Fri Mar 05 18:54:52 2021

Number of Points = 14577

Depth (nm)	Load (N)	Time (s)
6.788708	95.049116	0.000000
6.433299	75.423707	0.005005
6.037947	39.880512	0.010010
3.957320	8.212736	0.015014
0.202502	-15.293662	0.020019
-5.285207	-14.219542	0.025024
-10.682555	-11.650676	0.030029
-14.908095	-15.319513	0.035034
-19.222283	-0.340870	0.040038
-22.727235	-10.703714	0.045043
-26.355410	-8.019648	0.050048
-30.175677	-5.017925	0.055053
-33.482954	-11.253849	0.060058
-37.423920	1.153192	0.065062
-40.644604	-11.535255	0.070067
-44.199954	-8.769740	0.075072
-48.529128	-6.628245	0.080077
-52.179802	-14.389467	0.085082
-56.382611	-2.451560	0.090086
-59.806872	-9.135563	0.095091
-63.932351	-17.887037	0.100096
-67.731101	-5.196716	0.105101
-71.140250	-14.620707	0.110106
-74.945383	-9.200703	0.115110
-78.674889	-4.849319	0.120115
-82.038112	-9.508752	0.125120
-86.422206	-11.001197	0.130125
-89.794241	-11.869786	0.135130
-93.593532	-10.798354	0.140134
-97.470698	-13.532300	0.145139
-101.181526	-8.193535	0.150144
-104.868715	-6.487111	0.155149
-108.577949	-16.801452	0.160154
-112.583842	-14.760313	0.165158
-116.747894	-8.166491	0.170163
-120.920743	-7.752924	0.175168
-124.376276	-11.344160	0.180173
-127.757227	-9.563565	0.185178
-131.517484	-4.415563	0.190182
-135.307732	3.228824	0.195187
-138.926075	-5.579793	0.200192
-142.618289	0.396310	0.205197
-146.148760	-0.861659	0.210202
-150.101830	-3.256979	0.215206
-154.006928	-0.580572	0.220211
-157.675664	-3.685152	0.225216
-161.949256	2.322256	0.230221
-165.275062	-10.283001	0.235226
-169.265029	-0.238108	0.240230
-172.642513	-6.907331	0.245235
-176.625745	-0.575653	0.250240
-180.563702	1.358563	0.255245
-184.073892	-9.403741	0.260250
-187.736905	2.240076	0.265254
-191.743690	-4.300303	0.270259
-195.232360	-9.057824	0.275264
-199.177877	2.705212	0.280269
-202.893126	-11.738064	0.285274
-206.727301	-0.926346	0.290278
-210.189358	-1.099155	0.295283
-213.748228	-4.610690	0.300288
-218.233645	-3.550979	0.305293
-221.501164	-0.173557	0.310298
-225.441390	-8.785578	0.315302
-229.191930	-4.329686	0.320307
-232.935778	-0.007320	0.325312
-237.273257	-7.983480	0.330317
-240.520062	-2.054674	0.335322
-244.323420	0.626138	0.340326
-248.050485	-5.066235	0.345331
-251.754688	-13.247526	0.350336
-255.576696	0.954349	0.355341
-259.353397	-7.800411	0.360346
-262.940686	-4.393969	0.365350
-266.768711	-3.964230	0.370355
-270.859393	-11.408863	0.375360
-274.628710	-7.312604	0.380365
-278.137566	-6.473325	0.385370
-282.128185	-1.375055	0.390374
-285.702931	-11.117642	0.395379
-289.158146	-2.536185	0.400384
-293.446157	-5.172687	0.405389
-296.746032	-11.464607	0.410394
-300.865200	1.058009	0.415398
-304.325680	-3.924624	0.420403
-307.947699	-16.157518	0.425408
-312.144819	3.078031	0.430413
-315.756344	-14.890329	0.435418
-319.554042	-8.900284	0.440422
-323.162512	-4.132617	0.445427
-326.816303	-12.944730	0.450432
-330.953010	-0.714159	0.455437
-334.859048	-10.679742	0.460442
-338.448998	-8.745639	0.465446
-342.132763	-7.160828	0.470451
-345.967864	-10.979718	0.475456
-349.855502	1.034500	0.480461
-353.075878	-9.225029	0.485466
-356.968768	-6.149703	0.490470
-360.938923	2.283835	0.495475
-364.949951	5.209304	0.500480
-368.503869	-0.721833	0.505485
-372.126109	-6.257277	0.510490
-375.966197	3.719854	0.515494
-379.677686	4.643675	0.520499
-383.349935	-18.078843	0.525504
-387.535380	-3.072853	0.530509
-391.230771	-7.607836	0.535514
-395.060143	-0.732677	0.540518
-398.384887	1.324747	0.545523
-402.263241	-16.826359	0.550528
-406.013337	-4.215860	0.555533
-409.595687	-17.006852	0.560538
-413.682178	0.495462	0.565542
-417.352537	-7.670465	0.570547
-420.804832	-5.671490	0.575552
-424.890414	2.376881	0.580557
-428.537524	-11.047141	0.585562
-432.163860	-10.327648	0.590566
-436.607116	-0.474880	0.595571
-439.996432	-10.806649	0.600576
-444.127599	-4.051954	0.605581
-447.144005	-6.542745	0.610586
-451.029019	2.328345	0.615590
-454.916932	-0.207758	0.620595
-458.471024	-10.789150	0.625600
-462.835688	0.498753	0.630605
-466.088725	-2.758467	0.635610
-470.133715	-3.714584	0.640614
-474.000738	1.037827	0.645619
-477.580388	-6.885447	0.650624
-481.258770	7.183433	0.655629
-484.994101	-0.396424	0.660634
-488.743743	1.585485	0.665638
-492.311465	-1.692401	0.670643
-496.216068	-11.475004	0.675648
-500.617489	-4.003692	0.680653
-504.093192	-14.802532	0.685658
-507.804859	-8.124199	0.690662
-511.219149	-8.524974	0.695667
-514.962221	-10.448600	0.700672
-518.860707	-5.143893	0.705677
-522.383819	-18.281628	0.710682
-526.698582	-15.529729	0.715686
-530.210558	-5.926482	0.720691
-533.750933	-10.861311	0.725696
-537.802338	-5.071679	0.730701
-541.236430	-7.434126	0.735706
-545.316215	-8.632137	0.740710
-549.225787	-7.258520	0.745715
-552.892612	-7.658318	0.750720
-556.998750	-6.431483	0.755725
-560.241010	-11.423356	0.760730
-564.082764	-6.556571	0.765734
-568.012210	-4.910091	0.770739
-571.281143	-14.491336	0.775744
-575.250061	0.645944	0.780749
-579.115613	-6.859334	0.785754
-583.162912	-0.251845	0.790758
-586.876354	-10.810726	0.795763
-590.197702	-15.124449	0.800768
-593.902998	-8.265657	0.805773
-597.786084	-14.137534	0.810778
-601.946060	-7.743827	0.815782
-605.835090	-11.610442	0.820787
-609.070512	-4.260572	0.825792
-612.840294	-11.779514	0.830797
-616.639531	-12.542832	0.835802
-620.518958	-5.753949	0.840806
-624.252891	0.398264	0.845811
-627.874147	-4.502999	0.850816
-631.955109	0.186072	0.855821
-635.583993	-11.236212	0.860826
-639.219143	-15.465031	0.865830
-642.963604	0.089070	0.870835
-646.709140	-9.554685	0.875840
-651.021392	-3.158639	0.880845
-654.385313	-9.187494	0.885850
-657.886976	-13.696233	0.890854
-661.976934	-4.992348	0.895859
-665.333543	-16.762436	0.900864
-669.504977	-14.274457	0.905869
-673.099123	-5.600896	0.910874
-676.718955	-6.919486	0.915878
-680.660609	-14.748314	0.920883
-684.450414	-7.180450	0.925888
-688.536733	-3.952258	0.930893
-692.420470	-10.692768	0.935898
-695.699515	-7.573069	0.940902
-699.363235	-7.660901	0.945907
-702.840369	-8.256359	0.950912
-707.167734	-10.478962	0.955917
-710.920953	-13.031430	0.960922
-714.597741	-7.383377	0.965926
-718.337954	-3.568629	0.970931
-721.877258	-13.413946	0.975936
-725.774093	-3.700037	0.980941
-729.273702	-10.855110	0.985946
-733.237916	-5.375556	0.990950
-737.197539	-9.120281	0.995955
-741.027200	-13.448739	1.000960
-744.824183	-11.954026	1.005965
-748.525451	-6.986403	1.010970
-751.877757	-12.073955	1.015974
-756.061702	-3.580396	1.020979
-759.839110	-5.335717	1.025984
-763.590981	-1.493805	1.030989
-767.191393	-11.252013	1.035994
-771.138166	-3.479154	1.040998
-774.568198	-7.570237	1.046003
-778.318969	-13.325760	1.051008
-782.219679	2.374939	1.056013
-785.622798	-12.634461	1.061018
-789.776046	-14.689200	1.066022
-793.853255	1.817161	1.071027
-797.711229	-9.763776	1.076032
-801.322167	-2.134437	1.081037
-804.693769	-8.996043	1.086042
-807.989367	0.224497	1.091046
-812.135605	-7.688094	1.096051
-815.951854	-5.698181	1.101056
-819.854986	-2.989479	1.106061
-823.781754	-15.745229	1.111066
-827.513124	-9.530045	1.116070
-831.315493	-5.831343	1.121075
-834.935407	-17.481803	1.126080
-838.655946	-10.038318	1.131085
-842.220080	-16.470118	1.136090
-846.162285	-14.601946	1.141094
-850.208406	-2.090136	1.146099
-853.796447	-15.909228	1.151104
-857.270375	-5.280292	1.156109
-860.874769	-12.396329	1.161114
-865.138468	-17.345886	1.166118
-868.773416	-9.676344	1.171123
-872.403729	-12.547820	1.176128
-876.418204	-8.774135	1.181133
-880.096195	-21.128009	1.186138
-884.113045	-6.047260	1.191142
-887.750685	-5.733694	1.196147
-890.826028	-8.660758	1.201152
-894.809732	-10.234641	1.206157
-899.057789	-5.348096	1.211162
-902.520513	-3.729959	1.216166
-906.579956	-2.639296	1.221171
-909.914422	-5.277322	1.226176
-913.619938	-7.529586	1.231181
-917.547077	1.751079	1.236186
-921.435491	-5.839839	1.241190
-925.355698	-1.805180	1.246195
-928.907140	-20.158971	1.251200
-933.130920	-1.388128	1.256205
-936.224000	-19.862510	1.261210
-939.819685	-4.995677	1.266214
-944.071764	0.889796	1.271219
-947.601140	-3.601453	1.276224
-951.804503	-5.045497	1.281229
-955.562506	-12.836978	1.286234
-959.066346	-11.481840	1.291238
-962.850011	-8.216426	1.296243
-966.462809	-6.679851	1.301248
-970.261535	-13.305742	1.306253
-973.950091	-10.471834	1.311258
-977.770373	-4.902938	1.316262
-981.966430	-11.026878	1.321267
-985.486528	-5.971175	1.326272
-989.290471	2.279082	1.331277
-993.137178	-4.033175	1.336282
-996.437385	-2.565470	1.341286
-1000.457015	-2.248983	1.346291
-1003.809954	-3.789521	1.351296
-1007.982053	0.342330	1.356301
-1011.409352	-5.674278	1.361306
-1016.078671	-8.694737	1.366310
-1019.466990	-3.716830	1.371315
-1022.754322	-9.719536	1.376320
-1026.531173	-7.817587	1.381325
-1030.343013	-16.338336	1.386330
-1034.458011	-3.233326	1.391334
-1038.597253	-0.894928	1.396339
-1041.608285	-19.959432	1.401344
-1045.617499	-1.479771	1.406349
-1049.257143	-13.215028	1.411354
-1052.728792	-11.505358	1.416358
-1056.904966	-6.122259	1.421363
-1060.505999	-8.614924	1.426368
-1064.468935	1.783441	1.431373
-1067.931122	-7.772459	1.436378
-1071.709908	-14.369828	1.441382
-1075.771196	-8.490993	1.446387
-1079.328181	-12.113455	1.451392
-1083.361893	-6.079747	1.456397
-1086.781223	-10.105837	1.461402
-1090.505363	-16.740300	1.466406
-1094.396986	-12.736748	1.471411
-1098.388667	-17.098607	1.476416
-1102.156792	-0.584445	1.481421
-1106.011786	-11.201799	1.486426
-1109.275452	-5.680743	1.491430
-1113.305971	-5.497936	1.496435
-1116.619425	-18.378078	1.501440
-1120.769908	-10.868538	1.506445
-1124.615969	-10.942301	1.511450
-1128.300015	-2.096009	1.516454
-1132.473867	-0.157182	1.521459
-1135.559047	-13.504324	1.526464
-1139.485590	-4.617642	1.531469
-1143.008159	-17.364939	1.536474
-1146.837851	-18.004251	1.541478
-1150.907099	-11.110047	1.546483
-1154.782728	-7.775998	1.551488
-1158.864440	-4.830012	1.556493
-1162.353784	-4.787326	1.561498
-1165.638453	-10.470127	1.566502
-1169.574842	-13.363118	1.571507
-1173.159448	-7.823740	1.576512
-1177.499135	-0.409979	1.581517
-1180.972608	-8.979883	1.586522
-1184.595070	-3.016540	1.591526
-1188.562398	-11.895333	1.596531
-1191.877696	-11.678604	1.601536
-1195.706576	-11.321341	1.606541
-1199.741336	-10.342930	1.611546
-1203.288081	-14.465147	1.616550
-1207.648774	-10.310655	1.621555
-1211.467673	-9.699500	1.626560
-1214.905820	-9.314847	1.631565
-1218.643038	-6.332423	1.636570
-1222.251820	-6.037147	1.641574
-1225.977471	-3.155909	1.646579
-1229.983217	-12.928909	1.651584
-1233.639120	-14.021661	1.656589
-1237.504873	-14.505243	1.661594
-1241.014309	-5.172647	1.666598
-1245.003905	-5.726283	1.671603
-1248.454986	-10.011972	1.676608
-1252.398811	-5.075721	1.681613
-1256.081292	-13.760284	1.686618
-1259.848215	-22.540128	1.691622
-1263.911180	-9.924045	1.696627
-1267.549773	-18.670801	1.701632
-1271.707313	-12.549154	1.706637
-1275.187917	-6.404957	1.711642
-1278.366195	-10.158681	1.716646
-1282.100110	-5.688059	1.721651
-1285.869646	-17.879931	1.726656
-1289.964305	-2.366629	1.731661
-1293.785303	-13.131012	1.736666
-1297.741261	-15.750993	1.741670
-1301.629328	-3.874035	1.746675
-1304.888454	-8.619289	1.751680
-1308.829496	-10.123592	1.756685
-1312.625072	-10.943129	1.761690
-1316.163576	-8.120091	1.766694
-1320.309999	-1.782518	1.771699
-1323.779753	-13.716388	1.776704
-1327.886678	-10.712459	1.781709
-1331.622643	-10.685232	1.786714
-1334.953939	-13.509219	1.791718
-1338.852074	-2.952062	1.796723
-1342.698916	-12.583136	1.801728
-1346.335101	-9.337567	1.806733
-1350.138581	-17.217285	1.811738
-1353.933004	-11.804898	1.816742
-1357.954694	-2.259245	1.821747
-1361.319359	-21.790192	1.826752
-1365.210380	-15.900283	1.831757
-1368.844688	-10.858853	1.836762
-1372.755835	-18.040059	1.841766
-1376.853669	-9.321118	1.846771
-1380.108506	-9.082260	1.851776
-1383.892564	-11.910959	1.856781
-1387.768892	-8.934381	1.861786
-1391.295716	-8.423307	1.866790
-1395.238055	3.440414	1.871795
-1399.009564	-6.737206	1.876800
-1403.075068	-10.345549	1.881805
-1406.728708	-14.604868	1.886810
-1410.761489	-6.440325	1.891814
-1414.290152	-5.826421	1.896819
-1417.955316	-18.960429	1.901824
-1421.698763	-5.996282	1.906829
-1425.430309	-2.360011	1.911834
-1429.093184	-2.618715	1.916838
-1432.600387	2.837698	1.921843
-1436.215254	-11.319885	1.926848
-1440.668437	-4.839947	1.931853
-1444.615723	5.884524	1.936858
-1448.035946	-10.071950	1.941862
-1451.923450	-6.677166	1.946867
-1455.217517	-9.890132	1.951872
-1458.943198	3.430774	1.956877
-1463.171070	-8.436666	1.961882
-1467.095777	-0.380794	1.966886
-1470.788462	0.046577	1.971891
-1474.106714	-7.215207	1.976896
-1478.158773	1.736275	1.981901
-1482.032826	-8.964087	1.986906
-1485.900060	-12.750685	1.991910
-1489.310860	6.255142	1.996915
-1493.402470	-4.131861	2.006912
-1494.053262	-6.967566	2.016909
-1491.406126	-4.797201	2.026906
-1489.036381	-3.258200	2.036902
-1486.556950	-12.862050	2.046899
-1485.064834	-7.958282	2.056896
-1483.193842	-10.837834	2.066893
-1480.888088	-7.297521	2.076890
-1479.235773	-4.599934	2.086886
-1477.309008	-5.202092	2.096883
-1475.035632	-6.139230	2.106880
-1473.379271	-9.454931	2.116877
-1471.680774	-4.573149	2.126874
-1469.812899	-8.529037	2.136870
-1467.690805	-2.180345	2.146867
-1466.030028	-3.496217	2.156864
-1463.951168	-4.776407	2.166861
-1462.154953	-7.392915	2.176858
-1460.126567	-8.996598	2.186854
-1458.021752	-9.175672	2.196851
-1456.335766	-14.316636	2.206848
-1454.580671	-8.174428	2.216845
-1452.837009	-10.305671	2.226842
-1450.711733	-1.017463	2.236838
-1448.756300	-15.097381	2.246835
-1446.768281	-10.143520	2.256832
-1445.190308	-10.096115	2.266829
-1443.354551	-9.962092	2.276826
-1441.311060	-9.577120	2.286822
-1439.423052	-14.057261	2.296819
-1437.493802	-7.734504	2.306816
-1435.653182	-12.357055	2.316813
-1434.043254	-4.356843	2.326810
-1431.688211	-2.098583	2.336806
-1430.049282	-3.777250	2.346803
-1428.338216	-1.179031	2.356800
-1425.940389	-9.863438	2.366797
-1424.326823	-12.070145	2.376794
-1422.885492	-10.901896	2.386790
-1420.719560	-6.281235	2.396787
-1418.580615	-5.890999	2.406784
-1416.836505	-12.830195	2.416781
-1414.877198	-8.787499	2.426778
-1413.171701	-5.986272	2.436774
-1411.343440	-5.996287	2.446771
-1409.332119	-8.590354	2.456768
-1407.424290	-13.070486	2.466765
-1405.647538	-15.503835	2.476762
-1403.601330	-13.425049	2.486758
-1401.884138	-12.237796	2.496755
-1400.013707	-17.278777	2.506752
-1397.962736	-16.171804	2.516749
-1396.337610	-10.927690	2.526746
-1394.259908	-7.488144	2.536742
-1392.458763	-12.405922	2.546739
-1390.617590	-4.657437	2.556736
-1388.674098	-4.123775	2.566733
-1386.665560	-10.500548	2.576730
-1384.779364	-8.554021	2.586726
-1382.990550	-14.125083	2.596723
-1381.374902	-8.884177	2.606720
-1379.466594	-13.449627	2.616717
-1377.258830	-12.453001	2.626714
-1375.860244	-9.217345	2.636710
-1373.627518	-6.860496	2.646707
-1371.784763	-15.749670	2.656704
-1369.903957	-16.292276	2.666701
-1367.813201	-13.649009	2.676698
-1366.044621	-10.186790	2.686694
-1364.188834	-16.665405	2.696691
-1362.295153	-12.114787	2.706688
-1360.349802	-12.514560	2.716685
-1358.859694	-13.291454	2.726682
-1356.519192	-8.861308	2.736678
-1354.972722	-11.898809	2.746675
-1353.164157	-16.216164	2.756672
-1351.306007	-7.666677	2.766669
-1349.190315	-8.133183	2.776666
-1347.228501	-12.402437	2.786662
-1345.473099	-15.411798	2.796659
-1343.376302	-7.871562	2.806656
-1341.777301	-10.844832	2.816653
-1339.960864	-8.478152	2.826650
-1337.737586	-4.283431	2.836646
-1335.861057	-9.795871	2.846643
-1334.172826	-8.536035	2.856640
-1332.669464	-10.601881	2.866637
-1330.453793	-13.013855	2.876634
-1328.652535	-6.951564	2.886630
-1326.764235	-8.101653	2.896627
-1324.888617	-5.877066	2.906624
-1322.775659	-11.305761	2.916621
-1321.142076	-14.961924	2.926618
-1319.202894	-6.276956	2.936614
-1317.102979	-12.573562	2.946611
-1315.440331	-8.833818	2.956608
-1313.515295	-7.910295	2.966605
-1311.669848	-12.222472	2.976602
-1309.899571	-11.361016	2.986598
-1307.972385	-13.567318	2.996595
-1306.065224	-15.940940	3.006592
-1304.089621	-10.760750	3.016589
-1302.282939	-2.569294	3.026586
-1300.312246	-6.969407	3.036582
-1298.648882	-8.868209	3.046579
-1296.792825	-13.039968	3.056576
-1294.710966	-10.971525	3.066573
-1292.923012	-8.423405	3.076570
-1291.100148	-12.286687	3.086566
-1288.962761	-11.097130	3.096563
-1287.135882	-8.735236	3.106560
-1285.482529	-15.981922	3.116557
-1283.461511	-10.676350	3.126554
-1281.442351	-13.508407	3.136550
-1279.777014	-13.130660	3.146547
-1278.124281	-13.181949	3.156544
-1275.997212	-19.252337	3.166541
-1274.370285	-18.022120	3.176538
-1272.223077	-16.617804	3.186534
-1270.258812	-16.682632	3.196531
-1268.204951	-14.319158	3.206528
-1266.767850	-16.265408	3.216525
-1264.896656	-12.104266	3.226522
-1262.871536	-17.405166	3.236518
-1260.854066	-12.290059	3.246515
-1258.912849	-11.399079	3.256512
-1257.149895	-12.994843	3.266509
-1255.450135	-15.387336	3.276506
-1253.815215	-2.639908	3.286502
-1251.746549	-11.299892	3.296499
-1249.666360	-9.246930	3.306496
-1247.590490	-7.935383	3.316493
-1245.811205	-8.362167	3.326490
-1244.247234	-11.415030	3.336486
-1242.212287	-7.876919	3.346483
-1240.303951	-9.309620	3.356480
-1238.293639	-2.585967	3.366477
-1236.585635	-7.305569	3.376474
-1234.757393	-7.086492	3.386470
-1232.995296	-0.762059	3.396467
-1230.836816	-4.369533	3.406464
-1229.316877	-10.129565	3.416461
-1227.383572	-9.969928	3.426458
-1225.449326	-12.415715	3.436454
-1223.463284	-10.139241	3.446451
-1221.350994	-5.884010	3.456448
-1219.776442	-7.392753	3.466445
-1217.835837	-14.405891	3.476442
-1216.040615	-7.774115	3.486438
-1214.056920	-9.056222	3.496435
-1212.024542	-10.674540	3.506432
-1210.109590	-5.546136	3.516429
-1208.485228	-8.933906	3.526426
-1206.796937	-5.193445	3.536422
-1204.786920	-5.778700	3.546419
-1202.944029	-3.823512	3.556416
-1200.994164	-4.909141	3.566413
-1198.784113	-11.221694	3.576410
-1197.372065	-4.598059	3.586406
-1195.440143	-2.830796	3.596403
-1193.439035	-10.439391	3.606400
-1191.677686	-3.334801	3.616397
-1189.629084	-4.529379	3.626394
-1187.672032	-8.856165	3.636390
-1185.859690	-7.944501	3.646387
-1184.012182	-10.122164	3.656384
-1181.881076	-11.363095	3.666381
-1180.249066	-8.666773	3.676378
-1178.739660	-8.564003	3.686374
-1176.809118	-5.498602	3.696371
-1174.684740	-8.596881	3.706368
-1172.582316	-7.737939	3.716365
-1170.764045	-4.472987	3.726362
-1169.081371	-8.591645	3.736358
-1167.067763	-2.703719	3.746355
-1165.271066	-5.782718	3.756352
-1163.344803	-4.489788	3.766349
-1161.355739	-8.992202	3.776346
-1159.613738	-9.825063	3.786342
-1157.889721	-7.844502	3.796339
-1155.878889	-7.270891	3.806336
-1154.052865	-8.050875	3.816333
-1152.301589	-4.434135	3.826330
-1150.223478	-0.437051	3.836326
-1148.511771	-8.978262	3.846323
-1146.691140	-8.768951	3.856320
-1144.448572	-10.308735	3.866317
-1142.508087	-10.508599	3.876314
-1140.974640	-4.548564	3.886310
-1139.001393	-4.136294	3.896307
-1137.109040	-8.376898	3.906304
-1135.111636	-5.315842	3.916301
-1133.667358	-9.742125	3.926298
-1131.384065	-12.674737	3.936294
-1129.665862	-4.977400	3.946291
-1127.834898	-9.002911	3.956288
-1126.003942	-9.303660	3.966285
-1124.075723	-12.522090	3.976282
-1121.853347	-7.341739	3.986278
-1120.426383	-6.112578	3.996275
-1118.282283	-8.296588	4.006272
-1116.256199	-15.198586	4.016269
-1114.527278	-8.744013	4.026266
-1112.843943	-6.621119	4.036262
-1111.020174	-7.947028	4.046259
-1108.930880	-13.753863	4.056256
-1106.896372	-9.939241	4.066253
-1104.987479	-15.262472	4.076250
-1103.436455	-15.665262	4.086246
-1101.869059	-17.589627	4.096243
-1099.743308	-12.308534	4.106240
-1097.549286	-18.608957	4.116237
-1095.837226	-13.152732	4.126234
-1093.798889	-17.271391	4.136230
-1092.018744	-8.399716	4.146227
-1090.457299	-15.783157	4.156224
-1088.211311	-17.336066	4.166221
-1086.531388	-11.964693	4.176218
-1084.634129	-13.892868	4.186214
-1082.765693	-14.952740	4.196211
-1080.554137	-17.996985	4.206208
-1078.888034	-19.692387	4.216205
-1077.143589	-12.730266	4.226202
-1075.591018	-14.964876	4.236198
-1073.275515	-5.136710	4.246195
-1071.568726	-7.118092	4.256192
-1069.472849	-7.230646	4.266189
-1067.492469	-6.156294	4.276186
-1065.711749	-11.065833	4.286182
-1063.931161	-8.393193	4.296179
-1062.130334	-8.183805	4.306176
-1059.973471	-6.183986	4.316173
-1058.508215	-14.170973	4.326170
-1056.653021	-11.732895	4.336166
-1054.562494	-14.391439	4.346163
-1052.483451	-15.514976	4.356160
-1050.838513	-12.752733	4.366157
-1048.799054	-7.689893	4.376154
-1047.033466	-12.544892	4.386150
-1045.342110	-10.205335	4.396147
-1043.262115	-13.770086	4.406144
-1041.440426	-9.217147	4.416141
-1039.541043	-6.001379	4.426138
-1037.722335	-5.423777	4.436134
-1035.964372	-3.394867	4.446131
-1033.902360	-5.199354	4.456128
-1032.110282	-10.690164	4.466125
-1030.066334	-8.302780	4.476122
-1027.975805	-5.406525	4.486118
-1026.385372	-1.642378	4.496115
-1024.835445	-12.410807	4.506112
-1022.757888	-5.653497	4.516109
-1020.469230	-8.815812	4.526106
-1019.089918	-10.834778	4.536102
-1017.403697	-7.504371	4.546099
-1015.042146	-11.952558	4.556096
-1013.115896	-9.655283	4.566093
-1011.464860	-4.340807	4.576090
-1009.717494	-8.982865	4.586086
-1007.557281	-9.495657	4.596083
-1005.599430	-14.484009	4.606080
-1004.078922	-13.373947	4.616077
-1001.949927	-8.093277	4.626074
-1000.121043	-12.325204	4.636070
-998.498998	-9.382416	4.646067
-996.624950	-12.142079	4.656064
-994.485900	-13.332005	4.666061
-992.295575	-7.625341	4.676058
-991.044042	-5.472771	4.686054
-988.774561	-14.251504	4.696051
-986.673309	-10.654290	4.706048
-985.215604	-5.935723	4.716045
-983.398376	-10.522618	4.726042
-981.410968	-10.729853	4.736038
-979.214615	-6.467308	4.746035
-977.594624	-4.912082	4.756032
-975.732806	-8.283988	4.766029
-973.945910	-10.819694	4.776026
-972.263459	-8.229182	4.786022
-970.244196	-8.653082	4.796019
-968.245880	-6.698875	4.806016
-966.427797	-7.317969	4.816013
-964.362851	-9.424445	4.826010
-962.680212	-4.478147	4.836006
-960.560821	-9.335982	4.846003
-958.805126	-8.392975	4.856000
-956.918094	-10.341519	4.865997
-955.093523	-13.195870	4.875994
-953.182335	-11.221401	4.885990
-951.427544	-11.208252	4.895987
-949.460217	-12.102253	4.905984
-947.714921	-8.654924	4.915981
-946.013336	-5.120075	4.925978
-944.015458	-12.961646	4.935974
-941.699233	-7.969806	4.945971
-940.195496	-7.264392	4.955968
-938.192997	-12.165094	4.965965
-936.046711	-4.460261	4.975962
-934.509693	-7.507039	4.985958
-932.598596	-12.285751	4.995955
-930.751217	-8.726836	5.005952
-928.995006	-12.852352	5.015949
-926.974719	-13.799014	5.025946
-925.033500	-7.664026	5.035942
-923.188068	-8.344302	5.045939
-921.276257	-5.370423	5.055936
-919.660239	-12.623542	5.065933
-917.631079	-16.985327	5.075930
-915.532195	-15.391369	5.085926
-914.096101	-14.703543	5.095923
-912.047826	-14.797293	5.105920
-909.979097	-16.410112	5.115917
-908.122940	-14.625756	5.125914
-906.339865	-16.080791	5.135910
-904.463371	-18.060767	5.145907
-902.638753	-16.181362	5.155904
-900.549843	-15.042115	5.165901
-899.047941	-10.829509	5.175898
-896.855434	-8.413653	5.185894
-895.260358	-9.219669	5.195891
-893.098367	-13.188985	5.205888
-891.285823	-16.066628	5.215885
-889.463023	-25.863332	5.225882
-887.500284	-17.145419	5.235878
-885.579183	-17.635658	5.245875
-883.932404	-8.287740	5.255872
-882.036778	-15.463960	5.265869
-880.024364	-7.044505	5.275866
-877.889745	-9.618367	5.285862
-876.232197	-11.533316	5.295859
-874.365373	-16.590696	5.305856
-872.535160	-18.864829	5.315853
-870.650900	-19.603377	5.325850
-869.228017	-18.987623	5.335846
-867.149986	-11.581289	5.345843
-864.766996	-13.678528	5.355840
-863.200032	-15.436878	5.365837
-861.350737	-19.403541	5.375834
-859.511572	-21.470672	5.385830
-857.570337	-6.458707	5.395827
-855.636391	-13.470507	5.405824
-853.815844	-20.318910	5.415821
-851.690585	-16.640145	5.425818
-849.887380	-19.205208	5.435814
-848.163100	-21.115015	5.445811
-846.250824	-17.157457	5.455808
-844.451325	-16.444000	5.465805
-842.633371	-20.351954	5.475802
-840.840513	-20.540599	5.485798
-838.741284	-13.893950	5.495795
-836.802121	-17.344431	5.505792
-835.037652	-14.874299	5.515789
-833.252058	-11.254900	5.525786
-831.344258	-11.220332	5.535782
-829.488427	-15.813286	5.545779
-827.453426	-9.704256	5.555776
-825.685572	-14.621041	5.565773
-823.488590	-18.322729	5.575770
-821.864633	-14.900116	5.585766
-820.286745	-14.021739	5.595763
-817.775382	-16.712616	5.605760
-816.125571	-10.644633	5.615757
-814.668493	-15.538573	5.625754
-812.726915	-11.059874	5.635750
-810.788744	-7.510636	5.645747
-808.453780	-10.102253	5.655744
-806.858099	-13.851492	5.665741
-804.971576	-14.113504	5.675738
-803.220960	-20.666479	5.685734
-801.440586	-10.926164	5.695731
-799.385435	-18.727829	5.705728
-797.461203	-19.520077	5.715725
-795.878502	-14.440836	5.725722
-793.609248	-17.677203	5.735718
-791.909619	-14.228769	5.745715
-789.975866	-13.328307	5.755712
-788.193187	-17.846379	5.765709
-786.229327	-19.532330	5.775706
-784.318983	-16.164941	5.785702
-782.751650	-17.005920	5.795699
-780.440600	-18.185252	5.805696
-778.621981	-15.603730	5.815693
-776.947511	-19.141330	5.825690
-775.101759	-18.326265	5.835686
-773.223861	-19.545303	5.845683
-770.921282	-19.903790	5.855680
-769.260887	-24.056508	5.865677
-767.355267	-21.743098	5.875674
-765.564835	-14.219645	5.885670
-763.667387	-19.078151	5.895667
-762.124966	-17.385638	5.905664
-760.120433	-15.051714	5.915661
-758.076343	-21.057875	5.925658
-756.169852	-19.815130	5.935654
-754.066729	-23.119644	5.945651
-752.393299	-12.327975	5.955648
-750.628388	-19.827420	5.965645
-748.751282	-14.400458	5.975642
-747.146100	-16.703267	5.985638
-744.881795	-11.148710	5.995635
-743.043240	-12.239857	6.005632
-741.267671	-16.055699	6.015629
-739.106665	-15.860997	6.025626
-737.310430	-20.220144	6.035622
-735.967894	-17.167759	6.045619
-733.813866	-14.859283	6.055616
-731.803085	-23.784339	6.065613
-730.157622	-16.829800	6.075610
-728.228497	-13.657998	6.085606
-725.917226	-11.243590	6.095603
-724.277084	-19.438348	6.105600
-722.404624	-12.531132	6.115597
-720.539484	-14.134936	6.125594
-718.680000	-14.493612	6.135590
-716.854124	-11.771093	6.145587
-715.157741	-11.701064	6.155584
-712.982326	-10.580209	6.165581
-711.197868	-14.964300	6.175578
-709.485058	-8.975776	6.185574
-707.755695	-12.072099	6.195571
-705.347916	-14.132089	6.205568
-703.185408	-18.990277	6.215565
-701.808735	-20.467057	6.225562
-700.001313	-12.755209	6.235558
-698.172498	-11.632636	6.245555
-696.162671	-18.277491	6.255552
-694.153067	-13.485873	6.265549
-692.473458	-17.021080	6.275546
-690.701380	-20.640536	6.285542
-688.775580	-12.770752	6.295539
-686.603219	-19.859998	6.305536
-684.678209	-16.840661	6.315533
-683.074644	-16.722619	6.325530
-681.321105	-15.392212	6.335526
-679.366366	-13.088155	6.345523
-677.353508	-16.517129	6.355520
-675.621885	-15.022161	6.365517
-673.539424	-15.749594	6.375514
-671.699628	-18.418269	6.385510
-669.906930	-14.780929	6.395507
-668.226005	-16.151570	6.405504
-666.006117	-12.445118	6.415501
-664.249676	-10.249888	6.425498
-662.439441	-12.148036	6.435494
-660.610156	-12.163942	6.445491
-658.693339	-13.343320	6.455488
-656.893668	-12.628167	6.465485
-654.841352	-13.901826	6.475482
-653.086148	-7.147917	6.485478
-651.160896	-11.112353	6.495475
-649.171094	-8.428605	6.505472
-647.379496	-6.338454	6.515469
-645.169620	-13.946826	6.525466
-643.592685	-12.051324	6.535462
-642.163284	-7.703797	6.545459
-640.113457	-9.768108	6.555456
-637.806313	-8.554545	6.565453
-636.008738	-17.739154	6.575450
-634.643004	-12.621969	6.585446
-632.222570	-15.836553	6.595443
-630.527528	-12.060417	6.605440
-628.802498	-14.374404	6.615437
-626.317862	-17.643451	6.625434
-624.828602	-15.247606	6.635430
-623.207874	-15.444900	6.645427
-621.036211	-12.452286	6.655424
-619.361996	-16.215533	6.665421
-617.443968	-17.082436	6.675418
-615.568430	-12.503013	6.685414
-613.565727	-5.196503	6.695411
-611.704692	-14.189129	6.705408
-609.761019	-15.650657	6.715405
-607.874034	-14.731519	6.725402
-605.968776	-15.653216	6.735398
-604.469251	-6.339968	6.745395
-602.609185	-18.585101	6.755392
-600.429465	-12.533720	6.765389
-598.641528	-16.168278	6.775386
-596.668757	-14.727568	6.785382
-594.932346	-18.860738	6.795379
-592.825893	-17.119274	6.805376
-591.026160	-12.661931	6.815373
-589.320674	-16.524892	6.825370
-587.444463	-7.436024	6.835366
-585.486444	-10.423527	6.845363
-583.475218	-11.643191	6.855360
-581.654361	-11.959273	6.865357
-580.037790	-14.878011	6.875354
-577.793960	-14.443758	6.885350
-576.243724	-13.876592	6.895347
-574.469474	-7.334086	6.905344
-572.104121	-12.665100	6.915341
-570.664569	-7.760195	6.925338
-568.535899	-14.504466	6.935334
-566.651929	-13.030596	6.945331
-564.851857	-9.770143	6.955328
-562.963211	-11.612847	6.965325
-560.974118	-15.647412	6.975322
-559.229415	-14.418135	6.985318
-557.343060	-12.666740	6.995315
-555.427889	-10.282045	7.005312
-553.632904	-12.600839	7.015309
-551.548274	-12.433238	7.025306
-550.025114	-17.081793	7.035302
-548.056736	-4.183354	7.045299
-546.177958	-6.689215	7.055296
-544.117695	-8.759849	7.065293
-542.411996	-8.331180	7.075290
-540.414437	-13.655519	7.085286
-538.660037	-9.492474	7.095283
-536.770513	-10.863187	7.105280
-534.526734	-14.144195	7.115277
-532.783973	-11.896153	7.125274
-531.061668	-14.274374	7.135270
-529.227086	-13.379961	7.145267
-527.251735	-14.259107	7.155264
-525.387124	-10.830508	7.165261
-523.782138	-4.979352	7.175258
-521.869455	-7.916931	7.185254
-519.904101	-5.777067	7.195251
-518.080188	-6.922546	7.205248
-515.665211	-9.664033	7.215245
-514.176523	-11.865978	7.225242
-512.262219	-3.520503	7.235238
-510.472861	-5.025199	7.245235
-508.547178	-6.460088	7.255232
-506.718259	-3.884729	7.265229
-504.748668	-7.819820	7.275226
-502.900953	-10.278054	7.285222
-500.998933	-8.895436	7.295219
-499.311077	-3.946457	7.305216
-497.347484	-6.003190	7.315213
-495.416039	-4.810007	7.325210
-493.665156	-7.930145	7.335206
-491.715292	-8.735717	7.345203
-489.545487	-6.993223	7.355200
-487.936352	-6.760673	7.365197
-485.869294	-10.360785	7.375194
-484.209157	-6.163693	7.385190
-482.307742	-9.603133	7.395187
-480.617917	-2.352318	7.405184
-478.160281	-3.496349	7.415181
-476.562749	-13.762080	7.425178
-474.945341	-13.524527	7.435174
-472.736507	-7.765040	7.445171
-470.940362	-12.586624	7.455168
-469.309712	-10.165890	7.465165
-467.437192	-2.710555	7.475162
-465.419237	-10.147597	7.485158
-463.472459	-13.021102	7.495155
-461.820660	-6.831583	7.505152
-459.550467	-8.826724	7.515149
-457.570947	-10.742282	7.525146
-456.105054	-14.312675	7.535142
-454.362638	-8.731316	7.545139
-452.420832	-13.666151	7.555136
-450.218794	-8.107664	7.565133
-448.446421	-7.198516	7.575130
-446.393414	-10.712665	7.585126
-444.800887	-5.431048	7.595123
-443.035590	-8.453978	7.605120
-441.289723	-10.299051	7.615117
-439.021142	-9.314400	7.625114
-437.021982	-10.991496	7.635110
-435.262922	-10.558640	7.645107
-433.606957	-7.680863	7.655104
-431.699201	-8.545978	7.665101
-429.929753	-12.670103	7.675098
-427.605023	-11.564933	7.685094
-426.053402	-11.632635	7.695091
-424.162494	-7.721829	7.705088
-422.190264	-6.397728	7.715085
-420.374678	-16.248240	7.725082
-418.294198	-12.734024	7.735078
-416.465856	-11.069569	7.745075
-414.803444	-6.526995	7.755072
-413.106990	-9.231012	7.765069
-410.759268	-9.283723	7.775066
-409.347277	-10.383869	7.785062
-407.291929	-9.136187	7.795059
-405.253596	-4.211522	7.805056
-403.427633	-10.973639	7.815053
-401.409585	-10.912118	7.825050
-399.794434	-8.315173	7.835046
-398.103931	-4.171814	7.845043
-395.988937	-1.957842	7.855040
-393.896758	-6.968752	7.865037
-392.147394	-11.893340	7.875034
-390.580627	-7.199684	7.885030
-388.455313	-9.361102	7.895027
-386.659438	-4.645604	7.905024
-384.626158	-12.505037	7.915021
-382.796015	-11.628749	7.925018
-381.203765	-8.450230	7.935014
-379.075522	-8.666816	7.945011
-376.803726	-8.465788	7.955008
-375.310970	-9.525125	7.965005
-373.456206	-6.366411	7.975002
-371.894807	-1.818728	7.984998
-369.615754	-3.808885	7.994995
-367.961306	-8.459351	8.004992
-365.736312	-10.916142	8.014989
-363.834670	-10.875477	8.024986
-362.200739	-2.796158	8.034982
-360.425505	-3.194789	8.044979
-358.769326	-2.906504	8.054976
-356.500998	-6.770754	8.064973
-354.321786	-9.741285	8.074970
-352.800410	-5.765103	8.084966
-351.116432	-8.054974	8.094963
-348.937816	-12.451216	8.104960
-347.265260	-8.442325	8.114957
-345.240821	-6.911755	8.124954
-343.575889	-7.284867	8.134950
-341.383138	-10.747030	8.144947
-339.669999	-8.982015	8.154944
-337.669176	-10.892983	8.164941
-335.982577	-10.707435	8.174938
-334.190181	-5.792390	8.184934
-332.237695	-9.449874	8.194931
-330.341411	-10.409395	8.204928
-328.190845	-12.421631	8.214925
-326.534365	-10.745457	8.224922
-324.802752	-7.126510	8.234918
-322.607754	-4.901560	8.244915
-320.888199	-8.793430	8.254912
-319.236600	-13.129194	8.264909
-317.167417	-9.778874	8.274906
-315.237739	-9.286324	8.284902
-313.284532	-6.223804	8.294899
-311.432343	-7.694174	8.304896
-309.695088	-12.323084	8.314893
-307.883548	-6.315268	8.324890
-306.142313	-4.587871	8.334886
-303.953872	-5.505590	8.344883
-302.120141	-3.442424	8.354880
-300.300044	-9.011411	8.364877
-298.317993	-8.672473	8.374874
-296.325575	-6.754638	8.384870
-294.635436	-4.973285	8.394867
-292.923381	-6.804961	8.404864
-290.992402	-4.051510	8.414861
-288.903318	-1.855410	8.424858
-286.866060	-8.537492	8.434854
-285.393149	-8.782015	8.444851
-283.384115	-10.803198	8.454848
-281.591596	-8.687649	8.464845
-279.725065	-11.507147	8.474842
-277.874920	-5.472310	8.484838
-275.990517	-10.653643	8.494835
-274.120179	-6.802587	8.504832
-271.918719	-10.629243	8.514829
-270.320173	-2.642101	8.524826
-268.345307	-10.447911	8.534822
-266.514222	-13.484375	8.544819
-264.519679	-14.058471	8.554816
-262.998283	-8.542734	8.564813
-260.549787	-9.399292	8.574810
-258.992658	-8.675120	8.584807
-257.341781	-9.514884	8.594803
-255.246260	-3.945518	8.604800
-253.361494	-11.654828	8.614797
-251.639018	-11.219154	8.624794
-249.735646	-11.309730	8.634791
-247.665611	-10.067411	8.644787
-245.898975	-6.196621	8.654784
-243.740613	-11.780086	8.664781
-241.974467	-4.623372	8.674778
-240.540807	-6.249520	8.684775
-238.451999	-6.123365	8.694771
-236.373678	-2.381265	8.704768
-234.506498	-8.914579	8.714765
-232.759137	-1.451695	8.724762
-230.916355	-6.678460	8.734759
-229.097788	-10.912919	8.744755
-227.055449	-7.881922	8.754752
-225.420941	-9.197481	8.764749
-223.326406	-8.762749	8.774746
-221.663196	-7.899166	8.784743
-219.351125	-16.557718	8.794739
-217.946395	-12.183875	8.804736
-215.792293	-11.856540	8.814733
-213.606948	-16.913750	8.824730
-212.065159	-8.132759	8.834727
-210.182381	-9.437405	8.844723
-208.408581	-9.500952	8.854720
-206.558101	-6.159837	8.864717
-204.499703	-10.912565	8.874714
-202.689736	-8.963952	8.884711
-200.873303	-13.078049	8.894707
-198.923939	-11.494318	8.904704
-196.879937	-11.512558	8.914701
-195.084877	-16.403251	8.924698
-193.333187	-18.406974	8.934695
-191.565513	-16.244759	8.944691
-189.545028	-17.438732	8.954688
-187.679012	-17.515403	8.964685
-185.890485	-19.716055	8.974682
-183.828716	-15.532315	8.984679
-182.057620	-18.363351	8.994675
-180.266410	-17.115951	9.004672
-178.166615	-13.708812	9.014669
-176.266295	-18.674712	9.024666
-174.763333	-20.675044	9.034663
-172.679641	-18.626406	9.044659
-170.671680	-16.436205	9.054656
-169.203866	-19.330939	9.064653
-167.160609	-26.157565	9.074650
-165.030718	-22.420478	9.084647
-163.318022	-23.922159	9.094643
-161.559359	-21.062157	9.104640
-159.584444	-21.563559	9.114637
-157.459538	-19.952544	9.124634
-155.924990	-21.403686	9.134631
-154.009473	-16.857101	9.144627
-151.960116	-17.777751	9.154624
-150.107173	-19.442333	9.164621
-148.273411	-20.364892	9.174618
-146.578407	-23.093758	9.184615
-144.569040	-21.203765	9.194611
-142.559923	-17.655807	9.204608
-140.786224	-16.198737	9.214605
-139.033430	-17.559956	9.224602
-137.086332	-22.268023	9.234599
-135.150051	-20.407412	9.244595
-133.417811	-15.176289	9.254592
-131.598842	-19.235476	9.264589
-129.263543	-22.489668	9.274586
-127.377278	-22.368993	9.284583
-125.833252	-20.388940	9.294579
-124.152965	-17.653773	9.304576
-122.103695	-17.745423	9.314573
-120.057998	-17.309124	9.324570
-118.255435	-18.433528	9.334567
-116.298318	-16.895179	9.344563
-114.742993	-13.341104	9.354560
-112.956393	-21.003068	9.364557
-110.864145	-25.516377	9.374554
-108.860453	-20.379078	9.384551
-107.025834	-24.207054	9.394547
-105.114011	-22.863578	9.404544
-103.054122	-18.865785	9.414541
-101.413628	-23.242267	9.424538
-99.532389	-17.374882	9.434535
-97.674022	-6.417964	9.444531
-95.798500	-10.310885	9.454528
-93.875985	-16.287653	9.464525
-92.012493	-12.975366	9.474522
-89.973769	-22.245465	9.484519
-88.238480	-18.276395	9.494515
-86.675041	-15.416766	9.504512
-84.629704	-14.844587	9.514509
-82.546500	-13.620016	9.524506
-80.717015	-10.354400	9.534503
-79.100258	-12.892315	9.544499
-77.063146	-10.785632	9.554496
-74.844920	-9.164168	9.564493
-73.184811	-11.892156	9.574490
-71.397426	-16.202056	9.584487
-69.481540	-9.136991	9.594483
-67.728188	-11.156681	9.604480
-65.905738	-11.730000	9.614477
-64.032043	-13.413618	9.624474
-61.529191	-13.343894	9.634471
-60.208009	-13.106170	9.644467
-58.568080	-14.596170	9.654464
-56.386010	-15.719496	9.664461
-54.554797	-18.230028	9.674458
-52.375693	-17.229155	9.684455
-50.804727	-14.031222	9.694451
-48.966348	-13.711791	9.704448
-46.892316	-15.021560	9.714445
-45.056336	-17.153891	9.724442
-43.458986	-15.548612	9.734439
-41.447499	-12.046734	9.744435
-39.174934	-16.584016	9.754432
-37.795217	-12.147647	9.764429
-35.842777	-11.606397	9.774426
-33.655601	-12.499987	9.784423
-31.937782	-13.037641	9.794419
-30.094702	-13.276324	9.804416
-28.168285	-11.393523	9.814413
-26.459402	-9.392333	9.824410
-24.554460	-10.684583	9.834407
-22.713631	-8.592331	9.844403
-20.833324	-10.738033	9.854400
-18.753344	-10.525015	9.864397
-16.947553	-9.530874	9.874394
-15.119594	-1.357501	9.884391
-13.203128	-0.117322	9.894387
-11.547558	6.425632	9.904384
-9.771889	17.411629	9.914381
-7.612421	14.711392	9.924378
-6.293401	26.436572	9.934375
-4.804372	45.979028	9.944371
-2.913525	72.682853	9.954368
-1.432758	106.036529	9.964365
0.000000	135.167701	9.969370
0.914738	157.460598	9.974375
1.419396	180.979601	9.979379
2.179978	192.753469	9.984384
2.297061	204.352447	9.989389
2.942007	201.482006	9.994394
3.012255	211.306472	9.999399
2.969428	203.830566	10.004403
2.880932	189.114149	10.009408
2.779620	197.513574	10.014413
3.048045	188.158730	10.019418
2.645294	192.200157	10.024423
2.571527	194.616857	10.029427
3.070202	188.992689	10.034432
2.995936	193.399617	10.039437
3.355430	186.607032	10.044442
3.040377	193.384722	10.049447
2.918992	200.144138	10.054451
3.520567	196.416431	10.059456
3.332247	203.498767	10.064461
3.291990	200.758127	10.069466
3.005989	211.598225	10.074471
3.158412	207.871197	10.079475
3.400838	195.994171	10.084480
3.221091	207.345605	10.089485
3.294821	205.730093	10.094490
3.195901	220.367689	10.099495
3.357673	214.805137	10.104499
3.875389	211.157037	10.109504
3.446042	219.738114	10.114509
3.674670	209.041284	10.119514
3.664606	219.730137	10.124519
3.563211	219.624922	10.129523
3.902570	219.919342	10.134528
3.467929	213.097300	10.139533
3.996286	215.517306	10.144538
3.762927	221.799421	10.149543
3.942602	217.467213	10.154547
4.149587	221.070757	10.159552
3.780979	220.222830	10.164557
3.629523	223.229103	10.169562
3.756396	247.120719	10.174567
4.253041	242.111880	10.179571
4.536337	250.915196	10.184576
4.561814	262.000542	10.189581
4.657332	239.702530	10.194586
4.311892	237.037374	10.199591
4.180268	233.418729	10.204595
4.370969	227.175032	10.209600
4.117638	237.827007	10.214605
4.594528	252.890037	10.219610
4.746623	261.991838	10.224615
4.471854	255.808185	10.229619
4.656770	259.563496	10.234624
4.613331	269.041852	10.239629
5.041717	261.435556	10.244634
4.767055	255.089457	10.249639
4.731332	246.711936	10.254643
4.889655	243.911226	10.259648
4.168938	256.292027	10.264653
5.188781	267.322843	10.269658
5.183209	272.439521	10.274663
5.305294	266.600999	10.279667
5.159220	257.752209	10.284672
4.902838	266.859245	10.289677
5.557523	271.443238	10.294682
5.072819	252.932645	10.299687
4.912848	256.509575	10.304691
5.263928	266.171008	10.309696
5.279910	274.384607	10.314701
5.479901	268.861671	10.319706
5.264438	280.078506	10.324711
5.572163	280.226583	10.329715
5.621187	275.361676	10.334720
5.407385	296.390286	10.339725
5.585630	281.899315	10.344730
5.827691	284.142646	10.349735
5.631054	277.930751	10.354739
5.830372	282.059094	10.359744
5.727441	284.278606	10.364749
6.102423	284.852781	10.369754
5.725852	286.199712	10.374759
5.739979	282.426915	10.379763
6.045180	277.771885	10.384768
5.636372	292.208243	10.389773
5.814978	290.733692	10.394778
5.947067	291.930098	10.399783
5.771636	286.873904	10.404787
5.833884	290.328661	10.409792
5.552913	300.937782	10.414797
6.184464	287.563548	10.419802
6.065034	304.918501	10.424807
6.535845	310.709851	10.429811
6.460984	302.453662	10.434816
5.848882	306.828142	10.439821
6.387091	314.062729	10.444826
6.282729	319.682473	10.449831
6.377485	320.731868	10.454835
6.376387	325.234400	10.459840
6.352209	332.651748	10.464845
6.528958	324.128323	10.469850
6.558346	323.123860	10.474855
6.657190	326.610637	10.479859
6.967244	325.701756	10.484864
6.728969	327.094442	10.489869
6.864961	331.008967	10.494874
6.760357	329.596935	10.499879
6.877444	332.566702	10.504883
7.283779	330.026044	10.509888
6.882593	331.674957	10.514893
7.101437	332.113187	10.519898
7.358517	336.262294	10.524903
7.323193	340.839679	10.529907
7.238646	337.394853	10.534912
7.259664	337.978182	10.539917
7.258906	334.567301	10.544922
7.664309	335.906199	10.549927
7.363969	336.402013	10.554931
7.641312	335.741207	10.559936
7.177956	339.120540	10.564941
7.514640	339.782830	10.569946
7.629406	352.434153	10.574951
7.271770	359.605075	10.579955
7.672833	362.587900	10.584960
7.880145	379.267119	10.589965
8.250076	373.941759	10.594970
7.939953	370.764726	10.599975
7.881154	364.060861	10.604979
7.648893	345.243367	10.609984
7.963063	371.388803	10.614989
7.949653	369.888101	10.619994
8.346276	370.971353	10.624999
8.016077	371.088720	10.630003
8.257771	370.195472	10.635008
8.074488	373.334590	10.640013
8.377506	381.856500	10.645018
8.141415	381.170356	10.650023
8.052693	380.351891	10.655027
8.253474	378.571010	10.660032
8.329487	380.897615	10.665037
8.559827	383.647472	10.670042
8.342795	376.274172	10.675047
8.443886	380.057868	10.680051
8.628201	373.636138	10.685056
8.596785	378.456557	10.690061
8.865470	378.588784	10.695066
8.850499	383.151897	10.700071
8.905205	385.707413	10.705075
8.883435	382.077515	10.710080
8.548447	385.751783	10.715085
8.930444	386.804251	10.720090
8.861753	382.759202	10.725095
8.663173	397.977439	10.730099
8.843248	389.350941	10.735104
8.590558	391.619591	10.740109
8.676527	386.259883	10.745114
8.947450	385.467631	10.750119
8.523848	386.552406	10.755123
9.023921	391.172141	10.760128
8.924242	413.119455	10.765133
8.855604	404.061097	10.770138
9.378298	410.164343	10.775143
9.088106	416.237980	10.780147
9.466587	409.059052	10.785152
9.181597	425.745099	10.790157
9.257641	420.628244	10.795162
9.390530	419.386484	10.800167
9.648516	427.101082	10.805171
9.580588	430.529327	10.810176
9.841002	453.059527	10.815181
9.868496	445.062905	10.820186
9.872738	432.843621	10.825191
9.579912	435.509777	10.830195
10.092492	438.448020	10.835200
9.965384	448.936508	10.840205
9.894479	439.615129	10.845210
9.888182	442.131499	10.850215
10.216990	448.571628	10.855219
10.298697	445.972342	10.860224
9.949291	435.730261	10.865229
9.961033	451.601004	10.870234
10.488739	455.047789	10.875239
10.270594	459.220695	10.880243
10.427550	456.035373	10.885248
10.363392	458.682404	10.890253
10.222370	455.732277	10.895258
10.107918	455.676453	10.900263
10.228074	460.164417	10.905267
10.381258	457.763469	10.910272
10.341806	466.129527	10.915277
10.558933	461.778657	10.920282
10.669569	454.801709	10.925287
10.434052	463.101265	10.930291
10.670366	453.106377	10.935296
10.398401	458.683520	10.940301
10.405303	463.394562	10.945306
10.793254	477.626737	10.950311
10.945274	483.155183	10.955315
11.090153	490.872086	10.960320
10.776758	495.109084	10.965325
10.780844	494.222190	10.970330
11.062201	492.422135	10.975335
10.806074	491.262923	10.980339
11.288118	496.089002	10.985344
10.818048	502.222908	10.990349
10.839092	500.301942	10.995354
10.790230	499.499190	11.000359
10.849396	518.724634	11.005363
11.428557	518.189149	11.010368
11.255356	527.005524	11.015373
11.555424	533.844530	11.020378
11.606279	524.975202	11.025383
11.564331	533.423701	11.030387
11.777783	535.878225	11.035392
11.483886	537.694558	11.040397
11.576449	530.977510	11.045402
11.821394	533.799186	11.050407
11.405495	544.158759	11.055411
11.867382	540.074766	11.060416
11.521567	549.044849	11.065421
11.798284	541.948324	11.070426
11.879929	536.977197	11.075431
11.832067	539.591680	11.080435
12.101396	549.854572	11.085440
11.855062	557.279084	11.090445
12.306056	553.674662	11.095450
11.973943	560.376390	11.100455
12.305533	558.912105	11.105459
12.658430	551.055916	11.110464
12.445509	563.337051	11.115469
12.276781	560.440210	11.120474
12.377117	567.837816	11.125479
12.248351	564.808437	11.130483
12.725680	563.224706	11.135488
12.092554	566.120216	11.140493
12.674241	560.533132	11.145498
12.149528	570.545788	11.150503
12.244727	578.327435	11.155507
12.432959	563.514456	11.160512
12.267759	565.136791	11.165517
12.509903	579.602068	11.170522
12.504765	582.827937	11.175527
12.726435	599.958514	11.180531
12.949781	605.918774	11.185536
12.868311	599.038635	11.190541
13.043885	603.404257	11.195546
12.653213	611.290233	11.200551
12.472063	609.955041	11.205555
12.934713	599.788325	11.210560
13.156422	613.162441	11.215565
13.082744	630.231350	11.220570
13.430570	638.693435	11.225575
13.223698	640.573172	11.230579
13.624479	635.380787	11.235584
13.325356	638.943735	11.240589
13.432894	641.594953	11.245594
13.540818	632.565062	11.250599
13.436235	640.977881	11.255603
14.031861	632.775410	11.260608
13.654795	637.303315	11.265613
13.430617	640.743917	11.270618
13.707715	646.638847	11.275623
13.514901	644.479149	11.280627
13.726054	644.257841	11.285632
13.538015	648.425998	11.290637
14.041189	644.677606	11.295642
14.075139	642.929613	11.300647
13.890815	648.865028	11.305651
13.814081	639.741579	11.310656
13.695754	646.784579	11.315661
13.518705	645.396687	11.320666
13.936231	654.289231	11.325671
13.877401	677.219225	11.330675
14.330167	670.939845	11.335680
14.292000	683.521229	11.340685
14.343674	680.811568	11.345690
14.452350	684.205395	11.350695
14.384109	694.268332	11.355699
14.514876	685.152759	11.360704
14.647701	682.781832	11.365709
14.594709	689.467483	11.370714
14.840451	687.390797	11.375719
14.470102	689.135759	11.380723
14.794003	683.302729	11.385728
14.446959	699.054344	11.390733
14.278232	688.756454	11.395738
14.538234	688.498966	11.400743
14.283751	693.469406	11.405747
14.758435	687.273260	11.410752
14.507655	687.863686	11.415757
14.406782	700.518168	11.420762
14.905725	710.583690	11.425767
14.754236	721.017912	11.430771
15.001208	709.682244	11.435776
14.756724	720.460899	11.440781
15.043285	713.253906	11.445786
15.217993	710.305406	11.450791
14.976296	729.191168	11.455795
15.036250	733.662010	11.460800
15.116366	744.574997	11.465805
15.238012	745.579131	11.470810
15.330250	752.921350	11.475815
15.427937	755.705055	11.480819
15.575993	748.751961	11.485824
15.516237	755.823520	11.490829
15.645293	752.998995	11.495834
15.808461	753.974428	11.500839
15.876012	755.565966	11.505843
15.644059	749.823150	11.510848
15.856699	752.284149	11.515853
15.813284	761.720242	11.520858
15.956220	755.129105	11.525863
15.657773	756.427343	11.530867
15.803045	757.393015	11.535872
15.731686	763.548590	11.540877
15.801781	764.985173	11.545882
16.373624	778.038648	11.550887
15.994103	788.741117	11.555891
16.269608	790.892456	11.560896
16.138707	792.324831	11.565901
16.221495	784.393324	11.570906
16.464220	791.825106	11.575911
16.236885	786.480531	11.580915
16.321341	780.953753	11.585920
16.274878	791.309768	11.590925
16.294652	788.848041	11.595930
16.795602	781.087969	11.600935
16.434057	790.445508	11.605939
17.166377	785.990286	11.610944
16.789590	786.383182	11.615949
16.559478	788.943197	11.620954
16.508945	790.670276	11.625959
16.370455	798.669100	11.630963
16.634372	788.787858	11.635968
16.567799	812.350118	11.640973
16.775470	821.110649	11.645978
17.106727	821.401646	11.650983
16.789671	834.863481	11.655987
17.008594	829.040830	11.660992
17.039731	838.953966	11.665997
17.049106	831.286472	11.671002
17.157593	834.970542	11.676007
16.985209	833.906759	11.681011
16.954718	823.760199	11.686016
17.200491	832.741754	11.691021
17.050054	837.880161	11.696026
17.302237	848.245353	11.701031
17.462609	854.693607	11.706035
17.668570	854.949395	11.711040
17.645696	866.552302	11.716045
17.547653	861.352667	11.721050
17.723750	862.469557	11.726055
17.602085	869.633053	11.731059
17.839990	858.480077	11.736064
17.618730	862.421768	11.741069
17.548529	865.588687	11.746074
17.830678	862.610403	11.751079
17.493359	863.615210	11.756083
17.607234	852.972486	11.761088
17.926695	860.041957	11.766093
18.137186	859.599965	11.771098
17.703058	863.025219	11.776103
17.602417	882.722940	11.781107
18.341350	879.354804	11.786112
18.362716	886.810904	11.791117
18.240006	894.324684	11.796122
18.587478	893.480771	11.801127
18.267030	897.279010	11.806131
18.415949	889.024641	11.811136
18.384125	895.692816	11.816141
18.367735	892.541358	11.821146
18.701390	894.136200	11.826151
18.367418	906.096288	11.831155
18.704827	895.838951	11.836160
18.870268	893.376049	11.841165
18.316435	894.453244	11.846170
18.553018	893.936121	11.851175
18.356361	901.286647	11.856179
18.638015	887.964526	11.861184
18.731587	906.850659	11.866189
18.570141	916.337220	11.871194
18.845236	926.515875	11.876199
18.769964	933.665694	11.881203
18.987784	927.054649	11.886208
18.940242	935.344991	11.891213
19.027340	933.216299	11.896218
19.177751	927.633211	11.901223
18.951364	936.873083	11.906227
19.279659	928.098037	11.911232
18.892725	936.456708	11.916237
19.208421	941.839366	11.921242
19.511856	949.769359	11.926247
19.609768	965.779893	11.931251
19.861023	955.365934	11.936256
19.831360	937.799084	11.941261
19.619098	934.267247	11.946266
19.671208	935.831304	11.951271
19.319136	945.619544	11.956275
19.383728	934.435804	11.961280
19.378013	959.496265	11.966285
19.540780	954.922092	11.971290
20.003813	954.077090	11.976295
19.542026	971.041137	11.981299
19.616488	967.097678	11.986304
19.644176	966.208568	11.991309
19.713392	975.144252	11.996314
19.923486	970.378009	12.001319
19.930967	966.812691	12.006323
20.205305	969.513062	12.011328
20.005918	976.064490	12.016333
19.783869	970.099217	12.021338
20.054187	976.422748	12.026343
19.737178	970.073625	12.031347
19.965596	963.435640	12.036352
20.035881	971.986349	12.041357
19.792359	977.595424	12.046362
20.078529	966.065634	12.051367
19.701283	959.741895	12.056371
19.878636	941.698865	12.061376
19.528935	946.660922	12.066381
19.485105	970.287624	12.071386
20.060134	963.742596	12.076391
19.639271	972.952006	12.081395
19.797932	963.502203	12.086400
19.979182	971.612558	12.091405
20.174024	976.391566	12.096410
20.012879	961.991904	12.101415
20.199274	952.443061	12.106419
20.071436	943.062626	12.111424
19.747736	949.318459	12.116429
19.565909	946.527714	12.121434
19.978574	935.687449	12.126439
19.461909	942.092337	12.131443
19.721607	936.146437	12.136448
19.862466	937.639563	12.141453
19.520446	942.061039	12.146458
19.716416	936.499067	12.151463
19.836697	944.510315	12.156467
20.258510	943.238197	12.161472
20.074115	944.338473	12.166477
19.989189	946.386468	12.171482
20.412565	941.513670	12.176487
20.012502	943.867415	12.181491
20.037778	942.932956	12.186496
20.385349	943.178774	12.191501
19.506505	937.319856	12.196506
20.128383	932.538409	12.201511
19.478686	928.429753	12.206515
19.523151	928.012664	12.211520
19.978574	942.398549	12.216525
19.970216	950.502864	12.221530
19.945889	944.578609	12.226535
19.846333	936.736033	12.231539
19.699062	925.975627	12.236544
19.927264	938.159905	12.241549
19.717411	935.909834	12.246554
19.679957	927.682017	12.251559
19.492917	946.352746	12.256563
19.987855	947.720005	12.261568
19.871494	948.077673	12.266573
19.767953	954.903982	12.271578
19.997144	955.725385	12.276583
19.791781	947.905989	12.281587
19.762396	945.947274	12.286592
19.700037	939.696327	12.291597
19.807590	948.498137	12.296602
19.943540	947.564950	12.301607
19.739394	950.231245	12.306611
19.800645	933.012624	12.311616
19.828334	941.986453	12.316621
19.830786	936.177786	12.321626
20.037082	930.998972	12.326631
19.500115	925.009828	12.331635
19.697262	937.391460	12.336640
19.947236	946.180014	12.341645
19.725077	946.546672	12.346650
19.919588	945.662495	12.351655
19.861752	951.052695	12.356659
19.721842	931.606232	12.361664
19.332747	925.975150	12.366669
19.697979	940.148322	12.371674
20.136511	944.369596	12.376679
19.876891	963.271136	12.381683
20.143159	949.837864	12.386688
20.086089	938.039548	12.391693
19.807929	934.478795	12.396698
19.371039	926.051324	12.401703
19.484436	930.930045	12.406707
19.920176	941.846384	12.411712
19.815932	952.203844	12.416717
19.941178	961.324561	12.421722
20.013256	946.196961	12.426727
19.565709	940.352831	12.431731
19.822949	959.093069	12.436736
19.868942	948.962608	12.441741
19.752099	947.585585	12.446746
19.900730	934.836611	12.451751
19.708087	947.199995	12.456755
19.807414	943.804548	12.461760
20.031937	943.068559	12.466765
19.613077	930.749176	12.471770
19.788457	930.490990	12.476775
19.829496	940.197598	12.481779
19.833994	937.454411	12.486784
19.733994	932.750260	12.491789
19.752695	933.147889	12.496794
19.980384	937.478491	12.501799
19.534059	942.112159	12.506803
19.847616	940.873080	12.511808
20.072510	953.138328	12.516813
19.841007	947.933139	12.521818
19.833810	927.153398	12.526823
19.728253	934.568263	12.531827
19.729182	926.135615	12.536832
19.809268	929.699651	12.541837
19.630779	942.811455	12.546842
19.628925	939.827990	12.551847
19.882837	954.979364	12.556851
19.974099	956.406281	12.561856
20.225654	939.373355	12.566861
20.108841	933.017548	12.571866
20.086108	923.445307	12.576871
19.893309	937.278528	12.581875
19.762017	928.199872	12.586880
20.055086	929.645063	12.591885
19.894616	924.086331	12.596890
20.082443	932.096260	12.601895
19.901611	932.729157	12.606899
20.118401	932.612610	12.611904
19.957530	932.592574	12.616909
19.727858	943.110394	12.621914
19.992593	938.165123	12.626919
19.625508	939.873321	12.631923
20.134493	937.219987	12.636928
19.834694	938.087918	12.641933
19.801243	942.289852	12.646938
19.910296	925.391644	12.651943
19.735618	932.729217	12.656947
19.795343	920.289347	12.661952
19.942881	927.692225	12.666957
19.579297	924.096212	12.671962
20.039937	925.643992	12.676967
19.532414	924.362406	12.681971
19.768213	926.269348	12.686976
19.888423	934.387841	12.691981
19.615576	944.972477	12.696986
19.986476	936.994931	12.701991
19.699604	947.868831	12.706995
19.828671	935.170289	12.712000
20.161148	932.392135	12.717005
19.894581	927.295056	12.722010
19.848130	912.970195	12.727015
19.846053	921.422022	12.732019
19.635486	915.322467	12.737024
19.817802	913.186476	12.742029
19.475345	913.337340	12.747034
19.951437	919.833041	12.752039
20.044870	921.669644	12.757043
19.819930	908.986589	12.762048
20.031475	909.419694	12.767053
19.971868	911.329595	12.772058
19.793434	905.862051	12.777063
19.384167	917.233299	12.782067
19.448142	909.449815	12.787072
19.930253	921.620388	12.792077
19.919532	925.907007	12.797082
19.779497	917.746024	12.802087
19.863482	916.636611	12.807091
19.558272	920.769916	12.812096
19.643159	928.155977	12.817101
19.756159	937.335406	12.822106
19.951645	944.837884	12.827111
20.084822	948.106431	12.832115
20.045076	928.555680	12.837120
20.211177	912.764945	12.842125
19.913492	919.059196	12.847130
20.112342	912.832832	12.852135
19.891700	915.832934	12.857139
19.621798	917.022546	12.862144
19.629638	914.147935	12.867149
19.915794	916.202972	12.872154
20.026981	921.963618	12.877159
20.014421	917.939430	12.882163
19.991477	914.853672	12.887168
19.908703	916.108059	12.892173
19.730988	921.881670	12.897178
20.160226	911.825731	12.902183
19.997040	919.013222	12.907187
19.892139	915.569927	12.912192
19.814938	918.244355	12.917197
19.788837	916.240962	12.922202
19.904999	910.765852	12.927207
19.685428	926.938955	12.932211
19.863935	928.109087	12.937216
20.127995	921.720920	12.942221
19.818730	913.501772	12.947226
20.043014	899.564276	12.952231
19.773862	897.151770	12.957235
19.503801	892.417983	12.962240
19.737484	891.365124	12.967245
19.581319	913.809514	12.972250
20.207224	909.092091	12.977255
19.477216	905.830515	12.982259
19.773250	911.413430	12.987264
20.041894	922.739633	12.992269
19.662628	921.943825	12.997274
19.897425	911.805353	13.002279
19.482510	904.606071	13.007283
19.442364	914.019662	13.012288
19.717549	919.132788	13.017293
19.853285	923.455973	13.022298
19.971967	926.493423	13.027303
19.729597	926.656710	13.032307
19.846952	925.538819	13.037312
19.860478	926.378851	13.042317
19.645319	932.169478	13.047322
19.918717	916.563488	13.052327
20.035743	924.575244	13.057331
20.177467	921.059491	13.062336
19.785895	915.480851	13.067341
19.416349	917.220980	13.072346
19.751320	916.826944	13.077351
19.712882	922.420633	13.082355
20.011797	921.171274	13.087360
20.040581	923.554390	13.092365
19.642905	922.293132	13.097370
20.081125	920.821266	13.102375
19.792609	923.087825	13.107379
20.247022	906.945158	13.112384
19.896145	906.289912	13.117389
19.795524	907.458830	13.122394
19.614801	901.762979	13.127399
19.508276	900.780156	13.132403
19.349664	907.203616	13.137408
19.820367	914.465047	13.142413
19.809186	931.778247	13.147418
19.945929	929.643214	13.152423
20.205873	929.491396	13.157427
19.989290	916.477395	13.162432
19.957099	913.837843	13.167437
19.706250	913.286498	13.172442
19.897517	904.985938	13.177447
19.857554	907.957220	13.182451
19.893170	908.618673	13.187456
20.070829	907.374463	13.192461
19.524315	904.752291	13.197466
19.653942	902.301409	13.202471
19.978363	904.329839	13.207475
19.920675	907.031116	13.212480
19.861398	897.344866	13.217485
19.667124	907.248269	13.222490
19.946993	902.798946	13.227495
19.742658	905.750711	13.232499
19.623644	907.662203	13.237504
19.881239	904.903884	13.242509
19.911389	906.449361	13.247514
19.851506	907.543968	13.252519
19.959462	909.570654	13.257523
20.111207	900.735470	13.262528
19.993311	908.349422	13.267533
19.955551	909.216557	13.272538
20.187860	900.382717	13.277543
19.791697	904.226152	13.282547
19.782096	911.748710	13.287552
19.933055	906.569269	13.292557
19.677095	907.595797	13.297562
20.014022	912.870971	13.302567
19.992722	909.758142	13.307571
19.753610	907.452814	13.312576
19.870011	910.246180	13.317581
19.606690	915.028857	13.322586
19.860512	906.888641	13.327591
19.713330	916.954862	13.332595
19.400747	917.465261	13.337600
19.539423	908.701548	13.342605
19.680076	912.973481	13.347610
19.592587	910.274936	13.352615
19.764434	910.436811	13.357619
19.456054	918.141079	13.362624
19.803958	912.947569	13.367629
19.473276	918.685650	13.372634
19.722946	908.205740	13.377639
19.837504	912.559111	13.382643
19.510199	916.880454	13.387648
19.864726	911.515566	13.392653
19.747695	921.518629	13.397658
19.693368	916.662108	13.402663
19.774764	915.775474	13.407667
19.816160	906.446922	13.412672
19.646558	912.258661	13.417677
19.842182	918.318095	13.422682
19.960055	928.745773	13.427687
19.786659	920.577493	13.432691
19.684703	916.372009	13.437696
19.804086	915.879888	13.442701
19.574134	924.355448	13.447706
19.937674	932.461938	13.452711
19.928878	942.463522	13.457715
19.616836	943.385449	13.462720
20.081641	927.526550	13.467725
19.699236	930.252817	13.472730
19.960120	913.879220	13.477735
19.758128	919.446954	13.482739
19.636669	920.131886	13.487744
19.828937	921.411793	13.492749
19.760220	928.492749	13.497754
20.297188	922.898470	13.502759
19.834993	924.451514	13.507763
19.972218	924.052748	13.512768
20.210659	921.956692	13.517773
19.954650	920.590830	13.522778
20.053493	922.861838	13.527783
19.953815	922.601792	13.532787
19.991932	924.406215	13.537792
20.090073	921.575550	13.542797
19.954056	922.122445	13.547802
19.935987	919.046948	13.552807
19.650205	920.871494	13.557811
19.688321	921.442657	13.562816
20.054262	913.582617	13.567821
19.762402	930.779727	13.572826
20.139132	915.202991	13.577831
19.672026	908.168160	13.582835
19.737986	917.105905	13.587840
20.039746	916.479031	13.592845
19.810712	911.232458	13.597850
19.638662	888.696992	13.602855
19.833258	904.944366	13.607859
19.606018	910.542934	13.612864
20.200161	914.493356	13.617869
19.622437	908.605344	13.622874
19.965533	899.600858	13.627879
20.018011	896.908376	13.632883
19.747301	891.923941	13.637888
19.726099	892.362630	13.642893
19.821904	896.771030	13.647898
19.724621	883.017315	13.652903
19.651879	883.867950	13.657907
19.934201	885.567180	13.662912
20.131200	883.378385	13.667917
19.636448	902.202226	13.672922
19.511481	884.773652	13.677927
19.996337	887.853618	13.682931
19.351838	896.832129	13.687936
20.063243	904.362687	13.692941
19.860181	904.153827	13.697946
19.811612	895.503573	13.702951
19.840524	895.226170	13.707955
19.665134	893.779638	13.712960
19.922871	892.038500	13.717965
19.523694	900.449569	13.722970
19.938789	913.053476	13.727975
20.027964	916.409464	13.732979
19.690154	900.889944	13.737984
19.872354	897.695768	13.742989
19.618669	894.042807	13.747994
19.965561	903.946626	13.752999
19.831720	906.128582	13.758003
20.082761	898.504512	13.763008
20.019042	891.848499	13.768013
19.839495	896.699814	13.773018
19.873745	899.430583	13.778023
19.916071	897.323232	13.783027
19.737299	903.467613	13.788032
19.735967	894.760935	13.793037
19.728980	903.254538	13.798042
19.859792	897.775519	13.803047
20.021370	897.469069	13.808051
19.629675	898.242839	13.813056
19.678042	888.216128	13.818061
19.627510	898.569714	13.823066
19.856561	895.904265	13.828071
19.795497	888.924533	13.833075
19.813249	899.390238	13.838080
19.782085	900.127002	13.843085
19.872737	906.177943	13.848090
19.921893	903.585345	13.853095
19.767500	897.451605	13.858099
19.695254	902.482939	13.863104
19.785951	888.735507	13.868109
19.481760	906.122224	13.873114
19.696433	885.785000	13.878119
19.663418	904.122005	13.883123
19.935180	915.655876	13.888128
20.027235	903.551508	13.893133
19.478186	899.838418	13.898138
19.806333	903.618363	13.903143
19.809056	902.332667	13.908147
19.624793	900.766116	13.913152
19.799469	912.671886	13.918157
19.962179	919.280656	13.923162
19.826154	917.373650	13.928167
19.834741	905.968614	13.933171
19.578647	899.800629	13.938176
19.835184	913.440721	13.943181
19.880645	921.380306	13.948186
19.894399	909.543907	13.953191
19.751173	908.683639	13.958195
19.628575	906.162595	13.963200
20.020930	916.231069	13.968205
19.572607	923.069934	13.973223
19.837258	922.161016	13.978240
19.785818	926.682301	13.983258
19.979602	927.381319	13.988275
20.286915	931.936618	13.993293
19.914702	919.463649	13.998311
20.103123	903.690702	14.003328
19.713187	893.474739	14.008346
19.499842	899.794649	14.013363
19.937101	912.848766	14.018381
19.670192	928.992973	14.023399
19.771470	930.878659	14.028416
19.865619	933.725035	14.033434
19.752232	932.487877	14.038451
20.209840	942.996748	14.043469
19.910252	941.012209	14.048487
20.213282	929.919618	14.053504
20.046460	939.541794	14.058522
19.911036	944.636482	14.063539
20.145874	931.096108	14.068557
19.712580	936.148643	14.073575
20.019719	940.968243	14.078592
20.179408	941.671127	14.083610
19.903194	941.167807	14.088627
20.256545	933.773264	14.093645
20.065782	939.082845	14.098663
20.362460	952.373355	14.103680
20.724592	957.503516	14.108698
20.346615	946.382683	14.113715
20.709387	944.393167	14.118733
20.343401	942.161240	14.123751
20.261131	936.819782	14.128768
20.176698	942.135999	14.133786
20.137325	944.361875	14.138803
20.421736	939.344176	14.143821
20.278202	945.656116	14.148839
20.445878	951.477968	14.153856
20.745430	951.806183	14.158874
20.367393	950.614383	14.163891
20.414274	948.829410	14.168909
20.679275	952.312360	14.173927
20.492234	960.591254	14.178944
20.388113	957.611260	14.183962
20.511504	962.888043	14.188979
20.624418	963.132770	14.193997
20.288229	976.017729	14.199015
20.546092	969.407617	14.204032
20.749711	968.734950	14.209050
20.138090	967.257933	14.214067
20.451358	972.630276	14.219085
20.438980	973.310271	14.224103
20.566961	970.403366	14.229120
20.474202	969.886513	14.234138
20.684665	967.452521	14.239155
20.758884	967.291283	14.244173
20.625372	976.867272	14.249191
20.661704	970.157213	14.254208
20.817323	985.637904	14.259226
20.951984	989.827500	14.264243
21.131946	989.333213	14.269261
21.007614	982.540236	14.274279
21.198072	971.062871	14.279296
20.939929	978.841878	14.284314
20.868009	972.576953	14.289331
20.790855	964.404767	14.294349
20.764568	975.089948	14.299367
21.190607	978.092608	14.304384
20.933798	974.010668	14.309402
20.768419	978.985876	14.314419
21.073839	987.642416	14.319437
21.073317	999.876098	14.324455
21.123766	1000.063148	14.329472
21.432260	999.144087	14.334490
21.171191	996.598111	14.339507
21.203334	972.868395	14.344525
20.930526	975.809491	14.349543
20.885188	990.763812	14.354560
21.468234	995.703018	14.359578
21.247604	1011.825777	14.364595
21.204330	1011.352940	14.369613
21.562770	1007.322293	14.374631
21.189489	991.541318	14.379648
21.409241	998.404102	14.384666
21.185478	1008.205295	14.389683
21.664496	999.812240	14.394701
21.316329	991.485064	14.399719
21.181519	980.888567	14.404736
21.421153	988.372673	14.409754
21.464122	999.894696	14.414771
21.428884	993.395819	14.419789
21.910606	1003.043579	14.424807
21.351769	978.157549	14.429824
21.322050	979.283907	14.434842
21.021347	993.744129	14.439859
21.499034	988.596482	14.444877
21.474192	1005.701045	14.449895
21.680510	1010.780572	14.454912
21.662387	1000.487924	14.459930
21.370345	1006.743353	14.464947
21.473918	1011.301287	14.469965
21.533584	1003.673552	14.474983
21.337952	1010.209337	14.480000
21.736709	1009.044640	14.485018
21.344411	1012.239188	14.490035
21.648679	1000.506116	14.495053
21.539673	1003.696373	14.500071
21.311510	1009.095317	14.505088
21.880889	1017.527298	14.510106
21.874974	1031.783232	14.515123
22.019212	1030.073957	14.520141
22.030623	1019.307816	14.525159
21.624805	1008.548458	14.530176
21.876214	1012.950676	14.535194
21.571683	1024.600507	14.540211
22.349819	1030.354906	14.545229
22.102271	1026.996648	14.550247
21.958910	1026.895284	14.555264
21.834908	1009.761033	14.560282
21.650391	1021.593068	14.565299
22.188246	1034.744509	14.570317
22.265723	1040.717639	14.575335
22.065227	1028.792921	14.580352
22.147614	1017.486916	14.585370
21.975067	1021.020799	14.590387
22.300417	1017.932963	14.595405
22.181719	1014.898653	14.600423
21.677637	1027.576054	14.605440
22.136049	1030.729293	14.610458
22.149541	1038.947930	14.615475
22.161053	1045.246193	14.620493
22.043547	1039.177277	14.625511
22.320549	1042.930472	14.630528
22.106046	1037.470067	14.635546
21.749468	1052.955449	14.640563
22.260510	1041.549591	14.645581
22.013640	1039.624271	14.650599
22.025183	1042.186538	14.655616
22.225122	1034.794392	14.660634
22.342155	1043.558094	14.665651
22.435862	1064.296436	14.670669
22.508853	1061.077382	14.675687
22.377699	1070.767888	14.680704
22.573715	1074.239849	14.685722
22.657334	1078.285025	14.690739
22.569988	1062.186227	14.695757
22.394716	1055.088304	14.700775
22.260322	1074.606178	14.705792
22.574835	1070.720949	14.710810
22.593467	1072.382305	14.715827
22.741231	1077.630074	14.720845
22.731647	1076.536797	14.725863
22.649376	1084.723543	14.730880
22.791343	1076.617018	14.735898
22.743956	1082.375697	14.740915
22.590581	1080.227815	14.745933
22.768261	1073.355161	14.750951
22.838344	1081.921878	14.755968
22.969184	1067.307841	14.760986
22.830457	1076.172134	14.766003
22.762459	1078.721926	14.771021
23.088830	1071.630498	14.776039
22.969448	1079.470796	14.781056
23.110276	1075.550348	14.786074
22.723859	1063.678852	14.791091
22.681078	1075.986981	14.796109
22.981550	1070.008686	14.801127
22.763203	1078.980063	14.806144
22.898594	1074.689242	14.811162
22.798593	1080.221928	14.816179
22.708564	1075.565934	14.821197
23.022697	1074.718330	14.826215
22.933032	1078.119453	14.831232
22.702800	1070.662195	14.836250
22.673257	1082.590685	14.841267
22.712318	1082.815733	14.846285
22.786331	1092.808589	14.851303
22.979534	1111.612002	14.856320
22.867666	1101.919411	14.861338
22.719393	1117.867148	14.866355
23.280186	1118.410107	14.871373
23.428504	1111.749762	14.876391
23.288785	1112.277038	14.881408
23.324848	1108.436215	14.886426
23.501842	1121.053825	14.891443
23.101570	1106.802895	14.896461
23.723241	1108.580430	14.901479
23.623009	1115.692514	14.906496
23.628224	1115.545427	14.911514
23.127999	1112.531054	14.916531
23.206331	1109.830245	14.921549
23.614332	1106.966739	14.926567
23.605337	1116.049467	14.931584
23.628631	1111.877191	14.936602
23.724258	1105.110421	14.941619
23.280281	1109.113917	14.946637
23.832428	1103.079735	14.951655
23.596899	1113.485355	14.956672
23.616786	1116.935081	14.961690
23.411271	1113.840665	14.966707
23.380300	1124.243552	14.971725
23.671696	1106.193478	14.976743
23.173922	1109.304194	14.981760
23.615897	1115.230226	14.986778
23.910678	1130.177631	14.991795
23.456703	1135.799833	14.996813
23.786607	1140.576542	15.001831
23.830776	1146.591209	15.006848
23.940904	1146.141091	15.011866
23.729558	1140.813853	15.016883
23.808026	1137.906947	15.021901
23.831473	1140.881048	15.026919
23.709169	1151.918308	15.031936
24.116153	1145.680743	15.036954
23.944285	1145.720780	15.041971
24.296670	1141.035097	15.046989
24.357975	1138.305538	15.052007
24.144388	1152.360330	15.057024
23.975598	1145.278633	15.062042
24.018894	1145.237159	15.067059
23.859611	1147.118815	15.072077
24.175614	1138.522017	15.077095
23.997425	1145.679585	15.082112
23.934326	1142.035471	15.087130
24.231217	1135.338833	15.092147
24.102909	1146.863122	15.097165
24.295669	1136.824610	15.102183
24.367744	1133.764565	15.107200
24.278553	1135.218180	15.112218
24.339775	1128.924085	15.117235
24.030573	1135.342758	15.122253
24.074671	1132.856623	15.127271
24.020837	1137.312286	15.132288
24.283139	1135.057193	15.137306
24.446206	1136.800913	15.142323
24.178006	1140.129853	15.147341
24.595504	1133.951964	15.152359
24.428378	1140.335393	15.157376
24.295512	1136.628475	15.162394
24.414781	1144.466922	15.167411
24.468390	1160.777343	15.172429
24.686796	1168.456841	15.177447
24.627859	1174.494258	15.182464
24.688506	1167.843153	15.187482
24.827674	1168.900115	15.192499
24.617533	1161.743206	15.197517
24.565397	1159.937821	15.202535
24.954196	1167.726997	15.207552
24.381293	1161.672465	15.212570
25.100595	1161.892833	15.217587
24.562352	1170.965630	15.222605
24.624077	1171.289313	15.227623
24.721137	1179.571779	15.232640
24.686931	1167.817056	15.237658
25.152504	1172.435279	15.242675
24.986125	1178.916136	15.247693
25.239872	1181.016640	15.252711
25.324846	1178.092958	15.257728
24.681090	1161.316719	15.262746
25.054006	1158.734085	15.267763
24.907440	1175.782756	15.272781
25.220009	1161.323686	15.277799
25.376174	1155.077359	15.282816
25.353743	1137.782034	15.287834
25.594072	1130.694863	15.292851
25.303616	1133.305317	15.297869
25.509561	1132.808455	15.302887
25.072526	1123.825254	15.307904
25.007204	1123.549416	15.312922
25.291522	1118.687404	15.317939
25.249555	1127.300335	15.322957
25.083423	1132.178185	15.327975
25.163545	1134.145925	15.332992
25.190619	1130.396194	15.338010
25.355525	1124.434782	15.343027
24.909482	1134.019824	15.348045
25.372037	1130.911653	15.353063
25.137861	1130.653310	15.358080
25.133729	1144.666819	15.363098
25.634236	1151.701976	15.368115
25.427216	1165.644046	15.373133
25.529500	1163.551328	15.378151
25.626131	1166.332859	15.383168
25.520245	1159.871919	15.388186
25.775050	1143.152153	15.393203
25.174214	1141.287997	15.398221
25.567912	1158.876551	15.403239
25.656460	1154.226655	15.408256
25.415604	1164.088881	15.413274
25.707650	1162.278935	15.418291
25.618596	1163.521741	15.423309
25.757650	1168.442161	15.428327
25.485027	1168.630407	15.433344
25.575821	1171.647256	15.438362
25.747219	1165.689511	15.443379
25.470525	1174.505082	15.448397
25.631721	1170.475965	15.453415
25.864993	1161.783807	15.458432
25.900779	1173.121491	15.463450
25.711991	1168.048628	15.468467
25.778032	1172.902043	15.473485
25.773161	1160.977474	15.478503
25.832042	1163.151532	15.483520
25.836599	1170.150971	15.488538
26.306397	1179.442093	15.493555
26.122945	1176.120769	15.498573
25.999795	1166.299371	15.503591
26.261429	1169.981117	15.508608
26.145105	1169.494757	15.513626
26.249751	1163.824519	15.518643
26.180151	1177.408045	15.523661
26.196196	1165.771153	15.528679
26.527851	1165.444579	15.533696
25.976224	1168.960308	15.538714
26.410438	1169.441660	15.543731
25.904663	1169.901481	15.548749
26.231283	1177.203493	15.553767
26.336913	1190.950995	15.558784
26.298921	1196.001914	15.563802
26.581549	1193.704244	15.568819
26.203398	1198.809421	15.573837
26.426377	1195.874734	15.578855
26.481671	1207.174726	15.583872
26.583174	1201.346094	15.588890
26.381699	1197.044474	15.593907
26.201443	1201.180540	15.598925
26.643457	1197.224603	15.603943
26.724240	1194.502938	15.608960
26.495591	1194.474953	15.613978
26.545846	1194.960919	15.618995
26.602520	1195.559121	15.624013
26.705164	1195.382336	15.629031
26.725603	1178.317658	15.634048
26.532348	1188.619058	15.639066
26.620274	1178.763983	15.644083
26.850876	1186.419524	15.649101
26.298169	1187.879435	15.654119
27.325555	1187.463910	15.659136
26.883816	1190.518513	15.664154
27.062290	1184.910425	15.669171
27.075593	1181.117258	15.674189
27.173802	1183.970901	15.679207
27.260287	1191.059532	15.684224
26.971854	1195.518026	15.689242
27.128497	1183.630599	15.694259
27.197026	1185.946269	15.699277
27.042697	1188.925140	15.704295
27.222963	1183.063503	15.709312
26.819776	1181.822210	15.714330
27.112750	1182.299349	15.719347
27.249051	1184.015883	15.724365
27.388807	1186.645817	15.729383
27.439303	1185.535084	15.734400
27.067239	1178.956139	15.739418
27.181828	1169.290305	15.744435
27.300136	1176.128455	15.749453
27.439217	1183.471395	15.754471
27.338644	1173.877630	15.759488
27.273124	1173.899132	15.764506
27.376857	1184.373387	15.769523
27.310771	1185.252299	15.774541
27.034891	1185.450503	15.779559
27.546551	1187.896844	15.784576
27.446398	1194.886256	15.789594
27.236808	1184.428957	15.794611
27.515515	1195.455771	15.799629
27.360949	1200.023478	15.804647
27.306671	1187.930584	15.809664
27.598761	1188.519552	15.814682
27.613992	1185.495305	15.819699
27.343723	1196.869240	15.824717
27.452076	1190.503105	15.829735
27.704400	1182.467011	15.834752
27.522326	1190.586363	15.839770
27.652040	1192.442379	15.844787
27.871793	1189.479893	15.849805
27.574428	1190.250973	15.854823
28.149970	1191.845536	15.859840
27.759228	1193.882097	15.864858
27.778088	1184.129273	15.869875
27.741403	1194.578741	15.874893
27.705896	1205.702874	15.879911
27.917727	1202.444339	15.884928
27.694356	1211.636828	15.889946
27.684814	1214.167882	15.894963
27.700041	1209.919784	15.899981
27.822453	1209.311971	15.904999
28.118559	1205.047388	15.910016
27.672892	1205.439419	15.915034
27.667193	1203.378078	15.920051
27.981695	1226.587329	15.925069
27.771577	1239.067008	15.930087
28.232613	1238.276190	15.935104
28.181981	1240.338735	15.940122
28.396839	1246.024189	15.945139
28.618065	1237.141994	15.950157
28.351532	1241.622177	15.955175
28.619674	1246.520461	15.960192
28.335275	1247.322511	15.965210
28.637503	1239.932823	15.970227
28.529201	1237.129622	15.975245
27.797415	1239.324410	15.980263
28.219262	1236.414626	15.985280
28.433640	1245.285622	15.990298
28.360354	1242.314809	15.995315
28.490467	1247.258706	16.000333
28.539154	1246.429836	16.005351
28.647457	1246.291474	16.010368
28.444340	1249.391400	16.015386
28.487366	1244.841548	16.020403
28.663558	1252.535690	16.025421
28.218590	1255.554640	16.030439
28.568736	1243.209997	16.035456
28.352845	1247.216476	16.040474
28.443883	1264.626126	16.045491
28.613297	1267.830235	16.050509
28.605420	1278.908330	16.055527
28.720164	1271.469877	16.060544
28.692827	1278.825251	16.065562
28.901130	1272.303922	16.070579
29.052679	1273.058460	16.075597
28.801218	1278.070309	16.080615
28.969279	1271.025272	16.085632
28.741926	1275.179096	16.090650
28.497447	1272.071983	16.095667
28.846704	1273.373877	16.100685
29.051480	1298.027522	16.105703
29.342962	1303.232786	16.110720
29.165970	1308.566259	16.115738
29.270150	1307.295152	16.120755
29.515775	1306.954769	16.125773
29.260895	1310.995799	16.130791
29.304960	1306.102831	16.135808
29.363716	1310.927566	16.140826
29.260727	1308.682733	16.145843
29.472461	1308.033927	16.150861
29.670784	1305.567209	16.155879
30.102400	1289.092790	16.160896
29.816768	1273.308538	16.165914
29.694705	1263.063744	16.170931
29.838369	1257.317244	16.175949
29.777163	1259.411367	16.180967
29.929092	1253.440961	16.185984
29.758716	1263.509882	16.191002
29.747015	1258.242782	16.196019
30.205451	1251.561224	16.201037
29.566687	1243.176430	16.206055
29.451346	1225.206816	16.211072
29.526654	1233.242665	16.216090
29.701832	1247.394418	16.221107
29.997652	1250.948033	16.226125
29.654207	1260.033072	16.231143
29.958325	1253.474445	16.236160
29.589175	1263.377651	16.241178
29.810069	1263.610666	16.246195
30.277856	1258.750018	16.251213
30.075666	1266.593400	16.256231
29.708034	1253.286469	16.261248
29.616235	1253.765207	16.266266
29.824280	1261.166401	16.271283
30.040454	1250.103152	16.276301
29.628263	1263.720954	16.281319
29.765331	1269.197807	16.286336
30.078225	1259.183309	16.291354
29.965468	1264.357079	16.296371
29.960168	1258.000391	16.301389
30.097674	1265.275194	16.306407
30.196094	1257.972277	16.311424
29.899703	1260.949439	16.316442
30.242278	1272.381416	16.321459
30.427485	1283.638723	16.326477
30.489067	1292.792891	16.331495
30.621067	1287.500499	16.336512
30.740808	1277.412974	16.341530
30.311783	1277.174694	16.346547
30.510410	1260.720166	16.351565
30.594647	1258.917399	16.356583
30.211814	1257.570602	16.361600
30.341496	1271.779975	16.366618
30.642057	1281.682554	16.371635
30.671422	1283.072441	16.376653
30.470668	1293.658264	16.381671
30.913045	1294.092700	16.386688
30.910823	1281.843556	16.391706
30.707585	1288.814060	16.396723
30.925393	1285.115666	16.401741
30.516033	1290.750473	16.406759
30.639158	1291.524490	16.411776
30.899519	1282.391413	16.416794
31.007578	1283.854480	16.421811
31.069179	1279.450309	16.426829
30.720621	1282.748051	16.431847
30.955924	1284.521168	16.436864
31.233842	1279.535064	16.441882
30.638023	1289.711977	16.446899
30.963024	1287.184157	16.451917
30.809928	1289.519464	16.456935
30.919397	1287.615138	16.461952
30.930007	1282.983138	16.466970
30.997876	1293.681064	16.471987
31.313282	1286.014749	16.477005
31.265302	1287.747318	16.482023
31.187824	1287.434876	16.487040
31.224388	1275.457198	16.492058
31.380081	1282.235950	16.497075
31.459614	1281.412384	16.502093
31.282345	1288.392117	16.507111
31.232510	1275.717190	16.512128
31.589952	1283.077262	16.517146
31.192038	1286.127253	16.522163
31.428517	1283.659959	16.527181
31.166377	1283.936199	16.532199
30.734578	1292.819840	16.537216
31.518305	1300.023835	16.542234
31.456190	1312.104005	16.547251
31.794529	1317.660462	16.552269
31.485070	1320.752195	16.557287
31.863095	1317.837587	16.562304
31.785104	1312.152376	16.567322
31.373459	1315.096021	16.572339
31.841587	1310.958131	16.577357
31.825539	1317.197199	16.582375
31.652737	1317.408851	16.587392
31.680236	1313.016402	16.592410
31.702930	1320.823943	16.597427
31.925691	1325.613086	16.602445
32.073540	1312.299387	16.607463
31.723000	1319.825101	16.612480
31.916322	1312.640731	16.617498
31.885809	1321.117452	16.622515
31.940030	1326.666532	16.627533
32.017937	1333.226473	16.632551
31.888347	1329.462351	16.637568
32.096955	1333.556093	16.642586
32.131230	1337.348082	16.647603
32.474495	1350.202862	16.652621
32.572636	1343.326252	16.657639
31.961767	1328.326872	16.662656
32.420526	1340.847033	16.667674
31.986335	1341.049253	16.672691
31.976553	1341.484236	16.677709
32.154293	1349.298524	16.682727
32.000727	1357.263191	16.687744
32.131697	1347.383047	16.692762
32.108755	1349.308265	16.697779
32.484366	1348.823661	16.702797
32.497981	1354.398106	16.707815
32.573250	1353.885899	16.712832
32.585599	1345.390112	16.717850
32.325603	1357.173894	16.722867
33.135511	1375.154879	16.727885
32.773142	1363.700100	16.732903
32.533864	1362.541975	16.737920
32.972095	1356.968684	16.742938
32.615256	1360.506086	16.747955
32.806374	1354.202974	16.752973
32.839964	1351.652408	16.757991
33.115250	1369.109876	16.763008
32.933048	1366.340461	16.768026
32.707733	1358.786311	16.773043
32.738849	1364.903041	16.778061
33.334439	1369.366093	16.783079
32.748358	1381.993954	16.788096
33.378785	1373.032251	16.793114
33.171603	1384.741561	16.798131
33.305468	1374.167206	16.803149
32.963186	1365.487290	16.808167
32.910930	1370.007269	16.813184
33.505039	1374.255046	16.818202
33.264909	1378.076657	16.823219
33.669712	1377.646387	16.828237
33.289413	1351.536477	16.833255
33.101540	1353.668907	16.838272
33.264960	1356.124419	16.843290
33.171592	1370.045409	16.848307
33.319310	1368.002834	16.853325
33.381110	1376.829032	16.858343
33.377460	1379.042197	16.863360
33.631321	1371.154411	16.868378
33.243767	1379.408106	16.873395
33.642928	1366.615077	16.878413
33.669722	1371.901912	16.883431
33.265053	1372.876526	16.888448
33.570051	1372.378016	16.893466
33.415829	1376.413233	16.898483
33.521146	1369.734461	16.903501
34.040548	1372.789171	16.908519
33.579017	1375.047054	16.913536
33.826592	1377.914666	16.918554
33.961065	1378.720699	16.923571
33.580613	1386.050650	16.928589
33.893553	1398.118262	16.933607
34.014523	1403.393232	16.938624
34.305300	1393.693641	16.943642
34.480321	1400.713982	16.948659
34.303435	1384.968107	16.953677
34.276264	1378.540134	16.958695
33.932560	1373.239427	16.963712
34.094342	1365.877583	16.968730
33.947113	1367.927238	16.973747
34.035906	1385.055022	16.978765
34.043179	1394.089710	16.983783
33.917354	1412.908219	16.988800
34.132613	1398.319712	16.993818
34.011691	1399.870440	16.998835
34.151778	1404.469867	17.003853
34.554816	1399.337132	17.008871
34.234514	1402.859278	17.013888
34.540714	1400.542086	17.018906
34.591764	1405.976080	17.023923
34.369594	1410.873186	17.028941
34.480979	1402.380446	17.033959
34.305868	1406.084722	17.038976
34.441370	1405.332449	17.043994
34.306924	1416.301844	17.049011
34.699241	1429.875639	17.054029
34.881583	1435.643435	17.059047
34.516591	1435.535730	17.064064
34.941414	1428.147631	17.069082
34.951283	1439.399204	17.074099
34.701001	1437.686739	17.079117
35.205942	1431.909289	17.084135
34.667814	1438.288313	17.089152
34.949278	1429.171442	17.094170
35.130340	1435.648906	17.099187
35.114650	1435.195251	17.104205
35.275476	1430.514862	17.109223
34.908693	1435.578193	17.114240
34.818263	1435.207249	17.119258
34.988312	1436.231777	17.124275
34.885880	1441.744537	17.129293
35.359659	1432.753511	17.134311
35.288567	1439.982233	17.139328
35.168879	1437.200473	17.144346
35.401320	1429.791933	17.149363
35.368759	1441.370399	17.154381
35.591600	1441.128033	17.159399
35.174980	1436.832341	17.164416
35.563224	1429.519291	17.169434
35.564996	1437.048648	17.174451
35.462231	1434.456107	17.179469
35.291506	1424.133227	17.184487
35.199841	1439.162253	17.189504
35.491393	1454.123093	17.194522
35.567620	1468.151626	17.199539
35.591042	1467.477791	17.204557
35.680311	1462.976339	17.209575
35.482779	1467.440079	17.214592
35.802578	1461.742487	17.219610
35.664253	1462.597543	17.224627
35.878307	1459.679173	17.229645
35.948211	1458.688811	17.234663
35.632529	1463.816364	17.239680
36.101646	1468.042419	17.244698
36.084954	1464.185533	17.249715
36.056766	1456.838213	17.254733
35.906981	1466.447006	17.259751
35.847440	1466.014503	17.264768
35.931424	1455.990762	17.269786
36.124973	1460.771238	17.274803
35.616047	1470.868345	17.279821
36.366074	1473.827302	17.284839
36.700371	1485.527408	17.289856
36.393993	1491.314973	17.294874
36.378312	1478.547115	17.299891
36.140361	1464.299043	17.304909
36.366843	1472.071801	17.309927
36.329016	1485.478293	17.314944
36.483192	1483.494449	17.319962
36.691097	1487.434970	17.324979
36.605898	1490.207024	17.329997
36.634447	1485.454903	17.335015
36.533464	1480.161849	17.340032
36.564781	1478.595595	17.345050
36.642653	1476.602686	17.350067
36.738386	1481.988681	17.355085
36.416031	1480.002977	17.360103
36.579627	1483.427509	17.365120
36.984590	1481.538951	17.370138
36.921738	1479.972773	17.375155
36.575269	1489.922067	17.380173
36.695316	1479.377368	17.385191
36.720244	1482.572323	17.390208
36.616402	1485.300157	17.395226
36.747816	1487.055262	17.400243
36.791945	1505.438564	17.405261
37.205818	1504.812567	17.410279
36.841416	1517.330464	17.415296
37.093564	1519.428129	17.420314
37.335226	1511.584687	17.425331
37.045361	1516.949611	17.430349
37.341227	1511.848876	17.435367
37.333435	1515.419522	17.440384
37.103727	1518.199686	17.445402
37.104151	1525.310073	17.450419
37.265716	1524.432508	17.455437
37.475640	1515.476439	17.460455
37.518860	1515.556892	17.465472
37.307062	1519.489642	17.470490
37.516938	1513.065486	17.475507
37.196583	1515.426720	17.480525
37.836672	1516.458870	17.485543
37.893437	1508.316930	17.490560
37.697877	1506.097056	17.495578
37.630422	1509.043258	17.500595
37.783714	1510.861733	17.505613
37.886948	1512.262669	17.510631
37.544057	1514.327821	17.515648
37.606247	1536.096739	17.520666
38.119478	1532.535216	17.525683
38.249817	1527.311433	17.530701
38.453434	1530.371712	17.535719
38.290533	1515.568899	17.540736
37.902219	1504.041852	17.545754
37.891892	1499.152775	17.550771
38.089536	1510.033090	17.555789
38.195511	1508.512343	17.560807
38.019726	1520.610816	17.565824
38.423675	1526.417238	17.570842
38.422468	1518.779279	17.575859
38.035509	1527.339716	17.580877
38.430716	1526.709616	17.585895
38.356347	1524.141632	17.590912
38.319338	1531.386986	17.595930
38.540002	1525.840469	17.600947
38.299082	1529.615837	17.605965
38.638035	1524.427211	17.610983
38.398662	1528.317169	17.616000
38.356509	1524.907942	17.621018
38.671755	1521.200240	17.626035
38.601146	1530.153049	17.631053
38.553244	1528.074796	17.636071
38.724396	1527.434027	17.641088
38.399795	1521.464010	17.646106
38.741513	1523.158046	17.651123
38.446581	1530.045758	17.656141
38.443121	1524.591620	17.661159
38.719775	1547.375606	17.666176
38.560216	1550.878441	17.671194
39.320992	1546.186484	17.676211
38.908328	1566.629552	17.681229
39.088504	1563.387785	17.686247
39.172050	1558.950928	17.691264
39.160718	1555.583185	17.696282
39.310619	1552.701771	17.701299
39.244972	1563.978070	17.706317
39.163128	1561.663755	17.711335
39.185766	1562.178521	17.716352
38.940759	1567.222474	17.721370
39.221330	1560.702861	17.726387
39.195447	1562.161364	17.731405
39.094289	1564.510453	17.736423
39.372207	1565.699479	17.741440
39.348382	1578.801000	17.746458
39.675340	1577.032631	17.751475
39.527541	1591.005774	17.756493
39.962173	1583.541310	17.761511
39.999190	1586.870433	17.766528
39.500836	1569.857368	17.771546
39.868006	1563.742387	17.776563
39.645088	1578.368540	17.781581
39.599700	1579.860832	17.786599
40.225302	1584.408046	17.791616
40.176227	1586.565565	17.796634
40.271495	1568.059326	17.801651
39.691695	1558.823329	17.806669
39.834685	1557.803214	17.811687
40.308770	1569.285241	17.816704
40.165435	1580.185386	17.821722
40.118088	1577.263852	17.826739
40.268955	1583.990817	17.831757
39.985520	1573.453775	17.836775
40.199800	1573.893141	17.841792
40.034743	1573.423192	17.846810
40.302411	1581.536310	17.851827
40.204266	1592.850064	17.856845
40.236302	1581.584688	17.861863
40.711782	1584.805335	17.866880
40.080707	1592.983940	17.871898
40.651193	1587.560937	17.876915
40.588709	1584.202919	17.881933
40.442196	1590.076715	17.886951
40.458295	1588.199042	17.891968
40.504939	1590.473435	17.896986
40.785950	1589.441528	17.902003
40.441689	1587.419974	17.907021
40.577820	1579.573665	17.912039
40.603644	1580.180737	17.917056
40.409351	1578.495506	17.922074
40.711719	1590.616091	17.927091
40.645518	1603.960360	17.932109
40.632589	1614.083065	17.937127
40.864296	1610.262031	17.942144
40.831737	1614.454883	17.947162
40.905354	1613.993271	17.952179
40.856384	1615.991106	17.957197
40.873934	1615.603721	17.962215
41.384584	1606.133203	17.967232
40.860863	1609.095566	17.972250
41.379435	1615.911770	17.977267
41.455577	1619.004199	17.982285
41.429763	1627.739126	17.987303
41.831301	1613.842752	17.992320
41.431527	1617.203008	17.997338
41.492887	1610.711258	18.002355
41.387594	1610.712361	18.007373
41.174953	1604.844008	18.012391
41.214563	1614.086044	18.017408
41.576012	1626.487474	18.022426
41.712020	1617.597404	18.027443
41.754479	1622.523948	18.032461
41.673866	1630.643092	18.037479
41.538595	1630.551442	18.042496
41.676948	1634.101167	18.047514
41.897505	1623.804616	18.052531
41.841100	1634.606776	18.057549
41.520767	1635.688297	18.062567
41.827515	1628.875026	18.067584
41.596077	1631.804146	18.072602
41.996732	1645.078709	18.077619
42.165847	1661.061365	18.082637
41.997585	1666.674377	18.087655
42.396921	1656.117254	18.092672
42.275257	1663.699452	18.097690
42.409133	1658.042451	18.102707
42.345025	1662.064947	18.107725
42.217104	1659.446488	18.112743
42.594295	1652.920862	18.117760
42.291446	1660.721518	18.122778
42.271421	1653.304366	18.127795
42.450095	1658.495504	18.132813
42.466171	1667.723237	18.137831
42.599708	1662.579124	18.142848
42.837126	1653.800280	18.147866
42.890420	1654.609839	18.152883
42.568803	1653.943049	18.157901
42.547278	1661.099477	18.162919
42.929853	1655.027622	18.167936
42.861621	1654.227603	18.172954
42.473176	1651.489455	18.177971
42.780902	1655.499049	18.182989
42.578011	1654.534880	18.188007
43.069095	1648.886980	18.193024
42.504156	1658.937303	18.198042
42.680451	1654.203250	18.203059
43.059062	1663.978806	18.208077
43.169631	1686.256214	18.213095
43.528661	1685.109604	18.218112
43.193717	1684.952269	18.223130
43.213712	1694.392551	18.228147
43.307311	1679.648553	18.233165
43.457227	1689.052379	18.238183
43.321002	1678.103219	18.243200
43.406341	1684.483585	18.248218
43.278949	1687.212853	18.253235
43.618223	1676.638552	18.258253
43.444437	1674.627550	18.263271
43.508411	1677.706988	18.268288
43.239876	1679.025657	18.273306
43.315676	1685.099213	18.278323
43.706397	1671.609588	18.283341
43.624153	1676.047137	18.288359
43.525159	1675.112016	18.293376
43.914197	1702.305860	18.298394
44.024937	1697.262905	18.303411
44.252137	1701.507952	18.308429
44.009572	1692.997561	18.313447
44.506027	1687.830950	18.318464
43.840716	1678.969545	18.323482
43.970326	1685.928837	18.328499
44.375559	1700.887531	18.333517
44.172889	1710.655939	18.338535
44.568032	1699.080072	18.343552
43.961208	1697.547933	18.348570
44.464674	1702.669192	18.353587
44.414253	1700.713233	18.358605
44.417776	1701.898843	18.363623
44.737926	1704.312898	18.368640
44.425237	1708.563829	18.373658
44.485007	1709.403821	18.378675
44.830258	1710.688306	18.383693
44.592824	1703.013205	18.388711
44.555184	1700.142011	18.393728
44.648508	1707.957372	18.398746
44.469603	1701.398504	18.403763
44.571220	1696.648032	18.408781
44.410095	1702.513191	18.413799
44.783903	1702.353716	18.418816
44.808223	1710.161994	18.423834
44.795084	1707.072159	18.428851
44.736911	1703.328798	18.433869
44.709954	1702.724340	18.438887
44.666432	1706.305450	18.443904
44.591513	1720.554974	18.448922
45.061585	1729.533359	18.453939
45.283853	1727.724251	18.458957
44.971137	1736.932892	18.463975
44.843075	1734.525241	18.468992
45.184683	1729.030934	18.474010
44.991363	1733.240809	18.479027
45.331602	1732.281249	18.484045
45.209904	1752.213309	18.489063
45.555345	1759.363954	18.494080
45.844314	1754.902139	18.499098
45.745676	1757.114781	18.504115
46.155608	1758.811339	18.509133
45.600359	1748.009976	18.514151
45.829469	1734.605062	18.519168
45.739430	1729.939420	18.524186
45.800194	1732.964323	18.529203
46.199965	1735.296467	18.534221
45.745296	1735.704100	18.539239
45.983334	1735.834497	18.544256
46.144037	1758.421791	18.549274
46.097697	1749.050245	18.554291
46.309139	1735.353974	18.559309
45.721394	1739.345172	18.564327
46.019075	1742.595787	18.569344
46.196137	1750.237356	18.574362
46.011181	1755.304044	18.579379
46.237873	1760.323954	18.584397
46.231103	1759.884598	18.589415
46.550298	1747.761560	18.594432
46.447728	1746.089209	18.599450
46.483267	1747.972116	18.604467
46.914719	1733.056979	18.609485
46.713794	1748.787274	18.614503
46.621029	1738.410047	18.619520
46.726892	1746.910098	18.624538
46.737158	1746.490836	18.629555
47.000446	1744.039641	18.634573
46.842680	1753.421005	18.639591
46.801628	1743.419370	18.644608
46.531468	1744.729651	18.649626
46.477103	1748.747470	18.654643
46.454643	1743.787883	18.659661
46.623967	1755.774874	18.664679
46.737253	1765.328532	18.669696
47.257674	1770.609144	18.674714
47.053868	1785.782264	18.679731
47.115715	1774.865938	18.684749
47.059454	1786.676562	18.689767
47.218992	1780.278410	18.694784
47.254821	1769.418938	18.699802
47.032357	1783.340462	18.704819
47.168496	1769.340757	18.709837
46.973365	1778.750122	18.714855
46.991977	1775.526212	18.719872
47.526408	1785.413861	18.724890
47.521731	1805.173948	18.729907
47.724601	1798.318962	18.734925
47.701021	1803.666688	18.739943
47.927804	1802.402727	18.744960
47.995148	1805.300745	18.749978
47.720047	1805.483097	18.754995
47.848541	1799.377772	18.760013
48.034713	1811.672028	18.765031
47.992850	1801.667336	18.770048
48.310057	1795.022218	18.775066
48.014951	1803.371523	18.780083
48.076271	1808.015891	18.785101
48.092295	1807.483230	18.790119
48.108608	1797.901872	18.795136
48.307640	1803.012731	18.800154
48.392590	1805.067889	18.805171
48.712013	1803.677460	18.810189
48.660967	1792.824748	18.815207
48.463397	1799.776499	18.820224
48.618169	1784.610478	18.825242
48.745824	1787.157503	18.830259
49.077979	1780.008967	18.835277
48.727765	1770.982409	18.840295
48.744695	1767.846864	18.845312
48.661038	1752.279216	18.850330
48.528627	1755.225601	18.855347
48.603887	1774.421517	18.860365
48.893669	1788.420231	18.865383
48.801062	1796.253497	18.870400
49.138331	1791.197190	18.875418
48.717010	1782.886727	18.880435
48.991218	1790.958806	18.885453
48.995795	1795.469066	18.890471
49.070918	1781.660777	18.895488
49.232379	1783.422925	18.900506
48.955491	1791.230521	18.905523
49.055373	1781.733379	18.910541
49.260541	1783.699355	18.915559
49.128974	1784.135685	18.920576
49.367613	1782.134397	18.925594
49.277561	1788.556942	18.930611
49.369154	1791.617841	18.935629
49.799391	1810.541668	18.940647
49.601370	1805.874347	18.945664
49.964557	1793.534241	18.950682
49.722626	1788.969103	18.955699
49.735342	1767.615828	18.960717
49.753807	1776.916400	18.965735
49.927743	1785.611697	18.970752
49.810005	1781.085745	18.975770
49.834121	1794.124754	18.980787
50.169630	1797.890055	18.985805
50.185897	1811.751506	18.990823
50.039985	1800.707052	18.995840
49.935462	1788.460426	19.000858
49.937589	1805.293408	19.005875
50.128556	1796.794825	19.010893
50.001440	1805.247907	19.015911
49.904688	1805.828132	19.020928
50.177690	1808.351193	19.025946
50.236261	1799.939010	19.030963
50.228166	1801.507966	19.035981
50.066355	1803.481349	19.040999
50.200672	1818.079081	19.046016
50.947258	1830.067664	19.051034
50.626598	1840.222304	19.056051
50.529084	1837.037354	19.061069
50.579649	1833.375723	19.066087
50.653902	1834.417919	19.071104
50.940458	1822.558019	19.076122
50.765264	1826.354442	19.081139
50.905061	1822.810725	19.086157
50.904042	1835.799508	19.091175
50.766233	1833.388674	19.096192
51.012164	1833.874916	19.101210
50.979123	1835.105697	19.106227
50.981482	1830.673840	19.111245
51.047946	1852.130283	19.116263
51.175761	1863.049531	19.121280
51.379703	1861.958321	19.126298
51.289064	1861.887867	19.131315
51.605361	1855.402542	19.136333
51.357907	1859.199486	19.141351
51.645897	1861.159342	19.146368
51.747732	1847.475728	19.151386
51.451608	1857.356674	19.156403
51.834403	1849.760335	19.161421
51.747237	1851.807556	19.166439
51.546729	1848.443174	19.171456
51.885975	1850.243046	19.176474
51.821946	1852.908752	19.181491
51.708616	1855.233086	19.186509
51.761191	1858.367867	19.191527
51.768190	1855.517839	19.196544
52.223500	1854.916685	19.201562
52.056879	1858.023501	19.206579
51.852022	1862.478303	19.211597
52.372952	1874.398301	19.216615
52.234646	1883.810468	19.221632
52.480349	1882.185594	19.226650
52.641733	1882.841063	19.231667
52.481100	1878.104830	19.236685
52.792288	1870.754299	19.241703
52.710911	1866.488382	19.246720
52.424081	1852.442792	19.251738
52.191018	1852.885873	19.256755
52.464629	1866.794427	19.261773
52.509030	1877.394272	19.266791
52.654968	1875.618558	19.271808
52.415425	1878.498679	19.276826
52.777215	1881.820118	19.281843
52.656065	1879.999693	19.286861
52.641170	1875.877337	19.291879
52.687917	1890.304265	19.296896
53.034080	1890.238867	19.301914
53.151178	1898.947230	19.306931
52.824866	1912.736779	19.311949
53.339690	1908.082367	19.316967
53.162229	1909.159210	19.321984
53.153125	1912.254287	19.327002
52.972388	1917.065508	19.332019
53.268204	1913.323839	19.337037
53.739519	1904.473718	19.342055
53.383434	1912.935851	19.347072
53.627186	1909.349576	19.352090
53.289592	1910.707595	19.357107
53.526391	1917.656195	19.362125
53.792038	1936.254054	19.367143
53.671343	1934.972352	19.372160
54.109643	1934.320421	19.377178
53.946348	1927.464783	19.382195
53.995848	1930.339715	19.387213
54.456080	1928.443075	19.392231
54.450449	1925.046807	19.397248
54.544691	1905.648331	19.402266
54.447150	1896.347783	19.407283
54.288478	1886.177605	19.412301
54.467870	1882.924882	19.417319
54.617501	1887.859593	19.422336
54.577068	1887.985640	19.427354
54.547197	1874.569990	19.432371
54.468577	1875.966931	19.437389
54.667216	1879.227869	19.442407
54.576811	1884.949678	19.447424
54.464574	1878.233008	19.452442
54.518212	1877.298700	19.457459
54.340321	1883.946096	19.462477
54.838940	1895.240415	19.467495
54.834298	1897.725971	19.472512
55.140890	1905.958129	19.477530
55.239352	1913.381856	19.482547
55.137467	1910.662450	19.487565
55.193634	1902.206543	19.492583
55.197986	1915.668843	19.497600
55.016715	1899.141256	19.502618
55.366027	1902.926408	19.507635
55.136832	1907.342630	19.512653
55.192001	1910.239465	19.517671
55.300860	1906.831233	19.522688
55.184766	1905.957031	19.527706
55.235265	1907.318436	19.532723
55.312774	1899.742447	19.537741
55.828843	1899.365212	19.542759
55.496876	1910.641781	19.547776
55.567399	1902.577657	19.552794
55.591654	1900.647516	19.557811
55.151785	1909.337743	19.562829
55.695332	1904.231980	19.567847
55.966064	1920.052413	19.572864
55.934133	1929.440564	19.577882
56.066740	1934.337105	19.582899
56.253582	1937.023380	19.587917
56.452253	1924.246899	19.592935
56.049312	1940.951147	19.597952
56.124285	1935.986966	19.602970
56.428960	1927.445002	19.607987
56.205168	1935.974931	19.613005
56.059148	1930.003790	19.618023
56.048472	1923.179658	19.623040
56.310851	1924.593795	19.628058
56.405076	1934.747614	19.633075
56.314014	1934.080218	19.638093
56.593772	1923.925824	19.643111
56.520395	1956.743952	19.648128
56.368032	1959.153184	19.653146
56.736970	1963.963274	19.658163
56.491279	1958.924377	19.663181
56.655320	1960.480840	19.668199
56.598965	1966.278267	19.673216
56.704731	1965.097308	19.678234
56.715637	1967.399484	19.683251
56.844040	1977.436975	19.688269
57.347578	1982.523716	19.693287
57.382721	1983.779817	19.698304
57.101420	1987.175533	19.703322
57.362251	1981.096219	19.708339
57.100358	1993.222974	19.713357
57.179946	1987.417190	19.718375
57.387589	1993.034085	19.723392
57.189352	2009.589349	19.728410
57.391165	2009.277966	19.733427
57.252928	2017.346735	19.738445
57.530981	2011.009811	19.743463
57.368072	2017.093262	19.748480
57.425118	2020.839323	19.753498
58.167718	2029.088535	19.758515
58.134647	2037.742274	19.763533
57.981377	2041.523457	19.768551
57.963995	2043.628006	19.773568
58.177586	2042.695707	19.778586
58.099157	2038.880764	19.783603
58.077421	2041.431211	19.788621
58.249904	2037.582543	19.793639
58.503833	2039.503809	19.798656
58.204522	2033.277839	19.803674
58.687514	2036.287377	19.808691
58.371135	2043.618446	19.813709
58.536027	2030.357221	19.818727
58.502411	2028.765869	19.823744
58.411483	2029.124146	19.828762
58.597836	2037.476238	19.833779
58.600531	2048.530422	19.838797
58.995636	2051.837936	19.843815
59.049868	2066.000339	19.848832
58.987158	2071.582512	19.853850
59.289014	2071.012119	19.858867
58.818043	2072.677739	19.863885
59.182319	2066.108371	19.868903
59.296681	2072.819362	19.873920
59.194430	2068.189381	19.878938
59.232867	2058.303851	19.883955
59.115170	2067.235395	19.888973
59.265909	2065.578453	19.893991
59.428172	2061.224065	19.899008
59.377841	2078.805115	19.904026
59.665865	2059.827024	19.909043
59.133731	2065.586320	19.914061
59.558547	2087.851979	19.919079
60.014976	2094.208736	19.924096
60.149136	2086.917009	19.929114
60.331224	2088.203170	19.934131
60.166875	2095.233140	19.939149
60.086805	2088.981618	19.944167
60.146908	2084.406756	19.949184
59.879695	2092.282973	19.954202
60.076448	2083.650370	19.959219
60.325048	2083.810551	19.964237
60.381723	2081.968032	19.969255
60.447404	2083.704591	19.974272
60.360082	2094.591467	19.979290
60.683832	2082.997581	19.984307
60.615504	2087.249762	19.989325
60.928191	2081.346197	19.994343
60.706474	2075.647427	19.999360
60.958636	2080.253579	20.004378
61.439569	2069.174229	20.009395
60.952966	2068.677674	20.014413
60.869491	2074.964790	20.019431
61.058782	2071.490991	20.024448
60.932970	2075.491978	20.029466
61.090805	2069.237917	20.034483
60.858471	2073.473775	20.039501
61.225352	2064.195011	20.044519
61.233347	2064.756966	20.049536
60.842230	2077.057784	20.054554
61.533820	2069.124981	20.059571
61.070447	2065.417835	20.064589
60.984431	2069.404608	20.069607
61.557975	2092.698999	20.074624
61.224757	2094.778417	20.079642
61.745430	2096.071931	20.084659
61.238036	2103.702505	20.089677
61.424469	2103.327501	20.094695
61.365441	2095.947807	20.099712
61.234324	2115.368228	20.104730
61.542658	2118.522841	20.109747
61.827910	2123.435216	20.114765
61.964150	2125.298179	20.119783
61.924698	2128.855933	20.124800
62.051396	2130.412078	20.129818
62.031675	2128.680060	20.134835
62.264864	2138.662408	20.139853
62.603460	2148.869431	20.144871
62.756467	2157.315009	20.149888
62.520725	2163.019991	20.154906
62.718740	2162.324571	20.159923
62.627313	2159.744248	20.164941
62.546426	2158.418421	20.169959
62.898266	2159.633466	20.174976
62.705480	2167.916317	20.179994
63.063652	2153.387643	20.185011
62.864303	2164.232657	20.190029
63.119629	2167.741833	20.195047
62.975786	2164.612181	20.200064
62.908655	2168.278975	20.205082
63.093064	2161.132581	20.210099
62.887501	2171.551476	20.215117
62.896579	2165.552355	20.220135
63.542030	2163.569513	20.225152
63.250282	2160.629420	20.230170
63.800341	2169.083258	20.235187
63.684587	2176.295083	20.240205
63.455519	2169.423863	20.245223
63.894790	2173.502294	20.250240
63.707408	2184.668702	20.255258
63.879391	2175.435897	20.260275
63.787806	2180.475253	20.265293
63.884827	2186.401690	20.270311
63.713433	2183.185970	20.275328
63.683212	2188.749634	20.280346
63.756449	2180.271180	20.285363
63.893624	2177.028272	20.290381
63.978426	2176.862189	20.295399
64.354792	2191.363484	20.300416
64.276615	2214.225561	20.305434
64.258768	2205.962985	20.310451
64.785307	2203.309266	20.315469
64.806462	2203.615847	20.320487
65.253727	2204.200566	20.325504
65.046557	2185.061383	20.330522
64.859211	2167.874514	20.335539
64.776933	2177.265348	20.340557
64.702568	2175.897576	20.345575
65.014013	2165.739534	20.350592
64.586434	2168.064481	20.355610
64.784525	2179.561125	20.360627
64.620516	2187.298225	20.365645
64.816818	2200.274740	20.370663
64.922088	2188.781690	20.375680
64.730678	2204.819299	20.380698
65.234872	2200.345049	20.385715
65.334879	2223.892944	20.390733
65.136659	2226.872730	20.395751
65.583892	2225.045776	20.400768
65.607616	2225.152154	20.405786
65.450237	2225.303934	20.410803
65.598600	2222.336111	20.415821
65.569832	2228.159133	20.420839
65.849691	2220.340685	20.425856
65.403043	2225.718284	20.430874
65.695402	2239.560493	20.435891
65.720787	2251.913017	20.440909
65.747374	2263.675417	20.445927
66.282614	2253.998411	20.450944
66.316936	2251.580506	20.455962
66.084837	2252.986229	20.460979
66.553029	2262.468666	20.465997
65.989302	2257.001354	20.471015
66.512387	2266.972164	20.476032
66.436538	2281.384422	20.481050
66.783051	2290.686490	20.486067
66.744154	2284.789362	20.491085
66.769884	2288.008750	20.496103
66.742934	2282.464471	20.501120
66.734172	2282.579963	20.506138
66.680611	2276.756758	20.511155
67.020146	2288.019335	20.516173
67.196088	2275.256400	20.521191
67.361301	2268.907472	20.526208
67.288811	2274.538478	20.531226
67.201882	2271.290389	20.536243
67.588268	2270.623916	20.541261
67.228292	2273.852115	20.546279
67.566790	2274.387325	20.551296
67.333332	2270.466472	20.556314
67.451659	2284.714830	20.561331
67.799316	2297.207923	20.566349
67.829306	2297.664909	20.571367
68.226743	2297.481999	20.576384
68.003368	2301.658286	20.581402
68.133323	2290.906909	20.586419
68.000267	2275.116108	20.591437
68.126813	2285.524592	20.596455
68.343235	2282.787387	20.601472
68.067943	2285.655982	20.606490
67.831591	2294.732443	20.611507
68.486326	2287.330847	20.616525
68.250104	2288.825329	20.621543
68.452094	2280.889482	20.626560
68.186171	2290.478008	20.631578
68.371008	2291.305167	20.636595
68.589021	2288.619621	20.641613
68.039725	2295.721307	20.646631
68.645582	2293.482043	20.651648
68.677145	2314.930574	20.656666
68.456508	2324.799794	20.661683
69.250807	2320.018878	20.666701
69.303570	2320.419531	20.671719
69.082964	2314.245387	20.676736
68.812790	2316.739540	20.681754
69.094289	2316.288801	20.686771
69.491791	2313.552600	20.691789
69.161125	2324.037178	20.696807
69.611476	2315.046996	20.701824
69.421190	2318.298483	20.706842
69.425942	2328.697319	20.711859
69.596126	2333.274938	20.716877
69.873469	2341.583590	20.721895
70.048695	2347.136573	20.726912
70.076017	2351.634725	20.731930
69.693099	2344.091821	20.736947
70.019782	2335.469812	20.741965
69.785163	2346.835018	20.746983
70.403819	2337.518287	20.752000
70.266864	2338.704329	20.757018
70.096000	2344.516236	20.762035
70.314326	2348.741653	20.767053
70.138400	2348.688731	20.772071
70.226180	2346.477811	20.777088
70.436051	2345.059971	20.782106
70.226363	2360.480829	20.787123
70.490884	2357.461416	20.792141
70.263450	2370.243727	20.797159
70.691439	2365.612464	20.802176
70.900501	2367.882314	20.807194
70.804041	2370.458107	20.812211
70.820215	2368.471772	20.817229
70.907717	2392.519062	20.822247
71.341623	2388.768624	20.827264
71.092017	2401.922626	20.832282
71.223917	2399.302710	20.837299
71.791416	2394.915844	20.842317
71.419677	2393.803141	20.847335
71.576555	2391.478936	20.852352
71.675722	2392.930950	20.857370
71.544332	2389.374500	20.862387
71.708483	2392.024364	20.867405
71.608853	2393.250866	20.872423
71.720544	2388.031324	20.877440
72.018661	2390.710164	20.882458
71.929888	2402.554002	20.887475
72.102622	2386.048063	20.892493
71.644689	2396.188795	20.897511
71.838667	2411.471386	20.902528
72.204724	2414.560225	20.907546
72.141079	2420.320451	20.912563
72.229953	2420.145064	20.917581
72.162386	2426.924564	20.922599
72.255519	2410.453317	20.927616
72.233272	2418.697311	20.932634
72.437579	2442.940010	20.937651
72.655246	2444.479321	20.942669
72.579148	2456.803368	20.947687
72.585490	2453.719708	20.952704
72.915525	2448.642307	20.957722
72.829160	2448.224277	20.962739
72.738669	2450.367289	20.967757
73.123996	2468.554229	20.972775
73.366530	2474.250700	20.977792
73.111811	2475.460254	20.982810
72.969009	2485.502019	20.987827
73.521848	2475.040180	20.992845
73.612072	2476.510934	20.997863
73.497237	2483.548925	21.002880
73.785798	2478.566228	21.007898
73.447816	2482.893779	21.012915
73.898850	2495.037823	21.017933
73.713643	2499.195492	21.022951
73.704893	2510.366695	21.027968
73.827124	2511.326562	21.032986
73.821734	2512.484555	21.038003
74.079961	2507.940105	21.043021
74.116895	2505.259015	21.048039
74.200217	2512.266990	21.053056
74.668461	2514.331913	21.058074
74.465340	2538.250381	21.063091
74.428278	2536.950567	21.068109
74.576656	2541.357889	21.073127
74.780572	2541.591279	21.078144
74.478491	2538.275186	21.083162
74.476093	2542.282575	21.088179
74.756971	2541.560551	21.093197
74.677706	2535.303988	21.098215
74.907669	2560.052511	21.103232
75.177154	2566.751576	21.108250
75.102011	2576.396388	21.113267
75.151329	2573.408108	21.118285
75.699667	2572.240684	21.123303
76.257133	2543.712067	21.128320
76.388286	2534.848173	21.133338
76.326564	2526.618371	21.138355
76.242735	2514.972731	21.143373
76.394730	2508.980567	21.148391
76.310608	2506.391938	21.153408
76.397900	2495.082434	21.158426
76.370405	2492.821442	21.163443
76.198070	2483.624478	21.168461
76.033661	2475.953051	21.173479
75.833534	2471.953673	21.178496
76.439049	2477.667770	21.183514
76.291446	2493.746691	21.188531
76.455626	2502.514768	21.193549
76.281493	2494.811057	21.198567
76.249164	2492.491841	21.203584
76.509794	2491.695175	21.208602
76.602088	2497.414830	21.213619
76.378316	2494.790267	21.218637
76.733996	2493.933605	21.223655
76.812782	2495.512377	21.228672
76.954365	2497.914933	21.233690
76.859326	2509.405099	21.238707
77.465111	2512.256716	21.243725
77.300970	2514.020541	21.248743
77.370609	2522.076100	21.253760
77.513763	2517.178722	21.258778
77.612586	2513.006585	21.263795
77.717026	2515.089414	21.268813
77.704672	2514.495964	21.273831
77.235005	2511.625863	21.278848
77.801744	2508.429219	21.283866
77.893828	2504.625503	21.288883
77.952931	2505.269784	21.293901
78.109383	2509.752897	21.298919
78.037983	2517.415619	21.303936
77.960700	2509.383386	21.308954
77.920260	2515.662254	21.313971
77.882177	2517.139316	21.318989
78.234912	2528.133318	21.324007
78.195580	2535.194690	21.329024
78.771570	2536.444030	21.334042
78.507664	2542.944187	21.339059
78.517621	2540.536412	21.344077
78.462936	2533.946342	21.349095
78.531320	2542.674660	21.354112
78.624856	2548.976225	21.359130
78.385091	2564.425691	21.364147
78.546943	2571.801888	21.369165
78.851921	2571.491348	21.374183
78.464942	2584.827103	21.379200
78.826629	2592.103005	21.384218
79.099051	2606.668490	21.389235
79.285778	2603.426239	21.394253
79.439933	2600.319761	21.399271
79.017681	2608.036126	21.404288
79.469255	2624.313036	21.409306
79.486002	2639.915966	21.414323
79.529696	2638.067581	21.419341
79.935676	2636.067811	21.424359
79.454061	2646.367453	21.429376
79.883808	2637.886940	21.434394
79.832091	2647.716850	21.439411
79.837622	2664.319016	21.444429
80.439127	2667.523750	21.449447
80.437590	2664.074741	21.454464
80.425096	2662.461072	21.459482
80.642626	2664.228547	21.464499
80.534478	2658.664036	21.469517
80.827348	2663.170277	21.474535
80.826361	2660.118420	21.479552
81.011093	2657.441263	21.484570
80.793862	2654.736965	21.489587
80.759066	2662.305825	21.494605
81.069374	2647.774858	21.499623
81.019288	2657.592716	21.504640
80.934438	2653.641765	21.509658
81.147002	2674.007899	21.514675
81.130105	2686.447768	21.519693
81.274010	2685.339331	21.524711
81.322797	2689.311853	21.529728
81.608081	2686.856998	21.534746
81.610850	2684.266278	21.539763
81.577491	2698.270997	21.544781
81.955528	2694.323301	21.549799
81.672319	2715.296377	21.554816
81.888256	2713.328479	21.559834
81.631922	2716.959509	21.564851
81.872868	2721.395387	21.569869
82.057460	2714.010352	21.574887
82.016135	2725.319066	21.579904
82.310667	2731.004986	21.584922
82.183806	2741.487248	21.589939
82.339202	2750.039769	21.594957
82.853227	2747.996795	21.599975
82.810057	2749.797205	21.604992
82.780595	2741.901168	21.610010
82.864265	2741.006854	21.615027
82.862328	2744.316496	21.620045
83.072478	2737.583411	21.625063
82.768523	2749.382399	21.630080
83.119936	2752.556242	21.635098
83.074809	2761.013318	21.640115
82.941969	2755.944344	21.645133
83.209138	2756.333627	21.650151
83.327895	2772.413638	21.655168
83.574984	2776.159476	21.660186
83.916646	2791.650180	21.665203
83.887796	2796.361161	21.670221
84.063800	2797.071767	21.675239
84.080321	2798.253033	21.680256
84.322754	2794.289966	21.685274
84.151270	2798.551724	21.690291
84.288184	2798.197189	21.695309
84.397395	2790.599164	21.700327
84.275524	2800.901324	21.705344
84.283116	2798.385330	21.710362
84.461892	2796.126006	21.715379
84.452547	2799.584727	21.720397
84.729709	2792.221074	21.725415
84.386780	2792.929485	21.730432
84.588868	2799.646486	21.735450
84.557554	2811.782767	21.740467
84.480190	2817.402172	21.745485
84.947910	2819.087288	21.750503
84.963116	2834.564811	21.755520
85.074572	2819.875026	21.760538
85.111660	2841.574381	21.765555
85.437728	2852.398252	21.770573
85.436682	2844.512574	21.775591
85.476373	2856.116037	21.780608
85.676367	2857.395480	21.785626
85.741636	2853.621910	21.790643
85.724103	2860.874257	21.795661
85.857087	2859.093413	21.800679
85.882904	2852.343263	21.805696
86.071356	2866.188481	21.810714
86.182295	2869.509255	21.815731
85.923505	2892.846425	21.820749
86.338129	2885.162673	21.825767
86.098499	2885.620986	21.830784
86.180580	2877.294109	21.835802
86.385816	2882.937693	21.840819
86.202361	2900.412741	21.845837
86.667139	2901.641308	21.850855
86.844863	2918.209222	21.855872
86.662309	2908.476354	21.860890
86.894186	2909.440788	21.865907
86.787817	2914.706941	21.870925
87.063671	2930.250765	21.875943
87.204408	2936.414390	21.880960
87.310940	2936.568924	21.885978
87.843815	2933.066875	21.890995
87.637140	2940.192100	21.896013
87.708070	2929.075235	21.901031
87.551404	2937.949806	21.906048
87.852169	2932.978384	21.911066
88.167595	2930.405409	21.916083
87.921189	2938.664205	21.921101
87.816242	2930.702229	21.926119
87.993308	2948.268510	21.931136
88.251887	2956.767726	21.936154
88.564359	2956.209771	21.941171
88.436545	2959.513578	21.946189
88.714324	2951.227820	21.951207
88.779432	2950.161822	21.956224
88.738946	2950.353175	21.961242
88.650479	2943.260147	21.966259
88.789411	2949.700172	21.971277
89.266104	2941.503050	21.976295
89.070750	2946.238274	21.981312
88.746480	2950.651876	21.986330
89.108035	2943.405269	21.991347
89.091264	2944.580057	21.996365
89.125977	2953.883508	22.001383
89.222462	2965.572395	22.006400
89.319478	2978.917848	22.011418
89.512812	2974.300222	22.016435
89.337852	2986.279418	22.021453
89.861901	2978.935296	22.026471
89.629714	2975.490745	22.031488
89.631084	2982.401887	22.036506
90.265955	2991.723711	22.041523
89.795043	3006.670090	22.046541
90.231853	3008.456128	22.051559
90.347415	3008.469203	22.056576
90.287236	3002.813529	22.061594
90.398530	3005.601729	22.066611
90.312010	3006.631106	22.071629
90.516186	3005.276258	22.076647
90.769185	3018.544953	22.081664
90.754257	3030.463265	22.086682
90.709162	3033.945048	22.091699
91.007745	3035.982044	22.096717
90.694322	3020.261679	22.101735
90.967662	3039.627475	22.106752
91.161195	3042.094207	22.111770
91.445974	3045.360553	22.116787
91.579068	3060.648815	22.121805
91.966608	3052.190529	22.126823
91.905053	3057.231690	22.131840
92.078192	3061.067273	22.136858
92.232595	3055.146873	22.141875
92.267255	3052.226123	22.146893
92.079162	3047.183165	22.151911
92.255264	3045.300240	22.156928
92.201560	3043.367436	22.161946
92.400610	3051.015625	22.166963
92.217804	3045.344878	22.171981
92.526635	3046.626647	22.176999
92.355038	3049.813956	22.182016
92.397705	3051.989310	22.187034
92.660086	3042.435544	22.192051
92.819272	3044.033806	22.197069
93.156849	3059.599391	22.202087
93.465543	3064.783672	22.207104
93.375281	3065.326724	22.212122
93.483048	3071.002445	22.217139
93.393225	3067.189836	22.222157
93.603429	3070.243889	22.227175
93.569022	3067.375843	22.232192
93.802311	3071.140479	22.237210
93.724608	3056.346109	22.242227
93.692892	3058.014148	22.247245
93.843673	3057.582666	22.252263
93.896445	3057.984911	22.257280
93.658166	3067.450752	22.262298
93.758851	3055.553425	22.267315
93.626089	3066.346793	22.272333
93.726540	3079.415681	22.277351
94.081723	3092.919872	22.282368
94.062424	3101.614522	22.287386
94.254323	3100.412657	22.292403
94.157244	3108.822367	22.297421
94.450262	3116.842630	22.302439
94.749176	3119.622957	22.307456
95.009686	3122.753956	22.312474
95.062636	3114.273477	22.317491
95.076269	3128.446533	22.322509
94.962407	3117.985944	22.327527
95.069268	3125.035298	22.332544
95.407088	3141.471737	22.337562
95.122533	3148.445862	22.342579
95.333626	3155.079782	22.347597
95.153326	3146.837076	22.352615
95.453835	3154.585561	22.357632
95.853405	3167.294530	22.362650
95.898412	3174.539418	22.367667
95.954059	3181.661471	22.372685
95.981483	3172.479414	22.377703
96.331258	3170.805555	22.382720
96.155750	3184.833408	22.387738
96.326335	3179.011855	22.392755
96.668441	3197.573175	22.397773
96.460333	3209.310833	22.402791
96.733503	3193.265460	22.407808
96.609417	3204.446147	22.412826
96.863945	3203.111571	22.417843
96.736229	3202.563236	22.422861
96.639934	3208.552384	22.427879
97.005935	3222.905329	22.432896
97.059659	3232.942222	22.437914
97.284670	3236.952867	22.442931
97.180034	3233.428915	22.447949
97.309901	3237.619142	22.452967
97.461120	3253.759796	22.457984
97.535786	3268.982863	22.463002
97.854432	3260.335638	22.468019
97.886629	3262.380538	22.473037
97.817302	3271.809339	22.478055
97.846154	3265.385759	22.483072
97.898822	3281.944922	22.488090
98.322572	3288.793570	22.493107
98.204648	3294.326014	22.498125
98.276413	3285.642628	22.503143
98.697818	3281.279594	22.508160
98.745551	3296.702860	22.513178
99.093577	3297.689703	22.518195
98.912793	3303.709670	22.523213
99.045297	3319.904514	22.528231
99.340335	3315.035356	22.533248
99.395469	3334.013125	22.538266
99.289107	3317.103833	22.543283
99.508055	3324.153500	22.548301
99.485975	3311.219077	22.553319
99.489261	3317.689549	22.558336
99.495829	3320.418207	22.563354
99.455930	3312.330798	22.568371
99.784142	3315.038053	22.573389
99.413194	3321.222083	22.578407
100.272980	3328.253726	22.583424
100.097315	3338.820502	22.588442
100.277937	3342.411105	22.593459
100.346385	3349.830125	22.598477
100.040158	3353.936535	22.603495
100.187716	3347.325645	22.608512
100.089691	3358.392948	22.613530
100.683536	3367.192143	22.618547
100.783801	3379.320495	22.623565
100.475201	3385.790390	22.628583
101.095931	3374.777451	22.633600
101.168679	3392.911559	22.638618
101.319352	3404.963455	22.643635
101.429036	3397.899178	22.648653
101.580521	3403.798545	22.653671
101.680244	3398.290281	22.658688
101.459535	3408.187769	22.663706
101.820673	3390.550130	22.668723
101.571881	3391.311204	22.673741
101.523327	3407.413088	22.678759
102.356537	3416.582413	22.683776
102.469161	3432.138644	22.688794
102.358946	3440.753595	22.693811
102.378474	3429.999328	22.698829
102.481116	3429.912987	22.703847
102.453869	3428.499036	22.708864
102.570489	3434.308004	22.713882
102.673568	3428.639502	22.718899
102.943023	3430.548257	22.723917
102.888778	3455.272035	22.728935
103.234748	3449.546697	22.733952
103.118564	3456.127535	22.738970
103.146695	3445.875344	22.743987
103.364947	3456.450970	22.749005
103.176285	3453.476076	22.754023
103.326234	3449.400146	22.759040
103.438103	3471.024789	22.764058
103.462074	3480.612697	22.769075
103.648502	3482.796655	22.774093
103.864100	3483.858124	22.779111
103.750669	3494.883147	22.784128
103.711297	3495.840533	22.789146
104.214084	3509.721192	22.794163
104.434082	3516.423083	22.799181
104.531773	3515.227557	22.804199
104.554563	3514.298852	22.809216
104.643723	3511.259975	22.814234
104.714150	3502.148733	22.819251
104.890176	3517.635157	22.824269
104.859821	3533.235536	22.829287
105.070034	3541.227545	22.834304
105.359901	3535.598441	22.839322
105.413008	3540.422456	22.844339
105.580407	3532.062724	22.849357
105.335812	3525.223229	22.854375
105.586248	3532.575559	22.859392
105.781831	3534.430816	22.864410
105.537844	3531.592167	22.869427
105.675927	3538.113613	22.874445
105.581248	3563.797452	22.879463
105.818959	3563.355240	22.884480
105.872157	3572.965293	22.889498
105.798475	3571.756972	22.894515
106.650257	3584.826067	22.899533
106.481656	3592.061174	22.904551
106.981008	3600.086559	22.909568
107.364247	3592.058956	22.914586
107.206167	3588.273616	22.919603
107.127796	3584.323740	22.924621
106.927709	3593.729547	22.929639
106.871517	3593.095058	22.934656
107.042218	3580.965088	22.939674
107.151494	3592.986768	22.944691
107.499876	3603.314403	22.949709
107.638861	3599.858498	22.954727
107.839531	3601.394354	22.959744
107.837787	3611.794350	22.964762
107.610558	3602.019370	22.969779
107.809130	3596.890173	22.974797
107.488144	3623.332361	22.979815
108.010694	3622.059633	22.984832
108.222168	3620.764141	22.989850
108.141836	3637.015303	22.994867
108.486447	3653.060265	22.999885
108.605976	3664.316517	23.004903
108.732716	3664.647197	23.009920
108.987852	3664.886603	23.014938
109.043957	3670.093289	23.019955
109.100787	3653.280305	23.024973
109.181611	3670.261003	23.029991
109.650389	3665.552824	23.035008
109.565824	3669.755344	23.040026
109.521937	3676.321604	23.045043
109.912148	3690.969296	23.050061
109.591277	3696.308482	23.055079
109.979010	3692.558793	23.060096
110.314873	3698.481584	23.065114
110.293920	3704.757852	23.070131
110.286090	3696.072757	23.075149
110.022441	3693.475572	23.080167
110.231446	3699.619193	23.085184
110.413389	3693.845186	23.090202
110.474069	3698.275499	23.095219
110.552987	3716.914850	23.100237
110.695625	3728.850295	23.105255
110.855071	3726.397247	23.110272
110.689392	3719.351555	23.115290
110.652980	3719.513161	23.120307
111.346224	3724.235155	23.125325
111.464541	3732.407911	23.130343
111.325688	3752.405213	23.135360
111.596157	3744.189405	23.140378
111.955287	3756.711031	23.145395
112.031952	3746.767918	23.150413
112.135736	3757.270763	23.155431
111.817587	3749.862328	23.160448
112.043703	3741.161139	23.165466
111.971766	3745.918630	23.170483
112.257732	3764.684718	23.175501
112.360860	3777.413174	23.180519
112.064789	3787.011411	23.185536
112.502581	3783.732014	23.190554
112.356317	3786.648758	23.195571
112.746411	3794.103244	23.200589
112.582140	3815.687470	23.205607
112.529101	3811.502997	23.210624
112.981476	3820.589352	23.215642
112.809536	3839.024994	23.220659
113.400444	3840.054960	23.225677
113.405502	3840.150167	23.230695
113.301080	3844.896349	23.235712
114.038334	3851.880139	23.240730
113.890343	3858.641657	23.245747
114.260772	3858.975962	23.250765
114.179087	3869.887642	23.255783
114.463705	3864.857911	23.260800
114.575719	3854.278175	23.265818
114.257775	3860.088958	23.270835
114.690537	3858.286151	23.275853
114.424311	3865.734415	23.280871
114.774892	3880.143960	23.285888
115.031696	3884.028567	23.290906
115.071238	3897.103964	23.295923
114.973516	3888.005925	23.300941
115.138562	3891.844592	23.305959
115.024130	3890.833118	23.310976
115.693970	3901.513269	23.315994
115.394758	3917.090848	23.321011
115.944341	3915.521142	23.326029
115.826578	3913.402554	23.331047
115.465785	3921.363108	23.336064
115.974283	3920.506392	23.341082
116.256877	3932.086918	23.346099
116.481691	3929.060937	23.351117
116.755154	3929.864622	23.356135
116.859339	3936.073832	23.361152
117.198165	3930.149634	23.366170
117.072276	3936.649632	23.371187
117.063025	3925.193153	23.376205
117.154915	3924.186536	23.381223
117.246518	3937.151399	23.386240
117.437525	3926.275023	23.391258
117.134365	3930.598224	23.396275
117.720807	3919.960879	23.401293
117.338311	3932.489213	23.406311
117.424093	3928.429678	23.411328
117.736055	3918.902841	23.416346
117.426937	3934.714089	23.421363
117.605660	3944.910113	23.426381
117.767012	3953.120184	23.431399
117.964724	3953.007666	23.436416
117.973800	3965.476732	23.441434
118.098141	3984.224035	23.446451
118.406137	3975.787350	23.451469
118.239461	3983.775982	23.456487
118.173399	3995.627709	23.461504
118.467858	4004.008533	23.466522
118.352077	4017.344812	23.471539
118.793748	4022.987323	23.476557
119.086673	4042.310417	23.481575
119.051968	4048.497769	23.486592
119.241483	4052.192546	23.491610
119.131028	4064.843602	23.496627
119.462108	4068.203493	23.501645
119.516484	4082.190034	23.506663
119.439724	4093.020064	23.511680
119.914157	4103.183202	23.516698
119.973834	4107.908021	23.521715
119.933085	4107.252166	23.526733
120.495877	4114.006657	23.531751
120.366427	4140.667036	23.536768
120.608790	4134.448183	23.541786
120.867237	4143.244695	23.546803
121.090073	4137.074583	23.551821
121.343891	4135.656651	23.556839
121.038037	4139.123636	23.561856
121.287869	4142.514595	23.566874
121.463291	4160.182503	23.571891
121.371272	4158.436599	23.576909
121.746721	4153.658189	23.581927
121.568148	4163.665894	23.586944
121.665790	4167.486275	23.591962
122.018477	4182.426800	23.596979
122.045375	4190.047970	23.601997
122.095566	4195.608225	23.607015
122.183900	4198.762982	23.612032
122.560182	4189.033762	23.617050
122.488902	4211.251188	23.622067
122.789753	4223.500871	23.627085
123.239515	4215.675520	23.632103
123.229002	4203.669126	23.637120
123.258846	4199.442218	23.642138
123.436700	4201.122596	23.647155
123.600568	4200.606393	23.652173
123.630601	4192.401144	23.657191
123.559595	4193.277083	23.662208
123.782545	4189.402504	23.667226
123.887621	4205.348598	23.672243
123.975850	4198.816805	23.677261
124.024311	4182.383737	23.682279
124.058512	4224.479850	23.687296
124.317202	4219.381759	23.692314
124.249337	4232.729472	23.697331
123.876994	4231.077823	23.702349
124.439716	4242.886909	23.707367
124.503623	4258.437624	23.712384
125.120885	4251.616904	23.717402
125.194022	4256.876938	23.722419
124.921189	4254.609168	23.727437
125.062469	4260.012530	23.732455
125.233284	4266.206535	23.737472
125.096888	4284.922637	23.742490
125.605065	4299.377481	23.747507
125.828993	4296.488453	23.752525
125.984744	4289.813687	23.757543
125.841958	4296.055353	23.762560
126.234486	4319.575705	23.767578
126.370205	4322.328009	23.772595
126.524923	4327.066850	23.777613
126.506643	4318.212340	23.782631
126.606946	4322.930750	23.787648
126.657940	4329.737848	23.792666
126.508233	4337.849051	23.797683
126.825495	4348.634531	23.802701
127.043853	4359.109308	23.807719
126.956641	4363.613755	23.812736
126.881186	4362.613340	23.817754
127.587608	4383.193393	23.822771
127.510234	4393.714567	23.827789
127.687804	4378.601237	23.832807
127.589798	4394.535078	23.837824
127.862229	4403.091146	23.842842
128.136305	4401.770658	23.847859
128.443224	4407.308148	23.852877
128.968723	4395.538674	23.857895
128.663385	4399.428883	23.862912
128.719577	4399.593823	23.867930
129.076624	4401.804211	23.872947
128.858245	4424.105203	23.877965
129.350211	4422.525757	23.882983
129.120015	4428.266124	23.888000
129.429336	4421.551076	23.893018
129.355174	4423.513186	23.898035
129.428055	4423.009126	23.903053
130.263122	4414.864190	23.908071
129.931575	4417.840497	23.913088
129.873190	4421.746402	23.918106
130.270551	4433.039971	23.923123
130.283464	4445.851049	23.928141
130.593784	4443.782126	23.933159
130.883406	4443.533011	23.938176
130.867157	4441.446147	23.943194
130.759583	4443.563849	23.948211
130.740415	4445.900319	23.953229
131.151063	4441.989450	23.958247
130.926944	4450.826124	23.963264
130.867039	4448.418164	23.968282
131.188324	4449.431386	23.973299
131.307934	4463.058588	23.978317
131.750230	4460.435230	23.983335
131.236475	4463.758431	23.988352
131.577539	4471.731658	23.993370
131.785707	4489.043868	23.998387
131.808745	4497.593344	24.003405
132.486145	4494.486426	24.008423
132.213985	4501.024943	24.013440
132.195708	4519.243400	24.018458
132.708624	4515.482987	24.023475
132.519995	4521.009857	24.028493
132.724471	4516.838402	24.033511
132.968301	4525.662651	24.038528
133.116131	4542.079827	24.043546
133.202588	4543.166691	24.048563
133.493807	4551.583748	24.053581
133.632722	4543.351501	24.058599
133.367684	4555.096158	24.063616
133.573254	4573.887904	24.068634
133.858964	4583.267223	24.073651
134.229147	4586.521875	24.078669
134.257792	4581.652303	24.083687
134.219872	4580.396499	24.088704
134.171931	4595.554740	24.093722
134.908173	4606.711014	24.098739
134.648404	4615.392193	24.103757
134.808107	4610.130383	24.108775
134.651511	4615.125080	24.113792
135.106080	4629.620269	24.118810
135.384052	4627.343279	24.123827
135.188057	4636.638955	24.128845
135.618499	4629.839989	24.133863
135.712025	4641.144406	24.138880
135.620121	4662.595603	24.143898
135.908316	4673.142075	24.148915
135.863442	4677.497469	24.153933
136.423579	4655.142464	24.158951
136.208690	4664.752711	24.163968
136.180680	4685.408607	24.168986
136.605208	4681.419151	24.174003
136.604498	4697.639905	24.179021
136.638072	4696.382918	24.184039
136.676569	4717.207626	24.189056
136.937229	4722.701476	24.194074
137.071580	4720.158648	24.199091
137.033805	4735.914894	24.204109
137.243644	4740.859856	24.209127
137.848390	4738.323048	24.214144
138.058366	4735.676898	24.219162
138.363191	4727.189943	24.224179
138.380103	4736.406102	24.229197
138.506451	4733.682028	24.234215
138.377635	4743.354913	24.239232
138.238053	4734.874307	24.244250
138.543475	4743.946911	24.249267
138.759390	4769.234019	24.254285
139.112467	4759.035306	24.259303
139.177564	4765.410020	24.264320
138.904858	4765.368578	24.269338
139.421310	4762.444616	24.274355
139.318112	4783.771914	24.279373
139.737467	4790.097229	24.284391
139.880502	4783.017532	24.289408
140.016955	4787.142643	24.294426
140.192329	4786.458589	24.299443
139.935988	4793.624092	24.304461
140.170076	4806.150823	24.309479
140.466321	4814.364256	24.314496
140.591426	4818.449488	24.319514
141.003569	4813.550943	24.324531
140.736719	4820.633169	24.329549
140.803118	4817.650365	24.334567
141.198546	4831.924674	24.339584
141.400483	4846.391130	24.344602
141.557618	4833.952325	24.349619
141.287035	4846.689375	24.354637
141.596245	4846.341151	24.359655
142.097080	4859.709676	24.364672
141.516026	4871.384605	24.369690
142.040917	4864.306918	24.374707
142.110088	4878.051903	24.379725
142.642278	4882.076961	24.384743
142.406870	4896.910589	24.389760
142.521601	4895.789336	24.394778
142.782604	4892.164196	24.399795
142.545186	4910.042020	24.404813
142.972273	4916.978236	24.409831
143.100102	4928.019355	24.414848
142.921500	4941.721302	24.419866
143.164272	4948.486305	24.424883
143.562224	4957.715009	24.429901
143.394546	4968.405191	24.434919
143.642493	4974.717009	24.439936
143.870068	4987.274829	24.444954
144.056362	4993.443072	24.449971
144.080993	5000.813268	24.454989
144.390888	5019.133425	24.460007
144.572091	5019.475124	24.465024
144.857933	5029.923886	24.470042
145.023738	5017.897369	24.475059
144.753335	5022.963848	24.480077
144.714090	5036.022137	24.485095
144.868343	5057.500741	24.490112
145.234718	5060.417024	24.495130
145.384758	5066.122182	24.500147
145.649350	5091.535040	24.505165
145.849556	5093.864167	24.510183
145.823773	5084.060796	24.515200
145.670853	5108.087146	24.520218
146.022248	5120.161157	24.525235
145.746773	5124.293828	24.530253
146.060217	5145.859681	24.535271
146.590969	5150.858248	24.540288
146.518081	5159.491063	24.545306
146.899453	5172.929275	24.550323
146.726678	5186.412589	24.555341
146.855092	5199.035179	24.560359
147.199306	5203.530093	24.565376
147.796441	5212.593450	24.570394
147.832834	5210.760857	24.575411
148.335490	5207.866548	24.580429
148.244952	5210.002096	24.585447
148.552021	5226.463877	24.590464
148.444739	5244.121519	24.595482
148.966872	5235.109480	24.600499
149.044579	5244.544419	24.605517
149.133383	5244.553114	24.610535
149.453944	5240.576157	24.615552
149.152580	5245.759366	24.620570
149.570733	5237.951111	24.625587
149.507546	5241.732117	24.630605
149.830217	5255.487384	24.635623
149.906368	5262.356989	24.640640
149.837823	5270.564331	24.645658
150.035938	5266.220597	24.650675
149.642060	5271.233681	24.655693
149.860525	5284.069356	24.660711
150.624025	5290.992232	24.665728
150.465513	5296.398934	24.670746
150.904508	5296.413156	24.675763
150.693750	5310.808193	24.680781
151.001947	5321.877493	24.685799
151.233775	5321.855515	24.690816
151.179475	5326.942711	24.695834
151.464692	5338.361860	24.700851
151.750267	5349.238099	24.705869
151.703236	5359.316899	24.710887
151.701101	5354.307217	24.715904
152.002643	5370.538734	24.720922
152.162262	5375.284214	24.725939
152.303994	5384.971024	24.730957
152.152318	5392.329403	24.735975
152.666134	5400.865660	24.740992
152.616653	5414.655240	24.746010
152.731005	5421.509387	24.751027
152.894275	5429.341547	24.756045
152.918616	5440.848005	24.761063
153.210588	5443.267982	24.766080
153.112283	5449.780766	24.771098
153.261829	5471.021548	24.776115
153.673025	5475.004698	24.781133
153.827633	5476.265655	24.786151
154.033089	5486.662257	24.791168
154.025272	5513.654253	24.796186
154.099844	5511.840711	24.801203
154.437896	5515.850485	24.806221
154.764360	5537.420343	24.811239
155.381177	5530.257664	24.816256
154.956824	5540.793280	24.821274
154.657559	5546.471134	24.826291
155.460990	5556.954969	24.831309
155.453070	5566.865599	24.836327
156.137203	5558.667802	24.841344
156.245102	5550.680693	24.846362
156.570280	5544.658114	24.851379
156.640689	5541.767364	24.856397
156.280966	5555.326455	24.861415
157.140282	5558.711829	24.866432
157.390581	5570.115483	24.871450
157.186996	5577.322517	24.876467
157.323965	5569.611638	24.881485
157.427685	5583.963089	24.886503
157.610333	5572.293777	24.891520
157.663243	5576.219218	24.896538
157.780836	5579.399504	24.901555
157.903823	5578.102222	24.906573
157.888642	5590.396359	24.911591
158.292066	5602.483714	24.916608
158.020374	5616.850997	24.921626
158.124048	5601.724601	24.926643
157.920966	5618.015610	24.931661
158.165851	5638.857488	24.936679
158.715056	5644.286795	24.941696
158.722591	5671.410381	24.946714
158.947124	5673.843511	24.951731
159.181592	5679.692799	24.956749
159.431082	5698.485269	24.961767
159.593655	5698.769375	24.966784
159.594531	5703.972213	24.971802
159.921659	5720.861713	24.976819
160.066787	5730.342860	24.981837
160.253216	5736.342237	24.986855
160.606318	5740.965719	24.991872
160.446198	5748.792179	24.996890
160.695610	5750.469197	25.001907
161.346869	5751.492058	25.006925
161.138224	5763.893503	25.011943
161.446347	5759.106439	25.016960
161.487594	5749.925294	25.021978
161.425038	5755.204353	25.026995
161.759494	5770.848848	25.032013
161.974696	5789.891590	25.037031
162.105552	5786.525381	25.042048
162.024859	5793.429683	25.047066
161.882982	5790.848893	25.052083
162.346652	5810.168328	25.057101
162.146330	5824.730568	25.062119
162.427665	5832.218390	25.067136
162.664821	5843.853305	25.072154
162.476532	5850.033641	25.077171
162.828567	5869.826501	25.082189
162.894658	5883.331369	25.087207
163.173749	5891.758999	25.092224
163.495738	5905.369427	25.097242
163.318678	5919.157001	25.102259
164.631969	5914.400018	25.107277
164.349995	5918.470999	25.112295
164.417090	5929.225147	25.117312
165.040778	5931.420010	25.122330
165.003554	5931.558164	25.127347
165.357923	5923.200319	25.132365
165.471141	5930.558426	25.137383
165.328593	5924.064245	25.142400
165.553786	5937.827824	25.147418
165.894564	5948.834180	25.152435
165.953579	5952.132464	25.157453
166.013293	5955.603730	25.162471
166.170705	5956.332413	25.167488
166.339973	5964.953050	25.172506
166.367561	5988.782098	25.177523
166.953899	5990.944373	25.182541
167.135906	5980.264625	25.187559
167.255123	5976.073314	25.192576
167.368346	5982.195401	25.197594
167.211048	5989.427512	25.202611
167.347302	5996.359473	25.207629
167.401943	6012.442235	25.212647
167.521075	6024.387224	25.217664
167.806386	6033.255333	25.222682
168.079483	6040.930258	25.227699
168.048331	6042.947879	25.232717
168.550121	6050.100107	25.237735
168.572795	6065.368972	25.242752
168.678458	6069.404151	25.247770
168.743714	6070.636133	25.252787
168.970711	6075.518228	25.257805
169.058995	6097.266143	25.262823
169.404218	6102.783223	25.267840
169.872017	6103.576510	25.272858
169.926896	6114.375226	25.277875
170.223477	6119.720679	25.282893
170.330459	6131.607895	25.287911
170.447503	6129.482230	25.292928
170.539468	6132.111244	25.297946
170.567496	6128.187778	25.302963
170.912890	6123.600010	25.307981
170.822887	6133.521746	25.312999
171.102426	6147.453099	25.318016
171.697524	6142.530462	25.323034
171.587420	6159.513784	25.328051
171.811166	6153.322237	25.333069
171.451682	6154.144362	25.338087
172.005771	6158.415705	25.343104
172.176641	6163.389392	25.348122
171.913366	6172.348989	25.353139
172.354746	6170.088203	25.358157
172.729989	6185.540951	25.363175
172.318364	6202.565317	25.368192
172.689161	6202.591996	25.373210
172.689079	6220.327336	25.378227
172.992104	6241.774499	25.383245
173.045580	6248.546680	25.388263
173.432719	6271.835758	25.393280
173.513857	6281.021394	25.398298
173.362549	6286.553194	25.403315
173.775557	6295.274425	25.408333
174.230270	6298.679645	25.413351
174.108823	6306.988838	25.418368
174.485837	6322.228221	25.423386
174.427200	6337.567768	25.428403
174.931031	6350.284125	25.433421
174.739970	6363.100273	25.438439
175.042616	6367.891722	25.443456
175.404522	6383.862951	25.448474
175.430752	6403.596747	25.453491
175.623446	6403.831218	25.458509
175.878222	6418.358456	25.463527
175.741483	6427.671766	25.468544
176.359982	6436.578264	25.473562
176.195582	6459.480340	25.478579
176.314134	6464.926691	25.483597
176.450069	6485.902008	25.488615
176.770948	6498.782208	25.493632
177.323571	6504.077535	25.498650
177.464547	6516.183882	25.503667
178.386869	6514.205154	25.508685
178.450714	6505.269361	25.513703
178.310287	6511.545411	25.518720
178.893739	6508.310663	25.523738
178.876091	6504.640655	25.528755
179.505178	6492.602025	25.533773
179.276779	6496.719697	25.538791
179.321394	6488.599761	25.543808
179.616680	6484.857046	25.548826
179.486272	6494.421169	25.553843
179.752501	6489.144860	25.558861
180.056236	6503.385843	25.563879
179.986398	6517.222968	25.568896
180.483455	6513.145150	25.573914
180.130061	6513.323491	25.578931
180.498607	6518.024227	25.583949
180.423483	6522.631260	25.588967
180.394387	6519.066933	25.593984
181.139087	6532.581431	25.599002
180.834101	6548.069841	25.604019
181.412540	6546.290713	25.609037
181.355715	6540.409687	25.614055
181.157140	6552.283800	25.619072
181.572402	6567.477212	25.624090
181.484730	6575.088767	25.629107
181.627281	6594.667364	25.634125
181.957954	6605.040856	25.639143
181.915122	6614.899528	25.644160
182.719518	6637.719801	25.649178
182.496782	6644.331628	25.654195
182.470620	6646.172287	25.659213
183.066904	6670.315396	25.664231
183.151931	6684.700794	25.669248
183.083128	6692.041879	25.674266
183.696763	6699.750977	25.679284
183.365968	6708.773590	25.684301
183.907669	6724.502504	25.689319
184.916799	6721.591683	25.694336
185.882969	6700.047765	25.699354
185.779578	6706.842806	25.704372
185.911077	6686.529612	25.709389
186.057364	6665.976466	25.714407
185.820758	6668.966398	25.719424
185.932340	6662.823212	25.724442
185.892847	6666.390719	25.729460
186.168424	6662.977635	25.734477
186.220826	6675.078564	25.739495
186.254944	6693.948341	25.744512
186.459678	6699.361367	25.749530
186.097036	6698.751210	25.754548
186.373847	6708.246609	25.759565
186.881299	6713.083414	25.764583
186.898947	6729.816478	25.769600
187.177174	6731.012199	25.774618
187.109505	6751.408989	25.779636
187.226536	6756.713274	25.784653
187.471526	6782.409128	25.789671
187.326708	6792.861713	25.794688
187.530712	6798.152146	25.799706
187.793464	6815.407238	25.804724
187.948610	6839.310946	25.809741
188.457310	6852.119021	25.814759
188.710382	6866.804339	25.819776
188.803464	6880.074482	25.824794
189.030445	6892.422359	25.829812
189.321619	6896.174825	25.834829
189.662383	6917.148781	25.839847
189.491951	6929.464058	25.844864
190.001821	6924.498107	25.849882
190.175758	6938.407701	25.854900
190.149189	6948.250624	25.859917
190.379410	6951.999446	25.864935
190.450641	6971.287764	25.869952
191.059924	6977.023518	25.874970
190.922677	6982.156371	25.879988
191.032605	6984.681958	25.885005
191.619826	6997.989088	25.890023
191.876224	7011.337960	25.895040
192.072757	6998.404009	25.900058
191.872630	7012.605430	25.905076
192.223492	7030.605241	25.910093
192.511419	7029.434187	25.915111
192.656626	7037.620226	25.920128
192.795871	7048.682355	25.925146
192.725194	7066.245050	25.930164
193.007566	7067.336275	25.935181
193.305766	7076.464978	25.940199
193.054622	7098.998672	25.945216
193.482784	7104.557987	25.950234
193.842472	7121.506059	25.955252
194.021243	7134.256822	25.960269
194.133640	7140.435387	25.965287
194.216236	7164.673007	25.970304
194.795859	7162.420726	25.975322
194.887133	7178.438323	25.980340
194.865772	7196.399325	25.985357
195.253849	7185.117753	25.990375
195.092653	7210.521090	25.995392
195.385977	7218.424739	26.000410
195.979506	7219.739405	26.005428
195.792134	7247.857693	26.010445
196.190733	7247.732021	26.015463
196.207033	7262.816647	26.020480
196.492026	7279.651698	26.025498
196.526018	7287.634500	26.030516
196.693183	7305.660786	26.035533
197.405024	7309.989153	26.040551
197.286645	7330.859854	26.045568
197.505745	7341.625412	26.050586
198.053733	7338.066453	26.055604
198.539688	7336.134383	26.060621
199.089020	7345.323932	26.065639
198.941829	7360.584227	26.070656
199.005385	7360.721276	26.075674
199.265669	7360.815945	26.080692
199.009938	7366.884908	26.085709
199.648335	7361.821212	26.090727
199.641898	7384.262815	26.095744
200.063342	7396.339328	26.100762
200.386415	7382.584630	26.105780
199.924648	7400.330461	26.110797
200.529838	7379.083120	26.115815
200.973084	7401.234307	26.120832
201.040216	7409.501456	26.125850
201.444966	7412.394790	26.130868
201.387009	7413.141362	26.135885
201.756857	7407.339897	26.140903
201.520936	7412.943830	26.145920
201.535742	7409.357340	26.150938
202.031615	7407.197065	26.155956
201.798968	7431.239090	26.160973
202.374441	7429.166839	26.165991
202.372974	7441.616906	26.171008
202.179816	7446.468085	26.176026
202.536284	7470.795520	26.181044
202.595284	7479.069513	26.186061
203.116974	7490.755572	26.191079
202.878548	7505.076875	26.196096
203.206794	7530.294134	26.201114
203.566046	7534.398659	26.206132
203.529742	7544.208904	26.211149
203.930815	7551.454253	26.216167
204.182064	7575.106186	26.221184
204.292414	7588.093294	26.226202
204.561121	7597.611015	26.231220
204.597024	7623.639097	26.236237
204.981529	7628.897116	26.241255
205.005460	7652.128238	26.246272
205.163017	7678.572163	26.251290
205.473682	7683.635811	26.256308
205.871006	7700.264580	26.261325
206.084169	7715.123131	26.266343
206.619221	7720.132134	26.271360
206.940536	7717.686467	26.276378
207.416471	7732.217504	26.281396
207.315497	7734.094617	26.286413
207.516611	7736.421664	26.291431
207.861702	7750.914564	26.296448
207.844522	7748.991054	26.301466
208.121965	7741.588724	26.306484
208.184045	7768.600422	26.311501
208.506286	7785.695289	26.316519
208.364729	7793.636317	26.321536
208.563300	7805.976894	26.326554
209.000339	7812.943588	26.331572
209.097764	7827.047194	26.336589
209.355022	7834.220397	26.341607
209.917678	7844.228464	26.346624
209.867435	7850.524139	26.351642
210.153934	7851.576211	26.356660
210.188742	7866.951220	26.361677
210.709998	7871.951064	26.366695
210.817348	7874.713281	26.371712
211.308150	7895.068630	26.376730
211.301059	7902.491356	26.381748
211.123159	7911.302246	26.386765
211.470929	7916.823933	26.391783
211.770065	7925.831043	26.396800
211.829278	7937.483383	26.401818
211.990153	7944.132197	26.406836
212.156278	7942.828625	26.411853
212.229173	7962.078221	26.416871
212.418043	7974.347696	26.421888
212.383634	7987.442428	26.426906
212.571789	7998.332216	26.431924
212.679291	8019.340983	26.436941
213.223117	8033.267384	26.441959
213.432246	8051.793464	26.446976
213.412703	8076.851093	26.451994
213.762713	8075.292746	26.457012
213.994162	8099.416086	26.462029
214.568686	8109.948090	26.467047
215.004814	8130.641009	26.472064
215.092138	8145.277292	26.477082
215.278676	8147.537088	26.482100
215.371772	8143.573211	26.487117
215.949556	8156.564588	26.492135
216.355421	8160.302636	26.497152
216.314259	8161.458511	26.502170
216.725595	8161.834426	26.507188
216.849790	8182.191171	26.512205
217.207438	8180.160240	26.517223
217.214384	8172.473471	26.522240
217.171089	8168.237422	26.527258
217.477061	8180.456529	26.532276
217.481829	8195.775680	26.537293
217.737107	8202.279720	26.542311
217.969339	8209.215515	26.547328
218.301652	8220.940606	26.552346
218.476533	8224.857138	26.557364
218.718260	8242.041302	26.562381
218.865650	8258.050718	26.567399
219.079677	8264.242270	26.572416
219.330179	8284.145430	26.577434
219.884966	8281.507826	26.582452
220.063522	8304.493795	26.587469
220.070393	8314.164280	26.592487
220.133618	8317.280642	26.597504
220.336178	8326.068892	26.602522
220.754321	8340.785222	26.607540
220.658053	8352.761307	26.612557
221.014261	8371.403620	26.617575
221.461056	8382.126549	26.622592
221.488943	8394.443675	26.627610
221.900287	8407.150583	26.632628
222.116351	8428.739100	26.637645
222.263959	8425.948803	26.642663
222.512202	8430.807832	26.647680
222.513181	8450.638858	26.652698
223.166498	8452.702707	26.657716
222.770839	8472.400658	26.662733
223.558109	8477.212722	26.667751
223.571789	8488.885342	26.672768
223.656012	8505.764412	26.677786
223.727190	8512.846816	26.682804
224.025011	8520.194090	26.687821
224.332754	8526.058796	26.692839
224.598911	8539.503096	26.697856
224.516479	8552.682309	26.702874
225.196851	8563.041165	26.707892
225.080162	8568.999127	26.712909
225.251637	8587.944224	26.717927
225.471580	8604.895807	26.722944
225.482552	8623.135087	26.727962
225.838073	8646.535230	26.732980
226.266310	8654.607001	26.737997
226.036972	8667.416270	26.743015
226.457058	8690.303733	26.748032
226.542316	8704.387286	26.753050
226.759710	8712.886955	26.758068
227.235574	8728.868905	26.763085
227.432283	8739.149177	26.768103
227.572051	8755.635649	26.773120
227.962123	8772.271494	26.778138
229.034176	8780.470482	26.783156
229.218612	8790.872755	26.788173
229.642587	8786.943310	26.793191
229.669579	8775.982919	26.798208
229.678809	8790.704289	26.803226
229.756350	8791.847190	26.808244
230.140019	8804.643446	26.813261
230.192255	8807.172246	26.818279
230.662404	8808.427653	26.823296
231.174468	8827.478505	26.828314
231.463422	8832.272943	26.833332
231.655464	8837.315373	26.838349
231.470815	8842.758995	26.843367
231.866325	8833.926719	26.848384
231.812054	8840.155382	26.853402
231.987913	8854.936814	26.858420
232.158680	8857.723336	26.863437
232.401653	8858.277600	26.868455
232.762629	8884.527940	26.873472
232.986172	8902.204847	26.878490
233.347372	8893.625500	26.883508
233.195951	8915.241827	26.888525
233.481243	8925.591129	26.893543
233.808726	8928.680443	26.898560
233.708583	8955.137805	26.903578
234.001169	8961.827459	26.908596
234.394372	8981.139049	26.913613
234.607555	8994.807828	26.918631
235.059443	9001.582670	26.923648
235.303631	9026.172529	26.928666
235.476750	9014.316729	26.933684
235.945620	9027.393125	26.938701
236.083763	9038.965276	26.943719
236.512275	9036.817093	26.948736
236.459211	9046.142691	26.953754
236.762953	9049.490001	26.958772
237.044101	9055.042409	26.963789
237.515618	9072.740975	26.968807
237.783165	9075.497552	26.973824
237.592573	9077.616153	26.978842
237.434048	9075.495838	26.983860
237.899799	9104.395662	26.988877
237.525758	9109.754284	26.993895
238.101897	9122.924231	26.998912
238.084721	9132.074572	27.003930
238.154953	9157.850777	27.008948
238.601446	9167.889277	27.013965
238.814943	9190.948946	27.018983
239.308400	9207.443276	27.024000
239.465026	9232.902464	27.029018
239.793015	9248.799158	27.034036
240.539493	9252.743672	27.039053
240.206659	9265.875682	27.044071
240.943222	9272.526177	27.049088
240.873778	9291.884379	27.054106
241.157979	9307.608295	27.059124
241.730571	9312.625240	27.064141
241.811869	9321.637626	27.069159
242.329327	9339.975677	27.074176
242.483273	9354.717025	27.079194
242.748611	9347.285543	27.084212
242.956513	9356.657478	27.089229
242.808868	9377.465651	27.094247
243.171131	9380.867452	27.099264
243.559550	9401.310434	27.104282
243.795414	9410.204190	27.109300
244.268871	9410.217287	27.114317
244.195142	9433.601311	27.119335
244.433137	9435.572154	27.124352
244.561673	9449.396104	27.129370
244.887708	9468.273212	27.134388
245.235211	9478.032194	27.139405
245.034605	9494.074405	27.144423
245.609501	9496.858795	27.149440
245.354092	9519.553408	27.154458
245.900165	9538.907061	27.159476
246.069133	9557.999769	27.164493
246.389451	9578.153617	27.169511
246.860454	9600.378017	27.174528
246.969694	9610.177823	27.179546
247.192755	9627.392131	27.184564
247.628559	9636.426891	27.189581
247.554380	9654.329610	27.194599
248.054066	9668.829637	27.199616
248.120224	9682.307634	27.204634
248.093662	9693.359986	27.209652
248.646932	9709.218502	27.214669
248.776050	9735.720174	27.219687
249.468449	9745.295285	27.224704
249.263489	9761.764627	27.229722
249.661217	9766.900895	27.234740
250.387075	9768.908912	27.239757
250.222284	9789.810104	27.244775
250.503181	9783.467482	27.249792
251.011126	9795.328722	27.254810
251.034725	9817.851419	27.259828
251.670334	9813.695951	27.264845
251.702483	9826.961110	27.269863
252.002871	9834.211825	27.274880
252.091778	9855.113588	27.279898
252.424050	9859.643714	27.284916
252.477952	9862.126388	27.289933
252.762339	9873.910394	27.294951
252.652564	9895.229512	27.299968
253.133901	9905.528567	27.304986
253.491384	9922.377869	27.310004
253.717385	9938.850321	27.315021
253.966869	9953.009996	27.320039
254.063455	9973.368458	27.325056
254.515112	9990.449941	27.330074
254.541794	10011.999705	27.335092
255.147711	10010.967804	27.340109
255.045953	10041.082951	27.345127
255.663998	10047.552006	27.350144
255.858546	10062.406021	27.355162
255.831914	10084.649475	27.360180
256.057959	10093.671123	27.365197
256.412910	10122.991945	27.370215
256.674452	10117.657672	27.375232
256.594907	10136.292554	27.380250
256.931328	10155.497446	27.385268
257.802856	10159.862214	27.390285
257.837227	10187.012539	27.395303
258.443470	10195.366463	27.400320
258.756284	10193.670997	27.405338
258.772687	10207.386810	27.410356
259.449340	10207.633140	27.415373
259.931283	10219.516177	27.420391
260.187825	10218.071686	27.425408
260.542125	10220.059117	27.430426
260.563483	10227.500100	27.435444
261.089381	10236.861246	27.440461
260.979123	10240.421206	27.445479
261.332864	10238.329247	27.450496
261.811537	10237.927553	27.455514
261.544062	10238.199644	27.460532
261.878363	10253.244064	27.465549
261.933176	10267.905309	27.470567
261.997624	10272.895962	27.475584
262.185153	10289.774343	27.480602
262.391397	10309.099348	27.485620
262.990947	10317.769609	27.490637
262.717098	10331.390926	27.495655
262.902278	10349.363703	27.500672
263.370634	10364.603295	27.505690
263.403442	10394.124351	27.510708
263.580944	10397.858057	27.515725
263.960641	10421.755303	27.520743
264.308148	10431.586134	27.525760
264.830648	10454.743298	27.530778
264.565149	10474.188967	27.535796
265.081754	10484.100700	27.540813
265.514679	10509.910338	27.545831
265.721322	10522.477746	27.550848
265.873945	10529.411571	27.555866
266.266905	10559.098662	27.560884
266.478148	10574.556534	27.565901
266.787524	10599.045313	27.570919
266.732087	10608.252626	27.575936
266.941691	10626.194686	27.580954
267.109384	10648.494960	27.585972
267.528565	10666.799146	27.590989
267.791380	10690.373090	27.596007
268.034454	10710.589173	27.601024
268.323548	10730.082529	27.606042
268.641160	10749.492267	27.611060
269.039505	10766.104612	27.616077
269.538009	10796.076389	27.621095
269.718833	10809.576468	27.626112
270.271166	10828.229142	27.631130
270.292452	10845.640320	27.636148
270.915653	10860.425219	27.641165
271.201646	10879.698104	27.646183
271.108733	10897.628106	27.651200
271.635536	10897.057383	27.656218
271.800840	10924.219250	27.661236
272.091835	10933.450636	27.666253
272.472580	10954.565948	27.671271
272.446212	10969.014143	27.676288
272.701624	10980.409324	27.681306
272.842745	11004.782732	27.686324
273.111617	11031.519409	27.691341
273.330527	11040.306646	27.696359
273.466388	11060.328964	27.701376
274.059114	11086.810661	27.706394
274.773304	11098.075739	27.711412
275.124572	11105.950575	27.716429
275.807047	11119.684611	27.721447
275.816578	11125.333033	27.726464
276.361624	11121.796512	27.731482
276.470909	11130.334858	27.736500
276.741066	11136.651865	27.741517
276.932719	11137.457015	27.746535
276.972230	11151.901574	27.751552
277.690432	11160.810389	27.756570
277.700806	11175.039827	27.761588
277.859619	11172.616571	27.766605
277.973438	11186.610531	27.771623
278.199201	11201.047092	27.776640
278.578639	11199.524286	27.781658
278.283591	11234.127001	27.786676
278.575230	11237.476935	27.791693
278.883852	11249.598957	27.796711
278.917817	11271.215272	27.801728
279.585501	11297.531915	27.806746
279.646378	11315.342859	27.811764
279.779731	11331.781427	27.816781
280.328868	11349.179881	27.821799
280.290792	11377.670106	27.826816
280.780220	11391.885565	27.831834
280.789623	11413.749401	27.836852
281.433006	11436.235732	27.841869
281.771514	11454.842985	27.846887
281.623345	11485.010510	27.851904
282.159532	11503.558569	27.856922
282.559606	11520.079579	27.861940
282.537386	11530.705590	27.866957
283.201128	11559.326708	27.871975
283.217840	11577.511976	27.876992
284.094494	11597.789608	27.882010
283.919695	11619.008964	27.887028
284.502582	11638.287833	27.892045
285.281496	11645.233912	27.897063
285.077795	11656.018020	27.902080
285.481711	11670.429190	27.907098
285.663614	11684.793708	27.912116
285.732056	11696.075589	27.917133
286.160706	11716.145768	27.922151
286.318433	11735.101347	27.927168
286.814906	11753.466159	27.932186
287.234825	11776.911679	27.937204
287.640721	11783.403505	27.942221
288.262782	11797.578727	27.947239
287.881568	11800.032296	27.952256
288.574004	11808.635885	27.957274
289.362675	11816.854205	27.962292
289.748465	11814.383454	27.967309
290.049534	11810.878190	27.972327
290.384139	11823.110858	27.977344
291.133444	11823.209290	27.982362
290.993715	11839.342271	27.987380
291.120977	11831.755081	27.992397
291.590651	11822.970061	27.997415
291.467207	11837.843847	28.002432
291.707143	11828.377414	28.007450
291.656791	11849.583946	28.012468
292.014880	11858.282967	28.017485
291.992365	11865.657959	28.022503
292.280776	11897.359442	28.027520
292.685566	11896.923449	28.032538
292.735311	11931.611913	28.037556
292.872360	11947.402383	28.042573
293.326842	11959.179409	28.047591
293.129043	11978.258078	28.052608
293.422712	12003.229409	28.057626
293.654873	12017.873920	28.062644
293.851108	12051.211263	28.067661
294.455884	12068.204781	28.072679
294.632553	12102.843494	28.077696
294.944106	12114.281943	28.082714
295.094560	12146.738932	28.087732
295.692774	12162.591700	28.092749
296.051167	12174.544584	28.097767
295.984985	12198.783725	28.102784
296.655780	12209.430214	28.107802
296.900559	12229.613620	28.112820
297.269731	12260.982043	28.117837
297.542061	12264.071798	28.122855
297.864175	12294.027829	28.127872
298.333938	12302.398395	28.132890
298.824678	12318.428243	28.137908
299.025022	12343.087369	28.142925
299.795000	12341.518147	28.147943
299.988312	12352.185548	28.152960
300.266747	12378.079283	28.157978
300.637014	12393.014042	28.162996
300.247143	12401.134612	28.168013
300.708948	12421.577083	28.173031
301.312573	12442.827790	28.178048
301.850537	12439.087647	28.183066
302.301442	12451.403433	28.188084
302.100169	12478.190051	28.193101
302.463598	12481.307443	28.198119
302.525409	12507.581674	28.203136
302.823667	12523.169746	28.208154
303.315825	12535.844254	28.213172
303.610991	12541.328820	28.218189
304.376147	12553.269317	28.223207
304.883705	12557.408279	28.228224
305.389541	12557.998134	28.233242
305.597868	12575.508016	28.238260
305.627924	12588.272555	28.243277
306.103051	12588.556979	28.248295
306.258127	12593.079777	28.253312
306.512407	12616.152544	28.258330
306.927927	12631.571696	28.263348
306.864456	12629.509517	28.268365
307.346323	12645.473236	28.273383
306.979455	12658.153510	28.278400
307.432423	12677.231263	28.283418
307.915101	12689.504200	28.288436
307.462944	12719.245222	28.293453
308.118196	12738.740662	28.298471
308.274818	12769.274222	28.303488
308.298604	12797.701064	28.308506
309.142285	12825.054965	28.313524
308.929576	12850.666782	28.318541
309.532174	12864.904853	28.323559
309.612252	12898.019929	28.328576
309.847877	12921.019187	28.333594
310.468768	12942.058953	28.338612
310.867185	12976.016681	28.343629
311.007050	12981.407496	28.348647
311.186770	13011.463204	28.353664
311.596526	13030.707490	28.358682
312.120761	13052.763293	28.363700
312.216474	13078.215049	28.368717
312.687977	13097.587430	28.373735
312.795994	13117.957151	28.378752
313.333470	13140.911287	28.383770
313.854053	13167.278468	28.388788
313.964399	13184.120818	28.393805
314.403090	13198.982098	28.398823
314.572016	13214.583524	28.403840
314.708664	13238.415527	28.408858
315.237778	13253.097536	28.413876
315.489920	13279.438205	28.418893
316.252211	13301.988259	28.423911
316.263274	13319.496491	28.428928
316.584054	13348.466221	28.433946
317.337054	13362.299895	28.438964
317.571476	13377.898921	28.443981
317.969960	13396.380628	28.448999
317.809522	13413.034959	28.454016
318.217763	13435.840896	28.459034
318.821689	13445.051889	28.464052
318.913807	13469.795720	28.469069
319.342827	13479.614173	28.474087
319.752253	13497.549727	28.479104
319.637720	13522.922379	28.484122
320.418235	13536.388640	28.489140
320.327897	13574.407668	28.494157
320.649029	13594.847082	28.499175
321.039451	13604.602593	28.504192
321.415776	13631.404753	28.509210
321.995943	13653.831643	28.514228
322.488502	13676.488023	28.519245
323.054035	13675.485278	28.524263
323.447874	13697.948523	28.529280
323.882049	13701.827427	28.534298
324.556297	13704.379140	28.539316
324.705154	13720.823036	28.544333
324.948759	13723.763186	28.549351
325.124180	13720.916229	28.554368
325.400119	13734.651424	28.559386
325.523669	13751.844074	28.564404
325.942203	13750.463087	28.569421
326.257187	13769.760609	28.574439
326.499197	13780.052156	28.579456
326.557005	13794.537044	28.584474
327.102250	13808.891319	28.589492
326.971626	13816.105297	28.594509
327.591008	13832.778082	28.599527
328.073888	13851.639803	28.604544
328.229520	13867.687210	28.609562
328.731740	13880.056398	28.614580
328.625187	13896.409040	28.619597
329.311871	13897.413527	28.624615
329.685961	13917.161051	28.629632
329.599762	13942.121028	28.634650
329.843536	13942.353407	28.639668
329.960811	13961.045637	28.644685
330.516570	13987.845190	28.649703
330.911642	14010.941222	28.654720
330.995975	14029.004689	28.659738
331.620685	14045.645568	28.664756
332.104411	14057.701587	28.669773
332.607861	14065.763312	28.674791
332.957272	14089.016704	28.679808
332.926734	14103.607478	28.684826
333.553314	14114.964559	28.689844
333.818447	14136.471246	28.694861
334.213412	14149.266017	28.699879
334.693654	14167.846826	28.704896
334.818542	14179.327998	28.709914
335.430526	14189.390030	28.714932
335.288138	14211.335108	28.719949
335.622221	14223.920602	28.724967
335.861469	14248.902323	28.729984
335.972276	14265.076359	28.735002
336.260440	14280.051546	28.740020
336.699637	14316.451953	28.745037
337.051836	14334.264573	28.750055
337.354441	14364.964136	28.755072
337.557153	14384.282494	28.760090
338.298758	14405.703584	28.765108
338.682006	14436.889050	28.770125
339.026818	14450.491303	28.775143
339.258301	14468.139106	28.780160
339.458580	14495.463944	28.785178
339.898789	14516.171182	28.790196
340.253047	14535.193884	28.795213
340.598195	14560.623508	28.800231
341.303418	14578.015856	28.805248
341.378223	14600.664024	28.810266
341.972800	14614.956683	28.815284
341.864353	14640.944851	28.820301
342.260117	14659.347734	28.825319
342.830431	14678.969911	28.830336
342.753337	14705.535948	28.835354
343.320867	14717.665731	28.840372
343.795483	14747.288659	28.845389
343.865004	14775.480731	28.850407
344.486880	14792.195403	28.855424
344.513072	14816.995020	28.860442
345.096702	14837.415616	28.865460
344.943923	14872.007526	28.870477
345.027174	14884.945391	28.875495
346.017396	14919.340287	28.880512
345.944781	14948.363641	28.885530
346.452485	14963.008106	28.890548
346.551604	14995.673782	28.895565
346.967438	15013.896268	28.900583
347.516869	15039.299442	28.905600
347.614148	15072.905073	28.910618
348.322290	15096.414284	28.915636
348.433691	15127.734227	28.920653
348.584968	15156.584127	28.925671
349.267398	15169.741056	28.930688
349.465892	15196.713253	28.935706
350.340919	15206.576095	28.940724
350.781763	15239.323533	28.945741
351.194519	15246.819729	28.950759
351.550440	15273.234088	28.955776
352.419352	15272.036767	28.960794
353.353477	15273.762629	28.965812
353.399393	15282.245304	28.970829
353.751700	15285.785855	28.975847
354.050835	15282.965642	28.980864
354.129098	15294.838482	28.985882
354.577666	15304.190903	28.990900
354.617548	15319.350648	28.995917
354.853919	15331.485085	29.000935
355.160948	15344.450459	29.005952
355.340902	15370.551745	29.010970
355.812563	15373.897142	29.015988
356.275482	15401.585610	29.021005
356.299604	15423.979724	29.026023
356.314245	15439.776387	29.031040
356.648053	15471.357013	29.036058
356.923670	15496.165900	29.041076
357.082131	15531.410076	29.046093
357.499844	15572.114585	29.051111
358.302651	15590.990452	29.056128
358.120361	15624.038285	29.061146
358.569938	15654.692894	29.066164
359.135663	15691.241238	29.071181
358.915265	15726.540332	29.076199
359.661385	15745.005992	29.081216
359.706046	15785.602428	29.086234
360.204692	15817.135842	29.091252
360.481401	15850.166908	29.096269
360.956598	15882.090757	29.101287
361.840530	15898.305979	29.106304
362.197299	15942.594755	29.111322
362.965390	15954.926999	29.116340
363.375307	15977.262992	29.121357
363.362062	16013.735885	29.126375
364.010216	16020.372406	29.131392
364.362332	16045.208171	29.136410
364.937862	16068.790988	29.141428
365.338170	16080.418054	29.146445
365.352120	16104.663980	29.151463
365.848921	16114.362912	29.156480
365.794141	16141.014469	29.161498
366.114596	16158.340129	29.166516
366.669986	16172.372804	29.171533
367.118319	16201.260973	29.176551
367.941812	16203.682270	29.181568
368.067417	16217.827372	29.186586
368.424968	16241.844365	29.191604
368.861461	16254.768816	29.196621
368.805280	16274.292996	29.201639
369.255843	16298.579282	29.206656
369.470087	16323.319171	29.211674
369.797745	16344.542339	29.216692
369.960471	16366.569307	29.221709
370.162670	16394.761698	29.226727
370.615589	16416.103573	29.231744
370.891963	16450.909442	29.236762
371.124739	16492.584944	29.241780
371.624229	16513.041456	29.246797
371.977213	16549.544054	29.251815
372.502522	16572.197533	29.256832
372.923739	16599.657025	29.261850
373.474398	16622.752567	29.266868
374.163263	16640.540295	29.271885
374.376911	16676.061535	29.276903
375.149445	16692.870312	29.281920
375.421525	16721.867460	29.286938
375.771520	16746.883027	29.291956
375.791044	16765.768246	29.296973
376.088137	16798.797896	29.301991
376.614582	16828.388721	29.307008
376.924977	16857.915811	29.312026
377.305088	16882.319945	29.317044
377.935944	16905.405099	29.322061
377.948977	16928.578508	29.327079
378.667792	16948.501463	29.332096
378.968141	16979.692105	29.337114
379.045777	17006.106343	29.342132
379.903587	17028.174463	29.347149
379.893268	17053.432384	29.352167
380.445688	17070.205395	29.357184
380.794297	17097.959614	29.362202
381.172966	17127.031476	29.367220
381.548350	17151.217506	29.372237
381.754919	17187.618569	29.377255
383.053189	17185.495261	29.382272
383.405053	17209.561120	29.387290
383.512169	17241.261017	29.392308
383.699204	17246.216504	29.397325
384.066552	17278.273812	29.402343
384.684069	17300.037712	29.407360
385.191853	17314.792185	29.412378
385.333387	17343.678628	29.417396
386.108483	17350.538016	29.422413
385.836375	17382.725392	29.427431
386.718571	17396.278971	29.432448
387.039070	17408.068969	29.437466
386.975922	17426.422708	29.442484
387.452547	17447.702983	29.447501
387.552413	17462.643464	29.452519
388.056956	17481.709542	29.457536
388.534143	17506.460209	29.462554
388.916674	17534.033823	29.467572
389.305973	17545.804695	29.472589
389.168650	17577.877690	29.477607
389.446604	17606.038561	29.482624
390.179826	17633.214740	29.487642
390.117288	17665.444107	29.492660
391.198535	17692.566900	29.497677
391.497888	17712.978551	29.502695
391.766685	17738.371847	29.507712
391.893302	17769.521291	29.512730
392.626977	17802.198864	29.517748
393.067871	17825.230233	29.522765
393.498521	17855.768803	29.527783
394.006001	17879.671141	29.532800
394.299160	17901.460018	29.537818
394.709445	17932.644508	29.542836
395.019858	17959.128392	29.547853
395.109442	17990.891274	29.552871
395.666635	18021.499770	29.557888
395.767615	18048.948296	29.562906
396.214930	18078.918105	29.567924
397.075760	18103.984583	29.572941
397.823286	18136.072453	29.577959
398.467211	18140.742819	29.582976
400.138122	18118.819850	29.587994
400.250249	18136.167735	29.593012
400.352049	18137.710247	29.598029
400.953946	18156.124230	29.603047
401.178933	18163.437011	29.608064
401.523484	18165.973545	29.613082
401.690408	18183.554096	29.618100
402.285301	18193.472185	29.623117
402.307413	18209.063585	29.628135
402.445848	18218.623706	29.633152
402.962892	18236.721377	29.638170
402.933192	18261.743397	29.643188
403.756095	18281.434950	29.648205
403.791151	18307.018002	29.653223
403.676739	18328.411779	29.658240
403.989687	18355.405796	29.663258
404.278488	18384.451027	29.668276
405.013032	18416.535249	29.673293
405.322780	18457.017495	29.678311
405.681246	18479.809417	29.683328
406.058014	18519.277952	29.688346
406.368749	18545.317489	29.693364
406.948268	18571.776073	29.698381
407.109392	18608.025099	29.703399
407.215803	18639.594879	29.708416
407.618311	18667.822871	29.713434
407.945069	18712.146588	29.718452
408.876077	18734.616142	29.723469
409.613369	18747.776266	29.728487
410.143854	18780.090617	29.733504
410.458323	18798.638178	29.738522
410.788535	18826.021229	29.743540
411.398441	18841.009329	29.748557
411.827642	18871.988740	29.753575
412.217955	18901.448317	29.758592
412.612040	18917.791447	29.763610
412.930442	18937.791012	29.768628
413.652053	18958.091736	29.773645
413.777377	18983.217778	29.778663
414.000278	19009.760707	29.783680
414.585187	19038.592639	29.788698
414.613618	19064.351623	29.793716
415.136639	19090.737409	29.798733
415.483853	19122.601713	29.803751
415.714086	19154.694977	29.808768
416.689439	19177.905418	29.813786
416.540482	19219.551412	29.818804
417.069854	19234.476734	29.823821
417.532786	19264.338849	29.828839
417.946349	19302.388803	29.833856
418.360680	19330.644461	29.838874
418.786218	19360.424914	29.843892
419.386051	19390.115047	29.848909
419.812277	19424.410145	29.853927
420.355814	19467.855315	29.858944
420.731643	19485.993480	29.863962
420.726117	19519.411810	29.868980
421.425157	19548.687574	29.873997
421.711826	19581.025898	29.879015
422.099507	19619.454018	29.884032
422.835361	19645.393791	29.889050
422.992689	19686.809916	29.894068
423.372835	19711.988269	29.899085
423.515536	19753.363983	29.904103
424.079142	19793.566692	29.909120
424.456127	19821.072792	29.914138
424.512289	19862.801996	29.919156
425.179764	19907.860744	29.924173
425.758447	19938.802702	29.929191
425.911289	19985.172581	29.934208
426.948276	20018.744804	29.939226
426.973882	20060.510903	29.944244
427.632113	20093.072222	29.949261
428.179999	20133.681912	29.954279
428.420555	20165.591322	29.959296
428.980302	20198.104763	29.964314
429.017352	20246.589854	29.969332
429.470567	20277.670601	29.974349
430.067861	20309.434078	29.979367
430.478549	20353.756947	29.984384
431.067328	20381.159011	29.989402
431.872378	20407.817885	29.994420
432.283401	20434.986119	29.999437
432.354248	20454.473433	30.004455
432.824004	20473.464066	30.009472
433.688251	20501.744655	30.014490
433.787786	20537.602770	30.019508
434.448436	20566.552248	30.024525
434.812107	20593.922037	30.029543
435.009841	20621.642781	30.034560
435.519670	20636.068139	30.039578
435.827574	20675.761786	30.044596
436.829552	20705.747887	30.049613
436.858293	20737.217711	30.054631
437.027400	20768.836918	30.059648
437.718065	20798.601882	30.064666
437.827479	20836.153916	30.069684
438.320063	20865.620583	30.074701
439.052058	20895.082237	30.079719
439.429438	20922.058211	30.084736
440.365870	20942.822668	30.089754
440.769668	20965.558226	30.094772
441.101460	21006.092377	30.099789
441.549519	21032.096452	30.104807
441.764840	21072.053933	30.109824
442.771385	21083.467667	30.114842
443.044297	21120.068937	30.119860
443.424496	21144.026094	30.124877
443.733166	21160.997122	30.129895
444.293992	21193.829846	30.134912
445.020149	21221.082330	30.139930
444.944212	21249.526672	30.144948
445.322564	21280.608733	30.149965
445.790648	21306.524225	30.154983
445.977656	21353.608995	30.160000
446.740149	21377.028322	30.165018
446.970263	21413.709550	30.170036
447.077678	21449.985905	30.175053
447.885226	21485.351391	30.180071
448.075526	21521.902174	30.185088
448.967869	21550.954382	30.190106
449.118318	21595.446651	30.195124
449.472532	21638.444018	30.200141
450.295004	21674.046980	30.205159
450.529114	21704.069125	30.210176
451.367647	21724.601339	30.215194
452.281702	21752.873102	30.220212
452.359954	21787.073252	30.225229
452.946741	21807.158159	30.230247
453.399545	21835.290907	30.235264
453.485857	21856.661438	30.240282
453.818930	21892.840636	30.245300
454.282192	21929.195288	30.250317
455.148245	21953.724469	30.255335
455.203175	21988.095742	30.260352
455.764558	22012.139556	30.265370
456.040236	22035.957988	30.270388
456.334570	22058.655858	30.275405
457.272196	22080.266748	30.280423
457.580668	22111.780592	30.285440
457.907417	22139.047896	30.290458
458.459245	22168.950207	30.295476
458.789715	22195.519971	30.300493
459.495972	22233.305523	30.305511
459.446729	22268.802977	30.310528
460.071790	22294.497391	30.315546
460.562918	22326.919050	30.320564
460.493897	22368.319214	30.325581
461.496600	22396.263746	30.330599
461.792128	22437.533546	30.335616
461.927767	22480.429404	30.340634
462.220165	22514.103945	30.345652
462.729949	22555.909380	30.350669
463.177680	22599.185887	30.355687
463.455889	22645.725949	30.360704
463.808331	22680.982319	30.365722
464.376285	22727.213384	30.370740
464.411345	22785.529343	30.375757
465.299916	22829.108012	30.380775
465.450658	22888.616541	30.385792
466.360646	22932.459887	30.390810
466.741278	22983.017430	30.395828
467.644993	23030.208816	30.400845
468.133228	23067.676648	30.405863
468.221978	23120.542517	30.410880
469.050936	23161.929282	30.415898
469.271829	23195.988442	30.420916
469.511086	23247.885550	30.425933
470.607652	23269.471964	30.430951
471.308312	23320.159971	30.435968
471.918135	23352.369474	30.440986
472.505115	23388.959036	30.446004
473.114523	23422.424312	30.451021
473.664561	23441.565635	30.456039
473.906638	23481.799047	30.461056
474.711064	23521.536521	30.466074
475.179813	23543.525018	30.471092
475.591620	23576.509314	30.476109
476.015146	23599.143910	30.481127
476.363926	23636.918871	30.486144
476.725439	23664.657452	30.491162
477.161529	23694.180146	30.496180
477.627834	23732.225694	30.501197
477.855628	23767.579166	30.506215
478.449808	23807.493425	30.511232
478.939533	23844.619414	30.516250
479.454212	23882.199171	30.521268
479.919717	23925.173980	30.526285
480.244976	23945.533284	30.531303
481.000156	23979.108057	30.536320
481.571859	24004.968927	30.541338
482.094909	24030.497300	30.546356
482.420486	24060.256476	30.551373
483.037623	24074.062141	30.556391
483.732823	24107.207983	30.561408
484.168440	24142.419685	30.566426
484.407910	24164.419575	30.571444
484.598925	24195.040149	30.576461
485.173887	24224.627565	30.581479
485.433565	24259.210594	30.586496
485.988145	24291.296890	30.591514
486.541896	24330.198797	30.596532
486.739043	24361.407146	30.601549
487.513193	24398.389072	30.606567
488.168184	24430.165040	30.611584
489.407851	24449.316663	30.616602
490.642775	24452.220483	30.621620
490.668108	24483.947989	30.626637
491.422541	24484.187046	30.631655
491.725155	24512.364228	30.636672
492.101259	24529.788165	30.641690
492.310304	24551.623285	30.646708
492.473516	24570.697622	30.651725
492.734212	24599.441717	30.656743
492.638546	24637.997248	30.661760
492.900543	24681.432686	30.666778
493.809967	24712.232844	30.671796
494.158094	24762.182045	30.676813
494.645065	24806.659623	30.681831
495.110519	24843.625591	30.686848
495.656224	24890.458879	30.691866
496.560024	24926.107402	30.696884
496.905603	24960.796429	30.701901
497.725704	24998.606666	30.706919
498.104254	25032.718682	30.711936
498.373589	25068.140890	30.716954
499.052507	25105.717849	30.721972
499.315374	25148.474574	30.726989
499.784621	25189.594637	30.732007
500.328998	25225.509847	30.737024
500.648919	25266.998153	30.742042
501.296078	25315.064354	30.747060
501.497633	25353.209514	30.752077
502.464430	25390.370237	30.757095
502.824285	25435.549667	30.762112
503.022364	25483.902192	30.767130
503.672209	25517.426087	30.772148
503.940987	25560.499659	30.777165
504.652088	25603.674620	30.782183
505.297372	25637.331054	30.787200
505.610647	25690.760498	30.792218
505.957864	25737.819317	30.797236
506.285372	25791.289369	30.802253
507.178287	25834.286306	30.807271
507.453412	25877.015446	30.812288
508.054248	25913.848086	30.817306
508.441798	25946.099816	30.822324
508.813823	25991.383649	30.827341
509.451355	26033.115615	30.832359
509.962133	26076.794872	30.837376
510.744187	26125.470687	30.842394
511.356252	26158.894013	30.847412
512.070896	26200.466808	30.852429
512.455643	26230.812247	30.857447
512.669165	26272.457969	30.862464
513.295314	26313.566158	30.867482
513.958063	26359.098572	30.872500
514.194458	26403.745761	30.877517
514.872204	26436.437549	30.882535
515.497151	26474.444653	30.887552
515.878200	26525.223683	30.892570
516.449713	26568.276938	30.897588
516.471996	26612.045708	30.902605
517.526800	26648.748628	30.907623
517.584299	26691.011954	30.912640
518.123278	26743.864539	30.917658
519.314595	26776.835254	30.922676
519.494328	26826.486803	30.927693
520.436694	26855.810203	30.932711
520.930659	26900.960567	30.937728
521.237869	26944.506795	30.942746
521.965088	26971.433357	30.947764
522.163049	27020.633521	30.952781
523.119433	27058.378849	30.957799
523.122160	27092.275414	30.962816
523.561548	27152.231239	30.967834
524.407879	27192.537643	30.972852
524.793225	27232.526798	30.977869
524.978190	27281.055407	30.982887
525.621769	27326.714154	30.987904
525.726823	27377.181346	30.992922
526.555346	27417.946542	30.997940
526.568939	27482.914569	31.002957
527.317203	27543.435613	31.007975
528.485078	27586.744046	31.012992
528.433485	27639.361149	31.018010
529.137233	27688.949205	31.023028
529.822929	27734.411725	31.028045
530.230181	27792.474641	31.033063
530.608102	27841.273592	31.038080
531.222886	27904.677324	31.043098
531.816096	27948.298880	31.048116
532.454049	27998.213525	31.053133
533.123219	28044.666008	31.058151
533.736599	28092.930252	31.063168
533.779288	28145.920054	31.068186
534.700263	28186.209168	31.073204
535.219141	28243.704378	31.078221
535.893365	28293.634642	31.083239
536.619411	28332.343085	31.088256
536.756609	28366.228771	31.093274
537.621321	28407.217619	31.098292
538.135733	28450.509544	31.103309
538.504545	28494.009152	31.108327
539.634676	28513.784313	31.113344
539.955007	28549.871057	31.118362
540.770546	28582.052787	31.123380
541.031067	28618.626699	31.128397
541.698341	28656.908763	31.133415
542.155667	28688.555235	31.138432
542.584666	28722.992443	31.143450
543.612823	28760.884756	31.148468
543.673071	28799.008555	31.153485
544.098048	28831.522471	31.158503
544.669475	28870.581463	31.163520
544.861520	28923.250586	31.168538
545.670854	28956.236182	31.173556
546.501040	29003.942249	31.178573
546.804800	29050.963263	31.183591
547.227458	29090.093758	31.188608
547.849034	29129.132776	31.193626
548.517431	29174.411403	31.198644
548.737130	29232.113782	31.203661
549.062452	29280.432167	31.208679
549.962687	29322.676846	31.213696
550.237885	29379.645973	31.218714
551.206307	29419.847072	31.223732
551.850090	29463.549745	31.228749
552.413553	29515.345274	31.233767
553.073859	29558.103146	31.238784
553.307020	29597.892277	31.243802
554.435086	29629.637042	31.248820
555.008859	29678.796425	31.253837
555.506427	29712.521919	31.258855
556.288712	29737.198550	31.263872
556.676435	29781.149316	31.268890
557.362166	29814.436869	31.273908
558.011880	29844.877684	31.278925
558.850896	29895.382344	31.283943
559.555829	29919.970710	31.288960
559.852000	29960.015455	31.293978
560.409036	29987.643950	31.298996
560.872102	30017.489143	31.304013
561.198488	30066.096518	31.309031
561.816741	30094.219767	31.314048
562.019220	30136.065493	31.319066
562.635094	30183.235481	31.324084
562.992047	30229.996102	31.329101
563.645946	30276.370712	31.334119
564.260919	30319.977828	31.339136
564.586799	30366.280433	31.344154
565.156579	30407.357554	31.349172
565.528171	30459.120443	31.354189
565.823375	30514.856291	31.359207
566.078198	30545.326636	31.364224
566.805467	30611.468484	31.369242
567.393178	30658.122649	31.374260
567.820101	30706.952322	31.379277
568.257294	30753.192584	31.384295
569.006439	30803.498442	31.389312
569.276726	30866.743189	31.394330
569.977680	30918.444034	31.399348
570.848135	30963.425928	31.404365
571.027984	31021.675259	31.409383
571.950548	31077.874187	31.414400
572.441535	31122.909078	31.419418
573.084626	31182.029285	31.424436
574.075924	31218.092285	31.429453
574.512276	31276.139321	31.434471
575.304110	31319.870661	31.439488
575.728605	31365.629220	31.444506
576.379377	31418.077266	31.449524
577.066681	31461.496218	31.454541
577.709554	31511.100874	31.459559
578.525691	31549.536240	31.464576
579.223971	31602.278353	31.469594
579.346678	31648.317461	31.474612
579.908622	31684.697331	31.479629
580.288108	31746.799533	31.484647
580.637718	31785.003977	31.489664
581.019202	31847.172437	31.494682
582.146834	31897.854817	31.499700
583.074283	31945.539794	31.504717
583.579973	32001.097416	31.509735
584.841967	32035.363216	31.514752
585.053076	32079.633560	31.519770
585.352800	32131.684269	31.524788
586.005620	32172.459405	31.529805
586.316600	32222.899293	31.534823
586.972719	32271.035094	31.539840
587.682328	32320.890062	31.544858
588.292329	32371.594872	31.549876
588.823219	32418.029800	31.554893
589.145321	32473.862570	31.559911
589.419950	32524.425810	31.564928
590.230157	32580.606788	31.569946
590.818975	32641.191030	31.574964
591.351779	32693.390807	31.579981
591.944043	32758.643826	31.584999
592.576764	32799.661730	31.590016
593.202124	32860.483702	31.595034
594.347278	32897.752233	31.600052
595.866027	32922.385735	31.605069
596.714079	32962.669879	31.610087
597.560031	32987.615551	31.615104
597.928316	33015.510923	31.620122
598.259055	33045.942278	31.625140
598.689307	33078.157976	31.630157
599.350883	33111.329966	31.635175
599.487356	33141.488211	31.640192
600.224529	33171.921272	31.645210
600.559010	33214.605001	31.650228
601.574232	33231.420258	31.655245
601.747534	33271.253028	31.660263
602.270418	33308.287416	31.665280
602.941201	33349.155602	31.670298
603.190487	33388.752714	31.675316
604.005815	33428.660160	31.680333
604.309326	33473.810146	31.685351
604.688362	33509.535888	31.690368
605.000204	33563.685704	31.695386
605.428894	33624.863382	31.700404
606.247563	33671.467227	31.705421
606.354446	33736.588594	31.710439
607.111789	33795.821347	31.715456
607.845515	33852.545332	31.720474
608.279420	33913.250328	31.725492
609.187249	33968.097887	31.730509
609.777757	34026.260868	31.735527
610.607368	34082.889973	31.740544
611.237269	34136.352560	31.745562
611.655593	34195.974929	31.750580
612.810714	34248.041082	31.755597
613.104339	34303.263437	31.760615
613.674831	34352.246545	31.765632
614.613118	34406.717089	31.770650
615.250229	34456.698808	31.775668
616.137865	34503.301887	31.780685
616.589275	34559.767419	31.785703
617.472547	34609.907449	31.790720
617.928695	34657.966952	31.795738
618.315823	34705.586720	31.800756
619.552142	34750.236910	31.805773
619.793360	34806.435647	31.810791
620.348417	34849.816770	31.815808
621.061745	34889.381386	31.820826
621.534057	34946.328873	31.825844
621.983233	34999.414704	31.830861
622.762864	35054.056095	31.835879
623.162161	35104.883215	31.840896
623.816377	35172.877368	31.845914
624.159030	35230.459731	31.850932
624.734914	35274.439289	31.855949
625.165107	35335.919390	31.860967
626.360482	35398.226925	31.865984
627.271051	35442.943463	31.871002
627.702063	35501.959938	31.876020
628.484989	35557.841604	31.881037
628.926999	35611.939503	31.886055
629.530153	35658.498101	31.891072
630.204444	35714.659298	31.896090
630.981593	35775.611220	31.901108
631.938331	35822.091893	31.906125
632.012364	35871.541624	31.911143
632.653133	35919.204859	31.916160
632.940720	35957.703099	31.921178
633.796305	36004.867280	31.926196
634.568164	36055.951696	31.931213
635.098299	36110.626812	31.936231
635.371325	36164.400248	31.941248
636.157979	36216.559610	31.946266
637.008684	36255.705128	31.951284
638.567520	36288.939221	31.956301
639.081889	36326.133026	31.961319
639.541133	36373.947862	31.966336
640.455382	36416.321998	31.971354
641.315395	36453.763754	31.976372
641.975576	36481.971608	31.981389
642.310167	36522.193213	31.986407
643.046804	36555.667559	31.991424
644.102540	36577.096148	31.996442
644.459699	36609.081204	32.001460
645.226635	36646.096755	32.006477
645.957850	36680.396796	32.011495
646.420691	36727.743805	32.016512
647.181821	36763.068800	32.021530
647.469541	36800.799549	32.026548
648.489569	36839.312459	32.031565
648.618265	36883.195599	32.036583
649.038444	36932.172359	32.041600
650.112653	36967.083718	32.046618
650.407731	37017.155934	32.051636
651.037490	37063.723658	32.056653
651.888535	37115.478240	32.061671
652.099369	37168.385002	32.066688
652.680910	37210.166109	32.071706
653.320387	37266.743253	32.076724
653.552003	37327.712002	32.081741
654.574555	37393.986774	32.086759
654.966500	37448.699285	32.091776
655.668428	37499.652595	32.096794
656.219119	37565.957458	32.101812
657.324697	37625.728554	32.106829
657.669173	37676.988444	32.111847
658.178115	37741.679764	32.116864
658.844941	37801.354214	32.121882
659.417887	37869.802676	32.126900
659.987144	37929.630293	32.131917
660.631266	37994.058231	32.136935
661.391018	38066.206785	32.141952
662.126629	38114.381472	32.146970
662.616012	38200.703128	32.151988
663.007193	38261.555224	32.157005
663.836913	38338.329551	32.162023
664.219367	38403.141300	32.167040
665.025746	38465.238334	32.172058
665.796722	38538.960766	32.177076
666.638787	38594.586081	32.182093
667.085019	38667.217588	32.187111
667.422282	38738.100706	32.192128
669.086303	38787.409859	32.197146
669.810049	38840.035179	32.202164
670.310567	38887.904174	32.207181
671.134017	38935.937910	32.212199
671.740173	38994.943449	32.217216
672.332077	39038.466695	32.222234
672.791879	39096.750038	32.227252
673.567046	39148.745266	32.232269
674.156631	39203.212783	32.237287
674.688362	39268.708928	32.242304
675.578239	39315.637229	32.247322
676.326077	39378.167954	32.252340
676.942011	39441.555667	32.257357
677.600514	39495.453348	32.262375
678.085055	39566.343272	32.267392
678.598852	39620.101967	32.272410
679.312294	39688.421850	32.277428
680.439725	39738.875756	32.282445
681.486144	39803.934043	32.287463
681.962033	39866.941944	32.292480
682.974217	39907.251351	32.297498
683.205438	39976.946997	32.302516
684.192126	40036.124211	32.307533
684.893264	40078.016347	32.312551
685.010642	40148.386833	32.317568
685.768038	40208.881649	32.322586
686.550481	40271.608840	32.327604
687.220752	40327.532112	32.332621
688.030351	40397.336076	32.337639
688.733930	40458.433292	32.342656
689.388576	40510.852425	32.347674
690.018559	40579.014116	32.352692
690.220418	40646.862611	32.357709
690.964287	40716.157929	32.362727
691.513744	40785.812504	32.367744
692.071082	40858.364683	32.372762
692.825549	40927.072513	32.377780
693.246201	41007.087532	32.382797
694.254454	41093.049458	32.387815
694.380791	41168.406177	32.392832
695.172215	41257.784661	32.397850
696.108033	41340.406523	32.402868
696.848944	41417.328711	32.407885
697.832553	41491.843817	32.412903
698.667737	41557.604787	32.417920
699.474896	41632.457709	32.422938
700.471455	41696.036044	32.427956
701.292660	41768.786620	32.432973
702.189524	41823.341303	32.437991
702.562418	41897.882864	32.443008
703.527335	41944.535176	32.448026
703.956489	42010.491852	32.453044
704.702401	42080.527295	32.458061
705.722654	42138.558274	32.463079
706.205723	42209.380504	32.468096
706.895450	42257.623090	32.473114
707.486480	42309.524766	32.478132
708.137314	42372.816829	32.483149
709.050360	42427.654743	32.488167
709.757337	42488.730253	32.493184
710.935327	42534.082191	32.498202
711.877828	42583.266450	32.503220
712.106567	42628.378633	32.508237
712.910308	42677.632571	32.513255
713.507445	42735.780247	32.518272
714.151094	42793.933331	32.523290
715.089513	42850.576027	32.528308
715.440375	42895.505433	32.533325
716.465068	42948.794178	32.538343
716.839087	43002.536829	32.543360
717.508048	43060.693090	32.548378
718.196229	43135.483158	32.553396
718.824750	43202.374756	32.558413
719.709641	43258.566759	32.563431
720.518763	43331.272225	32.568448
721.118898	43396.061881	32.573466
721.902967	43459.134821	32.578484
722.616894	43525.247518	32.583501
723.212075	43574.682328	32.588519
723.677396	43648.390227	32.593536
724.727259	43718.049532	32.598554
725.316231	43778.763528	32.603572
725.850839	43848.278261	32.608589
726.932322	43922.608472	32.613607
728.255459	43964.054579	32.618624
729.382516	44017.589001	32.623642
730.039602	44079.621305	32.628660
730.518793	44134.208781	32.633677
731.516719	44176.921717	32.638695
731.865148	44239.211940	32.643712
732.737200	44300.157147	32.648730
733.500342	44348.059481	32.653748
733.699490	44413.339504	32.658765
734.738757	44478.157926	32.663783
735.103267	44546.393324	32.668800
735.578523	44615.630339	32.673818
736.569522	44679.409822	32.678836
736.969692	44758.546350	32.683853
737.939710	44824.452862	32.688871
738.311368	44897.950666	32.693888
738.653914	44972.895159	32.698906
739.733301	45044.384867	32.703924
740.039400	45129.421786	32.708941
740.968475	45216.590413	32.713959
741.806532	45296.369504	32.718976
742.346484	45375.830452	32.723994
743.167772	45450.732323	32.729012
743.860732	45540.760629	32.734029
744.858367	45611.281343	32.739047
745.560254	45685.326161	32.744064
746.032019	45759.915874	32.749082
746.902018	45821.030779	32.754100
747.594539	45905.574562	32.759117
749.040583	45954.669283	32.764135
749.925680	46016.438704	32.769152
750.736979	46074.396228	32.774170
751.737822	46131.481381	32.779188
752.360990	46193.760068	32.784205
753.054230	46236.447688	32.789223
753.638284	46306.674218	32.794240
754.028752	46370.918312	32.799258
755.015636	46433.114705	32.804276
755.534182	46502.431167	32.809293
756.634216	46564.502740	32.814311
757.402943	46629.517349	32.819328
757.714494	46709.459260	32.824346
758.626177	46775.565407	32.829364
758.787572	46851.736249	32.834381
759.658038	46921.553642	32.839399
760.310100	47008.141091	32.844416
761.678195	47064.243194	32.849434
763.299031	47122.087923	32.854452
764.632402	47188.794238	32.859469
765.742193	47234.345999	32.864487
766.512634	47280.769103	32.869504
767.314428	47334.119371	32.874522
768.234583	47373.268174	32.879540
768.908221	47425.995456	32.884557
769.626062	47461.851037	32.889575
769.953537	47517.716379	32.894592
770.677009	47568.549308	32.899610
771.519764	47619.249804	32.904628
771.670656	47686.007416	32.909645
772.481555	47749.113652	32.914663
772.945701	47810.050819	32.919680
773.781971	47878.640568	32.924698
774.649362	47947.089950	32.929716
774.842074	48015.432436	32.934733
775.969489	48085.749947	32.939751
776.821361	48148.049623	32.944768
777.320686	48220.032719	32.949786
778.331887	48277.205230	32.954804
778.492527	48362.609081	32.959821
779.458136	48441.249340	32.964839
780.213569	48517.960723	32.969856
780.779916	48597.895856	32.974874
781.366051	48665.171626	32.979892
782.160463	48767.579159	32.984909
783.393138	48841.183550	32.989927
783.918669	48912.471074	32.994944
784.673715	49002.800637	32.999962
785.343573	49072.525931	33.004980
785.697212	49159.329187	33.009997
787.018820	49244.214816	33.015015
787.806693	49328.135006	33.020032
788.581436	49402.884364	33.025050
789.432441	49474.049747	33.030068
789.734628	49550.377017	33.035085
790.623155	49625.942283	33.040103
791.326253	49714.011666	33.045120
791.568536	49799.459900	33.050138
792.628644	49877.346732	33.055156
793.039901	49976.474033	33.060173
793.835367	50061.939602	33.065191
794.724797	50147.314885	33.070208
795.550393	50245.910676	33.075226
796.374802	50337.652887	33.080244
796.972391	50435.938886	33.085261
797.772732	50535.089395	33.090279
798.816951	50630.944835	33.095296
798.992733	50728.100371	33.100314
800.462593	50823.030699	33.105332
801.003771	50922.069966	33.110349
801.772524	51009.115928	33.115367
802.915009	51113.264577	33.120384
803.664975	51214.566560	33.125402
804.366705	51312.250625	33.130420
804.968580	51414.621921	33.135437
806.217006	51511.721408	33.140455
807.288111	51601.594042	33.145472
807.934656	51706.213257	33.150490
809.048093	51787.647253	33.155508
809.752459	51884.478725	33.160525
810.535092	51979.038529	33.165543
811.166214	52079.212337	33.170560
811.930491	52165.096860	33.175578
813.003913	52257.721347	33.180596
813.730725	52366.980548	33.185613
814.711710	52448.110376	33.190631
815.940889	52541.112353	33.195648
816.450395	52639.992516	33.200666
817.512732	52727.817500	33.205684
818.037587	52815.826305	33.210701
819.059012	52903.791215	33.215719
820.472713	52965.380692	33.220736
821.684033	53047.786381	33.225754
822.865040	53119.216687	33.230772
823.827624	53196.779936	33.235789
824.768574	53260.112172	33.240807
825.809026	53324.280989	33.245824
826.984360	53382.709362	33.250842
827.774805	53437.755660	33.255860
828.696746	53497.758700	33.260877
829.203826	53560.179433	33.265895
830.185022	53615.805081	33.270912
830.689365	53673.100754	33.275930
831.571443	53735.370867	33.280948
831.818806	53810.787479	33.285965
832.725089	53873.521356	33.290983
833.505586	53929.463986	33.296000
833.868862	54008.701135	33.301018
834.811792	54061.720742	33.306036
835.804199	54127.651859	33.311053
836.123319	54202.645181	33.316071
837.444211	54270.241631	33.321088
837.830631	54339.183366	33.326106
838.640635	54407.395084	33.331124
838.811738	54486.380815	33.336141
839.578429	54563.917953	33.341159
840.511748	54650.746921	33.346176
840.781379	54751.857905	33.351194
841.652128	54835.115048	33.356212
842.310855	54935.173961	33.361229
843.036583	55031.494838	33.366247
844.237716	55134.615620	33.371264
844.583140	55235.385769	33.376282
845.583083	55332.097040	33.381300
846.384930	55452.351065	33.386317
846.976784	55552.903808	33.391335
847.826062	55655.145992	33.396352
848.679961	55762.773347	33.401370
850.098024	55850.430517	33.406388
851.382876	55957.387490	33.411405
852.317781	56052.471411	33.416423
853.328451	56135.500694	33.421440
853.909879	56245.096713	33.426458
854.996829	56329.535287	33.431476
855.986617	56417.626364	33.436493
856.867087	56528.401320	33.441511
858.364461	56602.478234	33.446528
858.738275	56699.908793	33.451546
859.818348	56782.453266	33.456564
860.868192	56874.918721	33.461581
861.889256	56954.682664	33.466599
863.121323	57026.685229	33.471616
864.005040	57112.195210	33.476634
864.902854	57177.593589	33.481652
865.859701	57260.630202	33.486669
866.362971	57334.012742	33.491687
867.090020	57418.030570	33.496704
868.221238	57512.317322	33.501722
869.232394	57586.140937	33.506740
870.077564	57658.324354	33.511757
870.515925	57737.859246	33.516775
871.473478	57819.272381	33.521792
872.159692	57908.264981	33.526810
873.241257	57988.105843	33.531828
873.802634	58066.956425	33.536845
874.682169	58160.775086	33.541863
875.524655	58240.178360	33.546880
876.267391	58333.934426	33.551898
877.213469	58428.469993	33.556916
878.143129	58506.420868	33.561933
878.579511	58601.998215	33.566951
879.451794	58695.097734	33.571968
880.133319	58778.882711	33.576986
880.739088	58869.752322	33.582004
881.575665	58965.599355	33.587021
882.191856	59058.021592	33.592039
883.316168	59155.553991	33.597056
883.917413	59253.921582	33.602074
884.765273	59350.040323	33.607092
885.601378	59460.262074	33.612109
886.462678	59567.604118	33.617127
887.433403	59660.200244	33.622144
888.071540	59773.271717	33.627162
889.040595	59875.227666	33.632180
889.964456	59980.051987	33.637197
890.556948	60101.638799	33.642215
891.564978	60208.332838	33.647232
892.477184	60314.133380	33.652250
893.483319	60420.007981	33.657268
894.675124	60534.912537	33.662285
895.619062	60640.337283	33.667303
896.526063	60744.783343	33.672320
897.739989	60842.932318	33.677338
899.041835	60937.891287	33.682356
900.484458	61036.251170	33.687373
901.041459	61139.880471	33.692391
901.901925	61227.604425	33.697408
902.836195	61327.950782	33.702426
903.610413	61424.410801	33.707444
904.556735	61522.612224	33.712461
905.414873	61629.379235	33.717479
906.261402	61722.169498	33.722496
907.057858	61830.163179	33.727514
907.782862	61932.510164	33.732532
908.690031	62030.647833	33.737549
909.275272	62133.030775	33.742567
910.426509	62241.532433	33.747584
911.634067	62360.680230	33.752602
912.119202	62470.501802	33.757620
912.913995	62584.790468	33.762637
914.034593	62701.380593	33.767655
915.149320	62802.113426	33.772672
915.904868	62909.646090	33.777690
917.113184	63018.439958	33.782708
918.255021	63117.768034	33.787725
918.960851	63226.977800	33.792743
920.019030	63328.631920	33.797760
921.266270	63436.095635	33.802778
922.224960	63530.626436	33.807796
922.927449	63626.979603	33.812813
923.854194	63732.781184	33.817831
924.900185	63826.339515	33.822848
925.871777	63927.372683	33.827866
926.880583	64033.333410	33.832884
928.087549	64117.090088	33.837901
928.888154	64220.258475	33.842919
929.581544	64295.779157	33.847936
930.930692	64372.828554	33.852954
931.619390	64467.861738	33.857972
932.553032	64541.020747	33.862989
933.555496	64627.569300	33.868007
934.801337	64706.395597	33.873024
935.429452	64797.271223	33.878042
936.183608	64878.001919	33.883060
937.553454	64948.566490	33.888077
938.099811	65043.201974	33.893095
938.866261	65129.480841	33.898112
939.882363	65222.071696	33.903130
940.393022	65316.935289	33.908148
941.844119	65407.515463	33.913165
942.510127	65506.675859	33.918183
943.487839	65589.357413	33.923200
944.698957	65688.122489	33.928218
945.525005	65777.057286	33.933236
946.652346	65860.347874	33.938253
947.472768	65964.640565	33.943271
948.108797	66062.204119	33.948288
949.281156	66153.495433	33.953306
950.217564	66247.436770	33.958324
951.441955	66344.769163	33.963341
951.971517	66453.182052	33.968359
953.076696	66548.462469	33.973376
953.733537	66650.460232	33.978394
954.931971	66756.825902	33.983412
956.375810	66841.314835	33.988429
957.465548	66942.089224	33.993447
958.094688	67035.925358	33.998464
959.312027	67126.099133	34.003482
960.093293	67221.099593	34.008500
961.071420	67326.277904	34.013517
961.716061	67422.052842	34.018535
962.641409	67521.125458	34.023552
963.485457	67634.381376	34.028570
963.974724	67745.710738	34.033588
965.185170	67845.794654	34.038605
965.741364	67971.556332	34.043623
966.405404	68086.290225	34.048640
967.127899	68211.565812	34.053658
968.005523	68340.892373	34.058676
969.119231	68467.446689	34.063693
970.366385	68592.514891	34.068711
971.645550	68700.072401	34.073728
972.655557	68816.556090	34.078746
973.920114	68928.318489	34.083764
975.564018	69033.975012	34.088781
976.229863	69153.491163	34.093799
977.062085	69253.219186	34.098816
978.326472	69350.440237	34.103834
979.560827	69461.591333	34.108852
980.569914	69560.983202	34.113869
981.230180	69661.119739	34.118887
982.193249	69755.301226	34.123904
983.295776	69850.674050	34.128922
983.683291	69947.803808	34.133940
985.074087	70037.584368	34.138957
985.890065	70139.094877	34.143975
986.590902	70247.188853	34.148992
987.353801	70344.886350	34.154010
988.344590	70455.374179	34.159028
989.479011	70565.075260	34.164045
990.381961	70675.483524	34.169063
990.956102	70782.911894	34.174080
991.834640	70893.154663	34.179098
992.609947	71017.327717	34.184116
993.250679	71136.013229	34.189133
994.364738	71267.962582	34.194151
995.149761	71401.601676	34.199168
996.209624	71535.153715	34.204186
996.850366	71669.342014	34.209204
997.988321	71801.689196	34.214221
999.083540	71948.621426	34.219239
1000.335707	72090.721164	34.224256
1001.660518	72207.035801	34.229274
1002.461290	72356.539109	34.234292
1003.610763	72487.625250	34.239309
1004.539902	72617.376092	34.244327
1005.343643	72754.976983	34.249344
1006.379937	72889.060026	34.254362
1007.602196	73018.349786	34.259380
1009.055908	73156.336609	34.264397
1010.224356	73283.551331	34.269415
1011.052268	73421.765931	34.274432
1012.364552	73536.169275	34.279450
1013.076794	73666.258442	34.284468
1014.416789	73793.853553	34.289485
1015.521548	73906.111854	34.294503
1016.676006	74043.463593	34.299520
1018.049716	74160.931972	34.304538
1018.887462	74276.274482	34.309556
1020.156080	74394.999570	34.314573
1021.508037	74504.586650	34.319591
1022.369425	74621.324003	34.324608
1023.715174	74719.285181	34.329626
1024.521072	74848.861536	34.334644
1025.667394	74955.292352	34.339661
1026.772540	75062.160023	34.344679
1027.778402	75185.001485	34.349696
1029.115518	75275.060702	34.354714
1030.355623	75391.287241	34.359732
1031.353860	75485.446007	34.364749
1032.275041	75595.354027	34.369767
1033.060390	75702.238042	34.374784
1034.497289	75796.745591	34.379802
1034.920573	75919.892757	34.384820
1035.794332	76025.468812	34.389837
1036.747969	76132.113443	34.394855
1037.492026	76251.406908	34.399872
1038.269131	76352.240999	34.404890
1038.769479	76464.002954	34.409908
1040.106174	76584.006758	34.414925
1041.264853	76696.727062	34.419943
1041.830300	76812.133678	34.424960
1042.422206	76927.738988	34.429978
1043.267053	77072.245641	34.434996
1044.020598	77201.396614	34.440013
1045.135582	77336.375241	34.445031
1045.760149	77468.215647	34.450048
1047.310051	77612.993199	34.455066
1048.083003	77754.924700	34.460084
1049.378356	77896.198908	34.465101
1050.339759	78044.543150	34.470119
1051.297873	78187.965157	34.475136
1052.785575	78318.624498	34.480154
1053.726111	78468.877674	34.485172
1054.573407	78620.335098	34.490189
1056.520598	78754.640779	34.495207
1057.799138	78891.152249	34.500224
1059.170434	79022.890185	34.505242
1060.090815	79146.110447	34.510260
1061.118710	79284.339462	34.515277
1062.529829	79399.183646	34.520295
1063.272396	79538.338380	34.525312
1064.646479	79644.871229	34.530330
1065.981467	79779.666574	34.535348
1067.205063	79899.777326	34.540365
1068.681858	80006.959436	34.545383
1069.752527	80128.840514	34.550400
1071.310687	80242.344849	34.555418
1072.807193	80344.531720	34.560436
1074.114926	80431.489271	34.565453
1075.203157	80528.691201	34.570471
1075.935705	80645.951252	34.575488
1077.356347	80742.279518	34.580506
1077.991995	80847.058537	34.585524
1078.592503	80948.670255	34.590541
1080.130487	81056.954339	34.595559
1081.170962	81152.820289	34.600576
1082.052058	81261.424860	34.605594
1082.795221	81385.603274	34.610612
1084.061112	81493.338672	34.615629
1084.770254	81605.847601	34.620647
1085.610083	81736.100571	34.625664
1086.696145	81845.421551	34.630682
1087.587195	81978.683396	34.635700
1088.226198	82105.120594	34.640717
1089.730827	82231.882370	34.645735
1091.326799	82354.811913	34.650752
1092.336908	82473.890427	34.655770
1093.425846	82591.964519	34.660788
1094.326659	82713.609564	34.665805
1095.616714	82825.210776	34.670823
1095.791193	82950.588974	34.675840
1097.035587	83065.675911	34.680858
1098.053432	83180.546625	34.685876
1098.515233	83306.469207	34.690893
1099.973631	83430.305726	34.695911
1100.773411	83562.498380	34.700928
1101.791184	83691.786830	34.705946
1102.571899	83834.283374	34.710964
1103.615957	83977.093052	34.715981
1104.773115	84104.806534	34.720999
1105.622885	84258.656492	34.726016
1106.880630	84390.870001	34.731034
1107.969655	84544.974823	34.736052
1108.720460	84690.067839	34.741069
1110.080970	84842.108383	34.746087
1110.787599	85000.829692	34.751104
1112.093274	85148.556378	34.756122
1113.248176	85313.297589	34.761140
1114.432089	85468.203338	34.766157
1115.845516	85612.097068	34.771175
1117.080351	85766.781908	34.776192
1118.439525	85909.206691	34.781210
1119.418422	86060.418756	34.786228
1120.518587	86210.221516	34.791245
1121.839438	86362.399353	34.796263
1122.760006	86522.033774	34.801280
1123.716370	86666.513154	34.806298
1125.154801	86824.777521	34.811316
1125.991605	86981.753926	34.816333
1127.592539	87130.123947	34.821351
1128.663098	87282.107826	34.826368
1130.041261	87435.650021	34.831386
1131.252688	87585.710269	34.836404
1132.044968	87743.856517	34.841421
1133.657641	87886.342636	34.846439
1134.924190	88021.783275	34.851456
1136.336987	88158.927874	34.856474
1137.613391	88309.868141	34.861492
1138.769264	88444.361499	34.866509
1139.975489	88577.007452	34.871527
1140.937513	88729.246433	34.876544
1142.537663	88859.251329	34.881562
1143.889641	88984.477632	34.886580
1144.871395	89119.894547	34.891597
1146.137397	89251.377830	34.896615
1147.163547	89392.746606	34.901632
1148.338280	89524.853166	34.906650
1149.697955	89656.501075	34.911668
1150.940116	89789.445951	34.916685
1152.167485	89920.009762	34.921703
1153.117660	90046.931402	34.926720
1154.272038	90177.090959	34.931738
1155.829180	90303.044809	34.936756
1156.890121	90442.688316	34.941773
1157.802413	90556.350433	34.946791
1159.022454	90673.309821	34.951808
1159.816356	90783.380695	34.956826
1160.625388	90900.931589	34.961844
1161.625311	91033.220529	34.966861
1163.129982	91146.386729	34.971879
1163.705168	91285.783974	34.976896
1164.680018	91420.741891	34.981914
1166.193167	91552.756276	34.986932
1166.765648	91693.174801	34.991949
1167.727939	91832.931377	34.996967
1168.580564	91980.049371	35.001984
1169.508482	92137.168601	35.007002
1170.999818	92291.157077	35.012020
1171.883256	92439.392732	35.017037
1173.633027	92601.381262	35.022055
1174.537208	92761.645888	35.027072
1175.305130	92910.617791	35.032090
1176.736983	93063.640710	35.037108
1178.190972	93233.403853	35.042125
1179.536051	93390.149363	35.047143
1180.636324	93544.347881	35.052160
1181.886949	93688.523274	35.057178
1183.193696	93841.988911	35.062196
1184.327226	94002.928115	35.067213
1185.619859	94161.066318	35.072231
1186.739160	94320.643781	35.077248
1187.941092	94471.062555	35.082266
1189.592761	94631.266034	35.087284
1190.357050	94785.273518	35.092301
1191.885007	94946.207388	35.097319
1193.046774	95099.856519	35.102336
1194.281119	95247.795678	35.107354
1195.423967	95394.776191	35.112372
1196.199709	95562.514098	35.117389
1198.224520	95716.586877	35.122407
1199.271721	95875.756692	35.127424
1200.394679	96030.607613	35.132442
1201.754276	96178.140753	35.137460
1202.945149	96351.745962	35.142477
1204.539990	96489.767329	35.147495
1205.586867	96650.131948	35.152512
1206.770369	96792.769049	35.157530
1208.451681	96934.505484	35.162548
1209.428867	97090.057404	35.167565
1211.326689	97225.251527	35.172583
1212.299935	97368.191378	35.177600
1213.306433	97522.817953	35.182618
1214.698376	97655.691057	35.187636
1215.941095	97807.409816	35.192653
1217.294194	97953.880033	35.197671
1218.195053	98093.002089	35.202688
1219.376677	98248.598998	35.207706
1220.620367	98369.751407	35.212724
1221.678030	98526.401149	35.217741
1222.840245	98669.255827	35.222759
1223.983517	98805.452374	35.227776
1225.284320	98935.095473	35.232794
1226.879530	99054.993530	35.237812
1227.887796	99185.405809	35.242829
1229.255658	99310.326883	35.247847
1230.220651	99439.924994	35.252864
1231.120931	99581.934901	35.257882
1232.387966	99717.547748	35.262900
1233.431489	99862.883575	35.267917
1235.080875	99998.298084	35.272935
1236.265508	100132.205513	35.277952
1237.222047	100287.731788	35.282970
1238.354389	100428.280069	35.287988
1239.590945	100579.151279	35.293005
1240.566049	100725.212045	35.298023
1241.670169	100881.256650	35.303040
1242.866230	101039.533886	35.308058
1244.393703	101196.607925	35.313076
1245.303909	101358.501416	35.318093
1246.497514	101511.865854	35.323111
1247.724870	101673.078358	35.328128
1248.404085	101847.939052	35.333146
1250.105208	102005.206066	35.338164
1251.386985	102177.132332	35.343181
1252.643000	102340.312775	35.348199
1254.212086	102496.597985	35.353216
1255.336604	102672.210308	35.358234
1257.096139	102843.546626	35.363252
1257.691113	103006.457129	35.368269
1258.919288	103167.224174	35.373287
1260.578656	103340.794806	35.378304
1261.505796	103514.470474	35.383322
1263.307481	103673.605763	35.388340
1264.820133	103845.450568	35.393357
1265.914179	104015.236923	35.398375
1266.941284	104172.853407	35.403392
1268.660688	104348.130501	35.408410
1270.404297	104501.667469	35.413428
1271.570517	104666.479332	35.418445
1273.183426	104815.090376	35.423463
1274.660899	104978.336117	35.428480
1275.500770	105131.052588	35.433498
1276.595174	105287.406409	35.438516
1277.712204	105456.680475	35.443533
1279.087528	105613.972694	35.448551
1280.336100	105775.830032	35.453568
1281.732620	105942.651911	35.458586
1282.903755	106104.530111	35.463604
1283.409034	106272.540206	35.468621
1284.664630	106448.039376	35.473639
1286.291090	106624.189697	35.478656
1287.013414	106802.390033	35.483674
1288.610659	106973.800911	35.488692
1290.021740	107157.204332	35.493709
1291.269383	107321.262049	35.498727
1292.594792	107485.492060	35.503744
1293.349299	107641.693728	35.508762
1295.005768	107794.284654	35.513780
1296.416244	107962.574009	35.518797
1297.820836	108128.624927	35.523815
1299.363070	108274.306553	35.528832
1300.649541	108429.359084	35.533850
1301.848039	108588.559644	35.538868
1303.117125	108758.193492	35.543885
1303.994984	108910.794956	35.548903
1305.673916	109077.384719	35.553920
1306.954952	109251.330459	35.558938
1308.151246	109405.270555	35.563956
1309.533529	109585.456168	35.568973
1310.441779	109759.774934	35.573991
1311.535922	109925.703883	35.579008
1312.439219	110106.931581	35.584026
1313.951650	110301.153754	35.589044
1315.533389	110482.308020	35.594061
1316.839198	110658.627155	35.599079
1318.175762	110834.328661	35.604096
1319.199401	111025.830097	35.609114
1320.717482	111212.241053	35.614132
1322.189391	111394.729789	35.619149
1323.303979	111587.607398	35.624167
1324.719498	111766.145189	35.629184
1326.236190	111958.493332	35.634202
1327.956319	112130.205681	35.639220
1329.455631	112315.406177	35.644237
1331.353193	112485.434240	35.649255
1333.348208	112652.573985	35.654272
1334.775253	112813.202509	35.659290
1336.876594	112964.672335	35.664308
1337.800109	113115.564313	35.669325
1338.916935	113271.731456	35.674343
1340.554625	113435.685680	35.679360
1341.744699	113600.174261	35.684378
1343.095438	113754.813207	35.689396
1344.210830	113913.225623	35.694413
1345.330286	114065.497580	35.699431
1346.554115	114234.821627	35.704448
1347.737519	114397.702136	35.709466
1349.113425	114575.190039	35.714484
1350.270725	114740.387671	35.719501
1351.175198	114924.638392	35.724519
1352.538471	115082.189391	35.729536
1353.585408	115280.468512	35.734554
1355.344833	115460.934230	35.739572
1356.658090	115639.667779	35.744589
1358.188930	115815.531637	35.749607
1359.316724	115995.126544	35.754624
1360.507028	116184.399603	35.759642
1361.922138	116361.108685	35.764660
1363.490379	116536.939917	35.769677
1364.460994	116721.781946	35.774695
1366.012457	116897.611992	35.779712
1367.065631	117079.790609	35.784730
1368.324205	117248.375749	35.789748
1369.567518	117417.116379	35.794765
1370.789196	117592.560392	35.799783
1373.048575	117757.133852	35.804800
1374.212992	117939.237558	35.809818
1375.469291	118100.198951	35.814836
1376.861718	118274.879656	35.819853
1378.158945	118447.810094	35.824871
1379.734128	118619.032233	35.829888
1381.235548	118797.036027	35.834906
1382.814641	118961.149080	35.839924
1383.910397	119138.067274	35.844941
1385.551019	119321.479050	35.849959
1386.934055	119486.329434	35.854976
1388.298911	119668.806013	35.859994
1389.839772	119835.678796	35.865012
1391.230626	120018.584274	35.870029
1392.275230	120201.039482	35.875047
1393.681250	120379.651814	35.880064
1395.304236	120562.638180	35.885082
1396.431606	120744.653417	35.890100
1398.023306	120913.576675	35.895117
1399.040400	121107.352242	35.900135
1400.438198	121294.191628	35.905152
1401.924019	121486.894955	35.910170
1403.571590	121670.708348	35.915188
1405.192139	121843.913815	35.920205
1406.647820	122056.890526	35.925223
1407.865418	122242.815351	35.930240
1409.181249	122428.459889	35.935258
1410.554446	122617.946961	35.940276
1412.043780	122807.378927	35.945293
1413.697410	122992.783732	35.950311
1415.632837	123161.464052	35.955328
1417.107098	123347.723113	35.960346
1418.614783	123525.010582	35.965364
1420.727605	123697.263259	35.970381
1422.120554	123871.316055	35.975399
1423.540650	124040.932457	35.980416
1425.167718	124218.332204	35.985434
1426.037640	124394.282802	35.990452
1427.812051	124556.094263	35.995469
1428.635247	124736.361147	36.000487
1430.268660	124896.791064	36.005504
1431.556972	125074.148944	36.010522
1432.423565	125269.511311	36.015540
1434.019199	125451.205567	36.020557
1435.006529	125643.308694	36.025575
1436.354056	125826.754944	36.030592
1438.180593	126019.842080	36.035610
1439.269636	126214.542528	36.040628
1440.620819	126408.683344	36.045645
1441.873089	126597.305558	36.050663
1443.123818	126782.686415	36.055680
1444.265879	126969.859270	36.060698
1445.614244	127164.005893	36.065716
1447.826266	127340.826373	36.070733
1448.603340	127520.320927	36.075751
1450.007787	127715.982690	36.080768
1451.521000	127907.891467	36.085786
1452.514234	128103.710003	36.090804
1454.173217	128304.212747	36.095821
1455.402794	128504.430465	36.100839
1456.961068	128702.152383	36.105856
1458.592500	128914.027542	36.110874
1459.760828	129121.936601	36.115892
1461.049396	129329.853445	36.120909
1462.339813	129555.507943	36.125927
1463.915821	129763.179640	36.130944
1465.557240	129980.584986	36.135962
1467.078201	130196.490864	36.140980
1468.557944	130410.833968	36.145997
1469.852588	130624.612661	36.151015
1471.590488	130830.264786	36.156032
1473.035845	131064.458678	36.161050
1474.547769	131290.472017	36.166068
1476.283117	131503.199116	36.171085
1477.390297	131728.786151	36.176103
1479.136831	131938.930100	36.181120
1480.579998	132166.633789	36.186138
1482.017670	132393.985411	36.191156
1483.623395	132620.450569	36.196173
1484.841426	132847.954744	36.201191
1486.441257	133067.240305	36.206208
1488.430120	133298.464727	36.211226
1489.741764	133527.239152	36.216244
1491.834087	133734.249750	36.221261
1493.352530	133956.342604	36.226279
1495.072100	134176.593273	36.231296
1496.838936	134381.860978	36.236314
1497.959983	134596.685393	36.241332
1500.006006	134800.049058	36.246349
1501.749971	135006.490583	36.251367
1503.314950	135200.556745	36.256384
1504.836772	135399.712313	36.261402
1506.470822	135613.575749	36.266420
1508.311801	135801.912549	36.271437
1509.829525	135999.286170	36.276455
1511.391931	136209.224454	36.281472
1512.769851	136390.833866	36.286490
1514.106118	136594.525588	36.291508
1515.686258	136792.604272	36.296525
1517.114093	137008.132691	36.301543
1518.497958	137198.249166	36.306560
1519.999062	137396.116370	36.311578
1521.102499	137608.101777	36.316596
1522.932790	137806.122186	36.321613
1524.414948	138009.141536	36.326631
1525.732648	138195.131003	36.331648
1527.810077	138378.973295	36.336666
1528.766373	138565.808210	36.341684
1530.276119	138747.664632	36.346701
1531.285735	138947.052305	36.351719
1532.713309	139133.397693	36.356736
1534.565492	139322.148047	36.361754
1535.773832	139532.787146	36.366772
1537.383471	139730.766699	36.371789
1538.746183	139932.132561	36.376807
1540.490445	140133.984115	36.381824
1542.104645	140332.613254	36.386842
1543.218987	140537.723303	36.391860
1545.300192	140749.258810	36.396877
1546.734354	140958.845431	36.401895
1547.924957	141174.771128	36.406912
1549.734469	141380.612924	36.411930
1550.989012	141601.119481	36.416948
1552.710153	141798.448482	36.421965
1554.699118	142010.615792	36.426983
1556.278903	142226.829326	36.432000
1558.136556	142430.224412	36.437018
1559.633075	142649.470674	36.442036
1560.984075	142852.163227	36.447053
1562.739122	143064.286274	36.452071
1564.317872	143270.405593	36.457088
1565.956785	143486.200331	36.462106
1567.191403	143711.021997	36.467124
1568.980139	143922.638593	36.472141
1570.633720	144136.217400	36.477159
1572.055188	144349.314866	36.482176
1573.254618	144561.587141	36.487194
1574.921688	144791.532131	36.492212
1576.813963	145007.614080	36.497229
1578.022126	145235.353648	36.502247
1579.704687	145461.840674	36.507264
1581.376025	145685.453720	36.512282
1582.791256	145908.817496	36.517300
1584.263279	146143.239933	36.522317
1586.054964	146370.058414	36.527335
1587.317432	146591.587912	36.532352
1589.206018	146819.775925	36.537370
1590.527737	147053.024738	36.542388
1592.385031	147280.777366	36.547405
1593.876286	147518.604196	36.552423
1595.027591	147756.829068	36.557440
1596.924792	147997.662719	36.562458
1598.772135	148231.305692	36.567476
1600.345396	148463.257174	36.572493
1601.946134	148687.219483	36.577511
1603.456503	148933.610726	36.582528
1605.178218	149169.777854	36.587546
1606.915406	149410.546087	36.592564
1608.859688	149631.988322	36.597581
1610.253880	149856.600057	36.602599
1611.398577	150080.188064	36.607616
1613.104734	150289.679693	36.612634
1614.530690	150504.833381	36.617652
1616.378222	150720.542733	36.622669
1617.806524	150937.803405	36.627687
1619.002446	151159.831289	36.632704
1620.690833	151373.376938	36.637722
1622.221716	151610.213280	36.642740
1624.057714	151834.235934	36.647757
1625.580713	152070.633098	36.652775
1627.150072	152308.406529	36.657792
1628.936848	152532.416373	36.662810
1630.751435	152769.735772	36.667828
1632.141867	153011.016571	36.672845
1633.766424	153231.278657	36.677863
1634.958170	153476.068340	36.682880
1636.977171	153712.601250	36.687898
1638.526260	153957.033396	36.692916
1640.195959	154199.926675	36.697933
1641.517918	154448.620600	36.702951
1643.346447	154709.306559	36.707968
1645.404968	154934.734744	36.712986
1647.167670	155176.948273	36.718004
1648.821683	155421.374352	36.723021
1650.921011	155668.546337	36.728039
1652.437171	155910.842288	36.733056
1654.114918	156140.586649	36.738074
1655.697926	156389.380110	36.743092
1657.190731	156624.812323	36.748109
1659.031866	156873.606337	36.753127
1660.696878	157115.937878	36.758144
1662.937105	157357.913482	36.763162
1664.363726	157603.469047	36.768180
1665.908096	157844.379295	36.773197
1667.715002	158078.604930	36.778215
1669.313123	158329.058425	36.783232
1671.228396	158565.438508	36.788250
1673.060279	158819.231458	36.793268
1674.592165	159066.771499	36.798285
1676.163762	159305.240095	36.803303
1677.739829	159546.309211	36.808320
1679.783388	159780.331114	36.813338
1681.433075	160033.236038	36.818356
1683.240324	160271.026996	36.823373
1684.928115	160509.244324	36.828391
1686.567643	160750.869547	36.833408
1688.568572	160985.552932	36.838426
1689.936452	161241.478689	36.843444
1691.681682	161476.890717	36.848461
1693.152036	161707.782491	36.853479
1694.709959	161961.730209	36.858496
1696.809782	162203.736005	36.863514
1698.273914	162447.886188	36.868532
1699.909019	162701.471757	36.873549
1701.596231	162937.181543	36.878567
1702.721442	163181.682181	36.883584
1704.389900	163397.905203	36.888602
1705.841221	163640.429405	36.893620
1707.786941	163871.411666	36.898637
1709.171219	164117.158362	36.903655
1710.752326	164360.592555	36.908672
1712.658845	164588.795355	36.913690
1714.287810	164843.259185	36.918708
1715.705377	165095.995402	36.923725
1717.340489	165338.717221	36.928743
1718.379708	165597.249678	36.933760
1720.583575	165852.922826	36.938778
1722.062911	166116.221310	36.943796
1723.776199	166383.289524	36.948813
1726.535017	166642.431310	36.953831
1728.256331	166899.925879	36.958848
1730.724784	167140.624530	36.963866
1732.508968	167384.566261	36.968884
1734.074310	167636.776129	36.973901
1736.292099	167875.515215	36.978919
1738.053269	168122.052866	36.983936
1739.618089	168362.699823	36.988954
1741.187930	168612.594255	36.993972
1742.952142	168860.861240	36.998989
1744.569310	169109.521026	37.004007
1746.393591	169357.198202	37.009024
1748.137135	169605.739651	37.014042
1749.956541	169869.606308	37.019060
1751.444272	170126.969455	37.024077
1753.099823	170378.713685	37.029095
1754.520093	170644.881500	37.034112
1756.420884	170911.456859	37.039130
1758.262816	171181.265372	37.044148
1759.331963	171454.217494	37.049165
1761.305006	171722.359842	37.054183
1763.018849	172006.883797	37.059200
1765.023359	172277.917163	37.064218
1767.033295	172556.981410	37.069236
1768.614128	172839.375928	37.074253
1770.360559	173113.322897	37.079271
1772.087635	173385.473445	37.084288
1773.798229	173662.068486	37.089306
1775.659996	173947.724522	37.094324
1777.190259	174242.099739	37.099341
1779.296007	174511.546405	37.104359
1780.920555	174804.616762	37.109376
1782.303581	175080.981732	37.114394
1784.237602	175365.811680	37.119412
1785.940773	175647.686268	37.124429
1787.888346	175943.859743	37.129447
1789.976365	176228.607801	37.134464
1792.011101	176503.762466	37.139482
1794.081510	176791.612751	37.144500
1795.821275	177069.989700	37.149517
1798.118029	177327.904865	37.154535
1800.193453	177575.275799	37.159552
1802.238304	177808.557706	37.164570
1804.379754	178037.029835	37.169588
1806.494870	178259.950388	37.174605
1809.068408	178475.935528	37.179623
1810.717715	178700.936957	37.184640
1812.382437	178917.576131	37.189658
1814.424037	179132.393022	37.194676
1815.856599	179349.883258	37.199693
1817.762331	179564.292524	37.204711
1819.418280	179791.874259	37.209728
1820.976011	180016.808372	37.214746
1823.031493	180248.211552	37.219764
1824.313163	180478.140150	37.224781
1826.324974	180704.718639	37.229799
1827.708161	180944.860086	37.234816
1829.835304	181183.197247	37.239834
1831.154312	181427.741630	37.244852
1832.964875	181672.602687	37.249869
1834.678202	181930.777886	37.254887
1836.060836	182203.078507	37.259904
1837.260644	182471.209961	37.264922
1839.434321	182732.197068	37.269940
1841.089787	183015.828321	37.274957
1842.873651	183288.896707	37.279975
1844.359209	183575.629169	37.284992
1846.245390	183854.623125	37.290010
1848.126830	184134.609310	37.295028
1849.459004	184428.109402	37.300045
1851.703444	184710.668177	37.305063
1853.758823	185005.985969	37.310080
1855.415461	185293.133658	37.315098
1857.388823	185577.491988	37.320116
1859.213618	185875.592928	37.325133
1861.659978	186163.673961	37.330151
1863.973302	186446.346785	37.335168
1865.790704	186733.972891	37.340186
1867.702891	187018.349860	37.345204
1869.334158	187301.821431	37.350221
1871.698764	187581.231771	37.355239
1873.239216	187870.786982	37.360256
1874.762389	188156.615855	37.365274
1876.796627	188451.502227	37.370292
1878.155878	188743.769192	37.375309
1880.309954	189044.909205	37.380327
1881.910455	189339.083161	37.385344
1883.868557	189629.128544	37.390362
1885.616064	189941.404815	37.395380
1887.575719	190256.009896	37.400397
1889.632922	190551.984330	37.405415
1891.579543	190851.506157	37.410432
1893.409676	191152.292026	37.415450
1895.360692	191455.852567	37.420468
1897.224809	191759.504934	37.425485
1899.323782	192047.334222	37.430503
1901.077968	192334.864569	37.435520
1902.559811	192615.865769	37.440538
1904.455041	192889.391245	37.445556
1906.275808	193178.464256	37.450573
1908.433408	193459.426429	37.455591
1910.258892	193745.811394	37.460608
1911.837103	194038.189583	37.465626
1914.063678	194323.346552	37.470644
1915.880214	194611.565453	37.475661
1917.486410	194913.437659	37.480679
1919.561514	195200.527366	37.485696
1921.050000	195497.395730	37.490714
1923.228537	195794.448208	37.495732
1925.301642	196112.169147	37.500749
1927.362649	196412.708776	37.505767
1929.125419	196720.925506	37.510784
1930.792291	197031.596201	37.515802
1933.064023	197342.451975	37.520820
1934.801446	197661.746024	37.525837
1936.680975	197970.433878	37.530855
1938.464423	198298.698087	37.535872
1940.534724	198609.834439	37.540890
1942.386283	198923.596641	37.545908
1944.306095	199249.433423	37.550925
1946.472944	199559.836471	37.555943
1948.524927	199890.822161	37.560960
1951.031196	200214.388489	37.565978
1953.988635	200505.961911	37.570996
1956.467904	200801.953845	37.576013
1958.870097	201091.232175	37.581031
1961.044264	201382.820314	37.586048
1963.070830	201663.440930	37.591066
1965.579896	201938.274336	37.596084
1967.417208	202223.649772	37.601101
1969.474586	202488.326584	37.606119
1971.433957	202769.229974	37.611136
1972.930316	203054.536789	37.616154
1974.849649	203326.284440	37.621172
1976.576075	203618.221803	37.626189
1978.617121	203897.264506	37.631207
1980.379151	204185.898698	37.636224
1982.002175	204482.947141	37.641242
1984.394751	204768.196431	37.646260
1985.923513	205070.822850	37.651277
1987.932973	205363.003383	37.656295
1989.834115	205661.422757	37.661312
1992.055899	205953.483675	37.666330
1994.162866	206262.257398	37.671348
1995.982015	206558.955177	37.676365
1998.028136	206845.158121	37.681383
2000.035398	207153.457192	37.686400
2001.655568	207460.854470	37.691418
2003.840103	207767.224348	37.696436
2005.711833	208068.757914	37.701453
2007.317396	208369.687765	37.706471
2009.438344	208657.055320	37.711488
2011.003733	208942.138410	37.716506
2013.043028	209222.209252	37.721524
2014.812196	209513.280077	37.726541
2016.799419	209801.791327	37.731559
2018.727704	210103.478182	37.736576
2020.841298	210403.537477	37.741594
2022.769527	210694.791663	37.746612
2024.696540	211016.033872	37.751629
2026.337787	211310.116696	37.756647
2028.845700	211607.364187	37.761664
2031.067807	211922.482969	37.766682
2033.052252	212231.839092	37.771700
2034.932898	212539.283410	37.776717
2036.883229	212856.087576	37.781735
2038.755877	213181.361002	37.786752
2040.359712	213513.686798	37.791770
2042.789151	213832.222439	37.796788
2045.402374	214148.394379	37.801805
2047.271488	214469.231054	37.806823
2049.714011	214789.381561	37.811840
2051.627005	215110.658679	37.816858
2053.727670	215434.916541	37.821876
2055.385824	215770.812464	37.826893
2057.365097	216090.483920	37.831911
2059.729003	216425.128376	37.836928
2061.370642	216765.564352	37.841946
2063.586237	217097.696260	37.846964
2065.586325	217440.998835	37.851981
2067.516306	217783.768235	37.856999
2069.591622	218124.992615	37.862016
2071.639544	218466.553078	37.867034
2073.857901	218806.653371	37.872052
2076.028436	219162.430813	37.877069
2078.219717	219508.696670	37.882087
2080.537157	219836.901679	37.887104
2082.379907	220194.145473	37.892122
2084.547373	220545.435294	37.897140
2086.929352	220887.855481	37.902157
2089.085659	221224.942085	37.907175
2091.474163	221623.829247	37.912192
2093.462949	221968.094297	37.917210
2095.748031	222309.533142	37.922228
2097.760115	222654.216563	37.927245
2099.605622	222995.194854	37.932263
2102.168050	223331.426270	37.937280
2103.867757	223688.493141	37.942298
2106.329609	224016.680407	37.947316
2108.672574	224356.379345	37.952333
2111.263057	224690.999417	37.957351
2113.910497	225015.631316	37.962368
2115.864484	225337.580967	37.967386
2118.470348	225659.745919	37.972404
2120.340041	225969.559460	37.977421
2122.434555	226279.947996	37.982439
2124.272552	226575.394615	37.987456
2125.799270	226885.113562	37.992474
2128.117331	227175.000523	37.997492
2130.155112	227481.567607	38.002509
2131.901323	227791.280413	38.007527
2133.931472	228092.009668	38.012544
2135.424975	228410.374224	38.017562
2137.256255	228735.670480	38.022580
2139.372078	229061.710102	38.027597
2141.453079	229391.819963	38.032615
2143.478200	229727.908222	38.037632
2145.525753	230074.432422	38.042650
2147.406484	230414.406500	38.047668
2149.662290	230764.862261	38.052685
2151.593906	231111.586546	38.057703
2153.773588	231459.999808	38.062720
2156.167105	231818.234742	38.067738
2158.463720	232160.231827	38.072756
2160.843499	232508.794991	38.077773
2162.566206	232871.051541	38.082791
2165.209651	233222.775600	38.087808
2167.254587	233592.577735	38.092826
2169.462709	233943.332091	38.097844
2171.839321	234305.769585	38.102861
2174.066892	234670.314693	38.107879
2176.188959	235029.747345	38.112896
2178.508584	235378.711103	38.117914
2180.959984	235751.250512	38.122932
2183.535614	236108.176704	38.127949
2185.578702	236462.496290	38.132967
2187.959745	236820.573297	38.137984
2190.383031	237189.109198	38.143002
2192.753186	237534.439995	38.148020
2194.919639	237883.385476	38.153037
2196.657507	238252.186061	38.158055
2199.202768	238603.105668	38.163072
2201.053492	238962.315137	38.168090
2203.175637	239324.225841	38.173108
2205.286154	239688.806486	38.178125
2207.764227	240058.638514	38.183143
2209.955705	240422.599020	38.188160
2211.687897	240794.710626	38.193178
2213.749483	241165.501153	38.198196
2216.086586	241545.342313	38.203213
2217.829946	241928.809421	38.208231
2220.290602	242299.159087	38.213248
2222.611240	242685.381787	38.218266
2224.158611	243074.547723	38.223284
2226.992988	243462.291519	38.228301
2229.209998	243860.015150	38.233319
2231.277235	244237.087710	38.238336
2233.608438	244629.512233	38.243354
2235.926842	245015.132548	38.248372
2238.444418	245404.862686	38.253389
2240.392834	245785.844696	38.258407
2242.880744	246144.364020	38.263424
2245.013145	246501.238762	38.268442
2247.439384	246850.142683	38.273460
2249.999968	247201.337632	38.278477
2252.003268	247556.990780	38.283495
2254.047648	247901.741156	38.288512
2256.745734	248261.222975	38.293530
2259.425442	248607.982506	38.298548
2261.927561	248947.429984	38.303565
2264.277855	249296.808813	38.308583
2266.586020	249628.769692	38.313600
2268.881795	249977.066383	38.318618
2270.930834	250321.440295	38.323636
2273.361822	250665.170119	38.328653
2275.210499	251018.594805	38.333671
2277.459724	251376.986247	38.338688
2279.237344	251743.708781	38.343706
2281.261097	252112.272782	38.348724
2284.032069	252481.709733	38.353741
2285.850833	252856.937642	38.358759
2288.375161	253219.226438	38.363776
2290.835312	253593.744478	38.368794
2293.227304	253963.371457	38.373812
2295.628905	254346.663951	38.378829
2297.478661	254734.642473	38.383847
2299.848678	255107.729755	38.388864
2301.842920	255502.138983	38.393882
2303.795398	255896.682580	38.398900
2306.070554	256291.048726	38.403917
2308.173581	256696.619926	38.408935
2310.444642	257094.188846	38.413952
2312.925758	257507.703315	38.418970
2315.285954	257914.277388	38.423988
2317.766116	258318.750115	38.429005
2319.945972	258728.377042	38.434023
2322.286510	259136.785231	38.439040
2324.910627	259544.895074	38.444058
2327.150064	259950.805687	38.449076
2330.202458	260360.398428	38.454093
2332.467082	260770.853342	38.459111
2334.864312	261170.085158	38.464128
2337.540287	261576.386122	38.469146
2339.419645	261973.084603	38.474164
2342.135106	262378.542054	38.479181
2344.171599	262788.248333	38.484199
2346.548005	263191.220229	38.489216
2349.115206	263608.743679	38.494234
2351.016240	264016.694655	38.499252
2353.524142	264427.191782	38.504269
2355.835032	264837.695169	38.509287
2358.070102	265261.115782	38.514304
2360.460950	265673.919001	38.519322
2362.348751	266097.192251	38.524340
2364.853386	266509.241495	38.529357
2367.002361	266933.159967	38.534375
2369.228168	267334.000459	38.539392
2371.593894	267735.123905	38.544410
2373.881344	268128.461232	38.549428
2376.605617	268516.725118	38.554445
2378.893808	268911.587017	38.559463
2381.266143	269304.860798	38.564480
2383.735642	269711.887995	38.569498
2385.988342	270108.763024	38.574516
2388.363490	270523.655211	38.579533
2390.250739	270928.412764	38.584551
2392.700788	271331.379235	38.589568
2395.310248	271752.102947	38.594586
2397.171852	272176.476412	38.599604
2399.607494	272597.100910	38.604621
2401.635216	273032.244705	38.609639
2403.808545	273463.478779	38.614656
2406.303228	273903.807207	38.619674
2408.925328	274360.932544	38.624692
2411.546141	274800.682172	38.629709
2413.388293	275252.418621	38.634727
2415.721521	275696.583201	38.639744
2418.939185	276147.796716	38.644762
2421.242879	276598.672370	38.649780
2423.775577	277053.347552	38.654797
2426.419361	277504.499346	38.659815
2429.018625	277951.796748	38.664832
2431.680843	278403.377189	38.669850
2433.843348	278858.110464	38.674868
2436.982532	279303.060861	38.679885
2439.579799	279753.101393	38.684903
2441.934850	280190.656231	38.689920
2444.615958	280638.472883	38.694938
2447.277532	281082.151610	38.699956
2449.881630	281514.661703	38.704973
2452.830701	281951.994240	38.709991
2455.451569	282381.198619	38.715008
2458.223213	282808.803762	38.720026
2460.455539	283243.048048	38.725044
2462.965039	283676.485922	38.730061
2465.364663	284101.075103	38.735079
2467.679106	284532.637831	38.740096
2470.264761	284964.309552	38.745114
2472.275520	285401.940030	38.750132
2475.040199	285839.425125	38.755149
2477.471733	286272.415363	38.760167
2479.707133	286716.334036	38.765184
2482.546590	287149.792004	38.770202
2484.647845	287599.116196	38.775220
2487.380733	288036.324099	38.780237
2489.525730	288485.919523	38.785255
2491.965759	288932.800221	38.790272
2494.742950	289366.417364	38.795290
2496.562200	289827.290343	38.800308
2499.163408	290271.425276	38.805325
2501.729117	290715.539685	38.810343
2504.240204	291142.235810	38.815360
2506.831890	291557.182461	38.820378
2508.516703	291972.627752	38.825396
2511.355958	292398.634613	38.830413
2513.699925	292822.534574	38.835431
2516.020489	293260.027712	38.840448
2518.485221	293685.964493	38.845466
2520.738087	294125.270192	38.850484
2523.445916	294560.311522	38.855501
2525.881120	295010.534816	38.860519
2528.245112	295463.435611	38.865536
2530.594023	295909.174387	38.870554
2533.109927	296369.593414	38.875572
2535.658018	296817.051251	38.880589
2538.114819	297286.952302	38.885607
2540.601563	297764.213909	38.890624
2543.252990	298222.701680	38.895642
2545.960034	298691.035271	38.900660
2548.653892	299158.124991	38.905677
2551.393180	299622.920078	38.910695
2553.912890	300094.530826	38.915712
2556.927070	300551.100452	38.920730
2559.655948	301030.067094	38.925748
2562.326598	301488.898340	38.930765
2565.186850	301951.432134	38.935783
2567.649177	302427.667914	38.940800
2570.410084	302884.804133	38.945818
2572.762635	303355.745493	38.950836
2575.523700	303815.952242	38.955853
2579.019197	304266.338052	38.960871
2581.992572	304707.914903	38.965888
2584.630640	305164.809182	38.970906
2587.056554	305620.948107	38.975924
2589.949282	306070.890014	38.980941
2592.046513	306528.576489	38.985959
2594.435846	306998.356350	38.990976
2597.052520	307449.200780	38.995994
2599.001796	307915.541726	39.001012
2601.445398	308399.252326	39.006029
2604.019804	308874.863140	39.011047
2606.331734	309356.304783	39.016064
2608.995547	309839.593685	39.021082
2611.213705	310337.835287	39.026100
2613.766509	310818.902532	39.031117
2616.305270	311323.210289	39.036135
2618.618562	311828.669055	39.041152
2621.542696	312331.260237	39.046170
2623.924957	312837.744780	39.051188
2626.362803	313355.418993	39.056205
2628.970854	313861.151738	39.061223
2631.485430	314373.119487	39.066240
2634.046260	314887.845795	39.071258
2636.835089	315417.873947	39.076276
2639.516868	315928.918447	39.081293
2642.426984	316435.327101	39.086311
2644.773378	316933.441138	39.091328
2647.709847	317410.150416	39.096346
2650.881142	317871.175176	39.101364
2653.315933	318349.152917	39.106381
2656.409704	318816.814084	39.111399
2658.567006	319304.481890	39.116416
2661.498955	319762.817706	39.121434
2664.174820	320252.912615	39.126452
2666.832878	320727.414005	39.131469
2669.527773	321199.519735	39.136487
2671.788634	321686.243923	39.141504
2674.773177	322175.796743	39.146522
2677.294695	322658.004410	39.151540
2679.771612	323152.025620	39.156557
2682.797134	323640.649280	39.161575
2685.311975	324132.601641	39.166592
2688.436445	324617.089763	39.171610
2690.953803	325114.191185	39.176628
2693.929031	325608.525127	39.181645
2696.518822	326095.831808	39.186663
2698.904225	326607.369378	39.191680
2702.447132	327097.236202	39.196698
2704.811097	327600.644317	39.201716
2707.413367	328115.210415	39.206733
2710.373660	328610.188053	39.211751
2712.750309	329127.881164	39.216768
2715.880072	329618.584510	39.221786
2718.540684	330140.517231	39.226804
2721.263570	330642.248397	39.231821
2724.460078	331148.268793	39.236839
2726.706272	331669.469030	39.241856
2729.149173	332187.079283	39.246874
2731.962643	332698.177260	39.251892
2734.397240	333226.649422	39.256909
2737.444818	333742.908232	39.261927
2739.760883	334273.498796	39.266944
2742.463636	334806.461667	39.271962
2745.254733	335352.559430	39.276980
2748.077051	335885.977313	39.281997
2750.499279	336424.278701	39.287015
2753.351969	336970.251915	39.292032
2755.959376	337513.796487	39.297050
2758.828352	338066.054976	39.302068
2761.894268	338596.898536	39.307085
2765.121185	339140.077385	39.312103
2767.897806	339691.955596	39.317120
2771.067058	340229.192872	39.322138
2773.614188	340766.701767	39.327156
2776.148406	341307.534079	39.332173
2779.242843	341845.429290	39.337191
2781.569417	342398.395580	39.342208
2784.124232	342942.815356	39.347226
2786.953563	343492.112123	39.352244
2789.745226	344043.948623	39.357261
2792.791787	344590.230337	39.362279
2795.613956	345103.588815	39.367296
2798.259533	345610.801476	39.372314
2800.540520	346131.675147	39.377332
2803.012954	346657.718165	39.382349
2805.868588	347176.003332	39.387367
2808.362786	347708.176812	39.392384
2811.193637	348242.221305	39.397402
2813.957679	348773.961078	39.402420
2816.359566	349333.830133	39.407437
2819.127586	349872.285964	39.412455
2821.761959	350432.436939	39.417472
2824.557796	350982.326230	39.422490
2827.537691	351549.290277	39.427508
2830.597240	352108.747141	39.432525
2833.206830	352662.862405	39.437543
2835.983312	353242.481960	39.442560
2839.018622	353814.489642	39.447578
2842.113061	354381.201808	39.452596
2844.575466	354962.704777	39.457613
2847.752867	355540.889617	39.462631
2850.081696	356131.462097	39.467648
2853.251445	356718.950104	39.472666
2856.150031	357309.037712	39.477684
2858.698221	357905.519229	39.482701
2861.748781	358501.787047	39.487719
2864.788352	359101.628066	39.492736
2867.384381	359696.912526	39.497754
2870.825295	360289.568535	39.502772
2874.101313	360890.923362	39.507789
2877.326699	361483.040235	39.512807
2880.057495	362080.659209	39.517824
2883.198331	362665.389027	39.522842
2886.448154	363254.154870	39.527860
2889.227550	363845.068718	39.532877
2892.634504	364426.637843	39.537895
2895.859602	365002.340599	39.542912
2898.764882	365586.994244	39.547930
2901.941818	366156.726088	39.552948
2904.990524	366739.235640	39.557965
2907.887568	367309.047777	39.562983
2911.079451	367882.891475	39.568000
2913.621089	368457.160474	39.573018
2916.600400	369044.065870	39.578036
2919.246916	369621.779322	39.583053
2922.529050	370190.706104	39.588071
2925.041575	370776.773592	39.593088
2927.502815	371370.225054	39.598106
2930.511523	371957.745476	39.603124
2933.436345	372548.011299	39.608141
2936.765093	373131.759997	39.613159
2939.833406	373716.074524	39.618176
2942.725571	374295.181884	39.623194
2945.880361	374879.466161	39.628212
2948.628776	375465.354056	39.633229
2951.592273	376025.980134	39.638247
2954.551038	376583.199411	39.643264
2957.485602	377130.038091	39.648282
2960.518217	377662.976084	39.653300
2963.099403	378211.631727	39.658317
2965.988525	378748.408665	39.663335
2968.711817	379300.121720	39.668352
2972.004699	379851.635329	39.673370
2974.840816	380403.644652	39.678388
2977.563304	380959.393200	39.683405
2980.665410	381524.256812	39.688423
2983.461593	382086.141735	39.693440
2986.648232	382649.554671	39.698458
2989.144810	383210.912232	39.703476
2991.769003	383796.592987	39.708493
2994.815070	384374.587974	39.713511
2997.438076	384977.981194	39.718528
3000.309052	385578.712695	39.723546
3003.654539	386179.486097	39.728564
3006.504999	386774.418064	39.733581
3009.341571	387381.060640	39.738599
3012.150378	387998.426201	39.743616
3014.518297	388622.191708	39.748634
3018.151929	389250.564918	39.753652
3021.013401	389886.581792	39.758669
3024.054296	390524.486318	39.763687
3026.885916	391153.738835	39.768704
3030.396680	391790.176461	39.773722
3033.681633	392428.565558	39.778740
3036.389382	393082.909490	39.783757
3039.414550	393720.073156	39.788775
3042.302092	394365.184072	39.793792
3045.372161	395021.994817	39.798810
3048.630251	395677.799456	39.803828
3051.443998	396340.685633	39.808845
3054.679228	396996.772396	39.813863
3057.791034	397663.819729	39.818880
3060.680821	398332.638307	39.823898
3064.081401	398998.446597	39.828916
3066.762764	399676.221233	39.833933
3069.530882	400349.125354	39.838951
3072.633761	401032.180106	39.843968
3075.611223	401725.406872	39.848986
3078.933424	402408.042710	39.854004
3081.880141	403098.379688	39.859021
3084.879338	403794.904463	39.864039
3087.784107	404491.758348	39.869056
3090.897254	405191.453721	39.874074
3094.371756	405886.918825	39.879092
3097.759407	406582.584863	39.884109
3100.482057	407275.146484	39.889127
3104.178521	407971.467356	39.894144
3107.398747	408659.381584	39.899162
3111.022172	409339.536272	39.904180
3114.259666	410028.633312	39.909197
3117.829068	410693.380663	39.914215
3120.821160	411337.218622	39.919232
3123.703541	411969.249323	39.924250
3126.835591	412599.554309	39.929268
3129.785513	413225.160697	39.934285
3132.799338	413868.002348	39.939303
3136.021500	414497.492006	39.944320
3138.677867	415151.436625	39.949338
3141.596209	415799.521817	39.954356
3144.465452	416449.703489	39.959373
3147.357027	417105.821863	39.964391
3150.442529	417767.925330	39.969408
3153.120144	418449.994466	39.974426
3156.614076	419115.599978	39.979444
3159.386833	419814.927265	39.984461
3162.338193	420497.511555	39.989479
3165.650887	421188.763110	39.994496
3168.463083	421892.263239	39.999514
3171.840877	422606.676844	40.004532
3174.918966	423323.171383	40.009549
3177.944096	424024.936434	40.014567
3181.321284	424747.603726	40.019584
3184.358462	425475.448043	40.024602
3187.635304	426189.200840	40.029620
3190.655510	426922.227041	40.034637
3194.155223	427653.789389	40.039655
3197.183624	428391.029371	40.044672
3200.587706	429125.428463	40.049690
3204.283667	429855.505673	40.054708
3207.729055	430609.511578	40.059725
3211.076036	431328.205281	40.064743
3214.593599	432062.605066	40.069760
3217.608412	432808.004134	40.074778
3221.312481	433527.846322	40.079796
3224.491605	434270.872244	40.084813
3227.402378	435014.906512	40.089831
3230.900336	435753.280358	40.094848
3233.858662	436495.440239	40.099866
3237.002166	437245.702286	40.104884
3239.815836	437998.728551	40.109901
3242.648156	438751.956915	40.114919
3246.102048	439520.609806	40.119936
3249.212884	440294.407192	40.124954
3252.732737	441061.077233	40.129972
3255.746315	441837.575387	40.134989
3259.100759	442601.843257	40.140007
3262.776395	443377.427819	40.145024
3266.040137	444155.280128	40.150042
3269.598862	444919.897617	40.155060
3272.686384	445692.158794	40.160077
3276.198899	446457.139106	40.165095
3279.320518	447225.902427	40.170112
3282.692096	448006.192996	40.175130
3286.452642	448750.659578	40.180148
3289.492092	449532.773864	40.185165
3292.712997	450289.677490	40.190183
3296.180366	451016.807346	40.195200
3299.241248	451747.926176	40.200218
3302.351930	452468.638709	40.205236
3305.455034	453190.240591	40.210253
3308.758943	453924.793714	40.215271
3311.858508	454643.819485	40.220288
3314.994993	455382.045784	40.225306
3318.408077	456114.233002	40.230324
3321.729706	456863.462915	40.235341
3324.844768	457607.437992	40.240359
3328.108953	458354.450877	40.245376
3331.145458	459125.658857	40.250394
3334.788603	459879.440924	40.255412
3338.436532	460634.966932	40.260429
3341.193177	461424.553323	40.265447
3345.020621	462188.344181	40.270464
3347.981562	462964.992700	40.275482
3351.373702	463741.696719	40.280500
3354.715613	464516.458355	40.285517
3357.867994	465313.679532	40.290535
3361.248667	466101.882247	40.295552
3364.740872	466885.840055	40.300570
3368.544559	467676.041250	40.305588
3372.176681	468464.014558	40.310605
3375.361568	469272.611202	40.315623
3379.108411	470056.106438	40.320640
3382.324000	470854.421591	40.325658
3386.150420	471648.867416	40.330676
3389.532161	472447.397840	40.335693
3392.867040	473245.803346	40.340711
3396.467439	474035.338248	40.345728
3399.900121	474858.691671	40.350746
3403.129507	475648.323378	40.355764
3406.136474	476447.058804	40.360781
3409.576598	477273.446439	40.365799
3413.110131	478090.938981	40.370816
3416.169752	478913.123102	40.375834
3419.756724	479738.272899	40.380852
3423.541962	480552.136297	40.385869
3426.912117	481373.006140	40.390887
3430.100266	482194.072413	40.395904
3433.640820	483022.679300	40.400922
3437.615365	483848.200622	40.405940
3440.803174	484671.486524	40.410957
3444.340417	485505.596350	40.415975
3447.951057	486323.944141	40.420992
3451.069897	487168.860384	40.426010
3454.444330	487989.498035	40.431028
3458.113190	488827.382221	40.436045
3461.414457	489653.162752	40.441063
3465.146395	490482.577074	40.446080
3468.715091	491315.263809	40.451098
3472.439149	492144.655964	40.456116
3476.079030	492964.174922	40.461133
3479.602068	493782.903900	40.466138
3483.232046	494528.598277	40.471143
3486.194262	495249.355372	40.476148
3489.220487	495896.659364	40.481152
3492.433447	496496.876407	40.486157
3495.255027	497025.092423	40.491162
3497.884689	497491.053031	40.496167
3500.572510	497906.316661	40.501172
3503.072024	498253.511016	40.506176
3505.209853	498560.510304	40.511181
3506.952444	498796.796405	40.516186
3508.788850	498990.339508	40.521191
3510.309243	499146.267945	40.526196
3511.766848	499264.441428	40.531200
3513.001184	499338.001588	40.536205
3514.007642	499365.380450	40.541210
3515.232560	499370.957682	40.546215
3516.094235	499341.764992	40.551220
3516.948665	499287.161511	40.556224
3517.812719	499198.994269	40.561229
3518.047486	499103.484650	40.566234
3518.434080	498975.096743	40.571239
3518.725560	498841.761941	40.576244
3519.044068	498684.882188	40.581248
3519.458166	498516.089442	40.586253
3519.590347	498336.759262	40.591258
3519.705548	498142.647621	40.596263
3519.905929	497946.697925	40.601268
3519.983913	497736.185259	40.606272
3520.179532	497518.968879	40.611277
3519.869208	497309.423896	40.616282
3519.895221	497066.257286	40.621287
3519.938134	496844.956130	40.626292
3519.696659	496611.799458	40.631296
3519.659961	496376.936653	40.636301
3519.565167	496142.434410	40.641306
3519.424436	495903.480899	40.646311
3519.022868	495666.995795	40.651316
3519.115266	495422.935995	40.656320
3519.115002	495183.191370	40.661325
3518.459849	494953.066204	40.666330
3518.413743	494714.740425	40.671335
3518.464614	494475.687334	40.676340
3517.907041	494247.411369	40.681344
3517.941724	493998.075634	40.686349
3517.758988	493786.697774	40.691354
3517.799273	493538.367660	40.696359
3516.948401	493320.304650	40.701364
3516.855429	493087.484727	40.706368
3516.654155	492862.426785	40.711373
3516.452406	492654.229223	40.716378
3516.377297	492419.980160	40.721383
3516.123439	492217.001880	40.726388
3515.601585	492005.201473	40.731392
3515.637933	491791.639229	40.736397
3515.192527	491595.976897	40.741402
3515.277890	491389.796115	40.746407
3515.039560	491190.197258	40.751412
3514.841396	490988.918654	40.756416
3514.455841	490789.288132	40.761421
3514.246791	490609.885715	40.766426
3514.084243	490417.306312	40.771431
3513.953579	490225.783460	40.776436
3513.432493	490044.804261	40.781440
3513.726166	489864.454239	40.786445
3513.098796	489694.833460	40.791450
3512.814628	489512.798721	40.796455
3512.918043	489360.279816	40.801460
3512.879737	489177.240641	40.806464
3512.522397	489009.242413	40.811469
3512.351342	488851.393906	40.816474
3511.997972	488693.522243	40.821479
3511.792672	488535.980411	40.826484
3511.651944	488401.169491	40.831488
3511.610952	488232.962390	40.836493
3511.453059	488089.034644	40.841498
3511.141903	487944.420894	40.846503
3510.944511	487799.585446	40.851508
3510.731661	487662.349322	40.856512
3510.840778	487528.404450	40.861517
3510.421328	487391.553598	40.866522
3510.205214	487257.050371	40.871527
3510.127843	487120.548728	40.876532
3510.009544	487004.922447	40.881536
3509.979680	486870.488354	40.886541
3509.980399	486752.055678	40.891546
3510.089250	486627.374486	40.896551
3509.697924	486511.839021	40.901556
3509.263483	486391.699918	40.906560
3509.466864	486261.125218	40.911565
3509.069973	486157.188928	40.916570
3508.983864	486040.893164	40.921575
3508.598388	485939.284132	40.926580
3508.264462	485838.679572	40.931584
3508.735306	485733.843948	40.936589
3508.499147	485637.630156	40.941594
3508.383343	485532.784843	40.946599
3508.238466	485445.724918	40.951604
3507.900499	485349.981705	40.956608
3508.235403	485242.581252	40.961613
3507.915285	485159.347201	40.966618
3507.649135	485067.441377	40.971623
3507.908617	484970.841931	40.976628
3507.948113	484890.488174	40.981632
3507.886834	484791.000212	40.986637
3507.434974	484705.809245	40.991642
3507.471510	484633.104703	40.996647
3507.630139	484546.600661	41.001652
3507.325776	484460.068091	41.006656
3507.494540	484372.447107	41.011661
3506.867357	484298.174368	41.016666
3506.738018	484212.575601	41.021671
3506.695403	484138.919119	41.026676
3506.461206	484072.334764	41.031680
3506.490319	484012.142749	41.036685
3506.323480	483939.062432	41.041690
3506.273519	483874.322806	41.046695
3506.278337	483812.968755	41.051700
3506.085989	483749.112495	41.056704
3506.284484	483687.322122	41.061709
3506.318451	483630.218640	41.066714
3506.359458	483559.282580	41.071719
3506.494575	483499.224204	41.076724
3506.484307	483436.047429	41.081728
3506.612880	483364.387511	41.086733
3506.045304	483314.673885	41.091738
3506.065408	483245.665241	41.096743
3505.924837	483195.123838	41.101748
3505.779393	483131.714110	41.106752
3506.080882	483056.580487	41.111757
3505.473426	483023.946656	41.116762
3505.550534	482954.319977	41.121767
3505.463145	482911.166616	41.126772
3505.169064	482854.315363	41.131776
3505.038612	482803.315345	41.136781
3505.080207	482765.663874	41.141786
3505.527606	482709.302986	41.146791
3505.196940	482671.811508	41.151796
3504.968639	482624.778469	41.156800
3505.427356	482573.735386	41.161805
3505.296425	482529.473392	41.166810
3505.243785	482482.716242	41.171815
3505.072318	482439.119120	41.176820
3504.934478	482396.783263	41.181824
3504.940118	482354.120630	41.186829
3504.826138	482312.338157	41.191834
3505.090230	482272.978539	41.196839
3504.738197	482231.790864	41.201844
3504.459020	482184.004787	41.206848
3504.663024	482149.619851	41.211853
3504.617156	482129.309348	41.216858
3504.850272	482084.988798	41.221863
3504.514197	482045.571584	41.226868
3504.741770	482008.699940	41.231872
3504.831183	481977.068893	41.236877
3504.511899	481939.422198	41.241882
3504.465420	481906.748483	41.246887
3504.467069	481876.144514	41.251892
3504.381491	481843.223529	41.256896
3504.503279	481807.786947	41.261901
3504.438807	481770.099647	41.266906
3504.109038	481736.001030	41.271911
3504.389356	481707.176826	41.276916
3504.521510	481676.602584	41.281920
3504.252459	481646.699741	41.286925
3504.056911	481616.177204	41.291930
3504.370755	481588.766262	41.296935
3504.396849	481559.728679	41.301940
3504.118757	481532.765911	41.306944
3504.379221	481495.736090	41.311949
3504.380409	481469.945158	41.316954
3504.261765	481437.130054	41.321959
3504.230955	481409.824011	41.326964
3503.851195	481375.529987	41.331968
3504.640051	481340.037783	41.336973
3504.009219	481328.280780	41.341978
3504.311004	481291.294711	41.346983
3503.984978	481260.386882	41.351988
3503.789583	481240.707131	41.356992
3503.807300	481222.463108	41.361997
3503.677733	481197.655218	41.367002
3503.999431	481167.202229	41.372007
3504.385818	481151.382712	41.377012
3503.973963	481128.696841	41.382016
3504.408604	481084.696860	41.387021
3504.462839	481063.964061	41.392026
3504.282421	481035.515720	41.397031
3504.048021	481012.598980	41.402036
3503.848022	480980.910727	41.407040
3504.167933	480950.001646	41.412045
3503.919964	480932.458073	41.417050
3504.126879	480905.367103	41.422055
3504.153280	480879.976775	41.427060
3503.739306	480853.541259	41.432064
3503.891409	480825.648105	41.437069
3503.836645	480805.844344	41.442074
3503.748448	480781.637442	41.447079
3503.933787	480765.089323	41.452084
3503.697976	480743.996662	41.457088
3504.023097	480716.582718	41.462093
3504.229988	480702.818073	41.467098
3504.202722	480676.473206	41.472103
3504.272658	480637.647703	41.477108
3503.943672	480627.362714	41.482112
3504.049148	480585.947233	41.487117
3504.183828	480580.656111	41.492122
3504.303159	480548.308620	41.497127
3504.244634	480516.799942	41.502132
3503.892132	480490.252874	41.507136
3504.332379	480459.273327	41.512141
3503.791018	480434.732252	41.517146
3504.025997	480405.305234	41.522151
3504.052697	480384.525397	41.527156
3503.966549	480357.530668	41.532160
3504.207923	480322.528547	41.537165
3503.992066	480309.489193	41.542170
3503.982505	480278.783154	41.547175
3504.064441	480249.937494	41.552180
3503.901040	480223.866901	41.557184
3503.898423	480192.450210	41.562189
3503.662447	480183.315762	41.567194
3503.857610	480152.830529	41.572199
3504.206040	480126.172173	41.577204
3503.853319	480104.387881	41.582208
3504.024585	480079.733716	41.587213
3503.861435	480068.155391	41.592218
3503.604700	480043.011429	41.597223
3503.747731	480027.280150	41.602228
3503.624805	480006.016831	41.607232
3503.917372	479987.424176	41.612237
3503.785991	479967.581007	41.617242
3503.918756	479936.395875	41.622247
3503.963370	479912.521623	41.627252
3503.640775	479891.289742	41.632256
3504.017946	479860.319225	41.637261
3503.852524	479835.413932	41.642266
3503.482552	479815.405629	41.647271
3503.568789	479787.318718	41.652276
3503.650622	479775.397453	41.657280
3503.329996	479747.070754	41.662285
3503.418630	479748.577002	41.667290
3503.925799	479723.463904	41.672295
3503.820675	479704.021712	41.677300
3503.509457	479687.703201	41.682304
3503.843034	479657.600716	41.687309
3503.632910	479642.837089	41.692314
3502.999151	479625.404002	41.697319
3503.606344	479600.933703	41.702324
3503.534641	479589.391316	41.707328
3503.578487	479578.388075	41.712333
3503.490164	479559.753875	41.717338
3503.562269	479539.472714	41.722343
3503.851923	479517.383534	41.727348
3503.572659	479502.326683	41.732352
3503.498569	479474.467368	41.737357
3503.461493	479467.733532	41.742362
3503.587338	479453.676777	41.747367
3503.529859	479435.138933	41.752372
3503.265569	479416.380389	41.757376
3503.401033	479397.558637	41.762381
3503.373873	479390.671182	41.767386
3503.534838	479364.852229	41.772391
3503.724551	479353.065681	41.777396
3503.508109	479342.812903	41.782400
3503.813893	479309.572430	41.787405
3503.534657	479291.626931	41.792410
3503.372078	479277.919693	41.797415
3503.496509	479253.981353	41.802420
3503.593336	479245.604666	41.807424
3503.809700	479219.067312	41.812429
3503.385433	479214.877684	41.817434
3503.588387	479190.622803	41.822439
3503.528745	479170.615466	41.827444
3503.348092	479163.093413	41.832448
3503.828208	479137.831821	41.837453
3503.338949	479128.331514	41.842458
3503.365935	479105.219206	41.847463
3503.326708	479090.985584	41.852468
3503.188002	479082.240653	41.857472
3503.566446	479057.248408	41.862477
3503.289194	479060.028764	41.867482
3503.522753	479030.853299	41.872487
3503.713584	479019.269079	41.877492
3503.603376	478997.090497	41.882496
3503.594385	478978.493885	41.887501
3503.541173	478964.566438	41.892506
3503.201562	478946.022056	41.897511
3503.655223	478928.568491	41.902516
3503.482954	478901.382676	41.907520
3503.688949	478888.022317	41.912525
3503.420187	478876.358633	41.917530
3503.392163	478861.920370	41.922535
3503.861701	478838.129681	41.927540
3503.241307	478825.761404	41.932544
3503.117475	478800.493496	41.937549
3503.409320	478797.862905	41.942554
3503.252417	478780.303016	41.947559
3503.294343	478754.806143	41.952564
3503.446120	478752.400393	41.957568
3503.560556	478733.479980	41.962573
3503.315380	478718.670526	41.967578
3503.261317	478702.867994	41.972583
3503.522965	478682.708023	41.977588
3503.442759	478670.761029	41.982592
3503.293693	478652.084898	41.987597
3503.630949	478628.112160	41.992602
3503.417029	478609.294210	41.997607
3503.415868	478600.983416	42.002612
3503.189076	478592.809638	42.007616
3503.331374	478573.124515	42.012621
3503.216118	478554.797687	42.017626
3503.333762	478549.052622	42.022631
3503.378515	478530.345739	42.027636
3503.461448	478523.085840	42.032640
3503.277284	478506.644913	42.037645
3503.156706	478489.737828	42.042650
3503.367170	478476.883257	42.047655
3503.536134	478471.535476	42.052660
3503.282478	478444.260544	42.057664
3503.449524	478434.858868	42.062669
3503.334595	478413.187152	42.067674
3503.377047	478400.815187	42.072679
3503.804241	478384.226844	42.077684
3503.232160	478373.016228	42.082688
3503.551281	478358.167982	42.087693
3503.445216	478338.572563	42.092698
3503.409962	478316.736114	42.097703
3503.349210	478298.096367	42.102708
3503.194926	478287.326438	42.107712
3503.547613	478275.412134	42.112717
3503.398450	478251.819897	42.117722
3503.402774	478237.730811	42.122727
3503.328342	478224.312977	42.127732
3503.622753	478220.009534	42.132736
3503.318808	478187.927797	42.137741
3503.475082	478181.872451	42.142746
3503.351704	478166.992653	42.147751
3503.409314	478135.765885	42.152756
3503.351214	478136.839349	42.157760
3503.403905	478115.596914	42.162765
3503.259131	478089.469882	42.167770
3503.250430	478088.153662	42.172775
3503.464941	478071.700034	42.177780
3503.092933	478066.488334	42.182784
3503.329537	478054.845638	42.187789
3502.931266	478034.687968	42.192794
3502.972515	478021.606459	42.197799
3503.223757	478008.035643	42.202804
3503.036945	478005.734002	42.207808
3503.343422	477984.096562	42.212813
3503.089800	477982.717693	42.217818
3503.120440	477968.624256	42.222823
3503.157737	477956.151472	42.227828
3503.076743	477949.829490	42.232832
3503.347921	477931.998468	42.237837
3503.191592	477918.948123	42.242842
3503.182117	477901.718902	42.247847
3503.339359	477896.727570	42.252852
3503.099924	477881.764546	42.257856
3503.300752	477862.626934	42.262861
3503.332624	477854.259927	42.267866
3503.296023	477837.947158	42.272871
3503.147013	477823.932695	42.277876
3503.160947	477819.014676	42.282880
3503.222911	477786.570377	42.287885
3503.143160	477782.478022	42.292890
3503.449092	477775.588032	42.297895
3503.590490	477740.495792	42.302900
3503.287832	477747.283996	42.307904
3503.085774	477720.303987	42.312909
3503.419189	477704.996883	42.317914
3503.272718	477692.198228	42.322919
3503.504050	477669.558740	42.327924
3503.280505	477665.641127	42.332928
3503.550236	477650.952201	42.337933
3503.146955	477628.260941	42.342938
3503.121066	477619.446851	42.347943
3503.630372	477602.794200	42.352948
3503.434919	477605.359109	42.357952
3503.673619	477582.312921	42.362957
3503.139131	477564.456883	42.367962
3503.232408	477554.813055	42.372967
3503.472159	477534.604704	42.377972
3503.411940	477517.687250	42.382976
3503.561005	477498.506791	42.387981
3503.169743	477480.070560	42.392986
3503.564867	477459.229415	42.397991
3503.604636	477436.366544	42.402996
3503.442544	477434.263649	42.408000
3503.544725	477402.268486	42.413005
3503.490062	477386.110242	42.418010
3503.263937	477380.723260	42.423015
3503.227407	477357.973719	42.428020
3503.436324	477348.412873	42.433024
3503.213697	477322.854621	42.438029
3503.388419	477312.893721	42.443034
3503.225283	477299.083843	42.448039
3503.546102	477281.345753	42.453044
3503.079173	477278.834904	42.458048
3503.245972	477251.137111	42.463053
3503.195942	477227.325267	42.468058
3503.063302	477221.416661	42.473063
3503.156451	477214.813516	42.478068
3502.806686	477196.471824	42.483072
3503.268340	477189.050213	42.488077
3503.157123	477191.500497	42.493082
3503.149610	477176.044157	42.498087
3503.468608	477156.633786	42.503092
3503.248090	477151.296536	42.508096
3503.483863	477120.344099	42.513101
3503.334864	477115.806426	42.518106
3502.958638	477101.168521	42.523111
3503.151329	477069.361241	42.528116
3502.764885	477069.574408	42.533120
3503.219819	477064.738536	42.538125
3503.095592	477058.423105	42.543130
3503.303090	477034.874409	42.548135
3503.341987	477027.570245	42.553140
3502.810095	477016.859316	42.558144
3502.978297	476989.566387	42.563149
3503.153753	476992.731597	42.568154
3502.870726	477003.318026	42.573159
3503.266957	476984.908900	42.578164
3502.890568	476978.430578	42.583168
3503.296135	476965.493513	42.588173
3503.260677	476963.269189	42.593178
3502.952485	476929.716342	42.598183
3503.190314	476920.961620	42.603188
3502.885747	476923.999994	42.608192
3502.916102	476910.970160	42.613197
3503.074472	476893.510812	42.618202
3502.950602	476890.134784	42.623207
3503.336966	476885.411071	42.628212
3503.003387	476861.846338	42.633216
3503.136866	476849.509702	42.638221
3503.172967	476852.139467	42.643226
3502.775206	476835.325471	42.648231
3503.300373	476820.899647	42.653236
3503.298413	476821.710899	42.658240
3503.335491	476801.027028	42.663245
3503.422493	476770.198929	42.668250
3502.814397	476767.051467	42.673255
3503.086353	476769.238508	42.678260
3503.203208	476744.436759	42.683264
3503.329999	476738.436319	42.688269
3503.062379	476735.488442	42.693274
3502.850309	476705.011606	42.698279
3503.374507	476689.521523	42.703284
3503.177201	476690.465023	42.708288
3503.306019	476676.963337	42.713293
3503.524397	476660.659982	42.718298
3503.416235	476643.293228	42.723303
3503.326262	476622.730620	42.728308
3503.123114	476616.072750	42.733312
3503.108654	476607.661863	42.738317
3503.275285	476591.924134	42.743322
3503.256245	476576.215742	42.748327
3503.261452	476554.776424	42.753332
3502.901266	476542.416269	42.758336
3503.295089	476538.096753	42.763341
3503.028750	476530.992704	42.768346
3503.090649	476509.088235	42.773351
3503.246249	476498.673813	42.778356
3502.905967	476502.984952	42.783360
3503.012219	476480.009113	42.788365
3503.159220	476461.740268	42.793370
3503.044032	476456.284818	42.798375
3503.334586	476444.531293	42.803380
3503.196387	476432.490758	42.808385
3503.038404	476410.874351	42.813389
3503.227156	476407.499508	42.818394
3503.020440	476391.060399	42.823399
3503.301473	476374.746908	42.828404
3502.595579	476379.926787	42.833409
3502.991511	476369.879769	42.838413
3503.254940	476356.508637	42.843418
3502.925744	476349.718555	42.848423
3503.016855	476343.672954	42.853428
3503.070951	476344.982192	42.858433
3503.059543	476310.114325	42.863437
3502.917120	476306.690449	42.868442
3502.865893	476309.688869	42.873447
3503.320414	476298.517534	42.878452
3503.194343	476279.176666	42.883457
3503.408473	476266.776241	42.888461
3503.330967	476255.486248	42.893466
3502.987781	476233.189365	42.898471
3503.264300	476232.892279	42.903476
3503.420830	476218.220196	42.908481
3503.284975	476188.389405	42.913485
3502.915769	476184.950673	42.918490
3503.040281	476177.024469	42.923495
3503.289855	476145.409464	42.928500
3502.709579	476146.312158	42.933505
3503.280623	476134.514115	42.938509
3503.468942	476118.823271	42.943514
3503.498795	476118.261075	42.948519
3503.631174	476092.087618	42.953524
3503.255453	476075.421548	42.958529
3503.437794	476065.306774	42.963533
3503.312461	476041.049272	42.968538
3503.246914	476035.687227	42.973543
3503.447620	476010.719266	42.978548
3503.289714	475998.478850	42.983553
3503.750571	475972.962885	42.988557
3503.636152	475954.633535	42.993562
3503.365928	475948.036728	42.998567
3503.373195	475911.137870	43.003572
3503.373837	475906.424216	43.008577
3503.261093	475884.293253	43.013581
3503.137847	475862.569397	43.018586
3502.951474	475857.074351	43.023591
3503.266995	475849.573980	43.028596
3502.879992	475839.244986	43.033601
3502.873765	475815.830012	43.038605
3503.139274	475812.594989	43.043610
3502.554936	475816.488695	43.048615
3502.997492	475783.575516	43.053620
3503.022595	475778.503178	43.058625
3503.034800	475772.723299	43.063629
3502.990157	475775.872810	43.068634
3502.729856	475762.786806	43.073639
3503.227735	475739.393427	43.078644
3502.609847	475742.228082	43.083649
3502.969192	475736.038531	43.088653
3502.883142	475733.264540	43.093658
3502.786793	475728.059334	43.098663
3502.776499	475712.703673	43.103668
3502.898594	475708.122828	43.108673
3502.646913	475707.605123	43.113677
3502.754664	475702.925175	43.118682
3502.727962	475710.532077	43.123687
3503.113971	475686.091950	43.128692
3502.776076	475684.574185	43.133697
3502.953352	475676.436706	43.138701
3502.848489	475662.616486	43.143706
3503.207362	475662.205007	43.148711
3502.787272	475636.827868	43.153716
3502.760818	475636.781404	43.158721
3502.658202	475634.111387	43.163725
3502.704757	475620.267203	43.168730
3502.430844	475633.184399	43.173735
3502.713473	475615.400191	43.178740
3502.469239	475622.585351	43.183745
3502.494424	475598.404890	43.188749
3502.730007	475585.139017	43.193754
3502.774088	475594.660789	43.198759
3502.971039	475586.773586	43.203764
3502.726178	475592.691741	43.208769
3503.019354	475581.393460	43.213773
3502.974380	475569.540409	43.218778
3502.698175	475564.414275	43.223783
3502.938748	475548.968150	43.228788
3503.200780	475558.911648	43.233793
3502.971417	475541.664468	43.238797
3502.945346	475522.053641	43.243802
3502.846039	475518.166651	43.248807
3503.196376	475514.867487	43.253812
3502.994518	475504.357000	43.258817
3503.060560	475485.035685	43.263821
3503.110752	475488.778467	43.268826
3502.801504	475487.205475	43.273831
3503.253594	475461.994358	43.278836
3503.083693	475448.944545	43.283841
3503.050041	475445.249903	43.288845
3503.450384	475434.846929	43.293850
3503.096717	475409.763113	43.298855
3502.945689	475395.645897	43.303860
3502.797641	475395.365227	43.308865
3502.711470	475388.029551	43.313869
3503.156753	475360.791980	43.318874
3502.709711	475359.798295	43.323879
3503.347170	475347.989296	43.328884
3502.923239	475352.161846	43.333889
3502.959449	475331.527284	43.338893
3503.312251	475317.533113	43.343898
3502.749888	475316.608340	43.348903
3502.945443	475308.619879	43.353908
3502.821197	475285.881852	43.358913
3502.971002	475281.397901	43.363917
3503.067092	475275.401878	43.368922
3502.655149	475281.346535	43.373927
3502.983855	475269.687666	43.378932
3502.913820	475244.862923	43.383937
3502.764128	475232.519372	43.388941
3503.028965	475232.832346	43.393946
3502.656927	475243.180342	43.398951
3502.915700	475231.481820	43.403956
3502.973535	475216.368438	43.408961
3502.950118	475189.255410	43.413965
3502.844677	475198.142091	43.418970
3502.655129	475205.369440	43.423975
3502.806792	475185.730191	43.428980
3502.861855	475167.221276	43.433985
3502.767432	475167.641725	43.438989
3503.031039	475171.401518	43.443994
3502.802665	475172.907539	43.448999
3503.061284	475144.989585	43.454004
3502.901437	475127.781747	43.459009
3503.051788	475118.989385	43.464013
3502.764007	475122.228117	43.469018
3502.660960	475125.589704	43.474023
3503.167866	475115.727264	43.479028
3503.062483	475104.593089	43.484033
3502.711909	475101.404652	43.489037
3502.881166	475091.494202	43.494042
3502.888401	475085.968341	43.499047
3503.325727	475063.191981	43.504052
3503.049091	475053.656110	43.509057
3502.937146	475048.351822	43.514061
3502.982696	475026.853811	43.519066
3502.503549	475017.552678	43.524071
3502.896054	475006.998666	43.529076
3502.765934	475017.207165	43.534081
3503.024083	475013.415632	43.539085
3502.912081	475016.423851	43.544090
3503.083651	474987.505718	43.549095
3502.992259	474968.462224	43.554100
3502.773966	474973.362638	43.559105
3503.106154	474963.071567	43.564109
3503.097437	474941.531358	43.569114
3502.849972	474945.067862	43.574119
3503.096725	474931.647735	43.579124
3502.946130	474920.672664	43.584129
3503.113031	474911.167988	43.589133
3502.876160	474903.399780	43.594138
3502.899075	474898.479625	43.599143
3503.019762	474877.679187	43.604148
3502.927208	474869.888154	43.609153
3502.774636	474855.263939	43.614157
3503.222140	474849.972539	43.619162
3502.855497	474851.196321	43.624167
3502.697729	474836.218109	43.629172
3503.013359	474815.893657	43.634177
3502.584258	474821.891847	43.639181
3503.054320	474803.621119	43.644186
3502.882611	474816.725426	43.649191
3503.045655	474794.397611	43.654196
3502.711722	474780.866428	43.659201
3502.990278	474768.302839	43.664205
3503.160480	474779.427032	43.669210
3502.812214	474763.566519	43.674215
3502.901658	474751.184872	43.679220
3503.221524	474740.895637	43.684225
3502.826422	474738.727915	43.689229
3502.843380	474723.215132	43.694234
3502.813355	474717.188193	43.699239
3502.991434	474707.833715	43.704244
3502.915651	474706.274442	43.709249
3503.043862	474700.019738	43.714253
3503.159050	474671.414186	43.719258
3502.838457	474660.769966	43.724263
3502.865201	474651.946254	43.729268
3503.064102	474658.504152	43.734273
3503.044873	474650.042514	43.739277
3502.822258	474627.319294	43.744282
3502.576606	474621.782593	43.749287
3502.805632	474617.184598	43.754292
3502.663703	474624.404628	43.759297
3502.820441	474630.614391	43.764301
3503.022240	474597.027719	43.769306
3502.846720	474591.226488	43.774311
3502.847952	474581.190287	43.779316
3502.980534	474582.233798	43.784321
3502.820139	474571.868331	43.789325
3503.032355	474550.343469	43.794330
3502.615209	474545.188665	43.799335
3502.699160	474538.281974	43.804340
3502.646641	474539.760244	43.809345
3502.619996	474539.054873	43.814349
3502.876857	474535.314143	43.819354
3502.951909	474531.450089	43.824359
3502.872960	474518.233234	43.829364
3502.962477	474509.855723	43.834369
3502.815779	474504.049911	43.839373
3502.959559	474511.224818	43.844378
3502.622613	474495.615741	43.849383
3503.050426	474480.291265	43.854388
3502.697622	474477.001706	43.859393
3502.977366	474482.887947	43.864397
3503.004677	474465.295148	43.869402
3503.038978	474450.083539	43.874407
3503.227816	474432.972055	43.879412
3503.173126	474431.409427	43.884417
3502.851031	474419.244692	43.889421
3502.903626	474395.616021	43.894426
3502.928461	474402.657706	43.899431
3503.168174	474396.740096	43.904436
3503.227604	474381.423088	43.909441
3502.979808	474360.781741	43.914445
3503.040794	474343.741078	43.919450
3503.117700	474350.673174	43.924455
3502.936544	474321.455032	43.929460
3502.906813	474314.667610	43.934465
3502.881072	474311.326324	43.939469
3503.014405	474303.955557	43.944474
3503.037482	474294.676078	43.949479
3503.121524	474267.696890	43.954484
3502.811429	474272.155792	43.959489
3502.571549	474278.124231	43.964493
3502.877200	474262.159958	43.969498
3502.817011	474243.617728	43.974503
3502.934541	474232.346460	43.979508
3502.799124	474233.178912	43.984513
3503.002938	474238.621035	43.989517
3502.884014	474216.996098	43.994522
3502.703431	474202.730655	43.999527
3502.962114	474198.127878	44.004532
3502.815752	474190.547841	44.009537
3502.723951	474192.691290	44.014541
3503.018492	474185.649814	44.019546
3502.555755	474175.534688	44.024551
3502.709941	474156.502299	44.029556
3502.525992	474160.941285	44.034561
3502.451473	474157.151491	44.039565
3502.866085	474162.458937	44.044570
3502.643091	474164.673815	44.049575
3502.847286	474154.351879	44.054580
3503.197469	474142.739657	44.059585
3502.754903	474126.741484	44.064589
3502.924687	474115.715333	44.069594
3502.599866	474117.490118	44.074599
3502.953122	474117.991888	44.079604
3502.895549	474087.892173	44.084609
3502.697335	474078.191380	44.089613
3502.947118	474067.456686	44.094618
3502.754189	474082.338916	44.099623
3502.692246	474073.731724	44.104628
3503.010659	474071.653896	44.109633
3502.656253	474056.554123	44.114637
3502.870580	474037.207985	44.119642
3502.739876	474046.403295	44.124647
3502.998494	474030.192833	44.129652
3502.674009	474040.635301	44.134657
3502.630506	474018.643412	44.139661
3503.276383	473995.021871	44.144666
3503.062239	474004.078324	44.149671
3503.232935	473991.987501	44.154676
3503.187790	473975.013994	44.159681
3502.754125	473965.147609	44.164685
3502.675369	473963.031174	44.169690
3502.768810	473966.108450	44.174695
3503.085922	473951.764159	44.179700
3502.885950	473936.183687	44.184705
3502.915592	473927.714022	44.189709
3503.111993	473916.227356	44.194714
3502.592468	473923.811454	44.199719
3503.054481	473909.190784	44.204724
3503.006691	473888.314585	44.209729
3502.951858	473878.743097	44.214733
3502.829145	473883.425909	44.219738
3502.695566	473874.829956	44.224743
3502.854085	473869.482605	44.229748
3503.223582	473848.540403	44.234753
3502.986966	473846.398220	44.239757
3502.878524	473848.442958	44.244762
3503.018490	473830.071467	44.249767
3502.786534	473821.186908	44.254772
3503.028594	473814.559111	44.259777
3502.923892	473809.354730	44.264781
3503.131766	473794.723461	44.269786
3502.711633	473776.693903	44.274791
3502.831582	473769.984016	44.279796
3502.934916	473761.553322	44.284801
3502.845287	473764.203365	44.289805
3502.923656	473748.984265	44.294810
3502.671846	473725.250863	44.299815
3502.559505	473724.660389	44.304820
3502.886124	473718.374020	44.309825
3502.884557	473719.540160	44.314829
3502.726178	473727.320690	44.319834
3502.821157	473718.891299	44.324839
3503.007130	473700.106904	44.329844
3502.981890	473688.097562	44.334849
3502.591170	473692.265199	44.339853
3502.823579	473678.745134	44.344858
3502.480479	473681.638011	44.349863
3502.871362	473679.548688	44.354868
3503.073080	473653.361113	44.359873
3502.776911	473639.569749	44.364877
3503.091915	473636.326558	44.369882
3502.885716	473636.511259	44.374887
3502.780206	473608.800817	44.379892
3503.097268	473592.631457	44.384897
3502.783855	473599.270682	44.389901
3503.122870	473595.719552	44.394906
3502.958235	473581.653909	44.399911
3502.758856	473567.390990	44.404916
3502.816239	473562.769200	44.409921
3502.624737	473560.619855	44.414925
3502.732565	473552.340433	44.419930
3502.651997	473558.030450	44.424935
3502.795381	473538.593673	44.429940
3502.452030	473522.883478	44.434945
3502.472911	473522.626768	44.439949
3503.086103	473512.138476	44.444954
3502.717498	473524.565084	44.449959
3502.690109	473524.670831	44.454964
3502.908904	473526.714565	44.459969
3502.660517	473506.021750	44.464973
3502.982344	473487.063615	44.469978
3502.776012	473484.916606	44.474983
3502.658248	473476.723503	44.479988
3502.662535	473479.460116	44.484993
3502.559697	473482.821942	44.489997
3502.884288	473464.420937	44.495002
3502.511707	473458.194321	44.500007
3502.683979	473447.826384	44.505012
3502.578670	473440.695786	44.510017
3502.548943	473448.456086	44.515021
3502.788281	473440.257211	44.520026
3502.540561	473441.969175	44.525031
3502.678403	473445.799862	44.530036
3502.762857	473447.307249	44.535041
3502.353666	473423.142162	44.540045
3502.702404	473400.428632	44.545050
3502.887455	473394.113851	44.550055
3502.629218	473404.799623	44.555060
3502.606062	473407.033684	44.560065
3502.844073	473406.539890	44.565069
3502.772535	473403.611214	44.570074
3502.590302	473396.594141	44.575079
3502.602117	473377.482147	44.580084
3502.727230	473368.642327	44.585089
3502.789109	473373.346767	44.590093
3502.773323	473373.906892	44.595098
3502.801199	473369.695244	44.600103
3502.593000	473364.050897	44.605108
3502.520982	473366.596828	44.610113
3502.507333	473349.364368	44.615117
3502.699341	473335.039418	44.620122
3502.481895	473337.709720	44.625127
3502.505230	473330.254608	44.630132
3502.839388	473328.681119	44.635137
3502.573892	473338.658409	44.640141
3503.025625	473327.587263	44.645146
3502.640045	473331.247258	44.650151
3502.577998	473327.860859	44.655156
3502.887499	473311.439020	44.660161
3502.801092	473297.817027	44.665165
3503.045013	473293.115000	44.670170
3502.879970	473297.703256	44.675175
3502.942982	473286.135940	44.680180
3503.057200	473258.998572	44.685185
3502.582740	473263.483675	44.690189
3502.966329	473252.828783	44.695194
3502.840392	473256.701201	44.700199
3502.989640	473248.313727	44.705204
3502.918349	473229.823017	44.710209
3502.616360	473232.760149	44.715213
3503.386262	473227.518750	44.720218
3503.014438	473223.623705	44.725223
3502.922532	473202.196179	44.730228
3502.934125	473189.116218	44.735233
3502.427002	473183.924598	44.740237
3502.670840	473177.448386	44.745242
3503.217018	473173.256149	44.750247
3503.116546	473155.631725	44.755252
3502.946031	473150.792413	44.760257
3502.720322	473145.100082	44.765261
3503.158987	473126.934194	44.770266
3502.866770	473112.533559	44.775271
3502.580984	473100.412982	44.780276
3502.892361	473089.059748	44.785281
3502.850411	473099.204583	44.790285
3503.033746	473096.438338	44.795290
3503.138979	473075.638497	44.800295
3502.783440	473059.727107	44.805300
3502.920048	473060.364534	44.810305
3502.474196	473062.006468	44.815309
3502.792408	473057.698170	44.820314
3502.768785	473050.199687	44.825319
3502.739478	473026.633062	44.830324
3502.980231	473014.074367	44.835329
3502.803885	473019.019309	44.840333
3503.213913	473019.562826	44.845338
3503.235860	472993.960422	44.850343
3502.961085	472990.151373	44.855348
3503.006084	472980.563682	44.860353
3502.728280	472983.243571	44.865357
3503.355194	472957.342728	44.870362
3502.971257	472944.274442	44.875367
3502.912477	472939.417417	44.880372
3503.064448	472931.333530	44.885377
3502.863823	472919.909062	44.890381
3502.739977	472901.629126	44.895386
3503.093262	472904.614799	44.900391
3502.731043	472895.344894	44.905396
3502.686649	472890.840423	44.910401
3502.585778	472871.289545	44.915405
3502.617069	472850.197015	44.920410
3502.580579	472853.649838	44.925415
3502.385086	472849.321317	44.930420
3502.785152	472853.566888	44.935425
3502.874326	472854.566659	44.940429
3502.820869	472848.289411	44.945434
3502.700630	472851.755474	44.950439
3502.710245	472817.942785	44.955444
3503.036272	472810.338253	44.960449
3502.722225	472816.673681	44.965453
3503.040788	472803.291493	44.970458
3502.886538	472809.246824	44.975463
3502.521298	472796.327562	44.980468
3502.919370	472779.232305	44.985473
3502.797456	472768.150151	44.990477
3502.592475	472770.919939	44.995482
3502.628090	472763.209220	45.000487
3502.640486	472768.529921	45.005492
3502.711409	472766.491084	45.010497
3502.441195	472756.091356	45.015501
3502.801836	472733.375203	45.020506
3502.474616	472729.929237	45.025511
3502.780559	472731.553742	45.030516
3503.188432	472732.198992	45.035521
3502.995473	472732.888525	45.040525
3502.888330	472711.767042	45.045530
3502.855893	472694.841150	45.050535
3503.116316	472686.334489	45.055540
3503.018673	472682.142540	45.060545
3502.423301	472683.149143	45.065549
3502.728894	472655.879339	45.070554
3502.769997	472649.029472	45.075559
3502.729330	472652.482990	45.080564
3502.780409	472645.073933	45.085569
3502.370608	472652.843923	45.090573
3502.821232	472647.247311	45.095578
3502.796888	472651.914855	45.100583
3502.677549	472639.463542	45.105588
3502.691015	472615.636222	45.110593
3502.431892	472617.856977	45.115597
3502.852532	472605.168212	45.120602
3503.012223	472604.686779	45.125607
3502.662710	472605.907983	45.130612
3502.489470	472613.741978	45.135617
3502.727463	472613.907165	45.140621
3502.594325	472589.139840	45.145626
3502.713924	472581.060932	45.150631
3502.361756	472571.434446	45.155636
3502.555184	472576.473121	45.160641
3502.461395	472588.907547	45.165645
3502.715096	472576.346537	45.170650
3502.830356	472580.535801	45.175655
3502.817048	472585.252308	45.180660
3502.617697	472569.366537	45.185665
3502.440303	472550.587830	45.190669
3502.999638	472545.126083	45.195674
3502.374449	472549.229629	45.200679
3502.591185	472535.407132	45.205684
3502.867277	472538.911983	45.210689
3502.536814	472547.024317	45.215693
3502.620357	472548.329147	45.220698
3502.756262	472540.855951	45.225703
3502.518901	472514.533552	45.230708
3502.519154	472506.929710	45.235713
3502.697807	472508.726431	45.240717
3502.948197	472498.649818	45.245722
3502.622864	472505.950280	45.250727
3502.560243	472500.586835	45.255732
3503.085318	472494.826337	45.260737
3502.745605	472495.437690	45.265741
3502.795659	472475.659807	45.270746
3502.795385	472467.903957	45.275751
3502.743658	472461.220778	45.280756
3502.796012	472466.433857	45.285761
3502.824841	472471.853423	45.290765
3502.653489	472451.198052	45.295770
3502.424568	472441.197175	45.300775
3502.454071	472430.090903	45.305780
3502.807278	472426.233174	45.310785
3502.686789	472438.621220	45.315789
3502.617049	472433.917885	45.320794
3502.811866	472427.043645	45.325799
3502.974836	472432.036478	45.330804
3502.741968	472416.307964	45.335809
3502.377929	472398.724548	45.340813
3502.835567	472387.246421	45.345818
3502.475825	472392.575352	45.350823
3502.368087	472393.555580	45.355828
3502.692661	472383.720647	45.360833
3502.643059	472392.802497	45.365837
3502.723406	472389.139970	45.370842
3502.622743	472390.473928	45.375847
3502.834177	472382.785966	45.380852
3502.937040	472357.981055	45.385857
3502.678275	472352.699269	45.390861
3502.853358	472347.247516	45.395866
3502.726771	472350.207740	45.400871
3502.395396	472351.476784	45.405876
3502.640124	472348.396578	45.410881
3502.597377	472342.979258	45.415885
3502.748812	472326.530922	45.420890
3502.611161	472313.980920	45.425895
3502.564787	472300.453318	45.430900
3502.831147	472303.199357	45.435905
3502.744808	472307.826086	45.440909
3502.825117	472301.375447	45.445914
3502.754878	472304.073307	45.450919
3502.530794	472284.845501	45.455924
3502.943974	472270.484845	45.460929
3502.481914	472275.170972	45.465933
3502.580331	472271.657647	45.470938
3502.744781	472274.723956	45.475943
3502.695889	472264.694535	45.480948
3502.722462	472261.192565	45.485953
3502.300163	472270.181303	45.490957
3502.744276	472248.820126	45.495962
3502.839360	472235.168735	45.500967
3502.210443	472233.848785	45.505972
3502.978470	472235.552367	45.510977
3502.782712	472229.094651	45.515981
3502.746327	472236.501613	45.520986
3502.789171	472236.190722	45.525991
3502.889050	472222.234407	45.530996
3502.761657	472201.419756	45.536001
3502.469880	472193.000178	45.541005
3502.583548	472184.415120	45.546010
3502.801603	472179.666234	45.551015
3502.761393	472196.350649	45.556020
3502.738438	472179.929762	45.561025
3502.612292	472165.451512	45.566029
3502.518782	472146.456402	45.571034
3502.891686	472142.494121	45.576039
3502.996844	472150.284286	45.581044
3503.039409	472152.609481	45.586049
3502.334348	472157.181968	45.591053
3502.956507	472147.654734	45.596058
3502.682483	472119.614053	45.601063
3502.240412	472118.061787	45.606068
3502.429565	472119.451337	45.611073
3502.623320	472113.236173	45.616077
3502.952767	472109.939767	45.621082
3502.747518	472103.939751	45.626087
3502.637933	472115.312403	45.631092
3503.040445	472101.612328	45.636097
3502.282405	472085.206174	45.641101
3502.468371	472072.756949	45.646106
3502.528597	472074.268269	45.651111
3502.314035	472076.684811	45.656116
3502.526379	472069.199361	45.661121
3502.566197	472070.308360	45.666125
3502.733073	472069.065380	45.671130
3502.717068	472071.856084	45.676135
3502.490660	472073.868952	45.681140
3502.965646	472074.706389	45.686145
3502.628744	472061.883568	45.691149
3502.715430	472042.606410	45.696154
3502.724159	472029.120613	45.701159
3502.211608	472034.372404	45.706164
3502.137541	472029.264112	45.711169
3502.643114	472035.013981	45.716173
3502.614008	472030.760371	45.721178
3502.893084	472032.591954	45.726183
3502.638823	472035.673791	45.731188
3502.764483	472031.699878	45.736193
3502.771089	472028.707958	45.741197
3502.770954	472006.504269	45.746202
3502.562640	471999.135982	45.751207
3502.414668	471992.417170	45.756212
3502.818110	471983.634143	45.761217
3502.684242	471991.614232	45.766221
3502.769486	471987.494618	45.771226
3502.911843	471994.924107	45.776231
3502.687992	471987.051335	45.781236
3503.038822	471968.442064	45.786241
3502.761427	471973.352538	45.791245
3503.026481	471960.992131	45.796250
3502.827664	471965.180474	45.801255
3502.823998	471948.959128	45.806260
3502.847663	471927.714771	45.811265
3502.759166	471925.802438	45.816269
3503.093646	471918.044158	45.821274
3502.967674	471915.326648	45.826279
3502.878894	471893.593093	45.831284
3503.008492	471876.691604	45.836289
3502.973221	471881.462439	45.841293
3502.974679	471879.941432	45.846298
3502.830050	471852.336177	45.851303
3502.454880	471848.137231	45.856308
3502.810862	471832.163106	45.861313
3502.563916	471828.907073	45.866317
3502.533206	471833.727892	45.871322
3502.538863	471836.920755	45.876327
3502.327916	471841.770062	45.881332
3502.595046	471832.907130	45.886337
3502.741129	471840.386780	45.891341
3502.313749	471825.753131	45.896346
3502.475539	471812.597855	45.901351
3502.711043	471810.837071	45.906356
3502.397524	471808.149192	45.911361
3502.723782	471810.632359	45.916365
3502.665183	471800.756328	45.921370
3502.920314	471805.329194	45.926375
3502.816615	471810.313637	45.931380
3503.057584	471798.058327	45.936385
3502.779685	471778.737165	45.941389
3502.683241	471769.880982	45.946394
3503.173841	471760.982696	45.951399
3502.839554	471758.754340	45.956404
3503.059505	471745.437744	45.961409
3503.051572	471736.314086	45.966413
3503.103471	471727.028883	45.971418
3502.809973	471728.494754	45.976423
3502.405842	471721.664261	45.981428
3502.297107	471707.385712	45.986433
3502.198655	471712.014491	45.991437
3502.317421	471718.484618	45.996442
3502.473699	471723.174517	46.001447
3502.428367	471730.532382	46.006452
3502.521830	471708.262881	46.011457
3502.193589	471700.355806	46.016461
3502.790083	471681.301888	46.021466
3502.771705	471685.157600	46.026471
3502.638932	471683.252243	46.031476
3502.754755	471674.565244	46.036481
3502.951287	471683.760584	46.041485
3502.597617	471683.056113	46.046490
3503.132009	471672.984897	46.051495
3502.699972	471652.116455	46.056500
3502.865834	471644.181949	46.061505
3502.719252	471651.809319	46.066509
3502.535760	471643.220313	46.071514
3502.768848	471652.714056	46.076519
3502.460029	471644.803889	46.081524
3502.596743	471620.601069	46.086529
3502.794783	471614.537160	46.091533
3502.420364	471612.365827	46.096538
3502.996380	471605.988696	46.101543
3502.455843	471611.245017	46.106548
3502.570758	471599.820627	46.111553
3502.506336	471609.209334	46.116557
3502.776343	471606.429189	46.121562
3503.008106	471602.742588	46.126567
3502.784542	471582.094593	46.131572
3502.882115	471561.193037	46.136577
3502.945167	471569.497024	46.141581
3502.754254	471563.291805	46.146586
3502.977541	471556.311385	46.151591
3502.500701	471536.565189	46.156596
3502.566396	471514.604036	46.161601
3502.507551	471526.932193	46.166605
3502.513705	471516.082590	46.171610
3502.713872	471523.249638	46.176615
3502.381951	471528.827867	46.181620
3502.745066	471521.977417	46.186625
3502.755712	471532.165409	46.191629
3502.875192	471515.721475	46.196634
3502.808684	471495.048567	46.201639
3502.878749	471489.562493	46.206644
3502.635669	471479.816859	46.211649
3502.715463	471478.891778	46.216653
3503.002517	471479.708253	46.221658
3502.687810	471461.102337	46.226663
3502.493096	471446.735808	46.231668
3502.560048	471438.056434	46.236673
3502.721334	471437.371944	46.241677
3502.563421	471439.069877	46.246682
3502.807034	471439.893221	46.251687
3502.650926	471450.563866	46.256692
3502.763969	471430.268069	46.261697
3502.428615	471435.035747	46.266701
3502.656191	471415.228781	46.271706
3502.791731	471404.510752	46.276711
3502.472730	471405.068166	46.281716
3502.486609	471396.752029	46.286721
3502.410483	471405.838508	46.291725
3502.689337	471401.992342	46.296730
3502.505639	471409.220109	46.301735
3502.322066	471408.032486	46.306740
3502.317049	471398.604046	46.311745
3502.531316	471416.364160	46.316749
3502.723905	471414.762211	46.321754
3502.896429	471403.379301	46.326759
3502.299854	471390.394325	46.331764
3502.637395	471368.187264	46.336769
3502.667815	471360.121973	46.341773
3502.375998	471368.532832	46.346778
3502.422944	471358.842685	46.351783
3502.396212	471370.608213	46.356788
3502.839839	471367.699202	46.361793
3502.685523	471364.580538	46.366797
3503.120992	471358.529719	46.371802
3503.190589	471353.753415	46.376807
3502.599437	471339.196000	46.381812
3503.208476	471324.550250	46.386817
3502.940355	471336.607430	46.391821
3502.867729	471318.875631	46.396826
3502.689128	471297.814682	46.401831
3502.800344	471292.626223	46.406836
3502.635420	471279.319469	46.411841
3502.712824	471286.759482	46.416845
3502.735072	471280.317700	46.421850
3502.754161	471284.674518	46.426855
3502.358060	471277.386350	46.431860
3503.021918	471252.136558	46.436865
3502.737768	471254.310719	46.441869
3502.734338	471254.818254	46.446874
3502.592592	471254.485831	46.451879
3502.739047	471247.162585	46.456884
3502.750392	471250.912289	46.461889
3502.401713	471229.675372	46.466893
3502.405413	471216.848877	46.471898
3502.685071	471201.342587	46.476903
3502.613031	471209.617379	46.481908
3502.609016	471210.378485	46.486913
3502.785753	471213.493706	46.491917
3502.974272	471214.579246	46.496922
3503.068553	471211.319871	46.501927
3502.419655	471201.993121	46.506932
3502.792503	471185.458178	46.511937
3502.619519	471187.209209	46.516941
3502.706489	471177.309868	46.521946
3502.769196	471169.999832	46.526951
3502.491020	471179.574610	46.531956
3502.619853	471177.120897	46.536961
3502.682080	471174.018670	46.541965
3502.828722	471163.248065	46.546970
3502.846247	471133.588387	46.551975
3502.689190	471130.824990	46.556980
3502.805724	471130.553130	46.561985
3502.639615	471132.962123	46.566989
3502.519240	471131.257537	46.571994
3502.802914	471128.018907	46.576999
3502.596245	471105.187847	46.582004
3502.829562	471082.692780	46.587009
3502.566581	471085.066395	46.592013
3502.735711	471084.836916	46.597018
3502.491259	471078.437229	46.602023
3502.487659	471090.909002	46.607028
3502.924666	471082.525853	46.612033
3502.788356	471094.207469	46.617037
3502.677349	471070.398030	46.622042
3502.611818	471049.825911	46.627047
3502.271970	471046.533743	46.632052
3502.253179	471045.320051	46.637057
3502.415008	471053.304458	46.642061
3502.811210	471048.527152	46.647066
3503.075427	471046.609678	46.652071
3502.564171	471052.114991	46.657076
3502.701496	471044.387548	46.662081
3502.670530	471046.116142	46.667085
3502.706147	471027.961416	46.672090
3502.573395	471013.686181	46.677095
3502.688182	471013.211812	46.682100
3502.693201	471010.726955	46.687105
3502.851442	471005.480294	46.692109
3502.765752	471004.378567	46.697114
3502.910497	470994.267221	46.702119
3502.535553	470973.591848	46.707124
3502.882374	470961.370005	46.712129
3503.115833	470957.328148	46.717133
3502.784550	470959.408398	46.722138
3503.134610	470960.316328	46.727143
3502.569402	470931.762395	46.732148
3502.866207	470930.143936	46.737153
3502.812616	470925.336310	46.742157
3502.809119	470925.945256	46.747162
3502.736438	470913.992481	46.752167
3502.531768	470907.434364	46.757172
3502.712492	470881.094476	46.762177
3502.697800	470882.212156	46.767181
3502.582844	470884.004736	46.772186
3502.820001	470873.726635	46.777191
3502.804217	470880.928044	46.782196
3502.952211	470872.539799	46.787201
3502.432652	470860.252061	46.792205
3502.414086	470850.470638	46.797210
3502.829016	470839.150491	46.802215
3502.607516	470846.384430	46.807220
3503.067390	470835.310659	46.812225
3502.559880	470838.939669	46.817229
3502.355164	470845.106331	46.822234
3502.485094	470839.407836	46.827239
3502.607815	470841.467028	46.832244
3502.930437	470835.535287	46.837249
3502.745355	470822.079334	46.842253
3502.650440	470814.388517	46.847258
3502.525748	470802.139720	46.852263
3502.306956	470809.069065	46.857268
3502.469425	470792.668455	46.862273
3502.717961	470808.497209	46.867277
3502.687282	470806.626328	46.872282
3502.693818	470798.361807	46.877287
3502.872570	470800.006574	46.882292
3502.626843	470773.074904	46.887297
3502.634809	470762.326011	46.892301
3502.940346	470757.917846	46.897306
3502.875387	470752.300830	46.902311
3502.103012	470768.696565	46.907316
3503.091067	470762.913100	46.912321
3502.733028	470745.732890	46.917325
3502.566276	470730.448901	46.922330
3502.694337	470722.520016	46.927335
3502.476420	470721.794051	46.932340
3502.561858	470714.530958	46.937345
3502.514324	470728.074525	46.942349
3502.421437	470722.056343	46.947354
3502.837959	470714.335340	46.952359
3502.634102	470713.505759	46.957364
3502.454919	470717.691252	46.962369
3502.608718	470718.224643	46.967373
3502.630534	470708.639556	46.972378
3502.701369	470692.811016	46.977383
3502.699879	470691.645265	46.982388
3503.043978	470687.028203	46.987393
3502.700767	470697.373935	46.992397
3502.476137	470692.897471	46.997402
3502.787336	470690.668358	47.002407
3502.422680	470674.655159	47.007412
3502.491394	470657.610204	47.012417
3502.741002	470643.020789	47.017421
3502.426306	470641.803150	47.022426
3502.875910	470642.492572	47.027431
3502.663631	470652.209268	47.032436
3502.870538	470641.885137	47.037441
3502.740179	470650.879128	47.042445
3502.577747	470634.428357	47.047450
3503.087360	470597.034889	47.052455
3503.010238	470607.946969	47.057460
3502.921371	470601.218358	47.062465
3502.964794	470605.723564	47.067469
3502.645865	470584.025005	47.072474
3503.062670	470568.597955	47.077479
3502.769661	470575.336321	47.082484
3502.942628	470563.597999	47.087489
3503.186726	470563.052482	47.092493
3502.823930	470541.056630	47.097498
3502.908945	470530.954499	47.102503
3502.942465	470530.847845	47.107508
3502.819579	470525.037136	47.112513
3503.164379	470512.713953	47.117517
3502.977640	470484.048877	47.122522
3503.050487	470478.460700	47.127527
3502.728697	470487.991995	47.132532
3502.707974	470470.403353	47.137537
3502.368223	470444.500063	47.142541
3502.627913	470439.946986	47.147546
3502.823398	470422.881799	47.152551
3502.535652	470439.049095	47.157556
3503.005659	470437.301825	47.162561
3502.956472	470439.743113	47.167565
3502.892112	470427.839439	47.172570
3502.986763	470404.402301	47.177575
3502.755237	470395.820368	47.182580
3502.898866	470390.880046	47.187585
3502.989632	470386.302962	47.192589
3502.928002	470375.007196	47.197594
3502.740183	470359.371379	47.202599
3502.534166	470346.628191	47.207604
3502.672904	470354.160241	47.212609
3502.665715	470354.668393	47.217613
3502.706911	470355.270290	47.222618
3502.809573	470350.387133	47.227623
3502.665049	470329.269109	47.232628
3502.697681	470314.054690	47.237633
3502.576733	470309.105473	47.242637
3502.534171	470311.951311	47.247642
3502.710591	470304.470901	47.252647
3502.473929	470304.305559	47.257652
3502.463528	470308.413756	47.262657
3502.559379	470305.306083	47.267661
3502.575615	470304.492392	47.272666
3502.612492	470306.261022	47.277671
3502.465855	470293.407019	47.282676
3502.761628	470268.670493	47.287681
3502.799139	470261.566910	47.292685
3502.728109	470261.983759	47.297690
3502.762838	470254.982009	47.302695
3502.328810	470259.917647	47.307700
3502.511327	470263.133495	47.312705
3502.976959	470265.797612	47.317709
3502.812523	470249.853829	47.322714
3502.841483	470230.077122	47.327719
3502.488257	470231.552538	47.332724
3502.461502	470231.962389	47.337729
3502.738885	470219.903179	47.342733
3502.456653	470235.309293	47.347738
3502.517365	470226.275511	47.352743
3502.431337	470229.483116	47.357748
3502.746135	470218.634740	47.362753
3502.642110	470216.521910	47.367757
3502.723293	470194.506205	47.372762
3502.610583	470179.923038	47.377767
3502.447183	470189.936412	47.382772
3502.576973	470181.601463	47.387777
3502.843532	470182.776118	47.392781
3502.845307	470191.850818	47.397786
3502.741124	470187.760788	47.402791
3502.734864	470169.459833	47.407796
3502.523657	470159.201553	47.412801
3502.847385	470149.061502	47.417805
3502.447231	470145.068947	47.422810
3502.842282	470146.780973	47.427815
3502.239578	470153.213543	47.432820
3502.666802	470143.513412	47.437825
3502.978948	470145.542732	47.442829
3502.312450	470137.891315	47.447834
3502.572413	470135.771638	47.452839
3502.508062	470122.904522	47.457844
3502.622552	470100.731359	47.462849
3502.767170	470110.746780	47.467853
3502.693862	470107.970007	47.472858
3502.734448	470092.095091	47.477863
3502.513430	470103.030183	47.482868
3502.720602	470094.835061	47.487873
3502.792330	470096.953087	47.492877
3502.572416	470089.129663	47.497882
3502.527532	470066.069087	47.502887
3502.630371	470058.701616	47.507892
3503.075552	470054.068436	47.512897
3502.703951	470059.653331	47.517901
3502.517603	470060.139111	47.522906
3502.813481	470056.442102	47.527911
3502.832588	470058.872639	47.532916
3502.582246	470036.402188	47.537921
3502.554716	470027.230173	47.542925
3502.450388	470026.841116	47.547930
3502.824931	470027.035442	47.552935
3502.684871	470029.846032	47.557940
3502.664833	470030.204127	47.562945
3502.759643	470032.470606	47.567949
3502.590184	470018.758168	47.572954
3502.909061	469988.440829	47.577959
3502.507763	469993.776944	47.582964
3502.379513	469990.400458	47.587969
3502.969155	469996.593901	47.592973
3502.543100	469996.407795	47.597978
3502.355295	469993.091422	47.602983
3502.659262	469995.172747	47.607988
3502.667198	469991.115654	47.612993
3502.552455	469987.838430	47.617997
3502.388800	469976.406477	47.623002
3502.740955	469950.089005	47.628007
3502.549670	469950.778362	47.633012
3502.462105	469945.874480	47.638017
3502.545372	469936.837006	47.643021
3502.494181	469939.785656	47.648026
3502.534676	469948.093863	47.653031
3502.539968	469948.042367	47.658036
3502.927378	469946.460209	47.663041
3502.540887	469947.079026	47.668045
3502.369703	469954.964403	47.673050
3502.474607	469937.507547	47.678055
3502.548405	469933.642826	47.683060
3502.557495	469919.293714	47.688065
3502.653265	469913.144077	47.693069
3502.703655	469909.942134	47.698074
3502.625783	469901.741296	47.703079
3502.481211	469905.059602	47.708084
3502.777946	469904.809941	47.713089
3502.794954	469900.295108	47.718093
3502.523662	469902.923664	47.723098
3502.903292	469886.234516	47.728103
3502.601451	469878.829553	47.733108
3502.693202	469865.481313	47.738113
3502.849490	469857.496936	47.743117
3502.894589	469856.932160	47.748122
3502.959379	469863.867692	47.753127
3502.547368	469847.151553	47.758132
3502.494308	469829.516780	47.763137
3502.411203	469824.814960	47.768141
3502.221344	469820.180712	47.773146
3502.674853	469814.633583	47.778151
3502.704045	469823.298519	47.783156
3502.531728	469819.928970	47.788161
3502.611890	469817.178597	47.793165
3502.806482	469825.513194	47.798170
3502.784701	469823.133828	47.803175
3502.518765	469824.291279	47.808180
3502.742708	469811.885388	47.813185
3502.966173	469791.976119	47.818189
3502.531075	469788.090416	47.823194
3502.767510	469780.803127	47.828199
3503.042225	469788.922276	47.833204
3502.618658	469773.576777	47.838209
3502.685702	469756.531345	47.843213
3502.914703	469748.484733	47.848218
3502.583255	469741.642090	47.853223
3502.731506	469742.987570	47.858228
3502.657632	469738.537767	47.863233
3502.966954	469732.506417	47.868237
3502.354305	469734.073572	47.873242
3502.695029	469728.240054	47.878247
3502.828446	469709.663117	47.883252
3502.669527	469707.508213	47.888257
3502.710691	469689.807727	47.893261
3502.405462	469696.396212	47.898266
3502.819605	469693.542330	47.903271
3502.641217	469704.115999	47.908276
3502.479914	469697.347844	47.913281
3502.650847	469696.915270	47.918285
3502.483759	469676.763431	47.923290
3502.716043	469659.945296	47.928295
3502.753245	469652.993651	47.933300
3502.493152	469659.220117	47.938305
3502.438771	469652.130851	47.943309
3502.544599	469655.105420	47.948314
3502.534619	469647.502141	47.953319
3502.706539	469663.293184	47.958324
3502.751127	469655.275688	47.963329
3502.949238	469644.039863	47.968333
3502.729401	469635.151569	47.973338
3503.063226	469618.570846	47.978343
3502.812228	469618.610561	47.983348
3502.589153	469614.944806	47.988353
3502.761652	469610.557430	47.993357
3502.641932	469598.053636	47.998362
3503.158180	469566.741194	48.003367
3502.803012	469571.157533	48.008372
3502.599617	469569.313841	48.013377
3502.888591	469569.116103	48.018381
3502.646375	469566.923651	48.023386
3502.977126	469542.028631	48.028391
3502.863694	469531.703885	48.033396
3502.727930	469532.435179	48.038401
3502.671777	469525.498248	48.043405
3502.548475	469527.596462	48.048410
3502.478808	469526.897718	48.053415
3502.636577	469534.072162	48.058420
3502.300740	469506.037694	48.063425
3502.796041	469485.578166	48.068429
3502.724911	469486.147145	48.073434
3502.768086	469487.864149	48.078439
3502.878112	469486.376504	48.083444
3502.650909	469483.269076	48.088449
3502.815130	469486.994934	48.093453
3502.517904	469476.395015	48.098458
3502.471264	469455.362027	48.103463
3502.480477	469452.217222	48.108468
3502.250395	469446.828752	48.113473
3502.756598	469434.530118	48.118477
3502.688350	469451.930981	48.123482
3503.027058	469448.835492	48.128487
3502.629248	469432.116773	48.133492
3502.372216	469435.605030	48.138497
3502.712797	469438.846722	48.143501
3502.453170	469446.898371	48.148506
3502.902501	469425.533454	48.153511
3502.681478	469407.367174	48.158516
3502.145019	469400.759624	48.163521
3502.845397	469391.675065	48.168525
3502.546137	469410.734877	48.173530
3502.629497	469401.240857	48.178535
3502.676518	469407.570952	48.183540
3502.604465	469403.526388	48.188545
3502.530706	469402.067788	48.193549
3502.446123	469396.757706	48.198554
3502.540510	469396.185126	48.203559
3502.655632	469386.026978	48.208564
3502.632283	469380.960712	48.213569
3502.591691	469368.799172	48.218573
3502.607536	469374.272305	48.223578
3502.478720	469369.222707	48.228583
3502.537922	469375.449487	48.233588
3502.571939	469370.475550	48.238593
3502.985591	469374.060601	48.243597
3502.716460	469379.426679	48.248602
3502.444113	469351.381966	48.253607
3502.546589	469339.501994	48.258612
3502.291631	469324.028109	48.263617
3502.646424	469315.860046	48.268621
3502.281684	469320.227250	48.273626
3502.390781	469320.463545	48.278631
3502.299333	469322.708844	48.283636
3502.473471	469325.013561	48.288641
3502.506444	469320.039777	48.293645
3502.109707	469335.870259	48.298650
3502.401990	469316.101757	48.303655
3502.450111	469317.919394	48.308660
3502.400332	469336.128637	48.313665
3502.857843	469321.353328	48.318669
3502.255237	469323.527327	48.323674
3502.447814	469324.156026	48.328679
3502.382685	469330.503873	48.333684
3502.649077	469330.664603	48.338689
3502.685934	469326.450708	48.343693
3502.364423	469342.522794	48.348698
3502.660456	469323.717007	48.353703
3502.623673	469320.021752	48.358708
3502.588704	469298.074157	48.363713
3502.245070	469291.030491	48.368717
3502.330852	469290.205767	48.373722
3502.523413	469281.049331	48.378727
3502.442658	469283.546446	48.383732
3502.285577	469282.405210	48.388737
3502.318269	469282.602882	48.393741
3502.484836	469296.062842	48.398746
3502.196652	469291.697519	48.403751
3502.334299	469286.960682	48.408756
3502.373353	469290.807762	48.413761
3502.532786	469278.056848	48.418765
3502.183074	469292.561724	48.423770
3502.315414	469281.944503	48.428775
3502.268293	469291.382227	48.433780
3502.371574	469292.836245	48.438785
3502.785374	469288.917659	48.443789
3502.440625	469293.687311	48.448794
3502.779058	469289.425738	48.453799
3502.764893	469289.428015	48.458804
3502.540844	469291.035176	48.463809
3502.761097	469283.902372	48.468813
3502.662588	469287.669797	48.473818
3502.486629	469258.494318	48.478823
3502.597782	469257.513482	48.483828
3502.279493	469259.845345	48.488833
3502.697778	469239.955453	48.493837
3502.701329	469251.717399	48.498842
3502.841239	469248.298403	48.503847
3502.672192	469258.008917	48.508852
3502.457572	469262.098902	48.513857
3502.543818	469248.548335	48.518861
3502.342921	469255.576769	48.523866
3502.403702	469253.082887	48.528871
3502.398587	469259.624069	48.533876
3502.438273	469249.224278	48.538881
3502.484401	469221.788152	48.543885
3502.384993	469221.854605	48.548890
3502.463156	469222.450692	48.553895
3502.648303	469217.250028	48.558900
3502.260122	469214.421507	48.563905
3502.524030	469208.853488	48.568909
3502.618088	469219.536437	48.573914
3502.615976	469213.300665	48.578919
3502.378519	469223.833214	48.583924
3502.248293	469224.715744	48.588929
3502.550689	469217.468532	48.593933
3502.462524	469220.118926	48.598938
3502.618583	469215.328462	48.603943
3502.737312	469215.208332	48.608948
3502.175652	469223.054309	48.613953
3502.661181	469216.133051	48.618957
3502.597083	469227.246600	48.623962
3502.695260	469204.162452	48.628967
3502.421006	469186.917000	48.633972
3502.268330	469182.580934	48.638977
3502.781943	469178.038145	48.643981
3502.492820	469177.627582	48.648986
3502.391404	469180.736380	48.653991
3502.948423	469177.504941	48.658996
3502.802458	469179.454671	48.664001
3502.648763	469174.763861	48.669005
3502.614550	469182.678580	48.674010
3502.638091	469160.670891	48.679015
3502.684957	469155.846973	48.684020
3502.516844	469150.854235	48.689025
3502.622342	469141.356596	48.694029
3502.517535	469135.998943	48.699034
3502.598678	469137.456472	48.704039
3502.472135	469139.403135	48.709044
3502.506801	469137.876678	48.714049
3502.718421	469142.558417	48.719053
3502.698505	469146.212043	48.724058
3502.869697	469129.251034	48.729063
3502.803240	469101.224139	48.734068
3502.402714	469104.126726	48.739073
3502.861646	469087.830009	48.744077
3502.522991	469096.654795	48.749082
3502.455306	469094.536106	48.754087
3502.575042	469098.269066	48.759092
3502.491893	469097.116134	48.764097
3502.589505	469086.909908	48.769101
3502.826337	469099.902582	48.774106
3502.723370	469074.669957	48.779111
3502.571096	469069.725396	48.784116
3502.507395	469068.214483	48.789121
3503.033042	469059.360203	48.794125
3502.957885	469060.335437	48.799130
3502.816548	469062.233745	48.804135
3502.726420	469030.205136	48.809140
3502.861930	469023.643348	48.814145
3502.667110	469018.299893	48.819149
3502.542635	469024.707914	48.824154
3502.807033	469013.968280	48.829159
3502.885142	469008.632381	48.834164
3502.449472	469002.769284	48.839169
3502.762401	468980.512857	48.844173
3502.622110	468979.875959	48.849178
3502.487208	468978.984706	48.854183
3502.754162	468976.711705	48.859188
3502.904082	468979.324495	48.864193
3502.723244	468976.209660	48.869197
3502.662696	468979.413430	48.874202
3502.919275	468952.045084	48.879207
3503.042955	468929.869218	48.884212
3502.540551	468935.576491	48.889217
3502.822768	468932.641959	48.894221
3502.582385	468936.533276	48.899226
3502.543030	468923.762868	48.904231
3502.519013	468918.443089	48.909236
3502.365964	468903.916102	48.914241
3502.588082	468893.639399	48.919245
3502.393508	468893.619494	48.924250
3502.276441	468885.323047	48.929255
3502.615008	468887.500419	48.934260
3502.663925	468894.438785	48.939265
3502.778926	468887.626690	48.944269
3502.549011	468891.161452	48.949274
3502.110441	468887.478931	48.954279
3502.472908	468890.463743	48.959284
3502.527928	468892.584534	48.964289
3502.631789	468881.768806	48.969293
3502.375978	468901.126423	48.974298
3502.268834	468894.248043	48.979303
3502.637803	468894.341862	48.984308
3502.207218	468891.215791	48.989313
3502.652299	468882.931886	48.994317
3502.579435	468888.976882	48.999322
3502.562611	468866.113342	49.004327
3502.534837	468859.526612	49.009332
3502.165115	468851.827803	49.014337
3502.368620	468841.908926	49.019341
3502.221140	468847.103807	49.024346
3502.514786	468843.305535	49.029351
3502.622739	468834.517187	49.034356
3502.552311	468851.107676	49.039361
3502.603842	468842.378951	49.044365
3502.791233	468840.422720	49.049370
3502.994020	468848.046596	49.054375
3502.683838	468846.321122	49.059380
3502.858948	468836.710939	49.064385
3503.087643	468817.104120	49.069389
3502.793059	468812.942513	49.074394
3502.667334	468807.638783	49.079399
3502.702107	468807.531922	49.084404
3502.383715	468812.551023	49.089409
3502.926452	468797.102755	49.094413
3502.783234	468783.182547	49.099418
3502.908694	468769.067754	49.104423
3502.574875	468762.022355	49.109428
3502.267120	468773.073258	49.114433
3502.727244	468758.449244	49.119437
3502.508989	468764.567960	49.124442
3502.187119	468756.506641	49.129447
3502.775617	468765.692025	49.134452
3502.324665	468771.594014	49.139457
3502.469127	468760.011284	49.144461
3502.353275	468756.835443	49.149466
3502.397857	468763.064716	49.154471
3502.631378	468752.279127	49.159476
3502.566618	468740.982966	49.164481
3502.909380	468733.323593	49.169485
3502.652732	468738.130146	49.174490
3502.777250	468729.237732	49.179495
3502.594480	468729.368065	49.184500
3502.682186	468734.170887	49.189505
3502.806017	468728.219270	49.194509
3502.793833	468710.982699	49.199514
3502.552129	468699.156767	49.204519
3502.629263	468692.451998	49.209524
3502.556491	468688.863723	49.214529
3502.678262	468687.931883	49.219533
3502.549130	468698.548978	49.224538
3502.527898	468698.501671	49.229543
3502.692475	468688.081858	49.234548
3502.696116	468684.836416	49.239553
3502.879319	468669.292781	49.244557
3502.540797	468663.363530	49.249562
3502.616164	468651.740960	49.254567
3502.360998	468653.353087	49.259572
3502.452052	468651.817681	49.264577
3503.021456	468643.108415	49.269581
3502.676332	468654.773708	49.274586
3502.757892	468649.589278	49.279591
3502.546637	468622.953574	49.284596
3502.474732	468612.672509	49.289601
3502.594207	468602.563994	49.294605
3502.715789	468606.347454	49.299610
3503.057902	468604.417445	49.304615
3503.095895	468608.923943	49.309620
3502.334843	468593.935128	49.314625
3502.600512	468573.358900	49.319629
3502.610666	468572.901016	49.324634
3502.692627	468567.108078	49.329639
3502.864555	468566.117603	49.334644
3502.753939	468563.549327	49.339649
3502.594129	468568.442015	49.344653
3502.724718	468570.601595	49.349658
3502.594778	468553.332805	49.354663
3502.562670	468536.859769	49.359668
3502.605899	468526.154846	49.364673
3503.013903	468512.350131	49.369677
3503.079992	468514.469211	49.374682
3502.793983	468523.894341	49.379687
3502.678818	468509.868112	49.384692
3502.627625	468481.178842	49.389697
3502.686845	468477.569667	49.394701
3502.534254	468480.382445	49.399706
3502.844435	468481.905219	49.404711
3503.012250	468475.439557	49.409716
3502.546537	468472.065464	49.414721
3502.606693	468468.304033	49.419725
3502.692523	468444.308356	49.424730
3502.561477	468439.157480	49.429735
3502.707233	468437.004984	49.434740
3502.422742	468440.649853	49.439745
3502.910106	468428.100095	49.444749
3502.644444	468440.868397	49.449754
3502.573210	468437.482645	49.454759
3502.783384	468425.686533	49.459764
3502.524740	468412.950476	49.464769
3502.539994	468400.019007	49.469773
3502.630872	468399.700467	49.474778
3502.266483	468405.436768	49.479783
3502.465200	468397.394424	49.484788
3502.527232	468404.077368	49.489793
3502.726851	468388.023906	49.494797
3502.702002	468395.988145	49.499802
3502.677022	468393.710526	49.504807
3502.696950	468385.088011	49.509812
3502.298618	468393.212693	49.514817
3502.850614	468389.677715	49.519821
3502.876127	468368.480117	49.524826
3502.630871	468359.189675	49.529831
3502.618720	468351.079240	49.534836
3502.434172	468357.699772	49.539841
3502.651356	468353.000853	49.544845
3502.400059	468361.406521	49.549850
3502.605856	468356.557296	49.554855
3502.571567	468348.450360	49.559860
3502.492092	468357.234488	49.564865
3502.678928	468334.287471	49.569869
3502.639942	468328.868503	49.574874
3502.549170	468314.584773	49.579879
3502.488566	468315.659145	49.584884
3502.994030	468313.652587	49.589889
3502.839998	468304.094188	49.594893
3502.796161	468304.760290	49.599898
3502.617140	468297.943777	49.604903
3502.571685	468278.278383	49.609908
3502.500847	468271.444760	49.614913
3502.512057	468259.578600	49.619917
3502.819555	468270.228298	49.624922
3502.764887	468266.738494	49.629927
3503.112530	468256.745853	49.634932
3502.755040	468264.052886	49.639937
3503.020106	468236.479451	49.644941
3502.705761	468229.988523	49.649946
3502.440421	468222.019466	49.654951
3502.499689	468220.235539	49.659956
3502.303674	468232.840851	49.664961
3502.479065	468225.968291	49.669965
3502.596920	468223.059642	49.674970
3502.272464	468219.865991	49.679975
3502.634968	468225.639548	49.684980
3502.416432	468229.020514	49.689985
3502.738196	468225.014874	49.694989
3502.736427	468210.666302	49.699994
3502.593705	468194.413292	49.704999
3502.642330	468177.115965	49.710004
3502.669498	468179.038420	49.715009
3502.467297	468170.957957	49.720013
3502.434990	468169.340610	49.725018
3502.501515	468177.442597	49.730023
3502.616637	468175.193511	49.735028
3502.482952	468178.155450	49.740033
3502.596782	468173.117909	49.745037
3502.622892	468171.896950	49.750042
3502.544899	468161.667328	49.755047
3502.806372	468143.018052	49.760052
3502.587555	468134.483875	49.765057
3502.596327	468130.426287	49.770061
3502.513609	468140.326485	49.775066
3502.605170	468132.960117	49.780071
3502.884164	468135.856828	49.785076
3502.544925	468137.025957	49.790081
3502.695044	468132.692512	49.795085
3502.759338	468109.054776	49.800090
3502.496718	468105.192192	49.805095
3502.509997	468087.342644	49.810100
3502.887113	468092.809710	49.815105
3502.456723	468096.984732	49.820109
3502.494721	468087.243769	49.825114
3502.700473	468093.853391	49.830119
3502.545634	468090.582204	49.835124
3502.407318	468104.040425	49.840129
3502.511133	468105.950771	49.845133
3502.464229	468098.606278	49.850138
3502.122444	468107.431975	49.855143
3502.576079	468097.574613	49.860148
3502.422792	468103.024112	49.865153
3502.468113	468097.693164	49.870157
3502.618085	468081.241690	49.875162
3502.409931	468078.384554	49.880167
3502.470410	468068.437216	49.885172
3502.597804	468073.538136	49.890177
3502.370667	468066.222122	49.895181
3502.872039	468078.007444	49.900186
3502.269751	468074.959094	49.905191
3502.260792	468066.442419	49.910196
3502.072271	468078.133982	49.915201
3502.354089	468072.005096	49.920205
3502.224309	468071.265103	49.925210
3502.471237	468068.640248	49.930215
3502.158231	468069.298203	49.935220
3502.220037	468076.640428	49.940225
3502.223728	468066.042925	49.945229
3501.925091	468074.354784	49.950234
3501.931293	468074.505952	49.955239
3502.253300	468085.001342	49.960244
3502.368032	468096.949177	49.965249
3502.245213	468101.481204	49.970253
3502.417968	468098.918781	49.975258
3502.204055	468107.318641	49.980263
3502.638064	468092.394072	49.985268
3502.104518	468107.638671	49.990273
3502.472508	468107.631244	49.995277
3502.547336	468108.532110	50.000282
3502.226475	468103.056234	50.005287
3502.201998	468106.660060	50.010292
3502.305901	468104.007115	50.015297
3502.272459	468109.488371	50.020301
3502.147022	468101.852075	50.025306
3502.286580	468106.241221	50.030311
3502.782301	468097.796892	50.035316
3502.504589	468106.358946	50.040321
3502.352021	468095.532643	50.045325
3502.408816	468093.698393	50.050330
3502.363854	468091.322494	50.055335
3502.497290	468086.636754	50.060340
3502.207535	468084.654471	50.065345
3502.623055	468087.935233	50.070349
3502.880003	468090.379107	50.075354
3502.610274	468086.213425	50.080359
3502.815603	468082.074054	50.085364
3502.649329	468084.736939	50.090369
3502.828623	468084.607230	50.095373
3502.923442	468070.091184	50.100378
3502.461457	468049.680166	50.105383
3502.429046	468034.930691	50.110388
3502.424828	468038.531327	50.115393
3502.457082	468041.923383	50.120397
3502.481603	468035.835159	50.125402
3502.491745	468030.966083	50.130407
3502.696708	468024.849332	50.135412
3502.584383	468035.311996	50.140417
3502.324502	468032.361624	50.145421
3502.539696	468036.688125	50.150426
3502.573576	468035.719447	50.155431
3502.641321	468028.052587	50.160436
3502.600428	468040.075758	50.165441
3502.754335	468031.584028	50.170445
3502.450432	468010.539545	50.175450
3502.364043	468000.057654	50.180455
3502.566028	467989.276658	50.185460
3502.289075	468000.170989	50.190465
3502.647851	467983.432916	50.195469
3502.748694	467983.518421	50.200474
3502.512806	467995.471034	50.205479
3502.679940	467992.250343	50.210484
3502.335544	467997.121639	50.215489
3502.896312	467992.317625	50.220493
3502.722701	467989.962050	50.225498
3502.465772	467967.034074	50.230503
3502.626064	467956.462464	50.235508
3502.435350	467956.289836	50.240513
3502.291658	467949.416921	50.245517
3502.368777	467948.745625	50.250522
3502.151722	467958.109407	50.255527
3502.375075	467956.400926	50.260532
3502.246606	467956.522680	50.265537
3502.535547	467944.663143	50.270541
3502.435283	467949.191638	50.275546
3502.118455	467961.968320	50.280551
3502.357035	467946.364691	50.285556
3502.466344	467950.707948	50.290561
3502.547819	467954.193645	50.295565
3502.701036	467943.268223	50.300570
3502.499303	467959.474548	50.305575
3502.476304	467955.776873	50.310580
3502.377573	467964.310693	50.315585
3502.628109	467955.905065	50.320589
3502.283375	467963.818627	50.325594
3502.233334	467961.544922	50.330599
3502.787026	467948.477359	50.335604
3502.120184	467957.810833	50.340609
3502.497311	467951.869660	50.345613
3502.432022	467958.775686	50.350618
3502.201752	467959.369862	50.355623
3502.287734	467959.508420	50.360628
3502.624678	467962.243885	50.365633
3502.765590	467958.571003	50.370637
3502.568855	467947.903715	50.375642
3502.367103	467934.397821	50.380647
3502.835421	467919.062078	50.385652
3502.646043	467927.306020	50.390657
3502.650257	467919.395646	50.395661
3502.576112	467920.421475	50.400666
3502.282765	467926.095974	50.405671
3502.425990	467923.031163	50.410676
3502.013244	467927.051319	50.415681
3502.426977	467912.788973	50.420685
3502.774133	467912.074990	50.425690
3502.470773	467931.339613	50.430695
3502.638340	467920.817539	50.435700
3502.655773	467925.783766	50.440705
3502.394954	467909.701314	50.445709
3502.520579	467888.690218	50.450714
3502.563909	467869.923070	50.455719
3502.328981	467874.726386	50.460724
3502.128870	467882.465007	50.465729
3502.003330	467877.515936	50.470733
3502.610233	467890.450866	50.475738
3502.524033	467891.072974	50.480743
3502.469646	467874.501531	50.485748
3502.217526	467855.679665	50.490753
3502.449698	467824.156000	50.495757
3502.253519	467785.753573	50.500762
3501.923433	467735.406110	50.505767
3502.155398	467669.707747	50.510772
3501.876337	467604.698408	50.515777
3502.070714	467527.292848	50.520781
3502.331503	467427.414332	50.525786
3501.440618	467332.939999	50.530791
3501.566871	467215.740647	50.535796
3501.417056	467100.764618	50.540801
3501.428599	466965.632252	50.545805
3500.949589	466828.649728	50.550810
3500.391139	466691.171806	50.555815
3500.529867	466534.821251	50.560820
3499.999112	466390.187319	50.565825
3499.733821	466216.049324	50.570829
3499.834910	466052.500664	50.575834
3499.348359	465878.546987	50.580839
3499.015504	465686.870189	50.585844
3498.770615	465502.074222	50.590849
3498.475521	465304.759262	50.595853
3498.390291	465096.050190	50.600858
3498.054214	464880.786316	50.605863
3497.730259	464667.090399	50.610868
3497.143640	464448.616235	50.615873
3496.794887	464216.815587	50.620877
3496.338576	463980.617398	50.625882
3495.756976	463752.651994	50.630887
3495.402716	463510.854001	50.635892
3495.015915	463262.364091	50.640897
3494.852463	463009.880209	50.645901
3494.455090	462757.481055	50.650906
3493.676091	462497.379650	50.655911
3493.349593	462227.770198	50.660916
3492.698946	461972.206707	50.665921
3492.210869	461700.333917	50.670925
3492.257912	461413.664615	50.675930
3491.538442	461139.640450	50.680935
3491.245300	460839.120148	50.685940
3490.676851	460562.173767	50.690945
3489.906207	460261.619532	50.695949
3489.593441	459968.698577	50.700954
3489.104871	459667.229290	50.705959
3488.830706	459360.751028	50.710964
3488.093860	459053.935828	50.715969
3487.258510	458747.689890	50.720973
3487.138739	458426.210245	50.725978
3486.342730	458118.579737	50.730983
3486.069034	457799.702354	50.735988
3485.404936	457486.462181	50.740993
3484.715337	457166.626863	50.745997
3484.381526	456831.917658	50.751002
3483.868382	456510.472383	50.756007
3483.494446	456171.396781	50.761012
3482.498940	455855.750931	50.766017
3482.004274	455513.285394	50.771021
3481.414676	455164.082091	50.776026
3480.995271	454825.906496	50.781031
3480.542719	454494.935409	50.786036
3479.544579	454146.947797	50.791041
3479.084378	453803.537533	50.796045
3478.496016	453457.554717	50.801050
3477.608333	453102.937741	50.806055
3477.037709	452753.186767	50.811060
3476.621420	452408.429234	50.816065
3476.018540	452067.704471	50.821069
3475.642210	451713.340203	50.826074
3474.999955	451364.594095	50.831079
3474.314553	451002.148988	50.836084
3473.209381	450653.211541	50.841089
3472.858463	450292.630630	50.846093
3471.990282	449939.230161	50.851098
3471.194823	449579.723300	50.856103
3470.880107	449217.445292	50.861108
3469.948336	448867.743034	50.866113
3469.279745	448509.620475	50.871117
3468.989268	448156.812024	50.876122
3468.113173	447792.367652	50.881127
3467.397787	447426.724941	50.886132
3466.757842	447077.102001	50.891137
3466.331335	446714.701368	50.896141
3465.641214	446348.124357	50.901146
3464.647751	445993.922730	50.906151
3464.205084	445621.864705	50.911156
3463.388129	445260.873883	50.916161
3462.378187	444904.476119	50.921165
3461.888164	444539.666734	50.926170
3461.086922	444187.793364	50.931175
3460.531289	443833.845662	50.936180
3459.706052	443480.392188	50.941185
3459.224463	443114.849142	50.946189
3458.725999	442764.125264	50.951194
3457.813474	442411.380541	50.956199
3457.431106	442040.374089	50.961204
3456.462331	441681.790004	50.966209
3456.068320	441318.947154	50.971213
3455.599793	440957.684367	50.976218
3454.579879	440598.178647	50.981223
3454.158243	440238.623819	50.986228
3453.177373	439882.604247	50.991233
3452.803794	439517.294643	50.996237
3451.999124	439149.864751	51.001242
3451.360092	438784.484715	51.006247
3450.769399	438419.243946	51.011252
3449.918959	438062.999795	51.016257
3449.120748	437700.370528	51.021261
3448.445831	437335.000202	51.026266
3447.626739	436976.196957	51.031271
3447.073710	436612.751531	51.036276
3446.180488	436263.190491	51.041281
3445.595742	435901.643796	51.046285
3445.132732	435536.543780	51.051290
3444.535270	435192.379453	51.056295
3444.187502	434818.390428	51.061300
3443.183212	434453.741183	51.066305
3442.350054	434094.188243	51.071309
3441.869625	433731.476946	51.076314
3440.848898	433362.676191	51.081319
3440.169516	433002.271081	51.086324
3439.599804	432648.368931	51.091329
3438.625540	432290.158638	51.096333
3438.178589	431924.191840	51.101338
3437.624019	431587.843456	51.106343
3436.936618	431212.433541	51.111348
3436.159673	430857.600107	51.116353
3435.419187	430497.499790	51.121357
3435.007855	430144.630242	51.126362
3434.158489	429781.921787	51.131367
3433.241555	429420.412491	51.136372
3432.428325	429071.908952	51.141377
3431.942215	428720.428725	51.146381
3431.360798	428364.108494	51.151386
3430.385385	428007.769567	51.156391
3430.072172	427658.685806	51.161396
3429.566089	427305.869386	51.166401
3428.068969	426945.738540	51.171405
3427.903050	426593.569994	51.176410
3426.944266	426250.664989	51.181415
3426.481460	425897.442168	51.186420
3425.722293	425551.855376	51.191425
3425.069207	425199.847155	51.196429
3424.469721	424849.476740	51.201434
3423.654710	424499.364449	51.206439
3422.948425	424146.411192	51.211444
3422.296440	423794.663919	51.216449
3421.913101	423449.448060	51.221453
3421.160460	423089.605218	51.226458
3420.198916	422741.500080	51.231463
3419.577059	422392.193802	51.236468
3418.735386	422043.654462	51.241473
3418.071355	421695.031827	51.246477
3417.675069	421360.612579	51.251482
3417.040322	421010.630424	51.256487
3416.140180	420654.919587	51.261492
3415.651491	420301.806382	51.266497
3414.908622	419956.324264	51.271501
3414.126013	419610.361509	51.276506
3413.297031	419260.057873	51.281511
3412.849612	418910.832697	51.286516
3411.826528	418570.102878	51.291521
3410.755055	418225.565981	51.296525
3410.517842	417875.913712	51.301530
3409.466004	417548.437252	51.306535
3408.844614	417206.128642	51.311540
3408.500151	416869.767795	51.316545
3407.849849	416525.753445	51.321549
3406.872148	416183.361901	51.326554
3406.022267	415852.175619	51.331559
3405.739521	415512.740359	51.336564
3405.012881	415178.198594	51.341569
3404.265920	414831.460757	51.346573
3403.736298	414490.528117	51.351578
3402.960371	414161.140121	51.356583
3402.334845	413825.169358	51.361588
3401.795832	413483.311736	51.366593
3401.199389	413145.016409	51.371597
3400.274307	412800.137431	51.376602
3399.662071	412467.452169	51.381607
3399.228047	412126.502311	51.386612
3398.219661	411787.113110	51.391617
3397.224736	411455.163041	51.396621
3396.887209	411105.216438	51.401626
3395.967056	410776.956893	51.406631
3395.436065	410452.088087	51.411636
3394.847051	410113.350429	51.416641
3393.827256	409774.880359	51.421645
3393.132692	409438.032232	51.426650
3392.511775	409113.518949	51.431655
3392.158500	408773.560006	51.436660
3391.413279	408442.680701	51.441665
3390.514153	408111.720481	51.446669
3390.200550	407767.932094	51.451674
3388.986908	407437.497146	51.456679
3388.624199	407117.547003	51.461684
3388.061386	406786.595511	51.466689
3387.127958	406454.555426	51.471693
3386.565135	406116.048709	51.476698
3385.563567	405786.756992	51.481703
3385.405567	405466.426978	51.486708
3384.561009	405136.951056	51.491713
3383.751602	404815.548250	51.496717
3383.388026	404473.561051	51.501722
3382.612430	404142.665875	51.506727
3381.862671	403809.297739	51.511732
3381.463137	403469.338612	51.516737
3380.512881	403144.560573	51.521741
3379.880896	402815.458787	51.526746
3378.894919	402487.934615	51.531751
3378.745344	402161.825292	51.536756
3377.849251	401826.451454	51.541761
3377.077917	401498.018972	51.546765
3376.272462	401164.403149	51.551770
3375.739158	400839.434048	51.556775
3375.486813	400523.034291	51.561780
3374.266531	400185.228964	51.566785
3373.802436	399856.553249	51.571789
3373.311171	399519.744176	51.576794
3372.231557	399192.608023	51.581799
3371.638773	398873.729468	51.586804
3370.982826	398546.265655	51.591809
3370.153582	398226.020069	51.596813
3369.851740	397891.731813	51.601818
3368.785990	397569.559834	51.606823
3368.305656	397240.885914	51.611828
3367.613082	396912.699897	51.616833
3366.950201	396594.522240	51.621837
3366.626399	396253.077371	51.626842
3365.603958	395942.449949	51.631847
3364.940315	395605.857092	51.636852
3364.340140	395288.140154	51.641857
3363.268224	394961.494987	51.646861
3362.781985	394631.703224	51.651866
3362.008477	394314.970658	51.656871
3360.903201	393997.194377	51.661876
3360.672906	393674.649554	51.666881
3359.790884	393367.510292	51.671885
3359.456083	393040.882691	51.676890
3358.014260	392724.927560	51.681895
3357.493124	392408.239156	51.686900
3357.182727	392083.836051	51.691905
3356.370032	391780.409229	51.696909
3355.959627	391468.500179	51.701914
3355.145811	391147.829280	51.706919
3354.723333	390827.678359	51.711924
3353.909135	390505.704897	51.716929
3353.219866	390195.430483	51.721933
3352.800624	389866.599764	51.726938
3351.499483	389553.136381	51.731943
3350.791304	389236.779430	51.736948
3350.523120	388929.987180	51.741953
3349.558123	388614.097581	51.746957
3349.178848	388291.730096	51.751962
3348.412734	387978.498821	51.756967
3347.688237	387657.833084	51.761972
3346.934031	387349.959890	51.766977
3346.071753	387044.059201	51.771981
3345.900492	386724.416571	51.776986
3344.996332	386409.947503	51.781991
3344.538042	386099.270523	51.786996
3344.090124	385782.994683	51.792001
3342.757992	385471.153643	51.797005
3342.251009	385154.017103	51.802010
3341.848519	384847.287839	51.807015
3340.783815	384520.824757	51.812020
3340.020830	384206.746843	51.817025
3339.053953	383905.236107	51.822029
3339.006974	383591.319512	51.827034
3337.927064	383292.364846	51.832039
3337.361402	382981.398943	51.837044
3336.877464	382662.253860	51.842049
3336.071151	382362.689032	51.847053
3335.430696	382047.530941	51.852058
3334.683584	381741.695456	51.857063
3334.234727	381433.241624	51.862068
3333.498450	381120.481701	51.867073
3332.728896	380812.022710	51.872077
3332.421319	380498.045413	51.877082
3331.544494	380196.058551	51.882087
3330.727760	379880.757901	51.887092
3330.281048	379565.294427	51.892097
3329.429028	379261.770312	51.897101
3328.989357	378940.705116	51.902106
3327.848998	378646.937802	51.907111
3327.567666	378339.984326	51.912116
3326.959032	378031.045412	51.917121
3325.825801	377722.721187	51.922125
3325.173252	377402.618206	51.927130
3324.864699	377102.806798	51.932135
3324.159664	376806.006400	51.937140
3323.529489	376485.510966	51.942145
3322.483467	376192.956899	51.947149
3322.210635	375876.317265	51.952154
3321.235568	375570.418734	51.957159
3320.738147	375256.048179	51.962164
3320.250421	374957.953368	51.967169
3319.144282	374654.815856	51.972173
3319.051940	374336.405915	51.977178
3318.326647	374031.193983	51.982183
3317.488193	373714.855914	51.987188
3316.705846	373413.972851	51.992193
3316.056091	373104.900964	51.997197
3315.893632	372791.654120	52.002202
3314.776178	372488.044547	52.007207
3314.099295	372176.502503	52.012212
3313.705576	371864.913354	52.017217
3312.718472	371558.427251	52.022221
3312.281113	371242.210463	52.027226
3311.446118	370939.664339	52.032231
3310.700699	370634.710556	52.037236
3310.259858	370328.841455	52.042241
3309.285199	370023.766911	52.047245
3308.985494	369703.700895	52.052250
3307.752753	369396.729246	52.057255
3307.523090	369100.688862	52.062260
3306.874152	368792.373984	52.067265
3305.718113	368486.096072	52.072269
3305.491673	368180.762940	52.077274
3304.834394	367873.104331	52.082279
3304.238682	367562.508049	52.087284
3303.733844	367255.736890	52.092289
3302.764380	366947.943084	52.097293
3301.881560	366643.440894	52.102298
3301.211182	366344.296760	52.107303
3300.740956	366019.854671	52.112308
3299.973450	365713.750452	52.117313
3299.319385	365422.128556	52.122317
3298.886055	365104.339996	52.127322
3297.818299	364798.989440	52.132327
3297.203485	364499.086366	52.137332
3296.855189	364193.974144	52.142337
3296.023203	363889.597917	52.147341
3295.486305	363583.468258	52.152346
3294.663704	363283.208405	52.157351
3293.805276	362981.654612	52.162356
3293.164039	362672.558441	52.167361
3292.501376	362370.664371	52.172365
3291.972320	362069.739548	52.177370
3291.321411	361767.737935	52.182375
3290.606547	361451.469888	52.187380
3290.123049	361151.651539	52.192385
3289.119200	360844.992481	52.197389
3288.606373	360546.040068	52.202394
3287.709907	360254.194878	52.207399
3287.188858	359946.868409	52.212404
3286.517649	359640.301648	52.217409
3285.573455	359349.425432	52.222413
3285.022603	359049.375502	52.227418
3284.290663	358745.789863	52.232423
3283.236568	358453.449751	52.237428
3282.884388	358156.212885	52.242433
3282.185067	357856.917033	52.247437
3281.546553	357561.503125	52.252442
3280.834839	357265.208374	52.257447
3280.302118	356979.418710	52.262452
3279.909679	356669.302907	52.267457
3279.005912	356379.166073	52.272461
3278.311836	356075.125365	52.277466
3277.997540	355781.787200	52.282471
3276.865240	355480.458790	52.287476
3276.186041	355179.794909	52.292481
3275.460869	354897.637462	52.297485
3275.121705	354584.522927	52.302490
3274.295920	354303.243353	52.307495
3273.570569	354010.010872	52.312500
3273.009823	353699.801695	52.317505
3271.997108	353413.151649	52.322509
3271.522523	353111.985189	52.327514
3271.030422	352820.312370	52.332519
3270.376720	352530.343152	52.337524
3269.737514	352233.574981	52.342529
3268.730319	351937.346891	52.347533
3268.463862	351638.531325	52.352538
3267.361468	351353.309397	52.357543
3266.733891	351056.634587	52.362548
3266.274335	350755.477740	52.367553
3265.274527	350474.001542	52.372557
3264.797066	350181.039366	52.377562
3264.402815	349887.680678	52.382567
3263.545790	349592.612045	52.387572
3262.904062	349291.526762	52.392577
3262.256515	349001.791970	52.397581
3261.449733	348700.093268	52.402586
3260.852188	348412.918049	52.407591
3260.039613	348118.750717	52.412596
3259.975859	347821.663686	52.417601
3258.987240	347527.750146	52.422605
3258.319469	347234.598774	52.427610
3257.443981	346949.903384	52.432615
3256.723648	346654.313906	52.437620
3256.349682	346355.537453	52.442625
3255.542404	346064.769162	52.447629
3255.364060	345760.715433	52.452634
3254.405242	345465.921104	52.457639
3253.788561	345176.238086	52.462644
3253.059229	344876.644756	52.467649
3252.302474	344587.668190	52.472653
3251.607647	344288.855428	52.477658
3251.038354	343992.439360	52.482663
3250.137129	343702.004985	52.487668
3249.434619	343416.119410	52.492673
3248.786621	343115.842442	52.497677
3248.186856	342816.370857	52.502682
3247.670962	342531.902398	52.507687
3246.994228	342233.509152	52.512692
3246.530109	341932.484461	52.517697
3245.684267	341644.704054	52.522701
3244.801564	341349.011757	52.527706
3243.999654	341060.356193	52.532711
3243.567338	340764.208011	52.537716
3242.996219	340468.742195	52.542721
3242.046047	340178.705946	52.547725
3241.829377	339886.694086	52.552730
3240.833672	339596.840525	52.557735
3240.071356	339302.544927	52.562740
3239.528637	339010.173292	52.567745
3238.480315	338719.891288	52.572749
3237.901913	338421.616890	52.577754
3237.296493	338145.975625	52.582759
3236.771191	337851.864938	52.587764
3235.958842	337559.554792	52.592769
3235.196645	337282.814581	52.597773
3234.505680	336987.809765	52.602778
3234.250789	336701.975312	52.607783
3233.436576	336423.254099	52.612788
3232.997708	336127.645505	52.617793
3232.031293	335840.265210	52.622797
3231.488261	335552.231191	52.627802
3230.878549	335271.792657	52.632807
3230.069617	334977.535831	52.637812
3229.536271	334682.419500	52.642817
3228.313828	334403.576278	52.647821
3228.195820	334104.827723	52.652826
3226.841725	333823.457229	52.657831
3226.403355	333539.140383	52.662836
3225.768602	333248.081693	52.667841
3225.246224	332977.421169	52.672845
3224.423072	332690.259546	52.677850
3223.889903	332406.920493	52.682855
3223.344103	332120.629163	52.687860
3222.658647	331833.824152	52.692865
3221.488316	331554.426693	52.697869
3221.465771	331265.732451	52.702874
3220.953983	330987.272402	52.707879
3219.973421	330707.612515	52.712884
3219.635871	330404.427813	52.717889
3218.611923	330127.394818	52.722893
3217.909036	329831.699523	52.727898
3217.320794	329545.379287	52.732903
3216.315139	329262.128161	52.737908
3216.031798	328976.572197	52.742913
3214.868704	328711.572690	52.747917
3214.439900	328422.957068	52.752922
3213.907275	328138.252077	52.757927
3213.012000	327865.823998	52.762932
3212.538900	327569.217852	52.767937
3211.807471	327287.800000	52.772941
3211.506216	327002.901450	52.777946
3210.436273	326723.088164	52.782951
3209.864342	326438.637742	52.787956
3209.044491	326150.457419	52.792961
3208.122980	325871.763337	52.797965
3207.775550	325598.145900	52.802970
3207.065632	325315.750121	52.807975
3206.199540	325033.912731	52.812980
3205.771227	324756.613466	52.817985
3204.942722	324479.071045	52.822989
3204.491029	324211.957898	52.827994
3203.561569	323926.434909	52.832999
3203.019902	323651.110335	52.838004
3202.614413	323372.707988	52.843009
3201.820350	323095.410098	52.848013
3201.476334	322804.036449	52.853018
3200.779895	322525.906490	52.858023
3199.738847	322244.138253	52.863028
3199.418629	321957.748373	52.868033
3198.562828	321678.724273	52.873037
3197.888309	321397.710054	52.878042
3197.142228	321115.305862	52.883047
3196.332329	320838.716140	52.888052
3195.648820	320556.198411	52.893057
3194.869385	320284.592662	52.898061
3194.202897	320002.808885	52.903066
3193.858391	319731.794665	52.908071
3192.770615	319457.816312	52.913076
3192.494435	319178.590823	52.918081
3191.577262	318904.914832	52.923085
3191.187939	318622.930168	52.928090
3190.336024	318345.066370	52.933095
3189.598047	318070.035522	52.938100
3189.015179	317786.576671	52.943105
3188.273849	317522.952006	52.948109
3187.672582	317241.505992	52.953114
3187.315635	316972.344502	52.958119
3186.410962	316692.421732	52.963124
3186.010662	316411.960021	52.968129
3184.854447	316139.561575	52.973133
3184.346692	315850.890703	52.978138
3183.699546	315578.410166	52.983143
3182.858098	315309.397167	52.988148
3182.354792	315031.672420	52.993153
3181.521412	314746.665680	52.998157
3181.074160	314476.162148	53.003162
3180.208063	314203.508847	53.008167
3179.567450	313927.483420	53.013172
3178.888241	313665.137352	53.018177
3178.351431	313394.034040	53.023181
3177.694178	313102.221565	53.028186
3177.207382	312833.604357	53.033191
3176.393694	312563.001085	53.038196
3175.886318	312278.878219	53.043201
3175.108708	312012.316635	53.048205
3174.531647	311727.770471	53.053210
3174.030671	311445.325062	53.058215
3173.208862	311175.076142	53.063220
3172.718639	310890.233987	53.068225
3171.501385	310614.622392	53.073229
3171.018081	310330.668988	53.078234
3170.561969	310064.204684	53.083239
3169.381719	309793.143401	53.088244
3169.044754	309510.234337	53.093249
3168.081641	309239.595776	53.098253
3167.726104	308968.427561	53.103258
3167.102862	308695.238439	53.108263
3166.390232	308409.203093	53.113268
3165.440324	308135.631490	53.118273
3164.648975	307871.710869	53.123277
3164.234181	307594.437364	53.128282
3163.524063	307318.508687	53.133287
3162.550461	307067.627847	53.138292
3162.253638	306788.933309	53.143297
3161.605197	306526.846198	53.148301
3160.897482	306245.414315	53.153306
3160.423542	305975.124115	53.158311
3159.572175	305697.457180	53.163316
3159.310499	305424.840374	53.168321
3158.142312	305159.038407	53.173325
3157.159334	304879.531608	53.178330
3156.854044	304614.330529	53.183335
3155.899269	304351.421751	53.188340
3155.762902	304075.726520	53.193345
3155.144583	303795.828758	53.198349
3154.425474	303534.256294	53.203354
3153.740598	303262.466128	53.208359
3153.057570	302991.668322	53.213364
3152.680699	302712.545132	53.218369
3151.361830	302443.604065	53.223373
3150.960332	302169.627867	53.228378
3150.610280	301895.311965	53.233383
3149.587410	301630.931951	53.238388
3149.025828	301358.507572	53.243393
3148.409365	301091.006373	53.248397
3147.782141	300815.841069	53.253402
3147.134194	300544.320243	53.258407
3145.982348	300262.794010	53.263412
3145.896732	299990.368331	53.268417
3145.093843	299728.395066	53.273421
3144.144178	299454.755493	53.278426
3143.907289	299178.736157	53.283431
3143.220528	298920.639611	53.288436
3142.359825	298639.675720	53.293441
3141.758169	298366.208502	53.298445
3140.897758	298094.284330	53.303450
3140.528598	297819.964527	53.308455
3139.547396	297551.904103	53.313460
3139.099069	297270.108751	53.318465
3138.249741	297014.861927	53.323469
3137.956625	296747.098897	53.328474
3137.377298	296460.662590	53.333479
3135.982525	296188.412640	53.338484
3135.843264	295922.228504	53.343489
3134.827356	295652.566406	53.348493
3134.318975	295379.156366	53.353498
3133.549961	295114.573337	53.358503
3132.719004	294839.761976	53.363508
3132.334517	294575.473929	53.368513
3131.228251	294317.233615	53.373517
3130.561302	294045.655039	53.378522
3130.378395	293780.646470	53.383527
3129.494035	293522.446470	53.388532
3129.061067	293246.474947	53.393537
3128.431612	292988.132109	53.398541
3127.413386	292709.476591	53.403546
3127.195897	292447.044094	53.408551
3126.039316	292184.377894	53.413556
3125.576472	291908.282132	53.418561
3124.700384	291647.073526	53.423565
3124.078312	291376.325053	53.428570
3123.563545	291106.374262	53.433575
3122.814947	290842.521465	53.438580
3122.370329	290568.484181	53.443585
3121.851986	290299.551799	53.448589
3121.074194	290043.368559	53.453594
3120.389523	289767.840365	53.458599
3119.533322	289505.582244	53.463604
3119.102416	289233.502429	53.468609
3118.179931	288965.091097	53.473613
3117.626861	288700.874172	53.478618
3116.668789	288439.726300	53.483623
3115.882590	288167.956384	53.488628
3115.508963	287913.821088	53.493633
3114.477131	287650.926927	53.498637
3113.965248	287392.458081	53.503642
3113.562006	287135.270697	53.508647
3112.823149	286868.127328	53.513652
3112.243202	286606.204995	53.518657
3111.400889	286352.652008	53.523661
3110.625708	286078.128061	53.528666
3110.200705	285814.830813	53.533671
3109.138243	285558.688899	53.538676
3108.563563	285297.019456	53.543681
3107.909697	285031.083734	53.548685
3107.385118	284769.202264	53.553690
3106.817905	284518.940821	53.558695
3105.840079	284258.862584	53.563700
3105.327501	283999.627413	53.568705
3104.615561	283735.941247	53.573709
3104.048604	283482.164561	53.578714
3103.307259	283217.005597	53.583719
3102.501829	282967.595962	53.588724
3101.852001	282704.434221	53.593729
3100.856883	282452.965957	53.598733
3100.583431	282196.620809	53.603738
3100.234509	281936.059757	53.608743
3099.322655	281683.330018	53.613748
3098.688062	281418.560745	53.618753
3098.047571	281160.210291	53.623757
3097.228015	280891.904508	53.628762
3097.167101	280647.800762	53.633767
3095.977270	280379.247755	53.638772
3095.557789	280125.981052	53.643777
3094.939710	279865.869252	53.648781
3094.221952	279602.283981	53.653786
3093.403564	279338.561742	53.658791
3092.375969	279082.818653	53.663796
3092.092870	278814.019753	53.668801
3091.259960	278564.128901	53.673805
3090.889829	278306.753459	53.678810
3090.312526	278046.074391	53.683815
3089.525332	277788.739372	53.688820
3088.929984	277515.685426	53.693825
3088.195293	277267.103118	53.698829
3087.571123	277008.723424	53.703834
3086.864515	276746.612887	53.708839
3085.813192	276490.974903	53.713844
3085.471845	276222.184714	53.718849
3084.995097	275973.153926	53.723853
3084.219292	275711.869218	53.728858
3083.569604	275446.158500	53.733863
3082.911802	275176.985353	53.738868
3082.197957	274924.630204	53.743873
3081.473861	274664.483347	53.748877
3080.770715	274404.129427	53.753882
3080.090355	274135.112652	53.758887
3079.035746	273888.338086	53.763892
3078.753513	273617.042574	53.768897
3078.216924	273364.150044	53.773901
3077.362166	273101.502562	53.778906
3076.860676	272843.994746	53.783911
3075.701392	272595.708747	53.788916
3075.744543	272332.078789	53.793921
3074.775223	272081.623451	53.798925
3074.412790	271819.000095	53.803930
3073.784887	271551.910903	53.808935
3072.636410	271295.498993	53.813940
3072.028762	271043.764123	53.818945
3071.632684	270780.433195	53.823949
3070.693768	270514.233921	53.828954
3070.100640	270258.804032	53.833959
3069.613022	270011.863934	53.838964
3069.038239	269741.888875	53.843969
3067.834757	269496.386581	53.848973
3067.410751	269230.004330	53.853978
3067.225121	268978.228711	53.858983
3066.363981	268715.303115	53.863988
3065.667269	268449.779300	53.868993
3064.990362	268193.344628	53.873997
3064.202998	267923.327496	53.879002
3063.410890	267659.245335	53.884007
3062.656892	267408.044186	53.889012
3062.097033	267145.784684	53.894017
3061.037524	266896.618643	53.899021
3060.570142	266644.939523	53.904026
3060.273103	266393.029821	53.909031
3059.667373	266134.725660	53.914036
3058.695147	265872.506614	53.919041
3057.911238	265618.764269	53.924045
3057.306578	265369.577957	53.929050
3056.953628	265114.137728	53.934055
3055.942604	264852.740404	53.939060
3055.685640	264594.356467	53.944065
3054.355190	264342.866171	53.949069
3053.818348	264088.678153	53.954074
3053.466673	263833.849761	53.959079
3052.562943	263585.195775	53.964084
3051.979585	263336.567652	53.969089
3051.258363	263082.485907	53.974093
3050.490865	262829.812407	53.979098
3049.701885	262579.434608	53.984103
3048.967285	262337.452799	53.989108
3048.495750	262075.768311	53.994113
3047.727693	261830.277603	53.999117
3047.124748	261585.524987	54.004122
3046.654934	261334.486401	54.009127
3045.703595	261085.561663	54.014132
3045.081953	260838.265821	54.019137
3044.462884	260592.752523	54.024141
3043.733301	260347.638942	54.029146
3043.397874	260101.036990	54.034151
3042.863954	259846.928231	54.039156
3042.032781	259595.642734	54.044161
3041.142870	259353.305917	54.049165
3040.631847	259096.672939	54.054170
3040.114497	258833.241361	54.059175
3039.618884	258592.982115	54.064180
3038.796507	258336.602915	54.069185
3037.874796	258087.650755	54.074189
3037.196469	257834.916598	54.079194
3036.436068	257586.779843	54.084199
3035.878138	257345.156433	54.089204
3035.480188	257087.438000	54.094209
3034.686972	256835.461648	54.099213
3033.905017	256590.385450	54.104218
3033.486427	256341.890311	54.109223
3032.473510	256088.115920	54.114228
3031.968748	255840.348070	54.119233
3031.437517	255596.761322	54.124237
3030.667492	255348.144671	54.129242
3030.040770	255090.413839	54.134247
3029.328892	254855.820993	54.139252
3028.593578	254602.539244	54.144257
3027.733632	254347.749512	54.149261
3026.951178	254102.879996	54.154266
3026.522802	253856.655915	54.159271
3025.857275	253617.422176	54.164276
3025.169786	253367.979949	54.169281
3024.468174	253123.557271	54.174285
3023.720639	252878.760174	54.179290
3023.287201	252645.271906	54.184295
3022.344648	252399.742301	54.189300
3021.888571	252145.731971	54.194305
3021.387460	251907.645861	54.199309
3020.508006	251662.336467	54.204314
3019.892293	251410.084186	54.209319
3019.062562	251176.431348	54.214324
3018.555192	250930.834878	54.219329
3017.619146	250686.223412	54.224333
3017.202780	250439.518177	54.229338
3016.561894	250199.597472	54.234343
3015.393916	249962.943860	54.239348
3015.193614	249715.976293	54.244353
3014.486496	249481.262271	54.249357
3013.635142	249232.539448	54.254362
3013.402666	248987.691791	54.259367
3012.350611	248744.349429	54.264372
3011.685350	248501.073545	54.269377
3011.145305	248257.778219	54.274381
3010.736933	248016.652524	54.279386
3010.207134	247769.816548	54.284391
3009.302404	247530.807484	54.289396
3008.620351	247283.385218	54.294401
3007.862491	247036.764809	54.299405
3007.085168	246797.583956	54.304410
3006.693003	246546.424467	54.309415
3005.977483	246307.514760	54.314420
3005.281167	246059.052717	54.319425
3004.599080	245820.545982	54.324429
3003.996901	245576.297203	54.329434
3003.405970	245327.616035	54.334439
3002.457511	245087.522907	54.339444
3001.924910	244843.111607	54.344449
3001.507976	244599.268140	54.349453
3000.481545	244355.088682	54.354458
3000.067685	244107.858699	54.359463
2999.470342	243873.340006	54.364468
2998.838598	243626.043548	54.369473
2997.826212	243377.636404	54.374477
2997.275551	243142.984297	54.379482
2996.539088	242893.057413	54.384487
2995.915860	242651.160093	54.389492
2995.272979	242400.608191	54.394497
2994.851178	242159.774920	54.399501
2993.581069	241926.359407	54.404506
2993.204387	241666.955919	54.409511
2992.684927	241439.890599	54.414516
2991.791958	241187.700037	54.419521
2991.313954	240959.584983	54.424525
2990.662630	240714.309054	54.429530
2990.244283	240460.084081	54.434535
2989.412873	240235.005724	54.439540
2988.815776	239990.130132	54.444545
2988.008234	239737.725381	54.449549
2987.312844	239497.500934	54.454554
2986.928262	239246.328980	54.459559
2985.885491	239010.107534	54.464564
2985.588043	238763.022616	54.469569
2984.845849	238521.279756	54.474573
2983.970745	238281.188167	54.479578
2983.648588	238038.157564	54.484583
2982.639816	237802.136975	54.489588
2982.119963	237547.399765	54.494593
2981.401519	237304.993716	54.499597
2980.372299	237074.783727	54.504602
2980.152130	236826.570462	54.509607
2979.528098	236589.829520	54.514612
2978.906408	236339.465587	54.519617
2978.130255	236093.175433	54.524621
2977.322747	235852.187264	54.529626
2976.960219	235590.350874	54.534631
2976.344453	235366.317713	54.539636
2975.583921	235110.249379	54.544641
2974.820938	234867.983262	54.549645
2974.024565	234627.174417	54.554650
2973.464537	234384.240731	54.559655
2972.529579	234150.559226	54.564660
2971.937878	233903.964995	54.569665
2971.307497	233661.171505	54.574669
2970.698327	233425.937788	54.579674
2969.966745	233172.059607	54.584679
2969.149671	232942.512748	54.589684
2968.800325	232693.515107	54.594689
2968.016265	232451.130875	54.599693
2967.336880	232229.075439	54.604698
2966.877936	231981.090030	54.609703
2966.080290	231735.374137	54.614708
2965.643383	231483.618059	54.619713
2964.762248	231254.798323	54.624717
2964.299285	231017.332091	54.629722
2963.429754	230766.537611	54.634727
2962.580433	230533.640620	54.639732
2962.050235	230290.967110	54.644737
2961.489419	230053.111441	54.649741
2960.494255	229813.797428	54.654746
2959.975605	229571.913321	54.659751
2959.621627	229333.772164	54.664756
2958.550346	229088.233933	54.669761
2957.996276	228854.046861	54.674765
2957.410669	228610.953773	54.679770
2956.720492	228371.340700	54.684775
2955.705586	228133.027310	54.689780
2955.087510	227901.984676	54.694785
2954.674876	227660.776446	54.699789
2954.018711	227435.800918	54.704794
2953.553680	227191.470531	54.709799
2952.874272	226944.399498	54.714804
2951.844122	226702.782488	54.719809
2951.499790	226466.455348	54.724813
2950.791265	226247.143611	54.729818
2950.199848	225997.171568	54.734823
2949.279384	225755.068874	54.739828
2948.532486	225509.514917	54.744833
2947.912030	225278.365205	54.749837
2947.195405	225046.798532	54.754842
2946.651629	224806.561255	54.759847
2945.771540	224577.656964	54.764852
2945.141225	224336.276315	54.769857
2944.631001	224096.239502	54.774861
2943.646330	223873.387879	54.779866
2943.275376	223634.616139	54.784871
2942.688701	223405.872397	54.789876
2941.981760	223172.285468	54.794881
2941.273875	222935.096779	54.799885
2940.361193	222704.624472	54.804890
2939.789536	222468.268530	54.809895
2938.793907	222245.079511	54.814900
2938.444377	222012.928840	54.819905
2938.000269	221779.215337	54.824909
2937.121066	221555.373379	54.829914
2936.799661	221320.928970	54.834919
2936.207726	221088.246625	54.839924
2935.523251	220852.180816	54.844929
2934.583288	220610.211449	54.849933
2933.972078	220377.152448	54.854938
2933.441216	220140.135282	54.859943
2932.654922	219918.549306	54.864948
2932.063741	219670.277550	54.869953
2931.394091	219437.612616	54.874957
2930.612496	219208.301244	54.879962
2930.098777	218974.938422	54.884967
2929.243199	218741.223132	54.889972
2928.420464	218508.139855	54.894977
2928.083449	218270.945250	54.899981
2927.334605	218049.358983	54.904986
2926.875572	217806.851684	54.909991
2926.170313	217571.512497	54.914996
2925.521122	217339.398392	54.920001
2924.846630	217102.171977	54.925005
2923.933013	216864.513245	54.930010
2923.693235	216624.864736	54.935015
2922.808356	216397.207985	54.940020
2922.023029	216162.942658	54.945025
2921.339118	215927.427365	54.950029
2920.875920	215695.683827	54.955034
2920.524214	215466.940122	54.960039
2919.405338	215222.942386	54.965044
2919.023594	214997.527186	54.970049
2918.205849	214750.708605	54.975053
2917.414832	214522.597670	54.980058
2916.996805	214285.416652	54.985063
2915.928631	214043.999001	54.990068
2915.509880	213816.111531	54.995073
2914.749439	213578.859935	55.000077
2914.263923	213348.235299	55.005082
2913.614740	213108.040242	55.010087
2912.647363	212875.787953	55.015092
2912.190066	212644.613980	55.020097
2911.600453	212409.897886	55.025101
2910.775025	212179.216599	55.030106
2910.356471	211936.583686	55.035111
2909.657688	211700.423700	55.040116
2909.002052	211463.124953	55.045121
2908.327653	211225.295475	55.050125
2907.615365	210992.614940	55.055130
2906.851160	210741.004455	55.060135
2906.283176	210524.568942	55.065140
2905.559089	210289.640018	55.070145
2905.083454	210046.005065	55.075149
2904.185476	209817.023807	55.080154
2903.387906	209571.927073	55.085159
2902.632283	209348.919679	55.090164
2902.156250	209114.095868	55.095169
2901.395498	208874.316137	55.100173
2900.778791	208649.265587	55.105178
2899.993575	208416.975217	55.110183
2899.542612	208193.300094	55.115188
2899.114680	207951.103969	55.120193
2898.192944	207721.676027	55.125197
2897.245854	207496.045660	55.130202
2896.689299	207266.154341	55.135207
2896.064921	207035.141925	55.140212
2895.838679	206798.416551	55.145217
2894.867681	206567.486269	55.150221
2894.355432	206344.782189	55.155226
2893.543895	206102.705121	55.160231
2892.896556	205867.475520	55.165236
2891.902252	205646.084890	55.170241
2891.418097	205407.280506	55.175245
2890.934931	205178.314652	55.180250
2890.317411	204943.262186	55.185255
2889.303168	204708.044408	55.190260
2888.725919	204478.727118	55.195265
2888.344290	204252.077768	55.200269
2887.277214	204030.832038	55.205274
2886.737362	203784.534526	55.210279
2886.188193	203559.912462	55.215284
2885.314156	203337.709807	55.220289
2884.993347	203103.292323	55.225293
2883.937686	202869.208513	55.230298
2883.689145	202650.587348	55.235303
2882.433030	202416.791671	55.240308
2881.890103	202201.005869	55.245313
2881.339578	201974.074151	55.250317
2880.526558	201746.357734	55.255322
2880.030051	201509.989441	55.260327
2879.414072	201281.518342	55.265332
2878.693736	201063.856148	55.270337
2877.812337	200830.236829	55.275341
2877.246908	200607.665230	55.280346
2876.569497	200383.534288	55.285351
2876.050352	200161.351658	55.290356
2875.431794	199937.455005	55.295361
2874.710404	199708.841690	55.300365
2873.834030	199483.397048	55.305370
2873.612906	199265.459332	55.310375
2872.756443	199041.336813	55.315380
2872.098211	198802.040807	55.320385
2871.649943	198579.522573	55.325389
2871.093373	198358.689405	55.330394
2870.038210	198119.650180	55.335399
2869.243898	197902.750417	55.340404
2868.826831	197676.413502	55.345409
2868.015302	197441.550708	55.350413
2867.547043	197225.429204	55.355418
2867.144452	196992.908645	55.360423
2866.150145	196765.585442	55.365428
2865.366486	196538.255317	55.370433
2865.130768	196313.511581	55.375437
2864.292206	196079.995253	55.380442
2863.858203	195839.697364	55.385447
2863.028884	195623.665117	55.390452
2862.355674	195393.943038	55.395457
2861.763502	195157.261657	55.400461
2860.951848	194932.742375	55.405466
2860.457752	194690.359861	55.410471
2859.467475	194480.312860	55.415476
2858.593037	194248.350165	55.420481
2858.259035	194022.117842	55.425485
2857.523703	193800.963346	55.430490
2856.768071	193565.256836	55.435495
2856.094344	193348.967841	55.440500
2855.407821	193115.568246	55.445505
2854.781260	192886.995278	55.450509
2853.841915	192680.421311	55.455514
2853.516120	192449.334318	55.460519
2852.798504	192232.230078	55.465524
2851.863448	192013.519889	55.470529
2851.578826	191783.002047	55.475533
2850.787245	191569.729484	55.480538
2850.341479	191338.539457	55.485543
2849.348298	191114.778570	55.490548
2848.961878	190886.202287	55.495553
2848.363224	190655.688592	55.500557
2847.203600	190439.311181	55.505562
2846.917990	190211.574559	55.510567
2846.292544	189991.463029	55.515572
2845.617952	189765.889414	55.520577
2845.067919	189537.892502	55.525581
2843.884203	189320.938680	55.530586
2843.398456	189100.656440	55.535591
2842.867926	188875.853018	55.540596
2842.004173	188644.271360	55.545601
2841.684578	188427.146593	55.550605
2840.944640	188215.038466	55.555610
2840.307857	187985.726870	55.560615
2839.598366	187762.114832	55.565620
2839.037741	187540.146913	55.570625
2838.533963	187308.832871	55.575629
2837.457699	187089.658607	55.580634
2836.839957	186856.074856	55.585639
2836.253885	186640.590841	55.590644
2835.832304	186420.692666	55.595649
2835.366913	186192.914834	55.600653
2834.488158	185969.681717	55.605658
2833.758031	185739.009293	55.610663
2833.241724	185509.729007	55.615668
2832.167991	185279.876623	55.620673
2831.859569	185057.206437	55.625677
2830.990857	184838.938708	55.630682
2830.428297	184604.874249	55.635687
2829.653180	184378.223131	55.640692
2828.925815	184172.365131	55.645697
2828.591126	183934.133593	55.650701
2827.867451	183708.851603	55.655706
2827.243111	183477.805013	55.660711
2826.517500	183254.840881	55.665716
2825.638345	183027.920475	55.670721
2824.895532	182797.684881	55.675725
2824.377750	182582.667298	55.680730
2823.850102	182349.881199	55.685735
2822.959733	182134.950245	55.690740
2822.403956	181911.444418	55.695745
2821.994017	181676.518861	55.700749
2820.857393	181462.838667	55.705754
2820.245249	181235.401809	55.710759
2819.734973	181008.420663	55.715764
2818.887101	180789.558942	55.720769
2818.530343	180560.914877	55.725773
2817.679770	180341.127258	55.730778
2816.878460	180109.630311	55.735783
2816.352557	179893.138982	55.740788
2815.669599	179673.620784	55.745793
2815.323629	179444.383084	55.750797
2814.231577	179229.969100	55.755802
2813.798779	179008.341332	55.760807
2812.851141	178779.634973	55.765812
2812.312231	178558.344351	55.770817
2811.466116	178334.394238	55.775821
2811.105285	178124.550880	55.780826
2810.373030	177897.354252	55.785831
2809.847939	177679.055152	55.790836
2808.859325	177459.634972	55.795841
2808.483946	177229.065651	55.800845
2807.704854	177026.302414	55.805850
2807.027585	176799.510045	55.810855
2806.592970	176570.619968	55.815860
2805.706994	176349.879290	55.820865
2805.016090	176132.441286	55.825869
2803.942535	175912.177820	55.830874
2803.776204	175692.064372	55.835879
2803.157450	175474.173246	55.840884
2802.255609	175260.525317	55.845889
2802.102390	175019.923415	55.850893
2801.549208	174812.798178	55.855898
2800.490906	174573.881217	55.860903
2799.914160	174347.735079	55.865908
2799.418251	174129.348366	55.870913
2798.824735	173914.781083	55.875917
2797.796019	173685.810438	55.880922
2797.116490	173456.251618	55.885927
2796.549380	173236.927139	55.890932
2795.515770	173020.437575	55.895937
2795.140456	172799.291857	55.900941
2794.333393	172579.919954	55.905946
2793.768000	172358.018273	55.910951
2793.255022	172139.746820	55.915956
2792.370011	171915.825228	55.920961
2791.945937	171694.973155	55.925965
2791.167461	171471.329707	55.930970
2790.630327	171249.417036	55.935975
2789.878431	171033.326075	55.940980
2789.067937	170814.180693	55.945985
2788.346285	170586.883382	55.950989
2787.784200	170369.456129	55.955994
2786.920368	170153.146126	55.960999
2786.529601	169935.338075	55.966004
2785.559850	169720.369832	55.971009
2785.207981	169492.702403	55.976013
2784.341780	169285.045140	55.981018
2783.928797	169066.317156	55.986023
2783.372735	168845.463945	55.991028
2782.300130	168632.260241	55.996033
2781.942470	168403.951604	56.001037
2781.395780	168178.980563	56.006042
2780.685485	167955.944228	56.011047
2779.907522	167734.166119	56.016052
2779.320828	167515.728824	56.021057
2778.828471	167288.974146	56.026061
2778.126638	167083.337385	56.031066
2777.157239	166846.564290	56.036071
2776.589660	166627.493284	56.041076
2775.640926	166403.461135	56.046081
2774.971422	166185.985617	56.051085
2774.313451	165973.684855	56.056090
2773.735375	165756.705976	56.061095
2773.084383	165538.875242	56.066100
2772.543664	165318.141880	56.071105
2772.241538	165093.811697	56.076109
2771.168922	164882.676354	56.081114
2770.738959	164662.717695	56.086119
2770.045669	164443.590401	56.091124
2769.672809	164219.518303	56.096129
2768.964096	163991.063196	56.101133
2768.119394	163773.044655	56.106138
2767.605281	163539.717102	56.111143
2767.181025	163317.426020	56.116148
2766.223267	163092.728700	56.121153
2765.423508	162865.769947	56.126157
2764.743510	162648.571191	56.131162
2764.175649	162416.200217	56.136167
2763.706983	162204.615904	56.141172
2762.824001	161955.349402	56.146177
2762.150459	161696.948002	56.151181
2761.420340	161473.330802	56.156186
2761.049196	161254.260648	56.161191
2760.184341	161021.589703	56.166196
2759.595647	160806.358253	56.171201
2758.980339	160574.222815	56.176205
2758.087612	160363.682769	56.181210
2757.355219	160138.523182	56.186215
2756.782040	159904.211387	56.191220
2755.849273	159696.504070	56.196225
2755.429686	159472.252679	56.201229
2754.626473	159255.055868	56.206234
2754.102968	159035.438689	56.211239
2753.266459	158816.508127	56.216244
2752.648403	158599.286032	56.221249
2752.252948	158378.114379	56.226253
2751.272591	158164.588322	56.231258
2750.825454	157948.779761	56.236263
2750.507228	157717.518679	56.241268
2749.679416	157502.434254	56.246273
2748.855568	157285.125809	56.251277
2748.113526	157055.817751	56.256282
2747.237252	156826.774015	56.261287
2746.640005	156610.781438	56.266292
2745.814845	156409.331158	56.271297
2745.756788	156176.945886	56.276301
2745.021932	155962.568215	56.281306
2744.108927	155737.020703	56.286311
2743.214903	155526.115970	56.291316
2742.623384	155302.109408	56.296321
2742.121607	155086.772330	56.301325
2741.055572	154867.369237	56.306330
2740.451932	154647.284146	56.311335
2739.538447	154443.901844	56.316340
2739.293379	154225.110127	56.321345
2738.606627	153996.398561	56.326349
2737.993786	153787.760869	56.331354
2737.215687	153582.392041	56.336359
2736.577357	153363.337723	56.341364
2735.911037	153145.827322	56.346369
2735.612534	152935.073210	56.351373
2734.879568	152721.084390	56.356378
2734.238269	152492.719072	56.361383
2733.386708	152282.997301	56.366388
2732.424304	152072.709719	56.371393
2732.100225	151845.391719	56.376397
2731.176295	151636.562536	56.381402
2730.595031	151422.278417	56.386407
2730.335564	151206.483010	56.391412
2729.358271	150996.789309	56.396417
2728.574491	150774.343311	56.401421
2727.826295	150575.330762	56.406426
2727.252033	150362.412427	56.411431
2726.652901	150140.653242	56.416436
2725.851673	149927.697434	56.421441
2725.293476	149714.348640	56.426445
2724.835364	149497.121617	56.431450
2723.932101	149294.798773	56.436455
2723.367184	149070.270745	56.441460
2722.701535	148863.820456	56.446465
2722.233932	148645.901616	56.451469
2721.144100	148439.584787	56.456474
2720.415842	148229.933005	56.461479
2720.032320	148017.927611	56.466484
2719.120265	147808.866898	56.471489
2718.909432	147587.343289	56.476493
2718.043536	147385.064645	56.481498
2717.101275	147166.468505	56.486503
2716.691661	146961.324311	56.491508
2715.923450	146751.269155	56.496513
2715.654142	146536.624793	56.501517
2714.814268	146328.909456	56.506522
2713.746613	146113.619219	56.511527
2713.587822	145898.771040	56.516532
2712.689599	145692.098505	56.521537
2712.567995	145475.607949	56.526541
2711.369080	145264.334669	56.531546
2710.755825	145046.514360	56.536551
2709.954598	144834.367657	56.541556
2709.337004	144624.391751	56.546561
2708.850133	144415.019224	56.551565
2708.207474	144205.939644	56.556570
2707.344600	143991.038165	56.561575
2706.897759	143780.125944	56.566580
2705.731116	143572.226481	56.571585
2705.271980	143355.435569	56.576589
2704.790261	143152.119408	56.581594
2703.911096	142940.569790	56.586599
2703.532776	142728.332333	56.591604
2702.543647	142530.018289	56.596609
2702.257336	142311.657074	56.601613
2701.235279	142104.786556	56.606618
2701.027256	141888.512567	56.611623
2700.523037	141669.656764	56.616628
2699.342047	141461.595938	56.621633
2698.741259	141250.140933	56.626637
2698.097239	141045.733564	56.631642
2697.430630	140841.610685	56.636647
2696.988948	140627.352127	56.641652
2696.112114	140406.709334	56.646657
2695.822384	140194.818503	56.651661
2694.707127	139980.899946	56.656666
2693.865419	139769.925434	56.661671
2693.549516	139556.213593	56.666676
2692.553574	139342.585603	56.671681
2692.205218	139142.222770	56.676685
2691.549874	138941.833680	56.681690
2690.639409	138722.555337	56.686695
2690.212061	138507.369391	56.691700
2689.397592	138302.321550	56.696705
2688.870774	138088.882288	56.701709
2687.950618	137880.550769	56.706714
2687.104139	137675.626664	56.711719
2686.511386	137465.937573	56.716724
2685.924834	137263.198483	56.721729
2685.392209	137063.615700	56.726733
2684.513208	136862.742460	56.731738
2684.187133	136649.408807	56.736743
2683.509664	136446.791366	56.741748
2682.658153	136238.231870	56.746753
2682.187775	136031.099862	56.751757
2681.368564	135827.670673	56.756762
2680.545266	135618.501319	56.761767
2680.300387	135405.989604	56.766772
2679.178162	135197.836127	56.771777
2678.794689	134991.675912	56.776781
2678.172417	134790.331578	56.781786
2677.472972	134578.329851	56.786791
2676.836151	134377.041503	56.791796
2676.052622	134164.865570	56.796801
2675.943483	133946.575673	56.801805
2674.995252	133753.293282	56.806810
2674.061347	133545.858622	56.811815
2673.486370	133328.206153	56.816820
2672.857340	133130.863206	56.821825
2672.385227	132926.433960	56.826829
2671.600314	132717.660577	56.831834
2670.958085	132507.024220	56.836839
2670.441846	132297.817548	56.841844
2669.691135	132098.836958	56.846849
2669.157864	131873.338804	56.851853
2668.093277	131674.182273	56.856858
2667.687167	131462.169783	56.861863
2667.111101	131244.965238	56.866868
2666.293870	131038.711604	56.871873
2665.497247	130832.037045	56.876877
2664.944841	130627.395701	56.881882
2664.164945	130421.788451	56.886887
2663.685700	130215.030020	56.891892
2662.849262	130009.637967	56.896897
2662.247824	129793.210716	56.901901
2661.578014	129596.800618	56.906906
2660.899593	129385.164432	56.911911
2660.368735	129175.564057	56.916916
2659.507255	128977.359712	56.921921
2658.783816	128759.168944	56.926925
2658.216041	128561.530667	56.931930
2657.423714	128357.236052	56.936935
2657.075146	128155.514373	56.941940
2655.734272	127953.481474	56.946945
2655.409704	127748.710806	56.951949
2654.984248	127547.869374	56.956954
2654.062935	127348.009697	56.961959
2653.695744	127138.703585	56.966964
2652.719020	126941.751293	56.971969
2652.256907	126727.345189	56.976973
2651.591139	126533.077067	56.981978
2651.084390	126325.983654	56.986983
2650.568643	126118.702735	56.991988
2649.397187	125917.102449	56.996993
2649.099621	125702.246510	57.001997
2648.240012	125496.942437	57.007002
2647.478154	125302.520501	57.012007
2646.876967	125090.879647	57.017012
2646.287855	124886.083396	57.022017
2645.609253	124679.271016	57.027021
2645.134442	124487.298462	57.032026
2644.306399	124276.944417	57.037031
2643.843715	124072.261282	57.042036
2643.089875	123865.111491	57.047041
2642.125508	123652.091796	57.052045
2641.514536	123462.865617	57.057050
2640.804560	123264.678665	57.062055
2640.315777	123053.696297	57.067060
2639.397066	122855.735922	57.072065
2638.692066	122638.721330	57.077069
2638.372475	122446.611778	57.082074
2637.939445	122243.537855	57.087079
2637.450377	122040.550548	57.092084
2636.430668	121833.547501	57.097089
2635.491513	121625.771445	57.102093
2635.555776	121416.936485	57.107098
2634.531145	121216.160841	57.112103
2633.725319	121007.454291	57.117108
2633.196712	120802.832071	57.122113
2632.631365	120590.421203	57.127117
2631.746918	120394.048212	57.132122
2631.022049	120187.112918	57.137127
2630.263278	119978.775275	57.142132
2629.449390	119783.589172	57.147137
2629.118003	119582.386022	57.152141
2628.453972	119371.257625	57.157146
2627.576892	119175.711523	57.162151
2627.016326	118964.900124	57.167156
2626.223175	118772.886031	57.172161
2625.659243	118562.160951	57.177165
2625.102813	118363.319916	57.182170
2624.489249	118164.349802	57.187175
2624.135681	117959.087292	57.192180
2623.464949	117761.303701	57.197185
2622.464428	117544.270101	57.202189
2621.949264	117336.333963	57.207194
2621.058038	117143.452451	57.212199
2620.469353	116940.120576	57.217204
2619.920356	116724.406125	57.222209
2619.331479	116519.490698	57.227213
2618.608242	116313.982489	57.232218
2617.989291	116115.695534	57.237223
2617.463528	115905.005156	57.242228
2616.447020	115706.625690	57.247233
2616.044050	115500.248108	57.252237
2615.368721	115295.686249	57.257242
2614.064748	115090.629018	57.262247
2613.836986	114878.877992	57.267252
2613.108940	114693.904034	57.272257
2612.385710	114488.448627	57.277261
2611.481443	114292.201381	57.282266
2610.986342	114082.219422	57.287271
2610.428608	113887.361168	57.292276
2609.514197	113691.431198	57.297281
2609.087007	113494.156175	57.302285
2608.247852	113299.804034	57.307290
2607.973299	113096.154815	57.312295
2607.325853	112889.627830	57.317300
2606.505577	112694.960047	57.322305
2605.941066	112481.511806	57.327309
2605.372734	112287.676746	57.332314
2604.070330	112084.185953	57.337319
2603.746267	111887.103978	57.342324
2602.949666	111698.691438	57.347329
2602.529310	111493.618713	57.352333
2601.825735	111291.784737	57.357338
2600.921057	111092.522762	57.362343
2600.478383	110894.896290	57.367348
2599.574162	110702.497591	57.372353
2599.255440	110498.603712	57.377357
2598.598205	110293.800568	57.382362
2597.614132	110105.582161	57.387367
2597.186357	109894.825181	57.392372
2596.505053	109710.178984	57.397377
2595.767817	109509.786380	57.402381
2595.261546	109302.403854	57.407386
2594.497636	109105.382033	57.412391
2594.016062	108913.349160	57.417396
2593.221933	108705.598494	57.422401
2592.864703	108507.952276	57.427405
2592.006138	108308.654788	57.432410
2590.899779	108108.585985	57.437415
2590.587001	107898.874964	57.442420
2589.404965	107702.317811	57.447425
2588.953259	107505.265787	57.452429
2588.489564	107317.589187	57.457434
2587.698094	107121.571297	57.462439
2587.254363	106921.870465	57.467444
2586.418960	106728.997220	57.472449
2586.016868	106533.417308	57.477453
2585.058725	106337.482959	57.482458
2584.560593	106136.065072	57.487463
2584.114241	105930.935255	57.492468
2582.932015	105737.909192	57.497473
2582.260041	105540.521092	57.502477
2581.560994	105345.848105	57.507482
2580.899645	105154.983876	57.512487
2580.810565	104962.488729	57.517492
2580.018042	104768.780605	57.522497
2579.364791	104566.290201	57.527501
2578.488179	104371.888044	57.532506
2577.801524	104176.689696	57.537511
2577.657605	103973.089477	57.542516
2576.725477	103776.156904	57.547521
2576.118259	103574.289398	57.552525
2575.346833	103380.697097	57.557530
2574.692095	103186.155297	57.562535
2573.936280	102980.230781	57.567540
2573.227049	102783.486847	57.572545
2572.631720	102576.195486	57.577549
2572.446305	102372.685403	57.582554
2571.220876	102180.621326	57.587559
2570.686045	101979.650481	57.592564
2569.951281	101793.367157	57.597569
2569.149795	101581.962074	57.602573
2568.604353	101392.061393	57.607578
2567.822518	101197.993906	57.612583
2567.230059	100999.590741	57.617588
2566.559703	100816.857382	57.622593
2566.175932	100606.206896	57.627597
2565.655191	100413.443026	57.632602
2564.604695	100227.717026	57.637607
2564.279288	100020.329421	57.642612
2563.444996	99823.528723	57.647617
2562.874602	99626.897195	57.652621
2562.243611	99420.984260	57.657626
2561.378442	99229.547109	57.662631
2561.039802	99030.295950	57.667636
2560.208004	98831.010502	57.672641
2559.360030	98622.963444	57.677645
2558.906325	98430.408450	57.682650
2557.812806	98234.613822	57.687655
2557.319906	98038.662241	57.692660
2556.685691	97841.453510	57.697665
2556.024002	97644.434767	57.702669
2555.477424	97446.942810	57.707674
2554.586898	97247.540891	57.712679
2554.013671	97051.509017	57.717684
2553.627430	96872.307342	57.722689
2552.652274	96667.412348	57.727693
2552.360109	96457.444920	57.732698
2551.565731	96273.771559	57.737703
2550.748483	96066.992328	57.742708
2550.110738	95872.052680	57.747713
2549.492865	95675.266013	57.752717
2548.959615	95475.214182	57.757722
2548.051147	95283.614030	57.762727
2547.503330	95074.879546	57.767732
2546.687095	94896.750987	57.772737
2546.270831	94690.878417	57.777741
2545.559307	94492.867572	57.782746
2544.515050	94307.391680	57.787751
2544.017195	94102.095505	57.792756
2543.073928	93917.450271	57.797761
2542.847924	93721.557127	57.802765
2541.997511	93526.830038	57.807770
2541.223720	93337.191010	57.812775
2540.769747	93140.774703	57.817780
2539.899627	92953.957088	57.822785
2539.290001	92762.343802	57.827789
2538.962441	92560.871264	57.832794
2537.991145	92373.554582	57.837799
2537.380259	92178.845701	57.842804
2536.430201	91987.622796	57.847809
2535.999352	91790.105074	57.852813
2535.177993	91599.150469	57.857818
2534.718388	91413.821601	57.862823
2534.260674	91208.678913	57.867828
2533.359042	91026.365504	57.872833
2532.676662	90838.318547	57.877837
2532.276401	90642.822589	57.882842
2531.369558	90462.778289	57.887847
2530.988977	90261.956490	57.892852
2530.488195	90063.710799	57.897857
2529.819602	89861.708261	57.902861
2528.887457	89678.599302	57.907866
2528.024548	89491.042675	57.912871
2527.765674	89287.889956	57.917876
2526.545512	89089.202843	57.922881
2526.195630	88893.999819	57.927885
2525.790405	88711.088083	57.932890
2524.835437	88513.017223	57.937895
2524.125279	88310.014897	57.942900
2523.613288	88128.805080	57.947905
2523.064344	87930.142624	57.952909
2522.185495	87740.441723	57.957914
2521.587997	87546.304434	57.962919
2521.058697	87343.631181	57.967924
2520.299245	87160.744298	57.972929
2519.747194	86961.793269	57.977933
2519.142228	86773.344386	57.982938
2518.129181	86578.616026	57.987943
2517.721052	86373.789944	57.992948
2516.929329	86192.127234	57.997953
2516.408077	85990.479742	58.002957
2516.044290	85785.645904	58.007962
2514.977266	85598.675207	58.012967
2514.563370	85402.607393	58.017972
2513.585794	85218.224888	58.022977
2512.738261	85011.947427	58.027981
2512.468093	84826.606744	58.032986
2511.817723	84630.437713	58.037991
2511.095770	84434.769929	58.042996
2509.991257	84248.805875	58.048001
2509.599690	84055.345820	58.053005
2509.189423	83853.815032	58.058010
2508.055902	83655.341922	58.063015
2507.857507	83461.704536	58.068020
2506.612768	83279.238410	58.073025
2505.983374	83083.352924	58.078029
2505.366848	82896.848013	58.083034
2504.930309	82709.416179	58.088039
2503.965363	82515.439952	58.093044
2503.619391	82326.368237	58.098049
2502.993410	82143.541321	58.103053
2502.189817	81959.311742	58.108058
2501.444378	81765.434406	58.113063
2501.141882	81574.524540	58.118068
2500.594184	81381.063073	58.123073
2499.753381	81191.731443	58.128077
2499.132432	81003.196931	58.133082
2498.284761	80805.459625	58.138087
2497.916526	80613.751387	58.143092
2496.786057	80420.239105	58.148097
2496.029657	80225.452511	58.153101
2495.613536	80037.274525	58.158106
2494.954919	79848.737426	58.163111
2494.611232	79651.862801	58.168116
2493.625659	79469.819772	58.173121
2493.109266	79275.428652	58.178125
2492.461716	79088.347956	58.183130
2491.935478	78898.841600	58.188135
2491.199386	78707.855682	58.193140
2490.113294	78516.869984	58.198145
2489.676430	78330.035257	58.203149
2489.141920	78135.511998	58.208154
2487.991759	77951.886205	58.213159
2487.794843	77762.990791	58.218164
2487.118258	77564.097716	58.223169
2486.454901	77378.429154	58.228173
2485.703734	77192.142531	58.233178
2484.804401	77008.827604	58.238183
2484.338380	76806.588140	58.243188
2483.882688	76625.728255	58.248193
2483.053064	76436.596879	58.253197
2482.565406	76242.052500	58.258202
2481.969786	76059.851168	58.263207
2481.360378	75862.776191	58.268212
2480.628622	75679.136185	58.273217
2479.836895	75487.846991	58.278221
2479.126006	75295.197208	58.283226
2478.436498	75107.811074	58.288231
2477.757862	74903.957872	58.293236
2477.076102	74721.161302	58.298241
2476.417476	74531.558058	58.303245
2476.163768	74340.904026	58.308250
2475.166301	74155.793057	58.313255
2474.773110	73951.207299	58.318260
2473.753088	73775.188697	58.323265
2473.110615	73590.634865	58.328269
2472.214046	73395.758209	58.333274
2472.224971	73210.153969	58.338279
2471.215693	73012.872447	58.343284
2470.656461	72828.971300	58.348289
2469.910930	72635.566883	58.353293
2469.503880	72438.208224	58.358298
2468.251050	72252.319074	58.363303
2467.964916	72058.752386	58.368308
2467.515632	71870.807219	58.373313
2466.410401	71677.792197	58.378317
2465.550670	71485.538319	58.383322
2464.782199	71308.120576	58.388327
2464.765403	71115.584606	58.393332
2463.763693	70920.115332	58.398337
2462.812963	70741.534301	58.403341
2462.753282	70549.979816	58.408346
2461.569249	70367.885465	58.413351
2461.297842	70175.253306	58.418356
2460.706171	69988.507753	58.423361
2460.149464	69805.888393	58.428365
2459.517980	69607.947366	58.433370
2458.464999	69432.510839	58.438375
2457.847862	69232.297343	58.443380
2457.199216	69045.322738	58.448385
2456.490873	68866.612587	58.453389
2455.891440	68658.414956	58.458394
2455.053037	68482.908562	58.463399
2454.545760	68296.336724	58.468404
2453.865798	68112.922922	58.473409
2453.610077	67923.540570	58.478413
2452.526890	67732.467155	58.483418
2451.539080	67548.100419	58.488423
2451.218445	67346.035142	58.493428
2450.437106	67163.799039	58.498433
2449.537049	66988.917539	58.503437
2449.240625	66811.034907	58.508442
2448.558451	66631.023748	58.513447
2448.021481	66437.419147	58.518452
2447.237104	66264.840625	58.523457
2446.496092	66069.853419	58.528461
2445.971980	65882.506263	58.533466
2445.178514	65703.645485	58.538471
2444.568452	65503.497688	58.543476
2443.789996	65316.338841	58.548481
2443.450342	65150.032622	58.553485
2442.955523	64961.613187	58.558490
2442.110788	64770.756003	58.563495
2441.380541	64575.823361	58.568500
2440.735553	64392.869854	58.573505
2440.144185	64198.941727	58.578509
2439.587112	64012.653355	58.583514
2438.879958	63827.299284	58.588519
2437.982941	63632.269700	58.593524
2437.522861	63445.205267	58.598529
2436.550582	63260.091865	58.603533
2436.083491	63073.624243	58.608538
2435.364275	62894.033866	58.613543
2434.671411	62702.125285	58.618548
2433.751274	62518.967403	58.623553
2433.296626	62325.584340	58.628557
2433.030166	62136.257416	58.633562
2431.749346	61968.918714	58.638567
2431.277433	61772.226192	58.643572
2430.581273	61584.096784	58.648577
2429.778846	61413.337719	58.653581
2429.524013	61215.818782	58.658586
2428.687186	61040.737799	58.663591
2428.426385	60850.384480	58.668596
2427.158013	60674.298989	58.673601
2426.626505	60483.254701	58.678605
2426.348141	60291.922133	58.683610
2425.090310	60105.545796	58.688615
2424.596698	59920.452467	58.693620
2424.144904	59742.881885	58.698625
2423.383714	59563.655852	58.703629
2423.065057	59378.818686	58.708634
2422.171251	59204.210169	58.713639
2421.565703	58996.802278	58.718644
2420.594440	58824.786198	58.723649
2420.043112	58636.853236	58.728653
2419.505732	58448.489476	58.733658
2418.606469	58260.865526	58.738663
2417.973545	58076.151218	58.743668
2417.391523	57900.248878	58.748673
2416.892879	57716.564524	58.753677
2416.124717	57531.044638	58.758682
2415.738373	57344.684287	58.763687
2415.186233	57151.123102	58.768692
2414.428423	56968.753267	58.773697
2413.840939	56781.085339	58.778701
2413.181132	56587.597756	58.783706
2412.415894	56410.232081	58.788711
2411.629920	56212.236254	58.793716
2410.785812	56015.777235	58.798721
2410.206741	55846.125559	58.803725
2409.820589	55646.967880	58.808730
2409.174941	55472.833020	58.813735
2408.139707	55278.114826	58.818740
2407.593201	55092.384917	58.823745
2407.094817	54908.380333	58.828749
2406.536167	54705.937299	58.833754
2405.485791	54524.163395	58.838759
2405.065952	54345.345131	58.843764
2404.276985	54156.982755	58.848769
2403.483280	53975.179939	58.853773
2402.723073	53780.886587	58.858778
2402.392272	53595.745245	58.863783
2401.655833	53414.369304	58.868788
2400.678152	53232.897354	58.873793
2400.069101	53062.345903	58.878797
2399.707454	52869.394558	58.883802
2398.811676	52683.007252	58.888807
2398.013337	52495.742570	58.893812
2397.541837	52317.484003	58.898817
2396.854919	52137.634952	58.903821
2396.143139	51962.224621	58.908826
2395.327428	51778.108965	58.913831
2395.109838	51594.558473	58.918836
2394.509597	51416.351349	58.923841
2393.712505	51232.263618	58.928845
2393.147669	51041.186465	58.933850
2392.334702	50866.116069	58.938855
2391.561518	50675.300480	58.943860
2391.172544	50493.076102	58.948865
2390.200505	50303.194545	58.953869
2389.821251	50121.927881	58.958874
2388.996227	49942.587726	58.963879
2388.467049	49746.434451	58.968884
2387.463484	49562.969212	58.973889
2386.799598	49384.691094	58.978893
2386.858596	49191.579541	58.983898
2385.634679	49021.571951	58.988903
2385.073734	48838.461568	58.993908
2384.292114	48644.831198	58.998913
2383.822781	48464.639601	59.003917
2383.095409	48277.869514	59.008922
2382.342040	48093.500265	59.013927
2381.773409	47914.538436	59.018932
2380.621256	47730.562028	59.023937
2380.448881	47556.317732	59.028941
2379.907543	47362.353223	59.033946
2378.849618	47186.124059	59.038951
2378.455788	46999.422094	59.043956
2377.883326	46825.042823	59.048961
2376.971620	46639.856569	59.053965
2376.612555	46460.686410	59.058970
2375.712183	46273.392359	59.063975
2375.127964	46081.109371	59.068980
2374.122743	45908.484242	59.073985
2373.234584	45735.320341	59.078989
2373.025209	45546.937570	59.083994
2372.280155	45375.155744	59.088999
2371.542166	45181.391908	59.094004
2371.339457	45001.724717	59.099009
2370.358030	44826.329410	59.104013
2369.624407	44636.002653	59.109018
2369.297599	44470.071597	59.114023
2368.380140	44283.051363	59.119028
2367.575213	44099.209677	59.124033
2367.057560	43918.366917	59.129037
2366.634333	43733.646243	59.134042
2365.957414	43559.638584	59.139047
2365.257138	43382.154310	59.144052
2364.655855	43198.887567	59.149057
2364.057981	43010.460909	59.154061
2363.529544	42819.653386	59.159066
2362.515809	42636.888085	59.164071
2361.750669	42453.016377	59.169076
2361.159822	42280.301336	59.174081
2359.989638	42108.287072	59.179085
2360.107202	41915.486457	59.184090
2359.234120	41729.678888	59.189095
2358.616592	41556.032938	59.194100
2358.398502	41365.239667	59.199105
2357.227622	41183.039597	59.204109
2356.668134	41006.733701	59.209114
2355.633269	40827.864590	59.214119
2355.400703	40638.330722	59.219124
2354.712557	40460.125094	59.224129
2353.802240	40278.766026	59.229133
2353.000792	40091.070711	59.234138
2352.380847	39911.111368	59.239143
2351.680590	39736.240024	59.244148
2350.883850	39555.226324	59.249153
2349.994837	39381.128437	59.254157
2349.627110	39205.207465	59.259162
2349.101578	39040.201109	59.264167
2348.457141	38856.638028	59.269172
2347.926458	38684.401729	59.274177
2346.736653	38507.216082	59.279181
2346.228407	38330.460102	59.284186
2345.648179	38158.083642	59.289191
2345.047316	37981.873972	59.294196
2344.212790	37803.648142	59.299201
2343.643610	37630.220891	59.304205
2343.339653	37447.983236	59.309210
2342.274752	37283.466753	59.314215
2341.916295	37092.291336	59.319220
2341.135903	36922.972058	59.324225
2340.130281	36755.172898	59.329229
2339.865705	36575.968599	59.334234
2339.347030	36404.407951	59.339239
2338.630377	36221.284754	59.344244
2337.912075	36046.308839	59.349249
2337.289038	35869.286952	59.354253
2336.906631	35676.819446	59.359258
2335.917636	35498.302607	59.364263
2335.032646	35319.545150	59.369268
2335.070511	35140.317641	59.374273
2333.956222	34965.504289	59.379277
2333.304105	34788.702291	59.384282
2332.712212	34614.679037	59.389287
2332.050794	34427.536349	59.394292
2330.989973	34259.503761	59.399297
2330.341919	34077.200697	59.404301
2330.133213	33901.139046	59.409306
2329.184714	33731.554613	59.414311
2328.491231	33556.047614	59.419316
2328.094153	33373.326818	59.424321
2326.979996	33196.534355	59.429325
2326.685216	33018.652964	59.434330
2325.854499	32853.670266	59.439335
2325.113788	32674.542120	59.444340
2324.663389	32496.793716	59.449345
2323.778389	32319.441684	59.454349
2323.315042	32136.250371	59.459354
2322.390976	31975.485250	59.464359
2321.704935	31793.156364	59.469364
2320.982289	31621.169931	59.474369
2320.307566	31453.042865	59.479373
2320.110960	31274.355557	59.484378
2319.190739	31105.924902	59.489383
2318.395432	30931.245608	59.494388
2317.836004	30754.536622	59.499393
2316.942889	30601.467347	59.504397
2316.745850	30419.061869	59.509402
2315.821333	30253.421603	59.514407
2315.048258	30078.310155	59.519412
2314.623839	29897.616664	59.524417
2314.021879	29731.483351	59.529421
2313.440198	29553.430397	59.534426
2312.284270	29387.502196	59.539431
2312.120202	29213.440998	59.544436
2311.471640	29034.587440	59.549441
2310.851117	28861.512447	59.554445
2310.354426	28680.679531	59.559450
2309.474204	28515.686536	59.564455
2308.689401	28347.133190	59.569460
2308.047913	28160.726662	59.574465
2307.731411	27986.396221	59.579469
2306.695530	27807.867166	59.584474
2305.839013	27637.706872	59.589479
2305.145362	27459.549181	59.594484
2304.767301	27286.386116	59.599489
2303.676888	27124.094645	59.604493
2303.008933	26940.237132	59.609498
2302.361920	26782.306850	59.614503
2301.862373	26614.009019	59.619508
2300.815936	26443.406406	59.624513
2300.330841	26281.422306	59.629517
2299.632049	26117.371949	59.634522
2299.234869	25950.650795	59.639527
2298.611923	25778.848299	59.644532
2297.911601	25607.108085	59.649537
2297.105781	25445.457314	59.654541
2296.529021	25264.476164	59.659546
2296.079656	25106.035727	59.664551
2295.338601	24933.374836	59.669556
2294.613100	24761.593145	59.674561
2294.132302	24591.889481	59.679565
2293.250021	24418.302489	59.684570
2292.826789	24247.230213	59.689575
2292.042612	24072.893773	59.694580
2291.436642	23917.416701	59.699585
2290.517837	23745.941119	59.704589
2290.139799	23567.816670	59.709594
2289.532376	23394.505176	59.714599
2288.730838	23230.217109	59.719604
2287.856087	23052.805004	59.724609
2287.087927	22883.075813	59.729613
2286.899752	22719.308518	59.734618
2285.883075	22561.468909	59.739623
2285.262205	22381.624998	59.744628
2284.546358	22206.596896	59.749633
2283.908674	22049.107352	59.754637
2283.368001	21888.120111	59.759642
2282.511810	21717.111275	59.764647
2281.789121	21555.607489	59.769652
2281.185180	21388.369732	59.774657
2280.516393	21224.154780	59.779661
2280.057686	21055.538596	59.784666
2278.947391	20896.784477	59.789671
2278.368402	20733.116251	59.794676
2277.907358	20565.549487	59.799681
2276.956047	20404.648000	59.804685
2276.618807	20232.453307	59.809690
2275.677400	20077.236005	59.814695
2274.950874	19916.603085	59.819700
2274.222987	19753.025892	59.824705
2273.597380	19600.510762	59.829709
2273.004739	19424.366496	59.834714
2272.279046	19280.038254	59.839719
2271.514255	19120.403265	59.844724
2271.082809	18958.157105	59.849729
2269.988539	18810.962247	59.854733
2269.856071	18649.307392	59.859738
2269.319876	18487.282065	59.864743
2268.389829	18323.087121	59.869748
2267.870782	18175.811732	59.874753
2267.130135	18010.965174	59.879757
2266.628616	17842.780623	59.884762
2265.849097	17684.846082	59.889767
2265.169516	17525.850521	59.894772
2264.721194	17367.288808	59.899777
2263.499568	17213.934720	59.904782
2262.952069	17040.267155	59.909786
2262.218599	16893.413247	59.914791
2261.476337	16739.839786	59.919796
2260.947181	16580.367845	59.924801
2260.015675	16433.522268	59.929806
2259.443463	16281.664736	59.934810
2258.490577	16133.402584	59.939815
2257.913542	15979.469048	59.944820
2257.318348	15831.755111	59.949825
2256.129033	15690.947307	59.954830
2255.580997	15537.570631	59.959834
2254.924212	15398.002138	59.964839
2253.861215	15266.917639	59.969844
2253.071368	15129.148219	59.974849
2252.413008	15002.009823	59.979854
2251.814927	14858.086935	59.984858
2251.259843	14734.838242	59.989863
2250.145512	14596.392214	59.994868
2249.737097	14453.255572	59.999873
2248.989179	14341.572698	60.004878
2248.140636	14211.356502	60.009882
2247.459291	14088.393170	60.014887
2246.619104	13969.961469	60.019892
2245.972068	13831.357343	60.024897
2244.917610	13723.157384	60.029902
2244.700564	13605.785877	60.034906
2243.733191	13489.047554	60.039911
2242.948657	13379.659491	60.044916
2242.812835	13250.720578	60.049921
2241.791533	13141.806524	60.054926
2240.874430	13030.362662	60.059930
2240.300495	12915.713184	60.064935
2239.275390	12811.338672	60.069940
2238.969709	12698.003385	60.074945
2238.045263	12590.825708	60.079950
2237.548675	12478.634265	60.084954
2236.729955	12372.876629	60.089959
2236.426936	12273.682541	60.094964
2235.949163	12149.278276	60.099969
2235.012897	12040.629660	60.104974
2234.444064	11937.708645	60.109978
2233.671031	11817.876039	60.114983
2233.063467	11710.390913	60.119988
2232.649822	11604.086283	60.124993
2231.575656	11500.237735	60.129998
2231.432156	11379.829721	60.135002
2230.834570	11272.275681	60.140007
2230.103279	11165.014074	60.145012
2229.623275	11046.536370	60.150017
2228.594131	10935.890920	60.155022
2227.850030	10819.249871	60.160026
2227.335435	10716.245473	60.165031
2226.268023	10602.860599	60.170036
2225.847139	10495.036271	60.175041
2225.346488	10388.454311	60.180046
2224.688635	10280.196859	60.185050
2223.882514	10177.399394	60.190055
2223.535417	10064.881898	60.195060
2223.051491	9954.893687	60.200065
2221.863730	9848.558473	60.205070
2221.451814	9729.676485	60.210074
2220.878530	9616.689293	60.215079
2219.919420	9516.523936	60.220084
2219.449474	9406.669263	60.225089
2218.646694	9310.760397	60.230094
2218.055522	9193.584526	60.235098
2217.287508	9088.851071	60.240103
2216.841383	8977.989001	60.245108
2216.076057	8871.700374	60.250113
2215.369461	8771.618652	60.255118
2214.727583	8663.663367	60.260122
2214.069972	8555.129104	60.265127
2213.683037	8456.051629	60.270132
2212.582226	8342.098920	60.275137
2212.126768	8244.779641	60.280142
2211.364821	8133.414545	60.285146
2210.715720	8031.425729	60.290151
2209.906582	7929.582124	60.295156
2209.384030	7823.724312	60.300161
2208.850176	7718.714359	60.305166
2208.065827	7612.518135	60.310170
2207.331136	7514.998598	60.315175
2206.692119	7404.025704	60.320180
2206.572078	7300.737114	60.325185
2205.321373	7209.856309	60.330190
2205.131438	7086.606552	60.335194
2204.454914	6989.274491	60.340199
2203.585847	6879.985205	60.345204
2202.946952	6773.240565	60.350209
2202.341996	6668.930445	60.355214
2201.539171	6558.230816	60.360218
2201.140537	6458.785031	60.365223
2199.990837	6349.570977	60.370228
2199.578023	6245.946442	60.375233
2198.628281	6153.124036	60.380238
2198.058681	6051.630320	60.385242
2197.559440	5948.728350	60.390247
2196.655616	5849.596329	60.395252
2196.048236	5741.492593	60.400257
2195.404634	5646.949353	60.405262
2194.879839	5540.205704	60.410266
2194.088651	5436.366816	60.415271
2193.256869	5329.551913	60.420276
2192.817235	5230.284122	60.425281
2191.997673	5147.542934	60.430286
2191.679343	5041.681147	60.435290
2190.608721	4944.893516	60.440295
2189.964929	4847.551346	60.445300
2189.809911	4743.448372	60.450305
2189.152086	4633.564722	60.455310
2188.672115	4539.089346	60.460314
2187.566341	4439.251858	60.465319
2186.816326	4331.953991	60.470324
2186.480222	4228.627930	60.475329
2185.431533	4126.849542	60.480334
2184.885587	4035.941034	60.485338
2184.058502	3941.511143	60.490343
2183.381623	3845.520050	60.495348
2182.989366	3752.786711	60.500353
2182.135029	3645.198061	60.505358
2181.667832	3552.697127	60.510362
2181.060396	3451.054510	60.515367
2179.945918	3348.227214	60.520372
2179.489567	3247.444563	60.525377
2178.612644	3163.471970	60.530382
2178.005853	3067.134912	60.535386
2177.060628	2975.226870	60.540391
2176.078333	2881.275575	60.545396
2175.652479	2783.765752	60.550401
2174.982053	2699.351375	60.555406
2174.510586	2606.477728	60.560410
2173.577061	2521.296976	60.565415
2173.209865	2438.220830	60.570420
2172.321190	2337.061919	60.575425
2171.753260	2260.770832	60.580430
2171.358343	2161.484259	60.585434
2170.588748	2075.865274	60.590439
2169.710920	1988.348439	60.595444
2169.446894	1902.345850	60.600449
2168.557986	1819.733726	60.605454
2167.751531	1728.014156	60.610458
2166.907823	1643.918823	60.615463
2166.143714	1565.677611	60.620468
2165.530107	1477.884544	60.625473
2164.476546	1404.406611	60.630478
2163.928443	1323.793511	60.635482
2163.448240	1248.603300	60.640487
2162.782962	1164.625934	60.645492
2162.599569	1084.803989	60.650497
2161.612498	1012.655660	60.655502
2160.905256	916.532416	60.660506
2160.348914	842.167796	60.665511
2159.407377	763.650717	60.670516
2158.754347	687.439697	60.675521
2157.880766	608.007436	60.680526
2157.318437	531.467429	60.685530
2156.650183	468.324296	60.690535
2155.591831	397.205160	60.695540
2154.843028	323.417807	60.700545
2154.061417	268.049375	60.705550
2153.376092	198.247192	60.710554
2152.541889	127.432871	60.715559
2151.449641	82.685143	60.720564
2150.669157	26.264804	60.725569
2149.066125	-11.929575	60.730574
2148.285017	-55.491457	60.735578
2147.332876	-80.884411	60.740583
2146.392676	-108.084862	60.745588
2145.711434	-127.056656	60.750593
2144.821635	-146.734936	60.755598
2143.998299	-160.077971	60.760602
2143.468266	-174.049438	60.765607
2142.597628	-185.185060	60.770612
2142.506558	-217.071194	60.775617
2141.949395	-228.108288	60.780622
2141.036450	-255.241820	60.785626
2140.280797	-273.463591	60.790631
2139.626561	-276.978878	60.795636
2138.960039	-281.903600	60.800641
2137.801587	-291.899052	60.805646
2137.159877	-309.995352	60.810650
2136.132945	-304.568457	60.815655
2134.266000	-273.726358	60.820660
2132.417217	-229.686251	60.825665
2129.734733	-140.943570	60.830670
2129.320009	-92.353931	60.835674
2129.773342	-57.255835	60.840679
2130.230385	-20.891915	60.845684
2130.766493	-10.445776	60.850689
2130.604660	2.940253	60.855694
2130.636998	8.765319	60.860698
2130.871407	5.071106	60.865703
2130.634913	-7.357484	60.870708
2130.519520	-30.539876	60.875713
2129.631273	-53.053954	60.880718
2129.169068	-85.854482	60.885722
2128.389051	-93.352245	60.890727
2127.043818	-111.231494	60.895732
2125.137983	-104.528052	60.900737
2123.523558	-68.079980	60.905742
2122.872915	-58.778116	60.910746
2122.585862	-53.408607	60.915751
2121.740611	-38.362410	60.920756
2121.995061	-40.525380	60.925761
2121.539044	-28.218670	60.930766
2121.373744	-40.229585	60.935770
2120.957629	-52.705326	60.940775
2119.868604	-47.525530	60.945780
2119.108391	-59.296941	60.950785
2118.143521	-51.968486	60.955790
2117.587632	-46.647780	60.960794
2117.189342	-35.425744	60.965799
2116.133399	-31.515939	60.970804
2115.691440	-45.488880	60.975809
2114.682810	-36.904496	60.980814
2114.502654	-25.767531	60.985818
2114.063239	-34.825398	60.990823
2113.247547	-35.080705	60.995828
2112.680258	-38.740732	61.000833
2111.544343	-31.255808	61.005838
2111.195663	-30.098120	61.010842
2110.559022	-26.284812	61.015847
2110.088356	-29.900248	61.020852
2109.280379	-31.800004	61.025857
2108.225346	-19.797209	61.030862
2107.619091	-20.705509	61.035866
2107.436930	-16.530646	61.040871
2106.772009	-16.775183	61.045876
2106.317847	-22.851772	61.050881
2105.517528	-20.053303	61.055886
2104.640610	-12.570044	61.060890
2104.190624	-27.467422	61.065895
2102.914296	-9.872175	61.070900
2102.254905	-12.833174	61.075905
2101.838999	-7.395890	61.080910
2101.250488	-7.616281	61.085914
2101.036602	-16.057069	61.090919
2100.234907	-12.381570	61.095924
2099.758172	-13.633706	61.100929
2098.998019	-10.319623	61.105934
2098.126310	-10.044051	61.110938
2097.242640	-14.789309	61.115943
2096.787420	3.308026	61.120948
2096.711771	-6.214446	61.125953
2096.280676	-7.148964	61.130958
2094.982101	-2.669192	61.135962
2093.861634	-8.371956	61.140967
2093.286517	1.193939	61.145972
2093.034944	-9.566939	61.150977
2092.457439	-6.387497	61.155982
2091.574616	-1.101622	61.160986
2091.593613	-5.111743	61.165991
2090.711376	-0.079857	61.170996
2090.380393	-0.008369	61.176001
2089.181095	-1.339807	61.181006
2088.288439	-3.650334	61.186010
2087.744510	-8.771213	61.191015
2086.775360	3.476605	61.196020
2086.177284	-1.555256	61.201025
2085.352798	9.245582	61.206030
2084.674696	-1.532769	61.211034
2084.235841	5.590818	61.216039
2083.528976	8.369736	61.221044
2083.518481	4.622920	61.226049
2082.609673	3.688520	61.231054
2081.828981	-1.158236	61.236058
2081.224046	-0.145960	61.241063
2080.803139	7.326450	61.246068
2079.804707	2.072689	61.251073
2079.081570	2.636934	61.256078
2078.705634	6.419921	61.261082
2078.306141	5.231225	61.266087
2076.782583	11.752654	61.271092
2076.418062	2.627693	61.276097
2076.137363	6.640002	61.281102
2075.952492	6.846003	61.286106
2074.537281	-3.116753	61.291111
2073.676492	11.488832	61.296116
2073.061899	2.160702	61.301121
2072.835469	5.908924	61.306126
2072.319537	5.375815	61.311130
2071.310071	4.416392	61.316135
2070.200004	7.628319	61.321140
2070.181002	11.767836	61.326145
2069.913571	10.083506	61.331150
2068.472911	9.992053	61.336154
2067.892732	6.108561	61.341159
2067.070859	11.228651	61.346164
2066.955334	17.734790	61.351169
2066.497932	9.875127	61.356174
2065.476553	13.263799	61.361178
2064.512057	6.169034	61.366183
2063.781452	17.536894	61.371188
2063.474791	11.501548	61.376193
2063.096450	15.862102	61.381198
2062.032519	14.947597	61.386202
2061.454017	11.063840	61.391207
2060.751168	14.805672	61.396212
2060.227976	6.570090	61.401217
2059.613584	10.160683	61.406222
2058.783835	14.148166	61.411226
2058.339382	14.857427	61.416231
2057.686519	18.573981	61.421236
2056.969602	15.508575	61.426241
2056.161165	17.879409	61.431246
2055.823062	18.223276	61.436250
2055.231967	19.695422	61.441255
2054.574577	11.526870	61.446260
2054.040496	11.692100	61.451265
2053.046495	14.388861	61.456270
2051.588021	22.775026	61.461274
2051.873277	15.661691	61.466279
2051.006233	24.305662	61.471284
2050.043475	17.226392	61.476289
2049.320673	24.385594	61.481294
2048.923906	21.690436	61.486298
2048.653131	17.625373	61.491303
2047.447187	30.634645	61.496308
2047.086290	19.886375	61.501313
2046.161771	19.331383	61.506318
2045.430329	23.349002	61.511322
2045.062411	21.994445	61.516327
2044.176964	25.432518	61.521332
2043.905606	22.263281	61.526337
2043.420031	17.797059	61.531342
2042.424077	24.185885	61.536346
2042.189587	24.581119	61.541351
2041.371348	30.042854	61.546356
2040.992421	22.867769	61.551361
2039.475269	27.774938	61.556366
2038.754932	21.270647	61.561370
2038.878188	28.782864	61.566375
2037.651007	29.682593	61.571380
2037.047933	19.395399	61.576385
2036.233278	28.225031	61.581390
2035.720026	28.831672	61.586394
2035.566522	22.242147	61.591399
2034.409136	21.257328	61.596404
2034.226528	23.118820	61.601409
2033.514600	28.931124	61.606414
2032.925138	21.185466	61.611418
2032.271446	21.327106	61.616423
2031.016956	23.037018	61.621428
2030.152766	25.667453	61.626433
2029.465509	30.401906	61.631438
2029.169482	36.509335	61.636442
2029.273899	22.519023	61.641447
2028.093440	34.680567	61.646452
2027.570911	26.244599	61.651457
2026.980009	28.222938	61.656462
2026.166628	22.074050	61.661466
2025.515907	24.012996	61.666471
2023.929287	28.727767	61.671476
2023.770188	26.258249	61.676481
2023.761005	29.287581	61.681486
2022.449426	26.926866	61.686490
2022.030629	23.951349	61.691495
2021.147384	19.261237	61.696500
2020.579126	25.743040	61.701505
2019.947856	28.267121	61.706510
2019.403115	21.011124	61.711514
2018.984366	26.731162	61.716519
2018.189367	36.574847	61.721524
2017.696695	22.978937	61.726529
2017.264005	22.938842	61.731534
2016.215152	24.075211	61.736538
2015.440740	24.634996	61.741543
2014.649664	31.065434	61.746548
2013.999044	26.049809	61.751553
2013.261660	26.181082	61.756558
2012.704616	31.352200	61.761562
2012.443768	22.978785	61.766567
2011.792840	26.575191	61.771572
2010.963673	20.711098	61.776577
2009.810444	22.477489	61.781582
2009.036016	27.492295	61.786586
2008.485378	24.856261	61.791591
2007.828574	33.630884	61.796596
2008.226698	29.216794	61.801601
2007.177023	31.070832	61.806606
2006.162599	32.676418	61.811610
2006.092761	28.809705	61.816615
2005.393823	20.149428	61.821620
2004.090471	27.459140	61.826625
2003.368479	31.858481	61.831630
2002.523119	24.964026	61.836634
2002.086879	24.118651	61.841639
2001.184934	26.685700	61.846644
2000.851508	23.887453	61.851649
2000.257489	34.505083	61.856654
1999.762940	30.098641	61.861658
1999.487521	23.205187	61.866663
1998.784399	28.435765	61.871668
1998.288093	29.826645	61.876673
1997.430988	33.269696	61.881678
1996.264978	33.929494	61.886682
1995.822680	31.661052	61.891687
1994.694695	31.627243	61.896692
1994.032196	29.114627	61.901697
1993.840870	23.627123	61.906702
1992.782306	29.101785	61.911706
1992.056634	24.154852	61.916711
1990.923343	31.577929	61.921716
1991.053716	26.991867	61.926721
1990.455992	26.400791	61.931726
1989.795277	33.718893	61.936730
1989.596270	28.623703	61.941735
1988.833502	26.136466	61.946740
1988.489642	19.184493	61.951745
1987.423767	20.788789	61.956750
1986.178969	20.278350	61.961754
1985.620570	19.529642	61.966759
1984.735153	31.595477	61.971764
1984.743326	33.964445	61.976769
1983.953262	30.983211	61.981774
1983.324767	25.790613	61.986778
1982.452966	29.127188	61.991783
1981.266458	33.516690	61.996788
1980.692903	23.874549	62.001793
1980.305256	33.904320	62.006798
1980.011766	29.439157	62.011802
1979.525693	22.924509	62.016807
1979.095307	38.321278	62.021812
1978.563936	28.547855	62.026817
1977.321656	34.338700	62.031822
1976.700935	31.165002	62.036826
1976.126077	29.151003	62.041831
1975.511586	30.300442	62.046836
1974.219711	31.877540	62.051841
1973.092806	34.209065	62.056846
1973.301473	31.006216	62.061850
1972.954805	30.864161	62.066855
1971.585646	35.793608	62.071860
1971.195113	25.849595	62.076865
1970.670563	28.290512	62.081870
1969.979493	27.974463	62.086874
1969.791451	25.686167	62.091879
1969.188893	26.925179	62.096884
1967.998052	25.540412	62.101889
1967.071342	22.814272	62.106894
1966.190375	28.306484	62.111898
1965.873254	19.681808	62.116903
1965.267034	25.242371	62.121908
1965.111457	26.911914	62.126913
1964.654088	27.618510	62.131918
1963.391849	30.696940	62.136922
1962.673579	19.759411	62.141927
1962.058032	24.468300	62.146932
1961.400013	22.894872	62.151937
1960.953143	30.841369	62.156942
1959.915532	29.933766	62.161946
1959.254599	30.915535	62.166951
1958.270821	37.852832	62.171956
1957.874194	27.196986	62.176961
1957.374052	20.231979	62.181966
1956.538265	34.246995	62.186970
1956.362714	28.063112	62.191975
1955.873683	36.151927	62.196980
1955.328248	32.188823	62.201985
1954.065389	33.204645	62.206990
1953.031022	39.333091	62.211994
1952.497647	33.366863	62.216999
1952.296139	52.143089	62.222004
1951.824150	42.557363	62.227009
1951.190130	39.696450	62.232014
1950.463656	47.531221	62.237018
1949.698381	36.651609	62.242023
1948.560502	45.272377	62.247028
1948.305521	37.565105	62.252033
1947.762025	34.458004	62.257038
1947.120778	42.574142	62.262042
1946.093769	41.379424	62.267047
1945.100869	43.519372	62.272052
1944.746194	33.110762	62.277057
1944.056708	36.830004	62.282062
1943.316862	35.602316	62.287066
1943.300592	34.999371	62.292071
1942.459718	47.466598	62.297076
1942.167524	37.404468	62.302081
1940.927537	28.940492	62.307086
1940.271077	32.025268	62.312090
1939.991891	27.887435	62.317095
1939.361158	39.499680	62.322100
1938.414261	50.761569	62.327105
1937.200182	41.216385	62.332110
1936.201720	46.251011	62.337114
1936.261567	35.948487	62.342119
1935.613395	37.133246	62.347124
1935.287849	36.374390	62.352129
1934.817925	38.120648	62.357134
1933.854138	43.141884	62.362138
1932.574957	36.669570	62.367143
1932.008405	41.086833	62.372148
1931.561101	30.450075	62.377153
1931.506212	42.114412	62.382158
1930.769294	44.046566	62.387162
1930.329470	37.707512	62.392167
1929.042563	44.863260	62.397172
1928.059830	35.525792	62.402177
1927.368619	42.602739	62.407182
1926.887829	42.726417	62.412186
1926.939851	35.525513	62.417191
1926.424493	44.279277	62.422196
1925.154066	34.017631	62.427201
1924.373934	43.352762	62.432206
1923.418822	41.585227	62.437210
1923.329825	38.060614	62.442215
1922.744871	46.664574	62.447220
1922.166060	40.965770	62.452225
1920.917153	39.401002	62.457230
1920.022781	46.877647	62.462234
1919.618126	36.048032	62.467239
1919.334796	47.622480	62.472244
1918.958288	41.643970	62.477249
1918.490808	40.391972	62.482254
1916.978487	37.407150	62.487258
1916.445814	42.451412	62.492263
1915.613991	43.938154	62.497268
1915.074612	41.653599	62.502273
1915.063329	39.124349	62.507278
1913.856016	50.244656	62.512282
1913.219255	36.165429	62.517287
1912.141500	44.732508	62.522292
1911.988311	42.869202	62.527297
1911.533235	41.604197	62.532302
1911.025447	38.969265	62.537306
1910.315769	31.655899	62.542311
1909.077246	40.759447	62.547316
1908.614397	48.159700	62.552321
1908.023011	39.103892	62.557326
1907.573080	39.435569	62.562330
1906.908293	29.743275	62.567335
1905.485440	28.232942	62.572340
1905.036053	34.000437	62.577345
1904.447008	32.042325	62.582350
1903.695514	34.396279	62.587354
1903.760374	30.851972	62.592359
1903.121500	36.289998	62.597364
1902.219884	34.286892	62.602369
1901.286024	29.907642	62.607374
1900.626305	34.451666	62.612378
1900.412846	32.071215	62.617383
1899.727535	35.406593	62.622388
1898.903643	41.266668	62.627393
1898.128494	42.014267	62.632398
1896.818932	43.311928	62.637402
1896.659790	40.495486	62.642407
1896.073952	38.103191	62.647412
1895.768923	37.635982	62.652417
1894.789589	42.237063	62.657422
1893.551678	46.237362	62.662426
1893.339587	39.300748	62.667431
1892.877972	44.281692	62.672436
1892.140481	39.880727	62.677441
1892.051164	39.995875	62.682446
1890.659464	47.739151	62.687450
1889.952283	37.418059	62.692455
1889.251049	47.459783	62.697460
1888.823150	32.615682	62.702465
1888.302402	35.994322	62.707470
1887.727810	44.104618	62.712474
1887.321732	36.818750	62.717479
1886.034666	43.542444	62.722484
1885.491378	38.599700	62.727489
1885.076333	31.789935	62.732494
1884.144722	42.913782	62.737498
1883.221582	39.963171	62.742503
1882.303138	42.401988	62.747508
1881.760048	38.432221	62.752513
1881.565393	41.965676	62.757518
1880.766650	44.863318	62.762522
1880.889975	43.938580	62.767527
1880.273949	34.900889	62.772532
1879.351196	37.649482	62.777537
1878.737774	41.545902	62.782542
1877.756351	48.235265	62.787546
1876.454418	39.502026	62.792551
1875.719673	37.314734	62.797556
1874.823176	42.183374	62.802561
1875.294891	50.047118	62.807566
1874.450346	56.170689	62.812570
1873.774363	40.560129	62.817575
1873.542771	39.474118	62.822580
1872.399160	43.311215	62.827585
1871.659900	41.123063	62.832590
1870.654311	43.892698	62.837594
1870.303602	40.250366	62.842599
1870.141662	39.219530	62.847604
1869.430113	38.793215	62.852609
1868.302431	43.532981	62.857614
1867.309809	48.555663	62.862618
1867.250965	35.007608	62.867623
1866.681887	33.640862	62.872628
1865.764359	46.095041	62.877633
1864.721482	38.579120	62.882638
1863.379526	47.560336	62.887642
1863.600940	45.421505	62.892647
1863.182896	44.500722	62.897652
1862.861292	43.638745	62.902657
1862.386336	42.744346	62.907662
1861.146755	45.319319	62.912666
1860.463662	38.079019	62.917671
1859.585742	38.680517	62.922676
1859.191682	38.293682	62.927681
1858.893638	42.352923	62.932686
1857.693685	48.023558	62.937690
1857.517289	35.809385	62.942695
1856.354198	41.865260	62.947700
1855.949360	38.458613	62.952705
1855.661236	33.743452	62.957710
1854.055214	40.046281	62.962714
1853.900697	29.044504	62.967719
1853.284560	43.464649	62.972724
1852.421727	41.885922	62.977729
1852.413772	39.944365	62.982734
1851.143221	41.477135	62.987738
1850.391744	36.102245	62.992743
1849.886089	45.553085	62.997748
1849.225647	46.548997	63.002753
1849.204750	36.107910	63.007758
1847.802901	46.106342	63.012762
1847.233738	35.613538	63.017767
1846.454605	44.065409	63.022772
1846.007071	39.804503	63.027777
1845.710483	41.073808	63.032782
1844.275665	44.234893	63.037786
1843.813465	29.727425	63.042791
1843.131259	41.253236	63.047796
1842.536369	36.041148	63.052801
1842.096031	36.511665	63.057806
1841.546506	38.772062	63.062810
1840.490709	37.356448	63.067815
1839.672166	29.998892	63.072820
1838.948406	33.312003	63.077825
1838.825417	45.769335	63.082830
1838.122188	40.467214	63.087834
1837.741655	35.287323	63.092839
1836.647604	38.160904	63.097844
1835.923558	32.560885	63.102849
1835.741409	37.849126	63.107854
1835.069319	42.849305	63.112858
1833.940458	36.039355	63.117863
1833.115514	43.432454	63.122868
1832.720350	46.076785	63.127873
1832.230941	33.502304	63.132878
1831.673142	39.611885	63.137882
1830.692369	37.678146	63.142887
1829.703574	46.035578	63.147892
1829.130980	42.100471	63.152897
1829.010072	35.179354	63.157902
1828.343237	42.881669	63.162906
1827.669211	33.380108	63.167911
1826.493223	41.852421	63.172916
1826.105924	46.346897	63.177921
1825.963075	43.945777	63.182926
1825.102139	50.981888	63.187930
1824.439094	31.109837	63.192935
1823.299851	46.401553	63.197940
1822.883268	49.687970	63.202945
1822.531392	45.492304	63.207950
1821.116578	39.300217	63.212954
1820.308202	42.309795	63.217959
1819.798090	42.434995	63.222964
1819.329815	54.112933	63.227969
1819.205671	40.865418	63.232974
1818.085488	44.826553	63.237978
1818.066365	37.952352	63.242983
1816.846287	47.147629	63.247988
1816.013065	49.744828	63.252993
1815.732709	35.880287	63.257998
1815.275255	48.668284	63.263002
1814.575771	36.616035	63.268007
1813.549854	33.315910	63.273012
1812.743546	42.623679	63.278017
1812.288564	32.320920	63.283022
1811.818838	47.484242	63.288026
1810.923502	48.692511	63.293031
1809.823360	46.113819	63.298036
1809.235144	52.228239	63.303041
1808.904398	41.046284	63.308046
1808.324954	41.370158	63.313050
1807.822237	42.218027	63.318055
1807.409759	38.104531	63.323060
1806.142722	43.651793	63.328065
1805.624068	41.807108	63.333070
1804.687781	40.803050	63.338074
1804.653946	38.113378	63.343079
1804.001684	41.389912	63.348084
1802.852748	43.508958	63.353089
1802.512286	41.449890	63.358094
1801.639496	42.304488	63.363098
1801.073512	37.264444	63.368103
1800.422488	38.064901	63.373108
1799.669774	36.214809	63.378113
1799.218199	31.429419	63.383118
1798.151352	43.478380	63.388122
1798.023409	42.260796	63.393127
1797.200712	41.563563	63.398132
1796.301149	41.195512	63.403137
1795.640153	38.405160	63.408142
1795.370031	48.433630	63.413146
1794.829880	41.754139	63.418151
1793.771924	40.381466	63.423156
1792.837492	46.672297	63.428161
1792.591657	41.764342	63.433166
1792.063516	41.255305	63.438170
1791.408387	43.341667	63.443175
1790.391064	43.503266	63.448180
1789.750502	46.631286	63.453185
1789.338469	40.672639	63.458190
1788.797349	40.492101	63.463194
1787.698477	33.746801	63.468199
1786.698191	38.105232	63.473204
1786.192983	43.465282	63.478209
1786.180904	35.292099	63.483214
1785.643048	47.041009	63.488218
1784.676806	42.294774	63.493223
1783.742393	36.158886	63.498228
1782.864622	38.488771	63.503233
1782.366544	36.188226	63.508238
1781.806414	38.002453	63.513242
1781.584887	31.879511	63.518247
1780.621890	32.873025	63.523252
1779.665280	41.677954	63.528257
1779.033437	31.043739	63.533262
1778.617198	41.494389	63.538266
1778.263024	39.694553	63.543271
1777.362062	37.256138	63.548276
1776.663778	42.396110	63.553281
1776.227096	38.879415	63.558286
1775.495789	48.487529	63.563290
1774.710074	33.156227	63.568295
1773.662161	41.138274	63.573300
1773.109072	39.825782	63.578305
1772.694548	41.460763	63.583310
1772.171271	46.178695	63.588314
1771.365110	42.499900	63.593319
1770.535071	38.796513	63.598324
1769.484935	46.446171	63.603329
1769.466856	38.627188	63.608334
1768.932827	47.792376	63.613338
1768.292072	40.119594	63.618343
1767.064130	46.256768	63.623348
1766.311880	45.840100	63.628353
1766.121030	35.725645	63.633358
1765.345380	50.169560	63.638362
1765.162243	47.722802	63.643367
1764.159475	33.603993	63.648372
1763.286514	40.061690	63.653377
1762.987573	41.407073	63.658382
1762.387610	43.134588	63.663386
1761.592105	37.750951	63.668391
1760.741511	30.319666	63.673396
1759.885701	33.295791	63.678401
1759.505831	34.918962	63.683406
1759.030947	41.296091	63.688410
1757.921873	43.486097	63.693415
1756.960534	46.575182	63.698420
1756.580499	44.713222	63.703425
1756.030149	50.588241	63.708430
1755.678521	48.761194	63.713434
1755.047620	54.338340	63.718439
1754.517130	45.736543	63.723444
1753.542153	52.669356	63.728449
1753.251032	45.317948	63.733454
1752.123689	54.656224	63.738458
1751.409568	49.019958	63.743463
1750.405013	48.365815	63.748468
1749.970825	51.803276	63.753473
1749.617900	39.479960	63.758478
1748.955081	55.380452	63.763482
1748.626686	43.346558	63.768487
1747.407485	42.735970	63.773492
1746.671107	45.265767	63.778497
1746.255054	39.968528	63.783502
1745.762813	51.487844	63.788506
1745.357375	46.963222	63.793511
1744.702996	40.743447	63.798516
1743.705426	51.423635	63.803521
1743.531678	43.531602	63.808526
1742.534858	48.092932	63.813530
1741.529648	39.785744	63.818535
1741.169831	46.051559	63.823540
1740.092783	46.113851	63.828545
1739.495803	32.854724	63.833550
1738.369252	49.270422	63.838554
1737.919578	42.521381	63.843559
1738.200243	40.198086	63.848564
1737.199766	45.988477	63.853569
1736.646961	41.961940	63.858574
1735.322671	45.318419	63.863578
1734.637791	40.442360	63.868583
1734.472308	36.896792	63.873588
1734.039134	43.238914	63.878593
1733.261464	41.653009	63.883598
1732.029806	47.007023	63.888602
1731.624138	54.125393	63.893607
1731.269485	48.857827	63.898612
1730.670342	52.039208	63.903617
1729.830017	42.433200	63.908622
1728.653138	49.087420	63.913626
1728.453586	41.002365	63.918631
1728.154218	41.231308	63.923636
1726.848195	45.111606	63.928641
1726.478914	35.815573	63.933646
1725.619556	41.353310	63.938650
1725.271725	41.377056	63.943655
1724.509674	44.281530	63.948660
1723.350178	51.500709	63.953665
1722.899804	43.387683	63.958670
1722.163590	44.610131	63.963674
1721.798229	45.619130	63.968679
1721.435646	36.178528	63.973684
1721.169647	45.782129	63.978689
1720.268824	42.424325	63.983694
1719.166832	48.689751	63.988698
1718.729850	46.516713	63.993703
1718.069153	44.437559	63.998708
1716.625746	43.184490	64.003713
1716.219648	42.282336	64.008718
1715.444638	49.293786	64.013722
1714.929383	52.778822	64.018727
1714.932959	42.116235	64.023732
1714.186450	52.759708	64.028737
1713.352629	49.045900	64.033742
1712.236957	53.028439	64.038746
1711.832653	52.547057	64.043751
1711.663702	46.183951	64.048756
1710.719034	51.314189	64.053761
1710.265399	44.456971	64.058766
1709.222181	49.774755	64.063770
1708.511955	48.545584	64.068775
1707.598752	50.338636	64.073780
1706.470071	57.874637	64.078785
1706.596493	48.288545	64.083790
1705.816853	47.417340	64.088794
1705.697166	52.536390	64.093799
1705.142964	49.563514	64.098804
1704.368825	42.241531	64.103809
1703.679342	47.684482	64.108814
1702.833886	47.340986	64.113818
1702.059775	48.105824	64.118823
1700.803746	42.740164	64.123828
1700.100119	58.407441	64.128833
1700.186162	37.610609	64.133838
1699.518519	55.544615	64.138842
1699.065611	48.264647	64.143847
1698.248885	42.494885	64.148852
1697.011533	48.816515	64.153857
1696.736037	40.429707	64.158862
1696.288240	43.514511	64.163866
1695.963140	42.899123	64.168871
1694.952243	44.327641	64.173876
1694.477956	47.623240	64.178881
1693.474965	42.080191	64.183886
1692.637868	46.010601	64.188890
1691.757818	49.511007	64.193895
1691.416136	41.588887	64.198900
1690.899554	42.847421	64.203905
1690.102535	43.477126	64.208910
1689.365067	44.983641	64.213914
1688.696208	47.986865	64.218919
1688.326978	49.370230	64.223924
1687.661593	52.734035	64.228929
1686.923566	48.241755	64.233934
1685.909242	43.104220	64.238938
1685.218440	35.079863	64.243943
1685.084831	41.353902	64.248948
1684.329233	49.778416	64.253953
1683.558025	48.792335	64.258958
1682.482667	46.321730	64.263962
1682.295222	46.819912	64.268967
1681.964752	45.653431	64.273972
1680.824698	47.640226	64.278977
1680.066511	43.799297	64.283982
1679.221029	44.952380	64.288986
1678.732556	56.095780	64.293991
1678.649647	44.830329	64.298996
1678.084420	54.976645	64.304001
1677.115751	40.653759	64.309006
1676.025959	55.759467	64.314010
1675.656847	51.397826	64.319015
1674.923205	41.603003	64.324020
1673.937441	52.590425	64.329025
1673.360767	41.428646	64.334030
1672.696269	47.919489	64.339034
1672.239764	54.329984	64.344039
1672.185654	41.858292	64.349044
1670.640360	50.939702	64.354049
1670.305169	44.489467	64.359054
1669.593430	53.954142	64.364058
1669.165478	56.420772	64.369063
1668.696907	48.064636	64.374068
1667.204330	50.943245	64.379073
1666.923146	41.904471	64.384078
1666.372739	50.252236	64.389082
1666.008341	49.392352	64.394087
1665.438682	45.117768	64.399092
1663.925463	47.507635	64.404097
1663.780260	42.679910	64.409102
1663.528802	57.859034	64.414106
1662.374826	45.601487	64.419111
1661.885242	47.283103	64.424116
1660.806267	39.312533	64.429121
1660.594545	39.830342	64.434126
1659.988690	50.506673	64.439130
1658.895830	51.741640	64.444135
1658.187341	48.257107	64.449140
1657.371822	50.993470	64.454145
1657.437935	44.142010	64.459150
1656.980644	47.450684	64.464154
1655.998605	52.355058	64.469159
1655.019977	42.744244	64.474164
1654.311539	42.330110	64.479169
1653.961135	41.523200	64.484174
1652.653529	48.821128	64.489178
1651.799863	43.281185	64.494183
1651.905484	38.945062	64.499188
1651.150703	47.640694	64.504193
1651.001374	45.341545	64.509198
1650.224659	46.109965	64.514202
1648.969310	51.628631	64.519207
1648.717232	42.834401	64.524212
1648.102580	58.180035	64.529217
1647.172716	43.381053	64.534222
1646.300078	51.043557	64.539226
1645.869417	48.361736	64.544231
1645.512785	45.169826	64.549236
1645.005697	49.757470	64.554241
1643.818368	42.729815	64.559246
1643.035648	41.427023	64.564250
1642.816551	42.556302	64.569255
1642.030979	43.088005	64.574260
1641.051911	43.021229	64.579265
1640.340738	46.233041	64.584270
1639.698207	48.986082	64.589274
1639.249423	41.983029	64.594279
1639.079930	43.435596	64.599284
1637.788961	47.559555	64.604289
1637.224258	44.678252	64.609294
1636.684394	45.331776	64.614298
1635.892791	45.072790	64.619303
1635.540247	48.199242	64.624308
1634.240780	42.170297	64.629313
1633.473814	42.025672	64.634318
1633.236854	48.412328	64.639322
1632.777100	49.953589	64.644327
1632.393219	43.815457	64.649332
1631.723901	46.668951	64.654337
1630.779068	45.980136	64.659342
1630.283568	42.444429	64.664346
1629.233620	46.984274	64.669351
1628.189648	47.471877	64.674356
1627.444551	46.049569	64.679361
1626.837431	43.258589	64.684366
1626.628478	51.507957	64.689370
1626.386600	54.137424	64.694375
1626.351199	38.920377	64.699380
1625.047193	51.122191	64.704385
1624.446413	51.214524	64.709390
1623.569866	43.803182	64.714394
1622.528031	39.866985	64.719399
1621.629251	38.719837	64.724404
1621.122615	43.373644	64.729409
1621.026475	35.994443	64.734414
1620.532362	45.375659	64.739418
1619.667855	44.079560	64.744423
1619.004827	43.729187	64.749428
1618.084890	49.101534	64.754433
1617.749160	44.903340	64.759438
1616.581047	46.519296	64.764442
1615.644862	47.846086	64.769447
1615.503928	43.486055	64.774452
1614.761251	53.463445	64.779457
1614.560264	37.820113	64.784462
1613.297213	49.868763	64.789466
1612.332519	49.522164	64.794471
1612.069317	45.209944	64.799476
1611.454707	47.007628	64.804481
1611.565512	39.138220	64.809486
1610.538464	51.594088	64.814490
1609.467010	52.145991	64.819495
1609.226949	46.453379	64.824500
1608.281313	49.700873	64.829505
1607.172767	48.482976	64.834510
1606.471960	40.606894	64.839514
1605.673018	46.108257	64.844519
1605.594384	42.777567	64.849524
1605.017552	55.972484	64.854529
1604.951960	48.471728	64.859534
1604.191714	45.241446	64.864538
1602.988738	49.338825	64.869543
1602.635916	39.289557	64.874548
1601.311136	52.737350	64.879553
1600.773420	42.233320	64.884558
1600.212462	43.875822	64.889562
1599.805212	43.972106	64.894567
1599.596840	33.314828	64.899572
1598.244171	50.400438	64.904577
1597.863085	46.405002	64.909582
1597.331587	47.076128	64.914586
1595.900649	46.228011	64.919591
1595.300343	38.928915	64.924596
1594.784419	50.936139	64.929601
1594.544062	43.236067	64.934606
1593.970885	47.217614	64.939610
1593.115922	51.657105	64.944615
1592.478626	41.186247	64.949620
1591.510298	49.053206	64.954625
1591.370576	40.400413	64.959630
1591.206320	45.848247	64.964634
1589.761387	50.709492	64.969639
1589.160382	47.625806	64.974644
1588.433411	60.198016	64.979649
1587.304316	49.821064	64.984654
1586.711677	42.807764	64.989658
1585.729557	56.043422	64.994663
1585.585328	49.862489	64.999668
1584.940656	59.348066	65.004673
1584.713196	52.082768	65.009678
1584.464537	51.999311	65.014682
1583.131909	45.169820	65.019687
1582.814495	48.883644	65.024692
1582.087231	55.089582	65.029697
1581.104679	51.569769	65.034702
1580.156654	50.611814	65.039706
1579.739014	50.949454	65.044711
1579.447001	51.726039	65.049716
1578.712344	52.325367	65.054721
1577.850695	46.458706	65.059726
1577.059091	53.551675	65.064730
1576.475918	47.845774	65.069735
1576.199214	40.400647	65.074740
1574.879665	51.901612	65.079745
1574.203256	41.588366	65.084750
1573.652522	42.861810	65.089754
1573.018333	49.011956	65.094759
1572.893803	45.423625	65.099764
1572.388506	47.684932	65.104769
1571.529822	40.501016	65.109774
1570.618162	47.507401	65.114778
1569.999618	51.794213	65.119783
1569.029977	44.424495	65.124788
1568.098777	46.772399	65.129793
1567.438998	49.340535	65.134798
1567.206212	54.553250	65.139802
1566.630748	50.320615	65.144807
1566.432256	48.459804	65.149812
1565.413904	53.213855	65.154817
1564.527285	43.533269	65.159822
1563.912789	39.234299	65.164826
1563.766706	47.117274	65.169831
1562.958520	43.918279	65.174836
1561.923524	49.614861	65.179841
1561.461627	44.775966	65.184846
1560.931659	41.464954	65.189850
1559.858149	49.433793	65.194855
1558.995538	47.066636	65.199860
1558.155433	60.478441	65.204865
1557.689883	43.738566	65.209870
1557.487406	51.051748	65.214874
1557.343816	47.064314	65.219879
1556.513736	44.053308	65.224884
1555.183986	51.958785	65.229889
1555.023014	40.650566	65.234894
1554.243217	48.121716	65.239898
1553.110902	52.384511	65.244903
1552.955674	47.960523	65.249908
1551.998270	41.549257	65.254913
1551.579642	53.481099	65.259918
1550.686531	56.885852	65.264922
1550.117174	53.473863	65.269927
1549.613377	40.493314	65.274932
1549.297165	53.717785	65.279937
1548.231576	47.946620	65.284942
1547.504361	45.617879	65.289946
1546.559396	41.607974	65.294951
1546.391539	41.992663	65.299956
1544.995963	46.928089	65.304961
1544.748407	50.264955	65.309966
1544.109109	42.533666	65.314970
1543.412426	51.319439	65.319975
1543.329806	50.965167	65.324980
1541.930052	54.174456	65.329985
1541.070686	45.809491	65.334990
1541.066776	47.119054	65.339994
1540.172202	45.983883	65.344999
1539.887938	40.127994	65.350004
1539.016073	53.212097	65.355009
1538.100078	44.660586	65.360014
1537.557000	50.124463	65.365018
1536.929971	47.538525	65.370023
1536.743895	44.381034	65.375028
1535.368132	55.589744	65.380033
1534.882865	45.777583	65.385038
1534.434340	43.871349	65.390042
1533.570554	49.127563	65.395047
1533.019118	47.337033	65.400052
1531.796481	47.849912	65.405057
1531.379421	48.144889	65.410062
1531.186057	48.562018	65.415066
1530.768933	48.956356	65.420071
1529.626227	40.574922	65.425076
1528.892131	51.307918	65.430081
1528.204966	43.290920	65.435086
1528.091935	41.038054	65.440090
1526.844219	52.188570	65.445095
1526.317343	35.038983	65.450100
1525.528705	33.705629	65.455105
1525.422492	37.952033	65.460110
1524.658794	43.709595	65.465114
1523.227583	52.478053	65.470119
1523.191738	39.853670	65.475124
1522.133748	45.301600	65.480129
1521.967371	47.849686	65.485134
1520.961978	45.287609	65.490138
1520.357999	39.671769	65.495143
1519.813353	35.148819	65.500148
1519.268496	36.558537	65.505153
1518.052465	35.340414	65.510158
1517.584840	36.280533	65.515162
1516.659533	42.670919	65.520167
1516.807886	37.008067	65.525172
1515.889577	40.905697	65.530177
1515.649826	39.969256	65.535182
1514.807179	39.543373	65.540186
1514.173951	38.398220	65.545191
1512.670424	33.505669	65.550196
1511.869566	37.714226	65.555201
1511.309473	34.835379	65.560206
1511.155962	30.371702	65.565210
1510.511923	42.517558	65.570215
1510.412069	32.160029	65.575220
1509.330303	43.862927	65.580225
1508.300737	35.687460	65.585230
1507.991817	40.491215	65.590234
1507.363573	33.087778	65.595239
1506.533393	33.162976	65.600244
1505.386162	39.410432	65.605249
1504.976053	41.131485	65.610254
1504.758603	35.722313	65.615258
1504.400378	48.565515	65.620263
1503.832345	34.704196	65.625268
1502.864825	39.136365	65.630273
1502.211076	37.385758	65.635278
1501.182008	47.850235	65.640282
1500.546463	51.556276	65.645287
1500.071923	38.134270	65.650292
1499.398252	47.894125	65.655297
1498.254276	44.934602	65.660302
1498.017957	38.221104	65.665306
1497.048525	46.233347	65.670311
1496.668468	36.727766	65.675316
1496.281011	43.420621	65.680321
1494.934135	38.864315	65.685326
1494.494730	37.040222	65.690330
1493.820188	43.797626	65.695335
1493.482248	35.293050	65.700340
1492.864247	43.621612	65.705345
1491.884308	41.435556	65.710350
1491.306707	45.887767	65.715354
1490.820717	41.139453	65.720359
1490.382463	31.359268	65.725364
1489.234511	39.518155	65.730369
1488.494290	46.134608	65.735374
1488.002426	45.939998	65.740378
1487.613726	45.828342	65.745383
1486.256669	39.376540	65.750388
1485.774426	40.815739	65.755393
1485.248932	38.628428	65.760398
1484.807397	31.977512	65.765402
1484.145849	40.298802	65.770407
1483.796751	32.537187	65.775412
1482.497166	33.765655	65.780417
1481.973813	33.960835	65.785422
1481.812814	26.562001	65.790426
1480.916653	38.361564	65.795431
1480.191634	36.962919	65.800436
1479.116210	45.632270	65.805441
1478.942525	45.622065	65.810446
1478.555266	40.872255	65.815450
1477.382055	49.442030	65.820455
1476.777647	37.280187	65.825460
1476.167115	38.763431	65.830465
1475.384840	37.553665	65.835470
1474.362770	41.444144	65.840474
1473.555187	36.854182	65.845479
1473.575963	33.160765	65.850484
1472.854306	31.707972	65.855489
1472.805708	40.922195	65.860494
1472.352957	33.255906	65.865498
1471.114725	41.985826	65.870503
1470.717001	43.156123	65.875508
1469.256198	44.623114	65.880513
1468.434112	43.984238	65.885518
1468.006547	36.804390	65.890522
1467.644690	35.975672	65.895527
1467.772171	36.319735	65.900532
1466.066213	40.478185	65.905537
1465.426857	45.208303	65.910542
1464.917225	38.415244	65.915546
1464.240087	46.201265	65.920551
1463.585599	30.888682	65.925556
1462.955411	39.189220	65.930561
1462.182298	37.288857	65.935566
1461.744459	41.343535	65.940570
1460.893038	39.119720	65.945575
1459.845576	30.557608	65.950580
1459.418605	36.845150	65.955585
1458.640678	37.908715	65.960590
1458.446760	36.821490	65.965594
1458.034678	34.259761	65.970599
1457.501266	38.619795	65.975604
1456.733925	42.346790	65.980609
1455.836281	31.713936	65.985614
1454.694749	31.811827	65.990618
1453.547331	40.218230	65.995623
1453.381267	31.199058	66.000628
1452.651963	39.621009	66.005633
1452.601377	38.774360	66.010638
1452.441687	29.443509	66.015642
1451.019490	46.827228	66.020647
1450.866205	36.516044	66.025652
1450.061647	37.511303	66.030657
1448.759611	30.460989	66.035662
1447.887749	37.524157	66.040666
1447.241458	35.444366	66.045671
1447.156688	33.450373	66.050676
1446.895130	31.471863	66.055681
1446.188336	35.736450	66.060686
1445.573109	32.696068	66.065690
1444.207121	43.499544	66.070695
1444.167139	40.916522	66.075700
1442.781775	45.594902	66.080705
1441.983644	35.674804	66.085710
1441.955498	30.109395	66.090714
1441.479595	38.986246	66.095719
1440.828472	35.552592	66.100724
1439.653936	39.125111	66.105729
1438.811176	35.811805	66.110734
1438.520395	37.649521	66.115738
1437.618071	47.985059	66.120743
1437.496006	34.615865	66.125748
1436.769816	41.554957	66.130753
1435.737327	41.720683	66.135758
1435.451524	39.761796	66.140762
1434.434741	32.961046	66.145767
1433.874668	32.383041	66.150772
1433.008064	42.205108	66.155777
1432.560346	34.580608	66.160782
1432.491006	32.886944	66.165786
1431.137979	40.436615	66.170791
1430.520871	32.247670	66.175796
1429.847887	35.232681	66.180801
1429.352950	43.737238	66.185806
1428.248840	32.298255	66.190810
1427.318891	39.745986	66.195815
1427.166368	28.319760	66.200820
1426.981508	32.258534	66.205825
1426.730649	34.679698	66.210830
1425.637267	29.438155	66.215834
1424.584894	34.319084	66.220839
1424.219364	29.879655	66.225844
1422.969934	35.033186	66.230849
1421.939148	35.260149	66.235854
1421.743983	33.649566	66.240858
1421.163384	41.202622	66.245863
1420.912249	34.092515	66.250868
1420.700318	33.597951	66.255873
1419.416135	34.158512	66.260878
1418.820809	31.657458	66.265882
1417.951180	27.517360	66.270887
1417.488763	27.291274	66.275892
1416.423667	27.252451	66.280897
1415.825362	36.755899	66.285902
1415.508344	32.956902	66.290906
1415.071834	35.836518	66.295911
1414.325702	26.456964	66.300916
1413.423272	32.824816	66.305921
1412.540031	33.790014	66.310926
1412.332850	28.607889	66.315930
1410.941172	37.717043	66.320935
1410.842639	31.699190	66.325940
1410.452717	40.608110	66.330945
1409.841624	34.029896	66.335950
1408.942996	33.434748	66.340954
1408.035705	50.955840	66.345959
1407.648104	36.431925	66.350964
1407.059920	39.997987	66.355969
1405.899717	45.936878	66.360974
1405.243466	38.066404	66.365978
1404.502949	46.411301	66.370983
1404.337739	33.698693	66.375988
1403.667264	41.163534	66.380993
1402.929581	45.228035	66.385998
1402.300772	41.256245	66.391002
1401.348025	39.914324	66.396007
1401.192762	32.061991	66.401012
1399.869368	41.862057	66.406017
1399.266937	42.154982	66.411022
1398.414530	38.877918	66.416026
1398.009590	46.931348	66.421031
1397.806078	41.204577	66.426036
1397.445095	42.435277	66.431041
1396.228066	46.796756	66.436046
1395.685422	34.981526	66.441050
1395.232126	47.819339	66.446055
1394.192579	40.456084	66.451060
1393.156077	44.057145	66.456065
1392.810636	38.568983	66.461070
1392.878992	39.977445	66.466074
1391.491150	42.938904	66.471079
1390.842043	40.534716	66.476084
1390.458878	44.268469	66.481089
1389.959002	44.273852	66.486094
1389.076210	34.195343	66.491098
1388.173354	40.205296	66.496103
1387.745159	30.612780	66.501108
1387.086692	41.171340	66.506113
1385.903186	40.947921	66.511118
1385.446500	32.818646	66.516122
1384.361729	36.804281	66.521127
1384.281382	25.675681	66.526132
1383.906703	40.861740	66.531137
1383.350315	40.604865	66.536142
1382.477804	36.802712	66.541146
1381.374412	39.151242	66.546151
1381.211289	25.187763	66.551156
1380.960551	33.150441	66.556161
1379.516966	34.204726	66.561166
1378.764771	38.656324	66.566170
1377.671001	41.411766	66.571175
1377.613621	42.807099	66.576180
1377.253796	39.869639	66.581185
1376.691339	37.019587	66.586190
1375.938412	36.998966	66.591194
1375.095804	43.368362	66.596199
1374.604599	37.165346	66.601204
1374.244693	44.323774	66.606209
1373.054762	32.209321	66.611214
1372.600802	48.027746	66.616218
1371.833311	47.071133	66.621223
1371.241460	38.985424	66.626228
1370.281712	45.453870	66.631233
1369.751013	38.104356	66.636238
1369.525963	39.548421	66.641242
1368.449531	39.800008	66.646247
1367.483378	29.231706	66.651252
1366.742659	43.159173	66.656257
1366.327121	43.125921	66.661262
1365.991945	38.993919	66.666266
1365.068839	45.401347	66.671271
1365.044696	45.626003	66.676276
1364.173154	44.261724	66.681281
1363.449821	45.568957	66.686286
1363.067818	32.714199	66.691290
1361.635378	47.040225	66.696295
1361.526575	34.848525	66.701300
1360.636494	41.064618	66.706305
1359.426284	43.040623	66.711310
1358.714665	35.350860	66.716314
1358.434575	39.290584	66.721319
1358.311426	41.368169	66.726324
1357.593634	39.306077	66.731329
1356.377476	43.486080	66.736334
1355.803886	39.576490	66.741338
1355.117948	44.672011	66.746343
1354.754888	36.762829	66.751348
1354.282662	37.393041	66.756353
1353.374664	49.038400	66.761358
1352.192820	40.497700	66.766362
1351.758412	50.446628	66.771367
1351.721256	40.511244	66.776372
1350.958976	34.321368	66.781377
1349.947644	50.682578	66.786382
1349.380350	40.385187	66.791386
1348.695697	41.713083	66.796391
1348.305091	45.064816	66.801396
1347.269867	47.858273	66.806401
1346.494210	42.676640	66.811406
1346.352284	44.588473	66.816410
1344.992457	43.760733	66.821415
1344.495926	40.184255	66.826420
1343.984145	42.911842	66.831425
1343.609523	50.698678	66.836430
1343.578158	39.461360	66.841434
1342.215867	43.029076	66.846439
1341.396373	40.199395	66.851444
1341.068613	39.858872	66.856449
1339.887152	38.364098	66.861454
1338.925226	39.737655	66.866458
1338.103181	47.647663	66.871463
1338.035054	46.056314	66.876468
1337.722075	38.270063	66.881473
1337.033588	41.755889	66.886478
1336.486762	39.116254	66.891482
1335.299925	36.488484	66.896487
1334.735039	43.171713	66.901492
1334.329950	45.499131	66.906497
1333.548947	48.524995	66.911502
1332.809063	30.955182	66.916506
1331.785381	39.460229	66.921511
1331.658364	30.007506	66.926516
1331.355705	31.501760	66.931521
1329.860691	49.630400	66.936526
1329.488496	43.837413	66.941530
1328.899771	39.375137	66.946535
1328.701390	35.984656	66.951540
1327.543830	45.733157	66.956545
1327.026809	46.532925	66.961550
1326.485207	27.945977	66.966554
1325.212837	47.373348	66.971559
1324.628391	40.190090	66.976564
1323.982969	35.779409	66.981569
1323.523832	38.514398	66.986574
1323.089552	34.708828	66.991578
1322.305307	43.361897	66.996583
1321.524456	41.279879	67.001588
1321.091388	43.736329	67.006593
1320.628364	46.151810	67.011598
1320.084509	48.441368	67.016602
1318.927686	45.354660	67.021607
1318.360226	47.324689	67.026612
1317.902075	45.483107	67.031617
1316.614018	44.609277	67.036622
1316.273988	38.675560	67.041626
1315.610629	45.942165	67.046631
1315.250663	45.947395	67.051636
1314.401260	40.130935	67.056641
1313.414331	40.445587	67.061646
1313.026108	29.132552	67.066650
1312.126770	40.498988	67.071655
1312.152056	41.143148	67.076660
1310.856227	45.279067	67.081665
1309.872518	44.486164	67.086670
1309.668477	39.756145	67.091674
1308.961805	45.487345	67.096679
1308.613847	39.148027	67.101684
1307.809571	43.424993	67.106689
1307.141463	51.102373	67.111694
1306.775227	48.817239	67.116698
1305.808752	52.446624	67.121703
1305.017713	41.046237	67.126708
1304.095721	38.899932	67.131713
1303.184499	50.933755	67.136718
1302.983390	38.042364	67.141722
1302.907355	40.990841	67.146727
1302.286222	42.242415	67.151732
1301.058137	44.055705	67.156737
1300.693363	38.956997	67.161742
1300.127150	39.770900	67.166746
1298.973935	40.176653	67.171751
1298.442228	45.963616	67.176756
1298.407314	37.634834	67.181761
1297.038408	43.793035	67.186766
1296.089803	43.469229	67.191770
1295.473552	44.213816	67.196775
1295.098340	47.485836	67.201780
1295.110058	38.815317	67.206785
1293.907146	43.026358	67.211790
1293.612765	36.454593	67.216794
1292.863675	43.733255	67.221799
1291.828045	44.022542	67.226804
1290.862601	32.555280	67.231809
1290.278155	42.386134	67.236814
1289.987173	33.166072	67.241818
1289.444397	37.109720	67.246823
1288.360808	34.192738	67.251828
1287.753936	39.444437	67.256833
1286.712172	47.838835	67.261838
1286.787249	35.252049	67.266842
1286.110083	42.492467	67.271847
1285.425977	39.720128	67.276852
1284.563190	39.523033	67.281857
1283.880280	38.059403	67.286862
1283.604321	39.694499	67.291866
1282.609161	49.073412	67.296871
1281.358293	37.135861	67.301876
1280.953173	37.873689	67.306881
1280.460357	43.320148	67.311886
1280.473456	35.045238	67.316890
1279.856128	41.257409	67.321895
1278.763094	37.208079	67.326900
1277.920727	40.973858	67.331905
1277.297978	51.682884	67.336910
1277.035075	41.021719	67.341914
1275.849286	43.783949	67.346919
1275.390117	38.094693	67.351924
1275.165621	42.657955	67.356929
1273.775836	54.039315	67.361934
1273.162872	40.618893	67.366938
1272.894723	48.494460	67.371943
1272.140530	40.029310	67.376948
1271.895008	42.864386	67.381953
1270.770980	53.519077	67.386958
1270.289438	46.292661	67.391962
1269.334520	50.828564	67.396967
1268.694582	47.202363	67.401972
1267.547330	47.048930	67.406977
1267.055728	50.104489	67.411982
1266.787206	39.277062	67.416986
1266.254566	42.927361	67.421991
1265.970045	33.947555	67.426996
1264.749153	39.025653	67.432001
1263.883478	42.773065	67.437006
1263.997471	37.148795	67.442010
1263.064115	52.002643	67.447015
1262.261057	51.715631	67.452020
1261.441667	45.698871	67.457025
1260.914869	53.591915	67.462030
1260.080256	47.013014	67.467034
1258.969488	45.183755	67.472039
1258.633594	41.283703	67.477044
1258.325562	43.067407	67.482049
1257.931684	48.643222	67.487054
1256.966707	37.443986	67.492058
1256.191623	45.210924	67.497063
1255.797159	42.974444	67.502068
1255.097517	37.216198	67.507073
1254.121224	44.436377	67.512078
1253.342731	35.620280	67.517082
1252.724718	40.559937	67.522087
1252.628565	34.842926	67.527092
1251.939571	40.344238	67.532097
1250.447546	48.983715	67.537102
1250.322106	44.100852	67.542106
1249.890886	39.110494	67.547111
1249.375749	30.643615	67.552116
1248.065065	37.010201	67.557121
1247.028187	47.772466	67.562126
1247.046898	38.455853	67.567130
1246.465766	41.049401	67.572135
1245.515822	41.403931	67.577140
1244.747477	39.676348	67.582145
1243.994736	42.923250	67.587150
1243.730121	38.062521	67.592154
1243.379849	38.586625	67.597159
1242.718345	36.092986	67.602164
1241.841133	29.535068	67.607169
1240.916504	41.960544	67.612174
1240.469247	31.456447	67.617178
1239.252800	39.462309	67.622183
1238.694070	41.751093	67.627188
1238.564483	45.032945	67.632193
1237.918096	48.901616	67.637198
1237.557514	34.591084	67.642202
1236.317077	44.152517	67.647207
1235.700755	40.424800	67.652212
1235.251990	40.316427	67.657217
1234.091137	40.035858	67.662222
1233.693512	37.708420	67.667226
1232.650462	49.274357	67.672231
1232.226560	49.449042	67.677236
1232.209184	40.076665	67.682241
1231.316117	45.201998	67.687246
1230.918535	42.198026	67.692250
1229.906440	45.453059	67.697255
1229.254615	45.804341	67.702260
1228.299461	40.545639	67.707265
1227.754154	44.327272	67.712270
1227.649604	37.676445	67.717274
1226.642098	40.233721	67.722279
1225.372328	41.520653	67.727284
1224.727262	38.504000	67.732289
1224.301269	46.237508	67.737294
1223.871848	31.179400	67.742298
1223.723171	44.126471	67.747303
1222.708582	40.044192	67.752308
1221.991205	39.641063	67.757313
1221.096548	37.944615	67.762318
1221.049418	39.451861	67.767322
1219.755326	39.110485	67.772327
1218.729954	39.593717	67.777332
1218.522053	44.644784	67.782337
1218.084065	51.301545	67.787342
1217.423556	40.017638	67.792346
1216.344322	46.888340	67.797351
1215.629868	31.533358	67.802356
1215.540780	35.672955	67.807361
1214.718840	37.662973	67.812366
1213.981161	38.854253	67.817370
1213.001512	48.478305	67.822375
1212.820932	38.266122	67.827380
1212.401802	37.519092	67.832385
1211.085508	47.307071	67.837390
1210.439365	37.315589	67.842394
1209.957327	39.238936	67.847399
1209.495464	35.470893	67.852404
1209.260991	37.897353	67.857409
1207.812690	41.287998	67.862414
1207.360448	31.037021	67.867418
1206.726436	26.943114	67.872423
1205.785663	36.191964	67.877428
1204.881611	29.609944	67.882433
1203.990197	41.820408	67.887438
1204.047367	42.005324	67.892442
1203.814286	36.116124	67.897447
1202.859958	36.707914	67.902452
1202.137703	33.899090	67.907457
1201.119043	38.708505	67.912462
1200.851096	34.045437	67.917466
1200.415386	39.197390	67.922471
1199.352972	36.947299	67.927476
1198.884801	30.975639	67.932481
1197.986039	40.695638	67.937486
1198.004309	35.771004	67.942490
1196.253217	36.122075	67.947495
1195.832562	32.164553	67.952500
1195.731314	34.227619	67.957505
1194.990650	45.065791	67.962510
1194.241539	27.048077	67.967514
1193.545422	35.690306	67.972519
1192.745718	40.247278	67.977524
1192.727234	41.267412	67.982529
1190.893887	46.966508	67.987534
1190.562288	33.696922	67.992538
1190.024494	43.104045	67.997543
1189.414761	36.539876	68.002548
1189.269514	33.150422	68.007553
1188.171670	48.647044	68.012558
1187.697242	38.533639	68.017562
1187.001917	42.914738	68.022567
1186.484036	42.689630	68.027572
1185.647498	35.344656	68.032577
1184.557131	43.286334	68.037582
1184.297688	33.868886	68.042586
1183.880000	33.553726	68.047591
1182.906581	40.270410	68.052596
1182.138452	35.625394	68.057601
1181.315320	42.203057	68.062606
1181.210121	37.834235	68.067610
1180.135880	45.017975	68.072615
1179.242890	43.685560	68.077620
1179.049280	33.388724	68.082625
1178.245262	37.768187	68.087630
1177.748346	31.315393	68.092634
1176.796514	43.934450	68.097639
1175.579228	36.632690	68.102644
1175.569993	42.295570	68.107649
1174.846768	40.546640	68.112654
1174.860972	35.562729	68.117658
1174.185896	39.822335	68.122663
1172.980450	42.590889	68.127668
1172.654958	34.432920	68.132673
1171.607307	50.541318	68.137678
1170.836234	49.206861	68.142682
1170.124206	43.584655	68.147687
1169.567051	43.279063	68.152692
1169.632874	41.522912	68.157697
1168.252452	48.987172	68.162702
1167.560746	38.083569	68.167706
1167.039592	38.573360	68.172711
1166.349613	38.738335	68.177716
1166.355024	34.642087	68.182721
1165.023849	50.219983	68.187726
1164.571104	30.374726	68.192730
1164.023783	33.229423	68.197735
1162.683185	33.900011	68.202740
1162.235690	39.058573	68.207745
1161.023285	43.823124	68.212750
1161.025012	40.959086	68.217754
1160.667348	40.560264	68.222759
1160.076998	46.470117	68.227764
1159.131668	31.390006	68.232769
1158.446799	44.386085	68.237774
1158.114222	32.717303	68.242778
1157.252707	31.149651	68.247783
1156.224913	28.532945	68.252788
1155.407707	25.117909	68.257793
1154.943997	41.204387	68.262798
1154.946594	33.913619	68.267802
1154.345814	40.123179	68.272807
1153.241938	33.465727	68.277812
1152.755585	30.414390	68.282817
1151.429984	35.873472	68.287822
1150.923217	26.465412	68.292826
1150.280091	32.837826	68.297831
1149.600167	32.810392	68.302836
1149.555573	29.267736	68.307841
1148.859214	32.392149	68.312846
1147.806375	35.494416	68.317850
1147.284024	35.421417	68.322855
1146.671057	39.633303	68.327860
1146.323117	34.503564	68.332865
1144.960576	41.326309	68.337870
1144.526479	32.487018	68.342874
1144.129055	37.697543	68.347879
1143.386513	42.466214	68.352884
1142.939457	37.729140	68.357889
1141.374335	43.254713	68.362894
1141.409797	32.162921	68.367898
1140.905603	29.478707	68.372903
1139.889525	38.503007	68.377908
1139.235301	29.446415	68.382913
1138.401651	41.152532	68.387918
1138.111111	40.448141	68.392922
1137.442896	38.308843	68.397927
1136.602311	41.270118	68.402932
1136.362816	39.057897	68.407937
1135.660954	40.674018	68.412942
1134.523959	43.400161	68.417946
1133.809950	39.197569	68.422951
1133.415594	42.912629	68.427956
1132.874306	36.809109	68.432961
1132.280939	39.387279	68.437966
1131.366790	32.042058	68.442970
1130.652117	33.839994	68.447975
1130.133885	39.432443	68.452980
1129.526222	28.884508	68.457985
1128.187939	47.675857	68.462990
1127.880769	37.397092	68.467994
1127.435026	31.368265	68.472999
1127.062600	34.201456	68.478004
1126.538536	33.732912	68.483009
1125.181308	40.876526	68.488014
1125.092921	37.202061	68.493018
1124.357859	41.352947	68.498023
1123.511179	39.995838	68.503028
1122.637235	32.103321	68.508033
1121.631104	37.442214	68.513038
1121.750357	29.894770	68.518042
1120.917289	37.145821	68.523047
1119.923452	44.384602	68.528052
1119.739557	42.489974	68.533057
1119.260636	39.538387	68.538062
1118.229397	44.427106	68.543066
1117.520778	33.425289	68.548071
1116.555462	30.423340	68.553076
1116.525595	29.440939	68.558081
1115.402754	43.892858	68.563086
1114.772617	25.857836	68.568090
1114.292961	28.397420	68.573095
1113.802466	31.824992	68.578100
1113.439564	27.118696	68.583105
1111.769046	39.342722	68.588110
1111.081814	24.571679	68.593114
1111.031566	36.451230	68.598119
1110.305643	29.973381	68.603124
1109.871332	29.078972	68.608129
1108.749786	38.541112	68.613134
1108.248374	39.898268	68.618138
1107.790733	33.970687	68.623143
1106.702138	27.709808	68.628148
1106.067145	27.034983	68.633153
1104.954046	40.521815	68.638158
1104.455224	34.247542	68.643162
1104.518357	36.521009	68.648167
1104.105872	32.409238	68.653172
1103.568013	29.361375	68.658177
1102.345394	45.396690	68.663182
1101.933024	35.528913	68.668186
1101.259087	39.834086	68.673191
1099.985280	37.146149	68.678196
1099.833189	28.735106	68.683201
1099.004828	44.583123	68.688206
1098.614973	37.898847	68.693210
1097.245950	40.952081	68.698215
1096.262738	42.286533	68.703220
1096.435773	33.372751	68.708225
1095.937811	37.025446	68.713230
1095.652431	31.743838	68.718234
1094.485563	33.623179	68.723239
1093.652365	40.071576	68.728244
1093.608100	35.437598	68.733249
1092.256459	38.945393	68.738254
1091.757510	36.038001	68.743258
1091.263280	37.166932	68.748263
1090.705966	44.410398	68.753268
1089.815832	35.884944	68.758273
1088.877046	40.815736	68.763278
1088.546563	38.655843	68.768282
1087.964420	35.072544	68.773287
1086.876026	31.226000	68.778292
1086.187232	32.056295	68.783297
1085.515517	42.429345	68.788302
1085.624657	34.626460	68.793306
1085.007516	39.977603	68.798311
1083.415754	37.141556	68.803316
1083.255735	32.693154	68.808321
1082.493012	40.566972	68.813326
1082.072183	32.422614	68.818330
1080.805013	35.473844	68.823335
1080.041010	40.335832	68.828340
1079.769447	32.186652	68.833345
1079.409241	38.439956	68.838350
1079.136281	29.923562	68.843354
1077.862884	28.161261	68.848359
1077.360838	33.129810	68.853364
1077.023712	30.515228	68.858369
1075.581732	35.087673	68.863374
1074.793436	38.283502	68.868378
1074.544779	27.747862	68.873383
1073.998030	31.507670	68.878388
1073.657741	20.652293	68.883393
1072.357808	37.428473	68.888398
1072.108214	30.182565	68.893402
1071.524266	33.166110	68.898407
1070.629266	32.819668	68.903412
1069.632162	31.879179	68.908417
1068.615563	34.395380	68.913422
1068.368416	33.392353	68.918426
1068.415577	29.401435	68.923431
1067.781298	35.362443	68.928436
1066.903434	29.590038	68.933441
1065.912135	42.256400	68.938446
1065.613310	34.455341	68.943450
1064.768488	30.820798	68.948455
1063.465041	38.135658	68.953460
1063.048635	31.454040	68.958465
1062.343277	38.300006	68.963470
1062.192224	40.183338	68.968474
1061.949823	33.250105	68.973479
1060.434866	33.085877	68.978484
1060.086140	22.018952	68.983489
1059.255604	31.576735	68.988494
1058.870683	41.811120	68.993498
1058.111004	38.439003	68.998503
1057.519591	45.367772	69.003508
1057.065685	37.140369	69.008513
1056.158657	38.387020	69.013518
1055.194916	37.365533	69.018522
1054.703521	38.743183	69.023527
1053.598163	43.599561	69.028532
1054.057372	32.098157	69.033537
1053.174995	31.429586	69.038542
1052.196123	34.110105	69.043546
1051.590992	35.772360	69.048551
1050.514328	30.731770	69.053556
1049.933343	26.255729	69.058561
1049.267175	35.937180	69.063566
1048.747132	29.819267	69.068570
1048.305915	30.980773	69.073575
1047.897200	34.455270	69.078580
1047.435065	37.501443	69.083585
1046.593432	37.897162	69.088590
1045.201816	43.030902	69.093594
1044.368656	38.063536	69.098599
1043.584481	43.354529	69.103604
1043.586824	30.861349	69.108609
1043.019141	33.602610	69.113614
1042.559846	40.445704	69.118618
1041.831797	30.276504	69.123623
1040.903428	37.299883	69.128628
1040.378411	33.176067	69.133633
1039.619437	39.447085	69.138638
1038.654647	37.082183	69.143642
1038.121421	37.334219	69.148647
1037.258655	35.054013	69.153652
1037.110319	33.481747	69.158657
1036.431850	40.156281	69.163662
1035.562270	35.793967	69.168666
1034.963431	35.483999	69.173671
1034.131997	45.384144	69.178676
1034.442460	40.542340	69.183681
1032.907917	42.557479	69.188686
1032.359713	43.799090	69.193690
1031.727686	50.942489	69.198695
1031.007474	50.722796	69.203700
1030.277357	37.568697	69.208705
1029.350458	38.753863	69.213710
1028.871966	31.897625	69.218714
1028.881732	32.999996	69.223719
1027.634815	32.176542	69.228724
1026.900069	24.821751	69.233729
1025.961967	37.426038	69.238734
1025.903812	35.863080	69.243738
1025.305641	38.949825	69.248743
1023.926360	33.167326	69.253748
1023.718763	40.673708	69.258753
1022.731995	35.136270	69.263758
1022.730646	38.173789	69.268762
1022.069924	36.692511	69.273767
1021.216100	35.920058	69.278772
1020.508545	36.477383	69.283777
1019.804166	39.059047	69.288782
1019.036239	42.917138	69.293786
1018.180461	33.954158	69.298791
1017.600801	36.369319	69.303796
1017.516384	28.647701	69.308801
1016.557073	29.391742	69.313806
1015.625124	42.092829	69.318810
1015.058760	33.071187	69.323815
1014.588839	35.658125	69.328820
1014.628496	35.560390	69.333825
1013.334471	36.135335	69.338830
1012.606087	34.778367	69.343834
1011.415929	36.976847	69.348839
1010.327646	42.559089	69.353844
1009.812063	34.871379	69.358849
1009.647541	42.965430	69.363854
1009.022731	38.086354	69.368858
1008.975582	36.002819	69.373863
1008.339743	42.870853	69.378868
1007.471837	27.545117	69.383873
1006.648956	43.980488	69.388878
1006.203286	39.672162	69.393882
1005.292439	32.922571	69.398887
1004.423309	41.213890	69.403892
1003.954660	36.339932	69.408897
1003.158623	38.833680	69.413902
1002.880362	36.715954	69.418906
1001.778867	35.096653	69.423911
1001.393006	34.573029	69.428916
1000.961271	27.182649	69.433921
999.740273	37.761382	69.438926
998.868377	37.255168	69.443930
998.695115	33.773995	69.448935
997.843831	41.786505	69.453940
997.766222	26.253023	69.458945
996.377821	36.565074	69.463950
995.958855	31.583864	69.468954
995.456556	41.724963	69.473959
994.860082	35.608185	69.478964
994.304268	23.769967	69.483969
993.256564	27.675732	69.488974
992.667480	24.658126	69.493978
992.628972	23.771722	69.498983
991.324998	31.657561	69.503988
990.809031	28.385464	69.508993
989.794079	30.513496	69.513998
989.350251	26.600707	69.519002
988.388684	20.501029	69.524007
987.394446	31.627161	69.529012
987.137634	25.618772	69.534017
986.739695	27.935635	69.539022
986.380805	26.964590	69.544026
986.103221	23.252435	69.549031
984.919616	29.521642	69.554036
984.378176	30.112470	69.559041
983.347446	26.417652	69.564046
982.539496	35.344223	69.569050
982.133456	31.948979	69.574055
981.414533	36.993054	69.579060
981.293556	26.963829	69.584065
980.035231	32.894840	69.589070
979.634652	36.757566	69.594074
979.108151	32.749121	69.599079
977.680720	36.669586	69.604084
977.393963	20.806688	69.609089
976.661630	33.168502	69.614094
975.730526	24.502966	69.619098
975.980861	20.550687	69.624103
975.194498	33.462002	69.629108
973.855586	25.000134	69.634113
973.215680	26.475547	69.639118
972.597036	31.746521	69.644122
972.792436	30.316686	69.649127
971.725762	27.824520	69.654132
970.790725	23.926822	69.659137
970.002409	34.252204	69.664142
969.547315	30.123588	69.669146
969.177659	26.287312	69.674151
968.021307	31.833088	69.679156
967.436191	26.067758	69.684161
966.698091	33.589167	69.689166
966.281404	30.876876	69.694170
966.182879	29.063297	69.699175
964.785324	32.611577	69.704180
964.809534	13.684023	69.709185
963.730416	22.068683	69.714190
962.874124	29.299811	69.719194
962.375174	27.717112	69.724199
961.638195	33.579362	69.729204
961.152781	25.150421	69.734209
960.054720	28.138526	69.739214
959.433740	28.967524	69.744218
959.228237	16.061158	69.749223
958.319810	28.458878	69.754228
958.185171	24.883254	69.759233
957.120548	28.143587	69.764238
956.320100	30.276921	69.769242
955.694964	20.666983	69.774247
954.622616	31.936444	69.779252
954.185279	29.531798	69.784257
953.605636	28.597465	69.789262
953.358876	32.904077	69.794266
952.586499	30.401358	69.799271
951.406179	32.743380	69.804276
951.357982	26.692336	69.809281
950.729938	30.214363	69.814286
949.872272	37.784767	69.819290
949.142896	27.882327	69.824295
948.151228	29.328568	69.829300
948.135400	23.269221	69.834305
947.293577	27.342516	69.839310
946.279183	23.518959	69.844314
945.873128	19.067152	69.849319
945.292297	20.607288	69.854324
944.303752	26.673579	69.859329
943.513025	28.464742	69.864334
942.605023	28.579316	69.869338
942.520763	22.554514	69.874343
941.697721	23.671142	69.879348
941.604784	23.966673	69.884353
940.622047	22.514587	69.889358
939.769835	28.122360	69.894362
939.569928	29.127208	69.899367
938.251156	29.770786	69.904372
937.462938	12.916943	69.909377
937.205734	18.816384	69.914382
936.723008	25.063958	69.919386
936.418351	18.456057	69.924391
935.126070	20.591972	69.929396
934.364751	18.864951	69.934401
933.926670	26.373311	69.939406
933.361920	26.586230	69.944410
932.338193	25.886580	69.949415
931.533882	24.778268	69.954420
931.043857	21.634526	69.959425
930.624017	28.827743	69.964430
930.320826	29.949956	69.969434
929.172969	30.556876	69.974439
928.612352	30.122577	69.979444
928.113985	29.083850	69.984449
927.687305	35.481785	69.989454
926.604007	27.050230	69.994458
926.015694	29.498325	69.999463
925.055890	30.699802	70.004468
924.878696	25.249619	70.009473
923.861516	31.479750	70.014478
922.952725	34.846187	70.019482
922.733928	33.480690	70.024487
922.062270	25.705883	70.029492
921.752890	21.339621	70.034497
920.696972	26.104596	70.039502
919.810071	23.639039	70.044506
919.614482	20.626639	70.049511
918.551204	35.947502	70.054516
917.356235	23.067723	70.059521
917.021343	26.964154	70.064526
916.657308	27.856350	70.069530
916.229683	18.986136	70.074535
915.773771	23.810166	70.079540
915.116437	18.586213	70.084545
914.317595	24.235962	70.089550
913.518228	27.584986	70.094554
913.147436	21.353472	70.099559
911.714123	29.624210	70.104564
911.630634	24.942873	70.109569
911.166358	22.605604	70.114574
909.991142	31.398248	70.119578
909.564329	21.327825	70.124583
908.702142	25.582570	70.129588
908.337314	20.882931	70.134593
907.133059	29.033636	70.139598
906.312135	27.256184	70.144602
906.272518	22.501633	70.149607
905.611734	28.157799	70.154612
905.187307	28.764713	70.159617
904.131436	20.617396	70.164622
903.274334	34.591826	70.169626
903.192342	25.168278	70.174631
902.275766	29.365449	70.179636
901.751805	23.814338	70.184641
900.827780	36.831158	70.189646
900.108534	38.653537	70.194650
899.760606	27.618062	70.199655
898.737528	39.959934	70.204660
898.287122	32.804364	70.209665
897.379768	28.662588	70.214670
896.927818	43.088217	70.219674
896.093989	26.829851	70.224679
894.885694	36.917736	70.229684
894.794931	27.142341	70.234689
894.348471	36.364641	70.239694
893.594368	35.831832	70.244698
893.683240	26.880992	70.249703
892.399265	32.541729	70.254708
892.103288	28.443001	70.259713
891.274408	24.585210	70.264718
889.858122	29.732411	70.269722
889.565832	27.500238	70.274727
888.929023	29.833054	70.279732
888.770179	26.430026	70.284737
887.412419	29.798544	70.289742
886.663699	29.231764	70.294746
886.305988	33.691659	70.299751
885.703978	23.027797	70.304756
885.379527	26.108849	70.309761
884.427579	35.685998	70.314766
883.239980	30.078086	70.319770
883.375344	20.780800	70.324775
882.563942	31.466269	70.329780
881.531804	26.085933	70.334785
881.015554	28.823770	70.339790
880.141637	30.024210	70.344794
880.018171	26.388466	70.349799
878.868410	34.852215	70.354804
877.956696	27.580840	70.359809
877.741625	35.566232	70.364814
877.188562	28.343430	70.369818
877.118557	31.801884	70.374823
875.744016	39.055601	70.379828
875.337044	34.446252	70.384833
874.665588	29.196170	70.389838
873.421720	32.669573	70.394842
873.070046	26.171668	70.399847
872.271402	41.811556	70.404852
871.763138	34.982174	70.409857
871.621634	33.252714	70.414862
870.458225	27.760810	70.419866
870.130478	31.548875	70.424871
869.172421	27.585494	70.429876
868.810032	33.618382	70.434881
867.839340	31.443727	70.439886
867.037234	35.624269	70.444890
867.061370	32.305659	70.449895
865.798708	38.302068	70.454900
864.706620	26.553983	70.459905
863.933951	27.102791	70.464910
863.811991	32.991752	70.469914
863.468973	35.747752	70.474919
862.988419	39.709955	70.479924
862.122174	40.623748	70.484929
861.292314	36.042288	70.489934
860.757450	42.283985	70.494938
859.927361	34.338868	70.499943
858.707362	40.303259	70.504948
858.237604	32.895310	70.509953
857.992535	28.069382	70.514958
857.560128	40.367710	70.519962
856.845158	26.126325	70.524967
855.599264	32.288804	70.529972
855.307109	30.581747	70.534977
854.907219	28.360399	70.539982
853.753917	28.236502	70.544986
853.514872	26.700768	70.549991
852.410883	33.752153	70.554996
851.955314	32.168881	70.560001
851.947720	31.023667	70.565006
850.491749	29.916605	70.570010
849.741441	27.096590	70.575015
849.413861	42.488033	70.580020
848.939662	29.452560	70.585025
848.336849	34.517607	70.590030
847.248175	40.755994	70.595034
847.305785	31.370153	70.600039
845.939520	42.656477	70.605044
845.199663	33.962131	70.610049
844.731086	39.098856	70.615054
844.069807	45.325985	70.620058
843.910659	26.337738	70.625063
842.607007	35.217086	70.630068
842.097463	32.354016	70.635073
841.702003	30.920453	70.640078
840.526007	38.059002	70.645082
839.809749	26.522347	70.650087
838.919817	31.915377	70.655092
838.840167	27.689181	70.660097
838.492339	28.523614	70.665102
837.342319	21.772748	70.670106
836.656908	24.923878	70.675111
835.818976	27.842240	70.680116
835.336630	26.600707	70.685121
835.243236	33.899668	70.690126
834.505742	28.533954	70.695130
833.834080	30.099612	70.700135
832.826905	29.618145	70.705140
832.286037	30.858628	70.710145
831.405542	31.948166	70.715150
830.258469	33.225222	70.720154
830.370001	25.232736	70.725159
829.843696	34.190202	70.730164
829.177268	33.441603	70.735169
828.308634	27.131656	70.740174
827.463148	32.889782	70.745178
826.984998	24.715194	70.750183
825.878202	31.997273	70.755188
825.287515	26.903088	70.760193
824.964366	22.643115	70.765198
824.274237	29.934562	70.770202
824.157823	23.132710	70.775207
822.739474	30.579504	70.780212
822.402183	29.152454	70.785217
822.040502	33.054737	70.790222
820.648755	39.295646	70.795226
820.102666	33.014781	70.800231
819.182765	40.598281	70.805236
818.877825	37.295786	70.810241
818.679489	33.703504	70.815246
817.753700	34.718254	70.820250
817.103671	24.713351	70.825255
816.567683	29.815074	70.830260
815.825579	35.925760	70.835265
814.924447	23.794064	70.840270
814.118878	35.544657	70.845274
813.662052	36.677147	70.850279
812.964432	39.281441	70.855284
812.435752	35.814288	70.860289
811.516156	23.168285	70.865294
810.794129	43.547415	70.870298
810.261817	28.233013	70.875303
809.880170	37.011334	70.880308
809.393116	26.299234	70.885313
808.498914	26.675014	70.890318
807.525838	33.713461	70.895322
807.299983	23.475454	70.900327
806.236674	30.211292	70.905332
805.584950	29.677982	70.910337
804.821605	28.998436	70.915342
804.569362	42.007689	70.920346
804.587965	27.215878	70.925351
803.332636	34.122638	70.930356
802.720423	23.346887	70.935361
801.996785	25.152642	70.940366
800.877486	33.078551	70.945370
800.433994	33.915603	70.950375
799.888560	36.065157	70.955380
799.179600	24.334968	70.960385
797.844002	27.690541	70.965390
797.075593	29.788858	70.970394
797.111168	24.000464	70.975399
796.214780	31.528183	70.980404
795.987504	30.913112	70.985409
795.659257	27.661642	70.990414
794.965696	30.452953	70.995418
794.404369	24.475728	71.000423
793.583684	35.747754	71.005428
792.324321	38.996577	71.010433
791.758359	29.517622	71.015438
791.045259	38.383405	71.020442
791.078209	23.551469	71.025447
789.671890	30.641544	71.030452
789.124020	33.445934	71.035457
788.611948	30.373542	71.040462
788.041943	35.723542	71.045466
787.539415	24.395739	71.050471
786.181697	32.298107	71.055476
785.520703	28.594979	71.060481
785.258169	29.969359	71.065486
784.647229	33.507622	71.070490
784.522931	25.063820	71.075495
783.345830	37.707789	71.080500
782.454829	32.868008	71.085505
782.326579	27.935183	71.090510
781.326166	30.795850	71.095514
780.841170	36.957076	71.100519
779.972850	36.213824	71.105524
779.480641	33.472591	71.110529
778.636804	29.122051	71.115534
777.599642	37.489064	71.120538
777.243645	35.435784	71.125543
776.954949	36.178808	71.130548
776.383959	30.075389	71.135553
775.624303	35.207999	71.140558
774.452595	34.216578	71.145562
774.472757	31.936254	71.150567
773.221836	31.337496	71.155572
772.574542	31.765445	71.160577
772.160221	32.553702	71.165582
771.252165	31.968169	71.170586
771.382964	30.670034	71.175591
770.054448	34.858715	71.180596
769.094139	22.342220	71.185601
768.879768	35.714448	71.190606
767.994941	42.738861	71.195610
767.292156	34.918597	71.200615
766.560463	36.192628	71.205620
766.174185	32.950400	71.210625
765.637169	28.128389	71.215630
764.959753	39.538466	71.220634
764.367878	27.961537	71.225639
763.368588	25.597512	71.230644
762.727475	27.888464	71.235649
762.364169	35.107392	71.240654
761.075530	28.597832	71.245658
760.607048	26.579812	71.250663
760.248675	26.334129	71.255668
759.968066	27.274566	71.260673
759.237513	20.680889	71.265678
758.013782	37.358307	71.270682
757.659622	30.737816	71.275687
757.038030	41.301634	71.280692
756.104689	38.267933	71.285697
755.458330	33.062779	71.290702
754.703506	40.965374	71.295706
754.583902	25.451244	71.300711
753.654095	37.543333	71.305716
752.654103	39.459336	71.310721
752.395191	31.722952	71.315726
752.003189	37.214931	71.320730
751.008534	38.499294	71.325735
749.962912	34.584598	71.330740
749.261634	37.637351	71.335745
748.960009	35.745733	71.340750
748.361961	34.248245	71.345754
747.369551	30.312462	71.350759
746.702992	36.562525	71.355764
746.162403	37.889715	71.360769
746.194804	35.653175	71.365774
745.037878	43.011080	71.370778
744.453909	41.279535	71.375783
743.696915	38.925825	71.380788
743.156015	41.361679	71.385793
742.622270	36.677924	71.390798
741.613540	46.376125	71.395802
741.218216	35.874941	71.400807
740.471078	41.546472	71.405812
739.592422	48.170938	71.410817
739.179062	33.399021	71.415822
738.023854	40.721962	71.420826
737.823880	32.351713	71.425831
737.259086	35.078382	71.430836
736.062160	31.886383	71.435841
735.628964	44.705247	71.440846
734.899021	44.200179	71.445850
734.946072	38.976089	71.450855
733.755180	42.165152	71.455860
732.846972	38.473014	71.460865
732.668353	34.942259	71.465870
732.061673	39.192649	71.470874
731.323052	30.794625	71.475879
730.408210	34.699836	71.480884
729.679952	44.077410	71.485889
729.626379	34.524774	71.490894
727.927474	39.062614	71.495898
727.673588	38.655217	71.500903
726.948486	37.695212	71.505908
726.471717	44.072761	71.510913
726.079462	47.580951	71.515918
725.159835	43.296112	71.520922
724.736298	36.574708	71.525927
723.802042	40.836257	71.530932
723.693193	38.816174	71.535937
722.349237	33.630641	71.540942
721.235077	39.079912	71.545946
721.181520	36.943792	71.550951
720.830995	37.974215	71.555956
720.121416	33.998141	71.560961
719.250939	36.481746	71.565966
718.316337	39.464424	71.570970
718.368299	36.705944	71.575975
717.049279	40.290735	71.580980
715.882186	38.016526	71.585985
715.569698	39.682722	71.590990
715.289274	41.719133	71.595994
714.833744	36.425258	71.600999
714.283546	39.487080	71.606004
713.257959	42.197238	71.611009
712.832625	38.874505	71.616014
712.001804	40.826666	71.621018
711.312675	41.873158	71.626023
710.388942	43.340213	71.631028
709.876043	39.485789	71.636033
709.751792	34.175436	71.641038
709.059785	36.502892	71.646042
708.015449	40.416115	71.651047
707.137428	40.193259	71.656052
706.296106	32.704165	71.661057
706.011604	32.894587	71.666062
705.057737	35.460862	71.671066
704.229250	33.328287	71.676071
704.088430	31.444187	71.681076
703.478374	41.000064	71.686081
703.268980	29.631916	71.691086
702.381964	36.268757	71.696090
701.502281	36.758960	71.701095
700.858647	35.249819	71.706100
700.206300	37.033213	71.711105
699.437335	37.076849	71.716110
698.501336	38.041228	71.721114
698.451688	36.811247	71.726119
697.767468	38.577640	71.731124
696.751603	31.080073	71.736129
695.963894	32.292080	71.741134
695.087530	38.350055	71.746138
695.003825	29.245355	71.751143
693.795595	40.019290	71.756148
693.337942	40.527450	71.761153
692.643146	27.998673	71.766158
692.072425	34.411683	71.771162
691.790645	28.662788	71.776167
690.783281	31.893607	71.781172
690.005855	34.305633	71.786177
689.769492	26.658714	71.791182
689.037532	35.153774	71.796186
688.371386	33.148321	71.801191
687.843192	38.963196	71.806196
687.161378	30.347983	71.811201
686.425461	21.936935	71.816206
685.410904	25.594682	71.821210
684.841161	29.951162	71.826215
684.344457	31.438535	71.831220
683.503412	36.751288	71.836225
682.874114	29.755152	71.841230
682.083749	45.024740	71.846234
681.688825	29.224877	71.851239
681.014465	29.187221	71.856244
679.962558	41.175771	71.861249
679.657490	31.721540	71.866254
678.845425	33.435754	71.871258
678.550526	27.162241	71.876263
677.826130	34.197398	71.881268
676.971859	35.449972	71.886273
676.464532	30.156472	71.891278
675.694557	35.028971	71.896282
674.544922	24.179574	71.901287
673.589955	28.742482	71.906292
673.043988	38.650860	71.911297
673.380521	38.319760	71.916302
672.780850	37.920124	71.921306
672.402376	29.449002	71.926311
671.008581	41.069369	71.931316
670.440518	36.775880	71.936321
669.875997	30.833890	71.941326
668.543605	37.418662	71.946330
667.977155	30.075050	71.951335
667.963687	33.510307	71.956340
667.369996	30.898802	71.961345
666.757803	35.265201	71.966350
665.638160	37.312256	71.971354
665.339565	32.966395	71.976359
664.402487	36.536120	71.981364
663.063801	43.445179	71.986369
663.084771	33.726137	71.991374
662.288075	40.173564	71.996378
661.883874	21.793685	72.001383
661.454063	36.644723	72.006388
660.241811	39.709484	72.011393
659.653108	27.113364	72.016398
658.903668	36.319276	72.021402
658.494944	29.764268	72.026407
658.102184	31.850112	72.031412
656.982417	41.004614	72.036417
656.686305	34.783335	72.041422
655.962212	34.100739	72.046426
655.279111	35.110016	72.051431
654.349254	40.850089	72.056436
653.566194	42.198565	72.061441
653.585150	38.005564	72.066446
652.599816	44.823662	72.071450
651.659821	30.028413	72.076455
651.333370	33.869908	72.081460
650.382827	31.972836	72.086465
650.227183	24.764086	72.091470
648.833118	30.937633	72.096474
648.207433	34.812592	72.101479
647.855325	31.708450	72.106484
647.631035	31.894021	72.111489
647.186124	23.859272	72.116494
645.649312	41.982210	72.121498
645.359894	36.803824	72.126503
644.760960	32.994660	72.131508
643.859810	42.415553	72.136513
643.280397	36.289858	72.141518
642.496100	38.988424	72.146522
642.470912	30.456315	72.151527
641.458317	31.011861	72.156532
640.480050	35.304099	72.161537
640.214642	32.162497	72.166542
639.264366	33.073977	72.171546
638.269111	38.357685	72.176551
637.721460	36.164638	72.181556
637.029133	28.994049	72.186561
636.957681	28.631725	72.191566
636.385566	36.883718	72.196570
635.502248	32.993689	72.201575
634.948077	35.122590	72.206580
634.180276	40.146145	72.211585
633.196845	31.905420	72.216590
632.466497	36.552421	72.221594
631.812138	40.635381	72.226599
631.708832	36.521777	72.231604
630.815304	50.623502	72.236609
630.004263	38.835510	72.241614
628.999150	36.243807	72.246618
628.719095	37.988426	72.251623
628.279964	36.151841	72.256628
627.564436	38.818959	72.261633
626.467983	36.555621	72.266638
625.996866	38.606641	72.271642
625.338388	36.592099	72.276647
625.098918	39.399444	72.281652
624.129667	45.068530	72.286657
623.433535	32.003820	72.291662
622.595437	39.605887	72.296666
622.288595	43.562538	72.301671
621.906283	34.309858	72.306676
620.722033	36.961741	72.311681
620.271007	35.227978	72.316686
619.659821	37.764937	72.321690
618.640473	30.230117	72.326695
618.140873	40.802909	72.331700
617.552987	37.152843	72.336705
617.335470	36.440040	72.341710
615.862249	29.303942	72.346714
615.152432	32.703445	72.351719
615.018278	30.766250	72.356724
614.027256	29.902249	72.361729
613.959008	28.418188	72.366734
612.752882	37.693692	72.371738
612.021685	36.979123	72.376743
611.619708	33.417723	72.381748
610.969819	33.354111	72.386753
610.746913	25.962110	72.391758
609.406466	37.566120	72.396762
609.277783	31.682466	72.401767
608.654193	24.605022	72.406772
607.039441	37.635726	72.411777
606.583858	26.157000	72.416782
605.929465	34.811612	72.421786
605.691999	33.395504	72.426791
605.669753	33.421164	72.431796
604.539590	29.251915	72.436801
604.082368	32.034017	72.441806
602.984807	34.210047	72.446810
602.018571	32.451113	72.451815
601.054303	32.674122	72.456820
600.578359	29.788412	72.461825
600.675879	32.234573	72.466830
599.942568	37.916549	72.471834
599.234934	31.322429	72.476839
598.761341	30.456447	72.481844
598.106451	37.442704	72.486849
597.176056	28.485491	72.491854
596.469637	25.024626	72.496858
596.050885	24.660849	72.501863
595.161547	29.665921	72.506868
593.941722	29.611089	72.511873
593.500412	25.672755	72.516878
593.039393	28.692008	72.521882
592.449043	32.654390	72.526887
592.211323	27.322701	72.531892
590.867079	28.856775	72.536897
590.386038	26.938564	72.541902
589.912262	34.443183	72.546906
588.929114	26.256055	72.551911
587.992546	28.603569	72.556916
587.166713	39.614683	72.561921
586.991024	33.792135	72.566926
586.794184	32.158244	72.571930
586.186351	31.696850	72.576935
585.515412	33.375998	72.581940
584.738765	36.743576	72.586945
584.236889	22.473105	72.591950
583.193962	31.874012	72.596954
582.557726	33.613866	72.601959
582.034132	28.736149	72.606964
581.225072	37.912149	72.611969
580.143331	30.015121	72.616974
579.258475	37.052204	72.621978
578.665341	25.511816	72.626983
578.470668	26.184691	72.631988
578.029707	36.030620	72.636993
577.916732	24.344365	72.641998
576.526122	31.963482	72.647002
576.075468	29.887467	72.652007
575.492614	26.935212	72.657012
574.610571	32.850620	72.662017
573.920018	24.098071	72.667022
573.050560	31.386592	72.672026
572.649207	30.147982	72.677031
571.770272	21.477482	72.682036
570.635985	32.028364	72.687041
570.084140	22.982483	72.692046
569.626177	30.154997	72.697050
569.396847	30.123755	72.702055
569.036685	30.865570	72.707060
568.561025	29.575717	72.712065
567.913304	27.775525	72.717070
566.878616	21.785457	72.722074
565.536670	32.591772	72.727079
565.332812	26.163429	72.732084
564.595679	34.208324	72.737089
564.240013	26.919480	72.742094
563.861806	38.310310	72.747098
562.720882	34.257914	72.752103
562.276912	29.550447	72.757108
561.257896	34.539917	72.762113
560.627157	29.343377	72.767118
559.729991	27.988203	72.772122
559.239734	28.438501	72.777127
558.698732	30.267271	72.782132
558.295707	27.912434	72.787137
557.837045	26.301328	72.792142
556.652066	42.654092	72.797146
556.015381	26.692509	72.802151
555.723717	30.777633	72.807156
554.256267	41.279094	72.812161
554.012870	31.036044	72.817166
553.507473	34.032410	72.822170
553.203990	35.608879	72.827175
552.102710	35.989351	72.832180
550.798073	43.093313	72.837185
550.839819	32.202437	72.842190
550.035758	39.032692	72.847194
549.918882	32.675649	72.852199
548.850048	38.400045	72.857204
547.853981	34.762980	72.862209
547.639455	22.878440	72.867214
546.937565	40.174551	72.872218
546.436733	20.821347	72.877223
545.382507	23.020459	72.882228
544.619893	30.843908	72.887233
544.498789	34.613278	72.892238
543.765481	34.555087	72.897242
542.904646	30.924869	72.902247
542.705615	35.801071	72.907252
541.595244	33.994159	72.912257
540.279351	23.647570	72.917262
539.569404	33.405460	72.922266
539.121493	34.784161	72.927271
539.029754	36.150279	72.932276
538.449684	33.550832	72.937281
538.324896	28.059233	72.942286
537.017585	29.510180	72.947290
536.202572	30.158874	72.952295
535.791326	32.935240	72.957300
534.982330	39.329463	72.962305
534.313657	23.721499	72.967310
533.480789	27.932262	72.972314
533.004123	28.971764	72.977319
532.510183	29.578774	72.982324
531.429387	31.354766	72.987329
531.071711	27.243849	72.992334
530.599092	32.684034	72.997338
529.705656	30.926149	73.002343
529.012218	31.840910	73.007348
528.338616	33.646655	73.012353
528.114254	24.955476	73.017358
526.755759	25.518862	73.022362
526.056765	26.212156	73.027367
525.684373	35.755426	73.032372
524.991462	35.283946	73.037377
524.490193	29.093801	73.042382
523.704812	35.080558	73.047386
523.018028	38.952661	73.052391
522.610273	33.405215	73.057396
521.765433	41.011535	73.062401
521.232570	38.776736	73.067406
520.024613	41.536522	73.072410
519.935361	32.967321	73.077415
519.405125	31.712981	73.082420
518.204336	26.112100	73.087425
517.803760	25.795903	73.092430
517.004067	38.674731	73.097434
516.640822	30.065602	73.102439
516.101245	30.607345	73.107444
514.753384	41.226970	73.112449
514.449274	32.745615	73.117454
513.593303	34.400642	73.122458
513.727313	33.436303	73.127463
512.602938	22.267583	73.132468
511.767545	39.165489	73.137473
511.487604	34.293127	73.142478
510.016456	35.025859	73.147482
509.655613	33.323484	73.152487
509.229297	34.302929	73.157492
508.427468	36.263150	73.162497
508.434998	33.270474	73.167502
507.355158	38.835788	73.172506
506.479710	34.801052	73.177511
506.156341	30.780868	73.182516
505.332315	41.651361	73.187521
504.470648	29.130324	73.192526
503.689812	37.683673	73.197530
502.983579	24.157001	73.202535
502.713462	31.648106	73.207540
502.257157	35.410954	73.212545
501.492896	31.243389	73.217550
500.356016	34.225250	73.222554
500.141323	25.803775	73.227559
499.375704	26.805738	73.232564
498.181147	36.158290	73.237569
497.962988	26.806954	73.242574
497.124870	30.644823	73.247578
496.986192	35.120322	73.252583
496.303921	28.027031	73.257588
495.373437	34.487926	73.262593
495.038029	24.000929	73.267598
493.834261	24.476603	73.272602
492.753759	29.982100	73.277607
492.392626	31.263403	73.282612
491.581123	28.852229	73.287617
491.857425	33.736283	73.292622
491.096206	29.997173	73.297626
489.875586	26.364372	73.302631
489.499551	27.965021	73.307636
488.655126	30.301044	73.312641
488.345416	32.250676	73.317646
486.995635	31.344535	73.322650
486.573869	33.580105	73.327655
485.868911	29.392059	73.332660
485.848843	31.715019	73.337665
485.346761	36.872897	73.342670
484.024836	38.345124	73.347674
483.647609	40.538906	73.352679
483.008193	27.383222	73.357684
481.718107	29.519012	73.362689
481.129118	36.472713	73.367694
480.921282	26.369098	73.372698
480.508905	26.778617	73.377703
479.378466	28.926820	73.382708
478.073561	32.534709	73.387713
478.052770	21.108181	73.392718
477.359503	28.346578	73.397722
477.007006	32.069235	73.402727
476.466380	27.014485	73.407732
475.515532	34.222961	73.412737
475.232460	29.877814	73.417742
474.179611	37.006348	73.422746
473.166269	28.822508	73.427751
472.874055	30.914435	73.432756
471.991102	35.494325	73.437761
471.900621	23.888085	73.442766
471.024438	27.498634	73.447770
470.102351	38.815270	73.452775
469.723099	30.527250	73.457780
469.114982	23.862131	73.462785
468.455681	24.238453	73.467790
467.397088	29.015062	73.472794
466.642717	31.190086	73.477799
466.429198	26.020143	73.482804
465.683837	22.590757	73.487809
465.122714	32.580417	73.492814
464.343160	24.685769	73.497818
463.795336	26.902002	73.502823
462.705105	28.334169	73.507828
461.880236	29.741403	73.512833
461.671109	25.969534	73.517838
461.104004	32.676897	73.522842
460.096431	31.982755	73.527847
459.391132	24.807992	73.532852
458.652854	32.353190	73.537857
458.383558	35.020216	73.542862
458.021118	28.524114	73.547866
457.296801	29.152075	73.552871
456.479945	25.891781	73.557876
455.862120	31.550656	73.562881
455.375225	29.945646	73.567886
454.303862	31.958289	73.572890
453.389133	38.479768	73.577895
453.324196	40.760992	73.582900
452.454107	34.082421	73.587905
451.814219	31.760612	73.592910
450.799139	36.978156	73.597914
450.179115	34.257363	73.602919
449.795780	28.531000	73.607924
449.267974	35.758812	73.612929
448.425187	26.093845	73.617934
447.617186	38.563997	73.622938
446.626811	37.318334	73.627943
446.916864	30.503800	73.632948
445.678376	34.135817	73.637953
445.242907	27.641893	73.642958
444.549630	31.434621	73.647962
443.867264	31.070295	73.652967
443.115471	27.679788	73.657972
442.089542	30.880541	73.662977
441.786885	33.434610	73.667982
441.358981	38.378824	73.672986
440.902615	36.357363	73.677991
439.863659	37.677290	73.682996
438.813405	35.718919	73.688001
438.642567	33.353916	73.693006
438.024744	31.093251	73.698010
437.156585	39.570642	73.703015
436.603551	38.097601	73.708020
435.460510	41.957269	73.713025
435.475771	29.100991	73.718030
434.770843	35.163262	73.723034
433.737335	32.626631	73.728039
433.313398	24.796757	73.733044
432.656106	30.430385	73.738049
432.035977	25.520782	73.743054
431.287622	33.099132	73.748058
430.411628	37.435072	73.753063
430.242635	38.474454	73.758068
429.068307	29.836889	73.763073
428.636731	32.983942	73.768078
427.843436	29.532244	73.773082
427.454371	28.253854	73.778087
427.032315	23.787359	73.783092
425.711479	35.594900	73.788097
425.318900	28.521706	73.793102
424.533205	35.842655	73.798106
423.979293	30.831037	73.803111
423.350812	26.269700	73.808116
422.479782	31.200944	73.813121
422.175698	28.562282	73.818126
421.643650	34.338384	73.823130
420.805667	33.115759	73.828135
420.521671	20.450680	73.833140
419.403212	27.458795	73.838145
418.184236	27.872273	73.843150
417.720657	32.569857	73.848154
416.962682	27.636491	73.853159
416.936032	32.526228	73.858164
416.384056	36.376874	73.863169
415.648804	26.084498	73.868174
414.604913	27.135560	73.873178
414.245502	26.738704	73.878183
413.826187	21.890149	73.883188
412.729523	31.818494	73.888193
412.116027	23.798057	73.893198
411.581876	22.927570	73.898202
410.600766	36.481881	73.903207
409.857333	25.031739	73.908212
409.008906	32.941435	73.913217
408.556500	35.595065	73.918222
408.401309	28.129229	73.923226
407.792410	30.484517	73.928231
406.991274	23.640439	73.933236
406.265313	30.880908	73.938241
405.809811	27.728630	73.943246
404.801655	29.155628	73.948250
403.850758	35.335950	73.953255
403.450627	29.290572	73.958260
402.881963	35.015741	73.963265
402.518782	28.013563	73.968270
401.138487	29.496710	73.973274
400.617861	23.655042	73.978279
400.393271	16.253889	73.983284
399.907275	33.370520	73.988289
399.092854	21.378181	73.993294
398.181903	27.679871	73.998298
397.538914	37.245767	74.003303
397.256570	26.482252	74.008308
396.025576	31.805184	74.013313
395.539498	27.430899	74.018318
394.991750	33.660521	74.023322
394.174790	38.543735	74.028327
393.604782	30.907458	74.033332
392.451515	29.787126	74.038337
391.970148	33.131355	74.043342
391.509621	22.829906	74.048346
391.228300	36.498211	74.053351
390.862229	20.941441	74.058356
389.387478	29.102338	74.063361
388.786818	23.431124	74.068366
388.389608	32.191445	74.073370
387.996664	35.725013	74.078375
387.239218	20.970213	74.083380
386.362238	32.172442	74.088385
386.029209	27.770616	74.093390
384.708220	33.609371	74.098394
383.946749	30.542128	74.103399
383.852093	21.032362	74.108404
383.166993	33.306315	74.113409
382.716093	28.245177	74.118414
381.712275	29.539027	74.123418
380.781387	38.409632	74.128423
380.612908	34.435749	74.133428
379.697417	32.968444	74.138433
378.933625	32.842619	74.143438
378.365789	25.721673	74.148442
377.639550	32.995309	74.153447
377.596939	30.554683	74.158452
376.292488	31.857022	74.163457
375.994281	34.687935	74.168462
375.182473	29.465115	74.173466
374.612785	42.480784	74.178471
373.776049	36.716303	74.183476
372.880175	43.917630	74.188481
372.808887	37.335720	74.193486
372.236155	39.527556	74.198490
370.740374	30.409815	74.203495
370.305651	26.241820	74.208500
369.612864	32.959765	74.213505
369.380332	35.198311	74.218510
368.280605	34.236616	74.223514
367.380828	36.281876	74.228519
367.138486	32.376537	74.233524
366.374086	43.786345	74.238529
366.202816	27.999832	74.243534
365.441091	34.127940	74.248538
364.444544	40.050621	74.253543
364.218267	29.735497	74.258548
363.332850	28.605608	74.263553
362.266772	32.358420	74.268558
361.455784	39.614030	74.273562
361.077570	29.600668	74.278567
361.051698	31.471961	74.283572
360.067919	37.875160	74.288577
359.044513	29.546324	74.293582
358.322016	33.159225	74.298586
357.961552	33.964195	74.303591
357.899002	30.842343	74.308596
356.711115	42.464725	74.313601
355.856669	35.271185	74.318606
355.760588	23.626434	74.323610
354.720700	30.431239	74.328615
353.862145	27.630217	74.333620
352.995973	45.029804	74.338625
352.832713	40.616693	74.343630
352.077223	35.558371	74.348634
350.858954	40.759448	74.353639
350.310625	30.836279	74.358644
349.760737	41.199486	74.363649
349.473817	39.376544	74.368654
349.296843	37.211225	74.373658
347.927094	37.129944	74.378663
347.297123	35.978272	74.383668
346.929753	34.314812	74.388673
346.231731	33.076214	74.393678
344.990455	32.430406	74.398682
344.459448	40.172836	74.403687
344.298101	29.170849	74.408692
343.598062	33.480348	74.413697
342.578232	34.136517	74.418702
341.896060	30.544135	74.423706
341.560090	33.235988	74.428711
341.125498	29.012785	74.433716
339.899802	40.054564	74.438721
339.085152	36.992656	74.443726
338.463009	31.458921	74.448730
338.452304	37.546188	74.453735
338.028149	31.736467	74.458740
336.596294	36.326611	74.463745
335.973143	28.631014	74.468750
335.453834	33.533035	74.473754
334.870829	42.876494	74.478759
334.565420	33.275737	74.483764
333.332712	37.728486	74.488769
332.890817	31.016414	74.493774
332.690334	31.753311	74.498778
331.256267	37.925510	74.503783
330.950371	30.928408	74.508788
330.534202	38.390760	74.513793
329.298911	27.039546	74.518798
328.423065	25.346744	74.523802
327.736213	36.368875	74.528807
327.465277	27.699348	74.533812
326.773003	35.204128	74.538817
326.807264	38.658576	74.543822
326.197079	28.068756	74.548826
325.048594	37.871352	74.553831
324.570480	27.378755	74.558836
323.368458	28.108126	74.563841
322.617703	26.010608	74.568846
322.366696	30.412547	74.573850
321.778257	30.772883	74.578855
321.145720	27.516376	74.583860
319.914723	40.065012	74.588865
319.475122	33.650623	74.593870
319.262273	37.089263	74.598874
318.582399	35.138145	74.603879
317.635956	31.155802	74.608884
316.704017	31.774318	74.613889
316.336486	38.512975	74.618894
315.884532	34.152193	74.623898
314.464276	36.349816	74.628903
313.999935	38.409270	74.633908
313.358630	42.931770	74.638913
312.989579	29.744098	74.643918
313.198021	25.063591	74.648922
312.013419	31.678587	74.653927
311.455939	28.447966	74.658932
310.412831	31.377115	74.663937
309.335795	25.796047	74.668942
308.505578	34.242189	74.673946
307.923531	31.805545	74.678951
307.775426	31.698303	74.683956
307.116918	33.911709	74.688961
306.686096	30.940024	74.693966
305.674119	36.180779	74.698970
304.818380	36.996891	74.703975
304.836339	31.164017	74.708980
304.022463	37.751466	74.713985
302.899624	29.365967	74.718990
302.453302	35.073230	74.723994
301.548305	33.949639	74.728999
301.550131	31.555550	74.734004
300.287524	28.634447	74.739009
299.820094	26.799285	74.744014
299.365579	27.638178	74.749018
298.793649	29.700589	74.754023
297.888577	32.434274	74.759028
297.154249	37.167147	74.764033
296.656152	37.334892	74.769038
296.059285	27.777451	74.774042
294.707051	34.712491	74.779047
294.461891	33.422224	74.784052
293.708607	38.487706	74.789057
293.230419	35.690732	74.794062
292.699076	29.421864	74.799066
291.654296	33.866753	74.804071
291.316402	31.012724	74.809076
290.845322	43.402396	74.814081
290.368684	37.036495	74.819086
289.378166	29.713288	74.824090
288.602612	33.973336	74.829095
288.313044	30.799365	74.834100
287.132139	35.229683	74.839105
286.628078	38.312617	74.844110
286.235018	33.819450	74.849114
285.168623	32.792556	74.854119
284.491293	31.569602	74.859124
283.805978	28.860841	74.864129
283.502713	36.573283	74.869134
282.762174	31.067900	74.874138
281.450557	33.489499	74.879143
281.345288	24.115481	74.884148
280.534521	27.441270	74.889153
280.269771	28.693045	74.894158
279.524191	27.146655	74.899162
278.331519	33.463328	74.904167
277.908379	25.168162	74.909172
277.650530	24.619518	74.914177
276.766931	22.208875	74.919182
275.749494	23.705213	74.924186
274.993798	35.053718	74.929191
274.820680	29.664471	74.934196
274.586123	30.892510	74.939201
273.484322	28.062484	74.944206
272.786632	19.481501	74.949210
272.032726	33.084782	74.954215
271.653525	26.186113	74.959220
270.385587	33.000493	74.964225
269.687064	28.177552	74.969230
269.134281	19.947213	74.974234
268.761531	40.344813	74.979239
268.613783	32.351101	74.984244
267.695155	36.165604	74.989249
266.984547	31.145892	74.994254
266.538559	21.701610	74.999258
264.982909	34.659985	75.004263
264.461834	29.059699	75.009268
263.676076	31.701835	75.014273
263.432963	31.100381	75.019278
263.271158	28.357060	75.024282
262.515998	29.116151	75.029287
261.724639	29.144569	75.034292
261.158779	27.189487	75.039297
260.236020	29.929158	75.044302
259.430770	20.144754	75.049306
258.358501	29.574094	75.054311
258.197038	27.556124	75.059316
257.610935	34.063119	75.064321
256.926388	31.631790	75.069326
256.122156	28.981418	75.074330
255.309270	32.041047	75.079335
254.806184	22.709950	75.084340
254.499888	27.701028	75.089345
253.882766	31.825441	75.094350
253.092446	26.651284	75.099354
252.331468	27.665197	75.104359
251.856178	23.169380	75.109364
250.902869	36.474869	75.114369
249.858459	32.200664	75.119374
249.644559	25.662007	75.124378
249.206327	40.372467	75.129383
248.200730	30.418148	75.134388
247.371173	40.283473	75.139393
246.855889	24.777341	75.144398
246.629907	22.966779	75.149402
245.711878	23.628835	75.154407
245.028510	26.913825	75.159412
244.404172	33.392224	75.164417
243.999870	30.064661	75.169422
243.129502	21.525409	75.174426
242.279619	25.182300	75.179431
241.889510	26.294789	75.184436
241.212218	35.222775	75.189441
240.283512	26.181884	75.194446
239.767689	23.886092	75.199450
238.804386	30.230869	75.204455
238.675377	24.769941	75.209460
237.420115	20.256545	75.214465
236.279749	25.683370	75.219470
236.204499	19.045342	75.224474
235.638847	29.288063	75.229479
235.547521	17.369764	75.234484
234.805503	23.149402	75.239489
233.660011	24.027499	75.244494
233.338265	20.390310	75.249498
232.460428	19.568348	75.254503
232.062493	25.171706	75.259508
230.974421	27.997666	75.264513
230.437360	22.120818	75.269518
230.335506	13.810721	75.274522
228.995888	18.676373	75.279527
228.262026	26.973127	75.284532
227.425349	32.990214	75.289537
227.694063	27.555766	75.294542
226.678904	19.985785	75.299546
225.564860	26.417676	75.304551
225.175430	21.633785	75.309556
224.608699	19.997400	75.314561
223.647918	17.745741	75.319566
223.318585	20.701477	75.324570
222.390754	21.637920	75.329575
221.763653	15.171455	75.334580
221.427163	24.038796	75.339585
220.728392	26.151408	75.344590
220.043805	24.065453	75.349594
218.994277	29.143488	75.354599
219.029052	20.045200	75.359604
217.380393	25.340179	75.364609
216.866287	25.513645	75.369614
216.643212	20.610194	75.374618
216.026963	32.316525	75.379623
215.680173	24.707799	75.384628
214.864277	28.990067	75.389633
214.079773	21.525245	75.394638
213.463624	17.045589	75.399642
212.224897	21.171338	75.404647
211.647728	23.084791	75.409652
210.593069	24.922982	75.414657
210.467699	27.573387	75.419662
210.355131	25.642244	75.424666
209.717709	33.665008	75.429671
208.805474	24.694048	75.434676
208.188186	31.854155	75.439681
207.072043	25.645433	75.444686
206.917689	26.532682	75.449690
205.563109	29.724420	75.454695
205.054331	23.128705	75.459700
204.787845	28.469834	75.464705
204.047101	28.870250	75.469710
203.839432	25.350496	75.474714
202.758130	30.608646	75.479719
202.460303	18.007332	75.484724
201.564863	23.171192	75.489729
200.367964	28.286921	75.494734
199.798844	24.255512	75.499738
199.253176	31.609207	75.504743
198.952512	23.316613	75.509748
198.041586	28.522368	75.514753
197.361287	34.929274	75.519758
196.743261	28.472403	75.524762
196.389916	29.637385	75.529767
195.923042	22.566632	75.534772
194.729633	32.346472	75.539777
193.934315	20.456841	75.544782
193.839975	30.435187	75.549786
192.755583	30.620736	75.554791
191.819034	14.219853	75.559796
191.364027	33.637066	75.564801
190.612430	33.309081	75.569806
190.846334	23.718571	75.574810
189.603627	29.251620	75.579815
188.774749	27.516689	75.584820
188.268985	25.093148	75.589825
187.365691	26.251197	75.594830
186.565697	25.214988	75.599834
185.397846	27.258897	75.604839
185.323714	22.675480	75.609844
184.841060	27.227901	75.614849
184.863502	28.164233	75.619854
184.273783	28.283530	75.624858
183.254680	18.544297	75.629863
182.346450	19.826138	75.634868
181.140793	31.063473	75.639873
180.384441	30.619554	75.644878
180.293897	16.343577	75.649882
179.426907	24.298864	75.654887
179.302656	16.654669	75.659892
178.558878	16.926265	75.664897
177.508047	19.528686	75.669902
176.985591	33.817328	75.674906
176.465905	31.569474	75.679911
175.809551	21.609976	75.684916
175.136534	28.261728	75.689921
174.265400	25.264084	75.694926
173.827511	20.066882	75.699930
172.631394	30.542602	75.704935
171.956136	28.269091	75.709940
171.393909	27.554524	75.714945
170.983291	31.660220	75.719950
170.804500	33.838171	75.724954
170.206002	32.539602	75.729959
169.121002	30.232077	75.734964
168.634742	26.756747	75.739969
167.321215	34.983518	75.744974
167.018268	22.854539	75.749978
166.214301	29.257512	75.754983
165.981648	27.886419	75.759988
165.409029	25.673816	75.764993
164.225535	31.946495	75.769998
163.607022	22.755257	75.775002
162.881305	32.821660	75.780007
162.729771	27.044208	75.785012
161.337546	24.998564	75.790017
160.697389	30.107540	75.795022
160.370916	20.322532	75.800026
159.844150	25.195806	75.805031
159.565739	19.115310	75.810036
158.744911	30.149363	75.815041
157.742044	24.493468	75.820046
157.418410	22.759988	75.825050
156.634458	27.309993	75.830055
155.940590	21.265781	75.835060
155.014408	26.574907	75.840065
154.336417	24.875854	75.845070
154.384547	25.142610	75.850074
153.306401	24.984980	75.855079
152.429595	25.858118	75.860084
151.820946	25.253461	75.865089
151.108904	28.271808	75.870094
150.439979	16.568628	75.875098
149.250086	31.501441	75.880103
149.158073	29.358864	75.885108
148.916337	25.751508	75.890113
148.170485	23.247987	75.895118
147.655395	24.079219	75.900122
146.443004	28.708584	75.905127
146.130103	25.563588	75.910132
145.294841	32.673308	75.915137
144.515876	27.304992	75.920142
143.815644	22.360942	75.925146
143.310672	28.866056	75.930151
142.694599	25.998064	75.935156
141.559941	32.624089	75.940161
141.088854	38.398400	75.945166
141.128255	27.202013	75.950170
140.237297	34.828399	75.955175
139.220714	31.652109	75.960180
138.677053	28.928690	75.965185
138.061324	31.742447	75.970190
137.195470	24.811025	75.975194
136.534726	39.072840	75.980199
136.030076	27.854398	75.985204
135.455747	32.128131	75.990209
134.831720	29.026441	75.995214
133.963368	24.676910	76.000218
133.274651	33.218803	76.005223
132.952024	30.048550	76.010228
132.470688	27.950711	76.015233
131.442025	27.124451	76.020238
130.673712	23.016015	76.025242
129.793537	20.579653	76.030247
129.439721	11.617462	76.035252
128.386676	18.153201	76.040257
127.431377	28.379221	76.045262
127.652408	23.324537	76.050266
126.709750	24.275995	76.055271
126.281282	27.252282	76.060276
125.796171	27.208254	76.065281
124.848231	32.481438	76.070286
124.626796	27.795357	76.075290
122.910864	31.880554	76.080295
121.998117	28.282433	76.085300
121.503781	27.432471	76.090305
121.419431	28.516720	76.095310
121.282790	28.625283	76.100314
120.640919	31.682911	76.105319
119.930812	35.719678	76.110324
119.007581	30.762309	76.115329
118.458207	28.183310	76.120334
117.575422	29.822243	76.125338
116.473816	31.108138	76.130343
116.083862	21.431035	76.135348
115.420712	24.687600	76.140353
115.015474	24.600874	76.145358
114.042875	19.230335	76.150362
113.104625	23.519527	76.155367
112.677440	17.213605	76.160372
112.569187	19.974823	76.165377
111.799137	18.661050	76.170382
110.960311	17.919644	76.175386
109.871704	19.334356	76.180391
109.767832	12.992647	76.185396
109.500731	20.781322	76.190401
108.245278	19.615922	76.195406
107.791967	18.373066	76.200410
107.146235	27.378040	76.205415
106.224726	23.647283	76.210420
105.357327	23.069708	76.215425
104.430915	26.786155	76.220430
104.679517	25.549633	76.225434
104.077813	25.853788	76.230439
103.007717	25.213922	76.235444
102.287450	18.877471	76.240449
101.992946	22.559376	76.245454
101.273842	20.636659	76.250458
100.010162	17.249058	76.255463
99.146446	21.021739	76.260468
98.946237	15.083327	76.265473
98.686718	16.350053	76.270478
97.922925	10.611909	76.275482
96.796261	19.267798	76.280487
96.522554	23.533017	76.285492
95.991017	32.310048	76.290497
94.905382	34.339310	76.295502
93.788387	23.447202	76.300506
93.343604	31.562265	76.305511
93.013478	30.031681	76.310516
92.910118	27.870418	76.315521
92.166509	38.479012	76.320526
91.439056	23.380519	76.325530
90.789351	29.888222	76.330535
89.743402	23.662060	76.335540
89.035598	26.924176	76.340545
88.150327	35.088991	76.345550
88.153525	21.982377	76.350554
87.062364	23.843787	76.355559
86.434696	24.133164	76.360564
85.804798	29.038668	76.365569
84.890499	31.874822	76.370574
84.738312	23.522303	76.375578
83.736708	32.826892	76.380583
82.980318	24.635389	76.385588
82.747946	19.358123	76.390593
82.094091	30.982157	76.395598
81.157170	20.025069	76.400602
80.018532	29.766254	76.405607
79.935358	18.004376	76.410612
79.594687	17.699200	76.415617
78.262435	37.106510	76.420622
77.556716	29.898835	76.425626
77.249888	22.731626	76.430631
76.844802	16.420613	76.435636
76.362265	22.616224	76.440641
74.947014	28.443349	76.445646
74.676689	26.419103	76.450650
74.181575	30.711752	76.455655
73.414206	25.669623	76.460660
72.296612	34.459702	76.465665
71.625951	34.621897	76.470670
71.160097	27.901099	76.475674
71.020622	26.213955	76.480679
69.990297	24.919629	76.485684
68.987401	26.479962	76.490689
68.489819	23.443282	76.495694
68.059348	21.100802	76.500698
67.472037	26.980387	76.505703
66.641339	21.744934	76.510708
66.075352	23.694481	76.515713
65.269859	30.851513	76.520718
64.815648	22.558207	76.525722
64.179405	22.429485	76.530727
63.378341	22.893180	76.535732
63.142988	30.817147	76.540737
62.139183	27.665663	76.545742
61.683917	16.054600	76.550746
60.608203	26.903819	76.555751
60.209083	23.964978	76.560756
59.217691	24.239833	76.565761
58.409881	30.036317	76.570766
58.235184	16.369878	76.575770
57.417540	29.674270	76.580775
56.836759	25.731493	76.585780
55.827092	21.667886	76.590785
55.394775	19.716790	76.595790
55.092390	18.227520	76.600794
54.186612	25.736440	76.605799
53.049412	18.843605	76.610804
52.770987	20.524939	76.615809
52.261849	28.923083	76.620814
52.043826	24.184430	76.625818
50.713124	31.786360	76.630823
49.602479	24.167040	76.635828
49.660391	25.588147	76.640833
49.102479	21.577070	76.645838
48.224147	23.325703	76.650842
47.238880	25.553442	76.655847
46.945779	27.290734	76.660852
46.443649	22.638398	76.665857
45.264198	26.833620	76.670862
45.008741	25.802070	76.675866
44.331259	30.339855	76.680871
43.667343	24.193132	76.685876
42.714316	23.250768	76.690881
41.807828	28.261898	76.695886
41.555002	22.021222	76.700890
40.904838	24.654410	76.705895
40.268912	32.850430	76.710900
39.391030	27.838555	76.715905
38.633628	31.428719	76.720910
38.268157	30.630761	76.725914
37.515838	32.693615	76.730919
37.178504	27.494597	76.735924
36.444475	33.916413	76.740929
35.450542	34.608001	76.745934
35.246277	26.330027	76.750938
34.539657	31.930605	76.755943
33.503126	23.200330	76.760948
32.863214	26.390129	76.765953
32.244082	27.693722	76.770958
31.954197	23.374968	76.775962
30.482639	23.977160	76.780967
30.010503	29.459911	76.785972
29.604033	32.864792	76.790977
29.249227	31.973670	76.795982
28.805443	21.633390	76.800986
27.560115	29.699531	76.805991
27.064249	34.161043	76.810996
27.106463	28.526169	76.816001
25.463013	31.950160	76.821006
25.127728	18.761930	76.826010
24.366069	28.922399	76.831015
23.929964	30.398650	76.836020
23.168775	23.829055	76.841025
22.178683	26.248386	76.846030
21.586677	18.584204	76.851034
21.342940	29.456849	76.856039
20.693660	22.268582	76.861044
19.460628	21.681552	76.866049
19.020527	30.469237	76.871054
18.901386	27.648171	76.876058
17.722169	33.087593	76.881063
16.931691	20.397751	76.886068
16.349430	25.130088	76.891073
15.798368	30.677471	76.896078
15.364815	17.233682	76.901082
14.165922	29.107090	76.906087
13.161197	25.441686	76.911092
13.206372	27.642265	76.916097
12.636395	29.813236	76.921102
12.250068	23.735787	76.926106
10.992183	26.402843	76.931111
10.415249	29.265633	76.936116
10.096657	19.200283	76.941121
9.223020	30.249100	76.946126
8.506336	27.881322	76.951130
7.714694	28.135374	76.956135
7.381667	20.224880	76.961140
7.005148	19.036026	76.966145
5.600944	22.794027	76.971150
4.929404	19.860806	76.976154
4.622981	23.431079	76.981159
3.887605	18.601496	76.986164
3.407160	20.788148	76.991169
2.364722	30.004656	76.996174