.301274
207.295918	7723.041649	26.306292
207.537775	7744.935137	26.311309
207.145300	7761.724527	26.316327
207.873566	7784.850700	26.321344
208.355310	7798.217883	26.326362
208.587729	7809.766193	26.331380
208.441948	7834.823124	26.336397
208.611349	7849.420870	26.341415
209.217850	7864.793681	26.346432
209.113668	7897.070498	26.351450
209.699276	7903.431648	26.356468
210.038746	7916.699256	26.361485
209.791597	7927.730786	26.366503
210.277916	7936.641971	26.371520
210.658879	7949.898273	26.376538
210.971352	7965.868099	26.381556
211.093884	7983.700509	26.386573
211.272266	7980.999786	26.391591
211.786229	7997.332548	26.396608
211.847910	8014.929577	26.401626
211.917619	8020.364212	26.406644
212.455529	8023.833296	26.411661
211.962190	8038.135947	26.416679
212.280366	8040.540370	26.421696
212.326184	8067.384493	26.426714
212.456307	8082.343227	26.431732
212.660045	8106.547765	26.436749
212.779626	8112.831421	26.441767
213.188456	8134.406922	26.446784
213.306414	8148.081859	26.451802
213.755115	8165.943151	26.456820
214.223626	8175.976694	26.461837
214.133394	8189.577443	26.466855
214.687830	8195.136715	26.471872
214.459213	8218.748564	26.476890
215.095960	8212.985266	26.481908
215.076716	8238.578259	26.486925
214.897290	8255.443618	26.491943
215.551950	8254.588170	26.496960
215.531323	8278.577726	26.501978
215.494545	8281.437734	26.506996
215.698008	8304.833297	26.512013
215.780682	8327.601306	26.517031
216.342434	8331.946829	26.522048
216.157631	8361.886981	26.527066
216.633983	8377.309399	26.532084
217.281858	8399.072236	26.537101
216.903654	8418.846047	26.542119
217.675504	8431.483330	26.547136
218.042403	8452.524967	26.552154
218.139069	8450.397868	26.557172
218.197052	8468.673952	26.562189
218.395759	8488.190639	26.567207
218.816228	8499.554484	26.572224
218.658147	8514.885378	26.577242
219.456197	8518.655033	26.582260
219.547713	8544.053046	26.587277
219.567904	8551.801069	26.592295
219.743880	8552.763379	26.597312
220.217748	8581.829755	26.602330
220.292700	8571.930463	26.607348
220.794358	8598.335773	26.612365
220.892452	8603.908530	26.617383
221.162523	8617.605291	26.622400
221.064236	8631.076699	26.627418
221.909109	8637.878050	26.632436
221.915608	8638.025364	26.637453
221.960383	8662.758597	26.642471
222.153338	8670.045148	26.647488
222.321057	8672.428804	26.652506
222.409431	8693.963337	26.657524
222.994290	8701.551785	26.662541
222.566275	8717.889121	26.667559
223.068373	8726.383946	26.672576
223.197723	8748.694634	26.677594
223.335362	8760.912340	26.682612
223.664611	8779.861283	26.687629
223.827215	8801.091003	26.692647
224.745840	8793.548535	26.697664
224.914930	8800.023291	26.702682
225.291392	8814.002311	26.707700
225.601965	8820.579647	26.712717
225.701422	8829.023425	26.717735
225.663316	8821.565376	26.722752
225.751081	8821.841388	26.727770
226.098655	8821.661662	26.732788
226.327799	8833.289981	26.737805
226.472121	8848.946417	26.742823
226.924983	8845.781561	26.747840
226.895347	8848.909673	26.752858
227.306201	8858.860010	26.757876
227.446192	8867.520447	26.762893
227.608181	8874.898992	26.767911
227.880451	8868.029264	26.772928
227.859530	8901.091750	26.777946
227.896456	8905.673375	26.782964
228.105968	8908.842468	26.787981
228.244781	8941.476271	26.792999
228.718624	8942.278594	26.798016
228.689284	8957.282115	26.803034
228.738228	8981.866869	26.808052
229.274383	8990.567319	26.813069
229.327870	9019.361986	26.818087
229.964496	9010.809455	26.823104
230.605275	9030.482632	26.828122
230.827478	9026.138666	26.833140
231.363920	9015.311285	26.838157
231.173679	9031.889641	26.843175
231.680326	9034.775706	26.848192
231.860257	9043.944152	26.853210
232.199286	9046.875824	26.858228
232.362903	9049.947598	26.863245
232.195991	9052.749407	26.868263
232.874935	9035.568261	26.873280
232.545010	9061.017408	26.878298
232.733273	9077.902596	26.883316
232.951883	9071.610690	26.888333
232.955989	9097.571295	26.893351
232.978400	9109.973308	26.898368
233.570601	9117.601329	26.903386
233.848623	9136.548267	26.908404
233.752449	9151.737340	26.913421
234.004463	9170.646364	26.918439
234.326773	9177.961731	26.923456
234.610466	9197.564166	26.928474
234.646691	9219.236041	26.933492
235.348246	9226.367822	26.938509
235.585590	9239.157100	26.943527
235.780958	9245.899757	26.948544
236.033844	9263.492957	26.953562
236.231542	9275.336753	26.958580
236.603210	9281.219896	26.963597
236.488897	9293.688318	26.968615
236.574866	9295.463008	26.973632
236.904825	9304.142210	26.978650
236.884178	9340.489235	26.983668
237.220886	9337.094113	26.988685
237.057462	9372.199709	26.993703
237.644135	9398.094337	26.998720
237.706199	9404.654882	27.003738
238.019159	9424.302528	27.008756
238.331945	9431.887895	27.013773
238.382345	9455.506789	27.018791
238.553417	9467.634356	27.023808
238.787202	9488.289836	27.028826
238.850724	9509.284520	27.033844
239.384885	9531.547980	27.038861
239.280348	9563.100478	27.043879
239.628611	9569.944434	27.048896
239.894818	9585.857654	27.053914
240.244441	9608.517376	27.058932
241.130556	9626.982386	27.063949
241.175548	9639.688553	27.068967
241.460991	9643.719646	27.073984
241.638484	9661.535061	27.079002
241.611031	9673.676731	27.084020
242.104802	9699.215624	27.089037
242.268371	9706.693094	27.094055
243.001885	9732.033678	27.099072
242.888876	9735.120961	27.104090
243.294432	9741.465570	27.109108
243.506546	9764.766807	27.114125
243.532878	9778.010825	27.119143
243.955813	9783.298114	27.124160
244.206687	9785.473521	27.129178
244.405151	9804.804263	27.134196
244.970605	9805.576692	27.139213
244.935491	9826.860233	27.144231
245.106587	9826.638195	27.149248
245.625075	9846.798628	27.154266
245.569235	9869.282945	27.159284
245.908155	9861.954344	27.164301
245.983549	9890.238000	27.169319
246.184815	9893.617960	27.174336
246.247190	9928.067524	27.179354
246.412597	9938.317415	27.184372
246.575043	9954.286127	27.189389
246.724009	9972.803740	27.194407
247.026272	9996.364843	27.199424
247.614506	10019.347600	27.204442
247.558616	10046.220127	27.209460
248.176723	10062.161578	27.214477
248.188410	10083.419527	27.219495
248.898937	10088.779530	27.224512
249.726713	10075.527806	27.229530
249.763879	10080.988838	27.234548
250.976270	10073.051857	27.239565
251.008635	10078.390487	27.244583
251.117674	10066.799405	27.249600
251.143580	10057.884416	27.254618
251.094344	10072.208310	27.259636
251.432682	10075.645558	27.264653
251.563987	10090.110293	27.269671
251.922494	10084.564576	27.274688
251.863299	10091.786553	27.279706
251.677362	10093.173792	27.284724
251.923229	10099.259504	27.289741
252.346942	10111.421302	27.294759
252.459671	10127.526798	27.299776
252.623337	10128.097279	27.304794
252.827175	10155.950537	27.309812
252.980998	10153.559492	27.314829
253.213497	10188.533050	27.319847
253.371827	10194.724441	27.324864
253.686744	10217.013241	27.329882
253.809032	10230.350380	27.334900
254.164584	10252.098766	27.339917
254.098423	10264.326176	27.344935
254.419052	10292.758417	27.349952
254.818664	10310.626951	27.354970
254.619963	10333.195329	27.359988
255.151308	10353.660546	27.365005
255.432516	10380.182051	27.370023
255.617735	10404.814305	27.375040
256.150376	10425.170410	27.380058
256.007497	10454.390664	27.385076
256.885954	10455.032967	27.390093
257.554832	10456.993102	27.395111
258.789973	10460.927353	27.400128
259.126979	10465.179476	27.405146
259.516102	10447.181137	27.410164
259.956502	10425.467759	27.415181
259.911731	10413.295311	27.420199
260.204889	10416.178298	27.425216
260.373021	10410.614012	27.430234
260.229301	10417.676077	27.435252
260.414144	10418.231389	27.440269
260.180448	10413.671248	27.445287
260.115708	10410.795957	27.450304
260.733460	10437.845142	27.455322
260.283509	10449.634505	27.460340
260.787008	10459.926096	27.465357
260.970196	10483.948465	27.470375
261.158898	10494.685341	27.475392
261.692938	10515.421875	27.480410
261.449561	10536.623918	27.485428
261.431108	10558.550807	27.490445
261.834857	10578.816300	27.495463
261.695141	10603.235045	27.500480
262.449453	10634.217664	27.505498
262.252118	10659.631446	27.510516
262.718087	10684.262303	27.515533
262.713896	10711.089602	27.520551
262.937030	10737.472635	27.525568
263.500359	10756.380472	27.530586
263.564083	10791.886036	27.535604
263.864161	10805.872795	27.540621
264.259010	10837.168520	27.545639
264.675960	10870.120278	27.550656
265.578686	10875.382645	27.555674
265.397337	10912.324956	27.560692
265.907694	10917.804531	27.565709
266.125798	10926.543037	27.570727
266.177524	10942.008234	27.575744
266.818080	10957.359528	27.580762
266.867157	10980.537910	27.585780
267.154015	10981.893946	27.590797
267.874505	11001.906072	27.595815
267.681219	11016.242407	27.600832
267.864396	11028.584170	27.605850
268.088699	11049.512083	27.610868
268.376913	11060.530222	27.615885
268.440431	11083.407771	27.620903
268.485963	11108.876076	27.625920
269.052823	11123.087226	27.630938
269.353018	11149.863443	27.635956
269.876520	11168.124687	27.640973
269.901419	11186.016597	27.645991
270.183320	11204.141269	27.651008
270.599045	11217.400242	27.656026
270.403183	11243.648270	27.661044
271.371396	11254.554236	27.666061
271.736217	11265.417659	27.671079
272.195438	11273.198640	27.676096
272.776867	11288.788735	27.681114
272.578437	11316.456384	27.686132
273.159588	11311.507743	27.691149
273.181599	11325.145767	27.696167
273.109011	11347.716019	27.701184
273.545596	11342.946052	27.706202
273.606879	11361.814834	27.711220
273.634977	11379.177550	27.716237
274.444421	11395.784520	27.721255
274.500134	11411.996890	27.726272
274.824797	11424.532282	27.731290
274.798713	11440.140650	27.736308
274.659084	11465.026325	27.741325
275.223412	11486.814448	27.746343
275.194493	11512.884230	27.751360
275.393844	11531.563570	27.756378
275.426358	11581.693854	27.761396
276.217481	11603.266544	27.766413
276.967395	11623.780314	27.771431
276.901928	11648.504331	27.776448
277.141158	11668.418919	27.781466
277.535678	11691.645653	27.786484
277.973340	11704.380111	27.791501
278.397179	11723.880265	27.796519
278.017836	11750.670414	27.801536
278.603845	11764.909619	27.806554
278.846421	11792.090489	27.811572
279.043618	11815.275859	27.816589
279.434393	11827.538355	27.821607
279.843975	11862.481461	27.826624
280.060581	11872.292192	27.831642
280.617919	11891.759676	27.836660
280.178302	11898.270210	27.841677
281.013110	11922.135517	27.846695
280.889289	11935.391186	27.851712
281.437523	11953.860974	27.856730
281.207123	11974.460817	27.861748
281.695779	11995.034244	27.866765
282.526583	12012.650317	27.871783
282.374651	12030.885264	27.876800
282.861154	12046.096734	27.881818
283.059345	12068.403328	27.886836
283.335144	12090.884918	27.891853
283.072594	12109.016965	27.896871
283.735622	12136.690685	27.901888
283.999713	12154.718584	27.906906
284.312470	12184.096631	27.911924
284.735334	12190.925569	27.916941
285.254102	12210.288234	27.921959
285.473022	12233.871620	27.926976
286.144786	12248.945343	27.931994
286.122304	12260.326951	27.937012
286.608438	12279.202562	27.942029
286.843088	12296.835661	27.947047
287.031860	12314.307844	27.952064
287.656829	12319.522515	27.957082
287.445446	12339.656205	27.962100
287.676428	12359.766648	27.967117
287.871456	12370.228748	27.972135
288.577838	12390.828425	27.977152
289.017434	12401.306471	27.982170
289.376548	12422.742171	27.987188
289.768085	12428.348684	27.992205
290.239596	12425.623093	27.997223
290.076866	12442.942068	28.002240
290.724792	12446.691819	28.007258
290.687233	12460.569017	28.012276
291.060615	12464.709652	28.017293
291.370959	12474.957058	28.022311
291.536348	12489.639052	28.027328
291.765488	12498.370215	28.032346
292.012073	12514.582465	28.037364
292.487421	12527.636699	28.042381
293.149069	12538.359868	28.047399
293.007011	12560.733022	28.052416
293.276620	12566.113433	28.057434
293.615317	12580.887933	28.062452
293.712868	12605.251416	28.067469
294.176034	12602.240804	28.072487
294.062164	12634.931904	28.077504
294.130999	12639.909051	28.082522
294.409157	12676.736169	28.087540
295.009503	12697.729812	28.092557
295.229624	12715.819304	28.097575
295.134404	12739.983682	28.102592
295.488557	12749.847151	28.107610
296.067042	12781.156000	28.112628
295.865985	12799.190510	28.117645
296.924290	12806.456179	28.122663
296.910747	12829.575436	28.127680
296.996918	12856.386610	28.132698
297.323976	12876.479375	28.137716
297.571963	12895.517094	28.142733
298.118191	12909.735187	28.147751
298.188739	12928.770625	28.152768
298.439214	12955.758088	28.157786
298.769048	12966.716375	28.162804
298.862084	12995.460055	28.167821
299.524290	13006.622802	28.172839
299.613748	13039.554819	28.177856
299.659304	13058.843932	28.182874
300.141797	13090.096592	28.187892
300.570871	13110.409261	28.192909
300.630190	13130.427374	28.197927
300.919815	13167.168737	28.202944
301.368241	13185.296790	28.207962
301.712213	13214.311723	28.212980
301.913876	13240.652938	28.217997
302.543812	13253.250217	28.223015
303.173655	13266.609012	28.228032
303.481415	13280.815079	28.233050
304.268005	13289.784534	28.238068
304.505283	13309.653273	28.243085
305.237953	13322.011270	28.248103
305.274645	13318.349797	28.253120
305.646189	13314.855075	28.258138
305.707358	13330.224375	28.263156
305.480423	13348.597418	28.268173
306.466078	13343.955711	28.273191
306.635069	13359.378309	28.278208
307.374957	13374.383656	28.283226
307.470853	13366.122509	28.288244
307.674443	13372.907525	28.293261
308.308777	13385.048438	28.298279
308.226192	13402.390856	28.303296
308.479482	13408.493354	28.308314
308.859040	13406.437184	28.313332
308.390577	13429.994705	28.318349
309.155911	13434.828446	28.323367
309.350347	13468.438559	28.328384
309.295151	13479.432306	28.333402
309.753032	13491.295703	28.338420
309.868510	13511.335155	28.343437
310.331001	13525.468183	28.348455
310.389877	13554.799206	28.353472
310.641240	13565.061866	28.358490
310.995957	13596.335633	28.363508
311.200025	13621.522809	28.368525
311.673273	13636.630539	28.373543
312.064784	13661.497338	28.378560
311.777097	13679.397517	28.383578
312.381717	13704.522373	28.388596
312.678307	13717.185365	28.393613
313.061505	13747.250495	28.398631
313.295317	13775.479832	28.403648
313.293873	13787.667777	28.408666
313.892850	13817.653295	28.413684
314.134081	13846.978054	28.418701
314.724936	13851.039645	28.423719
314.834690	13892.094093	28.428736
315.281030	13903.588977	28.433754
315.469753	13931.068399	28.438772
315.638398	13951.967629	28.443789
316.425982	13978.043262	28.448807
316.473124	13994.939501	28.453824
316.812148	14018.562795	28.458842
317.492480	14029.535761	28.463860
317.500985	14053.168288	28.468877
318.386961	14070.179986	28.473895
318.149968	14089.575058	28.478912
318.716458	14108.379129	28.483930
319.229780	14116.466569	28.488948
319.974057	14135.417103	28.493965
320.584885	14138.859987	28.498983
320.585451	14138.135672	28.504000
320.658611	14150.767520	28.509018
321.802473	14155.755003	28.514036
321.866397	14159.562541	28.519053
322.108191	14159.069897	28.524071
322.241294	14177.710496	28.529088
322.338674	14184.484066	28.534106
322.692089	14181.394015	28.539124
322.955034	14208.065342	28.544141
323.288844	14221.112300	28.549159
323.424535	14235.833378	28.554176
323.340495	14254.133268	28.559194
324.077608	14266.704966	28.564212
323.788974	14296.486694	28.569229
323.813566	14320.417888	28.574247
323.853566	14348.757006	28.579264
324.592381	14384.657544	28.584282
324.734349	14415.773725	28.589300
325.022360	14451.962945	28.594317
325.783111	14471.907715	28.599335
325.979171	14499.397221	28.604352
326.025729	14531.987097	28.609370
326.268441	14560.954303	28.614388
326.492547	14588.509366	28.619405
327.153774	14616.785899	28.624423
327.667008	14636.776823	28.629440
328.189516	14674.175108	28.634458
328.271145	14682.617315	28.639476
328.567227	14716.459688	28.644493
329.226877	14745.293195	28.649511
329.540207	14752.389620	28.654528
329.915043	14781.017450	28.659546
330.331960	14798.930637	28.664564
330.383173	14823.237334	28.669581
330.794405	14830.030454	28.674599
331.046992	14850.834602	28.679616
331.212153	14869.026429	28.684634
331.960502	14886.847247	28.689652
332.141000	14912.025048	28.694669
332.665197	14922.838440	28.699687
332.624832	14945.271392	28.704704
332.911722	14972.703382	28.709722
333.481180	14985.257715	28.714740
333.610196	15008.258444	28.719757
334.006087	15033.377224	28.724775
334.107434	15058.825510	28.729792
334.228954	15083.317050	28.734810
334.875512	15100.574320	28.739828
335.272871	15134.576346	28.744845
335.335748	15159.101953	28.749863
335.683414	15184.512180	28.754880
335.704768	15218.289022	28.759898
336.420060	15241.206909	28.764916
336.398998	15268.933736	28.769933
336.797393	15297.057476	28.774951
337.359127	15334.910398	28.779968
337.935153	15365.301857	28.784986
338.620850	15386.817415	28.790004
338.756963	15418.813098	28.795021
339.095378	15436.665930	28.800039
339.435200	15459.791198	28.805056
339.404206	15493.930280	28.810074
340.134071	15514.538915	28.815092
340.262585	15533.992994	28.820109
340.665180	15563.790131	28.825127
341.224493	15583.133307	28.830144
341.295261	15624.698919	28.835162
341.832452	15642.403402	28.840180
341.631542	15680.471800	28.845197
342.339766	15688.241560	28.850215
343.271608	15703.253066	28.855232
343.487183	15721.574170	28.860250
344.275966	15719.568818	28.865268
344.919644	15733.246338	28.870285
345.534485	15736.337722	28.875303
345.838620	15738.918849	28.880320
345.838340	15745.643817	28.885338
346.647059	15738.743208	28.890356
346.694467	15763.275982	28.895373
347.206455	15766.150525	28.900391
347.472691	15765.092695	28.905408
347.113170	15777.599774	28.910426
347.998103	15792.179531	28.915444
348.464236	15797.299095	28.920461
348.135308	15805.396173	28.925479
348.018426	15821.620252	28.930496
348.101351	15843.541128	28.935514
349.154640	15852.262162	28.940532
349.040380	15879.934279	28.945549
349.318888	15899.766838	28.950567
349.809425	15911.716968	28.955584
350.057497	15930.167968	28.960602
350.171411	15950.786574	28.965620
350.427373	15978.257369	28.970637
350.706987	16001.971130	28.975655
350.938438	16028.951883	28.980672
351.175230	16067.579961	28.985690
351.601066	16083.807194	28.990708
351.978555	16119.002525	28.995725
352.338548	16146.163372	29.000743
352.649432	16184.810642	29.005760
352.853333	16221.460690	29.010778
353.371331	16235.006339	29.015796
353.996426	16259.018559	29.020813
354.344240	16292.920126	29.025831
354.746266	16304.523479	29.030848
355.104128	16331.223421	29.035866
355.684647	16360.479820	29.040884
355.796581	16384.723993	29.045901
356.312868	16405.198191	29.050919
357.064691	16427.845717	29.055936
356.998987	16451.032566	29.060954
357.640149	16476.638100	29.065972
357.842029	16500.941148	29.070989
358.477648	16528.164645	29.076007
358.490848	16544.079011	29.081024
358.669548	16564.638707	29.086042
359.416784	16586.237279	29.091060
359.622958	16609.590870	29.096077
360.093459	16631.599126	29.101095
360.681675	16649.845027	29.106112
360.844760	16682.965330	29.111130
360.896822	16701.690201	29.116148
361.280980	16713.869900	29.121165
361.900562	16748.760392	29.126183
362.207732	16759.757198	29.131200
362.154061	16791.238757	29.136218
362.673271	16811.640790	29.141236
362.870658	16846.465713	29.146253
363.004526	16879.438935	29.151271
363.297609	16894.510684	29.156288
363.344642	16941.216400	29.161306
363.831027	16976.813831	29.166324
364.293656	17007.071687	29.171341
364.670944	17040.780049	29.176359
365.128674	17082.167845	29.181376
365.487437	17116.802118	29.186394
366.078374	17138.366923	29.191412
366.096668	17175.562563	29.196429
366.494780	17214.127642	29.201447
367.387164	17229.341617	29.206464
367.391907	17264.858980	29.211482
368.202122	17289.207863	29.216500
368.602043	17317.640155	29.221517
368.735442	17330.357134	29.226535
369.688400	17342.043165	29.231552
370.192235	17358.024672	29.236570
370.707158	17367.698291	29.241588
371.167511	17383.550537	29.246605
371.294696	17401.368439	29.251623
371.814846	17408.681070	29.256640
372.234041	17423.351753	29.261658
372.348989	17428.245155	29.266676
373.073383	17445.702208	29.271693
373.410563	17447.672077	29.276711
373.846640	17449.110450	29.281728
373.670652	17467.245627	29.286746
374.492558	17485.663548	29.291764
374.671453	17504.729606	29.296781
374.942326	17527.578612	29.301799
375.365942	17530.629978	29.306816
375.480470	17565.779754	29.311834
375.898370	17571.324134	29.316852
376.016318	17596.358210	29.321869
375.733232	17626.210514	29.326887
376.108389	17647.158057	29.331904
376.291115	17686.336973	29.336922
376.897085	17717.283611	29.341940
377.362196	17762.364951	29.346957
377.338619	17801.304587	29.351975
377.594055	17826.575001	29.356992
377.652537	17878.159288	29.362010
378.393448	17911.359239	29.367028
378.814362	17952.456403	29.372045
379.482551	17995.278474	29.377063
379.895804	18035.649115	29.382080
380.001418	18073.207011	29.387098
380.535865	18107.038320	29.392116
381.243960	18141.240470	29.397133
381.550941	18176.658606	29.402151
382.331148	18202.184214	29.407168
382.427759	18230.555481	29.412186
383.147617	18251.887119	29.417204
383.912428	18284.093872	29.422221
383.833215	18302.435473	29.427239
384.819314	18315.907189	29.432256
385.142896	18356.419332	29.437274
385.727103	18362.403659	29.442292
386.324539	18386.603918	29.447309
386.378959	18399.306795	29.452327
386.587149	18419.674873	29.457344
386.919830	18445.792683	29.462362
387.384140	18452.035529	29.467380
387.780423	18467.560104	29.472397
388.201922	18489.308522	29.477415
388.859878	18495.877242	29.482432
388.997806	18525.830727	29.487450
389.279467	18518.189432	29.492468
389.258422	18550.207761	29.497485
389.275015	18565.308654	29.502503
390.260381	18588.590682	29.507520
390.348807	18620.118853	29.512538
390.765246	18636.588468	29.517556
390.931671	18665.328951	29.522573
390.966796	18694.928646	29.527591
391.483859	18728.019939	29.532608
391.793494	18760.072631	29.537626
392.232619	18793.393030	29.542644
392.628534	18826.160110	29.547661
392.567741	18865.951303	29.552679
393.118539	18898.537941	29.557696
393.656894	18930.852988	29.562714
393.875590	18966.792536	29.567732
394.086218	19004.467053	29.572749
394.321689	19048.931961	29.577767
394.978271	19084.164950	29.582784
395.235375	19134.731502	29.587802
395.737191	19161.945709	29.592820
396.689802	19188.033713	29.597837
397.137291	19231.542047	29.602855
397.738688	19252.907718	29.607872
398.222865	19289.584917	29.612890
398.668647	19320.876837	29.617908
398.945587	19345.104452	29.622925
399.117405	19373.713082	29.627943
399.684859	19402.089418	29.632960
399.939559	19440.270616	29.637978
400.080155	19471.137789	29.642996
401.018379	19507.966017	29.648013
400.831734	19557.006425	29.653031
401.410593	19571.199319	29.658048
401.989368	19602.186328	29.663066
402.574452	19639.046325	29.668084
403.152789	19660.214236	29.673101
403.314731	19692.071477	29.678119
404.239900	19711.686771	29.683136
404.451983	19737.310932	29.688154
405.147782	19754.550316	29.693172
405.562620	19777.839585	29.698189
405.423996	19805.953119	29.703207
406.451094	19823.586704	29.708224
406.992458	19850.194551	29.713242
407.252526	19861.133731	29.718260
407.349749	19878.118967	29.723277
407.538684	19908.584758	29.728295
408.170742	19929.236533	29.733312
408.497523	19950.187007	29.738330
408.575583	19987.569220	29.743348
409.168478	20012.641358	29.748365
409.368408	20044.348359	29.753383
409.750129	20076.485584	29.758400
410.036717	20096.007406	29.763418
410.136199	20125.002610	29.768436
410.946935	20155.761606	29.773453
411.042904	20188.229276	29.778471
411.444679	20208.505446	29.783488
411.802494	20236.140987	29.788506
411.934129	20279.991579	29.793524
412.546512	20305.183935	29.798541
413.088064	20346.975382	29.803559
413.407349	20378.684125	29.808576
413.700108	20403.680277	29.813594
414.344988	20450.624125	29.818612
414.625776	20474.628426	29.823629
414.877201	20528.311151	29.828647
415.600907	20548.408890	29.833664
416.092852	20579.594380	29.838682
416.532619	20621.947754	29.843700
417.260006	20645.122758	29.848717
417.436374	20677.370716	29.853735
417.636193	20712.970753	29.858752
417.886894	20747.393250	29.863770
418.606731	20769.674983	29.868788
419.475066	20792.863977	29.873805
419.763852	20820.197310	29.878823
420.366318	20854.917612	29.883840
420.806823	20873.339289	29.888858
421.024076	20899.198822	29.893876
421.380693	20920.666810	29.898893
421.965051	20957.528449	29.903911
422.004513	20991.687437	29.908928
422.559847	21023.153531	29.913946
423.035399	21049.589611	29.918964
423.835651	21084.629377	29.923981
423.882698	21117.172912	29.928999
424.541901	21135.087513	29.934016
425.031015	21153.949904	29.939034
425.217821	21186.448477	29.944052
425.477954	21214.010730	29.949069
426.095103	21253.065172	29.954087
426.503117	21284.329225	29.959104
427.184314	21314.616537	29.964122
427.440093	21329.646934	29.969140
428.006940	21355.431043	29.974157
428.311909	21383.584223	29.979175
428.793178	21417.439046	29.984192
429.330937	21432.371062	29.989210
429.646123	21467.268436	29.994228
430.080982	21495.527925	29.999245
430.414195	21522.250531	30.004263
430.716783	21554.018647	30.009280
431.416435	21590.943737	30.014298
431.489273	21618.983102	30.019316
431.971537	21635.918343	30.024333
431.995561	21687.302872	30.029351
432.528049	21709.006188	30.034368
433.028100	21744.057446	30.039386
433.515196	21779.606248	30.044404
434.193291	21802.920772	30.049421
435.431566	21797.230764	30.054439
436.426029	21800.474796	30.059456
437.069015	21800.464525	30.064474
437.640213	21792.559723	30.069492
438.300893	21781.180730	30.074509
438.319749	21805.831308	30.079527
438.309867	21820.320096	30.084544
438.889049	21821.931429	30.089562
438.662251	21836.060985	30.094580
439.713515	21842.169953	30.099597
439.543701	21852.060213	30.104615
440.285851	21874.050913	30.109632
440.605047	21878.222441	30.114650
440.958969	21894.597155	30.119668
441.166921	21904.354019	30.124685
441.677297	21936.776599	30.129703
441.749072	21954.708537	30.134720
442.406745	21973.842779	30.139738
442.312482	22010.620458	30.144756
442.474987	22038.002013	30.149773
442.755690	22077.665008	30.154791
443.001004	22118.476576	30.159808
443.748587	22158.192988	30.164826
443.965359	22206.448419	30.169844
444.422974	22233.020878	30.174861
444.820715	22283.026170	30.179879
445.324707	22326.995623	30.184896
445.704361	22367.370562	30.189914
445.989436	22417.087837	30.194932
446.469483	22442.403160	30.199949
446.958578	22487.966458	30.204967
447.364156	22530.431224	30.209984
447.877226	22579.800783	30.215002
448.269807	22622.825518	30.220020
449.008618	22666.002365	30.225037
449.237712	22706.715637	30.230055
449.933515	22749.627824	30.235072
451.071750	22770.413796	30.240090
451.581092	22810.020146	30.245108
452.061055	22834.260174	30.250125
452.653195	22857.077191	30.255143
453.022638	22886.410564	30.260160
453.702196	22920.628488	30.265178
454.254677	22927.609736	30.270196
454.923760	22952.397173	30.275213
455.364984	22959.414274	30.280231
455.699290	22982.730178	30.285248
455.988247	23001.290338	30.290266
456.279570	23027.378642	30.295284
456.769645	23055.462779	30.300301
457.339446	23080.672670	30.305319
457.578198	23102.454630	30.310336
457.993017	23119.858273	30.315354
457.959539	23154.045360	30.320372
458.361973	23174.164562	30.325389
458.900776	23207.457173	30.330407
459.026958	23246.074106	30.335424
459.904011	23271.898578	30.340442
460.255209	23306.682423	30.345460
460.486861	23339.848588	30.350477
460.852102	23373.730812	30.355495
461.302163	23408.137584	30.360512
461.712269	23447.518728	30.365530
462.012533	23487.865055	30.370548
462.701447	23528.353584	30.375565
463.037884	23563.906765	30.380583
463.270710	23607.649637	30.385600
463.820821	23644.832569	30.390618
464.084837	23682.687382	30.395636
464.566862	23718.692698	30.400653
465.133836	23764.909710	30.405671
465.777655	23800.894952	30.410688
466.300106	23844.193759	30.415706
466.471564	23895.106649	30.420724
467.176235	23938.308941	30.425741
467.767386	23981.253734	30.430759
467.908523	24017.602332	30.435776
468.617605	24064.013408	30.440794
468.919126	24111.124444	30.445812
469.808884	24149.909448	30.450829
470.690464	24179.484228	30.455847
471.076110	24209.046689	30.460864
471.376234	24241.613031	30.465882
472.306171	24270.178291	30.470900
472.865595	24295.163324	30.475917
473.270012	24333.959921	30.480935
473.503111	24360.649695	30.485952
474.191028	24384.220903	30.490970
474.443289	24428.807379	30.495988
475.230038	24436.014298	30.501005
476.386981	24451.019905	30.506023
477.005682	24468.342136	30.511040
477.892756	24468.671909	30.516058
478.161938	24484.544471	30.521076
478.824590	24495.798884	30.526093
479.169097	24519.191040	30.531111
479.490005	24536.349667	30.536128
479.853920	24536.512279	30.541146
480.269050	24557.259040	30.546164
480.493447	24579.246970	30.551181
480.784528	24603.936506	30.556199
481.002607	24617.590392	30.561216
481.781116	24645.985880	30.566234
482.117572	24676.646496	30.571252
482.411581	24693.201438	30.576269
482.820151	24714.637940	30.581287
482.874906	24736.166280	30.586304
483.677521	24761.399261	30.591322
483.991671	24794.990938	30.596340
483.947798	24826.400133	30.601357
484.590313	24849.685434	30.606375
484.567299	24884.687520	30.611392
485.439422	24914.539317	30.616410
485.577261	24967.034132	30.621428
485.986034	25001.762876	30.626445
486.390879	25046.768706	30.631463
486.364164	25092.936038	30.636480
486.937109	25131.491092	30.641498
487.838921	25186.782827	30.646516
487.942447	25235.076498	30.651533
488.504030	25284.064644	30.656551
488.828609	25332.132754	30.661568
489.674581	25370.158833	30.666586
490.365906	25425.131995	30.671604
490.917232	25477.327067	30.676621
491.695505	25511.111800	30.681639
492.207682	25559.643076	30.686656
492.840756	25582.474032	30.691674
493.326947	25632.097606	30.696692
493.851139	25664.903732	30.701709
494.498526	25690.763997	30.706727
494.908041	25739.235753	30.711744
495.523448	25766.005627	30.716762
496.189388	25813.172343	30.721780
496.618265	25833.551456	30.726797
497.135075	25868.300321	30.731815
497.494140	25907.382114	30.736832
498.147382	25942.926364	30.741850
498.432720	25972.675079	30.746868
498.854286	26017.112169	30.751885
499.881609	26042.318474	30.756903
499.888459	26082.096499	30.761920
500.286134	26115.803689	30.766938
500.908094	26147.506467	30.771956
502.026322	26181.372395	30.776973
502.447127	26205.982286	30.781991
502.986837	26248.683748	30.787008
503.127334	26271.864371	30.792026
503.353062	26313.514639	30.797044
504.011579	26344.817282	30.802061
503.975985	26391.469541	30.807079
504.667184	26443.665171	30.812096
505.212715	26478.798395	30.817114
505.480241	26525.678502	30.822132
505.924259	26568.866394	30.827149
506.802207	26609.260142	30.832167
507.082542	26663.295357	30.837184
507.768742	26708.269692	30.842202
508.223071	26743.877336	30.847220
508.671780	26792.944000	30.852237
509.120421	26824.205373	30.857255
509.462216	26875.919166	30.862272
509.999171	26901.842307	30.867290
510.276443	26951.883763	30.872308
510.755588	27005.492163	30.877325
511.356616	27036.253807	30.882343
511.901963	27082.827347	30.887360
512.053799	27132.697103	30.892378
512.337101	27175.461557	30.897396
513.131919	27230.084045	30.902413
513.590166	27278.933214	30.907431
513.709949	27323.017792	30.912448
514.529737	27378.731953	30.917466
515.205783	27428.035365	30.922484
515.779823	27468.838161	30.927501
517.336485	27495.802149	30.932519
518.651993	27513.871553	30.937536
519.918936	27530.803127	30.942554
520.593044	27542.318666	30.947572
520.824330	27546.567944	30.952589
521.175857	27574.321236	30.957607
521.235565	27582.816204	30.962624
521.653899	27605.708669	30.967642
522.062963	27635.852813	30.972660
521.888318	27673.909030	30.977677
522.366314	27696.588844	30.982695
522.599229	27740.995336	30.987712
523.285380	27786.788948	30.992730
523.510344	27817.301549	30.997748
524.395178	27849.297515	31.002765
525.495551	27874.081422	31.007783
525.963709	27920.954894	31.012800
526.643468	27941.251809	31.017818
527.038402	27981.710962	31.022836
527.234235	28019.308723	31.027853
527.889172	28051.899549	31.032871
528.054815	28091.383817	31.037888
528.415771	28133.296944	31.042906
529.141872	28179.145185	31.047924
529.286250	28222.437224	31.052941
529.953363	28255.127372	31.057959
530.147509	28308.260728	31.062976
530.744395	28352.232719	31.067994
531.103011	28389.673039	31.073012
531.501074	28459.388656	31.078029
531.952848	28495.909839	31.083047
532.589932	28561.147036	31.088064
532.987541	28617.969629	31.093082
533.816069	28664.954896	31.098100
534.006841	28720.740768	31.103117
534.863116	28772.025673	31.108135
535.250285	28823.056092	31.113152
535.915664	28873.865860	31.118170
536.608728	28931.536027	31.123188
536.989300	28975.273101	31.128205
537.496399	29026.839779	31.133223
537.902988	29071.934561	31.138240
538.375276	29129.301769	31.143258
538.879290	29172.580028	31.148276
539.020864	29217.668568	31.153293
539.802588	29270.763485	31.158311
540.200347	29326.776918	31.163328
540.924033	29362.180368	31.168346
541.676274	29422.280842	31.173364
541.976465	29472.923704	31.178381
542.961602	29512.529900	31.183399
543.309057	29564.465689	31.188416
543.520993	29610.450288	31.193434
545.188731	29630.867766	31.198452
546.433835	29671.397443	31.203469
547.362111	29687.857287	31.208487
547.835727	29729.056845	31.213504
548.393406	29750.391983	31.218522
548.663802	29765.889741	31.223540
549.038592	29815.353979	31.228557
549.527850	29831.012364	31.233575
550.257708	29868.262999	31.238592
550.468267	29893.494316	31.243610
551.254759	29927.115994	31.248628
551.652428	29951.195486	31.253645
552.271533	29982.662746	31.258663
552.494867	30034.262044	31.263680
553.138542	30050.132450	31.268698
553.493242	30091.752171	31.273716
553.738584	30137.193934	31.278733
554.542898	30172.882600	31.283751
554.630990	30224.277088	31.288768
555.221665	30279.689390	31.293786
555.490904	30325.381611	31.298804
555.997426	30376.085822	31.303821
556.792427	30428.377035	31.308839
557.139917	30479.084827	31.313856
557.538265	30534.910028	31.318874
558.267445	30594.266708	31.323892
558.587315	30658.407553	31.328909
559.260373	30691.591810	31.333927
559.778293	30753.471336	31.338944
560.391669	30796.769581	31.343962
560.872772	30851.416375	31.348980
561.713784	30898.302071	31.353997
562.650607	30952.641786	31.359015
563.186897	30994.743961	31.364032
563.950601	31045.711896	31.369050
564.601717	31083.761170	31.374068
565.116047	31128.253422	31.379085
565.960330	31169.605622	31.384103
566.761638	31202.551410	31.389120
567.519380	31247.755457	31.394138
568.073679	31266.925939	31.399156
568.552979	31301.488307	31.404173
569.311849	31333.876862	31.409191
569.693869	31358.272993	31.414208
569.985134	31384.237690	31.419226
570.802057	31415.187599	31.424244
570.838651	31444.529651	31.429261
571.392633	31486.447437	31.434279
571.579905	31530.332456	31.439296
571.861940	31565.346053	31.444314
572.471898	31613.293519	31.449332
572.985574	31660.061722	31.454349
573.364895	31713.898529	31.459367
573.562314	31756.009337	31.464384
574.262463	31827.979806	31.469402
574.942916	31871.095245	31.474420
574.919312	31936.033428	31.479437
575.435716	31984.863782	31.484455
576.023943	32060.202514	31.489472
576.666471	32113.831632	31.494490
577.336583	32193.645411	31.499508
577.993974	32254.427084	31.504525
578.780786	32318.719130	31.509543
579.266561	32370.725307	31.514560
579.569135	32441.384134	31.519578
580.602702	32498.274950	31.524596
581.383817	32559.484121	31.529613
581.642421	32615.201495	31.534631
582.370791	32680.327064	31.539648
582.834941	32731.748297	31.544666
583.587816	32797.452068	31.549684
583.939095	32867.873246	31.554701
585.360443	32895.930207	31.559719
586.651317	32944.952171	31.564736
587.392241	32976.886543	31.569754
588.418280	33006.962830	31.574772
588.993517	33049.549554	31.579789
589.568823	33077.204038	31.584807
589.876129	33122.194921	31.589824
590.484407	33152.427851	31.594842
591.195973	33178.818673	31.599860
591.288190	33230.812989	31.604877
592.120950	33255.898359	31.609895
592.519616	33289.787307	31.614912
592.688331	33340.210798	31.619930
593.525585	33385.693364	31.624948
593.992915	33441.012991	31.629965
593.930955	33492.380073	31.634983
594.519703	33544.200142	31.640000
594.788458	33596.943053	31.645018
595.681663	33659.648591	31.650036
595.711609	33728.127344	31.655053
596.436050	33784.498016	31.660071
596.995258	33840.302475	31.665088
597.679152	33913.001852	31.670106
599.162298	33953.340271	31.675124
599.732527	34018.423768	31.680141
600.157998	34065.507603	31.685159
600.733194	34103.293755	31.690176
601.106399	34155.407008	31.695194
601.704449	34204.309726	31.700212
602.086885	34252.947403	31.705229
602.817273	34304.072581	31.710247
603.667771	34359.258578	31.715264
603.933524	34418.436388	31.720282
604.711100	34458.033968	31.725300
604.996060	34513.455566	31.730317
605.511688	34551.290056	31.735335
606.623693	34600.911354	31.740352
607.154647	34667.455551	31.745370
607.891234	34717.267823	31.750388
608.159184	34770.041376	31.755405
608.776715	34821.619642	31.760423
609.575736	34883.780418	31.765440
609.796068	34939.481721	31.770458
610.388218	35004.803627	31.775476
611.035505	35056.437787	31.780493
611.658247	35110.032446	31.785511
612.617543	35171.063646	31.790528
612.830534	35223.678697	31.795546
613.751888	35286.581369	31.800564
613.974136	35351.753856	31.805581
614.664180	35397.353652	31.810599
615.352775	35472.352920	31.815616
615.468700	35531.112368	31.820634
616.276637	35606.410116	31.825652
616.966494	35663.439032	31.830669
617.971528	35718.901310	31.835687
618.707279	35785.530856	31.840704
619.271545	35841.245030	31.845722
620.144726	35903.030447	31.850740
620.752631	35948.886041	31.855757
621.501725	36005.832592	31.860775
622.575647	36047.225049	31.865792
623.086662	36105.759633	31.870810
623.727536	36151.755578	31.875828
624.722628	36194.545203	31.880845
625.260398	36252.735494	31.885863
625.720183	36284.437199	31.890880
626.415875	36337.648940	31.895898
627.096561	36374.658779	31.900916
627.544499	36426.174398	31.905933
627.860399	36482.401659	31.910951
628.595649	36523.915442	31.915968
629.373883	36573.873239	31.920986
630.055465	36629.949744	31.926004
630.729057	36678.355758	31.931021
630.908519	36739.168409	31.936039
631.681351	36780.640580	31.941056
632.086857	36838.978515	31.946074
632.823118	36890.744482	31.951092
633.171487	36945.400915	31.956109
633.701010	37000.069674	31.961127
634.580973	37043.076881	31.966144
634.769097	37114.268778	31.971162
635.467745	37157.514847	31.976180
636.263686	37201.729392	31.981197
636.651849	37260.402652	31.986215
637.335873	37320.876904	31.991232
637.543231	37385.807370	31.996250
638.365977	37434.559182	32.001268
638.971894	37498.398602	32.006285
639.617906	37563.936320	32.011303
640.488783	37623.245083	32.016320
640.605001	37688.407235	32.021338
641.197076	37753.452873	32.026356
642.251389	37806.260539	32.031373
643.132468	37863.741072	32.036391
643.821938	37927.147814	32.041408
644.193702	38001.431459	32.046426
644.951746	38046.267615	32.051444
645.564257	38107.585451	32.056461
645.604512	38187.692124	32.061479
646.804708	38243.336640	32.066496
647.063853	38315.771098	32.071514
647.745249	38383.406649	32.076532
648.808999	38451.057276	32.081549
649.116063	38522.616166	32.086567
650.343685	38575.091161	32.091584
650.623023	38644.765950	32.096602
651.561518	38705.614609	32.101620
652.495735	38759.352631	32.106637
652.815764	38832.922808	32.111655
653.731547	38882.453981	32.116672
654.294762	38948.041774	32.121690
654.789031	39017.311730	32.126708
655.216517	39070.290951	32.131725
656.098424	39156.955673	32.136743
656.545749	39216.982398	32.141760
657.098050	39296.653236	32.146778
658.208931	39340.007977	32.151796
659.504304	39394.461607	32.156813
660.334397	39457.033268	32.161831
661.263477	39500.721708	32.166848
661.612321	39553.547803	32.171866
661.947310	39608.818910	32.176884
662.870350	39664.769259	32.181901
663.148284	39725.487053	32.186919
663.812734	39771.938523	32.191936
664.121672	39847.520702	32.196954
664.684500	39907.585085	32.201972
665.223795	39973.008746	32.206989
665.418751	40045.681555	32.212007
666.354363	40115.395061	32.217024
667.026940	40187.897811	32.222042
667.787678	40249.269155	32.227060
668.549646	40317.440466	32.232077
669.144927	40383.399265	32.237095
669.946387	40444.928836	32.242112
670.515474	40509.154445	32.247130
671.113276	40571.309846	32.252148
672.336549	40623.276182	32.257165
672.558370	40691.749456	32.262183
673.421008	40742.865213	32.267200
674.171924	40813.610804	32.272218
674.502184	40866.205781	32.277236
675.266682	40921.948939	32.282253
675.677149	40992.165967	32.287271
676.551661	41052.534850	32.292288
677.019132	41121.730867	32.297306
677.801624	41173.116151	32.302324
678.505546	41246.460543	32.307341
678.844691	41315.914333	32.312359
679.907416	41387.994166	32.317376
680.528885	41447.136753	32.322394
681.205115	41520.407869	32.327412
681.919088	41577.933854	32.332429
682.789895	41655.732379	32.337447
683.491297	41703.252486	32.342464
683.966368	41791.280672	32.347482
684.476438	41851.019608	32.352500
685.712384	41917.995757	32.357517
686.244318	41992.859523	32.362535
687.067391	42053.968753	32.367552
687.820147	42124.527039	32.372570
688.382449	42178.133157	32.377588
689.090209	42242.661755	32.382605
689.250805	42316.746998	32.387623
690.093357	42384.244970	32.392640
690.496712	42464.080413	32.397658
691.272574	42531.204746	32.402676
692.154909	42613.283083	32.407693
692.482937	42696.550943	32.412711
693.359121	42763.224899	32.417728
694.385335	42838.855869	32.422746
695.366493	42912.257848	32.427764
696.005657	42973.159876	32.432781
696.350204	43051.827631	32.437799
697.446480	43116.594160	32.442816
697.702553	43196.336559	32.447834
698.390416	43277.486890	32.452852
699.249093	43337.967250	32.457869
699.810594	43420.081566	32.462887
700.492170	43487.890227	32.467904
701.427630	43561.945763	32.472922
702.007977	43647.685895	32.477940
702.376424	43717.384418	32.482957
702.924016	43795.852872	32.487975
704.188533	43859.402959	32.492992
705.058692	43940.896460	32.498010
705.693134	44007.175198	32.503028
706.683704	44073.255534	32.508045
707.340722	44143.073866	32.513063
708.468627	44187.280453	32.518080
709.546080	44237.425977	32.523098
710.284666	44288.218675	32.528116
711.136969	44330.024620	32.533133
712.000100	44374.608234	32.538151
712.914294	44400.599443	32.543168
713.524669	44451.441422	32.548186
714.193343	44487.570098	32.553204
714.862292	44530.090289	32.558221
715.050957	44582.122868	32.563239
715.788100	44629.582234	32.568256
716.595747	44676.623542	32.573274
716.950891	44735.617865	32.578292
718.002431	44791.728475	32.583309
718.181098	44851.492656	32.588327
718.645617	44898.191683	32.593344
719.364541	44960.914614	32.598362
719.918576	45033.450272	32.603380
720.904545	45094.916567	32.608397
721.432488	45161.216652	32.613415
722.024618	45234.198222	32.618432
722.585221	45298.657502	32.623450
723.232170	45365.299071	32.628468
723.955995	45445.384282	32.633485
724.357753	45521.631125	32.638503
725.077422	45599.979349	32.643520
726.185807	45677.710775	32.648538
726.481067	45770.564324	32.653556
726.968961	45846.234130	32.658573
727.431513	45923.804441	32.663591
728.223616	46019.258792	32.668608
728.730138	46113.733744	32.673626
729.478772	46197.112276	32.678644
730.748396	46287.970915	32.683661
731.018730	46382.727849	32.688679
731.958661	46476.343836	32.693696
732.784555	46562.097042	32.698714
733.302746	46655.626519	32.703732
734.643300	46734.354236	32.708749
735.095947	46831.308927	32.713767
736.043084	46912.198238	32.718784
736.893421	47001.792680	32.723802
737.302373	47082.058528	32.728820
738.223901	47168.364243	32.733837
738.817150	47258.338519	32.738855
739.850100	47347.845701	32.743872
740.840964	47421.934013	32.748890
741.341358	47518.354796	32.753908
742.339426	47582.784367	32.758925
743.017410	47660.725598	32.763943
743.772365	47743.940059	32.768960
745.019803	47813.568589	32.773978
745.649315	47899.387958	32.778996
746.767885	47963.821826	32.784013
747.158180	48039.614401	32.789031
748.163303	48085.999193	32.794048
748.940752	48148.175150	32.799066
749.734661	48216.356568	32.804084
749.986818	48273.138821	32.809101
750.637556	48341.687451	32.814119
751.374139	48403.927608	32.819136
752.443339	48478.888246	32.824154
752.964105	48545.754418	32.829172
753.819148	48609.216531	32.834189
754.102777	48695.056944	32.839207
754.888539	48763.257540	32.844224
755.854886	48840.022084	32.849242
756.125375	48916.695771	32.854260
756.791427	48996.743195	32.859277
757.373937	49080.852841	32.864295
757.980467	49159.512565	32.869312
759.041310	49258.980757	32.874330
759.479167	49350.643908	32.879348
760.435984	49430.763758	32.884365
760.985610	49512.744331	32.889383
761.948440	49604.192687	32.894400
763.131690	49703.896330	32.899418
763.594588	49783.632505	32.904436
764.721135	49869.641036	32.909453
765.460551	49952.470700	32.914471
766.341128	50029.976682	32.919488
767.612762	50102.270611	32.924506
768.200621	50196.303111	32.929524
769.553749	50254.068279	32.934541
770.832934	50319.302472	32.939559
771.533286	50385.253880	32.944576
772.629436	50438.828658	32.949594
772.882996	50496.656023	32.954612
773.548768	50563.651850	32.959629
774.249288	50626.896441	32.964647
775.105107	50699.306311	32.969664
775.754645	50769.256193	32.974682
776.440496	50849.794774	32.979700
777.154190	50909.812982	32.984717
777.961010	50992.128637	32.989735
778.644023	51054.086767	32.994752
779.347086	51122.186464	32.999770
779.829147	51197.122597	33.004788
780.687352	51270.926157	33.009805
781.755137	51347.792642	33.014823
782.294990	51436.063908	33.019840
783.180912	51503.176534	33.024858
783.818863	51601.270161	33.029876
784.655472	51654.609005	33.034893
785.225368	51745.657442	33.039911
785.726453	51823.989028	33.044928
787.075297	51897.811750	33.049946
787.330621	51988.296053	33.054964
788.250818	52079.662835	33.059981
788.902108	52152.635025	33.064999
789.546685	52236.402435	33.070016
790.810768	52296.972048	33.075034
791.096656	52382.630926	33.080052
791.806360	52445.110357	33.085069
792.453117	52527.455353	33.090087
793.477244	52606.249943	33.095104
794.668263	52684.115648	33.100122
795.298638	52756.642274	33.105140
796.099099	52832.680223	33.110157
796.567721	52911.368873	33.115175
797.612892	52996.089191	33.120192
798.378327	53076.937526	33.125210
799.373310	53144.872152	33.130228
800.910089	53199.720133	33.135245
802.235039	53266.040346	33.140263
803.109418	53324.857420	33.145280
803.791431	53382.351250	33.150298
804.359831	53444.234833	33.155316
805.158923	53497.054836	33.160333
806.226786	53556.785609	33.165351
806.704979	53635.270717	33.170368
807.631607	53698.540602	33.175386
808.438312	53768.950553	33.180404
809.067631	53839.471076	33.185421
809.664136	53906.474563	33.190439
810.015278	53977.529135	33.195456
811.063219	54050.793049	33.200474
811.816739	54121.342243	33.205492
813.064208	54184.512256	33.210509
813.833095	54262.751794	33.215527
814.501111	54332.873514	33.220544
815.509386	54402.527852	33.225562
815.768511	54481.165105	33.230580
816.769185	54566.067127	33.235597
817.274225	54643.561166	33.240615
817.487669	54727.033063	33.245632
818.531922	54809.694458	33.250650
819.138269	54902.716311	33.255668
819.912804	54988.552751	33.260685
820.907925	55075.108914	33.265703
821.783695	55183.401947	33.270720
822.750594	55255.783970	33.275738
823.059397	55364.427149	33.280756
824.042526	55448.142852	33.285773
824.748251	55555.941145	33.290791
825.187295	55654.233520	33.295808
826.327734	55749.134975	33.300826
826.814126	55847.515551	33.305844
827.807403	55941.286060	33.310861
829.131456	56049.635978	33.315879
829.962581	56149.510119	33.320896
830.596255	56235.889372	33.325914
831.700309	56340.797237	33.330932
832.927437	56410.320216	33.335949
834.301261	56499.067333	33.340967
835.013322	56557.731250	33.345984
836.077078	56618.495517	33.351002
836.705475	56702.393354	33.356020
837.317573	56770.124608	33.361037
838.042485	56837.825529	33.366055
838.727504	56926.349695	33.371072
839.557719	56985.595985	33.376090
839.943094	57088.510504	33.381108
840.669911	57158.302190	33.386125
842.003922	57243.722338	33.391143
842.320312	57335.382011	33.396160
843.281389	57417.446461	33.401178
844.118486	57503.464637	33.406196
844.940953	57598.653536	33.411213
845.755717	57682.611406	33.416231
846.338063	57775.676857	33.421248
847.480216	57867.037268	33.426266
847.800447	57950.424694	33.431284
848.785645	58062.884593	33.436301
850.349561	58141.917059	33.441319
850.773269	58246.874565	33.446336
852.241065	58324.199310	33.451354
853.017366	58418.206363	33.456372
853.859886	58513.447281	33.461389
855.022478	58581.375392	33.466407
855.877233	58669.246281	33.471424
857.096244	58742.132287	33.476442
857.494360	58840.078718	33.481460
858.558136	58917.820686	33.486477
859.710256	58993.629306	33.491495
859.897390	59090.467699	33.496512
860.701692	59169.991671	33.501530
861.874043	59266.579479	33.506548
862.034809	59353.212703	33.511565
862.967680	59449.757478	33.516583
863.535276	59551.674706	33.521600
864.687048	59634.893146	33.526618
865.386760	59750.929138	33.531636
866.028442	59844.039688	33.536653
867.216351	59933.852684	33.541671
867.825057	60052.787753	33.546688
868.799530	60145.202726	33.551706
869.574168	60257.993546	33.556724
870.364219	60356.109730	33.561741
871.116483	60467.512916	33.566759
872.084426	60576.056456	33.571776
872.704296	60680.592252	33.576794
873.585427	60797.436284	33.581812
874.091586	60913.860757	33.586829
875.214041	61013.158935	33.591847
875.920523	61146.903993	33.596864
877.043311	61240.150155	33.601882
877.740654	61367.320872	33.606900
878.294260	61471.344272	33.611917
879.530512	61587.811457	33.616935
880.088163	61697.487737	33.621952
881.236474	61788.664247	33.626970
882.285720	61903.596905	33.631988
883.192667	62008.688040	33.637005
884.048028	62113.904806	33.642023
884.793820	62218.523820	33.647040
886.351270	62301.837937	33.652058
887.167450	62408.846744	33.657076
887.995033	62502.922944	33.662093
888.967384	62599.417605	33.667111
889.847729	62709.582080	33.672128
891.231129	62792.202899	33.677146
891.761230	62887.957820	33.682164
892.451516	62991.885720	33.687181
893.608229	63084.131360	33.692199
894.313606	63196.802332	33.697216
894.922652	63299.952193	33.702234
895.992687	63398.434375	33.707252
897.049480	63503.983652	33.712269
897.923905	63608.340373	33.717287
898.946064	63710.018240	33.722304
900.256242	63793.466686	33.727322
901.208338	63896.637829	33.732340
901.829795	64004.577179	33.737357
903.011358	64102.669442	33.742375
903.837792	64198.030088	33.747392
904.506710	64291.695084	33.752410
905.399788	64400.705119	33.757428
906.365060	64493.884966	33.762445
907.513044	64590.879717	33.767463
908.219331	64703.537332	33.772480
909.160961	64799.738524	33.777498
910.092985	64910.504398	33.782516
910.682259	65010.280998	33.787533
911.804640	65110.816554	33.792551
912.613512	65215.530413	33.797568
913.404768	65319.685467	33.802586
914.308275	65435.916478	33.807604
914.810456	65541.296785	33.812621
916.048997	65651.756021	33.817639
916.696465	65765.013517	33.822656
917.939307	65876.420876	33.827674
918.788859	65981.517757	33.832692
919.534522	66103.390430	33.837709
920.785009	66211.930646	33.842727
921.450160	66331.894070	33.847744
922.223249	66445.694625	33.852762
923.082256	66563.774604	33.857780
923.828620	66671.614302	33.862797
925.176554	66789.952676	33.867815
925.729598	66916.857957	33.872832
926.615368	67029.743824	33.877850
928.108188	67147.328538	33.882868
929.049064	67261.634681	33.887885
930.309616	67358.170619	33.892903
931.191838	67457.275210	33.897920
932.099143	67546.268545	33.902938
932.965905	67650.228309	33.907956
934.004444	67743.023687	33.912973
934.804711	67843.034042	33.917991
935.589128	67937.942905	33.923008
936.784822	68031.226372	33.928026
937.837072	68129.321806	33.933044
938.840991	68220.722477	33.938061
939.994844	68314.860516	33.943079
941.025534	68399.188368	33.948096
942.083640	68494.662894	33.953114
943.446227	68578.085833	33.958132
944.503684	68651.026044	33.963149
946.013242	68718.783553	33.968167
946.645158	68806.897760	33.973184
947.420381	68885.487608	33.978202
948.630191	68964.987892	33.983220
949.135374	69056.749813	33.988237
949.901606	69138.450488	33.993255
950.881860	69222.474030	33.998272
951.614375	69318.092833	34.003290
952.169477	69417.903863	34.008308
953.172518	69508.950581	34.013325
954.323448	69603.998772	34.018343
954.899513	69704.913581	34.023360
955.572649	69815.549635	34.028378
956.665034	69915.050263	34.033396
957.083457	70039.160425	34.038413
958.276840	70146.171084	34.043431
959.088522	70255.157474	34.048448
959.879171	70372.468969	34.053466
960.915401	70485.218187	34.058484
961.476866	70608.923762	34.063501
962.607211	70724.742728	34.068519
963.249326	70855.797931	34.073536
964.103299	70987.527967	34.078554
965.235155	71105.434017	34.083572
965.928111	71249.348211	34.088589
966.888913	71386.592636	34.093607
967.775748	71518.156691	34.098624
968.734903	71644.901604	34.103642
969.719676	71774.992169	34.108660
970.623475	71911.876493	34.113677
972.086613	72038.044558	34.118695
973.076874	72172.256709	34.123712
974.178224	72301.801396	34.128730
975.450810	72431.622993	34.133748
976.148586	72555.312704	34.138765
976.988007	72690.019944	34.143783
978.357107	72811.260096	34.148800
979.333562	72934.857274	34.153818
980.755090	73046.744599	34.158836
981.491871	73165.932679	34.163853
982.655527	73268.756373	34.168871
983.753207	73388.495009	34.173888
984.590120	73493.608844	34.178906
985.927923	73585.531025	34.183924
986.847147	73694.892023	34.188941
987.919773	73794.377341	34.193959
988.810888	73892.419613	34.198976
989.842810	73999.053328	34.203994
990.695218	74101.829705	34.209012
991.493652	74221.304950	34.214029
992.437060	74321.982547	34.219047
993.205442	74429.355617	34.224064
994.088369	74549.779946	34.229082
995.250560	74652.522499	34.234100
996.028083	74773.969755	34.239117
997.324006	74871.257245	34.244135
998.375060	74988.687199	34.249152
999.476080	75105.439994	34.254170
1000.501031	75218.432645	34.259188
1001.308496	75340.441011	34.264205
1002.793840	75442.813877	34.269223
1003.866184	75552.236451	34.274240
1004.716482	75674.480176	34.279258
1005.710602	75774.114168	34.284276
1006.906494	75886.097444	34.289293
1007.761585	76007.931619	34.294311
1009.045938	76108.051970	34.299328
1009.688745	76216.130763	34.304346
1010.946075	76336.145934	34.309364
1011.544154	76450.629078	34.314381
1012.786500	76561.755472	34.319399
1014.171194	76671.128082	34.324416
1015.116905	76780.362540	34.329434
1016.571883	76888.069224	34.334452
1017.511278	76994.499615	34.339469
1018.301203	77091.796103	34.344487
1019.539251	77212.015444	34.349504
1020.675083	77306.072443	34.354522
1022.290255	77417.321179	34.359540
1022.983087	77514.199013	34.364557
1024.223984	77617.772072	34.369575
1024.937103	77714.932056	34.374592
1025.583587	77829.971455	34.379610
1026.428039	77932.161747	34.384628
1027.294962	78047.439091	34.389645
1028.045315	78172.545372	34.394663
1029.326431	78283.466396	34.399680
1030.073774	78400.130025	34.404698
1031.946697	78501.154559	34.409716
1032.623115	78618.646097	34.414733
1033.495939	78732.491517	34.419751
1034.940061	78843.326432	34.424768
1035.904998	78955.300084	34.429786
1037.172917	79052.852229	34.434804
1038.010465	79171.825690	34.439821
1038.703252	79272.011403	34.444839
1039.401824	79374.598694	34.449856
1040.269602	79481.900419	34.454874
1041.496963	79595.081066	34.459892
1042.194861	79712.979979	34.464909
1042.970667	79819.507937	34.469927
1043.954937	79932.052725	34.474944
1044.681243	80060.884874	34.479962
1045.671710	80181.426469	34.484980
1046.509796	80308.978114	34.489997
1047.532529	80440.192876	34.495015
1048.818315	80570.393126	34.500032
1049.662283	80698.989271	34.505050
1050.965264	80831.078545	34.510068
1051.920493	80955.473730	34.515085
1053.058929	81096.270370	34.520103
1054.642850	81208.366374	34.525120
1055.661293	81343.702910	34.530138
1056.879754	81457.577881	34.535156
1057.817366	81578.344600	34.540173
1058.949811	81704.732712	34.545191
1059.650006	81845.977103	34.550208
1060.716257	81971.587127	34.555226
1061.704591	82107.344323	34.560244
1062.627758	82249.434718	34.565261
1063.377588	82384.978768	34.570279
1064.488420	82531.789050	34.575296
1064.879222	82666.740851	34.580314
1066.768307	82822.836649	34.585332
1067.447814	82968.207592	34.590349
1068.908359	83117.406704	34.595367
1069.832968	83262.361364	34.600384
1070.364734	83416.369818	34.605402
1071.862241	83558.624286	34.610420
1072.783575	83715.399053	34.615437
1074.023089	83875.171797	34.620455
1075.607563	84013.508230	34.625472
1076.695950	84145.494461	34.630490
1078.282520	84281.948206	34.635508
1079.929152	84404.970393	34.640525
1081.067313	84537.899545	34.645543
1082.092048	84670.246915	34.650560
1083.030483	84809.917901	34.655578
1084.137627	84926.611354	34.660596
1085.111750	85071.165873	34.665613
1085.971825	85196.220906	34.670631
1087.339273	85329.858320	34.675648
1088.023650	85464.313375	34.680666
1088.954077	85600.057966	34.685684
1089.878214	85745.965480	34.690701
1090.766544	85883.476362	34.695719
1091.810879	86025.338892	34.700736
1092.289035	86188.772068	34.705754
1093.602390	86331.890087	34.710772
1094.910294	86481.427995	34.715789
1096.274775	86625.918310	34.720807
1097.777574	86743.880338	34.725824
1098.775576	86873.520283	34.730842
1100.039579	87000.317455	34.735860
1101.798409	87114.472078	34.740877
1102.763032	87228.348912	34.745895
1103.885198	87350.472395	34.750912
1105.114023	87474.185780	34.755930
1106.122251	87589.663763	34.760948
1107.051889	87708.202827	34.765965
1107.904631	87827.235365	34.770983
1109.302569	87950.412377	34.776000
1110.038889	88072.133359	34.781018
1111.193171	88202.780888	34.786036
1112.345189	88326.327986	34.791053
1113.285471	88460.457551	34.796071
1114.878138	88587.142228	34.801088
1115.736556	88719.376617	34.806106
1116.897130	88840.572808	34.811124
1118.052170	88978.857855	34.816141
1119.105554	89099.920764	34.821159
1120.489238	89220.685186	34.826176
1121.659129	89351.413043	34.831194
1122.156217	89493.809122	34.836212
1123.555146	89623.793893	34.841229
1124.728522	89755.491213	34.846247
1125.457745	89894.937552	34.851264
1126.544343	90026.587065	34.856282
1127.864826	90183.042000	34.861300
1129.019374	90304.234646	34.866317
1129.814506	90453.078345	34.871335
1131.498327	90581.600530	34.876352
1132.305532	90728.312851	34.881370
1133.754510	90868.903181	34.886388
1135.039820	91013.606087	34.891405
1136.608206	91145.229983	34.896423
1137.823848	91270.794863	34.901440
1138.730432	91412.221225	34.906458
1139.972017	91530.782077	34.911476
1141.435908	91656.980103	34.916493
1142.425832	91783.266869	34.921511
1143.652286	91911.154867	34.926528
1144.649679	92039.187553	34.931546
1145.732559	92179.831823	34.936564
1146.836325	92299.399077	34.941581
1147.593987	92438.167608	34.946599
1148.950290	92574.210623	34.951616
1149.714277	92722.037301	34.956634
1151.300170	92864.655243	34.961652
1152.354701	92991.242233	34.966669
1153.149936	93128.377229	34.971687
1154.370063	93275.325440	34.976704
1155.502449	93420.542812	34.981722
1157.099373	93551.525004	34.986740
1158.587822	93681.165277	34.991757
1159.444900	93799.767789	34.996775
1160.987194	93922.974374	35.001792
1161.711924	94046.602606	35.006810
1162.920200	94156.390493	35.011828
1164.066348	94284.602225	35.016845
1164.803570	94411.057969	35.021863
1165.850910	94544.992508	35.026880
1166.951793	94661.751722	35.031898
1167.986174	94792.381525	35.036916
1168.830245	94928.931527	35.041933
1169.764531	95088.335384	35.046951
1170.929440	95224.842494	35.051968
1171.939433	95370.749859	35.056986
1173.001550	95528.947265	35.062004
1174.327318	95673.193296	35.067021
1175.286166	95836.419359	35.072039
1176.688835	95986.481323	35.077056
1177.546438	96134.903956	35.082074
1178.678388	96292.905832	35.087092
1179.714548	96468.175252	35.092109
1180.636508	96622.796734	35.097127
1182.252929	96787.430718	35.102144
1183.272533	96956.791579	35.107162
1184.499154	97133.471904	35.112180
1185.742951	97295.321997	35.117197
1186.290147	97483.297980	35.122215
1187.594290	97644.388120	35.127232
1188.731193	97829.799572	35.132250
1190.015085	98006.711637	35.137268
1191.049578	98192.110677	35.142285
1192.179572	98375.003350	35.147303
1193.352016	98551.956329	35.152320
1194.507700	98745.008481	35.157338
1195.690006	98932.509452	35.162356
1196.865155	99114.110175	35.167373
1198.258991	99310.223019	35.172391
1199.697023	99486.584202	35.177408
1200.810221	99666.490862	35.182426
1202.139740	99856.430808	35.187444
1203.683892	100037.239872	35.192461
1204.781106	100220.310589	35.197479
1206.494251	100390.390072	35.202496
1208.017407	100581.361819	35.207514
1208.672990	100748.106788	35.212532
1210.477589	100914.448820	35.217549
1211.410081	101095.705058	35.222567
1212.693230	101266.042812	35.227584
1213.892624	101435.382737	35.232602
1215.109372	101607.011683	35.237620
1216.705131	101771.355588	35.242637
1217.861943	101946.280547	35.247655
1219.403606	102093.905201	35.252672
1220.941500	102257.825121	35.257690
1222.390367	102418.178858	35.262708
1224.048723	102562.965761	35.267725
1225.735265	102702.338819	35.272743
1227.533391	102814.896649	35.277760
1228.795625	102930.856007	35.282778
1230.103848	103049.194236	35.287796
1231.253548	103163.046463	35.292813
1232.225043	103281.110341	35.297831
1233.738457	103394.791964	35.302848
1234.394607	103514.944752	35.307866
1235.228266	103646.251574	35.312884
1236.192938	103762.901466	35.317901
1237.309164	103906.441273	35.322919
1238.379262	104045.977238	35.327936
1239.244677	104189.457382	35.332954
1240.312011	104330.102892	35.337972
1241.315183	104476.056190	35.342989
1242.188718	104646.394958	35.348007
1243.376290	104802.414596	35.353024
1244.423716	104972.658444	35.358042
1245.647584	105137.692470	35.363060
1247.053317	105302.350661	35.368077
1247.965741	105464.765841	35.373095
1249.322033	105642.882355	35.378112
1250.566056	105822.176181	35.383130
1251.540401	105994.546360	35.388148
1252.847549	106174.509954	35.393165
1253.610453	106364.769703	35.398183
1255.004180	106543.412246	35.403200
1256.431268	106735.512290	35.408218
1257.567995	106915.983191	35.413236
1259.247213	107090.128861	35.418253
1260.556269	107287.207635	35.423271
1261.684278	107473.494117	35.428288
1262.866717	107666.159444	35.433306
1263.899774	107846.014533	35.438324
1265.343945	108038.482986	35.443341
1266.371570	108242.753610	35.448359
1267.841373	108418.796602	35.453376
1269.126698	108609.111219	35.458394
1270.004738	108818.296708	35.463412
1271.540875	109011.315227	35.468429
1272.817833	109206.294311	35.473447
1274.268529	109395.253249	35.478464
1275.637961	109586.840688	35.483482
1277.340547	109780.630024	35.488500
1278.960667	109955.267679	35.493517
1279.517966	110157.863091	35.498535
1280.864115	110351.890827	35.503552
1282.559387	110543.826388	35.508570
1283.799206	110725.670032	35.513588
1285.686085	110899.487082	35.518605
1287.047171	111080.307604	35.523623
1288.273245	111254.466400	35.528640
1289.900636	111431.974540	35.533658
1291.238954	111611.327655	35.538676
1292.627350	111774.475223	35.543693
1294.062806	111950.226148	35.548711
1295.372224	112110.679150	35.553728
1296.441896	112256.617971	35.558746
1297.839563	112410.779243	35.563764
1298.895660	112562.406643	35.568781
1299.812092	112729.927478	35.573799
1301.056232	112885.610062	35.578816
1301.982849	113052.637667	35.583834
1303.669285	113213.664556	35.588852
1304.974355	113380.862096	35.593869
1305.650718	113563.588380	35.598887
1306.901985	113735.905642	35.603904
1308.451452	113912.544871	35.608922
1309.797472	114087.375431	35.613940
1311.280176	114252.125858	35.618957
1312.308818	114428.129776	35.623975
1313.853042	114607.224742	35.628992
1314.983187	114794.154831	35.634010
1315.926886	114975.240796	35.639028
1317.522399	115153.134922	35.644045
1318.627846	115350.816771	35.649063
1319.881450	115545.279401	35.654080
1321.455694	115731.860914	35.659098
1322.239675	115930.668328	35.664116
1323.453302	116122.989113	35.669133
1324.805216	116332.029331	35.674151
1326.234548	116521.988917	35.679168
1327.656492	116727.520000	35.684186
1328.929382	116933.304355	35.689204
1330.579680	117124.164011	35.694221
1331.628853	117340.795059	35.699239
1332.561569	117539.350716	35.704256
1334.409965	117732.830016	35.709274
1335.590037	117955.048934	35.714292
1337.022148	118167.098895	35.719309
1338.271957	118380.040695	35.724327
1339.660006	118580.583492	35.729344
1341.014030	118789.814292	35.734362
1342.296851	118998.798483	35.739380
1343.799953	119200.999424	35.744397
1345.205698	119417.717821	35.749415
1346.513686	119611.638966	35.754432
1348.853432	119809.386834	35.759450
1350.090503	120014.466836	35.764468
1351.674105	120209.222457	35.769485
1353.085210	120397.446681	35.774503
1354.500709	120592.092553	35.779520
1355.854504	120783.900099	35.784538
1356.743526	120977.467334	35.789556
1358.277824	121168.109154	35.794573
1359.577298	121371.416734	35.799591
1360.823221	121558.282355	35.804608
1362.746109	121755.794502	35.809626
1363.982495	121960.889776	35.814644
1365.389524	122149.291803	35.819661
1366.842105	122326.516940	35.824679
1368.257437	122497.416379	35.829696
1369.692978	122678.129609	35.834714
1370.694214	122849.185775	35.839732
1372.372979	123008.343466	35.844749
1373.679090	123191.879899	35.849767
1374.387009	123365.354512	35.854784
1376.013616	123543.928018	35.859802
1377.270082	123720.674275	35.864820
1378.796815	123907.005108	35.869837
1379.741266	124088.983878	35.874855
1381.214965	124279.239622	35.879872
1383.010007	124453.941819	35.884890
1384.216772	124644.546561	35.889908
1385.961634	124812.026420	35.894925
1387.188484	125013.903933	35.899943
1388.537834	125190.619744	35.904960
1390.694017	125370.463900	35.909978
1392.020459	125552.100486	35.914996
1393.387058	125716.441293	35.920013
1394.394317	125899.194959	35.925031
1395.884265	126101.165425	35.930048
1397.349078	126277.819292	35.935066
1398.468062	126458.620845	35.940084
1400.056686	126639.260294	35.945101
1401.465310	126827.124750	35.950119
1402.664127	127020.103588	35.955136
1404.334161	127199.986405	35.960154
1405.164056	127405.973072	35.965172
1406.548412	127603.334952	35.970189
1407.772575	127800.901054	35.975207
1409.462876	128003.043718	35.980224
1410.832562	128195.965645	35.985242
1411.724509	128413.110704	35.990260
1413.346058	128610.049369	35.995277
1414.750258	128827.863718	36.000295
1416.338922	129026.178766	36.005312
1418.059032	129217.544550	36.010330
1419.603202	129418.656585	36.015348
1421.212384	129622.052812	36.020365
1423.227205	129804.849631	36.025383
1425.730646	129973.203285	36.030400
1427.685764	130130.255527	36.035418
1429.614321	130303.960213	36.040436
1431.105869	130453.157000	36.045453
1432.847845	130601.123870	36.050471
1433.528754	130756.367658	36.055488
1434.966850	130920.690039	36.060506
1436.138096	131086.905536	36.065524
1437.200645	131254.862354	36.070541
1438.664242	131429.129316	36.075559
1439.786425	131599.447944	36.080576
1440.796909	131779.781873	36.085594
1441.927382	131956.854376	36.090612
1443.266522	132144.981109	36.095629
1444.714918	132322.486838	36.100647
1445.389399	132511.215734	36.105664
1446.793710	132671.575197	36.110682
1448.359125	132865.309008	36.115700
1449.190472	133059.008721	36.120717
1450.623705	133247.153116	36.125735
1451.587051	133432.484505	36.130752
1452.888040	133621.970114	36.135770
1454.258925	133842.438601	36.140788
1455.846080	134031.374610	36.145805
1457.475861	134238.500583	36.150823
1458.711739	134444.613588	36.155840
1460.377288	134642.398212	36.160858
1461.881090	134857.582143	36.165876
1463.254639	135079.770269	36.170893
1465.249948	135273.249241	36.175911
1466.209726	135488.435583	36.180928
1467.720076	135691.941526	36.185946
1468.771906	135925.097465	36.190964
1470.108177	136143.536134	36.195981
1471.594973	136366.007522	36.200999
1472.758645	136594.018905	36.206016
1474.758599	136820.517937	36.211034
1476.097248	137045.413034	36.216052
1477.478452	137279.896003	36.221069
1478.982354	137505.211884	36.226087
1480.310497	137750.453196	36.231104
1482.230137	137978.735358	36.236122
1483.368388	138215.558078	36.241140
1484.795067	138452.831099	36.246157
1486.528841	138690.285336	36.251175
1487.528610	138926.666815	36.256192
1489.461321	139168.921662	36.261210
1490.780564	139420.362610	36.266228
1492.264981	139662.388513	36.271245
1493.722731	139902.532267	36.276263
1495.196729	140162.889588	36.281280
1496.790794	140401.913072	36.286298
1498.412211	140661.757008	36.291316
1499.595789	140893.625576	36.296333
1501.240112	141153.672872	36.301351
1502.691866	141401.826731	36.306368
1504.493424	141645.883996	36.311386
1506.613094	141885.963671	36.316404
1508.744986	142118.159867	36.321421
1511.486471	142323.011007	36.326439
1513.208184	142530.775885	36.331456
1515.359927	142731.819706	36.336474
1517.073295	142925.545161	36.341492
1518.273974	143132.408256	36.346509
1520.062549	143320.547366	36.351527
1521.684522	143509.690056	36.356544
1522.848254	143706.625755	36.361562
1524.353717	143891.847374	36.366580
1525.833131	144095.402473	36.371597
1527.227117	144280.276541	36.376615
1528.116796	144478.591569	36.381632
1529.945424	144651.699512	36.386650
1531.571250	144832.090979	36.391668
1532.653016	145024.510240	36.396685
1534.208167	145203.102479	36.401703
1535.489036	145401.399250	36.406720
1536.711472	145595.498211	36.411738
1538.197435	145792.471948	36.416756
1539.473612	145989.226724	36.421773
1540.749578	146182.585600	36.426791
1541.729983	146411.054590	36.431808
1543.238950	146614.976294	36.436826
1544.610891	146841.649564	36.441844
1545.838214	147064.595232	36.446861
1547.475182	147298.772082	36.451879
1548.524323	147532.752466	36.456896
1550.070284	147761.686420	36.461914
1551.302174	148018.890235	36.466932
1552.835865	148263.979857	36.471949
1554.758391	148514.524040	36.476967
1556.320857	148754.060348	36.481984
1558.416724	149002.920114	36.487002
1560.054931	149238.594156	36.492020
1561.138030	149495.389697	36.497037
1563.088582	149727.328594	36.502055
1564.520385	149983.819066	36.507072
1565.860085	150234.811442	36.512090
1567.616595	150486.905891	36.517108
1568.902361	150742.462021	36.522125
1570.695837	150990.294748	36.527143
1572.376747	151253.056513	36.532160
1573.972238	151498.946763	36.537178
1575.635731	151753.297057	36.542196
1577.385050	152009.030287	36.547213
1579.642719	152250.535711	36.552231
1580.909249	152506.793210	36.557248
1582.506241	152741.865069	36.562266
1584.451186	152992.782326	36.567284
1586.553955	153223.821523	36.572301
1588.708391	153448.869717	36.577319
1589.976599	153699.620835	36.582336
1591.661445	153918.217134	36.587354
1593.302393	154156.651890	36.592372
1594.573221	154395.413381	36.597389
1596.189746	154629.810711	36.602407
1597.692780	154868.044172	36.607424
1599.302325	155098.756171	36.612442
1600.794602	155344.006407	36.617460
1602.182531	155581.096637	36.622477
1603.754937	155819.592023	36.627495
1605.328346	156059.090618	36.632512
1607.089296	156311.557973	36.637530
1608.711844	156549.543289	36.642548
1610.387845	156785.049153	36.647565
1611.999827	157006.098765	36.652583
1613.763466	157234.708475	36.657600
1615.442768	157457.221189	36.662618
1616.852115	157675.200591	36.667636
1618.537351	157888.788151	36.672653
1620.553754	158101.449475	36.677671
1621.980185	158331.007603	36.682688
1623.323341	158534.153904	36.687706
1624.995659	158749.384602	36.692724
1625.895545	158993.182436	36.697741
1627.550059	159219.869662	36.702759
1629.319801	159461.998214	36.707776
1630.888876	159684.276324	36.712794
1632.521109	159931.743321	36.717812
1634.247904	160168.658890	36.722829
1635.459510	160414.965978	36.727847
1636.817789	160642.774610	36.732864
1638.433847	160897.428606	36.737882
1640.224815	161140.034465	36.742900
1641.608595	161404.671356	36.747917
1643.255721	161657.829389	36.752935
1644.493248	161918.587298	36.757952
1646.146562	162189.845162	36.762970
1647.906443	162451.690717	36.767988
1649.407268	162726.033202	36.773005
1651.426064	162987.549825	36.778023
1653.240475	163260.350041	36.783040
1654.795017	163526.928432	36.788058
1656.540667	163799.312393	36.793076
1658.117255	164069.315524	36.798093
1659.831730	164327.947695	36.803111
1661.353475	164608.211142	36.808128
1663.053451	164883.273781	36.813146
1664.559419	165161.958567	36.818164
1666.163510	165444.041623	36.823181
1668.192181	165717.815312	36.828199
1669.547978	166008.528604	36.833216
1671.115932	166287.516369	36.838234
1672.807335	166566.435873	36.843252
1674.478836	166866.821248	36.848269
1676.207686	167152.639029	36.853287
1677.865086	167442.059829	36.858304
1679.764062	167739.397278	36.863322
1681.839136	168011.138182	36.868340
1683.050602	168303.287305	36.873357
1685.020809	168584.435163	36.878375
1687.044562	168863.027048	36.883392
1688.463720	169146.575063	36.888410
1690.474826	169420.733475	36.893428
1692.218808	169702.673817	36.898445
1694.143226	169969.911449	36.903463
1696.189925	170256.348850	36.908480
1697.908192	170527.517261	36.913498
1699.460858	170786.612464	36.918516
1701.347955	171071.305308	36.923533
1703.701202	171309.194420	36.928551
1705.392819	171552.340192	36.933568
1707.097967	171789.979934	36.938586
1708.800284	172005.143229	36.943604
1710.747404	172243.990440	36.948621
1712.596091	172454.375928	36.953639
1714.511930	172692.710706	36.958656
1716.414555	172908.100805	36.963674
1717.937412	173135.426125	36.968692
1719.352187	173383.168530	36.973709
1721.504734	173587.790493	36.978727
1723.453959	173816.269815	36.983744
1724.832721	174055.712849	36.988762
1726.260749	174276.640599	36.993780
1727.399144	174513.764912	36.998797
1729.255836	174757.906184	37.003815
1730.785759	175002.823917	37.008832
1732.180034	175253.803340	37.013850
1733.853292	175508.533239	37.018868
1735.218106	175772.409888	37.023885
1736.658093	176032.140481	37.028903
1738.426862	176297.491434	37.033920
1739.814859	176579.942799	37.038938
1741.574808	176851.870427	37.043956
1742.800336	177152.975707	37.048973
1744.069469	177433.548709	37.053991
1745.569776	177739.841628	37.059008
1746.795504	178040.712211	37.064026
1748.824305	178350.630330	37.069044
1750.384142	178672.817716	37.074061
1752.080517	178983.947802	37.079079
1754.113192	179302.474358	37.084096
1755.834908	179630.162381	37.089114
1757.837757	179939.728273	37.094132
1759.736602	180263.510576	37.099149
1761.123935	180581.654271	37.104167
1763.002914	180905.685619	37.109184
1765.077951	181235.765865	37.114202
1767.151464	181551.371624	37.119220
1768.694914	181871.327079	37.124237
1770.636789	182197.527745	37.129255
1772.987799	182512.525401	37.134272
1774.815236	182833.242147	37.139290
1776.970212	183131.069645	37.144308
1779.377753	183442.296420	37.149325
1781.481158	183732.319871	37.154343
1783.394610	184018.327599	37.159360
1785.399345	184294.552146	37.164378
1787.623663	184580.526798	37.169396
1789.379008	184880.459631	37.174413
1791.271419	185151.136721	37.179431
1792.974060	185418.736673	37.184448
1794.550626	185713.982974	37.189466
1797.087656	185974.867952	37.194484
1799.255333	186238.452469	37.199501
1800.857405	186493.930805	37.204519
1802.885323	186742.947370	37.209536
1804.387661	186986.807850	37.214554
1805.998829	187213.013527	37.219572
1807.849241	187472.861204	37.224589
1809.398213	187703.545970	37.229607
1811.130317	187951.220076	37.234624
1812.459157	188204.847690	37.239642
1814.335856	188456.207007	37.244660
1815.895331	188724.127960	37.249677
1817.759169	188977.585977	37.254695
1819.374990	189236.934960	37.259712
1820.795872	189522.179346	37.264730
1822.774277	189788.072788	37.269748
1823.806603	190073.179087	37.274765
1825.750706	190361.175411	37.279783
1827.413748	190642.098582	37.284800
1828.542326	190954.873245	37.289818
1830.180387	191251.248598	37.294836
1831.959634	191568.949510	37.299853
1833.336507	191882.426783	37.304871
1835.203220	192201.818509	37.309888
1837.032763	192518.299230	37.314906
1839.009508	192837.652220	37.319924
1840.408599	193181.237907	37.324941
1842.053037	193515.623793	37.329959
1844.215721	193851.630319	37.334976
1845.806684	194192.869935	37.339994
1847.722817	194531.902655	37.345012
1849.990455	194873.775576	37.350029
1851.946923	195208.580041	37.355047
1854.235625	195541.747472	37.360064
1856.165675	195877.372781	37.365082
1858.325834	196207.607679	37.370100
1860.182650	196548.833499	37.375117
1862.062458	196870.867182	37.380135
1864.625713	197188.352055	37.385152
1866.451641	197527.850316	37.390170
1868.291201	197849.858316	37.395188
1869.919938	198183.045827	37.400205
1871.700535	198517.087117	37.405223
1873.258429	198854.085173	37.410240
1874.776807	199191.700871	37.415258
1876.931637	199539.257766	37.420276
1878.731438	199873.075957	37.425293
1880.511635	200225.405802	37.430311
1882.763552	200552.721016	37.435328
1884.730675	200907.779998	37.440346
1886.682840	201244.984156	37.445364
1888.482375	201583.801262	37.450381
1890.790452	201918.630140	37.455399
1892.634706	202240.346051	37.460416
1894.418690	202590.380114	37.465434
1896.517533	202919.688364	37.470452
1898.587249	203251.986184	37.475469
1900.414011	203577.292116	37.480487
1902.836683	203882.410886	37.485504
1904.560715	204182.437624	37.490522
1906.581101	204482.317339	37.495540
1908.458417	204778.032260	37.500557
1910.290863	205091.210275	37.505575
1912.126400	205381.019405	37.510592
1913.607570	205703.370890	37.515610
1915.580790	206014.386153	37.520628
1917.194883	206332.061141	37.525645
1918.888405	206643.669945	37.530663
1920.836230	206969.572179	37.535680
1922.451788	207290.755725	37.540698
1924.553426	207633.432142	37.545716
1926.444059	207953.102967	37.550733
1928.777069	208267.487692	37.555751
1930.732903	208595.860190	37.560768
1932.487877	208928.290618	37.565786
1934.490343	209271.017322	37.570804
1936.144533	209597.018245	37.575821
1937.878018	209942.774672	37.580839
1940.118792	210262.998541	37.585856
1942.143067	210612.838456	37.590874
1944.105933	210957.116771	37.595892
1946.318759	211301.750838	37.600909
1948.426494	211623.335683	37.605927
1950.639687	211963.161637	37.610944
1952.484914	212305.421844	37.615962
1954.711218	212631.741047	37.620980
1956.934184	212963.178801	37.625997
1958.873873	213291.108336	37.631015
1960.993628	213621.042267	37.636032
1963.033808	213963.559459	37.641050
1965.085777	214287.641903	37.646068
1966.812600	214621.032944	37.651085
1968.850333	214949.297834	37.656103
1970.872512	215275.573469	37.661120
1972.440156	215613.565257	37.666138
1974.640484	215950.442611	37.671156
1976.271140	216292.973012	37.676173
1978.423119	216637.631563	37.681191
1980.737815	216968.160161	37.686208
1982.398509	217321.520950	37.691226
1984.455536	217648.436996	37.696244
1986.324852	217994.975327	37.701261
1988.270909	218343.966328	37.706279
1990.333120	218681.919745	37.711296
1991.924869	219053.126329	37.716314
1993.371087	219398.125993	37.721332
1995.563233	219754.233078	37.726349
1997.189375	220122.163765	37.731367
1999.232702	220468.978239	37.736384
2001.444263	220837.060807	37.741402
2003.777054	221186.448282	37.746420
2005.759098	221601.296857	37.751437
2007.880963	221949.908662	37.756455
2010.232740	222282.588385	37.761472
2012.071585	222614.690642	37.766490
2014.069026	222935.201696	37.771508
2016.243122	223262.377658	37.776525
2018.240109	223592.427343	37.781543
2020.083282	223921.283820	37.786560
2021.883506	224252.154703	37.791578
2023.636834	224586.018364	37.796596
2025.789961	224924.607061	37.801613
2027.438537	225272.940306	37.806631
2029.372991	225620.543982	37.811648
2031.569335	225975.662884	37.816666
2033.291967	226326.261747	37.821684
2035.565658	226686.145860	37.826701
2037.328830	227043.522063	37.831719
2039.332006	227401.598184	37.836736
2041.276380	227781.957900	37.841754
2043.030416	228138.933754	37.846772
2045.427666	228511.859785	37.851789
2047.220502	228883.257876	37.856807
2049.582845	229255.456070	37.861824
2051.402465	229641.989671	37.866842
2053.393578	230016.205478	37.871860
2056.259047	230394.347690	37.876877
2058.163165	230768.631171	37.881895
2060.470405	231140.896609	37.886912
2062.704294	231511.244949	37.891930
2064.616162	231892.693827	37.896948
2067.048543	232250.543301	37.901965
2069.240171	232630.731656	37.906983
2071.513811	232999.225418	37.912000
2072.939532	233368.058256	37.917018
2075.142816	233738.877185	37.922036
2077.766798	234118.647155	37.927053
2079.664275	234496.019366	37.932071
2081.849668	234869.131167	37.937088
2083.752223	235242.035209	37.942106
2085.926755	235619.215229	37.947124
2087.923689	235992.995956	37.952141
2089.794584	236382.138901	37.957159
2091.934183	236764.281343	37.962176
2094.195807	237143.510304	37.967194
2096.333498	237518.036016	37.972212
2099.132212	237886.946539	37.977229
2101.119514	238261.905026	37.982247
2103.588993	238629.676473	37.987264
2105.770193	239001.050766	37.992282
2107.619058	239363.360551	37.997300
2110.273217	239724.730963	38.002317
2112.069410	240095.052268	38.007335
2114.337874	240458.238700	38.012352
2116.805766	240821.318414	38.017370
2118.954056	241172.892956	38.022388
2121.623226	241525.020904	38.027405
2123.327606	241870.267068	38.032423
2125.617671	242187.912970	38.037440
2127.267889	242520.266267	38.042458
2128.988147	242842.830231	38.047476
2131.375160	243178.827632	38.052493
2133.203636	243517.606933	38.057511
2135.204968	243843.405471	38.062528
2137.115066	244196.804239	38.067546
2139.012848	244538.267625	38.072564
2141.331339	244882.078214	38.077581
2143.229509	245242.441391	38.082599
2145.385379	245585.746121	38.087616
2147.327302	245946.205788	38.092634
2149.609076	246308.365139	38.097652
2151.438356	246661.986241	38.102669
2153.381350	247039.111522	38.107687
2155.786720	247416.189844	38.112704
2157.639786	247785.202938	38.117722
2159.391072	248154.614093	38.122740
2161.852020	248532.727838	38.127757
2163.889796	248915.989883	38.132775
2166.111998	249293.203479	38.137792
2168.488993	249684.262616	38.142810
2170.576121	250074.860632	38.147828
2172.780836	250462.494342	38.152845
2174.739897	250861.471634	38.157863
2177.163023	251264.211925	38.162880
2179.143886	251655.287674	38.167898
2181.135227	252067.446134	38.172916
2183.271091	252470.869780	38.177933
2185.006851	252883.781879	38.182951
2187.479546	253290.557761	38.187968
2189.620689	253711.180399	38.192986
2191.223566	254125.386371	38.198004
2193.338854	254560.265510	38.203021
2195.432443	255006.808639	38.208039
2197.650013	255430.725065	38.213056
2200.303328	255865.166009	38.218074
2203.102469	256287.086746	38.223092
2206.162470	256698.018491	38.228109
2208.503829	257119.251324	38.233127
2210.870922	257523.461172	38.238144
2213.488841	257911.856966	38.243162
2216.079559	258322.154719	38.248180
2219.080134	258697.840605	38.253197
2221.342650	259090.613051	38.258215
2223.531389	259468.206980	38.263232
2225.958918	259849.497782	38.268250
2227.699122	260225.360298	38.273268
2230.403367	260609.910634	38.278285
2232.594104	260995.990867	38.283303
2234.753335	261377.300861	38.288320
2236.764383	261752.893776	38.293338
2238.988789	262134.448403	38.298356
2241.111826	262511.320008	38.303373
2243.134168	262900.630064	38.308391
2245.387199	263262.773572	38.313408
2247.515330	263616.452643	38.318426
2249.361263	263985.317021	38.323444
2251.160348	264345.094884	38.328461
2253.333163	264716.346832	38.333479
2255.681339	265090.467275	38.338496
2257.565643	265457.091459	38.343514
2259.632250	265843.603132	38.348532
2262.022078	266229.911469	38.353549
2263.906755	266606.138923	38.358567
2266.144969	266999.457791	38.363584
2268.293797	267398.075002	38.368602
2270.408008	267803.506065	38.373620
2273.027598	268195.063303	38.378637
2274.930243	268600.045784	38.383655
2277.207466	269007.814299	38.388672
2279.494370	269415.378289	38.393690
2281.468639	269830.943309	38.398708
2284.039491	270247.252268	38.403725
2286.200109	270676.074108	38.408743
2288.453627	271089.410749	38.413760
2290.785351	271520.796954	38.418778
2293.131782	271939.987348	38.423796
2295.735749	272362.845935	38.428813
2298.279814	272796.408958	38.433831
2300.535079	273216.833489	38.438848
2303.030102	273644.714086	38.443866
2305.339867	274062.843788	38.448884
2307.767921	274487.153205	38.453901
2310.192697	274927.772149	38.458919
2312.408812	275347.745784	38.463936
2315.310987	275762.733183	38.468954
2317.539419	276191.113330	38.473972
2319.563494	276610.456794	38.478989
2322.303842	277041.702444	38.484007
2324.575076	277468.678376	38.489024
2327.003293	277897.712381	38.494042
2329.141975	278332.152257	38.499060
2331.689200	278750.726313	38.504077
2333.872849	279179.163528	38.509095
2335.948654	279617.626559	38.514112
2338.781993	280039.431715	38.519130
2341.130601	280468.019955	38.524148
2343.480185	280890.815833	38.529165
2345.878585	281320.513399	38.534183
2347.968146	281755.365682	38.539200
2350.498754	282184.686033	38.544218
2352.922124	282613.718212	38.549236
2355.347124	283041.606635	38.554253
2357.814384	283470.681940	38.559271
2359.761655	283906.596516	38.564288
2362.358446	284323.711010	38.569306
2364.601068	284756.986805	38.574324
2366.973937	285194.687036	38.579341
2369.275944	285620.179145	38.584359
2371.550214	286043.287286	38.589376
2373.416638	286446.060975	38.594394
2375.550040	286868.479181	38.599412
2377.926163	287274.016246	38.604429
2380.286411	287695.533748	38.609447
2382.381927	288116.025727	38.614464
2384.905040	288532.740544	38.619482
2386.943216	288965.052742	38.624500
2389.199591	289400.124010	38.629517
2391.428167	289841.041631	38.634535
2393.764680	290287.021961	38.639552
2396.036801	290729.760207	38.644570
2398.008476	291184.179685	38.649588
2400.186139	291634.196453	38.654605
2402.698177	292103.973326	38.659623
2404.687916	292575.686419	38.664640
2407.461717	293045.013468	38.669658
2410.034562	293520.645755	38.674676
2412.206113	294002.818181	38.679693
2414.464691	294472.884270	38.684711
2416.905038	294966.519082	38.689728
2419.127778	295452.795170	38.694746
2421.473411	295950.964132	38.699764
2424.270663	296448.018757	38.704781
2426.880257	296947.489588	38.709799
2429.125559	297449.379166	38.714816
2431.470060	297947.060337	38.719834
2434.189857	298448.389273	38.724852
2436.775745	298942.117494	38.729869
2439.276331	299447.974318	38.734887
2442.059278	299952.921201	38.739904
2444.639493	300451.116476	38.744922
2447.061166	300960.207064	38.749940
2449.418251	301459.425159	38.754957
2452.596770	301943.931215	38.759975
2455.107496	302461.258063	38.764992
2457.664374	302927.545286	38.770010
2460.103513	303433.144803	38.775028
2463.024418	303923.501925	38.780045
2465.733535	304412.011242	38.785063
2468.351147	304895.072199	38.790080
2471.074031	305369.173779	38.795098
2473.312280	305858.590715	38.800116
2475.956029	306336.155828	38.805133
2478.786415	306812.521195	38.810151
2481.194268	307290.323341	38.815168
2483.577475	307754.132159	38.820186
2485.811464	308237.825631	38.825204
2488.257921	308719.426135	38.830221
2490.808156	309207.510596	38.835239
2493.288057	309689.381286	38.840256
2496.072705	310161.676885	38.845274
2498.163726	310660.445045	38.850292
2500.738710	311137.062344	38.855309
2503.081084	311606.272514	38.860327
2505.397434	312062.937671	38.865344
2508.140878	312510.922999	38.870362
2510.667580	312960.058364	38.875380
2512.848682	313409.906968	38.880397
2515.449674	313865.782809	38.885415
2517.754840	314310.909146	38.890432
2520.521651	314769.066018	38.895450
2522.967974	315226.865238	38.900468
2525.287675	315684.682444	38.905485
2528.228512	316139.071989	38.910503
2530.724063	316594.647502	38.915520
2533.650356	317039.282363	38.920538
2535.899166	317504.467692	38.925556
2538.550998	317971.872689	38.930573
2540.930017	318435.610564	38.935591
2543.408682	318903.368532	38.940608
2545.841848	319359.854974	38.945626
2547.921129	319841.385951	38.950644
2550.441444	320328.431828	38.955661
2553.079929	320812.154750	38.960679
2554.996603	321300.002061	38.965696
2557.549483	321798.158450	38.970714
2560.093858	322308.655972	38.975732
2562.373776	322825.338243	38.980749
2565.085697	323334.330109	38.985767
2567.190830	323858.144656	38.990784
2569.492459	324366.611131	38.995802
2572.003010	324896.754607	39.000820
2574.277008	325441.585269	39.005837
2577.400828	325971.243629	39.010855
2580.248654	326519.531395	39.015872
2582.721508	327051.926747	39.020890
2585.386240	327587.944915	39.025908
2588.209475	328113.547880	39.030925
2590.756872	328663.137835	39.035943
2593.213064	329203.545550	39.040960
2596.199126	329743.129007	39.045978
2598.565833	330284.381071	39.050996
2601.134088	330839.106639	39.056013
2603.653339	331387.842889	39.061031
2605.891045	331947.817981	39.066048
2608.365991	332497.949385	39.071066
2610.903491	333065.714627	39.076084
2613.723506	333619.083672	39.081101
2616.632522	334187.695058	39.086119
2619.051805	334745.943104	39.091136
2622.076496	335298.275903	39.096154
2625.135041	335872.232632	39.101172
2627.434100	336435.284780	39.106189
2630.395907	336989.695660	39.111207
2632.753975	337552.627344	39.116224
2635.210444	338123.460537	39.121242
2638.193651	338680.265742	39.126260
2640.931139	339237.257352	39.131277
2643.652811	339788.178292	39.136295
2645.945817	340335.226834	39.141312
2648.560775	340852.158021	39.146330
2651.461444	341376.961188	39.151348
2653.487811	341908.271071	39.156365
2656.163900	342437.670772	39.161383
2658.569677	342976.197878	39.166400
2661.615194	343509.794957	39.171418
2664.112433	344039.868909	39.176436
2666.439968	344579.790221	39.181453
2669.027055	345129.592152	39.186471
2671.334845	345687.024046	39.191488
2674.519864	346235.146710	39.196506
2677.035857	346805.660094	39.201524
2679.506335	347371.757598	39.206541
2682.917220	347920.818264	39.211559
2685.782275	348473.844102	39.216576
2688.476350	349025.444475	39.221594
2691.034885	349596.633379	39.226612
2693.671884	350160.797408	39.231629
2696.661604	350724.391985	39.236647
2698.660295	351298.850143	39.241664
2701.788557	351870.635502	39.246682
2704.370316	352442.247379	39.251700
2706.998949	353030.218523	39.256717
2709.915184	353606.435428	39.261735
2712.430477	354194.868242	39.266752
2714.962776	354785.880735	39.271770
2717.957727	355371.254187	39.276788
2721.029270	355951.862131	39.281805
2724.283938	356523.322003	39.286823
2726.221359	357121.635355	39.291840
2729.389701	357704.136620	39.296858
2732.336712	358286.691410	39.301876
2735.082233	358878.789181	39.306893
2738.393767	359458.886355	39.311911
2740.870658	360037.966565	39.316928
2743.687376	360623.001125	39.321946
2746.602765	361211.286892	39.326964
2749.547372	361781.794795	39.331981
2753.085260	362363.800258	39.336999
2755.010460	362948.718616	39.342016
2757.632323	363520.398367	39.347034
2760.464653	364101.859190	39.352052
2762.865901	364698.252516	39.357069
2765.921971	365273.267611	39.362087
2768.970561	365863.503105	39.367104
2771.940463	366436.106070	39.372122
2775.019352	367022.134180	39.377140
2777.986437	367598.605238	39.382157
2780.892999	368163.836617	39.387175
2783.466066	368747.485656	39.392192
2787.062533	369306.325096	39.397210
2789.442464	369872.378850	39.402228
2791.819748	370451.316009	39.407245
2794.799978	371005.358860	39.412263
2797.090948	371547.450808	39.417280
2799.642666	372101.141131	39.422298
2802.263505	372635.656113	39.427316
2804.833218	373183.620163	39.432333
2807.025394	373736.178486	39.437351
2809.529020	374304.614069	39.442368
2811.819924	374874.902234	39.447386
2814.205137	375458.868286	39.452404
2816.842366	376045.094814	39.457421
2819.447211	376649.052337	39.462439
2822.013150	377259.248094	39.467456
2824.557188	377868.144060	39.472474
2826.943470	378503.694048	39.477492
2829.199808	379145.114676	39.482509
2831.948325	379775.081487	39.487527
2834.670780	380446.519973	39.492544
2837.001315	381109.028452	39.497562
2840.188493	381771.795740	39.502580
2842.761777	382441.979826	39.507597
2845.610478	383123.701099	39.512615
2848.708381	383809.556010	39.517632
2851.816112	384490.704065	39.522650
2854.781615	385173.713808	39.527668
2857.698435	385865.215881	39.532685
2860.780046	386550.464508	39.537703
2863.562014	387240.287835	39.542720
2866.905900	387936.451406	39.547738
2870.299071	388634.166208	39.552756
2873.024707	389325.429511	39.557773
2876.089979	390017.183568	39.562791
2879.070346	390716.343090	39.567808
2882.090630	391399.783861	39.572826
2885.270330	392085.798149	39.577844
2887.870836	392784.824180	39.582861
2891.136527	393472.851500	39.587879
2894.297482	394166.257702	39.592896
2897.327901	394846.889754	39.597914
2900.282675	395533.453881	39.602932
2902.923257	396223.223431	39.607949
2906.973064	396891.785498	39.612967
2910.624781	397558.647552	39.617984
2913.548929	398210.980936	39.623002
2916.944020	398870.072842	39.628020
2920.198882	399535.461714	39.633037
2923.141547	400180.856400	39.638055
2926.084841	400832.956935	39.643072
2928.476259	401479.046807	39.648090
2931.557657	402138.502221	39.653108
2934.450556	402792.421671	39.658125
2937.411407	403438.483171	39.663143
2939.961495	404104.345169	39.668160
2942.713736	404752.136644	39.673178
2946.018178	405420.234282	39.678196
2948.540857	406087.021711	39.683213
2951.485401	406732.536089	39.688231
2953.803379	407361.101789	39.693248
2956.515356	407999.300590	39.698266
2959.332539	408624.795576	39.703284
2962.062095	409254.803327	39.708301
2964.969751	409888.140850	39.713319
2967.514329	410536.856840	39.718336
2970.763609	411183.242192	39.723354
2973.652681	411838.769342	39.728372
2976.615229	412492.572295	39.733389
2979.784196	413140.194892	39.738407
2983.058103	413786.899580	39.743424
2986.500107	414430.775657	39.748442
2989.854842	415079.897105	39.753460
2992.570401	415730.296192	39.758477
2995.992661	416362.956788	39.763495
2998.866958	417029.215498	39.768512
3001.505676	417677.403312	39.773530
3004.325586	418348.226278	39.778548
3006.827392	419021.516176	39.783565
3009.547539	419689.485116	39.788583
3012.582002	420371.019914	39.793600
3015.202609	421058.456335	39.798618
3018.425333	421759.005914	39.803636
3020.926467	422466.517816	39.808653
3023.823207	423180.915985	39.813671
3026.567734	423891.874134	39.818688
3029.706331	424618.382120	39.823706
3032.831410	425337.171585	39.828724
3035.411354	426081.258924	39.833741
3038.862812	426799.349684	39.838759
3042.248971	427539.089230	39.843776
3044.965337	428272.606972	39.848794
3048.208891	429020.281349	39.853812
3051.105875	429768.090619	39.858829
3054.501611	430510.227483	39.863847
3057.167264	431254.915443	39.868864
3060.072199	432011.802132	39.873882
3063.454555	432772.719157	39.878900
3065.956569	433530.789894	39.883917
3069.078056	434308.138416	39.888935
3073.000378	435056.113301	39.893952
3076.260584	435824.454236	39.898970
3079.783663	436552.974821	39.903988
3083.094549	437307.791120	39.909005
3086.424258	438050.605071	39.914023
3089.882150	438792.692887	39.919040
3092.918966	439543.737260	39.924058
3096.569393	440271.520918	39.929076
3099.162198	441022.894087	39.934093
3102.402831	441750.192177	39.939111
3105.434979	442501.247640	39.944128
3108.084336	443261.099286	39.949146
3111.185139	444000.958574	39.954164
3114.230347	444760.295095	39.959181
3117.069633	445491.593660	39.964199
3120.067670	446214.289180	39.969216
3123.074415	446925.166265	39.974234
3126.007183	447625.403247	39.979252
3128.989946	448364.031252	39.984269
3132.413241	449064.046307	39.989287
3135.254934	449786.706975	39.994304
3137.708171	450518.415868	39.999322
3140.844070	451251.663756	40.004340
3143.919019	451996.740836	40.009357
3146.692995	452747.458862	40.014375
3149.495645	453500.829784	40.019392
3152.362713	454261.300903	40.024410
3155.479682	455030.765014	40.029428
3158.133894	455832.307330	40.034445
3161.378475	456611.564429	40.039463
3164.349341	457410.571103	40.044480
3167.088277	458212.621468	40.049498
3170.215110	459022.575353	40.054516
3173.428251	459848.726153	40.059533
3176.396983	460669.724065	40.064551
3179.811431	461503.723166	40.069568
3183.399405	462316.972419	40.074586
3186.859050	463157.173405	40.079604
3190.284056	463989.506526	40.084621
3193.425004	464827.567873	40.089639
3197.153761	465669.549602	40.094656
3200.342964	466502.226332	40.099674
3203.703089	467331.353427	40.104692
3206.630608	468180.695044	40.109709
3210.475377	469007.656177	40.114727
3214.304937	469829.479316	40.119744
3217.086875	470669.083590	40.124762
3220.962957	471486.939766	40.129780
3223.585766	472322.658774	40.134797
3227.479321	473149.041621	40.139815
3231.009648	473979.341432	40.144832
3234.249198	474793.272669	40.149850
3237.572303	475635.216015	40.154868
3240.897577	476453.212153	40.159885
3244.363213	477279.999098	40.164903
3247.319022	478108.247745	40.169920
3250.351260	478928.008438	40.174938
3253.584765	479752.555609	40.179956
3257.014244	480592.452742	40.184973
3259.975407	481432.640656	40.189991
3263.416048	482256.544367	40.195008
3266.363454	483099.543265	40.200026
3269.716125	483946.029289	40.205044
3272.797307	484786.507826	40.210061
3276.404633	485619.539619	40.215079
3279.544587	486467.110345	40.220096
3282.406307	487313.171611	40.225114
3285.992710	488160.697288	40.230132
3288.913989	489017.686912	40.235149
3291.657370	489861.126790	40.240167
3294.973577	490693.021556	40.245184
3297.730514	491512.995948	40.250202
3300.798923	492331.723175	40.255220
3304.010562	493170.746761	40.260237
3307.136109	494005.351710	40.265255
3310.289381	494843.500197	40.270272
3313.292900	495699.865282	40.275290
3316.060805	496544.915445	40.280308
3319.151875	497425.324392	40.285325
3321.974744	498293.311142	40.290343
3325.126751	499181.956451	40.295360
3328.204212	500078.950868	40.300378
3331.919534	500966.762167	40.305396
3335.125114	501875.611468	40.310413
3338.095251	502804.391866	40.315431
3341.477551	503720.236428	40.320448
3344.310327	504659.894766	40.325466
3347.415048	505606.627000	40.330484
3351.242150	506549.408254	40.335501
3354.767863	507496.879522	40.340519
3358.426990	508444.631018	40.345536
3361.916643	509411.734923	40.350554
3365.509262	510343.849508	40.355572
3368.881725	511308.341678	40.360589
3372.543324	512267.233861	40.365607
3376.640032	513213.036841	40.370624
3379.801607	514172.505321	40.375642
3383.651487	515117.433047	40.380660
3387.620575	516055.831787	40.385677
3390.787755	516999.701514	40.390695
3394.794678	517953.421825	40.395712
3398.079158	518896.307406	40.400730
3401.353531	519833.189610	40.405748
3405.379990	520764.806056	40.410765
3408.525954	521715.065217	40.415783
3412.734612	522637.418665	40.420800
3416.002671	523572.826206	40.425818
3420.274644	524476.358830	40.430836
3423.988590	525411.135320	40.435853
3427.483496	526326.281819	40.440871
3431.097301	527224.974233	40.445888
3434.234208	528159.731227	40.450906
3437.753644	529055.864920	40.455924
3440.771634	529972.489275	40.460941
3444.126070	530899.489520	40.465959
3447.795353	531809.956705	40.470976
3451.137263	532742.040167	40.475994
3454.358937	533658.466477	40.481012
3458.296924	534576.589559	40.486029
3461.597522	535481.105215	40.491047
3465.197044	536384.109773	40.496064
3468.815910	537335.973028	40.501082
3472.405422	538218.166309	40.506100
3475.753259	539144.571369	40.511117
3479.257542	540030.643055	40.516122
3482.805998	540888.787838	40.521127
3485.596183	541693.383075	40.526132
3488.253862	542447.115167	40.531136
3491.434091	543123.888245	40.536141
3493.627392	543752.726670	40.541146
3496.569076	544340.530545	40.546151
3498.948894	544851.267548	40.551156
3501.343826	545297.372958	40.556160
3503.524904	545722.702411	40.561165
3505.459893	546046.552908	40.566170
3507.316856	546345.524795	40.571175
3508.772092	546596.705324	40.576180
3510.202221	546822.295896	40.581184
3511.846305	546974.563782	40.586189
3512.492886	547125.019330	40.591194
3514.267865	547195.550401	40.596199
3514.897520	547258.287682	40.601204
3516.257420	547294.260591	40.606208
3516.582056	547288.354657	40.611213
3517.470636	547262.524440	40.616218
3518.495481	547201.897901	40.621223
3518.636210	547141.461301	40.626228
3519.182574	547034.929995	40.631232
3519.807751	546917.937688	40.636237
3520.130103	546801.799872	40.641242
3520.343853	546643.078897	40.646247
3520.638014	546496.810539	40.651252
3520.939296	546323.283454	40.656256
3521.251664	546125.675985	40.661261
3521.105392	545941.716320	40.666266
3522.038170	545728.913255	40.671271
3521.741534	545527.002568	40.676276
3521.532242	545310.891048	40.681280
3521.599553	545093.117345	40.686285
3521.759717	544850.893745	40.691290
3521.916158	544613.361440	40.696295
3522.067464	544391.525740	40.701300
3522.168762	544134.609780	40.706304
3521.940666	543890.614525	40.711309
3521.455854	543643.172475	40.716314
3522.000610	543377.237773	40.721319
3521.705811	543126.627081	40.726324
3521.677079	542861.177693	40.731328
3521.516400	542603.721395	40.736333
3521.048483	542367.110222	40.741338
3521.123067	542101.580534	40.746343
3520.828124	541852.463170	40.751348
3520.599323	541594.343918	40.756352
3520.555590	541355.428159	40.761357
3520.044363	541108.756210	40.766362
3520.174843	540848.800151	40.771367
3519.971845	540608.281919	40.776372
3519.767584	540362.710591	40.781376
3519.675735	540109.290711	40.786381
3519.453226	539870.783619	40.791386
3519.305491	539627.615221	40.796391
3519.136332	539393.788397	40.801396
3519.110180	539155.794478	40.806400
3518.842052	538916.421079	40.811405
3518.415519	538695.046997	40.816410
3518.493711	538455.409596	40.821415
3518.325067	538220.807096	40.826420
3518.201927	538007.202811	40.831424
3517.648098	537781.088306	40.836429
3517.566779	537566.511670	40.841434
3517.732011	537345.428463	40.846439
3517.007006	537128.169632	40.851444
3517.067303	536907.096663	40.856448
3517.168246	536689.044483	40.861453
3516.622758	536482.607061	40.866458
3516.215936	536284.276751	40.871463
3516.377062	536080.500189	40.876468
3516.235578	535891.214443	40.881472
3515.989713	535694.770432	40.886477
3515.956012	535500.209786	40.891482
3515.619960	535306.452131	40.896487
3515.085272	535123.886568	40.901492
3514.756998	534936.083428	40.906496
3514.959783	534756.276177	40.911501
3514.772686	534583.852935	40.916506
3514.862120	534405.726465	40.921511
3514.791610	534232.422131	40.926516
3514.567179	534053.229872	40.931520
3514.325049	533882.171412	40.936525
3514.283345	533715.575360	40.941530
3514.236970	533528.821924	40.946535
3513.757097	533378.810595	40.951540
3513.793971	533217.299049	40.956544
3513.814138	533058.617509	40.961549
3513.245106	532904.675227	40.966554
3513.651155	532747.192503	40.971559
3513.234811	532592.768324	40.976564
3513.151357	532440.664475	40.981568
3512.642054	532284.584744	40.986573
3512.575875	532140.508100	40.991578
3512.899884	531999.652399	40.996583
3512.556118	531862.892243	41.001588
3512.451049	531728.972975	41.006592
3512.192030	531576.231638	41.011597
3511.911957	531444.308001	41.016602
3511.942792	531309.050033	41.021607
3512.207935	531177.896899	41.026612
3511.680659	531042.724830	41.031616
3511.604730	530919.757991	41.036621
3511.557586	530794.663546	41.041626
3511.395767	530668.828329	41.046631
3510.902588	530556.737232	41.051636
3511.083265	530428.471200	41.056640
3511.301121	530315.760740	41.061645
3510.751438	530202.513907	41.066650
3510.528722	530085.980774	41.071655
3510.394285	529993.080224	41.076660
3510.602879	529872.232941	41.081664
3510.434978	529772.717081	41.086669
3510.143576	529673.169578	41.091674
3510.411194	529571.511903	41.096679
3510.002140	529464.654831	41.101684
3509.974957	529359.353665	41.106688
3510.074122	529260.853506	41.111693
3509.941215	529165.320221	41.116698
3509.783174	529064.484515	41.121703
3509.685776	528977.534846	41.126708
3509.875179	528881.645715	41.131712
3509.888775	528789.927449	41.136717
3509.582583	528701.392218	41.141722
3509.812005	528606.303616	41.146727
3509.407409	528505.048506	41.151732
3509.397951	528420.709610	41.156736
3509.502738	528332.056827	41.161741
3509.157247	528258.736028	41.166746
3509.307874	528167.447303	41.171751
3508.985939	528081.235673	41.176756
3508.847786	527994.287038	41.181760
3508.828719	527917.224016	41.186765
3508.601734	527841.052581	41.191770
3508.852351	527759.448514	41.196775
3508.754997	527684.468699	41.201780
3508.616181	527609.292937	41.206784
3508.539822	527544.618527	41.211789
3508.511701	527461.641961	41.216794
3508.285858	527392.290643	41.221799
3508.505864	527328.882478	41.226804
3508.181836	527251.864421	41.231808
3508.219207	527184.289942	41.236813
3507.967673	527129.799577	41.241818
3508.146656	527053.812896	41.246823
3508.057367	526990.047957	41.251828
3507.966415	526931.336864	41.256832
3508.124750	526872.384003	41.261837
3507.825133	526802.081537	41.266842
3508.046086	526735.335298	41.271847
3507.670024	526683.642730	41.276852
3508.046628	526619.196207	41.281856
3508.116371	526549.440726	41.286861
3507.660295	526491.998667	41.291866
3507.841740	526422.730375	41.296871
3507.516346	526376.284959	41.301876
3507.449605	526315.091303	41.306880
3507.644220	526256.585295	41.311885
3507.320929	526206.955001	41.316890
3507.303203	526148.128369	41.321895
3507.052856	526110.211720	41.326900
3507.138637	526051.621079	41.331904
3507.285149	526006.464619	41.336909
3507.145144	525971.411056	41.341914
3507.099670	525897.627621	41.346919
3507.160088	525855.617923	41.351924
3507.137278	525811.144713	41.356928
3507.227917	525767.361039	41.361933
3507.121350	525723.760038	41.366938
3507.014579	525662.418582	41.371943
3506.952315	525612.492476	41.376948
3507.319409	525571.949842	41.381952
3507.068236	525514.067540	41.386957
3506.990897	525473.999239	41.391962
3507.152699	525427.524611	41.396967
3506.975176	525379.334460	41.401972
3506.776113	525334.331804	41.406976
3506.727014	525292.641197	41.411981
3506.697514	525251.654996	41.416986
3506.973890	525203.847476	41.421991
3506.620447	525164.125299	41.426996
3506.628502	525121.970319	41.432000
3506.740238	525084.853266	41.437005
3506.675852	525045.742187	41.442010
3506.676443	525010.462122	41.447015
3506.614430	524959.523054	41.452020
3506.523500	524926.430686	41.457024
3506.692117	524885.462784	41.462029
3506.513036	524855.467436	41.467034
3506.498875	524806.441027	41.472039
3506.226075	524778.482150	41.477044
3506.205941	524754.021461	41.482048
3506.258130	524710.544250	41.487053
3506.200764	524689.930797	41.492058
3506.302250	524641.744881	41.497063
3506.203085	524608.147703	41.502068
3505.967675	524580.536392	41.507072
3505.951464	524552.031112	41.512077
3505.793236	524521.475840	41.517082
3506.068566	524495.198953	41.522087
3506.083081	524471.440003	41.527092
3505.828781	524436.350599	41.532096
3506.218974	524406.719362	41.537101
3506.066798	524386.625967	41.542106
3506.169803	524363.055058	41.547111
3505.891520	524335.803928	41.552116
3505.993190	524292.722139	41.557120
3506.102191	524259.748442	41.562125
3505.851584	524243.764716	41.567130
3506.330925	524213.007003	41.572135
3505.905552	524185.374488	41.577140
3506.071931	524162.046004	41.582144
3506.110991	524131.812642	41.587149
3505.914392	524098.280345	41.592154
3505.956257	524071.079264	41.597159
3506.027918	524047.816132	41.602164
3505.857472	524015.189383	41.607168
3506.001849	523999.547371	41.612173
3505.699357	523973.512596	41.617178
3505.874921	523931.833500	41.622183
3505.880682	523918.487969	41.627188
3505.798161	523888.172269	41.632192
3505.791351	523866.639908	41.637197
3505.293131	523836.339259	41.642202
3505.784178	523812.857864	41.647207
3505.651098	523802.465975	41.652212
3505.731372	523780.717544	41.657216
3505.431402	523751.497467	41.662221
3505.336367	523749.642209	41.667226
3505.567429	523708.105410	41.672231
3505.586569	523702.036573	41.677236
3505.585339	523671.101035	41.682240
3505.890625	523650.732230	41.687245
3505.647874	523631.713730	41.692250
3505.706127	523598.999446	41.697255
3505.761569	523582.259010	41.702260
3505.540211	523562.175520	41.707264
3505.773051	523545.811402	41.712269
3505.332567	523513.529608	41.717274
3505.419075	523489.302890	41.722279
3505.648292	523471.776638	41.727284
3505.538896	523460.015955	41.732288
3505.848563	523433.327518	41.737293
3505.457020	523410.490518	41.742298
3505.743257	523398.717814	41.747303
3505.722793	523386.791374	41.752308
3505.631160	523361.733276	41.757312
3505.733161	523332.398363	41.762317
3505.515626	523308.421624	41.767322
3505.836352	523285.876279	41.772327
3505.448555	523257.680184	41.777332
3505.378447	523246.873585	41.782336
3505.524083	523212.223808	41.787341
3505.439060	523207.232800	41.792346
3505.799569	523187.107434	41.797351
3505.777921	523166.840239	41.802356
3505.647883	523132.840463	41.807360
3505.691625	523118.628913	41.812365
3505.379431	523099.064706	41.817370
3505.458830	523073.574728	41.822375
3505.733707	523052.097864	41.827380
3505.603631	523037.155453	41.832384
3505.928514	523005.459393	41.837389
3505.584895	522998.992666	41.842394
3505.710302	522961.110300	41.847399
3505.548632	522941.471563	41.852404
3505.347867	522915.520104	41.857408
3505.720760	522907.979633	41.862413
3505.271898	522884.594886	41.867418
3505.443328	522862.476955	41.872423
3505.362013	522843.634218	41.877428
3505.315865	522825.341966	41.882432
3505.491339	522818.944783	41.887437
3505.514311	522797.254636	41.892442
3505.485031	522782.852126	41.897447
3505.452449	522762.687256	41.902452
3505.494395	522744.229334	41.907456
3505.239723	522724.908341	41.912461
3504.958647	522731.979449	41.917466
3505.434112	522695.052169	41.922471
3505.444061	522680.744472	41.927476
3505.078952	522665.990518	41.932480
3505.332303	522635.012764	41.937485
3505.383951	522647.137065	41.942490
3505.500658	522622.752622	41.947495
3505.174551	522601.471246	41.952500
3505.162635	522586.408641	41.957504
3505.132726	522564.726540	41.962509
3505.270609	522557.020840	41.967514
3505.565577	522541.201963	41.972519
3505.337069	522524.353652	41.977524
3505.207832	522516.690149	41.982528
3505.412842	522486.124168	41.987533
3504.996860	522476.888288	41.992538
3505.408355	522465.954502	41.997543
3505.322284	522452.420065	42.002548
3505.460456	522436.676419	42.007552
3505.747461	522406.956724	42.012557
3505.628463	522398.027731	42.017562
3505.437818	522367.827373	42.022567
3505.378936	522348.879410	42.027572
3505.035555	522332.554581	42.032576
3505.430545	522303.879241	42.037581
3505.394605	522302.418900	42.042586
3505.605737	522272.710950	42.047591
3505.235756	522264.074314	42.052596
3505.382663	522246.812512	42.057600
3505.367764	522221.386650	42.062605
3505.400760	522216.174471	42.067610
3505.465469	522189.826021	42.072615
3505.612276	522166.699968	42.077620
3505.138438	522156.461981	42.082624
3504.963655	522138.644264	42.087629
3505.352398	522126.399457	42.092634
3505.243535	522100.533275	42.097639
3505.126820	522097.012985	42.102644
3505.257114	522084.657332	42.107648
3505.390045	522057.539581	42.112653
3504.927058	522069.492879	42.117658
3504.984948	522050.627220	42.122663
3505.287547	522022.926507	42.127668
3504.944343	522018.683687	42.132672
3504.970666	522018.831202	42.137677
3504.929676	521988.606487	42.142682
3505.175781	521970.823175	42.147687
3504.918996	521986.687154	42.152692
3504.917522	521953.271230	42.157696
3505.134298	521947.625488	42.162701
3505.221212	521937.349294	42.167706
3505.599182	521927.178757	42.172711
3505.398135	521913.055392	42.177716
3505.309808	521889.005576	42.182720
3505.345468	521875.956961	42.187725
3505.075243	521865.636056	42.192730
3505.624791	521845.024165	42.197735
3505.606921	521822.833628	42.202740
3505.356763	521801.741415	42.207744
3505.420068	521787.020062	42.212749
3505.379951	521782.072071	42.217754
3505.515566	521755.003947	42.222759
3505.643832	521740.019511	42.227764
3505.529438	521716.832990	42.232768
3505.524444	521700.150717	42.237773
3505.490097	521679.175903	42.242778
3505.787786	521655.115290	42.247783
3505.576810	521631.337252	42.252788
3505.323544	521629.203426	42.257792
3505.316079	521586.182239	42.262797
3505.174741	521563.606420	42.267802
3504.956535	521564.399247	42.272807
3505.156045	521539.949539	42.277812
3505.084605	521520.395930	42.282816
3505.080533	521517.514932	42.287821
3505.130069	521514.473794	42.292826
3505.397712	521492.237683	42.297831
3505.366234	521477.682697	42.302836
3505.193477	521461.228914	42.307840
3505.695601	521451.038460	42.312845
3505.288425	521436.694479	42.317850
3505.185490	521421.796846	42.322855
3505.143115	521405.069622	42.327860
3504.973838	521383.660750	42.332864
3504.910151	521371.992438	42.337869
3504.993154	521380.624378	42.342874
3505.321121	521354.384637	42.347879
3505.290595	521345.036635	42.352884
3504.970781	521331.639317	42.357888
3505.089866	521303.966384	42.362893
3505.033609	521290.224042	42.367898
3504.956023	521298.982516	42.372903
3504.790282	521288.998624	42.377908
3505.103802	521257.098728	42.382912
3505.201040	521246.062124	42.387917
3504.840304	521252.236449	42.392922
3505.171339	521238.129518	42.397927
3505.100156	521222.620010	42.402932
3504.884156	521215.323498	42.407936
3505.193459	521205.011695	42.412941
3504.605747	521177.955815	42.417946
3505.289257	521166.523164	42.422951
3505.076386	521167.466836	42.427956
3505.156724	521147.838237	42.432960
3505.210190	521133.775083	42.437965
3505.016013	521134.260794	42.442970
3505.442069	521116.144772	42.447975
3505.299431	521090.787889	42.452980
3505.016254	521078.244035	42.457984
3505.208243	521050.306366	42.462989
3505.297765	521051.910050	42.467994
3505.315843	521045.233706	42.472999
3505.198210	521024.422882	42.478004
3505.286318	521013.286450	42.483008
3505.189297	520982.462039	42.488013
3505.025995	520971.314753	42.493018
3505.218965	520962.790681	42.498023
3505.148846	520949.151357	42.503028
3505.011075	520935.421599	42.508032
3505.022736	520926.117247	42.513037
3504.838842	520907.541262	42.518042
3505.214231	520882.911102	42.523047
3504.933372	520895.038702	42.528052
3505.054126	520876.869551	42.533056
3505.081847	520860.332920	42.538061
3504.924976	520855.908674	42.543066
3505.334959	520852.962120	42.548071
3505.138447	520822.153130	42.553076
3505.160128	520814.768317	42.558080
3504.974113	520810.803682	42.563085
3504.776457	520804.211892	42.568090
3505.284503	520773.645364	42.573095
3504.809747	520791.718931	42.578100
3504.745841	520778.482943	42.583104
3505.228307	520774.008190	42.588109
3505.104728	520746.372663	42.593114
3504.873437	520739.128912	42.598119
3504.875478	520736.802945	42.603124
3504.867710	520715.772132	42.608128
3505.076587	520705.627561	42.613133
3505.189664	520703.840178	42.618138
3505.058309	520680.705421	42.623143
3505.049735	520675.145413	42.628148
3504.808454	520662.139595	42.633152
3505.330475	520653.462242	42.638157
3504.908172	520641.142271	42.643162
3505.096092	520626.652967	42.648167
3504.980992	520623.536567	42.653172
3504.669052	520601.694191	42.658176
3504.871527	520580.983886	42.663181
3505.027506	520588.290196	42.668186
3505.159724	520565.416970	42.673191
3505.064841	520562.701830	42.678196
3504.680707	520546.381646	42.683200
3505.352986	520533.281904	42.688205
3505.095229	520534.788848	42.693210
3505.101806	520506.272852	42.698215
3505.063098	520498.240179	42.703220
3504.702339	520492.735769	42.708224
3505.331557	520489.147800	42.713229
3505.124478	520469.917720	42.718234
3505.213627	520450.236332	42.723239
3505.249742	520433.647384	42.728244
3504.860773	520415.153808	42.733248
3504.896943	520413.681901	42.738253
3504.660795	520419.179584	42.743258
3505.180833	520403.373625	42.748263
3504.955166	520382.225144	42.753268
3505.215632	520375.611337	42.758272
3505.285719	520367.713083	42.763277
3504.965602	520338.945073	42.768282
3505.262699	520323.376507	42.773287
3505.119659	520320.163346	42.778292
3504.695564	520310.876952	42.783296
3505.105719	520300.700320	42.788301
3504.702024	520302.938177	42.793306
3505.036370	520290.144445	42.798311
3505.018316	520266.333925	42.803316
3504.959162	520254.765217	42.808321
3504.925867	520261.646554	42.813325
3504.437814	520245.089695	42.818330
3504.704418	520215.874827	42.823335
3504.524457	520211.605733	42.828340
3504.533247	520211.402120	42.833345
3504.768090	520206.561874	42.838349
3504.747154	520221.631899	42.843354
3505.171965	520217.115549	42.848359
3504.925390	520190.914184	42.853364
3505.276583	520177.612107	42.858369
3505.246111	520176.100151	42.863373
3504.858567	520159.881239	42.868378
3505.110834	520149.223870	42.873383
3504.849345	520142.136304	42.878388
3504.570473	520126.557459	42.883393
3505.354659	520116.473280	42.888397
3504.812147	520108.014440	42.893402
3504.854032	520098.199244	42.898407
3504.669504	520098.632899	42.903412
3504.954042	520088.475988	42.908417
3505.110991	520071.513658	42.913421
3504.972911	520069.968139	42.918426
3504.933966	520053.744588	42.923431
3504.716875	520042.402930	42.928436
3504.865661	520035.907756	42.933441
3505.119031	520024.845654	42.938445
3504.912728	520022.805312	42.943450
3504.875464	520006.884809	42.948455
3504.593798	519995.856684	42.953460
3504.682227	519987.399187	42.958465
3504.739738	519984.305945	42.963469
3504.910055	519992.368658	42.968474
3505.095884	519971.862454	42.973479
3504.957820	519963.642981	42.978484
3504.472636	519959.523178	42.983489
3504.743751	519958.620822	42.988493
3504.841287	519951.880914	42.993498
3504.707884	519927.734210	42.998503
3504.867343	519919.316013	43.003508
3504.600053	519911.521419	43.008513
3505.107541	519902.694288	43.013517
3504.779197	519909.824643	43.018522
3505.210905	519887.257061	43.023527
3504.976500	519863.834072	43.028532
3504.983872	519872.428201	43.033537
3504.830774	519856.273055	43.038541
3504.748720	519838.235925	43.043546
3504.679704	519828.943700	43.048551
3504.593225	519845.794050	43.053556
3504.608093	519838.915479	43.058561
3504.832309	519828.009533	43.063565
3504.460186	519819.776418	43.068570
3504.985274	519799.165821	43.073575
3505.038157	519798.651870	43.078580
3504.746876	519787.625124	43.083585
3504.929247	519794.523133	43.088589
3505.028856	519781.159374	43.093594
3504.782209	519756.019101	43.098599
3505.003079	519749.866348	43.103604
3505.012397	519749.814328	43.108609
3504.897866	519721.771154	43.113613
3505.044827	519719.624383	43.118618
3505.171021	519711.261897	43.123623
3504.994230	519702.188877	43.128628
3504.996099	519678.273232	43.133633
3505.146003	519669.451929	43.138637
3505.080000	519669.209568	43.143642
3505.021439	519644.393325	43.148647
3505.088317	519637.557011	43.153652
3505.032491	519632.661413	43.158657
3505.188590	519611.603284	43.163661
3504.761058	519606.260810	43.168666
3505.174256	519590.521517	43.173671
3505.299140	519583.827698	43.178676
3505.014427	519565.063875	43.183681
3505.390178	519548.116987	43.188685
3504.805781	519545.175672	43.193690
3504.865396	519526.863002	43.198695
3504.986906	519524.012367	43.203700
3504.778103	519527.028510	43.208705
3505.208018	519507.494382	43.213709
3504.561254	519505.321340	43.218714
3504.807341	519488.192635	43.223719
3505.107255	519478.487974	43.228724
3504.754897	519484.004334	43.233729
3504.919617	519451.467138	43.238733
3504.871247	519445.407385	43.243738
3504.906558	519445.553503	43.248743
3504.835510	519435.856882	43.253748
3504.951095	519422.035250	43.258753
3505.002852	519411.510217	43.263757
3504.703153	519412.922766	43.268762
3505.176971	519390.196162	43.273767
3504.972626	519388.357679	43.278772
3504.761550	519372.969649	43.283777
3504.890566	519368.247007	43.288781
3504.541708	519370.678569	43.293786
3504.965829	519358.021610	43.298791
3505.170608	519335.084638	43.303796
3505.146059	519329.981758	43.308801
3505.075265	519323.065947	43.313805
3504.495614	519310.719275	43.318810
3504.796018	519298.688570	43.323815
3504.849764	519281.033863	43.328820
3504.630693	519289.158462	43.333825
3504.824536	519278.358077	43.338829
3504.539172	519284.015603	43.343834
3504.933048	519261.453142	43.348839
3504.988606	519260.685940	43.353844
3504.467070	519261.931312	43.358849
3505.016446	519248.849975	43.363853
3504.944571	519239.456743	43.368858
3504.692482	519214.013124	43.373863
3504.860886	519211.357273	43.378868
3504.724790	519204.906795	43.383873
3504.688149	519210.525038	43.388877
3504.481845	519205.956468	43.393882
3504.694079	519187.872114	43.398887
3504.638591	519165.683915	43.403892
3504.643884	519169.829228	43.408897
3504.727219	519159.905794	43.413901
3504.660353	519163.506324	43.418906
3504.830041	519164.288522	43.423911
3505.026998	519156.369635	43.428916
3505.056448	519138.162426	43.433921
3505.032493	519127.092986	43.438925
3505.007058	519128.715028	43.443930
3504.898115	519108.355458	43.448935
3504.719063	519089.726082	43.453940
3504.647648	519080.585500	43.458945
3504.870875	519074.027620	43.463949
3504.753540	519080.315978	43.468954
3504.614213	519064.511817	43.473959
3504.683064	519057.219883	43.478964
3504.782362	519042.743189	43.483969
3505.051556	519036.835348	43.488973
3504.691339	519053.628646	43.493978
3504.916637	519019.867511	43.498983
3504.854875	519014.467035	43.503988
3504.631568	519012.227001	43.508993
3504.899028	518990.897664	43.513997
3504.896562	519007.432216	43.519002
3504.484927	518991.620457	43.524007
3504.679043	518966.156499	43.529012
3504.580453	518966.526036	43.534017
3504.873120	518965.266279	43.539021
3504.810409	518975.237161	43.544026
3504.932064	518961.717563	43.549031
3504.667661	518942.899256	43.554036
3504.428077	518934.290804	43.559041
3504.652591	518927.682099	43.564045
3504.612766	518934.008826	43.569050
3504.487974	518928.163213	43.574055
3504.789316	518924.525603	43.579060
3504.458695	518927.510544	43.584065
3504.664672	518919.539554	43.589069
3504.534258	518916.829756	43.594074
3504.465164	518898.789545	43.599079
3504.534451	518899.385370	43.604084
3504.511345	518898.428330	43.609089
3505.096263	518906.223800	43.614093
3504.822643	518909.604243	43.619098
3504.646369	518891.833782	43.624103
3504.659921	518882.831352	43.629108
3504.546740	518874.910781	43.634113
3504.749429	518859.254624	43.639117
3504.588283	518869.544509	43.644122
3504.632945	518860.587714	43.649127
3504.824801	518865.462072	43.654132
3504.514653	518848.825120	43.659137
3504.672227	518836.614396	43.664141
3504.443116	518826.386196	43.669146
3504.675530	518831.557537	43.674151
3504.718669	518835.039625	43.679156
3504.654721	518832.319308	43.684161
3504.703125	518827.508123	43.689165
3504.430262	518828.158025	43.694170
3504.648344	518825.595389	43.699175
3504.960510	518793.842610	43.704180
3504.422992	518790.489236	43.709185
3504.787192	518783.757270	43.714189
3504.716929	518785.538122	43.719194
3504.608713	518796.375888	43.724199
3504.706106	518789.534400	43.729204
3504.568754	518755.223271	43.734209
3504.625323	518773.821848	43.739213
3504.616904	518771.193872	43.744218
3504.588230	518757.141662	43.749223
3504.833180	518752.501649	43.754228
3504.384753	518769.005794	43.759233
3504.972211	518751.417862	43.764237
3504.432154	518730.064117	43.769242
3504.613641	518719.619266	43.774247
3504.911663	518721.645304	43.779252
3504.263224	518721.697234	43.784257
3504.659472	518717.387248	43.789261
3504.606188	518724.474643	43.794266
3504.595544	518720.785167	43.799271
3505.113971	518715.646847	43.804276
3504.757189	518699.371062	43.809281
3504.890584	518681.045791	43.814285
3504.457024	518680.406427	43.819290
3504.687460	518676.223764	43.824295
3504.803378	518679.947204	43.829300
3504.348113	518658.681093	43.834305
3504.955329	518623.190169	43.839309
3504.701159	518648.714740	43.844314
3504.557517	518637.866144	43.849319
3504.875992	518630.433442	43.854324
3504.480887	518652.592474	43.859329
3504.964395	518618.031245	43.864333
3504.766968	518606.028149	43.869338
3504.955608	518599.627240	43.874343
3505.206947	518608.739681	43.879348
3504.901847	518604.085428	43.884353
3505.393896	518572.101536	43.889357
3504.696407	518579.341369	43.894362
3504.983121	518564.935764	43.899367
3504.888176	518539.516831	43.904372
3504.872582	518541.744149	43.909377
3505.105127	518532.150708	43.914381
3504.834116	518517.327560	43.919386
3504.789044	518493.923259	43.924391
3504.943406	518474.229198	43.929396
3504.739340	518480.834880	43.934401
3504.905146	518479.898524	43.939405
3504.688615	518473.409906	43.944410
3504.740493	518452.569026	43.949415
3504.932488	518441.717821	43.954420
3504.792284	518444.976143	43.959425
3505.091770	518448.266106	43.964429
3504.723562	518427.137631	43.969434
3504.992485	518405.807306	43.974439
3504.848528	518416.650971	43.979444
3504.512265	518420.901017	43.984449
3504.869786	518402.438886	43.989453
3504.887405	518383.474238	43.994458
3504.673841	518362.675196	43.999463
3504.542166	518360.926241	44.004468
3504.396179	518372.629862	44.009473
3504.561710	518359.760182	44.014477
3504.672601	518355.899722	44.019482
3504.910758	518354.901360	44.024487
3504.915116	518327.848322	44.029492
3504.543032	518328.109401	44.034497
3504.830354	518325.131224	44.039501
3505.051825	518331.366321	44.044506
3504.887403	518317.486886	44.049511
3505.139866	518311.278040	44.054516
3504.824116	518293.630106	44.059521
3504.854238	518276.938798	44.064525
3504.683275	518280.252579	44.069530
3504.851608	518254.589336	44.074535
3504.990827	518246.122918	44.079540
3504.731519	518255.366824	44.084545
3504.774879	518254.399242	44.089549
3504.607262	518226.361908	44.094554
3504.497200	518219.097880	44.099559
3504.780254	518213.086425	44.104564
3504.438587	518207.477093	44.109569
3504.855374	518208.776507	44.114573
3504.478880	518211.920522	44.119578
3504.818305	518203.776401	44.124583
3504.820711	518192.348208	44.129588
3504.538481	518183.442709	44.134593
3504.882165	518164.729671	44.139597
3504.545896	518177.221988	44.144602
3504.448822	518173.394353	44.149607
3504.622311	518171.900543	44.154612
3504.671011	518176.140377	44.159617
3504.585245	518169.428710	44.164621
3504.635215	518153.694889	44.169626
3504.596374	518138.581878	44.174631
3504.783357	518131.523695	44.179636
3504.383321	518148.172508	44.184641
3504.642217	518125.882657	44.189645
3504.659979	518145.651090	44.194650
3504.314641	518133.569893	44.199655
3504.415159	518144.476231	44.204660
3504.360425	518142.361132	44.209665
3504.927750	518117.595369	44.214669
3504.798657	518114.784097	44.219674
3504.559640	518098.034011	44.224679
3504.844356	518123.069701	44.229684
3504.698213	518091.944228	44.234689
3504.645251	518108.993322	44.239693
3504.915679	518075.880480	44.244698
3504.577587	518061.370918	44.249703
3504.553716	518076.139977	44.254708
3504.560341	518056.418201	44.259713
3504.699403	518057.053595	44.264717
3504.566328	518078.008966	44.269722
3504.414709	518065.947670	44.274727
3505.112551	518029.935491	44.279732
3504.694029	518053.059783	44.284737
3504.939405	518016.107761	44.289741
3504.502915	518030.992636	44.294746
3504.701101	518017.409604	44.299751
3504.623987	518015.955387	44.304756
3504.604411	518016.615854	44.309761
3504.619851	517986.071439	44.314765
3504.845435	518005.706062	44.319770
3504.695570	517998.903323	44.324775
3504.971733	517984.650580	44.329780
3504.675309	517983.635550	44.334785
3504.924408	517962.257220	44.339789
3504.820668	517955.548306	44.344794
3504.705765	517941.053932	44.349799
3504.649034	517933.730783	44.354804
3504.465963	517941.142424	44.359809
3504.838874	517928.492467	44.364813
3504.448473	517915.659736	44.369818
3504.510854	517915.953290	44.374823
3504.675545	517912.589888	44.379828
3504.617056	517916.796163	44.384833
3504.773345	517907.163845	44.389837
3504.982831	517903.692230	44.394842
3504.719234	517886.187316	44.399847
3505.166521	517867.558703	44.404852
3505.006287	517866.016475	44.409857
3504.904465	517863.049150	44.414861
3505.026640	517837.341988	44.419866
3504.733765	517832.533883	44.424871
3505.117973	517827.467070	44.429876
3504.893130	517826.289017	44.434881
3505.122428	517794.699115	44.439885
3505.258125	517777.636650	44.444890
3504.819166	517778.211707	44.449895
3505.127226	517758.694771	44.454900
3504.803476	517747.469517	44.459905
3505.170927	517733.910069	44.464909
3504.707218	517744.754140	44.469914
3505.240568	517694.203929	44.474919
3505.112875	517720.620152	44.479924
3505.002069	517706.883431	44.484929
3504.960535	517697.433957	44.489933
3504.766422	517673.445242	44.494938
3504.688446	517657.781737	44.499943
3504.636305	517670.735204	44.504948
3504.769737	517674.203268	44.509953
3504.565599	517662.554515	44.514957
3504.598644	517650.615433	44.519962
3504.738885	517624.449979	44.524967
3504.677941	517630.477139	44.529972
3504.487410	517621.961382	44.534977
3504.770956	517622.169421	44.539981
3504.373572	517626.884435	44.544986
3504.560866	517628.220167	44.549991
3504.566331	517629.888039	44.554996
3504.267768	517601.718638	44.560001
3504.662614	517587.497364	44.565005
3504.415362	517589.559152	44.570010
3504.297406	517593.623205	44.575015
3504.532164	517589.540720	44.580020
3504.443941	517596.684688	44.585025
3504.653215	517584.667140	44.590029
3504.582654	517595.449175	44.595034
3504.435212	517580.858492	44.600039
3504.440897	517597.393169	44.605044
3504.699639	517598.768179	44.610049
3504.711819	517574.746718	44.615053
3504.374906	517573.333520	44.620058
3504.435284	517529.481898	44.625063
3504.324479	517562.924606	44.630068
3504.493972	517529.169245	44.635073
3504.343675	517556.904061	44.640077
3504.451041	517549.200834	44.645082
3504.392482	517543.698235	44.650087
3504.505254	517547.119023	44.655092
3504.255271	517551.102816	44.660097
3504.922213	517556.205886	44.665101
3504.399557	517560.738446	44.670106
3504.303983	517565.405779	44.675111
3504.396081	517556.137375	44.680116
3504.396666	517560.132134	44.685121
3504.517462	517548.229677	44.690125
3504.382832	517549.060049	44.695130
3504.750423	517528.319812	44.700135
3504.746737	517519.471067	44.705140
3504.272888	517536.182726	44.710145
3504.552332	517525.822777	44.715149
3504.427876	517519.470934	44.720154
3504.427181	517535.854977	44.725159
3504.945316	517526.721496	44.730164
3504.649005	517522.368953	44.735169
3504.690737	517496.320001	44.740173
3504.830037	517493.112231	44.745178
3504.552259	517493.611255	44.750183
3504.874934	517468.731485	44.755188
3504.778067	517482.956363	44.760193
3504.928777	517477.976914	44.765197
3505.049118	517469.614219	44.770202
3504.877876	517442.638052	44.775207
3504.703495	517466.331392	44.780212
3504.886710	517448.199153	44.785217
3505.011464	517411.618821	44.790221
3504.750530	517410.345305	44.795226
3504.821971	517408.311308	44.800231
3505.094336	517392.845024	44.805236
3505.072564	517388.600761	44.810241
3505.424558	517375.346871	44.815245
3505.175630	517361.581124	44.820250
3504.999535	517345.123740	44.825255
3505.007346	517324.237835	44.830260
3505.070036	517317.097813	44.835265
3504.951776	517305.789214	44.840269
3504.560531	517285.370874	44.845274
3504.952403	517265.840113	44.850279
3504.823486	517283.660587	44.855284
3504.690789	517279.029279	44.860289
3504.878988	517262.210828	44.865293
3504.484598	517253.524826	44.870298
3504.655041	517244.294434	44.875303
3504.788757	517247.964817	44.880308
3504.709420	517240.695503	44.885313
3504.808373	517231.172991	44.890317
3504.452657	517221.520057	44.895322
3504.400987	517209.695183	44.900327
3504.760603	517202.305911	44.905332
3504.404243	517206.610010	44.910337
3504.541220	517197.738862	44.915341
3504.730310	517204.586328	44.920346
3504.903890	517189.337742	44.925351
3504.680017	517193.974887	44.930356
3504.134413	517178.182558	44.935361
3504.586697	517152.927850	44.940365
3504.498183	517160.830584	44.945370
3504.606453	517154.290113	44.950375
3504.592774	517163.748650	44.955380
3504.062590	517163.225630	44.960385
3504.423976	517155.684351	44.965389
3504.211383	517167.298212	44.970394
3504.417864	517162.360423	44.975399
3504.600944	517163.747428	44.980404
3504.434298	517168.122692	44.985409
3504.965561	517161.262530	44.990413
3504.358394	517168.134716	44.995418
3504.378398	517156.955870	45.000423
3504.803716	517135.194643	45.005428
3504.634663	517133.400896	45.010433
3504.690388	517119.081110	45.015437
3504.673461	517131.877726	45.020442
3504.473101	517132.870213	45.025447
3504.578923	517127.189790	45.030452
3504.143522	517135.046220	45.035457
3504.863960	517126.537943	45.040461
3504.526229	517112.432041	45.045466
3504.315598	517095.423608	45.050471
3504.378255	517089.598286	45.055476
3504.448122	517099.448208	45.060481
3504.598294	517092.749385	45.065485
3504.429869	517084.937823	45.070490
3504.568036	517084.713725	45.075495
3504.688341	517088.436831	45.080500
3504.447680	517099.195502	45.085505
3504.875004	517090.227842	45.090509
3504.659753	517096.684134	45.095514
3504.622919	517081.064151	45.100519
3504.573882	517068.733070	45.105524
3504.605290	517064.025197	45.110529
3504.840760	517061.712389	45.115533
3504.365585	517060.169290	45.120538
3504.516130	517057.971040	45.125543
3504.533338	517063.379226	45.130548
3504.370852	517064.618577	45.135553
3504.909434	517048.250225	45.140557
3504.710274	517031.593898	45.145562
3504.519660	517023.836383	45.150567
3504.664474	517024.622617	45.155572
3504.916004	517028.375567	45.160577
3504.846097	517026.768416	45.165581
3504.905863	517001.575513	45.170586
3504.782567	516994.414176	45.175591
3504.946051	516981.796597	45.180596
3504.922508	516992.268177	45.185601
3504.660159	516968.440933	45.190605
3504.688458	516951.344022	45.195610
3504.556462	516945.650552	45.200615
3504.662664	516936.227865	45.205620
3504.609800	516945.844428	45.210625
3504.831527	516944.090039	45.215629
3504.551506	516948.938403	45.220634
3504.708007	516921.252188	45.225639
3504.664741	516910.942858	45.230644
3504.458980	516910.621404	45.235649
3504.950622	516903.312272	45.240653
3504.659327	516918.276336	45.245658
3504.542013	516907.119024	45.250663
3504.566863	516899.681386	45.255668
3504.741043	516883.522171	45.260673
3504.628694	516857.243719	45.265677
3504.273813	516874.190089	45.270682
3504.630194	516868.217130	45.275687
3504.977679	516867.808239	45.280692
3504.594158	516866.402345	45.285697
3504.853908	516851.999515	45.290701
3504.792099	516834.006469	45.295706
3504.750323	516831.889155	45.300711
3504.736824	516824.609253	45.305716
3504.632457	516831.199834	45.310721
3504.860697	516816.093976	45.315725
3504.696222	516805.146328	45.320730
3504.654249	516785.279010	45.325735
3505.056096	516773.432720	45.330740
3504.631121	516782.905906	45.335745
3504.801478	516771.905319	45.340749
3504.847068	516769.774190	45.345754
3504.885714	516743.016563	45.350759
3504.950101	516742.804121	45.355764
3504.692286	516748.205304	45.360769
3504.753134	516746.071760	45.365773
3504.660209	516715.693841	45.370778
3504.705698	516706.432329	45.375783
3504.946493	516696.684814	45.380788
3504.472789	516694.180613	45.385793
3504.591006	516693.150540	45.390797
3504.856688	516696.041636	45.395802
3504.699215	516687.469603	45.400807
3504.570699	516670.801748	45.405812
3504.781669	516664.447136	45.410817
3504.923947	516655.777143	45.415821
3504.635417	516661.486630	45.420826
3504.507409	516656.399274	45.425831
3505.136689	516643.202120	45.430836
3504.682267	516630.479648	45.435841
3505.126733	516618.019668	45.440845
3504.763475	516621.060747	45.445850
3504.630635	516609.045991	45.450855
3504.699659	516585.974954	45.455860
3504.932876	516587.708078	45.460865
3505.012716	516576.114821	45.465869
3504.717063	516575.200720	45.470874
3504.485112	516577.513066	45.475879
3504.805476	516543.782429	45.480884
3504.913095	516537.595814	45.485889
3504.898571	516532.187061	45.490893
3504.950776	516532.381107	45.495898
3504.897685	516526.826735	45.500903
3504.656044	516501.073859	45.505908
3504.442616	516493.370272	45.510913
3505.056947	516494.588037	45.515917
3504.779794	516492.558449	45.520922
3504.649960	516490.556150	45.525927
3504.828953	516458.870516	45.530932
3504.430527	516457.568083	45.535937
3504.673919	516452.118542	45.540941
3504.423334	516455.748695	45.545946
3504.384574	516444.629228	45.550951
3504.726811	516439.821484	45.555956
3504.614686	516454.049654	45.560961
3504.996953	516443.369356	45.565965
3504.496295	516433.890581	45.570970
3504.730918	516422.727894	45.575975
3504.855853	516417.853344	45.580980
3504.599467	516429.322928	45.585985
3504.426629	516421.865748	45.590989
3504.619298	516409.040838	45.595994
3504.910868	516395.188866	45.600999
3504.650652	516377.631252	45.606004
3504.127744	516385.400721	45.611009
3504.628574	516373.032793	45.616013
3504.681401	516375.451873	45.621018
3504.602336	516377.588372	45.626023
3504.688255	516375.147391	45.631028
3504.271789	516381.231191	45.636033
3504.689081	516380.811257	45.641037
3504.470816	516362.387287	45.646042
3504.633975	516337.278180	45.651047
3504.798475	516343.067892	45.656052
3504.927649	516331.770095	45.661057
3504.754129	516334.528382	45.666061
3504.769269	516338.318849	45.671066
3504.522711	516311.150461	45.676071
3504.728947	516290.434182	45.681076
3504.737607	516300.243680	45.686081
3504.618419	516294.143391	45.691085
3504.762178	516293.362114	45.696090
3504.727010	516287.248544	45.701095
3504.545476	516279.034102	45.706100
3504.458995	516274.041209	45.711105
3504.745851	516253.716715	45.716109
3504.945166	516255.202374	45.721114
3504.621694	516249.892927	45.726119
3504.725846	516260.041358	45.731124
3504.804520	516245.464336	45.736129
3504.863632	516218.095772	45.741133
3504.841743	516220.678399	45.746138
3504.675263	516210.236392	45.751143
3504.663730	516210.743945	45.756148
3504.558720	516210.709983	45.761153
3504.819952	516198.177506	45.766157
3504.545561	516177.081900	45.771162
3504.353601	516181.815425	45.776167
3505.142349	516151.499420	45.781172
3504.754693	516173.458294	45.786177
3504.582192	516175.306154	45.791181
3504.613016	516185.415647	45.796186
3504.634929	516161.845750	45.801191
3504.705214	516137.813028	45.806196
3504.694384	516138.522760	45.811201
3504.743827	516128.653439	45.816205
3504.859252	516134.703840	45.821210
3504.651073	516132.663307	45.826215
3504.757560	516102.859615	45.831220
3504.689440	516113.743369	45.836225
3505.236241	516083.971199	45.841229
3504.868600	516084.787897	45.846234
3504.631997	516084.016151	45.851239
3504.801317	516051.471546	45.856244
3504.334996	516048.864934	45.861249
3504.727678	516044.251393	45.866253
3504.801809	516054.606983	45.871258
3504.499066	516045.754144	45.876263
3504.954746	516050.183063	45.881268
3504.522884	516032.095917	45.886273
3504.732262	516009.153616	45.891277
3504.555694	516014.946773	45.896282
3504.343056	516010.479461	45.901287
3504.741046	516005.106486	45.906292
3504.555089	516017.526095	45.911297
3504.557989	516006.298607	45.916301
3505.004661	516007.593479	45.921306
3504.702892	515980.483849	45.926311
3504.726185	515970.972575	45.931316
3504.588073	515968.212934	45.936321
3504.777188	515955.388238	45.941325
3504.647401	515971.996515	45.946330
3504.759677	515966.668683	45.951335
3504.641633	515924.004189	45.956340
3504.364085	515939.674972	45.961345
3504.933822	515928.661283	45.966349
3504.983961	515919.954897	45.971354
3504.614290	515921.631656	45.976359
3504.489349	515921.398553	45.981364
3504.270315	515923.456085	45.986369
3504.784357	515884.737397	45.991373
3504.372166	515886.876032	45.996378
3504.365896	515891.125139	46.001383
3504.664312	515876.715356	46.006388
3504.345691	515886.222814	46.011393
3504.252231	515875.971347	46.016397
3504.376439	515885.813401	46.021402
3504.507169	515897.171596	46.026407
3504.336786	515886.628857	46.031412
3504.146903	515887.265752	46.036417
3504.322308	515882.231352	46.041421
3504.121428	515894.147684	46.046426
3504.238594	515888.060465	46.051431
3504.717722	515891.474268	46.056436
3504.294011	515892.704417	46.061441
3504.437098	515890.406048	46.066445
3504.774997	515894.701906	46.071450
3504.712748	515892.891143	46.076455
3504.795958	515861.624093	46.081460
3504.637181	515859.778009	46.086465
3504.578436	515852.656551	46.091469
3504.526935	515847.860292	46.096474
3504.368249	515852.841515	46.101479
3504.734197	515842.820859	46.106484
3504.301994	515854.065760	46.111489
3504.583175	515849.621506	46.116493
3504.565344	515847.955437	46.121498
3504.591876	515827.519848	46.126503
3504.774689	515808.728440	46.131508
3504.517142	515799.160307	46.136513
3504.709009	515808.131974	46.141517
3504.617657	515813.051994	46.146522
3504.706686	515809.700128	46.151527
3505.011567	515797.211024	46.156532
3504.558480	515787.218631	46.161537
3504.654650	515785.079382	46.166541
3504.678195	515784.367653	46.171546
3504.567688	515780.946170	46.176551
3504.690349	515783.000290	46.181556
3504.530319	515782.418720	46.186561
3504.657272	515766.569325	46.191565
3504.551206	515743.120208	46.196570
3504.373274	515747.497627	46.201575
3504.751678	515736.969208	46.206580
3504.121093	515739.749255	46.211585
3504.818012	515748.185977	46.216589
3504.336076	515746.441526	46.221594
3504.603131	515737.751337	46.226599
3504.708208	515731.615398	46.231604
3504.312213	515742.146627	46.236609
3504.471867	515736.912381	46.241613
3504.451150	515740.253493	46.246618
3504.228457	515715.558442	46.251623
3504.430021	515710.469283	46.256628
3504.368465	515708.557244	46.261633
3504.630890	515708.465210	46.266637
3504.607582	515705.282797	46.271642
3504.737666	515714.770010	46.276647
3504.262531	515695.121568	46.281652
3504.166870	515704.037586	46.286657
3504.713735	515702.029390	46.291661
3504.475984	515704.899078	46.296666
3504.761597	515701.971280	46.301671
3505.036781	515694.898126	46.306676
3504.694967	515682.865155	46.311681
3504.633064	515670.079911	46.316685
3504.464018	515658.778218	46.321690
3504.845110	515659.375456	46.326695
3504.510534	515651.892918	46.331700
3504.534983	515665.645016	46.336705
3504.792533	515643.807212	46.341709
3504.525192	515630.396952	46.346714
3504.574477	515621.083664	46.351719
3504.652564	515618.795531	46.356724
3504.854973	515621.292229	46.361729
3504.761522	515618.626619	46.366733
3504.785187	515612.351782	46.371738
3504.354842	515588.801978	46.376743
3504.538193	515572.994059	46.381748
3504.017775	515584.910539	46.386753
3504.837294	515575.728364	46.391757
3504.875645	515575.064860	46.396762
3504.418008	515598.249315	46.401767
3504.560340	515579.362900	46.406772
3503.974133	515589.317404	46.411777
3504.444750	515593.592365	46.416781
3504.691802	515573.728497	46.421786
3504.603392	515570.708067	46.426791
3504.740733	515558.751000	46.431796
3504.348646	515535.498516	46.436801
3504.782010	515546.505679	46.441805
3504.357511	515532.462719	46.446810
3504.284062	515554.271601	46.451815
3504.933591	515523.369577	46.456820
3504.197596	515551.604890	46.461825
3504.658306	515540.810472	46.466829
3504.511249	515538.305042	46.471834
3504.024893	515552.441404	46.476839
3504.737102	515538.977407	46.481844
3504.410874	515520.114404	46.486849
3505.070334	515530.529534	46.491853
3504.960645	515497.370486	46.496858
3504.435064	515521.223245	46.501863
3504.814172	515484.295036	46.506868
3504.638031	515525.540537	46.511873
3504.389386	515470.504953	46.516877
3504.521663	515467.803644	46.521882
3504.556700	515449.996092	46.526887
3504.540240	515454.803234	46.531892
3504.307598	515465.763986	46.536897
3504.603503	515456.108186	46.541901
3504.171205	515471.298126	46.546906
3504.583405	515435.527779	46.551911
3504.635473	515475.827004	46.556916
3504.380262	515454.171139	46.561921
3504.646162	515465.912857	46.566925
3504.830068	515452.431137	46.571930
3504.370454	515435.864947	46.576935
3504.982931	515419.938490	46.581940
3504.446084	515417.798090	46.586945
3504.614051	515421.817483	46.591949
3504.717923	515422.256247	46.596954
3504.479298	515414.100975	46.601959
3504.521497	515422.489614	46.606964
3504.485127	515424.214894	46.611969
3504.900447	515403.666768	46.616973
3504.616124	515388.438328	46.621978
3504.599798	515379.742165	46.626983
3504.625890	515375.489823	46.631988
3504.458562	515382.798964	46.636993
3504.305884	515391.977031	46.641997
3504.457835	515376.881928	46.647002
3504.226411	515378.081723	46.652007
3504.294990	515374.682427	46.657012
3504.270498	515381.210382	46.662017
3504.259399	515381.060427	46.667021
3504.636382	515386.614595	46.672026
3504.257235	515390.619314	46.677031
3504.906574	515376.153640	46.682036
3504.444344	515360.700421	46.687041
3504.193209	515328.119708	46.692045
3504.400204	515341.084608	46.697050
3504.426746	515344.064310	46.702055
3504.786162	515339.506409	46.707060
3504.252518	515344.547042	46.712065
3504.618795	515331.491571	46.717069
3504.713139	515326.419241	46.722074
3504.552242	515341.718128	46.727079
3504.757407	515334.655888	46.732084
3504.980116	515308.928931	46.737089
3505.059931	515304.971527	46.742093
3504.738080	515297.840840	46.747098
3504.542316	515302.322342	46.752103
3504.730340	515285.451350	46.757108
3504.467897	515284.885948	46.762113
3504.635082	515264.123994	46.767117
3504.492416	515255.599457	46.772122
3504.432415	515253.231949	46.777127
3504.671737	515257.745850	46.782132
3504.705800	515264.214022	46.787137
3504.538590	515257.412898	46.792141
3504.426384	515259.099606	46.797146
3504.591841	515254.572335	46.802151
3504.637821	515235.700760	46.807156
3504.122419	515233.051199	46.812161
3504.598783	515219.118474	46.817165
3504.604833	515220.533622	46.822170
3504.357519	515231.243973	46.827175
3504.624373	515222.856996	46.832180
3504.738628	515222.130908	46.837185
3504.645223	515223.511199	46.842189
3504.385676	515232.807392	46.847194
3504.673170	515222.596466	46.852199
3504.863655	515201.679029	46.857204
3504.227721	515197.682994	46.862209
3504.597012	515187.661419	46.867213
3504.483363	515185.201230	46.872218
3504.378298	515180.817843	46.877223
3504.658968	515176.828665	46.882228
3504.609285	515181.944585	46.887233
3504.667534	515174.248025	46.892237
3504.363070	515179.404211	46.897242
3504.434867	515175.245745	46.902247
3504.784895	515171.296179	46.907252
3504.310660	515162.318248	46.912257
3504.571193	515153.375912	46.917261
3504.747544	515149.757239	46.922266
3504.504442	515159.152023	46.927271
3504.740525	515161.289444	46.932276
3504.482723	515160.976178	46.937281
3504.732035	515157.952874	46.942285
3504.493779	515135.939892	46.947290
3504.928237	515117.107937	46.952295
3504.740725	515115.418036	46.957300
3504.513854	515113.835506	46.962305
3504.727139	515108.086837	46.967309
3504.985851	515107.287338	46.972314
3504.797850	515094.622733	46.977319
3504.911992	515082.668992	46.982324
3504.302812	515079.933078	46.987329
3504.658880	515072.846879	46.992333
3504.705350	515064.949829	46.997338
3504.756774	515076.776293	47.002343
3504.896622	515056.271278	47.007348
3504.545904	515027.650579	47.012353
3504.521934	515023.254334	47.017357
3505.115089	515021.087018	47.022362
3504.765773	515026.756093	47.027367
3505.073120	515014.013140	47.032372
3504.709018	515000.921117	47.037377
3504.881684	514991.486829	47.042381
3504.838058	514979.507374	47.047386
3504.573747	514997.604565	47.052391
3504.775315	514973.195392	47.057396
3504.439265	514955.597688	47.062401
3504.542123	514953.457276	47.067405
3504.896085	514932.463091	47.072410
3504.813576	514942.034918	47.077415
3504.803738	514940.923825	47.082420
3504.677359	514947.619778	47.087425
3504.963125	514925.776579	47.092429
3504.833820	514917.907240	47.097434
3504.574300	514907.529697	47.102439
3504.739422	514902.243750	47.107444
3504.653915	514915.406935	47.112449
3504.844907	514891.505070	47.117453
3504.776378	514866.278642	47.122458
3504.634154	514871.965615	47.127463
3504.749048	514859.505839	47.132468
3504.539459	514859.286098	47.137473
3504.664093	514854.866323	47.142477
3504.542409	514858.881054	47.147482
3504.636925	514844.047426	47.152487
3504.861149	514827.423132	47.157492
3504.642740	514826.951905	47.162497
3504.777200	514810.493508	47.167501
3504.712151	514824.007563	47.172506
3504.506802	514817.364016	47.177511
3504.522146	514786.965472	47.182516
3504.500003	514786.766681	47.187521
3504.627392	514778.806132	47.192525
3504.849962	514778.619243	47.197530
3504.342699	514779.154610	47.202535
3504.528134	514780.136837	47.207540
3504.363424	514780.314610	47.212545
3504.104562	514773.376046	47.217549
3504.444489	514776.812082	47.222554
3504.482584	514778.121051	47.227559
3504.624668	514776.075569	47.232564
3504.542168	514779.932397	47.237569
3504.647299	514762.315341	47.242573
3504.916585	514745.178083	47.247578
3504.501713	514755.814065	47.252583
3504.553947	514743.616987	47.257588
3504.716055	514742.579859	47.262593
3504.674763	514739.096647	47.267597
3504.974032	514732.575619	47.272602
3504.577627	514711.750324	47.277607
3504.744986	514697.056783	47.282612
3504.628776	514691.511775	47.287617
3504.678822	514689.278524	47.292621
3504.630335	514696.063419	47.297626
3504.250617	514697.134969	47.302631
3504.773026	514695.130523	47.307636
3504.503373	514676.358777	47.312641
3504.507756	514659.718485	47.317645
3504.634307	514657.776597	47.322650
3504.419153	514660.288856	47.327655
3504.746541	514656.443901	47.332660
3504.373183	514663.077848	47.337665
3504.555017	514658.750134	47.342669
3504.784007	514657.702430	47.347674
3504.304889	514654.541278	47.352679
3504.696329	514624.892223	47.357684
3504.507973	514622.898946	47.362689
3504.445247	514620.228320	47.367693
3504.535773	514610.806799	47.372698
3504.520039	514606.914909	47.377703
3504.862527	514604.888310	47.382708
3504.465878	514620.528573	47.387713
3504.431766	514607.434666	47.392717
3504.654699	514617.464171	47.397722
3504.489558	514598.979280	47.402727
3504.997559	514570.677274	47.407732
3504.622534	514582.369178	47.412737
3504.422315	514572.386667	47.417741
3504.423321	514571.627872	47.422746
3504.481978	514576.929160	47.427751
3504.526001	514572.420898	47.432756
3504.405740	514577.447003	47.437761
3504.464873	514575.060570	47.442765
3504.669543	514566.531364	47.447770
3504.457241	514546.991760	47.452775
3504.574390	514525.731033	47.457780
3504.693184	514532.691864	47.462785
3504.456068	514527.317640	47.467789
3504.410391	514534.911385	47.472794
3504.039781	514523.135011	47.477799
3504.367742	514517.469170	47.482804
3503.949406	514523.857396	47.487809
3504.432319	514528.181267	47.492813
3504.821259	514535.251133	47.497818
3504.436189	514535.564888	47.502823
3504.623793	514539.277930	47.507828
3504.279751	514535.690793	47.512833
3504.462509	514534.397505	47.517837
3504.531893	514540.860374	47.522842
3504.552614	514533.978678	47.527847
3504.643782	514515.352034	47.532852
3504.425421	514520.191352	47.537857
3504.448674	514518.973849	47.542861
3504.688454	514507.910225	47.547866
3504.523948	514518.860826	47.552871
3504.402194	514511.900485	47.557876
3504.232755	514514.810155	47.562881
3504.150914	514501.521400	47.567885
3504.354801	514503.360534	47.572890
3504.263896	514526.286203	47.577895
3504.663666	514515.045568	47.582900
3504.288303	514507.619538	47.587905
3504.284956	514516.622752	47.592909
3504.440629	514518.368350	47.597914
3504.247580	514527.603846	47.602919
3504.465507	514524.635966	47.607924
3504.419483	514512.808287	47.612929
3504.391381	514499.157000	47.617933
3504.503069	514491.552834	47.622938
3504.543884	514480.824099	47.627943
3504.509199	514479.362864	47.632948
3504.373650	514486.970834	47.637953
3504.434471	514476.643549	47.642957
3504.579813	514472.827324	47.647962
3504.397084	514477.509293	47.652967
3504.639264	514482.124107	47.657972
3504.231567	514485.374898	47.662977
3504.505710	514476.076013	47.667981
3504.813414	514477.038935	47.672986
3504.498953	514467.580185	47.677991
3504.757052	514450.292664	47.682996
3504.654918	514435.135716	47.688001
3504.517589	514436.573590	47.693005
3504.483925	514435.466230	47.698010
3504.449751	514442.097234	47.703015
3504.405913	514442.154753	47.708020
3504.410719	514437.854961	47.713025
3504.328013	514442.976325	47.718029
3504.801019	514432.229831	47.723034
3504.427816	514419.948023	47.728039
3504.661313	514397.505473	47.733044
3504.732518	514394.560758	47.738049
3504.783822	514396.120556	47.743053
3504.855215	514390.040027	47.748058
3504.593304	514393.419527	47.753063
3504.383979	514389.001832	47.758068
3504.563386	514389.934458	47.763073
3504.506066	514361.974332	47.768077
3504.577311	514358.018060	47.773082
3504.214584	514353.928063	47.778087
3504.445857	514346.254355	47.783092
3504.520642	514360.050148	47.788097
3504.380869	514358.858397	47.793101
3504.675577	514356.080662	47.798106
3504.610488	514356.040386	47.803111
3504.762552	514359.455621	47.808116
3504.561990	514356.958469	47.813121
3504.614857	514335.252464	47.818125
3504.625479	514313.907150	47.823130
3504.506186	514310.183289	47.828135
3504.813676	514306.088513	47.833140
3504.855728	514303.300122	47.838145
3504.618516	514309.154029	47.843149
3504.703900	514306.257636	47.848154
3504.534334	514285.294804	47.853159
3504.434825	514276.611215	47.858164
3504.635703	514271.926350	47.863169
3504.471916	514259.307862	47.868173
3504.341413	514271.618845	47.873178
3504.273714	514285.032598	47.878183
3504.368404	514268.984575	47.883188
3504.424626	514264.676613	47.888193
3504.381904	514268.426116	47.893197
3504.552506	514259.902139	47.898202
3504.355566	514258.567684	47.903207
3504.548357	514258.537228	47.908212
3504.428702	514274.993854	47.913217
3504.636713	514263.935091	47.918221
3504.511370	514239.930560	47.923226
3504.268319	514226.768222	47.928231
3504.536481	514230.013402	47.933236
3504.320226	514226.911779	47.938241
3504.194174	514226.779981	47.943245
3504.649854	514227.719531	47.948250
3504.578809	514239.869407	47.953255
3504.666484	514229.385993	47.958260
3504.208610	514233.302272	47.963265
3504.516834	514236.642275	47.968269
3504.689138	514240.104914	47.973274
3504.582191	514234.457135	47.978279
3504.701047	514207.126417	47.983284
3504.527887	514194.458784	47.988289
3504.720178	514187.903876	47.993293
3504.394076	514190.383161	47.998298
3504.461514	514198.212069	48.003303
3504.482994	514189.863358	48.008308
3504.126288	514201.350319	48.013313
3504.371486	514190.943142	48.018317
3504.585158	514196.321207	48.023322
3504.416942	514200.545759	48.028327
3504.846234	514191.121042	48.033332
3504.781071	514184.859709	48.038337
3504.635496	514153.827939	48.043341
3504.609364	514151.758390	48.048346
3504.466678	514147.380677	48.053351
3505.111993	514146.924658	48.058356
3504.726142	514144.305024	48.063361
3504.690899	514136.723919	48.068365
3504.484830	514113.440057	48.073370
3504.077979	514116.994252	48.078375
3504.562325	514102.047782	48.083380
3504.546199	514107.613928	48.088385
3504.474287	514106.512590	48.093389
3504.620311	514114.329118	48.098394
3504.448254	514115.823086	48.103399
3504.549057	514100.330295	48.108404
3504.504442	514115.814234	48.113409
3504.606738	514112.308198	48.118413
3504.778827	514087.598929	48.123418
3504.563434	514069.576599	48.128423
3504.759391	514059.682904	48.133428
3504.511005	514060.936049	48.138433
3504.643467	514059.852987	48.143437
3504.597541	514061.175291	48.148442
3504.714576	514057.818650	48.153447
3504.753104	514049.922378	48.158452
3504.291694	514039.879672	48.163457
3504.646603	514028.848117	48.168461
3504.605890	514018.789489	48.173466
3504.340953	514022.321275	48.178471
3504.248392	514030.023814	48.183476
3504.445320	514021.192086	48.188481
3504.101956	514024.179906	48.193485
3504.517275	514020.725537	48.198490
3504.236806	514017.077662	48.203495
3504.560181	514022.792493	48.208500
3504.657636	514033.904322	48.213505
3504.386281	514032.278140	48.218509
3504.979162	514003.607719	48.223514
3504.315761	514008.618676	48.228519
3504.328820	513990.863626	48.233524
3504.315736	513994.355615	48.238529
3504.593869	513988.191689	48.243533
3504.354865	513967.947533	48.248538
3504.415966	513998.993024	48.253543
3504.530116	513987.341974	48.258548
3504.305949	513980.397597	48.263553
3504.300124	513986.821987	48.268557
3504.363397	513978.163095	48.273562
3504.412512	513988.422761	48.278567
3504.554886	513984.354003	48.283572
3504.362050	513982.816563	48.288577
3504.434873	513991.352814	48.293581
3504.690328	513987.569656	48.298586
3504.185616	513995.640818	48.303591
3504.448153	513984.927303	48.308596
3504.034526	513992.731179	48.313601
3504.082360	513993.532887	48.318605
3504.400716	513989.436317	48.323610
3504.243123	513991.180902	48.328615
3504.262408	513993.757365	48.333620
3504.146835	513988.515493	48.338625
3504.156343	513987.856486	48.343629
3504.241823	513996.845939	48.348634
3504.298008	513997.342857	48.353639
3504.249864	513988.094639	48.358644
3504.562461	513984.808232	48.363649
3504.425870	513994.945508	48.368653
3504.685887	513995.966574	48.373658
3504.400394	513978.713901	48.378663
3504.506656	513962.866071	48.383668
3504.585054	513948.388249	48.388673
3504.462833	513957.966913	48.393677
3504.704203	513947.661348	48.398682
3504.588216	513947.477378	48.403687
3504.767845	513945.223549	48.408692
3504.354746	513954.443557	48.413697
3504.297896	513950.153384	48.418701
3504.670767	513943.569842	48.423706
3504.339504	513927.588812	48.428711
3504.492361	513907.636702	48.433716
3504.603062	513914.194440	48.438721
3504.667135	513918.888137	48.443725
3504.655701	513917.979544	48.448730
3504.447787	513919.023989	48.453735
3504.780033	513909.715609	48.458740
3504.593975	513913.740738	48.463745
3504.427993	513912.047311	48.468749
3504.613944	513895.782195	48.473754
3504.483648	513883.714498	48.478759
3504.660932	513884.698067	48.483764
3504.694992	513874.071169	48.488769
3504.586088	513875.504599	48.493773
3504.771840	513882.657433	48.498778
3504.436015	513884.986562	48.503783
3504.707167	513878.317913	48.508788
3504.865190	513857.505089	48.513793
3504.828913	513844.208613	48.518797
3504.856299	513831.660748	48.523802
3504.650150	513849.345352	48.528807
3504.821917	513843.805130	48.533812
3504.617605	513821.026373	48.538817
3504.913564	513799.888205	48.543821
3504.679049	513802.605966	48.548826
3504.403743	513804.116279	48.553831
3504.766407	513790.200343	48.558836
3504.869736	513791.145027	48.563841
3504.629758	513774.593056	48.568845
3504.599093	513756.591774	48.573850
3504.563092	513751.741885	48.578855
3505.041489	513746.760120	48.583860
3504.537530	513755.589964	48.588865
3504.661993	513748.893867	48.593869
3504.616595	513743.084458	48.598874
3504.368616	513726.938338	48.603879
3504.650312	513713.793822	48.608884
3504.731266	513704.626203	48.613889
3504.637993	513710.558727	48.618893
3504.705006	513712.065527	48.623898
3504.522162	513718.821471	48.628903
3504.658949	513713.084417	48.633908
3504.510679	513701.019429	48.638913
3504.630476	513677.329407	48.643917
3504.880651	513669.197190	48.648922
3504.592783	513673.592522	48.653927
3504.705275	513667.302920	48.658932
3504.539959	513670.616718	48.663937
3504.602772	513661.704839	48.668941
3504.594870	513649.111836	48.673946
3504.392378	513638.775072	48.678951
3504.415011	513622.029708	48.683956
3504.201873	513631.622926	48.688961
3504.379334	513626.638107	48.693965
3504.576365	513621.447875	48.698970
3504.412814	513625.570674	48.703975
3504.351015	513613.896593	48.708980
3504.721394	513622.487164	48.713985
3504.689488	513623.149754	48.718989
3504.705595	513616.925945	48.723994
3504.210733	513633.189599	48.728999
3504.532181	513627.575071	48.734004
3504.397630	513615.305535	48.739009
3504.506923	513604.363100	48.744013
3505.003328	513592.044409	48.749018
3504.520103	513585.292549	48.754023
3504.547961	513575.829774	48.759028
3504.727074	513576.256697	48.764033
3504.741225	513577.114328	48.769037
3504.723286	513568.012843	48.774042
3504.457349	513558.495331	48.779047
3504.685245	513536.305417	48.784052
3504.905918	513545.324325	48.789057
3504.537880	513545.483664	48.794061
3504.645667	513533.024030	48.799066
3504.735671	513543.075186	48.804071
3504.703134	513525.377431	48.809076
3504.264454	513512.245450	48.814081
3504.426819	513494.668599	48.819085
3504.654052	513493.115304	48.824090
3504.518493	513499.155746	48.829095
3504.538627	513489.997622	48.834100
3504.697719	513499.228608	48.839105
3504.593034	513505.668806	48.844109
3504.691581	513498.976706	48.849114
3504.564843	513497.985153	48.854119
3504.754650	513467.961289	48.859124
3504.575614	513462.931603	48.864129
3504.200348	513458.843368	48.869133
3504.565336	513445.837220	48.874138
3504.308793	513463.884253	48.879143
3504.470750	513455.158916	48.884148
3504.297976	513458.372774	48.889153
3504.417657	513458.606773	48.894157
3504.803737	513452.273852	48.899162
3504.314506	513449.872765	48.904167
3504.311657	513448.305249	48.909172
3504.307263	513463.328212	48.914177
3504.351564	513459.982946	48.919181
3504.193611	513452.774987	48.924186
3504.428852	513466.950793	48.929191
3504.327433	513462.111160	48.934196
3504.341647	513467.622142	48.939201
3504.347103	513461.703439	48.944205
3504.399173	513421.888746	48.949210
3504.202391	513418.733314	48.954215
3504.308501	513417.047415	48.959220
3504.401637	513417.285610	48.964225
3504.116334	513418.746956	48.969229
3504.463258	513416.011396	48.974234
3504.161103	513420.206731	48.979239
3504.275114	513410.983148	48.984244
3504.281093	513417.254150	48.989249
3504.064266	513415.973349	48.994253
3504.375868	513429.074937	48.999258
3504.206887	513436.992145	49.004263
3504.326665	513434.545387	49.009268
3504.253537	513429.903593	49.014273
3504.000376	513444.409508	49.019277
3504.335046	513451.690730	49.024282
3504.116452	513464.167964	49.029287
3504.310984	513466.565072	49.034292
3504.481615	513470.028135	49.039297
3503.955323	513473.753080	49.044301
3504.248257	513471.127221	49.049306
3503.940443	513475.980976	49.054311
3503.985891	513466.464779	49.059316
3503.903950	513476.441990	49.064321
3503.938503	513480.584096	49.069325
3504.466276	513471.396314	49.074330
3504.057596	513475.507311	49.079335
3504.195049	513467.493971	49.084340
3504.142432	513473.571893	49.089345
3504.335242	513476.677390	49.094349
3504.523538	513471.741392	49.099354
3504.325205	513465.551418	49.104359
3504.390670	513473.836196	49.109364
3504.239020	513482.408182	49.114369
3504.163490	513482.673032	49.119373
3504.290127	513467.934275	49.124378
3504.373657	513475.760977	49.129383
3504.210946	513460.562143	49.134388
3504.449986	513468.667751	49.139393
3504.527226	513480.642999	49.144397
3504.717941	513478.690836	49.149402
3504.638219	513476.123873	49.154407
3504.609638	513467.630975	49.159412
3504.886774	513466.777911	49.164417
3504.775902	513449.345356	49.169421
3504.651743	513444.762212	49.174426
3504.595446	513434.250477	49.179431
3504.787906	513422.687819	49.184436
3504.807228	513443.574340	49.189441
3504.762657	513414.346122	49.194445
3504.653044	513409.254868	49.199450
3504.729878	513400.947597	49.204455
3504.867894	513387.016253	49.209460
3504.786675	513407.615226	49.214465
3504.679378	513378.750922	49.219469
3505.021648	513354.570064	49.224474
3504.552759	513353.329095	49.229479
3504.919762	513347.403792	49.234484
3504.806679	513350.102434	49.239489
3504.424165	513330.082511	49.244493
3504.850282	513315.650353	49.249498
3504.653403	513316.440188	49.254503
3504.710777	513311.019030	49.259508
3504.662218	513312.847613	49.264513
3504.521416	513309.733894	49.269517
3504.669465	513320.180653	49.274522
3504.617880	513306.329788	49.279527
3504.872776	513273.311045	49.284532
3504.681065	513274.504710	49.289537
3504.538574	513272.048798	49.294541
3504.621982	513267.078736	49.299546
3504.390995	513268.885575	49.304551
3504.643405	513263.382998	49.309556
3504.573756	513268.350913	49.314561
3504.759827	513262.353015	49.319565
3504.892977	513240.278846	49.324570
3504.795968	513247.122575	49.329575
3504.622341	513242.446032	49.334580
3504.521015	513238.415610	49.339585
3504.634279	513234.755917	49.344589
3504.734966	513212.788004	49.349594
3504.679485	513206.423616	49.354599
3504.693319	513201.110466	49.359604
3504.645979	513193.176783	49.364609
3504.616116	513205.624381	49.369613
3504.911722	513183.119817	49.374618
3504.689671	513184.368863	49.379623
3504.506239	513157.185378	49.384628
3504.623675	513145.937873	49.389633
3504.945493	513142.295781	49.394637
3504.965016	513139.763663	49.399642
3504.694923	513153.007980	49.404647
3504.597144	513128.087051	49.409652
3504.520100	513120.512095	49.414657
3504.542048	513118.738305	49.419661
3505.038377	513107.481475	49.424666
3504.677574	513110.927440	49.429671
3504.688975	513113.100635	49.434676
3504.843277	513091.275834	49.439681
3504.753133	513076.318090	49.444685
3504.871932	513065.222060	49.449690
3504.510088	513072.461783	49.454695
3504.842584	513062.141275	49.459700
3504.905810	513056.719112	49.464705
3504.341825	513048.209457	49.469709
3504.764800	513020.171194	49.474714
3504.391065	513015.981446	49.479719
3504.750563	513013.193253	49.484724
3504.741635	513018.303389	49.489729
3504.560537	513023.997128	49.494733
3504.676955	513022.208398	49.499738
3504.619676	513000.518081	49.504743
3504.517885	512983.892911	49.509748
3504.586920	512976.952362	49.514753
3504.602789	512990.404519	49.519757
3504.569577	512966.130704	49.524762
3504.506048	512977.976813	49.529767
3504.696603	512975.316477	49.534772
3504.732164	512976.980058	49.539777
3504.525667	512958.145828	49.544781
3504.450221	512943.084480	49.549786
3504.369267	512937.634483	49.554791
3504.437299	512930.946981	49.559796
3504.617232	512932.031352	49.564801
3504.364597	512938.141078	49.569805
3504.553486	512933.255412	49.574810
3504.366437	512939.101864	49.579815
3504.448885	512935.902211	49.584820
3504.685734	512936.876423	49.589825
3504.495051	512937.462970	49.594829
3504.699197	512932.574892	49.599834
3504.390764	512904.803777	49.604839
3504.664141	512884.629083	49.609844
3504.391143	512885.178060	49.614849
3504.100760	512896.554261	49.619853
3504.549073	512890.919439	49.624858
3504.611678	512899.103788	49.629863
3504.440701	512893.263351	49.634868
3504.654085	512895.910469	49.639873
3504.736141	512885.073036	49.644877
3504.843083	512888.141631	49.649882
3504.165782	512877.171296	49.654887
3504.368209	512859.688617	49.659892
3504.546337	512853.691829	49.664897
3504.441055	512847.739830	49.669901
3504.590449	512849.183106	49.674906
3504.376674	512865.757145	49.679911
3504.567640	512848.225684	49.684916
3504.426274	512857.049271	49.689921
3504.336442	512851.752395	49.694925
3504.590035	512843.821569	49.699930
3504.419294	512847.439875	49.704935
3504.571961	512853.738485	49.709940
3504.917401	512853.886232	49.714945
3504.542800	512837.708688	49.719949
3504.494122	512821.985438	49.724954
3504.706161	512817.804226	49.729959
3504.786974	512808.534979	49.734964
3504.665183	512806.379218	49.739969
3504.587829	512813.523507	49.744973
3504.654504	512811.742617	49.749978
3504.569807	512785.048747	49.754983
3504.548657	512774.480464	49.759988
3504.626500	512763.694201	49.764993
3504.273791	512776.091974	49.769997
3504.828126	512767.506599	49.775002
3504.536366	512758.802027	49.780007
3504.413074	512758.922691	49.785012
3504.402155	512755.333103	49.790017
3504.350600	512762.018098	49.795021
3504.462942	512756.588075	49.800026
3504.299549	512767.438473	49.805031
3504.247939	512761.225051	49.810036
3504.450890	512757.197006	49.815041
3504.295366	512761.824568	49.820045
3504.308254	512746.546756	49.825050
3504.521741	512760.119610	49.830055
3504.428623	512738.586367	49.835060
3504.444071	512726.393642	49.840065
3504.371539	512738.898909	49.845069
3504.637433	512726.261946	49.850074
3504.315038	512729.145513	49.855079
3504.567240	512726.171902	49.860084
3504.764638	512727.708766	49.865089
3504.377528	512724.785612	49.870093
3504.189917	512720.718120	49.875098
3504.245992	512728.347180	49.880103
3504.599374	512729.758226	49.885108
3504.560025	512721.114908	49.890113
3504.528632	512732.399706	49.895117
3504.574426	512702.093749	49.900122
3504.477720	512695.179278	49.905127
3504.437458	512692.353048	49.910132
3504.943136	512684.028231	49.915137
3504.404647	512680.269095	49.920141
3504.526147	512669.829949	49.925146
3504.073549	512694.889148	49.930151
3504.226201	512687.277695	49.935156
3504.686965	512684.625192	49.940161
3504.497236	512685.666837	49.945165
3504.718477	512687.806923	49.950170
3504.266145	512688.080754	49.955175
3504.017536	512689.991603	49.960180
3504.402288	512678.701540	49.965185
3504.183451	512689.965409	49.970189
3504.270727	512682.617198	49.975194
3504.374573	512683.410116	49.980199
3504.313937	512688.022701	49.985204
3504.196064	512681.516228	49.990209
3504.174847	512695.429722	49.995213
3504.416882	512691.395485	50.000218
3504.576156	512691.167998	50.005223
3504.468154	512675.403405	50.010228
3504.428526	512663.067591	50.015233
3504.258735	512654.798931	50.020237
3504.558812	512648.631050	50.025242
3504.458846	512658.055187	50.030247
3504.581146	512645.137362	50.035252
3504.683452	512651.747502	50.040257
3504.391291	512650.933789	50.045261
3504.573900	512644.480978	50.050266
3504.517474	512646.513205	50.055271
3504.449782	512643.134896	50.060276
3504.486689	512644.343055	50.065281
3504.387181	512635.658618	50.070285
3504.311549	512618.978372	50.075290
3504.407588	512620.834760	50.080295
3504.267732	512602.040183	50.085300
3504.611040	512611.748367	50.090305
3504.142154	512611.771902	50.095309
3504.514850	512607.666413	50.100314
3504.558289	512603.410629	50.105319
3504.515261	512609.841424	50.110324
3504.697251	512610.976073	50.115329
3504.577680	512612.107799	50.120333
3504.977046	512607.492270	50.125338
3504.482205	512595.228350	50.130343
3504.366358	512584.067923	50.135348
3504.809985	512574.134217	50.140353
3504.536232	512579.943913	50.145357
3504.870210	512572.758996	50.150362
3504.801442	512564.676656	50.155367
3504.556100	512573.668571	50.160372
3505.018565	512565.906935	50.165377
3504.698968	512550.934406	50.170381
3504.891627	512529.254566	50.175386
3504.366931	512540.061045	50.180391
3504.665122	512528.835146	50.185396
3504.833943	512528.707314	50.190401
3504.424376	512515.165289	50.195405
3504.741399	512492.504674	50.200410
3504.433087	512483.549662	50.205415
3504.570907	512474.979383	50.210420
3504.672455	512484.321186	50.215425
3504.525467	512481.714119	50.220429
3504.661376	512475.723871	50.225434
3504.886650	512479.987829	50.230439
3504.679113	512456.398410	50.235444
3504.452722	512439.842980	50.240449
3504.058763	512433.683543	50.245453
3504.636349	512428.179888	50.250458
3504.722189	512438.839357	50.255463
3504.673587	512439.150550	50.260468
3504.504928	512435.181160	50.265473
3504.518277	512437.252968	50.270477
3504.639364	512431.872043	50.275482
3504.462450	512424.261975	50.280487
3504.592279	512407.852548	50.285492
3504.961156	512396.868306	50.290497
3504.712932	512400.094288	50.295501
3504.736141	512397.359144	50.300506
3504.592857	512386.607589	50.305511
3504.464365	512379.091014	50.310516
3504.441849	512365.841781	50.315521
3504.212691	512364.562848	50.320525
3504.474540	512344.439917	50.325530
3504.605326	512356.660417	50.330535
3504.139813	512358.858499	50.335540
3504.409599	512350.773134	50.340545
3504.235006	512356.111985	50.345549
3504.147826	512352.180282	50.350554
3503.822866	512348.184990	50.355559
3504.199681	512350.502865	50.360564
3504.453629	512346.466664	50.365569
3504.189188	512350.201052	50.370573
3504.592869	512347.911601	50.375578
3504.540389	512357.581316	50.380583
3504.306053	512354.330452	50.385588
3504.604363	512344.824245	50.390593
3504.266362	512350.138340	50.395597
3504.570671	512353.074674	50.400602
3504.370563	512359.075140	50.405607
3504.723185	512360.688672	50.410612
3504.615872	512355.596736	50.415617
3504.341399	512360.597288	50.420621
3504.444768	512344.697814	50.425626
3504.307570	512333.591180	50.430631
3504.142200	512324.006492	50.435636
3504.438509	512328.613346	50.440641
3504.408726	512320.676478	50.445645
3504.622617	512313.055179	50.450650
3504.207662	512319.393114	50.455655
3504.514129	512316.208523	50.460660
3504.644963	512317.907695	50.465665
3504.446494	512315.409906	50.470669
3504.822428	512313.681254	50.475674
3504.652247	512317.400751	50.480679
3504.494181	512313.530825	50.485684
3504.821094	512306.599828	50.490689
3504.608922	512287.816331	50.495693
3504.657825	512272.431232	50.500698
3504.624430	512272.183607	50.505703
3504.802831	512263.556224	50.510708
3504.726442	512273.988519	50.515713
3504.239555	512263.291189	50.520717
3504.867961	512265.012895	50.525722
3504.756454	512246.011108	50.530727
3504.296429	512228.177221	50.535732
3504.715137	512197.103252	50.540737
3504.319512	512164.336908	50.545741
3504.631432	512114.260127	50.550746
3504.254631	512061.206414	50.555751
3504.067363	511999.624413	50.560756
3504.330338	511920.165270	50.565761
3503.799893	511839.313606	50.570765
3504.042494	511742.910931	50.575770
3504.094845	511639.658163	50.580775
3503.749195	511517.245085	50.585780
3503.653942	511389.075317	50.590785
3503.535693	511263.134024	50.595789
3503.345938	511108.115605	50.600794
3503.055456	510963.229180	50.605799
3502.949452	510796.256049	50.610804
3502.856706	510636.108622	50.615809
3502.591200	510473.963439	50.620813
3502.554716	510282.084545	50.625818
3502.136801	510082.675275	50.630823
3501.682385	509885.697797	50.635828
3501.369206	509663.754251	50.640833
3501.198311	509453.573256	50.645837
3500.947165	509236.117045	50.650842
3500.685580	509028.778359	50.655847
3500.472420	508784.799601	50.660852
3500.488778	508535.974622	50.665857
3499.659067	508285.154760	50.670861
3499.467253	508023.402867	50.675866
3499.045227	507765.022780	50.680871
3498.701689	507509.308096	50.685876
3498.503038	507223.410088	50.690881
3497.815408	506945.731121	50.695885
3497.531178	506646.074109	50.700890
3496.981817	506353.942773	50.705895
3496.966830	506059.849803	50.710900
3496.596113	505764.593621	50.715905
3496.127818	505453.812564	50.720909
3495.741814	505133.600527	50.725914
3495.295472	504817.744227	50.730919
3494.738210	504505.948263	50.735924
3494.355006	504168.208319	50.740929
3493.741484	503844.466157	50.745933
3493.402968	503511.210649	50.750938
3492.869443	503187.848631	50.755943
3492.412687	502834.607999	50.760948
3492.388789	502488.175138	50.765953
3491.606368	502139.223495	50.770957
3491.148439	501770.676625	50.775962
3490.700728	501408.498002	50.780967
3490.019976	501048.626561	50.785972
3489.824185	500679.610702	50.790977
3489.209017	500315.360995	50.795981
3488.954128	499936.164819	50.800986
3488.089571	499567.029195	50.805991
3487.828212	499167.569581	50.810996
3487.635565	498778.923471	50.816001
3486.598560	498398.198474	50.821005
3486.312753	498005.399243	50.826010
3485.705514	497593.404404	50.831015
3485.155291	497204.882143	50.836020
3484.928412	496783.594624	50.841025
3484.364062	496386.095851	50.846029
3483.819626	495966.662239	50.851034
3483.089418	495552.969713	50.856039
3482.551650	495135.794362	50.861044
3482.192165	494707.138035	50.866049
3480.953422	494293.446760	50.871053
3480.636412	493872.308848	50.876058
3480.173658	493444.702736	50.881063
3479.618809	493024.950254	50.886068
3478.962057	492590.873274	50.891073
3478.516220	492170.577770	50.896077
3478.207461	491718.599721	50.901082
3477.239558	491292.543002	50.906087
3476.827249	490849.321504	50.911092
3476.589647	490404.137328	50.916097
3475.749735	489971.902087	50.921101
3474.967163	489506.929101	50.926106
3474.532080	489068.480625	50.931111
3473.877651	488614.810781	50.936116
3473.094635	488166.367486	50.941121
3472.510110	487707.143739	50.946125
3472.027168	487247.538224	50.951130
3471.259260	486803.771132	50.956135
3470.363047	486344.867633	50.961140
3470.313793	485885.312639	50.966145
3469.412683	485430.997813	50.971149
3468.859414	484973.526952	50.976154
3468.082040	484513.446215	50.981159
3467.366556	484059.626869	50.986164
3466.485808	483597.615412	50.991169
3465.769426	483136.630897	50.996173
3465.476869	482683.320365	51.001178
3464.561816	482219.508139	51.006183
3463.578574	481772.618978	51.011188
3463.191239	481297.706284	51.016193
3462.493094	480833.826816	51.021197
3461.805202	480382.906849	51.026202
3461.022025	479928.241755	51.031207
3460.387829	479471.312924	51.036212
3459.827449	479002.250324	51.041217
3459.146767	478559.750355	51.046221
3458.302661	478081.284864	51.051226
3457.520806	477627.833612	51.056231
3456.801321	477172.943120	51.061236
3456.514332	476707.786882	51.066241
3455.568847	476257.320571	51.071245
3454.855088	475796.315928	51.076250
3454.174429	475339.603712	51.081255
3453.641174	474877.941271	51.086260
3452.721965	474420.941839	51.091265
3452.064409	473963.434528	51.096269
3451.787003	473499.621973	51.101274
3450.999576	473031.925569	51.106279
3449.969814	472590.565898	51.111284
3449.437610	472117.232065	51.116289
3448.699692	471671.396120	51.121293
3448.241365	471202.287805	51.126298
3447.488511	470741.124016	51.131303
3446.764900	470289.780643	51.136308
3446.255118	469822.068604	51.141313
3445.050807	469377.220064	51.146317
3444.778744	468904.734679	51.151322
3443.850106	468455.209043	51.156327
3443.039478	467998.100287	51.161332
3442.567184	467536.922418	51.166337
3441.671109	467095.373705	51.171341
3440.996947	466637.858792	51.176346
3440.256318	466184.857433	51.181351
3439.269182	465735.434937	51.186356
3439.018424	465272.803370	51.191361
3438.015404	464843.039862	51.196365
3437.636051	464378.431436	51.201370
3436.696640	463932.056686	51.206375
3436.092432	463487.597475	51.211380
3435.235271	463025.165167	51.216385
3434.614686	462588.449339	51.221389
3434.029506	462148.726744	51.226394
3433.444713	461702.097452	51.231399
3432.916964	461244.038081	51.236404
3432.064447	460788.860722	51.241409
3430.747171	460359.463064	51.246413
3430.603973	459886.757277	51.251418
3429.804647	459460.506295	51.256423
3428.897313	459012.807638	51.261428
3428.435147	458562.696106	51.266433
3427.423796	458122.959684	51.271437
3426.818944	457686.548987	51.276442
3426.322084	457247.576183	51.281447
3425.641699	456805.072634	51.286452
3424.953015	456354.901273	51.291457
3423.760288	455931.536050	51.296461
3423.483347	455468.192967	51.301466
3423.093321	455039.509244	51.306471
3422.100009	454597.214377	51.311476
3421.627438	454153.763051	51.316481
3420.765491	453717.163268	51.321485
3420.217106	453274.061821	51.326490
3419.200323	452855.989114	51.331495
3418.263932	452395.224123	51.336500
3418.167540	451957.353215	51.341505
3417.119028	451534.237973	51.346509
3416.368646	451085.595107	51.351514
3415.705754	450657.531459	51.356519
3415.012404	450216.778591	51.361524
3414.466869	449784.925110	51.366529
3413.558661	449351.141803	51.371533
3412.909978	448924.363213	51.376538
3411.997730	448494.827314	51.381543
3411.451419	448063.550932	51.386548
3410.617442	447636.930319	51.391553
3410.126672	447211.364200	51.396557
3409.506957	446786.927298	51.401562
3409.049242	446356.214554	51.406567
3408.175561	445933.477282	51.411572
3407.345261	445501.336012	51.416577
3406.459788	445073.712832	51.421581
3405.641577	444645.106962	51.426586
3404.903643	444227.748813	51.431591
3404.238006	443799.560463	51.436596
3403.761114	443374.227894	51.441601
3402.976742	442964.621235	51.446605
3402.050879	442540.055543	51.451610
3401.389914	442124.120761	51.456615
3400.475836	441708.929529	51.461620
3400.037638	441284.163197	51.466625
3399.395773	440876.326172	51.471629
3398.845947	440452.730580	51.476634
3397.686492	440041.154057	51.481639
3397.049016	439630.808041	51.486644
3396.559758	439210.049742	51.491649
3395.813309	438803.819361	51.496653
3394.994542	438394.242954	51.501658
3394.028344	437993.593266	51.506663
3393.461833	437582.998950	51.511668
3393.009209	437170.983633	51.516673
3392.346895	436769.860039	51.521677
3391.695197	436364.361812	51.526682
3391.361410	435954.820983	51.531687
3390.317120	435545.081169	51.536692
3389.900705	435127.263592	51.541697
3389.066761	434725.271345	51.546701
3388.630935	434308.408089	51.551706
3387.826926	433906.626646	51.556711
3386.999998	433488.973961	51.561716
3385.908005	433083.899051	51.566721
3385.554160	432680.757659	51.571725
3384.656906	432275.436071	51.576730
3383.951283	431871.398151	51.581735
3383.104844	431473.241645	51.586740
3382.292454	431068.420916	51.591745
3381.579154	430676.045892	51.596749
3380.976078	430276.080467	51.601754
3380.344474	429887.718114	51.606759
3379.712882	429484.164633	51.611764
3379.468596	429082.702196	51.616769
3378.154122	428687.827607	51.621773
3377.785398	428285.153756	51.626778
3376.961723	427884.856659	51.631783
3376.229540	427507.877514	51.636788
3375.637689	427102.986178	51.641793
3374.795675	426709.632745	51.646797
3374.060519	426304.294812	51.651802
3373.002361	425922.824205	51.656807
3372.306863	425535.220870	51.661812
3372.102752	425145.045284	51.666817
3371.186506	424772.501335	51.671821
3370.931293	424366.778968	51.676826
3370.310093	423979.217768	51.681831
3369.067141	423588.752249	51.686836
3368.761242	423192.164086	51.691841
3368.177936	422814.257571	51.696845
3367.124493	422418.157395	51.701850
3366.295227	422038.501074	51.706855
3365.852361	421646.433556	51.711860
3365.635198	421258.363604	51.716865
3364.287966	420879.255884	51.721869
3363.811644	420479.709057	51.726874
3363.360579	420092.498079	51.731879
3362.434268	419718.261474	51.736884
3361.824539	419321.640498	51.741889
3361.211848	418954.812630	51.746893
3360.355999	418545.949773	51.751898
3359.478651	418168.407716	51.756903
3358.821197	417797.329401	51.761908
3358.427264	417402.654309	51.766913
3356.955489	417020.770541	51.771917
3356.810005	416638.621143	51.776922
3356.433471	416258.078342	51.781927
3355.555938	415878.346492	51.786932
3354.503051	415500.593661	51.791937
3353.855017	415126.684523	51.796941
3353.235530	414751.902196	51.801946
3352.975601	414369.893264	51.806951
3351.998452	413989.999943	51.811956
3351.508722	413610.888482	51.816961
3350.321929	413242.579301	51.821965
3349.950174	412865.599264	51.826970
3349.100282	412491.510413	51.831975
3348.404737	412120.721051	51.836980
3348.090897	411747.071611	51.841985
3347.281023	411372.454086	51.846989
3346.337315	410993.838160	51.851994
3345.813649	410621.300406	51.856999
3345.001883	410252.742278	51.862004
3344.473992	409874.605477	51.867009
3343.554064	409508.062811	51.872013
3343.395026	409133.873431	51.877018
3342.727077	408761.182981	51.882023
3341.884308	408395.376998	51.887028
3341.233016	408013.907397	51.892033
3340.427529	407649.179312	51.897037
3339.739200	407272.306098	51.902042
3339.047366	406895.377980	51.907047
3338.529839	406529.422010	51.912052
3337.816752	406157.520225	51.917057
3336.922012	405791.488088	51.922061
3336.455626	405420.783773	51.927066
3335.409422	405042.084640	51.932071
3334.818831	404685.064676	51.937076
3334.314811	404311.964067	51.942081
3333.294031	403949.158071	51.947085
3332.780228	403580.777751	51.952090
3332.033398	403210.752467	51.957095
3331.182122	402851.033316	51.962100
3330.785179	402478.859956	51.967105
3330.000859	402130.890337	51.972109
3329.469021	401764.576043	51.977114
3328.885565	401400.604204	51.982119
3328.039713	401044.091955	51.987124
3327.215087	400673.134491	51.992129
3326.401582	400314.423038	51.997133
3325.862631	399945.013454	52.002138
3325.392160	399586.290543	52.007143
3324.617916	399215.537218	52.012148
3323.842219	398862.802900	52.017153
3322.985997	398501.841258	52.022157
3322.573253	398135.975564	52.027162
3322.116153	397777.256158	52.032167
3321.362772	397419.825361	52.037172
3320.804012	397060.249937	52.042177
3319.577078	396702.123649	52.047181
3319.289076	396331.896596	52.052186
3318.279790	395977.210962	52.057191
3317.308773	395623.354477	52.062196
3317.072258	395260.480061	52.067201
3316.226281	394911.909747	52.072205
3315.700946	394555.480107	52.077210
3315.182139	394191.062610	52.082215
3314.188837	393840.674081	52.087220
3314.025610	393486.896375	52.092225
3313.081652	393131.306209	52.097229
3312.149136	392762.184513	52.102234
3311.816515	392405.244350	52.107239
3311.165238	392063.301040	52.112244
3310.537710	391691.704273	52.117249
3310.037692	391334.271050	52.122253
3309.285781	390980.459096	52.127258
3308.473957	390613.126165	52.132263
3307.567011	390266.654346	52.137268
3307.193804	389900.439664	52.142273
3306.329650	389554.894886	52.147277
3305.514290	389196.752421	52.152282
3304.660832	388829.966942	52.157287
3303.934410	388491.967519	52.162292
3303.305513	388141.489649	52.167297
3302.579265	387791.862891	52.172301
3301.810696	387443.154865	52.177306
3301.316886	387094.730597	52.182311
3300.406898	386747.284247	52.187316
3299.917024	386403.023106	52.192321
3299.373635	386053.248933	52.197325
3298.843226	385710.996624	52.202330
3298.099893	385360.764289	52.207335
3297.082489	385011.767194	52.212340
3296.894698	384661.160621	52.217345
3296.007915	384318.443127	52.222349
3295.448191	383969.440122	52.227354
3294.719982	383619.722983	52.232359
3294.124535	383276.186890	52.237364
3293.629146	382919.483565	52.242369
3292.438071	382580.231560	52.247373
3292.208545	382228.413472	52.252378
3291.586934	381877.773157	52.257383
3290.812049	381530.561839	52.262388
3290.093328	381166.527254	52.267393
3289.250572	380823.567556	52.272397
3288.817074	380475.529675	52.277402
3288.494601	380137.517404	52.282407
3287.640200	379786.309790	52.287412
3287.043545	379437.728818	52.292417
3286.004774	379078.939149	52.297421
3285.436402	378722.284599	52.302426
3284.684810	378372.726668	52.307431
3283.902667	378032.810352	52.312436
3283.356029	377683.697154	52.317441
3282.674092	377335.441645	52.322445
3282.063644	376988.850534	52.327450
3281.413507	376645.518487	52.332455
3280.301594	376298.415659	52.337460
3279.917297	375938.476547	52.342465
3278.933913	375607.117988	52.347469
3278.742088	375260.827285	52.352474
3278.113822	374919.155880	52.357479
3276.859106	374575.494825	52.362484
3276.705075	374224.407112	52.367489
3275.774731	373896.790971	52.372493
3275.315985	373540.988753	52.377498
3274.749357	373195.706472	52.382503
3273.712103	372846.196663	52.387508
3273.439319	372503.787553	52.392513
3272.444270	372161.133718	52.397517
3271.816040	371813.789168	52.402522
3271.193672	371470.841794	52.407527
3270.007761	371138.080186	52.412532
3269.723885	370788.484931	52.417537
3269.123366	370452.267323	52.422541
3268.344169	370100.506046	52.427546
3267.805872	369771.142025	52.432551
3267.027846	369434.054070	52.437556
3266.518127	369080.359214	52.442561
3265.833265	368748.110314	52.447565
3265.035565	368401.044615	52.452570
3264.500154	368062.915405	52.457575
3263.979193	367718.064763	52.462580
3263.150216	367378.602859	52.467585
3262.409083	367041.286992	52.472589
3261.790694	366702.524383	52.477594
3261.110623	366361.173838	52.482599
3260.211355	366013.876383	52.487604
3259.745553	365669.535335	52.492609
3258.882204	365334.184927	52.497613
3258.121980	364996.780272	52.502618
3257.638213	364651.874530	52.507623
3256.680793	364323.859119	52.512628
3256.345223	363982.537805	52.517633
3255.349339	363652.793489	52.522637
3254.842862	363310.094785	52.527642
3254.113997	362983.992797	52.532647
3253.393004	362648.498331	52.537652
3252.810138	362305.295369	52.542657
3252.153419	361981.744807	52.547661
3251.574627	361651.971149	52.552666
3250.861642	361299.952035	52.557671
3250.104512	360976.283193	52.562676
3249.942706	360635.215140	52.567681
3248.906082	360301.585870	52.572685
3248.376856	359959.298806	52.577690
3247.436600	359627.532563	52.582695
3246.661201	359297.468285	52.587700
3246.450655	358951.917430	52.592705
3245.260581	358618.962339	52.597709
3244.589003	358284.523393	52.602714
3244.164550	357955.386886	52.607719
3243.400131	357621.365236	52.612724
3242.690701	357291.226026	52.617729
3242.226499	356961.045821	52.622733
3241.360102	356628.662209	52.627738
3240.816664	356304.190398	52.632743
3239.779667	355971.905736	52.637748
3239.783487	355625.076152	52.642753
3238.582947	355303.679217	52.647757
3237.590704	354973.747567	52.652762
3237.328595	354647.617347	52.657767
3236.337540	354324.119755	52.662772
3236.224954	353989.410953	52.667777
3235.257451	353665.625548	52.672781
3234.611335	353321.784288	52.677786
3233.977476	352997.916482	52.682791
3233.387651	352672.410936	52.687796
3232.749066	352334.237185	52.692801
3231.801917	352015.044673	52.697805
3231.292057	351675.166644	52.702810
3231.026594	351343.417248	52.707815
3229.932805	351026.583380	52.712820
3229.525233	350685.257638	52.717825
3228.904653	350364.069338	52.722829
3228.277456	350028.907747	52.727834
3227.219296	349690.987206	52.732839
3226.473208	349366.046113	52.737844
3226.047960	349032.577106	52.742849
3225.149915	348708.572388	52.747853
3224.290888	348385.475846	52.752858
3223.703828	348050.193985	52.757863
3223.089772	347735.606646	52.762868
3222.865446	347402.223295	52.767873
3221.985965	347082.354823	52.772877
3221.441170	346744.335089	52.777882
3220.772491	346413.357779	52.782887
3219.879716	346091.551433	52.787892
3219.348728	345757.901480	52.792897
3218.443058	345432.911894	52.797901
3217.764357	345103.888466	52.802906
3217.217469	344781.714646	52.807911
3216.273527	344464.208880	52.812916
3215.978720	344128.374113	52.817921
3215.313129	343821.205798	52.822925
3214.653314	343483.185185	52.827930
3214.079816	343154.617793	52.832935
3213.242181	342840.319103	52.837940
3212.807926	342499.762749	52.842945
3212.065740	342177.300194	52.847949
3211.051384	341852.231724	52.852954
3210.342035	341519.196931	52.857959
3209.691418	341198.878326	52.862964
3209.489897	340879.021558	52.867969
3208.559565	340552.380153	52.872973
3207.826322	340217.051152	52.877978
3207.190528	339888.195987	52.882983
3206.225266	339575.351659	52.887988
3205.688594	339249.812106	52.892993
3204.859850	338922.153360	52.897997
3204.403901	338606.958130	52.903002
3203.954376	338285.192739	52.908007
3202.972242	337968.906638	52.913012
3202.267315	337637.479712	52.918017
3201.541512	337326.953895	52.923021
3201.123402	336996.140187	52.928026
3200.366438	336663.367355	52.933031
3199.603800	336359.410530	52.938036
3199.221100	336033.066728	52.943041
3197.992148	335718.819878	52.948045
3197.591048	335392.577681	52.953050
3197.332591	335076.315942	52.958055
3196.584261	334751.983936	52.963060
3196.015456	334425.330828	52.968065
3194.990987	334110.153145	52.973069
3194.499131	333783.764837	52.978074
3193.920743	333465.967890	52.983079
3192.939106	333150.346271	52.988084
3192.486886	332820.128503	52.993089
3191.984521	332498.318244	52.998093
3191.107762	332177.915022	53.003098
3190.215620	331851.148240	53.008103
3189.580989	331540.301584	53.013108
3188.800641	331217.842137	53.018113
3188.010403	330897.113994	53.023117
3187.450609	330575.838807	53.028122
3187.075020	330263.443629	53.033127
3186.097081	329950.531400	53.038132
3185.625740	329632.293155	53.043137
3184.920469	329318.011252	53.048141
3183.934277	328999.953590	53.053146
3183.352285	328682.670795	53.058151
3182.874094	328380.518588	53.063156
3182.369069	328057.772691	53.068161
3181.385083	327754.094069	53.073165
3180.504020	327432.779849	53.078170
3180.282414	327113.829571	53.083175
3179.314835	326804.899907	53.088180
3178.847760	326486.571478	53.093185
3178.290654	326181.520727	53.098189
3177.510624	325866.931028	53.103194
3177.173765	325550.233153	53.108199
3176.213884	325236.000410	53.113204
3175.731231	324904.046807	53.118209
3175.315759	324599.756914	53.123213
3174.223622	324285.770565	53.128218
3173.806659	323952.809741	53.133223
3172.450026	323638.633627	53.138228
3172.088305	323334.381489	53.143233
3171.146199	323020.443006	53.148237
3170.803905	322713.919514	53.153242
3169.934532	322393.983822	53.158247
3169.467572	322088.190721	53.163252
3168.741640	321773.831527	53.168257
3167.845395	321466.856529	53.173261
3167.238264	321163.832190	53.178266
3166.837532	320849.901990	53.183271
3166.066605	320533.661293	53.188276
3165.419254	320219.615109	53.193281
3164.283880	319917.001088	53.198285
3163.879513	319603.550862	53.203290
3163.200007	319301.626526	53.208295
3162.616751	319007.935738	53.213300
3162.361602	318683.713679	53.218305
3161.389657	318386.084821	53.223309
3160.560549	318073.460459	53.228314
3160.301641	317761.890664	53.233319
3159.194220	317446.685610	53.238324
3158.475297	317141.399456	53.243329
3157.806525	316832.743302	53.248333
3157.242780	316526.590377	53.253338
3156.831913	316211.678494	53.258343
3155.708503	315913.811287	53.263348
3155.590228	315592.485365	53.268353
3154.614027	315300.143998	53.273357
3153.733196	314983.902101	53.278362
3153.492813	314683.447049	53.283367
3152.285574	314387.014529	53.288372
3151.894752	314082.176336	53.293377
3151.002335	313777.212895	53.298381
3150.421743	313463.821672	53.303386
3149.882224	313163.333150	53.308391
3148.805390	312864.456618	53.313396
3148.325038	312545.673954	53.318401
3147.710866	312259.199855	53.323405
3146.940896	311961.316291	53.328410
3146.716579	311654.866033	53.333415
3146.018184	311355.237942	53.338420
3145.387527	311050.836511	53.343425
3144.674540	310748.713605	53.348429
3143.966783	310439.306248	53.353434
3143.275062	310136.541741	53.358439
3142.331871	309832.874036	53.363444
3141.785801	309509.560428	53.368449
3141.214207	309221.136563	53.373453
3140.530806	308919.055126	53.378458
3140.029754	308607.089195	53.383463
3139.287665	308316.296427	53.388468
3138.527229	308007.858674	53.393473
3137.896264	307712.208548	53.398477
3136.842603	307401.141845	53.403482
3136.364200	307099.711021	53.408487
3135.530564	306801.849873	53.413492
3135.134120	306503.129433	53.418497
3134.416970	306203.644151	53.423501
3133.578017	305903.133368	53.428506
3133.064604	305595.440073	53.433511
3132.102329	305310.735998	53.438516
3131.847832	305003.382346	53.443521
3131.367736	304706.453643	53.448525
3130.413378	304404.098753	53.453530
3129.970337	304101.534967	53.458535
3129.043237	303805.871929	53.463540
3128.478338	303501.747246	53.468545
3128.110291	303198.558466	53.473549
3127.233066	302901.204902	53.478554
3126.598232	302597.649613	53.483559
3125.554645	302307.477091	53.488564
3124.962223	302000.272219	53.493569
3124.135076	301702.195256	53.498573
3123.887943	301401.402917	53.503578
3123.329286	301096.075359	53.508583
3122.395054	300797.427851	53.513588
3121.929552	300491.091181	53.518593
3121.159360	300190.073663	53.523597
3120.404844	299891.192277	53.528602
3119.883213	299599.225831	53.533607
3118.973193	299306.861921	53.538612
3118.275833	298993.988747	53.543617
3117.532276	298703.150900	53.548621
3116.879326	298412.629284	53.553626
3116.288325	298103.990569	53.558631
3115.556943	297814.295292	53.563636
3115.090169	297521.934594	53.568641
3114.628019	297234.564180	53.573645
3113.454825	296928.893290	53.578650
3112.937664	296620.749666	53.583655
3112.340713	296348.933993	53.588660
3111.783355	296043.011400	53.593665
3111.170840	295746.825441	53.598669
3110.451308	295452.489589	53.603674
3110.053500	295157.287442	53.608679
3109.071238	294859.656093	53.613684
3108.215763	294563.685076	53.618689
3107.512752	294263.283683	53.623693
3106.843007	293971.178909	53.628698
3106.369244	293671.810019	53.633703
3105.579243	293399.104076	53.638708
3105.258893	293086.288835	53.643713
3104.217684	292793.477230	53.648717
3103.581084	292513.665996	53.653722
3102.970445	292202.729114	53.658727
3102.103068	291917.299904	53.663732
3101.809796	291624.062855	53.668737
3101.121307	291330.760650	53.673741
3100.183702	291039.433046	53.678746
3099.491075	290743.584043	53.683751
3098.773873	290448.375274	53.688756
3098.203901	290155.384023	53.693761
3097.612970	289865.757496	53.698765
3096.891887	289575.820170	53.703770
3096.205503	289273.703475	53.708775
3095.700357	288995.471992	53.713780
3094.962191	288700.519315	53.718785
3094.067432	288406.202344	53.723789
3093.575059	288116.838570	53.728794
3092.839946	287824.227579	53.733799
3092.075855	287538.930176	53.738804
3091.807200	287248.842558	53.743809
3090.921256	286956.356505	53.748813
3090.213319	286666.770839	53.753818
3089.652468	286370.769192	53.758823
3088.850497	286077.912544	53.763828
3087.963250	285784.916341	53.768833
3087.513303	285500.102346	53.773837
3086.958190	285208.683085	53.778842
3086.318927	284921.097130	53.783847
3085.314419	284636.701339	53.788852
3085.129649	284341.962924	53.793857
3083.822394	284053.157724	53.798861
3083.260477	283769.557226	53.803866
3082.994410	283484.432579	53.808871
3082.196395	283210.903544	53.813876
3081.389407	282915.014711	53.818881
3080.447070	282624.826527	53.823885
3080.224120	282338.115357	53.828890
3079.653697	282049.141409	53.833895
3078.565022	281768.704775	53.838900
3077.990123	281483.373202	53.843905
3077.408700	281194.680715	53.848909
3076.314240	280907.902996	53.853914
3076.220938	280615.949470	53.858919
3075.374758	280335.983184	53.863924
3074.938482	280055.162405	53.868929
3073.966841	279784.231541	53.873933
3072.983894	279488.801851	53.878938
3072.573318	279205.022381	53.883943
3072.028729	278929.974198	53.888948
3071.261452	278634.611970	53.893953
3070.692455	278342.299950	53.898957
3069.917830	278065.657964	53.903962
3069.065604	277783.577964	53.908967
3068.565814	277502.511802	53.913972
3068.152995	277221.533694	53.918977
3067.108688	276932.098096	53.923981
3066.344586	276655.326830	53.928986
3065.946466	276366.603874	53.933991
3065.234977	276097.821283	53.938996
3064.545826	275816.020785	53.944001
3064.174049	275532.820214	53.949005
3063.165551	275256.062018	53.954010
3062.533325	274975.092917	53.959015
3061.783877	274707.717012	53.964020
3061.129633	274427.948402	53.969025
3060.585098	274147.245572	53.974029
3059.819647	273870.703592	53.979034
3059.182733	273583.622839	53.984039
3058.461666	273312.396763	53.989044
3057.948280	273025.525724	53.994049
3057.386955	272740.012128	53.999053
3056.697169	272470.614914	54.004058
3056.041106	272191.763636	54.009063
3055.191852	271911.669559	54.014068
3054.748675	271626.952433	54.019073
3053.971008	271356.372304	54.024077
3053.425816	271072.944862	54.029082
3052.803268	270786.244316	54.034087
3051.839896	270515.719244	54.039092
3051.410179	270233.343421	54.044097
3050.544821	269951.214906	54.049101
3049.956483	269678.313108	54.054106
3049.363830	269389.876417	54.059111
3048.530141	269114.670556	54.064116
3047.858386	268831.926026	54.069121
3047.420683	268559.790308	54.074125
3046.775036	268284.809695	54.079130
3046.086812	267992.975952	54.084135
3045.237426	267718.257046	54.089140
3044.546240	267446.696758	54.094145
3044.131566	267156.093549	54.099149
3043.435696	266886.597202	54.104154
3042.734444	266607.602209	54.109159
3041.986060	266335.058276	54.114164
3041.198253	266056.026353	54.119169
3040.977129	265775.580564	54.124173
3040.027055	265502.737943	54.129178
3039.484264	265213.276754	54.134183
3038.386472	264948.556716	54.139188
3037.912044	264665.910529	54.144193
3037.470627	264388.123713	54.149197
3036.497064	264105.505978	54.154202
3035.899106	263818.932395	54.159207
3035.289271	263552.251424	54.164212
3034.669467	263269.145369	54.169217
3034.024811	262998.471841	54.174221
3033.169615	262728.926964	54.179226
3032.948957	262444.663281	54.184231
3032.042231	262172.478338	54.189236
3031.418907	261888.431668	54.194241
3030.746848	261609.486535	54.199245
3029.994318	261332.642750	54.204250
3029.617780	261060.680463	54.209255
3028.789913	260783.212405	54.214260
3028.306203	260496.419872	54.219265
3027.484643	260223.917563	54.224269
3026.632888	259937.260242	54.229274
3026.392275	259659.929539	54.234279
3025.423827	259385.490288	54.239284
3024.972515	259107.658677	54.244289
3024.269416	258822.838148	54.249293
3023.268706	258558.209897	54.254298
3022.770217	258274.936584	54.259303
3021.669932	257991.555099	54.264308
3021.544039	257717.646438	54.269313
3020.627157	257447.759801	54.274317
3019.842985	257167.894697	54.279322
3019.506859	256889.639863	54.284327
3018.499385	256632.807821	54.289332
3017.772827	256349.547430	54.294337
3016.764418	256079.651417	54.299341
3016.612921	255809.238097	54.304346
3015.822383	255537.805699	54.309351
3014.967900	255268.675817	54.314356
3014.267177	254992.976873	54.319361
3013.541498	254733.657627	54.324365
3012.791703	254476.201627	54.329370
3012.531893	254195.238674	54.334375
3011.833821	253940.143612	54.339380
3011.173280	253661.613277	54.344385
3010.767675	253394.095661	54.349389
3009.667212	253126.943067	54.354394
3009.182202	252845.431965	54.359399
3008.449924	252587.339015	54.364404
3007.977796	252312.804602	54.369409
3007.348509	252048.125662	54.374413
3006.164193	251780.071478	54.379418
3005.947294	251504.122689	54.384423
3005.061965	251236.454936	54.389428
3004.369628	250967.076249	54.394433
3003.677469	250701.849010	54.399437
3002.867483	250430.401524	54.404442
3002.617150	250172.337686	54.409447
3001.658577	249907.866926	54.414452
3000.990994	249631.916096	54.419457
3000.593222	249372.781786	54.424461
2999.793143	249112.845712	54.429466
2999.370230	248831.280388	54.434471
2998.485531	248572.835636	54.439476
2997.652515	248306.081138	54.444481
2997.359706	248038.630403	54.449485
2996.413646	247761.580932	54.454490
2995.816649	247496.012858	54.459495
2994.804420	247236.011644	54.464500
2994.368444	246975.537681	54.469505
2993.601257	246702.409088	54.474509
2992.667769	246445.452718	54.479514
2992.396943	246181.923583	54.484519
2991.659107	245923.612949	54.489524
2991.205741	245659.247833	54.494529
2990.398438	245392.087073	54.499533
2989.622555	245129.658468	54.504538
2989.185879	244867.762378	54.509543
2988.554846	244602.765285	54.514548
2987.862551	244333.500194	54.519553
2987.249865	244066.565865	54.524557
2986.141968	243809.158131	54.529562
2985.869873	243533.716435	54.534567
2984.868666	243272.294796	54.539572
2984.586851	243012.847963	54.544577
2983.863083	242747.181695	54.549581
2983.174680	242485.941321	54.554586
2982.305446	242221.928945	54.559591
2981.864453	241965.998157	54.564596
2981.130778	241690.786275	54.569601
2980.671058	241425.412042	54.574605
2979.616913	241174.927584	54.579610
2979.243610	240895.891630	54.584615
2978.392025	240643.644593	54.589620
2977.497133	240376.329815	54.594625
2977.101569	240115.277303	54.599629
2976.147593	239856.809292	54.604634
2975.997282	239594.853312	54.609639
2974.978905	239333.111722	54.614644
2974.553251	239065.343683	54.619649
2973.534813	238812.541309	54.624653
2973.125748	238551.800019	54.629658
2972.717645	238283.929178	54.634663
2971.480733	238026.808751	54.639668
2970.562601	237766.429972	54.644673
2970.094581	237513.085038	54.649677
2969.741901	237257.710770	54.654682
2969.214339	236990.574958	54.659687
2968.171838	236739.639976	54.664692
2967.805984	236476.503136	54.669697
2967.342628	236214.222680	54.674701
2966.787928	235947.883134	54.679706
2966.290618	235686.627909	54.684711
2965.023404	235418.798279	54.689716
2964.758690	235154.986666	54.694721
2963.974743	234899.406230	54.699725
2962.943637	234636.328386	54.704730
2962.412150	234366.373417	54.709735
2961.550769	234112.793349	54.714740
2961.136609	233854.814378	54.719745
2960.344114	233594.578814	54.724749
2959.706240	233338.342622	54.729754
2959.130602	233081.104184	54.734759
2958.290897	232824.977664	54.739764
2957.855901	232563.924340	54.744769
2956.934488	232308.703314	54.749773
2956.499604	232054.424454	54.754778
2956.060425	231780.184210	54.759783
2955.056334	231527.346380	54.764788
2954.449350	231265.330774	54.769793
2953.925976	231005.848907	54.774797
2953.082890	230748.608137	54.779802
2952.669559	230488.804738	54.784807
2951.289391	230232.898074	54.789812
2951.055882	229974.824552	54.794817
2950.245793	229716.155555	54.799821
2949.546374	229470.073484	54.804826
2949.173201	229206.804531	54.809831
2948.450819	228956.449886	54.814836
2947.370243	228691.664870	54.819841
2946.835353	228437.717346	54.824845
2945.843643	228184.530334	54.829850
2945.717434	227938.489056	54.834855
2944.877797	227682.427720	54.839860
2944.233917	227429.773445	54.844865
2944.069873	227172.995587	54.849869
2942.996509	226928.863947	54.854874
2942.646787	226658.469763	54.859879
2941.782869	226408.985057	54.864884
2940.870738	226141.176747	54.869889
2940.368287	225893.596842	54.874893
2939.281863	225640.317759	54.879898
2939.033984	225379.497592	54.884903
2937.904621	225130.797079	54.889908
2937.677663	224878.619108	54.894913
2937.095555	224636.427771	54.899917
2936.185539	224379.343732	54.904922
2935.734964	224124.415561	54.909927
2935.065502	223875.951589	54.914932
2934.517035	223627.558341	54.919937
2934.187461	223367.024880	54.924941
2932.974326	223112.360676	54.929946
2932.445066	222845.597346	54.934951
2931.372957	222605.411945	54.939956
2930.954020	222349.847945	54.944961
2930.531618	222093.865242	54.949965
2929.874953	221848.753577	54.954970
2929.330095	221586.745252	54.959975
2928.475736	221339.960705	54.964980
2927.903571	221079.638763	54.969985
2927.040916	220819.605563	54.974989
2926.443735	220573.253782	54.979994
2925.735939	220305.458206	54.984999
2925.167239	220061.967748	54.990004
2924.669818	219804.375222	54.995009
2924.085229	219554.091374	55.000013
2923.077151	219305.237466	55.005018
2922.634218	219031.268955	55.010023
2921.900206	218779.292925	55.015028
2921.446414	218528.088074	55.020033
2920.867371	218280.773612	55.025037
2920.074162	218018.320687	55.030042
2919.298892	217746.968195	55.035047
2918.558903	217504.086165	55.040052
2917.863165	217247.094147	55.045057
2917.306595	216989.075430	55.050061
2916.492413	216743.318256	55.055066
2915.876249	216480.461092	55.060071
2914.655364	216222.728559	55.065076
2913.688277	215972.390436	55.070081
2913.603444	215728.672525	55.075085
2912.703637	215476.594422	55.080090
2912.327712	215237.277558	55.085095
2911.417959	214990.205191	55.090100
2911.121416	214739.625363	55.095105
2910.208295	214488.851317	55.100109
2909.438092	214255.302712	55.105114
2909.186525	214000.225325	55.110119
2908.341537	213752.727169	55.115124
2907.425249	213504.897548	55.120129
2906.795700	213257.367115	55.125133
2905.991208	213015.325734	55.130138
2905.746941	212759.284579	55.135143
2904.889065	212520.015490	55.140148
2904.474490	212269.374498	55.145153
2903.822660	212019.090231	55.150157
2903.000080	211778.660008	55.155162
2902.325805	211529.004854	55.160167
2901.997396	211278.875881	55.165172
2900.893962	211028.654212	55.170177
2900.191560	210775.646265	55.175181
2899.607929	210534.215538	55.180186
2899.100597	210283.660578	55.185191
2898.186902	210052.186128	55.190196
2897.829203	209789.759942	55.195201
2897.212115	209539.823508	55.200205
2896.265638	209292.523913	55.205210
2895.745555	209050.605156	55.210215
2895.102646	208802.012148	55.215220
2894.106054	208555.703430	55.220225
2893.621512	208314.761926	55.225229
2892.697518	208073.763670	55.230234
2892.443858	207824.463881	55.235239
2891.679368	207577.422339	55.240244
2891.179027	207336.499913	55.245249
2890.835564	207084.048316	55.250253
2889.885870	206836.670028	55.255258
2889.236080	206574.621970	55.260263
2888.558434	206333.998888	55.265268
2888.034451	206089.865280	55.270273
2887.460917	205831.359206	55.275277
2886.518886	205585.015761	55.280282
2886.336403	205328.066266	55.285287
2885.059349	205086.652280	55.290292
2884.385990	204832.646172	55.295297
2884.024429	204578.680886	55.300301
2883.302469	204339.740132	55.305306
2882.620897	204081.818835	55.310311
2881.506802	203838.602519	55.315316
2881.227243	203583.877750	55.320321
2880.550567	203338.087204	55.325325
2879.650888	203095.069160	55.330330
2879.322748	202845.929452	55.335335
2878.597848	202600.786027	55.340340
2877.139275	202354.856279	55.345345
2877.279880	202114.235659	55.350349
2876.440027	201868.171891	55.355354
2875.785003	201623.008929	55.360359
2875.090039	201382.307408	55.365364
2874.608593	201128.007436	55.370369
2874.036103	200888.828479	55.375373
2873.165389	200639.173647	55.380378
2872.762825	200389.458545	55.385383
2872.104433	200137.469033	55.390388
2871.302505	199896.994531	55.395393
2870.862156	199639.666256	55.400397
2869.695635	199395.446791	55.405402
2869.080456	199146.038274	55.410407
2868.762720	198901.355782	55.415412
2867.824234	198655.563797	55.420417
2867.351499	198403.871074	55.425421
2866.641899	198170.948367	55.430426
2865.707680	197916.200640	55.435431
2864.959221	197669.110601	55.440436
2864.434693	197431.669914	55.445441
2863.858726	197178.955889	55.450445
2862.824739	196939.994752	55.455450
2862.312025	196699.157976	55.460455
2861.783684	196459.330031	55.465460
2861.134041	196214.979707	55.470465
2860.611164	195966.882162	55.475469
2859.770474	195734.258219	55.480474
2859.515362	195482.290522	55.485479
2858.675176	195232.541670	55.490484
2857.678582	194996.204779	55.495489
2857.166025	194748.874921	55.500493
2856.385272	194511.131875	55.505498
2855.944551	194260.777374	55.510503
2855.114249	194020.028851	55.515508
2854.364411	193780.184862	55.520513
2853.600532	193534.542114	55.525517
2852.812571	193302.722524	55.530522
2852.509610	193059.681131	55.535527
2851.914032	192826.713584	55.540532
2851.073819	192586.546072	55.545537
2850.587975	192335.953833	55.550541
2849.845886	192092.604985	55.555546
2849.348253	191840.363056	55.560551
2848.513213	191607.502776	55.565556
2847.747952	191370.319319	55.570561
2847.317675	191125.615368	55.575565
2846.314712	190882.084805	55.580570
2845.918820	190633.153755	55.585575
2844.983371	190398.813800	55.590580
2844.282372	190166.320871	55.595585
2843.857612	189922.729015	55.600589
2843.042084	189688.080891	55.605594
2842.580577	189442.868746	55.610599
2841.763941	189204.877043	55.615604
2841.070766	188971.269053	55.620609
2840.892604	188722.453364	55.625613
2839.933115	188484.933176	55.630618
2839.249775	188238.960833	55.635623
2838.438560	188004.129489	55.640628
2837.721930	187756.345617	55.645633
2837.231429	187514.175978	55.650637
2836.581128	187279.882560	55.655642
2836.209577	187036.958662	55.660647
2835.271730	186800.715795	55.665652
2834.650169	186553.750192	55.670657
2834.102537	186306.863255	55.675661
2833.109670	186070.263889	55.680666
2832.937221	185830.457119	55.685671
2831.989240	185580.647824	55.690676
2831.307879	185342.463537	55.695681
2830.578037	185107.850249	55.700685
2829.837301	184868.342062	55.705690
2829.286810	184623.309290	55.710695
2828.373104	184389.619339	55.715700
2827.742036	184150.199354	55.720705
2827.494461	183910.274663	55.725709
2826.147417	183680.867786	55.730714
2825.900921	183431.760697	55.735719
2825.000750	183197.756770	55.740724
2824.687921	182962.897794	55.745729
2823.606897	182721.483165	55.750733
2823.231826	182475.162251	55.755738
2822.756532	182239.658619	55.760743
2821.957214	182012.183517	55.765748
2821.277819	181774.272295	55.770753
2820.851493	181538.255830	55.775757
2819.898391	181298.889490	55.780762
2819.421461	181057.706338	55.785767
2818.675830	180825.738543	55.790772
2817.722283	180574.482601	55.795777
2817.489332	180334.485985	55.800781
2816.442745	180114.666703	55.805786
2816.039129	179870.718244	55.810791
2815.564658	179622.063220	55.815796
2814.691969	179377.403198	55.820801
2814.165312	179144.239525	55.825805
2813.114364	178907.153380	55.830810
2812.475835	178666.594323	55.835815
2812.199306	178433.471249	55.840820
2811.183055	178191.690006	55.845825
2810.974457	177951.970019	55.850829
2809.775330	177720.357986	55.855834
2808.930398	177469.599183	55.860839
2808.228198	177239.933503	55.865844
2807.600259	177005.411252	55.870849
2807.196713	176776.527577	55.875853
2806.375936	176554.045402	55.880858
2805.684010	176307.581159	55.885863
2805.322334	176076.964904	55.890868
2804.574567	175846.500113	55.895873
2803.951674	175613.180514	55.900877
2803.259953	175381.539307	55.905882
2802.708279	175137.272923	55.910887
2802.207934	174906.519842	55.915892
2801.152315	174663.468061	55.920897
2800.883315	174424.032405	55.925901
2800.126563	174197.788154	55.930906
2799.140558	173958.824911	55.935911
2798.835454	173714.299080	55.940916
2797.961582	173477.940897	55.945921
2797.314169	173244.066434	55.950925
2796.268537	173012.393042	55.955930
2796.447831	172772.972483	55.960935
2795.321149	172546.401834	55.965940
2794.550602	172309.016741	55.970945
2794.165485	172068.036472	55.975949
2793.331910	171842.440834	55.980954
2792.657971	171599.703232	55.985959
2791.811043	171364.141795	55.990964
2791.244482	171131.831195	55.995969
2790.743049	170894.005005	56.000973
2789.965004	170668.661634	56.005978
2789.741978	170428.237985	56.010983
2788.483124	170201.867047	56.015988
2787.964169	169959.140472	56.020993
2787.745364	169728.067555	56.025997
2786.926353	169488.036588	56.031002
2786.078469	169249.588575	56.036007
2785.350394	169016.565855	56.041012
2784.626788	168783.073315	56.046017
2784.115272	168538.548692	56.051021
2783.610380	168317.982611	56.056026
2782.776795	168076.792819	56.061031
2782.545920	167841.371364	56.066036
2781.559982	167605.702172	56.071041
2781.352195	167363.629362	56.076045
2780.393397	167131.544799	56.081050
2779.124293	166888.765694	56.086055
2778.678918	166648.553483	56.091060
2777.747455	166413.480735	56.096065
2777.577630	166173.698399	56.101069
2776.395540	165968.435978	56.106074
2775.815201	165658.950449	56.111079
2775.474646	165417.292639	56.116084
2774.554603	165196.429055	56.121089
2774.479669	164961.420501	56.126093
2773.423934	164723.364502	56.131098
2772.825058	164483.533825	56.136103
2772.119840	164251.897425	56.141108
2771.695394	164019.048217	56.146113
2771.135504	163788.764943	56.151117
2770.403314	163550.182099	56.156122
2769.603511	163313.353455	56.161127
2769.019561	163079.263983	56.166132
2767.993060	162846.085277	56.171137
2767.957718	162595.789754	56.176141
2766.939219	162366.236527	56.181146
2766.568978	162129.334829	56.186151
2765.591501	161900.579067	56.191156
2765.118394	161660.950422	56.196161
2764.364336	161408.996935	56.201165
2763.125939	161184.164884	56.206170
2762.870756	160938.467321	56.211175
2762.181440	160712.419711	56.216180
2761.316837	160485.765601	56.221185
2761.018998	160247.440884	56.226189
2760.097356	160009.051288	56.231194
2759.457788	159773.733454	56.236199
2758.560144	159557.528390	56.241204
2758.064330	159313.342212	56.246209
2757.449589	159075.037428	56.251213
2756.625149	158862.473767	56.256218
2756.201349	158619.946431	56.261223
2755.709575	158394.200159	56.266228
2754.594401	158163.418010	56.271233
2754.114960	157934.100386	56.276237
2753.850462	157697.529305	56.281242
2752.824515	157465.618907	56.286247
2751.813080	157240.051404	56.291252
2751.726893	157007.054479	56.296257
2751.248117	156764.167382	56.301261
2750.050058	156543.884258	56.306266
2749.760860	156301.339052	56.311271
2749.343273	156074.617261	56.316276
2748.472203	155840.303338	56.321281
2747.922951	155601.656061	56.326285
2747.022930	155367.807595	56.331290
2746.468549	155131.910209	56.336295
2745.671545	154907.480842	56.341300
2744.856738	154667.877927	56.346305
2744.416310	154421.683605	56.351309
2743.538904	154202.063940	56.356314
2742.781081	153959.202848	56.361319
2742.184447	153729.474280	56.366324
2741.562762	153501.213050	56.371329
2741.030898	153267.740248	56.376333
2740.351502	153045.135050	56.381338
2739.542894	152802.493741	56.386343
2738.955147	152573.801278	56.391348
2738.389867	152343.162060	56.396353
2737.769030	152103.584840	56.401357
2737.005200	151877.441791	56.406362
2736.442487	151636.638508	56.411367
2735.835054	151403.826270	56.416372
2734.908503	151172.578762	56.421377
2734.388013	150940.175468	56.426381
2733.426026	150717.338312	56.431386
2733.170375	150476.278792	56.436391
2732.583977	150250.004412	56.441396
2731.666859	150024.012763	56.446401
2731.319338	149776.821313	56.451405
2730.030241	149548.210097	56.456410
2729.399578	149328.634479	56.461415
2729.175109	149089.423173	56.466420
2728.238639	148863.226593	56.471425
2727.741346	148622.155524	56.476429
2727.127077	148394.119158	56.481434
2726.786900	148166.028279	56.486439
2725.933045	147944.921467	56.491444
2724.925172	147708.678637	56.496449
2724.581162	147465.647463	56.501453
2723.582536	147243.094184	56.506458
2722.873892	147018.424986	56.511463
2722.202306	146784.169131	56.516468
2721.616459	146545.834660	56.521473
2721.184747	146323.096340	56.526477
2720.135713	146095.183370	56.531482
2719.655088	145862.263873	56.536487
2719.040991	145636.560107	56.541492
2718.156784	145402.398984	56.546497
2717.749728	145171.264787	56.551501
2716.895663	144951.843605	56.556506
2716.138715	144716.765168	56.561511
2715.619760	144489.110267	56.566516
2715.155158	144267.179586	56.571521
2714.339574	144029.116592	56.576525
2713.653125	143798.595930	56.581530
2712.972596	143568.546213	56.586535
2712.239418	143347.821008	56.591540
2711.498057	143124.404740	56.596545
2711.092949	142894.138501	56.601549
2710.355319	142676.404972	56.606554
2709.564628	142442.200467	56.611559
2709.084796	142215.712391	56.616564
2708.344718	141986.611497	56.621569
2707.634422	141756.427531	56.626573
2706.647632	141541.969010	56.631578
2706.072002	141315.972905	56.636583
2705.556764	141090.947300	56.641588
2704.815054	140870.647857	56.646593
2704.477010	140640.718293	56.651597
2703.421785	140413.623188	56.656602
2702.811003	140187.450450	56.661607
2702.210470	139970.286276	56.666612
2701.635529	139740.769546	56.671617
2700.835425	139514.009259	56.676621
2700.434321	139307.313202	56.681626
2699.814203	139072.040368	56.686631
2699.245098	138844.397271	56.691636
2697.978321	138622.787119	56.696641
2697.731778	138393.266785	56.701645
2696.749500	138177.141658	56.706650
2696.441160	137950.683758	56.711655
2695.691746	137723.916306	56.716660
2694.945503	137498.014015	56.721665
2694.496329	137268.585277	56.726669
2693.262863	137056.967476	56.731674
2693.308798	136825.227718	56.736679
2692.656494	136597.907213	56.741684
2691.960003	136375.905898	56.746689
2691.362145	136149.126524	56.751693
2690.510703	135926.683092	56.756698
2689.768098	135694.696035	56.761703
2688.870676	135460.804338	56.766708
2688.084034	135247.756760	56.771713
2687.862107	135011.805249	56.776717
2686.850675	134799.736640	56.781722
2686.506675	134580.195751	56.786727
2686.044494	134350.410808	56.791732
2684.913541	134129.524394	56.796737
2684.364301	133898.956512	56.801741
2683.620523	133680.133650	56.806746
2683.137031	133460.648761	56.811751
2682.446445	133234.198991	56.816756
2681.713459	133016.027322	56.821761
2681.384745	132789.079130	56.826765
2680.298858	132566.647831	56.831770
2679.934564	132334.500764	56.836775
2679.388019	132111.212706	56.841780
2678.397456	131887.768096	56.846785
2677.495058	131663.447516	56.851789
2677.139250	131439.842353	56.856794
2676.270871	131214.935625	56.861799
2675.629103	131007.663293	56.866804
2675.353302	130788.623322	56.871809
2674.444235	130548.663858	56.876813
2674.030124	130329.776378	56.881818
2673.075781	130107.495942	56.886823
2672.307279	129875.318744	56.891828
2671.573422	129668.007350	56.896833
2671.600150	129436.469883	56.901837
2670.661724	129215.260910	56.906842
2669.919323	128985.068349	56.911847
2669.164001	128762.513040	56.916852
2668.499046	128543.907878	56.921857
2668.123313	128314.704241	56.926861
2667.260811	128096.095797	56.931866
2666.572116	127868.202801	56.936871
2665.828321	127642.682705	56.941876
2664.825178	127427.797668	56.946881
2664.514683	127204.155666	56.951885
2663.650108	126982.444790	56.956890
2663.013617	126766.668609	56.961895
2662.641853	126547.207284	56.966900
2661.812185	126333.624112	56.971905
2661.265247	126102.281605	56.976909
2660.516675	125890.975002	56.981914
2660.010170	125660.633104	56.986919
2659.477220	125431.376797	56.991924
2658.498741	125209.393549	56.996929
2658.027974	124980.880450	57.001933
2657.093615	124770.666019	57.006938
2656.620976	124548.773122	57.011943
2656.114979	124320.207680	57.016948
2655.175929	124105.808506	57.021953
2654.818867	123876.067631	57.026957
2653.857959	123664.621539	57.031962
2653.043044	123436.963339	57.036967
2652.666636	123207.624893	57.041972
2651.838859	123005.127994	57.046977
2651.392964	122774.191579	57.051981
2650.595116	122557.801472	57.056986
2649.982765	122331.352297	57.061991
2649.135033	122103.164632	57.066996
2648.375082	121890.367447	57.072001
2648.186009	121661.406232	57.077005
2647.156374	121442.268427	57.082010
2646.695517	121224.604108	57.087015
2646.196474	121009.474409	57.092020
2645.250935	120789.947762	57.097025
2644.469713	120567.298799	57.102029
2643.595070	120347.256719	57.107034
2643.190300	120130.773364	57.112039
2642.374822	119912.896726	57.117044
2641.672335	119698.609872	57.122049
2641.158666	119477.387881	57.127053
2640.730529	119263.632468	57.132058
2640.127887	119037.025924	57.137063
2639.677865	118812.428577	57.142068
2638.695034	118598.569707	57.147073
2638.080948	118369.203011	57.152077
2637.166352	118158.853770	57.157082
2636.527473	117938.147137	57.162087
2635.929771	117718.553089	57.167092
2635.333820	117500.084195	57.172097
2634.848620	117274.128260	57.177101
2634.126171	117053.702680	57.182106
2633.344891	116837.553945	57.187111
2632.671036	116624.614598	57.192116
2631.957959	116405.729213	57.197121
2631.262732	116183.694500	57.202125
2630.683348	115967.825783	57.207130
2630.019895	115748.582694	57.212135
2629.452376	115522.921810	57.217140
2628.646494	115308.268816	57.222145
2628.072706	115087.087628	57.227149
2627.575707	114867.121204	57.232154
2626.825429	114649.964166	57.237159
2626.268671	114435.056925	57.242164
2625.474634	114215.695412	57.247169
2624.983435	113980.045933	57.252173
2623.996208	113768.017927	57.257178
2623.524420	113549.487015	57.262183
2622.885467	113327.138325	57.267188
2621.987557	113102.389137	57.272193
2621.564522	112881.038354	57.277197
2620.949882	112662.099871	57.282202
2620.160194	112449.410683	57.287207
2619.377183	112223.470710	57.292212
2618.778196	112011.637197	57.297217
2617.861198	111786.947275	57.302221
2616.997597	111569.993469	57.307226
2616.625969	111361.302639	57.312231
2616.157727	111141.852946	57.317236
2615.361538	110932.782407	57.322241
2614.750126	110710.268625	57.327245
2614.068501	110496.715938	57.332250
2613.280700	110271.187940	57.337255
2612.519570	110060.570794	57.342260
2611.818699	109847.915208	57.347265
2611.201017	109627.392109	57.352269
2610.397156	109426.858033	57.357274
2609.670279	109211.515110	57.362279
2609.374865	108998.015763	57.367284
2608.476112	108782.887868	57.372289
2607.876483	108571.496434	57.377293
2607.389065	108357.284327	57.382298
2606.890654	108140.245764	57.387303
2605.751760	107932.625692	57.392308
2604.982616	107719.149145	57.397313
2604.740425	107502.342178	57.402317
2603.509027	107296.639450	57.407322
2603.412071	107085.422398	57.412327
2603.083951	106868.089034	57.417332
2601.907644	106663.791579	57.422337
2601.389948	106438.306967	57.427341
2600.285882	106223.253330	57.432346
2599.761471	106010.470070	57.437351
2598.855495	105802.634696	57.442356
2598.068413	105603.214524	57.447361
2597.891553	105394.924525	57.452365
2597.242697	105192.224669	57.457370
2596.451692	104977.399071	57.462375
2596.097360	104776.565804	57.467380
2595.196647	104568.975060	57.472385
2594.639329	104353.299606	57.477389
2594.430608	104143.020719	57.482394
2593.397798	103929.461013	57.487399
2592.838560	103725.509592	57.492404
2592.093507	103507.727189	57.497409
2591.833250	103289.444904	57.502413
2590.833770	103083.868530	57.507418
2590.219737	102853.611514	57.512423
2589.352121	102646.222684	57.517428
2588.758154	102431.452357	57.522433
2588.192485	102216.546284	57.527437
2587.345475	102007.497718	57.532442
2586.628910	101794.998355	57.537447
2586.056493	101587.819495	57.542452
2585.077766	101380.415046	57.547457
2584.911412	101165.683699	57.552461
2584.041930	100956.787636	57.557466
2583.210443	100738.093060	57.562471
2582.790560	100526.687357	57.567476
2582.262795	100324.784031	57.572481
2581.558827	100108.333411	57.577485
2580.524515	99897.861772	57.582490
2580.070118	99691.638903	57.587495
2579.507963	99476.510127	57.592500
2578.571331	99272.650947	57.597505
2578.196592	99063.883812	57.602509
2577.430339	98855.129865	57.607514
2576.578213	98640.137293	57.612519
2576.132581	98437.000559	57.617524
2575.367496	98230.269127	57.622529
2575.004844	98015.147748	57.627533
2573.939371	97807.998360	57.632538
2573.408050	97596.472234	57.637543
2572.612805	97393.368434	57.642548
2572.058226	97185.046460	57.647553
2571.462806	96977.658859	57.652557
2570.725319	96765.608621	57.657562
2569.864379	96555.254301	57.662567
2569.483005	96352.195668	57.667572
2568.565089	96142.729432	57.672577
2568.160368	95931.071860	57.677581
2567.413767	95732.237119	57.682586
2566.964226	95528.803450	57.687591
2566.221540	95313.996123	57.692596
2565.117512	95109.471312	57.697601
2564.854235	94906.578163	57.702605
2563.957941	94696.456005	57.707610
2563.411672	94498.862408	57.712615
2563.246533	94287.397899	57.717620
2562.419884	94075.444098	57.722625
2561.908648	93866.879458	57.727629
2560.883021	93647.300600	57.732634
2560.190697	93429.763762	57.737639
2559.767655	93226.441851	57.742644
2559.017752	93014.479601	57.747649
2558.245414	92804.476039	57.752653
2557.676129	92603.478534	57.757658
2556.865277	92395.926307	57.762663
2556.284542	92173.964250	57.767668
2555.338507	91969.576284	57.772673
2554.735424	91761.381985	57.777677
2553.891724	91562.168494	57.782682
2553.383917	91358.528361	57.787687
2553.031624	91144.181183	57.792692
2552.077943	90943.253323	57.797697
2551.655991	90723.886709	57.802701
2551.089840	90525.735534	57.807706
2550.169986	90313.788036	57.812711
2549.686891	90102.261587	57.817716
2548.783388	89891.945087	57.822721
2548.713144	89692.556197	57.827725
2547.650654	89482.528783	57.832730
2546.857272	89276.892592	57.837735
2546.456999	89062.408499	57.842740
2545.579628	88860.910679	57.847745
2544.883351	88645.120811	57.852749
2544.446131	88445.167467	57.857754
2543.688465	88239.478350	57.862759
2543.163150	88022.241078	57.867764
2542.390282	87823.265943	57.872769
2541.751504	87602.684398	57.877773
2540.868230	87404.535764	57.882778
2540.371042	87196.843612	57.887783
2539.931996	86992.149218	57.892788
2538.893974	86781.611540	57.897793
2538.734128	86564.102779	57.902797
2537.606096	86347.364584	57.907802
2536.925143	86158.064199	57.912807
2536.678716	85938.572251	57.917812
2535.541964	85736.333252	57.922817
2535.065519	85533.059654	57.927821
2534.409788	85312.478922	57.932826
2533.346899	85120.852055	57.937831
2532.842998	84909.569836	57.942836
2532.303232	84707.404439	57.947841
2531.409813	84499.617383	57.952845
2530.529318	84303.037326	57.957850
2530.043536	84099.499967	57.962855
2529.603124	83901.972788	57.967860
2529.032482	83698.249889	57.972865
2528.439341	83490.304689	57.977869
2527.612129	83284.008611	57.982874
2527.028995	83082.898744	57.987879
2526.378884	82879.006180	57.992884
2525.425950	82684.208374	57.997889
2524.993363	82471.715856	58.002893
2524.185328	82274.091029	58.007898
2523.391402	82064.518425	58.012903
2523.130383	81864.687474	58.017908
2522.243266	81664.425265	58.022913
2522.143159	81464.496566	58.027917
2521.076626	81254.702733	58.032922
2520.445147	81046.502564	58.037927
2520.141615	80830.704210	58.042932
2518.958890	80642.477030	58.047937
2518.350811	80424.595340	58.052941
2517.968988	80219.399592	58.057946
2517.112382	80003.120751	58.062951
2516.387982	79803.224536	58.067956
2515.631726	79596.959879	58.072961
2515.472683	79390.881460	58.077965
2514.565226	79187.617052	58.082970
2513.830218	78985.607424	58.087975
2513.568333	78772.688271	58.092980
2512.384309	78578.998412	58.097985
2511.594888	78372.155549	58.102989
2510.950862	78164.214437	58.107994
2510.588042	77961.674243	58.112999
2510.097768	77753.788955	58.118004
2508.960815	77554.778350	58.123009
2508.757955	77345.400524	58.128013
2507.822149	77144.980618	58.133018
2507.069841	76940.991445	58.138023
2506.654346	76727.851694	58.143028
2505.912752	76525.227324	58.148033
2505.213930	76316.838417	58.153037
2504.764306	76116.484611	58.158042
2504.134212	75918.271354	58.163047
2503.515664	75701.315743	58.168052
2502.559313	75496.923501	58.173057
2502.045061	75282.097449	58.178061
2501.337574	75086.248926	58.183066
2500.629530	74875.550957	58.188071
2499.875675	74669.589001	58.193076
2499.177341	74460.522137	58.198081
2498.400992	74254.118143	58.203085
2498.131015	74058.558701	58.208090
2497.307179	73842.479205	58.213095
2496.691373	73639.014796	58.218100
2496.087329	73439.085781	58.223105
2495.377550	73221.651760	58.228109
2494.862566	73026.831748	58.233114
2493.801851	72819.923712	58.238119
2493.537750	72607.950077	58.243124
2492.621877	72403.899576	58.248129
2492.228497	72192.514667	58.253133
2491.354170	71993.352465	58.258138
2490.636859	71795.542052	58.263143
2489.974827	71589.337441	58.268148
2489.196394	71383.052061	58.273153
2488.696728	71173.234182	58.278157
2487.788100	70969.570987	58.283162
2487.006710	70770.932084	58.288167
2486.534449	70562.934358	58.293172
2485.544823	70372.763768	58.298177
2485.458749	70167.375813	58.303181
2484.449781	69972.619673	58.308186
2484.083433	69764.284177	58.313191
2483.044434	69566.071947	58.318196
2482.090049	69365.251287	58.323201
2481.946451	69162.891650	58.328205
2481.232852	68960.181064	58.333210
2480.514695	68758.106693	58.338215
2479.935514	68567.742800	58.343220
2478.999718	68368.937243	58.348225
2478.601521	68163.683025	58.353229
2477.673840	67972.689779	58.358234
2477.031199	67769.251896	58.363239
2476.617955	67567.344171	58.368244
2475.535413	67384.982259	58.373249
2475.146530	67170.661045	58.378253
2474.387761	66975.559374	58.383258
2473.616996	66779.175894	58.388263
2473.242755	66577.215259	58.393268
2472.482049	66388.206079	58.398273
2472.012220	66193.582624	58.403277
2471.146203	65994.631931	58.408282
2470.050105	65791.451300	58.413287
2469.925859	65593.713917	58.418292
2468.869791	65411.518369	58.423297
2468.609135	65213.280876	58.428301
2468.058051	65012.466527	58.433306
2467.225040	64813.779256	58.438311
2466.871274	64615.366363	58.443316
2465.949122	64414.262455	58.448321
2464.998940	64215.460630	58.453325
2464.675524	64020.671265	58.458330
2463.947953	63823.614466	58.463335
2463.531792	63616.796572	58.468340
2462.726270	63429.248322	58.473345
2462.207418	63211.664116	58.478349
2461.843562	63017.895023	58.483354
2460.853814	62820.712833	58.488359
2460.162910	62610.827696	58.493364
2459.612229	62403.195798	58.498369
2458.961429	62194.711412	58.503373
2458.433098	62001.564435	58.508378
2457.683455	61807.254649	58.513383
2457.086188	61587.361890	58.518388
2456.104871	61401.950941	58.523393
2455.656439	61186.955704	58.528397
2455.099404	60990.243132	58.533402
2454.522500	60775.931407	58.538407
2454.233709	60575.191881	58.543412
2453.111575	60375.305193	58.548417
2452.216858	60161.060340	58.553421
2451.648456	59962.768012	58.558426
2450.721363	59761.185530	58.563431
2450.501597	59562.598415	58.568436
2449.552641	59362.144266	58.573441
2448.889820	59149.998206	58.578445
2448.292135	58954.044595	58.583450
2447.678150	58753.917374	58.588455
2447.076981	58555.091206	58.593460
2446.473779	58348.680325	58.598465
2445.484213	58142.643173	58.603469
2444.743674	57948.485804	58.608474
2444.049119	57743.669216	58.613479
2443.534173	57542.285902	58.618484
2442.898025	57353.185581	58.623489
2442.151836	57149.412391	58.628493
2441.744080	56945.071889	58.633498
2441.082873	56745.622595	58.638503
2440.681108	56528.445353	58.643508
2439.685490	56336.051219	58.648513
2439.019829	56131.444099	58.653517
2438.043573	55932.332042	58.658522
2437.580617	55731.311495	58.663527
2436.921306	55525.890402	58.668532
2436.394810	55342.065819	58.673537
2435.763011	55128.865831	58.678541
2435.085257	54927.555827	58.683546
2434.103240	54737.853573	58.688551
2433.571343	54532.733528	58.693556
2432.781348	54337.061835	58.698561
2432.441519	54132.168996	58.703565
2431.625102	53937.002608	58.708570
2430.372634	53734.717739	58.713575
2430.347441	53530.123537	58.718580
2429.701305	53346.863257	58.723585
2428.824325	53154.993172	58.728589
2427.974707	52951.175378	58.733594
2427.612970	52756.281814	58.738599
2426.885913	52561.970362	58.743604
2425.951438	52361.223005	58.748609
2425.297871	52173.571119	58.753613
2424.888104	51981.174236	58.758618
2424.280761	51796.926741	58.763623
2423.479408	51581.539109	58.768628
2423.019579	51396.598356	58.773633
2422.534554	51191.467445	58.778637
2421.736071	50996.228603	58.783642
2420.844147	50798.228729	58.788647
2420.570796	50601.882620	58.793652
2419.827073	50410.302122	58.798657
2419.210034	50199.998830	58.803661
2418.655746	49998.173430	58.808666
2417.643997	49806.043914	58.813671
2417.151895	49602.264219	58.818676
2416.406825	49402.092460	58.823681
2415.963548	49199.024617	58.828685
2415.511204	48996.520484	58.833690
2414.325728	48801.572534	58.838695
2413.718693	48602.517266	58.843700
2412.775988	48411.900830	58.848705
2412.303200	48207.760693	58.853709
2411.725675	48008.568193	58.858714
2411.142303	47812.592906	58.863719
2410.597225	47618.843910	58.868724
2409.707625	47419.343708	58.873729
2409.155238	47216.600488	58.878733
2408.664868	47024.067203	58.883738
2408.026691	46822.673845	58.888743
2407.345698	46612.739375	58.893748
2406.375654	46423.467724	58.898753
2405.970433	46216.148166	58.903757
2405.407111	46020.591273	58.908762
2404.311210	45831.902640	58.913767
2403.993805	45620.808934	58.918772
2403.050058	45425.622623	58.923777
2402.586681	45229.258442	58.928781
2402.092969	45034.935038	58.933786
2401.195193	44832.868640	58.938791
2400.797716	44634.558649	58.943796
2399.710901	44447.230854	58.948801
2399.056335	44249.418275	58.953805
2398.693665	44054.857255	58.958810
2397.727190	43848.369449	58.963815
2397.390750	43647.957766	58.968820
2396.533798	43456.255470	58.973825
2395.627779	43263.611118	58.978829
2395.299339	43061.756434	58.983834
2394.366193	42866.306088	58.988839
2393.951054	42664.055477	58.993844
2392.981025	42479.329927	58.998849
2392.277216	42278.388250	59.003853
2391.816509	42086.840649	59.008858
2391.020352	41891.559836	59.013863
2390.666606	41688.545589	59.018868
2389.884879	41494.629939	59.023873
2389.233847	41292.812232	59.028877
2388.733366	41098.805844	59.033882
2387.873976	40904.627707	59.038887
2387.234418	40699.874293	59.043892
2386.893133	40513.764122	59.048897
2386.034340	40308.664350	59.053901
2385.047115	40110.572343	59.058906
2384.129538	39926.172559	59.063911
2383.618469	39730.052111	59.068916
2383.071323	39543.427020	59.073921
2382.333088	39341.418411	59.078925
2381.562276	39158.034414	59.083930
2380.858101	38962.154168	59.088935
2380.340188	38772.039046	59.093940
2379.685246	38595.058011	59.098945
2379.132489	38398.143730	59.103949
2378.340987	38196.579216	59.108954
2377.602427	38010.797988	59.113959
2377.287304	37812.079124	59.118964
2376.632913	37626.762993	59.123969
2375.793701	37439.170262	59.128973
2375.205332	37243.547533	59.133978
2374.500395	37055.789165	59.138983
2373.890207	36853.084799	59.143988
2373.322558	36664.981793	59.148993
2372.559118	36471.779445	59.153997
2372.142628	36277.994774	59.159002
2371.404778	36081.791152	59.164007
2370.817539	35887.004306	59.169012
2369.662445	35693.158540	59.174017
2369.316455	35506.120776	59.179021
2368.329090	35316.621516	59.184026
2367.718708	35133.086544	59.189031
2367.038339	34928.252684	59.194036
2366.535511	34746.754842	59.199041
2365.866969	34551.615468	59.204045
2365.295782	34360.783977	59.209050
2364.771711	34174.473649	59.214055
2363.999735	33979.870997	59.219060
2363.238576	33786.449481	59.224065
2362.476177	33579.860833	59.229069
2361.973205	33401.124380	59.234074
2360.812236	33211.298794	59.239079
2360.650729	33016.408302	59.244084
2359.339280	32836.306353	59.249089
2358.715249	32649.068081	59.254093
2358.438708	32464.758855	59.259098
2357.681831	32281.218427	59.264103
2357.168661	32099.152125	59.269108
2356.437296	31913.979300	59.274113
2355.921743	31719.850742	59.279117
2355.560589	31530.149867	59.284122
2354.514340	31339.728618	59.289127
2354.186860	31147.939350	59.294132
2353.296914	30964.090162	59.299137
2352.523956	30771.097564	59.304141
2351.818913	30580.591476	59.309146
2351.296660	30391.632395	59.314151
2350.766299	30200.535749	59.319156
2350.034564	30014.736472	59.324161
2349.402350	29820.536599	59.329165
2348.748919	29635.909493	59.334170
2347.802549	29443.533539	59.339175
2347.701892	29252.457217	59.344180
2346.822092	29063.348929	59.349185
2345.785907	28870.347745	59.354189
2345.361337	28685.216345	59.359194
2344.549800	28501.214855	59.364199
2343.930744	28294.657043	59.369204
2343.127020	28118.276937	59.374209
2342.533114	27930.698950	59.379213
2342.286008	27746.400037	59.384218
2341.412682	27558.839049	59.389223
2340.971411	27358.274613	59.394228
2340.083564	27184.576802	59.399233
2339.373642	26984.026416	59.404237
2338.726068	26791.874518	59.409242
2337.793277	26611.665573	59.414247
2337.677338	26424.955710	59.419252
2336.625510	26243.869297	59.424257
2335.994833	26050.599563	59.429261
2335.444123	25861.606679	59.434266
2334.548981	25670.806641	59.439271
2333.956949	25483.600264	59.444276
2333.460799	25310.422038	59.449281
2332.316279	25121.201862	59.454285
2331.838215	24936.936034	59.459290
2331.315874	24748.266841	59.464295
2330.836546	24564.670475	59.469300
2329.704434	24387.421211	59.474305
2329.153231	24201.107829	59.479309
2328.657823	24014.295755	59.484314
2327.979811	23835.750955	59.489319
2327.425273	23639.454500	59.494324
2326.801783	23460.465367	59.499329
2325.883958	23270.902569	59.504333
2325.187206	23100.710625	59.509338
2324.054152	22920.581953	59.514343
2323.661728	22730.158894	59.519348
2323.129455	22553.465020	59.524353
2322.569052	22376.128467	59.529357
2322.129824	22186.395284	59.534362
2321.072807	22017.777917	59.539367
2320.148114	21826.150334	59.544372
2319.701011	21654.636900	59.549377
2319.150967	21473.545424	59.554381
2318.581727	21296.462377	59.559386
2317.895133	21117.220625	59.564391
2317.205667	20937.321261	59.569396
2316.731179	20754.016761	59.574401
2316.021169	20573.275999	59.579405
2315.160306	20392.855738	59.584410
2313.908063	20217.264569	59.589415
2313.610847	20036.905852	59.594420
2312.923789	19865.938609	59.599425
2311.926333	19702.518232	59.604429
2311.557225	19530.141094	59.609434
2310.835837	19359.165066	59.614439
2310.532881	19184.383482	59.619444
2309.308362	19009.501302	59.624449
2308.805302	18839.446862	59.629453
2308.364332	18658.715039	59.634458
2307.365365	18506.422401	59.639463
2306.950728	18318.407482	59.644468
2306.300410	18149.524656	59.649473
2305.496042	17984.568720	59.654477
2304.666974	17815.035385	59.659482
2304.043460	17650.077195	59.664487
2303.578895	17469.388518	59.669492
2302.185416	17315.490976	59.674497
2301.773458	17159.815104	59.679501
2301.452383	16998.110414	59.684506
2300.440895	16829.766876	59.689511
2299.766055	16660.477805	59.694516
2298.969881	16500.105393	59.699521
2298.469290	16342.059588	59.704525
2297.851713	16173.802775	59.709530
2297.284399	16012.783215	59.714535
2296.476783	15845.323006	59.719540
2295.756331	15695.021579	59.724545
2295.068334	15526.900373	59.729549
2294.635327	15373.694810	59.734554
2293.708564	15214.374829	59.739559
2293.120195	15056.448614	59.744564
2292.203742	14903.469222	59.749569
2291.747263	14738.822728	59.754573
2291.625891	14583.673618	59.759578
2290.543935	14426.934937	59.764583
2289.879927	14263.895481	59.769588
2288.902261	14116.557142	59.774593
2287.967928	13951.848936	59.779597
2287.676767	13796.923312	59.784602
2286.801054	13649.363153	59.789607
2286.427931	13487.602147	59.794612
2285.502276	13340.494049	59.799617
2285.116306	13185.667465	59.804621
2284.285116	13029.606260	59.809626
2283.335099	12888.718375	59.814631
2282.812356	12733.629091	59.819636
2281.875360	12589.955911	59.824641
2281.441890	12444.429109	59.829645
2280.644776	12295.078543	59.834650
2280.017171	12144.677357	59.839655
2279.613181	11996.496356	59.844660
2278.725431	11862.249637	59.849665
2277.872378	11709.920408	59.854669
2277.227286	11562.842640	59.859674
2276.484124	11417.045402	59.864679
2275.804220	11277.590987	59.869684
2275.248065	11134.315196	59.874689
2274.354009	10991.492441	59.879693
2273.755794	10848.016520	59.884698
2273.071043	10715.928933	59.889703
2272.670714	10579.167955	59.894708
2271.879463	10447.353678	59.899713
2271.275540	10306.276599	59.904718
2270.681925	10160.243233	59.909722
2269.615600	10034.019196	59.914727
2268.960493	9887.768012	59.919732
2268.098517	9755.962297	59.924737
2267.298199	9623.513981	59.929742
2266.938467	9488.583772	59.934746
2266.219883	9368.957911	59.939751
2265.334040	9231.972491	59.944756
2264.749917	9101.064172	59.949761
2264.082826	8979.282068	59.954766
2263.627161	8846.181950	59.959770
2262.737757	8725.277811	59.964775
2261.990858	8589.670299	59.969780
2261.148183	8468.810515	59.974785
2260.391701	8345.857582	59.979790
2259.929185	8228.174905	59.984794
2259.187780	8118.117461	59.989799
2258.161927	8000.297526	59.994804
2257.525740	7879.382124	59.999809
2256.461796	7765.392402	60.004814
2256.093365	7654.980991	60.009818
2254.770734	7550.628265	60.014823
2254.138869	7436.979981	60.019828
2253.334955	7344.593689	60.024833
2252.381803	7242.044724	60.029838
2251.773575	7154.651419	60.034842
2250.996585	7070.380165	60.039847
2250.279991	6969.190291	60.044852
2249.310531	6881.355736	60.049857
2248.673096	6804.394020	60.054862
2247.512425	6714.857639	60.059866
2246.530558	6648.359587	60.064871
2245.979392	6568.560905	60.069876
2245.317312	6495.749325	60.074881
2244.637115	6429.710052	60.079886
2244.099111	6353.795890	60.084890
2243.197056	6296.139919	60.089895
2242.528040	6223.204558	60.094900
2241.955203	6167.492618	60.099905
2241.183462	6102.306269	60.104910
2241.049817	6024.165107	60.109914
2240.258143	5967.881232	60.114919
2239.355882	5890.522141	60.119924
2238.916519	5826.249006	60.124929
2238.069870	5753.007304	60.129934
2237.799936	5687.095569	60.134938
2237.089537	5623.007500	60.139943
2236.191756	5545.162019	60.144948
2235.619640	5490.279955	60.149953
2234.856306	5419.933394	60.154958
2234.102933	5347.660155	60.159962
2233.512323	5298.880641	60.164967
2232.878645	5229.504343	60.169972
2232.423575	5174.024341	60.174977
2231.516747	5108.679212	60.179982
2231.076846	5032.103138	60.184986
2230.207148	4975.061626	60.189991
2230.005572	4911.508797	60.194996
2229.491762	4855.431957	60.200001
2228.646086	4779.554928	60.205006
2228.320675	4707.493784	60.210010
2227.355859	4644.201990	60.215015
2226.903012	4575.983197	60.220020
2226.306734	4495.109218	60.225025
2225.453540	4436.921124	60.230030
2224.728521	4371.901403	60.235034
2224.147433	4301.864884	60.240039
2223.338022	4236.262866	60.245044
2222.552403	4175.978107	60.250049
2221.882747	4104.174056	60.255054
2221.446454	4029.075146	60.260058
2220.218241	3979.576128	60.265063
2219.704518	3910.267443	60.270068
2219.262375	3849.056433	60.275073
2218.358971	3786.805983	60.280078
2217.604245	3731.766183	60.285082
2217.225828	3677.401963	60.290087
2216.967623	3609.454889	60.295092
2216.022427	3552.903284	60.300097
2215.411175	3492.286862	60.305102
2215.067533	3422.837553	60.310106
2214.046374	3368.616652	60.315111
2213.324474	3308.991772	60.320116
2212.548205	3242.775332	60.325121
2211.577922	3186.059554	60.330126
2211.320521	3130.071633	60.335130
2210.458037	3076.705219	60.340135
2209.932038	3021.042664	60.345140
2209.462523	2978.800679	60.350145
2208.557876	2909.762981	60.355150
2208.258360	2833.008065	60.360154
2207.400928	2791.440940	60.365159
2206.654553	2726.976045	60.370164
2206.306983	2674.165854	60.375169
2205.559261	2609.870457	60.380174
2205.194665	2537.752003	60.385178
2204.140242	2483.294389	60.390183
2203.525206	2419.097865	60.395188
2202.645825	2373.865906	60.400193
2201.706440	2311.168442	60.405198
2201.452606	2261.711510	60.410202
2200.856024	2207.791111	60.415207
2199.819740	2146.576557	60.420212
2199.472361	2089.119548	60.425217
2198.613272	2031.978946	60.430222
2198.126531	1977.053844	60.435226
2197.000058	1930.349907	60.440231
2196.462329	1874.374183	60.445236
2195.965524	1822.804393	60.450241
2195.149740	1779.023098	60.455246
2194.600181	1720.308677	60.460250
2193.997369	1671.487927	60.465255
2193.277131	1614.521714	60.470260
2192.437630	1570.990057	60.475265
2191.957779	1520.696154	60.480270
2191.634506	1471.229251	60.485274
2190.322833	1430.812895	60.490279
2190.132747	1370.005171	60.495284
2189.342335	1324.795473	60.500289
2188.389914	1270.714182	60.505294
2188.304216	1217.762036	60.510298
2187.612958	1177.074480	60.515303
2186.728540	1123.970230	60.520308
2186.078482	1071.613611	60.525313
2185.336663	1022.978740	60.530318
2184.721427	964.856579	60.535322
2183.669148	938.085790	60.540327
2183.358625	872.465425	60.545332
2182.794819	832.279845	60.550337
2181.930270	785.451295	60.555342
2181.604593	722.752407	60.560346
2180.680249	678.206260	60.565351
2180.096779	626.485703	60.570356
2179.182447	576.183556	60.575361
2178.411926	540.397679	60.580366
2177.494367	487.484741	60.585370
2176.522574	459.747164	60.590375
2176.377196	414.546784	60.595380
2175.988625	381.389572	60.600385
2175.226938	347.906829	60.605390
2174.730849	299.133679	60.610394
2173.654651	262.364026	60.615399
2173.168197	210.276306	60.620404
2172.456181	181.737926	60.625409
2171.576007	126.111053	60.630414
2171.132686	86.980004	60.635418
2170.387388	61.279454	60.640423
2169.114642	21.069026	60.645428
2168.727092	-4.208754	60.650433
2167.583799	-32.579727	60.655438
2167.236208	-64.524978	60.660442
2166.685997	-83.867813	60.665447
2165.414529	-120.952447	60.670452
2164.939944	-145.880272	60.675457
2164.465275	-162.536762	60.680462
2163.646058	-183.919981	60.685466
2162.316016	-183.576492	60.690471
2161.679384	-192.208799	60.695476
2159.346837	-178.007025	60.700481
2154.931682	-82.944358	60.705486
2154.159196	-31.621487	60.710490
2154.727310	-1.634281	60.715495
2155.414569	10.680319	60.720500
2155.856445	40.915517	60.725505
2156.044048	46.793233	60.730510
2156.287767	32.157816	60.735514
2156.180361	37.191324	60.740519
2156.049556	17.548423	60.745524
2155.493815	-5.250425	60.750529
2154.591448	-27.091413	60.755534
2154.252731	-52.391043	60.760538
2152.927987	-52.431599	60.765543
2151.574906	-52.735747	60.770548
2149.934017	-36.574547	60.775553
2148.723448	-26.042098	60.780558
2148.349452	-22.920217	60.785562
2148.056083	-11.061933	60.790567
2147.507001	-14.467860	60.795572
2147.533212	-8.955659	60.800577
2147.224291	-5.471927	60.805582
2147.108356	-17.569610	60.810586
2146.104560	-20.302556	60.815591
2145.144305	-19.479969	60.820596
2143.795344	-8.383061	60.825601
2142.890550	-2.011133	60.830606
2142.493261	-12.423312	60.835610
2141.221843	-1.039859	60.840615
2141.220491	8.029705	60.845620
2140.758790	-0.600501	60.850625
2140.266602	11.913837	60.855630
2140.234854	-2.477560	60.860634
2139.690983	9.437831	60.865639
2138.896169	-1.739999	60.870644
2137.487905	-4.034236	60.875649
2136.297886	4.321084	60.880654
2136.051977	1.294423	60.885658
2134.919703	14.233603	60.890663
2135.082535	18.773205	60.895668
2134.740335	12.599929	60.900673
2134.025886	17.471113	60.905678
2133.760025	5.852953	60.910682
2132.937758	8.139189	60.915687
2132.250280	8.480096	60.920692
2130.955288	10.000793	60.925697
2130.042333	15.078520	60.930702
2129.688756	10.504553	60.935706
2128.764927	18.920944	60.940711
2128.327647	19.062879	60.945716
2127.649733	21.852934	60.950721
2127.046259	23.325419	60.955726
2126.964726	16.114119	60.960730
2126.022632	24.676918	60.965735
2125.781242	11.698650	60.970740
2124.879383	12.537213	60.975745
2123.903978	16.486254	60.980750
2123.365379	15.493054	60.985754
2122.457097	24.208190	60.990759
2121.623117	23.673453	60.995764
2121.112504	16.609082	61.000769
2120.042190	17.245709	61.005774
2119.667763	26.139502	61.010778
2119.597951	31.859347	61.015783
2119.117866	28.645903	61.020788
2118.161175	27.465141	61.025793
2117.598962	32.227021	61.030798
2117.170724	22.476557	61.035802
2115.511770	30.894475	61.040807
2115.251121	27.086378	61.045812
2115.029085	24.885431	61.050817
2114.275872	27.269531	61.055822
2113.874838	27.033545	61.060826
2112.809788	33.549987	61.065831
2112.244414	31.234776	61.070836
2111.450768	27.907077	61.075841
2110.664203	32.013828	61.080846
2110.061097	25.520814	61.085850
2109.331712	26.904468	61.090855
2108.548281	33.168063	61.095860
2108.022042	35.448342	61.100865
2107.236324	34.543241	61.105870
2106.761004	26.049234	61.110874
2106.101767	45.145712	61.115879
2105.893311	29.276288	61.120884
2105.140386	32.548199	61.125889
2103.996634	30.051939	61.130894
2103.818889	25.257679	61.135898
2103.021385	38.489136	61.140903
2102.268727	37.621369	61.145908
2101.677054	28.884042	61.150913
2100.940726	42.102641	61.155918
2100.799180	38.816558	61.160922
2099.407606	34.951357	61.165927
2098.770072	40.622509	61.170932
2098.749087	36.863120	61.175937
2097.702268	42.842074	61.180942
2097.233182	31.836486	61.185946
2096.375935	29.206457	61.190951
2095.484992	40.700693	61.195956
2095.174550	44.774482	61.200961
2094.529714	43.380236	61.205966
2094.083488	34.690794	61.210970
2093.150250	45.179308	61.215975
2092.259553	43.182234	61.220980
2091.618836	34.313912	61.225985
2090.902391	41.271806	61.230990
2090.712967	39.172921	61.235994
2089.564927	42.717274	61.240999
2088.881196	37.061828	61.246004
2089.073973	44.358016	61.251009
2088.227329	43.889956	61.256014
2087.888608	45.758849	61.261018
2086.919195	46.633378	61.266023
2086.242728	36.876567	61.271028
2085.362469	45.421692	61.276033
2084.065084	46.184254	61.281038
2083.942893	43.645755	61.286042
2083.359428	49.503882	61.291047
2082.656125	40.367938	61.296052
2081.801995	46.289514	61.301057
2081.281573	51.795429	61.306062
2080.420518	43.181272	61.311066
2079.444651	47.023173	61.316071
2079.302835	48.561192	61.321076
2079.145201	51.528912	61.326081
2078.118775	55.615389	61.331086
2077.173463	47.615440	61.336090
2076.286828	59.015966	61.341095
2075.733766	45.771735	61.346100
2075.779639	54.649318	61.351105
2074.868208	58.561426	61.356110
2074.397697	51.079089	61.361114
2073.208142	55.118911	61.366119
2072.424450	51.426928	61.371124
2072.082631	51.783968	61.376129
2071.420661	56.473380	61.381134
2071.129921	46.420386	61.386138
2070.554629	46.230982	61.391143
2069.933247	50.152259	61.396148
2069.131144	48.718318	61.401153
2067.621979	51.963583	61.406158
2066.903379	45.463668	61.411162
2066.465394	54.462186	61.416167
2066.607353	52.955712	61.421172
2065.740452	45.818564	61.426177
2064.554307	61.073512	61.431182
2064.083957	48.390187	61.436186
2063.518168	55.751555	61.441191
2062.462926	48.582792	61.446196
2061.985985	48.399861	61.451201
2061.185547	53.896596	61.456206
2061.095016	50.364291	61.461210
2060.346143	59.735432	61.466215
2059.647531	61.185185	61.471220
2059.544328	49.938601	61.476225
2058.718213	59.309384	61.481230
2057.988019	51.038755	61.486234
2056.518826	54.607278	61.491239
2055.666395	63.818232	61.496244
2056.022250	58.674353	61.501249
2055.086040	59.631937	61.506254
2054.389672	48.331245	61.511258
2053.545829	58.318297	61.516263
2053.186784	56.050781	61.521268
2052.704500	45.233377	61.526273
2051.825992	60.814837	61.531278
2051.368064	46.897904	61.536282
2050.335278	52.153960	61.541287
2049.360235	58.804389	61.546292
2048.886907	63.225745	61.551297
2048.146038	56.808215	61.556302
2047.396435	55.493686	61.561306
2047.010229	68.743490	61.566311
2046.649516	59.013845	61.571316
2045.914093	55.001963	61.576321
2045.293786	60.580510	61.581326
2044.800263	51.810264	61.586330
2044.249591	49.522696	61.591335
2043.258982	61.669884	61.596340
2042.292896	51.064878	61.601345
2041.281561	55.207322	61.606350
2040.625869	58.102690	61.611354
2040.618218	57.310684	61.616359
2039.961026	64.987773	61.621364
2039.030913	48.100577	61.626369
2038.112330	61.942656	61.631374
2037.802541	46.434676	61.636378
2037.075889	60.492308	61.641383
2037.104624	59.016415	61.646388
2036.451701	53.365552	61.651393
2035.587556	64.227917	61.656398
2034.535730	55.943678	61.661402
2033.944515	60.697567	61.666407
2032.794665	67.654876	61.671412
2032.661775	53.858255	61.676417
2031.511026	64.696716	61.681422
2031.336981	56.935519	61.686426
2030.873646	60.696102	61.691431
2030.139189	57.218677	61.696436
2030.024612	55.729257	61.701441
2028.356637	58.025158	61.706446
2027.846524	53.827711	61.711450
2027.007931	63.597889	61.716455
2026.399096	60.676135	61.721460
2026.475771	54.146218	61.726465
2025.758699	70.042705	61.731470
2024.969163	56.191014	61.736474
2023.647664	64.886617	61.741479
2023.174863	54.867252	61.746484
2022.604147	55.539754	61.751489
2021.557838	61.564393	61.756494
2021.251852	63.502220	61.761498
2020.619566	64.234958	61.766503
2020.091698	55.066454	61.771508
2019.827290	54.083377	61.776513
2019.111886	67.502122	61.781518
2018.673316	63.834234	61.786522
2017.410973	56.196867	61.791527
2016.307726	60.945285	61.796532
2015.779180	59.710804	61.801537
2015.074278	59.748569	61.806542
2014.919474	59.158119	61.811546
2014.206775	65.383714	61.816551
2013.797648	59.678395	61.821556
2013.483310	64.282687	61.826561
2012.327491	62.381333	61.831566
2011.980672	69.900358	61.836570
2011.024169	70.119985	61.841575
2010.282390	64.120516	61.846580
2010.001795	55.154054	61.851585
2008.717029	62.206901	61.856590
2007.942919	55.157551	61.861594
2007.055144	58.277423	61.866599
2006.428077	71.216937	61.871604
2006.041161	51.288237	61.876609
2005.350418	62.481067	61.881614
2004.902329	56.405030	61.886618
2004.389089	60.198768	61.891623
2004.024459	63.448511	61.896628
2003.671118	50.221491	61.901633
2002.194395	55.385588	61.906638
2001.766416	46.385752	61.911642
2000.842781	63.226525	61.916647
2000.382416	50.745068	61.921652
1999.728197	59.194420	61.926657
1999.248953	52.800044	61.931662
1998.141552	44.652387	61.936666
1997.128760	51.461789	61.941671
1996.456695	52.561979	61.946676
1996.196160	50.780326	61.951681
1995.418540	60.411517	61.956686
1995.183497	50.039028	61.961690
1994.747563	56.252238	61.966695
1994.080964	59.095729	61.971700
1993.438677	56.390613	61.976705
1992.343741	58.202914	61.981710
1991.724706	55.940400	61.986714
1991.117641	56.815803	61.991719
1990.419142	59.845713	61.996724
1989.918892	55.919531	62.001729
1988.861793	59.878440	62.006734
1988.831108	50.821856	62.011738
1987.426848	64.036110	62.016743
1986.438879	67.129312	62.021748
1986.064578	55.071027	62.026753
1985.369907	58.592356	62.031758
1984.930901	57.616492	62.036762
1984.384873	65.525114	62.041767
1983.581254	65.846646	62.046772
1983.498370	60.184173	62.051777
1982.752355	63.945473	62.056782
1982.692060	62.220351	62.061786
1981.122122	62.551543	62.066791
1980.395866	68.296735	62.071796
1980.044729	58.699631	62.076801
1979.532520	69.195484	62.081806
1978.872093	64.042582	62.086810
1977.793154	57.423260	62.091815
1976.801291	62.135089	62.096820
1976.372408	58.372630	62.101825
1975.700698	59.078518	62.106830
1975.215410	58.833847	62.111834
1975.100074	71.070803	62.116839
1974.249286	60.363942	62.121844
1973.317145	68.458433	62.126849
1972.626791	61.151364	62.131854
1972.154554	63.667535	62.136858
1971.371590	68.450294	62.141863
1970.685494	70.970447	62.146868
1970.028353	58.398795	62.151873
1968.788111	69.831822	62.156878
1968.363980	60.780911	62.161882
1967.605103	64.129503	62.166887
1967.191158	64.671475	62.171892
1966.949913	53.759060	62.176897
1966.262804	69.105153	62.181902
1965.969324	67.279843	62.186906
1964.735275	63.127925	62.191911
1963.824322	64.855840	62.196916
1963.403413	66.583248	62.201921
1962.572191	75.123790	62.206926
1962.245255	64.578219	62.211930
1962.030164	59.714197	62.216935
1960.363467	70.626693	62.221940
1959.652464	55.294376	62.226945
1959.213703	64.698321	62.231950
1958.367542	68.387211	62.236954
1957.922084	57.294313	62.241959
1957.810418	60.863465	62.246964
1957.587855	54.821031	62.251969
1956.218628	67.320087	62.256974
1955.332673	72.535529	62.261978
1954.690512	64.892797	62.266983
1953.996404	70.913600	62.271988
1953.736385	66.589735	62.276993
1952.825517	65.166785	62.281998
1951.952312	66.731013	62.287002
1950.987711	70.432397	62.292007
1950.559452	73.969799	62.297012
1950.425493	70.669903	62.302017
1949.237763	76.592435	62.307022
1949.278259	76.037223	62.312026
1948.658122	68.840443	62.317031
1947.930557	67.429401	62.322036
1946.941525	65.657726	62.327041
1945.943202	74.846135	62.332046
1945.824082	62.829354	62.337050
1945.072332	66.187860	62.342055
1943.797586	70.802675	62.347060
1943.126912	68.914233	62.352065
1942.417409	65.196322	62.357070
1941.921009	61.316849	62.362074
1941.551566	78.347234	62.367079
1941.281171	64.137195	62.372084
1940.711197	72.923287	62.377089
1939.981852	65.515180	62.382094
1938.883709	69.665133	62.387098
1938.232442	75.929884	62.392103
1937.795729	72.946136	62.397108
1937.530168	73.310012	62.402113
1936.509037	70.248714	62.407118
1935.193896	71.140328	62.412122
1934.541694	75.720987	62.417127
1934.242160	73.160180	62.422132
1933.475573	70.946332	62.427137
1933.230635	76.973116	62.432142
1932.732683	71.740817	62.437146
1932.237279	75.782484	62.442151
1930.800449	70.371201	62.447156
1930.436769	68.706855	62.452161
1929.603337	67.120229	62.457166
1929.432393	69.232178	62.462170
1928.197187	66.674813	62.467175
1927.183316	67.095971	62.472180
1926.766685	63.751059	62.477185
1926.109968	68.975852	62.482190
1925.700401	59.935256	62.487194
1925.434331	70.485085	62.492199
1924.584660	64.154255	62.497204
1924.382131	73.484438	62.502209
1923.137972	63.921865	62.507214
1922.419803	61.600985	62.512218
1922.124788	70.365510	62.517223
1921.200822	64.697777	62.522228
1920.303361	66.406218	62.527233
1919.205082	70.986723	62.532238
1918.785442	64.732716	62.537242
1918.366263	65.284988	62.542247
1917.542857	62.368937	62.547252
1917.098811	68.712762	62.552257
1916.544187	66.889488	62.557262
1916.515275	68.933158	62.562266
1915.860218	64.832862	62.567271
1914.539560	70.614076	62.572276
1913.783001	64.618564	62.577281
1913.183023	70.253836	62.582286
1912.919070	61.997554	62.587290
1911.887460	65.069323	62.592295
1910.861883	65.263679	62.597300
1910.403403	64.745097	62.602305
1909.809009	60.690370	62.607310
1909.602900	62.344262	62.612314
1909.288226	62.791633	62.617319
1907.660217	63.515299	62.622324
1907.345301	59.334203	62.627329
1906.523882	69.133224	62.632334
1906.114589	67.890874	62.637338
1905.545149	68.571083	62.642343
1904.075497	68.271370	62.647348
1903.744414	63.586621	62.652353
1903.019668	71.375388	62.657358
1902.781612	61.424448	62.662362
1902.406911	62.808627	62.667367
1901.677118	66.374977	62.672372
1900.397271	69.287456	62.677377
1899.688666	75.778942	62.682382
1899.034103	63.542807	62.687386
1898.738596	66.871477	62.692391
1897.926769	60.958865	62.697396
1897.645681	71.829633	62.702401
1896.897754	71.021100	62.707406
1896.327331	70.744226	62.712410
1895.433029	64.770587	62.717415
1894.686516	65.589298	62.722420
1894.428694	52.470150	62.727425
1893.407989	64.850820	62.732430
1892.420402	70.203841	62.737434
1891.683269	74.337505	62.742439
1891.001636	78.788800	62.747444
1890.883978	64.004152	62.752449
1890.270109	75.823490	62.757454
1889.774829	71.767224	62.762458
1889.261253	66.050124	62.767463
1888.198068	64.700265	62.772468
1887.495153	65.786456	62.777473
1886.990804	77.359744	62.782478
1886.338938	65.501665	62.787482
1885.384772	80.305104	62.792487
1884.877420	73.934134	62.797492
1884.132872	61.228151	62.802497
1883.322022	65.212663	62.807502
1883.443097	65.698097	62.812506
1882.373687	58.840757	62.817511
1881.172857	63.568445	62.822516
1880.810890	65.746992	62.827521
1880.336416	60.848462	62.832526
1879.690811	62.679364	62.837530
1879.003707	68.628103	62.842535
1877.915829	64.795234	62.847540
1877.488370	66.820171	62.852545
1877.047820	68.050799	62.857550
1876.821021	60.488816	62.862554
1875.766430	69.384967	62.867559
1874.617508	69.936398	62.872564
1874.194994	63.231835	62.877569
1873.272313	82.961571	62.882574
1872.985423	65.809897	62.887578
1872.847704	65.816004	62.892583
1871.709795	69.719975	62.897588
1870.909574	65.831979	62.902593
1870.165184	72.374885	62.907598
1869.772330	61.382472	62.912602
1869.327949	67.202789	62.917607
1867.940713	67.604394	62.922612
1867.434200	58.180224	62.927617
1866.556337	65.699981	62.932622
1866.185589	66.861180	62.937626
1865.807307	63.811399	62.942631
1865.594240	63.599227	62.947636
1864.907309	67.510453	62.952641
1863.678777	74.423546	62.957646
1863.019499	58.327671	62.962650
1862.791938	61.330155	62.967655
1861.551648	65.458547	62.972660
1860.587396	65.157470	62.977665
1859.903186	72.484057	62.982670
1859.319160	59.282654	62.987674
1859.031651	64.991331	62.992679
1858.623487	72.867045	62.997684
1857.962530	51.225124	63.002689
1857.587997	71.905489	63.007694
1856.777580	60.455809	63.012698
1855.746282	63.030792	63.017703
1854.931708	65.396321	63.022708
1855.045024	63.225736	63.027713
1853.639762	69.267996	63.032718
1852.886212	61.072110	63.037722
1852.237689	60.632598	63.042727
1851.712741	62.348153	63.047732
1851.493806	51.056896	63.052737
1850.753208	68.879499	63.057742
1850.213256	60.835788	63.062746
1849.727550	56.230795	63.067751
1848.671253	58.007055	63.072756
1847.593397	66.835942	63.077761
1846.508813	68.369105	63.082766
1846.052569	67.895913	63.087770
1845.721997	63.263135	63.092775
1845.607149	65.530189	63.097780
1844.977404	64.190382	63.102785
1844.435941	70.967588	63.107790
1843.191548	67.172199	63.112794
1842.559595	59.193562	63.117799
1841.687605	64.916187	63.122804
1841.682081	55.918702	63.127809
1840.827598	61.996526	63.132814
1839.908915	65.359484	63.137818
1838.984946	62.364807	63.142823
1838.384988	64.683650	63.147828
1838.196973	64.073252	63.152833
1837.525453	66.080172	63.157838
1836.909180	62.503615	63.162842
1835.984409	62.628378	63.167847
1835.181223	67.280335	63.172852
1834.839438	58.426128	63.177857
1833.515324	71.804347	63.182862
1832.714316	56.927935	63.187866
1832.823696	63.194936	63.192871
1831.883236	63.382117	63.197876
1831.596797	56.299560	63.202881
1831.052430	66.302195	63.207886
1830.480014	66.312666	63.212890
1829.760032	59.931321	63.217895
1828.650629	66.775045	63.222900
1828.085791	55.316353	63.227905
1827.591089	60.706255	63.232910
1826.466616	57.286088	63.237914
1825.590325	68.421673	63.242919
1825.169668	60.370068	63.247924
1824.770346	51.867211	63.252929
1824.198768	66.892186	63.257934
1824.018134	57.001536	63.262938
1822.904465	61.001027	63.267943
1822.129147	58.531551	63.272948
1822.012048	54.240212	63.277953
1820.732249	61.888454	63.282958
1819.805771	70.379492	63.287962
1819.166020	65.622338	63.292967
1818.715614	67.056397	63.297972
1818.203863	55.207645	63.302977
1817.700926	61.877804	63.307982
1817.154379	62.138068	63.312986
1816.481390	59.642885	63.317991
1815.540428	66.999204	63.322996
1815.132691	59.413920	63.328001
1814.227557	61.864804	63.333006
1813.233584	61.456497	63.338010
1812.486248	59.160783	63.343015
1811.571178	68.566248	63.348020
1811.739428	64.969214	63.353025
1811.306981	69.220103	63.358030
1810.835756	72.240779	63.363034
1809.986162	64.936971	63.368039
1808.915170	73.170253	63.373044
1808.270965	60.238629	63.378049
1806.875760	69.222001	63.383054
1806.893039	75.666060	63.388058
1806.367951	60.969780	63.393063
1805.201189	67.513528	63.398068
1805.077567	70.001180	63.403073
1804.170282	80.804221	63.408078
1803.821925	67.648992	63.413082
1803.199663	63.992968	63.418087
1802.249249	68.930095	63.423092
1801.788816	60.643529	63.428097
1801.004226	72.393785	63.433102
1800.710787	68.515233	63.438106
1799.890051	60.689591	63.443111
1798.865209	69.713510	63.448116
1798.732303	72.530653	63.453121
1797.706437	63.748802	63.458126
1796.607844	73.951416	63.463130
1796.089558	63.376343	63.468135
1795.198802	80.459538	63.473140
1795.180345	67.945810	63.478145
1794.704977	67.951918	63.483150
1794.225040	74.257300	63.488154
1793.124798	68.879391	63.493159
1792.188081	71.906174	63.498164
1791.717945	64.624124	63.503169
1791.295013	62.046662	63.508174
1790.423547	75.561189	63.513178
1789.354537	64.764474	63.518183
1788.431070	77.741617	63.523188
1788.549929	60.847255	63.528193
1787.834256	76.994293	63.533198
1787.781122	62.669369	63.538202
1786.906245	74.511238	63.543207
1785.487406	65.884835	63.548212
1785.307468	66.261938	63.553217
1784.544307	68.792794	63.558222
1784.200305	72.228526	63.563226
1783.229479	70.797810	63.568231
1782.350992	65.660671	63.573236
1781.869914	65.634571	63.578241
1781.611790	55.786197	63.583246
1780.078548	72.518808	63.588250
1779.831751	65.504080	63.593255
1778.733162	79.652362	63.598260
1778.522470	56.669486	63.603265
1777.986989	75.995531	63.608270
1777.525659	62.314188	63.613274
1776.626318	66.336435	63.618279
1775.811373	64.311673	63.623284
1775.694177	55.852338	63.628289
1775.019882	69.370247	63.633294
1773.812005	58.628713	63.638298
1772.919140	66.617668	63.643303
1772.562841	79.356515	63.648308
1772.149179	63.442452	63.653313
1771.870540	69.086645	63.658318
1770.528794	69.438499	63.663322
1769.901746	63.255311	63.668327
1769.267574	71.617941	63.673332
1769.125237	59.406179	63.678337
1767.744883	67.694905	63.683342
1766.956447	68.682740	63.688346
1766.703955	71.581954	63.693351
1765.833584	73.664625	63.698356
1765.722909	67.205466	63.703361
1765.130566	64.065112	63.708366
1764.097209	73.241787	63.713370
1763.556649	56.617733	63.718375
1762.730705	61.375827	63.723380
1762.101221	56.437284	63.728385
1760.566560	58.762642	63.733390
1760.122148	65.131771	63.738394
1759.922738	60.079200	63.743399
1759.330600	62.286427	63.748404
1759.300808	65.082464	63.753409
1758.617431	66.865774	63.758414
1757.564937	67.632185	63.763418
1757.102627	59.282851	63.768423
1756.400445	67.713053	63.773428
1755.029275	61.644884	63.778433
1754.321551	60.372679	63.783438
1753.724702	75.999363	63.788442
1753.222800	58.949689	63.793447
1752.533120	70.951393	63.798452
1752.715354	60.429100	63.803457
1752.038660	60.254292	63.808462
1750.820566	69.031361	63.813466
1750.490321	63.611624	63.818471
1749.576342	56.962273	63.823476
1748.674388	55.837613	63.828481
1747.583257	65.286033	63.833486
1747.282724	66.074964	63.838490
1746.935714	52.340003	63.843495
1746.458637	65.792686	63.848500
1746.166235	56.139792	63.853505
1744.949028	65.521500	63.858510
1744.405195	63.333842	63.863514
1743.756678	59.872822	63.868519
1742.762669	70.869420	63.873524
1741.964308	57.122553	63.878529
1741.128138	67.568153	63.883534
1740.670649	66.360295	63.888538
1740.239744	62.347461	63.893543
1739.579319	63.217201	63.898548
1739.464556	52.365965	63.903553
1738.499262	61.119446	63.908558
1737.984801	58.185147	63.913562
1737.244582	58.184439	63.918567
1735.847015	61.160630	63.923572
1735.159268	49.747514	63.928577
1734.344354	58.023725	63.933582
1733.851529	58.551450	63.938586
1733.626163	58.532059	63.943591
1733.093959	55.653409	63.948596
1732.791752	50.279692	63.953601
1732.127618	53.698453	63.958606
1731.208495	60.015235	63.963610
1730.502688	59.138559	63.968615
1729.726426	61.973505	63.973620
1728.793942	54.835079	63.978625
1728.005424	60.640673	63.983630
1727.278579	62.936322	63.988634
1727.104451	57.740176	63.993639
1726.581237	62.509339	63.998644
1726.188487	55.081765	64.003649
1725.190726	58.829488	64.008654
1724.452101	50.893068	64.013658
1724.065952	49.708578	64.018663
1722.923907	45.406556	64.023668
1722.209497	45.759732	64.028673
1721.438395	58.953957	64.033678
1720.806835	66.175217	64.038682
1720.700015	60.798065	64.043687
1720.040528	66.002047	64.048692
1719.476370	65.402508	64.053697
1718.478865	57.593147	64.058702
1717.697014	62.123470	64.063706
1717.244332	54.368726	64.068711
1716.596501	64.416977	64.073716
1715.746033	49.911982	64.078721
1714.824027	62.004199	64.083726
1714.213108	68.592960	64.088730
1714.023588	58.018534	64.093735
1713.572924	68.454956	64.098740
1712.717897	62.133735	64.103745
1711.753731	60.703567	64.108750
1711.064699	67.648521	64.113754
1710.773763	57.132781	64.118759
1709.919751	58.665650	64.123764
1709.009032	60.581275	64.128769
1708.580012	61.974105	64.133774
1707.811656	70.491313	64.138778
1707.580377	53.267002	64.143783
1706.199553	60.032445	64.148788
1705.599980	70.090384	64.153793
1704.608695	64.864742	64.158798
1704.126715	59.104827	64.163802
1704.197898	63.151157	64.168807
1703.856168	62.808041	64.173812
1702.924614	67.001800	64.178817
1701.961229	65.111816	64.183822
1701.388963	63.792880	64.188826
1700.990199	59.338122	64.193831
1699.951200	62.769119	64.198836
1699.204688	58.237124	64.203841
1698.895050	58.612754	64.208846
1698.226964	58.264700	64.213850
1697.346571	59.297123	64.218855
1696.172353	54.112371	64.223860
1695.626496	62.137696	64.228865
1695.099293	73.120882	64.233870
1694.746162	64.485342	64.238874
1694.705579	56.803928	64.243879
1693.524641	70.574995	64.248884
1692.778894	63.686051	64.253889
1692.741103	54.897140	64.258894
1691.276769	68.531861	64.263898
1690.324208	59.100526	64.268903
1689.696182	64.293997	64.273908
1689.506204	58.834648	64.278913
1688.890914	57.848988	64.283918
1688.205492	56.365096	64.288922
1687.400588	61.110405	64.293927
1686.252973	68.807886	64.298932
1686.374298	62.421492	64.303937
1685.665136	60.091368	64.308942
1684.850341	57.994072	64.313946
1684.315214	61.688831	64.318951
1682.883414	66.114230	64.323956
1682.587785	67.791817	64.328961
1682.149655	70.620381	64.333966
1681.864311	70.451244	64.338970
1681.067886	69.268844	64.343975
1680.203946	75.496455	64.348980
1679.774816	63.452475	64.353985
1679.106998	64.078969	64.358990
1677.975916	67.428404	64.363994
1677.320137	64.186182	64.368999
1676.575086	66.982279	64.374004
1676.446500	64.670334	64.379009
1676.015952	66.653211	64.384014
1674.768029	67.903294	64.389018
1674.195210	65.712371	64.394023
1673.338184	69.018279	64.399028
1673.088422	64.904145	64.404033
1672.377738	66.228175	64.409038
1671.288326	67.697518	64.414042
1670.876440	56.408557	64.419047
1670.332335	70.662758	64.424052
1670.113134	60.828723	64.429057
1669.037152	73.187485	64.434062
1667.889533	69.874359	64.439066
1668.006596	64.304739	64.444071
1667.205911	63.451036	64.449076
1666.093247	66.501075	64.454081
1665.145226	73.540794	64.459086
1664.758587	76.461323	64.464090
1664.401553	65.738460	64.469095
1664.009493	61.894520	64.474100
1663.270788	64.542951	64.479105
1662.409064	62.580852	64.484110
1661.478197	68.010095	64.489114
1660.954815	66.524126	64.494119
1660.256791	71.853307	64.499124
1659.305218	63.733102	64.504129
1658.829691	60.287208	64.509134
1658.233022	67.487956	64.514138
1658.060459	58.800880	64.519143
1657.459279	72.218879	64.524148
1656.701961	68.789357	64.529153
1655.725848	65.429283	64.534158
1654.779744	69.667160	64.539162
1654.927299	65.944094	64.544167
1653.562822	61.808324	64.549172
1652.543258	70.637476	64.554177
1652.034315	66.673326	64.559182
1651.548146	66.279041	64.564186
1651.179506	66.326571	64.569191
1650.774960	68.347901	64.574196
1650.027084	63.149066	64.579201
1649.498603	66.330251	64.584206
1648.484855	68.886754	64.589210
1648.086826	61.670562	64.594215
1646.902180	75.390196	64.599220
1646.426794	66.174826	64.604225
1645.782981	59.999071	64.609230
1645.000997	68.446701	64.614234
1644.987042	54.147127	64.619239
1643.758607	67.470787	64.624244
1643.666695	65.184558	64.629249
1642.618557	70.602472	64.634254
1641.583424	76.924309	64.639258
1640.505387	67.126558	64.644263
1639.622923	64.339837	64.649268
1639.319152	56.018971	64.654273
1639.230138	64.949476	64.659278
1638.654411	72.372413	64.664282
1638.694041	63.637439	64.669287
1638.040550	72.178206	64.674292
1636.689346	64.400620	64.679297
1636.356582	69.436810	64.684302
1634.885931	63.548522	64.689306
1634.563953	64.730389	64.694311
1633.583110	63.772847	64.699316
1633.093863	66.264963	64.704321
1633.171075	61.121157	64.709326
1632.376364	63.991387	64.714330
1631.378176	64.996811	64.719335
1630.417758	68.697635	64.724340
1630.185792	58.952371	64.729345
1629.270475	71.715354	64.734350
1628.054077	61.385276	64.739354
1627.786502	58.169715	64.744359
1627.229272	75.078520	64.749364
1627.121342	57.762880	64.754369
1626.578447	56.701078	64.759374
1625.286716	60.697389	64.764378
1624.732354	60.794926	64.769383
1624.075984	61.312379	64.774388
1623.624201	53.893418	64.779393
1622.149764	61.425997	64.784398
1621.447656	61.993296	64.789402
1621.144349	54.900842	64.794407
1620.933034	56.948251	64.799412
1620.480885	60.082621	64.804417
1619.802473	59.704687	64.809422
1618.830079	59.203138	64.814426
1618.438882	55.488385	64.819431
1617.362626	55.736639	64.824436
1616.181295	53.580894	64.829441
1615.805797	55.419411	64.834446
1615.343653	65.610861	64.839450
1614.906241	61.420886	64.844455
1614.376084	65.463385	64.849460
1613.992392	52.268104	64.854465
1612.659506	65.751872	64.859470
1611.570377	56.866622	64.864474
1611.425178	64.214859	64.869479
1611.129232	57.857695	64.874484
1610.564600	54.254076	64.879489
1609.422563	51.302016	64.884494
1608.757680	68.566970	64.889498
1608.779628	52.293606	64.894503
1607.222220	67.213418	64.899508
1606.733152	50.226428	64.904513
1606.031262	63.056431	64.909518
1605.552793	61.214824	64.914522
1605.191094	67.146617	64.919527
1604.265160	66.282867	64.924532
1603.456531	61.156780	64.929537
1603.074728	63.237582	64.934542
1602.399760	68.996785	64.939546
1601.567374	62.444135	64.944551
1600.857368	73.881370	64.949556
1599.970253	72.271843	64.954561
1599.772899	63.818954	64.959566
1599.045582	67.806042	64.964570
1598.327946	64.617826	64.969575
1597.524446	54.889247	64.974580
1596.780774	56.844605	64.979585
1596.353813	59.366255	64.984590
1595.555465	66.805638	64.989594
1594.871331	57.181102	64.994599
1593.718125	61.358854	64.999604
1593.455106	61.320225	65.004609
1593.140073	57.735306	65.009614
1592.623883	65.694430	65.014618
1592.324928	58.341084	65.019623
1590.898458	62.309930	65.024628
1590.430625	54.412542	65.029633
1589.570846	63.265211	65.034638
1588.567743	57.818356	65.039642
1588.004344	56.848132	65.044647
1587.377025	62.265442	65.049652
1587.084231	66.181925	65.054657
1586.732587	70.673900	65.059662
1586.219197	74.425152	65.064666
1585.359761	57.217872	65.069671
1584.077598	70.359273	65.074676
1583.736617	66.193409	65.079681
1583.557504	61.956098	65.084686
1582.415103	66.742437	65.089690
1581.564100	60.498690	65.094695
1581.225040	65.908056	65.099700
1580.621510	63.400327	65.104705
1579.661067	62.660345	65.109710
1578.676588	63.411290	65.114714
1578.543141	53.625157	65.119719
1577.754605	60.695541	65.124724
1577.424407	63.296442	65.129729
1576.488233	60.751674	65.134734
1575.477622	65.570696	65.139738
1575.527144	56.173397	65.144743
1574.630269	60.854497	65.149748
1574.074734	58.657700	65.154753
1573.208205	60.418111	65.159758
1572.126446	66.398069	65.164762
1572.181947	57.296296	65.169767
1571.584066	66.873784	65.174772
1570.764488	59.899630	65.179777
1570.139991	66.770489	65.184782
1569.173497	65.946313	65.189786
1567.925394	67.623842	65.194791
1567.602429	55.555939	65.199796
1566.972181	54.941703	65.204801
1566.585988	60.077850	65.209806
1566.137845	56.777441	65.214810
1565.862471	53.701905	65.219815
1564.384168	61.124737	65.224820
1563.705098	61.521228	65.229825
1563.199260	58.944367	65.234830
1562.660785	64.650350	65.239834
1562.453623	51.802364	65.244839
1561.494356	60.066854	65.249844
1560.943988	56.979813	65.254849
1560.306181	55.387464	65.259854
1558.927882	61.703129	65.264858
1558.891896	54.606065	65.269863
1557.835250	66.986224	65.274868
1557.604686	57.171365	65.279873
1556.322109	60.708924	65.284878
1555.481081	67.032275	65.289882
1555.243585	50.883722	65.294887
1554.603225	68.166860	65.299892
1554.026955	66.317147	65.304897
1553.649675	69.229892	65.309902
1552.824248	58.799895	65.314906
1552.323306	61.960951	65.319911
1551.382437	69.897665	65.324916
1550.931612	55.762135	65.329921
1550.002973	60.151814	65.334926
1549.087567	73.190803	65.339930
1548.858548	56.690805	65.344935
1548.137396	57.962912	65.349940
1547.395077	60.124654	65.354945
1546.573693	62.335230	65.359950
1545.627194	64.513644	65.364954
1545.513968	52.205840	65.369959
1544.831406	64.264783	65.374964
1544.498496	61.732992	65.379969
1543.305490	61.958824	65.384974
1542.491165	64.111508	65.389978
1542.362729	62.379884	65.394983
1541.593233	64.601142	65.399988
1541.216186	57.230252	65.404993
1539.963019	72.560665	65.409998
1538.903841	62.167812	65.415002
1538.920785	59.080527	65.420007
1538.565271	61.505676	65.425012
1538.077873	62.306972	65.430017
1536.745409	68.102843	65.435022
1536.140503	67.339504	65.440026
1535.696237	65.793682	65.445031
1534.388110	57.198741	65.450036
1534.084096	65.180931	65.455041
1533.427621	67.106682	65.460046
1532.953060	62.829585	65.465050
1532.469044	52.299623	65.470055
1531.481861	71.358375	65.475060
1530.708737	57.961630	65.480065
1530.163177	58.994524	65.485070
1529.315586	61.147766	65.490074
1529.117845	64.036718	65.495079
1528.337904	64.105460	65.500084
1527.719389	49.091392	65.505089
1527.184081	62.049482	65.510094
1526.823786	60.536054	65.515098
1525.691519	58.757343	65.520103
1524.942561	63.047515	65.525108
1524.153298	64.179059	65.530113
1524.134276	46.362038	65.535118
1523.111363	61.021907	65.540122
1522.517663	56.464115	65.545127
1521.890509	60.815361	65.550132
1520.684353	64.413336	65.555137
1519.940535	59.083012	65.560142
1519.432635	61.112895	65.565146
1519.182995	56.599785	65.570151
1518.358077	50.689401	65.575156
1517.647133	61.671036	65.580161
1517.293542	56.895316	65.585166
1516.013992	55.144743	65.590170
1515.409520	55.105182	65.595175
1514.725029	69.676595	65.600180
1514.846273	51.354721	65.605185
1514.085011	59.406408	65.610190
1512.683010	58.031695	65.615194
1512.561475	48.377727	65.620199
1511.621593	58.952603	65.625204
1511.080276	51.172574	65.630209
1510.461932	55.345797	65.635214
1509.373303	48.753478	65.640218
1509.152591	57.804247	65.645223
1508.718238	63.812247	65.650228
1508.100961	57.031485	65.655233
1507.346627	55.263695	65.660238
1506.210629	66.230872	65.665242
1505.849288	50.169823	65.670247
1505.454487	61.113842	65.675252
1504.227461	57.260678	65.680257
1503.589915	58.771831	65.685262
1502.448905	60.542762	65.690266
1502.517700	55.580076	65.695271
1502.165382	59.532830	65.700276
1501.543969	64.673244	65.705281
1500.804904	57.281038	65.710286
1499.628669	60.705528	65.715290
1499.708587	51.358604	65.720295
1498.664418	57.958679	65.725300
1497.803562	58.671086	65.730305
1497.340856	55.939149	65.735310
1496.922930	57.688226	65.740314
1496.023643	53.671022	65.745319
1494.999015	54.396838	65.750324
1494.603127	57.057071	65.755329
1494.275396	51.843574	65.760334
1492.685736	63.256588	65.765338
1492.333687	57.487119	65.770343
1491.366921	68.468413	65.775348
1490.827406	59.945333	65.780353
1490.961392	51.592787	65.785358
1490.226507	59.148265	65.790362
1489.692653	57.641921	65.795367
1488.598193	56.383937	65.800372
1488.001635	61.361126	65.805377
1487.528141	64.424788	65.810382
1486.407464	59.895548	65.815386
1485.723826	55.926084	65.820391
1484.956043	63.493101	65.825396
1484.564818	46.659353	65.830401
1484.325115	59.603586	65.835406
1483.771804	62.049134	65.840410
1483.040041	51.214771	65.845415
1482.148191	61.622747	65.850420
1481.645991	55.217957	65.855425
1480.645187	54.914945	65.860430
1479.826471	59.272985	65.865434
1479.190658	57.699264	65.870439
1478.713126	56.325902	65.875444
1478.485319	53.753766	65.880449
1477.565215	49.036539	65.885454
1476.586267	54.935532	65.890458
1475.788997	54.264280	65.895463
1475.634326	56.838874	65.900468
1474.772373	55.058233	65.905473
1474.427805	48.618937	65.910478
1473.501540	64.498250	65.915482
1473.194599	52.793691	65.920487
1472.406952	49.414787	65.925492
1471.123198	58.382165	65.930497
1470.947113	42.916186	65.935502
1470.171167	57.360196	65.940506
1469.328432	41.473441	65.945511
1468.503014	52.342378	65.950516
1467.767255	45.812280	65.955521
1467.689678	40.057555	65.960526
1467.250350	48.805582	65.965530
1466.586746	46.413091	65.970535
1465.339876	50.066444	65.975540
1464.726316	47.912012	65.980545
1464.364414	42.839575	65.985550
1463.647306	49.223676	65.990554
1462.790107	47.830225	65.995559
1462.031950	51.593578	66.000564
1461.612199	57.509371	66.005569
1461.516476	49.333685	66.010574
1460.046649	58.005776	66.015578
1459.289416	47.924546	66.020583
1458.522654	52.911438	66.025588
1458.021768	50.874724	66.030593
1457.832119	49.753670	66.035598
1457.121226	56.121017	66.040602
1456.258804	46.493333	66.045607
1455.549714	53.880709	66.050612
1454.976844	56.209517	66.055617
1454.762138	51.921109	66.060622
1453.440737	59.576109	66.065626
1452.960356	46.445133	66.070631
1452.135699	57.550505	66.075636
1451.670954	63.118628	66.080641
1451.424259	58.064151	66.085646
1450.345057	52.206818	66.090650
1449.876691	46.441654	66.095655
1449.321767	52.156571	66.100660
1447.894872	53.933532	66.105665
1447.439673	44.436685	66.110670
1446.707462	50.771149	66.115674
1446.619694	54.243460	66.120679
1446.124561	62.875783	66.125684
1444.888936	55.993031	66.130689
1444.416404	46.595135	66.135694
1443.983345	58.417311	66.140698
1443.709455	52.206490	66.145703
1442.075890	49.965000	66.150708
1441.213909	52.273522	66.155713
1440.636256	53.210607	66.160718
1440.236045	48.313000	66.165722
1439.892686	44.532332	66.170727
1439.504798	42.778871	66.175732
1438.599950	58.954409	66.180737
1438.209342	58.212232	66.185742
1437.114890	54.423192	66.190746
1436.223855	45.952848	66.195751
1435.415230	47.246770	66.200756
1434.755516	54.140589	66.205761
1434.561749	54.942547	66.210766
1433.953810	57.560793	66.215770
1433.705858	48.847893	66.220775
1432.404834	55.837325	66.225780
1431.579458	48.266472	66.230785
1431.786581	52.415757	66.235790
1430.611114	50.547760	66.240794
1429.864069	54.560098	66.245799
1429.169076	43.278361	66.250804
1428.568063	51.016003	66.255809
1428.253790	45.585910	66.260814
1426.993682	53.598618	66.265818
1426.563000	41.956323	66.270823
1426.314378	44.873863	66.275828
1425.563438	57.314277	66.280833
1424.234524	49.339316	66.285838
1423.537238	52.791799	66.290842
1423.199088	49.902883	66.295847
1422.828677	47.913252	66.300852
1421.750886	48.970829	66.305857
1421.233079	44.102955	66.310862
1420.424581	50.317081	66.315866
1420.291567	47.587958	66.320871
1419.625905	54.875397	66.325876
1418.553212	49.491721	66.330881
1418.015972	38.564976	66.335886
1416.993876	58.733174	66.340890
1417.033307	40.250863	66.345895
1415.966199	56.344955	66.350900
1414.752331	55.528615	66.355905
1414.691148	54.268873	66.360910
1413.790884	60.619018	66.365914
1413.665175	47.453763	66.370919
1412.813242	55.360603	66.375924
1411.805447	50.177933	66.380929
1411.404256	52.496811	66.385934
1410.879155	54.997813	66.390938
1410.418169	48.219055	66.395943
1409.166435	49.391017	66.400948
1408.480984	59.321492	66.405953
1408.192051	54.822530	66.410958
1407.544824	56.694799	66.415962
1406.819196	49.000866	66.420967
1406.040991	60.534117	66.425972
1405.210514	56.562784	66.430977
1405.112470	45.733395	66.435982
1403.728263	63.879101	66.440986
1403.343053	56.971600	66.445991
1402.503714	54.613365	66.450996
1402.052734	57.014276	66.456001
1401.741223	53.097661	66.461006
1401.299020	51.549962	66.466010
1400.075393	42.033332	66.471015
1399.472117	51.513916	66.476020
1399.137240	50.608342	66.481025
1398.652146	53.623396	66.486030
1397.266126	50.932572	66.491034
1396.785897	44.716710	66.496039
1396.223175	43.864698	66.501044
1395.636522	43.137918	66.506049
1394.565525	42.311496	66.511054
1393.832095	50.278353	66.516058
1393.740302	43.075059	66.521063
1392.929866	44.359820	66.526068
1392.304906	50.604708	66.531073
1391.669276	49.969294	66.536078
1390.630197	52.539375	66.541082
1390.700393	47.868217	66.546087
1389.783982	49.005815	66.551092
1388.710550	50.690356	66.556097
1388.009960	48.194954	66.561102
1387.502191	45.749331	66.566106
1387.009286	50.689559	66.571111
1386.096780	57.161508	66.576116
1385.406312	53.055963	66.581121
1384.817269	49.787451	66.586126
1384.307794	56.796176	66.591130
1383.970618	44.475116	66.596135
1383.252018	48.121811	66.601140
1381.997412	50.267247	66.606145
1381.951304	51.730155	66.611150
1381.147913	60.510829	66.616154
1380.649229	43.090211	66.621159
1379.834417	52.364718	66.626164
1379.336353	46.471824	66.631169
1378.669625	46.317608	66.636174
1377.339069	58.940047	66.641178
1376.524133	50.364588	66.646183
1376.249523	54.164648	66.651188
1376.150335	54.445363	66.656193
1375.220521	44.260710	66.661198
1374.171517	62.050362	66.666202
1373.483990	44.855308	66.671207
1373.200121	48.365096	66.676212
1372.776077	52.455420	66.681217
1371.689091	46.837491	66.686222
1370.860851	50.993638	66.691226
1370.461828	45.217473	66.696231
1370.329507	53.967175	66.701236
1369.048187	51.286533	66.706241
1368.207854	48.871698	66.711246
1367.847428	55.640684	66.716250
1367.163354	45.718180	66.721255
1366.180211	56.624827	66.726260
1365.322637	59.177107	66.731265
1365.392693	51.586955	66.736270
1364.085941	55.737163	66.741274
1363.792996	61.191252	66.746279
1363.596056	52.618493	66.751284
1362.494655	58.357210	66.756289
1362.178341	45.652783	66.761294
1361.414027	53.946264	66.766298
1360.395404	56.379061	66.771303
1359.578334	49.939198	66.776308
1358.818771	52.923766	66.781313
1358.781249	53.845978	66.786318
1358.228234	60.315988	66.791322
1357.416361	54.741067	66.796327
1356.472883	54.857935	66.801332
1355.824928	52.581261	66.806337
1355.746212	51.764289	66.811342
1354.345803	52.822712	66.816346
1353.619144	47.727849	66.821351
1353.226640	47.096377	66.826356
1352.863524	55.505864	66.831361
1351.939017	49.970929	66.836366
1350.822881	52.633701	66.841370
1350.386528	50.561520	66.846375
1350.116631	54.769274	66.851380
1349.465420	54.980038	66.856385
1349.085909	42.154773	66.861390
1347.709394	55.068384	66.866394
1347.245970	42.330577	66.871399
1346.483983	45.350226	66.876404
1345.853003	56.662958	66.881409
1345.307070	42.511087	66.886414
1344.375846	52.209393	66.891418
1344.256088	45.698118	66.896423
1343.942197	46.825113	66.901428
1342.838315	53.439461	66.906433
1342.169232	35.935564	66.911438
1341.029339	42.323813	66.916442
1341.119784	39.324205	66.921447
1339.675480	45.450179	66.926452
1338.768247	50.617128	66.931457
1338.876422	38.190598	66.936462
1338.073565	53.376931	66.941466
1337.859441	44.116190	66.946471
1336.823259	43.514500	66.951476
1335.975317	44.196521	66.956481
1335.947588	38.388153	66.961486
1334.861173	46.032652	66.966490
1333.689708	46.786603	66.971495
1333.270612	41.688590	66.976500
1332.386019	54.963990	66.981505
1332.522655	38.019583	66.986510
1331.446040	45.802878	66.991514
1330.579698	45.765564	66.996519
1329.703053	53.250563	67.001524
1329.251423	48.889445	67.006529
1329.137988	46.518349	67.011534
1328.878488	46.867127	67.016538
1327.342626	46.802201	67.021543
1327.086318	44.187305	67.026548
1326.326440	51.647434	67.031553
1325.373072	44.642612	67.036558
1324.511720	55.159315	67.041562
1323.851907	46.784730	67.046567
1323.810387	45.061385	67.051572
1323.284580	48.497669	67.056577
1322.264127	45.397107	67.061582
1321.083336	52.342240	67.066586
1320.486247	49.215377	67.071591
1320.370647	52.625878	67.076596
1319.587539	47.387031	67.081601
1319.315041	43.169333	67.086606
1318.206696	51.230499	67.091610
1317.645874	54.819012	67.096615
1317.162191	53.623284	67.101620
1316.337112	49.733131	67.106625
1315.403855	45.984759	67.111630
1314.965088	53.338650	67.116634
1314.697560	45.963023	67.121639
1313.683963	48.136411	67.126644
1312.441163	52.002078	67.131649
1312.250883	50.885868	67.136654
1311.555843	55.497110	67.141658
1311.268161	53.760855	67.146663
1310.365907	57.884632	67.151668
1309.366256	53.295239	67.156673
1309.116213	52.445579	67.161678
1308.764633	49.148800	67.166682
1307.640543	51.300331	67.171687
1306.576097	55.874104	67.176692
1306.022919	57.289887	67.181697
1305.777829	58.909010	67.186702
1305.341696	49.863343	67.191706
1304.654254	49.239341	67.196711
1303.870499	45.113961	67.201716
1303.152020	49.809355	67.206721
1302.917575	42.776988	67.211726
1301.378034	49.334448	67.216730
1300.663798	50.110345	67.221735
1300.725353	52.242128	67.226740
1299.828645	53.666792	67.231745
1299.177706	54.437358	67.236750
1298.019453	42.466057	67.241754
1297.597679	48.435802	67.246759
1297.298561	44.769554	67.251764
1296.445138	51.000315	67.256769
1295.636791	54.940429	67.261774
1294.657040	48.375063	67.266778
1293.997582	48.390028	67.271783
1294.040316	54.751141	67.276788
1293.816781	53.627603	67.281793
1292.527422	46.116379	67.286798
1291.450926	56.665716	67.291802
1291.154667	46.817206	67.296807
1291.060695	43.643484	67.301812
1289.704726	47.440417	67.306817
1289.120753	38.337838	67.311822
1288.198778	42.048427	67.316826
1288.265038	43.267960	67.321831
1287.583316	44.686834	67.326836
1286.026806	49.189027	67.331841
1285.948491	39.730085	67.336846
1285.383480	54.216277	67.341850
1284.954196	54.189920	67.346855
1283.826574	46.413285	67.351860
1282.726505	51.689758	67.356865
1282.812413	46.793749	67.361870
1282.149183	48.872021	67.366874
1281.376243	48.469782	67.371879
1280.404060	47.395882	67.376884
1279.758140	53.147370	67.381889
1279.491823	42.172864	67.386894
1278.675064	52.777105	67.391898
1277.340823	39.395582	67.396903
1277.186686	47.087430	67.401908
1276.631384	52.518575	67.406913
1276.433980	47.326978	67.411918
1275.430165	55.013565	67.416922
1274.945946	47.377498	67.421927
1274.159948	51.255714	67.426932
1273.450027	49.436782	67.431937
1272.593484	48.161568	67.436942
1271.723732	46.986228	67.441946
1271.243673	52.365987	67.446951
1270.904979	48.362251	67.451956
1270.101839	57.705893	67.456961
1269.128294	41.382709	67.461966
1268.653334	49.008868	67.466970
1268.128564	46.824601	67.471975
1267.536502	50.113730	67.476980
1266.830846	38.769100	67.481985
1266.039366	42.930469	67.486990
1265.406002	49.052131	67.491994
1264.998328	47.498969	67.496999
1263.978858	36.697833	67.502004
1262.788321	44.201211	67.507009
1262.606216	33.911933	67.512014
1261.877913	35.756121	67.517018
1261.834433	32.050815	67.522023
1261.258280	34.306062	67.527028
1259.765378	45.574480	67.532033
1259.611485	39.852409	67.537038
1259.047987	44.734489	67.542042
1258.067064	44.685453	67.547047
1257.309844	38.092613	67.552052
1256.224136	49.307334	67.557057
1256.214093	45.983071	67.562062
1255.916910	50.098971	67.567066
1255.149574	46.401515	67.572071
1254.015857	41.374562	67.577076
1253.307458	44.871429	67.582081
1253.343809	37.231455	67.587086
1252.097513	46.571435	67.592090
1251.642208	43.174461	67.597095
1250.573848	37.506323	67.602100
1250.216400	48.300896	67.607105
1250.221322	47.200965	67.612110
1249.054699	40.430364	67.617114
1248.264643	48.806807	67.622119
1247.896273	45.038034	67.627124
1246.521863	48.147199	67.632129
1245.794559	44.244681	67.637134
1245.119626	43.156650	67.642138
1245.039544	37.033329	67.647143
1244.795607	45.777113	67.652148
1243.881781	41.931061	67.657153
1242.849416	47.165243	67.662158
1242.065421	44.542795	67.667162
1241.819736	44.116660	67.672167
1241.506002	42.236322	67.677172
1240.542496	42.744356	67.682177
1239.736837	41.849003	67.687182
1239.071102	53.627752	67.692186
1237.846293	44.292758	67.697191
1237.090976	47.428073	67.702196
1236.644219	46.090869	67.707201
1236.826456	40.211275	67.712206
1236.306159	43.252449	67.717210
1235.316590	40.984396	67.722215
1234.232576	48.018254	67.727220
1233.692770	46.405680	67.732225
1233.445974	41.461647	67.737230
1231.943255	48.131563	67.742234
1231.092618	48.867664	67.747239
1230.937992	38.703333	67.752244
1230.138886	45.385953	67.757249
1230.147253	37.196907	67.762254
1229.538658	44.617229	67.767258
1228.240783	42.806641	67.772263
1227.989812	41.091371	67.777268
1227.163551	46.625532	67.782273
1226.472663	35.617624	67.787278
1225.381173	40.391268	67.792282
1224.992164	43.714351	67.797287
1224.441189	42.273871	67.802292
1223.927645	50.089100	67.807297
1223.314980	45.045544	67.812302
1222.165219	49.779571	67.817306
1221.871129	44.959756	67.822311
1221.848376	36.627422	67.827316
1220.499678	47.833506	67.832321
1219.916496	34.856162	67.837326
1219.258025	45.104073	67.842330
1218.404615	39.578394	67.847335
1217.365076	37.293062	67.852340
1216.684380	50.119734	67.857345
1216.548172	45.676947	67.862350
1216.104158	54.594479	67.867354
1215.433964	44.050068	67.872359
1214.994429	48.052985	67.877364
1213.487192	48.174391	67.882369
1213.213347	36.975591	67.887374
1212.906614	47.607555	67.892378
1211.653144	43.462277	67.897383
1211.015295	36.834704	67.902388
1210.056945	48.511745	67.907393
1210.063567	44.833165	67.912398
1209.418176	42.176073	67.917402
1208.926533	46.133658	67.922407
1207.800959	42.396987	67.927412
1207.323870	44.846233	67.932417
1207.181453	35.514194	67.937422
1205.989234	43.796894	67.942426
1204.764496	39.766904	67.947431
1204.733652	43.700102	67.952436
1203.868350	43.258956	67.957441
1203.725751	43.540271	67.962446
1202.630199	47.267451	67.967450
1201.746239	38.404996	67.972455
1201.333644	43.963272	67.977460
1200.917198	49.135799	67.982465
1200.571280	43.269224	67.987470
1198.973475	44.587782	67.992474
1198.391526	44.189891	67.997479
1198.328938	45.822579	68.002484
1197.597039	47.392962	68.007489
1196.822988	37.552646	68.012494
1195.820518	44.671321	68.017498
1195.283246	48.773363	68.022503
1195.155380	36.701358	68.027508
1193.915453	46.494520	68.032513
1193.164716	33.089659	68.037518
1192.790264	44.355299	68.042522
1192.267472	49.555777	68.047527
1191.932719	37.381050	68.052532
1190.379012	47.312422	68.057537
1189.787128	45.845337	68.062542
1189.290476	49.407899	68.067546
1188.994641	44.225659	68.072551
1188.175764	39.536613	68.077556
1187.203283	49.216285	68.082561
1187.304089	49.037839	68.087566
1186.557645	49.090320	68.092570
1185.167100	44.574183	68.097575
1184.703893	44.146375	68.102580
1183.715957	46.795135	68.107585
1183.427343	39.399234	68.112590
1183.254067	42.643859	68.117594
1182.194635	47.874482	68.122599
1181.612714	45.049604	68.127604
1180.555338	49.049849	68.132609
1180.563459	35.010218	68.137614
1179.438048	41.946594	68.142618
1178.582766	58.907520	68.147623
1178.062101	39.812563	68.152628
1177.418383	57.238172	68.157633
1177.298935	47.989212	68.162638
1176.609937	45.066243	68.167642
1175.703811	50.751894	68.172647
1175.067156	43.184254	68.177652
1174.097613	49.170156	68.182657
1173.439610	37.877911	68.187662
1172.305418	47.627459	68.192666
1171.885534	48.184689	68.197671
1171.583256	46.600589	68.202676
1171.350099	47.284247	68.207681
1170.994697	49.054966	68.212686
1169.945345	49.726492	68.217690
1169.380860	46.066195	68.222695
1168.058904	51.720203	68.227700
1167.271091	44.936712	68.232705
1166.698008	43.744193	68.237710
1166.497784	49.905805	68.242714
1165.967004	45.582544	68.247719
1165.417637	42.678375	68.252724
1163.963724	43.049956	68.257729
1163.646692	42.073768	68.262734
1163.434694	47.418794	68.267738
1162.346616	45.268940	68.272743
1161.572852	48.350438	68.277748
1161.001150	49.455374	68.282753
1160.588219	38.906346	68.287758
1159.559138	47.546329	68.292762
1158.853901	45.721955	68.297767
1157.977104	42.597042	68.302772
1157.560613	52.383851	68.307777
1157.485396	44.567653	68.312782
1156.750320	43.806185	68.317786
1155.667767	48.914335	68.322791
1155.366390	42.906641	68.327796
1154.774776	39.387861	68.332801
1153.726840	38.717152	68.337806
1152.810639	39.985688	68.342810
1152.052141	46.761220	68.347815
1152.036567	35.658560	68.352820
1151.346348	53.433768	68.357825
1150.821329	32.382480	68.362830
1149.771962	37.657243	68.367834
1149.056547	48.220158	68.372839
1148.910821	45.237607	68.377844
1147.426720	55.531682	68.382849
1147.119320	43.750012	68.387854
1146.452322	46.279935	68.392858
1145.912281	39.933300	68.397863
1145.760468	39.959034	68.402868
1144.242146	57.372349	68.407873
1143.948929	34.685129	68.412878
1143.473786	42.596760	68.417882
1142.688834	46.615196	68.422887
1141.965963	33.697946	68.427892
1140.939955	49.082223	68.432897
1140.502301	58.046060	68.437902
1140.249151	39.345400	68.442906
1138.987166	39.751127	68.447911
1138.553852	43.393510	68.452916
1137.984933	41.665737	68.457921
1137.669871	36.549647	68.462926
1136.483970	42.986292	68.467930
1135.599484	46.746163	68.472935
1134.952535	37.637882	68.477940
1134.515614	42.409962	68.482945
1134.167522	43.197059	68.487950
1133.492029	47.494562	68.492954
1132.721135	45.223312	68.497959
1132.099025	42.654004	68.502964
1131.239695	56.849542	68.507969
1130.915301	46.617603	68.512974
1129.956694	42.709332	68.517978
1129.227156	51.811054	68.522983
1129.040786	42.656328	68.527988
1127.980653	48.319177	68.532993
1127.020186	46.637909	68.537998
1126.283027	43.676883	68.543002
1125.916207	39.288132	68.548007
1125.895843	39.182573	68.553012
1124.509861	45.449191	68.558017
1124.017160	27.824309	68.563022
1123.367910	36.586817	68.568026
1122.724286	43.047610	68.573031
1122.667689	35.654246	68.578036
1121.227978	45.644794	68.583041
1120.332379	42.757856	68.588046
1120.110830	39.039876	68.593050
1119.630890	45.012580	68.598055
1119.091826	35.477130	68.603060
1118.148696	50.526526	68.608065
1117.584362	40.733312	68.613070
1117.278493	36.683384	68.618074
1115.985019	50.287211	68.623079
1115.295117	41.105339	68.628084
1114.444729	42.527428	68.633089
1114.397372	34.818776	68.638094
1113.666557	47.841091	68.643098
1112.478017	49.253885	68.648103
1112.211048	38.512917	68.653108
1111.510254	49.592343	68.658113
1111.160321	35.843064	68.663118
1109.896311	48.417163	68.668122
1108.986459	42.361174	68.673127
1108.545902	47.789864	68.678132
1108.098906	41.835302	68.683137
1107.860914	38.810660	68.688142
1107.516049	44.134240	68.693146
1106.409697	40.481296	68.698151
1106.018810	39.059536	68.703156
1104.606639	45.508529	68.708161
1103.865576	41.180883	68.713166
1103.311971	42.577850	68.718170
1102.951129	41.657524	68.723175
1102.666149	47.042546	68.728180
1101.944523	46.854555	68.733185
1100.821026	45.618708	68.738190
1100.545174	36.557073	68.743194
1099.984169	45.455368	68.748199
1098.981829	36.006226	68.753204
1098.010568	46.005855	68.758209
1097.612954	41.756051	68.763214
1097.292790	37.668974	68.768218
1096.212127	43.710420	68.773223
1095.636225	44.119010	68.778228
1094.845044	46.785393	68.783233
1094.720507	41.006632	68.788238
1093.915070	43.520738	68.793242
1092.809966	43.113042	68.798247
1092.479054	39.784629	68.803252
1091.530791	44.228031	68.808257
1091.394667	44.196079	68.813262
1089.799656	42.530599	68.818266
1089.340716	46.058791	68.823271
1089.175521	44.071267	68.828276
1088.560232	47.625905	68.833281
1088.149894	38.448465	68.838286
1087.030105	42.329357	68.843290
1086.168731	51.950385	68.848295
1085.888216	50.621461	68.853300
1085.183603	51.518891	68.858305
1084.143696	50.659271	68.863310
1083.423270	54.391488	68.868314
1082.966853	51.642868	68.873319
1082.809665	35.048016	68.878324
1082.159120	49.166191	68.883329
1081.239712	49.159480	68.888334
1080.277816	42.045737	68.893338
1080.072605	42.267631	68.898343
1079.621101	30.226630	68.903348
1078.261609	43.047741	68.908353
1077.694934	48.236292	68.913358
1077.446935	39.316889	68.918362
1076.304174	42.698381	68.923367
1075.643315	29.594677	68.928372
1075.056115	46.626505	68.933377
1074.575360	40.387157	68.938382
1074.083597	43.370203	68.943386
1073.190039	36.601995	68.948391
1072.578057	43.330583	68.953396
1071.774893	50.674647	68.958401
1071.605612	44.341597	68.963406
1070.603886	42.972851	68.968410
1069.435755	44.472306	68.973415
1069.421696	34.824975	68.978420
1068.290721	45.933407	68.983425
1068.233863	37.106609	68.988430
1067.182808	39.650329	68.993434
1066.372827	50.531083	68.998439
1065.919999	36.213122	69.003444
1065.040877	42.460645	69.008449
1065.040808	35.238072	69.013454
1063.979933	40.265532	69.018458
1063.051634	43.343251	69.023463
1062.925329	32.827511	69.028468
1062.265004	37.037457	69.033473
1061.311380	30.639941	69.038478
1060.406824	35.065359	69.043482
1059.830546	41.859233	69.048487
1059.670824	38.470479	69.053492
1058.813050	37.916219	69.058497
1057.938335	41.283466	69.063502
1057.434093	40.262954	69.068506
1056.954907	41.061452	69.073511
1056.303333	28.325295	69.078516
1055.032982	39.438550	69.083521
1054.753011	41.107395	69.088526
1054.326359	40.019347	69.093530
1053.369787	40.657237	69.098535
1052.807015	26.408820	69.103540
1051.966498	40.793756	69.108545
1051.565883	38.802684	69.113550
1050.783814	46.684302	69.118554
1049.525115	35.246383	69.123559
1049.021247	37.433402	69.128564
1048.460513	42.499583	69.133569
1048.031567	36.835487	69.138574
1047.605053	33.082313	69.143578
1047.068434	30.830597	69.148583
1046.462555	38.428712	69.153588
1045.338061	41.860928	69.158593
1044.915202	33.824078	69.163598
1043.870524	42.509154	69.168602
1043.030820	42.690055	69.173607
1042.622096	33.758383	69.178612
1042.166233	41.558145	69.183617
1041.991721	41.341487	69.188622
1041.488631	34.933811	69.193626
1040.168121	42.073165	69.198631
1039.736840	33.771145	69.203636
1038.576952	40.571128	69.208641
1037.716931	42.373250	69.213646
1037.311894	40.308766	69.218650
1036.584313	42.815234	69.223655
1036.487745	32.649589	69.228660
1035.809576	38.603372	69.233665
1034.988893	31.788896	69.238670
1034.370833	23.740528	69.243674
1033.491192	39.151999	69.248679
1033.198834	23.610025	69.253684
1032.104489	33.723863	69.258689
1031.417267	34.782546	69.263694
1031.139632	31.119234	69.268698
1030.357288	40.210444	69.273703
1029.875549	26.994686	69.278708
1028.703231	45.915783	69.283713
1028.320515	27.470755	69.288718
1028.092276	36.598396	69.293722
1026.514577	43.967910	69.298727
1025.972666	30.592984	69.303732
1025.121418	34.134706	69.308737
1024.900037	34.121051	69.313742
1024.843276	30.148208	69.318746
1024.217518	33.832257	69.323751
1023.265022	28.604703	69.328756
1022.570791	47.804569	69.333761
1022.024919	41.075688	69.338766
1021.020894	36.890832	69.343770
1019.894669	39.523802	69.348775
1019.718814	34.549595	69.353780
1019.063104	33.937972	69.358785
1018.630364	32.915555	69.363790
1017.438578	40.461803	69.368794
1016.623309	38.658131	69.373799
1016.473532	36.431615	69.378804
1015.869059	37.127047	69.383809
1015.202546	43.588347	69.388814
1014.230016	36.496830	69.393818
1013.682040	37.355167	69.398823
1013.409511	38.437770	69.403828
1012.213955	41.198470	69.408833
1011.364649	40.059395	69.413838
1010.744670	34.457240	69.418842
1010.284805	42.262373	69.423847
1010.420916	33.758128	69.428852
1009.603201	44.420918	69.433857
1008.639208	42.473749	69.438862
1008.170913	36.965736	69.443866
1007.360156	42.076431	69.448871
1006.270964	39.715509	69.453876
1005.692690	39.304463	69.458881
1005.443500	34.871792	69.463886
1004.590946	47.415162	69.468890
1003.512671	48.428832	69.473895
1003.253262	40.224057	69.478900
1002.670735	46.897508	69.483905
1002.505807	43.419698	69.488910
1001.290091	38.344416	69.493914
1000.428401	37.429670	69.498919
1000.215504	37.668562	69.503924
998.914069	46.938563	69.508929
998.056565	48.401247	69.513934
997.714395	35.754656	69.518938
997.115548	44.822990	69.523943
996.685398	35.010049	69.528948
996.056227	44.053244	69.533953
995.389467	34.878779	69.538958
994.400853	43.045585	69.543962
993.623571	46.638630	69.548967
993.238511	34.380497	69.553972
992.593650	39.262947	69.558977
992.253371	31.848498	69.563982
991.282359	40.096083	69.568986
990.581484	32.321104	69.573991
990.307930	30.052780	69.578996
989.401275	34.622059	69.584001
988.540433	37.502985	69.589006
988.109134	32.577308	69.594010
987.399688	34.085825	69.599015
987.109049	34.726602	69.604020
985.728507	47.243590	69.609025
985.158385	40.821360	69.614030
984.740426	43.655480	69.619034
984.085439	41.574001	69.624039
983.149849	42.829911	69.629044
982.717872	38.956190	69.634049
981.938543	40.778609	69.639054
981.809450	35.847429	69.644058
980.581009	52.810976	69.649063
979.873900	35.926743	69.654068
979.316677	41.679942	69.659073
979.026825	35.563215	69.664078
978.554924	30.079440	69.669082
977.291658	39.592536	69.674087
976.767620	32.353986	69.679092
976.039006	35.658587	69.684097
975.438357	38.898674	69.689102
974.810687	38.356719	69.694106
973.836185	35.922372	69.699111
973.558695	32.834645	69.704116
973.099220	42.095275	69.709121
972.129634	29.745645	69.714126
971.111208	28.045278	69.719130
970.285418	40.106565	69.724135
970.260470	33.933500	69.729140
969.682293	42.919699	69.734145
969.131394	42.258296	69.739150
968.417735	44.082887	69.744154
967.327014	40.771304	69.749159
967.303734	28.345233	69.754164
965.928407	40.087094	69.759169
965.216183	37.898030	69.764174
964.939009	28.147497	69.769178
964.422375	34.607034	69.774183
964.069017	33.450569	69.779188
962.935488	45.978727	69.784193
962.375716	42.030724	69.789198
961.876738	30.449908	69.794202
960.535379	37.389181	69.799207
959.988774	35.867641	69.804212
959.390275	39.681411	69.809217
959.127590	37.187429	69.814222
958.691972	40.808124	69.819226
957.740165	37.698376	69.824231
957.032663	32.766189	69.829236
956.264882	29.109912	69.834241
955.692738	32.146766	69.839246
954.779747	31.125079	69.844250
953.945872	36.945954	69.849255
953.822634	31.258471	69.854260
953.250045	31.877881	69.859265
952.454969	37.310952	69.864270
951.686916	37.210818	69.869274
950.678368	41.264880	69.874279
950.447859	31.036981	69.879284
949.953438	40.566530	69.884289
949.101919	35.900115	69.889294
948.282039	42.305404	69.894298
947.603856	35.879880	69.899303
947.484121	36.072414	69.904308
946.328897	44.409251	69.909313
945.154049	43.366153	69.914318
945.062677	31.641636	69.919322
944.602273	37.480360	69.924327
944.050407	36.571530	69.929332
943.057005	35.149472	69.934337
942.336065	33.302432	69.939342
941.958647	34.526313	69.944346
941.173724	39.577720	69.949351
940.264712	33.912764	69.954356
939.691633	40.327671	69.959361
938.967036	34.732722	69.964366
938.889573	32.370124	69.969370
937.630747	43.770181	69.974375
936.866485	39.911494	69.979380
936.370773	29.732107	69.984385
935.902508	31.378883	69.989390
935.320218	29.419895	69.994394
934.616375	34.021576	69.999399
933.652467	23.412057	70.004404
933.119078	34.937956	70.009409
932.726401	34.478471	70.014414
931.894970	41.142650	70.019418
930.961571	32.154143	70.024423
930.354202	32.826401	70.029428
930.085666	26.241086	70.034433
929.576425	35.355090	70.039438
928.885786	28.688703	70.044442
927.817184	41.389466	70.049447
927.521793	30.788690	70.054452
926.262828	39.447973	70.059457
925.294409	38.245879	70.064462
924.904370	41.272687	70.069466
924.439660	36.970517	70.074471
924.045631	29.280780	70.079476
923.703045	46.731016	70.084481
922.748284	37.280698	70.089486
922.154853	34.897700	70.094490
921.433020	40.155120	70.099495
920.958743	34.840472	70.104500
919.754615	37.501650	70.109505
919.059629	35.633139	70.114510
918.961242	28.355262	70.119514
918.135548	36.385774	70.124519
917.394438	32.383061	70.129524
916.703948	42.349097	70.134529
915.935694	34.155926	70.139534
915.721403	34.839757	70.144538
914.312044	42.401743	70.149543
913.716124	38.877406	70.154548
913.672271	37.772625	70.159553
912.732227	34.069656	70.164558
912.238490	33.448057	70.169562
911.293521	37.843682	70.174567
911.073973	37.187913	70.179572
910.228961	44.133386	70.184577
909.200336	44.908955	70.189582
908.619614	30.187196	70.194586
907.726920	43.583809	70.199591
907.755822	35.938738	70.204596
907.078099	40.290261	70.209601
905.874166	44.078958	70.214606
905.170025	39.422223	70.219610
905.019415	32.431783	70.224615
904.375614	33.215502	70.229620
903.268251	44.701859	70.234625
902.455999	28.157684	70.239630
902.418366	35.018830	70.244634
901.670460	39.577068	70.249639
900.973492	34.018738	70.254644
900.277645	33.596464	70.259649
899.501061	35.058917	70.264654
899.257478	32.353742	70.269658
897.703780	34.731506	70.274663
897.227264	36.657151	70.279668
896.714952	42.534106	70.284673
896.218051	43.065788	70.289678
896.050381	35.242261	70.294682
894.646182	43.979866	70.299687
894.238285	38.804474	70.304692
893.878597	35.091160	70.309697
893.013219	39.524589	70.314702
892.052132	36.875248	70.319706
891.173831	49.731829	70.324711
890.899663	39.378418	70.329716
890.111458	42.385013	70.334721
889.454879	35.317393	70.339726
888.672869	28.950994	70.344730
888.015051	36.808138	70.349735
887.925915	31.069504	70.354740
887.314417	37.660846	70.359745
886.276558	37.162113	70.364750
885.507086	36.658518	70.369754
884.625514	34.666743	70.374759
884.472367	35.900675	70.379764
883.888602	30.294374	70.384769
883.039176	36.105125	70.389774
882.369113	34.619020	70.394778
881.594288	42.258242	70.399783
881.361199	29.909726	70.404788
880.139535	36.688059	70.409793
879.171306	35.061745	70.414798
879.014818	34.537872	70.419802
878.330442	42.973270	70.424807
878.120067	33.464439	70.429812
877.208607	36.479613	70.434817
876.417799	39.201192	70.439822
875.978779	29.120036	70.444826
875.039278	38.017086	70.449831
874.437432	33.173770	70.454836
873.571579	33.543395	70.459841
872.856910	38.878534	70.464846
873.016136	37.990599	70.469850
871.532239	43.681551	70.474855
871.321381	30.575701	70.479860
870.852941	30.954622	70.484865
869.932918	38.323633	70.489870
868.904905	35.517792	70.494874
867.992163	42.426745	70.499879
867.514910	31.966890	70.504884
867.504748	33.840399	70.509889
866.250795	30.755121	70.514894
865.922159	30.381651	70.519898
864.650146	36.059384	70.524903
864.626754	35.632605	70.529908
864.287776	33.554486	70.534913
863.014219	39.112616	70.539918
862.350457	31.328623	70.544922
861.713065	41.942243	70.549927
861.723312	29.652779	70.554932
860.533904	36.853348	70.559937
859.901051	36.876808	70.564942
859.279326	33.080622	70.569946
858.503120	43.005116	70.574951
857.870590	34.484433	70.579956
856.769809	31.587675	70.584961
855.905002	29.296771	70.589966
855.918813	33.330084	70.594970
855.581072	34.995525	70.599975
855.020747	31.919712	70.604980
854.136416	35.020464	70.609985
853.378497	34.038791	70.614990
852.945632	32.122276	70.619994
851.776044	30.507519	70.624999
851.156236	23.861428	70.630004
850.776918	23.991198	70.635009
849.969152	30.290498	70.640014
848.802739	26.385461	70.645018
848.378416	30.168375	70.650023
848.069945	32.819503	70.655028
847.247561	33.361995	70.660033
846.995980	32.985726	70.665038
846.516220	29.537542	70.670042
845.223682	29.965623	70.675047
844.636109	30.999034	70.680052
844.220910	33.389600	70.685057
842.836200	35.104977	70.690062
842.608957	28.274980	70.695066
841.921335	39.415421	70.700071
841.940379	33.035088	70.705076
840.845481	30.724039	70.710081
839.676977	31.965029	70.715086
839.323211	34.386820	70.720090
838.904820	32.327652	70.725095
838.326411	23.240117	70.730100
837.513459	34.403657	70.735105
836.205406	35.504430	70.740110
836.242624	30.133628	70.745114
835.380433	35.864421	70.750119
835.071612	25.436122	70.755124
833.810347	23.323447	70.760129
832.946273	36.272383	70.765134
832.776662	26.544185	70.770138
832.371328	37.001020	70.775143
831.724731	33.221417	70.780148
830.789389	30.679970	70.785153
830.256109	38.905241	70.790158
829.846595	29.642586	70.795162
828.806816	27.737516	70.800167
827.995397	28.595242	70.805172
827.476789	35.083497	70.810177
827.011412	34.768067	70.815182
826.070550	26.987192	70.820186
825.232399	31.138756	70.825191
824.988347	28.722254	70.830196
824.852846	31.863104	70.835201
823.357283	35.527937	70.840206
822.411144	32.056215	70.845210
822.169369	36.127053	70.850215
821.634869	28.874446	70.855220
821.230979	27.263991	70.860225
820.151466	39.741012	70.865230
819.440758	24.595274	70.870234
818.470778	31.846089	70.875239
818.594221	31.096313	70.880244
817.721355	36.412487	70.885249
816.635205	34.786043	70.890254
816.372327	23.066774	70.895258
815.772488	36.044620	70.900263
815.345308	33.138440	70.905268
814.245935	29.858272	70.910273
813.389945	28.881183	70.915278
812.926687	27.907817	70.920282
812.554380	33.084394	70.925287
811.769206	24.723648	70.930292
810.651198	33.589201	70.935297
810.003716	35.026400	70.940302
809.825076	19.788099	70.945306
809.199932	33.919589	70.950311
808.407642	23.960919	70.955316
807.928896	26.003629	70.960321
807.100960	30.975179	70.965326
806.528077	32.331118	70.970330
805.579134	31.420867	70.975335
804.771497	24.891421	70.980340
804.809726	28.525021	70.985345
804.054219	36.083909	70.990350
803.022384	22.435388	70.995354
802.257880	33.092896	71.000359
801.929271	26.701672	71.005364
800.817656	37.168425	71.010369
799.678488	31.074955	71.015374
799.316209	27.314764	71.020378
798.344662	29.085827	71.025383
798.368751	26.222941	71.030388
798.418757	26.900982	71.035393
797.618837	36.660521	71.040398
796.874251	37.037679	71.045402
795.766521	37.335443	71.050407
795.617604	19.898832	71.055412
794.914905	36.859157	71.060417
793.647385	32.987586	71.065422
793.290933	27.868688	71.070426
792.244741	36.714933	71.075431
791.396418	41.696044	71.080436
790.857113	34.461555	71.085441
790.270808	40.126370	71.090446
790.254341	29.225757	71.095450
789.690499	35.599790	71.100455
788.545525	36.581588	71.105460
787.896634	37.826625	71.110465
787.229979	41.797937	71.115470
786.910592	31.415483	71.120474
785.697889	44.476700	71.125479
785.134530	30.296285	71.130484
784.878715	29.680996	71.135489
783.803903	24.912995	71.140494
782.967835	30.636489	71.145498
782.063747	32.726409	71.150503
781.676480	28.435602	71.155508
781.536244	28.888454	71.160513
780.895919	30.233056	71.165518
780.394709	23.031936	71.170522
779.397618	42.615916	71.175527
779.018057	36.586046	71.180532
777.619736	26.410037	71.185537
776.829736	39.309348	71.190542
776.676851	17.372673	71.195546
776.176446	31.306109	71.200551
775.338973	28.061542	71.205556
774.552618	32.356266	71.210561
773.693749	31.147833	71.215566
773.384395	34.146045	71.220570
772.704564	40.197918	71.225575
772.040760	44.921001	71.230580
771.657348	37.934518	71.235585
770.618756	37.991047	71.240590
770.350907	27.116263	71.245594
769.582776	35.476697	71.250599
768.702903	41.328599	71.255604
768.089720	35.132491	71.260609
767.431319	42.248571	71.265614
766.963897	33.550246	71.270618
765.925795	36.021057	71.275623
765.338070	24.145350	71.280628
764.815251	28.681980	71.285633
764.162704	32.534353	71.290638
763.226170	29.387562	71.295642
762.605129	36.376266	71.300647
761.844287	34.376357	71.305652
761.857487	30.635249	71.310657
760.967220	35.563119	71.315662
759.958158	25.112265	71.320666
759.129177	39.541146	71.325671
758.804979	32.206192	71.330676
758.539525	20.839015	71.335681
757.621891	31.290669	71.340686
756.931667	21.572822	71.345690
756.406925	31.551917	71.350695
755.196278	27.013714	71.355700
754.563266	26.764408	71.360705
753.493853	35.261118	71.365710
753.626719	29.450886	71.370714
753.071823	32.417223	71.375719
752.621089	32.000126	71.380724
751.449352	33.060318	71.385729
750.527069	36.980867	71.390734
750.332309	22.099964	71.395738
750.089526	38.428829	71.400743
749.091231	30.392198	71.405748
747.717397	30.708689	71.410753
747.435776	24.022987	71.415758
747.195846	21.771422	71.420762
746.328656	37.150997	71.425767
745.554744	38.964737	71.430772
744.914259	31.498784	71.435777
744.232613	33.688926	71.440782
743.811845	26.363043	71.445786
742.875790	31.381785	71.450791
742.239140	40.451438	71.455796
741.837643	26.882376	71.460801
741.156137	31.362270	71.465806
740.188028	27.299560	71.470810
739.412303	31.912728	71.475815
738.966411	37.870593	71.480820
738.802175	36.302426	71.485825
737.384425	29.513735	71.490830
736.987811	23.451901	71.495834
736.104872	39.223501	71.500839
735.797291	28.498554	71.505844
735.595670	32.728585	71.510849
734.524490	31.719548	71.515854
734.311105	30.211247	71.520858
733.209996	37.976561	71.525863
731.892545	32.477645	71.530868
731.454469	21.048068	71.535873
730.494317	32.936817	71.540878
730.565541	33.054805	71.545882
730.012052	35.270280	71.550887
729.307187	34.923608	71.555892
728.586953	32.444152	71.560897
727.736206	37.345240	71.565902
727.313998	29.177481	71.570906
726.144634	36.267677	71.575911
725.516896	36.288779	71.580916
725.381978	35.591170	71.585921
724.722489	39.078798	71.590926
723.876801	33.870640	71.595930
722.890000	43.431289	71.600935
722.564612	33.688481	71.605940
722.265439	33.833897	71.610945
721.094589	46.338109	71.615950
720.211406	38.447167	71.620954
719.559771	37.513271	71.625959
719.089788	31.702820	71.630964
719.094348	29.267252	71.635969
718.032530	33.489150	71.640974
717.544892	28.392729	71.645978
716.822622	32.191556	71.650983
715.614290	27.151527	71.655988
714.754707	23.238710	71.660993
714.390269	29.289265	71.665998
714.143813	28.953195	71.671002
713.546096	31.934242	71.676007
712.648085	25.501223	71.681012
711.842246	25.131207	71.686017
710.989696	46.560913	71.691022
710.720886	16.860315	71.696026
709.746432	38.233722	71.701031
709.007185	26.896252	71.706036
708.364030	20.014224	71.711041
707.710371	37.731585	71.716046
707.690448	24.029245	71.721050
706.932999	29.746549	71.726055
705.793742	24.339132	71.731060
705.148133	26.157686	71.736065
704.221338	36.760628	71.741070
704.284112	24.860224	71.746074
703.230610	31.533005	71.751079
702.847840	30.685620	71.756084
702.235285	27.081991	71.761089
701.579707	28.531543	71.766094
701.039096	23.189669	71.771098
699.718687	30.076835	71.776103
699.594315	23.977974	71.781108
698.994244	31.240895	71.786113
697.704172	31.870513	71.791118
697.456165	25.248854	71.796122
696.801659	36.267346	71.801127
695.847486	36.979106	71.806132
695.367172	25.245596	71.811137
694.010581	33.720237	71.816142
694.038002	28.882445	71.821146
693.437559	34.265669	71.826151
692.752301	34.871535	71.831156
693.000861	27.886959	71.836161
691.446755	36.229044	71.841166
691.185994	30.970348	71.846170
690.241999	36.777286	71.851175
689.170337	40.750024	71.856180
688.786698	30.738953	71.861185
687.834378	42.984448	71.866190
688.178375	30.870529	71.871194
686.522776	41.810295	71.876199
685.988681	28.544639	71.881204
685.706596	30.194930	71.886209
685.041810	33.314397	71.891214
684.249141	29.971265	71.896218
683.450636	32.996903	71.901223
682.747915	35.959982	71.906228
682.395209	33.040394	71.911233
681.224084	30.971794	71.916238
680.859766	30.153015	71.921242
680.050805	37.893910	71.926247
679.617030	31.978354	71.931252
679.465468	21.231738	71.936257
678.046757	33.559372	71.941262
677.044936	26.076859	71.946266
676.770145	36.539724	71.951271
676.076376	24.130568	71.956276
675.890420	35.129653	71.961281
674.774186	37.997723	71.966286
673.929759	34.442057	71.971290
673.319095	33.747659	71.976295
672.872830	38.731019	71.981300
672.678306	36.063794	71.986305
671.482934	36.766658	71.991310
671.161998	26.663607	71.996314
670.621199	32.944100	72.001319
669.994861	30.605834	72.006324
669.062001	25.958791	72.011329
668.301667	33.266159	72.016334
668.226074	24.585905	72.021338
666.824028	28.571830	72.026343
666.283854	30.832507	72.031348
665.798006	25.163372	72.036353
665.135459	36.812363	72.041358
664.051884	29.997318	72.046362
663.318083	30.615652	72.051367
662.836591	27.658227	72.056372
662.493122	18.877125	72.061377
661.928262	29.435058	72.066382
661.125136	27.260564	72.071386
660.452223	30.477525	72.076391
659.849443	31.563861	72.081396
659.312190	30.059827	72.086401
658.145846	32.819185	72.091406
657.367959	19.089312	72.096410
656.804691	24.786746	72.101415
656.570295	32.983367	72.106420
656.319945	31.266491	72.111425
654.761884	30.727683	72.116430
654.216275	27.659041	72.121434
653.536378	30.971735	72.126439
653.336059	32.788785	72.131444
653.219664	27.683731	72.136449
651.827404	30.709303	72.141454
651.174798	28.635426	72.146458
650.748250	30.501115	72.151463
649.683256	29.792334	72.156468
648.990883	28.491201	72.161473
648.024277	36.764992	72.166478
647.923380	26.776722	72.171482
647.191434	22.234895	72.176487
646.494667	26.991633	72.181492
645.913810	22.840492	72.186497
645.133121	32.052941	72.191502
644.857108	21.531156	72.196506
643.947222	23.853861	72.201511
643.250854	24.311696	72.206516
642.702999	25.955424	72.211521
642.386559	30.213203	72.216526
641.395397	20.607978	72.221530
640.556666	25.464595	72.226535
639.862955	25.019977	72.231540
639.797433	19.077336	72.236545
638.203767	25.052393	72.241550
638.170440	27.962506	72.246554
637.550974	32.167612	72.251559
636.479005	23.589252	72.256564
635.653784	19.795577	72.261569
634.659056	31.158414	72.266574
634.372125	19.239591	72.271578
633.737563	22.795808	72.276583
633.436837	26.825577	72.281588
633.276478	24.531393	72.286593
632.120388	36.255825	72.291598
631.420086	24.174163	72.296602
631.215185	26.165411	72.301607
629.923918	28.943096	72.306612
629.095877	20.187125	72.311617
628.349630	25.071596	72.316622
628.246926	28.379117	72.321626
627.130377	26.730791	72.326631
626.104493	29.623917	72.331636
625.831090	23.881538	72.336641
625.221342	28.316914	72.341646
624.803662	19.345785	72.346650
624.555395	26.333494	72.351655
623.811642	33.053173	72.356660
623.025915	19.105364	72.361665
622.331922	25.418141	72.366670
621.258785	21.268129	72.371674
620.727298	27.365792	72.376679
620.058098	30.210005	72.381684
619.903792	29.302598	72.386689
618.677236	30.235960	72.391694
617.798432	29.098567	72.396698
617.114235	34.859424	72.401703
616.658364	31.125209	72.406708
616.609561	25.891122	72.411713
615.274297	36.677407	72.416718
614.640350	30.139297	72.421722
614.157209	25.602014	72.426727
613.802946	26.547859	72.431732
613.226379	35.932818	72.436737
611.773555	29.099330	72.441742
611.549652	23.371149	72.446746
610.745269	35.936880	72.451751
610.604531	33.694766	72.456756
609.598492	29.010515	72.461761
608.423270	34.086312	72.466766
608.168368	23.289931	72.471770
608.184423	22.019499	72.476775
606.564843	30.635408	72.481780
605.976612	30.479935	72.486785
605.663646	42.612595	72.491790
605.125832	24.928870	72.496794
604.031452	33.962623	72.501799
603.241591	33.886570	72.506804
602.774831	29.991664	72.511809
602.272626	32.719400	72.516814
602.037788	26.854186	72.521818
601.178231	29.550520	72.526823
600.022908	38.658638	72.531828
599.714894	23.483564	72.536833
599.009206	29.727247	72.541838
598.514616	30.230233	72.546842
597.674069	42.566761	72.551847
597.012878	43.359635	72.556852
596.849738	30.474911	72.561857
594.942503	42.714805	72.566862
594.518158	31.592163	72.571866
593.982887	29.949054	72.576871
593.608328	24.552378	72.581876
593.423958	20.920015	72.586881
592.653821	31.318257	72.591886
591.885066	31.574743	72.596890
591.203408	29.967564	72.601895
590.665605	29.701560	72.606900
589.696224	26.068055	72.611905
588.498109	32.014843	72.616910
588.028022	25.184140	72.621914
587.500348	31.271740	72.626919
587.216918	42.078189	72.631924
587.168348	28.456121	72.636929
585.986184	33.807426	72.641934
585.350573	31.235690	72.646938
584.557989	27.394256	72.651943
583.229339	28.626173	72.656948
582.627339	32.757545	72.661953
582.208594	39.225200	72.666958
581.856016	29.688612	72.671962
581.632013	27.281563	72.676967
580.531078	27.326023	72.681972
579.711865	26.705864	72.686977
578.987385	44.852420	72.691982
578.872249	32.362182	72.696986
578.107570	29.658037	72.701991
576.944751	41.123363	72.706996
576.795063	22.143066	72.712001
575.887782	32.966861	72.717006
575.217206	28.314356	72.722010
574.271623	26.574171	72.727015
573.523772	31.239713	72.732020
573.464126	18.922003	72.737025
572.669663	34.135479	72.742030
571.645875	31.368521	72.747034
570.944417	36.375189	72.752039
570.521449	32.571088	72.757044
570.381870	33.591558	72.762049
569.487987	37.185939	72.767054
568.739179	20.423678	72.772058
567.949048	32.831023	72.777063
567.379543	28.706481	72.782068
566.384409	29.658204	72.787073
565.377348	38.160817	72.792078
565.596700	28.637225	72.797082
564.876558	34.747600	72.802087
563.961963	33.234298	72.807092
563.184119	35.118103	72.812097
562.453025	44.213867	72.817102
562.198366	30.085298	72.822106
561.613585	28.085801	72.827111
560.418281	24.567141	72.832116
559.871712	29.094971	72.837121
559.021310	37.519017	72.842126
559.047750	21.125304	72.847130
557.818113	28.784988	72.852135
556.918062	28.223445	72.857140
556.786233	14.423841	72.862145
556.370021	28.939972	72.867150
556.005923	36.340380	72.872154
554.837269	24.722856	72.877159
553.761955	28.385561	72.882164
553.409634	27.241611	72.887169
552.690350	39.579332	72.892174
551.884472	36.347161	72.897178
551.713321	25.157401	72.902183
551.005890	31.935967	72.907188
550.821945	27.746867	72.912193
549.307508	34.758049	72.917198
548.782236	25.042393	72.922202
548.319080	34.548071	72.927207
547.148476	38.989214	72.932212
546.562110	24.006726	72.937217
545.938945	46.204170	72.942222
545.629991	23.352536	72.947226
545.235593	34.592974	72.952231
543.799924	36.297704	72.957236
543.592668	29.668002	72.962241
542.965394	32.101850	72.967246
542.489132	29.910029	72.972250
541.315597	30.197885	72.977255
540.571466	31.975400	72.982260
540.093510	31.124279	72.987265
539.576816	36.333341	72.992270
538.986384	26.941884	72.997274
537.947767	27.826427	73.002279
536.959969	27.272558	73.007284
536.431878	26.237033	73.012289
536.236623	32.402583	73.017294
536.096034	35.624675	73.022298
535.140047	24.047409	73.027303
534.165102	30.058022	73.032308
533.648518	35.134600	73.037313
533.193655	35.866241	73.042318
532.331551	28.210153	73.047322
531.556779	33.140196	73.052327
531.072261	32.372124	73.057332
530.725084	26.619434	73.062337
529.684201	34.127640	73.067342
529.017905	23.953477	73.072346
528.215398	31.923615	73.077351
527.524498	29.316547	73.082356
526.570109	29.649929	73.087361
525.655637	31.434080	73.092366
525.199825	27.452292	73.097370
525.052850	37.270315	73.102375
524.250654	31.801416	73.107380
524.330988	21.051008	73.112385
523.080244	44.441255	73.117390
522.207447	40.081175	73.122394
521.762513	32.018015	73.127399
521.300658	35.352782	73.132404
520.365865	27.113758	73.137409
519.346719	22.239248	73.142414
519.118515	28.211346	73.147418
518.738307	23.637190	73.152423
517.686569	34.726864	73.157428
516.889384	32.256578	73.162433
516.400185	39.897693	73.167438
516.152752	23.003553	73.172442
515.278498	20.917712	73.177447
514.372481	36.628368	73.182452
513.938229	22.324996	73.187457
513.046625	32.927109	73.192462
511.893676	22.218604	73.197466
511.272076	24.321966	73.202471
510.911932	32.101796	73.207476
510.756689	21.655422	73.212481
510.207939	35.975049	73.217486
509.474650	21.578962	73.222490
508.611663	24.156020	73.227495
507.887222	30.418479	73.232500
507.398760	22.133601	73.237505
506.176992	30.329802	73.242510
505.672916	32.089589	73.247514
505.138071	33.420609	73.252519
504.830842	37.199110	73.257524
503.901786	31.583267	73.262529
502.916868	26.417878	73.267534
502.592113	32.613518	73.272538
502.416785	38.375346	73.277543
501.093117	30.783332	73.282548
500.290312	26.449963	73.287553
499.494790	25.947484	73.292558
499.523682	25.020366	73.297562
499.049136	20.458089	73.302567
497.893402	29.004901	73.307572
497.410722	26.251132	73.312577
496.431481	32.366523	73.317582
496.103858	34.881961	73.322586
494.994981	26.948228	73.327591
493.965906	30.594129	73.332596
493.843177	31.581956	73.337601
493.390486	42.222975	73.342606
492.788572	33.197641	73.347610
492.248964	19.535544	73.352615
491.149162	31.326748	73.357620
491.055021	24.907700	73.362625
490.012029	32.971350	73.367630
489.322272	23.971055	73.372634
488.615583	26.393910	73.377639
488.231065	28.480013	73.382644
487.773340	23.251152	73.387649
486.630170	33.951693	73.392654
486.006155	26.888490	73.397658
485.457172	24.996853	73.402663
484.159459	27.230003	73.407668
483.549061	33.597306	73.412673
482.900777	28.043981	73.417678
482.806541	24.253766	73.422682
482.380716	33.239407	73.427687
481.743829	37.661791	73.432692
480.867654	22.105746	73.437697
480.107674	27.965435	73.442702
479.463022	33.026152	73.447706
478.912211	32.705474	73.452711
477.815518	31.281140	73.457716
477.067848	34.607826	73.462721
476.669219	35.838304	73.467726
476.198229	22.914343	73.472730
475.945601	33.193899	73.477735
474.608176	35.073831	73.482740
474.563866	26.828593	73.487745
473.637181	36.499583	73.492750
472.328767	34.689503	73.497754
471.925972	30.494273	73.502759
471.084967	26.118115	73.507764
470.773034	34.043234	73.512769
470.715624	27.080587	73.517774
469.864364	22.160430	73.522778
469.019381	26.306877	73.527783
468.386408	29.224203	73.532788
467.397951	21.763320	73.537793
466.517403	29.066228	73.542798
465.806013	28.268079	73.547802
465.610458	17.708288	73.552807
464.978624	35.015325	73.557812
464.334714	18.636958	73.562817
462.873177	27.394927	73.567822
462.642122	29.161691	73.572826
462.178708	22.162800	73.577831
461.837489	29.310403	73.582836
461.627295	27.323798	73.587841
460.543536	27.554812	73.592846
459.880746	23.102958	73.597850
459.289102	34.638177	73.602855
458.126126	32.383883	73.607860
457.834917	23.805815	73.612865
457.164474	29.113498	73.617870
455.892280	34.551742	73.622874
455.191528	26.382699	73.627879
454.386026	27.163905	73.632884
454.351939	29.432307	73.637889
454.033589	29.809472	73.642894
453.437621	22.560461	73.647898
452.266651	32.492725	73.652903
451.732966	26.192591	73.657908
451.545362	24.658135	73.662913
450.169070	35.042587	73.667918
449.117987	37.886178	73.672922
448.813650	36.851295	73.677927
448.405121	34.022643	73.682932
448.313965	30.553642	73.687937
447.020532	27.452802	73.692942
445.940585	33.842877	73.697946
445.976577	33.898659	73.702951
445.529462	31.375781	73.707956
444.682433	29.566330	73.712961
443.471413	30.364835	73.717966
443.090103	32.731134	73.722970
442.516797	24.016661	73.727975
441.152029	28.215963	73.732980
440.989453	21.579163	73.737985
440.081329	33.172688	73.742990
439.701556	36.317769	73.747994
439.361789	25.880302	73.752999
438.641223	44.147673	73.758004
437.961393	31.023596	73.763009
437.083091	41.396530	73.768014
436.820596	29.603167	73.773018
435.962161	32.162178	73.778023
434.631315	35.184389	73.783028
434.362747	29.507504	73.788033
433.855921	28.408688	73.793038
433.444277	33.460678	73.798042
432.726291	24.972687	73.803047
431.519112	43.625094	73.808052
431.141019	26.936296	73.813057
430.737716	28.025597	73.818062
429.575176	24.859758	73.823066
429.019627	22.120769	73.828071
428.533504	30.521501	73.833076
428.138809	22.292669	73.838081
427.351492	40.312047	73.843086
426.547899	30.404224	73.848090
426.159582	31.084279	73.853095
425.347526	37.103672	73.858100
424.880339	27.970165	73.863105
423.595127	26.979597	73.868110
422.965837	32.059955	73.873114
422.515120	25.828614	73.878119
421.828195	35.950280	73.883124
421.721240	32.934813	73.888129
420.345988	29.820214	73.893134
420.040283	26.006925	73.898138
419.488438	28.851412	73.903143
418.798675	24.735033	73.908148
418.082639	18.359885	73.913153
417.432543	30.872679	73.918158
416.711162	26.417558	73.923162
416.213322	22.321065	73.928167
415.203293	35.744353	73.933172
415.017277	23.836312	73.938177
414.307102	32.121353	73.943182
413.001732	37.695792	73.948186
412.282355	26.528750	73.953191
411.439443	29.928975	73.958196
411.550114	29.422494	73.963201
411.388674	35.349267	73.968206
410.349058	33.023302	73.973210
409.507466	32.586541	73.978215
408.850396	27.268032	73.983220
408.093871	31.588064	73.988225
407.130386	30.259234	73.993230
406.268699	29.984950	73.998234
406.012370	25.646549	74.003239
405.649611	32.231456	74.008244
405.463173	24.696432	74.013249
404.020785	30.135006	74.018254
403.161516	31.795285	74.023258
402.996816	29.064991	74.028263
402.038786	26.331788	74.033268
401.417519	23.735742	74.038273
400.188179	32.456748	74.043278
399.812660	25.612604	74.048282
399.837363	31.620105	74.053287
399.254367	40.957233	74.058292
398.464921	27.808064	74.063297
397.392611	31.244845	74.068302
397.116654	31.309329	74.073306
396.530999	26.752162	74.078311
395.599512	32.740127	74.083316
394.815848	24.470776	74.088321
394.120135	32.652591	74.093326
393.824989	31.488516	74.098330
392.680412	34.985701	74.103335
391.765173	27.528955	74.108340
391.709729	29.393901	74.113345
391.101751	41.376441	74.118350
390.047459	31.210531	74.123354
388.935227	25.955091	74.128359
388.312202	35.391636	74.133364
388.480636	24.040566	74.138369
388.097402	31.409337	74.143374
387.132399	25.171640	74.148378
386.281878	23.015832	74.153383
385.411639	31.567660	74.158388
385.202311	35.251723	74.163393
384.426125	36.774189	74.168398
383.409904	28.385775	74.173402
383.197853	20.116816	74.178407
382.345178	23.118053	74.183412
382.107176	22.626128	74.188417
380.901514	29.135605	74.193422
380.243384	23.158101	74.198426
379.765585	24.155200	74.203431
378.932389	34.787464	74.208436
378.239484	19.041423	74.213441
377.309815	26.173983	74.218446
376.976964	24.052389	74.223450
376.614288	20.732317	74.228455
375.827926	22.902965	74.233460
374.889057	26.681195	74.238465
374.253182	31.562336	74.243470
373.638775	25.566828	74.248474
373.635260	22.366148	74.253479
372.439655	29.213075	74.258484
371.639344	11.115547	74.263489
371.405219	26.424264	74.268494
370.757415	27.755963	74.273498
370.084094	25.696507	74.278503
369.170384	26.670026	74.283508
368.388725	18.685802	74.288513
367.550449	25.368557	74.293518
366.516382	27.510869	74.298522
366.393341	15.537616	74.303527
365.555710	36.103938	74.308532
365.377039	13.793029	74.313537
364.685440	23.387156	74.318542
363.609235	24.470150	74.323546
363.129634	22.100703	74.328551
362.489071	31.693011	74.333556
362.361983	7.921500	74.338561
361.021872	29.775842	74.343566
360.388329	26.891601	74.348570
360.300365	18.676991	74.353575
358.940097	33.378254	74.358580
358.090349	18.567130	74.363585
357.639592	35.605620	74.368590
357.018876	25.678150	74.373594
356.798253	24.894872	74.378599
356.415156	29.097062	74.383604
355.575499	16.955725	74.388609
355.067699	30.144450	74.393614
353.851257	28.609943	74.398618
352.948246	27.760360	74.403623
352.224433	23.799241	74.408628
351.911582	26.097871	74.413633
351.696204	32.224051	74.418638
350.791656	27.539516	74.423642
349.876623	31.331304	74.428647
348.936780	33.144791	74.433652
348.751766	27.282717	74.438657
348.177673	36.443386	74.443662
347.097045	30.202053	74.448666
346.701805	26.251655	74.453671
345.780847	27.931244	74.458676
345.312598	21.442518	74.463681
345.056425	27.556274	74.468686
343.797866	31.226185	74.473690
343.455779	26.526140	74.478695
343.008023	29.812953	74.483700
342.222553	27.832878	74.488705
341.239128	24.029829	74.493710
340.605934	26.321161	74.498714
340.336634	23.273224	74.503719
339.380737	26.013378	74.508724
338.372882	30.811877	74.513729
337.915363	22.326572	74.518734
337.571267	26.877367	74.523738
337.052172	29.453296	74.528743
335.711317	30.548514	74.533748
335.091456	32.463981	74.538753
334.777253	26.977315	74.543758
334.034561	25.179663	74.548762
333.816616	21.633105	74.553767
332.617039	30.696328	74.558772
331.938125	29.976623	74.563777
331.617961	31.678749	74.568782
330.894220	25.926184	74.573786
330.097693	20.399690	74.578791
329.033130	25.897941	74.583796
328.545120	27.797127	74.588801
328.013291	26.842670	74.593806
327.515001	24.537710	74.598810
327.524817	26.491605	74.603815
326.319092	23.313777	74.608820
325.830602	17.299798	74.613825
325.157459	23.964132	74.618830
323.883030	36.499167	74.623834
323.735668	18.158826	74.628839
323.090037	35.706194	74.633844
322.373979	27.656335	74.638849
321.539592	34.436259	74.643854
320.917866	26.909115	74.648858
320.586670	21.869868	74.653863
319.101103	32.878925	74.658868
318.620051	20.581104	74.663873
318.278831	30.120981	74.668878
317.247076	29.326623	74.673882
317.541613	24.626053	74.678887
316.360473	31.937483	74.683892
315.452320	21.325702	74.688897
314.932400	23.423943	74.693902
314.230429	28.716180	74.698906
314.173445	27.397465	74.703911
312.898090	25.418200	74.708916
312.172393	18.451689	74.713921
311.588700	31.879597	74.718926
310.828342	25.509971	74.723930
309.949307	25.858236	74.728935
308.850210	23.332060	74.733940
309.065552	23.606841	74.738945
308.778072	29.036452	74.743950
308.316528	28.657431	74.748954
307.277090	29.726705	74.753959
306.227555	36.832662	74.758964
305.937596	29.952824	74.763969
305.149296	25.166203	74.768974
303.973635	25.574359	74.773978
303.887426	21.560527	74.778983
303.141887	31.749900	74.783988
302.418823	27.055385	74.788993
301.385452	28.273507	74.793998
300.759481	28.554635	74.799002
300.487608	29.526815	74.804007
299.666374	30.179689	74.809012
299.454810	26.939627	74.814017
298.398022	25.345011	74.819022
297.671330	26.186247	74.824026
297.505104	23.490900	74.829031
296.391217	30.545612	74.834036
295.438987	22.632755	74.839041
295.020889	25.727188	74.844046
294.811056	30.384325	74.849050
294.232786	25.816550	74.854055
292.865832	28.150718	74.859060
292.405997	20.318662	74.864065
291.871634	26.508296	74.869070
291.288527	21.252157	74.874074
290.492029	20.361968	74.879079
289.250110	27.397662	74.884084
289.338768	31.042120	74.889089
288.752067	25.685627	74.894094
288.059263	28.416985	74.899098
286.818811	27.083461	74.904103
286.455009	26.452320	74.909108
286.210181	18.013559	74.914113
285.485177	19.486895	74.919118
284.892359	37.639292	74.924122
284.097154	21.248845	74.929127
283.286297	27.343774	74.934132
282.259618	13.697889	74.939137
281.563121	21.457216	74.944142
280.597449	26.034543	74.949146
280.652115	24.926695	74.954151
279.991517	24.044812	74.959156
279.883482	22.838315	74.964161
278.861082	24.997726	74.969166
278.235704	27.010279	74.974170
278.028083	14.757207	74.979175
276.595172	30.124520	74.984180
276.081339	28.168983	74.989185
275.425419	22.087082	74.994190
274.339463	25.414120	74.999194
273.858134	22.433104	75.004199
273.229154	18.813294	75.009204
272.633799	25.436856	75.014209
272.058521	22.660050	75.019214
271.293606	26.003731	75.024218
270.359863	20.013422	75.029223
269.612175	27.553831	75.034228
269.661704	28.662446	75.039233
269.284211	29.067984	75.044238
267.872994	34.571049	75.049242
267.630284	24.829371	75.054247
266.923528	30.322658	75.059252
266.218376	24.120871	75.064257
265.486849	32.548119	75.069262
264.644179	33.863595	75.074266
264.384057	14.667604	75.079271
263.630895	23.752738	75.084276
262.289332	25.161924	75.089281
261.920166	28.431492	75.094286
261.161541	32.218880	75.099290
261.577567	20.011486	75.104295
259.957614	27.960588	75.109300
259.081331	22.164554	75.114305
258.760633	24.316209	75.119310
258.156045	33.284627	75.124314
257.967008	29.381805	75.129319
256.802331	31.070310	75.134324
255.983209	22.742013	75.139329
255.759093	26.266008	75.144334
254.630883	21.547778	75.149338
253.851771	22.450999	75.154343
253.016640	22.339696	75.159348
252.718226	23.500615	75.164353
252.481817	23.410576	75.169358
252.068774	21.517829	75.174362
251.198783	23.569378	75.179367
250.302244	21.361031	75.184372
249.665085	19.794170	75.189377
248.545257	20.992977	75.194382
247.608782	32.356097	75.199386
247.290517	19.740613	75.204391
246.957035	21.530026	75.209396
246.713069	17.456190	75.214401
246.026464	16.682542	75.219406
244.917714	20.913674	75.224410
244.485429	16.696388	75.229415
243.760015	32.103911	75.234420
243.001912	22.277233	75.239425
242.005855	22.637867	75.244430
241.346343	27.809811	75.249434
241.045233	16.412172	75.254439
240.673101	27.352596	75.259444
239.532591	22.924919	75.264449
238.911903	25.520213	75.269454
238.405362	26.326375	75.274458
238.024552	15.206373	75.279463
236.439510	21.352175	75.284468
235.694610	26.802662	75.289473
235.314987	31.814875	75.294478
234.976032	29.583887	75.299482
235.104328	26.253390	75.304487
234.236598	34.929439	75.309492
233.419437	21.366873	75.314497
232.809873	19.507032	75.319502
231.596841	27.440173	75.324506
230.752915	29.121717	75.329511
230.171674	25.763970	75.334516
229.691866	26.275710	75.339521
229.060408	27.958081	75.344526
228.198800	30.505048	75.349530
227.675764	19.294175	75.354535
226.978936	30.447209	75.359540
226.396622	23.796920	75.364545
226.313633	26.101501	75.369550
225.134639	32.592601	75.374554
224.693133	25.762169	75.379559
223.702423	29.961881	75.384564
223.332333	27.376309	75.389569
222.275435	31.170252	75.394574
221.446765	31.450595	75.399578
221.214095	25.777488	75.404583
220.996163	28.048385	75.409588
220.008137	23.897613	75.414593
218.960066	23.006549	75.419598
218.106232	30.552852	75.424602
217.848608	26.865975	75.429607
217.387394	33.868717	75.434612
216.719277	31.871554	75.439617
215.908063	27.993800	75.444622
215.065916	30.219121	75.449626
215.111610	24.132631	75.454631
213.663539	32.577916	75.459636
213.175853	32.759751	75.464641
212.711914	29.088416	75.469646
211.676168	31.849230	75.474650
211.046300	30.011553	75.479655
210.206122	28.062322	75.484660
209.358397	30.143452	75.489665
209.752857	26.899837	75.494670
208.869350	38.719735	75.499674
208.005376	25.896354	75.504679
207.032430	29.929235	75.509684
206.703370	28.256499	75.514689
206.353305	20.110498	75.519694
205.459425	26.677580	75.524698
204.718019	15.973042	75.529703
203.721283	22.728409	75.534708
203.482925	26.956429	75.539713
202.815465	17.891190	75.544718
201.781924	28.542810	75.549722
201.468026	21.214222	75.554727
200.463870	25.658938	75.559732
200.111386	26.144078	75.564737
199.075819	28.778711	75.569742
198.512725	33.340777	75.574746
198.403823	21.810001	75.579751
197.859170	29.321214	75.584756
196.654055	23.259079	75.589761
195.948637	21.105442	75.594766
195.260173	26.625790	75.599770
195.185579	22.416148	75.604775
193.932325	28.792940	75.609780
192.923656	27.805718	75.614785
192.765428	24.308006	75.619790
191.821049	23.518696	75.624794
192.008504	22.528452	75.629799
190.915454	22.169701	75.634804
190.310666	22.012236	75.639809
189.837899	14.540245	75.644814
188.567472	23.540697	75.649818
188.182832	27.087132	75.654823
187.604656	27.392208	75.659828
187.205420	28.351587	75.664833
186.002698	18.807129	75.669838
185.188337	29.859057	75.674842
184.988607	21.315352	75.679847
184.519938	24.957186	75.684852
183.482351	28.361707	75.689857
182.355959	19.333368	75.694862
181.655882	22.788162	75.699866
181.684861	8.660229	75.704871
180.812329	21.421396	75.709876
180.598112	23.718511	75.714881
179.899310	17.845333	75.719886
178.778315	22.918969	75.724890
178.134869	17.182047	75.729895
177.549527	19.762257	75.734900
176.432627	23.602052	75.739905
176.128126	28.066124	75.744910
175.623054	28.854718	75.749914
175.470755	17.639954	75.754919
173.830649	28.648483	75.759924
173.056937	25.159008	75.764929
173.099428	21.436909	75.769934
172.543689	32.310415	75.774938
172.382914	21.590591	75.779943
171.037561	27.020125	75.784948
170.615891	18.813008	75.789953
169.910520	15.560226	75.794958
168.596182	20.969044	75.799962
168.005142	14.954110	75.804967
167.417214	23.989266	75.809972
167.282593	29.233664	75.814977
166.509189	22.864598	75.819982
165.350531	33.296480	75.824986
164.852552	25.869511	75.829991
164.783168	24.907597	75.834996
163.846641	22.398150	75.840001
162.887924	25.113585	75.845006
162.083379	25.207173	75.850010
161.465127	22.177048	75.855015
161.276971	28.264197	75.860020
160.406546	25.677980	75.865025
159.655108	25.610136	75.870030
158.798009	27.550850	75.875034
158.537702	18.220440	75.880039
158.232742	25.909486	75.885044
157.243257	23.430562	75.890049
156.374422	16.005956	75.895054
155.456683	24.639530	75.900058
155.514780	20.728861	75.905063
154.317709	22.812088	75.910068
153.612367	25.818294	75.915073
153.159788	26.240550	75.920078
152.474420	28.631709	75.925082
152.311169	20.466974	75.930087
150.989097	23.033761	75.935092
150.188332	23.683421	75.940097
150.150424	17.033096	75.945102
149.109599	26.976256	75.950106
148.414345	23.384395	75.955111
147.900136	27.058726	75.960116
146.911538	24.584396	75.965121
146.771109	21.370860	75.970126
145.576152	22.837160	75.975130
145.076173	16.082309	75.980135
144.564599	21.959243	75.985140
144.101300	28.790435	75.990145
143.641059	22.346216	75.995150
142.410324	33.606468	76.000154
141.976095	24.806840	76.005159
141.332185	26.215247	76.010164
140.563888	32.092117	76.015169
139.572598	27.604429	76.020174
138.990537	20.526770	76.025178
138.955621	20.461387	76.030183
138.326809	32.357384	76.035188
136.860693	22.459129	76.040193
136.541452	19.751925	76.045198
135.585791	32.947417	76.050202
135.849695	29.614219	76.055207
134.980692	30.061873	76.060212
133.941736	25.003041	76.065217
133.569272	23.917561	76.070222
132.837146	25.685392	76.075226
131.751473	19.813987	76.080231
130.732093	36.992026	76.085236
130.282358	31.987482	76.090241
130.256545	26.776575	76.095246
129.531678	27.451987	76.100250
128.743963	18.398065	76.105255
127.977826	24.815490	76.110260
127.188625	26.671270	76.115265
127.210326	18.618979	76.120270
125.946052	24.122339	76.125274
125.501865	21.848224	76.130279
124.724422	25.667033	76.135284
124.177154	19.064808	76.140289
123.159584	23.708810	76.145294
122.374796	22.625997	76.150298
121.976674	19.718482	76.155303
121.414943	21.463878	76.160308
120.928842	23.452683	76.165313
120.547088	22.915895	76.170318
119.518037	35.118566	76.175322
119.091399	22.339043	76.180327
117.981931	32.933411	76.185332
117.024546	30.417846	76.190337
116.723836	23.164444	76.195342
115.990840	31.327025	76.200346
115.703317	22.615978	76.205351
115.152868	27.062500	76.210356
114.219348	30.396838	76.215361
113.546656	23.757841	76.220366
113.110741	32.470725	76.225370
112.179599	24.814792	76.230375
111.035339	25.244841	76.235380
110.487698	30.403707	76.240385
110.718036	18.591773	76.245390
109.523796	29.332124	76.250394
108.875068	20.989337	76.255399
108.054772	34.324103	76.260404
107.455548	34.940064	76.265409
107.404438	19.916566	76.270414
106.092428	27.655803	76.275418
105.349552	31.122174	76.280423
104.663879	30.638580	76.285428
104.399232	24.341380	76.290433
104.025074	24.713294	76.295438
102.585358	28.467398	76.300442
102.225920	27.529659	76.305447
101.866890	23.507305	76.310452
101.161003	24.048811	76.315457
100.535262	20.444305	76.320462
99.267266	25.792151	76.325466
99.414154	24.346318	76.330471
98.584110	32.784578	76.335476
97.795310	34.293371	76.340481
97.204830	32.838957	76.345486
96.105342	28.583009	76.350490
95.356107	24.484104	76.355495
94.650195	30.054566	76.360500
93.972022	28.166277	76.365505
93.766033	20.673848	76.370510
93.182839	24.255108	76.375514
93.015578	23.512233	76.380519
92.024089	29.732211	76.385524
91.225945	25.704184	76.390529
90.259175	22.884197	76.395534
89.076687	33.371946	76.400538
88.792777	26.683578	76.405543
88.477380	29.435231	76.410548
87.847566	29.622407	76.415553
87.470127	23.925098	76.420558
86.491050	26.211718	76.425562
85.540953	29.040926	76.430567
84.980631	37.521338	76.435572
84.577229	31.673623	76.440577
83.736508	29.270357	76.445582
82.820296	33.865099	76.450586
82.391326	26.031330	76.455591
82.193137	26.498190	76.460596
81.373976	29.716532	76.465601
80.515331	27.344511	76.470606
79.592485	33.383237	76.475610
79.513841	19.363934	76.480615
78.317595	29.857032	76.485620
77.310972	17.203129	76.490625
77.284889	17.357114	76.495630
76.492110	31.253627	76.500634
76.112076	28.302234	76.505639
75.100616	30.407940	76.510644
74.632586	26.250007	76.515649
73.956053	25.733425	76.520654
73.265045	36.043459	76.525658
72.246489	35.355911	76.530663
71.651700	31.960943	76.535668
71.358011	33.974270	76.540673
70.907764	25.109406	76.545678
70.022262	25.269551	76.550682
69.381657	20.954635	76.555687
68.719983	26.350889	76.560692
67.946250	25.042401	76.565697
66.701701	27.417095	76.570702
65.888215	27.116322	76.575706
65.645263	27.560360	76.580711
65.424301	23.074445	76.585716
64.923002	26.179023	76.590721
64.669572	21.520089	76.595726
63.428261	23.971539	76.600730
62.857462	26.249832	76.605735
62.134431	27.158361	76.610740
60.698782	26.661913	76.615745
60.391243	28.713719	76.620750
59.721155	32.114878	76.625754
59.330509	30.504025	76.630759
59.029240	32.934881	76.635764
58.193941	25.027144	76.640769
57.779243	20.371851	76.645774
56.937739	31.751414	76.650778
56.221542	22.353375	76.655783
55.513425	22.934673	76.660788
54.511231	29.746157	76.665793
54.259981	21.814669	76.670798
52.900477	27.014703	76.675802
52.570694	22.073054	76.680807
51.716143	31.054555	76.685812
51.260430	26.869432	76.690817
50.902893	18.324110	76.695822
50.505177	26.229805	76.700826
49.739852	24.681860	76.705831
49.014771	20.164378	76.710836
48.085476	25.193304	76.715841
47.052826	30.107825	76.720846
46.123997	22.109353	76.725850
45.916566	23.087051	76.730855
45.689270	27.013690	76.735860
45.152202	23.956459	76.740865
44.687177	12.936676	76.745870
43.486841	28.858356	76.750874
42.950888	19.188726	76.755879
42.407868	21.464169	76.760884
41.073440	27.104914	76.765889
40.501300	16.750346	76.770894
40.030317	24.655109	76.775898
39.905575	20.054505	76.780903
39.135192	23.793363	76.785908
37.770963	28.979966	76.790913
37.556747	25.448620	76.795918
36.767805	26.479634	76.800922
36.488621	22.670065	76.805927
35.425234	24.932303	76.810932
34.351022	26.332090	76.815937
33.909969	21.001333	76.820942
33.456483	32.044628	76.825946
33.114970	17.800750	76.830951
32.744685	23.708785	76.835956
31.530849	25.695395	76.840961
31.085698	13.015056	76.845966
30.532841	26.565799	76.850970
29.719662	19.961855	76.855975
28.803742	29.604435	76.860980
28.074115	28.445046	76.865985
27.997957	21.815023	76.870990
27.092527	16.815375	76.875994
25.852758	21.155802	76.880999
25.539261	23.719498	76.886004
25.288683	28.425719	76.891009
24.776143	16.707037	76.896014
23.315768	23.432328	76.901018
22.729902	20.417579	76.906023
22.498158	11.401194	76.911028
21.825088	23.307410	76.916033
21.082474	13.505169	76.921038
20.069233	16.467472	76.926042
19.617189	14.290828	76.931047
19.410217	24.503166	76.936052
18.476847	23.677475	76.941057
17.859050	17.256843	76.946062
17.057992	33.118009	76.951066
16.408358	20.659517	76.956071
15.549394	14.466586	76.961076
14.771322	21.429993	76.966081
14.435704	18.067827	76.971086
13.541323	22.375251	76.976090
13.584511	22.458264	76.981095
12.353039	21.818893	76.986100
11.573411	28.700551	76.991105
11.241831	19.233304	76.996110
10.866201	23.459571	77.001114
9.950310	19.680593	77.006119
9.126759	16.643832	77.011124
8.537259	22.930610	77.016129
8.422797	20.072494	77.021134
6.952937	27.865337	77.026139
6.501634	25.866774	77.031143
6.060803	16.639307	77.036148
5.006704	17.528115	77.041153
4.390707	15.875945	77.046158