Fri Mar 05 18:45:03 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.174860	99.792563	0.000000
0.114429	88.809116	0.005005
-0.699786	58.027217	0.010010
-2.762950	16.432657	0.015014
-7.207970	15.585172	0.020019
-12.195908	0.131740	0.025024
-17.102890	6.593058	0.030029
-21.774404	9.263659	0.035034
-25.299311	10.008829	0.040038
-29.395360	6.877473	0.045043
-33.031977	5.778082	0.050048
-36.964700	7.092949	0.055053
-40.516204	8.052120	0.060058
-43.735199	-1.435495	0.065062
-48.159898	12.139893	0.070067
-51.669692	21.861913	0.075072
-55.220149	7.029243	0.080077
-58.994767	10.190777	0.085082
-62.393023	6.687964	0.090086
-66.791656	6.355163	0.095091
-70.426523	7.841765	0.100096
-74.222973	15.146328	0.105101
-77.862852	9.739267	0.110106
-81.427686	11.582144	0.115110
-85.712596	14.926054	0.120115
-89.326741	6.748917	0.125120
-93.172681	17.127016	0.130125
-96.741335	10.584247	0.135130
-100.422583	7.161331	0.140134
-104.466966	11.805738	0.145139
-107.809848	5.029848	0.150144
-111.773222	6.814929	0.155149
-115.564653	3.360731	0.160154
-119.291138	7.648510	0.165158
-123.540330	14.165939	0.170163
-127.073277	7.738947	0.175168
-130.481868	11.427241	0.180173
-134.489159	-1.785403	0.185178
-137.976991	7.660406	0.190182
-141.606429	-3.540388	0.195187
-145.678080	-8.673438	0.200192
-149.335607	-4.101728	0.205197
-153.599699	-0.664831	0.210202
-157.109260	11.659268	0.215206
-161.070129	5.705890	0.220211
-164.936502	11.977797	0.225216
-168.405294	18.414930	0.230221
-172.198251	8.624841	0.235226
-175.833341	4.937633	0.240230
-179.690094	19.453949	0.245235
-183.192710	2.584311	0.250240
-187.165905	15.252097	0.255245
-191.018838	3.536684	0.260250
-194.245897	-1.776795	0.265254
-198.319793	13.709331	0.270259
-202.144489	7.732714	0.275264
-205.669758	15.000505	0.280269
-210.024113	12.610851	0.285274
-213.278168	9.492098	0.290278
-217.012234	7.232126	0.295283
-220.999438	10.634416	0.300288
-224.911071	16.696020	0.305293
-228.733014	12.633434	0.310298
-231.631552	3.467104	0.315302
-235.767929	7.000458	0.320307
-239.883038	14.209467	0.325312
-243.412221	11.683447	0.330317
-247.744654	16.118594	0.335322
-251.142255	10.291512	0.340326
-255.190334	22.532964	0.345331
-258.553995	14.811277	0.350336
-262.176163	9.895265	0.355341
-265.999748	12.407340	0.360346
-269.413817	12.543814	0.365350
-273.655868	10.566862	0.370355
-277.554377	7.705604	0.375360
-281.181582	18.591542	0.380365
-284.945662	15.469139	0.385370
-288.629414	15.107790	0.390374
-292.791339	9.577813	0.395379
-296.245037	5.576409	0.400384
-299.687245	13.837168	0.405389
-303.986033	16.839897	0.410394
-307.362057	16.191334	0.415398
-311.276485	11.880294	0.420403
-315.042684	10.802016	0.425408
-318.743533	5.619533	0.430413
-322.710140	8.280683	0.435418
-326.331670	3.823567	0.440422
-330.296185	6.120118	0.445427
-333.600725	13.832243	0.450432
-337.335630	9.361702	0.455437
-341.333514	17.195563	0.460442
-344.820023	15.616940	0.465446
-348.910974	11.026638	0.470451
-352.680750	9.609945	0.475456
-356.578828	10.850411	0.480461
-360.263320	20.778932	0.485466
-363.782122	2.461374	0.490470
-367.874704	17.222191	0.495475
-371.260830	-1.321535	0.500480
-375.144433	7.107564	0.505485
-378.987128	0.463911	0.510490
-382.984871	13.679961	0.515494
-386.523029	18.229812	0.520499
-390.216906	6.746391	0.525504
-393.857981	11.339491	0.530509
-397.678496	16.188331	0.535514
-401.413150	4.244662	0.540518
-405.640984	8.042062	0.545523
-409.106791	8.409346	0.550528
-412.803597	12.159818	0.555533
-416.722933	15.099003	0.560538
-420.174476	0.441955	0.565542
-424.223575	3.602144	0.570547
-428.023959	5.098362	0.575552
-431.705538	1.333820	0.580557
-435.462813	-1.917156	0.585562
-439.055302	4.715136	0.590566
-442.880578	15.069952	0.595571
-446.451755	8.157547	0.600576
-450.179154	4.529661	0.605581
-454.642166	11.777230	0.610586
-458.206224	0.706859	0.615590
-461.978472	8.996885	0.620595
-465.105614	9.795870	0.625600
-468.788460	9.522963	0.630605
-473.252712	9.772243	0.635610
-476.844729	3.730541	0.640614
-480.891089	0.462725	0.645619
-484.473785	7.650184	0.650624
-487.973241	8.070265	0.655629
-491.991581	13.250463	0.660634
-495.225146	8.026751	0.665638
-499.390636	7.938206	0.670643
-502.881023	8.735329	0.675648
-507.125619	8.456004	0.680653
-511.133022	7.780836	0.685658
-514.485726	16.685181	0.690662
-518.238336	18.549227	0.695667
-521.934099	15.529835	0.700672
-525.369091	13.159505	0.705677
-529.461574	9.555362	0.710682
-532.707075	11.530823	0.715686
-537.125923	17.525695	0.720691
-540.638112	13.565533	0.725696
-544.442826	9.519638	0.730701
-548.107610	8.587957	0.735706
-551.726366	4.400409	0.740710
-556.059569	13.026182	0.745715
-559.884955	4.132910	0.750720
-563.508812	11.852182	0.755725
-567.438650	8.028162	0.760730
-570.466405	5.737929	0.765734
-574.529925	15.650027	0.770739
-578.131963	14.255784	0.775744
-581.935133	2.153058	0.780749
-585.980428	8.320154	0.785754
-589.655367	4.887538	0.790758
-593.874671	11.063522	0.795763
-597.233902	7.271402	0.800768
-600.937435	8.350299	0.805773
-604.762504	12.015894	0.810778
-608.331380	13.205755	0.815782
-612.260407	11.419101	0.820787
-616.120347	5.806773	0.825792
-619.565237	7.443620	0.830797
-623.379669	10.549304	0.835802
-626.820628	13.885488	0.840806
-630.803336	13.255462	0.845811
-634.718762	9.071285	0.850816
-638.486762	7.552263	0.855821
-642.490918	15.409680	0.860826
-646.104960	3.127038	0.865830
-650.259979	16.532629	0.870835
-653.770991	10.481415	0.875840
-657.392775	4.266558	0.880845
-661.333485	7.690521	0.885850
-664.755981	9.110966	0.890854
-668.693570	13.051683	0.895859
-672.406995	12.552167	0.900864
-675.990598	10.628427	0.905869
-679.644047	10.377959	0.910874
-683.566414	10.340776	0.915878
-687.646279	7.389331	0.920883
-691.248815	5.339331	0.925888
-694.825820	7.702293	0.930893
-698.837542	12.462303	0.935898
-702.263612	6.066433	0.940902
-706.391040	14.722664	0.945907
-710.286879	5.156510	0.950912
-713.842337	8.787079	0.955917
-717.470537	13.597797	0.960922
-720.811882	-3.886494	0.965926
-724.814999	11.128656	0.970931
-728.815698	5.491704	0.975936
-732.569811	10.358834	0.980941
-736.508187	10.007331	0.985946
-740.282148	7.260982	0.990950
-743.923406	14.574867	0.995955
-747.971897	8.652272	1.000960
-751.510509	12.846329	1.005965
-755.219404	10.286724	1.010970
-758.711543	8.137183	1.015974
-762.527624	16.226510	1.020979
-766.253864	9.765168	1.025984
-769.817912	9.106314	1.030989
-774.043301	7.570725	1.035994
-777.599336	6.130013	1.040998
-781.692244	16.373569	1.046003
-785.322304	10.928211	1.051008
-788.711944	15.322439	1.056013
-792.760546	16.589250	1.061018
-796.627873	13.112017	1.066022
-800.361071	17.452364	1.071027
-804.379699	10.634120	1.076032
-807.811414	1.072804	1.081037
-811.843359	11.104813	1.086042
-815.012361	7.094948	1.091046
-818.941890	14.289441	1.096051
-822.714140	11.353718	1.101056
-826.419282	6.191664	1.106061
-830.502068	16.911497	1.111066
-834.269904	16.378355	1.116070
-838.347208	8.136106	1.121075
-841.530227	5.511502	1.126080
-845.189759	4.368134	1.131085
-849.355549	6.938986	1.136090
-852.751265	-2.661128	1.141094
-856.762837	11.704298	1.146099
-860.549006	7.020451	1.151104
-864.099508	14.272696	1.156109
-868.143927	13.995135	1.161114
-871.902413	7.083387	1.166118
-875.653725	11.521360	1.171123
-879.165340	13.166095	1.176128
-882.849372	0.522880	1.181133
-886.709204	9.370013	1.186138
-890.339276	-2.621072	1.191142
-894.361495	8.812993	1.196147
-898.149058	9.136237	1.201152
-901.879626	7.797735	1.206157
-905.517650	6.053360	1.211162
-909.110694	6.134212	1.216166
-913.430801	-0.569400	1.221171
-916.976371	6.308392	1.226176
-920.584603	2.938178	1.231181
-924.430649	6.076201	1.236186
-928.111642	9.161032	1.241190
-932.002103	15.023247	1.246195
-935.946813	1.609674	1.251200
-939.702658	2.260648	1.256205
-943.382987	6.223754	1.261210
-946.848887	-1.050036	1.266214
-950.716531	13.956417	1.271219
-954.296469	3.433439	1.276224
-958.136597	-0.872609	1.281229
-962.224673	-4.006756	1.286234
-965.393609	3.596198	1.291238
-969.457638	-2.566361	1.296243
-973.380672	0.667627	1.301248
-976.936333	4.514655	1.306253
-980.921708	3.384183	1.311258
-984.460609	-0.706640	1.316262
-988.176024	5.712715	1.321267
-992.150265	-0.743281	1.326272
-995.802206	0.424174	1.331277
-1000.038426	10.572729	1.336282
-1003.421795	-1.925971	1.341286
-1007.407522	9.735826	1.346291
-1011.132560	-4.982173	1.351296
-1014.935701	5.784692	1.356301
-1018.514665	12.407777	1.361306
-1021.933800	0.988722	1.366310
-1025.992341	2.681718	1.371315
-1029.693057	-1.562926	1.376320
-1033.313361	1.012468	1.381325
-1037.329327	8.497095	1.386330
-1040.864890	4.148783	1.391334
-1044.884493	11.381695	1.396339
-1048.423431	1.451555	1.401344
-1052.365401	-5.801119	1.406349
-1056.508452	11.605489	1.411354
-1059.730843	5.832021	1.416358
-1063.895886	3.087254	1.421363
-1067.509725	4.668193	1.426368
-1070.966312	-3.078398	1.431373
-1074.574130	4.363083	1.436378
-1078.262582	5.680008	1.441382
-1082.478811	5.558032	1.446387
-1086.234831	5.617916	1.451392
-1089.690627	6.000364	1.456397
-1094.005770	0.971017	1.461402
-1097.400474	-5.269988	1.466406
-1101.211805	2.200931	1.471411
-1104.996341	7.160234	1.476416
-1108.831084	16.200820	1.481421
-1112.678216	5.049066	1.486426
-1115.939474	-0.841101	1.491430
-1119.720275	4.011972	1.496435
-1123.519019	0.754557	1.501440
-1127.798047	-4.682620	1.506445
-1131.586450	3.658304	1.511450
-1135.035484	2.987918	1.516454
-1138.791334	-2.209663	1.521459
-1142.619679	6.005206	1.526464
-1145.821419	-13.098160	1.531469
-1150.044684	0.811150	1.536474
-1153.785993	8.483838	1.541478
-1157.874021	12.275958	1.546483
-1161.465435	3.459833	1.551488
-1165.314920	-1.722723	1.556493
-1169.216744	6.560713	1.561498
-1172.756904	1.251410	1.566502
-1176.633808	3.901193	1.571507
-1180.081157	3.743110	1.576512
-1183.536710	1.489013	1.581517
-1187.661477	3.719582	1.586522
-1191.203986	-4.588654	1.591526
-1195.340860	2.917152	1.596531
-1199.090299	1.694112	1.601536
-1202.851915	-0.465252	1.606541
-1206.958193	7.694842	1.611546
-1210.199980	2.840899	1.616550
-1213.764970	0.216433	1.621555
-1217.581805	1.726005	1.626560
-1221.375273	-3.889614	1.631565
-1225.378160	6.149447	1.636570
-1228.924580	0.470654	1.641574
-1232.933596	6.713438	1.646579
-1236.540372	9.719061	1.651584
-1240.587246	0.378290	1.656589
-1244.321975	9.429885	1.661594
-1247.633532	-7.998388	1.666598
-1251.709509	4.081930	1.671603
-1255.716474	3.417429	1.676608
-1258.826204	9.254575	1.681613
-1263.063657	14.892154	1.686618
-1266.529358	-1.557379	1.691622
-1270.473016	-2.156291	1.696627
-1274.094486	6.402564	1.701632
-1277.844636	-3.663706	1.706637
-1281.883712	7.710598	1.711642
-1285.715760	1.166135	1.716646
-1289.239874	0.881730	1.721651
-1293.364471	9.262519	1.726656
-1296.623859	2.661116	1.731661
-1300.512328	13.891503	1.736666
-1304.202730	6.069156	1.741670
-1307.975348	8.193114	1.746675
-1311.908287	4.292024	1.751680
-1315.417144	-9.460254	1.756685
-1319.053839	-0.315433	1.761690
-1323.148910	-3.458852	1.766694
-1326.727092	7.715600	1.771699
-1330.633516	10.917559	1.776704
-1334.288605	2.197066	1.781709
-1338.539293	7.283390	1.786714
-1341.664280	-3.422148	1.791718
-1345.298358	6.558074	1.796723
-1349.598559	5.434477	1.801728
-1353.401554	0.697383	1.806733
-1357.337432	5.827965	1.811738
-1360.779304	3.570370	1.816742
-1364.351144	12.845231	1.821747
-1368.217742	1.402165	1.826752
-1371.700428	8.950209	1.831757
-1375.890387	-0.406829	1.836762
-1379.305380	1.311492	1.841766
-1383.217139	6.509217	1.846771
-1387.224639	1.964189	1.851776
-1390.979941	6.001486	1.856781
-1394.720623	3.921087	1.861786
-1398.251268	-1.401995	1.866790
-1401.820305	-2.095348	1.871795
-1405.574449	6.945406	1.876800
-1409.419177	2.103126	1.881805
-1413.424245	3.674693	1.886810
-1417.339243	6.837168	1.891814
-1421.160015	1.622070	1.896819
-1424.620758	2.529351	1.901824
-1427.995935	2.033657	1.906829
-1432.058090	-0.502984	1.911834
-1435.934852	4.156220	1.916838
-1439.694665	3.802549	1.921843
-1443.772266	-1.596890	1.926848
-1447.210695	9.132740	1.931853
-1451.248467	4.742481	1.936858
-1454.783817	5.286442	1.941862
-1458.566112	5.696486	1.946867
-1462.251533	13.174621	1.951872
-1465.939116	2.138302	1.956877
-1469.872873	6.921805	1.961882
-1473.313048	4.299837	1.966886
-1477.169371	3.081752	1.971891
-1481.435270	3.124573	1.976896
-1485.014511	0.725163	1.981901
-1488.476459	13.429788	1.986906
-1492.251227	5.186034	1.991910
-1495.980971	2.055390	1.996915
-1500.409466	6.933673	2.006912
-1500.984056	3.065631	2.016909
-1498.155724	3.781111	2.026906
-1495.357487	8.680906	2.036902
-1493.618458	4.488170	2.046899
-1491.902059	-2.006213	2.056896
-1490.076357	1.737208	2.066893
-1487.847234	7.201831	2.076890
-1485.702508	-2.255359	2.086886
-1483.852860	0.753177	2.096883
-1481.855357	3.226459	2.106880
-1480.375410	-0.087935	2.116877
-1478.210847	4.548609	2.126874
-1476.365993	7.660553	2.136870
-1474.521757	0.760446	2.146867
-1472.638866	-1.168984	2.156864
-1470.878427	-0.691427	2.166861
-1468.952138	-1.130954	2.176858
-1466.845278	2.087466	2.186854
-1464.848704	1.493003	2.196851
-1463.145727	0.051864	2.206848
-1461.350272	1.408037	2.216845
-1459.619984	6.286241	2.226842
-1457.330678	3.205428	2.236838
-1455.482013	-3.876952	2.246835
-1453.780683	2.251687	2.256832
-1452.221664	-0.680612	2.266829
-1450.266885	1.335326	2.276826
-1448.011864	-3.281047	2.286822
-1445.986190	-5.988056	2.296819
-1444.070288	-7.212219	2.306816
-1442.557254	-1.359742	2.316813
-1440.840987	6.831791	2.326810
-1438.541583	1.181999	2.336806
-1436.671836	-2.003725	2.346803
-1434.758907	-0.952131	2.356800
-1432.921420	2.072606	2.366797
-1431.391892	2.680323	2.376794
-1429.393732	-1.909119	2.386790
-1427.488864	-1.914128	2.396787
-1425.363782	-0.822281	2.406784
-1423.456953	1.180831	2.416781
-1421.991780	-0.700629	2.426778
-1419.843391	1.866973	2.436774
-1417.983287	3.935992	2.446771
-1415.980916	7.946457	2.456768
-1414.028396	0.798530	2.466765
-1412.506466	2.271164	2.476762
-1410.487216	2.830492	2.486758
-1408.700725	-3.086105	2.496755
-1406.960850	3.023770	2.506752
-1404.604229	-0.418297	2.516749
-1402.980894	-3.359281	2.526746
-1400.964400	-6.945839	2.536742
-1399.141065	-0.061422	2.546739
-1397.223257	-10.426421	2.556736
-1395.587378	-2.905675	2.566733
-1393.400472	3.075804	2.576730
-1391.512332	2.358237	2.586726
-1389.634885	2.000805	2.596723
-1388.006419	-2.314682	2.606720
-1386.044167	-4.004114	2.616717
-1384.417519	-1.828222	2.626714
-1382.497678	0.948109	2.636710
-1380.191219	-5.230127	2.646707
-1378.276162	-3.660929	2.656704
-1376.788405	0.138264	2.666701
-1374.794820	0.120676	2.676698
-1372.836917	-2.002262	2.686694
-1371.089401	0.612190	2.696691
-1368.961905	1.927915	2.706688
-1367.090632	0.431484	2.716685
-1365.587960	-2.280159	2.726682
-1363.470802	-3.492261	2.736678
-1361.693491	-5.494702	2.746675
-1359.726898	-7.031648	2.756672
-1357.748895	-3.811447	2.766669
-1356.056885	-1.117046	2.776666
-1354.160138	-1.807540	2.786662
-1352.114550	-1.852380	2.796659
-1350.361687	-2.017731	2.806656
-1348.471540	6.198151	2.816653
-1346.439343	-7.643039	2.826650
-1344.816775	0.263566	2.836646
-1342.940695	-4.307843	2.846643
-1340.948112	1.668478	2.856640
-1339.230641	2.798808	2.866637
-1337.359826	-2.228074	2.876634
-1335.326862	2.597045	2.886630
-1333.393879	-1.184513	2.896627
-1331.547314	0.100424	2.906624
-1329.719668	-2.915845	2.916621
-1327.855675	-4.728450	2.926618
-1326.146620	-2.802549	2.936614
-1323.687856	-2.240860	2.946611
-1322.415154	-7.832000	2.956608
-1320.392521	-1.661523	2.966605
-1318.363201	-6.797443	2.976602
-1316.338905	-5.493572	2.986598
-1314.618485	-3.435270	2.996595
-1312.823692	-2.765720	3.006592
-1311.109354	2.467263	3.016589
-1309.219147	-0.746900	3.026586
-1307.263173	2.811612	3.036582
-1305.187882	-8.075900	3.046579
-1303.340803	0.388494	3.056576
-1301.441920	0.101914	3.066573
-1299.753953	0.280147	3.076570
-1297.848691	3.860996	3.086566
-1295.945739	-1.245209	3.096563
-1293.880777	-1.094150	3.106560
-1292.065451	-1.743141	3.116557
-1290.388242	1.473157	3.126554
-1288.450793	4.189908	3.136550
-1286.518467	3.708514	3.146547
-1284.643640	1.117361	3.156544
-1282.405431	-1.683524	3.166541
-1281.037198	2.698551	3.176538
-1279.078954	-3.861235	3.186534
-1276.979730	5.942841	3.196531
-1275.293339	-6.897161	3.206528
-1273.486263	-1.980572	3.216525
-1271.631741	4.469491	3.226522
-1269.366348	-4.927882	3.236518
-1267.761856	-4.826267	3.246515
-1265.841862	0.399103	3.256512
-1263.894087	-4.622670	3.266509
-1262.487902	-1.175084	3.276506
-1260.558021	1.422902	3.286502
-1258.490780	2.661531	3.296499
-1256.163550	1.452224	3.306496
-1254.513757	2.890293	3.316493
-1252.926378	5.963099	3.326490
-1250.859400	2.895957	3.336486
-1248.904934	-4.577418	3.346483
-1247.085568	1.859343	3.356480
-1245.254161	-5.014859	3.366477
-1243.566120	3.523988	3.376474
-1241.302845	4.208627	3.386470
-1239.378040	1.527406	3.396467
-1237.819717	2.422752	3.406464
-1236.233838	0.743144	3.416461
-1234.189681	4.524455	3.426458
-1232.175810	8.976935	3.436454
-1229.843229	10.176290	3.446451
-1228.088180	5.588016	3.456448
-1226.340572	2.523052	3.466445
-1224.851509	4.601076	3.476442
-1222.739465	6.129413	3.486438
-1220.668749	-3.083608	3.496435
-1219.078468	-1.320200	3.506432
-1217.039404	2.030885	3.516429
-1215.002518	2.612826	3.526426
-1213.475757	2.837444	3.536422
-1211.851388	2.032753	3.546419
-1209.428602	4.171385	3.556416
-1207.749781	2.928507	3.566413
-1205.953434	1.084190	3.576410
-1203.939135	-3.000805	3.586406
-1201.970532	2.235792	3.596403
-1200.142255	-3.810503	3.606400
-1198.184887	-2.265290	3.616397
-1196.433192	0.111786	3.626394
-1194.218159	-1.938462	3.636390
-1192.712573	5.045924	3.646387
-1190.707211	-1.091857	3.656384
-1189.079693	-1.331768	3.666381
-1187.112133	7.058192	3.676378
-1185.248355	7.514699	3.686374
-1183.138055	2.890145	3.696371
-1181.479971	2.992719	3.706368
-1179.716758	4.177430	3.716365
-1177.837411	8.135164	3.726362
-1175.684410	11.212268	3.736358
-1173.621947	4.642201	3.746355
-1172.162147	5.480722	3.756352
-1170.373634	6.471918	3.766349
-1168.268833	5.655129	3.776346
-1166.262957	2.992575	3.786342
-1164.495365	10.102436	3.796339
-1162.778330	5.714502	3.806336
-1161.068536	4.989338	3.816333
-1158.885149	6.523689	3.826330
-1157.102150	11.256335	3.836326
-1154.985668	4.088689	3.846323
-1153.210364	4.647797	3.856320
-1151.318253	-0.347615	3.866317
-1149.748714	-2.572450	3.876314
-1147.536069	3.894638	3.886310
-1145.632791	-1.977299	3.896307
-1143.899008	1.699010	3.906304
-1141.900765	3.836158	3.916301
-1140.334857	2.390337	3.926298
-1138.249802	0.408304	3.936294
-1136.455101	-4.806777	3.946291
-1134.564983	-5.183398	3.956288
-1132.604281	-8.389752	3.966285
-1130.664024	-5.060678	3.976282
-1128.728307	-3.379310	3.986278
-1126.988481	-1.164493	3.996275
-1124.863771	-2.901804	4.006272
-1123.599554	2.469652	4.016269
-1121.452477	2.438781	4.026266
-1119.396406	-0.468607	4.036262
-1117.640169	-2.109072	4.046259
-1115.675557	0.174007	4.056256
-1113.783580	-1.328694	4.066253
-1112.090128	-0.792777	4.076250
-1110.302337	2.568601	4.086246
-1108.205394	-0.763740	4.096243
-1106.189671	-0.999377	4.106240
-1104.382082	0.656719	4.116237
-1102.926778	2.157587	4.126234
-1100.696489	0.267619	4.136230
-1098.785558	3.449834	4.146227
-1096.978174	4.349646	4.156224
-1095.083850	-0.290811	4.166221
-1093.032323	4.327879	4.176218
-1091.246287	2.177399	4.186214
-1089.546095	-2.146208	4.196211
-1087.630728	-2.984729	4.206208
-1085.637811	-3.693546	4.216205
-1083.836141	2.469867	4.226202
-1082.050838	4.074282	4.236198
-1079.888395	-2.259064	4.246195
-1078.093886	-5.945638	4.256192
-1076.358371	-3.504302	4.266189
-1074.545188	2.562540	4.276186
-1072.696225	-3.894344	4.286182
-1070.811983	-2.514169	4.296179
-1068.844461	1.349025	4.306176
-1066.847206	-5.489997	4.316173
-1065.049160	-0.784950	4.326170
-1063.281351	-4.129345	4.336166
-1061.405904	-2.689334	4.346163
-1059.526555	-7.122102	4.356160
-1057.634794	0.310618	4.366157
-1055.849122	-2.992418	4.376154
-1053.740583	1.958245	4.386150
-1051.879711	-3.712627	4.396147
-1050.168567	-4.237399	4.406144
-1048.351275	1.066169	4.416141
-1046.136627	-2.640210	4.426138
-1044.293067	4.609179	4.436134
-1042.604565	-3.115190	4.446131
-1041.077053	-3.357951	4.456128
-1038.483743	1.404666	4.466125
-1036.917704	0.449950	4.476122
-1034.727101	-0.835183	4.486118
-1033.257717	-1.087591	4.496115
-1031.472395	2.781092	4.506112
-1029.409988	-1.414087	4.516109
-1027.472949	-0.640746	4.526106
-1025.892736	4.091278	4.536102
-1023.762437	-8.475356	4.546099
-1021.764446	-3.115403	4.556096
-1019.910576	-3.602978	4.566093
-1018.301024	-1.514086	4.576090
-1016.362934	0.370685	4.586086
-1014.618978	-5.035143	4.596083
-1012.372888	-5.253856	4.606080
-1010.566127	-5.241253	4.616077
-1008.743831	-0.538458	4.626074
-1007.031908	-2.599653	4.636070
-1005.318055	-13.677026	4.646067
-1003.135656	-7.846017	4.656064
-1001.015440	-9.468812	4.666061
-999.411776	-10.358467	4.676058
-997.722757	-8.168585	4.686054
-995.491210	-9.194964	4.696051
-993.899894	-3.526790	4.706048
-991.861354	-1.290164	4.716045
-990.026558	-1.642032	4.726042
-987.976005	4.549558	4.736038
-986.223832	-2.916533	4.746035
-984.312780	-5.911143	4.756032
-982.778024	1.081361	4.766029
-980.834712	0.770569	4.776026
-978.584948	-4.122429	4.786022
-976.843907	-1.884006	4.796019
-974.778861	-3.846908	4.806016
-973.247957	-1.878041	4.816013
-971.380366	1.199106	4.826010
-969.228757	-1.837117	4.836006
-967.540905	-7.087097	4.846003
-965.673870	-4.268807	4.856000
-963.712909	-7.636121	4.865997
-962.128704	-1.632047	4.875994
-960.070268	-1.804913	4.885990
-957.848340	-4.430786	4.895987
-956.460415	-7.441200	4.905984
-954.539668	-4.839913	4.915981
-952.747355	-0.095961	4.925978
-950.486069	1.593502	4.935974
-948.660377	-2.462706	4.945971
-946.859361	-3.424935	4.955968
-944.895537	4.018471	4.965965
-943.158910	3.826022	4.975962
-941.147362	4.033305	4.985958
-939.300051	-0.695834	4.995955
-937.396463	-4.816593	5.005952
-935.651931	-7.023479	5.015949
-933.806841	6.445299	5.025946
-931.919759	9.063044	5.035942
-930.108763	3.144441	5.045939
-928.099430	2.112602	5.055936
-926.240519	-2.741540	5.065933
-924.368388	0.620712	5.075930
-922.419315	2.726441	5.085926
-920.539643	-2.798918	5.095923
-918.544996	-4.655778	5.105920
-916.903904	0.623966	5.115917
-915.256149	4.426316	5.125914
-913.065759	-5.664553	5.135910
-911.071687	-0.343345	5.145907
-909.349123	-3.067758	5.155904
-907.145818	0.539985	5.165901
-905.500142	0.322630	5.175898
-904.052789	-2.337252	5.185894
-902.055917	-2.272854	5.195891
-900.030542	-4.870408	5.205888
-898.006052	-2.399344	5.215885
-896.132207	-5.920047	5.225882
-894.070304	2.518261	5.235878
-892.554777	-3.880449	5.245875
-890.755659	-3.233368	5.255872
-888.488661	-1.191070	5.265869
-886.938145	6.965843	5.275866
-884.812606	-1.054089	5.285862
-882.971983	-4.244204	5.295859
-881.095941	-2.175713	5.305856
-879.506338	-5.260958	5.315853
-877.529527	-2.444356	5.325850
-875.762215	1.318383	5.335846
-873.721076	-0.002708	5.345843
-871.835100	-1.739524	5.355840
-869.801724	5.114932	5.365837
-867.931933	4.675458	5.375834
-866.244064	6.312986	5.385830
-864.260087	4.715248	5.395827
-862.536786	4.272354	5.405824
-860.686431	5.220746	5.415821
-858.630264	3.576735	5.425818
-856.641649	-1.190721	5.435814
-854.971621	4.387607	5.445811
-853.034698	0.722640	5.455808
-851.112220	-5.553203	5.465805
-849.532802	3.668075	5.475802
-847.541228	4.447059	5.485798
-845.511051	0.775085	5.495795
-843.593233	2.955352	5.505792
-841.849193	3.413905	5.515789
-839.965250	-0.675219	5.525786
-837.663728	-1.730003	5.535782
-836.257446	3.764181	5.545779
-834.379986	-3.878154	5.555776
-832.476277	1.520730	5.565773
-830.712129	1.192910	5.575770
-828.569578	-1.750161	5.585766
-826.806264	5.401717	5.595763
-824.619684	-1.560541	5.605760
-823.140293	5.065138	5.615757
-821.380184	1.231087	5.625754
-819.323109	2.838056	5.635750
-817.441848	0.854139	5.645747
-815.371716	4.866948	5.655744
-813.600383	-1.084706	5.665741
-811.726930	-4.614757	5.675738
-809.921302	5.056717	5.685734
-808.052802	1.746936	5.695731
-806.264200	5.378431	5.705728
-804.190919	7.345986	5.715725
-802.385616	7.850041	5.725722
-800.408807	3.864525	5.735718
-798.664868	4.127334	5.745715
-796.973147	1.297402	5.755712
-794.878833	3.539501	5.765709
-792.841752	1.704384	5.775706
-791.304102	7.772873	5.785702
-789.471898	3.390473	5.795699
-787.086818	3.541344	5.805696
-785.542428	4.412380	5.815693
-783.638453	1.903800	5.825690
-781.755319	0.320669	5.835686
-779.677115	-0.894159	5.845683
-778.019803	4.585206	5.855680
-776.023131	-1.921916	5.865677
-774.350607	-2.231892	5.875674
-772.359109	4.097236	5.885670
-770.841160	-6.274471	5.895667
-768.560324	-4.824800	5.905664
-766.803463	-2.617167	5.915661
-764.814071	0.938059	5.925658
-762.798310	3.879593	5.935654
-761.067827	6.877774	5.945651
-759.331061	4.076983	5.955648
-757.300040	7.357141	5.965645
-755.612281	2.749951	5.975642
-753.526373	10.144025	5.985638
-751.524139	9.285577	5.995635
-749.806897	5.557901	6.005632
-747.996268	10.191727	6.015629
-746.163606	8.496687	6.025626
-744.468650	10.396860	6.035622
-742.467125	4.683206	6.045619
-740.410752	8.024065	6.055616
-738.570989	8.012656	6.065613
-736.691293	6.488530	6.075610
-734.891997	5.234627	6.085606
-732.569907	2.859797	6.095603
-731.111599	7.406253	6.105600
-729.592325	4.352867	6.115597
-727.310231	12.362993	6.125594
-725.518428	11.604511	6.135590
-723.276929	8.762562	6.145587
-721.653687	9.226298	6.155584
-719.706519	6.564020	6.165581
-718.138012	8.956531	6.175578
-716.174154	9.337419	6.185574
-714.308981	4.512430	6.195571
-712.484952	3.104589	6.205568
-710.167739	2.582691	6.215565
-708.750131	7.756199	6.225562
-706.672901	7.329495	6.235558
-704.827373	5.447691	6.245555
-702.994747	9.642243	6.255552
-701.037108	5.050387	6.265549
-699.191512	6.874416	6.275546
-697.129653	5.395425	6.285542
-695.484363	1.204015	6.295539
-693.508646	5.020441	6.305536
-691.668640	6.873791	6.315533
-689.896086	1.623088	6.325530
-688.221041	6.545472	6.335526
-686.193888	7.541543	6.345523
-683.879365	10.575938	6.355520
-682.226480	8.644406	6.365517
-680.577364	9.997733	6.375514
-678.650527	13.267766	6.385510
-676.597021	10.193789	6.395507
-674.725069	14.385240	6.405504
-672.990656	8.291154	6.415501
-671.019019	11.434034	6.425498
-669.249945	11.880822	6.435494
-666.968631	9.162038	6.445491
-665.607660	6.244512	6.455488
-663.548539	8.490776	6.465485
-661.376199	5.138875	6.475482
-659.894260	4.584689	6.485478
-658.048355	3.135499	6.495475
-656.190858	3.825540	6.505472
-653.750686	2.859308	6.515469
-652.624099	12.400991	6.525466
-650.552343	11.790471	6.535462
-648.248301	8.313326	6.545459
-646.450122	1.999070	6.555456
-645.136439	9.603469	6.565453
-642.942384	8.226563	6.575450
-640.968198	8.195331	6.585446
-639.427332	3.515370	6.595443
-637.317974	7.703659	6.605440
-635.170184	4.107804	6.615437
-633.410646	6.218797	6.625434
-631.936151	8.819021	6.635430
-629.560610	10.591599	6.645427
-627.898133	5.001677	6.655424
-625.906993	9.128335	6.665421
-624.192821	6.411776	6.675418
-622.222136	12.115940	6.685414
-620.302306	7.639135	6.695411
-618.525674	16.115398	6.705408
-616.572156	12.309011	6.715405
-614.883529	11.603411	6.725402
-612.854634	10.458184	6.735398
-611.094889	12.711269	6.745395
-609.243783	5.657518	6.755392
-606.947202	9.669081	6.765389
-605.787464	8.937451	6.775386
-603.494574	14.947007	6.785382
-601.450309	10.451916	6.795379
-599.745241	14.638510	6.805376
-597.918786	13.211419	6.815373
-595.856909	12.899371	6.825370
-594.101684	13.741591	6.835366
-592.164539	18.082174	6.845363
-590.541560	9.122742	6.855360
-588.416558	11.707502	6.865357
-586.490786	8.816639	6.875354
-584.888552	9.261719	6.885350
-582.956095	7.386648	6.895347
-580.737842	7.817013	6.905344
-579.116999	4.766442	6.915341
-577.128308	11.271466	6.925338
-575.652786	12.049430	6.935334
-573.552194	4.028996	6.945331
-571.672221	9.375057	6.955328
-569.554556	11.244153	6.965325
-567.898928	17.186592	6.975322
-565.824773	10.056187	6.985318
-564.108505	9.044624	6.995315
-562.368586	7.898229	7.005312
-560.178208	8.047272	7.015309
-558.718594	4.932466	7.025306
-556.858605	10.134888	7.035302
-554.659861	14.965830	7.045299
-552.700598	13.737037	7.055296
-550.885277	4.345850	7.065293
-549.077841	14.317272	7.075290
-547.267163	14.495397	7.085286
-545.080666	8.608664	7.095283
-543.731255	10.366806	7.105280
-541.434118	9.129846	7.115277
-539.667486	9.783966	7.125274
-537.626442	12.907981	7.135270
-536.065577	12.977591	7.145267
-534.052979	7.622336	7.155264
-532.207179	7.793283	7.165261
-530.773510	1.406271	7.175258
-528.509290	9.795255	7.185254
-526.321829	16.451740	7.195251
-524.583368	5.970722	7.205248
-523.055474	4.564531	7.215245
-521.009788	1.046664	7.225242
-518.956986	6.477272	7.235238
-517.032360	10.557807	7.245235
-515.286080	6.869865	7.255232
-513.574700	5.655431	7.265229
-511.487274	5.552536	7.275226
-509.600671	0.975332	7.285222
-508.013211	-3.067770	7.295219
-505.878733	-1.738153	7.305216
-503.878551	2.576643	7.315213
-502.281534	7.535315	7.325210
-500.502707	6.505911	7.335206
-498.227984	4.696247	7.345203
-496.578042	-2.757932	7.355200
-494.846969	-0.219125	7.365197
-492.752189	0.060513	7.375194
-490.958653	2.778825	7.385190
-488.976883	9.495036	7.395187
-487.131914	8.194548	7.405184
-485.154520	1.940204	7.415181
-483.449249	3.193122	7.425178
-481.487730	11.231017	7.435174
-479.557671	1.761553	7.445171
-477.688450	0.831416	7.455168
-476.146305	-0.420703	7.465165
-474.097440	0.963669	7.475162
-472.000579	5.976751	7.485158
-470.394817	0.733888	7.495155
-468.399933	-0.871583	7.505152
-466.481571	-0.944282	7.515149
-464.740385	1.640303	7.525146
-462.524781	4.190182	7.535142
-460.909567	3.262726	7.545139
-458.970292	2.438260	7.555136
-457.191004	1.598291	7.565133
-455.324451	-2.192500	7.575130
-453.368633	-0.878516	7.585126
-451.517302	6.168036	7.595123
-449.884257	3.046125	7.605120
-447.706546	3.075713	7.615117
-445.693713	0.643171	7.625114
-444.206511	-0.495942	7.635110
-442.125650	-2.522495	7.645107
-440.496362	2.686860	7.655104
-438.059435	4.105614	7.665101
-436.301839	-0.368829	7.675098
-434.704305	5.052447	7.685094
-432.831441	2.031203	7.695091
-430.805148	-0.754008	7.705088
-429.045742	2.023487	7.715085
-427.208915	-0.442516	7.725082
-425.026277	1.307387	7.735078
-423.482235	1.809238	7.745075
-421.586192	3.304901	7.755072
-419.809961	0.474363	7.765069
-417.931218	-0.054610	7.775066
-415.866208	1.633555	7.785062
-413.865417	5.870966	7.795059
-412.030722	-0.430012	7.805056
-410.279907	2.200446	7.815053
-408.320232	10.995030	7.825050
-406.475562	10.627825	7.835046
-404.583498	3.747681	7.845043
-402.893732	1.755185	7.855040
-400.636321	4.104234	7.865037
-398.805435	2.619743	7.875034
-396.991656	6.162280	7.885030
-395.416991	1.396540	7.895027
-393.308361	2.791967	7.905024
-391.411080	0.606869	7.915021
-389.609219	3.889204	7.925018
-387.920039	7.999546	7.935014
-385.947072	9.475062	7.945011
-383.898683	6.318459	7.955008
-381.883895	3.631441	7.965005
-380.163534	0.056681	7.975002
-378.467663	1.603285	7.984998
-376.366170	1.905638	7.994995
-374.624397	1.712782	8.004992
-372.734537	-2.369042	8.014989
-370.714580	0.916382	8.024986
-369.103285	3.937048	8.034982
-367.272517	8.220593	8.044979
-365.135006	-1.439807	8.054976
-363.267406	3.777350	8.064973
-361.486665	0.229278	8.074970
-359.386084	8.481928	8.084966
-357.580460	6.725180	8.094963
-355.854516	0.097386	8.104960
-354.355103	5.393857	8.114957
-351.892056	4.140064	8.124954
-350.047606	10.227786	8.134950
-348.548704	5.313113	8.144947
-346.184551	6.243046	8.154944
-344.467169	0.494536	8.164941
-342.882413	-0.135869	8.174938
-341.251134	8.845414	8.184934
-338.971111	8.096123	8.194931
-336.880112	5.540662	8.204928
-335.118142	11.259453	8.214925
-333.098200	5.584230	8.224922
-331.361841	10.762365	8.234918
-329.658738	8.459888	8.244915
-327.826109	5.825678	8.254912
-325.488434	8.011985	8.264909
-324.020109	15.348743	8.274906
-322.016214	10.835057	8.284902
-320.114065	4.055997	8.294899
-318.415104	8.248515	8.304896
-316.081699	9.762870	8.314893
-314.691277	13.316212	8.324890
-313.032818	8.750305	8.334886
-310.862141	6.840580	8.344883
-308.838801	5.202274	8.354880
-307.072816	2.940303	8.364877
-305.022986	10.541096	8.374874
-303.448610	9.102359	8.384870
-301.465730	14.719598	8.394867
-299.453950	6.168808	8.404864
-297.502181	7.259354	8.414861
-295.777178	9.402959	8.424858
-293.917860	12.635147	8.434854
-292.280232	12.913721	8.444851
-290.017178	8.344482	8.454848
-288.154845	12.060939	8.464845
-286.687919	8.591431	8.474842
-284.734183	5.754760	8.484838
-282.604846	12.957614	8.494835
-280.672203	6.431087	8.504832
-278.889946	8.428195	8.514829
-276.767295	12.347851	8.524826
-274.948021	10.104239	8.534822
-273.489357	8.281351	8.544819
-271.485611	15.008465	8.554816
-269.474027	17.302142	8.564813
-267.487988	13.974002	8.574810
-265.683161	15.323296	8.584807
-263.813744	10.057421	8.594803
-261.768206	10.386174	8.604800
-260.575085	10.520976	8.614797
-258.306571	7.125653	8.624794
-256.360934	11.029370	8.634791
-254.289254	2.739060	8.644787
-252.981070	9.842472	8.654784
-250.903071	13.014528	8.664781
-248.634268	13.129234	8.674778
-247.224617	12.042093	8.684775
-245.176675	12.814169	8.694771
-243.191468	7.599305	8.704768
-241.400290	10.405033	8.714765
-239.512906	4.321557	8.724762
-237.448193	9.450519	8.734759
-235.527521	10.959771	8.744755
-233.607129	5.537360	8.754752
-231.860211	-3.304267	8.764749
-230.226907	4.685180	8.774746
-228.372999	1.480795	8.784743
-226.421390	-0.532844	8.794739
-224.328528	1.708424	8.804736
-222.530942	5.054732	8.814733
-220.759823	6.616285	8.824730
-218.728854	2.897323	8.834727
-216.972181	7.930197	8.844723
-215.237324	1.662657	8.854720
-213.187276	3.689711	8.864717
-211.470113	7.042547	8.874714
-209.463857	5.223888	8.884711
-207.366170	1.792716	8.894707
-205.821600	5.342049	8.904704
-204.277451	7.091418	8.914701
-201.896496	-4.903535	8.924698
-199.928757	2.527291	8.934695
-198.413143	3.220144	8.944691
-196.338659	-1.787872	8.954688
-194.308254	5.778226	8.964685
-192.560958	5.775678	8.974682
-190.616704	2.135315	8.984679
-189.006196	1.036681	8.994675
-187.090811	-0.715351	9.004672
-184.934334	3.510049	9.014669
-183.206610	-2.418430	9.024666
-181.509370	4.575570	9.034663
-179.635793	2.197045	9.044659
-177.522752	-6.519809	9.054656
-175.650009	-3.850208	9.064653
-173.699507	-0.548791	9.074650
-171.850372	-0.264412	9.084647
-170.328167	0.795308	9.094643
-167.888420	3.016011	9.104640
-166.189242	1.200598	9.114637
-164.364197	3.606236	9.124634
-162.932949	0.753558	9.134631
-160.814865	4.533519	9.144627
-158.804670	1.602673	9.154624
-156.850726	1.295592	9.164621
-154.959922	2.947045	9.174618
-153.226567	3.876767	9.184615
-151.345377	-0.798785	9.194611
-149.721250	-2.074832	9.204608
-147.725616	-3.662793	9.214605
-145.610977	-4.166036	9.224602
-143.732667	-3.082591	9.234599
-141.899482	-8.844706	9.244595
-139.992694	2.219651	9.254592
-138.207928	3.276974	9.264589
-136.132088	-1.134357	9.274586
-134.463203	5.316299	9.284583
-132.660158	7.166515	9.294579
-130.508775	3.172617	9.304576
-128.731992	1.709591	9.314573
-127.012183	8.875301	9.324570
-125.106523	7.165921	9.334567
-122.952540	1.884747	9.344563
-121.486111	3.160245	9.354560
-119.617118	-0.867536	9.364557
-117.395047	4.343797	9.374554
-115.651779	5.800922	9.384551
-113.942884	7.547750	9.394547
-112.214955	15.039028	9.404544
-109.781998	9.414926	9.414541
-108.220807	11.711124	9.424538
-106.436121	9.830003	9.434535
-104.322269	9.042705	9.444531
-102.532973	6.426626	9.454528
-100.453340	9.448552	9.464525
-98.606380	7.162756	9.474522
-96.923592	8.069007	9.484519
-95.293584	11.227411	9.494515
-93.279698	7.899703	9.504512
-91.372254	7.919047	9.514509
-89.550773	4.933098	9.524506
-87.456641	9.744864	9.534503
-85.327946	9.138377	9.544499
-83.770371	8.706691	9.554496
-81.860529	9.000402	9.564493
-80.151178	8.242920	9.574490
-78.036325	4.098575	9.584487
-76.301065	7.360202	9.594483
-74.339596	8.589913	9.604480
-72.588969	-0.250629	9.614477
-70.569394	5.600961	9.624474
-68.903412	5.349363	9.634471
-66.965859	-1.457268	9.644467
-64.859993	-0.310587	9.654464
-63.176520	12.546877	9.664461
-61.450853	8.414103	9.674458
-59.323496	6.757830	9.684455
-57.723070	2.349769	9.694451
-55.618873	5.010967	9.704448
-53.565349	-1.916788	9.714445
-51.621717	5.857499	9.724442
-50.033498	4.034602	9.734439
-48.134072	1.086776	9.744435
-46.453393	3.681329	9.754432
-44.238149	7.501163	9.764429
-42.411635	6.502381	9.774426
-40.462729	9.000466	9.784423
-39.089347	8.171866	9.794419
-37.064912	4.957786	9.804416
-34.814241	2.253948	9.814413
-33.053172	1.832466	9.824410
-31.180628	6.641734	9.834407
-29.440757	5.072560	9.844403
-27.509098	9.292917	9.854400
-25.507651	2.894552	9.864397
-23.784154	7.724443	9.874394
-21.981351	2.325682	9.884391
-20.034300	6.849911	9.894387
-17.892963	9.704171	9.904384
-16.126952	2.132289	9.914381
-14.396173	3.520427	9.924378
-12.410030	2.082513	9.934375
-10.777207	0.066206	9.944371
-8.588405	1.619717	9.954368
-6.858857	3.786495	9.964365
-5.360811	15.893570	9.974362
-3.926687	37.195802	9.984359
-2.708635	73.447646	9.994355
-0.946846	121.974791	10.004352
0.000000	172.759355	10.009357
0.717810	207.434642	10.014362
1.267073	238.464091	10.019367
2.261913	256.748271	10.024371
2.251389	278.692174	10.029376
2.643656	284.876054	10.034381
2.654265	294.535001	10.039386
3.266587	312.676832	10.044391
3.628333	312.070322	10.049395
3.392062	328.213849	10.054400
3.578890	323.736901	10.059405
3.539766	328.573464	10.064410
3.337477	329.001538	10.069415
3.765448	326.731771	10.074419
3.382734	336.567025	10.079424
3.652669	338.152991	10.084429
3.561809	339.966820	10.089434
3.473355	339.370612	10.094439
3.854507	340.197651	10.099443
3.922360	338.366955	10.104448
3.756908	338.486369	10.109453
3.958121	346.752424	10.114458
3.762233	349.814642	10.119463
4.103346	344.701204	10.124467
4.040965	346.537301	10.129472
4.262571	342.408049	10.134477
4.092254	349.897554	10.139482
4.251137	353.226473	10.144487
4.520321	347.317083	10.149491
4.038998	354.838849	10.154496
4.330194	351.348219	10.159501
4.056863	357.035091	10.164506
4.065795	379.103779	10.169511
4.595044	381.271306	10.174515
4.544905	389.228957	10.179520
4.723277	388.932399	10.184525
4.809677	389.836416	10.189530
4.948157	393.242717	10.194535
4.480455	371.488426	10.199539
4.699103	387.878014	10.204544
5.164045	382.639153	10.209549
4.743148	372.610300	10.214554
4.797441	381.456490	10.219559
5.267091	378.952979	10.224563
4.653769	378.008387	10.229568
5.360569	391.167692	10.234573
5.268545	377.475043	10.239578
4.873705	390.874715	10.244583
4.899914	375.663479	10.249587
5.053816	396.408045	10.254592
5.470223	394.400318	10.259597
5.469033	398.500701	10.264602
5.006615	399.575836	10.269607
5.443074	396.789025	10.274611
5.350181	405.382729	10.279616
5.874659	409.853450	10.284621
5.455424	398.537477	10.289626
5.277883	398.468002	10.294631
5.750292	407.821548	10.299635
5.440323	422.142877	10.304640
5.447185	421.444727	10.309645
5.378323	420.764964	10.314650
5.355764	431.339225	10.319655
6.056763	422.456083	10.324659
5.716679	421.963086	10.329664
5.881758	427.008394	10.334669
5.823887	433.111165	10.339674
5.500149	430.056077	10.344679
5.683499	419.751036	10.349683
5.778853	426.826033	10.354688
5.735801	435.146868	10.359693
6.196345	439.044302	10.364698
6.021449	451.000679	10.369703
6.091384	455.884547	10.374707
6.077211	461.154007	10.379712
6.373369	460.020191	10.384717
6.324893	459.289864	10.389722
6.040580	461.872605	10.394727
6.324891	461.420371	10.399731
6.193028	472.318036	10.404736
6.548337	461.741101	10.409741
6.529924	467.266714	10.414746
6.287973	467.339981	10.419751
6.628348	469.521877	10.424755
6.359942	472.672961	10.429760
6.326395	493.728272	10.434765
6.583539	496.201002	10.439770
6.727495	512.282510	10.444775
7.201910	501.334874	10.449779
6.907032	512.521931	10.454784
7.077164	508.679974	10.459789
7.053553	506.045374	10.464794
7.158955	513.934129	10.469799
7.476958	511.778073	10.474803
6.995453	519.557006	10.479808
7.306528	515.563252	10.484813
6.992868	512.033433	10.489818
7.236444	517.796412	10.494823
7.534688	508.573740	10.499827
7.385167	520.319538	10.504832
7.032889	513.627651	10.509837
7.461462	514.164851	10.514842
7.143893	515.325705	10.519847
7.438948	514.633626	10.524851
7.340955	521.085046	10.529856
7.390441	519.946414	10.534861
7.110547	521.998582	10.539866
7.413950	535.796395	10.544871
8.060954	540.895769	10.549875
8.038436	544.007650	10.554880
7.991070	552.695109	10.559885
8.232169	549.877925	10.564890
7.837089	538.956975	10.569895
7.921231	539.585384	10.574899
7.913536	548.608726	10.579904
8.151970	544.896221	10.584909
8.249011	554.350736	10.589914
7.681926	559.807771	10.594919
8.256726	550.957297	10.599923
8.090832	554.205593	10.604928
8.205901	557.316033	10.609933
8.503811	556.003728	10.614938
8.326256	563.349411	10.619943
8.487301	559.709172	10.624947
8.639664	564.289758	10.629952
8.526869	558.628874	10.634957
8.651102	568.824992	10.639962
8.484672	563.014958	10.644967
8.555841	562.330201	10.649971
8.241441	568.552795	10.654976
8.285513	571.919001	10.659981
8.390409	575.641375	10.664986
8.077819	569.253805	10.669991
8.689559	577.214806	10.674995
8.512205	599.058062	10.680000
8.692517	597.064311	10.685005
8.739093	606.504830	10.690010
8.668668	613.123789	10.695015
9.414476	605.452433	10.700019
8.870022	602.516094	10.705024
8.931480	612.845264	10.710029
8.674788	613.042313	10.715034
9.239204	623.631908	10.720039
9.341132	635.553747	10.725043
9.383537	632.810818	10.730048
9.568439	633.732258	10.735053
9.747644	638.351166	10.740058
9.577008	645.080745	10.745063
9.650711	620.820560	10.750067
9.348052	622.818023	10.755072
9.502524	632.840621	10.760077
9.513082	632.709603	10.765082
9.703461	643.835134	10.770087
10.024882	634.042533	10.775091
9.866681	642.900695	10.780096
9.840129	647.189706	10.785101
10.035963	642.649721	10.790106
9.490474	658.546451	10.795111
10.203518	646.248555	10.800115
10.126701	656.385334	10.805120
10.109508	648.960238	10.810125
10.106637	649.440096	10.815130
9.762710	649.819802	10.820135
10.046174	653.130496	10.825139
9.684259	651.160139	10.830144
9.874960	649.464360	10.835149
10.415568	648.026601	10.840154
9.638277	658.645707	10.845159
10.230419	653.137292	10.850163
10.206768	665.366204	10.855168
10.450680	679.263534	10.860173
10.682993	679.898280	10.865178
10.560451	685.301805	10.870183
10.595362	682.810812	10.875187
10.412649	689.334169	10.880192
10.743861	688.147435	10.885197
10.997128	682.937499	10.890202
11.054129	690.152790	10.895207
10.986878	679.625748	10.900211
11.043514	683.693332	10.905216
10.974585	680.643283	10.910221
10.962809	673.646264	10.915226
10.897866	681.825644	10.920231
11.023755	677.181681	10.925235
11.058741	689.380759	10.930240
11.076000	686.498321	10.935245
11.487207	681.296313	10.940250
10.991391	694.701329	10.945255
11.366234	685.384323	10.950259
11.411709	689.094126	10.955264
11.075757	690.953397	10.960269
11.408838	696.804679	10.965274
10.998476	692.987448	10.970279
11.236678	685.934782	10.975283
10.869218	689.893382	10.980288
10.842710	685.480315	10.985293
11.164994	705.222281	10.990298
11.401214	718.442749	10.995303
11.462091	714.851566	11.000307
11.750275	715.950514	11.005312
11.852222	713.041947	11.010317
12.114655	719.853884	11.015322
12.149194	724.095324	11.020327
12.101888	709.253453	11.025331
12.238858	722.360438	11.030336
11.873009	715.240089	11.035341
12.089246	714.330325	11.040346
11.993896	724.173624	11.045351
12.419891	713.839137	11.050355
12.002117	717.545558	11.055360
12.159094	722.543373	11.060365
12.642432	715.375896	11.065370
12.268939	718.602143	11.070375
12.231995	720.133015	11.075379
12.174773	725.248578	11.080384
11.941506	724.483052	11.085389
12.108588	711.702870	11.090394
11.966519	724.485335	11.095399
12.168680	728.868786	11.100403
12.296651	749.442940	11.105408
12.660010	756.298724	11.110413
12.679389	745.270511	11.115418
12.488887	750.020965	11.120423
12.810591	748.444636	11.125427
12.923916	751.736756	11.130432
12.936705	749.460603	11.135437
13.015524	745.822393	11.140442
12.952198	751.552409	11.145447
13.010358	743.443425	11.150451
13.246498	753.088785	11.155456
13.237944	752.311072	11.160461
13.479060	751.949303	11.165466
13.055160	753.832072	11.170471
13.274591	745.618513	11.175475
13.355932	755.430498	11.180480
13.335902	749.836749	11.185485
13.523437	756.646456	11.190490
13.325984	760.823978	11.195495
13.666728	748.907095	11.200499
13.366059	757.743893	11.205504
13.359084	758.274874	11.210509
13.630228	762.992705	11.215514
13.138021	759.816174	11.220519
13.547233	757.645535	11.225523
13.643580	763.225502	11.230528
13.466759	768.216644	11.235533
13.803322	778.670798	11.240538
13.727532	787.246229	11.245543
13.790993	782.208466	11.250547
13.802581	781.752410	11.255552
14.083492	785.243326	11.260557
14.384886	786.073652	11.265562
14.251542	785.632828	11.270567
14.579226	782.404375	11.275571
14.264331	780.719830	11.280576
13.901806	772.255280	11.285581
14.352219	771.809664	11.290586
14.206082	778.417118	11.295591
14.607823	780.169781	11.300595
14.352506	791.836472	11.305600
14.718339	785.085119	11.310605
14.569412	773.714699	11.315610
14.254373	773.482637	11.320615
14.361564	773.735198	11.325619
14.791370	786.010166	11.330624
14.590980	793.402187	11.335629
14.616329	784.431038	11.340634
14.690867	792.216051	11.345639
14.742696	785.065321	11.350643
14.459388	784.866048	11.355648
14.631257	783.340424	11.360653
14.848181	792.498413	11.365658
14.305985	786.106364	11.370663
14.710467	781.239727	11.375667
14.709773	790.757296	11.380672
14.667524	807.725167	11.385677
15.172848	810.435930	11.390682
15.122852	823.106019	11.395687
15.142722	823.668993	11.400691
15.263312	822.124734	11.405696
15.188394	819.510876	11.410701
15.718347	812.045741	11.415706
15.424154	825.868178	11.420711
15.577536	810.413840	11.425715
15.493725	812.638212	11.430720
15.446651	813.478385	11.435725
16.108321	816.154750	11.440730
15.672655	819.815161	11.445735
15.909449	818.607204	11.450739
15.889662	811.411111	11.455744
15.596596	795.151155	11.460749
15.706695	800.867723	11.465754
15.808348	815.680483	11.470759
16.148669	817.982299	11.475763
16.013236	819.472115	11.480768
15.793634	815.261704	11.485773
15.821086	810.507235	11.490778
15.894594	821.086959	11.495783
16.107307	819.359263	11.500787
16.062435	826.731228	11.505792
15.995274	822.233134	11.510797
16.195128	816.550670	11.515802
15.734710	824.405252	11.520807
16.204353	817.036471	11.525811
16.157272	825.288782	11.530816
16.391852	829.905227	11.535821
16.251227	823.223595	11.540826
16.137331	821.688348	11.545831
16.456236	836.701460	11.550835
16.750561	849.483823	11.555840
16.835966	853.141564	11.560845
16.967914	831.923337	11.565850
16.643062	825.580188	11.570855
16.625917	820.547383	11.575859
16.507013	829.065056	11.580864
16.508290	840.531578	11.585869
17.178858	840.836219	11.590874
17.024897	849.425732	11.595879
17.444566	848.699571	11.600883
17.140610	832.898655	11.605888
16.881169	831.069633	11.610893
16.834658	827.355193	11.615898
17.053713	838.225549	11.620903
17.134094	849.494946	11.625907
17.247365	845.474302	11.630912
17.066363	855.558446	11.635917
17.379155	853.933063	11.640922
17.253092	849.857543	11.645927
17.357369	842.192186	11.650931
17.441649	852.491077	11.655936
17.585570	852.606885	11.660941
17.617368	846.202113	11.665946
17.362194	850.242201	11.670951
17.464869	843.770929	11.675955
17.645331	850.203315	11.680960
17.440507	850.737468	11.685965
17.656920	853.276686	11.690970
17.602483	846.767388	11.695975
17.484344	849.191219	11.700979
17.671782	861.090143	11.705984
17.830807	874.097547	11.710989
18.244454	886.200125	11.715994
18.204230	886.529819	11.720999
18.203869	879.505647	11.726003
18.276554	882.700193	11.731008
17.965549	867.706239	11.736013
18.049608	870.938395	11.741018
18.095777	887.168388	11.746023
18.104723	887.013969	11.751027
18.444023	883.469807	11.756032
18.307511	886.590480	11.761037
18.438483	884.123557	11.766042
18.512626	888.809768	11.771047
18.375431	879.396099	11.776051
18.405524	892.845158	11.781056
18.422666	886.439551	11.786061
18.722710	876.993996	11.791066
18.579899	883.490574	11.796071
18.895346	879.079682	11.801075
18.910192	883.556138	11.806080
18.826785	886.400241	11.811085
19.076880	890.954304	11.816090
18.930501	889.285449	11.821095
18.849615	877.207036	11.826099
18.736944	883.679881	11.831104
18.388264	882.592109	11.836109
19.080250	880.067250	11.841114
18.535195	889.081886	11.846119
19.328634	894.446636	11.851123
19.264941	914.297761	11.856128
18.885641	915.190926	11.861133
19.116881	905.138120	11.866138
19.286727	921.490361	11.871143
19.517241	917.471499	11.876147
19.354444	924.641533	11.881152
19.562952	921.890983	11.886157
19.495277	910.766133	11.891162
19.367464	924.144206	11.896167
19.581467	908.134432	11.901171
19.294526	918.356949	11.906176
19.463198	919.217915	11.911181
19.645971	914.750897	11.916186
19.548209	928.240883	11.921191
19.806746	908.904290	11.926195
19.764260	911.424882	11.931200
19.697840	919.371226	11.936205
19.849703	922.261396	11.941210
19.556400	944.590474	11.946215
19.976262	944.818403	11.951219
20.385989	946.834761	11.956224
20.239924	948.389368	11.961229
20.333158	937.721416	11.966234
20.292373	941.366188	11.971239
20.116733	930.983992	11.976243
20.334133	943.136842	11.981248
20.231794	945.056663	11.986253
20.782941	932.650301	11.991258
20.708395	939.336303	11.996263
20.552838	939.234930	12.001267
20.739763	932.180861	12.006272
20.571798	922.505548	12.011277
20.521975	905.303016	12.016282
20.527935	913.375018	12.021287
20.529245	914.920310	12.026291
20.534600	906.638296	12.031296
20.475152	908.953421	12.036301
20.790468	904.749137	12.041306
20.243590	914.047949	12.046311
20.704416	918.830203	12.051315
21.209151	907.664527	12.056320
20.512988	911.227726	12.061325
20.623252	904.364105	12.066330
20.384300	917.124342	12.071335
20.446283	909.396305	12.076339
20.315210	911.673965	12.081344
20.109144	909.148822	12.086349
20.455870	914.099093	12.091354
20.737730	938.380298	12.096359
20.620583	934.361683	12.101363
20.922921	921.447774	12.106368
20.673800	921.241467	12.111373
20.657955	913.005411	12.116378
20.864008	915.211955	12.121383
20.939498	919.092083	12.126387
20.984864	910.634940	12.131392
20.667399	912.822472	12.136397
20.571297	906.524810	12.141402
20.253399	914.303089	12.146407
20.573206	914.395577	12.151411
20.638784	909.855783	12.156416
20.747329	912.998882	12.161421
20.761890	905.571743	12.166426
20.543427	913.193804	12.171431
20.781423	908.945077	12.176435
20.742156	910.290246	12.181440
20.461603	898.494412	12.186445
20.734006	891.459849	12.191450
20.622034	890.703354	12.196455
20.479206	878.716825	12.201459
20.623286	878.597627	12.206464
20.138053	885.785950	12.211469
20.553198	891.930173	12.216474
20.364280	914.002843	12.221479
20.732463	906.181814	12.226483
20.983467	913.065056	12.231488
20.780790	900.469847	12.236493
20.757293	885.322779	12.241498
20.340276	891.544528	12.246503
20.428843	885.480791	12.251507
20.474352	882.973879	12.256512
20.510100	881.687590	12.261517
20.668154	881.367454	12.266522
20.321298	887.377725	12.271527
20.125583	887.673868	12.276531
20.753615	905.577384	12.281536
20.456850	913.410643	12.286541
20.826677	905.567273	12.291546
20.643947	905.926004	12.296551
20.452684	888.373865	12.301555
20.594085	891.081182	12.306560
20.513199	890.102095	12.311565
20.428915	889.338031	12.316570
20.054686	893.646294	12.321575
20.669651	905.440795	12.326579
20.825004	912.914919	12.331584
20.481143	927.956556	12.336589
20.856688	921.317141	12.341594
20.529425	905.042014	12.346599
20.674768	896.840186	12.351603
20.801094	897.715790	12.356608
20.374349	897.704982	12.361613
20.496011	890.842704	12.366618
20.346591	898.713960	12.371623
20.212264	892.353011	12.376627
20.398951	918.966061	12.381632
20.299680	924.872200	12.386637
20.820097	918.316920	12.391642
20.417653	927.130626	12.396647
20.706269	925.136905	12.401651
20.698363	927.077934	12.406656
20.715893	926.253471	12.411661
20.884213	905.445679	12.416666
20.209415	903.780672	12.421671
20.599270	903.832023	12.426675
20.411481	901.988410	12.431680
20.465388	912.664374	12.436685
21.031950	911.444819	12.441690
20.752039	912.244856	12.446695
20.498774	899.813845	12.451699
20.573113	893.102626	12.456704
20.424980	899.022856	12.461709
20.439800	894.904352	12.466714
20.645039	900.810803	12.471719
20.580706	893.255896	12.476723
20.921522	894.827468	12.481728
20.628348	897.217717	12.486733
20.569586	893.558834	12.491738
20.495514	899.527180	12.496743
20.451569	893.158124	12.501747
20.468153	891.299263	12.506752
20.664918	896.475309	12.511757
20.742696	884.554522	12.516762
20.670971	896.835455	12.521767
20.724497	898.219443	12.526771
20.791113	895.806940	12.531776
20.696343	899.827766	12.536781
20.837411	891.937304	12.541786
20.771876	896.073323	12.546791
20.527185	900.256842	12.551795
20.387707	894.298864	12.556800
20.687483	898.835543	12.561805
21.091384	891.177570	12.566810
20.435110	891.051972	12.571815
20.544170	879.843761	12.576819
21.025787	882.731796	12.581824
20.592062	877.259177	12.586829
20.425448	870.471273	12.591834
20.436826	867.865722	12.596839
20.405744	866.678408	12.601843
20.359556	873.575913	12.606848
20.281006	885.096206	12.611853
21.007693	895.392023	12.616858
20.700594	879.405464	12.621863
20.526539	871.555810	12.626867
20.778678	870.550420	12.631872
20.856601	869.511311	12.636877
20.496760	866.821454	12.641882
20.747701	870.099538	12.646887
20.462347	875.447094	12.651891
20.418022	869.652157	12.656896
20.103253	881.325247	12.661901
20.696413	863.244302	12.666906
20.485853	872.462638	12.671911
20.189677	868.300696	12.676915
20.670757	858.430438	12.681920
20.472553	873.600186	12.686925
20.478062	871.252630	12.691930
20.738629	873.515133	12.696935
20.627903	872.103962	12.701939
20.849762	872.568486	12.706944
20.461321	877.435712	12.711949
20.775550	866.242100	12.716954
20.641841	877.449465	12.721959
20.336199	875.293470	12.726963
20.785249	870.777689	12.731968
20.521419	879.286964	12.736973
20.640616	873.693041	12.741978
20.641902	875.276183	12.746983
20.691440	880.235992	12.751987
20.872902	882.692474	12.756992
20.731885	881.532155	12.761997
20.794603	881.325002	12.767002
20.716497	881.069341	12.772007
20.520580	884.137983	12.777011
21.014534	876.970313	12.782016
20.462500	873.109391	12.787021
20.999875	876.636702	12.792026
20.417300	864.769209	12.797031
20.244480	857.517071	12.802035
20.449567	867.353552	12.807040
20.226947	876.341987	12.812045
20.648782	871.116139	12.817050
20.407689	884.652600	12.822055
20.754624	879.418194	12.827059
20.787981	876.820175	12.832064
20.554375	879.013252	12.837069
20.313191	879.117937	12.842074
20.391738	880.833846	12.847079
20.424691	880.081048	12.852083
20.752144	880.926149	12.857088
20.559271	881.851084	12.862093
20.694254	879.478146	12.867098
20.765612	882.217134	12.872103
20.328726	870.432064	12.877107
20.817540	859.947097	12.882112
20.401248	867.537604	12.887117
20.597054	870.464912	12.892122
20.298756	864.584320	12.897127
20.577576	873.732489	12.902131
20.517754	879.081925	12.907136
20.653343	878.257560	12.912141
20.734530	882.143078	12.917146
20.458699	863.191414	12.922151
20.115508	866.116373	12.927155
20.827221	860.856912	12.932160
20.340504	872.759283	12.937165
20.940724	872.356008	12.942170
20.562940	882.047328	12.947175
20.508050	865.120060	12.952179
20.434768	858.788815	12.957184
20.646127	882.562321	12.962189
20.835215	869.764297	12.967194
20.381085	863.134224	12.972199
20.141228	856.293350	12.977203
20.450047	864.399027	12.982208
20.688394	873.189352	12.987213
20.951511	876.523846	12.992218
20.749656	868.850527	12.997223
20.196140	872.171755	13.002227
20.634989	858.438138	13.007232
20.596073	866.652898	13.012237
20.615440	856.878360	13.017242
20.505550	860.368542	13.022247
20.509542	856.617652	13.027251
20.449901	861.692646	13.032256
20.171877	867.037453	13.037261
20.632592	871.986877	13.042266
20.529675	887.117785	13.047271
20.652529	890.785334	13.052275
20.711671	882.426941	13.057280
20.622640	880.220627	13.062285
20.606369	870.161585	13.067290
20.577271	867.201344	13.072295
20.294751	868.255701	13.077299
20.264320	868.549138	13.082304
20.515442	882.655263	13.087309
20.623733	883.715103	13.092314
20.694275	887.692213	13.097319
20.606588	899.485228	13.102323
20.687394	890.377427	13.107328
20.468856	891.945165	13.112333
20.783119	879.466235	13.117338
20.552788	874.230854	13.122343
20.154958	866.185066	13.127347
20.688121	874.858981	13.132352
20.722383	884.459351	13.137357
20.513370	876.530109	13.142362
20.417946	870.438950	13.147367
20.568303	874.379670	13.152371
20.667483	865.805152	13.157376
20.585790	870.984598	13.162381
20.287978	866.833957	13.167386
20.818867	876.486009	13.172391
20.825562	882.209639	13.177395
20.779706	866.399062	13.182400
20.520417	868.028493	13.187405
20.603734	863.750830	13.192410
20.557197	871.176703	13.197415
20.550478	866.385085	13.202419
20.741670	861.500398	13.207424
20.587830	858.796612	13.212429
20.636862	859.588340	13.217434
20.427405	857.267187	13.222439
20.442688	863.549295	13.227443
20.684737	863.028093	13.232448
20.467053	871.938462	13.237453
20.702040	867.313310	13.242458
20.452252	870.586096	13.247463
20.388808	870.320212	13.252467
20.728371	866.386480	13.257472
20.737718	875.494046	13.262477
20.702660	864.293062	13.267482
20.688876	861.570091	13.272487
20.614587	865.399972	13.277491
20.659804	864.569520	13.282496
20.443269	871.738637	13.287501
20.768282	866.411531	13.292506
20.567677	866.714762	13.297511
20.541704	868.888914	13.302515
20.702076	861.356536	13.307520
20.613850	870.265181	13.312525
20.623442	864.198278	13.317530
20.755876	863.219866	13.322535
20.607176	862.598549	13.327539
20.774197	867.197395	13.332544
20.148693	874.731382	13.337549
20.256031	871.068091	13.342554
20.911487	872.092705	13.347559
20.704206	871.408186	13.352563
20.827256	868.611348	13.357568
20.516392	863.264227	13.362573
20.504165	845.846021	13.367578
20.598935	850.122050	13.372583
20.622577	854.841538	13.377587
20.431925	837.596888	13.382592
20.064025	860.688412	13.387597
20.627005	866.127758	13.392602
20.953168	877.562995	13.397607
20.595817	868.632329	13.402611
20.419634	861.540007	13.407616
20.518535	869.426839	13.412621
20.490585	874.596137	13.417626
20.613100	870.143475	13.422631
20.799637	864.909423	13.427635
20.359781	851.456318	13.432640
20.031274	854.337929	13.437645
20.518144	867.769309	13.442650
20.710076	871.632430	13.447655
20.358924	876.749192	13.452659
20.941722	866.966791	13.457664
20.690568	874.775407	13.462669
20.780705	865.099970	13.467674
20.555452	865.738313	13.472679
20.414291	852.461509	13.477683
20.643868	839.996119	13.482688
20.221033	850.099906	13.487693
20.263120	851.544065	13.492698
20.621064	871.572327	13.497703
20.653966	874.598163	13.502707
20.941316	874.523928	13.507712
20.675859	865.761547	13.512717
20.525999	848.392099	13.517722
20.453433	852.078189	13.522727
20.346031	851.800392	13.527731
20.326104	853.449997	13.532736
20.388192	872.702225	13.537741
20.466466	876.064624	13.542746
20.913272	882.352036	13.547751
20.529662	876.198021	13.552755
20.780749	876.787202	13.557760
20.239670	873.601091	13.562765
20.372773	875.309874	13.567770
20.630491	874.486533	13.572775
20.657973	877.089006	13.577779
20.659774	888.993904	13.582784
20.436194	887.099227	13.587789
20.543927	886.537942	13.592794
20.580117	885.814591	13.597799
20.809057	886.651749	13.602803
20.545162	865.654312	13.607808
20.540725	856.170595	13.612813
20.470829	854.577861	13.617818
20.516832	855.023120	13.622823
20.432598	862.819301	13.627827
20.894123	861.607040	13.632832
20.357305	859.364908	13.637837
20.361503	859.003075	13.642842
20.678676	864.320765	13.647847
20.470890	879.205022	13.652851
20.687958	869.657581	13.657856
20.628938	871.324462	13.662861
20.575252	848.871018	13.667866
20.349519	862.575331	13.672871
20.064687	868.365954	13.677875
20.891969	880.448291	13.682880
20.386644	887.236092	13.687885
20.754843	883.092771	13.692890
20.898497	881.152140	13.697895
20.329129	872.714211	13.702899
20.307993	867.560592	13.707904
20.367311	876.205996	13.712909
20.679224	883.325531	13.717914
20.751925	887.731255	13.722919
20.602879	880.230869	13.727923
20.621633	868.917213	13.732928
20.246971	871.413502	13.737933
20.337107	890.112465	13.742938
20.651477	891.041661	13.747943
20.601206	905.358314	13.752947
20.800760	892.739963	13.757952
20.392399	893.246652	13.762957
20.831346	888.002298	13.767962
20.300820	874.992592	13.772967
20.173179	880.706105	13.777971
20.657740	881.600271	13.782976
20.775265	892.108368	13.787981
20.802135	888.237118	13.792986
20.781917	873.056422	13.797991
20.378879	870.433382	13.802995
20.355289	856.661552	13.808000
20.449695	861.488034	13.813005
20.651088	869.520956	13.818010
20.580103	874.512602	13.823015
20.384077	881.448203	13.828019
20.784103	883.362013	13.833024
20.620136	870.096716	13.838029
20.455758	874.724764	13.843034
20.560056	862.096398	13.848039
20.287769	867.385094	13.853043
20.661165	875.103561	13.858048
20.438789	881.253259	13.863053
20.432446	889.461259	13.868058
20.858757	887.324148	13.873063
20.705508	889.893944	13.878067
20.646365	867.073887	13.883072
20.340388	871.593623	13.888077
20.561897	865.185395	13.893082
20.470331	854.482318	13.898087
20.185625	869.951305	13.903091
20.642239	883.581504	13.908096
20.420117	894.280977	13.913101
20.820166	893.691994	13.918106
20.832038	890.337258	13.923111
20.599613	871.003321	13.928115
20.373582	869.120076	13.933120
20.528915	866.754934	13.938125
20.306101	866.167516	13.943130
20.937535	871.515517	13.948135
20.843181	867.504324	13.953139
20.903702	865.692080	13.958144
20.537239	865.632231	13.963149
20.621448	866.172329	13.968154
20.309544	857.466249	13.973159
20.286586	863.708721	13.978163
20.406104	858.860699	13.983168
20.561089	859.490440	13.988173
20.297612	860.063912	13.993178
20.620094	856.104520	13.998183
20.522415	860.832320	14.003187
20.770970	862.790788	14.008192
20.570122	862.740960	14.013210
20.536863	862.513438	14.018227
20.670743	860.064880	14.023245
20.359522	865.086852	14.028263
20.603542	870.487461	14.033280
20.640317	869.970342	14.038298
20.616087	858.524089	14.043315
20.788892	861.084147	14.048333
20.900439	866.633298	14.053351
20.599515	856.052301	14.058368
20.553633	868.798012	14.063386
20.442830	870.396564	14.068403
20.646790	878.661765	14.073421
20.632764	892.360394	14.078439
21.159904	890.852704	14.083456
20.675034	896.883958	14.088474
20.768472	899.107467	14.093491
20.814915	899.938470	14.098509
21.032115	910.293715	14.103527
21.054913	905.113198	14.108544
20.674150	908.447398	14.113562
21.051837	909.434784	14.118579
21.183667	903.939573	14.123597
20.889289	901.897514	14.128615
20.882210	900.149410	14.133632
20.753543	904.203177	14.138650
20.911859	913.949614	14.143667
21.052521	906.148494	14.148685
20.817690	908.632002	14.153703
21.337556	910.763906	14.158720
21.031798	908.736245	14.163738
20.951179	906.436721	14.168755
21.093315	909.937636	14.173773
21.055965	913.446729	14.178791
21.385141	903.032617	14.183808
21.409436	910.349636	14.188826
21.086717	914.332109	14.193843
21.122703	913.780508	14.198861
21.198875	912.634182	14.203879
21.058691	909.527751	14.208896
21.056585	911.318185	14.213914
20.920318	917.043734	14.218931
21.049021	906.442942	14.223949
20.955209	906.906202	14.228967
21.151964	908.863121	14.233984
21.008104	919.939782	14.239002
21.159284	931.886476	14.244019
21.377019	930.357344	14.249037
21.534419	937.802586	14.254055
21.781455	937.407661	14.259072
21.747964	946.144932	14.264090
21.392852	926.607768	14.269107
21.645721	921.064931	14.274125
21.278569	919.770659	14.279143
21.305759	923.933282	14.284160
21.392409	936.442408	14.289178
21.384548	945.723009	14.294195
21.589711	943.555653	14.299213
21.572953	945.397192	14.304231
21.940291	947.301742	14.309248
21.749815	947.794578	14.314266
22.057462	944.160533	14.319283
22.050449	928.775731	14.324301
21.635993	927.784734	14.329319
21.596687	918.261519	14.334336
21.752110	912.705912	14.339354
21.406352	918.372065	14.344371
21.808074	918.628875	14.349389
21.584534	933.534444	14.354407
21.678398	928.962361	14.359424
21.748939	943.731374	14.364442
21.687128	949.849332	14.369459
21.722397	951.614934	14.374477
21.604127	950.988832	14.379495
21.678430	947.752229	14.384512
22.007857	945.572919	14.389530
21.724048	947.202219	14.394547
21.817969	952.389268	14.399565
21.466283	949.808924	14.404583
21.492408	938.357723	14.409600
22.094781	953.298329	14.414618
21.969630	958.175825	14.419635
22.171297	953.923171	14.424653
22.081147	947.606040	14.429671
21.937356	954.885396	14.434688
22.091902	971.577453	14.439706
22.040725	983.732645	14.444723
22.300433	969.060323	14.449741
22.082931	982.200024	14.454759
22.075731	975.712347	14.459776
22.319469	972.931639	14.464794
22.168397	978.938002	14.469811
22.598201	971.104890	14.474829
22.422431	975.155178	14.479847
22.096447	963.162360	14.484864
22.059326	963.865120	14.489882
22.026902	972.215268	14.494899
22.599901	976.294001	14.499917
22.215672	982.411485	14.504935
22.435837	971.052008	14.509952
22.569493	971.406631	14.514970
22.249732	981.978131	14.519987
22.375792	977.844496	14.525005
22.680255	979.038624	14.530023
22.579754	974.867192	14.535040
22.819801	983.834568	14.540058
22.629667	964.120029	14.545075
22.547388	970.486655	14.550093
22.562111	978.771084	14.555111
22.576372	975.451241	14.560128
22.725328	977.234894	14.565146
22.606969	980.434449	14.570163
22.465865	966.414374	14.575181
22.681837	972.481746	14.580199
22.594969	972.265918	14.585216
22.721196	974.032746	14.590234
22.623876	974.886682	14.595251
22.744051	973.519399	14.600269
22.685027	976.643422	14.605287
22.855516	980.256237	14.610304
22.997218	973.342112	14.615322
22.770347	979.756972	14.620339
22.740367	972.099438	14.625357
22.760825	982.769262	14.630375
22.975318	982.464471	14.635392
22.823917	972.971683	14.640410
22.581783	977.902450	14.645427
22.869126	969.351156	14.650445
22.723349	972.254631	14.655463
22.704588	966.056668	14.660480
22.921235	966.179401	14.665498
22.640995	974.704357	14.670515
22.993520	970.754831	14.675533
22.796351	974.003134	14.680551
22.836809	980.211761	14.685568
22.802717	973.862082	14.690586
22.685859	988.322824	14.695603
23.196023	996.551841	14.700621
22.810065	1002.826914	14.705639
23.037845	1005.769918	14.710656
22.986982	1007.604320	14.715674
22.785842	1008.256163	14.720691
23.210954	1000.151646	14.725709
23.368842	1001.938596	14.730727
23.326656	1005.391853	14.735744
23.314818	999.777946	14.740762
23.295293	1005.812104	14.745779
23.274086	995.936735	14.750797
23.297085	1005.218743	14.755815
23.460685	1002.041820	14.760832
23.636342	999.056458	14.765850
23.436567	1000.098198	14.770867
23.543851	1002.266032	14.775885
23.539597	1011.003397	14.780903
23.198466	1005.959540	14.785920
23.606862	993.652938	14.790938
23.342728	1003.613105	14.795955
23.326874	1004.084384	14.800973
23.700583	1006.187702	14.805991
23.573342	1008.076759	14.811008
23.650375	1005.627804	14.816026
23.587870	1002.952564	14.821043
23.500492	1002.277488	14.826061
23.857480	1001.413560	14.831079
23.712194	1014.647167	14.836096
23.924518	1009.017954	14.841114
23.944237	1008.503551	14.846131
23.587706	1010.795697	14.851149
23.728779	1009.758564	14.856167
23.577041	1010.618035	14.861184
23.905898	999.464573	14.866202
23.809663	1014.670823	14.871219
23.953433	1002.164170	14.876237
23.867961	1002.292616	14.881255
23.834873	1001.805512	14.886272
23.900511	1000.626252	14.891290
23.915308	1010.029123	14.896307
23.781101	1000.324359	14.901325
23.731481	1005.196116	14.906343
23.715333	1002.422246	14.911360
23.895071	1009.248901	14.916378
24.067848	1025.393839	14.921395
24.517705	1024.102960	14.926413
24.464640	1013.274673	14.931431
23.976234	1009.879262	14.936448
24.394046	998.074529	14.941466
24.063448	1000.449056	14.946483
24.071038	992.470910	14.951501
24.074415	998.259163	14.956519
23.793217	1002.077732	14.961536
24.028609	1007.026731	14.966554
24.290524	1017.318292	14.971571
24.674116	1021.678935	14.976589
24.289223	1010.337276	14.981607
24.103603	1008.389542	14.986624
24.385464	1014.301702	14.991642
24.446515	1021.303025	14.996659
24.530557	1014.387066	15.001677
24.647538	1004.326054	15.006695
24.102850	1007.450464	15.011712
24.689234	996.183571	15.016730
24.319106	1000.617228	15.021747
24.140771	1004.858272	15.026765
24.566256	1013.423279	15.031783
24.858525	1030.637713	15.036800
24.435586	1016.645237	15.041818
24.212387	1019.952758	15.046835
24.430450	1029.008613	15.051853
24.689274	1037.833026	15.056871
24.465361	1034.839025	15.061888
24.738090	1025.056758	15.066906
24.645165	1034.015922	15.071923
24.635741	1033.358299	15.076941
24.742845	1037.031575	15.081959
24.786974	1033.986959	15.086976
24.906356	1036.283431	15.091994
24.884149	1035.305371	15.097011
24.762576	1032.296621	15.102029
24.582103	1027.472528	15.107047
24.580919	1037.710110	15.112064
24.984261	1035.526864	15.117082
24.815264	1034.232437	15.122099
24.407564	1032.836080	15.127117
24.904573	1033.935008	15.132135
24.448796	1031.549005	15.137152
25.010455	1029.445904	15.142170
24.714802	1033.013526	15.147187
24.838203	1040.295927	15.152205
24.899562	1044.369764	15.157223
24.966175	1057.711189	15.162240
25.185205	1050.537726	15.167258
25.046559	1056.169325	15.172275
25.315330	1049.923896	15.177293
25.367889	1050.104261	15.182311
25.351856	1058.230044	15.187328
24.890614	1056.738402	15.192346
25.423716	1053.606356	15.197363
25.277482	1048.584883	15.202381
25.208518	1045.849316	15.207399
25.198603	1055.781558	15.212416
25.197620	1055.869787	15.217434
25.461542	1055.741159	15.222451
25.469591	1061.833864	15.227469
25.485815	1050.618539	15.232487
25.699038	1055.936039	15.237504
25.549365	1046.280902	15.242522
25.348613	1042.647692	15.247539
25.086094	1045.233168	15.252557
25.582207	1041.540726	15.257575
25.354847	1048.690309	15.262592
25.412197	1046.532355	15.267610
25.367731	1046.056502	15.272627
25.569607	1062.413921	15.277645
25.491684	1056.025579	15.282663
25.381757	1061.210572	15.287680
25.556188	1057.626061	15.292698
25.598383	1053.820391	15.297715
25.398408	1058.853002	15.302733
25.503274	1046.229818	15.307751
25.239770	1060.150868	15.312768
25.578212	1062.783646	15.317786
25.886161	1080.856100	15.322803
25.677211	1083.489669	15.327821
26.124592	1082.266821	15.332839
26.146392	1088.443863	15.337856
26.016712	1073.106788	15.342874
25.935111	1059.984786	15.347891
25.624610	1057.743924	15.352909
26.066808	1063.142886	15.357927
25.829085	1078.607726	15.362944
25.902967	1079.704929	15.367962
26.292005	1077.052042	15.372979
26.073590	1082.951209	15.377997
26.297107	1077.595469	15.383015
26.018417	1070.224520	15.388032
26.265609	1054.839941	15.393050
26.026559	1045.243106	15.398067
25.855487	1055.704427	15.403085
26.237032	1066.865718	15.408103
26.314729	1079.411003	15.413120
26.365055	1082.973794	15.418138
26.370241	1077.407480	15.423155
26.314194	1062.483397	15.428173
26.274827	1046.897561	15.433191
26.135462	1051.155999	15.438208
25.967446	1069.291766	15.443226
26.245728	1075.711046	15.448243
26.026907	1077.303252	15.453261
26.191671	1084.675036	15.458279
26.256323	1083.760200	15.463296
25.812344	1080.719488	15.468314
26.261104	1082.329494	15.473331
26.594274	1084.340188	15.478349
26.558627	1082.805833	15.483367
26.379086	1081.487915	15.488384
26.277936	1086.910622	15.493402
26.737265	1090.966619	15.498419
26.606815	1113.711798	15.503437
26.712076	1102.951003	15.508455
26.774081	1109.739854	15.513472
26.381045	1100.880136	15.518490
26.856437	1102.750170	15.523507
26.867751	1111.279042	15.528525
26.920161	1105.533722	15.533543
26.730624	1108.285324	15.538560
26.628760	1102.482811	15.543578
27.043818	1104.708541	15.548595
27.049226	1109.881449	15.553613
27.187921	1095.225154	15.558631
26.841576	1089.453773	15.563648
26.733712	1087.820823	15.568666
26.900400	1083.663375	15.573683
26.843669	1099.308587	15.578701
27.306481	1094.399178	15.583719
27.241069	1110.892091	15.588736
27.073318	1088.016685	15.593754
27.140047	1080.263445	15.598771
26.762922	1084.212167	15.603789
27.258404	1082.717375	15.608807
27.193249	1093.898021	15.613824
26.953062	1102.018679	15.618842
27.247341	1097.738629	15.623859
26.926538	1095.106140	15.628877
27.100379	1093.648488	15.633895
27.200759	1100.127613	15.638912
27.230702	1103.811640	15.643930
27.329307	1103.138358	15.648947
27.380291	1106.935435	15.653965
27.479562	1094.177819	15.658983
27.477446	1097.214139	15.664000
27.317687	1106.528506	15.669018
27.614054	1101.548111	15.674035
27.279511	1092.658620	15.679053
27.396392	1095.057749	15.684071
27.472275	1098.047021	15.689088
27.445302	1107.980446	15.694106
27.711517	1103.154300	15.699123
27.656388	1101.605748	15.704141
27.674822	1106.730959	15.709159
27.786336	1098.802248	15.714176
27.273916	1110.853354	15.719194
27.871605	1100.937409	15.724211
27.447952	1095.393864	15.729229
27.718851	1100.699035	15.734247
27.670366	1102.618015	15.739264
27.666497	1100.927578	15.744282
27.704616	1099.607977	15.749299
27.636033	1102.445682	15.754317
27.586103	1099.172229	15.759335
27.896804	1090.931750	15.764352
27.618880	1110.697481	15.769370
27.815479	1117.828245	15.774387
28.062479	1126.119759	15.779405
28.085897	1122.463360	15.784423
28.293640	1123.784614	15.789440
28.107834	1118.418636	15.794458
28.119074	1113.524611	15.799475
27.964615	1109.885574	15.804493
28.207578	1109.527475	15.809511
28.351241	1115.647339	15.814528
28.178643	1101.344287	15.819546
28.143910	1092.273269	15.824563
28.211830	1096.251691	15.829581
27.786033	1107.491438	15.834599
28.176208	1115.429769	15.839616
28.390740	1129.845663	15.844634
28.582060	1114.213525	15.849651
28.450109	1130.614824	15.854669
28.404977	1126.223727	15.859687
28.484811	1130.610827	15.864704
28.659611	1127.702656	15.869722
28.373946	1103.820396	15.874739
28.214494	1115.129357	15.879757
28.389102	1122.356442	15.884775
28.608326	1123.510693	15.889792
28.417152	1132.430530	15.894810
28.526450	1126.630510	15.899827
28.237250	1133.945730	15.904845
28.487458	1126.303204	15.909863
28.535080	1121.659783	15.914880
28.665778	1130.196368	15.919898
28.766295	1130.318748	15.924915
28.569862	1129.978817	15.929933
28.575929	1123.076816	15.934951
28.751463	1120.288082	15.939968
28.621125	1128.092353	15.944986
28.950075	1122.969898	15.950003
28.560636	1130.802910	15.955021
28.733686	1124.393386	15.960039
28.868154	1124.757322	15.965056
28.563852	1124.189197	15.970074
28.566352	1136.228987	15.975091
28.704365	1150.911943	15.980109
28.874675	1157.268254	15.985127
29.078817	1159.124927	15.990144
28.883168	1161.287615	15.995162
29.173227	1152.333076	16.000179
29.354291	1149.780988	16.005197
29.307124	1149.701974	16.010215
29.677263	1147.396590	16.015232
29.519009	1154.426661	16.020250
29.374052	1141.309970	16.025267
29.425434	1130.971463	16.030285
29.302521	1125.063756	16.035303
29.361930	1123.481203	16.040320
29.167920	1121.929629	16.045338
29.854895	1115.799948	16.050355
29.111753	1120.551113	16.055373
29.369142	1121.719727	16.060391
29.432706	1116.302966	16.065408
29.372324	1120.249946	16.070426
29.236021	1121.094377	16.075443
29.355638	1124.273313	16.080461
29.337227	1142.154071	16.085479
29.608926	1141.330481	16.090496
29.484793	1155.729627	16.095514
29.638523	1146.600203	16.100531
29.611937	1147.332753	16.105549
29.662185	1143.634317	16.110567
29.790173	1143.974117	16.115584
29.508187	1156.351886	16.120602
29.459851	1156.815766	16.125619
29.426160	1156.007847	16.130637
29.552454	1151.531199	16.135655
29.807796	1144.726287	16.140672
29.618303	1157.249758	16.145690
29.674872	1147.663909	16.150707
29.749972	1155.532959	16.155725
29.651521	1171.630080	16.160743
30.147241	1179.634985	16.165760
30.118735	1184.508154	16.170778
30.463016	1178.313550	16.175795
30.110168	1167.614759	16.180813
29.923389	1164.949870	16.185831
30.143826	1151.965234	16.190848
29.766956	1160.436494	16.195866
30.292244	1170.404581	16.200883
30.513820	1174.154019	16.205901
30.327772	1166.688019	16.210919
30.358546	1158.039105	16.215936
29.851505	1157.001506	16.220954
30.188850	1160.084375	16.225971
30.269148	1185.920160	16.230989
30.088067	1175.851511	16.236007
30.686103	1172.812907	16.241024
30.212275	1194.055642	16.246042
30.358525	1177.801396	16.251059
30.564250	1177.265187	16.256077
30.367008	1191.682321	16.261095
30.542152	1175.950446	16.266112
30.486879	1178.309404	16.271130
30.333229	1170.979810	16.276147
30.338203	1179.270628	16.281165
30.400374	1183.349094	16.286183
30.540862	1177.056428	16.291200
30.316736	1181.753150	16.296218
30.684214	1184.713239	16.301235
30.792695	1175.232353	16.306253
30.352547	1174.976909	16.311271
30.717821	1178.815119	16.316288
30.661617	1185.045542	16.321306
30.943536	1193.353548	16.326323
31.168998	1202.291925	16.331341
30.624556	1200.080486	16.336359
30.905161	1188.228269	16.341376
31.005362	1213.442714	16.346394
31.007405	1204.024405	16.351411
31.304882	1201.065193	16.356429
30.992951	1198.511496	16.361447
30.978228	1177.579451	16.366464
30.753261	1179.856932	16.371482
31.029477	1194.344853	16.376499
31.061269	1209.994942	16.381517
30.735898	1200.732676	16.386535
31.265045	1201.167378	16.391552
31.344902	1205.523036	16.396570
31.346365	1195.752457	16.401587
31.450113	1193.443933	16.406605
31.203292	1214.065311	16.411623
31.261501	1192.152602	16.416640
31.163275	1206.675085	16.421658
31.580933	1190.215513	16.426675
31.617508	1197.389143	16.431693
31.533419	1206.490153	16.436711
31.375076	1197.655867	16.441728
31.197383	1194.756709	16.446746
31.487727	1200.145335	16.451763
31.408742	1191.668067	16.456781
31.389159	1195.326982	16.461799
31.385866	1191.533250	16.466816
31.317719	1197.399059	16.471834
31.668271	1224.779037	16.476851
31.735159	1221.710302	16.481869
31.401317	1233.895053	16.486887
31.930329	1233.307281	16.491904
32.037887	1235.071614	16.496922
32.135909	1229.132561	16.501939
32.290973	1232.752619	16.506957
31.688982	1210.668315	16.511975
31.809668	1197.463587	16.516992
31.889144	1211.010747	16.522010
32.184797	1220.663125	16.527027
32.343817	1207.214741	16.532045
32.066755	1202.278575	16.537063
32.376745	1192.671157	16.542080
32.305158	1193.904829	16.547098
31.923326	1190.195066	16.552115
32.071390	1195.807735	16.557133
32.108890	1189.275079	16.562151
32.204242	1189.841889	16.567168
31.915156	1198.203212	16.572186
31.910642	1206.103865	16.577203
32.603117	1216.274988	16.582221
32.152342	1227.190039	16.587239
32.292807	1223.395394	16.592256
32.635354	1234.603936	16.597274
32.671406	1230.264355	16.602291
32.629003	1209.429490	16.607309
32.118702	1208.397126	16.612327
32.362807	1218.625602	16.617344
32.845535	1221.718333	16.622362
32.789418	1221.662769	16.627379
32.560803	1206.083348	16.632397
32.325796	1213.725028	16.637415
32.726098	1218.644653	16.642432
32.645807	1223.220918	16.647450
32.598884	1220.310338	16.652467
32.979088	1213.842568	16.657485
32.722721	1221.851038	16.662503
32.741199	1224.449932	16.667520
32.753761	1223.705421	16.672538
32.798203	1227.574363	16.677555
33.342812	1218.130862	16.682573
32.623013	1228.094639	16.687591
32.971949	1221.010489	16.692608
32.740481	1215.905021	16.697626
32.498093	1227.345276	16.702643
33.016105	1218.819971	16.707661
32.803564	1230.570084	16.712679
33.088244	1223.625173	16.717696
32.997517	1221.862055	16.722714
32.734766	1222.314513	16.727731
33.292876	1224.410480	16.732749
32.771450	1231.614916	16.737767
33.324621	1241.194777	16.742784
33.470295	1240.584770	16.747802
33.293763	1245.768653	16.752819
33.499236	1240.697312	16.757837
33.300047	1250.675605	16.762855
32.987638	1242.685434	16.767872
33.329014	1249.517886	16.772890
33.172438	1245.384420	16.777907
33.510452	1246.236584	16.782925
33.170209	1250.884205	16.787943
33.256406	1241.942462	16.792960
33.232321	1252.422954	16.797978
33.095398	1252.970181	16.802995
33.489993	1257.926123	16.808013
33.335618	1270.148352	16.813031
33.819230	1279.291791	16.818048
34.091804	1278.386255	16.823066
33.785831	1276.640942	16.828083
33.932925	1272.649379	16.833101
34.058037	1272.430414	16.838119
33.896762	1279.108658	16.843136
34.297718	1265.816695	16.848154
34.000636	1262.905104	16.853171
33.896663	1244.291751	16.858189
33.838008	1244.389967	16.863207
33.771601	1255.001484	16.868224
34.137979	1264.565532	16.873242
34.008270	1280.024370	16.878259
33.973527	1272.194399	16.883277
33.804932	1287.502925	16.888295
33.966704	1282.193140	16.893312
34.211413	1279.205361	16.898330
34.007653	1285.031483	16.903347
33.937145	1274.783889	16.908365
34.357982	1279.364409	16.913383
34.319959	1274.044018	16.918400
34.078223	1277.108366	16.923418
34.055440	1277.001080	16.928435
34.533045	1289.096576	16.933453
34.442191	1283.832586	16.938471
34.451062	1281.296926	16.943488
34.863492	1291.233545	16.948506
34.507935	1287.082250	16.953523
34.387165	1277.921015	16.958541
34.803714	1292.692617	16.963559
34.734080	1298.347911	16.968576
34.687790	1284.631741	16.973594
34.851197	1286.693136	16.978611
34.756273	1282.672527	16.983629
34.784244	1285.655322	16.988647
34.777314	1291.063078	16.993664
34.950914	1301.060604	16.998682
34.755727	1308.662948	17.003699
34.915037	1305.855531	17.008717
35.097216	1310.238947	17.013735
35.027759	1308.243543	17.018752
35.082953	1306.897604	17.023770
35.082017	1309.376910	17.028787
35.241713	1297.370849	17.033805
35.081090	1294.443780	17.038823
34.951374	1296.374954	17.043840
35.065530	1296.758651	17.048858
35.110093	1310.290235	17.053875
35.020370	1303.312187	17.058893
35.187984	1306.382831	17.063911
35.271415	1300.402816	17.068928
35.419906	1301.682412	17.073946
35.284783	1300.730208	17.078963
35.405754	1303.095686	17.083981
35.087696	1303.656858	17.088999
35.108324	1306.690380	17.094016
35.491722	1307.701270	17.099034
34.966418	1306.000372	17.104051
34.969567	1304.751613	17.109069
35.260933	1318.448343	17.114087
35.511398	1327.665178	17.119104
35.954260	1341.953630	17.124122
35.680471	1341.891881	17.129139
35.805640	1339.129229	17.134157
36.028366	1337.458470	17.139175
35.639788	1342.723398	17.144192
35.974542	1331.295028	17.149210
35.687782	1334.888832	17.154227
35.646868	1342.561761	17.159245
35.396650	1340.016286	17.164263
35.660526	1332.604290	17.169280
35.802043	1330.914235	17.174298
35.307310	1341.961441	17.179315
35.678829	1333.898324	17.184333
35.943618	1338.641395	17.189351
35.645575	1360.561077	17.194368
35.920151	1359.090479	17.199386
36.020799	1357.790772	17.204403
36.117991	1358.036385	17.209421
36.211805	1359.709326	17.214439
36.086577	1359.760742	17.219456
36.287658	1351.505352	17.224474
36.178735	1358.849350	17.229491
36.456259	1351.682141	17.234509
36.481397	1356.497260	17.239527
36.337329	1365.404221	17.244544
36.363110	1350.785341	17.249562
36.246404	1356.383668	17.254579
36.410244	1360.252480	17.259597
36.794872	1372.941770	17.264615
36.876380	1371.107905	17.269632
36.690196	1355.221097	17.274650
36.456948	1360.186756	17.279667
36.733432	1368.133133	17.284685
37.346689	1353.153919	17.289703
37.382594	1349.039278	17.294720
37.452882	1340.823631	17.299738
37.217879	1333.678395	17.304755
37.272547	1336.822903	17.309773
37.335382	1336.208013	17.314791
37.070973	1329.315230	17.319808
37.513631	1320.539180	17.324826
37.240696	1309.334377	17.329843
37.017616	1300.123375	17.334861
37.078259	1304.058968	17.339879
37.206582	1311.287237	17.344896
37.123147	1303.392653	17.349914
36.782083	1306.808701	17.354931
36.763068	1312.068163	17.359949
37.347778	1313.267178	17.364967
37.227854	1316.357727	17.369984
37.723374	1329.630998	17.375002
37.385965	1321.353750	17.380019
36.950140	1310.823821	17.385037
37.347351	1314.295952	17.390055
37.537007	1330.738210	17.395072
37.769223	1334.382957	17.400090
37.848280	1331.341360	17.405107
37.627590	1320.969029	17.410125
37.319665	1308.630896	17.415143
37.042490	1326.003358	17.420160
37.602868	1330.842434	17.425178
37.658854	1324.607228	17.430195
37.532524	1330.019097	17.435213
37.689537	1328.234545	17.440231
37.635444	1334.954711	17.445248
37.753262	1326.102259	17.450266
37.740073	1332.379370	17.455283
37.753375	1336.667814	17.460301
37.976618	1332.988146	17.465319
37.656893	1342.218846	17.470336
37.787854	1335.604363	17.475354
38.090576	1355.488614	17.480371
38.228068	1359.899622	17.485389
38.317286	1359.923916	17.490407
38.148776	1360.325954	17.495424
38.112397	1367.280846	17.500442
38.079222	1365.689436	17.505459
38.012756	1364.080526	17.510477
38.163164	1366.152658	17.515495
38.465069	1365.123672	17.520512
38.374162	1366.089083	17.525530
38.085961	1378.011048	17.530547
38.196677	1368.844298	17.535565
38.293934	1362.841603	17.540583
38.136535	1368.560474	17.545600
38.483074	1370.051532	17.550618
38.286678	1370.863874	17.555635
38.569031	1382.230788	17.560653
38.965376	1389.483207	17.565671
38.848971	1386.009497	17.570688
38.841484	1372.569425	17.575706
38.969952	1367.273572	17.580723
38.838596	1363.068408	17.585741
38.891758	1366.034617	17.590759
38.864900	1365.946857	17.595776
38.794638	1366.398509	17.600794
38.831463	1362.121690	17.605811
38.876539	1367.494437	17.610829
39.206852	1364.036794	17.615847
39.040241	1373.866824	17.620864
39.252341	1367.384110	17.625882
39.048824	1358.061408	17.630899
39.187936	1366.174418	17.635917
39.113009	1362.617017	17.640935
39.095840	1373.692693	17.645952
39.198553	1385.268378	17.650970
39.482437	1395.548054	17.655987
39.247759	1394.057994	17.661005
39.373186	1379.832983	17.666023
39.224000	1396.489024	17.671040
39.429363	1389.138243	17.676058
39.567332	1382.983536	17.681075
39.186949	1388.122899	17.686093
39.454733	1387.108792	17.691111
39.266993	1392.033382	17.696128
39.227630	1389.971030	17.701146
39.162741	1390.894539	17.706163
38.787860	1402.468538	17.711181
39.570730	1414.797825	17.716199
39.570594	1419.756214	17.721216
39.842189	1410.507149	17.726234
40.157587	1422.268389	17.731251
39.855724	1419.196285	17.736269
39.940350	1417.564059	17.741287
39.792674	1423.316795	17.746304
40.065882	1417.778394	17.751322
40.361427	1415.315759	17.756339
40.143217	1409.794384	17.761357
40.249247	1410.191178	17.766375
40.009925	1409.582002	17.771392
40.135875	1406.871125	17.776410
40.298997	1404.450848	17.781427
40.259384	1408.920792	17.786445
40.365107	1401.168241	17.791463
40.729996	1409.324708	17.796480
40.412696	1408.717742	17.801498
40.615197	1411.857567	17.806515
40.737172	1409.017543	17.811533
40.862735	1409.356952	17.816551
40.464100	1410.148064	17.821568
40.630707	1409.831240	17.826586
40.716634	1411.150713	17.831603
40.319725	1409.327859	17.836621
40.562954	1402.447679	17.841639
40.525053	1406.784424	17.846656
40.652528	1404.225108	17.851674
40.862311	1407.409390	17.856691
40.794334	1410.549878	17.861709
40.973104	1405.343520	17.866727
40.564999	1405.713768	17.871744
40.284699	1404.427619	17.876762
40.766126	1395.998500	17.881779
40.644434	1418.992094	17.886797
40.929794	1415.965557	17.891815
41.286311	1422.041380	17.896832
41.234745	1429.852913	17.901850
41.280820	1420.174959	17.906867
40.869045	1428.566992	17.911885
41.250066	1417.205898	17.916903
40.973986	1427.983120	17.921920
41.334803	1425.081405	17.926938
41.595668	1421.019746	17.931955
41.366800	1435.335194	17.936973
41.354846	1429.894179	17.941991
41.047695	1423.753813	17.947008
41.297803	1427.374494	17.952026
41.584926	1426.601129	17.957043
41.424594	1428.144716	17.962061
41.505391	1421.238521	17.967079
41.270351	1425.215011	17.972096
41.554843	1424.735448	17.977114
42.007539	1437.693165	17.982131
41.491999	1445.772979	17.987149
41.762300	1452.028526	17.992167
41.767623	1440.102027	17.997184
41.795429	1449.489737	18.002202
41.898352	1453.365929	18.007219
41.882482	1444.012459	18.012237
41.957008	1451.531748	18.017255
41.933557	1456.126550	18.022272
42.034503	1456.845069	18.027290
42.365477	1442.552607	18.032307
42.058880	1447.876074	18.037325
42.314915	1446.211002	18.042343
42.170335	1452.192927	18.047360
41.930338	1451.371488	18.052378
42.117301	1450.982200	18.057395
42.041771	1444.644430	18.062413
42.299516	1456.388150	18.067431
42.188064	1463.863957	18.072448
42.190117	1477.812268	18.077466
42.777100	1468.220272	18.082483
42.310730	1481.791813	18.087501
42.405678	1474.368146	18.092519
42.423206	1468.562175	18.097536
42.423345	1476.797303	18.102554
42.897388	1473.414244	18.107571
42.722923	1480.369975	18.112589
42.546772	1478.803715	18.117607
42.350997	1483.588038	18.122624
42.652400	1488.257676	18.127642
43.291571	1501.743374	18.132659
43.160431	1510.742747	18.137677
43.241811	1502.955483	18.142695
43.299136	1481.157316	18.147712
42.882856	1479.136186	18.152730
42.964619	1473.229516	18.157747
43.016339	1479.613534	18.162765
43.349875	1493.442138	18.167783
43.314850	1499.574145	18.172800
43.113915	1497.406192	18.177818
43.411993	1496.040378	18.182835
43.491946	1502.722725	18.187853
43.360494	1494.963902	18.192871
43.458987	1492.016705	18.197888
43.861965	1497.857051	18.202906
43.543613	1495.139934	18.207923
43.405375	1482.895719	18.212941
43.670760	1497.836365	18.217959
43.813874	1496.199522	18.222976
43.376880	1503.407141	18.227994
43.494161	1495.376618	18.233011
43.625414	1490.788958	18.238029
43.750257	1487.299558	18.243047
43.929664	1478.672369	18.248064
43.815371	1499.066938	18.253082
43.831293	1488.309882	18.258099
43.771495	1506.132404	18.263117
43.684661	1493.536259	18.268135
43.862983	1491.475357	18.273152
43.771327	1507.106914	18.278170
44.325347	1500.703325	18.283187
44.330011	1508.234572	18.288205
43.695612	1501.939499	18.293223
44.060177	1509.369302	18.298240
44.179500	1532.706115	18.303258
44.696550	1523.244006	18.308275
44.249396	1523.688126	18.313293
44.547122	1517.935768	18.318311
44.709035	1516.125244	18.323328
44.717938	1516.004250	18.328346
44.740158	1522.780762	18.333363
44.794886	1517.225255	18.338381
44.562112	1523.911867	18.343399
44.773875	1519.183150	18.348416
44.546563	1515.134037	18.353434
44.538466	1513.693562	18.358451
44.622860	1522.263720	18.363469
44.553333	1520.365043	18.368487
44.788291	1522.337193	18.373504
44.785360	1525.377665	18.378522
44.860539	1513.449403	18.383539
44.700518	1519.438537	18.388557
44.716535	1517.152606	18.393575
45.174854	1536.375971	18.398592
45.019647	1547.377048	18.403610
45.407911	1547.212070	18.408627
45.344815	1552.800350	18.413645
45.362110	1553.502325	18.418663
45.397785	1548.508298	18.423680
44.893436	1559.303930	18.428698
45.360794	1552.524796	18.433715
45.365394	1547.846413	18.438733
44.987777	1553.692503	18.443751
45.613753	1551.498062	18.448768
45.319800	1552.421931	18.453786
45.621013	1550.003991	18.458803
45.182399	1553.504082	18.463821
45.397228	1552.746174	18.468839
45.703965	1548.113992	18.473856
45.651814	1566.655065	18.478874
45.836546	1573.346691	18.483891
45.822962	1572.836006	18.488909
46.015325	1576.581557	18.493927
46.200862	1573.439554	18.498944
46.180771	1581.557624	18.503962
46.177735	1571.218831	18.508979
46.044062	1561.899016	18.513997
45.849215	1561.577697	18.519015
46.159808	1563.411155	18.524032
46.036178	1575.797058	18.529050
46.348773	1573.366287	18.534067
46.323957	1576.337110	18.539085
46.390372	1580.149942	18.544103
46.220917	1572.122631	18.549120
46.428367	1581.317386	18.554138
46.481608	1576.784615	18.559155
46.399100	1577.323174	18.564173
46.487828	1579.327305	18.569191
46.565837	1568.036443	18.574208
46.060728	1578.745690	18.579226
46.601325	1571.771599	18.584243
46.596877	1567.263762	18.589261
46.490393	1573.362364	18.594279
46.920354	1594.946846	18.599296
46.588967	1597.200460	18.604314
46.881520	1604.217057	18.609331
47.031934	1603.833595	18.614349
46.743546	1611.089144	18.619367
47.143162	1607.270375	18.624384
47.174354	1610.299130	18.629402
47.267541	1609.242063	18.634419
47.194291	1604.367641	18.639437
47.009759	1613.028720	18.644455
47.330607	1600.559385	18.649472
47.174820	1600.128796	18.654490
47.315607	1598.333429	18.659507
47.471034	1590.354188	18.664525
47.014230	1598.022001	18.669543
47.351156	1603.036029	18.674560
47.140175	1601.312493	18.679578
47.187756	1615.201762	18.684595
47.638607	1623.600272	18.689613
47.303548	1635.106752	18.694631
47.600687	1630.255053	18.699648
47.511484	1642.166733	18.704666
47.579316	1630.295393	18.709683
47.853025	1638.790594	18.714701
47.658131	1637.305961	18.719719
47.819223	1629.360404	18.724736
47.730832	1636.348888	18.729754
47.806816	1637.973579	18.734771
48.136624	1651.315263	18.739789
48.106939	1656.737795	18.744807
48.268183	1652.255420	18.749824
47.877190	1666.048718	18.754842
47.771377	1658.820579	18.759859
47.805736	1659.512759	18.764877
47.609995	1651.926923	18.769895
48.021061	1659.070946	18.774912
48.101983	1671.674434	18.779930
48.118148	1674.088149	18.784947
48.341941	1684.369749	18.789965
48.568830	1688.731993	18.794983
48.658577	1679.348156	18.800000
48.851156	1686.464898	18.805018
48.442269	1686.752686	18.810035
48.900575	1678.940611	18.815053
48.767060	1690.298581	18.820071
48.919672	1676.741454	18.825088
48.911692	1682.509768	18.830106
48.904030	1687.795084	18.835123
49.203347	1684.570414	18.840141
48.858526	1683.786128	18.845159
49.154375	1680.893940	18.850176
49.013549	1693.483258	18.855194
49.078636	1672.234947	18.860211
49.337326	1673.952420	18.865229
48.795838	1675.766831	18.870247
49.362947	1690.176609	18.875264
49.578383	1697.125320	18.880282
49.620827	1697.875992	18.885299
49.451075	1684.139807	18.890317
49.485317	1689.932852	18.895335
49.743131	1681.901837	18.900352
49.806052	1686.088870	18.905370
49.566394	1674.887129	18.910387
49.606666	1666.621026	18.915405
49.545749	1692.289099	18.920423
49.955836	1698.464255	18.925440
49.802127	1698.572126	18.930458
49.651593	1712.331839	18.935475
49.926890	1701.196612	18.940493
50.055928	1704.898024	18.945511
50.228526	1700.446072	18.950528
49.828595	1710.543214	18.955546
49.859609	1713.843382	18.960563
50.236193	1700.628065	18.965581
50.006850	1714.410573	18.970599
50.301891	1702.900152	18.975616
50.230115	1698.250419	18.980634
50.051222	1711.900603	18.985651
50.444573	1699.127806	18.990669
50.265288	1702.294760	18.995687
50.205621	1706.376286	19.000704
50.430767	1697.383002	19.005722
50.278700	1717.157011	19.010739
50.926895	1714.565723	19.015757
50.669534	1719.105098	19.020775
50.571820	1731.602624	19.025792
50.852179	1732.493118	19.030810
50.861789	1730.069741	19.035827
51.059215	1729.847889	19.040845
51.089360	1730.773568	19.045863
50.929857	1718.735478	19.050880
51.037834	1718.656101	19.055898
51.047309	1721.361133	19.060915
51.121363	1719.758876	19.065933
50.958835	1734.458104	19.070951
51.304764	1723.385534	19.075968
51.176691	1730.187684	19.080986
51.097969	1727.447251	19.086003
51.150587	1720.169431	19.091021
51.272823	1730.486138	19.096039
51.355523	1717.014060	19.101056
51.271015	1736.579107	19.106074
51.204868	1730.784803	19.111091
51.175963	1728.872542	19.116109
51.205484	1743.050335	19.121127
51.454353	1753.501029	19.126144
51.696896	1758.767706	19.131162
51.308993	1764.171111	19.136179
51.571505	1756.413030	19.141197
51.615022	1764.155305	19.146215
51.455884	1756.486493	19.151232
52.059721	1770.651379	19.156250
52.525401	1778.761306	19.161267
52.799689	1760.548681	19.166285
52.262570	1760.644548	19.171303
52.559318	1755.169911	19.176320
52.246297	1750.498070	19.181338
51.895355	1756.515389	19.186355
52.098300	1743.009953	19.191373
52.411648	1743.152671	19.196391
52.502407	1748.240617	19.201408
52.538744	1741.015723	19.206426
52.286070	1754.448823	19.211443
52.787913	1759.460989	19.216461
52.709977	1765.374994	19.221479
52.761051	1767.820913	19.226496
52.950684	1763.410274	19.231514
52.536257	1754.841444	19.236531
52.751203	1757.616754	19.241549
52.690150	1773.643291	19.246567
52.640989	1781.496316	19.251584
53.155030	1766.797579	19.256602
52.905137	1777.246816	19.261619
53.037546	1767.230012	19.266637
53.043604	1770.190445	19.271655
53.018491	1768.685014	19.276672
53.366176	1763.575083	19.281690
52.956087	1775.509730	19.286707
53.165198	1761.280441	19.291725
52.920837	1771.963188	19.296743
53.242687	1767.843728	19.301760
53.277993	1778.181411	19.306778
53.476868	1800.384324	19.311795
53.794625	1796.314276	19.316813
53.801793	1798.823049	19.321831
53.976716	1798.240605	19.326848
53.944038	1774.965022	19.331866
53.675569	1774.171701	19.336883
53.839567	1763.064402	19.341901
53.710990	1773.088422	19.346919
53.992863	1785.234429	19.351936
54.377028	1783.934304	19.356954
53.904299	1789.848355	19.361971
54.227458	1784.979084	19.366989
54.481964	1794.282096	19.372007
53.932681	1777.105344	19.377024
54.377952	1779.224113	19.382042
54.440690	1792.308051	19.387059
54.289659	1788.350522	19.392077
54.814660	1790.287466	19.397095
54.143367	1781.966452	19.402112
54.496124	1779.023481	19.407130
54.214410	1798.296782	19.412147
54.409077	1787.493695	19.417165
54.267832	1792.094804	19.422183
54.602754	1791.558421	19.427200
54.746672	1785.030551	19.432218
54.489770	1792.556466	19.437235
54.560882	1776.951441	19.442253
54.693820	1789.519992	19.447271
54.646260	1797.408953	19.452288
54.972108	1802.007938	19.457306
54.951398	1818.447330	19.462323
55.099598	1807.892328	19.467341
55.110237	1814.989382	19.472359
55.408245	1815.000045	19.477376
55.331814	1810.014367	19.482394
55.316727	1809.319070	19.487411
55.554942	1807.614327	19.492429
55.397385	1809.851263	19.497447
55.250796	1807.778421	19.502464
55.343065	1814.274105	19.507482
55.179254	1812.447059	19.512499
55.378600	1805.632682	19.517517
55.703666	1826.188890	19.522535
55.452803	1840.561729	19.527552
55.744753	1838.676940	19.532570
55.784251	1832.816194	19.537587
55.746434	1839.482083	19.542605
55.760917	1840.753210	19.547623
55.622804	1840.607679	19.552640
55.854591	1833.874638	19.557658
55.621742	1834.491455	19.562675
55.881306	1845.981927	19.567693
56.234855	1854.154614	19.572711
55.979454	1872.940077	19.577728
56.395144	1868.195245	19.582746
56.233827	1866.279698	19.587763
56.233360	1865.586786	19.592781
56.224658	1860.139586	19.597799
56.140208	1863.612371	19.602816
56.414915	1862.006415	19.607834
56.373323	1871.929321	19.612851
56.655597	1882.245783	19.617869
57.226730	1886.918158	19.622887
56.909111	1876.888885	19.627904
56.990786	1855.127177	19.632922
57.260634	1851.040371	19.637939
57.149298	1853.398153	19.642957
57.285542	1840.038555	19.647975
57.573348	1839.514405	19.652992
57.630599	1835.065863	19.658010
57.497258	1838.763532	19.663027
57.549002	1838.967635	19.668045
57.619790	1837.394990	19.673063
57.767004	1838.186380	19.678080
57.888776	1831.983727	19.683098
57.394274	1826.558167	19.688115
57.531547	1828.871578	19.693133
57.601969	1837.699785	19.698151
57.324006	1846.357811	19.703168
57.846745	1838.199512	19.708186
57.619480	1840.199014	19.713203
57.711256	1833.904396	19.718221
57.994520	1842.725406	19.723239
58.005375	1844.571308	19.728256
58.079590	1837.805974	19.733274
57.814701	1838.961195	19.738291
57.929260	1833.841223	19.743309
58.230274	1844.077587	19.748327
57.939054	1839.587083	19.753344
58.139995	1830.361607	19.758362
57.886874	1833.379903	19.763379
57.628856	1845.049665	19.768397
58.452508	1857.299683	19.773415
58.338714	1867.074426	19.778432
58.405962	1870.866751	19.783450
58.323622	1872.370416	19.788467
58.361628	1876.157180	19.793485
58.317667	1877.359760	19.798503
58.293275	1877.223623	19.803520
58.962491	1879.766051	19.808538
58.726320	1892.794708	19.813555
58.598899	1903.521828	19.818573
58.786909	1901.583603	19.823591
58.505846	1903.855193	19.828608
58.922744	1898.521804	19.833626
58.860081	1899.751752	19.838643
58.796127	1904.168310	19.843661
58.825620	1898.700059	19.848679
58.653674	1922.732084	19.853696
59.133853	1929.833758	19.858714
59.240319	1933.285552	19.863731
59.145058	1943.288643	19.868749
59.484831	1941.575554	19.873767
59.093639	1942.082337	19.878784
59.517906	1941.587548	19.883802
59.862656	1960.644744	19.888819
59.762086	1967.613305	19.893837
60.021502	1955.953413	19.898855
59.769734	1969.225317	19.903872
59.942467	1959.663671	19.908890
60.185175	1957.318708	19.913907
60.188945	1961.284788	19.918925
60.207038	1954.625100	19.923943
59.869229	1959.173444	19.928960
60.353325	1957.886472	19.933978
60.559834	1962.386554	19.938995
60.491654	1952.280480	19.944013
60.385342	1955.638787	19.949031
60.271530	1961.745798	19.954048
60.352719	1948.108567	19.959066
60.579401	1958.968821	19.964083
60.413717	1948.893244	19.969101
60.594719	1948.959536	19.974119
60.724372	1949.284148	19.979136
60.765357	1943.634709	19.984154
60.473466	1951.230783	19.989171
60.726724	1950.134007	19.994189
60.879910	1945.574170	19.999207
60.667595	1955.685607	20.004224
60.854870	1965.941768	20.009242
61.017258	1984.366568	20.014259
60.608930	1988.672889	20.019277
61.046022	1981.063043	20.024295
61.003687	1987.186982	20.029312
60.941305	1981.834034	20.034330
60.981706	1996.765453	20.039347
61.222849	2016.488958	20.044365
61.447530	2004.535667	20.049383
61.568123	2014.895312	20.054400
61.968771	2008.349212	20.059418
62.029759	2008.089336	20.064435
61.754085	2014.495911	20.069453
62.097363	2005.021092	20.074471
61.787974	2005.889241	20.079488
61.888493	2003.584252	20.084506
61.908800	2012.034347	20.089523
61.870674	2004.394873	20.094541
62.380523	1996.101679	20.099559
61.911290	2011.445536	20.104576
61.976677	2004.520285	20.109594
62.219211	2009.830318	20.114611
61.787911	2016.934236	20.119629
61.961735	2022.957646	20.124647
62.029300	2034.887908	20.129664
62.152123	2038.176655	20.134682
62.497349	2038.061803	20.139699
62.624926	2042.764850	20.144717
62.959462	2036.691002	20.149735
62.301731	2048.378261	20.154752
62.797827	2056.001322	20.159770
62.977082	2058.720243	20.164787
62.754069	2065.341044	20.169805
63.033773	2059.878452	20.174823
63.044057	2057.666503	20.179840
62.912004	2068.020856	20.184858
63.373782	2055.022102	20.189875
62.910308	2061.634054	20.194893
63.250190	2054.848277	20.199911
63.178598	2063.448350	20.204928
62.874927	2061.804824	20.209946
63.496359	2070.316406	20.214963
63.376825	2078.933571	20.219981
63.837864	2084.289804	20.224999
64.412268	2084.054239	20.230016
64.139636	2074.765694	20.235034
64.108664	2061.208385	20.240051
63.635576	2058.997222	20.245069
63.847719	2051.276910	20.250087
64.295615	2064.239890	20.255104
64.013633	2058.039390	20.260122
64.177463	2068.130247	20.265139
63.874109	2080.772561	20.270157
64.529030	2076.709235	20.275175
64.341119	2076.914592	20.280192
64.530437	2089.007969	20.285210
64.874966	2076.418040	20.290227
64.662761	2078.966564	20.295245
64.872273	2059.232424	20.300263
64.435141	2056.698536	20.305280
64.306852	2067.502212	20.310298
64.768669	2064.298741	20.315315
64.584934	2072.947379	20.320333
64.811191	2067.230590	20.325351
64.703866	2069.657772	20.330368
64.577631	2076.117627	20.335386
64.391771	2065.830450	20.340403
64.750774	2081.776178	20.345421
64.924196	2094.568219	20.350439
64.896172	2098.701443	20.355456
64.859099	2091.926996	20.360474
64.897071	2094.537882	20.365491
64.992520	2108.534829	20.370509
65.518989	2126.775895	20.375527
65.445670	2131.836654	20.380544
65.480855	2131.285136	20.385562
65.900744	2125.146512	20.390579
65.669058	2141.208530	20.395597
66.080734	2126.588686	20.400615
65.870429	2131.178889	20.405632
65.737118	2136.049424	20.410650
66.037893	2128.211894	20.415667
65.948551	2123.085010	20.420685
65.958729	2127.188552	20.425703
66.036921	2130.406566	20.430720
66.008589	2122.697035	20.435738
66.270053	2120.261746	20.440755
66.050525	2135.134076	20.445773
65.881358	2130.325114	20.450791
66.212502	2149.098411	20.455808
65.785010	2140.566044	20.460826
66.066700	2159.183630	20.465843
66.198368	2157.694846	20.470861
66.486015	2170.980806	20.475879
66.282507	2189.891333	20.480896
66.418184	2190.943370	20.485914
66.561624	2186.388946	20.490931
66.794659	2195.027041	20.495949
67.078291	2192.241320	20.500967
67.363902	2197.536686	20.505984
67.002852	2212.653481	20.511002
67.295661	2214.426935	20.516019
67.338528	2215.777734	20.521037
67.567207	2212.553203	20.526055
67.830936	2209.153967	20.531072
67.765754	2220.347279	20.536090
67.613552	2209.524471	20.541107
67.677933	2216.437741	20.546125
67.682303	2210.877416	20.551143
68.003455	2210.331419	20.556160
67.961893	2218.972416	20.561178
68.191927	2203.848941	20.566195
68.001500	2205.398194	20.571213
67.894990	2207.817403	20.576231
68.246882	2200.084952	20.581248
67.905793	2208.341872	20.586266
68.312736	2199.673254	20.591283
68.030768	2208.209424	20.596301
68.258282	2206.751758	20.601319
68.271915	2206.851823	20.606336
68.341700	2216.654944	20.611354
68.243674	2209.912974	20.616371
68.330557	2224.583146	20.621389
68.243253	2232.366983	20.626407
68.572262	2234.689213	20.631424
68.558393	2237.069268	20.636442
68.679927	2236.167315	20.641459
68.576756	2234.757663	20.646477
68.537177	2234.239301	20.651495
68.753394	2244.975583	20.656512
68.826550	2260.749994	20.661530
69.044241	2260.637388	20.666547
69.214586	2268.253515	20.671565
69.375179	2259.871138	20.676583
69.189777	2267.343416	20.681600
69.011847	2267.189284	20.686618
69.118694	2276.230620	20.691635
69.291163	2295.399109	20.696653
69.161770	2294.327934	20.701671
69.779266	2301.462956	20.706688
69.515198	2302.569310	20.711706
69.774865	2296.712597	20.716723
70.143404	2289.616159	20.721741
69.884762	2297.271609	20.726759
70.106271	2291.377720	20.731776
70.092739	2298.170520	20.736794
70.479967	2297.224619	20.741811
70.284295	2304.253342	20.746829
70.313273	2311.877091	20.751847
70.476143	2308.664608	20.756864
70.332529	2315.597722	20.761882
70.412209	2317.796901	20.766899
70.756827	2321.095966	20.771917
70.722786	2317.110982	20.776935
71.034361	2316.314012	20.781952
70.876143	2315.832659	20.786970
70.788166	2311.093282	20.791987
70.515017	2317.339119	20.797005
70.343455	2323.534149	20.802023
70.974651	2323.461791	20.807040
71.052163	2338.791952	20.812058
71.380267	2343.727414	20.817075
71.190958	2344.806118	20.822093
71.340184	2356.113222	20.827111
71.571917	2343.347550	20.832128
71.326342	2348.433494	20.837146
71.379363	2347.942051	20.842163
71.661363	2345.181732	20.847181
71.157758	2352.237560	20.852199
71.954322	2342.882168	20.857216
71.549466	2360.343077	20.862234
72.346840	2360.841245	20.867251
72.058216	2368.371725	20.872269
71.972506	2378.661485	20.877287
72.310191	2377.701456	20.882304
72.221985	2375.769461	20.887322
72.742439	2373.625561	20.892339
72.367118	2379.569146	20.897357
72.420182	2386.398563	20.902375
72.737103	2377.508217	20.907392
72.432181	2378.956183	20.912410
72.720763	2377.307059	20.917427
72.773710	2372.003222	20.922445
72.483910	2386.238070	20.927463
72.915423	2385.909661	20.932480
72.597543	2383.601328	20.937498
72.706569	2377.037070	20.942515
72.666267	2377.612976	20.947533
72.692780	2377.893478	20.952551
73.127919	2373.302705	20.957568
72.826223	2379.710441	20.962586
72.920102	2396.096026	20.967603
73.296140	2397.345728	20.972621
73.406563	2396.051452	20.977639
73.627160	2402.625259	20.982656
73.442748	2404.896457	20.987674
73.581129	2398.171761	20.992691
73.413308	2392.538142	20.997709
73.532795	2398.436651	21.002727
73.717161	2405.744628	21.007744
73.730391	2423.688773	21.012762
74.004834	2426.232905	21.017779
73.934704	2425.224636	21.022797
73.695042	2434.886108	21.027815
74.011783	2417.655442	21.032832
74.006112	2434.695665	21.037850
74.324469	2438.407977	21.042867
74.639596	2455.632260	21.047885
74.381422	2465.026113	21.052903
74.692963	2458.140054	21.057920
74.691162	2457.006830	21.062938
74.654380	2453.479262	21.067955
74.698537	2456.572200	21.072973
74.468589	2466.284846	21.077991
74.820522	2463.440986	21.083008
74.556825	2461.508649	21.088026
74.791036	2463.461385	21.093043
75.304903	2484.853680	21.098061
75.194837	2484.035055	21.103079
75.091570	2479.069160	21.108096
75.093669	2485.566937	21.113114
75.027064	2491.527411	21.118131
75.287760	2492.745173	21.123149
74.870076	2496.390025	21.128167
75.573525	2496.434362	21.133184
75.602796	2508.541025	21.138202
75.689817	2504.544551	21.143219
75.832291	2511.317291	21.148237
75.804105	2516.923182	21.153255
76.178831	2506.633610	21.158272
76.096254	2509.709799	21.163290
76.141911	2510.530009	21.168307
76.590162	2500.862720	21.173325
76.200635	2512.310135	21.178343
76.604297	2519.729507	21.183360
76.548820	2534.679126	21.188378
76.693331	2530.980253	21.193395
77.036461	2524.250380	21.198413
76.529562	2511.645613	21.203431
76.901603	2512.813370	21.208448
76.736644	2513.916520	21.213466
77.006076	2522.829038	21.218483
77.216697	2523.601703	21.223501
77.235365	2532.077532	21.228519
77.057439	2518.358381	21.233536
77.089515	2520.060968	21.238554
77.115498	2517.453143	21.243571
77.140687	2519.742063	21.248589
77.121080	2520.965196	21.253607
77.169181	2525.469477	21.258624
77.504865	2537.409310	21.263642
77.294151	2524.128016	21.268659
77.644994	2541.412780	21.273677
77.598846	2558.229912	21.278695
77.703330	2565.939293	21.283712
77.666978	2570.376821	21.288730
77.579350	2561.409289	21.293747
78.178341	2552.324402	21.298765
77.995287	2558.683404	21.303783
78.208496	2559.229903	21.308800
78.639738	2575.342427	21.313818
78.688428	2577.724361	21.318835
79.093843	2571.420315	21.323853
79.020873	2558.707766	21.328871
79.332814	2535.227345	21.333888
79.117079	2545.552903	21.338906
79.284154	2527.367436	21.343923
79.180967	2533.354999	21.348941
79.219593	2539.905185	21.353959
79.293379	2536.270292	21.358976
79.337093	2530.188344	21.363994
79.278172	2533.119177	21.369011
79.627765	2526.455134	21.374029
79.295180	2532.861568	21.379047
79.762112	2526.911930	21.384064
79.269299	2524.956338	21.389082
79.104817	2527.795452	21.394099
79.480077	2530.250371	21.399117
79.145274	2528.938982	21.404135
79.448694	2528.219604	21.409152
79.966081	2545.536811	21.414170
79.669995	2553.269946	21.419187
79.553730	2558.144195	21.424205
79.691802	2555.589284	21.429223
79.788327	2548.277306	21.434240
79.713515	2562.975963	21.439258
79.983185	2581.385983	21.444275
80.435150	2587.038831	21.449293
80.074224	2593.296422	21.454311
80.605159	2591.322302	21.459328
80.714308	2593.198247	21.464346
80.457523	2594.316046	21.469363
80.677572	2595.583563	21.474381
80.728874	2612.474891	21.479399
80.809511	2605.845836	21.484416
80.637958	2620.626053	21.489434
80.659168	2620.326887	21.494451
80.815877	2612.926619	21.499469
80.615383	2623.545566	21.504487
80.907808	2633.333916	21.509504
81.503685	2644.994789	21.514522
81.187985	2645.508429	21.519539
81.589611	2651.111907	21.524557
81.392436	2660.393110	21.529575
81.562709	2655.831117	21.534592
81.529007	2647.634465	21.539610
81.834714	2677.926936	21.544627
81.953005	2672.108352	21.549645
82.087861	2676.892252	21.554663
82.246293	2675.500621	21.559680
82.319772	2673.564042	21.564698
82.063161	2675.644634	21.569715
82.448782	2666.106790	21.574733
82.176473	2674.736869	21.579751
82.251453	2665.601751	21.584768
82.524490	2670.302258	21.589786
82.178269	2687.510354	21.594803
82.835402	2691.311873	21.599821
82.650446	2700.543170	21.604839
82.827470	2696.835138	21.609856
83.040350	2689.274057	21.614874
82.981960	2695.091713	21.619891
83.312444	2689.080388	21.624909
83.150657	2700.137655	21.629927
83.223160	2695.988481	21.634944
83.176746	2699.664637	21.639962
83.045197	2717.843043	21.644979
83.533403	2714.149886	21.649997
83.456919	2722.761351	21.655015
83.940130	2713.097002	21.660032
84.013858	2724.326757	21.665050
84.315818	2736.915584	21.670067
84.332496	2727.479798	21.675085
83.845305	2724.366168	21.680103
84.015393	2712.704188	21.685120
84.393514	2712.077510	21.690138
83.905697	2725.916344	21.695155
84.191223	2710.468066	21.700173
84.171978	2734.532922	21.705191
84.085864	2747.886092	21.710208
84.596123	2742.793952	21.715226
84.619667	2743.882791	21.720243
84.712647	2738.253859	21.725261
84.617583	2745.469695	21.730279
84.947243	2750.561587	21.735296
85.578578	2762.694378	21.740314
85.113734	2755.261002	21.745331
85.383232	2750.559658	21.750349
85.303186	2753.486824	21.755367
85.115126	2753.873919	21.760384
85.531533	2751.873205	21.765402
85.144452	2769.424585	21.770419
85.372333	2773.610799	21.775437
85.650611	2778.998011	21.780455
85.416116	2770.950515	21.785472
85.761912	2774.987347	21.790490
85.410640	2794.911783	21.795507
85.836933	2796.399721	21.800525
85.995207	2807.565715	21.805543
86.291179	2811.998306	21.810560
86.366727	2814.316999	21.815578
86.575654	2822.602973	21.820595
86.449137	2807.300535	21.825613
86.399222	2810.123793	21.830631
86.239096	2811.272605	21.835648
86.526050	2812.135375	21.840666
86.213054	2831.923965	21.845683
86.417442	2843.394135	21.850701
86.538678	2846.660508	21.855719
86.546015	2840.298688	21.860736
86.768274	2844.389064	21.865754
86.993415	2871.198245	21.870771
87.113316	2872.795620	21.875789
87.162463	2875.721088	21.880807
86.955353	2870.496299	21.885824
87.350352	2865.238428	21.890842
87.484123	2880.293520	21.895859
87.736411	2885.669970	21.900877
87.963462	2889.890175	21.905895
88.090916	2887.430508	21.910912
88.254477	2880.740908	21.915930
88.133454	2892.813645	21.920947
88.398419	2888.833528	21.925965
88.189978	2889.316699	21.930983
88.337710	2889.374932	21.936000
88.912606	2886.093474	21.941018
88.785548	2886.380384	21.946035
88.594764	2874.882803	21.951053
88.599582	2882.185827	21.956071
88.129211	2885.572507	21.961088
88.373802	2882.915598	21.966106
88.576318	2892.303122	21.971123
88.884126	2902.202475	21.976141
89.098887	2913.966030	21.981159
88.842819	2916.435949	21.986176
89.288839	2910.211815	21.991194
88.994700	2913.731657	21.996211
89.123184	2913.406726	22.001229
89.224644	2923.250109	22.006247
89.484803	2933.942922	22.011264
89.459291	2937.955627	22.016282
89.701929	2944.417612	22.021299
89.597881	2943.080398	22.026317
89.533825	2935.318711	22.031335
89.520803	2945.030119	22.036352
90.050628	2962.030402	22.041370
89.906326	2971.206614	22.046387
89.873389	2968.003187	22.051405
90.114933	2963.812035	22.056423
90.265232	2966.140072	22.061440
90.031846	2963.785917	22.066458
90.253592	2995.748291	22.071475
90.465744	2991.770275	22.076493
90.509005	2988.841813	22.081511
90.574335	3001.721111	22.086528
90.975691	2994.234441	22.091546
91.080240	3016.635175	22.096563
91.022693	3032.251909	22.101581
91.123513	3020.906731	22.106599
91.422059	3027.612346	22.111616
91.291877	3024.010644	22.116634
91.038950	3022.945741	22.121651
91.121491	3023.291265	22.126669
91.552021	3030.699536	22.131687
91.482937	3037.941266	22.136704
92.008131	3033.655305	22.141722
92.145147	3036.412613	22.146739
91.979002	3041.747290	22.151757
92.223961	3033.618475	22.156775
92.139632	3040.566862	22.161792
92.302124	3029.347931	22.166810
92.338443	3048.019155	22.171827
92.411300	3038.414524	22.176845
93.132139	3045.494109	22.181863
92.620751	3061.757487	22.186880
92.941121	3063.718593	22.191898
92.943225	3065.285216	22.196915
92.890287	3059.143731	22.201933
93.363595	3057.148851	22.206951
93.050735	3064.395641	22.211968
93.069046	3061.105357	22.216986
93.037177	3067.363380	22.222003
93.485439	3061.457412	22.227021
93.663734	3060.769763	22.232039
93.400986	3077.040708	22.237056
93.476538	3063.353781	22.242074
93.561512	3079.713234	22.247091
93.277700	3095.888442	22.252109
93.779541	3088.829364	22.257127
93.675874	3090.603221	22.262144
94.155034	3092.057590	22.267162
94.230629	3112.779687	22.272179
94.142698	3127.645409	22.277197
94.559638	3128.574002	22.282215
94.792284	3131.721984	22.287232
94.571728	3127.153730	22.292250
94.666482	3116.384479	22.297267
94.326987	3124.586590	22.302285
94.369375	3119.288101	22.307303
94.657140	3117.717692	22.312320
94.671977	3129.540047	22.317338
94.887686	3143.576235	22.322355
95.029647	3147.464749	22.327373
94.898992	3149.499362	22.332391
94.834115	3157.751310	22.337408
94.992483	3171.253887	22.342426
95.428655	3183.676957	22.347443
95.465375	3191.891485	22.352461
95.492857	3189.481535	22.357479
95.416751	3188.891086	22.362496
96.083013	3199.892205	22.367514
96.499420	3209.024779	22.372531
96.313535	3209.785194	22.377549
96.458190	3209.595341	22.382567
96.512179	3223.656607	22.387584
96.550266	3211.333262	22.392602
96.770019	3209.397674	22.397619
96.400270	3201.870239	22.402637
96.509453	3201.252603	22.407655
96.607518	3205.168585	22.412672
96.915664	3197.348980	22.417690
96.798862	3194.395655	22.422707
96.829453	3213.130148	22.427725
97.533023	3216.861475	22.432743
97.360116	3237.355129	22.437760
97.322744	3233.480556	22.442778
97.539983	3227.969285	22.447795
97.258658	3246.519925	22.452813
97.645562	3235.106151	22.457831
97.499505	3239.540922	22.462848
97.412444	3229.693421	22.467866
97.783494	3241.069676	22.472883
97.986981	3265.013355	22.477901
98.449888	3260.336861	22.482919
98.170484	3274.742397	22.487936
98.176997	3270.860817	22.492954
98.385901	3265.667092	22.497971
97.757334	3258.757510	22.502989
98.327537	3283.579638	22.508007
98.352241	3295.226704	22.513024
98.368100	3298.115086	22.518042
98.540455	3290.431936	22.523059
98.560090	3317.148841	22.528077
98.990220	3321.507492	22.533095
99.092667	3331.098478	22.538112
99.441403	3325.811636	22.543130
99.792938	3321.209521	22.548147
99.492265	3324.743874	22.553165
99.395081	3325.306861	22.558183
99.291378	3328.359057	22.563200
99.478248	3346.703007	22.568218
99.911169	3350.531806	22.573235
99.529912	3348.115423	22.578253
100.027032	3340.858743	22.583271
100.035208	3346.769094	22.588288
99.819495	3350.853933	22.593306
100.483723	3361.276525	22.598323
100.692689	3376.925859	22.603341
100.690801	3377.155058	22.608359
100.320096	3375.983830	22.613376
100.671325	3379.237248	22.618394
100.762713	3379.730834	22.623411
100.875069	3387.853172	22.628429
100.992679	3375.704232	22.633447
101.133769	3374.766054	22.638464
101.272988	3376.663266	22.643482
101.429763	3377.817440	22.648499
101.206537	3382.202413	22.653517
101.241265	3395.901123	22.658535
101.417471	3409.475807	22.663552
101.206367	3404.112225	22.668570
101.878418	3407.617353	22.673587
101.589344	3414.502594	22.678605
101.820428	3420.036021	22.683623
101.845706	3435.740668	22.688640
101.779121	3447.806754	22.693658
102.214428	3435.719596	22.698675
102.057851	3445.005833	22.703693
102.508655	3451.301118	22.708711
102.639568	3470.710625	22.713728
102.601163	3462.242871	22.718746
102.715465	3466.187799	22.723763
102.414527	3473.808123	22.728781
102.757997	3469.125436	22.733799
102.780272	3485.686497	22.738816
102.709808	3491.318382	22.743834
102.979311	3494.050718	22.748851
102.827432	3494.985868	22.753869
102.972466	3505.312782	22.758887
103.384882	3518.064030	22.763904
103.792139	3523.858895	22.768922
103.755826	3523.301420	22.773939
103.557482	3526.917836	22.778957
104.100340	3543.960774	22.783975
104.341217	3543.282005	22.788992
104.170023	3547.623330	22.794010
104.287593	3550.314611	22.799027
104.514657	3553.326696	22.804045
104.563389	3545.810232	22.809063
104.936315	3545.757042	22.814080
104.494992	3544.444447	22.819098
105.247180	3538.600748	22.824115
105.146990	3538.787411	22.829133
105.334537	3537.649084	22.834151
105.452016	3528.166817	22.839168
105.284345	3532.094580	22.844186
106.003485	3520.922606	22.849203
105.945078	3526.753180	22.854221
105.850587	3518.302203	22.859239
105.928879	3525.099809	22.864256
105.902167	3521.076356	22.869274
106.599224	3518.743662	22.874291
106.150655	3518.551641	22.879309
106.434498	3515.573698	22.884327
106.529655	3515.288683	22.889344
106.437617	3510.507870	22.894362
106.613603	3504.726957	22.899379
106.331771	3516.629970	22.904397
106.469968	3517.621132	22.909415
106.676565	3511.018784	22.914432
106.697690	3515.780189	22.919450
107.233812	3503.645435	22.924467
106.697062	3520.084852	22.929485
106.954957	3536.724039	22.934503
107.184428	3541.022714	22.939520
107.154374	3546.986441	22.944538
107.237183	3546.940965	22.949555
107.312681	3543.196992	22.954573
107.313618	3541.608558	22.959591
107.585398	3563.068575	22.964608
107.510174	3563.595029	22.969626
107.854340	3564.033369	22.974643
107.293148	3565.787412	22.979661
107.451808	3580.102941	22.984679
107.794518	3602.448501	22.989696
107.727883	3614.587891	22.994714
108.000664	3620.987157	22.999731
108.481108	3636.582467	23.004749
108.287389	3644.262874	23.009767
108.368712	3642.775677	23.014784
108.520021	3659.612933	23.019802
108.845635	3663.538381	23.024819
108.980468	3667.168570	23.029837
109.000914	3671.727174	23.034855
109.392085	3667.444313	23.039872
109.088168	3679.554726	23.044890
109.200565	3686.395742	23.049907
109.670110	3692.653531	23.054925
109.793240	3694.315776	23.059943
109.997610	3699.714330	23.064960
109.904167	3698.291182	23.069978
110.028406	3695.809868	23.074995
110.010416	3705.658664	23.080013
109.980210	3729.092844	23.085031
110.394153	3722.324392	23.090048
110.242764	3737.281089	23.095066
110.301854	3728.847982	23.100083
110.561195	3737.151611	23.105101
110.626335	3750.336039	23.110119
110.900873	3752.851287	23.115136
111.076640	3768.344279	23.120154
111.355245	3751.155897	23.125171
111.491927	3759.375256	23.130189
111.592541	3755.752305	23.135207
111.577712	3754.654885	23.140224
111.226842	3752.936870	23.145242
111.274614	3755.496931	23.150259
111.036586	3771.201442	23.155277
111.705781	3781.573199	23.160295
111.986937	3785.148620	23.165312
111.501604	3801.228506	23.170330
112.023618	3804.343081	23.175347
112.021029	3814.253215	23.180365
111.990519	3819.676679	23.185383
112.112332	3812.254627	23.190400
112.374445	3836.064023	23.195418
112.257760	3847.689233	23.200435
112.522440	3856.528592	23.205453
112.546799	3846.540188	23.210471
112.929508	3860.019428	23.215488
112.710699	3873.690570	23.220506
113.271755	3879.226625	23.225523
113.171229	3886.067858	23.230541
113.188178	3893.465425	23.235559
113.901883	3900.444304	23.240576
113.805046	3915.241441	23.245594
113.840202	3912.291274	23.250611
113.901651	3917.525467	23.255629
113.682776	3917.748366	23.260647
113.619001	3915.698989	23.265664
113.889779	3937.466519	23.270682
114.061895	3937.564926	23.275699
114.425567	3936.797333	23.280717
114.492420	3938.769092	23.285735
114.623163	3953.529979	23.290752
114.815008	3969.297531	23.295770
114.957182	3964.277047	23.300787
114.950307	3968.367303	23.305805
115.077915	3963.251593	23.310823
115.524886	3970.498029	23.315840
115.643908	3985.780027	23.320858
115.980868	3991.013584	23.325875
115.910244	3985.794165	23.330893
116.015009	3993.126646	23.335911
116.116733	3991.520519	23.340928
115.910669	3992.029302	23.345946
116.097861	3981.601833	23.350963
116.188758	3989.012045	23.355981
116.227326	3988.281341	23.360999
116.322109	3983.647588	23.366016
116.392615	4004.714750	23.371034
116.941980	4004.590947	23.376051
117.322108	4008.455876	23.381069
116.919727	4003.489954	23.386087
117.151280	4015.742611	23.391104
117.095765	4008.562715	23.396122
117.133523	4010.290530	23.401139
116.965323	4018.691599	23.406157
117.174284	4023.306789	23.411175
117.766366	4027.425066	23.416192
117.661836	4050.180111	23.421210
117.363252	4033.248639	23.426227
117.983100	4032.238802	23.431245
117.782202	4042.156323	23.436263
117.900679	4047.185585	23.441280
117.873655	4058.408040	23.446298
118.188436	4065.237417	23.451315
118.502293	4073.468036	23.456333
118.330164	4071.811164	23.461351
118.686214	4080.146770	23.466368
118.407693	4100.539674	23.471386
118.603147	4107.153663	23.476403
118.941201	4102.119993	23.481421
118.798343	4110.294440	23.486439
119.067226	4125.098767	23.491456
119.458521	4128.061186	23.496474
119.250018	4132.258373	23.501491
119.364949	4131.579995	23.506509
119.412960	4144.864271	23.511527
120.049859	4148.820459	23.516544
119.821777	4162.978736	23.521562
120.495112	4162.220759	23.526579
120.660095	4157.130490	23.531597
120.352208	4157.977272	23.536615
120.814666	4150.405544	23.541632
120.849559	4154.013243	23.546650
121.057452	4149.174170	23.551667
121.158325	4142.706403	23.556685
121.008190	4147.125575	23.561703
121.270261	4158.712664	23.566720
121.235308	4169.632805	23.571738
121.308134	4174.875504	23.576755
121.496465	4167.659795	23.581773
121.704339	4183.783755	23.586791
121.756206	4180.146445	23.591808
121.834301	4176.172970	23.596826
121.847346	4168.552528	23.601843
121.962704	4185.702930	23.606861
122.061461	4195.988149	23.611879
122.238313	4195.082767	23.616896
122.270726	4197.522629	23.621914
122.284883	4210.383614	23.626931
122.696131	4213.914010	23.631949
122.797632	4231.126464	23.636967
123.049074	4228.037903	23.641984
123.161898	4235.481717	23.647002
122.988246	4226.271992	23.652019
123.315520	4231.431657	23.657037
122.988130	4237.190543	23.662055
123.574808	4242.146791	23.667072
123.602195	4259.591371	23.672090
123.618563	4264.175984	23.677107
124.044724	4264.821551	23.682125
123.796215	4263.124913	23.687143
123.907331	4260.843846	23.692160
124.022212	4263.940837	23.697178
123.897591	4269.103341	23.702195
124.155640	4283.100043	23.707213
124.070266	4297.759636	23.712231
124.272287	4289.510320	23.717248
124.577070	4304.122657	23.722266
124.558999	4321.481728	23.727283
124.993961	4312.491946	23.732301
125.090168	4315.561244	23.737319
125.389721	4308.545649	23.742336
125.162689	4330.950123	23.747354
125.621087	4339.407231	23.752371
126.022309	4344.599202	23.757389
125.613506	4353.016796	23.762407
126.022938	4347.000084	23.767424
125.888334	4343.888089	23.772442
125.900879	4341.951568	23.777459
126.201266	4348.453745	23.782477
126.393015	4369.319582	23.787495
126.509155	4370.511784	23.792512
126.386025	4373.412311	23.797530
126.413022	4366.819338	23.802547
126.744417	4382.989119	23.807565
126.694210	4397.316721	23.812583
126.873822	4393.470181	23.817600
127.268286	4403.981382	23.822618
127.012628	4416.800604	23.827635
127.190783	4423.783314	23.832653
126.980373	4433.313980	23.837671
127.094922	4441.844854	23.842688
127.476272	4459.912162	23.847706
127.713691	4457.148340	23.852723
128.387459	4459.490705	23.857741
128.356112	4479.722780	23.862759
128.701667	4478.139873	23.867776
128.777336	4482.775675	23.872794
128.632940	4476.023532	23.877811
129.286257	4482.264950	23.882829
128.958390	4476.409801	23.887847
129.089601	4486.790748	23.892864
129.310658	4475.572394	23.897882
129.264469	4476.421521	23.902899
129.749527	4486.377867	23.907917
129.489014	4506.545821	23.912935
129.611957	4506.055746	23.917952
129.854358	4509.296880	23.922970
129.700891	4510.129285	23.927987
129.878735	4511.431241	23.933005
129.961218	4522.984316	23.938023
130.243422	4522.568760	23.943040
130.440643	4530.226627	23.948058
130.519830	4531.996675	23.953075
130.953808	4529.452462	23.958093
130.618878	4539.217822	23.963111
130.731837	4540.311420	23.968128
130.954659	4544.894670	23.973146
131.019395	4559.940467	23.978163
131.468096	4557.258586	23.983181
131.151103	4571.864910	23.988199
131.333271	4565.386356	23.993216
131.551855	4570.236200	23.998234
131.511495	4586.881652	24.003251
131.605785	4590.400529	24.008269
131.295105	4605.293817	24.013287
131.713923	4608.481669	24.018304
132.405074	4611.609578	24.023322
131.944965	4628.768074	24.028339
132.220582	4634.644953	24.033357
132.162166	4652.785764	24.038375
132.768384	4655.293916	24.043392
133.080044	4654.592015	24.048410
132.971700	4669.563247	24.053427
133.328560	4674.269136	24.058445
133.360410	4682.493140	24.063463
133.267363	4684.138045	24.068480
133.702490	4682.330781	24.073498
133.713264	4685.541228	24.078515
134.017971	4699.073016	24.083533
134.114795	4704.911559	24.088551
134.454695	4699.605189	24.093568
134.773157	4702.149790	24.098586
134.606559	4705.626113	24.103603
135.017962	4695.435385	24.108621
134.740199	4689.999352	24.113639
135.084667	4687.625155	24.118656
135.309296	4684.555724	24.123674
135.045135	4699.151389	24.128691
135.436096	4710.081906	24.133709
135.880947	4720.645879	24.138727
135.696292	4719.459030	24.143744
136.249793	4720.580740	24.148762
135.823708	4726.810276	24.153779
135.982146	4725.506570	24.158797
136.112278	4721.523865	24.163815
136.148645	4716.746573	24.168832
136.584539	4717.485806	24.173850
136.294552	4729.334448	24.178867
136.393138	4744.822682	24.183885
136.558376	4745.532692	24.188903
136.696193	4758.233615	24.193920
136.579576	4752.482349	24.198938
136.660728	4777.145039	24.203955
136.962135	4779.675852	24.208973
137.056702	4790.169064	24.213991
137.187371	4797.690564	24.219008
137.651098	4796.904620	24.224026
137.442991	4806.616105	24.229043
137.354966	4798.185389	24.234061
137.520389	4814.629141	24.239079
137.967756	4826.317024	24.244096
138.117292	4829.884581	24.249114
137.925586	4846.766088	24.254131
138.287866	4848.207027	24.259149
138.538302	4870.087753	24.264167
138.510723	4872.294193	24.269184
138.962286	4864.083444	24.274202
139.104484	4892.317792	24.279219
139.047398	4898.587693	24.284237
139.581794	4901.582528	24.289255
139.348782	4905.919158	24.294272
139.317179	4900.672737	24.299290
139.459585	4917.509706	24.304307
139.562040	4920.981730	24.309325
140.172157	4926.253107	24.314343
140.133607	4933.997554	24.319360
140.672094	4943.116476	24.324378
140.436819	4958.267945	24.329395
140.604788	4957.311224	24.334413
140.664253	4958.182869	24.339431
140.996319	4947.527858	24.344448
141.607803	4945.812029	24.349466
141.490170	4947.752761	24.354483
141.515137	4939.313389	24.359501
141.756947	4944.713516	24.364519
141.946816	4974.623247	24.369536
142.460766	4963.043919	24.374554
142.310313	4970.372736	24.379571
142.426342	4974.217881	24.384589
142.369476	4969.068299	24.389607
142.310204	4972.491381	24.394624
142.338006	4967.144990	24.399642
141.972258	4974.298077	24.404659
142.342070	4979.122371	24.409677
142.658149	4993.928706	24.414695
142.655451	5008.931428	24.419712
142.888909	5007.284520	24.424730
142.967309	5029.963917	24.429747
142.958378	5027.315584	24.434765
143.403045	5035.733590	24.439783
143.641074	5056.722048	24.444800
143.822314	5056.601871	24.449818
144.278116	5061.702003	24.454835
144.283735	5056.713937	24.459853
144.377271	5052.767661	24.464871
144.071688	5061.124351	24.469888
144.796720	5070.905156	24.474906
144.630384	5092.440410	24.479923
144.639419	5097.055560	24.484941
144.529009	5096.670334	24.489959
144.748561	5121.023583	24.494976
145.188023	5122.557669	24.499994
145.211017	5128.194158	24.505011
145.139170	5128.496691	24.510029
145.255031	5146.150862	24.515047
145.528770	5159.841428	24.520064
145.586649	5149.570649	24.525082
145.950299	5166.210558	24.530099
145.895955	5181.870756	24.535117
146.185914	5182.073120	24.540135
146.424788	5185.776788	24.545152
146.698191	5203.675764	24.550170
146.717363	5221.261258	24.555187
146.836311	5215.764137	24.560205
147.185112	5216.726561	24.565223
147.141166	5221.558686	24.570240
147.606312	5229.761903	24.575258
147.633183	5247.998417	24.580275
147.441727	5247.238240	24.585293
147.544872	5252.137399	24.590311
147.412210	5252.207311	24.595328
147.956394	5262.594555	24.600346
147.743572	5275.731044	24.605363
147.908231	5289.657052	24.610381
148.651403	5291.691101	24.615399
148.415148	5303.379790	24.620416
148.480966	5308.178707	24.625434
148.486418	5323.151339	24.630451
148.987045	5337.955345	24.635469
148.794558	5336.291344	24.640487
149.263460	5368.372889	24.645504
149.851562	5367.655993	24.650522
149.616915	5373.209346	24.655539
149.305865	5376.283219	24.660557
149.920645	5384.413099	24.665575
150.110556	5397.034671	24.670592
150.143391	5405.004798	24.675610
150.337397	5406.494655	24.680627
150.604249	5422.014992	24.685645
151.093111	5420.170754	24.690663
150.976406	5435.472959	24.695680
151.345520	5422.918754	24.700698
150.876628	5432.347294	24.705715
150.949738	5449.503542	24.710733
151.922024	5456.692143	24.715751
151.535237	5463.656848	24.720768
151.809101	5456.240415	24.725786
151.672102	5477.654322	24.730803
151.924993	5484.771173	24.735821
152.104522	5489.724321	24.740839
152.160562	5511.806147	24.745856
152.472529	5519.329794	24.750874
152.757179	5522.671419	24.755891
152.631330	5525.959692	24.760909
153.420032	5535.417526	24.765927
153.051804	5553.670204	24.770944
153.174885	5559.165017	24.775962
153.162667	5556.567467	24.780979
153.273185	5547.838739	24.785997
153.801315	5562.879338	24.791015
153.649097	5577.789247	24.796032
154.075956	5577.526054	24.801050
154.082111	5579.115901	24.806067
154.347867	5580.296151	24.811085
154.415973	5584.097170	24.816103
154.433636	5603.970497	24.821120
154.167885	5606.138703	24.826138
154.563622	5621.006924	24.831155
154.944979	5640.419487	24.836173
155.250515	5637.989197	24.841191
155.565602	5637.103391	24.846208
156.311083	5622.155447	24.851226
156.226945	5622.596061	24.856243
156.088663	5620.082327	24.861261
156.328042	5624.280906	24.866279
156.582723	5645.944171	24.871296
156.800873	5649.050954	24.876314
157.198210	5646.726403	24.881331
157.118456	5644.218282	24.886349
157.055576	5642.012739	24.891367
157.109294	5652.833292	24.896384
157.250704	5645.344257	24.901402
157.383752	5634.509631	24.906419
157.318873	5653.808467	24.911437
157.585500	5657.374867	24.916455
157.463303	5671.134542	24.921472
157.720395	5670.671037	24.926490
157.583307	5682.359948	24.931507
157.784501	5705.001133	24.936525
158.232382	5704.932854	24.941543
158.385864	5717.337064	24.946560
158.434517	5723.517286	24.951578
158.731166	5723.478626	24.956595
158.790130	5733.743725	24.961613
159.096876	5750.435853	24.966631
158.908754	5766.769450	24.971648
158.971715	5763.588676	24.976666
159.512591	5779.060980	24.981683
159.352267	5793.925191	24.986701
159.868284	5787.939691	24.991719
159.659056	5810.382901	24.996736
159.860512	5826.474279	25.001754
160.246823	5822.392214	25.006771
160.156739	5852.779513	25.011789
160.596225	5848.196438	25.016807
160.958888	5846.688558	25.021824
161.195466	5842.827843	25.026842
161.621186	5856.644315	25.031859
161.552746	5875.176105	25.036877
161.920759	5875.421113	25.041895
161.854489	5877.116167	25.046912
161.887875	5880.560877	25.051930
162.227997	5876.256421	25.056947
162.158250	5884.451659	25.061965
162.334509	5877.135552	25.066983
162.555896	5892.597543	25.072000
162.855191	5900.882655	25.077018
162.937011	5896.229917	25.082035
163.201849	5906.219196	25.087053
163.531855	5893.843924	25.092071
163.246668	5898.331566	25.097088
163.329365	5897.277446	25.102106
163.838020	5900.005944	25.107123
163.375658	5927.807576	25.112141
163.974203	5922.448524	25.117159
164.231690	5921.405875	25.122176
164.041691	5923.329158	25.127194
164.319883	5932.797834	25.132211
164.446175	5955.615783	25.137229
164.852786	5951.591818	25.142247
164.609154	5954.704626	25.147264
164.605708	5972.075104	25.152282
164.965050	5976.847111	25.157299
164.883580	5990.482570	25.162317
165.385225	6002.609636	25.167335
165.417798	6014.679317	25.172352
165.788957	6022.492767	25.177370
166.064650	6029.593658	25.182387
165.865472	6055.274075	25.187405
166.263963	6052.474055	25.192423
166.316864	6054.684362	25.197440
166.440311	6079.352709	25.202458
166.974151	6083.359703	25.207475
166.600747	6089.690767	25.212493
166.751008	6103.297252	25.217511
166.949043	6120.893064	25.222528
167.113365	6124.282336	25.227546
166.946997	6137.203677	25.232563
167.273289	6158.802774	25.237581
167.887654	6170.152745	25.242599
167.912846	6183.551858	25.247616
167.667261	6187.152843	25.252634
167.808476	6203.379336	25.257651
168.150004	6219.141956	25.262669
168.394391	6234.264672	25.267687
168.500158	6247.536124	25.272704
168.884194	6264.185825	25.277722
169.315004	6264.169052	25.282739
169.286241	6286.638498	25.287757
169.787697	6286.758382	25.292775
169.957495	6297.870902	25.297792
169.417233	6313.090470	25.302810
170.253669	6305.812887	25.307827
170.562684	6321.572145	25.312845
170.647749	6332.953126	25.317863
170.869123	6333.675512	25.322880
171.098700	6334.288797	25.327898
171.380903	6335.238314	25.332915
171.265909	6335.605186	25.337933
171.558490	6329.455246	25.342951
171.597244	6327.234183	25.347968
171.546248	6341.504781	25.352986
172.065832	6352.360152	25.358003
171.542659	6365.080502	25.363021
172.150246	6363.326594	25.368039
172.308404	6373.601500	25.373056
172.201605	6392.346196	25.378074
172.817000	6392.316519	25.383091
172.504012	6403.171693	25.388109
172.702800	6407.322678	25.393127
173.050077	6419.322058	25.398144
173.059480	6435.702791	25.403162
173.170710	6445.631162	25.408179
173.385074	6455.750030	25.413197
173.494581	6459.665057	25.418215
174.028738	6478.018126	25.423232
173.618913	6484.066400	25.428250
174.109448	6492.134880	25.433267
174.436225	6513.026281	25.438285
174.915881	6512.945071	25.443303
174.853348	6517.590957	25.448320
174.614725	6525.406686	25.453338
175.359946	6544.277748	25.458355
175.341784	6550.682982	25.463373
175.545634	6553.330375	25.468391
176.174703	6562.172283	25.473408
176.150519	6576.470304	25.478426
176.437809	6573.426694	25.483443
176.391502	6580.588629	25.488461
176.483338	6584.179975	25.493479
176.796946	6583.147219	25.498496
176.617175	6605.272201	25.503514
177.122867	6605.175826	25.508531
177.166807	6618.508610	25.513549
176.865760	6624.806331	25.518567
177.200887	6644.144968	25.523584
177.501506	6646.780098	25.528602
178.109990	6657.259582	25.533619
178.104541	6671.505137	25.538637
178.299403	6679.153484	25.543655
178.570366	6677.446915	25.548672
178.304297	6682.486455	25.553690
178.603561	6688.409960	25.558707
178.870783	6692.372293	25.563725
178.734450	6701.652617	25.568743
178.877756	6722.122710	25.573760
179.070290	6728.372470	25.578778
179.530422	6746.810850	25.583795
179.485280	6759.598526	25.588813
179.670415	6758.580732	25.593831
180.473956	6771.674529	25.598848
180.208199	6792.251636	25.603866
180.457207	6786.856734	25.608883
180.811870	6795.090247	25.613901
181.331453	6789.987399	25.618919
181.642279	6788.260300	25.623936
181.381269	6793.016597	25.628954
181.752226	6792.582120	25.633971
182.050521	6802.449435	25.638989
182.122258	6802.003648	25.644007
182.331992	6801.911968	25.649024
182.039120	6803.197904	25.654042
182.442124	6801.024923	25.659059
182.416022	6791.124408	25.664077
182.404545	6805.879347	25.669095
182.604115	6818.724842	25.674112
182.663089	6828.992271	25.679130
183.480638	6841.835258	25.684148
183.455832	6854.608757	25.689165
183.481871	6859.338984	25.694183
183.637084	6853.152505	25.699200
183.494629	6870.469083	25.704218
183.760261	6876.856753	25.709236
184.227831	6890.209582	25.714253
184.665321	6913.412939	25.719271
184.683509	6918.950160	25.724288
184.722098	6920.682906	25.729306
185.101731	6918.203620	25.734324
185.219816	6933.778376	25.739341
184.937076	6944.344283	25.744359
185.397539	6937.672408	25.749376
185.357979	6962.945357	25.754394
185.625099	6969.546850	25.759412
185.979289	6983.445811	25.764429
186.012659	6996.781406	25.769447
186.422335	7009.158444	25.774464
186.029376	7029.018882	25.779482
186.754580	7030.268428	25.784500
186.985053	7048.046651	25.789517
187.045593	7070.730442	25.794535
187.480571	7060.793224	25.799552
187.480906	7072.436137	25.804570
187.536179	7084.618734	25.809588
187.639484	7104.109809	25.814605
187.831744	7108.330489	25.819623
188.305824	7126.628634	25.824640
188.351711	7145.641069	25.829658
188.813904	7135.132930	25.834676
189.340989	7154.442418	25.839693
188.743275	7171.579344	25.844711
189.253098	7166.528286	25.849728
189.136722	7175.124306	25.854746
189.313588	7190.351612	25.859764
189.802459	7196.104248	25.864781
189.848079	7208.130327	25.869799
190.196252	7223.770210	25.874816
190.339606	7226.940400	25.879834
190.662081	7233.467877	25.884852
190.655742	7239.205841	25.889869
190.793489	7249.639619	25.894887
191.609090	7245.797972	25.899904
191.218944	7258.907821	25.904922
191.529271	7262.899633	25.909940
191.715448	7266.489482	25.914957
191.770909	7280.854167	25.919975
192.012294	7283.345419	25.924992
191.836834	7292.749588	25.930010
192.373380	7308.830859	25.935028
192.684607	7316.392527	25.940045
192.563094	7317.981668	25.945063
192.922975	7325.751185	25.950080
193.248191	7337.993247	25.955098
193.146520	7337.856786	25.960116
193.532422	7353.022608	25.965133
193.702836	7373.107647	25.970151
193.845760	7373.236709	25.975168
193.784597	7385.652141	25.980186
194.250664	7396.409016	25.985204
194.473927	7395.562148	25.990221
194.483892	7423.418734	25.995239
194.901755	7427.128273	26.000256
195.006007	7429.177161	26.005274
195.342127	7445.851568	26.010292
195.606147	7455.949827	26.015309
195.821320	7464.899182	26.020327
195.839174	7457.392741	26.025344
196.063191	7484.978471	26.030362
196.312863	7492.174706	26.035380
196.846856	7488.742215	26.040397
196.471652	7507.529526	26.045415
197.107828	7510.686523	26.050432
197.282118	7537.226657	26.055450
197.294562	7524.363231	26.060468
197.506769	7540.276135	26.065485
197.019047	7553.345141	26.070503
197.828502	7555.177756	26.075520
197.814436	7589.873268	26.080538
197.990743	7592.413505	26.085556
198.188010	7606.320755	26.090573
198.230690	7628.966538	26.095591
198.440253	7634.102110	26.100608
198.469827	7645.801398	26.105626
198.755405	7660.210813	26.110644
198.926153	7677.335970	26.115661
199.343816	7689.996369	26.120679
199.575067	7710.327113	26.125696
199.517500	7716.057689	26.130714
199.420536	7742.050482	26.135732
200.036140	7764.077924	26.140749
200.096742	7769.428502	26.145767
200.785229	7778.372625	26.150784
201.297095	7786.314877	26.155802
201.384561	7789.161245	26.160820
201.918936	7797.502800	26.165837
201.822195	7815.762170	26.170855
202.054793	7810.648471	26.175872
202.453697	7809.853057	26.180890
202.526988	7808.300631	26.185908
202.678574	7805.179656	26.190925
202.428017	7813.750613	26.195943
203.033977	7818.374138	26.200960
203.211375	7826.664027	26.205978
203.318473	7837.964352	26.210996
203.820002	7836.938937	26.216013
203.635611	7838.904059	26.221031
204.061620	7847.567444	26.226048
203.896018	7867.886914	26.231066
204.024690	7867.448152	26.236084
204.446149	7869.452434	26.241101
204.316444	7898.224505	26.246119
204.470053	7903.130662	26.251136
204.629919	7914.575683	26.256154
204.768573	7931.051161	26.261172
205.047446	7929.764576	26.266189
205.185791	7955.334256	26.271207
205.422032	7957.032861	26.276224
205.686988	7986.691181	26.281242
205.742549	8004.613318	26.286260
206.306294	8009.146058	26.291277
206.269565	8025.194772	26.296295
206.428805	8044.985050	26.301312
206.911967	8059.484142	26.306330
206.723160	8065.668962	26.311348
206.812012	8084.903159	26.316365
207.007656	8103.755627	26.321383
207.636676	8127.691282	26.326400
207.922802	8131.443642	26.331418
208.224947	8156.518953	26.336436
208.541058	8153.039998	26.341453
208.355962	8172.081906	26.346471
208.533598	8182.487159	26.351488
209.301871	8182.747498	26.356506
209.178000	8200.210197	26.361524
209.747221	8207.558468	26.366541
210.002722	8208.429352	26.371559
210.480379	8201.714838	26.376576
210.745929	8207.078149	26.381594
210.553911	8231.674052	26.386612
211.192232	8227.987120	26.391629
211.116323	8240.552764	26.396647
210.992777	8237.803701	26.401664
211.131071	8244.977137	26.406682
211.489793	8263.207333	26.411700
211.444345	8265.355350	26.416717
211.539023	8273.304565	26.421735
211.947533	8293.733360	26.426752
212.343455	8303.661655	26.431770
211.994152	8315.180283	26.436788
212.702317	8323.980352	26.441805
212.737002	8336.568185	26.446823
212.751366	8350.371511	26.451840
213.147334	8363.931454	26.456858
213.264256	8375.147599	26.461876
213.191415	8381.830279	26.466893
213.453419	8407.361740	26.471911
213.743884	8403.327318	26.476928
213.821327	8432.462818	26.481946
213.709121	8444.567776	26.486964
214.483247	8461.884088	26.491981
214.711467	8472.062714	26.496999
214.914055	8498.898289	26.502016
215.294425	8507.758592	26.507034
215.310188	8523.138455	26.512052
215.620938	8527.809659	26.517069
215.736691	8540.801418	26.522087
215.892672	8558.153820	26.527104
216.383021	8570.444939	26.532122
216.593880	8581.053708	26.537140
217.308508	8592.422619	26.542157
216.942750	8606.670797	26.547175
216.894888	8611.241809	26.552192
217.560320	8626.909712	26.557210
217.576855	8647.283437	26.562228
217.764385	8646.414263	26.567245
218.080327	8656.782060	26.572263
217.803265	8664.802546	26.577280
218.248273	8674.325864	26.582298
218.345174	8703.562271	26.587316
218.561259	8712.420948	26.592333
219.059842	8714.715238	26.597351
219.312224	8741.288737	26.602368
219.714342	8754.187815	26.607386
219.659882	8763.823861	26.612404
220.109117	8778.045373	26.617421
220.187149	8792.740000	26.622439
220.032608	8814.757201	26.627456
220.828905	8815.791376	26.632474
220.554729	8840.379730	26.637492
220.580350	8856.847884	26.642509
221.302825	8862.522622	26.647527
221.545383	8890.432212	26.652544
221.931461	8890.672442	26.657562
222.075068	8913.229713	26.662580
222.474778	8917.466632	26.667597
222.682875	8931.044841	26.672615
222.669848	8944.451344	26.677632
222.987946	8949.106166	26.682650
222.989324	8961.638451	26.687668
223.436423	8980.344129	26.692685
223.661567	8985.349413	26.697703
223.526956	9001.812576	26.702720
223.941162	9018.599061	26.707738
224.285830	9035.995125	26.712756
224.370693	9029.253149	26.717773
224.322211	9054.476751	26.722791
224.413139	9069.354921	26.727808
225.058857	9076.747699	26.732826
224.857529	9092.004180	26.737844
224.923424	9107.839773	26.742861
225.253149	9129.394631	26.747879
225.485248	9153.444784	26.752896
226.087190	9166.783754	26.757914
225.901373	9184.417616	26.762932
226.167350	9187.949568	26.767949
226.659180	9209.146603	26.772967
226.703733	9233.905141	26.777984
227.177473	9239.379259	26.783002
227.185563	9266.389652	26.788020
227.496137	9265.209261	26.793037
228.873629	9257.047634	26.798055
229.602493	9261.739774	26.803072
230.053664	9252.127095	26.808090
230.033849	9253.633728	26.813108
230.488162	9231.869471	26.818125
230.759744	9219.528320	26.823143
230.502068	9209.227142	26.828160
230.917543	9210.569161	26.833178
230.921889	9208.744277	26.838196
230.817736	9204.928759	26.843213
231.046543	9203.170400	26.848231
230.821304	9209.043956	26.853248
231.121940	9206.909784	26.858266
231.063241	9219.264958	26.863284
231.407954	9229.226432	26.868301
231.325281	9245.862191	26.873319
231.184267	9254.760800	26.878336
231.677960	9271.932316	26.883354
231.693890	9290.762594	26.888372
231.895177	9314.682561	26.893389
232.344223	9332.950031	26.898407
231.993882	9348.427266	26.903424
232.555678	9369.642495	26.908442
232.425036	9393.636746	26.913460
232.694182	9420.733686	26.918477
233.212929	9436.927127	26.923495
233.425829	9464.207032	26.928512
233.924841	9465.938296	26.933530
234.093237	9505.186980	26.938548
234.353109	9519.227688	26.943565
234.587606	9533.507366	26.948583
234.870708	9554.256926	26.953600
235.323206	9579.635677	26.958618
235.502834	9582.151332	26.963636
235.370796	9608.256039	26.968653
236.053494	9611.465110	26.973671
236.235918	9645.487157	26.978688
237.090011	9637.982475	26.983706
237.002706	9649.307286	26.988724
236.899307	9646.806978	26.993741
237.434044	9662.218214	26.998759
237.584769	9670.321749	27.003776
237.699085	9670.731235	27.008794
238.040347	9683.484601	27.013812
238.367604	9696.505426	27.018829
238.645757	9696.416605	27.023847
238.537833	9709.399385	27.028864
238.887186	9719.756694	27.033882
238.893611	9733.270584	27.038900
238.861992	9746.496611	27.043917
239.259660	9758.836145	27.048935
239.228877	9779.424351	27.053952
239.562313	9797.877658	27.058970
239.781818	9823.794881	27.063988
239.975655	9834.370659	27.069005
240.790579	9854.203617	27.074023
240.979045	9875.385813	27.079040
241.455787	9889.947917	27.084058
241.420933	9899.447775	27.089076
241.253461	9915.140015	27.094093
241.764375	9925.998608	27.099111
242.037302	9953.561416	27.104128
242.109510	9966.009269	27.109146
242.437488	9981.651723	27.114164
243.284598	9988.486355	27.119181
243.369597	9991.415385	27.124199
243.502981	10023.339301	27.129216
243.661427	10017.289129	27.134234
244.098445	10032.891825	27.139252
244.193737	10064.599572	27.144269
244.448469	10054.411706	27.149287
244.789889	10074.347190	27.154304
245.098923	10089.120380	27.159322
245.435690	10098.853501	27.164340
245.194268	10110.719894	27.169357
245.694360	10119.509343	27.174375
245.597510	10140.357267	27.179392
245.922597	10162.857973	27.184410
246.346263	10166.655824	27.189428
246.312287	10190.846459	27.194445
246.835329	10200.616850	27.199463
246.787287	10223.933049	27.204480
247.216978	10224.768817	27.209498
247.581891	10254.727545	27.214516
247.600565	10266.940993	27.219533
248.272812	10281.150426	27.224551
247.641382	10305.831953	27.229568
248.067901	10318.872518	27.234586
248.683639	10326.259291	27.239604
248.755424	10355.995194	27.244621
249.113489	10366.754122	27.249639
249.456383	10388.791134	27.254656
249.878876	10391.917114	27.259674
249.580345	10397.851212	27.264692
250.038857	10416.665082	27.269709
250.417035	10431.468512	27.274727
250.564465	10444.587514	27.279744
250.987539	10453.619249	27.284762
251.791620	10459.785299	27.289780
251.693911	10481.928094	27.294797
251.798362	10484.360654	27.299815
252.159703	10506.194206	27.304832
252.201865	10512.404202	27.309850
252.638961	10522.385261	27.314868
252.984528	10536.071296	27.319885
253.012596	10543.298033	27.324903
253.302004	10553.322722	27.329920
253.570311	10564.503782	27.334938
254.339509	10566.843385	27.339956
254.036532	10580.115755	27.344973
254.254208	10598.982014	27.349991
254.464170	10612.280477	27.355008
254.329844	10622.719441	27.360026
254.928633	10647.203071	27.365044
254.762764	10662.906849	27.370061
255.102711	10677.721338	27.375079
255.376676	10699.441991	27.380096
255.512185	10712.142061	27.385114
255.968514	10737.375768	27.390132
255.829247	10763.929088	27.395149
256.184247	10773.814001	27.400167
256.715582	10797.583368	27.405184
257.200742	10805.644440	27.410202
257.708862	10821.449126	27.415220
257.964904	10837.050417	27.420237
258.497029	10847.306178	27.425255
258.807506	10863.025928	27.430272
258.740303	10870.374257	27.435290
259.141905	10882.394550	27.440308
259.186613	10897.077654	27.445325
259.621239	10896.660879	27.450343
259.848671	10913.703173	27.455360
259.948163	10923.660786	27.460378
260.734446	10933.455418	27.465396
260.686565	10962.687019	27.470413
261.031412	10959.622350	27.475431
261.290707	10965.374490	27.480448
261.400944	10985.556600	27.485466
261.979271	10991.782863	27.490484
261.780994	10998.021152	27.495501
262.471706	11009.020698	27.500519
262.667565	11019.051559	27.505536
262.764764	11016.460806	27.510554
262.761511	11041.559707	27.515572
262.866187	11057.842151	27.520589
263.557458	11060.607069	27.525607
263.694563	11086.312532	27.530624
263.615315	11092.800273	27.535642
263.755199	11105.665260	27.540660
264.080779	11123.793243	27.545677
264.670513	11133.710634	27.550695
264.472388	11155.123104	27.555712
264.674227	11165.960831	27.560730
264.847079	11187.432079	27.565748
265.244143	11200.193189	27.570765
265.590932	11214.545700	27.575783
265.976682	11232.739979	27.580800
265.977788	11258.631120	27.585818
266.264685	11265.108980	27.590836
266.594112	11281.731274	27.595853
267.295361	11302.694628	27.600871
267.258367	11319.742732	27.605888
267.908844	11323.328624	27.610906
268.184043	11340.140258	27.615924
267.923306	11354.703467	27.620941
268.165486	11378.396270	27.625959
268.734615	11386.891920	27.630976
268.461755	11404.413359	27.635994
269.009967	11426.111219	27.641012
269.466773	11451.314169	27.646029
269.732690	11465.551122	27.651047
270.035084	11484.929179	27.656064
270.272306	11495.796922	27.661082
270.511610	11512.758308	27.666100
270.802704	11532.000880	27.671117
271.018239	11547.991491	27.676135
271.109753	11571.897903	27.681152
271.318141	11591.320989	27.686170
271.936354	11611.152604	27.691188
272.265195	11626.219696	27.696205
272.607058	11646.216025	27.701223
272.818050	11666.012460	27.706240
272.997688	11677.837954	27.711258
273.749958	11686.273888	27.716276
273.466347	11704.657870	27.721293
273.957469	11719.807809	27.726311
274.311749	11726.544707	27.731328
274.300121	11750.774807	27.736346
274.860111	11758.980312	27.741364
274.650690	11782.691612	27.746381
274.796523	11798.890568	27.751399
275.194076	11822.052804	27.756416
275.557072	11838.397434	27.761434
275.837563	11859.543543	27.766452
276.531219	11883.458174	27.771469
276.482513	11900.988534	27.776487
277.038637	11905.203940	27.781504
277.147366	11927.692766	27.786522
277.563077	11946.162353	27.791540
277.910100	11973.773709	27.796557
278.086829	11978.304038	27.801575
278.029284	11996.897720	27.806592
278.289427	12010.663057	27.811610
278.710051	12020.461194	27.816628
278.823760	12034.174723	27.821645
278.894818	12073.058333	27.826663
279.443976	12076.747142	27.831680
279.739860	12102.325515	27.836698
280.100303	12115.776842	27.841716
280.271718	12126.514437	27.846733
280.637792	12149.930526	27.851751
280.857266	12166.759438	27.856768
280.794431	12169.941505	27.861786
281.490478	12185.341824	27.866804
281.770226	12214.415781	27.871821
282.056079	12223.760900	27.876839
282.432973	12234.490026	27.881856
282.340069	12264.734687	27.886874
282.903109	12269.606537	27.891892
283.154901	12304.671166	27.896909
283.404739	12314.338898	27.901927
283.647475	12323.055743	27.906944
283.943909	12349.049061	27.911962
284.263851	12357.919507	27.916980
284.187412	12380.478462	27.921997
284.474572	12408.195785	27.927015
284.913022	12417.524180	27.932032
284.985241	12445.407083	27.937050
285.380282	12461.327345	27.942068
285.816699	12486.071255	27.947085
286.119438	12516.699268	27.952103
286.433830	12529.671068	27.957120
286.901061	12558.284650	27.962138
287.308643	12566.308856	27.967156
287.347889	12581.888253	27.972173
287.221558	12610.990497	27.977191
288.057533	12631.440101	27.982208
287.968684	12649.988209	27.987226
288.725067	12669.586665	27.992244
288.778065	12692.072712	27.997261
289.187717	12706.834397	28.002279
289.840871	12720.708944	28.007296
289.746339	12742.934224	28.012314
290.264765	12752.567595	28.017332
290.527820	12782.303252	28.022349
290.734940	12799.383179	28.027367
291.121561	12800.960184	28.032384
291.231309	12827.475450	28.037402
291.522701	12826.611045	28.042420
291.750069	12858.018243	28.047437
291.777431	12862.629810	28.052455
292.470932	12885.677923	28.057472
292.812135	12912.305317	28.062490
293.385985	12921.828125	28.067508
293.624811	12928.481830	28.072525
293.692627	12954.415406	28.077543
294.220744	12959.252117	28.082560
294.427448	12968.956659	28.087578
295.207671	12996.264784	28.092596
295.157400	13003.828306	28.097613
295.422212	12991.460385	28.102631
296.263614	12978.489125	28.107648
296.180234	13001.073324	28.112666
296.435279	13012.756287	28.117684
296.603803	13015.576855	28.122701
296.667559	13023.618418	28.127719
296.833547	13026.583541	28.132736
296.892740	13045.854959	28.137754
297.429339	13063.754647	28.142772
297.745430	13079.743736	28.147789
297.947709	13101.093549	28.152807
298.492297	13116.143679	28.157824
298.033374	13138.043006	28.162842
298.581401	13148.499026	28.167860
298.718350	13166.488703	28.172877
299.317720	13194.107322	28.177895
299.618683	13208.979409	28.182912
299.655578	13242.307451	28.187930
299.936757	13252.629844	28.192948
300.526386	13290.699681	28.197965
300.627685	13299.819047	28.202983
300.999091	13320.177434	28.208000
300.997318	13343.040583	28.213018
301.709916	13364.357057	28.218036
302.234096	13378.291828	28.223053
302.438367	13401.566981	28.228071
302.571415	13410.057613	28.233088
302.635028	13436.818133	28.238106
303.388740	13451.962398	28.243124
303.648686	13475.354838	28.248141
303.899620	13492.672094	28.253159
304.466616	13500.938345	28.258176
304.561029	13527.278284	28.263194
305.287902	13536.243481	28.268212
305.215761	13541.175654	28.273229
305.444685	13582.597586	28.278247
306.129456	13571.507079	28.283264
306.486504	13602.546026	28.288282
307.113937	13601.265526	28.293300
307.026216	13623.635941	28.298317
306.943760	13639.263463	28.303335
307.760192	13648.820591	28.308352
307.629938	13670.277333	28.313370
307.741627	13686.475868	28.318388
308.288872	13711.129031	28.323405
308.302629	13733.277091	28.328423
308.462726	13743.956133	28.333440
308.852861	13766.803015	28.338458
309.042229	13795.409581	28.343476
309.697840	13813.731132	28.348493
309.616830	13853.678879	28.353511
310.200470	13858.963316	28.358528
310.278108	13882.362211	28.363546
310.427631	13900.434488	28.368564
310.795418	13923.237343	28.373581
310.961313	13952.267916	28.378599
311.367065	13971.195060	28.383616
311.514909	14002.912884	28.388634
311.554330	14017.624540	28.393652
312.104073	14054.549772	28.398669
312.247695	14073.549347	28.403687
313.180315	14104.434313	28.408704
313.287750	14136.951873	28.413722
313.813841	14156.695034	28.418740
313.987865	14186.981646	28.423757
314.298713	14207.277460	28.428775
314.645835	14231.194638	28.433792
314.981236	14244.507192	28.438810
315.166856	14266.475026	28.443828
315.888705	14282.526274	28.448845
315.961229	14320.464210	28.453863
316.528245	14322.613975	28.458880
317.023173	14344.580156	28.463898
317.339603	14366.296924	28.468916
317.753455	14369.900415	28.473933
317.687834	14408.108659	28.478951
318.005685	14422.124505	28.483968
318.048122	14447.069104	28.488986
318.480640	14466.176341	28.494004
318.847806	14479.472328	28.499021
319.159212	14513.125844	28.504039
319.791103	14527.998928	28.509056
320.139850	14543.925798	28.514074
320.399141	14565.898164	28.519092
320.699156	14592.149307	28.524109
320.860308	14607.421045	28.529127
320.847246	14624.574316	28.534144
321.402339	14650.373476	28.539162
321.584724	14677.874660	28.544180
321.784000	14710.000332	28.549197
322.349721	14724.017003	28.554215
322.620721	14748.605750	28.559232
322.952858	14779.845013	28.564250
323.226923	14799.789768	28.569268
324.440250	14814.334298	28.574285
324.893432	14831.147898	28.579303
325.159896	14837.950271	28.584320
325.671315	14842.996810	28.589338
325.847543	14861.953591	28.594356
326.306029	14865.804569	28.599373
326.426096	14876.119690	28.604391
326.880170	14894.675410	28.609408
326.664737	14903.945009	28.614426
326.881800	14927.633852	28.619444
327.414773	14941.351865	28.624461
327.223971	14960.784899	28.629479
327.841860	14966.098122	28.634496
328.067249	14994.442078	28.639514
328.493331	15009.168150	28.644532
328.859077	15027.743225	28.649549
328.767609	15047.140562	28.654567
329.295219	15067.762457	28.659584
329.422562	15082.475293	28.664602
329.653181	15114.000265	28.669620
329.955896	15130.026502	28.674637
330.066904	15162.706957	28.679655
330.539384	15180.528817	28.684672
330.845680	15206.551211	28.689690
330.936020	15234.779359	28.694708
331.401142	15266.839129	28.699725
331.241108	15288.365067	28.704743
331.727197	15318.877561	28.709760
332.532937	15349.805835	28.714778
332.712979	15387.665698	28.719796
333.051705	15402.796166	28.724813
333.173555	15441.254713	28.729831
333.700789	15473.575841	28.734848
334.501917	15507.193939	28.739866
334.581739	15524.844556	28.744884
335.195505	15549.409485	28.749901
335.216020	15584.761565	28.754919
335.599296	15600.858810	28.759936
335.910607	15624.852265	28.764954
336.127880	15658.733203	28.769972
336.789580	15680.988657	28.774989
337.353113	15709.523712	28.780007
337.474085	15733.284120	28.785024
337.704593	15750.817098	28.790042
338.031490	15788.206569	28.795060
338.817445	15793.667000	28.800077
339.286062	15813.075441	28.805095
339.861135	15832.775563	28.810112
340.532058	15842.319777	28.815130
340.779162	15860.618446	28.820148
341.168527	15861.347226	28.825165
341.305751	15877.143463	28.830183
341.618176	15888.367864	28.835200
341.982270	15904.569850	28.840218
342.003032	15917.349032	28.845236
342.600432	15927.293552	28.850253
342.788217	15943.577212	28.855271
342.758963	15966.145529	28.860288
343.257737	15974.421742	28.865306
343.354982	16000.837019	28.870324
343.950228	16032.556820	28.875341
343.982726	16050.991871	28.880359
344.157592	16062.799478	28.885376
344.640222	16083.209459	28.890394
345.027991	16117.212644	28.895412
345.482712	16140.439641	28.900429
345.656572	16158.092728	28.905447
345.860851	16183.316384	28.910464
346.523844	16198.755375	28.915482
346.573582	16230.543815	28.920500
347.001367	16253.268436	28.925517
347.402048	16272.652657	28.930535
347.859571	16287.329676	28.935552
347.909264	16311.786520	28.940570
348.210327	16339.634718	28.945588
349.040127	16345.368654	28.950605
349.419451	16378.618517	28.955623
349.891124	16391.603967	28.960640
350.117004	16407.548219	28.965658
350.525608	16424.811282	28.970676
350.609423	16444.445999	28.975693
351.066147	16469.603913	28.980711
351.413859	16482.296031	28.985728
351.892654	16499.305100	28.990746
351.779511	16533.633690	28.995764
352.194113	16541.818908	29.000781
352.323620	16570.558965	29.005799
352.682683	16603.064960	29.010816
353.322605	16611.569795	29.015834
353.546662	16643.855479	29.020852
353.649419	16669.950965	29.025869
354.086179	16697.617764	29.030887
354.720444	16732.592206	29.035904
355.207071	16750.707907	29.040922
355.389096	16781.299705	29.045940
356.068151	16794.064862	29.050957
356.245210	16822.932644	29.055975
356.358135	16859.531890	29.060992
357.272083	16871.699283	29.066010
357.206346	16908.830432	29.071028
357.483565	16924.111758	29.076045
357.678532	16953.605437	29.081063
357.937779	16980.698109	29.086080
358.246138	17008.014881	29.091098
358.869189	17032.255323	29.096116
359.552760	17053.009945	29.101133
360.085968	17078.913912	29.106151
360.183709	17107.684829	29.111168
360.680605	17129.394851	29.116186
360.750588	17158.894271	29.121204
361.171275	17175.174203	29.126221
361.372048	17200.198312	29.131239
361.699815	17233.282644	29.136256
362.093148	17258.319862	29.141274
362.236306	17292.917546	29.146292
362.786276	17313.182800	29.151309
363.356571	17348.918808	29.156327
363.276755	17381.470782	29.161344
364.031014	17395.089986	29.166362
364.689543	17421.752491	29.171380
365.560005	17425.872328	29.176397
366.011062	17445.510620	29.181415
366.458343	17453.599388	29.186432
366.732656	17472.696993	29.191450
366.911009	17481.737666	29.196468
367.633510	17482.436283	29.201485
367.669774	17495.176305	29.206503
368.035479	17507.816993	29.211520
368.486403	17509.779338	29.216538
368.375241	17529.369531	29.221556
368.718618	17557.953719	29.226573
369.102883	17568.386020	29.231591
369.379893	17586.490436	29.236608
369.590984	17610.707669	29.241626
369.353592	17639.572344	29.246644
370.021477	17657.035430	29.251661
370.576330	17689.075109	29.256679
370.974267	17721.982769	29.261696
371.124723	17731.352441	29.266714
371.479412	17764.400546	29.271732
371.926436	17780.309596	29.276749
372.406877	17806.046419	29.281767
372.676016	17839.172488	29.286784
373.082321	17856.943230	29.291802
373.251075	17896.582299	29.296820
373.830478	17932.160720	29.301837
373.956137	17954.431453	29.306855
374.279495	17992.394932	29.311872
374.757289	18021.538877	29.316890
374.984711	18050.020005	29.321908
375.546473	18079.644783	29.326925
376.077059	18114.558947	29.331943
376.685361	18135.366784	29.336960
377.179277	18161.688677	29.341978
377.143793	18190.606452	29.346996
377.732205	18217.498042	29.352013
378.014275	18242.771515	29.357031
378.594590	18265.280886	29.362048
378.823700	18286.279666	29.367066
379.140002	18313.363211	29.372084
379.470639	18344.021418	29.377101
379.773569	18376.560549	29.382119
379.875797	18403.495678	29.387136
380.486791	18431.357701	29.392154
380.723221	18475.202593	29.397172
380.821987	18501.830555	29.402189
382.061759	18530.180388	29.407207
382.086902	18560.395549	29.412224
382.749715	18587.495621	29.417242
383.201346	18611.291025	29.422260
383.701818	18640.058481	29.427277
383.856682	18664.364664	29.432295
384.186678	18687.376371	29.437312
384.783675	18721.053291	29.442330
384.822274	18748.157824	29.447348
384.919456	18775.341658	29.452365
385.577431	18803.622874	29.457383
385.563252	18837.892739	29.462400
386.194687	18866.908269	29.467418
386.415412	18901.250300	29.472436
386.849529	18930.009179	29.477453
387.138376	18952.448263	29.482471
387.398502	18991.259351	29.487488
388.006181	19016.796788	29.492506
388.311194	19048.680245	29.497524
388.509679	19085.259082	29.502541
389.119936	19109.365038	29.507559
389.562754	19150.868904	29.512576
390.128400	19168.536617	29.517594
390.251300	19196.864431	29.522612
390.682735	19235.260212	29.527629
391.324150	19260.297745	29.532647
391.503108	19296.856564	29.537664
392.160078	19319.926171	29.542682
392.345172	19347.806116	29.547700
392.420159	19390.735900	29.552717
393.239344	19410.512530	29.557735
393.341765	19449.514074	29.562752
394.142008	19473.318640	29.567770
394.512683	19514.331368	29.572788
394.491277	19546.594658	29.577805
395.207948	19566.847716	29.582823
395.446907	19608.757762	29.587840
396.060956	19630.252987	29.592858
396.123844	19670.540271	29.597876
396.413488	19703.529219	29.602893
397.142783	19734.287680	29.607911
397.295026	19781.721354	29.612928
397.995234	19802.260841	29.617946
398.550560	19846.728933	29.622964
398.693489	19871.872468	29.627981
399.232703	19899.416619	29.632999
399.254162	19947.562277	29.638016
400.036078	19968.959165	29.643034
400.620265	20010.435304	29.648052
401.032381	20043.604302	29.653069
401.485875	20053.570486	29.658087
401.893032	20086.852587	29.663104
402.001669	20109.659890	29.668122
402.623191	20139.009730	29.673140
403.094294	20161.795583	29.678157
403.441346	20197.916665	29.683175
403.729798	20221.013639	29.688192
404.546481	20249.009156	29.693210
404.767973	20282.858741	29.698228
404.640563	20313.450856	29.703245
405.923949	20327.899908	29.708263
406.557104	20350.759445	29.713280
406.497632	20369.120738	29.718298
407.456611	20385.173756	29.723316
407.870324	20415.956278	29.728333
408.011670	20433.642234	29.733351
408.218916	20449.594583	29.738368
408.330961	20467.248231	29.743386
408.988037	20498.310304	29.748404
409.035133	20514.407154	29.753421
410.221013	20537.815231	29.758439
409.977172	20555.368961	29.763456
410.417861	20573.060146	29.768474
410.950100	20585.946931	29.773492
410.871626	20612.733515	29.778509
411.499534	20633.705773	29.783527
411.546258	20659.624303	29.788544
411.988988	20694.594856	29.793562
412.300238	20730.695305	29.798580
412.484395	20762.512118	29.803597
413.094830	20792.693061	29.808615
413.320298	20838.437620	29.813632
413.444632	20870.801296	29.818650
414.014915	20917.396049	29.823668
414.735789	20956.747375	29.828685
415.125629	20995.350591	29.833703
415.179104	21032.641857	29.838720
415.469624	21076.714194	29.843738
416.466377	21105.985191	29.848756
416.335997	21142.913801	29.853773
416.989382	21178.398440	29.858791
417.464700	21225.733802	29.863808
418.006523	21263.640872	29.868826
418.443791	21314.944861	29.873844
418.720084	21342.324336	29.878861
419.783506	21366.275333	29.883879
419.933459	21417.226127	29.888896
420.073058	21449.923282	29.893914
420.469641	21478.953510	29.898932
420.739780	21527.389648	29.903949
421.225752	21564.776294	29.908967
421.913193	21602.390835	29.913984
423.506986	21609.022815	29.919002
424.315746	21618.974354	29.924020
424.622431	21635.502758	29.929037
424.953012	21642.362791	29.934055
425.623610	21665.412030	29.939072
425.585971	21680.922634	29.944090
426.223673	21701.359982	29.949108
426.349533	21715.388303	29.954125
426.953105	21735.702755	29.959143
426.782953	21753.883241	29.964160
427.398462	21786.356414	29.969178
427.727288	21803.909289	29.974196
427.945537	21834.714702	29.979213
428.679859	21860.598902	29.984231
428.901649	21895.297793	29.989248
429.134627	21924.773917	29.994266
429.668560	21942.001277	29.999284
430.006038	21982.867031	30.004301
430.794584	22004.375521	30.009319
431.114313	22029.552617	30.014336
431.919141	22052.323488	30.019354
432.140631	22075.761502	30.024372
432.411698	22097.526629	30.029389
432.799531	22105.929351	30.034407
432.967142	22132.003526	30.039424
433.220443	22159.707069	30.044442
433.943302	22185.722801	30.049460
434.071859	22221.598217	30.054477
434.441339	22242.386176	30.059495
434.378283	22282.825827	30.064512
434.631428	22315.705952	30.069530
435.255397	22358.255877	30.074548
435.691658	22393.897567	30.079565
436.367838	22430.792833	30.084583
436.428171	22470.673775	30.089600
436.766805	22514.137553	30.094618
437.137949	22551.548768	30.099636
437.424618	22598.451230	30.104653
438.158008	22636.939927	30.109671
438.741108	22686.506495	30.114688
439.142324	22729.593062	30.119706
439.706989	22758.954883	30.124724
440.579170	22806.904410	30.129741
441.525937	22822.710624	30.134759
442.656903	22842.128836	30.139776
443.592916	22852.030173	30.144794
444.304702	22845.535177	30.149812
444.833008	22851.014199	30.154829
444.981622	22852.198768	30.159847
445.318150	22870.495148	30.164864
445.706423	22875.203319	30.169882
446.306406	22877.020145	30.174900
446.310635	22906.243107	30.179917
446.628190	22914.406196	30.184935
446.742413	22947.948557	30.189952
447.072149	22968.520107	30.194970
447.372831	22984.968178	30.199988
447.320104	23020.863255	30.205005
447.663024	23051.087994	30.210023
448.042987	23085.680801	30.215040
448.475232	23125.623076	30.220058
449.087857	23157.687579	30.225076
448.720450	23210.511423	30.230093
449.183444	23252.632548	30.235111
449.986187	23299.103560	30.240128
450.132582	23331.434883	30.245146
450.775163	23371.207998	30.250164
451.099836	23425.392109	30.255181
451.384578	23470.327457	30.260199
451.539934	23513.158362	30.265216
452.122481	23566.744977	30.270234
453.060659	23612.358803	30.275252
453.152288	23672.120724	30.280269
453.596563	23713.617470	30.285287
454.077894	23761.316283	30.290304
454.374816	23811.882710	30.295322
455.182908	23857.089452	30.300340
455.327200	23907.433946	30.305357
455.851485	23943.766152	30.310375
456.629635	23988.057204	30.315392
456.997253	24026.581552	30.320410
457.820238	24054.804185	30.325428
458.473739	24103.402947	30.330445
458.397410	24132.460602	30.335463
459.426970	24155.123873	30.340480
459.857233	24202.453250	30.345498
460.383523	24227.133020	30.350516
460.839139	24260.745854	30.355533
461.121530	24304.958434	30.360551
461.571063	24331.741221	30.365568
461.609873	24370.922183	30.370586
462.241561	24405.066560	30.375604
462.746594	24452.709313	30.380621
462.656638	24490.065418	30.385639
463.465575	24537.776595	30.390656
463.996993	24590.516162	30.395674
464.667228	24628.625092	30.400692
464.946756	24675.953101	30.405709
465.356225	24714.691436	30.410727
466.074377	24759.846534	30.415744
466.352834	24810.037791	30.420762
466.616803	24843.290082	30.425780
467.295341	24891.063264	30.430797
467.883672	24928.591990	30.435815
468.661693	24968.252197	30.440832
468.902259	25022.771806	30.445850
469.406737	25054.628908	30.450868
470.533261	25087.939664	30.455885
471.272383	25108.775686	30.460903
472.114743	25131.242511	30.465920
472.504273	25166.271581	30.470938
473.110892	25180.448524	30.475956
473.107315	25204.836087	30.480973
473.809348	25232.500279	30.485991
474.522884	25243.357117	30.491008
474.519037	25280.502039	30.496026
475.391290	25301.542410	30.501044
475.782804	25320.615110	30.506061
476.050343	25347.871325	30.511079
476.555673	25367.367894	30.516096
476.841104	25391.595474	30.521114
477.722797	25410.705212	30.526132
478.419511	25437.203903	30.531149
478.902517	25449.790551	30.536167
479.471383	25469.968798	30.541184
479.455328	25505.238896	30.546202
480.026840	25523.264558	30.551220
480.516557	25547.917536	30.556237
480.518945	25576.852615	30.561255
481.174683	25603.717342	30.566272
481.416214	25632.735746	30.571290
481.695709	25661.652832	30.576308
482.008413	25693.350323	30.581325
482.325355	25721.098765	30.586343
482.899683	25755.252805	30.591360
482.852699	25793.546516	30.596378
483.670882	25821.888855	30.601396
483.850211	25869.215867	30.606413
484.249427	25911.235206	30.611431
484.450966	25958.253273	30.616448
485.257641	26004.663792	30.621466
485.857104	26043.357744	30.626484
486.148326	26090.332762	30.631501
486.196002	26145.736176	30.636519
486.795700	26189.020264	30.641536
486.935022	26247.577250	30.646554
487.598684	26295.829685	30.651572
488.416048	26364.357728	30.656589
488.438953	26407.281283	30.661607
488.941129	26452.625246	30.666624
489.181153	26520.996968	30.671642
489.924608	26568.772688	30.676660
490.942188	26630.964907	30.681677
491.427356	26680.482263	30.686695
492.239613	26720.357224	30.691712
492.500385	26770.888319	30.696730
493.039645	26818.728821	30.701748
493.687571	26876.053658	30.706765
493.975602	26924.805859	30.711783
494.722446	26950.200796	30.716800
495.181452	27006.654883	30.721818
495.991395	27040.810363	30.726836
496.777866	27079.662164	30.731853
497.474140	27121.807520	30.736871
498.183601	27149.534505	30.741888
498.690462	27187.838632	30.746906
499.171079	27211.571444	30.751924
499.856696	27245.800739	30.756941
500.528066	27276.302589	30.761959
501.031260	27298.566491	30.766976
501.100041	27329.416547	30.771994
501.530147	27368.560598	30.777012
501.857487	27396.686088	30.782029
502.527765	27432.564889	30.787047
503.446479	27445.867645	30.792064
504.176362	27488.397820	30.797082
504.805172	27517.345322	30.802100
505.184104	27537.711639	30.807117
505.557995	27554.601056	30.812135
505.844578	27577.185062	30.817152
505.917292	27622.459691	30.822170
506.186727	27649.413011	30.827188
506.623410	27695.291695	30.832205
506.912209	27741.075881	30.837223
507.685631	27778.806333	30.842240
507.767665	27824.782846	30.847258
508.341433	27854.403131	30.852276
509.077336	27883.532782	30.857293
509.320313	27925.883234	30.862311
510.257989	27964.872241	30.867328
510.646459	28002.306824	30.872346
511.083709	28028.824333	30.877364
511.792626	28057.490579	30.882381
512.451683	28095.629216	30.887399
513.131525	28124.511373	30.892416
513.429815	28168.290803	30.897434
513.771712	28200.961646	30.902452
514.562087	28222.949433	30.907469
514.946876	28264.747125	30.912487
515.411299	28298.287423	30.917504
515.801755	28335.824890	30.922522
516.269034	28366.277788	30.927540
516.774644	28412.147523	30.932557
516.974021	28452.030625	30.937575
518.100713	28486.335698	30.942592
518.452438	28526.369637	30.947610
518.698971	28568.918183	30.952628
519.443443	28604.918566	30.957645
519.800685	28652.656385	30.962663
520.356828	28699.800072	30.967680
520.485689	28744.014618	30.972698
521.047526	28782.535962	30.977716
521.634353	28831.370802	30.982733
521.812970	28890.986934	30.987751
522.704770	28930.452042	30.992768
523.209587	28981.886457	30.997786
523.491807	29030.289760	31.002804
524.117561	29080.069422	31.007821
524.627574	29129.817243	31.012839
525.276074	29177.259636	31.017856
525.779951	29230.133808	31.022874
526.207754	29277.222389	31.027892
527.112623	29319.786233	31.032909
527.144607	29375.534914	31.037927
527.639883	29425.394724	31.042944
528.372755	29477.815597	31.047962
528.919460	29532.524647	31.052980
529.577551	29576.586235	31.057997
530.577563	29616.472316	31.063015
531.270269	29658.746190	31.068032
531.307085	29709.647541	31.073050
531.927641	29741.422913	31.078068
533.050401	29772.621921	31.083085
533.785672	29829.484674	31.088103
534.637716	29845.929963	31.093120
535.482425	29869.173705	31.098138
536.131125	29884.278729	31.103156
536.957564	29907.421420	31.108173
537.141945	29928.077039	31.113191
537.886470	29942.542759	31.118208
538.192142	29965.346109	31.123226
538.623262	29986.473128	31.128244
539.107534	29986.982252	31.133261
539.251637	30026.666825	31.138279
539.521298	30047.212875	31.143296
540.070266	30073.241549	31.148314
540.584978	30100.525502	31.153332
540.749594	30131.370332	31.158349
540.993321	30167.740768	31.163367
541.560242	30204.874616	31.168384
541.998085	30248.569638	31.173402
542.235296	30294.200584	31.178420
542.787732	30332.905185	31.183437
543.004049	30381.163809	31.188455
543.396495	30441.145550	31.193472
543.987713	30492.752211	31.198490
544.557576	30548.921981	31.203508
544.943933	30605.783117	31.208525
545.509106	30669.066834	31.213543
545.998280	30704.193672	31.218560
546.714301	30771.190634	31.223578
547.159332	30828.114119	31.228596
548.104872	30866.111175	31.233613
548.337551	30942.719598	31.238631
549.073628	30987.379369	31.243648
549.977676	31038.846511	31.248666
550.555420	31099.797247	31.253684
551.242763	31141.716459	31.258701
552.232602	31175.032412	31.263719
553.083985	31214.901946	31.268736
553.951174	31249.362939	31.273754
554.115447	31292.492776	31.278772
554.776271	31320.258279	31.283789
555.002660	31361.321548	31.288807
555.526244	31403.056307	31.293824
556.134590	31444.243358	31.298842
556.440727	31491.740692	31.303860
556.719959	31533.052886	31.308877
557.270613	31591.853582	31.313895
557.843860	31633.105014	31.318912
558.151447	31683.354653	31.323930
558.405382	31746.939550	31.328948
559.578018	31791.878740	31.333965
559.961578	31836.989435	31.338983
560.888623	31884.620712	31.344000
561.523594	31939.254387	31.349018
561.657967	31991.255331	31.354036
562.457830	32028.349903	31.359053
562.973464	32082.177127	31.364071
563.674246	32131.019428	31.369088
564.071426	32184.550609	31.374106
564.588855	32239.375806	31.379124
565.413599	32272.780182	31.384141
566.209490	32327.666931	31.389159
566.666248	32370.020056	31.394176
567.724665	32399.699085	31.399194
568.065613	32434.654623	31.404212
568.465882	32469.317064	31.409229
568.849285	32509.765518	31.414247
569.310734	32538.230009	31.419264
569.853299	32569.213095	31.424282
570.524951	32615.913038	31.429300
571.222367	32648.912867	31.434317
571.922734	32692.276236	31.439335
572.576291	32730.574738	31.444352
573.334648	32761.462344	31.449370
573.458824	32807.310562	31.454388
574.031823	32844.726834	31.459405
574.690341	32879.848688	31.464423
575.001597	32922.751306	31.469440
575.920377	32962.064219	31.474458
576.307735	33002.116023	31.479476
577.242242	33034.295446	31.484493
577.895381	33076.357442	31.489511
578.416582	33106.402310	31.494528
579.218601	33140.388995	31.499546
579.470108	33179.302700	31.504564
580.441786	33205.245377	31.509581
581.266362	33250.179356	31.514599
581.378203	33280.130526	31.519616
582.236470	33319.132359	31.524634
582.286139	33363.576864	31.529652
583.073963	33393.157336	31.534669
583.437146	33434.033728	31.539687
583.685147	33488.158790	31.544704
584.503778	33531.628483	31.549722
584.513980	33577.791757	31.554740
585.138768	33626.410977	31.559757
585.784982	33686.441347	31.564775
586.135567	33729.735456	31.569792
586.557819	33784.317677	31.574810
587.177562	33843.686026	31.579828
587.720707	33905.420323	31.584845
588.559652	33959.552122	31.589863
589.530269	34008.834643	31.594880
590.062651	34065.265117	31.599898
590.270697	34124.337462	31.604916
590.813135	34182.220174	31.609933
591.578671	34248.123027	31.614951
592.003438	34298.305188	31.619968
593.203116	34341.669028	31.624986
593.496864	34398.813344	31.630004
594.228160	34452.970199	31.635021
595.083447	34498.473338	31.640039
595.465207	34545.863342	31.645056
596.206744	34589.464739	31.650074
596.818128	34646.740613	31.655092
597.534574	34695.001542	31.660109
598.051984	34731.530768	31.665127
598.337856	34802.479624	31.670144
599.205548	34832.321099	31.675162
599.545688	34883.464379	31.680180
600.124625	34928.749432	31.685197
600.872047	34968.419150	31.690215
601.387073	35009.199557	31.695232
602.127864	35050.276751	31.700250
602.448668	35099.213534	31.705268
603.057775	35147.626869	31.710285
603.417414	35184.692997	31.715303
603.765945	35247.243623	31.720320
604.385903	35299.002595	31.725338
604.637015	35374.439861	31.730356
605.404899	35424.553426	31.735373
606.034089	35473.461111	31.740391
606.664658	35541.295014	31.745408
607.234219	35607.016881	31.750426
607.707535	35667.156014	31.755444
608.614484	35720.426639	31.760461
609.259724	35778.412025	31.765479
609.327250	35847.121953	31.770496
610.358575	35912.818783	31.775514
610.711074	35978.658654	31.780532
611.524855	36046.430740	31.785549
612.063272	36095.100867	31.790567
612.268761	36175.414346	31.795584
613.102807	36227.949312	31.800602
613.427312	36294.808634	31.805620
614.457770	36347.656397	31.810637
615.400672	36418.838554	31.815655
616.260083	36477.473350	31.820672
617.106554	36529.762906	31.825690
617.784169	36582.027486	31.830708
618.836014	36642.081139	31.835725
619.801121	36683.377307	31.840743
620.389307	36729.006310	31.845760
621.125703	36767.023418	31.850778
621.718583	36814.203328	31.855796
622.776195	36838.372151	31.860813
623.546859	36866.517314	31.865831
624.472639	36906.262556	31.870848
625.985943	36906.325858	31.875866
627.500217	36927.196242	31.880884
628.025701	36926.954881	31.885901
628.710452	36922.755957	31.890919
628.846542	36939.525755	31.895936
629.534910	36932.942334	31.900954
629.884596	36945.648169	31.905972
630.452359	36954.916839	31.910989
630.661556	36963.528380	31.916007
630.649237	37004.276215	31.921024
631.195355	37022.857045	31.926042
631.646729	37072.494602	31.931060
631.848021	37094.941253	31.936077
632.410305	37131.068094	31.941095
632.252446	37182.786456	31.946112
632.665514	37231.747874	31.951130
632.695569	37286.794989	31.956148
633.335804	37335.245948	31.961165
634.077032	37388.305450	31.966183
634.182182	37454.436450	31.971200
635.004507	37512.584100	31.976218
635.413423	37578.358177	31.981236
635.598586	37648.742239	31.986253
636.574301	37719.897875	31.991271
636.569517	37790.027381	31.996288
637.351565	37866.573831	32.001306
637.899417	37945.004305	32.006324
638.606537	38025.677172	32.011341
639.830098	38097.187547	32.016359
639.826818	38178.639660	32.021376
640.765233	38248.255059	32.026394
641.545386	38319.058042	32.031412
642.296385	38406.223707	32.036429
642.925327	38469.389713	32.041447
643.926449	38545.410807	32.046464
644.630582	38625.718031	32.051482
645.456841	38682.956097	32.056500
646.245078	38740.938369	32.061517
646.918140	38802.813472	32.066535
647.346165	38881.119132	32.071552
648.284108	38934.844396	32.076570
649.129115	38985.968623	32.081588
649.738212	39061.325943	32.086605
650.763324	39116.537501	32.091623
651.232120	39170.182101	32.096640
652.054560	39232.036560	32.101658
652.814496	39289.687761	32.106676
653.412072	39343.582051	32.111693
654.141934	39396.116664	32.116711
654.591060	39457.944657	32.121728
655.648652	39499.862181	32.126746
656.629198	39550.953914	32.131764
656.948875	39605.530353	32.136781
657.616533	39661.462902	32.141799
658.240386	39715.146031	32.146816
658.725662	39769.830667	32.151834
659.096425	39836.042179	32.156852
659.981987	39887.654665	32.161869
660.779053	39947.237086	32.166887
661.168010	40000.110117	32.171904
662.754597	40031.983136	32.176922
663.634722	40081.362534	32.181940
664.370376	40125.211019	32.186957
665.136506	40161.841725	32.191975
665.360789	40202.091192	32.196992
665.625039	40267.108646	32.202010
666.165523	40309.910030	32.207028
666.714447	40375.169578	32.212045
667.719256	40420.543490	32.217063
668.044337	40484.908674	32.222080
668.242880	40538.198474	32.227098
668.873904	40597.790679	32.232116
669.238864	40654.911700	32.237133
669.794401	40705.845900	32.242151
670.214912	40783.295702	32.247168
671.356597	40841.441747	32.252186
671.489097	40909.478967	32.257204
672.081541	40967.577266	32.262221
673.424428	41026.966155	32.267239
673.556304	41121.303128	32.272256
673.958404	41169.165802	32.277274
674.948321	41249.558153	32.282292
675.537612	41317.404403	32.287309
676.432281	41388.167204	32.292327
677.388011	41452.987586	32.297344
677.773049	41511.262685	32.302362
678.444988	41583.758703	32.307380
678.909987	41662.485987	32.312397
679.381688	41729.207607	32.317415
680.161431	41812.134194	32.322432
680.793667	41890.391147	32.327450
681.707005	41957.658415	32.332468
682.372629	42032.333766	32.337485
683.150714	42112.237116	32.342503
683.959695	42183.672925	32.347520
684.991532	42245.812486	32.352538
685.941814	42318.371373	32.357556
686.514941	42386.054075	32.362573
687.960044	42431.177106	32.367591
688.321359	42495.146596	32.372608
689.004098	42562.497102	32.377626
689.465520	42614.552817	32.382644
690.073631	42676.871799	32.387661
690.745622	42740.732801	32.392679
691.592976	42800.484308	32.397696
692.028084	42861.503492	32.402714
693.063799	42936.420350	32.407732
693.475042	42994.645816	32.412749
694.714514	43049.660865	32.417767
694.819598	43126.508981	32.422784
695.917184	43181.928732	32.427802
696.835518	43230.043006	32.432820
697.356188	43302.453612	32.437837
698.297382	43359.857781	32.442855
698.471867	43419.377866	32.447872
699.247730	43491.051481	32.452890
700.027993	43548.024487	32.457908
700.334927	43620.233857	32.462925
701.406257	43679.637287	32.467943
701.700095	43751.902917	32.472960
702.456537	43828.293970	32.477978
703.720234	43884.462404	32.482996
704.103881	43948.067767	32.488013
704.785988	44007.231443	32.493031
705.530399	44065.391689	32.498048
706.261800	44123.478489	32.503066
707.190182	44181.840126	32.508084
707.314966	44248.036766	32.513101
708.294654	44301.037151	32.518119
708.962381	44360.996147	32.523136
709.379605	44418.282182	32.528154
710.436097	44469.359101	32.533172
711.524776	44529.819512	32.538189
712.084985	44583.240869	32.543207
713.099520	44636.691013	32.548224
713.605239	44687.947747	32.553242
714.486790	44734.466283	32.558260
714.743853	44806.218453	32.563277
715.415986	44858.935096	32.568295
716.297159	44917.180526	32.573312
716.548484	44986.498846	32.578330
717.476859	45044.368074	32.583348
717.906136	45115.601945	32.588365
718.515415	45185.024963	32.593383
718.687715	45259.657087	32.598400
719.497759	45337.876047	32.603418
720.345203	45404.589844	32.608436
721.066191	45489.101880	32.613453
721.933584	45552.203859	32.618471
722.674189	45636.079345	32.623488
723.275618	45712.484404	32.628506
724.023202	45792.601994	32.633524
724.784576	45872.862884	32.638541
725.346387	45944.981352	32.643559
726.171451	46023.396592	32.648576
726.867820	46101.962027	32.653594
727.954243	46175.954034	32.658612
728.824478	46256.473837	32.663629
729.548879	46325.993476	32.668647
730.582541	46396.451692	32.673664
731.293735	46470.533073	32.678682
732.134305	46540.360040	32.683700
732.825943	46612.536304	32.688717
733.755600	46677.926184	32.693735
734.611763	46733.433538	32.698752
735.322223	46801.237735	32.703770
736.262146	46849.863395	32.708788
736.848763	46922.212251	32.713805
737.938787	46970.464128	32.718823
738.987867	47026.945042	32.723840
739.574297	47094.028646	32.728858
740.815647	47141.310348	32.733876
741.632205	47185.135436	32.738893
742.293418	47234.200930	32.743911
743.015091	47277.659573	32.748928
743.467392	47333.946195	32.753946
744.316334	47378.220963	32.758964
744.936012	47438.892299	32.763981
745.645389	47487.392351	32.768999
746.124616	47530.735606	32.774016
746.621174	47601.028575	32.779034
747.440025	47649.476938	32.784052
747.704605	47712.430219	32.789069
748.102702	47770.443343	32.794087
748.861128	47838.691950	32.799104
749.114695	47899.158100	32.804122
750.065805	47950.167296	32.809140
750.586620	48029.513936	32.814157
751.375952	48096.124143	32.819175
752.656222	48154.521888	32.824192
753.141584	48228.208006	32.829210
754.124852	48297.356588	32.834228
754.535744	48364.476114	32.839245
755.385588	48432.863921	32.844263
756.252468	48497.103035	32.849280
756.910497	48582.046986	32.854298
757.644388	48655.379772	32.859316
758.322247	48735.039050	32.864333
758.758333	48816.598912	32.869351
760.046770	48888.721032	32.874368
760.590250	48961.018829	32.879386
761.492508	49039.151189	32.884404
762.166805	49117.433780	32.889421
762.612376	49187.119509	32.894439
763.437140	49264.511016	32.899456
764.461586	49345.642002	32.904474
765.240350	49422.211598	32.909492
766.435685	49506.796746	32.914509
766.833210	49576.289687	32.919527
767.839767	49651.773185	32.924544
768.954014	49725.602077	32.929562
769.718636	49800.746040	32.934580
770.242853	49877.544295	32.939597
771.181053	49940.309880	32.944615
771.885443	50018.869342	32.949632
772.367701	50094.902062	32.954650
773.205125	50166.204930	32.959668
774.064273	50252.866801	32.964685
774.692342	50330.754984	32.969703
775.516534	50405.421800	32.974720
775.973955	50494.976363	32.979738
776.902084	50566.878614	32.984756
777.593850	50647.288991	32.989773
777.991185	50731.360021	32.994791
779.116865	50812.137574	32.999808
780.011447	50897.774432	33.004826
781.307195	50970.288832	33.009844
781.869491	51061.252828	33.014861
782.534110	51129.617348	33.019879
783.601346	51206.183383	33.024896
784.449262	51273.462043	33.029914
785.402464	51340.269742	33.034932
786.148181	51420.078522	33.039949
786.978492	51471.356895	33.044967
787.767041	51544.456148	33.049984
788.410409	51624.645064	33.055002
789.404884	51685.899252	33.060020
789.981051	51750.335213	33.065037
790.434452	51820.074127	33.070055
791.242203	51874.014612	33.075072
792.098927	51948.449125	33.080090
793.086822	51997.437876	33.085108
793.467244	52085.554523	33.090125
794.292505	52153.221965	33.095143
795.003044	52223.903055	33.100160
795.579516	52313.293075	33.105178
796.131767	52392.347929	33.110196
796.981030	52462.667012	33.115213
797.699731	52550.094542	33.120231
798.509545	52641.828785	33.125248
799.141794	52731.524455	33.130266
799.948486	52803.246672	33.135284
800.651840	52894.150122	33.140301
800.937689	52990.053662	33.145319
802.155481	53073.935592	33.150336
802.840357	53169.953323	33.155354
803.989838	53258.335180	33.160372
805.170352	53350.465358	33.165389
805.430119	53439.485245	33.170407
806.709180	53514.777473	33.175424
808.163835	53592.046338	33.180442
809.154691	53663.973064	33.185460
809.718880	53741.128627	33.190477
810.854493	53818.430299	33.195495
811.658168	53898.553280	33.200512
812.190314	53977.854978	33.205530
813.435083	54044.547367	33.210548
814.436192	54115.858752	33.215565
814.938513	54197.656572	33.220583
815.894511	54272.340512	33.225600
816.553321	54344.834126	33.230618
817.446338	54417.780007	33.235636
818.153518	54486.945877	33.240653
818.775723	54565.399330	33.245671
819.641195	54635.534868	33.250688
820.390334	54727.188293	33.255706
821.093928	54800.576202	33.260724
822.191813	54884.438231	33.265741
822.651639	54973.102329	33.270759
823.192983	55054.017092	33.275776
824.669802	55126.465693	33.280794
825.840549	55200.882513	33.285812
826.741333	55263.397946	33.290829
827.406334	55340.837799	33.295847
828.221827	55413.124477	33.300864
828.745447	55501.739946	33.305882
829.523375	55578.335785	33.310900
830.492551	55658.604302	33.315917
831.326531	55737.578342	33.320935
832.216026	55799.923786	33.325952
833.554812	55874.281880	33.330970
834.539380	55940.561737	33.335988
835.275279	55986.173151	33.341005
835.882936	56042.228689	33.346023
836.834544	56095.328593	33.351040
837.372525	56166.576482	33.356058
838.059057	56231.291710	33.361076
838.760079	56296.345794	33.366093
839.448559	56364.931417	33.371111
840.185766	56436.464327	33.376128
841.246357	56496.600389	33.381146
842.526780	56566.661505	33.386164
843.133752	56623.808038	33.391181
844.046887	56706.801797	33.396199
845.185435	56764.647073	33.401216
845.891676	56841.666828	33.406234
846.719710	56918.661208	33.411252
847.421361	56984.693110	33.416269
847.675182	57063.064340	33.421287
848.603537	57129.859385	33.426304
849.261665	57213.558967	33.431322
850.025321	57305.781736	33.436340
850.868849	57382.870296	33.441357
851.571887	57469.746130	33.446375
852.550726	57568.448854	33.451392
852.936257	57662.747755	33.456410
853.560327	57752.267289	33.461428
854.635548	57856.039053	33.466445
855.442270	57954.269252	33.471463
856.451737	58044.382379	33.476480
857.340646	58143.181405	33.481498
858.140306	58234.181265	33.486516
858.797041	58329.977918	33.491533
859.525523	58431.623339	33.496551
860.554618	58526.105196	33.501568
861.200034	58635.976775	33.506586
862.151095	58745.304679	33.511604
863.370787	58818.538060	33.516621
864.305050	58927.336136	33.521639
864.869140	59025.468532	33.526656
866.005198	59130.718492	33.531674
866.686416	59235.927767	33.536692
867.927997	59326.221710	33.541709
868.411293	59429.758624	33.546727
869.904017	59523.492936	33.551744
870.832317	59622.823980	33.556762
871.476464	59721.698748	33.561780
872.844306	59803.443670	33.566797
873.590331	59901.551717	33.571815
874.792111	59977.321590	33.576832
875.552673	60070.142682	33.581850
876.550974	60150.176605	33.586868
877.995877	60221.141027	33.591885
879.250363	60287.096689	33.596903
880.503807	60357.125907	33.601920
880.912664	60423.658665	33.606938
881.746562	60484.074235	33.611956
882.480658	60548.935880	33.616973
883.060488	60620.254187	33.621991
883.770165	60681.252200	33.627008
884.453956	60762.279735	33.632026
885.035109	60834.084908	33.637044
885.856889	60909.805354	33.642061
886.212774	61002.745978	33.647079
886.715514	61094.280658	33.652096
888.279460	61187.573067	33.657114
888.292568	61282.120009	33.662132
889.639852	61373.610071	33.667149
890.078920	61489.796021	33.672167
890.617313	61579.360150	33.677184
891.346142	61691.923571	33.682202
892.100156	61791.726432	33.687220
893.472470	61904.195038	33.692237
893.939415	62019.663002	33.697255
894.939076	62134.402713	33.702272
896.076621	62246.490729	33.707290
896.898738	62355.260206	33.712308
897.776462	62464.021459	33.717325
898.877098	62588.095059	33.722343
899.927390	62685.644988	33.727360
900.964292	62795.443861	33.732378
901.628060	62904.478527	33.737396
902.994174	63006.681986	33.742413
903.622885	63131.686875	33.747431
904.497973	63229.030629	33.752448
905.559944	63343.644581	33.757466
906.178134	63460.455175	33.762484
907.441009	63566.777164	33.767501
908.471429	63674.106254	33.772519
909.400029	63772.189569	33.777536
910.303331	63890.650151	33.782554
911.244596	63996.201453	33.787572
912.488389	64100.543018	33.792589
913.141201	64219.462368	33.797607
913.854705	64320.147126	33.802624
914.694843	64422.239754	33.807642
915.752384	64539.985024	33.812660
916.870961	64646.414945	33.817677
917.800034	64758.127728	33.822695
918.874542	64865.074351	33.827712
919.578222	64975.737832	33.832730
920.590437	65077.973964	33.837748
921.897472	65176.462217	33.842765
922.857569	65283.353578	33.847783
924.283032	65374.664130	33.852800
925.235845	65447.394044	33.857818
926.365152	65566.195397	33.862836
927.209319	65651.782076	33.867853
928.229100	65740.790144	33.872871
928.689310	65839.422855	33.877888
929.506608	65929.812650	33.882906
930.171850	66017.033894	33.887924
931.426877	66105.260829	33.892941
931.830480	66202.325182	33.897959
932.746933	66283.768750	33.902976
933.673573	66375.807751	33.907994
934.238881	66488.090662	33.913012
935.137947	66573.600053	33.918029
935.964398	66676.209033	33.923047
936.769192	66778.183976	33.928064
937.657504	66893.645885	33.933082
938.181787	67013.594741	33.938100
939.300806	67118.427382	33.943117
940.224210	67238.370981	33.948135
940.934902	67352.234031	33.953152
941.780868	67465.608745	33.958170
942.582015	67584.942205	33.963188
943.435079	67716.700784	33.968205
944.724789	67844.903554	33.973223
946.065476	67964.665215	33.978240
947.359139	68070.189084	33.983258
948.101979	68187.457052	33.988276
949.663836	68285.699502	33.993293
950.568448	68409.450185	33.998311
951.427632	68513.434588	34.003328
952.605164	68620.881535	34.008346
953.608068	68714.710560	34.013364
954.929114	68810.466879	34.018381
955.873961	68914.212348	34.023399
957.477932	69004.560803	34.028416
958.603670	69086.462984	34.033434
959.363556	69197.839758	34.038452
960.830161	69267.722401	34.043469
961.590377	69371.802932	34.048487
962.282845	69455.222398	34.053504
963.879291	69533.545094	34.058522
964.342396	69627.388563	34.063540
965.189596	69714.354197	34.068557
966.182066	69806.793833	34.073575
966.928061	69905.824996	34.078592
967.952098	70000.035909	34.083610
968.401626	70106.419021	34.088628
969.361919	70200.552581	34.093645
970.314610	70308.695335	34.098663
971.091004	70421.820257	34.103680
971.948273	70519.630016	34.108698
972.445219	70636.616886	34.113716
973.764797	70742.953472	34.118733
974.366246	70870.805356	34.123751
975.565313	70985.616469	34.128768
976.138624	71099.719035	34.133786
976.701863	71233.423948	34.138804
978.172894	71340.289368	34.143821
979.340028	71468.213081	34.148839
980.120437	71584.023108	34.153856
981.418048	71674.805381	34.158874
982.122892	71794.186072	34.163892
983.261766	71896.191377	34.168909
984.234745	72005.989380	34.173927
985.019052	72106.643086	34.178944
986.469838	72211.481771	34.183962
986.925952	72322.873955	34.188980
988.038149	72431.274644	34.193997
989.308735	72530.898981	34.199015
990.067398	72650.623794	34.204032
991.622568	72756.068006	34.209050
992.387418	72868.298787	34.214068
993.612378	72966.460223	34.219085
994.471604	73077.040521	34.224103
995.040760	73186.422703	34.229120
996.334655	73291.127735	34.234138
997.323998	73399.224634	34.239156
998.281852	73507.314488	34.244173
999.343020	73634.302135	34.249191
1000.116592	73745.171483	34.254208
1001.201221	73844.692937	34.259226
1002.101982	73961.849975	34.264244
1003.209574	74080.535694	34.269261
1004.050512	74192.275198	34.274279
1004.749814	74315.918531	34.279296
1006.034214	74437.023882	34.284314
1006.855929	74566.140969	34.289332
1008.102928	74681.957930	34.294349
1008.923639	74800.219564	34.299367
1009.674064	74941.294560	34.304384
1010.879140	75062.403653	34.309402
1012.619277	75173.152396	34.314420
1013.952807	75290.614874	34.319437
1015.033767	75398.360364	34.324455
1016.123833	75503.482230	34.329472
1017.053842	75609.969925	34.334490
1017.838406	75732.255914	34.339508
1019.183773	75848.607443	34.344525
1020.151204	75958.567014	34.349543
1020.678228	76078.039407	34.354560
1021.633484	76186.624378	34.359578
1022.784646	76301.562099	34.364596
1023.932639	76428.755781	34.369613
1024.681985	76545.572688	34.374631
1025.440829	76677.146528	34.379648
1026.664596	76795.589552	34.384666
1027.420325	76915.782600	34.389684
1028.420220	77039.894064	34.394701
1029.781725	77162.349701	34.399719
1030.533071	77301.614370	34.404736
1031.741973	77426.535558	34.409754
1032.538315	77546.005325	34.414772
1033.636974	77670.585273	34.419789
1034.942553	77793.540277	34.424807
1035.815904	77928.428599	34.429824
1036.763262	78047.302094	34.434842
1037.548789	78177.629861	34.439860
1038.758461	78294.048551	34.444877
1040.116712	78394.326279	34.449895
1040.868949	78513.739177	34.454912
1042.497541	78616.168312	34.459930
1043.282631	78729.231109	34.464948
1044.205365	78834.655932	34.469965
1045.618252	78955.173604	34.474983
1046.411064	79068.350813	34.480000
1048.324646	79145.244745	34.485018
1049.922842	79244.262186	34.490036
1050.655295	79346.616269	34.495053
1051.942426	79432.681659	34.500071
1052.419786	79542.049456	34.505088
1053.574038	79655.842441	34.510106
1054.587560	79741.649225	34.515124
1055.431630	79865.928991	34.520141
1056.291440	79960.168366	34.525159
1057.059929	80079.296970	34.530176
1058.321068	80201.122963	34.535194
1058.814358	80317.401538	34.540212
1059.704626	80438.086854	34.545229
1060.740788	80575.868130	34.550247
1061.559090	80707.628990	34.555264
1062.294592	80832.759933	34.560282
1063.480520	80977.461083	34.565300
1064.624059	81113.224906	34.570317
1065.687221	81252.953429	34.575335
1066.407034	81404.995264	34.580352
1068.079059	81535.765826	34.585370
1068.645172	81670.152152	34.590388
1069.745951	81809.378998	34.595405
1071.252964	81945.874335	34.600423
1072.821224	82073.326829	34.605440
1074.013602	82198.488125	34.610458
1075.488298	82328.827218	34.615476
1076.607174	82450.651065	34.620493
1077.824844	82576.000255	34.625511
1078.819877	82698.806194	34.630528
1080.506239	82805.621730	34.635546
1081.565886	82915.534187	34.640564
1082.612732	83029.969618	34.645581
1083.700591	83144.304315	34.650599
1084.648381	83266.191717	34.655616
1085.631401	83388.674839	34.660634
1086.221432	83513.004073	34.665652
1087.019661	83639.469498	34.670669
1088.298152	83760.902532	34.675687
1089.225438	83894.063351	34.680704
1090.540706	84018.115831	34.685722
1091.808114	84150.193605	34.690740
1092.439396	84288.367163	34.695757
1093.373742	84409.017754	34.700775
1094.231078	84542.769135	34.705792
1095.258678	84684.669503	34.710810
1096.406230	84811.705998	34.715828
1097.097805	84933.005159	34.720845
1098.172190	85079.117999	34.725863
1098.933554	85216.897541	34.730880
1099.840013	85333.353131	34.735898
1101.308308	85470.136680	34.740916
1102.584128	85612.591794	34.745933
1103.592114	85746.478535	34.750951
1104.656569	85889.114539	34.755968
1105.292586	86020.223109	34.760986
1106.854500	86170.350599	34.766004
1108.155067	86313.242747	34.771021
1108.891366	86457.458611	34.776039
1109.317836	86607.074186	34.781056
1110.934265	86749.128602	34.786074
1112.439466	86895.956794	34.791092
1113.512873	87043.139213	34.796109
1114.791627	87184.447143	34.801127
1115.855368	87327.073858	34.806144
1117.144552	87471.227571	34.811162
1118.203983	87629.102941	34.816180
1119.240042	87781.456362	34.821197
1120.769096	87920.838564	34.826215
1121.199810	88080.227388	34.831232
1122.555213	88224.647521	34.836250
1123.409398	88379.626808	34.841268
1124.272949	88527.870854	34.846285
1125.760132	88674.948007	34.851303
1127.094180	88836.911673	34.856320
1128.003208	88996.332347	34.861338
1129.500452	89138.781916	34.866356
1131.182344	89291.258266	34.871373
1132.370515	89431.102808	34.876391
1133.487205	89579.990452	34.881408
1134.688752	89726.905130	34.886426
1135.954071	89873.393259	34.891444
1136.977779	90021.116075	34.896461
1138.164890	90153.344704	34.901479
1138.999124	90304.596895	34.906496
1140.453759	90444.171555	34.911514
1141.757672	90587.502474	34.916532
1142.543228	90738.082361	34.921549
1143.957334	90875.832126	34.926567
1145.178496	91024.833158	34.931584
1146.511976	91159.435258	34.936602
1147.837647	91301.546739	34.941620
1148.361455	91439.821092	34.946637
1149.978396	91577.530353	34.951655
1150.891456	91732.353290	34.956672
1152.031871	91877.204932	34.961690
1153.244267	92017.890672	34.966708
1153.971942	92161.955962	34.971725
1154.875571	92316.841418	34.976743
1155.667167	92475.161243	34.981760
1156.655794	92626.645176	34.986778
1157.830995	92773.489526	34.991796
1159.104642	92928.206564	34.996813
1159.911245	93069.418915	35.001831
1161.273269	93223.080310	35.006848
1162.399332	93369.968042	35.011866
1163.164726	93520.898999	35.016884
1164.113422	93682.706630	35.021901
1165.523504	93838.104082	35.026919
1166.624228	94009.789062	35.031936
1167.695272	94164.395094	35.036954
1168.982044	94324.211707	35.041972
1169.861930	94505.316284	35.046989
1170.863169	94658.355445	35.052007
1172.118130	94834.766400	35.057024
1173.704229	94986.165024	35.062042
1175.501114	95151.536262	35.067060
1176.660844	95309.064885	35.072077
1178.410984	95460.288804	35.077095
1179.738729	95612.200835	35.082112
1181.033330	95765.934686	35.087130
1182.128509	95905.271873	35.092148
1183.316202	96060.878226	35.097165
1184.675878	96199.251581	35.102183
1186.192684	96346.008105	35.107200
1187.334147	96477.364325	35.112218
1188.898662	96618.927651	35.117236
1190.033005	96752.418499	35.122253
1191.380149	96885.680186	35.127271
1192.796793	97030.989398	35.132288
1193.710484	97167.978222	35.137306
1195.049830	97314.978002	35.142324
1195.716067	97462.515946	35.147341
1196.875843	97595.438330	35.152359
1197.940622	97750.632964	35.157376
1199.342798	97899.353639	35.162394
1200.291594	98047.173086	35.167412
1201.164330	98207.810528	35.172429
1202.447439	98355.091665	35.177447
1203.552196	98502.560273	35.182464
1203.958319	98676.750933	35.187482
1205.540869	98835.388237	35.192500
1206.733961	99011.721283	35.197517
1207.808057	99172.801647	35.202535
1209.128536	99341.796837	35.207552
1209.756759	99507.942334	35.212570
1211.093576	99673.324689	35.217588
1212.051364	99864.785150	35.222605
1213.529737	100040.485968	35.227623
1214.557215	100213.931434	35.232640
1216.066597	100389.262998	35.237658
1217.837774	100551.678413	35.242676
1219.159279	100713.698244	35.247693
1220.928509	100877.267809	35.252711
1222.220424	101030.771702	35.257728
1223.554281	101177.872969	35.262746
1224.653002	101316.154178	35.267764
1225.625426	101461.391167	35.272781
1227.040785	101603.660653	35.277799
1228.136509	101739.078496	35.282816
1229.272591	101879.805858	35.287834
1230.664526	102025.340331	35.292852
1231.675150	102181.699647	35.297869
1232.583768	102325.585381	35.302887
1234.137096	102475.652925	35.307904
1235.267380	102625.870947	35.312922
1236.542779	102773.580035	35.317940
1237.671024	102926.299784	35.322957
1239.020653	103079.567494	35.327975
1240.306967	103230.669463	35.332992
1241.360737	103400.027585	35.338010
1242.315428	103549.361862	35.343028
1243.906601	103711.207701	35.348045
1244.942443	103879.211578	35.353063
1246.184383	104040.507694	35.358080
1246.958549	104208.795979	35.363098
1248.472589	104363.393787	35.368116
1249.509739	104540.033842	35.373133
1250.717037	104700.479309	35.378151
1252.053511	104873.277266	35.383168
1253.132511	105056.736479	35.388186
1254.699903	105226.880331	35.393204
1255.892990	105401.483211	35.398221
1257.304960	105574.261592	35.403239
1258.419016	105759.334411	35.408256
1259.738466	105932.592077	35.413274
1260.974522	106112.351159	35.418292
1262.254347	106293.515938	35.423309
1263.472832	106468.882013	35.428327
1264.921336	106646.067148	35.433344
1265.520957	106837.394341	35.438362
1266.813749	107008.303332	35.443380
1268.529448	107197.493995	35.448397
1269.879806	107387.446741	35.453415
1270.945636	107560.674173	35.458432
1271.728169	107756.295991	35.463450
1273.243560	107932.296391	35.468468
1274.825453	108124.344713	35.473485
1276.441740	108299.097540	35.478503
1278.461053	108472.622967	35.483520
1279.759867	108643.934966	35.488538
1280.872591	108808.366052	35.493556
1282.050857	108996.504238	35.498573
1283.819359	109160.681550	35.503591
1285.252489	109331.711192	35.508608
1286.303700	109485.054623	35.513626
1287.422871	109659.067051	35.518644
1288.875400	109831.831419	35.523661
1290.084224	109995.533632	35.528679
1291.561836	110148.357695	35.533696
1292.904925	110315.547376	35.538714
1294.493429	110466.279621	35.543732
1295.969510	110602.864438	35.548749
1297.290379	110745.393135	35.553767
1298.359803	110888.696896	35.558784
1299.238690	111037.399587	35.563802
1300.281260	111181.032141	35.568820
1301.342476	111331.220489	35.573837
1302.473520	111499.882491	35.578855
1303.924413	111645.573416	35.583872
1305.109453	111819.445032	35.588890
1306.363377	111971.600630	35.593908
1307.798950	112140.573074	35.598925
1308.789456	112306.040795	35.603943
1310.105449	112478.535192	35.608960
1311.516582	112656.022989	35.613978
1312.666850	112828.014393	35.618996
1314.121745	113001.376584	35.624013
1315.079452	113183.067662	35.629031
1316.691501	113354.482845	35.634048
1317.719495	113539.071056	35.639066
1319.121529	113719.916734	35.644084
1320.545184	113893.505304	35.649101
1321.981685	114070.024161	35.654119
1323.865437	114242.516430	35.659136
1325.808528	114403.440371	35.664154
1327.058195	114561.746955	35.669172
1328.554168	114735.272854	35.674189
1329.605857	114892.815285	35.679207
1331.524225	115040.996708	35.684224
1333.036995	115205.311589	35.689242
1334.262937	115348.717321	35.694260
1335.546088	115514.216620	35.699277
1337.024008	115674.855384	35.704295
1338.689530	115824.721340	35.709312
1340.099444	115985.290568	35.714330
1341.217676	116126.685489	35.719348
1342.524416	116279.548846	35.724365
1343.840223	116447.283964	35.729383
1345.435609	116586.712529	35.734400
1346.723166	116751.307444	35.739418
1347.993673	116905.085692	35.744436
1349.075713	117069.727980	35.749453
1350.200531	117221.156972	35.754471
1351.303730	117392.306766	35.759488
1352.389963	117556.856534	35.764506
1354.169518	117720.720984	35.769524
1355.417973	117891.870008	35.774541
1356.109579	118067.648515	35.779559
1357.811918	118229.249047	35.784576
1358.971357	118415.985508	35.789594
1360.318176	118587.351450	35.794612
1362.038967	118760.862589	35.799629
1362.865059	118936.815576	35.804647
1364.659944	119114.977616	35.809664
1365.384410	119285.187007	35.814682
1366.782184	119457.779005	35.819700
1368.492979	119608.653938	35.824717
1369.590074	119792.415110	35.829735
1370.901913	119944.229223	35.834752
1372.048429	120114.687225	35.839770
1373.357993	120284.284566	35.844788
1374.606031	120461.339575	35.849805
1376.143840	120637.007269	35.854823
1377.020225	120813.376498	35.859840
1378.205346	121008.733151	35.864858
1379.349605	121191.420110	35.869876
1380.781566	121387.056963	35.874893
1381.436633	121588.594039	35.879911
1383.310294	121785.822785	35.884928
1384.291960	121994.238939	35.889946
1385.625692	122197.673921	35.894964
1387.472684	122411.161334	35.899981
1389.161679	122612.909183	35.904999
1390.785601	122796.404911	35.910016
1392.233848	122993.684905	35.915034
1393.851072	123196.094533	35.920052
1396.021942	123375.403570	35.925069
1398.323011	123553.971154	35.930087
1400.324743	123706.140540	35.935104
1401.832656	123874.120733	35.940122
1403.360417	124045.632728	35.945140
1404.909168	124202.158131	35.950157
1405.952499	124362.184710	35.955175
1407.738102	124514.317027	35.960192
1408.894384	124667.398872	35.965210
1410.242812	124834.675745	35.970228
1411.577309	124996.344489	35.975245
1412.641289	125173.675410	35.980263
1414.075918	125327.312104	35.985280
1415.244574	125503.399857	35.990298
1416.288323	125675.366464	35.995316
1417.485738	125870.097981	36.000333
1418.410443	126059.541307	36.005351
1420.134189	126240.371854	36.010368
1421.507841	126428.074311	36.015386
1422.433467	126626.743322	36.020404
1424.023994	126827.296936	36.025421
1424.954227	127038.293796	36.030439
1426.311704	127231.932827	36.035456
1427.413425	127438.725138	36.040474
1429.008077	127651.787342	36.045492
1430.943372	127857.474909	36.050509
1432.351608	128059.510644	36.055527
1433.670796	128262.157416	36.060544
1434.867029	128478.849100	36.065562
1436.325650	128685.467354	36.070580
1437.832731	128900.782753	36.075597
1439.338993	129116.746052	36.080615
1440.669574	129320.285548	36.085632
1442.234137	129525.715019	36.090650
1443.645361	129712.230297	36.095668
1445.163678	129912.526373	36.100685
1446.145849	130104.180051	36.105703
1447.521871	130299.940627	36.110720
1449.173392	130508.720838	36.115738
1450.466154	130698.821581	36.120756
1452.006266	130914.742704	36.125773
1453.231063	131126.382586	36.130791
1454.676333	131323.710310	36.135808
1456.143366	131542.207118	36.140826
1457.417444	131744.556865	36.145844
1458.756766	131956.932286	36.150861
1459.859671	132192.254303	36.155879
1461.418932	132405.472364	36.160896
1462.540887	132638.096297	36.165914
1463.928536	132861.937370	36.170932
1465.169862	133103.466053	36.175949
1466.681307	133336.363216	36.180967
1468.342335	133575.928614	36.185984
1469.705374	133822.854391	36.191002
1471.662867	134049.389094	36.196020
1473.427448	134288.310429	36.201037
1474.664962	134522.705211	36.206055
1476.629466	134753.045649	36.211072
1478.423635	134967.778628	36.216090
1479.717112	135207.048497	36.221108
1481.538674	135423.896619	36.226125
1482.674313	135670.924979	36.231143
1484.163948	135889.920117	36.236160
1485.874646	136123.657063	36.241178
1487.371998	136350.929101	36.246196
1489.182133	136584.020332	36.251213
1490.567373	136805.142451	36.256231
1492.473271	137013.916861	36.261248
1493.958404	137246.760851	36.266266
1495.509798	137468.837322	36.271284
1497.214538	137696.289563	36.276301
1498.834489	137920.956392	36.281319
1500.273933	138136.656024	36.286336
1501.934575	138360.711433	36.291354
1503.054525	138577.060639	36.296372
1504.624727	138796.951667	36.301389
1505.931075	139031.472877	36.306407
1507.685416	139249.956629	36.311424
1509.242222	139463.480115	36.316442
1510.626008	139699.603754	36.321460
1512.590902	139902.229861	36.326477
1514.083501	140125.387359	36.331495
1515.464740	140348.031911	36.336512
1516.899832	140560.049017	36.341530
1518.587653	140778.744550	36.346548
1520.285275	141000.050920	36.351565
1521.498269	141223.184898	36.356583
1522.944714	141447.360720	36.361600
1524.658375	141658.149891	36.366618
1525.656144	141875.733555	36.371636
1527.060076	142072.290958	36.376653
1528.359286	142288.752360	36.381671
1529.938842	142498.085728	36.386688
1531.412243	142708.337282	36.391706
1533.132646	142922.163311	36.396724
1534.336908	143131.966205	36.401741
1535.811784	143364.339419	36.406759
1537.381753	143571.539567	36.411776
1539.325518	143798.112500	36.416794
1540.415159	144016.736060	36.421812
1542.124169	144228.722379	36.426829
1543.609543	144462.762612	36.431847
1545.422752	144685.623555	36.436864
1546.821274	144910.022317	36.441882
1548.443578	145130.267590	36.446900
1550.352775	145353.460290	36.451917
1551.583051	145578.891947	36.456935
1553.313299	145801.888101	36.461952
1554.901647	146026.404132	36.466970
1555.969785	146264.757854	36.471988
1557.730017	146485.370992	36.477005
1558.963742	146714.410228	36.482023
1560.406033	146958.021058	36.487040
1561.962093	147206.077768	36.492058
1563.245918	147442.073623	36.497076
1565.221356	147678.557165	36.502093
1566.829558	147928.639466	36.507111
1568.419030	148179.740836	36.512128
1570.165897	148415.898510	36.517146
1571.350862	148669.210350	36.522164
1573.327756	148914.893576	36.527181
1575.121576	149164.068616	36.532199
1576.665277	149410.597730	36.537216
1578.342263	149648.841923	36.542234
1579.920758	149888.168415	36.547252
1581.572527	150133.557565	36.552269
1582.754731	150386.249393	36.557287
1583.927983	150635.090569	36.562304
1585.677508	150889.978171	36.567322
1587.300853	151146.802162	36.572340
1589.055768	151401.692882	36.577357
1590.629488	151645.356192	36.582375
1592.430971	151901.371735	36.587392
1594.545879	152150.176237	36.592410
1595.764112	152411.372366	36.597428
1597.531729	152656.546414	36.602445
1598.994641	152908.858000	36.607463
1600.508220	153151.058535	36.612480
1602.337072	153401.325170	36.617498
1603.692113	153665.222653	36.622516
1605.231192	153913.092112	36.627533
1607.109026	154156.509960	36.632551
1608.745856	154417.008638	36.637568
1610.167833	154663.051058	36.642586
1611.624625	154904.322305	36.647604
1613.443398	155130.259062	36.652621
1614.794150	155369.711943	36.657639
1616.208677	155604.109897	36.662656
1617.762786	155826.961454	36.667674
1619.202070	156081.823782	36.672692
1620.627988	156320.840286	36.677709
1622.425725	156574.495480	36.682727
1623.789650	156811.585212	36.687744
1625.802773	157055.991354	36.692762
1627.111661	157313.622436	36.697780
1629.190611	157554.914997	36.702797
1630.813822	157812.842243	36.707815
1632.110959	158076.529420	36.712832
1634.047397	158325.838698	36.717850
1635.099279	158586.829673	36.722868
1636.944410	158840.012056	36.727885
1638.434165	159103.473500	36.732903
1640.078052	159365.771154	36.737920
1641.932259	159638.955768	36.742938
1643.319170	159906.966702	36.747956
1645.265354	160171.061104	36.752973
1647.172259	160438.651087	36.757991
1648.956077	160699.046883	36.763008
1650.938514	160957.561535	36.768026
1652.511439	161221.735697	36.773044
1654.076958	161487.193840	36.778061
1655.778130	161753.355270	36.783079
1657.119535	162021.414682	36.788096
1658.663636	162281.416180	36.793114
1660.087635	162564.558111	36.798132
1661.782769	162835.015031	36.803149
1663.775608	163110.486931	36.808167
1665.385291	163382.775067	36.813184
1667.713728	163643.295886	36.818202
1669.625548	163907.093415	36.823220
1671.403738	164170.292613	36.828237
1673.087048	164435.855074	36.833255
1674.266815	164696.781389	36.838272
1676.446335	164963.866896	36.843290
1678.131260	165226.466978	36.848308
1679.808974	165480.090413	36.853325
1682.098746	165742.281019	36.858343
1683.182740	166006.389869	36.863360
1685.006033	166257.636384	36.868378
1686.772660	166528.730536	36.873396
1688.429298	166794.529696	36.878413
1690.224813	167049.971502	36.883431
1691.820039	167318.536462	36.888448
1693.600848	167575.772567	36.893466
1694.917174	167848.216084	36.898484
1696.539183	168104.339433	36.903501
1698.391388	168365.679164	36.908519
1699.785359	168643.329196	36.913536
1701.483034	168898.329644	36.918554
1703.114151	169153.875098	36.923572
1704.863912	169409.175089	36.928589
1706.585427	169657.454033	36.933607
1707.899618	169897.833319	36.938624
1709.656499	170158.654928	36.943642
1710.830388	170415.346829	36.948660
1712.560512	170685.613684	36.953677
1714.233181	170936.394784	36.958695
1715.848753	171218.873735	36.963712
1717.728354	171480.915135	36.968730
1719.082668	171761.663552	36.973748
1720.753048	172035.995766	36.978765
1722.590315	172308.692341	36.983783
1724.146339	172599.918165	36.988800
1725.821464	172883.376334	36.993818
1727.561845	173167.105239	36.998836
1729.611298	173450.076682	37.003853
1731.372650	173725.801514	37.008871
1732.934391	174020.385823	37.013888
1734.836629	174298.401041	37.018906
1736.550537	174593.142968	37.023924
1738.135554	174888.097791	37.028941
1740.413920	175169.230803	37.033959
1742.384474	175451.137746	37.038976
1744.481718	175731.275787	37.043994
1746.354139	176012.352179	37.049012
1748.463581	176295.930183	37.054029
1750.832439	176556.823181	37.059047
1752.015044	176836.479611	37.064064
1754.347188	177095.123580	37.069082
1756.315573	177358.838252	37.074100
1757.876974	177623.887907	37.079117
1759.967783	177883.628103	37.084135
1761.892222	178139.247613	37.089152
1763.936864	178387.985786	37.094170
1765.801037	178632.757568	37.099188
1767.819797	178881.528133	37.104205
1770.031809	179123.735428	37.109223
1771.499702	179375.476400	37.114240
1773.289964	179617.055643	37.119258
1774.880765	179856.599824	37.124276
1776.584108	180112.723076	37.129293
1778.408257	180349.213274	37.134311
1780.265846	180611.151414	37.139328
1781.950893	180851.460136	37.144346
1783.890255	181106.815921	37.149364
1785.309542	181355.759447	37.154381
1787.275776	181610.390701	37.159399
1788.249991	181868.987408	37.164416
1790.333894	182135.606158	37.169434
1791.963222	182406.917282	37.174452
1793.261493	182666.621887	37.179469
1795.248679	182947.700438	37.184487
1796.723423	183208.243032	37.189504
1798.983259	183450.492250	37.194522
1800.520575	183718.577698	37.199540
1801.794245	183962.064793	37.204557
1803.695619	184209.970833	37.209575
1804.805367	184477.976430	37.214592
1806.563271	184733.775329	37.219610
1808.410935	184996.438958	37.224628
1809.748250	185275.224331	37.229645
1811.498659	185541.865601	37.234663
1812.997941	185825.412507	37.239680
1814.871905	186111.997927	37.244698
1816.222647	186405.482485	37.249716
1817.891852	186711.722213	37.254733
1819.786921	187002.002508	37.259751
1821.467811	187308.079359	37.264768
1823.334636	187607.555345	37.269786
1825.310262	187918.754207	37.274804
1827.064497	188222.985367	37.279821
1828.940517	188531.742233	37.284839
1831.007187	188851.105266	37.289856
1832.733097	189150.346950	37.294874
1834.593078	189471.688585	37.299892
1835.986260	189794.172478	37.304909
1838.166283	190107.916755	37.309927
1840.687869	190420.745902	37.314944
1843.169486	190722.466351	37.319962
1845.661142	191023.400260	37.324980
1847.581070	191321.596715	37.329997
1849.665833	191610.910546	37.335015
1851.533368	191892.506350	37.340032
1853.350077	192175.038286	37.345050
1855.474105	192469.896957	37.350068
1857.007437	192760.726487	37.355085
1859.119461	193049.536790	37.360103
1860.704353	193347.798685	37.365120
1862.703562	193638.546705	37.370138
1864.486697	193929.774909	37.375156
1865.929507	194220.665374	37.380173
1867.909802	194533.961883	37.385191
1869.859974	194829.928149	37.390208
1871.703625	195125.722664	37.395226
1873.335553	195440.958439	37.400244
1875.134541	195746.472948	37.405261
1876.955682	196045.297032	37.410279
1878.635025	196357.446715	37.415296
1880.399020	196674.293653	37.420314
1882.652393	196987.942542	37.425332
1884.320916	197313.490043	37.430349
1886.458891	197625.485667	37.435367
1887.992217	197939.406822	37.440384
1889.985118	198262.243262	37.445402
1891.931944	198580.049979	37.450420
1893.540947	198906.733667	37.455437
1895.604881	199216.326053	37.460455
1897.582750	199544.655913	37.465472
1899.358707	199845.679128	37.470490
1901.265123	200145.680554	37.475508
1903.050126	200452.430252	37.480525
1905.286817	200748.930047	37.485543
1906.454804	201049.409021	37.490560
1908.332081	201343.798509	37.495578
1910.380526	201645.410322	37.500596
1911.650382	201962.024069	37.505613
1913.819543	202263.708922	37.510631
1915.999891	202583.456618	37.515648
1917.645845	202902.097727	37.520666
1919.511826	203219.487111	37.525684
1921.036954	203550.235479	37.530701
1923.165625	203864.832207	37.535719
1924.706129	204199.199637	37.540736
1926.881786	204523.858825	37.545754
1929.142453	204853.990195	37.550772
1930.675475	205199.814667	37.555789
1932.927511	205528.148645	37.560807
1934.876442	205866.929209	37.565824
1936.650809	206203.048203	37.570842
1938.913765	206543.725047	37.575860
1940.659209	206886.923311	37.580877
1942.678157	207234.688281	37.585895
1944.392375	207577.209927	37.590912
1946.660354	207912.371539	37.595930
1949.100314	208244.879877	37.600948
1951.086285	208588.506622	37.605965
1953.317073	208930.255667	37.610983
1955.517480	209251.915181	37.616000
1957.498490	209585.734994	37.621018
1959.823140	209918.448364	37.626036
1961.397061	210251.003326	37.631053
1963.777470	210581.146913	37.636071
1965.361416	210916.077799	37.641088
1967.836365	211249.218657	37.646106
1969.721470	211564.427231	37.651124
1971.241997	211911.891141	37.656141
1973.304823	212251.412268	37.661159
1975.411482	212586.395846	37.666176
1977.138169	212923.866319	37.671194
1979.345776	213271.495049	37.676212
1981.253475	213605.829806	37.681229
1983.311479	213958.538835	37.686247
1984.711101	214296.487140	37.691264
1986.634125	214635.839535	37.696282
1989.180485	214984.477183	37.701300
1991.090451	215335.604479	37.706317
1993.070449	215674.978402	37.711335
1994.964751	216026.200584	37.716352
1996.931688	216378.593786	37.721370
1999.087888	216717.221158	37.726388
2000.855432	217077.013465	37.731405
2002.848105	217411.797681	37.736423
2005.221284	217765.999774	37.741440
2007.040289	218107.302805	37.746458
2009.226755	218429.707141	37.751476
2010.666320	218751.342639	37.756493
2012.563166	219079.776023	37.761511
2014.655563	219406.808586	37.766528
2016.893541	219730.708742	37.771546
2018.810204	220054.877144	37.776564
2020.661369	220388.999185	37.781581
2022.851617	220711.044705	37.786599
2024.806208	221050.359116	37.791616
2026.647742	221402.339473	37.796634
2028.902786	221733.203664	37.801652
2030.199181	222097.831367	37.806669
2032.244794	222478.721642	37.811687
2034.663446	222821.131915	37.816704
2036.454798	223171.909320	37.821722
2038.774564	223526.820064	37.826740
2040.578140	223881.039726	37.831757
2042.913827	224225.069138	37.836775
2045.016141	224591.612136	37.841792
2046.797502	224939.021254	37.846810
2049.548125	225293.122252	37.851828
2051.697011	225649.263022	37.856845
2054.200568	225971.089829	37.861863
2057.218713	226303.147068	37.866880
2059.249810	226639.247823	37.871898
2061.399027	226973.274074	37.876916
2063.382611	227307.734252	37.881933
2065.630898	227639.868056	37.886951
2067.821670	227956.723505	37.891968
2069.581996	228300.899049	37.896986
2072.179703	228615.609808	37.902004
2074.325787	228953.479101	37.907021
2076.284392	229277.360284	37.912039
2078.300934	229599.125490	37.917056
2079.975822	229933.619226	37.922074
2082.092533	230265.580573	37.927092
2083.795382	230614.040861	37.932109
2085.494130	230948.128158	37.937127
2087.585965	231294.802277	37.942144
2089.459622	231651.468159	37.947162
2092.057464	231989.734150	37.952180
2093.984693	232344.717892	37.957197
2095.819847	232696.745994	37.962215
2098.201267	233044.345668	37.967232
2099.993441	233407.837662	37.972250
2102.193877	233760.370416	37.977268
2103.995621	234136.334078	37.982285
2106.258981	234494.904237	37.987303
2108.104616	234845.719198	37.992320
2110.170446	235223.016527	37.997338
2112.184300	235587.852746	38.002356
2114.322901	235957.521616	38.007373
2116.652841	236325.535915	38.012391
2118.775636	236697.394185	38.017408
2120.787104	237047.936248	38.022426
2123.162295	237393.214948	38.027444
2124.532876	237745.867444	38.032461
2127.085591	238086.116539	38.037479
2129.412601	238420.179646	38.042496
2131.020385	238774.296343	38.047514
2133.201700	239120.398547	38.052532
2135.244256	239467.971582	38.057549
2136.974971	239830.403101	38.062567
2139.485114	240187.403590	38.067584
2141.420609	240550.414449	38.072602
2143.675613	240908.956166	38.077620
2145.533810	241272.260873	38.082637
2147.618160	241644.369998	38.087655
2150.015143	242013.077855	38.092672
2151.856349	242379.766738	38.097690
2154.619237	242743.237086	38.102708
2156.786242	243109.165207	38.107725
2159.031428	243465.506030	38.112743
2161.566795	243839.378913	38.117760
2163.692944	244219.871091	38.122778
2165.675403	244592.995572	38.127796
2167.818220	244973.360240	38.132813
2170.260088	245342.832429	38.137831
2172.725529	245702.928976	38.142848
2174.875628	246087.461281	38.147866
2177.274911	246449.119678	38.152884
2179.501789	246827.520177	38.157901
2181.032653	247204.787384	38.162919
2183.020120	247584.523255	38.167936
2184.956716	247975.089059	38.172954
2187.280293	248360.438044	38.177972
2189.317607	248756.755953	38.182989
2191.198355	249152.032835	38.188007
2193.579862	249546.748662	38.193024
2195.370009	249963.683939	38.198042
2197.918700	250360.432748	38.203060
2200.266536	250766.333536	38.208077
2202.175022	251171.771530	38.213095
2204.537514	251573.734647	38.218112
2206.625223	251997.994239	38.223130
2208.854236	252405.899032	38.228148
2211.219950	252824.451867	38.233165
2213.692814	253240.880291	38.238183
2216.044633	253642.468639	38.243200
2217.960643	254061.298738	38.248218
2220.473686	254465.860665	38.253236
2222.707524	254881.238209	38.258253
2225.205509	255279.987050	38.263271
2227.761632	255681.445479	38.268288
2229.889725	256088.942083	38.273306
2232.129371	256483.898388	38.278324
2234.576751	256885.782718	38.283341
2236.882761	257281.060131	38.288359
2239.718506	257669.700372	38.293376
2241.907497	258064.718229	38.298394
2244.294858	258423.303364	38.303412
2246.437620	258780.860890	38.308429
2248.614125	259141.792121	38.313447
2250.892221	259495.290159	38.318464
2252.721250	259858.411294	38.323482
2254.412564	260210.580756	38.328500
2256.841395	260584.302305	38.333517
2258.936737	260959.601387	38.338535
2261.442703	261335.496316	38.343552
2263.294160	261714.950279	38.348570
2265.327159	262094.756964	38.353588
2267.470653	262476.807442	38.358605
2269.395594	262862.728862	38.363623
2272.047822	263257.680490	38.368640
2273.936546	263676.683270	38.373658
2276.276893	264071.151776	38.378676
2278.338619	264482.253083	38.383693
2280.168418	264904.314927	38.388711
2282.722132	265313.687876	38.393728
2284.835228	265744.774569	38.398746
2287.106475	266163.516054	38.403764
2289.424241	266583.825535	38.408781
2291.794672	267011.417750	38.413799
2294.547563	267434.250079	38.418816
2296.590309	267872.716714	38.423834
2299.541007	268284.594910	38.428852
2302.375417	268701.242232	38.433869
2304.948776	269122.249766	38.438887
2307.489643	269525.581979	38.443904
2309.504296	269951.860837	38.448922
2311.975994	270348.701173	38.453940
2314.014183	270776.373885	38.458957
2316.266786	271199.160742	38.463975
2319.104850	271605.850811	38.468992
2321.127316	272027.480485	38.474010
2323.578098	272428.821273	38.479028
2326.151444	272860.550603	38.484045
2327.866482	273284.820467	38.489063
2330.462627	273699.678475	38.494080
2332.756362	274123.856715	38.499098
2334.854225	274546.821270	38.504116
2337.293488	274977.937020	38.509133
2339.314966	275413.437571	38.514151
2341.642098	275847.390841	38.519168
2343.926333	276280.029885	38.524186
2346.433116	276706.816205	38.529204
2349.212760	277141.713679	38.534221
2351.208460	277583.391002	38.539239
2353.924411	278012.252331	38.544256
2356.002104	278454.449846	38.549274
2358.170883	278887.081084	38.554292
2360.824132	279318.492190	38.559309
2363.121832	279765.734923	38.564327
2365.742106	280194.661292	38.569344
2368.277163	280613.744442	38.574362
2370.768354	281014.188277	38.579380
2373.308500	281408.806759	38.584397
2375.309474	281808.667313	38.589415
2377.870534	282199.928731	38.594432
2380.267106	282596.830057	38.599450
2382.322631	282990.635143	38.604468
2384.794736	283402.892812	38.609485
2387.589101	283799.272874	38.614503
2389.565546	284194.689897	38.619520
2391.911900	284616.035319	38.624538
2393.965994	285011.058230	38.629556
2396.521843	285423.961190	38.634573
2398.286900	285852.967556	38.639591
2400.671465	286271.180568	38.644608
2402.966475	286700.482981	38.649626
2405.193671	287138.000756	38.654644
2407.314534	287575.052150	38.659661
2409.570189	288024.706811	38.664679
2412.104418	288473.376761	38.669696
2414.310136	288933.046707	38.674714
2417.082281	289380.407426	38.679732
2419.788271	289834.738260	38.684749
2421.938881	290294.160680	38.689767
2424.121518	290752.738937	38.694784
2426.732267	291215.643169	38.699802
2428.899316	291682.935289	38.704820
2431.660705	292150.233924	38.709837
2433.477459	292628.934614	38.714855
2436.135358	293104.681335	38.719872
2439.002332	293582.705518	38.724890
2441.466236	294053.019437	38.729908
2443.942930	294517.818009	38.734925
2446.310825	295002.776681	38.739943
2449.372614	295477.412588	38.744960
2452.057808	295951.192562	38.749978
2454.292658	296423.010586	38.754996
2456.992737	296889.444708	38.760013
2459.475303	297375.293720	38.765031
2462.315662	297830.551810	38.770048
2464.249380	298313.284631	38.775066
2466.769400	298787.743877	38.780084
2469.742502	299245.847607	38.785101
2471.764287	299735.116042	38.790119
2474.420176	300203.910605	38.795136
2477.271191	300681.791959	38.800154
2479.831273	301156.771423	38.805172
2482.451416	301622.951107	38.810189
2484.893537	302095.660253	38.815207
2487.711918	302559.417929	38.820224
2489.506974	303034.106294	38.825242
2492.012355	303510.865017	38.830260
2494.568985	303984.032513	38.835277
2496.577279	304474.964166	38.840295
2498.977815	304952.191802	38.845312
2501.850909	305420.071696	38.850330
2504.312079	305868.914113	38.855348
2506.761563	306319.865075	38.860365
2508.911115	306773.275014	38.865383
2511.504189	307214.344798	38.870400
2513.950414	307672.962342	38.875418
2516.243543	308125.354061	38.880436
2519.072964	308575.373148	38.885453
2521.067824	309054.072129	38.890471
2523.969042	309500.825202	38.895488
2526.916647	309946.375449	38.900506
2529.440521	310410.100947	38.905524
2532.211244	310866.114849	38.910541
2534.388814	311330.450255	38.915559
2536.996746	311779.933236	38.920576
2538.986775	312258.264012	38.925594
2541.338691	312735.824182	38.930612
2544.226920	313202.985339	38.935629
2546.735518	313695.425508	38.940647
2549.075755	314174.606579	38.945664
2551.893761	314656.249588	38.950682
2554.192819	315162.227971	38.955700
2556.479291	315645.322021	38.960717
2558.651851	316149.918573	38.965735
2561.098062	316661.453629	38.970752
2563.887992	317169.756819	38.975770
2566.001455	317693.225328	38.980788
2568.396374	318206.182577	38.985805
2570.851263	318731.851629	38.990823
2573.383487	319261.492826	38.995840
2576.172184	319791.547483	39.000858
2578.898581	320316.351741	39.005876
2582.090620	320842.729953	39.010893
2584.326503	321383.224677	39.015911
2587.364939	321906.039943	39.020928
2590.265476	322432.759541	39.025946
2592.388048	322970.138564	39.030964
2595.493624	323502.584002	39.035981
2598.124959	324038.453438	39.040999
2600.803641	324564.788520	39.046016
2603.651889	325090.915593	39.051034
2606.054858	325625.464870	39.056052
2608.904665	326142.518692	39.061069
2611.733163	326681.920162	39.066087
2614.438434	327202.316698	39.071104
2617.533803	327720.337046	39.076122
2619.468673	328249.203442	39.081140
2622.276429	328772.722065	39.086157
2624.914137	329303.602914	39.091175
2627.310033	329832.588358	39.096192
2630.165279	330367.896506	39.101210
2632.737013	330887.298465	39.106228
2635.295575	331414.189866	39.111245
2638.040869	331950.697273	39.116263
2640.765252	332482.582424	39.121280
2643.596740	332990.983595	39.126298
2645.941269	333491.053231	39.131316
2648.293865	333980.224602	39.136333
2650.681089	334486.044387	39.141351
2653.056130	334987.799616	39.146368
2655.594282	335491.048812	39.151386
2658.196015	336005.380368	39.156404
2660.889792	336523.451327	39.161421
2662.694282	337052.628142	39.166439
2665.052168	337578.234446	39.171456
2667.550677	338116.205005	39.176474
2669.754923	338676.383777	39.181492
2672.449141	339215.532872	39.186509
2674.783071	339777.738032	39.191527
2677.643883	340352.168881	39.196544
2680.436026	340920.257850	39.201562
2682.723252	341496.343103	39.206580
2685.286202	342081.646364	39.211597
2688.065864	342662.644286	39.216615
2690.564050	343260.869410	39.221632
2693.636207	343852.193486	39.226650
2695.816231	344460.510773	39.231668
2698.757048	345057.657449	39.236685
2701.428846	345661.923780	39.241703
2704.120859	346277.097197	39.246720
2707.123445	346884.573235	39.251738
2710.222379	347495.632441	39.256756
2713.076678	348107.612265	39.261773
2715.404859	348712.433548	39.266791
2718.445166	349330.386985	39.271808
2721.632662	349945.238445	39.276826
2724.160763	350564.553675	39.281844
2727.282020	351173.867595	39.286861
2730.100709	351774.490042	39.291879
2732.797586	352390.838087	39.296896
2735.897738	352993.534395	39.301914
2739.353950	353591.978975	39.306932
2742.504127	354185.083730	39.311949
2745.903384	354767.100363	39.316967
2748.660092	355349.872063	39.321984
2752.163428	355922.061055	39.327002
2754.662810	356500.468956	39.332020
2757.503586	357076.150947	39.337037
2760.508741	357649.744272	39.342055
2763.148066	358220.546079	39.347072
2766.209291	358787.924059	39.352090
2768.783462	359354.611092	39.357108
2771.248466	359927.222489	39.362125
2773.892767	360504.671713	39.367143
2776.373667	361074.094259	39.372160
2779.475648	361646.203392	39.377178
2782.021085	362223.571116	39.382196
2784.277955	362797.195861	39.387213
2787.453176	363379.906047	39.392231
2790.083961	363966.451097	39.397248
2793.097332	364533.868902	39.402266
2795.071256	365080.989494	39.407284
2798.007690	365645.157160	39.412301
2800.718514	366194.989835	39.417319
2802.689266	366750.262094	39.422336
2805.590893	367312.155610	39.427354
2807.936721	367882.402676	39.432372
2810.850850	368467.651122	39.437389
2813.344863	369045.421603	39.442407
2815.989835	369629.580444	39.447424
2818.615780	370228.832522	39.452442
2821.107093	370832.944071	39.457460
2823.728805	371434.387440	39.462477
2826.163194	372054.527132	39.467495
2828.879043	372671.263767	39.472512
2832.374077	373292.866427	39.477530
2834.880210	373929.028068	39.482548
2837.840427	374561.733437	39.487565
2840.426953	375191.291282	39.492583
2843.289896	375831.426315	39.497600
2845.852362	376483.168032	39.502618
2848.425087	377142.711730	39.507636
2851.256553	377793.755194	39.512653
2854.239191	378470.438411	39.517671
2856.753990	379149.518027	39.522688
2859.950405	379808.030439	39.527706
2863.125078	380485.155697	39.532724
2866.133049	381164.781525	39.537741
2869.252378	381836.741963	39.542759
2872.094211	382514.340629	39.547776
2875.404853	383181.477894	39.552794
2878.488227	383851.074456	39.557812
2881.295342	384530.062765	39.562829
2884.412533	385194.556609	39.567847
2887.417256	385865.473626	39.572864
2890.730581	386534.224251	39.577882
2893.845730	387205.961562	39.582900
2897.039391	387878.967525	39.587917
2900.326381	388528.916396	39.592935
2903.367480	389190.609938	39.597952
2906.624057	389837.851328	39.602970
2909.524012	390485.365575	39.607988
2912.486924	391121.242466	39.613005
2915.774082	391779.754405	39.618023
2918.439408	392437.211083	39.623040
2921.185929	393083.686955	39.628058
2923.650233	393745.284169	39.633076
2926.533044	394392.373142	39.638093
2929.685424	395048.130425	39.643111
2932.967566	395699.873263	39.648128
2936.517757	396345.652770	39.653146
2939.324125	396992.044676	39.658164
2942.301400	397634.339949	39.663181
2945.206549	398282.871735	39.668199
2947.646715	398929.613395	39.673216
2950.891011	399549.490903	39.678234
2953.574016	400178.243456	39.683252
2956.014578	400786.282629	39.688269
2958.840332	401397.722815	39.693287
2961.796460	402007.381366	39.698304
2964.621891	402634.618276	39.703322
2967.226459	403251.204563	39.708340
2970.339411	403875.227785	39.713357
2973.110918	404505.833242	39.718375
2975.647220	405144.347241	39.723392
2978.372590	405785.277194	39.728410
2981.696869	406426.175173	39.733428
2984.209557	407090.686739	39.738445
2986.836144	407748.195104	39.743463
2989.771378	408417.630001	39.748480
2992.796920	409081.231347	39.753498
2995.661120	409767.275495	39.758516
2998.455390	410445.483128	39.763533
3001.899080	411129.706253	39.768551
3004.715501	411815.482935	39.773568
3007.630543	412510.529529	39.778586
3010.637069	413210.563330	39.783604
3013.564875	413917.334166	39.788621
3016.428618	414625.618580	39.793639
3019.299404	415342.222094	39.798656
3022.452775	416051.211424	39.803674
3025.585191	416782.638388	39.808692
3028.344116	417514.865946	39.813709
3031.693421	418232.005698	39.818727
3034.525454	418977.689807	39.823744
3037.911276	419702.083971	39.828762
3041.429784	420430.796435	39.833780
3044.380608	421166.192546	39.838797
3047.431392	421894.408585	39.843815
3050.231004	422631.259166	39.848832
3053.539728	423357.318190	39.853850
3056.463306	424101.101978	39.858868
3059.637780	424855.187027	39.863885
3062.752326	425605.764637	39.868903
3065.589958	426353.578618	39.873920
3068.761407	427101.293566	39.878938
3071.873741	427853.708341	39.883956
3074.695001	428610.301884	39.888973
3077.757860	429373.699655	39.893991
3080.755330	430141.214068	39.899008
3083.919625	430896.623640	39.904026
3086.799464	431677.003105	39.909044
3089.424650	432447.243587	39.914061
3092.756668	433223.452560	39.919079
3095.468978	434014.297591	39.924096
3098.757765	434797.075238	39.929114
3101.899305	435590.234376	39.934132
3104.637106	436387.509289	39.939149
3107.675291	437172.506502	39.944167
3110.852375	437987.132626	39.949184
3114.246399	438759.768417	39.954202
3117.565222	439506.667987	39.959220
3120.892537	440273.595473	39.964237
3123.973153	441008.182446	39.969255
3127.010059	441759.361859	39.974272
3130.270730	442489.723691	39.979290
3133.496095	443231.511412	39.984308
3136.510562	443998.168172	39.989325
3139.844865	444737.056931	39.994343
3142.708266	445494.728613	39.999360
3145.892558	446240.681912	40.004378
3149.316928	446996.596837	40.009396
3152.376177	447754.620656	40.014413
3155.643380	448508.284448	40.019431
3158.909607	449268.605481	40.024448
3162.046376	450021.076690	40.029466
3165.215786	450791.637957	40.034484
3168.216357	451551.622199	40.039501
3171.166917	452330.163137	40.044519
3174.229222	453100.815481	40.049536
3177.435640	453889.536133	40.054554
3180.738069	454662.728905	40.059572
3183.948285	455462.982489	40.064589
3187.757477	456239.330013	40.069607
3191.104722	457034.546691	40.074624
3194.082399	457813.854978	40.079642
3197.405330	458619.087616	40.084660
3200.264017	459391.123745	40.089677
3203.472442	460205.625675	40.094695
3206.992970	460998.648002	40.099712
3210.322589	461811.957659	40.104730
3213.325541	462606.672429	40.109748
3215.833749	463433.203473	40.114765
3219.330982	464234.355893	40.119783
3222.500811	465069.065282	40.124800
3225.900269	465889.442260	40.129818
3229.031990	466708.413604	40.134836
3232.046980	467536.070490	40.139853
3235.589424	468365.280205	40.144871
3238.736232	469197.098680	40.149888
3242.213244	470015.430831	40.154906
3245.490863	470865.568853	40.159924
3248.828692	471695.234026	40.164941
3252.411655	472515.523292	40.169959
3255.648832	473355.502502	40.174976
3258.965026	474176.778320	40.179994
3262.131832	475015.840447	40.185012
3265.397737	475844.235517	40.190029
3268.281562	476685.446640	40.195047
3271.433286	477533.252672	40.200064
3274.351104	478379.947535	40.205082
3277.970239	479233.015788	40.210100
3281.145182	480080.102695	40.215117
3284.597616	480926.250015	40.220135
3287.994909	481776.008326	40.225152
3291.151344	482602.368887	40.230170
3294.662073	483423.079376	40.235188
3298.049605	484211.130101	40.240205
3301.637113	485004.119540	40.245223
3304.827572	485787.690056	40.250240
3308.137392	486592.380360	40.255258
3311.276678	487378.066297	40.260276
3314.440758	488166.999744	40.265293
3318.115247	488975.926733	40.270311
3321.119115	489760.928747	40.275328
3323.928478	490580.229200	40.280346
3327.232375	491395.980575	40.285364
3330.435484	492218.228142	40.290381
3333.923161	493044.738056	40.295399
3336.845081	493880.088678	40.300416
3339.652830	494725.772920	40.305434
3342.967101	495564.974713	40.310452
3346.178185	496435.110856	40.315469
3349.605923	497274.922902	40.320487
3352.892362	498149.156217	40.325504
3356.054647	499021.094588	40.330522
3359.067875	499915.835877	40.335540
3362.032387	500795.545195	40.340557
3365.446069	501688.922578	40.345575
3368.718832	502600.350106	40.350592
3371.928109	503519.767002	40.355610
3375.251858	504434.372867	40.360628
3378.474585	505366.512225	40.365645
3381.486715	506288.136871	40.370663
3384.875737	507238.067371	40.375680
3388.081492	508186.561631	40.380698
3391.640477	509136.461761	40.385716
3394.756328	510106.917005	40.390733
3398.458378	511063.802597	40.395751
3401.798600	512045.212850	40.400768
3404.941419	512996.073772	40.405786
3408.654193	513981.399392	40.410804
3412.102873	514964.640665	40.415821
3415.314151	515949.828981	40.420839
3418.997801	516919.197350	40.425856
3422.320489	517918.324325	40.430874
3426.078450	518900.123898	40.435892
3429.154326	519895.690068	40.440909
3433.070494	520874.875384	40.445927
3436.699715	521871.393630	40.450944
3440.481604	522861.221297	40.455962
3444.582375	523836.568515	40.460980
3448.078833	524820.119633	40.465997
3451.428126	525784.980878	40.471015
3455.382880	526758.308309	40.476032
3458.841944	527734.931031	40.481050
3462.502154	528710.050501	40.486068
3465.748319	529691.626504	40.491085
3469.490289	530660.665083	40.496103
3473.058096	531619.693137	40.501120
3475.977839	532573.079092	40.506125
3479.470795	533479.441727	40.511130
3482.620306	534346.606361	40.516135
3485.675866	535142.869026	40.521140
3488.653192	535878.592547	40.526144
3491.345793	536560.788155	40.531149
3493.988010	537175.991488	40.536154
3496.631024	537727.384197	40.541159
3499.551587	538205.990598	40.546164
3502.352294	538632.939020	40.551168
3503.819135	539008.274167	40.556173
3506.133096	539316.657240	40.561178
3508.085840	539582.168503	40.566183
3509.925989	539796.035019	40.571188
3512.032699	539949.311760	40.576192
3513.356757	540052.871473	40.581197
3514.918650	540123.520388	40.586202
3515.618596	540163.856550	40.591207
3516.679707	540155.407604	40.596212
3517.649614	540123.341218	40.601216
3518.190517	540063.620480	40.606221
3518.615019	539995.333606	40.611226
3519.415493	539880.530524	40.616231
3519.896594	539736.943437	40.621236
3520.296991	539594.983653	40.626240
3521.066289	539432.108682	40.631245
3521.116294	539251.671224	40.636250
3521.020212	539053.176068	40.641255
3521.278334	538842.098413	40.646260
3521.352332	538657.610118	40.651264
3521.327437	538426.623772	40.656269
3521.939943	538191.291028	40.661274
3521.887510	537959.594917	40.666279
3521.772875	537713.208611	40.671284
3522.003558	537465.804169	40.676288
3521.599024	537221.021359	40.681293
3522.127107	536947.349353	40.686298
3521.840648	536688.650201	40.691303
3521.563674	536425.399483	40.696308
3521.802772	536148.778920	40.701312
3521.024258	535892.720030	40.706317
3521.013435	535622.998773	40.711322
3520.903662	535356.268585	40.716327
3520.653176	535083.292509	40.721332
3520.316415	534833.056074	40.726336
3520.625321	534579.228086	40.731341
3520.690105	534301.035931	40.736346
3520.170793	534053.796079	40.741351
3519.897543	533767.817847	40.746356
3519.779919	533504.441501	40.751360
3519.517747	533248.863317	40.756365
3519.565921	532989.190360	40.761370
3519.544789	532734.778076	40.766375
3519.170765	532471.980454	40.771380
3519.081888	532223.632994	40.776384
3518.805504	531967.429736	40.781389
3518.796401	531709.361195	40.786394
3518.093866	531461.098575	40.791399
3518.250802	531220.931707	40.796404
3517.865595	530978.573188	40.801408
3517.475807	530729.542172	40.806413
3517.403394	530492.987753	40.811418
3517.093369	530264.652824	40.816423
3516.844854	530035.900624	40.821428
3516.309428	529797.286703	40.826432
3516.457101	529576.853072	40.831437
3516.731666	529358.265938	40.836442
3516.086645	529153.666702	40.841447
3515.976507	528923.613192	40.846452
3515.908866	528717.198955	40.851456
3515.692640	528506.661767	40.856461
3515.506251	528299.048037	40.861466
3515.309684	528098.305916	40.866471
3515.057603	527889.534901	40.871476
3514.979246	527692.710721	40.876480
3514.802792	527486.196566	40.881485
3514.708163	527290.279629	40.886490
3514.234973	527097.351305	40.891495
3514.204227	526905.967948	40.896500
3514.161791	526726.915679	40.901504
3513.706155	526538.425244	40.906509
3513.601622	526358.468936	40.911514
3513.748285	526182.312001	40.916519
3513.399109	526011.740495	40.921524
3513.546033	525824.106680	40.926528
3512.643862	525667.517923	40.931533
3512.940720	525492.087783	40.936538
3512.870621	525326.771879	40.941543
3512.607285	525159.766312	40.946548
3512.348797	525001.249723	40.951552
3512.058965	524840.512541	40.956557
3512.243203	524682.782103	40.961562
3512.073548	524548.306661	40.966567
3511.650448	524377.982178	40.971572
3511.617425	524234.384145	40.976576
3511.248722	524082.649203	40.981581
3511.464108	523948.967205	40.986586
3511.012266	523806.998537	40.991591
3510.820512	523665.796292	40.996596
3510.779818	523537.307324	41.001600
3510.591023	523399.539624	41.006605
3510.587934	523277.715188	41.011610
3510.396185	523159.306522	41.016615
3510.236314	523018.245229	41.021620
3510.466039	522894.814041	41.026624
3510.088443	522775.875879	41.031629
3510.370657	522643.840724	41.036634
3509.502441	522541.609954	41.041639
3509.410467	522425.909976	41.046644
3509.761295	522309.279790	41.051648
3509.732145	522197.814706	41.056653
3509.805175	522091.741948	41.061658
3509.480243	521971.222396	41.066663
3509.129113	521862.535815	41.071668
3509.187361	521765.563046	41.076672
3508.879101	521662.530472	41.081677
3508.666328	521553.819960	41.086682
3508.746623	521457.954091	41.091687
3508.447729	521348.649153	41.096692
3508.731461	521254.519393	41.101696
3508.413811	521172.364916	41.106701
3508.758744	521077.011104	41.111706
3508.356824	520990.824487	41.116711
3508.407185	520894.403908	41.121716
3508.418258	520806.533211	41.126720
3508.308176	520719.540674	41.131725
3508.334578	520616.044130	41.136730
3508.372704	520527.712634	41.141735
3508.140319	520439.221179	41.146740
3508.014335	520355.111065	41.151744
3507.939986	520276.351641	41.156749
3508.045070	520190.737944	41.161754
3507.547785	520100.870857	41.166759
3507.660767	520027.035489	41.171764
3507.691427	519943.050181	41.176768
3507.737865	519867.455000	41.181773
3507.506279	519785.987800	41.186778
3507.201730	519715.655151	41.191783
3507.032734	519647.323225	41.196788
3506.989596	519575.735192	41.201792
3507.001334	519513.138145	41.206797
3507.103945	519440.768064	41.211802
3506.675171	519374.700781	41.216807
3506.852434	519302.571104	41.221812
3506.735183	519238.476529	41.226816
3506.706139	519185.744360	41.231821
3506.667840	519124.872872	41.236826
3506.693980	519060.401001	41.241831
3506.580274	518996.001542	41.246836
3506.575862	518939.826392	41.251840
3506.475069	518879.924580	41.256845
3506.354176	518823.565188	41.261850
3506.395680	518777.292719	41.266855
3506.299448	518714.911954	41.271860
3506.508761	518655.010877	41.276864
3505.816714	518605.061538	41.281869
3506.331613	518550.421046	41.286874
3506.171771	518504.634714	41.291879
3506.121929	518443.206319	41.296884
3506.166636	518384.796658	41.301888
3506.172259	518350.462019	41.306893
3506.280325	518300.536997	41.311898
3505.724409	518246.014172	41.316903
3505.867691	518193.706681	41.321908
3506.047603	518147.006043	41.326912
3505.718670	518111.409071	41.331917
3505.847825	518052.327530	41.336922
3505.768349	518010.471281	41.341927
3505.800894	517959.090742	41.346932
3505.745425	517916.320266	41.351936
3505.621209	517881.145540	41.356941
3505.584424	517831.595961	41.361946
3505.541548	517799.189379	41.366951
3505.441048	517743.278176	41.371956
3505.698436	517704.250234	41.376960
3505.434208	517662.118900	41.381965
3505.845410	517623.066457	41.386970
3505.466698	517579.941658	41.391975
3505.150627	517538.475580	41.396980
3505.309913	517503.710355	41.401984
3505.022516	517477.055947	41.406989
3505.503703	517425.046597	41.411994
3504.892048	517401.477396	41.416999
3505.185712	517366.690645	41.422004
3505.212223	517329.518765	41.427008
3504.731405	517301.478730	41.432013
3504.704031	517263.000438	41.437018
3504.969998	517241.365613	41.442023
3504.885006	517206.284391	41.447028
3504.965968	517167.030224	41.452032
3504.827199	517138.076183	41.457037
3505.060447	517108.709312	41.462042
3504.603890	517095.835784	41.467047
3504.826219	517050.086161	41.472052
3504.925675	517013.205459	41.477056
3504.863410	516990.863643	41.482061
3505.067163	516958.062452	41.487066
3504.816074	516933.070221	41.492071
3504.607332	516913.886763	41.497076
3505.034138	516874.931233	41.502080
3504.620859	516862.657520	41.507085
3504.842915	516826.818992	41.512090
3504.819326	516801.284908	41.517095
3504.681433	516784.618599	41.522100
3504.749092	516741.775061	41.527104
3504.575001	516723.597308	41.532109
3504.841554	516695.690979	41.537114
3504.883534	516668.325799	41.542119
3504.905530	516650.976671	41.547124
3504.744713	516609.837726	41.552128
3504.380806	516590.830129	41.557133
3504.765909	516568.518182	41.562138
3504.659165	516531.567858	41.567143
3504.684147	516507.795623	41.572148
3504.768787	516482.597941	41.577152
3504.514929	516454.520602	41.582157
3504.590110	516432.257454	41.587162
3504.420148	516413.522428	41.592167
3504.466655	516389.746623	41.597172
3504.497479	516358.387572	41.602176
3504.321681	516352.296214	41.607181
3504.595897	516321.960624	41.612186
3504.548603	516290.866650	41.617191
3504.117401	516282.641058	41.622196
3504.216888	516266.290712	41.627200
3504.456228	516242.888793	41.632205
3504.231868	516226.791878	41.637210
3504.053126	516204.265128	41.642215
3504.331831	516189.605821	41.647220
3504.515736	516169.145723	41.652224
3503.980043	516162.200881	41.657229
3504.182937	516132.280794	41.662234
3504.178127	516116.604221	41.667239
3504.174438	516095.111669	41.672244
3504.327403	516080.370995	41.677248
3504.116148	516069.430212	41.682253
3504.001780	516045.932202	41.687258
3504.321940	516032.732801	41.692263
3504.306681	516009.775371	41.697268
3504.296334	515991.722656	41.702272
3504.380610	515984.174031	41.707277
3504.415507	515946.643727	41.712282
3504.523719	515934.489196	41.717287
3504.222318	515917.342134	41.722292
3504.356933	515894.310286	41.727296
3504.346201	515867.660138	41.732301
3504.602477	515851.840907	41.737306
3504.260020	515838.644932	41.742311
3504.266572	515809.867900	41.747316
3504.325385	515779.160785	41.752320
3504.097192	515781.219754	41.757325
3504.399826	515748.349979	41.762330
3504.224875	515736.543496	41.767335
3504.137710	515714.254475	41.772340
3504.383212	515699.245974	41.777344
3504.274248	515686.872721	41.782349
3504.288970	515659.965352	41.787354
3504.468456	515650.631460	41.792359
3504.269972	515622.240525	41.797364
3504.494758	515606.324891	41.802368
3504.166966	515602.887104	41.807373
3504.130605	515576.442837	41.812378
3504.235130	515541.378725	41.817383
3503.857853	515546.748578	41.822388
3504.081422	515518.745926	41.827392
3504.261205	515506.428051	41.832397
3504.469985	515492.284924	41.837402
3504.172344	515471.343765	41.842407
3504.260881	515454.488616	41.847412
3504.036578	515444.004650	41.852416
3503.822298	515440.498315	41.857421
3504.010800	515412.753898	41.862426
3504.137329	515395.639813	41.867431
3504.014202	515387.314511	41.872436
3503.971195	515368.406522	41.877440
3503.793412	515357.409407	41.882445
3504.373445	515344.320113	41.887450
3504.470309	515336.061166	41.892455
3504.162610	515306.928339	41.897460
3504.157760	515284.979757	41.902464
3503.768684	515277.202178	41.907469
3504.027836	515270.637084	41.912474
3503.966372	515244.550280	41.917479
3504.085097	515238.310815	41.922484
3504.061579	515222.484635	41.927488
3503.594730	515208.751498	41.932493
3504.187473	515191.917545	41.937498
3504.211357	515180.888440	41.942503
3503.643763	515167.828665	41.947508
3504.222300	515148.771619	41.952512
3503.820888	515143.221224	41.957517
3504.064618	515122.345790	41.962522
3504.033069	515108.240321	41.967527
3503.549981	515096.633811	41.972532
3503.924155	515073.461820	41.977536
3503.901493	515060.771012	41.982541
3503.795761	515060.281953	41.987546
3503.852680	515040.042843	41.992551
3503.766274	515038.134622	41.997556
3504.265071	515025.917700	42.002560
3504.179575	515007.117168	42.007565
3503.944195	514986.823041	42.012570
3504.037098	514995.962491	42.017575
3504.170555	514984.814788	42.022580
3503.969309	514966.942863	42.027584
3503.745615	514953.322811	42.032589
3503.979245	514922.738220	42.037594
3504.219710	514927.707184	42.042599
3503.735401	514916.050164	42.047604
3503.841334	514883.917839	42.052608
3503.766928	514879.023734	42.057613
3504.269668	514871.914228	42.062618
3503.837159	514849.526907	42.067623
3504.068957	514841.347541	42.072628
3503.830734	514843.408209	42.077632
3503.605588	514815.525875	42.082637
3503.867489	514800.362249	42.087642
3504.193242	514804.963738	42.092647
3504.033922	514783.089487	42.097652
3504.431242	514766.640027	42.102656
3504.127456	514743.928764	42.107661
3503.953875	514730.047730	42.112666
3504.046425	514729.274442	42.117671
3503.914074	514693.133314	42.122676
3503.973276	514682.098299	42.127680
3503.858193	514676.148460	42.132685
3504.360476	514664.031877	42.137690
3504.316379	514656.907555	42.142695
3504.070378	514631.809914	42.147700
3503.895595	514611.202295	42.152704
3503.968837	514603.907675	42.157709
3504.226918	514580.601623	42.162714
3504.267140	514573.312208	42.167719
3504.252206	514548.279076	42.172724
3504.174076	514522.750127	42.177728
3504.054871	514523.679332	42.182733
3503.942074	514489.254286	42.187738
3503.857158	514489.520574	42.192743
3503.982325	514480.801540	42.197748
3504.537413	514443.135071	42.202752
3504.146462	514441.679530	42.207757
3504.496966	514428.726957	42.212762
3503.838294	514410.876155	42.217767
3503.895154	514389.776459	42.222772
3503.967122	514372.063026	42.227776
3504.080113	514366.279339	42.232781
3503.948911	514341.061965	42.237786
3503.832293	514337.438807	42.242791
3503.805551	514331.879502	42.247796
3503.564739	514327.416155	42.252800
3504.086927	514309.833810	42.257805
3504.083499	514296.178411	42.262810
3504.020916	514293.001901	42.267815
3503.815663	514264.103955	42.272820
3503.556539	514253.827056	42.277824
3503.688491	514258.257015	42.282829
3503.974721	514238.840517	42.287834
3504.418772	514225.670692	42.292839
3503.941908	514217.299560	42.297844
3504.011754	514185.070444	42.302848
3503.780926	514166.747140	42.307853
3504.176679	514163.751056	42.312858
3503.751471	514159.114495	42.317863
3503.877146	514132.844650	42.322868
3503.980972	514123.218399	42.327872
3503.586681	514123.027808	42.332877
3503.584269	514088.837386	42.337882
3503.789726	514096.189302	42.342887
3503.568118	514094.605810	42.347892
3504.180280	514088.237353	42.352896
3504.173643	514067.096709	42.357901
3503.643234	514063.235421	42.362906
3503.680206	514056.755547	42.367911
3503.802825	514024.669519	42.372916
3504.062175	514025.083716	42.377920
3503.888773	514021.064838	42.382925
3504.244896	513986.615228	42.387930
3504.143350	513983.900023	42.392935
3503.926476	513967.546855	42.397940
3503.937232	513944.430746	42.402944
3503.960743	513943.466020	42.407949
3504.158708	513923.860794	42.412954
3503.818180	513912.180349	42.417959
3503.646919	513909.981937	42.422964
3503.597315	513895.372516	42.427968
3503.556459	513877.322343	42.432973
3503.696144	513867.184490	42.437978
3503.765981	513857.765775	42.442983
3503.652610	513865.370498	42.447988
3503.856331	513842.426067	42.452992
3503.420864	513834.655146	42.457997
3503.842030	513809.299093	42.463002
3503.845486	513824.472216	42.468007
3503.555371	513810.811154	42.473012
3503.795930	513786.191718	42.478016
3503.605511	513785.159635	42.483021
3503.892493	513782.332412	42.488026
3503.754368	513779.319481	42.493031
3503.719872	513759.548488	42.498036
3503.817395	513742.690199	42.503040
3503.775793	513747.299462	42.508045
3503.346274	513735.582379	42.513050
3503.465357	513719.934560	42.518055
3503.475682	513715.835991	42.523060
3503.410056	513704.921222	42.528064
3503.086640	513716.706711	42.533069
3503.623830	513707.416365	42.538074
3503.713432	513718.074411	42.543079
3503.642648	513714.342716	42.548084
3504.137713	513683.714551	42.553088
3503.763541	513681.851655	42.558093
3503.578954	513669.134807	42.563098
3503.604381	513662.100233	42.568103
3503.778519	513647.252916	42.573108
3503.869387	513629.080499	42.578112
3503.588904	513650.216458	42.583117
3503.582622	513624.421891	42.588122
3503.849815	513610.419686	42.593127
3503.547129	513605.358970	42.598132
3503.823328	513603.039218	42.603136
3503.190667	513601.824121	42.608141
3503.540354	513594.535952	42.613146
3503.584088	513579.709186	42.618151
3503.480043	513576.033296	42.623156
3504.046255	513564.563358	42.628160
3503.779814	513567.589654	42.633165
3503.544422	513540.667835	42.638170
3503.721610	513525.314131	42.643175
3503.258428	513528.826747	42.648180
3503.663879	513520.315816	42.653184
3503.527635	513525.850534	42.658189
3503.645896	513515.564117	42.663194
3503.553140	513499.848415	42.668199
3503.419655	513497.087599	42.673204
3503.932273	513490.835813	42.678208
3503.556948	513497.369345	42.683213
3503.501719	513474.819399	42.688218
3503.578136	513467.776684	42.693223
3503.714335	513456.273476	42.698228
3503.672549	513453.245260	42.703232
3503.575367	513458.166865	42.708237
3503.794052	513435.978216	42.713242
3503.758886	513431.785607	42.718247
3503.708634	513421.323446	42.723252
3504.074896	513419.950457	42.728256
3503.802075	513395.917391	42.733261
3503.771716	513384.440458	42.738266
3503.872048	513375.674197	42.743271
3503.833673	513363.996195	42.748276
3503.679679	513349.251057	42.753280
3503.512937	513343.056008	42.758285
3503.800410	513337.901936	42.763290
3503.877656	513331.820062	42.768295
3503.913993	513309.204842	42.773300
3504.001603	513292.802894	42.778304
3503.820807	513292.072743	42.783309
3503.742422	513277.062690	42.788314
3503.571153	513266.012591	42.793319
3503.718349	513260.324280	42.798324
3503.621548	513261.502916	42.803329
3503.535296	513245.431885	42.808333
3503.937876	513225.439444	42.813338
3503.594052	513217.805494	42.818343
3503.468774	513221.922317	42.823348
3503.808331	513214.787328	42.828353
3503.806942	513207.857964	42.833357
3504.110205	513194.608426	42.838362
3503.795199	513182.569373	42.843367
3503.876493	513169.405479	42.848372
3504.036002	513154.560041	42.853377
3503.784591	513158.241586	42.858381
3503.610298	513131.511781	42.863386
3503.969522	513114.206854	42.868391
3503.469224	513115.702178	42.873396
3503.804804	513112.057866	42.878401
3503.801625	513103.408986	42.883405
3503.825423	513080.795442	42.888410
3503.825003	513073.663545	42.893415
3503.961255	513065.245514	42.898420
3504.207878	513035.869390	42.903425
3503.706908	513044.395624	42.908429
3503.994599	513030.996676	42.913434
3504.032974	512998.011545	42.918439
3503.699719	512993.360126	42.923444
3503.797639	512989.196954	42.928449
3503.540272	512978.160275	42.933453
3503.620506	512958.370209	42.938458
3503.947607	512960.291173	42.943463
3503.505701	512964.812172	42.948468
3503.999822	512943.843882	42.953473
3503.912152	512923.271007	42.958477
3503.786789	512917.069260	42.963482
3503.863478	512904.866939	42.968487
3503.657560	512884.262123	42.973492
3504.027737	512878.538443	42.978497
3503.807935	512875.487676	42.983501
3504.079312	512857.994045	42.988506
3503.838207	512834.663311	42.993511
3503.837644	512834.713964	42.998516
3504.122740	512809.731992	43.003521
3503.732890	512810.097081	43.008525
3503.568670	512799.450218	43.013530
3503.830341	512781.148730	43.018535
3503.538350	512770.016221	43.023540
3503.788638	512745.848969	43.028545
3503.582396	512744.414665	43.033549
3503.581856	512741.582131	43.038554
3503.860407	512735.063569	43.043559
3503.461893	512722.278652	43.048564
3503.527386	512707.093605	43.053569
3503.427698	512721.828781	43.058573
3503.580203	512708.096868	43.063578
3503.620408	512708.748065	43.068583
3503.381603	512693.965176	43.073588
3503.855390	512669.610745	43.078593
3503.569089	512682.149824	43.083597
3503.725592	512670.592290	43.088602
3503.585856	512669.703874	43.093607
3503.518249	512657.675927	43.098612
3503.720678	512638.270834	43.103617
3503.416878	512638.065919	43.108621
3503.516406	512636.532696	43.113626
3503.805810	512633.199076	43.118631
3503.542566	512621.252606	43.123636
3503.815832	512595.513449	43.128641
3503.439557	512602.856796	43.133645
3503.731473	512594.768007	43.138650
3503.603687	512590.336915	43.143655
3503.699479	512571.353260	43.148660
3503.955614	512550.675011	43.153665
3503.522590	512560.101238	43.158669
3503.644349	512545.463563	43.163674
3503.568031	512532.071169	43.168679
3503.661146	512529.173215	43.173684
3503.539823	512516.850160	43.178689
3503.758999	512519.243479	43.183693
3504.004782	512511.718353	43.188698
3503.856132	512490.142931	43.193703
3503.435170	512498.707376	43.198708
3503.878110	512480.882743	43.203713
3503.539923	512457.111585	43.208717
3503.358016	512447.934203	43.213722
3503.654086	512448.747304	43.218727
3503.403127	512451.113771	43.223732
3503.665042	512443.838980	43.228737
3503.569607	512439.149820	43.233741
3503.569377	512411.784368	43.238746
3503.862073	512406.629189	43.243751
3503.378947	512417.884408	43.248756
3503.905467	512405.762382	43.253761
3503.716109	512394.259322	43.258765
3503.554534	512387.203189	43.263770
3503.571744	512380.270546	43.268775
3503.562218	512370.155379	43.273780
3503.748817	512370.935202	43.278785
3503.465980	512350.999476	43.283789
3503.477517	512346.647466	43.288794
3503.599197	512336.562126	43.293799
3503.060780	512343.577127	43.298804
3503.537464	512342.692436	43.303809
3503.357518	512347.323945	43.308813
3503.359071	512339.736176	43.313818
3503.330753	512310.604582	43.318823
3503.081543	512297.340494	43.323828
3503.410311	512295.467508	43.328833
3503.290629	512302.821014	43.333837
3503.646021	512309.998265	43.338842
3503.687610	512298.104555	43.343847
3503.119136	512297.789715	43.348852
3503.390765	512300.174775	43.353857
3503.260522	512304.849024	43.358861
3503.442224	512298.800852	43.363866
3503.491465	512290.193855	43.368871
3503.304044	512274.491974	43.373876
3503.655897	512269.934407	43.378881
3503.560117	512262.918407	43.383885
3503.281024	512268.020860	43.388890
3503.389818	512262.894703	43.393895
3503.428770	512273.359334	43.398900
3503.446390	512249.025812	43.403905
3503.299275	512249.504298	43.408909
3503.428898	512241.946828	43.413914
3503.575551	512236.764097	43.418919
3503.080791	512239.371460	43.423924
3503.440782	512239.263962	43.428929
3503.451743	512245.281669	43.433933
3503.269825	512241.820130	43.438938
3503.613956	512229.018633	43.443943
3503.409039	512214.179384	43.448948
3503.760954	512203.197652	43.453953
3503.710890	512205.431233	43.458957
3503.608783	512200.085472	43.463962
3503.513473	512194.890386	43.468967
3503.481629	512167.934207	43.473972
3503.225125	512166.356045	43.478977
3503.333129	512173.825372	43.483981
3503.181969	512166.818085	43.488986
3503.247987	512159.068295	43.493991
3503.191965	512172.228946	43.498996
3503.740902	512166.982613	43.504001
3503.696498	512179.635583	43.509005
3503.525675	512142.584554	43.514010
3503.203478	512134.794942	43.519015
3503.299412	512134.273922	43.524020
3503.533532	512134.287486	43.529025
3503.416559	512134.053036	43.534029
3503.494489	512134.850046	43.539034
3503.436139	512126.209385	43.544039
3503.754301	512124.894482	43.549044
3503.526171	512100.903092	43.554049
3503.195161	512099.184947	43.559053
3503.645527	512085.304285	43.564058
3503.554649	512091.439310	43.569063
3503.620109	512094.666330	43.574068
3503.653925	512083.785380	43.579073
3503.591111	512074.943062	43.584077
3503.651357	512061.376959	43.589082
3503.938376	512064.821889	43.594087
3503.484844	512060.998567	43.599092
3503.763628	512035.763532	43.604097
3503.697474	512020.902182	43.609101
3503.371284	512024.545205	43.614106
3503.728200	512016.749375	43.619111
3503.450867	512009.053783	43.624116
3503.512068	511989.923190	43.629121
3503.252032	511992.746414	43.634125
3503.465162	511993.218556	43.639130
3503.849502	511982.180972	43.644135
3503.636048	511981.860599	43.649140
3503.806429	511973.335463	43.654145
3503.506945	511965.643352	43.659149
3503.764421	511940.715050	43.664154
3503.637109	511950.447389	43.669159
3503.435225	511950.327525	43.674164
3503.449379	511929.029164	43.679169
3503.669054	511929.399104	43.684173
3503.493339	511926.037689	43.689178
3503.526340	511919.557624	43.694183
3503.565376	511921.979499	43.699188
3503.745477	511919.624123	43.704193
3503.609023	511896.983740	43.709197
3503.582073	511873.061401	43.714202
3503.664353	511877.398669	43.719207
3503.440343	511879.457446	43.724212
3503.916431	511866.179558	43.729217
3503.647277	511844.824698	43.734221
3503.485598	511842.675084	43.739226
3503.685580	511843.756327	43.744231
3503.622636	511838.910110	43.749236
3503.614064	511819.436259	43.754241
3503.094662	511805.556884	43.759245
3503.322496	511797.680185	43.764250
3503.318014	511799.552521	43.769255
3503.084458	511800.247021	43.774260
3503.645209	511790.395471	43.779265
3503.328097	511793.581844	43.784269
3503.390761	511801.362012	43.789274
3503.425146	511799.434330	43.794279
3502.902962	511804.018907	43.799284
3503.529675	511795.219219	43.804289
3503.406361	511790.028435	43.809293
3503.446136	511768.219973	43.814298
3503.431424	511763.113186	43.819303
3503.543067	511773.617221	43.824308
3503.596307	511778.262615	43.829313
3503.593346	511779.730031	43.834317
3503.328357	511759.032011	43.839322
3503.555636	511739.014941	43.844327
3503.526291	511737.400835	43.849332
3503.436540	511723.149977	43.854337
3503.269423	511734.305116	43.859341
3503.517304	511736.896351	43.864346
3503.409246	511731.703137	43.869351
3503.124751	511725.677859	43.874356
3503.777345	511698.562175	43.879361
3503.745478	511700.135338	43.884365
3503.848990	511695.414528	43.889370
3503.844960	511680.138379	43.894375
3503.654467	511677.639200	43.899380
3503.750026	511660.273294	43.904385
3503.500863	511651.055524	43.909389
3503.586040	511651.952582	43.914394
3503.703301	511645.712022	43.919399
3503.529238	511629.400406	43.924404
3503.565557	511623.273802	43.929409
3503.410960	511612.928184	43.934413
3503.352544	511614.202037	43.939418
3503.850428	511605.574371	43.944423
3503.871439	511596.364456	43.949428
3504.013354	511573.983160	43.954433
3503.703105	511578.483714	43.959437
3503.814322	511561.772846	43.964442
3503.765759	511550.651646	43.969447
3503.649096	511533.167394	43.974452
3503.889470	511535.102231	43.979457
3503.721402	511521.420024	43.984461
3503.631760	511507.320725	43.989466
3503.718959	511498.504983	43.994471
3503.722767	511488.134253	43.999476
3503.554271	511489.981959	44.004481
3503.168283	511486.400760	44.009485
3503.515148	511466.920914	44.014490
3503.632862	511461.894279	44.019495
3503.528412	511462.315457	44.024500
3503.596494	511453.654472	44.029505
3503.682588	511451.263304	44.034509
3503.337038	511435.484465	44.039514
3503.554677	511413.293334	44.044519
3503.670632	511413.780851	44.049524
3503.734577	511405.373425	44.054529
3503.520112	511413.551675	44.059533
3503.652576	511395.673804	44.064538
3503.638935	511373.114484	44.069543
3503.230067	511395.335856	44.074548
3503.490671	511372.632019	44.079553
3503.702762	511379.427625	44.084557
3503.539945	511366.655016	44.089562
3503.388606	511354.538205	44.094567
3503.437071	511338.241726	44.099572
3503.512509	511338.381544	44.104577
3503.571772	511339.282714	44.109581
3503.793421	511340.461738	44.114586
3503.695879	511335.165568	44.119591
3503.794868	511320.833956	44.124596
3503.982638	511305.274224	44.129601
3504.192150	511307.112792	44.134605
3503.790962	511273.687913	44.139610
3503.567249	511278.781908	44.144615
3503.639145	511273.206007	44.149620
3503.544865	511260.118966	44.154625
3503.771682	511245.868260	44.159629
3503.629464	511236.076909	44.164634
3503.781784	511220.725050	44.169639
3503.616269	511228.187437	44.174644
3503.565037	511205.279729	44.179649
3503.551609	511186.514135	44.184653
3503.599966	511179.879600	44.189658
3503.558417	511188.840017	44.194663
3503.315156	511188.726686	44.199668
3503.700492	511171.112134	44.204673
3503.685774	511158.417135	44.209677
3503.356301	511154.371651	44.214682
3503.906622	511137.843901	44.219687
3503.516877	511149.135784	44.224692
3503.435397	511130.583231	44.229697
3503.571947	511100.816460	44.234701
3503.606238	511088.265424	44.239706
3503.373420	511100.190170	44.244711
3503.475300	511093.193033	44.249716
3503.779724	511100.024744	44.254721
3503.620665	511092.006519	44.259725
3503.301356	511076.678483	44.264730
3503.607429	511056.951681	44.269735
3503.362674	511069.232445	44.274740
3503.789226	511058.187593	44.279745
3503.537116	511062.932030	44.284749
3503.786377	511039.369560	44.289754
3503.622984	511027.153246	44.294759
3503.331549	511035.445016	44.299764
3503.974621	511017.688397	44.304769
3503.397196	511018.589037	44.309773
3503.542231	511007.942757	44.314778
3504.059853	510994.101166	44.319783
3503.364464	510993.907529	44.324788
3503.445380	510988.279522	44.329793
3503.502230	510991.255176	44.334797
3503.528911	510974.405330	44.339802
3503.777766	510945.126412	44.344807
3503.625167	510935.235352	44.349812
3503.712208	510955.153066	44.354817
3503.679321	510946.558368	44.359821
3503.597423	510908.377667	44.364826
3503.647861	510911.253173	44.369831
3503.599495	510904.583231	44.374836
3503.880418	510906.815258	44.379841
3504.037479	510884.278899	44.384845
3504.043633	510870.669808	44.389850
3503.786775	510865.196320	44.394855
3503.446288	510854.727856	44.399860
3503.475991	510833.931545	44.404865
3503.884747	510822.939942	44.409869
3503.681453	510825.906152	44.414874
3503.803789	510820.524482	44.419879
3503.585581	510803.662584	44.424884
3503.603811	510777.455105	44.429889
3503.645238	510779.421473	44.434893
3503.586034	510768.908499	44.439898
3503.946064	510766.524529	44.444903
3503.621782	510752.714628	44.449908
3503.578215	510728.641541	44.454913
3503.525538	510743.067474	44.459917
3503.329567	510746.336069	44.464922
3503.282290	510742.448237	44.469927
3503.286242	510734.707609	44.474932
3503.294321	510714.066333	44.479937
3503.080594	510705.297742	44.484941
3503.206713	510697.031905	44.489946
3503.498310	510698.604626	44.494951
3503.265293	510703.548497	44.499956
3503.276322	510700.916147	44.504961
3503.604814	510701.673624	44.509965
3503.352661	510703.635812	44.514970
3503.549542	510705.931737	44.519975
3503.464459	510695.372221	44.524980
3503.716374	510676.968834	44.529985
3503.454764	510685.660766	44.534989
3503.455167	510671.900660	44.539994
3503.700180	510665.538375	44.544999
3503.320434	510678.144285	44.550004
3503.396626	510660.679244	44.555009
3503.663307	510637.315819	44.560013
3503.277483	510638.236784	44.565018
3503.593293	510627.816219	44.570023
3503.425875	510628.348546	44.575028
3503.564400	510630.097231	44.580033
3503.452691	510636.134895	44.585037
3503.635213	510622.194201	44.590042
3503.606474	510596.550341	44.595047
3502.991525	510593.207492	44.600052
3503.384401	510587.277105	44.605057
3503.718788	510589.551313	44.610061
3503.570654	510589.675885	44.615066
3503.829459	510583.311388	44.620071
3503.248265	510572.830206	44.625076
3503.374797	510558.240656	44.630081
3503.331164	510553.896907	44.635085
3503.636242	510553.089842	44.640090
3503.665827	510540.387380	44.645095
3503.518403	510549.567222	44.650100
3503.471190	510533.234505	44.655105
3503.636168	510520.864752	44.660109
3503.513375	510526.600675	44.665114
3503.888087	510520.015481	44.670119
3503.865320	510508.434224	44.675124
3503.698304	510481.446147	44.680129
3503.617673	510476.804692	44.685133
3503.400800	510473.753027	44.690138
3503.753763	510459.279372	44.695143
3503.443815	510452.245883	44.700148
3503.892844	510440.387657	44.705153
3503.678207	510433.946165	44.710157
3503.741626	510426.651299	44.715162
3503.704152	510419.625322	44.720167
3503.841934	510403.819724	44.725172
3503.800317	510390.723692	44.730177
3503.558702	510389.699488	44.735181
3503.623193	510384.579770	44.740186
3503.988239	510345.467153	44.745191
3503.797629	510352.326817	44.750196
3504.036300	510358.106845	44.755201
3503.847205	510328.794909	44.760205
3503.475837	510313.828539	44.765210
3503.887975	510318.923502	44.770215
3503.408323	510313.839174	44.775220
3503.883830	510288.772819	44.780225
3503.680821	510273.577446	44.785229
3503.684314	510265.583730	44.790234
3503.651330	510260.934686	44.795239
3503.752726	510255.303201	44.800244
3503.753149	510226.315263	44.805249
3503.724047	510214.835987	44.810253
3503.484489	510224.941178	44.815258
3503.805497	510212.344183	44.820263
3503.533283	510195.945526	44.825268
3503.581996	510184.656291	44.830273
3503.768995	510186.093822	44.835277
3503.759737	510193.936682	44.840282
3504.023888	510163.642212	44.845287
3503.458515	510149.768747	44.850292
3503.632583	510142.304502	44.855297
3503.621641	510146.049867	44.860301
3503.635792	510129.504707	44.865306
3503.518677	510118.089866	44.870311
3503.645072	510108.457772	44.875316
3503.746111	510096.401358	44.880321
3503.525562	510096.385608	44.885325
3503.462712	510082.533844	44.890330
3503.665746	510057.459625	44.895335
3503.542597	510058.035562	44.900340
3503.695692	510058.921971	44.905345
3503.483886	510058.955429	44.910349
3503.494802	510060.926702	44.915354
3503.314725	510027.767972	44.920359
3503.344644	510034.188187	44.925364
3503.459201	510023.495521	44.930369
3503.149822	510033.965992	44.935373
3503.239311	510024.845586	44.940378
3503.488312	510030.168781	44.945383
3503.371527	510032.817913	44.950388
3503.625683	510025.897453	44.955393
3503.598701	510030.201871	44.960397
3503.276876	509993.675931	44.965402
3503.718135	509987.889462	44.970407
3503.495160	510005.479535	44.975412
3503.456016	509981.354105	44.980417
3503.609208	509989.373746	44.985421
3503.091130	509982.676499	44.990426
3503.495206	509966.423687	44.995431
3503.143193	509964.556868	45.000436
3503.205457	509954.580690	45.005441
3503.305272	509948.494040	45.010445
3503.725583	509943.419133	45.015450
3503.210549	509958.070574	45.020455
3503.252954	509951.588275	45.025460
3503.616137	509943.790512	45.030465
3503.168964	509950.286162	45.035469
3503.334663	509941.254847	45.040474
3503.255591	509911.773035	45.045479
3503.109470	509909.165401	45.050484
3503.148065	509904.656719	45.055489
3503.552904	509910.360046	45.060493
3503.378442	509914.283078	45.065498
3503.370801	509916.510253	45.070503
3503.104754	509916.096969	45.075508
3503.382109	509911.702325	45.080513
3503.693762	509918.027465	45.085517
3503.560581	509916.075464	45.090522
3503.716515	509885.747015	45.095527
3503.481551	509880.978019	45.100532
3503.343705	509877.863165	45.105537
3503.084145	509887.566990	45.110541
3503.561678	509878.739311	45.115546
3503.815779	509874.753059	45.120551
3503.634796	509877.159408	45.125556
3503.791928	509839.950353	45.130561
3503.810642	509840.554468	45.135565
3503.543032	509831.743352	45.140570
3503.745345	509822.959143	45.145575
3503.501251	509815.560847	45.150580
3503.682750	509788.921320	45.155585
3503.500344	509798.865956	45.160589
3503.471796	509799.528133	45.165594
3503.578438	509791.011983	45.170599
3503.361559	509770.556895	45.175604
3503.107527	509762.704827	45.180609
3503.502749	509754.800732	45.185613
3503.461527	509754.402501	45.190618
3503.334885	509754.574273	45.195623
3503.532521	509743.058844	45.200628
3503.596318	509756.404787	45.205633
3503.541150	509743.259810	45.210637
3503.277197	509727.011170	45.215642
3503.702382	509713.284339	45.220647
3503.365937	509715.057596	45.225652
3503.653871	509716.479215	45.230657
3503.438791	509709.126877	45.235661
3503.430251	509716.514522	45.240666
3503.250903	509684.468017	45.245671
3503.019886	509680.052479	45.250676
3502.983525	509674.189619	45.255681
3503.156405	509666.624173	45.260685
3503.388753	509670.584147	45.265690
3503.558092	509665.852373	45.270695
3503.199339	509680.529942	45.275700
3503.474723	509668.040941	45.280705
3503.297449	509667.360663	45.285709
3503.486426	509675.931299	45.290714
3503.295553	509677.175640	45.295719
3503.222535	509678.097806	45.300724
3503.352464	509677.672522	45.305729
3503.126989	509653.778446	45.310733
3503.159869	509641.783075	45.315738
3503.500412	509630.295577	45.320743
3503.330754	509640.238290	45.325748
3503.347242	509639.780344	45.330753
3503.457018	509618.919307	45.335757
3503.337747	509638.314659	45.340762
3503.896045	509637.872263	45.345767
3503.412326	509624.390195	45.350772
3503.622460	509604.069785	45.355777
3503.342451	509590.302536	45.360781
3503.483961	509594.175701	45.365786
3503.639915	509596.427654	45.370791
3503.421175	509600.003615	45.375796
3503.441981	509593.322227	45.380801
3503.356927	509576.387479	45.385805
3503.614623	509564.103565	45.390810
3503.546037	509557.992800	45.395815
3503.598987	509565.927299	45.400820
3503.547587	509560.370327	45.405825
3503.769573	509557.552684	45.410829
3503.636108	509545.583538	45.415834
3503.621227	509517.305101	45.420839
3503.372899	509523.921259	45.425844
3503.471159	509507.210429	45.430849
3503.713056	509523.614504	45.435853
3503.138421	509496.233969	45.440858
3503.344181	509482.541634	45.445863
3503.328459	509478.648527	45.450868
3503.578880	509462.824259	45.455873
3503.593883	509465.250282	45.460877
3503.368133	509481.981267	45.465882
3503.878268	509474.413026	45.470887
3503.597489	509470.359441	45.475892
3503.689766	509445.301832	45.480897
3503.669595	509438.019756	45.485901
3503.315804	509438.530983	45.490906
3503.659799	509427.194579	45.495911
3503.477050	509426.262196	45.500916
3503.369359	509408.167243	45.505921
3503.326964	509414.295567	45.510925
3503.497016	509412.599135	45.515930
3503.646067	509407.263392	45.520935
3503.304625	509410.909376	45.525940
3503.466999	509414.829877	45.530945
3503.566870	509384.914140	45.535949
3503.596868	509374.436803	45.540954
3503.496809	509367.572061	45.545959
3503.292711	509376.508526	45.550964
3503.754251	509365.001727	45.555969
3503.522292	509374.043781	45.560973
3503.138516	509352.552136	45.565978
3503.293352	509327.686836	45.570983
3503.257845	509323.695636	45.575988
3503.176389	509330.437271	45.580993
3503.617741	509339.069373	45.585997
3503.090946	509331.968509	45.591002
3503.533429	509322.741348	45.596007
3503.438831	509327.866106	45.601012
3503.754530	509314.763369	45.606017
3503.366427	509297.926835	45.611021
3503.031470	509307.895866	45.616026
3503.465783	509285.718322	45.621031
3503.378811	509293.219731	45.626036
3503.456733	509296.242942	45.631041
3503.184867	509293.250348	45.636045
3503.332082	509282.147319	45.641050
3503.083995	509286.183315	45.646055
3502.953078	509292.831597	45.651060
3503.417694	509292.808740	45.656065
3503.447446	509298.217408	45.661069
3503.023870	509304.102462	45.666074
3503.363258	509291.198333	45.671079
3503.100677	509286.484127	45.676084
3503.261654	509268.144194	45.681089
3503.141477	509262.952142	45.686093
3503.392726	509257.903756	45.691098
3503.530188	509259.045640	45.696103
3503.456537	509273.273756	45.701108
3503.610581	509262.270820	45.706113
3503.193208	509268.256090	45.711117
3503.221376	509269.415248	45.716122
3503.682943	509260.083852	45.721127
3503.414908	509241.153992	45.726132
3503.295839	509240.616275	45.731137
3503.442718	509227.489561	45.736141
3503.212261	509223.175001	45.741146
3503.475652	509213.976087	45.746151
3503.054786	509230.636970	45.751156
3503.290173	509221.442485	45.756161
3503.498801	509229.048980	45.761165
3503.202179	509220.191541	45.766170
3503.627981	509214.710813	45.771175
3503.396265	509194.257382	45.776180
3503.686298	509177.617107	45.781185
3503.649745	509191.991205	45.786189
3503.749716	509192.633092	45.791194
3503.834389	509161.049807	45.796199
3503.244196	509149.962055	45.801204
3503.342292	509137.298317	45.806209
3503.486656	509134.948211	45.811213
3503.277865	509139.281587	45.816218
3503.482536	509143.701394	45.821223
3503.503812	509140.105920	45.826228
3503.214184	509128.565906	45.831233
3503.338114	509120.451434	45.836237
3503.106951	509110.875293	45.841242
3503.545040	509095.324583	45.846247
3503.264948	509113.025783	45.851252
3503.104389	509097.468505	45.856257
3503.358500	509097.580105	45.861261
3503.222738	509107.770733	45.866266
3503.246134	509100.329850	45.871271
3503.283707	509102.752357	45.876276
3503.293365	509100.929466	45.881281
3503.487200	509101.505929	45.886285
3503.280041	509108.115739	45.891290
3503.520742	509094.670538	45.896295
3503.482919	509070.442431	45.901300
3503.292430	509059.392633	45.906305
3503.600138	509058.079154	45.911309
3503.170257	509060.221396	45.916314
3503.480403	509055.214235	45.921319
3503.585036	509061.774785	45.926324
3503.619523	509042.594520	45.931329
3503.505156	509027.333437	45.936333
3503.374767	509025.583265	45.941338
3503.585404	509016.847922	45.946343
3503.408038	509025.173226	45.951348
3503.628812	509023.873484	45.956353
3503.732297	509016.976433	45.961357
3503.449206	508995.215459	45.966362
3503.593628	508971.565529	45.971367
3503.527764	508982.858239	45.976372
3503.407954	508975.844682	45.981377
3503.421658	508974.223511	45.986381
3503.225981	508986.548602	45.991386
3503.651463	508969.836126	45.996391
3503.290304	508943.837582	46.001396
3502.972156	508952.083984	46.006401
3503.182057	508943.196940	46.011405
3503.230638	508934.638949	46.016410
3503.342597	508936.746162	46.021415
3503.182979	508948.256086	46.026420
3503.279851	508940.297586	46.031425
3503.358091	508944.737427	46.036429
3503.221076	508945.113218	46.041434
3503.470618	508938.850766	46.046439
3503.323901	508943.477941	46.051444
3503.558496	508945.616364	46.056449
3503.549647	508912.630788	46.061453
3503.192009	508908.842185	46.066458
3503.351144	508898.040586	46.071463
3503.125664	508918.161846	46.076468
3503.200795	508911.168046	46.081473
3503.512988	508894.827557	46.086477
3503.232796	508901.600770	46.091482
3503.342646	508910.386671	46.096487
3503.172867	508904.999976	46.101492
3503.018230	508915.294889	46.106497
3503.296647	508912.771784	46.111501
3503.110843	508906.021597	46.116506
3503.319403	508903.914280	46.121511
3502.995412	508912.465187	46.126516
3503.342782	508899.812471	46.131521
3503.261671	508887.986371	46.136525
3503.138697	508886.083232	46.141530
3503.465631	508865.136365	46.146535
3503.241267	508869.320489	46.151540
3503.605799	508867.390891	46.156545
3503.301138	508882.111185	46.161549
3502.912036	508876.607364	46.166554
3503.296480	508876.799553	46.171559
3502.968443	508896.228737	46.176564
3503.224508	508873.117556	46.181569
3503.619672	508876.697826	46.186573
3503.272856	508879.940022	46.191578
3503.579158	508856.061974	46.196583
3503.352464	508853.011568	46.201588
3503.118288	508847.685627	46.206593
3503.343680	508840.971613	46.211597
3503.268935	508836.278189	46.216602
3503.491479	508821.216643	46.221607
3503.218641	508825.712002	46.226612
3503.115337	508825.981280	46.231617
3503.282799	508826.308952	46.236621
3503.022471	508826.097110	46.241626
3503.297083	508831.871976	46.246631
3503.188600	508836.189574	46.251636
3502.991683	508825.697172	46.256641
3503.266636	508830.004765	46.261645
3502.968613	508834.352321	46.266650
3503.229726	508841.900098	46.271655
3503.305366	508844.266032	46.276660
3503.102612	508840.402341	46.281665
3503.235233	508830.515577	46.286669
3503.204218	508820.351108	46.291674
3503.267990	508814.421534	46.296679
3502.967974	508814.823091	46.301684
3503.158987	508810.492408	46.306689
3502.782024	508806.858618	46.311693
3503.069860	508813.491495	46.316698
3502.946240	508808.451631	46.321703
3502.882175	508820.503071	46.326708
3502.914321	508831.780389	46.331713
3503.101782	508838.530309	46.336717
3503.285815	508854.590013	46.341722
3503.593280	508852.062308	46.346727
3503.548912	508837.751274	46.351732
3503.374254	508824.877447	46.356737
3503.438000	508819.302036	46.361741
3503.049540	508822.955574	46.366746
3503.112751	508815.660057	46.371751
3503.108440	508822.339104	46.376756
3502.998471	508829.540786	46.381761
3503.166414	508825.972660	46.386765
3503.168968	508835.230901	46.391770
3503.375590	508823.713437	46.396775
3502.904173	508833.704309	46.401780
3503.328431	508824.226793	46.406785
3503.627052	508831.616866	46.411789
3503.189157	508836.087716	46.416794
3503.509523	508827.942060	46.421799
3503.180435	508807.807120	46.426804
3503.095379	508798.157117	46.431809
3503.447215	508786.970835	46.436813
3503.271219	508784.671314	46.441818
3503.359628	508773.071312	46.446823
3503.359074	508784.505611	46.451828
3503.257932	508779.917532	46.456833
3503.320206	508783.853998	46.461837
3502.873769	508787.972052	46.466842
3503.537432	508781.745279	46.471847
3503.179304	508792.628960	46.476852
3503.223434	508789.232177	46.481857
3503.848020	508781.746732	46.486861
3503.392390	508770.030337	46.491866
3503.147331	508745.733338	46.496871
3503.186331	508745.676563	46.501876
3503.333807	508746.209771	46.506881
3503.218387	508751.540368	46.511885
3503.111027	508738.959404	46.516890
3502.987698	508742.975808	46.521895
3503.051775	508752.730310	46.526900
3503.016946	508750.560254	46.531905
3503.228573	508746.023921	46.536909
3503.255415	508752.040350	46.541914
3503.550010	508742.735065	46.546919
3503.373606	508762.899344	46.551924
3503.532083	508743.597961	46.556929
3503.695275	508726.016011	46.561933
3503.698097	508725.054259	46.566938
3503.550027	508721.283087	46.571943
3503.300175	508713.429876	46.576948
3503.405240	508718.067912	46.581953
3503.182420	508707.883097	46.586957
3503.170888	508705.557571	46.591962
3503.301662	508706.700550	46.596967
3503.366869	508708.410427	46.601972
3503.320435	508681.400455	46.606977
3503.206846	508666.543682	46.611981
3502.863660	508671.252577	46.616986
3503.287113	508669.010080	46.621991
3503.227319	508669.525455	46.626996
3503.431627	508669.746118	46.632001
3503.393712	508675.418649	46.637005
3503.014288	508668.547186	46.642010
3503.419215	508672.530711	46.647015
3503.417747	508691.048410	46.652020
3503.223997	508677.975113	46.657025
3503.375105	508675.219124	46.662029
3503.373669	508681.341235	46.667034
3503.136737	508658.661844	46.672039
3503.287517	508641.840683	46.677044
3503.340939	508634.496042	46.682049
3503.220837	508628.241304	46.687053
3503.025680	508642.944495	46.692058
3503.406056	508636.003528	46.697063
3503.206383	508638.868352	46.702068
3503.143289	508642.166939	46.707073
3503.541620	508644.431304	46.712077
3502.948957	508646.902890	46.717082
3503.211728	508638.007333	46.722087
3503.121472	508636.554344	46.727092
3503.044122	508645.622938	46.732097
3503.493519	508649.346468	46.737101
3503.188375	508645.802481	46.742106
3503.430623	508643.942780	46.747111
3503.369820	508638.386995	46.752116
3503.525598	508619.693032	46.757121
3503.455505	508609.534615	46.762125
3503.350317	508615.824931	46.767130
3503.352241	508600.393305	46.772135
3503.432265	508598.963995	46.777140
3503.498550	508610.438441	46.782145
3503.831640	508602.644829	46.787149
3503.320554	508588.204974	46.792154
3503.460420	508563.543313	46.797159
3503.368555	508558.194790	46.802164
3503.261576	508571.315672	46.807169
3503.505972	508570.315732	46.812173
3503.609783	508573.689141	46.817178
3503.595459	508561.346316	46.822183
3503.157044	508542.543802	46.827188
3503.294783	508535.034008	46.832193
3503.410468	508533.396678	46.837197
3503.296565	508533.262878	46.842202
3503.226354	508522.649076	46.847207
3503.082051	508523.936733	46.852212
3503.381518	508525.609604	46.857217
3503.569607	508532.359545	46.862221
3503.454950	508530.202078	46.867226
3503.514895	508506.008318	46.872231
3503.425804	508487.909456	46.877236
3503.445128	508489.171254	46.882241
3503.413337	508481.131688	46.887245
3503.286892	508487.020652	46.892250
3503.711591	508483.209496	46.897255
3503.028971	508499.457101	46.902260
3503.348399	508479.118088	46.907265
3503.735973	508472.985436	46.912269
3503.438548	508462.812266	46.917274
3503.448088	508448.188819	46.922279
3503.690686	508454.980770	46.927284
3503.339619	508453.265417	46.932289
3503.677865	508444.307237	46.937293
3503.222290	508436.941768	46.942298
3503.490593	508414.283392	46.947303
3503.502589	508408.918407	46.952308
3503.424469	508416.621177	46.957313
3503.344685	508413.547474	46.962317
3503.213308	508418.678316	46.967322
3503.275898	508399.341107	46.972327
3503.461321	508407.912940	46.977332
3503.166507	508400.117287	46.982337
3503.482921	508404.924384	46.987341
3503.112751	508398.911466	46.992346
3503.403142	508380.145373	46.997351
3503.221196	508369.447946	47.002356
3502.966983	508362.505976	47.007361
3503.422049	508359.853682	47.012365
3503.261066	508377.233241	47.017370
3503.380521	508366.083415	47.022375
3503.399969	508376.654706	47.027380
3503.440957	508375.484523	47.032385
3503.670073	508373.576274	47.037389
3503.456297	508362.985064	47.042394
3503.755724	508333.693696	47.047399
3503.521992	508341.623476	47.052404
3503.024218	508339.627727	47.057409
3503.406308	508334.204225	47.062413
3503.345242	508332.847787	47.067418
3503.406071	508338.656608	47.072423
3503.345915	508336.237527	47.077428
3503.503963	508323.917883	47.082433
3503.590314	508299.922042	47.087437
3503.574715	508291.728042	47.092442
3503.583296	508280.140326	47.097447
3503.464929	508290.885237	47.102452
3503.409817	508293.170722	47.107457
3503.493609	508277.169319	47.112461
3503.492711	508265.380709	47.117466
3503.306829	508244.817712	47.122471
3503.421956	508246.873914	47.127476
3503.383644	508247.132929	47.132481
3503.662334	508251.794245	47.137485
3503.540914	508260.515839	47.142490
3503.799111	508247.471976	47.147495
3503.726171	508231.495302	47.152500
3503.611719	508234.093746	47.157505
3503.871996	508220.745961	47.162509
3503.700280	508207.213463	47.167514
3503.393514	508190.615965	47.172519
3503.324641	508190.323258	47.177524
3503.331289	508176.914334	47.182529
3503.714173	508181.053244	47.187533
3503.374561	508181.612859	47.192538
3503.654229	508176.559666	47.197543
3503.569229	508151.629382	47.202548
3503.416696	508147.656406	47.207553
3503.737415	508131.060868	47.212557
3503.383761	508132.634620	47.217562
3503.298424	508136.392181	47.222567
3503.204578	508141.011215	47.227572
3503.321339	508138.058186	47.232577
3503.441500	508110.009071	47.237581
3503.138865	508106.464576	47.242586
3503.717068	508092.003929	47.247591
3503.449612	508094.677172	47.252596
3503.154667	508101.958988	47.257601
3503.754844	508084.914471	47.262605
3503.626134	508092.018230	47.267610
3503.317117	508072.182832	47.272615
3503.395736	508069.084032	47.277620
3503.371210	508061.751466	47.282625
3503.538427	508048.519448	47.287629
3503.177052	508064.008343	47.292634
3503.355702	508059.730022	47.297639
3503.334713	508053.054642	47.302644
3503.321328	508054.169854	47.307649
3503.471457	508050.047826	47.312653
3503.383079	508044.799784	47.317658
3503.487759	508028.491273	47.322663
3503.557562	508017.855031	47.327668
3503.394648	508013.782471	47.332673
3503.623837	508009.546747	47.337677
3503.095389	508023.948967	47.342682
3503.391094	508013.277018	47.347687
3503.177414	508018.370390	47.352692
3503.114013	508014.535084	47.357697
3503.346323	508003.670764	47.362701
3503.164800	507986.952082	47.367706
3503.170488	507974.049114	47.372711
3503.104989	507980.991140	47.377716
3503.214135	507978.494654	47.382721
3503.784797	507973.243622	47.387725
3503.203831	507979.204595	47.392730
3503.392356	507966.930476	47.397735
3503.295191	507971.195906	47.402740
3503.253950	507977.476347	47.407745
3503.457550	507971.170210	47.412749
3503.226784	507986.638531	47.417754
3503.231315	507958.708638	47.422759
3503.055847	507945.480106	47.427764
3503.188395	507939.185187	47.432769
3503.408875	507925.033921	47.437773
3503.105067	507939.097129	47.442778
3503.066176	507948.463589	47.447783
3503.571207	507928.043998	47.452788
3503.052548	507941.230425	47.457793
3503.286530	507931.630705	47.462797
3503.125431	507940.004557	47.467802
3503.442497	507934.641805	47.472807
3503.300245	507940.735839	47.477812
3503.527764	507950.110789	47.482817
3503.326878	507939.618473	47.487821
3503.322458	507946.146088	47.492826
3503.346430	507915.986813	47.497831
3503.586182	507908.410027	47.502836
3503.164552	507909.134402	47.507841
3503.283052	507894.999230	47.512845
3503.485536	507904.631144	47.517850
3503.591163	507900.819694	47.522855
3503.324426	507903.037484	47.527860
3503.503673	507902.604365	47.532865
3503.526841	507880.945366	47.537869
3503.371786	507857.998997	47.542874
3503.491504	507852.465023	47.547879
3503.322328	507847.432077	47.552884
3502.973737	507855.582620	47.557889
3503.049562	507849.752003	47.562893
3503.270532	507854.169567	47.567898
3503.282088	507852.953403	47.572903
3503.583240	507861.254234	47.577908
3503.392702	507860.727768	47.582913
3503.634363	507845.510560	47.587917
3503.561289	507839.551683	47.592922
3503.616711	507835.191590	47.597927
3503.372530	507830.777654	47.602932
3503.635841	507816.315950	47.607937
3503.491171	507808.344507	47.612941
3503.442922	507800.863790	47.617946
3503.602557	507775.691911	47.622951
3503.467649	507777.939478	47.627956
3503.245199	507769.727326	47.632961
3503.530468	507765.685067	47.637965
3503.192301	507774.188178	47.642970
3503.204060	507775.198240	47.647975
3503.353530	507772.391770	47.652980
3503.206206	507770.340564	47.657985
3503.324339	507778.923345	47.662989
3503.294625	507753.174198	47.667994
3503.328747	507735.814026	47.672999
3503.358580	507740.464217	47.678004
3503.048108	507740.563866	47.683009
3503.376045	507730.443216	47.688013
3503.252800	507744.781625	47.693018
3503.155423	507734.171631	47.698023
3503.266178	507735.570825	47.703028
3503.398180	507735.802929	47.708033
3503.299293	507739.512121	47.713037
3503.358291	507744.613073	47.718042
3503.428891	507726.437575	47.723047
3503.561321	507707.341539	47.728052
3503.269744	507701.923119	47.733057
3503.361245	507699.884756	47.738061
3503.110506	507709.841397	47.743066
3503.250030	507697.726623	47.748071
3503.337187	507710.817476	47.753076
3503.091752	507705.138779	47.758081
3502.990018	507701.764835	47.763085
3503.142234	507704.928377	47.768090
3503.196112	507703.857305	47.773095
3503.376935	507700.084523	47.778100
3503.184327	507713.776159	47.783105
3503.543912	507705.724972	47.788109
3503.359877	507704.843293	47.793114
3503.287229	507686.842185	47.798119
3503.277605	507675.611120	47.803124
3503.371749	507664.819022	47.808129
3503.457265	507662.983989	47.813133
3503.245615	507665.952060	47.818138
3503.471326	507660.654260	47.823143
3503.459715	507665.412215	47.828148
3502.948615	507669.996126	47.833153
3503.360115	507658.951478	47.838157
3503.420237	507668.049455	47.843162
3503.247030	507649.811216	47.848167
3503.468017	507632.674393	47.853172
3503.547905	507626.387684	47.858177
3503.525180	507623.608405	47.863181
3503.427602	507623.117836	47.868186
3503.148090	507621.897062	47.873191
3503.475868	507622.148823	47.878196
3503.302782	507630.322330	47.883201
3503.778841	507610.109332	47.888205
3503.783192	507609.046082	47.893210
3503.708134	507598.179490	47.898215
3503.850382	507596.183692	47.903220
3503.421920	507581.932321	47.908225
3503.516984	507560.565143	47.913229
3503.179060	507548.120944	47.918234
3503.336086	507555.078569	47.923239
3503.583682	507541.631069	47.928244
3503.087400	507544.340562	47.933249
3503.258427	507551.295975	47.938253
3503.457491	507548.380436	47.943258
3503.875344	507536.575742	47.948263
3503.450637	507524.550024	47.953268
3503.323019	507503.723946	47.958273
3503.584552	507505.251121	47.963277
3503.135693	507509.875835	47.968282
3503.078731	507498.500344	47.973287
3503.445965	507501.022767	47.978292
3503.243340	507511.528492	47.983297
3503.180362	507502.936824	47.988301
3503.146334	507498.287198	47.993306
3503.328986	507502.508518	47.998311
3503.392904	507503.004375	48.003316
3503.173239	507484.874499	48.008321
3503.317799	507466.079866	48.013325
3503.182157	507469.440740	48.018330
3503.568396	507456.780827	48.023335
3503.486697	507463.573827	48.028340
3503.043062	507468.197726	48.033345
3503.517182	507460.735497	48.038349
3503.422796	507469.655607	48.043354
3503.382548	507451.952721	48.048359
3503.332237	507468.809723	48.053364
3503.037537	507455.144279	48.058369
3503.297020	507421.152082	48.063373
3503.245611	507433.657870	48.068378
3502.992013	507421.352046	48.073383
3503.441254	507422.141191	48.078388
3503.145630	507425.071977	48.083393
3503.327345	507417.099367	48.088397
3503.200890	507432.501099	48.093402
3503.314035	507422.363619	48.098407
3503.575070	507428.444691	48.103412
3503.410711	507426.244343	48.108417
3503.372903	507418.458222	48.113421
3503.339245	507426.862777	48.118426
3503.049051	507391.490059	48.123431
3503.511920	507396.324890	48.128436
3503.074133	507384.807121	48.133441
3503.548370	507387.616238	48.138445
3503.410621	507390.370284	48.143450
3503.538035	507381.090691	48.148455
3503.727296	507381.313751	48.153460
3503.188818	507383.372162	48.158465
3503.590337	507382.701508	48.163469
3503.323321	507367.614875	48.168474
3503.089204	507350.802693	48.173479
3503.587136	507339.238200	48.178484
3503.507375	507344.361201	48.183489
3503.351709	507340.388533	48.188493
3503.186528	507346.081614	48.193498
3503.614597	507335.894311	48.198503
3503.722365	507333.903932	48.203508
3503.316669	507325.366343	48.208513
3503.559526	507311.818218	48.213517
3503.094142	507306.022358	48.218522
3503.297979	507304.421578	48.223527
3503.687318	507312.708736	48.228532
3503.053114	507305.624003	48.233537
3503.239771	507311.059095	48.238541
3503.246766	507313.587883	48.243546
3503.387756	507305.267470	48.248551
3503.418342	507288.514588	48.253556
3503.205092	507286.625539	48.258561
3503.502736	507276.813002	48.263565
3503.163647	507269.934604	48.268570
3503.053583	507260.186496	48.273575
3503.156749	507264.218043	48.278580
3503.341037	507265.959842	48.283585
3503.270586	507269.006861	48.288589
3503.304751	507264.245197	48.293594
3503.463794	507274.795100	48.298599
3503.254909	507264.708424	48.303604
3502.989232	507285.900504	48.308609
3503.357903	507266.614849	48.313613
3503.160599	507271.908244	48.318618
3503.151404	507275.856351	48.323623
3503.249264	507281.912667	48.328628
3503.249219	507270.730423	48.333633
3503.359423	507251.435003	48.338637
3503.163014	507246.507383	48.343642
3503.483382	507231.074802	48.348647
3503.345530	507228.920838	48.353652
3503.114681	507234.067751	48.358657
3503.262185	507218.409488	48.363661
3503.309760	507239.552115	48.368666
3503.001701	507235.046925	48.373671
3503.279801	507225.085653	48.378676
3503.265329	507225.948097	48.383681
3503.324605	507222.396816	48.388685
3503.239932	507229.898757	48.393690
3503.115440	507232.195347	48.398695
3503.149565	507229.710610	48.403700
3503.179034	507238.712462	48.408705
3503.370707	507223.249616	48.413709
3503.178980	507196.665072	48.418714
3503.246241	507184.814354	48.423719
3503.261052	507187.847911	48.428724
3503.104171	507191.414590	48.433729
3503.509988	507181.382509	48.438733
3503.165303	507193.428836	48.443738
3503.448981	507186.097786	48.448743
3503.382998	507194.406366	48.453748
3502.864096	507181.686915	48.458753
3502.950208	507183.697232	48.463757
3503.412846	507181.600150	48.468762
3503.210693	507197.722435	48.473767
3503.270755	507193.614440	48.478772
3503.512607	507190.135494	48.483777
3503.457042	507178.860769	48.488781
3503.359200	507159.142740	48.493786
3503.178366	507145.813246	48.498791
3503.365746	507146.036607	48.503796
3503.067899	507150.435153	48.508801
3503.411346	507146.889543	48.513805
3503.344902	507152.415286	48.518810
3503.110747	507151.490901	48.523815
3503.311371	507144.628348	48.528820
3503.251297	507152.531224	48.533825
3503.292323	507145.289107	48.538829
3502.930363	507159.766927	48.543834
3503.035812	507165.720886	48.548839
3503.415528	507149.013886	48.553844
3503.264010	507159.967134	48.558849
3503.083238	507151.292712	48.563853
3503.205186	507166.756618	48.568858
3503.403614	507152.456411	48.573863
3503.199007	507138.422286	48.578868
3503.644931	507117.960485	48.583873
3503.338594	507125.092715	48.588877
3503.172511	507130.887207	48.593882
3503.326956	507119.275658	48.598887
3503.521684	507119.447259	48.603892
3502.983743	507123.225974	48.608897
3503.527289	507123.595439	48.613901
3503.434158	507122.699362	48.618906
3503.219945	507106.440383	48.623911
3503.261707	507089.533745	48.628916
3503.129202	507083.078012	48.633921
3503.413099	507078.580420	48.638925
3503.426989	507067.497041	48.643930
3502.976439	507080.066168	48.648935
3503.363683	507072.212712	48.653940
3503.148092	507079.887207	48.658945
3503.246651	507071.269794	48.663949
3503.422029	507073.215417	48.668954
3503.254256	507077.138033	48.673959
3503.350799	507077.274553	48.678964
3503.015744	507077.580485	48.683969
3503.570973	507062.464828	48.688973
3503.507556	507058.022124	48.693978
3503.117597	507031.974647	48.698983
3503.391218	507023.734335	48.703988
3503.303031	507038.776175	48.708993
3503.273538	507040.551785	48.713997
3503.542875	507037.220262	48.719002
3503.501884	507031.407832	48.724007
3503.772044	507033.793870	48.729012
3502.975690	507019.751977	48.734017
3503.639452	506993.740299	48.739021
3503.075573	506996.612356	48.744026
3503.134376	506987.444594	48.749031
3503.678608	506987.409160	48.754036
3503.180197	506991.131057	48.759041
3503.572331	506982.517801	48.764045
3503.238465	506996.535923	48.769050
3503.322970	506984.834140	48.774055
3503.096435	506989.778047	48.779060
3503.124309	507001.512629	48.784065
3503.493413	506991.385043	48.789069
3503.252296	506979.481725	48.794074
3503.206699	506974.631389	48.799079
3503.161328	506958.041990	48.804084
3503.210607	506954.441635	48.809089
3503.319678	506962.823857	48.814093
3503.470456	506966.898548	48.819098
3503.341505	506962.972170	48.824103
3503.641487	506960.698373	48.829108
3503.223938	506973.920152	48.834113
3503.301829	506969.708087	48.839117
3503.310428	506971.072890	48.844122
3503.372249	506961.449245	48.849127
3503.462206	506928.191264	48.854132
3503.282621	506919.617737	48.859137
3503.366492	506919.958660	48.864141
3503.511953	506910.878360	48.869146
3503.599626	506920.022976	48.874151
3503.364310	506908.827084	48.879156
3503.381959	506929.721822	48.884161
3503.530769	506892.457122	48.889165
3503.401830	506882.812984	48.894170
3503.538343	506880.008418	48.899175
3503.328775	506882.672696	48.904180
3503.026324	506876.952138	48.909185
3503.527721	506884.513398	48.914189
3503.067193	506876.743245	48.919194
3503.274490	506885.413577	48.924199
3503.538615	506877.630092	48.929204
3503.162864	506882.294016	48.934209
3503.649111	506872.603242	48.939213
3503.442963	506843.490459	48.944218
3503.106383	506848.957794	48.949223
3503.174498	506851.325191	48.954228
3503.312789	506844.877169	48.959233
3503.492796	506833.160190	48.964237
3503.223456	506840.590286	48.969242
3503.454888	506841.818681	48.974247
3503.441718	506839.442563	48.979252
3503.190746	506851.018920	48.984257
3503.645945	506826.001347	48.989261
3503.498319	506809.529166	48.994266
3502.981797	506805.866406	48.999271
3503.464200	506798.200186	49.004276
3503.416606	506805.241052	49.009281
3503.534761	506810.940127	49.014285
3503.189782	506807.604453	49.019290
3503.171615	506797.284963	49.024295
3503.577141	506789.276692	49.029300
3503.113423	506798.053121	49.034305
3503.222715	506777.289926	49.039309
3503.180804	506770.971557	49.044314
3502.916846	506753.151513	49.049319
3503.155232	506753.974017	49.054324
3503.092452	506763.446094	49.059329
3503.392435	506763.702263	49.064333
3502.990584	506775.302516	49.069338
3502.996806	506772.670325	49.074343
3503.254882	506756.639971	49.079348
3503.208469	506767.273256	49.084353
3503.218665	506757.354058	49.089357
3503.397337	506760.007594	49.094362
3503.340615	506755.867353	49.099367
3503.082491	506760.866917	49.104372
3503.030153	506772.563731	49.109377
3503.299639	506768.371937	49.114381
3503.311213	506756.681527	49.119386
3503.364833	506768.665196	49.124391
3503.417716	506768.150822	49.129396
3503.033683	506763.202118	49.134401
3503.432740	506769.109809	49.139405
3503.456284	506757.012709	49.144410
3503.558263	506737.515618	49.149415
3503.567507	506717.324763	49.154420
3503.188677	506730.135807	49.159425
3503.483040	506726.243670	49.164429
3503.485914	506728.368396	49.169434
3503.424992	506718.561616	49.174439
3503.640390	506705.776358	49.179444
3503.401554	506693.265283	49.184449
3503.322210	506684.776996	49.189453
3503.314890	506681.134931	49.194458
3503.377125	506677.532471	49.199463
3503.545028	506677.505916	49.204468
3503.519702	506683.733711	49.209473
3503.636196	506670.103857	49.214477
3503.599375	506651.640610	49.219482
3503.095818	506647.014363	49.224487
3503.585042	506640.409600	49.229492
3503.140846	506653.484033	49.234497
3503.362329	506652.690007	49.239501
3503.531149	506649.374297	49.244506
3503.221177	506646.184859	49.249511
3503.648486	506626.383225	49.254516
3503.343584	506617.728154	49.259521
3503.486331	506600.096675	49.264525
3503.502716	506607.076910	49.269530
3503.440280	506606.530157	49.274535
3503.798833	506594.025793	49.279540
3503.233011	506590.977983	49.284545
3503.306595	506572.396001	49.289549
3503.461643	506562.403197	49.294554
3503.438993	506558.561127	49.299559
3503.705047	506558.620261	49.304564
3503.489761	506561.083089	49.309569
3503.419613	506555.123307	49.314573
3503.470566	506554.052627	49.319578
3503.342876	506536.818030	49.324583
3503.354458	506513.084532	49.329588
3503.115853	506506.240548	49.334593
3503.409348	506506.194143	49.339597
3503.243808	506510.217735	49.344602
3503.070165	506523.350705	49.349607
3503.296988	506508.134671	49.354612
3502.960835	506513.905647	49.359617
3503.155068	506502.793403	49.364621
3502.973194	506505.605164	49.369626
3502.665518	506520.783343	49.374631
3503.224067	506509.815927	49.379636
3503.409532	506510.090200	49.384641
3503.207617	506507.490865	49.389645
3502.869384	506516.095801	49.394650
3502.888073	506518.319254	49.399655
3503.216693	506518.874504	49.404660
3502.935651	506525.041571	49.409665
3503.054826	506508.931741	49.414669
3503.042021	506514.550411	49.419674
3503.118311	506527.643876	49.424679
3503.207841	506517.509600	49.429684
3503.190672	506521.509740	49.434689
3503.242077	506510.571877	49.439693
3503.394960	506512.723521	49.444698
3503.326283	506529.230134	49.449703
3503.465381	506516.811001	49.454708
3502.894671	506528.134503	49.459713
3503.295712	506515.522167	49.464717
3503.349025	506519.106363	49.469722
3503.115140	506509.225600	49.474727
3503.338026	506482.878035	49.479732
3503.350311	506484.039891	49.484737
3503.292855	506492.094456	49.489741
3503.213617	506491.044348	49.494746
3502.969643	506492.651510	49.499751
3503.185446	506486.848912	49.504756
3503.089082	506487.370132	49.509761
3503.316778	506478.428411	49.514765
3503.134567	506479.216202	49.519770
3503.144229	506482.453100	49.524775
3503.442449	506484.429974	49.529780
3503.399058	506488.586068	49.534785
3503.492840	506485.939994	49.539789
3503.105884	506495.868258	49.544794
3503.116853	506491.110048	49.549799
3503.381638	506470.929119	49.554804
3503.135850	506461.353814	49.559809
3503.105828	506446.836130	49.564813
3503.419408	506442.637288	49.569818
3503.260039	506439.525210	49.574823
3503.474614	506445.715174	49.579828
3503.256909	506442.662918	49.584833
3503.414471	506441.524781	49.589837
3503.512822	506445.253676	49.594842
3503.330750	506441.082570	49.599847
3503.506510	506441.813785	49.604852
3503.506939	506425.166038	49.609857
3503.228979	506406.082830	49.614861
3503.223084	506407.247564	49.619866
3503.246901	506403.600519	49.624871
3503.596440	506409.819765	49.629876
3503.308734	506403.287106	49.634881
3503.270762	506388.467023	49.639885
3503.222405	506402.997109	49.644890
3502.912943	506398.087114	49.649895
3503.336336	506411.125808	49.654900
3503.043725	506417.092337	49.659905
3503.388479	506408.081479	49.664909
3503.421120	506398.664538	49.669914
3503.116785	506387.884025	49.674919
3503.261924	506359.979933	49.679924
3503.322156	506360.678810	49.684929
3503.426864	506360.156233	49.689933
3503.477561	506363.589071	49.694938
3503.055428	506358.747473	49.699943
3503.297487	506352.738277	49.704948
3503.232494	506366.512007	49.709953
3503.325939	506359.311878	49.714957
3503.235319	506362.210441	49.719962
3503.156062	506370.369709	49.724967
3503.463776	506358.278020	49.729972
3503.230128	506364.184647	49.734977
3503.327929	506334.871168	49.739981
3503.361202	506333.044253	49.744986
3503.193913	506335.600730	49.749991
3503.313115	506321.666569	49.754996
3503.147965	506345.677569	49.760001
3503.317464	506333.101696	49.765005
3503.427192	506338.903460	49.770010
3503.222705	506327.854123	49.775015
3503.412288	506323.472446	49.780020
3503.014271	506342.561345	49.785025
3503.187828	506335.550949	49.790029
3503.281128	506336.801212	49.795034
3503.135964	506337.178345	49.800039
3503.429168	506326.809364	49.805044
3502.980600	506314.533567	49.810049
3503.013912	506285.736210	49.815053
3503.034294	506307.238479	49.820058
3503.189723	506315.664289	49.825063
3503.149920	506300.136005	49.830068
3503.217784	506300.985481	49.835073
3503.273487	506291.767242	49.840077
3503.258678	506300.422370	49.845082
3502.967258	506301.733440	49.850087
3503.323515	506293.024312	49.855092
3502.864406	506292.287237	49.860097
3503.195344	506297.244434	49.865101
3503.352769	506303.595285	49.870106
3503.030788	506290.742851	49.875111
3503.350444	506287.150227	49.880116
3503.033853	506307.288920	49.885121
3503.268063	506289.743874	49.890125
3503.178753	506302.054063	49.895130
3502.859826	506304.836915	49.900135
3503.378528	506293.774459	49.905140
3503.283722	506300.165176	49.910145
3503.243952	506306.749597	49.915149
3503.356884	506291.551373	49.920154
3503.179292	506299.270806	49.925159
3503.380267	506304.855756	49.930164
3503.310154	506300.110309	49.935169
3503.441885	506284.605501	49.940173
3503.339021	506265.848674	49.945178
3503.262908	506263.229419	49.950183
3503.529706	506265.008881	49.955188
3503.051250	506258.759320	49.960193
3503.135562	506268.562628	49.965197
3503.462716	506251.711271	49.970202
3503.199293	506257.774444	49.975207
3503.401785	506257.894227	49.980212
3502.890431	506254.635342	49.985217
3503.079148	506255.364517	49.990221
3503.272697	506257.003753	49.995226
3503.012248	506259.827971	50.000231
3503.469900	506252.620836	50.005236
3503.174984	506263.344306	50.010241
3503.259212	506260.294898	50.015245
3503.146200	506241.084237	50.020250
3503.401015	506224.294888	50.025255
3503.194883	506215.421600	50.030260
3502.913944	506225.232058	50.035265
3502.868778	506227.010228	50.040269
3503.310296	506219.552623	50.045274
3502.709670	506228.401577	50.050279
3503.099649	506224.949630	50.055284
3503.099145	506225.860517	50.060289
3503.011964	506222.281578	50.065293
3502.862933	506238.649364	50.070298
3502.920771	506258.172321	50.075303
3503.281145	506269.500637	50.080308
3502.885460	506263.845212	50.085313
3502.766597	506268.063887	50.090317
3503.194595	506269.058851	50.095322
3502.754141	506276.465631	50.100327
3502.882106	506278.064628	50.105332
3502.837331	506276.401846	50.110337
3502.936597	506274.311488	50.115341
3502.915810	506280.943520	50.120346
3502.986362	506277.086656	50.125351
3503.318835	506266.104217	50.130356
3502.843970	506277.210329	50.135361
3502.896993	506285.348730	50.140365
3502.988136	506274.353837	50.145370
3503.060168	506283.450660	50.150375
3503.130552	506278.581799	50.155380
3502.762314	506290.227663	50.160385
3503.016175	506272.983101	50.165389
3503.186567	506282.165581	50.170394
3503.152700	506279.489050	50.175399
3503.088849	506276.969061	50.180404
3502.957982	506281.645042	50.185409
3503.166058	506282.168752	50.190413
3503.684766	506278.696469	50.195418
3503.411282	506288.606916	50.200423
3503.162402	506279.285006	50.205428
3502.672857	506287.306754	50.210433
3502.990215	506284.979523	50.215437
3503.525598	506281.251599	50.220442
3503.286093	506278.303962	50.225447
3503.380918	506285.474333	50.230452
3503.183750	506280.748962	50.235457
3503.236931	506287.065693	50.240461
3503.274209	506275.370897	50.245466
3502.874253	506282.518267	50.250471
3502.991633	506281.791280	50.255476
3502.950097	506296.117972	50.260481
3503.197277	506287.729688	50.265485
3503.339376	506287.859015	50.270490
3503.249962	506293.995876	50.275495
3503.646242	506274.350549	50.280500
3503.205702	506256.557905	50.285505
3502.865539	506252.259936	50.290509
3503.102247	506233.145797	50.295514
3503.209407	506236.822743	50.300519
3503.209956	506249.118767	50.305524
3503.249800	506249.365459	50.310529
3503.264253	506242.177766	50.315533
3503.001367	506249.961303	50.320538
3502.983347	506257.149521	50.325543
3503.463898	506255.454310	50.330548
3503.063370	506258.401871	50.335553
3503.009041	506256.335786	50.340557
3503.198314	506252.105944	50.345562
3502.955364	506259.127306	50.350567
3503.280079	506245.970224	50.355572
3503.327490	506261.345515	50.360577
3503.415343	506254.702841	50.365581
3503.406702	506249.897063	50.370586
3503.174127	506260.509479	50.375591
3503.227215	506252.404861	50.380596
3503.104188	506269.578128	50.385601
3503.140368	506264.613467	50.390605
3503.388631	506262.499558	50.395610
3503.294716	506251.078487	50.400615
3503.099656	506224.796588	50.405620
3503.060284	506226.978653	50.410625
3503.385092	506215.896191	50.415629
3503.219549	506227.206453	50.420634
3502.903573	506219.817968	50.425639
3503.622590	506210.444248	50.430644
3503.342233	506217.471538	50.435649
3503.362592	506217.164695	50.440653
3503.333626	506230.173817	50.445658
3503.205519	506225.285711	50.450663
3503.279466	506223.249950	50.455668
3503.371262	506237.859225	50.460673
3503.159268	506237.234895	50.465677
3502.976655	506223.753169	50.470682
3502.894816	506232.975540	50.475687
3503.622391	506222.031830	50.480692
3503.192403	506207.880769	50.485697
3503.005506	506188.226313	50.490701
3503.490808	506179.648538	50.495706
3503.298245	506187.572792	50.500711
3503.161585	506179.498130	50.505716
3503.259105	506190.817440	50.510721
3503.408912	506181.483066	50.515725
3503.134112	506185.473399	50.520730
3503.299350	506176.187185	50.525735
3503.213396	506133.391791	50.530740
3503.028639	506113.028489	50.535745
3502.915618	506068.820366	50.540749
3503.120317	506022.537835	50.545754
3502.996997	505951.511965	50.550759
3502.921562	505876.632453	50.555764
3502.550910	505803.924589	50.560769
3502.901497	505707.875711	50.565773
3502.834584	505600.455966	50.570778
3502.339149	505484.753703	50.575783
3502.453312	505360.048038	50.580788
3501.964012	505225.872650	50.585793
3501.865987	505087.079966	50.590797
3501.877175	504941.740859	50.595802
3501.700105	504781.198023	50.600807
3501.847654	504612.556044	50.605812
3501.356214	504439.205810	50.610817
3501.225994	504253.904103	50.615821
3500.976195	504055.714383	50.620826
3500.340728	503855.559052	50.625831
3500.400995	503649.471461	50.630836
3499.993394	503438.698116	50.635841
3499.648984	503205.947478	50.640845
3499.400815	502983.452544	50.645850
3498.820811	502755.946111	50.650855
3498.968468	502501.345484	50.655860
3498.501838	502272.701443	50.660865
3498.343804	502002.603820	50.665869
3498.068506	501737.328977	50.670874
3497.388091	501482.793979	50.675879
3497.594854	501209.235415	50.680884
3497.049846	500918.278111	50.685889
3496.688477	500643.180911	50.690893
3496.250031	500345.262818	50.695898
3496.112074	500052.354173	50.700903
3495.908461	499745.277518	50.705908
3495.208134	499431.035323	50.710913
3494.913380	499112.319423	50.715917
3494.707522	498774.144702	50.720922
3494.003280	498461.101097	50.725927
3493.792769	498119.219284	50.730932
3493.383704	497787.892482	50.735937
3493.001525	497433.874704	50.740941
3492.492017	497101.842437	50.745946
3491.856233	496730.688298	50.750951
3491.675159	496369.226189	50.755956
3490.853106	496012.819993	50.760961
3490.431773	495648.191823	50.765965
3490.219276	495280.536044	50.770970
3489.144160	494922.021974	50.775975
3488.951390	494538.094807	50.780980
3488.434083	494173.604322	50.785985
3487.995911	493784.180905	50.790989
3487.570476	493391.607700	50.795994
3486.753431	493016.912872	50.800999
3486.561958	492614.259689	50.806004
3486.129320	492223.435195	50.811009
3485.224074	491820.016674	50.816013
3484.939005	491414.212427	50.821018
3484.439768	491004.027142	50.826023
3483.813376	490588.990982	50.831028
3483.317427	490179.850621	50.836033
3482.822383	489761.432674	50.841037
3482.490523	489348.044472	50.846042
3481.440847	488926.757971	50.851047
3481.390761	488498.567470	50.856052
3480.423932	488072.690202	50.861057
3479.925137	487645.108460	50.866061
3479.412565	487213.720169	50.871066
3478.499463	486781.169656	50.876071
3477.933371	486346.376223	50.881076
3477.372187	485916.181966	50.886081
3476.830756	485473.158176	50.891085
3476.197687	485030.037302	50.896090
3475.695577	484596.764462	50.901095
3475.622197	484147.556734	50.906100
3474.521642	483696.829000	50.911105
3473.972849	483270.373326	50.916109
3473.161585	482804.835607	50.921114
3472.315225	482354.188431	50.926119
3471.722374	481898.930585	50.931124
3471.580060	481465.885492	50.936129
3470.708966	481005.583832	50.941133
3470.077462	480564.286103	50.946138
3469.312641	480099.335221	50.951143
3468.826064	479644.818931	50.956148
3468.172927	479191.382672	50.961153
3467.293927	478742.481920	50.966157
3466.976292	478277.924200	50.971162
3466.089000	477822.618533	50.976167
3465.576097	477361.820499	50.981172
3464.491620	476904.649850	50.986177
3464.088522	476442.698255	50.991181
3463.599064	475987.541255	50.996186
3462.814814	475527.757544	51.001191
3462.131739	475068.808993	51.006196
3461.516299	474598.536106	51.011201
3460.833943	474140.732153	51.016205
3460.333647	473675.133614	51.021210
3459.393840	473220.390954	51.026215
3458.936342	472741.229913	51.031220
3458.078318	472290.762380	51.036225
3457.409303	471822.917732	51.041229
3456.756750	471359.571674	51.046234
3456.155401	470886.372010	51.051239
3455.383942	470435.799405	51.056244
3454.894225	469974.170868	51.061249
3453.782077	469501.223018	51.066253
3453.096959	469050.555925	51.071258
3452.498404	468589.623616	51.076263
3452.079714	468131.796275	51.081268
3451.105285	467657.821450	51.086273
3450.563094	467206.128589	51.091277
3449.858526	466742.890648	51.096282
3448.814124	466292.068852	51.101287
3448.382077	465814.011570	51.106292
3447.804154	465358.583067	51.111297
3446.978547	464903.792473	51.116301
3446.385379	464438.255217	51.121306
3445.758937	463989.600463	51.126311
3444.890768	463523.072468	51.131316
3444.087825	463059.617628	51.136321
3443.353585	462603.140763	51.141325
3442.620181	462150.153581	51.146330
3441.791574	461700.620791	51.151335
3441.439953	461239.997159	51.156340
3440.961822	460791.658096	51.161345
3440.058802	460327.704022	51.166349
3439.379252	459867.204608	51.171354
3438.569046	459411.991407	51.176359
3437.901238	458954.920152	51.181364
3437.266666	458503.819772	51.186369
3436.662076	458048.748727	51.191373
3436.067756	457593.311588	51.196378
3435.092528	457139.497891	51.201383
3434.354876	456691.166914	51.206388
3433.695756	456238.705286	51.211393
3432.728136	455794.603286	51.216397
3432.097826	455331.414290	51.221402
3431.332296	454902.583999	51.226407
3430.853527	454436.968098	51.231412
3429.917714	453991.861441	51.236417
3429.398533	453550.789845	51.241421
3429.111451	453100.692348	51.246426
3428.032045	452655.835825	51.251431
3427.438932	452202.470896	51.256436
3427.034156	451759.875016	51.261441
3425.913639	451309.011306	51.266445
3425.329354	450867.289177	51.271450
3424.339429	450407.456367	51.276455
3423.590930	449964.322050	51.281460
3422.751986	449519.671162	51.286465
3422.044239	449091.686716	51.291469
3421.547667	448648.081435	51.296474
3420.648261	448219.147032	51.301479
3419.828064	447777.454062	51.306484
3419.504724	447345.672085	51.311489
3418.688299	446904.926345	51.316493
3417.739243	446478.505527	51.321498
3417.302351	446040.373499	51.326503
3416.472624	445604.630165	51.331508
3415.675707	445178.973941	51.336513
3415.147828	444751.237318	51.341517
3414.541076	444312.998770	51.346522
3413.328552	443898.653470	51.351527
3412.782724	443461.760170	51.356532
3412.210073	443041.157071	51.361537
3411.313435	442617.349165	51.366541
3410.787077	442190.835678	51.371546
3410.228992	441776.654976	51.376551
3409.554253	441335.834889	51.381556
3409.018507	440907.117509	51.386561
3407.990458	440491.415544	51.391565
3407.578464	440052.662873	51.396570
3406.382298	439642.455811	51.401575
3405.733546	439210.705979	51.406580
3405.251724	438799.331193	51.411585
3404.108613	438373.940195	51.416589
3404.013926	437954.214731	51.421594
3403.081176	437544.134279	51.426599
3402.549211	437119.564452	51.431604
3401.536876	436712.427689	51.436609
3401.067900	436294.282050	51.441613
3400.027686	435869.949101	51.446618
3399.000389	435450.100584	51.451623
3398.403172	435039.672248	51.456628
3397.610039	434636.377022	51.461633
3396.930761	434237.703560	51.466637
3396.773891	433835.056687	51.471642
3395.492046	433427.731883	51.476647
3394.856269	433022.634335	51.481652
3394.581178	432618.844448	51.486657
3393.516364	432214.817606	51.491661
3393.238942	431806.978193	51.496666
3392.272168	431403.710280	51.501671
3391.714388	430995.597703	51.506676
3391.113331	430586.647603	51.511681
3390.380050	430176.264589	51.516685
3389.935432	429772.558718	51.521690
3388.977790	429366.896239	51.526695
3388.542827	428962.490737	51.531700
3387.636598	428561.810342	51.536705
3386.894969	428151.473176	51.541709
3386.216915	427752.979189	51.546714
3385.649257	427347.249396	51.551719
3385.009468	426947.086553	51.556724
3384.269745	426545.282741	51.561729
3383.824186	426140.531146	51.566733
3383.107483	425722.838347	51.571738
3382.216722	425322.843300	51.576743
3381.516217	424914.151534	51.581748
3380.682519	424515.633986	51.586753
3379.803149	424115.492284	51.591757
3379.311426	423714.318234	51.596762
3378.652751	423315.018839	51.601767
3377.822798	422924.783028	51.606772
3377.160024	422529.181189	51.611777
3376.361426	422136.363790	51.616781
3376.043538	421730.510317	51.621786
3375.069230	421348.428669	51.626791
3374.599280	420944.670618	51.631796
3374.025728	420546.105090	51.636801
3373.073851	420149.041614	51.641805
3372.604298	419743.437122	51.646810
3371.724256	419354.556092	51.651815
3370.818079	418952.794264	51.656820
3370.253615	418568.958567	51.661825
3369.386218	418178.026990	51.666829
3368.826194	417783.052909	51.671834
3368.135091	417404.556401	51.676839
3367.627783	417008.140553	51.681844
3366.858375	416616.130399	51.686849
3366.036248	416230.017379	51.691853
3365.436473	415842.187199	51.696858
3364.670953	415455.699145	51.701863
3364.284226	415063.175401	51.706868
3363.350965	414679.167961	51.711873
3362.726674	414287.408090	51.716877
3362.178605	413903.481946	51.721882
3361.198828	413519.161668	51.726887
3360.499396	413139.467197	51.731892
3360.054833	412750.504080	51.736897
3359.066220	412366.957796	51.741901
3358.755715	411981.037852	51.746906
3357.507753	411597.776696	51.751911
3356.991382	411218.994163	51.756916
3356.185439	410838.219756	51.761921
3355.749168	410463.607706	51.766925
3355.356817	410073.356139	51.771930
3354.162738	409702.107041	51.776935
3353.558229	409320.951170	51.781940
3352.694011	408931.140597	51.786945
3351.970462	408567.858809	51.791949
3351.655329	408188.370979	51.796954
3350.710337	407814.746795	51.801959
3350.199890	407445.395020	51.806964
3349.536073	407066.253351	51.811969
3348.581596	406692.489911	51.816973
3348.124942	406308.045437	51.821978
3347.159531	405945.812793	51.826983
3346.838555	405575.214154	51.831988
3346.251907	405191.106776	51.836993
3345.218551	404832.582528	51.841997
3344.851906	404450.261166	51.847002
3344.225695	404078.066406	51.852007
3343.405430	403699.569226	51.857012
3342.749197	403324.193245	51.862017
3341.843641	402952.918965	51.867021
3341.243959	402574.703864	51.872026
3340.473023	402208.127223	51.877031
3339.787183	401840.973718	51.882036
3339.130967	401468.143047	51.887041
3338.330597	401095.610445	51.892045
3337.633754	400726.819148	51.897050
3336.902397	400363.545047	51.902055
3336.575527	399991.204436	51.907060
3335.582278	399632.767831	51.912065
3334.950283	399269.440359	51.917069
3334.446843	398901.639971	51.922074
3333.701826	398542.033652	51.927079
3332.859072	398166.779624	51.932084
3332.210907	397801.430209	51.937089
3331.510016	397427.467242	51.942093
3330.655804	397062.650686	51.947098
3330.210239	396710.883235	51.952103
3329.620270	396337.678554	51.957108
3328.765160	395979.307539	51.962113
3328.073330	395632.118318	51.967117
3327.663384	395259.279941	51.972122
3326.663038	394895.301858	51.977127
3325.896252	394539.698136	51.982132
3325.470391	394174.553680	51.987137
3324.578122	393813.750322	51.992141
3323.722816	393458.276432	51.997146
3323.233627	393108.817450	52.002151
3322.799253	392746.481242	52.007156
3321.737319	392382.969210	52.012161
3320.970222	392032.958496	52.017165
3320.689789	391665.603236	52.022170
3319.604148	391321.610773	52.027175
3318.811598	390969.101641	52.032180
3318.406339	390620.214551	52.037185
3317.831650	390256.857556	52.042189
3317.200705	389911.736861	52.047194
3316.334536	389563.344455	52.052199
3315.537247	389199.096407	52.057204
3315.146696	388857.029583	52.062209
3314.116160	388504.228366	52.067213
3313.784812	388145.795170	52.072218
3312.863654	387803.649619	52.077223
3311.757240	387452.706344	52.082228
3311.544233	387103.983266	52.087233
3310.706908	386759.373382	52.092237
3310.139389	386405.461237	52.097242
3309.257796	386072.320536	52.102247
3308.433165	385723.045212	52.107252
3307.967113	385383.551334	52.112257
3307.024446	385046.901614	52.117261
3306.791716	384701.540991	52.122266
3305.950508	384357.824661	52.127271
3305.306633	384013.463596	52.132276
3304.937194	383667.301183	52.137281
3303.963094	383326.495530	52.142285
3303.545676	382974.663059	52.147290
3302.969910	382635.848120	52.152295
3302.194009	382276.665098	52.157300
3301.433348	381922.842523	52.162305
3300.908881	381584.696745	52.167309
3300.355490	381236.659111	52.172314
3299.281246	380890.913372	52.177319
3298.897834	380545.741964	52.182324
3298.384196	380193.110556	52.187329
3297.712889	379852.480234	52.192333
3297.071335	379500.905536	52.197338
3295.786738	379157.924433	52.202343
3295.209218	378804.781827	52.207348
3294.898678	378455.409034	52.212353
3294.156777	378121.921944	52.217357
3293.515750	377764.532378	52.222362
3292.907188	377423.057059	52.227367
3292.161980	377079.438377	52.232372
3291.639933	376733.924613	52.237377
3290.879889	376381.832104	52.242381
3290.213109	376022.421514	52.247386
3289.190945	375686.414706	52.252391
3288.867202	375341.290015	52.257396
3288.267954	374990.177384	52.262401
3287.322942	374649.164110	52.267405
3286.762033	374302.541873	52.272410
3285.966026	373965.187752	52.277415
3285.526666	373610.731079	52.282420
3284.730129	373267.876741	52.287425
3283.678819	372928.722969	52.292429
3283.373302	372580.036224	52.297434
3282.499643	372247.895265	52.302439
3282.007336	371909.865840	52.307444
3281.411200	371564.854353	52.312449
3280.544358	371228.099756	52.317453
3279.721015	370877.267530	52.322458
3279.339804	370538.395472	52.327463
3278.436594	370198.636556	52.332468
3277.625897	369861.531518	52.337473
3277.149510	369520.911066	52.342477
3276.734425	369180.303661	52.347482
3276.059882	368845.458771	52.352487
3275.204903	368507.866767	52.357492
3274.659220	368162.311026	52.362497
3273.647339	367814.765533	52.367501
3273.256888	367478.567689	52.372506
3272.487496	367140.875263	52.377511
3271.619922	366800.931446	52.382516
3271.109066	366464.566824	52.387521
3270.467504	366135.420504	52.392525
3269.796136	365794.572916	52.397530
3269.148691	365455.398166	52.402535
3268.277353	365115.518424	52.407540
3267.561519	364769.403412	52.412545
3266.662583	364442.295398	52.417549
3266.335882	364116.977337	52.422554
3265.870015	363769.364894	52.427559
3264.890621	363442.873084	52.432564
3264.511022	363101.043123	52.437569
3263.557186	362774.389866	52.442573
3263.055312	362433.337632	52.447578
3262.303101	362113.339701	52.452583
3261.617048	361773.354992	52.457588
3260.911750	361422.098754	52.462593
3259.878438	361102.189264	52.467597
3259.519486	360773.341431	52.472602
3258.805708	360443.173384	52.477607
3258.093163	360107.353917	52.482612
3257.493373	359779.504241	52.487617
3256.405784	359449.642906	52.492621
3256.313784	359115.016082	52.497626
3255.844023	358794.874764	52.502631
3254.838206	358451.710693	52.507636
3254.479856	358123.251766	52.512641
3253.519830	357787.175402	52.517645
3252.876126	357448.832812	52.522650
3252.433868	357124.324763	52.527655
3251.700003	356796.247184	52.532660
3250.872932	356453.982453	52.537665
3250.193133	356131.821221	52.542669
3249.898394	355794.201046	52.547674
3249.003611	355450.947705	52.552679
3248.329226	355141.452401	52.557684
3247.778863	354792.516061	52.562689
3246.752261	354468.337754	52.567693
3246.087315	354131.299486	52.572698
3245.658506	353806.055382	52.577703
3245.060305	353469.612996	52.582708
3244.117572	353130.219915	52.587713
3243.390926	352806.467249	52.592717
3243.183943	352462.906995	52.597722
3242.420823	352136.941848	52.602727
3241.504212	351800.335477	52.607732
3241.012673	351468.469779	52.612737
3239.913365	351148.430670	52.617741
3239.568128	350816.639569	52.622746
3238.591859	350479.499828	52.627751
3238.066408	350156.717175	52.632756
3237.613841	349817.632563	52.637761
3236.765289	349501.158008	52.642765
3236.069006	349170.023153	52.647770
3235.128297	348837.805106	52.652775
3234.552161	348517.311381	52.657780
3233.701544	348192.634259	52.662785
3233.028020	347868.741680	52.667789
3232.717531	347551.941761	52.672794
3232.053211	347223.589915	52.677799
3231.086013	346898.720101	52.682804
3230.368293	346572.969030	52.687809
3229.618242	346257.682150	52.692813
3229.213551	345932.666923	52.697818
3228.582220	345614.379764	52.702823
3227.488975	345294.204043	52.707828
3227.057929	344969.976585	52.712833
3225.959984	344660.106562	52.717837
3225.576778	344339.202382	52.722842
3225.117799	344024.468154	52.727847
3224.112344	343705.873389	52.732852
3223.974651	343381.234388	52.737857
3223.001242	343070.318147	52.742861
3222.292912	342750.016758	52.747866
3221.403192	342431.065962	52.752871
3220.942596	342108.711095	52.757876
3220.354305	341801.723683	52.762881
3219.595602	341481.983531	52.767885
3219.074173	341162.127808	52.772890
3218.138745	340853.739634	52.777895
3217.610004	340531.081767	52.782900
3217.114457	340207.398769	52.787905
3216.148290	339904.559926	52.792909
3215.748125	339583.531394	52.797914
3214.718133	339271.942984	52.802919
3214.001431	338950.528561	52.807924
3213.548854	338632.507241	52.812929
3212.932554	338323.190653	52.817933
3212.418436	338002.426714	52.822938
3211.432520	337687.896170	52.827943
3210.580976	337374.412000	52.832948
3210.388539	337062.043957	52.837953
3209.417173	336746.971984	52.842957
3208.806422	336425.502786	52.847962
3208.327510	336125.954780	52.852967
3207.632926	335805.208621	52.857972
3206.738322	335500.810411	52.862977
3205.982686	335187.326154	52.867981
3205.613977	334861.661653	52.872986
3205.046123	334557.334784	52.877991
3204.231625	334247.801364	52.882996
3203.612684	333922.375621	52.888001
3202.761370	333615.594582	52.893005
3202.139777	333299.254673	52.898010
3201.599009	332985.497236	52.903015
3200.606532	332674.126521	52.908020
3199.984972	332371.020523	52.913025
3199.316656	332059.824939	52.918029
3198.683972	331746.432949	52.923034
3197.857673	331435.285092	52.928039
3197.255655	331129.752187	52.933044
3196.923521	330821.985859	52.938049
3196.154537	330515.585730	52.943053
3195.658563	330199.059451	52.948058
3195.193773	329882.017698	52.953063
3194.012297	329568.524931	52.958068
3193.400484	329248.194059	52.963073
3192.817394	328951.916227	52.968077
3192.104622	328634.908405	52.973082
3191.297277	328333.648138	52.978087
3190.586056	328022.518637	52.983092
3190.230314	327712.680995	52.988097
3189.469854	327414.286630	52.993101
3188.953326	327096.757657	52.998106
3188.499053	326782.781932	53.003111
3187.545081	326472.626626	53.008116
3187.001385	326159.655500	53.013121
3186.135703	325852.768152	53.018125
3185.651813	325531.281377	53.023130
3185.049020	325230.205928	53.028135
3183.942893	324920.170501	53.033140
3183.684703	324597.065750	53.038145
3182.880737	324299.634088	53.043149
3181.990736	323987.345851	53.048154
3181.505624	323675.323373	53.053159
3180.536192	323367.857485	53.058164
3179.882727	323057.106923	53.063169
3178.844388	322763.780634	53.068173
3178.854196	322447.576053	53.073178
3177.968968	322142.001988	53.078183
3177.650362	321834.707660	53.083188
3176.678535	321524.612970	53.088193
3175.919308	321227.672670	53.093197
3175.612848	320923.454067	53.098202
3174.696821	320616.606440	53.103207
3173.984937	320300.992025	53.108212
3173.538334	319998.880306	53.113217
3172.623068	319687.751760	53.118221
3171.886069	319377.383271	53.123226
3171.114461	319072.111653	53.128231
3170.518668	318779.516908	53.133236
3170.240717	318467.494059	53.138241
3169.437076	318164.057810	53.143245
3168.694241	317862.571579	53.148250
3168.038279	317553.839247	53.153255
3167.158592	317245.701491	53.158260
3166.559662	316940.853956	53.163265
3165.804205	316641.479285	53.168269
3165.395912	316332.525612	53.173274
3164.505022	316029.401971	53.178279
3163.512248	315729.145391	53.183284
3163.431095	315430.220540	53.188289
3162.423543	315134.064085	53.193293
3161.773590	314830.185712	53.198298
3161.276547	314521.265941	53.203303
3160.466478	314228.946049	53.208308
3160.192629	313919.607206	53.213313
3159.097778	313625.726464	53.218317
3158.766327	313323.499332	53.223322
3157.953478	313016.483912	53.228327
3157.269222	312710.338498	53.233332
3156.932406	312412.463953	53.238337
3156.176538	312112.566839	53.243341
3155.247502	311801.084673	53.248346
3154.661822	311509.740383	53.253351
3154.101187	311201.916007	53.258356
3153.193109	310895.953721	53.263361
3152.270944	310598.090504	53.268365
3151.868387	310291.282671	53.273370
3151.712032	309996.505238	53.278375
3150.687954	309680.117602	53.283380
3150.056721	309383.351118	53.288385
3149.371198	309083.001952	53.293389
3148.465951	308770.922070	53.298394
3147.929475	308478.314553	53.303399
3147.135497	308170.620924	53.308404
3146.464000	307863.569228	53.313409
3145.362181	307586.149737	53.318413
3144.868152	307273.440728	53.323418
3144.494226	306983.274049	53.328423
3143.921524	306685.625922	53.333428
3143.378478	306390.391608	53.338433
3142.374638	306092.071826	53.343437
3141.613356	305790.453414	53.348442
3140.726515	305493.514349	53.353447
3140.165088	305204.697551	53.358452
3139.739052	304898.211088	53.363457
3138.798992	304620.708714	53.368461
3138.624158	304316.116576	53.373466
3137.704700	304025.087476	53.378471
3137.162744	303730.152707	53.383476
3136.542190	303440.068260	53.388481
3135.721150	303141.331083	53.393485
3135.162734	302839.164764	53.398490
3134.321265	302551.201679	53.403495
3133.502249	302248.795244	53.408500
3133.165035	301948.527506	53.413505
3132.631054	301657.330773	53.418509
3131.742434	301357.531095	53.423514
3131.066865	301061.236924	53.428519
3130.223030	300768.075695	53.433524
3129.590574	300470.220136	53.438529
3129.420551	300181.102207	53.443533
3128.749335	299884.550470	53.448538
3127.841837	299588.162908	53.453543
3127.001468	299288.529944	53.458548
3126.469900	298987.421450	53.463553
3125.721951	298706.185129	53.468557
3125.102692	298399.741480	53.473562
3124.442815	298107.514119	53.478567
3123.932346	297823.055444	53.483572
3123.144299	297523.716709	53.488577
3122.339579	297233.242560	53.493581
3121.962782	296929.915877	53.498586
3121.078652	296634.818373	53.503591
3120.517190	296349.397710	53.508596
3120.173832	296039.595685	53.513601
3119.008560	295750.831624	53.518605
3118.629939	295449.030868	53.523610
3117.713085	295148.027892	53.528615
3117.114382	294866.685672	53.533620
3116.652673	294560.159833	53.538625
3115.464895	294277.789457	53.543629
3115.147658	293975.773052	53.548634
3114.267221	293692.843913	53.553639
3113.633207	293399.408349	53.558644
3113.247802	293102.876972	53.563649
3112.199908	292819.387449	53.568653
3111.562275	292517.572527	53.573658
3110.935691	292219.219029	53.578663
3110.000787	291937.467788	53.583668
3109.232451	291646.929036	53.588673
3108.711683	291367.480066	53.593677
3108.363900	291072.035249	53.598682
3107.743613	290791.939219	53.603687
3106.588658	290509.839140	53.608692
3106.443564	290213.342545	53.613697
3105.511883	289934.975723	53.618701
3104.869828	289639.932379	53.623706
3104.038569	289350.776231	53.628711
3103.504698	289064.094030	53.633716
3103.081204	288779.915383	53.638721
3102.108909	288498.140869	53.643725
3101.583698	288208.451251	53.648730
3100.919808	287914.351894	53.653735
3100.074938	287628.201403	53.658740
3099.800011	287333.479655	53.663745
3099.052303	287050.929711	53.668749
3098.138748	286759.084505	53.673754
3097.492726	286478.962907	53.678759
3096.735794	286190.224989	53.683764
3096.260460	285908.929866	53.688769
3095.437150	285631.815409	53.693773
3095.078778	285334.838509	53.698778
3094.176165	285052.336952	53.703783
3093.489181	284771.227283	53.708788
3093.014692	284474.166235	53.713793
3092.243072	284196.380417	53.718797
3091.219251	283915.858303	53.723802
3090.746077	283621.241395	53.728807
3089.937153	283336.278924	53.733812
3089.499411	283051.079265	53.738817
3088.753318	282771.251086	53.743821
3088.078014	282485.120903	53.748826
3087.613887	282201.427562	53.753831
3087.004395	281922.850722	53.758836
3086.316268	281632.825480	53.763841
3085.339511	281347.328182	53.768845
3084.712446	281068.269820	53.773850
3084.321864	280781.686239	53.778855
3083.664067	280498.099144	53.783860
3082.694028	280210.664696	53.788865
3081.758509	279942.860737	53.793869
3081.651486	279654.398114	53.798874
3080.461898	279372.219104	53.803879
3079.702188	279108.079956	53.808884
3079.566272	278816.718237	53.813889
3078.691452	278539.633764	53.818893
3078.086143	278259.221150	53.823898
3077.447945	277983.856406	53.828903
3076.823658	277703.191980	53.833908
3076.438506	277414.747267	53.838913
3075.059474	277133.922016	53.843917
3074.636963	276838.377433	53.848922
3074.134900	276546.665650	53.853927
3073.461561	276275.381108	53.858932
3072.714560	275984.497537	53.863937
3072.200243	275707.584729	53.868941
3071.331727	275426.092708	53.873946
3070.589777	275150.922272	53.878951
3069.888125	274875.261550	53.883956
3069.583122	274583.391091	53.888961
3068.519349	274306.972685	53.893965
3068.013225	274034.082547	53.898970
3067.158088	273757.605673	53.903975
3066.487660	273483.875639	53.908980
3066.181584	273206.267708	53.913985
3065.675070	272931.467578	53.918989
3064.631627	272632.506556	53.923994
3063.991168	272363.228866	53.928999
3063.079949	272085.360289	53.934004
3062.629740	271811.060778	53.939009
3061.720268	271540.654255	53.944013
3061.064727	271265.241273	53.949018
3060.632186	270987.526378	53.954023
3059.752035	270721.292210	53.959028
3059.200801	270439.241154	53.964033
3058.673452	270170.837425	53.969037
3057.737742	269894.195730	53.974042
3057.131453	269619.259303	53.979047
3056.372336	269347.556163	53.984052
3055.742022	269062.360006	53.989057
3054.927392	268812.339364	53.994061
3054.577199	268537.311866	53.999066
3053.972880	268259.421318	54.004071
3053.188322	267993.504027	54.009076
3052.548584	267716.943674	54.014081
3051.765593	267449.931242	54.019085
3051.384597	267176.182640	54.024090
3050.648901	266905.011664	54.029095
3049.689381	266636.805093	54.034100
3049.415426	266356.672928	54.039105
3048.626739	266085.714521	54.044109
3048.011291	265812.131099	54.049114
3047.416055	265531.897457	54.054119
3047.044007	265260.389699	54.059124
3046.344578	264986.667264	54.064129
3045.538369	264709.498245	54.069133
3044.634944	264425.748571	54.074138
3043.987059	264150.897940	54.079143
3043.152837	263882.775086	54.084148
3042.925065	263594.513114	54.089153
3041.873005	263317.791486	54.094157
3041.411452	263050.756314	54.099162
3041.020556	262772.529730	54.104167
3040.099354	262496.857691	54.109172
3039.664229	262217.543440	54.114177
3038.864571	261955.758093	54.119181
3038.240710	261674.207537	54.124186
3037.155017	261401.847816	54.129191
3036.537947	261135.882994	54.134196
3036.139928	260855.239751	54.139201
3035.155663	260587.525319	54.144205
3034.284466	260308.689298	54.149210
3033.854555	260036.023300	54.154215
3033.274955	259769.442573	54.159220
3032.527274	259497.718769	54.164225
3031.792754	259223.089844	54.169229
3031.190568	258962.371049	54.174234
3030.751709	258677.432446	54.179239
3029.917955	258418.227973	54.184244
3029.494830	258144.773353	54.189249
3028.647350	257872.328497	54.194253
3027.720163	257609.676077	54.199258
3027.101331	257331.338120	54.204263
3026.334357	257068.737342	54.209268
3025.714890	256802.726350	54.214273
3024.717925	256541.792489	54.219277
3024.379988	256275.508348	54.224282
3023.897427	256003.237131	54.229287
3023.215604	255748.493812	54.234292
3022.489276	255468.494327	54.239297
3022.011246	255202.615681	54.244301
3020.989343	254925.923501	54.249306
3020.605507	254661.736937	54.254311
3019.566597	254393.808863	54.259316
3018.897767	254139.600261	54.264321
3018.599305	253874.076927	54.269325
3017.783887	253610.571267	54.274330
3017.164447	253340.821002	54.279335
3016.544748	253080.926866	54.284340
3016.212037	252804.255903	54.289345
3015.200286	252541.903340	54.294349
3014.611018	252278.796675	54.299354
3013.811722	252006.046250	54.304359
3013.760134	251742.294989	54.309364
3013.235734	251466.038394	54.314369
3012.210246	251193.019414	54.319373
3011.518697	250919.718806	54.324378
3010.895412	250635.049725	54.329383
3009.761424	250382.702615	54.334388
3009.388047	250109.684012	54.339393
3008.791943	249838.076299	54.344397
3008.088147	249570.127780	54.349402
3007.305530	249294.883324	54.354407
3006.389749	249037.308596	54.359412
3005.907825	248760.438549	54.364417
3005.108468	248502.387867	54.369421
3004.600182	248233.315599	54.374426
3004.272025	247969.996108	54.379431
3003.231142	247712.239637	54.384436
3002.787496	247420.901166	54.389441
3002.161627	247166.084935	54.394445
3001.413722	246894.429969	54.399450
3000.478992	246617.100704	54.404455
2999.833732	246356.380845	54.409460
2999.257508	246087.526923	54.414465
2998.455020	245837.452153	54.419469
2998.019097	245567.863961	54.424474
2997.062511	245302.891597	54.429479
2995.914847	245045.640613	54.434484
2995.676874	244776.862986	54.439489
2995.022877	244525.646582	54.444493
2994.125962	244262.347508	54.449498
2993.545110	244003.710031	54.454503
2992.431339	243748.748036	54.459508
2992.310336	243488.103403	54.464513
2991.721300	243238.101480	54.469517
2991.182317	242977.829610	54.474522
2990.505540	242719.566364	54.479527
2989.731507	242449.808780	54.484532
2989.315614	242190.282983	54.489537
2988.356941	241933.008170	54.494541
2987.549501	241673.545421	54.499546
2987.267379	241407.404640	54.504551
2986.293854	241156.270845	54.509556
2985.659630	240890.950868	54.514561
2984.810925	240635.418438	54.519565
2983.881954	240372.285303	54.524570
2983.792981	240117.983348	54.529575
2983.154693	239870.822593	54.534580
2982.570263	239611.405375	54.539585
2981.785815	239354.999744	54.544589
2980.837311	239097.551144	54.549594
2980.139162	238837.109620	54.554599
2979.464028	238580.255520	54.559604
2978.735039	238318.648706	54.564609
2977.911882	238071.139124	54.569613
2977.355053	237832.984210	54.574618
2976.986892	237568.673761	54.579623
2976.400876	237323.063581	54.584628
2975.792221	237060.702228	54.589633
2974.889707	236809.923187	54.594637
2974.175186	236549.769729	54.599642
2973.527276	236293.960669	54.604647
2972.705953	236054.451011	54.609652
2972.442932	235798.531290	54.614657
2971.665294	235550.205425	54.619661
2970.862782	235296.714984	54.624666
2970.505357	235033.198474	54.629671
2969.438697	234780.336773	54.634676
2969.120487	234529.266971	54.639681
2968.398578	234272.175960	54.644685
2967.491261	234011.753805	54.649690
2967.183299	233764.707470	54.654695
2966.366590	233508.830188	54.659700
2966.009729	233250.792801	54.664705
2964.944338	232993.555751	54.669709
2964.215187	232743.701321	54.674714
2963.673094	232482.079544	54.679719
2962.708019	232232.340166	54.684724
2962.190039	231984.618603	54.689729
2961.322034	231738.455388	54.694733
2960.759219	231489.978325	54.699738
2960.037072	231244.684492	54.704743
2959.013387	230997.452961	54.709748
2958.785960	230750.070569	54.714753
2958.303535	230500.819528	54.719757
2957.465798	230249.181030	54.724762
2957.149631	229991.935360	54.729767
2956.237587	229755.841910	54.734772
2955.738647	229496.971532	54.739777
2955.022386	229249.746956	54.744781
2953.987729	228997.786627	54.749786
2953.621265	228749.336808	54.754791
2952.866814	228502.018497	54.759796
2952.184295	228245.294128	54.764801
2951.426274	228000.880419	54.769805
2950.510485	227751.629215	54.774810
2950.215665	227505.564948	54.779815
2949.627946	227265.302024	54.784820
2949.046478	227013.683029	54.789825
2948.339697	226771.072432	54.794829
2947.685908	226514.348644	54.799834
2946.805401	226263.364811	54.804839
2946.009194	226017.002285	54.809844
2945.630204	225759.855372	54.814849
2944.925402	225525.624694	54.819853
2944.001334	225282.072544	54.824858
2943.744423	225020.198343	54.829863
2943.072398	224785.480819	54.834868
2942.400170	224530.280969	54.839873
2941.745538	224275.524691	54.844877
2940.788505	224021.466329	54.849882
2940.582390	223778.428781	54.854887
2939.665987	223538.445076	54.859892
2939.305427	223284.294617	54.864897
2938.446740	223033.126281	54.869901
2937.695008	222776.187847	54.874906
2936.956995	222524.938375	54.879911
2936.328258	222282.672465	54.884916
2935.778878	222032.336726	54.889921
2935.137973	221787.095493	54.894925
2934.247430	221536.357096	54.899930
2933.714340	221275.850118	54.904935
2932.778158	221033.789556	54.909940
2932.559432	220783.430995	54.914945
2931.982025	220535.268625	54.919949
2930.964359	220286.260241	54.924954
2930.323990	220030.802715	54.929959
2929.503444	219800.719040	54.934964
2928.990085	219536.192418	54.939969
2928.194272	219300.785460	54.944973
2927.553594	219050.232185	54.949978
2927.251079	218800.835514	54.954983
2926.197931	218574.153036	54.959988
2925.522801	218315.333690	54.964993
2924.784581	218070.832887	54.969997
2924.002068	217826.034426	54.975002
2923.674845	217575.029279	54.980007
2922.519889	217343.249681	54.985012
2922.265563	217095.213285	54.990017
2921.483794	216856.247931	54.995021
2920.661219	216614.222168	55.000026
2920.223565	216367.375686	55.005031
2919.260652	216135.124137	55.010036
2918.984004	215881.863988	55.015041
2918.487249	215637.002413	55.020045
2917.556885	215405.231845	55.025050
2917.221029	215156.006004	55.030055
2916.176575	214909.999045	55.035060
2915.642791	214667.081539	55.040065
2914.985891	214422.962452	55.045069
2914.097359	214178.257220	55.050074
2913.834851	213935.732154	55.055079
2912.931106	213697.713516	55.060084
2912.077928	213451.757947	55.065089
2911.534415	213210.387365	55.070093
2910.623949	212969.979465	55.075098
2910.410713	212717.077487	55.080103
2909.810758	212481.229820	55.085108
2908.945254	212241.390227	55.090113
2908.287443	211998.718451	55.095117
2907.469461	211744.223139	55.100122
2906.882114	211500.638375	55.105127
2905.895912	211265.429023	55.110132
2905.506073	211025.620436	55.115137
2905.019205	210784.784423	55.120141
2904.143388	210551.813039	55.125146
2903.848530	210306.697346	55.130151
2902.702928	210069.252096	55.135156
2902.123985	209823.686871	55.140161
2901.246404	209580.193576	55.145165
2900.659529	209347.919083	55.150170
2900.474512	209112.781775	55.155175
2899.913879	208879.181211	55.160180
2899.027520	208633.898428	55.165185
2898.463057	208387.216551	55.170189
2897.563878	208141.848662	55.175194
2897.113916	207903.741528	55.180199
2896.565770	207664.479964	55.185204
2895.964922	207408.695108	55.190209
2895.195379	207173.555946	55.195213
2894.296523	206932.151008	55.200218
2894.471447	206679.542710	55.205223
2893.041411	206435.423930	55.210228
2892.231942	206198.449494	55.215233
2891.851358	205947.230387	55.220237
2890.949339	205712.550645	55.225242
2890.417451	205466.346434	55.230247
2889.494419	205226.988508	55.235252
2888.997912	204978.209944	55.240257
2888.296553	204745.029484	55.245261
2887.540137	204515.282110	55.250266
2887.261855	204260.261503	55.255271
2886.488405	204024.842758	55.260276
2885.751778	203777.100010	55.265281
2885.325745	203538.726626	55.270285
2884.250114	203296.970091	55.275290
2884.005036	203052.754173	55.280295
2883.071321	202817.073056	55.285300
2882.331284	202570.125099	55.290305
2881.663616	202330.687856	55.295309
2880.932956	202101.671468	55.300314
2880.423748	201848.899789	55.305319
2879.804703	201615.171840	55.310324
2879.208136	201371.324273	55.315329
2878.549300	201131.763493	55.320333
2877.741657	200897.864806	55.325338
2877.271055	200644.570725	55.330343
2876.378460	200414.696120	55.335348
2876.034295	200163.827548	55.340353
2875.369136	199923.802172	55.345357
2874.504133	199681.747974	55.350362
2874.059760	199432.196624	55.355367
2873.474401	199186.537245	55.360372
2872.458322	198952.349025	55.365377
2872.161621	198709.572921	55.370381
2871.504836	198467.605715	55.375386
2870.722941	198214.932156	55.380391
2869.518261	197972.430418	55.385396
2869.066315	197725.573176	55.390401
2868.678332	197489.497687	55.395405
2867.682731	197248.913065	55.400410
2866.992501	197006.652412	55.405415
2866.656948	196776.170730	55.410420
2865.711372	196537.910072	55.415425
2864.985946	196296.727149	55.420429
2864.227971	196051.338664	55.425434
2863.530836	195818.946159	55.430439
2862.493144	195593.085374	55.435444
2862.214277	195350.423727	55.440449
2861.322688	195123.625709	55.445453
2860.483380	194894.453698	55.450458
2860.202681	194662.763930	55.455463
2859.330938	194435.520473	55.460468
2859.056331	194195.866533	55.465473
2858.122935	193963.812511	55.470477
2857.560946	193735.785146	55.475482
2856.937877	193496.406007	55.480487
2856.111181	193272.736070	55.485492
2855.675097	193039.729612	55.490497
2855.292172	192799.857714	55.495501
2854.163175	192572.663405	55.500506
2854.017227	192332.679891	55.505511
2853.297513	192101.860307	55.510516
2852.367643	191852.575084	55.515521
2851.618748	191618.759632	55.520525
2850.716199	191392.959919	55.525530
2850.512881	191150.497459	55.530535
2849.427850	190929.805391	55.535540
2848.592189	190694.621260	55.540545
2848.471437	190465.597573	55.545549
2847.209673	190243.842418	55.550554
2847.055354	190002.713850	55.555559
2846.352176	189772.729665	55.560564
2845.788484	189545.498088	55.565569
2845.030380	189311.224468	55.570573
2844.277256	189082.638296	55.575578
2844.356343	188840.486233	55.580583
2843.517203	188606.228912	55.585588
2842.868042	188372.515181	55.590593
2842.174223	188127.766517	55.595597
2841.263264	187898.460421	55.600602
2840.474150	187653.296751	55.605607
2839.783202	187414.925270	55.610612
2839.329705	187176.937237	55.615617
2838.542231	186943.163470	55.620621
2837.909297	186704.430212	55.625626
2837.582657	186461.247840	55.630631
2836.722108	186231.178638	55.635636
2836.117268	185992.711768	55.640641
2835.494767	185743.231780	55.645645
2834.554339	185517.109863	55.650650
2833.978622	185272.942748	55.655655
2833.484721	185043.330312	55.660660
2832.585536	184796.927070	55.665665
2831.980406	184556.419562	55.670669
2830.926822	184322.357814	55.675674
2830.553516	184097.667007	55.680679
2829.897402	183863.913617	55.685684
2829.251685	183624.486102	55.690689
2828.658583	183393.485703	55.695693
2827.714593	183168.444684	55.700698
2827.238714	182924.796040	55.705703
2826.509826	182696.199603	55.710708
2825.713905	182457.743500	55.715713
2825.248989	182218.905519	55.720717
2824.235362	181999.949323	55.725722
2824.131619	181762.862974	55.730727
2823.162967	181528.662544	55.735732
2822.251482	181294.734168	55.740737
2821.847004	181067.595851	55.745741
2821.075284	180837.222270	55.750746
2820.481295	180600.715964	55.755751
2819.921585	180363.900232	55.760756
2819.058662	180128.202320	55.765761
2818.474952	179905.728654	55.770765
2817.792986	179683.564263	55.775770
2817.355960	179454.149946	55.780775
2816.484458	179223.927986	55.785780
2815.744222	178993.126801	55.790785
2815.183521	178757.223205	55.795789
2814.621119	178521.384787	55.800794
2813.799445	178283.057516	55.805799
2813.100825	178060.993260	55.810804
2812.702656	177830.653016	55.815809
2811.899192	177600.009351	55.820813
2811.316242	177369.522823	55.825818
2810.848522	177129.378024	55.830823
2810.118783	176895.953736	55.835828
2809.370962	176667.901136	55.840833
2808.738791	176429.554385	55.845837
2808.185368	176204.716927	55.850842
2807.252380	175965.797249	55.855847
2806.538416	175737.464589	55.860852
2805.800629	175494.879105	55.865857
2805.344940	175259.207560	55.870861
2804.381178	175041.144249	55.875866
2804.281489	174805.533401	55.880871
2803.494077	174577.104366	55.885876
2802.476437	174347.542972	55.890881
2801.913139	174111.284608	55.895885
2801.177118	173881.808432	55.900890
2800.700836	173647.790143	55.905895
2799.563088	173425.896698	55.910900
2798.919223	173192.772432	55.915905
2798.300293	172962.786937	55.920909
2797.594092	172744.186486	55.925914
2797.339142	172514.730947	55.930919
2796.315255	172295.979777	55.935924
2795.763743	172060.799907	55.940929
2795.308001	171835.983923	55.945933
2794.516415	171608.945944	55.950938
2794.168615	171382.347686	55.955943
2793.156933	171155.219999	55.960948
2792.578096	170914.264811	55.965953
2792.392101	170693.647515	55.970957
2790.952869	170476.778071	55.975962
2790.665017	170233.008617	55.980967
2789.851228	170006.937206	55.985972
2789.270303	169772.322517	55.990977
2788.612570	169547.093823	55.995981
2787.735532	169323.732408	56.000986
2787.346272	169085.098412	56.005991
2786.460292	168860.825477	56.010996
2785.866960	168634.968780	56.016001
2785.203018	168406.593990	56.021005
2784.454304	168188.979455	56.026010
2784.150889	167954.980414	56.031015
2783.385288	167731.496157	56.036020
2782.726499	167508.555810	56.041025
2781.901949	167276.856110	56.046029
2780.984415	167057.036724	56.051034
2780.580576	166821.025982	56.056039
2780.022064	166604.140642	56.061044
2779.355375	166378.728581	56.066049
2778.711596	166145.672016	56.071053
2778.196546	165919.590182	56.076058
2777.404783	165680.430945	56.081063
2776.922618	165451.104232	56.086068
2775.933324	165236.240524	56.091073
2775.549173	165021.409363	56.096077
2774.816615	164728.447766	56.101082
2774.233133	164473.928567	56.106087
2773.392051	164250.387992	56.111092
2772.614594	164030.513366	56.116097
2772.063066	163800.597526	56.121101
2771.305376	163571.554967	56.126106
2771.014733	163339.044988	56.131111
2770.221301	163126.413080	56.136116
2769.644454	162890.200418	56.141121
2768.813712	162659.229794	56.146125
2768.271250	162432.601502	56.151130
2767.608553	162196.851951	56.156135
2766.773028	161975.040871	56.161140
2766.192153	161738.671056	56.166145
2765.572932	161510.064551	56.171149
2764.878363	161281.102723	56.176154
2764.381980	161048.245882	56.181159
2763.552239	160831.551995	56.186164
2762.836165	160586.743648	56.191169
2761.983437	160360.851382	56.196173
2761.104584	160145.606103	56.201178
2760.951935	159909.828931	56.206183
2760.122180	159687.535276	56.211188
2759.400450	159466.433689	56.216193
2759.033051	159229.474562	56.221197
2758.108201	159009.081825	56.226202
2757.949069	158779.364773	56.231207
2756.929773	158544.153528	56.236212
2756.175294	158314.190564	56.241217
2755.920711	158077.462884	56.246221
2754.809162	157859.992798	56.251226
2753.905283	157619.836873	56.256231
2753.108336	157399.510293	56.261236
2752.449214	157189.956354	56.266241
2752.037080	156961.677022	56.271245
2751.288216	156739.618107	56.276250
2750.871621	156518.105475	56.281255
2750.162277	156288.403028	56.286260
2749.788193	156062.259297	56.291265
2749.069341	155835.650466	56.296269
2748.017004	155609.731563	56.301274
2747.652031	155374.832284	56.306279
2746.835247	155159.468163	56.311284
2746.099812	154930.961170	56.316289
2745.644343	154704.839314	56.321293
2744.758346	154483.007440	56.326298
2744.153027	154261.221542	56.331303
2743.657971	154031.551202	56.336308
2742.960823	153793.512182	56.341313
2742.291950	153565.486902	56.346317
2741.154533	153349.041075	56.351322
2740.663381	153123.545608	56.356327
2739.793265	152901.619948	56.361332
2739.367687	152679.955832	56.366337
2738.810610	152456.216716	56.371341
2738.134442	152241.802300	56.376346
2737.778655	152011.920374	56.381351
2736.764120	151788.029425	56.386356
2736.272211	151570.005755	56.391361
2735.681440	151340.724975	56.396365
2734.797738	151118.686278	56.401370
2734.412107	150894.409427	56.406375
2733.596989	150664.724028	56.411380
2732.854074	150442.032089	56.416385
2732.425178	150225.443591	56.421389
2731.598282	149997.900024	56.426394
2730.999483	149771.389542	56.431399
2730.552701	149540.395416	56.436404
2729.727301	149314.381561	56.441409
2729.151000	149092.803608	56.446413
2728.277568	148864.093352	56.451418
2727.520704	148634.285947	56.456423
2726.956009	148409.609732	56.461428
2726.123811	148198.970359	56.466433
2725.777106	147964.209691	56.471437
2724.862200	147741.766886	56.476442
2723.967499	147520.173928	56.481447
2723.365890	147297.989592	56.486452
2722.853647	147078.169196	56.491457
2722.416378	146854.208099	56.496461
2721.758345	146632.609231	56.501466
2721.013614	146407.136824	56.506471
2720.357123	146181.957045	56.511476
2719.743577	145964.053964	56.516481
2719.184246	145738.239241	56.521485
2718.181137	145521.201550	56.526490
2717.777036	145284.131444	56.531495
2716.919571	145059.677749	56.536500
2716.324289	144838.666098	56.541505
2715.752993	144615.911232	56.546509
2714.790994	144399.535595	56.551514
2714.316028	144167.962196	56.556519
2713.581776	143946.190997	56.561524
2712.927829	143733.583451	56.566529
2712.302609	143501.987981	56.571533
2711.449654	143278.944198	56.576538
2710.775773	143060.079737	56.581543
2710.107334	142841.152428	56.586548
2709.366396	142625.783416	56.591553
2709.222352	142394.145434	56.596557
2708.265395	142180.910399	56.601562
2707.736195	141956.084064	56.606567
2707.029317	141735.048695	56.611572
2706.615909	141514.044670	56.616577
2705.877342	141288.201767	56.621581
2704.863840	141070.116859	56.626586
2704.285556	140845.471658	56.631591
2703.598758	140624.237860	56.636596
2702.881284	140397.915392	56.641601
2702.485810	140173.665506	56.646605
2701.295187	139961.728214	56.651610
2700.822535	139738.700844	56.656615
2700.128315	139533.777766	56.661620
2699.461427	139309.462951	56.666625
2698.933615	139085.750349	56.671629
2698.313906	138875.496338	56.676634
2697.829989	138650.064798	56.681639
2696.904014	138435.949146	56.686644
2696.603838	138206.337226	56.691649
2695.958008	137981.597055	56.696653
2694.796658	137768.806700	56.701658
2694.267320	137546.185803	56.706663
2693.867581	137331.600883	56.711668
2693.171430	137110.178530	56.716673
2692.657634	136893.582105	56.721677
2691.734639	136664.957405	56.726682
2691.148192	136447.765949	56.731687
2690.528011	136227.608630	56.736692
2689.741365	136003.096379	56.741697
2689.215669	135777.515472	56.746701
2688.414552	135565.509725	56.751706
2687.964988	135339.043561	56.756711
2687.279618	135113.925007	56.761716
2686.682816	134889.823164	56.766721
2686.001574	134665.380723	56.771725
2685.070006	134454.864648	56.776730
2684.499620	134231.005072	56.781735
2683.596099	134008.826035	56.786740
2682.706495	133789.466623	56.791745
2682.416182	133566.368130	56.796749
2681.863363	133360.563707	56.801754
2681.137397	133140.421130	56.806759
2680.364821	132917.963001	56.811764
2679.529248	132704.815007	56.816769
2678.863643	132481.276289	56.821773
2678.088507	132274.041378	56.826778
2677.764834	132053.093976	56.831783
2676.909342	131836.830806	56.836788
2676.238752	131619.612720	56.841793
2676.186534	131406.794901	56.846797
2675.205354	131196.120085	56.851802
2674.557503	130970.875638	56.856807
2673.853456	130752.183367	56.861812
2673.074630	130533.618953	56.866817
2672.704801	130314.724700	56.871821
2671.802936	130102.762607	56.876826
2671.264533	129874.575507	56.881831
2670.962159	129650.950776	56.886836
2669.948795	129432.520996	56.891841
2669.329401	129206.968634	56.896845
2668.560041	129001.776322	56.901850
2667.770844	128778.235701	56.906855
2667.702736	128553.045819	56.911860
2666.766684	128338.244822	56.916865
2665.950637	128108.249132	56.921869
2664.915739	127893.594248	56.926874
2664.659574	127669.152567	56.931879
2664.118633	127458.702867	56.936884
2662.862467	127232.264105	56.941889
2662.316272	127009.042172	56.946893
2661.769351	126810.815959	56.951898
2661.083432	126576.735686	56.956903
2660.443899	126372.977411	56.961908
2659.742331	126155.705188	56.966913
2659.229699	125938.239661	56.971917
2658.497940	125729.001827	56.976922
2657.936310	125507.826509	56.981927
2657.095003	125296.717126	56.986932
2656.226710	125076.838441	56.991937
2655.932501	124854.127553	56.996941
2655.024084	124646.018175	57.001946
2654.603676	124436.601273	57.006951
2653.684520	124222.147360	57.011956
2653.232817	124005.462292	57.016961
2652.554293	123784.154482	57.021965
2651.717162	123579.356395	57.026970
2650.848187	123368.749002	57.031975
2650.546850	123151.208890	57.036980
2649.467883	122933.133442	57.041985
2649.240119	122721.058129	57.046989
2648.434625	122510.485523	57.051994
2647.638235	122305.614535	57.056999
2647.204889	122095.735422	57.062004
2646.303827	121879.735549	57.067009
2645.930359	121660.238162	57.072013
2644.443208	121462.847773	57.077018
2644.382336	121248.129351	57.082023
2643.983431	121039.522882	57.087028
2643.274583	120824.021754	57.092033
2642.678900	120611.196257	57.097037
2641.853921	120400.046734	57.102042
2641.286724	120181.163694	57.107047
2640.748730	119967.699412	57.112052
2640.017772	119753.670693	57.117057
2639.144496	119538.409304	57.122061
2638.316785	119330.182708	57.127066
2637.791896	119119.516507	57.132071
2637.141093	118900.993871	57.137076
2636.297463	118691.765533	57.142081
2636.091561	118485.599171	57.147085
2635.247081	118267.614039	57.152090
2634.694653	118065.384560	57.157095
2633.825816	117851.006091	57.162100
2633.345777	117630.880105	57.167105
2632.952609	117419.311775	57.172109
2631.815061	117209.170765	57.177114
2631.478643	116997.114476	57.182119
2630.622692	116780.851238	57.187124
2629.702480	116568.307003	57.192129
2629.286480	116356.782761	57.197133
2628.400429	116144.668258	57.202138
2627.824498	115935.362724	57.207143
2627.063376	115729.458715	57.212148
2626.377965	115515.705401	57.217153
2626.193147	115298.377203	57.222157
2625.070771	115099.923765	57.227162
2624.400784	114893.618542	57.232167
2624.171305	114667.911827	57.237172
2623.170877	114462.595497	57.242177
2622.532340	114244.485006	57.247181
2621.987537	114042.121076	57.252186
2621.478853	113832.803163	57.257191
2620.377286	113617.348309	57.262196
2619.965824	113418.497111	57.267201
2619.453405	113185.314802	57.272205
2618.400170	112987.165304	57.277210
2617.827382	112788.268497	57.282215
2617.364028	112571.268102	57.287220
2616.587690	112365.279674	57.292225
2616.284750	112149.095267	57.297229
2615.384845	111938.649312	57.302234
2614.852198	111727.353641	57.307239
2614.277943	111520.026469	57.312244
2613.434349	111307.876108	57.317249
2612.869429	111092.072397	57.322253
2611.960835	110882.893311	57.327258
2611.680414	110668.438020	57.332263
2610.782272	110447.209687	57.337268
2610.280046	110235.737870	57.342273
2609.378398	110020.466473	57.347277
2608.763076	109813.191838	57.352282
2607.878928	109598.448070	57.357287
2607.378185	109395.435899	57.362292
2606.596301	109177.221155	57.367297
2606.189560	108961.880612	57.372301
2605.157291	108756.667171	57.377306
2604.469413	108546.870143	57.382311
2603.975492	108351.772129	57.387316
2603.180555	108133.264191	57.392321
2602.983457	107930.235108	57.397325
2601.860210	107727.798655	57.402330
2601.221685	107515.528004	57.407335
2600.580680	107310.163232	57.412340
2599.521337	107110.856357	57.417345
2599.118287	106900.654040	57.422349
2598.737889	106697.607217	57.427354
2597.784692	106489.576844	57.432359
2597.321874	106282.593620	57.437364
2596.325457	106077.225860	57.442369
2595.833378	105870.599788	57.447373
2595.064293	105671.455513	57.452378
2594.534062	105465.460766	57.457383
2594.117288	105261.632390	57.462388
2592.979398	105063.293946	57.467393
2592.884530	104848.054808	57.472397
2591.978174	104648.306343	57.477402
2591.447103	104440.467955	57.482407
2590.595061	104235.105820	57.487412
2589.796298	104030.714050	57.492417
2589.562517	103814.827412	57.497421
2588.731046	103616.649140	57.502426
2588.109053	103408.358371	57.507431
2587.480871	103200.654079	57.512436
2586.668252	102999.699246	57.517441
2586.176326	102781.604437	57.522445
2585.129752	102578.869524	57.527450
2584.594041	102378.745229	57.532455
2584.291952	102174.011674	57.537460
2583.205837	101975.919260	57.542465
2582.554626	101764.824646	57.547469
2581.977621	101561.941629	57.552474
2581.081120	101354.308850	57.557479
2580.537979	101152.280413	57.562484
2579.985374	100955.799488	57.567489
2579.401143	100750.063722	57.572493
2578.750533	100545.006355	57.577498
2578.219097	100330.917960	57.582503
2577.582959	100132.845998	57.587508
2576.880048	99931.652730	57.592513
2576.202297	99719.990915	57.597517
2575.492256	99520.819487	57.602522
2574.725484	99305.826379	57.607527
2574.250621	99100.925195	57.612532
2573.333307	98901.049823	57.617537
2572.665359	98701.587015	57.622541
2572.063469	98488.744679	57.627546
2571.538006	98293.303243	57.632551
2570.756824	98088.878237	57.637556
2569.989293	97881.370333	57.642561
2569.625305	97678.772996	57.647565
2568.706278	97486.578478	57.652570
2568.060411	97269.409750	57.657575
2567.783699	97060.239534	57.662580
2566.711672	96858.009041	57.667585
2566.164838	96656.667494	57.672589
2565.587627	96459.892667	57.677594
2565.207480	96257.304172	57.682599
2564.307173	96046.225266	57.687604
2563.459596	95846.987089	57.692609
2562.758420	95640.167697	57.697613
2561.989057	95438.035077	57.702618
2560.949579	95236.828609	57.707623
2560.647347	95033.065458	57.712628
2559.682041	94840.742135	57.717633
2559.479004	94637.461505	57.722637
2558.537051	94436.785781	57.727642
2558.165036	94242.020764	57.732647
2557.422464	94041.437468	57.737652
2556.776888	93842.781118	57.742657
2555.991590	93636.589580	57.747661
2555.529142	93444.426828	57.752666
2554.603554	93245.388942	57.757671
2554.135445	93037.313658	57.762676
2553.575541	92841.430146	57.767681
2552.787059	92631.304118	57.772685
2551.958581	92435.929651	57.777690
2551.209859	92245.984948	57.782695
2551.028503	92041.925507	57.787700
2549.881785	91841.920661	57.792705
2549.236709	91636.296128	57.797709
2548.427259	91444.795364	57.802714
2548.201077	91243.337475	57.807719
2547.196979	91040.229295	57.812724
2546.579910	90856.267701	57.817729
2546.009093	90645.574390	57.822733
2545.356435	90455.870800	57.827738
2544.524449	90259.615773	57.832743
2543.875989	90067.334269	57.837748
2543.200906	89867.659376	57.842753
2543.063877	89671.844745	57.847757
2542.065842	89474.069678	57.852762
2541.035083	89274.380488	57.857767
2540.751092	89076.375389	57.862772
2540.172640	88880.441266	57.867777
2539.558647	88684.971026	57.872781
2538.635772	88489.564177	57.877786
2538.044483	88290.486401	57.882791
2537.758113	88094.215090	57.887796
2536.758074	87908.341934	57.892801
2536.571008	87697.286581	57.897805
2535.661167	87498.501141	57.902810
2534.872684	87307.420042	57.907815
2534.652714	87100.376078	57.912820
2533.631687	86896.725943	57.917825
2533.054951	86694.484424	57.922829
2532.420313	86490.789568	57.927834
2531.564786	86297.065486	57.932839
2530.993425	86092.977668	57.937844
2530.258552	85893.577078	57.942849
2529.855354	85692.845252	57.947853
2529.044721	85500.845517	57.952858
2528.540047	85303.138194	57.957863
2527.701116	85091.850396	57.962868
2526.945385	84892.684312	57.967873
2526.342220	84694.744676	57.972877
2525.565734	84493.126117	57.977882
2524.903880	84302.476448	57.982887
2524.113965	84094.841930	57.987892
2523.381306	83899.066385	57.992897
2523.041253	83697.538335	57.997901
2522.153896	83512.585563	58.002906
2521.712532	83316.350889	58.007911
2521.119338	83119.051889	58.012916
2520.362575	82914.611936	58.017921
2520.049480	82705.540046	58.022925
2518.924395	82518.453282	58.027930
2518.350105	82313.888825	58.032935
2517.791261	82114.812747	58.037940
2516.734443	81916.641437	58.042945
2516.336351	81719.565480	58.047949
2515.488308	81528.507711	58.052954
2514.860979	81329.602055	58.057959
2514.315418	81138.690039	58.062964
2513.782919	80941.180052	58.067969
2513.240814	80741.271455	58.072973
2512.641361	80539.085964	58.077978
2511.818449	80339.510925	58.082983
2511.154593	80143.233468	58.087988
2510.339106	79946.240412	58.092993
2509.868341	79738.116757	58.097997
2509.256311	79542.457833	58.103002
2508.094681	79343.712880	58.108007
2507.617069	79157.282425	58.113012
2506.947475	78966.600138	58.118017
2506.124088	78765.924983	58.123021
2505.721585	78565.552616	58.128026
2504.864099	78370.716816	58.133031
2504.283931	78170.782019	58.138036
2503.317517	77990.928622	58.143041
2502.942526	77789.076620	58.148045
2502.348857	77605.219674	58.153050
2501.484560	77405.045876	58.158055
2501.261212	77203.264315	58.163060
2500.477437	77021.755615	58.168065
2499.589304	76821.299822	58.173069
2498.921335	76627.603795	58.178074
2498.562475	76432.105424	58.183079
2497.953031	76228.233977	58.188084
2496.836161	76047.870257	58.193089
2496.259264	75834.886007	58.198093
2495.510239	75647.871520	58.203098
2494.918723	75458.932958	58.208103
2494.218055	75260.826190	58.213108
2493.811104	75079.199053	58.218113
2492.907328	74874.899979	58.223117
2492.319076	74681.038808	58.228122
2491.464242	74500.552288	58.233127
2490.876553	74295.803476	58.238132
2489.971127	74105.970617	58.243137
2489.475267	73912.159211	58.248141
2489.046515	73731.574026	58.253146
2488.170036	73537.459100	58.258151
2487.699456	73345.543465	58.263156
2486.993782	73154.465188	58.268161
2486.477680	72967.489315	58.273165
2485.903338	72775.836322	58.278170
2485.266748	72572.398888	58.283175
2484.803579	72378.692145	58.288180
2483.904032	72190.701008	58.293185
2483.008996	71991.491613	58.298189
2482.731395	71791.628861	58.303194
2481.964191	71601.538105	58.308199
2481.551417	71413.116058	58.313204
2480.394305	71218.631052	58.318209
2479.827628	71017.928698	58.323213
2479.371167	70823.513872	58.328218
2478.586516	70625.364899	58.333223
2478.414563	70426.170608	58.338228
2477.427597	70236.989266	58.343233
2476.666425	70032.793107	58.348237
2475.821138	69836.143908	58.353242
2475.213329	69644.437758	58.358247
2474.775326	69448.456306	58.363252
2473.752374	69266.764343	58.368257
2473.252254	69053.162429	58.373261
2472.537990	68867.713458	58.378266
2471.639504	68680.148231	58.383271
2471.395877	68470.299708	58.388276
2470.431730	68292.464788	58.393281
2469.923256	68098.452478	58.398285
2469.546568	67906.283310	58.403290
2468.809130	67712.038784	58.408295
2467.934039	67512.301467	58.413300
2467.051234	67316.101521	58.418305
2466.693117	67122.176421	58.423309
2465.976654	66932.591430	58.428314
2464.942612	66745.224630	58.433319
2464.965522	66546.501211	58.438324
2463.942735	66356.533411	58.443329
2463.469994	66163.671533	58.448333
2462.679701	65979.896047	58.453338
2462.122552	65779.970995	58.458343
2461.331721	65581.332647	58.463348
2460.466161	65391.726215	58.468353
2460.201113	65189.275319	58.473357
2459.334361	65002.117376	58.478362
2458.920484	64810.491406	58.483367
2458.202753	64609.096774	58.488372
2457.434842	64422.853366	58.493377
2456.469892	64223.819686	58.498381
2455.710290	64026.259473	58.503386
2454.975290	63841.020191	58.508391
2454.392989	63653.532688	58.513396
2453.878665	63461.603674	58.518401
2453.465244	63270.578757	58.523405
2452.728533	63079.166921	58.528410
2451.826723	62893.744812	58.533415
2451.806796	62695.292762	58.538420
2450.709715	62505.093081	58.543425
2450.044555	62313.886550	58.548429
2449.431547	62124.009685	58.553434
2448.723503	61926.238280	58.558439
2448.399424	61731.061037	58.563444
2447.088886	61552.384073	58.568449
2447.004135	61351.107121	58.573453
2446.150378	61161.990364	58.578458
2445.226130	60960.435947	58.583463
2444.640421	60758.111406	58.588468
2443.900104	60582.297301	58.593473
2443.344150	60390.760502	58.598477
2442.791328	60203.270765	58.603482
2442.189948	60015.296771	58.608487
2441.743880	59814.188470	58.613492
2440.434069	59634.526116	58.618497
2440.383310	59436.993163	58.623501
2439.758522	59248.733007	58.628506
2438.683028	59051.107016	58.633511
2438.290709	58855.194883	58.638516
2437.326715	58670.029903	58.643521
2436.733117	58475.961057	58.648525
2436.167764	58286.172342	58.653530
2435.420706	58093.046571	58.658535
2435.013381	57899.808803	58.663540
2433.911297	57713.041990	58.668545
2433.649400	57514.103717	58.673549
2432.695502	57323.743902	58.678554
2432.034070	57144.632610	58.683559
2431.471304	56946.571037	58.688564
2430.967386	56761.016642	58.693569
2430.309127	56563.936462	58.698573
2429.426410	56378.104148	58.703578
2428.843124	56189.191096	58.708583
2428.393851	55996.796369	58.713588
2427.529651	55807.406397	58.718593
2426.904629	55615.223913	58.723597
2426.158931	55418.252124	58.728602
2425.350487	55229.128271	58.733607
2425.097495	55035.563676	58.738612
2424.299219	54851.755630	58.743617
2423.644360	54658.372656	58.748621
2423.132950	54460.383473	58.753626
2422.275701	54268.682295	58.758631
2421.831325	54075.816410	58.763636
2420.847485	53888.933555	58.768641
2419.967256	53693.799077	58.773645
2419.962939	53503.755462	58.778650
2418.786283	53312.855443	58.783655
2418.536673	53116.079779	58.788660
2417.700989	52923.762777	58.793665
2416.826023	52740.772907	58.798669
2416.258652	52554.834479	58.803674
2415.455685	52360.034312	58.808679
2415.038583	52157.894236	58.813684
2414.239862	51978.636892	58.818689
2413.474165	51791.392972	58.823693
2413.203461	51601.503260	58.828698
2412.262627	51411.066829	58.833703
2411.848934	51217.587293	58.838708
2411.088118	51035.523640	58.843713
2410.478230	50838.757073	58.848717
2409.910998	50640.112846	58.853722
2409.148406	50450.094940	58.858727
2408.447184	50251.178849	58.863732
2407.692768	50070.120575	58.868737
2406.959354	49875.446965	58.873741
2406.312934	49675.715472	58.878746
2405.578126	49483.166070	58.883751
2405.036389	49298.013326	58.888756
2404.354578	49113.020746	58.893761
2403.529132	48924.806971	58.898765
2402.975209	48745.584207	58.903770
2402.080064	48553.816860	58.908775
2401.570227	48359.257195	58.913780
2400.953555	48172.226739	58.918785
2400.377802	47984.691936	58.923789
2399.977876	47796.783256	58.928794
2398.868639	47604.433737	58.933799
2398.208499	47420.546691	58.938804
2397.401093	47237.694005	58.943809
2396.769309	47047.245592	58.948813
2396.196915	46862.812666	58.953818
2395.503167	46671.524043	58.958823
2394.955948	46482.836549	58.963828
2393.997055	46306.821552	58.968833
2393.127737	46126.223386	58.973837
2392.779401	45943.633954	58.978842
2391.975869	45756.854776	58.983847
2391.564140	45574.333000	58.988852
2390.949035	45395.055811	58.993857
2390.549314	45216.306148	58.998861
2389.771557	45023.122514	59.003866
2388.899142	44837.856941	59.008871
2388.270482	44645.890521	59.013876
2387.318516	44458.838742	59.018881
2386.842182	44279.503523	59.023885
2386.543717	44097.298615	59.028890
2385.489352	43917.366121	59.033895
2385.040839	43722.866906	59.038900
2384.184825	43547.938632	59.043905
2383.775037	43360.645040	59.048909
2383.091600	43178.950379	59.053914
2382.369135	42998.680635	59.058919
2381.609746	42809.120768	59.063924
2380.732067	42633.183639	59.068929
2380.146589	42453.024344	59.073933
2379.743704	42262.825703	59.078938
2379.041175	42085.003696	59.083943
2378.459592	41895.820929	59.088948
2377.804978	41721.318713	59.093953
2377.146863	41527.661598	59.098957
2376.658409	41344.807348	59.103962
2375.670977	41159.577102	59.108967
2375.111873	40958.947444	59.113972
2374.470795	40786.549077	59.118977
2373.752881	40597.588739	59.123981
2373.315588	40408.753573	59.128986
2372.485629	40219.578003	59.133991
2371.717228	40034.995503	59.138996
2371.213284	39853.070235	59.144001
2370.583137	39669.162230	59.149005
2369.675262	39482.027649	59.154010
2369.049693	39303.115530	59.159015
2368.573993	39116.678436	59.164020
2367.710737	38927.825964	59.169025
2366.877090	38747.436570	59.174029
2366.515132	38560.546448	59.179034
2365.542453	38388.224821	59.184039
2364.986952	38196.019761	59.189044
2364.796076	38017.757258	59.194049
2364.036922	37828.657026	59.199053
2363.484972	37637.983193	59.204058
2362.643402	37459.613161	59.209063
2362.083834	37266.695270	59.214068
2361.271369	37079.994040	59.219073
2360.773818	36899.749602	59.224077
2359.880075	36716.413242	59.229082
2358.999778	36528.394747	59.234087
2358.768385	36335.651992	59.239092
2357.763238	36159.313261	59.244097
2357.464838	35966.493672	59.249101
2356.882219	35781.573860	59.254106
2356.178558	35593.148957	59.259111
2355.601057	35405.504355	59.264116
2354.679247	35219.598165	59.269121
2354.143481	35032.703458	59.274125
2353.612600	34844.684722	59.279130
2352.621866	34664.139388	59.284135
2352.353325	34468.126985	59.289140
2351.409977	34284.164372	59.294145
2350.776397	34095.602944	59.299149
2350.153366	33908.627152	59.304154
2349.293829	33717.494939	59.309159
2348.680011	33530.996045	59.314164
2348.043753	33341.501643	59.319169
2347.193959	33153.819593	59.324173
2346.573621	32980.354883	59.329178
2345.749783	32802.907040	59.334183
2345.182582	32612.913763	59.339188
2344.493512	32440.753546	59.344193
2343.646023	32255.265260	59.349197
2343.335525	32075.204282	59.354202
2342.288811	31898.713271	59.359207
2342.035605	31707.109816	59.364212
2341.154521	31537.432476	59.369217
2340.460746	31349.235706	59.374221
2340.214210	31166.974838	59.379226
2339.088980	30985.323052	59.384231
2338.697427	30792.639711	59.389236
2337.690639	30621.566439	59.394241
2337.168848	30443.106866	59.399245
2336.622204	30264.052735	59.404250
2335.543965	30086.508503	59.409255
2335.208954	29902.867811	59.414260
2334.395545	29727.933639	59.419265
2333.978735	29554.107658	59.424269
2333.427630	29374.940694	59.429274
2332.528246	29185.434592	59.434279
2332.597050	29001.378144	59.439284
2331.645517	28829.442663	59.444289
2330.845492	28643.676317	59.449293
2330.242564	28454.637258	59.454298
2329.614632	28275.897404	59.459303
2328.751628	28085.244977	59.464308
2328.115783	27908.475783	59.469313
2327.405226	27716.991443	59.474317
2327.009008	27540.854939	59.479322
2326.258297	27363.819194	59.484327
2325.545596	27166.196218	59.489332
2324.446101	26987.156686	59.494337
2323.801020	26812.505148	59.499341
2323.515367	26621.865229	59.504346
2322.452427	26455.189623	59.509351
2321.838654	26275.758669	59.514356
2321.294226	26098.486043	59.519361
2320.778361	25921.206093	59.524365
2319.949934	25745.359857	59.529370
2319.389745	25561.886005	59.534375
2318.494911	25376.319032	59.539380
2317.909403	25203.003912	59.544385
2316.988412	25033.259228	59.549389
2316.444074	24843.976596	59.554394
2315.850655	24678.275578	59.559399
2315.118323	24491.691613	59.564404
2314.701929	24315.477393	59.569409
2313.899440	24152.440905	59.574413
2313.445585	23970.921405	59.579418
2312.590777	23795.629823	59.584423
2312.032308	23616.507236	59.589428
2311.182683	23452.815669	59.594433
2310.319855	23272.773856	59.599437
2309.989405	23109.321726	59.604442
2309.412711	22925.231532	59.609447
2308.338324	22755.405829	59.614452
2307.935940	22573.054625	59.619457
2307.071410	22403.779800	59.624461
2306.772107	22215.723668	59.629466
2305.867106	22057.000037	59.634471
2305.202791	21876.550080	59.639476
2304.801202	21718.092702	59.644481
2303.974923	21525.381076	59.649485
2303.336207	21350.048990	59.654490
2302.798661	21181.305448	59.659495
2302.399919	21004.127789	59.664500
2301.484573	20830.412675	59.669505
2300.581990	20649.907101	59.674509
2300.149623	20473.537404	59.679514
2299.429307	20299.000535	59.684519
2298.820308	20121.315804	59.689524
2297.995208	19943.812626	59.694529
2297.327107	19775.443925	59.699533
2296.822663	19600.475136	59.704538
2295.932845	19425.135182	59.709543
2295.016158	19249.142604	59.714548
2294.243303	19083.422247	59.719553
2293.718718	18910.154260	59.724557
2293.017607	18736.673815	59.729562
2292.354899	18585.254913	59.734567
2291.853192	18408.683326	59.739572
2291.110295	18244.621805	59.744577
2290.488223	18071.770916	59.749581
2289.897426	17897.927025	59.754586
2289.002912	17731.665963	59.759591
2288.593846	17560.187005	59.764596
2287.848256	17403.373337	59.769601
2287.090337	17230.142428	59.774605
2286.902747	17055.966498	59.779610
2285.732277	16893.507378	59.784615
2285.606484	16726.627549	59.789620
2285.060498	16550.750649	59.794625
2283.797055	16382.506803	59.799629
2283.273731	16203.020900	59.804634
2282.418317	16042.787338	59.809639
2282.233172	15863.043742	59.814644
2281.543291	15689.584599	59.819649
2280.925884	15525.420364	59.824653
2280.374157	15350.756964	59.829658
2279.536833	15191.982260	59.834663
2278.628769	15003.126739	59.839668
2277.932397	14842.671326	59.844673
2277.183111	14676.521997	59.849677
2276.464056	14510.958259	59.854682
2276.121710	14341.263005	59.859687
2275.387863	14169.917175	59.864692
2274.512900	14016.203354	59.869697
2273.683595	13840.956971	59.874701
2273.360430	13679.820045	59.879706
2272.414317	13508.575264	59.884711
2272.062040	13338.279736	59.889716
2271.176407	13175.699158	59.894721
2270.626469	13004.668333	59.899725
2269.934931	12838.846089	59.904730
2269.018350	12675.547987	59.909735
2268.586637	12506.541715	59.914740
2268.055018	12346.634334	59.919745
2266.789126	12177.365787	59.924750
2266.625709	12021.791349	59.929754
2265.698698	11859.921236	59.934759
2265.256252	11702.810528	59.939764
2264.590897	11536.225833	59.944769
2263.721918	11369.809801	59.949774
2263.210196	11210.504294	59.954778
2262.354968	11052.098671	59.959783
2261.978565	10889.582422	59.964788
2261.164157	10737.657853	59.969793
2260.511363	10570.880338	59.974798
2260.071158	10406.020687	59.979802
2258.874955	10249.742478	59.984807
2258.390602	10079.085627	59.989812
2257.857715	9925.565020	59.994817
2257.311368	9762.985628	59.999822
2256.701799	9600.316427	60.004826
2255.578027	9436.498906	60.009831
2254.972578	9273.867285	60.014836
2254.325981	9114.678397	60.019841
2253.484311	8957.765192	60.024846
2252.967719	8800.273056	60.029850
2252.034766	8658.851893	60.034855
2251.396682	8509.976224	60.039860
2250.938284	8349.555318	60.044865
2250.060542	8198.454504	60.049870
2249.824193	8033.114289	60.054874
2248.532332	7895.968933	60.059879
2248.239248	7742.649882	60.064884
2247.536548	7583.924342	60.069889
2246.742636	7439.953519	60.074894
2246.369814	7292.153494	60.079898
2245.346065	7144.252280	60.084903
2244.782830	6991.690604	60.089908
2244.271304	6835.985753	60.094913
2243.595724	6682.578877	60.099918
2242.716677	6537.925401	60.104922
2241.857745	6392.884787	60.109927
2241.654913	6235.072049	60.114932
2240.505059	6102.217412	60.119937
2239.785360	5955.534776	60.124942
2239.348950	5801.977546	60.129946
2238.455575	5664.044850	60.134951
2237.885659	5516.019175	60.139956
2237.396079	5377.241026	60.144961
2236.244447	5228.343437	60.149966
2235.302707	5082.892537	60.154970
2234.058862	4956.567278	60.159975
2233.665356	4820.124890	60.164980
2233.127017	4698.230018	60.169985
2232.166136	4574.925856	60.174990
2231.649847	4449.710491	60.179994
2230.690521	4321.560604	60.184999
2229.871786	4201.587541	60.190004
2229.157578	4086.159247	60.195009
2228.608921	3970.531289	60.200014
2228.258729	3851.198955	60.205018
2227.035305	3737.273049	60.210023
2226.490397	3609.088057	60.215028
2225.621673	3510.388597	60.220033
2224.958839	3400.490960	60.225038
2224.512234	3291.920311	60.230042
2223.366635	3176.043101	60.235047
2222.746673	3072.006462	60.240052
2221.937586	2973.210449	60.245057
2221.419233	2859.336437	60.250062
2220.978444	2755.131659	60.255066
2219.528836	2666.988277	60.260071
2219.364032	2551.253785	60.265076
2218.737493	2466.611930	60.270081
2217.794520	2367.718201	60.275086
2217.515106	2263.996030	60.280090
2216.607338	2170.041134	60.285095
2215.869001	2068.736125	60.290100
2215.130210	1968.125863	60.295105
2214.442735	1871.214575	60.300110
2214.129113	1770.470404	60.305114
2213.113675	1681.810639	60.310119
2212.358846	1579.836596	60.315124
2211.916199	1486.644261	60.320129
2210.918566	1409.249776	60.325134
2210.279145	1314.118316	60.330138
2209.371882	1235.138797	60.335143
2209.019503	1148.030712	60.340148
2208.275583	1065.276589	60.345153
2207.367380	976.465310	60.350158
2206.777608	892.590047	60.355162
2205.905518	812.977974	60.360167
2205.057722	729.769896	60.365172
2204.453284	655.601306	60.370177
2203.464550	584.856355	60.375182
2202.745983	505.708921	60.380186
2202.370620	439.046571	60.385191
2201.315167	364.170375	60.390196
2200.340232	308.887459	60.395201
2199.270909	243.148269	60.400206
2198.835026	184.255660	60.405210
2197.375522	140.918914	60.410215
2197.031702	97.274414	60.415220
2196.184928	43.924516	60.420225
2195.059760	13.988546	60.425230
2194.436190	-26.737116	60.430234
2193.529975	-53.268250	60.435239
2193.313446	-95.572994	60.440244
2192.387494	-121.630929	60.445249
2191.575938	-149.996745	60.450254
2191.040302	-184.242681	60.455258
2189.953871	-196.388129	60.460263
2188.375002	-217.207665	60.465268
2180.180486	-18.891527	60.470273
2178.865820	48.067542	60.475278
2181.010925	71.081094	60.480282
2182.647600	95.936865	60.485287
2184.220446	98.518056	60.490292
2185.071818	103.114004	60.495297
2185.193827	89.710545	60.500302
2185.107973	56.137039	60.505306
2183.812698	37.904170	60.510311
2183.430885	32.459405	60.515316
2182.287556	13.904409	60.520321
2180.760912	14.922472	60.525326
2180.111077	14.088809	60.530330
2179.174438	14.999078	60.535335
2178.368689	11.143386	60.540340
2178.217568	17.592046	60.545345
2177.463886	10.641902	60.550350
2176.697040	13.622645	60.555354
2176.002807	20.583260	60.560359
2175.122455	7.651935	60.565364
2174.385566	14.741533	60.570369
2173.610725	24.850018	60.575374
2173.515684	21.493448	60.580378
2172.872249	19.780382	60.585383
2172.175459	26.883336	60.590388
2172.422453	21.386129	60.595393
2171.091289	27.637218	60.600398
2170.468632	16.378418	60.605402
2169.245701	32.154776	60.610407
2168.896416	19.445917	60.615412
2168.142043	21.131544	60.620417
2167.473707	37.767700	60.625422
2167.211650	30.061442	60.630426
2166.531685	26.117982	60.635431
2166.216476	29.429214	60.640436
2165.841976	25.500372	60.645441
2164.577164	35.271849	60.650446
2163.974108	26.298166	60.655450
2162.522763	36.892470	60.660455
2162.088322	41.127822	60.665460
2161.903761	40.649290	60.670465
2160.876459	35.685419	60.675470
2160.724154	40.196140	60.680474
2160.042537	45.063661	60.685479
2159.291624	31.554315	60.690484
2158.745085	39.690033	60.695489
2158.169052	39.283072	60.700494
2158.122441	36.462883	60.705498
2157.325826	35.225144	60.710503
2156.430081	37.646011	60.715508
2155.539026	37.353688	60.720513
2154.191287	47.029520	60.725518
2153.709109	37.836375	60.730522
2153.052229	54.745132	60.735527
2152.845294	44.972132	60.740532
2151.982780	44.052365	60.745537
2151.434251	53.364852	60.750542
2151.372621	52.012080	60.755546
2151.031879	52.726888	60.760551
2150.154369	50.122106	60.765556
2149.601582	47.109402	60.770561
2147.887582	58.854035	60.775566
2147.007627	58.102622	60.780570
2146.564376	50.081318	60.785575
2145.936812	65.827916	60.790580
2145.971481	46.319575	60.795585
2145.106834	56.833433	60.800590
2145.108566	46.525838	60.805594
2143.928087	57.785265	60.810599
2143.222843	43.462819	60.815604
2142.220688	48.813301	60.820609
2141.439825	48.260641	60.825614
2140.799552	45.725459	60.830618
2140.566367	51.330841	60.835623
2139.986300	47.125521	60.840628
2139.522983	50.127511	60.845633
2138.711290	61.241694	60.850638
2138.243491	47.245862	60.855642
2137.218209	56.380097	60.860647
2136.555128	53.364393	60.865652
2136.138420	42.118641	60.870657
2134.602391	61.836764	60.875662
2134.617093	45.026698	60.880666
2133.685462	56.320763	60.885671
2132.863995	53.489468	60.890676
2132.865537	49.731204	60.895681
2132.092927	54.282000	60.900686
2131.863726	41.975138	60.905690
2131.116666	52.277944	60.910695
2130.001278	50.865279	60.915700
2129.988310	48.429270	60.920705
2128.459958	60.369970	60.925710
2127.501135	50.307826	60.930714
2127.105810	59.297956	60.935719
2126.603234	59.857090	60.940724
2125.941312	55.784611	60.945729
2125.235306	50.261977	60.950734
2124.573404	61.822344	60.955738
2124.481016	57.000310	60.960743
2124.070884	61.514099	60.965748
2123.218635	58.444831	60.970753
2121.799894	54.680100	60.975758
2121.225517	49.478792	60.980762
2121.099933	65.530532	60.985767
2120.552557	55.111357	60.990772
2119.129621	59.618684	60.995777
2118.708552	59.439464	61.000782
2118.989432	55.058116	61.005786
2117.946697	60.159574	61.010791
2116.611279	62.954582	61.015796
2116.154191	53.498827	61.020801
2115.828349	66.196514	61.025806
2114.949499	54.044767	61.030810
2114.451430	58.481043	61.035815
2113.683227	64.639692	61.040820
2112.919321	62.414301	61.045825
2112.484355	74.552126	61.050830
2111.752700	57.904632	61.055834
2110.724886	68.023334	61.060839
2110.511913	64.986679	61.065844
2110.257107	68.990108	61.070849
2108.362199	69.421653	61.075854
2108.392990	68.301806	61.080858
2107.906051	67.177374	61.085863
2107.368841	68.349155	61.090868
2106.155963	55.282131	61.095873
2105.192314	74.038952	61.100878
2105.601471	60.567886	61.105882
2105.109172	74.465285	61.110887
2103.783385	74.740294	61.115892
2102.657837	57.734244	61.120897
2102.332330	74.976813	61.125902
2102.326163	68.499433	61.130906
2101.092610	69.292836	61.135911
2100.013903	68.990882	61.140916
2100.243122	68.333152	61.145921
2099.303575	66.280719	61.150926
2098.571507	64.758355	61.155930
2097.677949	73.171520	61.160935
2096.846569	73.145723	61.165940
2097.058399	66.275772	61.170945
2095.915409	68.890442	61.175950
2095.039544	62.413868	61.180954
2094.447090	68.484710	61.185959
2093.607873	64.710039	61.190964
2093.558376	65.044315	61.195969
2092.324994	66.315527	61.200974
2092.424164	61.116158	61.205978
2091.704014	64.124217	61.210983
2090.709870	63.499756	61.215988
2090.322850	62.558175	61.220993
2089.383680	71.924782	61.225998
2088.882730	65.833433	61.231002
2088.349464	69.898396	61.236007
2087.651509	68.728602	61.241012
2086.504665	68.530509	61.246017
2085.665529	66.580423	61.251022
2085.889785	69.027026	61.256026
2084.854153	61.842501	61.261031
2083.553378	72.069185	61.266036
2083.439266	60.141461	61.271041
2082.626517	70.817422	61.276046
2082.160184	73.654318	61.281050
2081.047952	59.260843	61.286055
2080.431546	76.669426	61.291060
2080.699736	63.239651	61.296065
2079.623643	75.477638	61.301070
2078.888020	61.964295	61.306074
2078.162885	65.113502	61.311079
2077.625991	68.475698	61.316084
2077.022474	61.370845	61.321089
2075.957556	69.235598	61.326094
2075.589029	56.607058	61.331098
2074.996578	70.928791	61.336103
2074.302712	66.162780	61.341108
2074.194440	59.794652	61.346113
2072.592269	71.168339	61.351118
2071.855052	66.382399	61.356122
2071.215558	75.018614	61.361127
2071.384459	68.045084	61.366132
2070.537729	67.092876	61.371137
2069.228154	75.196738	61.376142
2068.571439	69.259425	61.381146
2068.035393	77.022912	61.386151
2067.379016	66.826054	61.391156
2066.952802	61.523971	61.396161
2066.245237	78.822440	61.401166
2065.863624	70.412882	61.406170
2065.092875	61.409048	61.411175
2064.597579	79.422909	61.416180
2064.150846	62.662406	61.421185
2063.535670	79.566156	61.426190
2062.522712	73.939274	61.431194
2061.534827	72.268275	61.436199
2060.580193	76.551504	61.441204
2060.300593	68.808604	61.446209
2059.498080	84.195047	61.451214
2058.966722	72.387149	61.456218
2058.448564	76.255749	61.461223
2057.925667	74.165598	61.466228
2057.469395	75.644676	61.471233
2056.689824	76.944817	61.476238
2056.237773	65.777220	61.481242
2055.475506	72.160456	61.486247
2053.950019	65.282346	61.491252
2053.301338	69.181121	61.496257
2052.574018	77.083777	61.501262
2052.916287	63.984457	61.506266
2052.217261	75.956025	61.511271
2050.925241	73.352398	61.516276
2050.704333	69.955874	61.521281
2049.946919	82.797759	61.526286
2049.835054	70.011785	61.531290
2048.609995	74.248043	61.536295
2047.361508	78.325589	61.541300
2047.123540	73.250684	61.546305
2046.425905	81.905596	61.551310
2045.764587	77.467173	61.556314
2045.150669	76.933780	61.561319
2044.417092	70.598651	61.566324
2044.060641	77.967775	61.571329
2043.536186	72.682860	61.576334
2043.182563	71.390623	61.581338
2042.572899	78.195938	61.586343
2041.238361	83.823148	61.591348
2040.481882	71.543188	61.596353
2039.474018	67.826839	61.601358
2038.940235	67.941496	61.606362
2038.471425	71.611449	61.611367
2037.881172	74.690375	61.616372
2037.813805	73.343247	61.621377
2036.895519	70.344414	61.626382
2036.522532	80.269334	61.631386
2035.788300	64.354007	61.636391
2034.400039	84.520269	61.641396
2034.134018	66.917357	61.646401
2033.093072	76.475180	61.651406
2032.633170	69.178806	61.656410
2032.096936	67.412486	61.661415
2031.455740	70.753395	61.666420
2031.358141	70.789368	61.671425
2030.360886	67.989156	61.676430
2029.392102	75.248871	61.681434
2028.442245	73.862019	61.686439
2027.677033	83.048071	61.691444
2027.362677	66.742823	61.696449
2026.674132	74.279772	61.701454
2026.406101	66.628086	61.706458
2025.862496	71.058988	61.711463
2025.221885	76.057239	61.716468
2024.342922	70.535269	61.721473
2023.210990	74.772528	61.726478
2022.305192	72.388327	61.731482
2021.663778	69.241476	61.736487
2021.079432	80.991419	61.741492
2021.220201	71.508607	61.746497
2020.377675	73.384893	61.751502
2019.941537	71.438682	61.756506
2019.431237	72.368081	61.761511
2018.564778	73.606325	61.766516
2017.554745	69.652202	61.771521
2016.532435	71.172234	61.776526
2016.024778	71.243324	61.781530
2015.901438	63.999200	61.786535
2014.807860	77.791753	61.791540
2014.568506	62.386119	61.796545
2014.093172	74.806330	61.801550
2012.984998	68.191608	61.806554
2012.048833	74.375365	61.811559
2011.409064	75.686448	61.816564
2011.248123	64.731292	61.821569
2010.518333	75.439837	61.826574
2010.182242	67.098766	61.831578
2008.997630	76.868638	61.836583
2007.530226	75.313190	61.841588
2007.232656	79.938446	61.846593
2007.385552	73.331743	61.851598
2006.295537	76.191940	61.856602
2005.728201	77.277055	61.861607
2004.921667	75.429057	61.866612
2004.641993	75.468696	61.871617
2004.070013	76.092486	61.876622
2003.383456	75.777220	61.881626
2002.256976	71.997708	61.886631
2001.208910	72.663943	61.891636
2000.869932	63.725649	61.896641
2000.263043	72.847147	61.901646
2000.185203	68.626804	61.906650
1999.563031	65.875888	61.911655
1998.429621	68.888058	61.916660
1997.877451	66.431971	61.921665
1996.775964	68.013463	61.926670
1996.513957	67.583506	61.931674
1995.661517	72.184859	61.936679
1995.291958	80.199485	61.941684
1995.036659	70.235471	61.946689
1994.316490	82.125249	61.951694
1993.419364	76.882148	61.956698
1992.669852	70.688342	61.961703
1992.211383	72.675574	61.966708
1991.338844	63.352021	61.971713
1989.894944	77.122909	61.976718
1989.210784	76.403553	61.981722
1989.402619	75.202950	61.986727
1988.772538	77.622711	61.991732
1987.887534	69.703091	61.996737
1987.364838	74.570666	62.001742
1987.232618	71.434471	62.006746
1986.017289	74.229407	62.011751
1984.751528	75.887442	62.016756
1984.199244	69.930427	62.021761
1983.680932	81.936406	62.026766
1983.385910	74.642257	62.031770
1982.917662	82.734052	62.036775
1982.262684	77.256973	62.041780
1981.961718	73.343290	62.046785
1980.811046	78.320002	62.051790
1980.100000	69.612658	62.056794
1979.425757	68.950080	62.061799
1978.714040	74.405917	62.066804
1978.291422	70.927873	62.071809
1976.954894	84.208629	62.076814
1975.993312	79.210738	62.081818
1975.289407	82.236752	62.086823
1975.199675	81.044568	62.091828
1974.579868	73.620617	62.096833
1973.851584	84.196467	62.101838
1973.332421	76.906356	62.106842
1973.110834	75.344004	62.111847
1972.776490	78.248278	62.116852
1971.927592	73.312933	62.121857
1970.744301	80.297622	62.126862
1970.430564	72.001896	62.131866
1969.947470	74.503990	62.136871
1968.573329	81.091604	62.141876
1968.029301	78.981171	62.146881
1966.703460	81.214896	62.151886
1966.311907	80.756617	62.156890
1966.143496	80.573589	62.161895
1965.231086	84.366008	62.166900
1965.333459	71.686396	62.171905
1965.093620	81.534990	62.176910
1963.855835	80.480878	62.181914
1962.810530	77.380804	62.186919
1961.857824	76.587382	62.191924
1961.528333	77.808224	62.196929
1960.924156	81.813501	62.201934
1960.189081	81.516986	62.206938
1959.245842	81.417521	62.211943
1958.635661	85.152507	62.216948
1958.208075	75.532822	62.221953
1957.527512	76.467180	62.226958
1957.194272	85.258239	62.231962
1956.735296	75.049007	62.236967
1955.383901	75.504779	62.241972
1954.630329	75.133928	62.246977
1953.797966	77.825510	62.251982
1953.173450	72.045553	62.256986
1952.935188	72.029737	62.261991
1952.624660	75.192015	62.266996
1952.161607	72.431623	62.272001
1951.186213	73.600445	62.277006
1950.078830	71.514783	62.282010
1949.414259	68.289624	62.287015
1948.244694	84.768859	62.292020
1948.529847	72.173780	62.297025
1947.923000	78.429866	62.302030
1947.222099	73.981987	62.307034
1947.119798	69.972118	62.312039
1945.557709	73.989096	62.317044
1945.005534	76.223030	62.322049
1944.526524	72.037984	62.327054
1943.884626	68.891232	62.332058
1943.222141	71.303529	62.337063
1941.686873	75.393525	62.342068
1941.462746	71.497615	62.347073
1940.924523	78.879829	62.352078
1940.435157	76.022687	62.357082
1939.903676	75.697014	62.362087
1939.181205	75.849527	62.367092
1938.733914	69.282904	62.372097
1937.693932	69.646673	62.377102
1936.771191	70.600555	62.382106
1936.537373	73.271249	62.387111
1935.777650	76.113736	62.392116
1935.574732	73.239512	62.397121
1934.114566	76.215265	62.402126
1933.374742	82.068250	62.407130
1932.909758	74.198675	62.412135
1932.262304	82.049254	62.417140
1932.118843	74.762596	62.422145
1931.427892	74.738215	62.427150
1930.918968	79.053239	62.432154
1930.059020	72.470118	62.437159
1928.933073	82.497222	62.442164
1928.714248	79.978771	62.447169
1928.003596	71.061641	62.452174
1927.609767	76.085393	62.457178
1926.809422	62.388417	62.462183
1925.851284	75.809397	62.467188
1925.338176	63.982883	62.472193
1924.898526	61.535762	62.477198
1923.499833	69.073490	62.482202
1923.006015	71.175157	62.487207
1922.078952	76.316673	62.492212
1921.654827	69.744800	62.497217
1921.456318	70.224163	62.502222
1920.645658	72.207388	62.507226
1920.535154	65.022742	62.512231
1919.519603	74.209123	62.517236
1918.648938	68.961854	62.522241
1917.788213	78.047965	62.527246
1917.845757	68.220392	62.532250
1917.049008	63.536998	62.537255
1915.809408	78.354153	62.542260
1915.295730	67.445547	62.547265
1914.504483	65.074742	62.552270
1913.907048	64.786354	62.557274
1913.630827	62.360600	62.562279
1912.488384	77.564468	62.567284
1911.746490	68.589226	62.572289
1910.905992	70.846858	62.577294
1910.578193	65.925012	62.582298
1910.258117	67.434533	62.587303
1909.515487	67.717991	62.592308
1909.097420	63.901762	62.597313
1908.348264	69.081272	62.602318
1907.161806	72.888824	62.607322
1906.768733	73.101022	62.612327
1906.062845	66.507649	62.617332
1905.874198	67.706138	62.622337
1904.874766	69.503285	62.627342
1903.575738	80.117708	62.632346
1903.283568	68.126810	62.637351
1902.632550	74.697429	62.642356
1902.297732	64.184649	62.647361
1902.005112	62.256679	62.652366
1901.279026	70.047196	62.657370
1900.098511	62.436313	62.662375
1899.216622	68.743951	62.667380
1898.496621	70.460470	62.672385
1898.398469	69.594490	62.677390
1897.775764	68.308720	62.682394
1896.873999	70.371072	62.687399
1896.007681	69.994482	62.692404
1895.707894	64.566706	62.697409
1895.087863	71.126098	62.702414
1894.080120	71.249793	62.707418
1893.223263	60.315252	62.712423
1892.471677	64.922698	62.717428
1892.241296	59.991700	62.722433
1891.629353	64.319926	62.727438
1891.039337	66.686036	62.732442
1890.728884	68.681325	62.737447
1889.563153	77.558811	62.742452
1888.768260	65.296058	62.747457
1888.109087	73.069649	62.752462
1887.550179	65.205541	62.757466
1887.194055	53.271333	62.762471
1886.295968	62.987077	62.767476
1885.605985	66.826207	62.772481
1884.735900	64.758097	62.777486
1884.001201	66.349215	62.782490
1884.240143	59.825057	62.787495
1883.358461	75.340781	62.792500
1882.159688	69.986338	62.797505
1881.228781	65.716929	62.802510
1880.767215	67.925449	62.807514
1880.540715	62.142255	62.812519
1880.217631	78.934983	62.817524
1879.398021	72.947893	62.822529
1878.407238	70.667127	62.827534
1877.542539	71.755322	62.832538
1877.247295	68.252346	62.837543
1876.519958	78.747630	62.842548
1875.555227	71.402127	62.847553
1874.924747	80.169411	62.852558
1874.056296	78.224049	62.857562
1873.712504	60.781777	62.862567
1873.170855	71.854722	62.867572
1872.593316	72.930445	62.872577
1871.944607	61.209061	62.877582
1871.009732	67.427344	62.882586
1870.566560	61.189681	62.887591
1869.763993	72.589488	62.892596
1869.587218	65.246630	62.897601
1868.408419	68.551494	62.902606
1867.420098	72.654045	62.907610
1867.261345	70.510854	62.912615
1866.651457	67.508857	62.917620
1866.563410	70.115409	62.922625
1865.398025	70.008668	62.927630
1864.355040	73.839192	62.932634
1863.789286	63.986002	62.937639
1863.307118	71.867116	62.942644
1862.453148	68.709900	62.947649
1861.413102	73.120296	62.952654
1860.428473	67.951070	62.957658
1860.482966	63.340711	62.962663
1859.587330	70.215109	62.967668
1859.398889	69.317733	62.972673
1859.003354	73.455486	62.977678
1858.393153	69.729696	62.982682
1857.290299	74.974837	62.987687
1856.564736	81.057393	62.992692
1855.882153	72.646781	62.997697
1855.576691	69.694227	63.002702
1854.260226	75.517350	63.007706
1853.685724	58.979856	63.012711
1853.160573	71.416654	63.017716
1852.777583	65.946900	63.022721
1852.358319	64.192012	63.027726
1851.590996	66.714018	63.032730
1850.336710	65.249408	63.037735
1849.620151	70.865317	63.042740
1849.409123	65.464458	63.047745
1849.210377	68.326712	63.052750
1848.163098	73.214515	63.057754
1847.627892	63.417983	63.062759
1846.412084	69.322899	63.067764
1845.962286	60.740505	63.072769
1845.631565	61.095781	63.077774
1844.508238	69.385421	63.082778
1843.841657	58.687995	63.087783
1842.872871	70.313686	63.092788
1842.543019	69.363068	63.097793
1842.346279	72.324356	63.102798
1841.609420	72.512297	63.107802
1841.237759	63.046992	63.112807
1839.914474	68.775792	63.117812
1839.456293	66.676992	63.122817
1839.230377	66.984088	63.127822
1837.865219	69.944806	63.132826
1837.271717	62.924382	63.137831
1836.588572	73.626336	63.142836
1836.350748	67.609971	63.147841
1835.725930	65.554977	63.152846
1834.824371	61.012048	63.157850
1833.858813	59.090007	63.162855
1833.264914	69.566470	63.167860
1832.532710	66.520823	63.172865
1832.491194	65.518116	63.177870
1831.967939	67.070945	63.182874
1831.228784	70.818545	63.187879
1829.988905	70.911311	63.192884
1829.527454	67.565623	63.197889
1829.049978	69.757754	63.202894
1828.360629	73.046425	63.207898
1827.264494	73.453847	63.212903
1826.312796	76.225916	63.217908
1825.883810	79.944772	63.222913
1825.660893	74.489029	63.227918
1825.048244	72.812161	63.232922
1824.893319	77.435279	63.237927
1823.856506	76.727805	63.242932
1822.895898	74.913793	63.247937
1822.236256	71.974902	63.252942
1821.663028	83.070220	63.257946
1821.014858	66.506580	63.262951
1819.966642	81.868197	63.267956
1819.376147	65.404215	63.272961
1818.937948	71.241655	63.277966
1818.474645	80.129064	63.282970
1818.099844	71.138146	63.287975
1816.788773	74.300028	63.292980
1816.098067	64.737149	63.297985
1815.689131	70.612522	63.302990
1815.243809	72.264947	63.307994
1814.618748	73.214182	63.312999
1813.532778	78.995994	63.318004
1813.124658	74.899072	63.323009
1812.779104	76.598736	63.328014
1811.463982	74.099829	63.333018
1810.749297	72.790838	63.338023
1809.779451	70.735440	63.343028
1809.454077	72.485517	63.348033
1809.424385	74.193375	63.353038
1808.731822	78.744163	63.358042
1808.068117	64.564271	63.363047
1806.922355	67.925418	63.368052
1806.104212	75.337112	63.373057
1805.934041	73.728765	63.378062
1805.311126	82.732987	63.383066
1804.609487	69.200954	63.388071
1803.423299	77.626754	63.393076
1803.030190	67.698068	63.398081
1802.628905	64.535228	63.403086
1802.069602	82.760321	63.408090
1801.548520	73.065637	63.413095
1800.276864	76.084069	63.418100
1799.587071	80.875701	63.423105
1799.381101	77.292324	63.428110
1798.700156	81.803422	63.433114
1797.482164	76.018398	63.438119
1796.795837	76.203059	63.443124
1796.338926	71.762218	63.448129
1795.876230	72.340312	63.453134
1795.548893	82.108178	63.458138
1794.675761	77.353370	63.463143
1793.709927	78.128058	63.468148
1793.236935	77.452495	63.473153
1792.660021	81.183807	63.478158
1791.947777	79.442334	63.483162
1791.134538	71.430974	63.488167
1790.267361	75.809214	63.493172
1789.415084	75.111876	63.498177
1789.333868	74.309445	63.503182
1788.767475	77.116540	63.508186
1788.619610	74.848620	63.513191
1787.383949	82.844667	63.518196
1786.774662	83.813483	63.523201
1786.095973	78.124180	63.528206
1785.236295	73.685795	63.533210
1784.323860	77.976604	63.538215
1783.166030	78.666662	63.543220
1782.893433	78.623197	63.548225
1782.738337	71.080570	63.553230
1781.766002	71.829485	63.558234
1781.384109	76.855297	63.563239
1781.094441	79.569564	63.568244
1780.471012	82.641192	63.573249
1779.676893	81.362170	63.578254
1778.894809	74.348839	63.583258
1777.854966	73.733331	63.588263
1776.666425	78.558435	63.593268
1776.044667	77.253621	63.598273
1775.644502	79.378289	63.603278
1775.099133	74.147229	63.608282
1775.339642	71.853119	63.613287
1774.563771	74.200668	63.618292
1774.316894	77.685601	63.623297
1773.078335	79.012976	63.628302
1772.023432	73.795808	63.633306
1771.191012	68.159313	63.638311
1770.051075	73.126514	63.643316
1769.554764	76.669193	63.648321
1769.703733	73.148520	63.653326
1768.806892	71.448986	63.658330
1768.627398	65.918547	63.663335
1767.698239	84.465736	63.668340
1766.542820	69.835645	63.673345
1765.995250	69.241319	63.678350
1765.480701	79.202132	63.683354
1765.269298	64.564065	63.688359
1763.940303	72.496087	63.693364
1763.374365	74.762203	63.698369
1762.680412	74.880273	63.703374
1762.160765	70.723801	63.708378
1762.023428	55.669481	63.713383
1761.233383	72.728744	63.718388
1760.593292	69.947619	63.723393
1760.057744	71.158627	63.728398
1758.786130	74.662787	63.733402
1757.941628	68.709661	63.738407
1756.900481	80.290100	63.743412
1756.841711	81.729756	63.748417
1756.432272	72.380855	63.753422
1755.659494	74.566275	63.758426
1754.572308	72.239365	63.763431
1753.945081	67.499144	63.768436
1753.424888	66.714387	63.773441
1753.448290	68.560473	63.778446
1752.714417	74.275350	63.783450
1751.539541	65.577095	63.788455
1750.583410	68.947575	63.793460
1750.218518	69.570071	63.798465
1749.858798	72.349082	63.803470
1749.111369	71.777037	63.808474
1748.357607	75.186346	63.813479
1747.822437	77.141641	63.818484
1747.114498	78.577943	63.823489
1746.581470	76.670035	63.828494
1745.079391	79.823649	63.833498
1744.190431	73.285423	63.838503
1743.901785	73.938390	63.843508
1744.145799	70.627346	63.848513
1743.673814	71.169076	63.853518
1742.685821	79.178635	63.858522
1741.970648	71.630341	63.863527
1740.761952	72.467272	63.868532
1740.283513	82.803989	63.873537
1739.992223	73.113043	63.878542
1739.110869	75.079161	63.883546
1738.392078	64.922299	63.888551
1737.501065	66.552474	63.893556
1737.485466	71.282777	63.898561
1736.897738	64.883593	63.903566
1735.445137	73.153812	63.908570
1734.935302	75.510374	63.913575
1734.507527	72.181436	63.918580
1733.682127	74.345256	63.923585
1733.130876	69.525163	63.928590
1731.969527	78.039299	63.933594
1731.625892	63.385182	63.938599
1731.179356	72.262044	63.943604
1730.231464	73.342997	63.948609
1730.383309	65.403904	63.953614
1728.986708	66.352687	63.958618
1728.420790	71.917888	63.963623
1727.700085	68.488813	63.968628
1727.414680	69.901381	63.973633
1727.169686	61.911771	63.978638
1725.663309	71.258162	63.983642
1725.102807	71.760336	63.988647
1724.463301	66.462239	63.993652
1724.217590	61.440656	63.998657
1723.417956	64.614396	64.003662
1722.266698	71.695014	64.008666
1721.795126	71.717850	64.013671
1721.297302	74.681229	64.018676
1720.854190	72.797684	64.023681
1719.857779	63.202178	64.028686
1718.855895	67.529287	64.033690
1718.698207	65.269243	64.038695
1718.164689	64.887167	64.043700
1717.526959	64.438062	64.048705
1716.589586	65.324955	64.053710
1715.471142	67.098493	64.058714
1715.085120	59.910323	64.063719
1714.488209	58.822359	64.068724
1714.399328	71.569144	64.073729
1713.640934	69.158493	64.078734
1712.551322	72.234786	64.083738
1712.144831	72.346638	64.088743
1711.627472	72.491869	64.093748
1710.696895	69.384723	64.098753
1709.902254	71.974186	64.103758
1709.110098	73.927724	64.108762
1708.989245	72.063964	64.113767
1708.329634	69.241799	64.118772
1707.233710	66.958877	64.123777
1706.606824	71.377824	64.128782
1705.805149	70.924798	64.133786
1705.461519	70.719152	64.138791
1705.014053	73.010619	64.143796
1703.690702	80.716263	64.148801
1702.931587	62.002714	64.153806
1702.480973	67.201087	64.158810
1702.193625	69.135953	64.163815
1701.437872	72.808948	64.168820
1701.094011	78.588053	64.173825
1700.248743	63.695064	64.178830
1699.505962	75.823443	64.183834
1698.949916	69.102260	64.188839
1698.312983	67.572788	64.193844
1697.375353	77.155302	64.198849
1696.594970	77.605670	64.203854
1695.959090	73.872964	64.208858
1695.420077	73.827666	64.213863
1695.204940	73.748275	64.218868
1694.155108	73.571216	64.223873
1693.332222	67.904850	64.228878
1692.290311	79.468869	64.233882
1692.723736	66.840790	64.238887
1692.108579	67.318535	64.243892
1690.571659	66.061326	64.248897
1690.302573	73.448130	64.253902
1689.542146	79.927354	64.258906
1689.262256	67.478805	64.263911
1687.940166	66.001390	64.268916
1687.176884	69.957866	64.273921
1686.757654	65.758656	64.278926
1685.999796	75.864566	64.283930
1685.746612	71.030259	64.288935
1685.149363	74.383184	64.293940
1684.194284	71.204244	64.298945
1683.836946	68.124333	64.303950
1682.919259	65.109772	64.308954
1682.438768	66.980696	64.313959
1681.364571	69.529412	64.318964
1680.541122	71.068447	64.323969
1680.070109	68.579043	64.328974
1679.967554	70.863039	64.333978
1679.388367	67.484043	64.338983
1678.289963	64.297909	64.343988
1677.565397	60.856849	64.348993
1677.170898	70.413020	64.353998
1676.446896	69.870392	64.359002
1675.895252	63.481265	64.364007
1674.874907	71.895747	64.369012
1674.197491	68.199609	64.374017
1673.850439	67.674381	64.379022
1672.776231	74.704931	64.384026
1672.201107	73.952571	64.389031
1671.440647	78.129385	64.394036
1670.672380	71.046091	64.399041
1670.651990	66.816649	64.404046
1670.084235	75.509339	64.409050
1669.353259	71.854826	64.414055
1668.296738	72.735429	64.419060
1667.693791	72.347045	64.424065
1667.250770	65.582687	64.429070
1666.702398	69.894551	64.434074
1665.977057	75.828871	64.439079
1665.173788	70.019046	64.444084
1664.669035	71.915906	64.449089
1663.793998	59.388435	64.454094
1662.424048	73.983512	64.459098
1662.069742	72.634668	64.464103
1661.976139	59.502088	64.469108
1661.325496	72.751273	64.474113
1661.223169	62.226856	64.479118
1659.936533	75.450906	64.484122
1659.327522	68.077385	64.489127
1658.521973	73.890402	64.494132
1657.728089	76.393025	64.499137
1657.289643	68.360035	64.504142
1656.342315	72.440374	64.509146
1656.232812	69.049857	64.514151
1655.069920	68.353018	64.519156
1654.372222	76.180078	64.524161
1653.623356	64.802699	64.529166
1652.883061	64.161738	64.534170
1652.841242	67.442210	64.539175
1652.557272	78.136769	64.544180
1651.208836	71.528850	64.549185
1650.420744	64.691573	64.554190
1649.656399	79.919035	64.559194
1649.458206	66.752601	64.564199
1648.826948	70.686539	64.569204
1647.815418	73.523366	64.574209
1647.408234	67.472431	64.579214
1646.567392	76.311009	64.584218
1646.193616	70.820908	64.589223
1644.940072	64.686792	64.594228
1644.174766	65.812890	64.599233
1643.895011	67.027443	64.604238
1643.053485	69.444594	64.609242
1643.181925	68.126304	64.614247
1642.194463	62.637494	64.619252
1641.330217	70.789063	64.624257
1640.896727	64.683960	64.629262
1639.960702	70.524015	64.634266
1639.384392	63.030187	64.639271
1638.323316	66.152439	64.644276
1637.481354	73.023102	64.649281
1637.584078	58.242918	64.654286
1636.952805	70.389860	64.659290
1636.523823	58.099061	64.664295
1635.574241	58.312967	64.669300
1634.440447	65.573771	64.674305
1634.393068	64.180906	64.679310
1632.997956	73.016067	64.684314
1632.526855	75.886903	64.689319
1631.923960	74.399351	64.694324
1631.330428	73.079051	64.699329
1631.313854	66.822563	64.704334
1630.445196	76.140239	64.709338
1629.153242	59.771213	64.714343
1628.555707	65.783008	64.719348
1627.734238	66.025452	64.724353
1627.575528	59.226982	64.729358
1627.077922	64.846001	64.734362
1626.089346	57.469712	64.739367
1625.552494	56.417962	64.744372
1624.755778	60.988484	64.749377
1624.515526	61.682662	64.754382
1623.250685	72.952516	64.759386
1622.454386	69.423516	64.764391
1621.834489	70.048691	64.769396
1621.415035	71.469948	64.774401
1621.461093	66.406760	64.779406
1620.426225	73.073100	64.784410
1619.760047	63.967669	64.789415
1619.100704	67.598559	64.794420
1618.187977	70.796603	64.799425
1617.539373	60.661759	64.804430
1616.536236	62.968968	64.809434
1616.022127	68.067049	64.814439
1615.751865	64.963856	64.819444
1615.204017	68.151245	64.824449
1614.511834	61.674073	64.829454
1613.373507	66.693117	64.834458
1612.995681	65.600336	64.839463
1612.551894	60.876749	64.844468
1611.300961	65.582513	64.849473
1610.706079	68.309007	64.854478
1609.936459	76.871344	64.859482
1609.848341	72.953869	64.864487
1609.304949	67.552226	64.869492
1608.572977	69.619237	64.874497
1607.604046	66.362102	64.879502
1606.542789	70.112039	64.884506
1606.319443	75.186010	64.889511
1606.175587	67.752802	64.894516
1604.903904	73.411220	64.899521
1604.720155	67.778973	64.904526
1603.722485	65.680768	64.909530
1603.075670	62.918104	64.914535
1602.510875	65.652435	64.919540
1601.378891	68.068432	64.924545
1600.851875	58.491460	64.929550
1600.481913	71.735484	64.934554
1600.117875	72.261668	64.939559
1599.073989	65.372005	64.944564
1597.890978	67.783493	64.949569
1597.826188	56.604981	64.954574
1597.186836	66.280478	64.959578
1596.821452	61.997037	64.964583
1595.684549	64.446934	64.969588
1595.157208	63.504069	64.974593
1594.572395	59.810592	64.979598
1593.680365	65.571127	64.984602
1592.794288	53.587936	64.989607
1592.413134	58.866750	64.994612
1591.644193	64.675541	64.999617
1591.703491	57.006633	65.004622
1590.470846	65.467481	65.009626
1589.570546	61.339989	65.014631
1589.255489	64.424165	65.019636
1588.628385	61.213660	65.024641
1588.342277	58.491469	65.029646
1587.241466	64.996400	65.034650
1586.498971	63.215640	65.039655
1586.009036	58.672861	65.044660
1584.925650	68.120854	65.049665
1583.907295	58.273431	65.054670
1583.193627	62.121121	65.059674
1582.965096	58.885145	65.064679
1582.410658	57.899278	65.069684
1581.838005	61.435975	65.074689
1581.943703	61.431781	65.079694
1581.019932	58.639006	65.084698
1580.068522	60.930125	65.089703
1579.567142	58.789354	65.094708
1578.324952	67.522967	65.099713
1577.885419	54.647222	65.104718
1576.884244	62.508312	65.109722
1576.750063	57.927939	65.114727
1576.142797	57.803621	65.119732
1575.462191	64.011554	65.124737
1574.888623	57.747370	65.129742
1573.764836	58.676545	65.134746
1573.453242	64.674460	65.139751
1572.806617	63.077174	65.144756
1571.382306	64.659663	65.149761
1571.041408	57.681983	65.154766
1570.079366	66.200774	65.159770
1569.797345	56.718933	65.164775
1569.728491	57.333844	65.169780
1569.259962	59.739064	65.174785
1568.729118	54.896853	65.179790
1567.788815	67.925552	65.184794
1566.778496	61.055805	65.189799
1565.754219	57.881601	65.194804
1565.010912	55.003389	65.199809
1564.732320	45.956262	65.204814
1564.250538	57.863402	65.209818
1563.534815	54.368934	65.214823
1562.742097	59.637445	65.219828
1561.996498	62.752179	65.224833
1561.862004	58.044121	65.229838
1560.849336	66.648231	65.234842
1559.760732	68.071730	65.239847
1559.470860	58.043920	65.244852
1558.745634	69.608116	65.249857
1558.433052	56.570276	65.254862
1557.044874	70.977468	65.259866
1556.620879	60.854269	65.264871
1555.883332	60.548800	65.269876
1555.426432	64.737334	65.274881
1555.531889	56.960167	65.279886
1554.341080	60.503618	65.284890
1553.444446	52.412571	65.289895
1553.114980	58.738185	65.294900
1552.055258	54.533535	65.299905
1551.525256	61.608544	65.304910
1550.465170	70.445704	65.309914
1549.904353	64.348237	65.314919
1549.803959	64.744227	65.319924
1549.119529	68.826984	65.324929
1548.412947	61.574663	65.329934
1547.265666	72.220299	65.334938
1546.474902	68.427088	65.339943
1546.514149	61.802184	65.344948
1545.672148	67.671482	65.349953
1544.976558	60.628733	65.354958
1544.246445	72.223673	65.359962
1543.721932	68.530088	65.364967
1543.766957	65.622822	65.369972
1541.991413	70.359930	65.374977
1541.407054	61.941715	65.379982
1540.783321	69.531530	65.384986
1540.662160	66.480353	65.389991
1539.791737	66.823645	65.394996
1538.722730	71.224562	65.400001
1538.185424	60.753508	65.405006
1537.996362	63.303569	65.410010
1537.106381	67.114629	65.415015
1536.251894	58.934885	65.420020
1535.197848	61.284907	65.425025
1535.208315	52.116157	65.430030
1534.823382	56.490381	65.435034
1533.417084	62.529769	65.440039
1532.982729	61.974276	65.445044
1532.149607	65.735301	65.450049
1532.044614	60.645656	65.455054
1531.344550	61.106966	65.460058
1530.212545	59.413346	65.465063
1529.464329	56.147984	65.470068
1528.691365	49.852420	65.475073
1528.634653	58.288870	65.480078
1527.863239	62.123670	65.485082
1526.959938	61.268944	65.490087
1526.306313	59.371578	65.495092
1525.709149	66.712738	65.500097
1525.388184	55.887187	65.505102
1524.136973	67.148599	65.510106
1523.484616	59.608543	65.515111
1523.139092	61.060645	65.520116
1522.799416	63.006994	65.525121
1522.143294	58.687761	65.530126
1520.970442	65.994237	65.535130
1520.145437	62.548685	65.540135
1519.867697	61.697067	65.545140
1519.316071	66.796391	65.550145
1519.032791	57.507154	65.555150
1517.693205	60.591700	65.560154
1517.002454	63.882239	65.565159
1517.045693	54.315611	65.570164
1516.156832	63.483547	65.575169
1515.273550	58.596423	65.580174
1514.550609	65.161188	65.585178
1513.835370	60.687343	65.590183
1512.734859	53.882420	65.595188
1511.980429	70.145976	65.600193
1511.857510	57.948511	65.605198
1511.063634	56.049779	65.610202
1510.820169	59.406444	65.615207
1510.492385	57.096174	65.620212
1509.286148	62.756845	65.625217
1508.325679	60.165477	65.630222
1508.134292	57.568598	65.635226
1506.897948	68.351403	65.640231
1506.542066	62.489473	65.645236
1505.669297	64.208290	65.650241
1505.499474	53.882290	65.655246
1504.855757	59.565542	65.660250
1504.165620	57.032147	65.665255
1503.327565	58.545169	65.670260
1502.558457	61.584804	65.675265
1502.143233	57.747707	65.680270
1501.657480	56.657902	65.685274
1500.376458	61.653929	65.690279
1499.570815	57.730634	65.695284
1499.192073	62.220576	65.700289
1498.906437	59.678100	65.705294
1498.342784	59.431750	65.710298
1497.298606	68.449328	65.715303
1496.683331	46.680484	65.720308
1495.874086	56.974359	65.725313
1495.874780	56.376550	65.730318
1494.840134	60.330461	65.735322
1493.698014	63.178631	65.740327
1493.360154	61.231096	65.745332
1493.037821	66.929517	65.750337
1492.353461	62.587970	65.755342
1491.425067	63.933997	65.760346
1490.386161	61.299905	65.765351
1490.269589	53.854500	65.770356
1489.506142	69.618006	65.775361
1488.826590	58.016792	65.780366
1487.392555	71.229628	65.785370
1487.316922	63.473353	65.790375
1487.025605	55.237256	65.795380
1486.480210	65.424554	65.800385
1485.709088	62.926110	65.805390
1484.703772	61.199763	65.810394
1484.309358	61.442199	65.815399
1483.927342	50.380352	65.820404
1482.255303	62.110783	65.825409
1482.059973	54.944406	65.830414
1481.421215	55.143668	65.835418
1480.886430	62.375570	65.840423
1480.659705	59.770117	65.845428
1479.838569	67.646783	65.850433
1478.904651	63.772264	65.855438
1478.372306	61.089218	65.860442
1476.965533	65.567485	65.865447
1476.501546	57.809850	65.870452
1475.584833	64.052168	65.875457
1475.625227	58.157236	65.880462
1475.148100	65.327937	65.885466
1474.751766	60.415486	65.890471
1473.525166	61.231728	65.895476
1472.721825	65.893231	65.900481
1472.335861	59.616610	65.905486
1471.625171	66.646228	65.910490
1471.063107	69.140448	65.915495
1470.436897	61.621486	65.920500
1469.655054	64.278368	65.925505
1469.096523	52.706820	65.930510
1468.564752	63.544828	65.935514
1467.667833	66.052837	65.940519
1467.193225	60.720730	65.945524
1466.461410	59.282095	65.950529
1465.458078	56.625014	65.955534
1464.858773	56.370144	65.960538
1464.308244	59.504367	65.965543
1464.004921	54.572408	65.970548
1462.657276	76.880245	65.975553
1461.972768	59.269899	65.980558
1461.494051	67.047997	65.985562
1460.650384	61.859700	65.990567
1460.634821	62.210671	65.995572
1460.233824	67.541540	66.000577
1459.462192	56.680388	66.005582
1458.390485	56.729258	66.010586
1457.961467	63.390830	66.015591
1457.366802	71.736151	66.020596
1456.002556	71.922979	66.025601
1455.479673	63.758378	66.030606
1455.196301	61.658683	66.035610
1454.505257	57.747154	66.040615
1454.100457	64.502652	66.045620
1452.779094	66.448899	66.050625
1452.518771	59.972537	66.055630
1451.779715	60.271327	66.060634
1451.327938	57.819918	66.065639
1450.279340	60.963910	66.070644
1449.081215	61.955416	66.075649
1449.015781	58.099010	66.080654
1448.429343	62.759164	66.085658
1448.347398	61.483766	66.090663
1447.802292	62.727892	66.095668
1446.579126	59.315682	66.100673
1445.829561	63.118646	66.105678
1445.556752	63.116252	66.110682
1444.128956	65.659751	66.115687
1443.805653	60.530691	66.120692
1442.834360	69.396351	66.125697
1442.855942	59.585580	66.130702
1442.213893	58.804485	66.135706
1441.018854	55.846713	66.140711
1440.625457	57.222852	66.145716
1440.053836	59.425274	66.150721
1439.197488	61.180926	66.155726
1438.271690	65.970713	66.160730
1437.526595	58.705629	66.165735
1437.146331	52.038596	66.170740
1436.853600	61.058190	66.175745
1436.436080	62.234732	66.180750
1435.322448	63.753724	66.185754
1434.515068	63.017831	66.190759
1434.209693	54.438618	66.195764
1433.095653	65.947927	66.200769
1432.151024	66.303049	66.205774
1431.744356	62.275365	66.210778
1431.136203	60.686196	66.215783
1430.853104	63.230706	66.220788
1430.326980	65.102616	66.225793
1429.645545	61.769901	66.230798
1428.614810	56.160329	66.235802
1428.100794	57.145622	66.240807
1427.546264	56.585593	66.245812
1426.462199	63.258233	66.250817
1425.958740	60.723577	66.255822
1425.371409	61.271080	66.260826
1424.854397	68.060186	66.265831
1424.168845	54.804109	66.270836
1422.849752	61.206591	66.275841
1422.721065	57.872762	66.280846
1422.174267	62.450925	66.285850
1421.666606	60.074637	66.290855
1420.897584	59.286919	66.295860
1420.268452	64.630394	66.300865
1419.780793	56.881267	66.305870
1418.645393	66.031641	66.310874
1417.822804	61.068675	66.315879
1417.155962	53.161944	66.320884
1416.505829	67.920250	66.325889
1416.345004	62.196076	66.330894
1415.872145	60.705259	66.335898
1414.474034	66.696094	66.340903
1414.050651	58.786937	66.345908
1413.434963	64.990892	66.350913
1413.062582	58.939213	66.355918
1412.049339	57.537439	66.360922
1411.485361	65.778535	66.365927
1410.979106	58.213719	66.370932
1410.378535	59.600713	66.375937
1409.840341	60.559889	66.380942
1408.578672	59.905670	66.385946
1407.733608	56.062792	66.390951
1407.563899	56.338913	66.395956
1407.014604	63.543168	66.400961
1406.267362	61.649675	66.405966
1405.529575	62.878701	66.410970
1404.680064	63.933093	66.415975
1404.950976	62.614228	66.420980
1403.753558	57.504258	66.425985
1402.798074	55.910377	66.430990
1402.133202	55.717984	66.435994
1401.637708	61.803485	66.440999
1401.249489	53.630119	66.446004
1399.921512	60.106563	66.451009
1399.529775	58.516121	66.456014
1398.628886	59.596028	66.461018
1398.443113	63.668946	66.466023
1398.157351	52.279578	66.471028
1396.830701	62.397088	66.476033
1396.223869	54.670065	66.481038
1395.906694	58.489471	66.486042
1394.629165	63.984897	66.491047
1393.999163	63.345406	66.496052
1393.102198	69.122553	66.501057
1392.685705	63.953118	66.506062
1392.604910	64.722899	66.511066
1392.024964	66.746878	66.516071
1391.681001	65.691329	66.521076
1390.364507	65.495276	66.526081
1390.033162	57.163056	66.531086
1389.257274	64.543682	66.536090
1387.986798	64.427051	66.541095
1387.338632	54.599738	66.546100
1386.942546	57.159056	66.551105
1386.891790	51.664982	66.556110
1385.852909	63.849925	66.561114
1384.704013	66.445322	66.566119
1384.527975	60.780343	66.571124
1383.964021	58.558094	66.576129
1383.313145	59.093629	66.581134
1382.263098	59.582222	66.586138
1381.416564	63.187721	66.591143
1381.372837	62.619052	66.596148
1380.837770	65.858068	66.601153
1379.642458	58.487945	66.606158
1378.612496	57.861569	66.611162
1378.401000	62.328093	66.616167
1378.406784	52.149251	66.621172
1377.446853	61.287515	66.626177
1376.419683	52.718965	66.631182
1375.828687	60.995897	66.636186
1375.169011	59.350276	66.641191
1375.135936	53.856545	66.646196
1373.767834	67.929444	66.651201
1373.308083	53.642416	66.656206
1373.009092	54.278141	66.661210
1371.600806	61.372929	66.666215
1371.020734	54.997873	66.671220
1370.422996	52.970239	66.676225
1370.022227	55.844123	66.681230
1369.541439	57.879153	66.686234
1368.459816	59.648557	66.691239
1367.951379	48.149512	66.696244
1367.129732	52.793448	66.701249
1366.992209	56.696265	66.706254
1365.643249	51.846954	66.711258
1364.616762	59.811480	66.716263
1364.499337	51.951479	66.721268
1364.066872	58.654607	66.726273
1363.661819	53.721490	66.731278
1362.880287	62.396151	66.736282
1361.799075	67.978661	66.741287
1361.704548	58.438673	66.746292
1360.701115	68.884879	66.751297
1359.596935	61.959184	66.756302
1359.164635	62.827419	66.761306
1358.251752	68.141894	66.766311
1358.011866	51.519091	66.771316
1357.704018	55.657146	66.776321
1356.655076	61.608273	66.781326
1355.962550	58.799328	66.786330
1355.159865	57.859282	66.791335
1354.947128	50.556918	66.796340
1354.449003	60.875487	66.801345
1353.337045	55.843424	66.806350
1352.963265	45.923626	66.811354
1352.095946	61.978049	66.816359
1351.233140	59.992554	66.821364
1350.234260	60.537683	66.826369
1349.737536	55.680643	66.831374
1349.343362	54.254605	66.836378
1348.896874	59.230004	66.841383
1348.679750	57.965060	66.846388
1347.493670	61.928904	66.851393
1346.741527	56.722949	66.856398
1346.345251	59.118295	66.861402
1345.022243	63.198526	66.866407
1344.662409	56.469915	66.871412
1343.917581	61.377621	66.876417
1343.591196	61.265480	66.881422
1343.313818	58.518281	66.886426
1342.331824	57.226688	66.891431
1341.569416	53.916335	66.896436
1340.791044	58.608595	66.901441
1340.374771	58.944416	66.906446
1339.335746	64.384605	66.911450
1338.459248	67.070763	66.916455
1337.980092	54.963080	66.921460
1337.701177	62.655808	66.926465
1337.336062	60.220608	66.931470
1336.404311	56.968715	66.936474
1335.252350	59.208219	66.941479
1334.815453	55.945472	66.946484
1334.462667	58.504221	66.951489
1333.568256	60.977180	66.956494
1332.577474	56.913060	66.961498
1331.944655	60.957696	66.966503
1332.048787	56.820447	66.971508
1331.297025	52.407665	66.976513
1330.072367	53.393981	66.981518
1329.560392	51.202909	66.986522
1328.960961	60.722280	66.991527
1328.518084	54.095186	66.996532
1327.627704	66.707560	67.001537
1326.745873	57.657022	67.006542
1326.479775	49.076322	67.011546
1325.817035	61.136828	67.016551
1324.620261	59.174471	67.021556
1324.209562	57.986035	67.026561
1323.581095	49.888730	67.031566
1323.078545	55.246791	67.036570
1322.531360	57.874293	67.041575
1321.658905	58.326793	67.046580
1320.959147	61.129942	67.051585
1320.407524	52.438511	67.056590
1320.130548	55.999214	67.061594
1318.908218	57.962899	67.066599
1318.126564	57.229261	67.071604
1317.557443	55.141895	67.076609
1317.138292	59.319727	67.081614
1316.882495	51.347686	67.086618
1315.566840	64.625348	67.091623
1315.148275	53.602472	67.096628
1314.660699	57.485245	67.101633
1313.766142	65.972878	67.106638
1312.828286	56.641088	67.111642
1312.222973	66.461028	67.116647
1311.744823	53.586776	67.121652
1311.403404	53.951703	67.126657
1310.617734	61.857461	67.131662
1309.675624	63.983188	67.136666
1308.637658	65.045493	67.141671
1308.767706	50.877617	67.146676
1308.126218	58.878727	67.151681
1306.759370	60.813352	67.156686
1306.141731	58.218026	67.161690
1305.668623	64.508144	67.166695
1305.166098	58.715303	67.171700
1304.956412	53.754293	67.176705
1304.150245	54.792363	67.181710
1303.499965	58.713621	67.186714
1302.699347	69.409881	67.191719
1301.546393	58.002276	67.196724
1300.569047	58.200217	67.201729
1299.915186	59.479010	67.206734
1299.775272	57.761815	67.211738
1299.253901	60.634382	67.216743
1298.999066	61.215787	67.221748
1298.068596	63.877421	67.226753
1296.991678	53.113763	67.231758
1296.881711	52.096723	67.236762
1296.251542	54.234362	67.241767
1295.459167	50.635469	67.246772
1294.268551	60.896976	67.251777
1293.779205	51.383503	67.256782
1293.446539	49.133969	67.261786
1292.921050	58.282034	67.266791
1291.850928	57.826084	67.271796
1290.918099	61.017964	67.276801
1290.394618	55.931798	67.281806
1290.358786	52.781920	67.286810
1289.041823	57.827909	67.291815
1288.507523	59.806803	67.296820
1287.711619	62.243615	67.301825
1287.518236	64.368586	67.306830
1287.037072	62.413903	67.311834
1285.966565	65.097806	67.316839
1285.396901	61.539201	67.321844
1284.393784	59.867780	67.326849
1284.410463	59.948691	67.331854
1283.808859	56.239044	67.336858
1282.536402	69.263844	67.341863
1281.977093	58.750641	67.346868
1281.614858	68.353739	67.351873
1280.382230	56.544067	67.356878
1279.909265	59.632874	67.361882
1279.504105	67.053934	67.366887
1279.060928	65.474844	67.371892
1278.369920	67.164835	67.376897
1277.405121	64.154767	67.381902
1277.203738	65.350587	67.386906
1276.325940	68.095320	67.391911
1275.248936	59.582049	67.396916
1274.491431	56.236244	67.401921
1274.179869	58.182881	67.406926
1273.661590	62.736033	67.411930
1272.967727	56.342827	67.416935
1272.080912	59.718213	67.421940
1271.279262	63.531078	67.426945
1270.842435	62.329459	67.431950
1270.693422	61.993579	67.436954
1269.219459	70.540231	67.441959
1268.829054	61.253884	67.446964
1268.381190	68.071440	67.451969
1267.385350	67.381334	67.456974
1266.432141	52.526233	67.461978
1265.312735	57.335814	67.466983
1265.284712	58.546649	67.471988
1264.977003	64.643313	67.476993
1264.446693	68.804134	67.481998
1264.393520	53.350182	67.487002
1263.037812	64.562067	67.492007
1262.352476	54.040526	67.497012
1261.768683	67.053609	67.502017
1260.831557	55.272661	67.507022
1260.113779	59.691950	67.512026
1259.368645	58.886291	67.517031
1258.996722	53.380212	67.522036
1258.568180	53.374213	67.527041
1257.762207	57.627748	67.532046
1256.882209	55.175078	67.537050
1255.941422	63.305790	67.542055
1255.929987	49.343348	67.547060
1254.950415	58.990980	67.552065
1253.892215	63.309853	67.557070
1253.736176	68.668027	67.562074
1252.924593	71.506322	67.567079
1252.662876	59.613253	67.572084
1251.465902	65.113281	67.577089
1250.953888	62.166853	67.582094
1250.572194	60.918623	67.587098
1249.855042	63.844407	67.592103
1248.994968	63.017601	67.597108
1247.983586	63.056967	67.602113
1247.817442	59.465752	67.607118
1247.358086	60.145913	67.612122
1246.706739	68.566508	67.617127
1245.699065	57.410233	67.622132
1244.853668	53.053370	67.627137
1244.476327	62.037534	67.632142
1243.946264	54.738334	67.637146
1242.571896	73.981655	67.642151
1241.852796	60.628479	67.647156
1241.583811	64.758789	67.652161
1241.238103	62.542875	67.657166
1241.034406	57.987783	67.662170
1239.802760	63.895460	67.667175
1238.801315	54.578548	67.672180
1238.551960	65.067312	67.677185
1238.175730	68.659575	67.682190
1237.307528	57.230386	67.687194
1236.179855	60.601502	67.692199
1236.112149	50.383899	67.697204
1235.404250	59.936298	67.702209
1234.226738	61.058668	67.707214
1233.890564	56.870003	67.712218
1233.220877	58.323220	67.717223
1232.953594	59.277202	67.722228
1231.594310	52.090935	67.727233
1231.144455	51.523768	67.732238
1230.766398	47.958368	67.737242
1230.196854	59.488390	67.742247
1229.008558	56.480765	67.747252
1228.345010	59.246639	67.752257
1227.768601	59.413971	67.757262
1227.490576	56.125984	67.762266
1226.839358	70.709437	67.767271
1225.823256	59.472507	67.772276
1225.178804	57.594265	67.777281
1224.436710	59.927919	67.782286
1224.084608	53.152373	67.787290
1223.163972	65.922546	67.792295
1222.530841	63.086849	67.797300
1221.950058	63.696435	67.802305
1221.702516	65.259152	67.807310
1220.995054	53.725564	67.812314
1219.829182	62.902927	67.817319
1219.455282	66.151037	67.822324
1218.644009	63.838843	67.827329
1217.528641	60.611464	67.832334
1216.809211	54.797944	67.837338
1216.195908	58.672338	67.842343
1215.978973	59.919521	67.847348
1215.787847	61.260373	67.852353
1214.891800	66.720449	67.857358
1214.175971	61.071939	67.862362
1213.192830	64.740212	67.867367
1212.911164	62.033137	67.872372
1212.500936	55.022402	67.877377
1211.137181	61.753785	67.882382
1210.662245	58.222716	67.887386
1210.027567	64.038632	67.892391
1209.636038	56.704794	67.897396
1208.496687	57.571943	67.902401
1207.742993	57.081482	67.907406
1207.477317	60.649858	67.912410
1206.798299	62.743246	67.917415
1206.243257	53.066775	67.922420
1205.271438	57.706250	67.927425
1204.419391	68.147350	67.932430
1204.191576	51.688254	67.937434
1203.492508	58.676648	67.942439
1203.060614	59.026014	67.947444
1202.135492	55.781006	67.952449
1201.482021	59.021534	67.957454
1201.341339	48.041241	67.962458
1200.281079	59.196703	67.967463
1199.443890	53.390877	67.972468
1199.023909	51.885388	67.977473
1198.174522	52.753741	67.982478
1197.311036	49.484742	67.987482
1196.762866	63.670173	67.992487
1196.225425	54.135989	67.997492
1195.517511	47.836512	68.002497
1194.914122	54.869617	68.007502
1194.043105	50.600429	68.012506
1192.938725	59.012643	68.017511
1192.494606	59.272490	68.022516
1192.262068	58.087285	68.027521
1191.987568	61.382670	68.032526
1191.756282	51.459174	68.037530
1190.517504	59.490629	68.042535
1190.099520	61.219228	68.047540
1188.554905	62.374765	68.052545
1187.880420	60.225336	68.057550
1187.610971	55.880986	68.062554
1187.084552	58.938883	68.067559
1186.309186	50.401349	68.072564
1185.533876	63.558435	68.077569
1184.904157	62.652440	68.082574
1184.639468	62.923179	68.087578
1183.798392	53.196006	68.092583
1182.873586	52.150855	68.097588
1182.153461	58.857167	68.102593
1181.559021	57.393618	68.107598
1181.410650	56.228146	68.112602
1180.299098	55.750446	68.117607
1179.350100	61.537503	68.122612
1178.958700	70.933928	68.127617
1178.426449	67.325245	68.132622
1177.928280	63.707988	68.137626
1177.113638	66.862187	68.142631
1176.462449	61.843668	68.147636
1175.938042	69.378320	68.152641
1174.944187	67.289146	68.157646
1173.880284	53.784254	68.162650
1173.239041	66.063719	68.167655
1172.906626	66.974447	68.172660
1172.703581	54.739326	68.177665
1171.897696	70.172145	68.182670
1171.040705	70.991253	68.187674
1170.265750	73.784322	68.192679
1170.210023	62.262221	68.197684
1169.638525	58.457928	68.202689
1168.321130	62.124178	68.207694
1167.951327	55.636893	68.212698
1167.266937	67.399662	68.217703
1166.384091	67.628358	68.222708
1165.485604	66.063351	68.227713
1164.817521	66.197967	68.232718
1164.448566	53.465674	68.237722
1163.998027	64.831697	68.242727
1163.258559	59.939188	68.247732
1162.322738	57.750903	68.252737
1161.623136	62.127900	68.257742
1161.211259	55.355565	68.262746
1160.791556	61.064758	68.267751
1159.852637	61.728161	68.272756
1159.187365	57.645465	68.277761
1158.666347	61.385344	68.282766
1158.280252	57.233017	68.287770
1156.864816	64.073573	68.292775
1156.314839	55.730443	68.297780
1155.867831	55.566546	68.302785
1155.023766	61.201301	68.307790
1155.131080	58.269942	68.312794
1153.656157	64.489164	68.317799
1152.759121	58.983038	68.322804
1152.680331	58.784235	68.327809
1152.333286	63.278633	68.332814
1151.742763	56.071077	68.337818
1150.364960	61.339700	68.342823
1150.017527	58.345043	68.347828
1149.549119	57.673606	68.352833
1148.327536	56.379193	68.357838
1147.697473	68.683694	68.362842
1147.146971	70.518533	68.367847
1146.663040	65.397725	68.372852
1146.420157	56.991564	68.377857
1145.421748	63.360514	68.382862
1144.449857	58.790412	68.387866
1143.606563	65.849069	68.392871
1143.667982	65.279452	68.397876
1143.260809	56.434210	68.402881
1141.826235	57.674778	68.407886
1141.900076	52.586694	68.412890
1140.801112	61.491662	68.417895
1139.895984	64.016852	68.422900
1139.066330	57.288889	68.427905
1138.258150	60.940398	68.432910
1138.067171	61.595242	68.437914
1137.548212	61.089546	68.442919
1136.872992	62.289771	68.447924
1136.214195	64.105564	68.452929
1135.452014	66.488170	68.457934
1135.193642	52.353702	68.462938
1134.149910	64.709801	68.467943
1133.198655	65.679534	68.472948
1132.763972	56.900172	68.477953
1132.365619	67.075158	68.482958
1131.560463	55.631261	68.487962
1130.466902	62.690300	68.492967
1130.032517	64.665949	68.497972
1129.777153	58.425403	68.502977
1128.573242	62.948851	68.507982
1128.042772	61.905658	68.512986
1126.987629	59.917717	68.517991
1126.929523	56.383451	68.522996
1126.731829	55.421374	68.528001
1125.728914	59.501260	68.533006
1124.979506	56.917479	68.538010
1124.469571	74.523637	68.543015
1123.753485	60.635433	68.548020
1122.669877	60.165930	68.553025
1121.726607	62.832813	68.558030
1121.481837	57.973603	68.563034
1120.916561	56.234188	68.568039
1120.793674	56.969668	68.573044
1119.747536	55.721483	68.578049
1118.596523	60.432067	68.583054
1118.687075	57.364599	68.588058
1117.304063	66.040361	68.593063
1116.365607	57.114044	68.598068
1116.323648	65.805171	68.603073
1115.358789	60.833407	68.608078
1115.355766	61.513552	68.613082
1114.560139	61.272644	68.618087
1113.396881	65.325998	68.623092
1112.970347	63.569248	68.628097
1112.303497	65.943004	68.633102
1111.933005	50.154771	68.638106
1110.790908	62.592753	68.643111
1109.966307	64.635202	68.648116
1109.629933	51.252756	68.653121
1109.045169	56.731158	68.658126
1108.539710	47.745442	68.663130
1107.557669	57.076532	68.668135
1106.646134	51.601120	68.673140
1106.401446	53.497711	68.678145
1105.839263	58.354344	68.683150
1105.425893	49.741919	68.688154
1104.372057	57.222009	68.693159
1103.756992	54.555364	68.698164
1103.384872	48.109467	68.703169
1102.232577	61.181444	68.708174
1101.430582	57.024317	68.713178
1100.954014	55.284990	68.718183
1100.670303	49.801185	68.723188
1100.172632	49.577545	68.728193
1098.712094	53.520489	68.733198
1098.484927	50.027310	68.738202
1097.924403	54.905757	68.743207
1097.171489	59.102009	68.748212
1096.691769	55.320986	68.753217
1095.402500	61.540670	68.758222
1095.172144	57.292619	68.763226
1094.752189	58.704570	68.768231
1093.729735	49.838938	68.773236
1092.915980	53.005634	68.778241
1092.324798	63.960360	68.783246
1092.272111	55.345758	68.788250
1091.275001	52.244713	68.793255
1090.324196	57.320862	68.798260
1089.656935	56.750454	68.803265
1089.295543	57.728881	68.808270
1088.684242	55.675089	68.813274
1087.508093	59.071323	68.818279
1086.990082	49.951987	68.823284
1086.397040	49.465971	68.828289
1085.753474	60.265021	68.833294
1085.813719	49.624955	68.838298
1084.888425	58.995913	68.843303
1083.921398	53.906236	68.848308
1083.426682	45.565384	68.853313
1081.862272	60.456528	68.858318
1081.397833	49.142969	68.863322
1081.106805	44.860419	68.868327
1080.735851	46.062723	68.873332
1080.430904	49.818705	68.878337
1079.605008	57.199466	68.883342
1078.521573	55.739607	68.888346
1077.820729	51.437087	68.893351
1077.320495	49.004503	68.898356
1077.213884	49.377842	68.903361
1076.131114	50.045233	68.908366
1075.448509	47.963364	68.913370
1074.951251	50.977215	68.918375
1073.829669	48.944674	68.923380
1073.135371	51.542004	68.928385
1072.254028	55.979469	68.933390
1072.126839	39.677885	68.938394
1071.629009	50.414323	68.943399
1070.452034	47.196816	68.948404
1069.636483	55.153109	68.953409
1068.568092	50.282996	68.958414
1068.916730	47.699612	68.963418
1068.348466	51.429672	68.968423
1067.714875	44.131226	68.973428
1067.171323	50.203908	68.978433
1066.112968	56.260711	68.983438
1065.664230	48.585922	68.988442
1064.395679	45.595879	68.993447
1063.698308	49.811687	68.998452
1063.636796	48.993537	69.003457
1062.806209	54.307619	69.008462
1062.259475	48.449337	69.013466
1061.222004	52.752365	69.018471
1060.440176	51.955757	69.023476
1060.391637	37.698056	69.028481
1059.705379	49.967334	69.033486
1058.934864	48.821991	69.038490
1057.845524	50.335698	69.043495
1057.585652	48.642336	69.048500
1057.001675	42.066147	69.053505
1056.243438	53.414881	69.058510
1055.596727	47.433731	69.063514
1054.901747	49.958633	69.068519
1054.120590	48.819715	69.073524
1053.450178	48.932653	69.078529
1052.415139	52.757470	69.083534
1052.012438	53.699894	69.088538
1051.620514	51.366782	69.093543
1051.541890	51.003950	69.098548
1050.630080	52.090442	69.103553
1049.763610	57.202075	69.108558
1049.193153	53.806089	69.113562
1048.085479	53.383026	69.118567
1047.440161	57.156889	69.123572
1047.018371	63.429410	69.128577
1046.301762	65.852100	69.133582
1045.304632	61.410637	69.138586
1044.529680	62.137885	69.143591
1043.592026	53.979469	69.148596
1043.230151	56.489232	69.153601
1043.042227	55.196018	69.158606
1043.030386	47.488004	69.163610
1042.179355	59.105401	69.168615
1040.963327	59.505417	69.173620
1040.979584	48.996936	69.178625
1039.367342	58.773660	69.183630
1038.659784	53.134937	69.188634
1038.139599	48.827346	69.193639
1037.522902	55.288570	69.198644
1037.650547	50.002692	69.203649
1036.342419	55.786997	69.208654
1035.742444	54.321211	69.213658
1034.820492	64.095361	69.218663
1034.604420	60.728158	69.223668
1033.581921	56.946764	69.228673
1032.689871	57.476597	69.233678
1032.231834	49.139384	69.238682
1031.821198	49.144768	69.243687
1031.290797	57.248100	69.248692
1030.699643	49.286887	69.253697
1029.708573	55.716205	69.258702
1029.294603	42.764036	69.263706
1028.634844	47.421731	69.268711
1027.290048	49.237871	69.273716
1026.869759	53.948937	69.278721
1026.016188	49.055708	69.283726
1026.011151	52.169460	69.288730
1025.675627	55.830962	69.293735
1024.551083	51.425551	69.298740
1024.005217	43.857692	69.303745
1023.329430	52.953998	69.308750
1022.483114	56.364019	69.313754
1021.523939	51.214773	69.318759
1020.873463	55.530367	69.323764
1020.415368	55.418720	69.328769
1019.721593	51.409991	69.333774
1019.704099	54.136210	69.338778
1018.345616	53.209001	69.343783
1017.536411	63.189150	69.348788
1017.213460	52.800867	69.353793
1016.936708	66.235064	69.358798
1015.701476	52.571436	69.363802
1014.739269	61.405803	69.368807
1014.259281	64.052635	69.373812
1014.312776	58.628737	69.378817
1013.115050	58.380868	69.383822
1012.455884	59.767809	69.388826
1011.738506	58.651874	69.393831
1011.222945	54.947537	69.398836
1010.995185	54.433387	69.403841
1009.611326	51.699842	69.408846
1009.168166	55.108806	69.413850
1008.337615	60.233661	69.418855
1007.954250	59.406792	69.423860
1007.797491	55.697413	69.428865
1006.579714	62.304738	69.433870
1005.615611	57.952659	69.438874
1005.709195	52.667468	69.443879
1005.111852	63.566412	69.448884
1004.540156	54.868810	69.453889
1003.286690	55.954481	69.458894
1002.842126	59.035657	69.463898
1001.894753	57.330253	69.468903
1001.189041	57.879338	69.473908
1000.831839	61.549024	69.478913
1000.227240	65.458349	69.483918
999.635583	62.185599	69.488922
998.650888	56.180964	69.493927
997.716120	60.268977	69.498932
997.430919	61.711543	69.503937
996.784251	63.533325	69.508942
996.051869	56.695324	69.513946
995.576609	59.108013	69.518951
994.761955	56.419535	69.523956
994.138482	64.736383	69.528961
992.800426	64.296380	69.533966
992.376367	61.208283	69.538970
992.063496	56.135996	69.543975
991.361619	61.510048	69.548980
991.486658	60.111851	69.553985
990.249473	60.310250	69.558990
989.788217	50.230992	69.563994
989.248739	57.417968	69.568999
987.750548	53.687047	69.574004
987.316090	52.090858	69.579009
986.451401	51.365806	69.584014
986.075039	58.654566	69.589018
985.689999	60.458379	69.594023
984.938780	58.024745	69.599028
984.166918	58.302079	69.604033
983.497061	58.701958	69.609038
983.299912	58.462067	69.614042
981.972681	55.441977	69.619047
980.843912	56.107265	69.624052
980.606168	54.024030	69.629057
980.311159	59.199304	69.634062
980.193486	58.429517	69.639066
979.315964	51.127329	69.644071
978.057349	54.144060	69.649076
977.799296	49.917782	69.654081
976.730189	52.786087	69.659086
975.929900	52.722587	69.664090
975.634788	53.099114	69.669095
974.676467	58.944488	69.674100
974.572141	52.867601	69.679105
973.779818	55.038998	69.684110
972.920744	54.628454	69.689114
972.396013	54.475378	69.694119
971.761010	61.157153	69.699124
971.053105	49.109643	69.704129
970.292894	52.345126	69.709134
969.538581	53.482283	69.714138
969.070981	45.667016	69.719143
968.185695	51.475536	69.724148
967.365654	47.874853	69.729153
966.627004	56.979596	69.734158
966.162407	48.356434	69.739162
966.005372	49.483714	69.744167
965.125481	55.221991	69.749172
964.330719	47.506090	69.754177
963.397432	48.454101	69.759182
963.000393	56.110435	69.764186
962.711461	53.997499	69.769191
961.838591	52.854279	69.774196
961.519994	50.353395	69.779201
960.494952	59.308163	69.784206
959.788149	51.888931	69.789210
959.094207	44.242149	69.794215
958.214704	52.563463	69.799220
958.170339	50.676547	69.804225
957.009795	56.923117	69.809230
956.309519	52.062294	69.814234
955.604354	55.856737	69.819239
954.816790	57.190004	69.824244
954.415080	65.129366	69.829249
953.755967	51.328376	69.834254
952.998447	51.250193	69.839258
952.423711	52.451823	69.844263
951.762041	52.476662	69.849268
951.926831	50.414538	69.854273
950.522880	54.168781	69.859278
949.749463	47.772578	69.864282
949.469623	51.176063	69.869287
948.309247	52.310028	69.874292
947.496916	45.897941	69.879297
946.650467	58.894489	69.884302
946.258019	50.972648	69.889306
946.191108	52.823617	69.894311
945.760257	50.925658	69.899316
945.022918	45.175011	69.904321
944.169416	51.494155	69.909326
943.061648	51.228851	69.914330
942.085135	43.368413	69.919335
941.123650	55.594772	69.924340
940.786099	48.971518	69.929345
940.289516	52.926743	69.934350
940.215366	53.950948	69.939354
939.796960	42.540225	69.944359
938.933305	50.628783	69.949364
938.374070	50.165808	69.954369
937.578117	53.799656	69.959374
936.550971	50.063202	69.964378
935.578536	47.890295	69.969383
935.179016	46.384753	69.974388
934.789275	44.965966	69.979393
934.192337	50.115166	69.984398
933.211735	46.060642	69.989402
932.500969	44.235614	69.994407
931.750356	50.631430	69.999412
931.485580	47.409190	70.004417
930.892992	50.955484	70.009422
930.050689	47.886647	70.014426
929.507856	44.979895	70.019431
928.684625	50.903133	70.024436
928.151629	46.760039	70.029441
927.190073	62.343815	70.034446
926.753007	51.323997	70.039450
926.490106	42.791759	70.044455
925.166198	60.390229	70.049460
924.609733	50.846545	70.054465
923.687444	53.538541	70.059470
923.049619	54.273967	70.064474
922.978405	47.138394	70.069479
922.411163	58.904626	70.074484
921.430034	48.944387	70.079489
920.818892	52.727029	70.084494
920.407769	46.514465	70.089498
919.367115	45.429500	70.094503
918.317813	47.525109	70.099508
918.152848	49.573034	70.104513
917.509688	54.704362	70.109518
917.312463	53.478873	70.114522
916.326138	49.582965	70.119527
915.439056	54.891884	70.124532
915.053560	45.883983	70.129537
913.964798	50.076951	70.134542
913.257868	53.143119	70.139546
913.170003	45.168089	70.144551
912.339899	61.650330	70.149556
912.014574	45.922788	70.154561
910.738883	57.722909	70.159566
910.114860	49.431068	70.164570
909.666698	58.409169	70.169575
908.624500	56.681044	70.174580
907.903789	51.489168	70.179585
907.253824	53.964366	70.184590
906.810096	51.893418	70.189594
906.559429	41.023727	70.194599
905.826304	49.069442	70.199604
904.463918	46.419275	70.204609
904.050154	49.867730	70.209614
903.905399	49.256801	70.214618
903.195069	47.617796	70.219623
901.941674	53.073323	70.224628
901.437732	49.140081	70.229633
900.648692	51.309399	70.234638
900.293767	58.124813	70.239642
900.069645	51.751602	70.244647
898.544918	55.532977	70.249652
898.000505	48.997846	70.254657
897.737971	52.408043	70.259662
897.209353	51.123328	70.264666
896.802280	54.398828	70.269671
895.495148	55.693369	70.274676
895.417036	47.237385	70.279681
894.706557	49.614980	70.284686
893.532393	48.117603	70.289690
892.918381	45.881366	70.294695
892.447737	57.968124	70.299700
891.828106	40.663138	70.304705
890.698726	53.908149	70.309710
889.872582	45.967033	70.314714
889.721244	44.179147	70.319719
888.835122	43.323497	70.324724
889.003721	47.792623	70.329729
888.189824	52.968475	70.334734
887.231561	49.698907	70.339738
886.719604	35.644301	70.344743
885.301426	48.910038	70.349748
884.836313	52.655255	70.354753
884.037603	42.926210	70.359758
883.731915	42.861298	70.364762
883.694154	43.419233	70.369767
882.535547	55.735326	70.374772
881.704948	46.549106	70.379777
881.281037	48.092607	70.384782
880.951891	45.716419	70.389786
879.734946	50.246774	70.394791
878.856256	44.433491	70.399796
878.492974	45.371244	70.404801
877.708564	48.790378	70.409806
877.512591	49.479150	70.414810
876.346169	47.643075	70.419815
875.442943	62.277697	70.424820
875.038450	48.086130	70.429825
874.689012	46.684594	70.434830
874.213030	49.572087	70.439834
873.427818	41.208143	70.444839
872.396350	55.907325	70.449844
872.167589	49.183191	70.454849
870.915536	51.785758	70.459854
870.106790	46.833416	70.464858
869.996991	48.550859	70.469863
869.080098	46.716076	70.474868
869.030796	51.733977	70.479873
868.126522	53.752907	70.484878
867.549103	45.273889	70.489882
867.005463	47.061956	70.494887
865.726339	53.510361	70.499892
865.132307	42.909795	70.504897
864.458735	54.147315	70.509902
863.994517	47.951098	70.514906
863.783243	38.958065	70.519911
862.207956	44.229866	70.524916
862.156300	40.404429	70.529921
861.579695	46.865607	70.534926
860.597490	50.358804	70.539930
859.632258	47.385252	70.544935
859.256345	50.160626	70.549940
858.600453	44.581555	70.554945
858.535135	47.804244	70.559950
857.559535	53.114651	70.564954
856.781339	46.055336	70.569959
855.960164	52.612213	70.574964
855.777409	43.248780	70.579969
854.340875	51.288185	70.584974
853.472013	55.649610	70.589978
853.477723	53.655378	70.594983
852.739908	51.230694	70.599988
852.400881	57.100545	70.604993
851.405687	59.272726	70.609998
850.482037	57.311289	70.615002
850.124999	43.935366	70.620007
849.360724	52.460724	70.625012
848.932045	52.070032	70.630017
847.451898	54.311514	70.635022
847.027288	54.590393	70.640026
846.776843	49.757362	70.645031
846.455214	52.249702	70.650036
845.903317	43.713013	70.655041
844.711701	53.766672	70.660046
843.973181	55.582607	70.665050
843.619664	57.376689	70.670055
843.106371	63.589677	70.675060
842.258007	53.133671	70.680065
841.379448	54.926163	70.685070
840.961412	57.063259	70.690074
840.292736	52.369335	70.695079
839.191238	57.504243	70.700084
838.630081	46.288159	70.705089
838.063504	45.148274	70.710094
837.586751	53.115352	70.715098
837.266444	46.811080	70.720103
836.050313	54.408555	70.725108
835.429653	35.946258	70.730113
834.669762	44.776851	70.735118
834.512189	54.388382	70.740122
833.689844	46.162828	70.745127
832.386493	52.552025	70.750132
831.964361	40.459096	70.755137
831.825030	52.220301	70.760142
831.318686	52.933245	70.765146
830.411718	53.820344	70.770151
829.445415	58.370755	70.775156
829.422357	42.259235	70.780161
828.488708	50.084566	70.785166
827.327141	48.960537	70.790170
826.846757	47.594043	70.795175
826.160830	51.767083	70.800180
825.867838	50.031711	70.805185
824.891080	46.892848	70.810190
823.802639	48.561054	70.815194
823.501772	44.494582	70.820199
823.232148	50.172033	70.825204
822.802478	43.959290	70.830209
822.168620	45.585103	70.835214
821.607029	51.883048	70.840218
820.598903	43.579837	70.845223
819.246208	47.363835	70.850228
818.714791	46.428096	70.855233
818.344252	49.913837	70.860238
817.865789	52.508416	70.865242
817.612880	45.285079	70.870247
816.453768	52.987027	70.875252
815.777623	50.483152	70.880257
815.355489	44.674495	70.885262
814.143124	56.161791	70.890266
813.363839	43.056521	70.895271
812.728304	53.493195	70.900276
812.635940	48.715434	70.905281
812.295157	48.706580	70.910286
811.146265	53.399601	70.915290
810.402534	50.972719	70.920295
809.719343	57.947624	70.925300
809.600054	53.642511	70.930305
808.276152	53.667141	70.935310
807.382960	55.001495	70.940314
807.252945	48.338926	70.945319
806.274384	56.816401	70.950324
806.164124	50.622204	70.955329
805.158070	50.517393	70.960334
804.411655	55.926959	70.965338
804.161379	48.474542	70.970343
803.167194	51.499726	70.975348
801.930311	55.629583	70.980353
801.485189	42.531053	70.985358
801.078396	52.628538	70.990362
800.977115	48.965545	70.995367
800.182372	59.394451	71.000372
799.397933	48.636552	71.005377
798.573453	53.266900	71.010382
798.112141	60.994981	71.015386
797.380291	46.254719	71.020391
796.129713	47.018327	71.025396
795.481984	46.894329	71.030401
795.358397	47.259343	71.035406
794.964961	51.412640	71.040410
794.260569	47.821997	71.045415
792.920220	54.377953	71.050420
792.361025	42.335238	71.055425
792.088581	51.135560	71.060430
791.443460	48.948457	71.065434
790.814752	42.368430	71.070439
789.876758	44.761766	71.075444
789.514289	33.654433	71.080449
788.932829	39.239591	71.085454
787.923434	44.386662	71.090458
787.443963	44.322616	71.095463
786.841030	44.618852	71.100468
786.147212	41.198421	71.105473
784.838531	46.412058	71.110478
784.212492	50.719079	71.115482
784.244961	34.849477	71.120487
783.321571	42.476061	71.125492
783.303747	39.539391	71.130497
782.265129	46.225516	71.135502
781.297954	43.919370	71.140506
781.095218	35.210428	71.145511
779.705295	38.918367	71.150516
778.939295	36.993367	71.155521
778.464200	36.550152	71.160526
777.897896	37.848248	71.165530
777.929127	31.916973	71.170535
777.026918	42.246282	71.175540
776.278731	44.987884	71.180545
775.934390	44.922830	71.185550
774.677982	41.787505	71.190554
773.859875	40.705024	71.195559
773.300986	45.684188	71.200564
772.635989	46.453939	71.205569
772.280040	39.182361	71.210574
771.567232	47.898238	71.215578
770.907288	34.203130	71.220583
769.892628	48.144281	71.225588
769.715018	41.085590	71.230593
769.079261	46.576895	71.235598
767.862001	54.303889	71.240602
767.461367	45.292127	71.245607
766.664453	48.134530	71.250612
766.353419	45.397503	71.255617
766.012614	49.315339	71.260622
765.106044	47.762809	71.265626
764.429864	45.071295	71.270631
763.886585	44.440237	71.275636
762.477333	47.306003	71.280641
761.952279	48.222216	71.285646
761.323961	48.076213	71.290650
761.130843	37.244705	71.295655
760.477663	45.004903	71.300660
759.631001	41.422728	71.305665
758.756884	41.617059	71.310670
758.306341	45.008307	71.315674
757.957940	46.822085	71.320679
756.590563	54.549326	71.325684
755.863399	50.408799	71.330689
755.637444	48.412026	71.335694
754.956281	44.656846	71.340698
754.875261	38.254575	71.345703
753.617780	47.577569	71.350708
752.951279	41.467203	71.355713
752.588294	42.452235	71.360718
751.909791	46.474296	71.365722
751.247781	47.215191	71.370727
750.362071	47.690495	71.375732
749.861148	48.700642	71.380737
748.904452	46.362877	71.385742
747.556889	45.907173	71.390746
747.454750	40.503339	71.395751
746.767933	48.478634	71.400756
746.364112	38.808212	71.405761
746.177548	42.882846	71.410766
745.096812	48.071252	71.415770
744.218938	37.353491	71.420775
743.738890	47.076278	71.425780
743.535862	43.855274	71.430785
742.477340	41.462759	71.435790
741.365878	49.223381	71.440794
741.247835	36.921219	71.445799
740.454271	41.737472	71.450804
739.923258	40.025814	71.455809
739.068892	39.625640	71.460814
738.211066	44.475780	71.465818
738.139802	35.709645	71.470823
737.142135	44.724770	71.475828
736.244032	46.132470	71.480833
735.921745	43.805677	71.485838
735.159992	45.734151	71.490842
735.007801	31.854144	71.495847
733.950092	41.968520	71.500852
733.178954	43.871680	71.505857
732.409879	42.655247	71.510862
731.759986	38.199651	71.515866
731.008466	38.298778	71.520871
730.444321	42.200132	71.525876
730.055381	42.298307	71.530881
729.847057	39.073418	71.535886
728.534830	46.121671	71.540890
728.046193	34.215988	71.545895
727.012023	44.086919	71.550900
726.548163	44.250639	71.555905
725.723763	48.794259	71.560910
724.842847	45.353170	71.565914
724.437790	40.754515	71.570919
723.828593	42.275498	71.575924
723.985547	34.939621	71.580929
723.226019	39.176439	71.585934
722.018952	47.565732	71.590938
721.490359	37.336431	71.595943
720.102952	49.294754	71.600948
719.228180	45.278669	71.605953
718.878644	45.239682	71.610958
718.339752	43.811562	71.615962
718.066758	38.781868	71.620967
717.786109	51.549598	71.625972
717.318199	39.296833	71.630977
716.490165	45.709752	71.635982
715.284224	47.521292	71.640986
714.992095	43.593798	71.645991
713.748917	50.388212	71.650996
713.332196	41.812697	71.656001
712.623219	37.120505	71.661006
712.243047	59.966786	71.666010
711.272902	34.383355	71.671015
710.512483	53.093829	71.676020
710.230607	41.705593	71.681025
709.773770	44.952768	71.686030
708.534726	46.175059	71.691034
708.143326	38.934371	71.696039
707.299606	48.737141	71.701044
707.055037	47.167544	71.706049
705.998213	44.483034	71.711054
704.868594	43.620487	71.716058
704.865044	27.753486	71.721063
704.199984	36.554808	71.726068
703.789690	37.503223	71.731073
703.298246	38.664835	71.736078
702.036477	53.329760	71.741082
701.605526	44.051603	71.746087
700.526441	46.645634	71.751092
699.769544	40.270554	71.756097
699.404716	51.697062	71.761102
698.633933	42.195466	71.766106
698.259754	40.520348	71.771111
697.828965	51.471649	71.776116
697.076111	47.051377	71.781121
696.405534	45.672614	71.786126
695.725224	46.028501	71.791130
694.687875	44.962029	71.796135
693.787138	38.999368	71.801140
693.225278	42.766322	71.806145
693.129703	44.216572	71.811150
692.540492	46.658490	71.816154
691.394721	35.723208	71.821159
690.480381	42.345420	71.826164
689.847289	46.204143	71.831169
689.723473	42.100042	71.836174
689.389165	39.555971	71.841178
688.604240	41.648999	71.846183
687.320717	41.747689	71.851188
686.893200	25.478260	71.856193
686.782014	38.192186	71.861198
685.679785	45.035131	71.866202
684.904502	42.466655	71.871207
684.531065	47.162413	71.876212
683.946499	43.860238	71.881217
682.881565	38.237545	71.886222
681.879364	47.284950	71.891226
681.587430	41.308936	71.896231
681.066186	44.353478	71.901236
680.312860	35.829995	71.906241
679.350604	38.925832	71.911246
678.735323	41.288323	71.916250
678.414122	30.702738	71.921255
677.964092	39.288476	71.926260
677.141705	36.880471	71.931265
676.492902	36.745637	71.936270
675.633854	46.511428	71.941274
675.578687	36.339227	71.946279
674.785481	46.760020	71.951284
673.586164	42.185339	71.956289
673.346559	34.422167	71.961294
672.097971	37.584100	71.966298
671.135473	42.373654	71.971303
670.570138	44.106865	71.976308
670.315350	41.384552	71.981313
670.169616	32.089381	71.986318
669.513150	42.376434	71.991322
668.931386	34.924791	71.996327
668.044990	37.237412	72.001332
667.338244	32.615845	72.006337
666.049176	33.358836	72.011342
665.270785	46.204239	72.016346
665.008725	35.921478	72.021351
664.571438	43.858630	72.026356
664.214436	46.044378	72.031361
663.449152	40.905421	72.036366
662.228449	41.613873	72.041370
661.989731	38.116284	72.046375
661.323725	48.661908	72.051380
660.466841	44.754964	72.056385
659.811003	45.482284	72.061390
659.043052	59.294301	72.066394
658.628824	47.815181	72.071399
658.130171	46.506825	72.076404
656.922882	45.554164	72.081409
656.527256	45.560373	72.086414
655.483674	43.849926	72.091418
655.387043	38.883624	72.096423
654.903439	47.017392	72.101428
653.780007	42.990465	72.106433
653.374371	46.402963	72.111438
652.575856	47.706523	72.116442
652.309158	37.672088	72.121447
650.903403	50.590588	72.126452
650.643515	51.313208	72.131457
649.884036	43.068261	72.136462
649.559127	47.500825	72.141466
648.878242	37.302106	72.146471
647.922943	50.637740	72.151476
647.379721	48.134826	72.156481
646.801449	41.111569	72.161486
645.437120	51.454580	72.166490
645.448957	40.786000	72.171495
644.600755	47.421351	72.176500
644.214087	51.877944	72.181505
643.820461	47.050398	72.186510
642.455981	45.892536	72.191514
642.174645	49.392477	72.196519
641.721858	46.842047	72.201524
640.661687	54.324877	72.206529
640.396611	42.489273	72.211534
639.304143	51.212018	72.216538
638.787433	42.050039	72.221543
637.925191	43.996120	72.226548
636.998254	45.452601	72.231553
636.583891	41.714899	72.236558
635.990005	52.223813	72.241562
635.775713	42.766091	72.246567
634.670991	44.086879	72.251572
633.886812	44.899299	72.256577
633.461251	43.891551	72.261582
632.878791	49.498977	72.266586
632.563959	35.004636	72.271591
631.223538	41.554365	72.276596
630.648116	44.568119	72.281601
630.598093	39.643283	72.286606
629.337774	54.967180	72.291610
628.754143	43.789443	72.296615
628.035809	49.596706	72.301620
627.870564	55.065154	72.306625
627.365510	48.134320	72.311630
626.031396	46.443345	72.316634
625.757171	40.458213	72.321639
625.097877	39.236949	72.326644
623.452241	47.390188	72.331649
622.940401	45.191371	72.336654
621.973114	49.079675	72.341658
621.998936	39.525372	72.346663
621.850968	48.564495	72.351668
621.556141	52.123358	72.356673
620.801438	44.322368	72.361678
619.892212	51.334881	72.366682
619.342275	43.685789	72.371687
618.216728	49.497978	72.376692
617.220950	51.998350	72.381697
616.756019	41.333158	72.386702
616.279895	52.585001	72.391706
615.575267	45.157667	72.396711
614.825116	42.899031	72.401716
613.598093	42.684405	72.406721
613.297352	47.177779	72.411726
612.654009	53.473006	72.416730
612.898915	45.266820	72.421735
612.314982	50.141190	72.426740
611.290427	47.986179	72.431745
611.004251	40.329781	72.436750
609.365589	48.701118	72.441754
608.730146	49.250159	72.446759
608.109679	44.458747	72.451764
607.367597	43.045665	72.456769
607.230655	43.455392	72.461774
606.519143	55.821800	72.466778
605.690549	47.975810	72.471783
605.046167	47.846598	72.476788
604.701315	52.298113	72.481793
603.879793	51.719288	72.486798
602.533177	51.350245	72.491802
602.383699	44.124670	72.496807
602.339449	41.001401	72.501812
600.981405	49.916265	72.506817
600.421123	47.526468	72.511822
599.336728	55.024208	72.516826
599.037493	51.706576	72.521831
598.692943	55.104623	72.526836
597.911044	45.958080	72.531841
597.358554	46.027127	72.536846
596.447261	46.493944	72.541850
595.915331	49.489740	72.546855
594.819170	51.329585	72.551860
593.991671	48.126048	72.556865
593.862904	55.992000	72.561870
593.153842	61.651139	72.566874
592.829120	58.567804	72.571879
591.822155	55.995254	72.576884
591.071793	54.253906	72.581889
590.786579	47.062563	72.586894
589.878125	56.301655	72.591898
588.842479	48.904970	72.596903
588.649291	54.041972	72.601908
587.735006	59.128236	72.606913
587.783788	46.367434	72.611918
586.290306	53.212806	72.616922
585.839921	54.733760	72.621927
585.188924	59.812787	72.626932
584.723514	61.807652	72.631937
584.070183	59.281286	72.636942
582.796280	56.804871	72.641946
582.321616	49.916518	72.646951
581.839485	54.962342	72.651956
581.113224	61.381173	72.656961
581.116184	50.532655	72.661966
580.017195	59.932986	72.666970
579.437952	48.000770	72.671975
578.845094	50.506372	72.676980
577.532138	56.488777	72.681985
577.209251	51.918064	72.686990
576.369454	61.316541	72.691994
576.131667	49.821959	72.696999
575.922016	60.110416	72.702004
574.564868	59.389823	72.707009
573.922680	56.156777	72.712014
573.178161	54.999563	72.717018
572.772321	46.072261	72.722023
572.191956	59.420746	72.727028
571.091676	54.781457	72.732033
571.003720	47.911943	72.737038
570.143163	44.849301	72.742042
569.200436	47.386973	72.747047
568.692851	45.859283	72.752052
568.073552	50.718793	72.757057
567.971891	48.516161	72.762062
566.418408	50.603899	72.767066
565.578322	50.628871	72.772071
565.237085	46.037430	72.777076
564.396390	56.286040	72.782081
564.308016	50.675021	72.787086
564.014098	55.518980	72.792090
562.962330	51.791346	72.797095
562.352344	58.062348	72.802100
561.253293	47.345200	72.807105
560.494856	49.419855	72.812110
559.603991	55.841250	72.817114
559.385114	47.324149	72.822119
559.065844	44.769818	72.827124
558.465821	50.834224	72.832129
557.612833	55.000818	72.837134
556.548948	62.892709	72.842138
556.385840	50.388009	72.847143
556.087557	59.394307	72.852148
554.526552	50.789770	72.857153
554.018975	44.997938	72.862158
553.293437	44.968399	72.867162
553.423767	51.679734	72.872167
552.331613	49.198042	72.877172
551.207799	47.019443	72.882177
551.035830	42.997142	72.887182
550.309609	50.838400	72.892186
550.023629	42.461304	72.897191
549.105650	41.147221	72.902196
548.705854	43.606307	72.907201
547.925986	40.485090	72.912206
546.764542	49.554747	72.917210
546.343951	49.473485	72.922215
545.651941	47.623509	72.927220
544.367506	53.595078	72.932225
543.801095	44.742246	72.937230
543.127440	44.202968	72.942234
542.937572	47.500686	72.947239
542.491658	45.557896	72.952244
542.014745	47.862108	72.957249
541.234321	45.641434	72.962254
540.111420	50.885520	72.967258
539.789548	49.866004	72.972263
539.375852	50.515362	72.977268
538.080022	54.027089	72.982273
537.828430	54.885596	72.987278
536.888202	55.208808	72.992282
536.568988	43.981103	72.997287
535.539216	47.489876	73.002292
534.449489	54.550089	73.007297
534.507715	42.316079	73.012302
533.754794	55.450772	73.017306
533.115706	40.380466	73.022311
532.305603	41.720602	73.027316
531.415803	52.376013	73.032321
531.134717	40.360059	73.037326
530.601796	44.001007	73.042330
529.864168	49.473891	73.047335
528.896070	51.246056	73.052340
528.266547	58.865336	73.057345
528.126974	42.949053	73.062350
527.337578	53.823443	73.067354
526.629813	46.270482	73.072359
525.727476	41.306372	73.077364
525.025897	55.968863	73.082369
524.678739	45.642910	73.087374
523.111721	54.121160	73.092378
522.803253	50.806587	73.097383
522.403749	46.126663	73.102388
521.802177	50.445610	73.107393
521.925364	46.882505	73.112398
520.622853	51.480264	73.117402
520.120168	45.276070	73.122407
519.411114	52.116376	73.127412
518.224630	53.055994	73.132417
517.483600	52.642574	73.137422
516.809437	52.448742	73.142426
516.746281	47.680548	73.147431
516.282444	47.021122	73.152436
514.869104	57.425617	73.157441
514.476332	45.678192	73.162446
514.235799	56.463579	73.167450
513.682290	48.681044	73.172455
512.443341	50.568899	73.177460
511.529498	50.798030	73.182465
511.258342	47.322973	73.187470
510.555052	54.165517	73.192474
509.747055	54.992808	73.197479
509.017667	49.389286	73.202484
508.482420	50.493256	73.207489
508.129848	42.863224	73.212494
507.716996	48.568234	73.217498
506.633905	52.716303	73.222503
506.126711	50.947286	73.227508
505.092364	46.876279	73.232513
505.256163	44.279699	73.237518
504.038520	53.616951	73.242522
503.257116	46.400586	73.247527
502.981345	43.752602	73.252532
501.596640	45.641602	73.257537
501.024997	35.699934	73.262542
500.390850	51.137014	73.267546
499.986122	50.758338	73.272551
499.686973	50.116836	73.277556
499.085670	49.843592	73.282561
498.235478	46.616897	73.287566
497.482657	52.469108	73.292570
496.752910	52.460757	73.297575
495.723047	48.512044	73.302580
494.913012	46.370220	73.307585
494.663801	36.312534	73.312590
494.365771	44.514527	73.317594
493.741137	41.870077	73.322599
492.778550	41.865702	73.327604
491.994709	47.104680	73.332609
491.586310	46.754976	73.337614
491.157357	42.888739	73.342618
489.968195	43.923415	73.347623
489.526552	47.530906	73.352628
488.737043	37.865224	73.357633
488.612205	43.634742	73.362638
487.517098	42.077659	73.367642
486.672291	41.939405	73.372647
486.172514	38.328884	73.377652
485.410537	43.919198	73.382657
484.455306	36.572840	73.387662
483.680390	45.689754	73.392666
482.917873	38.501932	73.397671
482.661740	42.060947	73.402676
482.224951	47.014402	73.407681
482.275371	39.771193	73.412686
481.226203	55.334319	73.417690
480.127932	46.282380	73.422695
479.992412	39.776854	73.427700
478.647323	43.884666	73.432705
477.917034	32.470156	73.437710
477.384409	39.687640	73.442714
476.710350	39.635730	73.447719
476.412621	41.250655	73.452724
475.544556	48.606739	73.457729
474.711197	34.330669	73.462734
474.102279	45.761368	73.467738
473.753308	47.665159	73.472743
473.374270	39.425909	73.477748
472.046551	47.017648	73.482753
471.565460	30.648013	73.487758
470.875840	39.983152	73.492762
470.597530	40.043241	73.497767
469.759688	46.221242	73.502772
468.514856	50.814567	73.507777
468.500657	34.408396	73.512782
468.183421	48.279517	73.517786
466.874597	39.696377	73.522791
466.320911	38.661763	73.527796
465.415342	46.624650	73.532801
465.052474	39.292740	73.537806
464.298515	44.050718	73.542810
463.643792	43.265592	73.547815
462.796070	37.867025	73.552820
462.583905	46.648283	73.557825
462.114257	38.363547	73.562830
460.786213	44.756842	73.567834
460.394358	37.427975	73.572839
459.810881	38.873957	73.577844
459.293455	40.493921	73.582849
458.810373	43.299030	73.587854
458.072461	46.072197	73.592858
457.246936	36.797049	73.597863
456.163604	36.343564	73.602868
455.316950	45.486105	73.607873
454.886323	35.665491	73.612878
454.406666	40.729857	73.617882
453.863217	39.113288	73.622887
453.503027	32.722411	73.627892
452.478241	45.088279	73.632897
451.970187	37.500380	73.637902
451.588395	40.333507	73.642906
450.373904	40.044425	73.647911
449.905424	41.811137	73.652916
449.186699	33.531396	73.657921
448.696476	37.309059	73.662926
447.366948	47.384830	73.667930
446.946300	41.664335	73.672935
446.458405	45.022154	73.677940
445.974593	41.576257	73.682945
445.431780	39.046521	73.687950
444.472725	46.579537	73.692954
443.502515	43.799344	73.697959
443.356909	36.546369	73.702964
442.806763	46.381275	73.707969
441.900082	37.079638	73.712974
440.856540	40.871340	73.717978
440.160941	31.654352	73.722983
440.153550	33.401220	73.727988
439.559826	39.365289	73.732993
438.804795	29.254165	73.737998
437.901183	38.237045	73.743002
437.333068	43.774406	73.748007
436.785855	30.020481	73.753012
435.571406	41.623351	73.758017
435.080098	39.075950	73.763022
434.957025	38.530984	73.768026
433.977562	36.261634	73.773031
433.428018	32.865639	73.778036
432.345942	46.262520	73.783041
431.914955	38.335914	73.788046
431.338757	43.164927	73.793050
430.817114	43.913503	73.798055
429.988400	44.051828	73.803060
428.980172	41.493745	73.808065
428.761472	43.548675	73.813070
428.044138	49.415748	73.818074
427.275091	49.500412	73.823079
426.662882	39.011712	73.828084
425.665085	47.288930	73.833089
425.855813	34.682163	73.838094
425.036739	40.057658	73.843098
423.852012	51.327795	73.848103
423.633716	41.028649	73.853108
422.923124	49.094526	73.858113
422.007068	43.681630	73.863118
421.029680	54.494529	73.868122
420.018171	56.388770	73.873127
420.264023	40.672883	73.878132
419.606145	51.792846	73.883137
419.118699	48.429535	73.888142
418.106183	50.014849	73.893146
417.664491	44.767651	73.898151
416.986962	38.663888	73.903156
416.292835	49.672929	73.908161
415.245657	40.090910	73.913166
414.777580	52.563638	73.918170
414.191863	49.654385	73.923175
413.876888	42.962991	73.928180
412.851224	45.969678	73.933185
412.401294	37.145644	73.938190
411.848392	43.300336	73.943194
410.631260	46.928896	73.948199
410.191190	40.497135	73.953204
409.309591	51.671670	73.958209
409.001395	39.056085	73.963214
408.237567	43.768339	73.968218
407.111748	43.944550	73.973223
407.084854	40.604057	73.978228
406.255449	45.099677	73.983233
405.943602	47.924821	73.988238
404.824920	51.542429	73.993242
403.939507	41.948833	73.998247
403.705639	44.777321	74.003252
403.060524	37.916181	74.008257
402.832726	42.684955	74.013262
401.824660	43.277650	74.018266
400.964439	42.553671	74.023271
400.122288	37.964806	74.028276
399.051783	45.977646	74.033281
398.630796	46.565109	74.038286
398.310811	44.427238	74.043290
398.062108	37.583363	74.048295
397.777678	38.481808	74.053300
396.244986	41.676523	74.058305
395.692524	40.457224	74.063310
395.317544	39.390997	74.068314
393.831880	38.172160	74.073319
393.446901	34.327325	74.078324
392.505626	45.159702	74.083329
392.431028	39.262654	74.088334
391.711937	44.986509	74.093338
391.126252	40.323665	74.098343
390.201085	37.906908	74.103348
389.361528	45.569134	74.108353
389.377468	45.989205	74.113358
388.753109	40.561384	74.118362
387.684214	43.795745	74.123367
387.112859	35.383734	74.128372
386.276945	50.543886	74.133377
386.163981	35.366159	74.138382
384.879712	35.922447	74.143386
384.459951	32.244007	74.148391
384.181912	32.160559	74.153396
382.944477	39.711139	74.158401
381.953222	41.031302	74.163406
381.485083	44.490063	74.168410
381.085583	36.105863	74.173415
380.969968	39.795459	74.178420
379.916563	46.245955	74.183425
378.918803	39.519865	74.188430
378.468797	40.876786	74.193434
377.777181	44.044725	74.198439
377.520032	40.160598	74.203444
376.248181	42.433811	74.208449
375.768647	39.067675	74.213454
374.961589	39.677237	74.218458
374.479242	47.383474	74.223463
374.415068	39.933025	74.228468
373.031521	42.652974	74.233473
372.669877	32.606925	74.238478
372.332507	34.639766	74.243482
371.302963	41.523282	74.248487
370.391236	38.118784	74.253492
369.512785	43.052742	74.258497
368.958762	41.272296	74.263502
368.959726	48.918865	74.268506
367.886459	46.642411	74.273511
367.408879	34.796587	74.278516
366.761132	43.934261	74.283521
366.195929	40.558124	74.288526
365.000475	42.875939	74.293530
364.222363	43.010954	74.298535
364.155429	34.182675	74.303540
363.248130	32.799152	74.308545
362.943268	32.608015	74.313550
362.017696	42.226782	74.318554
361.138570	45.792040	74.323559
361.184752	35.632117	74.328564
359.413366	46.161541	74.333569
358.848220	43.364145	74.338574
358.520736	41.599642	74.343578
358.083039	44.195682	74.348583
357.958043	39.867871	74.353588
356.866513	44.988756	74.358593
355.902806	43.811345	74.363598
355.487969	42.084417	74.368602
354.906829	45.611653	74.373607
354.059604	41.722212	74.378612
352.961685	45.440612	74.383617
352.704169	39.711490	74.388622
352.210028	40.671744	74.393626
351.451088	39.695097	74.398631
350.516664	34.398704	74.403636
349.723206	50.490395	74.408641
349.535443	39.252832	74.413646
349.345279	37.835458	74.418650
348.385460	37.649347	74.423655
347.549666	34.433033	74.428660
346.800614	44.482574	74.433665
346.367334	31.787597	74.438670
345.126387	42.704010	74.443674
344.296030	45.499824	74.448679
344.180090	36.745589	74.453684
343.884417	33.826407	74.458689
342.972677	35.047179	74.463694
341.949312	35.375827	74.468698
341.170582	40.975154	74.473703
341.155816	31.646551	74.478708
340.110570	45.982194	74.483713
339.535995	35.334565	74.488718
338.662839	43.675524	74.493722
337.923812	46.646022	74.498727
337.733937	43.579090	74.503732
336.916396	43.718820	74.508737
335.996191	32.487601	74.513742
335.288089	36.847212	74.518746
334.909886	42.152473	74.523751
334.755819	31.207597	74.528756
333.282812	47.051187	74.533761
332.719810	34.369000	74.538766
332.157042	36.791007	74.543770
331.728344	44.428772	74.548775
331.544312	36.849195	74.553780
330.543943	37.705623	74.558785
330.009292	36.489810	74.563790
328.925261	41.715166	74.568794
327.602533	42.007950	74.573799
327.337798	38.634402	74.578804
326.753961	42.720320	74.583809
326.421818	32.677466	74.588814
326.163568	41.737302	74.593818
325.126293	41.077837	74.598823
324.333590	40.174389	74.603828
323.930200	42.884816	74.608833
323.032156	39.629545	74.613838
322.155643	43.325287	74.618842
321.528516	47.507995	74.623847
321.353627	38.460377	74.628852
320.363547	43.623455	74.633857
319.381881	36.047996	74.638862
318.620938	38.383317	74.643866
318.164586	37.910397	74.648871
318.343718	37.093345	74.653876
317.334993	47.665254	74.658881
316.421222	37.396546	74.663886
315.961029	35.955978	74.668890
315.355508	41.444127	74.673895
314.168692	41.857185	74.678900
313.295511	48.007744	74.683905
313.123507	43.879819	74.688910
312.495451	37.787130	74.693914
311.678185	47.629930	74.698919
311.157823	44.038500	74.703924
310.030533	48.274114	74.708929
309.871543	44.215078	74.713934
309.637836	43.332933	74.718938
308.483084	37.273725	74.723943
307.693054	44.210556	74.728948
307.298597	50.150779	74.733953
306.648173	46.466536	74.738958
305.959998	39.407285	74.743962
305.059484	51.818050	74.748967
304.562780	42.708180	74.753972
303.669951	48.434515	74.758977
303.497634	41.089619	74.763982
302.653513	44.108415	74.768986
301.794355	45.812837	74.773991
301.504625	41.448207	74.778996
300.208340	45.346478	74.784001
299.533070	47.835311	74.789006
299.310681	34.777147	74.794010
298.337188	36.064548	74.799015
298.367423	38.295855	74.804020
297.025134	48.898857	74.809025
296.562441	48.873234	74.814030
295.968446	41.970864	74.819034
295.174052	50.685644	74.824039
295.027662	39.922474	74.829044
293.775667	44.796142	74.834049
293.344085	48.949266	74.839054
293.076938	45.005242	74.844058
291.685345	45.715880	74.849063
291.102526	42.927626	74.854068
290.461443	44.983653	74.859073
289.824369	41.589028	74.864078
289.779443	42.122879	74.869082
288.623166	54.080821	74.874087
287.633670	43.267521	74.879092
287.286554	44.314743	74.884097
286.584026	44.319462	74.889102
286.311782	51.826642	74.894106
285.417127	46.903985	74.899111
284.677952	43.118776	74.904116
284.132773	43.912134	74.909121
283.476149	42.991742	74.914126
282.724297	41.742747	74.919130
281.640164	44.601106	74.924135
281.448769	33.450873	74.929140
280.990905	37.313291	74.934145
280.202844	37.181833	74.939150
279.311459	36.634754	74.944154
278.678986	31.293421	74.949159
278.530384	31.943146	74.954164
277.436269	48.122189	74.959169
276.927538	35.141209	74.964174
276.228655	32.177493	74.969178
275.587835	48.154976	74.974183
274.741001	35.153769	74.979188
273.890087	39.465194	74.984193
273.426096	32.256684	74.989198
273.031267	38.291582	74.994202
271.884315	41.279807	74.999207
271.324216	39.419928	75.004212
270.494474	40.111987	75.009217
270.087074	39.252800	75.014222
269.792972	36.670850	75.019226
269.113799	40.975404	75.024231
268.461156	32.278342	75.029236
267.648046	37.458961	75.034241
266.862843	34.349733	75.039246
266.239421	39.481194	75.044250
265.376701	43.223642	75.049255
265.203005	34.336698	75.054260
264.304637	39.576640	75.059265
263.118801	41.033520	75.064270
262.695322	31.818957	75.069274
261.994635	42.822756	75.074279
261.741138	37.446251	75.079284
261.088059	44.913204	75.084289
260.217926	39.545100	75.089294
259.727896	38.492503	75.094298
259.225069	48.181114	75.099303
258.763007	33.800237	75.104308
257.615689	38.143143	75.109313
256.824994	41.590257	75.114318
256.710346	34.084790	75.119322
255.235217	37.730888	75.124327
254.532384	37.831860	75.129332
253.896513	39.667865	75.134337
253.439866	38.736106	75.139342
253.134911	33.498695	75.144346
252.798565	38.133386	75.149351
251.935733	31.669707	75.154356
250.756825	42.565229	75.159361
250.151480	42.045107	75.164366
250.103904	38.580185	75.169370
248.798483	51.501786	75.174375
248.136060	36.764912	75.179380
247.694210	41.247687	75.184385
247.427793	38.188236	75.189390
246.133161	36.655184	75.194394
245.188621	46.551402	75.199399
245.038152	37.111971	75.204404
244.446775	43.886264	75.209409
244.243676	35.724685	75.214414
243.454362	42.757612	75.219418
242.744478	45.600486	75.224423
242.082073	34.589996	75.229428
240.679062	43.505879	75.234433
239.923052	37.794736	75.239438
239.493110	38.484578	75.244442
239.420957	38.901343	75.249447
238.938283	38.557214	75.254452
237.722474	38.809348	75.259457
237.010999	40.401939	75.264462
236.510175	39.150792	75.269466
235.982423	36.691248	75.274471
235.390072	38.206503	75.279476
234.025366	39.848030	75.284481
233.311214	35.640955	75.289486
233.556842	33.985389	75.294490
232.754731	48.145110	75.299495
232.115749	31.371797	75.304500
231.071627	44.027816	75.309505
230.708628	45.265236	75.314510
230.040240	28.581772	75.319514
228.816873	39.790319	75.324519
228.340689	39.552391	75.329524
227.665215	43.507855	75.334529
227.568665	40.126435	75.339534
226.995632	37.137942	75.344538
225.464044	40.949176	75.349543
225.257776	32.072164	75.354548
224.555524	42.029110	75.359553
224.305487	36.461247	75.364558
223.445147	36.382330	75.369562
222.491395	39.469089	75.374567
222.460898	43.499936	75.379572
221.222545	52.807482	75.384577
220.759722	38.543431	75.389582
220.056556	38.802164	75.394586
219.111099	46.653205	75.399591
218.667703	40.029633	75.404596
217.475635	43.502895	75.409601
217.166253	45.096050	75.414606
216.878339	42.579353	75.419610
216.235566	39.078426	75.424615
215.508657	38.282798	75.429620
214.685712	40.929234	75.434625
214.092081	48.230601	75.439630
213.599853	34.083209	75.444634
212.433234	44.774935	75.449639
212.194958	36.245227	75.454644
211.493304	41.691950	75.459649
210.784401	32.183853	75.464654
209.929786	34.679219	75.469658
208.741734	42.065881	75.474663
208.660325	38.000799	75.479668
207.959967	36.570153	75.484673
207.543783	38.186642	75.489678
207.495204	35.029392	75.494682
205.989398	38.406015	75.499687
205.732813	29.223212	75.504692
204.543965	35.400465	75.509697
203.268367	42.091450	75.514702
203.074271	33.354428	75.519706
202.248837	42.356449	75.524711
202.171979	35.108318	75.529716
201.736035	41.985573	75.534721
201.587832	34.129067	75.539726
200.661879	37.329675	75.544730
199.963241	38.295750	75.549735
198.847600	37.393363	75.554740
197.540041	34.533015	75.559745
197.424217	48.036125	75.564750
196.911356	40.538952	75.569754
196.424734	41.463344	75.574759
195.818006	29.201349	75.579764
194.623729	40.029952	75.584769
193.973591	35.497292	75.589774
193.615179	31.170441	75.594778
193.111669	40.408150	75.599783
192.079392	36.803744	75.604788
191.265520	38.270745	75.609793
190.693893	34.619711	75.614798
190.441919	38.258506	75.619802
189.902365	36.660303	75.624807
189.027632	34.016388	75.629812
188.338060	39.864893	75.634817
187.768419	40.635363	75.639822
187.032516	40.110839	75.644826
186.353970	39.151390	75.649831
185.634176	38.934962	75.654836
185.277597	36.804536	75.659841
183.935046	32.814357	75.664846
183.616294	37.605523	75.669850
182.922951	36.858171	75.674855
182.630265	31.800169	75.679860
181.343130	31.579572	75.684865
180.620523	38.136673	75.689870
180.331952	29.321677	75.694874
179.598807	35.796877	75.699879
179.685765	37.263769	75.704884
178.734563	41.893990	75.709889
177.610004	37.477971	75.714894
177.384495	38.106846	75.719898
176.016063	41.338582	75.724903
175.500354	37.044695	75.729908
174.693731	42.500276	75.734913
174.148496	39.724986	75.739918
174.158151	40.981850	75.744922
173.359669	40.289110	75.749927
172.242512	40.781017	75.754932
171.644872	34.675642	75.759937
171.242573	38.888766	75.764942
170.897979	40.886512	75.769946
169.357502	39.365890	75.774951
168.749258	40.700765	75.779956
168.257088	36.600249	75.784961
167.822888	31.118529	75.789966
167.664157	38.036745	75.794970
165.984564	47.286923	75.799975
165.953187	32.909955	75.804980
165.625191	36.950382	75.809985
164.650096	40.881089	75.814990
163.934038	33.944610	75.819994
163.021243	39.827132	75.824999
162.698997	28.991105	75.830004
161.721734	32.534223	75.835009
160.669526	31.088725	75.840014
160.746284	35.641791	75.845018
159.930850	42.231044	75.850023
159.835071	35.285559	75.855028
158.029565	36.641010	75.860033
157.322072	42.713155	75.865038
157.128021	37.715124	75.870042
156.824585	37.918028	75.875047
156.344723	31.287674	75.880052
155.274766	25.926246	75.885057
154.448596	29.073111	75.890062
154.391992	28.225825	75.895066
153.227374	40.358598	75.900071
152.354746	29.944642	75.905076
151.798774	39.870392	75.910081
151.177413	40.207565	75.915086
151.152894	33.968241	75.920090
149.558089	36.073857	75.925095
149.182513	38.175894	75.930100
148.690024	39.605860	75.935105
148.263982	35.442766	75.940110
147.144179	30.379450	75.945114
146.133647	46.221921	75.950119
145.691561	40.448144	75.955124
145.586860	38.394261	75.960129
144.908430	35.104047	75.965134
143.892529	34.411290	75.970138
143.157726	38.756281	75.975143
142.591541	32.108154	75.980148
142.153112	44.273384	75.985153
141.582349	45.802565	75.990158
141.002659	38.636190	75.995162
140.559058	41.357784	76.000167
139.802507	40.406055	76.005172
138.579262	44.012058	76.010177
137.719469	38.990866	76.015182
137.558083	45.045330	76.020186
136.793561	36.440269	76.025191
135.690898	37.655287	76.030196
135.202673	42.575983	76.035201
134.816251	36.477942	76.040206
134.489472	31.379652	76.045210
133.554829	34.859214	76.050215
132.478672	32.991766	76.055220
132.001804	35.538891	76.060225
131.745940	41.531146	76.065230
131.117128	28.604063	76.070234
129.697657	41.969667	76.075239
129.639098	36.694568	76.080244
129.049801	42.927648	76.085249
128.041584	39.415629	76.090254
127.219235	34.554054	76.095258
126.530147	38.910684	76.100263
126.143297	43.375244	76.105268
126.155769	41.592840	76.110273
125.010968	43.819110	76.115278
124.227317	29.737146	76.120282
123.500730	32.907567	76.125287
123.129566	33.372012	76.130292
121.882687	37.213603	76.135297
121.265706	39.764148	76.140302
120.961891	34.488732	76.145306
120.399680	42.950480	76.150311
120.029069	31.478771	76.155316
118.852926	35.592939	76.160321
118.096490	46.995164	76.165326
117.818224	35.119217	76.170330
116.346481	45.183111	76.175335
115.539053	38.810002	76.180340
115.302151	32.167726	76.185345
114.479378	39.177633	76.190350
114.536789	31.031311	76.195354
113.966777	39.005442	76.200359
113.565622	26.929899	76.205364
112.109551	30.599845	76.210369
111.670449	35.290356	76.215374
111.656263	33.158964	76.220378
110.073383	32.715902	76.225383
109.511240	34.969120	76.230388
109.058938	37.452407	76.235393
108.702994	40.839701	76.240398
107.826599	34.103853	76.245402
106.706571	33.594874	76.250407
106.403674	38.088625	76.255412
105.919835	40.228432	76.260417
105.026405	38.346052	76.265422
104.155879	31.394803	76.270426
103.533612	43.311802	76.275431
103.185950	39.109409	76.280436
102.753563	39.840665	76.285441
101.562334	42.353473	76.290446
100.911033	41.496937	76.295450
100.537618	41.763047	76.300455
99.904890	42.398515	76.305460
98.983154	36.559309	76.310465
98.371563	43.444083	76.315470
97.824378	34.217752	76.320474
96.789925	39.952536	76.325479
96.780523	41.683950	76.330484
95.924946	39.320870	76.335489
95.576036	45.679629	76.340494
94.894151	36.897404	76.345498
93.551912	44.906371	76.350503
92.880346	36.549859	76.355508
92.246455	37.767416	76.360513
91.590291	41.879105	76.365518
91.609819	33.104884	76.370522
90.302136	40.646289	76.375527
89.981897	35.677852	76.380532
89.264500	35.076290	76.385537
88.722549	38.956876	76.390542
87.804194	34.282515	76.395546
87.220909	42.790206	76.400551
86.841688	35.864697	76.405556
86.054430	41.164248	76.410561
84.951987	52.545965	76.415566
84.716790	37.231673	76.420570
84.069933	42.108286	76.425575
83.276673	39.247991	76.430580
82.160003	37.661419	76.435585
81.619131	33.780004	76.440590
81.322188	34.275197	76.445594
80.811186	41.915069	76.450599
80.170638	34.791536	76.455604
79.389301	39.818906	76.460609
78.596776	43.290018	76.465614
78.421921	39.003302	76.470618
77.264691	42.161986	76.475623
76.399729	34.457647	76.480628
76.062827	39.977121	76.485633
75.602940	36.842890	76.490638
74.609891	43.044171	76.495642
73.974722	43.859810	76.500647
73.765847	44.228995	76.505652
72.926237	42.577743	76.510657
71.540295	36.916657	76.515662
71.360289	37.978257	76.520666
70.498559	42.714096	76.525671
69.955905	32.965076	76.530676
69.493126	33.010473	76.535681
68.369337	34.979525	76.540686
68.035427	29.825615	76.545690
67.196002	34.117921	76.550695
67.112901	41.388356	76.555700
66.212956	39.894963	76.560705
64.791508	33.837418	76.565710
64.596328	41.862169	76.570714
64.092054	43.103218	76.575719
63.591187	35.484324	76.580724
62.668491	32.710912	76.585729
61.641954	39.199812	76.590734
61.227492	37.654231	76.595738
60.723070	35.437016	76.600743
60.669129	42.956693	76.605748
59.634287	32.434606	76.610753
59.032632	36.875079	76.615758
58.865562	34.405367	76.620762
57.252498	38.679129	76.625767
56.362388	39.660009	76.630772
55.949375	34.709528	76.635777
55.054320	46.897122	76.640782
55.195188	38.128781	76.645786
54.432061	42.929325	76.650791
53.813900	41.564465	76.655796
52.984222	33.690506	76.660801
52.312040	40.149706	76.665806
51.575967	34.832851	76.670810
50.666212	42.190965	76.675815
50.149058	37.115165	76.680820
49.935532	40.886611	76.685825
48.747132	45.988371	76.690830
48.130654	26.071817	76.695834
47.312003	38.559460	76.700839
46.799685	34.813851	76.705844
46.503746	37.604951	76.710849
45.509083	45.340887	76.715854
44.835072	31.183126	76.720858
44.344406	34.129861	76.725863
43.982293	40.951201	76.730868
42.954249	36.365316	76.735873
41.908789	44.607676	76.740878
41.662026	35.831771	76.745882
41.221870	39.995755	76.750887
40.306707	34.679081	76.755892
39.438509	39.643042	76.760897
38.635002	37.902466	76.765902
38.467873	29.391412	76.770906
38.082471	40.677701	76.775911
36.997633	39.548125	76.780916
36.126140	38.433409	76.785921
35.502725	35.287422	76.790926
35.449351	30.856758	76.795930
34.510725	37.706965	76.800935
33.417158	37.509192	76.805940
33.281089	28.830757	76.810945
32.531633	41.482414	76.815950
31.926711	32.547590	76.820954
30.803655	31.414651	76.825959
30.040264	35.590762	76.830964
29.666745	33.843114	76.835969
29.143951	36.202037	76.840974
28.772955	33.104104	76.845978
27.777073	41.650799	76.850983
27.048238	37.908186	76.855988
26.737901	31.738112	76.860993
25.103681	39.041464	76.865998
24.914474	34.399073	76.871002
23.958585	37.908870	76.876007
23.574874	31.890849	76.881012
23.264795	32.744538	76.886017
22.741315	46.049293	76.891022
22.292260	32.948499	76.896026
21.327994	35.608071	76.901031
20.542037	35.813832	76.906036
20.133755	36.199056	76.911041
18.764342	39.628151	76.916046
18.583994	31.447216	76.921050
17.888824	37.219378	76.926055
17.384106	35.699239	76.931060
16.554098	39.769285	76.936065
15.557333	41.155125	76.941070
15.328685	39.546799	76.946074
14.806255	38.972512	76.951079
14.000529	39.581977	76.956084
13.455598	43.500900	76.961089
12.519841	49.937496	76.966094
11.916222	40.400066	76.971098
10.736762	53.434136	76.976103
10.324338	49.038658	76.981108
9.914843	45.141037	76.986113
9.292978	50.931476	76.991118
9.092879	38.156831	76.996122
8.023409	40.000551	77.001127
7.353346	36.187070	77.006132
7.115096	33.113700	77.011137
5.905785	42.099724	77.016142
5.256275	31.830024	77.021147
4.693150	46.099897	77.026151
4.252716	44.700396	77.031156
3.336641	42.381693	77.036161