Fri Mar 05 18:51:38 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.178648	91.516849	0.000000
-0.267292	94.219756	0.005005
-0.584198	55.604680	0.010010
-2.332639	15.869754	0.015014
-6.207460	-18.902234	0.020019
-11.828300	-18.138049	0.025024
-17.540489	-6.826778	0.030029
-21.891472	-12.322231	0.035034
-26.099105	-11.665178	0.040038
-29.686221	-4.226837	0.045043
-33.030923	-10.144572	0.050048
-37.091721	-5.852382	0.055053
-40.309001	-8.559247	0.060058
-44.219356	-12.469146	0.065062
-47.909470	-3.544625	0.070067
-51.457100	-15.608477	0.075072
-55.660514	-0.213801	0.080077
-59.025687	-7.407147	0.085082
-62.661275	-5.300605	0.090086
-66.670328	-11.495501	0.095091
-70.239909	-5.564319	0.100096
-74.622645	-4.715242	0.105101
-78.005267	-6.927321	0.110106
-81.785025	-7.409190	0.115110
-86.003116	-1.606330	0.120115
-89.186189	-7.534002	0.125120
-93.029733	-9.464361	0.130125
-96.901371	-3.161671	0.135130
-100.668553	-7.102207	0.140134
-104.072157	0.067262	0.145139
-107.815250	-5.567604	0.150144
-112.098969	-14.891433	0.155149
-115.647925	-19.891781	0.160154
-119.586801	-10.504845	0.165158
-123.394587	-14.779485	0.170163
-127.198412	-16.266694	0.175168
-131.305182	-9.429694	0.180173
-134.753724	-13.055163	0.185178
-138.428596	-7.427207	0.190182
-142.222231	-6.460698	0.195187
-145.713348	-15.355850	0.200192
-149.710434	-2.643239	0.205197
-152.962251	-14.183275	0.210202
-156.735771	-9.813731	0.215206
-160.912004	-3.497030	0.220211
-164.758545	-10.067775	0.225216
-168.790552	-1.459105	0.230221
-172.153599	-6.312421	0.235226
-175.872683	-3.555297	0.240230
-179.432765	-7.591834	0.245235
-183.534894	-11.505590	0.250240
-187.354800	-8.186733	0.255245
-190.994907	-6.246437	0.260250
-194.684914	-12.272832	0.265254
-198.619578	-2.038041	0.270259
-202.255391	-1.211744	0.275264
-205.719984	-6.045651	0.280269
-209.379496	-5.948844	0.285274
-213.577735	-3.181422	0.290278
-217.392158	-1.938665	0.295283
-221.125154	-5.729922	0.300288
-224.920588	-4.617917	0.305293
-228.598083	-13.401194	0.310298
-232.292267	-4.128830	0.315302
-236.339601	-6.122626	0.320307
-239.752210	-5.905909	0.325312
-243.699509	-1.584188	0.330317
-247.556094	-10.223733	0.335322
-251.211644	-15.613716	0.340326
-255.182836	-4.108294	0.345331
-258.348774	-10.169353	0.350336
-262.541608	-0.937199	0.355341
-266.279751	6.227541	0.360346
-269.733178	-1.913352	0.365350
-274.010563	-0.613952	0.370355
-277.445938	-9.962504	0.375360
-281.417871	-5.988451	0.380365
-284.871773	-6.659211	0.385370
-288.536489	-0.291486	0.390374
-292.638067	-10.998656	0.395379
-296.017637	-14.352623	0.400384
-300.190077	1.461694	0.405389
-304.014654	-13.812376	0.410394
-307.574545	-10.463878	0.415398
-311.371236	2.455112	0.420403
-314.816323	-4.236244	0.425408
-318.839423	-2.225153	0.430413
-322.677031	-11.695500	0.435418
-326.388914	-1.157035	0.440422
-330.251118	-13.618075	0.445427
-333.876153	-10.121944	0.450432
-337.919035	-1.855046	0.455437
-341.539873	-5.629325	0.460442
-345.545163	-3.543762	0.465446
-349.211622	-1.827681	0.470451
-352.519398	-12.156851	0.475456
-356.655556	-0.659626	0.480461
-359.983791	-11.679378	0.485466
-363.878691	-3.849229	0.490470
-367.895775	3.607778	0.495475
-371.684973	-13.108426	0.500480
-375.377253	-9.286107	0.505485
-379.085550	-8.086848	0.510490
-382.760129	-8.640230	0.515494
-386.523215	-5.257595	0.520499
-390.415164	-5.629601	0.525504
-394.048101	-2.411238	0.530509
-397.879577	-5.560438	0.535514
-401.592202	-7.908594	0.540518
-405.537007	-1.279932	0.545523
-409.038504	-7.277739	0.550528
-413.086929	3.040203	0.555533
-416.411511	2.169209	0.560538
-420.523906	-2.097309	0.565542
-424.412309	-3.862274	0.570547
-427.956464	-3.460280	0.575552
-431.908527	-1.845122	0.580557
-435.323963	0.474400	0.585562
-439.187484	2.228396	0.590566
-442.858524	-3.603515	0.595571
-446.806654	-4.810125	0.600576
-450.869149	-2.138090	0.605581
-454.439461	-8.948005	0.610586
-458.043911	-3.206246	0.615590
-462.249271	-7.178722	0.620595
-465.202447	-13.521052	0.625600
-469.461598	-11.822097	0.630605
-473.101911	-12.551121	0.635610
-476.670999	-9.240333	0.640614
-480.933952	-4.902512	0.645619
-484.337264	-12.880762	0.650624
-488.461218	-1.325352	0.655629
-491.814925	-9.229514	0.660634
-495.537502	-5.991953	0.665638
-499.518780	-3.711276	0.670643
-502.970149	-10.617383	0.675648
-506.849693	-9.822660	0.680653
-511.019396	-8.948469	0.685658
-514.609850	-8.549991	0.690662
-518.686518	-5.790423	0.695667
-521.842724	-10.860768	0.700672
-525.533172	-3.428878	0.705677
-529.306658	-17.400261	0.710682
-533.119589	-16.879485	0.715686
-537.311918	-7.473498	0.720691
-540.646561	-14.120647	0.725696
-544.850210	-5.618006	0.730701
-548.633361	-0.415271	0.735706
-552.356193	-7.853526	0.740710
-556.171445	5.795759	0.745715
-559.306892	-10.939391	0.750720
-563.451615	-1.182994	0.755725
-567.360899	1.958347	0.760730
-570.717829	-5.363290	0.765734
-574.680145	-5.025165	0.770739
-578.158547	-2.340569	0.775744
-582.225195	-1.944763	0.780749
-586.327793	-5.810430	0.785754
-590.053267	-10.073803	0.790758
-593.675690	1.538850	0.795763
-597.114801	-4.216325	0.800768
-600.831041	2.544866	0.805773
-604.649837	-13.119101	0.810778
-608.498401	-15.423133	0.815782
-612.688753	-5.355017	0.820787
-616.056360	-16.825400	0.825792
-620.090252	-11.498920	0.830797
-623.702250	-9.512003	0.835802
-626.975224	-9.306005	0.840806
-631.302999	-2.423410	0.845811
-634.764962	-6.410271	0.850816
-638.557694	-3.610712	0.855821
-642.763175	0.164702	0.860826
-646.183077	-2.057951	0.865830
-649.829847	-1.506769	0.870835
-653.223258	-10.457745	0.875840
-657.157094	-10.215496	0.880845
-661.355768	-9.711727	0.885850
-665.058210	-10.044177	0.890854
-668.961725	-3.674007	0.895859
-672.417334	-8.410876	0.900864
-676.432655	-16.313115	0.905869
-680.085817	-12.154390	0.910874
-683.993827	-16.691214	0.915878
-687.700351	-2.504034	0.920883
-691.326269	-13.385825	0.925888
-695.142577	-3.033570	0.930893
-698.666527	-11.102603	0.935898
-702.368569	-7.979970	0.940902
-706.543225	2.495804	0.945907
-710.055338	-0.964115	0.950912
-713.650989	-7.703341	0.955917
-717.579475	-2.988051	0.960922
-721.598440	-5.707787	0.965926
-725.534628	-3.673638	0.970931
-728.743360	-13.540254	0.975936
-732.368520	-6.665694	0.980941
-736.463786	-4.664451	0.985946
-740.119695	-4.824448	0.990950
-744.245551	-2.696878	0.995955
-747.760499	-15.028176	1.000960
-751.614649	-4.907908	1.005965
-755.601926	-7.454454	1.010970
-758.813542	-5.693751	1.015974
-762.932545	-2.015529	1.020979
-766.159507	-15.955578	1.025984
-770.416524	-1.399599	1.030989
-774.400727	-5.275970	1.035994
-777.770102	-13.839512	1.040998
-781.915474	-12.196033	1.046003
-785.026857	-19.133968	1.051008
-788.814356	-9.044800	1.056013
-792.807020	-10.275249	1.061018
-796.703476	-12.467236	1.066022
-800.429363	0.381221	1.071027
-804.147344	-13.294205	1.076032
-807.893031	-5.662259	1.081037
-811.643278	-15.465846	1.086042
-815.267226	-16.723656	1.091046
-819.462382	-6.452582	1.096051
-822.891016	-9.223930	1.101056
-826.890444	-4.738396	1.106061
-830.721627	-11.152777	1.111066
-834.493951	-15.908153	1.116070
-837.945946	-8.409844	1.121075
-841.536071	-18.141205	1.126080
-845.674729	-3.974607	1.131085
-849.401156	-12.678078	1.136090
-852.643292	-13.828137	1.141094
-857.010561	-12.901255	1.146099
-860.607449	-16.481427	1.151104
-864.264716	-14.173099	1.156109
-868.081502	-8.871456	1.161114
-871.713899	-8.402654	1.166118
-875.622042	-3.982095	1.171123
-879.470971	-13.161090	1.176128
-883.518450	-1.806502	1.181133
-887.095909	-7.983813	1.186138
-890.396274	-3.978946	1.191142
-894.170874	-2.642131	1.196147
-898.091867	-8.337146	1.201152
-901.867088	-4.492882	1.206157
-905.703556	-9.321463	1.211162
-909.343455	-8.126010	1.216166
-913.520661	-3.287057	1.221171
-917.284841	-8.139793	1.226176
-920.850956	-0.698812	1.231181
-924.237209	-6.056666	1.236186
-928.147708	-6.673975	1.241190
-932.399788	2.346420	1.246195
-935.972459	-7.803897	1.251200
-939.320042	-1.367653	1.256205
-943.550173	-4.233008	1.261210
-947.058884	-12.889128	1.266214
-950.888089	-7.093363	1.271219
-954.388754	-14.172238	1.276224
-958.219405	-4.630995	1.281229
-962.140627	-5.796886	1.286234
-965.836566	-10.299334	1.291238
-969.770994	-5.790843	1.296243
-973.346120	-10.645333	1.301248
-977.466428	-1.973940	1.306253
-980.898824	-9.812740	1.311258
-984.545183	-12.739838	1.316262
-988.574272	-13.238733	1.321267
-992.376509	-23.181922	1.326272
-996.031389	-16.376344	1.331277
-999.837535	-12.717791	1.336282
-1003.503816	-11.565281	1.341286
-1007.261229	-0.652697	1.346291
-1010.916730	-11.841460	1.351296
-1014.569516	-12.304302	1.356301
-1018.589125	-14.726951	1.361306
-1022.134547	-6.246779	1.366310
-1026.330090	-1.108232	1.371315
-1029.896189	-11.134865	1.376320
-1033.565823	-8.493141	1.381325
-1037.375303	-15.224449	1.386330
-1041.202685	-20.347561	1.391334
-1045.050314	-4.407406	1.396339
-1048.832474	-7.978149	1.401344
-1052.546586	-4.398886	1.406349
-1056.236184	5.009565	1.411354
-1059.681948	-6.283631	1.416358
-1063.605806	0.019459	1.421363
-1067.490846	-8.281386	1.426368
-1071.239821	-2.424147	1.431373
-1075.094848	-4.485099	1.436378
-1078.716873	-18.208508	1.441382
-1082.824766	-7.328060	1.446387
-1086.412550	-17.571898	1.451392
-1089.827397	-3.550655	1.456397
-1093.853108	-6.599819	1.461402
-1097.192656	-2.435438	1.466406
-1101.730637	8.070733	1.471411
-1105.053732	-9.937698	1.476416
-1109.079830	-6.781520	1.481421
-1112.949718	-0.488561	1.486426
-1116.060168	-7.708457	1.491430
-1119.898744	0.363021	1.496435
-1123.511076	1.999093	1.501440
-1127.697669	-8.726043	1.506445
-1131.455117	-14.252850	1.511450
-1134.919809	-14.568978	1.516454
-1139.027054	4.175656	1.521459
-1142.612275	-3.889179	1.526464
-1146.717942	-0.606665	1.531469
-1150.450132	-1.998022	1.536474
-1153.686195	-11.835982	1.541478
-1157.318781	-2.505893	1.546483
-1161.399744	-12.718011	1.551488
-1165.436948	-10.818356	1.556493
-1169.396082	-2.363240	1.561498
-1172.758802	-5.313344	1.566502
-1176.544037	1.503908	1.571507
-1179.929207	-9.912326	1.576512
-1183.858569	-6.784115	1.581517
-1187.697130	4.351459	1.586522
-1191.677742	-6.143167	1.591526
-1195.693531	-3.471033	1.596531
-1199.077399	-9.978438	1.601536
-1202.919713	-10.787543	1.606541
-1206.749442	-13.385324	1.611546
-1210.371967	-6.015324	1.616550
-1214.198864	-6.456297	1.621555
-1217.850470	-4.788565	1.626560
-1221.589798	-6.863054	1.631565
-1225.856703	-5.833275	1.636570
-1229.117320	-6.095188	1.641574
-1233.011603	-1.296224	1.646579
-1236.771470	-3.331132	1.651584
-1240.461989	-4.011504	1.656589
-1244.509352	-8.567642	1.661594
-1247.904045	-10.135851	1.666598
-1251.526285	-1.423861	1.671603
-1255.338736	-5.998652	1.676608
-1259.105613	-9.842723	1.681613
-1263.123843	0.974792	1.686618
-1266.933586	-5.953202	1.691622
-1270.517728	-5.300694	1.696627
-1274.240277	-4.805799	1.701632
-1278.018779	-3.615975	1.706637
-1282.385249	-7.583237	1.711642
-1285.162443	-7.988674	1.716646
-1289.022747	-9.337222	1.721651
-1292.953617	-15.908315	1.726656
-1297.092940	-18.987818	1.731661
-1300.908724	-13.993156	1.736666
-1304.498431	-13.218280	1.741670
-1308.582315	-9.391778	1.746675
-1312.209173	-6.928354	1.751680
-1315.596693	-10.516088	1.756685
-1319.343932	-7.224417	1.761690
-1323.023348	-18.645356	1.766694
-1327.037416	-8.626338	1.771699
-1330.814548	0.194140	1.776704
-1334.345413	-0.248289	1.781709
-1338.391382	-6.034492	1.786714
-1341.713253	-5.515319	1.791718
-1345.834204	-9.606914	1.796723
-1349.666657	-8.859341	1.801728
-1353.250828	-3.397050	1.806733
-1357.166629	-9.030591	1.811738
-1360.499042	-12.534039	1.816742
-1364.606166	-0.041618	1.821747
-1368.271767	-10.873347	1.826752
-1372.077942	-6.208109	1.831757
-1376.162363	-3.143062	1.836762
-1379.581341	-8.930217	1.841766
-1383.558566	-9.318457	1.846771
-1387.020555	-6.971198	1.851776
-1390.829673	-11.629868	1.856781
-1395.143421	-7.845261	1.861786
-1398.543079	-14.069135	1.866790
-1402.127286	-5.232129	1.871795
-1405.916727	-10.958353	1.876800
-1409.623736	-12.116777	1.881805
-1413.439092	-7.508350	1.886810
-1416.996598	-11.653756	1.891814
-1421.286965	-2.911813	1.896819
-1424.968970	-13.220428	1.901824
-1428.352450	-6.150149	1.906829
-1432.305777	-2.612414	1.911834
-1435.689350	-10.955051	1.916838
-1440.002949	-2.633550	1.921843
-1444.032922	-5.571025	1.926848
-1447.700651	-2.358112	1.931853
-1451.264358	-2.957527	1.936858
-1454.582502	-4.802611	1.941862
-1458.417748	0.302656	1.946867
-1462.328618	-5.413492	1.951872
-1466.110219	-3.204168	1.956877
-1469.936098	-2.006446	1.961882
-1473.968311	-8.630377	1.966886
-1477.517027	-5.215705	1.971891
-1480.904584	-4.458735	1.976896
-1484.794772	-0.222979	1.981901
-1488.554206	8.430912	1.986906
-1492.516567	-0.735153	1.991910
-1496.361168	2.012582	1.996915
-1500.238470	-3.340646	2.006912
-1501.296048	-2.689629	2.016909
-1498.727603	0.734388	2.026906
-1495.504347	0.669851	2.036902
-1493.577041	-4.350316	2.046899
-1491.799113	-3.907073	2.056896
-1489.821538	-9.334760	2.066893
-1487.707469	-6.711128	2.076890
-1486.068169	-4.813570	2.086886
-1484.479374	-8.138990	2.096883
-1482.218375	-3.412033	2.106880
-1480.033213	-8.220849	2.116877
-1478.434426	-4.598900	2.126874
-1476.806429	-1.259521	2.136870
-1474.743735	-2.248185	2.146867
-1472.654806	-2.652099	2.156864
-1470.642944	-8.304736	2.166861
-1469.247685	1.135091	2.176858
-1466.964227	1.547930	2.186854
-1464.945716	-1.835236	2.196851
-1463.340694	-1.264808	2.206848
-1461.481491	-6.120886	2.216845
-1459.481363	-5.934251	2.226842
-1457.616128	-5.193907	2.236838
-1455.414553	-6.144792	2.246835
-1453.966923	-9.870746	2.256832
-1452.089848	-1.307008	2.266829
-1450.241739	-4.973929	2.276826
-1448.055737	-2.890725	2.286822
-1446.244121	-2.455998	2.296819
-1444.390538	-4.519576	2.306816
-1442.657814	-7.789066	2.316813
-1440.677888	-5.843385	2.326810
-1438.897777	-7.574667	2.336806
-1436.804879	-13.091829	2.346803
-1434.901523	-9.769669	2.356800
-1433.212215	-12.999042	2.366797
-1431.521344	-8.791802	2.376794
-1429.605290	-9.935367	2.386790
-1427.316040	-8.662889	2.396787
-1425.669003	-8.746532	2.406784
-1423.653272	-9.358156	2.416781
-1421.684636	-10.614345	2.426778
-1420.036001	-10.565608	2.436774
-1418.212032	-6.254930	2.446771
-1416.119667	-12.886730	2.456768
-1414.249492	-10.110294	2.466765
-1412.730919	-14.359161	2.476762
-1410.532953	-4.990973	2.486758
-1408.719909	-4.681182	2.496755
-1406.628278	-1.412824	2.506752
-1404.870101	-7.043740	2.516749
-1403.227773	-5.656608	2.526746
-1401.198702	-5.172976	2.536742
-1399.252169	-9.049827	2.546739
-1397.309655	-5.571271	2.556736
-1395.600900	-6.967410	2.566733
-1393.672853	-2.248635	2.576730
-1391.682100	-6.989931	2.586726
-1389.817625	-8.463102	2.596723
-1387.925272	-9.381785	2.606720
-1386.270805	-7.729742	2.616717
-1384.686621	-7.050133	2.626714
-1382.574904	-1.852330	2.636710
-1380.433835	-8.089266	2.646707
-1378.540631	-12.527564	2.656704
-1376.669070	-4.897616	2.666701
-1374.767531	-1.110899	2.676698
-1373.141367	-3.959069	2.686694
-1371.105124	-6.279201	2.696691
-1369.063722	-9.035947	2.706688
-1367.194385	-7.596710	2.716685
-1365.535803	-3.216879	2.726682
-1363.636655	-6.549271	2.736678
-1361.778816	-14.444538	2.746675
-1359.778091	-10.323161	2.756672
-1358.193732	-6.960921	2.766669
-1356.187429	-6.317288	2.776666
-1354.317347	-6.940272	2.786662
-1351.972169	-6.472463	2.796659
-1350.343898	-4.737252	2.806656
-1348.702682	-7.920973	2.816653
-1346.878263	-8.838222	2.826650
-1344.834786	-3.149457	2.836646
-1342.841626	-6.710041	2.846643
-1340.909871	-1.499179	2.856640
-1339.131082	-0.317003	2.866637
-1337.590504	-5.991987	2.876634
-1335.753406	-7.547576	2.886630
-1333.539289	-7.172453	2.896627
-1331.555787	-4.382507	2.906624
-1329.517431	-6.447151	2.916621
-1327.983851	-6.229931	2.926618
-1326.025404	-6.898616	2.936614
-1324.293136	-9.463735	2.946611
-1322.185147	-9.306878	2.956608
-1320.581020	-13.184119	2.966605
-1318.596193	-12.094909	2.976602
-1316.534462	-10.149582	2.986598
-1314.594142	-8.751664	2.996595
-1313.061046	-9.972783	3.006592
-1311.118963	-9.942518	3.016589
-1309.429197	-7.692908	3.026586
-1307.199184	-12.369799	3.036582
-1305.209665	-13.182388	3.046579
-1303.261630	-9.766214	3.056576
-1301.658234	-6.061188	3.066573
-1300.055129	-1.885585	3.076570
-1298.080581	-1.847873	3.086566
-1295.849818	-6.136453	3.096563
-1293.937649	-5.611909	3.106560
-1292.067877	-12.929561	3.116557
-1290.322127	-4.657291	3.126554
-1288.834314	-10.170640	3.136550
-1286.845149	-10.010522	3.146547
-1284.678454	-6.169851	3.156544
-1283.072459	-10.937898	3.166541
-1281.035555	-8.398036	3.176538
-1278.934663	-11.067910	3.186534
-1277.183449	-13.246025	3.196531
-1275.378199	-10.455924	3.206528
-1273.590617	-0.418745	3.216525
-1271.656412	0.238081	3.226522
-1269.626997	-5.159835	3.236518
-1267.683083	-8.118788	3.246515
-1265.985872	-5.267176	3.256512
-1264.442191	-4.517843	3.266509
-1262.331285	-2.381387	3.276506
-1260.333222	-1.622666	3.286502
-1258.553287	-0.464295	3.296499
-1256.346522	-4.024258	3.306496
-1254.832892	0.860440	3.316493
-1252.957273	-2.217047	3.326490
-1250.815464	-6.260822	3.336486
-1249.067395	-1.863643	3.346483
-1247.067834	-6.727811	3.356480
-1245.262932	-7.651331	3.366477
-1243.538173	-2.061464	3.376474
-1241.521973	-3.876169	3.386470
-1239.626499	-6.165766	3.396467
-1238.119425	-3.275809	3.406464
-1236.145120	-11.194363	3.416461
-1234.023825	-10.632183	3.426458
-1232.329365	-6.600626	3.436454
-1230.268821	-10.514534	3.446451
-1228.312539	-5.616972	3.456448
-1226.533997	-6.559944	3.466445
-1224.653617	-7.656580	3.476442
-1222.645571	-8.895224	3.486438
-1221.011990	-10.241312	3.496435
-1219.026173	-7.067952	3.506432
-1217.201242	-3.486736	3.516429
-1215.163783	-5.079030	3.526426
-1213.550795	-1.988109	3.536422
-1211.732262	-6.941702	3.546419
-1209.866244	4.267202	3.556416
-1207.665557	-7.153369	3.566413
-1205.790327	-1.248074	3.576410
-1204.254139	0.953561	3.586406
-1201.972312	0.080074	3.596403
-1200.370014	3.719036	3.606400
-1198.409710	1.996995	3.616397
-1196.506272	4.517241	3.626394
-1194.645096	-2.287387	3.636390
-1192.743004	-9.876984	3.646387
-1191.084216	0.101929	3.656384
-1188.936940	1.586841	3.666381
-1187.316321	-0.262417	3.676378
-1185.383306	-1.929553	3.686374
-1183.583735	-2.015325	3.696371
-1181.469635	-5.130916	3.706368
-1179.344870	-2.327122	3.716365
-1178.043379	-2.535301	3.726362
-1175.982604	-3.021285	3.736358
-1173.935261	-1.460369	3.746355
-1172.178027	0.443812	3.756352
-1170.152335	-0.582874	3.766349
-1168.496763	-4.859831	3.776346
-1166.250852	-9.079662	3.786342
-1164.577085	-5.363689	3.796339
-1162.954512	-4.810070	3.806336
-1161.128108	-8.361192	3.816333
-1159.187205	-1.800044	3.826330
-1156.919772	-6.563314	3.836326
-1155.171653	-7.626102	3.846323
-1153.392963	-8.469568	3.856320
-1151.517897	-2.325776	3.866317
-1149.697683	-1.145344	3.876314
-1147.687885	-4.473166	3.886310
-1145.732440	-2.499624	3.896307
-1143.890920	-7.775795	3.906304
-1142.324409	-3.880012	3.916301
-1140.322872	-1.856998	3.926298
-1138.443171	-2.445032	3.936294
-1136.774174	-3.187251	3.946291
-1134.758930	-7.114358	3.956288
-1132.606031	0.751854	3.966285
-1130.778076	-2.043174	3.976282
-1128.987309	-3.534348	3.986278
-1127.181319	-3.572156	3.996275
-1125.266902	-1.385189	4.006272
-1123.347926	-2.390024	4.016269
-1121.494881	1.065194	4.026266
-1119.430675	-4.459745	4.036262
-1117.684101	-8.523856	4.046259
-1115.734981	1.279197	4.056256
-1113.771572	-3.176447	4.066253
-1112.227308	4.384523	4.076250
-1110.460892	3.457789	4.086246
-1108.638366	-2.873221	4.096243
-1106.288527	-6.266460	4.106240
-1104.368421	-4.879339	4.116237
-1102.816073	-4.497602	4.126234
-1100.867739	-5.401325	4.136230
-1099.124791	-8.484311	4.146227
-1096.975448	-7.785965	4.156224
-1095.051339	-8.580018	4.166221
-1093.485762	-9.705138	4.176218
-1091.506233	-7.459085	4.186214
-1089.714274	-8.697786	4.196211
-1087.282679	-11.772502	4.206208
-1085.978101	-7.888464	4.216205
-1084.120865	-9.961819	4.226202
-1082.024077	-5.167130	4.236198
-1080.132308	-5.597573	4.246195
-1078.445110	-4.601071	4.256192
-1076.425190	-4.423586	4.266189
-1074.599960	-7.998140	4.276186
-1072.767953	-7.105325	4.286182
-1070.730275	-7.983841	4.296179
-1068.755182	-8.279181	4.306176
-1067.262381	-1.516797	4.316173
-1065.338508	-1.274990	4.326170
-1063.154702	-1.723713	4.336166
-1061.322006	-7.749996	4.346163
-1059.732839	-10.926777	4.356160
-1057.450855	-5.675368	4.366157
-1055.950432	-10.260593	4.376154
-1053.935363	-13.218123	4.386150
-1052.011770	-11.024669	4.396147
-1050.000303	-7.207888	4.406144
-1048.227366	-13.038284	4.416141
-1046.495211	-9.707355	4.426138
-1044.545858	-15.755440	4.436134
-1042.713157	-14.038497	4.446131
-1040.678394	-12.225975	4.456128
-1038.979815	-12.985487	4.466125
-1037.127258	-10.610131	4.476122
-1035.306919	-13.275971	4.486118
-1033.340436	-15.622551	4.496115
-1031.554077	-10.817638	4.506112
-1029.311110	-14.285287	4.516109
-1027.519863	-15.575932	4.526106
-1025.924872	-8.569337	4.536102
-1023.982894	-10.319881	4.546099
-1021.959959	-7.284915	4.556096
-1019.972964	-13.449530	4.566093
-1018.350797	-4.598313	4.576090
-1016.633889	-6.955491	4.586086
-1014.412226	-15.726600	4.596083
-1012.545318	-10.055074	4.606080
-1010.650798	-6.974295	4.616077
-1009.085857	-4.349229	4.626074
-1006.996124	-4.154428	4.636070
-1005.055018	-13.951194	4.646067
-1003.416004	-5.835298	4.656064
-1001.407380	0.996219	4.666061
-999.270955	-5.653339	4.676058
-997.675995	-0.516202	4.686054
-995.678592	-4.727713	4.696051
-993.968538	-4.817971	4.706048
-992.126523	-5.088806	4.716045
-989.969648	-6.954218	4.726042
-988.476605	-5.291857	4.736038
-986.312472	-10.709506	4.746035
-984.466691	-7.943020	4.756032
-982.880298	-6.701377	4.766029
-981.006196	-5.107846	4.776026
-978.889593	-3.267303	4.786022
-977.068959	-0.226785	4.796019
-975.159225	-3.473725	4.806016
-973.201703	-15.357321	4.816013
-971.031523	-8.714249	4.826010
-969.498893	-10.323497	4.836006
-967.549169	-5.359916	4.846003
-965.907733	-8.766049	4.856000
-963.797378	-16.691940	4.865997
-961.884638	-9.486634	4.875994
-960.146455	-12.295598	4.885990
-958.065780	-9.427704	4.895987
-956.431692	-14.997409	4.905984
-954.820792	-7.465931	4.915981
-952.741405	-6.192576	4.925978
-950.670711	-10.081029	4.935974
-948.683934	-19.150839	4.945971
-947.053704	-11.342972	4.955968
-945.150408	-11.514622	4.965965
-943.178533	-11.359339	4.975962
-941.227043	-3.563361	4.985958
-939.549090	-6.627946	4.995955
-937.564500	-7.221539	5.005952
-935.790081	-9.273642	5.015949
-933.758101	-8.030585	5.025946
-932.018324	-5.324473	5.035942
-930.188611	-6.452248	5.045939
-928.090772	-6.787624	5.055936
-926.255206	-3.214185	5.065933
-924.636564	-1.935026	5.075930
-922.722268	-2.334208	5.085926
-920.801487	-5.159710	5.095923
-918.580874	-4.932072	5.105920
-916.964409	-7.563648	5.115917
-915.060596	3.189481	5.125914
-913.242003	-6.472371	5.135910
-911.617623	-3.829898	5.145907
-909.623899	-11.481307	5.155904
-907.370298	-9.446286	5.165901
-905.467906	-8.586697	5.175898
-904.137931	-8.497696	5.185894
-901.969453	-4.865360	5.195891
-899.774111	-7.546849	5.205888
-898.299967	-8.769328	5.215885
-896.203538	-7.408645	5.225882
-894.497984	-6.034413	5.235878
-892.616617	-1.235100	5.245875
-890.753965	-8.503957	5.255872
-888.849482	-7.987324	5.265869
-886.915680	-4.025345	5.275866
-885.021396	-1.459163	5.285862
-882.894122	-7.262414	5.295859
-881.284116	-4.336566	5.305856
-879.439959	-5.411348	5.315853
-877.550723	-4.841740	5.325850
-876.052056	-2.363881	5.335846
-873.795858	-4.601914	5.345843
-871.775512	-0.194278	5.355840
-870.177171	-2.687135	5.365837
-868.083173	-4.308699	5.375834
-866.107734	-4.089183	5.385830
-864.343895	-8.245878	5.395827
-862.515831	-7.873323	5.405824
-860.782759	-7.041891	5.415821
-858.546726	-10.214589	5.425818
-857.051183	-7.575164	5.435814
-854.935674	-9.575947	5.445811
-852.957208	-6.277928	5.455808
-851.466254	-3.947242	5.465805
-849.451791	-4.815540	5.475802
-847.688518	-6.545268	5.485798
-845.549371	-7.327705	5.495795
-843.892103	-7.835735	5.505792
-841.899325	-8.790560	5.515789
-839.961921	-5.539650	5.525786
-838.096801	-5.585109	5.535782
-836.331249	-10.533118	5.545779
-834.395552	-5.794547	5.555776
-832.422913	-1.778728	5.565773
-830.625130	-0.234453	5.575770
-828.746227	-6.237957	5.585766
-827.063735	-2.924180	5.595763
-824.989333	-3.243086	5.605760
-823.103841	-1.929144	5.615757
-821.271578	0.326476	5.625754
-819.553906	-1.664366	5.635750
-817.723284	-5.435385	5.645747
-815.359168	-2.772143	5.655744
-813.570937	-3.575825	5.665741
-812.039263	-8.263799	5.675738
-810.099472	-5.496407	5.685734
-807.829792	0.576711	5.695731
-806.202744	-6.176000	5.705728
-804.511957	-3.940384	5.715725
-802.522232	-0.579382	5.725722
-800.499432	-3.108462	5.735718
-798.872364	-8.523788	5.745715
-796.920827	-6.074055	5.755712
-794.880815	-6.324280	5.765709
-793.402766	-9.195756	5.775706
-791.326630	-1.507986	5.785702
-789.242490	-0.986829	5.795699
-787.335950	-5.002068	5.805696
-785.580228	-3.826829	5.815693
-783.714643	-5.844445	5.825690
-782.003376	-4.739467	5.835686
-779.979011	-9.155641	5.845683
-778.031532	-5.034700	5.855680
-776.143240	-6.926464	5.865677
-774.497211	-6.242110	5.875674
-772.376824	-4.998830	5.885670
-770.872459	-10.533475	5.895667
-768.976091	-4.864867	5.905664
-766.571993	-1.287428	5.915661
-764.960832	-4.052268	5.925658
-763.280311	3.506130	5.935654
-761.014960	1.426215	5.945651
-759.194168	-4.612162	5.955648
-757.639505	-3.880035	5.965645
-755.628479	-2.240309	5.975642
-753.675357	6.161908	5.985638
-751.812583	0.505250	5.995635
-749.990400	-3.763324	6.005632
-747.839116	-2.076533	6.015629
-746.206563	-2.526860	6.025626
-744.525821	-4.756486	6.035622
-742.484253	-3.658477	6.045619
-740.392782	-5.690056	6.055616
-738.699142	-6.476986	6.065613
-736.977613	-1.604626	6.075610
-735.028980	-6.847092	6.085606
-733.106533	-6.748470	6.095603
-731.183223	-7.913157	6.105600
-729.174113	-6.430998	6.115597
-727.529005	-5.904360	6.125594
-725.405755	-1.696198	6.135590
-723.673152	-5.967805	6.145587
-721.626938	-8.958461	6.155584
-720.155262	-5.824073	6.165581
-718.326295	-6.190505	6.175578
-716.330102	-8.167362	6.185574
-714.250610	-6.146959	6.195571
-712.414577	-12.182999	6.205568
-710.485626	-4.239523	6.215565
-708.754126	-6.538815	6.225562
-706.758425	2.276644	6.235558
-704.908166	-4.277990	6.245555
-703.353082	-3.198521	6.255552
-701.282173	-0.139353	6.265549
-699.247150	-4.061372	6.275546
-697.355394	-3.324651	6.285542
-695.361235	-10.330171	6.295539
-693.564365	-3.294003	6.305536
-692.045966	-6.606083	6.315533
-689.795695	-4.835582	6.325530
-688.035438	-1.161491	6.335526
-686.297566	-1.609659	6.345523
-683.986615	-1.967821	6.355520
-682.374026	-5.345474	6.365517
-680.632200	0.613175	6.375514
-678.874547	1.050809	6.385510
-676.798388	-3.253558	6.395507
-674.769849	-1.686035	6.405504
-672.937362	-0.278237	6.415501
-671.261673	-0.787511	6.425498
-669.417143	-1.582713	6.435494
-667.479594	-3.240683	6.445491
-665.567327	-2.172473	6.455488
-663.681067	0.260963	6.465485
-661.821783	1.841332	6.475482
-659.748885	4.118633	6.485478
-657.935627	1.812628	6.495475
-656.243369	-2.624594	6.505472
-654.188006	-4.358221	6.515469
-652.493978	-5.260416	6.525466
-650.773687	0.761698	6.535462
-648.430482	-0.823703	6.545459
-646.458505	-0.115549	6.555456
-644.984671	3.496973	6.565453
-643.307604	6.358593	6.575450
-641.031883	8.933509	6.585446
-639.292361	2.020818	6.595443
-637.533291	-3.758135	6.605440
-635.290720	-3.637950	6.615437
-633.476627	-4.237207	6.625434
-631.704933	-0.763848	6.635430
-630.045381	-3.053169	6.645427
-628.058751	-5.693171	6.655424
-626.058426	-5.690590	6.665421
-624.397247	3.181552	6.675418
-622.386087	1.597121	6.685414
-620.325750	0.508526	6.695411
-618.608792	-3.749457	6.705408
-616.764295	-5.823576	6.715405
-614.671815	-2.638302	6.725402
-612.912850	-5.298761	6.735398
-611.483982	-5.487503	6.745395
-609.163112	-10.260388	6.755392
-607.245605	-3.546583	6.765389
-605.416211	-7.075668	6.775386
-603.622897	-5.056813	6.785382
-601.872268	-4.693789	6.795379
-599.798923	2.036181	6.805376
-598.167061	-0.698700	6.815373
-596.296576	-2.383794	6.825370
-594.179871	-3.448213	6.835366
-592.126447	-3.221979	6.845363
-590.434223	-6.315449	6.855360
-588.549898	-5.447979	6.865357
-586.623638	-4.162464	6.875354
-585.080094	1.791622	6.885350
-583.073673	-2.757320	6.895347
-581.233508	-1.197516	6.905344
-579.207297	-6.141200	6.915341
-577.263057	-4.844339	6.925338
-575.535850	0.810409	6.935334
-573.458964	-4.566108	6.945331
-571.551686	-2.454906	6.955328
-569.635787	-1.071404	6.965325
-568.068763	1.572584	6.975322
-566.066617	2.665992	6.985318
-564.234685	-7.523556	6.995315
-562.387569	1.118402	7.005312
-560.538971	-3.509522	7.015309
-558.775863	-6.426397	7.025306
-556.635022	-5.029871	7.035302
-554.750977	-4.228645	7.045299
-552.998886	-3.859502	7.055296
-551.139003	-2.026506	7.065293
-549.384842	-2.260857	7.075290
-547.164790	-3.843856	7.085286
-545.301830	-6.546143	7.095283
-543.639057	-3.446901	7.105280
-541.637678	3.064092	7.115277
-539.821368	1.076638	7.125274
-537.950022	-4.338072	7.135270
-536.050252	-6.051481	7.145267
-534.160371	-7.496464	7.155264
-532.245196	-4.186475	7.165261
-530.765615	-1.179542	7.175258
-528.586103	-8.492441	7.185254
-526.558890	-5.111921	7.195251
-524.803994	-7.192186	7.205248
-523.008431	-8.135772	7.215245
-520.994523	-6.602094	7.225242
-519.267145	-1.308913	7.235238
-517.343193	-4.818301	7.245235
-515.533374	-3.840975	7.255232
-513.500780	1.529778	7.265229
-511.603221	1.242550	7.275226
-509.597533	4.427575	7.285222
-507.946973	0.890807	7.295219
-506.053032	-1.172179	7.305216
-504.407003	-2.695034	7.315213
-502.332812	-3.511001	7.325210
-500.453309	5.354792	7.335206
-498.700816	-1.165134	7.345203
-496.486037	-0.836692	7.355200
-494.568348	-0.501850	7.365197
-492.991301	3.078497	7.375194
-490.909056	5.093927	7.385190
-489.284319	2.908157	7.395187
-487.123818	-1.619529	7.405184
-485.091284	-4.100956	7.415181
-483.557161	-1.737448	7.425178
-481.834104	-2.680477	7.435174
-479.641340	-1.778495	7.445171
-478.049048	-1.342722	7.455168
-476.278066	-3.438154	7.465165
-474.129003	-2.614451	7.475162
-472.222662	3.108087	7.485158
-470.261258	1.718048	7.495155
-468.521668	-4.326105	7.505152
-466.759026	-7.124418	7.515149
-464.624638	0.176991	7.525146
-462.971455	3.364669	7.535142
-460.938374	4.311118	7.545139
-458.974618	-4.077283	7.555136
-457.265512	-8.000740	7.565133
-455.490256	-1.384084	7.575130
-453.452665	0.287978	7.585126
-451.566581	-3.445841	7.595123
-449.798753	-1.454375	7.605120
-448.043202	1.949073	7.615117
-446.144188	2.121145	7.625114
-444.100605	-0.144116	7.635110
-442.118019	-4.689139	7.645107
-440.145461	-5.071974	7.655104
-438.623975	-9.837046	7.665101
-436.646553	-6.434285	7.675098
-434.811030	1.584364	7.685094
-432.769593	-5.777460	7.695091
-430.913319	-10.659150	7.705088
-429.089300	-4.778166	7.715085
-427.110761	-0.388717	7.725082
-425.463747	-0.676921	7.735078
-423.640137	-2.676507	7.745075
-421.724819	-4.521786	7.755072
-419.617576	-4.210838	7.765069
-417.780796	-3.888277	7.775066
-415.911203	-2.784628	7.785062
-413.919851	-7.662613	7.795059
-412.160074	-5.012982	7.805056
-410.289206	-4.489014	7.815053
-408.698876	-5.960278	7.825050
-406.728561	-3.416894	7.835046
-404.546197	-7.014827	7.845043
-402.814525	-5.903355	7.855040
-400.936496	-6.181062	7.865037
-398.928768	-5.986838	7.875034
-397.284250	-5.650931	7.885030
-395.416044	-4.466517	7.895027
-393.703198	-4.192044	7.905024
-391.535316	-7.678704	7.915021
-389.607861	-6.279532	7.925018
-387.886544	-5.183765	7.935014
-386.094664	-6.330348	7.945011
-384.012974	-7.063725	7.955008
-381.945171	-6.402230	7.965005
-380.419443	-9.192654	7.975002
-378.509079	-3.811737	7.984998
-376.402067	-2.101744	7.994995
-374.633368	-2.361974	8.004992
-372.818687	-9.466489	8.014989
-370.898058	-2.235071	8.024986
-369.206293	-0.315084	8.034982
-367.289217	-3.625888	8.044979
-365.341991	-3.327237	8.054976
-363.491544	-6.561082	8.064973
-361.859990	0.542813	8.074970
-359.433469	-3.716179	8.084966
-357.543688	-4.856267	8.094963
-355.825117	-6.354288	8.104960
-354.081890	-3.310385	8.114957
-352.475383	-4.871039	8.124954
-350.393538	-8.729195	8.134950
-348.331424	-6.037785	8.144947
-346.309741	0.084874	8.154944
-344.466025	-7.324263	8.164941
-343.017848	-4.016926	8.174938
-341.373133	-1.691507	8.184934
-338.974349	-0.298068	8.194931
-337.050754	-2.970405	8.204928
-335.309625	-8.686288	8.214925
-333.232818	-3.270325	8.224922
-331.764127	-8.690076	8.234918
-329.613969	-7.182723	8.244915
-327.786809	-0.237927	8.254912
-325.812877	-3.804095	8.264909
-323.988460	-1.246822	8.274906
-322.315019	2.251938	8.284902
-319.939676	-2.189901	8.294899
-318.501835	-3.752028	8.304896
-316.566336	-5.534130	8.314893
-314.733977	-2.498110	8.324890
-312.875717	-2.947858	8.334886
-310.968900	-1.794804	8.344883
-309.088926	0.655716	8.354880
-307.154601	-4.066239	8.364877
-305.182596	-5.478364	8.374874
-303.543262	-2.908898	8.384870
-301.566574	-8.870787	8.394867
-299.431156	-10.154255	8.404864
-297.811321	-5.034790	8.414861
-295.962994	-2.392890	8.424858
-294.062161	-4.122071	8.434854
-291.991047	1.046942	8.444851
-290.124792	-4.872048	8.454848
-288.736532	-4.738321	8.464845
-286.581809	-7.854888	8.474842
-284.735317	-3.426868	8.484838
-282.775810	-10.036537	8.494835
-280.519912	-6.141244	8.504832
-278.974700	-4.646226	8.514829
-277.370296	-0.406928	8.524826
-275.294335	-4.649354	8.534822
-273.157159	-4.257789	8.544819
-271.431372	-11.330676	8.554816
-269.723076	-10.351167	8.564813
-267.851013	-9.811489	8.574810
-265.933356	-8.080646	8.584807
-263.758604	-5.250821	8.594803
-261.841398	-10.140537	8.604800
-260.457507	-12.794561	8.614797
-258.749633	-9.727575	8.624794
-256.570392	-3.661566	8.634791
-254.517899	-8.820769	8.644787
-252.778293	-1.962991	8.654784
-250.782865	-4.365670	8.664781
-248.941617	-3.558948	8.674778
-247.268334	-7.009170	8.684775
-245.242826	-6.801866	8.694771
-243.402958	-8.717069	8.704768
-241.147635	-4.164792	8.714765
-239.511531	-4.127438	8.724762
-237.801528	-10.040397	8.734759
-235.800945	-7.588543	8.744755
-234.023444	-9.708526	8.754752
-232.219403	-8.869010	8.764749
-230.278189	-7.539800	8.774746
-228.377918	-9.456738	8.784743
-226.609847	-9.462544	8.794739
-224.411182	-12.305014	8.804736
-222.469791	-16.001696	8.814733
-220.844438	-10.418840	8.824730
-219.020648	-9.648784	8.834727
-217.358593	-9.073969	8.844723
-215.027736	-14.755995	8.854720
-213.175601	-16.134704	8.864717
-211.876113	-13.401985	8.874714
-209.764144	-12.714232	8.884711
-207.438168	-16.963343	8.894707
-205.202390	-21.318057	8.904704
-203.967728	-15.165987	8.914701
-202.033838	-15.675089	8.924698
-200.265930	-11.204460	8.934695
-198.453253	-19.056966	8.944691
-196.360718	-18.187676	8.954688
-194.619540	-11.320632	8.964685
-192.710523	-12.154184	8.974682
-190.843174	-8.991018	8.984679
-188.908012	-2.507035	8.994675
-186.606463	-13.576556	9.004672
-185.283573	-10.154388	9.014669
-183.567125	-14.912529	9.024666
-181.445210	-17.518498	9.034663
-179.765153	-20.080792	9.044659
-177.845191	-21.146608	9.054656
-175.790809	-18.696975	9.064653
-173.873850	-13.893265	9.074650
-172.035573	-9.435422	9.084647
-169.964578	-11.059028	9.094643
-168.474737	-13.729910	9.104640
-166.502938	-11.707623	9.114637
-164.552996	-14.750352	9.124634
-162.631483	-10.435260	9.134631
-160.809056	-12.554465	9.144627
-158.994987	-16.769211	9.154624
-156.990984	-15.235221	9.164621
-155.207811	-16.954992	9.174618
-153.175066	-19.420389	9.184615
-151.609040	-11.451659	9.194611
-149.707642	-17.072990	9.204608
-147.641964	-12.580362	9.214605
-145.831340	-15.005572	9.224602
-144.170653	-13.437313	9.234599
-142.005424	-9.187937	9.244595
-140.033599	-9.077769	9.254592
-138.207597	-11.211738	9.264589
-136.255070	-10.143208	9.274586
-134.746728	-14.375471	9.284583
-132.493333	-10.272788	9.294579
-130.971767	-8.574950	9.304576
-128.901178	-12.317442	9.314573
-127.072839	-11.593831	9.324570
-124.932341	-1.521967	9.334567
-123.496633	-0.353591	9.344563
-121.379344	-6.833578	9.354560
-119.761367	-11.635968	9.364557
-117.722857	-10.915885	9.374554
-115.625925	-11.086190	9.384551
-113.916729	-8.432999	9.394547
-111.916356	-13.940620	9.404544
-110.048471	-11.102743	9.414541
-108.039553	-6.031011	9.424538
-106.505355	-7.013115	9.434535
-104.597557	-2.853681	9.444531
-102.753681	-9.128973	9.454528
-100.763009	-9.553895	9.464525
-98.913586	-6.882013	9.474522
-97.183312	-7.465914	9.484519
-95.150761	-4.597454	9.494515
-93.190610	-4.254854	9.504512
-91.477914	-0.301127	9.514509
-89.490074	-2.348776	9.524506
-87.719832	-4.082226	9.534503
-85.674173	-7.283854	9.544499
-83.761367	-5.324717	9.554496
-82.094573	-0.733647	9.564493
-80.130462	-1.166947	9.574490
-78.103810	2.397221	9.584487
-76.336131	1.073142	9.594483
-74.390684	-5.500973	9.604480
-72.790366	-3.662500	9.614477
-70.759007	1.574638	9.624474
-69.065207	-2.423489	9.634471
-67.103974	-4.373715	9.644467
-65.139361	-5.233406	9.654464
-63.278519	-0.603806	9.664461
-61.521169	4.146521	9.674458
-59.770218	2.585118	9.684455
-57.449599	-1.925116	9.694451
-55.450311	1.662385	9.704448
-53.799335	-1.332566	9.714445
-51.950777	-1.300557	9.724442
-50.108709	1.198852	9.734439
-48.430332	-6.186865	9.744435
-46.285557	-4.381548	9.754432
-44.549842	-4.770487	9.764429
-42.561568	-5.185505	9.774426
-40.872600	-6.260155	9.784423
-38.855192	-11.238323	9.794419
-36.791310	-7.593217	9.804416
-35.112303	-5.806747	9.814413
-33.211636	-4.107742	9.824410
-31.568479	-4.714016	9.834407
-29.432608	-8.755794	9.844403
-27.441694	-7.893829	9.854400
-25.887742	-5.310545	9.864397
-23.775570	-6.637435	9.874394
-21.762561	-3.326837	9.884391
-20.304677	1.720770	9.894387
-18.322381	-1.434380	9.904384
-16.282696	-1.383884	9.914381
-14.696112	-9.779692	9.924378
-12.740622	-0.587694	9.934375
-10.873074	-7.482500	9.944371
-8.690747	1.299101	9.954368
-7.192048	12.621387	9.964365
-5.683544	25.162672	9.974362
-4.189546	57.238308	9.984359
-2.495019	95.389556	9.994355
-1.055190	141.692822	10.004352
0.000000	182.949583	10.009357
0.919834	217.444431	10.014362
1.598052	249.355375	10.019367
1.848734	268.136765	10.024371
2.169517	285.514516	10.029376
2.425017	295.765236	10.034381
2.690571	301.881064	10.039386
2.686920	307.741784	10.044391
3.192624	317.446395	10.049395
3.289622	334.806284	10.054400
3.267554	352.541586	10.059405
4.104334	342.749039	10.064410
3.585051	339.474481	10.069415
3.777120	317.597769	10.074419
3.610339	326.479229	10.079424
3.568455	323.683626	10.084429
3.787710	327.201655	10.089434
3.705722	328.447978	10.094439
3.616770	321.750513	10.099443
3.723573	324.253548	10.104448
3.626372	330.055081	10.109453
4.173400	331.407655	10.114458
3.867219	332.013208	10.119463
3.973472	334.118930	10.124467
3.708166	338.146352	10.129472
3.801815	334.685713	10.134477
4.299008	337.563306	10.139482
3.772921	350.761561	10.144487
4.090835	357.698561	10.149491
4.023765	362.235279	10.154496
4.306249	367.365964	10.159501
4.280575	375.768405	10.164506
4.382291	381.049358	10.169511
4.273987	372.844979	10.174515
4.236196	384.808646	10.179520
4.612249	386.273656	10.184525
4.855996	385.977759	10.189530
4.438997	380.624158	10.194535
4.840043	381.213100	10.199539
4.845693	382.847583	10.204544
4.713299	391.412928	10.209549
4.792385	391.523354	10.214554
4.830391	394.688677	10.219559
4.757897	382.781299	10.224563
4.791799	389.698960	10.229568
4.725073	393.715223	10.234573
4.949405	394.475860	10.239578
4.666093	403.587273	10.244583
5.016792	394.145049	10.249587
5.131455	398.305849	10.254592
4.689949	401.721131	10.259597
5.226755	396.373082	10.264602
5.051645	401.841708	10.269607
5.218667	398.187994	10.274611
4.987775	398.160202	10.279616
4.846595	402.774988	10.284621
5.394474	399.147259	10.289626
5.232994	407.390814	10.294631
5.434488	394.666990	10.299635
5.394030	410.670595	10.304640
5.522362	427.415296	10.309645
6.212918	434.502635	10.314650
5.402091	425.338709	10.319655
5.844009	415.795186	10.324659
5.716229	414.902517	10.329664
5.270555	419.698347	10.334669
5.919648	427.952972	10.339674
5.813547	450.935882	10.344679
6.006421	447.572933	10.349683
6.019146	443.418677	10.354688
5.971153	453.577567	10.359693
6.242704	450.616821	10.364698
6.214932	457.265222	10.369703
6.224817	440.151567	10.374707
5.739041	439.118875	10.379712
5.907974	442.436795	10.384717
6.255470	445.251554	10.389722
6.097531	462.925083	10.394727
6.098735	450.332511	10.399731
6.090654	453.041558	10.404736
6.195870	457.952961	10.409741
6.099417	458.917741	10.414746
6.140855	465.515681	10.419751
6.274947	466.134592	10.424755
6.274009	485.147218	10.429760
6.492798	488.146525	10.434765
6.940674	489.309919	10.439770
6.719750	493.902760	10.444775
6.841966	494.020500	10.449779
6.786285	493.630432	10.454784
6.567305	500.211577	10.459789
6.917176	488.331362	10.464794
6.959672	504.424344	10.469799
7.282706	498.682987	10.474803
6.968846	502.279788	10.479808
7.121929	497.555905	10.484813
7.163876	494.750051	10.489818
7.038083	501.942407	10.494823
7.063872	503.890671	10.499827
7.124196	504.068748	10.504832
7.071925	500.978288	10.509837
7.631969	499.895472	10.514842
7.027334	511.242370	10.519847
7.392797	506.568188	10.524851
7.211773	508.661410	10.529856
7.140768	514.227016	10.534861
7.507271	515.376583	10.539866
7.570673	531.854207	10.544871
7.733009	535.305670	10.549875
7.799983	534.041293	10.554880
7.483254	545.682929	10.559885
7.564788	540.853745	10.564890
7.662444	551.055705	10.569895
7.956758	537.041144	10.574899
7.917351	536.656364	10.579904
7.995470	544.399711	10.584909
8.423359	538.860818	10.589914
8.067987	548.628816	10.594919
7.941684	549.194646	10.599923
8.152395	552.105364	10.604928
8.153278	549.864314	10.609933
7.990833	554.632357	10.614938
7.743106	550.508576	10.619943
7.890900	550.100243	10.624947
8.158923	550.025985	10.629952
7.943919	561.676641	10.634957
8.382707	570.452193	10.639962
8.423612	577.857704	10.644967
8.476933	580.016062	10.649971
8.365515	588.855733	10.654976
8.690834	584.588494	10.659981
8.621758	577.365746	10.664986
8.456422	590.213346	10.669991
8.882955	590.430786	10.674995
8.804868	579.596515	10.680000
8.384574	585.381873	10.685005
8.649915	588.138799	10.690010
8.412816	592.573394	10.695015
8.311027	595.455117	10.700019
8.803209	613.349995	10.705024
9.005566	614.123612	10.710029
9.243420	621.535578	10.715034
8.954834	627.525459	10.720039
9.209189	621.034882	10.725043
9.305113	620.298915	10.730048
9.095107	630.540543	10.735053
9.361987	624.803363	10.740058
9.100823	633.635406	10.745063
9.134443	629.883060	10.750067
9.429104	633.844899	10.755072
9.303203	630.100650	10.760077
9.432961	638.523395	10.765082
9.111364	634.107007	10.770087
9.331268	635.423478	10.775091
9.577200	645.395262	10.780096
9.946619	659.400324	10.785101
10.076173	659.502702	10.790106
9.594410	646.201636	10.795111
9.727042	665.068607	10.800115
10.067648	662.308127	10.805120
9.933986	667.855399	10.810125
9.976466	667.943280	10.815130
10.056477	662.956595	10.820135
9.608693	663.529551	10.825139
10.138287	665.440056	10.830144
9.711212	669.160617	10.835149
9.963364	667.243764	10.840154
9.789586	674.382355	10.845159
9.922456	668.226541	10.850163
10.139268	670.530730	10.855168
9.861143	668.066071	10.860173
10.201204	682.162575	10.865178
10.115468	697.713224	10.870183
10.133442	696.704243	10.875187
10.315023	687.033327	10.880192
10.352202	706.251485	10.885197
10.602075	697.924342	10.890202
10.617959	708.713497	10.895207
10.762649	705.613655	10.900211
10.715330	706.116427	10.905216
10.634426	709.414332	10.910221
11.070303	702.883725	10.915226
10.803508	706.679661	10.920231
10.789031	703.046937	10.925235
11.010633	716.593060	10.930240
10.947611	740.887959	10.935245
11.247009	737.678273	10.940250
11.406293	728.496614	10.945255
11.027187	718.722712	10.950259
11.133432	713.449536	10.955264
10.981558	728.091355	10.960269
11.517754	737.272542	10.965274
11.182214	746.573858	10.970279
11.475684	748.648201	10.975283
11.720472	750.493753	10.980288
11.284351	748.183599	10.985293
11.555654	735.751135	10.990298
11.562162	743.483933	10.995303
11.774445	735.389858	11.000307
11.497033	744.170941	11.005312
11.404972	747.107915	11.010317
11.945296	740.171103	11.015322
11.667751	742.987843	11.020327
11.557978	740.698179	11.025331
11.854297	738.457286	11.030336
11.699750	746.050186	11.035341
11.814679	742.417313	11.040346
11.803976	745.398083	11.045351
11.759874	747.191939	11.050355
11.704225	750.451130	11.055360
11.527848	759.058402	11.060365
12.066916	765.122914	11.065370
12.044367	774.954676	11.070375
12.014841	780.559501	11.075379
12.277924	778.117312	11.080384
12.234558	782.495829	11.085389
12.357392	779.218098	11.090394
12.427601	776.754631	11.095399
12.574286	775.567410	11.100403
12.585384	782.510975	11.105408
12.142408	788.115516	11.110413
12.654238	779.962598	11.115418
12.420044	788.615381	11.120423
12.535742	788.751511	11.125427
12.600714	779.425582	11.130432
12.340503	791.738105	11.135437
13.077891	800.679070	11.140442
13.014922	806.394903	11.145447
13.213778	795.218234	11.150451
13.087374	798.395676	11.155456
12.938257	801.458464	11.160461
12.768664	781.288334	11.165466
13.046887	792.903080	11.170471
13.117376	802.347838	11.175475
13.206440	808.310672	11.180480
12.996549	822.067654	11.185485
13.395083	809.237919	11.190490
13.179780	823.795329	11.195495
13.338095	821.019739	11.200499
13.553312	820.815124	11.205504
13.201891	819.644269	11.210509
13.581264	817.350691	11.215514
13.260499	826.454147	11.220519
13.387271	824.610893	11.225523
13.434929	826.719725	11.230528
13.598988	826.340332	11.235533
13.724461	822.765685	11.240538
13.501650	833.900531	11.245543
13.783091	828.310768	11.250547
13.790371	831.173563	11.255552
13.266782	830.665720	11.260557
13.553199	829.867817	11.265562
14.061810	846.331557	11.270567
13.953450	859.162421	11.275571
14.230689	851.308672	11.280576
14.104489	865.274710	11.285581
14.031488	857.826930	11.290586
13.920959	859.147240	11.295591
14.215060	860.275268	11.300595
14.151409	863.324436	11.305600
13.988472	862.661288	11.310605
14.612871	854.137113	11.315610
14.369863	857.642269	11.320615
14.228299	855.425471	11.325619
14.405978	876.337275	11.330624
14.376512	867.053163	11.335629
14.310739	862.218983	11.340634
14.444675	868.020133	11.345639
14.040712	871.230824	11.350643
14.454381	876.168868	11.355648
14.932558	896.821446	11.360653
15.121725	892.930673	11.365658
14.949093	894.623615	11.370663
15.046660	895.104860	11.375667
14.957750	875.998859	11.380672
14.825348	867.298905	11.385677
14.892175	877.359346	11.390682
15.008510	896.263912	11.395687
14.960730	893.764048	11.400691
15.163301	896.693483	11.405696
15.183432	903.515809	11.410701
15.549312	893.312278	11.415706
15.148421	900.495090	11.420711
14.940257	902.997999	11.425715
15.141185	896.085286	11.430720
15.025179	904.470111	11.435725
15.232355	895.490457	11.440730
15.201474	898.214262	11.445735
15.202673	895.493683	11.450739
15.617637	905.873953	11.455744
15.499315	920.233051	11.460749
15.807741	921.857150	11.465754
15.591208	934.572861	11.470759
15.560962	935.102881	11.475763
15.846597	934.264094	11.480768
15.686175	929.787210	11.485773
15.971464	925.773857	11.490778
15.929569	936.553472	11.495783
15.913415	928.062036	11.500787
16.163389	931.928576	11.505792
15.951507	932.664199	11.510797
16.115127	931.720287	11.515802
15.988351	923.125065	11.520807
15.993241	934.543811	11.525811
16.092966	932.988728	11.530816
15.879199	935.347447	11.535821
16.246340	933.099960	11.540826
15.991467	928.682299	11.545831
16.380800	927.341238	11.550835
16.516615	938.929928	11.555840
16.435034	955.579401	11.560845
16.961138	951.721608	11.565850
16.755477	944.261825	11.570855
16.705861	938.376296	11.575859
16.704658	933.128065	11.580864
16.585034	942.060728	11.585869
16.936798	927.352185	11.590874
16.490645	936.516713	11.595879
16.607235	952.569986	11.600883
16.951056	962.229887	11.605888
16.994962	973.726025	11.610893
16.905016	967.287058	11.615898
17.000516	974.600479	11.620903
17.022656	975.913831	11.625907
16.920563	974.313659	11.630912
16.751921	976.124253	11.635917
16.909513	973.216276	11.640922
17.075052	970.600367	11.645927
16.890367	974.520478	11.650931
17.094361	971.598792	11.655936
17.043472	971.341997	11.660941
17.291925	982.449098	11.665946
17.482954	988.074022	11.670951
17.569105	984.890412	11.675955
17.748781	984.286158	11.680960
17.352775	992.690462	11.685965
17.594987	984.891118	11.690970
17.415986	994.997160	11.695975
17.584293	991.887183	11.700979
17.980749	984.694064	11.705984
17.749400	992.721995	11.710989
17.859406	991.624193	11.715994
18.218255	989.617735	11.720999
18.080101	985.927391	11.726003
17.962060	985.058366	11.731008
17.861087	987.925842	11.736013
18.182951	982.764844	11.741018
18.168709	981.240550	11.746023
17.894364	986.588017	11.751027
18.258935	985.777640	11.756032
17.711600	985.459672	11.761037
17.705042	990.791236	11.766042
18.075554	1000.710277	11.771047
18.158590	1012.111887	11.776051
18.212018	1015.347431	11.781056
18.401585	1030.589576	11.786061
18.703049	1020.574440	11.791066
18.562822	1020.024366	11.796071
18.103524	1025.664718	11.801075
18.587679	1022.482276	11.806080
18.654450	1022.766573	11.811085
18.708499	1026.293778	11.816090
18.568013	1033.536051	11.821095
18.515225	1027.521672	11.826099
18.825305	1027.883863	11.831104
18.811906	1038.649546	11.836109
19.012267	1041.237138	11.841114
19.106882	1046.194591	11.846119
19.119386	1051.009012	11.851123
19.245155	1054.393887	11.856128
18.953365	1043.006685	11.861133
19.225408	1050.441806	11.866138
19.300095	1059.696812	11.871143
19.098347	1057.401265	11.876147
19.014210	1058.190641	11.881152
18.808689	1064.079134	11.886157
19.047213	1054.473014	11.891162
19.166240	1059.439194	11.896167
19.433771	1065.078755	11.901171
19.506655	1065.966097	11.906176
19.106573	1063.273220	11.911181
19.790811	1062.777732	11.916186
19.716415	1073.471163	11.921191
19.639958	1074.954804	11.926195
19.749023	1067.884761	11.931200
19.720762	1082.669658	11.936205
20.103661	1088.628321	11.941210
20.049663	1080.746853	11.946215
19.652535	1068.643092	11.951219
19.961731	1083.913524	11.956224
19.632613	1089.619876	11.961229
20.161538	1092.606115	11.966234
20.046152	1091.411781	11.971239
19.883149	1092.070223	11.976243
20.138928	1098.252610	11.981248
20.122101	1096.946354	11.986253
20.240574	1099.054970	11.991258
20.047644	1093.261628	11.996263
20.162009	1099.127500	12.001267
20.160684	1102.698251	12.006272
20.017106	1094.889416	12.011277
20.152423	1094.907294	12.016282
20.677856	1104.421620	12.021287
20.446479	1119.883977	12.026291
20.514552	1103.397402	12.031296
20.209149	1107.699532	12.036301
20.478269	1118.333472	12.041306
20.599469	1122.476090	12.046311
20.389408	1119.208801	12.051315
20.517653	1099.110581	12.056320
20.360325	1096.104566	12.061325
20.611310	1097.218988	12.066330
20.419923	1102.654198	12.071335
20.163712	1102.715601	12.076339
20.600716	1105.625034	12.081344
20.455734	1107.343554	12.086349
20.620973	1100.255073	12.091354
20.859468	1103.030575	12.096359
20.653561	1100.866582	12.101363
20.702697	1105.673601	12.106368
20.609519	1109.060293	12.111373
20.773723	1093.674968	12.116378
20.698409	1105.757974	12.121383
20.809588	1107.818866	12.126387
21.031925	1091.913296	12.131392
20.373558	1084.689665	12.136397
20.415195	1074.960383	12.141402
20.712770	1063.446040	12.146407
20.180320	1065.223203	12.151411
20.345887	1065.037545	12.156416
20.296260	1062.865978	12.161421
20.463575	1068.663463	12.166426
20.513825	1060.683370	12.171431
20.357941	1067.820875	12.176435
20.815869	1057.525272	12.181440
20.457441	1070.640655	12.186445
20.581396	1059.510427	12.191450
20.494374	1063.435486	12.196455
20.523201	1074.349014	12.201459
20.583251	1063.853498	12.206464
20.422491	1070.979165	12.211469
20.517264	1062.134041	12.216474
20.652163	1057.852882	12.221479
20.251917	1065.269078	12.226483
20.317668	1057.232894	12.231488
20.168706	1067.449320	12.236493
20.313421	1069.258833	12.241498
20.572327	1079.337666	12.246503
20.147249	1068.883254	12.251507
20.345531	1068.457393	12.256512
20.215470	1077.164705	12.261517
20.186781	1071.633780	12.266522
20.497045	1079.122748	12.271527
20.592752	1078.729019	12.276531
20.660704	1079.691271	12.281536
20.365041	1076.634779	12.286541
20.307079	1072.292907	12.291546
20.364538	1075.587750	12.296551
20.229593	1071.964688	12.301555
20.916115	1076.649529	12.306560
20.380229	1082.398321	12.311565
20.594796	1064.697730	12.316570
20.325021	1066.813071	12.321575
20.218968	1083.542294	12.326579
20.887340	1063.932026	12.331584
20.675068	1072.646140	12.336589
20.467348	1071.996433	12.341594
20.592821	1073.364281	12.346599
20.653812	1076.240636	12.351603
20.830176	1076.961651	12.356608
20.667787	1076.689520	12.361613
20.497804	1079.292033	12.366618
20.725795	1072.083161	12.371623
20.425288	1082.531944	12.376627
20.923015	1072.364034	12.381632
20.833845	1067.211793	12.386637
20.406966	1050.851536	12.391642
20.585191	1042.586092	12.396647
20.565682	1047.809349	12.401651
20.489011	1044.684815	12.406656
20.324781	1050.901056	12.411661
20.573156	1044.871751	12.416666
20.413813	1052.317330	12.421671
20.450672	1049.827595	12.426675
20.245119	1043.429113	12.431680
20.065830	1047.799426	12.436685
20.175824	1049.188665	12.441690
20.643218	1047.981810	12.446695
20.325782	1056.950827	12.451699
20.644118	1038.643891	12.456704
20.267201	1052.642213	12.461709
20.522179	1055.105970	12.466714
20.432003	1044.079300	12.471719
20.156117	1052.988067	12.476723
20.404745	1056.440085	12.481728
20.650068	1072.299479	12.486733
20.741920	1059.247185	12.491738
20.656989	1057.538602	12.496743
20.557594	1056.778570	12.501747
20.649850	1050.513948	12.506752
20.549561	1052.343613	12.511757
20.829183	1051.999403	12.516762
20.911981	1050.199407	12.521767
20.385848	1051.035626	12.526771
20.704211	1056.119831	12.531776
20.538847	1056.655637	12.536781
20.688295	1053.763137	12.541786
20.680959	1031.909274	12.546791
20.247869	1020.028925	12.551795
20.303890	1015.637348	12.556800
20.282282	1031.439918	12.561805
20.444904	1041.882616	12.566810
20.793858	1038.846325	12.571815
20.606711	1030.457803	12.576819
20.235066	1030.302635	12.581824
20.269415	1027.915813	12.586829
20.210701	1027.180836	12.591834
20.196489	1047.809658	12.596839
20.464990	1051.982382	12.601843
20.650051	1053.091546	12.606848
20.350996	1061.340065	12.611853
20.243604	1060.365250	12.616858
20.461433	1058.687228	12.621863
20.138279	1061.520766	12.626867
20.440242	1058.156050	12.631872
20.473059	1058.090921	12.636877
20.435817	1061.818791	12.641882
20.477389	1059.588520	12.646887
20.426724	1062.689279	12.651891
20.632416	1053.503167	12.656896
20.457435	1062.444734	12.661901
20.425937	1062.402481	12.666906
20.697266	1056.123486	12.671911
20.608183	1060.704936	12.676915
20.550501	1053.473825	12.681920
20.752015	1049.385485	12.686925
20.443286	1038.994544	12.691930
20.171236	1040.857913	12.696935
20.129776	1034.944233	12.701939
20.536851	1035.103281	12.706944
20.609908	1046.829811	12.711949
20.402535	1044.421614	12.716954
20.459429	1041.173267	12.721959
20.166765	1044.672194	12.726963
20.606420	1046.030930	12.731968
20.801740	1041.462573	12.736973
20.657710	1044.204454	12.741978
20.664539	1031.719299	12.746983
20.626353	1039.344257	12.751987
20.602012	1030.923458	12.756992
20.324494	1043.538596	12.761997
20.283288	1045.872963	12.767002
20.454658	1036.894202	12.772007
20.236460	1034.856768	12.777011
20.333822	1036.886734	12.782016
20.546690	1040.259291	12.787021
20.294620	1036.514559	12.792026
20.629594	1036.161521	12.797031
20.535878	1040.363629	12.802035
20.472894	1032.532510	12.807040
20.604837	1032.729135	12.812045
20.440817	1036.161806	12.817050
20.846181	1032.749060	12.822055
20.182075	1042.855235	12.827059
20.390200	1029.983133	12.832064
20.505688	1042.780030	12.837069
20.708643	1038.973759	12.842074
20.880113	1033.544974	12.847079
20.806043	1043.743130	12.852083
20.658728	1039.130070	12.857088
20.263332	1031.798283	12.862093
20.372115	1039.954928	12.867098
20.528360	1032.929420	12.872103
20.501736	1041.533474	12.877107
20.547628	1025.358053	12.882112
19.999570	1024.887223	12.887117
20.195213	1030.926196	12.892122
20.362895	1032.468671	12.897127
20.115823	1037.182554	12.902131
20.709360	1032.299929	12.907136
20.695720	1043.429957	12.912141
20.411224	1041.951918	12.917146
20.751782	1040.538196	12.922151
20.312012	1047.410289	12.927155
20.597496	1035.716533	12.932160
20.483656	1038.346357	12.937165
20.362278	1033.897908	12.942170
20.274484	1031.593651	12.947175
20.125012	1046.281141	12.952179
20.684854	1046.822708	12.957184
20.494872	1050.128626	12.962189
20.534384	1044.851781	12.967194
20.329845	1043.083424	12.972199
19.862830	1048.075262	12.977203
20.324292	1044.756076	12.982208
20.365567	1047.908403	12.987213
20.399550	1048.543309	12.992218
20.228985	1050.794223	12.997223
20.172326	1060.510183	13.002227
20.664595	1046.277465	13.007232
20.665302	1046.769433	13.012237
20.252464	1054.764841	13.017242
20.729480	1052.545547	13.022247
20.301734	1051.065123	13.027251
20.825394	1048.466200	13.032256
20.656749	1056.440007	13.037261
20.553894	1052.291396	13.042266
20.916781	1057.742267	13.047271
20.564399	1041.964694	13.052275
20.288266	1032.749785	13.057280
20.304936	1036.185176	13.062285
20.371448	1029.462587	13.067290
20.575164	1026.969898	13.072295
20.496700	1030.261178	13.077299
20.329394	1033.740107	13.082304
20.070880	1036.060244	13.087309
20.439640	1043.710188	13.092314
20.878795	1035.961412	13.097319
20.658926	1043.853489	13.102323
20.768170	1034.047214	13.107328
20.831381	1027.394543	13.112333
20.602886	1029.858135	13.117338
20.706261	1041.277027	13.122343
20.452246	1035.545495	13.127347
20.501112	1030.894838	13.132352
20.195289	1037.067420	13.137357
20.058659	1028.598297	13.142362
20.360652	1021.488041	13.147367
20.223596	1039.561091	13.152371
20.510936	1029.988205	13.157376
20.381983	1032.084234	13.162381
20.579728	1042.338389	13.167386
20.182174	1033.344712	13.172391
20.623277	1037.441012	13.177395
20.682207	1039.742057	13.182400
20.460039	1038.785550	13.187405
20.096935	1045.421470	13.192410
20.628280	1037.344151	13.197415
20.288397	1047.024847	13.202419
20.681945	1041.783003	13.207424
20.542560	1036.253977	13.212429
20.383833	1034.134512	13.217434
20.538292	1032.280507	13.222439
20.376620	1034.621470	13.227443
20.646367	1034.439697	13.232448
20.453236	1044.983298	13.237453
20.226831	1039.348294	13.242458
20.515749	1027.384317	13.247463
20.306199	1035.675320	13.252467
20.623504	1037.428913	13.257472
20.601436	1039.130974	13.262477
20.610406	1040.667223	13.267482
20.284295	1040.582069	13.272487
20.276807	1042.390622	13.277491
20.540568	1037.713571	13.282496
20.485956	1048.026907	13.287501
20.296373	1044.562388	13.292506
20.415021	1040.239668	13.297511
20.437459	1038.635395	13.302515
20.406681	1037.501693	13.307520
20.524229	1042.245736	13.312525
20.673177	1038.875466	13.317530
20.580806	1032.406893	13.322535
20.252935	1048.553245	13.327539
20.701660	1041.102584	13.332544
20.517969	1047.208378	13.337549
20.107581	1050.260847	13.342554
20.488778	1037.834254	13.347559
20.447243	1044.366838	13.352563
20.345558	1054.476360	13.357568
20.480244	1041.885640	13.362573
20.417835	1040.581928	13.367578
20.526017	1036.084246	13.372583
20.351137	1043.639540	13.377587
20.582985	1040.453181	13.382592
20.757916	1037.178122	13.387597
20.342761	1047.452764	13.392602
20.663226	1043.186168	13.397607
20.420407	1052.553319	13.402611
20.178786	1042.842429	13.407616
20.398711	1054.020374	13.412621
20.490200	1043.985094	13.417626
20.653223	1047.654207	13.422631
20.349172	1051.140758	13.427635
20.485412	1048.527931	13.432640
20.698959	1050.872130	13.437645
20.168523	1044.664251	13.442650
20.580614	1038.457436	13.447655
20.349628	1050.861716	13.452659
20.648319	1051.220993	13.457664
20.556488	1032.835974	13.462669
20.337796	1022.913266	13.467674
20.375723	1018.806870	13.472679
20.502593	1030.389174	13.477683
20.532208	1022.844511	13.482688
20.477082	1025.304106	13.487693
20.137028	1021.680653	13.492698
20.604385	1024.228810	13.497703
20.652495	1013.325196	13.502707
20.507829	1014.564226	13.507712
20.167444	1021.308483	13.512717
20.284546	1025.492731	13.517722
20.263136	1016.331827	13.522727
20.050633	1042.663414	13.527731
20.323244	1046.773975	13.532736
20.631010	1053.115219	13.537741
20.414802	1060.393240	13.542746
20.683232	1053.575350	13.547751
20.792197	1051.591394	13.552755
20.547101	1037.277585	13.557760
20.547678	1030.567089	13.562765
20.278530	1024.333313	13.567770
20.249729	1011.571563	13.572775
19.970990	1028.503322	13.577779
20.624026	1034.593930	13.582784
20.752554	1049.831637	13.587789
20.221943	1043.888735	13.592794
20.551392	1049.441137	13.597799
20.299804	1042.499601	13.602803
20.567170	1044.691701	13.607808
20.208554	1044.526569	13.612813
20.091478	1054.526573	13.617818
20.559998	1052.844839	13.622823
20.291642	1057.743487	13.627827
20.553030	1060.360776	13.632832
20.480932	1057.707056	13.637837
20.505530	1060.229639	13.642842
20.430065	1061.441864	13.647847
20.803905	1067.562826	13.652851
20.471603	1052.192079	13.657856
20.150374	1038.544898	13.662861
20.562185	1053.726386	13.667866
20.561924	1044.584170	13.672871
20.118688	1050.543692	13.677875
20.613607	1059.427295	13.682880
20.502932	1053.560920	13.687885
19.973679	1052.962500	13.692890
20.362814	1050.705180	13.697895
20.497982	1060.814776	13.702899
20.693843	1056.659522	13.707904
20.616711	1070.263088	13.712909
20.402831	1061.683254	13.717914
20.525197	1045.560274	13.722919
20.056436	1051.963872	13.727923
20.589557	1055.993456	13.732928
20.682665	1050.905194	13.737933
20.504683	1043.428328	13.742938
20.377826	1032.483217	13.747943
20.035482	1042.195844	13.752947
20.537603	1051.264387	13.757952
20.396458	1060.735184	13.762957
20.651291	1062.184907	13.767962
20.747337	1050.179130	13.772967
20.286850	1041.578715	13.777971
20.270532	1039.501194	13.782976
20.539318	1043.241753	13.787981
20.497230	1048.145311	13.792986
20.208740	1039.154736	13.797991
20.323941	1044.985756	13.802995
20.710606	1042.774567	13.808000
20.442601	1038.507211	13.813005
20.164178	1037.695306	13.818010
20.498967	1046.254331	13.823015
20.627665	1058.768417	13.828019
20.296064	1041.102927	13.833024
20.336711	1042.739788	13.838029
20.407421	1060.487966	13.843034
20.403989	1059.851410	13.848039
20.478646	1074.085254	13.853043
20.639451	1068.782746	13.858048
20.759902	1054.328606	13.863053
20.068099	1037.340365	13.868058
20.452732	1032.038441	13.873063
20.184864	1039.898745	13.878067
20.585712	1061.825551	13.883072
20.515275	1057.886250	13.888077
20.290392	1043.778962	13.893082
20.754936	1043.190775	13.898087
20.351106	1037.538336	13.903091
20.437590	1036.319693	13.908096
20.533246	1029.836901	13.913101
20.510595	1034.887176	13.918106
20.565175	1025.280452	13.923111
20.401879	1030.081903	13.928115
20.302585	1037.803346	13.933120
20.453228	1035.565143	13.938125
20.279916	1033.345495	13.943130
20.477066	1037.100632	13.948135
20.281071	1043.351901	13.953139
20.394502	1037.068136	13.958144
20.459949	1041.825220	13.963149
20.464683	1046.081018	13.968154
20.623211	1039.294858	13.973159
20.371195	1034.234840	13.978163
20.618798	1047.871751	13.983168
20.563420	1035.915371	13.988173
20.340196	1032.859951	13.993178
20.502142	1035.694962	13.998183
20.351134	1040.377753	14.003187
20.567302	1036.283926	14.008192
20.450291	1044.617658	14.013210
20.400008	1043.639411	14.018227
20.694474	1033.255974	14.023245
20.207388	1038.469704	14.028263
20.684638	1038.977217	14.033280
20.456268	1037.210964	14.038298
20.395235	1047.599712	14.043315
20.375851	1033.015956	14.048333
20.399316	1037.155657	14.053351
20.891246	1038.794996	14.058368
20.942445	1029.205428	14.063386
20.438346	1040.512714	14.068403
20.584091	1036.511262	14.073421
20.507428	1031.219206	14.078439
20.506602	1041.411153	14.083456
20.667231	1048.069454	14.088474
20.845471	1063.716507	14.093491
21.035491	1052.906116	14.098509
20.359691	1052.520006	14.103527
20.696389	1050.723396	14.108544
20.952614	1065.069685	14.113562
20.773944	1077.794323	14.118579
21.078090	1068.736973	14.123597
20.742386	1057.384359	14.128615
20.627290	1047.590065	14.133632
20.780134	1059.893716	14.138650
20.768442	1073.019586	14.143667
20.985599	1070.295064	14.148685
20.861177	1080.780464	14.153703
20.918113	1072.338281	14.158720
21.270080	1075.701992	14.163738
20.918294	1078.874355	14.168755
21.034574	1071.544294	14.173773
20.930878	1080.149737	14.178791
20.880567	1087.823287	14.183808
20.903877	1078.666005	14.188826
20.978652	1085.018687	14.193843
21.036043	1079.577814	14.198861
20.443584	1085.766357	14.203879
20.827170	1080.581773	14.208896
21.089307	1077.359283	14.213914
20.616256	1082.216852	14.218931
21.137003	1080.787292	14.223949
21.038984	1093.091659	14.228967
21.281289	1095.318244	14.233984
21.097219	1103.923936	14.239002
20.871904	1112.287669	14.244019
21.059183	1111.781195	14.249037
21.086235	1101.874527	14.254055
21.034749	1117.479628	14.259072
21.171743	1098.445855	14.264090
20.918925	1105.428109	14.269107
21.123868	1106.447829	14.274125
21.460609	1118.119716	14.279143
21.377335	1127.764867	14.284160
21.394450	1127.994984	14.289178
21.217738	1135.292310	14.294195
21.502827	1135.429346	14.299213
21.735170	1139.219575	14.304231
21.520398	1138.988020	14.309248
21.599965	1123.318710	14.314266
21.223155	1126.273274	14.319283
21.635734	1133.747170	14.324301
21.709919	1140.995041	14.329319
21.452467	1146.386118	14.334336
21.822650	1144.293140	14.339354
21.666430	1146.372509	14.344371
21.591843	1139.164096	14.349389
21.588338	1133.734489	14.354407
21.215066	1141.168564	14.359424
21.748056	1134.723706	14.364442
21.593637	1153.757229	14.369459
21.748997	1148.719138	14.374477
22.029916	1142.874492	14.379495
21.832045	1136.716099	14.384512
22.239470	1143.391708	14.389530
21.873123	1141.562505	14.394547
21.917278	1140.185362	14.399565
21.682039	1143.902305	14.404583
21.642003	1149.538708	14.409600
21.952514	1139.449946	14.414618
21.601975	1153.032638	14.419635
21.822554	1140.205363	14.424653
21.874709	1148.848910	14.429671
21.956558	1145.713364	14.434688
22.246431	1147.215055	14.439706
22.164423	1147.560086	14.444723
21.980482	1141.207555	14.449741
21.991539	1149.385739	14.454759
21.891866	1153.125107	14.459776
22.280288	1139.388574	14.464794
21.893967	1153.060346	14.469811
21.766686	1143.275796	14.474829
22.089167	1145.804212	14.479847
21.964282	1148.380390	14.484864
22.072709	1138.188578	14.489882
21.677628	1150.372058	14.494899
22.092544	1144.466711	14.499917
22.144247	1157.486589	14.504935
22.264700	1167.206239	14.509952
22.651754	1166.615988	14.514970
22.331629	1164.865927	14.519987
22.154572	1154.231990	14.525005
22.189431	1162.020985	14.530023
22.345359	1172.114087	14.535040
22.615764	1164.981198	14.540058
22.346392	1176.130023	14.545075
22.399117	1174.068800	14.550093
22.681956	1173.927764	14.555111
22.546609	1180.052874	14.560128
22.584731	1154.605687	14.565146
22.344697	1155.745151	14.570163
22.479911	1165.242216	14.575181
22.477766	1162.670636	14.580199
22.453406	1172.847552	14.585216
22.520712	1172.066050	14.590234
22.438029	1186.965177	14.595251
22.624105	1175.982286	14.600269
22.959952	1174.255013	14.605287
22.547645	1185.472262	14.610304
22.675517	1171.651412	14.615322
22.803711	1175.793325	14.620339
22.757936	1180.283893	14.625357
22.690220	1172.504918	14.630375
22.551499	1178.822479	14.635392
22.448616	1171.432941	14.640410
22.263927	1190.814269	14.645427
22.530037	1175.428189	14.650445
22.735223	1167.473550	14.655463
22.592864	1179.302131	14.660480
22.735229	1180.424649	14.665498
22.778859	1184.764101	14.670515
22.823398	1185.266705	14.675533
22.763509	1181.618917	14.680551
22.800165	1210.057279	14.685568
23.028169	1208.123827	14.690586
22.984462	1216.861358	14.695603
22.875716	1214.663858	14.700621
23.281261	1211.891958	14.705639
23.140865	1226.897861	14.710656
23.134028	1214.213763	14.715674
23.186190	1213.006800	14.720691
23.129879	1208.859773	14.725709
23.271788	1205.752389	14.730727
23.201042	1197.643539	14.735744
22.999762	1186.807371	14.740762
23.241036	1194.291319	14.745779
23.246029	1199.357402	14.750797
23.561053	1205.808673	14.755815
22.933012	1193.316488	14.760832
23.465202	1201.625517	14.765850
23.579810	1193.141031	14.770867
23.060069	1186.310345	14.775885
23.170183	1183.403096	14.780903
23.167630	1201.133557	14.785920
23.495704	1197.651979	14.790938
23.495562	1205.578718	14.795955
23.117039	1204.969002	14.800973
23.364955	1201.160426	14.805991
23.424497	1209.683277	14.811008
23.560756	1208.986732	14.816026
23.525418	1208.734421	14.821043
23.530052	1214.344848	14.826061
23.189073	1209.746136	14.831079
23.205187	1213.953129	14.836096
23.129479	1209.672338	14.841114
22.969333	1216.468400	14.846131
23.147410	1217.605674	14.851149
23.572188	1228.747642	14.856167
23.598170	1233.994439	14.861184
23.636231	1239.391898	14.866202
23.882393	1238.242082	14.871219
23.980231	1241.635355	14.876237
23.922076	1240.280813	14.881255
24.087972	1236.505761	14.886272
23.836415	1226.807046	14.891290
23.852599	1217.377099	14.896307
23.591934	1216.559816	14.901325
23.993140	1216.675187	14.906343
23.662581	1224.579131	14.911360
24.128383	1233.841035	14.916378
23.910638	1223.347249	14.921395
23.967406	1225.002535	14.926413
24.089499	1222.400117	14.931431
23.823936	1222.851508	14.936448
24.145443	1224.403218	14.941466
23.891357	1227.147886	14.946483
23.885860	1238.267254	14.951501
24.196339	1233.155627	14.956519
24.214946	1238.505851	14.961536
24.083732	1234.675939	14.966554
23.922142	1232.587542	14.971571
23.919804	1240.149697	14.976589
24.014505	1228.615037	14.981607
23.986693	1237.872304	14.986624
24.009930	1238.667752	14.991642
24.308483	1244.245467	14.996659
24.134542	1246.109020	15.001677
24.398105	1239.505737	15.006695
24.424289	1245.677471	15.011712
24.226484	1246.794475	15.016730
24.520665	1241.776683	15.021747
24.350905	1245.914229	15.026765
24.335985	1239.328624	15.031783
24.264018	1244.139576	15.036800
24.335441	1238.351903	15.041818
24.514566	1239.135071	15.046835
24.282442	1247.967170	15.051853
24.415609	1243.346304	15.056871
24.251630	1241.185925	15.061888
24.344181	1243.980702	15.066906
24.579697	1238.050449	15.071923
24.439609	1248.895556	15.076941
24.613651	1256.150366	15.081959
24.692662	1268.389677	15.086976
24.595448	1267.169568	15.091994
24.811192	1271.515414	15.097011
24.595070	1270.861701	15.102029
24.980931	1267.168750	15.107047
24.556171	1260.342542	15.112064
24.778347	1257.404821	15.117082
24.973957	1263.964043	15.122099
24.697644	1254.869386	15.127117
24.589518	1249.270014	15.132135
24.774955	1270.013681	15.137152
25.108514	1263.148318	15.142170
25.229771	1270.424926	15.147187
24.975628	1258.491265	15.152205
24.805540	1245.903967	15.157223
24.807899	1245.120236	15.162240
24.786194	1254.963295	15.167258
25.061694	1262.260129	15.172275
25.078443	1272.885963	15.177293
24.904674	1260.955997	15.182311
25.080808	1267.503384	15.187328
24.903225	1272.421643	15.192346
25.099498	1268.136780	15.197363
24.990699	1269.708366	15.202381
25.088884	1263.965966	15.207399
25.047518	1265.465445	15.212416
25.014236	1262.097333	15.217434
25.217595	1260.608266	15.222451
24.941628	1273.129936	15.227469
25.078553	1270.197158	15.232487
25.021933	1272.667298	15.237504
25.192330	1273.145111	15.242522
25.188576	1264.401028	15.247539
25.054912	1279.044104	15.252557
25.067865	1274.510046	15.257575
25.584977	1294.606223	15.262592
25.257824	1303.493625	15.267610
25.526911	1298.366555	15.272627
25.259919	1308.359676	15.277645
25.486748	1304.523762	15.282663
25.359128	1310.007451	15.287680
25.594950	1312.227239	15.292698
25.788696	1305.623265	15.297715
25.521441	1307.403391	15.302733
25.718333	1299.721360	15.307751
25.637899	1303.828944	15.312768
25.647878	1306.260938	15.317786
25.793434	1308.703555	15.322803
25.551992	1299.666230	15.327821
25.637490	1299.617234	15.332839
25.772875	1307.630167	15.337856
25.858374	1305.118517	15.342874
25.989190	1304.063388	15.347891
25.684235	1310.068522	15.352909
25.414386	1301.019210	15.357927
25.889939	1304.128088	15.362944
25.900941	1308.700091	15.367962
26.086769	1303.021565	15.372979
25.912900	1307.231358	15.377997
26.011732	1302.971466	15.383015
26.092300	1303.010561	15.388032
25.920688	1305.031844	15.393050
25.999608	1300.188371	15.398067
25.455827	1305.165050	15.403085
25.751297	1304.347936	15.408103
25.761175	1298.321510	15.413120
25.596076	1308.928396	15.418138
26.252822	1325.352017	15.423155
26.054877	1340.209121	15.428173
26.168717	1341.502948	15.433191
26.279419	1345.090042	15.438208
26.154272	1341.905671	15.443226
26.610690	1342.027968	15.448243
26.175297	1342.692860	15.453261
26.050868	1344.572911	15.458279
26.495706	1337.635493	15.463296
25.818921	1338.699123	15.468314
26.258495	1343.427729	15.473331
26.631983	1343.727641	15.478349
26.325355	1339.965794	15.483367
26.736427	1333.755808	15.488384
26.396563	1343.445959	15.493402
26.530660	1334.959069	15.498419
26.388574	1340.219340	15.503437
26.485145	1334.463799	15.508455
26.647846	1333.074022	15.513472
26.449839	1339.412120	15.518490
26.654861	1340.327235	15.523507
26.552174	1343.706897	15.528525
26.596976	1340.121812	15.533543
26.560391	1336.836010	15.538560
26.472961	1336.782347	15.543578
26.549973	1334.829703	15.548595
26.277841	1345.227164	15.553613
26.142384	1342.903340	15.558631
26.683429	1343.965426	15.563648
26.973167	1361.679350	15.568666
27.136095	1357.485513	15.573683
26.690597	1368.538303	15.578701
26.841120	1370.838562	15.583719
27.201512	1362.690742	15.588736
27.106489	1366.758197	15.593754
27.008131	1358.657594	15.598771
26.895653	1364.570700	15.603789
26.954902	1366.159538	15.608807
27.372289	1365.146002	15.613824
27.010266	1367.813527	15.618842
27.037678	1359.824216	15.623859
27.027027	1370.141447	15.628877
27.170228	1367.544289	15.633895
27.388508	1366.823643	15.638912
26.823118	1371.319281	15.643930
27.342467	1360.973678	15.648947
27.369156	1360.230893	15.653965
26.975079	1369.639475	15.658983
27.328134	1368.919356	15.664000
27.180003	1375.955043	15.669018
27.277100	1366.943119	15.674035
27.214028	1369.346662	15.679053
27.370713	1368.461228	15.684071
27.602639	1366.748936	15.689088
27.146703	1371.471730	15.694106
27.681401	1357.554353	15.699123
27.596700	1369.355801	15.704141
27.219993	1359.827188	15.709159
27.537505	1361.293032	15.714176
27.294556	1370.527280	15.719194
27.149935	1359.943863	15.724211
27.134059	1365.876170	15.729229
27.445984	1359.814912	15.734247
27.562245	1361.131951	15.739264
27.517888	1369.622703	15.744282
27.787342	1383.628983	15.749299
27.718636	1388.417440	15.754317
27.794632	1391.694677	15.759335
27.958448	1392.308043	15.764352
27.484934	1379.377327	15.769370
27.541620	1392.231446	15.774387
27.753339	1389.152215	15.779405
27.780138	1399.313264	15.784423
27.906376	1396.585880	15.789440
27.555107	1403.869494	15.794458
27.988633	1396.857558	15.799475
27.981616	1391.827980	15.804493
27.891821	1390.434424	15.809511
27.962263	1386.136563	15.814528
27.838979	1397.348774	15.819546
27.921631	1386.851788	15.824563
27.805736	1400.401217	15.829581
27.761811	1393.474875	15.834599
27.747812	1394.103231	15.839616
28.098389	1415.591578	15.844634
28.084194	1416.517281	15.849651
28.350228	1418.483718	15.854669
28.277652	1421.753985	15.859687
28.669216	1422.968914	15.864704
28.471024	1422.201430	15.869722
28.439995	1416.649475	15.874739
28.439220	1408.311474	15.879757
28.520576	1419.461174	15.884775
28.493622	1392.972339	15.889792
28.448903	1406.932008	15.894810
28.539978	1404.585413	15.899827
28.575859	1394.836806	15.904845
28.236937	1405.553288	15.909863
28.371577	1413.468867	15.914880
28.486897	1426.054104	15.919898
28.753531	1424.653247	15.924915
29.007760	1430.975884	15.929933
28.591680	1414.668774	15.934951
28.740630	1405.823956	15.939968
28.543235	1398.929169	15.944986
28.584008	1421.133141	15.950003
28.793124	1424.459942	15.955021
28.559563	1429.306168	15.960039
28.857125	1424.100577	15.965056
28.806321	1431.286728	15.970074
28.952684	1426.361667	15.975091
29.112202	1419.958164	15.980109
28.649412	1428.908177	15.985127
28.981487	1420.616184	15.990144
28.642379	1427.922253	15.995162
28.914857	1425.048051	16.000179
29.176259	1426.654204	16.005197
29.301546	1421.679021	16.010215
29.090869	1426.295857	16.015232
29.167234	1432.706642	16.020250
29.132417	1421.822510	16.025267
29.163576	1426.607635	16.030285
29.052982	1430.893105	16.035303
29.370251	1429.043706	16.040320
28.975100	1430.231527	16.045338
28.794770	1430.693711	16.050355
29.309515	1423.645998	16.055373
28.993041	1423.720107	16.060391
29.262444	1431.655888	16.065408
29.139711	1428.501788	16.070426
28.900969	1425.204950	16.075443
29.117317	1426.186693	16.080461
28.757865	1438.482711	16.085479
29.364490	1443.532359	16.090496
29.048569	1455.069509	16.095514
29.291960	1465.514609	16.100531
29.456923	1458.241086	16.105549
29.460229	1469.555077	16.110567
29.521534	1455.728058	16.115584
29.460085	1469.202009	16.120602
29.605391	1458.498342	16.125619
29.667906	1457.601180	16.130637
29.122612	1468.538609	16.135655
29.632097	1457.160203	16.140672
29.630471	1466.104325	16.145690
29.679139	1481.265958	16.150707
30.088093	1486.893016	16.155725
29.740709	1488.280871	16.160743
30.055704	1488.650682	16.165760
29.771486	1480.444370	16.170778
29.875303	1472.326401	16.175795
29.962768	1476.680972	16.180813
29.705214	1479.742431	16.185831
29.943368	1473.520640	16.190848
30.195888	1486.128093	16.195866
30.041182	1494.509097	16.200883
30.215316	1480.724622	16.205901
29.958848	1488.289686	16.210919
30.201875	1491.907623	16.215936
30.318492	1498.840577	16.220954
30.148571	1484.758602	16.225971
30.544428	1485.628344	16.230989
29.860264	1484.308344	16.236007
30.157398	1480.985012	16.241024
30.591554	1489.025113	16.246042
30.284641	1495.521442	16.251059
30.530981	1480.588101	16.256077
30.477062	1483.882148	16.261095
30.151018	1473.848280	16.266112
30.049312	1479.428577	16.271130
30.391800	1482.428152	16.276147
30.460679	1484.190867	16.281165
30.245508	1488.233473	16.286183
30.504925	1485.470672	16.291200
30.665220	1476.660969	16.296218
30.340808	1491.218273	16.301235
30.501602	1486.574048	16.306253
30.289496	1494.584304	16.311271
30.420763	1494.082034	16.316288
30.406353	1495.331834	16.321306
30.383265	1487.587259	16.326323
30.702854	1493.300148	16.331341
30.546070	1510.980077	16.336359
30.751675	1512.251418	16.341376
30.703117	1519.723558	16.346394
30.585376	1517.614754	16.351411
31.233836	1513.417366	16.356429
31.073540	1517.966418	16.361447
31.139817	1517.520919	16.366464
31.173172	1521.439733	16.371482
30.597779	1522.613836	16.376499
31.111219	1522.474559	16.381517
30.998652	1521.136535	16.386535
31.132763	1524.937028	16.391552
31.133688	1523.864847	16.396570
30.886267	1526.332427	16.401587
31.267878	1518.034839	16.406605
30.715898	1524.330370	16.411623
30.778880	1511.653754	16.416640
30.918986	1513.752767	16.421658
30.813729	1528.401787	16.426675
31.238243	1537.521815	16.431693
31.375275	1546.738827	16.436711
31.352152	1545.198549	16.441728
31.420006	1544.824374	16.446746
31.304658	1557.539329	16.451763
31.585170	1547.422036	16.456781
31.388494	1550.502903	16.461799
31.486237	1550.359139	16.466816
31.706024	1544.905563	16.471834
31.375062	1557.082298	16.476851
31.644442	1540.457280	16.481869
31.714148	1540.967681	16.486887
31.697615	1552.815036	16.491904
31.983010	1545.142356	16.496922
31.764745	1547.717766	16.501939
32.235327	1549.780591	16.506957
31.982012	1541.493020	16.511975
31.927836	1542.715345	16.516992
32.081736	1538.677847	16.522010
31.881074	1525.653141	16.527027
31.712572	1514.339569	16.532045
31.663198	1521.818919	16.537063
31.610081	1530.048454	16.542080
32.051007	1533.987998	16.547098
31.862593	1541.772694	16.552115
32.014171	1536.332359	16.557133
32.046182	1537.367896	16.562151
32.023142	1544.312135	16.567168
32.121890	1538.955735	16.572186
32.067956	1547.192488	16.577203
32.094044	1548.591570	16.582221
32.015142	1542.990570	16.587239
32.323812	1549.259742	16.592256
32.385356	1536.304109	16.597274
31.895014	1547.615095	16.602291
32.344993	1536.610292	16.607309
32.183214	1543.403619	16.612327
32.044082	1544.177788	16.617344
32.358839	1541.224458	16.622362
32.271204	1548.856223	16.627379
32.701346	1565.448403	16.632397
32.689640	1567.521298	16.637415
32.683199	1565.308214	16.642432
32.579203	1549.751099	16.647450
32.398636	1551.795867	16.652467
32.505828	1553.329099	16.657485
32.795909	1571.772358	16.662503
32.706978	1581.366798	16.667520
32.732368	1581.362783	16.672538
32.613832	1586.606014	16.677555
32.805212	1573.758633	16.682573
32.941846	1581.121826	16.687591
32.695001	1577.790063	16.692608
32.937495	1574.841960	16.697626
32.789019	1581.160463	16.702643
32.698130	1575.267978	16.707661
32.925705	1571.550646	16.712679
32.999588	1576.805657	16.717696
32.990917	1573.050496	16.722714
32.791936	1579.620886	16.727731
32.965192	1579.472158	16.732749
33.107705	1580.387820	16.737767
32.816366	1581.730563	16.742784
33.047376	1570.348507	16.747802
32.870612	1586.312309	16.752819
32.718104	1576.598348	16.757837
33.166089	1589.531022	16.762855
33.271541	1593.701852	16.767872
33.441807	1605.465183	16.772890
33.263653	1602.622708	16.777907
33.348713	1593.401768	16.782925
33.481956	1597.291299	16.787943
33.209340	1601.019824	16.792960
33.270268	1597.609079	16.797978
33.509825	1597.882380	16.802995
33.234307	1593.706495	16.808013
33.433692	1600.717538	16.813031
33.201565	1599.688028	16.818048
33.387874	1596.985634	16.823066
33.314406	1597.913723	16.828083
33.652273	1611.618287	16.833101
33.768809	1617.447774	16.838119
33.704147	1632.096716	16.843136
33.901322	1631.385717	16.848154
33.760660	1630.784448	16.853171
33.841147	1627.263604	16.858189
33.905889	1627.915593	16.863207
33.935431	1625.311348	16.868224
33.832639	1627.611150	16.873242
33.857222	1631.291493	16.878259
33.872650	1626.698725	16.883277
34.075403	1616.305121	16.888295
33.887590	1639.167264	16.893312
33.888318	1632.243125	16.898330
33.995354	1622.942365	16.903347
34.192092	1627.814411	16.908365
34.346584	1627.804749	16.913383
34.249951	1636.764916	16.918400
34.634244	1620.728700	16.923418
34.358134	1633.437900	16.928435
34.245994	1631.447743	16.933453
34.447181	1627.119518	16.938471
34.575566	1623.608340	16.943488
34.493733	1622.447099	16.948506
34.595450	1628.587284	16.953523
34.295724	1630.331727	16.958541
34.654883	1624.081920	16.963559
34.253615	1629.591284	16.968576
34.185314	1625.150305	16.973594
34.284840	1637.069671	16.978611
34.224546	1634.029056	16.983629
34.523892	1628.598941	16.988647
34.308713	1644.945694	16.993664
34.591606	1650.912265	16.998682
35.044190	1656.887954	17.003699
34.842560	1655.163765	17.008717
34.831632	1660.979778	17.013735
34.844555	1657.722189	17.018752
35.056132	1651.185219	17.023770
34.772583	1660.401742	17.028787
34.501719	1661.473010	17.033805
34.964588	1654.323344	17.038823
34.905638	1655.396994	17.043840
34.566884	1665.834411	17.048858
34.774195	1660.838985	17.053875
35.002602	1659.556681	17.058893
35.147406	1655.773874	17.063911
35.043637	1662.013705	17.068928
35.212142	1657.996655	17.073946
35.250268	1659.609345	17.078963
35.040430	1660.480533	17.083981
35.312577	1655.668261	17.088999
34.980713	1670.426716	17.094016
35.180539	1686.616083	17.099034
35.571834	1687.039014	17.104051
35.414799	1691.559283	17.109069
35.742979	1690.423881	17.114087
35.733900	1695.898246	17.119104
35.875300	1680.051726	17.124122
35.344491	1673.924182	17.129139
35.369209	1670.017371	17.134157
35.848854	1669.441439	17.139175
35.622963	1684.792590	17.144192
35.782066	1683.949226	17.149210
35.276472	1682.675447	17.154227
35.579519	1680.252525	17.159245
35.853503	1686.190642	17.164263
35.823154	1689.446367	17.169280
36.201996	1676.754624	17.174298
35.866564	1682.153614	17.179315
35.871291	1687.623414	17.184333
36.200565	1678.682026	17.189351
35.781718	1683.755314	17.194368
35.817821	1684.742228	17.199386
36.005341	1687.592734	17.204403
35.984868	1678.345312	17.209421
36.357852	1679.450751	17.214439
35.939302	1682.842328	17.219456
35.861329	1679.521362	17.224474
35.835479	1679.650583	17.229491
35.825449	1686.566859	17.234509
36.110932	1693.535897	17.239527
36.007079	1707.282689	17.244544
36.008793	1707.475157	17.249562
36.097735	1713.290207	17.254579
36.066943	1717.216159	17.259597
36.283862	1711.199800	17.264615
36.211691	1721.232132	17.269632
36.347782	1713.429013	17.274650
36.647842	1716.766547	17.279667
36.502266	1728.528441	17.284685
36.875811	1726.324730	17.289703
36.422980	1725.065341	17.294720
37.005585	1743.186865	17.299738
37.012816	1727.639350	17.304755
36.739111	1723.166604	17.309773
36.715644	1706.152351	17.314791
36.545996	1722.399902	17.319808
36.835025	1735.070178	17.324826
37.098383	1748.501234	17.329843
36.801329	1743.726233	17.334861
36.711688	1740.860961	17.339879
36.862147	1754.347783	17.344896
36.947894	1753.931421	17.349914
37.120410	1748.762179	17.354931
36.850184	1748.857227	17.359949
37.007118	1743.923295	17.364967
36.820521	1752.633597	17.369984
37.220308	1745.117972	17.375002
36.837583	1745.895608	17.380019
36.744939	1750.039873	17.385037
37.375441	1747.262672	17.390055
37.483920	1770.225635	17.395072
37.233205	1761.672451	17.400090
37.494162	1762.749357	17.405107
37.621943	1770.000005	17.410125
37.528333	1758.384056	17.415143
37.267031	1762.180034	17.420160
37.226979	1764.144214	17.425178
37.623365	1765.474030	17.430195
37.242181	1763.914541	17.435213
37.451417	1774.462059	17.440231
37.722456	1776.257065	17.445248
37.843236	1770.740539	17.450266
38.075320	1766.355433	17.455283
37.825118	1768.095925	17.460301
38.210012	1761.005839	17.465319
37.661872	1774.971430	17.470336
38.129339	1769.484559	17.475354
38.033332	1772.572225	17.480371
37.986275	1772.845624	17.485389
38.010284	1765.094176	17.490407
37.836760	1769.989143	17.495424
37.727888	1771.655181	17.500442
38.202147	1760.798145	17.505459
38.089534	1770.592340	17.510477
38.142557	1765.629353	17.515495
38.005223	1775.972583	17.520512
37.906530	1768.365768	17.525530
38.492474	1761.754881	17.530547
38.204262	1765.725050	17.535565
38.178695	1762.963605	17.540583
38.170854	1776.404119	17.545600
38.131110	1788.972715	17.550618
38.631834	1794.611213	17.555635
38.230859	1794.738127	17.560653
38.710264	1793.311166	17.565671
39.101450	1800.065969	17.570688
38.817135	1801.818985	17.575706
39.065781	1792.027525	17.580723
38.581970	1786.025367	17.585741
38.583409	1769.412148	17.590759
38.654455	1780.200376	17.595776
38.850428	1786.242219	17.600794
39.172070	1793.795462	17.605811
38.943400	1783.822145	17.610829
38.842165	1767.764888	17.615847
38.835156	1773.792693	17.620864
39.011957	1781.818160	17.625882
39.430815	1783.554981	17.630899
38.792088	1776.064971	17.635917
38.750386	1779.297357	17.640935
39.114002	1788.456360	17.645952
39.047856	1790.588310	17.650970
39.292898	1787.486378	17.655987
38.973934	1798.679767	17.661005
39.319431	1791.004453	17.666023
39.106555	1789.086973	17.671040
39.060866	1800.820409	17.676058
39.411255	1785.733299	17.681075
39.042235	1795.262433	17.686093
38.753172	1794.367054	17.691111
39.428684	1794.762748	17.696128
39.234682	1799.925278	17.701146
39.583091	1805.062648	17.706163
39.617538	1817.172666	17.711181
40.159640	1815.487935	17.716199
39.646479	1809.660345	17.721216
39.576387	1803.006201	17.726234
39.860941	1802.784660	17.731251
40.049548	1807.686379	17.736269
39.696414	1800.525211	17.741287
39.657642	1795.627195	17.746304
39.608296	1809.210435	17.751322
39.846686	1821.110164	17.756339
39.687667	1826.168802	17.761357
40.162150	1821.135429	17.766375
39.837316	1825.224720	17.771392
39.935446	1826.963934	17.776410
40.049774	1820.154517	17.781427
39.694775	1825.660506	17.786445
40.044795	1823.438509	17.791463
40.075823	1814.893056	17.796480
39.942890	1814.874178	17.801498
40.521969	1834.672553	17.806515
40.379789	1837.591406	17.811533
40.339843	1827.089275	17.816551
40.564845	1830.981538	17.821568
40.367174	1839.240595	17.826586
40.551936	1843.818874	17.831603
40.620801	1843.149568	17.836621
40.414786	1841.905862	17.841639
40.521794	1847.418401	17.846656
40.400220	1848.642849	17.851674
40.713720	1843.932467	17.856691
40.578208	1856.432232	17.861709
41.048132	1846.008438	17.866727
40.881611	1837.826412	17.871744
40.592403	1848.216726	17.876762
40.611414	1843.117555	17.881779
40.453642	1847.516072	17.886797
40.664314	1847.283503	17.891815
40.928371	1848.594319	17.896832
40.580051	1848.897678	17.901850
40.647347	1838.303710	17.906867
41.332308	1857.613288	17.911885
41.479403	1855.290722	17.916903
41.488379	1839.560325	17.921920
41.217888	1844.965534	17.926938
41.348655	1829.244039	17.931955
41.485581	1834.947657	17.936973
41.267497	1835.994787	17.941991
41.317596	1830.542213	17.947008
41.089049	1836.370981	17.952026
41.090760	1826.726643	17.957043
41.475474	1851.909417	17.962061
41.579273	1856.134860	17.967079
41.565938	1860.675522	17.972096
41.625995	1867.200792	17.977114
41.970360	1862.481549	17.982131
41.811181	1860.396608	17.987149
41.672477	1845.744547	17.992167
41.772169	1843.888899	17.997184
41.822909	1853.459667	18.002202
41.887794	1853.900843	18.007219
42.193481	1867.185248	18.012237
42.041971	1853.480678	18.017255
41.966549	1837.678008	18.022272
41.708043	1831.074352	18.027290
42.173171	1840.225063	18.032307
42.171747	1846.402242	18.037325
42.019986	1841.690557	18.042343
42.104988	1842.409329	18.047360
42.271631	1852.299048	18.052378
42.242451	1853.780125	18.057395
42.268710	1854.923575	18.062413
42.047835	1866.348353	18.067431
42.217860	1858.811111	18.072448
42.171117	1856.147414	18.077466
42.165984	1856.873484	18.082483
42.424678	1857.702203	18.087501
42.218287	1853.333519	18.092519
42.117184	1853.064155	18.097536
42.200275	1860.369170	18.102554
42.788979	1865.598021	18.107571
42.680766	1862.568934	18.112589
42.587997	1871.818086	18.117607
42.938719	1872.232550	18.122624
42.601322	1887.965880	18.127642
42.856956	1887.280942	18.132659
42.656315	1886.502024	18.137677
42.953139	1892.302867	18.142695
42.840462	1891.115847	18.147712
42.809452	1886.758509	18.152730
42.555947	1883.647977	18.157747
42.643138	1890.892574	18.162765
42.625912	1893.946463	18.167783
43.118249	1888.942469	18.172800
42.955169	1891.537453	18.177818
43.220959	1887.768326	18.182835
43.054534	1890.507785	18.187853
43.141418	1910.521630	18.192871
43.307334	1914.133095	18.197888
43.235557	1922.331217	18.202906
43.654679	1911.385330	18.207923
43.631468	1909.975598	18.212941
43.319874	1927.209566	18.217959
43.634072	1914.071717	18.222976
43.543608	1923.517963	18.227994
43.241773	1914.893397	18.233011
43.738758	1918.844559	18.238029
43.455491	1916.534778	18.243047
43.339904	1906.222418	18.248064
43.808630	1916.082091	18.253082
43.832868	1909.214637	18.258099
43.679503	1916.772128	18.263117
43.608133	1920.663705	18.268135
43.843265	1911.675051	18.273152
44.099362	1926.285714	18.278170
44.091557	1928.598730	18.283187
44.282174	1930.464788	18.288205
43.757414	1921.272473	18.293223
43.987736	1931.876522	18.298240
44.078930	1947.820005	18.303258
44.129457	1946.642346	18.308275
44.413159	1944.034477	18.313293
44.020990	1948.015768	18.318311
44.298133	1945.502546	18.323328
44.546706	1951.830247	18.328346
44.346168	1939.818256	18.333363
44.328924	1944.130675	18.338381
44.512608	1946.659350	18.343399
44.692498	1936.483900	18.348416
44.605377	1940.863310	18.353434
45.046486	1944.591352	18.358451
44.858958	1946.084323	18.363469
44.596642	1950.166823	18.368487
44.760225	1941.322494	18.373504
44.838011	1941.903985	18.378522
44.785671	1941.567062	18.383539
44.940049	1944.208958	18.388557
44.813646	1941.670430	18.393575
44.590576	1945.343158	18.398592
44.589321	1953.725120	18.403610
44.971698	1967.702943	18.408627
45.015253	1964.785705	18.413645
44.973958	1972.319845	18.418663
45.295984	1971.932651	18.423680
45.501763	1977.895925	18.428698
45.460723	1972.741001	18.433715
45.766155	1974.122315	18.438733
45.126982	1977.102371	18.443751
45.356172	1973.430302	18.448768
45.269532	1969.700060	18.453786
45.489377	1971.575620	18.458803
45.583563	1975.605201	18.463821
45.567658	1975.427647	18.468839
45.629376	1965.906577	18.473856
45.686811	1969.026444	18.478874
45.615540	1972.766210	18.483891
45.913752	1964.172550	18.488909
45.355117	1968.155227	18.493927
45.691382	1964.650141	18.498944
45.402447	1968.461590	18.503962
45.543301	1966.989503	18.508979
45.862765	1974.176645	18.513997
45.460157	2001.351794	18.519015
45.638790	2004.154226	18.524032
46.127920	1997.874880	18.529050
46.122032	1996.053357	18.534067
46.108536	2000.837141	18.539085
46.397796	1999.657584	18.544103
46.233932	2002.202371	18.549120
46.177906	2004.989530	18.554138
46.137518	2003.766587	18.559155
46.325340	1996.339703	18.564173
46.313261	2007.588919	18.569191
46.132229	2005.387882	18.574208
46.529114	2009.693263	18.579226
46.427240	2024.121213	18.584243
46.770789	2031.730081	18.589261
46.394074	2023.358872	18.594279
46.378931	2025.717909	18.599296
46.449395	2026.321809	18.604314
46.315057	2027.191200	18.609331
46.778213	2020.901042	18.614349
46.320358	2029.661851	18.619367
46.649882	2042.525729	18.624384
46.661592	2054.640357	18.629402
46.687290	2054.174571	18.634419
47.229849	2046.919191	18.639437
47.131674	2060.663836	18.644455
47.021361	2059.579467	18.649472
47.099119	2058.975592	18.654490
47.039304	2058.889991	18.659507
47.317165	2050.377397	18.664525
46.920850	2054.477365	18.669543
47.084114	2054.732169	18.674560
47.559532	2071.696839	18.679578
47.526798	2073.641015	18.684595
47.562241	2071.944249	18.689613
47.739200	2083.438677	18.694631
48.022143	2072.150204	18.699648
47.741087	2061.553426	18.704666
47.539797	2064.208022	18.709683
47.883462	2056.881317	18.714701
47.671608	2049.702997	18.719719
47.783277	2066.617915	18.724736
47.822819	2071.012558	18.729754
47.806352	2079.068228	18.734771
47.941263	2074.301306	18.739789
47.981571	2084.917682	18.744807
48.335712	2074.022941	18.749824
48.144582	2077.275292	18.754842
48.137172	2078.989681	18.759859
48.338019	2081.359899	18.764877
47.986978	2083.295064	18.769895
48.191792	2068.581697	18.774912
48.423414	2075.996063	18.779930
48.652449	2081.180103	18.784947
48.637421	2069.829821	18.789965
48.578598	2078.083385	18.794983
48.616100	2075.727136	18.800000
48.603938	2071.108739	18.805018
48.188722	2075.542090	18.810035
48.399634	2074.965746	18.815053
48.524718	2074.016093	18.820071
48.532309	2064.074119	18.825088
48.916740	2072.495318	18.830106
48.497379	2069.674702	18.835123
48.529348	2068.319080	18.840141
48.320148	2068.192805	18.845159
48.504854	2085.175541	18.850176
48.615845	2101.888457	18.855194
48.619056	2104.735406	18.860211
49.182935	2089.795634	18.865229
49.359983	2099.928489	18.870247
48.964340	2100.540660	18.875264
49.183072	2096.729431	18.880282
49.076514	2099.796037	18.885299
49.224724	2099.488477	18.890317
49.373370	2102.211548	18.895335
49.436137	2098.484973	18.900352
49.572058	2108.183907	18.905370
49.610130	2127.111699	18.910387
49.944280	2113.293242	18.915405
49.733840	2111.349372	18.920423
49.441038	2101.320778	18.925440
49.374155	2103.330185	18.930458
49.484805	2119.331319	18.935475
49.648639	2121.187516	18.940493
49.893414	2117.290323	18.945511
49.882723	2128.897306	18.950528
50.031970	2117.177050	18.955546
49.887431	2129.805915	18.960563
49.679926	2123.416595	18.965581
49.881335	2127.398439	18.970599
49.945923	2124.605242	18.975616
50.218334	2121.898460	18.980634
49.920181	2126.127522	18.985651
50.273292	2125.412868	18.990669
50.209850	2124.669475	18.995687
50.202605	2145.819537	19.000704
50.767706	2149.954186	19.005722
50.554343	2154.899684	19.010739
50.360133	2148.048867	19.015757
50.485180	2150.848862	19.020775
50.619621	2154.181451	19.025792
50.664958	2154.718571	19.030810
50.688575	2161.097188	19.035827
50.702774	2149.756341	19.040845
50.638184	2156.902571	19.045863
50.468527	2154.683966	19.050880
50.932974	2147.688769	19.055898
50.442736	2153.818973	19.060915
50.937487	2146.432731	19.065933
50.340559	2155.497392	19.070951
50.843016	2157.351501	19.075968
51.319685	2173.671878	19.080986
51.038267	2182.069551	19.086003
51.372395	2185.515031	19.091021
51.310171	2187.846992	19.096039
51.259058	2181.955783	19.101056
51.519987	2184.345539	19.106074
51.280040	2193.887381	19.111091
51.521124	2184.513757	19.116109
51.484953	2176.899116	19.121127
51.568077	2182.933165	19.126144
51.620366	2177.858460	19.131162
51.301676	2189.822957	19.136179
51.398843	2184.420951	19.141197
51.224687	2182.866151	19.146215
51.506204	2192.202901	19.151232
51.650312	2201.805415	19.156250
51.729268	2211.694419	19.161267
51.918349	2215.904005	19.166285
51.901242	2217.546017	19.171303
51.841452	2218.650519	19.176320
52.190597	2216.571764	19.181338
51.969059	2217.904215	19.186355
52.140621	2217.899698	19.191373
52.013747	2218.525641	19.196391
51.488631	2218.437164	19.201408
52.631892	2227.528735	19.206426
52.283731	2237.386767	19.211443
52.120244	2239.349459	19.216461
52.543987	2243.591633	19.221479
52.248077	2243.182640	19.226496
52.569901	2241.897975	19.231514
52.482106	2242.371381	19.236531
52.663083	2241.636981	19.241549
52.609217	2236.224434	19.246567
52.569509	2238.890260	19.251584
53.337940	2246.252134	19.256602
53.279744	2238.788066	19.261619
52.893936	2245.396415	19.266637
53.262635	2238.302392	19.271655
52.698048	2241.413762	19.276672
53.072478	2234.248033	19.281690
53.260241	2241.688358	19.286707
53.431808	2236.758219	19.291725
53.433498	2232.065982	19.296743
53.190450	2235.226751	19.301760
53.429593	2231.260420	19.306778
53.229697	2229.328225	19.311795
53.445661	2234.643405	19.316813
53.429647	2237.089926	19.321831
53.474398	2254.512073	19.326848
53.474642	2255.702179	19.331866
53.450486	2263.103161	19.336883
53.434676	2249.245214	19.341901
53.666039	2255.836155	19.346919
53.507399	2270.138893	19.351936
54.092013	2258.265709	19.356954
53.951560	2262.236828	19.361971
53.785275	2259.822594	19.366989
53.907610	2259.354761	19.372007
53.897611	2266.221751	19.377024
53.899312	2260.284330	19.382042
53.927679	2264.387415	19.387059
54.302301	2287.696537	19.392077
54.260164	2285.428469	19.397095
54.721613	2281.766477	19.402112
54.934942	2270.160946	19.407130
54.866417	2258.658585	19.412147
54.618373	2247.237565	19.417165
54.935496	2244.471715	19.422183
54.689478	2244.746178	19.427200
54.714558	2237.836745	19.432218
54.803891	2239.387058	19.437235
54.992222	2233.667658	19.442253
55.058184	2230.025492	19.447271
54.468225	2239.577564	19.452288
54.782365	2235.180019	19.457306
54.538494	2233.431819	19.462323
54.652065	2248.704248	19.467341
55.368056	2244.488025	19.472359
55.012326	2263.343508	19.477376
55.225668	2262.792727	19.482394
55.175514	2268.981003	19.487411
55.328910	2270.668981	19.492429
55.692323	2270.363279	19.497447
55.404096	2273.067960	19.502464
55.615922	2269.893353	19.507482
55.593303	2271.273529	19.512499
55.354938	2279.637647	19.517517
55.796024	2269.921367	19.522535
55.649110	2270.143841	19.527552
55.587028	2264.874967	19.532570
55.638032	2282.667421	19.537587
55.512524	2275.065404	19.542605
55.714605	2265.739638	19.547623
55.406059	2278.313770	19.552640
55.533410	2269.018799	19.557658
55.421630	2281.220171	19.562675
55.621768	2301.907117	19.567693
55.736053	2303.794838	19.572711
55.961775	2300.483502	19.577728
56.047046	2304.498864	19.582746
56.405385	2304.500741	19.587763
55.998714	2300.873370	19.592781
56.545327	2291.224412	19.597799
56.372423	2302.525463	19.602816
56.143008	2302.248236	19.607834
56.268992	2298.716043	19.612851
56.150094	2318.009711	19.617869
56.321059	2325.071260	19.622887
56.334295	2328.723699	19.627904
56.534768	2327.988546	19.632922
56.717087	2321.537751	19.637939
56.682761	2325.889977	19.642957
56.939458	2326.096062	19.647975
56.937347	2325.933608	19.652992
56.756175	2330.075638	19.658010
57.136120	2340.408346	19.663027
56.724698	2348.897642	19.668045
57.022858	2360.105515	19.673063
57.372800	2367.913337	19.678080
57.543328	2357.182179	19.683098
57.618628	2354.159117	19.688115
57.324261	2356.317322	19.693133
57.680931	2351.472467	19.698151
57.313072	2360.396101	19.703168
57.294338	2355.888785	19.708186
57.546027	2358.763801	19.713203
57.253139	2364.832725	19.718221
57.359110	2359.634552	19.723239
57.311893	2365.062549	19.728256
57.623144	2376.124400	19.733274
57.712804	2383.335812	19.738291
57.679384	2392.467277	19.743309
58.066316	2388.526889	19.748327
57.878007	2397.327518	19.753344
57.820982	2390.546739	19.758362
57.889562	2398.935910	19.763379
57.736260	2397.760833	19.768397
58.231776	2412.635068	19.773415
58.271803	2422.452550	19.778432
58.571663	2426.168637	19.783450
58.296256	2425.436223	19.788467
58.325230	2428.622083	19.793485
58.221369	2422.669182	19.798503
58.254522	2415.833105	19.803520
57.984952	2423.482543	19.808538
58.714994	2431.226631	19.813555
58.491817	2443.639408	19.818573
59.064184	2441.742123	19.823591
59.138432	2444.005163	19.828608
59.341194	2441.037268	19.833626
59.266674	2438.616235	19.838643
58.904932	2450.569717	19.843661
59.056206	2445.635666	19.848679
59.233881	2441.303875	19.853696
59.365596	2434.013934	19.858714
59.759581	2441.543394	19.863731
59.699203	2447.225232	19.868749
59.452163	2425.655199	19.873767
59.393126	2424.382492	19.878784
59.313471	2426.049449	19.883802
59.805256	2436.741957	19.888819
59.699716	2446.866634	19.893837
59.736714	2437.895101	19.898855
59.808931	2437.085219	19.903872
59.345378	2443.337141	19.908890
59.403525	2447.848493	19.913907
59.399873	2437.716915	19.918925
59.653950	2435.748471	19.923943
59.418973	2443.889534	19.928960
59.960673	2455.241132	19.933978
60.079094	2464.402700	19.938995
59.964715	2474.384071	19.944013
60.219876	2464.623376	19.949031
60.255780	2468.383932	19.954048
60.284269	2467.384372	19.959066
60.627399	2462.147553	19.964083
60.489351	2464.926642	19.969101
60.474529	2471.718197	19.974119
60.286958	2472.012445	19.979136
60.381331	2464.702487	19.984154
60.756786	2478.164323	19.989171
60.666529	2495.892254	19.994189
61.196245	2494.647566	19.999207
61.110487	2495.716899	20.004224
60.917938	2497.399509	20.009242
61.108416	2490.900143	20.014259
61.129192	2495.434776	20.019277
61.097599	2493.183872	20.024295
61.056947	2491.124772	20.029312
61.089633	2489.917665	20.034330
61.407677	2479.628560	20.039347
61.067068	2492.775914	20.044365
61.373670	2488.746840	20.049383
61.614780	2487.975308	20.054400
61.209141	2495.062825	20.059418
61.293769	2488.983869	20.064435
61.194386	2489.778491	20.069453
61.438576	2512.639174	20.074471
61.633190	2519.561750	20.079488
61.600187	2520.677733	20.084506
62.052699	2520.751120	20.089523
61.878407	2524.300579	20.094541
62.031280	2525.563118	20.099559
62.001010	2523.768229	20.104576
62.078365	2522.557142	20.109594
61.974295	2510.764488	20.114611
61.891838	2521.596625	20.119629
61.931305	2519.960521	20.124647
62.138706	2533.349312	20.129664
62.152932	2537.964450	20.134682
62.585280	2541.520995	20.139699
62.155642	2546.822838	20.144717
62.302879	2546.779725	20.149735
62.188145	2543.762547	20.154752
62.295170	2551.737427	20.159770
62.760194	2566.078644	20.164787
62.809306	2575.669024	20.169805
63.102779	2576.774634	20.174823
63.292699	2568.664351	20.179840
62.858312	2581.158125	20.184858
63.141296	2569.854319	20.189875
63.202814	2580.334736	20.194893
63.099913	2580.305558	20.199911
63.320995	2571.737218	20.204928
62.859351	2577.540525	20.209946
62.868386	2577.716892	20.214963
62.889227	2579.691921	20.219981
63.168648	2589.783619	20.224999
63.357191	2598.525051	20.230016
63.292462	2605.875255	20.235034
63.202461	2604.756140	20.240051
63.134290	2609.938214	20.245069
63.199079	2617.923799	20.250087
63.772240	2627.157681	20.255104
63.470930	2632.432008	20.260122
63.616378	2635.103773	20.265139
63.882846	2638.981777	20.270157
63.949622	2636.575933	20.275175
64.347141	2653.537189	20.280192
64.336162	2654.504934	20.285210
64.656873	2647.569398	20.290227
64.655775	2661.867058	20.295245
64.607239	2650.832380	20.300263
64.520877	2644.199325	20.305280
64.546874	2640.824586	20.310298
64.821821	2639.242160	20.315315
64.707736	2651.234182	20.320333
64.833469	2648.093677	20.325351
65.348438	2654.452355	20.330368
64.880700	2644.868975	20.335386
65.266258	2627.045854	20.340403
65.071974	2623.966619	20.345421
65.127509	2621.365131	20.350439
65.046160	2614.518905	20.355456
64.773955	2627.370718	20.360474
65.102074	2637.513678	20.365491
65.060760	2651.220704	20.370509
65.094092	2649.035723	20.375527
65.321115	2651.160372	20.380544
65.099337	2658.975365	20.385562
65.617522	2645.697351	20.390579
65.500656	2652.057683	20.395597
65.558273	2649.993900	20.400615
65.710951	2646.635141	20.405632
65.378746	2649.493212	20.410650
65.866896	2654.652653	20.415667
65.909309	2679.317226	20.420685
65.960377	2681.023932	20.425703
66.048988	2679.988811	20.430720
66.103111	2684.448176	20.435738
66.212625	2680.044591	20.440755
66.170708	2676.206348	20.445773
66.327405	2676.603802	20.450791
66.517363	2673.365736	20.455808
66.328312	2678.350007	20.460826
66.552716	2680.754326	20.465843
66.563104	2678.880566	20.470861
66.398096	2672.046868	20.475879
66.611271	2666.855875	20.480896
66.436435	2677.374056	20.485914
66.758121	2668.966602	20.490931
66.710305	2672.836530	20.495949
66.626751	2695.170822	20.500967
67.248402	2692.484541	20.505984
67.300804	2699.552595	20.511002
67.225614	2691.985599	20.516019
67.477216	2697.482480	20.521037
67.451272	2692.822820	20.526055
67.639005	2689.266526	20.531072
67.536093	2694.170203	20.536090
67.513426	2691.928858	20.541107
67.838579	2691.808601	20.546125
67.451077	2702.149904	20.551143
67.694833	2693.693509	20.556160
67.640021	2698.318922	20.561178
67.571815	2693.706906	20.566195
67.686204	2700.375701	20.571213
67.489096	2696.647157	20.576231
67.601837	2691.045041	20.581248
67.826145	2704.673571	20.586266
67.827865	2715.932144	20.591283
68.039195	2724.614956	20.596301
67.852804	2730.487696	20.601319
68.233980	2730.392328	20.606336
67.952924	2739.418766	20.611354
67.894056	2723.116928	20.616371
68.013531	2738.076642	20.621389
68.233808	2754.122345	20.626407
68.600764	2747.271421	20.631424
68.207538	2760.130065	20.636442
68.558384	2749.386382	20.641459
68.729790	2754.573562	20.646477
68.697197	2759.986787	20.651495
68.967466	2770.428541	20.656512
69.090896	2781.858116	20.661530
69.160546	2780.022088	20.666547
69.478290	2787.442750	20.671565
69.455004	2786.139138	20.676583
69.488862	2773.315043	20.681600
69.372527	2767.791123	20.686618
69.795356	2764.887967	20.691635
69.765771	2750.978251	20.696653
69.440738	2747.877364	20.701671
69.369816	2749.837946	20.706688
69.523410	2767.248065	20.711706
69.679960	2772.797106	20.716723
69.945178	2769.974149	20.721741
69.643471	2778.291228	20.726759
69.588305	2777.298696	20.731776
69.552132	2779.522763	20.736794
69.870160	2779.132259	20.741811
70.149100	2775.208207	20.746829
69.900719	2792.555819	20.751847
70.498953	2798.301092	20.756864
70.318150	2803.085862	20.761882
70.361056	2806.086301	20.766899
70.490728	2809.290795	20.771917
70.572370	2810.206808	20.776935
70.484565	2799.599909	20.781952
70.348720	2805.177501	20.786970
70.499665	2797.069376	20.791987
70.691529	2804.488883	20.797005
70.788019	2825.975003	20.802023
70.888555	2831.488162	20.807040
71.226150	2824.834607	20.812058
70.921437	2836.470165	20.817075
71.197924	2830.115044	20.822093
71.178434	2829.210427	20.827111
71.613122	2825.575384	20.832128
71.209037	2833.954446	20.837146
71.504802	2832.845373	20.842163
71.438887	2818.605500	20.847181
71.340530	2827.678370	20.852199
71.510245	2829.280430	20.857216
71.465235	2831.357242	20.862234
71.474650	2835.880420	20.867251
71.642945	2842.094669	20.872269
71.593897	2844.136729	20.877287
71.823130	2846.622114	20.882304
72.130720	2849.747900	20.887322
71.571020	2852.716234	20.892339
72.132535	2858.733265	20.897357
71.870161	2877.588018	20.902375
71.970817	2882.919467	20.907392
71.978522	2874.035721	20.912410
72.148465	2877.755340	20.917427
72.417490	2876.556133	20.922445
72.385188	2896.295354	20.927463
72.628166	2895.183682	20.932480
72.729073	2909.981342	20.937498
72.205517	2911.096141	20.942515
72.915134	2908.067771	20.947533
72.720134	2913.438517	20.952551
72.741967	2906.530073	20.957568
72.918927	2905.771112	20.962586
73.127681	2928.213319	20.967603
73.536165	2926.143098	20.972621
73.527108	2934.043879	20.977639
73.527272	2932.894626	20.982656
73.586792	2927.951448	20.987674
73.441597	2931.693808	20.992691
73.816264	2932.869880	20.997709
73.742424	2930.635873	21.002727
73.850452	2929.722711	21.007744
73.970019	2934.707408	21.012762
74.169386	2923.381268	21.017779
74.330656	2916.865134	21.022797
74.063952	2929.967267	21.027815
74.157581	2922.568310	21.032832
73.946216	2925.658882	21.037850
74.038086	2935.692630	21.042867
74.346662	2936.101269	21.047885
73.977229	2932.574778	21.052903
74.251122	2936.311659	21.057920
74.616964	2929.942244	21.062938
74.423750	2936.295997	21.067955
74.914058	2940.697675	21.072973
74.810927	2954.539131	21.077991
75.096843	2962.211959	21.083008
75.195895	2955.211729	21.088026
74.644784	2950.068583	21.093043
74.896949	2948.580221	21.098061
75.125759	2960.329019	21.103079
75.036759	2947.837443	21.108096
75.032775	2954.203502	21.113114
75.023028	2954.534688	21.118131
75.122326	2954.544058	21.123149
75.153334	2963.268357	21.128167
75.433657	2976.955858	21.133184
75.681894	2980.191039	21.138202
75.159571	2997.879142	21.143219
75.306527	2983.517843	21.148237
75.395457	2990.622691	21.153255
75.930107	3006.603589	21.158272
75.879231	3017.566356	21.163290
76.000944	3014.380004	21.168307
75.939636	3007.921353	21.173325
75.973951	3016.557839	21.178343
76.279936	3012.287228	21.183360
76.430881	3010.342238	21.188378
75.925682	3013.154810	21.193395
76.470021	3011.997429	21.198413
76.240363	3020.649271	21.203431
76.676330	3033.561557	21.208448
76.912493	3053.862308	21.213466
76.517846	3049.148061	21.218483
76.600128	3050.329082	21.223501
76.700653	3050.943964	21.228519
76.899101	3054.553674	21.233536
77.307101	3045.849840	21.238554
76.921575	3044.543405	21.243571
76.954432	3040.621557	21.248589
76.874244	3051.693646	21.253607
77.034342	3065.416923	21.258624
77.179250	3071.390356	21.263642
77.192505	3067.634461	21.268659
77.254184	3072.959609	21.273677
77.297843	3089.589212	21.278695
77.582311	3104.387686	21.283712
77.908752	3102.354125	21.288730
77.900077	3109.675189	21.293747
77.945384	3110.272921	21.298765
78.057550	3101.864024	21.303783
77.728201	3101.579117	21.308800
78.170328	3099.011860	21.313818
78.090265	3092.665505	21.318835
78.521096	3107.214876	21.323853
78.466077	3125.683678	21.328871
78.527211	3131.836477	21.333888
78.698726	3130.724386	21.338906
78.484541	3136.846364	21.343923
78.815590	3137.679357	21.348941
78.820181	3133.514989	21.353959
78.919552	3133.418152	21.358976
78.915058	3128.250698	21.363994
78.936355	3134.462556	21.369011
79.138671	3127.293954	21.374029
78.982088	3126.129565	21.379047
79.174023	3132.229252	21.384064
79.328883	3141.586814	21.389082
79.458642	3158.209843	21.394099
79.595144	3157.233129	21.399117
79.722148	3164.495610	21.404135
79.780190	3150.720215	21.409152
79.742448	3147.933704	21.414170
79.703971	3162.259839	21.419187
79.628635	3156.133748	21.424205
79.969424	3156.981708	21.429223
79.710061	3162.637345	21.434240
79.914183	3158.886386	21.439258
79.713063	3172.285063	21.444275
80.170378	3183.634172	21.449293
80.148685	3186.066811	21.454311
80.114282	3190.527862	21.459328
80.475877	3180.774105	21.464346
80.624281	3186.377307	21.469363
80.784017	3185.888537	21.474381
80.454732	3179.343537	21.479399
80.567486	3206.965773	21.484416
81.045471	3211.614933	21.489434
80.757474	3220.040204	21.494451
81.176571	3220.386389	21.499469
81.071237	3221.560372	21.504487
80.987265	3218.672663	21.509504
81.300094	3211.432118	21.514522
81.097986	3226.323261	21.519539
81.396937	3213.038011	21.524557
81.033929	3224.358288	21.529575
81.095546	3229.779474	21.534592
81.509070	3237.339273	21.539610
81.318283	3249.845893	21.544627
81.491790	3240.798607	21.549645
81.746755	3247.394888	21.554663
81.961750	3266.557104	21.559680
82.317578	3279.085133	21.564698
82.089071	3287.208323	21.569715
82.598548	3277.377427	21.574733
82.282423	3275.499810	21.579751
82.069133	3285.178915	21.584768
82.502343	3271.531584	21.589786
82.181009	3265.239364	21.594803
82.688148	3257.720801	21.599821
82.999601	3264.878399	21.604839
82.925250	3265.870449	21.609856
83.242187	3259.797392	21.614874
83.126722	3256.628360	21.619891
83.107435	3250.492504	21.624909
82.962555	3257.433388	21.629927
83.153173	3263.075513	21.634944
83.528670	3261.805806	21.639962
83.364062	3282.638055	21.644979
83.725853	3278.754151	21.649997
83.659741	3275.877742	21.655015
83.697324	3275.874930	21.660032
84.167584	3275.015684	21.665050
83.844098	3278.129716	21.670067
83.881852	3274.176346	21.675085
83.959102	3275.605194	21.680103
83.775380	3276.170233	21.685120
84.156652	3261.230084	21.690138
84.031827	3274.703218	21.695155
83.940709	3274.025537	21.700173
84.101118	3271.292359	21.705191
83.843324	3280.711886	21.710208
84.259894	3297.207522	21.715226
84.205475	3307.380491	21.720243
84.534193	3303.152584	21.725261
84.347095	3301.447115	21.730279
84.322516	3311.944147	21.735296
84.821971	3324.694744	21.740314
85.101608	3333.300161	21.745331
85.191940	3339.523122	21.750349
84.992809	3326.512292	21.755367
85.118022	3338.956793	21.760384
85.313177	3331.576053	21.765402
85.198885	3331.549476	21.770419
85.213517	3324.477575	21.775437
85.544656	3335.045331	21.780455
85.467487	3357.535370	21.785472
85.940449	3357.515830	21.790490
85.492256	3364.971619	21.795507
85.672519	3369.079110	21.800525
85.835565	3363.584354	21.805543
85.906375	3363.695814	21.810560
86.165102	3347.375671	21.815578
86.166298	3364.353763	21.820595
85.913712	3360.952488	21.825613
86.356140	3369.047389	21.830631
86.276182	3384.686195	21.835648
86.472197	3380.928606	21.840666
86.659991	3389.626582	21.845683
86.681929	3389.946431	21.850701
86.824092	3386.556929	21.855719
86.892389	3388.015535	21.860736
87.174407	3384.405494	21.865754
86.842082	3391.055380	21.870771
87.005377	3399.954718	21.875789
87.620527	3401.109000	21.880807
87.415102	3417.320080	21.885824
87.524100	3416.184899	21.890842
87.405103	3413.438828	21.895859
87.500632	3411.788965	21.900877
87.801517	3404.208037	21.905895
87.605641	3413.335366	21.910912
87.535859	3409.864021	21.915930
87.808396	3404.620823	21.920947
87.918484	3407.988264	21.925965
88.068329	3410.191414	21.930983
88.060921	3436.514817	21.936000
88.464710	3435.473434	21.941018
88.435998	3439.925000	21.946035
88.348887	3438.093437	21.951053
88.983179	3438.561068	21.956071
88.681856	3437.615613	21.961088
89.046676	3439.009631	21.966106
88.909510	3434.251834	21.971123
89.008003	3433.035728	21.976141
89.223795	3427.625362	21.981159
88.905164	3431.980776	21.986176
88.983959	3433.534472	21.991194
88.991307	3426.422777	21.996211
89.202613	3436.424448	22.001229
89.310432	3438.308630	22.006247
89.613014	3458.931320	22.011264
89.844948	3456.139503	22.016282
89.743921	3461.854962	22.021299
89.779200	3461.652707	22.026317
89.807882	3454.215068	22.031335
89.343982	3469.451068	22.036352
89.683364	3460.160864	22.041370
89.538711	3472.901033	22.046387
89.648365	3470.774557	22.051405
89.901002	3480.921492	22.056423
89.937094	3499.178784	22.061440
90.293178	3487.969603	22.066458
90.267261	3491.876373	22.071475
90.212731	3497.291794	22.076493
90.441667	3506.429312	22.081511
90.765078	3525.034145	22.086528
90.460120	3524.666671	22.091546
90.769845	3519.702273	22.096563
90.820659	3524.269407	22.101581
90.960372	3522.138131	22.106599
90.990155	3535.186438	22.111616
91.175064	3543.342957	22.116634
91.428145	3552.821211	22.121651
91.408763	3559.134135	22.126669
91.477221	3546.815175	22.131687
91.318955	3546.947435	22.136704
91.410537	3552.512641	22.141722
91.964702	3557.487243	22.146739
91.685828	3577.899963	22.151757
91.999847	3579.971545	22.156775
91.962754	3588.504904	22.161792
92.441554	3578.442704	22.166810
92.386917	3571.711342	22.171827
92.015320	3588.616198	22.176845
92.160144	3582.435152	22.181863
92.450976	3597.486417	22.186880
92.776942	3606.074380	22.191898
92.960196	3604.434892	22.196915
92.983392	3606.541843	22.201933
93.147703	3599.143075	22.206951
92.963729	3613.610067	22.211968
92.803511	3605.620346	22.216986
93.258502	3605.791686	22.222003
92.920586	3615.967600	22.227021
93.130130	3608.957305	22.232039
93.399119	3621.415305	22.237056
93.392100	3642.226866	22.242074
93.694689	3634.544856	22.247091
93.579748	3640.414429	22.252109
93.517418	3639.184621	22.257127
93.160187	3650.317862	22.262144
93.493583	3655.035065	22.267162
94.153941	3661.584192	22.272179
94.082763	3658.991715	22.277197
94.532866	3660.422501	22.282215
94.333038	3670.599244	22.287232
94.151263	3659.577188	22.292250
94.437147	3662.439934	22.297267
94.450498	3678.233305	22.302285
94.944016	3679.115943	22.307303
95.003121	3693.277568	22.312320
95.157018	3685.661724	22.317338
95.155355	3671.281762	22.322355
94.879731	3689.221628	22.327373
94.980585	3680.743405	22.332391
95.290950	3677.285319	22.337408
94.967557	3677.757793	22.342426
95.453664	3677.564667	22.347443
95.480102	3677.221432	22.352461
95.393130	3678.864522	22.357479
95.573663	3689.968674	22.362496
95.966103	3691.390566	22.367514
96.168775	3686.182799	22.372531
96.033722	3696.674910	22.377549
96.001336	3694.380680	22.382567
96.050661	3695.053316	22.387584
96.037477	3695.666694	22.392602
96.362630	3699.346826	22.397619
96.542740	3719.708574	22.402637
96.912740	3718.210001	22.407655
96.947250	3730.253939	22.412672
97.104172	3719.288745	22.417690
97.564027	3709.651132	22.422707
97.079333	3702.197690	22.427725
97.025968	3687.382277	22.432743
97.230225	3695.775730	22.437760
97.165792	3702.652861	22.442778
97.537418	3699.923681	22.447795
97.195777	3710.805108	22.452813
97.638468	3707.480887	22.457831
97.627429	3712.227864	22.462848
97.180274	3708.205386	22.467866
97.687056	3713.622627	22.472883
97.589169	3725.647555	22.477901
98.112414	3729.508506	22.482919
97.797572	3734.244938	22.487936
97.914103	3737.709761	22.492954
98.082670	3737.410727	22.497971
98.020341	3747.253287	22.502989
98.269954	3752.160885	22.508007
98.513766	3758.473616	22.513024
98.439240	3779.410204	22.518042
98.718048	3761.008802	22.523059
98.730889	3777.575659	22.528077
98.510540	3790.527989	22.533095
98.750569	3792.725469	22.538112
98.603516	3796.779865	22.543130
99.045735	3799.101650	22.548147
99.395675	3820.622758	22.553165
99.634385	3829.745547	22.558183
99.797155	3830.849290	22.563200
99.580169	3832.548531	22.568218
100.376961	3819.510602	22.573235
100.104200	3831.867946	22.578253
99.982987	3831.230438	22.583271
100.139209	3829.946880	22.588288
100.440597	3829.031937	22.593306
100.556184	3821.621948	22.598323
100.275409	3823.966206	22.603341
100.510444	3830.043580	22.608359
100.688599	3831.223536	22.613376
100.306015	3826.584202	22.618394
100.530059	3822.238320	22.623411
100.562368	3821.616450	22.628429
100.629693	3823.327778	22.633447
100.872729	3840.670631	22.638464
100.641518	3852.842792	22.643482
100.930111	3855.314954	22.648499
100.965725	3860.764121	22.653517
101.311125	3860.863263	22.658535
101.657898	3865.036383	22.663552
101.460312	3884.109441	22.668570
101.784189	3887.280845	22.673587
101.858383	3901.972059	22.678605
101.933178	3887.442811	22.683623
101.693744	3886.224704	22.688640
101.718942	3896.377518	22.693658
102.064280	3890.420037	22.698675
101.749126	3899.306296	22.703693
102.359006	3914.705069	22.708711
102.347004	3914.756579	22.713728
102.326813	3922.293074	22.718746
102.609065	3913.454597	22.723763
102.588021	3923.514896	22.728781
102.708506	3936.995930	22.733799
102.940873	3947.122821	22.738816
102.974576	3946.851583	22.743834
103.330533	3938.347478	22.748851
103.452359	3942.412530	22.753869
103.118869	3947.074908	22.758887
103.732547	3951.805727	22.763904
103.655413	3964.382937	22.768922
103.792508	3962.544662	22.773939
104.022050	3960.954395	22.778957
103.785460	3967.730088	22.783975
104.139493	3963.374449	22.788992
104.085491	3964.290140	22.794010
104.304478	3967.613597	22.799027
103.793936	3967.284400	22.804045
103.932773	3975.115741	22.809063
104.543302	3984.623023	22.814080
104.588250	3993.163200	22.819098
104.988953	3985.798130	22.824115
105.106606	3994.956848	22.829133
104.865339	3976.813543	22.834151
105.301691	3981.902270	22.839168
105.279503	3983.846589	22.844186
105.720923	3977.566946	22.849203
105.544037	3978.806679	22.854221
105.531007	3976.724083	22.859239
105.861028	3965.676821	22.864256
105.445004	3971.064315	22.869274
105.550897	3964.808289	22.874291
105.461150	3963.261859	22.879309
105.834353	3979.102798	22.884327
105.884044	3991.535511	22.889344
105.906972	3996.513955	22.894362
106.092306	3999.136345	22.899379
106.308580	3995.498880	22.904397
106.163424	3996.665900	22.909415
106.560204	4002.636525	22.914432
106.512532	4022.268788	22.919450
106.657392	4028.364558	22.924467
106.574244	4020.511003	22.929485
106.713638	4022.579816	22.934503
106.736783	4025.999026	22.939520
106.997152	4039.251736	22.944538
107.343851	4046.022557	22.949555
107.461283	4055.520410	22.954573
107.291226	4061.180240	22.959591
107.751576	4048.383783	22.964608
107.720355	4055.398958	22.969626
107.733538	4050.524942	22.974643
107.724339	4054.945261	22.979661
107.990141	4077.203130	22.984679
108.457351	4076.172047	22.989696
108.094347	4083.683050	22.994714
108.341255	4086.564685	22.999731
108.169875	4084.380668	23.004749
108.241527	4084.464466	23.009767
108.854210	4091.969354	23.014784
108.512520	4104.112138	23.019802
108.779644	4113.291149	23.024819
109.069925	4114.464262	23.029837
108.610213	4108.482456	23.034855
109.176222	4111.622378	23.039872
109.087778	4127.791983	23.044890
109.388875	4134.733749	23.049907
109.563286	4137.912523	23.054925
109.413716	4149.453570	23.059943
109.842211	4135.697633	23.064960
109.622923	4138.397946	23.069978
109.506800	4143.575619	23.074995
110.086354	4159.434195	23.080013
110.110646	4163.578584	23.085031
110.200272	4162.280445	23.090048
110.257692	4170.390776	23.095066
110.538927	4164.349006	23.100083
110.338023	4172.428944	23.105101
110.207245	4188.731237	23.110119
110.826681	4197.097319	23.115136
110.376585	4197.462566	23.120154
110.531452	4201.942516	23.125171
110.861156	4207.397622	23.130189
111.190543	4218.258164	23.135207
111.509141	4217.154008	23.140224
111.244234	4231.117652	23.145242
111.766470	4223.049445	23.150259
111.807163	4215.884063	23.155277
111.996694	4224.468976	23.160295
112.194501	4210.666366	23.165312
112.250161	4218.983906	23.170330
112.178867	4215.319870	23.175347
112.363227	4209.583033	23.180365
112.041193	4217.780649	23.185383
112.519400	4225.958435	23.190400
112.726841	4236.951721	23.195418
112.826417	4239.045009	23.200435
112.984568	4245.938821	23.205453
112.703116	4259.116072	23.210471
113.287029	4248.696806	23.215488
113.273909	4249.210286	23.220506
112.974017	4242.319477	23.225523
113.124804	4245.601166	23.230541
112.808453	4248.877105	23.235559
113.200065	4263.938947	23.240576
113.142222	4273.129758	23.245594
113.394484	4276.529010	23.250611
113.715081	4289.639391	23.255629
113.491554	4314.755059	23.260647
114.023813	4309.978336	23.265664
113.941993	4308.720111	23.270682
114.017495	4311.594509	23.275699
114.243597	4332.475290	23.280717
114.676641	4334.006420	23.285735
114.913494	4336.138407	23.290752
114.774277	4336.910369	23.295770
114.757935	4332.457132	23.300787
114.976553	4325.289286	23.305805
115.090739	4338.485334	23.310823
115.407026	4333.511754	23.315840
115.512705	4346.056204	23.320858
115.458676	4351.929720	23.325875
115.949103	4350.228582	23.330893
115.812829	4351.462656	23.335911
115.858859	4348.522524	23.340928
115.996783	4361.450476	23.345946
115.820881	4351.330883	23.350963
115.933787	4346.772068	23.355981
115.992542	4359.017985	23.360999
116.078595	4369.294373	23.366016
116.362710	4374.911007	23.371034
116.390173	4374.252125	23.376051
116.535458	4374.797778	23.381069
116.692918	4392.593912	23.386087
117.160073	4397.848591	23.391104
116.935197	4408.996695	23.396122
116.955001	4413.788543	23.401139
117.349542	4405.967173	23.406157
117.187873	4412.440039	23.411175
116.972458	4400.637656	23.416192
117.421969	4408.007455	23.421210
117.455069	4429.582344	23.426227
117.906386	4430.525261	23.431245
117.878071	4430.672992	23.436263
117.960575	4420.477530	23.441280
118.150821	4429.223723	23.446298
118.025810	4430.622789	23.451315
118.169965	4447.654859	23.456333
118.287379	4451.040254	23.461351
118.577615	4456.006123	23.466368
118.683878	4455.359846	23.471386
118.800441	4453.880377	23.476403
119.083869	4456.853027	23.481421
119.211440	4474.394412	23.486439
119.501160	4475.220708	23.491456
119.562409	4478.767687	23.496474
119.660865	4475.179576	23.501491
120.946382	4434.587393	23.506509
120.685020	4435.764323	23.511527
120.813316	4411.586510	23.516544
120.875559	4405.010776	23.521562
120.811622	4401.272356	23.526579
121.078455	4394.925974	23.531597
121.015439	4381.174237	23.536615
120.603100	4361.210554	23.541632
120.792551	4366.243599	23.546650
120.814023	4367.277085	23.551667
121.400705	4357.638498	23.556685
120.767678	4360.603075	23.561703
120.760604	4361.803173	23.566720
121.093765	4370.675229	23.571738
121.122885	4385.972011	23.576755
121.517607	4385.281312	23.581773
121.262285	4394.540665	23.586791
121.534775	4388.242159	23.591808
121.573375	4392.869729	23.596826
121.682456	4415.040604	23.601843
122.357093	4417.404103	23.606861
121.749428	4423.788392	23.611879
122.112939	4424.842077	23.616896
121.924362	4427.759395	23.621914
122.019271	4439.396210	23.626931
122.536573	4451.176516	23.631949
122.367400	4461.625049	23.636967
122.286225	4461.844146	23.641984
122.634010	4460.876140	23.647002
122.611146	4478.613810	23.652019
123.014467	4474.748152	23.657037
122.912895	4481.252374	23.662055
123.223388	4491.239738	23.667072
123.497664	4500.708149	23.672090
123.413728	4503.879424	23.677107
123.778146	4492.485640	23.682125
123.714696	4504.010084	23.687143
123.687482	4508.641891	23.692160
123.708771	4511.185901	23.697178
123.868983	4524.825563	23.702195
124.388263	4527.465603	23.707213
124.373776	4532.510771	23.712231
124.143614	4531.954327	23.717248
124.613807	4544.956118	23.722266
124.542240	4558.930936	23.727283
124.807386	4553.921382	23.732301
124.749904	4565.020884	23.737319
125.048887	4562.910479	23.742336
125.463901	4568.423710	23.747354
125.490940	4590.569383	23.752371
125.570470	4588.580507	23.757389
125.639301	4589.260302	23.762407
125.639323	4592.018556	23.767424
125.958507	4591.311574	23.772442
125.936857	4587.512866	23.777459
125.904596	4604.715646	23.782477
126.191510	4622.125593	23.787495
126.302624	4619.063315	23.792512
126.596570	4614.741460	23.797530
126.304304	4627.027053	23.802547
126.558118	4624.419556	23.807565
126.807314	4644.814842	23.812583
126.877810	4649.128226	23.817600
127.010710	4646.296124	23.822618
127.077575	4646.264255	23.827635
127.285488	4666.424631	23.832653
127.491071	4681.500048	23.837671
128.171130	4664.614059	23.842688
128.814107	4659.598505	23.847706
128.895719	4668.000273	23.852723
128.798195	4647.434509	23.857741
128.891176	4623.837069	23.862759
128.696955	4627.905507	23.867776
128.819208	4616.587219	23.872794
128.700997	4615.054698	23.877811
128.965250	4607.718162	23.882829
128.975740	4622.930048	23.887847
129.538844	4645.378175	23.892864
129.018630	4647.244653	23.897882
129.275419	4653.678432	23.902899
129.406479	4653.638687	23.907917
129.543448	4650.801216	23.912935
129.607611	4664.713581	23.917952
129.807929	4642.220072	23.922970
129.805645	4655.859807	23.927987
129.594774	4650.681456	23.933005
129.792234	4674.376664	23.938023
129.486945	4685.454407	23.943040
129.681845	4684.712168	23.948058
129.851439	4702.615311	23.953075
130.020167	4708.289810	23.958093
130.486625	4718.364175	23.963111
130.264529	4732.655034	23.968128
130.573862	4733.349196	23.973146
130.545500	4748.335324	23.978163
130.802271	4744.953986	23.983181
130.798287	4773.480489	23.988199
131.065960	4778.203034	23.993216
131.484829	4776.672968	23.998234
131.741967	4793.667756	24.003251
132.532943	4784.807434	24.008269
132.422570	4783.705558	24.013287
132.323410	4781.620061	24.018304
132.848196	4771.043861	24.023322
132.686664	4784.668199	24.028339
132.533280	4782.253843	24.033357
132.642462	4780.894314	24.038375
132.808094	4785.109174	24.043392
133.083716	4779.025568	24.048410
133.007735	4783.677038	24.053427
133.138385	4780.570703	24.058445
133.287138	4791.893962	24.063463
133.067982	4801.722110	24.068480
133.351995	4807.548198	24.073498
133.304807	4811.664045	24.078515
133.581201	4822.878074	24.083533
133.673488	4834.809069	24.088551
133.727450	4838.325829	24.093568
134.027081	4840.189049	24.098586
134.242474	4861.346072	24.103603
134.151189	4880.566319	24.108621
134.506662	4879.077035	24.113639
134.551643	4886.353451	24.118656
134.911061	4887.505379	24.123674
134.825053	4897.498815	24.128691
135.345566	4902.030819	24.133709
135.453052	4903.245736	24.138727
135.147142	4907.856809	24.143744
135.291713	4905.821330	24.148762
135.659792	4920.939528	24.153779
135.616775	4935.970666	24.158797
135.786275	4930.637156	24.163815
135.535454	4945.346622	24.168832
135.912702	4955.192275	24.173850
136.093205	4962.735850	24.178867
136.318142	4962.050961	24.183885
136.580350	4960.296463	24.188903
136.812840	4985.104535	24.193920
137.562546	4977.263211	24.198938
137.700941	4971.045634	24.203955
137.899086	4966.636678	24.208973
137.956323	4943.033415	24.213991
137.852760	4936.531086	24.219008
138.140188	4924.888053	24.224026
138.006761	4931.622558	24.229043
137.901796	4932.169588	24.234061
138.138170	4924.010485	24.239079
137.790338	4931.803504	24.244096
138.335788	4939.197614	24.249114
138.467204	4955.867261	24.254131
138.389040	4960.128127	24.259149
138.249930	4957.006551	24.264167
138.646493	4962.223130	24.269184
138.813195	4957.439984	24.274202
138.964762	4981.745643	24.279219
139.012792	4985.636297	24.284237
139.039539	4986.070279	24.289255
138.914795	4995.653774	24.294272
139.127467	5003.709128	24.299290
139.263201	5017.532527	24.304307
139.339576	5025.261100	24.309325
139.498258	5044.942855	24.314343
139.776915	5050.287623	24.319360
140.102688	5050.729784	24.324378
140.230190	5064.714249	24.329395
140.022456	5076.919074	24.334413
140.372941	5087.936608	24.339431
140.322770	5096.566548	24.344448
140.831844	5108.613831	24.349466
140.821207	5120.135841	24.354483
140.895700	5125.791698	24.359501
141.135259	5127.589008	24.364519
141.351559	5143.696971	24.369536
141.636420	5140.878309	24.374554
141.811008	5140.159743	24.379571
141.815881	5145.417602	24.384589
142.143883	5162.189095	24.389607
142.181867	5167.758741	24.394624
142.704178	5168.378842	24.399642
142.807165	5172.726536	24.404659
142.375535	5174.497914	24.409677
142.790093	5162.315958	24.414695
142.806382	5183.520927	24.419712
143.010978	5189.048279	24.424730
143.442387	5204.281763	24.429747
143.413193	5204.520904	24.434765
143.823863	5195.772908	24.439783
143.596853	5197.776009	24.444800
144.025839	5185.903285	24.449818
144.224038	5197.432181	24.454835
144.630408	5206.284418	24.459853
145.081596	5198.944533	24.464871
145.343279	5174.618323	24.469888
145.289575	5156.587624	24.474906
145.401664	5158.229033	24.479923
145.250068	5150.619450	24.484941
145.483226	5146.121463	24.489959
145.131874	5155.526414	24.494976
145.467917	5152.739713	24.499994
145.394525	5154.689203	24.505011
145.463668	5154.911090	24.510029
145.766559	5149.412257	24.515047
145.523101	5152.939540	24.520064
145.918592	5169.661731	24.525082
145.896015	5185.730729	24.530099
145.934619	5182.975715	24.535117
146.251265	5176.338617	24.540135
145.963360	5185.644568	24.545152
146.354481	5194.215214	24.550170
146.372620	5205.231545	24.555187
146.362233	5218.836114	24.560205
146.534281	5229.362953	24.565223
146.932900	5238.887544	24.570240
146.623209	5249.189099	24.575258
146.972644	5266.749552	24.580275
146.934589	5276.719076	24.585293
147.608711	5278.827901	24.590311
147.507557	5304.370252	24.595328
147.903246	5302.332443	24.600346
148.811672	5280.654210	24.605363
149.039656	5282.773594	24.610381
149.062526	5281.696852	24.615399
149.070260	5285.083408	24.620416
149.458733	5275.517537	24.625434
149.596042	5272.196041	24.630451
149.398616	5277.380779	24.635469
149.607367	5271.703372	24.640487
149.435439	5275.191741	24.645504
149.668386	5271.024973	24.650522
149.518961	5267.506092	24.655539
149.687597	5285.670512	24.660557
149.748875	5290.426922	24.665575
149.828966	5302.384631	24.670592
149.655025	5299.073420	24.675610
150.108437	5313.015596	24.680627
150.084390	5327.616901	24.685645
150.294488	5332.212699	24.690663
150.525430	5355.710910	24.695680
150.758823	5364.413805	24.700698
151.326848	5362.310746	24.705715
151.288815	5379.634936	24.710733
151.433910	5392.838017	24.715751
151.487285	5391.099460	24.720768
151.820438	5396.410490	24.725786
151.515938	5395.134963	24.730803
151.475769	5419.387733	24.735821
152.136306	5422.414535	24.740839
152.091869	5422.350847	24.745856
152.160126	5442.391365	24.750874
152.473483	5453.072067	24.755891
152.213272	5453.643869	24.760909
152.961367	5465.613211	24.765927
152.938664	5488.027006	24.770944
153.079121	5482.404467	24.775962
153.461923	5486.374051	24.780979
153.509976	5491.468582	24.785997
153.403396	5491.981271	24.791015
153.736347	5517.306861	24.796032
154.017398	5519.069280	24.801050
154.199876	5517.502881	24.806067
154.131065	5522.354851	24.811085
154.087419	5523.553794	24.816103
154.270976	5541.284215	24.821120
154.513258	5550.074707	24.826138
154.440813	5551.813246	24.831155
154.760554	5568.836712	24.836173
155.151610	5573.852978	24.841191
155.137978	5580.061210	24.846208
155.236440	5588.816436	24.851226
155.761835	5592.230670	24.856243
155.342540	5601.105437	24.861261
155.529848	5605.767110	24.866279
155.880076	5613.543592	24.871296
156.050498	5633.941008	24.876314
156.500316	5628.734856	24.881331
156.400528	5622.646250	24.886349
156.534731	5635.123523	24.891367
156.540017	5652.071341	24.896384
156.537102	5661.743629	24.901402
157.144157	5665.804175	24.906419
157.481969	5681.316648	24.911437
157.726454	5688.008547	24.916455
157.669051	5682.961928	24.921472
158.020348	5681.737591	24.926490
158.279138	5682.765588	24.931507
158.167367	5688.674804	24.936525
158.297925	5701.752236	24.941543
158.225359	5712.289312	24.946560
158.394621	5714.747780	24.951578
158.670967	5710.110561	24.956595
158.759394	5726.686439	24.961613
159.146908	5727.236011	24.966631
159.346319	5724.651163	24.971648
159.117421	5727.011830	24.976666
159.481434	5743.468255	24.981683
159.206419	5757.829120	24.986701
159.666865	5759.933539	24.991719
160.034371	5771.099934	24.996736
159.807650	5793.557736	25.001754
160.493474	5786.655369	25.006771
160.555962	5789.585633	25.011789
160.569472	5794.072875	25.016807
160.763701	5812.887677	25.021824
160.769688	5818.923723	25.026842
161.474326	5821.696531	25.031859
161.283056	5831.072447	25.036877
161.491718	5826.789020	25.041895
161.693524	5841.513750	25.046912
161.660798	5850.792802	25.051930
161.789052	5852.589855	25.056947
161.765489	5849.215990	25.061965
162.105779	5856.067356	25.066983
162.325588	5866.913550	25.072000
162.250203	5873.100280	25.077018
162.493903	5876.070118	25.082035
162.510708	5891.574200	25.087053
162.925130	5906.783585	25.092071
163.190409	5902.919120	25.097088
163.277586	5910.312838	25.102106
163.574789	5902.410221	25.107123
163.474980	5911.121720	25.112141
163.851873	5930.249011	25.117159
164.080977	5936.866372	25.122176
163.901551	5936.912324	25.127194
164.376576	5921.875874	25.132211
164.487925	5941.902330	25.137229
164.637650	5954.272755	25.142247
164.953672	5958.498594	25.147264
164.932453	5952.804094	25.152282
165.286474	5956.101759	25.157299
165.670473	5950.923300	25.162317
165.891493	5969.796186	25.167335
166.127692	5970.594916	25.172352
165.978099	5980.849419	25.177370
166.400617	5978.882777	25.182387
166.230540	5974.609341	25.187405
166.231277	5973.822469	25.192423
166.482563	5967.772946	25.197440
166.582010	5976.280407	25.202458
166.821395	5993.189717	25.207475
166.929789	6000.456571	25.212493
167.196898	5996.294384	25.217511
167.344502	5995.873555	25.222528
167.164858	6003.630873	25.227546
167.701105	6011.608437	25.232563
167.528928	6030.216788	25.237581
168.001868	6022.054772	25.242599
168.444453	6021.712010	25.247616
168.448626	6030.496694	25.252634
168.683762	6036.608018	25.257651
168.712323	6050.310211	25.262669
168.913136	6046.854105	25.267687
169.249558	6042.353548	25.272704
169.036806	6052.243657	25.277722
169.437837	6054.524394	25.282739
169.313642	6079.244047	25.287757
169.472581	6078.893007	25.292775
169.733728	6077.615350	25.297792
169.397140	6081.793428	25.302810
169.885109	6097.666354	25.307827
169.982528	6110.482708	25.312845
170.220173	6116.491381	25.317863
170.470195	6138.228518	25.322880
170.294619	6139.815979	25.327898
170.595639	6138.468229	25.332915
170.753645	6162.931378	25.337933
170.545200	6167.523361	25.342951
171.250881	6165.100839	25.347968
171.282305	6194.169687	25.352986
171.055494	6201.958232	25.358003
171.309389	6210.441989	25.363021
171.850834	6231.504143	25.368039
172.049136	6230.628322	25.373056
172.053868	6245.955308	25.378074
172.122089	6252.523716	25.383091
172.515265	6259.331432	25.388109
172.479842	6276.387166	25.393127
173.049215	6287.162198	25.398144
172.993558	6300.394165	25.403162
173.182904	6292.155264	25.408179
173.249213	6320.092091	25.413197
173.555511	6332.926475	25.418215
173.564120	6327.600809	25.423232
173.760007	6340.239579	25.428250
174.521396	6344.569980	25.433267
174.896339	6344.531477	25.438285
174.724935	6345.945984	25.443303
175.300965	6363.890199	25.448320
175.131478	6375.946792	25.453338
175.576268	6375.994718	25.458355
175.775919	6375.545124	25.463373
175.972381	6373.772625	25.468391
176.110123	6375.993107	25.473408
175.770185	6386.454482	25.478426
176.026278	6366.990490	25.483443
176.127825	6395.727534	25.488461
176.246840	6405.387947	25.493479
176.406530	6398.984626	25.498496
176.548537	6407.059884	25.503514
176.649495	6426.837659	25.508531
176.768369	6435.479979	25.513549
177.049487	6444.605504	25.518567
177.853721	6449.317792	25.523584
178.088833	6457.954967	25.528602
177.858204	6450.574475	25.533619
178.270003	6442.739066	25.538637
178.074813	6455.555949	25.543655
178.667131	6469.780787	25.548672
178.449594	6479.508284	25.553690
178.905160	6469.403001	25.558707
179.236674	6472.376271	25.563725
179.376764	6472.277649	25.568743
179.516281	6468.119939	25.573760
179.687018	6484.394781	25.578778
179.629185	6489.835428	25.583795
180.095894	6489.948314	25.588813
179.928579	6499.935334	25.593831
180.397088	6499.784349	25.598848
180.472382	6503.032161	25.603866
180.582929	6499.664305	25.608883
180.514977	6511.815760	25.613901
180.657621	6517.701265	25.618919
180.934850	6535.195274	25.623936
180.543847	6539.263343	25.628954
180.540238	6545.061235	25.633971
181.251423	6552.853054	25.638989
181.179336	6577.426747	25.644007
181.419814	6586.562774	25.649024
181.724575	6600.523578	25.654042
181.988598	6602.313239	25.659059
182.290622	6622.886955	25.664077
182.498600	6623.384149	25.669095
182.880681	6611.333659	25.674112
183.091398	6628.619646	25.679130
183.529588	6636.245741	25.684148
183.792436	6631.199668	25.689165
183.211339	6637.546814	25.694183
183.906883	6637.037034	25.699200
183.934297	6646.326665	25.704218
183.901388	6655.875344	25.709236
184.251850	6665.875128	25.714253
184.071458	6663.647309	25.719271
184.626213	6669.552146	25.724288
184.564524	6695.610689	25.729306
184.695094	6700.091345	25.734324
184.893495	6697.863713	25.739341
185.109626	6720.498583	25.744359
185.202599	6725.291317	25.749376
185.394857	6738.528996	25.754394
185.399506	6756.448338	25.759412
185.604272	6771.672372	25.764429
185.764132	6794.587784	25.769447
186.147584	6794.023110	25.774464
186.170609	6807.498703	25.779482
186.231936	6825.755299	25.784500
186.647693	6835.363173	25.789517
186.880279	6856.473103	25.794535
187.590648	6838.457808	25.799552
188.280731	6831.478756	25.804570
188.508742	6833.659737	25.809588
189.037345	6826.256363	25.814605
189.112533	6832.135437	25.819623
189.527686	6819.270641	25.824640
189.176660	6821.848443	25.829658
189.062749	6821.108132	25.834676
189.637976	6816.964263	25.839693
189.483537	6816.046294	25.844711
189.550868	6810.427833	25.849728
189.461942	6814.940371	25.854746
189.809125	6813.918822	25.859764
189.870831	6802.044363	25.864781
189.631551	6820.056964	25.869799
189.828458	6823.797686	25.874816
190.166708	6841.239840	25.879834
190.310657	6850.090850	25.884852
190.779404	6865.646641	25.889869
190.733545	6872.644240	25.894887
190.546398	6873.248503	25.899904
190.724094	6885.161242	25.904922
191.023192	6900.344404	25.909940
191.330261	6902.220874	25.914957
191.206706	6930.868949	25.919975
191.225114	6941.490746	25.924992
191.306235	6964.245869	25.930010
191.630775	6983.992281	25.935028
192.361874	6990.032010	25.940045
192.200316	7003.591501	25.945063
192.467607	7016.472828	25.950080
192.455421	7045.120677	25.955098
192.948725	7051.809723	25.960116
193.346402	7058.052139	25.965133
193.040955	7074.077793	25.970151
193.623686	7080.761250	25.975168
193.888586	7097.271182	25.980186
193.805398	7104.168617	25.985204
194.480376	7110.271636	25.990221
194.639919	7118.904723	25.995239
194.762238	7134.669464	26.000256
194.957314	7155.977005	26.005274
195.208118	7160.593641	26.010292
195.353143	7167.822180	26.015309
195.283760	7183.364170	26.020327
195.839869	7188.519918	26.025344
195.755390	7198.604358	26.030362
195.973829	7220.235597	26.035380
196.510789	7223.617693	26.040397
196.412514	7223.811225	26.045415
196.769661	7239.745581	26.050432
197.459015	7241.332959	26.055450
197.456229	7249.579690	26.060468
198.216063	7244.155961	26.065485
197.832383	7244.441420	26.070503
198.191731	7244.730380	26.075520
198.098553	7259.370571	26.080538
198.066813	7274.534471	26.085556
198.395579	7269.428105	26.090573
198.586509	7290.867118	26.095591
198.838656	7288.531687	26.100608
199.290903	7297.108770	26.105626
199.062665	7302.061487	26.110644
199.518524	7303.936321	26.115661
200.255140	7315.231527	26.120679
200.120800	7322.027844	26.125696
200.171793	7318.999780	26.130714
200.178747	7324.805734	26.135732
200.469540	7313.190992	26.140749
200.404175	7328.799376	26.145767
200.642386	7347.584722	26.150784
200.826198	7353.947129	26.155802
201.155646	7361.366682	26.160820
201.451088	7375.967849	26.165837
201.395952	7387.163509	26.170855
201.461590	7387.814832	26.175872
201.667896	7382.268423	26.180890
201.488802	7403.905867	26.185908
201.810690	7416.623038	26.190925
201.697349	7432.247047	26.195943
202.492894	7444.195499	26.200960
202.823492	7449.879086	26.205978
202.916263	7477.167849	26.210996
203.471665	7468.662996	26.216013
203.739160	7475.114407	26.221031
204.326627	7484.547399	26.226048
205.128378	7473.567124	26.231066
205.163590	7462.426577	26.236084
205.136326	7446.171136	26.241101
205.205550	7443.855402	26.246119
205.192658	7439.082786	26.251136
205.393560	7435.574417	26.256154
205.370094	7444.359622	26.261172
205.840602	7453.634197	26.266189
205.834095	7467.519546	26.271207
205.592044	7469.978575	26.276224
205.683410	7464.910779	26.281242
205.641210	7488.529099	26.286260
206.270154	7489.332189	26.291277
206.690862	7505.085948	26.296295
206.681346	7517.368969	26.301312
207.260628	7531.833761	26.306330
206.803171	7531.768237	26.311348
207.395653	7547.174399	26.316365
207.538199	7561.875665	26.321383
207.662630	7568.301926	26.326400
207.782350	7581.865098	26.331418
207.717293	7594.537884	26.336436
207.960495	7608.245850	26.341453
208.002035	7622.009586	26.346471
208.231397	7635.746537	26.351488
208.706778	7654.899702	26.356506
208.633108	7674.463832	26.361524
209.179549	7693.121787	26.366541
209.203688	7706.151855	26.371559
209.398868	7727.335870	26.376576
209.885273	7727.329966	26.381594
209.825226	7752.120854	26.386612
210.039475	7765.355156	26.391629
210.425926	7786.222336	26.396647
210.445309	7799.067538	26.401664
211.166308	7797.163251	26.406682
211.444364	7811.040536	26.411700
212.043104	7812.070363	26.416717
212.047306	7810.961006	26.421735
212.095498	7828.199547	26.426752
212.664828	7830.678002	26.431770
212.819378	7843.215266	26.436788
212.726342	7847.771263	26.441805
213.022058	7845.983557	26.446823
212.852437	7847.085522	26.451840
213.209993	7839.064858	26.456858
213.253195	7863.863471	26.461876
213.444753	7874.532296	26.466893
213.675481	7877.590383	26.471911
213.941571	7882.506582	26.476928
214.458224	7883.507010	26.481946
214.617783	7900.775880	26.486964
214.765618	7900.085457	26.491981
215.294324	7898.843294	26.496999
215.648792	7920.147765	26.502016
215.735427	7917.330293	26.507034
215.687721	7924.651305	26.512052
215.976743	7915.770437	26.517069
216.255155	7915.574216	26.522087
216.109136	7930.184143	26.527104
216.333647	7942.670207	26.532122
216.511758	7945.386136	26.537140
216.702664	7953.353325	26.542157
217.086390	7972.220526	26.547175
217.093732	7976.207765	26.552192
217.151519	7973.983872	26.557210
217.303161	7999.559006	26.562228
217.557066	8009.397257	26.567245
217.574720	8026.095181	26.572263
217.713432	8042.926877	26.577280
218.273168	8047.659790	26.582298
218.077778	8066.853930	26.587316
218.350629	8088.640252	26.592333
218.649472	8108.005493	26.597351
218.764367	8133.823572	26.602368
219.265973	8140.403988	26.607386
219.454728	8173.811455	26.612404
219.822181	8174.228594	26.617421
220.476573	8188.318898	26.622439
220.211489	8199.765429	26.627456
220.830186	8207.576029	26.632474
221.168965	8224.340623	26.637492
221.126481	8222.516297	26.642509
221.926427	8213.191431	26.647527
222.273162	8227.762832	26.652544
222.683746	8229.367623	26.657562
222.696891	8235.652171	26.662580
222.777135	8230.203846	26.667597
222.911825	8237.124119	26.672615
222.839099	8236.768261	26.677632
223.148021	8226.094215	26.682650
223.313332	8238.360581	26.687668
223.261919	8247.599644	26.692685
223.423154	8253.723669	26.697703
223.745652	8270.527503	26.702720
224.195454	8280.477527	26.707738
224.266787	8307.013038	26.712756
224.547653	8303.124232	26.717773
224.593828	8312.339122	26.722791
224.722331	8327.403787	26.727808
225.058298	8328.733656	26.732826
225.471284	8326.713160	26.737844
225.457371	8353.051449	26.742861
225.770861	8355.175753	26.747879
225.646420	8361.717968	26.752896
226.016686	8371.450955	26.757914
225.962161	8392.795728	26.762932
226.238988	8401.192888	26.767949
226.483829	8422.326693	26.772967
226.462951	8438.273419	26.777984
226.862435	8444.396132	26.783002
227.024337	8464.301461	26.788020
227.420954	8480.930037	26.793037
227.895341	8489.377985	26.798055
227.820007	8518.840992	26.803072
228.317993	8522.335451	26.808090
228.402183	8541.714229	26.813108
228.790805	8553.215381	26.818125
229.457034	8553.133996	26.823143
229.427780	8571.915915	26.828160
229.710231	8571.803640	26.833178
229.685806	8570.948639	26.838196
230.007404	8587.908786	26.843213
230.353915	8600.387756	26.848231
230.492718	8606.016984	26.853248
231.369691	8606.970257	26.858266
231.494488	8606.715892	26.863284
231.453451	8613.782000	26.868301
232.258280	8595.920316	26.873319
232.340199	8607.656907	26.878336
232.771540	8597.572165	26.883354
232.753629	8593.006549	26.888372
233.015294	8610.844651	26.893389
233.339818	8617.224515	26.898407
233.779738	8622.483500	26.903424
234.688997	8595.496867	26.908442
234.578253	8588.666323	26.913460
234.511166	8558.811241	26.918477
234.904453	8548.486290	26.923495
234.544030	8550.335610	26.928512
234.655269	8553.379049	26.933530
234.935171	8567.002177	26.938548
235.115691	8569.801645	26.943565
235.118273	8578.540476	26.948583
235.341684	8592.742760	26.953600
235.672737	8590.470886	26.958618
235.670269	8613.021510	26.963636
235.583108	8616.043866	26.968653
236.161135	8621.517307	26.973671
236.287441	8638.695934	26.978688
236.556939	8647.142011	26.983706
236.411719	8648.191353	26.988724
236.771868	8667.137559	26.993741
237.015994	8672.136216	26.998759
236.702821	8691.096538	27.003776
237.439232	8703.020820	27.008794
237.793254	8710.309259	27.013812
237.773289	8738.425299	27.018829
238.079170	8743.498731	27.023847
238.121938	8764.043163	27.028864
238.386758	8777.119998	27.033882
238.740436	8800.951529	27.038900
238.977554	8805.484694	27.043917
239.287603	8822.728674	27.048935
239.770361	8843.200320	27.053952
240.127163	8833.966575	27.058970
240.572083	8851.398808	27.063988
240.430709	8854.005692	27.069005
240.937532	8857.734120	27.074023
240.689708	8879.933542	27.079040
241.260991	8874.712432	27.084058
241.735555	8878.038766	27.089076
241.656864	8905.186705	27.094093
242.151438	8909.000122	27.099111
242.051043	8918.514180	27.104128
242.796349	8936.720984	27.109146
243.263315	8946.639998	27.114164
242.964814	8948.275674	27.119181
243.148717	8953.358786	27.124199
243.138040	8978.492058	27.129216
243.364478	8985.666009	27.134234
243.620460	8996.129811	27.139252
243.678943	9012.582309	27.144269
244.046933	9027.074378	27.149287
244.226016	9055.481931	27.154304
244.430137	9064.436020	27.159322
244.997579	9078.612648	27.164340
245.526910	9091.391440	27.169357
245.902341	9092.152026	27.174375
245.904275	9101.873776	27.179392
245.919403	9113.783916	27.184410
246.109170	9124.774607	27.189428
246.230777	9145.394738	27.194445
246.842340	9149.412671	27.199463
246.895828	9180.828949	27.204480
247.226475	9191.537535	27.209498
247.448477	9204.211959	27.214516
247.752624	9210.714946	27.219533
248.144599	9224.616311	27.224551
248.298736	9237.845371	27.229568
248.504243	9255.799828	27.234586
248.501582	9261.393619	27.239604
248.612301	9271.404659	27.244621
249.464979	9297.028440	27.249639
249.488080	9310.413416	27.254656
249.534463	9323.024647	27.259674
249.892652	9328.980000	27.264692
250.335291	9347.454725	27.269709
250.548076	9340.831570	27.274727
250.656078	9363.587635	27.279744
250.965396	9370.892969	27.284762
251.204864	9379.292702	27.289780
251.191849	9388.252874	27.294797
251.309290	9396.707876	27.299815
251.390907	9424.939251	27.304832
251.752630	9440.335376	27.309850
252.516843	9457.087841	27.314868
252.405962	9478.783113	27.319885
252.579591	9471.113173	27.324903
252.725153	9499.806679	27.329920
253.124410	9523.646654	27.334938
253.310997	9539.472943	27.339956
253.526731	9565.356899	27.344973
253.718831	9572.830936	27.349991
254.026542	9589.975834	27.355008
254.070771	9610.783254	27.360026
254.693031	9630.687970	27.365044
254.686853	9658.863345	27.370061
255.301998	9678.463122	27.375079
255.635295	9683.957872	27.380096
255.838827	9712.315550	27.385114
256.034636	9721.569232	27.390132
255.986213	9738.582192	27.395149
256.301035	9747.426573	27.400167
256.653789	9772.734218	27.405184
256.738320	9785.466855	27.410202
257.247144	9799.816026	27.415220
257.634578	9818.178936	27.420237
257.779863	9836.212155	27.425255
258.319749	9849.098913	27.430272
258.246041	9867.453150	27.435290
258.363620	9888.032444	27.440308
258.800299	9905.723780	27.445325
259.314914	9918.705525	27.450343
259.556975	9939.219794	27.455360
259.529559	9950.281125	27.460378
259.737252	9966.184379	27.465396
260.028771	9988.167634	27.470413
260.235151	9994.968688	27.475431
260.513602	10019.502773	27.480448
261.055891	10032.462104	27.485466
261.406457	10048.783786	27.490484
261.674638	10055.607283	27.495501
262.698517	10064.739410	27.500519
262.795478	10088.220408	27.505536
262.720335	10096.422000	27.510554
263.246743	10081.700611	27.515572
263.418210	10087.186284	27.520589
263.442368	10101.439468	27.525607
264.032710	10110.621056	27.530624
263.994734	10114.267050	27.535642
264.093571	10106.563851	27.540660
264.371932	10127.549910	27.545677
264.802003	10139.263682	27.550695
265.127441	10138.216670	27.555712
265.276014	10151.281756	27.560730
265.623863	10158.180746	27.565748
265.772393	10172.543242	27.570765
265.866060	10171.443060	27.575783
266.230482	10179.113442	27.580800
266.374733	10202.426136	27.585818
266.491548	10199.527482	27.590836
266.518911	10228.644169	27.595853
267.000028	10238.201338	27.600871
267.233786	10251.600792	27.605888
267.443629	10267.962262	27.610906
267.622271	10277.373672	27.615924
267.951916	10290.913706	27.620941
268.414741	10313.404908	27.625959
268.432923	10325.623638	27.630976
268.595526	10342.084209	27.635994
268.923159	10348.816907	27.641012
269.324386	10369.750665	27.646029
269.551307	10388.586493	27.651047
269.881557	10404.913768	27.656064
270.418629	10430.767274	27.661082
270.615500	10433.515300	27.666100
270.945684	10443.786486	27.671117
271.313016	10456.929118	27.676135
271.603027	10471.378744	27.681152
271.967602	10485.002712	27.686170
272.247878	10496.951172	27.691188
272.272713	10513.879742	27.696205
272.520798	10514.213676	27.701223
273.007721	10528.564678	27.706240
273.031212	10549.993731	27.711258
273.088748	10556.812863	27.716276
273.150994	10581.143464	27.721293
273.631849	10596.065702	27.726311
274.308763	10601.090073	27.731328
274.622710	10617.489043	27.736346
274.874193	10629.935668	27.741364
274.796286	10653.407641	27.746381
275.370838	10657.013583	27.751399
275.597386	10666.572646	27.756416
275.533517	10697.121049	27.761434
275.728208	10703.183292	27.766452
276.599982	10706.308999	27.771469
277.037432	10720.462655	27.776487
277.351309	10723.419932	27.781504
277.495073	10745.025275	27.786522
277.655817	10749.532249	27.791540
277.513009	10762.879243	27.796557
277.861580	10783.524076	27.801575
278.432165	10783.300544	27.806592
278.190591	10815.647961	27.811610
278.701870	10817.779272	27.816628
278.993305	10825.166086	27.821645
278.915553	10837.308436	27.826663
279.569203	10856.669868	27.831680
279.915733	10873.020243	27.836698
280.393926	10883.386588	27.841716
280.293336	10894.387865	27.846733
280.429788	10906.125035	27.851751
280.930654	10924.045817	27.856768
280.832870	10946.816612	27.861786
281.294134	10958.186835	27.866804
281.582458	10977.692836	27.871821
281.519982	10985.173919	27.876839
281.755872	11004.011447	27.881856
282.065066	11032.571208	27.886874
282.509475	11059.625476	27.891892
282.823454	11079.704038	27.896909
283.149675	11099.724008	27.901927
283.641096	11111.017918	27.906944
283.985398	11135.692670	27.911962
284.252135	11148.471988	27.916980
284.566306	11165.803007	27.921997
284.472203	11192.853231	27.927015
285.070917	11199.356964	27.932032
285.291369	11219.409299	27.937050
285.724847	11228.532759	27.942068
285.843553	11251.143179	27.947085
286.220579	11266.918301	27.952103
286.788607	11276.787931	27.957120
287.040464	11304.728085	27.962138
287.056021	11308.602741	27.967156
288.113626	11308.842886	27.972173
288.277602	11323.262259	27.977191
288.641892	11326.298790	27.982208
289.005689	11327.617226	27.987226
289.047804	11336.859212	27.992244
289.091882	11351.754421	27.997261
289.598488	11356.098424	28.002279
290.516098	11356.475601	28.007296
290.397278	11364.272022	28.012314
290.670069	11356.808066	28.017332
291.244215	11367.297190	28.022349
291.408821	11379.535147	28.027367
291.971225	11380.703282	28.032384
292.031130	11398.737418	28.037402
292.090045	11396.085070	28.042420
292.063484	11404.611771	28.047437
292.134808	11421.368268	28.052455
292.368187	11425.552186	28.057472
292.607344	11448.098052	28.062490
292.783830	11459.596690	28.067508
293.426107	11482.738319	28.072525
293.489459	11496.783309	28.077543
293.773662	11513.330457	28.082560
293.655819	11535.050843	28.087578
294.180219	11553.137453	28.092596
294.519856	11567.666210	28.097613
294.383743	11591.180593	28.102631
294.874606	11602.769332	28.107648
294.930555	11626.800378	28.112666
295.056991	11654.353065	28.117684
295.657677	11667.802339	28.122701
295.811531	11693.260223	28.127719
296.061454	11713.680416	28.132736
296.103017	11747.183820	28.137754
296.488293	11775.156509	28.142772
297.178312	11804.264467	28.147789
297.028720	11823.545412	28.152807
297.515973	11840.002309	28.157824
298.262994	11861.642966	28.162842
298.375020	11882.683560	28.167860
298.449249	11901.825032	28.172877
298.930256	11928.369706	28.177895
299.236728	11953.721449	28.182912
299.365967	11980.117043	28.187930
299.695817	11999.633684	28.192948
300.324019	12021.350573	28.197965
300.549851	12045.620065	28.202983
300.818024	12069.220102	28.208000
301.052081	12103.834130	28.213018
301.540953	12121.559110	28.218036
301.780189	12132.920353	28.223053
302.171716	12158.228971	28.228071
302.543698	12168.776459	28.233088
302.535338	12196.565513	28.238106
302.782227	12226.534782	28.243124
303.284070	12241.258922	28.248141
303.734965	12271.543474	28.253159
304.356241	12285.908193	28.258176
304.549925	12300.342651	28.263194
304.464088	12322.249147	28.268212
305.118256	12336.708833	28.273229
305.256816	12353.922405	28.278247
305.899205	12381.304837	28.283264
306.195837	12403.100311	28.288282
306.437088	12412.653611	28.293300
306.899261	12416.006146	28.298317
306.816686	12442.212955	28.303335
307.645795	12446.193191	28.308352
307.571558	12467.778671	28.313370
307.857204	12482.188019	28.318388
307.814030	12495.539936	28.323405
308.246270	12522.062921	28.328423
308.439457	12546.506469	28.333440
308.707112	12573.384010	28.338458
309.135510	12586.623063	28.343476
309.650153	12599.866093	28.348493
309.778760	12624.155153	28.353511
310.467058	12633.174505	28.358528
310.868418	12649.173888	28.363546
311.140866	12671.261496	28.368564
311.795411	12675.339477	28.373581
311.589841	12693.117364	28.378599
311.871939	12699.969954	28.383616
312.213240	12713.898171	28.388634
312.413690	12725.497853	28.393652
312.962723	12742.129487	28.398669
312.684001	12765.336827	28.403687
312.915470	12782.332009	28.408704
313.287286	12803.657365	28.413722
313.748614	12823.120165	28.418740
314.232558	12840.371828	28.423757
314.439773	12860.218471	28.428775
315.309480	12867.482341	28.433792
315.684363	12882.322193	28.438810
316.065195	12899.861040	28.443828
316.592684	12907.243232	28.448845
316.385881	12909.618200	28.453863
316.792530	12925.029226	28.458880
316.675791	12936.418387	28.463898
316.959529	12955.598244	28.468916
317.757118	12966.132081	28.473933
317.614856	12989.686302	28.478951
317.799690	13002.767554	28.483968
318.296785	13016.143627	28.488986
319.014162	13032.334016	28.494004
319.518464	13045.894048	28.499021
319.453308	13056.794910	28.504039
319.601180	13080.883560	28.509056
319.858578	13087.583618	28.514074
320.377126	13114.084731	28.519092
320.449652	13137.678252	28.524109
320.502252	13163.104872	28.529127
321.188596	13170.237731	28.534144
321.600004	13200.036285	28.539162
321.345869	13216.785822	28.544180
322.278256	13237.645392	28.549197
322.195549	13268.356640	28.554215
322.909021	13281.866031	28.559232
323.516406	13300.157682	28.564250
323.569946	13316.148459	28.569268
324.127579	13329.687355	28.574285
324.257427	13343.489268	28.579303
325.383286	13346.800492	28.584320
325.979444	13353.144796	28.589338
325.777241	13363.940197	28.594356
326.614140	13351.983976	28.599373
326.437863	13359.866239	28.604391
326.819385	13381.339538	28.609408
326.935726	13389.720299	28.614426
327.269531	13393.489662	28.619444
327.781877	13400.458686	28.624461
328.125580	13412.659506	28.629479
328.203127	13421.872119	28.634496
328.387492	13444.317705	28.639514
328.308478	13453.400805	28.644532
328.890482	13465.798465	28.649549
328.727417	13486.948488	28.654567
328.958799	13512.136207	28.659584
329.491944	13517.808727	28.664602
329.796576	13543.595578	28.669620
330.035963	13551.724501	28.674637
330.254651	13573.954628	28.679655
330.440958	13600.861022	28.684672
331.292062	13625.376497	28.689690
331.048008	13654.566819	28.694708
331.439384	13671.611407	28.699725
331.854219	13696.268653	28.704743
331.885813	13727.640084	28.709760
332.495114	13756.653761	28.714778
332.695393	13782.123680	28.719796
333.512423	13786.158264	28.724813
333.695587	13814.135530	28.729831
334.636623	13826.340276	28.734848
335.375173	13830.933599	28.739866
335.597018	13839.763126	28.744884
335.741523	13848.638933	28.749901
336.028692	13864.534797	28.754919
336.087374	13880.143060	28.759936
336.534971	13888.474845	28.764954
337.101835	13904.756775	28.769972
337.730421	13918.769021	28.774989
337.448224	13932.985867	28.780007
337.730896	13945.218982	28.785024
338.301512	13963.839164	28.790042
338.383744	13973.976503	28.795060
338.804161	13993.293031	28.800077
338.924643	14007.130788	28.805095
338.957782	14029.999959	28.810112
339.565621	14044.017694	28.815130
339.429951	14071.730769	28.820148
339.942663	14093.630120	28.825165
340.147304	14134.089056	28.830183
340.544190	14157.624389	28.835200
341.027069	14187.740080	28.840218
341.076925	14215.491155	28.845236
341.897388	14231.667975	28.850253
341.859680	14260.770081	28.855271
342.414506	14289.776924	28.860288
342.798266	14303.000876	28.865306
343.094763	14339.930470	28.870324
343.484009	14362.109076	28.875341
343.789699	14390.661437	28.880359
344.165738	14410.656579	28.885376
344.994288	14431.256157	28.890394
345.093342	14452.906662	28.895412
345.565716	14476.152660	28.900429
345.735895	14494.853841	28.905447
345.899366	14508.304966	28.910464
347.091002	14512.734483	28.915482
347.410286	14515.155156	28.920500
347.960853	14525.988752	28.925517
348.248454	14548.670439	28.930535
348.453406	14562.783857	28.935552
349.013860	14549.395888	28.940570
348.623553	14567.071656	28.945588
349.087915	14577.813538	28.950605
349.257601	14581.237878	28.955623
349.436664	14610.532235	28.960640
349.907758	14624.643544	28.965658
349.790267	14650.696151	28.970676
350.475785	14668.561533	28.975693
350.932213	14698.734307	28.980711
351.142091	14718.337716	28.985728
351.346124	14740.015489	28.990746
351.290465	14762.402757	28.995764
352.105656	14784.814923	29.000781
352.610085	14809.475139	29.005799
352.854317	14831.908103	29.010816
353.022649	14847.258289	29.015834
353.546182	14880.590692	29.020852
354.185656	14896.725032	29.025869
354.720604	14921.403592	29.030887
354.783228	14944.002546	29.035904
355.118354	14956.361257	29.040922
355.563342	14976.146090	29.045940
355.903970	15002.368463	29.050957
356.345476	15018.799592	29.055975
356.285162	15041.454396	29.060992
356.821215	15064.472185	29.066010
357.021610	15092.909292	29.071028
357.580722	15109.974319	29.076045
357.618703	15141.548965	29.081063
357.902287	15170.967670	29.086080
358.445631	15185.414677	29.091098
358.753504	15212.566490	29.096116
359.268190	15232.208776	29.101133
359.888182	15258.172831	29.106151
359.941508	15290.548453	29.111168
360.359198	15304.855584	29.116186
360.828511	15335.908519	29.121204
361.432598	15352.683230	29.126221
361.837912	15379.583135	29.131239
361.920798	15396.771218	29.136256
362.326857	15414.527998	29.141274
362.783838	15438.995344	29.146292
363.267442	15461.974064	29.151309
363.627550	15484.613694	29.156327
363.820165	15502.656916	29.161344
365.431603	15474.970781	29.166362
366.298378	15472.390730	29.171380
366.760573	15469.862951	29.176397
367.040893	15471.575923	29.181415
367.221160	15474.420224	29.186432
367.601765	15467.252013	29.191450
367.815591	15466.734188	29.196468
367.701272	15473.775990	29.201485
368.077991	15474.965016	29.206503
368.042727	15471.992771	29.211520
368.090687	15476.738189	29.216538
368.335272	15502.382818	29.221556
368.723826	15506.608093	29.226573
369.242406	15525.961991	29.231591
368.843834	15549.288089	29.236608
369.445710	15568.235517	29.241626
369.386673	15593.881839	29.246644
369.716877	15618.689315	29.251661
369.927282	15646.792632	29.256679
370.059322	15683.246520	29.261696
370.790202	15707.161857	29.266714
370.827459	15753.410799	29.271732
371.249905	15788.931374	29.276749
371.859004	15805.586903	29.281767
372.378422	15853.291001	29.286784
373.052769	15879.012831	29.291802
373.146768	15904.658703	29.296820
373.286704	15931.006070	29.301837
374.068400	15962.442527	29.306855
374.342350	15998.497424	29.311872
374.857514	16008.877537	29.316890
375.091622	16041.166879	29.321908
375.752029	16062.130754	29.326925
376.225514	16088.182744	29.331943
376.313094	16120.474738	29.336960
376.911022	16141.757700	29.341978
377.277885	16162.853915	29.346996
377.385186	16189.935194	29.352013
377.758316	16212.639169	29.357031
378.391821	16246.017144	29.362048
378.772145	16264.608455	29.367066
379.265291	16300.358485	29.372084
379.576591	16331.028807	29.377101
380.141961	16352.944947	29.382119
380.038646	16381.534002	29.387136
380.320086	16403.795235	29.392154
380.705941	16426.349873	29.397172
381.197572	16466.258036	29.402189
381.645407	16498.518212	29.407207
381.693577	16523.921845	29.412224
382.586049	16547.945408	29.417242
382.571396	16585.278078	29.422260
382.886203	16615.582096	29.427277
383.667330	16641.185437	29.432295
383.634567	16678.821195	29.437312
384.331305	16704.013119	29.442330
384.733450	16745.076535	29.447348
385.277759	16769.335047	29.452365
385.569610	16793.724569	29.457383
386.022314	16826.033272	29.462400
386.190680	16850.649241	29.467418
386.630992	16870.898748	29.472436
386.611014	16905.816450	29.477453
387.276863	16921.092966	29.482471
387.189849	16964.448566	29.487488
387.549237	16985.815783	29.492506
388.169229	17029.256136	29.497524
388.423710	17057.237480	29.502541
388.855481	17086.123258	29.507559
389.315235	17125.652983	29.512576
389.690278	17149.830015	29.517594
389.980616	17178.379068	29.522612
390.356230	17210.328235	29.527629
390.749844	17248.929480	29.532647
391.244645	17278.542554	29.537664
391.453310	17316.125048	29.542682
392.060417	17349.513551	29.547700
392.429586	17382.602650	29.552717
393.206164	17413.954105	29.557735
393.217576	17448.187333	29.562752
393.587484	17480.778503	29.567770
394.377929	17508.400065	29.572788
394.615955	17550.231516	29.577805
395.225426	17567.108184	29.582823
395.595186	17596.849271	29.587840
396.075483	17620.095710	29.592858
396.502186	17651.147891	29.597876
396.795565	17676.347803	29.602893
397.551965	17698.220059	29.607911
397.788559	17721.876349	29.612928
398.207944	17744.287803	29.617946
398.695212	17773.022712	29.622964
398.950315	17805.647032	29.627981
399.591463	17826.988229	29.632999
399.731109	17844.570775	29.638016
400.160763	17874.255212	29.643034
400.782908	17900.960196	29.648052
400.962770	17922.376604	29.653069
401.590202	17955.879712	29.658087
401.932461	17979.206168	29.663104
402.079742	17998.177056	29.668122
402.798086	18031.495761	29.673140
402.784142	18061.588648	29.678157
403.048249	18087.984858	29.683175
403.634102	18114.183384	29.688192
404.006371	18138.926979	29.693210
404.634849	18169.017710	29.698228
404.723542	18200.893766	29.703245
405.234659	18234.860511	29.708263
405.539603	18264.158073	29.713280
405.816202	18292.609000	29.718298
406.394772	18329.862158	29.723316
406.453104	18367.029005	29.728333
407.114764	18391.892644	29.733351
407.426349	18421.621745	29.738368
407.743919	18467.574648	29.743386
408.368997	18487.425159	29.748404
408.565625	18527.252359	29.753421
409.091622	18550.418104	29.758439
409.507330	18575.375167	29.763456
409.796528	18610.656503	29.768474
410.369824	18632.488781	29.773492
410.323834	18664.254561	29.778509
410.926647	18692.567225	29.783527
411.298230	18729.486585	29.788544
411.690167	18765.178697	29.793562
411.971256	18789.931162	29.798580
412.691661	18833.783820	29.803597
413.248947	18860.768918	29.808615
413.832934	18879.996120	29.813632
414.619835	18877.398946	29.818650
415.739340	18902.004611	29.823668
415.856334	18921.858284	29.828685
416.349499	18939.295179	29.833703
416.712716	18951.283497	29.838720
416.898451	18971.858225	29.843738
417.532048	18978.250704	29.848756
418.014300	19013.465181	29.853773
417.887949	19034.972858	29.858791
418.488530	19064.252774	29.863808
418.974217	19078.846299	29.868826
419.457868	19092.208958	29.873844
419.162498	19123.041309	29.878861
419.490469	19139.710195	29.883879
420.185513	19159.745317	29.888896
420.577781	19188.192441	29.893914
421.727477	19196.125364	29.898932
422.761344	19202.514403	29.903949
423.259267	19225.737996	29.908967
423.576579	19232.662125	29.913984
423.846138	19240.993208	29.919002
424.142561	19259.211486	29.924020
424.259922	19264.949265	29.929037
424.710370	19274.976509	29.934055
424.679057	19298.689694	29.939072
424.765678	19332.494954	29.944090
425.487171	19356.918281	29.949108
426.009794	19385.301290	29.954125
426.257848	19402.780123	29.959143
426.289079	19436.610183	29.964160
426.697139	19468.302887	29.969178
427.374324	19489.542985	29.974196
427.393559	19522.423070	29.979213
427.975421	19554.839521	29.984231
428.005738	19589.436284	29.989248
428.536968	19631.324251	29.994266
429.054023	19672.481036	29.999284
429.300173	19711.362700	30.004301
429.579064	19750.611731	30.009319
430.235481	19791.002829	30.014336
430.513057	19831.630795	30.019354
431.380173	19855.716700	30.024372
431.609993	19895.904350	30.029389
431.994792	19928.318717	30.034407
432.416183	19947.861770	30.039424
432.820211	19983.227530	30.044442
433.173287	20012.503380	30.049460
433.784939	20055.351065	30.054477
434.432305	20079.874750	30.059495
434.569655	20108.400785	30.064512
434.888224	20141.226598	30.069530
435.854508	20167.498301	30.074548
436.058775	20210.013227	30.079565
436.247596	20235.210702	30.084583
436.872331	20278.001391	30.089600
437.059526	20309.983785	30.094618
437.961075	20341.197201	30.099636
438.526541	20369.529888	30.104653
438.732756	20401.696083	30.109671
439.382614	20433.589262	30.114688
439.489394	20459.081318	30.119706
440.108879	20491.341720	30.124724
440.522316	20518.659351	30.129741
441.894937	20518.576932	30.134759
443.364084	20517.880606	30.139776
443.649970	20526.835081	30.144794
444.435112	20532.726030	30.149812
445.020288	20549.747636	30.154829
445.340268	20550.242455	30.159847
445.896011	20545.227096	30.164864
445.774831	20552.075983	30.169882
446.353146	20541.246561	30.174900
446.335650	20544.639741	30.179917
446.047226	20572.884397	30.184935
447.039619	20585.635694	30.189952
447.183132	20604.847005	30.194970
447.339650	20621.629845	30.199988
447.747396	20658.221167	30.205005
447.811442	20678.749404	30.210023
447.984006	20703.924234	30.215040
448.312684	20753.572531	30.220058
448.982391	20780.144931	30.225076
449.236696	20825.860461	30.230093
449.241996	20859.503191	30.235111
450.523407	20889.769609	30.240128
450.613957	20928.145509	30.245146
451.125957	20957.971541	30.250164
451.893452	20991.284413	30.255181
452.161949	21023.529378	30.260199
452.952444	21053.474247	30.265216
453.295515	21085.036451	30.270234
454.077598	21090.712310	30.275252
454.221777	21132.375343	30.280269
454.755196	21169.262860	30.285287
455.172679	21192.373817	30.290304
455.464821	21231.998931	30.295322
455.768442	21262.254890	30.300340
455.994799	21292.950083	30.305357
456.128848	21318.494317	30.310375
456.768416	21354.387183	30.315392
456.897800	21395.023112	30.320410
457.682567	21418.880795	30.325428
458.038003	21456.411655	30.330445
458.264745	21489.617204	30.335463
459.066512	21530.308598	30.340480
459.216604	21571.661538	30.345498
459.615475	21602.630709	30.350516
459.958911	21654.032671	30.355533
460.806076	21687.666692	30.360551
461.096996	21718.055502	30.365568
461.073924	21776.793663	30.370586
461.733781	21815.307846	30.375604
462.321845	21864.482770	30.380621
462.655468	21906.081431	30.385639
463.354570	21950.559757	30.390656
463.619253	21996.026563	30.395674
464.347818	22039.688418	30.400692
464.660066	22084.059416	30.405709
465.156973	22130.053543	30.410727
466.165333	22163.269088	30.415744
466.487540	22199.347547	30.420762
467.060729	22242.089570	30.425780
467.942992	22283.096160	30.430797
468.072652	22313.459823	30.435815
468.851493	22351.337282	30.440832
469.249497	22387.987729	30.445850
469.540742	22419.767218	30.450868
469.853760	22450.649337	30.455885
470.225563	22494.294462	30.460903
471.339006	22525.727361	30.465920
471.418186	22569.632763	30.470938
471.827216	22597.611595	30.475956
472.269963	22631.902005	30.480973
472.441472	22679.094802	30.485991
473.059829	22712.691848	30.491008
473.587925	22756.532549	30.496026
473.980343	22794.881424	30.501044
474.615467	22839.496106	30.506061
474.773217	22881.620782	30.511079
475.554706	22918.019172	30.516096
476.192872	22956.185145	30.521114
476.767521	22990.612849	30.526132
477.230480	23030.719356	30.531149
477.639016	23066.882131	30.536167
478.037445	23101.079007	30.541184
478.085626	23142.586184	30.546202
478.668888	23182.493533	30.551220
479.802581	23232.113519	30.556237
480.017815	23269.856905	30.561255
480.289454	23301.138746	30.566272
480.836076	23342.880533	30.571290
481.128862	23381.008030	30.576308
481.833001	23401.346452	30.581325
482.331479	23438.893093	30.586343
483.011519	23463.660640	30.591360
483.399984	23496.933639	30.596378
483.886543	23517.985072	30.601396
484.332085	23557.363923	30.606413
484.642338	23598.048360	30.611431
485.385775	23624.914710	30.616448
485.818425	23652.974349	30.621466
486.485147	23681.900234	30.626484
487.043412	23710.978934	30.631501
487.348016	23744.802234	30.636519
487.862023	23773.667544	30.641536
488.267007	23815.264568	30.646554
488.688967	23845.339617	30.651572
489.159982	23867.136006	30.656589
489.241528	23917.353477	30.661607
490.125798	23945.059685	30.666624
490.453363	23986.077133	30.671642
491.183578	24024.388553	30.676660
491.715182	24057.476077	30.681677
491.814189	24088.649118	30.686695
492.486788	24135.259904	30.691712
492.558061	24175.740484	30.696730
493.098440	24217.146053	30.701748
493.932285	24268.828103	30.706765
493.964505	24309.841443	30.711783
494.913591	24340.621967	30.716800
495.178041	24389.019701	30.721818
495.520688	24440.538725	30.726836
496.224892	24475.096313	30.731853
496.469076	24532.600774	30.736871
497.259829	24568.744671	30.741888
497.767411	24609.256097	30.746906
498.211782	24657.275436	30.751924
498.563871	24697.589713	30.756941
499.033327	24747.111495	30.761959
499.975132	24787.129602	30.766976
500.886687	24819.286928	30.771994
501.196541	24856.319471	30.777012
501.998876	24888.540026	30.782029
502.417781	24927.017434	30.787047
503.043019	24956.584027	30.792064
503.116648	25001.531334	30.797082
503.901574	25046.567123	30.802100
504.154938	25074.137113	30.807117
504.384033	25120.577221	30.812135
505.089679	25144.382236	30.817152
505.658732	25193.044258	30.822170
505.775600	25244.090574	30.827188
506.461189	25277.924177	30.832205
507.216182	25314.637144	30.837223
507.719468	25349.374371	30.842240
507.762524	25390.647142	30.847258
508.559921	25424.239514	30.852276
508.976317	25460.378893	30.857293
509.412800	25498.187621	30.862311
510.024830	25526.211739	30.867328
510.779563	25568.290943	30.872346
511.096160	25595.145111	30.877364
511.896485	25626.801056	30.882381
512.449887	25662.184057	30.887399
512.716710	25699.020576	30.892416
513.139130	25730.993749	30.897434
513.293373	25762.463761	30.902452
513.961518	25796.861365	30.907469
514.464624	25841.172240	30.912487
515.000922	25875.941589	30.917504
515.534194	25922.705830	30.922522
515.926794	25961.598784	30.927540
516.611720	25994.668259	30.932557
517.061845	26036.543542	30.937575
517.457733	26073.548647	30.942592
518.144084	26124.845804	30.947610
518.735878	26160.750049	30.952628
519.050667	26202.722954	30.957645
519.727575	26255.374717	30.962663
520.390173	26291.437357	30.967680
520.811319	26340.814192	30.972698
521.131304	26379.243876	30.977716
521.564730	26427.305711	30.982733
522.024007	26467.689296	30.987751
522.287000	26511.596718	30.992768
523.266744	26561.688052	30.997786
523.474361	26613.563303	31.002804
524.418433	26656.595273	31.007821
524.574991	26706.190276	31.012839
524.915828	26746.998379	31.017856
526.181990	26787.931783	31.022874
526.144202	26832.550571	31.027892
526.991647	26872.603894	31.032909
527.119128	26922.423215	31.037927
527.841656	26975.173274	31.042944
528.500358	27030.787299	31.047962
528.953650	27071.633461	31.052980
529.822259	27119.163986	31.057997
530.006559	27169.956698	31.063015
530.733071	27208.668687	31.068032
531.296230	27259.031031	31.073050
531.781714	27309.774630	31.078068
532.086597	27362.485331	31.083085
532.697240	27415.005680	31.088103
533.097367	27450.604545	31.093120
533.688421	27498.233975	31.098138
534.306150	27551.762130	31.103156
535.038348	27587.453371	31.108173
535.304108	27628.447419	31.113191
535.757375	27669.369156	31.118208
536.696498	27717.569374	31.123226
536.905831	27760.707936	31.128244
537.748732	27791.082612	31.133261
538.264401	27842.440785	31.138279
538.885841	27884.204543	31.143296
539.360015	27919.403421	31.148314
539.701115	27954.935583	31.153332
540.378082	27992.850531	31.158349
540.740887	28035.019888	31.163367
541.266538	28082.387263	31.168384
542.000378	28120.591281	31.173402
542.025032	28165.074573	31.178420
542.784896	28203.993221	31.183437
543.246067	28247.182784	31.188455
543.932529	28297.293919	31.193472
544.568823	28338.823259	31.198490
544.888600	28393.101330	31.203508
545.866773	28433.490695	31.208525
546.083860	28488.370083	31.213543
546.371391	28524.203559	31.218560
546.967868	28570.505249	31.223578
547.608079	28626.502760	31.228596
548.177127	28671.764303	31.233613
548.972196	28721.002170	31.238631
549.350899	28760.118392	31.243648
549.731509	28814.254228	31.248666
550.158977	28871.499907	31.253684
550.918749	28911.865367	31.258701
551.275809	28967.727926	31.263719
551.816399	29020.934396	31.268736
552.647769	29068.314261	31.273754
553.125992	29128.334251	31.278772
553.625482	29176.514280	31.283789
554.618751	29233.039161	31.288807
555.418408	29259.948553	31.293824
556.325123	29292.011591	31.298842
556.793489	29345.993382	31.303860
557.557615	29377.970562	31.308877
558.104813	29421.206276	31.313895
558.552326	29460.475544	31.318912
558.745241	29492.731469	31.323930
559.474415	29543.099676	31.328948
559.857472	29592.960547	31.333965
560.584115	29624.941031	31.338983
561.201745	29666.470433	31.344000
561.911023	29708.098814	31.349018
561.846216	29750.421101	31.354036
562.479211	29783.501089	31.359053
563.105772	29841.156585	31.364071
563.355853	29890.563595	31.369088
564.077183	29933.713045	31.374106
564.321751	29989.004441	31.379124
565.043064	30034.658433	31.384141
565.408356	30088.610241	31.389159
565.926369	30135.975353	31.394176
566.489625	30186.435013	31.399194
566.933162	30239.186532	31.404212
567.487305	30285.550272	31.409229
568.404218	30328.850859	31.414247
568.668396	30381.002562	31.419264
569.571036	30423.088966	31.424282
569.951695	30471.072672	31.429300
570.808792	30504.357987	31.434317
571.555495	30544.950225	31.439335
573.996667	30529.464383	31.444352
575.465222	30544.269268	31.449370
576.152307	30550.467259	31.454388
576.782662	30558.625451	31.459405
577.408072	30563.162647	31.464423
577.614500	30574.989667	31.469440
578.058304	30561.925965	31.474458
578.339522	30577.172160	31.479476
578.523042	30570.592851	31.484493
578.696750	30587.526804	31.489511
579.106264	30606.040261	31.494528
579.650912	30628.574827	31.499546
579.490146	30660.014670	31.504564
579.760765	30693.177861	31.509581
580.329768	30730.082485	31.514599
580.458066	30784.941179	31.519616
580.947143	30824.358411	31.524634
581.310080	30872.686553	31.529652
581.846706	30933.332733	31.534669
582.538093	30992.977305	31.539687
582.899135	31053.450153	31.544704
583.299425	31107.577844	31.549722
583.660656	31170.856575	31.554740
584.290150	31228.552743	31.559757
584.724490	31288.541944	31.564775
585.239418	31352.438379	31.569792
586.078808	31408.382184	31.574810
586.852182	31479.117811	31.579828
587.509675	31540.744684	31.584845
588.098011	31600.297541	31.589863
588.574694	31657.921832	31.594880
589.271913	31724.848442	31.599898
589.823006	31792.044481	31.604916
590.523875	31838.009383	31.609933
590.905455	31908.170898	31.614951
591.288623	31974.691445	31.619968
592.448120	32034.924091	31.624986
593.169077	32093.715220	31.630004
593.985242	32140.453861	31.635021
594.642840	32195.184087	31.640039
595.318687	32255.010669	31.645056
595.901158	32302.504170	31.650074
596.191642	32353.809929	31.655092
597.132167	32394.388485	31.660109
598.212510	32447.991417	31.665127
598.668362	32489.671955	31.670144
599.595072	32538.853064	31.675162
600.084260	32580.071409	31.680180
600.089478	32621.297580	31.685197
600.731361	32658.497566	31.690215
601.190622	32703.675825	31.695232
601.900185	32745.830466	31.700250
602.581417	32790.144493	31.705268
602.718451	32831.808890	31.710285
603.484003	32885.518547	31.715303
603.489220	32936.631950	31.720320
604.446775	32989.173287	31.725338
605.009471	33051.867559	31.730356
605.537089	33095.432906	31.735373
606.362806	33150.677043	31.740391
607.044197	33204.054351	31.745408
607.618389	33249.348206	31.750426
608.322758	33300.045577	31.755444
609.345647	33349.410823	31.760461
610.526591	33376.778575	31.765479
611.064850	33419.083593	31.770496
611.824074	33454.039324	31.775514
612.730321	33497.301098	31.780532
613.071100	33529.304936	31.785549
613.844984	33570.485139	31.790567
613.771529	33612.914868	31.795584
614.493604	33642.397516	31.800602
614.892164	33688.185567	31.805620
615.329400	33746.425589	31.810637
616.247145	33772.305265	31.815655
616.711923	33829.600101	31.820672
617.697353	33864.771319	31.825690
618.283873	33921.115445	31.830708
618.886475	33959.894690	31.835725
619.263760	34003.339761	31.840743
619.588173	34049.046032	31.845760
620.524270	34104.009360	31.850778
620.778856	34157.279574	31.855796
621.483448	34205.279299	31.860813
622.611547	34252.333657	31.865831
622.729268	34307.850466	31.870848
623.664158	34348.612856	31.875866
623.793547	34405.606816	31.880884
624.385140	34459.253114	31.885901
625.418239	34512.498223	31.890919
625.831340	34567.820672	31.895936
626.614442	34610.598924	31.900954
627.345859	34669.290331	31.905972
627.852697	34717.914197	31.910989
628.451093	34762.517837	31.916007
628.853862	34827.331511	31.921024
629.710970	34873.555845	31.926042
630.440312	34919.351359	31.931060
631.037508	34967.646269	31.936077
631.756556	35012.984923	31.941095
631.863301	35075.880827	31.946112
632.635401	35111.287299	31.951130
633.415569	35165.990468	31.956148
634.205402	35209.147546	31.961165
634.692929	35248.761595	31.966183
635.163294	35297.698800	31.971200
635.471524	35342.656043	31.976218
636.213760	35401.097635	31.981236
636.703768	35466.626670	31.986253
637.094039	35513.343323	31.991271
637.299861	35572.581951	31.996288
638.205311	35626.598226	32.001306
639.090368	35688.040307	32.006324
639.008620	35764.030511	32.011341
639.788428	35829.845894	32.016359
640.311714	35904.299407	32.021376
642.318549	35929.018934	32.026394
643.538660	35974.745496	32.031412
644.088678	36029.730934	32.036429
644.746755	36068.689134	32.041447
645.498849	36116.604811	32.046464
645.992707	36159.053135	32.051482
646.593491	36202.025312	32.056500
646.766548	36250.372547	32.061517
647.440628	36296.620506	32.066535
648.185404	36357.504039	32.071552
648.583102	36422.067703	32.076570
649.018698	36462.585257	32.081588
649.712633	36526.354830	32.086605
650.445818	36580.100478	32.091623
651.189954	36648.160416	32.096640
651.715245	36703.582420	32.101658
652.471109	36764.389982	32.106676
652.697991	36823.899274	32.111693
653.554300	36880.230907	32.116711
653.863102	36949.731504	32.121728
654.937801	37005.822238	32.126746
655.329530	37070.193830	32.131764
656.435955	37127.675278	32.136781
657.444152	37177.021091	32.141799
658.000407	37248.608890	32.146816
658.599768	37301.857844	32.151834
659.504507	37358.418295	32.156852
659.942216	37414.334324	32.161869
660.600532	37460.471318	32.166887
661.282545	37512.120025	32.171904
662.352104	37566.203131	32.176922
662.719455	37609.452583	32.181940
662.971370	37679.274280	32.186957
663.820376	37726.999368	32.191975
664.359877	37788.786393	32.196992
665.081111	37854.589068	32.202010
665.829279	37907.403129	32.207028
666.095949	37971.566286	32.212045
666.824761	38033.319329	32.217063
667.388127	38091.108131	32.222080
668.079625	38160.581151	32.227098
668.877726	38214.408395	32.232116
669.583108	38270.893273	32.237133
670.058349	38313.263264	32.242151
671.040012	38370.218515	32.247168
671.284312	38427.499507	32.252186
672.158495	38489.082845	32.257204
672.595004	38544.414650	32.262221
673.239688	38604.508595	32.267239
673.809453	38672.426277	32.272256
674.565095	38722.647813	32.277274
675.217643	38786.295327	32.282292
675.834994	38845.175582	32.287309
676.982288	38900.344910	32.292327
677.484821	38960.746584	32.297344
677.979344	39028.961506	32.302362
678.903344	39080.658465	32.307380
679.770756	39151.965081	32.312397
680.625971	39197.872044	32.317415
680.992014	39259.876542	32.322432
681.600007	39326.179178	32.327450
682.499360	39375.080408	32.332468
682.756372	39437.864553	32.337485
683.608642	39497.537534	32.342503
683.846644	39570.584524	32.347520
684.386056	39653.658753	32.352538
685.373580	39713.646838	32.357556
685.761837	39796.416253	32.362573
686.570553	39875.131047	32.367591
686.953073	39938.780135	32.372608
687.626082	40015.416695	32.377626
688.115097	40084.005722	32.382644
688.777438	40171.869462	32.387661
689.926472	40253.638434	32.392679
690.774869	40327.908243	32.397696
691.592669	40402.183247	32.402714
693.018422	40464.692032	32.407732
693.664885	40529.053517	32.412749
694.633870	40582.624502	32.417767
695.159951	40637.751715	32.422784
695.870103	40701.453981	32.427802
696.669791	40759.329336	32.432820
696.986146	40826.217264	32.437837
697.882647	40888.881261	32.442855
698.670864	40944.989642	32.447872
699.070974	41006.159222	32.452890
700.393598	41053.799322	32.457908
701.730230	41095.693711	32.462925
702.830732	41152.254553	32.467943
703.706785	41186.608479	32.472960
704.386829	41226.759420	32.477978
705.072726	41243.827611	32.482996
705.423788	41293.405153	32.488013
705.956994	41334.097003	32.493031
706.706335	41376.848893	32.498048
706.960907	41427.337963	32.503066
707.435526	41467.159446	32.508084
708.370809	41515.688900	32.513101
708.753777	41565.164367	32.518119
709.183984	41614.168788	32.523136
709.438387	41668.014655	32.528154
710.022129	41716.865602	32.533172
710.591261	41790.331424	32.538189
711.331647	41849.784400	32.543207
711.814145	41914.170881	32.548224
712.287934	41988.047007	32.553242
713.054189	42049.127307	32.558260
713.599448	42128.490557	32.563277
714.415131	42204.962781	32.568295
715.189720	42275.076478	32.573312
715.846934	42349.912252	32.578330
716.572571	42420.630503	32.583348
717.255233	42507.004646	32.588365
717.713549	42578.387512	32.593383
718.542417	42648.528784	32.598400
719.081946	42734.138254	32.603418
720.276623	42805.294417	32.608436
721.140716	42878.976575	32.613453
722.200142	42946.088799	32.618471
723.391339	43013.905828	32.623488
723.774097	43082.940125	32.628506
724.811349	43147.201873	32.633524
725.295184	43217.684290	32.638541
726.178405	43276.040606	32.643559
726.921950	43337.649574	32.648576
727.166112	43416.965731	32.653594
728.122540	43483.768370	32.658612
728.498820	43559.549992	32.663629
729.555487	43623.517046	32.668647
730.584918	43695.990245	32.673664
731.270008	43760.253554	32.678682
732.546107	43818.290474	32.683700
732.896682	43887.279467	32.688717
733.528620	43959.744496	32.693735
734.593450	44005.840741	32.698752
735.679828	44071.867848	32.703770
736.832657	44114.524433	32.708788
737.908592	44160.534148	32.713805
738.722836	44215.929771	32.718823
739.355845	44255.896510	32.723840
739.811049	44309.860586	32.728858
740.218170	44352.576538	32.733876
741.190509	44398.511892	32.738893
741.896983	44450.871671	32.743911
742.838204	44495.118156	32.748928
743.341822	44553.053379	32.753946
744.009623	44606.511320	32.758964
744.531555	44654.020711	32.763981
745.049379	44713.323366	32.768999
745.912132	44766.413202	32.774016
746.243433	44827.559931	32.779034
746.866017	44892.036127	32.784052
747.511583	44946.435624	32.789069
748.061292	45009.396931	32.794087
749.469765	45048.330298	32.799104
750.578229	45094.072305	32.804122
751.317418	45137.762637	32.809140
752.298619	45184.623025	32.814157
752.692127	45230.709515	32.819175
753.336133	45278.857384	32.824192
753.759464	45335.426160	32.829210
754.726436	45382.226247	32.834228
755.164832	45445.045949	32.839245
755.658092	45506.999009	32.844263
756.309434	45565.702802	32.849280
756.948150	45634.264781	32.854298
757.454114	45708.523893	32.859316
758.026068	45795.988906	32.864333
758.663016	45869.098373	32.869351
759.485986	45939.310656	32.874368
759.745062	46023.974514	32.879386
760.606033	46109.606199	32.884404
761.521254	46194.693312	32.889421
761.988248	46289.061755	32.894439
762.852632	46365.834794	32.899456
763.610385	46456.968091	32.904474
764.280186	46544.055265	32.909492
765.414715	46624.108735	32.914509
766.353799	46696.599321	32.919527
767.254549	46793.782041	32.924544
767.992641	46860.932112	32.929562
769.237273	46930.708927	32.934580
770.282571	47004.376524	32.939597
770.877568	47095.990230	32.944615
771.940679	47149.493973	32.949632
772.923551	47232.417187	32.954650
773.383957	47303.434111	32.959668
774.428355	47372.332694	32.964685
774.950449	47451.338916	32.969703
775.666778	47516.273655	32.974720
776.416849	47593.186989	32.979738
777.474087	47656.897371	32.984756
778.468994	47713.609992	32.989773
779.083939	47786.816121	32.994791
780.180805	47848.047124	32.999808
780.842287	47920.659510	33.004826
781.448512	47982.969324	33.009844
782.178152	48045.733015	33.014861
782.338230	48122.108343	33.019879
783.226158	48201.779106	33.024896
783.854667	48283.545686	33.029914
784.626828	48362.945306	33.034932
785.653672	48428.887875	33.039949
786.554540	48508.785150	33.044967
787.424525	48575.475830	33.049984
788.204023	48656.166174	33.055002
788.789640	48723.155113	33.060020
789.516929	48792.021357	33.065037
789.611017	48863.229066	33.070055
791.041467	48928.945164	33.075072
792.011456	48998.827518	33.080090
793.206617	49047.406000	33.085108
794.165474	49110.051773	33.090125
794.138100	49173.511111	33.095143
795.416225	49230.669469	33.100160
795.904895	49304.776056	33.105178
796.628489	49363.837570	33.110196
797.763513	49441.107873	33.115213
798.380737	49506.059368	33.120231
799.172047	49567.720473	33.125248
800.365531	49646.162566	33.130266
801.236726	49714.876941	33.135284
802.159735	49774.390890	33.140301
802.415272	49850.341893	33.145319
803.193056	49917.686578	33.150336
804.434025	49989.205360	33.155354
804.856441	50060.425546	33.160372
806.125154	50114.063314	33.165389
807.503874	50173.051633	33.170407
808.342552	50231.091026	33.175424
809.195649	50297.610976	33.180442
809.725117	50352.061397	33.185460
810.312902	50413.445402	33.190477
810.379443	50488.062747	33.195495
811.324131	50551.956073	33.200512
812.232110	50628.166289	33.205530
812.604231	50712.518946	33.210548
813.363849	50785.827997	33.215565
814.267606	50878.977351	33.220583
814.776071	50957.859297	33.225600
815.443392	51050.371818	33.230618
816.160227	51137.789621	33.235636
817.288255	51218.502352	33.240653
817.539696	51317.419523	33.245671
818.386294	51406.878805	33.250688
819.224620	51509.497068	33.255706
820.046366	51599.500934	33.260724
820.749511	51708.939838	33.265741
821.550598	51806.127930	33.270759
822.525054	51886.309488	33.275776
823.282925	52001.962002	33.280794
823.853834	52096.442530	33.285812
824.522410	52189.604543	33.290829
825.208836	52305.854251	33.295847
826.131072	52406.412795	33.300864
827.492586	52499.229404	33.305882
828.236163	52597.601840	33.310900
829.306623	52695.158988	33.315917
830.074636	52797.988298	33.320935
831.245782	52877.306564	33.325952
832.356536	52965.216552	33.330970
833.133800	53044.774992	33.335988
834.639524	53119.720186	33.341005
835.063937	53182.509446	33.346023
835.832272	53245.297840	33.351040
836.846022	53318.718778	33.356058
837.858456	53400.333966	33.361076
838.374771	53461.907018	33.366093
839.069143	53538.387639	33.371111
839.863393	53612.696910	33.376128
840.697812	53701.658169	33.381146
841.415520	53779.316565	33.386164
842.548889	53851.666398	33.391181
843.214376	53934.813237	33.396199
844.022450	54013.594551	33.401216
844.879999	54089.833731	33.406234
845.343927	54182.549316	33.411252
846.365546	54267.064542	33.416269
847.001192	54362.035820	33.421287
847.899311	54453.585230	33.426304
848.796229	54540.773015	33.431322
849.371961	54636.796902	33.436340
850.518010	54728.418710	33.441357
851.625331	54810.031436	33.446375
852.516649	54893.986348	33.451392
853.737698	54979.713665	33.456410
854.385391	55072.584447	33.461428
855.647645	55150.995360	33.466445
856.770580	55222.017058	33.471463
858.107558	55285.662663	33.476480
858.833009	55359.791143	33.481498
859.243743	55437.246612	33.486516
860.480638	55507.108575	33.491533
861.031795	55584.744345	33.496551
861.952126	55658.887213	33.501568
863.142302	55735.818995	33.506586
863.524361	55810.319619	33.511604
864.361870	55890.509085	33.516621
865.000465	55968.776536	33.521639
865.787178	56046.092662	33.526656
866.601168	56132.227936	33.531674
867.192837	56227.140128	33.536692
868.321959	56309.990379	33.541709
868.647402	56404.061949	33.546727
869.535333	56492.097013	33.551744
870.727465	56591.556062	33.556762
871.336452	56684.403277	33.561780
872.541966	56758.041139	33.566797
873.540946	56860.480901	33.571815
874.146072	56950.533065	33.576832
875.091669	57039.161379	33.581850
875.671062	57133.546672	33.586868
876.856996	57224.533745	33.591885
877.990623	57302.548135	33.596903
878.374757	57401.218306	33.601920
879.605635	57481.102694	33.606938
879.970811	57571.979008	33.611956
880.948046	57654.218601	33.616973
881.695943	57749.022203	33.621991
882.277744	57837.952179	33.627008
883.380476	57922.610242	33.632026
884.019203	58018.165035	33.637044
885.095759	58107.219620	33.642061
886.009392	58194.876700	33.647079
886.778997	58282.222459	33.652096
887.461436	58377.200702	33.657114
888.272514	58482.208223	33.662132
889.923532	58571.413561	33.667149
890.609509	58661.060211	33.672167
891.676575	58747.243170	33.677184
892.524468	58828.706624	33.682202
893.289343	58922.042245	33.687220
894.379855	59017.315586	33.692237
895.258593	59106.557992	33.697255
896.311858	59190.184651	33.702272
897.692952	59279.256380	33.707290
898.501962	59367.687077	33.712308
899.634497	59447.033581	33.717325
900.410862	59535.410278	33.722343
901.315254	59609.997773	33.727360
902.717577	59685.560890	33.732378
903.083188	59779.608444	33.737396
904.047245	59855.463010	33.742413
905.325243	59943.591312	33.747431
905.925042	60035.146414	33.752448
906.706883	60120.860137	33.757466
907.341266	60200.276485	33.762484
907.929334	60286.091264	33.767501
908.675963	60392.357518	33.772519
909.676749	60486.935885	33.777536
910.722534	60580.222457	33.782554
911.674019	60673.357149	33.787572
912.801912	60760.537504	33.792589
913.619476	60851.638825	33.797607
914.460551	60943.662018	33.802624
915.781604	61036.692340	33.807642
916.641018	61135.009805	33.812660
917.203466	61231.846745	33.817677
918.156459	61327.728422	33.822695
918.690115	61430.425243	33.827712
920.191258	61519.422220	33.832730
920.674301	61622.649158	33.837748
921.603256	61718.454548	33.842765
922.582306	61820.735271	33.847783
923.226743	61935.205019	33.852800
924.138580	62026.631741	33.857818
924.939994	62139.843062	33.862836
925.879936	62246.300585	33.867853
926.426087	62353.032943	33.872871
927.383340	62467.342450	33.877888
928.388329	62570.027301	33.882906
929.140478	62681.130776	33.887924
930.178309	62777.429463	33.892941
931.457786	62868.678594	33.897959
932.401897	62958.986784	33.902976
933.373050	63054.163794	33.907994
934.192787	63152.712803	33.913012
935.086983	63249.933602	33.918029
936.278100	63359.938545	33.923047
937.215123	63444.319474	33.928064
938.673180	63532.663287	33.933082
939.552126	63625.789332	33.938100
940.115493	63724.495786	33.943117
941.041964	63816.238292	33.948135
941.651554	63922.963052	33.953152
943.306953	64021.453068	33.958170
944.398215	64103.251160	33.963188
945.675396	64205.629937	33.968205
946.075411	64291.120139	33.973223
946.750509	64389.060612	33.978240
948.022539	64486.274971	33.983258
948.713093	64591.165158	33.988276
949.537893	64698.924317	33.993293
950.911686	64795.609270	33.998311
951.354510	64905.461106	34.003328
952.210051	65008.170245	34.008346
952.948479	65105.602141	34.013364
953.865586	65216.015103	34.018381
954.974143	65326.259271	34.023399
956.125369	65430.714386	34.028416
957.492978	65530.685533	34.033434
958.503939	65644.519145	34.038452
959.657957	65739.838356	34.043469
960.829933	65827.786653	34.048487
961.761822	65918.369763	34.053504
963.000309	66015.221361	34.058522
963.748223	66118.822126	34.063540
964.763386	66222.649394	34.068557
965.657079	66316.016734	34.073575
966.349999	66420.575410	34.078592
967.863962	66497.206024	34.083610
968.663672	66602.288796	34.088628
969.462989	66700.543449	34.093645
970.434565	66799.238658	34.098663
971.117604	66896.508387	34.103680
972.175713	67001.027891	34.108698
973.322822	67105.767535	34.113716
973.703735	67211.052905	34.118733
975.021711	67310.314695	34.123751
975.801076	67428.949417	34.128768
976.753934	67525.724527	34.133786
977.809465	67631.745051	34.138804
978.619783	67744.400541	34.143821
979.422389	67847.682823	34.148839
980.446831	67958.713492	34.153856
981.522773	68064.215093	34.158874
982.403637	68172.869172	34.163892
983.203876	68276.678463	34.168909
983.991853	68373.054426	34.173927
984.337161	68489.591412	34.178944
985.730387	68597.067067	34.183962
986.542963	68710.719660	34.188980
987.540001	68828.045773	34.193997
988.395714	68932.740531	34.199015
989.227398	69050.928238	34.204032
990.401124	69168.247234	34.209050
991.382793	69303.331864	34.214068
992.428903	69415.763629	34.219085
993.392908	69530.546758	34.224103
994.481835	69646.909142	34.229120
995.988764	69754.537338	34.234138
997.908176	69848.181749	34.239156
998.824624	69950.812588	34.244173
1000.427928	70053.157780	34.249191
1001.534968	70142.788134	34.254208
1002.822661	70227.651500	34.259226
1003.766637	70307.218369	34.264244
1004.939296	70397.237494	34.269261
1006.280203	70478.365702	34.274279
1006.672565	70575.150303	34.279296
1007.704055	70651.678167	34.284314
1008.585664	70748.335237	34.289332
1009.191980	70840.101901	34.294349
1010.216866	70939.681491	34.299367
1011.038504	71042.952312	34.304384
1011.954605	71133.243080	34.309402
1012.606045	71249.002138	34.314420
1013.524750	71355.816487	34.319437
1014.842809	71468.602148	34.324455
1015.395939	71582.748596	34.329472
1016.046684	71692.153800	34.334490
1016.931865	71821.293572	34.339508
1017.459708	71950.219324	34.344525
1018.676204	72078.752011	34.349543
1019.412102	72218.438917	34.354560
1020.781030	72354.645493	34.359578
1021.787853	72481.122585	34.364596
1022.538550	72620.727813	34.369613
1023.727610	72756.201155	34.374631
1024.620083	72884.297708	34.379648
1025.784908	73019.334359	34.384666
1027.386906	73137.196471	34.389684
1028.278435	73264.284551	34.394701
1029.438477	73392.367074	34.399719
1030.387305	73522.531457	34.404736
1031.586382	73642.944119	34.409754
1032.647484	73767.272163	34.414772
1033.733544	73887.268239	34.419789
1035.293769	73993.577600	34.424807
1036.080943	74128.252092	34.429824
1037.041260	74241.710706	34.434842
1038.955297	74320.886554	34.439860
1040.129963	74418.285804	34.444877
1041.743487	74501.605235	34.449895
1042.630047	74589.274781	34.454912
1043.384644	74667.385161	34.459930
1044.088581	74770.814081	34.464948
1044.768577	74866.512051	34.469965
1045.924111	74969.427776	34.474983
1046.828602	75071.505516	34.480000
1047.405107	75187.040194	34.485018
1048.280043	75293.623443	34.490036
1049.114038	75405.219084	34.495053
1050.264807	75518.515560	34.500071
1051.299004	75636.122439	34.505088
1052.004117	75750.236854	34.510106
1053.127552	75879.573432	34.515124
1053.863472	76007.158628	34.520141
1055.087825	76121.856144	34.525159
1056.197036	76257.909315	34.530176
1056.874463	76390.461194	34.535194
1058.697399	76510.791754	34.540212
1059.726176	76640.438968	34.545229
1060.602010	76766.875359	34.550247
1061.744022	76889.882508	34.555264
1062.744986	77013.974656	34.560282
1064.461133	77134.427022	34.565300
1065.009775	77270.614056	34.570317
1066.397143	77383.371350	34.575335
1067.337004	77510.206676	34.580352
1068.813022	77627.558865	34.585370
1070.484344	77735.456690	34.590388
1071.501819	77857.579324	34.595405
1072.194434	77973.452676	34.600423
1073.259460	78099.190916	34.605440
1074.397156	78211.556368	34.610458
1075.256050	78332.822158	34.615476
1076.430784	78459.158269	34.620493
1077.828042	78576.345125	34.625511
1078.847716	78695.229813	34.630528
1079.623890	78819.109508	34.635546
1080.877163	78922.617527	34.640564
1082.186935	79026.723894	34.645581
1083.154700	79146.807791	34.650599
1084.451850	79263.875429	34.655616
1085.631014	79387.972574	34.660634
1087.023653	79493.092134	34.665652
1088.065270	79596.826843	34.670669
1089.202354	79702.885724	34.675687
1090.085462	79818.625388	34.680704
1091.401915	79931.976877	34.685722
1092.389630	80038.067557	34.690740
1093.017630	80158.394697	34.695757
1094.340493	80269.521914	34.700775
1095.164383	80391.949546	34.705792
1096.199765	80503.996098	34.710810
1097.169268	80615.415266	34.715828
1097.941573	80724.255623	34.720845
1099.039218	80834.397609	34.725863
1100.323273	80943.650800	34.730880
1101.221345	81061.645494	34.735898
1102.459283	81174.453644	34.740916
1103.500610	81282.546113	34.745933
1104.307506	81406.012850	34.750951
1105.516738	81517.088956	34.755968
1106.621869	81638.315995	34.760986
1108.086390	81755.187755	34.766004
1108.520192	81886.467198	34.771021
1109.776642	81999.864801	34.776039
1110.822404	82130.479476	34.781056
1111.466276	82262.258904	34.786074
1113.003331	82392.733857	34.791092
1113.566987	82531.336519	34.796109
1114.753713	82663.006839	34.801127
1115.840945	82797.216331	34.806144
1116.781181	82935.230707	34.811162
1117.786943	83076.927728	34.816180
1118.671728	83236.960476	34.821197
1120.337495	83370.405135	34.826215
1121.663740	83508.482000	34.831232
1122.800455	83655.883795	34.836250
1123.803950	83796.131868	34.841268
1124.800116	83935.092258	34.846285
1126.012752	84085.974974	34.851303
1127.224986	84231.282347	34.856320
1128.336962	84380.893376	34.861338
1129.680344	84519.808707	34.866356
1130.882550	84659.898127	34.871373
1132.055439	84801.624394	34.876391
1133.272604	84943.894646	34.881408
1134.414513	85087.935555	34.886426
1135.921063	85223.503753	34.891444
1137.036324	85357.092756	34.896461
1138.175014	85492.417673	34.901479
1139.646741	85626.229882	34.906496
1140.684177	85760.548285	34.911514
1142.106678	85885.245870	34.916532
1143.338903	86020.356924	34.921549
1144.240528	86155.167316	34.926567
1145.640249	86277.221429	34.931584
1146.531219	86412.073072	34.936602
1147.711432	86545.412577	34.941620
1148.680105	86680.424279	34.946637
1150.029589	86817.254291	34.951655
1150.976092	86946.801535	34.956672
1151.805885	87098.101598	34.961690
1153.200920	87226.143787	34.966708
1154.343976	87368.732842	34.971725
1155.326880	87515.762121	34.976743
1156.582746	87639.453032	34.981760
1157.753627	87781.496570	34.986778
1158.803517	87905.247056	34.991796
1159.895349	88036.807628	34.996813
1161.241451	88146.688868	35.001831
1162.649367	88267.785458	35.006848
1163.448704	88389.042743	35.011866
1164.761705	88522.455583	35.016884
1166.018617	88642.844724	35.021901
1167.247597	88769.588149	35.026919
1167.904996	88895.620073	35.031936
1169.019105	89032.640693	35.036954
1170.252243	89165.538977	35.041972
1171.211985	89308.150996	35.046989
1172.107391	89440.295189	35.052007
1173.177241	89576.801377	35.057024
1174.018761	89729.186735	35.062042
1175.329769	89875.098408	35.067060
1176.637757	90033.672671	35.072077
1177.640622	90179.281220	35.077095
1178.953372	90336.263201	35.082112
1179.976825	90491.660622	35.087130
1181.369408	90653.065569	35.092148
1182.816398	90805.279924	35.097165
1184.316776	90934.339151	35.102183
1185.954103	91084.279979	35.107200
1186.964998	91223.424177	35.112218
1188.394553	91356.854791	35.117236
1189.699316	91505.637049	35.122253
1190.567972	91654.938713	35.127271
1191.922166	91778.504671	35.132288
1193.118081	91932.158197	35.137306
1194.135142	92080.667519	35.142324
1195.515303	92217.077543	35.147341
1196.253744	92367.638080	35.152359
1197.738533	92509.390473	35.157376
1198.300224	92667.748200	35.162394
1199.813196	92817.726911	35.167412
1200.898955	92972.701810	35.172429
1201.776179	93133.352965	35.177447
1202.895162	93288.906698	35.182464
1203.954298	93457.576894	35.187482
1205.712128	93615.245154	35.192500
1206.998463	93761.199121	35.197517
1208.383401	93933.413890	35.202535
1209.629018	94080.280945	35.207552
1210.691521	94238.975034	35.212570
1211.970956	94387.394789	35.217588
1213.312755	94543.130576	35.222605
1214.223775	94697.405152	35.227623
1215.738854	94854.418618	35.232640
1216.709538	95018.250251	35.237658
1218.107431	95178.453775	35.242676
1219.409057	95329.368564	35.247693
1220.734824	95487.175644	35.252711
1222.034685	95634.600921	35.257728
1223.063050	95781.874228	35.262746
1224.869017	95916.676665	35.267764
1226.298836	96041.683882	35.272781
1227.684476	96167.856471	35.277799
1229.246441	96276.428047	35.282816
1230.511285	96400.071754	35.287834
1231.793997	96507.214870	35.292852
1233.312664	96628.080275	35.297869
1234.155997	96742.986924	35.302887
1235.589492	96857.616863	35.307904
1236.766685	96990.007858	35.312922
1238.003288	97099.444870	35.317940
1239.056804	97223.715013	35.322957
1240.079859	97358.144417	35.327975
1240.800977	97478.268123	35.332992
1241.922250	97627.797161	35.338010
1243.098001	97756.877818	35.343028
1244.090587	97902.139796	35.348045
1245.133106	98051.842295	35.353063
1246.743899	98199.127254	35.358080
1247.395012	98349.640464	35.363098
1248.753263	98495.316241	35.368116
1250.316567	98649.438086	35.373133
1251.041362	98815.613820	35.378151
1252.294554	98969.666912	35.383168
1253.664481	99127.536523	35.388186
1254.836230	99281.478118	35.393204
1255.949218	99447.482815	35.398221
1257.187245	99607.205158	35.403239
1258.491427	99769.777885	35.408256
1259.260389	99951.690001	35.413274
1260.911319	100111.084449	35.418292
1263.029530	100257.289592	35.423309
1264.582986	100424.123404	35.428327
1266.322425	100564.386233	35.433344
1268.127144	100697.673246	35.438362
1269.978543	100831.054842	35.443380
1271.139213	100962.901918	35.448397
1272.202840	101094.638623	35.453415
1273.521456	101220.678859	35.458432
1274.140638	101370.128517	35.463450
1275.461983	101503.863994	35.468468
1276.837455	101643.786249	35.473485
1277.479857	101797.202288	35.478503
1278.957951	101946.228019	35.483520
1280.188851	102105.924395	35.488538
1280.944641	102258.958433	35.493556
1282.328153	102412.254356	35.498573
1283.635219	102573.346558	35.503591
1284.969100	102723.640402	35.508608
1286.066625	102891.140175	35.513626
1287.395393	103044.252766	35.518644
1289.262930	103191.496995	35.523661
1290.703684	103348.251294	35.528679
1291.878241	103494.753310	35.533696
1293.095333	103642.034150	35.538714
1294.490027	103782.940622	35.543732
1295.444193	103912.533707	35.548749
1296.359393	104057.080759	35.553767
1297.876398	104189.724646	35.558784
1298.833131	104344.037554	35.563802
1299.976507	104491.322742	35.568820
1301.522225	104635.804733	35.573837
1302.292287	104793.510561	35.578855
1303.437290	104948.316389	35.583872
1304.736081	105110.490371	35.588890
1305.674621	105277.545015	35.593908
1306.889481	105433.387086	35.598925
1308.003334	105609.371022	35.603943
1309.472344	105773.958948	35.608960
1310.500743	105963.306086	35.613978
1311.921439	106135.302366	35.618996
1313.582796	106308.533700	35.624013
1314.949793	106490.515157	35.629031
1316.052485	106658.679865	35.634048
1317.685743	106832.330819	35.639066
1319.396633	107003.926444	35.644084
1321.299711	107165.752468	35.649101
1322.641665	107325.554886	35.654119
1324.334592	107493.410082	35.659136
1325.683260	107644.954140	35.664154
1326.693211	107814.015059	35.669172
1327.987612	107965.822917	35.674189
1329.098349	108142.477772	35.679207
1330.612235	108298.468084	35.684224
1332.024245	108469.691232	35.689242
1333.410149	108633.280215	35.694260
1334.852718	108799.874079	35.699277
1335.815284	108970.026569	35.704295
1337.407061	109133.617835	35.709312
1338.698366	109294.637538	35.714330
1340.062123	109474.502548	35.719348
1341.557204	109639.308858	35.724365
1342.754655	109800.948125	35.729383
1344.101941	109967.318239	35.734400
1345.383494	110146.327750	35.739418
1346.815218	110314.035025	35.744436
1347.785709	110476.056619	35.749453
1349.291545	110663.231362	35.754471
1350.599545	110832.075889	35.759488
1351.736985	111015.191087	35.764506
1353.425770	111178.742585	35.769524
1355.326240	111336.608794	35.774541
1356.536504	111513.215153	35.779559
1357.944684	111683.239628	35.784576
1359.836624	111853.511218	35.789594
1361.039535	112013.986705	35.794612
1362.626322	112167.609853	35.799629
1363.778764	112338.730286	35.804647
1364.757400	112505.397638	35.809664
1366.072727	112654.072297	35.814682
1367.037621	112821.706164	35.819700
1368.488487	112981.920581	35.824717
1369.713602	113133.119292	35.829735
1370.705120	113295.877621	35.834752
1372.152432	113463.407459	35.839770
1373.096500	113639.678694	35.844788
1374.169870	113796.533451	35.849805
1375.252600	113982.097457	35.854823
1376.288803	114158.009492	35.859840
1378.030749	114340.331311	35.864858
1379.647880	114529.720520	35.869876
1381.417451	114703.816806	35.874893
1382.912942	114884.301451	35.879911
1384.023769	115063.462034	35.884928
1385.433986	115247.039675	35.889946
1386.287918	115446.313156	35.894964
1388.139153	115629.196692	35.899981
1389.428543	115825.630907	35.904999
1390.534167	116010.902247	35.910016
1392.165269	116206.721613	35.915034
1393.303018	116404.887500	35.920052
1395.143126	116594.845485	35.925069
1396.657498	116796.702719	35.930087
1397.929746	116980.093167	35.935104
1399.535044	117171.650287	35.940122
1400.831309	117374.015258	35.945140
1402.136256	117560.139883	35.950157
1403.654377	117761.421596	35.955175
1405.016376	117958.734390	35.960192
1406.461223	118154.237311	35.965210
1407.629155	118359.093455	35.970228
1409.215357	118559.889354	35.975245
1410.883716	118767.391892	35.980263
1412.082596	118965.827372	35.985280
1413.740033	119162.589500	35.990298
1415.040469	119368.192389	35.995316
1416.363402	119561.490076	36.000333
1417.279777	119770.316882	36.005351
1419.464581	119971.915050	36.010368
1421.169994	120167.625993	36.015386
1422.807872	120353.179490	36.020404
1424.494222	120544.273714	36.025421
1425.706414	120733.317004	36.030439
1427.588178	120918.088519	36.035456
1429.137020	121121.177059	36.040474
1430.460557	121305.710717	36.045492
1432.159106	121486.563852	36.050509
1433.484776	121670.403140	36.055527
1434.557720	121866.024583	36.060544
1436.217716	122041.340246	36.065562
1437.102436	122250.495722	36.070580
1438.736226	122432.619493	36.075597
1440.183367	122627.123175	36.080615
1441.365673	122829.358468	36.085632
1442.966151	123005.462560	36.090650
1444.276392	123199.802189	36.095668
1445.827078	123367.468416	36.100685
1446.950899	123555.811242	36.105703
1448.229478	123741.610231	36.110720
1450.079056	123911.626278	36.115738
1451.168710	124088.375987	36.120756
1452.605485	124272.696884	36.125773
1454.240035	124456.468291	36.130791
1455.394665	124639.291218	36.135808
1456.891097	124834.031087	36.140826
1457.954316	125031.032552	36.145844
1459.743129	125209.388525	36.150861
1461.229396	125413.393660	36.155879
1462.147166	125610.701124	36.160896
1464.080084	125795.916268	36.165914
1465.111253	126011.727983	36.170932
1466.660553	126210.497517	36.175949
1468.110182	126406.092148	36.180967
1469.891933	126618.381860	36.185984
1471.358927	126810.733745	36.191002
1472.972019	127021.799295	36.196020
1474.461427	127229.997864	36.201037
1475.913690	127424.851955	36.206055
1477.729351	127635.066620	36.211072
1479.540774	127826.864179	36.216090
1481.382632	128016.745345	36.221108
1482.596475	128220.954051	36.226125
1484.181805	128421.444086	36.231143
1485.585844	128608.687859	36.236160
1487.088092	128810.106035	36.241178
1488.522521	129020.391813	36.246196
1490.021925	129204.406623	36.251213
1490.991802	129421.382306	36.256231
1492.585903	129624.299370	36.261248
1493.960423	129837.134609	36.266266
1495.187651	130042.406088	36.271284
1496.759958	130256.036577	36.276301
1498.680043	130475.821383	36.281319
1500.121127	130689.919450	36.286336
1501.754384	130895.272019	36.291354
1503.034757	131104.115602	36.296372
1504.471032	131318.738664	36.301389
1506.076971	131526.380705	36.306407
1507.604347	131739.877551	36.311424
1509.413730	131952.228916	36.316442
1510.675692	132164.212723	36.321460
1512.493159	132379.936232	36.326477
1513.801539	132589.445158	36.331495
1515.340989	132801.592347	36.336512
1517.040901	133018.238957	36.341530
1518.802863	133207.471053	36.346548
1521.273869	133397.440680	36.351565
1523.088804	133581.775992	36.356583
1524.386675	133785.606222	36.361600
1526.532411	133954.686477	36.366618
1528.045669	134120.282345	36.371636
1529.190734	134288.813972	36.376653
1530.489014	134438.619784	36.381671
1532.080971	134614.456859	36.386688
1533.514997	134777.636235	36.391706
1534.652535	134946.451659	36.396724
1535.726422	135135.197521	36.401741
1537.062594	135310.445891	36.406759
1538.207431	135509.940953	36.411776
1539.437886	135696.080594	36.416794
1540.907638	135906.056839	36.421812
1541.980560	136122.484208	36.426829
1543.429895	136323.621801	36.431847
1544.708569	136556.873270	36.436864
1546.067316	136762.780252	36.441882
1547.230145	137002.972605	36.446900
1548.673787	137237.723926	36.451917
1550.265433	137454.839038	36.456935
1551.857764	137709.529439	36.461952
1553.588539	137932.455287	36.466970
1555.088276	138180.650760	36.471988
1556.749243	138415.452935	36.477005
1558.544368	138653.619303	36.482023
1560.126028	138894.153311	36.487040
1561.833490	139132.045949	36.492058
1563.366791	139369.993493	36.497076
1564.802535	139616.386143	36.502093
1566.436079	139849.378995	36.507111
1568.092156	140095.563147	36.512128
1569.894275	140328.989178	36.517146
1571.590771	140568.770625	36.522164
1573.098567	140815.681259	36.527181
1574.904352	141053.624167	36.532199
1576.670295	141289.737545	36.537216
1578.345775	141509.226089	36.542234
1580.368511	141744.706529	36.547252
1581.989831	141978.490832	36.552269
1584.709207	142190.505420	36.557287
1586.565895	142408.843639	36.562304
1588.328088	142619.771157	36.567322
1590.133079	142810.084430	36.572340
1591.358517	143017.082093	36.577357
1592.899755	143226.147669	36.582375
1594.554112	143432.534976	36.587392
1596.266535	143639.991809	36.592410
1597.393895	143843.182761	36.597428
1599.083191	144053.371167	36.602445
1601.162325	144253.713830	36.607463
1602.660586	144456.494977	36.612480
1604.084496	144666.755037	36.617498
1605.706420	144867.731994	36.622516
1607.252113	145075.300947	36.627533
1609.061286	145271.522791	36.632551
1610.599780	145472.009861	36.637568
1612.342509	145669.993998	36.642586
1613.745195	145860.288459	36.647604
1614.927773	146044.813465	36.652621
1616.695195	146223.529789	36.657639
1618.034475	146423.433441	36.662656
1619.618460	146604.348664	36.667674
1621.568902	146793.496956	36.672692
1623.121803	146987.957502	36.677709
1625.052612	147175.805538	36.682727
1626.179200	147369.993873	36.687744
1627.865849	147565.488854	36.692762
1629.023714	147765.252297	36.697780
1629.992523	147970.675460	36.702797
1631.599344	148188.827486	36.707815
1632.931436	148406.720387	36.712832
1634.507413	148631.814560	36.717850
1636.117094	148866.894453	36.722868
1637.014430	149099.756609	36.727885
1638.677236	149339.699522	36.732903
1640.271081	149583.914744	36.737920
1641.462863	149831.479110	36.742938
1643.397281	150089.639904	36.747956
1644.696031	150356.385025	36.752973
1646.519722	150604.298619	36.757991
1648.035994	150862.214995	36.763008
1649.726847	151139.604299	36.768026
1651.666676	151397.863310	36.773044
1653.265884	151657.256085	36.778061
1655.031650	151922.139470	36.783079
1656.390063	152187.115030	36.788096
1658.028852	152450.780338	36.793114
1660.600862	152706.717777	36.798132
1662.334051	152970.055252	36.803149
1664.714209	153202.926553	36.808167
1666.511440	153460.869285	36.813184
1667.983366	153701.039142	36.818202
1669.993564	153950.900730	36.823220
1671.434694	154199.180914	36.828237
1673.454051	154444.594360	36.833255
1674.876034	154698.903870	36.838272
1676.931574	154924.459334	36.843290
1679.214234	155151.007267	36.848308
1680.949556	155394.076297	36.853325
1683.030600	155619.759130	36.858343
1684.274906	155847.579732	36.863360
1685.725702	156088.949105	36.868378
1687.743257	156316.269640	36.873396
1688.880459	156560.684586	36.878413
1691.027767	156788.951325	36.883431
1692.401567	157034.980473	36.888448
1693.993493	157262.628461	36.893466
1695.489755	157507.551031	36.898484
1697.438659	157743.818826	36.903501
1699.253701	157982.987956	36.908519
1701.035565	158214.530302	36.913536
1702.719469	158445.024568	36.918554
1704.742928	158651.360378	36.923572
1706.272088	158862.214178	36.928589
1708.165055	159074.469777	36.933607
1709.917824	159283.629410	36.938624
1712.247921	159470.367335	36.943642
1714.371281	159657.024952	36.948660
1716.027193	159853.572998	36.953677
1717.804506	160051.878231	36.958695
1719.465575	160258.750230	36.963712
1720.728601	160450.684582	36.968730
1722.295080	160655.139089	36.973748
1723.724386	160866.210940	36.978765
1725.140302	161075.789739	36.983783
1726.478812	161299.243120	36.988800
1728.173593	161525.000128	36.993818
1729.525522	161756.836866	36.998836
1730.817351	161998.132668	37.003853
1732.300484	162248.061515	37.008871
1733.641898	162493.410996	37.013888
1734.983431	162746.079736	37.018906
1736.780626	163014.999962	37.023924
1738.570038	163273.320957	37.028941
1740.413726	163535.439902	37.033959
1742.193542	163815.237654	37.038976
1743.617584	164077.642720	37.043994
1745.308302	164342.949711	37.049012
1747.252865	164618.148959	37.054029
1748.919069	164888.270560	37.059047
1750.692864	165166.164419	37.064064
1752.334715	165448.330151	37.069082
1754.077437	165739.728066	37.074100
1755.954899	166010.864314	37.079117
1758.162994	166293.377770	37.084135
1760.592557	166552.013239	37.089152
1762.912124	166815.335511	37.094170
1765.696133	167052.508292	37.099188
1767.559468	167306.672742	37.104205
1769.865786	167544.140083	37.109223
1771.971710	167790.481407	37.114240
1773.001192	168029.194590	37.119258
1774.995871	168252.814207	37.124276
1776.507604	168507.613303	37.129293
1778.520760	168731.372317	37.134311
1780.191837	168976.686817	37.139328
1781.607907	169213.215048	37.144346
1783.812481	169460.616962	37.149364
1784.807651	169712.829644	37.154381
1786.324061	169954.496407	37.159399
1787.992759	170214.178133	37.164416
1789.576255	170487.663480	37.169434
1791.787433	170730.886473	37.174452
1793.624029	170986.271889	37.179469
1795.766328	171227.986718	37.184487
1797.737963	171480.842284	37.189504
1799.071463	171727.458192	37.194522
1801.065213	171946.887789	37.199540
1802.836539	172172.950287	37.204557
1804.264333	172408.328958	37.209575
1805.929772	172650.255060	37.214592
1807.445535	172882.083320	37.219610
1808.793764	173134.604418	37.224628
1810.643973	173388.455532	37.229645
1811.998834	173639.088585	37.234663
1813.532149	173909.281862	37.239680
1815.016042	174168.346521	37.244698
1816.488438	174444.857976	37.249716
1818.333039	174727.338142	37.254733
1819.497615	175015.763888	37.259751
1822.097295	175291.569324	37.264768
1823.926995	175578.675573	37.269786
1825.852621	175870.132757	37.274804
1827.683119	176163.598902	37.279821
1829.649290	176442.976083	37.284839
1831.223038	176732.072066	37.289856
1833.056572	177029.793937	37.294874
1835.298783	177329.444912	37.299892
1837.064101	177616.499406	37.304909
1838.742280	177919.631584	37.309927
1840.871547	178207.850316	37.314944
1842.821380	178502.328964	37.319962
1844.869854	178801.437586	37.324980
1846.733878	179097.557983	37.329997
1848.669696	179399.695635	37.335015
1850.705160	179683.118023	37.340032
1852.257768	179989.076216	37.345050
1854.302096	180284.732152	37.350068
1856.038705	180583.902764	37.355085
1857.986871	180896.871781	37.360103
1859.942021	181188.081884	37.365120
1861.742286	181518.791430	37.370138
1863.534594	181797.977692	37.375156
1865.117608	182113.639886	37.380173
1867.110053	182422.742878	37.385191
1869.027787	182729.702848	37.390208
1870.949026	183047.614670	37.395226
1873.002376	183349.418520	37.400244
1874.717203	183663.294438	37.405261
1876.484200	183968.028285	37.410279
1878.498485	184283.003017	37.415296
1880.195258	184590.670701	37.420314
1882.374731	184903.732886	37.425332
1884.217498	185214.858471	37.430349
1886.448439	185529.274555	37.435367
1888.417760	185837.770312	37.440384
1889.764289	186156.036393	37.445402
1892.015577	186452.258864	37.450420
1893.552415	186779.825890	37.455437
1895.228794	187090.647995	37.460455
1897.447403	187402.223648	37.465472
1899.007691	187711.215612	37.470490
1901.092599	188010.228152	37.475508
1902.688616	188306.338025	37.480525
1904.500895	188597.999261	37.485543
1906.811668	188898.720151	37.490560
1908.085248	189211.168449	37.495578
1910.642119	189500.382045	37.500596
1912.205885	189790.643347	37.505613
1913.857292	190089.788576	37.510631
1916.298295	190388.137745	37.515648
1918.449427	190696.458904	37.520666
1920.593431	190992.549236	37.525684
1922.206081	191292.558346	37.530701
1924.589841	191579.920959	37.535719
1927.123342	191860.751006	37.540736
1928.938666	192167.700686	37.545754
1931.216490	192434.170199	37.550772
1933.413132	192730.097699	37.555789
1935.733716	192993.060656	37.560807
1938.320255	193259.396776	37.565824
1940.632591	193527.503873	37.570842
1942.889747	193786.914789	37.575860
1944.637080	194043.082762	37.580877
1946.435841	194303.749407	37.585895
1948.674701	194551.719312	37.590912
1950.341519	194822.029873	37.595930
1952.165029	195075.284565	37.600948
1954.413251	195339.185073	37.605965
1955.969142	195605.417903	37.610983
1957.936861	195864.999596	37.616000
1959.876423	196154.806934	37.621018
1961.504390	196413.683775	37.626036
1963.281572	196698.684210	37.631053
1964.833979	196980.358414	37.636071
1967.025522	197261.196552	37.641088
1968.584016	197547.454781	37.646106
1970.144958	197836.278060	37.651124
1972.014961	198141.262287	37.656141
1973.892152	198434.151032	37.661159
1975.850751	198736.078374	37.666176
1977.589851	199045.391376	37.671194
1979.684517	199359.117621	37.676212
1981.340446	199680.289907	37.681229
1983.372009	199986.718674	37.686247
1985.643595	200306.603825	37.691264
1987.371897	200605.024080	37.696282
1989.297526	200939.133384	37.701300
1991.374831	201237.019344	37.706317
1993.340161	201567.889359	37.711335
1995.617337	201878.960855	37.716352
1997.345275	202211.243250	37.721370
2000.037030	202520.513517	37.726388
2002.364606	202830.960313	37.731405
2004.016612	203147.317043	37.736423
2006.166360	203445.088997	37.741440
2007.891387	203755.788780	37.746458
2009.600270	204052.897606	37.751476
2011.719760	204348.584557	37.756493
2013.797982	204636.917015	37.761511
2015.650428	204918.952363	37.766528
2017.972413	205210.841425	37.771546
2019.767310	205493.993076	37.776564
2022.004707	205793.641953	37.781581
2023.259183	206103.870389	37.786599
2025.532309	206390.073276	37.791616
2027.384147	206692.034785	37.796634
2029.706620	206994.760987	37.801652
2032.096652	207293.237991	37.806669
2033.554292	207616.187439	37.811687
2035.949102	207911.911991	37.816704
2037.567853	208227.526945	37.821722
2039.606479	208540.918779	37.826740
2041.775409	208863.660411	37.831757
2043.058521	209187.039377	37.836775
2045.120100	209508.265303	37.841792
2047.274854	209852.011995	37.846810
2049.341509	210179.397712	37.851828
2051.821260	210505.538928	37.856845
2053.461571	210844.408794	37.861863
2055.545213	211183.070476	37.866880
2057.135594	211522.091506	37.871898
2059.356056	211854.057194	37.876916
2061.831487	212208.290338	37.881933
2063.836378	212555.300039	37.886951
2066.874692	212884.513226	37.891968
2068.854335	213213.058096	37.896986
2070.728683	213561.883926	37.902004
2073.095815	213880.023482	37.907021
2075.403389	214224.124636	37.912039
2077.475933	214555.809991	37.917056
2079.472542	214887.026566	37.922074
2081.311619	215213.953040	37.927092
2083.710127	215563.582106	37.932109
2085.787460	215900.097817	37.937127
2088.154895	216228.214925	37.942144
2090.494750	216561.949784	37.947162
2092.345271	216898.658664	37.952180
2094.747292	217210.802701	37.957197
2096.593485	217559.792993	37.962215
2098.608937	217882.933101	37.967232
2100.729431	218228.797857	37.972250
2102.776838	218556.113151	37.977268
2105.360781	218886.607904	37.982285
2107.060583	219225.827521	37.987303
2109.319953	219569.581638	37.992320
2111.804750	219905.531017	37.997338
2113.543428	220237.854634	38.002356
2115.802217	220619.539905	38.007373
2117.707042	220963.928071	38.012391
2119.866305	221288.431621	38.017408
2121.683983	221628.722712	38.022426
2123.636397	221936.145843	38.027444
2125.563574	222250.608574	38.032461
2127.228898	222581.887477	38.037479
2129.387829	222903.401275	38.042496
2131.309890	223231.378937	38.047514
2133.256096	223565.944201	38.052532
2135.262851	223895.066658	38.057549
2137.050170	224232.339129	38.062567
2139.131829	224576.194570	38.067584
2141.042639	224939.582458	38.072602
2142.641226	225299.808916	38.077620
2144.724469	225654.538046	38.082637
2146.939578	226028.294797	38.087655
2149.126224	226390.858035	38.092672
2151.586282	226770.521938	38.097690
2153.561643	227144.550236	38.102708
2155.945034	227504.242634	38.107725
2158.488132	227877.066629	38.112743
2161.378527	228228.859480	38.117760
2163.729544	228585.945638	38.122778
2166.295562	228950.542017	38.127796
2169.210206	229290.246344	38.132813
2171.814549	229635.080593	38.137831
2174.361632	229965.474250	38.142848
2176.779110	230300.384981	38.147866
2178.709657	230634.155093	38.152884
2180.866386	230966.011128	38.157901
2182.998805	231300.996101	38.162919
2184.972942	231640.147189	38.167936
2187.071906	231981.540095	38.172954
2188.412166	232333.340670	38.177972
2190.778687	232683.354304	38.182989
2192.451913	233052.197486	38.188007
2194.552578	233406.217975	38.193024
2196.667772	233772.047591	38.198042
2198.352125	234157.300376	38.203060
2200.746754	234528.803062	38.208077
2203.116022	234910.038751	38.213095
2205.357965	235287.283080	38.218112
2207.680591	235662.407905	38.223130
2209.374491	236049.698198	38.228148
2211.853480	236420.660946	38.233165
2213.878503	236816.638737	38.238183
2215.954990	237204.736128	38.243200
2218.544446	237588.638901	38.248218
2220.399852	237984.749452	38.253236
2222.519924	238378.279517	38.258253
2224.688783	238778.000679	38.263271
2226.726708	239183.535097	38.268288
2229.172185	239572.039410	38.273306
2231.706053	239974.297622	38.278324
2234.291862	240367.989269	38.283341
2236.479794	240767.282481	38.288359
2238.790209	241144.307285	38.293376
2241.542673	241519.027965	38.298394
2243.517935	241883.586017	38.303412
2246.154800	242232.825551	38.308429
2248.018945	242583.204603	38.313447
2250.351427	242938.387210	38.318464
2252.616414	243298.940977	38.323482
2254.365480	243658.688545	38.328500
2256.848419	244021.927598	38.333517
2259.176492	244382.169541	38.338535
2261.248739	244755.991546	38.343552
2263.296564	245124.331905	38.348570
2265.441371	245497.179207	38.353588
2267.357152	245881.138583	38.358605
2269.352369	246259.904626	38.363623
2271.649420	246639.360441	38.368640
2273.965542	247020.643100	38.373658
2276.490539	247420.868245	38.378676
2279.012461	247797.675087	38.383693
2281.409283	248191.419918	38.388711
2283.639915	248583.007602	38.393728
2286.318491	248965.456966	38.398746
2288.352581	249360.887960	38.403764
2290.453148	249748.257122	38.408781
2293.176057	250140.100807	38.413799
2295.607594	250532.982281	38.418816
2297.767378	250934.696734	38.423834
2299.948880	251336.103866	38.428852
2302.628529	251724.351035	38.433869
2304.736220	252118.201936	38.438887
2307.291774	252525.039258	38.443904
2310.066153	252907.050504	38.448922
2312.251109	253314.202343	38.453940
2314.681923	253701.248465	38.458957
2316.711133	254095.420816	38.463975
2318.955401	254495.503960	38.468992
2321.307451	254893.818062	38.474010
2323.587807	255301.314514	38.479028
2326.245323	255698.845073	38.484045
2328.412743	256109.231447	38.489063
2330.451726	256511.484791	38.494080
2333.141952	256899.740487	38.499098
2335.586185	257316.537415	38.504116
2338.260091	257710.283999	38.509133
2340.526829	258109.481127	38.514151
2343.138052	258500.089022	38.519168
2345.547823	258896.165630	38.524186
2347.567831	259301.322589	38.529204
2349.987114	259700.650458	38.534221
2352.506070	260095.517637	38.539239
2354.910882	260502.520602	38.544256
2357.176704	260898.572165	38.549274
2359.288845	261305.292421	38.554292
2361.473022	261712.484460	38.559309
2363.728463	262118.192364	38.564327
2366.183818	262528.467024	38.569344
2368.371361	262923.238021	38.574362
2370.720821	263327.560739	38.579380
2373.046675	263701.353209	38.584397
2375.344000	264086.505752	38.589415
2377.517287	264460.551795	38.594432
2379.983243	264834.526397	38.599450
2381.919959	265229.644434	38.604468
2384.040912	265617.417523	38.609485
2386.803237	266010.296935	38.614503
2389.140751	266409.467805	38.619520
2391.677197	266804.111099	38.624538
2393.476337	267216.349003	38.629556
2395.656936	267618.009807	38.634573
2398.474481	268023.431229	38.639591
2400.874762	268444.948546	38.644608
2403.102140	268857.348356	38.649626
2405.690327	269274.238418	38.654644
2407.824155	269693.868086	38.659661
2410.241301	270119.549872	38.664679
2412.671093	270547.439954	38.669696
2414.971729	270974.436179	38.674714
2417.326913	271417.809112	38.679732
2419.735667	271852.739791	38.684749
2422.390267	272288.546163	38.689767
2424.694539	272727.227958	38.694784
2427.094311	273164.091073	38.699802
2429.702040	273601.632601	38.704820
2431.851356	274046.054959	38.709837
2434.647959	274494.490114	38.714855
2438.000835	274922.031721	38.719872
2440.821445	275351.842380	38.724890
2443.303511	275775.381223	38.729908
2445.744526	276215.464151	38.734925
2448.494163	276646.581504	38.739943
2450.493268	277077.919340	38.744960
2453.227143	277508.022869	38.749978
2455.587159	277940.827482	38.754996
2458.148199	278375.479942	38.760013
2460.783614	278808.418425	38.765031
2462.846983	279250.465578	38.770048
2465.555098	279680.546974	38.775066
2467.475183	280125.537778	38.780084
2469.529700	280573.657030	38.785101
2472.406515	281017.784377	38.790119
2474.566639	281480.213755	38.795136
2476.999228	281929.643941	38.800154
2479.296993	282387.300388	38.805172
2481.436789	282852.526236	38.810189
2484.323580	283313.924410	38.815207
2486.217564	283795.802010	38.820224
2488.552682	284254.162094	38.825242
2490.935623	284730.372499	38.830260
2493.651647	285210.213015	38.835277
2496.253854	285683.364577	38.840295
2498.870044	286162.991097	38.845312
2501.597325	286613.512961	38.850330
2504.358795	287061.209093	38.855348
2506.660820	287488.147042	38.860365
2509.171029	287918.734853	38.865383
2511.526992	288359.355232	38.870400
2514.331616	288787.761330	38.875418
2516.183055	289235.192101	38.880436
2518.910674	289670.747263	38.885453
2521.727096	290113.502027	38.890471
2524.105270	290557.824258	38.895488
2526.613896	291007.027758	38.900506
2528.967868	291449.929728	38.905524
2531.696311	291904.101079	38.910541
2534.350698	292352.720163	38.915559
2536.698653	292822.521741	38.920576
2539.197756	293282.162857	38.925594
2541.578658	293746.698987	38.930612
2544.480387	294208.941596	38.935629
2547.563194	294654.592272	38.940647
2549.691674	295124.423613	38.945664
2552.063469	295584.892743	38.950682
2554.776827	296050.793508	38.955700
2557.212948	296509.878545	38.960717
2560.066586	296979.717512	38.965735
2562.572541	297456.672075	38.970752
2565.244388	297936.291676	38.975770
2567.667756	298410.005352	38.980788
2569.994076	298897.907205	38.985805
2572.842167	299366.572225	38.990823
2574.875922	299855.838527	38.995840
2577.328732	300349.202792	39.000858
2579.964410	300846.499165	39.005876
2582.400181	301335.113014	39.010893
2584.973046	301833.686240	39.015911
2587.578700	302358.542716	39.020928
2589.833854	302853.276519	39.025946
2592.785559	303360.700327	39.030964
2595.066509	303882.351440	39.035981
2598.116658	304383.177187	39.040999
2600.612175	304904.130059	39.046016
2602.933529	305418.732997	39.051034
2605.667029	305931.744630	39.056052
2608.300208	306458.867315	39.061069
2611.309595	306969.900724	39.066087
2613.761844	307492.856782	39.071104
2616.874290	308006.638265	39.076122
2619.511596	308513.457109	39.081140
2622.203738	309035.759004	39.086157
2625.029866	309551.484274	39.091175
2627.491864	310066.375982	39.096192
2630.199099	310576.121264	39.101210
2632.938609	311090.380234	39.106228
2635.491565	311604.463213	39.111245
2638.546999	312110.742890	39.116263
2641.299765	312625.907010	39.121280
2643.870814	313129.160002	39.126298
2646.867378	313599.477258	39.131316
2649.467734	314067.289916	39.136333
2652.246958	314517.648761	39.141351
2654.902736	314980.089423	39.146368
2657.477683	315433.956168	39.151386
2660.282710	315891.924318	39.156404
2662.691944	316366.766553	39.161421
2665.448733	316827.100025	39.166439
2667.668614	317307.885394	39.171456
2670.256855	317779.670028	39.176474
2673.113327	318244.222328	39.181492
2675.147340	318730.109446	39.186509
2677.913725	319212.728755	39.191527
2680.214663	319705.349537	39.196544
2682.793448	320206.304650	39.201562
2685.166911	320714.070452	39.206580
2687.532426	321223.282226	39.211597
2690.517104	321746.488070	39.216615
2692.823177	322277.518756	39.221632
2695.281629	322802.426927	39.226650
2698.263060	323323.312631	39.231668
2700.482433	323866.689620	39.236685
2703.376499	324396.496445	39.241703
2706.090942	324946.873343	39.246720
2708.758302	325483.946776	39.251738
2711.574083	326034.122463	39.256756
2714.244155	326593.637418	39.261773
2717.273941	327136.127642	39.266791
2719.624885	327696.015404	39.271808
2722.673788	328249.922426	39.276826
2726.137679	328792.256067	39.281844
2729.159435	329350.501795	39.286861
2732.467979	329884.903788	39.291879
2735.417105	330424.107486	39.296896
2738.404261	330959.162041	39.301914
2741.981248	331466.415024	39.306932
2744.917507	331995.324766	39.311949
2747.972767	332505.395491	39.316967
2750.889133	333006.901742	39.321984
2753.494059	333522.038814	39.327002
2756.698964	334012.903390	39.332020
2759.382674	334536.323781	39.337037
2761.962263	335034.872371	39.342055
2764.377343	335552.309550	39.347072
2766.906888	336058.399901	39.352090
2769.970121	336574.177634	39.357108
2772.135424	337085.370744	39.362125
2775.453142	337595.691810	39.367143
2778.431643	338108.296986	39.372160
2780.879744	338629.589536	39.377178
2783.668955	339144.704699	39.382196
2786.066671	339669.652945	39.387213
2788.426275	340193.384118	39.392231
2791.249439	340716.986708	39.397248
2793.419998	341240.281973	39.402266
2796.197994	341750.223290	39.407284
2798.309753	342267.907999	39.412301
2800.976200	342769.911576	39.417319
2803.459382	343280.216727	39.422336
2806.267339	343807.298721	39.427354
2809.144889	344316.973959	39.432372
2812.116769	344854.683736	39.437389
2814.748152	345379.494626	39.442407
2817.260339	345907.848511	39.447424
2819.930779	346445.895860	39.452442
2822.792547	346987.512811	39.457460
2825.353690	347543.718890	39.462477
2828.318622	348091.934868	39.467495
2831.275510	348653.703077	39.472512
2833.885299	349212.499571	39.477530
2836.759841	349774.218600	39.482548
2839.049509	350345.137882	39.487565
2841.999063	350924.704601	39.492583
2844.870126	351514.609212	39.497600
2847.467900	352097.722028	39.502618
2850.473708	352680.966871	39.507636
2852.914351	353283.053656	39.512653
2856.581607	353872.196514	39.517671
2859.660212	354464.878014	39.522688
2862.511156	355054.491922	39.527706
2865.647251	355648.902006	39.532724
2868.613206	356242.316707	39.537741
2871.856001	356829.893340	39.542759
2875.159564	357422.935951	39.547776
2877.783340	358018.566476	39.552794
2880.715627	358601.856242	39.557812
2883.178689	359201.101959	39.562829
2886.375141	359798.523612	39.567847
2889.606530	360393.419609	39.572864
2891.957751	360994.589542	39.577882
2895.403635	361585.274269	39.582900
2898.107087	362181.551101	39.587917
2900.905468	362783.058801	39.592935
2904.025664	363399.303693	39.597952
2907.037265	364008.603770	39.602970
2910.152158	364610.494279	39.607988
2912.652389	365215.341814	39.613005
2915.588324	365824.578722	39.618023
2918.507197	366432.744191	39.623040
2921.519783	367037.333736	39.628058
2925.020559	367635.392072	39.633076
2928.474966	368246.645240	39.638093
2931.176954	368846.285281	39.643111
2934.387428	369435.077304	39.648128
2937.165325	370026.162761	39.653146
2940.516797	370614.078903	39.658164
2943.768765	371220.855905	39.663181
2946.470683	371794.090543	39.668199
2949.743177	372377.554170	39.673216
2952.170955	372957.007478	39.678234
2955.344972	373506.927176	39.683252
2958.011823	374063.263007	39.688269
2960.884452	374613.520089	39.693287
2963.782901	375161.862758	39.698304
2966.169127	375713.526670	39.703322
2969.523651	376252.115749	39.708340
2972.552361	376813.456239	39.713357
2975.251711	377371.441294	39.718375
2977.924370	377939.773813	39.723392
2980.076556	378511.884538	39.728410
2982.910745	379089.105112	39.733428
2985.899851	379692.093082	39.738445
2988.416897	380285.861425	39.743463
2991.176301	380894.295935	39.748480
2993.754824	381508.939210	39.753498
2997.233393	382132.460983	39.758516
2999.705118	382754.381520	39.763533
3002.795132	383381.876089	39.768551
3006.081718	384014.858893	39.773568
3009.048149	384662.517705	39.778586
3012.163055	385293.552724	39.783604
3014.830335	385936.721495	39.788621
3017.894684	386576.645566	39.793639
3021.232129	387232.595986	39.798656
3024.293165	387885.965809	39.803674
3027.756450	388525.792279	39.808692
3031.082783	389177.600167	39.813709
3034.089582	389829.218418	39.818727
3037.370068	390475.252489	39.823744
3040.017472	391133.675101	39.828762
3043.422882	391773.781663	39.833780
3046.711536	392423.557208	39.838797
3049.547974	393075.902731	39.843815
3052.974106	393734.102017	39.848832
3055.737983	394397.820232	39.853850
3058.920096	395052.837459	39.858868
3061.748967	395705.767833	39.863885
3065.217764	396371.592618	39.868903
3068.606878	397033.689295	39.873920
3071.590723	397686.911471	39.878938
3074.690270	398333.611334	39.883956
3078.238403	399006.926732	39.888973
3081.214206	399649.411257	39.893991
3084.280444	400317.375291	39.899008
3087.152745	400971.513039	39.904026
3090.262165	401646.668598	39.909044
3093.885878	402303.728080	39.914061
3096.787465	402956.020641	39.919079
3100.198075	403604.517891	39.924096
3102.675563	404275.154315	39.929114
3105.584056	404939.345199	39.934132
3108.826759	405605.294288	39.939149
3111.670565	406280.849008	39.944167
3114.989607	406937.149902	39.949184
3117.884080	407601.007117	39.954202
3121.020475	408223.291697	39.959220
3124.158179	408875.194514	39.964237
3126.653517	409501.939430	39.969255
3129.902886	410133.469221	39.974272
3132.709893	410778.032780	39.979290
3135.334231	411424.943099	39.984308
3138.733598	412065.684681	39.989325
3141.540034	412725.286226	39.994343
3144.425468	413376.750548	39.999360
3147.102000	414055.806654	40.004378
3150.226576	414728.643200	40.009396
3153.415669	415419.091857	40.014413
3156.173616	416114.280340	40.019431
3159.552140	416801.979713	40.024448
3162.814151	417495.686556	40.029466
3165.951480	418203.358200	40.034484
3169.305532	418900.842379	40.039501
3172.355600	419613.762942	40.044519
3175.432282	420327.421288	40.049536
3178.566649	421044.498054	40.054554
3181.927376	421754.451702	40.059572
3185.658229	422481.353994	40.064589
3189.082452	423202.483891	40.069607
3192.514768	423919.058678	40.074624
3195.822037	424636.267714	40.079642
3199.019310	425352.081850	40.084660
3202.688153	426053.413725	40.089677
3205.799406	426774.472683	40.094695
3209.234850	427498.373923	40.099712
3212.318225	428214.053519	40.104730
3215.668815	428937.650239	40.109748
3218.931722	429653.743634	40.114765
3222.147048	430372.129827	40.119783
3225.447069	431094.636505	40.124800
3228.598278	431809.624602	40.129818
3232.237862	432544.675070	40.134836
3235.905552	433258.730832	40.139853
3239.016489	433976.552099	40.144871
3242.087406	434695.271121	40.149888
3245.575321	435428.211326	40.154906
3248.602837	436149.301587	40.159924
3252.018647	436874.563762	40.164941
3254.957054	437606.767673	40.169959
3258.190450	438328.243642	40.174976
3261.466867	439059.667624	40.179994
3264.554151	439798.594134	40.185012
3268.034177	440534.398160	40.190029
3271.049631	441276.532143	40.195047
3274.257161	441998.157563	40.200064
3277.364018	442747.016919	40.205082
3280.871052	443490.372386	40.210100
3284.199219	444230.695456	40.215117
3287.093183	444981.037653	40.220135
3290.614700	445742.596879	40.225152
3293.981288	446461.683352	40.230170
3296.763138	447187.471806	40.235188
3300.283784	447889.633304	40.240205
3303.581410	448588.164457	40.245223
3306.987476	449290.858729	40.250240
3310.034590	449997.890797	40.255258
3313.240643	450694.348398	40.260276
3316.980930	451394.192696	40.265293
3320.093075	452111.525080	40.270311
3324.063600	452812.149959	40.275328
3327.618589	453508.871551	40.280346
3330.778132	454204.622112	40.285364
3334.451091	454914.591118	40.290381
3337.958807	455611.508246	40.295399
3341.231185	456322.103254	40.300416
3344.384786	457032.441388	40.305434
3347.876496	457730.711566	40.310452
3351.294340	458437.623381	40.315469
3354.520162	459160.024909	40.320487
3357.715638	459869.253206	40.325504
3361.038282	460590.276808	40.330522
3364.349943	461340.063891	40.335540
3367.291697	462065.145944	40.340557
3370.878667	462801.736506	40.345575
3374.202666	463547.752160	40.350592
3377.476037	464305.333311	40.355610
3380.687307	465049.594553	40.360628
3383.841043	465813.665900	40.365645
3387.122625	466579.712541	40.370663
3390.362842	467336.027358	40.375680
3393.729109	468122.285227	40.380698
3396.893965	468897.166702	40.385716
3400.477115	469682.522316	40.390733
3403.776007	470464.049949	40.395751
3407.418953	471250.600777	40.400768
3410.741116	472031.862993	40.405786
3413.913219	472824.849561	40.410804
3417.964448	473623.581856	40.415821
3421.025763	474421.933652	40.420839
3424.804419	475217.562166	40.425856
3428.102628	476018.189523	40.430874
3431.380307	476820.405847	40.435892
3434.854938	477617.149961	40.440909
3437.984684	478431.760189	40.445927
3441.600536	479227.810783	40.450944
3445.222229	480053.042780	40.455962
3448.277802	480871.910817	40.460980
3452.379242	481687.193114	40.465997
3455.696431	482507.568519	40.471015
3459.586953	483302.298207	40.476032
3463.540974	484091.578123	40.481050
3467.417057	484900.039951	40.486068
3470.944074	485702.004630	40.491085
3474.651591	486503.957666	40.496103
3478.143392	487279.435918	40.501120
3481.878766	488047.529767	40.506125
3485.243711	488771.564073	40.511130
3489.015314	489435.589196	40.516135
3492.022771	490039.543241	40.521140
3494.923924	490583.783787	40.526144
3498.008685	491073.992958	40.531149
3500.250925	491518.946461	40.536154
3502.828734	491868.528470	40.541159
3504.699719	492194.414355	40.546164
3507.118692	492432.853487	40.551168
3509.138362	492654.135152	40.556173
3510.535170	492812.416138	40.561178
3511.956478	492930.433941	40.566183
3513.454888	493011.725732	40.571188
3514.357780	493056.904697	40.576192
3515.828903	493060.571381	40.581197
3516.477012	493031.604933	40.586202
3517.272610	492993.449504	40.591207
3517.628956	492919.764230	40.596212
3518.556101	492818.086212	40.601216
3519.055935	492711.208661	40.606221
3518.957479	492578.699982	40.611226
3519.918718	492426.323768	40.616231
3519.789134	492262.167490	40.621236
3520.137770	492096.668140	40.626240
3519.983359	491909.673442	40.631245
3519.951912	491709.186573	40.636250
3520.242237	491514.926399	40.641255
3520.000160	491299.022326	40.646260
3519.902908	491093.474883	40.651264
3520.169930	490886.095037	40.656269
3520.031441	490674.978600	40.661274
3519.852324	490451.356705	40.666279
3519.739453	490223.264788	40.671284
3519.561753	489995.281632	40.676288
3519.376567	489774.843377	40.681293
3519.053909	489543.990736	40.686298
3519.083237	489320.423699	40.691303
3518.702236	489101.376008	40.696308
3518.536064	488873.022864	40.701312
3518.640566	488650.448991	40.706317
3518.419963	488426.708249	40.711322
3517.983628	488205.734152	40.716327
3517.813812	487988.919492	40.721332
3517.413727	487762.717294	40.726336
3517.253434	487548.884616	40.731341
3516.796361	487343.201092	40.736346
3516.705131	487126.009561	40.741351
3516.532968	486926.051118	40.746356
3516.115337	486719.797403	40.751360
3515.842586	486508.300955	40.756365
3515.060568	486325.605081	40.761370
3515.351789	486137.570775	40.766375
3515.194259	485943.931875	40.771380
3514.948911	485756.434550	40.776384
3514.904250	485577.566321	40.781389
3514.518768	485403.005668	40.786394
3514.521402	485205.331898	40.791399
3513.891798	485053.147589	40.796404
3514.153565	484879.037123	40.801408
3513.932158	484702.113770	40.806413
3513.267693	484541.673158	40.811418
3513.389174	484378.827190	40.816423
3513.112756	484226.073887	40.821428
3512.835651	484058.221977	40.826432
3512.560741	483904.452631	40.831437
3512.460751	483753.086263	40.836442
3512.770265	483597.144888	40.841447
3512.308853	483457.891364	40.846452
3512.176113	483299.180286	40.851456
3512.089218	483156.774845	40.856461
3511.417170	483021.452690	40.861466
3511.434093	482877.458156	40.866471
3511.513739	482754.580457	40.871476
3510.844144	482620.927102	40.876480
3511.006604	482483.341293	40.881485
3510.603531	482366.161462	40.886490
3510.794805	482247.265621	40.891495
3510.343588	482125.177198	40.896500
3510.379174	482005.443135	40.901504
3510.727270	481875.221234	40.906509
3510.012675	481776.530416	40.911514
3510.005965	481658.219631	40.916519
3509.792388	481555.851000	40.921524
3509.853671	481436.109381	40.926528
3509.880991	481329.850596	40.931533
3509.428174	481217.789385	40.936538
3509.354215	481107.694467	40.941543
3508.891024	481012.304298	40.946548
3508.472444	480924.963296	40.951552
3508.677113	480830.074726	40.956557
3508.541519	480745.323095	40.961562
3509.052610	480644.101935	40.966567
3508.619589	480562.183468	40.971572
3508.777924	480471.354238	40.976576
3508.528894	480385.048145	40.981581
3508.412589	480298.923384	40.986586
3508.211381	480210.734081	40.991591
3508.421684	480133.576726	40.996596
3507.997445	480042.786927	41.001600
3507.921419	479951.333587	41.006605
3507.351299	479879.669981	41.011610
3507.373484	479794.483920	41.016615
3507.312849	479723.702017	41.021620
3506.871506	479660.733193	41.026624
3507.061243	479586.566724	41.031629
3506.914623	479525.172462	41.036634
3507.504204	479458.188771	41.041639
3507.099407	479399.976761	41.046644
3506.948362	479331.994861	41.051648
3506.968199	479268.090411	41.056653
3506.484664	479202.593031	41.061658
3506.664830	479153.054671	41.066663
3506.704644	479091.477565	41.071668
3506.720640	479036.238509	41.076672
3506.657080	478986.028794	41.081677
3506.245283	478932.732079	41.086682
3506.419056	478869.460797	41.091687
3506.416838	478813.970619	41.096692
3506.108012	478770.488406	41.101696
3506.468329	478715.092677	41.106701
3506.260986	478663.739308	41.111706
3506.162853	478610.848237	41.116711
3506.003794	478567.037843	41.121716
3506.117348	478518.420611	41.126720
3506.180730	478465.757008	41.131725
3505.797495	478428.367078	41.136730
3505.754133	478376.987046	41.141735
3506.109631	478331.422440	41.146740
3505.836665	478294.369570	41.151744
3506.025462	478245.993166	41.156749
3505.895524	478201.417194	41.161754
3505.947710	478147.994349	41.166759
3505.800673	478109.704955	41.171764
3505.526397	478057.549745	41.176768
3505.970575	478021.295219	41.181773
3505.582564	477981.016531	41.186778
3505.503213	477935.114323	41.191783
3505.833705	477898.320078	41.196788
3505.330550	477853.700962	41.201792
3505.427679	477818.261105	41.206797
3505.247826	477786.969967	41.211802
3505.257195	477754.432572	41.216807
3505.315122	477715.096438	41.221812
3505.348363	477680.882737	41.226816
3505.491948	477647.209007	41.231821
3505.093988	477607.133851	41.236826
3505.216115	477574.324941	41.241831
3505.551251	477541.887745	41.246836
3505.073481	477511.656857	41.251840
3505.481562	477476.927438	41.256845
3505.213274	477446.714020	41.261850
3505.436305	477397.417904	41.266855
3505.467905	477369.488246	41.271860
3505.290079	477333.229427	41.276864
3505.344781	477294.349095	41.281869
3505.051807	477271.792030	41.286874
3505.358734	477224.813522	41.291879
3505.050751	477193.034899	41.296884
3504.863888	477166.355821	41.301888
3504.706698	477134.908034	41.306893
3504.846107	477111.674275	41.311898
3504.879069	477070.921757	41.316903
3504.450711	477065.515971	41.321908
3504.784233	477031.405733	41.326912
3505.155477	477003.117790	41.331917
3504.530763	476986.035705	41.336922
3505.130664	476956.241803	41.341927
3505.012167	476927.879122	41.346932
3505.119078	476896.287852	41.351936
3505.181467	476858.419082	41.356941
3505.033919	476842.427121	41.361946
3504.938035	476794.041511	41.366951
3505.096157	476763.658293	41.371956
3504.838680	476740.486838	41.376960
3505.359517	476705.484848	41.381965
3504.716436	476677.306095	41.386970
3504.790946	476643.540229	41.391975
3504.846997	476626.350229	41.396980
3504.552588	476605.971962	41.401984
3504.731815	476588.863824	41.406989
3504.826539	476552.003003	41.411994
3504.805916	476527.881584	41.416999
3504.464945	476501.783481	41.422004
3504.292153	476476.571043	41.427008
3504.831827	476446.887269	41.432013
3504.465730	476436.707323	41.437018
3504.791451	476410.300989	41.442023
3504.611543	476380.680177	41.447028
3504.428205	476358.155433	41.452032
3504.630475	476329.234375	41.457037
3504.589312	476309.018506	41.462042
3504.812585	476285.618485	41.467047
3504.501311	476271.172431	41.472052
3503.969849	476241.606983	41.477056
3504.785476	476213.754514	41.482061
3504.501745	476194.286434	41.487066
3504.599193	476169.436357	41.492071
3504.743790	476147.518421	41.497076
3504.688115	476126.189633	41.502080
3504.706282	476097.094608	41.507085
3504.406336	476085.738310	41.512090
3504.543716	476047.856154	41.517095
3504.494930	476032.861604	41.522100
3504.512782	475998.546090	41.527104
3504.806102	475984.206997	41.532109
3504.272877	475965.538385	41.537114
3504.397026	475932.827832	41.542119
3504.762645	475919.389572	41.547124
3504.487773	475909.600406	41.552128
3504.282842	475878.969133	41.557133
3504.418893	475855.126243	41.562138
3504.756311	475828.717297	41.567143
3504.757467	475811.788696	41.572148
3504.508118	475782.634133	41.577152
3504.956381	475767.712870	41.582157
3504.632163	475731.423605	41.587162
3504.176503	475712.641128	41.592167
3504.378456	475695.275216	41.597172
3504.123400	475667.489864	41.602176
3504.523680	475647.102183	41.607181
3504.172680	475629.874303	41.612186
3504.592265	475604.921925	41.617191
3504.502672	475587.196527	41.622196
3503.883206	475568.186385	41.627200
3504.205826	475541.728717	41.632205
3504.296561	475536.544570	41.637210
3504.408599	475510.474940	41.642215
3504.400520	475497.095468	41.647220
3504.358428	475466.893990	41.652224
3504.532344	475446.440518	41.657229
3504.160646	475442.849990	41.662234
3504.446228	475415.232257	41.667239
3504.657047	475385.700271	41.672244
3504.450813	475380.461655	41.677248
3504.764670	475353.042108	41.682253
3504.435779	475321.618617	41.687258
3504.271067	475300.306188	41.692263
3504.405606	475287.613628	41.697268
3504.208720	475260.933597	41.702272
3504.056162	475255.382351	41.707277
3503.990917	475239.376102	41.712282
3503.967371	475215.253569	41.717287
3504.088616	475215.741294	41.722292
3503.909909	475193.163825	41.727296
3503.982308	475181.900217	41.732301
3503.966788	475162.388740	41.737306
3504.145951	475141.579330	41.742311
3504.131057	475135.043262	41.747316
3504.240532	475118.553129	41.752320
3504.351449	475096.081829	41.757325
3504.250918	475070.247974	41.762330
3504.239921	475059.707081	41.767335
3504.124459	475044.468904	41.772340
3504.042571	475040.072205	41.777344
3504.339032	475010.526133	41.782349
3504.124644	474994.543264	41.787354
3504.025726	474966.580206	41.792359
3504.332964	474952.035436	41.797364
3504.000604	474950.871537	41.802368
3504.288006	474911.949809	41.807373
3504.047857	474922.023682	41.812378
3504.217615	474882.867062	41.817383
3504.390591	474866.366685	41.822388
3503.818787	474847.297639	41.827392
3504.298562	474833.992673	41.832397
3504.082789	474814.411141	41.837402
3504.027851	474791.965719	41.842407
3503.956783	474787.313821	41.847412
3504.293182	474772.257447	41.852416
3504.219690	474756.404178	41.857421
3503.729900	474740.920821	41.862426
3504.081716	474721.807035	41.867431
3504.164302	474708.716829	41.872436
3503.652811	474696.683569	41.877440
3503.987309	474684.820699	41.882445
3503.892116	474661.976001	41.887450
3504.273869	474655.731890	41.892455
3504.124995	474627.826946	41.897460
3504.003577	474612.437323	41.902464
3504.095026	474614.399696	41.907469
3504.006929	474586.180966	41.912474
3504.186365	474580.779805	41.917479
3504.181286	474554.626080	41.922484
3504.114868	474544.195053	41.927488
3503.917288	474521.417068	41.932493
3504.016518	474507.158294	41.937498
3504.242090	474491.663044	41.942503
3504.192397	474473.930361	41.947508
3504.444853	474463.905075	41.952512
3504.668776	474430.973568	41.957517
3504.192183	474420.810062	41.962522
3504.297309	474399.200591	41.967527
3504.280088	474375.937745	41.972532
3503.742618	474355.798367	41.977536
3504.009152	474347.544867	41.982541
3504.256314	474320.539965	41.987546
3504.572624	474297.629811	41.992551
3504.246553	474288.202763	41.997556
3504.251891	474266.203421	42.002560
3504.333706	474243.837150	42.007565
3504.016223	474236.588302	42.012570
3504.142559	474208.791343	42.017575
3504.143870	474187.198056	42.022580
3504.033112	474174.644947	42.027584
3504.371126	474165.366313	42.032589
3504.402859	474155.274388	42.037594
3504.290967	474127.667038	42.042599
3504.151002	474109.998994	42.047604
3504.109156	474088.919306	42.052608
3504.496864	474074.918760	42.057613
3504.142891	474059.666852	42.062618
3504.241201	474034.459193	42.067623
3504.501808	474019.363552	42.072628
3503.790540	473997.679945	42.077632
3504.061961	473966.514275	42.082637
3504.067268	473964.181793	42.087642
3504.067102	473951.154867	42.092647
3504.277667	473936.878094	42.097652
3504.204147	473916.005989	42.102656
3504.079007	473883.787722	42.107661
3503.973501	473874.984572	42.112666
3504.054736	473858.244432	42.117671
3503.937600	473849.341732	42.122676
3504.056436	473830.061178	42.127680
3504.016763	473809.487747	42.132685
3504.022265	473802.745269	42.137690
3504.277255	473778.120794	42.142695
3504.173743	473774.842398	42.147700
3503.863098	473753.754162	42.152704
3504.154218	473737.994530	42.157709
3504.151207	473718.834510	42.162714
3503.775803	473705.359847	42.167719
3503.989189	473695.036222	42.172724
3503.802771	473675.601016	42.177728
3503.936204	473665.847598	42.182733
3503.946450	473651.602289	42.187738
3503.905624	473630.876791	42.192743
3504.045713	473626.546076	42.197748
3503.647485	473609.678761	42.202752
3503.910928	473587.435126	42.207757
3504.030354	473594.157997	42.212762
3503.685474	473579.056359	42.217767
3504.164484	473558.045859	42.222772
3504.254703	473549.211630	42.227776
3504.049625	473520.705770	42.232781
3503.893360	473514.444974	42.237786
3503.815484	473497.324169	42.242791
3504.007642	473483.404817	42.247796
3504.094068	473485.063955	42.252800
3503.979570	473445.898802	42.257805
3503.807175	473434.013948	42.262810
3503.649810	473424.357070	42.267815
3503.844853	473394.672607	42.272820
3503.953399	473392.881331	42.277824
3504.050536	473383.691106	42.282829
3503.457317	473372.075494	42.287834
3503.572569	473350.311237	42.292839
3503.453340	473360.721601	42.297844
3503.596913	473365.666575	42.302848
3503.630934	473323.943205	42.307853
3503.923778	473314.113731	42.312858
3503.676457	473318.917743	42.317863
3503.695677	473304.366631	42.322868
3503.932803	473279.592306	42.327872
3504.048616	473278.813679	42.332877
3503.704644	473267.716203	42.337882
3503.567392	473255.116023	42.342887
3503.798054	473237.287254	42.347892
3503.817896	473239.514532	42.352896
3504.089616	473210.425966	42.357901
3503.743579	473213.217986	42.362906
3503.853720	473199.514166	42.367911
3504.106847	473174.230278	42.372916
3503.810692	473174.226435	42.377920
3503.837762	473143.351582	42.382925
3503.465756	473135.806813	42.387930
3504.078293	473123.240107	42.392935
3503.899581	473112.065732	42.397940
3503.748873	473105.297025	42.402944
3503.897567	473101.218292	42.407949
3504.085213	473076.096705	42.412954
3503.819568	473059.613503	42.417959
3503.925446	473049.205164	42.422964
3503.763841	473033.313786	42.427968
3503.537706	473020.575438	42.432973
3503.605433	473022.085497	42.437978
3503.782694	473005.735005	42.442983
3503.955767	472982.440484	42.447988
3503.687923	472990.492047	42.452992
3503.763056	472976.033244	42.457997
3503.636392	472962.265314	42.463002
3503.746338	472964.681144	42.468007
3503.802182	472956.663150	42.473012
3503.610424	472939.306422	42.478016
3503.910373	472925.673798	42.483021
3503.651677	472913.852972	42.488026
3503.638422	472907.366618	42.493031
3504.075913	472886.919595	42.498036
3503.651768	472881.157170	42.503040
3503.671735	472873.702419	42.508045
3503.629461	472846.944079	42.513050
3503.809151	472834.192157	42.518055
3504.004000	472840.244366	42.523060
3503.625167	472833.866467	42.528064
3503.847778	472811.780517	42.533069
3503.830913	472816.142687	42.538074
3503.833345	472793.483221	42.543079
3503.879766	472772.844442	42.548084
3503.910955	472774.968594	42.553088
3503.962185	472758.435060	42.558093
3503.658466	472742.363152	42.563098
3503.545074	472734.118363	42.568103
3503.735247	472725.420053	42.573108
3503.337568	472704.243102	42.578112
3503.980351	472691.417891	42.583117
3503.940207	472697.507288	42.588122
3503.724741	472674.932825	42.593127
3504.154638	472664.726533	42.598132
3503.912884	472655.082629	42.603136
3503.771466	472628.542442	42.608141
3503.616193	472625.525501	42.613146
3503.536848	472618.542583	42.618151
3503.720879	472600.163018	42.623156
3503.616109	472594.045875	42.628160
3503.741586	472575.776927	42.633165
3503.852599	472580.372394	42.638170
3503.841929	472558.576505	42.643175
3504.236758	472538.845568	42.648180
3504.104416	472540.640748	42.653184
3504.163722	472508.391151	42.658189
3504.095025	472497.300434	42.663194
3503.899498	472480.907064	42.668199
3503.955898	472467.616787	42.673204
3503.859785	472449.332060	42.678208
3503.981236	472430.201848	42.683213
3503.925169	472422.758951	42.688218
3503.513097	472408.832991	42.693223
3503.732430	472378.737672	42.698228
3503.672395	472381.738059	42.703232
3503.692586	472385.334075	42.708237
3503.777437	472381.468061	42.713242
3503.772617	472358.403719	42.718247
3504.050126	472353.138545	42.723252
3503.759705	472330.524857	42.728256
3504.029606	472319.380522	42.733261
3503.555866	472314.082009	42.738266
3503.325958	472298.200855	42.743271
3503.442487	472278.615043	42.748276
3503.594343	472269.111511	42.753280
3503.422405	472272.991380	42.758285
3503.811651	472275.008294	42.763290
3504.120699	472250.119968	42.768295
3503.747642	472241.003552	42.773300
3503.445150	472248.706032	42.778304
3503.718160	472226.205940	42.783309
3503.727122	472208.208546	42.788314
3503.368558	472205.933379	42.793319
3503.228283	472203.927866	42.798324
3503.461276	472205.665327	42.803329
3503.678212	472184.897616	42.808333
3503.384653	472169.888205	42.813338
3503.493949	472168.857101	42.818343
3503.689450	472152.401659	42.823348
3503.518302	472171.540055	42.828353
3503.682109	472137.600483	42.833357
3503.582732	472126.159562	42.838362
3503.685985	472127.005060	42.843367
3503.701935	472128.168517	42.848372
3503.716224	472104.948789	42.853377
3503.792493	472091.300274	42.858381
3503.622631	472089.502199	42.863386
3503.811308	472070.411718	42.868391
3503.696396	472062.572445	42.873396
3503.529494	472069.898705	42.878401
3503.910053	472056.911776	42.883405
3503.960800	472028.768940	42.888410
3503.701649	472023.335044	42.893415
3503.889384	472012.000756	42.898420
3503.670335	471999.919666	42.903425
3503.739988	471984.903401	42.908429
3503.862441	471977.229349	42.913434
3503.600575	471960.085644	42.918439
3503.983165	471946.236532	42.923444
3503.710706	471937.864484	42.928449
3503.688669	471921.899486	42.933453
3503.583877	471901.892056	42.938458
3503.880896	471905.038848	42.943463
3503.415056	471904.859048	42.948468
3503.263145	471879.029259	42.953473
3503.453622	471866.072256	42.958477
3503.623062	471860.621263	42.963482
3503.489277	471861.757710	42.968487
3503.708672	471857.515473	42.973492
3503.421332	471840.679858	42.978497
3503.600451	471820.880941	42.983501
3503.743055	471824.761869	42.988506
3503.843510	471825.100882	42.993511
3503.545020	471802.690662	42.998516
3503.622804	471785.797287	43.003521
3503.767349	471776.294683	43.008525
3503.754584	471784.255704	43.013530
3503.504535	471775.474495	43.018535
3503.761061	471761.493103	43.023540
3503.436505	471766.867321	43.028545
3503.852444	471749.007971	43.033549
3503.860997	471731.314388	43.038554
3503.514952	471724.626792	43.043559
3503.759937	471724.334631	43.048564
3503.534564	471711.392569	43.053569
3503.583889	471675.594641	43.058573
3503.542593	471690.708108	43.063578
3503.617309	471686.691482	43.068583
3504.041958	471665.129998	43.073588
3503.223509	471656.489278	43.078593
3503.748215	471640.285555	43.083597
3503.699578	471641.205777	43.088602
3503.389611	471634.918004	43.093607
3503.788988	471609.558374	43.098612
3503.335223	471619.566252	43.103617
3503.303790	471599.800404	43.108621
3503.773051	471602.413072	43.113626
3503.838472	471593.176362	43.118631
3503.881004	471578.113392	43.123636
3503.571524	471569.189405	43.128641
3503.610424	471551.085313	43.133645
3503.825412	471531.686004	43.138650
3503.795205	471523.985220	43.143655
3503.833705	471526.108346	43.148660
3503.383636	471511.528749	43.153665
3503.643780	471496.177848	43.158669
3503.758940	471497.021490	43.163674
3503.472890	471486.775699	43.168679
3503.507112	471466.897955	43.173684
3503.769252	471463.713473	43.178689
3503.290278	471455.272481	43.183693
3503.695235	471451.203609	43.188698
3503.485171	471436.586022	43.193703
3503.655463	471431.743121	43.198708
3503.358124	471422.462285	43.203713
3503.769804	471410.737403	43.208717
3503.712672	471409.022839	43.213722
3503.317232	471393.319233	43.218727
3503.665517	471376.382764	43.223732
3503.580949	471381.110807	43.228737
3503.527432	471373.920602	43.233741
3503.625857	471352.968002	43.238746
3503.386683	471338.152166	43.243751
3503.657874	471332.330084	43.248756
3503.522146	471338.941944	43.253761
3503.658387	471337.906540	43.258765
3503.699200	471310.575413	43.263770
3503.019265	471314.535761	43.268775
3503.400469	471297.087071	43.273780
3503.257499	471311.507154	43.278785
3503.382731	471307.533165	43.283789
3503.601994	471300.958854	43.288794
3503.393838	471273.007993	43.293799
3503.695356	471268.701959	43.298804
3503.449127	471279.133455	43.303809
3503.915902	471257.666277	43.308813
3503.952697	471249.397150	43.313818
3503.565900	471227.557909	43.318823
3504.025537	471209.944661	43.323828
3503.842061	471202.825634	43.328833
3503.827015	471190.509038	43.333837
3504.047668	471181.196911	43.338842
3503.782042	471175.763812	43.343847
3503.927817	471154.904918	43.348852
3503.799926	471151.224388	43.353857
3503.892348	471124.493204	43.358861
3504.041908	471113.722109	43.363866
3503.474544	471105.345640	43.368871
3503.842484	471073.501264	43.373876
3503.443115	471069.762240	43.378881
3503.327698	471078.196023	43.383885
3503.704092	471078.795606	43.388890
3503.628011	471055.791761	43.393895
3503.948628	471033.941886	43.398900
3503.399758	471031.088316	43.403905
3503.409795	471028.551968	43.408909
3503.819746	471005.521936	43.413914
3503.249087	471002.773199	43.418919
3503.706157	470994.741713	43.423924
3503.606599	470992.121292	43.428929
3503.548637	470984.069821	43.433933
3503.634815	470960.786741	43.438938
3503.632607	470953.385494	43.443943
3503.817011	470958.172509	43.448948
3503.208106	470940.271670	43.453953
3503.308152	470929.204129	43.458957
3503.632120	470915.566377	43.463962
3503.443207	470927.763357	43.468967
3503.459227	470913.312445	43.473972
3503.336482	470921.139096	43.478977
3503.852187	470906.862676	43.483981
3503.530130	470881.869668	43.488986
3503.253010	470874.866722	43.493991
3503.666328	470872.368001	43.498996
3503.364646	470872.517114	43.504001
3503.516449	470855.814062	43.509005
3503.761824	470846.700662	43.514010
3503.457433	470849.689200	43.519015
3504.031545	470840.270352	43.524020
3503.778006	470829.816309	43.529025
3503.813290	470809.278708	43.534029
3503.802639	470797.265361	43.539034
3503.374510	470785.520783	43.544039
3503.418407	470766.806854	43.549044
3503.642121	470773.108596	43.554049
3503.760338	470764.572922	43.559053
3504.088559	470741.961088	43.564058
3503.553996	470736.418293	43.569063
3503.601941	470723.280315	43.574068
3503.563989	470725.415608	43.579073
3503.477798	470693.997308	43.584077
3503.672057	470693.662456	43.589082
3503.582425	470689.925099	43.594087
3504.062835	470678.493119	43.599092
3503.480588	470664.187297	43.604097
3503.512574	470642.636116	43.609101
3503.626117	470646.876739	43.614106
3503.659128	470627.251861	43.619111
3503.806073	470615.061406	43.624116
3503.611837	470607.791782	43.629121
3503.405366	470605.137514	43.634125
3503.848743	470595.384342	43.639130
3503.461539	470583.024816	43.644135
3503.762707	470568.173710	43.649140
3503.564232	470574.288763	43.654145
3503.663515	470567.226214	43.659149
3503.709831	470542.630840	43.664154
3503.349439	470531.737261	43.669159
3503.255627	470540.979002	43.674164
3503.192800	470535.868557	43.679169
3503.393136	470541.515003	43.684173
3503.541127	470537.233086	43.689178
3503.159241	470511.437932	43.694183
3503.717757	470496.850280	43.699188
3503.223379	470496.877763	43.704193
3503.327317	470498.585073	43.709197
3503.610142	470495.701357	43.714202
3503.446439	470485.841305	43.719207
3503.535198	470464.027478	43.724212
3503.392575	470473.175570	43.729217
3503.453973	470468.451051	43.734221
3503.567593	470452.007194	43.739226
3503.634454	470457.674761	43.744231
3503.873125	470422.960069	43.749236
3503.598894	470418.542078	43.754241
3503.477655	470424.087295	43.759245
3503.872255	470405.013418	43.764250
3503.401845	470399.105509	43.769255
3503.251459	470389.953071	43.774260
3503.222309	470387.929813	43.779265
3503.683316	470387.856977	43.784269
3503.877400	470377.027763	43.789274
3503.343500	470359.722932	43.794279
3503.870766	470336.470821	43.799284
3503.782006	470349.767659	43.804289
3503.662521	470327.023350	43.809293
3503.550847	470304.784757	43.814298
3503.496317	470300.078525	43.819303
3503.529705	470298.552350	43.824308
3503.246274	470287.190197	43.829313
3503.378947	470255.483145	43.834317
3503.463207	470258.207543	43.839322
3503.187949	470263.574357	43.844327
3503.688230	470247.981779	43.849332
3503.451395	470264.749530	43.854337
3503.293038	470256.916435	43.859341
3503.393163	470240.981522	43.864346
3503.406548	470241.283628	43.869351
3503.547321	470226.102746	43.874356
3503.132711	470246.092580	43.879361
3503.472923	470229.359239	43.884365
3503.907931	470225.640264	43.889370
3503.574863	470211.953813	43.894375
3503.870552	470184.834397	43.899380
3504.069173	470192.762619	43.904385
3503.840629	470167.855360	43.909389
3503.823260	470146.717048	43.914394
3503.360294	470152.316354	43.919399
3503.189242	470118.781274	43.924404
3503.199243	470118.830425	43.929409
3503.439917	470105.762986	43.934413
3503.831373	470107.272787	43.939418
3503.086738	470111.801267	43.944423
3503.446036	470101.909059	43.949428
3503.691202	470101.971737	43.954433
3503.334070	470089.302971	43.959437
3503.679236	470083.418148	43.964442
3503.490193	470072.395845	43.969447
3503.820881	470074.523633	43.974452
3503.555630	470053.018822	43.979457
3503.463080	470033.768116	43.984461
3503.632931	470035.921332	43.989466
3503.485791	470041.470744	43.994471
3503.641691	470011.280598	43.999476
3504.158959	469995.583750	44.004481
3503.848384	470008.256788	44.009485
3503.586919	469977.219993	44.014490
3503.590534	469960.995929	44.019495
3503.495051	469950.617852	44.024500
3503.425923	469957.270325	44.029505
3503.356154	469951.603149	44.034509
3503.653615	469932.240002	44.039514
3503.261309	469928.246158	44.044519
3503.206630	469921.866808	44.049524
3503.259898	469917.751832	44.054529
3503.213804	469905.642172	44.059533
3503.612401	469919.115743	44.064538
3503.209944	469933.983392	44.069543
3503.512015	469898.142430	44.074548
3503.212218	469894.488848	44.079553
3503.160787	469880.656260	44.084557
3503.629430	469878.503568	44.089562
3503.392012	469885.081268	44.094567
3503.484633	469890.643521	44.099572
3503.430678	469877.470414	44.104577
3503.352383	469856.240039	44.109581
3503.325984	469852.898125	44.114586
3503.405726	469852.023675	44.119591
3503.101758	469840.765920	44.124596
3503.017535	469854.467948	44.129601
3503.453326	469851.458567	44.134605
3503.477356	469841.010845	44.139610
3503.510184	469821.030340	44.144615
3503.383491	469815.220027	44.149620
3503.541272	469803.382275	44.154625
3503.672246	469805.896552	44.159629
3503.235748	469794.811818	44.164634
3503.156596	469788.486994	44.169639
3503.567204	469767.939732	44.174644
3503.366619	469770.607821	44.179649
3503.529362	469779.099563	44.184653
3503.526941	469766.323831	44.189658
3503.583564	469766.619109	44.194663
3503.358789	469742.014936	44.199668
3503.403120	469744.796412	44.204673
3503.538945	469739.958564	44.209677
3503.604604	469735.740196	44.214682
3503.409121	469741.753622	44.219687
3503.669571	469699.987104	44.224692
3503.516202	469701.684454	44.229697
3503.362061	469707.082965	44.234701
3503.856563	469687.587045	44.239706
3503.520085	469675.269655	44.244711
3503.744454	469657.793678	44.249716
3503.669205	469659.478683	44.254721
3503.519458	469646.827564	44.259725
3503.720154	469641.168250	44.264730
3503.587522	469624.103570	44.269735
3503.684988	469611.565451	44.274740
3503.972708	469601.582921	44.279745
3503.578282	469584.660989	44.284749
3503.623827	469574.209732	44.289754
3503.455531	469581.435695	44.294759
3503.442029	469561.715760	44.299764
3503.453931	469548.126438	44.304769
3503.570175	469540.046868	44.309773
3503.662129	469533.644220	44.314778
3503.395633	469542.508105	44.319783
3503.778273	469525.412595	44.324788
3503.585716	469510.537377	44.329793
3503.616220	469501.355952	44.334797
3503.717870	469491.656280	44.339802
3503.551179	469478.095142	44.344807
3503.589812	469469.571515	44.349812
3503.452055	469457.425382	44.354817
3503.566375	469460.804230	44.359821
3503.539981	469461.568933	44.364826
3503.459422	469440.287790	44.369831
3503.522754	469421.873773	44.374836
3503.385757	469409.524693	44.379841
3503.234959	469413.655254	44.384845
3503.516568	469405.650892	44.389850
3503.142952	469413.213567	44.394855
3503.487823	469391.003229	44.399860
3503.530862	469379.284771	44.404865
3503.651916	469374.043574	44.409869
3503.737070	469376.362347	44.414874
3503.417740	469371.292160	44.419879
3503.354713	469337.688041	44.424884
3503.430087	469345.331869	44.429889
3503.431519	469341.275673	44.434893
3503.630606	469331.408425	44.439898
3503.655502	469343.065539	44.444903
3503.559242	469315.195742	44.449908
3503.601968	469317.876129	44.454913
3503.397805	469303.813798	44.459917
3503.656153	469306.054502	44.464922
3503.205337	469302.424686	44.469927
3503.484668	469262.428809	44.474932
3503.651359	469266.205013	44.479937
3503.570449	469264.443329	44.484941
3503.643097	469263.874177	44.489946
3503.333942	469252.566221	44.494951
3503.492704	469226.582604	44.499956
3503.334154	469229.801821	44.504961
3503.311887	469230.008177	44.509965
3503.662573	469226.200954	44.514970
3503.276569	469211.711002	44.519975
3503.008496	469200.497924	44.524980
3503.251175	469196.099364	44.529985
3503.170620	469190.636486	44.534989
3503.540366	469183.581416	44.539994
3503.410893	469194.958811	44.544999
3503.300483	469191.376568	44.550004
3503.615236	469184.735794	44.555009
3503.504209	469178.922827	44.560013
3503.507378	469148.502067	44.565018
3503.302082	469158.623955	44.570023
3503.571481	469154.880268	44.575028
3503.723883	469150.242466	44.580033
3503.478416	469142.118515	44.585037
3503.481560	469119.961904	44.590042
3503.228635	469118.075295	44.595047
3503.419369	469114.851042	44.600052
3503.291520	469121.867968	44.605057
3503.075690	469122.003520	44.610061
3503.345220	469111.415224	44.615066
3503.282065	469100.473906	44.620071
3503.235669	469090.087639	44.625076
3503.375881	469066.895292	44.630081
3503.283627	469071.878579	44.635085
3503.291910	469078.012089	44.640090
3503.414367	469073.176200	44.645095
3503.629823	469062.241522	44.650100
3503.651773	469052.097937	44.655105
3503.249477	469046.787281	44.660109
3503.449191	469026.475427	44.665114
3503.264564	469040.092461	44.670119
3503.236310	469036.395804	44.675124
3503.422326	469039.053577	44.680129
3503.636622	469026.395236	44.685133
3503.401030	469009.954736	44.690138
3503.246239	469003.996536	44.695143
3503.334357	468998.659048	44.700148
3503.606573	468993.495263	44.705153
3503.217467	469001.111236	44.710157
3503.547276	468984.632045	44.715162
3503.616103	468968.650402	44.720167
3503.370200	468962.453087	44.725172
3503.230821	468950.864625	44.730177
3503.302549	468961.500530	44.735181
3503.319833	468964.438489	44.740186
3503.448513	468961.883134	44.745191
3503.378671	468935.124073	44.750196
3503.487410	468928.921391	44.755201
3503.073661	468932.738705	44.760205
3503.598291	468920.436854	44.765210
3503.202442	468928.459528	44.770215
3503.231371	468915.019204	44.775220
3503.285161	468924.035528	44.780225
3503.272115	468900.461613	44.785229
3503.405137	468881.833297	44.790234
3503.079411	468883.608659	44.795239
3503.285305	468875.768166	44.800244
3503.532148	468877.402321	44.805249
3503.223643	468886.628033	44.810253
3503.682386	468881.434736	44.815258
3503.272813	468866.897567	44.820263
3503.121153	468846.387574	44.825268
3503.429749	468846.541634	44.830273
3503.278373	468844.588247	44.835277
3503.454140	468844.104186	44.840282
3503.297822	468864.510829	44.845287
3503.551290	468848.195701	44.850292
3503.611675	468826.333937	44.855297
3503.265117	468830.242050	44.860301
3503.321939	468813.146757	44.865306
3503.201838	468809.058967	44.870311
3503.225557	468819.651832	44.875316
3503.211756	468817.473891	44.880321
3503.324586	468814.566114	44.885325
3503.708131	468793.565858	44.890330
3503.458697	468774.997902	44.895335
3503.627220	468774.413582	44.900340
3503.501085	468772.506900	44.905345
3503.412232	468767.907147	44.910349
3503.541612	468739.291092	44.915354
3503.129330	468736.770517	44.920359
3503.278982	468733.451297	44.925364
3503.170061	468728.246289	44.930369
3503.061887	468736.781281	44.935373
3503.347644	468732.933531	44.940378
3502.984163	468741.914489	44.945383
3503.629716	468730.252533	44.950388
3503.663049	468716.152264	44.955393
3503.286281	468708.555914	44.960397
3503.744718	468700.979646	44.965402
3503.641484	468697.598990	44.970407
3503.487935	468696.406457	44.975412
3503.093898	468669.089880	44.980417
3503.274528	468659.022424	44.985421
3503.739763	468654.436466	44.990426
3503.416876	468666.148933	44.995431
3503.559969	468654.414253	45.000436
3503.508034	468634.699515	45.005441
3503.343698	468624.534466	45.010445
3503.548027	468619.381320	45.015450
3503.643936	468619.011281	45.020455
3503.329952	468608.058650	45.025460
3503.436128	468590.549759	45.030465
3503.455293	468583.042884	45.035469
3503.566096	468568.017635	45.040474
3503.369565	468579.101755	45.045479
3503.446732	468570.419562	45.050484
3503.874585	468567.411254	45.055489
3503.404446	468562.364706	45.060493
3503.474255	468541.413789	45.065498
3503.378978	468536.105173	45.070503
3503.247931	468541.956653	45.075508
3503.468614	468533.860184	45.080513
3503.373207	468523.684191	45.085517
3503.572836	468505.399925	45.090522
3503.454188	468511.452262	45.095527
3503.238423	468495.667349	45.100532
3503.539435	468493.388909	45.105537
3503.153527	468477.174557	45.110541
3503.498390	468470.478095	45.115546
3503.472683	468468.301999	45.120551
3503.605056	468456.670307	45.125556
3503.413089	468465.269357	45.130561
3503.571884	468449.678713	45.135565
3503.652758	468425.886606	45.140570
3503.318389	468431.263233	45.145575
3503.331240	468421.932016	45.150580
3503.608713	468412.913883	45.155585
3503.140664	468426.221201	45.160589
3503.364699	468425.070372	45.165594
3503.278860	468405.462182	45.170599
3503.180891	468383.979902	45.175604
3503.381179	468383.998979	45.180609
3503.099290	468397.834615	45.185613
3503.470846	468384.238386	45.190618
3503.414529	468388.252810	45.195623
3503.461632	468391.895970	45.200628
3503.564289	468357.250032	45.205633
3503.322089	468350.190007	45.210637
3503.325668	468337.818070	45.215642
3503.302487	468350.801604	45.220647
3503.576883	468336.003842	45.225652
3503.549016	468338.999728	45.230657
3503.360494	468317.379586	45.235661
3503.447406	468305.957806	45.240666
3503.473704	468300.934128	45.245671
3503.662350	468305.619683	45.250676
3503.493445	468293.832713	45.255681
3503.298056	468271.858690	45.260685
3503.020362	468266.680245	45.265690
3503.383249	468258.307679	45.270695
3503.431036	468262.812699	45.275700
3503.463316	468257.585254	45.280705
3503.463487	468262.402016	45.285709
3503.564226	468243.321910	45.290714
3503.034494	468235.850972	45.295719
3503.182666	468241.100669	45.300724
3503.602615	468218.420892	45.305729
3502.998207	468226.628909	45.310733
3503.108446	468233.659201	45.315738
3503.460754	468226.758674	45.320743
3503.381183	468222.968578	45.325748
3503.482974	468213.369696	45.330753
3503.197052	468197.240726	45.335757
3503.432865	468180.775760	45.340762
3503.137670	468190.405297	45.345767
3503.309494	468189.566926	45.350772
3503.320052	468183.075325	45.355777
3503.661497	468195.798507	45.360781
3503.584553	468170.307159	45.365786
3503.368372	468153.254479	45.370791
3503.287334	468146.625237	45.375796
3503.314284	468141.246496	45.380801
3503.091799	468146.402698	45.385805
3503.483369	468128.746903	45.390810
3503.486306	468142.030656	45.395815
3503.024552	468124.915364	45.400820
3503.471640	468109.532412	45.405825
3503.430541	468100.615204	45.410829
3503.495757	468104.661175	45.415834
3503.448893	468104.161587	45.420839
3503.382270	468104.172152	45.425844
3503.264831	468084.974280	45.430849
3503.345199	468085.367236	45.435853
3503.572518	468074.176651	45.440858
3503.529939	468075.096072	45.445863
3503.369862	468077.149535	45.450868
3503.905316	468068.698912	45.455873
3503.519930	468056.438995	45.460877
3503.512621	468036.513826	45.465882
3503.713615	468042.110147	45.470887
3503.653653	468021.584848	45.475892
3503.225072	468009.585247	45.480897
3503.242121	468004.968587	45.485901
3503.823238	467984.291213	45.490906
3503.312496	467986.653630	45.495911
3503.301307	468005.517070	45.500916
3503.705002	467968.541256	45.505921
3503.534864	467962.737293	45.510925
3503.457812	467946.270894	45.515930
3503.272894	467958.114057	45.520935
3503.302210	467951.365902	45.525940
3503.554442	467951.478177	45.530945
3503.072724	467946.889639	45.535949
3503.239506	467913.500417	45.540954
3503.458940	467909.510890	45.545959
3503.295959	467916.280256	45.550964
3503.358322	467907.245205	45.555969
3503.250309	467923.132515	45.560973
3503.269535	467912.684586	45.565978
3503.164979	467922.385519	45.570983
3503.414316	467899.985883	45.575988
3503.402648	467877.171148	45.580993
3503.213510	467880.851739	45.585997
3503.276228	467876.025017	45.591002
3503.188779	467881.007828	45.596007
3503.123259	467871.435236	45.601012
3503.324474	467872.265426	45.606017
3503.416528	467874.887498	45.611021
3503.352374	467860.396433	45.616026
3503.295149	467852.495741	45.621031
3503.500124	467844.147971	45.626036
3503.834558	467831.419215	45.631041
3503.352035	467838.492634	45.636045
3503.487307	467825.947466	45.641050
3503.321431	467810.204852	45.646055
3503.674614	467796.915370	45.651060
3503.418410	467799.998130	45.656065
3503.242921	467798.504790	45.661069
3503.591943	467793.734200	45.666074
3503.590314	467775.328999	45.671079
3503.276058	467752.764774	45.676084
3503.602185	467751.040029	45.681089
3503.016744	467758.991709	45.686093
3503.362314	467755.337142	45.691098
3503.490132	467753.136704	45.696103
3503.409905	467745.594535	45.701108
3503.437545	467717.652316	45.706113
3503.277050	467719.705879	45.711117
3503.462498	467703.603428	45.716122
3503.177248	467711.456971	45.721127
3503.251926	467719.202914	45.726132
3503.420506	467702.393271	45.731137
3503.263855	467694.508236	45.736141
3503.175283	467686.003988	45.741146
3503.347994	467674.010557	45.746151
3503.531175	467669.570378	45.751156
3503.401783	467674.813389	45.756161
3503.237392	467679.605593	45.761165
3503.419069	467674.912133	45.766170
3503.247674	467665.001253	45.771175
3503.151041	467654.470102	45.776180
3503.180829	467624.854181	45.781185
3503.304688	467630.868439	45.786189
3503.448368	467624.254214	45.791194
3503.295693	467627.117818	45.796199
3503.058257	467627.713130	45.801204
3503.146161	467627.445748	45.806209
3502.696210	467641.815491	45.811213
3503.054879	467621.477147	45.816218
3503.041480	467637.045493	45.821223
3502.532464	467637.430213	45.826228
3503.178571	467635.046428	45.831233
3503.193673	467639.708861	45.836237
3503.217302	467629.868546	45.841242
3503.354470	467644.196185	45.846247
3503.294585	467622.605695	45.851252
3503.460417	467613.756978	45.856257
3503.204954	467610.653730	45.861261
3503.360836	467600.741791	45.866266
3503.512332	467598.740412	45.871271
3503.334618	467609.162913	45.876276
3503.366284	467600.436808	45.881281
3503.114227	467591.856954	45.886285
3503.207452	467575.616869	45.891290
3503.078995	467555.710393	45.896295
3503.115587	467558.189158	45.901300
3503.378729	467560.125069	45.906305
3503.291827	467560.797996	45.911309
3503.419225	467561.132824	45.916314
3503.484318	467561.883134	45.921319
3503.315416	467558.005630	45.926324
3503.575610	467531.496829	45.931329
3503.638699	467531.486891	45.936333
3503.438086	467530.403139	45.941338
3503.358225	467524.838306	45.946343
3503.396111	467528.838004	45.951348
3503.649721	467503.445707	45.956353
3503.275720	467487.228703	45.961357
3503.392378	467482.951115	45.966362
3503.092213	467483.657755	45.971367
3503.195094	467478.418956	45.976372
3503.619684	467477.185671	45.981377
3503.378244	467488.277465	45.986381
3503.452863	467462.254252	45.991386
3503.253201	467453.716765	45.996391
3503.194413	467447.235897	46.001396
3503.417337	467444.918985	46.006401
3503.041466	467463.181397	46.011405
3503.524611	467450.124676	46.016410
3503.640060	467443.565561	46.021415
3503.374938	467431.996132	46.026420
3503.536830	467411.080234	46.031425
3503.510444	467402.971679	46.036429
3503.319350	467398.539900	46.041434
3503.086805	467414.193756	46.046439
3503.257851	467412.949840	46.051444
3503.491808	467389.487292	46.056449
3503.226101	467387.349020	46.061453
3503.259318	467372.791522	46.066458
3503.418973	467366.022576	46.071463
3502.839804	467370.170547	46.076468
3503.354595	467368.973702	46.081473
3502.835067	467361.551540	46.086477
3503.364375	467363.039757	46.091482
3503.194748	467365.956781	46.096487
3503.245633	467362.602251	46.101492
3503.305731	467345.606652	46.106497
3502.905117	467351.044730	46.111501
3502.964363	467324.263203	46.116506
3503.091197	467320.389612	46.121511
3503.070236	467326.528259	46.126516
3503.355711	467318.674605	46.131521
3503.014623	467327.906152	46.136525
3503.248046	467328.984798	46.141530
3503.045734	467322.881513	46.146535
3503.182821	467326.257109	46.151540
3503.249032	467328.477695	46.156545
3503.273586	467321.983615	46.161549
3503.283091	467333.542874	46.166554
3503.423000	467330.427792	46.171559
3503.284387	467324.010209	46.176564
3503.503633	467305.113337	46.181569
3503.516202	467285.133607	46.186573
3503.420208	467296.101102	46.191578
3503.393665	467295.192641	46.196583
3502.972751	467305.755146	46.201588
3503.567370	467291.514491	46.206593
3503.097600	467271.357465	46.211597
3503.034891	467258.792549	46.216602
3503.399700	467257.315175	46.221607
3503.122957	467255.127929	46.226612
3503.339171	467253.166992	46.231617
3502.979969	467254.085792	46.236621
3503.050516	467257.015572	46.241626
3503.340406	467263.358627	46.246631
3502.730156	467259.855061	46.251636
3503.228943	467243.347791	46.256641
3502.794417	467265.676058	46.261645
3502.716273	467264.471522	46.266650
3503.077321	467262.994743	46.271655
3503.279119	467256.928972	46.276660
3503.332238	467259.050224	46.281665
3503.431125	467271.254555	46.286669
3503.339942	467249.617923	46.291674
3503.191208	467229.105880	46.296679
3503.096464	467226.788452	46.301684
3503.265431	467223.313825	46.306689
3503.241310	467223.165557	46.311693
3503.244720	467222.759411	46.316698
3503.188905	467226.013400	46.321703
3503.437713	467232.261547	46.326708
3503.424838	467222.984568	46.331713
3503.537898	467197.259182	46.336717
3503.502975	467187.529326	46.341722
3503.236598	467187.672876	46.346727
3503.224209	467186.204416	46.351732
3503.313720	467174.325262	46.356737
3503.285381	467181.834161	46.361741
3503.323152	467184.109962	46.366746
3503.438359	467167.156213	46.371751
3503.400564	467146.271616	46.376756
3503.624882	467145.323496	46.381761
3503.544649	467144.119283	46.386765
3503.530613	467135.653735	46.391770
3503.682843	467125.894267	46.396775
3503.210346	467118.413878	46.401780
3503.690125	467095.267084	46.406785
3503.513564	467104.574132	46.411789
3503.565177	467101.067329	46.416794
3503.683326	467075.543812	46.421799
3503.209214	467070.193294	46.426804
3503.326653	467061.250584	46.431809
3503.350815	467070.221686	46.436813
3503.277314	467055.021664	46.441818
3503.545058	467048.083414	46.446823
3503.255663	467040.066998	46.451828
3503.521831	467022.227274	46.456833
3503.229052	467023.135584	46.461837
3502.895029	467019.131963	46.466842
3503.551783	467013.906910	46.471847
3503.405310	467014.335743	46.476852
3503.147497	467015.745583	46.481857
3503.165294	467014.424456	46.486861
3503.268050	466991.337143	46.491866
3503.025646	466989.651499	46.496871
3502.885630	466984.096031	46.501876
3503.383719	466980.670752	46.506881
3503.448326	466984.057861	46.511885
3503.175451	466982.022091	46.516890
3503.357320	466985.897722	46.521895
3503.285559	466985.148513	46.526900
3503.286125	466978.607413	46.531905
3503.250398	466988.450014	46.536909
3503.136530	466959.413628	46.541914
3503.103415	466945.677612	46.546919
3503.196454	466948.705291	46.551924
3503.378893	466933.363314	46.556929
3503.372092	466941.781600	46.561933
3503.251039	466938.504887	46.566938
3503.252824	466941.192050	46.571943
3503.284731	466925.772450	46.576948
3503.249162	466935.057286	46.581953
3503.177176	466933.699640	46.586957
3503.458720	466912.815040	46.591962
3503.403279	466901.262880	46.596967
3502.922753	466911.327944	46.601972
3503.387129	466900.758441	46.606977
3503.342689	466899.751381	46.611981
3503.477488	466910.074124	46.616986
3503.706458	466902.077129	46.621991
3503.242472	466880.752577	46.626996
3503.277104	466863.101435	46.632001
3503.289107	466866.446172	46.637005
3503.268544	466858.691429	46.642010
3503.442804	466851.311536	46.647015
3503.005478	466866.491108	46.652020
3503.508065	466860.681914	46.657025
3503.301549	466864.111898	46.662029
3503.385353	466844.424726	46.667034
3503.435537	466823.779432	46.672039
3503.190891	466833.401599	46.677044
3503.411046	466817.242277	46.682049
3503.136498	466826.919879	46.687053
3503.210087	466829.037940	46.692058
3503.510673	466816.009684	46.697063
3503.318141	466813.758374	46.702068
3503.585984	466782.937396	46.707073
3503.410500	466776.373355	46.712077
3503.301959	466794.644796	46.717082
3503.365611	466790.933214	46.722087
3503.294913	466788.256993	46.727092
3503.492991	466766.624847	46.732097
3503.166032	466758.563555	46.737101
3503.018667	466756.862869	46.742106
3503.124639	466743.459680	46.747111
3502.877002	466745.273581	46.752116
3503.331906	466747.787732	46.757121
3503.305201	466742.062171	46.762125
3503.134635	466747.666864	46.767130
3503.376069	466741.036910	46.772135
3503.126656	466755.984032	46.777140
3503.467030	466741.529664	46.782145
3503.523906	466730.365307	46.787149
3503.215470	466713.224626	46.792154
3503.611629	466700.637550	46.797159
3503.180581	466720.227695	46.802164
3503.387473	466698.847618	46.807169
3503.373874	466712.185596	46.812173
3503.109116	466690.575826	46.817178
3503.524198	466678.746343	46.822183
3503.171230	466670.537009	46.827188
3503.392088	466661.222836	46.832193
3503.237936	466679.298760	46.837197
3503.160540	466665.569562	46.842202
3503.140882	466672.265965	46.847207
3503.195765	466673.930639	46.852212
3503.624832	466672.240242	46.857217
3503.360865	466660.822325	46.862221
3503.000082	466630.911797	46.867226
3503.387666	466628.467355	46.872231
3503.313329	466630.355285	46.877236
3503.546540	466626.059099	46.882241
3503.328433	466632.178404	46.887245
3503.009516	466637.248804	46.892250
3503.640452	466615.446669	46.897255
3503.312721	466611.087028	46.902260
3503.248233	466606.280122	46.907265
3503.140752	466590.983723	46.912269
3503.122609	466595.702349	46.917274
3503.117015	466599.759804	46.922279
3503.088774	466592.563950	46.927284
3503.428051	466587.997457	46.932289
3503.785902	466593.265131	46.937293
3503.279928	466575.749909	46.942298
3503.389995	466552.660960	46.947303
3503.208377	466557.608263	46.952308
3503.160816	466553.102910	46.957313
3503.049246	466549.064035	46.962317
3503.131087	466545.958016	46.967322
3503.370552	466545.159596	46.972327
3503.080704	466556.817307	46.977332
3503.293879	466551.865085	46.982337
3503.167771	466548.335576	46.987341
3502.830381	466545.955014	46.992346
3503.199073	466543.969910	46.997351
3503.275065	466532.954547	47.002356
3503.035201	466523.307485	47.007361
3503.097376	466517.719934	47.012365
3503.007699	466520.066661	47.017370
3503.147363	466510.359601	47.022375
3503.130602	466519.945888	47.027380
3503.668910	466519.505884	47.032385
3503.573465	466507.807711	47.037389
3503.304262	466519.512886	47.042394
3503.447730	466507.523413	47.047399
3503.203668	466493.161257	47.052404
3502.966479	466474.082255	47.057409
3503.258189	466479.563241	47.062413
3503.374975	466472.243008	47.067418
3503.514427	466474.249279	47.072423
3503.043824	466479.090158	47.077428
3503.543107	466477.337941	47.082433
3503.409355	466480.959313	47.087437
3502.977886	466454.355661	47.092442
3503.166167	466445.350785	47.097447
3503.379374	466433.705197	47.102452
3503.563313	466439.507471	47.107457
3503.130966	466437.648977	47.112461
3503.188634	466444.586765	47.117466
3503.354249	466434.165669	47.122471
3503.159115	466428.263818	47.127476
3503.490807	466422.532225	47.132481
3503.755209	466399.773663	47.137485
3503.038524	466405.008408	47.142490
3503.029171	466391.978176	47.147495
3503.481556	466382.170918	47.152500
3503.297922	466380.678763	47.157505
3503.176057	466387.492827	47.162509
3503.309896	466387.877363	47.167514
3503.414196	466374.474204	47.172519
3503.223417	466366.086992	47.177524
3503.107325	466347.698635	47.182529
3503.153402	466349.415434	47.187533
3503.097997	466352.365250	47.192538
3503.075242	466347.298151	47.197543
3502.868936	466359.906203	47.202548
3503.004209	466346.092473	47.207553
3503.085746	466353.888542	47.212557
3502.831278	466352.762532	47.217562
3503.249445	466354.927588	47.222567
3502.906793	466358.936953	47.227572
3503.132917	466355.250320	47.232577
3503.304618	466359.026259	47.237581
3503.040789	466360.690629	47.242586
3503.260343	466352.086429	47.247591
3503.097147	466365.194736	47.252596
3502.975200	466345.235377	47.257601
3503.210463	466360.613239	47.262605
3502.958585	466333.727511	47.267610
3503.444762	466319.554052	47.272615
3503.029645	466316.273017	47.277620
3503.125487	466314.736680	47.282625
3503.455730	466321.327179	47.287629
3503.276313	466313.445223	47.292634
3503.451302	466312.555571	47.297639
3503.346788	466313.332737	47.302644
3503.309836	466319.017838	47.307649
3503.344011	466290.667032	47.312653
3503.339116	466289.552277	47.317658
3503.742650	466279.397742	47.322663
3503.290076	466285.402087	47.327668
3503.273816	466278.407062	47.332673
3503.158070	466273.101108	47.337677
3503.324693	466274.443906	47.342682
3503.428751	466262.359109	47.347687
3503.475996	466247.747909	47.352692
3503.277595	466224.960899	47.357697
3503.064153	466237.620859	47.362701
3503.166410	466237.756853	47.367706
3503.666248	466222.820556	47.372711
3503.462706	466228.075647	47.377716
3503.253620	466211.983712	47.382721
3503.524532	466203.726286	47.387725
3503.336767	466205.327938	47.392730
3503.579224	466195.249531	47.397735
3503.478970	466205.711189	47.402740
3503.551985	466188.763324	47.407745
3503.518531	466180.604708	47.412749
3502.949278	466163.403390	47.417754
3503.519943	466146.528950	47.422759
3503.152021	466162.560088	47.427764
3503.391649	466157.400761	47.432769
3503.965696	466143.314711	47.437773
3503.531028	466131.365703	47.442778
3503.392184	466122.767353	47.447783
3503.042222	466117.599798	47.452788
3503.483341	466110.938083	47.457793
3503.718976	466121.955183	47.462797
3503.235413	466094.852233	47.467802
3503.695003	466073.178041	47.472807
3503.078193	466072.971326	47.477812
3503.243255	466073.198809	47.482817
3503.249627	466075.581110	47.487821
3502.919456	466081.566164	47.492826
3502.913953	466078.524592	47.497831
3503.138484	466071.237897	47.502836
3503.413391	466078.445715	47.507841
3503.302439	466067.459660	47.512845
3503.481420	466050.393517	47.517850
3503.343398	466030.740650	47.522855
3503.390259	466033.167264	47.527860
3503.390524	466034.992746	47.532865
3503.674618	466028.913615	47.537869
3503.328963	466019.435169	47.542874
3503.272416	466002.913298	47.547879
3503.126381	466000.147469	47.552884
3503.265631	465986.637124	47.557889
3503.234506	465998.051413	47.562893
3503.059640	466001.628658	47.567898
3503.341915	465992.608732	47.572903
3503.017525	465998.694312	47.577908
3502.708323	465998.540389	47.582913
3503.214133	465992.274076	47.587917
3502.957596	465997.131935	47.592922
3503.737140	465985.599412	47.597927
3503.222741	465981.167730	47.602932
3503.588395	465960.370310	47.607937
3503.211344	465957.640992	47.612941
3503.406573	465952.032260	47.617946
3503.670705	465955.945786	47.622951
3503.101935	465956.999182	47.627956
3503.591453	465942.824944	47.632961
3503.270914	465924.722077	47.637965
3503.233151	465923.409664	47.642970
3503.245697	465909.158673	47.647975
3503.052657	465923.184722	47.652980
3503.240423	465919.706910	47.657985
3503.411258	465911.820149	47.662989
3503.150833	465910.542931	47.667994
3503.438923	465909.483260	47.672999
3503.299498	465897.335326	47.678004
3503.118948	465879.463834	47.683009
3503.621894	465880.702786	47.688013
3502.830308	465878.546068	47.693018
3503.323809	465883.336103	47.698023
3503.470515	465883.211530	47.703028
3503.369064	465878.714552	47.708033
3503.393374	465873.538483	47.713037
3503.018008	465864.774582	47.718042
3503.221883	465835.939966	47.723047
3503.190778	465834.981455	47.728052
3503.055742	465837.386135	47.733057
3503.064631	465837.536890	47.738061
3503.072880	465843.722059	47.743066
3503.026554	465833.232752	47.748071
3503.054831	465829.323759	47.753076
3503.289287	465839.276314	47.758081
3503.507564	465829.759350	47.763085
3502.873918	465847.151150	47.768090
3503.297576	465830.553240	47.773095
3503.297678	465836.739699	47.778100
3503.376385	465825.723539	47.783105
3503.327518	465807.374794	47.788109
3503.018778	465812.849450	47.793114
3503.450910	465794.171119	47.798119
3503.355512	465794.744028	47.803124
3503.129210	465800.307073	47.808129
3503.543022	465787.868791	47.813133
3503.234262	465804.448642	47.818138
3503.270841	465786.694876	47.823143
3503.249455	465775.440969	47.828148
3503.387292	465763.756217	47.833153
3503.741957	465752.645690	47.838157
3503.204468	465762.314633	47.843162
3503.306485	465744.144818	47.848167
3503.286214	465761.896110	47.853172
3503.318575	465743.889431	47.858177
3503.635110	465721.882532	47.863181
3503.015239	465725.682291	47.868186
3503.458580	465701.728393	47.873191
3503.293113	465714.482500	47.878196
3503.206441	465702.782494	47.883201
3503.051399	465717.461887	47.888205
3503.035589	465711.683615	47.893210
3503.127490	465707.257455	47.898215
3503.199889	465713.077560	47.903220
3502.942792	465709.923578	47.908225
3503.579502	465693.291883	47.913229
3503.258385	465684.925002	47.918234
3503.655372	465670.765209	47.923239
3503.341797	465664.577612	47.928244
3503.298938	465670.669492	47.933249
3503.354481	465663.105116	47.938253
3503.277215	465662.153894	47.943258
3503.206301	465634.173783	47.948263
3503.321361	465631.366634	47.953268
3503.184696	465632.757414	47.958273
3503.430569	465622.881032	47.963277
3503.104530	465632.415191	47.968282
3503.149475	465629.517707	47.973287
3503.169272	465624.849382	47.978292
3503.070482	465634.043365	47.983297
3503.310612	465634.766077	47.988301
3503.392782	465628.313078	47.993306
3503.238655	465597.303529	47.998311
3503.254870	465599.329364	48.003316
3502.921775	465588.226047	48.008321
3503.445000	465587.534866	48.013325
3502.958750	465592.986928	48.018330
3503.248378	465590.862108	48.023335
3503.163299	465582.762131	48.028340
3503.107417	465578.207176	48.033345
3503.306857	465588.368220	48.038349
3503.061180	465586.581560	48.043354
3503.380444	465583.539290	48.048359
3503.104934	465571.260552	48.053364
3503.172089	465573.633301	48.058369
3503.354110	465558.290393	48.063373
3503.165320	465557.965305	48.068378
3503.190131	465561.206806	48.073383
3503.265036	465559.115923	48.078388
3503.207140	465554.764118	48.083393
3503.143454	465567.096551	48.088397
3502.856968	465559.738330	48.093402
3503.136396	465556.296680	48.098407
3503.548415	465556.383714	48.103412
3502.774436	465561.729138	48.108417
3503.253347	465558.560210	48.113421
3503.228575	465549.588631	48.118426
3502.984587	465530.053468	48.123431
3502.847070	465524.192965	48.128436
3503.200396	465505.932512	48.133441
3503.243473	465515.357668	48.138445
3503.017549	465520.667180	48.143450
3503.603175	465514.033146	48.148455
3502.878407	465526.774356	48.153460
3503.083261	465528.415414	48.158465
3503.216417	465509.581256	48.163469
3503.245601	465517.588746	48.168474
3503.300838	465515.551677	48.173479
3503.020985	465525.991351	48.178484
3503.455932	465524.249227	48.183489
3503.302307	465500.389464	48.188493
3503.189795	465504.109064	48.193498
3503.070284	465480.142467	48.198503
3502.989616	465480.865184	48.203508
3503.128112	465484.950785	48.208513
3503.511114	465476.472522	48.213517
3503.042745	465489.325353	48.218522
3503.272966	465481.327625	48.223527
3503.083323	465482.929627	48.228532
3503.416470	465483.536223	48.233537
3503.241266	465482.245508	48.238541
3503.253102	465468.754974	48.243546
3503.206448	465452.433948	48.248551
3503.405706	465445.151034	48.253556
3503.164491	465450.209433	48.258561
3502.992304	465432.640499	48.263565
3502.814234	465441.390711	48.268570
3503.231256	465433.262019	48.273575
3502.975530	465446.385521	48.278580
3503.099403	465435.919823	48.283585
3503.221206	465440.616586	48.288589
3502.895190	465444.420654	48.293594
3503.106556	465451.385183	48.298599
3503.272090	465455.010131	48.303604
3502.927306	465453.391254	48.308609
3503.039813	465454.134146	48.313613
3502.803650	465455.337828	48.318618
3502.844363	465455.686392	48.323623
3502.866373	465453.046057	48.328628
3502.854099	465453.301578	48.333633
3503.107965	465453.464322	48.338637
3502.886557	465454.462834	48.343642
3503.390136	465448.095296	48.348647
3503.301752	465444.052544	48.353652
3503.009788	465442.780283	48.358657
3503.275025	465451.663256	48.363661
3503.197758	465434.890670	48.368666
3503.273668	465422.099911	48.373671
3503.271389	465411.958400	48.378676
3503.180371	465418.869318	48.383681
3503.617647	465410.433159	48.388685
3503.448290	465427.498364	48.393690
3503.191847	465422.721530	48.398695
3503.292885	465421.539275	48.403700
3503.257623	465392.386890	48.408705
3503.336631	465388.824764	48.413709
3503.405894	465381.359538	48.418714
3503.332163	465370.620786	48.423719
3503.353402	465378.325327	48.428724
3503.349233	465370.415318	48.433729
3503.557702	465366.579176	48.438733
3502.963602	465343.042410	48.443738
3502.969342	465342.585149	48.448743
3503.112507	465324.408471	48.453748
3503.396644	465331.868633	48.458753
3503.197265	465327.336307	48.463757
3503.274297	465337.212563	48.468762
3503.353287	465326.398938	48.473767
3503.316803	465332.642037	48.478772
3503.106882	465342.817197	48.483777
3503.374753	465332.835785	48.488781
3502.843801	465317.098305	48.493786
3503.055452	465305.908731	48.498791
3502.932620	465311.658388	48.503796
3503.027139	465320.669821	48.508801
3503.283538	465303.388001	48.513805
3503.178913	465306.548581	48.518810
3503.571348	465290.107313	48.523815
3503.247570	465302.227464	48.528820
3503.363643	465296.935330	48.533825
3503.549972	465293.102675	48.538829
3503.059388	465296.577814	48.543834
3503.072755	465289.628489	48.548839
3503.288790	465273.062963	48.553844
3503.442929	465259.144123	48.558849
3503.237961	465253.902725	48.563853
3503.058573	465268.129888	48.568858
3502.938027	465260.288944	48.573863
3503.025474	465273.054047	48.578868
3503.281576	465260.336127	48.583873
3503.285061	465258.865023	48.588877
3503.181450	465259.540664	48.593882
3503.268141	465259.526995	48.598887
3503.331791	465250.439894	48.603892
3503.352073	465229.848482	48.608897
3503.304654	465209.622721	48.613901
3502.953083	465218.603291	48.618906
3503.235004	465204.106406	48.623911
3503.652779	465220.470449	48.628916
3503.186930	465211.467028	48.633921
3503.487375	465203.711647	48.638925
3503.221492	465213.236484	48.643930
3503.068410	465199.315457	48.648935
3503.098320	465183.438512	48.653940
3503.030698	465171.988753	48.658945
3503.234969	465172.615730	48.663949
3503.212588	465186.919549	48.668954
3503.545613	465167.140712	48.673959
3503.375988	465168.790283	48.678964
3503.179112	465175.971564	48.683969
3503.662721	465171.381954	48.688973
3503.357575	465158.752690	48.693978
3503.476535	465133.581673	48.698983
3503.418042	465132.982431	48.703988
3503.136879	465133.381880	48.708993
3503.453045	465136.932363	48.713997
3503.373575	465134.257318	48.719002
3503.565644	465130.271596	48.724007
3503.334783	465109.516925	48.729012
3503.082511	465111.078143	48.734017
3503.352362	465100.944178	48.739021
3503.372394	465095.920727	48.744026
3503.264363	465088.736975	48.749031
3503.207038	465098.076766	48.754036
3503.568610	465080.930272	48.759041
3503.246231	465065.616029	48.764045
3503.420093	465062.951642	48.769050
3503.489979	465050.110900	48.774055
3503.156117	465046.816821	48.779060
3503.145217	465059.546888	48.784065
3503.657949	465049.120955	48.789069
3503.462277	465046.565688	48.794074
3503.477826	465022.070121	48.799079
3503.237879	465022.361636	48.804084
3503.376450	465018.739323	48.809089
3503.510718	465007.713956	48.814093
3503.187170	465008.728633	48.819098
3503.308705	465004.652616	48.824103
3503.536789	464996.097229	48.829108
3503.123241	464980.949468	48.834113
3503.003279	464966.211683	48.839117
3503.114830	464970.301643	48.844122
3503.271040	464964.952372	48.849127
3503.244272	464971.346174	48.854132
3503.134557	464976.840294	48.859137
3503.202620	464966.129635	48.864141
3502.994474	464972.349263	48.869146
3502.948288	464980.318160	48.874151
3503.218245	464972.871777	48.879156
3503.179780	464971.356574	48.884161
3503.096315	464970.304879	48.889165
3503.087529	464982.679684	48.894170
3503.105874	464977.047945	48.899175
3502.741619	464964.427908	48.904180
3502.893495	464972.923316	48.909185
3503.357268	464967.373298	48.914189
3502.945427	464950.906769	48.919194
3503.166306	464951.683259	48.924199
3503.355657	464942.322603	48.929204
3503.364940	464949.471372	48.934209
3503.026107	464946.431616	48.939213
3503.196058	464943.362147	48.944218
3503.150320	464937.994081	48.949223
3502.991228	464935.078043	48.954228
3503.283881	464939.443647	48.959233
3503.414812	464948.348061	48.964237
3503.202078	464954.872684	48.969242
3502.752630	464931.464727	48.974247
3503.130352	464945.857596	48.979252
3502.991148	464947.299532	48.984257
3503.476183	464928.206395	48.989261
3503.311043	464907.238295	48.994266
3503.139736	464895.297668	48.999271
3503.100049	464904.178359	49.004276
3503.146890	464909.799882	49.009281
3503.404592	464893.075342	49.014285
3503.073748	464911.789231	49.019290
3503.184813	464901.426717	49.024295
3503.379352	464900.026810	49.029300
3503.240555	464895.789080	49.034305
3503.669723	464866.410429	49.039309
3503.379155	464863.971561	49.044314
3503.454648	464859.091421	49.049319
3503.250391	464853.089149	49.054324
3503.233809	464851.012658	49.059329
3503.586196	464843.350357	49.064333
3502.879276	464833.167820	49.069338
3503.242556	464826.720853	49.074343
3503.668072	464814.584420	49.079348
3503.424294	464818.781287	49.084353
3503.259860	464810.034316	49.089357
3503.119041	464805.695465	49.094362
3503.324162	464808.198626	49.099367
3503.196082	464814.304222	49.104372
3503.208515	464804.971471	49.109377
3503.243394	464775.553598	49.114381
3503.232239	464777.279572	49.119386
3503.330230	464780.712468	49.124391
3503.327763	464767.375883	49.129396
3503.365478	464766.254312	49.134401
3503.441251	464773.291208	49.139405
3503.369869	464769.752751	49.144410
3503.056183	464760.572952	49.149415
3503.100510	464748.801003	49.154420
3502.965684	464734.116118	49.159425
3503.206518	464724.595095	49.164429
3502.727958	464736.435766	49.169434
3503.051887	464721.576935	49.174439
3503.237909	464723.271746	49.179444
3502.934832	464730.926363	49.184449
3503.029714	464728.629397	49.189453
3503.000836	464731.575244	49.194458
3503.302406	464733.505344	49.199463
3503.459308	464730.590041	49.204468
3503.128286	464743.878010	49.209473
3503.313555	464730.258171	49.214477
3503.320602	464742.377056	49.219482
3503.090612	464745.303980	49.224487
3503.210065	464734.889348	49.229492
3503.427921	464710.817844	49.234497
3503.423108	464703.566935	49.239501
3503.126761	464699.759759	49.244506
3502.868704	464689.201933	49.249511
3503.462223	464682.312839	49.254516
3502.551621	464693.410446	49.259521
3503.163257	464689.764011	49.264525
3503.233858	464688.180836	49.269530
3503.028589	464692.574486	49.274535
3503.282199	464697.554846	49.279540
3503.271763	464689.645574	49.284545
3503.280064	464701.764285	49.289549
3503.236997	464682.855828	49.294554
3503.133264	464656.502377	49.299559
3503.442959	464654.982829	49.304564
3503.298074	464648.261155	49.309569
3503.368559	464646.221594	49.314573
3503.276154	464661.246794	49.319578
3503.205765	464651.774933	49.324583
3503.408283	464649.359522	49.329588
3503.003069	464647.851556	49.334593
3503.014124	464621.936321	49.339597
3503.095063	464625.574783	49.344602
3503.242716	464605.976862	49.349607
3503.494278	464612.478910	49.354612
3503.061405	464622.182542	49.359617
3503.293672	464615.198395	49.364621
3503.480266	464620.138655	49.369626
3503.226290	464621.750890	49.374631
3503.229536	464609.883934	49.379636
3503.392481	464611.734535	49.384641
3503.441046	464582.466367	49.389645
3503.231723	464571.799356	49.394650
3503.493836	464570.540881	49.399655
3503.294285	464563.422129	49.404660
3503.138374	464570.242157	49.409665
3503.317979	464563.621298	49.414669
3503.494267	464565.824776	49.419674
3503.363077	464550.378516	49.424679
3503.420595	464547.732456	49.429684
3503.276654	464533.251720	49.434689
3503.518207	464531.185107	49.439693
3503.445793	464532.058685	49.444698
3503.457611	464520.494595	49.449703
3503.475948	464498.736415	49.454708
3503.034862	464492.720765	49.459713
3503.310565	464486.693233	49.464717
3503.298139	464489.078684	49.469722
3503.315840	464492.017201	49.474727
3503.532340	464486.455433	49.479732
3503.297438	464487.963239	49.484737
3503.503491	464477.027675	49.489741
3503.368786	464458.995605	49.494746
3503.128728	464453.759556	49.499751
3503.416208	464444.129611	49.504756
3503.168497	464454.919710	49.509761
3503.354940	464452.811089	49.514765
3503.248584	464449.734513	49.519770
3503.188465	464438.942427	49.524775
3503.122551	464409.083574	49.529780
3502.810952	464410.349949	49.534785
3503.113139	464397.421383	49.539789
3503.160798	464402.434367	49.544794
3502.823287	464407.203963	49.549799
3502.963460	464404.950515	49.554804
3502.936087	464398.970866	49.559809
3503.156887	464395.436873	49.564813
3503.239327	464401.864295	49.569818
3502.730697	464415.281966	49.574823
3503.138171	464412.124164	49.579828
3503.077751	464400.520715	49.584833
3503.235094	464406.429176	49.589837
3503.130700	464405.127201	49.594842
3503.183244	464397.360002	49.599847
3503.348297	464405.194298	49.604852
3503.039031	464403.873996	49.609857
3503.449446	464401.324271	49.614861
3503.072127	464401.536084	49.619866
3503.279315	464399.322754	49.624871
3503.112092	464382.462134	49.629876
3502.989968	464374.164704	49.634881
3503.137397	464352.690241	49.639885
3502.869331	464366.475614	49.644890
3503.064049	464367.966230	49.649895
3503.011970	464354.485092	49.654900
3502.713297	464370.658767	49.659905
3502.804466	464363.544706	49.664909
3502.966770	464378.073435	49.669914
3503.014897	464383.644182	49.674919
3503.407772	464376.026027	49.679924
3503.162628	464369.320113	49.684929
3503.510530	464367.185961	49.689933
3503.067892	464360.359126	49.694938
3503.213847	464374.028337	49.699943
3503.183639	464354.306164	49.704948
3503.252281	464372.145986	49.709953
3503.500393	464369.317640	49.714957
3503.240596	464369.308028	49.719962
3503.110212	464342.197722	49.724967
3503.220112	464335.182115	49.729972
3503.151820	464326.014051	49.734977
3503.242891	464323.159810	49.739981
3503.142920	464327.181905	49.744986
3502.918666	464317.937066	49.749991
3503.212805	464315.304286	49.754996
3503.142320	464318.003206	49.760001
3503.060713	464321.413854	49.765005
3503.219835	464327.474191	49.770010
3503.332204	464316.401218	49.775015
3503.439939	464318.361996	49.780020
3503.083842	464311.420041	49.785025
3503.189544	464299.688854	49.790029
3502.960783	464293.791722	49.795034
3503.102717	464301.528287	49.800039
3503.399131	464296.714521	49.805044
3502.986652	464299.568926	49.810049
3503.183464	464297.255802	49.815053
3502.994324	464298.097129	49.820058
3503.051247	464296.668224	49.825063
3503.179720	464290.308925	49.830068
3502.901921	464303.335193	49.835073
3503.087082	464296.206253	49.840077
3503.156470	464296.144606	49.845082
3502.880290	464295.326189	49.850087
3503.151239	464296.500487	49.855092
3503.090961	464302.088391	49.860097
3503.037979	464296.619883	49.865101
3502.899385	464298.721025	49.870106
3503.204633	464298.875658	49.875111
3503.123337	464300.866318	49.880116
3502.801330	464307.459123	49.885121
3503.281798	464307.941044	49.890125
3503.159174	464297.868737	49.895130
3503.073642	464276.532447	49.900135
3503.090367	464262.279691	49.905140
3503.167838	464258.514771	49.910145
3502.964268	464260.017640	49.915149
3502.961360	464260.322408	49.920154
3502.875319	464261.908123	49.925159
3503.267625	464247.241004	49.930164
3503.057278	464249.201356	49.935169
3503.122264	464256.442977	49.940173
3503.126175	464255.276010	49.945178
3502.851741	464254.660165	49.950183
3503.120413	464252.639950	49.955188
3503.250162	464263.015494	49.960193
3503.190951	464254.961634	49.965197
3503.163361	464272.411053	49.970202
3503.028951	464268.172504	49.975207
3503.084672	464258.122699	49.980212
3503.049287	464275.674772	49.985217
3503.219873	464272.909380	49.990221
3503.214672	464253.588859	49.995226
3503.481356	464251.416822	50.000231
3503.502716	464230.773561	50.005236
3503.356071	464221.972824	50.010241
3503.399766	464223.183049	50.015245
3503.372872	464214.261955	50.020250
3503.520895	464232.393620	50.025255
3503.708186	464195.141152	50.030260
3503.256302	464192.829131	50.035265
3503.151047	464176.059977	50.040269
3503.478887	464184.071473	50.045274
3503.221123	464172.752657	50.050279
3503.253408	464171.631914	50.055284
3503.049201	464175.366239	50.060289
3503.271202	464173.809807	50.065293
3503.014720	464151.689014	50.070298
3503.079170	464143.919840	50.075303
3503.141681	464136.556671	50.080308
3502.950944	464145.512267	50.085313
3503.178784	464137.007288	50.090317
3503.414626	464138.846408	50.095322
3503.147303	464137.265896	50.100327
3503.148922	464123.116860	50.105332
3503.114774	464132.149135	50.110337
3503.224122	464125.336397	50.115341
3502.984300	464134.299756	50.120346
3503.068755	464139.256274	50.125351
3503.470329	464130.165991	50.130356
3503.136937	464141.984043	50.135361
3503.218157	464108.805196	50.140365
3503.414710	464105.934253	50.145370
3503.320724	464099.305785	50.150375
3503.315799	464095.705999	50.155380
3503.225573	464103.631471	50.160385
3503.338936	464101.179378	50.165389
3503.279669	464105.550069	50.170394
3503.033959	464105.081816	50.175399
3503.379390	464093.718324	50.180404
3503.560559	464085.677116	50.185409
3503.467785	464062.972514	50.190413
3503.091092	464064.452049	50.195418
3503.211426	464058.398244	50.200423
3503.205556	464062.557653	50.205428
3503.296978	464061.072566	50.210433
3503.469963	464056.886810	50.215437
3503.148733	464040.151689	50.220442
3502.993326	464029.120894	50.225447
3503.204492	464010.120941	50.230452
3502.959970	464024.308516	50.235457
3502.962210	464015.230595	50.240461
3503.045711	464020.998696	50.245466
3502.875801	464017.069985	50.250471
3503.050143	464018.107431	50.255476
3502.894456	464018.892768	50.260481
3503.056037	464006.036904	50.265485
3503.267052	464019.543920	50.270490
3503.188509	464017.679994	50.275495
3503.254682	464007.932697	50.280500
3503.056651	464009.586846	50.285505
3503.157527	464019.409232	50.290509
3503.488678	464017.024129	50.295514
3503.020420	464020.850933	50.300519
3503.198390	464011.643807	50.305524
3503.091067	464023.324764	50.310529
3503.207600	464009.106776	50.315533
3503.113981	463995.276988	50.320538
3502.636643	463983.434937	50.325543
3503.205258	463980.099462	50.330548
3503.177848	463977.973885	50.335553
3502.959701	463985.108214	50.340557
3502.917783	463985.976995	50.345562
3502.947113	463982.371774	50.350567
3503.258163	463978.164179	50.355572
3503.320472	463988.195526	50.360577
3503.177237	463978.024900	50.365581
3503.266395	463984.400673	50.370586
3503.089815	463982.349389	50.375591
3503.286023	463982.216983	50.380596
3503.169454	463990.501651	50.385601
3503.024567	463978.404195	50.390605
3503.226194	463980.502302	50.395610
3503.045322	463984.638676	50.400615
3503.421051	463977.682358	50.405620
3503.139126	463950.443369	50.410625
3503.148541	463936.191552	50.415629
3503.282490	463940.836013	50.420634
3502.971876	463943.775790	50.425639
3503.052075	463935.243355	50.430644
3502.991088	463946.967742	50.435649
3503.134154	463943.496676	50.440653
3503.495184	463930.964232	50.445658
3503.232073	463928.064498	50.450663
3503.447600	463933.152484	50.455668
3502.982597	463933.631726	50.460673
3503.267182	463910.664461	50.465677
3503.416929	463893.905490	50.470682
3503.109924	463904.350247	50.475687
3503.092744	463898.115281	50.480692
3503.050228	463896.093510	50.485697
3503.241180	463896.012647	50.490701
3503.385969	463898.474739	50.495706
3503.277864	463891.087742	50.500711
3503.443584	463891.264433	50.505716
3503.458543	463895.826287	50.510721
3503.288693	463866.490236	50.515725
3503.179979	463858.444052	50.520730
3503.094194	463847.300731	50.525735
3503.367212	463827.935847	50.530740
3503.108464	463792.477436	50.535745
3502.997567	463739.955859	50.540749
3503.176836	463688.909696	50.545754
3502.839411	463629.628028	50.550759
3502.767915	463547.787168	50.555764
3502.186644	463482.356531	50.560769
3502.312216	463384.508940	50.565773
3502.377371	463282.004711	50.570778
3501.865492	463177.258322	50.575783
3501.851942	463069.643319	50.580788
3501.437450	462949.615174	50.585793
3501.166339	462819.927714	50.590797
3501.252813	462676.895354	50.595802
3500.743721	462537.557047	50.600807
3500.941498	462372.392729	50.605812
3500.386803	462230.320940	50.610817
3499.905878	462049.894156	50.615821
3499.473665	461882.999848	50.620826
3499.062101	461714.883748	50.625831
3498.812184	461524.931745	50.630836
3498.406975	461349.406867	50.635841
3497.813950	461144.239296	50.640845
3498.062244	460957.906107	50.645850
3497.370805	460755.032819	50.650855
3496.876999	460544.467526	50.655860
3496.327869	460330.713486	50.660865
3496.016898	460120.318079	50.665869
3495.716088	459897.694913	50.670874
3495.025013	459675.942740	50.675879
3494.509396	459445.283960	50.680884
3494.194801	459216.975009	50.685889
3493.634097	458985.659108	50.690893
3493.601620	458747.257197	50.695898
3493.272855	458507.834300	50.700903
3492.989422	458243.393560	50.705908
3492.012933	457990.574221	50.710913
3491.395437	457719.078237	50.715917
3491.380087	457457.578640	50.720922
3490.680784	457202.778811	50.725927
3489.823608	456921.723211	50.730932
3489.212678	456655.489019	50.735937
3489.061770	456395.621707	50.740941
3488.673917	456110.017376	50.745946
3487.959831	455850.435664	50.750951
3487.783151	455556.217195	50.755956
3486.915351	455278.643111	50.760961
3486.397775	454976.353621	50.765965
3486.130373	454679.753511	50.770970
3485.277735	454394.099320	50.775975
3484.677602	454091.303641	50.780980
3483.937227	453805.472042	50.785985
3483.523490	453492.998959	50.790989
3483.204872	453190.806305	50.795994
3482.006250	452892.503388	50.800999
3481.707578	452593.952811	50.806004
3481.064359	452284.340769	50.811009
3480.249500	451982.007550	50.816013
3479.813201	451681.284946	50.821018
3479.002933	451391.628482	50.826023
3478.693371	451065.303878	50.831028
3478.032285	450756.536622	50.836033
3477.176831	450441.402218	50.841037
3476.534222	450137.241433	50.846042
3476.063999	449824.676427	50.851047
3475.478260	449511.871730	50.856052
3474.339135	449196.004003	50.861057
3473.606352	448888.035069	50.866061
3473.415739	448571.653682	50.871066
3472.717492	448263.569535	50.876071
3471.926054	447950.218124	50.881076
3471.126899	447631.484233	50.886081
3470.474693	447312.824278	50.891085
3469.960255	447012.256464	50.896090
3469.161102	446702.086935	50.901095
3468.493095	446375.753226	50.906100
3467.922476	446054.982489	50.911105
3467.117738	445743.177136	50.916109
3466.587016	445431.882664	50.921114
3465.754374	445119.667488	50.926119
3465.192793	444809.587874	50.931124
3464.564316	444490.784640	50.936129
3463.938411	444181.062323	50.941133
3463.331932	443857.729756	50.946138
3462.432062	443550.935811	50.951143
3462.012725	443223.707450	50.956148
3461.481094	442908.776341	50.961153
3460.924006	442596.992310	50.966157
3460.325145	442265.312374	50.971162
3459.456747	441949.152957	50.976167
3458.842240	441622.847482	50.981172
3458.431297	441305.389052	50.986177
3457.405530	440975.586466	50.991181
3456.938921	440640.309947	50.996186
3456.032964	440321.952444	51.001191
3455.311755	440007.419823	51.006196
3454.646602	439688.305293	51.011201
3453.865468	439362.732103	51.016205
3453.462052	439041.816334	51.021210
3452.628665	438718.882847	51.026215
3451.740628	438400.319958	51.031220
3451.238599	438080.803470	51.036225
3450.503252	437764.340619	51.041229
3449.959035	437442.334826	51.046234
3449.155538	437119.705828	51.051239
3448.733711	436805.846777	51.056244
3447.854206	436481.368354	51.061249
3447.040652	436164.516797	51.066253
3446.601919	435837.700926	51.071258
3446.073808	435524.223468	51.076263
3445.173115	435197.726210	51.081268
3444.607102	434877.798172	51.086273
3443.739214	434558.548536	51.091277
3443.002700	434236.354386	51.096282
3442.387119	433918.173928	51.101287
3441.684863	433593.427299	51.106292
3440.842309	433283.907274	51.111297
3440.436928	432960.375164	51.116301
3439.737767	432643.613910	51.121306
3438.770526	432336.438090	51.126311
3438.157338	432014.044117	51.131316
3437.736610	431700.502699	51.136321
3436.580472	431382.274704	51.141325
3436.364877	431067.245853	51.146330
3435.478430	430752.192281	51.151335
3434.756394	430435.356803	51.156340
3433.936235	430126.150886	51.161345
3433.387673	429812.149822	51.166349
3433.023334	429491.640496	51.171354
3432.007991	429182.809804	51.176359
3431.596929	428859.100512	51.181364
3430.613905	428549.393870	51.186369
3429.992120	428240.108982	51.191373
3429.683911	427923.126968	51.196378
3428.618223	427611.568568	51.201383
3428.221784	427288.498021	51.206388
3427.422127	426979.937643	51.211393
3426.545998	426657.595583	51.216397
3426.136636	426340.839285	51.221402
3425.030938	426034.932234	51.226407
3424.602881	425713.625432	51.231412
3423.603206	425414.704186	51.236417
3422.981898	425110.462458	51.241421
3422.561751	424791.733989	51.246426
3421.731011	424491.759891	51.251431
3420.857158	424174.899183	51.256436
3420.240216	423871.658798	51.261441
3419.679523	423567.313975	51.266445
3419.182029	423260.187218	51.271450
3418.154983	422964.240451	51.276455
3417.353256	422648.188801	51.281460
3416.707654	422347.933258	51.286465
3415.998766	422044.280758	51.291469
3415.612536	421739.989677	51.296474
3414.470657	421444.171717	51.301479
3414.523252	421138.407570	51.306484
3413.415835	420830.867531	51.311489
3412.702120	420528.875690	51.316493
3412.225457	420222.499300	51.321498
3411.249920	419923.870007	51.326503
3410.871801	419622.501170	51.331508
3410.032115	419315.994432	51.336513
3409.111922	419011.326125	51.341517
3408.715606	418709.086653	51.346522
3407.672740	418417.031539	51.351527
3407.072015	418110.854971	51.356532
3406.609895	417809.683268	51.361537
3405.543529	417512.795696	51.366541
3405.291345	417216.690872	51.371546
3404.639586	416922.729385	51.376551
3404.001581	416614.891273	51.381556
3403.072339	416318.325272	51.386561
3402.328947	416016.518575	51.391565
3402.000673	415713.677632	51.396570
3401.275901	415426.038539	51.401575
3400.299938	415123.471658	51.406580
3399.606582	414826.192426	51.411585
3398.949341	414524.788440	51.416589
3398.495155	414228.735645	51.421594
3397.647209	413935.536972	51.426599
3397.083910	413629.662487	51.431604
3396.492776	413338.780181	51.436609
3395.709454	413048.230281	51.441613
3395.079468	412740.349780	51.446618
3394.144550	412451.876084	51.451623
3393.844560	412161.876244	51.456628
3393.073270	411860.717001	51.461633
3392.082483	411577.884566	51.466637
3391.625528	411261.423570	51.471642
3390.960926	410980.109305	51.476647
3390.482382	410678.663106	51.481652
3389.745405	410381.828707	51.486657
3388.845359	410098.764611	51.491661
3388.318473	409796.605671	51.496666
3387.345371	409509.176806	51.501671
3386.736076	409219.349777	51.506676
3386.017212	408928.622457	51.511681
3385.600118	408634.642663	51.516685
3384.948869	408340.747874	51.521690
3384.116154	408051.834461	51.526695
3383.458747	407761.594518	51.531700
3383.001259	407462.450930	51.536705
3382.085920	407172.932351	51.541709
3381.231965	406875.141822	51.546714
3380.655338	406592.146409	51.551719
3379.974487	406293.840019	51.556724
3379.240101	406003.316087	51.561729
3378.377376	405716.952343	51.566733
3378.054061	405430.144850	51.571738
3377.149791	405147.315122	51.576743
3376.534125	404853.965989	51.581748
3376.225067	404560.743529	51.586753
3375.396208	404285.696724	51.591757
3374.872633	403986.860466	51.596762
3374.075301	403702.628305	51.601767
3373.407680	403410.900557	51.606772
3372.659280	403118.293298	51.611777
3371.966664	402832.842159	51.616781
3371.397443	402541.243347	51.621786
3370.622968	402260.985168	51.626791
3370.047068	401958.655837	51.631796
3369.573491	401666.296784	51.636801
3368.544732	401380.021583	51.641805
3368.298659	401084.977750	51.646810
3367.188502	400812.055108	51.651815
3366.574211	400519.250339	51.656820
3366.034352	400221.143947	51.661825
3365.499852	399938.946556	51.666829
3364.655421	399644.009620	51.671834
3363.593057	399362.577034	51.676839
3362.960384	399071.109377	51.681844
3362.925092	398791.136344	51.686849
3361.946317	398505.717592	51.691853
3361.292252	398208.119288	51.696858
3360.625447	397927.933719	51.701863
3359.802727	397639.355997	51.706868
3358.932768	397350.300221	51.711873
3358.576540	397081.879359	51.716877
3357.881739	396782.825648	51.721882
3356.728623	396504.992938	51.726887
3356.597353	396212.429328	51.731892
3356.112917	395925.257751	51.736897
3355.367474	395644.175612	51.741901
3354.736575	395354.530889	51.746906
3354.183926	395063.269643	51.751911
3353.510617	394768.363997	51.756916
3352.924685	394476.975855	51.761921
3352.113140	394194.951449	51.766925
3351.447460	393895.460728	51.771930
3350.533849	393617.032479	51.776935
3349.466984	393328.100459	51.781940
3349.074889	393045.822270	51.786945
3348.403387	392753.288858	51.791949
3347.811021	392476.122657	51.796954
3347.156893	392190.777042	51.801959
3346.840135	391902.451788	51.806964
3345.718610	391619.285708	51.811969
3345.046960	391334.596901	51.816973
3344.724636	391047.765583	51.821978
3343.541307	390769.789324	51.826983
3342.974164	390483.526057	51.831988
3342.476863	390197.630817	51.836993
3341.595921	389924.812548	51.841997
3340.984269	389630.794166	51.847002
3340.236680	389356.297656	51.852007
3339.824457	389069.820447	51.857012
3339.312961	388784.602595	51.862017
3338.547524	388508.729273	51.867021
3338.043823	388216.767237	51.872026
3337.016935	387935.718067	51.877031
3336.554049	387651.449788	51.882036
3335.862472	387372.402909	51.887041
3334.948153	387088.939028	51.892045
3334.682887	386804.200540	51.897050
3333.769067	386528.844116	51.902055
3332.977816	386236.530121	51.907060
3332.402432	385947.053213	51.912065
3331.530182	385672.573801	51.917069
3331.006308	385385.957905	51.922074
3330.448271	385106.872571	51.927079
3329.499172	384827.516376	51.932084
3328.824409	384540.765193	51.937089
3328.340924	384265.654352	51.942093
3327.652309	383991.057109	51.947098
3326.881515	383697.524494	51.952103
3326.191277	383422.872464	51.957108
3325.768293	383144.590283	51.962113
3324.747777	382862.916369	51.967117
3324.520712	382582.284739	51.972122
3323.715682	382296.427083	51.977127
3322.744905	382012.093997	51.982132
3322.203791	381735.880148	51.987137
3321.503902	381461.367974	51.992141
3320.841718	381176.496617	51.997146
3320.092303	380910.686416	52.002151
3319.707358	380626.631854	52.007156
3319.239082	380345.614970	52.012161
3318.067568	380067.861046	52.017165
3317.728266	379780.384907	52.022170
3316.576663	379501.555545	52.027175
3316.001068	379231.509662	52.032180
3315.702275	378947.123942	52.037185
3314.999651	378670.506731	52.042189
3314.095782	378384.762845	52.047194
3313.410639	378124.646248	52.052199
3312.712147	377834.211270	52.057204
3312.144555	377569.137985	52.062209
3311.323054	377290.062650	52.067213
3310.802172	377004.146463	52.072218
3310.219050	376730.396444	52.077223
3309.446567	376459.218109	52.082228
3309.126375	376178.860216	52.087233
3307.963445	375910.385294	52.092237
3307.584998	375623.521012	52.097242
3306.645245	375360.654063	52.102247
3305.972374	375073.807010	52.107252
3305.436849	374800.646832	52.112257
3304.536724	374529.577473	52.117261
3303.990492	374254.329468	52.122266
3303.273361	373977.707572	52.127271
3302.565062	373712.351371	52.132276
3301.966003	373435.656277	52.137281
3301.349677	373168.068921	52.142285
3300.528959	372891.099982	52.147290
3299.841965	372623.189587	52.152295
3299.401760	372349.082280	52.157300
3298.613479	372063.428120	52.162305
3298.123633	371801.993614	52.167309
3297.377190	371530.676795	52.172314
3296.549274	371264.662491	52.177319
3295.867798	370990.330079	52.182324
3295.416511	370715.984921	52.187329
3294.725127	370447.832399	52.192333
3294.147629	370168.237630	52.197338
3293.436728	369898.710983	52.202343
3292.207904	369630.511131	52.207348
3291.921146	369356.461940	52.212353
3291.387514	369094.458021	52.217357
3290.791605	368804.884568	52.222362
3290.070107	368539.447056	52.227367
3289.246699	368269.851702	52.232372
3288.619596	367995.974941	52.237377
3287.975221	367724.897752	52.242381
3287.439486	367443.370659	52.247386
3286.459737	367179.466785	52.252391
3285.995523	366912.146905	52.257396
3285.445930	366640.895397	52.262401
3284.632498	366366.351035	52.267405
3284.132324	366094.147010	52.272410
3283.569894	365813.300721	52.277415
3282.629196	365543.351074	52.282420
3281.835061	365274.979519	52.287425
3281.202155	365006.809849	52.292429
3280.355832	364722.770393	52.297434
3280.143234	364458.347459	52.302439
3279.386975	364195.790017	52.307444
3278.797375	363919.516061	52.312449
3277.869792	363659.450658	52.317453
3277.363680	363386.824177	52.322458
3276.679824	363111.247243	52.327463
3275.772493	362833.159594	52.332468
3275.145562	362556.628913	52.337473
3274.299796	362295.194327	52.342477
3273.970074	362024.440253	52.347482
3273.420363	361758.528467	52.352487
3272.804993	361489.139604	52.357492
3272.077033	361216.637265	52.362497
3271.265040	360943.866745	52.367501
3270.722462	360676.013879	52.372506
3270.055218	360401.868738	52.377511
3269.520678	360132.586590	52.382516
3268.797388	359866.309935	52.387521
3268.034895	359589.325268	52.392525
3267.260416	359312.824374	52.397530
3266.873903	359047.940339	52.402535
3265.950719	358772.528614	52.407540
3265.446035	358501.629498	52.412545
3264.568771	358231.194954	52.417549
3264.143253	357955.318185	52.422554
3263.459626	357687.114766	52.427559
3262.635369	357419.135706	52.432564
3261.915193	357148.848478	52.437569
3261.142673	356878.924316	52.442573
3260.663108	356607.272812	52.447578
3259.755140	356347.418941	52.452583
3259.438056	356073.397649	52.457588
3258.610211	355800.168194	52.462593
3257.715398	355538.094080	52.467597
3257.230599	355270.609636	52.472602
3256.478322	354999.756019	52.477607
3255.691543	354736.973566	52.482612
3255.323847	354467.659533	52.487617
3254.166662	354201.471911	52.492621
3253.611212	353934.958685	52.497626
3253.413357	353674.851545	52.502631
3252.572066	353411.332906	52.507636
3251.672004	353140.238360	52.512641
3250.989663	352875.902934	52.517645
3250.338825	352611.841129	52.522650
3249.870838	352357.470813	52.527655
3249.057921	352088.265745	52.532660
3248.919447	351811.470358	52.537665
3247.840049	351551.313953	52.542669
3247.043053	351276.325089	52.547674
3246.338914	351017.277416	52.552679
3245.695681	350743.635797	52.557684
3245.254242	350481.286329	52.562689
3244.741716	350223.706092	52.567693
3244.064055	349948.564292	52.572698
3243.264548	349693.215691	52.577703
3242.536494	349421.184196	52.582708
3241.932418	349145.721284	52.587713
3241.301451	348883.852203	52.592717
3240.431019	348622.325173	52.597722
3239.827471	348351.134026	52.602727
3238.630627	348090.979594	52.607732
3238.438308	347826.974539	52.612737
3237.587452	347570.555250	52.617741
3237.061773	347302.655419	52.622746
3236.302448	347036.394753	52.627751
3235.763725	346778.166279	52.632756
3235.364052	346508.181114	52.637761
3234.537898	346249.104870	52.642765
3233.560575	345984.171824	52.647770
3233.299780	345727.956276	52.652775
3232.572948	345455.447173	52.657780
3231.926174	345191.730822	52.662785
3231.123481	344931.881340	52.667789
3230.290486	344664.908613	52.672794
3229.655081	344404.826690	52.677799
3228.895212	344147.054102	52.682804
3228.356057	343878.809546	52.687809
3227.546431	343621.297063	52.692813
3226.922956	343363.372206	52.697818
3226.631267	343100.328436	52.702823
3225.495251	342834.108067	52.707828
3225.206675	342573.301430	52.712833
3224.463388	342317.605516	52.717837
3223.863299	342048.904199	52.722842
3223.334538	341789.583066	52.727847
3222.132224	341533.574645	52.732852
3222.019191	341263.800085	52.737857
3221.103227	341003.315049	52.742861
3220.518429	340738.627388	52.747866
3219.959209	340480.654643	52.752871
3219.447787	340219.720482	52.757876
3218.702174	339946.145629	52.762881
3217.761626	339681.280651	52.767885
3216.796951	339412.574618	52.772890
3216.071483	339151.440774	52.777895
3215.537800	338896.486666	52.782900
3215.092206	338631.818999	52.787905
3214.055525	338385.750075	52.792909
3213.324979	338124.765561	52.797914
3212.915579	337865.256540	52.802919
3211.930080	337622.485875	52.807924
3211.742021	337355.302979	52.812929
3211.055663	337105.049860	52.817933
3210.390195	336839.569581	52.822938
3209.805532	336582.985204	52.827943
3208.958789	336327.637749	52.832948
3208.313229	336061.056556	52.837953
3207.642213	335808.428622	52.842957
3207.087161	335554.355803	52.847962
3206.253912	335289.328634	52.852967
3205.671268	335044.244553	52.857972
3205.237998	334771.082190	52.862977
3204.134471	334520.376222	52.867981
3203.526244	334255.360327	52.872986
3202.797294	334005.331474	52.877991
3202.244567	333733.889514	52.882996
3201.734019	333483.773304	52.888001
3200.462274	333227.895888	52.893005
3199.977200	332975.813578	52.898010
3199.535255	332725.938374	52.903015
3198.910117	332468.912114	52.908020
3198.445606	332213.463366	52.913025
3197.604646	331955.807479	52.918029
3197.168140	331695.184430	52.923034
3196.124701	331439.417168	52.928039
3195.404612	331182.986838	52.933044
3195.190100	330925.024473	52.938049
3194.487010	330673.783192	52.943053
3193.818759	330416.476360	52.948058
3193.119464	330158.868030	52.953063
3192.480193	329898.066941	52.958068
3191.569979	329632.419674	52.963073
3190.712940	329382.165782	52.968077
3190.005466	329121.831023	52.973082
3189.434131	328871.122874	52.978087
3188.660015	328623.399256	52.983092
3188.520760	328360.018685	52.988097
3187.749381	328113.209507	52.993101
3186.870204	327861.197375	52.998106
3186.269787	327599.032824	53.003111
3185.396272	327340.984152	53.008116
3185.074845	327093.565863	53.013121
3184.112325	326839.093983	53.018125
3183.575424	326570.983757	53.023130
3182.677120	326318.969651	53.028135
3181.849927	326074.734302	53.033140
3181.652342	325818.330433	53.038145
3180.699985	325573.756908	53.043149
3180.320780	325314.808670	53.048154
3179.619426	325056.674384	53.053159
3179.076512	324799.609014	53.058164
3178.451011	324547.749871	53.063169
3177.804824	324300.730763	53.068173
3177.169583	324033.977063	53.073178
3176.127291	323774.874249	53.078183
3175.396779	323533.824040	53.083188
3175.046071	323267.710311	53.088193
3173.886950	323020.284797	53.093197
3173.193009	322768.660247	53.098202
3172.307429	322520.222468	53.103207
3172.021699	322274.337037	53.108212
3171.567208	322034.842955	53.113217
3170.729788	321789.196195	53.118221
3170.062189	321524.833091	53.123226
3169.691718	321275.444536	53.128231
3168.808202	321033.393029	53.133236
3168.412708	320772.065468	53.138241
3167.542567	320524.281552	53.143245
3167.120500	320265.986666	53.148250
3166.643489	320008.896443	53.153255
3165.405764	319755.108607	53.158260
3165.036665	319499.884055	53.163265
3164.240117	319250.455416	53.168269
3163.455625	319000.438558	53.173274
3163.025493	318746.189131	53.178279
3161.942955	318505.359073	53.183284
3161.809961	318240.799898	53.188289
3160.866118	317994.955934	53.193293
3160.068829	317741.016493	53.198298
3159.470792	317491.908217	53.203303
3158.743747	317247.046520	53.208308
3158.218340	316993.927805	53.213313
3157.583402	316745.841945	53.218317
3156.739017	316498.297849	53.223322
3156.245721	316247.030902	53.228327
3155.437434	315997.188159	53.233332
3154.796166	315740.417847	53.238337
3154.303010	315495.896701	53.243341
3153.404803	315242.221346	53.248346
3152.876032	314991.720741	53.253351
3152.018747	314740.431204	53.258356
3151.745802	314494.217670	53.263361
3150.691034	314246.192026	53.268365
3150.312480	314002.234815	53.273370
3149.695115	313747.161746	53.278375
3148.862459	313505.923444	53.283380
3147.891647	313245.583169	53.288385
3147.390399	313007.066839	53.293389
3146.675249	312761.352081	53.298394
3146.375028	312513.584919	53.303399
3145.561643	312260.856517	53.308404
3144.644672	312001.650585	53.313409
3144.050594	311759.937719	53.318413
3143.758632	311514.815249	53.323418
3143.263605	311259.334967	53.328423
3142.374385	311025.000897	53.333428
3141.699840	310753.785480	53.338433
3140.813746	310514.102344	53.343437
3140.297858	310256.178510	53.348442
3139.637505	310013.963091	53.353447
3138.646383	309763.701775	53.358452
3138.211882	309507.418590	53.363457
3137.380041	309263.191576	53.368461
3136.880344	309026.194409	53.373466
3136.297400	308769.576606	53.378471
3135.516583	308523.150030	53.383476
3134.834488	308275.434085	53.388481
3134.027760	308029.163393	53.393485
3133.952376	307773.328974	53.398490
3133.023310	307532.602547	53.403495
3132.387383	307284.368001	53.408500
3131.595844	307025.207580	53.413505
3130.798948	306777.328552	53.418509
3130.292701	306521.916271	53.423514
3129.729333	306277.971897	53.428519
3129.005697	306030.792862	53.433524
3128.434980	305780.329592	53.438529
3127.698643	305536.003754	53.443533
3127.175032	305279.165723	53.448538
3126.530259	305029.247526	53.453543
3125.680034	304766.959644	53.458548
3125.033777	304521.828272	53.463553
3123.944193	304272.692108	53.468557
3123.487711	304028.370193	53.473562
3122.897536	303778.415609	53.478567
3122.261930	303535.470863	53.483572
3121.433152	303286.164342	53.488577
3121.060399	303037.396405	53.493581
3120.494545	302792.885939	53.498586
3119.536140	302537.486813	53.503591
3118.706648	302300.020383	53.508596
3118.032063	302048.038874	53.513601
3117.436219	301804.830284	53.518605
3116.796953	301561.806435	53.523610
3116.461245	301311.196172	53.528615
3115.409522	301066.021246	53.533620
3114.772956	300827.757991	53.538625
3114.093922	300580.664287	53.543629
3113.495371	300340.331506	53.548634
3113.073727	300087.466376	53.553639
3112.027343	299851.915011	53.558644
3111.592085	299590.036145	53.563649
3110.933963	299351.035576	53.568653
3110.015592	299114.597033	53.573658
3109.662367	298865.335439	53.578663
3108.561117	298624.646764	53.583668
3108.012631	298374.116552	53.588673
3107.434351	298134.668696	53.593677
3106.841513	297887.633734	53.598682
3106.404575	297640.955756	53.603687
3105.531445	297402.266633	53.608692
3104.971121	297157.084587	53.613697
3104.177677	296911.226030	53.618701
3103.682593	296672.552524	53.623706
3102.892739	296426.947424	53.628711
3102.270191	296181.442861	53.633716
3101.544663	295934.273457	53.638721
3100.983375	295689.955517	53.643725
3100.192492	295439.001238	53.648730
3100.019624	295194.086403	53.653735
3098.554509	294944.078608	53.658740
3097.964232	294698.923619	53.663745
3097.514029	294463.576497	53.668749
3096.262989	294229.883873	53.673754
3096.176098	293980.242543	53.678759
3095.498831	293738.232657	53.683764
3095.156800	293499.225520	53.688769
3094.173607	293262.178700	53.693773
3093.410954	293017.099978	53.698778
3092.911799	292767.649834	53.703783
3092.067779	292539.901279	53.708788
3091.498488	292290.130634	53.713793
3091.043316	292050.375837	53.718797
3090.254991	291810.800856	53.723802
3089.983043	291558.359228	53.728807
3088.718710	291315.293633	53.733812
3088.466932	291060.683558	53.738817
3087.698765	290817.717227	53.743821
3087.001462	290572.090818	53.748826
3086.333139	290334.914840	53.753831
3085.209027	290092.640845	53.758836
3084.852605	289837.027414	53.763841
3084.451818	289600.699808	53.768845
3083.205969	289351.797345	53.773850
3082.875815	289112.529357	53.778855
3082.242686	288881.356927	53.783860
3081.578888	288636.742176	53.788865
3080.908032	288397.782191	53.793869
3079.914010	288153.372108	53.798874
3079.455340	287910.175963	53.803879
3078.642759	287686.671361	53.808884
3078.232614	287436.183358	53.813889
3077.601236	287196.095608	53.818893
3076.838861	286961.504016	53.823898
3075.896492	286723.400703	53.828903
3075.096113	286478.296530	53.833908
3074.603170	286242.286531	53.838913
3074.168996	286013.729196	53.843917
3073.442953	285780.888346	53.848922
3072.895245	285543.358477	53.853927
3072.294012	285299.902876	53.858932
3071.573580	285058.579835	53.863937
3070.912232	284833.062967	53.868941
3069.851594	284584.407740	53.873946
3069.490987	284337.755426	53.878951
3068.705864	284108.080983	53.883956
3068.039878	283863.132154	53.888961
3067.462725	283631.794587	53.893965
3066.770956	283386.824112	53.898970
3066.394908	283135.207285	53.903975
3065.285068	282915.134198	53.908980
3064.468017	282668.298541	53.913985
3063.960430	282429.334398	53.918989
3063.094060	282208.050936	53.923994
3062.613810	281965.516710	53.928999
3061.980950	281736.020802	53.934004
3061.651714	281494.226522	53.939009
3060.919403	281258.404574	53.944013
3060.027788	281031.266960	53.949018
3059.437863	280781.516626	53.954023
3058.735544	280560.181124	53.959028
3058.379764	280310.699179	53.964033
3057.688773	280079.148950	53.969037
3056.871418	279837.278516	53.974042
3056.564488	279588.832803	53.979047
3055.737286	279357.482199	53.984052
3054.951835	279112.066408	53.989057
3054.152741	278876.610831	53.994061
3053.309276	278634.616856	53.999066
3053.102479	278405.358105	54.004071
3052.226825	278171.162434	54.009076
3051.895734	277920.886397	54.014081
3050.650334	277691.409864	54.019085
3050.204695	277453.911518	54.024090
3049.715914	277212.421427	54.029095
3048.992959	276977.055306	54.034100
3048.387082	276740.855634	54.039105
3047.960695	276498.795267	54.044109
3046.786575	276261.641277	54.049114
3046.439635	276007.037842	54.054119
3045.569188	275779.539203	54.059124
3044.878551	275542.537849	54.064129
3044.403935	275292.869972	54.069133
3043.603099	275061.438149	54.074138
3043.204013	274817.768843	54.079143
3042.255163	274580.477242	54.084148
3041.575340	274337.845637	54.089153
3040.969316	274103.199431	54.094157
3040.128280	273870.296812	54.099162
3039.622451	273629.496884	54.104167
3039.052091	273393.164153	54.109172
3038.186828	273166.097671	54.114177
3037.504287	272925.733260	54.119181
3036.762046	272684.410526	54.124186
3036.378466	272454.491820	54.129191
3035.549744	272214.965618	54.134196
3034.738915	271976.710038	54.139201
3034.463435	271745.679180	54.144205
3033.188065	271513.991637	54.149210
3032.935300	271271.878529	54.154215
3032.281421	271042.359388	54.159220
3031.701750	270800.654678	54.164225
3030.952528	270566.821110	54.169229
3030.362433	270339.660581	54.174234
3029.755912	270097.043432	54.179239
3028.836455	269863.313389	54.184244
3028.506676	269617.494500	54.189249
3027.705902	269384.891880	54.194253
3026.968365	269152.941498	54.199258
3026.521763	268912.031237	54.204263
3025.761012	268680.594046	54.209268
3025.082198	268440.382879	54.214273
3024.399039	268201.089346	54.219277
3023.327697	267951.695515	54.224282
3022.862211	267707.274069	54.229287
3021.958237	267481.692216	54.234292
3021.537635	267239.250385	54.239297
3021.044902	267019.104761	54.244301
3020.115364	266783.110745	54.249306
3019.498427	266541.871845	54.254311
3018.854339	266299.542228	54.259316
3017.874875	266075.551957	54.264321
3017.277602	265850.558974	54.269325
3016.557966	265615.551023	54.274330
3016.188959	265381.964846	54.279335
3015.372232	265167.372467	54.284340
3014.687199	264929.124956	54.289345
3014.518207	264702.638554	54.294349
3013.140737	264463.991555	54.299354
3012.959363	264232.948592	54.304359
3011.928413	264005.733111	54.309364
3011.563207	263771.459614	54.314369
3011.069872	263541.587041	54.319373
3010.391996	263310.190277	54.324378
3009.481949	263070.018494	54.329383
3008.516513	262838.769426	54.334388
3007.914990	262610.213447	54.339393
3007.399505	262378.002091	54.344397
3006.475911	262156.501080	54.349402
3006.233246	261925.061831	54.354407
3005.779224	261701.220161	54.359412
3004.861520	261469.557015	54.364417
3004.443731	261241.253066	54.369421
3003.327380	261009.927326	54.374426
3003.110923	260767.788313	54.379431
3002.364481	260539.511457	54.384436
3001.383483	260302.943956	54.389441
3001.110151	260073.242789	54.394445
3000.355267	259845.171568	54.399450
2999.932295	259608.363516	54.404455
2999.044776	259372.011221	54.409460
2998.378501	259144.588723	54.414465
2997.494226	258907.752443	54.419469
2996.998688	258676.916132	54.424474
2996.565653	258438.990151	54.429479
2995.482003	258216.855395	54.434484
2994.889841	257983.692001	54.439489
2994.485210	257739.930130	54.444493
2993.572106	257511.529481	54.449498
2992.808984	257281.526328	54.454503
2992.275898	257052.785823	54.459508
2991.504760	256818.556803	54.464513
2990.948808	256598.632090	54.469517
2990.218515	256369.337737	54.474522
2989.798811	256125.758221	54.479527
2988.862280	255902.660090	54.484532
2988.288972	255677.543710	54.489537
2987.757380	255442.794345	54.494541
2986.783062	255214.583996	54.499546
2986.131075	254987.061417	54.504551
2985.174373	254756.760471	54.509556
2984.658126	254531.559886	54.514561
2984.186143	254306.097872	54.519565
2983.332218	254086.477600	54.524570
2983.007680	253858.828050	54.529575
2982.113993	253639.596576	54.534580
2981.706009	253407.936973	54.539585
2981.075406	253182.093889	54.544589
2980.077545	252957.506158	54.549594
2979.598556	252723.159136	54.554599
2978.934407	252499.639670	54.559604
2978.430003	252267.258197	54.564609
2978.103303	252027.157916	54.569613
2976.761938	251806.955322	54.574618
2976.434056	251568.027313	54.579623
2975.506671	251342.590014	54.584628
2975.119633	251115.157466	54.589633
2974.188896	250882.845294	54.594637
2973.470253	250657.503174	54.599642
2972.950771	250427.214778	54.604647
2972.170849	250203.360024	54.609652
2971.252541	249979.349213	54.614657
2970.774136	249746.075675	54.619661
2970.209816	249527.662993	54.624666
2969.698803	249299.692270	54.629671
2968.446381	249076.575983	54.634676
2968.109547	248856.931280	54.639681
2967.730131	248626.190324	54.644685
2966.926083	248408.071788	54.649690
2966.566791	248181.504767	54.654695
2965.853175	247951.148781	54.659700
2964.735701	247725.899370	54.664705
2964.542434	247489.757292	54.669709
2963.737407	247264.968428	54.674714
2963.039093	247030.358594	54.679719
2962.159489	246808.943741	54.684724
2961.392735	246585.423151	54.689729
2960.786015	246351.309222	54.694733
2960.246333	246135.978861	54.699738
2959.539565	245914.843603	54.704743
2958.709927	245686.444930	54.709748
2958.188183	245462.225196	54.714753
2957.715786	245235.069454	54.719757
2956.861446	245018.288140	54.724762
2956.101271	244784.226575	54.729767
2955.745458	244565.686321	54.734772
2954.881826	244335.283483	54.739777
2954.443040	244104.482729	54.744781
2953.810383	243888.941398	54.749786
2953.000482	243660.950434	54.754791
2952.301365	243437.118643	54.759796
2951.642228	243210.683444	54.764801
2951.128765	242987.205013	54.769805
2950.152608	242765.429997	54.774810
2949.589946	242534.600694	54.779815
2948.843274	242311.033040	54.784820
2948.390327	242084.719980	54.789825
2947.699249	241867.026748	54.794829
2946.852160	241646.939421	54.799834
2946.068530	241415.765188	54.804839
2945.614173	241185.939828	54.809844
2944.983826	240973.280610	54.814849
2944.543492	240751.195168	54.819853
2943.572728	240525.119752	54.824858
2942.973144	240296.108485	54.829863
2942.512773	240079.196799	54.834868
2941.814220	239850.838679	54.839873
2941.157213	239626.319575	54.844877
2940.312461	239397.730841	54.849882
2940.155773	239169.899414	54.854887
2939.009094	238951.494223	54.859892
2938.331909	238724.815593	54.864897
2937.762448	238488.011026	54.869901
2936.979880	238278.640243	54.874906
2936.439364	238049.649546	54.879911
2935.705057	237828.278321	54.884916
2934.968934	237600.847367	54.889921
2934.354651	237373.397593	54.894925
2933.172959	237148.915558	54.899930
2933.000860	236929.341471	54.904935
2932.129276	236712.526820	54.909940
2931.532141	236487.469795	54.914945
2930.850907	236273.299599	54.919949
2930.075579	236058.075255	54.924954
2929.575169	235833.258937	54.929959
2928.934477	235619.414676	54.934964
2927.954825	235386.857854	54.939969
2927.633142	235177.878462	54.944973
2927.027062	234960.745279	54.949978
2926.494532	234726.667733	54.954983
2925.674650	234515.375004	54.959988
2924.729025	234291.778379	54.964993
2924.758974	234076.023250	54.969997
2924.003805	233861.818830	54.975002
2923.262410	233631.163494	54.980007
2922.592037	233402.509032	54.985012
2921.821224	233179.905738	54.990017
2921.194753	232948.368055	54.995021
2920.204272	232732.955651	55.000026
2919.699714	232491.825693	55.005031
2919.001148	232281.358790	55.010036
2918.221487	232067.162165	55.015041
2918.012907	231834.262380	55.020045
2916.867941	231616.126965	55.025050
2916.231489	231398.497177	55.030055
2915.864330	231174.714253	55.035060
2915.039368	230963.684643	55.040065
2914.171504	230731.375751	55.045069
2913.239058	230522.604848	55.050074
2912.800897	230306.270249	55.055079
2912.436016	230089.135227	55.060084
2911.812322	229872.372707	55.065089
2911.369855	229644.938859	55.070093
2910.518830	229434.400662	55.075098
2909.903354	229202.055689	55.080103
2909.333486	228983.122511	55.085108
2908.526537	228756.843477	55.090113
2907.968854	228530.169088	55.095117
2907.084547	228314.673756	55.100122
2906.736271	228089.418658	55.105127
2905.918178	227866.199068	55.110132
2904.947975	227649.242203	55.115137
2904.490622	227416.698660	55.120141
2903.695894	227200.300749	55.125146
2903.078230	226979.521462	55.130151
2902.694592	226760.004213	55.135156
2902.091790	226543.170193	55.140161
2901.271198	226308.675742	55.145165
2900.129277	226096.893145	55.150170
2900.173511	225872.752921	55.155175
2899.373491	225660.013427	55.160180
2898.492430	225430.890526	55.165185
2898.093264	225210.997867	55.170189
2896.888485	224991.220625	55.175194
2896.643936	224768.198459	55.180199
2895.687269	224549.121475	55.185204
2895.426293	224325.173810	55.190209
2894.640714	224099.425758	55.195213
2893.892898	223888.261142	55.200218
2893.212445	223655.648851	55.205223
2892.318208	223437.748901	55.210228
2892.150609	223216.551971	55.215233
2891.389921	222991.541447	55.220237
2890.383742	222775.761497	55.225242
2889.778913	222551.402241	55.230247
2889.031372	222341.132797	55.235252
2888.300812	222118.996968	55.240257
2887.793550	221904.260654	55.245261
2886.952691	221693.714953	55.250266
2886.480619	221470.381642	55.255271
2886.013226	221250.039732	55.260276
2884.973788	221028.681553	55.265281
2884.512832	220808.670870	55.270285
2883.542503	220606.677550	55.275290
2883.091101	220375.349963	55.280295
2882.444892	220164.637644	55.285300
2881.498381	219939.805502	55.290305
2881.289477	219728.337772	55.295309
2880.237439	219518.582605	55.300314
2879.807433	219297.680398	55.305319
2879.439784	219075.496041	55.310324
2878.450804	218856.491243	55.315329
2877.984572	218640.115667	55.320333
2876.952230	218425.752496	55.325338
2876.465703	218204.875268	55.330343
2875.832753	217989.877328	55.335348
2875.158402	217768.980259	55.340353
2874.606341	217549.184668	55.345357
2873.544692	217342.123147	55.350362
2873.275899	217124.460681	55.355367
2872.700254	216902.634174	55.360372
2871.592989	216695.454475	55.365377
2871.197543	216472.620655	55.370381
2870.300869	216261.208347	55.375386
2870.044582	216035.948122	55.380391
2869.268692	215819.731982	55.385396
2868.852420	215595.096773	55.390401
2868.121256	215376.609215	55.395405
2867.408007	215164.356566	55.400410
2867.046763	214945.137182	55.405415
2866.386037	214721.943687	55.410420
2865.362091	214506.356476	55.415425
2864.802775	214282.524667	55.420429
2863.862153	214058.448497	55.425434
2863.509615	213838.022105	55.430439
2862.665767	213623.478386	55.435444
2862.257511	213404.373268	55.440449
2861.628902	213177.895891	55.445453
2860.473724	212966.038350	55.450458
2859.919347	212742.949152	55.455463
2859.213088	212525.854276	55.460468
2858.691415	212307.368977	55.465473
2858.074685	212086.850236	55.470477
2857.201343	211867.951157	55.475482
2856.640614	211662.698649	55.480487
2855.881355	211439.060859	55.485492
2855.214830	211222.244053	55.490497
2854.629541	211000.705798	55.495501
2853.846056	210798.686016	55.500506
2853.345237	210577.606779	55.505511
2852.824896	210359.038769	55.510516
2852.238792	210147.571259	55.515521
2851.575768	209920.448880	55.520525
2850.634262	209712.997412	55.525530
2849.845560	209487.449268	55.530535
2849.354738	209267.620337	55.535540
2848.677362	209061.643776	55.540545
2848.215403	208840.271755	55.545549
2847.379113	208627.678073	55.550554
2846.643093	208400.407330	55.555559
2846.156631	208179.665197	55.560564
2845.547578	207973.439625	55.565569
2844.931658	207750.555903	55.570573
2843.962990	207532.094278	55.575578
2843.486757	207315.388162	55.580583
2843.060616	207095.811294	55.585588
2842.366966	206881.190225	55.590593
2841.321425	206652.078698	55.595597
2840.601013	206444.030555	55.600602
2839.968164	206226.067741	55.605607
2839.372934	206005.248952	55.610612
2838.492216	205798.386592	55.615617
2838.358725	205578.590772	55.620621
2837.591528	205357.737996	55.625626
2836.672514	205141.568051	55.630631
2835.942843	204923.676276	55.635636
2834.976537	204717.493055	55.640641
2834.862059	204498.487314	55.645645
2833.911655	204291.514038	55.650650
2833.490471	204076.452764	55.655655
2832.704751	203856.652173	55.660660
2831.969995	203642.100327	55.665665
2831.407472	203425.931220	55.670669
2830.597128	203218.914165	55.675674
2829.838653	202996.261879	55.680679
2829.553414	202781.705702	55.685684
2828.406129	202574.757078	55.690689
2828.369380	202356.332602	55.695693
2827.468791	202142.576233	55.700698
2826.919561	201922.669302	55.705703
2826.298643	201709.417507	55.710708
2825.386167	201490.409710	55.715713
2824.294154	201278.455852	55.720717
2823.839200	201067.419970	55.725722
2823.379632	200846.383217	55.730727
2822.811383	200639.591843	55.735732
2821.817760	200438.467882	55.740737
2821.540987	200206.091679	55.745741
2820.769381	200004.692361	55.750746
2820.333422	199791.965868	55.755751
2819.950035	199575.745117	55.760756
2818.967449	199355.420756	55.765761
2818.335256	199125.968654	55.770765
2816.915638	198923.352544	55.775770
2816.850618	198704.361649	55.780775
2816.029433	198491.281350	55.785780
2815.497963	198295.538510	55.790785
2814.827439	198066.924136	55.795789
2813.782001	197856.935898	55.800794
2813.414567	197642.387378	55.805799
2812.908165	197423.789767	55.810804
2812.253282	197218.704917	55.815809
2811.626225	197001.044357	55.820813
2810.789333	196792.312529	55.825818
2810.345585	196580.758009	55.830823
2809.522676	196362.813003	55.835828
2808.484821	196148.962096	55.840833
2808.224643	195931.158816	55.845837
2807.249088	195724.883615	55.850842
2806.541137	195519.075833	55.855847
2805.839189	195299.143857	55.860852
2805.544066	195094.023129	55.865857
2805.212990	194881.706974	55.870861
2804.082820	194678.781499	55.875866
2803.528032	194461.196522	55.880871
2802.742783	194239.131915	55.885876
2802.079012	194036.911305	55.890881
2801.706437	193823.931763	55.895885
2800.701703	193611.613097	55.900890
2800.443123	193404.012233	55.905895
2799.603013	193183.296974	55.910900
2799.074266	192970.345784	55.915905
2798.458922	192758.974238	55.920909
2797.243545	192549.327258	55.925914
2796.760812	192323.940503	55.930919
2796.477939	192112.264579	55.935924
2795.537811	191909.103909	55.940929
2795.254744	191690.177418	55.945933
2794.181437	191475.499450	55.950938
2793.669853	191261.127877	55.955943
2793.324031	191046.680097	55.960948
2792.463627	190834.146909	55.965953
2792.033914	190615.299349	55.970957
2791.197937	190401.008387	55.975962
2790.534698	190172.924651	55.980967
2790.064933	189958.145066	55.985972
2789.039647	189748.810792	55.990977
2788.608539	189527.067552	55.995981
2787.786551	189313.644374	56.000986
2787.058065	189098.248030	56.005991
2786.481287	188878.261173	56.010996
2785.241374	188668.863847	56.016001
2784.928839	188457.513948	56.021005
2784.238305	188253.858400	56.026010
2783.621240	188037.049748	56.031015
2783.193131	187821.497133	56.036020
2782.202652	187617.408395	56.041025
2781.482637	187393.011037	56.046029
2781.020695	187189.094899	56.051034
2780.240034	186975.434031	56.056039
2779.770936	186763.493175	56.061044
2778.802286	186552.802845	56.066049
2778.503575	186338.788687	56.071053
2777.493322	186125.715152	56.076058
2776.903533	185923.007980	56.081063
2776.250402	185708.060580	56.086068
2775.599372	185501.891901	56.091073
2775.027443	185282.837214	56.096077
2774.437651	185069.460280	56.101082
2773.468634	184861.283952	56.106087
2772.867089	184653.775502	56.111092
2772.057917	184445.652093	56.116097
2771.788371	184235.930316	56.121101
2770.865998	184028.208406	56.126106
2770.172201	183817.054655	56.131111
2769.543229	183603.945275	56.136116
2768.826301	183400.798831	56.141121
2768.411386	183184.858874	56.146125
2768.080821	182980.788105	56.151130
2767.268680	182768.411389	56.156135
2766.388170	182554.570888	56.161140
2765.500423	182352.334039	56.166145
2765.060725	182124.267420	56.171149
2764.571060	181930.390654	56.176154
2763.869453	181714.147103	56.181159
2763.208705	181497.656453	56.186164
2762.491397	181281.939069	56.191169
2761.916755	181066.480006	56.196173
2760.991680	180864.866519	56.201178
2760.340527	180655.883615	56.206183
2759.817966	180435.763755	56.211188
2758.891936	180224.931139	56.216193
2758.832697	180009.281207	56.221197
2757.840100	179808.103110	56.226202
2757.188885	179597.357238	56.231207
2756.594734	179375.015401	56.236212
2756.006743	179175.429790	56.241217
2755.460849	178951.696034	56.246221
2754.617134	178746.416257	56.251226
2753.787483	178527.385148	56.256231
2753.246731	178314.122324	56.261236
2752.740316	178113.002415	56.266241
2752.130040	177883.051860	56.271245
2751.427731	177681.837843	56.276250
2750.616208	177469.347196	56.281255
2750.201791	177240.195900	56.286260
2749.333732	177033.491031	56.291265
2748.603090	176814.847457	56.296269
2747.936567	176609.143029	56.301274
2747.260117	176387.033495	56.306279
2746.693632	176183.248640	56.311284
2745.670929	175974.385856	56.316289
2745.453482	175751.901766	56.321293
2744.529501	175546.955663	56.326298
2743.616327	175333.194730	56.331303
2743.406449	175125.670160	56.336308
2742.326754	174915.142912	56.341313
2741.631458	174701.516108	56.346317
2740.940056	174496.462113	56.351322
2740.298534	174291.948146	56.356327
2740.055717	174081.508854	56.361332
2739.270146	173884.549070	56.366337
2738.594546	173652.432169	56.371341
2737.653279	173455.524578	56.376346
2737.172923	173247.747215	56.381351
2736.546457	173037.437734	56.386356
2735.846155	172832.711550	56.391361
2735.322531	172621.319649	56.396365
2734.401343	172409.127028	56.401370
2733.901554	172194.337935	56.406375
2733.167874	171983.605866	56.411380
2732.372142	171788.909044	56.416385
2731.950886	171577.163099	56.421389
2731.228972	171364.346771	56.426394
2730.440105	171161.156625	56.431399
2729.932145	170943.056354	56.436404
2729.102527	170746.907542	56.441409
2728.741070	170529.485816	56.446413
2727.889797	170326.538790	56.451418
2727.262237	170123.633682	56.456423
2726.816586	169902.973190	56.461428
2725.834918	169697.621133	56.466433
2725.226074	169487.760170	56.471437
2724.771044	169271.263198	56.476442
2723.990515	169069.977443	56.481447
2723.300359	168858.810227	56.486452
2722.582141	168649.289066	56.491457
2722.176610	168442.084802	56.496461
2721.289444	168236.369492	56.501466
2720.667224	168021.660923	56.506471
2720.052105	167802.488980	56.511476
2719.234779	167598.520906	56.516481
2718.618829	167391.940624	56.521485
2718.150553	167187.385378	56.526490
2717.656350	166973.692453	56.531495
2717.259036	166758.472178	56.536500
2716.453778	166550.718452	56.541505
2715.891016	166335.895561	56.546509
2714.979378	166117.657746	56.551514
2714.292473	165902.284791	56.556519
2713.859295	165681.684881	56.561524
2712.848653	165481.421004	56.566529
2712.210821	165261.517210	56.571533
2711.406301	165051.444745	56.576538
2710.831476	164839.849378	56.581543
2710.088011	164627.836899	56.586548
2709.675146	164424.279762	56.591553
2708.976676	164203.845091	56.596557
2708.044208	163993.989628	56.601562
2707.445081	163789.689881	56.606567
2706.829014	163572.704427	56.611572
2705.924241	163376.249673	56.616577
2705.108131	163158.026879	56.621581
2704.611291	162953.461297	56.626586
2704.320428	162730.466109	56.631591
2703.791623	162476.244832	56.636596
2703.060679	162271.745601	56.641601
2702.669945	162046.024105	56.646605
2701.826739	161827.394020	56.651610
2700.913130	161626.156824	56.656615
2700.304431	161409.386550	56.661620
2699.598756	161200.591988	56.666625
2698.980361	160985.949065	56.671629
2698.376998	160771.800891	56.676634
2697.561175	160553.860778	56.681639
2696.771514	160347.220437	56.686644
2696.283433	160144.538347	56.691649
2695.573662	159931.302044	56.696653
2694.866933	159721.639061	56.701658
2694.103340	159513.257681	56.706663
2693.626658	159297.725258	56.711668
2692.290205	159094.052091	56.716673
2691.797727	158882.974387	56.721677
2691.417021	158677.969874	56.726682
2690.706055	158476.654842	56.731687
2690.370570	158266.013648	56.736692
2689.304857	158072.181581	56.741697
2688.870017	157861.189891	56.746701
2688.066022	157649.329926	56.751706
2687.030353	157444.588971	56.756711
2686.655229	157236.185017	56.761716
2685.921660	157044.645192	56.766721
2685.501050	156836.009312	56.771725
2684.889056	156636.316458	56.776730
2683.768819	156435.268782	56.781735
2683.339125	156231.608547	56.786740
2682.719115	156037.793530	56.791745
2682.169945	155820.895781	56.796749
2681.517512	155614.604941	56.801754
2680.679283	155418.234738	56.806759
2680.546117	155205.393679	56.811764
2679.667977	155001.608423	56.816769
2678.959779	154801.877950	56.821773
2678.269923	154587.565406	56.826778
2677.457365	154373.082983	56.831783
2677.067839	154168.958373	56.836788
2676.293834	153977.175203	56.841793
2675.711399	153758.554415	56.846797
2674.990274	153546.388948	56.851802
2674.260221	153340.213232	56.856807
2673.695849	153135.105694	56.861812
2673.067815	152929.018033	56.866817
2672.293838	152708.947237	56.871821
2671.788688	152507.164452	56.876826
2670.925666	152299.440070	56.881831
2670.574985	152084.276276	56.886836
2669.333202	151887.189843	56.891841
2668.936385	151676.561009	56.896845
2668.210609	151475.912562	56.901850
2667.523433	151270.848691	56.906855
2666.616694	151064.664238	56.911860
2666.117535	150869.563431	56.916865
2665.737988	150664.848613	56.921869
2664.832934	150459.277784	56.926874
2663.998189	150251.536395	56.931879
2663.429739	150057.722404	56.936884
2662.611141	149863.250153	56.941889
2662.001433	149650.240454	56.946893
2661.399569	149446.725086	56.951898
2660.541516	149246.683194	56.956903
2660.204156	149046.598165	56.961908
2659.560187	148847.808483	56.966913
2658.869278	148646.599960	56.971917
2658.120891	148443.228500	56.976922
2657.528990	148239.109100	56.981927
2657.119871	148042.168146	56.986932
2655.888946	147845.193392	56.991937
2655.162817	147634.528491	56.996941
2654.699799	147430.012545	57.001946
2653.748153	147239.860101	57.006951
2653.386783	147035.966016	57.011956
2652.616408	146841.453528	57.016961
2652.026846	146643.266201	57.021965
2651.403100	146442.823404	57.026970
2650.597646	146246.172374	57.031975
2650.108236	146044.592464	57.036980
2649.588130	145859.984309	57.041985
2649.182320	145649.281808	57.046989
2648.221070	145447.983802	57.051994
2647.358406	145246.912916	57.056999
2646.867683	145047.347468	57.062004
2646.176818	144850.598034	57.067009
2645.579907	144642.232697	57.072013
2644.868207	144450.038487	57.077018
2643.846763	144248.236708	57.082023
2643.621117	144041.138152	57.087028
2642.840286	143855.032791	57.092033
2642.133447	143659.271879	57.097037
2641.683372	143454.093494	57.102042
2640.811167	143255.616547	57.107047
2640.518455	143048.331924	57.112052
2639.798583	142854.115737	57.117057
2639.147721	142644.590590	57.122061
2638.595255	142434.936914	57.127066
2637.799289	142234.739022	57.132071
2637.443115	142030.609894	57.137076
2636.461989	141829.414739	57.142081
2635.729092	141626.694904	57.147085
2635.280519	141425.570501	57.152090
2634.525933	141228.701739	57.157095
2633.759385	141020.425850	57.162100
2633.014657	140817.433732	57.167105
2632.322914	140613.354550	57.172109
2631.973995	140416.490300	57.177114
2631.134843	140217.697462	57.182119
2630.556002	139997.798275	57.187124
2629.874899	139807.788288	57.192129
2628.966040	139598.375796	57.197133
2628.616898	139387.414919	57.202138
2627.828958	139195.278474	57.207143
2627.348472	138976.578193	57.212148
2626.595525	138784.222844	57.217153
2625.623924	138578.168937	57.222157
2625.137039	138377.350427	57.227162
2624.250080	138176.291742	57.232167
2623.632250	137970.910166	57.237172
2622.997288	137785.835263	57.242177
2622.361101	137584.397810	57.247181
2621.779024	137377.020010	57.252186
2620.964069	137180.644730	57.257191
2620.427026	136977.937926	57.262196
2619.606215	136780.397410	57.267201
2618.960541	136580.797753	57.272205
2618.579721	136378.934216	57.277210
2617.606591	136181.587014	57.282215
2617.336056	135972.238679	57.287220
2616.428460	135784.322983	57.292225
2615.534047	135586.497265	57.297229
2614.992030	135386.343040	57.302234
2614.113806	135180.971368	57.307239
2613.543894	134977.851667	57.312244
2612.928233	134790.645635	57.317249
2612.116987	134592.521305	57.322253
2611.598299	134406.687074	57.327258
2610.816773	134208.789321	57.332263
2610.661024	133997.722027	57.337268
2609.951044	133816.469693	57.342273
2608.986637	133621.729943	57.347277
2608.362984	133412.113023	57.352282
2607.550092	133219.676646	57.357287
2606.912117	133031.774182	57.362292
2606.263237	132825.214240	57.367297
2605.696003	132629.414759	57.372301
2605.187456	132435.804874	57.377306
2604.362893	132249.778996	57.382311
2603.872530	132042.450139	57.387316
2603.019414	131846.294855	57.392321
2602.374694	131644.150526	57.397325
2602.067197	131451.925422	57.402330
2600.917264	131248.746177	57.407335
2600.337720	131051.536864	57.412340
2599.794537	130867.723707	57.417345
2599.465221	130659.566512	57.422349
2599.237904	130457.707458	57.427354
2597.990905	130260.279201	57.432359
2597.678745	130046.242947	57.437364
2596.853957	129857.501994	57.442369
2596.072979	129649.512758	57.447373
2595.225542	129446.730429	57.452378
2594.870669	129252.190803	57.457383
2594.112375	129048.177923	57.462388
2593.364556	128844.634813	57.467393
2592.754478	128639.725064	57.472397
2592.191638	128438.009950	57.477402
2591.194483	128254.171580	57.482407
2590.629766	128039.606499	57.487412
2589.889816	127847.423840	57.492417
2588.990145	127642.186339	57.497421
2588.626350	127444.866678	57.502426
2587.668290	127257.752040	57.507431
2587.213160	127048.054209	57.512436
2586.595964	126861.523256	57.517441
2586.058301	126651.866925	57.522445
2585.713042	126456.634217	57.527450
2584.648914	126266.304662	57.532455
2584.203827	126060.257641	57.537460
2583.751995	125859.407398	57.542465
2582.491900	125653.810097	57.547469
2582.473249	125454.989609	57.552474
2581.358679	125252.559841	57.557479
2580.871862	125051.340121	57.562484
2579.789034	124853.607030	57.567489
2579.276404	124657.588287	57.572493
2578.426580	124459.249691	57.577498
2577.591370	124270.815380	57.582503
2577.192971	124075.112930	57.587508
2576.752353	123873.653372	57.592513
2575.738496	123677.010057	57.597517
2575.203459	123487.962213	57.602522
2574.394747	123288.939998	57.607527
2573.663066	123096.332419	57.612532
2572.772874	122911.484588	57.617537
2572.525352	122715.857018	57.622541
2572.030272	122509.006922	57.627546
2571.077696	122325.734895	57.632551
2570.569917	122133.111474	57.637556
2569.896458	121940.896639	57.642561
2569.351279	121750.300869	57.647565
2568.471602	121547.061864	57.652570
2567.590448	121354.236617	57.657575
2567.329497	121162.647712	57.662580
2566.411468	120977.970106	57.667585
2565.777128	120794.988355	57.672589
2565.179433	120594.175253	57.677594
2564.330133	120408.398789	57.682599
2563.893597	120206.496549	57.687604
2563.573554	120015.268165	57.692609
2562.927556	119819.826714	57.697613
2562.013709	119622.588153	57.702618
2561.349148	119431.418630	57.707623
2560.746469	119229.404237	57.712628
2559.888701	119041.435966	57.717633
2559.473958	118851.138892	57.722637
2558.861634	118650.565196	57.727642
2557.871349	118471.839493	57.732647
2557.453644	118265.943635	57.737652
2556.661950	118064.577650	57.742657
2556.051808	117873.283990	57.747661
2555.355548	117681.211909	57.752666
2555.059138	117484.367799	57.757671
2554.173840	117277.258960	57.762676
2553.374720	117085.924910	57.767681
2552.768593	116891.089516	57.772685
2552.340383	116697.376320	57.777690
2551.194548	116507.599567	57.782695
2550.433705	116306.032961	57.787700
2550.127515	116119.636187	57.792705
2549.254574	115920.870579	57.797709
2548.912374	115728.750628	57.802714
2547.927226	115537.349718	57.807719
2547.348306	115344.045146	57.812724
2546.556860	115163.140160	57.817729
2545.898644	114969.413043	57.822733
2545.506237	114769.228306	57.827738
2544.769345	114586.071894	57.832743
2544.205775	114392.772129	57.837748
2543.682824	114186.919376	57.842753
2542.834595	113998.516852	57.847757
2542.192853	113801.844722	57.852762
2541.372805	113610.952640	57.857767
2540.717414	113407.970627	57.862772
2540.047578	113213.065614	57.867777
2539.452699	113023.913045	57.872781
2539.283428	112829.820209	57.877786
2538.269463	112645.788858	57.882791
2537.523269	112450.425881	57.887796
2536.758702	112257.161692	57.892801
2536.006372	112066.086591	57.897805
2535.702570	111864.216420	57.902810
2534.648399	111684.006384	57.907815
2534.263793	111485.261813	57.912820
2533.745851	111292.619689	57.917825
2532.749528	111102.028559	57.922829
2532.341337	110905.120082	57.927834
2531.712036	110709.162058	57.932839
2530.900938	110511.736729	57.937844
2530.030870	110328.943557	57.942849
2529.546410	110130.815862	57.947853
2528.613048	109939.075104	57.952858
2528.153672	109748.790067	57.957863
2527.467833	109554.392229	57.962868
2527.266187	109364.811776	57.967873
2526.033954	109171.322183	57.972877
2525.819660	108977.679119	57.977882
2524.862143	108795.583861	57.982887
2524.097252	108595.412608	57.987892
2523.403068	108414.325474	57.992897
2522.705851	108224.026530	57.997901
2522.281237	108021.299592	58.002906
2521.416921	107841.823692	58.007911
2521.024572	107650.497378	58.012916
2520.227981	107452.561415	58.017921
2519.549311	107268.726506	58.022925
2518.877948	107061.896913	58.027930
2518.084763	106882.055173	58.032935
2517.654885	106687.335084	58.037940
2517.086224	106496.953180	58.042945
2516.390146	106313.153683	58.047949
2515.829958	106111.200250	58.052954
2515.077987	105918.548770	58.057959
2514.560223	105726.413712	58.062964
2513.883850	105528.480833	58.067969
2513.091201	105347.254634	58.072973
2512.348262	105138.435301	58.077978
2511.586379	104948.908421	58.082983
2511.233845	104753.195655	58.087988
2510.239837	104561.913132	58.092993
2509.645594	104373.937689	58.097997
2509.524599	104169.589923	58.103002
2508.400438	103986.555013	58.108007
2507.838367	103786.264719	58.113012
2507.397697	103594.781729	58.118017
2506.363675	103400.139765	58.123021
2505.612361	103199.687758	58.128026
2504.719294	103008.097248	58.133031
2504.304737	102826.665393	58.138036
2503.517538	102636.031763	58.143041
2502.606213	102446.389977	58.148045
2502.524409	102256.764139	58.153050
2501.455805	102075.663785	58.158055
2500.821607	101877.989412	58.163060
2500.383814	101684.079131	58.168065
2499.433346	101504.188808	58.173069
2498.853112	101301.359672	58.178074
2498.626746	101119.841397	58.183079
2497.839314	100934.017398	58.188084
2497.070179	100744.335140	58.193089
2496.502609	100550.588053	58.198093
2495.994240	100350.642057	58.203098
2495.122588	100166.271142	58.208103
2494.322254	99970.529580	58.213108
2493.855840	99782.989271	58.218113
2493.086748	99595.168616	58.223117
2492.654950	99394.108674	58.228122
2491.748695	99208.850147	58.233127
2490.894224	99017.958645	58.238132
2490.167860	98830.086695	58.243137
2489.329134	98646.115951	58.248141
2488.906533	98455.002083	58.253146
2487.931198	98270.878397	58.258151
2487.298416	98081.228089	58.263156
2486.944410	97902.952026	58.268161
2486.194591	97732.452765	58.273165
2485.693870	97534.806982	58.278170
2485.020868	97351.505356	58.283175
2484.384930	97160.385365	58.288180
2483.864600	96977.398694	58.293185
2482.727941	96793.597888	58.298189
2482.520202	96595.222480	58.303194
2481.650064	96411.858186	58.308199
2480.941696	96231.336422	58.313204
2480.305543	96038.069531	58.318209
2479.390922	95865.010082	58.323213
2478.862375	95676.308244	58.328218
2478.432357	95490.224305	58.333223
2477.962699	95305.200951	58.338228
2477.320189	95117.200440	58.343233
2476.464660	94929.964580	58.348237
2476.096676	94728.364866	58.353242
2475.491444	94542.899967	58.358247
2474.409552	94350.307974	58.363252
2473.844987	94167.262265	58.368257
2473.202647	93976.531667	58.373261
2472.418901	93786.655852	58.378266
2471.749076	93602.432891	58.383271
2471.079714	93417.513816	58.388276
2470.483093	93220.301459	58.393281
2469.807029	93040.529440	58.398285
2469.393696	92850.564817	58.403290
2468.475065	92669.280633	58.408295
2467.839628	92478.809047	58.413300
2467.553447	92277.586248	58.418305
2466.619041	92093.240163	58.423309
2465.894401	91906.142061	58.428314
2465.123350	91723.472551	58.433319
2464.604459	91529.040229	58.438324
2464.187092	91347.731777	58.443329
2462.857314	91161.230500	58.448333
2462.881633	90959.025687	58.453338
2462.135637	90781.730612	58.458343
2461.431457	90588.153909	58.463348
2460.644167	90396.874696	58.468353
2460.003559	90210.544872	58.473357
2459.478986	90021.624002	58.478362
2458.545430	89832.325768	58.483367
2457.606292	89638.319165	58.488372
2456.873990	89461.038936	58.493377
2456.647823	89278.138519	58.498381
2456.267138	89083.978563	58.503386
2455.392973	88903.263605	58.508391
2454.649345	88705.512633	58.513396
2454.246520	88527.338191	58.518401
2453.641996	88332.833678	58.523405
2453.073551	88131.363946	58.528410
2452.404746	87949.546576	58.533415
2451.495661	87763.426048	58.538420
2450.618695	87564.419632	58.543425
2450.197321	87378.605482	58.548429
2449.511280	87189.043778	58.553434
2448.684150	86992.367725	58.558439
2447.888115	86802.554255	58.563444
2447.182445	86619.536737	58.568449
2446.499727	86435.635957	58.573453
2445.996221	86257.572261	58.578458
2445.222962	86069.048551	58.583463
2444.750898	85881.004907	58.588468
2444.346794	85688.514692	58.593473
2443.268398	85499.239295	58.598477
2443.001066	85311.624614	58.603482
2442.133558	85127.257235	58.608487
2441.630197	84933.946460	58.613492
2440.991214	84740.310298	58.618497
2440.292586	84548.574337	58.623501
2439.735198	84366.230851	58.628506
2438.841446	84177.115412	58.633511
2437.986181	83984.287417	58.638516
2437.748924	83797.562390	58.643521
2436.747445	83609.179026	58.648525
2436.084265	83404.561437	58.653530
2435.372490	83234.675681	58.658535
2434.674944	83047.003421	58.663540
2434.021826	82858.533490	58.668545
2433.223903	82680.527398	58.673549
2432.780931	82485.511705	58.678554
2432.197886	82303.830237	58.683559
2431.459826	82109.809203	58.688564
2431.199004	81919.288977	58.693569
2429.946729	81741.426258	58.698573
2429.732006	81540.045130	58.703578
2428.864652	81354.975442	58.708583
2428.048139	81166.920540	58.713588
2427.563909	80993.670450	58.718593
2426.759246	80805.242997	58.723597
2426.209971	80622.639117	58.728602
2425.343664	80426.613300	58.733607
2424.533823	80247.311567	58.738612
2424.024940	80067.520037	58.743617
2423.349072	79880.994466	58.748621
2422.704735	79686.854350	58.753626
2421.980145	79499.503398	58.758631
2421.235650	79328.513845	58.763636
2420.664652	79143.733714	58.768641
2420.361839	78962.303107	58.773645
2419.542577	78776.000344	58.778650
2419.001828	78600.611897	58.783655
2418.080095	78406.464418	58.788660
2417.605225	78209.066771	58.793665
2416.817389	78036.662649	58.798669
2416.237063	77853.505137	58.803674
2415.599078	77663.609727	58.808679
2414.696960	77481.190931	58.813684
2414.342043	77290.905572	58.818689
2413.209775	77115.934087	58.823693
2412.772373	76928.928528	58.828698
2412.173215	76753.007515	58.833703
2411.639591	76566.882291	58.838708
2411.091676	76373.556563	58.843713
2410.248619	76193.927907	58.848717
2409.596091	76002.282408	58.853722
2409.094415	75821.722171	58.858727
2408.336892	75643.003571	58.863732
2407.761861	75448.132246	58.868737
2407.019891	75262.172382	58.873741
2406.558229	75067.426135	58.878746
2405.602517	74884.145735	58.883751
2404.923786	74698.371104	58.888756
2404.502216	74519.425415	58.893761
2403.556464	74342.408128	58.898765
2403.291314	74148.539255	58.903770
2402.279148	73964.268790	58.908775
2401.761899	73775.993488	58.913780
2400.962913	73588.664262	58.918785
2400.433091	73396.238416	58.923789
2399.771553	73207.047343	58.928794
2399.195894	73021.354211	58.933799
2398.057214	72841.270096	58.938804
2397.540637	72652.010599	58.943809
2396.977325	72475.227891	58.948813
2396.240488	72285.366941	58.953818
2395.613875	72109.161335	58.958823
2394.843659	71918.453940	58.963828
2394.136937	71737.557433	58.968833
2393.156774	71562.629029	58.973837
2392.823057	71376.729129	58.978842
2392.220877	71198.031804	58.983847
2391.492510	71016.714529	58.988852
2391.239672	70831.845797	58.993857
2390.534779	70654.487261	58.998861
2389.748339	70468.344598	59.003866
2388.727775	70290.082872	59.008871
2388.487298	70099.042928	59.013876
2387.699402	69911.993585	59.018881
2387.036936	69735.618397	59.023885
2386.475548	69547.225405	59.028890
2385.776846	69363.669952	59.033895
2384.907137	69198.999969	59.038900
2384.497842	69001.587318	59.043905
2383.990372	68817.449251	59.048909
2383.203243	68625.522189	59.053914
2382.274665	68451.607619	59.058919
2381.494809	68275.023479	59.063924
2380.836396	68085.665498	59.068929
2380.109982	67913.421106	59.073933
2379.891625	67733.433969	59.078938
2379.083482	67543.287953	59.083943
2378.163514	67360.141058	59.088948
2377.899785	67181.173244	59.093953
2377.262749	66998.972904	59.098957
2376.682295	66806.935961	59.103962
2375.802968	66629.977171	59.108967
2375.560432	66445.249493	59.113972
2375.116791	66260.425634	59.118977
2374.473330	66068.545324	59.123981
2373.472995	65874.269456	59.128986
2372.753983	65690.884805	59.133991
2372.067902	65498.377284	59.138996
2371.335447	65314.051576	59.144001
2370.506671	65132.060705	59.149005
2370.022610	64939.526733	59.154010
2369.140884	64753.114936	59.159015
2368.555723	64570.786778	59.164020
2368.026457	64382.793361	59.169025
2367.012512	64206.090300	59.174029
2366.509854	64021.066144	59.179034
2366.096184	63838.553111	59.184039
2365.364571	63645.488800	59.189044
2364.719626	63455.946083	59.194049
2364.094662	63284.423447	59.199053
2363.240492	63087.059340	59.204058
2362.178238	62905.854837	59.209063
2361.820177	62727.535423	59.214068
2361.296282	62538.356221	59.219073
2360.386554	62358.104700	59.224077
2359.805216	62175.703821	59.229082
2359.256286	61999.387531	59.234087
2358.500489	61823.596391	59.239092
2357.673125	61642.746595	59.244097
2357.060431	61457.084150	59.249101
2356.439985	61276.274691	59.254106
2355.675549	61102.941911	59.259111
2355.548032	60926.508642	59.264116
2355.242637	60736.154144	59.269121
2354.109469	60565.316007	59.274125
2353.413136	60366.578159	59.279130
2352.972308	60180.150778	59.284135
2352.084550	60002.457035	59.289140
2351.543227	59816.558850	59.294145
2350.707913	59633.412444	59.299149
2350.217426	59453.270968	59.304154
2349.338877	59265.418499	59.309159
2348.591856	59085.840367	59.314164
2348.300364	58886.370278	59.319169
2346.993567	58715.988025	59.324173
2346.736389	58529.744191	59.329178
2346.050263	58343.829791	59.334183
2345.307145	58165.269615	59.339188
2344.764883	57980.222294	59.344193
2343.967098	57807.381074	59.349197
2343.464187	57622.286762	59.354202
2342.666544	57443.602897	59.359207
2342.000054	57258.072887	59.364212
2341.373509	57073.472086	59.369217
2340.219441	56896.888304	59.374221
2339.789720	56725.071743	59.379226
2338.935599	56549.238125	59.384231
2338.084043	56364.512341	59.389236
2337.410921	56193.460925	59.394241
2336.826403	56024.223170	59.399245
2336.464945	55845.552038	59.404250
2335.777221	55674.697643	59.409255
2335.063831	55501.358226	59.414260
2334.878044	55316.094305	59.419265
2333.962502	55142.470693	59.424269
2333.168946	54957.699196	59.429274
2332.696587	54782.192185	59.434279
2331.761286	54602.171574	59.439284
2331.521945	54431.605749	59.444289
2330.673412	54246.774192	59.449293
2330.414972	54063.145214	59.454298
2329.517892	53891.698239	59.459303
2328.628022	53712.473477	59.464308
2327.890536	53519.290148	59.469313
2326.993867	53357.907861	59.474317
2326.368435	53181.785472	59.479322
2326.004021	53003.265959	59.484327
2325.530550	52829.496139	59.489332
2324.666802	52640.832324	59.494337
2324.057761	52471.868654	59.499341
2323.730148	52302.801805	59.504346
2322.946296	52117.231706	59.509351
2321.690694	51935.538476	59.514356
2321.405235	51757.154767	59.519361
2320.780537	51576.836404	59.524365
2320.100520	51405.739201	59.529370
2319.448888	51226.748022	59.534375
2318.529468	51057.312078	59.539380
2318.142584	50871.508315	59.544385
2317.505492	50703.103514	59.549389
2317.094617	50517.297721	59.554394
2316.571354	50331.271219	59.559399
2315.512938	50156.828920	59.564404
2315.133287	49970.115815	59.569409
2314.233869	49788.606079	59.574413
2313.658466	49608.258512	59.579418
2313.318530	49425.948716	59.584423
2312.469079	49249.618690	59.589428
2311.674474	49066.672839	59.594433
2310.768086	48890.124448	59.599437
2310.266974	48704.434035	59.604442
2309.694388	48527.374414	59.609447
2308.726951	48351.831234	59.614452
2308.439025	48164.084826	59.619457
2307.416698	47985.222817	59.624461
2306.551973	47813.297155	59.629466
2306.198559	47640.792250	59.634471
2305.653679	47463.156774	59.639476
2305.013248	47270.461791	59.644481
2304.235175	47095.770924	59.649485
2303.866229	46918.606483	59.654490
2303.136382	46742.314009	59.659495
2302.038895	46564.579081	59.664500
2301.210524	46389.033300	59.669505
2300.788155	46215.733968	59.674509
2300.147724	46031.858691	59.679514
2299.405723	45853.334390	59.684519
2298.641319	45682.438396	59.689524
2298.444435	45508.480819	59.694529
2297.347022	45330.701409	59.699533
2297.094086	45146.407031	59.704538
2296.109952	44964.988623	59.709543
2295.505996	44809.877622	59.714548
2295.191746	44626.983775	59.719553
2294.453117	44455.311266	59.724557
2293.695778	44274.389078	59.729562
2292.950756	44089.228714	59.734567
2292.070657	43914.443342	59.739572
2291.840044	43734.581791	59.744577
2290.950880	43573.546353	59.749581
2290.221024	43390.503667	59.754586
2289.356409	43209.840418	59.759591
2288.883759	43038.218748	59.764596
2288.589474	42857.699569	59.769601
2287.592530	42685.775547	59.774605
2286.731247	42510.748304	59.779610
2286.427069	42335.201213	59.784615
2285.648345	42160.442711	59.789620
2285.212169	41986.229332	59.794625
2284.199646	41818.525520	59.799629
2283.611534	41632.616993	59.804634
2282.938992	41447.416398	59.809639
2281.988034	41271.694928	59.814644
2281.719248	41105.843836	59.819649
2280.641369	40931.926290	59.824653
2280.457346	40754.845713	59.829658
2279.508494	40590.378639	59.834663
2278.803951	40414.848186	59.839668
2278.317703	40240.091228	59.844673
2277.527279	40068.732879	59.849677
2276.643275	39890.649719	59.854682
2276.189620	39716.658130	59.859687
2275.442000	39553.789588	59.864692
2274.945362	39381.011343	59.869697
2274.337496	39214.459229	59.874701
2273.629799	39036.238433	59.879706
2273.048639	38858.687120	59.884711
2271.985112	38683.201338	59.889716
2271.578277	38505.980167	59.894721
2270.773000	38342.787703	59.899725
2269.920716	38182.522486	59.904730
2269.581107	38006.225390	59.909735
2268.912360	37838.592974	59.914740
2268.278584	37657.459887	59.919745
2267.587922	37494.221039	59.924750
2266.697570	37325.874813	59.929754
2266.303566	37157.443628	59.934759
2265.662360	36984.458158	59.939764
2265.098338	36804.190951	59.944769
2264.289906	36638.957307	59.949774
2263.557641	36468.610771	59.954778
2262.638932	36300.668102	59.959783
2261.922863	36129.609543	59.964788
2261.485195	35961.571822	59.969793
2260.997740	35800.673828	59.974798
2260.392810	35623.526898	59.979802
2259.670960	35453.729540	59.984807
2258.855849	35293.662857	59.989812
2258.344119	35115.049222	59.994817
2258.037807	34947.264756	59.999822
2257.352287	34777.587018	60.004826
2256.493632	34595.800204	60.009831
2255.882259	34426.574187	60.014836
2255.363529	34246.060120	60.019841
2254.598233	34080.111470	60.024846
2253.917711	33904.772710	60.029850
2253.442011	33727.996729	60.034855
2252.485326	33557.571537	60.039860
2251.667403	33378.035694	60.044865
2251.011714	33209.582892	60.049870
2250.205529	33034.832672	60.054874
2249.989689	32862.838413	60.059879
2248.850359	32702.912789	60.064884
2248.088169	32531.073424	60.069889
2247.660929	32367.374931	60.074894
2246.971230	32194.729506	60.079898
2246.439163	32031.357533	60.084903
2245.583933	31869.569689	60.089908
2245.428976	31694.311529	60.094913
2244.582757	31527.028001	60.099918
2243.480031	31357.457651	60.104922
2243.150534	31174.129462	60.109927
2242.622401	31010.465143	60.114932
2242.451697	30830.882682	60.119937
2241.293074	30667.724718	60.124942
2240.204127	30493.613466	60.129946
2239.919012	30321.994766	60.134951
2238.964159	30155.857942	60.139956
2238.459013	29976.818200	60.144961
2238.018627	29815.559865	60.149966
2237.281863	29642.272382	60.154970
2236.363684	29478.238045	60.159975
2235.781231	29304.209173	60.164980
2235.259299	29133.086035	60.169985
2234.392511	28957.616034	60.174990
2233.933535	28787.589340	60.179994
2233.133336	28611.477356	60.184999
2232.382027	28458.397822	60.190004
2231.969369	28280.851826	60.195009
2231.189904	28117.197811	60.200014
2230.379938	27945.889512	60.205018
2229.787165	27770.635279	60.210023
2229.096482	27619.072254	60.215028
2228.422138	27447.144200	60.220033
2227.564367	27283.150806	60.225038
2227.368455	27115.504301	60.230042
2226.746244	26941.653894	60.235047
2225.703989	26785.332980	60.240052
2225.438803	26602.382340	60.245057
2224.616842	26443.675186	60.250062
2223.812928	26273.292724	60.255066
2223.223740	26102.684484	60.260071
2222.404731	25942.034829	60.265076
2221.945569	25775.504715	60.270081
2221.087241	25609.924241	60.275086
2220.222653	25446.947308	60.280090
2219.980607	25273.434447	60.285095
2218.800044	25109.407705	60.290100
2218.577925	24942.038278	60.295105
2217.787134	24776.268491	60.300110
2217.314881	24614.570902	60.305114
2216.713583	24451.090808	60.310119
2215.910136	24286.352413	60.315124
2215.423041	24106.441904	60.320129
2214.486875	23949.259829	60.325134
2214.068320	23782.014219	60.330138
2213.474984	23608.377658	60.335143
2212.490886	23449.306457	60.340148
2212.015471	23276.152319	60.345153
2211.180702	23116.956501	60.350158
2210.543657	22950.066984	60.355162
2210.050454	22783.833941	60.360167
2209.075974	22613.366588	60.365172
2208.505307	22449.268805	60.370177
2207.615313	22289.858647	60.375182
2206.920486	22134.135997	60.380186
2206.594605	21959.930905	60.385191
2205.455322	21806.218176	60.390196
2205.215108	21635.002079	60.395201
2204.223725	21482.065760	60.400206
2203.462618	21316.569642	60.405210
2203.211334	21159.004062	60.410215
2202.228805	21002.073241	60.415220
2201.865632	20845.565266	60.420225
2201.170067	20672.227305	60.425230
2200.351871	20522.488732	60.430234
2199.951089	20357.213951	60.435239
2198.922276	20192.166864	60.440244
2198.784980	20030.382208	60.445249
2197.976378	19874.276668	60.450254
2196.926107	19709.201336	60.455258
2196.366643	19549.520839	60.460263
2195.588927	19393.613341	60.465268
2194.812217	19226.169841	60.470273
2194.316808	19075.918548	60.475278
2193.496699	18922.264229	60.480282
2193.186701	18762.266369	60.485287
2192.311805	18606.464220	60.490292
2191.679726	18460.399049	60.495297
2191.255200	18294.829998	60.500302
2190.587418	18135.861990	60.505306
2189.789234	17974.704674	60.510311
2189.089290	17815.007699	60.515316
2188.383372	17651.841820	60.520321
2187.764900	17498.971160	60.525326
2186.859616	17351.700983	60.530330
2186.541667	17189.379897	60.535335
2185.668652	17034.563711	60.540340
2185.100368	16870.800818	60.545345
2184.418266	16726.070598	60.550350
2183.454498	16567.257912	60.555354
2182.844174	16410.224854	60.560359
2181.998679	16257.587325	60.565364
2181.842489	16096.926397	60.570369
2181.186131	15941.399420	60.575374
2180.185983	15792.663292	60.580378
2179.738849	15635.121826	60.585383
2179.114084	15489.355509	60.590388
2178.320487	15335.147321	60.595393
2177.655127	15182.646914	60.600398
2177.060387	15026.471153	60.605402
2176.416658	14875.020898	60.610407
2175.821443	14720.202029	60.615412
2175.133560	14569.288228	60.620417
2174.565220	14421.976378	60.625422
2173.997201	14269.172013	60.630426
2173.184669	14099.251516	60.635431
2172.401659	13952.861675	60.640436
2171.535060	13795.373792	60.645441
2171.082594	13647.845900	60.650446
2170.272793	13498.864363	60.655450
2169.393596	13343.583831	60.660455
2168.351453	13191.004913	60.665460
2168.328276	13032.974546	60.670465
2167.508338	12895.625308	60.675470
2166.770145	12748.384365	60.680474
2166.029273	12597.696642	60.685479
2165.539654	12464.545758	60.690484
2164.810624	12320.347050	60.695489
2163.929720	12171.472387	60.700494
2163.643931	12026.281554	60.705498
2162.804840	11872.922071	60.710503
2162.028980	11733.336856	60.715508
2161.479017	11583.327631	60.720513
2160.585747	11448.843760	60.725518
2159.806888	11307.564380	60.730522
2159.471331	11162.039915	60.735527
2158.536101	11031.051416	60.740532
2157.709459	10872.659975	60.745537
2157.386368	10737.685759	60.750542
2156.287157	10597.231581	60.755546
2155.725448	10459.428283	60.760551
2154.833460	10332.459780	60.765556
2154.221993	10190.546816	60.770561
2153.589036	10064.295363	60.775566
2152.905219	9928.086649	60.780570
2152.605689	9792.495364	60.785575
2151.485945	9673.827191	60.790580
2150.727904	9537.408711	60.795585
2150.108586	9408.676390	60.800590
2149.100688	9277.717957	60.805594
2148.657074	9153.232330	60.810599
2147.224384	9046.761239	60.815604
2146.434289	8923.891902	60.820609
2145.746193	8805.497395	60.825614
2145.060067	8699.150156	60.830618
2144.144552	8587.289368	60.835623
2143.431385	8487.495463	60.840628
2142.787438	8387.999715	60.845633
2142.026815	8280.617173	60.850638
2141.167476	8176.949981	60.855642
2140.760517	8077.727948	60.860647
2139.747187	7988.292744	60.865652
2138.855610	7887.171035	60.870657
2138.284926	7792.516309	60.875662
2137.766652	7704.844388	60.880666
2137.185154	7599.666183	60.885671
2136.474429	7520.020634	60.890676
2135.783354	7415.616086	60.895681
2134.733655	7328.136802	60.900686
2134.456385	7232.138578	60.905690
2133.821312	7136.795714	60.910695
2133.124889	7047.402630	60.915700
2132.489944	6947.495737	60.920705
2131.851407	6861.799110	60.925710
2131.186644	6777.034837	60.930714
2130.905988	6679.295742	60.935719
2129.832615	6587.060269	60.940724
2129.409766	6495.073576	60.945729
2128.574047	6407.704574	60.950734
2127.734547	6314.806155	60.955738
2127.385972	6221.713670	60.960743
2126.730420	6145.563199	60.965748
2125.982191	6040.833805	60.970753
2125.541532	5950.815887	60.975758
2124.642888	5858.677499	60.980762
2123.920750	5769.517819	60.985767
2123.665782	5686.087765	60.990772
2122.777292	5589.226877	60.995777
2122.285454	5496.025992	61.000782
2121.728081	5418.252166	61.005786
2120.949467	5320.174274	61.010791
2120.023950	5233.125377	61.015796
2119.520183	5142.994586	61.020801
2119.022609	5047.865719	61.025806
2118.338487	4953.730933	61.030810
2117.612079	4866.088633	61.035815
2116.883724	4774.517585	61.040820
2116.244771	4681.438238	61.045825
2115.476714	4603.091630	61.050830
2114.931008	4511.441959	61.055834
2114.282085	4417.209564	61.060839
2113.667331	4334.425503	61.065844
2112.890692	4252.208660	61.070849
2112.207364	4145.030211	61.075854
2111.718198	4055.358029	61.080858
2110.969896	3965.899451	61.085863
2110.300719	3881.106679	61.090868
2109.539125	3789.894828	61.095873
2108.943551	3707.500858	61.100878
2108.134883	3611.896649	61.105882
2107.671646	3523.643230	61.110887
2107.014929	3446.911367	61.115892
2106.149430	3359.828498	61.120897
2105.557760	3273.421962	61.125902
2104.493381	3194.168469	61.130906
2103.800214	3106.975362	61.135911
2103.154753	3033.870940	61.140916
2102.545141	2952.141959	61.145921
2101.854552	2874.201562	61.150926
2101.060291	2811.909843	61.155930
2100.360175	2727.138094	61.160935
2099.840152	2646.117420	61.165940
2099.011816	2567.885053	61.170945
2098.561490	2493.915610	61.175950
2097.864573	2424.970593	61.180954
2097.547640	2346.654309	61.185959
2096.544223	2272.757191	61.190964
2095.933975	2202.052675	61.195969
2095.136873	2118.463044	61.200974
2094.003551	2051.179671	61.205978
2093.500397	1971.548788	61.210983
2092.644605	1913.700245	61.215988
2091.987208	1854.387566	61.220993
2091.534282	1782.519799	61.225998
2090.647868	1721.651041	61.231002
2090.114304	1653.699440	61.236007
2089.257574	1602.311599	61.241012
2088.455836	1527.685193	61.246017
2087.738376	1474.929593	61.251022
2086.803017	1429.437630	61.256026
2086.042542	1368.031481	61.261031
2085.107861	1324.032506	61.266036
2084.238615	1269.756142	61.271041
2083.815344	1233.721241	61.276046
2083.154167	1188.961678	61.281050
2082.297251	1139.800033	61.286055
2081.404022	1095.608284	61.291060
2080.543737	1054.696561	61.296065
2080.176057	1020.801388	61.301070
2079.076508	992.641656	61.306074
2078.660130	938.677896	61.311079
2077.971231	919.691776	61.316084
2077.210890	883.812167	61.321089
2076.767921	838.235242	61.326094
2075.845370	795.350945	61.331098
2075.371100	770.300201	61.336103
2074.969797	741.068132	61.341108
2074.396026	687.204405	61.346113
2073.616469	657.945792	61.351118
2072.850326	624.010694	61.356122
2072.204525	591.699874	61.361127
2071.352944	556.460071	61.366132
2070.796442	524.007489	61.371137
2070.408226	476.842801	61.376142
2069.645188	451.370053	61.381146
2069.477004	416.832736	61.386151
2068.497163	385.117890	61.391156
2067.892975	342.345269	61.396161
2067.336712	308.926409	61.401166
2066.028592	269.714680	61.406170
2065.673055	226.865089	61.411175
2064.899838	200.586965	61.416180
2064.222089	164.185079	61.421185
2063.734903	131.236656	61.426190
2063.027770	105.579021	61.431194
2062.457172	58.873582	61.436199
2061.926201	32.214321	61.441204
2061.093534	5.324650	61.446209
2060.716781	-38.517451	61.451214
2059.585159	-57.889349	61.456218
2059.115841	-102.243281	61.461223
2058.173126	-133.790985	61.466228
2057.659002	-164.679653	61.471233
2057.204400	-186.901186	61.476238
2056.159246	-213.993271	61.481242
2055.542851	-236.310477	61.486247
2054.691917	-266.744922	61.491252
2053.683328	-287.900659	61.496257
2053.344584	-321.734208	61.501262
2051.960030	-326.268970	61.506266
2051.128356	-340.182919	61.511271
2050.178964	-345.892186	61.516276
2047.795427	-296.897750	61.521281
2039.579180	-60.734706	61.526286
2039.477240	6.470836	61.531290
2040.989342	47.813168	61.536295
2042.898207	92.946061	61.541300
2044.551315	108.996282	61.546305
2045.798872	115.215160	61.551310
2046.465425	105.295691	61.556314
2046.349980	87.236832	61.561319
2046.476294	56.955708	61.566324
2045.758967	38.114833	61.571329
2045.132667	2.096296	61.576334
2043.637588	-18.779186	61.581338
2042.137748	-30.540447	61.586343
2040.582637	-42.357582	61.591348
2039.621529	-41.474863	61.596353
2038.904425	-45.587350	61.601358
2037.880161	-35.947038	61.606362
2037.506272	-36.490074	61.611367
2037.062537	-36.295031	61.616372
2036.493867	-36.966428	61.621377
2036.312875	-30.763746	61.626382
2035.521010	-32.298605	61.631386
2035.154096	-35.268160	61.636391
2034.344496	-37.445192	61.641396
2033.521502	-43.717119	61.646401
2032.715651	-39.050606	61.651406
2031.186411	-32.367427	61.656410
2030.601556	-35.379664	61.661415
2029.815321	-26.005786	61.666420
2029.224125	-20.654227	61.671425
2029.385158	-21.616485	61.676430
2028.692202	-13.451187	61.681434
2028.501801	-15.496256	61.686439
2027.897896	-17.150835	61.691444
2027.369576	-23.860632	61.696449
2026.823471	-28.642096	61.701454
2025.286793	-26.232955	61.706458
2024.626060	-23.078148	61.711463
2023.778672	-14.823683	61.716468
2023.065793	-17.088607	61.721473
2022.602688	-25.633334	61.726478
2021.727614	-7.311680	61.731482
2021.439565	-6.502662	61.736487
2020.820289	-11.092739	61.741492
2020.565792	-12.331253	61.746497
2020.101629	-8.627308	61.751502
2019.158575	-4.871007	61.756506
2018.494044	-12.808167	61.761511
2017.725170	-15.881086	61.766516
2017.080604	-13.402217	61.771521
2016.238221	-15.167179	61.776526
2015.228307	-14.521137	61.781530
2014.438491	-7.103724	61.786535
2014.331088	-6.033211	61.791540
2013.638947	5.382156	61.796545
2013.431991	4.057246	61.801550
2012.261516	0.333690	61.806554
2012.248183	-6.028909	61.811559
2011.071415	-8.959812	61.816564
2010.008960	3.802735	61.821569
2009.888054	7.199883	61.826574
2009.044353	13.122984	61.831578
2008.682592	0.570783	61.836583
2008.256681	0.785080	61.841588
2007.265454	-0.532044	61.846593
2006.683984	-9.777098	61.851598
2006.061218	2.898313	61.856602
2005.265272	-6.588674	61.861607
2004.397373	7.895037	61.866612
2003.659152	8.521615	61.871617
2003.214417	1.632961	61.876622
2002.615517	4.435756	61.881626
2001.999932	-0.621696	61.886631
2001.367232	8.997506	61.891636
2000.419296	16.581961	61.896641
2000.102093	5.967122	61.901646
1999.329761	10.781307	61.906650
1998.786568	9.878785	61.911655
1998.014926	6.779499	61.916660
1997.275462	9.338095	61.921665
1996.820369	-2.464405	61.926670
1995.975647	12.624353	61.931674
1995.214646	7.181540	61.936679
1994.574566	9.267033	61.941684
1993.897701	12.060128	61.946689
1993.930674	5.579787	61.951694
1992.965062	19.381989	61.956698
1991.556761	11.045628	61.961703
1991.180963	19.827678	61.966708
1990.435043	22.841478	61.971713
1990.244515	16.062284	61.976718
1989.595595	15.941389	61.981722
1989.275612	18.330899	61.986727
1988.145420	20.776474	61.991732
1986.909440	14.682059	61.996737
1986.687543	13.542454	62.001742
1986.097939	22.374213	62.006746
1985.535642	20.474909	62.011751
1985.376738	17.693113	62.016756
1984.277545	8.233759	62.021761
1982.910182	3.030708	62.026766
1982.387617	17.864904	62.031770
1981.953840	18.857913	62.036775
1981.994817	20.881038	62.041780
1981.000887	16.427705	62.046785
1980.752117	3.491712	62.051790
1979.558106	10.814024	62.056794
1978.647885	15.867729	62.061799
1977.897522	13.829542	62.066804
1977.365812	16.282625	62.071809
1977.369722	21.943455	62.076814
1976.053402	19.536199	62.081818
1975.518186	3.551609	62.086823
1974.757702	18.748434	62.091828
1973.819003	21.975770	62.096833
1974.308699	21.290929	62.101838
1973.292976	21.799135	62.106842
1972.464288	7.794524	62.111847
1971.887391	14.342352	62.116852
1971.227411	11.094458	62.121857
1970.867070	9.666162	62.126862
1970.064572	21.654167	62.131866
1969.209554	13.808750	62.136871
1967.876512	16.217144	62.141876
1967.303712	20.960241	62.146881
1967.303707	16.920013	62.151886
1966.556272	12.410213	62.156890
1965.502360	11.464186	62.161895
1964.681354	19.652994	62.166900
1964.620589	16.388831	62.171905
1963.825162	19.590273	62.176910
1962.959165	22.809227	62.181914
1962.475649	22.349836	62.186919
1961.969837	25.038515	62.191924
1961.275354	24.743505	62.196929
1960.762309	25.268117	62.201934
1960.249688	24.527910	62.206938
1959.507657	19.386454	62.211943
1959.008857	23.345079	62.216948
1957.618990	16.962862	62.221953
1957.077040	19.412844	62.226958
1956.060044	20.780721	62.231962
1955.578392	19.407955	62.236967
1954.886959	21.414876	62.241972
1954.845060	23.958948	62.246977
1954.042844	19.396343	62.251982
1953.343253	28.149373	62.256986
1952.829175	22.153270	62.261991
1952.028651	19.421290	62.266996
1951.293858	29.633899	62.272001
1951.074293	19.416736	62.277006
1950.639448	29.671618	62.282010
1949.615951	25.327072	62.287015
1948.555917	20.715508	62.292020
1947.693966	36.070390	62.297025
1947.066428	27.595912	62.302030
1946.305414	35.063983	62.307034
1945.691988	40.851204	62.312039
1945.375488	28.105727	62.317044
1944.682246	38.553027	62.322049
1944.454182	29.975708	62.327054
1943.831566	38.445282	62.332058
1943.281022	41.491162	62.337063
1942.023770	32.572584	62.342068
1941.007599	36.600731	62.347073
1940.432665	30.983306	62.352078
1939.693433	34.883909	62.357082
1939.351706	29.125382	62.362087
1938.632579	23.199682	62.367092
1938.260351	35.529417	62.372097
1937.583817	30.715044	62.377102
1937.325784	35.681003	62.382106
1936.692241	33.247378	62.387111
1936.092460	29.671380	62.392116
1935.014436	38.713159	62.397121
1933.873342	33.936265	62.402126
1933.413811	45.414097	62.407130
1932.814893	39.926638	62.412135
1932.360446	39.331747	62.417140
1931.646382	43.914352	62.422145
1931.260743	32.208054	62.427150
1930.110965	35.632924	62.432154
1929.334552	32.187473	62.437159
1928.438976	29.901108	62.442164
1927.916080	32.400113	62.447169
1927.765027	34.695003	62.452174
1927.065208	44.607175	62.457178
1926.494012	40.287027	62.462183
1925.997705	33.138475	62.467188
1925.687010	35.416130	62.472193
1924.717130	35.111231	62.477198
1923.460553	39.789426	62.482202
1923.077548	33.501274	62.487207
1922.575260	34.183463	62.492212
1921.784853	32.626323	62.497217
1921.274184	36.635729	62.502222
1919.879437	35.068874	62.507226
1919.004869	35.419070	62.512231
1918.617258	38.002258	62.517236
1918.330102	45.893443	62.522241
1918.084041	37.145512	62.527246
1917.165407	34.899082	62.532250
1916.921956	37.202334	62.537255
1916.532236	29.864972	62.542260
1914.996068	35.759264	62.547265
1914.141769	29.192691	62.552270
1913.358312	34.049672	62.557274
1912.851402	35.533710	62.562279
1911.978745	34.926368	62.567284
1911.656328	36.887333	62.572289
1911.636076	38.525928	62.577294
1911.101953	36.876063	62.582298
1910.179068	37.386902	62.587303
1909.398452	35.471810	62.592308
1908.304096	33.308477	62.597313
1907.827020	35.240377	62.602318
1907.114244	38.679459	62.607322
1906.751958	46.065318	62.612327
1906.273434	40.823688	62.617332
1904.495668	39.204106	62.622337
1904.237189	36.810294	62.627342
1903.355761	39.571236	62.632346
1902.813657	41.310029	62.637351
1902.643190	41.810227	62.642356
1902.004366	51.982391	62.647361
1901.880908	38.130755	62.652366
1901.176393	47.220487	62.657370
1900.292612	41.076499	62.662375
1899.442729	41.074266	62.667380
1898.326916	48.411021	62.672385
1897.998154	37.531506	62.677390
1897.420796	44.596686	62.682394
1896.665712	42.221792	62.687399
1895.921097	43.363517	62.692404
1894.539148	40.272841	62.697409
1894.495280	42.076040	62.702414
1893.623118	47.134776	62.707418
1893.150818	45.653300	62.712423
1892.846593	41.984652	62.717428
1892.081893	50.465760	62.722433
1891.827493	38.175643	62.727438
1891.300136	41.383435	62.732442
1890.067526	44.554962	62.737447
1889.371155	37.641614	62.742452
1888.714796	33.850676	62.747457
1888.268404	35.008134	62.752462
1887.591006	46.228815	62.757466
1886.649334	41.062301	62.762471
1885.955494	37.838725	62.767476
1884.994387	35.264727	62.772481
1884.390316	36.638037	62.777486
1883.777914	36.266935	62.782490
1883.189900	43.939375	62.787495
1882.881065	38.539919	62.792500
1882.287581	45.131409	62.797505
1881.973007	35.932303	62.802510
1881.230004	39.745207	62.807514
1879.753103	35.138353	62.812519
1879.377975	29.590150	62.817524
1878.590844	41.547361	62.822529
1878.305724	38.345629	62.827534
1877.875627	36.106806	62.832538
1877.312202	37.803256	62.837543
1876.495047	25.283950	62.842548
1875.484844	36.582698	62.847553
1874.884169	34.120216	62.852558
1874.408983	33.979649	62.857562
1873.689997	32.080017	62.862567
1872.705054	32.003039	62.867572
1871.762928	32.045424	62.872577
1871.243801	42.887728	62.877582
1870.855780	43.160688	62.882586
1870.117194	47.240986	62.887591
1869.749676	37.072550	62.892596
1869.310459	41.818115	62.897601
1868.888512	37.267699	62.902606
1867.713507	34.674053	62.907610
1866.759012	44.133071	62.912615
1866.338391	38.210458	62.917620
1865.550808	46.584812	62.922625
1865.048239	38.620383	62.927630
1864.231755	39.560633	62.932634
1863.112650	39.796706	62.937639
1862.425285	37.554578	62.942644
1861.870554	51.160708	62.947649
1861.433428	44.650917	62.952654
1861.232836	44.633914	62.957658
1860.518681	51.132603	62.962663
1860.285192	42.857359	62.967668
1859.576744	51.961918	62.972673
1858.513113	46.299100	62.977678
1858.099821	46.801585	62.982682
1856.920612	38.214446	62.987687
1856.572669	35.924735	62.992692
1855.199196	41.801112	62.997697
1854.678178	32.481825	63.002702
1853.894926	37.512259	63.007706
1853.318078	33.446926	63.012711
1853.546296	40.977150	63.017716
1852.517911	39.456242	63.022721
1852.008041	34.501887	63.027726
1851.799876	41.606224	63.032730
1850.771951	42.529587	63.037735
1850.358095	38.924088	63.042740
1849.383795	41.078456	63.047745
1848.490903	35.473694	63.052750
1847.395542	39.276322	63.057754
1846.641147	41.250690	63.062759
1846.335219	40.312102	63.067764
1845.562808	38.980793	63.072769
1845.538477	41.815399	63.077774
1845.250090	38.666231	63.082778
1843.823218	44.399702	63.087783
1843.447210	38.451086	63.092788
1842.253629	43.699648	63.097793
1841.861209	39.511989	63.102798
1841.262325	38.296634	63.107802
1840.719392	48.513504	63.112807
1839.799598	41.271361	63.117812
1838.540175	42.627314	63.122817
1838.442865	39.220719	63.127822
1837.846001	35.590664	63.132826
1837.217051	51.843742	63.137831
1837.284478	44.962094	63.142836
1836.320136	48.404870	63.147841
1835.613112	39.285436	63.152846
1834.644203	43.416506	63.157850
1834.036398	47.641630	63.162855
1833.283970	44.242863	63.167860
1832.343202	47.612508	63.172865
1831.553178	43.096891	63.177870
1830.630632	43.235532	63.182874
1830.053187	42.089317	63.187879
1830.381147	38.987365	63.192884
1829.467930	51.861924	63.197889
1829.161247	40.253500	63.202894
1828.864550	39.750276	63.207898
1827.210142	43.178047	63.212903
1827.009674	35.550446	63.217908
1826.210778	40.772612	63.222913
1825.563682	42.745717	63.227918
1824.532645	38.047595	63.232922
1823.591889	45.231993	63.237927
1823.136123	37.159217	63.242932
1822.635484	47.109167	63.247937
1822.109964	39.167319	63.252942
1821.576169	43.142565	63.257946
1821.005480	48.680167	63.262951
1820.301720	43.474323	63.267956
1818.839686	56.008671	63.272961
1818.700318	48.265704	63.277966
1818.104790	40.235622	63.282970
1817.633354	45.314327	63.287975
1817.647537	39.144478	63.292980
1815.813194	44.319755	63.297985
1815.220974	47.536284	63.302990
1814.609175	35.451178	63.307994
1814.027377	42.247408	63.312999
1813.873894	34.661236	63.318004
1813.165632	45.073097	63.323009
1812.550921	40.535956	63.328014
1811.499128	36.199114	63.333018
1811.060900	39.711319	63.338023
1810.695215	37.615248	63.343028
1809.153439	42.457056	63.348033
1808.459798	45.115665	63.353038
1808.030440	43.321449	63.358042
1807.083611	49.877597	63.363047
1806.827474	41.700580	63.368052
1806.511185	44.720324	63.373057
1806.167268	41.512169	63.378062
1805.308037	41.519335	63.383066
1804.203605	38.326292	63.388071
1803.692578	32.884842	63.393076
1802.946590	43.700098	63.398081
1802.295466	36.319112	63.403086
1801.258614	35.062928	63.408090
1800.661829	39.040295	63.413095
1800.344701	37.731320	63.418100
1799.442371	43.764724	63.423105
1799.004238	40.317636	63.428110
1798.777869	38.270408	63.433114
1797.359659	49.681288	63.438119
1796.796226	33.751679	63.443124
1796.158838	39.948018	63.448129
1795.910384	42.643168	63.453134
1795.342867	40.402527	63.458138
1794.244239	44.768682	63.463143
1793.970328	32.956366	63.468148
1792.917236	41.409168	63.473153
1792.593421	42.138734	63.478158
1792.252150	33.722924	63.483162
1790.845507	43.316845	63.488167
1790.322727	35.771975	63.493172
1789.734308	41.506365	63.498177
1789.075159	42.003748	63.503182
1788.884588	41.942581	63.508186
1787.741289	41.625848	63.513191
1786.946522	42.170001	63.518196
1786.122606	44.420362	63.523201
1786.135115	42.656906	63.528206
1785.400664	36.751033	63.533210
1784.093132	48.021335	63.538215
1783.649519	40.459162	63.543220
1782.678703	37.389993	63.548225
1782.298666	32.170603	63.553230
1782.236768	38.236126	63.558234
1781.077327	39.976785	63.563239
1781.232556	28.037976	63.568244
1779.798904	33.132291	63.573249
1779.141222	31.475270	63.578254
1778.875620	25.851346	63.583258
1777.953935	45.177160	63.588263
1777.567326	31.200185	63.593268
1776.462531	45.114451	63.598273
1775.899108	36.163052	63.603278
1775.843148	41.978468	63.608282
1774.307245	41.604240	63.613287
1773.268842	42.377905	63.618292
1772.445356	44.095177	63.623297
1772.625635	38.520290	63.628302
1772.170403	39.251805	63.633306
1771.211674	43.584711	63.638311
1771.109196	41.210296	63.643316
1770.145830	41.967315	63.648321
1769.350493	46.017224	63.653326
1768.830157	40.507871	63.658330
1767.809861	44.502041	63.663335
1767.474616	35.785649	63.668340
1766.176406	35.673306	63.673345
1765.617889	39.955270	63.678350
1765.289606	33.811430	63.683354
1764.399424	41.747923	63.688359
1764.476689	32.399880	63.693364
1763.812520	34.434059	63.698369
1762.903501	40.955825	63.703374
1761.949879	38.268720	63.708378
1761.249607	35.708542	63.713383
1761.138859	40.255293	63.718388
1759.926170	38.643841	63.723393
1759.062648	30.585381	63.728398
1758.155784	21.399951	63.733402
1757.740866	38.535259	63.738407
1757.379919	34.460894	63.743412
1756.668225	39.249746	63.748417
1756.334393	35.301965	63.753422
1756.116174	38.489068	63.758426
1755.215663	39.059487	63.763431
1754.517064	37.136150	63.768436
1753.367457	39.296315	63.773441
1752.085678	28.839445	63.778446
1751.703596	33.708415	63.783450
1750.994938	43.305042	63.788455
1750.632940	30.860161	63.793460
1750.465246	26.805570	63.798465
1750.014188	35.052376	63.803470
1749.344189	34.783496	63.808474
1748.157887	35.793555	63.813479
1747.751217	27.988980	63.818484
1746.997608	41.420109	63.823489
1746.122433	43.019438	63.828494
1745.236412	43.579673	63.833498
1744.460395	43.535796	63.838503
1744.161017	39.867980	63.843508
1743.467808	36.100284	63.848513
1743.265060	35.228902	63.853518
1742.802632	32.020658	63.858522
1741.409432	41.948364	63.863527
1741.033697	32.249636	63.868532
1740.421409	41.988658	63.873537
1739.403310	39.210875	63.878542
1738.708475	32.947058	63.883546
1737.725965	34.320579	63.888551
1737.599679	32.473511	63.893556
1737.297107	35.538390	63.898561
1736.731210	34.316246	63.903566
1736.231103	42.033092	63.908570
1735.144846	38.946006	63.913575
1734.913216	35.658527	63.918580
1733.406422	42.402982	63.923585
1732.376326	36.654474	63.928590
1731.861332	30.745306	63.933594
1731.585572	40.645349	63.938599
1731.260743	38.750965	63.943604
1730.836134	40.721871	63.948609
1729.444635	38.883361	63.953614
1729.011120	27.514319	63.958618
1728.264213	35.931122	63.963623
1727.864457	38.336485	63.968628
1727.264638	35.508042	63.973633
1726.162965	47.765985	63.978638
1725.531045	40.528633	63.983642
1724.874326	43.405330	63.988647
1724.699564	32.629138	63.993652
1724.225906	40.907925	63.998657
1723.125643	41.700897	64.003662
1722.690844	39.797172	64.008666
1721.520919	36.300748	64.013671
1721.199220	35.938706	64.018676
1720.121304	43.479241	64.023681
1719.251203	43.256344	64.028686
1718.767259	40.306994	64.033690
1717.916754	45.357607	64.038695
1717.895097	38.553199	64.043700
1717.786300	40.193240	64.048705
1717.095722	30.760576	64.053710
1716.186703	38.974468	64.058714
1715.220181	46.314381	64.063719
1714.696214	44.732333	64.068724
1713.626081	40.554570	64.073729
1712.605026	51.903982	64.078734
1712.235666	46.392739	64.083738
1711.815589	45.325638	64.088743
1711.665029	38.473893	64.093748
1711.090635	40.291970	64.098753
1709.739966	49.902272	64.103758
1709.063425	37.360697	64.108762
1708.375925	43.922990	64.113767
1708.203920	37.738567	64.118772
1707.550599	45.572797	64.123777
1706.375021	46.458166	64.128782
1705.939423	33.983983	64.133786
1705.062847	46.819627	64.138791
1704.836142	35.520240	64.143796
1704.047769	50.783063	64.148801
1703.009313	46.784780	64.153806
1702.296247	42.824702	64.158810
1701.568636	44.055244	64.163815
1701.522698	40.968514	64.168820
1700.937446	44.944068	64.173825
1700.038193	42.257813	64.178830
1699.332614	38.208236	64.183834
1698.454234	39.484806	64.188839
1697.820190	38.148912	64.193844
1697.661516	36.748548	64.198849
1696.616935	41.476747	64.203854
1695.885549	37.861790	64.208858
1695.053685	47.325031	64.213863
1694.730050	46.867104	64.218868
1694.528603	47.247652	64.223873
1693.530928	48.964230	64.228878
1692.991959	40.901549	64.233882
1691.750158	43.079539	64.238887
1691.701385	46.788525	64.243892
1690.694533	46.836525	64.248897
1689.479174	43.303176	64.253902
1689.093954	43.815421	64.258906
1688.501462	45.732575	64.263911
1688.527705	45.614897	64.268916
1687.955562	48.528633	64.273921
1686.765216	38.957734	64.278926
1686.227486	42.785390	64.283930
1685.470261	47.822773	64.288935
1685.015770	48.470605	64.293940
1684.193411	54.234292	64.298945
1683.159685	51.400664	64.303950
1683.184433	46.681555	64.308954
1682.478777	57.227076	64.313959
1681.345919	42.367268	64.318964
1680.476139	41.387377	64.323969
1679.651471	50.065714	64.328974
1679.247021	49.177490	64.333978
1679.017715	49.994562	64.338983
1678.882253	47.776783	64.343988
1677.777497	46.540897	64.348993
1676.853088	48.495008	64.353998
1676.308876	43.478338	64.359002
1675.573898	46.086773	64.364007
1674.514607	43.394410	64.369012
1673.902002	34.693714	64.374017
1673.037777	47.204119	64.379022
1673.042399	41.154072	64.384026
1672.603380	46.498888	64.389031
1672.043214	42.593381	64.394036
1671.094098	45.223217	64.399041
1670.438374	49.462292	64.404046
1670.064917	52.820723	64.409050
1668.445690	55.610628	64.414055
1667.878222	49.066392	64.419060
1667.517997	49.232461	64.424065
1666.598573	60.578364	64.429070
1666.486211	48.336693	64.434074
1665.747795	51.861911	64.439079
1665.236476	43.244473	64.444084
1664.480747	49.926429	64.449089
1663.472480	51.158986	64.454094
1663.564265	39.078864	64.459098
1662.176141	47.463502	64.464103
1661.355497	46.456888	64.469108
1660.888653	43.476447	64.474113
1660.077889	49.973175	64.479118
1660.044240	45.132454	64.484122
1659.375861	45.538293	64.489127
1658.377295	46.477568	64.494132
1657.586150	41.362932	64.499137
1657.147351	41.453174	64.504142
1656.902086	37.180673	64.509146
1655.388057	45.514349	64.514151
1654.658789	34.017259	64.519156
1654.403378	41.379844	64.524161
1653.762487	36.362771	64.529166
1653.603745	35.763534	64.534170
1652.387150	42.066104	64.539175
1651.877153	45.242793	64.544180
1651.271917	50.479974	64.549185
1650.465584	38.490486	64.554190
1649.658297	43.551599	64.559194
1648.898703	44.358295	64.564199
1648.450923	34.390329	64.569204
1648.142253	34.499325	64.574209
1647.263381	46.975791	64.579214
1646.470152	38.250178	64.584218
1645.773106	47.250454	64.589223
1645.129268	44.884775	64.594228
1644.875650	42.693655	64.599233
1643.737856	38.884650	64.604238
1643.360889	37.060065	64.609242
1642.255732	43.084732	64.614247
1641.695599	46.794526	64.619252
1641.372760	40.321829	64.624257
1640.349157	45.073525	64.629262
1639.558447	45.689619	64.634266
1639.044567	51.700785	64.639271
1638.544808	37.565199	64.644276
1638.114498	44.220692	64.649281
1637.555359	47.696935	64.654286
1636.990813	36.911715	64.659290
1635.879183	49.075069	64.664295
1635.617694	44.486594	64.669300
1634.497684	41.914283	64.674305
1633.403856	47.096619	64.679310
1633.069718	40.928500	64.684314
1632.512080	44.655246	64.689319
1632.164036	43.341744	64.694324
1631.941615	44.444737	64.699329
1630.551972	52.473233	64.704334
1630.327247	42.723727	64.709338
1629.159034	45.880407	64.714343
1628.708331	37.316433	64.719348
1627.738164	38.590260	64.724353
1626.913967	46.383840	64.729358
1626.582669	47.789567	64.734362
1626.003252	44.631471	64.739367
1625.633261	42.286948	64.744372
1625.035607	39.320990	64.749377
1623.892688	40.396753	64.754382
1623.601941	34.015160	64.759386
1622.865182	47.837883	64.764391
1621.817550	53.643683	64.769396
1621.236712	48.301676	64.774401
1620.235970	47.948177	64.779406
1620.063615	45.576987	64.784410
1619.689362	48.465605	64.789415
1619.113846	47.549374	64.794420
1618.265792	42.289249	64.799425
1617.234550	55.745592	64.804430
1617.185892	46.843346	64.809434
1616.314781	43.479275	64.814439
1615.319505	42.380569	64.819444
1614.718392	38.483160	64.824449
1613.986734	50.259717	64.829454
1613.735517	45.138166	64.834458
1613.218974	45.966183	64.839463
1611.905530	44.845485	64.844468
1611.263384	43.264889	64.849473
1610.977943	43.851181	64.854478
1610.429152	41.787387	64.859482
1609.183009	52.246894	64.864487
1608.566548	46.696080	64.869492
1608.050384	52.590917	64.874497
1607.327927	53.595156	64.879502
1607.135684	47.700971	64.884506
1606.467556	54.960395	64.889511
1605.569998	51.226781	64.894516
1604.891116	41.733944	64.899521
1604.016628	52.954441	64.904526
1603.881454	46.666404	64.909530
1602.893169	54.441907	64.914535
1602.401182	43.692475	64.919540
1601.697169	49.226062	64.924545
1601.248119	51.385379	64.929550
1600.186951	48.002623	64.934554
1599.179647	50.331061	64.939559
1598.414965	39.918280	64.944564
1598.243169	37.986986	64.949569
1597.734392	43.970534	64.954574
1597.316954	49.392358	64.959578
1596.286655	54.785395	64.964583
1595.503078	51.197682	64.969588
1595.133711	47.405386	64.974593
1594.166296	48.593631	64.979598
1594.174621	41.298755	64.984602
1592.703159	45.378860	64.989607
1592.393813	44.822479	64.994612
1591.641979	44.932504	64.999617
1591.047273	47.693721	65.004622
1590.463724	44.777570	65.009626
1589.618910	42.975284	65.014631
1589.367393	47.104421	65.019636
1588.719306	39.711983	65.024641
1587.436628	45.944653	65.029646
1587.126676	35.100076	65.034650
1586.283557	53.831535	65.039655
1585.853739	49.373892	65.044660
1585.314669	43.329808	65.049665
1584.385433	45.388797	65.054670
1583.959951	52.455127	65.059674
1583.207773	44.423198	65.064679
1582.396445	49.317811	65.069684
1581.453602	51.445198	65.074689
1580.611051	63.130578	65.079694
1580.377245	44.813141	65.084698
1580.057977	49.978088	65.089703
1579.537481	38.271232	65.094708
1578.504008	41.808656	65.099713
1577.473293	53.648508	65.104718
1577.310470	41.277678	65.109722
1576.958233	45.897492	65.114727
1575.870477	48.776476	65.119732
1575.253567	34.769919	65.124737
1574.275713	50.108597	65.129742
1574.383108	43.605400	65.134746
1573.013009	53.414394	65.139751
1572.180999	48.579100	65.144756
1571.832977	46.830352	65.149761
1571.187718	42.134126	65.154766
1570.924101	47.810638	65.159770
1569.688092	42.807721	65.164775
1568.754083	48.511902	65.169780
1568.643617	38.509285	65.174785
1567.936432	47.851816	65.179790
1567.909009	42.965956	65.184794
1566.496849	48.635723	65.189799
1565.626866	37.794976	65.194804
1565.329220	38.928851	65.199809
1564.411711	41.498506	65.204814
1564.087199	37.826827	65.209818
1563.108804	44.123125	65.214823
1562.327847	42.454209	65.219828
1561.866039	38.566220	65.224833
1561.291318	40.537347	65.229838
1561.314268	41.009986	65.234842
1559.959455	45.304969	65.239847
1559.093587	50.734970	65.244852
1558.830267	42.901348	65.249857
1558.293992	49.609958	65.254862
1557.197210	37.699781	65.259866
1556.508840	46.050550	65.264871
1555.867685	45.840217	65.269876
1555.613328	38.774746	65.274881
1554.641274	41.785166	65.279886
1553.682724	41.801889	65.284890
1553.115597	40.420706	65.289895
1552.632120	35.744513	65.294900
1552.487113	36.325844	65.299905
1551.789437	44.473083	65.304910
1550.898582	39.831658	65.309914
1549.523740	50.308481	65.314919
1549.549178	41.396048	65.319924
1549.214402	38.989173	65.324929
1548.256061	54.329491	65.329934
1547.544693	42.730244	65.334938
1546.533218	41.962153	65.339943
1546.139958	40.898705	65.344948
1545.074682	44.982103	65.349953
1544.082833	45.053008	65.354958
1543.816569	38.604457	65.359962
1543.086046	41.723163	65.364967
1542.828431	37.758576	65.369972
1542.547509	35.444072	65.374977
1542.038887	40.244859	65.379982
1541.348927	38.646648	65.384986
1540.766107	42.415259	65.389991
1539.685008	44.351735	65.394996
1539.030327	36.695428	65.400001
1538.077628	46.084861	65.405006
1537.743055	49.020800	65.410010
1537.031736	47.400752	65.415015
1535.890746	46.615397	65.420020
1535.510898	45.846294	65.425025
1534.905029	53.404927	65.430030
1534.500604	47.487697	65.435034
1533.414958	42.670645	65.440039
1532.654001	45.228050	65.445044
1532.288488	36.466058	65.450049
1531.751334	47.773315	65.455054
1531.115532	45.229767	65.460058
1530.277609	41.620753	65.465063
1529.152109	41.134146	65.470068
1529.001319	43.034761	65.475073
1528.811200	44.681422	65.480078
1527.730893	39.943952	65.485082
1526.877950	40.421732	65.490087
1526.091035	45.585298	65.495092
1525.763171	30.294895	65.500097
1524.940576	49.012054	65.505102
1524.092034	37.237495	65.510106
1523.605908	44.204650	65.515111
1522.872307	44.661890	65.520116
1522.467274	45.328698	65.525121
1521.718344	40.347756	65.530126
1520.885042	36.053599	65.535130
1520.625358	44.011391	65.540135
1519.971301	46.763129	65.545140
1519.286362	40.835286	65.550145
1517.927818	47.021694	65.555150
1517.589029	37.094793	65.560154
1516.927106	43.683021	65.565159
1516.678171	40.352585	65.570164
1515.973311	38.453967	65.575169
1514.914728	40.839471	65.580174
1514.388354	42.766654	65.585178
1513.864272	41.847005	65.590183
1513.212343	53.263972	65.595188
1512.240055	38.989049	65.600193
1511.552224	43.110252	65.605198
1511.064465	38.903115	65.610202
1510.692285	44.067011	65.615207
1509.891317	42.611032	65.620212
1509.173716	37.006937	65.625217
1508.430333	48.034725	65.630222
1508.084877	42.634846	65.635226
1507.269492	43.100356	65.640231
1506.085410	45.641428	65.645236
1505.862574	42.060836	65.650241
1505.181629	47.634932	65.655246
1505.019001	46.941703	65.660250
1503.905074	41.687602	65.665255
1502.702083	43.006359	65.670260
1502.438865	42.034219	65.675265
1501.634043	42.124305	65.680270
1501.451839	36.197004	65.685274
1500.917501	44.655770	65.690279
1499.637525	45.491588	65.695284
1499.347981	39.543496	65.700289
1498.616049	48.254445	65.705294
1497.910476	38.223406	65.710298
1497.079592	31.099756	65.715303
1496.298356	44.734013	65.720308
1496.030045	35.915581	65.725313
1495.583578	41.517071	65.730318
1494.635562	38.636789	65.735322
1493.521950	47.362661	65.740327
1492.842128	43.223898	65.745332
1492.864109	41.406901	65.750337
1492.073377	44.535188	65.755342
1491.786309	41.090964	65.760346
1491.132397	41.953451	65.765351
1490.312812	46.436227	65.770356
1489.342618	34.837141	65.775361
1488.496022	44.739592	65.780366
1488.121553	45.358969	65.785370
1487.872254	34.555242	65.790375
1486.565196	36.093975	65.795380
1485.760099	34.867324	65.800385
1485.072424	45.175038	65.805390
1484.671123	38.479870	65.810394
1484.272031	32.801512	65.815399
1483.251062	38.372875	65.820404
1482.532608	33.642578	65.825409
1481.790189	39.056131	65.830414
1481.338115	42.627351	65.835418
1481.345736	38.887132	65.840423
1480.139056	37.358442	65.845428
1479.220476	33.030544	65.850433
1478.833357	34.782634	65.855438
1478.050835	38.674458	65.860442
1477.178031	41.653362	65.865447
1476.206953	42.121547	65.870452
1475.825768	39.256846	65.875457
1475.358243	41.341845	65.880462
1475.143185	34.773204	65.885466
1474.963515	40.013742	65.890471
1473.589489	35.400251	65.895476
1473.003571	28.702891	65.900481
1472.291190	40.395972	65.905486
1471.240678	42.258227	65.910490
1470.375876	40.030218	65.915495
1469.792204	42.411227	65.920500
1469.406056	38.367728	65.925505
1469.082741	38.819702	65.930510
1468.422217	34.280480	65.935514
1467.618320	38.868003	65.940519
1467.059269	39.477294	65.945524
1466.639547	29.615313	65.950529
1465.341480	42.126894	65.955534
1464.420730	35.623101	65.960538
1463.724173	41.474080	65.965543
1463.501216	41.916413	65.970548
1463.664675	35.705517	65.975553
1462.528215	36.422347	65.980558
1461.667758	38.282785	65.985562
1460.916729	43.820717	65.990567
1460.383738	38.630432	65.995572
1459.629707	40.004013	66.000577
1458.664970	42.261080	66.005582
1458.355585	49.681137	66.010586
1457.981161	32.283408	66.015591
1456.976255	36.231082	66.020596
1456.014989	32.633816	66.025601
1455.235460	39.655493	66.030606
1454.356580	34.606919	66.035610
1454.650773	37.766214	66.040615
1454.115589	46.524749	66.045620
1453.340493	46.846674	66.050625
1452.132644	43.709654	66.055630
1451.504857	45.135714	66.060634
1451.364701	45.375649	66.065639
1450.487349	44.901678	66.070644
1449.674638	43.059645	66.075649
1448.702935	41.643437	66.080654
1448.257070	29.112621	66.085658
1447.947546	40.514590	66.090663
1446.725927	44.605526	66.095668
1446.756187	33.973423	66.100673
1445.689863	34.535607	66.105678
1445.212662	32.118269	66.110682
1444.451251	38.566198	66.115687
1443.429916	30.171824	66.120692
1443.074090	30.756704	66.125697
1442.728123	34.471916	66.130702
1442.169873	31.523399	66.135706
1441.423242	35.537264	66.140711
1440.454158	35.221382	66.145716
1439.881485	28.599199	66.150721
1438.639957	36.795047	66.155726
1437.889376	41.214827	66.160730
1437.559996	35.391354	66.165735
1436.885680	45.741109	66.170740
1437.037331	37.442578	66.175745
1436.217791	43.571737	66.180750
1435.168747	39.874886	66.185754
1434.854373	37.486863	66.190759
1434.060173	38.258118	66.195764
1433.459937	27.961205	66.200769
1432.523206	37.887452	66.205774
1432.178770	35.583058	66.210778
1431.033319	42.203999	66.215783
1429.752815	45.411726	66.220788
1429.376106	34.708688	66.225793
1429.048602	39.152690	66.230798
1428.783438	40.090601	66.235802
1428.159995	40.695942	66.240807
1427.829171	40.209229	66.245812
1427.273474	34.103179	66.250817
1426.146504	42.060047	66.255822
1424.896341	33.621624	66.260826
1424.396767	34.063772	66.265831
1423.589136	47.798435	66.270836
1423.112120	33.378610	66.275841
1422.473939	31.436305	66.280846
1422.266841	30.371674	66.285850
1421.461133	27.506652	66.290855
1420.564099	46.543164	66.295860
1420.404114	30.156909	66.300865
1419.427431	32.852713	66.305870
1418.386254	31.125856	66.310874
1417.729818	38.813965	66.315879
1416.893453	41.951102	66.320884
1416.730551	33.106471	66.325889
1416.420264	43.896693	66.330894
1415.330441	39.922475	66.335898
1414.523921	33.987186	66.340903
1413.874163	37.810615	66.345908
1413.829641	33.346965	66.350913
1412.577868	41.837774	66.355918
1411.948305	37.500233	66.360922
1411.448443	37.201244	66.365927
1411.115447	43.178954	66.370932
1410.343081	30.375186	66.375937
1409.121100	36.125185	66.380942
1408.606238	32.411248	66.385946
1408.284919	29.425080	66.390951
1407.665975	43.904050	66.395956
1406.670641	34.507325	66.400961
1405.822461	43.189456	66.405966
1405.273202	42.407877	66.410970
1405.527330	28.889002	66.415975
1403.981019	45.305263	66.420980
1403.313589	37.986927	66.425985
1402.587978	41.600061	66.430990
1402.102558	36.908443	66.435994
1402.026852	37.972362	66.440999
1400.865666	40.151863	66.446004
1400.468099	31.898060	66.451009
1399.675625	45.914174	66.456014
1398.374362	28.687451	66.461018
1397.721828	26.241222	66.466023
1397.146691	38.560639	66.471028
1396.766819	33.405958	66.476033
1396.524130	35.254951	66.481038
1395.907996	40.571178	66.486042
1395.089271	38.972976	66.491047
1394.242297	41.570899	66.496052
1393.913680	34.745926	66.501057
1392.702464	35.608713	66.506062
1391.822364	39.222752	66.511066
1391.596144	36.059037	66.516071
1391.106747	36.827587	66.521076
1390.683282	27.377817	66.526081
1389.498461	44.958787	66.531086
1388.634749	30.622524	66.536090
1388.022289	32.913504	66.541095
1387.795643	32.274616	66.546100
1387.419163	31.358341	66.551105
1386.418073	37.749763	66.556110
1385.361904	31.704358	66.561114
1385.239172	30.552201	66.566119
1384.396820	38.068014	66.571124
1383.195173	27.668020	66.576129
1382.715770	33.888202	66.581134
1382.076862	30.209761	66.586138
1382.113811	35.581448	66.591143
1381.050693	38.868184	66.596148
1380.246301	28.136954	66.601153
1379.665379	41.231594	66.606158
1379.447242	37.683388	66.611162
1378.863820	29.662567	66.616167
1377.535818	38.917727	66.621172
1376.905052	37.884177	66.626177
1376.165820	33.072062	66.631182
1375.696377	44.161980	66.636186
1374.944132	30.432491	66.641191
1373.904417	31.343720	66.646196
1373.783086	33.064610	66.651201
1373.582378	36.747276	66.656206
1372.621815	45.392087	66.661210
1371.889488	42.605302	66.666215
1371.010085	44.112381	66.671220
1370.597097	38.182360	66.676225
1369.965752	38.071441	66.681230
1368.799817	44.730356	66.686234
1368.106757	42.874061	66.691239
1367.214335	51.690976	66.696244
1367.052106	35.065384	66.701249
1366.449274	40.966140	66.706254
1366.092432	38.400371	66.711258
1365.430680	33.336240	66.716263
1364.530136	47.634474	66.721268
1364.347538	32.612767	66.726273
1363.155711	38.723853	66.731278
1362.341817	42.545000	66.736282
1361.768525	40.452043	66.741287
1361.321741	36.582212	66.746292
1360.779243	38.892040	66.751297
1359.667832	39.011985	66.756302
1359.075732	47.998781	66.761306
1358.618262	40.410534	66.766311
1358.053892	39.763834	66.771316
1357.151860	34.595974	66.776321
1356.454497	34.366241	66.781326
1355.823665	44.157148	66.786330
1355.491326	34.391692	66.791335
1354.469493	42.043283	66.796340
1353.837961	42.947978	66.801345
1353.181149	43.558641	66.806350
1352.682229	36.544702	66.811354
1352.285728	33.108436	66.816359
1351.251688	38.123669	66.821364
1350.787930	33.874908	66.826369
1350.130688	30.800223	66.831374
1349.381733	37.820216	66.836378
1348.564103	28.120877	66.841383
1347.631200	35.578553	66.846388
1347.422481	31.532104	66.851393
1346.929092	41.069343	66.856398
1345.708943	49.846898	66.861402
1345.039531	35.366219	66.866407
1344.408502	46.155393	66.871412
1344.116015	35.812734	66.876417
1343.772435	38.141405	66.881422
1342.849253	35.274583	66.886426
1342.113557	35.957715	66.891431
1341.256345	37.738825	66.896436
1340.647346	33.849055	66.901441
1340.631436	42.720594	66.906446
1339.368577	37.854537	66.911450
1338.914081	37.062638	66.916455
1338.212723	36.795697	66.921460
1337.577267	29.436034	66.926465
1336.465418	37.964551	66.931470
1335.911098	44.635056	66.936474
1335.418690	37.184837	66.941479
1335.007345	47.598458	66.946484
1334.021095	30.193962	66.951489
1333.125028	31.782551	66.956494
1332.744081	39.100441	66.961498
1332.473560	33.486832	66.966503
1331.454842	41.025969	66.971508
1330.881401	36.859306	66.976513
1330.220034	40.798141	66.981518
1329.557765	33.035879	66.986522
1329.119786	29.674023	66.991527
1328.011562	47.749047	66.996532
1327.469919	36.507696	67.001537
1327.120877	40.947246	67.006542
1326.028423	37.640553	67.011546
1325.307954	36.548737	67.016551
1324.706796	42.047103	67.021556
1324.468095	34.927145	67.026561
1324.106985	37.745894	67.031566
1322.813408	39.186369	67.036570
1322.499743	32.368496	67.041575
1321.758824	40.502148	67.046580
1320.626519	37.263297	67.051585
1319.742443	35.749629	67.056590
1319.089600	41.790812	67.061594
1318.920072	35.069874	67.066599
1318.357592	39.891872	67.071604
1318.191100	37.284809	67.076609
1316.878263	40.603386	67.081614
1316.009796	47.218183	67.086618
1315.850923	35.562735	67.091623
1315.164852	45.917530	67.096628
1314.631306	35.553278	67.101633
1313.468355	37.132265	67.106638
1312.722490	36.648475	67.111642
1312.415267	45.000190	67.116647
1311.900245	42.685088	67.121652
1310.735740	44.784729	67.126657
1310.277772	44.412866	67.131662
1309.609470	34.109467	67.136666
1309.382552	36.561522	67.141671
1308.000575	42.688670	67.146676
1307.711942	41.561317	67.151681
1306.579272	36.554728	67.156686
1306.410724	37.086196	67.161690
1306.095226	27.499433	67.166695
1305.051804	35.413094	67.171700
1304.562871	34.063693	67.176705
1303.966038	30.030071	67.181710
1303.470247	39.698584	67.186714
1302.651266	39.297387	67.191719
1301.947100	39.199640	67.196724
1301.157885	40.388044	67.201729
1300.132087	44.681303	67.206734
1299.321761	43.018718	67.211738
1299.231483	39.483310	67.216743
1298.538189	45.343268	67.221748
1298.228858	38.887415	67.226753
1296.881319	39.675725	67.231758
1296.303100	37.359636	67.236762
1296.144007	29.184641	67.241767
1295.345392	39.062155	67.246772
1294.378200	38.012729	67.251777
1293.751976	44.347736	67.256782
1293.058543	42.991427	67.261786
1292.661494	35.661679	67.266791
1292.128822	45.263520	67.271796
1291.046382	50.218662	67.276801
1290.453914	50.237203	67.281806
1289.986492	43.752868	67.286810
1289.469914	44.541528	67.291815
1288.269719	43.122288	67.296820
1287.739025	34.815560	67.301825
1287.097625	50.498203	67.306830
1286.669317	53.220409	67.311834
1285.865091	32.475322	67.316839
1284.878301	56.862656	67.321844
1284.205889	46.745995	67.326849
1284.260061	43.403667	67.331854
1283.553028	47.789754	67.336858
1282.874664	33.010900	67.341863
1281.866939	43.099867	67.346868
1281.519529	40.881127	67.351873
1281.104832	39.182451	67.356878
1280.016358	49.675356	67.361882
1279.363842	43.673049	67.366887
1278.756423	39.661616	67.371892
1277.976133	40.589982	67.376897
1277.072093	41.728840	67.381902
1276.143504	45.847375	67.386906
1276.049731	38.918850	67.391911
1275.651410	42.923107	67.396916
1274.585137	48.463900	67.401921
1273.863636	44.353909	67.406926
1272.961974	44.416886	67.411930
1272.775043	37.394362	67.416935
1272.263857	46.286300	67.421940
1271.223096	44.321312	67.426945
1270.341368	40.963791	67.431950
1269.751144	40.824281	67.436954
1269.637668	40.110638	67.441959
1269.124645	41.225172	67.446964
1267.972568	38.093571	67.451969
1267.386634	41.424325	67.456974
1266.620188	48.226344	67.461978
1266.504368	46.090631	67.466983
1265.466371	43.114359	67.471988
1264.769314	39.992410	67.476993
1264.020740	35.913538	67.481998
1263.530968	41.649675	67.487002
1263.133343	40.919712	67.492007
1261.981301	41.542911	67.497012
1261.393883	39.693504	67.502017
1261.055231	42.945515	67.507022
1260.081112	42.170022	67.512026
1259.456874	41.991767	67.517031
1258.678411	43.424484	67.522036
1258.137711	44.226448	67.527041
1257.855523	39.087801	67.532046
1256.665796	49.588927	67.537050
1256.059823	42.290830	67.542055
1255.452681	45.478300	67.547060
1255.162918	37.514899	67.552065
1254.134533	40.009244	67.557070
1253.156272	40.604814	67.562074
1252.754835	34.496362	67.567079
1252.297811	41.687581	67.572084
1251.753394	43.182433	67.577089
1251.175342	40.893137	67.582094
1250.131500	44.454408	67.587098
1249.876878	34.279219	67.592103
1249.098866	36.973454	67.597108
1248.070498	37.643226	67.602113
1247.425438	39.854265	67.607118
1246.646923	48.307735	67.612122
1246.556109	40.038303	67.617127
1245.421438	43.784332	67.622132
1244.702256	42.608754	67.627137
1244.339615	41.209320	67.632142
1243.566038	45.940318	67.637146
1243.603040	35.619407	67.642151
1242.243777	40.028790	67.647156
1241.471937	40.900629	67.652161
1241.151181	39.505574	67.657166
1240.536946	47.937652	67.662170
1240.072580	32.719502	67.667175
1238.967568	41.374702	67.672180
1238.781092	39.951986	67.677185
1237.668012	34.718385	67.682190
1236.721008	40.380574	67.687194
1235.996205	40.323975	67.692199
1235.447994	42.685199	67.697204
1235.165841	33.829598	67.702209
1234.843190	35.949944	67.707214
1233.241052	48.309692	67.712218
1232.948654	37.566488	67.717223
1232.737261	39.074620	67.722228
1232.128871	44.304489	67.727233
1230.921426	35.947696	67.732238
1230.014282	37.889749	67.737242
1229.959800	33.681590	67.742247
1229.373741	36.195492	67.747252
1228.435953	33.577048	67.752257
1227.721862	40.369170	67.757262
1227.019035	39.430698	67.762266
1226.819363	26.925459	67.767271
1225.586589	44.574023	67.772276
1224.707480	43.900132	67.777281
1224.293594	36.874282	67.782286
1223.823332	39.380810	67.787290
1223.629173	41.543805	67.792295
1222.313807	42.557277	67.797300
1221.412599	45.540777	67.802305
1221.309777	39.939941	67.807310
1220.784833	51.295749	67.812314
1220.469963	39.188874	67.817319
1219.122348	44.323408	67.822324
1218.525413	38.504676	67.827329
1218.070412	33.469215	67.832334
1217.050847	42.911943	67.837338
1216.235945	41.440929	67.842343
1215.765595	45.988093	67.847348
1215.118408	34.851876	67.852353
1214.872712	39.238729	67.857358
1214.129799	46.888590	67.862362
1213.342108	34.069997	67.867367
1212.786466	39.737766	67.872372
1211.898023	39.644117	67.877377
1211.342016	39.653724	67.882382
1210.489244	40.880648	67.887386
1210.534817	35.598421	67.892391
1209.263725	36.883985	67.897396
1208.215334	41.587731	67.902401
1207.637411	32.533163	67.907406
1207.431161	49.318308	67.912410
1207.473225	46.241262	67.917415
1205.834868	38.071284	67.922420
1205.455397	31.227630	67.927425
1205.117637	39.549507	67.932430
1203.809197	44.633663	67.937434
1203.180667	32.056275	67.942439
1202.194286	44.866900	67.947444
1202.057900	34.169860	67.952449
1201.474293	33.765957	67.957454
1200.909227	43.210528	67.962458
1200.277708	35.802972	67.967463
1199.282008	47.837629	67.972468
1198.707839	41.857583	67.977473
1198.212589	43.175890	67.982478
1196.896306	41.582765	67.987482
1196.437480	39.337601	67.992487
1195.679954	49.995523	67.997492
1195.730553	45.799038	68.002497
1195.493205	41.320334	68.007502
1194.163531	48.238752	68.012506
1193.388313	40.945513	68.017511
1192.835330	42.703519	68.022516
1192.177776	40.595619	68.027521
1191.166470	42.158428	68.032526
1190.712835	48.246805	68.037530
1190.308150	42.977836	68.042535
1190.075406	43.973692	68.047540
1188.527652	41.237800	68.052545
1188.117409	39.426467	68.057550
1187.631513	45.903182	68.062554
1186.640560	34.712836	68.067559
1185.890167	43.347928	68.072564
1185.471287	38.466003	68.077569
1185.018561	35.740469	68.082574
1184.267129	47.829324	68.087578
1183.726295	36.829171	68.092583
1182.421440	44.243549	68.097588
1181.766991	48.075660	68.102593
1181.744455	37.157083	68.107598
1181.394680	53.197065	68.112602
1180.281893	40.745582	68.117607
1179.436551	37.216726	68.122612
1178.603114	46.749717	68.127617
1178.347894	42.034156	68.132622
1177.628826	43.690844	68.137626
1177.089257	35.787691	68.142631
1176.301761	36.669923	68.147636
1175.562619	40.777283	68.152641
1175.316974	40.215554	68.157646
1173.748651	43.398211	68.162650
1173.275101	33.109622	68.167655
1172.809182	42.973675	68.172660
1172.558529	41.302547	68.177665
1172.287924	35.042414	68.182670
1171.126598	43.392775	68.187674
1170.658962	42.188250	68.192679
1170.127472	45.090887	68.197684
1168.740190	40.173748	68.202689
1168.431699	35.368890	68.207694
1167.871160	35.664661	68.212698
1166.855732	36.277213	68.217703
1166.105530	38.563340	68.222708
1165.350757	35.969430	68.227713
1165.263017	33.695216	68.232718
1165.036242	43.740436	68.237722
1163.728462	41.548299	68.242727
1162.828280	37.947746	68.247732
1162.012677	40.502902	68.252737
1161.904775	45.154855	68.257742
1160.731492	48.124877	68.262746
1160.125899	40.257459	68.267751
1159.924632	41.510091	68.272756
1159.308002	37.936981	68.277761
1158.903318	35.292123	68.282766
1157.769138	42.469626	68.287770
1156.936027	34.293040	68.292775
1156.558160	40.140704	68.297780
1155.950766	46.843332	68.302785
1154.932006	38.335142	68.307790
1153.828097	46.323134	68.312794
1153.707834	42.357258	68.317799
1153.358714	41.964957	68.322804
1152.887658	45.411506	68.327809
1152.271796	43.208675	68.332814
1151.301491	46.496507	68.337818
1150.710957	38.254529	68.342823
1149.358107	41.762481	68.347828
1148.699468	41.605495	68.352833
1148.076621	43.175922	68.357838
1147.619911	48.536227	68.362842
1147.378181	36.521821	68.367847
1146.967773	37.006610	68.372852
1146.017833	39.332397	68.377857
1145.533650	43.433906	68.382862
1144.909199	46.832313	68.387866
1144.049991	47.230789	68.392871
1143.113499	43.509859	68.397876
1142.521234	41.673868	68.402881
1142.148258	35.817962	68.407886
1141.017762	40.104274	68.412890
1140.342541	36.535758	68.417895
1139.490786	39.360027	68.422900
1138.773865	44.902072	68.427905
1138.766708	39.290759	68.432910
1138.373439	49.900216	68.437914
1137.518006	36.556255	68.442919
1136.789453	36.738405	68.447924
1136.098449	42.817232	68.452929
1135.747754	42.390491	68.457934
1134.263580	51.145466	68.462938
1133.718149	41.190021	68.467943
1133.204950	46.426845	68.472948
1132.789391	40.481516	68.477953
1132.514586	30.134520	68.482958
1130.997142	47.082481	68.487962
1130.570858	43.100626	68.492967
1130.359042	40.508674	68.497972
1129.348583	47.677550	68.502977
1128.686185	45.277118	68.507982
1127.534204	42.498813	68.512986
1127.097300	40.325872	68.517991
1126.727612	42.605103	68.522996
1126.372996	46.913092	68.528001
1125.924103	35.562437	68.533006
1124.949764	40.885226	68.538010
1124.484214	37.374830	68.543015
1123.316422	39.336300	68.548020
1122.307261	42.127264	68.553025
1122.216405	35.292913	68.558030
1121.469606	42.728938	68.563034
1121.086687	36.485103	68.568039
1120.330305	40.423327	68.573044
1119.495667	39.871712	68.578049
1119.129721	35.889726	68.583054
1117.676585	47.606074	68.588058
1117.411337	42.713918	68.593063
1116.877986	41.903064	68.598068
1116.291572	43.179115	68.603073
1115.819868	31.013641	68.608078
1114.444045	45.595684	68.613082
1114.245584	35.857876	68.618087
1113.757457	41.126984	68.623092
1112.690452	42.788571	68.628097
1112.102772	34.822126	68.633102
1111.067780	42.690357	68.638106
1111.032523	36.151520	68.643111
1110.582120	35.243893	68.648116
1109.505412	43.563470	68.653121
1108.946366	40.709780	68.658126
1108.420664	45.760936	68.663130
1107.609894	37.118758	68.668135
1106.771845	38.742350	68.673140
1105.628224	44.699213	68.678145
1105.598411	42.344823	68.683150
1104.997713	46.690382	68.688154
1104.744660	41.381542	68.693159
1103.798029	40.991253	68.698164
1102.661571	40.481347	68.703169
1102.334514	37.305323	68.708174
1101.907912	46.366753	68.713178
1100.989813	40.062970	68.718183
1100.245279	33.050324	68.723188
1099.664532	41.382474	68.728193
1099.319955	31.202705	68.733198
1098.232966	40.315563	68.738202
1097.325276	33.813006	68.743207
1096.800127	42.440670	68.748212
1096.310135	47.519264	68.753217
1096.322376	39.244497	68.758222
1095.073788	42.795816	68.763226
1094.320097	41.625772	68.768231
1093.977750	33.681810	68.773236
1093.023092	39.969745	68.778241
1092.198776	36.453348	68.783246
1091.515655	40.239574	68.788250
1090.687826	35.843779	68.793255
1090.617204	35.670541	68.798260
1089.661965	42.251890	68.803265
1088.743118	37.824842	68.808270
1088.166754	39.586588	68.813274
1087.923552	35.556696	68.818279
1087.772535	34.776493	68.823284
1086.469710	39.214821	68.828289
1086.247576	34.959224	68.833294
1085.143230	41.315130	68.838298
1084.430325	37.462461	68.843303
1083.290870	41.732875	68.848308
1082.655021	41.692132	68.853313
1082.638668	43.185016	68.858318
1081.822745	43.199728	68.863322
1081.511356	41.213413	68.868327
1080.527238	38.206575	68.873332
1079.727897	39.213725	68.878337
1079.190007	36.176903	68.883342
1078.908483	44.251717	68.888346
1077.815799	39.860212	68.893351
1077.183425	35.835460	68.898356
1076.518466	29.611273	68.903361
1076.210324	34.530047	68.908366
1075.059389	42.624895	68.913370
1074.236302	46.725135	68.918375
1074.183374	44.609393	68.923380
1073.614849	44.526402	68.928385
1072.744604	39.317330	68.933390
1071.991508	44.884068	68.938394
1071.231012	43.650457	68.943399
1070.662084	37.360528	68.948404
1069.336820	44.972170	68.953409
1069.072252	36.705173	68.958414
1068.228914	36.749482	68.963418
1068.125966	45.805157	68.968423
1067.668238	30.109766	68.973428
1066.458489	42.922840	68.978433
1065.775155	31.068599	68.983438
1065.046018	37.669178	68.988442
1064.994093	40.872439	68.993447
1064.381627	36.593783	68.998452
1063.048917	44.392696	69.003457
1062.733461	42.419647	69.008462
1062.094767	44.345859	69.013466
1061.431003	42.011898	69.018471
1060.850519	29.683972	69.023476
1059.928224	43.815408	69.028481
1059.854868	36.002127	69.033486
1058.753205	44.199532	69.038490
1057.888416	42.045789	69.043495
1057.399714	44.753978	69.048500
1056.707143	46.961581	69.053505
1056.319671	43.538126	69.058510
1055.188680	45.268264	69.063514
1054.725091	42.867766	69.068519
1054.118005	39.203279	69.073524
1053.079470	49.978474	69.078529
1052.179390	41.088747	69.083534
1051.767821	50.587769	69.088538
1051.149343	48.051060	69.093543
1051.032604	49.443219	69.098548
1050.298503	53.119294	69.103553
1049.998122	39.530948	69.108558
1048.820654	40.937316	69.113562
1048.321244	49.977218	69.118567
1047.937268	41.292395	69.123572
1046.634347	48.920995	69.128577
1046.136746	44.671378	69.133582
1045.315577	47.364652	69.138586
1045.036883	46.283059	69.143591
1043.760917	41.688913	69.148596
1043.062038	45.479235	69.153601
1042.784447	34.658028	69.158606
1042.373958	43.803631	69.163610
1041.893442	40.401290	69.168615
1041.117847	43.035274	69.173620
1040.088728	42.173999	69.178625
1039.781445	39.698173	69.183630
1038.654639	38.396693	69.188634
1038.016757	40.500980	69.193639
1037.287550	41.834459	69.198644
1036.610155	43.560249	69.203649
1036.531572	38.717258	69.208654
1035.949509	38.879285	69.213658
1035.071093	41.436587	69.218663
1034.391223	39.475788	69.223668
1033.934121	40.395386	69.228673
1032.764822	32.734395	69.233678
1031.791593	36.730796	69.238682
1031.813407	43.142521	69.243687
1031.423823	47.372503	69.248692
1030.370629	50.794993	69.253697
1029.711729	39.457275	69.258702
1029.161990	50.317139	69.263706
1028.680505	36.029049	69.268711
1027.522498	38.036314	69.273716
1026.341957	35.688388	69.278721
1026.459417	30.724323	69.283726
1025.676157	38.268671	69.288730
1025.159307	32.861466	69.293735
1024.169303	35.646263	69.298740
1023.233417	45.887882	69.303745
1023.088475	32.282704	69.308750
1022.810093	41.353670	69.313754
1021.945367	38.200125	69.318759
1021.116212	45.135180	69.323764
1020.470141	42.375785	69.328769
1019.840916	39.563247	69.333774
1018.596879	51.534961	69.338778
1018.128288	45.095037	69.343783
1017.863353	36.291934	69.348788
1017.320213	47.160209	69.353793
1016.557763	40.021129	69.358798
1015.286928	41.089123	69.363802
1014.751140	43.315946	69.368807
1014.336968	44.501535	69.373812
1013.819491	38.865768	69.378817
1013.699973	35.820745	69.383822
1012.562615	40.267475	69.388826
1011.685961	43.482105	69.393831
1011.733800	37.783203	69.398836
1010.419631	39.982482	69.403841
1009.632830	39.984698	69.408846
1009.090337	43.710721	69.413850
1008.439162	40.695094	69.418855
1008.402684	34.188001	69.423860
1006.856606	39.401520	69.428865
1006.529858	28.646495	69.433870
1005.951734	37.312558	69.438874
1005.348748	37.074213	69.443879
1004.326627	29.733604	69.448884
1003.437878	38.931648	69.453889
1003.490930	27.193661	69.458894
1002.982596	37.575412	69.463898
1002.066428	39.269815	69.468903
1001.251498	39.110926	69.473908
1000.643366	38.627393	69.478913
1000.236682	34.740222	69.483918
999.032104	35.627368	69.488922
998.239598	40.023964	69.493927
997.743182	36.723515	69.498932
997.294296	43.385177	69.503937
996.838601	38.630579	69.508942
995.989102	43.078824	69.513946
995.254775	38.217170	69.518951
995.009727	35.988497	69.523956
993.893071	39.727030	69.528961
993.047453	40.806227	69.533966
992.505219	45.476824	69.538970
992.013180	42.407494	69.543975
991.728577	32.432678	69.548980
990.271540	36.524998	69.553985
989.677043	36.567586	69.558990
989.264641	38.287493	69.563994
988.827566	39.513000	69.568999
988.538945	36.256761	69.574004
987.214868	38.274699	69.579009
986.672636	22.485555	69.584014
986.248620	38.091041	69.589018
985.578822	45.447034	69.594023
984.989317	29.883029	69.599028
983.910753	35.017438	69.604033
983.774036	31.369594	69.609038
982.788994	40.119334	69.614042
981.987017	40.376290	69.619047
981.414167	31.890280	69.624052
980.786743	40.898512	69.629057
980.204032	33.699310	69.634062
979.104210	33.221478	69.639066
978.642338	35.433391	69.644071
978.449163	31.647872	69.649076
977.622671	33.072542	69.654081
976.789613	34.518758	69.659086
976.169618	38.511012	69.664090
975.544428	34.854160	69.669095
975.021563	36.359830	69.674100
973.456992	44.074249	69.679105
973.091251	33.533595	69.684110
972.676746	39.134788	69.689114
972.302264	40.599501	69.694119
972.130630	32.751407	69.699124
971.330216	38.805097	69.704129
970.386080	32.895031	69.709134
969.689337	30.277759	69.714138
968.472281	38.051999	69.719143
967.876610	35.667807	69.724148
967.371809	38.406957	69.729153
967.064261	31.610259	69.734158
966.622869	36.378354	69.739162
965.615494	36.306871	69.744167
965.197099	30.451924	69.749172
964.464182	34.257140	69.754177
963.245252	39.972146	69.759182
962.753583	26.564087	69.764186
961.891564	37.257594	69.769191
961.599897	38.079915	69.774196
961.271391	45.673345	69.779201
960.667843	29.815112	69.784206
959.453392	36.865107	69.789210
958.282007	35.796266	69.794215
958.076222	25.706416	69.799220
957.648172	32.030442	69.804225
957.455035	40.649443	69.809230
956.158148	38.545574	69.814234
955.489430	35.170049	69.819239
955.157353	34.536941	69.824244
954.513680	38.540851	69.829249
953.697647	35.508897	69.834254
952.862494	32.274978	69.839258
952.489536	36.477087	69.844263
952.006738	30.794820	69.849268
951.144454	38.265027	69.854273
950.339330	36.735776	69.859278
949.764127	37.601640	69.864282
948.798003	32.947205	69.869287
947.930902	32.225770	69.874292
947.066675	45.160524	69.879297
946.716745	35.601396	69.884302
946.675582	36.219849	69.889306
946.009334	37.240554	69.894311
945.725464	31.887760	69.899316
944.453119	39.322297	69.904321
944.204486	33.970203	69.909326
943.432785	33.384978	69.914330
941.788387	42.775830	69.919335
941.733919	26.931157	69.924340
941.031693	37.184494	69.929345
940.682374	37.276388	69.934350
940.188221	33.343224	69.939354
939.281620	35.441409	69.944359
938.943680	36.920811	69.949364
937.496148	46.688777	69.954369
936.710517	36.850474	69.959374
936.328603	39.789273	69.964378
935.505520	46.978855	69.969383
935.449717	35.644552	69.974388
934.628692	44.068580	69.979393
934.328163	41.645312	69.984398
933.372376	47.562889	69.989402
932.550225	40.330838	69.994407
932.091835	39.981190	69.999412
931.027588	36.455724	70.004417
930.614568	36.890499	70.009422
930.209167	36.336873	70.014426
929.248732	43.753321	70.019431
928.417479	39.176779	70.024436
927.880796	40.782430	70.029441
927.610986	35.906802	70.034446
926.780865	40.802999	70.039450
925.398650	41.174390	70.044455
925.187111	41.119779	70.049460
924.415897	51.749967	70.054465
924.463197	42.480867	70.059470
923.294491	40.282498	70.064474
922.516352	42.178893	70.069479
922.147544	39.594602	70.074484
921.250919	44.755279	70.079489
920.708240	42.452552	70.084494
919.536143	39.852595	70.089498
919.058842	35.326963	70.094503
918.696404	31.793896	70.099508
918.049614	37.052008	70.104513
917.536997	33.907124	70.109518
916.826071	32.077460	70.114522
916.067674	37.632460	70.119527
916.136491	36.101335	70.124532
914.522064	36.564882	70.129537
913.733720	37.862074	70.134542
913.290359	40.280790	70.139546
912.541747	40.349500	70.144551
912.529639	34.817841	70.149556
911.220052	43.901533	70.154561
910.609852	39.078503	70.159566
910.362007	36.348805	70.164570
909.414324	32.718066	70.169575
908.506139	39.380291	70.174580
907.746911	39.436499	70.179585
907.270792	32.559406	70.184590
907.234240	32.415445	70.189594
906.060171	37.940405	70.194599
905.584940	31.589884	70.199604
904.892414	40.452367	70.204609
904.463459	32.257299	70.209614
903.468224	28.747674	70.214618
902.395066	32.848332	70.219623
902.344572	29.006998	70.224628
901.564939	27.139388	70.229633
901.275539	23.476429	70.234638
900.316855	21.713012	70.239642
899.242670	36.095732	70.244647
899.063758	26.383245	70.249652
898.228790	26.468857	70.254657
897.294713	29.653235	70.259662
896.695152	36.728399	70.264666
896.234175	36.133160	70.269671
895.954078	23.356940	70.274676
894.798224	39.280754	70.279681
894.226965	32.034024	70.284686
893.901237	38.136766	70.289690
893.075481	38.585196	70.294695
892.126833	34.733840	70.299700
891.311087	38.646877	70.304705
890.772394	36.067553	70.309710
890.677296	37.760628	70.314714
889.493381	41.659721	70.319719
888.571234	39.267584	70.324724
887.947626	36.293338	70.329729
887.595881	37.781251	70.334734
887.541453	44.873740	70.339738
886.246292	45.485192	70.344743
885.952866	31.216112	70.349748
885.352758	26.782577	70.354753
884.411996	36.503022	70.359758
883.156007	38.617409	70.364762
882.577446	43.747975	70.369767
882.425286	36.972293	70.374772
881.830701	44.048248	70.379777
881.394538	41.299639	70.384782
880.626909	35.072932	70.389786
879.722309	48.376834	70.394791
879.133939	41.711579	70.399796
878.214017	44.119416	70.404801
877.538872	39.261000	70.409806
877.112959	35.272834	70.414810
876.521466	42.042362	70.419815
876.123230	33.353548	70.424820
875.056247	41.446146	70.429825
874.291674	41.810726	70.434830
873.949435	25.846287	70.439834
873.018765	41.486683	70.444839
872.341935	41.081925	70.449844
871.593811	42.604544	70.454849
871.229878	32.219751	70.459854
870.808811	29.605942	70.464858
869.230584	36.199778	70.469863
868.952689	38.163226	70.474868
868.449670	33.160722	70.479873
867.741147	38.619484	70.484878
867.922587	25.241522	70.489882
866.546168	39.432658	70.494887
865.879323	28.908421	70.499892
865.107644	35.153109	70.504897
864.293449	36.955909	70.509902
863.460398	34.453406	70.514906
862.432823	41.303385	70.519911
862.245783	33.432528	70.524916
862.018361	34.014395	70.529921
861.393518	38.676082	70.534926
861.153888	41.625360	70.539930
860.137977	41.373926	70.544935
859.723098	40.602620	70.549940
858.049562	40.419588	70.554945
857.641851	39.962537	70.559950
857.030160	42.718720	70.564954
856.501087	47.478710	70.569959
856.132763	38.223733	70.574964
855.354532	40.208472	70.579969
854.641443	42.138688	70.584974
854.103116	36.739676	70.589978
853.291165	45.785187	70.594983
852.826516	37.945900	70.599988
851.867803	40.454539	70.604993
851.231718	42.989098	70.609998
850.975826	35.242744	70.615002
850.152865	42.388170	70.620007
849.465495	33.926737	70.625012
848.668776	46.611066	70.630017
848.228109	37.197293	70.635022
847.296018	36.019452	70.640026
846.500163	48.651605	70.645031
846.369329	38.160325	70.650036
845.635701	37.162209	70.655041
844.616309	42.977971	70.660046
843.991695	42.448213	70.665050
843.163506	46.410556	70.670055
842.950327	44.689345	70.675060
841.798717	43.678914	70.680065
840.989849	37.616482	70.685070
840.511828	27.768686	70.690074
839.900666	34.178643	70.695079
840.252674	32.768023	70.700084
838.905159	41.416227	70.705089
838.228044	40.453273	70.710094
838.038475	32.123923	70.715098
836.835891	42.037449	70.720103
836.104608	40.042313	70.725108
835.195555	41.920147	70.730113
834.610951	44.722486	70.735118
834.168950	31.196173	70.740122
833.178512	42.271281	70.745127
832.787617	35.675536	70.750132
832.294405	40.204311	70.755137
831.825511	36.421695	70.760142
831.094846	31.671484	70.765146
829.760799	37.414331	70.770151
829.975636	41.593853	70.775156
828.802822	33.796337	70.780161
827.678078	38.777305	70.785166
827.163722	37.532976	70.790170
826.677684	42.387045	70.795175
826.313506	35.654583	70.800180
826.052153	38.735056	70.805185
824.868255	41.580753	70.810190
824.458277	35.404370	70.815194
823.392177	31.593817	70.820199
823.209081	31.474761	70.825204
821.975131	37.625885	70.830209
821.303797	44.777146	70.835214
820.770994	33.064622	70.840218
820.214018	39.995824	70.845223
819.887356	32.888379	70.850228
818.839889	33.149772	70.855233
818.083280	36.181346	70.860238
817.926706	27.520315	70.865242
816.951433	36.878836	70.870247
816.370470	30.560939	70.875252
815.577237	39.486777	70.880257
814.957689	37.062270	70.885262
814.764086	33.653736	70.890266
813.490771	40.024023	70.895271
812.903191	33.210431	70.900276
812.431781	40.782458	70.905281
811.635506	40.087643	70.910286
811.255978	30.006553	70.915290
810.310023	40.289250	70.920295
809.717702	30.136376	70.925300
809.137678	33.603474	70.930305
808.145893	43.267409	70.935310
807.535389	24.089238	70.940314
806.683297	41.030759	70.945319
806.545777	23.985064	70.950324
806.251654	26.540888	70.955329
804.856087	38.415364	70.960334
804.704307	33.675512	70.965338
804.129250	29.649603	70.970343
803.450490	29.576337	70.975348
801.952401	29.392223	70.980353
801.296938	32.484971	70.985358
801.096776	34.082808	70.990362
800.421983	39.804302	70.995367
800.201788	29.589039	71.000372
799.036582	34.831929	71.005377
798.395198	38.939589	71.010382
798.394266	30.138663	71.015386
796.817348	46.534825	71.020391
796.296191	33.445330	71.025396
795.583083	37.723683	71.030401
795.192696	32.381564	71.035406
795.099858	37.570439	71.040410
793.742203	42.399263	71.045415
793.349047	33.820050	71.050420
792.842824	37.808421	71.055425
791.548149	39.020672	71.060430
790.378169	33.626039	71.065434
789.868342	35.651648	71.070439
789.611851	34.569707	71.075444
789.262165	28.973526	71.080449
788.858251	31.751839	71.085454
788.809719	32.444007	71.090458
787.583772	31.893297	71.095463
786.870525	38.931384	71.100468
785.808223	34.765423	71.105473
785.118558	37.709078	71.110478
784.864441	31.802788	71.115482
784.289127	41.313694	71.120487
783.489444	35.486370	71.125492
782.412148	33.617300	71.130497
781.725393	37.137666	71.135502
781.487970	38.189494	71.140506
779.944241	36.211751	71.145511
779.311876	36.086950	71.150516
779.027342	34.121637	71.155521
778.710235	40.587297	71.160526
778.658249	34.117386	71.165530
777.318297	37.789051	71.170535
776.390959	33.232596	71.175540
776.107097	37.078336	71.180545
775.594595	35.795876	71.185550
775.143661	32.374697	71.190554
773.891995	39.974750	71.195559
773.302634	32.395043	71.200564
772.637268	28.996964	71.205569
772.151808	32.021653	71.210574
771.244103	31.871302	71.215578
770.518250	40.155633	71.220583
770.278297	32.670113	71.225588
769.980549	35.253328	71.230593
768.496197	35.883921	71.235598
768.080804	28.866310	71.240602
767.266612	34.625772	71.245607
767.167573	37.458055	71.250612
766.155038	36.234704	71.255617
765.346422	34.802267	71.260622
764.990413	32.059847	71.265626
764.301998	32.647305	71.270631
763.178265	25.726699	71.275636
762.548801	28.761699	71.280641
761.714127	35.226178	71.285646
762.131883	29.991952	71.290650
761.076289	41.369193	71.295655
760.334745	33.831064	71.300660
760.144936	27.890887	71.305665
758.775471	33.153696	71.310670
758.035027	32.647133	71.315674
757.028092	33.578620	71.320679
756.942807	32.321190	71.325684
756.852688	34.046592	71.330689
755.169752	38.827871	71.335694
754.602206	31.793485	71.340698
753.776727	29.357627	71.345703
753.678304	34.988943	71.350708
753.396711	35.467478	71.355713
752.249939	30.113327	71.360718
751.590991	25.824819	71.365722
751.065842	38.262492	71.370727
750.281577	27.345405	71.375732
749.415060	43.112809	71.380737
748.434975	44.371192	71.385742
748.279404	33.694632	71.390746
747.560565	36.491550	71.395751
747.548743	36.135494	71.400756
746.237354	31.078795	71.405761
745.490068	38.560708	71.410766
745.414469	28.836529	71.415770
744.266065	46.512804	71.420775
743.258161	28.609046	71.425780
743.094607	34.995064	71.430785
742.264492	40.925806	71.435790
741.901986	30.141846	71.440794
740.435035	42.054526	71.445799
740.143418	31.727641	71.450804
739.774039	35.705271	71.455809
739.375685	38.334470	71.460814
738.517142	29.726866	71.465818
737.557225	37.736228	71.470823
737.131469	39.125556	71.475828
736.414503	25.535825	71.480833
735.152421	34.569443	71.485838
734.893534	27.353456	71.490842
734.172959	31.027452	71.495847
733.985661	28.777001	71.500852
733.633879	30.290170	71.505857
732.687218	36.241047	71.510862
732.102838	22.622325	71.515866
731.057749	34.543530	71.520871
730.076065	22.306419	71.525876
729.592957	29.430875	71.530881
728.537396	39.891896	71.535886
728.252127	27.422472	71.540890
727.924271	39.812965	71.545895
727.689974	38.128246	71.550900
726.665650	35.990566	71.555905
725.808089	30.353834	71.560910
725.253232	21.011904	71.565914
723.967362	31.533246	71.570919
723.323952	23.739812	71.575924
723.038913	27.674050	71.580929
722.614575	30.080303	71.585934
721.971950	32.262688	71.590938
721.548437	32.185073	71.595943
720.848063	35.724968	71.600948
720.131269	33.159851	71.605953
719.325687	30.019083	71.610958
718.334631	19.093940	71.615962
717.745485	34.482858	71.620967
717.209924	25.082662	71.625972
716.827067	32.221120	71.630977
715.813493	32.510275	71.635982
715.322429	26.974469	71.640986
714.760024	28.514869	71.645991
714.235388	27.989726	71.650996
713.402304	28.146064	71.656001
712.135376	37.402818	71.661006
711.860836	32.898569	71.666010
710.880616	38.484207	71.671015
710.870976	32.967939	71.676020
710.069817	33.742100	71.681025
708.929002	36.642489	71.686030
708.592694	24.102351	71.691034
708.250613	40.760826	71.696039
707.625366	29.728547	71.701044
706.673745	32.308648	71.706049
705.911434	36.850326	71.711054
705.522550	29.617195	71.716058
704.324967	39.263463	71.721063
703.655525	30.152672	71.726068
703.309594	30.974198	71.731073
702.720446	38.404132	71.736078
702.548527	25.930860	71.741082
701.252730	31.981493	71.746087
700.511302	35.911134	71.751092
700.244651	33.744286	71.756097
699.720758	34.035901	71.761102
698.688435	31.940508	71.766106
697.819867	31.470134	71.771111
697.305024	26.739221	71.776116
697.061912	26.716465	71.781121
695.960896	31.442966	71.786126
695.493764	30.033450	71.791130
694.732752	35.797079	71.796135
694.430670	30.321071	71.801140
693.513278	33.226891	71.806145
692.447233	32.724885	71.811150
692.138893	23.725338	71.816154
691.679431	36.117861	71.821159
690.949898	34.496235	71.826164
690.069109	35.887063	71.831169
689.304085	29.185346	71.836174
689.139040	27.391833	71.841178
688.020473	36.500392	71.846183
687.027744	27.214003	71.851188
686.614577	28.971922	71.856193
685.985716	32.859987	71.861198
685.990322	26.830515	71.866202
685.187588	37.025780	71.871207
683.879473	32.244566	71.876212
683.384178	28.955053	71.881217
682.916550	22.784734	71.886222
682.610825	25.347148	71.891226
681.359681	33.418668	71.896231
680.839265	30.410703	71.901236
680.586567	23.269437	71.906241
679.958247	30.716647	71.911246
678.773695	29.627959	71.916250
678.112953	32.306832	71.921255
677.971443	30.810774	71.926260
677.324920	28.680765	71.931265
675.908475	27.059718	71.936270
675.669189	23.155422	71.941274
675.012307	29.922774	71.946279
674.347024	25.878153	71.951284
673.439645	27.446688	71.956289
672.552937	29.300517	71.961294
672.522842	22.565358	71.966298
671.982661	31.588123	71.971303
671.027955	30.540110	71.976308
670.509377	33.478625	71.981313
669.836299	38.181147	71.986318
669.360484	27.757455	71.991322
667.930773	31.492352	71.996327
667.339384	40.687284	72.001332
667.106153	38.163451	72.006337
666.636020	43.924925	72.011342
665.567695	32.322966	72.016346
664.831942	34.138567	72.021351
664.333717	39.109717	72.026356
663.662534	39.748075	72.031361
663.212037	36.840943	72.036366
662.427015	35.885762	72.041370
661.560201	46.114898	72.046375
661.170387	38.005122	72.051380
660.515959	38.680237	72.056385
659.687470	44.136075	72.061390
659.310461	36.456353	72.066394
658.576633	43.459898	72.071399
658.019507	39.830146	72.076404
657.345241	29.078509	72.081409
656.341384	33.892057	72.086414
655.944439	27.317820	72.091418
655.168479	39.333389	72.096423
654.067165	34.486142	72.101428
653.822914	30.729297	72.106433
652.912718	37.388761	72.111438
652.909784	36.588159	72.116442
651.975939	35.106317	72.121447
650.971173	37.639707	72.126452
650.681966	32.007114	72.131457
650.107892	29.324673	72.136462
649.383361	26.652000	72.141466
648.511309	30.693920	72.146471
648.029931	31.289439	72.151476
647.153407	23.536309	72.156481
645.855203	39.594828	72.161486
645.415066	27.273093	72.166490
644.822470	39.060763	72.171495
644.597760	32.356595	72.176500
644.309577	33.244627	72.181505
643.563158	29.094663	72.186510
642.821455	28.334442	72.191514
641.990310	28.684463	72.196519
641.614537	23.541905	72.201524
640.602180	24.684040	72.206529
639.383490	32.474438	72.211534
639.178055	28.168935	72.216538
638.973536	26.812226	72.221543
638.209799	26.025553	72.226548
637.386616	29.838918	72.231553
636.453003	30.023906	72.236558
636.268627	30.982141	72.241562
635.340093	29.057908	72.246567
634.436185	28.232057	72.251572
634.055777	26.428692	72.256577
633.410936	38.786086	72.261582
632.717608	26.132512	72.266586
631.886593	36.288137	72.271591
631.274882	31.910140	72.276596
630.731665	33.387577	72.281601
630.114313	33.228883	72.286606
629.545510	22.690705	72.291610
628.790735	28.224693	72.296615
627.919237	29.147277	72.301620
627.652751	17.652620	72.306625
626.677380	31.040371	72.311630
626.224163	23.767044	72.316634
625.375836	32.340567	72.321639
624.873665	34.215174	72.326644
623.743715	24.196880	72.331649
623.247794	30.855027	72.336654
622.854908	22.611716	72.341658
622.135042	30.429911	72.346663
621.515635	29.109318	72.351668
620.970269	23.990621	72.356673
620.034806	39.534056	72.361678
619.694516	25.931694	72.366682
619.135805	30.516661	72.371687
617.735194	37.397745	72.376692
617.231233	29.640483	72.381697
616.557020	38.314017	72.386702
616.592299	21.109962	72.391706
615.835943	29.765034	72.396711
614.966486	30.815033	72.401716
614.315703	28.777185	72.406721
613.533703	32.336413	72.411726
612.214196	28.511125	72.416730
611.876188	30.679714	72.421735
611.273068	36.954388	72.426740
611.166019	34.129765	72.431745
610.366870	35.212723	72.436750
609.832171	23.909018	72.441754
608.634256	29.737518	72.446759
607.991164	29.097222	72.451764
607.794834	27.788099	72.456769
607.446161	23.839732	72.461774
606.366226	29.289894	72.466778
605.600521	26.806722	72.471783
604.886783	24.236425	72.476788
604.020568	19.241377	72.481793
603.195152	33.557744	72.486798
603.006409	22.003397	72.491802
602.612415	25.436173	72.496807
601.901322	23.836871	72.501812
601.131198	26.848577	72.506817
600.408909	23.647278	72.511822
600.020085	18.637699	72.516826
598.766254	28.198340	72.521831
597.876068	29.858781	72.526836
597.798787	27.769019	72.531841
597.198309	30.752130	72.536846
596.616516	27.102672	72.541850
595.637011	26.030253	72.546855
594.790458	34.676043	72.551860
594.429631	31.855572	72.556865
593.770568	33.840329	72.561870
593.091144	35.721096	72.566874
592.351473	31.675732	72.571879
591.769116	36.341743	72.576884
591.524614	30.038134	72.581889
590.185731	38.552606	72.586894
589.605413	36.426269	72.591898
589.271552	34.872543	72.596903
588.349677	40.057840	72.601908
587.945045	28.094748	72.606913
586.636523	33.382629	72.611918
586.521988	34.500056	72.616922
586.286854	26.400362	72.621927
585.319691	29.030290	72.626932
584.463810	22.185391	72.631937
583.474079	36.739250	72.636942
583.348105	30.426226	72.641946
582.933238	42.040515	72.646951
581.655907	31.099529	72.651956
581.348980	27.153979	72.656961
580.731764	35.793208	72.661966
579.928320	36.842166	72.666970
579.080558	25.796495	72.671975
578.586419	34.330963	72.676980
578.163585	25.225097	72.681985
576.690669	37.037871	72.686990
576.192664	27.297418	72.691994
576.272570	24.808879	72.696999
575.505818	35.310675	72.702004
574.563976	36.219252	72.707009
573.486501	34.616813	72.712014
573.590210	28.256168	72.717018
572.986312	39.058461	72.722023
571.688088	35.769129	72.727028
570.666506	26.283966	72.732033
570.131383	30.718526	72.737038
570.031602	29.931775	72.742042
569.816913	36.712295	72.747047
569.023929	31.913752	72.752052
567.972300	37.649586	72.757057
567.406064	33.522987	72.762062
566.518140	30.824326	72.767066
565.529960	32.697508	72.772071
564.794955	27.998544	72.777076
564.505358	25.710788	72.782081
564.071681	24.433167	72.787086
564.132741	30.679324	72.792090
562.961569	26.925056	72.797095
561.727244	24.775167	72.802100
561.389201	24.089447	72.807105
560.612383	29.538653	72.812110
559.819675	35.547063	72.817114
559.194231	30.799109	72.822119
558.691396	29.092529	72.827124
558.773647	23.656256	72.832129
557.249211	34.606755	72.837134
556.367689	27.879491	72.842138
556.012102	23.462298	72.847143
555.513335	26.754072	72.852148
555.237592	18.980982	72.857153
553.996286	22.561346	72.862158
553.490302	26.273744	72.867162
553.048650	24.752965	72.872167
551.438117	33.779083	72.877172
551.315684	23.384297	72.882177
550.445233	32.130098	72.887182
550.059933	20.760040	72.892186
549.771114	26.006932	72.897191
548.661323	34.048106	72.902196
548.206478	20.352053	72.907201
547.369296	27.619663	72.912206
546.990483	28.717687	72.917210
546.388447	33.159756	72.922215
545.101277	32.073287	72.927220
544.822761	27.915057	72.932225
544.113014	32.158239	72.937230
543.688072	27.648014	72.942234
542.599341	21.185581	72.947239
541.888674	23.746280	72.952244
541.749307	30.976853	72.957249
540.722752	28.128395	72.962254
540.624170	22.463882	72.967258
539.682710	22.535038	72.972263
538.833790	27.860114	72.977268
538.675304	22.593079	72.982273
537.449192	35.565053	72.987278
536.469782	27.561851	72.992282
536.231512	34.249932	72.997287
535.693578	40.668780	73.002292
535.191640	31.545560	73.007297
533.800154	41.986036	73.012302
533.485460	40.069715	73.017306
533.162963	35.740293	73.022311
532.802725	34.749026	73.027316
531.726189	35.936121	73.032321
530.539813	45.117043	73.037326
530.290407	37.128438	73.042330
530.055775	34.606423	73.047335
528.473563	38.264763	73.052340
528.011879	31.937413	73.057345
527.249995	37.325903	73.062350
527.193277	38.801557	73.067354
526.878906	36.418403	73.072359
525.793580	34.902393	73.077364
525.350165	36.187332	73.082369
524.882800	37.865600	73.087374
523.718940	32.824952	73.092378
522.794506	39.458338	73.097383
522.007598	38.244879	73.102388
522.077723	32.583451	73.107393
520.965287	33.211713	73.112398
520.032497	30.253709	73.117402
519.173487	36.816748	73.122407
518.698084	38.947310	73.127412
519.103670	25.672441	73.132417
517.981517	34.873093	73.137422
517.219286	34.062563	73.142426
516.396313	36.177532	73.147431
515.769729	37.171527	73.152436
515.538913	33.237516	73.157441
514.334615	43.173514	73.162446
513.743206	29.254789	73.167450
513.341287	30.228764	73.172455
512.305341	32.650477	73.177460
511.680273	27.662779	73.182465
511.179043	36.785018	73.187470
510.729688	31.051804	73.192474
510.062490	34.832472	73.197479
508.789336	34.686819	73.202484
508.411084	27.051491	73.207489
507.885446	40.995269	73.212494
507.544657	30.439726	73.217498
506.719690	27.619095	73.222503
505.319449	35.052113	73.227508
505.525287	24.245488	73.232513
504.677366	32.708589	73.237518
503.398781	34.060349	73.242522
502.841568	34.612783	73.247527
501.965504	35.618141	73.252532
501.946747	32.189673	73.257537
501.579240	33.055665	73.262542
501.292784	38.587620	73.267546
500.115013	30.177636	73.272551
499.328857	36.686495	73.277556
498.581057	30.876250	73.282561
497.667370	35.095163	73.287566
497.195180	28.138707	73.292570
496.624792	30.129862	73.297575
496.083649	35.456383	73.302580
495.248067	37.068736	73.307585
494.339787	39.315576	73.312590
493.767307	34.593896	73.317594
493.502105	27.128221	73.322599
493.027483	33.779839	73.327604
492.202757	30.727359	73.332609
491.697595	36.633205	73.337614
490.723572	33.959329	73.342618
489.942192	30.838442	73.347623
488.887300	36.864986	73.352628
488.718451	30.683384	73.357633
488.369194	28.081865	73.362638
487.479893	27.629061	73.367642
486.322947	33.632439	73.372647
485.855914	36.247381	73.377652
485.720876	29.577840	73.382657
484.832066	33.355972	73.387662
483.942434	36.533411	73.392666
483.294634	27.824536	73.397671
482.838637	33.533314	73.402676
482.499366	28.815486	73.407681
481.328117	33.662071	73.412686
480.773346	31.888088	73.417690
480.202383	29.903794	73.422695
479.372604	36.481110	73.427700
478.844207	26.930035	73.432705
477.704929	34.114907	73.437710
477.323507	33.270528	73.442714
476.990938	27.700069	73.447719
476.097942	39.144529	73.452724
475.469794	29.177256	73.457729
474.826058	40.358075	73.462734
474.192661	38.352189	73.467738
473.889095	28.443592	73.472743
472.885293	37.056119	73.477748
472.465095	25.694792	73.482753
471.884142	31.475518	73.487758
470.778630	35.841698	73.492762
470.051509	32.343162	73.497767
469.321214	34.899123	73.502772
469.150067	22.957219	73.507777
468.212122	27.727213	73.512782
467.005718	35.296526	73.517786
466.561760	25.937009	73.522791
466.059258	34.141657	73.527796
466.168574	27.209259	73.532801
465.219304	28.756154	73.537806
464.117501	28.821346	73.542810
463.891246	19.966472	73.547815
462.722071	29.333906	73.552820
461.839220	17.505400	73.557825
461.030836	16.577663	73.562830
460.273459	17.556239	73.567834
460.138352	22.783376	73.572839
459.841383	29.528117	73.577844
459.645087	27.253897	73.582849
458.309846	32.194429	73.587854
457.831720	29.492021	73.592858
457.578303	23.454789	73.597863
456.222993	30.379194	73.602868
455.542117	28.686811	73.607873
454.762720	21.629505	73.612878
454.332147	22.362047	73.617882
454.206100	18.819791	73.622887
452.817716	28.275771	73.627892
452.292664	22.474210	73.632897
451.612400	29.163327	73.637902
451.284834	20.438139	73.642906
450.272442	16.955103	73.647911
449.173615	26.921618	73.652916
449.197555	18.812215	73.657921
448.536591	31.539628	73.662926
447.819510	36.514140	73.667930
447.093630	25.755043	73.672935
446.351772	30.552150	73.677940
446.425285	28.361099	73.682945
445.237710	34.905544	73.687950
444.334515	32.425408	73.692954
444.021450	21.550077	73.697959
442.850088	30.777517	73.702964
441.993644	24.286007	73.707969
441.184816	29.776614	73.712974
440.615186	31.589462	73.717978
440.010347	27.995758	73.722983
439.766759	30.001086	73.727988
439.858702	27.095885	73.732993
439.155996	22.729292	73.737998
438.006532	30.384160	73.743002
437.642090	24.391430	73.748007
436.207779	30.087357	73.753012
435.634848	31.985888	73.758017
435.099894	32.011236	73.763022
434.775372	38.526982	73.768026
434.018772	29.889077	73.773031
432.854516	34.663605	73.778036
432.592474	26.304873	73.783041
432.210753	29.816140	73.788046
431.084023	29.707121	73.793050
430.333668	24.007698	73.798055
429.726283	29.906184	73.803060
428.998895	25.909383	73.808065
428.889305	29.009856	73.813070
428.576736	35.372306	73.818074
427.501442	31.591791	73.823079
426.869269	30.538214	73.828084
425.903033	25.425130	73.833089
424.964516	27.801390	73.838094
424.252521	28.348541	73.843098
423.898086	24.566708	73.848103
423.405465	32.260425	73.853108
422.995158	16.042054	73.858113
421.910283	24.987633	73.863118
421.267569	28.813304	73.868122
420.866280	28.008371	73.873127
419.614371	36.510636	73.878132
418.884441	31.498673	73.883137
418.724853	26.261789	73.888142
417.871167	26.336351	73.893146
417.976472	14.911814	73.898151
416.715546	27.222314	73.903156
416.014569	29.693191	73.908161
415.695348	25.153534	73.913166
414.827597	25.541002	73.918170
413.936322	22.620583	73.923175
413.406888	30.490478	73.928180
412.896128	23.672659	73.933185
412.279557	33.712158	73.938190
410.970864	36.849162	73.943194
410.567852	30.660729	73.948199
409.960906	33.553446	73.953204
409.710031	32.459616	73.958209
408.808044	32.215445	73.963214
407.941826	34.058214	73.968218
407.352164	26.857149	73.973223
407.112632	29.607740	73.978228
406.409570	25.419411	73.983233
405.504197	23.538888	73.988238
404.699892	26.212316	73.993242
404.716838	31.782660	73.998247
403.554918	28.448050	74.003252
402.865801	30.366679	74.008257
402.429455	33.292138	74.013262
401.220455	28.976271	74.018266
400.836018	24.368160	74.023271
400.093930	33.602907	74.028276
399.441654	30.429940	74.033281
399.167627	23.634326	74.038286
397.826454	34.128342	74.043290
397.501202	28.898935	74.048295
396.594885	27.300842	74.053300
396.362460	26.732358	74.058305
395.899778	29.401814	74.063310
394.631626	31.945732	74.068314
394.246606	31.340063	74.073319
393.264232	32.482248	74.078324
393.193179	26.701397	74.083329
392.272650	34.931667	74.088334
391.217340	35.930934	74.093338
391.000877	24.792635	74.098343
390.271268	31.276737	74.103348
389.627496	27.037964	74.108353
388.905003	32.024390	74.113358
388.013781	32.989624	74.118362
387.950230	35.011999	74.123367
387.121080	40.245662	74.128372
386.178809	25.835694	74.133377
385.247610	31.139234	74.138382
384.667343	37.057064	74.143386
384.512381	27.347161	74.148391
384.263674	32.931452	74.153396
383.317147	33.656340	74.158401
382.445816	27.416388	74.163406
381.754872	42.772673	74.168410
380.742034	32.712193	74.173415
380.108635	39.409630	74.178420
379.730565	30.810774	74.183425
379.338912	35.373892	74.188430
378.468422	37.789793	74.193434
377.687084	23.833584	74.198439
377.166011	32.228859	74.203444
376.696657	33.360260	74.208449
375.689756	31.670970	74.213454
374.598958	22.340445	74.218458
374.541936	24.989412	74.223463
373.669990	27.802940	74.228468
373.314596	30.001135	74.233473
372.369545	25.515487	74.238478
371.292128	28.096829	74.243482
371.300444	29.426500	74.248487
370.796471	36.675752	74.253492
370.169042	33.779533	74.258497
369.176032	35.844374	74.263502
368.616150	31.999095	74.268506
367.968049	32.001487	74.273511
366.757776	35.025056	74.278516
366.349848	34.631202	74.283521
365.923523	39.859022	74.288526
365.312048	39.404565	74.293530
364.772598	42.952019	74.298535
363.789564	40.470444	74.303540
363.171567	33.840037	74.308545
363.020139	36.740597	74.313550
362.060097	37.149099	74.318554
361.381025	24.783531	74.323559
360.523407	30.122660	74.328564
359.439886	26.641537	74.333569
358.871272	32.377738	74.338574
358.100478	39.707363	74.343578
357.916182	31.837729	74.348583
357.354769	38.418040	74.353588
357.203338	38.240356	74.358593
355.930945	34.775140	74.363598
354.939155	37.621968	74.368602
354.615734	34.719882	74.373607
353.959829	33.050358	74.378612
353.199029	30.224287	74.383617
352.305923	33.162621	74.388622
351.809692	28.788381	74.393626
351.549369	29.810778	74.398631
350.718457	42.374484	74.403636
349.879757	37.693695	74.408641
349.163603	27.213788	74.413646
348.630885	34.254731	74.418650
348.343583	29.806193	74.423655
347.470029	31.601265	74.428660
346.945502	28.713886	74.433665
346.338699	27.492283	74.438670
345.377755	32.537222	74.443674
344.513212	29.360254	74.448679
343.527624	33.444018	74.453684
343.268241	26.266030	74.458689
342.725680	32.803912	74.463694
342.087855	33.495386	74.468698
341.871437	36.627079	74.473703
340.803523	30.738599	74.478708
340.253855	31.371868	74.483713
338.920596	33.222862	74.488718
338.165412	37.467028	74.493722
338.062246	30.942238	74.498727
337.551121	40.561243	74.503732
337.366347	27.279533	74.508737
336.208108	25.421990	74.513742
335.087140	35.710626	74.518746
334.964531	30.220273	74.523751
334.416609	33.805350	74.528756
333.481105	33.188077	74.533761
332.524961	31.714645	74.538766
331.829008	35.263392	74.543770
331.677628	28.872445	74.548775
330.894896	35.365030	74.553780
329.860844	26.504881	74.558785
329.592075	28.645119	74.563790
328.812741	36.805596	74.568794
328.539611	31.340810	74.573799
327.244913	31.178184	74.578804
326.888434	32.114983	74.583809
326.357941	29.118172	74.588814
325.731025	40.588069	74.593818
324.896114	29.166724	74.598823
324.055494	32.582408	74.603828
323.258192	40.203274	74.608833
323.251874	34.038368	74.613838
322.031818	35.800365	74.618842
321.406627	30.473696	74.623847
320.638708	39.947548	74.628852
320.185792	27.590104	74.633857
320.152579	29.423138	74.638862
318.796984	39.460592	74.643866
318.359396	24.282666	74.648871
317.754633	31.904381	74.653876
317.128662	33.967511	74.658881
316.338232	35.564840	74.663886
315.322803	35.116432	74.668890
315.248830	25.172858	74.673895
315.026290	37.645910	74.678900
314.141107	28.340990	74.683905
313.560507	32.749725	74.688910
311.948111	32.177269	74.693914
311.422983	30.409642	74.698919
310.824407	35.500917	74.703924
310.199206	31.503637	74.708929
310.019771	31.817703	74.713934
308.823667	37.016833	74.718938
308.145355	26.996117	74.723943
307.588244	33.545786	74.728948
307.029786	30.398894	74.733953
306.629861	24.948016	74.738958
305.420024	28.137124	74.743962
304.898698	25.591448	74.748967
304.101831	32.723386	74.753972
303.880913	28.552859	74.758977
303.562209	25.486027	74.763982
302.433658	36.547020	74.768986
302.111265	28.571674	74.773991
301.143685	35.492702	74.778996
300.487849	39.052409	74.784001
299.765526	35.228309	74.789006
299.020234	40.877565	74.794010
298.655620	33.244842	74.799015
297.578825	32.678488	74.804020
296.900366	36.560349	74.809025
296.416151	35.295564	74.814030
295.612473	34.904877	74.819034
295.713747	31.927223	74.824039
294.479588	28.246212	74.829044
293.695074	34.672856	74.834049
293.382197	28.992061	74.839054
292.562837	37.561052	74.844058
291.963319	26.904880	74.849063
291.150223	24.760532	74.854068
290.461548	28.722869	74.859073
290.174014	29.139323	74.864078
288.950689	37.540891	74.869082
288.404201	28.730781	74.874087
287.983806	34.608951	74.879092
287.206776	29.134607	74.884097
286.616269	29.574122	74.889102
285.834668	34.743461	74.894106
285.316445	20.196575	74.899111
284.749137	27.509545	74.904116
284.076783	32.123724	74.909121
282.934827	26.671281	74.914126
282.056289	33.565504	74.919130
282.118226	29.012423	74.924135
281.502525	35.533589	74.929140
280.793177	29.502827	74.934145
280.076193	30.102854	74.939150
279.131244	32.625273	74.944154
278.846217	23.719876	74.949159
277.840329	29.626717	74.954164
277.020741	32.506049	74.959169
276.551376	34.794963	74.964174
275.957926	37.292893	74.969178
275.865330	27.183557	74.974183
274.844757	36.842770	74.979188
273.905380	30.977989	74.984193
273.800510	25.877482	74.989198
272.576750	38.249930	74.994202
271.766016	27.761475	74.999207
270.987011	35.921912	75.004212
270.681242	31.288670	75.009217
270.296117	29.522390	75.014222
269.573163	35.546563	75.019226
269.080014	28.199269	75.024231
268.505857	34.871511	75.029236
267.584339	32.902149	75.034241
266.194922	33.204089	75.039246
265.678528	36.386758	75.044250
265.469178	32.698521	75.049255
265.069629	39.219929	75.054260
264.492295	35.907320	75.059265
263.672010	46.140172	75.064270
262.770176	41.575137	75.069274
262.488362	30.324275	75.074279
261.519599	30.816208	75.079284
260.607733	32.825576	75.084289
260.214728	26.980941	75.089294
259.361038	38.452301	75.094298
258.597379	33.351152	75.099303
257.879307	39.484939	75.104308
257.305963	38.821002	75.109313
257.029993	31.087426	75.114318
256.547903	30.525638	75.119322
255.672499	29.223873	75.124327
254.922803	36.353036	75.129332
254.096306	36.319240	75.134337
253.841061	33.019947	75.139342
252.440659	45.237638	75.144346
252.271166	40.488055	75.149351
251.686967	36.542603	75.154356
250.844302	33.860504	75.159361
250.133658	32.507244	75.164366
249.307309	32.293653	75.169370
248.912159	32.221060	75.174375
248.594546	28.316694	75.179380
247.889234	25.078110	75.184385
246.992090	32.095159	75.189390
246.306285	35.137679	75.194394
245.835515	24.893090	75.199399
244.615006	32.718632	75.204404
243.907975	37.059227	75.209409
243.686319	24.893604	75.214414
242.897647	34.356584	75.219418
242.792149	26.539066	75.224423
241.911557	28.292717	75.229428
241.073680	29.564892	75.234433
240.347797	29.144475	75.239438
239.718778	32.662072	75.244442
238.939770	25.046542	75.249447
238.226271	25.644449	75.254452
237.653496	32.890490	75.259457
237.594752	19.705414	75.264462
236.090772	27.308062	75.269466
235.502183	19.003009	75.274471
234.953171	24.846490	75.279476
234.534521	34.505952	75.284481
234.011415	33.217418	75.289486
232.677727	27.418671	75.294490
232.493402	24.182194	75.299495
231.863152	29.619156	75.304500
230.816025	28.135040	75.309505
230.241319	18.593010	75.314510
229.521662	31.060146	75.319514
229.230112	30.963156	75.324519
229.116734	28.928055	75.329524
227.570509	33.984338	75.334529
227.215498	22.595348	75.339534
226.362197	27.613703	75.344538
226.025016	22.561277	75.349543
225.008875	29.775498	75.354548
224.224869	24.922039	75.359553
224.349763	23.746247	75.364558
223.574441	34.148551	75.369562
222.422847	28.019579	75.374567
221.709511	32.206640	75.379572
221.229074	30.564374	75.384577
220.714115	25.656985	75.389582
219.428833	38.105492	75.394586
218.599390	25.574720	75.399591
218.435246	32.544305	75.404596
217.835999	36.801490	75.409601
217.708994	28.257267	75.414606
216.532621	28.873780	75.419610
216.136175	27.205510	75.424615
215.302339	25.066072	75.429620
214.709977	30.027061	75.434625
213.781571	31.638533	75.439630
212.905794	32.555634	75.444634
212.481891	31.751188	75.449639
211.971399	30.004905	75.454644
211.449523	38.100708	75.459649
210.526787	24.980835	75.464654
209.835073	33.549994	75.469658
209.534240	25.355189	75.474663
209.115097	24.762875	75.479668
208.121746	30.981558	75.484673
207.194043	36.536914	75.489678
206.606051	33.694380	75.494682
205.949635	24.624279	75.499687
205.001203	33.205982	75.504692
204.317147	35.153818	75.509697
204.307559	36.426417	75.514702
203.777887	32.915414	75.519706
203.074344	28.588455	75.524711
202.030843	33.061551	75.529716
201.240407	31.979650	75.534721
200.894361	30.576162	75.539726
199.591416	30.555267	75.544730
199.194851	30.377252	75.549735
198.595467	33.735590	75.554740
198.218498	33.507142	75.559745
197.881379	34.641146	75.564750
196.303062	35.766457	75.569754
195.883462	29.755762	75.574759
195.542085	36.116511	75.579764
195.173094	36.161183	75.584769
193.982692	36.103425	75.589774
193.168107	33.404255	75.594778
192.893474	23.847509	75.599783
192.515532	25.117334	75.604788
191.436546	24.210753	75.609793
190.737558	24.191343	75.614798
190.108961	32.357778	75.619802
189.646790	31.609900	75.624807
188.639698	27.995246	75.629812
187.725528	28.063762	75.634817
187.455566	20.089548	75.639822
187.133607	29.164309	75.644826
186.439043	26.179500	75.649831
185.279724	28.532702	75.654836
184.419758	32.937117	75.659841
184.591881	35.464394	75.664846
183.852879	29.452588	75.669850
182.943775	37.946027	75.674855
182.456476	32.094364	75.679860
181.458456	38.274379	75.684865
181.455564	30.639205	75.689870
180.186273	34.236823	75.694874
179.500709	38.659167	75.699879
178.913286	36.373218	75.704884
177.951111	41.372681	75.709889
177.294497	43.926437	75.714894
176.392523	36.743697	75.719898
175.920820	35.694564	75.724903
175.884254	35.869164	75.729908
175.209304	36.590254	75.734913
174.751198	27.291423	75.739918
173.325982	30.193231	75.744922
172.751564	34.168919	75.749927
172.205750	28.143662	75.754932
171.900372	36.840467	75.759937
171.298831	28.835541	75.764942
170.459794	39.935576	75.769946
169.963265	38.261192	75.774951
168.903047	32.649116	75.779956
167.806384	35.356615	75.784961
167.673303	41.031293	75.789966
167.171218	35.445343	75.794970
166.824769	37.254204	75.799975
165.628570	37.717783	75.804980
164.931118	35.573962	75.809985
164.477375	29.595527	75.814990
163.841251	43.176895	75.819994
163.132548	29.699638	75.824999
162.432177	34.468124	75.830004
161.951470	32.321284	75.835009
161.209567	25.956710	75.840014
160.166020	37.161894	75.845018
159.393813	28.583361	75.850023
158.979052	31.464411	75.855028
158.745475	35.111364	75.860033
157.863952	29.227949	75.865038
156.883169	34.254038	75.870042
156.435009	28.498645	75.875047
156.309898	23.349338	75.880052
154.957656	24.607361	75.885057
154.223671	23.585862	75.890062
153.695239	32.075379	75.895066
153.575011	24.468381	75.900071
152.762627	24.976423	75.905076
151.667509	28.010113	75.910081
151.476573	21.381072	75.915086
150.588605	30.271695	75.920090
149.367114	26.073075	75.925095
148.923984	28.780453	75.930100
148.238003	34.074931	75.935105
148.169676	24.368603	75.940110
147.631128	30.938990	75.945114
146.822906	33.835473	75.950119
145.885676	28.539692	75.955124
145.392864	38.652538	75.960129
144.662329	26.311035	75.965134
143.365209	38.037632	75.970138
142.955328	31.129683	75.975143
142.818912	28.316087	75.980148
141.789402	34.513752	75.985153
141.035829	28.720329	75.990158
140.457265	35.483182	75.995162
140.100329	31.067859	76.000167
139.716266	25.789533	76.005172
138.693058	32.347317	76.010177
138.186918	30.601934	76.015182
137.381251	38.353488	76.020186
137.176500	36.642048	76.025191
135.801492	29.487450	76.030196
135.171232	38.087827	76.035201
135.049091	38.342306	76.040206
134.022313	41.723080	76.045210
133.052325	25.720204	76.050215
132.655414	31.299752	76.055220
131.937325	38.466481	76.060225
131.736755	27.965949	76.065230
130.141386	28.945786	76.070234
129.745535	25.527006	76.075239
129.606659	28.930197	76.080244
129.041382	31.679134	76.085249
128.354388	32.490467	76.090254
126.947041	34.976287	76.095258
126.420088	32.745366	76.100263
126.179695	34.463202	76.105268
125.555470	37.689899	76.110273
124.827343	37.908546	76.115278
124.031553	39.453172	76.120282
123.660166	40.956929	76.125287
123.020268	39.562464	76.130292
121.874658	36.778910	76.135297
121.225030	34.097617	76.140302
120.693420	36.487947	76.145306
120.413564	30.136439	76.150311
119.743342	31.519115	76.155316
118.485070	37.810039	76.160321
118.423416	29.126098	76.165326
117.735945	33.209712	76.170330
116.754612	33.341004	76.175335
116.196039	27.248412	76.180340
115.353454	35.600373	76.185345
115.106140	23.151865	76.190350
114.011287	32.417691	76.195354
112.953438	32.523340	76.200359
112.855005	32.674690	76.205364
112.332392	28.886617	76.210369
112.201977	28.134736	76.215374
110.707313	31.135964	76.220378
109.972736	28.908195	76.225383
109.670315	28.399788	76.230388
108.763760	38.718966	76.235393
108.269191	34.421792	76.240398
107.321939	27.441851	76.245402
106.796881	26.158389	76.250407
106.827206	27.432506	76.255412
105.148128	38.464664	76.260417
104.776602	36.554317	76.265422
104.098917	35.788784	76.270426
103.550786	36.166392	76.275431
103.479762	30.582682	76.280436
102.391024	27.023666	76.285441
101.868641	25.418078	76.290446
101.091280	30.094775	76.295450
100.294123	28.987172	76.300455
99.504181	25.593398	76.305460
98.577162	28.772192	76.310465
98.193798	23.850157	76.315470
97.641937	28.681706	76.320474
97.390987	31.664376	76.325479
96.381024	35.914543	76.330484
95.644550	36.680159	76.335489
95.381719	31.759401	76.340494
94.219218	31.481198	76.345498
93.334270	37.599056	76.350503
92.687188	25.100764	76.355508
92.320907	37.505264	76.360513
92.127575	33.402906	76.365518
91.519168	32.643676	76.370522
90.503686	28.049532	76.375527
90.287687	28.683260	76.380532
88.811905	34.288211	76.385537
88.342378	21.771070	76.390542
87.656539	37.186492	76.395546
86.999486	31.201076	76.400551
86.558179	36.391892	76.405556
85.435500	35.115432	76.410561
84.883288	26.985974	76.415566
84.348178	32.428293	76.420570
84.072958	25.338036	76.425575
83.462900	30.836463	76.430580
82.399987	24.174605	76.435585
81.881651	25.190866	76.440590
81.141409	31.787122	76.445594
80.580952	26.306703	76.450599
79.603841	24.152317	76.455604
79.026486	35.649031	76.460609
79.034501	25.067937	76.465614
78.109708	27.554096	76.470618
77.196621	24.651482	76.475623
76.471263	24.773506	76.480628
75.723426	30.584069	76.485633
75.529935	16.890653	76.490638
74.372717	29.840760	76.495642
73.627605	25.372241	76.500647
73.191815	22.270504	76.505652
72.640161	29.410698	76.510657
71.867490	29.704274	76.515662
70.900580	28.226359	76.520666
70.451912	31.081290	76.525671
70.147411	30.156901	76.530676
69.640450	33.748110	76.535681
68.766598	30.698891	76.540686
67.876202	30.520808	76.545690
67.229837	26.992182	76.550695
66.828579	34.515250	76.555700
65.742938	31.649620	76.560705
65.105823	30.158533	76.565710
64.530099	34.342610	76.570714
64.380123	34.926386	76.575719
63.340115	27.095506	76.580724
62.142615	35.857326	76.585729
62.112763	25.906750	76.590734
61.719233	29.143975	76.595738
60.924203	32.569816	76.600743
60.094777	25.206829	76.605748
59.157688	30.484603	76.610753
58.952243	26.306913	76.615758
58.018942	27.089738	76.620762
57.180363	33.622836	76.625767
56.598416	23.850204	76.630772
55.978581	28.314130	76.635777
56.009433	20.137423	76.640782
55.100534	25.918483	76.645786
54.047507	34.222021	76.650791
53.579123	22.628809	76.655796
52.227235	29.847751	76.660801
51.882547	25.734848	76.665806
51.018693	34.848736	76.670810
50.598927	32.250652	76.675815
50.464347	31.732829	76.680820
49.550535	35.146080	76.685825
48.557316	23.204488	76.690830
48.108166	26.901597	76.695834
47.535547	27.724672	76.700839
47.521937	15.371378	76.705844
46.333299	29.420916	76.710849
45.489871	31.075666	76.715854
45.119552	27.588175	76.720858
44.026529	31.239746	76.725863
43.569341	27.403408	76.730868
42.999118	33.259769	76.735873
42.478252	30.939588	76.740878
41.337096	31.082209	76.745882
40.728171	33.923281	76.750887
40.326307	23.983159	76.755892
39.804136	34.755134	76.760897
38.987304	35.643971	76.765902
37.894263	35.696918	76.770906
37.543736	33.087793	76.775911
36.990732	31.392485	76.780916
35.682963	34.917462	76.785921
35.256540	32.610604	76.790926
34.673459	27.168499	76.795930
34.303167	43.418280	76.800935
34.006851	30.217505	76.805940
33.273556	40.252024	76.810945
32.178974	35.310975	76.815950
31.702039	34.324207	76.820954
31.276551	39.252310	76.825959
30.700394	34.446193	76.830964
29.256048	41.508010	76.835969
29.042840	31.895766	76.840974
28.475390	29.944143	76.845978
27.485412	34.295226	76.850983
26.886013	36.363648	76.855988
26.231783	40.118705	76.860993
26.010362	31.859229	76.865998
24.673071	34.646170	76.871002
23.750103	37.400143	76.876007
23.674562	22.697587	76.881012
23.053867	41.026317	76.886017
22.784794	18.649590	76.891022
21.686917	27.464917	76.896026
20.471850	41.206452	76.901031
20.284598	28.051365	76.906036
20.008368	28.860286	76.911041
19.475728	26.016861	76.916046
18.634072	35.108293	76.921050
17.716949	37.702062	76.926055
17.505980	28.425358	76.931060
16.347518	32.915284	76.936065
15.382988	37.069924	76.941070
15.285879	27.924871	76.946074
14.530559	34.490432	76.951079
14.099273	31.022132	76.956084
12.967881	35.233350	76.961089
12.485125	37.004047	76.966094
11.910089	31.855557	76.971098
11.345454	38.078466	76.976103
9.891833	31.147801	76.981108
9.426381	36.310939	76.986113
8.897353	34.223881	76.991118
8.867892	32.334682	76.996122
8.026272	31.606366	77.001127
7.524635	34.884497	77.006132
6.686820	34.568738	77.011137
5.864597	34.065988	77.016142
4.796095	33.107356	77.021147
4.057991	37.104456	77.026151
3.998373	26.654007	77.031156
3.260109	40.764195	77.036161