Fri Mar 05 18:58:05 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.701030	104.861738	0.000000
0.370409	89.345073	0.005005
-0.197533	52.458977	0.010010
-1.863365	4.862352	0.015014
-6.554330	-10.647799	0.020019
-12.007242	-11.722347	0.025024
-17.164063	-3.757689	0.030029
-21.384957	-0.957043	0.035034
-25.296612	1.892051	0.040038
-29.098866	4.319998	0.045043
-32.460618	-4.804151	0.050048
-36.195223	5.127219	0.055053
-40.040315	-4.716176	0.060058
-43.615233	-4.715141	0.065062
-47.479522	0.064512	0.070067
-51.316923	-4.918331	0.075072
-54.814542	5.350575	0.080077
-58.875826	-0.209977	0.085082
-62.101016	-1.926822	0.090086
-66.275557	4.260118	0.095091
-69.960011	1.244601	0.100096
-73.859564	-7.159746	0.105101
-77.708833	-2.868147	0.110106
-81.367799	-5.827787	0.115110
-85.273337	2.733740	0.120115
-88.819667	-1.786124	0.125120
-92.852368	-4.733426	0.130125
-96.372138	-2.375678	0.135130
-100.039481	-2.954326	0.140134
-103.529915	3.285950	0.145139
-107.012724	-4.352202	0.150144
-111.245198	-1.879139	0.155149
-115.500689	-9.903345	0.160154
-119.068299	-8.058327	0.165158
-123.159453	-3.578251	0.170163
-126.957358	-13.370674	0.175168
-131.027733	-3.057590	0.180173
-134.465410	-1.627521	0.185178
-137.702466	-4.761631	0.190182
-141.700082	-10.595544	0.195187
-145.313301	-5.084674	0.200192
-149.348707	3.584406	0.205197
-152.756195	-1.834304	0.210202
-156.221652	-4.257004	0.215206
-160.272668	-5.912896	0.220211
-163.800104	-1.554249	0.225216
-168.179754	5.015676	0.230221
-171.998617	-4.317594	0.235226
-175.775430	-3.322202	0.240230
-179.163341	-4.132980	0.245235
-182.566624	-8.609296	0.250240
-186.795739	-3.892633	0.255245
-190.615886	-1.849512	0.260250
-194.157103	-1.243352	0.265254
-198.190164	1.193306	0.270259
-201.907809	3.529169	0.275264
-205.486265	4.390449	0.280269
-209.294085	-0.350852	0.285274
-212.841270	-2.255800	0.290278
-216.668930	-1.233306	0.295283
-220.464491	-4.369626	0.300288
-224.440465	0.166351	0.305293
-228.248534	-3.373238	0.310298
-231.558280	-3.671292	0.315302
-235.914059	8.264471	0.320307
-239.379428	-0.845987	0.325312
-243.193856	-0.252917	0.330317
-247.294018	-2.179939	0.335322
-250.670867	1.471975	0.340326
-254.513554	1.077669	0.345331
-257.978431	-3.119048	0.350336
-261.548726	3.667204	0.355341
-265.761622	-0.074212	0.360346
-269.235296	-2.798210	0.365350
-273.621367	-3.376984	0.370355
-277.026059	-4.501913	0.375360
-280.841385	-3.366169	0.380365
-284.206814	-3.418718	0.385370
-288.356230	-5.063416	0.390374
-292.423424	-0.695695	0.395379
-295.988957	-4.639743	0.400384
-299.803700	3.822462	0.405389
-303.478243	-1.938171	0.410394
-306.837396	-2.016922	0.415398
-310.838123	-4.018055	0.420403
-314.141409	-1.134735	0.425408
-318.308583	3.411417	0.430413
-322.167612	1.237871	0.435418
-326.157822	1.223622	0.440422
-330.061958	5.022903	0.445427
-333.426423	0.488569	0.450432
-337.194155	5.762612	0.455437
-341.059210	0.029300	0.460442
-344.632462	-6.214214	0.465446
-348.703635	0.658434	0.470451
-352.047564	-4.759089	0.475456
-355.939893	-1.704398	0.480461
-359.582134	3.749916	0.485466
-363.407961	-5.099369	0.490470
-367.513940	-4.855368	0.495475
-370.980903	-5.085549	0.500480
-375.137909	-0.932010	0.505485
-379.045139	1.144234	0.510490
-382.159997	-8.438279	0.515494
-385.800652	-3.059876	0.520499
-389.429168	-3.630088	0.525504
-393.414601	-4.111765	0.530509
-397.859250	-1.872408	0.535514
-401.160993	-2.942634	0.540518
-405.091486	-5.008437	0.545523
-409.021904	-8.239612	0.550528
-412.351674	-3.290858	0.555533
-416.293243	-1.587539	0.560538
-419.650530	-3.826852	0.565542
-423.828840	-3.162774	0.570547
-427.430139	-10.202770	0.575552
-431.517250	-6.028759	0.580557
-435.134632	-1.898213	0.585562
-438.894219	-3.332088	0.590566
-442.751914	-0.945108	0.595571
-445.907478	-9.224776	0.600576
-450.091013	0.619608	0.605581
-453.895823	2.007835	0.610586
-457.678090	-7.250368	0.615590
-461.533562	-2.480942	0.620595
-464.940928	-13.087370	0.625600
-468.936161	-0.164861	0.630605
-472.688715	-4.646472	0.635610
-476.173964	-9.822047	0.640614
-480.385968	-5.746279	0.645619
-483.907281	-7.560334	0.650624
-487.708033	1.447118	0.655629
-491.453871	-2.568759	0.660634
-494.994897	-12.139814	0.665638
-499.440658	5.587125	0.670643
-502.683358	-3.698836	0.675648
-506.603193	-11.167221	0.680653
-510.324528	-13.419218	0.685658
-514.162645	-9.269071	0.690662
-517.732782	-3.272536	0.695667
-521.137047	-2.851772	0.700672
-525.226117	0.113190	0.705677
-529.090433	-2.040248	0.710682
-532.729336	-0.520701	0.715686
-536.928772	-2.912332	0.720691
-540.778377	-14.553440	0.725696
-544.271383	-10.141407	0.730701
-547.666821	-6.087150	0.735706
-551.344042	-10.795130	0.740710
-555.541858	-0.002122	0.745715
-559.376550	-3.945348	0.750720
-563.074983	-3.021794	0.755725
-566.873234	-5.373380	0.760730
-570.097945	-2.552729	0.765734
-574.470557	-0.967950	0.770739
-577.633246	-5.912627	0.775744
-581.658117	-6.712538	0.780749
-585.581314	-5.497578	0.785754
-589.456531	-8.068641	0.790758
-593.512151	-1.002538	0.795763
-596.967862	-3.098139	0.800768
-600.388399	-0.668785	0.805773
-604.327912	4.030714	0.810778
-607.685912	-4.552276	0.815782
-611.891300	0.817337	0.820787
-615.715566	-5.369880	0.825792
-619.235300	-2.826880	0.830797
-622.943919	-10.896510	0.835802
-626.754719	-5.091602	0.840806
-630.945718	-8.321769	0.845811
-634.578282	-12.107929	0.850816
-638.033716	-6.839174	0.855821
-641.917311	-1.714890	0.860826
-645.684679	-10.576185	0.865830
-649.575978	1.658217	0.870835
-653.154409	0.060121	0.875840
-657.077055	1.245149	0.880845
-660.997654	-6.624970	0.885850
-664.234542	-5.136345	0.890854
-668.409409	-0.315559	0.895859
-672.116739	-10.667155	0.900864
-675.910851	1.469755	0.905869
-679.742187	-0.966247	0.910874
-683.097824	-4.045957	0.915878
-687.008466	-9.869167	0.920883
-690.767232	-0.347728	0.925888
-694.678984	-0.460629	0.930893
-698.498984	-2.064206	0.935898
-701.972546	-9.679262	0.940902
-706.134388	4.217983	0.945907
-709.622570	0.670639	0.950912
-713.736210	1.988784	0.955917
-717.173038	4.318406	0.960922
-720.564741	-8.860552	0.965926
-724.853371	-1.809035	0.970931
-728.481458	-1.046277	0.975936
-732.163585	-5.295870	0.980941
-735.754320	-0.743364	0.985946
-739.525580	-6.937265	0.990950
-743.696035	3.443253	0.995955
-747.003814	-0.995456	1.000960
-751.022991	-4.940416	1.005965
-755.016217	-3.885871	1.010970
-758.672283	-8.481783	1.015974
-762.501668	-0.365047	1.020979
-765.987546	-0.203699	1.025984
-769.871568	0.325640	1.030989
-773.781255	-2.979195	1.035994
-777.060330	-1.945719	1.040998
-781.251197	1.971076	1.046003
-784.788882	-3.167263	1.051008
-788.799123	-2.942569	1.056013
-792.632096	3.380227	1.061018
-796.265679	-4.261146	1.066022
-799.712163	7.437188	1.071027
-803.444274	-1.334865	1.076032
-807.265252	-1.499935	1.081037
-811.411977	4.404691	1.086042
-814.746607	-8.185579	1.091046
-818.901541	-5.406710	1.096051
-822.558543	-5.847124	1.101056
-826.201709	-9.943521	1.106061
-829.891639	3.066358	1.111066
-833.751295	-5.915485	1.116070
-837.775402	-4.431666	1.121075
-841.089040	-3.695350	1.126080
-845.015749	-2.444708	1.131085
-848.950623	1.559013	1.136090
-852.518465	-7.746990	1.141094
-856.467461	-6.495919	1.146099
-860.110355	-9.553101	1.151104
-863.719844	0.618085	1.156109
-867.887413	5.332393	1.161114
-871.168900	-1.059441	1.166118
-875.260544	5.323763	1.171123
-878.759456	-5.674240	1.176128
-882.924461	-7.782170	1.181133
-886.685978	-7.533996	1.186138
-890.080791	-10.477830	1.191142
-893.684032	6.190980	1.196147
-897.580731	-4.990973	1.201152
-901.140776	-8.151222	1.206157
-905.583331	1.203903	1.211162
-908.985632	-10.452888	1.216166
-912.780209	-4.259048	1.221171
-916.565586	-3.267426	1.226176
-920.314999	-0.283564	1.231181
-923.981631	-0.140389	1.236186
-927.544872	-3.471973	1.241190
-931.418312	5.522542	1.246195
-935.372523	-8.592719	1.251200
-939.173009	-13.078513	1.256205
-943.233887	-3.527315	1.261210
-946.599278	-12.069179	1.266214
-950.340089	-6.104651	1.271219
-953.851122	-7.877063	1.276224
-957.633941	-2.810969	1.281229
-961.771939	3.311711	1.286234
-965.797465	-12.697030	1.291238
-969.310585	-2.101141	1.296243
-972.905129	-11.167711	1.301248
-976.463400	-5.289104	1.306253
-980.432229	-4.938242	1.311258
-984.190997	-5.761095	1.316262
-988.311585	-2.697266	1.321267
-991.883174	-7.806203	1.326272
-995.678094	-7.177201	1.331277
-999.148036	-6.932901	1.336282
-1002.908543	-10.406281	1.341286
-1006.685761	-5.519201	1.346291
-1010.528385	-0.457652	1.351296
-1014.426781	-2.469215	1.356301
-1018.271822	1.712801	1.361306
-1021.761336	-7.829379	1.366310
-1025.957341	-3.651142	1.371315
-1029.511647	-8.892092	1.376320
-1033.225911	-6.467180	1.381325
-1036.782925	-4.852730	1.386330
-1040.638337	-12.071868	1.391334
-1044.411164	-9.708534	1.396339
-1048.279328	-9.487198	1.401344
-1051.985708	-7.175481	1.406349
-1055.597803	0.416523	1.411354
-1059.294414	-9.306933	1.416358
-1063.176036	-3.911060	1.421363
-1066.906449	-20.783659	1.426368
-1071.006902	-3.845854	1.431373
-1074.643915	-2.928173	1.436378
-1078.222827	-7.963262	1.441382
-1082.447749	1.261174	1.446387
-1085.665256	-4.501916	1.451392
-1088.980314	-11.496752	1.456397
-1093.170735	-2.662593	1.461402
-1096.803480	0.080536	1.466406
-1101.126510	1.178964	1.471411
-1104.807102	-2.701268	1.476416
-1108.393036	-8.039535	1.481421
-1112.089653	-11.768957	1.486426
-1115.742512	-11.960418	1.491430
-1119.766257	4.796470	1.496435
-1123.516232	5.407450	1.501440
-1126.977504	-1.010437	1.506445
-1131.118373	-3.033472	1.511450
-1134.525349	-10.740502	1.516454
-1138.466008	-4.094013	1.521459
-1142.463298	-11.671894	1.526464
-1145.687808	-5.750246	1.531469
-1149.830721	4.798429	1.536474
-1153.091064	-6.804996	1.541478
-1157.158612	-12.323167	1.546483
-1160.886493	-12.972480	1.551488
-1164.863492	-9.904513	1.556493
-1169.059678	0.441406	1.561498
-1172.389019	-3.617919	1.566502
-1176.132298	-3.474699	1.571507
-1179.503401	-8.730532	1.576512
-1183.185377	-7.081674	1.581517
-1187.266183	-8.158594	1.586522
-1191.281259	-4.788024	1.591526
-1195.227699	-0.162149	1.596531
-1198.609141	1.243104	1.601536
-1202.449609	-1.658917	1.606541
-1206.171292	0.083063	1.611546
-1209.628141	-9.628042	1.616550
-1213.925322	-6.475640	1.621555
-1217.828736	-2.463734	1.626560
-1221.574965	-0.711494	1.631565
-1225.361463	4.822384	1.636570
-1228.536862	-6.753518	1.641574
-1232.552867	-0.000201	1.646579
-1236.136312	-1.211820	1.651584
-1239.895005	-9.064250	1.656589
-1243.780956	-0.996063	1.661594
-1247.363978	-4.809677	1.666598
-1251.330420	-3.872115	1.671603
-1255.042933	-10.191242	1.676608
-1258.556554	-6.345730	1.681613
-1262.601549	-1.847473	1.686618
-1266.356596	-4.266322	1.691622
-1270.053196	-5.948627	1.696627
-1273.802004	-4.057121	1.701632
-1277.464543	-8.185961	1.706637
-1281.383280	-6.076437	1.711642
-1285.050559	-13.676915	1.716646
-1288.899710	-4.340386	1.721651
-1292.613627	-3.201901	1.726656
-1296.362196	-10.425079	1.731661
-1300.238460	-8.312859	1.736666
-1303.598080	-13.762726	1.741670
-1307.941727	-3.735167	1.746675
-1311.758609	-6.844202	1.751680
-1315.175641	-2.950989	1.756685
-1319.068971	-7.058589	1.761690
-1322.409636	-8.741014	1.766694
-1326.607284	-6.607269	1.771699
-1330.108526	-8.749674	1.776704
-1334.171159	0.307292	1.781709
-1338.186019	4.289928	1.786714
-1341.680814	-9.573268	1.791718
-1345.128845	-2.633144	1.796723
-1348.809008	-9.871914	1.801728
-1352.352342	-4.649575	1.806733
-1356.897851	-1.007733	1.811738
-1360.487422	-4.686078	1.816742
-1364.321959	-0.599802	1.821747
-1367.938324	-3.619419	1.826752
-1371.331233	-9.577936	1.831757
-1375.568023	-0.570292	1.836762
-1379.019714	-6.202424	1.841766
-1382.735467	1.728352	1.846771
-1386.887538	0.049768	1.851776
-1390.235907	4.220677	1.856781
-1394.233769	2.224108	1.861786
-1397.941818	-5.718161	1.866790
-1401.653287	-3.433463	1.871795
-1405.656393	-0.594294	1.876800
-1409.591067	-0.027397	1.881805
-1413.059114	1.024607	1.886810
-1416.537949	-7.044213	1.891814
-1420.795945	1.028632	1.896819
-1424.398674	-4.344285	1.901824
-1427.885504	7.493819	1.906829
-1431.868915	7.360514	1.911834
-1435.579692	-8.180494	1.916838
-1439.631957	6.156136	1.921843
-1443.309352	-3.531899	1.926848
-1446.622874	-7.216461	1.931853
-1450.582265	5.919463	1.936858
-1454.049661	-4.496030	1.941862
-1457.572332	-0.502118	1.946867
-1461.707979	1.052670	1.951872
-1465.903589	-1.415149	1.956877
-1469.807576	-4.263967	1.961882
-1473.211182	-8.135910	1.966886
-1477.093268	4.930906	1.971891
-1481.092154	2.571959	1.976896
-1484.699657	-7.573467	1.981901
-1488.325952	2.380540	1.986906
-1491.587130	2.841300	1.991910
-1495.742783	-6.249667	1.996915
-1499.905892	-0.202133	2.006912
-1500.760220	-3.861091	2.016909
-1497.881159	-1.127920	2.026906
-1495.340853	1.237925	2.036902
-1493.178992	3.552273	2.046899
-1491.243998	0.652941	2.056896
-1489.281452	-6.116073	2.066893
-1487.482502	-2.932023	2.076890
-1485.565159	1.519915	2.086886
-1483.642647	-6.696897	2.096883
-1481.570290	-7.590844	2.106880
-1479.954771	-3.346359	2.116877
-1477.985448	-7.913812	2.126874
-1476.093347	-6.490989	2.136870
-1474.054879	-9.550560	2.146867
-1472.344078	-7.950281	2.156864
-1470.401753	-4.383386	2.166861
-1468.638358	-4.283635	2.176858
-1466.301332	-0.596782	2.186854
-1464.681782	-3.382421	2.196851
-1462.773011	-3.722787	2.206848
-1460.955492	-1.244321	2.216845
-1459.091271	2.529303	2.226842
-1457.254392	-3.494825	2.236838
-1455.221790	0.354471	2.246835
-1453.183796	-3.916063	2.256832
-1451.674277	-4.525648	2.266829
-1449.567039	-4.979888	2.276826
-1447.740574	-6.001801	2.286822
-1445.922659	-3.794967	2.296819
-1443.988986	-4.810359	2.306816
-1442.001700	-0.339582	2.316813
-1439.940055	0.167174	2.326810
-1438.573021	-5.282759	2.336806
-1436.353232	-12.345550	2.346803
-1434.502917	-5.263358	2.356800
-1432.709099	-4.101078	2.366797
-1430.828172	-7.912231	2.376794
-1428.982478	-9.576684	2.386790
-1427.077841	-15.041632	2.396787
-1425.235061	-14.648242	2.406784
-1423.015038	-14.384725	2.416781
-1421.526633	-6.875101	2.426778
-1419.596732	-7.714605	2.436774
-1417.527636	-10.616399	2.446771
-1415.734518	-11.691369	2.456768
-1413.816536	-2.883144	2.466765
-1412.045097	-8.884128	2.476762
-1409.916958	-8.255359	2.486758
-1408.132156	-7.555829	2.496755
-1406.671463	-10.298626	2.506752
-1404.419884	-10.948040	2.516749
-1402.513076	-4.487497	2.526746
-1400.878581	-14.020766	2.536742
-1398.652077	-11.936153	2.546739
-1397.059592	-11.475825	2.556736
-1395.013492	-5.842841	2.566733
-1393.187495	-6.177792	2.576730
-1391.339078	-8.688969	2.586726
-1389.569771	-10.982215	2.596723
-1387.311281	-10.647453	2.606720
-1385.542767	-14.096362	2.616717
-1384.174050	-10.211770	2.626714
-1381.912062	-2.818067	2.636710
-1379.695745	-10.439202	2.646707
-1378.021547	-6.398247	2.656704
-1376.473214	-4.602937	2.666701
-1374.489036	-7.241625	2.676698
-1372.566473	-5.643592	2.686694
-1370.682056	-6.055773	2.696691
-1368.547673	-7.720604	2.706688
-1366.642850	-8.421838	2.716685
-1365.204413	2.517421	2.726682
-1362.888374	-3.060712	2.736678
-1361.460327	-0.745606	2.746675
-1359.722309	-6.302255	2.756672
-1357.338381	-8.311762	2.766669
-1355.579907	-6.906921	2.776666
-1353.559165	-9.475655	2.786662
-1351.952904	-8.258024	2.796659
-1350.040885	-14.595678	2.806656
-1348.322688	-5.766465	2.816653
-1346.430294	-6.721484	2.826650
-1344.194359	-5.250960	2.836646
-1342.559049	-1.440594	2.846643
-1340.285877	-2.529194	2.856640
-1338.669985	-7.095221	2.866637
-1337.126722	-2.995379	2.876634
-1335.151774	-7.817829	2.886630
-1333.050327	-2.657857	2.896627
-1331.100289	-7.518947	2.906624
-1329.306657	-6.290240	2.916621
-1327.363062	-4.968694	2.926618
-1325.518031	-9.443496	2.936614
-1323.735715	-16.609844	2.946611
-1322.037234	-6.691135	2.956608
-1319.782623	-7.202004	2.966605
-1318.299342	-5.963085	2.976602
-1316.241005	-10.822551	2.986598
-1314.100649	-9.147224	2.996595
-1312.387994	-10.730289	3.006592
-1310.774749	-11.969020	3.016589
-1308.884447	-8.902079	3.026586
-1306.654516	-5.884762	3.036582
-1304.635677	-1.939965	3.046579
-1303.072957	-8.359046	3.056576
-1301.263179	-8.992909	3.066573
-1299.477776	-6.875489	3.076570
-1297.390565	-6.134275	3.086566
-1295.345867	-10.590486	3.096563
-1293.566532	-8.931566	3.106560
-1291.761070	-10.153680	3.116557
-1290.026998	-10.728049	3.126554
-1288.136964	-5.564197	3.136550
-1286.022335	-9.412643	3.146547
-1284.034162	-12.287158	3.156544
-1282.536624	-10.013126	3.166541
-1280.871196	-5.399111	3.176538
-1278.542200	-2.602884	3.186534
-1276.462530	-13.137333	3.196531
-1275.003844	-4.422840	3.206528
-1273.242641	-10.308403	3.216525
-1271.333623	-6.633370	3.226522
-1269.214454	-8.379361	3.236518
-1267.267573	-8.191979	3.246515
-1265.476139	-3.484433	3.256512
-1263.767771	-7.356262	3.266509
-1261.735918	-0.088230	3.276506
-1259.915459	-1.341142	3.286502
-1258.170487	-6.766201	3.296499
-1256.244925	-11.921736	3.306496
-1254.119680	-5.374439	3.316493
-1252.152546	-3.734489	3.326490
-1250.323315	-4.620900	3.336486
-1248.630373	-11.709737	3.346483
-1246.916456	-10.196628	3.356480
-1244.647717	-10.524948	3.366477
-1242.860731	-10.820380	3.376474
-1241.052743	-7.440207	3.386470
-1239.248318	-10.848967	3.396467
-1237.661384	-14.830817	3.406464
-1235.556869	-5.749120	3.416461
-1233.507530	-8.393383	3.426458
-1231.827083	-7.215960	3.436454
-1229.971940	-10.233354	3.446451
-1228.063583	-7.016075	3.456448
-1226.115174	-10.632604	3.466445
-1223.825068	-1.195328	3.476442
-1222.473698	-1.389455	3.486438
-1220.548869	-7.059586	3.496435
-1218.696015	-6.359745	3.506432
-1216.687216	-5.869596	3.516429
-1214.757695	-5.063598	3.526426
-1213.055120	-6.463400	3.536422
-1211.249643	-7.194400	3.546419
-1209.301323	-5.395085	3.556416
-1207.437172	-6.887054	3.566413
-1205.414689	-4.843813	3.576410
-1203.459664	-6.951902	3.586406
-1201.497708	-6.062662	3.596403
-1199.817142	-3.200489	3.606400
-1197.967373	-7.153320	3.616397
-1196.250448	-3.044850	3.626394
-1194.107774	-12.818786	3.636390
-1192.230755	-9.007513	3.646387
-1190.333857	-3.468881	3.656384
-1188.717694	-9.223809	3.666381
-1186.981385	-3.714742	3.676378
-1184.865968	-6.205324	3.686374
-1182.794466	-4.493592	3.696371
-1181.080572	-1.598842	3.706368
-1179.216535	-3.513931	3.716365
-1177.379800	-3.169901	3.726362
-1175.449830	-7.032915	3.736358
-1173.499452	-11.189721	3.746355
-1171.448419	-2.652035	3.756352
-1169.666106	-6.540367	3.766349
-1167.973079	-6.017018	3.776346
-1165.869653	-3.318794	3.786342
-1164.156381	-8.923453	3.796339
-1162.330617	-2.637622	3.806336
-1160.535123	-10.399657	3.816333
-1158.681024	-5.367311	3.826330
-1156.526091	-5.843127	3.836326
-1154.845933	-3.909281	3.846323
-1153.073323	-6.204460	3.856320
-1151.086232	-9.182905	3.866317
-1148.958771	-0.876899	3.876314
-1147.365025	-1.239235	3.886310
-1145.355302	-5.336040	3.896307
-1143.488284	-9.752644	3.906304
-1141.684531	-11.272793	3.916301
-1139.644598	-4.716470	3.926298
-1137.987918	-12.149962	3.936294
-1136.251378	-1.045068	3.946291
-1134.234706	5.398143	3.956288
-1132.159101	-1.529211	3.966285
-1130.414047	-1.980481	3.976282
-1128.690845	-1.105086	3.986278
-1126.500159	-8.477163	3.996275
-1124.610944	-5.722525	4.006272
-1122.957735	-1.482223	4.016269
-1121.195772	2.011203	4.026266
-1119.137368	-4.234436	4.036262
-1117.093374	-10.627766	4.046259
-1115.392304	-4.097735	4.056256
-1113.629493	-9.073965	4.066253
-1111.807560	-6.900662	4.076250
-1109.848967	-3.670791	4.086246
-1107.813885	-7.351619	4.096243
-1105.848046	-8.886618	4.106240
-1104.216265	-7.308155	4.116237
-1102.331574	-6.990685	4.126234
-1100.394908	-3.367295	4.136230
-1098.535029	-8.213780	4.146227
-1096.168771	-5.396483	4.156224
-1094.496040	-6.917742	4.166221
-1093.080305	-3.398908	4.176218
-1090.929960	-12.381351	4.186214
-1088.930350	-8.379599	4.196211
-1087.322965	-8.684076	4.206208
-1085.631018	-3.643097	4.216205
-1083.511868	-8.019462	4.226202
-1081.687428	-8.991819	4.236198
-1079.699916	-12.150273	4.246195
-1077.639431	-9.519309	4.256192
-1076.003792	-10.791462	4.266189
-1074.191740	-11.196564	4.276186
-1072.294048	-12.766424	4.286182
-1070.291436	-14.094115	4.296179
-1068.387935	-14.581736	4.306176
-1066.600129	-14.820322	4.316173
-1064.796343	-14.744091	4.326170
-1062.835202	-13.057230	4.336166
-1060.850798	-14.735688	4.346163
-1059.322217	-12.654368	4.356160
-1057.384646	-13.087429	4.366157
-1055.249167	-15.781633	4.376154
-1053.332122	-4.612384	4.386150
-1051.607965	-17.077699	4.396147
-1049.552362	-16.160678	4.406144
-1047.822127	-10.817899	4.416141
-1045.989046	-8.191586	4.426138
-1043.860493	-9.900982	4.436134
-1042.167137	-12.244981	4.446131
-1040.401598	-16.154219	4.456128
-1038.500968	-10.393421	4.466125
-1036.558391	-9.360414	4.476122
-1034.748555	-8.010909	4.486118
-1033.042315	-11.323285	4.496115
-1030.901451	-16.663083	4.506112
-1028.908945	-11.496449	4.516109
-1027.265332	-15.332492	4.526106
-1025.383145	-18.076157	4.536102
-1023.454069	-17.107297	4.546099
-1021.505768	-10.927790	4.556096
-1019.687890	-18.991727	4.566093
-1017.855248	-7.741053	4.576090
-1016.033081	-7.527197	4.586086
-1013.864404	-10.480887	4.596083
-1012.134483	-10.054905	4.606080
-1010.312797	-11.438874	4.616077
-1008.418372	-9.073396	4.626074
-1006.540054	-7.984296	4.636070
-1004.761533	-7.545555	4.646067
-1002.700298	-11.571533	4.656064
-1001.003810	-8.035962	4.666061
-998.905077	-8.758436	4.676058
-997.175279	-7.839788	4.686054
-995.215273	-5.312680	4.696051
-993.569100	-11.149652	4.706048
-991.552620	-13.250028	4.716045
-989.480943	-10.723406	4.726042
-987.776252	-13.225498	4.736038
-985.896402	-18.900884	4.746035
-984.109708	-9.583372	4.756032
-982.347149	-10.217332	4.766029
-980.410917	-12.983817	4.776026
-978.486010	-10.800032	4.786022
-976.427988	-15.444425	4.796019
-974.788791	-6.671739	4.806016
-972.520032	-8.272440	4.816013
-970.629041	-9.659567	4.826010
-969.237251	-3.316802	4.836006
-967.422259	-7.113898	4.846003
-965.025635	-8.645038	4.856000
-963.383570	-12.573950	4.865997
-961.448867	-12.591208	4.875994
-959.514547	-8.307317	4.885990
-957.560904	-11.198148	4.895987
-956.277156	-10.051824	4.905984
-954.139616	-8.416761	4.915981
-952.122865	-3.861831	4.925978
-950.077175	-6.339478	4.935974
-948.591561	-10.683893	4.945971
-946.359106	-5.599763	4.955968
-944.479500	-5.087139	4.965965
-942.824736	-5.798570	4.975962
-940.791911	-8.169941	4.985958
-939.148418	-2.764254	4.995955
-936.927077	-14.909527	5.005952
-935.224413	-14.510708	5.015949
-933.707271	-7.534277	5.025946
-931.461018	-9.481869	5.035942
-929.808381	-11.620330	5.045939
-927.735658	-6.717484	5.055936
-925.918281	-13.241793	5.065933
-924.141938	-6.584698	5.075930
-922.005018	-9.327963	5.085926
-920.255510	-3.607632	5.095923
-918.223654	-5.195664	5.105920
-916.520108	-5.758559	5.115917
-914.953204	-3.970638	5.125914
-912.525549	-9.356193	5.135910
-910.599315	-7.641514	5.145907
-908.834842	-12.099967	5.155904
-907.180012	-2.410770	5.165901
-905.150714	-5.940504	5.175898
-903.481791	-0.368328	5.185894
-901.473765	-2.228854	5.195891
-899.398071	-8.491288	5.205888
-898.056765	-5.400959	5.215885
-895.820826	-6.718442	5.225882
-893.897340	-5.363311	5.235878
-892.103765	-4.527414	5.245875
-890.208756	-6.534072	5.255872
-888.301326	-10.151676	5.265869
-886.478109	-8.744193	5.275866
-884.577255	-10.897046	5.285862
-882.763718	-7.004307	5.295859
-880.670186	-11.635351	5.305856
-879.008465	-5.705161	5.315853
-877.084093	-5.313325	5.325850
-875.367651	-4.971929	5.335846
-873.474411	-5.151433	5.345843
-871.350436	-9.081542	5.355840
-869.548957	-6.257400	5.365837
-867.685914	-1.022549	5.375834
-865.914804	-2.384112	5.385830
-863.631152	-5.247101	5.395827
-862.269652	-6.437386	5.405824
-860.141415	-1.830721	5.415821
-858.416428	-9.188116	5.425818
-856.394219	-6.947151	5.435814
-854.466133	-1.860057	5.445811
-852.602541	-8.164335	5.455808
-850.977994	-10.362990	5.465805
-848.979046	-10.722007	5.475802
-846.955467	-14.012354	5.485798
-845.181322	-14.637011	5.495795
-843.355888	-7.078215	5.505792
-841.512405	-7.202371	5.515789
-839.505863	-11.486313	5.525786
-837.758454	-11.923531	5.535782
-835.793103	-10.132937	5.545779
-833.670720	-9.485348	5.555776
-831.963958	-8.322892	5.565773
-830.169320	-6.565002	5.575770
-828.191386	-6.489586	5.585766
-826.387497	-5.176861	5.595763
-824.756961	-3.683263	5.605760
-822.818921	-6.827285	5.615757
-820.834354	-0.684969	5.625754
-819.068411	-1.832512	5.635750
-817.043588	-7.524637	5.645747
-814.973988	-1.271171	5.655744
-813.135043	-13.535220	5.665741
-811.486260	-8.765026	5.675738
-809.485006	-9.238064	5.685734
-807.506223	-1.383217	5.695731
-806.009747	-9.885116	5.705728
-803.929336	-13.609253	5.715725
-801.855402	-0.109030	5.725722
-800.186787	-10.444775	5.735718
-798.316845	-11.689452	5.745715
-796.369734	-13.254361	5.755712
-794.320804	-10.763400	5.765709
-793.148413	-12.663950	5.775706
-790.864325	-6.877384	5.785702
-788.878593	-14.026934	5.795699
-786.938100	-9.030189	5.805696
-785.136253	-8.658167	5.815693
-783.380302	-7.426168	5.825690
-781.368909	-2.969700	5.835686
-779.394772	-15.645339	5.845683
-777.822564	-13.232904	5.855680
-775.481148	-10.449198	5.865677
-773.777801	-10.310900	5.875674
-772.187268	-12.243537	5.885670
-770.272472	-8.430049	5.895667
-768.335162	-11.686017	5.905664
-766.057875	-12.113136	5.915661
-764.715263	-3.992358	5.925658
-762.533018	-2.684792	5.935654
-760.662338	-6.678534	5.945651
-758.868447	-9.654201	5.955648
-756.740487	-8.180057	5.965645
-755.169649	-4.502636	5.975642
-753.352279	-7.343104	5.985638
-751.256028	-8.011277	5.995635
-749.466126	-9.655234	6.005632
-747.495869	-14.490676	6.015629
-745.944653	-7.915875	6.025626
-744.134300	-13.431556	6.035622
-741.790997	-7.673350	6.045619
-740.008762	-14.687707	6.055616
-738.214951	-15.882275	6.065613
-736.442126	-8.564456	6.075610
-734.530920	-9.558307	6.085606
-732.772252	-10.177249	6.095603
-730.746009	-12.296336	6.105600
-728.588116	-12.510126	6.115597
-726.967872	-9.514799	6.125594
-725.068942	-12.567229	6.135590
-723.253295	-15.841612	6.145587
-721.347714	-4.337057	6.155584
-719.689371	-6.138390	6.165581
-717.801884	-6.424220	6.175578
-715.565235	3.273210	6.185574
-713.464945	1.093354	6.195571
-712.069204	-4.155520	6.205568
-710.334205	-6.512261	6.215565
-708.205331	-1.532917	6.225562
-706.200823	-4.520099	6.235558
-704.599151	-2.428112	6.245555
-702.448963	-3.815396	6.255552
-700.565251	-5.370097	6.265549
-698.939486	-6.525150	6.275546
-696.817228	-2.290009	6.285542
-694.951108	-5.308752	6.295539
-693.469041	-2.296056	6.305536
-691.435749	0.568555	6.315533
-689.341445	-3.002970	6.325530
-687.522197	-6.064744	6.335526
-685.903663	-7.070210	6.345523
-683.779583	-6.500126	6.355520
-681.678979	-4.693117	6.365517
-680.381879	-2.426127	6.375514
-678.336792	-2.386579	6.385510
-676.364364	-2.738055	6.395507
-674.016424	-7.062208	6.405504
-672.397948	-8.951876	6.415501
-670.907710	-5.648363	6.425498
-668.922829	-8.731853	6.435494
-666.703770	-7.949559	6.445491
-664.963865	-8.224397	6.455488
-663.400122	-8.077922	6.465485
-661.244878	-1.354832	6.475482
-659.450096	0.084217	6.485478
-657.664508	-15.215451	6.495475
-655.527326	-8.004731	6.505472
-653.546805	-11.496463	6.515469
-651.976086	-9.427916	6.525466
-650.228600	-8.608153	6.535462
-648.051491	-10.114954	6.545459
-646.355807	-8.115318	6.555456
-644.384598	-14.484008	6.565453
-642.452316	-9.736879	6.575450
-640.603778	-9.504840	6.585446
-638.898133	-11.394203	6.595443
-637.139467	-10.048841	6.605440
-635.054774	-10.020321	6.615437
-633.152366	-8.939505	6.625434
-631.249561	-4.732398	6.635430
-629.320738	-10.420088	6.645427
-627.448168	-8.230802	6.655424
-625.672503	-10.292398	6.665421
-624.012564	-6.523330	6.675418
-621.874361	-2.476984	6.685414
-619.942278	-12.892610	6.695411
-618.049733	-5.134339	6.705408
-616.058202	-9.701498	6.715405
-614.750284	-9.318327	6.725402
-612.825208	-2.815788	6.735398
-610.245276	-7.949060	6.745395
-608.622595	-6.409844	6.755392
-606.850728	-9.700834	6.765389
-605.193111	-8.192460	6.775386
-603.199708	-4.239807	6.785382
-601.125515	-5.911705	6.795379
-599.275270	-11.064179	6.805376
-597.512583	-6.398865	6.815373
-595.568902	-8.037276	6.825370
-593.744498	-7.097125	6.835366
-591.910184	-8.844377	6.845363
-590.142985	-10.865120	6.855360
-588.067057	-7.478276	6.865357
-586.460487	-8.147024	6.875354
-584.396995	-7.949280	6.885350
-582.561634	-9.856168	6.895347
-580.475528	-8.188859	6.905344
-578.764051	-9.120679	6.915341
-576.714033	-7.989186	6.925338
-575.092993	-7.018112	6.935334
-572.953035	-8.102064	6.945331
-571.463782	-10.184182	6.955328
-569.300452	-4.801258	6.965325
-567.413899	0.861150	6.975322
-565.849240	-4.752530	6.985318
-563.684441	-7.599410	6.995315
-561.794951	-8.723868	7.005312
-559.906980	-12.421796	7.015309
-558.318338	-8.756555	7.025306
-556.474386	-4.685249	7.035302
-554.260552	-11.525266	7.045299
-552.201224	-16.542155	7.055296
-550.662123	-12.660573	7.065293
-548.928006	-11.653859	7.075290
-546.800213	-7.179460	7.085286
-544.800874	-5.951421	7.095283
-543.003375	-8.657505	7.105280
-541.168267	-9.301149	7.115277
-539.354002	-10.288834	7.125274
-537.650945	-6.253428	7.135270
-535.567577	-16.562104	7.145267
-533.696850	-10.772406	7.155264
-531.979933	-7.953435	7.165261
-530.028582	-9.900917	7.175258
-527.836379	-6.651014	7.185254
-526.370261	-11.015754	7.195251
-524.515777	-12.384067	7.205248
-522.346984	-17.787895	7.215245
-520.329720	-13.641611	7.225242
-518.983862	-10.270726	7.235238
-516.658656	-10.291571	7.245235
-514.994589	-9.444172	7.255232
-512.985725	-12.073466	7.265229
-511.264659	-4.061918	7.275226
-509.320191	-3.720360	7.285222
-507.332173	-2.916803	7.295219
-505.685860	-10.649830	7.305216
-503.809490	-2.923611	7.315213
-501.968799	-3.814435	7.325210
-500.149032	-3.707165	7.335206
-497.872366	-5.922900	7.345203
-496.095884	-6.555566	7.355200
-494.097196	-6.857401	7.365197
-492.453769	-3.818238	7.375194
-490.640495	-7.201024	7.385190
-488.803731	-1.862180	7.395187
-486.428357	-4.519991	7.405184
-484.823823	-3.901486	7.415181
-483.326242	-4.783287	7.425178
-481.170835	-1.173771	7.435174
-479.281996	-8.116560	7.445171
-477.244835	-9.741384	7.455168
-475.722761	-15.622945	7.465165
-473.798332	-11.182316	7.475162
-471.748936	-4.154764	7.485158
-470.002263	-9.519556	7.495155
-467.982695	-11.332618	7.505152
-466.078405	-10.646708	7.515149
-463.805794	-5.822722	7.525146
-462.580828	-4.148833	7.535142
-460.534235	-11.061536	7.545139
-458.733660	-14.218055	7.555136
-456.692384	-9.293959	7.565133
-454.792488	-12.774236	7.575130
-452.883417	-5.511097	7.585126
-451.466991	-3.441457	7.595123
-449.465111	-5.087466	7.605120
-447.354562	-4.022370	7.615117
-445.357345	-5.890266	7.625114
-443.623349	-3.817650	7.635110
-441.853714	-11.418752	7.645107
-440.067947	-7.745433	7.655104
-438.160759	-5.915211	7.665101
-436.020081	-1.010125	7.675098
-434.155034	-1.682152	7.685094
-432.186876	1.409410	7.695091
-430.394940	-7.756849	7.705088
-428.950614	-4.526370	7.715085
-426.734458	-9.165567	7.725082
-424.918986	-2.200091	7.735078
-423.099149	-4.271752	7.745075
-420.979515	-6.486023	7.755072
-419.135010	-7.704240	7.765069
-417.491775	-5.411846	7.775066
-415.463678	1.994958	7.785062
-413.585894	-0.305427	7.795059
-411.780859	-4.323165	7.805056
-410.032129	-2.983940	7.815053
-407.930552	-3.363712	7.825050
-406.037409	-2.928609	7.835046
-404.046422	-10.405556	7.845043
-402.395665	-8.147511	7.855040
-400.561776	-5.193960	7.865037
-398.427083	-3.829512	7.875034
-396.962629	-5.948619	7.885030
-394.906069	-1.802179	7.895027
-392.920826	-8.937144	7.905024
-391.380432	-12.792607	7.915021
-389.067975	-6.072250	7.925018
-387.482788	-7.569567	7.935014
-385.455147	-2.463225	7.945011
-383.334743	-2.462291	7.955008
-381.722790	-1.330156	7.965005
-379.942644	1.019354	7.975002
-378.135456	-1.869741	7.984998
-375.933065	0.870254	7.994995
-374.161922	-2.714145	8.004992
-372.387295	-0.464802	8.014989
-370.700563	0.819614	8.024986
-368.693178	0.080699	8.034982
-366.782616	-5.325982	8.044979
-364.772493	-3.968457	8.054976
-362.880884	-3.962555	8.064973
-361.276801	-1.607026	8.074970
-359.166311	-2.000810	8.084966
-357.303493	-7.494599	8.094963
-355.253820	-7.979723	8.104960
-353.609640	-3.446875	8.114957
-351.786377	-4.292170	8.124954
-349.685891	-6.534902	8.134950
-347.942384	-4.650052	8.144947
-345.922551	-5.256723	8.154944
-344.205515	-11.207233	8.164941
-342.552987	-5.570431	8.174938
-340.711440	-5.567571	8.184934
-338.698200	-7.100039	8.194931
-336.620607	-5.123253	8.204928
-334.548221	-8.750980	8.214925
-332.831965	-4.676473	8.224922
-331.018963	-8.010151	8.234918
-329.462217	-7.226015	8.244915
-327.219879	1.485635	8.254912
-325.461276	-6.737325	8.264909
-323.576034	-1.156607	8.274906
-321.756710	4.595694	8.284902
-319.723431	1.463701	8.294899
-317.817899	-2.637910	8.304896
-316.138033	-9.597748	8.314893
-314.236057	0.387216	8.324890
-312.376839	1.307817	8.334886
-310.468135	-4.976434	8.344883
-308.527996	-3.427686	8.354880
-306.445677	-4.197459	8.364877
-304.960011	-6.119369	8.374874
-302.956864	-0.154817	8.384870
-301.276308	-4.179448	8.394867
-299.023439	-3.305888	8.404864
-297.187078	-3.149008	8.414861
-295.225221	-3.417954	8.424858
-293.651816	-5.064912	8.434854
-291.539065	-13.404382	8.444851
-289.559701	-8.048665	8.454848
-288.143352	-4.429941	8.464845
-286.308985	-2.253228	8.474842
-284.198762	-2.890065	8.484838
-282.264559	-5.313042	8.494835
-280.329123	-3.401936	8.504832
-278.514158	-9.851202	8.514829
-276.596417	-13.075242	8.524826
-274.696453	-6.568399	8.534822
-273.188154	-4.053833	8.544819
-270.982214	-2.803276	8.554816
-268.955344	-7.361594	8.564813
-267.283086	-5.550575	8.574810
-265.482290	-3.813758	8.584807
-263.268484	-6.893991	8.594803
-261.833453	0.877624	8.604800
-259.881289	-3.622973	8.614797
-257.733381	-8.975877	8.624794
-256.120185	-2.473770	8.634791
-254.338015	-1.853462	8.644787
-252.099849	-7.062871	8.654784
-250.280401	-11.095426	8.664781
-248.503544	-6.002617	8.674778
-246.727976	-6.314422	8.684775
-245.064424	-4.440418	8.694771
-242.567646	-5.721560	8.704768
-240.913950	-3.621765	8.714765
-239.137445	-2.733695	8.724762
-237.286884	-0.652688	8.734759
-235.459358	0.636196	8.744755
-233.643077	-3.181103	8.754752
-231.491253	-0.268687	8.764749
-229.789126	0.133885	8.774746
-227.953309	2.572523	8.784743
-226.071869	-1.228329	8.794739
-224.040489	-2.954653	8.804736
-222.033377	-7.299777	8.814733
-220.332659	-5.812220	8.824730
-218.619231	-2.597714	8.834727
-216.575368	-7.041858	8.844723
-214.587400	-10.556538	8.854720
-212.895452	-5.495939	8.864717
-210.910695	-2.828424	8.874714
-209.285644	-6.027807	8.884711
-206.948078	-10.326183	8.894707
-205.017507	-17.864389	8.904704
-203.575688	-15.719702	8.914701
-201.734531	-9.730789	8.924698
-199.825994	-7.186892	8.934695
-198.064098	-11.680759	8.944691
-195.908026	-9.397421	8.954688
-194.027338	-10.139655	8.964685
-191.926016	-14.785583	8.974682
-190.482257	-12.900148	8.984679
-188.562928	-9.206894	8.994675
-186.561778	-13.568406	9.004672
-184.596124	-14.643145	9.014669
-182.814763	-10.108381	9.024666
-181.002197	-15.835604	9.034663
-178.987095	-15.276098	9.044659
-177.490258	-12.235423	9.054656
-175.400845	-15.701522	9.064653
-173.656976	-12.116048	9.074650
-171.775139	-14.121627	9.084647
-169.566307	-9.762439	9.094643
-167.638354	-17.443888	9.104640
-165.692966	-19.443813	9.114637
-164.188450	-15.482236	9.124634
-162.274580	-16.502903	9.134631
-160.345797	-14.184842	9.144627
-158.338054	-14.329945	9.154624
-156.432864	-19.332971	9.164621
-154.471590	-19.262232	9.174618
-152.794771	-14.775501	9.184615
-151.302336	-14.483100	9.194611
-149.453669	-16.306523	9.204608
-146.790723	-21.253615	9.214605
-145.465597	-16.440754	9.224602
-143.562362	-14.503872	9.234599
-141.508784	-17.124211	9.244595
-139.577484	-16.930253	9.254592
-137.753101	-18.707160	9.264589
-136.338103	-20.445584	9.274586
-134.065167	-9.968597	9.284583
-132.172766	-17.265393	9.294579
-130.128306	-9.505673	9.304576
-128.145840	-13.824684	9.314573
-126.492069	-12.144828	9.324570
-124.831880	-11.523908	9.334567
-123.015590	-11.832647	9.344563
-121.128833	-20.206973	9.354560
-119.238538	-12.935812	9.364557
-117.037509	-8.998495	9.374554
-115.298342	-10.695472	9.384551
-113.375156	-12.431284	9.394547
-111.642029	-14.771517	9.404544
-109.544732	-12.582934	9.414541
-107.576948	-17.629071	9.424538
-106.205165	-6.442994	9.434535
-104.078648	-11.394455	9.444531
-102.084201	-9.844729	9.454528
-100.010876	-6.878615	9.464525
-98.567077	-9.709527	9.474522
-96.674795	-16.063632	9.484519
-94.779309	-13.664414	9.494515
-92.903101	-15.320081	9.504512
-90.743628	-19.307296	9.514509
-89.003871	-13.976335	9.524506
-87.477614	-8.333408	9.534503
-85.087584	-11.163700	9.544499
-83.142895	-13.979780	9.554496
-81.616086	-11.537518	9.564493
-79.845138	-11.340035	9.574490
-77.605736	-7.806703	9.584487
-75.858474	-13.586595	9.594483
-74.079495	-8.170297	9.604480
-72.262829	-5.532690	9.614477
-70.244086	-7.995832	9.624474
-68.766575	-10.832106	9.634471
-66.461017	-9.781993	9.644467
-64.636595	-11.336218	9.654464
-62.980097	-6.424590	9.664461
-60.808143	-0.210431	9.674458
-59.006017	-9.817031	9.684455
-57.037782	-3.312996	9.694451
-55.191294	-7.258147	9.704448
-53.490608	-8.656832	9.714445
-51.393006	-9.247243	9.724442
-49.746847	-3.228671	9.734439
-47.722643	-9.747477	9.744435
-45.766169	-8.617970	9.754432
-43.909586	-6.643562	9.764429
-42.116286	-7.471214	9.774426
-40.512108	-8.011322	9.784423
-38.653360	-6.738321	9.794419
-36.420223	-11.176199	9.804416
-34.381209	-12.679370	9.814413
-32.637811	-12.985888	9.824410
-30.921876	-16.073335	9.834407
-29.113712	-14.474884	9.844403
-26.994859	-14.594971	9.854400
-25.227944	-8.423539	9.864397
-23.306636	-15.222757	9.874394
-21.428260	-1.365276	9.884391
-19.668781	-4.797565	9.894387
-17.882259	-7.203094	9.904384
-15.571754	-9.850105	9.914381
-13.951063	-0.367906	9.924378
-12.588357	-6.054836	9.934375
-10.257311	-12.530978	9.944371
-8.417392	-9.248072	9.954368
-6.472582	-1.917609	9.964365
-5.025753	5.768617	9.974362
-3.533424	28.479477	9.984359
-2.021154	67.908633	9.994355
-0.617353	121.112940	10.004352
0.000000	163.879966	10.009357
0.709022	205.435380	10.014362
1.531023	244.716226	10.019367
2.016044	266.916953	10.024371
2.041355	291.548644	10.029376
2.644644	313.325292	10.034381
2.638989	324.464506	10.039386
3.019483	350.936765	10.044391
3.413879	356.347622	10.049395
3.476137	369.382627	10.054400
3.487855	365.294767	10.059405
3.998704	374.265263	10.064410
3.812484	371.726047	10.069415
3.753474	374.939933	10.074419
3.888228	389.091735	10.079424
4.111532	402.228819	10.084429
4.204921	405.084078	10.089434
4.171634	410.008069	10.094439
4.632581	398.425592	10.099443
4.256733	402.103197	10.104448
4.330864	395.917422	10.109453
4.440935	399.386626	10.114458
4.225059	399.862632	10.119463
3.994252	405.702827	10.124467
4.120597	409.171015	10.129472
4.507900	425.333460	10.134477
4.691249	428.735788	10.139482
4.552379	434.591292	10.144487
4.830807	433.250593	10.149491
4.660223	441.541324	10.154496
4.616670	443.525849	10.159501
4.898482	439.524199	10.164506
4.571724	441.563359	10.169511
5.161335	437.230329	10.174515
4.998598	458.288840	10.179520
4.918947	449.624860	10.184525
5.152713	453.077501	10.189530
4.546186	451.195115	10.194535
5.083176	447.687365	10.199539
5.131726	450.671214	10.204544
5.085333	449.562105	10.209549
4.876918	467.089111	10.214554
4.778121	456.611467	10.219559
5.409568	455.468353	10.224563
5.218930	459.621072	10.229568
5.125248	458.655127	10.234573
5.311124	458.229660	10.239578
5.059456	474.713288	10.244583
5.293134	464.739289	10.249587
5.155448	477.429380	10.254592
5.542471	496.487341	10.259597
5.502665	503.889890	10.264602
5.669036	492.333826	10.269607
5.948681	497.783541	10.274611
5.643453	517.745188	10.279616
5.727548	510.024917	10.284621
5.971164	507.185293	10.289626
5.409016	520.660668	10.294631
5.899626	513.457471	10.299635
5.640110	517.173321	10.304640
5.758347	508.272729	10.309645
5.956467	516.419532	10.314650
5.612397	516.327764	10.319655
6.008640	533.747362	10.324659
6.223511	541.173965	10.329664
6.252843	544.921022	10.334669
6.431409	550.642357	10.339674
6.282366	559.579451	10.344679
6.461269	552.460649	10.349683
6.268784	560.642973	10.354688
6.426338	559.980737	10.359693
6.333096	569.441969	10.364698
6.455821	567.302889	10.369703
6.878984	558.732113	10.374707
6.504192	569.432058	10.379712
6.393896	568.976556	10.384717
6.616853	571.550972	10.389722
6.247799	569.857781	10.394727
6.534833	576.443379	10.399731
6.522205	574.723298	10.404736
6.292557	582.498383	10.409741
6.943684	589.770265	10.414746
6.692245	599.737742	10.419751
6.896463	604.814735	10.424755
6.857897	611.570562	10.429760
6.716240	615.480535	10.434765
7.215609	607.342296	10.439770
6.690298	609.381609	10.444775
7.003865	609.054047	10.449779
7.094080	606.857066	10.454784
7.191444	633.281959	10.459789
7.374400	648.382792	10.464794
7.549366	648.463709	10.469799
7.617626	652.409598	10.474803
7.327837	656.370020	10.479808
7.476059	643.958827	10.484813
7.403876	653.566571	10.489818
6.979224	649.805292	10.494823
7.888931	654.895933	10.499827
7.704207	669.809420	10.504832
7.908887	659.392038	10.509837
7.844136	658.971848	10.514842
7.869969	656.923908	10.519847
8.070272	663.002960	10.524851
7.638048	664.548015	10.529856
7.839065	663.378923	10.534861
7.943324	660.864288	10.539866
7.770081	660.847777	10.544871
8.060784	654.482260	10.549875
7.858546	662.642541	10.554880
8.034857	673.016525	10.559885
8.156509	694.698676	10.564890
8.234075	698.105324	10.569895
8.454109	686.619398	10.574899
8.522892	708.265845	10.579904
7.967793	699.948805	10.584909
8.288198	700.362934	10.589914
8.188309	711.261996	10.594919
8.451935	699.072057	10.599923
8.149555	717.175776	10.604928
8.208593	709.202340	10.609933
8.588122	712.505629	10.614938
8.269972	722.445982	10.619943
8.619385	733.158269	10.624947
8.451750	736.973065	10.629952
8.750247	743.459134	10.634957
8.871610	742.154500	10.639962
8.606604	748.014480	10.644967
8.846428	744.765385	10.649971
8.757355	744.207138	10.654976
8.968268	749.008710	10.659981
8.745509	758.668929	10.664986
8.993900	778.194099	10.669991
9.646278	765.096800	10.674995
9.309895	779.235031	10.680000
9.250279	782.128963	10.685005
9.234610	791.180550	10.690010
9.181411	800.381640	10.695015
9.528410	786.397846	10.700019
9.187855	793.294972	10.705024
8.923708	789.222609	10.710029
9.161240	793.144689	10.715034
9.105283	797.892645	10.720039
9.606567	791.799426	10.725043
9.692073	809.068636	10.730048
9.848619	824.735294	10.735053
10.111682	820.801191	10.740058
9.735094	818.178714	10.745063
9.595962	799.765249	10.750067
9.712319	810.978420	10.755072
9.668043	822.685604	10.760077
9.919185	819.551389	10.765082
9.698724	836.825279	10.770087
9.990941	830.637652	10.775091
9.663971	832.976537	10.780096
10.055090	838.452758	10.785101
10.093744	830.542435	10.790106
9.932056	829.041653	10.795111
10.488521	842.911365	10.800115
10.074843	858.263712	10.805120
10.572847	859.609942	10.810125
10.614435	860.817650	10.815130
10.229842	865.389375	10.820135
10.232099	858.377454	10.825139
10.418187	863.805958	10.830144
10.579151	870.314022	10.835149
10.558392	869.815842	10.840154
10.824070	873.019050	10.845159
10.694054	869.147633	10.850163
10.648211	880.763646	10.855168
10.751495	873.565281	10.860173
10.766402	878.208913	10.865178
10.457473	870.472289	10.870183
10.773197	869.357429	10.875187
10.754805	876.370375	10.880192
10.825342	892.896126	10.885197
11.290858	901.550887	10.890202
11.133613	908.112879	10.895207
11.185905	910.362894	10.900211
11.069582	921.499716	10.905216
11.178775	920.143388	10.910221
11.311112	912.079296	10.915226
11.256513	930.796658	10.920231
11.678483	914.193905	10.925235
11.651825	911.537672	10.930240
11.385767	923.915869	10.935245
11.527288	909.333909	10.940250
11.372010	910.448434	10.945255
11.623380	916.836436	10.950259
11.298546	929.496843	10.955264
11.312874	918.989782	10.960269
11.819710	921.758693	10.965274
11.566797	915.451387	10.970279
11.252887	920.191639	10.975283
11.755977	934.798553	10.980288
11.615478	948.043050	10.985293
11.770862	956.843513	10.990298
11.685321	957.096882	10.995303
12.044649	958.965171	11.000307
11.911025	959.327141	11.005312
11.901640	961.322056	11.010317
12.233601	951.639576	11.015322
11.870514	964.307692	11.020327
12.051826	964.647815	11.025331
12.197873	980.198036	11.030336
12.571243	986.684888	11.035341
12.580793	982.184009	11.040346
11.985449	983.032819	11.045351
12.424735	984.583984	11.050355
12.434698	997.952770	11.055360
12.584631	996.518968	11.060365
12.659852	997.319170	11.065370
12.215787	1006.917074	11.070375
12.391901	995.406370	11.075379
12.529479	1000.363236	11.080384
12.317310	1001.366985	11.085389
12.265032	998.072957	11.090394
12.631708	1014.703009	11.095399
12.870583	1016.601558	11.100403
13.039276	1024.966246	11.105408
12.805564	1029.018755	11.110413
13.001716	1019.204917	11.115418
13.054253	1027.250641	11.120423
13.187871	1019.713027	11.125427
13.061027	1017.197344	11.130432
13.038941	1027.339855	11.135437
13.283624	1025.372082	11.140442
12.827628	1035.782522	11.145447
13.261695	1029.217344	11.150451
13.385426	1045.291626	11.155456
13.024243	1055.070322	11.160461
13.688419	1057.418318	11.165466
13.297447	1065.476454	11.170471
13.423738	1069.042587	11.175475
13.232039	1072.318794	11.180480
13.721219	1068.559887	11.185485
13.746636	1070.842601	11.190490
13.482020	1076.097052	11.195495
13.715600	1068.759528	11.200499
13.824181	1068.333757	11.205504
13.375253	1070.498153	11.210509
14.005293	1077.716872	11.215514
13.875716	1091.671018	11.220519
13.969062	1094.600542	11.225523
14.372037	1095.695428	11.230528
14.053275	1104.077984	11.235533
14.431061	1103.882107	11.240538
14.199286	1097.598161	11.245543
14.233219	1091.910551	11.250547
14.395862	1103.279003	11.255552
14.228196	1104.663622	11.260557
14.491539	1100.317783	11.265562
13.944954	1107.419821	11.270567
14.088751	1101.722568	11.275571
14.063806	1102.634955	11.280576
14.264928	1117.351726	11.285581
14.194704	1111.655489	11.290586
14.027604	1115.881915	11.295591
14.321327	1128.387055	11.300595
14.685123	1143.224573	11.305600
14.710532	1145.521494	11.310605
14.447715	1138.182682	11.315610
14.503559	1153.547186	11.320615
14.671246	1141.246015	11.325619
14.861441	1145.394957	11.330624
14.926915	1153.568008	11.335629
14.880929	1144.437736	11.340634
14.887675	1160.215389	11.345639
15.347282	1169.215058	11.350643
15.444069	1175.564748	11.355648
15.259515	1166.778290	11.360653
15.565015	1158.978202	11.365658
15.014920	1165.224470	11.370663
15.579991	1164.856783	11.375667
15.329523	1162.233049	11.380672
15.400383	1175.806768	11.385677
15.604345	1172.661079	11.390682
15.479037	1177.678862	11.395687
15.205380	1180.597551	11.400691
15.654944	1178.923535	11.405696
15.431407	1184.813346	11.410701
15.736017	1182.061644	11.415706
15.778558	1178.127925	11.420711
15.769684	1183.048284	11.425715
15.696376	1180.790560	11.430720
15.490588	1191.847233	11.435725
16.055070	1181.277464	11.440730
15.575067	1183.659738	11.445735
15.873781	1181.210200	11.450739
16.061689	1180.196137	11.455744
15.833092	1186.354861	11.460749
16.068243	1181.573487	11.465754
15.954489	1182.648291	11.470759
16.296638	1206.863532	11.475763
16.083433	1208.195495	11.480768
16.109792	1216.450521	11.485773
16.595275	1218.308184	11.490778
16.551691	1221.567108	11.495783
16.395493	1222.833204	11.500787
16.626084	1218.798510	11.505792
16.418592	1220.104329	11.510797
16.586294	1227.511998	11.515802
16.449581	1225.149254	11.520807
16.606561	1211.812005	11.525811
16.633976	1227.097536	11.530816
16.584095	1228.800877	11.535821
16.656021	1218.566712	11.540826
16.478507	1234.869043	11.545831
16.703618	1220.642479	11.550835
16.457778	1218.399652	11.555840
16.561159	1236.954214	11.560845
17.026991	1246.394524	11.565850
16.770537	1255.302651	11.570855
17.307402	1242.195755	11.575859
17.327077	1253.180239	11.580864
17.283543	1262.529115	11.585869
17.471689	1235.262707	11.590874
17.193191	1247.977505	11.595879
17.249306	1246.904816	11.600883
17.552325	1256.433397	11.605888
17.389453	1253.013436	11.610893
17.378331	1239.145473	11.615898
17.219623	1259.009849	11.620903
17.507175	1250.051835	11.625907
17.478268	1254.499130	11.630912
17.130123	1259.302516	11.635917
17.512059	1252.831505	11.640922
17.632730	1248.890036	11.645927
17.541498	1254.060908	11.650931
17.483313	1265.877910	11.655936
17.612108	1276.752746	11.660941
18.078470	1281.698270	11.665946
18.146866	1282.979014	11.670951
18.377961	1285.583014	11.675955
18.157623	1273.056593	11.680960
17.452345	1261.646049	11.685965
18.041450	1271.733825	11.690970
18.276490	1286.855402	11.695975
18.230242	1289.218975	11.700979
18.157209	1287.775762	11.705984
18.186996	1292.070191	11.710989
18.707364	1290.404583	11.715994
18.606299	1295.677184	11.720999
18.735591	1286.071758	11.726003
18.525281	1289.175135	11.731008
18.343307	1291.268594	11.736013
18.631026	1285.761222	11.741018
18.702766	1288.140671	11.746023
18.706555	1292.369855	11.751027
18.856679	1296.823304	11.756032
18.564024	1301.389961	11.761037
18.715038	1290.930221	11.766042
18.360281	1298.348714	11.771047
19.099488	1286.929331	11.776051
18.745899	1283.945886	11.781056
18.715820	1293.867487	11.786061
19.140859	1289.913732	11.791066
18.754058	1285.463362	11.796071
18.713878	1284.796362	11.801075
18.746164	1295.168529	11.806080
18.878597	1296.834124	11.811085
19.152091	1301.782819	11.816090
18.901643	1326.244183	11.821095
19.373620	1330.086433	11.826099
19.251292	1325.651431	11.831104
18.774863	1325.068206	11.836109
18.634902	1328.855085	11.841114
18.882758	1335.657822	11.846119
19.183038	1341.944373	11.851123
19.298860	1347.816393	11.856128
19.362887	1358.185908	11.861133
19.644282	1361.028716	11.866138
19.510869	1365.990292	11.871143
19.689837	1367.431620	11.876147
19.687480	1369.876523	11.881152
19.263575	1368.621745	11.886157
19.803845	1360.236059	11.891162
20.109705	1360.536613	11.896167
19.698704	1359.457990	11.901171
19.750031	1361.942430	11.906176
19.862902	1382.150836	11.911181
20.354134	1390.116536	11.916186
20.365111	1393.317905	11.921191
20.369193	1378.608362	11.926195
20.129884	1376.324253	11.931200
20.130331	1385.616513	11.936205
20.282903	1382.665075	11.941210
20.373892	1387.940195	11.946215
20.381864	1388.296938	11.951219
20.421798	1389.549113	11.956224
20.385736	1393.739735	11.961229
20.484087	1394.026075	11.966234
20.492296	1387.859069	11.971239
20.727573	1384.132695	11.976243
20.814936	1393.669743	11.981248
20.284897	1399.089660	11.986253
20.976156	1392.517206	11.991258
20.672572	1392.675249	11.996263
20.615574	1391.596146	12.001267
20.969443	1388.209648	12.006272
20.862963	1396.750918	12.011277
21.041068	1393.337256	12.016282
20.702631	1395.747450	12.021287
21.038831	1396.938176	12.026291
21.093285	1388.521143	12.031296
20.987368	1402.374031	12.036301
21.007785	1393.740052	12.041306
20.869459	1390.113484	12.046311
21.322508	1397.985132	12.051315
21.058214	1397.796253	12.056320
20.992893	1405.629150	12.061325
21.180826	1393.490134	12.066330
21.154676	1390.060161	12.071335
21.093878	1382.406699	12.076339
21.017144	1371.773473	12.081344
20.677014	1374.281715	12.086349
20.928022	1360.285874	12.091354
21.010921	1366.722238	12.096359
21.048104	1362.278341	12.101363
20.957704	1363.717686	12.106368
20.839075	1368.473458	12.111373
20.918251	1362.055423	12.116378
20.650994	1371.288651	12.121383
20.650867	1367.887651	12.126387
21.242839	1373.653770	12.131392
21.007994	1379.400369	12.136397
21.055328	1366.973900	12.141402
21.085126	1370.019282	12.146407
20.921219	1364.462480	12.151411
21.023109	1361.852689	12.156416
20.959318	1363.667084	12.161421
21.312735	1358.500901	12.166426
21.299116	1376.775441	12.171431
21.037568	1360.097474	12.176435
21.115407	1364.336158	12.181440
21.043780	1375.556092	12.186445
21.189520	1370.626477	12.191450
21.267838	1361.809011	12.196455
21.021727	1355.033605	12.201459
20.862021	1340.644355	12.206464
20.832312	1340.141277	12.211469
20.944863	1333.709257	12.216474
20.768409	1337.300089	12.221479
20.932527	1348.912950	12.226483
20.872393	1347.652195	12.231488
20.781455	1347.441973	12.236493
20.915024	1362.185539	12.241498
21.213370	1362.779056	12.246503
20.811414	1344.290117	12.251507
20.981124	1340.032477	12.256512
20.839434	1342.737742	12.261517
20.981385	1334.916335	12.266522
21.094177	1346.615447	12.271527
20.751764	1336.553742	12.276531
21.071425	1334.443858	12.281536
20.523557	1344.679917	12.286541
20.655280	1343.725273	12.291546
20.768931	1370.151271	12.296551
20.853619	1365.246378	12.301555
21.218908	1370.451718	12.306560
21.082072	1370.733777	12.311565
21.096405	1349.121999	12.316570
20.910073	1343.017584	12.321575
20.758415	1346.028032	12.326579
21.013923	1342.476655	12.331584
20.779016	1337.220586	12.336589
21.025531	1337.429671	12.341594
20.899025	1345.488358	12.346599
21.110669	1341.813078	12.351603
21.131003	1343.168521	12.356608
20.881163	1351.906902	12.361613
20.916195	1339.624358	12.366618
21.192407	1347.859319	12.371623
20.944266	1346.625398	12.376627
21.105947	1342.203443	12.381632
20.655005	1349.847058	12.386637
20.629918	1346.039998	12.391642
20.700258	1353.009843	12.396647
20.785383	1343.743405	12.401651
20.994987	1346.857883	12.406656
21.173227	1344.472482	12.411661
21.344451	1340.388082	12.416666
21.309146	1345.897818	12.421671
21.170626	1349.963619	12.426675
21.435387	1338.558365	12.431680
21.021517	1345.517911	12.436685
20.956865	1344.937608	12.441690
20.881134	1348.814393	12.446695
20.989980	1346.762578	12.451699
21.059507	1342.633681	12.456704
20.786158	1348.768068	12.461709
21.164465	1337.947946	12.466714
21.301664	1334.861762	12.471719
20.951814	1328.669095	12.476723
21.129752	1323.042800	12.481728
21.109682	1320.265583	12.486733
21.053714	1312.693396	12.491738
21.157899	1321.402890	12.496743
20.999263	1325.121776	12.501747
21.317425	1320.351562	12.506752
21.127036	1324.093650	12.511757
21.421987	1317.499278	12.516762
21.349365	1322.829648	12.521767
20.814505	1305.957194	12.526771
20.828626	1287.134643	12.531776
20.603059	1289.922669	12.536781
20.934640	1290.712751	12.541786
20.644277	1300.430634	12.546791
21.107906	1314.465432	12.551795
21.064960	1309.357756	12.556800
20.848601	1314.222937	12.561805
21.076574	1315.398587	12.566810
20.927664	1303.149356	12.571815
20.567068	1299.675757	12.576819
21.065203	1298.419010	12.581824
20.924054	1315.101231	12.586829
21.162102	1302.245390	12.591834
20.698471	1297.055783	12.596839
20.805252	1298.133269	12.601843
21.111856	1303.476479	12.606848
20.778638	1304.143919	12.611853
20.659974	1289.223000	12.616858
20.769900	1306.496791	12.621863
20.970022	1316.580405	12.626867
20.887014	1324.083311	12.631872
21.086405	1330.341791	12.636877
21.097585	1313.507613	12.641882
20.902546	1315.663877	12.646887
20.771040	1298.006361	12.651891
20.765415	1304.167419	12.656896
20.958182	1322.927839	12.661901
20.944679	1320.065987	12.666906
21.117504	1324.652243	12.671911
20.800883	1305.104124	12.676915
21.111141	1309.843512	12.681920
20.817206	1302.779263	12.686925
20.774923	1295.433582	12.691930
20.826653	1307.172367	12.696935
20.915022	1332.447104	12.701939
21.271072	1323.292021	12.706944
20.892367	1317.662255	12.711949
20.734871	1307.324259	12.716954
20.984791	1299.909100	12.721959
20.855835	1306.746694	12.726963
20.741384	1306.404593	12.731968
20.764185	1321.284067	12.736973
21.119172	1318.670975	12.741978
21.032714	1328.935939	12.746983
20.784362	1310.759253	12.751987
21.308295	1313.572040	12.756992
20.855781	1305.101865	12.761997
20.937835	1298.021805	12.767002
21.026690	1301.600276	12.772007
20.769316	1297.092196	12.777011
20.898227	1296.698662	12.782016
20.734298	1303.506347	12.787021
20.972018	1287.447483	12.792026
20.931881	1296.578988	12.797031
20.735937	1305.039060	12.802035
20.907807	1309.839161	12.807040
20.927618	1314.452974	12.812045
21.075655	1307.274856	12.817050
20.852750	1312.193913	12.822055
20.757703	1307.113473	12.827059
21.136158	1304.700086	12.832064
20.597571	1308.272972	12.837069
20.823186	1319.186019	12.842074
21.188857	1334.910554	12.847079
21.123935	1322.408979	12.852083
21.348953	1309.567827	12.857088
21.167300	1319.800655	12.862093
21.206074	1314.178425	12.867098
21.266411	1307.945573	12.872103
21.138089	1310.122737	12.877107
21.440206	1306.235897	12.882112
21.005242	1308.164688	12.887117
21.071278	1300.694484	12.892122
20.862629	1291.411852	12.897127
20.718930	1283.596607	12.902131
21.204578	1282.764515	12.907136
21.190182	1284.954256	12.912141
20.897683	1273.247607	12.917146
20.473672	1274.613988	12.922151
20.882771	1276.323768	12.927155
20.713551	1289.915386	12.932160
20.725245	1305.593839	12.937165
20.987986	1305.879979	12.942170
21.120746	1307.051890	12.947175
20.653577	1307.224197	12.952179
20.860644	1309.250084	12.957184
20.909051	1308.761359	12.962189
21.123514	1308.213028	12.967194
21.061622	1304.684687	12.972199
20.922994	1294.118166	12.977203
20.788386	1286.091715	12.982208
20.875068	1305.291695	12.987213
21.176680	1307.101422	12.992218
20.818395	1286.563245	12.997223
20.754029	1292.948154	13.002227
21.118700	1296.622991	13.007232
21.026719	1289.362518	13.012237
20.948223	1285.096383	13.017242
20.681423	1292.405429	13.022247
20.878614	1299.530862	13.027251
21.045337	1294.867609	13.032256
20.850438	1298.044231	13.037261
20.777922	1279.785916	13.042266
21.108937	1296.230363	13.047271
20.929021	1306.298886	13.052275
20.891327	1284.602453	13.057280
20.907133	1294.051492	13.062285
21.061168	1292.582312	13.067290
21.138396	1292.815244	13.072295
20.518324	1285.448176	13.077299
20.664558	1281.001892	13.082304
20.836095	1306.034639	13.087309
21.117806	1313.336638	13.092314
21.380186	1301.840321	13.097319
21.126990	1293.466894	13.102323
21.152473	1285.787892	13.107328
21.203515	1289.938570	13.112333
20.951849	1282.948020	13.117338
21.203594	1280.165305	13.122343
20.881600	1288.487764	13.127347
21.152415	1280.238940	13.132352
20.979642	1290.581517	13.137357
21.118654	1283.514458	13.142362
21.250561	1282.280642	13.147367
21.014404	1285.083761	13.152371
21.248762	1281.518425	13.157376
20.942494	1272.178829	13.162381
20.808331	1254.847460	13.167386
20.791255	1254.931415	13.172391
20.732763	1256.116480	13.177395
20.934492	1273.627925	13.182400
20.499903	1279.924421	13.187405
21.058434	1284.567425	13.192410
20.944537	1284.619511	13.197415
20.956263	1291.619178	13.202419
20.600774	1286.573190	13.207424
21.008368	1293.030278	13.212429
21.019544	1288.532988	13.217434
20.733229	1294.585046	13.222439
20.611614	1289.068052	13.227443
20.951972	1288.889972	13.232448
21.010057	1289.766259	13.237453
20.747216	1293.542763	13.242458
21.070220	1288.834083	13.247463
20.822833	1296.321400	13.252467
21.119608	1285.731173	13.257472
20.896100	1300.194920	13.262477
20.762598	1290.494200	13.267482
20.658853	1292.426145	13.272487
20.415503	1299.963287	13.277491
21.007831	1299.021918	13.282496
21.019569	1307.236746	13.287501
21.219466	1294.232442	13.292506
21.010400	1297.912052	13.297511
20.876678	1308.272069	13.302515
21.136491	1300.663714	13.307520
20.893214	1313.022834	13.312525
21.171068	1296.575112	13.317530
20.915060	1297.396621	13.322535
20.853709	1299.212196	13.327539
21.084717	1292.091821	13.332544
20.860189	1300.703121	13.337549
20.963085	1291.638115	13.342554
21.207636	1303.454961	13.347559
20.819934	1292.962865	13.352563
21.099510	1276.372163	13.357568
20.474024	1279.674237	13.362573
20.798418	1287.654663	13.367578
20.592136	1295.748127	13.372583
20.437851	1301.507868	13.377587
21.134765	1298.698302	13.382592
21.127677	1304.611201	13.387597
20.422720	1300.089349	13.392602
20.928724	1296.773231	13.397607
20.804207	1303.050245	13.402611
21.501401	1298.587045	13.407616
20.963808	1310.516824	13.412621
20.875875	1300.821445	13.417626
21.135413	1293.628703	13.422631
21.089793	1308.601876	13.427635
21.150083	1299.973420	13.432640
20.582249	1302.237246	13.437645
20.616311	1303.754514	13.442650
21.090996	1299.803089	13.447655
20.991164	1301.971764	13.452659
21.323392	1296.851564	13.457664
20.862212	1301.511340	13.462669
20.826372	1285.636473	13.467674
20.937145	1283.131733	13.472679
20.594400	1295.768502	13.477683
21.205747	1295.604763	13.482688
20.979545	1296.888339	13.487693
21.001505	1293.313507	13.492698
20.892104	1282.852729	13.497703
20.746310	1279.445020	13.502707
20.996860	1280.939583	13.507712
20.850709	1292.868417	13.512717
20.918900	1300.628707	13.517722
20.753765	1301.865481	13.522727
20.436765	1298.921932	13.527731
20.940310	1291.933933	13.532736
21.034129	1307.719149	13.537741
21.122028	1312.744764	13.542746
21.192720	1305.617623	13.547751
20.720015	1296.914897	13.552755
20.886223	1294.264894	13.557760
20.837136	1305.859683	13.562765
20.886831	1300.952507	13.567770
21.179469	1304.028499	13.572775
20.889353	1310.905993	13.577779
21.343555	1294.834671	13.582784
20.867750	1288.362462	13.587789
20.831914	1279.880250	13.592794
20.717567	1280.612925	13.597799
20.899209	1274.306329	13.602803
21.079956	1277.986054	13.607808
20.801151	1282.522896	13.612813
20.811493	1275.590705	13.617818
21.022835	1278.536931	13.622823
20.376130	1281.932284	13.627827
20.923876	1297.984162	13.632832
20.933534	1301.952980	13.637837
21.249979	1310.880947	13.642842
21.093819	1289.886287	13.647847
20.757860	1292.240082	13.652851
21.069845	1279.566452	13.657856
20.608766	1290.240468	13.662861
21.085251	1287.260252	13.667866
21.322823	1293.622235	13.672871
20.915086	1294.990753	13.677875
20.755286	1284.443387	13.682880
20.710126	1290.088726	13.687885
20.694216	1278.542189	13.692890
21.013130	1286.195453	13.697895
20.877593	1291.907253	13.702899
20.781799	1280.559554	13.707904
20.772047	1301.605132	13.712909
21.037100	1315.651103	13.717914
21.300549	1306.232442	13.722919
20.916351	1303.994322	13.727923
21.135267	1284.367907	13.732928
21.202844	1289.358906	13.737933
21.045370	1282.686100	13.742938
20.878364	1290.456300	13.747943
20.792081	1289.359008	13.752947
21.026839	1275.321680	13.757952
20.648993	1286.888461	13.762957
20.724832	1286.759670	13.767962
20.948930	1280.243643	13.772967
20.610939	1286.910335	13.777971
21.031150	1280.415860	13.782976
20.980604	1289.288799	13.787981
20.943820	1288.408348	13.792986
20.853614	1289.554316	13.797991
20.727133	1287.711948	13.802995
20.954015	1280.676612	13.808000
20.997611	1287.477211	13.813005
20.830071	1284.957721	13.818010
21.223608	1281.889013	13.823015
21.143376	1285.185339	13.828019
21.256092	1289.602171	13.833024
20.767789	1287.268685	13.838029
20.913790	1290.574663	13.843034
20.862809	1289.008861	13.848039
20.548390	1287.088439	13.853043
21.047196	1289.746731	13.858048
20.779396	1301.036538	13.863053
20.761305	1291.562647	13.868058
20.904767	1291.316616	13.873063
20.977139	1290.274450	13.878067
21.095157	1286.657488	13.883072
20.701322	1281.758768	13.888077
21.147102	1285.844904	13.893082
20.882865	1280.639270	13.898087
20.917387	1291.323344	13.903091
20.872496	1294.095169	13.908096
20.876380	1292.015156	13.913101
20.533046	1282.116866	13.918106
20.756616	1292.429344	13.923111
20.961583	1292.705774	13.928115
20.935034	1289.880705	13.933120
21.035933	1286.306689	13.938125
21.082385	1288.780066	13.943130
20.848164	1289.882766	13.948135
20.705530	1292.784521	13.953139
21.043237	1284.294769	13.958144
21.080867	1296.435589	13.963149
21.139802	1299.723914	13.968154
20.959073	1294.993067	13.973159
20.681343	1290.502430	13.978163
21.098935	1295.376095	13.983168
20.898902	1296.466246	13.988173
20.955712	1298.042180	13.993178
21.008763	1290.517277	13.998183
20.955984	1305.239252	14.003187
21.101303	1286.150537	14.008192
21.257366	1298.425913	14.013210
20.845521	1294.061047	14.018227
20.618920	1293.132120	14.023245
20.844568	1295.717670	14.028263
21.156463	1293.075504	14.033280
21.020417	1296.377864	14.038298
21.010618	1292.882492	14.043315
21.094404	1291.490338	14.048333
20.839965	1301.991100	14.053351
20.996088	1291.847399	14.058368
21.009121	1295.575094	14.063386
20.766436	1295.646062	14.068403
20.856082	1296.442695	14.073421
20.763173	1297.112711	14.078439
20.914507	1310.212761	14.083456
20.927433	1323.941321	14.088474
20.940339	1325.401450	14.093491
21.010648	1328.439660	14.098509
21.086690	1337.549831	14.103527
21.539409	1324.472198	14.108544
21.270715	1330.742887	14.113562
21.143949	1335.973944	14.118579
21.409905	1327.914334	14.123597
21.141170	1333.016233	14.128615
21.030286	1328.943137	14.133632
21.085479	1338.895086	14.138650
20.915908	1327.809910	14.143667
21.440462	1322.730941	14.148685
21.156284	1340.163527	14.153703
21.389226	1331.699393	14.158720
21.584591	1340.812557	14.163738
21.272044	1340.963098	14.168755
21.669065	1348.323151	14.173773
21.454029	1352.006224	14.178791
21.410800	1358.576029	14.183808
21.829359	1362.820311	14.188826
21.392632	1354.337919	14.193843
21.377031	1351.023576	14.198861
21.349746	1367.872506	14.203879
21.563554	1371.180430	14.208896
21.663982	1370.399904	14.213914
21.665645	1367.985753	14.218931
21.972904	1360.072127	14.223949
21.710182	1364.672051	14.228967
21.917101	1366.120902	14.233984
21.748469	1368.368218	14.239002
21.771963	1364.855719	14.244019
21.915318	1355.610668	14.249037
21.539619	1366.580719	14.254055
21.762881	1360.485604	14.259072
22.295015	1363.605894	14.264090
21.565416	1356.099907	14.269107
21.822549	1361.408958	14.274125
21.722848	1367.448207	14.279143
21.993068	1368.919210	14.284160
21.967545	1376.948380	14.289178
21.988976	1375.330202	14.294195
22.012962	1369.841830	14.299213
21.875090	1378.370284	14.304231
21.930861	1375.148375	14.309248
22.274772	1362.128177	14.314266
21.960578	1363.540593	14.319283
21.807685	1359.161146	14.324301
21.818389	1371.336686	14.329319
21.717501	1364.416278	14.334336
21.771643	1366.122314	14.339354
22.102905	1377.185684	14.344371
22.067185	1367.457937	14.349389
21.794560	1379.683395	14.354407
21.771706	1373.828885	14.359424
22.065079	1367.277401	14.364442
21.977375	1377.277338	14.369459
22.116147	1379.895637	14.374477
22.085304	1394.756787	14.379495
22.376434	1405.132849	14.384512
22.522132	1410.786894	14.389530
22.127711	1391.085552	14.394547
22.573378	1393.618722	14.399565
22.306742	1383.239570	14.404583
22.056606	1378.608204	14.409600
22.495134	1396.876513	14.414618
22.420870	1398.812254	14.419635
22.522159	1395.498920	14.424653
22.414486	1393.936727	14.429671
22.282525	1399.658652	14.434688
22.759573	1401.382184	14.439706
22.091275	1398.155419	14.444723
22.522167	1402.165716	14.449741
22.751215	1406.982954	14.454759
22.519003	1410.860698	14.459776
22.699287	1416.998460	14.464794
22.479867	1411.334170	14.469811
22.720134	1417.601582	14.474829
22.711436	1411.208377	14.479847
22.342270	1420.886707	14.484864
22.772773	1410.728262	14.489882
22.567654	1419.062178	14.494899
22.770344	1415.849861	14.499917
22.567051	1411.577541	14.504935
22.535823	1419.642253	14.509952
22.515728	1402.229025	14.514970
22.510529	1423.741061	14.519987
22.748231	1410.527753	14.525005
22.538993	1427.561510	14.530023
22.600905	1412.575839	14.535040
22.635889	1412.561618	14.540058
22.482881	1413.275047	14.545075
22.508379	1423.944399	14.550093
23.125940	1430.464683	14.555111
23.058883	1437.469350	14.560128
23.365654	1446.288733	14.565146
22.977608	1425.533929	14.570163
22.949998	1420.735702	14.575181
22.837896	1420.965961	14.580199
22.965203	1422.507744	14.585216
22.804160	1428.014872	14.590234
22.731044	1447.889178	14.595251
23.141665	1433.419684	14.600269
23.322212	1441.620523	14.605287
23.412211	1451.725093	14.610304
23.269622	1436.650100	14.615322
23.250931	1446.627278	14.620339
23.196443	1433.356731	14.625357
23.044807	1433.220474	14.630375
22.936602	1448.452682	14.635392
23.175572	1438.239821	14.640410
22.829395	1441.372015	14.645427
22.950335	1451.331644	14.650445
23.262055	1451.421940	14.655463
23.297396	1445.948246	14.660480
23.424203	1447.019757	14.665498
23.282877	1437.411058	14.670515
23.083310	1455.779646	14.675533
23.372304	1444.797424	14.680551
23.372464	1455.730401	14.685568
23.664344	1445.295942	14.690586
23.099144	1455.581315	14.695603
23.112451	1445.363542	14.700621
23.316977	1457.819711	14.705639
23.227361	1473.175615	14.710656
23.532761	1475.463746	14.715674
23.531696	1480.873015	14.720691
23.620647	1485.185639	14.725709
23.754122	1482.303685	14.730727
23.392474	1487.966321	14.735744
23.646008	1472.905977	14.740762
23.853064	1485.220188	14.745779
23.646697	1476.992790	14.750797
24.023545	1474.341806	14.755815
24.070614	1478.156930	14.760832
24.233711	1466.062145	14.765850
23.854937	1449.704199	14.770867
23.830181	1441.811238	14.775885
23.936282	1436.128052	14.780903
23.965803	1439.473251	14.785920
23.979022	1426.929690	14.790938
23.718838	1439.977514	14.795955
23.994214	1434.870608	14.800973
24.288908	1437.394046	14.805991
23.867741	1443.449992	14.811008
24.023648	1436.099250	14.816026
24.111525	1435.890182	14.821043
24.160772	1440.093502	14.826061
23.961133	1441.352367	14.831079
24.077661	1446.929279	14.836096
24.325395	1439.428603	14.841114
24.227733	1443.605018	14.846131
23.869812	1441.159330	14.851149
23.928874	1439.101756	14.856167
23.935324	1442.964250	14.861184
24.248589	1430.877004	14.866202
23.927453	1435.421770	14.871219
24.162255	1431.526325	14.876237
24.174197	1438.136918	14.881255
23.855056	1434.738831	14.886272
24.164880	1453.695518	14.891290
24.210692	1461.874598	14.896307
24.289737	1478.737372	14.901325
24.450955	1463.340176	14.906343
24.231167	1472.986849	14.911360
24.687985	1469.704097	14.916378
24.269800	1467.550387	14.921395
24.686155	1462.848868	14.926413
24.361949	1454.824330	14.931431
24.031604	1453.643727	14.936448
24.392230	1458.353476	14.941466
24.416789	1466.755395	14.946483
24.537522	1472.112199	14.951501
24.550148	1470.306643	14.956519
24.503444	1471.069976	14.961536
24.776709	1470.395590	14.966554
24.762463	1467.486862	14.971571
24.525998	1470.423016	14.976589
24.642510	1476.025898	14.981607
24.126021	1472.767036	14.986624
24.322550	1469.053873	14.991642
24.472709	1483.942089	14.996659
24.080463	1479.385268	15.001677
24.608560	1471.418268	15.006695
24.637502	1497.777965	15.011712
24.784403	1501.613353	15.016730
24.749552	1512.706121	15.021747
25.081004	1505.044974	15.026765
25.393588	1507.524669	15.031783
24.813032	1491.868213	15.036800
25.064402	1475.170618	15.041818
24.733516	1479.725605	15.046835
24.703981	1479.074346	15.051853
25.165841	1487.834410	15.056871
24.794857	1501.486725	15.061888
24.913569	1508.675737	15.066906
25.050543	1507.874431	15.071923
25.019561	1506.955188	15.076941
25.168800	1502.329297	15.081959
24.726648	1509.428435	15.086976
24.814214	1510.920721	15.091994
25.117579	1508.918557	15.097011
25.064637	1505.603842	15.102029
25.320066	1508.585820	15.107047
25.449739	1512.696892	15.112064
25.487468	1502.376079	15.117082
25.286982	1504.913226	15.122099
24.680625	1517.280123	15.127117
25.546577	1500.460090	15.132135
25.236452	1507.995154	15.137152
25.174309	1510.011564	15.142170
25.506300	1512.605361	15.147187
25.291521	1518.349980	15.152205
25.741381	1502.246788	15.157223
25.209624	1509.814844	15.162240
25.413320	1510.004959	15.167258
25.438742	1515.870934	15.172275
25.391926	1505.734285	15.177293
25.770870	1493.764718	15.182311
25.490891	1507.280609	15.187328
25.533501	1506.782230	15.192346
25.614863	1499.227046	15.197363
25.376966	1509.250242	15.202381
25.633173	1502.445065	15.207399
25.450666	1498.649986	15.212416
25.415397	1498.077509	15.217434
25.948616	1502.036119	15.222451
25.636627	1502.555462	15.227469
25.669982	1500.090615	15.232487
25.365051	1507.135617	15.237504
25.643445	1515.910802	15.242522
25.459935	1521.016476	15.247539
25.515414	1539.147851	15.252557
26.011585	1531.594131	15.257575
26.031127	1545.138578	15.262592
26.134612	1540.962800	15.267610
26.525214	1535.931081	15.272627
26.151725	1523.854191	15.277645
26.105839	1508.618188	15.282663
26.134296	1512.345837	15.287680
25.605487	1499.456066	15.292698
25.811006	1503.033556	15.297715
25.827671	1530.777237	15.302733
26.115884	1527.136743	15.307751
25.924110	1536.152109	15.312768
26.280878	1530.727007	15.317786
26.359872	1535.369225	15.322803
26.306647	1539.861852	15.327821
26.561100	1541.866310	15.332839
26.113173	1535.569850	15.337856
26.199798	1520.040553	15.342874
26.464970	1524.252718	15.347891
25.878633	1534.567473	15.352909
26.133046	1530.481675	15.357927
26.081320	1542.542255	15.362944
26.224077	1532.980994	15.367962
26.540456	1535.864376	15.372979
26.472764	1543.827214	15.377997
26.657919	1542.593483	15.383015
26.635006	1535.598419	15.388032
26.640436	1536.086798	15.393050
26.635510	1531.355707	15.398067
26.252956	1535.474550	15.403085
26.282042	1537.017854	15.408103
26.241554	1527.132663	15.413120
26.364037	1539.679071	15.418138
26.363126	1530.095894	15.423155
26.554238	1537.056284	15.428173
26.663492	1533.979187	15.433191
26.589533	1542.827107	15.438208
26.478939	1549.377854	15.443226
26.664737	1534.870184	15.448243
26.073777	1539.887475	15.453261
26.589089	1539.003798	15.458279
26.930862	1550.150572	15.463296
26.775552	1564.183059	15.468314
26.913153	1563.665594	15.473331
26.822888	1570.160408	15.478349
26.885281	1571.667728	15.483367
27.068348	1566.219979	15.488384
26.793070	1576.298736	15.493402
27.395897	1560.897070	15.498419
26.875995	1568.942276	15.503437
26.868659	1571.553238	15.508455
27.038022	1563.499468	15.513472
27.051030	1567.264990	15.518490
27.058317	1563.710195	15.523507
27.127167	1571.423957	15.528525
26.931865	1564.873247	15.533543
27.251323	1565.553798	15.538560
26.824364	1566.841066	15.543578
27.151761	1564.101994	15.548595
27.159715	1570.605526	15.553613
26.789389	1559.883331	15.558631
27.050666	1566.309487	15.563648
27.307537	1565.883117	15.568666
27.519177	1561.420295	15.573683
26.962064	1561.888285	15.578701
27.288547	1560.533691	15.583719
27.474496	1559.328934	15.588736
27.194858	1572.323346	15.593754
27.284229	1561.244670	15.598771
27.279221	1589.846903	15.603789
27.092056	1593.106357	15.608807
27.800009	1589.389459	15.613824
27.563854	1599.227599	15.618842
27.830063	1587.113121	15.623859
27.384599	1602.907398	15.628877
27.831068	1599.331311	15.633895
27.929404	1590.658825	15.638912
27.731195	1597.122101	15.643930
27.844673	1585.186150	15.648947
27.585045	1586.310657	15.653965
27.807647	1582.459592	15.658983
27.671845	1580.462968	15.664000
27.895978	1580.442174	15.669018
27.812501	1577.882685	15.674035
27.311199	1582.342182	15.679053
27.726826	1591.057770	15.684071
27.960498	1593.804124	15.689088
27.565675	1599.285681	15.694106
27.806607	1592.261877	15.699123
27.761458	1595.586774	15.704141
27.679112	1601.154565	15.709159
27.722087	1596.414238	15.714176
27.840894	1596.083824	15.719194
27.883103	1590.045022	15.724211
27.632533	1599.584211	15.729229
27.862176	1612.124601	15.734247
27.992350	1619.170260	15.739264
27.776111	1628.351615	15.744282
28.327344	1619.790142	15.749299
28.054993	1635.270535	15.754317
28.125269	1629.755019	15.759335
28.430704	1625.857696	15.764352
28.204193	1626.000807	15.769370
28.368105	1618.828818	15.774387
28.288234	1634.174684	15.779405
28.039127	1630.427161	15.784423
28.334713	1624.232307	15.789440
27.951645	1632.810243	15.794458
28.000869	1623.522619	15.799475
28.310446	1630.567984	15.804493
28.403434	1631.228815	15.809511
28.697632	1639.438381	15.814528
28.668705	1636.635001	15.819546
29.199767	1610.671845	15.824563
28.942406	1619.428721	15.829581
28.989337	1617.305414	15.834599
29.070092	1614.361053	15.839616
28.802186	1608.344964	15.844634
29.100955	1613.321047	15.849651
29.100787	1603.841527	15.854669
28.854659	1586.967526	15.859687
28.704143	1570.364599	15.864704
28.644668	1580.635465	15.869722
28.748975	1572.756456	15.874739
28.985577	1595.664851	15.879757
29.297331	1593.266487	15.884775
29.129401	1575.987535	15.889792
29.011298	1576.690685	15.894810
28.788159	1569.264260	15.899827
29.259196	1571.522056	15.904845
28.938776	1571.273498	15.909863
29.212786	1571.942421	15.914880
29.363587	1576.027331	15.919898
29.349569	1564.162859	15.924915
29.537801	1573.032689	15.929933
28.948904	1572.447048	15.934951
29.239111	1563.334967	15.939968
29.179002	1577.026648	15.944986
29.305943	1565.603758	15.950003
29.527975	1565.081479	15.955021
29.123874	1569.854248	15.960039
29.284801	1565.975270	15.965056
28.645653	1570.190108	15.970074
29.395125	1572.456193	15.975091
29.531259	1581.544348	15.980109
29.533781	1574.138560	15.985127
29.714856	1564.333627	15.990144
29.536097	1575.760871	15.995162
29.370545	1568.408637	16.000179
29.460499	1567.518081	16.005197
29.528057	1573.500847	16.010215
29.967790	1564.152547	16.015232
29.626411	1568.598330	16.020250
29.718338	1569.639233	16.025267
29.638650	1573.635844	16.030285
29.207033	1565.980751	16.035303
29.619790	1569.214515	16.040320
29.480055	1574.404465	16.045338
29.269351	1573.964579	16.050355
29.419943	1572.217234	16.055373
29.440951	1570.012333	16.060391
29.620998	1572.834094	16.065408
29.282584	1578.937460	16.070426
29.684333	1593.930386	16.075443
29.934081	1601.843411	16.080461
29.679622	1607.430005	16.085479
29.877688	1594.021496	16.090496
29.970324	1589.067174	16.095514
30.139529	1593.557375	16.100531
30.133460	1590.560011	16.105549
29.707511	1592.762668	16.110567
30.311025	1594.789328	16.115584
30.082570	1601.564187	16.120602
30.259476	1598.077502	16.125619
30.117409	1599.418438	16.130637
29.978493	1598.447188	16.135655
30.269961	1589.888624	16.140672
30.234294	1597.295796	16.145690
30.462756	1596.872383	16.150707
30.269732	1593.012885	16.155725
30.098994	1599.665274	16.160743
30.562333	1597.602974	16.165760
30.114184	1605.151450	16.170778
30.462814	1596.084302	16.175795
30.389373	1599.224939	16.180813
30.296093	1596.756677	16.185831
30.556286	1592.534653	16.190848
30.350157	1593.771756	16.195866
30.672205	1591.769747	16.200883
30.581795	1594.792747	16.205901
30.506267	1607.245734	16.210919
30.561152	1600.452173	16.215936
30.503418	1597.013925	16.220954
30.483692	1596.258845	16.225971
30.658142	1589.112719	16.230989
30.314571	1603.027398	16.236007
30.340051	1591.586849	16.241024
30.351906	1598.329669	16.246042
30.450340	1617.801659	16.251059
30.825876	1623.316876	16.256077
31.046569	1628.516215	16.261095
31.005262	1628.479554	16.266112
31.150874	1629.360093	16.271130
30.789692	1634.284920	16.276147
31.121032	1625.586261	16.281165
30.950712	1637.755502	16.286183
31.433463	1625.965124	16.291200
31.097001	1605.735117	16.296218
30.846351	1608.006562	16.301235
30.407265	1605.512440	16.306253
30.715828	1628.862465	16.311271
31.195946	1621.061135	16.316288
30.946782	1628.461475	16.321306
30.705202	1635.440587	16.326323
30.977671	1624.921002	16.331341
30.587834	1636.363869	16.336359
30.705592	1638.857359	16.341376
31.210869	1638.444852	16.346394
31.186632	1654.364705	16.351411
31.226143	1659.794311	16.356429
31.284973	1665.472537	16.361447
31.528172	1661.174549	16.366464
30.966874	1656.886108	16.371482
31.352852	1651.503497	16.376499
31.354637	1661.203834	16.381517
31.261491	1662.222349	16.386535
31.487115	1657.491412	16.391552
31.561125	1668.459963	16.396570
31.687536	1683.673874	16.401587
31.998378	1685.125060	16.406605
31.490621	1667.362982	16.411623
31.840497	1676.091469	16.416640
32.008912	1683.013076	16.421658
31.865876	1671.060550	16.426675
31.951816	1663.953675	16.431693
31.597999	1656.487484	16.436711
31.426512	1661.812311	16.441728
31.963512	1676.070342	16.446746
32.179684	1683.202995	16.451763
32.291919	1686.685292	16.456781
31.864615	1670.020999	16.461799
31.873370	1653.172338	16.466816
32.129928	1669.224395	16.471834
31.871279	1678.691774	16.476851
32.335509	1667.908752	16.481869
31.854505	1678.489967	16.486887
31.896317	1681.664152	16.491904
32.160131	1687.951524	16.496922
32.152386	1688.722025	16.501939
32.160941	1682.016044	16.506957
32.277381	1686.506825	16.511975
32.226786	1679.631730	16.516992
32.268314	1679.546462	16.522010
32.146412	1679.852224	16.527027
32.504324	1685.017898	16.532045
32.206501	1684.960799	16.537063
32.262235	1683.031144	16.542080
32.537985	1672.465381	16.547098
32.260652	1689.331756	16.552115
32.588444	1684.783514	16.557133
32.152819	1690.565784	16.562151
32.615041	1682.827841	16.567168
32.500381	1680.770412	16.572186
32.086344	1679.673142	16.577203
32.669554	1685.420330	16.582221
32.703061	1703.637217	16.587239
32.861502	1698.613370	16.592256
32.764813	1693.926751	16.597274
32.605011	1692.615886	16.602291
32.777151	1701.273631	16.607309
32.469607	1711.023339	16.612327
32.518203	1707.609007	16.617344
32.803995	1700.279890	16.622362
32.638499	1707.596135	16.627379
33.016746	1707.783582	16.632397
32.859808	1716.891823	16.637415
32.487138	1710.927795	16.642432
32.682802	1712.232964	16.647450
32.995109	1723.769987	16.652467
33.133097	1736.204760	16.657485
32.961929	1745.964202	16.662503
32.834846	1747.968979	16.667520
33.238431	1745.437173	16.672538
33.195934	1752.121876	16.677555
33.315485	1739.600414	16.682573
33.039917	1747.641354	16.687591
33.298117	1748.907449	16.692608
33.401129	1746.686296	16.697626
33.316888	1746.508609	16.702643
33.398767	1744.326222	16.707661
33.435675	1752.472278	16.712679
33.330491	1749.586650	16.717696
33.587473	1751.469605	16.722714
33.467863	1749.530153	16.727731
33.607143	1736.637436	16.732749
33.758192	1737.894664	16.737767
33.522538	1743.268297	16.742784
33.933297	1743.398647	16.747802
33.751275	1741.312625	16.752819
33.535382	1740.114528	16.757837
33.539115	1735.794934	16.762855
33.695517	1735.090410	16.767872
33.821417	1735.090791	16.772890
33.302238	1739.543747	16.777907
33.363730	1744.880998	16.782925
33.858059	1751.232311	16.787943
33.914149	1772.134152	16.792960
34.112297	1765.990175	16.797978
33.942054	1763.276167	16.802995
33.983429	1767.113513	16.808013
33.880127	1765.065272	16.813031
34.332693	1768.276215	16.818048
34.338126	1757.690581	16.823066
33.734923	1761.526908	16.828083
34.115299	1768.332946	16.833101
34.265673	1759.543514	16.838119
33.990706	1778.969089	16.843136
34.329793	1762.234366	16.848154
34.101320	1761.647074	16.853171
34.298057	1766.250135	16.858189
34.027468	1761.824054	16.863207
34.346903	1768.714535	16.868224
34.634115	1767.848351	16.873242
34.135589	1769.293350	16.878259
34.661091	1756.707912	16.883277
34.590688	1762.623880	16.888295
34.335855	1763.842807	16.893312
34.617044	1761.033201	16.898330
34.615641	1759.574361	16.903347
34.674539	1756.543004	16.908365
34.730731	1756.379887	16.913383
34.451392	1754.138701	16.918400
34.681500	1761.073316	16.923418
34.111096	1765.642995	16.928435
34.497767	1772.753218	16.933453
34.755918	1788.858640	16.938471
34.861002	1793.341040	16.943488
34.965251	1791.707247	16.948506
35.124854	1800.915286	16.953523
35.390131	1792.695071	16.958541
34.966626	1776.410747	16.963559
35.095587	1774.235005	16.968576
35.365162	1785.334484	16.973594
34.791295	1776.695952	16.978611
34.994724	1776.082246	16.983629
35.045152	1788.344613	16.988647
34.615458	1787.587267	16.993664
35.162485	1782.982004	16.998682
35.005459	1795.910650	17.003699
35.166091	1786.340080	17.008717
35.174998	1787.712012	17.013735
34.937926	1789.079129	17.018752
35.763496	1799.102014	17.023770
35.393023	1804.556165	17.028787
35.172197	1799.759528	17.033805
35.089841	1801.644700	17.038823
35.172530	1793.316745	17.043840
35.751817	1806.257743	17.048858
35.709421	1825.088611	17.053875
35.316073	1806.159727	17.058893
35.468680	1812.438934	17.063911
35.387323	1820.190157	17.068928
35.755599	1823.197464	17.073946
35.439525	1824.950017	17.078963
35.863484	1821.081720	17.083981
36.027697	1817.157318	17.088999
35.937780	1824.346727	17.094016
35.853200	1814.840419	17.099034
35.752048	1824.292997	17.104051
35.952032	1825.211284	17.109069
35.865889	1816.841812	17.114087
36.057887	1817.560798	17.119104
35.996802	1810.586634	17.124122
36.187964	1818.721495	17.129139
35.962043	1819.183072	17.134157
36.089275	1811.018688	17.139175
36.156602	1814.895955	17.144192
36.001053	1818.205475	17.149210
36.045026	1820.568396	17.154227
36.095246	1819.615731	17.159245
36.183870	1810.906122	17.164263
36.128442	1819.961267	17.169280
36.153510	1807.916531	17.174298
36.528820	1808.878430	17.179315
36.299916	1805.247196	17.184333
36.556702	1811.126729	17.189351
36.122438	1814.826791	17.194368
36.354093	1816.961563	17.199386
36.308360	1826.087530	17.204403
36.574072	1843.044444	17.209421
36.957949	1840.868935	17.214439
36.572337	1842.193677	17.219456
36.609629	1841.149472	17.224474
36.631269	1850.289092	17.229491
36.673990	1848.397673	17.234509
37.146505	1845.997226	17.239527
36.889810	1847.571199	17.244544
36.824055	1834.142410	17.249562
36.408012	1840.985054	17.254579
36.685226	1841.743936	17.259597
36.767306	1850.329611	17.264615
36.744924	1851.136278	17.269632
37.233834	1844.807457	17.274650
37.155415	1853.026236	17.279667
36.952694	1855.232654	17.284685
37.080562	1847.336368	17.289703
37.220689	1845.466382	17.294720
37.382881	1850.757721	17.299738
37.347813	1851.103909	17.304755
37.259914	1845.395661	17.309773
37.572424	1838.189638	17.314791
37.040138	1853.868248	17.319808
37.302933	1850.645464	17.324826
37.341992	1851.842694	17.329843
37.203653	1848.755467	17.334861
37.297544	1843.137783	17.339879
37.387281	1851.193665	17.344896
37.306229	1842.489862	17.349914
37.569285	1846.252543	17.354931
37.303221	1847.259322	17.359949
37.626962	1846.409332	17.364967
37.443259	1844.400646	17.369984
37.193068	1850.879405	17.375002
37.613346	1864.896672	17.380019
37.515063	1871.230865	17.385037
37.596690	1864.513146	17.390055
37.864273	1871.257780	17.395072
37.987743	1873.716576	17.400090
37.982690	1872.867899	17.405107
37.787590	1870.906649	17.410125
38.160602	1867.979336	17.415143
37.855401	1874.159330	17.420160
37.834790	1872.283515	17.425178
37.888664	1871.944575	17.430195
37.688478	1880.150541	17.435213
37.693157	1871.936451	17.440231
38.216084	1884.184103	17.445248
38.259715	1885.836818	17.450266
38.225787	1889.376298	17.455283
38.377792	1895.342582	17.460301
38.344116	1893.580541	17.465319
38.336693	1885.251962	17.470336
38.704593	1888.840618	17.475354
38.443635	1875.957341	17.480371
38.163311	1871.506821	17.485389
38.426720	1872.276559	17.490407
38.300579	1891.297060	17.495424
38.654512	1898.827090	17.500442
38.756837	1902.572947	17.505459
38.753141	1902.128348	17.510477
38.891976	1892.379488	17.515495
38.783497	1903.088651	17.520512
38.438711	1890.520775	17.525530
38.679966	1895.337017	17.530547
38.700130	1896.873917	17.535565
38.703271	1895.909878	17.540583
38.436844	1890.083785	17.545600
38.596084	1892.468448	17.550618
38.702368	1897.595676	17.555635
38.407664	1908.781317	17.560653
39.032201	1907.307578	17.565671
39.046646	1921.198492	17.570688
38.845405	1932.229235	17.575706
39.222027	1925.066431	17.580723
38.901033	1923.191326	17.585741
39.061670	1920.999497	17.590759
38.880841	1931.854725	17.595776
38.896963	1933.364743	17.600794
39.060321	1925.820644	17.605811
39.077630	1929.223751	17.610829
39.278222	1920.618136	17.615847
39.295690	1933.618181	17.620864
39.379357	1925.043011	17.625882
39.682412	1930.941170	17.630899
39.362147	1934.109448	17.635917
39.569162	1931.763919	17.640935
39.368541	1944.315015	17.645952
39.258667	1957.137962	17.650970
39.725044	1961.591892	17.655987
39.838681	1959.270691	17.661005
39.956915	1962.284086	17.666023
39.893381	1959.018938	17.671040
39.866206	1958.476614	17.676058
40.052225	1952.271568	17.681075
39.945312	1955.686628	17.686093
40.054804	1957.185690	17.691111
39.825654	1953.917854	17.696128
39.861273	1957.868649	17.701146
39.934879	1953.467054	17.706163
39.641971	1957.006955	17.711181
40.148324	1953.786991	17.716199
40.237298	1955.622045	17.721216
39.937030	1955.551961	17.726234
40.272893	1948.644205	17.731251
40.038975	1952.601019	17.736269
40.380333	1955.819517	17.741287
40.129615	1954.477507	17.746304
40.269385	1955.613061	17.751322
40.392927	1959.195875	17.756339
40.054800	1956.214428	17.761357
40.453750	1948.437671	17.766375
40.363738	1958.227572	17.771392
40.531280	1961.568183	17.776410
40.699752	1970.879530	17.781427
40.684929	1986.065156	17.786445
40.681009	1985.958818	17.791463
40.860531	1987.139948	17.796480
40.717406	1983.917379	17.801498
40.772989	1976.071881	17.806515
40.668472	1979.546344	17.811533
40.925948	1983.163648	17.816551
40.674163	1978.515832	17.821568
40.623780	1986.075784	17.826586
41.220409	1981.387825	17.831603
40.898557	1986.955420	17.836621
41.066562	1984.675884	17.841639
41.176248	1987.112515	17.846656
41.002242	1980.245950	17.851674
41.198949	1984.911226	17.856691
40.783149	1980.294289	17.861709
41.086172	1976.405125	17.866727
41.493994	1965.029940	17.871744
41.345172	1976.588798	17.876762
41.526707	1967.341205	17.881779
41.380555	1967.473860	17.886797
41.386453	1974.634689	17.891815
41.455222	1973.872554	17.896832
41.193005	1973.958435	17.901850
41.384531	1966.792884	17.906867
41.266574	1972.180078	17.911885
41.149121	1968.191226	17.916903
41.430772	1979.465121	17.921920
41.478294	1994.903528	17.926938
41.468849	2004.399802	17.931955
41.664143	2003.826714	17.936973
41.653146	2007.064454	17.941991
41.631304	1998.440783	17.947008
41.427970	2007.716279	17.952026
41.771514	2003.938632	17.957043
41.483097	2008.048883	17.962061
41.943513	2020.316847	17.967079
42.331255	2020.918886	17.972096
42.060805	2022.406974	17.977114
42.335268	2018.741023	17.982131
42.276264	2013.529149	17.987149
42.154887	1998.265345	17.992167
42.307316	2002.365849	17.997184
42.134135	1996.705751	18.002202
42.542079	2002.374049	18.007219
42.216230	1996.772124	18.012237
42.198975	2004.569068	18.017255
42.905871	2012.417271	18.022272
42.560121	2011.133674	18.027290
42.283681	2000.783959	18.032307
42.506473	2011.444299	18.037325
42.562532	2023.789343	18.042343
42.986807	2024.396568	18.047360
42.581047	2010.709574	18.052378
42.881310	2017.158817	18.057395
42.634596	2018.353659	18.062413
42.536216	2017.447494	18.067431
42.676009	2022.243779	18.072448
42.730917	2027.722981	18.077466
42.897021	2025.866921	18.082483
42.916585	2030.772054	18.087501
42.655262	2040.571242	18.092519
42.570158	2030.621246	18.097536
42.791634	2033.434917	18.102554
42.851051	2027.161935	18.107571
42.875222	2032.468276	18.112589
42.717733	2057.156566	18.117607
43.123025	2045.933531	18.122624
43.050299	2078.733694	18.127642
43.182367	2060.791212	18.132659
43.471026	2067.603369	18.137677
43.364371	2062.012867	18.142695
43.695430	2067.319041	18.147712
43.485778	2067.711171	18.152730
43.648093	2067.907109	18.157747
43.499882	2065.004683	18.162765
43.355808	2065.675028	18.167783
43.516392	2057.423383	18.172800
43.402269	2056.997179	18.177818
43.481369	2061.494818	18.182835
43.707088	2056.652044	18.187853
43.822609	2062.551851	18.192871
43.690196	2059.085289	18.197888
43.490521	2065.274489	18.202906
43.826471	2049.637217	18.207923
43.565697	2061.061402	18.212941
43.718478	2070.781977	18.217959
43.955713	2068.172822	18.222976
44.096990	2079.333105	18.227994
44.143443	2081.633533	18.233011
44.327115	2080.223015	18.238029
44.108857	2082.582182	18.243047
44.331861	2081.854434	18.248064
44.589008	2076.140617	18.253082
44.531094	2074.196787	18.258099
44.166971	2081.063510	18.263117
44.198101	2077.056437	18.268135
44.465403	2073.176092	18.273152
44.112440	2079.125455	18.278170
44.360088	2074.270525	18.283187
44.722604	2070.052497	18.288205
44.720178	2065.223298	18.293223
45.079618	2059.514409	18.298240
45.035952	2075.346577	18.303258
44.863030	2074.209243	18.308275
44.891135	2063.714947	18.313293
44.756240	2066.468263	18.318311
45.162011	2060.678046	18.323328
44.923341	2064.440576	18.328346
45.141421	2056.413374	18.333363
45.052777	2060.435930	18.338381
44.988503	2064.437295	18.343399
45.002447	2063.097898	18.348416
44.630677	2065.557844	18.353434
45.024985	2061.145182	18.358451
45.220287	2065.487424	18.363469
44.789162	2064.389700	18.368487
45.043640	2061.489908	18.373504
45.117143	2072.008921	18.378522
44.959053	2064.391741	18.383539
45.015922	2069.360943	18.388557
45.031033	2084.705506	18.393575
45.515518	2093.737635	18.398592
45.138227	2094.718908	18.403610
45.111302	2101.176324	18.408627
45.416987	2092.039424	18.413645
45.193990	2100.345901	18.418663
45.534471	2103.683346	18.423680
45.210159	2110.502044	18.428698
45.529660	2130.866841	18.433715
45.986242	2132.973651	18.438733
45.920007	2128.875118	18.443751
45.906636	2133.248303	18.448768
46.034659	2128.819884	18.453786
46.227158	2126.340561	18.458803
46.342437	2125.231196	18.463821
45.888078	2137.186582	18.468839
46.088301	2126.695466	18.473856
46.086221	2126.263189	18.478874
46.167989	2129.181752	18.483891
46.444478	2121.228577	18.488909
46.321641	2126.622112	18.493927
46.151770	2124.550614	18.498944
46.240677	2130.183322	18.503962
46.335665	2124.142960	18.508979
46.472923	2119.253708	18.513997
46.227849	2132.715052	18.519015
46.453716	2116.583987	18.524032
46.144755	2127.203369	18.529050
46.373341	2122.943761	18.534067
46.214802	2114.773658	18.539085
46.167140	2132.967844	18.544103
46.432638	2151.510118	18.549120
46.343992	2162.914008	18.554138
46.563223	2155.607081	18.559155
46.662690	2157.542743	18.564173
46.866434	2154.019398	18.569191
46.751274	2150.240936	18.574208
46.858996	2164.271375	18.579226
47.254511	2175.261396	18.584243
47.226500	2184.593992	18.589261
47.233221	2191.739065	18.594279
47.393955	2177.114408	18.599296
47.211038	2170.205126	18.604314
47.170501	2177.603930	18.609331
47.585677	2171.107389	18.614349
47.350022	2175.215564	18.619367
47.279833	2175.875702	18.624384
47.499889	2175.932647	18.629402
47.624796	2179.918029	18.634419
47.278256	2176.122975	18.639437
47.636559	2178.298955	18.644455
47.730452	2175.149449	18.649472
48.100040	2176.220050	18.654490
47.880785	2186.232082	18.659507
48.081204	2168.066189	18.664525
47.621097	2165.350354	18.669543
48.134237	2165.425053	18.674560
48.037935	2158.903906	18.679578
47.781908	2156.972785	18.684595
48.331354	2162.317316	18.689613
48.083584	2158.944641	18.694631
48.157520	2146.668441	18.699648
48.101423	2149.350998	18.704666
47.843541	2153.920503	18.709683
48.270706	2157.554836	18.714701
47.883833	2170.582613	18.719719
47.947040	2165.950570	18.724736
48.060491	2171.302502	18.729754
48.263737	2169.767719	18.734771
47.977347	2169.555407	18.739789
47.786033	2177.826985	18.744807
47.784159	2186.923371	18.749824
48.440642	2194.929168	18.754842
48.372546	2210.869994	18.759859
48.975227	2187.225055	18.764877
48.378303	2208.510124	18.769895
48.648203	2199.476401	18.774912
48.781594	2201.680391	18.779930
48.843233	2200.655087	18.784947
48.714753	2192.451829	18.789965
48.756087	2188.978763	18.794983
48.868504	2183.597116	18.800000
49.087277	2196.673051	18.805018
48.838746	2190.760602	18.810035
49.124823	2199.044149	18.815053
49.194999	2208.457851	18.820071
49.819946	2226.121694	18.825088
49.463106	2198.557606	18.830106
49.184839	2197.105125	18.835123
49.459434	2189.571466	18.840141
49.298983	2195.363531	18.845159
49.402825	2185.752203	18.850176
49.302928	2195.749138	18.855194
49.244401	2215.644188	18.860211
49.785341	2209.280170	18.865229
49.757654	2223.043586	18.870247
49.775433	2222.044154	18.875264
49.778989	2219.222108	18.880282
49.641665	2225.648419	18.885299
49.964050	2220.746912	18.890317
49.598058	2220.581118	18.895335
49.645300	2225.379646	18.900352
49.673436	2218.529497	18.905370
49.388419	2216.230935	18.910387
49.905726	2219.843828	18.915405
49.803896	2219.237103	18.920423
49.949599	2236.002025	18.925440
50.106162	2255.997331	18.930458
49.960828	2247.493893	18.935475
50.237127	2255.834093	18.940493
50.175331	2258.538030	18.945511
50.216678	2250.123591	18.950528
50.705872	2247.128907	18.955546
50.375473	2253.310718	18.960563
50.940278	2248.931376	18.965581
50.662517	2241.787050	18.970599
50.738140	2251.560168	18.975616
50.847955	2243.970958	18.980634
50.850368	2253.953188	18.985651
51.032868	2255.564131	18.990669
51.029139	2256.399309	18.995687
50.947985	2247.836865	19.000704
51.249786	2247.063507	19.005722
50.791524	2253.838348	19.010739
51.128302	2246.816251	19.015757
51.108426	2251.203094	19.020775
50.584722	2245.185845	19.025792
51.163728	2246.355199	19.030810
50.979659	2260.865680	19.035827
51.153158	2253.971092	19.040845
51.024468	2243.622809	19.045863
51.081422	2244.776315	19.050880
51.013907	2242.612962	19.055898
51.060082	2252.718786	19.060915
51.210598	2235.129472	19.065933
51.305428	2262.549018	19.070951
51.320693	2271.510577	19.075968
51.518664	2274.283995	19.080986
51.608462	2283.494035	19.086003
51.403581	2268.027740	19.091021
51.457197	2277.931028	19.096039
51.553390	2277.450822	19.101056
51.729161	2257.273504	19.106074
51.799240	2271.756833	19.111091
51.736609	2270.804833	19.116109
51.920262	2292.812687	19.121127
51.930542	2304.407783	19.126144
51.655749	2297.682997	19.131162
52.135456	2300.459468	19.136179
52.357569	2296.181964	19.141197
52.393056	2305.259094	19.146215
52.559850	2304.836060	19.151232
52.676296	2283.511877	19.156250
52.575754	2296.943241	19.161267
52.484694	2294.776557	19.166285
52.544474	2295.341245	19.171303
52.173405	2291.785263	19.176320
52.781853	2296.333843	19.181338
52.722269	2298.144653	19.186355
52.888728	2289.618206	19.191373
52.648485	2287.130789	19.196391
52.536562	2287.050326	19.201408
52.942637	2284.526688	19.206426
52.706359	2298.175563	19.211443
52.790166	2296.781739	19.216461
52.561485	2295.228521	19.221479
52.730152	2288.277266	19.226496
53.077913	2303.989045	19.231514
53.020205	2323.869952	19.236531
53.206183	2322.676144	19.241549
53.481625	2323.712217	19.246567
53.331373	2325.116663	19.251584
53.505189	2317.746105	19.256602
53.211157	2322.944410	19.261619
53.165250	2323.715525	19.266637
53.249309	2333.010677	19.271655
52.968912	2334.772543	19.276672
53.418776	2313.882827	19.281690
53.461057	2320.048489	19.286707
53.425611	2316.040170	19.291725
53.281939	2318.546369	19.296743
53.320883	2339.609077	19.301760
53.834259	2350.431769	19.306778
53.801872	2349.170528	19.311795
54.020616	2361.072230	19.316813
54.059082	2353.334663	19.321831
54.023502	2360.601408	19.326848
53.926633	2353.703485	19.331866
53.989937	2357.541422	19.336883
53.875595	2348.822174	19.341901
53.981419	2350.974735	19.346919
53.934855	2346.589829	19.351936
54.328416	2363.034552	19.356954
54.358016	2366.269043	19.361971
54.349555	2380.425197	19.366989
54.600613	2364.282763	19.372007
54.463300	2373.144436	19.377024
54.498302	2370.655582	19.382042
54.721637	2369.451879	19.387059
54.943021	2378.587504	19.392077
55.037411	2373.461946	19.397095
54.410755	2379.473959	19.402112
54.938758	2368.140650	19.407130
54.719455	2380.669142	19.412147
54.511931	2375.350250	19.417165
54.627661	2372.337233	19.422183
54.895691	2377.227240	19.427200
54.992077	2376.459893	19.432218
54.985454	2381.678453	19.437235
54.870701	2403.107148	19.442253
54.949390	2398.396263	19.447271
54.969189	2404.180114	19.452288
55.222201	2403.531732	19.457306
55.166206	2402.363924	19.462323
55.247391	2416.015765	19.467341
55.508799	2407.566925	19.472359
55.183047	2427.602420	19.477376
55.783500	2428.294051	19.482394
55.887124	2425.171257	19.487411
55.872033	2427.228271	19.492429
55.912645	2429.771958	19.497447
55.783449	2433.714558	19.502464
55.978948	2425.482308	19.507482
55.809461	2435.111365	19.512499
55.596815	2432.630533	19.517517
56.181582	2428.795429	19.522535
55.792662	2435.048003	19.527552
55.914884	2424.661147	19.532570
56.074065	2432.088795	19.537587
56.092146	2433.094342	19.542605
56.270469	2433.662942	19.547623
56.337617	2431.677093	19.552640
56.392694	2433.219494	19.557658
56.338355	2447.994218	19.562675
56.161248	2458.097251	19.567693
56.598945	2459.348157	19.572711
56.623149	2471.989704	19.577728
56.681711	2465.790611	19.582746
56.844648	2466.299524	19.587763
56.710598	2466.522285	19.592781
56.928900	2463.109815	19.597799
56.741737	2465.072355	19.602816
56.745860	2460.161747	19.607834
57.074869	2460.013319	19.612851
56.813900	2458.162391	19.617869
56.739788	2457.377396	19.622887
56.900317	2457.842643	19.627904
57.171381	2475.366582	19.632922
57.538226	2480.634165	19.637939
57.654592	2482.812596	19.642957
57.753355	2462.453773	19.647975
57.347495	2467.301047	19.652992
57.426698	2454.433012	19.658010
57.758733	2454.622340	19.663027
57.789529	2460.968452	19.668045
57.677780	2452.006456	19.673063
57.750864	2458.251430	19.678080
57.487238	2456.732084	19.683098
57.616611	2467.498904	19.688115
57.798060	2476.866715	19.693133
58.278388	2479.967203	19.698151
58.123792	2479.333485	19.703168
58.034635	2484.119242	19.708186
57.932869	2473.564345	19.713203
57.691034	2488.237651	19.718221
57.774860	2484.358930	19.723239
57.747683	2483.812655	19.728256
57.885022	2491.121106	19.733274
58.219242	2501.535920	19.738291
58.320941	2512.404726	19.743309
58.696070	2505.126251	19.748327
58.441243	2513.648060	19.753344
58.269198	2512.385480	19.758362
58.881832	2506.943601	19.763379
58.790678	2515.985211	19.768397
58.773417	2504.106332	19.773415
58.801712	2505.629413	19.778432
58.404912	2510.277819	19.783450
58.848570	2502.508588	19.788467
58.782667	2505.277726	19.793485
59.162402	2520.547289	19.798503
59.238104	2531.439920	19.803520
59.419531	2526.082538	19.808538
59.282410	2517.422671	19.813555
58.898836	2515.561398	19.818573
59.106634	2521.917064	19.823591
59.525107	2531.396562	19.828608
59.297428	2536.920239	19.833626
59.345796	2531.404730	19.838643
59.306581	2535.565841	19.843661
59.367776	2530.300001	19.848679
59.492069	2531.541902	19.853696
59.711905	2534.423582	19.858714
59.709704	2526.792308	19.863731
59.491030	2534.664922	19.868749
59.540338	2532.645721	19.873767
59.827198	2533.626500	19.878784
59.907986	2554.037829	19.883802
59.738374	2556.467185	19.888819
60.099862	2561.250316	19.893837
60.182302	2558.244143	19.898855
60.055465	2565.987282	19.903872
60.015158	2566.881013	19.908890
60.238996	2555.087925	19.913907
60.036677	2559.093349	19.918925
60.365187	2567.095027	19.923943
60.283300	2576.858088	19.928960
60.456251	2570.812187	19.933978
60.560461	2588.951255	19.938995
60.522967	2592.965012	19.944013
60.713551	2582.348465	19.949031
60.652246	2590.451657	19.954048
60.457894	2595.918124	19.959066
60.775164	2579.121448	19.964083
60.683400	2586.626169	19.969101
60.708438	2579.552161	19.974119
60.724252	2601.216756	19.979136
60.915214	2598.639275	19.984154
61.383154	2611.914187	19.989171
61.130640	2621.844506	19.994189
61.480937	2615.293618	19.999207
61.382928	2613.804477	20.004224
60.912930	2624.773197	20.009242
61.347567	2618.381911	20.014259
61.264752	2617.248254	20.019277
61.313705	2615.767925	20.024295
61.510198	2636.798855	20.029312
61.597561	2642.326602	20.034330
61.859073	2643.582027	20.039347
61.744046	2651.884180	20.044365
61.959153	2647.171910	20.049383
62.136844	2648.711297	20.054400
62.075227	2654.826809	20.059418
62.151350	2638.016610	20.064435
61.928045	2646.748213	20.069453
62.137205	2642.436492	20.074471
62.186893	2638.613518	20.079488
62.242666	2639.104919	20.084506
62.605544	2646.713361	20.089523
62.436821	2649.021452	20.094541
62.508562	2640.082779	20.099559
62.582016	2635.929572	20.104576
62.436355	2650.044940	20.109594
62.611955	2632.608472	20.114611
62.784341	2644.646017	20.119629
62.603978	2644.906844	20.124647
62.760479	2655.177058	20.129664
63.263242	2659.990394	20.134682
63.143254	2645.050561	20.139699
62.708233	2648.534629	20.144717
63.038461	2656.404718	20.149735
63.418680	2667.269336	20.154752
63.246759	2675.652159	20.159770
63.283013	2665.118374	20.164787
63.366021	2674.786766	20.169805
63.196231	2679.940208	20.174823
63.198344	2678.074038	20.179840
63.057505	2676.271571	20.184858
63.224453	2670.715073	20.189875
63.016406	2668.629132	20.194893
62.907341	2685.119772	20.199911
63.465925	2684.096201	20.204928
63.495243	2696.374498	20.209946
63.628882	2695.764808	20.214963
64.206768	2699.948685	20.219981
64.184325	2699.610099	20.224999
63.990335	2689.756467	20.230016
63.767858	2704.611756	20.235034
64.056180	2696.009002	20.240051
64.172752	2706.495646	20.245069
64.056093	2714.806748	20.250087
64.520884	2719.337472	20.255104
63.980850	2730.599835	20.260122
64.501403	2717.077512	20.265139
64.489320	2726.879096	20.270157
64.901477	2729.959834	20.275175
64.599659	2724.771485	20.280192
64.817810	2727.758092	20.285210
65.154336	2716.250535	20.290227
65.033892	2717.991655	20.295245
64.981182	2714.300625	20.300263
65.115607	2707.581965	20.305280
65.031990	2712.579298	20.310298
64.914182	2704.175822	20.315315
64.946533	2697.095085	20.320333
65.307736	2701.101922	20.325351
65.459836	2703.281766	20.330368
65.400732	2698.205747	20.335386
65.320612	2707.747574	20.340403
65.655334	2697.743539	20.345421
65.410451	2705.942149	20.350439
65.679837	2695.278341	20.355456
65.528743	2697.937604	20.360474
65.636094	2702.712544	20.365491
65.732239	2709.702804	20.370509
65.955392	2711.265626	20.375527
65.987949	2722.328896	20.380544
66.065466	2716.943180	20.385562
66.301725	2715.872687	20.390579
65.863074	2699.006072	20.395597
66.174734	2712.874723	20.400615
66.403492	2708.406467	20.405632
66.376306	2725.097266	20.410650
66.024723	2723.945108	20.415667
66.177523	2723.836583	20.420685
65.914752	2727.148460	20.425703
66.080089	2725.268051	20.430720
65.940849	2725.958891	20.435738
66.501479	2736.618587	20.440755
66.606334	2752.558379	20.445773
66.507333	2762.408460	20.450791
66.907940	2751.011796	20.455808
66.432189	2765.747070	20.460826
66.765674	2756.391365	20.465843
67.065373	2751.477570	20.470861
66.857503	2761.417382	20.475879
67.309823	2754.098943	20.480896
66.877762	2764.151600	20.485914
67.289488	2771.587915	20.490931
67.345501	2780.330900	20.495949
67.219344	2779.652515	20.500967
67.599668	2782.994779	20.505984
67.684311	2786.499834	20.511002
67.652044	2782.590780	20.516019
67.703366	2783.676791	20.521037
67.647304	2783.832055	20.526055
67.559885	2782.285358	20.531072
67.568250	2790.632413	20.536090
67.375076	2788.147627	20.541107
67.548679	2792.200141	20.546125
67.373800	2809.977312	20.551143
67.988277	2811.649218	20.556160
67.821295	2815.000114	20.561178
68.098774	2809.307157	20.566195
68.017180	2806.314509	20.571213
68.183450	2827.631357	20.576231
68.342852	2835.977949	20.581248
68.303814	2848.479664	20.586266
68.260296	2843.161975	20.591283
68.547206	2837.944195	20.596301
68.481479	2841.669900	20.601319
68.823213	2837.049862	20.606336
68.870811	2837.627528	20.611354
68.872344	2864.938798	20.616371
69.454191	2861.926072	20.621389
69.441623	2860.157401	20.626407
69.199886	2841.432680	20.631424
69.052892	2834.182250	20.636442
69.088482	2840.651262	20.641459
69.615080	2848.759164	20.646477
69.179730	2849.019755	20.651495
69.661849	2835.935309	20.656512
69.832862	2851.299077	20.661530
69.573348	2833.669818	20.666547
69.505929	2831.346678	20.671565
69.548262	2849.745298	20.676583
69.949668	2839.610966	20.681600
69.897437	2856.106106	20.686618
69.911294	2861.054119	20.691635
70.157931	2862.726486	20.696653
69.751092	2867.768341	20.701671
70.127229	2850.398746	20.706688
70.452297	2858.733090	20.711706
70.481745	2852.360700	20.716723
70.168453	2859.616133	20.721741
70.128199	2862.887046	20.726759
70.555196	2843.508968	20.731776
70.137190	2858.087239	20.736794
70.267536	2860.018072	20.741811
70.531371	2849.167035	20.746829
70.099801	2855.999248	20.751847
70.484475	2862.606106	20.756864
70.707601	2877.754709	20.761882
71.011176	2873.133666	20.766899
70.890366	2869.268601	20.771917
70.782499	2881.475325	20.776935
71.012965	2879.353242	20.781952
70.562999	2880.834644	20.786970
70.954848	2895.028142	20.791987
71.285507	2897.355743	20.797005
71.449640	2914.533844	20.802023
71.315758	2912.020701	20.807040
71.457744	2913.540639	20.812058
71.462316	2917.792417	20.817075
71.446420	2911.223497	20.822093
71.409334	2917.074834	20.827111
71.564199	2913.847009	20.832128
71.760087	2941.969902	20.837146
71.852925	2941.674282	20.842163
71.895067	2927.143307	20.847181
71.873541	2943.870424	20.852199
72.025118	2948.084606	20.857216
72.015007	2937.672080	20.862234
71.682306	2949.722781	20.867251
71.928902	2953.921024	20.872269
71.716730	2971.598930	20.877287
72.142252	2966.768046	20.882304
72.347358	2971.083039	20.887322
72.185010	2976.017502	20.892339
72.971867	2981.072758	20.897357
72.844506	2993.285043	20.902375
73.021613	2993.270182	20.907392
73.067982	2999.403227	20.912410
73.130341	2988.691988	20.917427
73.040234	2986.290632	20.922445
73.211290	2997.903902	20.927463
73.341147	2988.275313	20.932480
73.562739	2990.992400	20.937498
73.471033	2991.013329	20.942515
73.595526	2972.286670	20.947533
73.460993	2974.447766	20.952551
73.235646	2981.323450	20.957568
73.691257	2983.816782	20.962586
73.610084	2974.030708	20.967603
74.083364	2975.593000	20.972621
73.956113	2970.409759	20.977639
74.112606	2972.101235	20.982656
74.312178	2967.580919	20.987674
74.037944	2969.780026	20.992691
74.445248	2963.035036	20.997709
74.241523	2966.677372	21.002727
73.830901	2962.667352	21.007744
74.073104	2961.225392	21.012762
74.494285	2961.752923	21.017779
74.397483	2970.724130	21.022797
74.140560	2970.072097	21.027815
74.030604	2959.601536	21.032832
74.080929	2967.124695	21.037850
74.219731	2994.389929	21.042867
74.573591	2989.874892	21.047885
74.814113	2998.363606	21.052903
74.591203	2995.391883	21.057920
74.666731	2993.027040	21.062938
75.048318	3008.024647	21.067955
75.503407	3016.240017	21.072973
75.862663	3008.476117	21.077991
75.628779	2995.059699	21.083008
75.873305	2988.871633	21.088026
75.599008	2987.471925	21.093043
75.932589	2985.388447	21.098061
76.064668	2979.779183	21.103079
75.642963	2972.868268	21.108096
75.926633	2967.661186	21.113114
75.731048	2977.422193	21.118131
76.076366	2974.782272	21.123149
75.980062	2975.614948	21.128167
75.737456	2985.257599	21.133184
76.057173	2974.650853	21.138202
75.898031	2990.715604	21.143219
76.079368	2996.602147	21.148237
76.241314	2997.417238	21.153255
76.328279	3008.485421	21.158272
76.373811	3009.736779	21.163290
76.343586	3012.574266	21.168307
76.528682	3002.922699	21.173325
76.364173	3012.353895	21.178343
76.319941	3025.339579	21.183360
76.889268	3030.271434	21.188378
76.911420	3037.418392	21.193395
77.089621	3039.444666	21.198413
77.137748	3040.455690	21.203431
77.033445	3042.334293	21.208448
76.889247	3041.907347	21.213466
76.740607	3039.597914	21.218483
76.607892	3040.229516	21.223501
76.841205	3053.495055	21.228519
76.928278	3068.092099	21.233536
77.584177	3059.978010	21.238554
77.157746	3070.063014	21.243571
77.256793	3078.822128	21.248589
77.355082	3089.960936	21.253607
77.515025	3102.426414	21.258624
77.596461	3103.417184	21.263642
77.642054	3110.729566	21.268659
77.900095	3108.678571	21.273677
77.781806	3124.364087	21.278695
77.917839	3129.992027	21.283712
78.280874	3137.429217	21.288730
78.156570	3140.080353	21.293747
78.041277	3138.920368	21.298765
78.390169	3144.408958	21.303783
78.134373	3156.803122	21.308800
78.459190	3166.777823	21.313818
78.781486	3170.730425	21.318835
78.550704	3163.679628	21.323853
78.587213	3165.070100	21.328871
78.421750	3169.789585	21.333888
79.191357	3175.200864	21.338906
79.216944	3198.059689	21.343923
79.082400	3190.384671	21.348941
79.221721	3195.955474	21.353959
79.154443	3193.411207	21.358976
79.503609	3188.645134	21.363994
79.373349	3195.396410	21.369011
79.428440	3193.240108	21.374029
79.796673	3197.729747	21.379047
79.611520	3211.364236	21.384064
79.953435	3206.512783	21.389082
79.653446	3223.109206	21.394099
79.746511	3226.168570	21.399117
79.940184	3218.294879	21.404135
80.006547	3234.743212	21.409152
80.237180	3227.469336	21.414170
79.843862	3230.435568	21.419187
79.980541	3231.397871	21.424205
80.356337	3255.192103	21.429223
80.381585	3260.110116	21.434240
80.532380	3260.602116	21.439258
80.425160	3260.743517	21.444275
80.721364	3257.479704	21.449293
80.925448	3262.133204	21.454311
80.488741	3264.392090	21.459328
80.872306	3275.188193	21.464346
81.099737	3283.842783	21.469363
81.135749	3285.986165	21.474381
81.317267	3287.917547	21.479399
80.957343	3293.191990	21.484416
81.440296	3293.673498	21.489434
80.973735	3294.407125	21.494451
81.115616	3292.410029	21.499469
81.511442	3288.323224	21.504487
80.857815	3305.479591	21.509504
81.273322	3318.327710	21.514522
81.525622	3311.451527	21.519539
81.869122	3301.745397	21.524557
82.622246	3295.246391	21.529575
82.805497	3287.173730	21.534592
82.885479	3285.450033	21.539610
83.092447	3294.353327	21.544627
82.821229	3277.190306	21.549645
83.006210	3280.031283	21.554663
82.692384	3262.211146	21.559680
83.142755	3261.618575	21.564698
83.001938	3257.289331	21.569715
83.325339	3248.510747	21.574733
83.139515	3249.618881	21.579751
82.958639	3254.305452	21.584768
83.259523	3245.189058	21.589786
83.219598	3246.723883	21.594803
83.116670	3245.280300	21.599821
83.128087	3249.006391	21.604839
83.054167	3252.831050	21.609856
83.464633	3247.487226	21.614874
83.354198	3248.804383	21.619891
83.207617	3244.594845	21.624909
83.352591	3251.450929	21.629927
83.117758	3267.753033	21.634944
83.446708	3262.870591	21.639962
83.478273	3274.213695	21.644979
83.594042	3273.640659	21.649997
83.932237	3278.132754	21.655015
84.057344	3299.095786	21.660032
84.302602	3300.435674	21.665050
83.949759	3307.272844	21.670067
83.941007	3300.952764	21.675085
84.235220	3310.561148	21.680103
83.666547	3314.644080	21.685120
84.072174	3325.250267	21.690138
84.411021	3333.677871	21.695155
84.273516	3346.477333	21.700173
84.675451	3346.683065	21.705191
84.348120	3359.162752	21.710208
84.341346	3376.914586	21.715226
84.973076	3377.176496	21.720243
85.054186	3382.358609	21.725261
85.218138	3371.538851	21.730279
84.988689	3379.677160	21.735296
85.029476	3400.428015	21.740314
85.664320	3397.206925	21.745331
85.648722	3404.949284	21.750349
85.580826	3397.184077	21.755367
85.689491	3396.302229	21.760384
85.881461	3399.633772	21.765402
85.585364	3402.929873	21.770419
85.666808	3397.764331	21.775437
86.273104	3392.273587	21.780455
85.801076	3411.107360	21.785472
86.050675	3414.488714	21.790490
86.344574	3429.503100	21.795507
86.139824	3435.900572	21.800525
86.454749	3433.823155	21.805543
86.562460	3436.849549	21.810560
86.291435	3437.839913	21.815578
86.561854	3440.439953	21.820595
86.656305	3438.947567	21.825613
86.511513	3434.482813	21.830631
87.108281	3450.816123	21.835648
86.815622	3451.360758	21.840666
86.896497	3458.131976	21.845683
86.918548	3459.282493	21.850701
86.911332	3459.245895	21.855719
87.293692	3462.053071	21.860736
87.630452	3477.347012	21.865754
87.573305	3491.438059	21.870771
87.609017	3491.577906	21.875789
88.037034	3476.892025	21.880807
88.256464	3484.152484	21.885824
87.878952	3486.514454	21.890842
88.099511	3488.371985	21.895859
87.967447	3479.385851	21.900877
88.360468	3468.504318	21.905895
88.346964	3474.304916	21.910912
88.305555	3476.855573	21.915930
88.307442	3483.946195	21.920947
87.891787	3486.265475	21.925965
88.197165	3475.279916	21.930983
88.087825	3498.310978	21.936000
88.344256	3512.267077	21.941018
88.211072	3503.746808	21.946035
88.664316	3523.442446	21.951053
88.796179	3535.406163	21.956071
88.885745	3538.855548	21.961088
89.062917	3538.775385	21.966106
89.215232	3538.211458	21.971123
89.007359	3548.103814	21.976141
89.488461	3537.898870	21.981159
89.021349	3552.960012	21.986176
89.457813	3563.627534	21.991194
89.639233	3563.265070	21.996211
89.466205	3567.122135	22.001229
89.521784	3575.307136	22.006247
89.258071	3579.975553	22.011264
89.941662	3596.447793	22.016282
89.939533	3598.549317	22.021299
90.073945	3600.500054	22.026317
90.117382	3596.319897	22.031335
90.233177	3601.869434	22.036352
90.237360	3606.712256	22.041370
90.675030	3594.640371	22.046387
90.887058	3597.125459	22.051405
90.601164	3600.942319	22.056423
91.038103	3609.669105	22.061440
91.181676	3611.277758	22.066458
91.565763	3606.563410	22.071475
91.133549	3590.887313	22.076493
91.375049	3580.715044	22.081511
91.366153	3579.532549	22.086528
91.314413	3582.969079	22.091546
91.590940	3582.482101	22.096563
91.471982	3600.394482	22.101581
91.498268	3606.203734	22.106599
91.560922	3607.362733	22.111616
91.541119	3606.709039	22.116634
91.900200	3609.121119	22.121651
91.452233	3611.157652	22.126669
91.792068	3602.120573	22.131687
91.868173	3621.047345	22.136704
92.183689	3631.631153	22.141722
92.299421	3633.586447	22.146739
91.982181	3636.900917	22.151757
92.340436	3630.720406	22.156775
92.335503	3630.917870	22.161792
92.662524	3649.913225	22.166810
93.047710	3648.461773	22.171827
92.769226	3657.043079	22.176845
93.282332	3664.818474	22.181863
93.338048	3655.571793	22.186880
93.411910	3649.593960	22.191898
93.212746	3658.587417	22.196915
93.359701	3651.384104	22.201933
93.730005	3642.951019	22.206951
93.522385	3654.912333	22.211968
93.756898	3660.254160	22.216986
93.956431	3652.144090	22.222003
93.801042	3655.108648	22.227021
94.091008	3649.036566	22.232039
94.083096	3645.132837	22.237056
93.877589	3652.660173	22.242074
94.054508	3650.511910	22.247091
94.001736	3653.047890	22.252109
93.933207	3646.233728	22.257127
94.042645	3667.571878	22.262144
94.093809	3681.219462	22.267162
94.397768	3681.019173	22.272179
94.294943	3695.403259	22.277197
94.420583	3699.578530	22.282215
94.490190	3707.431754	22.287232
94.679211	3711.559946	22.292250
95.048336	3709.841223	22.297267
95.191614	3708.212797	22.302285
95.283026	3706.410922	22.307303
95.184408	3715.650339	22.312320
95.242822	3717.083784	22.317338
95.217476	3718.674547	22.322355
95.166386	3740.813271	22.327373
95.359700	3734.747128	22.332391
95.940381	3733.676707	22.337408
95.589296	3746.418535	22.342426
95.783157	3739.523940	22.347443
95.457212	3748.632857	22.352461
95.661428	3767.888669	22.357479
95.811504	3775.650430	22.362496
95.840174	3775.387841	22.367514
95.973735	3777.407178	22.372531
96.161949	3802.451557	22.377549
96.290207	3807.583821	22.382567
96.925141	3806.769066	22.387584
96.459980	3812.681944	22.392602
96.550844	3804.328732	22.397619
96.540873	3822.003733	22.402637
96.964001	3823.382174	22.407655
97.032725	3836.267174	22.412672
96.711746	3839.078026	22.417690
97.125408	3836.340523	22.422707
97.009953	3866.166071	22.427725
97.409577	3872.393403	22.432743
97.409776	3870.967925	22.437760
97.629917	3875.943959	22.442778
97.458334	3867.751352	22.447795
97.574316	3881.641307	22.452813
97.764986	3896.815024	22.457831
98.030457	3897.103104	22.462848
97.739525	3906.068865	22.467866
98.199395	3894.855395	22.472883
98.446546	3916.749366	22.477901
98.345984	3932.623293	22.482919
98.855441	3934.885579	22.487936
98.712498	3942.366111	22.492954
98.842969	3939.226129	22.497971
98.789049	3938.578648	22.502989
98.795276	3926.787699	22.508007
98.879268	3927.617636	22.513024
99.076107	3934.677386	22.518042
99.143550	3947.045839	22.523059
99.424488	3957.130349	22.528077
99.335680	3950.272080	22.533095
99.793374	3953.439439	22.538112
99.444373	3956.855020	22.543130
99.560514	3953.277566	22.548147
99.609823	3956.202459	22.553165
99.852780	3967.226823	22.558183
100.209457	3972.084355	22.563200
100.393186	3976.860119	22.568218
100.613378	3973.152785	22.573235
100.525666	3981.861193	22.578253
100.586884	3979.049280	22.583271
100.732675	3967.468113	22.588288
100.508283	3975.288910	22.593306
100.651157	3973.050054	22.598323
100.815084	3974.602794	22.603341
100.804145	3969.130819	22.608359
100.968361	3972.706857	22.613376
100.677106	3975.999164	22.618394
100.900382	3975.003818	22.623411
100.930858	3985.543656	22.628429
100.800620	4002.075337	22.633447
101.152494	3992.062187	22.638464
101.131110	4011.030969	22.643482
101.377452	4010.778505	22.648499
101.396915	4025.697237	22.653517
101.691234	4033.975012	22.658535
102.062516	4031.479451	22.663552
101.723030	4045.083467	22.668570
101.883100	4038.943046	22.673587
102.342798	4050.164194	22.678605
102.048103	4061.125684	22.683623
102.319282	4061.392405	22.688640
102.031999	4072.199317	22.693658
102.037731	4077.157690	22.698675
102.552767	4091.910925	22.703693
102.357555	4101.049558	22.708711
103.109738	4097.384014	22.713728
102.629596	4111.193032	22.718746
102.837503	4119.952715	22.723763
103.108749	4129.966514	22.728781
102.834850	4138.952513	22.733799
103.000939	4134.771526	22.738816
103.242376	4151.799506	22.743834
103.330027	4154.474451	22.748851
103.685175	4167.816762	22.753869
103.722912	4172.278380	22.758887
103.839823	4163.849222	22.763904
104.130646	4172.509178	22.768922
104.505732	4182.721221	22.773939
104.855087	4182.693055	22.778957
104.734108	4190.112781	22.783975
105.017395	4173.274083	22.788992
104.619123	4170.097221	22.794010
104.852317	4166.392486	22.799027
104.928332	4175.622436	22.804045
105.163718	4183.365302	22.809063
105.075496	4175.611578	22.814080
105.002842	4186.113724	22.819098
105.226220	4186.206344	22.824115
105.295815	4176.859573	22.829133
105.178863	4184.329789	22.834151
105.433811	4172.279493	22.839168
105.617195	4173.896807	22.844186
105.392616	4185.681102	22.849203
105.375588	4194.356336	22.854221
105.466611	4207.923316	22.859239
105.732056	4198.428868	22.864256
105.774204	4220.823281	22.869274
106.078135	4226.859125	22.874291
105.903433	4235.681465	22.879309
105.991487	4250.054534	22.884327
106.319018	4241.256611	22.889344
106.371618	4246.583608	22.894362
106.037686	4256.677480	22.899379
106.363707	4267.396172	22.904397
106.350314	4276.717540	22.909415
106.704442	4275.618705	22.914432
106.961420	4294.956478	22.919450
107.589180	4295.245798	22.924467
107.588312	4294.205145	22.929485
107.008694	4304.873970	22.934503
107.324185	4293.398439	22.939520
107.226697	4305.836763	22.944538
107.535414	4323.087863	22.949555
107.760806	4332.441991	22.954573
107.591575	4334.201305	22.959591
107.792691	4328.648178	22.964608
107.819651	4338.365154	22.969626
108.293050	4354.702631	22.974643
108.483400	4363.002679	22.979661
108.343030	4373.952377	22.984679
108.689396	4368.623097	22.989696
108.421055	4364.247777	22.994714
108.292038	4356.765581	22.999731
108.832716	4375.779728	23.004749
109.182979	4386.700758	23.009767
109.393971	4383.418823	23.014784
109.304849	4396.715757	23.019802
109.355241	4394.313791	23.024819
109.712045	4386.711626	23.029837
109.485573	4391.506524	23.034855
109.621312	4390.247403	23.039872
109.687961	4398.905481	23.044890
109.840181	4408.365730	23.049907
110.429106	4413.364957	23.054925
110.182864	4423.498454	23.059943
110.710834	4417.472284	23.064960
110.211720	4411.988307	23.069978
110.442175	4411.215999	23.074995
110.901264	4408.636358	23.080013
110.480395	4417.517729	23.085031
110.559191	4412.693685	23.090048
110.661840	4416.034986	23.095066
110.796539	4437.276606	23.100083
111.219221	4435.708178	23.105101
110.866463	4442.309054	23.110119
111.468612	4432.201416	23.115136
111.319809	4439.924652	23.120154
110.893931	4445.315435	23.125171
111.632062	4449.477426	23.130189
111.372347	4464.021020	23.135207
111.686851	4471.288838	23.140224
111.940072	4465.564502	23.145242
112.571815	4442.624082	23.150259
112.871116	4438.468182	23.155277
113.058468	4440.243022	23.160295
113.525800	4423.956854	23.165312
113.342415	4410.228989	23.170330
113.291080	4401.961838	23.175347
113.536606	4388.210440	23.180365
113.742266	4388.092691	23.185383
113.527768	4379.658828	23.190400
113.640730	4362.456085	23.195418
113.522349	4349.927859	23.200435
113.990192	4347.638700	23.205453
113.658965	4351.144365	23.210471
113.655665	4347.635425	23.215488
113.701741	4345.621213	23.220506
113.338021	4345.436134	23.225523
113.645720	4345.789869	23.230541
113.389073	4359.373096	23.235559
113.662232	4375.137554	23.240576
113.994844	4390.667552	23.245594
113.976119	4384.683732	23.250611
114.007298	4389.240080	23.255629
113.808259	4411.537145	23.260647
113.742942	4409.686228	23.265664
114.256396	4431.828010	23.270682
114.283760	4450.781718	23.275699
114.604428	4441.334951	23.280717
114.513962	4456.663431	23.285735
114.588458	4469.436354	23.290752
114.850950	4477.982217	23.295770
114.664195	4496.432805	23.300787
115.578378	4491.113634	23.305805
115.593053	4500.986086	23.310823
115.699070	4497.999361	23.315840
115.605360	4502.242881	23.320858
115.503910	4516.982356	23.325875
115.921038	4525.082697	23.330893
116.137318	4526.111853	23.335911
116.249742	4541.726685	23.340928
116.259995	4539.836166	23.345946
116.070161	4539.565138	23.350963
116.479931	4550.201453	23.355981
116.446303	4568.027451	23.360999
116.620390	4561.601362	23.366016
117.023391	4565.263770	23.371034
116.846519	4581.045930	23.376051
117.134109	4578.647805	23.381069
117.059277	4583.826102	23.386087
117.408775	4589.786387	23.391104
117.501663	4591.924824	23.396122
117.403988	4584.943371	23.401139
117.573394	4585.610250	23.406157
117.507597	4589.406424	23.411175
117.893249	4607.051536	23.416192
117.891905	4610.425985	23.421210
118.022817	4620.184788	23.426227
117.998483	4617.775821	23.431245
118.164840	4616.909091	23.436263
118.009825	4624.188133	23.441280
118.258922	4645.654121	23.446298
118.280999	4645.542045	23.451315
118.477407	4642.223043	23.456333
118.627551	4667.153812	23.461351
118.654598	4686.588558	23.466368
118.934668	4678.360451	23.471386
119.090092	4682.983617	23.476403
119.367284	4701.272366	23.481421
119.520473	4705.591434	23.486439
119.585883	4711.210004	23.491456
119.804031	4711.879344	23.496474
119.522971	4711.969804	23.501491
120.678098	4709.652815	23.506509
120.609902	4710.927175	23.511527
120.518805	4705.052319	23.516544
120.839590	4692.988741	23.521562
120.517209	4697.836007	23.526579
120.779558	4716.463072	23.531597
120.924617	4734.332368	23.536615
120.766334	4730.556177	23.541632
121.030034	4732.367656	23.546650
121.366982	4724.127307	23.551667
121.440219	4716.658305	23.556685
121.277700	4721.760159	23.561703
121.457513	4726.360569	23.566720
121.716214	4716.054969	23.571738
121.708384	4724.331754	23.576755
121.585042	4743.925086	23.581773
121.709272	4746.584080	23.586791
121.632326	4750.037488	23.591808
121.961351	4758.727103	23.596826
121.774722	4775.742249	23.601843
122.150305	4786.509277	23.606861
122.072192	4790.499428	23.611879
121.879281	4802.263428	23.616896
122.597191	4805.154254	23.621914
122.511627	4822.895221	23.626931
122.765262	4817.806360	23.631949
123.399525	4831.742018	23.636967
123.416926	4835.023056	23.641984
123.485107	4843.832989	23.647002
123.342254	4848.675278	23.652019
123.541816	4843.050615	23.657037
123.837074	4836.442232	23.662055
123.402486	4852.508089	23.667072
123.850042	4868.701570	23.672090
123.945983	4872.376045	23.677107
123.740121	4880.372164	23.682125
124.060065	4874.518236	23.687143
123.743133	4892.021611	23.692160
124.297498	4905.166827	23.697178
124.585972	4914.994322	23.702195
124.846773	4910.132439	23.707213
124.748219	4905.704705	23.712231
124.858648	4940.355260	23.717248
125.095696	4934.557797	23.722266
124.929445	4936.692764	23.727283
124.901859	4944.130231	23.732301
125.057851	4954.058337	23.737319
125.345602	4957.599185	23.742336
125.641678	4963.298292	23.747354
125.962743	4972.984523	23.752371
126.066458	4961.190576	23.757389
126.400650	4965.760150	23.762407
126.315864	4993.397536	23.767424
126.775788	4988.405534	23.772442
126.964810	4995.065808	23.777459
126.621599	4995.754657	23.782477
126.999168	4993.685923	23.787495
127.149396	4992.657317	23.792512
127.223661	4992.252118	23.797530
127.243700	4989.076027	23.802547
127.280534	4993.685159	23.807565
127.257836	4991.256201	23.812583
127.258656	5002.427738	23.817600
127.718418	5011.226468	23.822618
128.005414	5015.920021	23.827635
127.625747	5031.221258	23.832653
127.601141	5026.758094	23.837671
127.737880	5031.398511	23.842688
127.989026	5038.711332	23.847706
128.233864	5043.274723	23.852723
128.155719	5047.309005	23.857741
128.733639	5060.489156	23.862759
128.252459	5081.887345	23.867776
128.672030	5088.809860	23.872794
128.916959	5083.391079	23.877811
128.559742	5091.752105	23.882829
129.162186	5101.012770	23.887847
129.075283	5106.005929	23.892864
129.543645	5103.015590	23.897882
129.799139	5111.131804	23.902899
130.279038	5121.437149	23.907917
130.490490	5118.739531	23.912935
130.273041	5133.196793	23.917952
130.657994	5131.036389	23.922970
130.403108	5123.436979	23.927987
130.293053	5127.812310	23.933005
130.848976	5120.175661	23.938023
131.028359	5122.984850	23.943040
131.164625	5116.037435	23.948058
131.140784	5125.186348	23.953075
131.739944	5117.282394	23.958093
131.954285	5107.749097	23.963111
131.515894	5117.227667	23.968128
131.741603	5112.624646	23.973146
131.921673	5108.240538	23.978163
131.626630	5113.476162	23.983181
131.813599	5112.180491	23.988199
131.666032	5114.303849	23.993216
132.031981	5111.399859	23.998234
131.923598	5113.238461	24.003251
132.122123	5133.824207	24.008269
132.787528	5135.110651	24.013287
132.051271	5144.143447	24.018304
132.104156	5146.592814	24.023322
132.833736	5156.505123	24.028339
132.433282	5176.201434	24.033357
132.602706	5178.100384	24.038375
132.572261	5189.869468	24.043392
132.957226	5201.239527	24.048410
133.049672	5213.913462	24.053427
132.766876	5225.208280	24.058445
133.131829	5238.589342	24.063463
133.167467	5246.245037	24.068480
133.159456	5265.874169	24.073498
134.071677	5276.032011	24.078515
133.677990	5283.007196	24.083533
134.277445	5295.601929	24.088551
134.816426	5305.042783	24.093568
134.778653	5305.756895	24.098586
135.022474	5300.800823	24.103603
134.745227	5307.375090	24.108621
135.251939	5314.011601	24.113639
135.231696	5337.402673	24.118656
135.299990	5334.971738	24.123674
135.521794	5335.064622	24.128691
135.383887	5339.780400	24.133709
135.420688	5338.289151	24.138727
135.862734	5360.433493	24.143744
136.246212	5364.225100	24.148762
136.304585	5365.748404	24.153779
136.286339	5371.341227	24.158797
136.089954	5361.256444	24.163815
136.126725	5375.814235	24.168832
136.316603	5377.506179	24.173850
136.438311	5387.699675	24.178867
136.624723	5405.722116	24.183885
137.126371	5405.270000	24.188903
137.395968	5420.354815	24.193920
137.526473	5411.066000	24.198938
137.539462	5418.572764	24.203955
137.739275	5418.755699	24.208973
137.798648	5416.301783	24.213991
137.909275	5432.208946	24.219008
138.457375	5435.242636	24.224026
138.534452	5447.820091	24.229043
138.442446	5451.918846	24.234061
138.652225	5445.619647	24.239079
138.246530	5447.379030	24.244096
138.484858	5443.371046	24.249114
138.507902	5454.108236	24.254131
138.696251	5450.735269	24.259149
138.870831	5464.532405	24.264167
138.865651	5481.102443	24.269184
138.827582	5478.569644	24.274202
139.216023	5487.165248	24.279219
139.222857	5506.460318	24.284237
139.372877	5498.382312	24.289255
139.543389	5512.188796	24.294272
139.946605	5525.481408	24.299290
140.019926	5527.748198	24.304307
139.783187	5533.249252	24.309325
140.193713	5541.624220	24.314343
140.129394	5566.552941	24.319360
140.569784	5560.455312	24.324378
140.657000	5560.134577	24.329395
140.532449	5591.383597	24.334413
140.924650	5591.826963	24.339431
140.913273	5595.630451	24.344448
141.127042	5604.218572	24.349466
141.383690	5624.163171	24.354483
141.217878	5632.988070	24.359501
141.577403	5627.546886	24.364519
141.646241	5642.762287	24.369536
141.737266	5666.216386	24.374554
141.967351	5659.935102	24.379571
142.076740	5687.571146	24.384589
142.342185	5683.111101	24.389607
142.522848	5688.928815	24.394624
142.772086	5691.792278	24.399642
143.039138	5709.519780	24.404659
142.907142	5721.270860	24.409677
143.133162	5721.150647	24.414695
143.315339	5714.828985	24.419712
143.567144	5716.266408	24.424730
143.982648	5729.426640	24.429747
144.261979	5738.401707	24.434765
143.999461	5734.939278	24.439783
144.591028	5730.013374	24.444800
144.455847	5728.121503	24.449818
145.184210	5730.135176	24.454835
144.711075	5723.250029	24.459853
145.190301	5719.886481	24.464871
145.627214	5717.851462	24.469888
145.447948	5718.738429	24.474906
145.394640	5719.595083	24.479923
145.389205	5718.087714	24.484941
145.419295	5720.614768	24.489959
145.489757	5721.061447	24.494976
145.406912	5717.428754	24.499994
145.785285	5722.841239	24.505011
145.452790	5752.768143	24.510029
145.655387	5746.289004	24.515047
145.846711	5744.578741	24.520064
145.825316	5762.327910	24.525082
146.517670	5773.363013	24.530099
146.809926	5779.997741	24.535117
146.723230	5779.736991	24.540135
146.825548	5779.930757	24.545152
146.821954	5800.253831	24.550170
147.160056	5800.212520	24.555187
147.007025	5817.976451	24.560205
147.380068	5820.392190	24.565223
147.311446	5817.366172	24.570240
147.407936	5842.394813	24.575258
147.905434	5845.832411	24.580275
147.680847	5845.210483	24.585293
148.194656	5871.948399	24.590311
148.337987	5874.019185	24.595328
148.246993	5877.806330	24.600346
148.521234	5871.117444	24.605363
148.786087	5889.733005	24.610381
148.792720	5903.179674	24.615399
148.898086	5906.144011	24.620416
148.710023	5917.890812	24.625434
148.833624	5935.084414	24.630451
149.183902	5946.146654	24.635469
149.330349	5938.574883	24.640487
149.451646	5950.642172	24.645504
149.626647	5960.130472	24.650522
149.841468	5958.528949	24.655539
149.741734	5980.482087	24.660557
149.935808	5995.542554	24.665575
150.535931	5998.621572	24.670592
150.581935	6017.664010	24.675610
151.027810	6020.544178	24.680627
150.986321	6026.881325	24.685645
151.238944	6023.408286	24.690663
151.428663	6021.680152	24.695680
151.413278	6031.553698	24.700698
152.026615	6045.400223	24.705715
151.822615	6050.509932	24.710733
151.852364	6049.861603	24.715751
152.166957	6047.293718	24.720768
152.273854	6059.022709	24.725786
152.358508	6052.747140	24.730803
152.746363	6068.445557	24.735821
152.666674	6077.260134	24.740839
152.873336	6075.718123	24.745856
153.204648	6082.293258	24.750874
153.191845	6082.099399	24.755891
153.129429	6089.365179	24.760909
153.589254	6109.287479	24.765927
153.795362	6112.279068	24.770944
153.609304	6112.359888	24.775962
153.853999	6127.062293	24.780979
153.573869	6114.554426	24.785997
153.747067	6130.475966	24.791015
154.139831	6135.049945	24.796032
154.381582	6148.059654	24.801050
154.420159	6141.423173	24.806067
154.386012	6161.257505	24.811085
154.392039	6180.548073	24.816103
154.708354	6172.918413	24.821120
154.716032	6190.937265	24.826138
155.107381	6206.279638	24.831155
155.598779	6204.228001	24.836173
155.247626	6210.681479	24.841191
155.430717	6222.697436	24.846208
155.554814	6239.149359	24.851226
156.107419	6239.163543	24.856243
156.285378	6247.876556	24.861261
156.389611	6261.186033	24.866279
156.682365	6268.332325	24.871296
156.732123	6265.686249	24.876314
156.571266	6273.129896	24.881331
156.522383	6284.511746	24.886349
157.096478	6292.599844	24.891367
157.284643	6298.163252	24.896384
157.105854	6311.846786	24.901402
157.324825	6321.212647	24.906419
157.646213	6331.762064	24.911437
157.524509	6351.290380	24.916455
157.752412	6348.356238	24.921472
157.965481	6362.972651	24.926490
158.268593	6365.510573	24.931507
158.193217	6386.252675	24.936525
158.368787	6393.666344	24.941543
158.600915	6394.180897	24.946560
158.805473	6425.390213	24.951578
159.291197	6427.032749	24.956595
159.384903	6427.977730	24.961613
159.229003	6436.525352	24.966631
159.404804	6443.590452	24.971648
159.688241	6451.320560	24.976666
159.768344	6453.178055	24.981683
160.198354	6472.757041	24.986701
160.062576	6472.976191	24.991719
160.741885	6479.267055	24.996736
160.433011	6485.662767	25.001754
160.849656	6493.483386	25.006771
161.164314	6493.312056	25.011789
161.389374	6493.462658	25.016807
161.670735	6500.651794	25.021824
161.691709	6492.371157	25.026842
161.726454	6496.468873	25.031859
161.791961	6503.206962	25.036877
161.778688	6518.497725	25.041895
162.216917	6515.784158	25.046912
162.310887	6531.106618	25.051930
162.543281	6525.074024	25.056947
162.812383	6520.060017	25.061965
162.707717	6531.004038	25.066983
162.800383	6528.603643	25.072000
162.525758	6549.584675	25.077018
162.888875	6549.870629	25.082035
163.205583	6549.062436	25.087053
163.374371	6569.225318	25.092071
163.821801	6568.583545	25.097088
163.667057	6585.221938	25.102106
163.845655	6578.208868	25.107123
164.348707	6574.556507	25.112141
164.339339	6580.238067	25.117159
164.468372	6585.531691	25.122176
164.635663	6591.956959	25.127194
164.378123	6603.053660	25.132211
164.864666	6602.256154	25.137229
164.648569	6621.969828	25.142247
165.673340	6629.381976	25.147264
165.269558	6641.661013	25.152282
165.404797	6637.551913	25.157299
165.821086	6648.398795	25.162317
165.542688	6655.387705	25.167335
166.142710	6659.958703	25.172352
166.044935	6664.153130	25.177370
165.935588	6683.416325	25.182387
166.473606	6693.284690	25.187405
166.635977	6696.088240	25.192423
166.972157	6699.036394	25.197440
167.060404	6713.186009	25.202458
167.466283	6710.262762	25.207475
167.966640	6710.714890	25.212493
167.996222	6716.480777	25.217511
168.250074	6712.427493	25.222528
168.035747	6707.289075	25.227546
168.127228	6711.614639	25.232563
168.676723	6721.345860	25.237581
168.545009	6726.476533	25.242599
168.831962	6727.677914	25.247616
168.845986	6736.086099	25.252634
168.703041	6738.533121	25.257651
168.995719	6735.985138	25.262669
169.012889	6761.790414	25.267687
169.108192	6760.326676	25.272704
169.460096	6776.396668	25.277722
169.390411	6794.664636	25.282739
169.717212	6785.976279	25.287757
169.691231	6804.515829	25.292775
169.740047	6810.691773	25.297792
170.094764	6827.429392	25.302810
170.195714	6835.879639	25.307827
170.707276	6855.077103	25.312845
170.635398	6863.122949	25.317863
170.806748	6867.106140	25.322880
170.846700	6876.862054	25.327898
171.177975	6888.489046	25.332915
171.082106	6886.095049	25.337933
171.307849	6902.474061	25.342951
171.542132	6913.304521	25.347968
171.686552	6916.227428	25.352986
171.940644	6937.676279	25.358003
172.181418	6941.135403	25.363021
172.088477	6951.542025	25.368039
172.274589	6965.175059	25.373056
172.638482	6986.489236	25.378074
172.913786	6995.503872	25.383091
172.919711	6996.484131	25.388109
173.130823	7012.872680	25.393127
173.320724	7020.767501	25.398144
173.591611	7030.319884	25.403162
173.597098	7044.276069	25.408179
173.937944	7043.874737	25.413197
173.730230	7052.098924	25.418215
174.160933	7075.623841	25.423232
174.191131	7085.384593	25.428250
174.223993	7094.804223	25.433267
174.737024	7105.644672	25.438285
175.003476	7115.765135	25.443303
175.226714	7127.331642	25.448320
175.479622	7135.810550	25.453338
175.598887	7149.763643	25.458355
175.722415	7144.945746	25.463373
175.932179	7153.533833	25.468391
175.812177	7169.229412	25.473408
176.275534	7178.999849	25.478426
176.491504	7186.805622	25.483443
176.800918	7198.330905	25.488461
177.074178	7204.299694	25.493479
176.664399	7202.215356	25.498496
177.230478	7200.420001	25.503514
177.276360	7229.516064	25.508531
177.649581	7234.256384	25.513549
177.887620	7229.561836	25.518567
178.031588	7238.106170	25.523584
178.536914	7239.710270	25.528602
178.509085	7259.816523	25.533619
178.594483	7259.824950	25.538637
178.659312	7258.983705	25.543655
178.856830	7266.432082	25.548672
179.329407	7261.016351	25.553690
179.073084	7267.763609	25.558707
179.053431	7286.564773	25.563725
179.405966	7290.639580	25.568743
179.496589	7288.888547	25.573760
180.007997	7305.913320	25.578778
179.943519	7319.979276	25.583795
180.547790	7309.593186	25.588813
180.150483	7332.926341	25.593831
180.218316	7344.775098	25.598848
180.956756	7346.598561	25.603866
180.734228	7351.391413	25.608883
180.889246	7356.743331	25.613901
181.195061	7356.497869	25.618919
181.232932	7370.644338	25.623936
181.545059	7368.224556	25.628954
181.451072	7375.281970	25.633971
181.861072	7382.189788	25.638989
182.090672	7401.376263	25.644007
182.206837	7406.490466	25.649024
182.472320	7397.169452	25.654042
182.296115	7432.746521	25.659059
182.514667	7426.805476	25.664077
182.574992	7430.328108	25.669095
182.925962	7450.334093	25.674112
183.194535	7462.192643	25.679130
183.360021	7476.316505	25.684148
183.679148	7490.389132	25.689165
183.718883	7495.556469	25.694183
183.864721	7502.508035	25.699200
184.373669	7503.584386	25.704218
184.170687	7532.936321	25.709236
184.334653	7537.051491	25.714253
184.395548	7548.331822	25.719271
184.492799	7553.785086	25.724288
184.756356	7579.405350	25.729306
185.029840	7594.911167	25.734324
185.275376	7603.506401	25.739341
185.305520	7614.585524	25.744359
185.457721	7631.603418	25.749376
185.881689	7637.070720	25.754394
186.012185	7652.494740	25.759412
186.434588	7659.104058	25.764429
186.671978	7678.814495	25.769447
186.908634	7683.628668	25.774464
187.203702	7691.068001	25.779482
187.311297	7696.859600	25.784500
187.621404	7704.911882	25.789517
187.571944	7715.920362	25.794535
187.530110	7721.532779	25.799552
188.074780	7720.228647	25.804570
188.000865	7744.892645	25.809588
188.448567	7750.124076	25.814605
188.356415	7745.772370	25.819623
188.747679	7770.019164	25.824640
189.129033	7772.338697	25.829658
189.366694	7775.636415	25.834676
189.466066	7772.955409	25.839693
189.625945	7779.579096	25.844711
189.700463	7792.389502	25.849728
189.962470	7800.672193	25.854746
190.113460	7805.985572	25.859764
190.263427	7800.535315	25.864781
190.616055	7813.136153	25.869799
190.687961	7829.904256	25.874816
190.722500	7840.484746	25.879834
191.040044	7837.281075	25.884852
191.234332	7828.717113	25.889869
191.303169	7840.284399	25.894887
191.334674	7855.461984	25.899904
191.767250	7850.377801	25.904922
191.945526	7841.446547	25.909940
191.852883	7864.928677	25.914957
192.285750	7871.722129	25.919975
192.170765	7883.489511	25.924992
192.738299	7883.284153	25.930010
192.776517	7907.994674	25.935028
192.885943	7909.789448	25.940045
193.036126	7907.711337	25.945063
192.888491	7925.844394	25.950080
193.782749	7937.991114	25.955098
193.959182	7945.402276	25.960116
193.422487	7949.577334	25.965133
193.898912	7971.662269	25.970151
194.097088	7981.842996	25.975168
194.258446	7988.697494	25.980186
194.400359	8001.614582	25.985204
194.674412	8003.975653	25.990221
194.789485	8023.078105	25.995239
194.943647	8044.530714	26.000256
195.526408	8048.366795	26.005274
195.702324	8065.185859	26.010292
196.100134	8062.307318	26.015309
196.748039	8047.497299	26.020327
197.274750	8045.134874	26.025344
197.579371	8039.366754	26.030362
197.596759	8043.915409	26.035380
197.626308	8038.660529	26.040397
198.077921	8042.941656	26.045415
197.763262	8039.498402	26.050432
197.905760	8034.293976	26.055450
197.863919	8028.828576	26.060468
198.096867	8029.437884	26.065485
198.308108	8038.307171	26.070503
198.047777	8059.693687	26.075520
198.140046	8059.163569	26.080538
198.413526	8073.486784	26.085556
198.398775	8092.248836	26.090573
198.896935	8099.903083	26.095591
198.885140	8120.341977	26.100608
198.885754	8126.907012	26.105626
199.427863	8150.489840	26.110644
199.332850	8159.082640	26.115661
199.595347	8171.578150	26.120679
199.513113	8205.144910	26.125696
200.177042	8200.566692	26.130714
199.979311	8224.392312	26.135732
200.103866	8235.292380	26.140749
200.631050	8254.402214	26.145767
200.568360	8276.830085	26.150784
201.112772	8290.776665	26.155802
201.318947	8304.866104	26.160820
201.305033	8316.200648	26.165837
201.844847	8318.644520	26.170855
202.009081	8327.313729	26.175872
202.401194	8339.254008	26.180890
202.573317	8354.444699	26.185908
202.613213	8363.072766	26.190925
202.739497	8361.505570	26.195943
202.657996	8384.106574	26.200960
202.887713	8389.624799	26.205978
203.162615	8409.200775	26.210996
202.848993	8431.260472	26.216013
203.674777	8436.416527	26.221031
203.693984	8454.221053	26.226048
203.819657	8462.202818	26.231066
204.308453	8484.076434	26.236084
204.629574	8497.672429	26.241101
205.126386	8507.405756	26.246119
205.230747	8531.668053	26.251136
205.333798	8530.821431	26.256154
205.595223	8541.264732	26.261172
205.458083	8569.341646	26.266189
205.568605	8570.721616	26.271207
205.854325	8583.768158	26.276224
206.172115	8604.880320	26.281242
206.374254	8606.623019	26.286260
206.405636	8629.383455	26.291277
206.812823	8629.589646	26.296295
206.799738	8644.593754	26.301312
207.284246	8660.665498	26.306330
207.621931	8673.808102	26.311348
207.880333	8688.839795	26.316365
208.211826	8694.123142	26.321383
208.288641	8712.093095	26.326400
208.644905	8706.942888	26.331418
208.663169	8722.483878	26.336436
208.701128	8727.891153	26.341453
209.358675	8721.967356	26.346471
209.274916	8749.216504	26.351488
209.074879	8755.578510	26.356506
209.482927	8771.734961	26.361524
209.461516	8788.269556	26.366541
209.748411	8798.317870	26.371559
209.747191	8826.137119	26.376576
210.027954	8834.390641	26.381594
210.359554	8846.910718	26.386612
210.043960	8864.544436	26.391629
210.652898	8884.246021	26.396647
210.604482	8897.357911	26.401664
210.858970	8923.255388	26.406682
211.434771	8936.514110	26.411700
211.462439	8961.208376	26.416717
211.814170	8974.025177	26.421735
212.256065	8995.570600	26.426752
212.025059	9002.043884	26.431770
212.567836	9017.309545	26.436788
212.830185	9036.230453	26.441805
212.861396	9028.461051	26.446823
213.193091	9059.323910	26.451840
213.331974	9067.011146	26.456858
213.556214	9072.235785	26.461876
213.589440	9097.134390	26.466893
214.103140	9098.575653	26.471911
214.440872	9120.297219	26.476928
214.495685	9127.266809	26.481946
214.786501	9138.780823	26.486964
214.864862	9155.646569	26.491981
215.130288	9158.826851	26.496999
215.135431	9172.080356	26.502016
215.562931	9184.660583	26.507034
216.463226	9173.116812	26.512052
216.239071	9182.749107	26.517069
216.615581	9201.151125	26.522087
216.775540	9211.399380	26.527104
216.798532	9216.084821	26.532122
217.272464	9212.518720	26.537140
217.589243	9230.279089	26.542157
217.716100	9227.865338	26.547175
218.278902	9230.070008	26.552192
218.339806	9232.741875	26.557210
218.557585	9234.220492	26.562228
218.381338	9241.467387	26.567245
218.488828	9253.618643	26.572263
218.719230	9269.229079	26.577280
219.156741	9283.903474	26.582298
219.465247	9292.033208	26.587316
219.282870	9303.640099	26.592333
219.651245	9313.442042	26.597351
219.903415	9321.941203	26.602368
220.004486	9333.964092	26.607386
219.998209	9346.044239	26.612404
220.054604	9356.780889	26.617421
220.254929	9368.695907	26.622439
220.345039	9389.937550	26.627456
220.466133	9398.723646	26.632474
220.827471	9415.497748	26.637492
221.008908	9444.945988	26.642509
221.545369	9463.681689	26.647527
221.669307	9475.549553	26.652544
221.770175	9497.738328	26.657562
222.277344	9504.197240	26.662580
222.350013	9518.608549	26.667597
223.005534	9535.566865	26.672615
223.861570	9533.266618	26.677632
223.743160	9539.098109	26.682650
224.416030	9528.547684	26.687668
224.155058	9531.121787	26.692685
224.919226	9526.367051	26.697703
224.932561	9519.817302	26.702720
224.698572	9536.936705	26.707738
225.131760	9545.874207	26.712756
225.075844	9559.256621	26.717773
225.124362	9567.150149	26.722791
225.722558	9571.208071	26.727808
225.598675	9570.547096	26.732826
225.559302	9573.645813	26.737844
225.357350	9597.654104	26.742861
225.435033	9602.008679	26.747879
226.118585	9623.328395	26.752896
226.180686	9643.900419	26.757914
226.122212	9673.475888	26.762932
226.588865	9687.148926	26.767949
226.514843	9703.327360	26.772967
227.021598	9725.222360	26.777984
227.241188	9746.152286	26.783002
227.357793	9756.821386	26.788020
227.659886	9778.395339	26.793037
227.652858	9801.467844	26.798055
228.548142	9816.119758	26.803072
228.607807	9829.298650	26.808090
229.035137	9842.204880	26.813108
229.299569	9855.557343	26.818125
229.687762	9866.172208	26.823143
229.554526	9875.982083	26.828160
229.470242	9902.778914	26.833178
230.028956	9905.095701	26.838196
230.129013	9933.451356	26.843213
230.166511	9949.422216	26.848231
230.421673	9958.345847	26.853248
230.564944	9982.819528	26.858266
230.910637	9999.935975	26.863284
231.355348	10016.084779	26.868301
231.899159	10027.443457	26.873319
232.426813	10041.112997	26.878336
232.282930	10071.978201	26.883354
232.561720	10067.281396	26.888372
232.656643	10073.854677	26.893389
233.118157	10097.813480	26.898407
233.210539	10095.918216	26.903424
233.337772	10116.362451	26.908442
233.262893	10128.906690	26.913460
233.666495	10142.062901	26.918477
233.899867	10175.390141	26.923495
234.363347	10176.665201	26.928512
234.477602	10205.690030	26.933530
234.831886	10204.878820	26.938548
234.836669	10233.463113	26.943565
235.257759	10241.072123	26.948583
235.542863	10256.384457	26.953600
235.329914	10278.555349	26.958618
235.737308	10298.294864	26.963636
235.871207	10314.803621	26.968653
236.053364	10324.717370	26.973671
236.294119	10339.474142	26.978688
236.608349	10373.488589	26.983706
236.795999	10381.240343	26.988724
236.962343	10395.406175	26.993741
236.908677	10415.227606	26.998759
237.469159	10423.538154	27.003776
237.543549	10440.284378	27.008794
237.589276	10462.269687	27.013812
237.962515	10483.262323	27.018829
238.242922	10499.540939	27.023847
238.378621	10514.559788	27.028864
238.552671	10549.081786	27.033882
238.962412	10555.426436	27.038900
239.485906	10581.603028	27.043917
239.580619	10600.820614	27.048935
239.754641	10625.533235	27.053952
239.741177	10638.647756	27.058970
240.292206	10656.372863	27.063988
240.604353	10672.615912	27.069005
240.645384	10693.093559	27.074023
240.846844	10704.570683	27.079040
241.016922	10732.798228	27.084058
241.639376	10753.188780	27.089076
241.897700	10762.285140	27.094093
241.812256	10795.758230	27.099111
242.397513	10798.595101	27.104128
242.892023	10819.429567	27.109146
243.343445	10815.616016	27.114164
243.516716	10839.011597	27.119181
243.535724	10863.292046	27.124199
244.269938	10859.744287	27.129216
243.911795	10866.573518	27.134234
244.222394	10892.567758	27.139252
244.389802	10898.975977	27.144269
244.631110	10935.093710	27.149287
244.973134	10936.884435	27.154304
245.009321	10954.850556	27.159322
245.291594	10967.094570	27.164340
245.411420	10983.998647	27.169357
245.479070	11003.571690	27.174375
246.324596	11019.883564	27.179392
246.115301	11045.116828	27.184410
246.457918	11053.406183	27.189428
246.772480	11072.173363	27.194445
246.938295	11098.248098	27.199463
247.162007	11105.594653	27.204480
247.853059	11128.048085	27.209498
247.947059	11136.037895	27.214516
248.442727	11152.686665	27.219533
248.275571	11171.973284	27.224551
248.900058	11175.784260	27.229568
248.920054	11194.875005	27.234586
249.501320	11203.807800	27.239604
249.625243	11216.973921	27.244621
249.540195	11235.056311	27.249639
249.701322	11233.744181	27.254656
250.084958	11261.213783	27.259674
250.070716	11264.417454	27.264692
250.356037	11286.845485	27.269709
250.347259	11301.482413	27.274727
251.027259	11314.835844	27.279744
251.467249	11330.850848	27.284762
251.212864	11339.377987	27.289780
251.433515	11363.694388	27.294797
251.560576	11385.661383	27.299815
251.780382	11392.776908	27.304832
252.334147	11421.221231	27.309850
252.619685	11423.614868	27.314868
253.044476	11442.953670	27.319885
253.370615	11461.453458	27.324903
253.742749	11469.405011	27.329920
254.220392	11481.364861	27.334938
254.794724	11479.893378	27.339956
255.281068	11467.586855	27.344973
255.207270	11479.707412	27.349991
255.419093	11475.518875	27.355008
255.375883	11484.417580	27.360026
255.840534	11501.285765	27.365044
256.122987	11500.971374	27.370061
256.167034	11514.427342	27.375079
256.656893	11515.282546	27.380096
256.954947	11533.226499	27.385114
256.924852	11535.806239	27.390132
257.554869	11537.461798	27.395149
257.518747	11557.799433	27.400167
257.977299	11558.043936	27.405184
258.288192	11563.931737	27.410202
257.996314	11562.712844	27.415220
258.584789	11585.426127	27.420237
258.381111	11587.336584	27.425255
258.861324	11602.819105	27.430272
259.011403	11624.424261	27.435290
259.108695	11633.597585	27.440308
259.836468	11644.867956	27.445325
259.608461	11663.923068	27.450343
259.826120	11685.401640	27.455360
259.842444	11698.970808	27.460378
260.032359	11716.897388	27.465396
260.576007	11733.616878	27.470413
260.336531	11762.652871	27.475431
260.571771	11782.138813	27.480448
260.845697	11807.083209	27.485466
261.376430	11826.124229	27.490484
261.545980	11856.428539	27.495501
261.916739	11875.124989	27.500519
261.819063	11901.240747	27.505536
262.443201	11924.162157	27.510554
262.763288	11943.244380	27.515572
263.147930	11964.321872	27.520589
263.173995	11977.918860	27.525607
263.832010	11991.416109	27.530624
264.310462	12010.831109	27.535642
264.644232	12037.527688	27.540660
264.811496	12040.497353	27.545677
264.779516	12049.627976	27.550695
264.926162	12067.820236	27.555712
265.528172	12083.628786	27.560730
265.585147	12087.359070	27.565748
265.681057	12107.261587	27.570765
265.955691	12122.523371	27.575783
266.296419	12132.524211	27.580800
266.540846	12150.429824	27.585818
266.627191	12173.735063	27.590836
266.936382	12184.698684	27.595853
267.084101	12211.125729	27.600871
267.559317	12224.373097	27.605888
267.886078	12245.683749	27.610906
267.881999	12265.524290	27.615924
268.429493	12283.860516	27.620941
268.323647	12310.027078	27.625959
268.844416	12326.962410	27.630976
268.986705	12350.530166	27.635994
269.019602	12367.333542	27.641012
269.395288	12388.455557	27.646029
269.674769	12409.941239	27.651047
270.137959	12431.565720	27.656064
270.638488	12458.230948	27.661082
270.636021	12476.862282	27.666100
271.058277	12484.114891	27.671117
271.451952	12512.493117	27.676135
271.649644	12528.521841	27.681152
271.592408	12538.949450	27.686170
271.931357	12563.990397	27.691188
272.264277	12580.916403	27.696205
272.621514	12601.664619	27.701223
272.928295	12623.694688	27.706240
273.214737	12642.039309	27.711258
273.316853	12658.708392	27.716276
273.507397	12676.945942	27.721293
273.804010	12704.527473	27.726311
274.278362	12720.353299	27.731328
274.760729	12744.988150	27.736346
274.942819	12761.250633	27.741364
275.629662	12784.148495	27.746381
276.139954	12796.055088	27.751399
275.557357	12808.884763	27.756416
276.276161	12825.260617	27.761434
276.344555	12841.272006	27.766452
276.748519	12867.641833	27.771469
276.890289	12879.687620	27.776487
277.066962	12905.395933	27.781504
277.421466	12920.446048	27.786522
277.238192	12946.849595	27.791540
277.826566	12966.155807	27.796557
278.175359	12989.863334	27.801575
278.285830	13013.597472	27.806592
278.781795	13031.207121	27.811610
278.694996	13054.382693	27.816628
279.093845	13057.706076	27.821645
279.337112	13092.196358	27.826663
279.238869	13108.063774	27.831680
280.026287	13121.560991	27.836698
279.928456	13152.824397	27.841716
280.368288	13167.997656	27.846733
280.750093	13186.062852	27.851751
281.078370	13206.362019	27.856768
281.183294	13224.950091	27.861786
281.465418	13247.400125	27.866804
281.853918	13255.325710	27.871821
282.357895	13279.303157	27.876839
282.608368	13301.651753	27.881856
283.144040	13302.258010	27.886874
283.232181	13321.630043	27.891892
283.621657	13337.943625	27.896909
284.323736	13350.151386	27.901927
284.494283	13371.600392	27.906944
284.584556	13375.420737	27.911962
284.970587	13394.494666	27.916980
285.368318	13397.077276	27.921997
285.890180	13409.997867	27.927015
285.616442	13426.797462	27.932032
286.399409	13431.076245	27.937050
286.277138	13445.138118	27.942068
286.940464	13460.626514	27.947085
287.007199	13468.069397	27.952103
287.158188	13492.046274	27.957120
287.206509	13507.671120	27.962138
287.286245	13527.459304	27.967156
287.765067	13531.657988	27.972173
287.853314	13559.502365	27.977191
288.170458	13583.141570	27.982208
288.682078	13609.132925	27.987226
288.685131	13629.260736	27.992244
289.135700	13643.000249	27.997261
289.530328	13662.628211	28.002279
288.959285	13691.138195	28.007296
289.930249	13705.153384	28.012314
289.850713	13737.033504	28.017332
290.238381	13759.815312	28.022349
290.923523	13782.950225	28.027367
291.295223	13804.048668	28.032384
291.773755	13809.943198	28.037402
291.794564	13847.536975	28.042420
291.964421	13852.794382	28.047437
292.458188	13882.443228	28.052455
292.407253	13899.332205	28.057472
293.028825	13914.045142	28.062490
293.441769	13935.518199	28.067508
293.883345	13932.097882	28.072525
294.233249	13956.655539	28.077543
294.410424	13977.943849	28.082560
294.802739	13980.148581	28.087578
294.926522	14007.153548	28.092596
295.325242	14029.235941	28.097613
295.686436	14025.601109	28.102631
295.640396	14054.792664	28.107648
295.880225	14053.869723	28.112666
295.797035	14082.655246	28.117684
296.218820	14093.210860	28.122701
296.690635	14115.472429	28.127719
296.490639	14141.293142	28.132736
296.958012	14160.427194	28.137754
297.205504	14187.338491	28.142772
297.657848	14214.456401	28.147789
297.908067	14229.842274	28.152807
298.057517	14252.474739	28.157824
298.705401	14276.662754	28.162842
298.484739	14306.675056	28.167860
298.989440	14329.656138	28.172877
299.218998	14348.003318	28.177895
299.440256	14380.158906	28.182912
299.821547	14395.391012	28.187930
300.333219	14427.538395	28.192948
300.779367	14451.737390	28.197965
301.035011	14479.866633	28.202983
301.261703	14502.561844	28.208000
301.589545	14512.509136	28.213018
301.716578	14539.532358	28.218036
302.075556	14568.861572	28.223053
302.424926	14589.333196	28.228071
302.579653	14627.396708	28.233088
303.165191	14642.548387	28.238106
303.484704	14670.054441	28.243124
303.270023	14700.853308	28.248141
304.018404	14718.255716	28.253159
304.165241	14751.022051	28.258176
304.177938	14768.866512	28.263194
304.335999	14801.882397	28.268212
305.160359	14823.732872	28.273229
306.125724	14840.253953	28.278247
305.936469	14870.734600	28.283264
306.513204	14886.921981	28.288282
306.764111	14907.456171	28.293300
306.638359	14930.463260	28.298317
307.381093	14951.520779	28.303335
307.315682	14974.314319	28.308352
307.659442	14999.609925	28.313370
308.120916	15010.487644	28.318388
308.603412	15047.449064	28.323405
309.168340	15058.125518	28.328423
309.203512	15088.757014	28.333440
309.738008	15091.311923	28.338458
310.143298	15113.371116	28.343476
310.611537	15112.780152	28.348493
310.935954	15126.720409	28.353511
310.984838	15146.439431	28.358528
311.346907	15152.636859	28.363546
311.627819	15169.017036	28.368564
311.848901	15188.532024	28.373581
312.093752	15182.511251	28.378599
312.325522	15205.554567	28.383616
312.582150	15210.659070	28.388634
312.782671	15229.280687	28.393652
313.092613	15249.753475	28.398669
313.535589	15281.292442	28.403687
313.091702	15304.349415	28.408704
313.855101	15308.327878	28.413722
314.028068	15334.803139	28.418740
313.964099	15364.036250	28.423757
314.528828	15379.363310	28.428775
314.393916	15411.926194	28.433792
314.814588	15444.600961	28.438810
315.252526	15474.537436	28.443828
315.400464	15509.970754	28.448845
315.762248	15528.946896	28.453863
315.722955	15576.260234	28.458880
316.122792	15606.612231	28.463898
316.741259	15643.461792	28.468916
316.698303	15675.987155	28.473933
317.598413	15696.593414	28.478951
317.999398	15729.528385	28.483968
318.330668	15762.700098	28.488986
318.829372	15791.189702	28.494004
319.197997	15822.004518	28.499021
319.683772	15836.805515	28.504039
320.013011	15856.418270	28.509056
320.860530	15864.905346	28.514074
321.311792	15880.234065	28.519092
321.190168	15888.340051	28.524109
321.608578	15907.218080	28.529127
321.834119	15926.167811	28.534144
321.893714	15948.773694	28.539162
322.534456	15968.558179	28.544180
322.454170	15987.992699	28.549197
322.672686	16000.329855	28.554215
323.017558	16035.715871	28.559232
323.280154	16049.067970	28.564250
323.946884	16072.634041	28.569268
323.907839	16106.011756	28.574285
324.615780	16122.615608	28.579303
324.599215	16155.215521	28.584320
324.714268	16176.391397	28.589338
325.109750	16205.372578	28.594356
325.216207	16232.175498	28.599373
325.728918	16263.521917	28.604391
326.255116	16294.161792	28.609408
326.557511	16315.642220	28.614426
326.878023	16338.026594	28.619444
327.176248	16367.677259	28.624461
327.797017	16380.780060	28.629479
328.112894	16412.658697	28.634496
328.413886	16432.572725	28.639514
328.892631	16445.749787	28.644532
329.128722	16471.541408	28.649549
329.375615	16488.980487	28.654567
329.151463	16511.265910	28.659584
329.798886	16525.298565	28.664602
329.958005	16548.750415	28.669620
329.970631	16579.655369	28.674637
330.892657	16597.401113	28.679655
330.859299	16620.312139	28.684672
331.112852	16654.170150	28.689690
331.634977	16689.166448	28.694708
331.765721	16714.317043	28.699725
331.830022	16739.662901	28.704743
332.431854	16766.698603	28.709760
332.410768	16801.836253	28.714778
333.495702	16826.743035	28.719796
333.311153	16866.065082	28.724813
333.655233	16887.287512	28.729831
333.993525	16924.677870	28.734848
334.299740	16955.192314	28.739866
334.775742	16991.052307	28.744884
334.837244	17015.094800	28.749901
335.688827	17032.368441	28.754919
335.834701	17069.120949	28.759936
336.164997	17088.430393	28.764954
336.759082	17120.455117	28.769972
337.115376	17151.541075	28.774989
337.117206	17174.148505	28.780007
337.917965	17202.490613	28.785024
338.069118	17235.565655	28.790042
338.311156	17261.004506	28.795060
338.453446	17282.849578	28.800077
338.996772	17316.592581	28.805095
339.564117	17346.001253	28.810112
339.854590	17380.047283	28.815130
340.315716	17399.025249	28.820148
340.054875	17431.872281	28.825165
340.597801	17462.532673	28.830183
340.993427	17486.440758	28.835200
341.080004	17518.113337	28.840218
341.655369	17544.016844	28.845236
341.847550	17584.593834	28.850253
342.298770	17611.812495	28.855271
342.560302	17633.003631	28.860288
343.052252	17671.256723	28.865306
343.729265	17692.347080	28.870324
344.070992	17717.177490	28.875341
344.413303	17737.425586	28.880359
344.604693	17764.413090	28.885376
344.934308	17795.270339	28.890394
345.344686	17822.123044	28.895412
345.615081	17845.922901	28.900429
346.154413	17874.051998	28.905447
346.458395	17893.817429	28.910464
346.437077	17921.908008	28.915482
347.172278	17944.868583	28.920500
347.350730	17971.738429	28.925517
347.310231	17990.052173	28.930535
347.722765	18011.185508	28.935552
347.720100	18036.289425	28.940570
348.220301	18060.838826	28.945588
348.641399	18097.975110	28.950605
349.056623	18132.301337	28.955623
349.437750	18163.422373	28.960640
349.836529	18189.994485	28.965658
350.416355	18198.101897	28.970676
350.557308	18236.790280	28.975693
351.088176	18260.514616	28.980711
351.494885	18286.176154	28.985728
351.521206	18305.586346	28.990746
352.315741	18333.633478	28.995764
352.119628	18367.630077	29.000781
352.662161	18389.719229	29.005799
353.125982	18424.413567	29.010816
353.334869	18463.753131	29.015834
354.253028	18479.599223	29.020852
354.072035	18510.412880	29.025869
354.470512	18540.547609	29.030887
354.947630	18563.737642	29.035904
355.074444	18595.498129	29.040922
355.677981	18617.655053	29.045940
356.013140	18657.419493	29.050957
356.213728	18684.063012	29.055975
357.035348	18703.793833	29.060992
356.997298	18735.040296	29.066010
357.607581	18761.784810	29.071028
357.816333	18792.709363	29.076045
358.260926	18817.109756	29.081063
358.671721	18842.164829	29.086080
358.736627	18868.469632	29.091098
359.268925	18898.709327	29.096116
359.222876	18932.211159	29.101133
359.656491	18957.220650	29.106151
360.372022	18986.671812	29.111168
360.571139	19022.337293	29.116186
360.927549	19053.969992	29.121204
361.667281	19080.673950	29.126221
361.821001	19116.687854	29.131239
362.091486	19139.790010	29.136256
362.202075	19169.018602	29.141274
362.730270	19188.850743	29.146292
363.149646	19226.205756	29.151309
363.327947	19258.273587	29.156327
364.068663	19288.441451	29.161344
364.077941	19335.528740	29.166362
364.487012	19345.961829	29.171380
364.819997	19375.493588	29.176397
365.397433	19403.355966	29.181415
365.999024	19425.452140	29.186432
366.424987	19448.526826	29.191450
366.716920	19473.058884	29.196468
367.100781	19484.090241	29.201485
367.424784	19506.277227	29.206503
367.880457	19523.190720	29.211520
368.370634	19548.868206	29.216538
368.545714	19556.232476	29.221556
369.017144	19574.556662	29.226573
369.006333	19610.773139	29.231591
369.852566	19622.931838	29.236608
369.958862	19650.661052	29.241626
370.250060	19663.371672	29.246644
370.652725	19694.022196	29.251661
370.721380	19710.958192	29.256679
371.603199	19738.891183	29.261696
371.348608	19768.962649	29.266714
372.123596	19797.217925	29.271732
372.280626	19823.306477	29.276749
372.214800	19854.704893	29.281767
372.991617	19875.264530	29.286784
373.125784	19915.031123	29.291802
373.959978	19934.372084	29.296820
374.357565	19967.801889	29.301837
374.474229	20001.409227	29.306855
374.846184	20020.032506	29.311872
375.261637	20056.611278	29.316890
375.402258	20072.421076	29.321908
375.958107	20107.782540	29.326925
376.017810	20147.535994	29.331943
376.759331	20180.295999	29.336960
376.800451	20214.291478	29.341978
377.003235	20249.377190	29.346996
377.462965	20283.010789	29.352013
377.818095	20320.972841	29.357031
378.682606	20344.373516	29.362048
378.656160	20387.632026	29.367066
379.532283	20422.431269	29.372084
380.306155	20450.603246	29.377101
380.686142	20484.215332	29.382119
380.907100	20494.856758	29.387136
381.021357	20520.406733	29.392154
381.549146	20543.439245	29.397172
381.890990	20578.734282	29.402189
382.290357	20601.489653	29.407207
382.688701	20619.630221	29.412224
382.789604	20656.781475	29.417242
383.282793	20685.384498	29.422260
383.710808	20720.856709	29.427277
383.815680	20755.079461	29.432295
384.029238	20776.325036	29.437312
384.609750	20809.527841	29.442330
384.977607	20856.605075	29.447348
385.238554	20889.302170	29.452365
385.160134	20927.443456	29.457383
385.913682	20961.178173	29.462400
386.097444	20996.125246	29.467418
386.895370	21026.764218	29.472436
387.442713	21053.507722	29.477453
387.641948	21093.381909	29.482471
388.296153	21110.537982	29.487488
388.666031	21139.153605	29.492506
388.819558	21160.716416	29.497524
389.286866	21182.317464	29.502541
389.594492	21218.305362	29.507559
390.268334	21234.092790	29.512576
390.376766	21267.864809	29.517594
390.664966	21295.672292	29.522612
391.346522	21323.830621	29.527629
391.613144	21359.051185	29.532647
392.410362	21379.714696	29.537664
392.687302	21407.939225	29.542682
392.990193	21433.847326	29.547700
393.596521	21467.465614	29.552717
393.640039	21494.757977	29.557735
394.035270	21520.753106	29.562752
394.406095	21539.325994	29.567770
395.126963	21565.922218	29.572788
395.526643	21582.716908	29.577805
395.809849	21613.791886	29.582823
396.473619	21636.871280	29.587840
397.143650	21662.186479	29.592858
397.274883	21679.308369	29.597876
398.392789	21676.678464	29.602893
399.054469	21681.975156	29.607911
399.716672	21688.334234	29.612928
399.938530	21690.879057	29.617946
400.494086	21686.145304	29.622964
400.966968	21706.148941	29.627981
400.945546	21719.593496	29.632999
401.384338	21720.942839	29.638016
401.592981	21742.897765	29.643034
401.804101	21750.616469	29.648052
402.117712	21764.632244	29.653069
402.586688	21793.646757	29.658087
402.775022	21804.437613	29.663104
402.812847	21817.542018	29.668122
404.308023	21816.326370	29.673140
405.010341	21834.105653	29.678157
404.921146	21845.387331	29.683175
405.240773	21844.131378	29.688192
405.652301	21865.224800	29.693210
405.883813	21886.462712	29.698228
406.364508	21898.359314	29.703245
406.435405	21914.398665	29.708263
407.055626	21928.296421	29.713280
407.292238	21955.995937	29.718298
407.162939	21978.080649	29.723316
407.510248	21989.167645	29.728333
407.613235	22039.234708	29.733351
407.619425	22062.649492	29.738368
407.905287	22102.695155	29.743386
408.404788	22137.302240	29.748404
408.765035	22170.115339	29.753421
408.622756	22208.162774	29.758439
409.206782	22243.613557	29.763456
409.239703	22292.523750	29.768474
409.742776	22331.595743	29.773492
410.051836	22372.273218	29.778509
410.207265	22431.086094	29.783527
410.661917	22469.514770	29.788544
411.059987	22524.596111	29.793562
411.705849	22573.077908	29.798580
411.968893	22623.039395	29.803597
411.982359	22682.309812	29.808615
412.488315	22726.898987	29.813632
413.547333	22784.084478	29.818650
413.431436	22835.198696	29.823668
414.386178	22888.170695	29.828685
414.234980	22947.126494	29.833703
415.127527	22985.169220	29.838720
415.697124	23035.743218	29.843738
416.078899	23080.997484	29.848756
416.948908	23112.497826	29.853773
417.518930	23162.441240	29.858791
418.135746	23196.386058	29.863808
418.612912	23225.420009	29.868826
418.791195	23264.430263	29.873844
419.292663	23304.142924	29.878861
420.026888	23342.172351	29.883879
420.372513	23373.136863	29.888896
420.802709	23418.451328	29.893914
421.103069	23440.897320	29.898932
421.800148	23472.307780	29.903949
421.912612	23513.590575	29.908967
422.631806	23541.725600	29.913984
423.299828	23569.060660	29.919002
423.572619	23606.760947	29.924020
423.942268	23627.247416	29.929037
424.179372	23663.506533	29.934055
424.432774	23694.810895	29.939072
425.155479	23733.685930	29.944090
425.245334	23779.003662	29.949108
425.737835	23803.350203	29.954125
426.343353	23841.519489	29.959143
426.256833	23881.420227	29.964160
426.792693	23913.484260	29.969178
427.296845	23964.602555	29.974196
427.911854	23995.188217	29.979213
428.163328	24035.594760	29.984231
428.601768	24064.760874	29.989248
429.341812	24095.290571	29.994266
429.538132	24145.859832	29.999284
430.027952	24164.424720	30.004301
430.343986	24205.103410	30.009319
430.972632	24241.576371	30.014336
431.712538	24269.252507	30.019354
432.131686	24298.672619	30.024372
433.063629	24326.566392	30.029389
433.165145	24343.740004	30.034407
433.543955	24373.214732	30.039424
434.101120	24390.934951	30.044442
434.343541	24412.998469	30.049460
435.268457	24422.570138	30.054477
435.393202	24442.181333	30.059495
435.907429	24470.683874	30.064512
436.336129	24489.970993	30.069530
436.343086	24518.400833	30.074548
436.810712	24540.404226	30.079565
437.150407	24579.807119	30.084583
437.069250	24609.724232	30.089600
437.849120	24626.254403	30.094618
438.013193	24669.566699	30.099636
438.592162	24694.378988	30.104653
439.071025	24735.766477	30.109671
439.255109	24777.140384	30.114688
440.033484	24802.741904	30.119706
440.074045	24853.056205	30.124724
440.522736	24893.898271	30.129741
440.965292	24933.550332	30.134759
441.573627	24974.966653	30.139776
441.898982	25016.375387	30.144794
442.024473	25063.862937	30.149812
442.426460	25101.447699	30.154829
443.046556	25147.264620	30.159847
443.474061	25187.525501	30.164864
444.111952	25225.514119	30.169882
444.726840	25274.300554	30.174900
445.136744	25307.922829	30.179917
445.396344	25345.945219	30.184935
445.821750	25388.781394	30.189952
446.590564	25424.612382	30.194970
447.217889	25468.146871	30.199988
447.978348	25503.693402	30.205005
448.178751	25533.936062	30.210023
448.144179	25579.637157	30.215040
449.014275	25610.104920	30.220058
449.239545	25644.009409	30.225076
449.879876	25684.516508	30.230093
450.538958	25721.296028	30.235111
450.641907	25762.233995	30.240128
451.288942	25787.041076	30.245146
451.414972	25837.431500	30.250164
452.188496	25864.944340	30.255181
452.275464	25904.801988	30.260199
452.879833	25945.525032	30.265216
453.680780	25974.691235	30.270234
453.765895	26017.974845	30.275252
454.347222	26055.367042	30.280269
455.075878	26091.657337	30.285287
455.264239	26132.143038	30.290304
455.732506	26160.067413	30.295322
456.198321	26191.709941	30.300340
456.730967	26225.135748	30.305357
457.226930	26246.891964	30.310375
457.520386	26290.422002	30.315392
457.913504	26321.160129	30.320410
458.463430	26349.392468	30.325428
458.865827	26383.969887	30.330445
459.560195	26411.782260	30.335463
459.676598	26449.626028	30.340480
459.914327	26469.621131	30.345498
460.249649	26504.641227	30.350516
460.958707	26539.209515	30.355533
461.451675	26571.081662	30.360551
461.996361	26606.660290	30.365568
463.350042	26628.350491	30.370586
463.747029	26660.657239	30.375604
464.275576	26685.533436	30.380621
464.461382	26705.232209	30.385639
464.653226	26741.696949	30.390656
464.949649	26767.183804	30.395674
465.617996	26802.385482	30.400692
465.891181	26842.104694	30.405709
466.042918	26872.701125	30.410727
466.466995	26925.681255	30.415744
467.112226	26947.173556	30.420762
467.598269	26987.724279	30.425780
468.051605	27024.148784	30.430797
468.492554	27065.151239	30.435815
468.839441	27102.431164	30.440832
469.598392	27144.163140	30.445850
470.062253	27178.845138	30.450868
470.729839	27204.751000	30.455885
471.295856	27241.394405	30.460903
471.281047	27281.833420	30.465920
472.153105	27313.886944	30.470938
472.114252	27361.137209	30.475956
472.648515	27387.278907	30.480973
473.442919	27428.397731	30.485991
473.615503	27473.087124	30.491008
473.999656	27503.909300	30.496026
474.601106	27554.767469	30.501044
475.230499	27592.914313	30.506061
475.817857	27612.064094	30.511079
475.730663	27665.909686	30.516096
476.728429	27695.142207	30.521114
477.250347	27733.230867	30.526132
477.523383	27768.280174	30.531149
478.186060	27810.940019	30.536167
478.647639	27846.659110	30.541184
478.802130	27885.451165	30.546202
479.045494	27933.989690	30.551220
479.863432	27980.241720	30.556237
480.664793	28012.741246	30.561255
480.874277	28061.399008	30.566272
481.304180	28090.820414	30.571290
482.061251	28126.874398	30.576308
482.085287	28165.851791	30.581325
482.891748	28200.519221	30.586343
483.101392	28235.979898	30.591360
483.338901	28266.867860	30.596378
483.848624	28306.812997	30.601396
484.243503	28347.351712	30.606413
484.170027	28384.728346	30.611431
484.880290	28439.273628	30.616448
485.313060	28481.653543	30.621466
485.704917	28539.738838	30.626484
486.481136	28582.615855	30.631501
487.084557	28621.941708	30.636519
487.897074	28659.206193	30.641536
488.516729	28694.928761	30.646554
489.026827	28740.508675	30.651572
489.176967	28773.572055	30.656589
490.172346	28812.134657	30.661607
490.507471	28856.220460	30.666624
491.158328	28897.145260	30.671642
491.379017	28931.940666	30.676660
492.005598	28977.562573	30.681677
492.451420	29023.656235	30.686695
492.486161	29064.317146	30.691712
493.429802	29094.288897	30.696730
494.051236	29153.279057	30.701748
494.249533	29183.744779	30.706765
494.852255	29223.568617	30.711783
495.013830	29268.940776	30.716800
495.557800	29310.766168	30.721818
496.221544	29356.276052	30.726836
496.718071	29402.099525	30.731853
497.208449	29428.851946	30.736871
497.859086	29497.937394	30.741888
498.149543	29530.116330	30.746906
498.480376	29577.036767	30.751924
498.890513	29624.772088	30.756941
499.606979	29671.281498	30.761959
500.556948	29710.879429	30.766976
502.439762	29715.955165	30.771994
503.228677	29726.172647	30.777012
503.740020	29752.060201	30.782029
504.470686	29755.491351	30.787047
504.811890	29773.144748	30.792064
505.477555	29784.338523	30.797082
506.040027	29788.321277	30.802100
506.366867	29807.376474	30.807117
506.593624	29818.823006	30.812135
506.824066	29838.884892	30.817152
507.103840	29868.765256	30.822170
507.389351	29885.013980	30.827188
507.897507	29908.965395	30.832205
508.210878	29946.581846	30.837223
508.277622	29975.801324	30.842240
508.669595	30009.750648	30.847258
509.375027	30036.026953	30.852276
509.420301	30073.703739	30.857293
509.648585	30104.450086	30.862311
510.154005	30134.411615	30.867328
510.517645	30176.734458	30.872346
511.073615	30220.847083	30.877364
511.424884	30280.065599	30.882381
511.892109	30304.331441	30.887399
512.216300	30364.459220	30.892416
512.895476	30416.965652	30.897434
513.491837	30456.687921	30.902452
513.959471	30506.887907	30.907469
514.704475	30549.176179	30.912487
515.304951	30588.231440	30.917504
515.592767	30641.757605	30.922522
516.056183	30682.311697	30.927540
516.517886	30745.218069	30.932557
516.930232	30785.994900	30.937575
517.255018	30843.389839	30.942592
517.873597	30895.776644	30.947610
519.021848	30946.889290	30.952628
519.288411	31000.531912	30.957645
519.640624	31042.925008	30.962663
520.121274	31090.724298	30.967680
520.724206	31147.704032	30.972698
521.574435	31194.209079	30.977716
521.700457	31247.211347	30.982733
522.819974	31278.946434	30.987751
522.941399	31327.186634	30.992768
523.474827	31370.970229	30.997786
524.178058	31419.226775	31.002804
524.275339	31468.862969	31.007821
524.926152	31515.676517	31.012839
525.537059	31579.129728	31.017856
525.867730	31633.817076	31.022874
526.784739	31679.821098	31.027892
526.839039	31730.998537	31.032909
527.742751	31777.403722	31.037927
528.164067	31837.366952	31.042944
528.486463	31884.850152	31.047962
529.237770	31929.450091	31.052980
529.720675	31987.473224	31.057997
530.391283	32039.527537	31.063015
531.070193	32080.243049	31.068032
531.386351	32140.892444	31.073050
532.286648	32188.818801	31.078068
532.677936	32239.357785	31.083085
533.047863	32279.048024	31.088103
533.948056	32332.088084	31.093120
534.132734	32380.820953	31.098138
535.015975	32428.689252	31.103156
535.046549	32491.128740	31.108173
535.939248	32522.825131	31.113191
536.332025	32561.248259	31.118208
536.684026	32609.594188	31.123226
537.385210	32661.065531	31.128244
537.896903	32701.449826	31.133261
538.567730	32743.979392	31.138279
539.005960	32788.869542	31.143296
539.232390	32836.093338	31.148314
540.003346	32876.952208	31.153332
540.214940	32926.282958	31.158349
540.504529	32984.009362	31.163367
541.609188	33021.837824	31.168384
542.211059	33072.560188	31.173402
543.334706	33098.311357	31.178420
544.027289	33133.852296	31.183437
545.002480	33165.374425	31.188455
545.523993	33193.396958	31.193472
545.934822	33231.065292	31.198490
546.455476	33266.569273	31.203508
546.864213	33308.029159	31.208525
546.978127	33334.351374	31.213543
547.717942	33370.597798	31.218560
547.956688	33420.181058	31.223578
548.810851	33458.535933	31.228596
549.405103	33501.095409	31.233613
549.833640	33537.885174	31.238631
550.524278	33583.835987	31.243648
550.417523	33624.670992	31.248666
551.166681	33657.289372	31.253684
551.505700	33712.406301	31.258701
551.918096	33761.313461	31.263719
552.511757	33807.879359	31.268736
552.911982	33862.266636	31.273754
553.739557	33912.553646	31.278772
554.283800	33959.911302	31.283789
554.739804	34012.535672	31.288807
555.699688	34058.112295	31.293824
555.971972	34113.094577	31.298842
556.250644	34169.515279	31.303860
556.903628	34218.234127	31.308877
557.203053	34275.939808	31.313895
558.031721	34319.056774	31.318912
558.635070	34382.479374	31.323930
559.401185	34426.530366	31.328948
559.863534	34483.154609	31.333965
560.468230	34527.877917	31.338983
561.168216	34578.896661	31.344000
561.746525	34624.091057	31.349018
562.611794	34671.078011	31.354036
563.264184	34720.745872	31.359053
563.524881	34764.290241	31.364071
564.228979	34809.105672	31.369088
564.513930	34852.953819	31.374106
564.946267	34905.061391	31.379124
565.485239	34957.393341	31.384141
565.975388	35000.955382	31.389159
567.778970	35025.005865	31.394176
568.209967	35072.985365	31.399194
568.906797	35093.036108	31.404212
569.627116	35120.729121	31.409229
569.841179	35149.112917	31.414247
570.562031	35178.477027	31.419264
570.998783	35210.959039	31.424282
571.181784	35243.181993	31.429300
571.513361	35277.549043	31.434317
572.020247	35321.724094	31.439335
572.659713	35353.377957	31.444352
572.946713	35414.532661	31.449370
573.339634	35449.829901	31.454388
573.366971	35497.444519	31.459405
574.192946	35552.212501	31.464423
574.963541	35599.499351	31.469440
575.283514	35655.786066	31.474458
575.823355	35703.781570	31.479476
576.299247	35764.685173	31.484493
576.910090	35829.242463	31.489511
577.441805	35881.532742	31.494528
577.803757	35947.717728	31.499546
578.526774	35997.338721	31.504564
579.376203	36064.178058	31.509581
579.741558	36126.450133	31.514599
580.337596	36182.585862	31.519616
580.840858	36242.807329	31.524634
581.863676	36293.999042	31.529652
582.888998	36346.350895	31.534669
583.347465	36390.463952	31.539687
584.108910	36435.641961	31.544704
584.511144	36501.969340	31.549722
585.315236	36542.448818	31.554740
585.879351	36587.084770	31.559757
586.659091	36632.976187	31.564775
588.202288	36654.850618	31.569792
588.950217	36677.934886	31.574810
589.975419	36712.024130	31.579828
590.370476	36744.165741	31.584845
590.651327	36772.705620	31.589863
591.300717	36790.700554	31.594880
591.457123	36823.119975	31.599898
591.805882	36853.771350	31.604916
592.290801	36896.768406	31.609933
592.810636	36951.719005	31.614951
593.328954	36988.588789	31.619968
593.752147	37035.558196	31.624986
594.124507	37079.872824	31.630004
594.772745	37129.906398	31.635021
595.028335	37183.764628	31.640039
595.874317	37228.201301	31.645056
596.288095	37290.685980	31.650074
596.731480	37344.137982	31.655092
597.314270	37398.851391	31.660109
597.554408	37455.746531	31.665127
598.394971	37513.361401	31.670144
598.652122	37577.220177	31.675162
599.350904	37622.977400	31.680180
599.448780	37686.650673	31.685197
600.310481	37740.054652	31.690215
601.345736	37786.846682	31.695232
601.523149	37843.667973	31.700250
602.286992	37892.792960	31.705268
604.037097	37928.216686	31.710285
604.773961	37968.823831	31.715303
605.410864	38002.758367	31.720320
606.075207	38047.011688	31.725338
606.352323	38083.734645	31.730356
606.826954	38125.727338	31.735373
607.102963	38178.956353	31.740391
608.211313	38225.037871	31.745408
608.253931	38272.378799	31.750426
608.554536	38314.907402	31.755444
609.801795	38354.390355	31.760461
609.962713	38417.075567	31.765479
610.454785	38465.405066	31.770496
611.102718	38530.854541	31.775514
611.511956	38589.796915	31.780532
612.443556	38636.874293	31.785549
612.497936	38704.080932	31.790567
613.275629	38750.235462	31.795584
613.741886	38812.370496	31.800602
614.742793	38873.070835	31.805620
615.381104	38932.748994	31.810637
615.997484	38994.772484	31.815655
616.434348	39042.153690	31.820672
617.341065	39111.542607	31.825690
617.605632	39174.732894	31.830708
618.395848	39237.174262	31.835725
618.727365	39308.275036	31.840743
619.707448	39364.757556	31.845760
619.931719	39425.996697	31.850778
620.714458	39495.465269	31.855796
621.404905	39552.801912	31.860813
621.397829	39630.350727	31.865831
622.339601	39693.635360	31.870848
623.003191	39766.348810	31.875866
623.457337	39831.447805	31.880884
624.630610	39901.702653	31.885901
624.752341	39961.400451	31.890919
625.949687	40019.295025	31.895936
627.011778	40064.050080	31.900954
627.480949	40113.819782	31.905972
628.590146	40163.831484	31.910989
629.157366	40220.742140	31.916007
630.101878	40265.752995	31.921024
631.025410	40310.436146	31.926042
632.404096	40327.203798	31.931060
633.491252	40354.451189	31.936077
634.148921	40383.709859	31.941095
634.806393	40410.183656	31.946112
635.133836	40423.270967	31.951130
635.252622	40447.288503	31.956148
635.842737	40457.817139	31.961165
636.254461	40497.674695	31.966183
636.864407	40526.972752	31.971200
637.492858	40551.716695	31.976218
638.042168	40582.071630	31.981236
638.956015	40601.969809	31.986253
638.936874	40645.905065	31.991271
639.689263	40677.508359	31.996288
640.131760	40712.157385	32.001306
640.583626	40754.239044	32.006324
641.383354	40794.454992	32.011341
641.985822	40838.209749	32.016359
642.364065	40883.722440	32.021376
642.727969	40929.335310	32.026394
643.195171	40990.828393	32.031412
644.084053	41039.338560	32.036429
644.282312	41098.048793	32.041447
645.231329	41141.963620	32.046464
645.705338	41198.100693	32.051482
645.959604	41264.640554	32.056500
646.615016	41312.863799	32.061517
647.095864	41378.421778	32.066535
647.804773	41448.788481	32.071552
648.348910	41515.472403	32.076570
648.899825	41589.810713	32.081588
649.419981	41657.615587	32.086605
649.728285	41724.476657	32.091623
650.753604	41795.586102	32.096640
651.620557	41865.664389	32.101658
652.050999	41947.066839	32.106676
653.116408	42006.279246	32.111693
653.778255	42073.855015	32.116711
654.540045	42139.547796	32.121728
655.213418	42205.737515	32.126746
655.734501	42274.033584	32.131764
656.719156	42330.203438	32.136781
657.266539	42406.861108	32.141799
657.945210	42468.136537	32.146816
658.755648	42529.372274	32.151834
659.250990	42597.143788	32.156852
659.860271	42652.954936	32.161869
660.125791	42719.795131	32.166887
660.762933	42780.983651	32.171904
661.833173	42849.674021	32.176922
662.450767	42923.190467	32.181940
663.536579	42984.995932	32.186957
663.638143	43061.724341	32.191975
664.552449	43121.992995	32.196992
665.322675	43186.130110	32.202010
666.062313	43255.830545	32.207028
666.674097	43319.024953	32.212045
667.081447	43384.826227	32.217063
667.501524	43452.357559	32.222080
668.139357	43525.535804	32.227098
668.628784	43588.731751	32.232116
669.634906	43640.340968	32.237133
670.484868	43704.845855	32.242151
671.123179	43776.088174	32.247168
672.097732	43826.734517	32.252186
672.504104	43885.392691	32.257204
673.212382	43938.400393	32.262221
673.484782	43994.247423	32.267239
673.976717	44059.239664	32.272256
675.003897	44129.686484	32.277274
675.686414	44200.115914	32.282292
676.432737	44260.402657	32.287309
677.001272	44333.579568	32.292327
677.506881	44401.362807	32.297344
678.500460	44462.812822	32.302362
678.764130	44531.906440	32.307380
679.492022	44593.569576	32.312397
680.134850	44666.691891	32.317415
680.578003	44745.067432	32.322432
681.337078	44813.890845	32.327450
681.789942	44897.338399	32.332468
682.701585	44960.607757	32.337485
683.811774	45045.080773	32.342503
684.374268	45113.248918	32.347520
685.793427	45157.944599	32.352538
686.614517	45227.422285	32.357556
687.767393	45289.300997	32.362573
688.479558	45335.933215	32.367591
689.063484	45387.731578	32.372608
690.075625	45432.322410	32.377626
690.719320	45491.853653	32.382644
691.437819	45538.185688	32.387661
691.618314	45589.944774	32.392679
692.263086	45649.709846	32.397696
693.408496	45701.344021	32.402714
693.994042	45756.903901	32.407732
694.599482	45805.816460	32.412749
695.513162	45867.994016	32.417767
696.201042	45916.253301	32.422784
697.129015	45966.682978	32.427802
697.449479	46019.023646	32.432820
698.247268	46069.524827	32.437837
698.778498	46119.021132	32.442855
699.004105	46188.370287	32.447872
699.955349	46229.533880	32.452890
700.323425	46288.871935	32.457908
700.956239	46353.225583	32.462925
701.746327	46410.483935	32.467943
702.652548	46466.114898	32.472960
703.476179	46522.021059	32.477978
703.841509	46595.425938	32.482996
704.965892	46655.585033	32.488013
705.851550	46722.625788	32.493031
706.077921	46774.765985	32.498048
706.892658	46825.635795	32.503066
707.572600	46894.672452	32.508084
708.033375	46941.560367	32.513101
708.903564	46991.888608	32.518119
709.297717	47047.612408	32.523136
710.011198	47104.800030	32.528154
710.694755	47161.585583	32.533172
711.846819	47210.806273	32.538189
712.222724	47271.320129	32.543207
712.442876	47332.903370	32.548224
713.412031	47387.265140	32.553242
713.975990	47460.840779	32.558260
714.623257	47522.568081	32.563277
715.202382	47593.573478	32.568295
715.775576	47666.151435	32.573312
716.605100	47733.662493	32.578330
716.660909	47813.659494	32.583348
717.496478	47892.422037	32.588365
718.730121	47962.185636	32.593383
718.991772	48048.701407	32.598400
720.074073	48122.749462	32.603418
720.755888	48199.568903	32.608436
721.407753	48283.442594	32.613453
721.914589	48357.068919	32.618471
722.775153	48446.239638	32.623488
723.491382	48514.219781	32.628506
723.879060	48599.613772	32.633524
724.994963	48686.495210	32.638541
725.874179	48759.805172	32.643559
726.514731	48849.113918	32.648576
727.275656	48921.127538	32.653594
727.932710	49005.231010	32.658612
728.579363	49082.220801	32.663629
729.580625	49157.377895	32.668647
730.243016	49245.161023	32.673664
731.112134	49312.185833	32.678682
731.644379	49404.259960	32.683700
732.774416	49485.911086	32.688717
733.898130	49558.607942	32.693735
734.300442	49640.432434	32.698752
735.208078	49702.933715	32.703770
735.953955	49779.279594	32.708788
736.656052	49847.147168	32.713805
737.790756	49914.993463	32.718823
738.304558	49989.300748	32.723840
739.290688	50050.402246	32.728858
740.256072	50133.054509	32.733876
740.913414	50192.094502	32.738893
741.806761	50246.019530	32.743911
742.435469	50319.394730	32.748928
742.857311	50384.039600	32.753946
743.911263	50444.465783	32.758964
744.540350	50514.809024	32.763981
745.272141	50580.427735	32.768999
745.943190	50642.237826	32.774016
746.714376	50706.926077	32.779034
747.323522	50780.915357	32.784052
747.877195	50830.121444	32.789069
749.016464	50893.060238	32.794087
749.491183	50951.213456	32.799104
750.073836	51002.905382	32.804122
750.957075	51072.244654	32.809140
750.970363	51147.450644	32.814157
752.061760	51213.702414	32.819175
752.748892	51287.687681	32.824192
753.377602	51366.709962	32.829210
753.931528	51434.746006	32.834228
754.304007	51527.866393	32.839245
755.411021	51605.750021	32.844263
756.138356	51684.404527	32.849280
756.906901	51751.953141	32.854298
757.642244	51830.856338	32.859316
758.464835	51909.297834	32.864333
759.430356	51987.022587	32.869351
760.179948	52062.910507	32.874368
761.125549	52138.060584	32.879386
761.677436	52222.846062	32.884404
762.225247	52307.007679	32.889421
763.261169	52378.300245	32.894439
764.274053	52459.153518	32.899456
764.526395	52535.204641	32.904474
765.552496	52607.800009	32.909492
766.466185	52701.676679	32.914509
766.916892	52774.051851	32.919527
767.581232	52860.432072	32.924544
768.635570	52944.089934	32.929562
769.951791	53019.380366	32.934580
770.400603	53100.831300	32.939597
771.354429	53167.967502	32.944615
771.764703	53252.770882	32.949632
772.537020	53327.123390	32.954650
773.406778	53403.524908	32.959668
773.844354	53503.257543	32.964685
775.047074	53573.707631	32.969703
775.687491	53651.251413	32.974720
776.782627	53730.102467	32.979738
777.451212	53812.607394	32.984756
778.173483	53896.041594	32.989773
779.326438	53959.689639	32.994791
780.047974	54037.449417	32.999808
780.642262	54121.217507	33.004826
781.861695	54190.565740	33.009844
782.621820	54254.416234	33.014861
784.571858	54311.044964	33.019879
786.653764	54341.116535	33.024896
787.468919	54377.301855	33.029914
788.709160	54404.085905	33.034932
788.839918	54449.174230	33.039949
789.820988	54474.004747	33.044967
790.386009	54504.450624	33.049984
790.961425	54542.656708	33.055002
791.246281	54576.341671	33.060020
791.278356	54613.213967	33.065037
791.835901	54654.377617	33.070055
792.219469	54720.369828	33.075072
793.010055	54780.224320	33.080090
793.894507	54832.721951	33.085108
793.717461	54911.786949	33.090125
794.706050	54972.295526	33.095143
795.459416	55046.503411	33.100160
795.846481	55119.586182	33.105178
796.488694	55205.090905	33.110196
796.795809	55295.387454	33.115213
797.487744	55367.425193	33.120231
798.190726	55469.746341	33.125248
799.092818	55552.487129	33.130266
800.021834	55653.213929	33.135284
800.432817	55755.037042	33.140301
801.437685	55846.639440	33.145319
802.076727	55938.849798	33.150336
802.488851	56037.719594	33.155354
803.695400	56139.901188	33.160372
804.498040	56243.470334	33.165389
805.429753	56335.225713	33.170407
806.329019	56429.133348	33.175424
807.535225	56525.085586	33.180442
808.848841	56605.558991	33.185460
809.320000	56707.201011	33.190477
810.402096	56795.740004	33.195495
811.469603	56882.886399	33.200512
812.021933	56964.881054	33.205530
813.453641	57047.155973	33.210548
814.176518	57121.332899	33.215565
815.706291	57189.320353	33.220583
816.643868	57264.275015	33.225600
817.266411	57327.779283	33.230618
818.556843	57392.178226	33.235636
819.025397	57465.655125	33.240653
820.159476	57523.819099	33.245671
821.278536	57587.428338	33.250688
821.708329	57652.208264	33.255706
822.544716	57720.295415	33.260724
822.798362	57788.387172	33.265741
823.638576	57849.449760	33.270759
824.098521	57938.475265	33.275776
824.909695	58015.088456	33.280794
825.668162	58079.375570	33.285812
826.377773	58179.330251	33.290829
826.775341	58265.737379	33.295847
827.787253	58348.230140	33.300864
828.227261	58438.407259	33.305882
829.174799	58538.632248	33.310900
829.839840	58634.990981	33.315917
831.013886	58715.044315	33.320935
832.116406	58810.668158	33.325952
832.721332	58894.797262	33.330970
833.890088	58971.149106	33.335988
834.190908	59055.055813	33.341005
835.082655	59126.025048	33.346023
836.139687	59215.132124	33.351040
836.385568	59298.129896	33.356058
837.118884	59382.067113	33.361076
837.638820	59467.532087	33.366093
838.603795	59553.826464	33.371111
839.871449	59646.880337	33.376128
840.640615	59734.700147	33.381146
842.136481	59810.608697	33.386164
842.740829	59900.640433	33.391181
843.567891	59980.596562	33.396199
844.437345	60060.072671	33.401216
845.135611	60156.964422	33.406234
846.546481	60221.874997	33.411252
847.467424	60302.581666	33.416269
848.225713	60374.154704	33.421287
849.338626	60453.647414	33.426304
850.237818	60541.349275	33.431322
851.291471	60612.254184	33.436340
851.495468	60691.308417	33.441357
852.910088	60754.357298	33.446375
853.812585	60839.565564	33.451392
854.448465	60917.187945	33.456410
855.483369	60988.703517	33.461428
856.065196	61080.159098	33.466445
856.696278	61155.784465	33.471463
857.477968	61237.167784	33.476480
858.163675	61326.590304	33.481498
859.227198	61401.828914	33.486516
860.060569	61492.817024	33.491533
860.755513	61575.693403	33.496551
861.787477	61662.883608	33.501568
862.256262	61753.599442	33.506586
863.317433	61847.928609	33.511604
864.284835	61946.321404	33.516621
865.028164	62037.004378	33.521639
866.048231	62124.324920	33.526656
866.520126	62220.259147	33.531674
867.702444	62303.155887	33.536692
868.857967	62399.433792	33.541709
869.215078	62494.134017	33.546727
870.304058	62582.317270	33.551744
871.091831	62680.613000	33.556762
872.007848	62769.680434	33.561780
873.154309	62858.705298	33.566797
874.141654	62936.902152	33.571815
875.245927	63021.169202	33.576832
875.843498	63114.915301	33.581850
876.649005	63195.681146	33.586868
877.815385	63283.681656	33.591885
878.563419	63376.647187	33.596903
879.810980	63456.810093	33.601920
880.446531	63541.327736	33.606938
881.105539	63606.404373	33.611956
881.897681	63688.282904	33.616973
882.741069	63766.187120	33.621991
883.687719	63842.398290	33.627008
884.347339	63921.431392	33.632026
885.299860	63996.195844	33.637044
886.075849	64076.587996	33.642061
886.600151	64176.193466	33.647079
887.693954	64253.586105	33.652096
888.202787	64347.545034	33.657114
888.994195	64433.699853	33.662132
890.059750	64530.400797	33.667149
890.775375	64636.060862	33.672167
891.806263	64727.737318	33.677184
892.359141	64834.229719	33.682202
893.390897	64927.707183	33.687220
894.204817	65020.663916	33.692237
895.146891	65136.754014	33.697255
895.990613	65231.624100	33.702272
896.510437	65349.226016	33.707290
897.701906	65453.358879	33.712308
898.638453	65563.006286	33.717325
899.475100	65667.395748	33.722343
900.765784	65765.497833	33.727360
901.476744	65875.230294	33.732378
902.452627	65984.137934	33.737396
903.147499	66088.542765	33.742413
904.166125	66201.433932	33.747431
905.202000	66293.154966	33.752448
906.166918	66404.482952	33.757466
907.237405	66505.081144	33.762484
908.103183	66603.811010	33.767501
909.181260	66703.461473	33.772519
910.504953	66796.901563	33.777536
911.450552	66900.414918	33.782554
912.465860	66995.528543	33.787572
913.716888	67079.000449	33.792589
914.668986	67177.037249	33.797607
915.785492	67253.841382	33.802624
916.684548	67341.249217	33.807642
917.561579	67433.556860	33.812660
918.240210	67515.024386	33.817677
919.197551	67614.458693	33.822695
920.319643	67690.909898	33.827712
920.901911	67779.703085	33.832730
922.173854	67872.480638	33.837748
923.199430	67951.551015	33.842765
924.056814	68040.257392	33.847783
924.733921	68129.043401	33.852800
925.873862	68210.105606	33.857818
926.681937	68296.767793	33.862836
927.707474	68382.764002	33.867853
928.437332	68476.489890	33.872871
929.687170	68551.477413	33.877888
930.527635	68639.879648	33.882906
931.467619	68721.171648	33.887924
932.483715	68785.615088	33.892941
932.888122	68877.701533	33.897959
933.749536	68952.973530	33.902976
934.368604	69038.746690	33.907994
935.340523	69113.186721	33.913012
936.184208	69204.819419	33.918029
936.778596	69297.661027	33.923047
938.028473	69374.572352	33.928064
938.926361	69475.143883	33.933082
939.517859	69573.003717	33.938100
940.499151	69666.745845	33.943117
941.281985	69776.934311	33.948135
942.506555	69870.581841	33.953152
942.930555	69972.671849	33.958170
943.647146	70077.350501	33.963188
944.829358	70172.661568	33.968205
945.618206	70293.599212	33.973223
946.813265	70398.582535	33.978240
947.926320	70501.488112	33.983258
948.772278	70618.918332	33.988276
949.809652	70717.603799	33.993293
950.990515	70812.570670	33.998311
952.432143	70906.365511	34.003328
953.723150	71007.286705	34.008346
954.981633	71099.904783	34.013364
955.985161	71189.252961	34.018381
956.796325	71278.967033	34.023399
958.185477	71348.313271	34.028416
959.257294	71438.909108	34.033434
959.938151	71530.363710	34.038452
961.176912	71606.502028	34.043469
961.635363	71697.999109	34.048487
962.545120	71784.565725	34.053504
963.385991	71890.655923	34.058522
964.066513	71988.848466	34.063540
964.836732	72088.651155	34.068557
965.974050	72179.814967	34.073575
967.005041	72271.665915	34.078592
968.212817	72367.602755	34.083610
969.213342	72467.238006	34.088628
969.720530	72567.325065	34.093645
971.077935	72670.740157	34.098663
972.070040	72762.725939	34.103680
972.600533	72863.448998	34.108698
973.657826	72958.275200	34.113716
974.780863	73058.190912	34.118733
975.590910	73166.510821	34.123751
976.804495	73258.729058	34.128768
977.484681	73366.836906	34.133786
978.118854	73475.287577	34.138804
979.644592	73570.964769	34.143821
980.307417	73686.198919	34.148839
981.109012	73790.656140	34.153856
982.231052	73896.522697	34.158874
982.774676	73992.907946	34.163892
983.842831	74093.090335	34.168909
984.293196	74208.746773	34.173927
985.230789	74306.050362	34.178944
986.198101	74398.603729	34.183962
987.130240	74525.257154	34.188980
987.997878	74631.319730	34.193997
989.290626	74748.128127	34.199015
990.244102	74854.260377	34.204032
991.355644	74964.387371	34.209050
992.354880	75078.033969	34.214068
993.394753	75181.544145	34.219085
993.890996	75298.375016	34.224103
995.483675	75408.775480	34.229120
996.377249	75520.861421	34.234138
997.206820	75638.235294	34.239156
998.619816	75737.802213	34.244173
999.479933	75856.626081	34.249191
1000.658348	75976.461771	34.254208
1001.851457	76082.726673	34.259226
1002.872217	76197.968797	34.264244
1003.822585	76307.111213	34.269261
1004.961254	76415.977774	34.274279
1005.917205	76523.502505	34.279296
1007.011684	76629.337229	34.284314
1008.030779	76749.025862	34.289332
1008.975926	76852.509087	34.294349
1009.923429	76973.499770	34.299367
1010.824234	77092.760499	34.304384
1011.819769	77201.723561	34.309402
1012.361085	77321.023854	34.314420
1013.742667	77427.550223	34.319437
1014.713596	77550.285051	34.324455
1015.746848	77675.886549	34.329472
1017.064972	77794.345484	34.334490
1017.478924	77924.477760	34.339508
1018.796481	78038.867720	34.344525
1019.662559	78154.455226	34.349543
1020.974608	78270.408567	34.354560
1022.334892	78388.902161	34.359578
1023.517485	78502.121554	34.364596
1024.841724	78604.004745	34.369613
1025.573066	78714.345266	34.374631
1027.271828	78818.932164	34.379648
1028.141003	78919.384939	34.384666
1029.674521	79017.210458	34.389684
1030.815590	79110.408699	34.394701
1032.321788	79200.717464	34.399719
1033.149783	79292.967616	34.404736
1034.124322	79384.436340	34.409754
1035.229961	79476.219634	34.414772
1036.264559	79569.057623	34.419789
1037.085856	79664.679666	34.424807
1038.032933	79756.280831	34.429824
1038.942204	79841.339640	34.434842
1039.431599	79945.916049	34.439860
1040.304599	80026.449059	34.444877
1041.192305	80129.951633	34.449895
1042.148255	80210.636518	34.454912
1043.626624	80303.027935	34.459930
1044.081898	80405.412260	34.464948
1045.380066	80488.863130	34.469965
1046.115636	80592.366930	34.474983
1047.198071	80697.775727	34.480000
1048.589498	80790.587723	34.485018
1049.017749	80901.715110	34.490036
1049.945472	81018.440408	34.495053
1051.152823	81124.918811	34.500071
1051.804604	81238.281892	34.505088
1052.923290	81354.542505	34.510106
1053.683153	81477.713576	34.515124
1055.200586	81587.982301	34.520141
1055.996828	81714.322498	34.525159
1056.991882	81836.345640	34.530176
1058.061371	81944.158775	34.535194
1058.957612	82068.398994	34.540212
1059.638602	82197.700120	34.545229
1060.993336	82332.679474	34.550247
1062.142918	82459.284062	34.555264
1063.423329	82581.702379	34.560282
1064.587099	82709.159695	34.565300
1065.908427	82834.708732	34.570317
1066.759718	82971.352807	34.575335
1067.369337	83089.840926	34.580352
1068.934596	83210.965808	34.585370
1069.855331	83333.553196	34.590388
1071.162563	83461.327334	34.595405
1072.114461	83591.896342	34.600423
1073.540978	83714.411817	34.605440
1074.765535	83827.406957	34.610458
1075.643187	83963.882568	34.615476
1077.103969	84071.119616	34.620493
1078.341629	84194.072556	34.625511
1078.900575	84318.133130	34.630528
1080.149720	84432.392107	34.635546
1081.126456	84566.971713	34.640564
1082.360482	84684.332546	34.645581
1083.370386	84804.024818	34.650599
1084.071975	84928.369762	34.655616
1085.551080	85057.593085	34.660634
1086.400868	85188.668712	34.665652
1087.845555	85312.423497	34.670669
1088.786376	85440.135079	34.675687
1089.564831	85578.887804	34.680704
1091.171100	85695.961068	34.685722
1092.057882	85821.268153	34.690740
1093.221160	85946.784918	34.695757
1094.327569	86071.059496	34.700775
1095.203664	86201.435300	34.705792
1096.201539	86315.333352	34.710810
1097.277938	86427.455352	34.715828
1098.643053	86533.076012	34.720845
1099.732694	86654.308854	34.725863
1100.341153	86773.576491	34.730880
1101.947436	86882.157755	34.735898
1103.026622	87001.914568	34.740916
1104.007052	87110.716673	34.745933
1104.917626	87226.783405	34.750951
1105.848292	87347.760893	34.755968
1107.050993	87465.211551	34.760986
1107.949996	87595.124238	34.766004
1109.408919	87716.911402	34.771021
1110.550536	87832.090968	34.776039
1111.163371	87964.037001	34.781056
1112.443285	88078.677350	34.786074
1113.498883	88212.609675	34.791092
1114.766114	88345.263392	34.796109
1116.172119	88464.875176	34.801127
1117.461769	88589.647392	34.806144
1118.409837	88712.311894	34.811162
1119.458983	88851.137537	34.816180
1120.709614	88971.206853	34.821197
1121.975620	89092.185040	34.826215
1122.884324	89215.010419	34.831232
1124.407811	89329.163322	34.836250
1125.363513	89464.529527	34.841268
1126.480149	89587.393503	34.846285
1128.033793	89713.597387	34.851303
1128.982817	89836.799311	34.856320
1130.195080	89965.531702	34.861338
1130.910187	90097.107620	34.866356
1131.916488	90224.109823	34.871373
1133.002938	90348.146554	34.876391
1133.903387	90482.983968	34.881408
1135.029219	90619.323200	34.886426
1136.349685	90765.308734	34.891444
1137.563699	90898.321665	34.896461
1138.549512	91034.742667	34.901479
1139.811918	91183.162510	34.906496
1140.672255	91305.665798	34.911514
1141.663264	91461.543119	34.916532
1142.592116	91614.231132	34.921549
1144.170310	91745.723945	34.926567
1144.843157	91893.078579	34.931584
1146.279581	92035.967616	34.936602
1147.219340	92192.655179	34.941620
1148.448557	92336.913660	34.946637
1149.591106	92485.348677	34.951655
1150.186731	92638.103080	34.956672
1151.627270	92785.398495	34.961690
1152.718267	92935.691634	34.966708
1153.950476	93100.934884	34.971725
1155.584305	93238.917299	34.976743
1156.618631	93390.765867	34.981760
1158.224388	93529.153036	34.986778
1159.549148	93654.125561	34.991796
1160.868297	93776.455699	34.996813
1162.186803	93897.920040	35.001831
1162.922940	94027.087085	35.006848
1164.134121	94140.599835	35.011866
1165.107259	94271.122192	35.016884
1165.825386	94413.957312	35.021901
1167.336056	94537.779284	35.026919
1168.377619	94673.233341	35.031936
1169.562008	94800.745853	35.036954
1170.499052	94942.594362	35.041972
1171.917558	95078.345160	35.046989
1172.968401	95221.512053	35.052007
1173.739791	95363.750129	35.057024
1174.797523	95507.050583	35.062042
1175.925624	95648.594828	35.067060
1176.971376	95800.147945	35.072077
1178.306947	95953.098304	35.077095
1179.774653	96114.328355	35.082112
1180.806688	96262.521341	35.087130
1181.776651	96407.366035	35.092148
1183.273499	96559.251051	35.097165
1184.531440	96713.901640	35.102183
1185.464471	96873.798742	35.107200
1187.268381	97012.827461	35.112218
1188.342790	97162.683388	35.117236
1189.583684	97310.356560	35.122253
1191.213626	97452.458585	35.127271
1192.260273	97604.099535	35.132288
1193.762112	97747.375172	35.137306
1195.162253	97907.635458	35.142324
1195.932590	98039.900996	35.147341
1197.238887	98172.366771	35.152359
1198.534177	98331.457312	35.157376
1199.880570	98466.505989	35.162394
1200.693669	98607.872018	35.167412
1201.531578	98763.780058	35.172429
1203.171484	98905.294827	35.177447
1204.304186	99060.126746	35.182464
1205.609400	99204.296885	35.187482
1206.886182	99353.091059	35.192500
1208.255039	99500.163290	35.197517
1209.696723	99646.136646	35.202535
1210.457329	99805.702027	35.207552
1211.943820	99950.227630	35.212570
1212.937075	100077.540693	35.217588
1213.994939	100241.642613	35.222605
1214.991647	100382.990337	35.227623
1216.089043	100542.456631	35.232640
1217.033229	100692.660006	35.237658
1218.681090	100853.464541	35.242676
1219.808706	101005.051753	35.247693
1220.935074	101161.651418	35.252711
1222.243225	101328.328095	35.257728
1223.404855	101480.564718	35.262746
1224.620896	101621.752224	35.267764
1225.522477	101773.304444	35.272781
1226.442539	101919.830623	35.277799
1227.805349	102068.951245	35.282816
1228.851934	102221.173021	35.287834
1229.999500	102382.403012	35.292852
1230.744819	102539.268654	35.297869
1232.176089	102695.216328	35.302887
1233.189909	102859.280390	35.307904
1234.370155	103026.919688	35.312922
1235.827063	103194.364324	35.317940
1237.065280	103378.487438	35.322957
1238.210938	103540.244562	35.327975
1239.459476	103710.010397	35.332992
1240.959375	103878.826242	35.338010
1242.678225	104039.324956	35.343028
1244.034614	104207.140805	35.348045
1245.652762	104362.614166	35.353063
1246.705445	104523.215744	35.358080
1248.009467	104689.746041	35.363098
1249.271164	104849.658452	35.368116
1250.504853	105004.849084	35.373133
1251.824739	105157.957627	35.378151
1253.298686	105324.731145	35.383168
1254.283092	105481.489676	35.388186
1255.763373	105648.023964	35.393204
1257.071520	105804.726817	35.398221
1258.489013	105964.634592	35.403239
1259.821993	106117.278884	35.408256
1261.052674	106274.085727	35.413274
1262.453684	106432.341118	35.418292
1263.539990	106603.064709	35.423309
1264.380562	106763.696082	35.428327
1265.767899	106932.171709	35.433344
1266.434330	107107.098395	35.438362
1268.112456	107264.650665	35.443380
1269.439105	107442.569695	35.448397
1271.016739	107605.918576	35.453415
1272.390285	107764.984550	35.458432
1273.837492	107924.843662	35.463450
1275.594728	108078.787375	35.468468
1276.653049	108231.248210	35.473485
1278.514501	108378.227757	35.478503
1279.740382	108535.144989	35.483520
1281.030683	108692.578330	35.488538
1282.259598	108836.243352	35.493556
1283.085682	109009.715277	35.498573
1284.708273	109151.161233	35.503591
1285.648567	109315.540707	35.508608
1286.515402	109478.844280	35.513626
1288.453317	109633.142549	35.518644
1289.622919	109791.032573	35.523661
1290.814132	109951.591304	35.528679
1292.027605	110108.868751	35.533696
1293.053652	110260.151066	35.538714
1294.071337	110411.074842	35.543732
1294.973145	110574.266206	35.548749
1296.396621	110722.671406	35.553767
1297.663887	110882.363259	35.558784
1299.053141	111037.953929	35.563802
1300.374024	111182.896729	35.568820
1301.564133	111343.426729	35.573837
1302.908334	111502.762210	35.578855
1303.858115	111660.439623	35.583872
1305.388918	111827.103127	35.588890
1306.301982	111993.245589	35.593908
1307.450104	112172.145227	35.598925
1308.764855	112342.043306	35.603943
1310.014520	112519.283421	35.608960
1311.701964	112697.771926	35.613978
1312.908403	112871.615670	35.618996
1313.904546	113051.710575	35.624013
1315.142361	113230.217382	35.629031
1316.539950	113408.263256	35.634048
1317.614052	113594.502977	35.639066
1318.896827	113793.764727	35.644084
1320.044018	113984.819686	35.649101
1321.364143	114174.113979	35.654119
1322.640271	114379.781818	35.659136
1324.013693	114572.217039	35.664154
1325.773458	114755.089630	35.669172
1327.177445	114947.231627	35.674189
1328.589186	115136.347633	35.679207
1330.552485	115312.810261	35.684224
1331.798343	115504.861331	35.689242
1333.185105	115674.137364	35.694260
1334.765921	115863.725743	35.699277
1336.355309	116042.842329	35.704295
1338.225024	116208.474342	35.709312
1339.655950	116378.653409	35.714330
1341.427756	116538.028804	35.719348
1342.499904	116710.799648	35.724365
1343.571196	116879.291747	35.729383
1344.958510	117051.039751	35.734400
1346.324865	117218.537460	35.739418
1347.517618	117385.690292	35.744436
1348.422113	117564.071626	35.749453
1349.839238	117740.435233	35.754471
1351.137948	117930.989180	35.759488
1352.185494	118113.213903	35.764506
1353.498624	118288.793657	35.769524
1354.758927	118477.337901	35.774541
1356.033751	118671.858491	35.779559
1357.223531	118852.362537	35.784576
1358.394785	119049.770777	35.789594
1359.898477	119239.288653	35.794612
1360.889812	119440.945573	35.799629
1362.043443	119642.122344	35.804647
1363.525707	119836.840296	35.809664
1364.810962	120044.280739	35.814682
1366.186593	120224.783745	35.819700
1367.179000	120429.246968	35.824717
1368.477862	120618.617434	35.829735
1369.961963	120808.187790	35.834752
1371.242298	120998.957066	35.839770
1372.691816	121192.512454	35.844788
1373.805371	121393.696359	35.849805
1375.366345	121590.542532	35.854823
1376.860992	121782.904553	35.859840
1378.009861	121989.672749	35.864858
1379.306531	122188.135874	35.869876
1380.921328	122394.263229	35.874893
1381.742720	122615.071088	35.879911
1383.347518	122809.056906	35.884928
1385.060959	123016.186659	35.889946
1386.387311	123226.963995	35.894964
1387.825872	123434.292669	35.899981
1389.307328	123645.010651	35.904999
1391.255412	123843.509228	35.910016
1392.514245	124060.370972	35.915034
1393.921039	124258.147997	35.920052
1395.357246	124472.286926	35.925069
1396.791408	124664.691988	35.930087
1398.312690	124871.790607	35.935104
1399.843536	125071.263885	35.940122
1401.569348	125261.866167	35.945140
1403.217392	125472.141292	35.950157
1404.537400	125677.302012	35.955175
1406.012108	125865.617702	35.960192
1406.876574	126076.756728	35.965210
1408.463854	126277.901983	35.970228
1410.017217	126486.337894	35.975245
1411.377435	126692.842620	35.980263
1412.616836	126890.994796	35.985280
1413.607650	127102.831055	35.990298
1415.219513	127313.480820	35.995316
1416.438013	127533.416964	36.000333
1417.831653	127744.092039	36.005351
1419.656655	127945.161077	36.010368
1421.192219	128161.517442	36.015386
1422.882324	128370.630002	36.020404
1424.235769	128582.027283	36.025421
1425.111582	128792.349243	36.030439
1426.883866	129001.352154	36.035456
1428.063549	129229.314508	36.040474
1429.150368	129435.756514	36.045492
1430.724361	129664.939318	36.050509
1432.039255	129887.019856	36.055527
1433.729529	130096.107353	36.060544
1435.244439	130313.573278	36.065562
1436.913709	130527.823697	36.070580
1438.432206	130734.941505	36.075597
1440.265303	130957.784354	36.080615
1441.545109	131155.479080	36.085632
1443.233224	131365.551922	36.090650
1444.820251	131554.129138	36.095668
1446.597265	131735.886390	36.100685
1447.594409	131916.818489	36.105703
1449.900717	132079.412952	36.110720
1451.147528	132257.000681	36.115738
1452.443459	132439.142967	36.120756
1454.244415	132604.684195	36.125773
1455.556424	132776.816612	36.130791
1457.300446	132952.213729	36.135808
1458.550083	133127.500425	36.140826
1460.126389	133302.153444	36.145844
1461.375762	133479.127515	36.150861
1462.579180	133663.573017	36.155879
1464.133294	133842.705608	36.160896
1465.802740	134014.383204	36.165914
1467.120347	134196.875342	36.170932
1468.533745	134383.484164	36.175949
1469.572427	134575.754353	36.180967
1471.090887	134774.221819	36.185984
1472.618261	134964.807703	36.191002
1473.843810	135160.663393	36.196020
1475.588041	135363.495977	36.201037
1476.533842	135580.927723	36.206055
1477.744185	135768.794190	36.211072
1479.424083	135978.395249	36.216090
1480.735953	136196.546390	36.221108
1482.086584	136409.472180	36.226125
1483.552978	136614.930001	36.231143
1484.904102	136830.887374	36.236160
1486.192397	137048.782486	36.241178
1488.473508	137245.029325	36.246196
1490.484929	137451.939739	36.251213
1491.842453	137668.269733	36.256231
1493.560444	137866.473027	36.261248
1495.046221	138079.465451	36.266266
1496.383806	138288.769850	36.271284
1497.820706	138486.933243	36.276301
1499.082312	138710.648961	36.281319
1500.850852	138914.515993	36.286336
1502.132665	139140.005936	36.291354
1503.826669	139350.515795	36.296372
1504.990901	139565.749707	36.301389
1506.118406	139790.622728	36.306407
1507.537655	140005.134912	36.311424
1509.438035	140224.641590	36.316442
1510.486337	140446.427081	36.321460
1512.232627	140663.109870	36.326477
1513.692997	140904.376099	36.331495
1515.222367	141126.964640	36.336512
1516.383649	141351.818567	36.341530
1517.898938	141580.242699	36.346548
1519.831591	141807.702371	36.351565
1521.012061	142046.474620	36.356583
1522.606626	142281.152496	36.361600
1523.708435	142518.470697	36.366618
1524.926387	142752.768410	36.371636
1526.207274	142963.888640	36.376653
1527.598797	143188.427965	36.381671
1529.462336	143415.086683	36.386688
1530.814688	143643.666142	36.391706
1532.128653	143876.309394	36.396724
1533.897524	144107.779388	36.401741
1535.240302	144350.320885	36.406759
1536.624551	144584.175094	36.411776
1537.916397	144828.033959	36.416794
1539.327169	145070.899820	36.421812
1540.966953	145318.940859	36.426829
1542.357630	145578.621711	36.431847
1544.023311	145836.638517	36.436864
1545.354661	146097.917558	36.441882
1547.266074	146345.162985	36.446900
1549.140950	146579.372427	36.451917
1550.676708	146837.772987	36.456935
1552.585718	147083.186511	36.461952
1554.557255	147325.993334	36.466970
1556.294025	147576.736770	36.471988
1558.013151	147815.049226	36.477005
1559.792851	148051.845309	36.482023
1561.933309	148280.941730	36.487040
1563.403293	148506.710861	36.492058
1565.092342	148740.344531	36.497076
1566.991731	148960.851080	36.502093
1568.363275	149205.808469	36.507111
1569.382057	149427.713130	36.512128
1571.042854	149655.120706	36.517146
1572.360125	149903.350065	36.522164
1574.336207	150134.780372	36.527181
1575.902030	150377.370402	36.532199
1577.644984	150604.898343	36.537216
1578.960266	150841.940757	36.542234
1580.370969	151081.923675	36.547252
1582.139037	151326.263518	36.552269
1583.333214	151568.262146	36.557287
1584.907676	151810.392317	36.562304
1586.944700	152033.813756	36.567322
1588.567720	152286.462652	36.572340
1590.389285	152525.858323	36.577357
1592.108802	152766.184784	36.582375
1593.763201	153002.516881	36.587392
1595.556338	153238.422898	36.592410
1597.013540	153482.942131	36.597428
1599.061660	153701.681860	36.602445
1600.807937	153932.769562	36.607463
1602.368818	154149.763835	36.612480
1604.589552	154362.927033	36.617498
1605.803789	154589.818209	36.622516
1607.283826	154808.642692	36.627533
1608.531422	155029.851196	36.632551
1610.438631	155251.983409	36.637568
1612.190799	155455.097026	36.642586
1613.084387	155670.571381	36.647604
1615.002128	155884.946128	36.652621
1616.534318	156100.245686	36.657639
1617.685557	156297.652429	36.662656
1619.634335	156498.724933	36.667674
1621.396100	156710.530242	36.672692
1622.970515	156925.473235	36.677709
1624.397727	157144.346439	36.682727
1625.853490	157346.757542	36.687744
1627.434223	157560.308659	36.692762
1628.651785	157799.951635	36.697780
1630.160800	158021.366152	36.702797
1631.451995	158258.439136	36.707815
1632.837749	158491.098524	36.712832
1634.366631	158730.432162	36.717850
1635.642279	158987.395969	36.722868
1637.582456	159230.573396	36.727885
1639.129217	159488.360113	36.732903
1640.888615	159747.763487	36.737920
1643.016414	159985.729758	36.742938
1644.375758	160237.439374	36.747956
1646.429556	160477.411665	36.752973
1647.919335	160725.819553	36.757991
1649.454322	160977.367018	36.763008
1651.292194	161233.294042	36.768026
1652.915686	161488.419951	36.773044
1654.536407	161738.437343	36.778061
1656.288043	161998.111977	36.783079
1657.639041	162260.210963	36.788096
1659.216735	162518.230260	36.793114
1660.568204	162782.780601	36.798132
1662.242107	163044.542292	36.803149
1663.645593	163326.234767	36.808167
1664.914032	163605.820209	36.813184
1666.940114	163884.577242	36.818202
1668.734381	164168.370181	36.823220
1670.224280	164443.804979	36.828237
1671.958197	164719.469423	36.833255
1674.327941	164995.859344	36.838272
1676.237182	165261.937051	36.843290
1678.102724	165545.069737	36.848308
1680.380032	165790.419277	36.853325
1682.574134	166045.435642	36.858343
1684.712357	166291.127647	36.863360
1686.988129	166530.267437	36.868378
1688.649967	166769.759917	36.873396
1690.101472	167002.222542	36.878413
1692.065903	167236.127191	36.883431
1693.458716	167470.999244	36.888448
1695.353594	167707.594135	36.893466
1696.720148	167960.509848	36.898484
1698.625115	168188.747413	36.903501
1700.377854	168421.564111	36.908519
1701.550348	168659.636830	36.913536
1702.934770	168891.195719	36.918554
1704.281268	169121.062326	36.923572
1706.024787	169347.417103	36.928589
1708.101978	169570.333468	36.933607
1709.499486	169800.868307	36.938624
1710.736894	170034.791369	36.943642
1712.290432	170274.411814	36.948660
1713.650756	170518.377243	36.953677
1715.042431	170751.620509	36.958695
1716.480459	171026.794241	36.963712
1718.034267	171281.693512	36.968730
1719.592754	171548.847521	36.973748
1721.155401	171817.829351	36.978765
1722.604099	172092.526804	36.983783
1724.210381	172371.463429	36.988800
1725.666550	172656.705161	36.993818
1727.106119	172947.812303	36.998836
1728.942812	173239.721134	37.003853
1730.916251	173530.088089	37.008871
1732.218286	173837.778448	37.013888
1734.364950	174126.206639	37.018906
1735.921455	174433.455184	37.023924
1737.748579	174738.823599	37.028941
1739.529887	175050.722304	37.033959
1740.770044	175352.623690	37.038976
1743.164345	175662.996185	37.043994
1744.599934	175967.319548	37.049012
1746.825417	176270.010037	37.054029
1748.707842	176569.116134	37.059047
1750.749379	176887.660667	37.064064
1752.464482	177183.638750	37.069082
1754.667314	177486.595456	37.074100
1756.460672	177785.610259	37.079117
1758.989190	178068.829148	37.084135
1760.936665	178352.548192	37.089152
1762.889473	178640.074496	37.094170
1764.899615	178921.173824	37.099188
1766.852650	179202.220643	37.104205
1768.698394	179480.723465	37.109223
1770.095300	179758.753796	37.114240
1771.787794	180040.799079	37.119258
1773.605355	180332.202661	37.124276
1775.128565	180620.267275	37.129293
1776.644457	180904.490510	37.134311
1778.408751	181196.936109	37.139328
1780.304244	181495.072521	37.144346
1781.883619	181791.040715	37.149364
1783.470189	182079.257196	37.154381
1785.528078	182361.462562	37.159399
1787.169059	182677.639607	37.164416
1789.114515	182983.188286	37.169434
1790.787201	183275.713036	37.174452
1792.650746	183582.661912	37.179469
1794.419496	183882.433371	37.184487
1795.694344	184191.903462	37.189504
1797.544927	184477.466988	37.194522
1799.031748	184776.883126	37.199540
1800.662992	185058.856069	37.204557
1802.682984	185342.824710	37.209575
1804.434531	185634.603618	37.214592
1806.978386	185898.582988	37.219610
1808.866492	186170.573536	37.224628
1811.284116	186442.037501	37.229645
1813.215709	186711.829055	37.234663
1815.219488	186980.151409	37.239680
1817.416740	187229.079995	37.244698
1818.945194	187493.851502	37.249716
1820.612074	187761.521221	37.254733
1823.078570	188011.654862	37.259751
1824.586774	188279.784194	37.264768
1826.035583	188535.056684	37.269786
1828.435823	188809.049857	37.274804
1830.234485	189066.173212	37.279821
1832.135456	189339.170035	37.284839
1833.451535	189614.240975	37.289856
1835.033511	189872.431005	37.294874
1836.667438	190164.802557	37.299892
1838.190731	190440.885973	37.304909
1840.166119	190726.658362	37.309927
1841.504709	191022.635392	37.314944
1843.273293	191320.639962	37.319962
1845.121718	191629.915933	37.324980
1846.600437	191930.051547	37.329997
1848.548508	192226.243705	37.335015
1849.967387	192552.257088	37.340032
1851.914655	192857.857332	37.345050
1854.075632	193174.593917	37.350068
1855.598749	193488.083226	37.355085
1858.170813	193800.722656	37.360103
1860.080510	194118.545805	37.365120
1861.590616	194429.415892	37.370138
1863.718302	194735.113163	37.375156
1865.908290	195050.625850	37.380173
1868.298047	195356.031414	37.385191
1870.095075	195666.431983	37.390208
1872.336747	195965.556773	37.395226
1874.174892	196270.509567	37.400244
1875.597068	196577.662468	37.405261
1877.905226	196868.519300	37.410279
1879.395034	197179.929613	37.415296
1881.135902	197490.844999	37.420314
1883.140203	197806.860865	37.425332
1885.368480	198097.952957	37.430349
1887.549316	198399.855604	37.435367
1889.139971	198720.841922	37.440384
1891.208823	199009.121130	37.445402
1893.365379	199317.404584	37.450420
1895.382622	199607.256409	37.455437
1897.212489	199904.704544	37.460455
1899.049354	200200.325397	37.465472
1900.948004	200499.695209	37.470490
1902.598261	200788.672277	37.475508
1904.685236	201060.445655	37.480525
1906.393752	201330.477988	37.485543
1907.988846	201613.933845	37.490560
1909.480149	201893.091847	37.495578
1911.123088	202168.381046	37.500596
1912.862456	202480.404182	37.505613
1914.521951	202774.353281	37.510631
1916.410899	203079.437957	37.515648
1918.053453	203388.523834	37.520666
1920.014532	203703.577719	37.525684
1921.487224	204024.270782	37.530701
1923.566467	204326.970847	37.535719
1925.685714	204654.597273	37.540736
1927.853409	204964.408000	37.545754
1929.991995	205275.951403	37.550772
1932.311466	205586.794963	37.555789
1934.703654	205892.360480	37.560807
1936.833891	206192.396314	37.565824
1938.857387	206503.202807	37.570842
1940.837959	206817.940340	37.575860
1942.658907	207124.339125	37.580877
1944.923250	207425.464299	37.585895
1946.480736	207748.588839	37.590912
1948.709479	208042.600994	37.595930
1950.595653	208360.192475	37.600948
1952.131774	208687.095741	37.605965
1953.770130	208999.550328	37.610983
1955.620088	209324.706038	37.616000
1957.464156	209650.092895	37.621018
1959.609539	209988.953992	37.626036
1961.295327	210318.952397	37.631053
1963.413472	210644.262822	37.636071
1965.604631	210987.578067	37.641088
1967.453881	211318.457098	37.646106
1969.937301	211645.377767	37.651124
1971.670498	211980.544310	37.656141
1973.684052	212306.057499	37.661159
1975.637679	212643.769696	37.666176
1977.201101	212981.621725	37.671194
1979.049114	213316.522982	37.676212
1980.930978	213671.340421	37.681229
1982.980039	214009.463418	37.686247
1984.885437	214361.805076	37.691264
1986.503939	214713.153019	37.696282
1989.041367	215062.465242	37.701300
1991.026281	215411.841534	37.706317
1993.028147	215761.178826	37.711335
1995.252738	216110.850741	37.716352
1997.374225	216455.106711	37.721370
1999.718611	216793.831436	37.726388
2001.752221	217141.494685	37.731405
2003.802304	217477.361888	37.736423
2005.456843	217830.700562	37.741440
2007.335127	218170.356501	37.746458
2009.237471	218482.343941	37.751476
2010.826043	218828.359244	37.756493
2012.482321	219143.004116	37.761511
2014.927580	219470.450649	37.766528
2016.764975	219814.844014	37.771546
2018.690061	220145.677297	37.776564
2020.552275	220489.396905	37.781581
2022.507144	220812.038767	37.786599
2024.768532	221155.494929	37.791616
2026.518118	221501.408242	37.796634
2029.040417	221893.647440	37.801652
2031.040789	222237.480007	37.806669
2032.862776	222586.865801	37.811687
2034.953854	222930.750529	37.816704
2036.632737	223283.476189	37.821722
2038.928027	223627.179186	37.826740
2041.025757	223989.872667	37.831757
2042.928364	224352.865399	37.836775
2044.933933	224716.033893	37.841792
2046.394784	225083.937848	37.846810
2048.675638	225446.050084	37.851828
2050.239163	225831.464224	37.856845
2052.501536	226206.077527	37.861863
2054.465792	226595.241024	37.866880
2056.702610	226978.090182	37.871898
2058.879662	227357.242665	37.876916
2060.641377	227744.894363	37.881933
2063.897203	228091.803119	37.886951
2067.125640	228445.981071	37.891968
2069.752093	228782.274994	37.896986
2072.760632	229120.668321	37.902004
2075.162951	229450.041574	37.907021
2077.825347	229768.987357	37.912039
2079.849973	230086.054461	37.917056
2081.783778	230405.219653	37.922074
2084.123985	230724.016717	37.927092
2085.924054	231044.754581	37.932109
2088.003128	231355.747426	37.937127
2089.991371	231660.101532	37.942144
2091.464587	231990.774161	37.947162
2093.545226	232313.910023	37.952180
2095.512874	232657.103836	37.957197
2097.513946	232976.571849	37.962215
2099.118248	233319.952634	37.967232
2101.259383	233662.843090	37.972250
2103.446447	233991.809211	37.977268
2104.968368	234347.042203	37.982285
2107.086925	234688.060285	37.987303
2109.103232	235030.975219	37.992320
2110.917981	235395.029501	37.997338
2113.288022	235741.954468	38.002356
2115.102157	236110.786306	38.007373
2117.041629	236472.843459	38.012391
2118.870160	236830.576224	38.017408
2120.892033	237197.854943	38.022426
2122.696809	237549.802885	38.027444
2124.577515	237894.856735	38.032461
2126.795820	238240.874085	38.037479
2128.815258	238590.175168	38.042496
2130.296212	238959.247302	38.047514
2132.360382	239318.982704	38.052532
2134.395046	239687.232773	38.057549
2136.074499	240061.890270	38.062567
2138.172502	240451.138228	38.067584
2140.209265	240833.234424	38.072602
2142.475528	241215.778034	38.077620
2145.123060	241590.083580	38.082637
2147.676784	241980.356391	38.087655
2150.085211	242355.845190	38.092672
2152.099255	242737.671519	38.097690
2154.541338	243124.180960	38.102708
2156.739640	243510.095220	38.107725
2159.075583	243875.668435	38.112743
2161.199166	244260.529939	38.117760
2163.362161	244642.617637	38.122778
2165.842758	245018.001070	38.127796
2167.973765	245401.797819	38.132813
2170.310802	245791.049529	38.137831
2172.503974	246162.671529	38.142848
2174.661230	246560.640968	38.147866
2176.813880	246943.143022	38.152884
2179.354854	247335.617913	38.157901
2180.622887	247719.456131	38.162919
2183.012117	248110.026636	38.167936
2185.400372	248505.272129	38.172954
2188.020460	248888.187619	38.177972
2190.241376	249282.039145	38.182989
2192.576203	249687.177225	38.188007
2194.982092	250056.615916	38.193024
2196.848608	250463.049462	38.198042
2198.987508	250846.985752	38.203060
2201.394097	251246.197676	38.208077
2203.535164	251634.479074	38.213095
2205.563267	252023.896924	38.218112
2208.043674	252425.894019	38.223130
2209.650094	252823.407454	38.228148
2211.630809	253228.508377	38.233165
2213.442686	253643.721547	38.238183
2215.856919	254053.683466	38.243200
2218.237455	254474.752318	38.248218
2220.115903	254882.438518	38.253236
2222.574597	255302.785437	38.258253
2225.102649	255720.683584	38.263271
2227.458359	256137.746200	38.268288
2229.654542	256564.564024	38.273306
2231.742315	256966.200643	38.278324
2234.730760	257377.297281	38.283341
2236.661928	257780.560506	38.288359
2239.459366	258184.779354	38.293376
2241.289496	258579.880309	38.298394
2243.584543	258964.874120	38.303412
2245.587058	259344.072281	38.308429
2247.698707	259724.345998	38.313447
2250.205766	260097.292366	38.318464
2252.107207	260500.945620	38.323482
2254.096862	260877.328236	38.328500
2256.077855	261261.257356	38.333517
2257.653809	261657.165142	38.338535
2260.003976	262054.830486	38.343552
2262.265376	262476.338363	38.348570
2264.117035	262895.041211	38.353588
2266.377406	263308.218119	38.358605
2268.812172	263726.854914	38.363623
2271.153798	264148.428307	38.368640
2273.415472	264590.489735	38.373658
2275.604104	265015.035082	38.378676
2277.836402	265442.927155	38.383693
2279.927862	265878.437527	38.388711
2282.628589	266304.325516	38.393728
2284.984272	266731.919803	38.398746
2287.384967	267164.587963	38.403764
2289.988622	267595.776310	38.408781
2292.055596	268036.804936	38.413799
2294.410551	268475.171688	38.418816
2296.519919	268912.155092	38.423834
2299.180086	269352.506297	38.428852
2302.010465	269792.856180	38.433869
2303.895451	270238.995736	38.438887
2306.678504	270664.238584	38.443904
2308.916111	271114.387191	38.448922
2310.787157	271553.035559	38.453940
2312.732375	272003.256269	38.458957
2314.991077	272461.048439	38.463975
2317.470955	272913.597967	38.468992
2319.837503	273377.724111	38.474010
2322.235759	273833.309758	38.479028
2324.510922	274285.841159	38.484045
2326.431735	274753.365973	38.489063
2329.034160	275212.120166	38.494080
2331.221441	275695.987922	38.499098
2333.232486	276164.666924	38.504116
2335.743952	276632.529823	38.509133
2338.160714	277108.765358	38.514151
2340.706437	277584.345237	38.519168
2342.763276	278060.256501	38.524186
2345.583458	278525.758209	38.529204
2347.995160	278999.326535	38.534221
2350.190845	279480.397462	38.539239
2352.557469	279949.171217	38.544256
2354.932746	280425.564320	38.549274
2356.993187	280909.551802	38.554292
2359.315290	281395.910768	38.559309
2361.667078	281876.802947	38.564327
2364.423339	282353.439075	38.569344
2366.434806	282844.901312	38.574362
2368.869148	283286.073931	38.579380
2371.175373	283733.617249	38.584397
2372.959303	284202.505353	38.589415
2375.604568	284655.506487	38.594432
2377.833097	285103.263941	38.599450
2380.083203	285576.623751	38.604468
2382.802108	286029.738661	38.609485
2385.372155	286493.723682	38.614503
2387.588098	286953.318700	38.619520
2389.954734	287413.829113	38.624538
2392.542965	287882.432671	38.629556
2394.909002	288347.133307	38.634573
2397.257064	288833.504670	38.639591
2399.741208	289291.605780	38.644608
2402.347736	289759.111159	38.649626
2404.571482	290238.056811	38.654644
2407.582550	290714.641373	38.659661
2409.908762	291179.394390	38.664679
2412.439409	291642.589988	38.669696
2414.909034	292125.049457	38.674714
2417.033038	292599.535554	38.679732
2419.906151	293068.288013	38.684749
2421.827390	293552.634973	38.689767
2424.602098	294022.848937	38.694784
2427.369879	294498.016392	38.699802
2429.420164	294981.196547	38.704820
2432.356052	295448.612903	38.709837
2434.602754	295933.105942	38.714855
2437.365753	296405.221389	38.719872
2439.744760	296893.602930	38.724890
2441.810969	297381.804140	38.729908
2444.355932	297856.287411	38.734925
2446.694450	298357.372303	38.739943
2448.844011	298847.893219	38.744960
2451.281988	299325.590034	38.749978
2454.033915	299835.114569	38.754996
2456.690214	300322.985285	38.760013
2458.857909	300823.276987	38.765031
2461.268048	301315.273274	38.770048
2464.123424	301821.904693	38.775066
2466.316678	302326.912077	38.780084
2468.894023	302818.292752	38.785101
2470.955473	303320.142493	38.790119
2473.109410	303828.529225	38.795136
2475.838419	304345.357623	38.800154
2478.098994	304868.379871	38.805172
2480.812220	305381.726981	38.810189
2483.229828	305890.038884	38.815207
2485.963854	306395.860249	38.820224
2488.769306	306914.495424	38.825242
2491.018341	307428.441440	38.830260
2493.759001	307932.630039	38.835277
2496.356809	308451.571155	38.840295
2498.796161	308951.866318	38.845312
2501.686663	309446.753965	38.850330
2503.980173	309925.656203	38.855348
2506.415778	310389.878455	38.860365
2509.096944	310858.149217	38.865383
2511.470481	311328.828923	38.870400
2513.920624	311798.834131	38.875418
2516.171544	312276.818810	38.880436
2519.023765	312752.623400	38.885453
2521.210165	313242.018165	38.890471
2523.484730	313725.758194	38.895488
2526.040387	314201.120716	38.900506
2528.176511	314692.929549	38.905524
2530.468121	315197.435952	38.910541
2532.674870	315704.594698	38.915559
2535.500394	316208.909831	38.920576
2538.540511	316704.121314	38.925594
2541.144962	317217.000004	38.930612
2543.946234	317702.567657	38.935629
2546.641881	318212.861396	38.940647
2549.220308	318718.421623	38.945664
2552.075831	319214.233436	38.950682
2554.333275	319717.299331	38.955700
2556.866452	320228.979132	38.960717
2559.383193	320727.401466	38.965735
2561.943733	321246.690164	38.970752
2564.574052	321750.625218	38.975770
2567.077731	322279.745258	38.980788
2569.346034	322795.642492	38.985805
2571.928756	323328.679941	38.990823
2574.246715	323856.016479	38.995840
2576.908110	324394.799548	39.000858
2579.263084	324931.418222	39.005876
2581.883689	325463.826424	39.010893
2584.544831	326007.017675	39.015911
2587.086443	326554.566722	39.020928
2589.752860	327097.470322	39.025946
2591.782258	327652.431986	39.030964
2594.414010	328208.513174	39.035981
2597.164218	328768.329915	39.040999
2599.767894	329326.997596	39.046016
2602.348698	329883.404667	39.051034
2604.743842	330445.245851	39.056052
2607.430009	331012.775579	39.061069
2610.319793	331574.199595	39.066087
2613.004123	332152.233528	39.071104
2615.808386	332704.825389	39.076122
2618.685561	333279.391520	39.081140
2621.771464	333824.464466	39.086157
2624.781559	334384.780552	39.091175
2627.400739	334936.571427	39.096192
2630.610201	335474.806568	39.101210
2633.487111	336016.441793	39.106228
2635.969190	336544.144414	39.111245
2638.195995	337089.834945	39.116263
2641.137060	337632.411635	39.121280
2643.995103	338157.223293	39.126298
2646.121076	338668.968848	39.131316
2648.774191	339174.456906	39.136333
2651.050784	339675.201802	39.141351
2653.329618	340179.522365	39.146368
2656.007115	340692.230547	39.151386
2658.571755	341210.385756	39.156404
2661.546336	341723.647660	39.161421
2664.214181	342250.003913	39.166439
2666.908347	342765.434126	39.171456
2669.441306	343290.533202	39.176474
2671.605049	343820.433801	39.181492
2674.579656	344344.184169	39.186509
2677.359454	344869.534783	39.191527
2679.738861	345407.993462	39.196544
2682.463835	345945.681535	39.201562
2684.862673	346493.139607	39.206580
2687.659433	347026.414110	39.211597
2690.380013	347586.098068	39.216615
2692.801657	348140.670285	39.221632
2695.714158	348687.771776	39.226650
2698.374619	349258.491524	39.231668
2701.004406	349815.527178	39.236685
2703.867011	350368.864717	39.241703
2706.572610	350944.281352	39.246720
2709.396231	351499.771183	39.251738
2711.925779	352069.085760	39.256756
2714.871393	352643.303676	39.261773
2717.425351	353219.125769	39.266791
2719.987127	353796.996352	39.271808
2723.069538	354371.401977	39.276826
2725.497406	354966.541555	39.281844
2727.740845	355542.386813	39.286861
2730.569356	356138.946779	39.291879
2732.980385	356749.170800	39.296896
2735.476935	357340.387892	39.301914
2738.660475	357945.499930	39.306932
2741.130602	358565.007319	39.311949
2743.727791	359185.451189	39.316967
2745.696073	359815.859872	39.321984
2748.555000	360442.972031	39.327002
2750.896234	361083.558689	39.332020
2753.342871	361722.114957	39.337037
2756.201724	362370.977497	39.342055
2758.973202	363024.869911	39.347072
2761.867112	363682.362857	39.352090
2764.813753	364337.934641	39.357108
2768.074099	364984.869504	39.362125
2770.942111	365629.827013	39.367143
2773.605985	366286.531928	39.372160
2776.978062	366926.569208	39.377178
2779.803494	367579.854264	39.382196
2782.641011	368214.932907	39.387213
2786.104746	368854.648439	39.392231
2788.743331	369496.819729	39.397248
2791.679009	370121.044916	39.402266
2794.505805	370729.469736	39.407284
2797.237242	371317.296902	39.412301
2800.327121	371901.658999	39.417319
2802.698946	372503.177795	39.422336
2805.566500	373087.939126	39.427354
2808.067963	373690.435152	39.432372
2810.602527	374294.997680	39.437389
2813.619379	374907.619408	39.442407
2815.555772	375517.891171	39.447424
2818.826926	376117.286371	39.452442
2821.783639	376744.706733	39.457460
2824.691622	377361.266302	39.462477
2827.617085	377977.204644	39.467495
2830.178153	378601.943682	39.472512
2832.975999	379222.347840	39.477530
2835.876216	379847.951952	39.482548
2838.634982	380486.937652	39.487565
2841.496339	381125.769670	39.492583
2843.975096	381770.765249	39.497600
2846.606935	382418.262402	39.502618
2849.481824	383077.733925	39.507636
2852.108141	383731.906272	39.512653
2855.185006	384385.285591	39.517671
2858.177854	385059.263583	39.522688
2861.124029	385717.358089	39.527706
2864.007262	386377.302380	39.532724
2866.825558	387052.793277	39.537741
2869.975647	387713.330548	39.542759
2872.716394	388401.591844	39.547776
2876.206424	389068.923824	39.552794
2878.945178	389740.318750	39.557812
2881.829414	390415.127122	39.562829
2884.505788	391087.596860	39.567847
2887.309396	391780.449009	39.572864
2890.674205	392454.634756	39.577882
2893.192448	393132.567828	39.582900
2895.977643	393816.556878	39.587917
2899.016254	394502.622268	39.592935
2901.658287	395186.251472	39.597952
2904.881632	395872.995268	39.602970
2908.476833	396552.768982	39.607988
2911.600573	397226.010734	39.613005
2914.959786	397906.580238	39.618023
2917.548078	398586.066033	39.623040
2920.737627	399263.693095	39.628058
2924.330161	399916.166530	39.633076
2926.988296	400582.567444	39.638093
2930.596754	401250.807137	39.643111
2933.651722	401902.133955	39.648128
2936.442366	402559.852856	39.653146
2939.394813	403213.957909	39.658164
2942.284960	403867.628332	39.663181
2945.341286	404530.562718	39.668199
2947.770449	405190.616337	39.673216
2950.888771	405823.346388	39.678234
2953.794655	406452.345437	39.683252
2956.336097	407079.640276	39.688269
2959.244380	407694.519559	39.693287
2961.878890	408314.930311	39.698304
2964.791406	408947.501866	39.703322
2966.836956	409585.064026	39.708340
2969.753404	410226.961169	39.713357
2972.259606	410869.821957	39.718375
2974.886240	411530.290123	39.723392
2978.028548	412200.723823	39.728410
2980.472480	412865.879907	39.733428
2983.079348	413566.019866	39.738445
2985.842110	414251.444890	39.743463
2988.712973	414951.813961	39.748480
2991.666210	415658.944633	39.753498
2994.807550	416369.271848	39.758516
2997.422854	417084.808823	39.763533
3000.626637	417802.667349	39.768551
3003.915088	418535.799144	39.773568
3006.838769	419266.283767	39.778586
3010.057660	420003.163821	39.783604
3012.864788	420737.479898	39.788621
3016.164534	421462.830886	39.793639
3019.377670	422189.950076	39.798656
3022.682468	422928.056334	39.803674
3026.104631	423655.205005	39.808692
3029.152661	424396.327044	39.813709
3032.498006	425131.301863	39.818727
3035.448357	425866.521836	39.823744
3038.447704	426602.499217	39.828762
3041.549309	427344.114290	39.833780
3044.393083	428085.116231	39.838797
3047.651869	428825.423851	39.843815
3050.709276	429573.341176	39.848832
3053.716414	430318.256402	39.853850
3056.606691	431071.070986	39.858868
3059.504692	431821.735081	39.863885
3063.148462	432568.435151	39.868903
3065.570630	433331.033741	39.873920
3068.631269	434093.660527	39.878938
3072.057066	434853.218503	39.883956
3074.784958	435619.903890	39.888973
3078.018431	436383.497966	39.893991
3081.420565	437152.891342	39.899008
3084.781137	437899.175254	39.904026
3087.923315	438670.588534	39.909044
3091.322183	439434.037624	39.914061
3095.184966	440169.539607	39.919079
3098.699983	440914.695170	39.924096
3101.745131	441654.282010	39.929114
3105.230180	442392.257775	39.934132
3107.957464	443128.963885	39.939149
3111.289050	443854.211005	39.944167
3114.877745	444584.154457	39.949184
3117.610373	445301.149590	39.954202
3120.041679	446000.705420	39.959220
3122.913208	446700.727773	39.964237
3126.029316	447394.211124	39.969255
3128.460565	448087.832948	39.974272
3131.221738	448809.930644	39.979290
3134.033726	449528.809053	39.984308
3136.844412	450260.470964	39.989325
3139.622466	450991.305027	39.994343
3142.492706	451734.956649	39.999360
3145.278437	452479.559065	40.004378
3148.185801	453238.338869	40.009396
3151.042147	454019.115267	40.014413
3154.277238	454789.784991	40.019431
3157.362811	455568.599064	40.024448
3159.609445	456369.783362	40.029466
3163.026887	457174.396823	40.034484
3165.707591	457976.871350	40.039501
3168.941655	458803.262205	40.044519
3172.112490	459641.825125	40.049536
3174.983107	460462.999783	40.054554
3178.245728	461318.330916	40.059572
3181.559039	462154.953330	40.064589
3184.967675	462994.057542	40.069607
3188.774861	463848.038821	40.074624
3191.823934	464706.253641	40.079642
3195.627726	465555.007780	40.084660
3198.493432	466407.214450	40.089677
3201.740193	467258.618367	40.094695
3205.086513	468114.928259	40.099712
3208.152696	468980.653731	40.104730
3211.713802	469831.245733	40.109748
3214.832875	470699.015130	40.114765
3218.463392	471555.643867	40.119783
3222.368229	472409.513622	40.124800
3225.896878	473241.261388	40.129818
3229.758231	474080.101947	40.134836
3233.247141	474908.754158	40.139853
3236.504175	475739.785103	40.144871
3240.360245	476573.922328	40.149888
3243.534286	477403.077565	40.154906
3247.068915	478217.279949	40.159924
3250.073028	479048.314318	40.164941
3253.557976	479866.247760	40.169959
3256.970213	480674.757814	40.174976
3259.942875	481504.682604	40.179994
3263.464094	482324.832572	40.185012
3266.986107	483133.223451	40.190029
3270.022680	483946.761283	40.195047
3273.243389	484758.770264	40.200064
3276.188954	485585.644159	40.205082
3279.356786	486389.154006	40.210100
3282.733954	487217.910079	40.215117
3285.688978	488042.806450	40.220135
3289.367807	488857.953403	40.225152
3292.229249	489676.124420	40.230170
3295.163630	490459.543336	40.235188
3298.510855	491270.697608	40.240205
3301.259645	492050.593565	40.245223
3304.026299	492852.072262	40.250240
3307.348348	493645.650158	40.255258
3310.589704	494445.620841	40.260276
3313.347418	495267.299126	40.265293
3316.600763	496085.933025	40.270311
3319.599616	496916.387104	40.275328
3322.389513	497756.481045	40.280346
3325.615685	498604.697494	40.285364
3328.563057	499469.378369	40.290381
3331.236089	500323.559126	40.295399
3334.202318	501216.022699	40.300416
3337.245650	502106.561371	40.305434
3340.636243	503005.228882	40.310452
3343.921745	503915.073589	40.315469
3347.343680	504836.560144	40.320487
3351.127266	505763.997832	40.325504
3353.806081	506697.920174	40.330522
3357.419939	507619.834808	40.335540
3360.708636	508569.104047	40.340557
3363.532128	509504.315329	40.345575
3367.434056	510464.888328	40.350592
3370.887883	511421.138770	40.355610
3375.063462	512350.682266	40.360628
3378.366792	513311.996214	40.365645
3382.126346	514267.936534	40.370663
3385.491251	515223.329888	40.375680
3388.855781	516187.647532	40.380698
3392.146003	517137.898735	40.385716
3395.456924	518111.192389	40.390733
3398.742832	519089.728198	40.395751
3402.287196	520062.314904	40.400768
3405.411501	521053.820762	40.405786
3409.245906	522020.748379	40.410804
3412.667895	523008.255785	40.415821
3416.030756	524000.955801	40.420839
3419.782585	524971.753526	40.425856
3423.211474	525970.119298	40.430874
3426.970061	526952.491553	40.435892
3430.378299	527925.684552	40.440909
3434.187922	528915.337037	40.445927
3437.817784	529902.385469	40.450944
3440.927395	530894.645048	40.455962
3444.654354	531872.180350	40.460980
3448.064244	532861.042385	40.465997
3451.080506	533858.217608	40.471015
3454.655780	534841.384557	40.476032
3458.080452	535841.138290	40.481050
3462.082328	536833.481285	40.486068
3465.532314	537818.895428	40.491085
3469.039574	538809.223492	40.496103
3472.549201	539802.760434	40.501120
3476.280259	540764.348749	40.506125
3480.059488	541699.112706	40.511130
3483.699952	542549.678069	40.516135
3486.820509	543370.693239	40.521140
3489.760696	544100.218303	40.526144
3492.499690	544777.694714	40.531149
3495.271929	545396.984661	40.536154
3497.879868	545950.706654	40.541159
3500.289622	546449.674849	40.546164
3502.653481	546881.202072	40.551168
3504.378556	547260.832184	40.556173
3506.325338	547579.954198	40.561178
3508.085339	547866.546143	40.566183
3509.370621	548091.888420	40.571188
3511.174701	548271.875625	40.576192
3512.064855	548435.653658	40.581197
3513.252163	548537.914279	40.586202
3514.552281	548604.425962	40.591207
3515.449128	548650.158403	40.596212
3516.428473	548655.100754	40.601216
3516.740075	548645.866604	40.606221
3517.498729	548587.306306	40.611226
3518.146904	548521.092253	40.616231
3518.755953	548430.912131	40.621236
3519.440035	548320.431598	40.626240
3519.740172	548185.180598	40.631245
3520.097619	548039.068534	40.636250
3520.449167	547878.471288	40.641255
3520.496212	547712.015445	40.646260
3520.768495	547522.103849	40.651264
3520.683631	547340.573970	40.656269
3521.067344	547136.305986	40.661274
3521.087082	546929.871899	40.666279
3520.885114	546719.381627	40.671284
3521.170820	546485.391354	40.676288
3521.427932	546264.020580	40.681293
3521.426685	546025.121828	40.686298
3521.322141	545783.509809	40.691303
3521.295523	545535.571870	40.696308
3521.355667	545286.909368	40.701312
3521.066185	545041.881950	40.706317
3521.239330	544781.229588	40.711322
3521.127816	544536.569530	40.716327
3520.295082	544277.076898	40.721332
3520.823783	544030.389020	40.726336
3520.738507	543770.668451	40.731341
3520.495095	543513.139161	40.736346
3520.567858	543260.553465	40.741351
3520.244556	542995.556084	40.746356
3520.020357	542747.855288	40.751360
3519.652074	542494.670016	40.756365
3519.786324	542236.604634	40.761370
3520.008415	541982.509579	40.766375
3519.526044	541732.207337	40.771380
3519.105588	541477.043999	40.776384
3519.188631	541233.258394	40.781389
3519.020339	540987.589841	40.786394
3518.776099	540738.293751	40.791399
3518.315920	540495.844394	40.796404
3518.425378	540261.733786	40.801408
3517.911517	540026.556658	40.806413
3518.036826	539784.255813	40.811418
3518.065082	539550.046019	40.816423
3517.173064	539327.895626	40.821428
3517.270962	539091.041819	40.826432
3516.847069	538877.193657	40.831437
3516.499271	538639.847751	40.836442
3516.660089	538438.071601	40.841447
3516.405570	538222.722920	40.846452
3516.498717	538003.831564	40.851456
3515.785250	537796.680305	40.856461
3515.702485	537579.073231	40.861466
3515.408720	537392.809292	40.866471
3514.994636	537190.703447	40.871476
3515.123082	536984.165668	40.876480
3515.184134	536798.393969	40.881485
3514.779088	536613.299767	40.886490
3514.870582	536424.134733	40.891495
3514.548771	536230.992011	40.896500
3514.616815	536049.503343	40.901504
3514.014011	535864.936449	40.906509
3514.012364	535675.726398	40.911514
3513.629566	535501.879052	40.916519
3513.440296	535339.616775	40.921524
3513.140554	535170.652162	40.926528
3513.019355	535008.123072	40.931533
3512.847278	534839.437722	40.936538
3512.997271	534686.661904	40.941543
3512.656444	534536.588876	40.946548
3512.485228	534365.018905	40.951552
3512.251608	534215.835078	40.956557
3512.397088	534070.530106	40.961562
3512.620702	533917.937114	40.966567
3512.349652	533777.039597	40.971572
3512.213329	533613.689963	40.976576
3512.077582	533474.788992	40.981581
3511.803689	533319.843903	40.986586
3512.040217	533176.486358	40.991591
3511.722947	533048.017053	40.996596
3511.770236	532898.927704	41.001600
3511.308642	532756.181813	41.006605
3511.213840	532626.461385	41.011610
3511.300001	532489.688902	41.016615
3510.739243	532368.375877	41.021620
3510.807120	532236.201473	41.026624
3510.874006	532110.593955	41.031629
3510.936150	531993.120265	41.036634
3510.606819	531861.409642	41.041639
3510.459739	531744.118714	41.046644
3510.512420	531612.497182	41.051648
3510.265810	531504.213366	41.056653
3510.004329	531381.430692	41.061658
3510.312929	531262.750498	41.066663
3510.023258	531153.561616	41.071668
3510.035372	531055.237747	41.076672
3509.908126	530937.331327	41.081677
3509.594528	530830.215524	41.086682
3509.637393	530708.086830	41.091687
3509.437090	530613.835879	41.096692
3509.670987	530496.930128	41.101696
3509.146021	530401.162871	41.106701
3509.182856	530302.729321	41.111706
3509.221102	530208.488760	41.116711
3508.970678	530107.572986	41.121716
3508.911846	530007.232626	41.126720
3508.715195	529921.061528	41.131725
3508.840470	529828.522919	41.136730
3508.741309	529732.633757	41.141735
3508.354816	529658.113021	41.146740
3508.434309	529562.144054	41.151744
3508.532868	529480.016821	41.156749
3508.185846	529389.369373	41.161754
3508.297883	529306.127430	41.166759
3508.139270	529222.776230	41.171764
3507.982758	529136.240774	41.176768
3507.535258	529072.186924	41.181773
3507.693477	528991.765797	41.186778
3507.961610	528936.289780	41.191783
3507.579445	528851.102261	41.196788
3507.611674	528788.133680	41.201792
3507.560790	528713.100639	41.206797
3507.558098	528650.187561	41.211802
3507.674266	528573.661997	41.216807
3507.366983	528510.796505	41.221812
3507.700709	528427.464360	41.226816
3507.555460	528360.580494	41.231821
3507.363275	528294.866050	41.236826
3507.186352	528230.715487	41.241831
3507.064983	528173.226448	41.246836
3507.317795	528102.033671	41.251840
3507.014884	528032.545529	41.256845
3506.849947	527975.871220	41.261850
3507.268439	527916.021837	41.266855
3506.971758	527860.833465	41.271860
3507.010293	527775.017768	41.276864
3506.804167	527730.427151	41.281869
3506.780262	527674.335906	41.286874
3506.955813	527610.379803	41.291879
3506.582097	527555.758446	41.296884
3507.058500	527497.414428	41.301888
3506.767035	527447.934444	41.306893
3506.681773	527387.960545	41.311898
3506.879485	527342.648030	41.316903
3506.764273	527275.198929	41.321908
3506.444562	527218.192615	41.326912
3506.340135	527173.331673	41.331917
3506.409782	527118.234433	41.336922
3506.338200	527070.133580	41.341927
3506.204035	527026.338223	41.346932
3506.190046	526966.300930	41.351936
3506.513489	526929.558893	41.356941
3506.677812	526879.449177	41.361946
3506.302469	526817.800661	41.366951
3505.931017	526784.756382	41.371956
3506.204623	526728.261003	41.376960
3506.332840	526679.369304	41.381965
3506.231036	526645.726185	41.386970
3506.437698	526581.154556	41.391975
3506.046828	526549.679586	41.396980
3506.291905	526498.747274	41.401984
3506.033340	526453.858127	41.406989
3505.840424	526409.514419	41.411994
3505.789263	526365.603046	41.416999
3505.947098	526325.954457	41.422004
3505.807613	526282.309516	41.427008
3505.525767	526242.629133	41.432013
3505.606650	526210.068115	41.437018
3506.056389	526166.481351	41.442023
3505.732593	526137.825259	41.447028
3506.065083	526092.437347	41.452032
3505.932335	526050.610191	41.457037
3505.602572	526008.207567	41.462042
3505.742335	525963.658415	41.467047
3505.607887	525937.701281	41.472052
3505.823439	525891.623700	41.477056
3505.549549	525864.576567	41.482061
3505.385839	525825.988397	41.487066
3505.232728	525784.315388	41.492071
3504.908220	525758.640714	41.497076
3505.278930	525733.513166	41.502080
3505.525674	525699.358082	41.507085
3505.330371	525682.052903	41.512090
3505.195204	525641.994046	41.517095
3505.408413	525613.707020	41.522100
3505.403716	525577.569710	41.527104
3505.170499	525551.880275	41.532109
3504.970348	525519.766614	41.537114
3505.465184	525489.817481	41.542119
3505.199060	525463.981477	41.547124
3505.182291	525429.362035	41.552128
3505.213416	525412.374579	41.557133
3505.339234	525381.674877	41.562138
3505.361327	525352.103467	41.567143
3505.120675	525320.905592	41.572148
3505.014347	525288.422833	41.577152
3505.340593	525261.987438	41.582157
3505.044769	525233.679109	41.587162
3504.962524	525208.066348	41.592167
3505.176540	525183.619777	41.597172
3505.319973	525146.801011	41.602176
3505.190416	525128.625590	41.607181
3505.160031	525097.545679	41.612186
3505.498625	525075.505381	41.617191
3504.807367	525044.378188	41.622196
3505.085617	525006.476357	41.627200
3505.205186	524990.940269	41.632205
3505.290861	524960.296650	41.637210
3505.338236	524919.954413	41.642215
3505.103691	524894.061953	41.647220
3505.152156	524863.777846	41.652224
3504.957947	524837.221833	41.657229
3504.858651	524814.340575	41.662234
3505.002140	524789.146373	41.667239
3504.838209	524773.048340	41.672244
3504.942835	524748.820579	41.677248
3504.781480	524727.869732	41.682253
3504.730320	524694.719960	41.687258
3504.875049	524678.724683	41.692263
3504.688081	524655.755965	41.697268
3505.118877	524629.151368	41.702272
3504.982517	524622.551432	41.707277
3504.760900	524582.453046	41.712282
3505.113945	524550.856561	41.717287
3504.821567	524536.952072	41.722292
3505.043443	524524.331035	41.727296
3505.182980	524485.186247	41.732301
3505.050450	524467.718195	41.737306
3505.057708	524434.356468	41.742311
3505.118856	524409.225232	41.747316
3504.844481	524384.500815	41.752320
3505.138491	524353.418739	41.757325
3504.701758	524337.009559	41.762330
3504.818578	524300.951262	41.767335
3504.841744	524286.845042	41.772340
3504.698357	524259.875667	41.777344
3504.720385	524250.975931	41.782349
3504.896852	524229.617211	41.787354
3504.686310	524212.616136	41.792359
3504.600843	524181.442065	41.797364
3504.784621	524158.818416	41.802368
3504.823612	524144.153550	41.807373
3504.397570	524128.955603	41.812378
3504.750520	524117.122289	41.817383
3504.608431	524106.226516	41.822388
3504.931778	524087.978334	41.827392
3504.813050	524054.029162	41.832397
3504.790333	524040.132168	41.837402
3504.737595	524013.805173	41.842407
3504.670037	523991.574848	41.847412
3504.908303	523960.450277	41.852416
3504.804961	523949.396630	41.857421
3504.810324	523931.249079	41.862426
3504.848003	523908.445978	41.867431
3504.716902	523889.763920	41.872436
3504.879149	523855.769920	41.877440
3504.737370	523831.428081	41.882445
3504.416500	523818.285697	41.887450
3504.980127	523786.957722	41.892455
3504.929528	523781.759241	41.897460
3505.074651	523760.101563	41.902464
3504.924128	523731.919267	41.907469
3504.684088	523706.126859	41.912474
3504.803819	523671.987546	41.917479
3504.681095	523656.437919	41.922484
3504.726960	523631.358435	41.927488
3504.748475	523605.827820	41.932493
3504.492013	523591.310247	41.937498
3504.606427	523569.657168	41.942503
3504.409130	523572.468564	41.947508
3504.627672	523538.313351	41.952512
3504.400221	523522.881245	41.957517
3504.675568	523511.211402	41.962522
3504.777994	523491.582085	41.967527
3504.653826	523470.623724	41.972532
3504.926393	523453.039994	41.977536
3504.993232	523427.198637	41.982541
3504.698433	523399.240762	41.987546
3504.778315	523394.779777	41.992551
3504.571519	523378.434375	41.997556
3504.847189	523348.869755	42.002560
3504.530866	523329.154777	42.007565
3504.638764	523315.792564	42.012570
3504.619371	523285.465666	42.017575
3504.381434	523277.061432	42.022580
3504.472161	523257.433680	42.027584
3504.425165	523239.495826	42.032589
3504.374479	523231.264172	42.037594
3504.620596	523204.383119	42.042599
3504.421684	523198.247437	42.047604
3504.531295	523177.858349	42.052608
3504.613420	523154.491106	42.057613
3504.547622	523149.850878	42.062618
3504.899876	523106.473439	42.067623
3504.441795	523117.666972	42.072628
3504.794972	523084.601633	42.077632
3504.550838	523072.609176	42.082637
3504.670168	523037.811429	42.087642
3504.637331	523023.106347	42.092647
3504.539815	523005.125668	42.097652
3504.574665	522991.673631	42.102656
3504.774050	522960.907139	42.107661
3504.557467	522956.543443	42.112666
3504.861916	522934.960580	42.117671
3504.182476	522917.273984	42.122676
3504.470638	522910.555696	42.127680
3504.391683	522879.327530	42.132685
3504.393092	522866.537841	42.137690
3504.523337	522856.659757	42.142695
3504.396031	522837.925331	42.147700
3504.292980	522823.585025	42.152704
3504.639124	522808.769297	42.157709
3504.235388	522794.274285	42.162714
3504.729457	522785.096926	42.167719
3504.522362	522769.205918	42.172724
3504.443919	522747.329463	42.177728
3504.477499	522749.093475	42.182733
3504.070958	522714.479254	42.187738
3504.579593	522706.967758	42.192743
3504.087359	522692.688849	42.197748
3504.437726	522666.093737	42.202752
3504.957400	522658.631026	42.207757
3504.247456	522635.893745	42.212762
3504.366641	522628.848184	42.217767
3504.244299	522616.836139	42.222772
3504.389802	522591.435983	42.227776
3504.388093	522585.268898	42.232781
3504.201180	522570.132788	42.237786
3504.183772	522550.723479	42.242791
3504.235152	522546.721738	42.247796
3504.116018	522542.190870	42.252800
3504.498827	522518.977395	42.257805
3504.222557	522514.218593	42.262810
3504.471511	522506.141420	42.267815
3504.482674	522488.699067	42.272820
3504.470368	522465.042440	42.277824
3504.543060	522457.549181	42.282829
3504.797883	522429.502758	42.287834
3504.563817	522407.953758	42.292839
3504.352093	522390.849844	42.297844
3504.566996	522375.498384	42.302848
3504.567801	522352.547261	42.307853
3504.307531	522346.016529	42.312858
3504.463531	522329.713830	42.317863
3504.369811	522305.665415	42.322868
3503.860398	522298.112428	42.327872
3504.532595	522300.078870	42.332877
3504.542647	522266.914439	42.337882
3504.811660	522248.066137	42.342887
3504.207816	522234.208889	42.347892
3504.337367	522208.608442	42.352896
3504.343983	522203.754284	42.357901
3504.127333	522190.947974	42.362906
3504.109833	522178.009071	42.367911
3504.815908	522159.344353	42.372916
3504.432772	522138.324091	42.377920
3504.507095	522124.561775	42.382925
3504.546186	522123.038998	42.387930
3504.490749	522102.068002	42.392935
3504.412376	522098.440534	42.397940
3504.269680	522079.606556	42.402944
3504.612157	522051.040088	42.407949
3504.557342	522042.100728	42.412954
3504.386529	522016.496899	42.417959
3504.697728	522017.913788	42.422964
3504.496534	521986.753778	42.427968
3504.468000	521970.277670	42.432973
3504.256383	521959.340884	42.437978
3504.278887	521926.932103	42.442983
3504.295075	521926.879001	42.447988
3504.173170	521916.736874	42.452992
3504.141829	521893.436303	42.457997
3504.126760	521880.294561	42.463002
3504.518956	521876.087123	42.468007
3504.472262	521864.972543	42.473012
3504.365214	521839.914457	42.478016
3504.434539	521832.775323	42.483021
3504.373523	521813.928127	42.488026
3504.773887	521798.294036	42.493031
3504.210395	521791.659342	42.498036
3504.154285	521766.643646	42.503040
3503.984876	521748.723491	42.508045
3504.357468	521759.028341	42.513050
3504.358591	521728.948064	42.518055
3504.405616	521716.352479	42.523060
3504.366205	521709.078813	42.528064
3504.273532	521694.836978	42.533069
3504.332169	521686.486151	42.538074
3504.627427	521658.887004	42.543079
3504.271688	521642.563390	42.548084
3504.083535	521638.801505	42.553088
3504.724205	521626.819793	42.558093
3504.436614	521605.985960	42.563098
3504.413124	521594.210310	42.568103
3504.197524	521562.091212	42.573108
3504.057063	521554.429005	42.578112
3504.082392	521553.818348	42.583117
3504.372231	521546.138681	42.588122
3504.277442	521521.179277	42.593127
3504.395976	521514.487225	42.598132
3504.203854	521503.445940	42.603136
3504.293916	521470.267238	42.608141
3504.222152	521472.452485	42.613146
3504.408996	521458.469598	42.618151
3504.388322	521453.821753	42.623156
3504.302149	521437.960883	42.628160
3504.626909	521438.769012	42.633165
3504.074084	521411.859605	42.638170
3504.431169	521393.754732	42.643175
3504.415485	521383.443816	42.648180
3504.354101	521356.608309	42.653184
3504.432115	521347.698130	42.658189
3504.294952	521329.974641	42.663194
3504.182430	521303.399910	42.668199
3504.126660	521314.581647	42.673204
3504.242351	521298.587624	42.678208
3504.012741	521275.671400	42.683213
3504.414237	521280.158015	42.688218
3503.995619	521269.860157	42.693223
3504.434815	521240.013074	42.698228
3504.276552	521229.572927	42.703232
3504.445732	521230.961778	42.708237
3504.272236	521195.498579	42.713242
3504.549034	521190.803641	42.718247
3504.320446	521186.593033	42.723252
3504.102158	521155.383576	42.728256
3504.531029	521137.064846	42.733261
3504.003366	521151.152455	42.738266
3504.360900	521114.644572	42.743271
3504.313026	521117.028317	42.748276
3504.089724	521117.468076	42.753280
3504.039076	521088.608162	42.758285
3503.999556	521081.182562	42.763290
3504.107511	521058.869917	42.768295
3504.092882	521074.494326	42.773300
3504.174744	521054.056403	42.778304
3504.278136	521038.974095	42.783309
3503.796468	521023.883131	42.788314
3504.202778	521021.392184	42.793319
3504.036508	520999.982272	42.798324
3504.074484	520996.032825	42.803329
3504.087101	520984.301584	42.808333
3504.072997	520982.989338	42.813338
3503.952059	520970.116381	42.818343
3504.088330	520968.830923	42.823348
3503.860918	520946.065559	42.828353
3504.071067	520939.813808	42.833357
3503.999375	520955.497907	42.838362
3504.292653	520936.593697	42.843367
3504.230039	520906.875878	42.848372
3504.051022	520906.044707	42.853377
3504.498812	520904.002204	42.858381
3504.096273	520887.381884	42.863386
3504.248953	520868.196472	42.868391
3504.129463	520865.788608	42.873396
3504.385790	520853.816523	42.878401
3504.256439	520818.244412	42.883405
3504.230342	520830.989078	42.888410
3503.854257	520820.178635	42.893415
3504.073464	520798.303070	42.898420
3504.105115	520802.039351	42.903425
3504.249422	520790.792734	42.908429
3504.078534	520788.089635	42.913434
3504.321128	520747.554477	42.918439
3504.117277	520754.917602	42.923444
3504.387545	520745.875591	42.928449
3504.417151	520719.479676	42.933453
3503.919315	520712.429696	42.938458
3503.727258	520706.039195	42.943463
3503.824176	520709.310159	42.948468
3504.108370	520689.294823	42.953473
3503.796147	520683.631119	42.958477
3503.970169	520674.199816	42.963482
3504.209020	520667.185052	42.968487
3504.047399	520673.227027	42.973492
3503.884968	520654.546193	42.978497
3504.482476	520633.267871	42.983501
3503.938716	520634.718900	42.988506
3504.143412	520624.069322	42.993511
3504.645981	520595.677238	42.998516
3503.672490	520587.741775	43.003521
3504.005030	520584.352371	43.008525
3504.042755	520587.430482	43.013530
3504.021446	520566.654348	43.018535
3504.236914	520549.177626	43.023540
3504.230440	520556.560201	43.028545
3504.456944	520543.884785	43.033549
3504.303021	520526.870892	43.038554
3504.290174	520512.261498	43.043559
3504.194344	520505.653474	43.048564
3504.290733	520481.875670	43.053569
3504.279606	520473.838601	43.058573
3504.414402	520468.458079	43.063578
3504.301053	520432.377011	43.068583
3504.245655	520432.234101	43.073588
3503.980907	520422.366416	43.078593
3504.073719	520389.134524	43.083597
3504.205397	520400.186141	43.088602
3504.259119	520390.419777	43.093607
3504.049563	520373.515635	43.098612
3503.637622	520353.104326	43.103617
3504.195951	520343.713210	43.108621
3503.986484	520340.915016	43.113626
3504.195050	520338.960814	43.118631
3503.917344	520332.583703	43.123636
3503.955210	520325.954476	43.128641
3504.440689	520296.553391	43.133645
3503.958455	520315.235431	43.138650
3503.769358	520285.688151	43.143655
3503.706774	520276.496254	43.148660
3503.618157	520262.758122	43.153665
3504.044225	520267.038897	43.158669
3503.852855	520270.052159	43.163674
3504.097306	520265.311511	43.168679
3503.979014	520265.835812	43.173684
3503.995291	520254.255147	43.178689
3504.033649	520239.283500	43.183693
3503.898049	520235.968018	43.188698
3503.756617	520234.524158	43.193703
3504.049096	520227.905207	43.198708
3504.082274	520213.187152	43.203713
3504.263527	520205.776819	43.208717
3503.711263	520199.544171	43.213722
3503.843871	520196.843564	43.218727
3504.044441	520188.014501	43.223732
3503.670728	520190.702680	43.228737
3504.076556	520168.999016	43.233741
3503.971678	520171.037991	43.238746
3503.990958	520163.451001	43.243751
3503.945389	520164.873886	43.248756
3504.350397	520157.074248	43.253761
3504.160074	520129.700948	43.258765
3504.021356	520134.273266	43.263770
3504.024153	520121.278963	43.268775
3503.885160	520108.863220	43.273780
3503.834210	520093.753875	43.278785
3504.229774	520085.702896	43.283789
3504.234158	520088.027971	43.288794
3504.292441	520068.502624	43.293799
3504.260760	520053.946357	43.298804
3504.179741	520042.937081	43.303809
3504.378814	520024.350070	43.308813
3504.124586	520031.772041	43.313818
3504.172856	520001.782250	43.318823
3504.304405	520008.283734	43.323828
3504.087717	519986.678222	43.328833
3504.098267	519963.519956	43.333837
3504.103504	519959.170951	43.338842
3504.392071	519950.884016	43.343847
3503.958437	519927.897026	43.348852
3503.686520	519926.676005	43.353857
3503.804235	519920.590157	43.358861
3503.947187	519916.775539	43.363866
3504.110951	519918.772084	43.368871
3504.478347	519892.321446	43.373876
3504.119472	519885.501945	43.378881
3504.300902	519872.125287	43.383885
3504.131220	519862.848964	43.388890
3503.913648	519841.951250	43.393895
3504.043593	519841.071190	43.398900
3503.986039	519848.310476	43.403905
3503.780921	519831.961241	43.408909
3503.670241	519814.939772	43.413914
3503.717658	519800.168535	43.418919
3503.854177	519797.871731	43.423924
3503.900434	519793.718442	43.428929
3504.235149	519792.098163	43.433933
3504.271198	519791.384624	43.438938
3504.091906	519772.300961	43.443943
3504.456822	519765.114205	43.448948
3504.076747	519757.185661	43.453953
3504.302015	519729.290957	43.458957
3504.016117	519717.605990	43.463962
3503.922750	519716.761220	43.468967
3504.286434	519715.237477	43.473972
3503.824496	519688.614226	43.478977
3503.989029	519682.166962	43.483981
3503.892963	519681.929351	43.488986
3503.902349	519672.877423	43.493991
3504.026246	519682.110552	43.498996
3503.651600	519661.844168	43.504001
3503.900298	519635.159071	43.509005
3503.939650	519635.456230	43.514010
3504.365806	519636.754040	43.519015
3504.267957	519624.028058	43.524020
3503.781298	519619.352219	43.529025
3503.973902	519608.349965	43.534029
3504.026117	519595.802488	43.539034
3504.380365	519600.347599	43.544039
3504.572675	519569.221900	43.549044
3504.135866	519564.335921	43.554049
3504.410302	519546.444319	43.559053
3503.684242	519536.750134	43.564058
3504.229297	519533.225804	43.569063
3504.299660	519528.310213	43.574068
3504.228964	519520.332654	43.579073
3504.391174	519495.885715	43.584077
3503.942258	519491.304998	43.589082
3503.987309	519483.915867	43.594087
3504.048644	519474.956743	43.599092
3504.017097	519460.197681	43.604097
3504.291949	519449.586816	43.609101
3504.149132	519448.345353	43.614106
3503.950594	519427.090167	43.619111
3504.028161	519414.740793	43.624116
3503.783021	519400.167123	43.629121
3504.097271	519407.398398	43.634125
3504.140831	519396.571246	43.639130
3504.204440	519379.420654	43.644135
3503.976744	519371.012778	43.649140
3503.890377	519367.790462	43.654145
3504.240756	519355.094550	43.659149
3504.041218	519345.165344	43.664154
3503.915259	519322.179436	43.669159
3504.185444	519307.878169	43.674164
3503.725128	519316.142033	43.679169
3503.983576	519312.662957	43.684173
3503.649757	519291.934602	43.689178
3503.722662	519271.141936	43.694183
3503.937520	519271.360799	43.699188
3504.104037	519277.098610	43.704193
3504.253508	519283.344736	43.709197
3504.203569	519268.285034	43.714202
3504.208885	519232.485944	43.719207
3504.096147	519237.256655	43.724212
3503.900750	519232.130169	43.729217
3504.158358	519224.859014	43.734221
3503.947991	519213.616812	43.739226
3503.868694	519186.072701	43.744231
3503.682292	519200.866480	43.749236
3503.853920	519196.642662	43.754241
3503.785006	519190.080416	43.759245
3503.804239	519184.464926	43.764250
3503.635690	519162.395655	43.769255
3503.648738	519163.303734	43.774260
3503.480977	519151.751379	43.779265
3503.916063	519143.946508	43.784269
3503.903487	519149.813796	43.789274
3504.054233	519143.368501	43.794279
3504.137860	519142.091222	43.799284
3503.971001	519138.982710	43.804289
3503.810454	519121.563901	43.809293
3503.749371	519117.376845	43.814298
3503.667688	519118.451588	43.819303
3503.636993	519120.125027	43.824308
3503.538076	519126.107095	43.829313
3503.797428	519125.054856	43.834317
3503.832107	519132.431567	43.839322
3503.805876	519101.390088	43.844327
3503.804659	519092.895710	43.849332
3503.508248	519087.330077	43.854337
3503.968160	519088.116967	43.859341
3503.995585	519086.545189	43.864346
3503.778144	519088.551526	43.869351
3503.974140	519085.385651	43.874356
3503.951837	519063.899889	43.879361
3504.098144	519047.089821	43.884365
3503.894796	519053.695180	43.889370
3504.181410	519048.998082	43.894375
3504.275948	519028.656758	43.899380
3503.843703	519014.011191	43.904385
3504.123976	519001.831721	43.909389
3504.208169	519005.711797	43.914394
3504.020670	518993.050058	43.919399
3503.717715	518977.777264	43.924404
3503.822960	518969.063742	43.929409
3504.213914	518964.198438	43.934413
3503.764422	518966.190903	43.939418
3503.927069	518963.232530	43.944423
3504.028067	518942.283318	43.949428
3503.975370	518925.706834	43.954433
3504.164368	518927.446695	43.959437
3504.226692	518929.965031	43.964442
3503.808625	518913.142903	43.969447
3503.872863	518899.783977	43.974452
3504.036633	518899.555849	43.979457
3504.176487	518889.673851	43.984461
3504.011207	518894.301275	43.989466
3504.209319	518867.673493	43.994471
3504.269168	518841.977670	43.999476
3503.987917	518856.483366	44.004481
3503.963928	518845.464273	44.009485
3504.286773	518823.215751	44.014490
3503.799452	518814.798061	44.019495
3504.117326	518811.157796	44.024500
3504.278520	518808.503008	44.029505
3504.436980	518777.077779	44.034509
3504.098843	518784.412444	44.039514
3504.297809	518768.200537	44.044519
3504.276686	518747.776019	44.049524
3504.234757	518746.215171	44.054529
3504.334809	518723.850037	44.059533
3504.283984	518715.514998	44.064538
3504.320492	518696.699361	44.069543
3504.450064	518681.509620	44.074548
3504.009278	518673.792402	44.079553
3504.359715	518643.600682	44.084557
3504.160940	518634.732778	44.089562
3503.927276	518640.432934	44.094567
3504.351431	518604.566278	44.099572
3503.917612	518594.521955	44.104577
3503.874686	518598.270525	44.109581
3504.276173	518598.965546	44.114586
3503.982657	518578.887260	44.119591
3504.177856	518564.900589	44.124596
3504.181935	518562.624548	44.129601
3504.526973	518548.209663	44.134605
3504.024484	518529.226203	44.139610
3503.961901	518520.033323	44.144615
3504.191150	518513.322550	44.149620
3504.002554	518506.121605	44.154625
3504.010783	518483.315575	44.159629
3504.003483	518475.175794	44.164634
3503.820315	518472.727076	44.169639
3503.963867	518468.001861	44.174644
3503.763103	518467.527955	44.179649
3504.165659	518440.968300	44.184653
3503.531057	518439.551664	44.189658
3503.743279	518436.484232	44.194663
3503.944539	518425.024735	44.199668
3503.785513	518424.291406	44.204673
3504.183967	518426.099345	44.209677
3503.915069	518407.331650	44.214682
3503.831712	518387.523304	44.219687
3503.778133	518383.992221	44.224692
3503.745186	518389.711303	44.229697
3503.915844	518384.425564	44.234701
3503.687879	518389.720383	44.239706
3503.662975	518383.251989	44.244711
3503.865064	518355.662014	44.249716
3503.868182	518362.437276	44.254721
3503.970361	518345.077250	44.259725
3503.979855	518344.721804	44.264730
3504.087567	518346.828532	44.269735
3503.984680	518333.192172	44.274740
3504.036442	518318.166092	44.279745
3504.043158	518303.349379	44.284749
3504.004065	518304.771401	44.289754
3503.685640	518311.041287	44.294759
3503.972588	518307.102407	44.299764
3503.644317	518283.034586	44.304769
3504.074549	518277.202129	44.309773
3503.894984	518268.027598	44.314778
3504.116687	518261.671875	44.319783
3504.043580	518257.031410	44.324788
3503.786740	518255.757312	44.329793
3503.845434	518237.190472	44.334797
3503.992706	518234.740055	44.339802
3503.847285	518236.178889	44.344807
3504.145484	518236.081202	44.349812
3503.890204	518215.035682	44.354817
3503.934374	518186.509636	44.359821
3503.719451	518190.083221	44.364826
3504.083606	518194.172068	44.369831
3504.027262	518190.085158	44.374836
3503.880743	518179.894039	44.379841
3504.114366	518150.731198	44.384845
3504.299196	518154.039343	44.389850
3503.907869	518145.757834	44.394855
3504.123856	518139.200704	44.399860
3504.146970	518119.476340	44.404865
3504.124563	518101.630090	44.409869
3503.664909	518109.843883	44.414874
3504.043982	518108.418696	44.419879
3504.102961	518090.053911	44.424884
3503.967340	518072.528920	44.429889
3504.144828	518069.871439	44.434893
3503.944003	518067.273753	44.439898
3504.216323	518066.826193	44.444903
3504.190912	518043.721475	44.449908
3503.931437	518022.069577	44.454913
3504.102626	518021.991964	44.459917
3503.876533	518028.247363	44.464922
3503.983887	518004.312546	44.469927
3503.959103	517991.017522	44.474932
3503.443546	517986.143515	44.479937
3503.675952	517988.887944	44.484941
3503.739532	517986.652984	44.489946
3503.880549	517987.035238	44.494951
3504.050447	517991.761635	44.499956
3503.853494	517963.677848	44.504961
3503.725929	517946.606548	44.509965
3503.951707	517946.419174	44.514970
3503.881545	517936.367535	44.519975
3503.745017	517940.788414	44.524980
3503.871602	517940.566152	44.529985
3503.988708	517926.540718	44.534989
3503.918859	517920.129813	44.539994
3504.038460	517911.817997	44.544999
3504.244545	517904.756673	44.550004
3503.696966	517907.573831	44.555009
3504.001196	517896.755060	44.560013
3503.993181	517883.052766	44.565018
3503.815852	517869.225521	44.570023
3504.212997	517865.420821	44.575028
3503.829629	517870.083000	44.580033
3503.673340	517865.202739	44.585037
3503.740253	517852.853879	44.590042
3503.728368	517836.472117	44.595047
3504.177237	517816.326130	44.600052
3503.827240	517827.708444	44.605057
3503.957728	517819.040893	44.610061
3503.926763	517827.136501	44.615066
3503.932610	517802.560066	44.620071
3504.121737	517781.949421	44.625076
3504.073231	517787.822872	44.630081
3504.340346	517778.172931	44.635085
3504.174043	517761.562667	44.640090
3504.085058	517744.586195	44.645095
3503.730623	517745.603003	44.650100
3503.715731	517749.600170	44.655105
3503.953017	517732.926087	44.660109
3503.723662	517726.085213	44.665114
3503.815685	517713.985117	44.670119
3504.370360	517697.463102	44.675124
3503.967948	517700.914724	44.680129
3504.023647	517687.202197	44.685133
3504.042864	517692.053631	44.690138
3503.780827	517663.524515	44.695143
3504.048369	517665.252097	44.700148
3503.996425	517657.978615	44.705153
3504.153312	517652.037443	44.710157
3504.108124	517639.908412	44.715162
3503.853807	517629.430587	44.720167
3504.159184	517612.442216	44.725172
3503.606740	517620.418078	44.730177
3504.033180	517617.164933	44.735181
3503.836072	517611.785373	44.740186
3504.259058	517586.232470	44.745191
3503.974170	517587.895674	44.750196
3503.728338	517580.703370	44.755201
3503.921704	517581.835874	44.760205
3503.730077	517575.747489	44.765210
3503.796269	517550.250924	44.770215
3503.943073	517538.698287	44.775220
3503.802167	517543.423370	44.780225
3503.907025	517540.676149	44.785229
3503.858677	517545.993415	44.790234
3503.801956	517540.895049	44.795239
3504.226665	517507.352045	44.800244
3503.681773	517514.012000	44.805249
3504.398747	517501.914107	44.810253
3503.896718	517497.745766	44.815258
3503.978026	517500.615295	44.820263
3503.773713	517474.503986	44.825268
3503.948684	517451.923018	44.830273
3503.886597	517454.006131	44.835277
3503.810864	517456.192537	44.840282
3503.939509	517461.077311	44.845287
3504.019911	517460.255526	44.850292
3503.878202	517435.499597	44.855297
3504.076447	517415.948986	44.860301
3504.144373	517424.534841	44.865306
3504.199423	517413.704573	44.870311
3503.758543	517390.310634	44.875316
3503.539096	517389.030557	44.880321
3503.747492	517378.782846	44.885325
3503.812928	517386.711728	44.890330
3503.730821	517380.201414	44.895335
3503.926017	517380.777392	44.900340
3503.659334	517379.858757	44.905345
3503.481483	517379.482333	44.910349
3503.705333	517382.531626	44.915354
3503.553698	517358.889652	44.920359
3503.793844	517346.108488	44.925364
3503.777583	517342.369011	44.930369
3503.885201	517342.402580	44.935373
3503.520709	517336.189724	44.940378
3503.840212	517334.824458	44.945383
3503.716603	517339.294023	44.950388
3503.691750	517333.381462	44.955393
3503.766350	517337.870268	44.960397
3503.815018	517310.757917	44.965402
3503.540325	517303.620623	44.970407
3503.903837	517291.275034	44.975412
3503.707600	517306.729451	44.980417
3503.681646	517292.675524	44.985421
3503.821772	517307.065407	44.990426
3503.604468	517300.323588	44.995431
3504.027007	517299.498287	45.000436
3503.753846	517296.052246	45.005441
3504.048454	517271.328246	45.010445
3503.918679	517276.911311	45.015450
3503.883050	517264.224241	45.020455
3504.089267	517265.506441	45.025460
3504.205118	517258.762517	45.030465
3504.026959	517231.635320	45.035469
3504.013878	517233.205028	45.040474
3504.005205	517220.817075	45.045479
3504.014099	517203.015478	45.050484
3503.637673	517203.176124	45.055489
3503.605527	517179.515008	45.060493
3503.719222	517174.136749	45.065498
3503.591702	517178.202425	45.070503
3503.996426	517176.520263	45.075508
3503.839204	517184.130452	45.080513
3503.829598	517174.422761	45.085517
3503.807377	517177.814398	45.090522
3503.915849	517161.362377	45.095527
3504.158053	517141.349374	45.100532
3503.943641	517135.921824	45.105537
3503.963237	517144.313188	45.110541
3504.149372	517132.349500	45.115546
3503.478269	517122.948609	45.120551
3503.956686	517106.134646	45.125556
3503.804843	517102.113130	45.130561
3504.064179	517094.436216	45.135565
3504.125560	517099.331729	45.140570
3503.622444	517100.928334	45.145575
3503.866890	517075.301727	45.150580
3503.818262	517065.852986	45.155585
3503.794284	517056.400343	45.160589
3504.095072	517066.618363	45.165594
3503.738193	517061.213307	45.170599
3503.670679	517049.997619	45.175604
3503.902241	517062.249354	45.180609
3504.147550	517028.986586	45.185613
3504.322777	517021.525210	45.190618
3503.891729	517023.110431	45.195623
3504.233134	517003.435569	45.200628
3504.007025	517000.538293	45.205633
3503.895476	516979.771898	45.210637
3504.030738	516973.682193	45.215642
3503.975222	516980.366149	45.220647
3504.217324	516967.786663	45.225652
3504.132016	516950.303101	45.230657
3504.169461	516941.144102	45.235661
3504.119553	516939.331496	45.240666
3503.644071	516923.426664	45.245671
3503.872626	516898.459701	45.250676
3503.895103	516905.333638	45.255681
3503.847378	516895.783519	45.260685
3504.008534	516879.575739	45.265690
3503.900420	516897.595667	45.270695
3503.885059	516871.605252	45.275700
3504.002281	516866.580325	45.280705
3503.707709	516848.421754	45.285709
3503.946289	516850.356281	45.290714
3503.892606	516860.276466	45.295719
3504.167090	516842.938202	45.300724
3503.732267	516835.370887	45.305729
3503.456943	516812.101673	45.310733
3503.791383	516818.167789	45.315738
3503.710066	516806.347279	45.320743
3503.742558	516809.123503	45.325748
3503.837872	516805.012280	45.330753
3503.616106	516807.879262	45.335757
3503.888536	516811.376113	45.340762
3503.696598	516801.646453	45.345767
3503.867920	516791.555951	45.350772
3503.735763	516777.012673	45.355777
3503.469030	516774.273488	45.360781
3503.819822	516760.311274	45.365786
3503.693039	516775.603497	45.370791
3503.978599	516773.131008	45.375796
3504.170363	516776.691186	45.380801
3503.804408	516759.403492	45.385805
3503.717930	516742.425597	45.390810
3503.681103	516735.351601	45.395815
3504.187450	516733.501623	45.400820
3503.795104	516732.147681	45.405825
3504.039513	516730.945946	45.410829
3504.238768	516729.801919	45.415834
3503.851225	516696.486802	45.420839
3503.963272	516698.036783	45.425844
3503.846362	516689.508886	45.430849
3503.804815	516694.016224	45.435853
3504.054051	516680.120565	45.440858
3503.650814	516664.254634	45.445863
3504.177676	516654.107853	45.450868
3503.970337	516643.975971	45.455873
3504.064302	516654.884352	45.460877
3503.991515	516641.848685	45.465882
3503.971510	516627.641544	45.470887
3504.017155	516611.755184	45.475892
3503.787212	516618.466855	45.480897
3503.776791	516613.158604	45.485901
3503.993883	516609.988925	45.490906
3503.632088	516600.639988	45.495911
3503.809428	516573.202672	45.500916
3503.444951	516572.350019	45.505921
3503.618858	516557.707602	45.510925
3503.666838	516555.373775	45.515930
3503.749183	516580.089852	45.520935
3503.972255	516563.113419	45.525940
3503.627722	516571.916620	45.530945
3503.970044	516569.839696	45.535949
3504.074387	516541.604734	45.540954
3503.780198	516541.853527	45.545959
3503.794673	516521.926344	45.550964
3503.563402	516528.435978	45.555969
3503.574456	516514.324972	45.560973
3503.651790	516521.948961	45.565978
3503.754923	516525.927768	45.570983
3503.874449	516528.488000	45.575988
3503.651766	516513.756517	45.580993
3503.612813	516493.129752	45.585997
3503.820937	516486.775498	45.591002
3503.583136	516488.937076	45.596007
3503.942363	516478.968398	45.601012
3503.898644	516484.234701	45.606017
3503.975023	516479.064400	45.611021
3504.062235	516488.810824	45.616026
3504.057108	516470.100380	45.621031
3503.937684	516442.912039	45.626036
3503.766741	516458.970099	45.631041
3504.102791	516451.837047	45.636045
3504.239068	516450.854668	45.641050
3504.011473	516428.689936	45.646055
3504.292266	516410.338803	45.651060
3504.104609	516404.249358	45.656065
3503.777623	516383.617412	45.661069
3503.933165	516368.320306	45.666074
3503.786805	516374.664865	45.671079
3503.934968	516359.470059	45.676084
3503.942812	516363.514538	45.681089
3504.072001	516350.800719	45.686093
3504.076058	516331.785240	45.691098
3504.066370	516324.099922	45.696103
3504.033213	516320.008885	45.701108
3503.776777	516320.656286	45.706113
3503.794407	516316.203220	45.711117
3503.976695	516290.130086	45.716122
3503.648634	516291.699096	45.721127
3504.170017	516286.053826	45.726132
3503.961893	516296.099901	45.731137
3504.017279	516287.291707	45.736141
3504.066327	516262.453307	45.741146
3503.872909	516252.116698	45.746151
3503.827955	516238.368313	45.751156
3503.698061	516240.968012	45.756161
3503.694016	516237.074640	45.761165
3503.904560	516237.496519	45.766170
3503.804453	516238.321500	45.771175
3503.851842	516209.032970	45.776180
3503.559804	516211.405443	45.781185
3503.409074	516197.471455	45.786189
3503.863128	516195.730828	45.791194
3503.868140	516200.584944	45.796199
3503.979238	516195.661926	45.801204
3503.870540	516205.388910	45.806209
3503.819764	516195.080292	45.811213
3503.912111	516169.830335	45.816218
3503.838087	516165.948007	45.821223
3504.197327	516152.793100	45.826228
3504.017799	516154.642078	45.831233
3503.852752	516156.387623	45.836237
3504.088341	516120.444262	45.841242
3503.725957	516124.648460	45.846247
3503.941399	516117.332040	45.851252
3504.003875	516112.972977	45.856257
3503.971792	516103.773934	45.861261
3503.961838	516087.946435	45.866266
3504.005546	516082.275453	45.871271
3503.933260	516069.744981	45.876276
3503.530587	516076.130165	45.881281
3503.543770	516079.364714	45.886285
3503.691573	516063.765118	45.891290
3504.052673	516075.643101	45.896295
3503.925663	516049.820766	45.901300
3503.853588	516038.554545	45.906305
3503.737019	516028.559657	45.911309
3503.675375	516030.288871	45.916314
3503.629676	516025.896310	45.921319
3504.006025	516027.960876	45.926324
3503.901641	516030.202569	45.931329
3503.618411	516014.165331	45.936333
3503.884274	515998.496442	45.941338
3503.655199	515994.082284	45.946343
3503.815938	515988.949070	45.951348
3504.089585	515989.967851	45.956353
3503.950701	515983.718826	45.961357
3504.171010	515979.789933	45.966362
3503.950767	515965.158723	45.971367
3504.030982	515951.643180	45.976372
3503.824066	515945.303748	45.981377
3503.636909	515956.813319	45.986381
3503.733248	515939.755137	45.991386
3503.817897	515952.435492	45.996391
3503.987102	515929.094781	46.001396
3503.483138	515912.991189	46.006401
3503.792351	515888.920274	46.011405
3503.881954	515899.475830	46.016410
3503.467180	515913.752335	46.021415
3503.820551	515897.462647	46.026420
3503.972365	515891.926232	46.031425
3504.459971	515892.203182	46.036429
3504.278854	515862.596151	46.041434
3504.058119	515868.649220	46.046439
3504.077072	515848.265369	46.051444
3504.092231	515836.479493	46.056449
3503.904290	515819.112110	46.061453
3504.287767	515811.010403	46.066458
3503.981849	515823.651442	46.071463
3504.075317	515799.867364	46.076468
3503.796467	515794.601278	46.081473
3503.729166	515787.177684	46.086477
3503.876663	515784.069424	46.091482
3504.236784	515784.771112	46.096487
3504.205915	515768.036299	46.101492
3504.074136	515754.503530	46.106497
3503.578322	515731.115934	46.111501
3503.998599	515736.562001	46.116506
3503.755803	515730.784464	46.121511
3503.813869	515729.308673	46.126516
3503.687956	515705.306268	46.131521
3503.800598	515698.359927	46.136525
3503.816526	515687.939306	46.141530
3503.731106	515695.943411	46.146535
3503.860914	515682.925546	46.151540
3503.856318	515689.045664	46.156545
3504.009862	515684.368654	46.161549
3504.022416	515664.187883	46.166554
3503.825381	515663.763875	46.171559
3504.031454	515653.869487	46.176564
3503.994918	515654.583302	46.181569
3504.012248	515651.849605	46.186573
3503.853515	515629.470631	46.191578
3503.598061	515634.012065	46.196583
3504.137137	515613.899733	46.201588
3503.769136	515615.222249	46.206593
3503.839882	515620.167291	46.211597
3503.766353	515607.940110	46.216602
3503.886798	515620.817354	46.221607
3503.741948	515603.038346	46.226612
3503.977430	515569.470777	46.231617
3503.879878	515578.134316	46.236621
3503.635086	515582.977521	46.241626
3503.967095	515569.624165	46.246631
3503.952266	515558.652014	46.251636
3503.784290	515545.529387	46.256641
3503.827613	515539.807708	46.261645
3504.133271	515530.302097	46.266650
3503.619390	515535.238421	46.271655
3503.828579	515524.736578	46.276660
3504.004370	515534.773003	46.281665
3503.794756	515509.418053	46.286669
3503.962718	515498.720414	46.291674
3503.865212	515491.807202	46.296679
3503.889064	515483.307012	46.301684
3503.834433	515499.094741	46.306689
3503.819941	515481.598443	46.311693
3504.119580	515479.629281	46.316698
3503.439466	515459.203726	46.321703
3503.706142	515447.681266	46.326708
3504.079924	515448.886551	46.331713
3503.461145	515453.890053	46.336717
3503.633825	515440.157185	46.341722
3503.407116	515466.339838	46.346727
3504.043940	515450.662376	46.351732
3503.667257	515450.266758	46.356737
3503.818870	515445.033671	46.361741
3503.865890	515422.318454	46.366746
3503.277880	515409.818426	46.371751
3503.611347	515403.747395	46.376756
3503.692749	515400.143768	46.381761
3503.768230	515401.396205	46.386765
3503.625110	515394.287866	46.391770
3503.511384	515405.937932	46.396775
3503.587454	515391.107660	46.401780
3503.517871	515402.649603	46.406785
3503.852289	515404.316281	46.411789
3503.956931	515393.982603	46.416794
3503.748556	515401.247669	46.421799
3503.688467	515384.163071	46.426804
3503.847587	515361.227754	46.431809
3503.837081	515354.149012	46.436813
3503.930542	515363.288214	46.441818
3503.650824	515359.337061	46.446823
3503.919107	515350.444149	46.451828
3503.814696	515350.511237	46.456833
3503.964450	515328.791142	46.461837
3503.799398	515313.139147	46.466842
3503.745157	515326.752272	46.471847
3503.509381	515320.467738	46.476852
3504.023407	515313.306071	46.481857
3503.641131	515319.486020	46.486861
3503.723757	515311.178751	46.491866
3503.581400	515317.472503	46.496871
3503.663014	515296.774627	46.501876
3503.589383	515283.434584	46.506881
3503.521204	515294.116611	46.511885
3503.755940	515288.263442	46.516890
3503.506766	515277.277571	46.521895
3503.722478	515274.613606	46.526900
3503.527673	515282.837497	46.531905
3503.864125	515277.625718	46.536909
3504.221932	515280.249630	46.541914
3504.074102	515277.744275	46.546919
3504.195801	515248.846913	46.551924
3503.958641	515238.010841	46.556929
3503.981673	515238.664683	46.561933
3504.200012	515227.908334	46.566938
3504.000171	515218.128422	46.571943
3503.883219	515187.195106	46.576948
3503.873381	515211.068009	46.581953
3504.071750	515191.009021	46.586957
3504.274182	515184.098850	46.591962
3503.893705	515172.678489	46.596967
3503.718898	515142.057684	46.601972
3503.921373	515146.476295	46.606977
3503.720816	515140.944752	46.611981
3503.712661	515136.950623	46.616986
3504.049875	515145.141066	46.621991
3503.936513	515121.742740	46.626996
3503.836005	515110.834412	46.632001
3503.870846	515104.355297	46.637005
3503.925003	515095.192643	46.642010
3503.742790	515112.821608	46.647015
3503.698059	515095.886013	46.652020
3504.066493	515075.445980	46.657025
3503.793464	515065.475245	46.662029
3503.903754	515065.255523	46.667034
3503.908977	515062.827095	46.672039
3504.013382	515069.941717	46.677044
3503.880614	515062.022396	46.682049
3503.806542	515039.224647	46.687053
3504.004256	515014.462043	46.692058
3503.804757	515025.367299	46.697063
3503.771769	515022.287425	46.702068
3504.139205	515018.233903	46.707073
3504.000436	515008.646516	46.712077
3504.126075	514986.120582	46.717082
3503.478474	514985.110290	46.722087
3503.863707	514982.571211	46.727092
3504.013183	514968.234718	46.732097
3504.071063	514974.952129	46.737101
3504.036485	514947.697365	46.742106
3503.990921	514954.178257	46.747111
3503.981248	514943.306038	46.752116
3504.106010	514942.679421	46.757121
3503.928117	514918.633527	46.762125
3503.948626	514899.057484	46.767130
3503.792337	514901.459259	46.772135
3503.821337	514895.284441	46.777140
3503.692947	514896.872594	46.782145
3503.476229	514898.424133	46.787149
3504.057463	514884.373356	46.792154
3503.517344	514876.214876	46.797159
3503.715179	514856.964787	46.802164
3503.704806	514848.419108	46.807169
3503.848054	514852.695430	46.812173
3503.850037	514852.644552	46.817178
3503.767750	514859.384164	46.822183
3503.521869	514849.105553	46.827188
3503.801964	514849.213021	46.832193
3503.809035	514848.099244	46.837197
3503.866263	514833.018577	46.842202
3503.651277	514817.070553	46.847207
3503.655153	514822.380433	46.852212
3504.063456	514808.306349	46.857217
3503.748858	514809.418181	46.862221
3503.560896	514806.008730	46.867226
3503.544464	514807.275739	46.872231
3503.937612	514817.429970	46.877236
3503.512484	514817.648903	46.882241
3503.650634	514788.191810	46.887245
3503.579411	514786.078881	46.892250
3503.572404	514775.914198	46.897255
3503.887036	514789.520032	46.902260
3504.117219	514783.920289	46.907265
3503.823508	514782.500016	46.912269
3503.622110	514779.193835	46.917274
3503.588396	514788.606333	46.922279
3503.708641	514782.164171	46.927284
3503.474509	514772.439993	46.932289
3503.477394	514750.135449	46.937293
3503.866770	514745.117445	46.942298
3503.788321	514744.775822	46.947303
3503.809145	514743.710441	46.952308
3504.057112	514742.811463	46.957313
3503.812277	514744.873221	46.962317
3503.795120	514737.744693	46.967322
3503.846829	514728.177615	46.972327
3503.785729	514709.777504	46.977332
3503.885319	514704.248951	46.982337
3503.509338	514701.526689	46.987341
3503.598424	514695.139996	46.992346
3503.657648	514689.061478	46.997351
3503.667832	514694.623283	47.002356
3503.995320	514703.624704	47.007361
3503.582045	514699.492197	47.012365
3503.453945	514686.716628	47.017370
3503.447188	514708.769009	47.022375
3503.593337	514692.510904	47.027380
3503.363364	514690.726514	47.032385
3503.297581	514699.992402	47.037389
3504.000056	514686.428060	47.042394
3503.723544	514677.620901	47.047399
3503.441244	514659.862615	47.052404
3503.555937	514649.172854	47.057409
3503.883776	514648.463552	47.062413
3503.957851	514646.782829	47.067418
3503.547792	514651.703000	47.072423
3503.878635	514645.176923	47.077428
3503.743112	514650.610043	47.082433
3503.522902	514653.021957	47.087437
3503.811056	514636.488470	47.092442
3503.547719	514624.492877	47.097447
3503.581294	514622.464517	47.102452
3503.814432	514615.549259	47.107457
3503.917301	514613.914558	47.112461
3503.933783	514604.555284	47.117466
3503.520100	514622.878846	47.122471
3503.678416	514608.439495	47.127476
3503.898218	514611.287633	47.132481
3503.914512	514596.516683	47.137485
3503.937180	514580.632024	47.142490
3503.837706	514577.967191	47.147495
3503.766454	514571.150602	47.152500
3503.741852	514564.225484	47.157505
3503.706453	514565.748393	47.162509
3503.857390	514561.223213	47.167514
3503.642293	514552.406281	47.172519
3503.640637	514546.792526	47.177524
3503.928577	514522.672435	47.182529
3503.482518	514533.718134	47.187533
3503.757533	514524.115645	47.192538
3503.671320	514521.296976	47.197543
3503.658133	514526.508492	47.202548
3504.007103	514524.480847	47.207553
3503.848748	514524.000118	47.212557
3504.159181	514511.053947	47.217562
3503.644777	514496.215058	47.222567
3503.862963	514493.601157	47.227572
3503.800813	514478.690770	47.232577
3503.739769	514490.586030	47.237581
3503.671201	514485.083985	47.242586
3503.553827	514490.868327	47.247591
3503.877852	514474.733628	47.252596
3503.404478	514473.999227	47.257601
3503.640775	514455.652985	47.262605
3503.804629	514449.911883	47.267610
3503.804526	514453.654617	47.272615
3503.817751	514436.254001	47.277620
3504.221103	514437.909883	47.282625
3503.683927	514440.169616	47.287629
3503.675028	514436.984673	47.292634
3503.756035	514441.574402	47.297639
3503.919732	514416.765715	47.302644
3503.887144	514400.737888	47.307649
3503.939674	514404.168851	47.312653
3503.919169	514400.530539	47.317658
3503.719514	514414.521430	47.322663
3503.971764	514387.827347	47.327668
3504.067173	514366.165173	47.332673
3503.577244	514362.348163	47.337677
3503.721989	514358.026217	47.342682
3503.841866	514361.952317	47.347687
3503.916568	514349.195013	47.352692
3503.778216	514348.154766	47.357697
3503.448032	514355.793578	47.362701
3503.698744	514339.973802	47.367706
3503.692484	514322.980768	47.372711
3503.798537	514310.825409	47.377716
3504.281040	514309.332986	47.382721
3503.858374	514316.581813	47.387725
3504.211426	514308.686503	47.392730
3503.968056	514304.729353	47.397735
3503.872837	514282.642003	47.402740
3503.960599	514281.110814	47.407745
3503.695797	514275.133939	47.412749
3503.887023	514279.503981	47.417754
3503.988884	514270.535647	47.422759
3503.558423	514244.657332	47.427764
3504.204308	514236.766281	47.432769
3503.930024	514234.078445	47.437773
3503.701756	514232.243157	47.442778
3503.529387	514218.816717	47.447783
3503.805761	514226.460872	47.452788
3503.998301	514221.878448	47.457793
3504.024273	514199.721256	47.462797
3503.865656	514183.814298	47.467802
3503.405613	514186.618230	47.472807
3503.649933	514182.381657	47.477812
3503.679382	514183.439149	47.482817
3503.732581	514188.387388	47.487821
3503.953870	514179.804753	47.492826
3503.907867	514191.697847	47.497831
3503.989803	514165.131486	47.502836
3503.942176	514151.634697	47.507841
3504.028784	514148.687493	47.512845
3504.100892	514142.707898	47.517850
3504.182733	514133.692078	47.522855
3503.734846	514113.329324	47.527860
3504.205986	514102.785189	47.532865
3503.723629	514100.787735	47.537869
3503.824746	514103.705298	47.542874
3503.780769	514109.680483	47.547879
3503.978948	514070.602791	47.552884
3503.924893	514063.682121	47.557889
3503.711726	514065.233173	47.562893
3503.950180	514048.049447	47.567898
3503.974063	514059.122336	47.572903
3503.653938	514053.103547	47.577908
3504.007480	514031.804769	47.582913
3503.681993	514018.402370	47.587917
3503.711235	514021.988827	47.592922
3503.752359	514014.850779	47.597927
3503.891330	514009.467510	47.602932
3504.192566	514011.088997	47.607937
3503.856752	513998.143420	47.612941
3504.126027	513977.616569	47.617946
3504.130999	513973.670667	47.622951
3503.761153	513973.678557	47.627956
3503.951191	513964.342073	47.632961
3504.079782	513956.330340	47.637965
3504.193162	513931.174840	47.642970
3503.805248	513938.620651	47.647975
3503.772711	513924.413193	47.652980
3504.246610	513926.462607	47.657985
3504.034482	513909.349957	47.662989
3504.174473	513893.243789	47.667994
3504.265246	513884.934527	47.672999
3503.807804	513892.340769	47.678004
3504.092489	513873.783930	47.683009
3503.670051	513860.750780	47.688013
3503.948563	513844.268619	47.693018
3503.557447	513849.287186	47.698023
3504.103405	513851.021745	47.703028
3504.102340	513841.664820	47.708033
3503.645705	513820.949041	47.713037
3503.734994	513805.710647	47.718042
3503.582550	513798.805419	47.723047
3503.688225	513806.527326	47.728052
3503.889183	513796.784391	47.733057
3503.782239	513793.412506	47.738061
3503.857886	513793.147665	47.743066
3503.660181	513799.754207	47.748071
3504.082526	513792.252336	47.753076
3503.885939	513762.037086	47.758081
3503.569073	513756.776363	47.763085
3503.755888	513750.424444	47.768090
3504.065916	513755.180479	47.773095
3503.768468	513749.613210	47.778100
3503.854807	513756.882982	47.783105
3503.550205	513748.231511	47.788109
3503.690497	513731.669929	47.793114
3503.450905	513715.977643	47.798119
3503.653409	513705.475720	47.803124
3503.892459	513704.476940	47.808129
3503.751938	513707.989137	47.813133
3503.654049	513701.024667	47.818138
3503.631957	513720.046007	47.823143
3503.601005	513712.615748	47.828148
3503.618200	513707.555106	47.833153
3503.509283	513725.527996	47.838157
3503.618690	513706.391725	47.843162
3503.757703	513713.602611	47.848167
3503.651808	513694.399198	47.853172
3503.977867	513682.461510	47.858177
3503.406278	513676.735229	47.863181
3503.871844	513678.431934	47.868186
3503.976527	513667.085599	47.873191
3503.869671	513669.277417	47.878196
3503.686253	513673.858571	47.883201
3503.599352	513667.651042	47.888205
3503.878019	513659.160232	47.893210
3503.717828	513638.043315	47.898215
3503.537786	513631.496438	47.903220
3503.797113	513614.966506	47.908225
3503.615791	513629.663265	47.913229
3503.980267	513614.583521	47.918234
3503.763817	513628.071923	47.923239
3503.722186	513620.997369	47.928244
3504.037818	513622.009664	47.933249
3503.852171	513617.942068	47.938253
3503.827009	513587.497091	47.943258
3503.842507	513592.603203	47.948263
3503.713549	513593.786930	47.953268
3503.755141	513585.940512	47.958273
3503.276626	513590.467171	47.963277
3503.590062	513584.044596	47.968282
3503.744196	513586.700971	47.973287
3503.875965	513570.393475	47.978292
3503.862416	513560.330250	47.983297
3503.435006	513545.021549	47.988301
3503.721604	513538.754938	47.993306
3503.723607	513543.104501	47.998311
3503.828139	513542.430452	48.003316
3503.958330	513539.273934	48.008321
3503.714469	513547.455845	48.013325
3504.139929	513538.081915	48.018330
3503.662906	513516.610285	48.023335
3503.678683	513503.254694	48.028340
3503.832799	513504.039626	48.033345
3503.434788	513505.265885	48.038349
3503.559760	513496.091166	48.043354
3503.709756	513496.472109	48.048359
3503.729587	513507.040201	48.053364
3504.220857	513488.146806	48.058369
3503.861776	513490.833734	48.063373
3503.636623	513462.443341	48.068378
3503.829324	513462.362314	48.073383
3503.812709	513464.539895	48.078388
3504.004288	513448.121668	48.083393
3503.567908	513461.594384	48.088397
3503.970483	513454.297809	48.093402
3503.615623	513459.765981	48.098407
3503.814991	513445.470884	48.103412
3503.839497	513428.067442	48.108417
3503.725888	513429.097014	48.113421
3503.810848	513412.189802	48.118426
3503.831062	513422.808466	48.123431
3503.737552	513416.804211	48.128436
3503.594450	513409.037482	48.133441
3503.562822	513425.733969	48.138445
3503.963500	513406.753641	48.143450
3503.680362	513395.013199	48.148455
3503.494533	513380.778931	48.153460
3503.701777	513374.170740	48.158465
3503.445866	513367.382849	48.163469
3503.527026	513377.435525	48.168474
3503.693196	513374.829674	48.173479
3503.846782	513370.404917	48.178484
3503.746614	513366.576652	48.183489
3503.573521	513379.249113	48.188493
3503.258204	513364.681236	48.193498
3503.822172	513375.517468	48.198503
3503.457863	513368.089167	48.203508
3503.875450	513369.692327	48.208513
3503.768369	513361.464660	48.213517
3503.726741	513345.841899	48.218522
3503.498495	513327.517274	48.223527
3503.435936	513335.063666	48.228532
3503.609172	513327.449222	48.233537
3503.555237	513337.118631	48.238541
3503.782216	513329.091050	48.243546
3503.840154	513324.327336	48.248551
3503.640397	513334.677341	48.253556
3503.737769	513335.673571	48.258561
3503.601015	513335.695198	48.263565
3503.724075	513340.177420	48.268570
3503.592795	513307.219686	48.273575
3503.634995	513297.501556	48.278580
3503.555821	513287.499121	48.283585
3503.718364	513295.768660	48.288589
3503.751554	513281.347949	48.293594
3503.437655	513287.416669	48.298599
3503.608532	513287.490833	48.303604
3503.699068	513286.818986	48.308609
3503.466602	513290.396384	48.313613
3503.808324	513287.004062	48.318618
3503.657931	513295.980612	48.323623
3503.487333	513290.949527	48.328628
3504.007232	513287.225559	48.333633
3503.633881	513280.203293	48.338637
3503.894709	513261.396648	48.343642
3503.551864	513252.143997	48.348647
3503.968115	513254.506091	48.353652
3504.172938	513249.668559	48.358657
3504.018542	513246.354645	48.363661
3503.733136	513229.505789	48.368666
3503.908821	513212.482875	48.373671
3503.801184	513196.870410	48.378676
3504.076468	513190.656040	48.383681
3503.693077	513199.163660	48.388685
3503.617248	513205.295942	48.393690
3503.862547	513203.689175	48.398695
3503.773914	513205.170040	48.403700
3503.864323	513166.714257	48.408705
3503.864775	513175.312962	48.413709
3503.603510	513160.179973	48.418714
3503.915687	513168.324763	48.423719
3503.631401	513162.755218	48.428724
3503.852355	513154.677925	48.433729
3503.628540	513162.553368	48.438733
3503.823970	513145.679010	48.443738
3503.806552	513134.199872	48.448743
3503.703131	513126.123255	48.453748
3503.435650	513111.547597	48.458753
3503.816071	513112.499103	48.463757
3503.582660	513115.924942	48.468762
3503.485342	513111.893844	48.473767
3503.603904	513112.431508	48.478772
3503.646873	513115.156109	48.483777
3503.722895	513113.373764	48.488781
3503.757278	513120.247375	48.493786
3503.587944	513119.313109	48.498791
3503.584437	513118.403214	48.503796
3503.591903	513109.095115	48.508801
3503.649465	513093.507024	48.513805
3503.695153	513075.341152	48.518810
3503.576200	513080.670996	48.523815
3503.659242	513082.175318	48.528820
3503.933534	513066.704691	48.533825
3503.561778	513080.369821	48.538829
3503.614848	513080.766094	48.543834
3503.901428	513073.892339	48.548839
3503.695904	513082.220160	48.553844
3504.172696	513065.958806	48.558849
3503.806311	513055.344073	48.563853
3503.835294	513034.955219	48.568858
3503.586032	513036.764976	48.573863
3503.387978	513044.535240	48.578868
3503.999227	513039.431083	48.583873
3503.681329	513037.002854	48.588877
3503.548396	513041.677362	48.593882
3503.878550	513033.026356	48.598887
3503.493082	513034.554153	48.603892
3503.447367	513015.947432	48.608897
3503.412589	513020.960501	48.613901
3503.870416	513010.013140	48.618906
3503.673375	513009.285573	48.623911
3503.399188	512998.858557	48.628916
3503.617770	512991.843773	48.633921
3503.891831	512992.862678	48.638925
3503.867104	512997.520095	48.643930
3503.896553	512998.577662	48.648935
3503.434907	512988.938992	48.653940
3503.517171	512988.774256	48.658945
3503.560474	513002.070356	48.663949
3503.929258	512982.993432	48.668954
3503.679049	512982.122522	48.673959
3503.403524	512957.583437	48.678964
3503.679099	512949.345669	48.683969
3503.542690	512952.958536	48.688973
3503.411074	512940.131612	48.693978
3503.547882	512949.417023	48.698983
3503.442683	512954.795314	48.703988
3503.558372	512946.076999	48.708993
3503.522365	512950.736212	48.713997
3503.815603	512940.421800	48.719002
3503.549602	512951.136582	48.724007
3503.445142	512962.989201	48.729012
3503.521182	512952.000984	48.734017
3503.537605	512952.858287	48.739021
3503.190949	512952.862508	48.744026
3503.626333	512955.980345	48.749031
3503.653731	512952.232985	48.754036
3503.865088	512948.254222	48.759041
3503.489003	512960.250939	48.764045
3503.869986	512942.942397	48.769050
3503.745063	512953.837206	48.774055
3503.575143	512939.549469	48.779060
3503.795768	512913.616776	48.784065
3503.737908	512926.069036	48.789069
3503.250247	512921.037373	48.794074
3503.388241	512918.081833	48.799079
3503.369111	512921.220935	48.804084
3503.783693	512916.299572	48.809089
3503.729551	512927.233791	48.814093
3503.652753	512922.491260	48.819098
3503.779323	512915.642733	48.824103
3503.257732	512927.207236	48.829108
3503.428592	512927.938967	48.834113
3503.259842	512924.222604	48.839117
3503.770838	512917.212152	48.844122
3503.630158	512931.093787	48.849127
3503.409119	512917.674000	48.854132
3503.601449	512924.168654	48.859137
3503.512408	512939.559572	48.864141
3503.613651	512919.816720	48.869146
3503.848721	512915.985946	48.874151
3503.457113	512907.196048	48.879156
3503.906694	512886.588791	48.884161
3503.431669	512885.197011	48.889165
3503.404207	512885.454272	48.894170
3503.809449	512883.923358	48.899175
3503.565874	512892.307868	48.904180
3503.851885	512871.422956	48.909185
3503.793848	512881.295602	48.914189
3503.732262	512882.620474	48.919194
3503.896557	512887.602118	48.924199
3503.398346	512888.743094	48.929204
3503.667734	512874.689357	48.934209
3503.654402	512863.664626	48.939213
3503.692403	512847.017180	48.944218
3503.698947	512844.487059	48.949223
3503.409432	512839.879291	48.954228
3503.874873	512833.533570	48.959233
3503.435087	512837.295577	48.964237
3503.331859	512840.953806	48.969242
3503.566298	512844.406917	48.974247
3503.349344	512839.990007	48.979252
3503.339567	512846.364890	48.984257
3503.403347	512845.090271	48.989261
3503.545367	512839.200328	48.994266
3503.461253	512850.291080	48.999271
3503.556053	512841.576013	49.004276
3504.082437	512828.341510	49.009281
3503.884448	512847.088144	49.014285
3503.715298	512845.243359	49.019290
3503.922344	512842.732129	49.024295
3503.514519	512824.334176	49.029300
3504.009164	512793.046876	49.034305
3503.497651	512806.430823	49.039309
3503.438534	512789.141104	49.044314
3503.548051	512796.104135	49.049319
3503.437060	512801.078734	49.054324
3503.578810	512790.535264	49.059329
3503.107222	512804.823381	49.064333
3503.144472	512789.946370	49.069338
3503.681422	512809.436777	49.074343
3503.382326	512797.192619	49.079348
3503.594240	512801.863270	49.084353
3503.810669	512800.008117	49.089357
3503.767165	512801.785377	49.094362
3503.947612	512794.321300	49.099367
3503.464761	512810.482730	49.104372
3503.739239	512799.159556	49.109377
3503.716185	512805.081314	49.114381
3503.595223	512793.517146	49.119386
3503.928479	512776.367724	49.124391
3503.612661	512772.371080	49.129396
3503.756516	512762.434247	49.134401
3503.837586	512763.129595	49.139405
3503.567380	512770.405566	49.144410
3503.963016	512759.063215	49.149415
3503.822231	512766.773972	49.154420
3504.016030	512747.623276	49.159425
3503.574198	512740.561025	49.164429
3503.638321	512726.741938	49.169434
3503.702511	512714.086223	49.174439
3503.560210	512716.182602	49.179444
3503.577450	512715.168241	49.184449
3503.380763	512729.412971	49.189453
3503.542273	512718.360510	49.194458
3503.722028	512714.791346	49.199463
3503.443501	512723.282629	49.204468
3503.530343	512721.245621	49.209473
3503.764054	512722.321503	49.214477
3503.437855	512714.431647	49.219482
3503.835177	512725.851045	49.224487
3503.353082	512721.880671	49.229492
3503.709588	512724.252284	49.234497
3503.694441	512722.939549	49.239501
3503.604733	512691.238599	49.244506
3503.829377	512690.545532	49.249511
3503.820746	512686.955556	49.254516
3503.917114	512685.675774	49.259521
3503.964525	512682.936841	49.264525
3504.075875	512682.059350	49.269530
3503.857989	512660.697416	49.274535
3503.915903	512646.474585	49.279540
3504.019812	512638.516712	49.284545
3504.030587	512641.600556	49.289549
3503.581142	512633.730142	49.294554
3504.091233	512634.104772	49.299559
3503.745077	512633.350175	49.304564
3503.965768	512606.051271	49.309569
3503.798811	512599.299593	49.314573
3503.648755	512599.222156	49.319578
3503.754053	512594.855412	49.324583
3503.534051	512594.738448	49.329588
3503.789846	512594.950942	49.334593
3503.910371	512595.994140	49.339597
3503.614577	512586.025528	49.344602
3503.678169	512564.467234	49.349607
3503.316565	512565.283141	49.354612
3503.686116	512545.042198	49.359617
3503.918804	512553.048102	49.364621
3503.911158	512548.598032	49.369626
3504.108102	512556.963663	49.374631
3503.856933	512556.598711	49.379636
3504.115634	512530.254750	49.384641
3503.739500	512519.540054	49.389645
3503.709588	512504.521658	49.394650
3504.174717	512505.611560	49.399655
3503.742680	512502.695463	49.404660
3503.945507	512501.196509	49.409665
3504.212781	512473.890029	49.414669
3504.083987	512469.762586	49.419674
3503.951549	512464.826388	49.424679
3504.012252	512471.696103	49.429684
3504.149055	512436.367476	49.434689
3504.125005	512429.239059	49.439693
3503.889075	512424.774457	49.444698
3504.076511	512423.176762	49.449703
3503.648642	512405.085020	49.454708
3504.086359	512385.996528	49.459713
3504.020377	512372.147133	49.464717
3503.986010	512380.650579	49.469722
3503.986882	512380.701035	49.474727
3503.904672	512379.095373	49.479732
3503.843670	512352.953419	49.484737
3503.582074	512340.854752	49.489741
3503.608722	512338.877797	49.494746
3503.716288	512340.884144	49.499751
3503.650807	512338.618250	49.504756
3503.629052	512340.038036	49.509761
3503.841908	512329.988876	49.514765
3503.631803	512333.866440	49.519770
3503.776748	512329.240445	49.524775
3503.495435	512331.510593	49.529780
3503.328946	512310.443593	49.534785
3503.560246	512305.045189	49.539789
3503.740314	512307.647083	49.544794
3503.866450	512289.113567	49.549799
3503.825670	512291.193951	49.554804
3504.246458	512282.882324	49.559809
3504.277452	512283.180938	49.564813
3503.977654	512270.734174	49.569818
3504.008395	512254.643713	49.574823
3503.835862	512255.075664	49.579828
3504.051231	512252.613616	49.584833
3503.972263	512251.159180	49.589837
3503.751898	512231.972196	49.594842
3503.943331	512210.393246	49.599847
3503.615704	512214.795251	49.604852
3503.576528	512203.369504	49.609857
3503.840993	512201.203192	49.614861
3503.677741	512209.727095	49.619866
3503.509536	512195.691377	49.624871
3503.244541	512209.947339	49.629876
3503.737627	512198.740964	49.634881
3503.865870	512206.763540	49.639885
3503.605846	512208.423333	49.644890
3503.841893	512204.693414	49.649895
3503.261351	512186.271481	49.654900
3503.811397	512161.550167	49.659905
3503.917773	512170.739648	49.664909
3503.765647	512173.798742	49.669914
3503.808217	512166.052677	49.674919
3503.603258	512168.462531	49.679924
3503.880078	512161.185279	49.684929
3503.740724	512159.133372	49.689933
3503.315594	512161.578026	49.694938
3503.761615	512140.666923	49.699943
3503.617275	512129.713005	49.704948
3503.670765	512120.295919	49.709953
3503.584192	512115.807627	49.714957
3503.757093	512121.041058	49.719962
3503.770906	512105.914230	49.724967
3503.167953	512122.398801	49.729972
3503.247898	512115.304400	49.734977
3503.716716	512112.701103	49.739981
3503.633083	512118.632676	49.744986
3503.842465	512112.580081	49.749991
3503.792055	512120.074511	49.754996
3503.624364	512125.513526	49.760001
3503.655491	512124.345183	49.765005
3503.490328	512124.371299	49.770010
3503.791825	512108.187320	49.775015
3503.518298	512096.444454	49.780020
3503.668169	512072.646193	49.785025
3503.642770	512084.335177	49.790029
3503.922591	512078.524358	49.795034
3503.763895	512078.245947	49.800039
3503.800615	512081.578714	49.805044
3503.936394	512077.864614	49.810049
3503.844217	512089.462982	49.815053
3503.814355	512061.393456	49.820058
3504.122468	512042.780322	49.825063
3503.703263	512046.691002	49.830068
3503.915631	512031.684477	49.835073
3503.913962	512042.863896	49.840077
3503.438852	512050.779574	49.845082
3503.939157	512026.420016	49.850087
3503.296155	512017.821141	49.855092
3503.697066	511999.749722	49.860097
3503.488603	511997.658134	49.865101
3503.630502	511986.254205	49.870106
3503.788114	511982.688388	49.875111
3503.530523	511997.752710	49.880116
3503.871095	511988.189006	49.885121
3503.859587	511992.439934	49.890125
3503.765835	511998.828409	49.895130
3503.907106	511997.237972	49.900135
3503.588164	511982.467135	49.905140
3503.807763	511972.012021	49.910145
3503.715439	511951.236360	49.915149
3503.334292	511951.600122	49.920154
3503.636357	511948.163219	49.925159
3503.467356	511956.536404	49.930164
3503.805234	511941.560546	49.935169
3503.623188	511946.597211	49.940173
3503.459533	511951.934474	49.945178
3503.902671	511944.883765	49.950183
3503.530286	511953.491436	49.955188
3503.765870	511944.450148	49.960193
3503.668697	511944.313764	49.965197
3503.357172	511949.320308	49.970202
3503.928943	511938.202494	49.975207
3503.135917	511929.374363	49.980212
3503.487502	511935.085456	49.985217
3503.955622	511937.338371	49.990221
3503.586622	511921.513116	49.995226
3503.766301	511904.134164	50.000231
3503.597153	511904.818512	50.005236
3503.594692	511906.437624	50.010241
3503.301196	511907.546304	50.015245
3503.383847	511911.225938	50.020250
3503.808650	511899.676066	50.025255
3503.454109	511915.109878	50.030260
3503.519214	511907.714228	50.035265
3503.699924	511908.393862	50.040269
3503.645691	511908.705954	50.045274
3503.812711	511902.912904	50.050279
3503.596793	511911.799374	50.055284
3503.627574	511905.774935	50.060289
3503.576311	511899.055275	50.065293
3503.444921	511884.305293	50.070298
3503.723099	511872.120975	50.075303
3503.760691	511868.118841	50.080308
3503.385716	511863.878405	50.085313
3503.404324	511859.525175	50.090317
3503.472288	511865.837554	50.095322
3503.485972	511858.500594	50.100327
3503.711336	511873.488692	50.105332
3503.504181	511853.591003	50.110337
3503.737573	511865.593328	50.115341
3503.716614	511869.289347	50.120346
3503.989642	511863.327774	50.125351
3503.703960	511867.470314	50.130356
3503.529632	511869.673028	50.135361
3503.638282	511868.138321	50.140365
3503.897155	511861.470796	50.145370
3503.515060	511830.674392	50.150375
3503.331645	511837.785289	50.155380
3503.778844	511817.935887	50.160385
3503.682835	511820.783834	50.165389
3503.478548	511828.505053	50.170394
3503.917054	511816.447109	50.175399
3503.581257	511823.733852	50.180404
3503.615101	511825.094309	50.185409
3503.626819	511825.800657	50.190413
3503.396095	511820.728051	50.195418
3503.624080	511818.769797	50.200423
3503.309663	511821.197000	50.205428
3503.795015	511829.618576	50.210433
3503.539584	511824.954556	50.215437
3503.335675	511836.216661	50.220442
3503.468972	511830.884182	50.225447
3503.481207	511830.174070	50.230452
3503.597630	511832.684928	50.235457
3503.486961	511830.527277	50.240461
3503.670596	511831.206453	50.245466
3503.646214	511801.162815	50.250471
3503.302966	511797.271444	50.255476
3503.556822	511773.203403	50.260481
3503.666060	511790.081579	50.265485
3503.641071	511789.124423	50.270490
3503.651254	511781.079791	50.275495
3503.411945	511782.685766	50.280500
3503.357397	511787.904665	50.285505
3503.448164	511795.427509	50.290509
3503.483594	511782.674474	50.295514
3503.649706	511781.737698	50.300519
3503.314925	511795.398016	50.305524
3503.672015	511785.173981	50.310529
3503.591644	511783.315046	50.315533
3503.513418	511789.599975	50.320538
3503.609602	511776.887919	50.325543
3503.494804	511797.443628	50.330548
3503.543888	511786.155405	50.335553
3503.631225	511786.849803	50.340557
3503.307794	511793.122903	50.345562
3503.674990	511789.422748	50.350567
3503.741592	511796.848240	50.355572
3504.033252	511788.607368	50.360577
3503.912749	511774.766101	50.365581
3503.970843	511766.916231	50.370586
3503.674426	511760.741117	50.375591
3503.640475	511753.108129	50.380596
3503.769760	511746.258701	50.385601
3503.522464	511749.838765	50.390605
3503.328613	511755.990226	50.395610
3503.663440	511740.255896	50.400615
3503.522733	511764.306122	50.405620
3503.782309	511748.027256	50.410625
3503.775577	511733.965633	50.415629
3503.555036	511725.805687	50.420634
3504.063067	511696.385907	50.425639
3503.921800	511707.992293	50.430644
3503.695524	511707.572801	50.435649
3503.889949	511699.499010	50.440653
3503.439844	511701.492408	50.445658
3503.808693	511708.263142	50.450663
3503.401642	511692.494271	50.455668
3503.763345	511696.483943	50.460673
3503.869129	511668.594668	50.465677
3503.614596	511669.848961	50.470682
3503.436213	511667.752578	50.475687
3503.526706	511665.563111	50.480692
3503.652277	511665.290347	50.485697
3503.536578	511662.526444	50.490701
3503.468041	511665.521831	50.495706
3503.737296	511654.198720	50.500711
3503.764330	511667.144342	50.505716
3503.908169	511657.864476	50.510721
3503.520675	511664.046577	50.515725
3503.185616	511646.799306	50.520730
3503.493062	511619.383932	50.525735
3503.556109	511620.486861	50.530740
3503.500018	511590.700791	50.535745
3503.364432	511546.864381	50.540749
3503.437657	511485.390933	50.545754
3503.498767	511422.654523	50.550759
3502.824195	511351.130958	50.555764
3502.997603	511260.654828	50.560769
3502.922014	511167.688226	50.565773
3502.694679	511072.671025	50.570778
3502.443940	510962.480731	50.575783
3502.417439	510852.102518	50.580788
3502.289442	510711.639618	50.585793
3502.259497	510581.480160	50.590797
3502.219946	510442.771670	50.595802
3501.953071	510278.550263	50.600807
3501.524767	510121.890711	50.605812
3501.368550	509949.503651	50.610817
3501.493288	509764.726221	50.615821
3500.904599	509577.024062	50.620826
3501.180086	509372.386632	50.625831
3500.459731	509170.889144	50.630836
3500.212119	508955.654329	50.635841
3499.969009	508748.157007	50.640845
3499.668260	508526.095009	50.645850
3499.637767	508272.719439	50.650855
3498.920840	508051.172459	50.655860
3498.730204	507806.264903	50.660865
3498.779637	507552.360155	50.665869
3498.015841	507288.865333	50.670874
3497.749132	507002.265300	50.675879
3497.209453	506745.405881	50.680884
3497.137762	506462.055093	50.685889
3496.668318	506184.227530	50.690893
3496.105497	505890.925945	50.695898
3495.990669	505595.726890	50.700903
3495.401443	505306.366699	50.705908
3495.206062	505002.213403	50.710913
3494.763694	504686.859342	50.715917
3494.240575	504372.979965	50.720922
3493.888468	504055.677219	50.725927
3493.564765	503736.795382	50.730932
3492.650638	503389.457253	50.735937
3492.467350	503073.324734	50.740941
3491.806687	502749.214777	50.745946
3491.402866	502403.649199	50.750951
3490.840665	502058.203133	50.755956
3490.746071	501717.181109	50.760961
3490.318842	501358.995855	50.765965
3489.851735	500998.582562	50.770970
3489.275737	500638.938450	50.775975
3488.721452	500279.941694	50.780980
3487.943844	499899.864652	50.785985
3487.450498	499535.882600	50.790989
3486.739605	499165.802321	50.795994
3486.690880	498787.256991	50.800999
3486.132027	498425.085197	50.806004
3485.396567	498041.620987	50.811009
3484.920239	497651.880677	50.816013
3484.441313	497250.893171	50.821018
3484.262675	496851.823822	50.826023
3483.354527	496465.518334	50.831028
3483.073828	496063.207522	50.836033
3482.227316	495660.420318	50.841037
3481.835009	495264.590358	50.846042
3481.338858	494840.058918	50.851047
3480.746078	494439.179418	50.856052
3479.884996	494024.965668	50.861057
3479.662495	493602.843521	50.866061
3479.196297	493196.549382	50.871066
3478.311807	492763.726713	50.876071
3477.671501	492351.364775	50.881076
3476.910437	491917.591284	50.886081
3476.412793	491497.591549	50.891085
3475.549151	491085.743239	50.896090
3475.105245	490649.509783	50.901095
3474.626412	490227.604596	50.906100
3473.980589	489805.615004	50.911105
3473.267765	489369.039690	50.916109
3472.571532	488941.821838	50.921114
3472.432720	488507.161787	50.926119
3471.213324	488073.472978	50.931124
3470.823705	487637.920841	50.936129
3470.375483	487199.733927	50.941133
3469.578677	486764.226104	50.946138
3469.002492	486330.750371	50.951143
3467.974506	485895.005940	50.956148
3467.463309	485455.775719	50.961153
3467.202404	485015.685298	50.966157
3466.256494	484576.149028	50.971162
3465.644894	484128.038545	50.976167
3464.608085	483694.018737	50.981172
3464.014439	483242.135729	50.986177
3463.659845	482801.350935	50.991181
3462.746665	482362.265786	50.996186
3462.028935	481916.198253	51.001191
3461.419528	481484.746890	51.006196
3460.767612	481040.523708	51.011201
3460.205609	480600.532667	51.016205
3459.280241	480158.460935	51.021210
3458.925114	479714.414176	51.026215
3458.374295	479273.631564	51.031220
3457.571437	478826.595088	51.036225
3456.929771	478377.647964	51.041229
3456.092355	477930.799451	51.046234
3455.700432	477486.860579	51.051239
3455.051955	477036.870663	51.056244
3453.942983	476585.220215	51.061249
3453.563035	476141.502960	51.066253
3452.722225	475699.217226	51.071258
3452.347316	475247.876786	51.076263
3451.305898	474802.105759	51.081268
3450.470729	474355.734723	51.086273
3450.033361	473919.023210	51.091277
3449.158164	473473.855613	51.096282
3448.841037	473027.677610	51.101287
3447.811530	472586.063368	51.106292
3446.794233	472144.944581	51.111297
3446.524598	471705.269618	51.116301
3445.494667	471265.604043	51.121306
3445.180488	470813.091101	51.126311
3444.412422	470389.132020	51.131316
3443.702888	469941.022454	51.136321
3443.068433	469499.989286	51.141325
3442.170199	469061.371388	51.146330
3441.500091	468609.221484	51.151335
3440.811273	468183.531675	51.156340
3439.972409	467741.023205	51.161345
3439.630530	467306.488922	51.166349
3438.721598	466875.280488	51.171354
3438.258041	466425.231171	51.176359
3437.370949	465992.581424	51.181364
3436.466494	465553.992592	51.186369
3436.048933	465114.607767	51.191373
3435.339806	464685.605065	51.196378
3434.652420	464243.912198	51.201383
3433.862185	463815.107656	51.206388
3433.103607	463388.318093	51.211393
3432.420927	462940.156845	51.216397
3431.672790	462505.791490	51.221402
3431.157450	462069.757617	51.226407
3430.102479	461643.639648	51.231412
3429.673672	461215.030482	51.236417
3429.315436	460782.597659	51.241421
3428.473693	460356.014936	51.246426
3427.248395	459917.311105	51.251431
3426.837649	459487.295581	51.256436
3425.917480	459058.772446	51.261441
3425.341408	458633.230077	51.266445
3424.193290	458214.262910	51.271450
3423.912660	457780.033862	51.276455
3423.032874	457369.429004	51.281460
3422.476134	456943.090100	51.286465
3421.983052	456520.233346	51.291469
3421.013205	456094.958109	51.296474
3420.100852	455668.600305	51.301479
3419.286903	455249.372204	51.306484
3418.799663	454832.874994	51.311489
3418.405172	454417.522315	51.316493
3417.499630	454009.345825	51.321498
3417.309898	453581.007696	51.326503
3416.571636	453157.821985	51.331508
3415.402806	452740.683644	51.336513
3414.725973	452323.104690	51.341517
3413.911452	451911.780966	51.346522
3413.303670	451493.313332	51.351527
3412.645039	451074.744614	51.356532
3411.959551	450657.035155	51.361537
3411.716072	450243.764487	51.366541
3410.523948	449834.188577	51.371546
3409.927651	449401.523190	51.376551
3409.424882	448994.107019	51.381556
3408.386118	448589.356602	51.386561
3407.703983	448164.090969	51.391565
3407.035992	447759.775033	51.396570
3406.324021	447344.953682	51.401575
3405.482259	446940.245086	51.406580
3404.877848	446534.476956	51.411585
3404.373951	446123.762884	51.416589
3403.581033	445715.269809	51.421594
3402.896202	445305.534483	51.426599
3402.255437	444897.967633	51.431604
3401.630018	444501.304094	51.436609
3401.085373	444093.556032	51.441613
3400.030512	443678.877021	51.446618
3399.452286	443268.277753	51.451623
3398.743938	442868.300942	51.456628
3398.023911	442462.634104	51.461633
3397.605721	442051.125874	51.466637
3396.625456	441659.750829	51.471642
3396.075275	441249.062072	51.476647
3395.383536	440850.521479	51.481652
3394.751527	440436.735348	51.486657
3394.278292	440037.842367	51.491661
3393.502305	439633.558705	51.496666
3392.631388	439222.632825	51.501671
3391.912555	438824.088986	51.506676
3390.939257	438421.618937	51.511681
3390.829631	438015.604183	51.516685
3389.826893	437611.602542	51.521690
3389.358612	437212.206245	51.526695
3388.483856	436808.425216	51.531700
3387.535425	436411.960715	51.536705
3387.035095	436008.666107	51.541709
3386.292287	435611.115582	51.546714
3385.710621	435217.265345	51.551719
3384.833328	434822.440182	51.556724
3383.931268	434430.380160	51.561729
3383.616625	434027.760872	51.566733
3382.571711	433648.583696	51.571738
3382.361842	433247.814358	51.576743
3381.487166	432862.352678	51.581748
3380.656830	432460.932828	51.586753
3379.932517	432072.744111	51.591757
3379.049280	431680.689785	51.596762
3378.444431	431289.169508	51.601767
3377.690160	430904.675209	51.606772
3377.054728	430514.620838	51.611777
3376.445283	430128.822545	51.616781
3375.513345	429754.344207	51.621786
3374.937615	429364.263220	51.626791
3374.388181	428980.495416	51.631796
3373.536185	428597.455510	51.636801
3372.953663	428210.101097	51.641805
3371.957728	427825.803021	51.646810
3371.573232	427450.722874	51.651815
3370.923214	427065.140103	51.656820
3369.922994	426684.838772	51.661825
3369.780155	426298.275855	51.666829
3369.153228	425925.142753	51.671834
3368.368011	425529.502006	51.676839
3367.528397	425155.604540	51.681844
3366.495419	424775.052766	51.686849
3366.019885	424382.444810	51.691853
3365.379670	424008.626963	51.696858
3364.596283	423632.388297	51.701863
3363.996250	423250.171957	51.706868
3363.410003	422876.152260	51.711873
3362.783359	422490.652942	51.716877
3361.737215	422118.753070	51.721882
3360.766401	421737.031506	51.726887
3360.433463	421371.790839	51.731892
3359.841486	421002.699873	51.736897
3359.374370	420622.686820	51.741901
3358.153207	420246.115522	51.746906
3357.784544	419865.492329	51.751911
3356.845511	419502.685440	51.756916
3356.510945	419126.035082	51.761921
3356.206685	418751.508800	51.766925
3355.096948	418384.421267	51.771930
3354.315167	418004.625758	51.776935
3353.812326	417621.275209	51.781940
3353.050005	417257.522377	51.786945
3352.363231	416881.710836	51.791949
3351.424382	416518.078119	51.796954
3350.775184	416144.766120	51.801959
3350.204259	415772.326115	51.806964
3349.190963	415408.386253	51.811969
3348.854830	415038.592751	51.816973
3348.142882	414676.323699	51.821978
3347.138922	414309.649977	51.826983
3346.594558	413941.247445	51.831988
3345.833975	413579.378964	51.836993
3345.291406	413212.694728	51.841997
3344.494082	412854.685210	51.847002
3344.106423	412482.097919	51.852007
3343.606099	412129.165274	51.857012
3342.439922	411758.699324	51.862017
3342.165158	411390.145999	51.867021
3341.158110	411030.775432	51.872026
3340.738783	410667.013181	51.877031
3340.049312	410300.494014	51.882036
3339.562435	409936.072882	51.887041
3338.384716	409574.323161	51.892045
3337.442545	409220.994030	51.897050
3337.009646	408859.499138	51.902055
3336.521036	408493.307423	51.907060
3335.267233	408134.398734	51.912065
3335.134679	407779.832043	51.917069
3334.239310	407421.366548	51.922074
3333.732547	407072.594283	51.927079
3333.031505	406713.581515	51.932084
3332.113463	406352.845292	51.937089
3331.911926	405992.220279	51.942093
3330.903019	405644.680359	51.947098
3330.382455	405278.302902	51.952103
3329.760601	404921.315477	51.957108
3328.807646	404571.187766	51.962113
3328.260179	404203.251594	51.967117
3327.462569	403856.649593	51.972122
3326.885046	403503.934395	51.977127
3326.262152	403149.824503	51.982132
3325.504981	402797.587344	51.987137
3324.964209	402438.500167	51.992141
3324.390031	402082.006840	51.997146
3323.721792	401721.432102	52.002151
3323.107311	401358.404641	52.007156
3322.189466	401013.951244	52.012161
3321.749097	400642.423764	52.017165
3321.146794	400285.609927	52.022170
3320.126661	399925.553708	52.027175
3319.423548	399566.053438	52.032180
3318.365930	399211.638436	52.037185
3318.287889	398859.860906	52.042189
3317.548812	398513.802096	52.047194
3316.741898	398157.429504	52.052199
3316.274212	397805.854847	52.057204
3315.291292	397457.738983	52.062209
3314.769470	397096.581489	52.067213
3314.091423	396751.613137	52.072218
3313.470166	396399.590286	52.077223
3312.544747	396045.272967	52.082228
3312.017984	395687.838128	52.087233
3311.485325	395333.654570	52.092237
3310.402384	394983.622050	52.097242
3309.927211	394633.972835	52.102247
3309.427686	394284.578108	52.107252
3308.492977	393943.765682	52.112257
3308.087044	393592.213439	52.117261
3307.468502	393249.411841	52.122266
3306.386264	392888.272583	52.127271
3305.854481	392550.509840	52.132276
3305.110015	392203.293784	52.137281
3304.633375	391845.175160	52.142285
3303.795289	391502.721489	52.147290
3303.178115	391158.525966	52.152295
3302.755077	390812.084258	52.157300
3301.895594	390466.064129	52.162305
3301.212964	390114.291583	52.167309
3300.336589	389771.140535	52.172314
3299.786843	389422.747321	52.177319
3299.091476	389078.925259	52.182324
3298.617361	388725.249736	52.187329
3297.949488	388384.010268	52.192333
3297.315374	388032.692589	52.197338
3296.742972	387680.751429	52.202343
3295.873778	387337.525007	52.207348
3295.089813	386994.688713	52.212353
3294.439887	386646.513252	52.217357
3293.694486	386311.598359	52.222362
3293.031459	385956.755837	52.227367
3292.315463	385622.160564	52.232372
3291.438425	385276.983293	52.237377
3291.298877	384926.905209	52.242381
3290.063567	384595.815869	52.247386
3289.704333	384247.571689	52.252391
3289.233182	383904.021294	52.257396
3288.365682	383565.286103	52.262401
3287.405064	383212.244541	52.267405
3287.173462	382876.581510	52.272410
3286.391620	382533.169420	52.277415
3286.446935	382190.461068	52.282420
3284.978968	381839.267167	52.287425
3284.631478	381489.062712	52.292429
3283.696001	381146.628829	52.297434
3283.065792	380799.031507	52.302439
3281.990213	380454.121135	52.307444
3281.618214	380118.964686	52.312449
3280.817930	379773.877524	52.317453
3280.115094	379439.072726	52.322458
3279.653703	379095.350248	52.327463
3278.531928	378764.904337	52.332468
3277.964113	378420.734939	52.337473
3277.681391	378077.305921	52.342477
3276.463938	377745.315028	52.347482
3276.211909	377402.765525	52.352487
3275.577540	377066.607036	52.357492
3274.768868	376729.888253	52.362497
3274.040256	376393.153967	52.367501
3273.149751	376063.590078	52.372506
3272.910843	375723.287936	52.377511
3272.189465	375388.248343	52.382516
3271.610680	375050.029235	52.387521
3271.203525	374703.792880	52.392525
3269.936401	374361.912220	52.397530
3269.599414	374027.487434	52.402535
3268.765091	373695.606059	52.407540
3268.201053	373363.501191	52.412545
3267.649824	373010.099807	52.417549
3266.581799	372679.900726	52.422554
3265.979567	372334.947235	52.427559
3265.442955	372006.159643	52.432564
3264.299931	371676.575022	52.437569
3264.049071	371337.383288	52.442573
3263.351401	371013.268795	52.447578
3262.634255	370675.722753	52.452583
3262.290694	370339.310612	52.457588
3261.304571	369997.527837	52.462593
3260.823822	369670.672159	52.467597
3259.756654	369333.603359	52.472602
3259.155114	369004.726488	52.477607
3258.687057	368673.816174	52.482612
3257.744059	368337.483193	52.487617
3257.318258	368005.085524	52.492621
3256.896884	367671.666968	52.497626
3256.045336	367342.689885	52.502631
3255.420972	367013.699849	52.507636
3254.617281	366677.281217	52.512641
3253.682267	366334.596578	52.517645
3253.138957	366006.603937	52.522650
3252.642772	365675.421110	52.527655
3252.013592	365345.554455	52.532660
3250.923411	365009.397562	52.537665
3250.524751	364675.087903	52.542669
3249.828125	364360.287066	52.547674
3248.845333	364024.385756	52.552679
3248.501475	363687.261383	52.557684
3247.606265	363366.454948	52.562689
3246.938973	363031.870426	52.567693
3245.712014	362711.061017	52.572698
3245.761075	362389.284208	52.577703
3245.058226	362060.601404	52.582708
3244.372747	361740.971881	52.587713
3243.917909	361404.688139	52.592717
3243.042135	361078.493963	52.597722
3242.488727	360758.327969	52.602727
3241.966566	360431.869836	52.607732
3240.978799	360097.315060	52.612737
3240.529370	359754.759126	52.617741
3239.796451	359445.808884	52.622746
3239.221581	359115.253302	52.627751
3238.499090	358783.573725	52.632756
3237.628322	358472.603358	52.637761
3237.082102	358140.967852	52.642765
3236.351193	357813.227235	52.647770
3235.723003	357489.616046	52.652775
3234.925908	357161.143590	52.657780
3233.921497	356831.709301	52.662785
3233.483801	356511.217052	52.667789
3232.525090	356201.594984	52.672794
3232.033052	355875.050701	52.677799
3231.630426	355558.898392	52.682804
3230.646019	355234.565478	52.687809
3230.577743	354908.126042	52.692813
3229.924230	354574.956892	52.697818
3229.036464	354262.079764	52.702823
3228.187539	353934.561512	52.707828
3227.612163	353615.625108	52.712833
3227.375078	353285.461050	52.717837
3226.559486	352963.657432	52.722842
3225.613937	352635.459123	52.727847
3225.017338	352301.350142	52.732852
3224.367539	351985.978491	52.737857
3223.443638	351661.002795	52.742861
3222.756091	351339.703429	52.747866
3222.078439	351017.942456	52.752871
3221.634117	350696.855245	52.757876
3221.075998	350375.198755	52.762881
3220.305606	350048.127479	52.767885
3219.437839	349737.281820	52.772890
3218.523098	349414.912517	52.777895
3218.172939	349083.136878	52.782900
3217.409418	348774.101729	52.787905
3216.836607	348453.912400	52.792909
3215.998430	348136.791937	52.797914
3215.135809	347816.313904	52.802919
3214.900454	347497.490978	52.807924
3213.910307	347184.639609	52.812929
3213.482850	346853.219217	52.817933
3212.760639	346552.360829	52.822938
3212.149126	346229.619690	52.827943
3211.345539	345911.921272	52.832948
3210.737880	345597.244423	52.837953
3210.010023	345277.825184	52.842957
3209.162579	344964.735445	52.847962
3208.587908	344649.971865	52.852967
3207.986537	344335.898050	52.857972
3207.483158	344022.341571	52.862977
3206.877447	343692.127535	52.867981
3205.915229	343385.690897	52.872986
3205.285246	343065.124156	52.877991
3204.826971	342752.062901	52.882996
3203.811195	342435.270097	52.888001
3203.296564	342121.756303	52.893005
3202.753677	341813.183500	52.898010
3201.849058	341484.557316	52.903015
3201.305829	341167.046771	52.908020
3200.384561	340863.034501	52.913025
3200.127197	340539.137261	52.918029
3199.293900	340227.471485	52.923034
3198.700124	339916.504455	52.928039
3198.326493	339597.711743	52.933044
3197.267019	339286.000696	52.938049
3196.820502	338966.554484	52.943053
3196.152780	338659.080358	52.948058
3195.291876	338331.856183	52.953063
3194.592989	338014.176125	52.958068
3193.706280	337706.502976	52.963073
3193.279182	337384.805687	52.968077
3192.268367	337088.451773	52.973082
3191.431530	336783.515649	52.978087
3191.075624	336468.217599	52.983092
3190.393486	336163.712351	52.988097
3189.949771	335852.701976	52.993101
3189.512861	335541.485421	52.998106
3188.323716	335230.717375	53.003111
3188.404626	334911.931634	53.008116
3187.149466	334598.956362	53.013121
3186.578325	334280.958169	53.018125
3185.742575	333976.976501	53.023130
3184.809362	333666.669981	53.028135
3184.295804	333359.910664	53.033140
3183.533029	333059.630242	53.038145
3183.157972	332741.848537	53.043149
3182.844134	332434.824446	53.048154
3181.568127	332126.398306	53.053159
3181.382053	331811.993911	53.058164
3180.346142	331503.985340	53.063169
3179.736401	331202.883636	53.068173
3179.266242	330889.742159	53.073178
3178.359601	330581.556453	53.078183
3177.892957	330273.197998	53.083188
3177.099858	329965.297242	53.088193
3176.517026	329654.383235	53.093197
3175.826389	329352.191990	53.098202
3175.378776	329040.897602	53.103207
3174.673283	328723.990763	53.108212
3173.815912	328425.157338	53.113217
3173.162540	328113.866227	53.118221
3172.776930	327805.841233	53.123226
3171.655537	327501.266641	53.128231
3171.218150	327183.980023	53.133236
3170.513818	326883.665186	53.138241
3169.909527	326575.669907	53.143245
3169.268594	326265.769714	53.148250
3168.012098	325960.854060	53.153255
3167.567690	325651.709643	53.158260
3166.558765	325355.409009	53.163265
3166.149321	325043.787065	53.168269
3165.661125	324748.623922	53.173274
3164.970863	324446.617300	53.178279
3164.491941	324133.627997	53.183284
3163.724649	323830.969325	53.188289
3163.316135	323526.164986	53.193293
3162.371734	323224.932491	53.198298
3161.600438	322920.794419	53.203303
3161.083326	322606.379620	53.208308
3160.258427	322316.582542	53.213313
3159.776930	321996.176453	53.218317
3159.209993	321706.158274	53.223322
3158.572370	321395.144498	53.228327
3157.687952	321084.499668	53.233332
3156.872531	320789.221735	53.238337
3156.581994	320476.723938	53.243341
3155.470939	320173.164708	53.248346
3154.936307	319870.837272	53.253351
3154.855238	319566.578326	53.258356
3153.613574	319274.163687	53.263361
3153.418961	318962.740356	53.268365
3152.448790	318653.373828	53.273370
3151.733307	318353.132454	53.278375
3151.078981	318034.063627	53.283380
3150.728318	317747.079497	53.288385
3149.909170	317427.881929	53.293389
3149.106990	317131.571651	53.298394
3147.827567	316824.539722	53.303399
3147.704848	316521.576108	53.308404
3146.706491	316222.187613	53.313409
3146.173627	315916.002296	53.318413
3145.368707	315618.211000	53.323418
3145.092153	315314.886078	53.328423
3144.125254	315025.292354	53.333428
3143.285942	314723.480646	53.338433
3142.853430	314418.598987	53.343437
3142.184924	314126.791103	53.348442
3141.332917	313839.824056	53.353447
3141.037626	313527.686396	53.358452
3140.297724	313226.720364	53.363457
3139.934685	312929.538885	53.368461
3139.177817	312631.578588	53.373466
3138.568150	312321.957136	53.378471
3137.455442	312018.678556	53.383476
3136.939429	311733.104137	53.388481
3136.510698	311423.808011	53.393485
3135.525239	311130.285101	53.398490
3134.954458	310832.443265	53.403495
3134.351760	310512.935498	53.408500
3133.306714	310218.248288	53.413505
3132.972002	309922.989561	53.418509
3132.508758	309623.115866	53.423514
3131.712279	309322.173687	53.428519
3131.128779	309022.190163	53.433524
3130.072443	308730.149322	53.438529
3129.658470	308419.365857	53.443533
3128.916256	308131.501024	53.448538
3128.120548	307835.113214	53.453543
3127.704874	307529.446215	53.458548
3126.968395	307237.962354	53.463553
3126.000417	306931.973848	53.468557
3125.693733	306646.659573	53.473562
3125.152143	306342.537534	53.478567
3124.478605	306030.159427	53.483572
3123.337514	305737.946749	53.488577
3122.831170	305441.634905	53.493581
3122.195978	305148.143995	53.498586
3121.693875	304848.570580	53.503591
3120.877008	304558.468588	53.508596
3120.391339	304261.132254	53.513601
3119.744590	303948.592267	53.518605
3118.679404	303656.261227	53.523610
3117.931037	303360.186902	53.528615
3117.501071	303069.944195	53.533620
3116.706097	302782.050598	53.538625
3116.099827	302486.435843	53.543629
3115.204239	302195.195502	53.548634
3114.698648	301904.122070	53.553639
3114.240968	301603.541625	53.558644
3113.093430	301323.162570	53.563649
3112.578581	301020.272600	53.568653
3111.940844	300738.945958	53.573658
3111.250092	300445.225101	53.578663
3110.650130	300159.664038	53.583668
3109.888374	299877.031242	53.588673
3109.604958	299579.271580	53.593677
3108.765944	299290.079647	53.598682
3107.970982	298993.444006	53.603687
3107.498674	298694.897721	53.608692
3106.897868	298410.021366	53.613697
3106.089086	298110.381310	53.618701
3105.304145	297823.826863	53.623706
3104.858881	297525.325219	53.628711
3103.937296	297238.307584	53.633716
3103.091637	296957.364055	53.638721
3102.820428	296656.286751	53.643725
3101.977079	296372.489676	53.648730
3101.354874	296088.555311	53.653735
3100.668809	295791.005782	53.658740
3100.020687	295514.816640	53.663745
3099.443869	295220.788871	53.668749
3098.596977	294927.898494	53.673754
3097.580169	294637.657698	53.678759
3097.264699	294345.650135	53.683764
3096.310021	294071.035562	53.688769
3095.884803	293778.815372	53.693773
3095.205929	293491.244505	53.698778
3094.525836	293213.096359	53.703783
3093.834208	292919.007124	53.708788
3093.161256	292637.622774	53.713793
3092.459295	292357.312299	53.718797
3091.996074	292069.094261	53.723802
3091.604838	291784.073381	53.728807
3090.815386	291495.702533	53.733812
3089.582970	291208.725757	53.738817
3089.192046	290915.681534	53.743821
3088.667741	290631.750012	53.748826
3087.810856	290359.815124	53.753831
3087.386857	290074.644670	53.758836
3086.509191	289791.328443	53.763841
3085.670744	289497.793162	53.768845
3085.291768	289214.422883	53.773850
3084.549812	288930.473069	53.778855
3084.080981	288641.360726	53.783860
3083.268415	288360.987019	53.788865
3082.562461	288071.071207	53.793869
3082.367232	287777.967215	53.798874
3081.327384	287500.812170	53.803879
3080.494578	287201.950933	53.808884
3079.945186	286928.359688	53.813889
3079.034364	286643.670458	53.818893
3078.928514	286362.724727	53.823898
3077.894700	286079.633512	53.828903
3077.686614	285789.636903	53.833908
3076.338412	285504.914107	53.838913
3075.669793	285217.154720	53.843917
3075.283166	284927.160237	53.848922
3074.467443	284654.831899	53.853927
3074.238938	284370.567779	53.858932
3073.320812	284083.152689	53.863937
3072.743686	283787.329895	53.868941
3071.815759	283511.631327	53.873946
3070.971184	283230.723897	53.878951
3070.570060	282941.290685	53.883956
3069.661279	282671.293475	53.888961
3069.229086	282391.109817	53.893965
3068.805492	282102.316392	53.898970
3067.888088	281829.645956	53.903975
3067.075589	281539.283825	53.908980
3066.598728	281258.699180	53.913985
3066.315869	280962.879148	53.918989
3065.198787	280686.343157	53.923994
3064.392821	280408.815488	53.928999
3064.129561	280111.056395	53.934004
3063.206964	279847.580005	53.939009
3062.136868	279549.082469	53.944013
3061.530608	279262.201377	53.949018
3060.890832	278992.058194	53.954023
3060.405530	278704.139051	53.959028
3059.696327	278431.383463	53.964033
3058.868577	278157.296746	53.969037
3058.259578	277875.229215	53.974042
3057.520273	277595.143310	53.979047
3057.030178	277315.145248	53.984052
3056.516181	277048.037917	53.989057
3056.064330	276770.631483	53.994061
3055.137895	276494.166048	53.999066
3054.442438	276215.142652	54.004071
3054.033983	275931.896988	54.009076
3052.971465	275652.957103	54.014081
3052.714986	275373.991499	54.019085
3052.122772	275097.447581	54.024090
3050.834265	274814.188330	54.029095
3050.348041	274530.903970	54.034100
3049.491164	274268.282207	54.039105
3048.920361	273988.958845	54.044109
3048.252011	273708.020959	54.049114
3047.321512	273440.342677	54.054119
3046.912726	273164.584769	54.059124
3046.470228	272897.669754	54.064129
3045.651726	272618.563992	54.069133
3044.868507	272351.575632	54.074138
3044.235352	272084.181535	54.079143
3043.791264	271795.109448	54.084148
3043.019828	271525.419717	54.089153
3042.260546	271261.280221	54.094157
3041.964032	270983.773058	54.099162
3041.113199	270701.387375	54.104167
3040.561468	270430.440648	54.109172
3039.752090	270155.867338	54.114177
3039.032035	269875.829753	54.119181
3038.347833	269598.842783	54.124186
3037.540096	269338.200643	54.129191
3037.190334	269046.211040	54.134196
3036.172912	268777.376028	54.139201
3035.417994	268510.486096	54.144205
3035.515833	268235.642541	54.149210
3034.328943	267967.038428	54.154215
3033.909855	267688.074673	54.159220
3032.848809	267421.717561	54.164225
3032.248856	267146.373717	54.169229
3031.508014	266867.028338	54.174234
3030.830456	266597.707557	54.179239
3030.358484	266322.624040	54.184244
3029.846895	266059.033088	54.189249
3029.032509	265782.093966	54.194253
3028.239165	265518.038554	54.199258
3027.602468	265251.768247	54.204263
3026.924478	264971.166099	54.209268
3026.075263	264709.845111	54.214273
3025.810852	264436.741882	54.219277
3025.272093	264168.342917	54.224282
3024.221384	263907.258093	54.229287
3023.725185	263629.225853	54.234292
3023.077742	263356.591509	54.239297
3022.142776	263089.096477	54.244301
3021.515876	262816.866781	54.249306
3021.150688	262550.249757	54.254311
3020.488532	262270.309295	54.259316
3019.593967	262007.189199	54.264321
3019.047166	261732.120775	54.269325
3018.430646	261456.172253	54.274330
3017.897803	261192.740901	54.279335
3017.063557	260913.898531	54.284340
3016.314927	260649.050150	54.289345
3015.633048	260379.505376	54.294349
3014.841275	260107.558817	54.299354
3014.256874	259832.778250	54.304359
3013.825228	259572.363017	54.309364
3013.163108	259309.463219	54.314369
3012.391782	259021.062401	54.319373
3011.706866	258756.791511	54.324378
3010.984089	258498.842845	54.329383
3010.390904	258222.282618	54.334388
3009.417736	257956.122661	54.339393
3008.425677	257684.566876	54.344397
3008.226163	257427.937215	54.349402
3007.737575	257159.307493	54.354407
3007.482379	256888.731080	54.359412
3006.334691	256631.793971	54.364417
3005.456223	256360.858432	54.369421
3005.125627	256079.751440	54.374426
3004.098730	255825.750349	54.379431
3003.914122	255549.077706	54.384436
3003.288254	255284.292061	54.389441
3002.526079	255009.876261	54.394445
3002.043374	254736.791811	54.399450
3001.147681	254471.846176	54.404455
3000.436408	254199.104234	54.409460
2999.531245	253936.554711	54.414465
2999.057396	253662.680841	54.419469
2998.381923	253400.630485	54.424474
2997.581677	253134.168990	54.429479
2997.553595	252861.728248	54.434484
2996.357618	252591.153590	54.439489
2995.559850	252324.743788	54.444493
2995.163740	252065.452430	54.449498
2994.353545	251792.678675	54.454503
2993.661603	251510.260198	54.459508
2992.712649	251253.655139	54.464513
2992.281060	250997.095892	54.469517
2991.836570	250722.279513	54.474522
2990.851780	250467.693158	54.479527
2990.065024	250200.418975	54.484532
2989.767895	249931.717989	54.489537
2988.736071	249667.768635	54.494541
2988.263845	249402.865265	54.499546
2987.362636	249148.980773	54.504551
2986.913995	248878.599265	54.509556
2986.043556	248617.809377	54.514561
2985.741088	248358.483453	54.519565
2985.184527	248098.510598	54.524570
2984.040610	247834.964037	54.529575
2983.840318	247575.215801	54.534580
2982.919275	247317.415665	54.539585
2982.021583	247051.972473	54.544589
2981.575018	246783.529757	54.549594
2980.343440	246518.649703	54.554599
2980.060707	246256.548502	54.559604
2979.581445	246009.936649	54.564609
2978.567651	245745.914847	54.569613
2978.204038	245498.623465	54.574618
2977.496985	245232.975192	54.579623
2976.780898	244977.871634	54.584628
2976.004503	244719.009188	54.589633
2975.752413	244461.541235	54.594637
2975.091531	244199.682023	54.599642
2974.123551	243936.878787	54.604647
2974.023218	243666.859334	54.609652
2973.147816	243412.496996	54.614657
2972.053016	243156.005335	54.619661
2971.400477	242884.063160	54.624666
2970.641522	242625.303911	54.629671
2970.068088	242370.870357	54.634676
2969.086498	242114.897629	54.639681
2968.650317	241864.212203	54.644685
2968.208452	241610.803428	54.649690
2967.171933	241359.959411	54.654695
2966.912137	241094.681681	54.659700
2966.287539	240840.310297	54.664705
2965.207919	240589.907594	54.669709
2964.953652	240326.973434	54.674714
2963.805109	240077.066548	54.679719
2963.531636	239818.669266	54.684724
2962.981209	239555.274417	54.689729
2961.956141	239295.978697	54.694733
2961.743581	239036.020175	54.699738
2960.978011	238791.173775	54.704743
2960.593458	238531.625595	54.709748
2959.512989	238269.998258	54.714753
2958.890419	238010.106997	54.719757
2957.963228	237748.100117	54.724762
2957.234104	237494.694825	54.729767
2956.678197	237239.658462	54.734772
2956.335995	236999.128787	54.739777
2955.510827	236743.219513	54.744781
2955.116784	236476.038499	54.749786
2954.234129	236219.681225	54.754791
2953.735258	235968.967685	54.759796
2953.044890	235709.805658	54.764801
2952.283116	235449.229615	54.769805
2952.097868	235190.141688	54.774810
2950.923546	234927.849821	54.779815
2950.685028	234666.327150	54.784820
2949.761769	234411.075686	54.789825
2949.003370	234146.682910	54.794829
2948.502659	233884.312551	54.799834
2947.741910	233631.685506	54.804839
2947.106929	233368.039141	54.809844
2946.479212	233107.880761	54.814849
2945.480654	232851.499371	54.819853
2944.978849	232595.854820	54.824858
2944.297383	232332.116751	54.829863
2943.465258	232075.558285	54.834868
2942.917933	231833.469140	54.839873
2942.173414	231577.101843	54.844877
2941.757257	231314.546782	54.849882
2940.810197	231067.761385	54.854887
2940.177929	230812.040423	54.859892
2939.292626	230551.700618	54.864897
2938.489626	230295.167854	54.869901
2938.183954	230050.422446	54.874906
2937.394625	229802.164107	54.879911
2937.082310	229539.775872	54.884916
2936.295821	229297.934899	54.889921
2935.589284	229048.341497	54.894925
2934.876044	228784.975000	54.899930
2934.250589	228542.295795	54.904935
2933.794002	228279.959556	54.909940
2933.228044	228022.097196	54.914945
2932.128275	227766.204267	54.919949
2932.006671	227510.921064	54.924954
2931.140494	227252.573825	54.929959
2930.110941	226998.658036	54.934964
2929.422859	226740.691522	54.939969
2928.598075	226489.571023	54.944973
2928.192147	226229.880950	54.949978
2927.131917	225993.515709	54.954983
2926.723015	225744.012012	54.959988
2926.277357	225484.699719	54.964993
2925.771531	225244.124164	54.969997
2924.645038	224989.160440	54.975002
2924.039383	224742.402476	54.980007
2923.470161	224490.203661	54.985012
2922.412967	224245.530075	54.990017
2921.863272	224003.437488	54.995021
2921.426139	223752.658568	55.000026
2920.732239	223511.786928	55.005031
2919.976915	223263.224043	55.010036
2919.423755	223011.918427	55.015041
2918.831259	222763.535009	55.020045
2918.521114	222519.384935	55.025050
2917.526726	222267.795119	55.030055
2916.917963	222014.477444	55.035060
2916.372421	221766.140683	55.040065
2915.739093	221513.528679	55.045069
2915.177310	221248.876562	55.050074
2914.014586	221008.672444	55.055079
2913.290675	220752.894869	55.060084
2913.107784	220504.262922	55.065089
2912.091170	220258.717066	55.070093
2911.416803	220017.318573	55.075098
2910.574462	219763.421628	55.080103
2910.185279	219508.715491	55.085108
2909.764452	219255.988298	55.090113
2908.567155	219018.507408	55.095117
2908.404698	218765.384570	55.100122
2907.754009	218520.893993	55.105127
2906.938939	218259.729502	55.110132
2906.577664	218018.809896	55.115137
2905.420199	217767.630173	55.120141
2905.142809	217521.785497	55.125146
2904.258769	217279.512757	55.130151
2903.925595	217018.072818	55.135156
2903.115431	216769.043745	55.140161
2902.020744	216521.664447	55.145165
2901.526035	216270.741494	55.150170
2901.021414	216025.396242	55.155175
2899.804918	215770.554335	55.160180
2899.405281	215533.022406	55.165185
2898.778534	215295.794557	55.170189
2898.505382	215038.527545	55.175194
2897.429145	214797.897668	55.180199
2896.554562	214548.950415	55.185204
2895.845631	214306.558489	55.190209
2895.370413	214065.823312	55.195213
2895.141959	213812.003284	55.200218
2893.969062	213569.280168	55.205223
2893.749230	213326.330653	55.210228
2893.034147	213079.438305	55.215233
2891.974953	212831.328542	55.220237
2891.600800	212577.905409	55.225242
2890.941735	212345.644356	55.230247
2890.244003	212100.827616	55.235252
2889.913670	211848.393158	55.240257
2888.685227	211608.066213	55.245261
2888.196836	211360.902617	55.250266
2887.428679	211117.042611	55.255271
2886.912323	210867.556131	55.260276
2885.998659	210625.070191	55.265281
2885.746938	210376.956510	55.270285
2884.890431	210137.288940	55.275290
2884.287599	209899.223979	55.280295
2883.589093	209635.503478	55.285300
2883.211274	209393.357422	55.290305
2882.239917	209159.006432	55.295309
2881.803174	208909.820542	55.300314
2880.947882	208665.843802	55.305319
2880.362420	208408.423391	55.310324
2879.871442	208169.023684	55.315329
2878.902038	207926.722491	55.320333
2878.570184	207670.995920	55.325338
2877.474651	207425.280347	55.330343
2876.953707	207176.534823	55.335348
2876.169298	206937.911864	55.340353
2875.594630	206701.954760	55.345357
2874.912763	206451.519566	55.350362
2874.422912	206204.160377	55.355367
2873.609481	205959.806080	55.360372
2873.000463	205721.147474	55.365377
2872.178228	205472.520379	55.370381
2871.470596	205225.276120	55.375386
2870.623478	204994.854142	55.380391
2870.413355	204748.003996	55.385396
2869.815334	204500.898157	55.390401
2868.768688	204263.714698	55.395405
2868.051800	204016.680649	55.400410
2867.640058	203781.969362	55.405415
2866.643050	203527.524117	55.410420
2866.134854	203292.919186	55.415425
2865.388338	203054.293297	55.420429
2864.922135	202810.838986	55.425434
2864.509150	202576.145571	55.430439
2863.491851	202329.828140	55.435444
2862.927942	202089.013970	55.440449
2862.259485	201854.274933	55.445453
2861.449471	201607.406080	55.450458
2860.724979	201363.159020	55.455463
2860.085753	201129.474644	55.460468
2859.426446	200892.231232	55.465473
2859.066240	200657.550232	55.470477
2858.456252	200404.763074	55.475482
2857.158252	200168.387457	55.480487
2857.169508	199931.754625	55.485492
2856.672731	199688.738748	55.490497
2855.834813	199449.595593	55.495501
2855.185202	199197.074809	55.500506
2854.512584	198962.425119	55.505511
2853.681056	198723.067837	55.510516
2853.000317	198480.595531	55.515521
2852.291173	198229.552109	55.520525
2852.154601	197982.758429	55.525530
2851.041654	197749.990739	55.530535
2850.324709	197505.123585	55.535540
2849.714002	197269.873460	55.540545
2849.054795	197021.881812	55.545549
2848.425014	196775.260948	55.550554
2847.670007	196535.850522	55.555559
2847.015403	196288.459678	55.560564
2846.325617	196052.209576	55.565569
2845.629883	195819.944263	55.570573
2845.119210	195567.864167	55.575578
2844.223641	195333.762194	55.580583
2843.920967	195088.166393	55.585588
2843.602973	194850.679554	55.590593
2842.500205	194608.915523	55.595597
2841.742419	194363.713383	55.600602
2841.028959	194118.072788	55.605607
2840.776997	193864.891296	55.610612
2839.611647	193639.950234	55.615617
2838.861456	193398.377903	55.620621
2838.441733	193153.306238	55.625626
2837.680311	192911.140014	55.630631
2836.855974	192684.380632	55.635636
2836.348436	192439.580853	55.640641
2835.623999	192199.931520	55.645645
2834.999319	191955.152687	55.650650
2834.331856	191725.484609	55.655655
2833.800527	191485.286504	55.660660
2833.020505	191251.846890	55.665665
2832.175901	191011.166344	55.670669
2831.922461	190766.563670	55.675674
2831.194199	190534.646082	55.680679
2830.498121	190291.731744	55.685684
2830.119265	190060.320908	55.690689
2829.218739	189808.751544	55.695693
2828.595309	189563.399284	55.700698
2827.908689	189325.691994	55.705703
2827.443087	189077.212857	55.710708
2826.542007	188832.811638	55.715713
2825.806743	188605.268375	55.720717
2825.253768	188355.776312	55.725722
2824.765062	188115.893614	55.730727
2823.619126	187878.787942	55.735732
2823.130218	187635.447217	55.740737
2822.457999	187389.821324	55.745741
2822.009725	187150.369718	55.750746
2821.293014	186911.127244	55.755751
2820.674673	186673.244413	55.760756
2819.922957	186427.903354	55.765761
2819.214659	186195.444103	55.770765
2818.640911	185948.538044	55.775770
2817.860558	185706.334957	55.780775
2817.109078	185468.848363	55.785780
2816.404395	185238.492484	55.790785
2815.920928	184986.335962	55.795789
2815.535000	184741.823790	55.800794
2814.401918	184504.898806	55.805799
2813.701849	184264.433525	55.810804
2813.179147	184025.811479	55.815809
2812.242928	183797.713123	55.820813
2811.675305	183558.579100	55.825818
2811.001117	183333.672806	55.830823
2810.096443	183093.042670	55.835828
2809.739530	182859.349105	55.840833
2809.081820	182624.597684	55.845837
2808.204912	182391.001666	55.850842
2807.548354	182157.664563	55.855847
2807.138819	181926.324899	55.860852
2806.449221	181686.431599	55.865857
2805.827106	181453.779697	55.870861
2805.237909	181213.415144	55.875866
2804.310829	180973.461604	55.880871
2803.444703	180741.208325	55.885876
2803.135270	180512.378943	55.890881
2802.029599	180280.674888	55.895885
2801.728066	180040.512954	55.900890
2800.835182	179824.296346	55.905895
2800.539075	179585.357230	55.910900
2800.134438	179346.016873	55.915905
2799.021334	179118.072677	55.920909
2798.433441	178876.423503	55.925914
2797.473582	178647.846997	55.930919
2797.094452	178415.809007	55.935924
2796.523741	178182.746897	55.940929
2795.793900	177949.202493	55.945933
2795.368370	177720.788040	55.950938
2794.348754	177487.164901	55.955943
2793.839731	177244.965630	55.960948
2793.086129	177013.478019	55.965953
2792.248770	176788.110205	55.970957
2791.400999	176547.698455	55.975962
2791.116688	176319.879812	55.980967
2790.674674	176087.533980	55.985972
2789.795162	175854.342982	55.990977
2789.079873	175622.729873	55.995981
2788.979948	175383.554646	56.000986
2787.877435	175156.724184	56.005991
2787.088291	174916.872281	56.010996
2786.709586	174685.516404	56.016001
2785.815673	174452.806250	56.021005
2785.321520	174220.860809	56.026010
2784.681356	173983.674405	56.031015
2783.962001	173743.805650	56.036020
2783.396487	173514.940673	56.041025
2782.710576	173286.693821	56.046029
2782.204839	173035.209193	56.051034
2781.524764	172808.197792	56.056039
2780.691395	172566.230216	56.061044
2780.152439	172332.382347	56.066049
2779.621100	172095.177147	56.071053
2778.759963	171858.190931	56.076058
2778.222805	171627.297440	56.081063
2777.203500	171380.241329	56.086068
2776.847922	171147.248919	56.091073
2776.068815	170910.560618	56.096077
2775.380921	170660.862177	56.101082
2774.936938	170434.132213	56.106087
2774.160026	170194.141405	56.111092
2773.634527	169951.912192	56.116097
2772.868099	169721.841976	56.121101
2772.274232	169485.082108	56.126106
2771.382167	169260.451953	56.131111
2770.670728	169011.251070	56.136116
2769.933408	168770.448930	56.141121
2769.051081	168547.449128	56.146125
2768.760371	168306.172221	56.151130
2767.993251	168077.205555	56.156135
2766.981505	167841.488447	56.161140
2766.344271	167608.218591	56.166145
2765.359205	167393.113210	56.171149
2764.762640	167164.913421	56.176154
2764.678778	166940.474057	56.181159
2763.875437	166702.276804	56.186164
2763.417694	166473.207226	56.191169
2762.471398	166245.945787	56.196173
2762.051558	166015.436100	56.201178
2761.176207	165780.079002	56.206183
2760.398713	165547.416315	56.211188
2760.211936	165320.421653	56.216193
2759.476592	165101.271714	56.221197
2758.701237	164856.584159	56.226202
2758.081807	164633.527707	56.231207
2757.208017	164399.628643	56.236212
2756.769940	164169.743608	56.241217
2755.880360	163942.805136	56.246221
2755.453369	163706.194961	56.251226
2754.782250	163475.321266	56.256231
2754.133562	163250.090864	56.261236
2753.743761	163028.215684	56.266241
2752.832394	162707.911187	56.271245
2752.317858	162476.294273	56.276250
2751.592733	162247.407668	56.281255
2751.146919	162011.676053	56.286260
2750.392629	161770.387823	56.291265
2749.318886	161542.069482	56.296269
2748.984255	161305.816299	56.301274
2748.067436	161078.111755	56.306279
2747.451077	160836.668087	56.311284
2746.991015	160604.317165	56.316289
2746.089136	160372.241164	56.321293
2745.416675	160129.031233	56.326298
2744.799086	159907.084228	56.331303
2744.306949	159673.040835	56.336308
2743.552726	159438.646388	56.341313
2742.754165	159198.488631	56.346317
2742.290030	158967.941661	56.351322
2741.294935	158741.955373	56.356327
2740.909193	158507.724875	56.361332
2740.344721	158277.033063	56.366337
2739.408318	158046.414405	56.371341
2738.712668	157820.170512	56.376346
2738.176326	157590.266983	56.381351
2737.439385	157361.197655	56.386356
2736.709089	157117.038864	56.391361
2735.800469	156894.051044	56.396365
2735.507180	156669.441686	56.401370
2734.956661	156443.438038	56.406375
2734.095620	156201.836199	56.411380
2733.671960	155967.883095	56.416385
2732.796773	155745.215227	56.421389
2732.066043	155506.165501	56.426394
2731.474632	155297.502421	56.431399
2730.750479	155057.933602	56.436404
2730.315218	154818.943583	56.441409
2729.477995	154599.162767	56.446413
2728.868146	154366.267085	56.451418
2728.059197	154130.074122	56.456423
2727.547676	153899.123660	56.461428
2726.912625	153672.363678	56.466433
2726.124501	153449.913179	56.471437
2725.508425	153208.878548	56.476442
2724.843273	152984.987997	56.481447
2724.275427	152745.715905	56.486452
2723.631163	152520.998939	56.491457
2722.668602	152297.541444	56.496461
2722.064193	152065.270998	56.501466
2721.277966	151829.942288	56.506471
2720.905543	151600.816012	56.511476
2720.333398	151386.327323	56.516481
2719.481282	151154.649061	56.521485
2719.016999	150920.102007	56.526490
2718.485057	150694.388244	56.531495
2717.651296	150467.618065	56.536500
2717.266137	150234.550461	56.541505
2716.119715	150014.365925	56.546509
2715.552461	149770.501589	56.551514
2714.932617	149544.708009	56.556519
2713.851450	149320.628633	56.561524
2713.630771	149093.008307	56.566529
2712.579511	148868.901896	56.571533
2712.317222	148638.317332	56.576538
2711.418338	148411.584521	56.581543
2710.464254	148191.165841	56.586548
2710.188025	147953.420366	56.591553
2709.338578	147736.686592	56.596557
2708.468521	147517.237827	56.601562
2707.527956	147288.320900	56.606567
2707.239732	147071.909403	56.611572
2706.588778	146844.919641	56.616577
2705.798882	146625.388059	56.621581
2705.649778	146401.893078	56.626586
2704.941924	146191.349149	56.631591
2703.688741	145962.745466	56.636596
2703.653787	145736.047299	56.641601
2702.635069	145511.819507	56.646605
2701.814649	145278.856854	56.651610
2701.504626	145065.957245	56.656615
2700.559250	144845.052088	56.661620
2700.099905	144622.025528	56.666625
2699.150603	144402.687179	56.671629
2698.706441	144178.670174	56.676634
2698.142830	143960.874990	56.681639
2697.336555	143749.282897	56.686644
2696.974928	143515.269524	56.691649
2696.141749	143297.305675	56.696653
2695.535176	143076.105247	56.701658
2695.023109	142839.960590	56.706663
2694.253147	142625.562159	56.711668
2693.838303	142398.020835	56.716673
2693.017938	142174.509971	56.721677
2692.338423	141938.131921	56.726682
2691.534180	141723.529205	56.731687
2691.026706	141482.972343	56.736692
2690.651080	141267.695007	56.741697
2689.358349	141043.314268	56.746701
2688.813046	140812.946476	56.751706
2688.297502	140594.697393	56.756711
2687.535894	140369.602176	56.761716
2687.366039	140140.526850	56.766721
2685.952482	139920.125128	56.771725
2685.767013	139693.342725	56.776730
2685.110718	139468.999884	56.781735
2684.428051	139251.307921	56.786740
2683.730138	139027.178262	56.791745
2682.763349	138794.326151	56.796749
2682.375025	138568.168834	56.801754
2681.785649	138348.067354	56.806759
2680.596304	138121.824345	56.811764
2680.389211	137895.770464	56.816769
2679.462329	137679.183170	56.821773
2678.715900	137455.073015	56.826778
2678.243492	137236.917776	56.831783
2677.345397	137027.026089	56.836788
2677.127191	136797.082023	56.841793
2676.179942	136576.199194	56.846797
2675.586178	136348.973360	56.851802
2674.908115	136130.058521	56.856807
2674.542499	135907.259153	56.861812
2673.708481	135678.895087	56.866817
2673.037902	135461.229060	56.871821
2672.389007	135236.485162	56.876826
2672.119864	135013.347022	56.881831
2670.889105	134784.646299	56.886836
2670.606872	134565.007185	56.891841
2669.731535	134349.643153	56.896845
2669.297888	134121.850342	56.901850
2668.220081	133893.996247	56.906855
2667.590527	133668.905739	56.911860
2667.026815	133444.619554	56.916865
2666.263605	133234.759217	56.921869
2665.605101	133006.413808	56.926874
2664.801845	132792.510827	56.931879
2664.156412	132569.514708	56.936884
2664.041648	132353.219435	56.941889
2663.262046	132128.634784	56.946893
2662.311937	131897.816635	56.951898
2662.030176	131678.135997	56.956903
2661.092819	131459.437386	56.961908
2660.832584	131229.772874	56.966913
2659.751116	131018.277191	56.971917
2659.127208	130792.255819	56.976922
2658.390835	130565.072807	56.981927
2657.371960	130346.128988	56.986932
2656.925119	130128.988774	56.991937
2656.368034	129914.865261	56.996941
2655.726124	129684.727643	57.001946
2655.202532	129465.115251	57.006951
2654.369436	129244.385112	57.011956
2653.841780	129013.345829	57.016961
2652.962298	128805.099000	57.021965
2652.363374	128581.504679	57.026970
2651.934644	128366.496334	57.031975
2650.790885	128147.081501	57.036980
2650.516709	127924.139556	57.041985
2649.652387	127713.701309	57.046989
2649.035146	127480.186979	57.051994
2648.599607	127268.604649	57.056999
2647.715451	127045.512443	57.062004
2647.531205	126813.890980	57.067009
2646.444140	126603.534610	57.072013
2645.832006	126376.137540	57.077018
2645.422139	126161.498994	57.082023
2644.443813	125936.601962	57.087028
2643.858474	125715.124198	57.092033
2642.866744	125501.129125	57.097037
2642.189318	125277.180415	57.102042
2641.760374	125061.309014	57.107047
2641.328333	124840.080768	57.112052
2640.538414	124610.021687	57.117057
2639.488416	124403.930623	57.122061
2638.952571	124182.279739	57.127066
2638.545556	123965.880247	57.132071
2637.859710	123752.218793	57.137076
2637.003589	123526.370003	57.142081
2636.430629	123311.335420	57.147085
2635.759273	123094.591177	57.152090
2634.977395	122873.777364	57.157095
2634.474020	122655.118023	57.162100
2634.015551	122441.938909	57.167105
2633.300374	122228.154582	57.172109
2632.696447	122007.294346	57.177114
2632.163229	121783.605843	57.182119
2631.071507	121567.969135	57.187124
2630.288799	121353.491481	57.192129
2629.676369	121133.604876	57.197133
2629.379822	120911.994000	57.202138
2628.525548	120697.901227	57.207143
2627.670938	120476.788749	57.212148
2627.265968	120246.058739	57.217153
2626.381581	120044.317532	57.222157
2625.695877	119823.653568	57.227162
2625.022934	119611.305766	57.232167
2624.062542	119386.530851	57.237172
2623.546937	119185.232991	57.242177
2622.849525	118985.476361	57.247181
2622.325566	118750.353702	57.252186
2621.904573	118549.591696	57.257191
2620.707501	118337.292887	57.262196
2620.590483	118115.124953	57.267201
2619.609987	117912.076049	57.272205
2619.145063	117701.247064	57.277210
2618.700973	117478.330243	57.282215
2617.945437	117262.402809	57.287220
2617.196164	117042.648520	57.292225
2616.172923	116834.047929	57.297229
2615.603730	116615.373247	57.302234
2614.805318	116403.503245	57.307239
2614.075477	116204.598428	57.312244
2613.618958	115983.588093	57.317249
2612.870910	115789.037397	57.322253
2612.435985	115574.266677	57.327258
2611.640352	115363.877436	57.332263
2611.055700	115147.306020	57.337268
2610.443268	114927.598991	57.342273
2609.472655	114724.161209	57.347277
2609.098086	114520.364027	57.352282
2608.557524	114299.203917	57.357287
2607.763428	114095.952661	57.362292
2607.247897	113872.056773	57.367297
2606.088341	113672.256102	57.372301
2605.587514	113465.041088	57.377306
2604.990744	113256.833848	57.382311
2604.090015	113046.835955	57.387316
2603.765268	112827.888602	57.392321
2602.735173	112640.540468	57.397325
2602.401670	112426.700686	57.402330
2601.863746	112208.509694	57.407335
2600.776910	112011.680900	57.412340
2600.526179	111782.995509	57.417345
2599.790164	111586.685653	57.422349
2599.119953	111379.248212	57.427354
2598.409897	111167.490683	57.432359
2597.733348	110962.761226	57.437364
2597.100734	110736.068886	57.442369
2596.276654	110538.803978	57.447373
2595.828069	110328.516210	57.452378
2595.298314	110115.590482	57.457383
2594.435830	109911.838403	57.462388
2593.812275	109690.294427	57.467393
2593.266092	109489.084835	57.472397
2592.644593	109279.512433	57.477402
2591.475486	109083.107094	57.482407
2591.036574	108858.197187	57.487412
2590.709430	108644.211426	57.492417
2589.597507	108449.756556	57.497421
2588.976883	108238.892099	57.502426
2588.304836	108024.922012	57.507431
2587.824668	107822.973261	57.512436
2587.673917	107609.311283	57.517441
2586.891479	107400.567351	57.522445
2585.773694	107187.417681	57.527450
2585.285151	106978.706951	57.532455
2584.854743	106771.105546	57.537460
2584.054104	106562.961822	57.542465
2582.890426	106352.187155	57.547469
2582.527943	106136.522314	57.552474
2582.156163	105928.665077	57.557479
2580.958204	105725.267743	57.562484
2580.454360	105512.143460	57.567489
2579.892890	105296.524045	57.572493
2579.253940	105089.649096	57.577498
2578.435679	104898.221737	57.582503
2577.909411	104687.690609	57.587508
2577.350852	104472.078174	57.592513
2576.504217	104264.627879	57.597517
2575.681958	104051.655920	57.602522
2575.382702	103848.887131	57.607527
2574.557885	103653.619821	57.612532
2573.962646	103437.089986	57.617537
2573.272417	103225.068849	57.622541
2572.742310	103021.024149	57.627546
2572.068497	102806.123949	57.632551
2571.090392	102604.507495	57.637556
2570.642718	102384.227319	57.642561
2569.773240	102193.254980	57.647565
2569.128324	101979.816838	57.652570
2568.645742	101781.668761	57.657575
2567.818961	101574.384871	57.662580
2567.166491	101355.453615	57.667585
2566.621999	101160.067415	57.672589
2566.097258	100947.317438	57.677594
2565.180962	100738.164779	57.682599
2564.403838	100543.600863	57.687604
2564.096206	100330.346353	57.692609
2563.268082	100126.405819	57.697613
2562.740645	99920.281742	57.702618
2562.170809	99711.838262	57.707623
2561.066139	99506.196292	57.712628
2560.478097	99305.256962	57.717633
2559.979579	99103.689917	57.722637
2559.263619	98890.608527	57.727642
2558.648960	98684.801069	57.732647
2557.773274	98485.170376	57.737652
2557.177362	98281.742129	57.742657
2556.798548	98069.629758	57.747661
2555.973842	97861.852311	57.752666
2555.466475	97653.005288	57.757671
2554.731773	97454.553638	57.762676
2554.300506	97249.719435	57.767681
2553.565688	97046.432003	57.772685
2553.205746	96831.493039	57.777690
2551.938755	96618.253743	57.782695
2551.092325	96418.332029	57.787700
2550.747782	96202.052006	57.792705
2549.960941	96007.299731	57.797709
2549.320855	95799.289858	57.802714
2548.802191	95591.288019	57.807719
2547.786306	95381.299409	57.812724
2547.391476	95183.466958	57.817729
2546.433767	94987.069938	57.822733
2546.183682	94777.764648	57.827738
2545.582897	94573.660069	57.832743
2544.902068	94367.775323	57.837748
2544.091975	94154.321987	57.842753
2543.282063	93951.905038	57.847757
2542.722587	93747.395564	57.852762
2542.417181	93536.537911	57.857767
2541.484862	93332.503524	57.862772
2540.583752	93127.026565	57.867777
2539.661965	92920.242127	57.872781
2539.582096	92719.274258	57.877786
2539.243361	92508.704278	57.882791
2538.075083	92312.516305	57.887796
2537.346636	92101.003721	57.892801
2536.815257	91899.176355	57.897805
2536.151163	91692.508349	57.902810
2535.540682	91488.116500	57.907815
2534.462249	91283.306129	57.912820
2533.934845	91076.736353	57.917825
2533.129726	90882.868616	57.922829
2532.677593	90680.919350	57.927834
2532.175602	90472.899197	57.932839
2531.177852	90271.452315	57.937844
2530.913642	90067.297752	57.942849
2529.981827	89864.531676	57.947853
2529.049571	89664.956757	57.952858
2528.700791	89462.761389	57.957863
2528.125916	89265.384283	57.962868
2527.126446	89064.715957	57.967873
2526.330302	88869.254208	57.972877
2526.039523	88656.412022	57.977882
2525.501452	88470.467453	57.982887
2524.514716	88270.000979	57.987892
2523.995304	88068.980450	57.992897
2523.455830	87860.693156	57.997901
2522.911610	87665.253032	58.002906
2522.009034	87465.997899	58.007911
2521.606268	87268.427808	58.012916
2520.748786	87061.758178	58.017921
2520.341610	86862.715371	58.022925
2519.449807	86654.077150	58.027930
2518.827278	86449.886589	58.032935
2518.107063	86263.140400	58.037940
2517.550855	86050.125052	58.042945
2516.982481	85856.803479	58.047949
2516.121500	85658.002248	58.052954
2515.669275	85445.642043	58.057959
2514.582415	85250.753618	58.062964
2514.482435	85040.775808	58.067969
2513.631569	84851.786940	58.072973
2512.769422	84639.100384	58.077978
2512.538440	84428.629581	58.082983
2511.484266	84233.225501	58.087988
2510.843871	84033.580416	58.092993
2510.259559	83833.078939	58.097997
2509.566672	83633.889644	58.103002
2508.939420	83426.901757	58.108007
2508.239864	83228.414576	58.113012
2507.874113	83028.830509	58.118017
2507.127443	82829.555906	58.123021
2506.421058	82615.698724	58.128026
2506.029217	82412.974491	58.133031
2504.680638	82208.667212	58.138036
2503.933083	82005.115957	58.143041
2503.587698	81806.712800	58.148045
2503.055231	81606.179922	58.153050
2502.604989	81399.697293	58.158055
2501.656579	81209.260753	58.163060
2501.012227	80994.364521	58.168065
2499.986848	80798.803970	58.173069
2499.710209	80599.824631	58.178074
2499.406004	80398.677757	58.183079
2498.246269	80197.079052	58.188084
2498.026683	79985.725626	58.193089
2496.976875	79791.445917	58.198093
2496.079051	79584.690995	58.203098
2495.526653	79384.290401	58.208103
2494.777432	79189.639148	58.213108
2494.284960	78980.043957	58.218113
2493.318125	78792.528594	58.223117
2492.650803	78598.079060	58.228122
2492.596309	78398.325191	58.233127
2491.460229	78203.668523	58.238132
2490.835535	77999.877220	58.243137
2490.387058	77806.496754	58.248141
2489.439946	77602.329602	58.253146
2488.848157	77407.068254	58.258151
2488.010440	77208.502004	58.263156
2487.642491	76999.192413	58.268161
2486.975013	76803.777732	58.273165
2486.161908	76609.363821	58.278170
2485.405316	76413.428406	58.283175
2484.599372	76221.361527	58.288180
2484.249749	76028.235663	58.293185
2483.590207	75829.616573	58.298189
2482.521395	75634.213374	58.303194
2482.053300	75436.727294	58.308199
2481.377089	75249.578516	58.313204
2480.637183	75054.141440	58.318209
2480.529754	74864.333650	58.323213
2479.627811	74669.673614	58.328218
2479.042760	74466.798386	58.333223
2478.473491	74280.807407	58.338228
2477.716733	74082.696054	58.343233
2477.235077	73881.318215	58.348237
2476.458081	73676.232237	58.353242
2475.840338	73478.364555	58.358247
2474.914547	73284.127167	58.363252
2474.563676	73082.280455	58.368257
2473.764114	72876.902128	58.373261
2473.024404	72690.034283	58.378266
2472.660421	72480.454070	58.383271
2471.954535	72293.806298	58.388276
2471.105789	72097.091200	58.393281
2470.334686	71887.537410	58.398285
2469.630685	71689.270328	58.403290
2468.951324	71495.720779	58.408295
2468.336775	71300.610816	58.413300
2468.071147	71098.910021	58.418305
2467.330670	70908.872648	58.423309
2466.352963	70709.322131	58.428314
2465.870898	70509.276971	58.433319
2465.051916	70313.341308	58.438324
2464.802097	70120.332534	58.443329
2463.798419	69920.635738	58.448333
2463.207394	69714.401912	58.453338
2462.826872	69515.509897	58.458343
2461.862442	69317.865277	58.463348
2461.259945	69112.089306	58.468353
2460.419199	68918.438573	58.473357
2459.876496	68722.468610	58.478362
2459.331027	68518.773693	58.483367
2458.422334	68327.704796	58.488372
2457.710212	68119.904460	58.493377
2456.939866	67933.194119	58.498381
2456.389632	67745.525955	58.503386
2456.069186	67540.982179	58.508391
2455.303617	67344.542011	58.513396
2454.624650	67139.242270	58.518401
2453.867067	66935.109835	58.523405
2453.134727	66743.559840	58.528410
2452.507153	66551.387133	58.533415
2452.030487	66361.459689	58.538420
2451.353508	66157.572818	58.543425
2450.530258	65963.252040	58.548429
2449.605194	65771.374896	58.553434
2449.257681	65570.234837	58.558439
2448.190920	65386.027840	58.563444
2447.592238	65188.395665	58.568449
2446.979915	64994.497666	58.573453
2446.198924	64804.583121	58.578458
2445.721494	64605.193058	58.583463
2445.128964	64417.082590	58.588468
2444.465138	64227.839088	58.593473
2443.966307	64032.656807	58.598477
2443.237230	63846.929245	58.603482
2442.481899	63647.035956	58.608487
2441.830313	63451.820496	58.613492
2441.176127	63255.530974	58.618497
2440.594126	63068.445240	58.623501
2439.695005	62872.518265	58.628506
2439.173965	62672.126308	58.633511
2438.244264	62485.538334	58.638516
2437.807422	62291.206180	58.643521
2437.260326	62102.706074	58.648525
2436.547110	61913.091302	58.653530
2435.961229	61710.595475	58.658535
2435.259287	61525.240836	58.663540
2434.902915	61320.670853	58.668545
2434.358942	61128.716600	58.673549
2433.240534	60933.898612	58.678554
2432.844750	60746.397883	58.683559
2432.029009	60540.915161	58.688564
2431.389837	60343.925311	58.693569
2430.703604	60147.362839	58.698573
2430.154190	59953.648703	58.703578
2429.989863	59757.352605	58.708583
2429.029628	59565.081441	58.713588
2428.129257	59356.766672	58.718593
2427.334493	59160.326712	58.723597
2426.792725	58968.229569	58.728602
2426.223510	58771.932024	58.733607
2425.366147	58573.760890	58.738612
2424.761786	58374.272981	58.743617
2424.252165	58179.279476	58.748621
2423.335449	57990.144876	58.753626
2422.743690	57781.615176	58.758631
2421.788684	57599.707196	58.763636
2421.427217	57394.782064	58.768641
2420.948846	57198.882339	58.773645
2420.207624	57003.570746	58.778650
2419.629800	56807.827021	58.783655
2418.796792	56623.013312	58.788660
2418.175358	56413.699803	58.793665
2417.407875	56224.334852	58.798669
2416.724140	56034.161020	58.803674
2416.156116	55835.517535	58.808679
2415.164940	55645.146444	58.813684
2414.814103	55461.790191	58.818689
2413.849235	55251.648707	58.823693
2413.439086	55069.726734	58.828698
2412.795768	54866.649757	58.833703
2412.115729	54685.347193	58.838708
2411.723860	54488.911912	58.843713
2410.710698	54294.909535	58.848717
2409.927288	54107.806282	58.853722
2409.418875	53899.180715	58.858727
2408.714216	53710.682995	58.863732
2408.058430	53529.049460	58.868737
2407.527822	53335.879466	58.873741
2406.517836	53135.240517	58.878746
2405.925896	52943.441927	58.883751
2405.317729	52762.438197	58.888756
2405.067365	52566.137258	58.893761
2404.311217	52386.081548	58.898765
2403.207592	52191.271091	58.903770
2402.955247	51986.692864	58.908775
2402.343601	51794.678566	58.913780
2401.454227	51609.547963	58.918785
2400.720871	51415.066853	58.923789
2400.112832	51222.624589	58.928794
2399.546720	51035.021813	58.933799
2398.796332	50839.397919	58.938804
2398.310646	50641.579543	58.943809
2397.661709	50446.532327	58.948813
2396.233615	50259.295795	58.953818
2396.255443	50066.411674	58.958823
2395.421197	49885.624516	58.963828
2394.586230	49688.381401	58.968833
2394.237149	49502.481309	58.973837
2393.507733	49314.020754	58.978842
2392.780274	49118.839095	58.983847
2391.688820	48940.250407	58.988852
2391.232921	48747.519526	58.993857
2390.881582	48564.432502	58.998861
2390.094143	48382.397206	59.003866
2389.481106	48179.438063	59.008871
2389.066640	47996.689567	59.013876
2388.235881	47813.838136	59.018881
2387.369769	47617.464353	59.023885
2386.687180	47431.493243	59.028890
2386.188265	47237.504397	59.033895
2385.559386	47055.448081	59.038900
2384.941338	46855.105118	59.043905
2384.323495	46663.235504	59.048909
2383.337866	46484.332113	59.053914
2382.855418	46291.755493	59.058919
2382.132779	46103.176130	59.063924
2381.537178	45909.612593	59.068929
2380.736227	45728.713826	59.073933
2379.965323	45534.903863	59.078938
2379.790233	45348.823625	59.083943
2379.054531	45166.901816	59.088948
2378.493425	44967.501213	59.093953
2378.062020	44781.018508	59.098957
2377.227788	44584.746223	59.103962
2376.534951	44382.422234	59.108967
2375.691052	44192.664956	59.113972
2375.172412	43995.413065	59.118977
2374.551472	43807.699377	59.123981
2373.725973	43617.673444	59.128986
2373.157305	43422.877549	59.133991
2372.121875	43240.577401	59.138996
2371.514945	43044.201024	59.144001
2371.133731	42847.553884	59.149005
2370.261541	42668.747430	59.154010
2369.420760	42473.711217	59.159015
2368.824842	42292.024946	59.164020
2367.984372	42101.549942	59.169025
2367.508807	41914.959477	59.174029
2366.897685	41723.095619	59.179034
2366.602615	41537.653829	59.184039
2365.478717	41354.059411	59.189044
2365.097377	41166.418546	59.194049
2364.431867	40967.953172	59.199053
2363.559323	40789.763881	59.204058
2362.892595	40593.159211	59.209063
2362.331600	40408.144883	59.214068
2361.590499	40220.163482	59.219073
2360.979432	40035.793519	59.224077
2360.319179	39850.092657	59.229082
2359.981917	39659.647092	59.234087
2358.763429	39479.663884	59.239092
2358.250652	39278.050895	59.244097
2357.564074	39108.438843	59.249101
2356.863847	38925.658518	59.254106
2356.418396	38731.138004	59.259111
2355.619540	38549.852318	59.264116
2354.728149	38360.827563	59.269121
2354.324711	38180.403163	59.274125
2353.737798	37994.608108	59.279130
2353.200553	37800.642361	59.284135
2352.178104	37612.117798	59.289140
2351.421847	37420.876879	59.294145
2351.427236	37241.044161	59.299149
2350.441138	37053.888975	59.304154
2349.748668	36865.069063	59.309159
2348.981342	36689.370281	59.314164
2348.406395	36494.268404	59.319169
2347.544808	36316.593632	59.324173
2346.999279	36129.587471	59.329178
2346.427846	35937.953088	59.334183
2345.465200	35767.360805	59.339188
2344.733608	35580.192676	59.344193
2344.289741	35392.759721	59.349197
2343.492970	35214.092129	59.354202
2343.271687	35019.774727	59.359207
2342.503312	34839.467599	59.364212
2341.825962	34656.652353	59.369217
2340.947441	34479.012345	59.374221
2340.374949	34295.302503	59.379226
2339.827732	34102.136383	59.384231
2339.403803	33919.002948	59.389236
2338.436273	33732.709967	59.394241
2337.963679	33550.607665	59.399245
2337.159286	33367.888308	59.404250
2336.780816	33170.431272	59.409255
2335.751081	32983.143526	59.414260
2335.162252	32793.515451	59.419265
2334.651935	32603.404575	59.424269
2333.757365	32421.963107	59.429274
2333.515692	32242.283229	59.434279
2332.408708	32051.111805	59.439284
2331.805620	31866.194710	59.444289
2331.140569	31678.010541	59.449293
2330.626195	31493.450156	59.454298
2329.841033	31304.865789	59.459303
2329.255208	31126.407729	59.464308
2328.698380	30935.986809	59.469313
2328.131495	30753.912804	59.474317
2327.265795	30566.414671	59.479322
2326.845889	30378.524053	59.484327
2325.853261	30198.457759	59.489332
2324.991064	30005.678508	59.494337
2324.435851	29822.246214	59.499341
2323.471454	29639.550799	59.504346
2323.007217	29457.429062	59.509351
2322.518344	29278.166728	59.514356
2321.801560	29094.498027	59.519361
2321.297210	28910.491186	59.524365
2320.004380	28738.479993	59.529370
2319.665786	28551.531173	59.534375
2319.277841	28374.803261	59.539380
2318.376822	28192.039722	59.544385
2317.777364	28017.412567	59.549389
2316.794160	27830.082916	59.554394
2316.212231	27652.099711	59.559399
2316.048246	27483.265682	59.564404
2315.061435	27288.890523	59.569409
2314.366837	27110.537751	59.574413
2313.448168	26943.922241	59.579418
2313.039400	26754.286427	59.584423
2312.269000	26591.785231	59.589428
2311.452564	26406.291496	59.594433
2311.150022	26226.810492	59.599437
2310.533271	26052.752231	59.604442
2309.912027	25867.334036	59.609447
2309.021105	25701.347742	59.614452
2308.654894	25523.717043	59.619457
2308.258071	25334.813938	59.624461
2307.191017	25153.080922	59.629466
2306.555127	24972.335943	59.634471
2305.727789	24798.412303	59.639476
2305.366249	24621.870448	59.644481
2304.670981	24440.867608	59.649485
2303.752983	24257.062975	59.654490
2302.989019	24078.014761	59.659495
2302.436512	23908.835131	59.664500
2301.686479	23724.987066	59.669505
2301.465828	23543.048818	59.674509
2300.479944	23370.650498	59.679514
2299.954777	23190.146559	59.684519
2299.124290	23006.655935	59.689524
2298.360534	22827.342945	59.694529
2297.905890	22655.302427	59.699533
2297.593599	22475.621714	59.704538
2296.737786	22292.934577	59.709543
2295.803769	22114.074357	59.714548
2295.133735	21937.543196	59.719553
2294.322633	21760.453627	59.724557
2293.518901	21582.232552	59.729562
2293.257986	21413.084510	59.734567
2292.503754	21238.201881	59.739572
2291.834854	21059.357310	59.744577
2291.538530	20878.698840	59.749581
2290.467975	20701.257216	59.754586
2289.863509	20516.913904	59.759591
2288.904674	20348.173775	59.764596
2288.530849	20177.183243	59.769601
2287.801698	19995.050494	59.774605
2287.022569	19819.726438	59.779610
2286.530987	19640.445061	59.784615
2286.007859	19476.383097	59.789620
2284.949867	19300.661012	59.794625
2284.584649	19123.545316	59.799629
2283.857576	18958.355026	59.804634
2283.206448	18773.968092	59.809639
2282.476624	18601.682605	59.814644
2281.672690	18421.392993	59.819649
2281.407066	18238.756713	59.824653
2280.322780	18084.768719	59.829658
2279.523675	17903.451326	59.834663
2279.238780	17738.745725	59.839668
2278.292218	17562.824576	59.844673
2277.902971	17396.466758	59.849677
2277.129109	17225.172442	59.854682
2276.542883	17042.128957	59.859687
2275.698636	16886.646854	59.864692
2274.846923	16707.400968	59.869697
2274.568538	16533.480670	59.874701
2273.656470	16374.272070	59.879706
2273.212321	16196.522865	59.884711
2272.241668	16027.107817	59.889716
2271.613897	15863.824652	59.894721
2270.941030	15688.055369	59.899725
2270.261192	15533.504787	59.904730
2270.088880	15351.754469	59.909735
2269.001419	15192.087402	59.914740
2268.144342	15018.540321	59.919745
2267.641332	14853.580960	59.924750
2266.763566	14692.601347	59.929754
2266.116742	14520.645219	59.934759
2265.631550	14350.003949	59.939764
2264.777601	14187.418918	59.944769
2264.284665	14031.651620	59.949774
2263.390159	13866.005495	59.954778
2262.823666	13693.273811	59.959783
2262.086554	13540.379117	59.964788
2261.597900	13383.782526	59.969793
2260.802452	13212.790249	59.974798
2260.187804	13056.035083	59.979802
2259.391623	12884.916071	59.984807
2258.455469	12727.931827	59.989812
2258.153633	12573.958004	59.994817
2257.449151	12410.510193	59.999822
2256.986832	12256.014495	60.004826
2256.515784	12086.559676	60.009831
2255.607884	11929.398078	60.014836
2254.867542	11756.412913	60.019841
2254.599308	11601.032527	60.024846
2253.290506	11440.566111	60.029850
2252.823591	11262.994584	60.034855
2252.340704	11115.263248	60.039860
2251.250251	10962.887156	60.044865
2250.716820	10797.789815	60.049870
2250.090359	10648.369962	60.054874
2249.641318	10481.321975	60.059879
2248.653101	10321.284453	60.064884
2247.889253	10172.082038	60.069889
2247.521256	10011.291350	60.074894
2246.648110	9866.097644	60.079898
2246.207411	9697.083246	60.084903
2245.550822	9543.866954	60.089908
2244.621136	9380.384124	60.094913
2244.173297	9231.596908	60.099918
2243.241190	9074.304646	60.104922
2242.621633	8915.741932	60.109927
2241.751984	8770.316991	60.114932
2240.972150	8619.099302	60.119937
2240.959831	8466.875785	60.124942
2239.853647	8318.450939	60.129946
2239.060178	8163.486606	60.134951
2238.520060	8017.381189	60.139956
2238.101504	7874.996990	60.144961
2237.227976	7719.843636	60.149966
2235.888097	7580.445706	60.154970
2235.635154	7435.802472	60.159975
2234.808638	7289.613891	60.164980
2234.408651	7145.423577	60.169985
2233.638893	6993.421940	60.174990
2232.940013	6854.915968	60.179994
2231.962407	6703.440929	60.184999
2231.069950	6563.883293	60.190004
2230.602517	6418.565283	60.195009
2230.076622	6279.781622	60.200014
2228.927887	6152.767187	60.205018
2228.869988	6003.232712	60.210023
2228.232942	5869.410099	60.215028
2227.598550	5739.715301	60.220033
2226.490480	5597.467320	60.225038
2225.887396	5465.442204	60.230042
2225.008948	5329.153605	60.235047
2224.522367	5190.340741	60.240052
2223.763783	5060.337136	60.245057
2222.884677	4928.827533	60.250062
2221.839324	4806.226079	60.255066
2221.256705	4675.794877	60.260071
2220.917338	4544.418391	60.265076
2220.606143	4421.086072	60.270081
2219.706725	4294.710532	60.275086
2219.022482	4169.851776	60.280090
2218.157411	4042.805682	60.285095
2217.276475	3920.392921	60.290100
2216.313428	3797.778887	60.295105
2216.142003	3663.716190	60.300110
2215.026128	3561.634464	60.305114
2214.690782	3442.982398	60.310119
2213.931389	3324.319692	60.315124
2213.389633	3212.820040	60.320129
2212.630020	3097.007094	60.325134
2211.842135	2976.446297	60.330138
2211.550049	2859.270016	60.335143
2210.461545	2748.968676	60.340148
2210.014667	2630.877128	60.345153
2209.375860	2517.413926	60.350158
2207.904365	2408.197189	60.355162
2207.480102	2299.688131	60.360167
2206.835060	2195.066507	60.365172
2205.883141	2085.148319	60.370177
2205.424755	1980.762796	60.375182
2204.762515	1889.065024	60.380186
2204.079541	1778.067886	60.385191
2203.623671	1676.769901	60.390196
2202.706850	1573.822691	60.395201
2202.231940	1471.323404	60.400206
2201.109016	1371.969166	60.405210
2200.618316	1265.228155	60.410215
2199.775108	1172.252990	60.415220
2199.203351	1071.867867	60.420225
2198.040311	983.869970	60.425230
2197.152197	899.475228	60.430234
2196.599634	802.587697	60.435239
2195.961804	725.946626	60.440244
2195.167401	641.095355	60.445249
2194.733951	558.475624	60.450254
2193.502738	483.040222	60.455258
2192.720509	397.298986	60.460263
2191.867056	327.439224	60.465268
2190.855549	266.652269	60.470273
2190.143212	196.504231	60.475278
2188.754084	145.641948	60.480282
2188.126015	83.071253	60.485287
2187.139803	45.357560	60.490292
2185.740354	14.562374	60.495297
2184.878698	-14.626743	60.500302
2183.783251	-29.546347	60.505306
2182.496458	-38.775750	60.510311
2181.303615	-41.330453	60.515316
2180.343971	-31.575877	60.520321
2179.514837	-31.732907	60.525326
2179.023688	-31.232337	60.530330
2178.711305	-29.873859	60.535335
2178.188105	-29.641024	60.540340
2177.557869	-31.256789	60.545345
2177.494482	-45.922214	60.550350
2177.177907	-48.850913	60.555354
2176.439943	-59.402160	60.560359
2175.917808	-70.785600	60.565364
2174.993440	-73.106917	60.570369
2174.709678	-82.545891	60.575374
2173.717931	-88.568744	60.580378
2173.029048	-90.820184	60.585383
2172.367285	-93.465442	60.590388
2171.473765	-101.173901	60.595393
2170.942410	-96.681908	60.600398
2169.753776	-93.577459	60.605402
2169.152646	-95.417034	60.610407
2168.748457	-84.512685	60.615412
2168.186043	-80.526704	60.620417
2167.738834	-82.064265	60.625422
2167.126132	-85.138363	60.630426
2166.690453	-84.107263	60.635431
2165.954830	-84.977730	60.640436
2164.936521	-81.338893	60.645441
2164.847267	-80.591421	60.650446
2163.803337	-69.421551	60.655450
2162.919707	-65.118088	60.660455
2162.568842	-65.497656	60.665460
2161.600864	-62.336742	60.670465
2161.354855	-55.696417	60.675470
2160.430580	-49.882051	60.680474
2159.726961	-47.865395	60.685479
2159.546135	-50.465537	60.690484
2158.515991	-40.721854	60.695489
2158.366669	-49.112977	60.700494
2157.168771	-39.956126	60.705498
2156.596681	-44.402349	60.710503
2156.280039	-35.893112	60.715508
2155.853260	-30.146634	60.720513
2154.664803	-42.774271	60.725518
2154.123267	-32.155604	60.730522
2153.800597	-35.162184	60.735527
2153.508519	-33.190322	60.740532
2151.958947	-23.193893	60.745537
2151.742357	-26.050146	60.750542
2150.409469	-21.347369	60.755546
2150.026000	-13.595511	60.760551
2150.088580	-16.294206	60.765556
2149.081149	-14.573121	60.770561
2148.801369	-31.847263	60.775566
2147.476650	-13.817029	60.780570
2146.974620	-14.194689	60.785575
2146.750594	-15.162101	60.790580
2145.927118	-7.957029	60.795585
2145.264692	-12.541893	60.800590
2144.410980	-10.837313	60.805594
2143.902120	-7.108970	60.810599
2143.591312	-0.513533	60.815604
2142.668843	-1.021606	60.820609
2142.071845	-10.831977	60.825614
2141.017505	-12.437213	60.830618
2140.624568	-0.941637	60.835623
2140.438901	-4.935082	60.840628
2139.491534	-4.617588	60.845633
2138.992632	-9.067545	60.850638
2137.737593	-2.596681	60.855642
2137.311363	-8.866984	60.860647
2136.294264	2.000639	60.865652
2135.917104	9.637964	60.870657
2135.525889	0.394195	60.875662
2134.778042	2.007862	60.880666
2134.385547	8.475913	60.885671
2133.541791	1.450243	60.890676
2132.868066	15.321186	60.895681
2132.642959	5.385564	60.900686
2131.974501	4.397207	60.905690
2131.275120	-1.052295	60.910695
2130.609828	8.193553	60.915700
2129.808361	5.344946	60.920705
2128.840732	0.792740	60.925710
2128.232983	7.358026	60.930714
2127.182890	7.605090	60.935719
2126.136716	5.680009	60.940724
2126.038022	21.391535	60.945729
2126.041861	14.428492	60.950734
2125.238017	24.606263	60.955738
2124.293009	15.865112	60.960743
2123.727292	12.597463	60.965748
2122.887241	15.697105	60.970753
2122.089948	14.722886	60.975758
2121.598736	22.493438	60.980762
2121.484857	19.912626	60.985767
2120.523065	15.987138	60.990772
2119.848542	26.776768	60.995777
2119.725399	20.086192	61.000782
2118.695775	22.578811	61.005786
2117.440984	24.553633	61.010791
2116.819901	23.858969	61.015796
2116.339813	24.187481	61.020801
2116.002630	23.272720	61.025806
2115.398306	30.987107	61.030810
2114.948795	29.426253	61.035815
2114.068591	21.472781	61.040820
2113.343205	17.382046	61.045825
2112.383275	25.108703	61.050830
2111.567449	31.025757	61.055834
2111.202592	32.007786	61.060839
2110.473297	32.607663	61.065844
2109.614525	42.284796	61.070849
2109.681627	32.083587	61.075854
2109.295296	30.564750	61.080858
2107.775493	25.571873	61.085863
2107.009876	24.912762	61.090868
2106.699981	33.370505	61.095873
2106.458971	32.572952	61.100878
2105.938899	32.212354	61.105882
2104.778231	19.395773	61.110887
2103.881921	22.173179	61.115892
2102.765925	34.305510	61.120897
2102.410339	27.530389	61.125902
2102.309174	36.369763	61.130906
2101.983186	32.933182	61.135911
2101.257327	32.777134	61.140916
2100.247478	39.920349	61.145921
2099.456051	27.742203	61.150926
2099.071442	30.539339	61.155930
2098.165970	23.473002	61.160935
2097.164967	34.763894	61.165940
2096.855626	42.414132	61.170945
2096.725424	31.430503	61.175950
2095.299064	28.342011	61.180954
2095.026951	33.403214	61.185959
2094.160439	32.417908	61.190964
2093.351038	36.887842	61.195969
2093.479193	39.289787	61.200974
2092.170781	33.361327	61.205978
2091.020144	36.797283	61.210983
2091.021141	40.397426	61.215988
2090.145051	40.821902	61.220993
2089.949125	38.079062	61.225998
2089.191868	39.911866	61.231002
2088.500559	36.306171	61.236007
2087.680709	33.504645	61.241012
2086.380019	40.981033	61.246017
2086.529340	43.840104	61.251022
2085.783771	39.877156	61.256026
2084.907804	43.290029	61.261031
2084.435947	41.944044	61.266036
2083.650773	44.197607	61.271041
2082.885670	33.567054	61.276046
2082.662669	41.831236	61.281050
2081.867875	44.285028	61.286055
2080.902281	40.883717	61.291060
2080.196965	47.924996	61.296065
2079.683037	43.401725	61.301070
2079.437712	49.835403	61.306074
2078.832415	47.988608	61.311079
2078.015063	50.868618	61.316084
2077.184346	47.729763	61.321089
2076.710629	43.608554	61.326094
2076.265431	42.575317	61.331098
2075.344661	47.015622	61.336103
2074.908918	46.051849	61.341108
2074.060166	48.993616	61.346113
2073.024313	42.015782	61.351118
2071.962178	45.466088	61.356122
2071.687539	52.541528	61.361127
2071.936690	37.999909	61.366132
2070.566063	55.309751	61.371137
2069.789363	39.832551	61.376142
2068.853420	39.172095	61.381146
2068.218252	38.859733	61.386151
2067.701866	46.255818	61.391156
2067.270832	51.329633	61.396161
2066.961817	37.310271	61.401166
2066.038516	46.299046	61.406170
2065.001145	42.958019	61.411175
2064.956200	40.471927	61.416180
2064.344348	49.900147	61.421185
2064.055057	41.036020	61.426190
2063.490322	41.638180	61.431194
2061.737081	50.124718	61.436199
2060.539980	49.879460	61.441204
2060.268878	52.253302	61.446209
2060.557439	42.404887	61.451214
2059.657011	49.328897	61.456218
2058.396115	40.675741	61.461223
2057.735199	40.660790	61.466228
2057.021072	54.963980	61.471233
2056.793986	47.581822	61.476238
2056.093626	47.287694	61.481242
2055.340549	54.311329	61.486247
2055.014611	37.197427	61.491252
2054.282326	51.508227	61.496257
2053.757335	49.498878	61.501262
2053.327077	41.573363	61.506266
2052.603715	44.253953	61.511271
2051.409577	42.760823	61.516276
2050.169635	47.505688	61.521281
2050.297059	45.954209	61.526286
2049.336617	55.079779	61.531290
2048.697232	53.779312	61.536295
2047.973591	48.160198	61.541300
2047.064661	48.066336	61.546305
2047.123447	50.425671	61.551310
2046.698216	47.424328	61.556314
2045.652910	48.807681	61.561319
2045.287990	40.124301	61.566324
2044.392677	49.447696	61.571329
2043.883897	45.447181	61.576334
2043.147545	44.737710	61.581338
2041.855770	54.940917	61.586343
2041.494165	51.257674	61.591348
2040.685480	51.955328	61.596353
2040.077946	53.742306	61.601358
2039.671890	52.991453	61.606362
2038.946152	45.614321	61.611367
2038.229492	53.885893	61.616372
2037.725695	58.004561	61.621377
2037.521023	48.606595	61.626382
2036.788317	51.178284	61.631386
2035.873951	61.301886	61.636391
2034.830573	53.002944	61.641396
2033.679356	60.500584	61.646401
2033.528391	59.802289	61.651406
2033.182525	61.699130	61.656410
2032.599252	56.794988	61.661415
2031.941588	57.031847	61.666420
2031.247083	63.058204	61.671425
2030.699781	57.452895	61.676430
2030.088077	57.488489	61.681434
2029.262007	53.976739	61.686439
2028.296020	54.199454	61.691444
2027.482237	53.350885	61.696449
2026.719129	53.904111	61.701454
2026.058013	56.910732	61.706458
2025.641478	62.714770	61.711463
2025.189547	57.110097	61.716468
2024.497948	66.911334	61.721473
2024.499608	56.997266	61.726478
2024.081754	64.181390	61.731482
2023.270359	55.997025	61.736487
2022.262622	60.124713	61.741492
2021.076769	63.966062	61.746497
2020.513950	58.162940	61.751502
2019.993830	50.207535	61.756506
2018.756983	56.293951	61.761511
2018.303257	55.317271	61.766516
2017.643640	64.238197	61.771521
2017.360983	62.977314	61.776526
2016.356337	57.480870	61.781530
2015.385808	64.090375	61.786535
2014.956356	56.991870	61.791540
2014.285899	63.601057	61.796545
2014.080438	54.823767	61.801550
2013.818262	55.060939	61.806554
2013.016807	55.665988	61.811559
2012.863449	51.121772	61.816564
2011.397302	58.277521	61.821569
2010.606977	55.797769	61.826574
2009.931094	61.276320	61.831578
2009.439974	69.471895	61.836583
2009.053881	56.738193	61.841588
2007.939193	61.098911	61.846593
2007.456686	53.754145	61.851598
2006.445074	57.664828	61.856602
2005.486553	58.685906	61.861607
2005.231797	50.830315	61.866612
2004.361961	56.938910	61.871617
2003.963078	57.976820	61.876622
2003.819285	59.589270	61.881626
2003.016859	60.498838	61.886631
2002.555733	57.676669	61.891636
2001.544692	57.021848	61.896641
2000.758694	51.191867	61.901646
1999.741168	57.880586	61.906650
1999.377030	63.822184	61.911655
1999.187193	58.293401	61.916660
1998.149225	64.707028	61.921665
1997.849837	50.710588	61.926670
1996.979115	49.473662	61.931674
1995.837264	53.236281	61.936679
1995.467421	47.201472	61.941684
1994.491425	57.927027	61.946689
1994.003975	50.635091	61.951694
1993.582314	49.336351	61.956698
1993.015044	57.943777	61.961703
1992.958477	56.844136	61.966708
1991.450020	57.752230	61.971713
1990.786781	57.964752	61.976718
1990.066371	49.763596	61.981722
1989.271320	58.370908	61.986727
1989.018997	54.373851	61.991732
1988.367387	68.245291	61.996737
1988.197578	53.026609	62.001742
1986.931059	56.958835	62.006746
1986.055257	64.143899	62.011751
1985.517720	54.003967	62.016756
1984.883022	57.905293	62.021761
1984.418847	59.164887	62.026766
1984.240297	60.323949	62.031770
1983.014057	53.922014	62.036775
1982.294087	54.492060	62.041780
1980.999734	61.910724	62.046785
1980.751863	62.445258	62.051790
1980.208417	55.036052	62.056794
1979.326344	59.279430	62.061799
1979.488575	51.786598	62.066804
1978.295195	58.179954	62.071809
1978.142197	58.771971	62.076814
1977.448846	55.308559	62.081818
1976.069040	59.097920	62.086823
1975.640423	54.039143	62.091828
1974.986749	59.247661	62.096833
1974.338639	64.158823	62.101838
1974.062126	55.592308	62.106842
1973.368836	60.192087	62.111847
1972.442905	45.923729	62.116852
1971.475859	60.199270	62.121857
1970.812665	50.478273	62.126862
1970.402339	49.612989	62.131866
1969.662995	55.874348	62.136871
1969.387888	47.690827	62.141876
1968.740650	57.569394	62.146881
1967.835544	58.679780	62.151886
1966.664386	49.676526	62.156890
1966.081754	59.210516	62.161895
1965.769500	60.434958	62.166900
1965.331759	59.868925	62.171905
1965.006666	56.791774	62.176910
1964.581576	61.442024	62.181914
1963.159788	62.760589	62.186919
1962.677035	48.511773	62.191924
1961.744017	54.461669	62.196929
1961.293016	57.127436	62.201934
1960.740443	51.154756	62.206938
1959.451503	57.538056	62.211943
1958.951651	56.713793	62.216948
1958.041170	62.310022	62.221953
1957.833103	61.355860	62.226958
1957.438961	53.528711	62.231962
1956.707322	52.591429	62.236967
1956.371705	61.113202	62.241972
1955.649576	60.152331	62.246977
1954.812815	57.850285	62.251982
1954.118815	56.788753	62.256986
1953.026746	58.767787	62.261991
1952.889345	50.772148	62.266996
1951.717918	55.485678	62.272001
1950.878997	53.991401	62.277006
1950.092127	59.276263	62.282010
1949.832322	59.219743	62.287015
1949.320491	55.342737	62.292020
1948.481097	53.960502	62.297025
1947.916667	61.652826	62.302030
1947.722802	54.829974	62.307034
1946.953466	67.326828	62.312039
1946.162408	51.486877	62.317044
1945.011695	54.276337	62.322049
1944.223925	57.221078	62.327054
1944.314387	62.778267	62.332058
1943.310790	57.706689	62.337063
1943.259717	59.564628	62.342068
1942.400242	56.157562	62.347073
1941.602518	54.830217	62.352078
1940.665448	53.372024	62.357082
1939.736440	55.334639	62.362087
1939.594498	51.737972	62.367092
1938.884371	48.969539	62.372097
1938.354231	56.016156	62.377102
1937.619527	47.992336	62.382106
1936.649277	59.969131	62.387111
1936.298325	59.919197	62.392116
1935.989032	61.753471	62.397121
1935.512507	55.708798	62.402126
1934.129689	58.413681	62.407130
1933.468972	56.447982	62.412135
1933.271795	52.798581	62.417140
1932.069185	55.623095	62.422145
1930.812864	61.091302	62.427150
1930.263809	61.216325	62.432154
1929.827354	66.363562	62.437159
1929.518905	50.063794	62.442164
1928.866022	58.762092	62.447169
1928.127213	63.280796	62.452174
1928.105546	50.590985	62.457178
1927.151499	58.113344	62.462183
1926.176490	59.280574	62.467188
1925.343530	63.976656	62.472193
1924.774066	54.431609	62.477198
1924.269692	52.515212	62.482202
1923.363843	62.045326	62.487207
1923.590688	55.308657	62.492212
1922.392368	65.503388	62.497217
1921.561875	62.744604	62.502222
1920.913327	64.301569	62.507226
1920.120803	63.399194	62.512231
1919.929975	58.280599	62.517236
1919.108562	65.534319	62.522241
1918.052264	62.459714	62.527246
1917.275469	58.370882	62.532250
1916.525294	65.826188	62.537255
1916.382213	60.865597	62.542260
1915.938519	65.170290	62.547265
1915.534967	63.649484	62.552270
1915.037119	61.892906	62.557274
1913.767788	66.047970	62.562279
1912.911253	63.451023	62.567284
1912.338582	68.839092	62.572289
1911.896649	67.368535	62.577294
1911.321379	65.450778	62.582298
1909.951007	67.142843	62.587303
1909.506734	61.105670	62.592308
1908.807969	69.465899	62.597313
1908.531735	69.418299	62.602318
1908.445882	65.248161	62.607322
1907.097543	66.717526	62.612327
1906.264067	62.987790	62.617332
1905.454381	66.336580	62.622337
1904.888879	70.278980	62.627342
1904.929520	70.673097	62.632346
1904.249336	74.034446	62.637351
1903.413458	66.468251	62.642356
1901.770283	74.188344	62.647361
1901.501658	65.130139	62.652366
1901.213837	64.537161	62.657370
1900.470170	62.881115	62.662375
1899.953751	59.971548	62.667380
1899.719130	58.136912	62.672385
1898.427021	68.261385	62.677390
1897.690842	63.405997	62.682394
1897.284218	69.740714	62.687399
1897.118054	61.043148	62.692404
1895.638465	66.579935	62.697409
1894.705148	64.260122	62.702414
1894.055542	57.604252	62.707418
1893.419122	66.591692	62.712423
1893.437888	60.758560	62.717428
1892.808717	63.138801	62.722433
1892.596591	63.478429	62.727438
1891.995949	66.377705	62.732442
1890.589929	76.121291	62.737447
1890.303551	64.626288	62.742452
1889.567838	65.375483	62.747457
1888.440562	63.947508	62.752462
1887.563374	73.499896	62.757466
1886.854682	67.069455	62.762471
1886.418029	75.835944	62.767476
1886.148510	71.926785	62.772481
1885.512453	71.042158	62.777486
1885.041601	73.525004	62.782490
1883.984287	75.489086	62.787495
1883.314560	65.029535	62.792500
1882.765794	61.863326	62.797505
1882.079190	65.738222	62.802510
1881.352078	48.519317	62.807514
1880.120281	67.474868	62.812519
1879.797878	65.611590	62.817524
1879.158117	68.507619	62.822529
1878.641059	64.183590	62.827534
1878.708264	64.302244	62.832538
1877.625880	73.707437	62.837543
1877.169646	55.953494	62.842548
1876.499966	67.338522	62.847553
1875.635556	65.135512	62.852558
1874.411301	60.866996	62.857562
1873.613902	70.859316	62.862567
1872.927526	68.205403	62.867572
1872.295737	70.313246	62.872577
1872.122714	71.427281	62.877582
1871.650282	64.500427	62.882586
1871.062187	64.138060	62.887591
1870.912849	63.729685	62.892596
1869.809828	70.753733	62.897601
1868.729082	64.656769	62.902606
1868.319321	62.747439	62.907610
1867.295463	73.554755	62.912615
1866.904936	65.000051	62.917620
1865.682574	67.971238	62.922625
1865.027034	71.754472	62.927630
1864.826214	65.019467	62.932634
1864.153903	72.355188	62.937639
1863.909127	68.500453	62.942644
1863.271209	68.710564	62.947649
1862.276793	69.321065	62.952654
1861.628583	67.645143	62.957658
1860.726718	72.350608	62.962663
1860.353474	69.495588	62.967668
1859.645895	65.954042	62.972673
1858.687755	62.863877	62.977678
1858.093424	58.911680	62.982682
1857.261905	72.634290	62.987687
1856.763121	61.978869	62.992692
1856.559569	71.895826	62.997697
1855.834379	68.828600	63.002702
1855.007035	61.251610	63.007706
1853.937296	68.629933	63.012711
1853.555360	63.355604	63.017716
1853.032541	62.276381	63.022721
1852.614769	65.700155	63.027726
1852.036111	68.023499	63.032730
1850.622738	67.003676	63.037735
1850.120963	64.664245	63.042740
1849.609287	66.708864	63.047745
1849.192058	66.827165	63.052750
1848.869840	59.165242	63.057754
1847.630618	65.424000	63.062759
1846.750076	66.063735	63.067764
1846.583974	62.358943	63.072769
1845.910670	71.325440	63.077774
1845.421488	69.293101	63.082778
1843.837769	66.623982	63.087783
1843.463116	58.475209	63.092788
1843.088439	62.231195	63.097793
1842.535074	71.262229	63.102798
1842.368857	63.991862	63.107802
1841.048035	64.674700	63.112807
1840.173917	62.511092	63.117812
1839.411650	55.783241	63.122817
1838.778332	66.675208	63.127822
1839.282562	49.207185	63.132826
1838.194818	57.807385	63.137831
1836.976590	62.999916	63.142836
1836.264194	65.680399	63.147841
1835.392345	68.244272	63.152846
1835.375146	63.178543	63.157850
1834.520432	58.524932	63.162855
1833.968740	61.947894	63.167860
1833.243539	72.184232	63.172865
1832.475630	65.315346	63.177870
1832.302007	56.792447	63.182874
1831.262026	67.428859	63.187879
1830.375411	61.181238	63.192884
1829.326767	57.480966	63.197889
1828.972459	64.157472	63.202894
1828.819294	62.119092	63.207898
1827.948338	63.395995	63.212903
1827.793115	65.101733	63.217908
1826.408940	62.044538	63.222913
1825.452701	62.029230	63.227918
1825.468396	56.466258	63.232922
1824.690498	71.665889	63.237927
1824.194468	63.255686	63.242932
1823.197551	68.062989	63.247937
1822.625332	64.555156	63.252942
1822.394690	60.627220	63.257946
1821.441756	60.641351	63.262951
1820.543146	57.669487	63.267956
1819.775977	62.897636	63.272961
1819.105315	60.553491	63.277966
1818.866009	60.394377	63.282970
1818.081353	65.901279	63.287975
1817.585164	64.638058	63.292980
1816.748666	66.891962	63.297985
1815.462505	61.625606	63.302990
1815.485440	61.328653	63.307994
1814.911172	64.718934	63.312999
1814.180607	63.242188	63.318004
1813.470960	70.046089	63.323009
1812.347106	59.959888	63.328014
1811.817205	57.345805	63.333018
1811.096576	63.320370	63.338023
1811.430918	62.060885	63.343028
1810.213011	55.867460	63.348033
1809.488426	60.978459	63.353038
1809.073916	62.148191	63.358042
1808.058318	69.188340	63.363047
1807.057436	56.439569	63.368052
1806.132435	66.739175	63.373057
1805.929634	68.129186	63.378062
1805.323849	64.375944	63.383066
1804.779342	82.683060	63.388071
1804.675986	68.285719	63.393076
1803.810816	69.134345	63.398081
1802.850213	64.092270	63.403086
1802.209087	66.447621	63.408090
1801.725379	73.830676	63.413095
1800.820050	70.609141	63.418100
1799.684258	57.530126	63.423105
1798.838007	69.722242	63.428110
1798.692301	59.553259	63.433114
1798.376251	63.325172	63.438119
1798.168663	54.500159	63.443124
1797.405907	60.090321	63.448129
1796.495849	64.699329	63.453134
1796.017586	57.617302	63.458138
1794.552800	61.642602	63.463143
1793.572303	60.610841	63.468148
1793.059763	54.901516	63.473153
1792.510104	66.097179	63.478158
1792.269556	59.144563	63.483162
1791.844329	66.012112	63.488167
1791.558847	65.951800	63.493172
1790.467294	63.379603	63.498177
1789.457137	66.742914	63.503182
1789.003286	63.919632	63.508186
1788.381083	62.047207	63.513191
1788.089369	62.074620	63.518196
1786.811749	62.985596	63.523201
1785.913953	55.361477	63.528206
1785.910815	60.220711	63.533210
1785.231535	59.934347	63.538215
1784.651361	54.972222	63.543220
1783.562217	60.691492	63.548225
1782.494293	64.243756	63.553230
1782.280508	61.096916	63.558234
1781.872357	65.236704	63.563239
1781.427517	67.526194	63.568244
1780.532332	53.500633	63.573249
1779.551554	58.032564	63.578254
1779.142095	56.050660	63.583258
1778.407786	56.774430	63.588263
1777.514663	63.377231	63.593268
1776.831827	63.544032	63.598273
1776.473746	64.266403	63.603278
1775.955236	53.959508	63.608282
1775.300793	57.942862	63.613287
1774.519707	60.269981	63.618292
1773.495895	65.761257	63.623297
1772.598646	69.295882	63.628302
1772.557542	64.878944	63.633306
1771.567500	67.922090	63.638311
1771.282908	62.827866	63.643316
1770.172538	60.280745	63.648321
1769.103879	70.713567	63.653326
1768.953239	64.320702	63.658330
1768.508106	60.247059	63.663335
1768.278010	59.995022	63.668340
1768.148726	71.814655	63.673345
1766.583438	67.474194	63.678350
1766.323438	61.343132	63.683354
1765.385979	58.446846	63.688359
1764.523281	60.900473	63.693364
1763.822011	69.112888	63.698369
1763.084294	66.378850	63.703374
1762.503318	57.147927	63.708378
1761.598698	65.711189	63.713383
1760.721925	58.310827	63.718388
1760.123573	55.445845	63.723393
1759.582502	63.180217	63.728398
1759.262975	51.748869	63.733402
1758.588703	69.035761	63.738407
1758.663569	55.589451	63.743412
1757.572886	58.318991	63.748417
1756.322701	63.641214	63.753422
1756.417044	58.764363	63.758426
1755.364132	62.970283	63.763431
1754.288230	65.814176	63.768436
1753.527671	65.927093	63.773441
1752.922313	73.097654	63.778446
1752.848842	59.051988	63.783450
1752.125362	71.661444	63.788455
1751.757667	55.207125	63.793460
1750.609526	59.554329	63.798465
1749.947028	60.933771	63.803470
1749.456704	57.379835	63.808474
1748.891679	68.385550	63.813479
1748.013213	59.922566	63.818484
1747.067843	62.326249	63.823489
1745.915718	67.771679	63.828494
1746.046202	56.188432	63.833498
1745.215197	70.097063	63.838503
1744.742552	60.380571	63.843508
1744.694894	70.274341	63.848513
1743.309725	69.306869	63.853518
1742.900829	61.633502	63.858522
1741.898978	62.902836	63.863527
1741.712017	60.401462	63.868532
1740.577923	63.560540	63.873537
1739.720816	71.498081	63.878542
1739.534019	61.264669	63.883546
1738.843873	70.281166	63.888551
1738.375176	55.863026	63.893556
1737.381599	60.871680	63.898561
1736.481710	66.873156	63.903566
1736.205410	58.060642	63.908570
1735.928516	64.504080	63.913575
1735.090545	57.220572	63.918580
1733.956860	66.080426	63.923585
1733.395303	68.800057	63.928590
1733.153892	59.562521	63.933594
1732.239060	65.776112	63.938599
1731.289447	54.168870	63.943604
1730.628636	58.743040	63.948609
1729.998492	64.291655	63.953614
1729.740929	52.074591	63.958618
1729.263357	65.504449	63.963623
1728.239873	65.365813	63.968628
1727.502485	70.523022	63.973633
1726.522855	73.861007	63.978638
1726.070013	61.070962	63.983642
1725.931600	64.932941	63.988647
1724.801082	65.356947	63.993652
1724.227479	60.169859	63.998657
1723.536867	58.768799	64.003662
1723.390566	63.975631	64.008666
1722.096883	58.885568	64.013671
1721.142458	65.904987	64.018676
1721.297102	65.115593	64.023681
1720.362275	64.292655	64.028686
1720.127714	53.447078	64.033690
1718.858082	61.888546	64.038695
1718.198056	65.360277	64.043700
1717.613577	63.585959	64.048705
1716.987867	70.614674	64.053710
1716.252833	62.931611	64.058714
1715.082666	71.122315	64.063719
1714.799321	64.310553	64.068724
1714.383623	61.449687	64.073729
1713.899153	67.932405	64.078734
1713.672931	58.823351	64.083738
1712.414436	63.580771	64.088743
1711.462797	68.347802	64.093748
1711.518783	59.137152	64.098753
1710.228646	66.310825	64.103758
1709.194471	56.989474	64.108762
1708.727007	67.061885	64.113767
1708.516893	60.393039	64.118772
1708.315272	57.081846	64.123777
1707.248275	67.558576	64.128782
1706.398741	55.583778	64.133786
1705.457018	69.099982	64.138791
1705.231471	65.852513	64.143796
1704.806891	69.002990	64.148801
1703.703441	74.219928	64.153806
1703.093679	70.905750	64.158810
1702.258343	69.906161	64.163815
1701.907533	64.261055	64.168820
1701.518549	59.046226	64.173825
1700.272983	68.712362	64.178830
1699.939352	60.134471	64.183834
1699.016207	70.525277	64.188839
1698.601761	72.076649	64.193844
1697.840624	62.902747	64.198849
1696.747064	75.678233	64.203854
1695.869070	71.976143	64.208858
1695.621458	74.105005	64.213863
1695.142772	78.782727	64.218868
1694.870623	58.810737	64.223873
1693.900455	71.233874	64.228878
1693.648383	58.285792	64.233882
1692.454903	64.013784	64.238887
1691.920487	58.926140	64.243892
1691.843714	54.926472	64.248897
1690.472418	65.531968	64.253902
1689.976583	55.661479	64.258906
1689.270020	56.838194	64.263911
1688.389829	69.013644	64.268916
1687.684173	57.597911	64.273921
1686.388002	63.004740	64.278926
1686.554030	59.885892	64.283930
1685.820198	67.464809	64.288935
1685.592879	65.077086	64.293940
1685.247187	56.731358	64.298945
1683.927685	63.204789	64.303950
1683.406801	56.380304	64.308954
1682.944483	71.884649	64.313959
1681.824172	57.353984	64.318964
1680.965473	56.999951	64.323969
1680.350179	64.085363	64.328974
1679.952794	51.098870	64.333978
1679.456843	66.416158	64.338983
1678.948411	66.331348	64.343988
1678.067935	65.307398	64.348993
1677.096423	67.459785	64.353998
1676.899414	64.091089	64.359002
1676.068410	66.739988	64.364007
1675.701235	71.638124	64.369012
1674.431732	59.886172	64.374017
1673.940272	64.059706	64.379022
1673.331086	65.055373	64.384026
1673.163772	64.118418	64.389031
1672.322383	63.818410	64.394036
1671.393408	57.728976	64.399041
1670.814479	70.917893	64.404046
1670.413935	63.383568	64.409050
1668.753810	62.724750	64.414055
1667.984349	64.531221	64.419060
1667.782285	65.097932	64.424065
1667.238741	63.998386	64.429070
1666.844246	64.158837	64.434074
1666.382118	59.488659	64.439079
1666.081917	63.390532	64.444084
1665.538234	59.392493	64.449089
1664.575648	57.506360	64.454094
1663.985479	50.959402	64.459098
1662.261244	62.705944	64.464103
1661.717147	57.485802	64.469108
1661.559653	54.167605	64.474113
1660.993174	65.395913	64.479118
1660.609168	54.055258	64.484122
1659.436645	61.506741	64.489127
1658.702567	61.557130	64.494132
1658.587405	53.991672	64.499137
1657.377066	61.373467	64.504142
1656.741829	55.783018	64.509146
1655.801820	63.446732	64.514151
1655.141195	63.270983	64.519156
1654.898385	65.091570	64.524161
1654.427576	61.156075	64.529166
1654.275284	61.820539	64.534170
1653.071696	68.385961	64.539175
1651.879212	63.756111	64.544180
1651.869945	59.811955	64.549185
1651.067333	63.328428	64.554190
1650.224712	66.338735	64.559194
1649.562908	68.612247	64.564199
1649.058826	65.839552	64.569204
1648.654838	64.862924	64.574209
1647.025778	78.024702	64.579214
1646.288111	62.398757	64.584218
1645.876148	74.141859	64.589223
1645.481718	56.201561	64.594228
1645.289036	63.185147	64.599233
1645.027655	66.345976	64.604238
1644.053872	49.197909	64.609242
1643.049828	57.948883	64.614247
1642.481202	65.053696	64.619252
1641.845474	64.050804	64.624257
1640.373586	66.233807	64.629262
1639.895793	53.618075	64.634266
1639.636805	68.137611	64.639271
1638.941909	70.100984	64.644276
1639.004755	70.419026	64.649281
1637.792334	69.976117	64.654286
1636.887705	64.762790	64.659290
1636.298867	70.718035	64.664295
1635.878982	70.805252	64.669300
1635.387570	62.629342	64.674305
1634.491442	74.498248	64.679310
1633.835915	64.252583	64.684314
1633.421615	71.481121	64.689319
1632.574550	64.541304	64.694324
1631.519159	51.416502	64.699329
1630.878088	65.443210	64.704334
1630.242765	55.172265	64.709338
1630.181434	58.389624	64.714343
1629.265482	67.910378	64.719348
1628.295488	67.638701	64.724353
1627.625436	66.969280	64.729358
1627.392103	60.737809	64.734362
1626.528278	63.653717	64.739367
1625.669445	64.003063	64.744372
1625.149459	59.258505	64.749377
1624.312734	71.652575	64.754382
1623.948972	64.093493	64.759386
1623.188655	68.625148	64.764391
1622.788785	64.637388	64.769396
1621.720418	59.435889	64.774401
1621.070249	61.117763	64.779406
1620.357003	64.826633	64.784410
1620.219841	68.190086	64.789415
1619.675151	63.487301	64.794420
1619.031202	58.254647	64.799425
1618.053864	61.731077	64.804430
1617.446335	55.584290	64.809434
1616.302729	57.172665	64.814439
1615.811244	54.823767	64.819444
1615.115063	55.790689	64.824449
1614.795187	65.341328	64.829454
1614.613837	58.958094	64.834458
1613.466599	51.741120	64.839463
1612.618111	59.607928	64.844468
1611.966459	55.493013	64.849473
1610.745979	65.737105	64.854478
1610.136737	56.621113	64.859482
1609.960434	62.554974	64.864487
1609.008230	65.459697	64.869492
1608.638073	59.543288	64.874497
1608.407282	65.720778	64.879502
1607.846641	65.298915	64.884506
1606.631695	66.586385	64.889511
1606.062361	61.885942	64.894516
1605.904052	63.636335	64.899521
1604.451380	64.701371	64.904526
1603.936517	62.914444	64.909530
1603.050000	60.514765	64.914535
1602.794397	61.272918	64.919540
1602.373707	57.115002	64.924545
1601.100765	70.269103	64.929550
1600.419915	66.198252	64.934554
1599.705875	66.275437	64.939559
1599.567700	69.957604	64.944564
1599.523145	65.236866	64.949569
1598.205836	70.822141	64.954574
1597.837275	65.023753	64.959578
1596.691552	66.938912	64.964583
1596.177371	73.514678	64.969588
1595.180893	63.200192	64.974593
1594.364449	66.327784	64.979598
1593.923990	64.101673	64.984602
1593.544685	62.752116	64.989607
1593.061896	66.675120	64.994612
1592.947438	54.384885	64.999617
1591.331207	66.521173	65.004622
1590.749802	58.376923	65.009626
1590.408757	65.789370	65.014631
1589.712436	64.036007	65.019636
1588.478614	68.592438	65.024641
1587.786914	66.087692	65.029646
1587.381629	58.609338	65.034650
1586.854644	64.682497	65.039655
1586.409896	67.118662	65.044660
1585.711807	59.344621	65.049665
1584.497628	65.366112	65.054670
1583.973583	56.400600	65.059674
1583.734657	62.492648	65.064679
1583.070548	64.358100	65.069684
1582.290658	67.697513	65.074689
1581.376655	64.748684	65.079694
1580.579488	57.493449	65.084698
1580.590997	56.371967	65.089703
1580.016207	58.224805	65.094708
1579.180305	57.296313	65.099713
1578.122890	60.309227	65.104718
1577.828802	62.707261	65.109722
1576.776697	61.431489	65.114727
1575.849353	61.916319	65.119732
1575.602646	51.761850	65.124737
1574.883391	61.175666	65.129742
1574.739901	55.488185	65.134746
1573.859135	60.860601	65.139751
1573.295463	71.470295	65.144756
1572.589010	61.503988	65.149761
1571.938364	66.740492	65.154766
1571.488858	56.504700	65.159770
1570.389326	58.579690	65.164775
1569.973509	62.145117	65.169780
1568.968079	53.204057	65.174785
1568.062429	58.302876	65.179790
1567.723143	57.519414	65.184794
1567.358894	67.752058	65.189799
1566.481523	61.189255	65.194804
1565.598323	60.974775	65.199809
1564.261093	59.810546	65.204814
1564.205906	50.642810	65.209818
1563.652986	51.252659	65.214823
1563.196623	61.421086	65.219828
1562.846490	55.271266	65.224833
1561.850444	54.630006	65.229838
1560.890758	46.288829	65.234842
1560.683405	51.978454	65.239847
1560.156104	54.314194	65.244852
1559.107627	52.724032	65.249857
1558.229532	55.440371	65.254862
1557.726251	61.293719	65.259866
1557.241724	62.420996	65.264871
1556.554139	62.639073	65.269876
1555.825796	56.043135	65.274881
1554.922308	59.238185	65.279886
1554.389423	61.962755	65.284890
1554.348687	57.711359	65.289895
1553.409221	66.808503	65.294900
1552.597045	56.349638	65.299905
1551.703822	67.710304	65.304910
1551.160814	58.985939	65.309914
1550.884151	63.740387	65.314919
1549.804441	56.591563	65.319924
1549.457171	60.489884	65.324929
1548.524751	62.700760	65.329934
1548.017805	63.560358	65.334938
1546.859341	59.202709	65.339943
1546.108998	66.691234	65.344948
1545.828616	57.149261	65.349953
1545.132717	61.943516	65.354958
1544.831299	60.589476	65.359962
1544.698646	52.865959	65.364967
1543.297373	59.896505	65.369972
1542.714472	53.072453	65.374977
1542.436693	58.918355	65.379982
1540.963323	56.790152	65.384986
1540.227984	55.929274	65.389991
1539.568289	60.760356	65.394996
1539.509311	51.120127	65.400001
1538.860795	60.212040	65.405006
1538.262366	55.749636	65.410010
1537.122559	54.408967	65.415015
1536.281574	60.315980	65.420020
1535.977686	49.643891	65.425025
1535.657032	62.504757	65.430030
1534.907935	52.613059	65.435034
1534.153551	58.840632	65.440039
1533.390996	55.639094	65.445044
1533.087832	45.126171	65.450049
1531.965512	56.617856	65.455054
1531.067577	52.250357	65.460058
1530.568306	55.911052	65.465063
1529.917498	54.823851	65.470068
1529.669615	51.561032	65.475073
1528.855097	56.697422	65.480078
1527.659915	55.231513	65.485082
1527.496494	50.523365	65.490087
1527.243045	60.063447	65.495092
1526.415164	48.072682	65.500097
1525.378523	55.102063	65.505102
1524.579783	51.327523	65.510106
1524.471753	54.940241	65.515111
1523.606377	58.651229	65.520116
1523.138210	53.863771	65.525121
1522.015666	63.321181	65.530126
1521.665845	59.967325	65.535130
1520.995574	51.037688	65.540135
1519.723066	62.129036	65.545140
1519.680189	50.543398	65.550145
1518.994956	64.920917	65.555150
1518.448363	59.325885	65.560154
1517.528757	53.645047	65.565159
1516.384032	63.744666	65.570164
1516.096713	51.092400	65.575169
1515.759447	65.509245	65.580174
1515.293242	61.527317	65.585178
1514.436448	57.304677	65.590183
1513.651356	57.249671	65.595188
1513.272026	52.520640	65.600193
1512.047783	55.399236	65.605198
1510.963047	59.427368	65.610202
1510.599149	56.880017	65.615207
1509.951336	60.740944	65.620212
1510.066373	51.691246	65.625217
1509.586832	51.742231	65.630222
1508.165184	54.641159	65.635226
1507.762496	64.761637	65.640231
1506.721424	56.897048	65.645236
1506.493319	64.234779	65.650241
1505.415927	60.938198	65.655246
1504.633288	57.864443	65.660250
1504.319695	58.262804	65.665255
1503.165908	67.297823	65.670260
1503.235945	60.368441	65.675265
1502.957641	60.893661	65.680270
1501.610844	58.288039	65.685274
1501.334224	56.889062	65.690279
1500.588170	65.717357	65.695284
1499.235607	67.520344	65.700289
1498.291029	69.952372	65.705294
1498.040062	58.360375	65.710298
1497.507392	61.078612	65.715303
1496.727165	68.748520	65.720308
1497.012378	59.816857	65.725313
1496.132746	63.569545	65.730318
1495.361655	59.901009	65.735322
1495.014909	63.827638	65.740327
1493.792823	64.297835	65.745332
1492.856674	55.260644	65.750337
1491.596140	61.672746	65.755342
1491.593473	52.111885	65.760346
1491.317389	53.669682	65.765351
1490.742953	50.543922	65.770356
1490.472185	50.903939	65.775361
1489.146192	63.686448	65.780366
1488.358432	60.408504	65.785370
1487.910048	56.977275	65.790375
1486.593201	54.691762	65.795380
1486.223932	44.176740	65.800385
1485.501215	60.756962	65.805390
1485.238982	58.792715	65.810394
1485.078876	54.744804	65.815399
1484.167369	51.450257	65.820404
1483.363336	51.062372	65.825409
1482.561363	61.889717	65.830414
1481.943473	63.596456	65.835418
1480.773054	56.980911	65.840423
1479.943999	61.512484	65.845428
1479.684612	58.366619	65.850433
1478.816013	54.909133	65.855438
1478.656182	64.786008	65.860442
1478.368765	59.253879	65.865447
1477.756549	55.506483	65.870452
1476.976156	54.244343	65.875457
1476.012372	61.702145	65.880462
1475.352357	53.759666	65.885466
1474.773179	60.408850	65.890471
1473.844606	60.643171	65.895476
1473.712308	57.469224	65.900481
1472.698047	61.694334	65.905486
1471.728487	59.257438	65.910490
1471.602319	58.014331	65.915495
1470.924444	62.211212	65.920500
1469.940547	55.969740	65.925505
1468.861091	54.351423	65.930510
1468.076229	65.541916	65.935514
1468.199952	48.266834	65.940519
1467.717671	60.158304	65.945524
1467.130191	56.381748	65.950529
1466.009119	63.025592	65.955534
1465.439515	59.585247	65.960538
1464.736259	51.197049	65.965543
1463.438416	57.821676	65.970548
1462.923608	51.739052	65.975553
1462.139115	53.697782	65.980558
1461.831635	61.171132	65.985562
1461.802015	51.333854	65.990567
1461.271026	59.184933	65.995572
1460.619192	61.378053	66.000577
1459.474348	59.263918	66.005582
1458.799733	62.969840	66.010586
1458.222721	62.075938	66.015591
1456.854348	66.015127	66.020596
1456.644794	62.183238	66.025601
1455.585650	58.595191	66.030606
1455.401367	62.574852	66.035610
1455.211932	66.263590	66.040615
1454.459652	68.067390	66.045620
1453.643237	57.415271	66.050625
1453.002773	64.859543	66.055630
1452.228138	56.324992	66.060634
1451.301693	51.689237	66.065639
1450.562524	54.216368	66.070644
1450.112944	49.664100	66.075649
1449.695600	57.317340	66.080654
1449.076070	48.643023	66.085658
1448.055214	51.911954	66.090663
1447.226419	58.204990	66.095668
1447.153776	58.743262	66.100673
1446.362222	55.336622	66.105678
1445.885481	53.959997	66.110682
1445.141353	54.699612	66.115687
1444.096103	55.107032	66.120692
1443.617646	55.719265	66.125697
1442.328499	50.704335	66.130702
1441.792092	54.416678	66.135706
1441.449408	52.384798	66.140711
1441.014770	56.380594	66.145716
1440.489707	52.877984	66.150721
1439.976868	54.525456	66.155726
1438.990306	57.632819	66.160730
1438.243269	49.754650	66.165735
1437.705006	54.432406	66.170740
1437.352385	56.259422	66.175745
1435.967823	52.018193	66.180750
1435.206784	57.904638	66.185754
1435.247931	54.215839	66.190759
1434.595379	55.185334	66.195764
1433.474782	51.529794	66.200769
1432.676559	53.982736	66.205774
1432.035095	51.249276	66.210778
1432.052989	44.173648	66.215783
1430.906236	59.625914	66.220788
1430.232064	46.670877	66.225793
1429.321809	55.091606	66.230798
1428.819070	60.181621	66.235802
1428.840923	50.845534	66.240807
1428.417217	55.151838	66.245812
1427.491686	52.480877	66.250817
1426.660022	60.808692	66.255822
1425.641229	59.327411	66.260826
1425.060176	54.796044	66.265831
1424.180808	58.818375	66.270836
1423.836869	50.034028	66.275841
1423.547891	61.361754	66.280846
1422.491640	52.518733	66.285850
1421.866658	53.531160	66.290855
1421.056972	59.750202	66.295860
1420.750388	62.885113	66.300865
1419.749581	59.749867	66.305870
1418.657137	68.421921	66.310874
1418.768606	54.708055	66.315879
1418.067837	62.833714	66.320884
1417.091838	60.751109	66.325889
1416.206130	53.902684	66.330894
1415.419969	62.515013	66.335898
1415.357768	56.598583	66.340903
1414.631616	62.104167	66.345908
1413.897101	52.263817	66.350913
1412.971086	56.695697	66.355918
1412.299599	59.730911	66.360922
1412.409564	42.685117	66.365927
1411.159152	57.254980	66.370932
1410.106956	52.372719	66.375937
1409.655138	50.159490	66.380942
1409.304237	58.827215	66.385946
1408.859245	58.109464	66.390951
1407.913302	57.911320	66.395956
1407.257525	47.766717	66.400961
1406.622610	55.211686	66.405966
1405.948305	53.842817	66.410970
1405.414691	61.624933	66.415975
1404.637833	68.685608	66.420980
1404.004710	55.375534	66.425985
1403.375305	55.740526	66.430990
1402.656460	61.476768	66.435994
1401.721758	51.781786	66.440999
1400.528972	64.491115	66.446004
1400.548761	58.276218	66.451009
1400.190188	60.542588	66.456014
1399.428533	62.046688	66.461018
1399.425418	59.401006	66.466023
1398.043712	63.845402	66.471028
1397.552663	61.975886	66.476033
1396.426818	55.507847	66.481038
1395.643873	63.146667	66.486042
1395.120757	57.571592	66.491047
1394.579634	61.224768	66.496052
1394.401772	54.348993	66.501057
1393.653529	53.013959	66.506062
1392.393271	56.596939	66.511066
1391.870579	49.774403	66.516071
1391.373266	54.316343	66.521076
1391.062165	57.541862	66.526081
1390.289537	61.424232	66.531086
1389.322657	60.759480	66.536090
1388.868120	56.540756	66.541095
1388.253694	64.821434	66.546100
1387.339036	57.279015	66.551105
1386.396118	62.678710	66.556110
1385.697792	62.983697	66.561114
1385.482048	51.879729	66.566119
1384.828545	56.503271	66.571124
1384.608345	54.644322	66.576129
1383.569330	56.239825	66.581134
1382.481734	56.739158	66.586138
1382.173023	54.504763	66.591143
1382.009869	63.347656	66.596148
1380.545431	48.953885	66.601153
1380.447040	52.443642	66.606158
1379.575618	45.466807	66.611162
1378.837520	57.518796	66.616167
1377.384882	57.670874	66.621172
1377.282684	46.386432	66.626177
1376.948907	54.753383	66.631182
1376.627010	59.442489	66.636186
1376.111689	55.861072	66.641191
1374.627889	63.423646	66.646196
1374.213808	50.277469	66.651201
1373.938107	52.221578	66.656206
1373.130580	56.202541	66.661210
1372.282875	53.826742	66.666215
1371.254165	62.980696	66.671220
1370.801544	50.966617	66.676225
1370.633341	51.291417	66.681230
1369.438670	50.440529	66.686234
1368.791202	52.257652	66.691239
1367.924653	56.683248	66.696244
1367.565572	52.994993	66.701249
1367.351429	48.848451	66.706254
1366.256333	60.275937	66.711258
1365.938957	57.528822	66.716263
1365.261147	59.273498	66.721268
1364.217798	50.218717	66.726273
1363.319816	50.642184	66.731278
1362.500340	57.255465	66.736282
1362.141233	49.892834	66.741287
1361.732673	62.054872	66.746292
1361.345990	59.124806	66.751297
1360.650445	61.627680	66.756302
1359.704962	60.596830	66.761306
1359.487157	55.168777	66.766311
1358.166003	58.720452	66.771316
1357.237723	61.531567	66.776321
1356.686734	60.430120	66.781326
1356.486092	57.016307	66.786330
1356.271492	54.208701	66.791335
1354.916553	58.573166	66.796340
1354.452400	56.019702	66.801345
1353.915382	60.534845	66.806350
1353.294913	69.483558	66.811354
1352.349448	59.162664	66.816359
1351.141846	65.686263	66.821364
1350.893220	62.157073	66.826369
1350.664320	61.110082	66.831374
1350.086450	55.958472	66.836378
1349.158523	53.956565	66.841383
1348.099369	65.293189	66.846388
1347.734332	54.522050	66.851393
1347.759424	56.448306	66.856398
1346.595003	61.720797	66.861402
1345.964280	52.018518	66.866407
1345.075096	53.601255	66.871412
1344.565350	56.686466	66.876417
1343.900582	58.742894	66.881422
1342.574970	58.688713	66.886426
1342.182167	49.549446	66.891431
1341.732741	57.113175	66.896436
1341.654187	57.974094	66.901441
1340.886493	59.767759	66.906446
1339.925147	60.564015	66.911450
1339.503764	56.147639	66.916455
1338.571414	65.309940	66.921460
1337.621660	59.769590	66.926465
1336.528824	65.007050	66.931470
1335.936038	58.889543	66.936474
1336.042865	46.518450	66.941479
1334.973623	61.463248	66.946484
1335.094533	54.516327	66.951489
1334.650817	51.593758	66.956494
1333.370225	55.657824	66.961498
1332.914209	55.820221	66.966503
1331.814673	62.550578	66.971508
1331.209516	59.647366	66.976513
1330.849223	60.428495	66.981518
1330.134155	60.371874	66.986522
1329.435985	49.656860	66.991527
1328.210961	59.845000	66.996532
1327.419254	58.920605	67.001537
1327.201170	54.612263	67.006542
1326.964339	53.815700	67.011546
1326.654528	60.278576	67.016551
1325.230226	63.116520	67.021556
1324.707854	63.033997	67.026561
1324.073049	65.267020	67.031566
1323.502110	59.112927	67.036570
1322.757398	57.974477	67.041575
1321.927117	67.618885	67.046580
1321.185315	55.860532	67.051585
1321.050217	55.904100	67.056590
1319.744525	56.485443	67.061594
1319.147792	52.721438	67.066599
1318.457238	53.577153	67.071604
1318.304255	53.339706	67.076609
1317.875712	49.290336	67.081614
1316.376972	55.516449	67.086618
1316.101428	53.035511	67.091623
1315.136771	67.815456	67.096628
1315.036969	52.974529	67.101633
1314.489880	49.946971	67.106638
1313.175095	61.286396	67.111642
1312.607436	54.586149	67.116647
1311.977433	55.225653	67.121652
1311.572266	48.147906	67.126657
1310.490759	53.949710	67.131662
1309.581783	56.609534	67.136666
1309.463511	46.111422	67.141671
1309.000222	52.431537	67.146676
1308.566122	49.376554	67.151681
1307.900427	49.360976	67.156686
1306.720131	58.021796	67.161690
1306.516021	40.680596	67.166695
1305.806077	51.094357	67.171700
1304.927997	53.036472	67.176705
1304.067143	52.534672	67.181710
1303.493884	57.486102	67.186714
1303.058985	43.223602	67.191719
1301.814512	51.486184	67.196724
1300.766105	47.696225	67.201729
1300.888051	55.315772	67.206734
1300.290785	58.703495	67.211738
1300.278740	55.280204	67.216743
1298.891980	65.109289	67.221748
1298.622027	62.297872	67.226753
1298.202260	53.131361	67.231758
1296.496052	59.158655	67.236762
1295.964189	50.593455	67.241767
1295.239606	53.399011	67.246772
1294.963575	55.451991	67.251777
1294.489799	50.354813	67.256782
1293.757882	56.194082	67.261786
1293.130868	54.298897	67.266791
1292.142210	55.900622	67.271796
1291.692934	59.118156	67.276801
1291.336664	44.622379	67.281806
1289.957224	49.714605	67.286810
1289.495887	51.927939	67.291815
1289.030024	61.003464	67.296820
1288.624523	52.042851	67.301825
1288.076333	55.817019	67.306830
1286.842297	60.286876	67.311834
1286.334853	50.866223	67.316839
1285.496343	57.745907	67.321844
1285.161727	57.130479	67.326849
1284.438078	48.026485	67.331854
1283.545162	50.871425	67.336858
1283.509734	50.525401	67.341863
1282.918739	42.032691	67.346868
1281.778693	52.864935	67.351873
1281.109832	42.280906	67.356878
1280.488295	53.327181	67.361882
1280.205930	43.866015	67.366887
1278.753355	54.785801	67.371892
1278.167141	50.280528	67.376897
1277.672779	48.462030	67.381902
1277.152699	52.637015	67.386906
1277.029944	42.131739	67.391911
1275.722295	50.027477	67.396916
1275.004673	48.041046	67.401921
1274.743458	42.015927	67.406926
1273.603993	52.065896	67.411930
1272.826074	41.912382	67.416935
1272.138164	45.946891	67.421940
1271.519199	52.531464	67.426945
1271.261923	43.657681	67.431950
1270.777441	43.081855	67.436954
1269.943853	43.887784	67.441959
1269.266183	43.626534	67.446964
1268.499191	42.460104	67.451969
1268.232809	29.350419	67.456974
1267.072196	49.748770	67.461978
1266.626332	39.829472	67.466983
1266.154855	46.947269	67.471988
1265.248267	43.931154	67.476993
1264.350511	43.094607	67.481998
1263.537139	46.920405	67.487002
1263.244664	34.168111	67.492007
1262.720047	45.298320	67.497012
1262.233331	41.308678	67.502017
1261.421725	46.209699	67.507022
1260.504009	40.815686	67.512026
1260.343483	36.550246	67.517031
1259.586313	44.214951	67.522036
1258.329533	39.354257	67.527041
1257.843947	41.762265	67.532046
1257.309590	45.907981	67.537050
1256.819004	40.345124	67.542055
1255.525530	53.173005	67.547060
1254.982530	44.300503	67.552065
1254.421184	45.809061	67.557070
1253.976260	50.079333	67.562074
1254.074224	44.206842	67.567079
1252.821360	36.596844	67.572084
1251.937812	45.456500	67.577089
1251.820598	36.543107	67.582094
1250.747169	50.077179	67.587098
1249.732317	34.586989	67.592103
1249.167362	46.572032	67.597108
1248.544249	49.019258	67.602113
1248.475658	45.437803	67.607118
1247.774853	51.772037	67.612122
1246.657188	50.268706	67.617127
1245.620778	53.180631	67.622132
1245.116629	55.790295	67.627137
1245.372244	44.302320	67.632142
1244.137091	53.517520	67.637146
1243.468036	49.097972	67.642151
1242.864812	51.305489	67.647156
1242.262403	52.902584	67.652161
1241.319524	42.283294	67.657166
1240.389547	48.822708	67.662170
1240.011811	44.038287	67.667175
1239.769225	52.181002	67.672180
1239.119880	50.275190	67.677185
1238.307926	49.683634	67.682190
1237.586898	58.123211	67.687194
1237.303279	43.854023	67.692199
1236.245344	53.980928	67.697204
1235.264126	50.509904	67.702209
1234.607695	40.089502	67.707214
1234.105841	51.720733	67.712218
1233.905747	43.389810	67.717223
1232.809005	42.693729	67.722228
1232.019316	46.984134	67.727233
1231.861779	49.436177	67.732238
1230.905668	47.774696	67.737242
1230.392397	46.869135	67.742247
1229.283503	52.188033	67.747252
1228.716382	47.675008	67.752257
1228.261267	49.471037	67.757262
1227.826416	51.043067	67.762266
1227.075580	46.262784	67.767271
1226.088834	50.019967	67.772276
1225.353205	53.311432	67.777281
1225.293812	48.872211	67.782286
1224.053651	59.720399	67.787290
1223.237182	51.796580	67.792295
1222.945630	66.384347	67.797300
1222.340041	64.843748	67.802305
1222.129948	53.030848	67.807310
1220.738338	55.193428	67.812314
1219.721819	55.620025	67.817319
1219.902777	60.162942	67.822324
1219.122759	57.995634	67.827329
1218.954566	45.518474	67.832334
1217.231463	61.175998	67.837338
1217.124440	56.146673	67.842343
1216.370793	61.309735	67.847348
1215.921057	55.016550	67.852353
1215.056244	50.139275	67.857358
1214.170022	56.566084	67.862362
1213.605774	49.657164	67.867367
1213.176271	51.278809	67.872372
1212.730046	53.362015	67.877377
1211.533036	52.476880	67.882382
1210.409363	51.805592	67.887386
1210.527113	48.869455	67.892391
1209.857570	54.138993	67.897396
1209.004251	57.400292	67.902401
1208.592246	56.782989	67.907406
1207.633854	64.415059	67.912410
1207.325119	52.848089	67.917415
1206.707760	54.318256	67.922420
1205.761173	55.276219	67.927425
1205.277201	54.889563	67.932430
1204.816204	56.385328	67.937434
1203.757403	53.888615	67.942439
1203.054873	62.549192	67.947444
1202.045914	61.662540	67.952449
1201.912307	52.780137	67.957454
1201.141780	63.121555	67.962458
1200.741832	51.110191	67.967463
1200.135571	47.623708	67.972468
1199.117410	50.762987	67.977473
1198.619319	45.065716	67.982478
1197.463987	53.965459	67.987482
1197.068313	44.200626	67.992487
1196.431694	48.182840	67.997492
1196.091536	43.225292	68.002497
1195.777365	49.261500	68.007502
1194.539874	58.319395	68.012506
1193.747584	51.952959	68.017511
1193.325349	53.223360	68.022516
1192.562055	55.163026	68.027521
1191.811661	61.191342	68.032526
1190.875779	54.786240	68.037530
1190.483135	52.894811	68.042535
1190.060726	52.577216	68.047540
1189.680894	50.552860	68.052545
1188.925178	47.257309	68.057550
1188.059851	53.982005	68.062554
1187.562980	47.117573	68.067559
1186.092648	43.478349	68.072564
1185.473229	53.183862	68.077569
1184.897081	43.963408	68.082574
1184.415660	54.742979	68.087578
1184.155397	44.423593	68.092583
1183.975967	47.172438	68.097588
1183.139145	49.924908	68.102593
1182.378032	41.181737	68.107598
1181.239748	54.297207	68.112602
1180.595292	42.282164	68.117607
1179.753114	50.070797	68.122612
1178.841410	59.379667	68.127617
1178.860053	46.781334	68.132622
1178.386488	51.284834	68.137626
1178.019154	45.913709	68.142631
1176.731392	48.064526	68.147636
1175.943398	44.045547	68.152641
1175.788681	39.208324	68.157646
1174.607370	46.098395	68.162650
1174.017123	40.901499	68.167655
1173.295010	46.504261	68.172660
1172.867970	44.578882	68.177665
1172.360068	42.076572	68.182670
1171.121816	54.463609	68.187674
1170.544942	44.568326	68.192679
1170.248314	47.111879	68.197684
1169.762282	51.275158	68.202689
1168.850797	42.942269	68.207694
1168.094269	45.399692	68.212698
1167.553951	42.304862	68.217703
1167.160670	49.558469	68.222708
1165.474998	57.325142	68.227713
1165.029041	50.528312	68.232718
1164.619539	54.393986	68.237722
1164.301575	47.010664	68.242727
1164.125654	41.372552	68.247732
1163.140506	52.077694	68.252737
1162.221882	40.951528	68.257742
1161.399863	51.930352	68.262746
1161.098551	50.409186	68.267751
1160.343914	49.444256	68.272756
1159.339389	44.168171	68.277761
1158.802762	40.503466	68.282766
1158.299829	50.442770	68.287770
1158.070291	43.997885	68.292775
1156.663615	52.540218	68.297780
1155.890027	51.728116	68.302785
1155.837178	43.015812	68.307790
1154.953419	47.513591	68.312794
1154.487129	44.845391	68.317799
1153.367289	48.380912	68.322804
1152.632441	49.817737	68.327809
1152.669149	39.061613	68.332814
1151.605359	47.207203	68.337818
1151.037928	47.991338	68.342823
1150.429167	49.239372	68.347828
1149.927628	52.758556	68.352833
1148.831122	49.588186	68.357838
1147.874552	53.827886	68.362842
1147.359731	48.891817	68.367847
1146.869083	45.872671	68.372852
1146.520744	43.548418	68.377857
1146.403901	46.643709	68.382862
1145.421984	49.532810	68.387866
1144.968750	47.020234	68.392871
1144.070938	36.242438	68.397876
1142.794291	40.047334	68.402881
1142.159595	42.729818	68.407886
1141.674627	41.077016	68.412890
1140.950895	43.789432	68.417895
1140.175838	44.713828	68.422900
1139.104361	44.758105	68.427905
1138.914251	36.427191	68.432910
1138.397208	51.689482	68.437914
1138.238933	47.335384	68.442919
1137.672292	47.004469	68.447924
1136.481206	48.677872	68.452929
1136.023925	36.180486	68.457934
1135.371654	46.269701	68.462938
1134.329494	47.943073	68.467943
1133.496486	39.768033	68.472948
1133.109954	46.883371	68.477953
1133.042015	40.537370	68.482958
1131.753747	44.700519	68.487962
1130.890770	47.151229	68.492967
1130.338289	47.163423	68.497972
1129.826564	47.579149	68.502977
1129.130378	36.616322	68.507982
1127.724210	49.798068	68.512986
1127.616349	43.658693	68.517991
1127.123275	46.905292	68.522996
1126.585235	52.404669	68.528001
1126.767700	39.565822	68.533006
1125.302902	49.634470	68.538010
1124.508653	48.071867	68.543015
1124.223046	44.629020	68.548020
1123.356313	46.624582	68.553025
1122.575470	45.897225	68.558030
1122.026622	51.641178	68.563034
1121.370581	48.274600	68.568039
1120.383562	43.620234	68.573044
1119.316383	54.783147	68.578049
1118.994965	47.818284	68.583054
1118.379837	50.844598	68.588058
1117.930040	43.258326	68.593063
1117.934536	42.144272	68.598068
1116.553031	46.713351	68.603073
1116.093012	43.437023	68.608078
1115.450880	47.625139	68.613082
1114.827076	42.690646	68.618087
1113.651134	36.003644	68.623092
1113.207440	43.429277	68.628097
1112.545355	39.339831	68.633102
1112.195158	51.766978	68.638106
1111.824385	51.250368	68.643111
1110.620605	44.523636	68.648116
1109.887532	49.202467	68.653121
1109.664655	43.352630	68.658126
1108.828496	51.980856	68.663130
1107.697987	44.267895	68.668135
1107.258280	37.602558	68.673140
1106.710553	43.601802	68.678145
1106.332691	40.176788	68.683150
1105.315822	45.490554	68.688154
1104.521524	41.688650	68.693159
1103.968999	40.060795	68.698164
1103.305612	49.194557	68.703169
1103.390646	40.390940	68.708174
1101.795379	44.691249	68.713178
1101.175539	48.136216	68.718183
1101.008756	53.008827	68.723188
1100.487725	55.879827	68.728193
1099.910788	48.387899	68.733198
1098.998741	52.160052	68.738202
1098.192370	41.850285	68.743207
1097.117978	46.174975	68.748212
1096.228540	51.757063	68.753217
1096.091667	47.360140	68.758222
1095.438091	47.899365	68.763226
1095.469198	49.960276	68.768231
1094.482663	41.122110	68.773236
1093.156502	50.418076	68.778241
1092.980692	44.749992	68.783246
1092.594800	42.363912	68.788250
1091.853615	48.291431	68.793255
1090.917352	42.233375	68.798260
1090.243326	45.832046	68.803265
1089.468053	47.507135	68.808270
1088.544866	45.892514	68.813274
1088.115636	58.860528	68.818279
1087.799889	48.384403	68.823284
1087.072320	46.768627	68.828289
1086.026365	47.900139	68.833294
1085.050094	45.357235	68.838298
1084.786502	40.368605	68.843303
1084.577339	38.653016	68.848308
1083.711052	46.555894	68.853313
1083.219119	45.200684	68.858318
1082.150549	42.741853	68.863322
1081.620161	39.393148	68.868327
1081.488975	43.176707	68.873332
1079.946628	54.032013	68.878337
1079.394773	45.321826	68.883342
1078.822135	48.846023	68.888346
1078.602056	46.908239	68.893351
1078.069382	50.150108	68.898356
1076.724361	43.523136	68.903361
1076.413256	45.313626	68.908366
1075.708265	40.019894	68.913370
1075.363329	44.611755	68.918375
1074.417169	38.806022	68.923380
1073.279322	47.603674	68.928385
1073.071125	39.480654	68.933390
1072.450396	41.978002	68.938394
1071.855869	45.160322	68.943399
1071.326744	42.442211	68.948404
1070.154275	47.200414	68.953409
1069.900064	42.951474	68.958414
1068.800176	49.579471	68.963418
1067.836572	39.830906	68.968423
1067.215026	38.010609	68.973428
1066.781390	48.432491	68.978433
1066.707101	42.440750	68.983438
1066.496514	49.756766	68.988442
1065.400977	46.728209	68.993447
1064.633126	46.683214	68.998452
1063.947463	50.711106	69.003457
1063.288465	46.646413	69.008462
1062.046749	55.168856	69.013466
1061.536842	51.963554	69.018471
1061.377748	46.499399	69.023476
1060.526754	50.706561	69.028481
1060.119213	43.984075	69.033486
1058.916539	52.407264	69.038490
1058.503229	48.223060	69.043495
1058.429238	42.407894	69.048500
1057.149472	47.768232	69.053505
1056.400271	39.412732	69.058510
1055.688181	49.998766	69.063514
1055.193152	47.891833	69.068519
1054.867078	41.375590	69.073524
1053.882959	49.189988	69.078529
1053.381485	46.918498	69.083534
1052.808970	42.963055	69.088538
1051.949793	46.600653	69.093543
1051.105399	48.969583	69.098548
1050.370193	42.441157	69.103553
1050.358189	37.131805	69.108558
1048.959599	48.716473	69.113562
1048.099461	46.393233	69.118567
1047.689528	40.866484	69.123572
1047.324910	50.537784	69.128577
1047.264400	43.561392	69.133582
1046.111965	52.432341	69.138586
1045.257701	41.857399	69.143591
1045.080839	47.193668	69.148596
1043.763403	51.427733	69.153601
1043.080313	47.363725	69.158606
1042.240597	42.104053	69.163610
1042.138386	35.580584	69.168615
1041.875637	48.071088	69.173620
1040.579174	54.115348	69.178625
1039.980075	43.933481	69.183630
1039.281710	45.649966	69.188634
1038.889689	47.805001	69.193639
1038.529614	42.552601	69.198644
1036.891380	57.793003	69.203649
1036.616011	38.488833	69.208654
1036.239795	47.143247	69.213658
1035.239797	45.674910	69.218663
1034.772984	37.570965	69.223668
1033.813235	46.561073	69.228673
1033.363628	42.207606	69.233678
1032.920914	46.665214	69.238682
1032.167289	49.559037	69.243687
1031.728706	53.353658	69.248692
1030.587660	53.855335	69.253697
1029.947515	38.854440	69.258702
1029.340413	50.183879	69.263706
1028.352794	47.423604	69.268711
1028.017417	44.540634	69.273716
1027.339798	43.483065	69.278721
1026.956640	46.545032	69.283726
1026.488092	41.111194	69.288730
1025.639164	38.781449	69.293735
1024.926985	39.178625	69.298740
1023.664912	48.626852	69.303745
1023.437805	51.258709	69.308750
1023.117864	48.605099	69.313754
1021.934274	45.981664	69.318759
1021.373647	44.082299	69.323764
1020.904152	45.702449	69.328769
1020.704426	41.632509	69.333774
1019.511391	50.246571	69.338778
1018.665440	48.438334	69.343783
1018.360908	43.568193	69.348788
1017.493757	47.188146	69.353793
1016.659783	50.850131	69.358798
1015.783514	44.080804	69.363802
1015.296865	49.363859	69.368807
1015.050771	47.871776	69.373812
1014.810525	53.044664	69.378817
1014.045767	44.387296	69.383822
1012.999767	53.865808	69.388826
1012.400012	54.172559	69.393831
1011.739551	38.411646	69.398836
1010.473012	43.005062	69.403841
1010.161388	42.698257	69.408846
1009.669947	41.611072	69.413850
1009.242052	41.116182	69.418855
1008.541690	41.121968	69.423860
1007.219948	44.949873	69.428865
1007.159252	37.662852	69.433870
1006.376631	49.304076	69.438874
1005.916605	58.388156	69.443879
1005.004426	47.139609	69.448884
1004.499971	54.619082	69.453889
1003.766842	47.180422	69.458894
1002.913133	46.715436	69.463898
1001.944239	51.882832	69.468903
1001.613630	35.661004	69.473908
1000.905318	50.255130	69.478913
1000.799657	51.490959	69.483918
999.684328	51.909710	69.488922
998.997339	52.839059	69.493927
998.449217	53.243256	69.498932
997.602122	57.708443	69.503937
997.394816	53.376352	69.508942
996.360373	54.223789	69.513946
995.363753	51.174794	69.518951
995.260595	44.279311	69.523956
994.653168	55.705006	69.528961
993.740047	47.238411	69.533966
993.005900	43.912685	69.538970
992.376238	49.305233	69.543975
992.254078	49.471340	69.548980
990.894301	49.069535	69.553985
990.325584	42.852114	69.558990
989.972952	45.762569	69.563994
989.629758	45.549101	69.568999
988.785651	49.293132	69.574004
987.671993	49.186487	69.579009
987.269708	50.969417	69.584014
986.468635	44.790545	69.589018
985.404650	51.404975	69.594023
984.689363	39.437551	69.599028
983.926238	52.151180	69.604033
983.599660	39.822280	69.609038
983.424985	41.961661	69.614042
982.863705	49.976887	69.619047
982.568646	48.878959	69.624052
981.621747	47.630857	69.629057
980.721937	44.580658	69.634062
979.679396	44.226154	69.639066
978.766694	45.826946	69.644071
978.271647	44.161589	69.649076
977.857538	46.517268	69.654081
977.404132	39.502476	69.659086
977.233052	41.171345	69.664090
976.113214	41.877834	69.669095
975.471887	53.263191	69.674100
974.765919	53.328227	69.679105
973.867335	42.900719	69.684110
973.032381	42.852237	69.689114
972.652605	54.052471	69.694119
972.437638	40.898398	69.699124
970.974344	51.123001	69.704129
970.527881	52.245901	69.709134
969.968923	49.993038	69.714138
969.487535	52.512393	69.719143
969.036178	42.433200	69.724148
967.539313	48.946203	69.729153
967.085883	43.260810	69.734158
966.862833	42.367473	69.739162
965.900599	52.099179	69.744167
965.669341	45.022229	69.749172
964.562125	49.091990	69.754177
963.638910	50.632959	69.759182
963.386374	46.003716	69.764186
962.942531	54.367696	69.769191
962.463755	40.550694	69.774196
961.468125	55.611602	69.779201
960.921237	47.540915	69.784206
960.578881	48.650404	69.789210
959.117242	50.966193	69.794215
958.530378	46.371227	69.799220
958.274713	47.116831	69.804225
957.721482	43.710289	69.809230
956.592670	48.318086	69.814234
956.067525	42.715072	69.819239
955.807364	35.382526	69.824244
955.088679	49.281281	69.829249
953.947829	38.020268	69.834254
953.338866	35.903104	69.839258
952.704706	46.517752	69.844263
952.306605	40.872446	69.849268
951.679691	49.205631	69.854273
950.549577	51.515978	69.859278
950.101705	56.114772	69.864282
949.618984	45.859221	69.869287
949.187148	44.786217	69.874292
948.132761	47.220135	69.879297
947.329229	50.694366	69.884302
946.791184	49.173054	69.889306
946.613699	44.465637	69.894311
945.820582	45.206881	69.899316
945.198193	44.865957	69.904321
944.256402	41.227932	69.909326
943.360817	44.555960	69.914330
942.190507	43.941101	69.919335
942.032589	38.147188	69.924340
941.699751	43.524047	69.929345
941.190045	44.407853	69.934350
940.844928	43.565482	69.939354
940.134689	46.023486	69.944359
939.334136	44.433562	69.949364
937.774005	52.943644	69.954369
936.706016	43.222791	69.959374
936.733457	42.713802	69.964378
936.242830	48.853801	69.969383
936.049582	43.223206	69.974388
935.715848	43.773075	69.979393
934.347792	48.682310	69.984398
933.728884	45.628429	69.989402
932.982709	44.868807	69.994407
932.767692	43.059546	69.999412
931.338000	46.442611	70.004417
930.599225	38.836145	70.009422
930.275953	42.174025	70.014426
929.684506	47.188335	70.019431
929.482912	36.840749	70.024436
928.026304	43.820458	70.029441
927.488705	51.666341	70.034446
927.143920	41.683744	70.039450
926.436505	44.932945	70.044455
926.026709	43.468501	70.049460
925.026337	41.900919	70.054465
924.494907	36.693161	70.059470
924.019636	40.731756	70.064474
922.913809	47.540525	70.069479
922.547471	40.444080	70.074484
921.432753	46.468929	70.079489
921.075368	40.087008	70.084494
920.854839	48.517953	70.089498
919.831709	48.598785	70.094503
919.305950	44.757364	70.099508
918.548179	41.206762	70.104513
918.476473	43.219371	70.109518
917.132315	42.583304	70.114522
916.269145	48.568124	70.119527
916.412862	38.810570	70.124532
914.845910	43.770389	70.129537
914.154731	45.474724	70.134542
913.736382	40.889224	70.139546
913.362204	46.329437	70.144551
913.040507	32.448037	70.149556
911.944764	45.829628	70.154561
911.107570	36.084679	70.159566
910.709011	38.761173	70.164570
910.112463	37.979322	70.169575
909.132228	39.584578	70.174580
908.016835	39.967108	70.179585
907.591079	33.602382	70.184590
907.369641	31.032467	70.189594
906.745946	39.136479	70.194599
906.120125	38.054932	70.199604
905.316994	43.148666	70.204609
904.567162	40.095130	70.209614
904.197640	35.415130	70.214618
902.957031	42.529211	70.219623
902.676173	32.582185	70.224628
902.162705	43.103512	70.229633
901.559252	35.464482	70.234638
900.703969	31.506777	70.239642
899.779733	39.578196	70.244647
899.473686	39.882385	70.249652
898.832211	39.610744	70.254657
897.806902	32.068819	70.259662
897.293940	34.405547	70.264666
896.355903	38.601374	70.269671
895.941206	26.083103	70.274676
895.628760	29.892354	70.279681
894.273681	45.516684	70.284686
893.826673	39.150611	70.289690
892.990451	42.371433	70.294695
893.024039	30.056208	70.299700
892.322518	47.593479	70.304705
891.584359	42.470670	70.309710
890.880716	39.036044	70.314714
889.986329	36.104870	70.319719
889.630511	33.676194	70.324724
888.533280	44.004998	70.329729
887.961591	34.862788	70.334734
887.660508	31.408251	70.339738
886.951332	40.110930	70.344743
886.253976	37.733458	70.349748
885.250728	42.819622	70.354753
884.555507	40.321960	70.359758
884.583781	37.295981	70.364762
883.545428	43.474272	70.369767
882.461608	41.000610	70.374772
881.642166	44.337039	70.379777
881.051030	38.645200	70.384782
881.104279	43.066469	70.389786
880.484660	44.551262	70.394791
879.744201	49.212399	70.399796
878.745799	52.610431	70.404801
878.145708	42.513936	70.409806
878.059996	45.925978	70.414810
876.844233	50.489299	70.419815
876.059884	52.197434	70.424820
875.618039	38.718367	70.429825
874.750096	39.294920	70.434830
874.142601	41.684547	70.439834
873.052968	47.509877	70.444839
872.914267	43.119577	70.449844
872.382970	40.494902	70.454849
872.026696	35.724488	70.459854
871.463121	37.965197	70.464858
870.196897	48.970622	70.469863
870.023440	41.412974	70.474868
868.958479	34.719479	70.479873
867.913998	47.876880	70.484878
867.906239	37.405412	70.489882
866.911871	49.086672	70.494887
865.962524	39.091505	70.499892
865.410509	41.224718	70.504897
864.976548	44.389408	70.509902
864.742323	38.964047	70.514906
863.653544	49.810344	70.519911
862.980724	40.211141	70.524916
862.148528	47.537785	70.529921
861.862973	43.593491	70.534926
861.584252	44.183499	70.539930
860.152240	54.669686	70.544935
859.860431	47.801090	70.549940
859.408737	45.603723	70.554945
858.206567	47.185975	70.559950
857.558277	40.780983	70.564954
856.367937	50.515908	70.569959
856.148893	48.786145	70.574964
855.817740	45.095117	70.579969
855.483777	46.283709	70.584974
854.651456	40.841582	70.589978
853.408333	47.470376	70.594983
853.186522	38.773965	70.599988
852.742187	41.587065	70.604993
851.729085	44.599507	70.609998
851.086694	44.189250	70.615002
850.147392	45.810090	70.620007
850.211095	49.259853	70.625012
848.965545	42.878965	70.630017
848.350600	46.802606	70.635022
847.579095	43.560147	70.640026
847.237179	46.904158	70.645031
847.062192	33.024656	70.650036
845.782862	38.172124	70.655041
844.881551	46.172102	70.660046
844.706710	36.417950	70.665050
843.982737	47.401729	70.670055
842.899222	39.351843	70.675060
842.247533	40.065876	70.680065
841.691232	51.316287	70.685070
841.602934	40.692058	70.690074
840.612166	41.620916	70.695079
839.813049	36.242897	70.700084
838.992114	41.601260	70.705089
838.367421	34.932320	70.710094
838.562153	37.074409	70.715098
837.365087	50.424844	70.720103
836.582857	48.638069	70.725108
835.939822	51.170560	70.730113
835.212922	46.189482	70.735118
834.228932	35.677868	70.740122
833.445175	43.674906	70.745127
833.205141	44.653004	70.750132
832.807444	48.840117	70.755137
832.166242	44.280645	70.760142
831.372761	37.258522	70.765146
830.272638	45.840516	70.770151
830.128347	37.582786	70.775156
829.504382	40.413443	70.780161
828.631817	38.507008	70.785166
828.032373	33.964549	70.790170
827.347089	39.173586	70.795175
827.030085	41.436557	70.800180
826.142732	41.494237	70.805185
824.882611	44.497124	70.810190
824.870933	40.589666	70.815194
824.029664	45.883462	70.820199
823.871449	43.227795	70.825204
822.813114	43.158149	70.830209
822.294003	39.725711	70.835214
821.704718	37.195435	70.840218
820.141622	41.028732	70.845223
819.869736	39.450890	70.850228
819.322907	36.483342	70.855233
818.659253	44.951706	70.860238
818.504950	41.959521	70.865242
817.013901	43.966251	70.870247
816.592425	40.224953	70.875252
815.870897	38.422216	70.880257
815.662698	42.680091	70.885262
815.519482	39.019081	70.890266
814.174307	43.292362	70.895271
813.728032	41.791167	70.900276
813.078159	38.101998	70.905281
811.597196	34.836868	70.910286
811.354985	36.069207	70.915290
810.661465	43.960421	70.920295
810.247702	36.622390	70.925300
809.771646	43.058131	70.930305
808.585424	45.930989	70.935310
808.225187	35.014161	70.940314
807.600965	45.204616	70.945319
807.027929	40.473451	70.950324
806.163353	37.838767	70.955329
805.313336	49.117012	70.960334
804.638068	39.939275	70.965338
804.230367	46.386214	70.970343
803.419247	43.391354	70.975348
802.572940	47.214638	70.980353
802.318602	47.624150	70.985358
802.124176	39.106318	70.990362
801.260921	43.816983	70.995367
800.206741	42.053012	71.000372
799.885729	39.322338	71.005377
799.107705	42.645889	71.010382
798.428725	33.557060	71.015386
797.128681	44.105839	71.020391
796.704448	43.394358	71.025396
796.061560	50.943199	71.030401
795.566198	37.720265	71.035406
795.311159	48.512706	71.040410
794.356324	45.718925	71.045415
793.618824	39.151536	71.050420
792.884657	38.699132	71.055425
792.379841	49.739498	71.060430
791.636877	45.265625	71.065434
790.779615	50.915221	71.070439
790.426769	43.130671	71.075444
790.150863	53.311416	71.080449
789.001995	53.782908	71.085454
788.427652	43.089401	71.090458
787.508404	63.947783	71.095463
787.161993	43.945356	71.100468
786.568692	47.728367	71.105473
785.391213	50.054210	71.110478
785.080480	48.542480	71.115482
784.360311	52.987520	71.120487
784.058188	41.533156	71.125492
782.992472	43.186760	71.130497
782.297666	42.699708	71.135502
781.833628	42.229536	71.140506
781.394885	46.213451	71.145511
780.552907	44.300587	71.150516
780.260388	43.724260	71.155521
779.287214	49.657243	71.160526
778.522437	47.342576	71.165530
777.088922	49.001119	71.170535
777.055405	43.474431	71.175540
776.664311	47.200021	71.180545
776.095518	51.732929	71.185550
775.356890	45.162569	71.190554
774.100749	47.171351	71.195559
773.877343	41.088258	71.200564
773.506017	47.111511	71.205569
772.558593	48.817252	71.210574
771.961172	34.139257	71.215578
770.957718	42.024626	71.220583
770.726352	43.050235	71.225588
769.701169	49.776836	71.230593
768.562035	51.254475	71.235598
768.234470	46.785442	71.240602
767.888914	56.559379	71.245607
767.405527	51.385011	71.250612
767.011519	50.887922	71.255617
765.519994	47.015787	71.260622
765.110450	43.411374	71.265626
764.624929	55.122043	71.270631
764.465925	36.409729	71.275636
763.216025	48.328819	71.280641
762.724572	39.282685	71.285646
762.222737	43.491115	71.290650
761.263346	43.609173	71.295655
760.378184	39.126412	71.300660
759.601226	44.268058	71.305665
759.313414	52.124658	71.310670
759.058104	44.829219	71.315674
757.978024	51.182936	71.320679
757.245412	48.041549	71.325684
756.780642	40.749497	71.330689
755.890859	48.889594	71.335694
755.490252	41.085848	71.340698
754.584009	43.805343	71.345703
753.966680	47.013436	71.350708
753.618443	42.927749	71.355713
752.655100	46.023771	71.360718
752.021759	40.655661	71.365722
751.253053	48.241887	71.370727
750.699908	49.676703	71.375732
750.660747	48.374058	71.380737
749.250005	47.575215	71.385742
748.723260	34.436145	71.390746
748.101575	48.622263	71.395751
747.313814	42.346746	71.400756
746.428960	41.251287	71.405761
745.543966	33.559362	71.410766
745.463683	35.683725	71.415770
745.090161	48.866800	71.420775
744.614780	36.642083	71.425780
743.463811	42.108212	71.430785
742.339366	42.110628	71.435790
742.027412	43.213726	71.440794
741.600134	43.652355	71.445799
741.007914	47.950875	71.450804
740.255951	46.375359	71.455809
739.127603	47.991645	71.460814
739.072053	43.635429	71.465818
738.398789	42.451090	71.470823
737.093669	44.188563	71.475828
736.539217	42.111663	71.480833
736.106543	47.032918	71.485838
736.020931	41.746343	71.490842
735.030686	47.363508	71.495847
734.207442	48.481781	71.500852
733.924966	39.034947	71.505857
733.138306	50.426126	71.510862
732.160099	34.116678	71.515866
731.496372	48.281105	71.520871
730.794040	49.673445	71.525876
730.490673	44.003641	71.530881
729.239704	46.229243	71.535886
728.840880	44.518657	71.540890
728.263918	47.471166	71.545895
727.691765	43.761762	71.550900
727.477839	43.880990	71.555905
726.458247	47.577344	71.560910
725.930692	44.475860	71.565914
724.495649	48.034932	71.570919
723.390074	44.467232	71.575924
723.214714	40.697806	71.580929
722.591894	51.198718	71.585934
722.385294	40.230639	71.590938
721.673689	43.348091	71.595943
721.712312	40.087075	71.600948
721.009744	39.434117	71.605953
719.459887	50.954700	71.610958
719.478758	38.578753	71.615962
718.351864	42.587088	71.620967
717.311450	36.414892	71.625972
716.917116	32.910574	71.630977
716.241624	40.223338	71.635982
715.955595	31.261211	71.640986
714.695034	46.980947	71.645991
714.150909	36.210119	71.650996
713.702659	38.191219	71.656001
713.260389	44.127999	71.661006
712.872868	34.035570	71.666010
711.397055	44.423134	71.671015
710.709128	40.874097	71.676020
710.456541	43.224596	71.681025
709.979326	49.453952	71.686030
709.298657	35.538300	71.691034
708.287536	44.571371	71.696039
707.895983	33.795178	71.701044
707.645416	38.668514	71.706049
706.066576	36.702692	71.711054
705.726616	40.088983	71.716058
704.984155	42.996883	71.721063
704.572280	37.000584	71.726068
704.302547	36.843268	71.731073
702.898272	44.313081	71.736078
702.359762	30.683888	71.741082
702.007408	41.088112	71.746087
700.801492	38.023687	71.751092
700.036971	34.740744	71.756097
699.296936	42.694580	71.761102
699.129211	38.556506	71.766106
698.618045	39.902644	71.771111
698.243620	41.630715	71.776116
697.725811	35.697018	71.781121
696.977651	42.347989	71.786126
696.244486	33.720418	71.791130
694.991778	35.954197	71.796135
694.118680	39.240875	71.801140
693.734741	34.955879	71.806145
693.295861	41.428292	71.811150
692.974538	37.688421	71.816154
691.987425	38.407015	71.821159
691.070341	40.834940	71.826164
690.715151	29.559371	71.831169
690.199001	34.165909	71.836174
689.797859	37.997187	71.841178
688.856599	48.578771	71.846183
688.342060	42.701324	71.851188
687.271527	40.380180	71.856193
686.087384	47.269317	71.861198
685.667115	35.491590	71.866202
685.459806	31.880225	71.871207
685.027100	36.470323	71.876212
684.105271	20.137749	71.881217
683.007942	46.077097	71.886222
682.670617	37.501616	71.891226
682.246325	37.411493	71.896231
681.592022	36.416542	71.901236
680.583340	31.529279	71.906241
680.043147	34.832336	71.911246
679.762380	27.304428	71.916250
678.441950	43.784345	71.921255
677.711304	42.022526	71.926260
677.566701	35.726626	71.931265
676.478619	42.155761	71.936270
676.493832	29.122812	71.941274
675.511102	37.008061	71.946279
674.636561	37.711891	71.951284
674.303984	40.559261	71.956289
673.554288	47.249908	71.961294
672.942939	36.369949	71.966298
671.885338	37.557099	71.971303
671.465594	36.819694	71.976308
671.121021	41.129253	71.981313
669.877323	40.586134	71.986318
669.265576	32.193132	71.991322
668.604480	41.583642	71.996327
668.046397	47.284978	72.001332
668.023547	39.889461	72.006337
666.937328	47.945743	72.011342
666.386865	37.776767	72.016346
665.554206	40.770005	72.021351
664.693563	49.626163	72.026356
663.785924	43.592122	72.031361
663.085193	50.513100	72.036366
662.576102	50.155782	72.041370
662.129792	45.115889	72.046375
661.668998	45.917841	72.051380
661.412914	38.833861	72.056385
660.050674	47.074450	72.061390
659.523824	42.670289	72.066394
659.089131	42.961877	72.071399
658.068967	39.617154	72.076404
657.605694	38.621752	72.081409
656.701951	41.621582	72.086414
656.686277	32.647953	72.091418
655.803550	42.838592	72.096423
654.549705	39.297691	72.101428
654.410424	33.647508	72.106433
653.397085	45.409114	72.111438
653.652876	38.877563	72.116442
652.534794	34.062928	72.121447
651.637194	42.672655	72.126452
651.087007	35.894137	72.131457
650.211026	43.968982	72.136462
649.172531	41.246934	72.141466
648.811653	41.233451	72.146471
648.261186	44.186487	72.151476
647.806365	38.487202	72.156481
647.308258	45.727578	72.161486
646.228996	40.392668	72.166490
645.589960	45.015632	72.171495
645.049408	37.921763	72.176500
644.902441	40.216022	72.181505
643.743495	46.017780	72.186510
643.308105	45.582496	72.191514
642.762471	43.724992	72.196519
641.199366	50.013746	72.201524
640.738906	41.125139	72.206529
640.070101	45.680305	72.211534
639.838146	47.311577	72.216538
639.621787	50.085250	72.221543
638.628370	46.690542	72.226548
637.766167	42.678843	72.231553
636.626789	49.890459	72.236558
636.745578	45.897576	72.241562
635.668357	49.983192	72.246567
634.749911	47.611042	72.251572
634.736837	40.275473	72.256577
633.761450	46.773411	72.261582
633.392035	36.222373	72.266586
632.541031	45.020230	72.271591
631.584060	47.170672	72.276596
631.279796	41.956776	72.281601
630.704728	46.992186	72.286606
629.830639	41.867462	72.291610
628.929927	40.550641	72.296615
628.055647	48.119014	72.301620
628.134307	47.324318	72.306625
627.447655	44.333353	72.311630
626.861314	50.991690	72.316634
625.838901	43.365852	72.321639
625.224068	50.475010	72.326644
624.786880	38.610107	72.331649
623.106019	45.278749	72.336654
622.846059	36.129558	72.341658
622.577449	44.421498	72.346663
621.958833	47.375931	72.351668
621.943059	41.039019	72.356673
620.734248	41.565865	72.361678
620.216727	41.832803	72.366682
619.502599	38.425165	72.371687
618.385280	43.403431	72.376692
617.822332	40.063181	72.381697
616.986613	53.091210	72.386702
616.771711	41.947853	72.391706
616.368474	40.605424	72.396711
614.893572	39.406864	72.401716
614.623192	44.210821	72.406721
613.897587	35.325030	72.411726
613.567937	40.151041	72.416730
612.750204	34.015973	72.421735
611.530930	38.135258	72.426740
611.372465	36.850042	72.431745
610.453661	44.554822	72.436750
610.389644	39.488750	72.441754
609.429530	41.682278	72.446759
608.462812	40.268743	72.451764
608.048183	37.029455	72.456769
607.752680	49.580355	72.461774
607.037260	43.274447	72.466778
605.632241	47.795486	72.471783
605.134646	45.821528	72.476788
604.849725	38.013589	72.481793
604.298608	46.552377	72.486798
603.395164	36.007552	72.491802
602.788211	38.138526	72.496807
602.025232	40.776906	72.501812
601.758847	39.565650	72.506817
600.730424	34.520715	72.511822
599.851287	37.953466	72.516826
599.266170	34.266665	72.521831
598.756754	35.997324	72.526836
598.480712	31.472811	72.531841
597.544349	40.527123	72.536846
596.747402	35.858489	72.541850
596.627303	39.001612	72.546855
595.251430	44.101493	72.551860
594.942444	37.495890	72.556865
594.012091	48.004796	72.561870
593.695064	37.491155	72.566874
593.065235	38.438315	72.571879
591.917256	38.190655	72.576884
591.401571	35.841108	72.581889
590.599145	37.050728	72.586894
590.618929	36.279602	72.591898
589.641203	35.030257	72.596903
588.439326	39.720800	72.601908
588.166471	36.591400	72.606913
587.618593	41.560983	72.611918
587.347216	44.242494	72.616922
586.295950	39.303706	72.621927
585.526624	43.647809	72.626932
585.165017	36.944932	72.631937
584.671609	36.167235	72.636942
583.137005	29.367337	72.641946
582.951773	38.973805	72.646951
582.096732	41.975364	72.651956
582.136211	44.170542	72.656961
581.116202	47.029642	72.661966
580.174762	36.716386	72.666970
579.768127	37.590152	72.671975
579.023886	34.316637	72.676980
578.298986	38.887056	72.681985
577.001370	47.645676	72.686990
576.616486	37.243774	72.691994
576.569182	44.641015	72.696999
576.123593	41.411395	72.702004
575.293117	36.972039	72.707009
574.376262	45.181150	72.712014
573.858420	45.580615	72.717018
572.971275	40.360222	72.722023
571.855901	43.583026	72.727028
571.554165	37.835722	72.732033
570.944111	41.162544	72.737038
570.809146	37.151733	72.742042
570.222347	41.152949	72.747047
569.031942	39.242042	72.752052
568.732539	36.779203	72.757057
567.895360	47.514551	72.762062
566.520749	39.995307	72.767066
565.974945	40.096449	72.772071
565.440644	37.007119	72.777076
565.519891	40.222571	72.782081
564.637678	41.847035	72.787086
563.842540	36.585184	72.792090
562.965664	40.044395	72.797095
562.524287	39.165373	72.802100
562.328575	39.931428	72.807105
561.123479	49.861202	72.812110
560.336390	41.718514	72.817114
559.834413	31.778401	72.822119
559.350590	45.089431	72.827124
558.781333	36.202412	72.832129
557.519778	43.212739	72.837134
557.067283	35.065646	72.842138
556.788974	32.247785	72.847143
556.019926	43.229327	72.852148
554.982994	39.218685	72.857153
554.263982	43.726672	72.862158
554.006297	33.807571	72.867162
553.381535	38.494512	72.872167
552.481547	40.555479	72.877172
552.074863	37.296013	72.882177
551.563516	45.930975	72.887182
550.724801	39.346681	72.892186
549.682654	43.299007	72.897191
549.042059	41.677427	72.902196
548.799834	36.201350	72.907201
548.391751	37.553174	72.912206
547.126383	38.724585	72.917210
546.432650	33.462358	72.922215
545.676558	44.087020	72.927220
545.410220	36.782342	72.932225
544.514367	43.799078	72.937230
543.455673	39.471782	72.942234
542.826690	41.962676	72.947239
542.276287	35.557968	72.952244
542.062390	28.645492	72.957249
541.169318	42.001210	72.962254
541.329307	42.920342	72.967258
540.434517	40.320533	72.972263
539.271177	41.116145	72.977268
539.284844	37.223589	72.982273
537.564840	48.465431	72.987278
537.118182	37.764293	72.992282
536.776138	33.795935	72.997287
536.149498	42.066059	73.002292
535.680214	32.854037	73.007297
534.321792	47.711050	73.012302
533.893867	41.441374	73.017306
533.627892	43.524357	73.022311
533.262859	43.457935	73.027316
532.488795	43.672717	73.032321
531.488569	42.488480	73.037326
530.777503	44.424743	73.042330
530.219311	37.519801	73.047335
528.963275	40.895918	73.052340
528.527010	37.387276	73.057345
527.937087	45.157961	73.062350
527.728968	40.043888	73.067354
527.438120	43.939620	73.072359
525.988835	53.643378	73.077364
526.099212	32.551147	73.082369
524.371321	42.379706	73.087374
523.589148	44.437686	73.092378
523.380101	36.409517	73.097383
522.388959	51.882974	73.102388
522.248729	36.121407	73.107393
521.986998	46.039688	73.112398
521.475235	43.716341	73.117402
520.602630	36.782640	73.122407
519.542645	48.307285	73.127412
518.722817	41.250057	73.132417
517.693307	44.367740	73.137422
517.268831	40.995995	73.142426
516.661392	43.201185	73.147431
516.430095	44.769283	73.152436
515.947415	44.201205	73.157441
514.850235	50.259686	73.162446
514.149819	42.995775	73.167450
513.967219	33.282345	73.172455
513.241677	45.532736	73.177460
512.098792	39.197188	73.182465
511.354783	43.556201	73.187470
511.352729	44.917467	73.192474
510.692325	43.882533	73.197479
508.954948	47.338495	73.202484
508.880375	43.493112	73.207489
508.192888	40.817712	73.212494
507.997574	42.335922	73.217498
507.874841	38.449326	73.222503
506.520038	50.711658	73.227508
506.085717	41.273293	73.232513
505.219515	45.823665	73.237518
504.170090	37.814258	73.242522
503.727505	38.433563	73.247527
502.678042	43.492529	73.252532
502.011386	35.907854	73.257537
501.432031	38.972753	73.262542
500.782107	40.074526	73.267546
500.746845	42.872972	73.272551
499.887685	43.610682	73.277556
498.940588	37.770660	73.282561
497.992059	46.483161	73.287566
497.217053	44.714273	73.292570
497.278313	39.855336	73.297575
496.752172	39.660044	73.302580
496.174704	49.180767	73.307585
495.241134	47.011358	73.312590
494.518620	46.781117	73.317594
494.191440	40.869144	73.322599
492.809035	38.859552	73.327604
492.205882	37.209946	73.332609
491.616345	46.486584	73.337614
491.417769	45.557855	73.342618
490.573217	42.811287	73.347623
489.666576	50.009535	73.352628
489.006282	42.160493	73.357633
488.734114	46.333954	73.362638
487.495049	50.555800	73.367642
486.819183	41.572243	73.372647
486.278449	50.555677	73.377652
485.994658	43.272711	73.382657
485.691491	48.644879	73.387662
484.698791	41.525318	73.392666
484.040426	43.163034	73.397671
483.137234	55.717710	73.402676
482.673954	42.018254	73.407681
481.685905	42.730772	73.412686
481.268502	44.897809	73.417690
480.414181	33.539386	73.422695
479.982455	46.279142	73.427700
479.605199	43.298856	73.432705
478.523844	49.326443	73.437710
477.790537	45.168113	73.442714
477.401412	49.046391	73.447719
476.123357	48.165064	73.452724
475.732169	50.227000	73.457729
474.959738	52.171478	73.462734
474.643143	45.759497	73.467738
474.630742	43.003360	73.472743
473.778396	54.078623	73.477748
472.565828	54.853724	73.482753
472.084394	55.107058	73.487758
471.615230	52.237610	73.492762
470.618171	48.165457	73.497767
469.802431	50.206724	73.502772
469.403158	45.988869	73.507777
469.144064	55.774271	73.512782
467.729673	48.797594	73.517786
467.506491	40.667605	73.522791
466.603775	47.098824	73.527796
466.008649	39.029673	73.532801
465.185538	43.620499	73.537806
464.236147	44.095050	73.542810
463.735032	40.812799	73.547815
463.179174	51.818746	73.552820
463.306836	40.964623	73.557825
462.570775	55.329847	73.562830
461.823279	48.059261	73.567834
461.072104	44.514072	73.572839
459.991171	50.741875	73.577844
458.984224	48.174157	73.582849
458.467670	49.757746	73.587854
457.997078	41.698717	73.592858
457.631804	41.685962	73.597863
456.789396	48.377238	73.602868
456.124654	45.655651	73.607873
455.275259	43.155876	73.612878
454.268725	42.489923	73.617882
454.561382	37.685585	73.622887
453.200715	48.496481	73.627892
453.083827	39.542150	73.632897
452.303266	44.102546	73.637902
451.632126	43.067762	73.642906
451.141901	40.053441	73.647911
449.948615	39.749986	73.652916
449.542831	39.300558	73.657921
448.840045	42.323633	73.662926
448.303295	44.878701	73.667930
447.355809	44.499814	73.672935
446.396125	47.152232	73.677940
446.168759	36.140212	73.682945
445.831476	36.438394	73.687950
445.412081	39.931984	73.692954
444.475830	41.733836	73.697959
443.745381	47.748103	73.702964
442.574706	43.585354	73.707969
441.622337	54.376936	73.712974
441.151298	46.466215	73.717978
440.725043	51.099475	73.722983
440.285980	52.878882	73.727988
440.182163	50.108925	73.732993
439.410616	42.980957	73.737998
438.376591	48.893783	73.743002
438.080395	37.060091	73.748007
436.974185	50.322064	73.753012
435.983096	45.629227	73.758017
435.184092	47.980077	73.763022
434.665582	52.046136	73.768026
434.511356	48.360107	73.773031
433.831778	50.966322	73.778036
433.082217	43.355454	73.783041
432.754263	53.684842	73.788046
431.985232	49.609490	73.793050
430.909079	45.231410	73.798055
429.728551	49.981702	73.803060
429.531916	45.014046	73.808065
429.109480	40.823547	73.813070
428.860834	46.021448	73.818074
427.828476	41.491312	73.823079
427.059191	48.355450	73.828084
426.727652	43.114398	73.833089
426.068153	42.563473	73.838094
424.955029	42.332414	73.843098
424.596987	48.810901	73.848103
423.828422	42.862038	73.853108
423.231604	42.588135	73.858113
421.960900	45.559782	73.863118
421.007489	49.490134	73.868122
421.128356	37.744532	73.873127
420.465130	46.592947	73.878132
420.087926	38.219425	73.883137
419.336585	42.076576	73.888142
418.382283	41.818635	73.893146
418.087587	35.198175	73.898151
417.455054	46.411885	73.903156
416.767801	44.700004	73.908161
416.053024	38.939696	73.913166
415.268783	49.396982	73.918170
414.306176	37.652137	73.923175
413.506360	46.372506	73.928180
413.108277	43.075425	73.933185
412.751328	45.470961	73.938190
411.811271	47.194583	73.943194
411.379923	36.806438	73.948199
410.342989	43.120286	73.953204
409.814376	44.086056	73.958209
409.605067	43.526479	73.963214
408.584526	41.717897	73.968218
407.809288	44.162740	73.973223
406.911272	44.067725	73.978228
406.479121	42.957024	73.983233
406.191113	44.791213	73.988238
405.352502	44.353992	73.993242
404.262306	43.026448	73.998247
403.911352	49.973745	74.003252
403.719559	44.527499	74.008257
402.408630	41.331726	74.013262
401.558419	49.230643	74.018266
401.336361	42.658533	74.023271
400.474069	50.944157	74.028276
400.187543	46.224220	74.033281
399.332598	49.571180	74.038286
398.328680	44.948214	74.043290
397.934680	41.098547	74.048295
397.154448	48.729267	74.053300
397.020296	47.460694	74.058305
396.226512	45.338436	74.063310
395.789687	47.652084	74.068314
394.913881	38.754042	74.073319
393.639764	42.968898	74.078324
393.099696	40.370968	74.083329
392.511783	36.700438	74.088334
392.369672	47.496953	74.093338
392.058174	41.074717	74.098343
390.795830	43.565648	74.103348
390.119804	42.356617	74.108353
389.567820	40.523840	74.113358
388.362823	46.416619	74.118362
387.707280	35.827663	74.123367
387.108267	49.010402	74.128372
386.616867	48.748095	74.133377
386.395918	38.059920	74.138382
386.069500	44.374095	74.143386
384.767350	29.370166	74.148391
383.780243	33.439938	74.153396
383.235603	35.354449	74.158401
383.296318	40.520398	74.163406
382.096132	46.625304	74.168410
381.484472	35.117869	74.173415
381.277859	43.519782	74.178420
380.192397	42.729241	74.183425
378.900197	32.517717	74.188430
378.062779	44.126783	74.193434
378.326772	36.764432	74.198439
377.625497	44.852510	74.203444
377.346941	39.257668	74.208449
376.665193	37.548077	74.213454
375.570532	45.806079	74.218458
375.201091	34.515515	74.223463
374.058900	43.102792	74.228468
373.045234	44.262564	74.233473
372.694334	37.649491	74.238478
372.267720	45.622836	74.243482
372.177521	33.426749	74.248487
371.150966	44.245934	74.253492
370.214404	42.345137	74.258497
369.923965	40.562149	74.263502
369.082125	42.265402	74.268506
368.521010	33.998475	74.273511
367.649423	47.409159	74.278516
366.862529	37.580741	74.283521
365.804495	42.999094	74.288526
364.751837	50.174916	74.293530
364.883331	38.944871	74.298535
364.504296	42.236497	74.303540
363.931077	43.685630	74.308545
363.754464	41.285254	74.313550
362.493312	42.367774	74.318554
361.842289	38.100178	74.323559
361.192327	46.445012	74.328564
360.077001	36.137500	74.333569
359.385409	46.384486	74.338574
358.600375	41.844929	74.343578
358.481759	35.636394	74.348583
358.008060	45.795037	74.353588
356.900624	47.059647	74.358593
356.195949	43.776745	74.363598
355.463921	51.661571	74.368602
355.425044	36.506794	74.373607
354.902466	42.866424	74.378612
353.615965	44.161149	74.383617
352.965276	42.542809	74.388622
352.320388	46.972800	74.393626
351.985955	35.887977	74.398631
351.131934	43.235571	74.403636
350.184340	41.573086	74.408641
349.857538	39.329113	74.413646
349.102893	45.687882	74.418650
349.021205	43.488424	74.423655
347.956584	47.972694	74.428660
347.422422	37.936847	74.433665
346.212490	38.274768	74.438670
345.381060	45.438990	74.443674
344.601240	51.663002	74.448679
344.316395	47.666636	74.453684
344.186845	46.920887	74.458689
343.698624	38.987704	74.463694
342.586456	51.924224	74.468698
342.163610	37.642782	74.473703
341.296868	44.583973	74.478708
340.553878	29.028908	74.483713
339.757817	31.475511	74.488718
338.822439	42.940923	74.493722
338.514273	37.838091	74.498727
338.369277	37.638858	74.503732
336.978129	32.114112	74.508737
336.335845	29.623953	74.513742
335.991358	38.776396	74.518746
335.489422	35.601541	74.523751
334.460640	42.795641	74.528756
333.489229	39.701917	74.533761
333.083599	33.983834	74.538766
332.386276	40.760827	74.543770
332.292431	37.222885	74.548775
331.630932	41.015277	74.553780
330.884934	36.278698	74.558785
330.175446	33.696748	74.563790
329.361652	42.712677	74.568794
328.469733	28.602204	74.573799
327.640250	38.541580	74.578804
327.179971	38.413098	74.583809
327.064376	29.524818	74.588814
325.978310	46.371212	74.593818
325.678063	39.201291	74.598823
324.898162	39.540070	74.603828
324.460072	33.611118	74.608833
323.211223	40.084928	74.613838
322.127806	48.639205	74.618842
322.282909	42.360237	74.623847
321.812510	39.673949	74.628852
320.617847	40.083566	74.633857
319.993583	36.975521	74.638862
319.174348	46.295100	74.643866
319.175261	36.984543	74.648871
317.950681	40.743680	74.653876
317.015786	39.344115	74.658881
316.620899	37.197732	74.663886
315.893003	36.052184	74.668890
315.702002	30.214741	74.673895
314.909649	39.621496	74.678900
313.832152	42.393665	74.683905
313.536259	37.318844	74.688910
312.522688	48.284215	74.693914
312.885170	41.645761	74.698919
311.424300	41.449679	74.703924
310.657800	36.435674	74.708929
310.503570	41.623261	74.713934
309.392700	42.498927	74.718938
308.532940	37.939761	74.723943
308.181767	39.410285	74.728948
307.676383	43.469539	74.733953
307.033462	35.357597	74.738958
306.131881	37.347939	74.743962
305.203890	33.026735	74.748967
304.511130	36.194904	74.753972
304.346248	37.761893	74.758977
303.898844	29.983071	74.763982
302.789488	39.150194	74.768986
302.415282	37.855234	74.773991
301.759457	40.684777	74.778996
300.894940	37.228674	74.784001
299.957415	34.433919	74.789006
299.067905	42.917870	74.794010
299.148335	34.832563	74.799015
298.611662	37.543766	74.804020
297.781226	35.610314	74.809025
296.963357	34.412880	74.814030
296.084170	40.875090	74.819034
295.775270	28.384292	74.824039
295.203212	39.015935	74.829044
294.022424	37.909464	74.834049
293.563607	35.120412	74.839054
293.182405	39.524153	74.844058
292.480129	33.727205	74.849063
291.546615	33.592158	74.854068
290.828261	36.108392	74.859073
290.443974	32.842255	74.864078
289.829188	30.410805	74.869082
288.884724	29.596255	74.874087
287.747735	27.689593	74.879092
287.099339	16.899276	74.884097
287.293631	33.959477	74.889102
286.844600	36.147352	74.894106
286.319867	31.960577	74.899111
285.196395	34.315880	74.904116
284.547272	33.293404	74.909121
283.675419	25.058694	74.914126
282.611733	39.403609	74.919130
282.343982	27.620624	74.924135
281.766013	29.996209	74.929140
281.442561	35.898325	74.934145
280.818396	37.857072	74.939150
279.641127	37.784538	74.944154
279.479325	34.730523	74.949159
278.451506	39.253105	74.954164
277.007438	38.251689	74.959169
276.716251	23.698558	74.964174
276.257525	30.745035	74.969178
275.660949	30.467976	74.974183
275.401073	31.482400	74.979188
274.741285	34.336235	74.984193
274.335381	29.302615	74.989198
273.131403	37.664806	74.994202
272.748619	34.669672	74.999207
271.451000	42.871751	75.004212
270.704751	39.636505	75.009217
270.626669	34.517512	75.014222
269.539066	39.546372	75.019226
269.480409	35.878245	75.024231
268.925569	39.117480	75.029236
267.751976	45.984601	75.034241
267.177445	39.541241	75.039246
266.482636	39.929553	75.044250
266.404154	26.772826	75.049255
264.993031	39.047378	75.054260
264.371291	41.152401	75.059265
263.877037	29.211557	75.064270
263.375504	36.947688	75.069274
262.514004	44.116725	75.074279
261.823582	40.366377	75.079284
260.970746	41.833296	75.084289
260.629155	39.471845	75.089294
260.153102	44.442649	75.094298
259.594955	45.337463	75.099303
258.803222	41.945467	75.104308
257.983954	45.695217	75.109313
257.332893	34.219341	75.114318
256.466563	45.058752	75.119322
255.889049	34.559912	75.124327
255.434859	41.014310	75.129332
254.981517	37.541566	75.134337
253.892715	33.460486	75.139342
253.036650	41.131710	75.144346
253.098539	30.220284	75.149351
252.318166	29.436362	75.154356
251.202832	35.945688	75.159361
250.382679	33.693644	75.164366
249.797967	36.611212	75.169370
249.666059	34.017640	75.174375
248.960274	41.292745	75.179380
247.957893	38.500464	75.184385
247.453639	31.922907	75.189390
247.370355	35.941689	75.194394
246.233260	38.430069	75.199399
245.389454	37.479640	75.204404
244.875861	38.890908	75.209409
244.537642	32.717394	75.214414
243.304485	39.994568	75.219418
242.788430	31.561225	75.224423
242.009450	36.167155	75.229428
241.312595	38.616897	75.234433
240.293363	25.627491	75.239438
239.208984	38.490214	75.244442
239.283203	34.826139	75.249447
238.783195	36.684678	75.254452
238.494298	32.375162	75.259457
238.206564	31.244626	75.264462
237.327468	39.379999	75.269466
236.849138	36.808536	75.274471
235.434304	39.115691	75.279476
234.516673	40.209745	75.284481
234.226594	25.355248	75.289486
233.765634	37.237065	75.294490
233.045072	33.682345	75.299495
232.242867	35.278398	75.304500
231.329963	45.297332	75.309505
231.100139	39.190118	75.314510
230.255653	36.943536	75.319514
229.257234	38.238130	75.324519
228.676563	38.876342	75.329524
227.860631	40.316888	75.334529
228.037623	40.230335	75.339534
227.331577	43.130982	75.344538
226.575617	36.456359	75.349543
225.776186	36.377233	75.354548
224.987598	42.104347	75.359553
224.440867	34.566886	75.364558
223.308794	42.086576	75.369562
222.812805	33.005060	75.374567
222.407815	39.174072	75.379572
221.802913	44.463470	75.384577
220.866314	31.218043	75.389582
220.151408	48.834779	75.394586
219.753242	34.797030	75.399591
219.447662	45.947603	75.404596
218.424026	37.412257	75.409601
217.652992	41.304139	75.414606
217.089689	39.164124	75.419610
216.758668	44.417744	75.424615
215.658979	40.013561	75.429620
214.850816	42.148315	75.434625
214.774169	41.080324	75.439630
213.294710	44.104276	75.444634
212.540544	42.239119	75.449639
211.994516	44.827251	75.454644
211.462698	50.582822	75.459649
211.485762	34.263859	75.464654
210.753399	51.239979	75.469658
209.936918	42.562798	75.474663
208.912412	36.689516	75.479668
208.414330	46.911984	75.484673
208.070624	40.550114	75.489678
207.121930	38.365886	75.494682
206.200529	40.525004	75.499687
205.541093	38.417665	75.504692
205.298484	43.105252	75.509697
204.947265	28.381933	75.514702
203.358116	39.724524	75.519706
203.004491	32.359712	75.524711
202.682934	36.906918	75.529716
202.105335	39.236731	75.534721
201.477748	34.586977	75.539726
200.182570	42.591577	75.544730
199.658066	43.509426	75.549735
199.404297	37.959550	75.554740
198.062082	48.122635	75.559745
197.567513	38.266607	75.564750
197.089542	39.069804	75.569754
196.425317	41.815555	75.574759
196.162946	35.727730	75.579764
195.543419	37.425557	75.584769
194.588998	26.769215	75.589774
193.742080	31.023285	75.594778
193.422965	24.496654	75.599783
192.793240	28.085310	75.604788
191.360502	35.995147	75.609793
191.053573	30.765990	75.614798
190.318417	42.262595	75.619802
190.285401	33.132507	75.624807
189.811790	29.838054	75.629812
188.707176	34.462799	75.634817
188.348611	28.467586	75.639822
187.549625	31.761530	75.644826
186.609499	35.333446	75.649831
185.770227	33.016664	75.654836
185.068236	46.155914	75.659841
184.898162	28.648760	75.664846
183.506488	37.427270	75.669850
183.202326	28.032908	75.674855
182.688750	27.307397	75.679860
182.129630	28.927786	75.684865
181.859906	36.491348	75.689870
180.872770	29.874105	75.694874
180.352611	42.839281	75.699879
179.652234	41.230490	75.704884
178.496236	39.891464	75.709889
177.845709	34.367005	75.714894
177.349359	39.667487	75.719898
176.816745	38.194376	75.724903
176.225664	38.898916	75.729908
174.697578	43.406682	75.734913
174.491056	36.705978	75.739918
174.041363	46.633726	75.744922
173.681208	31.998571	75.749927
173.407184	42.399783	75.754932
171.984404	45.406836	75.759937
171.766517	37.416409	75.764942
171.136526	37.857492	75.769946
169.776655	39.397399	75.774951
169.168909	32.069959	75.779956
168.345414	38.107006	75.784961
168.299246	27.930339	75.789966
167.702578	30.983871	75.794970
166.530669	37.861799	75.799975
166.262747	40.273131	75.804980
165.312243	44.982127	75.809985
164.792227	33.132154	75.814990
164.534397	33.837178	75.819994
163.512287	32.265499	75.824999
162.825044	28.169324	75.830004
162.123291	30.017465	75.835009
161.984442	26.962957	75.840014
160.648100	32.491991	75.845018
160.009845	36.892577	75.850023
159.497366	33.404053	75.855028
158.975506	36.726359	75.860033
158.414597	26.393647	75.865038
157.519205	41.489208	75.870042
156.779254	29.666424	75.875047
156.587254	31.862222	75.880052
155.482022	35.365857	75.885057
154.988121	29.674506	75.890062
154.449730	29.683093	75.895066
153.910195	32.661285	75.900071
153.372042	33.549780	75.905076
151.747850	34.723409	75.910081
151.302910	30.158090	75.915086
150.681360	30.296632	75.920090
150.512682	28.024326	75.925095
150.002273	28.859511	75.930100
148.645608	34.505334	75.935105
148.619701	23.260990	75.940110
147.764478	30.660865	75.945114
146.778722	33.440549	75.950119
146.021197	31.057130	75.955124
145.451660	35.115599	75.960129
145.017245	34.380627	75.965134
144.529670	32.737915	75.970138
143.725025	30.188545	75.975143
143.325203	26.413979	75.980148
142.419828	33.336148	75.985153
142.422376	29.581001	75.990158
141.528293	34.211618	75.995162
140.711080	29.751395	76.000167
139.920989	32.334301	76.005172
138.556023	35.901437	76.010177
137.780770	29.597360	76.015182
137.402374	32.877870	76.020186
137.105581	35.927747	76.025191
136.818940	29.766533	76.030196
135.812353	43.250827	76.035201
134.922065	28.622950	76.040206
134.098042	34.541817	76.045210
134.017202	41.130662	76.050215
133.748792	35.740829	76.055220
132.504705	42.594013	76.060225
131.930468	30.410498	76.065230
131.402976	32.555714	76.070234
130.419822	31.573930	76.075239
129.553054	30.724977	76.080244
128.809973	38.690455	76.085249
128.359189	34.455657	76.090254
128.264013	39.324743	76.095258
127.338582	38.532452	76.100263
126.707298	27.673227	76.105268
125.927358	43.381171	76.110273
125.499593	35.134059	76.115278
124.106375	34.837414	76.120282
123.454080	31.156727	76.125287
123.379658	29.265211	76.130292
122.515263	33.526821	76.135297
122.321196	25.354414	76.140302
121.348111	22.790911	76.145306
120.402510	31.654434	76.150311
120.255362	27.666115	76.155316
119.627656	41.052146	76.160321
118.641740	20.940659	76.165326
117.972560	30.543853	76.170330
117.099848	33.887422	76.175335
117.123107	22.196847	76.180340
115.884588	36.886655	76.185345
115.334515	23.983357	76.190350
114.640478	34.257573	76.195354
113.956456	30.597719	76.200359
112.728367	31.995216	76.205364
111.929128	40.050078	76.210369
112.009640	24.280228	76.215374
111.477032	26.891467	76.220378
111.053387	28.512345	76.225383
110.440880	25.101288	76.230388
109.344063	38.637820	76.235393
108.798055	36.890893	76.240398
108.154935	37.928601	76.245402
107.049904	34.326424	76.250407
106.571185	33.046587	76.255412
105.894751	38.926157	76.260417
105.753861	19.312288	76.265422
104.888664	29.897651	76.270426
104.067631	26.627083	76.275431
103.609224	30.368213	76.280436
102.820727	22.229103	76.285441
102.290692	23.464822	76.290446
101.604986	28.618888	76.295450
100.914929	21.866001	76.300455
100.241642	27.954802	76.305460
99.178428	31.415489	76.310465
98.548969	25.395687	76.315470
98.216444	32.131897	76.320474
97.604171	28.454299	76.325479
97.172811	25.793377	76.330484
95.820129	21.273486	76.335489
95.122761	23.174562	76.340494
94.661860	20.871592	76.345498
94.410047	24.999248	76.350503
93.559668	12.008241	76.355508
92.792531	18.474707	76.360513
92.430706	20.278118	76.365518
92.010465	25.468698	76.370522
90.741824	28.162627	76.375527
90.279045	32.428009	76.380532
89.100556	33.021241	76.385537
89.007518	29.756005	76.390542
88.516407	36.247848	76.395546
87.198238	35.081387	76.400551
87.021104	37.106083	76.405556
86.148611	29.319419	76.410561
85.755418	40.435074	76.415566
84.664932	36.045260	76.420570
83.864313	34.107130	76.425575
83.389035	28.972651	76.430580
83.384619	39.469636	76.435585
82.726371	32.773179	76.440590
81.384973	38.515950	76.445594
80.584792	31.009493	76.450599
80.504530	30.601255	76.455604
79.724173	30.072855	76.460609
78.989684	26.665491	76.465614
78.090298	32.568005	76.470618
77.495477	22.324311	76.475623
77.299855	19.077017	76.480628
76.468506	32.926033	76.485633
75.786977	24.550675	76.490638
75.093733	36.397005	76.495642
74.721009	33.815045	76.500647
74.041600	30.875140	76.505652
72.666865	34.219939	76.510657
72.318669	31.490564	76.515662
71.859761	31.218409	76.520666
70.696227	22.965658	76.525671
69.992700	20.827546	76.530676
69.119769	31.141337	76.535681
69.002031	25.852069	76.540686
68.388467	34.202181	76.545690
68.029668	40.154105	76.550695
67.680257	35.583031	76.555700
66.606497	35.677020	76.560705
66.174854	29.895339	76.565710
65.294024	27.545806	76.570714
64.080947	42.640012	76.575719
63.689904	30.859394	76.580724
62.943211	38.677228	76.585729
62.891642	29.345110	76.590734
61.684872	25.049551	76.595738
60.808186	32.500181	76.600743
60.362209	32.430971	76.605748
60.064951	33.974929	76.610753
59.469942	29.072442	76.615758
58.406350	32.361316	76.620762
57.688633	35.787418	76.625767
57.358740	27.586220	76.630772
56.512052	36.495490	76.635777
55.634318	30.783381	76.640782
54.498634	32.347520	76.645786
54.275487	32.621242	76.650791
54.369130	26.511358	76.655796
53.745749	35.034927	76.660801
53.132664	29.198609	76.665806
52.603229	35.986729	76.670810
51.205904	34.424479	76.675815
50.178493	33.557021	76.680820
49.294148	35.459546	76.685825
49.194432	28.789139	76.690830
48.796294	25.359679	76.695834
47.999512	33.964522	76.700839
47.195499	36.265822	76.705844
46.352031	39.160047	76.710849
46.029708	34.330766	76.715854
45.546468	25.431781	76.720858
44.637579	31.271165	76.725863
43.714584	23.960935	76.730868
43.390124	34.712386	76.735873
42.964900	34.117893	76.740878
41.773817	33.456317	76.745882
40.938042	33.378318	76.750887
40.438137	23.860670	76.755892
39.938882	34.326184	76.760897
39.698553	26.139091	76.765902
38.849063	30.830437	76.770906
37.765465	36.314489	76.775911
37.330683	32.963414	76.780916
37.063203	37.560357	76.785921
35.934208	34.159157	76.790926
34.871588	33.790910	76.795930
34.527380	38.732830	76.800935
34.369727	26.143864	76.805940
33.799757	40.203519	76.810945
32.636000	36.489319	76.815950
32.050322	31.198995	76.820954
31.314255	35.512706	76.825959
31.201145	29.427913	76.830964
30.184839	34.163217	76.835969
29.671479	27.830026	76.840974
29.186726	34.879106	76.845978
28.124226	30.710364	76.850983
27.355181	31.999991	76.855988
26.664596	35.259346	76.860993
26.278534	33.363924	76.865998
25.716490	31.764655	76.871002
24.282510	31.911388	76.876007
24.071751	31.987594	76.881012
23.170794	34.659181	76.886017
22.988861	31.753485	76.891022
22.865616	29.937570	76.896026
21.331561	35.028274	76.901031
20.943626	29.827839	76.906036
20.362410	35.118224	76.911041
19.408398	33.135197	76.916046
18.844101	32.528199	76.921050
18.016782	37.116668	76.926055
17.584785	32.109343	76.931060
17.086113	33.188690	76.936065
16.279102	29.215745	76.941070
15.515664	30.744180	76.946074
14.774605	39.061023	76.951079
14.609222	28.357762	76.956084
13.370109	40.436255	76.961089
12.679988	36.936678	76.966094
12.467495	31.038051	76.971098
11.962130	34.887611	76.976103
11.098916	27.347084	76.981108
10.008594	35.960912	76.986113
9.188335	33.633277	76.991118
9.356252	33.298996	76.996122
8.515817	39.354559	77.001127
7.965206	31.642742	77.006132
7.012380	35.394942	77.011137
6.418411	32.976020	77.016142
5.533091	36.791571	77.021147
4.587479	35.803850	77.026151
4.337107	31.838315	77.031156
4.064959	36.208921	77.036161