Fri Mar 05 19:01:18 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.087813	99.329824	0.000000
0.069529	91.478240	0.005005
-0.588204	59.867247	0.010010
-2.413942	17.782399	0.015014
-6.627731	5.367405	0.020019
-12.505193	13.907492	0.025024
-17.399694	11.469707	0.030029
-21.925271	8.709727	0.035034
-25.667445	13.588142	0.040038
-29.355069	2.530595	0.045043
-32.622009	9.935184	0.050048
-36.662985	11.973874	0.055053
-40.167782	9.065275	0.060058
-43.674641	11.884517	0.065062
-47.392211	6.286470	0.070067
-51.407992	22.586319	0.075072
-54.993338	9.216442	0.080077
-58.869660	15.423605	0.085082
-62.458948	16.956613	0.090086
-66.282319	9.801671	0.095091
-70.223535	13.789388	0.100096
-73.594320	6.313093	0.105101
-77.694537	6.345953	0.110106
-81.824756	7.675133	0.115110
-85.427305	5.594330	0.120115
-89.295430	15.502925	0.125120
-92.823476	6.796492	0.130125
-96.225043	7.402309	0.135130
-100.230806	-0.343213	0.140134
-103.817083	-4.150194	0.145139
-108.087595	0.323785	0.150144
-111.755789	-4.689099	0.155149
-115.977663	5.310667	0.160154
-119.751638	0.776721	0.165158
-123.261966	8.324339	0.170163
-127.031031	10.212557	0.175168
-130.519484	10.770785	0.180173
-134.378012	11.813850	0.185178
-138.122430	10.085348	0.190182
-141.682891	5.656136	0.195187
-145.487472	11.654864	0.200192
-149.206663	6.659635	0.205197
-153.130498	16.346979	0.210202
-156.898733	14.563959	0.215206
-160.788375	1.108781	0.220211
-164.714161	9.344076	0.225216
-167.877313	8.568381	0.230221
-171.754424	8.627297	0.235226
-175.964072	5.443455	0.240230
-179.873341	5.337205	0.245235
-183.430878	10.484432	0.250240
-186.860254	0.101870	0.255245
-190.439371	6.220799	0.260250
-194.508802	5.684395	0.265254
-197.949604	3.201057	0.270259
-202.004545	11.833915	0.275264
-205.538290	8.909681	0.280269
-209.612302	12.322726	0.285274
-213.299116	10.227180	0.290278
-216.966897	10.219642	0.295283
-220.806829	4.117854	0.300288
-224.411409	2.203167	0.305293
-228.177433	11.212576	0.310298
-232.256639	17.395619	0.315302
-235.933497	9.783912	0.320307
-239.984859	12.288220	0.325312
-243.444412	12.930307	0.330317
-246.954997	11.044804	0.335322
-251.143530	18.861706	0.340326
-254.427777	12.729619	0.345331
-258.572000	14.058181	0.350336
-262.333896	4.747522	0.355341
-265.993468	9.122677	0.360346
-269.834138	17.366629	0.365350
-273.480530	9.467844	0.370355
-277.494404	15.965383	0.375360
-281.186207	10.759411	0.380365
-284.489602	13.857176	0.385370
-288.877244	15.150531	0.390374
-292.251993	13.481530	0.395379
-295.846595	16.616337	0.400384
-299.583198	13.642625	0.405389
-303.446267	16.709914	0.410394
-307.340146	17.432469	0.415398
-311.050335	10.597333	0.420403
-315.190188	22.752652	0.425408
-319.069123	12.424709	0.430413
-322.485218	8.155651	0.435418
-325.943812	10.614352	0.440422
-329.953234	7.857711	0.445427
-334.007372	16.470153	0.450432
-337.124479	15.997990	0.455437
-341.028030	21.810969	0.460442
-345.011077	22.825364	0.465446
-348.617208	16.091944	0.470451
-352.632353	19.363364	0.475456
-356.356143	16.624239	0.480461
-360.014305	19.116431	0.485466
-363.799404	14.918965	0.490470
-367.590742	15.421817	0.495475
-371.368930	19.522757	0.500480
-374.943633	14.211503	0.505485
-378.990198	12.211504	0.510490
-382.726397	14.653111	0.515494
-386.208810	11.339330	0.520499
-390.259283	12.099638	0.525504
-393.829227	11.417583	0.530509
-397.582127	17.676525	0.535514
-401.219080	14.349595	0.540518
-404.829329	8.815408	0.545523
-409.050708	16.210462	0.550528
-412.583182	6.229484	0.555533
-416.718150	17.032734	0.560538
-420.389132	18.139346	0.565542
-424.032139	5.277602	0.570547
-428.112813	10.551296	0.575552
-431.657840	5.621748	0.580557
-435.463241	19.333911	0.585562
-439.081357	18.544499	0.590566
-442.511354	15.484203	0.595571
-446.446144	13.152656	0.600576
-450.105139	10.870111	0.605581
-454.060609	10.729109	0.610586
-457.920188	27.652749	0.615590
-461.662490	7.108250	0.620595
-465.771747	8.318043	0.625600
-469.138478	8.734319	0.630605
-472.799229	5.157416	0.635610
-476.743503	14.886365	0.640614
-480.414775	14.059775	0.645619
-484.222843	21.664912	0.650624
-487.826113	12.701450	0.655629
-491.615606	17.055115	0.660634
-495.648526	23.161812	0.665638
-499.083093	14.527812	0.670643
-503.004909	15.988427	0.675648
-506.645505	11.553650	0.680653
-510.424259	15.196000	0.685658
-514.545818	18.940423	0.690662
-517.655042	6.865626	0.695667
-521.949958	14.512312	0.700672
-525.602444	14.155875	0.705677
-529.230109	10.728316	0.710682
-533.424631	12.954783	0.715686
-536.785237	6.723341	0.720691
-540.958844	14.461068	0.725696
-544.462635	19.205991	0.730701
-547.735146	17.435869	0.735706
-551.733064	19.777619	0.740710
-555.645833	13.602867	0.745715
-559.627619	21.333641	0.750720
-563.236536	17.937830	0.755725
-566.666109	24.069683	0.760730
-570.848530	28.191354	0.765734
-574.651634	15.071578	0.770739
-578.542264	19.354803	0.775744
-582.065803	15.041791	0.780749
-585.400852	13.716950	0.785754
-589.670311	21.752349	0.790758
-593.203241	12.486085	0.795763
-596.982462	14.487042	0.800768
-600.883785	11.434474	0.805773
-604.352133	10.317037	0.810778
-608.441696	11.788855	0.815782
-611.636859	6.923535	0.820787
-615.770501	10.491863	0.825792
-619.704630	12.596453	0.830797
-623.608336	12.958394	0.835802
-627.383130	12.039763	0.840806
-631.054462	14.031421	0.845811
-634.773933	15.500921	0.850816
-638.173378	9.502914	0.855821
-641.898268	9.677042	0.860826
-646.105709	14.875160	0.865830
-649.455275	11.039078	0.870835
-653.643294	14.168306	0.875840
-657.366210	13.249319	0.880845
-661.147955	7.172087	0.885850
-664.837449	12.363167	0.890854
-668.049700	4.821426	0.895859
-672.309934	17.695136	0.900864
-676.436813	4.119510	0.905869
-679.808329	13.875519	0.910874
-683.710587	14.773489	0.915878
-687.545627	13.342613	0.920883
-691.220664	23.517729	0.925888
-694.877139	4.499040	0.930893
-698.603504	14.272357	0.935898
-702.174441	18.025298	0.940902
-705.516732	10.261540	0.945907
-710.153643	10.811759	0.950912
-713.976475	11.687624	0.955917
-717.448947	7.896515	0.960922
-720.832357	5.403196	0.965926
-724.315386	5.627109	0.970931
-728.823630	16.991989	0.975936
-732.511007	10.850907	0.980941
-736.164136	11.824264	0.985946
-740.183075	9.413622	0.990950
-743.687527	9.782912	0.995955
-747.706978	15.857903	1.000960
-751.116640	18.787205	1.005965
-755.287449	14.286178	1.010970
-759.446334	7.856229	1.015974
-762.982923	9.905399	1.020979
-766.442804	14.766621	1.025984
-769.736145	3.984753	1.030989
-773.606530	8.484245	1.035994
-777.631051	12.615723	1.040998
-781.088677	9.749580	1.046003
-785.195242	15.991520	1.051008
-788.819322	13.189842	1.056013
-792.660732	5.288381	1.061018
-796.545003	14.710194	1.066022
-799.874959	1.750160	1.071027
-803.745758	9.468306	1.076032
-807.549685	9.160169	1.081037
-811.444120	13.829147	1.086042
-815.511840	11.681897	1.091046
-819.117228	7.576301	1.096051
-822.787502	12.498043	1.101056
-826.549159	6.575571	1.106061
-830.049408	15.144421	1.111066
-834.076338	17.008734	1.116070
-837.525620	13.589411	1.121075
-841.913291	13.600153	1.126080
-845.341899	1.222083	1.131085
-849.002663	8.788452	1.136090
-853.371561	14.017470	1.141094
-856.468807	10.789476	1.146099
-860.135775	19.657835	1.151104
-863.908297	6.126836	1.156109
-867.750112	2.226273	1.161114
-871.944988	6.826686	1.166118
-875.398797	5.678943	1.171123
-879.196086	7.083996	1.176128
-882.558588	12.385549	1.181133
-886.172123	8.767059	1.186138
-890.463524	13.586364	1.191142
-894.446374	12.742431	1.196147
-898.212653	8.418258	1.201152
-901.706740	10.593301	1.206157
-905.403657	12.914320	1.211162
-909.499267	18.334709	1.216166
-912.935407	11.529281	1.221171
-916.897551	13.419645	1.226176
-920.810217	13.980627	1.231181
-924.114516	9.863322	1.236186
-928.006425	17.255461	1.241190
-931.729104	7.118074	1.246195
-935.396752	12.914769	1.251200
-939.210886	10.697225	1.256205
-943.064050	10.259987	1.261210
-947.216729	14.615667	1.266214
-950.169342	9.855539	1.271219
-954.422764	19.107975	1.276224
-958.408588	3.739425	1.281229
-961.979039	5.382724	1.286234
-965.913027	13.404542	1.291238
-969.584785	8.548135	1.296243
-973.584564	16.263523	1.301248
-976.574164	12.173236	1.306253
-980.622651	13.257506	1.311258
-984.657180	15.410293	1.316262
-988.194973	7.831193	1.321267
-992.274104	17.970444	1.326272
-995.951060	14.792775	1.331277
-999.145065	15.331990	1.336282
-1002.957117	14.052497	1.341286
-1006.721917	11.086013	1.346291
-1011.135164	14.545199	1.351296
-1015.126976	18.264993	1.356301
-1018.437687	10.416233	1.361306
-1022.098617	13.452339	1.366310
-1025.579151	9.978376	1.371315
-1029.337918	23.341754	1.376320
-1033.178331	16.246360	1.381325
-1037.122043	8.060489	1.386330
-1041.353536	27.586486	1.391334
-1044.743856	9.298539	1.396339
-1048.390579	21.298892	1.401344
-1052.032710	13.045881	1.406349
-1055.569098	11.050605	1.411354
-1059.807915	18.137325	1.416358
-1063.541207	18.879586	1.421363
-1067.446254	17.115185	1.426368
-1070.965043	16.001780	1.431373
-1074.558995	12.758921	1.436378
-1078.619734	17.533780	1.441382
-1082.546810	11.942545	1.446387
-1086.352086	17.610099	1.451392
-1089.840172	11.112873	1.456397
-1093.148115	-0.442015	1.461402
-1097.187718	14.768820	1.466406
-1101.002143	10.507879	1.471411
-1105.040858	18.636561	1.476416
-1108.613720	15.451881	1.481421
-1112.374568	6.320689	1.486426
-1115.787637	4.584896	1.491430
-1119.646543	2.559318	1.496435
-1124.070918	6.777422	1.501440
-1127.864965	15.638119	1.506445
-1131.263210	3.071148	1.511450
-1134.982182	8.501042	1.516454
-1138.190273	-2.245012	1.521459
-1142.456618	7.927585	1.526464
-1146.361260	9.208320	1.531469
-1150.050650	4.698803	1.536474
-1153.996439	16.130571	1.541478
-1157.469578	0.789178	1.546483
-1160.967419	8.356749	1.551488
-1164.912063	10.011342	1.556493
-1168.476292	3.622620	1.561498
-1172.750699	3.109665	1.566502
-1176.363201	13.992980	1.571507
-1180.533969	14.453771	1.576512
-1184.003598	9.554332	1.581517
-1187.495333	6.530261	1.586522
-1191.305438	10.817354	1.591526
-1194.687044	14.699999	1.596531
-1198.806388	16.336873	1.601536
-1202.697141	15.070305	1.606541
-1206.420196	13.964563	1.611546
-1210.279722	13.374246	1.616550
-1213.856128	9.042292	1.621555
-1217.709562	22.771174	1.626560
-1221.579105	18.336330	1.631565
-1225.022205	20.128381	1.636570
-1228.847392	28.207331	1.641574
-1232.551258	10.179607	1.646579
-1236.452038	15.903680	1.651584
-1240.312605	19.494039	1.656589
-1244.033215	16.355295	1.661594
-1248.062652	20.953547	1.666598
-1251.454567	10.995579	1.671603
-1255.087874	18.933471	1.676608
-1259.179492	24.262354	1.681613
-1263.320684	15.774178	1.686618
-1266.793830	22.074828	1.691622
-1270.291811	14.871424	1.696627
-1273.982947	7.475021	1.701632
-1277.455259	11.733418	1.706637
-1281.357388	14.266063	1.711642
-1285.393733	11.595812	1.716646
-1289.118536	9.490707	1.721651
-1293.066912	10.620995	1.726656
-1296.962893	11.891134	1.731661
-1300.507346	9.232062	1.736666
-1304.381693	17.128185	1.741670
-1307.863669	22.644993	1.746675
-1311.714825	15.269532	1.751680
-1315.370213	15.342144	1.756685
-1319.140236	13.526597	1.761690
-1323.096028	18.769192	1.766694
-1326.873320	13.673221	1.771699
-1330.430041	12.569439	1.776704
-1334.347909	25.559771	1.781709
-1337.787176	13.982120	1.786714
-1342.004046	19.123038	1.791718
-1345.646100	12.521554	1.796723
-1348.975671	7.240411	1.801728
-1353.170050	19.131755	1.806733
-1356.797871	4.873578	1.811738
-1360.622095	16.294095	1.816742
-1364.032408	10.732590	1.821747
-1368.209876	16.056477	1.826752
-1371.947930	9.669102	1.831757
-1375.898335	10.473429	1.836762
-1379.247284	17.465552	1.841766
-1382.977280	14.002115	1.846771
-1386.951444	20.834152	1.851776
-1390.654656	13.725300	1.856781
-1394.360907	5.287590	1.861786
-1398.611656	15.836602	1.866790
-1402.311877	10.815152	1.871795
-1405.680338	20.382414	1.876800
-1409.424400	18.684284	1.881805
-1413.186279	6.346295	1.886810
-1417.209203	16.551360	1.891814
-1421.009551	17.735434	1.896819
-1424.412496	19.338424	1.901824
-1428.304430	16.955959	1.906829
-1431.934814	9.863902	1.911834
-1436.088155	21.054967	1.916838
-1439.610354	14.983219	1.921843
-1443.374227	15.570139	1.926848
-1447.100381	22.575449	1.931853
-1450.905814	14.543215	1.936858
-1454.754552	17.441333	1.941862
-1458.205621	9.227792	1.946867
-1462.313099	13.192360	1.951872
-1465.986434	21.469710	1.956877
-1469.823150	15.385298	1.961882
-1473.649637	23.233030	1.966886
-1477.077850	12.866497	1.971891
-1480.891684	22.596647	1.976896
-1485.014973	18.732742	1.981901
-1488.293482	5.046472	1.986906
-1491.963030	6.298023	1.991910
-1495.937503	7.838106	1.996915
-1500.155307	14.746580	2.006912
-1500.893501	9.428477	2.016909
-1498.278682	5.946553	2.026906
-1495.137275	6.390831	2.036902
-1493.250931	7.375583	2.046899
-1491.763003	10.460987	2.056896
-1489.532861	8.025941	2.066893
-1487.633259	4.912779	2.076890
-1486.053507	6.871900	2.086886
-1484.046132	10.175702	2.096883
-1481.888314	6.474875	2.106880
-1480.042571	11.918780	2.116877
-1478.040184	11.942328	2.126874
-1476.197775	6.657802	2.136870
-1474.645357	6.312884	2.146867
-1472.525748	9.488197	2.156864
-1470.587254	3.981447	2.166861
-1468.379639	2.071083	2.176858
-1467.007613	9.119281	2.186854
-1465.223658	4.767811	2.196851
-1463.046517	6.452864	2.206848
-1460.940017	4.156067	2.216845
-1459.196389	0.005271	2.226842
-1457.284808	5.069175	2.236838
-1455.695263	13.519396	2.246835
-1453.693182	13.375645	2.256832
-1451.737389	8.950878	2.266829
-1449.883630	6.584034	2.276826
-1447.733705	3.522399	2.286822
-1446.071391	3.219903	2.296819
-1444.299462	7.770918	2.306816
-1442.373157	10.404054	2.316813
-1440.483270	3.558266	2.326810
-1438.619541	5.868265	2.336806
-1436.565165	11.136695	2.346803
-1434.885846	7.267791	2.356800
-1432.783040	10.060569	2.366797
-1431.021934	8.098577	2.376794
-1428.976561	5.221068	2.386790
-1427.349129	12.972084	2.396787
-1425.411279	8.272315	2.406784
-1423.407065	8.068250	2.416781
-1421.716244	-0.752496	2.426778
-1420.083332	4.941852	2.436774
-1417.748399	5.608524	2.446771
-1415.880656	7.232636	2.456768
-1413.994202	8.631121	2.466765
-1412.150206	8.465350	2.476762
-1410.416445	10.519867	2.486758
-1408.709546	8.129201	2.496755
-1406.582457	4.098625	2.506752
-1404.483186	10.522004	2.516749
-1402.859898	15.262644	2.526746
-1401.010444	11.960209	2.536742
-1399.288553	16.355064	2.546739
-1397.353948	13.563210	2.556736
-1395.226968	13.650567	2.566733
-1393.285426	13.874984	2.576730
-1391.262588	14.316914	2.586726
-1389.672280	11.886506	2.596723
-1387.943064	11.524393	2.606720
-1386.114220	15.354239	2.616717
-1383.987078	13.041572	2.626714
-1382.127210	15.142238	2.636710
-1380.096194	12.012857	2.646707
-1378.305448	11.448268	2.656704
-1376.430736	18.056052	2.666701
-1375.023586	16.158662	2.676698
-1372.874718	10.526727	2.686694
-1371.048613	12.729123	2.696691
-1368.941400	17.790213	2.706688
-1366.929093	12.791199	2.716685
-1365.041262	10.771073	2.726682
-1363.454220	13.790171	2.736678
-1361.541508	13.240807	2.746675
-1359.693114	13.682270	2.756672
-1357.583834	14.675656	2.766669
-1355.696998	10.710427	2.776666
-1353.914958	12.866207	2.786662
-1352.061620	12.094249	2.796659
-1350.468185	15.448651	2.806656
-1348.408434	6.202571	2.816653
-1346.277217	9.672990	2.826650
-1344.482993	10.674191	2.836646
-1342.826949	10.941196	2.846643
-1340.788466	12.116458	2.856640
-1339.167733	6.090675	2.866637
-1336.957086	16.514729	2.876634
-1335.337689	16.253920	2.886630
-1333.351898	15.587090	2.896627
-1331.440750	18.096434	2.906624
-1329.463713	12.458884	2.916621
-1327.670085	12.280716	2.926618
-1326.209421	20.544830	2.936614
-1323.872563	18.484437	2.946611
-1322.111963	13.481541	2.956608
-1320.392107	15.263617	2.966605
-1318.155998	19.378857	2.976602
-1316.130369	18.637770	2.986598
-1314.366577	12.628575	2.996595
-1312.929911	17.160734	3.006592
-1310.939591	16.273724	3.016589
-1308.811574	12.110451	3.026586
-1307.002529	15.902479	3.036582
-1305.157918	13.507212	3.046579
-1303.334101	20.661631	3.056576
-1301.649360	18.595115	3.066573
-1299.648448	16.594835	3.076570
-1297.506404	11.019320	3.086566
-1295.744207	11.485685	3.096563
-1293.954520	16.780829	3.106560
-1292.041544	16.203058	3.116557
-1290.221657	21.043371	3.126554
-1288.238091	17.485869	3.136550
-1286.405450	17.753071	3.146547
-1284.485904	13.503185	3.156544
-1282.492437	14.638336	3.166541
-1280.871006	14.795662	3.176538
-1278.884000	16.028166	3.186534
-1277.350451	18.616940	3.196531
-1275.168447	12.962417	3.206528
-1272.993973	8.995426	3.216525
-1271.459485	10.270362	3.226522
-1269.506294	7.950903	3.236518
-1267.659361	16.312709	3.246515
-1265.810230	17.717293	3.256512
-1263.805609	13.400123	3.266509
-1262.034856	18.728325	3.276506
-1259.934434	1.380507	3.286502
-1258.223568	14.396748	3.296499
-1256.302619	12.335092	3.306496
-1254.495633	11.826420	3.316493
-1252.738104	11.714088	3.326490
-1250.812196	14.491139	3.336486
-1249.033442	15.308576	3.346483
-1247.090409	11.786017	3.356480
-1245.154101	13.606141	3.366477
-1243.081722	11.048153	3.376474
-1241.427339	10.950758	3.386470
-1239.401330	13.937590	3.396467
-1237.674868	11.081281	3.406464
-1235.578683	14.211622	3.416461
-1233.817277	8.622869	3.426458
-1232.033622	2.375292	3.436454
-1230.120819	9.586581	3.446451
-1228.438471	8.951034	3.456448
-1226.397758	9.538670	3.466445
-1224.191513	7.614543	3.476442
-1222.586024	9.820786	3.486438
-1220.678142	14.921811	3.496435
-1218.813623	7.502348	3.506432
-1217.084696	9.894106	3.516429
-1215.097753	9.067718	3.526426
-1213.003687	19.643196	3.536422
-1211.212996	12.960290	3.546419
-1209.658397	14.249420	3.556416
-1207.724036	6.433523	3.566413
-1205.529927	6.263995	3.576410
-1203.867447	10.539037	3.586406
-1202.178505	20.007770	3.596403
-1200.158605	11.185025	3.606400
-1198.041969	14.847396	3.616397
-1196.365428	13.867009	3.626394
-1194.318445	10.629439	3.636390
-1192.491250	17.533938	3.646387
-1190.709278	19.606175	3.656384
-1188.801432	15.702449	3.666381
-1187.028507	19.328251	3.676378
-1184.761423	14.332828	3.686374
-1183.203884	11.656746	3.696371
-1181.344355	16.298173	3.706368
-1179.615116	12.874616	3.716365
-1177.725408	17.132268	3.726362
-1176.034470	21.656993	3.736358
-1173.799289	16.361945	3.746355
-1171.760667	17.777338	3.756352
-1170.201428	21.331556	3.766349
-1168.020847	15.724722	3.776346
-1166.381000	10.993890	3.786342
-1164.435876	18.451127	3.796339
-1162.366975	14.591125	3.806336
-1160.519540	8.653919	3.816333
-1158.554150	14.904752	3.826330
-1156.816841	5.839888	3.836326
-1155.135237	15.140884	3.846323
-1153.380451	6.584808	3.856320
-1151.291444	5.570038	3.866317
-1149.533883	2.677238	3.876314
-1147.345485	11.458201	3.886310
-1145.643731	9.996972	3.896307
-1143.832309	13.717701	3.906304
-1141.874635	10.025515	3.916301
-1139.867859	6.625477	3.926298
-1138.261740	9.491683	3.936294
-1136.207453	11.285129	3.946291
-1134.447716	2.963541	3.956288
-1132.463032	7.513930	3.966285
-1130.403809	5.641833	3.976282
-1128.931842	7.577399	3.986278
-1127.208375	13.975913	3.996275
-1125.093815	14.056032	4.006272
-1123.100756	13.481376	4.016269
-1121.189588	10.972970	4.026266
-1119.088662	9.833163	4.036262
-1117.567104	13.933448	4.046259
-1115.679697	10.835159	4.056256
-1113.761598	11.456722	4.066253
-1111.738046	13.907217	4.076250
-1109.981008	12.632959	4.086246
-1108.200213	13.342809	4.096243
-1106.413960	19.284453	4.106240
-1104.220847	9.805647	4.116237
-1102.189186	11.215899	4.126234
-1100.515998	8.658738	4.136230
-1098.835825	11.465758	4.146227
-1097.292953	11.792097	4.156224
-1094.801876	6.460924	4.166221
-1092.919115	10.910812	4.176218
-1091.207061	9.634291	4.186214
-1089.451315	13.193444	4.196211
-1087.606613	10.545696	4.206208
-1085.568870	8.039176	4.216205
-1083.336933	13.729539	4.226202
-1082.093721	11.730651	4.236198
-1080.031725	10.560791	4.246195
-1077.927713	11.891595	4.256192
-1076.149507	9.856076	4.266189
-1074.673785	5.825776	4.276186
-1072.428860	10.492486	4.286182
-1070.487694	8.981960	4.296179
-1068.680482	10.904991	4.306176
-1067.042518	9.733497	4.316173
-1065.026459	6.294141	4.326170
-1062.876993	5.247673	4.336166
-1061.177148	15.731625	4.346163
-1059.308938	16.043844	4.356160
-1057.445170	12.106218	4.366157
-1055.566325	7.406704	4.376154
-1053.799378	8.207232	4.386150
-1051.834005	10.856561	4.396147
-1049.655172	6.061699	4.406144
-1048.370214	16.004127	4.416141
-1046.231778	5.154108	4.426138
-1044.158506	8.593032	4.436134
-1042.377253	11.224451	4.446131
-1040.600284	11.811807	4.456128
-1038.639369	8.052869	4.466125
-1036.863891	9.752052	4.476122
-1034.941320	4.167660	4.486118
-1033.122473	13.716805	4.496115
-1031.104630	16.956186	4.506112
-1029.473686	11.227387	4.516109
-1027.221507	6.106600	4.526106
-1025.429947	11.850090	4.536102
-1023.960826	11.357741	4.546099
-1021.908047	9.650981	4.556096
-1020.077948	6.107193	4.566093
-1018.096524	13.394544	4.576090
-1015.878865	10.660357	4.586086
-1014.377531	10.521286	4.596083
-1012.451373	13.484819	4.606080
-1010.537990	8.901395	4.616077
-1008.354784	9.569066	4.626074
-1006.702613	10.089564	4.636070
-1005.157521	5.062940	4.646067
-1002.896836	4.851375	4.656064
-1001.412450	14.695622	4.666061
-999.235689	6.987955	4.676058
-997.372200	7.247293	4.686054
-995.625624	8.276915	4.696051
-993.776130	10.218506	4.706048
-991.652188	6.779326	4.716045
-990.136148	9.290569	4.726042
-988.064491	7.978716	4.736038
-986.045946	5.104295	4.746035
-984.137128	8.032729	4.756032
-982.355328	8.649357	4.766029
-980.500807	5.714329	4.776026
-979.022205	2.664159	4.786022
-977.021251	7.054190	4.796019
-974.916499	12.280263	4.806016
-972.861564	9.720562	4.816013
-971.547797	11.493634	4.826010
-968.997067	6.479893	4.836006
-967.387567	9.929897	4.846003
-965.616445	11.149828	4.856000
-963.524135	6.102034	4.865997
-961.800578	8.396951	4.875994
-959.764416	8.865550	4.885990
-958.060649	6.909918	4.895987
-956.118180	14.628296	4.905984
-954.253391	13.865874	4.915981
-952.425486	13.883042	4.925978
-950.298285	8.992311	4.935974
-948.579423	12.543263	4.945971
-946.806422	14.985024	4.955968
-945.150544	15.992873	4.965965
-943.050776	8.728620	4.975962
-940.778698	8.845297	4.985958
-939.262386	14.306029	4.995955
-937.510239	12.997944	5.005952
-935.326949	14.194622	5.015949
-933.706722	19.190319	5.025946
-931.630949	14.246247	5.035942
-929.778080	17.374730	5.045939
-928.174593	22.101527	5.055936
-926.056833	14.962305	5.065933
-924.326412	17.425104	5.075930
-922.150163	17.372384	5.085926
-920.721723	14.117107	5.095923
-918.832314	19.731357	5.105920
-916.769641	17.838365	5.115917
-914.804415	14.088309	5.125914
-913.007762	12.046804	5.135910
-910.905823	19.449198	5.145907
-909.474096	24.887165	5.155904
-907.326563	12.332097	5.165901
-905.596299	16.640740	5.175898
-903.584001	11.706841	5.185894
-901.492461	15.484033	5.195891
-899.732239	12.526248	5.205888
-897.949967	15.427622	5.215885
-896.208817	14.468697	5.225882
-894.328253	13.189058	5.235878
-892.509626	19.972027	5.245875
-890.373637	20.429462	5.255872
-888.334171	18.830734	5.265869
-886.733223	13.476298	5.275866
-884.968889	16.854239	5.285862
-882.801184	12.362881	5.295859
-881.077338	9.729877	5.305856
-879.279507	13.972474	5.315853
-877.384789	11.239520	5.325850
-875.290213	9.835678	5.335846
-873.545800	5.622010	5.345843
-871.857513	14.135847	5.355840
-869.677999	10.477884	5.365837
-868.080336	3.091865	5.375834
-866.153915	6.532326	5.385830
-864.177833	4.670593	5.395827
-862.522339	9.098591	5.405824
-860.144999	6.400598	5.415821
-858.534065	6.065682	5.425818
-856.629778	6.467032	5.435814
-854.842584	12.626628	5.445811
-852.916166	16.370264	5.455808
-851.018874	9.097404	5.465805
-849.435743	9.362207	5.475802
-847.254462	8.506639	5.485798
-845.383437	11.722289	5.495795
-843.357840	7.686322	5.505792
-841.978933	7.210088	5.515789
-839.921479	7.727493	5.525786
-837.748438	4.880602	5.535782
-835.880387	4.226700	5.545779
-834.036301	6.804027	5.555776
-832.264239	9.380239	5.565773
-830.576565	9.830450	5.575770
-828.264573	10.130330	5.585766
-826.631347	10.969778	5.595763
-824.891027	5.365732	5.605760
-823.141461	6.642903	5.615757
-821.278811	14.491008	5.625754
-818.961943	3.974228	5.635750
-817.091496	11.142135	5.645747
-815.717997	3.335660	5.655744
-813.580565	5.987691	5.665741
-811.851164	7.380201	5.675738
-809.680865	5.722732	5.685734
-808.021583	7.925408	5.695731
-805.674154	11.579678	5.705728
-803.922248	14.612297	5.715725
-802.269379	15.601781	5.725722
-800.398401	8.835275	5.735718
-798.551299	13.745856	5.745715
-796.680551	12.317862	5.755712
-794.662682	11.328988	5.765709
-793.027734	12.656084	5.775706
-790.587335	9.605444	5.785702
-789.425267	7.228093	5.795699
-787.345071	4.004506	5.805696
-785.484666	9.902980	5.815693
-783.555660	3.932483	5.825690
-781.460585	6.531314	5.835686
-779.810601	4.963356	5.845683
-777.637255	5.639135	5.855680
-776.252722	6.290998	5.865677
-774.048485	1.978638	5.875674
-772.341702	2.852156	5.885670
-770.242348	2.923973	5.895667
-768.434771	3.331379	5.905664
-766.708306	2.722267	5.915661
-764.487685	0.831004	5.925658
-762.679471	-0.831707	5.935654
-761.337128	3.848525	5.945651
-759.317448	7.087854	5.955648
-757.066824	6.567079	5.965645
-755.380512	6.884928	5.975642
-753.455727	5.533595	5.985638
-751.484268	4.694283	5.995635
-749.683779	3.964404	6.005632
-747.834770	2.175182	6.015629
-746.294868	2.342753	6.025626
-744.014371	7.228321	6.035622
-742.206980	-1.348521	6.045619
-740.173694	8.731875	6.055616
-738.506028	9.403247	6.065613
-736.618466	4.678895	6.075610
-734.895823	6.820971	6.085606
-732.979686	5.529458	6.095603
-730.843803	1.551748	6.105600
-729.054369	5.729489	6.115597
-727.188434	8.202358	6.125594
-725.092688	5.028444	6.135590
-723.397715	6.358627	6.145587
-721.898439	4.682161	6.155584
-719.856056	3.918383	6.165581
-717.603245	6.032585	6.175578
-715.859754	1.523908	6.185574
-714.354360	5.442315	6.195571
-712.181694	8.811976	6.205568
-710.345304	6.079000	6.215565
-708.595745	7.256784	6.225562
-706.798190	10.646923	6.235558
-704.483428	11.327013	6.245555
-702.626940	5.319218	6.255552
-701.044204	8.933167	6.265549
-699.103085	11.067199	6.275546
-697.168534	3.550075	6.285542
-695.384088	6.167046	6.295539
-693.336546	10.497783	6.305536
-691.349448	13.134479	6.315533
-689.785547	11.111386	6.325530
-687.822205	6.843912	6.335526
-685.869194	8.451839	6.345523
-684.016344	7.131004	6.355520
-682.535946	5.272840	6.365517
-680.385491	12.402438	6.375514
-678.243772	5.802758	6.385510
-676.623674	4.838073	6.395507
-674.837077	8.307357	6.405504
-672.602648	12.437722	6.415501
-670.937099	12.719476	6.425498
-669.113708	8.457012	6.435494
-667.270005	7.848186	6.445491
-665.416915	1.651486	6.455488
-663.374329	5.610405	6.465485
-661.522781	7.976678	6.475482
-659.370733	5.850150	6.485478
-657.713288	6.382685	6.495475
-656.211719	8.520671	6.505472
-654.388212	16.678340	6.515469
-651.888295	10.924612	6.525466
-650.186202	9.056307	6.535462
-648.344437	14.245766	6.545459
-646.527987	14.838166	6.555456
-644.446642	10.885032	6.565453
-642.689675	13.239592	6.575450
-641.150984	8.531579	6.585446
-638.967077	7.781573	6.595443
-636.904598	6.798337	6.605440
-635.297151	7.353086	6.615437
-633.631850	14.876043	6.625434
-631.328547	6.636881	6.635430
-629.788906	9.291439	6.645427
-627.841688	11.168764	6.655424
-625.834076	8.812709	6.665421
-624.012239	9.090051	6.675418
-622.020436	3.745965	6.685414
-620.405891	3.653794	6.695411
-618.464135	11.562069	6.705408
-616.258773	12.054459	6.715405
-614.795288	7.500586	6.725402
-612.943127	8.756788	6.735398
-610.729534	6.748366	6.745395
-608.922545	5.269125	6.755392
-607.242502	10.626562	6.765389
-605.208542	14.293227	6.775386
-603.879775	8.838767	6.785382
-601.784212	15.094571	6.795379
-599.237277	12.128154	6.805376
-597.551941	9.656240	6.815373
-595.992305	8.428108	6.825370
-593.943872	12.551950	6.835366
-591.999132	5.476964	6.845363
-590.153700	10.045350	6.855360
-588.346876	9.246685	6.865357
-586.377192	12.432577	6.875354
-584.492102	2.506040	6.885350
-582.852355	7.947302	6.895347
-580.884439	10.250838	6.905344
-578.743148	15.378293	6.915341
-577.185144	4.671899	6.925338
-575.578927	3.291074	6.935334
-573.113368	7.634088	6.945331
-571.656135	3.450717	6.955328
-569.416731	8.873561	6.965325
-567.772338	3.875546	6.975322
-565.936737	10.338704	6.985318
-563.917416	10.121907	6.995315
-562.279815	10.602416	7.005312
-560.300547	10.927290	7.015309
-558.308596	10.517500	7.025306
-556.214791	-0.350263	7.035302
-554.631764	1.834777	7.045299
-552.759390	11.866851	7.055296
-550.643815	16.090536	7.065293
-549.551030	12.527506	7.075290
-547.263931	8.955275	7.085286
-544.706116	5.865598	7.095283
-543.670670	9.347607	7.105280
-541.408758	13.358447	7.115277
-539.626283	8.674712	7.125274
-537.634171	12.187068	7.135270
-535.822113	5.787010	7.145267
-533.719268	11.272757	7.155264
-532.388831	9.304426	7.165261
-530.369218	8.200232	7.175258
-528.196437	4.985758	7.185254
-526.606566	9.609229	7.195251
-524.306377	5.253340	7.205248
-522.475921	11.832621	7.215245
-521.010746	8.765918	7.225242
-519.097912	11.098833	7.235238
-516.884594	9.456860	7.245235
-515.181635	10.171702	7.255232
-513.678012	11.685762	7.265229
-511.356728	13.830283	7.275226
-509.575716	15.671098	7.285222
-507.652726	12.706541	7.295219
-505.866037	15.858574	7.305216
-503.962511	16.644021	7.315213
-502.052368	6.214583	7.325210
-500.004182	10.486972	7.335206
-498.149546	15.379233	7.345203
-496.471030	12.914792	7.355200
-494.905288	17.790042	7.365197
-492.704892	10.519554	7.375194
-490.756559	11.345223	7.385190
-488.843036	10.843805	7.395187
-487.122498	12.534820	7.405184
-485.021406	9.565520	7.415181
-483.251775	10.743426	7.425178
-481.403718	5.054508	7.435174
-479.594108	12.148740	7.445171
-477.763185	11.589470	7.455168
-475.585060	8.978933	7.465165
-473.804715	16.256270	7.475162
-471.980941	10.661236	7.485158
-470.207340	8.551106	7.495155
-468.369610	11.406064	7.505152
-466.525642	4.849377	7.515149
-464.686596	10.708904	7.525146
-462.347762	8.491139	7.535142
-460.803531	7.211869	7.545139
-459.071817	4.828960	7.555136
-456.815556	6.085485	7.565133
-454.956246	6.052232	7.575130
-453.201400	3.182469	7.585126
-451.505979	7.961245	7.595123
-449.556425	10.326248	7.605120
-447.399588	9.921797	7.615117
-445.880786	6.840257	7.625114
-443.698548	7.410713	7.635110
-442.016804	8.492158	7.645107
-440.148504	7.459573	7.655104
-438.506758	11.387973	7.665101
-436.459860	11.735309	7.675098
-434.475997	7.977920	7.685094
-432.707140	8.901774	7.695091
-430.765078	14.427507	7.705088
-428.898963	8.334683	7.715085
-427.023851	19.410137	7.725082
-425.170600	16.892576	7.735078
-423.060278	13.743431	7.745075
-421.421013	10.680564	7.755072
-419.430895	12.555950	7.765069
-417.568304	10.815337	7.775066
-415.498669	5.509508	7.785062
-413.900406	11.799113	7.795059
-412.165764	15.760068	7.805056
-410.200472	17.314160	7.815053
-408.334321	14.069805	7.825050
-406.597818	10.399307	7.835046
-404.276601	15.518724	7.845043
-402.339237	11.569835	7.855040
-400.938768	18.732627	7.865037
-398.795791	15.924082	7.875034
-397.124688	10.615588	7.885030
-394.926910	13.482588	7.895027
-393.408630	10.878012	7.905024
-391.120416	8.507342	7.915021
-389.401009	15.083942	7.925018
-387.659652	13.053231	7.935014
-385.752144	14.093931	7.945011
-384.076089	13.842096	7.955008
-382.085593	14.770072	7.965005
-380.149928	11.429375	7.975002
-378.083035	14.860456	7.984998
-376.381758	11.007705	7.994995
-374.250668	13.272732	8.004992
-372.575631	12.323163	8.014989
-370.591089	15.150022	8.024986
-368.731251	13.703574	8.034982
-367.082321	13.023444	8.044979
-365.300620	13.094233	8.054976
-363.011186	15.769784	8.064973
-361.132450	8.010758	8.074970
-359.618225	17.064390	8.084966
-357.761254	14.039436	8.094963
-355.761309	19.721787	8.104960
-353.734725	12.171267	8.114957
-352.098615	16.425899	8.124954
-350.005074	9.696811	8.134950
-348.029422	11.735623	8.144947
-346.536745	15.498415	8.154944
-344.268123	18.189940	8.164941
-342.647332	15.054283	8.174938
-340.829287	12.270823	8.184934
-338.570805	14.468175	8.194931
-336.821732	14.075240	8.204928
-335.116021	12.928165	8.214925
-333.241459	14.556808	8.224922
-331.466449	13.144457	8.234918
-329.504726	18.237661	8.244915
-327.442006	16.883592	8.254912
-325.651096	13.662364	8.264909
-323.832337	6.457685	8.274906
-322.151710	16.479529	8.284902
-320.005705	6.096244	8.294899
-318.330098	10.251435	8.304896
-316.270536	10.252637	8.314893
-314.320108	9.402829	8.324890
-312.389769	13.174721	8.334886
-310.508142	10.744297	8.344883
-308.664550	14.260037	8.354880
-306.900681	12.986853	8.364877
-305.468563	18.074625	8.374874
-303.465728	7.032093	8.384870
-301.146382	21.436269	8.394867
-299.459062	18.062646	8.404864
-297.459193	16.578107	8.414861
-295.594859	12.344111	8.424858
-293.589288	15.857690	8.434854
-292.068816	11.697538	8.444851
-290.136072	13.549035	8.454848
-288.255951	17.575285	8.464845
-286.236716	17.800849	8.474842
-284.204479	21.774398	8.484838
-282.600306	14.136623	8.494835
-280.617564	14.353806	8.504832
-279.128331	13.405541	8.514829
-276.898915	10.736463	8.524826
-274.868657	15.463505	8.534822
-273.052788	13.692563	8.544819
-271.257304	14.512813	8.554816
-269.244139	16.935711	8.564813
-267.518616	14.193916	8.574810
-265.675858	13.722919	8.584807
-263.741953	10.704703	8.594803
-262.193037	19.405495	8.604800
-259.917120	14.472658	8.614797
-257.914589	12.324558	8.624794
-256.154234	16.167843	8.634791
-254.541410	20.577846	8.644787
-252.441699	14.231539	8.654784
-250.655810	11.532227	8.664781
-248.932723	12.847214	8.674778
-247.148378	7.631270	8.684775
-244.793268	8.779061	8.694771
-243.279479	15.592285	8.704768
-241.252827	11.779269	8.714765
-239.146361	6.605074	8.724762
-237.467388	13.377724	8.734759
-235.837225	14.041227	8.744755
-233.508614	14.978519	8.754752
-231.812900	17.442645	8.764749
-230.164123	13.421525	8.774746
-228.076760	14.045218	8.784743
-226.106016	13.959619	8.794739
-224.414545	11.905406	8.804736
-222.967123	19.809256	8.814733
-220.608345	24.676550	8.824730
-218.391605	25.451711	8.834727
-216.785108	15.497247	8.844723
-215.038101	16.978971	8.854720
-213.206892	19.089901	8.864717
-211.076359	16.332451	8.874714
-209.427566	16.374041	8.884711
-207.470292	13.701091	8.894707
-205.784000	14.922508	8.904704
-203.827836	17.709829	8.914701
-201.802534	13.158100	8.924698
-199.652620	14.589742	8.934695
-197.960443	18.139212	8.944691
-195.987929	9.886904	8.954688
-194.233000	15.804295	8.964685
-192.545012	8.547942	8.974682
-190.710011	9.082467	8.984679
-188.747060	8.087075	8.994675
-186.780809	11.995449	9.004672
-185.001927	10.157842	9.014669
-182.746056	9.249920	9.024666
-181.251311	1.615463	9.034663
-179.425065	4.556169	9.044659
-177.559019	10.103726	9.054656
-175.655356	4.308254	9.064653
-173.663500	3.001941	9.074650
-171.714366	1.130859	9.084647
-170.047960	2.350737	9.094643
-168.396107	3.460831	9.104640
-166.268366	8.486627	9.114637
-164.336003	9.998809	9.124634
-162.326207	3.960616	9.134631
-160.575665	4.870227	9.144627
-158.682874	9.750363	9.154624
-156.860478	6.664760	9.164621
-155.041533	3.914452	9.174618
-153.053712	9.189961	9.184615
-150.989983	5.536894	9.194611
-149.213960	6.290866	9.204608
-147.332200	7.166915	9.214605
-145.640342	8.512225	9.224602
-143.720413	8.355854	9.234599
-141.891023	9.780274	9.244595
-140.115682	10.518572	9.254592
-138.464091	13.821925	9.264589
-136.086990	6.768281	9.274586
-134.035035	2.856576	9.284583
-132.600195	4.190802	9.294579
-130.578921	11.084178	9.304576
-128.677863	7.785513	9.314573
-126.517477	11.176637	9.324570
-125.146192	12.735749	9.334567
-123.138577	8.430068	9.344563
-120.920441	8.322448	9.354560
-119.331944	12.619584	9.364557
-117.402086	15.261172	9.374554
-115.304245	7.626832	9.384551
-113.845070	8.164541	9.394547
-111.896218	11.748908	9.404544
-109.980662	12.788545	9.414541
-108.202782	10.322721	9.424538
-106.173171	10.079404	9.434535
-103.963292	6.875169	9.444531
-102.491729	12.266256	9.454528
-100.508281	14.256664	9.464525
-98.485449	17.061857	9.474522
-97.071069	14.205611	9.484519
-94.828490	15.958885	9.494515
-93.046272	24.497843	9.504512
-90.951239	22.931970	9.514509
-89.155518	19.724351	9.524506
-87.398114	19.098157	9.534503
-85.647291	14.907687	9.544499
-83.749890	21.820876	9.554496
-81.592723	20.091937	9.564493
-80.154381	18.210842	9.574490
-78.039949	18.400865	9.584487
-76.310821	18.893948	9.594483
-74.237300	18.242592	9.604480
-72.239591	19.002306	9.614477
-70.551159	19.580835	9.624474
-68.535306	12.674886	9.634471
-66.903374	17.498824	9.644467
-64.867864	19.141477	9.654464
-63.045316	20.235465	9.664461
-61.259014	24.464771	9.674458
-59.037925	11.571764	9.684455
-57.326687	14.864081	9.694451
-55.693902	23.540596	9.704448
-53.729563	24.692499	9.714445
-51.778500	15.153690	9.724442
-49.835169	11.204117	9.734439
-47.866231	10.452624	9.744435
-46.068686	11.528508	9.754432
-44.434963	12.823164	9.764429
-42.337974	16.852914	9.774426
-40.238111	11.642037	9.784423
-38.767431	14.502210	9.794419
-36.969778	15.601769	9.804416
-35.022178	14.147888	9.814413
-32.793601	18.950879	9.824410
-31.001794	10.517515	9.834407
-29.516028	20.292784	9.844403
-27.408993	16.861858	9.854400
-25.409218	15.552822	9.864397
-23.683907	19.158715	9.874394
-21.831811	10.892584	9.884391
-19.543981	12.649763	9.894387
-17.991821	17.058559	9.904384
-16.295282	18.734801	9.914381
-14.210089	16.622659	9.924378
-12.337547	12.136501	9.934375
-10.488659	13.906867	9.944371
-8.814054	24.274147	9.954368
-6.855445	26.510182	9.964365
-5.101366	39.969071	9.974362
-3.880369	58.816809	9.984359
-2.360222	99.662644	9.994355
-0.859357	154.938918	10.004352
0.000000	192.094753	10.009357
0.617009	222.547142	10.014362
1.432577	259.135508	10.019367
1.541291	294.143035	10.024371
2.207897	303.706797	10.029376
2.505890	339.184145	10.034381
2.471575	346.798614	10.039386
3.212997	349.036375	10.044391
3.132244	377.696964	10.049395
3.349950	380.716881	10.054400
3.314034	391.988686	10.059405
3.573811	397.840495	10.064410
3.455108	394.000513	10.069415
3.315739	400.514463	10.074419
3.237050	397.690782	10.079424
3.494592	414.325692	10.084429
3.633354	433.397902	10.089434
4.047598	430.824389	10.094439
3.780902	451.490994	10.099443
4.001260	440.632860	10.104448
3.988611	451.172424	10.109453
4.013371	445.715191	10.114458
4.139971	446.229602	10.119463
4.239262	459.764973	10.124467
4.397354	455.715236	10.129472
4.315683	453.711274	10.134477
3.646576	454.093983	10.139482
4.161637	461.507333	10.144487
3.882806	463.573534	10.149491
3.570592	459.508927	10.154496
4.086777	477.547978	10.159501
4.585671	483.568267	10.164506
4.780045	491.121099	10.169511
4.694961	506.616184	10.174515
4.748286	499.798145	10.179520
4.751384	506.205047	10.184525
4.635005	501.308068	10.189530
4.837285	500.580340	10.194535
4.776923	510.673379	10.199539
4.882437	502.451359	10.204544
4.978973	507.834070	10.209549
4.958095	514.814101	10.214554
5.020598	508.884028	10.219559
4.887454	517.059997	10.224563
5.352467	512.775198	10.229568
5.002032	512.370611	10.234573
5.224980	521.014924	10.239578
5.295988	514.526807	10.244583
5.165580	527.187368	10.249587
5.286048	523.432207	10.254592
5.229000	521.105752	10.259597
5.547271	520.938284	10.264602
5.317038	522.107305	10.269607
4.975268	528.299559	10.274611
4.941463	524.043862	10.279616
5.139671	530.720861	10.284621
4.818193	536.988732	10.289626
5.018282	553.144880	10.294631
5.399567	562.296993	10.299635
5.751869	562.349610	10.304640
5.661622	569.638789	10.309645
5.722417	568.763309	10.314650
5.856371	570.467200	10.319655
5.538609	573.567842	10.324659
5.618662	570.637589	10.329664
5.713183	580.306984	10.334669
5.827055	596.409121	10.339674
6.416880	596.586284	10.344679
6.330832	599.977990	10.349683
6.263478	605.867871	10.354688
6.392455	610.180956	10.359693
6.420426	601.094424	10.364698
6.306628	600.913872	10.369703
6.431422	606.634326	10.374707
6.604217	601.270121	10.379712
6.182475	589.309456	10.384717
6.369213	607.204094	10.389722
6.430855	605.044780	10.394727
6.379585	614.921966	10.399731
6.597491	607.784297	10.404736
6.316030	619.992773	10.409741
6.480640	614.700835	10.414746
6.531124	612.188470	10.419751
6.428503	627.128214	10.424755
6.666770	624.894990	10.429760
6.859422	615.335883	10.434765
6.487700	620.053705	10.439770
6.703371	627.398199	10.444775
7.085741	649.708892	10.449779
7.206521	649.183401	10.454784
7.047553	657.029237	10.459789
7.172851	666.919296	10.464794
7.260422	657.529895	10.469799
7.019242	666.650472	10.474803
7.267456	662.909593	10.479808
6.827765	664.578837	10.484813
7.084541	666.357770	10.489818
7.314217	670.978100	10.494823
7.380825	668.693400	10.499827
7.452027	676.709122	10.504832
7.673231	675.672423	10.509837
7.547290	669.233001	10.514842
7.633573	671.658902	10.519847
7.525224	673.084473	10.524851
7.546688	670.157237	10.529856
7.564346	666.833198	10.534861
7.574467	672.461578	10.539866
7.642403	679.261933	10.544871
7.795886	700.694538	10.549875
7.971190	710.026266	10.554880
7.861036	710.486983	10.559885
7.805348	713.495385	10.564890
7.993523	715.654292	10.569895
7.761900	717.689342	10.574899
7.824043	716.006196	10.579904
8.011100	717.392535	10.584909
7.987971	716.686560	10.589914
8.249726	719.556012	10.594919
8.171406	717.401661	10.599923
8.354957	719.168624	10.604928
8.094396	725.595601	10.609933
8.215927	728.864334	10.614938
8.905473	734.545219	10.619943
8.596740	739.983199	10.624947
8.628672	727.360241	10.629952
8.493528	726.232140	10.634957
8.349216	740.227699	10.639962
8.737233	752.756872	10.644967
8.711074	759.107048	10.649971
9.007983	759.264702	10.654976
8.786942	762.525006	10.659981
8.680742	769.323217	10.664986
8.796238	768.175634	10.669991
8.640615	768.485902	10.674995
8.802939	761.729206	10.680000
9.006238	760.701666	10.685005
8.772306	773.631280	10.690010
9.122600	769.342629	10.695015
8.797091	769.375628	10.700019
8.914908	765.944121	10.705024
8.953179	788.101746	10.710029
8.930169	798.310458	10.715034
9.407217	799.240517	10.720039
9.284986	811.833785	10.725043
9.111403	810.997254	10.730048
9.032366	811.161258	10.735053
9.067243	815.036802	10.740058
9.314733	814.863275	10.745063
9.584620	837.471337	10.750067
9.915194	839.640667	10.755072
9.380201	847.606513	10.760077
9.368318	850.819280	10.765082
9.542311	847.345676	10.770087
9.531691	854.809964	10.775091
9.683446	845.575794	10.780096
9.737849	846.991191	10.785101
9.691557	844.391715	10.790106
9.818850	843.865179	10.795111
9.718094	867.073336	10.800115
10.048957	870.037457	10.805120
10.093552	876.448942	10.810125
10.106812	884.720042	10.815130
10.255859	890.685913	10.820135
10.299237	890.311541	10.825139
10.189531	896.257184	10.830144
10.400346	892.474901	10.835149
10.243491	894.647869	10.840154
10.321033	890.595090	10.845159
10.318649	902.841292	10.850163
10.308041	893.027402	10.855168
10.560988	895.686970	10.860173
10.321806	898.071778	10.865178
10.408358	902.558885	10.870183
10.570291	925.990179	10.875187
10.785334	928.132216	10.880192
10.748348	928.694817	10.885197
10.762247	937.230790	10.890202
11.061983	923.248101	10.895207
10.960870	935.899613	10.900211
10.907381	925.709316	10.905216
10.782257	937.752761	10.910221
10.742326	934.146091	10.915226
11.040259	931.526387	10.920231
10.902597	929.277384	10.925235
11.037371	935.911069	10.930240
11.216673	931.793158	10.935245
11.417936	936.321905	10.940250
11.654573	926.708267	10.945255
11.207697	936.776516	10.950259
11.197760	928.410235	10.955264
11.327110	937.098114	10.960269
11.203819	940.199352	10.965274
11.361891	948.521511	10.970279
11.637204	969.080312	10.975283
11.335410	966.460064	10.980288
11.702059	968.226240	10.985293
11.752068	967.669446	10.990298
11.954843	962.511653	10.995303
11.931421	964.713813	11.000307
12.051224	971.838791	11.005312
12.113624	973.468982	11.010317
11.962183	969.902170	11.015322
11.857195	967.463432	11.020327
11.440401	975.102967	11.025331
11.437405	969.784016	11.030336
11.830160	968.983302	11.035341
11.743763	982.763260	11.040346
11.858777	989.747075	11.045351
12.061192	1004.860916	11.050355
11.993561	1006.234289	11.055360
12.392644	1009.413078	11.060365
12.230667	1013.178139	11.065370
12.443625	1009.852834	11.070375
12.649268	1011.447564	11.075379
12.412038	1013.335304	11.080384
12.539490	1013.803865	11.085389
12.467258	1019.682075	11.090394
12.196298	1011.029352	11.095399
12.140515	1016.644721	11.100403
12.691342	1036.498879	11.105408
12.678882	1035.653981	11.110413
12.880382	1054.622376	11.115418
12.821243	1048.061735	11.120423
12.941319	1056.008364	11.125427
13.137745	1041.977381	11.130432
13.305511	1047.945063	11.135437
13.189099	1043.085756	11.140442
13.307767	1048.234885	11.145447
12.898330	1047.186784	11.150451
13.241905	1053.096460	11.155456
13.194983	1051.451175	11.160461
12.920039	1059.927630	11.165466
13.418002	1045.217717	11.170471
13.384203	1064.376633	11.175475
12.988247	1053.999581	11.180480
13.078772	1061.100886	11.185485
13.258306	1060.334180	11.190490
13.543254	1047.806214	11.195495
13.346627	1057.217994	11.200499
13.400666	1060.418714	11.205504
13.661011	1060.509661	11.210509
13.736892	1072.538502	11.215514
13.519894	1064.728759	11.220519
13.324838	1072.992190	11.225523
13.493670	1083.509572	11.230528
13.738738	1090.718715	11.235533
13.457268	1097.985039	11.240538
14.147706	1086.329143	11.245543
14.036057	1093.979993	11.250547
13.625813	1086.754616	11.255552
14.039307	1093.996824	11.260557
13.529773	1096.651887	11.265562
14.051875	1090.992069	11.270567
14.020322	1126.473440	11.275571
14.256399	1117.716120	11.280576
14.360716	1127.348044	11.285581
14.105368	1125.859009	11.290586
14.615333	1123.795278	11.295591
14.347837	1129.613208	11.300595
14.347814	1123.487839	11.305600
14.456794	1124.822012	11.310605
14.443566	1122.676142	11.315610
14.473311	1128.164362	11.320615
14.305111	1135.190269	11.325619
14.613428	1129.178154	11.330624
14.483190	1130.470054	11.335629
14.579197	1142.830084	11.340634
14.822667	1154.930040	11.345639
14.897222	1156.638745	11.350643
14.687324	1161.494943	11.355648
15.121468	1163.346579	11.360653
14.970497	1167.693445	11.365658
15.035623	1160.262884	11.370663
15.037774	1164.405536	11.375667
15.047815	1166.458874	11.380672
15.144023	1172.349705	11.385677
14.936641	1175.858677	11.390682
15.231691	1162.825911	11.395687
14.936668	1165.962476	11.400691
14.829301	1168.357843	11.405696
15.052001	1182.336287	11.410701
15.164384	1193.310645	11.415706
15.285447	1198.531991	11.420711
15.213445	1205.293408	11.425715
15.449773	1202.323907	11.430720
15.502708	1208.431407	11.435725
15.216170	1206.109906	11.440730
15.675590	1207.891279	11.445735
15.576558	1207.519112	11.450739
15.706674	1222.452307	11.455744
15.913276	1236.163688	11.460749
15.886997	1237.762319	11.465754
16.154083	1233.811687	11.470759
16.258231	1238.770795	11.475763
16.029848	1230.942276	11.480768
16.258707	1226.961470	11.485773
15.918595	1218.267610	11.490778
15.994381	1231.674973	11.495783
16.253158	1240.314001	11.500787
16.351058	1241.176825	11.505792
16.152069	1239.364947	11.510797
16.125778	1244.679207	11.515802
16.609897	1234.935996	11.520807
16.371679	1240.774534	11.525811
16.321975	1239.643803	11.530816
16.574294	1235.873737	11.535821
16.426960	1244.571238	11.540826
16.414519	1242.464652	11.545831
16.260242	1241.954627	11.550835
16.254481	1238.358203	11.555840
16.766893	1231.367236	11.560845
16.489185	1237.855524	11.565850
16.720016	1243.217087	11.570855
16.646352	1254.962401	11.575859
16.678871	1255.015566	11.580864
16.753978	1254.656626	11.585869
16.401123	1266.500892	11.590874
17.091508	1259.881317	11.595879
17.032480	1261.778513	11.600883
17.053634	1256.857764	11.605888
17.395381	1255.689825	11.610893
17.007927	1262.003224	11.615898
17.272237	1253.630861	11.620903
16.903039	1255.713162	11.625907
16.944725	1259.138266	11.630912
17.108612	1269.757506	11.635917
17.478601	1292.381850	11.640922
17.564223	1289.654011	11.645927
17.693406	1291.206559	11.650931
17.342348	1304.024425	11.655936
17.503945	1287.289309	11.660941
17.566480	1299.814886	11.665946
17.808776	1292.741598	11.670951
17.569702	1285.077984	11.675955
17.977846	1289.349896	11.680960
18.225573	1290.076850	11.685965
17.939012	1303.808607	11.690970
18.218714	1298.011530	11.695975
17.889306	1298.984310	11.700979
17.914822	1297.319557	11.705984
17.977267	1297.651827	11.710989
17.844364	1301.743515	11.715994
18.078721	1296.834480	11.720999
17.916175	1305.151209	11.726003
18.075144	1297.331049	11.731008
18.196731	1300.529722	11.736013
17.884332	1307.789255	11.741018
18.279579	1295.845935	11.746023
18.193668	1303.950148	11.751027
18.518633	1307.253589	11.756032
18.329116	1310.812577	11.761037
18.185422	1328.788409	11.766042
18.719055	1320.480291	11.771047
18.870738	1328.633360	11.776051
18.955519	1324.716514	11.781056
19.264839	1317.201975	11.786061
18.700067	1308.578591	11.791066
18.902301	1300.556756	11.796071
18.482487	1299.176734	11.801075
18.759838	1300.641776	11.806080
18.853022	1304.952892	11.811085
18.591216	1323.098958	11.816090
18.876760	1325.714768	11.821095
18.892357	1330.445947	11.826099
18.584979	1331.330052	11.831104
18.960787	1327.880130	11.836109
18.716044	1328.803134	11.841114
18.980083	1330.711892	11.846119
19.168030	1341.871446	11.851123
19.426025	1350.471237	11.856128
19.642532	1356.584251	11.861133
19.087262	1352.055852	11.866138
19.650458	1345.816107	11.871143
19.563050	1362.353359	11.876147
19.421763	1366.816233	11.881152
19.844044	1363.238242	11.886157
19.769479	1352.917742	11.891162
19.390699	1343.614115	11.896167
19.553690	1356.829472	11.901171
19.717527	1356.432719	11.906176
20.012579	1358.208788	11.911181
19.862690	1358.441663	11.916186
19.722836	1364.431733	11.921191
19.792516	1364.899270	11.926195
19.776253	1363.652010	11.931200
20.259910	1354.627954	11.936205
20.084618	1366.222394	11.941210
19.892145	1360.693803	11.946215
19.991810	1367.517019	11.951219
20.083451	1359.372430	11.956224
20.350987	1358.451309	11.961229
20.343079	1374.136875	11.966234
20.670989	1359.422231	11.971239
20.422692	1357.095393	11.976243
20.535774	1363.319533	11.981248
20.597903	1365.365378	11.986253
20.597121	1375.185347	11.991258
20.923381	1371.602168	11.996263
20.417482	1379.807322	12.001267
20.102122	1376.749938	12.006272
20.747254	1373.372964	12.011277
20.607762	1382.512463	12.016282
20.948533	1374.205902	12.021287
20.931802	1369.966947	12.026291
20.495547	1382.390001	12.031296
20.941636	1376.038023	12.036301
20.858727	1384.523461	12.041306
20.968478	1382.231768	12.046311
20.703340	1383.225055	12.051315
20.752000	1381.018020	12.056320
20.480926	1386.074091	12.061325
20.571125	1388.746305	12.066330
20.539439	1376.341111	12.071335
20.537182	1383.463682	12.076339
20.534879	1382.024940	12.081344
20.721323	1376.970542	12.086349
20.709071	1385.674180	12.091354
20.652862	1377.133654	12.096359
20.775543	1376.211981	12.101363
20.761691	1379.943258	12.106368
21.022127	1379.917488	12.111373
20.831150	1384.449800	12.116378
20.835261	1376.992588	12.121383
20.547012	1353.817281	12.126387
20.265421	1364.944505	12.131392
20.597555	1375.888680	12.136397
20.480096	1387.402155	12.141402
20.579528	1378.551346	12.146407
20.933052	1385.446052	12.151411
20.686649	1387.646780	12.156416
21.256960	1385.432237	12.161421
20.680492	1371.090517	12.166426
20.751940	1357.782555	12.171431
20.572037	1354.168931	12.176435
20.369407	1352.932473	12.181440
20.830114	1361.421082	12.186445
20.794497	1366.068970	12.191450
20.872340	1356.637300	12.196455
20.621101	1352.600564	12.201459
20.451420	1351.994423	12.206464
20.761084	1345.196607	12.211469
20.657251	1353.328152	12.216474
20.744490	1349.386462	12.221479
20.680095	1348.317207	12.226483
20.656666	1355.459701	12.231488
20.967243	1349.745997	12.236493
20.808220	1355.185557	12.241498
20.613361	1348.338105	12.246503
20.532513	1356.168701	12.251507
20.758554	1355.236063	12.256512
20.984532	1345.768155	12.261517
20.895060	1359.265869	12.266522
20.826832	1350.440243	12.271527
20.667261	1355.476941	12.276531
20.533990	1352.724075	12.281536
21.092860	1354.281427	12.286541
20.554815	1353.238832	12.291546
20.997299	1354.814749	12.296551
20.977772	1359.744735	12.301555
20.832054	1362.286614	12.306560
21.098879	1356.281024	12.311565
20.747641	1352.095431	12.316570
20.723311	1331.010307	12.321575
20.952051	1328.454403	12.326579
20.342084	1326.646561	12.331584
20.525635	1324.742112	12.336589
20.760073	1325.882812	12.341594
21.014184	1324.343246	12.346599
21.101719	1324.886789	12.351603
20.756057	1324.581557	12.356608
21.004542	1321.702354	12.361613
20.896227	1331.691636	12.366618
20.605052	1321.580768	12.371623
20.741667	1325.441797	12.376627
20.804054	1322.164884	12.381632
20.876645	1330.553729	12.386637
20.603139	1330.662806	12.391642
20.840042	1321.903655	12.396647
20.848840	1325.840270	12.401651
20.512426	1331.252918	12.406656
20.720872	1323.688228	12.411661
20.629347	1332.898111	12.416666
20.997868	1333.101128	12.421671
20.707865	1332.311523	12.426675
20.858051	1320.541325	12.431680
20.806395	1308.800967	12.436685
20.571058	1304.100115	12.441690
20.592012	1294.550603	12.446695
20.097007	1310.910728	12.451699
20.376042	1322.159827	12.456704
20.602334	1319.613778	12.461709
20.469925	1337.749474	12.466714
20.637548	1331.619356	12.471719
20.624687	1333.847486	12.476723
20.583771	1334.193878	12.481728
20.753559	1329.715429	12.486733
20.368192	1331.618952	12.491738
20.864351	1335.715186	12.496743
20.867566	1335.780124	12.501747
20.783839	1338.107875	12.506752
20.851140	1337.249449	12.511757
20.665594	1339.718033	12.516762
20.765216	1339.210876	12.521767
21.084898	1345.594460	12.526771
21.043698	1334.041666	12.531776
20.877771	1314.183268	12.536781
20.518023	1310.562069	12.541786
20.728134	1306.639431	12.546791
20.663034	1302.938904	12.551795
20.804307	1305.905759	12.556800
20.432869	1303.967612	12.561805
20.516095	1307.341156	12.566810
20.686450	1305.701400	12.571815
20.811364	1305.096373	12.576819
20.875031	1308.510098	12.581824
20.741038	1301.918700	12.586829
20.638644	1300.471486	12.591834
20.440125	1301.635508	12.596839
20.653761	1307.168587	12.601843
20.550864	1310.182276	12.606848
20.789799	1304.508404	12.611853
20.488001	1308.027736	12.616858
20.751522	1300.861952	12.621863
20.584267	1307.677249	12.626867
20.566894	1310.577150	12.631872
20.948051	1303.962722	12.636877
20.803573	1309.560021	12.641882
20.797293	1301.816683	12.646887
21.044704	1305.496016	12.651891
20.489119	1313.768200	12.656896
20.984989	1301.039202	12.661901
20.610710	1308.336993	12.666906
20.691707	1307.688503	12.671911
20.749569	1303.869005	12.676915
20.942842	1303.264902	12.681920
20.788228	1304.489736	12.686925
20.518540	1314.843035	12.691930
20.811103	1306.829656	12.696935
21.051366	1307.777808	12.701939
21.078412	1314.891729	12.706944
20.879359	1315.631597	12.711949
20.472159	1316.090035	12.716954
20.591545	1318.927908	12.721959
20.475036	1316.671527	12.726963
20.412106	1319.547943	12.731968
20.766258	1320.559150	12.736973
20.865300	1318.463947	12.741978
20.672616	1313.253193	12.746983
20.790569	1317.029668	12.751987
20.608378	1315.649591	12.756992
20.713366	1315.641519	12.761997
20.811279	1316.490152	12.767002
20.502176	1315.047521	12.772007
20.725481	1310.862556	12.777011
20.507204	1319.768555	12.782016
20.686434	1314.547368	12.787021
20.696915	1324.565009	12.792026
20.610522	1316.134999	12.797031
21.014203	1317.318095	12.802035
20.746276	1322.536872	12.807040
20.810832	1311.042140	12.812045
20.515809	1303.062558	12.817050
20.483730	1296.185223	12.822055
20.866751	1310.174491	12.827059
20.818383	1314.415140	12.832064
20.862478	1299.395710	12.837069
20.351282	1302.062901	12.842074
20.676439	1298.918349	12.847079
20.661959	1293.734376	12.852083
20.361138	1299.473314	12.857088
20.946929	1302.162665	12.862093
20.517660	1310.166305	12.867098
20.934030	1308.152964	12.872103
20.996969	1310.204192	12.877107
20.586876	1306.415966	12.882112
20.679175	1294.807213	12.887117
20.532911	1298.177932	12.892122
20.578600	1295.540047	12.897127
20.857306	1302.357542	12.902131
20.295492	1307.737531	12.907136
20.440795	1295.966555	12.912141
20.562824	1320.694127	12.917146
20.898793	1320.896817	12.922151
20.962122	1311.259314	12.927155
20.549966	1314.296311	12.932160
20.739840	1295.411820	12.937165
20.912929	1301.962284	12.942170
20.560436	1300.911387	12.947175
20.521322	1292.363453	12.952179
20.784210	1302.185474	12.957184
21.016829	1293.752694	12.962189
20.642462	1297.483890	12.967194
20.839773	1293.226587	12.972199
20.758411	1301.834744	12.977203
20.601522	1311.439063	12.982208
20.969364	1307.738870	12.987213
20.485986	1304.014378	12.992218
20.606762	1299.814228	12.997223
20.875961	1302.539884	13.002227
20.490115	1307.636315	13.007232
20.807394	1302.863876	13.012237
20.743428	1306.075588	13.017242
20.746883	1311.942632	13.022247
20.566288	1303.213024	13.027251
20.307172	1303.714868	13.032256
20.863866	1302.402244	13.037261
20.769844	1311.696886	13.042266
20.254976	1312.530500	13.047271
20.801216	1318.424519	13.052275
20.754082	1312.163069	13.057280
20.908610	1311.077822	13.062285
20.585348	1311.359642	13.067290
20.827268	1311.029291	13.072295
20.564632	1304.533324	13.077299
20.637622	1311.083987	13.082304
20.592511	1306.689502	13.087309
20.597355	1310.451686	13.092314
20.879243	1306.282611	13.097319
20.868807	1307.302293	13.102323
20.514628	1312.506437	13.107328
20.950879	1312.428967	13.112333
20.618403	1315.573902	13.117338
20.624256	1307.942966	13.122343
20.926611	1313.453222	13.127347
20.864585	1313.725703	13.132352
21.092490	1314.902928	13.137357
20.712845	1320.465196	13.142362
20.454347	1321.264225	13.147367
20.655463	1314.939520	13.152371
20.334433	1319.239432	13.157376
20.795839	1310.640038	13.162381
20.805905	1321.286217	13.167386
21.001989	1313.956125	13.172391
21.338476	1312.142411	13.177395
20.600004	1296.654032	13.182400
20.553370	1285.936427	13.187405
20.529572	1288.706450	13.192410
20.414061	1287.404846	13.197415
20.830874	1294.583542	13.202419
20.344051	1299.778875	13.207424
20.756258	1302.838932	13.212429
20.642812	1316.903455	13.217434
20.845999	1316.072245	13.222439
20.741743	1300.183051	13.227443
20.661796	1301.716126	13.232448
20.421001	1291.721044	13.237453
20.908552	1308.858082	13.242458
20.473470	1299.775583	13.247463
20.678629	1307.054284	13.252467
20.937131	1312.425653	13.257472
20.946663	1293.055797	13.262477
20.542497	1293.848884	13.267482
20.486903	1289.308617	13.272487
20.392163	1284.895244	13.277491
20.629199	1304.295153	13.282496
20.506577	1311.301258	13.287501
20.975315	1315.020990	13.292506
20.699153	1312.988001	13.297511
20.513095	1300.205335	13.302515
20.478889	1313.812474	13.307520
20.985058	1307.674101	13.312525
20.541050	1310.881773	13.317530
20.976318	1307.362443	13.322535
20.871407	1298.630228	13.327539
20.438776	1296.931310	13.332544
20.842584	1289.290529	13.337549
20.693685	1288.021061	13.342554
20.730637	1285.058112	13.347559
20.598444	1283.138582	13.352563
20.529703	1289.886901	13.357568
20.528922	1281.209845	13.362573
20.594422	1288.011663	13.367578
20.431861	1298.813106	13.372583
20.914777	1316.808045	13.377587
20.735931	1309.126926	13.382592
20.827627	1289.801532	13.387597
20.602476	1298.025732	13.392602
20.342464	1296.186518	13.397607
20.230516	1305.515559	13.402611
20.317944	1318.549739	13.407616
20.614796	1321.299375	13.412621
20.440803	1333.391946	13.417626
20.264799	1333.735441	13.422631
21.007684	1328.981058	13.427635
20.855407	1335.295614	13.432640
20.812894	1335.595736	13.437645
20.551317	1332.428060	13.442650
20.980950	1336.212388	13.447655
21.197114	1329.284401	13.452659
20.700589	1339.313531	13.457664
20.951154	1333.282157	13.462669
20.647674	1318.388330	13.467674
20.555164	1304.431571	13.472679
20.844073	1304.420184	13.477683
20.315129	1301.920481	13.482688
20.744657	1312.027405	13.487693
20.753830	1321.561083	13.492698
20.618532	1308.316109	13.497703
20.653746	1300.587444	13.502707
20.754581	1316.737407	13.507712
20.800593	1302.513315	13.512717
20.775701	1303.241173	13.517722
20.612363	1306.588596	13.522727
20.814657	1303.411595	13.527731
20.676063	1301.325123	13.532736
20.734609	1300.170024	13.537741
20.442907	1309.353469	13.542746
20.795890	1307.204357	13.547751
20.777965	1303.541252	13.552755
20.464516	1303.752903	13.557760
20.907474	1294.744838	13.562765
20.779442	1301.317311	13.567770
20.893641	1305.848234	13.572775
20.906343	1300.171022	13.577779
20.731956	1309.160697	13.582784
20.967346	1292.830158	13.587789
20.558925	1308.703340	13.592794
20.643252	1300.543391	13.597799
20.623379	1304.763721	13.602803
20.322396	1305.816342	13.607808
20.586025	1299.718236	13.612813
20.544411	1302.356262	13.617818
20.463148	1308.348002	13.622823
20.684325	1303.687883	13.627827
20.403475	1307.526391	13.632832
20.647485	1307.727189	13.637837
21.059856	1309.307115	13.642842
20.685421	1309.442541	13.647847
20.758807	1300.598299	13.652851
20.291316	1315.960470	13.657856
20.753711	1305.861888	13.662861
20.749729	1306.968070	13.667866
20.346680	1312.235207	13.672871
20.904282	1302.149041	13.677875
20.495183	1314.117444	13.682880
20.690929	1302.366805	13.687885
20.624256	1305.981109	13.692890
20.450884	1319.598623	13.697895
20.671151	1317.549533	13.702899
20.551332	1310.444890	13.707904
20.688542	1303.538972	13.712909
20.950233	1315.175644	13.717914
20.855800	1331.258200	13.722919
20.842936	1322.393006	13.727923
20.544953	1323.831539	13.732928
20.753530	1314.834037	13.737933
20.682622	1308.836602	13.742938
20.453753	1322.693228	13.747943
20.955289	1308.778917	13.752947
20.544799	1319.154677	13.757952
20.667352	1313.493846	13.762957
20.469604	1313.491481	13.767962
20.660299	1310.626230	13.772967
20.536433	1310.885707	13.777971
20.321513	1328.270448	13.782976
20.803232	1316.019978	13.787981
20.843938	1323.399042	13.792986
20.617872	1321.910835	13.797991
20.832332	1315.098254	13.802995
20.919596	1324.683352	13.808000
20.918348	1319.181050	13.813005
20.928816	1321.819446	13.818010
20.746700	1317.860011	13.823015
20.851427	1313.314666	13.828019
20.716481	1315.566210	13.833024
20.742382	1314.550370	13.838029
20.811979	1317.612246	13.843034
20.514646	1329.163040	13.848039
21.113563	1325.528496	13.853043
20.833398	1325.861794	13.858048
20.958823	1319.549948	13.863053
20.760243	1326.971914	13.868058
20.322951	1308.908967	13.873063
20.795666	1309.066976	13.878067
20.548510	1314.874638	13.883072
20.886409	1313.385581	13.888077
20.898260	1312.696076	13.893082
20.518220	1300.363071	13.898087
20.677401	1289.760882	13.903091
20.706843	1296.944592	13.908096
20.590624	1288.083288	13.913101
20.721708	1287.992988	13.918106
20.503192	1288.630294	13.923111
20.812450	1287.380795	13.928115
20.771942	1300.671931	13.933120
20.644276	1291.893671	13.938125
20.524958	1286.495379	13.943130
20.622447	1290.450957	13.948135
20.895382	1289.983972	13.953139
20.539496	1300.239035	13.958144
20.497325	1281.526417	13.963149
20.598662	1295.682039	13.968154
20.639967	1314.482343	13.973159
20.537975	1314.892099	13.978163
20.476772	1323.781720	13.983168
20.827978	1313.227738	13.988173
20.869408	1319.509813	13.993178
20.680244	1321.295298	13.998183
21.199183	1306.906660	14.003187
20.604678	1317.427688	14.008192
20.684221	1314.625875	14.013210
20.752961	1310.098611	14.018227
20.846662	1310.798628	14.023245
20.856641	1315.362102	14.028263
20.669122	1320.302370	14.033280
20.916021	1316.412885	14.038298
20.739533	1316.938129	14.043315
20.618979	1318.806509	14.048333
20.948065	1298.621803	14.053351
20.766403	1310.675363	14.058368
20.865603	1305.503787	14.063386
20.757260	1299.940587	14.068403
20.746134	1300.813059	14.073421
21.092422	1300.071177	14.078439
20.604483	1314.974452	14.083456
20.659571	1307.764913	14.088474
21.004599	1315.079737	14.093491
20.898086	1332.571250	14.098509
20.745503	1325.164371	14.103527
21.108200	1340.145141	14.108544
21.018572	1343.122331	14.113562
21.094323	1342.732710	14.118579
20.639059	1341.334500	14.123597
21.009727	1340.548614	14.128615
20.730392	1346.855597	14.133632
20.987940	1332.981652	14.138650
21.139204	1337.476977	14.143667
20.893092	1348.792063	14.148685
21.051467	1333.903569	14.153703
20.782710	1341.402042	14.158720
21.014019	1336.536583	14.163738
21.203911	1337.849703	14.168755
21.192889	1345.944951	14.173773
21.175553	1337.778720	14.178791
21.226287	1353.154554	14.183808
21.659543	1359.622381	14.188826
21.098705	1345.998517	14.193843
21.057674	1361.435403	14.198861
21.329698	1361.295269	14.203879
21.157555	1376.144301	14.208896
21.238612	1372.633624	14.213914
21.251918	1370.925495	14.218931
21.675372	1378.717070	14.223949
21.543306	1370.969470	14.228967
21.317523	1373.618373	14.233984
21.660396	1378.052473	14.239002
21.779010	1379.133925	14.244019
21.543822	1384.964318	14.249037
21.733211	1378.430985	14.254055
21.811096	1377.267852	14.259072
21.319317	1372.157483	14.264090
21.833174	1379.492603	14.269107
21.487340	1364.793831	14.274125
21.640114	1354.702534	14.279143
21.422859	1356.731068	14.284160
21.283368	1365.152782	14.289178
21.665673	1361.496526	14.294195
21.403335	1374.027064	14.299213
21.695030	1364.991949	14.304231
21.601634	1368.757073	14.309248
21.688020	1373.162081	14.314266
21.544787	1374.954645	14.319283
21.553624	1373.868596	14.324301
21.246976	1380.971997	14.329319
21.243852	1395.548689	14.334336
21.527284	1406.411251	14.339354
21.819243	1399.436815	14.344371
21.951320	1408.406717	14.349389
22.092450	1406.118963	14.354407
21.967487	1414.666595	14.359424
21.653325	1404.865256	14.364442
22.018475	1402.605480	14.369459
21.602177	1411.037552	14.374477
22.010838	1394.507672	14.379495
21.987912	1400.960976	14.384512
21.771573	1401.598762	14.389530
21.770324	1396.115975	14.394547
21.675054	1400.261306	14.399565
21.766000	1403.907369	14.404583
22.059306	1397.351946	14.409600
21.612369	1401.779894	14.414618
22.047410	1420.303594	14.419635
22.116060	1431.903604	14.424653
22.409462	1423.974062	14.429671
22.408592	1428.986058	14.434688
22.166322	1435.705609	14.439706
22.441280	1429.893236	14.444723
22.378706	1433.694361	14.449741
22.681152	1424.361753	14.454759
22.510913	1408.036673	14.459776
22.142951	1401.033785	14.464794
22.280235	1387.357516	14.469811
22.107720	1389.238913	14.474829
22.601259	1400.306280	14.479847
22.497694	1391.189471	14.484864
22.473672	1390.694636	14.489882
22.575590	1380.176475	14.494899
22.339420	1386.262651	14.499917
22.605820	1381.118650	14.504935
22.453742	1379.091608	14.509952
22.258730	1386.773404	14.514970
22.328361	1391.966846	14.519987
22.457243	1407.008576	14.525005
22.820173	1405.656037	14.530023
23.052298	1414.317391	14.535040
22.935500	1399.423956	14.540058
22.952816	1386.720899	14.545075
22.678312	1386.932219	14.550093
22.758581	1378.468813	14.555111
22.511651	1386.098326	14.560128
22.549199	1372.258649	14.565146
22.745524	1373.666704	14.570163
22.220060	1383.921285	14.575181
22.352192	1392.809369	14.580199
22.632878	1412.756152	14.585216
22.931056	1418.499909	14.590234
23.221460	1407.736151	14.595251
22.808619	1415.843619	14.600269
22.714155	1410.157822	14.605287
22.907769	1413.214908	14.610304
22.777883	1409.541233	14.615322
22.866284	1412.124298	14.620339
22.328586	1418.776915	14.625357
22.743405	1419.977871	14.630375
23.017075	1421.037740	14.635392
22.580084	1421.462174	14.640410
23.095657	1411.445108	14.645427
22.825776	1410.800718	14.650445
22.956479	1416.935358	14.655463
23.111955	1415.052743	14.660480
23.086693	1420.124472	14.665498
23.079245	1412.965757	14.670515
22.503345	1425.842095	14.675533
23.068885	1432.361218	14.680551
23.420919	1438.910466	14.685568
23.351816	1440.303448	14.690586
23.366909	1442.038518	14.695603
23.591428	1430.249373	14.700621
23.247360	1419.017351	14.705639
23.179473	1412.418857	14.710656
23.087728	1416.141256	14.715674
23.165098	1434.207625	14.720691
23.305815	1453.457101	14.725709
23.336088	1448.181634	14.730727
23.426960	1445.790200	14.735744
23.231304	1447.065723	14.740762
23.391715	1443.855417	14.745779
23.258887	1440.949085	14.750797
23.361378	1441.862433	14.755815
23.637446	1441.752329	14.760832
23.344128	1449.559168	14.765850
23.454625	1438.342718	14.770867
23.253942	1446.003426	14.775885
23.198547	1445.077061	14.780903
23.431453	1442.717244	14.785920
23.162734	1446.460801	14.790938
23.424362	1448.550607	14.795955
23.366120	1460.546063	14.800973
23.747576	1474.173480	14.805991
24.014486	1479.331552	14.811008
23.994540	1476.349003	14.816026
23.951317	1464.357922	14.821043
23.846938	1450.323721	14.826061
23.822573	1446.658376	14.831079
24.084641	1439.473175	14.836096
23.684047	1437.631275	14.841114
24.094419	1440.655366	14.846131
23.704694	1442.023981	14.851149
23.460807	1442.580429	14.856167
23.864944	1443.982087	14.861184
23.639487	1449.821964	14.866202
23.825832	1460.204530	14.871219
23.878425	1477.686569	14.876237
23.990392	1480.232065	14.881255
24.209818	1477.389881	14.886272
24.196782	1486.076224	14.891290
24.410476	1468.552489	14.896307
24.115397	1456.886315	14.901325
24.056389	1442.983317	14.906343
24.156907	1443.198529	14.911360
24.151818	1441.074097	14.916378
24.263883	1437.320922	14.921395
24.046156	1436.366965	14.926413
24.031380	1431.701182	14.931431
24.317961	1437.802315	14.936448
23.993531	1452.160529	14.941466
24.260829	1457.959567	14.946483
24.531962	1466.559672	14.951501
24.630109	1466.676944	14.956519
24.248925	1455.101588	14.961536
24.132697	1452.870607	14.966554
24.553147	1440.628614	14.971571
24.272708	1447.367629	14.976589
24.198734	1452.451072	14.981607
24.292123	1459.777005	14.986624
24.350572	1475.765244	14.991642
24.312560	1473.097836	14.996659
24.425897	1468.649144	15.001677
24.348625	1473.809415	15.006695
24.809048	1464.958906	15.011712
24.605056	1475.170926	15.016730
25.137105	1463.571025	15.021747
25.103599	1473.754277	15.026765
24.595301	1455.526138	15.031783
24.776834	1447.373743	15.036800
24.557334	1441.725182	15.041818
24.731469	1439.863185	15.046835
24.518212	1445.663361	15.051853
24.642712	1457.508538	15.056871
25.061385	1462.720266	15.061888
24.900344	1457.052149	15.066906
24.576812	1451.597150	15.071923
25.000722	1450.103528	15.076941
24.489328	1458.706532	15.081959
24.985446	1458.499978	15.086976
24.677150	1476.697132	15.091994
24.818609	1468.997090	15.097011
24.984606	1473.314708	15.102029
25.136358	1475.847565	15.107047
25.227404	1465.815590	15.112064
25.303025	1471.776560	15.117082
24.817931	1456.516290	15.122099
24.941530	1458.658003	15.127117
24.720728	1469.741834	15.132135
24.950510	1474.578624	15.137152
24.720212	1485.290371	15.142170
24.769035	1478.967399	15.147187
25.296832	1477.500463	15.152205
25.022920	1479.268265	15.157223
25.335674	1477.694838	15.162240
24.975806	1485.475343	15.167258
24.900887	1480.921389	15.172275
25.091754	1474.615089	15.177293
24.886674	1485.245732	15.182311
25.038775	1476.180903	15.187328
24.945154	1483.973211	15.192346
25.210098	1495.802310	15.197363
25.297751	1504.440355	15.202381
25.247520	1509.217210	15.207399
25.297401	1508.669682	15.212416
25.245027	1511.772318	15.217434
25.192918	1510.785646	15.222451
25.381273	1507.057253	15.227469
25.106237	1510.526541	15.232487
25.310820	1510.498628	15.237504
25.359738	1511.411088	15.242522
25.447608	1511.110769	15.247539
25.399012	1517.099436	15.252557
25.695291	1528.190500	15.257575
26.118610	1528.827727	15.262592
25.333565	1522.799772	15.267610
25.801874	1516.765393	15.272627
25.863539	1518.043925	15.277645
25.420663	1519.989699	15.282663
26.149325	1526.589817	15.287680
25.832785	1528.985797	15.292698
25.775730	1518.272660	15.297715
26.057637	1515.472415	15.302733
25.683414	1516.711929	15.307751
25.801672	1514.647253	15.312768
25.782381	1519.282317	15.317786
26.096198	1519.789925	15.322803
25.995364	1510.222700	15.327821
25.813337	1512.979485	15.332839
26.226399	1507.019992	15.337856
25.907462	1504.438288	15.342874
25.698254	1502.871820	15.347891
26.209906	1520.953187	15.352909
26.022876	1541.130486	15.357927
26.169710	1537.588041	15.362944
26.374205	1531.545397	15.367962
25.824850	1516.480940	15.372979
25.873225	1525.594833	15.377997
25.686692	1541.329623	15.383015
26.194007	1537.694285	15.388032
26.071632	1546.004830	15.393050
26.262824	1540.439380	15.398067
26.269200	1530.782679	15.403085
26.290766	1538.699008	15.408103
26.062679	1539.908923	15.413120
26.566481	1539.137186	15.418138
26.005138	1543.465443	15.423155
26.298943	1539.857867	15.428173
26.500715	1542.860981	15.433191
26.609073	1536.118695	15.438208
26.135823	1542.264774	15.443226
26.188874	1549.214923	15.448243
26.246633	1541.651682	15.453261
26.497221	1546.946882	15.458279
26.610855	1549.430775	15.463296
26.591139	1555.938694	15.468314
26.631957	1553.134423	15.473331
26.997164	1545.890245	15.478349
26.459256	1544.224397	15.483367
26.445117	1539.823545	15.488384
26.612141	1551.198738	15.493402
26.641449	1564.603971	15.498419
26.940894	1562.292514	15.503437
27.023465	1567.562609	15.508455
26.772143	1556.006573	15.513472
26.558877	1544.597066	15.518490
26.670404	1557.652535	15.523507
27.062214	1564.218307	15.528525
27.157273	1577.626436	15.533543
26.903235	1571.415442	15.538560
26.891515	1569.497339	15.543578
26.986057	1572.620601	15.548595
27.358876	1571.062754	15.553613
26.896233	1567.281659	15.558631
27.040768	1557.385028	15.563648
27.052703	1550.375744	15.568666
27.031931	1558.483677	15.573683
27.413031	1560.368031	15.578701
27.052985	1556.111229	15.583719
26.792557	1546.052672	15.588736
26.950869	1557.097335	15.593754
27.053021	1570.829172	15.598771
27.316278	1569.231382	15.603789
27.336195	1579.647658	15.608807
26.993128	1565.653779	15.613824
27.089964	1562.840570	15.618842
27.035163	1564.700067	15.623859
27.249094	1560.353284	15.628877
26.966034	1564.904586	15.633895
27.171712	1558.302504	15.638912
27.295317	1560.437939	15.643930
27.190929	1562.402877	15.648947
27.301302	1567.368075	15.653965
27.347341	1583.713147	15.658983
27.597722	1586.865040	15.664000
27.622889	1590.557037	15.669018
27.197096	1594.899082	15.674035
27.736880	1586.354396	15.679053
27.537287	1596.045101	15.684071
27.286167	1594.021241	15.689088
27.633791	1594.969435	15.694106
27.310362	1589.349192	15.699123
27.665363	1591.420980	15.704141
27.509565	1591.331781	15.709159
27.427369	1600.260470	15.714176
27.882161	1593.808984	15.719194
27.436980	1591.857765	15.724211
27.916810	1579.448088	15.729229
27.678784	1595.711061	15.734247
27.534051	1587.466691	15.739264
27.702226	1598.329691	15.744282
27.870618	1616.244907	15.749299
28.148965	1618.844905	15.754317
28.192605	1616.686719	15.759335
28.173459	1616.180873	15.764352
28.236026	1616.093811	15.769370
27.752464	1620.634637	15.774387
28.312445	1614.702007	15.779405
28.439804	1614.840577	15.784423
27.980810	1603.066717	15.789440
28.283864	1590.372179	15.794458
27.977794	1602.725835	15.799475
28.286777	1603.186238	15.804493
28.055031	1614.853973	15.809511
28.176219	1616.963059	15.814528
28.573962	1613.315290	15.819546
28.176251	1625.533351	15.824563
28.536696	1615.669099	15.829581
28.642261	1615.621586	15.834599
28.389422	1598.979112	15.839616
28.286328	1586.682072	15.844634
28.105323	1597.727402	15.849651
28.498088	1604.080670	15.854669
28.514901	1613.050207	15.859687
28.462318	1621.388990	15.864704
28.581099	1622.225029	15.869722
28.484088	1627.771555	15.874739
28.693392	1613.218377	15.879757
28.541732	1610.547835	15.884775
28.755513	1623.650764	15.889792
28.925668	1611.837109	15.894810
28.555857	1617.449168	15.899827
29.156262	1620.379275	15.904845
28.962385	1618.945636	15.909863
28.686854	1603.476383	15.914880
28.885497	1597.696567	15.919898
28.791790	1593.316256	15.924915
28.729640	1592.779516	15.929933
28.777266	1599.340424	15.934951
28.576485	1608.368262	15.939968
28.792328	1607.277493	15.944986
28.781291	1611.705979	15.950003
29.135374	1601.644539	15.955021
28.867345	1612.935795	15.960039
28.988631	1617.357334	15.965056
29.206247	1616.041327	15.970074
28.754711	1622.480507	15.975091
29.113153	1608.274799	15.980109
29.056989	1610.969053	15.985127
29.036531	1613.681995	15.990144
28.995292	1610.980468	15.995162
29.139099	1613.259774	16.000179
29.190135	1607.275398	16.005197
29.075242	1612.853873	16.010215
29.303897	1610.802251	16.015232
29.555310	1601.326653	16.020250
29.187186	1609.300459	16.025267
29.159361	1614.564584	16.030285
29.266169	1610.174308	16.035303
29.305806	1604.241305	16.040320
29.648559	1601.509207	16.045338
29.181980	1611.060813	16.050355
29.591973	1613.456545	16.055373
29.416680	1606.003592	16.060391
29.208955	1620.631235	16.065408
29.995613	1630.408483	16.070426
29.827656	1636.439048	16.075443
29.695344	1626.592034	16.080461
29.564210	1613.729191	16.085479
29.759907	1618.565174	16.090496
29.837260	1618.215404	16.095514
29.522363	1620.568663	16.100531
29.867009	1616.198655	16.105549
29.720042	1612.566194	16.110567
29.350982	1631.796539	16.115584
29.867220	1623.272105	16.120602
29.941429	1641.216533	16.125619
29.852432	1640.767448	16.130637
30.079961	1640.423614	16.135655
29.962252	1641.659190	16.140672
30.226011	1641.769712	16.145690
29.935167	1643.345954	16.150707
30.059560	1640.601485	16.155725
30.233219	1645.620327	16.160743
30.221656	1656.994985	16.165760
30.449766	1649.621605	16.170778
30.065817	1631.139016	16.175795
30.152197	1620.803282	16.180813
30.464403	1620.077834	16.185831
30.259761	1625.111389	16.190848
30.064055	1610.456852	16.195866
29.999940	1627.657223	16.200883
30.112580	1636.572162	16.205901
30.499904	1633.959584	16.210919
30.111819	1648.803223	16.215936
30.366047	1642.445058	16.220954
30.183691	1644.463344	16.225971
30.075934	1646.608952	16.230989
30.554366	1637.561188	16.236007
30.474284	1649.435220	16.241024
30.679825	1639.358121	16.246042
30.615331	1641.142091	16.251059
30.260985	1641.764144	16.256077
30.550689	1641.925586	16.261095
30.484486	1648.758730	16.266112
30.510671	1637.378601	16.271130
30.208912	1644.422357	16.276147
30.237517	1640.444903	16.281165
30.550169	1645.194596	16.286183
30.887856	1661.213223	16.291200
30.851738	1664.283409	16.296218
30.816393	1672.331592	16.301235
30.910621	1675.933153	16.306253
30.850917	1674.149325	16.311271
30.816040	1681.488751	16.316288
31.050624	1679.068065	16.321306
30.942624	1675.430946	16.326323
30.889713	1675.654116	16.331341
31.096007	1669.357070	16.336359
30.962287	1670.250691	16.341376
31.034985	1667.115679	16.346394
31.100712	1681.921575	16.351411
31.011324	1685.755358	16.356429
31.391558	1681.589664	16.361447
31.285391	1682.554401	16.366464
31.483360	1683.952787	16.371482
31.166984	1689.771080	16.376499
31.331544	1690.127886	16.381517
31.578657	1683.485317	16.386535
31.585021	1694.757253	16.391552
31.636209	1692.232889	16.396570
31.482737	1678.773407	16.401587
31.523134	1664.309257	16.406605
31.551115	1641.598492	16.411623
31.094992	1642.676464	16.416640
31.426737	1635.720740	16.421658
31.435008	1647.793048	16.426675
31.426675	1662.883673	16.431693
31.820787	1662.291459	16.436711
31.878931	1676.289192	16.441728
31.773287	1651.860647	16.446746
31.367891	1651.108864	16.451763
31.420647	1663.428934	16.456781
31.627946	1659.301056	16.461799
31.420660	1674.487924	16.466816
31.767574	1661.769811	16.471834
31.942002	1668.086356	16.476851
31.663057	1665.159237	16.481869
31.798678	1663.854732	16.486887
31.326004	1669.100164	16.491904
31.612821	1666.258206	16.496922
31.636228	1666.466843	16.501939
31.397151	1674.473587	16.506957
31.646306	1683.185872	16.511975
31.749034	1692.359630	16.516992
32.306703	1688.725664	16.522010
32.617755	1677.456590	16.527027
32.403502	1687.208685	16.532045
32.387723	1680.369723	16.537063
32.167599	1692.867844	16.542080
32.327070	1672.647539	16.547098
32.174479	1662.772273	16.552115
32.155680	1674.041127	16.557133
32.308787	1680.682781	16.562151
32.335743	1684.124391	16.567168
32.604760	1681.196389	16.572186
32.680686	1680.550313	16.577203
32.276181	1666.143754	16.582221
32.322680	1652.275640	16.587239
32.313982	1675.297969	16.592256
32.421428	1682.245799	16.597274
32.661540	1693.591354	16.602291
32.566857	1711.595844	16.607309
33.008040	1704.880623	16.612327
32.905923	1700.937374	16.617344
32.542488	1679.652875	16.622362
32.842896	1673.442282	16.627379
32.780337	1684.593062	16.632397
32.728857	1665.427366	16.637415
32.744575	1662.527184	16.642432
32.512019	1666.799886	16.647450
32.801481	1675.944637	16.652467
32.620670	1695.295272	16.657485
33.453223	1698.296127	16.662503
33.220235	1700.761396	16.667520
32.891397	1688.555334	16.672538
32.999016	1657.111276	16.677555
32.498008	1668.379171	16.682573
32.794373	1675.674411	16.687591
32.647151	1677.344159	16.692608
32.773118	1679.598792	16.697626
32.896445	1682.163749	16.702643
32.813251	1685.219425	16.707661
32.891400	1677.516000	16.712679
33.074272	1688.261886	16.717696
33.288124	1704.958662	16.722714
33.177737	1709.856082	16.727731
33.456323	1715.800510	16.732749
33.616315	1708.324702	16.737767
33.426533	1696.985265	16.742784
32.972922	1690.558286	16.747802
33.352323	1695.043292	16.752819
32.985488	1709.658647	16.757837
33.600673	1704.986683	16.762855
33.339103	1710.166995	16.767872
33.492486	1711.473388	16.772890
33.505080	1709.617460	16.777907
33.552134	1708.437982	16.782925
33.673071	1706.014969	16.787943
33.390103	1714.096378	16.792960
33.675515	1712.160753	16.797978
33.613440	1704.127301	16.802995
33.389995	1705.663696	16.808013
33.730890	1699.613385	16.813031
33.509715	1712.469575	16.818048
33.779648	1729.066193	16.823066
33.741068	1729.715753	16.828083
33.768535	1738.533435	16.833101
34.195393	1739.998358	16.838119
34.091530	1735.008466	16.843136
34.340523	1735.365178	16.848154
33.976108	1734.008281	16.853171
33.909938	1740.789550	16.858189
34.231966	1738.726950	16.863207
34.280508	1732.833375	16.868224
34.249171	1731.118167	16.873242
34.711096	1727.423166	16.878259
34.309572	1715.871294	16.883277
34.304366	1705.312567	16.888295
34.162949	1698.182945	16.893312
34.317941	1697.053896	16.898330
34.667936	1695.668788	16.903347
34.376367	1702.018775	16.908365
34.247935	1689.975813	16.913383
34.460567	1709.752951	16.918400
34.303706	1722.334608	16.923418
34.818862	1722.858091	16.928435
34.802567	1719.261393	16.933453
34.478020	1704.237177	16.938471
34.294652	1707.779198	16.943488
34.310909	1724.972370	16.948506
34.708116	1727.085427	16.953523
34.253254	1739.767330	16.958541
34.290438	1736.321769	16.963559
34.553316	1739.011566	16.968576
34.352316	1739.747598	16.973594
34.515867	1740.410539	16.978611
34.358119	1750.644477	16.983629
34.844801	1763.560851	16.988647
34.989800	1764.042697	16.993664
34.846454	1781.975592	16.998682
35.291801	1786.181889	17.003699
35.140102	1794.630181	17.008717
35.046009	1794.516980	17.013735
35.414550	1790.865961	17.018752
34.993117	1791.024422	17.023770
35.425901	1789.666215	17.028787
35.167846	1793.206011	17.033805
35.406241	1789.942290	17.038823
35.615031	1793.404476	17.043840
35.537806	1780.034206	17.048858
35.674988	1753.000204	17.053875
35.298423	1751.596477	17.058893
35.410133	1752.086778	17.063911
35.561032	1746.090350	17.068928
35.612292	1754.530630	17.073946
35.506801	1748.316317	17.078963
35.524021	1752.981026	17.083981
35.476935	1750.525026	17.088999
35.186681	1759.800837	17.094016
35.113022	1752.098776	17.099034
35.469331	1760.830198	17.104051
35.544392	1783.638766	17.109069
35.780918	1784.437943	17.114087
35.935924	1778.369270	17.119104
35.648807	1784.120007	17.124122
35.959479	1775.899639	17.129139
35.803458	1779.824304	17.134157
35.997838	1780.520085	17.139175
35.989304	1788.534166	17.144192
35.616275	1784.232958	17.149210
35.987058	1779.645574	17.154227
35.606339	1783.304826	17.159245
35.609522	1780.946989	17.164263
35.802952	1773.242430	17.169280
35.419187	1772.906428	17.174298
35.614967	1767.790075	17.179315
35.659556	1783.876824	17.184333
35.835124	1798.316085	17.189351
36.207117	1800.507112	17.194368
35.944870	1805.476766	17.199386
35.978105	1794.485525	17.204403
35.770750	1803.617571	17.209421
35.849332	1807.560670	17.214439
36.504841	1813.153990	17.219456
36.245309	1829.999565	17.224474
36.424551	1819.191885	17.229491
36.610518	1824.025556	17.234509
36.749887	1821.970055	17.239527
36.965068	1824.362288	17.244544
36.747432	1823.238391	17.249562
37.036105	1817.602229	17.254579
36.679850	1806.331735	17.259597
36.672381	1800.431335	17.264615
36.864788	1801.658362	17.269632
36.387508	1804.014739	17.274650
36.576422	1810.534330	17.279667
36.714841	1812.378770	17.284685
36.796195	1815.813308	17.289703
37.191193	1812.674051	17.294720
36.779343	1814.294781	17.299738
37.014097	1811.631784	17.304755
37.293213	1815.555485	17.309773
37.169140	1816.584438	17.314791
37.103095	1812.102901	17.319808
36.936153	1817.813247	17.324826
37.181219	1809.365781	17.329843
37.068533	1815.282204	17.334861
36.677197	1812.882675	17.339879
36.926741	1812.410262	17.344896
36.660959	1814.123319	17.349914
37.113460	1808.730035	17.354931
37.201367	1816.996968	17.359949
37.188788	1833.600225	17.364967
37.181855	1841.649475	17.369984
37.403598	1846.400364	17.375002
37.538551	1838.737347	17.380019
37.448234	1840.280052	17.385037
37.216308	1842.356611	17.390055
37.633748	1839.657392	17.395072
37.445177	1836.315461	17.400090
37.662331	1845.559947	17.405107
37.388737	1845.577630	17.410125
37.539436	1846.036545	17.415143
37.655378	1842.577611	17.420160
37.556993	1841.585713	17.425178
37.517545	1850.927764	17.430195
37.745484	1846.291566	17.435213
38.030853	1850.585538	17.440231
38.088820	1852.554508	17.445248
37.773554	1852.976840	17.450266
38.036257	1855.941985	17.455283
38.276804	1865.415577	17.460301
37.897627	1860.577314	17.465319
38.374149	1860.617721	17.470336
38.055832	1868.122007	17.475354
38.206064	1874.210464	17.480371
38.300949	1866.984863	17.485389
38.034956	1878.854126	17.490407
38.578855	1885.052056	17.495424
38.545738	1889.722478	17.500442
38.265750	1866.212564	17.505459
38.368020	1869.939528	17.510477
38.413026	1881.706489	17.515495
38.663415	1881.188318	17.520512
38.659722	1858.497999	17.525530
38.014339	1849.855100	17.530547
38.256614	1869.011059	17.535565
38.450345	1884.226997	17.540583
38.710443	1872.689816	17.545600
38.391415	1873.889877	17.550618
38.932035	1872.757513	17.555635
38.902428	1873.339577	17.560653
38.565777	1877.868846	17.565671
38.770433	1875.301094	17.570688
38.433073	1867.375959	17.575706
38.570262	1874.776919	17.580723
38.506125	1868.634615	17.585741
38.609326	1885.711069	17.590759
39.157772	1902.244585	17.595776
38.994494	1909.778436	17.600794
38.977887	1909.113288	17.605811
39.154047	1905.441799	17.610829
39.121238	1903.493980	17.615847
39.127966	1911.755037	17.620864
39.160750	1905.139475	17.625882
39.161413	1906.599244	17.630899
39.352841	1904.394632	17.635917
39.109066	1903.506936	17.640935
39.235998	1903.080034	17.645952
39.138469	1902.018777	17.650970
39.062873	1900.936717	17.655987
39.614207	1905.716859	17.661005
39.008555	1911.903085	17.666023
39.404791	1901.977087	17.671040
39.214513	1906.138501	17.676058
39.519559	1915.063824	17.681075
39.777787	1927.274260	17.686093
39.675562	1937.017305	17.691111
39.912946	1929.147553	17.696128
39.946175	1937.848024	17.701146
39.606627	1912.321327	17.706163
39.993517	1920.249600	17.711181
39.767795	1932.599370	17.716199
40.208116	1941.986874	17.721216
40.359206	1927.098938	17.726234
40.067043	1923.259878	17.731251
39.931188	1917.534863	17.736269
39.450520	1918.856671	17.741287
39.931687	1916.787543	17.746304
39.978506	1923.347940	17.751322
40.118585	1925.142576	17.756339
40.073033	1921.591396	17.761357
39.887109	1927.764956	17.766375
40.051969	1926.454977	17.771392
40.133266	1923.828236	17.776410
39.869087	1921.871697	17.781427
40.186580	1929.162123	17.786445
39.818997	1932.581771	17.791463
40.095744	1948.715050	17.796480
40.361118	1955.020361	17.801498
40.312269	1957.693847	17.806515
40.655528	1943.167743	17.811533
40.208526	1950.060979	17.816551
40.750845	1951.286482	17.821568
40.478693	1960.178831	17.826586
40.493075	1950.693620	17.831603
40.686785	1953.645406	17.836621
40.668248	1959.594851	17.841639
40.966577	1973.782667	17.846656
40.731066	1982.511084	17.851674
40.854061	1990.511376	17.856691
41.304836	1988.984316	17.861709
41.153102	1986.404958	17.866727
40.965002	1976.191409	17.871744
41.340953	1969.948192	17.876762
41.004674	1973.904019	17.881779
41.389084	1963.455221	17.886797
41.067097	1959.288189	17.891815
41.502136	1955.773613	17.896832
41.487740	1956.678108	17.901850
41.250539	1956.895281	17.906867
41.443950	1955.381743	17.911885
41.360648	1962.283047	17.916903
41.357617	1954.579838	17.921920
41.535159	1952.508006	17.926938
41.194044	1958.870725	17.931955
41.566544	1950.476791	17.936973
41.332197	1951.290517	17.941991
41.326519	1954.976514	17.947008
41.579146	1976.909138	17.952026
41.303867	1980.696349	17.957043
41.653042	1983.042067	17.962061
41.792201	1978.854176	17.967079
41.774683	1979.568033	17.972096
42.000102	1983.682830	17.977114
41.684889	1977.859760	17.982131
42.002099	1975.745197	17.987149
41.940573	1981.634649	17.992167
41.945944	1980.881828	17.997184
42.209604	1976.257983	18.002202
42.009867	1978.754964	18.007219
42.661828	1971.318539	18.012237
42.265179	1984.324087	18.017255
42.058832	1975.922569	18.022272
42.274899	1979.446566	18.027290
42.092920	1985.787848	18.032307
42.557503	1976.878164	18.037325
42.123876	1975.795784	18.042343
42.142655	1970.719390	18.047360
42.390613	1971.435739	18.052378
42.028850	1977.097776	18.057395
42.482730	1969.644178	18.062413
42.531345	1973.484341	18.067431
42.142544	1974.599577	18.072448
42.417813	1972.068527	18.077466
42.256894	1999.395394	18.082483
42.909829	1996.634989	18.087501
42.678635	2006.198074	18.092519
42.520794	2014.099229	18.097536
42.773317	2012.820096	18.102554
42.575797	2013.186682	18.107571
42.810954	2002.546927	18.112589
43.011739	2004.625283	18.117607
43.009345	2007.026293	18.122624
43.281753	2000.223019	18.127642
42.934535	2009.675613	18.132659
43.451473	2003.861389	18.137677
42.678010	2004.729642	18.142695
43.102962	2002.976233	18.147712
43.365252	1995.511492	18.152730
43.096301	2010.616515	18.157747
42.970891	2012.431483	18.162765
42.951514	2012.273327	18.167783
42.867789	2006.284325	18.172800
43.347839	2020.686254	18.177818
43.133792	2038.710185	18.182835
43.364647	2029.670994	18.187853
43.471375	2022.958635	18.192871
43.525055	2031.427793	18.197888
43.683678	2032.193789	18.202906
43.705070	2037.918229	18.207923
43.692928	2032.948215	18.212941
43.565923	2035.949598	18.217959
43.367509	2029.057011	18.222976
43.804101	2035.501804	18.227994
43.497193	2039.231148	18.233011
43.699511	2031.606054	18.238029
43.790922	2045.642098	18.243047
43.776072	2049.694554	18.248064
44.111901	2047.669041	18.253082
43.878275	2049.843435	18.258099
43.901256	2055.621117	18.263117
43.678887	2055.501629	18.268135
44.140786	2065.426938	18.273152
44.481133	2055.328051	18.278170
44.109842	2064.346396	18.283187
44.591660	2049.015442	18.288205
44.180495	2055.715019	18.293223
44.116158	2059.710872	18.298240
44.504557	2057.992390	18.303258
44.485329	2063.757929	18.308275
44.735166	2054.253974	18.313293
44.780393	2055.849806	18.318311
44.730695	2051.196474	18.323328
45.054600	2041.408558	18.328346
44.634272	2045.997632	18.333363
44.975544	2043.109162	18.338381
44.854941	2049.940159	18.343399
44.873019	2050.844986	18.348416
45.407230	2052.083591	18.353434
45.046500	2052.477783	18.358451
44.660617	2051.621395	18.363469
44.921998	2052.920034	18.368487
44.913422	2052.386529	18.373504
44.896809	2050.500607	18.378522
44.859156	2050.969120	18.383539
45.017716	2048.142041	18.388557
44.899818	2049.645118	18.393575
44.729372	2056.957587	18.398592
45.095565	2058.134108	18.403610
44.940584	2075.228367	18.408627
45.104460	2084.030007	18.413645
45.348298	2086.077125	18.418663
45.186382	2084.156166	18.423680
45.314616	2081.764177	18.428698
45.157304	2093.779887	18.433715
45.085865	2087.624497	18.438733
45.505107	2093.303594	18.443751
45.533330	2108.361319	18.448768
45.715335	2106.916445	18.453786
45.533574	2111.690878	18.458803
45.931284	2113.092845	18.463821
46.080042	2117.739050	18.468839
46.087835	2105.935948	18.473856
46.228349	2102.160762	18.478874
45.892012	2080.353782	18.483891
45.893931	2082.371839	18.488909
46.419638	2073.129064	18.493927
46.093188	2073.244845	18.498944
46.092305	2072.127258	18.503962
45.739660	2078.719975	18.508979
46.167103	2094.118313	18.513997
46.398112	2097.155423	18.519015
46.470782	2106.375926	18.524032
46.594799	2094.383608	18.529050
46.315876	2097.526435	18.534067
46.375841	2102.624136	18.539085
46.743404	2102.961948	18.544103
46.325430	2097.825386	18.549120
46.714000	2090.936683	18.554138
46.416407	2091.613413	18.559155
46.626557	2099.191629	18.564173
46.914351	2098.610853	18.569191
46.604003	2100.159575	18.574208
47.093137	2098.360523	18.579226
46.576019	2103.204172	18.584243
46.861562	2097.422886	18.589261
46.614673	2100.002132	18.594279
46.567136	2105.605447	18.599296
46.979856	2099.031454	18.604314
46.848669	2097.293586	18.609331
47.096848	2098.918406	18.614349
47.074457	2104.555466	18.619367
46.981040	2105.865864	18.624384
46.995320	2102.686589	18.629402
46.896629	2108.297277	18.634419
46.817925	2109.457452	18.639437
47.344040	2116.824820	18.644455
47.355080	2124.704605	18.649472
47.537585	2122.506105	18.654490
47.031083	2133.405536	18.659507
46.899545	2132.198662	18.664525
47.501582	2119.252256	18.669543
47.141380	2133.599536	18.674560
47.655315	2138.510790	18.679578
47.680148	2155.014842	18.684595
47.491880	2161.033129	18.689613
47.852977	2158.872212	18.694631
47.617504	2165.064786	18.699648
47.826434	2158.502819	18.704666
47.718593	2158.295057	18.709683
47.699303	2154.313304	18.714701
48.079258	2155.562363	18.719719
47.661084	2158.102866	18.724736
47.980009	2148.491081	18.729754
47.661056	2159.384215	18.734771
47.756554	2172.151757	18.739789
48.128231	2173.644407	18.744807
48.062392	2189.755510	18.749824
48.404090	2192.385626	18.754842
48.338552	2192.047622	18.759859
48.277679	2193.253728	18.764877
48.474661	2187.574629	18.769895
48.326383	2188.356547	18.774912
48.666579	2178.501442	18.779930
48.552801	2192.209312	18.784947
48.530345	2191.792858	18.789965
48.637109	2181.341781	18.794983
48.225534	2188.643220	18.800000
48.537789	2176.837909	18.805018
48.931903	2196.003117	18.810035
49.062577	2207.141567	18.815053
49.165218	2194.326662	18.820071
48.975720	2188.674595	18.825088
49.321490	2175.297849	18.830106
49.064532	2185.744560	18.835123
48.792110	2183.950549	18.840141
49.180894	2185.360240	18.845159
49.387408	2214.446702	18.850176
49.366941	2218.398632	18.855194
49.214014	2204.079623	18.860211
49.313899	2218.813758	18.865229
49.462527	2212.590965	18.870247
49.401687	2216.206381	18.875264
49.482166	2213.597810	18.880282
49.455239	2218.726716	18.885299
49.549991	2214.175360	18.890317
49.800332	2203.920825	18.895335
49.585908	2208.970297	18.900352
49.577222	2211.063215	18.905370
49.785697	2203.966422	18.910387
49.599288	2205.932729	18.915405
50.025465	2198.665923	18.920423
49.627574	2206.139023	18.925440
49.887075	2204.150834	18.930458
49.908648	2204.683059	18.935475
49.484983	2204.461955	18.940493
49.993774	2201.188841	18.945511
49.711813	2207.693256	18.950528
50.101435	2215.217738	18.955546
50.407092	2218.336571	18.960563
50.298174	2223.447879	18.965581
50.354979	2222.265232	18.970599
50.150847	2220.328964	18.975616
50.613365	2224.431971	18.980634
50.374342	2216.313190	18.985651
50.238454	2230.303074	18.990669
50.698621	2221.976022	18.995687
50.675953	2221.882102	19.000704
50.467756	2215.033462	19.005722
50.531102	2217.471216	19.010739
50.423082	2215.070478	19.015757
50.624899	2211.911609	19.020775
50.385526	2224.005801	19.025792
50.449147	2217.417430	19.030810
50.763650	2237.888540	19.035827
50.582370	2246.843653	19.040845
50.832167	2239.878692	19.045863
51.107556	2249.494857	19.050880
51.176691	2249.313141	19.055898
51.212783	2257.372277	19.060915
51.237656	2254.133858	19.065933
51.148957	2248.292641	19.070951
51.454760	2256.113685	19.075968
51.227295	2246.472568	19.080986
51.391276	2247.746645	19.086003
51.139474	2257.757602	19.091021
51.499937	2240.578443	19.096039
51.374868	2241.866371	19.101056
51.474292	2257.301468	19.106074
51.745896	2271.424619	19.111091
51.822370	2279.806121	19.116109
51.504932	2274.859546	19.121127
51.467918	2284.198339	19.126144
51.435588	2280.290997	19.131162
51.859912	2277.069881	19.136179
51.815153	2287.073007	19.141197
52.120758	2275.514094	19.146215
52.075505	2277.654543	19.151232
51.951165	2277.836413	19.156250
51.971587	2272.731335	19.161267
51.952448	2275.901198	19.166285
52.328808	2287.537765	19.171303
52.411342	2296.579833	19.176320
52.106885	2310.097193	19.181338
52.461997	2304.720838	19.186355
52.432511	2305.114904	19.191373
52.551519	2304.411589	19.196391
52.462780	2299.858008	19.201408
52.253272	2302.372332	19.206426
52.154537	2303.123543	19.211443
52.286736	2300.885058	19.216461
52.951095	2301.805598	19.221479
53.095330	2299.785439	19.226496
52.902894	2305.956263	19.231514
53.186232	2294.923969	19.236531
53.216671	2296.785694	19.241549
53.178999	2297.280963	19.246567
53.132280	2299.180953	19.251584
52.831168	2300.246827	19.256602
53.267008	2295.577330	19.261619
52.699083	2301.093816	19.266637
53.157176	2302.073998	19.271655
52.731537	2307.287766	19.276672
52.915998	2307.058552	19.281690
53.556055	2316.510409	19.286707
53.447451	2326.062015	19.291725
53.281887	2327.192798	19.296743
53.735559	2326.261481	19.301760
53.412985	2331.549277	19.306778
53.702187	2327.626823	19.311795
53.439503	2322.134256	19.316813
54.043601	2320.872177	19.321831
53.875890	2321.564384	19.326848
53.664342	2323.475720	19.331866
53.918330	2321.240619	19.336883
53.783509	2332.377461	19.341901
54.093262	2324.383473	19.346919
54.179627	2316.551759	19.351936
53.703593	2323.075380	19.356954
53.771609	2327.052555	19.361971
54.008688	2320.911573	19.366989
54.177295	2347.167109	19.372007
53.959029	2348.183590	19.377024
54.023404	2356.447504	19.382042
54.526128	2345.170161	19.387059
54.292042	2354.164439	19.392077
54.461052	2357.664571	19.397095
54.450180	2359.379508	19.402112
54.730929	2357.195981	19.407130
54.838347	2353.142835	19.412147
54.844264	2360.174830	19.417165
54.988659	2352.994581	19.422183
55.017837	2351.847007	19.427200
54.689425	2351.212690	19.432218
55.256025	2355.104846	19.437235
54.742990	2351.255276	19.442253
54.893343	2351.040154	19.447271
55.002384	2346.986751	19.452288
54.865106	2347.084160	19.457306
55.174719	2351.607248	19.462323
55.056355	2361.183245	19.467341
55.266916	2374.310964	19.472359
55.525687	2375.905023	19.477376
55.245009	2382.908799	19.482394
55.537063	2375.900063	19.487411
55.547497	2384.699615	19.492429
55.579329	2386.912738	19.497447
55.960045	2393.195913	19.502464
55.646585	2410.500689	19.507482
55.733542	2395.621719	19.512499
55.747251	2400.689146	19.517517
55.760460	2396.673038	19.522535
55.820994	2389.844383	19.527552
55.815938	2398.740019	19.532570
56.091902	2387.817381	19.537587
55.946614	2381.595772	19.542605
55.991712	2380.930986	19.547623
55.891968	2378.285843	19.552640
55.453223	2375.051334	19.557658
55.890097	2368.828124	19.562675
55.917244	2386.751086	19.567693
56.308643	2397.763146	19.572711
56.040760	2401.369940	19.577728
55.996357	2399.759781	19.582746
56.045569	2403.933479	19.587763
55.973905	2404.261121	19.592781
56.184670	2419.543337	19.597799
56.262551	2431.948935	19.602816
56.244352	2434.922820	19.607834
56.762673	2428.321613	19.612851
56.748958	2438.034356	19.617869
56.636064	2438.090119	19.622887
56.984931	2432.352092	19.627904
56.808740	2447.117904	19.632922
57.061608	2457.660479	19.637939
57.418584	2470.394445	19.642957
57.148145	2469.258465	19.647975
57.117960	2462.098141	19.652992
57.330474	2468.581227	19.658010
57.401001	2469.986646	19.663027
57.491934	2477.381132	19.668045
57.574359	2474.291592	19.673063
57.726537	2461.474844	19.678080
57.599710	2459.264276	19.683098
57.740293	2440.641146	19.688115
57.596336	2441.011783	19.693133
57.486165	2459.084164	19.698151
58.048790	2459.176921	19.703168
57.747249	2471.946696	19.708186
58.014269	2461.050602	19.713203
58.062424	2453.295704	19.718221
57.889802	2452.808014	19.723239
58.047804	2447.159417	19.728256
57.857971	2454.296618	19.733274
58.460062	2447.495618	19.738291
58.309687	2444.056207	19.743309
58.143895	2452.903572	19.748327
58.482818	2448.706499	19.753344
58.126825	2445.561033	19.758362
58.284774	2447.374124	19.763379
58.264405	2452.405314	19.768397
57.867314	2447.558696	19.773415
58.404474	2450.559639	19.778432
58.280697	2448.649066	19.783450
58.339923	2458.565717	19.788467
58.390626	2475.245350	19.793485
58.510519	2478.129571	19.798503
58.589692	2468.895628	19.803520
58.430104	2483.105848	19.808538
58.727250	2489.308788	19.813555
58.726607	2501.358840	19.818573
58.709356	2511.507973	19.823591
59.218312	2504.347379	19.828608
59.037725	2514.696404	19.833626
58.977020	2516.870817	19.838643
59.024460	2515.120140	19.843661
59.055183	2521.474923	19.848679
59.391210	2519.208616	19.853696
59.272954	2510.161883	19.858714
59.613632	2519.302146	19.863731
59.708849	2532.511333	19.868749
59.486405	2537.383637	19.873767
59.668332	2534.856368	19.878784
59.680721	2537.004181	19.883802
59.838531	2537.801799	19.888819
59.868406	2528.218564	19.893837
59.975867	2537.637521	19.898855
59.898599	2531.690536	19.903872
59.818877	2536.841346	19.908890
60.101563	2526.820555	19.913907
60.072495	2531.499189	19.918925
60.044196	2543.624481	19.923943
60.197275	2524.524929	19.928960
60.148327	2527.337763	19.933978
60.081971	2528.230915	19.938995
60.000902	2528.041689	19.944013
60.263765	2555.437300	19.949031
60.553148	2558.644544	19.954048
60.489900	2560.979050	19.959066
60.724452	2563.607446	19.964083
60.561707	2555.531372	19.969101
60.435965	2566.436468	19.974119
60.769663	2554.171990	19.979136
60.834248	2564.581846	19.984154
61.040076	2557.830625	19.989171
61.232422	2554.283037	19.994189
60.971982	2557.670006	19.999207
61.102299	2559.527635	20.004224
60.827315	2566.497551	20.009242
61.170805	2581.227023	20.014259
61.439722	2582.227960	20.019277
60.990562	2593.515033	20.024295
61.374679	2582.366552	20.029312
61.322188	2591.778018	20.034330
61.304196	2588.285208	20.039347
61.453810	2587.971089	20.044365
61.190228	2596.117537	20.049383
61.590719	2599.528893	20.054400
61.264411	2612.906068	20.059418
61.703069	2617.542382	20.064435
61.656894	2616.152731	20.069453
61.615878	2622.941409	20.074471
61.923487	2615.761745	20.079488
61.750994	2617.532380	20.084506
61.977799	2615.908046	20.089523
62.354192	2614.004993	20.094541
62.103961	2625.296547	20.099559
62.670878	2627.528198	20.104576
62.337254	2628.609505	20.109594
62.557007	2637.671590	20.114611
63.008383	2619.354212	20.119629
62.554571	2613.075517	20.124647
62.846105	2601.958306	20.129664
62.895108	2606.453818	20.134682
62.737782	2603.695893	20.139699
62.914174	2599.719779	20.144717
62.788046	2607.515510	20.149735
62.994798	2594.447667	20.154752
62.984048	2598.437479	20.159770
63.147690	2606.397805	20.164787
63.404483	2607.321230	20.169805
62.966648	2611.280836	20.174823
63.213835	2600.922695	20.179840
63.403118	2598.330527	20.184858
62.806955	2608.428109	20.189875
63.098186	2605.152637	20.194893
63.419906	2620.888546	20.199911
63.419432	2616.690495	20.204928
63.641146	2631.395390	20.209946
63.568807	2630.278144	20.214963
63.535295	2626.926243	20.219981
63.352958	2636.227084	20.224999
63.600764	2627.392488	20.230016
63.453050	2629.754635	20.235034
63.402590	2641.009620	20.240051
63.697729	2652.730229	20.245069
63.745544	2661.485442	20.250087
64.091427	2661.528604	20.255104
64.037745	2666.591139	20.260122
63.939044	2664.816555	20.265139
64.333504	2660.155118	20.270157
64.062988	2670.187432	20.275175
64.182528	2666.232167	20.280192
64.237984	2679.405351	20.285210
64.412518	2684.399243	20.290227
64.748398	2682.375212	20.295245
64.352211	2685.971074	20.300263
64.684905	2682.623683	20.305280
64.730265	2676.645282	20.310298
64.563543	2688.120218	20.315315
64.606340	2681.104682	20.320333
64.533014	2702.397381	20.325351
64.859929	2700.425907	20.330368
64.960730	2706.409326	20.335386
64.700006	2720.058532	20.340403
64.802582	2717.200925	20.345421
65.000293	2721.527231	20.350439
65.261147	2716.303418	20.355456
65.499156	2740.773207	20.360474
65.256587	2737.984802	20.365491
65.496815	2724.644842	20.370509
65.301113	2736.966901	20.375527
65.573547	2735.113452	20.380544
65.637734	2742.440756	20.385562
65.509509	2733.725852	20.390579
65.764919	2728.139488	20.395597
65.742889	2734.456367	20.400615
65.672231	2734.481796	20.405632
65.994385	2745.878807	20.410650
65.931695	2764.589016	20.415667
66.516051	2765.029144	20.420685
66.106960	2770.942881	20.425703
66.351013	2771.493134	20.430720
66.601894	2765.389884	20.435738
66.405643	2776.081409	20.440755
66.442628	2763.108928	20.445773
66.717267	2766.531743	20.450791
66.761098	2767.792778	20.455808
66.707509	2766.561619	20.460826
66.352789	2765.142501	20.465843
66.753539	2771.876524	20.470861
66.798521	2770.163966	20.475879
66.609205	2759.273570	20.480896
66.793602	2761.631540	20.485914
66.840163	2771.059575	20.490931
66.794074	2769.537744	20.495949
66.929758	2781.725967	20.500967
66.924393	2794.780737	20.505984
67.556125	2799.726137	20.511002
67.404430	2795.810162	20.516019
67.775302	2782.611357	20.521037
67.548794	2802.235045	20.526055
67.439115	2797.403826	20.531072
67.967825	2791.122530	20.536090
67.773871	2788.488404	20.541107
67.662976	2789.191234	20.546125
67.461974	2793.545755	20.551143
67.650510	2795.784291	20.556160
67.792830	2797.920859	20.561178
67.685604	2801.676756	20.566195
67.979651	2807.685246	20.571213
68.080598	2836.827544	20.576231
68.180390	2841.882968	20.581248
68.520741	2835.560898	20.586266
68.311636	2848.499539	20.591283
68.695849	2842.158672	20.596301
68.573101	2852.207660	20.601319
68.629486	2843.060498	20.606336
68.352686	2831.842607	20.611354
68.136060	2830.340102	20.616371
68.749005	2828.079928	20.621389
68.510628	2822.621838	20.626407
68.630659	2817.928605	20.631424
69.011734	2833.569537	20.636442
68.931151	2841.248000	20.641459
68.742260	2849.395262	20.646477
68.978303	2853.477149	20.651495
68.800197	2848.973833	20.656512
68.807176	2845.785335	20.661530
68.758859	2850.099002	20.666547
69.248007	2858.245896	20.671565
69.329924	2881.774059	20.676583
69.278150	2892.555900	20.681600
69.521577	2876.838904	20.686618
69.496027	2877.414067	20.691635
69.741727	2874.249633	20.696653
69.235619	2870.889667	20.701671
69.264583	2868.841405	20.706688
69.561647	2877.666336	20.711706
69.392581	2897.605078	20.716723
69.692063	2899.075498	20.721741
69.764578	2907.321119	20.726759
69.574565	2908.554959	20.731776
70.068634	2920.323507	20.736794
70.155966	2933.186625	20.741811
70.264177	2942.714279	20.746829
70.545650	2938.254846	20.751847
70.676637	2928.038508	20.756864
70.919927	2933.448658	20.761882
70.447666	2939.086992	20.766899
70.671422	2931.030876	20.771917
71.299802	2928.778452	20.776935
70.672361	2929.617949	20.781952
70.987174	2923.857632	20.786970
70.940979	2926.185542	20.791987
71.065460	2928.288004	20.797005
71.197492	2928.791625	20.802023
71.125175	2927.635022	20.807040
71.005636	2938.969689	20.812058
71.099736	2950.192416	20.817075
71.361601	2958.219864	20.822093
71.503188	2961.472796	20.827111
71.511727	2963.302701	20.832128
71.687216	2959.481600	20.837146
71.772261	2957.358305	20.842163
71.551510	2955.944546	20.847181
71.713656	2958.806392	20.852199
71.699498	2969.189764	20.857216
71.799718	2961.298073	20.862234
72.054107	2973.271654	20.867251
72.105153	2979.599011	20.872269
72.218881	2985.691397	20.877287
72.154057	2991.636058	20.882304
72.204542	2979.126917	20.887322
72.641019	2978.510599	20.892339
72.989212	2981.241303	20.897357
73.067171	2982.471741	20.902375
72.627927	2974.983091	20.907392
73.287734	2968.191531	20.912410
72.617231	2960.439280	20.917427
72.726321	2944.030167	20.922445
73.174478	2956.479419	20.927463
72.907568	2952.408719	20.932480
72.917645	2945.756977	20.937498
72.985818	2953.202532	20.942515
73.241167	2969.877623	20.947533
73.370472	2985.590337	20.952551
73.533258	2980.103606	20.957568
73.490100	2985.210197	20.962586
73.559796	2986.657490	20.967603
73.470653	2993.768667	20.972621
73.917503	2978.672021	20.977639
73.586420	2983.242427	20.982656
73.768496	2986.671405	20.987674
73.844201	2986.395811	20.992691
73.907275	2980.652023	20.997709
74.021601	2983.379907	21.002727
73.879457	2993.280266	21.007744
73.817194	2983.039646	21.012762
73.864369	2989.082079	21.017779
73.717802	2982.305843	21.022797
74.022343	2984.738297	21.027815
73.971283	2996.895913	21.032832
74.196931	3004.439880	21.037850
74.047984	3012.343299	21.042867
74.168274	3012.186455	21.047885
74.115419	3012.299507	21.052903
74.358996	3033.279411	21.057920
74.809090	3037.881000	21.062938
74.864916	3044.350003	21.067955
74.672204	3050.891684	21.072973
74.843808	3038.197983	21.077991
75.065721	3045.249350	21.083008
75.197159	3039.277525	21.088026
75.238304	3040.922101	21.093043
75.402889	3040.095849	21.098061
75.546108	3039.651374	21.103079
75.212409	3048.180544	21.108096
75.499199	3033.218712	21.113114
75.747945	3040.219385	21.118131
75.683500	3049.279854	21.123149
75.678156	3049.998901	21.128167
75.606398	3057.834970	21.133184
75.869806	3058.615778	21.138202
75.937737	3061.509189	21.143219
75.892208	3056.672372	21.148237
75.979582	3043.640475	21.153255
75.796571	3044.095231	21.158272
75.818080	3039.808595	21.163290
76.025239	3047.070773	21.168307
75.871899	3065.319125	21.173325
75.971567	3071.802387	21.178343
76.168088	3071.804870	21.183360
76.123488	3071.712868	21.188378
76.275570	3091.061812	21.193395
76.444811	3097.947758	21.198413
77.031095	3107.842150	21.203431
76.978097	3109.400273	21.208448
77.017841	3097.172786	21.213466
76.877815	3100.167021	21.218483
76.409165	3103.994009	21.223501
76.943702	3106.162466	21.228519
76.863209	3118.619865	21.233536
77.276714	3130.686195	21.238554
77.229226	3141.120628	21.243571
77.500466	3133.731763	21.248589
77.533369	3133.100354	21.253607
77.490677	3139.959549	21.258624
77.567556	3140.370499	21.263642
77.409557	3129.992438	21.268659
76.956851	3140.417553	21.273677
77.252124	3150.753277	21.278695
77.696426	3153.071434	21.283712
77.717792	3161.306477	21.288730
78.164988	3172.775918	21.293747
78.003638	3194.544339	21.298765
78.053977	3197.025238	21.303783
78.007895	3204.098183	21.308800
78.445898	3199.969269	21.313818
78.454830	3198.743834	21.318835
78.484169	3212.125403	21.323853
78.490743	3199.708821	21.328871
78.391280	3196.611952	21.333888
78.939563	3216.109480	21.338906
78.890282	3228.030224	21.343923
78.752346	3237.699590	21.348941
79.150474	3218.933709	21.353959
79.132438	3227.808319	21.358976
79.282908	3226.227559	21.363994
79.141259	3224.295348	21.369011
79.250124	3224.231575	21.374029
79.553623	3224.570986	21.379047
79.427050	3223.174433	21.384064
79.510626	3220.823209	21.389082
79.892123	3234.641072	21.394099
79.578006	3251.627565	21.399117
80.104926	3244.440153	21.404135
80.291292	3249.994802	21.409152
80.157390	3253.549755	21.414170
80.239080	3246.673275	21.419187
80.282235	3255.118862	21.424205
80.347443	3246.145463	21.429223
80.566096	3255.690320	21.434240
80.501858	3247.206403	21.439258
80.392868	3252.390451	21.444275
80.453534	3255.220555	21.449293
80.915843	3245.036114	21.454311
80.505177	3248.347293	21.459328
80.716521	3259.124413	21.464346
80.703127	3242.508735	21.469363
80.756710	3249.919796	21.474381
80.902673	3250.247360	21.479399
80.684291	3255.065760	21.484416
80.540940	3254.479761	21.489434
80.719594	3266.799199	21.494451
80.765759	3275.604601	21.499469
81.234764	3284.808266	21.504487
81.141364	3278.673967	21.509504
81.113125	3282.090932	21.514522
81.435278	3292.317059	21.519539
81.160436	3302.699762	21.524557
81.626145	3303.364150	21.529575
81.247433	3306.244671	21.534592
81.324799	3310.842860	21.539610
82.145572	3327.239390	21.544627
81.988336	3339.074390	21.549645
82.024645	3334.514703	21.554663
82.160031	3336.105737	21.559680
82.246798	3336.304294	21.564698
82.214941	3337.819737	21.569715
82.162054	3339.205591	21.574733
82.591538	3334.469921	21.579751
82.564518	3348.343604	21.584768
82.436898	3355.911053	21.589786
82.923929	3359.960923	21.594803
82.762121	3372.570741	21.599821
83.397096	3365.336147	21.604839
83.117847	3363.932463	21.609856
83.300581	3367.613941	21.614874
83.266914	3360.796711	21.619891
82.953367	3358.451373	21.624909
83.327998	3358.078541	21.629927
83.259793	3356.833929	21.634944
83.256274	3351.096683	21.639962
83.767792	3364.806616	21.644979
82.900444	3384.519123	21.649997
83.535971	3377.678546	21.655015
83.833796	3381.709037	21.660032
83.674963	3388.579005	21.665050
84.122234	3375.358047	21.670067
84.122750	3379.502031	21.675085
84.245587	3375.500425	21.680103
84.208362	3385.148319	21.685120
84.652818	3404.495889	21.690138
84.593516	3404.526586	21.695155
84.433622	3409.310535	21.700173
84.700281	3407.654589	21.705191
84.474761	3408.511818	21.710208
84.534065	3409.717736	21.715226
84.708621	3404.875597	21.720243
84.515195	3407.555884	21.725261
85.039331	3394.771828	21.730279
85.152841	3395.059732	21.735296
84.794839	3401.000183	21.740314
85.278554	3407.624514	21.745331
85.124275	3424.819350	21.750349
85.561488	3424.383831	21.755367
85.527427	3419.393241	21.760384
85.903934	3424.802782	21.765402
85.618233	3427.015571	21.770419
85.715839	3430.481726	21.775437
85.974311	3422.776946	21.780455
85.847977	3423.469681	21.785472
85.636807	3430.882937	21.790490
85.851455	3418.208790	21.795507
85.821749	3420.154983	21.800525
85.915425	3420.962881	21.805543
85.923373	3443.379619	21.810560
85.839120	3460.295867	21.815578
86.283181	3460.561736	21.820595
86.092288	3456.938962	21.825613
86.337971	3458.768869	21.830631
86.546000	3473.350931	21.835648
86.472955	3488.051779	21.840666
86.962075	3476.653029	21.845683
86.747021	3481.334880	21.850701
87.123591	3474.350695	21.855719
87.242427	3475.184476	21.860736
86.955573	3475.448127	21.865754
87.307394	3475.199289	21.870771
87.520561	3491.843158	21.875789
87.444279	3501.602769	21.880807
87.500004	3505.771811	21.885824
87.669254	3508.975615	21.890842
87.684575	3495.609467	21.895859
87.777106	3501.847835	21.900877
87.881923	3495.622048	21.905895
88.013631	3501.564678	21.910912
88.001634	3506.211007	21.915930
88.151916	3500.007074	21.920947
87.764966	3511.649145	21.925965
88.042935	3526.091094	21.930983
88.355272	3537.680663	21.936000
88.248294	3534.883850	21.941018
88.554171	3516.886707	21.946035
88.335510	3531.951444	21.951053
88.405159	3540.864965	21.956071
88.855415	3561.291899	21.961088
88.543562	3569.893403	21.966106
88.909152	3562.325652	21.971123
88.712740	3571.981750	21.976141
88.798457	3560.242141	21.981159
88.894282	3577.485375	21.986176
88.943641	3596.223614	21.991194
89.778891	3589.527302	21.996211
89.523941	3604.199063	22.001229
89.533624	3593.224388	22.006247
89.556344	3596.951110	22.011264
89.744137	3594.211902	22.016282
89.881546	3586.597930	22.021299
89.890046	3600.795797	22.026317
89.997438	3614.050432	22.031335
90.189425	3620.955025	22.036352
90.088308	3628.964426	22.041370
90.203392	3621.951072	22.046387
90.096974	3626.916936	22.051405
90.081833	3630.174560	22.056423
90.126141	3627.033431	22.061440
90.342891	3638.256793	22.066458
90.647070	3641.295935	22.071475
90.349088	3657.177419	22.076493
90.490709	3651.796868	22.081511
90.883738	3650.654099	22.086528
90.696710	3664.544945	22.091546
91.102054	3676.737323	22.096563
91.329933	3692.020502	22.101581
91.057850	3689.578030	22.106599
91.396618	3685.744077	22.111616
91.187229	3689.215985	22.116634
91.147387	3685.597385	22.121651
91.294098	3705.729943	22.126669
91.654937	3713.986678	22.131687
91.444757	3717.424106	22.136704
91.297904	3728.279149	22.141722
91.912342	3732.534580	22.146739
92.249240	3742.612352	22.151757
92.083918	3764.221769	22.156775
92.408735	3758.147227	22.161792
92.391723	3756.855083	22.166810
92.409884	3753.954098	22.171827
92.552206	3745.053844	22.176845
92.632431	3755.174132	22.181863
93.118133	3750.219326	22.186880
93.298006	3750.875043	22.191898
93.428199	3741.893337	22.196915
93.514435	3741.677412	22.201933
93.513650	3736.718380	22.206951
93.680585	3724.981421	22.211968
93.546730	3734.598542	22.216986
93.402686	3728.887492	22.222003
93.766966	3728.246477	22.227021
93.791860	3726.219985	22.232039
93.898276	3720.039475	22.237056
93.705941	3732.121896	22.242074
94.113007	3723.261248	22.247091
94.317997	3714.165364	22.252109
93.831449	3729.017358	22.257127
93.981070	3738.593206	22.262144
93.740109	3752.977324	22.267162
93.945422	3754.466786	22.272179
94.351180	3754.971626	22.277197
94.052121	3761.397634	22.282215
94.525856	3773.351839	22.287232
94.551410	3797.397862	22.292250
94.765140	3787.365975	22.297267
94.775538	3793.767032	22.302285
94.812820	3793.889315	22.307303
95.017509	3784.021712	22.312320
95.020413	3775.933490	22.317338
95.124205	3786.035881	22.322355
95.320917	3789.484742	22.327373
95.344030	3802.462707	22.332391
95.453781	3809.690453	22.337408
95.388685	3824.644464	22.342426
95.548084	3816.946626	22.347443
95.863276	3820.548095	22.352461
95.563076	3818.851917	22.357479
95.915800	3811.117744	22.362496
95.928557	3827.480860	22.367514
96.279702	3835.677063	22.372531
96.321280	3841.598018	22.377549
96.339412	3844.894437	22.382567
96.588544	3835.372929	22.387584
96.258661	3840.501943	22.392602
96.301151	3836.426491	22.397619
96.611071	3833.250040	22.402637
96.505221	3852.115626	22.407655
96.687247	3867.973494	22.412672
96.953821	3881.250972	22.417690
96.948543	3876.945551	22.422707
96.879866	3881.328061	22.427725
96.834388	3878.863579	22.432743
97.194168	3885.056343	22.437760
97.005585	3908.674133	22.442778
96.998983	3902.683853	22.447795
97.375198	3912.278746	22.452813
97.274720	3920.541513	22.457831
97.459701	3930.693990	22.462848
97.781538	3936.540396	22.467866
97.706014	3945.142976	22.472883
97.930652	3946.894487	22.477901
97.979205	3961.937502	22.482919
98.167627	3961.955441	22.487936
98.013770	3972.337413	22.492954
98.061095	3965.859419	22.497971
98.612911	3981.361859	22.502989
98.479819	3991.045106	22.508007
98.662159	3999.048837	22.513024
98.980903	3989.895309	22.518042
99.041585	3996.406438	22.523059
99.135157	3992.464400	22.528077
99.257222	3994.576842	22.533095
99.421570	3991.692618	22.538112
99.279692	4001.149922	22.543130
99.671169	4017.165713	22.548147
99.738820	4021.733422	22.553165
99.609325	4023.503657	22.558183
99.877980	4012.717082	22.563200
99.648761	4025.292581	22.568218
99.980134	4027.772857	22.573235
100.369069	4023.030852	22.578253
99.949555	4021.197127	22.583271
100.385659	4012.670736	22.588288
100.119298	4017.529288	22.593306
100.129237	4022.164415	22.598323
100.601472	4032.733723	22.603341
100.346528	4042.443516	22.608359
100.606493	4034.978906	22.613376
101.151295	4034.052632	22.618394
101.365654	4030.467357	22.623411
101.315819	4032.140714	22.628429
101.076297	4040.633407	22.633447
101.167404	4025.660082	22.638464
100.987661	4032.185969	22.643482
101.045168	4029.971723	22.648499
101.499173	4038.632301	22.653517
101.690572	4061.220543	22.658535
102.069088	4061.197154	22.663552
101.803435	4060.053984	22.668570
101.867115	4063.256653	22.673587
101.946653	4059.659830	22.678605
101.954420	4070.046776	22.683623
102.307942	4058.668419	22.688640
102.682447	4065.953979	22.693658
102.440645	4060.669039	22.698675
102.713874	4068.803851	22.703693
102.362829	4093.666422	22.708711
102.558737	4092.197116	22.713728
102.563779	4098.098041	22.718746
102.658286	4095.205267	22.723763
103.254585	4096.257951	22.728781
102.788175	4101.470187	22.733799
102.895147	4110.455985	22.738816
102.859721	4122.294216	22.743834
103.007487	4135.927575	22.748851
103.687982	4128.787625	22.753869
103.137453	4137.154539	22.758887
103.461057	4152.649500	22.763904
103.471546	4160.144989	22.768922
103.517245	4163.516539	22.773939
103.899677	4168.643780	22.778957
103.714150	4186.387304	22.783975
104.233109	4193.870165	22.788992
104.439407	4197.583497	22.794010
104.069001	4198.854861	22.799027
104.565800	4184.534142	22.804045
104.266540	4201.074875	22.809063
104.495188	4206.614493	22.814080
105.065068	4215.711407	22.819098
104.958833	4217.921651	22.824115
105.246244	4218.113399	22.829133
105.056399	4222.705713	22.834151
105.106713	4211.703644	22.839168
105.581928	4211.631007	22.844186
105.510765	4219.773623	22.849203
105.513255	4216.004963	22.854221
105.806907	4236.280021	22.859239
106.045639	4238.850631	22.864256
105.776557	4253.968199	22.869274
105.820532	4246.415990	22.874291
106.005554	4238.065610	22.879309
106.092433	4244.271367	22.884327
106.021630	4244.484052	22.889344
106.159329	4240.147071	22.894362
106.126033	4246.295684	22.899379
106.393908	4249.016627	22.904397
106.145581	4273.296698	22.909415
106.259144	4272.301511	22.914432
106.293382	4278.272588	22.919450
106.523294	4285.594690	22.924467
106.850878	4293.842898	22.929485
106.762400	4299.913010	22.934503
106.901086	4318.696140	22.939520
107.349815	4327.995745	22.944538
107.168255	4328.646192	22.949555
107.459065	4332.311467	22.954573
107.639002	4334.129944	22.959591
107.702448	4342.613043	22.964608
107.718904	4360.759612	22.969626
107.711834	4364.090847	22.974643
108.056348	4356.538643	22.979661
108.075652	4371.599328	22.984679
107.872413	4363.251005	22.989696
108.383925	4374.657642	22.994714
108.074538	4389.300314	22.999731
108.409437	4388.932227	23.004749
108.560412	4390.328150	23.009767
108.970363	4405.472900	23.014784
109.082283	4420.507852	23.019802
108.960285	4424.443524	23.024819
109.192795	4420.450894	23.029837
109.362124	4419.885786	23.034855
109.377959	4431.588644	23.039872
109.748134	4420.852453	23.044890
109.332187	4434.489447	23.049907
109.906538	4444.229316	23.054925
109.792108	4456.387229	23.059943
109.667713	4454.107524	23.064960
110.353694	4448.554123	23.069978
110.141080	4445.788928	23.074995
110.487608	4435.194958	23.080013
110.412308	4449.600537	23.085031
110.460554	4456.503273	23.090048
110.841412	4460.352470	23.095066
110.713029	4481.344988	23.100083
110.954216	4492.517119	23.105101
110.953860	4490.599968	23.110119
110.989867	4490.199298	23.115136
111.272485	4484.135912	23.120154
110.932743	4494.300866	23.125171
111.281618	4480.152927	23.130189
111.254647	4492.715452	23.135207
111.299396	4506.147664	23.140224
111.721574	4504.009721	23.145242
111.315649	4517.221943	23.150259
111.352717	4517.676258	23.155277
111.933407	4528.901268	23.160295
112.122299	4546.698802	23.165312
112.318043	4543.038488	23.170330
111.900697	4552.629759	23.175347
112.304712	4541.091145	23.180365
112.613228	4548.714742	23.185383
112.642480	4557.320638	23.190400
112.712326	4542.572819	23.195418
112.664983	4562.617916	23.200435
112.906483	4572.090759	23.205453
112.836028	4574.231627	23.210471
112.971567	4576.870676	23.215488
113.040299	4574.888213	23.220506
112.703514	4590.412638	23.225523
113.334055	4603.651611	23.230541
113.482904	4605.817301	23.235559
113.663808	4608.644227	23.240576
113.773922	4615.345999	23.245594
114.145749	4626.741281	23.250611
114.179637	4630.783530	23.255629
114.138873	4639.628787	23.260647
114.050214	4639.812069	23.265664
114.655540	4637.113082	23.270682
114.289887	4633.600488	23.275699
114.907817	4640.114298	23.280717
114.847360	4650.489718	23.285735
114.614567	4663.518691	23.290752
114.954741	4662.569160	23.295770
114.557780	4670.800167	23.300787
114.828835	4668.729571	23.305805
115.393107	4679.007747	23.310823
115.374612	4686.111619	23.315840
115.599500	4685.069544	23.320858
115.381582	4695.252184	23.325875
115.599003	4689.523239	23.330893
115.802497	4695.052107	23.335911
116.089051	4705.193643	23.340928
116.942929	4702.535254	23.345946
116.715008	4702.024044	23.350963
117.049314	4696.434588	23.355981
117.065224	4679.717420	23.360999
116.940756	4662.768547	23.366016
116.935100	4661.494967	23.371034
116.979628	4665.419095	23.376051
117.317932	4656.234504	23.381069
117.292701	4650.158778	23.386087
117.231500	4661.660117	23.391104
117.634327	4671.639906	23.396122
117.656893	4678.069303	23.401139
117.552324	4671.584539	23.406157
117.752919	4681.509259	23.411175
117.729191	4685.464731	23.416192
117.750996	4690.586728	23.421210
117.804629	4695.484944	23.426227
118.104104	4683.593920	23.431245
118.142140	4688.739290	23.436263
117.858132	4694.434010	23.441280
118.448286	4693.825386	23.446298
118.495660	4713.130229	23.451315
118.234110	4726.642956	23.456333
118.538277	4717.492880	23.461351
118.463111	4721.843631	23.466368
118.759656	4731.626421	23.471386
118.529084	4749.897041	23.476403
118.514609	4752.139935	23.481421
118.859184	4760.536748	23.486439
118.796208	4784.573325	23.491456
119.066825	4786.871462	23.496474
119.416120	4806.581434	23.501491
119.431330	4816.771825	23.506509
119.619286	4815.081075	23.511527
119.489791	4816.822295	23.516544
119.740954	4823.982360	23.521562
119.882352	4838.679466	23.526579
119.868031	4836.996582	23.531597
119.856778	4836.819789	23.536615
120.126297	4856.784862	23.541632
120.259589	4866.532411	23.546650
120.310929	4884.752734	23.551667
120.284525	4903.839866	23.556685
120.734187	4903.182834	23.561703
120.651875	4925.743670	23.566720
121.187834	4934.648188	23.571738
121.402656	4943.950085	23.576755
121.548078	4947.630046	23.581773
121.571038	4936.232139	23.586791
121.754436	4953.759619	23.591808
122.161472	4968.460912	23.596826
122.037530	4965.476928	23.601843
122.018835	4966.729242	23.606861
122.422248	4967.227427	23.611879
122.418452	4965.598707	23.616896
122.898529	4966.871401	23.621914
122.626913	4964.851899	23.626931
122.577099	4972.635920	23.631949
122.766016	4985.496439	23.636967
122.781738	4988.758095	23.641984
123.030936	5002.597942	23.647002
123.243443	4994.488216	23.652019
123.051498	5003.455353	23.657037
123.193238	5011.484207	23.662055
123.395232	5019.302839	23.667072
123.784563	5026.374097	23.672090
123.695957	5026.467687	23.677107
123.720887	5029.317208	23.682125
124.170660	5042.048064	23.687143
124.130624	5058.402082	23.692160
124.451697	5054.428992	23.697178
124.941839	5056.464012	23.702195
124.714073	5052.003336	23.707213
124.940942	5050.447180	23.712231
124.691964	5060.893074	23.717248
124.986928	5049.707395	23.722266
125.153390	5048.592791	23.727283
124.947884	5051.024328	23.732301
125.599344	5052.351521	23.737319
125.456220	5059.964011	23.742336
125.449116	5069.501208	23.747354
125.789985	5068.771043	23.752371
125.811427	5070.751781	23.757389
125.856997	5069.409418	23.762407
125.712341	5070.724312	23.767424
125.654996	5083.763439	23.772442
126.179585	5093.925506	23.777459
126.073569	5101.932551	23.782477
126.442178	5094.870205	23.787495
126.622896	5104.161120	23.792512
126.629209	5117.987096	23.797530
126.829496	5121.014797	23.802547
126.954234	5125.270063	23.807565
126.641543	5126.392256	23.812583
126.580533	5138.827798	23.817600
127.159889	5153.408963	23.822618
127.261617	5166.680062	23.827635
127.422391	5176.650016	23.832653
127.379575	5178.751160	23.837671
127.727113	5191.311203	23.842688
127.865421	5187.317657	23.847706
127.754275	5198.171231	23.852723
128.196435	5216.304466	23.857741
128.579874	5212.629007	23.862759
128.366849	5222.751435	23.867776
128.477339	5211.671366	23.872794
128.728887	5228.120689	23.877811
128.960470	5246.512551	23.882829
129.270639	5233.227624	23.887847
128.942471	5246.712109	23.892864
129.252160	5251.388726	23.897882
129.265541	5252.044315	23.902899
129.276579	5251.325040	23.907917
129.836903	5259.064631	23.912935
129.663782	5277.654026	23.917952
130.134707	5281.755003	23.922970
130.138993	5280.188687	23.927987
129.986056	5282.967489	23.933005
130.082375	5285.973253	23.938023
130.078050	5302.378492	23.943040
130.390730	5312.373881	23.948058
130.683020	5299.103547	23.953075
130.727647	5302.884640	23.958093
130.831344	5304.561195	23.963111
130.945969	5325.375332	23.968128
131.250337	5329.505242	23.973146
131.312550	5331.259223	23.978163
130.971977	5340.144052	23.983181
131.308135	5336.726290	23.988199
131.322077	5354.996428	23.993216
131.646567	5358.180606	23.998234
131.761612	5363.588509	24.003251
131.474408	5371.620659	24.008269
132.269556	5373.164145	24.013287
132.064241	5393.752459	24.018304
132.112075	5398.829640	24.023322
132.409760	5398.316411	24.028339
132.683980	5405.046661	24.033357
133.032633	5414.708305	24.038375
133.037957	5427.571736	24.043392
133.138389	5424.350469	24.048410
133.299668	5421.255608	24.053427
133.189694	5429.096669	24.058445
133.412046	5420.864766	24.063463
133.765969	5442.240419	24.068480
133.564116	5456.348520	24.073498
133.806444	5452.317860	24.078515
133.547841	5465.014918	24.083533
133.928633	5471.529155	24.088551
134.309655	5487.544286	24.093568
134.253503	5491.385556	24.098586
134.536489	5486.069916	24.103603
134.386607	5506.368672	24.108621
134.705850	5513.821122	24.113639
134.647551	5533.224136	24.118656
134.715738	5530.853759	24.123674
134.942291	5526.108853	24.128691
134.795276	5551.909839	24.133709
134.904348	5562.679784	24.138727
135.041791	5572.317778	24.143744
135.183077	5584.748973	24.148762
135.662824	5590.284481	24.153779
136.115428	5602.483518	24.158797
136.588373	5603.559144	24.163815
136.657351	5608.607849	24.168832
136.400419	5618.765085	24.173850
136.760418	5611.250691	24.178867
136.647355	5621.304737	24.183885
136.882975	5615.136666	24.188903
136.917252	5611.214669	24.193920
137.086145	5629.827858	24.198938
137.286993	5640.648528	24.203955
137.124024	5642.609968	24.208973
137.499865	5643.102350	24.213991
137.689105	5643.198058	24.219008
137.850131	5646.650691	24.224026
138.090045	5661.062259	24.229043
138.115556	5665.497939	24.234061
137.765381	5669.209116	24.239079
138.191904	5676.618578	24.244096
137.820292	5673.419028	24.249114
138.345060	5683.384784	24.254131
138.393836	5704.272896	24.259149
138.674129	5707.975602	24.264167
139.056441	5703.592895	24.269184
139.000174	5708.835482	24.274202
139.155336	5722.407762	24.279219
139.050573	5734.654874	24.284237
139.208032	5739.821693	24.289255
139.277189	5737.216669	24.294272
139.343142	5751.774868	24.299290
139.384666	5770.109569	24.304307
139.435838	5776.289408	24.309325
139.781474	5784.394746	24.314343
140.053924	5786.443342	24.319360
140.201017	5796.240446	24.324378
140.488762	5810.816837	24.329395
140.226387	5821.821653	24.334413
140.545598	5820.729057	24.339431
140.940300	5832.050032	24.344448
140.769254	5843.781447	24.349466
141.317989	5846.997639	24.354483
141.404921	5853.160793	24.359501
141.558306	5849.732722	24.364519
141.707141	5867.970968	24.369536
141.553234	5875.890866	24.374554
142.161268	5879.129867	24.379571
142.307029	5888.485073	24.384589
142.129886	5876.214337	24.389607
142.461579	5889.454137	24.394624
142.530290	5909.684756	24.399642
142.817989	5905.872547	24.404659
142.856991	5916.952115	24.409677
142.617376	5915.623679	24.414695
143.152696	5928.097761	24.419712
143.155153	5945.306725	24.424730
143.396709	5954.783598	24.429747
143.274907	5948.526041	24.434765
143.313709	5959.908585	24.439783
143.791259	5970.050437	24.444800
143.485438	5985.321967	24.449818
143.926086	5987.363443	24.454835
144.203122	6012.022071	24.459853
144.192233	6008.828657	24.464871
144.411497	6010.228011	24.469888
144.364410	6022.485833	24.474906
144.585515	6029.714223	24.479923
145.021239	6030.604629	24.484941
144.996311	6035.140517	24.489959
145.238359	6036.489820	24.494976
145.428392	6051.403827	24.499994
145.793753	6062.886230	24.505011
145.448979	6069.463714	24.510029
145.534074	6074.720868	24.515047
146.037311	6071.808171	24.520064
145.828863	6074.953175	24.525082
146.121234	6083.770564	24.530099
146.472886	6095.099392	24.535117
146.318409	6097.720444	24.540135
146.705836	6095.469020	24.545152
146.689192	6109.611939	24.550170
146.964246	6120.049760	24.555187
146.732113	6134.458381	24.560205
147.119054	6120.634842	24.565223
147.659950	6123.457376	24.570240
147.373227	6124.551894	24.575258
148.018805	6123.882462	24.580275
148.100877	6137.417209	24.585293
148.163099	6146.556154	24.590311
148.483980	6139.268037	24.595328
148.192208	6140.623790	24.600346
148.607433	6145.507317	24.605363
148.407193	6144.827982	24.610381
148.557347	6147.539731	24.615399
149.003900	6168.974051	24.620416
149.031934	6172.053042	24.625434
149.074089	6172.202107	24.630451
149.192442	6178.778963	24.635469
148.966190	6179.346129	24.640487
149.384993	6193.585708	24.645504
149.292346	6199.776068	24.650522
149.690040	6209.066127	24.655539
149.938319	6226.842056	24.660557
150.081740	6239.757344	24.665575
150.199885	6238.032720	24.670592
149.915499	6250.350599	24.675610
150.224208	6250.431984	24.680627
150.609797	6266.987767	24.685645
150.378431	6274.069694	24.690663
150.759357	6287.843322	24.695680
150.683989	6303.553660	24.700698
151.044463	6308.920415	24.705715
151.295684	6323.473238	24.710733
151.163285	6335.722891	24.715751
151.628546	6337.443409	24.720768
151.869356	6351.767386	24.725786
151.732979	6360.195384	24.730803
151.967418	6365.705785	24.735821
152.071961	6378.436198	24.740839
152.563309	6387.419531	24.745856
152.968665	6385.117998	24.750874
153.108061	6378.282793	24.755891
153.272975	6394.341237	24.760909
153.256475	6393.492540	24.765927
153.615787	6411.710484	24.770944
153.502382	6419.801245	24.775962
153.399113	6414.995348	24.780979
153.932066	6421.273308	24.785997
153.805757	6420.597907	24.791015
153.897044	6421.407930	24.796032
153.781794	6439.678760	24.801050
154.267455	6444.976821	24.806067
154.265422	6455.448834	24.811085
154.433798	6465.032908	24.816103
154.609627	6468.250478	24.821120
154.698070	6488.142770	24.826138
154.692936	6489.769935	24.831155
154.932590	6497.236362	24.836173
155.249529	6505.795158	24.841191
155.265876	6516.734799	24.846208
155.223751	6519.008333	24.851226
155.435962	6534.814688	24.856243
155.832970	6542.712402	24.861261
155.659361	6559.529991	24.866279
155.767285	6562.218651	24.871296
156.021453	6578.476290	24.876314
156.648725	6599.452028	24.881331
157.049233	6594.665672	24.886349
157.056740	6589.451793	24.891367
157.070446	6584.694069	24.896384
157.122339	6588.560882	24.901402
157.400536	6588.114459	24.906419
157.604169	6610.767597	24.911437
157.339713	6612.564376	24.916455
157.912528	6608.948870	24.921472
158.011215	6617.017722	24.926490
158.705256	6615.637914	24.931507
158.754868	6625.424359	24.936525
158.949747	6630.566640	24.941543
159.082337	6627.897843	24.946560
159.184147	6632.467209	24.951578
159.521471	6627.391138	24.956595
159.503922	6620.743719	24.961613
159.381697	6629.877752	24.966631
159.792221	6630.857195	24.971648
159.689481	6642.479207	24.976666
159.813786	6649.901945	24.981683
160.149403	6658.496407	24.986701
160.142554	6683.652270	24.991719
160.187332	6682.295726	24.996736
160.100083	6686.451485	25.001754
160.504815	6694.978296	25.006771
160.763124	6703.745623	25.011789
160.449835	6720.425153	25.016807
160.766184	6718.816795	25.021824
160.889961	6725.810835	25.026842
160.725225	6736.561559	25.031859
160.983607	6742.756759	25.036877
161.214565	6774.496803	25.041895
161.595405	6774.905816	25.046912
161.729815	6786.720669	25.051930
161.739355	6803.051394	25.056947
162.004875	6799.664239	25.061965
161.731379	6811.451305	25.066983
162.143389	6836.046509	25.072000
162.298109	6839.250215	25.077018
162.226974	6854.693724	25.082035
162.794111	6867.101370	25.087053
162.909352	6872.256434	25.092071
162.834384	6887.350446	25.097088
163.422263	6900.346513	25.102106
163.413113	6914.213609	25.107123
163.878813	6912.874121	25.112141
163.514675	6937.637310	25.117159
164.069897	6937.325320	25.122176
164.176633	6947.981767	25.127194
164.051992	6963.232488	25.132211
164.520429	6962.673891	25.137229
164.424915	6981.810123	25.142247
164.913603	6988.739807	25.147264
164.741777	7005.301104	25.152282
164.772055	7006.216095	25.157299
165.294805	7020.637789	25.162317
165.328168	7036.579418	25.167335
165.517010	7033.645069	25.172352
165.630785	7047.181886	25.177370
165.916448	7062.537245	25.182387
166.048759	7070.150907	25.187405
166.115526	7092.118440	25.192423
166.622390	7092.449143	25.197440
167.066822	7098.725772	25.202458
166.718399	7100.897159	25.207475
167.073235	7116.105420	25.212493
167.337597	7124.340909	25.217511
167.411454	7134.334698	25.222528
167.712512	7138.684394	25.227546
167.590976	7164.000199	25.232563
167.864635	7161.843873	25.237581
167.579683	7179.888516	25.242599
168.136466	7188.318978	25.247616
168.329517	7201.176831	25.252634
168.234623	7209.520008	25.257651
168.585497	7217.194892	25.262669
168.574955	7239.329192	25.267687
168.862450	7242.068030	25.272704
169.229046	7251.780739	25.277722
169.351950	7257.646819	25.282739
169.562180	7262.948178	25.287757
169.443718	7276.216932	25.292775
169.926467	7286.017369	25.297792
169.993113	7290.934040	25.302810
169.726078	7307.681600	25.307827
170.384229	7325.067734	25.312845
170.204001	7330.955422	25.317863
170.894105	7341.796897	25.322880
171.217974	7349.766507	25.327898
170.941499	7354.956656	25.332915
171.253143	7361.747144	25.337933
170.911842	7366.654921	25.342951
171.570413	7373.563996	25.347968
171.604435	7389.741169	25.352986
171.453207	7386.163028	25.358003
172.163655	7400.667293	25.363021
172.208815	7415.976384	25.368039
172.196146	7417.938481	25.373056
172.585208	7420.713879	25.378074
172.267232	7429.678174	25.383091
172.651031	7451.510707	25.388109
172.822804	7462.141415	25.393127
173.194045	7470.990335	25.398144
173.232142	7490.845570	25.403162
173.229925	7504.059008	25.408179
173.685370	7504.766177	25.413197
173.685594	7522.901104	25.418215
173.554434	7533.239449	25.423232
173.745498	7541.733148	25.428250
173.772834	7553.267458	25.433267
174.393657	7577.989544	25.438285
174.251572	7590.104853	25.443303
174.893185	7595.646005	25.448320
174.854030	7621.730029	25.453338
174.801441	7634.921713	25.458355
175.325583	7639.908766	25.463373
175.609890	7656.121075	25.468391
175.499402	7663.458216	25.473408
175.765480	7676.507063	25.478426
175.721801	7695.900335	25.483443
176.280422	7695.443796	25.488461
176.386972	7718.709766	25.493479
176.365423	7729.199948	25.498496
176.773238	7731.903957	25.503514
176.359229	7757.063597	25.508531
176.932630	7761.306317	25.513549
177.009853	7778.524363	25.518567
177.634241	7784.324857	25.523584
178.067465	7786.708497	25.528602
177.943735	7811.642537	25.533619
178.029417	7812.349662	25.538637
178.290054	7807.792177	25.543655
178.542964	7826.026462	25.548672
178.838243	7840.401420	25.553690
178.661481	7852.101486	25.558707
178.977479	7847.399031	25.563725
179.380294	7867.541665	25.568743
179.494587	7879.081641	25.573760
179.655620	7877.678519	25.578778
179.364539	7881.575960	25.583795
179.904106	7897.697472	25.588813
180.348013	7902.375964	25.593831
180.324287	7910.007459	25.598848
180.416583	7913.010072	25.603866
180.651220	7925.688805	25.608883
180.746723	7933.683731	25.613901
180.959775	7937.201001	25.618919
181.350856	7948.039845	25.623936
181.265229	7946.023318	25.628954
181.419020	7958.058307	25.633971
181.565697	7971.021400	25.638989
181.830759	7975.778398	25.644007
181.890773	7979.670640	25.649024
182.600688	7991.375411	25.654042
182.536726	8014.406600	25.659059
182.550033	8006.563465	25.664077
182.861186	8007.984955	25.669095
182.789273	8003.658665	25.674112
183.291087	8019.126912	25.679130
183.235187	8034.869804	25.684148
183.666393	8036.643964	25.689165
183.605709	8035.006273	25.694183
183.725881	8052.421987	25.699200
184.104789	8054.626265	25.704218
184.153360	8072.164370	25.709236
184.280454	8064.314080	25.714253
184.776147	8080.445935	25.719271
184.598217	8097.599193	25.724288
184.800430	8097.845515	25.729306
184.952135	8114.280125	25.734324
185.430552	8127.036622	25.739341
185.618508	8134.108832	25.744359
185.259345	8138.933146	25.749376
185.942971	8144.933261	25.754394
185.829374	8160.662665	25.759412
185.774855	8163.228398	25.764429
185.895673	8179.667611	25.769447
186.194839	8194.336987	25.774464
186.500387	8205.495369	25.779482
186.700074	8215.730286	25.784500
186.777563	8233.786082	25.789517
187.368496	8253.403101	25.794535
187.254620	8265.858337	25.799552
188.176191	8266.013577	25.804570
187.762891	8281.427733	25.809588
187.726149	8295.232048	25.814605
188.168619	8291.045178	25.819623
187.990284	8314.962238	25.824640
188.464360	8317.074265	25.829658
188.428565	8331.906956	25.834676
189.014562	8347.931060	25.839693
189.107623	8353.479696	25.844711
189.084777	8372.089905	25.849728
189.076353	8376.237498	25.854746
189.653900	8392.754820	25.859764
189.508992	8410.355252	25.864781
189.779301	8415.807583	25.869799
189.978185	8443.275863	25.874816
190.351320	8453.025303	25.879834
190.496647	8466.817666	25.884852
190.709155	8472.415371	25.889869
191.134718	8484.008092	25.894887
190.834028	8498.732880	25.899904
190.979755	8495.911358	25.904922
191.139100	8521.715847	25.909940
191.598213	8524.349659	25.914957
191.766613	8537.668224	25.919975
191.669266	8555.861272	25.924992
191.829513	8555.670863	25.930010
192.058550	8586.717855	25.935028
191.899404	8597.563453	25.940045
192.370871	8613.502230	25.945063
192.435415	8631.472827	25.950080
192.899554	8638.813259	25.955098
192.999760	8663.096060	25.960116
193.396356	8686.570683	25.965133
193.794502	8690.458776	25.970151
193.846044	8701.037925	25.975168
194.213030	8709.037198	25.980186
194.334430	8720.914285	25.985204
194.513170	8729.654575	25.990221
194.960519	8742.741164	25.995239
194.827037	8761.494617	26.000256
195.551402	8745.256036	26.005274
195.515415	8767.765331	26.010292
195.807165	8783.854132	26.015309
196.104433	8789.120126	26.020327
196.049461	8786.206999	26.025344
196.342529	8786.753624	26.030362
196.520577	8802.705547	26.035380
196.432045	8802.611852	26.040397
196.798412	8804.170202	26.045415
196.620022	8830.617305	26.050432
197.229599	8824.518538	26.055450
197.366810	8835.842733	26.060468
197.205783	8865.538758	26.065485
197.448083	8859.265206	26.070503
197.894044	8883.090718	26.075520
198.271070	8900.525489	26.080538
198.510104	8909.056388	26.085556
198.390756	8911.315054	26.090573
198.619039	8915.198811	26.095591
198.661092	8929.074169	26.100608
199.271111	8938.330520	26.105626
199.656161	8953.468165	26.110644
199.688633	8958.460873	26.115661
200.383761	8947.149863	26.120679
200.532153	8951.390655	26.125696
200.883406	8943.846489	26.130714
200.722173	8940.595361	26.135732
200.845218	8947.526819	26.140749
201.518606	8958.079801	26.145767
201.532456	8964.193334	26.150784
202.061245	8956.144361	26.155802
202.105916	8957.434518	26.160820
202.288875	8952.410613	26.165837
202.360371	8927.836343	26.170855
202.399115	8927.022369	26.175872
202.538003	8944.434564	26.180890
202.482610	8943.388892	26.185908
202.551173	8958.974015	26.190925
202.771246	8948.211697	26.195943
202.302241	8961.748730	26.200960
202.695779	8973.890326	26.205978
203.218711	8979.649238	26.210996
202.888822	9001.625370	26.216013
203.353616	9009.259807	26.221031
203.462292	9030.575850	26.226048
203.797262	9047.714130	26.231066
203.847698	9059.975420	26.236084
203.862250	9079.807006	26.241101
204.326697	9084.278388	26.246119
204.250889	9126.478593	26.251136
204.712790	9126.188147	26.256154
204.632384	9147.028095	26.261172
205.131911	9167.323508	26.266189
205.144479	9177.843890	26.271207
205.169727	9197.479941	26.276224
205.835080	9220.242461	26.281242
206.114958	9232.185188	26.286260
205.862014	9252.108045	26.291277
206.434538	9266.497625	26.296295
206.327605	9286.883985	26.301312
206.581765	9298.383084	26.306330
207.129379	9304.950334	26.311348
207.450651	9331.772341	26.316365
207.531724	9330.871327	26.321383
207.812318	9347.893098	26.326400
207.767362	9356.894492	26.331418
208.143437	9381.973380	26.336436
208.424892	9387.839023	26.341453
209.176770	9389.145530	26.346471
208.859520	9407.961746	26.351488
209.496316	9402.584389	26.356506
209.605814	9410.346505	26.361524
209.824243	9423.031061	26.366541
209.902348	9435.251259	26.371559
209.862933	9450.635330	26.376576
210.407294	9468.310475	26.381594
210.446938	9475.989718	26.386612
210.086316	9486.616639	26.391629
210.492976	9501.083649	26.396647
210.586062	9515.238264	26.401664
210.665608	9533.896939	26.406682
211.384985	9542.591255	26.411700
211.346310	9567.938435	26.416717
211.522532	9582.994327	26.421735
211.679625	9607.327429	26.426752
211.613600	9617.456535	26.431770
212.106257	9642.043903	26.436788
212.475355	9656.775182	26.441805
212.808830	9654.044708	26.446823
212.940568	9679.846147	26.451840
213.225597	9687.702404	26.456858
213.587200	9689.161271	26.461876
213.596021	9713.983685	26.466893
213.607487	9718.784822	26.471911
213.818003	9726.227220	26.476928
214.459140	9742.637922	26.481946
214.407832	9753.870096	26.486964
214.681471	9765.440817	26.491981
214.772179	9781.973156	26.496999
215.050477	9792.644023	26.502016
215.288582	9805.093210	26.507034
215.327909	9808.328548	26.512052
215.994856	9829.988385	26.517069
216.053358	9842.353303	26.522087
216.199868	9844.546506	26.527104
216.319981	9855.942272	26.532122
216.495632	9870.642822	26.537140
216.457324	9886.810612	26.542157
216.967282	9902.458558	26.547175
217.187719	9912.120758	26.552192
217.553353	9930.891321	26.557210
217.713872	9934.032994	26.562228
217.739648	9945.484004	26.567245
218.367950	9970.285598	26.572263
218.517546	9972.734102	26.577280
218.615439	9996.860060	26.582298
219.215081	9991.189364	26.587316
219.354028	10011.004705	26.592333
219.402534	10012.653214	26.597351
219.951980	10026.380225	26.602368
220.153687	10034.866169	26.607386
220.552516	10037.843559	26.612404
220.324845	10044.069620	26.617421
220.720240	10059.641161	26.622439
220.658659	10075.349319	26.627456
220.815283	10080.702729	26.632474
221.197341	10081.994679	26.637492
221.033946	10106.615389	26.642509
221.266325	10101.889764	26.647527
221.407267	10132.236643	26.652544
221.525859	10142.249705	26.657562
222.042509	10155.179316	26.662580
222.368306	10166.581877	26.667597
222.440234	10189.404670	26.672615
222.206699	10199.582514	26.677632
222.678947	10229.289661	26.682650
222.917668	10237.131554	26.687668
222.965177	10272.317597	26.692685
223.344141	10284.465729	26.697703
223.887716	10298.492401	26.702720
223.865545	10321.002603	26.707738
224.198446	10324.112548	26.712756
224.207995	10341.675658	26.717773
224.370742	10348.844623	26.722791
224.753496	10371.270670	26.727808
224.980237	10384.951866	26.732826
225.315390	10394.507942	26.737844
225.338373	10416.353138	26.742861
225.557165	10419.907467	26.747879
226.107264	10433.917682	26.752896
225.933913	10452.674084	26.757914
226.219182	10458.980274	26.762932
226.176021	10489.889643	26.767949
226.431105	10508.671469	26.772967
226.780975	10525.498973	26.777984
226.910408	10552.353348	26.783002
227.344143	10560.371308	26.788020
227.319020	10587.353878	26.793037
227.723137	10598.366113	26.798055
228.066947	10608.367191	26.803072
227.874578	10636.227685	26.808090
228.421216	10655.496821	26.813108
228.304937	10683.860385	26.818125
228.780257	10692.933104	26.823143
229.180625	10724.416039	26.828160
229.117672	10736.037233	26.833178
229.968370	10745.476321	26.838196
229.789186	10771.833294	26.843213
230.349848	10799.430404	26.848231
230.612955	10802.374099	26.853248
230.736638	10830.556836	26.858266
231.098741	10837.489621	26.863284
231.406718	10850.059184	26.868301
232.217371	10859.832926	26.873319
232.165420	10870.798436	26.878336
232.207178	10876.517922	26.883354
232.452455	10870.757794	26.888372
232.677335	10878.656928	26.893389
232.887102	10882.353293	26.898407
233.515433	10883.819346	26.903424
233.479715	10908.376537	26.908442
233.751916	10912.334488	26.913460
233.832412	10907.405371	26.918477
233.782875	10931.957720	26.923495
234.391580	10936.066271	26.928512
234.449417	10944.525687	26.933530
234.860019	10964.226172	26.938548
234.807268	10977.633314	26.943565
234.621124	10994.815966	26.948583
234.958475	11004.775444	26.953600
235.066502	11027.120335	26.958618
235.140679	11044.085243	26.963636
235.238056	11072.711012	26.968653
235.566474	11090.049825	26.973671
235.983952	11094.408887	26.978688
235.920847	11132.126060	26.983706
236.676832	11143.467473	26.988724
237.037746	11157.155331	26.993741
237.183065	11182.132139	26.998759
237.532155	11178.012109	27.003776
237.456290	11198.105274	27.008794
237.794858	11213.625680	27.013812
238.039598	11228.404691	27.018829
238.359257	11243.010623	27.023847
238.782428	11254.773719	27.028864
238.589350	11279.989005	27.033882
239.167961	11291.538257	27.038900
239.250528	11304.419804	27.043917
239.623984	11324.987142	27.048935
239.975920	11319.027636	27.053952
240.134132	11345.418003	27.058970
240.075742	11348.888448	27.063988
240.610087	11377.007720	27.069005
240.886194	11382.460804	27.074023
241.312965	11391.244960	27.079040
241.256296	11420.440992	27.084058
241.187633	11418.531480	27.089076
241.568634	11436.300511	27.094093
241.826780	11455.418517	27.099111
242.112846	11470.426907	27.104128
242.151594	11491.799684	27.109146
242.247967	11513.331740	27.114164
242.621730	11534.679899	27.119181
242.381345	11550.255952	27.124199
243.046634	11573.410084	27.129216
242.943481	11604.044792	27.134234
243.684293	11613.798681	27.139252
243.780282	11648.234038	27.144269
244.110472	11672.777426	27.149287
244.544574	11693.879278	27.154304
244.374803	11704.713446	27.159322
244.831399	11731.158058	27.164340
244.929605	11753.613417	27.169357
245.177990	11772.748531	27.174375
245.672705	11791.953413	27.179392
245.992687	11802.403398	27.184410
246.473852	11818.734635	27.189428
246.563089	11837.533728	27.194445
246.772815	11864.735365	27.199463
247.394202	11866.969261	27.204480
247.431410	11886.982738	27.209498
247.830506	11899.539437	27.214516
247.586885	11910.148213	27.219533
248.225941	11934.898005	27.224551
248.353243	11939.145957	27.229568
248.455924	11958.520591	27.234586
248.614489	11967.146342	27.239604
249.148583	11993.236079	27.244621
249.060517	12010.861745	27.249639
249.865208	12012.589853	27.254656
249.899866	12032.771974	27.259674
250.067854	12041.907096	27.264692
250.330996	12069.500041	27.269709
250.072054	12078.674120	27.274727
250.716461	12085.479047	27.279744
250.502040	12103.583453	27.284762
250.878052	12130.184666	27.289780
251.310529	12140.230874	27.294797
251.209195	12168.102096	27.299815
251.466989	12184.089161	27.304832
251.869853	12211.900751	27.309850
252.000032	12226.578965	27.314868
252.518146	12244.870001	27.319885
252.785404	12273.627001	27.324903
253.355374	12276.188924	27.329920
253.091899	12302.078105	27.334938
253.149947	12318.857904	27.339956
253.558073	12342.402117	27.344973
253.743035	12364.020827	27.349991
254.262470	12384.016333	27.355008
254.258450	12412.289860	27.360026
254.553911	12425.426902	27.365044
255.024881	12452.327014	27.370061
255.459109	12479.454213	27.375079
255.888801	12493.744114	27.380096
256.132700	12499.995573	27.385114
256.280518	12515.062064	27.390132
256.626620	12524.171838	27.395149
257.000855	12542.405883	27.400167
257.421748	12539.230999	27.405184
257.531851	12564.622446	27.410202
258.073281	12575.958807	27.415220
258.517482	12589.224787	27.420237
258.246178	12601.087045	27.425255
258.760384	12615.481462	27.430272
258.644139	12621.580610	27.435290
258.703504	12642.529223	27.440308
259.406763	12644.015596	27.445325
259.117062	12675.124762	27.450343
259.470053	12686.129555	27.455360
259.363321	12718.474968	27.460378
259.878398	12740.180914	27.465396
260.130073	12763.000573	27.470413
260.034248	12784.981269	27.475431
260.644382	12806.825355	27.480448
260.861008	12832.235885	27.485466
261.203871	12853.663934	27.490484
261.808858	12862.369180	27.495501
261.619085	12889.924331	27.500519
261.975101	12909.910471	27.505536
262.428607	12925.115685	27.510554
262.801078	12933.726976	27.515572
263.762891	12952.580616	27.520589
263.926199	12960.208361	27.525607
264.709136	12960.534104	27.530624
264.679961	12964.081827	27.535642
264.665119	12958.232993	27.540660
265.082140	12963.427453	27.545677
265.239849	12988.168323	27.550695
265.267466	12985.757985	27.555712
265.455448	12986.810062	27.560730
265.606594	12991.922247	27.565748
266.029682	13008.876040	27.570765
265.921057	13023.135556	27.575783
266.357227	13022.733259	27.580800
266.785339	13037.007690	27.585818
266.332227	13047.067265	27.590836
266.644913	13066.185101	27.595853
266.742747	13085.535869	27.600871
267.196213	13099.596244	27.605888
267.125125	13124.751545	27.610906
267.210666	13147.942549	27.615924
267.697641	13167.914549	27.620941
267.759167	13207.777097	27.625959
268.091503	13230.398435	27.630976
268.145280	13259.821750	27.635994
268.760050	13291.952118	27.641012
269.230980	13305.440284	27.646029
269.340067	13332.387833	27.651047
269.752814	13362.565699	27.656064
270.494004	13373.211068	27.661082
270.696733	13388.898425	27.666100
271.122824	13400.095766	27.671117
271.707360	13418.909763	27.676135
272.236407	13421.988404	27.681152
272.623517	13422.016535	27.686170
272.538225	13441.580160	27.691188
272.728087	13450.889266	27.696205
272.982012	13453.089788	27.701223
273.247026	13470.527825	27.706240
273.290620	13491.971318	27.711258
273.530529	13499.389640	27.716276
274.087701	13502.995852	27.721293
274.056118	13528.672340	27.726311
274.332399	13530.274791	27.731328
274.879102	13542.353547	27.736346
275.414359	13555.760640	27.741364
275.530045	13570.255208	27.746381
275.527664	13577.564002	27.751399
275.776429	13583.893263	27.756416
276.146643	13605.839817	27.761434
276.624488	13615.052149	27.766452
277.120154	13630.538086	27.771469
276.742087	13643.906442	27.776487
276.865963	13650.923075	27.781504
277.329316	13677.167201	27.786522
277.322380	13691.378757	27.791540
277.606930	13700.178764	27.796557
277.922972	13735.203872	27.801575
277.909737	13746.634840	27.806592
278.332960	13765.911282	27.811610
278.386920	13786.439702	27.816628
278.890996	13803.980823	27.821645
278.946974	13835.009299	27.826663
279.666129	13853.242089	27.831680
280.094110	13867.783297	27.836698
280.256108	13884.821800	27.841716
280.744494	13896.570360	27.846733
280.789217	13908.915499	27.851751
281.118324	13922.925711	27.856768
281.298578	13927.093849	27.861786
281.464593	13962.696205	27.866804
281.555437	13966.777943	27.871821
281.631432	13992.125540	27.876839
281.879801	14023.719622	27.881856
282.469990	14045.134230	27.886874
282.360303	14070.842871	27.891892
282.788878	14089.425535	27.896909
282.894431	14113.123154	27.901927
283.458529	14129.711414	27.906944
283.626359	14162.569033	27.911962
284.084159	14183.708650	27.916980
284.105701	14204.064984	27.921997
284.730550	14234.598373	27.927015
284.961348	14254.621785	27.932032
285.206969	14276.834284	27.937050
285.689334	14301.432639	27.942068
285.740880	14325.623730	27.947085
286.347180	14351.000556	27.952103
286.584421	14372.357145	27.957120
286.768830	14381.333216	27.962138
286.808403	14417.506463	27.967156
287.645423	14438.385637	27.972173
287.693300	14455.815817	27.977191
287.893284	14475.703122	27.982208
288.330529	14495.967702	27.987226
288.550187	14518.091895	27.992244
289.287376	14517.709881	27.997261
289.422811	14539.274227	28.002279
289.926120	14551.882149	28.007296
290.229178	14578.283465	28.012314
290.205562	14595.582906	28.017332
290.818039	14609.166574	28.022349
290.892156	14628.743599	28.027367
290.892595	14653.963319	28.032384
291.310436	14659.276911	28.037402
291.190156	14689.933325	28.042420
291.624441	14704.840886	28.047437
291.736664	14734.466534	28.052455
292.257824	14752.085240	28.057472
292.729209	14773.640748	28.062490
292.942104	14810.952911	28.067508
293.621439	14815.690534	28.072525
293.686274	14834.544442	28.077543
293.948698	14855.973463	28.082560
294.338868	14866.252296	28.087578
294.448466	14896.161297	28.092596
294.838517	14901.694915	28.097613
294.888522	14917.135794	28.102631
294.977433	14943.880574	28.107648
295.059047	14958.265275	28.112666
295.234530	14988.179010	28.117684
295.763983	15000.649401	28.122701
296.081300	15033.814230	28.127719
296.177421	15053.333573	28.132736
296.626762	15077.499838	28.137754
296.551168	15108.231935	28.142772
296.953101	15131.512592	28.147789
297.365047	15167.972778	28.152807
297.502149	15193.187541	28.157824
298.271157	15230.947819	28.162842
298.447277	15248.812121	28.167860
298.683309	15259.712243	28.172877
299.079007	15289.986674	28.177895
299.342698	15318.139640	28.182912
299.822186	15344.715202	28.187930
300.039680	15373.846147	28.192948
300.389670	15399.429614	28.197965
300.645227	15418.960026	28.202983
300.906029	15453.961256	28.208000
301.165848	15474.430679	28.213018
301.326567	15504.543016	28.218036
301.710350	15528.232619	28.223053
302.001883	15556.117055	28.228071
302.212241	15589.903388	28.233088
302.823259	15604.553671	28.238106
303.225667	15629.611130	28.243124
303.474660	15652.933882	28.248141
304.067475	15674.218680	28.253159
304.264993	15695.419683	28.258176
304.556788	15716.753700	28.263194
304.684030	15742.131345	28.268212
305.064088	15764.084345	28.273229
305.185927	15785.323515	28.278247
305.656505	15799.548003	28.283264
306.253160	15812.566146	28.288282
306.678392	15830.174812	28.293300
307.267121	15850.279360	28.298317
307.402701	15856.864386	28.303335
307.667090	15871.663468	28.308352
308.525665	15878.581046	28.313370
308.861146	15883.042360	28.318388
309.279192	15895.528484	28.323405
309.596374	15905.532186	28.328423
309.128151	15921.008251	28.333440
309.533335	15930.797181	28.338458
309.712686	15943.790229	28.343476
309.791352	15954.028608	28.348493
310.479059	15979.497410	28.353511
310.373796	15999.705287	28.358528
310.974238	16019.343481	28.363546
310.564074	16030.661872	28.368564
311.060580	16050.005290	28.373581
311.280301	16072.094903	28.378599
311.216676	16092.077785	28.383616
311.788920	16125.481666	28.388634
312.408353	16145.940920	28.393652
312.510845	16165.072116	28.398669
312.994696	16185.728605	28.403687
313.277019	16204.803238	28.408704
314.255247	16216.615952	28.413722
314.157648	16241.848384	28.418740
314.459972	16258.974033	28.423757
314.941708	16258.810254	28.428775
314.945341	16298.917657	28.433792
315.205519	16306.560665	28.438810
315.599686	16340.467955	28.443828
315.867600	16359.196094	28.448845
315.948387	16379.785995	28.453863
315.896629	16412.602420	28.458880
316.614064	16434.990553	28.463898
316.581110	16459.654228	28.468916
317.046111	16483.009551	28.473933
317.302242	16515.897781	28.478951
317.487114	16548.277600	28.483968
317.773543	16577.788776	28.488986
318.104741	16609.116547	28.494004
318.565803	16640.913606	28.499021
319.280411	16665.141950	28.504039
319.601227	16690.016713	28.509056
320.346493	16698.004422	28.514074
320.763890	16723.858262	28.519092
321.085119	16737.636198	28.524109
321.763821	16750.337361	28.529127
321.562669	16756.182992	28.534144
321.860482	16783.868858	28.539162
322.307709	16798.433405	28.544180
322.534814	16818.611029	28.549197
322.925536	16836.199971	28.554215
323.002602	16858.121528	28.559232
323.564691	16876.790418	28.564250
323.808156	16911.630798	28.569268
323.936810	16915.793509	28.574285
324.496325	16937.752649	28.579303
324.413425	16969.058178	28.584320
324.788841	16983.958934	28.589338
324.810107	17004.750480	28.594356
324.969410	17038.290259	28.599373
325.623370	17058.925531	28.604391
325.423723	17092.067540	28.609408
326.002203	17121.667255	28.614426
326.347190	17156.174893	28.619444
326.659835	17180.515354	28.624461
327.703232	17206.539707	28.629479
327.678411	17227.509757	28.634496
328.128156	17244.453955	28.639514
328.851179	17265.875317	28.644532
329.227363	17282.715538	28.649549
329.337775	17283.704992	28.654567
329.217502	17308.143391	28.659584
330.012247	17316.447151	28.664602
330.273857	17343.541580	28.669620
330.265033	17356.299280	28.674637
330.669187	17382.543526	28.679655
331.098792	17401.047754	28.684672
331.458622	17419.253290	28.689690
331.740532	17434.086315	28.694708
331.740368	17465.159977	28.699725
332.018969	17481.925419	28.704743
332.374365	17514.866091	28.709760
332.789275	17532.836609	28.714778
332.980611	17554.845070	28.719796
332.764992	17588.747362	28.724813
333.529923	17616.367158	28.729831
333.838548	17655.455654	28.734848
334.232989	17687.186940	28.739866
334.358862	17719.620537	28.744884
334.610506	17749.500313	28.749901
334.973759	17774.245843	28.754919
334.926150	17816.796230	28.759936
335.347295	17853.689342	28.764954
336.306506	17888.405048	28.769972
336.044821	17929.220957	28.774989
336.334317	17956.002166	28.780007
337.050260	17996.236060	28.785024
337.210014	18040.831197	28.790042
337.808172	18070.905581	28.795060
338.258457	18102.498497	28.800077
339.030924	18126.148644	28.805095
338.576617	18160.449280	28.810112
339.274267	18189.584002	28.815130
339.783217	18211.821126	28.820148
339.594794	18242.105062	28.825165
340.542651	18279.277847	28.830183
341.097829	18306.071255	28.835200
341.474396	18334.097937	28.840218
342.143114	18361.475727	28.845236
342.322475	18381.922647	28.850253
342.239386	18403.637056	28.855271
342.533528	18429.565159	28.860288
343.016142	18450.420550	28.865306
343.556399	18483.192861	28.870324
343.426954	18506.715270	28.875341
343.640097	18531.463881	28.880359
344.703780	18550.389316	28.885376
345.764737	18553.114458	28.890394
346.448156	18576.129454	28.895412
346.695490	18585.452688	28.900429
347.305844	18586.019622	28.905447
347.011355	18596.981650	28.910464
347.323101	18614.132027	28.915482
347.882406	18617.453297	28.920500
348.007655	18627.429510	28.925517
348.164029	18629.084202	28.930535
348.376595	18639.305968	28.935552
348.209471	18649.015781	28.940570
348.752984	18668.873520	28.945588
348.848802	18690.151526	28.950605
349.250099	18707.869263	28.955623
349.151058	18726.007330	28.960640
349.568870	18755.693648	28.965658
350.039761	18782.637934	28.970676
350.326871	18806.301507	28.975693
350.655052	18835.553415	28.980711
351.234253	18864.236993	28.985728
351.580087	18890.787195	28.990746
351.920094	18914.456283	28.995764
352.120660	18944.718960	29.000781
352.715663	18958.101082	29.005799
353.315099	18992.515942	29.010816
353.482468	19009.579127	29.015834
354.060002	19023.547205	29.020852
353.956355	19067.769508	29.025869
354.766573	19078.138067	29.030887
354.820405	19097.688536	29.035904
355.227494	19125.155435	29.040922
355.506905	19158.035311	29.045940
355.664182	19186.079182	29.050957
356.015758	19202.100141	29.055975
356.207090	19232.800712	29.060992
356.599626	19263.828367	29.066010
357.779464	19299.281826	29.071028
357.564596	19327.059243	29.076045
357.953819	19342.766836	29.081063
358.052017	19383.263413	29.086080
358.270671	19409.563873	29.091098
358.781652	19435.003534	29.096116
359.156048	19474.416459	29.101133
359.842243	19495.183321	29.106151
360.059062	19534.135631	29.111168
360.161958	19568.131625	29.116186
360.538199	19587.492727	29.121204
360.808767	19624.541996	29.126221
361.342768	19659.511337	29.131239
361.631624	19690.433512	29.136256
361.859725	19724.011418	29.141274
362.200463	19759.561849	29.146292
362.523991	19795.911265	29.151309
363.007637	19821.484668	29.156327
363.503680	19858.488320	29.161344
363.472523	19903.234171	29.166362
363.970489	19924.997479	29.171380
364.173618	19959.423288	29.176397
365.000775	19997.249422	29.181415
365.386560	20021.902399	29.186432
365.370865	20065.417337	29.191450
365.931875	20092.787773	29.196468
365.993689	20126.148517	29.201485
366.484881	20144.624934	29.206503
367.056837	20179.466141	29.211520
367.279722	20208.629114	29.216538
367.989959	20238.047992	29.221556
368.181292	20265.077581	29.226573
368.513633	20302.278473	29.231591
369.043633	20327.946120	29.236608
369.240193	20358.157433	29.241626
369.737977	20380.846356	29.246644
369.857572	20415.453434	29.251661
370.403090	20434.880750	29.256679
370.856690	20465.945157	29.261696
371.360701	20494.008170	29.266714
372.013943	20503.760864	29.271732
372.333424	20536.417130	29.276749
372.763859	20559.428122	29.281767
373.146101	20583.318635	29.286784
373.587478	20600.855332	29.291802
373.947459	20623.948525	29.296820
374.181677	20657.542417	29.301837
374.457406	20670.170843	29.306855
374.567554	20695.051514	29.311872
374.759546	20737.746882	29.316890
375.092169	20765.917236	29.321908
375.543939	20796.081633	29.326925
375.739993	20835.090882	29.331943
376.379690	20865.400301	29.336960
376.653512	20896.958079	29.341978
377.313604	20937.070241	29.346996
377.473990	20967.231784	29.352013
377.949820	20996.103497	29.357031
378.518722	21027.633416	29.362048
378.518885	21059.455647	29.367066
378.779790	21085.309965	29.372084
379.340088	21126.182761	29.377101
379.861799	21159.544469	29.382119
380.210988	21186.067706	29.387136
380.899174	21216.940277	29.392154
381.368644	21234.501559	29.397172
381.968406	21267.396629	29.402189
382.432954	21291.804353	29.407207
383.139649	21308.217433	29.412224
383.528096	21343.722499	29.417242
383.625294	21350.620368	29.422260
383.777325	21376.188509	29.427277
384.127273	21398.494497	29.432295
384.649623	21430.917884	29.437312
384.458806	21452.407553	29.442330
384.782444	21472.647283	29.447348
385.302138	21509.098959	29.452365
385.364337	21543.128546	29.457383
385.776648	21566.536907	29.462400
386.428630	21602.976384	29.467418
386.901870	21622.256021	29.472436
386.876066	21653.957573	29.477453
387.533638	21675.152469	29.482471
387.859728	21701.555815	29.487488
388.008304	21742.849451	29.492506
388.762179	21766.760513	29.497524
388.842731	21801.969918	29.502541
389.254931	21828.646442	29.507559
390.072165	21860.173112	29.512576
390.074846	21895.584159	29.517594
390.258124	21919.454849	29.522612
390.733489	21957.737934	29.527629
391.070577	21999.558252	29.532647
391.737950	22020.737088	29.537664
391.980470	22053.522966	29.542682
392.824122	22070.950733	29.547700
392.871268	22106.211032	29.552717
393.070367	22125.851593	29.557735
393.674813	22155.434269	29.562752
393.939816	22202.264047	29.567770
394.737081	22226.474491	29.572788
395.533786	22252.773049	29.577805
395.713535	22284.470675	29.582823
396.241182	22302.775274	29.587840
396.798495	22324.854198	29.592858
396.611550	22344.152493	29.597876
397.145559	22378.109480	29.602893
397.218673	22413.497859	29.607911
397.836936	22431.426645	29.612928
398.125409	22467.996144	29.617946
398.613494	22491.985318	29.622964
398.984290	22520.387440	29.627981
399.213346	22551.393287	29.632999
399.984011	22580.185477	29.638016
400.136786	22615.758523	29.643034
400.663279	22637.072482	29.648052
401.254425	22680.078111	29.653069
401.308590	22705.943609	29.658087
401.832363	22727.069876	29.663104
402.373281	22761.692147	29.668122
402.724057	22786.523590	29.673140
402.859913	22820.600107	29.678157
403.289864	22859.306916	29.683175
403.630792	22889.194459	29.688192
404.156449	22913.031781	29.693210
404.395942	22955.375849	29.698228
404.856535	22976.033621	29.703245
404.900780	23028.034187	29.708263
405.732885	23056.918277	29.713280
406.303885	23089.779196	29.718298
406.822712	23125.831456	29.723316
407.146781	23157.225057	29.728333
407.273443	23198.455085	29.733351
408.138207	23218.587196	29.738368
408.176750	23247.158563	29.743386
408.941931	23269.538871	29.748404
409.258475	23298.155826	29.753421
409.326072	23328.349258	29.758439
409.787513	23347.749460	29.763456
409.920233	23374.871690	29.768474
410.414996	23394.364312	29.773492
411.290524	23425.973042	29.778509
411.516951	23453.597193	29.783527
411.985198	23481.200189	29.788544
412.375642	23518.752281	29.793562
412.726322	23537.603231	29.798580
412.779654	23577.693542	29.803597
413.369163	23607.230902	29.808615
413.647922	23638.219924	29.813632
414.059335	23668.680594	29.818650
414.160350	23709.924699	29.823668
414.970812	23738.385763	29.828685
415.246575	23777.004374	29.833703
415.777466	23797.917470	29.838720
415.657238	23853.022904	29.843738
416.327952	23876.737736	29.848756
417.014960	23918.945319	29.853773
417.021212	23956.971632	29.858791
417.462403	23992.293057	29.863808
418.110938	24039.140393	29.868826
418.616701	24072.239026	29.873844
418.940605	24106.397036	29.878861
420.196638	24136.459349	29.883879
420.776743	24159.324917	29.888896
421.472958	24183.302394	29.893914
421.816583	24198.694806	29.898932
422.118881	24230.442166	29.903949
422.383953	24255.058759	29.908967
423.036573	24275.399320	29.913984
423.403035	24301.226313	29.919002
423.601043	24333.081871	29.924020
424.003869	24355.011792	29.929037
424.096554	24384.835358	29.934055
424.611342	24407.996850	29.939072
424.856029	24446.236046	29.944090
425.494441	24464.683044	29.949108
425.488871	24499.033821	29.954125
425.683797	24535.564687	29.959143
426.509892	24559.574028	29.964160
426.864423	24605.960999	29.969178
427.143978	24646.894702	29.974196
428.255435	24658.638499	29.979213
428.400960	24692.917566	29.984231
429.048030	24727.264887	29.989248
429.518789	24762.266635	29.994266
429.811920	24786.341545	29.999284
430.485111	24813.817305	30.004301
430.635496	24852.457707	30.009319
430.950995	24872.255633	30.014336
431.553508	24901.959541	30.019354
431.529938	24937.675366	30.024372
432.124537	24952.848123	30.029389
432.240498	24993.681163	30.034407
432.603353	25018.228209	30.039424
432.901364	25059.595658	30.044442
433.237098	25090.075829	30.049460
433.546007	25123.570381	30.054477
433.972779	25160.470644	30.059495
434.363833	25198.437019	30.064512
435.227545	25231.544834	30.069530
435.590849	25276.400138	30.074548
436.089155	25303.013636	30.079565
436.643344	25339.345719	30.084583
437.124075	25382.107610	30.089600
437.551224	25411.051841	30.094618
437.638134	25448.407898	30.099636
438.396018	25477.177446	30.104653
438.845716	25522.551427	30.109671
439.322049	25554.098009	30.114688
439.515607	25587.800979	30.119706
439.966983	25633.106468	30.124724
440.473860	25668.352596	30.129741
440.891884	25703.119800	30.134759
441.464880	25733.198644	30.139776
441.968914	25778.931017	30.144794
442.295425	25809.233620	30.149812
442.944876	25835.764836	30.154829
443.157927	25894.232204	30.159847
443.572072	25918.850451	30.164864
444.013875	25958.324698	30.169882
444.297303	25994.684863	30.174900
444.930696	26048.029671	30.179917
445.300360	26083.292270	30.184935
446.116076	26108.414051	30.189952
446.611001	26155.020267	30.194970
446.736353	26194.605388	30.199988
447.091967	26220.315883	30.205005
448.094241	26258.932659	30.210023
448.523713	26290.585059	30.215040
448.919623	26319.413006	30.220058
449.391979	26357.044586	30.225076
449.761534	26384.473733	30.230093
450.113980	26425.487021	30.235111
450.764805	26457.399129	30.240128
450.861097	26500.919328	30.245146
451.188578	26534.722695	30.250164
451.898498	26573.972958	30.255181
451.951967	26615.743417	30.260199
452.441020	26647.836881	30.265216
453.263756	26695.092034	30.270234
453.247251	26733.060005	30.275252
453.780586	26777.659994	30.280269
454.094990	26825.737883	30.285287
454.965788	26853.247901	30.290304
455.435381	26892.633349	30.295322
455.678885	26932.146306	30.300340
456.539075	26952.299639	30.305357
456.720170	26989.504813	30.310375
457.243061	27020.951527	30.315392
457.762291	27057.332460	30.320410
458.083401	27077.371722	30.325428
458.575692	27116.936885	30.330445
458.749845	27149.857565	30.335463
459.096282	27178.419181	30.340480
459.778140	27223.234675	30.345498
459.963906	27271.263477	30.350516
460.587588	27304.273577	30.355533
460.771788	27348.506895	30.360551
461.262906	27389.866114	30.365568
461.846755	27430.173817	30.370586
462.230581	27477.377496	30.375604
462.749653	27519.581927	30.380621
463.190829	27565.046536	30.385639
463.693007	27599.535759	30.390656
463.971053	27644.122087	30.395674
464.525989	27698.022983	30.400692
464.990064	27727.929878	30.405709
465.710843	27762.568987	30.410727
466.420407	27810.504907	30.415744
466.971982	27838.045409	30.420762
467.815942	27882.288529	30.425780
468.142792	27906.012123	30.430797
468.684716	27947.567952	30.435815
469.089862	27987.183797	30.440832
469.851405	28010.077173	30.445850
469.869918	28052.378501	30.450868
470.092442	28089.784459	30.455885
470.755382	28113.371293	30.460903
471.616254	28149.307876	30.465920
472.133820	28188.299610	30.470938
472.370611	28214.587694	30.475956
473.068691	28243.572645	30.480973
473.182252	28280.088721	30.485991
473.903598	28319.494267	30.491008
474.601156	28341.260551	30.496026
474.824269	28382.108731	30.501044
474.686520	28414.334719	30.506061
475.564413	28454.758867	30.511079
475.697829	28498.839525	30.516096
475.809585	28535.625934	30.521114
476.285833	28584.795820	30.526132
476.732187	28633.595560	30.531149
477.533770	28676.115719	30.536167
477.807440	28720.593816	30.541184
478.582673	28771.576172	30.546202
478.736072	28810.685727	30.551220
479.446503	28856.186703	30.556237
479.558442	28905.045262	30.561255
480.132055	28949.884357	30.566272
480.892302	28986.568472	30.571290
481.371846	29032.009017	30.576308
482.075264	29067.175311	30.581325
482.224903	29105.818126	30.586343
482.395366	29149.937194	30.591360
482.951345	29183.253457	30.596378
483.485224	29224.139341	30.601396
484.257973	29262.892858	30.606413
484.953491	29308.203635	30.611431
485.297496	29334.389773	30.616448
485.737726	29368.451364	30.621466
486.070217	29415.790203	30.626484
486.762114	29439.448426	30.631501
487.854674	29470.728771	30.636519
488.251232	29504.937865	30.641536
488.985053	29529.892857	30.646554
489.582718	29561.808533	30.651572
489.800685	29591.981859	30.656589
490.109118	29619.010958	30.661607
490.587117	29657.588586	30.666624
491.001225	29694.844787	30.671642
491.138794	29722.785399	30.676660
491.715786	29766.907562	30.681677
492.088815	29809.629767	30.686695
492.627531	29843.862629	30.691712
493.301865	29884.926370	30.696730
493.649119	29924.124334	30.701748
493.937453	29964.956635	30.706765
494.629892	30002.670365	30.711783
494.777782	30050.776447	30.716800
495.153043	30088.897083	30.721818
495.710537	30137.284889	30.726836
496.036630	30182.633309	30.731853
496.920399	30236.598979	30.736871
497.375027	30289.643444	30.741888
498.080427	30325.645862	30.746906
498.612852	30362.660939	30.751924
498.915867	30410.894666	30.756941
499.578146	30449.290355	30.761959
499.804312	30507.186743	30.766976
500.886281	30549.745933	30.771994
500.888042	30595.842206	30.777012
501.577638	30638.538209	30.782029
502.234794	30687.186000	30.787047
502.268554	30734.793743	30.792064
503.011316	30773.483130	30.797082
503.251474	30820.066888	30.802100
504.146467	30867.596134	30.807117
504.694006	30907.675525	30.812135
504.702066	30957.808177	30.817152
505.343090	31006.234103	30.822170
505.961284	31050.988334	30.827188
506.705996	31101.569895	30.832205
507.360301	31139.147319	30.837223
507.604198	31186.869475	30.842240
508.699684	31217.690911	30.847258
509.093173	31251.097173	30.852276
509.326763	31276.788619	30.857293
510.248610	31309.002814	30.862311
510.640764	31343.821688	30.867328
511.056486	31370.710498	30.872346
511.485852	31411.495564	30.877364
512.013729	31438.204276	30.882381
512.975619	31459.776592	30.887399
513.250495	31503.787645	30.892416
513.945089	31527.286126	30.897434
514.363528	31548.839530	30.902452
514.717353	31567.061809	30.907469
515.320017	31598.378576	30.912487
515.381987	31631.031429	30.917504
516.048093	31669.315885	30.922522
516.782701	31714.926577	30.927540
517.073632	31762.403333	30.932557
517.714728	31799.087532	30.937575
517.599805	31841.117281	30.942592
518.316746	31877.089748	30.947610
518.872533	31914.642086	30.952628
519.205216	31968.619285	30.957645
519.716343	32015.201091	30.962663
520.175977	32065.728582	30.967680
520.887320	32107.118272	30.972698
520.823604	32157.363732	30.977716
521.403215	32204.518361	30.982733
521.836398	32249.451915	30.987751
522.560818	32307.464412	30.992768
522.899524	32347.394586	30.997786
523.976820	32404.121753	31.002804
524.126980	32447.617696	31.007821
525.198810	32499.678825	31.012839
525.093276	32550.316742	31.017856
525.814000	32602.229211	31.022874
526.325584	32653.714892	31.027892
526.969635	32703.280236	31.032909
527.557698	32746.314719	31.037927
528.195937	32804.079453	31.042944
528.904506	32848.507346	31.047962
529.409884	32897.687108	31.052980
529.595078	32945.524583	31.057997
530.733086	32977.644568	31.063015
530.921992	33039.616304	31.068032
531.588214	33073.528213	31.073050
531.909112	33122.575670	31.078068
532.163536	33173.564837	31.083085
533.251500	33217.953780	31.088103
533.372583	33269.716383	31.093120
533.778371	33317.327481	31.098138
534.734709	33364.846290	31.103156
534.950809	33424.521578	31.108173
535.262672	33460.108041	31.113191
535.732858	33519.432659	31.118208
536.533956	33568.196866	31.123226
536.991411	33614.098135	31.128244
537.390890	33662.642850	31.133261
537.965793	33704.083497	31.138279
538.786585	33755.135564	31.143296
538.944929	33799.226459	31.148314
539.898316	33848.807437	31.153332
539.834939	33901.619725	31.158349
540.288438	33947.976542	31.163367
541.110375	33994.229085	31.168384
541.408111	34054.331865	31.173402
542.043938	34102.275870	31.178420
542.678044	34165.799846	31.183437
543.682946	34208.372899	31.188455
543.712964	34253.656707	31.193472
544.244674	34306.252527	31.198490
544.561663	34355.100887	31.203508
545.235461	34414.073098	31.208525
546.068731	34467.285067	31.213543
546.361320	34524.090895	31.218560
546.846018	34578.782263	31.223578
547.415008	34639.744094	31.228596
548.061956	34693.732123	31.233613
549.017997	34740.014251	31.238631
549.220017	34805.012535	31.243648
549.717025	34854.035468	31.248666
550.632539	34910.492731	31.253684
550.872317	34956.567950	31.258701
551.923534	35013.658185	31.263719
552.312106	35071.396474	31.268736
553.289373	35105.326051	31.273754
553.556842	35160.701864	31.278772
554.075699	35208.755968	31.283789
554.770892	35252.063649	31.288807
555.340819	35299.930160	31.293824
555.994550	35351.114629	31.298842
557.209351	35398.762045	31.303860
557.106420	35441.106394	31.308877
557.781791	35491.624132	31.313895
558.137766	35537.649336	31.318912
558.797771	35578.731104	31.323930
559.071215	35613.959375	31.328948
559.798304	35667.026549	31.333965
560.447754	35712.999185	31.338983
561.057232	35758.407603	31.344000
561.713931	35819.342425	31.349018
562.334922	35857.195997	31.354036
562.621915	35902.165860	31.359053
563.310247	35949.764697	31.364071
563.866893	36002.994092	31.369088
564.562044	36052.004743	31.374106
565.251668	36097.663028	31.379124
565.141174	36153.928453	31.384141
566.164356	36191.925255	31.389159
566.804215	36229.631618	31.394176
567.496953	36272.442552	31.399194
568.110935	36310.460656	31.404212
568.147632	36351.198996	31.409229
568.905935	36391.634883	31.414247
569.388686	36442.619737	31.419264
569.848415	36472.292531	31.424282
570.450047	36534.599343	31.429300
570.667520	36573.773797	31.434317
571.372556	36620.834249	31.439335
572.059779	36678.215178	31.444352
572.600647	36727.003267	31.449370
573.177412	36768.339282	31.454388
573.134017	36828.536310	31.459405
573.744818	36867.095395	31.464423
574.604819	36930.116162	31.469440
574.927934	36985.244747	31.474458
575.610458	37029.396251	31.479476
576.032435	37095.924543	31.484493
576.731139	37144.595679	31.489511
577.545606	37204.383070	31.494528
577.876058	37253.349676	31.499546
578.767429	37310.879989	31.504564
579.323943	37368.739756	31.509581
579.760088	37413.820768	31.514599
580.576802	37475.792502	31.519616
580.897055	37530.959590	31.524634
581.828173	37575.856561	31.529652
581.913086	37638.043201	31.534669
582.749756	37700.061459	31.539687
583.408424	37756.953939	31.544704
583.290680	37820.483795	31.549722
584.445117	37877.229919	31.554740
585.119701	37921.139051	31.559757
585.990098	37975.322795	31.564775
586.265400	38036.857758	31.569792
587.073126	38090.279238	31.574810
587.538432	38140.630260	31.579828
588.185037	38202.250173	31.584845
589.342203	38247.518161	31.589863
590.134805	38297.325566	31.594880
589.928062	38355.493179	31.599898
591.014409	38399.380546	31.604916
591.514133	38460.606941	31.609933
592.171453	38495.524657	31.614951
592.649546	38547.530498	31.619968
593.356595	38594.816891	31.624986
594.450240	38635.721954	31.630004
595.225868	38682.266026	31.635021
595.891990	38719.934360	31.640039
596.200182	38766.262973	31.645056
596.587843	38802.129370	31.650074
597.402173	38853.674200	31.655092
598.005511	38896.925478	31.660109
598.522458	38936.421961	31.665127
598.937584	38982.571718	31.670144
599.425784	39022.393080	31.675162
600.447488	39045.134194	31.680180
600.314459	39094.746031	31.685197
600.878214	39135.605815	31.690215
601.849558	39182.164243	31.695232
602.432065	39216.242273	31.700250
603.069338	39256.292742	31.705268
603.553830	39296.815472	31.710285
604.180860	39333.247237	31.715303
604.399253	39384.713556	31.720320
604.907425	39431.986651	31.725338
605.575113	39477.860995	31.730356
605.994666	39535.871396	31.735373
606.668827	39579.360707	31.740391
607.504405	39630.313171	31.745408
607.527797	39694.947157	31.750426
608.231931	39746.777170	31.755444
608.962689	39807.074352	31.760461
609.643743	39866.088156	31.765479
610.451349	39919.919114	31.770496
610.693550	39981.660349	31.775514
611.591697	40032.985674	31.780532
611.945631	40091.610809	31.785549
612.428565	40148.137169	31.790567
613.195603	40201.688471	31.795584
613.590633	40270.330859	31.800602
614.267572	40329.441539	31.805620
614.800478	40386.869067	31.810637
615.479918	40449.613128	31.815655
616.106062	40520.219332	31.820672
616.816935	40581.681507	31.825690
618.074519	40628.403317	31.830708
618.359246	40683.190460	31.835725
619.206360	40737.787285	31.840743
619.962547	40799.192562	31.845760
620.141813	40854.388148	31.850778
621.047410	40913.678907	31.855796
621.797187	40973.076693	31.860813
622.283489	41021.471058	31.865831
622.651318	41078.242760	31.870848
623.075704	41145.701197	31.875866
623.639636	41201.896418	31.880884
624.344011	41259.678060	31.885901
624.626433	41325.393502	31.890919
625.617500	41383.120441	31.895936
626.010313	41451.480884	31.900954
626.632168	41518.164955	31.905972
626.999145	41584.281117	31.910989
627.711592	41658.281624	31.916007
628.143562	41731.576414	31.921024
628.735424	41806.653422	31.926042
629.381807	41877.590026	31.931060
630.358213	41941.525559	31.936077
630.826418	42010.595384	31.941095
631.549362	42077.375922	31.946112
631.836462	42152.714308	31.951130
632.383002	42218.022043	31.956148
633.185231	42287.639101	31.961165
633.867601	42342.393439	31.966183
634.681952	42408.485679	31.971200
634.988047	42476.062795	31.976218
635.629832	42533.010162	31.981236
636.466188	42596.673921	31.986253
636.786516	42667.407039	31.991271
637.845644	42722.253995	31.996288
638.095955	42800.837469	32.001306
638.923923	42859.935958	32.006324
639.444855	42946.792038	32.011341
640.006701	43018.620572	32.016359
640.975576	43086.678100	32.021376
641.637778	43163.405897	32.026394
642.492461	43214.810750	32.031412
643.440180	43267.992690	32.036429
643.838954	43329.265175	32.041447
644.706561	43387.062655	32.046464
645.346458	43458.688160	32.051482
646.064854	43515.188084	32.056500
647.094412	43579.118067	32.061517
647.500136	43628.024688	32.066535
648.255298	43686.923087	32.071552
648.485533	43750.236511	32.076570
649.254374	43805.101585	32.081588
649.908018	43880.650950	32.086605
650.133965	43939.344256	32.091623
651.388047	43999.908769	32.096640
651.581390	44067.222972	32.101658
651.963055	44143.955614	32.106676
652.831241	44212.084072	32.111693
653.524172	44279.426799	32.116711
654.362957	44348.245036	32.121728
654.746489	44420.309666	32.126746
655.543079	44495.602336	32.131764
656.036958	44551.261219	32.136781
656.751562	44625.343474	32.141799
657.409076	44696.327708	32.146816
657.867785	44771.296804	32.151834
658.960589	44832.861570	32.156852
659.359309	44918.396721	32.161869
659.710007	44985.853461	32.166887
660.609973	45047.317191	32.171904
661.292381	45130.054055	32.176922
661.918931	45197.934602	32.181940
662.682613	45283.609025	32.186957
663.097054	45342.254951	32.191975
663.770686	45420.388486	32.196992
664.750524	45496.221017	32.202010
665.653514	45561.194315	32.207028
666.674556	45624.675711	32.212045
667.245560	45685.294918	32.217063
668.306476	45739.059522	32.222080
668.699773	45808.140596	32.227098
669.567701	45863.860833	32.232116
670.156504	45912.981332	32.237133
670.580252	45965.598724	32.242151
671.295189	46008.405230	32.247168
672.078871	46065.720171	32.252186
672.751176	46113.802565	32.257204
673.309036	46173.983856	32.262221
673.878282	46231.749947	32.267239
674.249252	46286.481107	32.272256
674.599090	46350.983820	32.277274
675.394389	46420.394519	32.282292
676.061073	46489.381106	32.287309
676.411968	46557.235092	32.292327
677.545130	46628.971749	32.297344
677.991304	46695.858259	32.302362
678.652531	46766.336013	32.307380
679.438764	46835.926483	32.312397
679.726551	46912.884981	32.317415
681.001680	46987.127767	32.322432
681.407437	47062.118244	32.327450
681.862275	47130.115644	32.332468
683.101930	47196.950282	32.337485
683.213220	47263.822857	32.342503
683.999170	47335.122312	32.347520
684.393914	47401.473836	32.352538
685.789580	47465.605860	32.357556
686.550992	47535.786767	32.362573
687.376393	47609.154054	32.367591
688.250477	47663.162552	32.372608
688.714801	47735.369917	32.377626
689.206491	47805.058442	32.382644
690.268004	47866.234970	32.387661
690.891052	47934.704070	32.392679
691.922414	47997.697014	32.397696
692.646129	48059.530668	32.402714
693.397002	48121.019435	32.407732
694.315598	48179.970035	32.412749
695.070660	48235.744157	32.417767
696.859943	48266.795387	32.422784
698.004211	48303.439759	32.427802
698.832216	48335.268936	32.432820
699.943657	48360.480335	32.437837
700.362233	48387.711110	32.442855
701.269164	48398.885164	32.447872
701.803946	48441.685258	32.452890
702.350531	48475.260267	32.457908
702.753183	48504.996011	32.462925
703.484172	48533.647700	32.467943
704.148362	48557.807259	32.472960
704.453064	48598.722703	32.477978
704.921899	48629.571458	32.482996
705.805397	48668.261822	32.488013
706.235803	48713.452097	32.493031
706.577703	48748.707369	32.498048
706.934271	48796.358258	32.503066
707.424139	48853.463990	32.508084
707.922832	48891.020178	32.513101
708.734808	48960.214174	32.518119
709.470667	49001.320650	32.523136
709.994365	49049.223293	32.528154
710.082359	49118.675175	32.533172
711.002503	49185.972127	32.538189
711.268461	49242.341649	32.543207
712.118988	49309.416641	32.548224
712.469732	49384.463577	32.553242
712.891802	49459.013511	32.558260
714.139505	49533.277678	32.563277
714.368727	49622.444243	32.568295
715.273465	49693.967800	32.573312
716.032104	49764.915331	32.578330
716.525022	49850.841221	32.583348
717.204033	49916.326949	32.588365
717.800783	50003.827505	32.593383
718.082605	50090.592860	32.598400
718.967717	50178.909871	32.603418
719.458284	50269.035261	32.608436
720.612215	50362.444773	32.613453
721.024576	50451.131882	32.618471
722.137164	50532.395983	32.623488
722.859748	50625.269631	32.628506
723.373812	50718.151713	32.633524
724.785240	50793.673167	32.638541
725.406476	50887.413230	32.643559
726.091793	50970.006528	32.648576
726.837708	51049.207456	32.653594
727.610034	51132.295745	32.658612
728.862602	51195.703470	32.663629
729.677333	51289.376955	32.668647
730.707136	51345.322209	32.673664
731.691263	51412.364890	32.678682
732.448270	51479.137852	32.683700
733.369628	51541.756894	32.688717
733.847910	51613.488570	32.693735
734.783616	51669.222585	32.698752
735.522886	51742.494374	32.703770
736.325323	51814.670736	32.708788
737.407246	51865.928951	32.713805
737.712641	51936.840469	32.718823
738.158335	51994.903760	32.723840
738.898707	52058.497073	32.728858
739.599411	52135.825822	32.733876
740.312679	52199.689059	32.738893
740.775975	52278.710003	32.743911
741.578450	52344.696227	32.748928
742.368937	52423.908737	32.753946
743.092877	52508.109411	32.758964
743.933451	52567.099547	32.763981
744.761880	52631.514085	32.768999
745.538768	52702.915344	32.774016
746.273451	52771.486198	32.779034
746.880015	52840.630043	32.784052
747.891495	52891.157530	32.789069
748.499553	52958.666676	32.794087
749.136795	53011.646490	32.799104
749.909706	53079.839993	32.804122
750.593489	53144.560292	32.809140
751.133080	53203.897111	32.814157
751.911094	53277.983278	32.819175
752.512303	53354.045321	32.824192
753.518715	53429.636013	32.829210
753.854378	53493.712281	32.834228
754.508090	53580.529920	32.839245
755.049150	53652.509041	32.844263
755.500354	53735.717252	32.849280
756.350861	53808.850298	32.854298
756.800854	53906.269421	32.859316
757.984237	53978.466371	32.864333
758.894459	54066.283946	32.869351
759.310879	54153.359888	32.874368
760.265133	54232.611047	32.879386
761.123694	54311.527420	32.884404
762.311266	54390.426480	32.889421
762.959184	54482.381750	32.894439
763.939811	54559.442696	32.899456
764.690049	54642.957817	32.904474
765.473708	54727.175060	32.909492
766.096428	54789.303651	32.914509
766.681034	54871.457312	32.919527
767.453011	54959.787308	32.924544
768.429226	55047.299232	32.929562
769.279940	55130.150331	32.934580
770.119331	55212.230241	32.939597
770.601226	55279.332470	32.944615
771.630078	55361.348167	32.949632
772.496358	55439.204403	32.954650
772.782310	55513.741010	32.959668
773.538887	55595.157139	32.964685
774.384918	55685.776906	32.969703
774.722170	55783.413384	32.974720
776.147460	55867.259101	32.979738
776.512955	55970.356351	32.984756
777.356912	56051.160815	32.989773
778.484920	56143.846664	32.994791
778.966653	56230.420163	32.999808
779.994345	56324.196195	33.004826
780.493649	56415.701838	33.009844
781.328842	56496.219228	33.014861
782.414539	56580.696807	33.019879
783.376333	56663.022583	33.024896
783.957344	56747.660188	33.029914
784.771678	56827.651994	33.034932
785.619622	56900.027530	33.039949
786.220341	56991.317846	33.044967
787.259783	57072.951201	33.049984
788.675667	57145.903406	33.055002
789.666369	57207.391260	33.060020
790.261182	57275.493021	33.065037
791.424505	57347.633851	33.070055
791.789114	57415.652809	33.075072
792.460815	57476.147378	33.080090
793.051256	57541.614729	33.085108
793.675965	57609.602467	33.090125
794.446740	57692.591491	33.095143
794.856205	57772.462418	33.100160
795.441881	57845.786323	33.105178
796.288824	57929.070517	33.110196
797.286121	58015.298809	33.115213
798.430822	58074.924459	33.120231
798.835081	58157.756069	33.125248
800.288341	58220.673293	33.130266
801.179674	58308.511004	33.135284
802.178880	58370.872745	33.140301
802.524332	58452.502689	33.145319
803.202946	58524.883124	33.150336
804.247770	58601.050996	33.155354
804.833796	58682.574198	33.160372
805.970672	58754.159584	33.165389
806.714313	58828.886129	33.170407
807.136028	58904.491413	33.175424
808.280022	58983.265570	33.180442
809.014709	59066.629567	33.185460
809.930044	59147.275184	33.190477
810.401875	59226.157360	33.195495
811.272430	59314.653533	33.200512
812.171599	59390.740476	33.205530
812.798572	59482.670332	33.210548
813.592389	59561.246929	33.215565
814.499346	59640.408904	33.220583
814.967883	59729.877198	33.225600
815.741123	59816.762037	33.230618
816.609581	59916.536429	33.235636
817.501645	60004.685133	33.240653
818.506009	60091.603924	33.245671
819.371290	60178.280031	33.250688
820.233096	60255.380511	33.255706
820.923786	60343.644958	33.260724
821.901951	60428.845503	33.265741
822.981721	60507.989958	33.270759
823.517494	60608.869283	33.275776
824.602682	60689.109300	33.280794
825.420294	60773.206568	33.285812
826.031085	60844.590057	33.290829
826.901101	60932.216164	33.295847
827.624922	61023.554013	33.300864
828.723597	61103.212657	33.305882
829.234557	61190.369796	33.310900
830.368433	61279.212254	33.315917
831.093529	61365.556186	33.320935
831.657900	61451.626117	33.325952
832.509176	61541.717863	33.330970
832.952980	61629.168753	33.335988
833.866285	61695.215028	33.341005
834.836803	61779.781901	33.346023
835.714092	61868.241684	33.351040
836.908157	61941.475343	33.356058
837.108742	62030.507781	33.361076
838.074664	62120.220899	33.366093
838.933359	62207.804214	33.371111
839.677337	62287.893783	33.376128
840.726909	62367.852948	33.381146
841.295456	62457.567758	33.386164
842.263936	62534.790066	33.391181
842.877796	62638.784605	33.396199
843.555888	62737.669520	33.401216
844.503395	62815.136309	33.406234
845.506312	62913.244126	33.411252
846.191569	63010.578791	33.416269
847.133836	63103.442464	33.421287
847.781780	63213.387437	33.426304
848.482799	63306.044175	33.431322
849.287598	63404.230272	33.436340
850.032653	63511.253003	33.441357
850.876501	63617.126883	33.446375
851.754346	63711.728059	33.451392
853.435690	63802.557429	33.456410
854.481215	63904.917479	33.461428
855.030888	63994.241468	33.466445
857.079231	64058.242590	33.471463
857.979319	64138.394067	33.476480
859.073738	64213.149305	33.481498
860.261356	64292.153483	33.486516
861.426218	64349.332515	33.491533
862.641378	64406.446867	33.496551
863.251981	64475.923911	33.501568
864.129274	64538.069696	33.506586
864.798621	64610.775010	33.511604
865.209251	64667.594989	33.516621
866.444017	64724.767180	33.521639
867.387319	64802.678561	33.526656
867.880451	64857.063620	33.531674
868.971584	64928.878718	33.536692
869.849301	64985.492659	33.541709
871.336788	65058.438983	33.546727
871.314312	65130.874225	33.551744
872.371160	65184.737817	33.556762
873.148738	65261.268846	33.561780
873.622929	65339.433933	33.566797
874.851144	65401.084511	33.571815
875.262208	65475.868168	33.576832
876.217663	65561.464915	33.581850
876.994707	65637.602736	33.586868
877.704356	65715.583437	33.591885
878.879452	65801.446343	33.596903
879.696969	65881.902515	33.601920
880.627079	65940.955537	33.606938
881.409435	66012.182677	33.611956
881.619246	66098.513212	33.616973
882.487948	66165.204305	33.621991
883.284097	66251.454845	33.627008
883.996841	66329.134326	33.632026
884.188192	66414.967016	33.637044
885.058973	66510.107439	33.642061
886.234551	66597.821539	33.647079
886.551368	66699.083810	33.652096
887.302211	66793.973084	33.657114
888.144001	66895.310763	33.662132
889.000306	67002.521616	33.667149
890.390307	67096.609453	33.672167
891.028587	67204.222517	33.677184
891.772063	67307.839565	33.682202
892.502913	67416.355074	33.687220
893.733358	67528.765283	33.692237
894.922713	67635.970859	33.697255
895.948939	67732.198086	33.702272
897.062861	67823.717989	33.707290
898.321330	67908.594632	33.712308
899.010552	68021.428647	33.717325
900.009727	68108.545912	33.722343
901.196226	68199.740161	33.727360
902.234903	68301.325502	33.732378
903.078464	68394.565275	33.737396
903.814542	68496.503033	33.742413
904.643376	68583.592671	33.747431
905.283658	68695.718162	33.752448
906.021297	68786.026293	33.757466
906.781917	68887.955871	33.762484
907.531782	69004.330186	33.767501
908.543084	69099.182940	33.772519
909.787111	69211.069999	33.777536
910.694035	69316.118508	33.782554
911.873401	69404.034210	33.787572
912.779806	69504.939251	33.792589
913.796638	69597.670705	33.797607
914.672333	69706.738204	33.802624
915.714506	69803.200554	33.807642
916.694039	69887.466796	33.812660
917.201285	69995.691045	33.817677
918.241481	70092.704808	33.822695
919.361390	70196.511053	33.827712
920.200351	70293.804240	33.832730
920.862313	70395.504622	33.837748
921.594215	70502.078432	33.842765
922.607980	70597.089674	33.847783
923.177865	70712.618186	33.852800
924.498133	70819.434959	33.857818
925.493399	70927.030647	33.862836
926.175187	71037.747572	33.867853
926.998119	71151.968377	33.872871
927.931639	71258.406773	33.877888
928.938843	71364.676052	33.882906
929.641546	71467.266386	33.887924
930.466152	71572.175744	33.892941
931.855237	71664.636542	33.897959
932.418440	71771.781126	33.902976
933.268787	71861.870599	33.907994
934.436857	71972.180477	33.913012
935.083560	72079.161784	33.918029
936.018269	72178.319370	33.923047
937.127205	72284.135073	33.928064
938.007244	72391.213626	33.933082
939.025786	72490.959726	33.938100
939.845039	72602.838831	33.943117
940.916663	72703.929809	33.948135
941.484358	72818.579955	33.953152
942.575050	72925.482524	33.958170
943.551999	73035.664415	33.963188
944.658573	73153.213349	33.968205
945.484366	73260.817054	33.973223
946.244930	73371.881999	33.978240
947.175659	73494.541555	33.983258
948.324442	73600.831849	33.988276
949.190970	73732.842963	33.993293
950.403913	73831.755961	33.998311
950.914888	73947.565402	34.003328
951.882903	74064.572993	34.008346
953.135211	74181.921516	34.013364
953.847852	74300.020142	34.018381
955.350408	74407.383293	34.023399
956.355836	74528.457407	34.028416
957.266731	74642.267114	34.033434
958.752839	74750.456265	34.038452
959.434623	74863.949781	34.043469
960.526671	74976.474941	34.048487
961.369605	75092.339268	34.053504
962.219082	75198.919475	34.058522
963.397776	75307.179489	34.063540
964.161123	75424.113791	34.068557
965.395060	75526.747855	34.073575
966.363355	75634.834547	34.078592
967.399242	75747.682617	34.083610
968.488215	75848.868836	34.088628
969.218770	75961.646601	34.093645
970.192134	76067.055111	34.098663
971.245755	76174.764547	34.103680
972.024186	76291.221131	34.108698
973.628370	76382.456031	34.113716
974.484967	76496.341699	34.118733
975.376547	76600.596762	34.123751
976.804154	76702.352744	34.128768
977.689795	76797.047240	34.133786
978.635914	76893.040856	34.138804
979.598393	77005.762237	34.143821
980.500543	77095.917499	34.148839
981.771775	77182.557186	34.153856
982.851282	77292.701779	34.158874
983.950186	77375.950360	34.163892
984.570260	77467.315106	34.168909
984.992722	77547.720347	34.173927
985.901219	77643.186240	34.178944
986.866368	77741.418292	34.183962
987.608894	77834.370619	34.188980
988.262608	77946.040215	34.193997
989.596289	78036.067767	34.199015
990.968654	78135.033325	34.204032
991.982997	78231.894638	34.209050
993.116544	78321.013501	34.214068
993.801496	78428.148785	34.219085
994.811781	78528.716119	34.224103
995.641445	78629.736179	34.229120
996.797657	78739.086252	34.234138
997.853058	78850.020529	34.239156
997.983705	78950.091461	34.244173
998.873647	79061.426136	34.249191
1000.126398	79183.164951	34.254208
1000.845140	79313.516528	34.259226
1002.218143	79419.757380	34.264244
1002.890341	79556.830884	34.269261
1003.690819	79676.754552	34.274279
1004.734037	79797.563191	34.279296
1005.754622	79934.090717	34.284314
1007.113679	80052.872056	34.289332
1007.881840	80179.668680	34.294349
1008.999384	80299.450696	34.299367
1010.082268	80409.801098	34.304384
1011.273451	80544.447022	34.309402
1012.390787	80660.874486	34.314420
1013.552456	80777.687483	34.319437
1015.014525	80897.291712	34.324455
1016.029288	81014.268484	34.329472
1016.904815	81128.435990	34.334490
1017.860019	81230.333807	34.339508
1019.300280	81351.454989	34.344525
1020.490478	81451.167138	34.349543
1021.620736	81561.155783	34.354560
1022.266471	81675.906513	34.359578
1023.550052	81780.422565	34.364596
1024.105723	81891.598030	34.369613
1025.459976	82000.611405	34.374631
1026.722194	82116.473957	34.379648
1027.518234	82213.616224	34.384666
1029.794600	82315.587334	34.389684
1031.369039	82399.083977	34.394701
1032.312292	82483.313565	34.399719
1033.689947	82569.396284	34.404736
1034.427760	82637.076489	34.409754
1035.470754	82719.577885	34.414772
1036.318750	82803.160095	34.419789
1036.974764	82902.458380	34.424807
1038.074938	82984.502851	34.429824
1038.761113	83084.600113	34.434842
1039.784858	83157.275294	34.439860
1040.567134	83240.692677	34.444877
1041.452510	83330.289805	34.449895
1042.441919	83414.737068	34.454912
1042.866368	83507.322845	34.459930
1043.903127	83609.914728	34.464948
1044.806483	83713.211147	34.469965
1045.975450	83810.130771	34.474983
1046.595990	83919.871464	34.480000
1047.377849	84041.795757	34.485018
1048.248848	84152.629540	34.490036
1049.197756	84270.633915	34.495053
1049.782353	84393.950962	34.500071
1050.734384	84521.497010	34.505088
1051.757488	84657.896882	34.510106
1052.760998	84787.427978	34.515124
1053.865596	84931.163616	34.520141
1054.671796	85063.389653	34.525159
1056.039133	85192.751536	34.530176
1056.834713	85341.091528	34.535194
1057.828735	85472.664268	34.540212
1058.873216	85617.678686	34.545229
1059.403625	85763.047751	34.550247
1060.934287	85904.136082	34.555264
1061.824071	86066.623393	34.560282
1063.017521	86207.900155	34.565300
1064.237975	86351.051533	34.570317
1065.683937	86492.865419	34.575335
1066.688508	86637.703408	34.580352
1067.741310	86790.685420	34.585370
1069.093694	86924.328390	34.590388
1070.293550	87069.644098	34.595405
1071.096669	87216.630042	34.600423
1072.485422	87347.297855	34.605440
1073.688295	87485.615836	34.610458
1074.750111	87621.933611	34.615476
1076.132475	87755.526391	34.620493
1076.961019	87889.467359	34.625511
1078.316050	88015.534679	34.630528
1079.268247	88153.713432	34.635546
1080.783276	88283.525786	34.640564
1081.930131	88414.466197	34.645581
1082.746263	88553.636682	34.650599
1084.245620	88673.158718	34.655616
1085.153376	88811.785084	34.660634
1086.467389	88931.938797	34.665652
1087.637909	89058.104780	34.670669
1088.794809	89185.083132	34.675687
1089.900355	89313.006350	34.680704
1091.046819	89439.089835	34.685722
1092.133924	89558.404060	34.690740
1093.137617	89682.589138	34.695757
1094.269199	89801.505524	34.700775
1095.619348	89916.656517	34.705792
1096.815271	90037.948183	34.710810
1097.884962	90152.721307	34.715828
1098.701980	90256.613158	34.720845
1099.441753	90363.458600	34.725863
1100.478938	90466.753566	34.730880
1101.642739	90600.202556	34.735898
1102.729243	90713.129223	34.740916
1103.556529	90823.213746	34.745933
1104.498649	90958.363508	34.750951
1105.495009	91067.151139	34.755968
1106.473810	91204.415300	34.760986
1107.453435	91332.383012	34.766004
1108.514713	91466.245699	34.771021
1109.395021	91598.373396	34.776039
1110.830556	91731.988434	34.781056
1111.908210	91865.269067	34.786074
1113.384132	91994.787155	34.791092
1114.435212	92123.095958	34.796109
1115.269092	92249.979005	34.801127
1117.029826	92383.362845	34.806144
1117.836536	92524.153939	34.811162
1118.666607	92662.424865	34.816180
1120.235168	92800.541252	34.821197
1121.315324	92935.118239	34.826215
1122.591779	93056.325184	34.831232
1123.572970	93201.343291	34.836250
1124.692873	93329.078869	34.841268
1126.118414	93457.639450	34.846285
1127.219601	93587.719818	34.851303
1128.505422	93721.497177	34.856320
1129.497785	93850.280726	34.861338
1130.612553	93980.917857	34.866356
1131.955748	94120.229501	34.871373
1133.039605	94243.156095	34.876391
1134.868410	94374.257584	34.881408
1135.670562	94500.431084	34.886426
1137.022824	94611.823574	34.891444
1138.346978	94741.634833	34.896461
1139.285494	94859.710910	34.901479
1140.905189	94974.706225	34.906496
1141.917836	95103.303992	34.911514
1142.833209	95224.232222	34.916532
1144.208775	95340.128532	34.921549
1145.189683	95464.754521	34.926567
1146.489928	95572.617618	34.931584
1147.047059	95706.668215	34.936602
1148.654855	95828.058898	34.941620
1149.911063	95949.974267	34.946637
1150.497044	96082.516939	34.951655
1151.478467	96204.578597	34.956672
1152.745233	96339.076779	34.961690
1153.524841	96477.259088	34.966708
1154.530207	96612.705093	34.971725
1155.408668	96761.172306	34.976743
1156.902657	96886.433069	34.981760
1157.825756	97021.881947	34.986778
1159.175371	97153.778040	34.991796
1160.370780	97274.925757	34.996813
1161.231841	97403.295009	35.001831
1162.177500	97534.390844	35.006848
1163.274226	97663.660387	35.011866
1164.027753	97797.420067	35.016884
1165.367110	97933.795097	35.021901
1166.240790	98079.703123	35.026919
1167.430393	98220.298153	35.031936
1168.529925	98368.342110	35.036954
1169.814260	98514.333115	35.041972
1171.583592	98651.365286	35.046989
1172.302678	98804.508586	35.052007
1173.778781	98949.731644	35.057024
1175.135479	99089.773991	35.062042
1176.203095	99231.685286	35.067060
1177.463675	99379.045837	35.072077
1178.319395	99527.484016	35.077095
1179.788745	99655.750179	35.082112
1180.656680	99806.181195	35.087130
1181.695238	99961.793200	35.092148
1183.132154	100106.998154	35.097165
1184.267544	100264.836581	35.102183
1185.213288	100408.489139	35.107200
1186.524530	100559.272150	35.112218
1187.497447	100723.207309	35.117236
1188.547300	100890.339321	35.122253
1189.741156	101047.781487	35.127271
1190.916586	101210.200957	35.132288
1192.267324	101373.833857	35.137306
1193.019974	101542.713557	35.142324
1194.857718	101711.244765	35.147341
1195.427102	101882.940167	35.152359
1197.245179	102033.544569	35.157376
1198.832063	102204.359191	35.162394
1200.124410	102361.035242	35.167412
1201.729860	102509.360589	35.172429
1202.717054	102671.092458	35.177447
1204.050991	102811.977154	35.182464
1205.251794	102962.230080	35.187482
1205.972993	103127.386449	35.192500
1207.658863	103271.267976	35.197517
1208.633282	103431.330204	35.202535
1209.909185	103580.189306	35.207552
1211.608603	103740.239599	35.212570
1212.584472	103878.295691	35.217588
1214.248564	104025.520185	35.222605
1215.554697	104179.554663	35.227623
1216.884732	104314.152434	35.232640
1217.916945	104463.100140	35.237658
1219.115567	104605.694043	35.242676
1221.052605	104732.356940	35.247693
1222.771328	104868.351567	35.252711
1224.384077	104988.682095	35.257728
1225.554845	105100.957830	35.262746
1226.885357	105216.993102	35.267764
1227.876446	105319.761482	35.272781
1228.950736	105434.889284	35.277799
1230.014041	105541.849262	35.282816
1230.586009	105657.146604	35.287834
1231.430736	105791.791930	35.292852
1232.523750	105912.735036	35.297869
1233.471040	106045.935216	35.302887
1234.516971	106181.139306	35.307904
1235.331805	106326.361312	35.312922
1236.493630	106481.515827	35.317940
1237.665601	106620.695811	35.322957
1238.239955	106787.059096	35.327975
1239.470360	106951.319289	35.332992
1240.737774	107116.631652	35.338010
1241.343661	107281.176926	35.343028
1242.748272	107451.558272	35.348045
1244.039400	107640.585330	35.353063
1245.156379	107799.882018	35.358080
1246.754158	107978.097129	35.363098
1248.022222	108158.682464	35.368116
1249.424332	108329.247603	35.373133
1250.603361	108505.102727	35.378151
1251.840728	108680.734650	35.383168
1253.364754	108865.917627	35.388186
1254.178562	109046.417209	35.393204
1255.577141	109212.507853	35.398221
1256.871664	109406.535737	35.403239
1258.220434	109579.852469	35.408256
1259.427203	109759.130193	35.413274
1260.680970	109944.199738	35.418292
1261.986226	110123.913878	35.423309
1263.263659	110313.520854	35.428327
1264.413877	110498.471781	35.433344
1265.984675	110675.736077	35.438362
1266.855241	110859.778366	35.443380
1268.529402	111046.871909	35.448397
1270.147367	111225.392318	35.453415
1271.322457	111406.908908	35.458432
1272.592438	111584.987160	35.463450
1273.684600	111769.874543	35.468468
1275.527857	111952.985385	35.473485
1276.762604	112122.426060	35.478503
1278.468350	112299.743838	35.483520
1280.264974	112459.241244	35.488538
1281.545637	112622.518627	35.493556
1282.991152	112780.687562	35.498573
1283.994386	112953.297910	35.503591
1285.497294	113113.966686	35.508608
1286.599462	113262.140447	35.513626
1287.670934	113441.314393	35.518644
1289.174873	113603.594112	35.523661
1290.140026	113776.855578	35.528679
1291.456470	113948.796255	35.533696
1292.690831	114109.134256	35.538714
1293.829829	114269.912601	35.543732
1295.155392	114421.267387	35.548749
1296.315247	114582.772454	35.553767
1297.216094	114725.630940	35.558784
1298.924117	114890.615124	35.563802
1299.664752	115063.864143	35.568820
1300.725791	115223.008561	35.573837
1302.013164	115405.637866	35.578855
1303.401069	115582.529186	35.583872
1304.684144	115759.292786	35.588890
1305.334887	115936.519010	35.593908
1306.778580	116108.435134	35.598925
1308.052650	116297.657437	35.603943
1309.125208	116482.937102	35.608960
1310.391135	116670.871871	35.613978
1311.531173	116875.049129	35.618996
1313.030999	117059.536933	35.624013
1314.752443	117254.209898	35.629031
1316.125864	117440.847925	35.634048
1317.808616	117628.375213	35.639066
1319.133408	117812.972229	35.644084
1320.374194	118002.516313	35.649101
1322.035101	118184.719832	35.654119
1323.117958	118378.812646	35.659136
1324.586685	118562.189096	35.664154
1325.907463	118761.679674	35.669172
1326.728681	118950.372936	35.674189
1328.401858	119138.343270	35.679207
1329.292460	119341.819842	35.684224
1331.453104	119530.437374	35.689242
1332.352664	119728.450963	35.694260
1333.743868	119919.511172	35.699277
1335.230589	120111.228808	35.704295
1336.718087	120299.933572	35.709312
1338.429536	120487.274313	35.714330
1339.872062	120679.573041	35.719348
1341.774672	120851.295761	35.724365
1343.211734	121027.083034	35.729383
1344.120870	121213.834588	35.734400
1345.697488	121392.540387	35.739418
1347.006830	121575.545362	35.744436
1348.384775	121748.433861	35.749453
1350.086642	121927.553990	35.754471
1351.353884	122112.291850	35.759488
1352.928280	122277.110059	35.764506
1354.019566	122457.622697	35.769524
1355.245767	122633.783469	35.774541
1356.505172	122798.794302	35.779559
1357.431277	122986.087601	35.784576
1359.144281	123169.647364	35.789594
1360.251977	123365.767919	35.794612
1361.284472	123558.418694	35.799629
1362.680081	123743.312116	35.804647
1364.087568	123930.738175	35.809664
1365.313364	124107.048049	35.814682
1366.476383	124295.858141	35.819700
1367.743202	124478.395807	35.824717
1369.109311	124639.753067	35.829735
1370.288950	124834.504918	35.834752
1371.730798	125011.635039	35.839770
1373.187321	125193.273382	35.844788
1374.798758	125382.551812	35.849805
1375.664128	125567.643357	35.854823
1376.777102	125765.946597	35.859840
1378.559413	125946.816183	35.864858
1379.720736	126145.228508	35.869876
1380.955560	126337.930278	35.874893
1382.324634	126535.413039	35.879911
1383.748865	126748.152867	35.884928
1385.116632	126938.342232	35.889946
1386.699648	127146.068863	35.894964
1387.917694	127345.658980	35.899981
1388.955360	127543.277683	35.904999
1390.706170	127753.503156	35.910016
1392.343756	127954.475166	35.915034
1393.130181	128163.678901	35.920052
1394.648382	128369.714855	35.925069
1396.448361	128578.899999	35.930087
1397.590279	128792.067866	35.935104
1398.926552	128995.413659	35.940122
1400.819033	129213.697606	35.945140
1402.615318	129426.753677	35.950157
1403.724612	129623.565033	35.955175
1404.767484	129834.640921	35.960192
1406.462589	130040.116372	35.965210
1407.622253	130248.921730	35.970228
1409.105498	130467.799952	35.975245
1410.836681	130674.021803	35.980263
1412.168865	130897.463007	35.985280
1413.662862	131102.623451	35.990298
1415.160899	131322.202793	35.995316
1416.309237	131528.409495	36.000333
1417.708120	131741.014155	36.005351
1418.835558	131959.035596	36.010368
1420.708543	132168.793407	36.015386
1421.965070	132401.368252	36.020404
1423.456805	132607.034084	36.025421
1425.647285	132810.132319	36.030439
1427.290856	133030.107190	36.035456
1429.089167	133214.581792	36.040474
1431.007657	133427.116468	36.045492
1432.241839	133622.846128	36.050509
1433.452636	133809.267838	36.055527
1434.903613	134012.251377	36.060544
1436.080299	134195.069820	36.065562
1437.590222	134400.796318	36.070580
1438.991785	134601.637789	36.075597
1440.961286	134788.718204	36.080615
1442.029202	134981.632493	36.085632
1443.797272	135160.650389	36.090650
1445.619244	135331.399064	36.095668
1447.048372	135501.805681	36.100685
1448.496879	135670.854361	36.105703
1449.615516	135841.730468	36.110720
1450.821681	136008.082540	36.115738
1451.751406	136192.904256	36.120756
1453.038430	136379.152971	36.125773
1454.502353	136564.120237	36.130791
1455.783950	136748.065865	36.135808
1456.879350	136945.550697	36.140826
1458.324145	137157.085490	36.145844
1459.207978	137362.412810	36.150861
1460.656646	137566.257845	36.155879
1461.636222	137788.832695	36.160896
1462.827240	138021.222204	36.165914
1464.335010	138235.694744	36.170932
1465.336947	138478.534806	36.175949
1467.332203	138695.632504	36.180967
1468.651691	138934.928120	36.185984
1470.054411	139173.122545	36.191002
1471.549011	139411.418326	36.196020
1473.065941	139644.516417	36.201037
1474.973551	139865.882083	36.206055
1477.092479	140096.695542	36.211072
1479.179970	140301.192826	36.216090
1480.410903	140522.506087	36.221108
1482.062744	140746.010012	36.226125
1484.181830	140957.489944	36.231143
1485.214627	141178.091727	36.236160
1486.789331	141391.701682	36.241178
1488.224514	141618.972620	36.246196
1489.463677	141829.825318	36.251213
1491.442914	142045.048573	36.256231
1492.823923	142267.415335	36.261248
1494.188874	142484.906603	36.266266
1495.546188	142708.395681	36.271284
1496.714441	142932.892371	36.276301
1498.536788	143163.345288	36.281319
1499.769581	143395.211782	36.286336
1501.255342	143623.833071	36.291354
1502.444120	143842.819533	36.296372
1503.926877	144084.753455	36.301389
1505.587845	144322.909091	36.306407
1507.094720	144556.971562	36.311424
1508.254902	144798.227118	36.316442
1509.993288	145033.625327	36.321460
1511.272579	145272.976976	36.326477
1512.820285	145513.707484	36.331495
1514.398301	145753.953343	36.336512
1515.903650	145999.206876	36.341530
1517.279457	146237.359004	36.346548
1518.964962	146485.896127	36.351565
1520.581479	146720.806610	36.356583
1522.235677	146965.841179	36.361600
1524.202059	147189.531767	36.366618
1525.977944	147396.457917	36.371636
1527.274818	147616.898622	36.376653
1529.153313	147825.814150	36.381671
1531.321285	148020.449140	36.386688
1532.789704	148217.465594	36.391706
1534.304032	148414.006923	36.396724
1535.773825	148617.085142	36.401741
1537.022223	148817.816540	36.406759
1538.673455	149017.914723	36.411776
1540.476016	149217.711210	36.416794
1542.244882	149420.696271	36.421812
1543.296194	149620.880820	36.426829
1544.959073	149828.347687	36.431847
1546.337950	150021.915783	36.436864
1547.720658	150233.968282	36.441882
1549.704740	150442.034592	36.446900
1551.119627	150652.677486	36.451917
1552.839504	150853.587454	36.456935
1554.474548	151062.980948	36.461952
1555.735667	151268.999456	36.466970
1557.514983	151483.862268	36.471988
1558.675928	151692.992785	36.477005
1560.680451	151903.334507	36.482023
1561.998130	152118.338181	36.487040
1563.664900	152333.985105	36.492058
1565.300935	152548.941001	36.497076
1566.302479	152776.931175	36.502093
1567.893605	152995.269579	36.507111
1568.972467	153238.693177	36.512128
1570.113072	153469.480665	36.517146
1571.616529	153696.890237	36.522164
1573.264392	153945.743898	36.527181
1574.672790	154197.135217	36.532199
1576.359823	154436.489670	36.537216
1577.534348	154696.898707	36.542234
1579.526542	154951.283965	36.547252
1580.817439	155194.117452	36.552269
1582.571779	155451.739466	36.557287
1583.846140	155707.854720	36.562304
1585.455027	155963.119936	36.567322
1586.978755	156226.705866	36.572340
1588.692634	156490.999054	36.577357
1590.282331	156751.788959	36.582375
1592.166264	157002.478779	36.587392
1593.719115	157263.772937	36.592410
1595.605020	157515.290383	36.597428
1597.033330	157779.245718	36.602445
1599.173762	158025.502117	36.607463
1600.582762	158283.301637	36.612480
1602.171763	158536.674280	36.617498
1604.224213	158782.544225	36.622516
1605.702342	159042.760392	36.627533
1607.130568	159285.867148	36.632551
1608.899665	159537.899607	36.637568
1610.383318	159792.325213	36.642586
1612.097765	160031.993115	36.647604
1613.712826	160252.339467	36.652621
1615.477504	160475.732314	36.657639
1616.926324	160708.358099	36.662656
1618.299522	160935.442908	36.667674
1620.402018	161158.190350	36.672692
1621.800383	161382.065557	36.677709
1623.205794	161608.984666	36.682727
1624.837858	161852.977020	36.687744
1626.317968	162086.925710	36.692762
1627.923549	162327.526729	36.697780
1629.383053	162579.059159	36.702797
1631.537651	162805.955587	36.707815
1633.335799	163050.627174	36.712832
1634.829375	163289.235889	36.717850
1636.737061	163519.308530	36.722868
1638.454720	163760.903160	36.727885
1640.529963	163984.369894	36.732903
1642.373452	164220.316502	36.737920
1643.531599	164456.132501	36.742938
1645.499519	164684.807792	36.747956
1647.523049	164908.973236	36.752973
1649.523908	165128.311425	36.757991
1651.244516	165363.219492	36.763008
1652.692598	165595.128373	36.768026
1654.512774	165810.009456	36.773044
1656.025404	166038.828827	36.778061
1657.409607	166259.260922	36.783079
1658.890693	166491.094029	36.788096
1660.429861	166721.511473	36.793114
1662.123284	166959.858452	36.798132
1663.456110	167209.045340	36.803149
1665.314494	167444.122156	36.808167
1666.861988	167700.660145	36.813184
1667.908722	167949.339251	36.818202
1669.688590	168196.368783	36.823220
1671.212356	168460.297763	36.828237
1672.820411	168717.365714	36.833255
1674.466496	168977.879474	36.838272
1675.991285	169247.826063	36.843290
1677.450495	169505.683990	36.848308
1679.285607	169781.331088	36.853325
1680.747662	170042.414017	36.858343
1682.468196	170315.482762	36.863360
1684.047858	170594.626447	36.868378
1685.900588	170859.306040	36.873396
1687.374413	171142.542298	36.878413
1688.950905	171413.510516	36.883431
1690.819555	171688.442716	36.888448
1692.509183	171974.923470	36.893466
1694.374125	172248.705803	36.898484
1695.724026	172537.363027	36.903501
1697.752906	172809.499460	36.908519
1699.434271	173083.735319	36.913536
1700.668094	173359.617155	36.918554
1702.366377	173624.479307	36.923572
1704.353806	173887.952588	36.928589
1705.679295	174145.253167	36.933607
1707.713546	174398.294507	36.938624
1709.429327	174673.550620	36.943642
1710.946247	174926.208020	36.948660
1712.573603	175194.098341	36.953677
1714.759718	175453.325720	36.958695
1716.582014	175720.604966	36.963712
1718.224248	175994.727202	36.968730
1719.984657	176249.320516	36.973748
1721.638780	176519.207033	36.978765
1723.003270	176793.721220	36.983783
1724.994713	177059.726293	36.988800
1726.310092	177340.176643	36.993818
1728.179331	177613.854876	36.998836
1730.137647	177892.798586	37.003853
1731.952687	178164.573272	37.008871
1733.943932	178444.809511	37.013888
1735.849815	178720.468348	37.018906
1737.933149	178979.036222	37.023924
1739.951564	179246.294231	37.028941
1741.344154	179519.058196	37.033959
1743.181836	179791.677106	37.038976
1745.364514	180065.042301	37.043994
1746.959842	180327.337217	37.049012
1748.374010	180606.169450	37.054029
1750.355495	180877.300616	37.059047
1752.422213	181142.101295	37.064064
1754.047240	181415.627030	37.069082
1755.810240	181680.174695	37.074100
1757.387460	181953.292680	37.079117
1759.096016	182223.130604	37.084135
1760.725338	182492.158016	37.089152
1762.569676	182770.098343	37.094170
1764.732484	183039.818392	37.099188
1766.071274	183324.745071	37.104205
1768.083846	183604.059672	37.109223
1769.870869	183883.627545	37.114240
1771.179828	184179.565648	37.119258
1773.213792	184460.252603	37.124276
1775.261658	184740.494984	37.129293
1777.087476	185021.903694	37.134311
1778.710070	185299.628470	37.139328
1780.503726	185578.114521	37.144346
1782.844144	185850.348420	37.149364
1784.417123	186123.581357	37.154381
1786.027193	186406.720569	37.159399
1787.426506	186681.976657	37.164416
1789.248308	186970.999085	37.169434
1791.075367	187264.565424	37.174452
1792.831969	187543.373804	37.179469
1794.361101	187827.143660	37.184487
1796.627247	188102.600481	37.189504
1798.524364	188391.175607	37.194522
1800.561578	188637.713137	37.199540
1802.342945	188891.678283	37.204557
1803.893920	189151.265096	37.209575
1806.003168	189394.774845	37.214592
1807.458983	189665.204446	37.219610
1809.095669	189932.180428	37.224628
1810.858084	190180.761994	37.229645
1812.222066	190458.253912	37.234663
1814.025331	190726.058129	37.239680
1815.977169	190995.109320	37.244698
1817.933782	191269.440639	37.249716
1819.788476	191535.515202	37.254733
1821.539841	191815.415417	37.259751
1823.347833	192087.490545	37.264768
1825.118671	192365.398306	37.269786
1827.009479	192641.143773	37.274804
1828.748015	192914.452842	37.279821
1830.614515	193197.185461	37.284839
1832.455786	193485.139862	37.289856
1834.238799	193772.864029	37.294874
1836.053482	194066.892526	37.299892
1838.458596	194356.196564	37.304909
1840.051352	194631.137280	37.309927
1842.151763	194918.284541	37.314944
1843.664192	195206.504030	37.319962
1845.599066	195488.883260	37.324980
1847.765792	195771.734921	37.329997
1849.529777	196063.688814	37.335015
1851.049120	196348.435982	37.340032
1853.347481	196635.916800	37.345050
1855.302294	196925.738349	37.350068
1857.443414	197200.872279	37.355085
1859.687230	197483.238716	37.360103
1861.819009	197755.178548	37.365120
1863.494405	198037.600106	37.370138
1865.317957	198313.247184	37.375156
1867.055392	198588.439731	37.380173
1868.788605	198875.057830	37.385191
1870.805751	199156.885284	37.390208
1872.553719	199451.792521	37.395226
1874.364252	199744.254393	37.400244
1875.953723	200028.642096	37.405261
1877.369049	200334.281753	37.410279
1879.596603	200618.139685	37.415296
1881.650822	200918.299299	37.420314
1883.416242	201216.323143	37.425332
1885.432510	201499.851052	37.430349
1886.923937	201807.009999	37.435367
1888.736447	202108.661475	37.440384
1890.397064	202412.179249	37.445402
1892.033906	202724.308712	37.450420
1894.173809	203027.842585	37.455437
1895.895972	203344.277781	37.460455
1897.765011	203654.687238	37.465472
1899.899847	203959.813612	37.470490
1901.635158	204233.371659	37.475508
1903.516907	204531.521473	37.480525
1905.656266	204817.470998	37.485543
1907.184250	205100.827803	37.490560
1908.780400	205393.860847	37.495578
1910.598822	205692.674056	37.500596
1912.603732	205994.099607	37.505613
1913.719950	206299.399894	37.510631
1915.682891	206602.726666	37.515648
1917.664139	206932.647133	37.520666
1919.078435	207252.478318	37.525684
1920.941018	207571.351424	37.530701
1922.327617	207916.986106	37.535719
1924.402238	208250.364613	37.540736
1926.039311	208595.937996	37.545754
1928.403644	208941.601020	37.550772
1930.361187	209272.820118	37.555789
1931.948988	209633.895056	37.560807
1934.291558	209969.652380	37.565824
1936.359971	210317.121933	37.570842
1938.221412	210663.724877	37.575860
1940.415465	211010.645093	37.580877
1942.364478	211364.448929	37.585895
1944.992023	211708.701569	37.590912
1946.708243	212052.123112	37.595930
1948.902121	212396.422842	37.600948
1950.967200	212740.592481	37.605965
1953.216252	213099.398361	37.610983
1955.415328	213441.620643	37.616000
1957.384179	213768.861959	37.621018
1959.220474	214119.118330	37.626036
1961.452321	214465.530336	37.631053
1963.229438	214813.171629	37.636071
1965.478563	215145.377429	37.641088
1967.612512	215477.387287	37.646106
1969.315572	215827.521262	37.651124
1971.518882	216160.031258	37.656141
1973.572730	216497.467382	37.661159
1975.548423	216839.767595	37.666176
1977.725274	217173.213458	37.671194
1979.492335	217508.998613	37.676212
1981.795587	217828.321579	37.681229
1983.967779	218160.884051	37.686247
1986.407093	218480.810474	37.691264
1988.324484	218806.890217	37.696282
1990.375153	219132.099583	37.701300
1992.893796	219456.258473	37.706317
1994.403966	219786.432131	37.711335
1996.458469	220100.370235	37.716352
1998.710378	220426.797687	37.721370
2000.302074	220749.687236	37.726388
2001.853263	221123.995646	37.731405
2003.913168	221454.292576	37.736423
2005.897273	221785.859999	37.741440
2007.760933	222113.283221	37.746458
2009.506406	222425.019847	37.751476
2011.625214	222726.210358	37.756493
2013.104027	223044.949997	37.761511
2014.910510	223365.518179	37.766528
2016.680953	223693.280244	37.771546
2018.729598	224015.425226	37.776564
2020.486747	224332.195816	37.781581
2022.490988	224663.645190	37.786599
2024.262500	225001.824609	37.791616
2026.203619	225345.959228	37.796634
2027.975539	225694.845770	37.801652
2030.150165	226033.105141	37.806669
2031.876875	226405.620133	37.811687
2033.953977	226757.484830	37.816704
2036.379424	227111.809957	37.821722
2038.280303	227475.997415	37.826740
2040.230262	227848.305524	37.831757
2042.221710	228195.897696	37.836775
2044.141581	228561.432720	37.841792
2046.237855	228930.166676	37.846810
2048.323853	229310.154653	37.851828
2050.281685	229677.034285	37.856845
2052.553014	230054.888049	37.861863
2054.876321	230435.249468	37.866880
2057.298624	230793.729601	37.871898
2059.280593	231182.351614	37.876916
2061.822134	231540.815713	37.881933
2063.971518	231902.010151	37.886951
2066.369355	232251.610554	37.891968
2068.714688	232610.871758	37.896986
2070.776368	232975.208099	37.902004
2073.460888	233324.792309	37.907021
2075.642778	233691.398075	37.912039
2077.005292	234048.280663	37.917056
2079.098503	234400.045133	37.922074
2081.198823	234759.835606	37.927092
2083.561734	235129.135537	37.932109
2085.347109	235489.562708	37.937127
2087.624981	235848.516076	37.942144
2089.985049	236203.571623	37.947162
2091.707532	236569.473231	37.952180
2093.961194	236926.554591	37.957197
2096.374158	237279.751213	37.962215
2098.449575	237635.872632	37.967232
2100.955376	237985.373942	37.972250
2102.788223	238341.129735	37.977268
2105.110759	238684.769685	37.982285
2107.082492	239037.635527	37.987303
2109.267602	239385.922102	37.992320
2111.620154	239743.631819	37.997338
2113.288511	240108.918674	38.002356
2115.362220	240449.326812	38.007373
2117.669448	240805.903970	38.012391
2119.742364	241164.500550	38.017408
2122.067661	241517.571765	38.022426
2123.669428	241855.874344	38.027444
2125.176262	242189.316087	38.032461
2127.174406	242534.542669	38.037479
2129.003835	242873.599297	38.042496
2131.300785	243213.649481	38.047514
2132.890786	243581.219710	38.052532
2134.882744	243941.640489	38.057549
2136.885859	244290.833453	38.062567
2138.745213	244665.399920	38.067584
2140.854061	245029.488180	38.072602
2142.779768	245411.742578	38.077620
2145.053029	245794.958935	38.082637
2146.611818	246190.736089	38.087655
2148.631903	246582.021411	38.092672
2150.885593	246969.435189	38.097690
2152.861672	247375.004992	38.102708
2155.104245	247780.635238	38.107725
2157.191051	248182.938322	38.112743
2159.228197	248596.782521	38.117760
2161.377441	249005.859991	38.122778
2163.450332	249438.167521	38.127796
2165.647423	249849.881318	38.132813
2168.046024	250281.402799	38.137831
2170.137776	250701.568746	38.142848
2172.544322	251126.816948	38.147866
2174.897728	251560.762024	38.152884
2177.108321	251981.725106	38.157901
2179.279280	252402.162028	38.162919
2181.435936	252825.574214	38.167936
2184.068940	253253.789000	38.172954
2186.015251	253672.181471	38.177972
2188.697614	254085.784134	38.182989
2191.342828	254508.868555	38.188007
2193.654423	254923.573255	38.193024
2196.191650	255325.364077	38.198042
2198.671768	255747.486558	38.203060
2200.921344	256157.580327	38.208077
2203.143890	256559.296368	38.213095
2205.462694	256970.930216	38.218112
2207.827606	257375.927450	38.223130
2209.939733	257786.935067	38.228148
2212.417607	258187.876780	38.233165
2214.514970	258600.742507	38.238183
2216.448939	259006.090241	38.243200
2218.843947	259408.342581	38.248218
2220.700136	259823.458548	38.253236
2222.767736	260232.241741	38.258253
2224.920333	260656.761784	38.263271
2227.173053	261072.858240	38.268288
2229.659744	261487.876662	38.273306
2231.420000	261899.759273	38.278324
2233.570424	262319.684086	38.283341
2236.404397	262735.970034	38.288359
2238.677140	263151.456391	38.293376
2241.029079	263547.090925	38.298394
2243.038075	263954.516483	38.303412
2245.377073	264334.861282	38.308429
2247.578576	264712.179886	38.313447
2249.339516	265110.932732	38.318464
2251.389202	265488.199914	38.323482
2253.418814	265899.688675	38.328500
2255.457699	266299.059014	38.333517
2257.594611	266698.210918	38.338535
2259.842377	267108.370566	38.343552
2262.203392	267513.406523	38.348570
2264.540517	267932.189733	38.353588
2266.713271	268347.976313	38.358605
2268.811940	268771.599133	38.363623
2270.797954	269192.674348	38.368640
2273.227157	269617.972700	38.373658
2274.987484	270058.289105	38.378676
2277.535208	270485.575983	38.383693
2279.712733	270924.531095	38.388711
2282.073394	271368.868276	38.393728
2284.722897	271807.977536	38.398746
2286.856855	272247.448121	38.403764
2289.292065	272698.556630	38.408781
2291.963705	273133.776034	38.413799
2294.120832	273575.885210	38.418816
2296.732749	274008.523077	38.423834
2298.982345	274461.464953	38.428852
2301.039316	274905.342965	38.433869
2303.600732	275354.653538	38.438887
2305.463319	275812.203977	38.443904
2307.879663	276261.816916	38.448922
2310.086934	276709.125820	38.453940
2312.494476	277176.598584	38.458957
2315.205514	277627.383886	38.463975
2317.455779	278087.361917	38.468992
2319.798222	278539.170684	38.474010
2322.208928	279005.905622	38.479028
2324.437519	279465.759500	38.484045
2326.995469	279919.210089	38.489063
2328.624488	280393.257367	38.494080
2330.948407	280854.695748	38.499098
2333.566180	281326.629593	38.504116
2335.503850	281800.728569	38.509133
2338.263947	282262.477821	38.514151
2340.522499	282748.134419	38.519168
2343.105433	283211.206501	38.524186
2345.787851	283679.495427	38.529204
2348.171327	284148.237722	38.534221
2350.353199	284613.277218	38.539239
2352.327713	285089.577235	38.544256
2355.086495	285557.039107	38.549274
2357.605026	286037.417826	38.554292
2359.832624	286506.690121	38.559309
2362.674086	286968.091171	38.564327
2364.782098	287429.633261	38.569344
2367.753352	287873.611473	38.574362
2370.162619	288312.089517	38.579380
2372.633400	288741.335955	38.584397
2374.940531	289152.520932	38.589415
2377.018620	289581.472736	38.594432
2379.018733	290005.279489	38.599450
2381.529210	290439.775403	38.604468
2383.809052	290878.168353	38.609485
2385.993528	291300.826072	38.614503
2388.169892	291745.228920	38.619520
2390.669218	292183.762591	38.624538
2393.123758	292631.371213	38.629556
2395.731214	293084.695662	38.634573
2398.265452	293512.526861	38.639591
2400.383591	293982.870386	38.644608
2402.421672	294428.661617	38.649626
2404.753109	294892.821966	38.654644
2406.643304	295356.136722	38.659661
2409.260951	295818.268209	38.664679
2411.410807	296294.723259	38.669696
2413.968053	296780.892284	38.674714
2415.982089	297262.853226	38.679732
2418.222083	297740.712793	38.684749
2421.143697	298226.820207	38.689767
2422.731569	298738.996535	38.694784
2425.231961	299238.402119	38.699802
2427.974993	299737.920165	38.704820
2429.941428	300254.172298	38.709837
2432.641534	300760.018953	38.714855
2434.731859	301285.367179	38.719872
2437.270311	301798.907260	38.724890
2439.774991	302322.357370	38.729908
2441.955149	302850.861061	38.734925
2444.376626	303379.629401	38.739943
2446.718423	303920.829399	38.744960
2449.359898	304448.441251	38.749978
2451.961295	304977.352867	38.754996
2454.362222	305518.156218	38.760013
2457.087691	306065.992644	38.765031
2459.571000	306590.522300	38.770048
2462.695138	307120.917298	38.775066
2465.273686	307656.705153	38.780084
2468.094528	308184.476716	38.785101
2470.793445	308694.079037	38.790119
2473.482316	309228.394743	38.795136
2475.982435	309742.392859	38.800154
2478.626362	310257.889899	38.805172
2480.805047	310765.940141	38.810189
2483.470495	311294.738385	38.815207
2486.057785	311815.469586	38.820224
2488.704118	312324.530814	38.825242
2490.921376	312848.998608	38.830260
2493.584565	313364.021020	38.835277
2496.379069	313868.174885	38.840295
2498.818099	314387.113812	38.845312
2501.007242	314894.939822	38.850330
2503.617731	315379.228506	38.855348
2505.855236	315865.935996	38.860365
2508.317770	316355.830999	38.865383
2510.504420	316850.161121	38.870400
2512.772065	317329.008635	38.875418
2514.973788	317831.966596	38.880436
2517.274782	318340.646004	38.885453
2519.819823	318841.283806	38.890471
2522.186042	319353.452198	38.895488
2524.120756	319868.860742	38.900506
2526.765342	320388.141196	38.905524
2528.969035	320920.491670	38.910541
2531.723389	321446.631097	38.915559
2534.107966	321994.666946	38.920576
2536.591858	322520.182433	38.925594
2539.316294	323063.713266	38.930612
2541.527402	323616.540698	38.935629
2544.402424	324157.145464	38.940647
2546.935530	324713.749360	38.945664
2548.984702	325277.689262	38.950682
2551.854175	325823.845511	38.955700
2553.997900	326393.248006	38.960717
2556.970535	326948.801790	38.965735
2559.449503	327521.393567	38.970752
2562.009807	328096.228343	38.975770
2564.833757	328662.306756	38.980788
2567.179975	329246.308763	38.985805
2570.128710	329825.411295	38.990823
2572.909936	330395.698802	38.995840
2575.008153	330971.956018	39.000858
2577.992723	331547.230256	39.005876
2580.989387	332124.986514	39.010893
2583.657241	332698.752692	39.015911
2586.607126	333264.826290	39.020928
2589.513087	333825.442851	39.025946
2592.186633	334398.406996	39.030964
2594.474465	334973.890496	39.035981
2597.011726	335540.290065	39.040999
2599.754195	336116.961396	39.046016
2602.226618	336691.461453	39.051034
2605.327433	337259.737654	39.056052
2607.976939	337828.283539	39.061069
2610.893545	338392.389503	39.066087
2613.603133	338962.921743	39.071104
2616.117615	339527.462251	39.076122
2618.684471	340089.882025	39.081140
2621.290124	340663.233657	39.086157
2624.103476	341202.372536	39.091175
2626.776945	341782.304354	39.096192
2629.710311	342341.167195	39.101210
2632.467223	342900.255932	39.106228
2635.175325	343461.251343	39.111245
2637.823799	344017.960244	39.116263
2640.549974	344569.954747	39.121280
2642.821382	345114.704321	39.126298
2645.440522	345640.835207	39.131316
2647.403886	346184.430271	39.136333
2650.099882	346699.673390	39.141351
2652.784844	347232.354527	39.146368
2655.191164	347767.562677	39.151386
2657.459739	348300.731207	39.156404
2659.645438	348848.479525	39.161421
2661.993880	349401.324616	39.166439
2664.411632	349970.958578	39.171456
2666.726771	350540.526659	39.176474
2669.543455	351120.188786	39.181492
2671.713737	351701.063955	39.186509
2674.175802	352286.075033	39.191527
2676.950551	352887.504603	39.196544
2679.080812	353506.645941	39.201562
2681.858257	354110.447060	39.206580
2684.249588	354730.166972	39.211597
2687.758962	355329.091073	39.216615
2690.635061	355941.256764	39.221632
2693.529839	356561.001450	39.226650
2696.597201	357159.745301	39.231668
2699.265569	357780.069057	39.236685
2702.120891	358394.644493	39.241703
2705.287372	358991.675136	39.246720
2708.088028	359606.446960	39.251738
2710.750149	360217.806466	39.256756
2713.604944	360832.350940	39.261773
2716.500194	361436.551346	39.266791
2719.092631	362055.233032	39.271808
2721.885412	362676.793430	39.276826
2724.941624	363278.482725	39.281844
2727.522892	363895.542762	39.286861
2730.172613	364515.070720	39.291879
2732.988515	365125.859243	39.296896
2735.704937	365758.150168	39.301914
2738.628253	366368.371874	39.306932
2741.317152	366991.082444	39.311949
2744.201036	367603.501205	39.316967
2747.318367	368223.969490	39.321984
2749.760576	368837.126097	39.327002
2752.544659	369458.543073	39.332020
2755.643302	370078.150380	39.337037
2758.408736	370692.244390	39.342055
2761.380882	371311.600054	39.347072
2764.226816	371932.032331	39.352090
2767.172468	372550.308251	39.357108
2769.771281	373167.970217	39.362125
2772.651935	373779.438090	39.367143
2775.039424	374397.825567	39.372160
2777.501950	375021.291625	39.377178
2780.687714	375643.035175	39.382196
2783.661266	376250.442543	39.387213
2786.507660	376865.979586	39.392231
2789.470017	377493.083149	39.397248
2792.130646	378096.985448	39.402266
2794.711629	378679.707284	39.407284
2797.410605	379272.169025	39.412301
2800.219276	379845.501467	39.417319
2802.478462	380429.897093	39.422336
2805.121559	381020.615893	39.427354
2807.990693	381603.121326	39.432372
2810.906866	382178.532864	39.437389
2813.350377	382780.468461	39.442407
2816.538926	383368.045737	39.447424
2819.362876	383967.289326	39.452442
2822.092201	384567.400713	39.457460
2824.377463	385183.933463	39.462477
2827.583335	385790.316301	39.467495
2830.265558	386402.402981	39.472512
2832.766398	387027.418511	39.477530
2835.647103	387644.931536	39.482548
2838.295482	388280.935304	39.487565
2841.093195	388906.277093	39.492583
2844.217918	389555.244687	39.497600
2847.168864	390194.311381	39.502618
2850.252616	390827.055808	39.507636
2853.090120	391471.088126	39.512653
2856.135377	392099.554969	39.517671
2858.728124	392751.438762	39.522688
2861.556247	393404.972073	39.527706
2864.469925	394047.752460	39.532724
2867.146860	394708.106436	39.537741
2870.162492	395350.592485	39.542759
2873.734944	395989.149136	39.547776
2876.558398	396650.938011	39.552794
2879.812114	397293.805604	39.557812
2882.404065	397952.106040	39.562829
2885.635286	398601.645853	39.567847
2888.625375	399248.979737	39.572864
2891.155492	399912.017479	39.577882
2894.300523	400554.229971	39.582900
2897.186190	401207.372861	39.587917
2899.849129	401873.112928	39.592935
2902.941310	402527.235742	39.597952
2905.650941	403189.695820	39.602970
2908.524279	403858.175161	39.607988
2911.138174	404536.390839	39.613005
2913.797762	405203.303636	39.618023
2916.998744	405876.707460	39.623040
2919.169620	406578.296149	39.628058
2922.189741	407258.137271	39.633076
2925.242156	407956.437097	39.638093
2927.994146	408643.539487	39.643111
2931.016231	409330.811704	39.648128
2933.967309	410027.077539	39.653146
2936.776548	410720.815104	39.658164
2940.123510	411419.216384	39.663181
2943.129292	412111.547186	39.668199
2946.159288	412800.005649	39.673216
2948.645403	413507.136265	39.678234
2951.868050	414160.482211	39.683252
2954.993941	414818.441145	39.688269
2957.604420	415479.558439	39.693287
2960.409377	416131.608335	39.698304
2963.063985	416788.938095	39.703322
2965.945520	417455.972767	39.708340
2968.815381	418133.256148	39.713357
2971.485702	418802.294453	39.718375
2974.529921	419478.504455	39.723392
2977.202205	420176.218017	39.728410
2980.235640	420872.767504	39.733428
2983.131010	421559.744242	39.738445
2986.123433	422264.575592	39.743463
2989.137914	422951.828195	39.748480
2992.069974	423672.872749	39.753498
2994.802520	424383.694977	39.758516
2997.974578	425093.593040	39.763533
3001.070458	425812.730834	39.768551
3004.178455	426528.731666	39.773568
3007.158741	427262.845252	39.778586
3009.978746	427985.767941	39.783604
3013.332471	428714.209628	39.788621
3016.348407	429446.256027	39.793639
3019.765317	430181.789831	39.798656
3022.667882	430915.991296	39.803674
3025.832144	431637.593830	39.808692
3029.196691	432385.559670	39.813709
3032.004934	433113.913998	39.818727
3035.256982	433850.129335	39.823744
3038.038218	434600.123479	39.828762
3040.944959	435336.882238	39.833780
3044.434799	436082.567345	39.838797
3047.080615	436831.681032	39.843815
3049.985496	437587.340059	39.848832
3053.124842	438343.420145	39.853850
3056.088391	439100.416486	39.858868
3058.817611	439870.845524	39.863885
3061.955279	440632.982810	39.868903
3065.698914	441387.810427	39.873920
3068.773105	442163.327928	39.878938
3071.970114	442931.004027	39.883956
3074.930546	443690.946852	39.888973
3077.867980	444462.564209	39.893991
3081.173779	445239.515322	39.899008
3084.062135	446005.167266	39.904026
3087.375449	446770.372843	39.909044
3090.435461	447551.893581	39.914061
3093.381522	448333.710019	39.919079
3097.135586	449095.024177	39.924096
3100.073489	449873.095147	39.929114
3103.321425	450637.323840	39.934132
3107.013884	451389.208610	39.939149
3110.049390	452149.472843	39.944167
3113.425710	452900.295140	39.949184
3116.983906	453638.867447	39.954202
3120.182967	454345.641342	39.959220
3123.509527	455038.810931	39.964237
3126.664730	455736.742898	39.969255
3130.192937	456415.567998	39.974272
3132.973648	457111.947579	39.979290
3135.814761	457801.920394	39.984308
3139.163049	458487.389542	39.989325
3141.613829	459185.881061	39.994343
3144.529311	459890.702187	39.999360
3147.459988	460598.432499	40.004378
3150.781271	461310.833477	40.009396
3153.751333	462047.296074	40.014413
3156.443461	462791.213757	40.019431
3160.109117	463520.079773	40.024448
3162.731099	464259.657965	40.029466
3165.925834	464996.287374	40.034484
3169.294635	465740.147182	40.039501
3171.808668	466499.997494	40.044519
3175.261610	467264.021440	40.049536
3178.286627	468019.588835	40.054554
3181.480902	468773.939006	40.059572
3184.748590	469537.504643	40.064589
3187.736851	470301.895482	40.069607
3191.081496	471071.966282	40.074624
3194.151668	471855.501919	40.079642
3197.081287	472640.445605	40.084660
3200.591057	473423.447165	40.089677
3203.488982	474214.453103	40.094695
3206.694231	475009.929666	40.099712
3209.757272	475800.493529	40.104730
3212.739779	476611.765715	40.109748
3216.401019	477414.860074	40.114765
3219.314556	478233.862098	40.119783
3222.635129	479038.006315	40.124800
3225.796640	479858.974336	40.129818
3228.637791	480682.789170	40.134836
3232.155279	481503.429997	40.139853
3235.545582	482322.843529	40.144871
3239.139473	483136.429214	40.149888
3242.622240	483965.411160	40.154906
3245.683670	484798.315062	40.159924
3249.018081	485621.084294	40.164941
3252.659019	486447.205533	40.169959
3255.870294	487264.618043	40.174976
3259.296112	488087.367392	40.179994
3262.262501	488909.900992	40.185012
3265.773872	489737.566422	40.190029
3269.009931	490562.106853	40.195047
3272.357277	491387.098441	40.200064
3275.379451	492217.661195	40.205082
3278.572625	493047.705113	40.210100
3281.595237	493889.203867	40.215117
3284.683497	494733.482027	40.220135
3287.796311	495586.706878	40.225152
3291.544088	496409.137712	40.230170
3294.235573	497209.428693	40.235188
3297.697740	498017.288319	40.240205
3300.545423	498825.764375	40.245223
3303.327930	499636.637966	40.250240
3306.667049	500453.546498	40.255258
3309.664753	501270.875511	40.260276
3312.823774	502094.855866	40.265293
3315.850194	502941.434799	40.270311
3318.992967	503778.313116	40.275328
3322.272902	504628.203484	40.280346
3325.261894	505482.691802	40.285364
3328.319371	506346.414318	40.290381
3331.475441	507225.471553	40.295399
3334.772894	508094.772115	40.300416
3337.842484	508989.095266	40.305434
3341.261716	509887.959053	40.310452
3344.746723	510770.567812	40.315469
3348.164208	511676.805653	40.320487
3352.263584	512578.094178	40.325504
3355.922490	513467.043756	40.330522
3359.255401	514360.639215	40.335540
3362.695063	515273.036919	40.340557
3366.103822	516165.868246	40.345575
3369.387554	517085.858774	40.350592
3373.129707	517981.969726	40.355610
3376.587858	518896.636953	40.360628
3380.104334	519789.961829	40.365645
3383.527823	520714.569247	40.370663
3386.984374	521628.983398	40.375680
3390.394068	522534.428595	40.380698
3393.644061	523456.134318	40.385716
3397.008616	524364.660686	40.390733
3400.173417	525293.333268	40.395751
3403.601295	526228.615215	40.400768
3407.268883	527152.311204	40.405786
3410.219580	528091.591914	40.410804
3413.593379	529029.137138	40.415821
3416.727474	529970.343742	40.420839
3420.542027	530920.004296	40.425856
3423.824477	531858.856661	40.430874
3427.178093	532819.712460	40.435892
3430.370906	533792.123423	40.440909
3433.761380	534745.396689	40.445927
3437.072642	535719.128766	40.450944
3440.693247	536688.820704	40.455962
3444.139661	537658.478707	40.460980
3447.985605	538628.868176	40.465997
3452.037866	539585.714583	40.471015
3455.080200	540560.287965	40.476032
3459.030831	541523.474349	40.481050
3461.867010	542478.667289	40.486068
3466.070670	543442.949226	40.491085
3469.958084	544403.694052	40.496103
3473.440252	545357.140106	40.501120
3477.039145	546292.522558	40.506125
3480.046341	547191.984444	40.511130
3483.581245	548032.562300	40.516135
3486.440731	548825.054114	40.521140
3489.204144	549554.337899	40.526144
3492.474253	550205.643553	40.531149
3494.907525	550812.799647	40.536154
3497.200100	551355.316938	40.541159
3499.518435	551844.629756	40.546164
3501.511397	552272.776784	40.551168
3503.875036	552654.637899	40.556173
3505.665600	552976.491754	40.561178
3507.274396	553238.583232	40.566183
3508.634770	553470.994266	40.571188
3510.308118	553657.493840	40.576192
3511.707363	553792.122691	40.581197
3512.780127	553901.678638	40.586202
3514.150549	553975.873109	40.591207
3515.215469	554011.876006	40.596212
3515.773435	554010.072592	40.601216
3516.733108	553994.736084	40.606221
3517.028225	553953.725623	40.611226
3518.006354	553868.969277	40.616231
3518.552567	553779.891656	40.621236
3519.150867	553670.776964	40.626240
3519.723274	553528.721972	40.631245
3520.073701	553381.756546	40.636250
3520.433577	553213.195229	40.641255
3520.611725	553037.294762	40.646260
3520.719650	552841.171992	40.651264
3520.933283	552627.018208	40.656269
3520.837414	552431.981579	40.661274
3521.094388	552198.692703	40.666279
3521.439966	551974.871605	40.671284
3521.435748	551740.052488	40.676288
3521.590913	551493.246119	40.681293
3521.471715	551259.799703	40.686298
3521.504253	551004.426587	40.691303
3521.412033	550761.128465	40.696308
3521.172086	550499.179342	40.701312
3521.433334	550234.724143	40.706317
3520.808534	549990.841284	40.711322
3521.153623	549722.175165	40.716327
3520.786924	549458.864823	40.721332
3520.325976	549197.179488	40.726336
3520.813340	548939.275897	40.731341
3520.408529	548680.852693	40.736346
3520.059706	548416.107642	40.741351
3520.167933	548156.534268	40.746356
3519.501212	547897.684403	40.751360
3519.924746	547633.610639	40.756365
3519.061138	547386.290043	40.761370
3519.361681	547142.061954	40.766375
3519.174541	546890.335987	40.771380
3518.606443	546633.063359	40.776384
3518.657676	546391.789687	40.781389
3518.422066	546141.017583	40.786394
3518.122357	545900.952277	40.791399
3518.108605	545665.077930	40.796404
3517.534775	545435.497092	40.801408
3517.634384	545189.299795	40.806413
3517.195781	544969.129823	40.811418
3517.013703	544728.421144	40.816423
3517.310891	544513.327558	40.821428
3516.781878	544288.971871	40.826432
3516.618082	544065.514237	40.831437
3516.302247	543855.909630	40.836442
3516.406048	543630.585782	40.841447
3516.034264	543428.203176	40.846452
3515.443433	543211.110770	40.851456
3515.384534	543011.045855	40.856461
3514.956001	542801.595692	40.861466
3515.130965	542608.354598	40.866471
3514.710396	542404.249256	40.871476
3514.747351	542218.800084	40.876480
3514.720701	542020.837347	40.881485
3514.466327	541839.670623	40.886490
3514.374530	541651.154899	40.891495
3514.231965	541462.644832	40.896500
3513.554373	541284.921205	40.901504
3513.626315	541091.727345	40.906509
3513.257518	540931.370583	40.911514
3513.425144	540763.807756	40.916519
3513.124566	540597.579416	40.921524
3513.061463	540442.824465	40.926528
3513.127088	540267.748560	40.931533
3513.005211	540095.376532	40.936538
3512.791302	539937.105533	40.941543
3512.690210	539776.290209	40.946548
3512.051014	539622.072371	40.951552
3512.364025	539466.238026	40.956557
3511.837290	539323.310869	40.961562
3511.607788	539169.680145	40.966567
3511.642672	539022.823480	40.971572
3511.540075	538883.915581	40.976576
3511.623169	538735.230522	40.981581
3511.196557	538604.249309	40.986586
3511.290339	538449.499684	40.991591
3510.865584	538327.100984	40.996596
3510.857909	538196.302547	41.001600
3511.278639	538072.859134	41.006605
3510.657460	537937.256702	41.011610
3510.756842	537803.458301	41.016615
3510.314778	537680.703614	41.021620
3510.178050	537557.748167	41.026624
3510.618031	537431.720809	41.031629
3509.859824	537314.467632	41.036634
3510.244077	537190.265268	41.041639
3510.011438	537079.694934	41.046644
3509.836024	536967.246030	41.051648
3509.937849	536846.519926	41.056653
3509.654116	536738.985592	41.061658
3509.753935	536617.500396	41.066663
3509.332204	536516.804786	41.071668
3509.315595	536397.962645	41.076672
3509.355656	536299.920051	41.081677
3509.456595	536201.109579	41.086682
3509.360874	536086.924322	41.091687
3508.963888	535993.999748	41.096692
3508.796549	535893.057795	41.101696
3509.157913	535790.869887	41.106701
3508.826476	535700.862754	41.111706
3508.996143	535601.734502	41.116711
3508.703424	535506.871098	41.121716
3508.609464	535413.440518	41.126720
3508.424864	535322.195691	41.131725
3508.209689	535232.015903	41.136730
3508.425269	535138.332682	41.141735
3508.626370	535046.015015	41.146740
3508.009485	534966.605791	41.151744
3508.471843	534870.911946	41.156749
3507.868553	534794.328411	41.161754
3507.959413	534706.673353	41.166759
3508.077507	534628.712139	41.171764
3507.732664	534546.681550	41.176768
3508.237890	534465.475939	41.181773
3507.454302	534383.867432	41.186778
3507.171041	534307.281410	41.191783
3507.504278	534235.042893	41.196788
3507.230388	534170.527806	41.201792
3507.514745	534102.085039	41.206797
3507.267072	534027.916752	41.211802
3507.126101	533956.661170	41.216807
3507.021799	533901.059478	41.221812
3506.965815	533835.548745	41.226816
3507.052998	533766.125331	41.231821
3506.718258	533705.507699	41.236826
3506.903805	533636.118671	41.241831
3507.043087	533574.162678	41.246836
3506.735673	533513.287388	41.251840
3506.701599	533440.850637	41.256845
3506.502342	533394.607897	41.261850
3506.552307	533331.250552	41.266855
3506.578270	533281.789243	41.271860
3506.133216	533224.369809	41.276864
3506.700876	533167.244762	41.281869
3506.173933	533118.375508	41.286874
3506.288210	533059.806166	41.291879
3506.026503	533016.401227	41.296884
3506.137375	532971.219626	41.301888
3506.196243	532908.616937	41.306893
3506.135743	532864.826136	41.311898
3505.885700	532809.445643	41.316903
3505.896411	532774.231679	41.321908
3505.740202	532717.522512	41.326912
3506.047324	532650.029623	41.331917
3505.776940	532597.935406	41.336922
3506.011541	532539.041962	41.341927
3506.177178	532491.273762	41.346932
3505.947854	532447.862116	41.351936
3505.919033	532402.599902	41.356941
3505.457405	532361.750783	41.361946
3505.669867	532322.159088	41.366951
3505.826665	532275.755699	41.371956
3505.535108	532240.234652	41.376960
3505.935170	532188.588833	41.381965
3505.377103	532164.729727	41.386970
3505.847764	532121.004446	41.391975
3505.803655	532073.268116	41.396980
3505.903464	532033.137750	41.401984
3505.537280	531988.837057	41.406989
3505.538885	531949.378788	41.411994
3505.750909	531901.904585	41.416999
3505.860135	531861.115494	41.422004
3505.595463	531820.941146	41.427008
3505.477540	531776.802701	41.432013
3505.225400	531750.873685	41.437018
3505.660123	531715.388218	41.442023
3505.699754	531672.437134	41.447028
3505.391585	531630.753469	41.452032
3505.438466	531585.679013	41.457037
3505.209667	531555.400946	41.462042
3505.320722	531508.042554	41.467047
3505.140966	531477.200821	41.472052
3505.106900	531449.064302	41.477056
3505.325422	531410.732441	41.482061
3505.281472	531383.961522	41.487066
3505.077077	531343.927991	41.492071
3505.053114	531315.991734	41.497076
3505.026360	531293.866199	41.502080
3505.015309	531283.712496	41.507085
3504.857319	531278.129232	41.512090
3504.618624	531245.123796	41.517095
3504.770327	531211.500811	41.522100
3504.519580	531198.656595	41.527104
3505.016758	531170.132458	41.532109
3504.736629	531145.469985	41.537114
3504.563991	531129.480811	41.542119
3504.387192	531096.061076	41.547124
3504.491506	531079.169146	41.552128
3504.435638	531067.607678	41.557133
3504.504530	531050.266588	41.562138
3504.587597	531023.474975	41.567143
3504.648686	530996.434163	41.572148
3504.886372	530982.552583	41.577152
3504.987231	530950.958100	41.582157
3504.668792	530923.572944	41.587162
3504.705838	530894.666301	41.592167
3504.768861	530881.469075	41.597172
3504.520483	530854.274827	41.602176
3504.968098	530835.964172	41.607181
3504.675868	530804.633629	41.612186
3504.758804	530785.319505	41.617191
3504.822114	530756.812667	41.622196
3504.867922	530737.100140	41.627200
3505.003362	530706.914440	41.632205
3504.934651	530678.731486	41.637210
3504.666806	530653.813663	41.642215
3505.241634	530626.640487	41.647220
3504.648238	530598.085577	41.652224
3504.606000	530564.289751	41.657229
3504.590417	530551.508888	41.662234
3504.456326	530511.613698	41.667239
3504.711679	530493.434086	41.672244
3504.537842	530473.250673	41.677248
3504.699354	530460.845963	41.682253
3504.513043	530436.773872	41.687258
3504.959506	530413.561751	41.692263
3504.608392	530389.161944	41.697268
3504.617217	530370.414826	41.702272
3504.949788	530344.744753	41.707277
3504.541544	530315.755842	41.712282
3504.526789	530297.921864	41.717287
3504.733559	530268.532492	41.722292
3504.158414	530255.688246	41.727296
3504.575312	530221.566473	41.732301
3504.376230	530212.098661	41.737306
3504.568456	530191.452801	41.742311
3504.600381	530169.670102	41.747316
3504.461757	530148.672254	41.752320
3504.642782	530113.981190	41.757325
3504.210878	530116.727461	41.762330
3504.330848	530090.989521	41.767335
3504.695930	530068.598211	41.772340
3504.525484	530070.494708	41.777344
3504.407968	530027.008139	41.782349
3504.241088	530014.958154	41.787354
3504.401865	529991.638981	41.792359
3504.685431	529975.020705	41.797364
3504.594599	529955.985670	41.802368
3504.703898	529929.642806	41.807373
3504.198214	529913.149211	41.812378
3504.412310	529881.837855	41.817383
3504.432545	529877.135444	41.822388
3504.197546	529848.977284	41.827392
3504.352731	529841.727070	41.832397
3504.299234	529821.826975	41.837402
3504.096557	529804.830609	41.842407
3504.374312	529803.978238	41.847412
3504.521940	529777.477472	41.852416
3504.401130	529760.821826	41.857421
3504.345310	529747.288725	41.862426
3504.381409	529727.728056	41.867431
3504.670968	529694.433743	41.872436
3504.316683	529689.083056	41.877440
3504.137266	529657.732392	41.882445
3504.288833	529650.583722	41.887450
3504.098999	529627.420485	41.892455
3504.813214	529605.529165	41.897460
3504.307875	529596.109387	41.902464
3504.513827	529567.325196	41.907469
3504.408676	529556.376766	41.912474
3504.366632	529533.998516	41.917479
3504.659762	529520.612187	41.922484
3504.349970	529500.701665	41.927488
3504.311532	529487.418245	41.932493
3504.422316	529459.457386	41.937498
3504.250412	529439.828175	41.942503
3504.082112	529440.056899	41.947508
3504.117286	529410.187741	41.952512
3504.434010	529399.981013	41.957517
3504.032060	529393.425021	41.962522
3504.049675	529374.018427	41.967527
3504.375617	529358.706605	41.972532
3504.226183	529345.541671	41.977536
3504.357909	529336.172636	41.982541
3503.977956	529313.695889	41.987546
3503.870509	529297.997730	41.992551
3503.835778	529293.657551	41.997556
3503.856845	529292.441476	42.002560
3504.378639	529271.237010	42.007565
3504.088442	529261.833557	42.012570
3504.144191	529239.085714	42.017575
3504.171824	529224.124098	42.022580
3503.812488	529221.047956	42.027584
3504.166322	529205.883171	42.032589
3504.065731	529198.470964	42.037594
3504.064307	529187.657477	42.042599
3504.212076	529159.993430	42.047604
3503.918373	529123.303429	42.052608
3504.164172	529091.429645	42.057613
3504.003837	529092.566685	42.062618
3504.137530	529056.162696	42.067623
3504.411342	529050.207196	42.072628
3504.313559	529037.589691	42.077632
3504.591498	529007.024485	42.082637
3503.990239	529002.420046	42.087642
3504.160716	528965.353119	42.092647
3504.135646	528968.843796	42.097652
3503.973314	528945.473082	42.102656
3504.102326	528925.340879	42.107661
3504.031619	528931.516985	42.112666
3503.832551	528918.864862	42.117671
3503.848510	528891.524372	42.122676
3503.619184	528890.853166	42.127680
3504.093150	528890.525591	42.132685
3503.910876	528881.862837	42.137690
3503.702220	528860.318484	42.142695
3504.126588	528844.940075	42.147700
3503.964334	528854.364760	42.152704
3504.190417	528831.791537	42.157709
3504.384892	528811.850973	42.162714
3504.190402	528804.605019	42.167719
3504.362144	528782.394043	42.172724
3504.104832	528768.740352	42.177728
3504.155338	528760.899795	42.182733
3503.946813	528743.903209	42.187738
3504.038445	528727.869819	42.192743
3504.233314	528709.546115	42.197748
3503.924989	528696.911082	42.202752
3504.007868	528684.012074	42.207757
3504.014508	528673.954956	42.212762
3503.937937	528650.721849	42.217767
3504.134795	528650.589669	42.222772
3503.975949	528640.609218	42.227776
3503.884173	528608.130886	42.232781
3503.961536	528600.740804	42.237786
3504.075566	528605.523441	42.242791
3503.961451	528589.168698	42.247796
3503.479637	528583.989389	42.252800
3503.949728	528567.693885	42.257805
3503.595669	528578.462918	42.262810
3503.925242	528561.128417	42.267815
3503.916146	528543.897961	42.272820
3503.743504	528545.643386	42.277824
3503.906771	528533.742218	42.282829
3503.847952	528538.046860	42.287834
3503.964873	528524.839141	42.292839
3504.221145	528507.162433	42.297844
3503.858729	528517.932828	42.302848
3503.930175	528485.327378	42.307853
3503.988080	528474.504025	42.312858
3503.666231	528470.967006	42.317863
3504.243770	528463.093534	42.322868
3504.291091	528448.683943	42.327872
3504.193546	528426.211828	42.332877
3503.844940	528416.059094	42.337882
3503.936879	528392.596838	42.342887
3504.025268	528388.439086	42.347892
3503.768468	528387.620599	42.352896
3503.902161	528357.228539	42.357901
3503.844686	528353.801309	42.362906
3503.729649	528353.718424	42.367911
3503.916848	528342.268137	42.372916
3503.797897	528333.241334	42.377920
3504.059777	528310.863848	42.382925
3503.798633	528329.602762	42.387930
3503.814217	528296.500412	42.392935
3504.065352	528286.606540	42.397940
3504.023939	528272.766691	42.402944
3503.780828	528279.374576	42.407949
3503.812055	528252.636980	42.412954
3503.913493	528239.785212	42.417959
3504.131370	528235.657487	42.422964
3504.068426	528229.754907	42.427968
3504.337659	528206.365422	42.432973
3504.231485	528204.562961	42.437978
3504.108646	528187.501699	42.442983
3504.046607	528164.720393	42.447988
3503.768673	528175.983012	42.452992
3503.976496	528158.919989	42.457997
3504.182285	528132.912620	42.463002
3503.969367	528116.876214	42.468007
3504.009995	528114.191448	42.473012
3503.680430	528095.444577	42.478016
3504.076519	528079.867758	42.483021
3503.882176	528075.249263	42.488026
3503.908438	528077.872929	42.493031
3504.204476	528047.100871	42.498036
3503.925891	528040.676419	42.503040
3503.964094	528049.261337	42.508045
3504.045731	528013.873880	42.513050
3503.685167	528003.166883	42.518055
3504.165202	528005.668304	42.523060
3503.921162	527980.136065	42.528064
3504.355945	527967.332459	42.533069
3504.395206	527973.996909	42.538074
3503.779195	527939.528119	42.543079
3504.159580	527927.491109	42.548084
3504.093552	527920.881406	42.553088
3504.106218	527898.845942	42.558093
3504.135403	527888.178335	42.563098
3504.116889	527888.383404	42.568103
3504.127128	527863.063463	42.573108
3503.920823	527855.364121	42.578112
3504.205814	527843.544268	42.583117
3503.857247	527817.826146	42.588122
3503.773053	527817.536240	42.593127
3503.870138	527811.911425	42.598132
3503.900062	527809.935800	42.603136
3503.941773	527786.935410	42.608141
3503.930304	527775.516115	42.613146
3504.057217	527779.134640	42.618151
3503.966186	527759.136807	42.623156
3503.894798	527742.926044	42.628160
3504.097277	527734.909351	42.633165
3503.912013	527733.624698	42.638170
3503.990210	527699.652092	42.643175
3503.978509	527695.863731	42.648180
3504.091022	527691.550375	42.653184
3503.864907	527673.039333	42.658189
3503.978986	527671.100926	42.663194
3503.757054	527649.102195	42.668199
3503.974634	527649.219414	42.673204
3503.662728	527624.606983	42.678208
3503.889074	527612.391937	42.683213
3503.951189	527625.572117	42.688218
3503.580766	527608.599900	42.693223
3504.237954	527588.281444	42.698228
3503.873080	527577.776986	42.703232
3504.073045	527570.720802	42.708237
3503.779463	527552.523502	42.713242
3503.534265	527535.076584	42.718247
3503.613747	527531.122162	42.723252
3503.587829	527543.810958	42.728256
3503.636874	527537.233444	42.733261
3503.741095	527537.570728	42.738266
3503.851352	527527.496504	42.743271
3503.671589	527508.068283	42.748276
3503.901197	527497.874103	42.753280
3503.740972	527493.148971	42.758285
3503.639299	527500.038044	42.763290
3503.646018	527473.404082	42.768295
3504.180229	527460.281132	42.773300
3503.815960	527464.684881	42.778304
3503.974291	527461.526569	42.783309
3503.978422	527442.928329	42.788314
3504.006384	527429.683223	42.793319
3504.229093	527421.713713	42.798324
3504.170559	527394.887785	42.803329
3503.899959	527383.964001	42.808333
3503.845522	527384.477977	42.813338
3503.912914	527369.407251	42.818343
3504.364825	527349.323086	42.823348
3504.066716	527351.593843	42.828353
3504.151572	527316.709697	42.833357
3503.947933	527302.439807	42.838362
3503.923171	527304.515754	42.843367
3504.265437	527293.899338	42.848372
3504.125485	527289.474165	42.853377
3504.134812	527275.979189	42.858381
3503.891580	527266.314435	42.863386
3504.163110	527242.923170	42.868391
3504.203531	527229.473778	42.873396
3503.821273	527216.192257	42.878401
3504.085130	527197.148377	42.883405
3503.913708	527185.652865	42.888410
3504.130294	527179.048721	42.893415
3504.324801	527151.778086	42.898420
3504.069166	527153.941082	42.903425
3504.357115	527122.764212	42.908429
3503.789207	527121.438911	42.913434
3503.649179	527115.548100	42.918439
3503.830706	527093.383753	42.923444
3503.621345	527079.872638	42.928449
3503.615772	527071.231501	42.933453
3504.194234	527068.916393	42.938458
3503.728854	527072.072777	42.943463
3503.940210	527041.110005	42.948468
3503.627520	527042.372346	42.953473
3503.805463	527033.550568	42.958477
3503.815345	527028.394104	42.963482
3503.636676	527027.563194	42.968487
3504.039845	527001.573316	42.973492
3503.832432	527001.252331	42.978497
3503.822220	526992.359193	42.983501
3503.907024	526988.252180	42.988506
3504.005105	526964.028768	42.993511
3503.518603	526961.528202	42.998516
3503.636716	526965.502073	43.003521
3504.255569	526954.841715	43.008525
3503.948624	526934.422124	43.013530
3503.703253	526918.187481	43.018535
3503.828130	526911.597722	43.023540
3503.514169	526912.253810	43.028545
3503.814559	526887.543457	43.033549
3503.949272	526881.558596	43.038554
3503.851261	526883.848331	43.043559
3503.884503	526870.197614	43.048564
3504.012734	526853.145772	43.053569
3504.091278	526834.787754	43.058573
3503.805615	526832.760812	43.063578
3503.595387	526820.563625	43.068583
3504.128644	526806.985440	43.073588
3504.228319	526806.615913	43.078593
3504.282846	526787.301396	43.083597
3504.224177	526765.427253	43.088602
3504.039747	526755.601276	43.093607
3503.921481	526732.877343	43.098612
3503.961785	526718.972686	43.103617
3503.981067	526713.814634	43.108621
3504.038312	526716.332549	43.113626
3504.173549	526688.666176	43.118631
3504.313218	526677.070586	43.123636
3503.937242	526675.158977	43.128641
3504.177899	526653.287909	43.133645
3503.990296	526651.750838	43.138650
3503.926674	526624.722259	43.143655
3503.930040	526601.271359	43.148660
3503.941034	526603.291207	43.153665
3503.907182	526587.174412	43.158669
3503.909147	526573.124068	43.163674
3504.115328	526559.496291	43.168679
3504.013564	526554.812178	43.173684
3503.710149	526542.023029	43.178689
3503.934251	526513.584210	43.183693
3504.228271	526511.819381	43.188698
3504.372715	526502.800445	43.193703
3504.276594	526487.350411	43.198708
3504.013224	526484.460719	43.203713
3504.363235	526453.879213	43.208717
3504.118532	526430.618892	43.213722
3503.452846	526431.229511	43.218727
3503.764370	526415.917137	43.223732
3503.591657	526393.403486	43.228737
3504.096940	526388.977157	43.233741
3503.974481	526386.216797	43.238746
3503.620882	526382.684325	43.243751
3503.917178	526351.201386	43.248756
3503.733653	526355.829571	43.253761
3503.971771	526348.564656	43.258765
3503.923876	526341.698728	43.263770
3503.552659	526341.757402	43.268775
3503.973610	526316.673328	43.273780
3503.588426	526320.170965	43.278785
3503.584300	526312.186215	43.283789
3503.601787	526314.811559	43.288794
3503.693430	526294.328146	43.293799
3504.145177	526271.008054	43.298804
3503.620993	526271.798475	43.303809
3503.507147	526267.065647	43.308813
3503.857444	526271.811644	43.313818
3503.633279	526247.183211	43.318823
3504.007731	526229.889623	43.323828
3503.872879	526233.246630	43.328833
3503.570801	526226.976777	43.333837
3503.831673	526220.365238	43.338842
3503.619675	526202.305119	43.343847
3503.825345	526187.868452	43.348852
3503.639901	526187.493437	43.353857
3503.787870	526190.856292	43.358861
3503.662879	526175.157813	43.363866
3503.521183	526158.501680	43.368871
3503.788495	526156.690494	43.373876
3503.890498	526161.020900	43.378881
3503.907498	526155.205995	43.383885
3503.706851	526132.292063	43.388890
3504.008796	526114.403318	43.393895
3504.007564	526116.273536	43.398900
3503.488507	526119.741835	43.403905
3503.658699	526106.523690	43.408909
3503.661756	526083.223702	43.413914
3503.410508	526090.137024	43.418919
3503.842928	526067.931598	43.423924
3503.414324	526083.414436	43.428929
3503.663381	526083.627777	43.433933
3503.401106	526072.752316	43.438938
3503.432391	526076.942299	43.443943
3503.996275	526053.351458	43.448948
3503.742590	526049.398788	43.453953
3503.748038	526040.199395	43.458957
3503.830355	526045.240524	43.463962
3503.674814	526036.268740	43.468967
3503.901635	526016.370103	43.473972
3503.284609	526023.644517	43.478977
3503.862916	526013.646984	43.483981
3503.795066	526012.646879	43.488986
3503.596930	526006.815383	43.493991
3503.946794	525973.604823	43.498996
3503.581018	525973.965887	43.504001
3503.838728	525971.195907	43.509005
3504.010526	525972.634460	43.514010
3503.772380	525953.365194	43.519015
3503.762803	525943.511079	43.524020
3503.539804	525941.170866	43.529025
3503.568407	525932.018293	43.534029
3503.605903	525937.875207	43.539034
3503.529564	525931.064140	43.544039
3504.196619	525905.283480	43.549044
3503.946847	525896.983556	43.554049
3503.909418	525885.971345	43.559053
3503.974150	525888.538749	43.564058
3503.807225	525869.915170	43.569063
3503.764057	525860.319022	43.574068
3503.602004	525862.164147	43.579073
3503.707813	525849.966806	43.584077
3503.499521	525827.559065	43.589082
3503.150113	525825.592610	43.594087
3503.692793	525812.921853	43.599092
3503.538974	525823.812717	43.604097
3503.274692	525824.208284	43.609101
3503.525209	525823.157847	43.614106
3503.305039	525830.773958	43.619111
3503.577960	525818.246927	43.624116
3503.527396	525834.731636	43.629121
3503.837799	525811.938636	43.634125
3503.475842	525805.880249	43.639130
3503.367422	525790.077689	43.644135
3503.997358	525777.494197	43.649140
3503.618879	525790.139029	43.654145
3503.923869	525788.524015	43.659149
3503.734858	525769.499472	43.664154
3503.780119	525757.261088	43.669159
3503.741660	525744.328335	43.674164
3503.615043	525757.994773	43.679169
3503.481138	525749.474289	43.684173
3503.701819	525744.890600	43.689178
3503.427943	525731.337995	43.694183
3503.580908	525714.786453	43.699188
3503.380459	525715.626815	43.704193
3503.638570	525713.513779	43.709197
3503.830489	525708.833541	43.714202
3503.736906	525704.097342	43.719207
3504.005660	525685.859567	43.724212
3503.790942	525670.023147	43.729217
3503.609573	525667.271973	43.734221
3503.758700	525668.562510	43.739226
3503.933954	525660.650166	43.744231
3504.288371	525639.214615	43.749236
3503.854416	525632.106146	43.754241
3503.701919	525630.866682	43.759245
3503.745684	525605.386228	43.764250
3503.891464	525582.315666	43.769255
3503.948535	525578.768646	43.774260
3503.660873	525587.052598	43.779265
3504.019321	525555.709899	43.784269
3503.469688	525550.439223	43.789274
3503.255910	525550.270841	43.794279
3503.735531	525541.046757	43.799284
3503.496850	525533.351406	43.804289
3503.664277	525548.690008	43.809293
3504.014886	525536.504278	43.814298
3503.569091	525522.018353	43.819303
3503.833057	525510.402272	43.824308
3503.217547	525513.481600	43.829313
3503.402926	525504.152374	43.834317
3503.908651	525500.635509	43.839322
3503.751488	525496.970704	43.844327
3504.010481	525471.051672	43.849332
3503.630491	525471.111733	43.854337
3503.782710	525466.134440	43.859341
3503.836069	525467.895019	43.864346
3503.459887	525438.133959	43.869351
3503.757982	525423.227106	43.874356
3503.352348	525429.861854	43.879361
3503.467523	525429.742563	43.884365
3503.789311	525423.879219	43.889370
3503.509602	525430.241347	43.894375
3503.533807	525412.244087	43.899380
3503.547511	525403.194654	43.904385
3503.653291	525387.560013	43.909389
3503.881871	525398.542355	43.914394
3503.652693	525406.513895	43.919399
3503.517807	525395.365120	43.924404
3503.475568	525407.148413	43.929409
3503.640769	525392.313079	43.934413
3503.652266	525362.237884	43.939418
3503.707538	525363.947629	43.944423
3503.967380	525355.415243	43.949428
3503.811830	525365.447452	43.954433
3503.788889	525332.799925	43.959437
3503.700994	525318.813225	43.964442
3503.856463	525320.304963	43.969447
3504.032150	525311.735312	43.974452
3503.773258	525292.569615	43.979457
3503.955196	525270.099414	43.984461
3504.041041	525270.742915	43.989466
3503.833766	525272.746887	43.994471
3503.694233	525240.471407	43.999476
3503.792609	525244.600459	44.004481
3503.895191	525237.609185	44.009485
3503.825269	525237.215885	44.014490
3503.384077	525220.505025	44.019495
3503.815247	525202.089398	44.024500
3503.845725	525202.438390	44.029505
3503.859844	525198.139914	44.034509
3503.966038	525185.992551	44.039514
3503.670010	525172.139709	44.044519
3503.822168	525157.761118	44.049524
3503.743104	525149.383279	44.054529
3503.841981	525146.739352	44.059533
3503.834457	525134.407747	44.064538
3503.756356	525120.773137	44.069543
3504.093572	525110.206619	44.074548
3503.717545	525118.504778	44.079553
3503.695170	525104.305359	44.084557
3503.800858	525081.846946	44.089562
3503.691974	525082.571778	44.094567
3503.480893	525081.796431	44.099572
3503.555906	525079.863887	44.104577
3503.840149	525066.323592	44.109581
3503.590888	525050.289840	44.114586
3503.803015	525041.259384	44.119591
3503.906453	525030.123231	44.124596
3503.654245	525030.264184	44.129601
3503.999791	525012.771676	44.134605
3503.689038	524996.545411	44.139610
3503.765721	524987.334155	44.144615
3503.721136	524993.810925	44.149620
3503.596684	524994.386588	44.154625
3503.573810	524982.208927	44.159629
3503.585013	524956.378775	44.164634
3503.698150	524950.800962	44.169639
3503.976834	524942.518104	44.174644
3503.726156	524949.836185	44.179649
3503.417647	524945.083187	44.184653
3503.588900	524925.191980	44.189658
3503.400056	524917.943359	44.194663
3503.384610	524912.234222	44.199668
3503.626748	524914.066113	44.204673
3503.796238	524907.923384	44.209677
3503.911576	524905.024091	44.214682
3503.109798	524903.280655	44.219687
3503.699662	524889.691906	44.224692
3503.543344	524886.330096	44.229697
3503.492372	524876.532413	44.234701
3503.855826	524866.719765	44.239706
3503.606915	524877.373575	44.244711
3503.605057	524858.672184	44.249716
3503.729868	524881.296657	44.254721
3503.677197	524841.475430	44.259725
3503.681089	524844.760252	44.264730
3503.617193	524844.416535	44.269735
3503.869723	524829.870151	44.274740
3503.727596	524841.720192	44.279745
3503.763362	524806.838328	44.284749
3503.695353	524797.852014	44.289754
3503.280413	524792.003796	44.294759
3503.531045	524790.144550	44.299764
3503.742818	524793.042707	44.304769
3504.060742	524798.097534	44.309773
3504.126321	524775.645033	44.314778
3503.854918	524788.728636	44.319783
3503.994005	524765.354686	44.324788
3503.831780	524741.826145	44.329793
3503.492400	524739.857967	44.334797
3503.919105	524719.976675	44.339802
3503.750647	524731.527686	44.344807
3503.940831	524722.197247	44.349812
3503.465731	524705.592299	44.354817
3503.751085	524691.950423	44.359821
3503.717064	524686.850689	44.364826
3503.605932	524694.146829	44.369831
3504.197595	524674.037225	44.374836
3503.695935	524653.999313	44.379841
3503.265313	524650.074261	44.384845
3503.904372	524638.853177	44.389850
3503.682116	524641.718872	44.394855
3504.008804	524639.190492	44.399860
3503.788041	524626.184560	44.404865
3503.665172	524607.906370	44.409869
3503.676618	524603.860888	44.414874
3503.608514	524613.374285	44.419879
3503.635320	524590.169464	44.424884
3503.437972	524585.044968	44.429889
3503.555414	524566.930932	44.434893
3503.857619	524571.432310	44.439898
3503.764907	524567.908741	44.444903
3503.658057	524564.286315	44.449908
3503.532644	524549.546685	44.454913
3503.559588	524529.930528	44.459917
3503.804127	524526.859107	44.464922
3503.480190	524525.545562	44.469927
3503.888624	524508.345844	44.474932
3504.118237	524517.761694	44.479937
3503.910938	524492.268610	44.484941
3503.862835	524485.401918	44.489946
3503.704587	524488.762987	44.494951
3504.043739	524476.527721	44.499956
3503.565594	524464.219441	44.504961
3503.499884	524449.217550	44.509965
3503.674080	524451.767884	44.514970
3503.563416	524445.062703	44.519975
3503.698280	524440.744940	44.524980
3503.474792	524426.172337	44.529985
3503.822466	524406.404243	44.534989
3503.879188	524398.004549	44.539994
3503.592445	524404.267099	44.544999
3503.908530	524389.002619	44.550004
3503.772705	524388.771355	44.555009
3503.537929	524360.603435	44.560013
3503.722787	524356.176654	44.565018
3503.550490	524364.999012	44.570023
3503.886911	524360.699917	44.575028
3503.869692	524346.600106	44.580033
3503.610768	524320.205067	44.585037
3503.598703	524310.956904	44.590042
3503.908443	524314.800054	44.595047
3503.883545	524307.272510	44.600052
3503.425588	524300.773802	44.605057
3503.507534	524290.550377	44.610061
3503.825395	524271.646127	44.615066
3503.588733	524288.111292	44.620071
3503.648363	524273.089425	44.625076
3503.753400	524286.113935	44.630081
3503.752803	524259.172496	44.635085
3503.894947	524248.888984	44.640090
3503.437057	524249.567922	44.645095
3503.877925	524229.431052	44.650100
3503.743261	524242.948408	44.655105
3503.739344	524220.405023	44.660109
3503.869752	524200.367735	44.665114
3503.610232	524199.246169	44.670119
3503.742198	524203.117445	44.675124
3503.561888	524204.460172	44.680129
3503.566572	524177.113383	44.685133
3503.598861	524169.020715	44.690138
3503.449091	524169.347672	44.695143
3503.545619	524158.869123	44.700148
3503.628088	524159.563751	44.705153
3503.429615	524163.740001	44.710157
3503.507119	524155.185254	44.715162
3503.484153	524164.034666	44.720167
3503.501198	524146.441499	44.725172
3503.367740	524140.093625	44.730177
3503.211928	524132.485596	44.735181
3503.096460	524125.781041	44.740186
3503.298546	524134.493803	44.745191
3503.748327	524119.207936	44.750196
3503.411944	524128.208001	44.755201
3503.454699	524130.526425	44.760205
3503.516150	524136.481306	44.765210
3503.570930	524131.973929	44.770215
3503.523282	524134.862663	44.775220
3503.480442	524105.147536	44.780225
3503.317410	524097.085704	44.785229
3503.404582	524082.109854	44.790234
3503.402730	524089.035162	44.795239
3503.491782	524088.616707	44.800244
3503.629563	524085.258791	44.805249
3503.330517	524081.363349	44.810253
3503.492906	524092.306501	44.815258
3503.275267	524091.026665	44.820263
3503.379849	524087.016879	44.825268
3503.480520	524097.161022	44.830273
3503.156346	524085.131400	44.835277
3503.580750	524070.001141	44.840282
3503.213482	524070.413025	44.845287
3503.760851	524046.518570	44.850292
3503.695752	524061.288775	44.855297
3503.377570	524056.638137	44.860301
3503.605818	524057.360275	44.865306
3503.595083	524056.856496	44.870311
3503.518364	524059.800386	44.875316
3503.535808	524040.336777	44.880321
3503.346644	524023.129903	44.885325
3503.570137	524008.587368	44.890330
3503.284485	524026.172594	44.895335
3503.866130	524008.894419	44.900340
3503.793346	524017.903428	44.905345
3503.322899	524012.923010	44.910349
3503.600117	524023.949154	44.915354
3503.533166	524004.498842	44.920359
3503.428884	523988.441114	44.925364
3503.560813	523989.835602	44.930369
3503.409890	523990.011101	44.935373
3503.456316	523980.753503	44.940378
3503.263193	523985.687172	44.945383
3503.594358	523997.260834	44.950388
3503.305515	523987.399111	44.955393
3503.224192	523982.761561	44.960397
3503.359512	523982.184147	44.965402
3503.484164	523992.071826	44.970407
3503.520478	523981.046652	44.975412
3503.422190	523960.337543	44.980417
3503.424926	523953.664780	44.985421
3503.256264	523947.170750	44.990426
3503.131841	523949.920008	44.995431
3503.524586	523936.867095	45.000436
3503.413821	523958.165306	45.005441
3503.051153	523955.088656	45.010445
3503.443129	523949.213684	45.015450
3503.267124	523951.313971	45.020455
3503.474435	523947.995585	45.025460
3503.730100	523956.548331	45.030465
3503.678061	523955.646693	45.035469
3503.991133	523936.085685	45.040474
3503.552247	523931.706828	45.045479
3503.589057	523916.132208	45.050484
3503.545792	523907.950255	45.055489
3503.510237	523912.454656	45.060493
3503.626146	523897.929026	45.065498
3503.537446	523901.936349	45.070503
3503.641321	523886.654388	45.075508
3503.597243	523876.855006	45.080513
3503.573299	523878.324689	45.085517
3503.997865	523872.444538	45.090522
3503.546444	523874.082885	45.095527
3503.658958	523850.459066	45.100532
3503.639004	523847.783161	45.105537
3503.533068	523839.611079	45.110541
3503.653242	523828.117611	45.115546
3503.700586	523838.674732	45.120551
3503.556784	523833.440435	45.125556
3503.656186	523836.963108	45.130561
3503.334076	523810.728866	45.135565
3503.836259	523789.469691	45.140570
3503.709702	523796.718127	45.145575
3503.762378	523786.852848	45.150580
3503.760405	523783.516960	45.155585
3503.703947	523776.651286	45.160589
3503.457274	523750.051182	45.165594
3503.354642	523758.711214	45.170599
3503.709912	523746.422300	45.175604
3503.394214	523759.210446	45.180609
3503.420177	523750.259242	45.185613
3503.795089	523750.301081	45.190618
3503.577544	523743.814695	45.195623
3503.572607	523720.916932	45.200628
3503.634900	523717.368678	45.205633
3503.666010	523708.214442	45.210637
3503.822619	523713.042367	45.215642
3503.469190	523707.992808	45.220647
3503.649216	523701.393017	45.225652
3503.444273	523688.788216	45.230657
3503.634755	523670.459433	45.235661
3503.850588	523665.623178	45.240666
3503.504928	523680.134783	45.245671
3503.507571	523665.374102	45.250676
3503.656259	523678.088912	45.255681
3503.267052	523660.155036	45.260685
3503.394610	523631.776924	45.265690
3503.273306	523636.446602	45.270695
3503.117924	523624.389956	45.275700
3503.262886	523631.039511	45.280705
3503.225670	523637.111270	45.285709
3503.612397	523630.327131	45.290714
3503.554608	523636.553789	45.295719
3503.652356	523640.683354	45.300724
3503.516293	523650.309158	45.305729
3503.450717	523635.104292	45.310733
3503.690172	523644.165255	45.315738
3503.433650	523633.438874	45.320743
3503.351748	523597.713658	45.325748
3503.276574	523607.178216	45.330753
3503.122230	523603.360883	45.335757
3503.180975	523596.325277	45.340762
3503.008601	523602.418412	45.345767
3503.217762	523601.677666	45.350772
3503.040010	523596.297010	45.355777
3503.048239	523599.025360	45.360781
3503.564002	523609.407496	45.365786
3503.429525	523611.248517	45.370791
3503.562544	523600.864936	45.375796
3503.233131	523595.508251	45.380801
3503.254961	523603.895948	45.385805
3503.683808	523608.933620	45.390810
3503.018823	523615.458455	45.395815
3503.417644	523611.553692	45.400820
3503.427273	523603.615969	45.405825
3503.377372	523609.285351	45.410829
3503.524115	523610.070942	45.415834
3503.324114	523614.348674	45.420839
3503.575370	523603.946406	45.425844
3503.610813	523584.428854	45.430849
3503.210140	523579.437271	45.435853
3503.436791	523564.539993	45.440858
3503.278598	523572.248472	45.445863
3503.605105	523573.157300	45.450868
3503.487610	523577.118705	45.455873
3503.404755	523584.613074	45.460877
3503.728701	523560.601569	45.465882
3503.658950	523569.761997	45.470887
3503.847134	523558.712530	45.475892
3503.657953	523548.177645	45.480897
3503.448472	523548.463502	45.485901
3503.634156	523565.570336	45.490906
3503.611231	523587.967233	45.495911
3503.825684	523582.372933	45.500916
3503.551721	523569.273457	45.505921
3503.783104	523549.421597	45.510925
3503.779113	523535.217887	45.515930
3503.524044	523567.862456	45.520935
3503.336391	523555.962506	45.525940
3503.496233	523567.917402	45.530945
3503.591776	523543.739776	45.535949
3503.811919	523522.878676	45.540954
3503.389102	523510.611468	45.545959
3504.000597	523502.224720	45.550964
3503.715874	523521.882871	45.555969
3503.424170	523500.849898	45.560973
3503.788746	523471.928548	45.565978
3503.358493	523482.005347	45.570983
3503.432149	523470.417879	45.575988
3503.322676	523466.340674	45.580993
3503.098979	523472.340871	45.585997
3503.343039	523468.409985	45.591002
3503.422518	523470.469952	45.596007
3503.421240	523461.017399	45.601012
3503.212024	523459.635081	45.606017
3503.622486	523477.970218	45.611021
3503.760543	523474.511034	45.616026
3503.204028	523467.016574	45.621031
3503.159517	523450.595017	45.626036
3503.509090	523455.796916	45.631041
3503.422791	523447.621531	45.636045
3503.360578	523450.108293	45.641050
3503.546728	523450.685465	45.646055
3503.729221	523453.639043	45.651060
3503.562388	523453.867612	45.656065
3503.704352	523454.300119	45.661069
3504.074275	523446.709768	45.666074
3503.711611	523432.865957	45.671079
3503.567995	523414.690791	45.676084
3503.775490	523410.462373	45.681089
3503.485447	523416.978574	45.686093
3503.876830	523389.215481	45.691098
3503.650124	523380.152360	45.696103
3503.782542	523363.399450	45.701108
3503.680232	523368.723351	45.706113
3503.521157	523372.388080	45.711117
3503.610265	523354.479361	45.716122
3503.720261	523349.861939	45.721127
3503.708610	523330.806473	45.726132
3503.831403	523321.991377	45.731137
3503.408644	523322.614248	45.736141
3503.416457	523327.870207	45.741146
3503.656425	523318.429989	45.746151
3503.604927	523308.479784	45.751156
3503.327981	523295.784957	45.756161
3503.279630	523282.649587	45.761165
3503.718672	523281.417541	45.766170
3503.657986	523289.818443	45.771175
3503.376684	523281.825447	45.776180
3503.746370	523293.899028	45.781185
3503.645706	523285.018130	45.786189
3503.683201	523261.759159	45.791194
3503.603233	523258.233290	45.796199
3503.350962	523237.901443	45.801204
3503.571428	523244.084271	45.806209
3503.111763	523231.317173	45.811213
3503.548902	523232.966787	45.816218
3503.855767	523244.645932	45.821223
3503.876875	523227.859925	45.826228
3503.724758	523207.057257	45.831233
3503.631305	523197.063065	45.836237
3503.805893	523192.688141	45.841242
3503.665515	523207.268823	45.846247
3503.892820	523179.986259	45.851252
3503.844266	523171.905870	45.856257
3503.565951	523160.019958	45.861261
3503.975122	523152.777119	45.866266
3503.926430	523156.929954	45.871271
3503.634187	523138.929622	45.876276
3504.007170	523117.841640	45.881281
3503.856271	523124.942571	45.886285
3504.149817	523106.799063	45.891290
3503.508913	523105.636599	45.896295
3503.529045	523075.454667	45.901300
3503.545422	523072.166282	45.906305
3503.165560	523077.736352	45.911309
3503.531655	523062.968224	45.916314
3503.217247	523076.969923	45.921319
3503.137522	523066.114118	45.926324
3503.396982	523084.423018	45.931329
3503.241159	523073.983652	45.936333
3503.643669	523066.387973	45.941338
3503.191876	523076.822283	45.946343
3503.391247	523079.520509	45.951348
3503.140566	523052.667135	45.956353
3502.862544	523047.302145	45.961357
3503.256525	523065.286500	45.966362
3503.541384	523073.279043	45.971367
3503.355691	523058.092619	45.976372
3503.225695	523053.462495	45.981377
3503.089987	523043.879293	45.986381
3503.886011	523048.960208	45.991386
3503.443992	523057.876461	45.996391
3503.280089	523040.057935	46.001396
3503.438226	523052.064033	46.006401
3503.265653	523052.445166	46.011405
3503.747077	523037.001626	46.016410
3503.379467	523044.895108	46.021415
3503.470672	523049.126961	46.026420
3503.776031	523052.010642	46.031425
3503.416161	523017.794052	46.036429
3503.831656	523008.881970	46.041434
3503.498304	523015.506279	46.046439
3503.608809	523010.433722	46.051444
3503.765996	523009.953919	46.056449
3503.724815	523005.259192	46.061453
3503.772098	522991.855716	46.066458
3503.692883	522996.367273	46.071463
3503.705423	522977.054812	46.076468
3503.629440	522980.150435	46.081473
3503.446105	522980.381617	46.086477
3503.778493	522973.959651	46.091482
3503.552178	522955.443183	46.096487
3503.652947	522933.791375	46.101492
3503.772067	522943.832225	46.106497
3503.487015	522944.686098	46.111501
3503.672578	522935.709217	46.116506
3503.752401	522924.272036	46.121511
3503.760270	522897.478641	46.126516
3503.650861	522890.772614	46.131521
3503.665927	522903.711359	46.136525
3503.656219	522902.600766	46.141530
3503.247215	522903.272029	46.146535
3503.404614	522876.202207	46.151540
3503.589672	522856.912886	46.156545
3503.404841	522842.636048	46.161549
3503.453052	522844.599935	46.166554
3503.435330	522865.126607	46.171559
3503.443821	522856.379875	46.176564
3503.454850	522860.877207	46.181569
3503.383706	522849.362732	46.186573
3503.806614	522842.825304	46.191578
3503.470478	522847.023652	46.196583
3503.509825	522828.869460	46.201588
3503.769856	522819.729090	46.206593
3503.548911	522820.926698	46.211597
3503.675770	522816.710871	46.216602
3503.547414	522814.658547	46.221607
3503.651227	522817.826885	46.226612
3503.748867	522799.966756	46.231617
3503.583907	522793.876087	46.236621
3503.640895	522783.807310	46.241626
3503.294426	522783.407108	46.246631
3503.682318	522780.868769	46.251636
3503.683154	522785.620490	46.256641
3503.569239	522777.196373	46.261645
3503.499216	522767.147660	46.266650
3503.456296	522754.011003	46.271655
3503.620610	522745.896755	46.276660
3503.552883	522741.863320	46.281665
3503.789727	522741.269816	46.286669
3504.028056	522723.235710	46.291674
3503.969761	522709.343169	46.296679
3503.889664	522702.531327	46.301684
3503.780183	522699.414415	46.306689
3503.400605	522696.643505	46.311693
3503.898996	522670.682138	46.316698
3503.817877	522660.988977	46.321703
3503.685848	522654.690843	46.326708
3503.633887	522656.518929	46.331713
3503.455207	522657.608764	46.336717
3503.703102	522645.335989	46.341722
3503.237282	522627.969147	46.346727
3503.293185	522611.631971	46.351732
3503.654096	522609.148422	46.356737
3503.283449	522613.099523	46.361741
3503.778838	522614.790549	46.366746
3503.612507	522615.524569	46.371751
3503.678713	522613.643676	46.376756
3503.330242	522601.717889	46.381761
3503.188530	522596.482860	46.386765
3503.732193	522592.757169	46.391770
3503.379334	522579.568255	46.396775
3503.688154	522569.611197	46.401780
3503.677747	522570.826097	46.406785
3503.484884	522569.036699	46.411789
3503.608314	522570.331550	46.416794
3503.375959	522559.701739	46.421799
3503.386025	522569.456744	46.426804
3503.298089	522545.407733	46.431809
3503.569986	522545.819729	46.436813
3503.854059	522522.722932	46.441818
3503.586777	522536.212123	46.446823
3503.573886	522535.809742	46.451828
3503.879846	522523.224382	46.456833
3503.517545	522518.327508	46.461837
3503.923510	522498.851188	46.466842
3503.628704	522497.077894	46.471847
3503.871811	522492.691952	46.476852
3503.982525	522487.619199	46.481857
3503.673047	522464.717241	46.486861
3503.399610	522457.784198	46.491866
3503.646244	522446.471972	46.496871
3503.532616	522448.057065	46.501876
3503.624589	522452.390058	46.506881
3503.310259	522453.299137	46.511885
3503.823532	522435.170701	46.516890
3503.507134	522418.639412	46.521895
3503.463542	522408.737958	46.526900
3503.584513	522408.061651	46.531905
3503.254525	522410.540343	46.536909
3503.614124	522399.917969	46.541914
3503.681753	522401.575523	46.546919
3503.334774	522416.189572	46.551924
3503.441653	522403.635587	46.556929
3503.126473	522399.186204	46.561933
3503.321224	522403.502964	46.566938
3503.511066	522388.357661	46.571943
3503.529220	522366.869812	46.576948
3503.476004	522367.434306	46.581953
3503.587084	522376.364614	46.586957
3503.566595	522365.953953	46.591962
3503.247825	522372.323453	46.596967
3503.255925	522371.766091	46.601972
3503.465992	522360.156268	46.606977
3503.487677	522374.459319	46.611981
3503.119878	522368.400551	46.616986
3503.110715	522376.591571	46.621991
3503.296383	522365.238372	46.626996
3503.630063	522371.100323	46.632001
3503.332394	522364.171069	46.637005
3503.672814	522345.261008	46.642010
3503.532491	522341.087288	46.647015
3503.270954	522342.392452	46.652020
3502.944695	522346.184943	46.657025
3503.084813	522340.551413	46.662029
3503.564681	522332.842060	46.667034
3503.191278	522345.084357	46.672039
3503.256919	522346.590572	46.677044
3503.348925	522350.873033	46.682049
3502.940973	522342.040188	46.687053
3503.102856	522349.951421	46.692058
3503.533034	522360.246785	46.697063
3503.389109	522355.517557	46.702068
3503.463988	522353.786921	46.707073
3503.253658	522357.257768	46.712077
3503.545881	522345.230524	46.717082
3503.505618	522361.616051	46.722087
3503.336880	522353.655355	46.727092
3503.624421	522347.139125	46.732097
3503.260140	522333.850710	46.737101
3503.594125	522313.930568	46.742106
3503.024524	522310.128011	46.747111
3503.341907	522314.728731	46.752116
3503.675012	522315.131058	46.757121
3503.578715	522309.130461	46.762125
3503.749698	522301.672128	46.767130
3503.396200	522300.211408	46.772135
3503.606347	522299.874874	46.777140
3503.624780	522289.356905	46.782145
3503.339186	522283.436772	46.787149
3503.328581	522264.379886	46.792154
3503.610112	522278.995822	46.797159
3503.532999	522271.778902	46.802164
3503.722624	522272.153356	46.807169
3503.663875	522271.606557	46.812173
3503.824017	522268.548052	46.817178
3503.697612	522254.362567	46.822183
3503.353243	522240.969821	46.827188
3503.919169	522247.502855	46.832193
3503.730350	522238.635317	46.837197
3503.826090	522233.463745	46.842202
3503.582489	522215.505249	46.847207
3503.584612	522205.646999	46.852212
3503.610762	522183.753217	46.857217
3503.555066	522154.845394	46.862221
3503.762461	522144.752447	46.867226
3503.434442	522144.248204	46.872231
3503.588760	522126.277269	46.877236
3503.678716	522096.638570	46.882241
3503.293241	522103.119825	46.887245
3503.498088	522101.318067	46.892250
3503.473439	522107.337859	46.897255
3503.055131	522102.803586	46.902260
3503.351662	522103.868900	46.907265
3503.241031	522110.407818	46.912269
3503.612753	522100.086655	46.917274
3503.363038	522106.900327	46.922279
3503.264322	522105.197104	46.927284
3503.622438	522099.984018	46.932289
3503.463075	522098.391487	46.937293
3503.735152	522072.262721	46.942298
3503.415224	522073.425473	46.947303
3503.474952	522070.281695	46.952308
3503.334607	522061.709721	46.957313
3503.365333	522059.783818	46.962317
3503.717955	522073.023749	46.967322
3503.449507	522066.443626	46.972327
3503.356415	522072.676464	46.977332
3503.368255	522077.527761	46.982337
3503.352265	522069.795552	46.987341
3503.207864	522049.647377	46.992346
3503.222521	522039.787044	46.997351
3503.422513	522022.870408	47.002356
3503.319639	522031.581954	47.007361
3503.195410	522027.708934	47.012365
3503.353446	522025.307918	47.017370
3503.052625	522023.788292	47.022375
3503.138468	522023.168076	47.027380
3503.322440	522027.992181	47.032385
3503.399796	522030.103222	47.037389
3503.479624	522031.000576	47.042394
3503.677280	522032.182630	47.047399
3503.511364	522036.404834	47.052404
3503.919107	522024.359095	47.057409
3503.156837	522037.775274	47.062413
3503.497858	522026.498392	47.067418
3503.302604	522022.636597	47.072423
3503.173973	522004.861912	47.077428
3503.233969	521986.754068	47.082433
3503.241048	521993.122766	47.087437
3503.336004	521989.771188	47.092442
3503.078894	521988.800745	47.097447
3503.423114	521983.438156	47.102452
3503.670625	521988.201676	47.107457
3503.434788	521987.278425	47.112461
3503.614990	521997.815748	47.117466
3503.722244	521992.288400	47.122471
3503.493475	521997.430522	47.127476
3503.662405	521992.449522	47.132481
3503.310647	521960.504349	47.137485
3503.716956	521951.896468	47.142490
3503.217409	521960.316871	47.147495
3503.237728	521947.573998	47.152500
3503.198365	521946.771353	47.157505
3502.932125	521947.925628	47.162509
3503.371401	521950.131137	47.167514
3502.983637	521948.372475	47.172519
3503.393962	521945.072149	47.177524
3503.491603	521944.298402	47.182529
3503.686509	521952.811261	47.187533
3503.857419	521947.678271	47.192538
3503.378896	521949.877184	47.197543
3503.589759	521947.821686	47.202548
3503.680652	521942.398017	47.207553
3503.594701	521921.987674	47.212557
3503.618280	521910.002571	47.217562
3503.553071	521908.799574	47.222567
3503.444141	521911.496172	47.227572
3503.823785	521916.390492	47.232577
3503.862430	521905.312982	47.237581
3503.760503	521877.776942	47.242586
3503.140995	521875.852684	47.247591
3503.138030	521867.056675	47.252596
3503.684014	521862.976573	47.257601
3503.468391	521878.581432	47.262605
3503.636802	521865.208434	47.267610
3503.528040	521868.916103	47.272615
3503.730931	521858.368700	47.277620
3503.883754	521848.991958	47.282625
3503.741052	521839.560813	47.287629
3503.551281	521821.694482	47.292634
3503.877012	521834.534421	47.297639
3503.427099	521827.881774	47.302644
3503.534414	521794.094302	47.307649
3503.811825	521785.203379	47.312653
3503.448842	521781.974694	47.317658
3503.318444	521791.246821	47.322663
3503.481662	521782.576164	47.327668
3503.643514	521793.065966	47.332673
3503.248910	521794.392205	47.337677
3503.400491	521787.846688	47.342682
3503.961094	521779.972650	47.347687
3503.369916	521766.770186	47.352692
3503.737048	521752.961248	47.357697
3503.257555	521754.098689	47.362701
3503.517486	521746.373268	47.367706
3503.615462	521746.357783	47.372711
3503.335129	521744.177679	47.377716
3503.348707	521756.207586	47.382721
3503.382339	521760.954424	47.387725
3503.695805	521735.728562	47.392730
3503.449829	521723.583709	47.397735
3503.055692	521715.658326	47.402740
3503.331914	521705.402563	47.407745
3503.547200	521714.367320	47.412749
3503.448240	521702.906983	47.417754
3503.299157	521711.373229	47.422759
3503.324400	521708.892046	47.427764
3503.292176	521710.565454	47.432769
3502.884833	521714.421461	47.437773
3503.421217	521713.173917	47.442778
3503.606343	521710.869683	47.447783
3503.533035	521714.976222	47.452788
3503.591099	521710.872093	47.457793
3503.184518	521709.773593	47.462797
3503.195651	521709.367395	47.467802
3503.307276	521697.216554	47.472807
3503.521486	521700.215997	47.477812
3503.271170	521692.116205	47.482817
3503.154572	521689.657438	47.487821
3503.320531	521680.632409	47.492826
3503.344065	521688.970273	47.497831
3503.395189	521696.646556	47.502836
3503.393169	521688.001967	47.507841
3503.509999	521691.067358	47.512845
3503.296598	521689.382217	47.517850
3503.545795	521700.768263	47.522855
3503.554061	521691.414280	47.527860
3503.724314	521674.299762	47.532865
3503.405403	521680.568443	47.537869
3503.802305	521649.818758	47.542874
3503.753242	521649.472628	47.547879
3503.611234	521648.483971	47.552884
3503.629547	521642.262791	47.557889
3503.499987	521646.782680	47.562893
3503.571832	521636.356957	47.567898
3503.611170	521608.090359	47.572903
3503.423224	521608.979506	47.577908
3503.566932	521609.614011	47.582913
3503.277742	521606.929735	47.587917
3503.392518	521602.664949	47.592922
3503.675093	521602.721397	47.597927
3503.222981	521601.933418	47.602932
3503.489777	521606.592891	47.607937
3503.359300	521604.591303	47.612941
3503.208845	521627.162731	47.617946
3503.646428	521632.250200	47.622951
3503.648145	521617.942798	47.627956
3503.998537	521600.698620	47.632961
3503.683575	521605.096159	47.637965
3503.783314	521604.625397	47.642970
3503.691301	521596.247759	47.647975
3503.633985	521567.895258	47.652980
3503.698646	521559.492838	47.657985
3503.384302	521578.146914	47.662989
3503.472935	521561.904620	47.667994
3503.752072	521557.361067	47.672999
3503.243598	521571.394733	47.678004
3503.336368	521563.442870	47.683009
3503.051323	521568.088468	47.688013
3503.267908	521557.993705	47.693018
3503.516619	521543.849420	47.698023
3503.441574	521533.497404	47.703028
3503.647513	521521.179859	47.708033
3503.572729	521528.471678	47.713037
3503.578026	521524.881398	47.718042
3503.329607	521531.947882	47.723047
3503.579262	521526.498981	47.728052
3503.558834	521525.491099	47.733057
3503.389038	521527.995159	47.738061
3503.483263	521496.635804	47.743066
3503.630564	521488.978620	47.748071
3503.099944	521483.400256	47.753076
3503.548935	521467.404244	47.758081
3503.516150	521476.256676	47.763085
3503.523290	521468.924970	47.768090
3503.443591	521473.538137	47.773095
3503.674842	521463.693777	47.778100
3503.896364	521459.412081	47.783105
3503.319233	521452.779387	47.788109
3503.445375	521427.178211	47.793114
3503.489213	521427.221838	47.798119
3503.578630	521424.983248	47.803124
3503.440654	521427.381182	47.808129
3503.307152	521432.811758	47.813133
3503.558306	521422.559780	47.818138
3503.420872	521423.188174	47.823143
3503.359740	521436.696246	47.828148
3503.697959	521422.386041	47.833153
3503.201851	521411.038827	47.838157
3503.403233	521389.166835	47.843162
3503.732105	521393.766002	47.848167
3503.499688	521401.588353	47.853172
3503.609593	521405.969347	47.858177
3503.585748	521398.743619	47.863181
3503.758725	521396.491817	47.868186
3503.772726	521374.649423	47.873191
3503.546980	521369.831727	47.878196
3504.032386	521359.744908	47.883201
3503.233451	521365.735690	47.888205
3503.461476	521355.082877	47.893210
3503.451779	521364.083388	47.898215
3503.364321	521365.260001	47.903220
3503.461565	521335.972658	47.908225
3503.597400	521326.699414	47.913229
3503.420621	521315.099435	47.918234
3503.325847	521302.677587	47.923239
3503.265992	521306.023759	47.928244
3503.528387	521298.044957	47.933249
3503.573203	521314.013640	47.938253
3503.427022	521300.993241	47.943258
3503.712515	521303.273704	47.948263
3503.334141	521282.858223	47.953268
3503.425224	521259.739584	47.958273
3503.425148	521264.289668	47.963277
3503.372783	521262.932924	47.968282
3503.414285	521257.971841	47.973287
3503.298994	521267.140765	47.978292
3503.359812	521268.041167	47.983297
3503.344548	521267.436904	47.988301
3503.265330	521268.157214	47.993306
3503.317714	521266.328907	47.998311
3503.298187	521256.675728	48.003316
3503.140290	521257.610701	48.008321
3503.004597	521269.209554	48.013325
3503.128727	521269.442717	48.018330
3503.152525	521259.024347	48.023335
3503.058518	521261.263686	48.028340
3503.514017	521261.040021	48.033345
3503.538973	521263.108888	48.038349
3503.491351	521266.908142	48.043354
3503.609403	521271.287885	48.048359
3503.477799	521254.220637	48.053364
3503.575046	521244.548995	48.058369
3503.259702	521233.071972	48.063373
3503.449889	521228.795169	48.068378
3503.533798	521232.371416	48.073383
3503.478222	521229.549039	48.078388
3503.706954	521224.153900	48.083393
3503.413299	521226.020349	48.088397
3503.617081	521229.628205	48.093402
3503.269212	521238.631681	48.098407
3503.142229	521237.033946	48.103412
3503.550437	521231.559886	48.108417
3503.167624	521209.324982	48.113421
3503.451681	521196.691505	48.118426
3503.390890	521184.365308	48.123431
3503.193232	521190.160002	48.128436
3503.855701	521174.787198	48.133441
3503.657509	521174.110731	48.138445
3503.396342	521168.843564	48.143450
3503.281835	521192.016593	48.148455
3503.487742	521182.277182	48.153460
3503.573823	521177.814594	48.158465
3503.144883	521184.960318	48.163469
3502.991785	521180.838876	48.168474
3503.592459	521179.025009	48.173479
3503.118054	521170.555923	48.178484
3503.662687	521146.050962	48.183489
3503.365386	521145.845170	48.188493
3502.966241	521134.431880	48.193498
3503.157056	521139.962962	48.198503
3503.447281	521144.568309	48.203508
3503.376444	521137.653234	48.208513
3502.956456	521147.375953	48.213517
3503.283099	521138.578010	48.218522
3503.341513	521150.399051	48.223527
3503.147592	521150.530816	48.228532
3503.538953	521158.558029	48.233537
3503.220319	521150.165425	48.238541
3503.093481	521151.196607	48.243546
3503.242659	521148.291296	48.248551
3503.345989	521146.808820	48.253556
3503.380932	521142.607089	48.258561
3503.419047	521159.234221	48.263565
3503.580803	521143.283293	48.268570
3503.802422	521150.882328	48.273575
3503.126478	521147.753539	48.278580
3503.335447	521133.059056	48.283585
3503.203915	521136.770489	48.288589
3503.073590	521119.349002	48.293594
3503.248389	521118.765248	48.298599
3503.443016	521124.851858	48.303604
3503.393521	521111.866583	48.308609
3503.497914	521110.990617	48.313613
3503.395872	521108.630575	48.318618
3503.444620	521113.577440	48.323623
3502.941195	521120.279953	48.328628
3503.174683	521108.311640	48.333633
3503.293007	521110.062427	48.338637
3503.149301	521105.636140	48.343642
3503.243606	521111.182487	48.348647
3503.207818	521117.305519	48.353652
3503.613882	521106.219949	48.358657
3503.468412	521118.073239	48.363661
3503.296711	521111.123538	48.368666
3503.396575	521118.691276	48.373671
3503.436694	521118.988276	48.378676
3503.607677	521111.529400	48.383681
3503.121024	521120.352649	48.388685
3503.403608	521113.432258	48.393690
3503.271826	521109.610769	48.398695
3503.079836	521101.754248	48.403700
3503.248869	521100.413053	48.408705
3503.343427	521108.739987	48.413709
3503.165793	521094.005462	48.418714
3503.493330	521100.627199	48.423719
3503.371936	521091.192251	48.428724
3503.564144	521093.032476	48.433729
3503.549677	521095.967062	48.438733
3503.705297	521091.847358	48.443738
3503.680231	521099.131510	48.448743
3503.314412	521098.936548	48.453748
3503.886139	521078.320081	48.458753
3503.579802	521059.207414	48.463757
3503.495641	521047.794833	48.468762
3503.637936	521047.721786	48.473767
3503.534892	521054.158814	48.478772
3503.392497	521040.783710	48.483777
3503.245067	521047.379428	48.488781
3503.633865	521042.515057	48.493786
3503.563517	521040.554452	48.498791
3503.363762	521022.941607	48.503796
3503.693445	521004.790045	48.508801
3503.338060	521001.762231	48.513805
3503.471671	521007.251843	48.518810
3503.456353	520995.019430	48.523815
3503.389920	520995.990517	48.528820
3503.553213	521003.346055	48.533825
3503.281859	521004.652875	48.538829
3503.361887	520996.702750	48.543834
3503.613738	521005.965462	48.548839
3503.061615	520988.661061	48.553844
3503.725680	520965.805340	48.558849
3503.384853	520973.948374	48.563853
3503.469738	520967.817529	48.568858
3503.713656	520973.593061	48.573863
3503.279841	520969.768721	48.578868
3503.558256	520971.696449	48.583873
3503.609095	520970.626711	48.588877
3503.831559	520955.424363	48.593882
3503.869006	520932.869869	48.598887
3503.122381	520938.094175	48.603892
3503.655978	520933.156328	48.608897
3503.464149	520927.271435	48.613901
3503.464324	520924.794095	48.618906
3503.807567	520920.594135	48.623911
3503.539500	520924.832771	48.628916
3503.664354	520898.017590	48.633921
3503.459325	520894.409858	48.638925
3503.801429	520896.681431	48.643930
3503.656497	520887.148970	48.648935
3503.586262	520889.131815	48.653940
3503.647732	520881.134011	48.658945
3503.180371	520871.804177	48.663949
3503.297542	520849.034735	48.668954
3503.339778	520842.961142	48.673959
3503.417872	520840.471474	48.678964
3503.230835	520839.034865	48.683969
3503.396315	520843.710572	48.688973
3503.332615	520838.007625	48.693978
3503.150316	520845.215628	48.698983
3503.313800	520843.420270	48.703988
3503.399064	520840.828353	48.708993
3503.364814	520854.433773	48.713997
3503.245464	520849.497990	48.719002
3503.501112	520845.412972	48.724007
3503.272480	520861.425319	48.729012
3503.314172	520854.593452	48.734017
3503.055377	520855.544395	48.739021
3503.109974	520851.946175	48.744026
3503.491761	520839.347533	48.749031
3503.253347	520865.119050	48.754036
3503.132068	520860.891382	48.759041
3503.356387	520863.131018	48.764045
3503.210704	520854.104233	48.769050
3503.182406	520854.260380	48.774055
3503.197594	520856.886976	48.779060
3503.610740	520851.209778	48.784065
3503.514708	520866.645028	48.789069
3503.361887	520839.317507	48.794074
3503.312757	520823.247926	48.799079
3503.224799	520832.463332	48.804084
3503.260537	520821.992238	48.809089
3503.080627	520811.656338	48.814093
3503.036722	520829.762945	48.819098
3503.301786	520825.019183	48.824103
3503.266199	520823.558634	48.829108
3503.560061	520822.652706	48.834113
3503.104552	520823.533627	48.839117
3502.940451	520820.576660	48.844122
3503.294579	520823.301362	48.849127
3503.062932	520823.944669	48.854132
3503.211823	520818.309228	48.859137
3503.191928	520832.316860	48.864141
3503.240202	520831.651980	48.869146
3503.573094	520829.526498	48.874151
3503.318056	520827.948963	48.879156
3503.560230	520820.225913	48.884161
3503.284275	520832.302266	48.889165
3503.259793	520829.525462	48.894170
3503.386129	520830.213302	48.899175
3503.331670	520832.345333	48.904180
3503.510981	520822.711028	48.909185
3503.416546	520823.383205	48.914189
3503.521184	520826.248456	48.919194
3503.694840	520818.536235	48.924199
3503.313311	520808.282759	48.929204
3503.548024	520785.595766	48.934209
3503.535259	520793.232016	48.939213
3503.584271	520779.421981	48.944218
3503.860086	520787.821545	48.949223
3503.322767	520791.445522	48.954228
3503.392456	520781.120709	48.959233
3503.829924	520789.545280	48.964237
3503.784742	520753.251865	48.969242
3503.837227	520759.816100	48.974247
3503.440388	520748.705521	48.979252
3503.784327	520746.932189	48.984257
3503.462667	520753.252216	48.989261
3503.721920	520727.881694	48.994266
3503.766810	520719.684198	48.999271
3503.483830	520708.858945	49.004276
3503.815145	520710.070529	49.009281
3503.723036	520705.635978	49.014285
3503.668443	520690.881640	49.019290
3503.705940	520674.899338	49.024295
3503.463371	520674.684888	49.029300
3503.652207	520657.263018	49.034305
3503.300312	520659.391526	49.039309
3503.370011	520659.178277	49.044314
3503.740167	520662.304939	49.049319
3503.516976	520654.250900	49.054324
3503.535794	520643.782367	49.059329
3503.477684	520621.697571	49.064333
3503.383198	520629.094023	49.069338
3503.534122	520626.390577	49.074343
3503.400579	520624.288235	49.079348
3503.843746	520616.482762	49.084353
3503.584308	520626.635437	49.089357
3503.343881	520620.960348	49.094362
3503.651937	520584.307374	49.099367
3503.568946	520580.933075	49.104372
3503.010139	520570.909704	49.109377
3503.394316	520583.488602	49.114381
3503.713438	520574.691546	49.119386
3503.736587	520574.435095	49.124391
3502.964688	520580.927470	49.129396
3503.226557	520574.060684	49.134401
3503.575689	520577.392920	49.139405
3503.105555	520584.292623	49.144410
3503.392984	520576.360071	49.149415
3503.340852	520590.474122	49.154420
3503.311868	520589.770885	49.159425
3503.336211	520581.374335	49.164429
3503.315801	520573.692672	49.169434
3503.416107	520556.537481	49.174439
3503.234970	520547.111661	49.179444
3503.282602	520531.279292	49.184449
3503.101815	520529.234964	49.189453
3502.939951	520539.978975	49.194458
3503.501289	520527.503389	49.199463
3503.349706	520542.290463	49.204468
3503.443271	520535.349147	49.209473
3503.206222	520539.431304	49.214477
3503.282819	520535.728419	49.219482
3503.364455	520540.215232	49.224487
3503.313630	520548.868783	49.229492
3503.421892	520540.863416	49.234497
3503.234753	520545.594944	49.239501
3503.276401	520553.071030	49.244506
3503.588519	520534.315021	49.249511
3503.239674	520544.481879	49.254516
3503.513361	520540.596168	49.259521
3503.242480	520537.706585	49.264525
3503.178924	520541.912995	49.269530
3503.360765	520547.749048	49.274535
3503.151902	520545.203575	49.279540
3503.504920	520540.749180	49.284545
3503.343603	520547.498970	49.289549
3503.296256	520518.283573	49.294554
3503.511828	520505.609830	49.299559
3503.330633	520505.132883	49.304564
3503.479972	520504.199222	49.309569
3503.210860	520507.174163	49.314573
3503.416839	520502.389088	49.319578
3503.473473	520505.514777	49.324583
3503.452418	520504.506932	49.329588
3503.201992	520493.726948	49.334593
3503.674730	520510.741072	49.339597
3503.238003	520509.748369	49.344602
3503.699466	520498.906427	49.349607
3503.507775	520497.874992	49.354612
3503.650194	520471.663041	49.359617
3503.487879	520483.721689	49.364621
3503.374561	520468.066375	49.369626
3503.454677	520465.677447	49.374631
3502.987055	520476.368710	49.379636
3503.153858	520468.910201	49.384641
3503.049223	520479.341853	49.389645
3503.327094	520481.775313	49.394650
3503.828449	520471.887664	49.399655
3503.549086	520476.785465	49.404660
3503.669968	520471.811597	49.409665
3503.438488	520463.657657	49.414669
3503.448553	520440.500105	49.419674
3503.379082	520428.983652	49.424679
3503.068076	520434.038145	49.429684
3503.356207	520434.852105	49.434689
3503.325544	520435.109746	49.439693
3503.255508	520435.525288	49.444698
3503.620777	520432.130665	49.449703
3503.422995	520439.695206	49.454708
3503.462238	520439.739562	49.459713
3503.533513	520436.189173	49.464717
3503.333759	520435.664599	49.469722
3503.510228	520425.272125	49.474727
3503.362411	520437.834104	49.479732
3503.278715	520423.185243	49.484737
3503.401791	520397.481820	49.489741
3503.274181	520395.884101	49.494746
3503.613086	520390.976866	49.499751
3503.414045	520393.485720	49.504756
3503.465522	520378.158186	49.509761
3503.387117	520390.304757	49.514765
3503.080312	520385.196227	49.519770
3503.231636	520389.166475	49.524775
3503.204314	520388.159613	49.529780
3503.258326	520384.814178	49.534785
3503.531716	520392.455944	49.539789
3503.304908	520394.311919	49.544794
3503.258811	520392.954111	49.549799
3503.383195	520388.687491	49.554804
3503.366403	520380.904048	49.559809
3503.496669	520392.410926	49.564813
3503.626389	520376.262078	49.569818
3503.780386	520354.345632	49.574823
3503.496390	520355.502823	49.579828
3503.612279	520353.664376	49.584833
3503.666929	520345.869624	49.589837
3503.536276	520342.553368	49.594842
3503.272260	520343.505165	49.599847
3503.372256	520350.871002	49.604852
3503.331942	520333.788363	49.609857
3503.424824	520312.690469	49.614861
3503.419020	520321.488702	49.619866
3503.536051	520308.425908	49.624871
3503.448074	520308.490373	49.629876
3503.504466	520311.666697	49.634881
3503.358653	520313.914353	49.639885
3503.037102	520310.577705	49.644890
3503.110423	520314.054708	49.649895
3503.265895	520314.586287	49.654900
3503.370530	520313.659681	49.659905
3503.255307	520315.447469	49.664909
3503.098625	520311.376932	49.669914
3503.362008	520314.874453	49.674919
3503.065464	520317.954882	49.679924
3503.166201	520313.439183	49.684929
3503.571212	520311.858389	49.689933
3503.289463	520328.284128	49.694938
3503.422399	520319.920838	49.699943
3503.152961	520330.985344	49.704948
3503.458021	520315.010958	49.709953
3503.275222	520331.522172	49.714957
3503.668175	520312.449777	49.719962
3503.461731	520298.325799	49.724967
3503.536986	520289.061542	49.729972
3503.399944	520271.690771	49.734977
3503.368588	520289.138720	49.739981
3503.321429	520279.893807	49.744986
3503.603661	520280.152554	49.749991
3503.296561	520289.099546	49.754996
3503.430119	520275.680198	49.760001
3503.813724	520275.518447	49.765005
3503.622400	520256.841695	49.770010
3503.935080	520247.994923	49.775015
3503.426661	520240.744156	49.780020
3503.242349	520239.610419	49.785025
3503.757906	520235.736966	49.790029
3503.525569	520231.728927	49.795034
3503.726577	520227.197355	49.800039
3503.205844	520212.971301	49.805044
3503.378734	520191.860605	49.810049
3503.237772	520190.871693	49.815053
3502.631948	520196.073976	49.820058
3503.230557	520197.698389	49.825063
3503.421673	520204.038696	49.830068
3503.297188	520193.592525	49.835073
3503.223558	520192.491851	49.840077
3503.157983	520199.125532	49.845082
3503.434979	520186.745191	49.850087
3503.066432	520198.280489	49.855092
3503.330194	520186.963993	49.860097
3503.448777	520197.815579	49.865101
3503.290629	520207.042431	49.870106
3503.396919	520198.228254	49.875111
3503.433612	520198.020216	49.880116
3503.360874	520195.250933	49.885121
3503.255969	520195.014716	49.890125
3503.200914	520201.848971	49.895130
3503.491837	520204.128732	49.900135
3502.939146	520209.524851	49.905140
3503.217055	520199.874595	49.910145
3503.112770	520200.598914	49.915149
3503.152798	520201.350983	49.920154
3502.956452	520198.196760	49.925159
3503.379363	520199.242227	49.930164
3503.205545	520205.943573	49.935169
3503.278243	520204.668093	49.940173
3503.286116	520212.048553	49.945178
3503.492133	520195.179632	49.950183
3503.294132	520217.002128	49.955188
3503.256504	520205.025448	49.960193
3503.485741	520203.927463	49.965197
3503.115048	520198.778412	49.970202
3503.580429	520197.188065	49.975207
3503.298472	520206.333366	49.980212
3503.415799	520197.568005	49.985217
3503.183416	520179.706609	49.990221
3502.968303	520176.504788	49.995226
3503.471293	520173.947860	50.000231
3503.206694	520177.680542	50.005236
3503.713605	520168.550229	50.010241
3503.576229	520168.774182	50.015245
3503.229173	520170.851428	50.020250
3503.608688	520159.162699	50.025255
3503.453160	520156.507614	50.030260
3503.594117	520171.754381	50.035265
3503.753797	520167.178766	50.040269
3503.372980	520150.149755	50.045274
3503.697189	520131.745294	50.050279
3503.434068	520126.275858	50.055284
3503.556868	520125.043012	50.060289
3503.547935	520121.808592	50.065293
3503.364542	520128.460923	50.070298
3503.351721	520123.204723	50.075303
3503.255172	520122.967185	50.080308
3503.553759	520126.610861	50.085313
3503.678234	520129.169741	50.090317
3503.565237	520108.913083	50.095322
3503.647170	520084.783031	50.100327
3503.567965	520082.318110	50.105332
3503.743533	520073.290677	50.110337
3503.619377	520091.461344	50.115341
3503.499605	520081.469396	50.120346
3503.870383	520063.714778	50.125351
3503.441988	520055.793999	50.130356
3503.338211	520047.518545	50.135361
3503.399751	520043.211208	50.140365
3503.536064	520036.060683	50.145370
3503.928684	520026.038273	50.150375
3503.452439	520038.399669	50.155380
3503.298827	520038.221708	50.160385
3503.548323	520016.239156	50.165389
3503.308302	520015.013089	50.170394
3503.585492	519996.009185	50.175399
3503.280298	519997.321431	50.180404
3503.501371	519995.618000	50.185409
3503.441792	520000.127281	50.190413
3503.296791	519995.448095	50.195418
3503.801899	519996.328904	50.200423
3503.459101	520003.663765	50.205428
3503.529884	520001.175125	50.210433
3503.579303	519966.179578	50.215437
3503.528059	519957.744094	50.220442
3503.271314	519952.425273	50.225447
3503.027841	519965.609458	50.230452
3502.997317	519954.895482	50.235457
3503.284888	519955.608435	50.240461
3503.399011	519951.697246	50.245466
3503.440544	519952.701890	50.250471
3503.401153	519957.005750	50.255476
3503.308027	519946.200542	50.260481
3503.500754	519950.417156	50.265485
3503.426751	519952.097347	50.270490
3503.658006	519947.308116	50.275495
3503.202549	519957.289946	50.280500
3503.850079	519954.103414	50.285505
3503.352163	519919.548201	50.290509
3503.050087	519921.517247	50.295514
3503.783926	519920.794531	50.300519
3503.530469	519919.671701	50.305524
3503.374401	519911.505565	50.310529
3503.648197	519916.316100	50.315533
3503.492798	519916.947389	50.320538
3503.359640	519914.895455	50.325543
3503.340435	519925.010593	50.330548
3503.337110	519914.545094	50.335553
3503.498245	519912.193841	50.340557
3503.099509	519897.948228	50.345562
3503.478008	519882.416859	50.350567
3503.501724	519881.300777	50.355572
3503.389932	519870.296227	50.360577
3503.306527	519870.713896	50.365581
3503.527606	519876.594549	50.370586
3503.256521	519886.041674	50.375591
3503.208716	519882.206623	50.380596
3503.486884	519880.393034	50.385601
3503.629449	519882.443487	50.390605
3503.292279	519885.682099	50.395610
3503.424497	519877.773744	50.400615
3503.306909	519886.943803	50.405620
3503.390778	519876.970104	50.410625
3503.600693	519856.409292	50.415629
3503.274339	519854.337326	50.420634
3503.326110	519849.323632	50.425639
3503.347717	519862.162637	50.430644
3503.369617	519849.872924	50.435649
3503.435474	519851.682702	50.440653
3503.359262	519858.924929	50.445658
3503.525518	519846.915762	50.450663
3503.599770	519853.729724	50.455668
3503.202229	519856.977884	50.460673
3503.303315	519851.299107	50.465677
3503.170653	519851.977366	50.470682
3503.528564	519853.083691	50.475687
3503.468769	519850.008939	50.480692
3503.458124	519822.151639	50.485697
3503.850561	519814.303244	50.490701
3503.326130	519819.290536	50.495706
3503.699615	519811.040649	50.500711
3503.714537	519806.791179	50.505716
3503.771250	519813.911295	50.510721
3503.879232	519783.861064	50.515725
3503.640260	519779.146108	50.520730
3503.589432	519759.637607	50.525735
3503.360125	519734.898941	50.530740
3503.447159	519696.711526	50.535745
3503.790194	519652.315076	50.540749
3503.491189	519591.081886	50.545754
3503.449894	519518.835839	50.550759
3503.206707	519440.756196	50.555764
3502.913605	519337.352377	50.560769
3502.896876	519246.241498	50.565773
3502.500445	519149.072023	50.570778
3502.810640	519026.255857	50.575783
3502.400442	518912.603529	50.580788
3502.450070	518770.005691	50.585793
3502.344831	518625.964727	50.590797
3501.830408	518485.728984	50.595802
3501.785991	518320.741851	50.600807
3501.455314	518153.067754	50.605812
3501.440503	517977.403094	50.610817
3501.195654	517803.745042	50.615821
3500.826640	517607.450519	50.620826
3500.700754	517404.187394	50.625831
3500.213481	517209.221617	50.630836
3499.941565	516990.502434	50.635841
3499.958024	516768.093736	50.640845
3499.327079	516553.471158	50.645850
3499.173054	516317.530395	50.650855
3498.879233	516077.259170	50.655860
3498.809616	515834.319246	50.660865
3498.649123	515576.218021	50.665869
3498.392738	515327.332533	50.670874
3497.971102	515045.595489	50.675879
3497.526288	514766.386178	50.680884
3497.174104	514482.909097	50.685889
3496.749903	514189.879377	50.690893
3496.670289	513896.587763	50.695898
3496.137221	513603.008652	50.700903
3495.825572	513295.783233	50.705908
3495.604430	512973.262269	50.710913
3494.779799	512661.655207	50.715917
3494.339001	512346.643219	50.720922
3494.010660	512003.330871	50.725927
3493.345732	511685.205773	50.730932
3493.004505	511356.046293	50.735937
3493.019547	511007.955007	50.740941
3492.506910	510673.649500	50.745946
3492.262953	510299.329247	50.750951
3491.582114	509935.086804	50.755956
3491.020938	509577.192249	50.760961
3490.255783	509207.180192	50.765965
3489.817773	508842.420806	50.770970
3489.740316	508472.790169	50.775975
3488.740850	508104.359858	50.780980
3488.807375	507715.615506	50.785985
3488.209508	507337.087094	50.790989
3487.411513	506946.944171	50.795994
3487.296011	506556.178580	50.800999
3486.568473	506164.033495	50.806004
3486.073806	505756.054663	50.811009
3485.410534	505358.314955	50.816013
3484.639678	504961.898927	50.821018
3484.541739	504555.296880	50.826023
3483.996732	504135.648710	50.831028
3483.231311	503726.906239	50.836033
3482.808776	503315.670791	50.841037
3482.336325	502904.129970	50.846042
3481.679606	502473.730285	50.851047
3481.074915	502060.064993	50.856052
3480.297630	501626.626961	50.861057
3480.027781	501215.369167	50.866061
3479.269300	500782.565586	50.871066
3478.983119	500346.386640	50.876071
3478.228296	499901.412683	50.881076
3477.694028	499480.437726	50.886081
3477.454549	499025.084503	50.891085
3476.397643	498596.780603	50.896090
3475.634203	498145.284684	50.901095
3475.242995	497712.602071	50.906100
3474.911075	497259.699530	50.911105
3474.383710	496802.361267	50.916109
3473.248883	496362.777248	50.921114
3473.046851	495909.567347	50.926119
3472.419825	495452.970378	50.931124
3471.650664	494998.814868	50.936129
3471.203629	494534.014528	50.941133
3470.564963	494083.056315	50.946138
3469.791317	493619.904821	50.951143
3468.958496	493155.940823	50.956148
3468.479499	492699.100074	50.961153
3467.946873	492235.571919	50.966157
3466.922395	491770.337453	50.971162
3466.279854	491309.487591	50.976167
3465.405987	490844.813894	50.981172
3465.017344	490394.739265	50.986177
3464.348492	489926.009281	50.991181
3463.470989	489474.470402	50.996186
3462.859822	489009.152498	51.001191
3462.082255	488554.587405	51.006196
3461.522385	488084.325426	51.011201
3460.943891	487618.562859	51.016205
3460.105505	487157.794093	51.021210
3459.298639	486696.097363	51.026215
3458.799951	486244.522802	51.031220
3457.934790	485782.914486	51.036225
3457.270171	485323.998942	51.041229
3456.513711	484860.628784	51.046234
3456.114551	484400.635982	51.051239
3455.013854	483949.558488	51.056244
3454.651692	483488.879463	51.061249
3453.961325	483027.582700	51.066253
3453.370925	482567.931162	51.071258
3452.901724	482107.489572	51.076263
3451.973833	481640.117263	51.081268
3451.237146	481172.804877	51.086273
3450.733621	480714.413342	51.091277
3449.761093	480259.987039	51.096282
3449.021826	479793.452953	51.101287
3448.289537	479328.376296	51.106292
3447.726881	478882.113459	51.111297
3447.059621	478422.275538	51.116301
3446.039110	477965.016735	51.121306
3445.727355	477511.233632	51.126311
3445.050164	477050.656041	51.131316
3444.186014	476595.013553	51.136321
3443.532784	476134.208337	51.141325
3442.697180	475672.661106	51.146330
3442.020223	475216.197447	51.151335
3441.435623	474776.688905	51.156340
3440.878933	474314.508931	51.161345
3440.463815	473856.705974	51.166349
3439.693284	473392.764685	51.171354
3438.822843	472943.579780	51.176359
3437.968263	472481.760066	51.181364
3437.048906	472027.645581	51.186369
3436.507399	471570.977257	51.191373
3435.257192	471127.946598	51.196378
3435.348661	470674.352130	51.201383
3434.375233	470232.627286	51.206388
3433.600185	469784.473563	51.211393
3432.928900	469332.187037	51.216397
3432.249353	468886.736645	51.221402
3431.379718	468440.242032	51.226407
3430.807036	467989.127615	51.231412
3429.997172	467537.483224	51.236417
3429.490898	467098.356102	51.241421
3428.595296	466665.315453	51.246426
3428.575997	466203.731053	51.251431
3427.642996	465757.797929	51.256436
3426.733635	465303.890227	51.261441
3426.148105	464855.854805	51.266445
3425.528500	464420.239782	51.271450
3424.888603	463971.737960	51.276455
3423.881365	463533.985485	51.281460
3423.335607	463087.073098	51.286465
3422.643052	462644.384071	51.291469
3422.100378	462204.198110	51.296474
3421.236611	461753.403104	51.301479
3420.518262	461308.712756	51.306484
3419.570178	460868.056524	51.311489
3419.003271	460427.939754	51.316493
3418.252149	459992.458963	51.321498
3417.582445	459546.203258	51.326503
3416.899811	459110.694089	51.331508
3416.207982	458668.887782	51.336513
3415.558247	458234.776375	51.341517
3414.538960	457802.794682	51.346522
3414.085082	457369.193303	51.351527
3413.307296	456933.706940	51.356532
3412.457700	456501.419415	51.361537
3412.110735	456067.116239	51.366541
3410.785489	455633.314421	51.371546
3410.372484	455201.693697	51.376551
3409.851377	454777.032369	51.381556
3409.044500	454347.740564	51.386561
3408.451368	453921.552439	51.391565
3407.355097	453497.566793	51.396570
3407.017609	453066.654331	51.401575
3406.455530	452641.502727	51.406580
3405.551638	452212.540986	51.411585
3404.934357	451782.511048	51.416589
3404.289330	451364.807712	51.421594
3403.540301	450927.627947	51.426599
3403.227543	450505.441817	51.431604
3402.295055	450071.167197	51.436609
3401.622904	449646.535689	51.441613
3400.444496	449228.877988	51.446618
3399.854050	448801.883756	51.451623
3399.149397	448383.526993	51.456628
3398.684966	447967.966716	51.461633
3397.764607	447539.732825	51.466637
3396.841892	447123.621028	51.471642
3396.444184	446701.836124	51.476647
3395.574839	446290.877886	51.481652
3394.908956	445870.744630	51.486657
3394.357062	445449.266275	51.491661
3393.223902	445040.967315	51.496666
3393.076044	444626.364017	51.501671
3392.408450	444205.694047	51.506676
3391.769489	443789.072821	51.511681
3390.922615	443369.431681	51.516685
3389.980282	442970.508423	51.521690
3389.214554	442549.977247	51.526695
3388.329250	442146.868960	51.531700
3387.783008	441732.075707	51.536705
3387.349199	441320.811038	51.541709
3386.349717	440928.868556	51.546714
3385.734587	440516.045288	51.551719
3385.275980	440105.068649	51.556724
3384.495185	439699.212758	51.561729
3383.620264	439288.034441	51.566733
3382.846440	438894.399198	51.571738
3382.110287	438487.323235	51.576743
3381.391205	438086.634928	51.581748
3380.871713	437680.069931	51.586753
3380.411541	437272.778111	51.591757
3379.295015	436879.368208	51.596762
3378.789503	436473.771421	51.601767
3378.117382	436071.520138	51.606772
3377.272239	435681.704288	51.611777
3376.640701	435279.306996	51.616781
3375.718423	434884.997375	51.621786
3375.174831	434485.924822	51.626791
3374.291061	434107.261867	51.631796
3373.509294	433708.087827	51.636801
3372.840775	433314.983214	51.641805
3372.145361	432933.556346	51.646810
3371.767980	432540.622332	51.651815
3371.143226	432151.403135	51.656820
3369.978096	431762.263511	51.661825
3369.440544	431372.434780	51.666829
3368.904460	430979.121222	51.671834
3368.309266	430597.618606	51.676839
3367.378318	430212.151410	51.681844
3366.911171	429826.935296	51.686849
3366.557585	429422.015440	51.691853
3365.679610	429036.598739	51.696858
3365.083924	428643.234079	51.701863
3364.399201	428256.454896	51.706868
3363.323958	427866.532015	51.711873
3363.036723	427466.676094	51.716877
3362.135665	427088.472398	51.721882
3361.640151	426694.453488	51.726887
3361.013324	426301.541593	51.731892
3360.163954	425917.116350	51.736897
3359.634056	425515.161654	51.741901
3358.723959	425141.224067	51.746906
3357.832527	424752.293441	51.751911
3357.466578	424368.074451	51.756916
3356.774001	423985.704996	51.761921
3355.758942	423604.600327	51.766925
3355.182140	423228.246952	51.771930
3354.582451	422834.747061	51.776935
3353.850921	422453.911726	51.781940
3353.018095	422069.175435	51.786945
3352.772863	421688.557423	51.791949
3351.651154	421315.515370	51.796954
3351.024503	420933.829639	51.801959
3350.454009	420544.178946	51.806964
3349.661821	420158.596845	51.811969
3349.186606	419783.247410	51.816973
3348.390680	419409.035995	51.821978
3347.959847	419025.235576	51.826983
3347.172011	418657.744793	51.831988
3346.166500	418271.814873	51.836993
3345.936223	417889.440741	51.841997
3344.855194	417522.515081	51.847002
3344.282881	417140.743874	51.852007
3343.875923	416761.888444	51.857012
3342.860153	416380.812350	51.862017
3342.362884	415995.965311	51.867021
3341.257248	415634.151364	51.872026
3340.887856	415248.334078	51.877031
3340.215186	414871.401287	51.882036
3339.692949	414507.346788	51.887041
3338.995609	414122.303205	51.892045
3337.841081	413751.834864	51.897050
3337.225944	413376.880872	51.902055
3336.677549	413010.143963	51.907060
3335.795923	412631.970284	51.912065
3335.358604	412266.324544	51.917069
3334.437275	411895.872164	51.922074
3333.983281	411521.377286	51.927079
3333.323093	411164.799169	51.932084
3332.318969	410797.852821	51.937089
3332.026382	410423.394855	51.942093
3331.198503	410059.283015	51.947098
3330.501885	409699.161032	51.952103
3329.798444	409331.691794	51.957108
3329.196068	408970.987155	51.962113
3328.337315	408590.497029	51.967117
3327.521667	408235.077755	51.972122
3327.065074	407856.369981	51.977127
3326.347976	407493.836229	51.982132
3325.422099	407134.202954	51.987137
3325.064485	406764.792863	51.992141
3324.256079	406407.292703	51.997146
3323.594531	406043.411530	52.002151
3322.809849	405686.636312	52.007156
3321.881350	405313.334452	52.012161
3321.371529	404956.558222	52.017165
3320.463706	404606.296471	52.022170
3319.891346	404250.767456	52.027175
3319.638794	403894.726345	52.032180
3318.603736	403547.700787	52.037185
3318.086474	403177.587215	52.042189
3317.385393	402817.436522	52.047194
3316.597657	402450.839405	52.052199
3316.033402	402094.446097	52.057204
3314.975153	401734.593828	52.062209
3314.376329	401373.724376	52.067213
3313.611743	401045.387524	52.072218
3312.987472	400680.752368	52.077223
3312.692070	400328.389394	52.082228
3311.850666	399977.456174	52.087233
3311.117190	399618.444036	52.092237
3310.482264	399260.505417	52.097242
3309.776779	398902.065632	52.102247
3308.996875	398567.300246	52.107252
3307.904612	398212.345874	52.112257
3307.894686	397859.656926	52.117261
3306.658868	397519.411201	52.122266
3306.121052	397168.552454	52.127271
3305.582782	396820.283111	52.132276
3304.959818	396473.345478	52.137281
3304.423793	396121.687346	52.142285
3303.620383	395786.592564	52.147290
3302.946074	395432.178010	52.152295
3302.400710	395076.366484	52.157300
3301.809534	394731.846487	52.162305
3301.278705	394373.610051	52.167309
3300.439565	394035.834083	52.172314
3299.892126	393675.609865	52.177319
3299.426483	393323.504769	52.182324
3298.392550	392977.003122	52.187329
3297.840221	392622.946854	52.192333
3297.167415	392268.219529	52.197338
3296.305382	391911.484454	52.202343
3295.895600	391568.277003	52.207348
3294.925243	391215.848892	52.212353
3294.434942	390859.451072	52.217357
3293.303163	390526.085866	52.222362
3293.100691	390174.568326	52.227367
3292.640733	389826.546093	52.232372
3291.428020	389471.799544	52.237377
3291.002627	389126.383984	52.242381
3290.569304	388771.507174	52.247386
3289.559602	388420.023652	52.252391
3288.861050	388077.870521	52.257396
3287.987584	387732.258083	52.262401
3287.538902	387382.989682	52.267405
3286.556757	387032.759692	52.272410
3286.277113	386704.080969	52.277415
3285.142193	386360.454845	52.282420
3284.659221	386012.628174	52.287425
3283.985178	385669.405822	52.292429
3283.028166	385334.845871	52.297434
3282.648821	384994.901972	52.302439
3282.107599	384646.919015	52.307444
3281.468771	384304.695624	52.312449
3280.909242	383950.351295	52.317453
3280.143473	383627.393165	52.322458
3279.370638	383285.461362	52.327463
3278.660159	382938.760821	52.332468
3277.836223	382596.576516	52.337473
3277.545851	382256.415600	52.342477
3276.781948	381915.512688	52.347482
3276.278148	381558.263154	52.352487
3275.801835	381213.697013	52.357492
3274.607147	380878.066737	52.362497
3274.474562	380535.729125	52.367501
3273.532101	380193.796342	52.372506
3272.603044	379851.782111	52.377511
3272.132240	379497.636586	52.382516
3271.279947	379159.978795	52.387521
3270.535098	378814.289186	52.392525
3269.845856	378484.153843	52.397530
3269.491781	378137.607979	52.402535
3268.985236	377798.484848	52.407540
3268.255726	377459.902786	52.412545
3267.634219	377102.961607	52.417549
3266.806153	376767.187161	52.422554
3266.307206	376427.313486	52.427559
3265.332767	376077.744579	52.432564
3264.460154	375745.071850	52.437569
3264.054340	375391.693306	52.442573
3263.371511	375060.129576	52.447578
3263.069192	374719.218369	52.452583
3262.227914	374374.472200	52.457588
3261.128626	374039.811805	52.462593
3260.743019	373686.160905	52.467597
3259.941171	373352.439942	52.472602
3259.081663	373008.829918	52.477607
3258.451775	372663.425470	52.482612
3257.730675	372333.702818	52.487617
3257.196277	371989.524179	52.492621
3256.539876	371662.838674	52.497626
3255.638733	371320.467860	52.502631
3255.221299	370986.031198	52.507636
3254.277184	370658.264090	52.512641
3253.628207	370311.520482	52.517645
3253.056728	369981.882989	52.522650
3252.417569	369653.118633	52.527655
3251.679475	369312.588461	52.532660
3251.037662	368987.228464	52.537665
3250.491676	368652.463176	52.542669
3249.703087	368317.733681	52.547674
3248.878914	367985.144312	52.552679
3248.200264	367648.687730	52.557684
3247.286201	367334.221960	52.562689
3247.120433	366997.450289	52.567693
3246.609358	366671.085584	52.572698
3245.621345	366322.811838	52.577703
3245.005272	365989.462122	52.582708
3244.213460	365661.582438	52.587713
3244.111442	365330.538104	52.592717
3242.961906	365005.381712	52.597722
3242.211922	364669.091996	52.602727
3241.736922	364341.788678	52.607732
3240.752694	364003.012194	52.612737
3240.000340	363661.499481	52.617741
3239.525408	363348.004977	52.622746
3238.946035	363019.105745	52.627751
3238.195755	362690.892758	52.632756
3237.180807	362352.617868	52.637761
3236.723431	362033.386681	52.642765
3236.116646	361717.001321	52.647770
3235.548826	361373.788655	52.652775
3234.996135	361054.387767	52.657780
3233.916102	360724.482883	52.662785
3233.460444	360393.204657	52.667789
3232.851954	360073.755102	52.672794
3232.277395	359747.733014	52.677799
3231.364697	359417.538160	52.682804
3230.647267	359090.160128	52.687809
3230.254903	358762.143189	52.692813
3229.247586	358438.954373	52.697818
3229.027058	358105.053115	52.702823
3227.982726	357779.244775	52.707828
3227.198680	357461.917862	52.712833
3226.524210	357129.481371	52.717837
3226.182979	356803.580805	52.722842
3225.226104	356481.058230	52.727847
3224.594166	356158.075003	52.732852
3223.806340	355850.306738	52.737857
3223.364954	355514.539839	52.742861
3222.679658	355201.076475	52.747866
3222.057457	354875.996739	52.752871
3221.293034	354547.323735	52.757876
3220.667163	354228.449893	52.762881
3220.139257	353908.260681	52.767885
3219.260927	353587.412344	52.772890
3218.640029	353261.024272	52.777895
3217.986625	352932.756043	52.782900
3217.299711	352623.069169	52.787905
3216.642003	352304.493925	52.792909
3215.745831	351976.003609	52.797914
3214.906798	351656.282442	52.802919
3214.769428	351332.834431	52.807924
3213.811286	351020.610611	52.812929
3213.273713	350701.243223	52.817933
3212.997531	350387.991617	52.822938
3212.054496	350049.749301	52.827943
3211.754940	349722.677803	52.832948
3210.561676	349403.737344	52.837953
3210.185413	349071.685680	52.842957
3208.953900	348755.801637	52.847962
3208.290612	348435.041015	52.852967
3208.010452	348116.483115	52.857972
3207.332896	347797.782646	52.862977
3206.740534	347479.423207	52.867981
3205.787757	347156.664874	52.872986
3205.072825	346836.539544	52.877991
3204.666361	346524.406535	52.882996
3203.996016	346206.179516	52.888001
3203.663612	345878.428891	52.893005
3202.697781	345563.502980	52.898010
3201.954784	345239.224337	52.903015
3201.325218	344917.318516	52.908020
3200.716651	344606.530627	52.913025
3200.374704	344274.954457	52.918029
3199.409288	343961.343375	52.923034
3198.726328	343630.097509	52.928039
3198.204850	343303.533184	52.933044
3197.415056	342983.932969	52.938049
3196.590452	342655.224019	52.943053
3196.065607	342341.356520	52.948058
3195.447996	342015.920371	52.953063
3194.836584	341682.361538	52.958068
3193.841646	341375.690652	52.963073
3193.248266	341050.805516	52.968077
3192.214839	340736.195665	52.973082
3191.453087	340416.475698	52.978087
3190.949445	340102.720647	52.983092
3190.297967	339798.354919	52.988097
3189.709684	339473.358909	52.993101
3189.169721	339160.368552	52.998106
3188.181584	338856.102449	53.003111
3187.877798	338527.390974	53.008116
3187.310692	338219.567793	53.013121
3186.537303	337903.655329	53.018125
3185.569313	337589.732226	53.023130
3184.637029	337269.692469	53.028135
3184.098192	336965.142705	53.033140
3183.482242	336659.407274	53.038145
3183.010673	336342.573982	53.043149
3182.041757	336040.837301	53.048154
3181.185915	335721.159782	53.053159
3180.992800	335411.635018	53.058164
3180.176698	335116.336045	53.063169
3179.646104	334798.079187	53.068173
3178.762763	334489.804980	53.073178
3177.822919	334182.582075	53.078183
3177.744408	333871.733841	53.083188
3176.717698	333581.273018	53.088193
3176.360444	333254.758779	53.093197
3175.421875	332950.686959	53.098202
3174.620868	332641.424095	53.103207
3174.234988	332334.945494	53.108212
3173.246462	332032.125060	53.113217
3172.778909	331719.394021	53.118221
3172.170650	331419.794942	53.123226
3171.562161	331108.560128	53.128231
3170.943406	330798.369403	53.133236
3169.918122	330496.388461	53.138241
3169.595843	330195.186101	53.143245
3169.185838	329888.064464	53.148250
3168.119976	329575.648014	53.153255
3167.737272	329265.668074	53.158260
3166.798461	328953.254376	53.163265
3166.401227	328641.950280	53.168269
3165.343708	328342.180662	53.173274
3164.622324	328030.416159	53.178279
3164.173803	327721.738750	53.183284
3163.208016	327425.006184	53.188289
3162.716171	327112.565155	53.193293
3162.327947	326815.407900	53.198298
3161.375431	326511.846496	53.203303
3160.917586	326205.965162	53.208308
3160.114629	325901.104743	53.213313
3159.629183	325595.403651	53.218317
3158.738791	325289.256260	53.223322
3158.245823	324977.927261	53.228327
3157.322800	324666.970643	53.233332
3156.538819	324376.945006	53.238337
3156.143867	324071.096557	53.243341
3155.448993	323773.543763	53.248346
3154.757358	323460.992874	53.253351
3154.252063	323157.017180	53.258356
3153.328317	322854.787038	53.263361
3153.150252	322549.102406	53.268365
3152.229524	322239.791372	53.273370
3151.520679	321938.211440	53.278375
3151.079538	321627.294638	53.283380
3149.954613	321329.572194	53.288385
3149.510708	321017.176884	53.293389
3148.571313	320712.853875	53.298394
3147.868488	320409.765484	53.303399
3147.282634	320115.594708	53.308404
3146.418714	319811.154838	53.313409
3146.060336	319511.802767	53.318413
3145.453825	319214.245868	53.323418
3144.613258	318919.245808	53.328423
3144.376713	318615.135547	53.333428
3143.300840	318321.443938	53.338433
3143.061266	318009.311506	53.343437
3142.319801	317707.417048	53.348442
3141.304899	317403.400568	53.353447
3140.486618	317098.664514	53.358452
3139.575468	316805.935204	53.363457
3139.366743	316505.760535	53.368461
3138.857286	316208.229758	53.373466
3137.852651	315907.007899	53.378471
3137.738774	315597.521420	53.383476
3136.829645	315306.187807	53.388481
3135.927584	315009.835956	53.393485
3135.196905	314699.884125	53.398490
3134.591556	314400.045988	53.403495
3133.867385	314098.545185	53.408500
3133.144563	313803.842081	53.413505
3132.627082	313498.334508	53.418509
3131.765791	313215.976096	53.423514
3130.931408	312922.510441	53.428519
3130.466031	312619.462085	53.433524
3129.662695	312319.980386	53.438529
3129.336245	312028.519968	53.443533
3128.670196	311733.649392	53.448538
3127.825494	311432.516644	53.453543
3127.383862	311137.048757	53.458548
3126.423190	310850.141844	53.463553
3125.993122	310555.459995	53.468557
3125.249181	310249.317119	53.473562
3124.480928	309959.831072	53.478567
3124.367588	309660.309479	53.483572
3123.390888	309363.037305	53.488577
3122.706698	309059.759351	53.493581
3122.136423	308762.421356	53.498586
3121.310181	308454.224177	53.503591
3120.892347	308163.124932	53.508596
3119.931046	307870.328447	53.513601
3119.212678	307569.038434	53.518605
3118.769179	307271.422098	53.523610
3117.883368	306980.979826	53.528615
3117.376128	306676.496582	53.533620
3116.404307	306385.811910	53.538625
3115.847377	306092.285207	53.543629
3115.145145	305800.028641	53.548634
3114.438989	305499.215658	53.553639
3114.049017	305203.801575	53.558644
3113.161239	304910.095412	53.563649
3112.681886	304615.127096	53.568653
3111.885899	304314.198354	53.573658
3111.156778	304028.665132	53.578663
3110.701785	303728.343266	53.583668
3109.962417	303436.902401	53.588673
3109.239965	303144.439628	53.593677
3108.113407	302854.306676	53.598682
3107.672977	302558.436585	53.603687
3107.054086	302259.843808	53.608692
3105.837774	301980.215333	53.613697
3106.099391	301688.536173	53.618701
3105.106036	301403.523460	53.623706
3104.273835	301120.343747	53.628711
3103.664750	300829.004469	53.633716
3103.051406	300540.339285	53.638721
3102.713102	300245.569056	53.643725
3101.813837	299966.268766	53.648730
3101.197533	299668.230840	53.653735
3100.660604	299375.451376	53.658740
3099.679091	299088.344390	53.663745
3099.048913	298790.536281	53.668749
3098.513910	298495.488449	53.673754
3097.774945	298211.779591	53.678759
3097.117848	297928.286514	53.683764
3096.280767	297638.098242	53.688769
3095.478876	297343.167104	53.693773
3094.792260	297061.536396	53.698778
3094.096851	296775.577278	53.703783
3093.768551	296477.692039	53.708788
3092.954395	296203.898554	53.713793
3092.319901	295914.592313	53.718797
3091.905873	295626.778769	53.723802
3091.189695	295345.201115	53.728807
3090.683560	295059.464150	53.733812
3089.454054	294756.600005	53.738817
3089.511582	294473.930934	53.743821
3088.290407	294188.738851	53.748826
3087.678566	293892.906509	53.753831
3087.360428	293599.217461	53.758836
3086.266208	293319.734260	53.763841
3085.957906	293030.703407	53.768845
3084.913459	292737.000815	53.773850
3084.417998	292454.696762	53.778855
3083.728355	292172.728703	53.783860
3082.927486	291889.020652	53.788865
3082.689621	291593.559046	53.793869
3081.434911	291305.694525	53.798874
3080.778195	291020.536460	53.803879
3080.331277	290730.302285	53.808884
3079.317359	290457.908445	53.813889
3078.690334	290171.929768	53.818893
3078.560325	289890.278031	53.823898
3077.792902	289611.451921	53.828903
3076.852662	289329.622220	53.833908
3076.018979	289041.484836	53.838913
3075.673575	288752.607722	53.843917
3074.874588	288474.345776	53.848922
3074.009711	288195.661045	53.853927
3073.647731	287907.320556	53.858932
3072.833695	287623.508221	53.863937
3072.423197	287349.411436	53.868941
3071.637028	287059.965786	53.873946
3070.818516	286778.547402	53.878951
3070.335134	286486.888561	53.883956
3069.455605	286209.656112	53.888961
3068.902006	285926.030331	53.893965
3068.437394	285645.675620	53.898970
3067.785723	285362.472416	53.903975
3067.202035	285068.332447	53.908980
3066.371304	284797.916668	53.913985
3065.944095	284505.050390	53.918989
3065.089283	284221.954933	53.923994
3064.166868	283939.150139	53.928999
3063.942476	283656.794987	53.934004
3063.174426	283369.635818	53.939009
3062.583608	283086.345056	53.944013
3061.840736	282805.192053	53.949018
3061.329813	282517.507792	53.954023
3060.459412	282234.133460	53.959028
3059.845805	281953.239692	53.964033
3059.175588	281664.179438	53.969037
3058.588558	281378.340344	53.974042
3057.725972	281081.898995	53.979047
3057.313938	280781.871577	53.984052
3056.210493	280501.716847	53.989057
3055.593161	280217.053584	53.994061
3054.858335	279940.813349	53.999066
3053.962192	279659.326607	54.004071
3053.502113	279370.334002	54.009076
3052.907355	279108.868415	54.014081
3052.124384	278826.166481	54.019085
3051.561151	278543.429688	54.024090
3050.723705	278273.928828	54.029095
3050.472551	277995.624929	54.034100
3049.428971	277718.184973	54.039105
3048.919392	277434.879122	54.044109
3048.083060	277153.636935	54.049114
3047.297770	276880.179946	54.054119
3046.966136	276595.852520	54.059124
3046.148380	276322.426062	54.064129
3045.540998	276046.113818	54.069133
3044.791718	275769.824008	54.074138
3044.050619	275483.039907	54.079143
3043.485840	275210.286434	54.084148
3042.864260	274936.599612	54.089153
3042.349835	274659.432124	54.094157
3041.552895	274390.459239	54.099162
3040.466747	274120.284184	54.104167
3040.084329	273832.882995	54.109172
3039.621834	273563.424244	54.114177
3038.816366	273285.971789	54.119181
3038.365966	273015.848991	54.124186
3037.183537	272732.114633	54.129191
3036.655181	272449.626611	54.134196
3035.819521	272190.847391	54.139201
3035.177262	271910.746044	54.144205
3034.794353	271643.668971	54.149210
3034.027335	271366.643685	54.154215
3033.735804	271092.242845	54.159220
3032.766232	270823.959923	54.164225
3032.146623	270547.395403	54.169229
3031.451769	270268.856342	54.174234
3030.576872	270010.338496	54.179239
3030.289998	269728.271334	54.184244
3029.330373	269455.683091	54.189249
3028.996306	269188.395207	54.194253
3028.346449	268916.725921	54.199258
3027.162359	268636.940517	54.204263
3026.727800	268363.709274	54.209268
3025.937591	268099.855824	54.214273
3025.368879	267824.404843	54.219277
3025.073044	267551.534024	54.224282
3024.322937	267277.996663	54.229287
3023.784549	266998.848388	54.234292
3022.766795	266724.920713	54.239297
3022.149189	266447.313364	54.244301
3021.623358	266186.347824	54.249306
3020.747499	265914.919485	54.254311
3020.248606	265633.320785	54.259316
3019.280022	265365.625798	54.264321
3018.819976	265097.035498	54.269325
3018.179769	264836.063377	54.274330
3017.209544	264557.647093	54.279335
3017.097873	264275.555040	54.284340
3016.086340	264019.404751	54.289345
3015.503363	263738.559223	54.294349
3014.891051	263464.976930	54.299354
3014.045288	263200.982288	54.304359
3013.558732	262919.027007	54.309364
3013.141368	262652.621913	54.314369
3012.323301	262372.527781	54.319373
3011.648043	262103.591686	54.324378
3010.805000	261837.407437	54.329383
3010.315957	261556.727101	54.334388
3009.139739	261289.271728	54.339393
3008.893381	261022.204222	54.344397
3008.129672	260748.036933	54.349402
3007.546683	260481.150541	54.354407
3006.706750	260205.264023	54.359412
3006.234051	259947.121575	54.364417
3005.371291	259672.436180	54.369421
3004.872640	259409.510421	54.374426
3003.953155	259136.337143	54.379431
3003.612771	258856.094355	54.384436
3002.874720	258590.380407	54.389441
3002.012218	258318.497823	54.394445
3001.661955	258046.305240	54.399450
3000.570099	257785.410585	54.404455
3000.037603	257516.456348	54.409460
2999.622440	257251.227554	54.414465
2998.841896	256981.880245	54.419469
2998.177532	256717.379130	54.424474
2997.352422	256450.662641	54.429479
2997.080927	256173.850175	54.434484
2996.237223	255922.086583	54.439489
2995.395890	255647.835314	54.444493
2994.551732	255371.572932	54.449498
2994.253812	255106.455475	54.454503
2993.583865	254837.857311	54.459508
2992.751813	254574.786059	54.464513
2992.165820	254298.102235	54.469517
2991.471021	254040.714582	54.474522
2990.686584	253772.950907	54.479527
2990.357606	253496.940593	54.484532
2989.105465	253232.689747	54.489537
2988.566125	252964.124387	54.494541
2988.008521	252710.002025	54.499546
2987.398734	252437.908676	54.504551
2986.904575	252176.518954	54.509556
2985.977713	251915.401841	54.514561
2985.345238	251646.827685	54.519565
2984.511822	251380.883349	54.524570
2984.065423	251129.699747	54.529575
2983.548891	250858.128845	54.534580
2982.620752	250588.278862	54.539585
2981.811728	250327.629340	54.544589
2981.279909	250064.746221	54.549594
2980.563020	249815.109910	54.554599
2980.035487	249539.442784	54.559604
2979.389358	249287.835164	54.564609
2978.896220	249021.815235	54.569613
2977.934374	248753.323321	54.574618
2977.371316	248490.549574	54.579623
2976.515899	248225.275931	54.584628
2976.091672	247975.214183	54.589633
2975.110074	247718.416159	54.594637
2974.821188	247451.067815	54.599642
2974.035449	247197.448400	54.604647
2973.328772	246926.118036	54.609652
2972.414531	246670.635385	54.614657
2971.574918	246408.571164	54.619661
2971.314456	246151.101451	54.624666
2969.973113	245899.482191	54.629671
2969.809182	245638.152785	54.634676
2969.264258	245391.450569	54.639681
2968.467517	245132.514203	54.644685
2967.748898	244873.667816	54.649690
2967.256892	244616.110253	54.654695
2966.564246	244357.617252	54.659700
2965.803088	244096.461718	54.664705
2965.145746	243838.677162	54.669709
2964.888732	243576.016774	54.674714
2963.949411	243327.776443	54.679719
2963.231800	243059.893223	54.684724
2962.586865	242804.757130	54.689729
2961.936361	242556.803605	54.694733
2961.031055	242295.496249	54.699738
2960.315262	242041.900813	54.704743
2960.007271	241785.312852	54.709748
2959.305518	241535.026676	54.714753
2958.608337	241280.971479	54.719757
2958.123809	241011.527832	54.724762
2957.527926	240760.869973	54.729767
2956.687823	240492.807946	54.734772
2955.813769	240242.806364	54.739777
2955.239501	239980.840396	54.744781
2954.874403	239725.131647	54.749786
2954.090457	239469.031408	54.754791
2953.462272	239207.508607	54.759796
2952.643767	238942.680694	54.764801
2951.977368	238695.603432	54.769805
2951.305334	238429.352984	54.774810
2950.464326	238186.047732	54.779815
2950.137921	237917.732102	54.784820
2949.243993	237672.730249	54.789825
2948.479107	237410.494802	54.794829
2948.038960	237152.002706	54.799834
2947.155026	236900.074791	54.804839
2946.650244	236626.137569	54.809844
2946.007345	236386.981024	54.814849
2945.470957	236119.365132	54.819853
2944.897932	235866.320950	54.824858
2944.015385	235624.301208	54.829863
2943.524225	235354.948572	54.834868
2942.862177	235100.112426	54.839873
2941.991913	234837.619915	54.844877
2941.345775	234585.150626	54.849882
2940.684723	234330.087066	54.854887
2940.225161	234060.758291	54.859892
2939.375078	233816.853399	54.864897
2938.810835	233561.267198	54.869901
2938.411423	233298.449513	54.874906
2937.275105	233040.408927	54.879911
2936.736385	232787.112360	54.884916
2935.812360	232530.567283	54.889921
2935.378453	232277.204524	54.894925
2934.609828	232023.946353	54.899930
2933.896790	231767.726382	54.904935
2933.276588	231511.314165	54.909940
2932.706869	231275.417439	54.914945
2931.971260	231014.365205	54.919949
2931.567634	230751.682469	54.924954
2929.907783	230502.821707	54.929959
2929.709034	230248.434135	54.934964
2929.063701	230005.575950	54.939969
2928.636917	229748.399569	54.944973
2928.130459	229503.611076	54.949978
2927.253417	229247.169419	54.954983
2926.771311	228997.617059	54.959988
2926.026474	228749.354623	54.964993
2925.267901	228494.831467	54.969997
2924.996467	228234.706730	54.975002
2923.675447	227984.653508	54.980007
2923.028231	227730.853319	54.985012
2922.489356	227488.621675	54.990017
2921.760328	227240.386470	54.995021
2921.072449	226989.013726	55.000026
2920.153300	226750.485337	55.005031
2919.273804	226494.714134	55.010036
2919.191911	226259.186280	55.015041
2918.252029	226011.790066	55.020045
2917.904908	225763.727856	55.025050
2916.702625	225517.163942	55.030055
2916.224473	225277.449629	55.035060
2915.863978	225034.547523	55.040065
2915.093063	224786.873599	55.045069
2914.571849	224538.104274	55.050074
2913.715997	224298.223481	55.055079
2913.164624	224051.077163	55.060084
2912.446903	223809.113659	55.065089
2911.810010	223555.528212	55.070093
2911.203821	223307.068933	55.075098
2910.539757	223061.916676	55.080103
2909.951056	222818.459066	55.085108
2909.291564	222572.060066	55.090113
2908.322162	222315.997981	55.095117
2908.180472	222082.312110	55.100122
2907.326442	221835.971699	55.105127
2906.880147	221580.809409	55.110132
2906.044557	221328.586532	55.115137
2905.454951	221087.171259	55.120141
2904.667898	220826.286147	55.125146
2903.978497	220584.328167	55.130151
2903.562088	220338.063323	55.135156
2902.607202	220094.723240	55.140161
2902.106773	219834.088962	55.145165
2901.184347	219585.666326	55.150170
2900.428150	219339.789546	55.155175
2900.029930	219094.327889	55.160180
2899.298745	218852.127569	55.165185
2898.550723	218605.220877	55.170189
2897.736999	218345.787114	55.175194
2896.828540	218119.707076	55.180199
2896.728919	217867.659459	55.185204
2895.947296	217625.725808	55.190209
2895.221454	217380.512769	55.195213
2894.515253	217131.364191	55.200218
2894.049939	216894.410907	55.205223
2893.253165	216645.240195	55.210228
2892.685917	216398.401599	55.215233
2891.834571	216155.745737	55.220237
2890.977694	215910.774951	55.225242
2890.442569	215671.952992	55.230247
2889.968361	215424.581236	55.235252
2889.351060	215177.423957	55.240257
2888.482835	214928.270721	55.245261
2887.903084	214682.789462	55.250266
2886.982824	214453.311871	55.255271
2886.484224	214205.146494	55.260276
2885.632439	213965.120523	55.265281
2885.217911	213719.285658	55.270285
2884.445826	213472.477318	55.275290
2883.729176	213234.239996	55.280295
2883.165174	212988.864255	55.285300
2882.347834	212761.539972	55.290305
2881.727936	212519.649631	55.295309
2881.173751	212272.009390	55.300314
2880.373576	212036.958926	55.305319
2879.869665	211791.858161	55.310324
2879.188505	211563.485508	55.315329
2878.566376	211317.450660	55.320333
2877.674639	211072.579499	55.325338
2877.215972	210838.904836	55.330343
2876.671042	210597.429819	55.335348
2875.562789	210350.113793	55.340353
2875.095018	210117.028697	55.345357
2874.802130	209875.834707	55.350362
2873.997309	209643.492026	55.355367
2873.272964	209402.546362	55.360372
2872.560001	209155.694262	55.365377
2871.787292	208917.532725	55.370381
2871.779004	208675.127373	55.375386
2870.919902	208434.410439	55.380391
2870.098938	208187.541117	55.385396
2869.322533	207944.305728	55.390401
2868.785696	207693.155230	55.395405
2868.417589	207450.760782	55.400410
2867.491643	207205.604769	55.405415
2866.505393	206961.808367	55.410420
2865.788676	206716.939383	55.415425
2865.018105	206489.464936	55.420429
2864.702130	206241.759957	55.425434
2864.200983	205997.636119	55.430439
2863.404774	205753.000032	55.435444
2862.613699	205517.591030	55.440449
2861.868929	205278.128546	55.445453
2861.602103	205030.255404	55.450458
2860.593709	204793.025630	55.455463
2860.125485	204548.151718	55.460468
2859.362637	204310.299603	55.465473
2858.969937	204069.348232	55.470477
2858.455009	203820.972293	55.475482
2857.672887	203582.757161	55.480487
2856.737137	203338.751444	55.485492
2855.973078	203090.812633	55.490497
2855.376611	202840.112237	55.495501
2854.880318	202595.632872	55.500506
2853.836337	202368.357828	55.505511
2853.352950	202128.256201	55.510516
2852.575099	201885.517059	55.515521
2852.006484	201648.039800	55.520525
2851.437847	201399.899309	55.525530
2850.654702	201169.609977	55.530535
2849.675567	200926.601468	55.535540
2849.145742	200682.619348	55.540545
2848.157628	200459.529983	55.545549
2848.153693	200206.800548	55.550554
2847.342998	199983.672294	55.555559
2846.864589	199737.968289	55.560564
2846.068581	199502.674155	55.565569
2845.494043	199263.528369	55.570573
2845.210389	199012.286738	55.575578
2844.182945	198778.979372	55.580583
2843.528723	198529.669286	55.585588
2842.794818	198295.986680	55.590593
2842.055190	198061.542499	55.595597
2841.643367	197806.254805	55.600602
2840.653545	197572.641354	55.605607
2839.845314	197333.910228	55.610612
2839.507796	197100.742728	55.615617
2838.335984	196854.016550	55.620621
2838.180771	196618.417341	55.625626
2837.324564	196389.470678	55.630631
2836.947394	196140.242514	55.635636
2836.314654	195900.624862	55.640641
2835.216784	195663.385111	55.645645
2834.742874	195414.735636	55.650650
2834.151159	195191.020288	55.655655
2833.189871	194962.109314	55.660660
2832.524903	194722.896702	55.665665
2832.196786	194479.305645	55.670669
2831.335591	194241.627824	55.675674
2830.260484	194019.062999	55.680679
2830.094903	193773.401018	55.685684
2829.380902	193548.096318	55.690689
2828.419843	193308.835489	55.695693
2828.123448	193068.808897	55.700698
2827.242094	192840.327482	55.705703
2826.726098	192599.498159	55.710708
2825.965727	192361.418841	55.715713
2825.130715	192132.602527	55.720717
2824.631675	191900.082414	55.725722
2823.942241	191665.303330	55.730727
2823.317832	191423.886182	55.735732
2823.039909	191196.805436	55.740737
2821.840011	190966.474652	55.745741
2821.462272	190722.617203	55.750746
2820.635901	190494.608737	55.755751
2819.966191	190254.527766	55.760756
2819.419502	190019.988467	55.765761
2818.988364	189785.317502	55.770765
2818.221592	189547.583730	55.775770
2817.716325	189316.374706	55.780775
2816.762520	189068.800014	55.785780
2816.097367	188843.878208	55.790785
2815.399805	188608.288295	55.795789
2814.907925	188360.593245	55.800794
2814.001140	188135.573124	55.805799
2813.193305	187890.894929	55.810804
2812.868168	187661.153981	55.815809
2811.878502	187435.259774	55.820813
2811.216611	187200.409157	55.825818
2810.436462	186973.593443	55.830823
2809.918460	186744.752662	55.835828
2809.259075	186503.607707	55.840833
2808.377484	186285.793213	55.845837
2808.165174	186048.727202	55.850842
2807.299202	185812.923634	55.855847
2806.646295	185583.384834	55.860852
2806.077135	185355.322367	55.865857
2805.395065	185126.566508	55.870861
2804.888558	184887.899285	55.875866
2803.996642	184667.537084	55.880871
2803.658883	184426.771944	55.885876
2803.041795	184191.446217	55.890881
2802.159522	183959.013307	55.895885
2801.633715	183719.413933	55.900890
2800.985525	183488.447498	55.905895
2800.297037	183250.593767	55.910900
2799.628877	183011.516859	55.915905
2798.730902	182778.380196	55.920909
2798.114128	182544.513287	55.925914
2797.571550	182314.630224	55.930919
2796.800482	182078.614945	55.935924
2796.164979	181846.090391	55.940929
2795.439128	181618.338919	55.945933
2794.917198	181376.067536	55.950938
2794.255366	181149.478663	55.955943
2793.185105	180916.353724	55.960948
2792.977559	180685.980925	55.965953
2791.892525	180456.384354	55.970957
2791.775013	180222.349017	55.975962
2790.769228	179992.233550	55.980967
2790.053920	179756.743560	55.985972
2789.644000	179525.365958	55.990977
2788.945158	179299.543135	55.995981
2788.529900	179063.678709	56.000986
2787.782415	178837.331799	56.005991
2786.780410	178603.432682	56.010996
2786.420651	178371.570044	56.016001
2785.544960	178126.231232	56.021005
2785.048466	177891.429203	56.026010
2784.319611	177667.718556	56.031015
2783.415197	177433.212650	56.036020
2783.012012	177197.967256	56.041025
2782.203165	176975.951931	56.046029
2781.773858	176739.403169	56.051034
2780.973320	176502.927271	56.056039
2780.426011	176263.372746	56.061044
2779.888021	176039.271748	56.066049
2778.985151	175808.145302	56.071053
2778.525294	175568.212106	56.076058
2777.598098	175330.554689	56.081063
2777.153862	175102.819078	56.086068
2776.719542	174870.758817	56.091073
2775.597669	174635.578259	56.096077
2775.221122	174391.479785	56.101082
2774.217286	174164.308641	56.106087
2773.658561	173925.125713	56.111092
2772.962627	173691.918096	56.116097
2771.919605	173459.987756	56.121101
2771.880263	173225.839429	56.126106
2771.077730	173001.936946	56.131111
2770.402264	172761.647514	56.136116
2769.733723	172533.516769	56.141121
2768.762909	172303.565684	56.146125
2768.015237	172070.172217	56.151130
2767.128817	171846.353101	56.156135
2766.649115	171623.996940	56.161140
2766.316057	171384.513676	56.166145
2765.372869	171169.991204	56.171149
2764.749953	170927.504433	56.176154
2764.009896	170709.035337	56.181159
2763.466220	170489.913205	56.186164
2763.055479	170262.479629	56.191169
2762.255985	170022.124776	56.196173
2761.661215	169787.970330	56.201178
2760.846608	169571.159915	56.206183
2760.301348	169334.965645	56.211188
2759.881480	169105.658187	56.216193
2758.635913	168880.158027	56.221197
2758.546443	168649.033320	56.226202
2758.118115	168425.008673	56.231207
2756.919856	168185.097202	56.236212
2756.301429	167953.500951	56.241217
2755.543343	167728.477156	56.246221
2755.067986	167505.915013	56.251226
2753.795855	167281.750984	56.256231
2753.414355	167041.526595	56.261236
2752.949892	166821.344661	56.266241
2752.255850	166603.095060	56.271245
2751.853916	166370.571348	56.276250
2750.919121	166151.701275	56.281255
2750.031611	165927.865843	56.286260
2749.569066	165695.368631	56.291265
2748.992981	165478.302160	56.296269
2748.279900	165234.225447	56.301274
2747.591105	165023.168494	56.306279
2746.868923	164780.316886	56.311284
2746.182171	164558.632209	56.316289
2745.216107	164341.303565	56.321293
2745.264629	164106.789910	56.326298
2744.449294	163823.982986	56.331303
2743.817312	163594.806274	56.336308
2743.287436	163370.039598	56.341313
2742.538471	163145.804886	56.346317
2741.703799	162908.679688	56.351322
2740.973901	162685.131384	56.356327
2740.238636	162459.029679	56.361332
2739.570745	162239.021661	56.366337
2739.015944	162011.177706	56.371341
2738.665997	161777.327003	56.376346
2737.709326	161557.190884	56.381351
2736.945206	161326.421995	56.386356
2736.244030	161095.250481	56.391361
2735.883722	160876.486181	56.396365
2735.034252	160639.225668	56.401370
2734.488140	160429.698415	56.406375
2733.533242	160196.869252	56.411380
2733.023279	159970.315255	56.416385
2732.237808	159748.052691	56.421389
2731.896217	159517.304854	56.426394
2731.351530	159285.522768	56.431399
2730.423797	159065.028777	56.436404
2729.998062	158838.532255	56.441409
2729.234851	158608.988637	56.446413
2728.827690	158371.965663	56.451418
2727.539072	158153.746649	56.456423
2727.026417	157923.773729	56.461428
2726.797218	157701.346997	56.466433
2726.012943	157470.428497	56.471437
2725.497265	157235.617036	56.476442
2724.808872	157010.979186	56.481447
2724.095118	156778.871849	56.486452
2723.596116	156542.702210	56.491457
2722.510112	156319.403095	56.496461
2721.994849	156077.073737	56.501466
2721.371517	155863.302049	56.506471
2720.378548	155627.344081	56.511476
2720.168816	155398.090007	56.516481
2719.188435	155174.514674	56.521485
2718.541304	154937.095667	56.526490
2717.488880	154714.551719	56.531495
2716.963729	154491.646041	56.536500
2716.477086	154259.443560	56.541505
2715.809925	154032.279604	56.546509
2715.131244	153811.258616	56.551514
2714.534643	153592.259888	56.556519
2713.874979	153371.988742	56.561524
2713.011961	153139.179919	56.566529
2712.614884	152927.856883	56.571533
2711.817470	152696.261013	56.576538
2710.894344	152474.702862	56.581543
2710.312307	152248.134927	56.586548
2710.088216	152014.902246	56.591553
2709.198507	151801.834058	56.596557
2708.880041	151570.767553	56.601562
2707.807433	151348.770316	56.606567
2707.186829	151120.309636	56.611572
2706.653082	150901.712686	56.616577
2706.071823	150674.634291	56.621581
2705.425838	150445.038406	56.626586
2704.669373	150225.667797	56.631591
2703.869698	149994.447119	56.636596
2703.692622	149762.938793	56.641601
2702.533597	149555.647290	56.646605
2702.102434	149309.909360	56.651610
2701.125349	149092.907208	56.656615
2700.585082	148859.721643	56.661620
2699.777971	148635.413083	56.666625
2698.962130	148413.026575	56.671629
2698.730162	148191.781894	56.676634
2697.802187	147969.568727	56.681639
2697.164464	147745.137862	56.686644
2696.563794	147516.750206	56.691649
2695.671368	147307.969389	56.696653
2695.211981	147081.786514	56.701658
2694.556736	146859.410763	56.706663
2693.779799	146635.975613	56.711668
2693.459122	146410.233044	56.716673
2692.563122	146199.363160	56.721677
2692.180787	145970.240338	56.726682
2691.206634	145745.787919	56.731687
2690.436640	145513.756095	56.736692
2690.006857	145284.874515	56.741697
2689.173397	145074.840976	56.746701
2688.542674	144847.430425	56.751706
2688.045893	144633.953486	56.756711
2687.153384	144414.720562	56.761716
2686.639279	144181.616021	56.766721
2685.848410	143968.063155	56.771725
2685.245170	143743.045314	56.776730
2684.545200	143525.046188	56.781735
2683.847992	143295.954705	56.786740
2683.665179	143072.590599	56.791745
2682.587424	142861.911803	56.796749
2681.952441	142624.047549	56.801754
2681.113132	142400.970219	56.806759
2680.490279	142185.598664	56.811764
2679.840315	141966.052403	56.816769
2678.862283	141749.533048	56.821773
2678.797640	141529.427033	56.826778
2678.073949	141312.235150	56.831783
2677.112615	141083.011426	56.836788
2676.471751	140869.824785	56.841793
2675.842335	140664.439422	56.846797
2675.195618	140432.477047	56.851802
2674.638997	140217.375731	56.856807
2674.070236	139996.788919	56.861812
2673.518651	139765.896586	56.866817
2672.651675	139561.585526	56.871821
2672.059418	139330.105811	56.876826
2671.309894	139105.615426	56.881831
2670.559574	138891.138730	56.886836
2670.179918	138668.155788	56.891841
2669.070787	138458.706835	56.896845
2668.589472	138238.919518	56.901850
2668.286662	138007.620162	56.906855
2667.270913	137792.469233	56.911860
2666.754420	137565.031375	56.916865
2665.656772	137350.176139	56.921869
2665.158652	137131.365246	56.926874
2664.721624	136916.154396	56.931879
2664.103257	136695.396574	56.936884
2663.603771	136489.981196	56.941889
2662.440090	136275.296707	56.946893
2662.138441	136042.272055	56.951898
2661.271750	135826.984805	56.956903
2660.643214	135600.926502	56.961908
2659.933229	135390.813579	56.966913
2659.267933	135168.931336	56.971917
2658.811078	134954.894073	56.976922
2657.800297	134739.891753	56.981927
2657.243301	134517.336731	56.986932
2656.585400	134299.359945	56.991937
2656.031363	134098.098673	56.996941
2655.532778	133870.013407	57.001946
2655.041543	133643.364237	57.006951
2653.677937	133426.941317	57.011956
2653.009643	133213.433161	57.016961
2652.014674	133005.974116	57.021965
2651.884702	132791.913789	57.026970
2650.945534	132575.963554	57.031975
2650.373386	132365.114050	57.036980
2649.995221	132150.056241	57.041985
2648.868934	131947.427235	57.046989
2648.481445	131737.709031	57.051994
2647.926485	131525.973853	57.056999
2647.189496	131318.575120	57.062004
2646.953741	131097.024625	57.067009
2645.761537	130883.718553	57.072013
2645.370456	130676.320525	57.077018
2644.594433	130455.826006	57.082023
2643.800434	130243.096770	57.087028
2643.582687	130031.979840	57.092033
2643.075699	129826.778403	57.097037
2642.372571	129598.289844	57.102042
2641.373444	129377.801040	57.107047
2640.724011	129169.769208	57.112052
2640.071574	128948.073055	57.117057
2639.385990	128731.362696	57.122061
2638.987722	128507.877039	57.127066
2637.954898	128299.531434	57.132071
2637.255913	128078.014704	57.137076
2636.640570	127864.868865	57.142081
2635.965597	127664.790203	57.147085
2635.453377	127443.071156	57.152090
2634.681243	127226.221181	57.157095
2633.998493	127010.298562	57.162100
2633.409965	126793.626105	57.167105
2632.641400	126590.242662	57.172109
2632.236660	126365.924470	57.177114
2631.176388	126155.910343	57.182119
2630.331406	125952.721543	57.187124
2630.320153	125734.784916	57.192129
2629.462439	125525.137231	57.197133
2628.483496	125303.776141	57.202138
2628.132232	125098.991548	57.207143
2627.473586	124881.799304	57.212148
2626.669919	124670.092389	57.217153
2625.838021	124471.636649	57.222157
2625.858390	124237.211042	57.227162
2624.943133	124032.498492	57.232167
2623.968042	123817.930100	57.237172
2623.706385	123605.574204	57.242177
2622.724825	123394.540423	57.247181
2622.321062	123174.464381	57.252186
2621.352809	122959.622401	57.257191
2620.707734	122742.038921	57.262196
2620.443165	122535.368051	57.267201
2619.228290	122332.341319	57.272205
2618.771416	122103.546303	57.277210
2618.221823	121892.100399	57.282215
2617.864569	121680.117790	57.287220
2617.088779	121459.581553	57.292225
2616.198673	121254.568868	57.297229
2615.816602	121039.992334	57.302234
2615.050745	120822.646871	57.307239
2614.289250	120601.214025	57.312244
2613.632070	120381.937705	57.317249
2612.842489	120176.688923	57.322253
2612.084105	119956.848128	57.327258
2611.704903	119753.657992	57.332263
2610.546767	119536.423422	57.337268
2610.304137	119316.664975	57.342273
2609.440318	119121.536319	57.347277
2609.007845	118899.818125	57.352282
2608.409752	118692.836637	57.357287
2607.478207	118475.962228	57.362292
2607.473006	118259.577629	57.367297
2606.150491	118059.038611	57.372301
2605.733227	117838.171344	57.377306
2605.204316	117623.766724	57.382311
2604.125305	117405.477338	57.387316
2603.287871	117193.061268	57.392321
2602.610011	116984.493753	57.397325
2601.949633	116775.201528	57.402330
2601.491282	116566.361408	57.407335
2600.597877	116350.838152	57.412340
2600.352760	116143.059463	57.417345
2599.203786	115947.930150	57.422349
2599.020996	115739.319695	57.427354
2598.201469	115524.959612	57.432359
2597.157727	115309.868845	57.437364
2596.881805	115096.644894	57.442369
2595.969358	114897.468349	57.447373
2595.190358	114690.205023	57.452378
2594.538134	114486.217431	57.457383
2593.936470	114286.031683	57.462388
2593.636514	114073.435805	57.467393
2592.693203	113872.069822	57.472397
2591.882998	113657.476522	57.477402
2591.744468	113452.812914	57.482407
2590.943552	113243.000827	57.487412
2590.444872	113036.303254	57.492417
2589.457311	112826.651161	57.497421
2588.848366	112618.070515	57.502426
2588.333453	112407.718710	57.507431
2587.549952	112203.592729	57.512436
2586.994880	111990.661431	57.517441
2586.241785	111789.472425	57.522445
2585.667927	111576.750725	57.527450
2584.819452	111373.117824	57.532455
2584.170753	111159.491347	57.537460
2583.658549	110953.866646	57.542465
2582.780361	110738.122472	57.547469
2582.070414	110529.384960	57.552474
2581.581804	110332.620798	57.557479
2580.729900	110127.323343	57.562484
2580.241779	109918.524114	57.567489
2579.478692	109716.217628	57.572493
2578.851560	109492.575700	57.577498
2578.252872	109291.788685	57.582503
2577.566858	109090.173176	57.587508
2577.032500	108881.110888	57.592513
2576.092642	108679.126531	57.597517
2575.565371	108469.387664	57.602522
2574.880115	108265.392919	57.607527
2574.329020	108067.267180	57.612532
2573.932127	107838.362573	57.617537
2573.007425	107649.880962	57.622541
2572.360191	107441.058317	57.627546
2571.786292	107227.263890	57.632551
2571.034426	107028.144185	57.637556
2570.483160	106813.981804	57.642561
2569.858967	106599.788465	57.647565
2569.035200	106382.145259	57.652570
2568.390875	106184.652478	57.657575
2567.508629	105983.411130	57.662580
2567.133183	105774.179140	57.667585
2566.430827	105569.803781	57.672589
2565.482744	105365.976689	57.677594
2565.016234	105159.714791	57.682599
2564.357132	104953.878563	57.687604
2564.011765	104744.936307	57.692609
2563.127047	104541.214068	57.697613
2562.512697	104320.967846	57.702618
2561.648270	104120.430905	57.707623
2560.885821	103915.476524	57.712628
2560.307273	103706.313885	57.717633
2559.848520	103505.920858	57.722637
2559.130750	103302.994845	57.727642
2558.771653	103089.139910	57.732647
2557.705358	102887.440023	57.737652
2556.924007	102679.771399	57.742657
2556.562243	102469.341925	57.747661
2555.906149	102258.402719	57.752666
2555.348508	102046.491884	57.757671
2554.027716	101843.007925	57.762676
2553.838054	101640.589823	57.767681
2553.083653	101429.806870	57.772685
2552.460246	101223.375802	57.777690
2551.701364	101021.281650	57.782695
2550.930282	100815.702257	57.787700
2550.430735	100606.231170	57.792705
2549.672436	100413.321165	57.797709
2549.086879	100196.667650	57.802714
2548.159244	100001.643858	57.807719
2547.478756	99793.211019	57.812724
2546.971722	99591.971086	57.817729
2546.266061	99397.202644	57.822733
2545.722731	99195.711845	57.827738
2545.068055	98990.891348	57.832743
2544.100711	98790.784294	57.837748
2543.435648	98582.880056	57.842753
2542.359992	98385.540167	57.847757
2542.075438	98189.440281	57.852762
2541.575024	97992.025283	57.857767
2540.856437	97800.570622	57.862772
2540.335022	97589.779383	57.867777
2539.737313	97404.803713	57.872781
2539.086406	97205.630750	57.877786
2538.668168	96996.744066	57.882791
2537.711616	96792.301845	57.887796
2537.203112	96587.714334	57.892801
2536.471663	96389.423833	57.897805
2535.868902	96185.768171	57.902810
2535.165315	95982.948457	57.907815
2534.112789	95786.470901	57.912820
2534.106202	95567.923808	57.917825
2533.398972	95376.919006	57.922829
2532.416429	95175.514280	57.927834
2531.912681	94966.272995	57.932839
2531.286422	94769.381580	57.937844
2530.720685	94553.621875	57.942849
2529.689940	94349.949141	57.947853
2529.089044	94151.689309	57.952858
2528.277307	93951.454363	57.957863
2527.780250	93751.570846	57.962868
2527.333616	93541.211336	57.967873
2526.888573	93343.511031	57.972877
2525.833851	93145.458879	57.977882
2525.217915	92948.676953	57.982887
2524.390978	92737.618003	57.987892
2524.131540	92531.804043	57.992897
2523.100421	92336.951308	57.997901
2522.234390	92131.788886	58.002906
2521.589304	91931.494950	58.007911
2520.909544	91744.194618	58.012916
2520.276489	91535.101101	58.017921
2519.556633	91345.160006	58.022925
2519.146190	91144.056084	58.027930
2518.517855	90944.776622	58.032935
2517.777855	90750.849177	58.037940
2517.123539	90538.845422	58.042945
2516.290217	90362.036861	58.047949
2515.788569	90147.856887	58.052954
2515.577141	89949.065651	58.057959
2514.535619	89757.540744	58.062964
2514.076650	89551.526265	58.067969
2513.114405	89349.131378	58.072973
2512.607757	89144.434393	58.077978
2511.969440	88949.669869	58.082983
2510.986312	88753.205536	58.087988
2510.647713	88562.568753	58.092993
2509.961508	88361.914498	58.097997
2509.130918	88153.429811	58.103002
2508.644796	87948.423832	58.108007
2507.983486	87764.679591	58.113012
2507.391847	87554.470060	58.118017
2506.537899	87353.160705	58.123021
2505.838406	87151.340592	58.128026
2505.479380	86954.020212	58.133031
2504.625394	86754.675378	58.138036
2504.062616	86549.098918	58.143041
2503.187186	86358.408179	58.148045
2502.509575	86154.850606	58.153050
2501.997844	85951.661704	58.158055
2501.157472	85758.720295	58.163060
2500.518178	85558.008628	58.168065
2500.289624	85366.400083	58.173069
2499.178795	85165.240707	58.178074
2498.701174	84970.023909	58.183079
2497.632051	84767.207202	58.188084
2497.459863	84559.248876	58.193089
2496.905219	84375.928776	58.198093
2495.882903	84171.886936	58.203098
2495.603541	83965.643853	58.208103
2494.738254	83775.380270	58.213108
2494.142185	83563.213978	58.218113
2493.276801	83362.444775	58.223117
2492.399293	83176.917042	58.228122
2491.669095	82983.476283	58.233127
2491.006066	82780.531821	58.238132
2490.789857	82582.810942	58.243137
2489.704900	82396.568710	58.248141
2489.371740	82197.811505	58.253146
2488.785909	82004.699117	58.258151
2487.763181	81808.298602	58.263156
2487.309479	81606.422438	58.268161
2486.601204	81416.846119	58.273165
2486.225463	81207.939020	58.278170
2485.534670	81013.223584	58.283175
2484.609236	80815.682503	58.288180
2484.414619	80619.789315	58.293185
2483.437076	80418.375262	58.298189
2482.543995	80217.025822	58.303194
2482.288782	80014.423787	58.308199
2481.623106	79822.484995	58.313204
2480.931275	79617.465437	58.318209
2480.103556	79426.937545	58.323213
2479.319016	79224.338421	58.328218
2478.456936	79025.017231	58.333223
2477.759407	78834.309395	58.338228
2477.271332	78636.890837	58.343233
2476.415915	78446.953051	58.348237
2475.919997	78259.545505	58.353242
2475.521566	78064.374181	58.358247
2474.455893	77875.495245	58.363252
2474.045587	77676.989968	58.368257
2473.232112	77484.411993	58.373261
2472.714922	77286.586459	58.378266
2472.208223	77089.813049	58.383271
2471.052533	76896.806938	58.388276
2471.132886	76694.114653	58.393281
2470.046770	76502.387547	58.398285
2469.522569	76303.286353	58.403290
2469.144176	76101.014851	58.408295
2468.206144	75908.965716	58.413300
2467.725614	75703.324478	58.418305
2466.790887	75523.855758	58.423309
2466.194119	75326.803189	58.428314
2465.585766	75120.953686	58.433319
2464.517857	74919.918402	58.438324
2464.368814	74717.174486	58.443329
2463.377941	74522.422454	58.448333
2462.653697	74335.948858	58.453338
2462.358533	74143.149308	58.458343
2461.614148	73948.300389	58.463348
2460.932786	73745.815357	58.468353
2460.149293	73548.119181	58.473357
2459.603435	73354.302574	58.478362
2459.143313	73152.941493	58.483367
2458.004869	72962.871790	58.488372
2457.537951	72763.036180	58.493377
2456.712802	72570.139368	58.498381
2455.740056	72381.277951	58.503386
2455.288622	72191.252377	58.508391
2454.398895	72000.227486	58.513396
2454.024723	71801.691805	58.518401
2453.313264	71611.003476	58.523405
2452.706508	71426.692209	58.528410
2451.966110	71235.315244	58.533415
2451.376536	71051.334144	58.538420
2450.662650	70857.448080	58.543425
2450.262511	70668.163751	58.548429
2449.581347	70463.608930	58.553434
2449.187029	70263.628559	58.558439
2448.299658	70085.423661	58.563444
2447.197803	69886.509446	58.568449
2446.765405	69687.776142	58.573453
2446.159914	69502.234758	58.578458
2445.646954	69305.114309	58.583463
2444.776591	69123.767351	58.588468
2444.585821	68924.085012	58.593473
2443.909543	68730.378591	58.598477
2443.073340	68534.938617	58.603482
2442.585883	68334.333903	58.608487
2441.457537	68136.119346	58.613492
2441.248200	67931.959427	58.618497
2440.254447	67743.766425	58.623501
2439.537096	67552.104953	58.628506
2438.819987	67355.695196	58.633511
2438.195398	67166.537216	58.638516
2437.658609	66969.197088	58.643521
2436.921576	66782.290025	58.648525
2435.957204	66594.179488	58.653530
2435.757217	66407.241557	58.658535
2434.836791	66220.942137	58.663540
2434.500787	66022.411344	58.668545
2433.515435	65830.989851	58.673549
2432.741125	65631.601613	58.678554
2432.447858	65444.861926	58.683559
2431.576833	65255.267722	58.688564
2430.987630	65057.100474	58.693569
2430.288172	64867.907177	58.698573
2429.678006	64673.284017	58.703578
2429.278538	64486.253834	58.708583
2428.306839	64294.291358	58.713588
2427.476265	64097.403952	58.718593
2426.925615	63915.507254	58.723597
2426.244818	63718.153568	58.728602
2425.792700	63526.860452	58.733607
2424.990960	63341.516789	58.738612
2423.780471	63150.100737	58.743617
2423.568090	62951.879686	58.748621
2423.151639	62764.900689	58.753626
2422.412185	62572.405803	58.758631
2421.389844	62388.891994	58.763636
2420.997856	62192.461259	58.768641
2420.414597	62015.488684	58.773645
2419.585200	61823.810283	58.778650
2418.964604	61619.367828	58.783655
2418.275363	61437.396484	58.788660
2417.923695	61245.755826	58.793665
2417.139006	61056.620205	58.798669
2416.329875	60869.399262	58.803674
2415.944889	60673.055997	58.808679
2415.095602	60483.968019	58.813684
2414.695692	60282.645341	58.818689
2413.798931	60100.270290	58.823693
2413.016537	59915.229334	58.828698
2412.671851	59711.786280	58.833703
2411.485953	59522.197898	58.838708
2411.165593	59329.574667	58.843713
2410.461462	59132.608044	58.848717
2409.811658	58948.043086	58.853722
2409.054751	58753.905991	58.858727
2408.290137	58567.691703	58.863732
2407.853364	58371.463045	58.868737
2407.385608	58185.177020	58.873741
2406.355679	57999.570725	58.878746
2405.898558	57802.199159	58.883751
2405.207192	57611.659204	58.888756
2404.390618	57417.035924	58.893761
2404.079603	57225.344500	58.898765
2403.263485	57039.451201	58.903770
2402.810081	56845.877764	58.908775
2401.935805	56655.294353	58.913780
2401.290988	56453.846114	58.918785
2400.781739	56264.623579	58.923789
2399.553962	56074.080067	58.928794
2399.338154	55878.643466	58.933799
2398.771077	55696.778350	58.938804
2398.113608	55500.732194	58.943809
2397.276120	55310.283448	58.948813
2396.743399	55105.857322	58.953818
2396.050261	54910.566826	58.958823
2394.889086	54727.055454	58.963828
2394.957218	54532.268545	58.968833
2394.067047	54348.933184	58.973837
2393.169935	54159.192568	58.978842
2392.701796	53958.541139	58.983847
2391.840206	53770.808387	58.988852
2391.176612	53577.837505	58.993857
2390.546480	53398.764600	58.998861
2389.587579	53202.977564	59.003866
2389.247398	53011.657504	59.008871
2388.085887	52834.405311	59.013876
2387.759252	52640.128386	59.018881
2387.312459	52465.494069	59.023885
2386.371514	52277.659587	59.028890
2385.667930	52076.351148	59.033895
2385.039494	51894.131806	59.038900
2384.611867	51702.390119	59.043905
2384.075042	51517.451567	59.048909
2383.244323	51333.842953	59.053914
2382.910334	51141.329841	59.058919
2382.140876	50950.194561	59.063924
2381.667079	50756.942043	59.068929
2380.603520	50573.112338	59.073933
2379.704804	50373.426318	59.078938
2379.558397	50178.894187	59.083943
2378.632877	49997.886452	59.088948
2377.771164	49802.358173	59.093953
2377.088199	49616.924503	59.098957
2376.591416	49429.065137	59.103962
2376.015389	49233.358571	59.108967
2375.197083	49057.370438	59.113972
2374.434417	48866.060163	59.118977
2373.765829	48685.211635	59.123981
2373.311230	48508.076650	59.128986
2372.603936	48310.642094	59.133991
2372.044976	48138.019532	59.138996
2371.225639	47938.556938	59.144001
2370.562785	47760.962597	59.149005
2369.978856	47569.758133	59.154010
2369.281452	47373.673701	59.159015
2368.549118	47193.527426	59.164020
2367.729632	47011.258426	59.169025
2367.300021	46828.910501	59.174029
2366.353746	46651.289992	59.179034
2366.107248	46450.453243	59.184039
2365.323406	46264.365179	59.189044
2364.660014	46077.611540	59.194049
2363.825124	45901.799714	59.199053
2363.063857	45715.388075	59.204058
2362.695176	45521.005455	59.209063
2362.071021	45344.419314	59.214068
2361.694967	45155.570803	59.219073
2360.912414	44970.713967	59.224077
2359.905703	44790.075961	59.229082
2359.568591	44593.019657	59.234087
2358.901656	44414.823967	59.239092
2358.097654	44222.371871	59.244097
2357.468044	44034.031113	59.249101
2356.822289	43845.707599	59.254106
2356.138797	43647.483437	59.259111
2355.288597	43478.665759	59.264116
2354.689946	43286.700615	59.269121
2353.906157	43108.182603	59.274125
2353.272657	42929.535065	59.279130
2352.721670	42726.180232	59.284135
2352.139590	42545.491838	59.289140
2351.792721	42370.159991	59.294145
2350.936810	42186.223504	59.299149
2350.253777	41987.989757	59.304154
2349.905742	41801.269830	59.309159
2348.964311	41614.655512	59.314164
2348.025417	41423.580846	59.319169
2347.271208	41237.930705	59.324173
2346.589447	41049.716016	59.329178
2346.037015	40863.652121	59.334183
2345.129900	40688.407232	59.339188
2344.704868	40495.509553	59.344193
2344.200286	40314.067009	59.349197
2342.796887	40141.676378	59.354202
2342.815713	39960.824915	59.359207
2342.022619	39780.862994	59.364212
2341.637071	39593.355614	59.369217
2340.997812	39407.246979	59.374221
2340.001098	39220.509355	59.379226
2339.615286	39029.653461	59.384231
2338.373571	38854.334966	59.389236
2338.204131	38672.897782	59.394241
2337.762891	38491.439237	59.399245
2336.918197	38303.837041	59.404250
2336.110708	38115.661915	59.409255
2335.417727	37937.660634	59.414260
2334.613422	37744.051123	59.419265
2334.475052	37562.563945	59.424269
2333.614602	37376.307092	59.429274
2333.211468	37190.423949	59.434279
2332.312003	37019.418749	59.439284
2331.951396	36827.402787	59.444289
2331.034818	36639.718178	59.449293
2329.965477	36464.747964	59.454298
2329.943401	36263.146930	59.459303
2328.894393	36083.710510	59.464308
2328.429233	35901.576958	59.469313
2327.334025	35715.691782	59.474317
2326.699893	35530.721825	59.479322
2326.477307	35349.621094	59.484327
2325.375770	35170.220141	59.489332
2324.786807	34980.761884	59.494337
2324.077535	34800.604077	59.499341
2323.213204	34623.483657	59.504346
2323.010060	34438.010112	59.509351
2322.052355	34259.476436	59.514356
2321.304363	34074.082277	59.519361
2320.881989	33899.878581	59.524365
2320.073319	33721.821693	59.529370
2319.346741	33535.967054	59.534375
2318.844162	33359.829925	59.539380
2318.285976	33172.056180	59.544385
2318.044797	32994.090908	59.549389
2316.960566	32819.930780	59.554394
2316.461446	32631.049126	59.559399
2315.739896	32445.136347	59.564404
2315.127469	32264.363216	59.569409
2314.288924	32073.975682	59.574413
2313.456580	31894.884935	59.579418
2313.063570	31705.698331	59.584423
2312.046093	31529.490052	59.589428
2311.683720	31352.176329	59.594433
2310.950668	31162.430442	59.599437
2310.131255	30998.254734	59.604442
2309.740155	30819.982650	59.609447
2308.965729	30625.886734	59.614452
2308.284756	30449.385391	59.619457
2307.477550	30264.864896	59.624461
2306.818204	30090.704086	59.629466
2306.278463	29907.044250	59.634471
2305.596420	29739.710276	59.639476
2304.951137	29551.781357	59.644481
2304.625072	29363.991983	59.649485
2303.748198	29199.840209	59.654490
2303.085798	29010.289676	59.659495
2302.402440	28830.565630	59.664500
2301.722551	28648.098669	59.669505
2300.900082	28463.589835	59.674509
2299.963880	28290.988272	59.679514
2299.355916	28104.218670	59.684519
2298.977294	27940.946883	59.689524
2298.461493	27763.061210	59.694529
2297.462717	27576.890476	59.699533
2296.806297	27406.536774	59.704538
2296.312154	27226.558710	59.709543
2295.780826	27050.913969	59.714548
2295.009270	26868.914367	59.719553
2294.261166	26695.254127	59.724557
2293.500139	26527.395394	59.729562
2293.249507	26338.168508	59.734567
2292.163832	26163.422236	59.739572
2291.348489	25987.648471	59.744577
2290.855373	25809.914919	59.749581
2289.669372	25638.704979	59.754586
2289.496846	25464.619159	59.759591
2288.960424	25282.960290	59.764596
2288.373242	25106.156114	59.769601
2287.705751	24933.864445	59.774605
2286.639125	24764.170746	59.779610
2286.414725	24583.475675	59.784615
2285.400720	24414.902742	59.789620
2284.986555	24247.291547	59.794625
2284.448590	24056.728926	59.799629
2283.246183	23886.667237	59.804634
2282.902411	23708.905600	59.809639
2282.148199	23537.732516	59.814644
2281.660652	23374.811691	59.819649
2280.763785	23197.991615	59.824653
2279.833600	23027.805870	59.829658
2279.544187	22847.901185	59.834663
2278.911246	22689.756410	59.839668
2277.707324	22520.823757	59.844673
2277.558736	22353.742288	59.849677
2276.940800	22191.051665	59.854682
2276.419233	21999.514484	59.859687
2275.674367	21830.538466	59.864692
2274.865247	21658.679684	59.869697
2274.352778	21487.833793	59.874701
2273.525261	21320.682170	59.879706
2273.114383	21129.370088	59.884711
2272.272366	20974.178133	59.889716
2271.437701	20788.432937	59.894721
2270.802845	20620.105376	59.899725
2269.988228	20450.363224	59.904730
2269.405643	20289.308301	59.909735
2268.952711	20121.645693	59.914740
2268.213323	19954.470080	59.919745
2267.675549	19786.931476	59.924750
2266.803435	19618.510528	59.929754
2266.330143	19446.630062	59.934759
2265.271836	19274.031479	59.939764
2264.596012	19115.832942	59.944769
2263.916760	18944.041572	59.949774
2263.299032	18786.163993	59.954778
2262.573152	18616.121257	59.959783
2261.885662	18450.565134	59.964788
2261.161158	18282.834979	59.969793
2261.040180	18118.450107	59.974798
2259.900379	17972.299987	59.979802
2259.357221	17797.948939	59.984807
2258.783426	17629.300762	59.989812
2257.808791	17474.115509	59.994817
2257.184650	17302.828792	59.999822
2256.436244	17146.303666	60.004826
2256.115844	16985.900660	60.009831
2255.264696	16828.446581	60.014836
2254.899534	16671.346424	60.019841
2254.104755	16507.429396	60.024846
2253.070255	16338.395466	60.029850
2252.614580	16176.877706	60.034855
2252.024295	16016.982577	60.039860
2251.215857	15856.252283	60.044865
2250.629655	15695.819525	60.049870
2249.756910	15547.973135	60.054874
2249.257780	15380.281955	60.059879
2248.626418	15230.034371	60.064884
2247.878469	15062.880405	60.069889
2247.495212	14904.424224	60.074894
2246.440160	14755.345477	60.079898
2245.827490	14584.317562	60.084903
2244.837153	14431.791469	60.089908
2243.900559	14276.144970	60.094913
2243.591176	14127.299513	60.099918
2242.595182	13983.999778	60.104922
2242.102615	13823.326198	60.109927
2241.442401	13679.900392	60.114932
2240.378036	13533.737622	60.119937
2240.328871	13386.501005	60.124942
2239.390880	13255.576953	60.129946
2238.631111	13098.283475	60.134951
2237.662842	12963.772165	60.139956
2236.886680	12814.423161	60.144961
2236.248746	12680.501172	60.149966
2235.199720	12547.495201	60.154970
2234.875397	12407.547468	60.159975
2234.050023	12276.419218	60.164980
2233.513293	12138.250381	60.169985
2233.017916	12003.193705	60.174990
2232.018716	11868.016530	60.179994
2231.642674	11731.913518	60.184999
2231.168738	11593.820145	60.190004
2230.273804	11455.389410	60.195009
2229.866032	11322.903664	60.200014
2229.070473	11189.243888	60.205018
2228.422625	11045.357230	60.210023
2227.633785	10924.079246	60.215028
2226.846504	10786.667471	60.220033
2226.237701	10652.534406	60.225038
2225.673934	10530.335776	60.230042
2225.017015	10387.697587	60.235047
2224.020192	10262.799071	60.240052
2223.127721	10121.342900	60.245057
2222.611572	10007.808882	60.250062
2221.917366	9884.115505	60.255066
2221.553234	9754.446647	60.260071
2220.709651	9642.908689	60.265076
2219.925713	9508.016261	60.270081
2219.382098	9385.392890	60.275086
2218.381857	9262.610206	60.280090
2217.723843	9136.724018	60.285095
2217.077041	9022.664270	60.290100
2216.136693	8905.606920	60.295105
2215.769615	8785.441347	60.300110
2215.002583	8679.466502	60.305114
2214.325345	8556.435180	60.310119
2213.272307	8452.966474	60.315124
2212.905326	8333.920460	60.320129
2212.412903	8227.091053	60.325134
2211.185249	8113.930333	60.330138
2210.347266	8008.416832	60.335143
2209.757525	7896.883503	60.340148
2208.860077	7798.823180	60.345153
2208.242417	7683.888153	60.350158
2207.458914	7586.660401	60.355162
2206.924641	7489.420169	60.360167
2206.047235	7387.950533	60.365172
2205.264517	7288.301515	60.370177
2204.788878	7188.653353	60.375182
2203.659242	7098.040483	60.380186
2202.910545	7006.981180	60.385191
2202.476090	6916.957269	60.390196
2201.418054	6831.855939	60.395201
2201.053307	6745.802602	60.400206
2200.192410	6674.484594	60.405210
2199.345331	6574.098383	60.410215
2198.680917	6490.629423	60.415220
2198.175445	6420.567301	60.420225
2197.583360	6323.946506	60.425230
2196.437642	6244.646188	60.430234
2195.901861	6169.801849	60.435239
2195.289391	6095.943461	60.440244
2194.717382	6028.410090	60.445249
2194.306483	5946.570737	60.450254
2193.247560	5868.549160	60.455258
2192.940191	5790.772396	60.460263
2192.013980	5720.818974	60.465268
2191.382010	5643.350054	60.470273
2190.930817	5563.096805	60.475278
2190.107750	5496.549083	60.480282
2189.554160	5419.300802	60.485287
2188.608018	5352.659668	60.490292
2187.860509	5285.606339	60.495297
2187.055572	5202.887853	60.500302
2186.063863	5138.320720	60.505306
2185.880171	5069.154925	60.510311
2184.890509	5009.638519	60.515316
2183.939981	4944.056868	60.520321
2183.628931	4884.415946	60.525326
2182.914674	4827.754479	60.530330
2182.298878	4762.787812	60.535335
2181.620827	4703.871553	60.540340
2180.976003	4644.077114	60.545345
2180.583036	4588.355467	60.550350
2179.802168	4526.837598	60.555354
2179.171754	4452.110803	60.560359
2178.418211	4399.915938	60.565364
2177.727823	4339.062808	60.570369
2177.249112	4269.901021	60.575374
2176.447897	4214.199812	60.580378
2175.739252	4151.598597	60.585383
2174.931056	4093.965796	60.590388
2174.364879	4027.750685	60.595393
2173.926570	3973.772143	60.600398
2172.933146	3928.855009	60.605402
2172.404198	3851.320765	60.610407
2171.957579	3799.300956	60.615412
2170.886479	3736.243992	60.620417
2170.769908	3661.202278	60.625422
2170.011492	3622.724761	60.630426
2169.467660	3554.613792	60.635431
2168.562272	3505.320961	60.640436
2167.764481	3443.883648	60.645441
2167.141452	3382.472494	60.650446
2166.238258	3335.513588	60.655450
2165.629552	3280.582722	60.660455
2165.369415	3240.276292	60.665460
2164.454314	3177.572383	60.670465
2163.927689	3110.344051	60.675470
2163.134912	3060.758813	60.680474
2162.795221	3001.397404	60.685479
2162.254230	2942.801625	60.690484
2161.592309	2887.146436	60.695489
2161.080783	2821.473041	60.700494
2160.050771	2770.789194	60.705498
2159.462607	2705.433685	60.710503
2158.492445	2644.212402	60.715508
2157.568303	2587.139398	60.720513
2157.417645	2538.103882	60.725518
2156.516222	2489.812249	60.730522
2156.191622	2423.889370	60.735527
2155.500732	2373.988247	60.740532
2154.557316	2324.242501	60.745537
2154.140640	2265.131296	60.750542
2153.291417	2207.889372	60.755546
2152.895412	2148.763527	60.760551
2152.014471	2100.156852	60.765556
2151.504093	2045.946053	60.770561
2150.883086	1995.984661	60.775566
2150.393159	1931.452151	60.780570
2149.273062	1880.927635	60.785575
2148.834914	1823.078648	60.790580
2147.856364	1774.057186	60.795585
2147.597095	1724.980114	60.800590
2146.488927	1676.445604	60.805594
2146.107731	1623.707093	60.810599
2145.980004	1568.116470	60.815604
2144.613060	1511.721984	60.820609
2144.284686	1451.563863	60.825614
2142.998471	1392.428559	60.830618
2142.572426	1341.936938	60.835623
2141.954731	1303.294947	60.840628
2141.127902	1257.306061	60.845633
2140.976873	1207.612666	60.850638
2140.384989	1157.413745	60.855642
2139.652458	1108.766326	60.860647
2139.131064	1050.666288	60.865652
2138.135386	995.780961	60.870657
2137.555866	944.394043	60.875662
2137.003511	906.304184	60.880666
2136.074866	850.020141	60.885671
2135.621237	799.422016	60.890676
2134.649756	748.597131	60.895681
2134.213297	688.264541	60.900686
2133.317121	658.544985	60.905690
2132.159796	607.685424	60.910695
2131.892994	562.562417	60.915700
2131.072806	513.488536	60.920705
2130.619317	475.222472	60.925710
2129.755587	426.419162	60.930714
2129.153313	378.896083	60.935719
2128.606660	342.857731	60.940724
2127.717515	298.159167	60.945729
2127.208380	255.352793	60.950734
2126.272658	219.906364	60.955738
2125.608966	180.975813	60.960743
2124.903584	133.245965	60.965748
2124.098902	114.564688	60.970753
2123.594437	79.097483	60.975758
2122.745759	48.233839	60.980762
2122.010207	11.817844	60.985767
2121.515713	-26.229073	60.990772
2120.572345	-51.284401	60.995777
2120.121553	-87.950339	61.000782
2118.775148	-116.874595	61.005786
2118.015744	-132.137532	61.010791
2117.054591	-144.603996	61.015796
2115.748195	-133.349953	61.020801
2111.821234	-72.072893	61.025806
2109.422617	5.919305	61.030810
2109.672763	36.168970	61.035815
2110.528416	63.865646	61.040820
2110.783844	79.231628	61.045825
2111.335273	89.162822	61.050830
2111.168246	89.422724	61.055834
2111.258756	67.434414	61.060839
2111.088333	49.061811	61.065844
2110.474552	35.992853	61.070849
2110.114247	21.847596	61.075854
2109.418551	17.756878	61.080858
2108.643333	-2.884389	61.085863
2106.862661	4.327494	61.090868
2104.989934	17.764196	61.095873
2104.475596	23.642854	61.100878
2103.635975	37.421847	61.105882
2103.458919	40.376853	61.110887
2102.927997	45.108519	61.115892
2102.478093	44.727316	61.120897
2102.438419	42.896410	61.125902
2101.875960	40.352081	61.130906
2101.042966	39.105973	61.135911
2100.360585	32.428442	61.140916
2099.152794	42.173560	61.145921
2098.543085	40.532464	61.150926
2098.158708	50.389776	61.155930
2097.557164	50.149336	61.160935
2096.971845	37.217795	61.165940
2095.755009	48.822057	61.170945
2095.724119	51.829565	61.175950
2095.112323	57.126020	61.180954
2094.703507	49.588184	61.185959
2093.726193	49.953019	61.190964
2092.836128	54.535096	61.195969
2092.284798	43.318664	61.200974
2091.224188	53.534035	61.205978
2090.607066	63.175971	61.210983
2090.590036	57.698600	61.215988
2089.913357	64.353690	61.220993
2089.482500	54.570548	61.225998
2088.561227	53.292720	61.231002
2087.443524	58.079664	61.236007
2086.778099	57.089251	61.241012
2085.948378	59.149595	61.246017
2085.781902	55.492145	61.251022
2085.011167	56.406112	61.256026
2084.814307	58.118435	61.261031
2083.771143	56.998728	61.266036
2083.139370	65.734641	61.271041
2082.663847	58.590600	61.276046
2081.735271	60.308655	61.281050
2080.696056	72.634616	61.286055
2080.297708	64.939779	61.291060
2080.199430	65.571984	61.296065
2079.471468	64.913204	61.301070
2078.787620	67.492890	61.306074
2078.038056	64.539850	61.311079
2077.459948	63.950332	61.316084
2076.580722	64.145060	61.321089
2076.143790	56.744155	61.326094
2075.266927	69.638089	61.331098
2074.332379	66.712830	61.336103
2073.734836	66.189477	61.341108
2072.881364	76.194584	61.346113
2073.076272	68.665801	61.351118
2072.518246	76.468261	61.356122
2071.500819	77.774632	61.361127
2070.488871	68.915575	61.366132
2070.248395	73.554639	61.371137
2069.820008	70.128780	61.376142
2068.910070	73.134658	61.381146
2067.845522	75.183391	61.386151
2067.398437	71.945798	61.391156
2066.720329	82.803834	61.396161
2066.426120	76.905231	61.401166
2065.889504	77.953943	61.406170
2065.062068	78.607248	61.411175
2064.592772	77.131536	61.416180
2063.200101	75.925375	61.421185
2062.482722	79.377739	61.426190
2062.175991	88.711806	61.431194
2061.264120	79.705184	61.436199
2061.069051	78.126025	61.441204
2059.947071	79.701314	61.446209
2059.729283	80.018162	61.451214
2059.272569	79.521348	61.456218
2058.349670	86.625551	61.461223
2057.875641	77.339702	61.466228
2056.853846	89.173258	61.471233
2056.665779	71.989348	61.476238
2055.658604	79.825247	61.481242
2055.136712	79.892306	61.486247
2054.374990	78.029330	61.491252
2053.615492	73.429118	61.496257
2053.167291	68.819715	61.501262
2052.253113	83.410920	61.506266
2051.619961	77.551920	61.511271
2051.260390	75.029014	61.516276
2050.360482	78.024634	61.521281
2049.939405	76.120212	61.526286
2049.497426	83.370446	61.531290
2048.395542	84.655537	61.536295
2048.009922	80.329521	61.541300
2046.644248	79.740422	61.546305
2046.687104	82.365636	61.551310
2046.009168	84.975934	61.556314
2044.659638	78.719684	61.561319
2044.427771	86.017000	61.566324
2044.038752	86.231711	61.571329
2043.626746	73.738654	61.576334
2042.110642	78.465058	61.581338
2041.643450	75.788919	61.586343
2041.478328	80.788987	61.591348
2040.410413	88.242651	61.596353
2040.088069	72.513550	61.601358
2038.902394	80.773612	61.606362
2038.425101	82.158277	61.611367
2038.266858	74.866897	61.616372
2037.029367	77.219855	61.621377
2036.759500	77.686900	61.626382
2035.651207	77.571059	61.631386
2035.120344	85.710638	61.636391
2034.783288	83.535831	61.641396
2034.242828	85.580247	61.646401
2033.417490	81.450185	61.651406
2032.590103	92.314579	61.656410
2031.990690	87.377503	61.661415
2031.584818	86.282826	61.666420
2030.452894	89.507673	61.671425
2030.442167	78.870925	61.676430
2029.382357	83.546205	61.681434
2029.148151	94.423689	61.686439
2028.753737	78.481301	61.691444
2027.283821	87.258797	61.696449
2026.268410	79.109166	61.701454
2025.835474	89.024678	61.706458
2025.817064	85.651240	61.711463
2024.668533	76.582059	61.716468
2023.451817	77.651989	61.721473
2023.663337	76.126574	61.726478
2022.996669	82.463907	61.731482
2022.354212	87.143913	61.736487
2021.688466	75.206814	61.741492
2020.835497	89.285253	61.746497
2020.309669	74.867401	61.751502
2019.609785	83.398883	61.756506
2018.886876	86.174026	61.761511
2018.518428	82.214309	61.766516
2018.010483	88.241803	61.771521
2016.750271	83.379653	61.776526
2015.907045	83.989748	61.781530
2015.108608	87.410834	61.786535
2014.916904	82.702374	61.791540
2014.066392	84.986823	61.796545
2013.812038	86.403918	61.801550
2012.728497	81.567347	61.806554
2012.087051	87.910931	61.811559
2011.872115	80.887968	61.816564
2010.784515	95.354538	61.821569
2010.649930	89.783852	61.826574
2010.114871	89.408295	61.831578
2009.464347	86.385934	61.836583
2008.551045	84.427180	61.841588
2007.104250	92.871425	61.846593
2006.588787	84.087341	61.851598
2006.425197	86.825749	61.856602
2005.372145	95.907688	61.861607
2004.872025	85.145185	61.866612
2003.987320	86.799534	61.871617
2004.128309	82.041422	61.876622
2003.469220	83.907548	61.881626
2002.623632	83.835180	61.886631
2002.027418	78.614536	61.891636
2001.385110	91.338016	61.896641
2000.895491	72.189730	61.901646
1999.934918	85.031534	61.906650
1998.612874	84.049169	61.911655
1998.514266	80.887954	61.916660
1997.431042	90.123707	61.921665
1997.149380	76.059779	61.926670
1996.644689	77.269021	61.931674
1995.808828	83.778300	61.936679
1995.643306	81.958694	61.941684
1994.794577	90.464924	61.946689
1993.471290	77.681274	61.951694
1992.862491	80.331074	61.956698
1991.896809	82.860898	61.961703
1992.602069	85.375446	61.966708
1991.457339	82.198929	61.971713
1990.833738	82.905061	61.976718
1989.995292	85.877540	61.981722
1989.245140	82.004437	61.986727
1989.063961	82.660843	61.991732
1987.587831	82.073537	61.996737
1986.694520	78.793246	62.001742
1986.272414	81.853396	62.006746
1985.809299	87.027717	62.011751
1985.104912	81.373225	62.016756
1984.478830	85.253466	62.021761
1984.130570	80.849778	62.026766
1983.625528	80.158794	62.031770
1983.078378	90.124767	62.036775
1982.711781	79.122666	62.041780
1981.182588	88.380327	62.046785
1980.256249	81.433234	62.051790
1979.596206	89.285023	62.056794
1978.985747	90.787034	62.061799
1978.786414	80.204674	62.066804
1977.817493	88.408277	62.071809
1977.420331	85.598815	62.076814
1976.777143	85.437555	62.081818
1976.174949	90.064658	62.086823
1976.141537	83.174527	62.091828
1974.537813	87.925917	62.096833
1973.640280	89.288990	62.101838
1973.207416	88.700093	62.106842
1972.419607	90.750668	62.111847
1972.111124	82.388704	62.116852
1971.608640	89.762885	62.121857
1971.040164	79.595526	62.126862
1970.755872	80.222568	62.131866
1969.782811	85.401355	62.136871
1969.033554	81.580947	62.141876
1967.861723	87.864437	62.146881
1967.339315	77.311288	62.151886
1966.731056	83.685881	62.156890
1966.426494	91.907034	62.161895
1965.743870	85.304469	62.166900
1965.242324	88.789618	62.171905
1964.083815	78.685963	62.176910
1963.437541	85.164366	62.181914
1962.664263	94.660023	62.186919
1962.107682	83.401068	62.191924
1961.347439	86.909149	62.196929
1961.202671	88.711776	62.201934
1960.487748	84.199135	62.206938
1959.999617	93.017150	62.211943
1958.932340	82.899011	62.216948
1958.036603	82.935547	62.221953
1957.343799	80.564906	62.226958
1956.360300	84.814924	62.231962
1955.914380	86.582564	62.236967
1955.802444	83.031583	62.241972
1954.994411	87.736310	62.246977
1954.805548	82.595308	62.251982
1954.215334	81.711263	62.256986
1953.056351	84.959359	62.261991
1952.446883	85.753145	62.266996
1951.395688	89.484040	62.272001
1951.270222	83.933993	62.277006
1950.858072	84.565565	62.282010
1949.875919	85.591984	62.287015
1948.952096	76.387032	62.292020
1947.791397	82.298954	62.297025
1947.667596	84.233085	62.302030
1946.873036	86.719991	62.307034
1946.479705	85.109235	62.312039
1946.075722	84.638764	62.317044
1945.159259	91.197125	62.322049
1944.091849	87.070039	62.327054
1943.275672	85.461754	62.332058
1942.533104	84.215533	62.337063
1942.346135	78.105956	62.342068
1941.779747	94.326216	62.347073
1941.120560	88.016413	62.352078
1940.849727	85.842147	62.357082
1940.426300	90.479513	62.362087
1939.862910	84.041750	62.367092
1938.302461	90.083373	62.372097
1937.560171	85.329861	62.377102
1937.319095	98.081122	62.382106
1936.582262	90.067870	62.387111
1936.105613	78.483204	62.392116
1934.954531	84.354179	62.397121
1934.046208	77.433423	62.402126
1933.844936	86.137296	62.407130
1932.937439	89.225624	62.412135
1932.713849	81.119071	62.417140
1932.114581	89.712660	62.422145
1931.823849	84.587832	62.427150
1930.863721	93.688946	62.432154
1929.492486	95.688648	62.437159
1929.366331	83.711647	62.442164
1928.284758	83.720923	62.447169
1927.913634	91.040349	62.452174
1927.787929	87.759645	62.457178
1927.113456	91.582135	62.462183
1926.233198	85.962678	62.467188
1925.330395	88.260187	62.472193
1924.926455	92.187966	62.477198
1923.850208	86.052406	62.482202
1922.579731	87.356428	62.487207
1922.703918	87.314635	62.492212
1921.393809	86.185331	62.497217
1920.820454	84.959562	62.502222
1920.769384	82.348274	62.507226
1920.178403	90.333405	62.512231
1920.186416	77.571054	62.517236
1919.136203	84.540960	62.522241
1917.956381	79.164615	62.527246
1917.164364	84.294175	62.532250
1916.494881	87.503998	62.537255
1915.930457	82.775874	62.542260
1915.544941	86.949893	62.547265
1915.215820	81.922631	62.552270
1914.131892	71.910461	62.557274
1912.963715	85.823697	62.562279
1912.411069	70.769096	62.567284
1911.611853	85.601494	62.572289
1911.125337	79.093187	62.577294
1910.799183	87.708074	62.582298
1910.142124	89.012488	62.587303
1909.924192	72.387672	62.592308
1909.174710	81.875610	62.597313
1908.379477	80.076349	62.602318
1907.453723	84.195786	62.607322
1906.438238	93.677078	62.612327
1906.266701	79.254267	62.617332
1905.902790	81.352680	62.622337
1905.123867	83.613179	62.627342
1904.332235	85.139239	62.632346
1903.354086	86.199733	62.637351
1903.103149	82.106259	62.642356
1902.276699	93.287507	62.647361
1901.222487	80.264858	62.652366
1900.388911	81.013809	62.657370
1899.627567	90.426365	62.662375
1900.182824	79.587806	62.667380
1899.164868	90.389438	62.672385
1898.399988	87.049362	62.677390
1898.273242	87.884795	62.682394
1896.763788	85.445126	62.687399
1896.148467	79.217478	62.692404
1895.008223	82.891565	62.697409
1894.704420	82.689058	62.702414
1894.193557	78.166909	62.707418
1893.537179	86.050456	62.712423
1893.374610	84.932944	62.717428
1892.584951	87.939495	62.722433
1891.751823	88.084387	62.727438
1891.129714	86.550966	62.732442
1890.120090	93.571213	62.737447
1890.025305	85.980394	62.742452
1888.671583	89.519641	62.747457
1887.816662	78.356182	62.752462
1887.320850	82.306434	62.757466
1886.372442	84.713700	62.762471
1886.754843	82.651775	62.767476
1885.899212	88.201463	62.772481
1885.324075	84.889616	62.777486
1884.682754	81.891061	62.782490
1883.659716	82.436703	62.787495
1882.878454	81.548314	62.792500
1882.160743	85.595302	62.797505
1881.673719	81.883102	62.802510
1881.150208	76.599697	62.807514
1880.635084	84.853491	62.812519
1880.203972	76.407728	62.817524
1879.008243	86.866993	62.822529
1878.420633	83.751099	62.827534
1878.025748	82.277801	62.832538
1877.343881	84.532360	62.837543
1876.470736	84.838157	62.842548
1875.446935	86.628175	62.847553
1874.654476	89.026455	62.852558
1874.279335	72.024475	62.857562
1873.612877	85.944797	62.862567
1873.314542	80.647718	62.867572
1872.527334	89.477742	62.872577
1872.505600	79.929312	62.877582
1871.751843	79.317266	62.882586
1870.498624	83.900305	62.887591
1870.310873	76.619153	62.892596
1869.446676	79.049324	62.897601
1867.989619	78.891156	62.902606
1867.519088	83.371999	62.907610
1866.606507	85.418759	62.912615
1866.405313	71.025906	62.917620
1865.808919	83.798087	62.922625
1865.557632	82.207370	62.927630
1865.467301	81.013733	62.932634
1864.184774	86.353657	62.937639
1863.407370	75.406568	62.942644
1862.441058	77.690524	62.947649
1861.881372	78.596277	62.952654
1861.463326	72.928693	62.957658
1860.499528	85.166261	62.962663
1860.000565	78.413932	62.967668
1859.180121	78.988918	62.972673
1858.558737	76.569118	62.977678
1858.403777	75.850958	62.982682
1857.588737	79.497077	62.987687
1856.872388	81.042736	62.992692
1856.078112	74.479230	62.997697
1855.139985	72.863531	63.002702
1855.071775	73.768519	63.007706
1853.983717	77.569957	63.012711
1853.028268	74.734835	63.017716
1852.674759	84.386998	63.022721
1851.865097	82.430770	63.027726
1851.643383	77.922644	63.032730
1851.010735	80.125238	63.037735
1850.051240	74.078416	63.042740
1849.121165	80.936223	63.047745
1848.185566	89.923860	63.052750
1848.232747	78.409013	63.057754
1847.436911	86.149128	63.062759
1847.356594	71.047937	63.067764
1845.915026	86.485404	63.072769
1845.203941	90.761593	63.077774
1844.764635	81.774648	63.082778
1844.192756	80.646437	63.087783
1843.792035	73.790203	63.092788
1843.106030	85.056391	63.097793
1841.944126	83.452573	63.102798
1841.349705	79.017823	63.107802
1840.721314	91.702051	63.112807
1840.105410	79.849358	63.117812
1840.155534	86.982046	63.122817
1839.112076	87.087811	63.127822
1838.189161	76.330999	63.132826
1837.304600	79.925084	63.137831
1836.848374	73.500301	63.142836
1836.284419	84.772341	63.147841
1835.700303	80.998295	63.152846
1834.624213	78.130296	63.157850
1833.697460	82.600007	63.162855
1833.508758	78.707979	63.167860
1833.327657	84.536934	63.172865
1832.537302	88.467734	63.177870
1831.594073	79.822595	63.182874
1830.248902	84.972202	63.187879
1829.739271	74.556634	63.192884
1829.408065	79.854320	63.197889
1828.892163	80.819361	63.202894
1828.681517	76.459297	63.207898
1828.146530	85.733415	63.212903
1827.444250	81.172289	63.217908
1826.314099	77.240519	63.222913
1825.475556	81.794000	63.227918
1825.506859	76.215921	63.232922
1823.919565	74.824746	63.237927
1823.512145	75.081837	63.242932
1822.837006	79.396475	63.247937
1822.236877	78.733238	63.252942
1821.969098	75.391526	63.257946
1821.240998	81.892407	63.262951
1820.184869	71.426428	63.267956
1819.525369	72.053141	63.272961
1818.970141	77.697070	63.277966
1818.517964	77.716834	63.282970
1817.755164	81.237971	63.287975
1817.391467	74.604528	63.292980
1815.951927	85.544090	63.297985
1815.527947	89.692689	63.302990
1815.119223	74.474913	63.307994
1814.401344	89.273911	63.312999
1814.155538	77.017097	63.318004
1813.299772	77.796407	63.323009
1812.153051	79.779438	63.328014
1811.625175	78.371426	63.333018
1810.877549	80.190153	63.338023
1810.917137	72.044987	63.343028
1810.447711	73.882615	63.348033
1809.298355	78.018665	63.353038
1808.422135	78.608831	63.358042
1808.044682	77.866081	63.363047
1807.204590	73.060336	63.368052
1806.253459	72.268335	63.373057
1805.032840	88.262106	63.378062
1804.763423	73.712937	63.383066
1804.273513	80.388891	63.388071
1804.143861	72.013551	63.393076
1803.707321	77.135572	63.398081
1802.842987	85.993625	63.403086
1802.101660	73.340831	63.408090
1801.267837	82.820105	63.413095
1800.822362	80.261995	63.418100
1800.221401	85.993619	63.423105
1798.737660	81.110312	63.428110
1798.457909	77.242210	63.433114
1797.781401	89.426288	63.438119
1797.444484	79.134691	63.443124
1796.690164	86.210616	63.448129
1796.278759	91.372807	63.453134
1795.317826	82.438750	63.458138
1794.258192	85.688480	63.463143
1793.630519	80.106239	63.468148
1793.562939	77.603239	63.473153
1792.658631	82.805856	63.478158
1791.935053	80.181523	63.483162
1791.187241	89.927851	63.488167
1791.046367	82.962548	63.493172
1790.321248	80.811559	63.498177
1789.330010	82.263691	63.503182
1788.522803	81.496149	63.508186
1787.706730	88.548767	63.513191
1787.448173	81.321449	63.518196
1786.972305	77.426145	63.523201
1786.316086	79.553646	63.528206
1785.475380	78.368790	63.533210
1784.204698	88.685447	63.538215
1784.031904	82.018536	63.543220
1783.513472	84.564139	63.548225
1782.815957	87.472505	63.553230
1782.199377	78.272452	63.558234
1781.389243	81.375327	63.563239
1780.816546	76.870911	63.568244
1780.449436	83.041652	63.573249
1779.033180	81.733731	63.578254
1778.157426	71.280130	63.583258
1777.660114	77.444737	63.588263
1777.922710	71.041432	63.593268
1776.872543	70.129549	63.598273
1776.128769	79.495175	63.603278
1775.859916	79.159394	63.608282
1775.207758	87.073831	63.613287
1774.335169	73.109333	63.618292
1773.636647	77.612202	63.623297
1772.856282	76.889290	63.628302
1771.710529	75.393330	63.633306
1770.638751	76.702137	63.638311
1770.325227	68.523167	63.643316
1769.853631	79.466719	63.648321
1769.457372	79.275755	63.653326
1769.227847	76.183448	63.658330
1768.885870	79.279786	63.663335
1768.071953	72.620083	63.668340
1767.303486	77.014210	63.673345
1766.427828	82.131858	63.678350
1765.967406	68.672781	63.683354
1764.450163	82.622572	63.688359
1763.755268	76.707232	63.693364
1763.529815	76.821888	63.698369
1762.771743	74.866959	63.703374
1762.868016	76.334045	63.708378
1761.440451	81.184523	63.713383
1760.903912	83.818163	63.718388
1760.416292	77.259607	63.723393
1759.700137	79.863424	63.728398
1759.307381	80.026730	63.733402
1758.139356	91.839434	63.738407
1757.239768	80.236836	63.743412
1756.608961	81.521346	63.748417
1756.109791	79.375484	63.753422
1756.080231	81.718865	63.758426
1755.442480	76.677570	63.763431
1754.441331	81.023499	63.768436
1753.636496	76.333603	63.773441
1753.007736	82.654714	63.778446
1752.675990	80.296176	63.783450
1751.557372	86.619394	63.788455
1750.680330	80.245694	63.793460
1749.763593	77.219956	63.798465
1749.271795	75.799920	63.803470
1749.216324	78.702518	63.808474
1748.503075	88.224160	63.813479
1748.485968	80.439669	63.818484
1747.887785	72.302759	63.823489
1747.006524	77.973249	63.828494
1746.079295	70.904186	63.833498
1744.646768	78.529394	63.838503
1743.951483	80.216819	63.843508
1743.521645	82.324145	63.848513
1742.973294	77.363275	63.853518
1742.887271	69.758474	63.858522
1741.857629	76.209489	63.863527
1741.013123	75.556699	63.868532
1740.446764	74.176894	63.873537
1739.771431	75.624602	63.878542
1739.361258	75.420083	63.883546
1738.868186	79.104986	63.888551
1737.949768	76.868017	63.893556
1736.954064	67.527924	63.898561
1736.375501	70.307015	63.903566
1736.304506	80.510412	63.908570
1734.713867	83.798770	63.913575
1734.066043	79.809360	63.918580
1733.594775	71.083002	63.923585
1733.162307	78.468949	63.928590
1733.037863	73.538527	63.933594
1732.531796	78.845069	63.938599
1731.604779	79.086928	63.943604
1730.657127	74.402377	63.948609
1730.002419	83.365927	63.953614
1729.151446	82.630587	63.958618
1728.153288	77.726971	63.963623
1727.451386	77.076768	63.968628
1726.844731	81.284352	63.973633
1726.350352	79.525676	63.978638
1726.297408	74.867757	63.983642
1726.108049	86.542370	63.988647
1724.921509	85.619050	63.993652
1724.067928	81.391080	63.998657
1723.583111	82.635063	64.003662
1723.130559	81.177258	64.008666
1721.890479	87.768945	64.013671
1721.002321	73.548318	64.018676
1720.620029	83.604036	64.023681
1719.955881	83.223812	64.028686
1719.668487	76.814818	64.033690
1718.288658	81.753932	64.038695
1717.715056	78.377228	64.043700
1717.219027	84.158432	64.048705
1716.539104	87.109753	64.053710
1716.492365	74.302512	64.058714
1715.337874	83.605652	64.063719
1714.151366	89.009241	64.068724
1714.128874	85.649081	64.073729
1713.278207	88.335779	64.078734
1713.086466	76.183945	64.083738
1712.397130	75.328317	64.088743
1711.426135	81.866225	64.093748
1710.747862	82.357172	64.098753
1709.949004	82.086659	64.103758
1709.626744	76.738216	64.108762
1709.010824	81.992823	64.113767
1707.878935	78.356284	64.118772
1707.442377	72.087686	64.123777
1706.714100	85.342889	64.128782
1706.489728	87.075376	64.133786
1705.833467	77.965233	64.138791
1704.826295	80.722525	64.143796
1703.940331	78.939319	64.148801
1703.530081	85.244655	64.153806
1703.280094	82.739093	64.158810
1701.901679	85.148491	64.163815
1701.207501	78.605413	64.168820
1700.682554	72.751413	64.173825
1700.304822	82.218187	64.178830
1700.053787	71.947671	64.183834
1698.816439	77.819819	64.188839
1698.083963	73.167337	64.193844
1697.295513	78.449351	64.198849
1696.997768	75.312694	64.203854
1696.422345	76.695656	64.208858
1695.871229	86.182089	64.213863
1694.919778	80.745928	64.218868
1694.691790	84.866561	64.223873
1693.873979	89.112426	64.228878
1692.895946	82.164995	64.233882
1691.898700	80.005221	64.238887
1691.527227	77.526844	64.243892
1691.189056	78.878428	64.248897
1690.533577	80.543774	64.253902
1689.369940	84.049767	64.258906
1688.524943	83.983714	64.263911
1688.222159	77.277542	64.268916
1687.785615	74.822118	64.273921
1687.488881	77.047084	64.278926
1686.846946	80.055455	64.283930
1685.580799	76.697304	64.288935
1684.738251	70.458509	64.293940
1684.657487	71.788129	64.298945
1683.452607	84.196501	64.303950
1682.459393	77.898056	64.308954
1681.701656	79.825659	64.313959
1681.345336	69.401557	64.318964
1681.294572	78.313330	64.323969
1680.540034	84.138757	64.328974
1680.571662	79.896348	64.333978
1679.223106	82.316783	64.338983
1678.284743	77.807401	64.343988
1678.019841	73.634176	64.348993
1677.294397	75.957206	64.353998
1676.376984	69.671959	64.359002
1675.434241	76.818838	64.364007
1674.792894	80.888436	64.369012
1674.615347	79.754396	64.374017
1674.274142	82.644034	64.379022
1673.541282	76.267965	64.384026
1672.284624	76.179000	64.389031
1671.579813	80.974636	64.394036
1671.203147	65.231416	64.399041
1670.384958	78.362125	64.404046
1669.561314	73.561705	64.409050
1669.078170	73.796154	64.414055
1668.409456	78.822605	64.419060
1668.311426	74.507752	64.424065
1667.366505	87.529289	64.429070
1666.579208	74.473835	64.434074
1665.551158	83.703288	64.439079
1665.088514	79.722329	64.444084
1664.964268	82.692624	64.449089
1663.832879	83.190906	64.454094
1662.945572	78.211360	64.459098
1662.185207	77.412763	64.464103
1662.082218	78.124578	64.469108
1661.717176	76.624498	64.474113
1660.805356	83.227141	64.479118
1659.909396	75.788860	64.484122
1659.144148	85.533247	64.489127
1658.746009	79.919314	64.494132
1658.261233	75.818868	64.499137
1657.207566	81.530965	64.504142
1656.586553	77.996225	64.509146
1655.799288	81.825650	64.514151
1655.074191	82.544828	64.519156
1654.851554	75.532610	64.524161
1653.427459	84.851792	64.529166
1653.183969	68.267381	64.534170
1652.223980	74.325726	64.539175
1652.007399	79.354473	64.544180
1651.716200	74.551477	64.549185
1651.013326	80.930112	64.554190
1650.222009	82.211759	64.559194
1649.427820	81.614086	64.564199
1648.718916	89.658988	64.569204
1648.713780	74.366113	64.574209
1647.309865	84.390162	64.579214
1646.658443	73.349033	64.584218
1646.061456	74.650273	64.589223
1645.390121	81.938555	64.594228
1644.691870	75.121748	64.599233
1643.705169	86.183415	64.604238
1643.231072	77.206785	64.609242
1643.029061	74.526449	64.614247
1642.412990	72.329796	64.619252
1641.311962	77.620479	64.624257
1640.392684	77.629323	64.629262
1640.411546	74.628462	64.634266
1640.063775	85.716362	64.639271
1639.047860	75.597332	64.644276
1638.218408	72.385879	64.649281
1637.113746	76.992725	64.654286
1636.948063	84.151791	64.659290
1636.345571	79.508641	64.664295
1635.179760	79.487265	64.669300
1634.791088	72.104026	64.674305
1634.060802	78.974309	64.679310
1633.699549	71.219276	64.684314
1633.160670	84.977423	64.689319
1632.012079	78.238472	64.694324
1631.341811	74.030303	64.699329
1630.558546	86.977278	64.704334
1630.647105	85.651150	64.709338
1629.586853	84.805585	64.714343
1628.784872	79.970196	64.719348
1627.890345	83.140139	64.724353
1627.330239	85.433762	64.729358
1627.199593	73.202854	64.734362
1626.668763	71.058896	64.739367
1625.144978	73.429924	64.744372
1624.809903	70.326018	64.749377
1624.147009	78.071866	64.754382
1624.124029	79.215684	64.759386
1622.760163	75.073555	64.764391
1622.306497	83.270302	64.769396
1621.631957	76.247880	64.774401
1620.830148	78.079996	64.779406
1620.757030	70.995144	64.784410
1619.581307	74.957257	64.789415
1619.120802	81.682178	64.794420
1618.740855	72.996537	64.799425
1617.497796	74.233266	64.804430
1616.331693	78.004614	64.809434
1615.838927	76.873349	64.814439
1615.049980	76.104539	64.819444
1614.904846	75.864239	64.824449
1613.957042	82.556192	64.829454
1614.162802	70.771749	64.834458
1613.570819	85.274790	64.839463
1613.055046	79.728443	64.844468
1612.480061	70.977595	64.849473
1611.202991	78.928259	64.854478
1610.203048	72.359675	64.859482
1609.474515	84.246102	64.864487
1608.782674	76.089420	64.869492
1608.707818	77.886470	64.874497
1607.794385	88.687343	64.879502
1607.132854	77.023342	64.884506
1606.319301	81.806306	64.889511
1605.666790	77.689942	64.894516
1605.402367	78.607185	64.899521
1604.540376	81.339870	64.904526
1603.398054	76.676839	64.909530
1603.235056	85.436127	64.914535
1602.883116	90.502154	64.919540
1602.379191	78.287974	64.924545
1600.689216	87.160557	64.929550
1600.073575	78.353088	64.934554
1599.922112	72.133838	64.939559
1599.392354	80.992396	64.944564
1598.955706	70.374492	64.949569
1597.356230	86.855880	64.954574
1597.072945	82.702932	64.959578
1596.612061	83.250834	64.964583
1596.258587	78.818872	64.969588
1595.378029	74.223069	64.974593
1594.194193	82.685644	64.979598
1594.013807	73.534628	64.984602
1593.687942	87.765150	64.989607
1592.550648	78.731475	64.994612
1591.857560	70.095595	64.999617
1590.920282	84.137822	65.004622
1590.785717	75.403737	65.009626
1590.294965	72.600545	65.014631
1589.121690	70.113960	65.019636
1588.498463	68.511408	65.024641
1587.791062	79.096612	65.029646
1587.518408	79.441139	65.034650
1586.843334	74.101466	65.039655
1585.702338	76.995183	65.044660
1585.169354	75.854544	65.049665
1584.568986	76.430919	65.054670
1584.147894	76.605061	65.059674
1583.366453	88.421051	65.064679
1582.335437	84.334869	65.069684
1581.933777	76.900087	65.074689
1581.322695	81.258216	65.079694
1581.017254	78.302576	65.084698
1580.049248	82.895617	65.089703
1579.195647	77.511770	65.094708
1578.847016	79.524213	65.099713
1577.866482	76.936043	65.104718
1577.466739	77.836941	65.109722
1576.681447	78.084722	65.114727
1575.850704	74.260046	65.119732
1575.376590	78.121738	65.124737
1574.737516	76.928570	65.129742
1574.626458	76.867367	65.134746
1573.452995	83.587302	65.139751
1572.506911	82.476033	65.144756
1571.907416	69.963234	65.149761
1571.339906	73.830303	65.154766
1571.457739	80.464913	65.159770
1570.174319	75.521535	65.164775
1569.146129	81.638055	65.169780
1568.979596	70.248669	65.174785
1568.346217	84.160609	65.179790
1567.487607	74.004007	65.184794
1566.788985	77.677439	65.189799
1566.196574	85.639188	65.194804
1565.633718	70.021778	65.199809
1564.703958	82.906880	65.204814
1563.934331	77.605892	65.209818
1563.526391	74.776932	65.214823
1562.916366	81.393149	65.219828
1562.654763	73.169700	65.224833
1561.386320	80.563913	65.229838
1560.762842	71.420231	65.234842
1560.109666	79.224471	65.239847
1559.888015	85.908294	65.244852
1559.057422	79.508368	65.249857
1557.686324	82.900719	65.254862
1557.309513	80.934158	65.259866
1556.569074	81.963314	65.264871
1556.548563	78.758971	65.269876
1556.168570	80.372689	65.274881
1554.614978	77.921319	65.279886
1554.144979	76.278658	65.284890
1553.781885	75.984684	65.289895
1553.133007	80.441867	65.294900
1552.029526	80.509974	65.299905
1551.305730	81.921274	65.304910
1551.005619	77.845127	65.309914
1550.574241	80.039459	65.314919
1550.084393	85.427031	65.319924
1548.961095	68.804250	65.324929
1548.159303	76.212627	65.329934
1547.654283	75.927014	65.334938
1547.506833	74.934861	65.339943
1546.365882	74.494826	65.344948
1546.067199	73.878374	65.349953
1545.038628	72.731337	65.354958
1544.361960	73.226802	65.359962
1543.517876	81.173349	65.364967
1542.722120	85.090888	65.369972
1542.348129	73.302374	65.374977
1541.365694	86.440288	65.379982
1541.073935	78.466066	65.384986
1540.936364	76.852586	65.389991
1539.630394	82.182181	65.394996
1539.142773	76.771734	65.400001
1538.372575	70.674468	65.405006
1538.005425	70.354333	65.410010
1537.006200	73.447897	65.415015
1536.112692	69.705751	65.420020
1535.787157	71.787069	65.425025
1535.113709	74.950294	65.430030
1534.902387	72.895938	65.435034
1534.111547	82.527715	65.440039
1533.109904	81.846347	65.445044
1532.770961	71.842154	65.450049
1531.094246	81.810251	65.455054
1530.650120	75.986030	65.460058
1530.112348	83.035484	65.465063
1529.514817	86.517817	65.470068
1529.187271	71.724065	65.475073
1528.463553	77.555665	65.480078
1528.591630	81.701726	65.485082
1527.462786	80.597438	65.490087
1526.538770	78.295205	65.495092
1526.347680	73.030034	65.500097
1525.080901	84.620374	65.505102
1524.575604	78.645021	65.510106
1524.042365	78.860649	65.515111
1522.983979	73.266511	65.520116
1522.886176	76.243644	65.525121
1521.665606	79.566358	65.530126
1521.169981	74.535666	65.535130
1520.571765	83.474501	65.540135
1519.976562	84.736060	65.545140
1519.356816	71.461656	65.550145
1518.483405	78.569178	65.555150
1517.775434	78.072965	65.560154
1517.180939	79.526806	65.565159
1516.570329	79.847773	65.570164
1516.371118	71.950318	65.575169
1515.017637	76.689793	65.580174
1514.392992	80.840350	65.585178
1513.794929	80.866004	65.590183
1513.303604	82.448533	65.595188
1513.177366	76.793002	65.600193
1511.730547	81.533120	65.605198
1511.201017	75.578970	65.610202
1510.945368	76.553176	65.615207
1510.154051	88.976313	65.620212
1509.620201	78.358105	65.625217
1508.810502	84.368960	65.630222
1508.382818	71.187044	65.635226
1507.382991	73.012813	65.640231
1506.066916	86.014517	65.645236
1505.776535	67.963111	65.650241
1504.926457	76.609224	65.655246
1504.705520	76.106581	65.660250
1504.392612	77.859459	65.665255
1503.616818	83.640993	65.670260
1502.726833	81.109428	65.675265
1501.837495	80.099557	65.680270
1501.852675	80.783137	65.685274
1501.376434	85.745919	65.690279
1500.124161	86.283984	65.695284
1499.786896	78.843717	65.700289
1498.960317	83.720246	65.705294
1498.192357	82.039789	65.710298
1497.322881	77.771853	65.715303
1496.691673	77.651387	65.720308
1496.571477	80.310372	65.725313
1495.586711	83.743862	65.730318
1494.577884	80.024788	65.735322
1494.213266	76.662240	65.740327
1493.887120	77.319637	65.745332
1493.013947	62.492765	65.750337
1491.967060	77.213184	65.755342
1491.144242	73.343123	65.760346
1490.785243	76.434307	65.765351
1490.136614	80.322169	65.770356
1490.167163	75.786619	65.775361
1488.598677	70.197870	65.780366
1487.885508	76.556094	65.785370
1487.386188	70.448914	65.790375
1486.717206	75.912270	65.795380
1486.615518	75.464795	65.800385
1485.629540	75.230399	65.805390
1484.866728	81.435662	65.810394
1484.639961	73.613555	65.815399
1483.706242	80.202379	65.820404
1482.738456	78.604149	65.825409
1481.926809	79.695106	65.830414
1481.800894	75.461973	65.835418
1481.600337	74.041439	65.840423
1480.005976	84.122636	65.845428
1479.718658	72.728806	65.850433
1478.789312	78.348663	65.855438
1478.335964	78.023312	65.860442
1478.070514	75.245840	65.865447
1476.680393	82.467034	65.870452
1476.259153	75.871194	65.875457
1475.493194	85.051166	65.880462
1475.493494	71.517382	65.885466
1474.753866	71.335303	65.890471
1473.522647	82.694499	65.895476
1473.200626	75.928346	65.900481
1472.573009	79.251463	65.905486
1471.444749	75.440992	65.910490
1470.464307	73.830586	65.915495
1469.772686	80.073423	65.920500
1469.876428	65.561241	65.925505
1469.483702	80.584565	65.930510
1468.759423	75.262212	65.935514
1467.657679	79.293058	65.940519
1467.062726	77.394299	65.945524
1466.589073	75.495186	65.950529
1466.013660	78.262792	65.955534
1465.262416	70.836291	65.960538
1464.216943	72.505324	65.965543
1463.469492	78.036351	65.970548
1463.263660	69.072335	65.975553
1462.505648	73.792890	65.980558
1461.453982	81.759832	65.985562
1461.154098	69.529047	65.990567
1460.434510	71.491648	65.995572
1460.212607	70.065047	66.000577
1459.450740	79.403643	66.005582
1458.445203	65.480938	66.010586
1457.922875	79.439891	66.015591
1457.183879	80.309569	66.020596
1456.308914	67.917869	66.025601
1455.263514	73.937809	66.030606
1454.941042	68.540562	66.035610
1454.964751	73.113219	66.040615
1454.054332	73.970718	66.045620
1453.555638	60.866349	66.050625
1452.564701	74.721577	66.055630
1451.929940	65.333719	66.060634
1451.705468	74.049147	66.065639
1450.977591	79.299516	66.070644
1450.273012	71.056608	66.075649
1449.324986	81.598076	66.080654
1448.112977	73.524129	66.085658
1447.414346	75.601676	66.090663
1446.616706	78.822509	66.095668
1446.334152	72.151018	66.100673
1446.381483	79.550618	66.105678
1445.588786	83.388847	66.110682
1445.313427	78.898765	66.115687
1444.027994	73.742884	66.120692
1443.387537	68.060282	66.125697
1442.684462	75.038243	66.130702
1441.678802	71.449581	66.135706
1441.017477	77.469983	66.140711
1439.998546	72.828424	66.145716
1440.036450	75.198923	66.150721
1439.610919	75.269713	66.155726
1439.363260	78.657027	66.160730
1438.256256	77.298568	66.165735
1437.492787	76.159901	66.170740
1437.065340	74.784896	66.175745
1436.004413	73.400190	66.180750
1435.223930	76.258745	66.185754
1434.779911	67.614876	66.190759
1434.263771	79.801887	66.195764
1433.905572	76.913004	66.200769
1432.558881	71.924566	66.205774
1432.101497	74.200320	66.210778
1431.456885	68.043708	66.215783
1430.521119	74.524058	66.220788
1430.029368	72.202043	66.225793
1429.130290	72.311832	66.230798
1428.367875	75.878739	66.235802
1428.126759	73.743972	66.240807
1427.908472	78.747764	66.245812
1427.341745	76.063919	66.250817
1426.188770	72.875579	66.255822
1425.641349	70.221784	66.260826
1424.791016	71.877161	66.265831
1423.529305	69.051467	66.270836
1423.354455	68.664512	66.275841
1422.638532	72.835902	66.280846
1422.470405	68.492789	66.285850
1421.894953	72.211332	66.290855
1420.408518	75.473845	66.295860
1420.102611	72.502535	66.300865
1419.567452	68.744476	66.305870
1419.256607	76.995808	66.310874
1419.085039	69.775236	66.315879
1417.159823	73.397661	66.320884
1417.041075	68.357555	66.325889
1416.274453	75.284120	66.330894
1414.961264	74.590817	66.335898
1414.543708	70.787258	66.340903
1414.053346	78.901541	66.345908
1413.769517	71.146867	66.350913
1412.919148	76.700572	66.355918
1412.626044	80.511438	66.360922
1411.851263	76.170134	66.365927
1411.049293	79.402704	66.370932
1410.627254	71.200056	66.375937
1409.263955	73.026866	66.380942
1408.237715	72.955021	66.385946
1408.132019	68.701336	66.390951
1407.380399	79.747770	66.395956
1407.019979	69.117804	66.400961
1406.738210	75.700790	66.405966
1406.184536	68.312295	66.410970
1405.325791	71.680049	66.415975
1404.533324	79.250984	66.420980
1403.929478	78.772946	66.425985
1402.871560	71.335291	66.430990
1401.981207	73.429132	66.435994
1401.951122	74.181407	66.440999
1401.326754	80.528689	66.446004
1400.304353	77.217100	66.451009
1399.316431	81.455389	66.456014
1398.713455	84.675255	66.461018
1398.591256	75.548139	66.466023
1397.868913	81.540403	66.471028
1397.267835	75.665468	66.476033
1396.379484	78.515948	66.481038
1395.572385	82.801190	66.486042
1395.193777	74.246280	66.491047
1394.548914	81.801641	66.496052
1393.634723	75.260526	66.501057
1392.911368	77.219013	66.506062
1392.302602	75.552709	66.511066
1392.463156	68.285655	66.516071
1391.276382	79.998943	66.521076
1390.637414	67.442025	66.526081
1389.840904	63.205114	66.531086
1389.139621	80.941019	66.536090
1388.144111	68.152189	66.541095
1387.351369	77.530400	66.546100
1386.927428	78.542408	66.551105
1386.338618	70.962379	66.556110
1386.061722	79.561562	66.561114
1385.753676	76.831875	66.566119
1384.491811	74.140269	66.571124
1384.101059	75.314163	66.576129
1383.456161	74.904158	66.581134
1382.662701	76.069527	66.586138
1381.912313	69.262678	66.591143
1381.100864	71.547415	66.596148
1380.771319	70.898042	66.601153
1380.076564	72.583896	66.606158
1379.086386	74.849736	66.611162
1378.777536	70.869627	66.616167
1377.942244	76.308978	66.621172
1377.313147	74.414094	66.626177
1376.270361	78.593300	66.631182
1375.168588	80.014269	66.636186
1374.931725	75.306763	66.641191
1374.470668	87.163322	66.646196
1374.354410	75.292880	66.651201
1373.979189	78.503353	66.656206
1372.706397	81.320336	66.661210
1372.000592	68.679430	66.666215
1371.499609	71.936702	66.671220
1370.932633	72.462084	66.676225
1369.687502	72.010304	66.681230
1369.129884	74.554320	66.686234
1368.825963	72.476854	66.691239
1368.194227	77.756113	66.696244
1367.407170	80.554230	66.701249
1366.509033	79.837549	66.706254
1365.742963	80.112301	66.711258
1365.651662	74.019138	66.716263
1364.864911	86.335913	66.721268
1364.049536	76.040059	66.726273
1363.010929	79.638275	66.731278
1362.646344	80.472113	66.736282
1362.394875	79.252076	66.741287
1361.477614	82.034622	66.746292
1360.587571	79.693935	66.751297
1359.908039	73.404120	66.756302
1359.443233	74.827915	66.761306
1359.353013	78.308479	66.766311
1358.141354	83.944869	66.771316
1357.340624	72.683152	66.776321
1356.984485	73.816853	66.781326
1356.128265	71.317824	66.786330
1355.563541	66.656137	66.791335
1354.948910	74.119960	66.796340
1354.498651	70.334228	66.801345
1354.053145	78.647972	66.806350
1352.711801	74.797315	66.811354
1352.023528	74.961929	66.816359
1351.468746	84.518369	66.821364
1350.966367	82.530803	66.826369
1349.690124	74.082338	66.831374
1348.656623	75.082446	66.836378
1348.779984	74.919329	66.841383
1348.229790	76.921263	66.846388
1347.972925	72.710539	66.851393
1347.331220	76.427014	66.856398
1346.125918	76.320581	66.861402
1345.613737	74.274651	66.866407
1345.005218	70.052023	66.871412
1344.265375	80.560420	66.876417
1343.254486	67.900218	66.881422
1342.601106	78.133087	66.886426
1342.459655	77.712442	66.891431
1341.844486	74.249403	66.896436
1340.982251	79.757706	66.901441
1340.169349	72.771571	66.906446
1339.379243	76.689840	66.911450
1339.166813	74.891153	66.916455
1338.648861	80.382569	66.921460
1337.904204	77.693917	66.926465
1336.962787	80.593855	66.931470
1336.104470	80.832818	66.936474
1336.013098	70.521226	66.941479
1334.735397	83.780247	66.946484
1334.179988	76.961338	66.951489
1333.648038	79.414546	66.956494
1333.317224	75.876339	66.961498
1332.881061	68.888662	66.966503
1332.014916	69.199835	66.971508
1331.166913	75.019696	66.976513
1330.079627	68.712716	66.981518
1328.898329	77.894088	66.986522
1328.716078	72.092939	66.991527
1328.110035	75.431579	66.996532
1327.956636	75.708286	67.001537
1327.740134	78.237503	67.006542
1326.789719	70.599864	67.011546
1325.934599	62.975463	67.016551
1324.935235	75.374926	67.021556
1324.681579	75.702267	67.026561
1323.729956	73.659973	67.031566
1322.518881	70.778972	67.036570
1322.418184	74.609715	67.041575
1322.020054	78.506672	67.046580
1321.294802	74.556504	67.051585
1320.684812	81.434535	67.056590
1319.570014	85.817606	67.061594
1319.242062	71.148563	67.066599
1318.628068	79.749301	67.071604
1317.839130	77.723723	67.076609
1317.162220	85.199036	67.081614
1316.501733	86.466289	67.086618
1316.148609	76.962728	67.091623
1314.835579	75.564538	67.096628
1313.962206	72.681889	67.101633
1313.680259	77.941816	67.106638
1313.018108	81.754593	67.111642
1312.973976	77.680364	67.116647
1312.374489	70.565691	67.121652
1311.494160	71.399532	67.126657
1310.749003	73.419854	67.131662
1309.926003	72.041529	67.136666
1308.901357	66.907342	67.141671
1308.014625	76.231124	67.146676
1308.048650	71.977311	67.151681
1307.538274	68.650589	67.156686
1306.888219	70.980650	67.161690
1305.787904	71.007358	67.166695
1305.013066	72.619230	67.171700
1304.630154	62.243613	67.176705
1304.442086	72.150184	67.181710
1303.300754	72.125066	67.186714
1302.578871	73.794753	67.191719
1301.552083	76.343991	67.196724
1301.487434	72.870705	67.201729
1301.002685	75.554539	67.206734
1299.690041	69.428489	67.211738
1299.161683	72.858864	67.216743
1298.504765	75.067014	67.221748
1298.314588	68.268898	67.226753
1297.592390	71.077220	67.231758
1296.438285	83.643229	67.236762
1295.919181	72.447150	67.241767
1295.470710	71.838775	67.246772
1295.155686	75.003414	67.251777
1294.014765	73.847535	67.256782
1293.136569	72.865930	67.261786
1292.842964	72.207701	67.266791
1292.309486	76.588238	67.271796
1291.310306	75.375129	67.276801
1290.742654	75.544236	67.281806
1289.814868	75.064115	67.286810
1289.665636	80.911659	67.291815
1288.925959	72.936169	67.296820
1287.955944	65.525599	67.301825
1287.387478	69.435448	67.306830
1286.949612	80.178120	67.311834
1286.471731	77.506992	67.316839
1285.385413	78.966542	67.321844
1284.928429	73.885609	67.326849
1284.271600	71.704994	67.331854
1283.244924	74.907093	67.336858
1282.449058	69.988858	67.341863
1281.698894	83.561418	67.346868
1281.060031	74.090685	67.351873
1280.672209	70.632517	67.356878
1280.026692	75.606470	67.361882
1280.156626	69.128049	67.366887
1279.026774	77.514342	67.371892
1278.228598	78.622144	67.376897
1277.793600	72.616757	67.381902
1276.876284	67.601139	67.386906
1276.362904	72.106217	67.391911
1275.106978	71.227260	67.396916
1274.740599	70.145356	67.401921
1274.501305	70.623385	67.406926
1273.648165	77.901215	67.411930
1273.041260	72.948205	67.416935
1272.192717	79.495161	67.421940
1271.841029	71.096855	67.426945
1271.460619	74.489517	67.431950
1270.014210	77.349923	67.436954
1269.488834	68.340558	67.441959
1268.745926	76.619594	67.446964
1268.371143	75.854424	67.451969
1267.861349	76.217767	67.456974
1266.426665	78.164813	67.461978
1266.396948	64.093357	67.466983
1265.696949	73.950440	67.471988
1265.278510	75.887284	67.476993
1264.583754	69.719774	67.481998
1263.273243	77.672742	67.487002
1263.002424	65.601396	67.492007
1262.408040	75.962092	67.497012
1261.984317	74.722147	67.502017
1261.313083	69.643751	67.507022
1260.469043	81.294699	67.512026
1260.330098	72.846796	67.517031
1258.858528	76.676325	67.522036
1258.349954	69.643409	67.527041
1258.104590	65.675305	67.532046
1256.893521	74.213293	67.537050
1256.062296	63.375955	67.542055
1255.025791	75.560563	67.547060
1254.825529	68.581127	67.552065
1254.552083	71.091016	67.557070
1254.026418	72.560776	67.562074
1253.451604	63.901485	67.567079
1252.009324	67.625431	67.572084
1251.396922	69.276145	67.577089
1251.298121	67.199196	67.582094
1250.687306	76.403422	67.587098
1250.397605	67.474861	67.592103
1249.275054	71.378206	67.597108
1248.501614	73.827252	67.602113
1247.686208	65.223568	67.607118
1246.461377	78.575135	67.612122
1246.207796	64.695402	67.617127
1245.312759	64.799882	67.622132
1245.285428	72.626079	67.627137
1245.227234	71.231815	67.632142
1244.043562	80.099776	67.637146
1243.408316	59.811941	67.642151
1242.922455	69.456774	67.647156
1242.007143	61.747362	67.652161
1241.032526	74.240683	67.657166
1240.406655	73.356170	67.662170
1240.024174	66.952927	67.667175
1239.541660	68.433175	67.672180
1238.521278	68.188575	67.677185
1237.784061	60.625891	67.682190
1237.278849	63.544804	67.687194
1236.912667	62.313061	67.692199
1235.702982	63.429542	67.697204
1234.859607	67.460389	67.702209
1234.369151	66.696272	67.707214
1233.821507	63.640429	67.712218
1233.787412	66.790360	67.717223
1232.763429	70.198634	67.722228
1231.991540	68.569352	67.727233
1231.320679	66.252209	67.732238
1230.818830	69.708342	67.737242
1230.256478	59.725566	67.742247
1229.066492	64.046504	67.747252
1228.289785	70.990482	67.752257
1227.882224	60.965743	67.757262
1227.446366	67.696241	67.762266
1226.930481	65.695083	67.767271
1225.804652	67.383294	67.772276
1225.270274	67.912985	67.777281
1225.059104	71.307124	67.782286
1223.699226	68.784157	67.787290
1223.051342	69.652026	67.792295
1222.596848	67.947041	67.797300
1222.018123	64.787331	67.802305
1221.766510	70.384642	67.807310
1221.011203	66.731031	67.812314
1220.257327	66.515021	67.817319
1219.930819	71.782037	67.822324
1218.560221	71.274588	67.827329
1217.555422	66.306025	67.832334
1216.902663	76.467848	67.837338
1216.423636	62.835293	67.842343
1215.956769	61.875037	67.847348
1215.737580	73.085990	67.852353
1215.603917	71.008279	67.857358
1214.460716	68.061344	67.862362
1214.020346	62.410075	67.867367
1213.110300	59.446565	67.872372
1212.276813	66.112563	67.877377
1211.530740	68.446877	67.882382
1210.791917	72.238750	67.887386
1209.777341	64.756454	67.892391
1208.940539	72.742919	67.897396
1208.493262	74.474618	67.902401
1208.367381	66.833642	67.907406
1207.594276	71.602391	67.912410
1207.475282	64.099096	67.917415
1206.282536	71.025663	67.922420
1205.291201	61.957958	67.927425
1205.268726	54.973916	67.932430
1204.153556	70.623062	67.937434
1203.085553	68.921031	67.942439
1202.456194	65.493406	67.947444
1201.958511	69.008806	67.952449
1202.115414	66.957428	67.957454
1201.154063	72.199249	67.962458
1200.361790	71.246591	67.967463
1199.561151	68.052791	67.972468
1198.943853	75.600644	67.977473
1198.689247	67.138031	67.982478
1197.215967	74.530274	67.987482
1196.951766	70.662945	67.992487
1196.191867	67.951533	67.997492
1195.522953	67.296233	68.002497
1195.531851	58.793295	68.007502
1194.302705	70.658463	68.012506
1193.854924	62.653939	68.017511
1193.087444	74.563961	68.022516
1192.157844	69.720645	68.027521
1191.620122	61.208445	68.032526
1190.649018	63.304157	68.037530
1190.408025	64.085245	68.042535
1190.108650	65.653071	68.047540
1189.183598	71.359064	68.052545
1188.441150	65.897771	68.057550
1187.630551	66.083461	68.062554
1187.213097	61.281704	68.067559
1186.041551	64.946856	68.072564
1185.072578	70.090543	68.077569
1185.020791	60.892345	68.082574
1184.356564	78.707526	68.087578
1184.441454	66.358847	68.092583
1183.685466	70.260691	68.097588
1182.503024	71.827036	68.102593
1182.133040	67.244813	68.107598
1180.802317	79.621321	68.112602
1180.102741	64.604567	68.117607
1179.483115	76.429575	68.122612
1178.800795	76.311008	68.127617
1178.668165	72.720807	68.132622
1178.094791	74.161899	68.137626
1177.247658	72.595064	68.142631
1176.404464	75.635555	68.147636
1175.615753	71.984117	68.152641
1175.401255	71.827417	68.157646
1174.505050	70.653173	68.162650
1173.841448	69.566516	68.167655
1173.121312	73.942065	68.172660
1172.385437	74.814480	68.177665
1172.455129	63.102171	68.182670
1171.134663	72.509161	68.187674
1170.714486	70.041775	68.192679
1170.184165	68.470288	68.197684
1169.031098	82.895436	68.202689
1168.563705	77.995962	68.207694
1167.644144	74.352721	68.212698
1167.599243	70.895227	68.217703
1166.876609	66.670301	68.222708
1165.425307	71.726703	68.227713
1164.973455	63.192967	68.232718
1164.399673	69.688360	68.237722
1164.333512	69.227365	68.242727
1163.869161	76.528543	68.247732
1162.412562	71.007375	68.252737
1162.218551	70.923113	68.257742
1161.590863	72.702437	68.262746
1160.166628	64.183009	68.267751
1159.502652	69.981529	68.272756
1158.906135	70.551079	68.277761
1158.536655	65.923049	68.282766
1158.129198	70.348218	68.287770
1157.798175	63.402213	68.292775
1156.863165	67.733091	68.297780
1156.044096	76.675558	68.302785
1155.719398	66.992477	68.307790
1154.395015	61.436096	68.312794
1153.922854	64.457001	68.317799
1153.158132	68.784450	68.322804
1152.937485	76.132023	68.327809
1152.716741	68.086665	68.332814
1151.131198	75.979344	68.337818
1150.557909	65.030062	68.342823
1149.955628	65.065933	68.347828
1149.528835	69.610875	68.352833
1148.589556	64.952050	68.357838
1147.601713	58.671927	68.362842
1147.194419	64.763941	68.367847
1146.655339	66.029269	68.372852
1146.418952	64.297493	68.377857
1146.099319	66.863623	68.382862
1144.893986	65.054148	68.387866
1144.487258	57.246541	68.392871
1143.206088	62.208081	68.397876
1142.207576	69.663607	68.402881
1141.931991	63.311195	68.407886
1141.218608	72.618482	68.412890
1140.982064	69.894808	68.417895
1140.442186	64.325617	68.422900
1139.505109	60.152157	68.427905
1138.871147	67.860364	68.432910
1137.893876	66.177047	68.437914
1137.884996	54.773718	68.442919
1137.289100	63.863613	68.447924
1136.071956	62.660006	68.452929
1135.761161	56.223311	68.457934
1134.790783	66.503470	68.462938
1134.010337	62.492760	68.467943
1133.433524	71.906060	68.472948
1132.494821	75.860637	68.477953
1131.980414	67.797336	68.482958
1131.334331	64.709867	68.487962
1131.598062	60.410063	68.492967
1130.326558	64.576849	68.497972
1129.417838	70.368572	68.502977
1128.994123	64.750944	68.507982
1128.323763	64.906462	68.512986
1127.505167	64.060519	68.517991
1126.622174	70.676067	68.522996
1126.050013	56.927474	68.528001
1125.817335	62.679471	68.533006
1125.467241	69.207099	68.538010
1124.870193	59.613084	68.543015
1123.930745	64.783633	68.548020
1123.214304	67.053331	68.553025
1122.494322	60.399445	68.558030
1121.264253	65.300826	68.563034
1121.023819	65.414767	68.568039
1120.723745	63.292570	68.573044
1119.552594	67.818721	68.578049
1119.151456	57.868687	68.583054
1118.092281	63.033050	68.588058
1117.861753	61.817596	68.593063
1116.905890	62.100534	68.598068
1116.252693	60.575414	68.603073
1115.832879	54.078794	68.608078
1114.939833	61.743057	68.613082
1114.584697	55.444309	68.618087
1113.732899	64.631685	68.623092
1112.857229	59.040223	68.628097
1112.480387	59.536992	68.633102
1111.920199	60.671642	68.638106
1111.488343	66.226661	68.643111
1110.231244	61.892804	68.648116
1109.670912	71.338179	68.653121
1109.315574	60.393669	68.658126
1108.407978	64.065753	68.663130
1107.463228	66.250345	68.668135
1106.903830	65.596571	68.673140
1106.193715	67.734378	68.678145
1106.031135	65.508309	68.683150
1105.420217	62.142436	68.688154
1104.566085	55.065189	68.693159
1103.821111	64.054221	68.698164
1103.299141	68.854010	68.703169
1102.844810	58.789437	68.708174
1101.570129	68.163939	68.713178
1100.859610	53.554257	68.718183
1100.762727	62.403923	68.723188
1100.218319	62.692379	68.728193
1099.395703	50.787711	68.733198
1098.425137	60.487576	68.738202
1097.989044	66.311359	68.743207
1097.573720	64.901371	68.748212
1096.068141	70.013752	68.753217
1095.736723	59.541690	68.758222
1095.055927	64.565444	68.763226
1094.690851	69.676174	68.768231
1094.223633	64.267328	68.773236
1093.179282	69.003558	68.778241
1092.586294	62.167051	68.783246
1091.940829	70.845364	68.788250
1091.575906	63.308666	68.793255
1090.286995	63.952106	68.798260
1089.453204	65.961355	68.803265
1089.022952	56.763452	68.808270
1088.395794	65.066682	68.813274
1088.442222	55.616327	68.818279
1087.801296	65.523962	68.823284
1086.397408	62.728949	68.828289
1085.670941	62.461310	68.833294
1085.364979	61.920192	68.838298
1084.983547	61.405272	68.843303
1083.912804	54.663696	68.848308
1082.756479	68.876482	68.853313
1082.808600	55.146868	68.858318
1082.396488	65.092220	68.863322
1081.746345	61.669515	68.868327
1081.021376	71.593678	68.873332
1080.170879	66.070763	68.878337
1079.786306	57.289804	68.883342
1078.335472	61.753227	68.888346
1077.601237	59.029888	68.893351
1077.414727	60.183948	68.898356
1076.766483	70.693582	68.903361
1076.514516	59.196462	68.908366
1075.548598	65.199153	68.913370
1074.966973	64.867473	68.918375
1074.451631	62.271741	68.923380
1073.453696	71.453993	68.928385
1072.877915	53.583765	68.933390
1072.120638	65.933732	68.938394
1071.703559	65.435525	68.943399
1070.806785	57.428347	68.948404
1069.995961	63.330669	68.953409
1069.580229	62.665088	68.958414
1068.830832	65.588183	68.963418
1068.509582	65.281315	68.968423
1067.406154	57.933077	68.973428
1066.568497	63.521119	68.978433
1066.636718	63.906089	68.983438
1065.648112	65.870587	68.988442
1064.738423	63.201973	68.993447
1064.219439	56.241738	68.998452
1063.557597	68.187011	69.003457
1063.128682	65.782539	69.008462
1061.785924	73.240818	69.013466
1061.057759	60.209360	69.018471
1060.511008	60.553391	69.023476
1060.301105	64.882484	69.028481
1060.121784	60.769859	69.033486
1059.026001	66.786907	69.038490
1058.076021	67.460023	69.043495
1057.576882	64.013300	69.048500
1057.051317	67.686125	69.053505
1056.740875	62.223962	69.058510
1055.415814	72.156866	69.063514
1055.141181	64.003404	69.068519
1054.461722	61.708182	69.073524
1053.311283	65.504075	69.078529
1052.639341	65.497435	69.083534
1051.962451	68.024215	69.088538
1051.943043	68.861527	69.093543
1051.637367	61.165600	69.098548
1050.138274	68.998844	69.103553
1049.784380	64.175964	69.108558
1049.175515	66.146287	69.113562
1048.346051	58.241952	69.118567
1047.361502	61.087344	69.123572
1046.603079	67.306195	69.128577
1046.503481	61.689062	69.133582
1045.867471	61.329771	69.138586
1045.510355	55.192205	69.143591
1044.344269	56.719738	69.148596
1043.497001	56.580141	69.153601
1043.102804	58.809630	69.158606
1042.457895	53.323414	69.163610
1041.230441	59.049172	69.168615
1040.772986	64.586194	69.173620
1040.079758	73.321002	69.178625
1040.065448	67.056351	69.183630
1039.445859	65.464403	69.188634
1038.795579	60.067351	69.193639
1037.956503	60.609286	69.198644
1036.861395	67.728546	69.203649
1036.717659	65.024813	69.208654
1035.736934	63.441436	69.213658
1034.822342	67.255009	69.218663
1034.489298	58.849068	69.223668
1033.852609	68.916890	69.228673
1033.601075	68.064338	69.233678
1032.430090	70.332261	69.238682
1031.637575	62.493017	69.243687
1031.438072	56.719891	69.248692
1030.495990	66.825263	69.253697
1029.781020	68.208487	69.258702
1029.065627	73.964752	69.263706
1028.486636	66.829562	69.268711
1028.334983	70.543829	69.273716
1027.030288	64.929194	69.278721
1026.430296	72.859103	69.283726
1025.898808	67.050483	69.288730
1025.817415	69.892539	69.293735
1024.814506	64.154195	69.298740
1023.551203	71.021096	69.303745
1023.125175	67.532785	69.308750
1022.606097	70.887612	69.313754
1022.083519	72.716477	69.318759
1021.394575	67.025953	69.323764
1020.309996	70.188474	69.328769
1020.080797	65.341029	69.333774
1019.448925	71.314245	69.338778
1018.557378	67.694995	69.343783
1018.122141	62.657979	69.348788
1017.322303	69.764961	69.353793
1016.949254	59.935066	69.358798
1015.638141	76.626289	69.363802
1014.711815	70.470477	69.368807
1014.314962	69.395040	69.373812
1013.688857	67.290039	69.378817
1013.990230	63.378484	69.383822
1013.486769	66.719787	69.388826
1012.114112	67.414439	69.393831
1011.682471	64.411158	69.398836
1010.666042	63.166215	69.403841
1010.078969	64.666293	69.408846
1009.254243	64.220341	69.413850
1008.627915	68.076367	69.418855
1008.467953	71.370902	69.423860
1006.973097	69.757375	69.428865
1006.538191	67.379099	69.433870
1005.942857	71.487243	69.438874
1005.583628	64.982581	69.443879
1005.108758	66.032714	69.448884
1003.787448	73.503376	69.453889
1003.735985	70.758154	69.458894
1002.881531	67.596641	69.463898
1002.086405	67.694771	69.468903
1001.097516	67.052588	69.473908
1000.389930	74.241093	69.478913
1000.174705	70.624626	69.483918
999.925630	68.622066	69.488922
999.019292	68.974440	69.493927
998.324812	62.531009	69.498932
997.642841	71.290841	69.503937
997.122944	69.818662	69.508942
995.942529	73.797549	69.513946
995.251499	67.117021	69.518951
995.014835	68.055135	69.523956
994.256982	66.387426	69.528961
993.597755	70.519931	69.533966
992.803386	73.896489	69.538970
991.809764	71.211294	69.543975
991.432474	66.049943	69.548980
990.910422	68.500060	69.553985
990.543638	66.672353	69.558990
989.232255	60.551018	69.563994
988.609457	69.749298	69.568999
988.597744	66.390615	69.574004
987.544362	63.027369	69.579009
987.046543	64.792374	69.584014
986.119860	65.054948	69.589018
985.840552	62.953122	69.594023
985.415296	51.019971	69.599028
984.249329	71.129072	69.604033
983.964633	68.504544	69.609038
983.067069	67.516670	69.614042
982.334233	60.948459	69.619047
981.561895	63.947768	69.624052
980.862136	63.772105	69.629057
980.625172	63.959625	69.634062
979.454861	67.739788	69.639066
978.643186	63.314624	69.644071
978.332852	64.163535	69.649076
977.987951	58.408822	69.654081
977.592629	55.792438	69.659086
976.109995	55.407031	69.664090
975.332717	68.427261	69.669095
974.980799	62.140644	69.674100
974.598282	66.210197	69.679105
974.006581	60.051624	69.684110
972.827490	66.044113	69.689114
972.025588	63.631200	69.694119
971.835060	61.152543	69.699124
970.984229	66.455698	69.704129
970.721794	64.288109	69.709134
969.485265	64.849156	69.714138
968.848623	75.290729	69.719143
968.789364	66.374445	69.724148
968.007483	75.875595	69.729153
967.288196	66.901911	69.734158
966.595983	62.850410	69.739162
965.707464	67.572927	69.744167
965.289099	63.916250	69.749172
964.304379	72.872501	69.754177
963.586964	62.332581	69.759182
962.653716	58.499214	69.764186
962.689600	65.589915	69.769191
962.353200	61.292558	69.774196
961.142035	70.094027	69.779201
960.635764	68.668574	69.784206
960.052366	71.126882	69.789210
959.274384	68.585586	69.794215
958.519740	56.143450	69.799220
957.425184	63.365151	69.804225
957.409379	61.245051	69.809230
956.911724	58.580300	69.814234
955.778141	63.499514	69.819239
955.199938	54.393003	69.824244
954.588083	67.724385	69.829249
953.688282	67.307745	69.834254
952.865325	62.203130	69.839258
952.027110	67.808641	69.844263
951.697771	61.542090	69.849268
950.891940	68.369338	69.854273
951.039235	61.831393	69.859278
950.582602	68.428027	69.864282
949.316069	71.271019	69.869287
949.125879	55.293361	69.874292
947.998771	66.636164	69.879297
947.094663	69.706916	69.884302
946.501764	71.750416	69.889306
945.693551	68.576834	69.894311
945.441692	57.904490	69.899316
945.068723	66.250872	69.904321
943.822506	60.111309	69.909326
943.263253	62.091106	69.914330
942.849086	63.970543	69.919335
942.317604	54.914948	69.924340
940.854928	68.304458	69.929345
940.442660	56.766648	69.934350
939.810285	65.285201	69.939354
939.287301	63.231621	69.944359
939.373999	56.630781	69.949364
938.188316	65.604823	69.954369
937.715734	56.708593	69.959374
937.027841	59.989369	69.964378
935.932131	63.628365	69.969383
935.355796	60.506199	69.974388
934.492837	63.420592	69.979393
934.372472	58.360297	69.984398
933.311277	60.008383	69.989402
932.415344	63.869481	69.994407
932.011917	65.040724	69.999412
931.410365	70.980745	70.004417
931.099865	58.587788	70.009422
930.238268	66.303869	70.014426
929.327865	59.847516	70.019431
928.892874	60.448184	70.024436
928.486111	61.724038	70.029441
927.552270	69.076297	70.034446
926.684098	70.031337	70.039450
925.909801	71.499727	70.044455
925.799685	65.196715	70.049460
924.950236	73.793976	70.054465
923.872470	65.903974	70.059470
923.112666	67.158742	70.064474
922.912821	65.865884	70.069479
922.620573	66.186789	70.074484
921.542065	64.412436	70.079489
920.865106	66.762637	70.084494
920.474541	65.252545	70.089498
919.464868	62.844331	70.094503
918.796862	60.954187	70.099508
917.621505	66.957142	70.104513
917.270612	63.685559	70.109518
917.206542	64.577288	70.114522
916.757582	64.680279	70.119527
915.979352	59.779877	70.124532
914.912506	69.580278	70.129537
914.551322	62.673818	70.134542
913.461371	59.095649	70.139546
912.122023	65.419600	70.144551
912.030906	60.133874	70.149556
911.485087	64.292502	70.154561
911.046649	64.614597	70.159566
910.682014	58.609144	70.164570
909.796158	67.901340	70.169575
908.990112	58.044189	70.174580
908.405029	67.725341	70.179585
908.348612	53.926291	70.184590
906.983742	63.624309	70.189594
905.943700	59.598223	70.194599
905.786937	56.361981	70.199604
905.101898	63.002853	70.204609
904.738773	57.834538	70.209614
903.655550	57.210561	70.214618
902.984930	55.672505	70.219623
902.803680	57.894929	70.224628
901.378179	61.501268	70.229633
900.949673	61.094796	70.234638
900.347456	67.624717	70.239642
900.134475	62.705322	70.244647
898.939791	54.797676	70.249652
897.777428	63.703365	70.254657
897.642491	65.880572	70.259662
897.215263	64.176043	70.264666
896.529403	67.781365	70.269671
896.375471	60.271058	70.274676
895.258754	67.059487	70.279681
894.580740	61.893979	70.284686
894.451348	55.674469	70.289690
893.014883	71.057862	70.294695
892.864565	59.319098	70.299700
891.856483	69.696790	70.304705
890.794870	68.744522	70.309710
890.237106	59.484963	70.314714
889.421592	67.248914	70.319719
889.242374	59.594397	70.324724
888.793190	67.618594	70.329729
887.955302	61.522884	70.334734
887.135894	59.696270	70.339738
886.168013	65.063810	70.344743
886.402148	59.000910	70.349748
885.280290	62.533699	70.354753
884.353677	59.990853	70.359758
883.626139	62.937326	70.364762
882.683488	59.895555	70.369767
882.741913	56.374325	70.374772
882.289485	65.001444	70.379777
881.383095	61.007714	70.384782
880.631759	62.190182	70.389786
879.937446	65.699080	70.394791
879.420659	61.422564	70.399796
878.141125	62.608676	70.404801
877.680308	56.672157	70.409806
877.505635	59.525904	70.414810
877.162034	63.970901	70.419815
876.002460	60.241403	70.424820
874.760348	58.747005	70.429825
874.259325	65.357019	70.434830
874.210724	58.970106	70.439834
873.606361	57.758985	70.444839
872.571772	60.740139	70.449844
872.024281	66.423978	70.454849
871.776483	65.316956	70.459854
870.721948	61.316847	70.464858
869.316801	64.358560	70.469863
869.418833	56.793325	70.474868
868.489574	63.384766	70.479873
868.335230	66.471826	70.484878
868.073410	58.082972	70.489882
867.126947	64.699230	70.494887
866.566512	62.112300	70.499892
865.026437	63.081264	70.504897
864.571396	56.524076	70.509902
863.569239	66.296849	70.514906
863.098822	63.813865	70.519911
863.088924	58.964656	70.524916
862.210189	74.051129	70.529921
861.111540	55.740657	70.534926
860.736702	59.190823	70.539930
859.910848	63.652657	70.544935
860.022512	58.851908	70.549940
858.715347	59.372212	70.554945
858.378458	58.679925	70.559950
857.547250	65.692586	70.564954
856.853874	64.233858	70.569959
856.366073	57.729196	70.574964
855.018698	65.880592	70.579969
854.832346	61.661874	70.584974
854.473585	56.906043	70.589978
853.364311	63.470947	70.594983
852.401053	57.846224	70.599988
851.938598	65.688030	70.604993
851.710193	56.961119	70.609998
851.208254	65.082026	70.615002
850.422673	65.055680	70.620007
849.685010	54.457532	70.625012
848.614300	64.676465	70.630017
848.298542	59.297191	70.635022
847.814806	59.705355	70.640026
846.718445	57.329896	70.645031
846.170747	60.380218	70.650036
845.773638	67.241781	70.655041
845.222291	58.460618	70.660046
844.384101	58.802199	70.665050
843.381329	60.423676	70.670055
843.138614	56.034157	70.675060
842.123433	63.445118	70.680065
841.116491	55.901864	70.685070
840.738993	59.741969	70.690074
840.091733	59.244171	70.695079
840.243755	56.534380	70.700084
839.129670	58.775982	70.705089
837.992805	68.877716	70.710094
837.751885	69.844907	70.715098
836.704918	62.834733	70.720103
836.602125	57.331674	70.725108
835.727961	63.263063	70.730113
834.827702	65.325549	70.735118
834.372747	60.649688	70.740122
833.796929	66.066803	70.745127
833.535984	58.934668	70.750132
832.302992	67.145139	70.755137
831.691920	62.732253	70.760142
831.291345	56.921776	70.765146
829.826056	69.207866	70.770151
829.295956	59.338363	70.775156
828.539377	68.270951	70.780161
828.149130	59.230755	70.785166
827.953744	65.033596	70.790170
827.798970	62.639150	70.795175
826.885639	49.856478	70.800180
825.732024	68.123315	70.805185
824.997792	49.426853	70.810190
824.721726	55.308767	70.815194
823.291470	58.028065	70.820199
823.014286	58.786560	70.825204
822.064861	61.050844	70.830209
822.053148	62.678573	70.835214
821.633366	63.068677	70.840218
820.354746	58.093421	70.845223
819.894804	54.845524	70.850228
819.261556	64.269419	70.855233
818.309466	55.108928	70.860238
817.721432	56.809475	70.865242
817.122808	62.779009	70.870247
816.739028	52.671754	70.875252
816.496263	62.691088	70.880257
815.031660	57.428469	70.885262
814.395056	56.470080	70.890266
813.658947	63.653696	70.895271
813.576921	59.577651	70.900276
812.448699	64.339949	70.905281
811.910620	70.383429	70.910286
811.070280	60.646898	70.915290
810.624791	70.271147	70.920295
809.910889	55.001378	70.925300
808.811302	55.487086	70.930305
808.119447	60.774439	70.935310
807.950278	56.660227	70.940314
807.614816	63.914108	70.945319
806.933934	54.443940	70.950324
805.807609	63.854865	70.955329
804.998378	57.885518	70.960334
804.655131	58.343866	70.965338
804.062245	68.105122	70.970343
803.770544	51.232171	70.975348
802.596659	61.436002	70.980353
801.806195	55.581942	70.985358
801.774589	52.010391	70.990362
800.720398	64.418706	70.995367
799.992225	64.028418	71.000372
799.435317	65.190996	71.005377
798.749934	63.842978	71.010382
797.783130	62.307946	71.015386
796.973812	66.462809	71.020391
796.596876	64.671444	71.025396
796.549462	65.212011	71.030401
795.685183	62.747588	71.035406
794.730882	59.042223	71.040410
794.194958	66.883115	71.045415
793.808820	55.486272	71.050420
792.705760	65.148969	71.055425
791.692516	62.741379	71.060430
791.514549	62.687708	71.065434
790.993465	69.143230	71.070439
790.228530	61.909983	71.075444
789.291441	60.084791	71.080449
788.393505	62.183193	71.085454
788.323753	54.413495	71.090458
787.348033	65.259154	71.095463
786.522579	55.515537	71.100468
785.986301	61.460958	71.105473
785.496723	67.949312	71.110478
785.301804	53.915286	71.115482
783.839054	73.625402	71.120487
783.396511	51.638677	71.125492
782.492240	60.295156	71.130497
781.958086	66.145623	71.135502
781.752373	62.273777	71.140506
781.223496	65.712206	71.145511
780.432804	56.671119	71.150516
779.694389	67.001179	71.155521
779.029449	63.964124	71.160526
778.468584	53.270049	71.165530
777.303659	60.140312	71.170535
777.141950	48.501165	71.175540
776.658920	58.134539	71.180545
775.024428	61.706407	71.185550
774.486467	60.349119	71.190554
773.725623	60.695757	71.195559
773.729176	61.516797	71.200564
773.352728	65.281048	71.205569
772.378739	62.504512	71.210574
771.436274	55.988678	71.215578
770.859317	64.143614	71.220583
770.679327	60.997816	71.225588
769.533181	64.930340	71.230593
768.954635	57.528655	71.235598
768.308447	65.212060	71.240602
767.657154	53.359115	71.245607
767.153128	55.800093	71.250612
766.123374	65.673482	71.255617
765.634415	67.610585	71.260622
765.684556	53.633744	71.265626
764.267687	66.746373	71.270631
763.514114	55.542080	71.275636
762.765392	65.507924	71.280641
762.092820	59.900040	71.285646
762.116891	61.246100	71.290650
761.245950	65.481748	71.295655
760.109453	60.491783	71.300660
759.397756	55.296991	71.305665
759.037146	53.720657	71.310670
758.928858	51.053886	71.315674
757.657415	63.358027	71.320679
757.280590	62.181672	71.325684
756.536859	57.198565	71.330689
755.704517	56.310780	71.335694
755.184651	59.263646	71.340698
754.237510	69.308394	71.345703
754.008707	61.434707	71.350708
753.268444	58.042217	71.355713
752.025270	54.865418	71.360718
751.482338	46.920326	71.365722
751.232464	61.681177	71.370727
750.668742	51.771325	71.375732
749.938525	54.877532	71.380737
749.268139	55.350125	71.385742
748.682722	46.713198	71.390746
747.913149	59.880466	71.395751
747.409242	54.192118	71.400756
746.382921	54.126863	71.405761
745.606580	65.172605	71.410766
745.791926	61.400930	71.415770
744.739476	57.558247	71.420775
744.120377	57.836593	71.425780
743.215123	54.733732	71.430785
742.369299	65.098245	71.435790
741.531345	51.770596	71.440794
740.794536	57.500365	71.445799
740.383318	57.682534	71.450804
739.913908	56.167682	71.455809
739.470878	63.028679	71.460814
738.778148	57.767794	71.465818
737.611938	62.130886	71.470823
737.716937	50.550207	71.475828
736.975735	58.628792	71.480833
735.669309	58.546637	71.485838
735.182041	58.704646	71.490842
734.563362	55.313305	71.495847
734.335340	55.603504	71.500852
733.043477	55.184713	71.505857
732.173632	63.614950	71.510862
732.031352	52.989864	71.515866
731.608262	56.944474	71.520871
730.919357	55.243794	71.525876
729.596349	54.345833	71.530881
728.987797	56.098552	71.535886
728.963365	47.261921	71.540890
728.178857	59.673046	71.545895
727.450836	57.772012	71.550900
726.412735	55.328984	71.555905
725.647185	61.966941	71.560910
725.268748	60.887044	71.565914
724.638128	66.358635	71.570919
724.298687	58.253409	71.575924
723.437847	55.600806	71.580929
722.500465	62.341819	71.585934
722.202214	52.564751	71.590938
721.522647	60.335479	71.595943
720.698393	58.668969	71.600948
719.811579	63.181550	71.605953
719.013215	55.144668	71.610958
719.043520	57.568385	71.615962
718.642343	66.182626	71.620967
717.537984	58.885181	71.625972
716.721487	57.275786	71.630977
716.178102	65.720279	71.635982
715.724468	62.116579	71.640986
714.583788	69.609069	71.645991
714.146483	56.763268	71.650996
713.862243	60.487611	71.656001
712.650999	60.283078	71.661006
712.045741	50.961758	71.666010
710.999568	53.489071	71.671015
710.481569	55.725699	71.676020
710.212840	56.408741	71.681025
710.005528	59.460083	71.686030
709.321143	51.695222	71.691034
708.441049	59.767544	71.696039
708.044004	55.971907	71.701044
706.680511	58.500863	71.706049
705.894192	54.016572	71.711054
705.627381	51.807137	71.716058
705.179806	48.989389	71.721063
704.578283	49.550378	71.726068
703.688584	53.013155	71.731073
702.959382	54.337231	71.736078
702.140010	46.680603	71.741082
700.983324	57.526710	71.746087
700.745148	58.414626	71.751092
699.924012	58.408182	71.756097
699.548169	49.786784	71.761102
698.988611	49.379138	71.766106
698.372053	51.694541	71.771111
697.966400	56.647757	71.776116
697.131253	50.632118	71.781121
696.448305	54.418372	71.786126
695.776658	50.379456	71.791130
694.462052	54.608496	71.796135
694.192716	53.779318	71.801140
693.580956	55.053156	71.806145
693.168702	54.540052	71.811150
692.419126	51.502310	71.816154
691.557610	56.991747	71.821159
690.899564	50.968410	71.826164
690.697955	57.194870	71.831169
689.746113	57.680758	71.836174
689.122767	51.136225	71.841178
688.368127	49.610032	71.846183
688.217519	45.478689	71.851188
687.169381	54.973395	71.856193
686.031130	58.523067	71.861198
685.760772	51.212687	71.866202
685.087586	60.117826	71.871207
684.588605	47.936308	71.876212
683.862140	57.655764	71.881217
682.919763	58.740975	71.886222
682.537857	56.278631	71.891226
681.982319	57.939339	71.896231
681.133526	51.064851	71.901236
680.314979	61.560652	71.906241
679.730059	54.475407	71.911246
679.570120	54.582879	71.916250
678.216921	57.428759	71.921255
677.418017	49.338366	71.926260
676.502487	50.698428	71.931265
675.784332	54.086588	71.936270
675.296826	40.058193	71.941274
674.920160	45.796855	71.946279
675.165802	44.068800	71.951284
674.700440	53.484898	71.956289
674.055063	53.168196	71.961294
672.828295	46.658260	71.966298
671.924846	55.778265	71.971303
671.398520	42.978205	71.976308
670.924600	49.273258	71.981313
669.309472	50.795193	71.986318
669.198289	52.623265	71.991322
668.400567	53.972454	71.996327
668.314271	44.730939	72.001332
667.007449	48.092993	72.006337
666.249092	55.478878	72.011342
665.947743	48.107205	72.016346
665.292251	47.692767	72.021351
664.787243	42.275861	72.026356
663.898453	45.369492	72.031361
663.056072	48.769552	72.036366
662.801106	49.800495	72.041370
662.811439	46.536092	72.046375
661.482209	40.569191	72.051380
660.647593	40.279474	72.056385
659.783284	49.680255	72.061390
659.589003	42.394039	72.066394
657.881597	38.990021	72.071399
657.198922	45.753563	72.076404
656.906043	50.354503	72.081409
656.646202	49.497009	72.086414
656.646158	51.425655	72.091418
656.026517	54.362886	72.096423
654.730277	49.300646	72.101428
654.167884	51.607433	72.106433
653.283302	58.958230	72.111438
652.583813	49.112613	72.116442
651.554122	57.699212	72.121447
650.783637	52.001304	72.126452
650.949355	54.862352	72.131457
650.144463	56.706282	72.136462
649.874643	56.121616	72.141466
648.397402	59.062961	72.146471
647.954795	59.530846	72.151476
647.432121	56.821263	72.156481
647.087148	56.770545	72.161486
646.438944	49.785278	72.166490
644.981991	56.107578	72.171495
644.772636	49.396204	72.176500
644.333348	47.329365	72.181505
643.701080	42.230779	72.186510
642.840360	48.212115	72.191514
642.138054	59.438473	72.196519
641.705221	46.984658	72.201524
640.553776	60.562848	72.206529
639.841998	53.333813	72.211534
639.670681	41.024439	72.216538
639.054004	51.354049	72.221543
638.288296	49.671937	72.226548
637.370112	49.871783	72.231553
636.589028	48.586364	72.236558
636.425344	48.252883	72.241562
635.916992	58.592056	72.246567
634.910758	50.405387	72.251572
634.028864	50.153172	72.256577
633.471826	46.950743	72.261582
633.418090	45.388637	72.266586
632.041861	56.564626	72.271591
631.327596	49.454266	72.276596
630.704431	52.948736	72.281601
630.250967	53.850443	72.286606
630.031846	45.249837	72.291610
629.029914	44.854313	72.296615
628.225456	48.710396	72.301620
627.723577	49.287074	72.306625
626.739911	47.869917	72.311630
625.805945	39.897256	72.316634
625.176668	55.167954	72.321639
624.950562	50.351619	72.326644
624.907161	50.473650	72.331649
624.135425	48.134906	72.336654
623.339475	42.240792	72.341658
622.048229	47.418636	72.346663
621.933695	45.093496	72.351668
620.999087	51.148110	72.356673
619.951571	51.182477	72.361678
619.403681	44.113436	72.366682
619.092818	56.889118	72.371687
618.604607	52.287994	72.376692
617.734627	47.146848	72.381697
616.822497	52.625442	72.386702
616.847751	40.373076	72.391706
616.153407	42.831773	72.396711
614.992292	45.995602	72.401716
614.344128	44.753677	72.406721
613.435577	59.703002	72.411726
613.488395	38.506387	72.416730
612.240320	47.763293	72.421735
611.955755	38.673217	72.426740
611.293192	49.981553	72.431745
610.560835	50.632789	72.436750
609.786493	48.032687	72.441754
608.756841	50.230974	72.446759
608.303615	53.979084	72.451764
608.017936	51.542429	72.456769
607.349520	53.790417	72.461774
606.603487	47.333263	72.466778
605.698988	48.171192	72.471783
604.858373	53.149538	72.476788
604.739952	54.877838	72.481793
603.698228	50.040022	72.486798
602.966948	49.122001	72.491802
602.380367	51.246568	72.496807
602.155483	53.304065	72.501812
601.591572	52.043993	72.506817
600.176895	55.087364	72.511822
599.719740	49.968783	72.516826
599.145583	56.199386	72.521831
598.837456	51.274691	72.526836
597.875272	47.340430	72.531841
597.063385	53.441738	72.536846
596.973306	51.863344	72.541850
596.103806	60.443371	72.546855
594.999739	60.390561	72.551860
594.501633	57.910469	72.556865
593.737478	56.728024	72.561870
593.506697	51.026179	72.566874
592.679573	55.488288	72.571879
591.663615	47.658010	72.576884
591.106462	51.082048	72.581889
590.177633	50.553469	72.586894
590.224339	54.084757	72.591898
589.513551	53.180822	72.596903
588.599576	61.118222	72.601908
588.209015	48.025324	72.606913
587.633182	58.723760	72.611918
586.523406	49.470228	72.616922
585.879688	51.600745	72.621927
585.239303	51.161844	72.626932
584.843811	49.887566	72.631937
584.339571	61.710021	72.636942
583.369359	53.378865	72.641946
582.441965	54.471188	72.646951
582.088384	64.613828	72.651956
581.331804	43.393167	72.656961
580.359611	51.715157	72.661966
579.885318	50.379313	72.666970
579.189167	45.951673	72.671975
578.835744	57.106698	72.676980
578.730694	45.419143	72.681985
577.662561	48.703797	72.686990
576.789114	47.972434	72.691994
576.238631	49.428929	72.696999
575.255737	44.305787	72.702004
574.588836	46.976169	72.707009
573.813591	51.002659	72.712014
573.502447	40.831867	72.717018
572.868544	48.611112	72.722023
572.421866	47.567343	72.727028
571.642096	48.565191	72.732033
570.601192	52.769617	72.737038
570.511785	46.485433	72.742042
569.720824	57.027323	72.747047
568.449115	46.362974	72.752052
568.350216	48.272671	72.757057
567.883133	49.074055	72.762062
566.801987	44.348194	72.767066
565.766720	55.542440	72.772071
565.224148	51.888287	72.777076
564.927121	45.118352	72.782081
564.487610	50.586335	72.787086
563.902810	47.165994	72.792090
562.854778	48.643397	72.797095
562.375032	51.328127	72.802100
561.746608	55.216115	72.807105
560.444363	57.506730	72.812110
560.000222	52.680978	72.817114
559.300823	61.994021	72.822119
559.029766	56.126704	72.827124
558.795840	48.471497	72.832129
557.345234	57.721268	72.837134
556.990758	47.653573	72.842138
556.362320	49.743816	72.847143
555.824949	53.120555	72.852148
554.857497	52.675413	72.857153
553.844371	52.120851	72.862158
553.685480	55.196026	72.867162
553.306464	50.758876	72.872167
552.425216	62.083141	72.877172
551.704157	52.281998	72.882177
550.787855	52.983053	72.887182
550.485197	51.078974	72.892186
550.363799	49.343143	72.897191
549.011365	51.096125	72.902196
548.500992	53.839353	72.907201
547.671053	54.930357	72.912206
546.647443	55.487656	72.917210
545.524744	57.655059	72.922215
545.112450	62.826974	72.927220
545.272802	53.199246	72.932225
544.478683	62.555765	72.937230
544.329186	55.746558	72.942234
543.483195	58.915416	72.947239
542.482045	53.341026	72.952244
542.146403	53.167409	72.957249
540.822039	53.357876	72.962254
540.111741	53.338559	72.967258
539.438799	43.140251	72.972263
539.423987	54.447918	72.977268
538.940080	50.565228	72.982273
537.668867	55.057093	72.987278
537.147108	47.886140	72.992282
536.584909	53.100855	72.997287
535.772778	55.786499	73.002292
535.088458	51.721267	73.007297
534.191884	53.642916	73.012302
533.816735	55.186608	73.017306
533.460839	57.884730	73.022311
532.762116	58.951683	73.027316
531.837579	54.994104	73.032321
531.038978	54.550459	73.037326
531.080533	46.668445	73.042330
529.587223	55.469287	73.047335
528.754430	46.824530	73.052340
528.664920	37.645052	73.057345
528.090134	49.606475	73.062350
527.320916	46.136674	73.067354
526.544729	48.281999	73.072359
526.026560	49.969902	73.077364
525.857716	49.608865	73.082369
524.630852	48.968515	73.087374
523.663477	47.503073	73.092378
523.024544	44.685885	73.097383
522.745408	43.126574	73.102388
522.288624	48.360768	73.107393
520.977736	58.745796	73.112398
520.337566	47.920944	73.117402
519.848340	46.630070	73.122407
519.139877	59.465938	73.127412
518.868718	45.212314	73.132417
517.698948	55.309929	73.137422
517.332567	50.443415	73.142426
516.968311	53.497689	73.147431
516.042227	48.953732	73.152436
515.234139	45.698288	73.157441
514.163335	55.633480	73.162446
513.976781	53.665178	73.167450
513.658255	54.271016	73.172455
512.808038	44.949368	73.177460
512.028071	44.283562	73.182465
511.112549	58.436070	73.187470
510.770218	46.858868	73.192474
510.607215	52.525661	73.197479
509.230219	58.057847	73.202484
508.774569	48.028360	73.207489
507.847217	58.483181	73.212494
507.491756	55.674452	73.217498
506.314478	44.501508	73.222503
505.577178	55.348678	73.227508
505.384844	47.924978	73.232513
504.722184	52.107017	73.237518
504.441917	49.224810	73.242522
503.722914	42.263490	73.247527
502.910528	53.054811	73.252532
502.566843	46.651870	73.257537
501.497835	52.160223	73.262542
500.557127	48.277776	73.267546
499.962294	53.049837	73.272551
499.283157	55.633878	73.277556
498.346717	42.832984	73.282561
498.271400	54.251211	73.287566
498.194667	49.254977	73.292570
497.093658	55.042824	73.297575
496.393905	45.577362	73.302580
495.227508	43.429272	73.307585
493.748008	58.497967	73.312590
493.476470	48.611041	73.317594
493.186390	48.256706	73.322599
492.617645	49.433849	73.327604
492.332447	52.822465	73.332609
492.004554	50.373628	73.337614
491.603066	48.075291	73.342618
490.390151	50.894185	73.347623
489.575624	52.675043	73.352628
488.945390	43.105469	73.357633
487.719095	54.478407	73.362638
487.098497	48.881262	73.367642
487.078609	56.130612	73.372647
486.861203	51.472183	73.377652
486.210383	50.842581	73.382657
485.006026	50.045698	73.387662
484.349273	51.613761	73.392666
483.912644	48.155642	73.397671
482.350200	46.799217	73.402676
481.956874	51.353093	73.407681
481.434098	48.523719	73.412686
481.288544	43.270368	73.417690
480.625717	46.645029	73.422695
479.494295	51.094148	73.427700
479.183025	47.013655	73.432705
478.212693	58.557133	73.437710
478.002446	46.785429	73.442714
476.983974	47.770873	73.447719
476.052042	54.973141	73.452724
475.585276	55.151588	73.457729
475.396629	55.198991	73.462734
474.445088	49.444840	73.467738
473.824975	57.431646	73.472743
472.970053	57.473238	73.477748
472.675685	46.363073	73.482753
471.358468	59.012082	73.487758
470.788303	48.250213	73.492762
470.401083	51.025873	73.497767
469.942963	57.928724	73.502772
469.926790	47.799266	73.507777
468.839935	58.464015	73.512782
468.262800	53.949637	73.517786
466.854162	54.872669	73.522791
466.113601	59.226404	73.527796
465.757115	56.280650	73.532801
465.312032	52.112668	73.537806
464.891864	54.114555	73.542810
463.617603	53.748295	73.547815
463.008803	61.369022	73.552820
462.663928	58.779391	73.557825
461.930505	61.630714	73.562830
460.990581	53.881425	73.567834
460.407812	54.860535	73.572839
459.747820	59.040584	73.577844
459.724149	50.995499	73.582849
458.620894	62.511277	73.587854
457.761465	49.731245	73.592858
457.398311	45.788335	73.597863
456.513080	51.086071	73.602868
456.025193	45.639682	73.607873
454.923550	41.150534	73.612878
454.525719	45.847057	73.617882
454.245956	50.398612	73.622887
452.885149	58.235354	73.627892
452.120138	46.559932	73.632897
451.628140	52.932011	73.637902
451.119915	59.155288	73.642906
450.780238	47.498830	73.647911
450.632153	49.842148	73.652916
449.382342	47.267396	73.657921
448.479823	55.335472	73.662926
448.133971	56.138063	73.667930
447.142903	50.573150	73.672935
446.050505	57.540795	73.677940
445.863002	46.639116	73.682945
445.555677	58.343470	73.687950
445.088255	49.161132	73.692954
443.934545	45.153376	73.697959
443.172766	59.579450	73.702964
442.745247	51.176085	73.707969
442.359473	58.684007	73.712974
441.601729	57.733981	73.717978
440.997249	50.916861	73.722983
440.066492	63.512193	73.727988
439.196371	50.413748	73.732993
438.169106	55.883935	73.737998
437.878920	46.592935	73.743002
437.363250	46.858030	73.748007
436.595396	48.899551	73.753012
436.677194	51.122661	73.758017
435.542233	51.590514	73.763022
435.153666	50.993255	73.768026
434.778831	45.051037	73.773031
433.360242	49.206883	73.778036
432.861959	51.599694	73.783041
432.106214	61.304940	73.788046
431.027757	51.661721	73.793050
430.014624	49.415123	73.798055
429.436544	57.712210	73.803060
429.361357	47.961171	73.808065
428.817707	44.289881	73.813070
428.472175	52.721800	73.818074
428.337469	53.381938	73.823079
426.534251	52.344614	73.828084
426.409749	50.532014	73.833089
425.925941	50.818843	73.838094
424.700154	56.090430	73.843098
423.657606	50.253031	73.848103
423.024064	52.344118	73.853108
422.857187	45.487239	73.858113
422.472598	50.047615	73.863118
421.754062	47.364567	73.868122
420.875162	48.983813	73.873127
420.077990	47.975422	73.878132
419.808448	51.986027	73.883137
418.706598	56.909859	73.888142
417.794662	49.873654	73.893146
417.646731	48.944737	73.898151
416.836295	48.894104	73.903156
416.922167	41.836102	73.908161
415.727271	46.798412	73.913166
414.619660	48.753729	73.918170
414.592639	51.982938	73.923175
413.912503	47.447142	73.928180
412.853335	48.986306	73.933185
412.140155	53.103875	73.938190
411.621559	44.964197	73.943194
411.471015	43.677726	73.948199
410.052945	48.650371	73.953204
409.699624	47.933958	73.958209
408.940419	54.418009	73.963214
408.408873	50.462516	73.968218
407.516359	51.199257	73.973223
406.676078	58.744914	73.978228
406.347014	48.491856	73.983233
405.519299	60.501488	73.988238
405.363633	54.002370	73.993242
404.454420	51.631990	73.998247
403.354616	61.062481	74.003252
403.017555	46.245372	74.008257
402.672253	48.244800	74.013262
401.693889	54.227606	74.018266
400.991920	44.538606	74.023271
400.220641	53.315918	74.028276
400.117697	44.841923	74.033281
399.172733	47.233379	74.038286
398.212997	39.249162	74.043290
397.576817	46.752829	74.048295
397.104111	52.629826	74.053300
397.000026	45.889102	74.058305
395.810778	49.360287	74.063310
394.778366	53.847280	74.068314
394.371871	49.679473	74.073319
394.148712	49.637764	74.078324
393.310557	47.904199	74.083329
392.342284	49.208111	74.088334
391.758086	49.704911	74.093338
391.408861	50.273078	74.098343
390.021410	59.243205	74.103348
389.715852	50.528680	74.108353
389.305695	51.313140	74.113358
388.778891	62.543112	74.118362
387.963320	51.987535	74.123367
386.863246	64.501052	74.128372
386.789303	61.559171	74.133377
385.968541	65.686010	74.138382
385.230882	55.177941	74.143386
384.349934	59.639226	74.148391
383.664913	65.207862	74.153396
383.357535	53.708697	74.158401
382.858981	56.170948	74.163406
381.968896	58.425932	74.168410
381.039932	55.309647	74.173415
380.364717	69.534286	74.178420
380.262344	54.657697	74.183425
379.387646	67.005991	74.188430
378.333309	57.921931	74.193434
378.038067	60.816989	74.198439
377.459025	71.520700	74.203444
377.169084	55.259460	74.208449
376.009456	60.471641	74.213454
375.170745	60.986928	74.218458
374.893082	59.509403	74.223463
373.811763	61.690786	74.228468
373.097345	55.012632	74.233473
372.490004	63.502053	74.238478
372.063800	58.391207	74.243482
371.892003	68.356650	74.248487
370.701717	56.424175	74.253492
370.123004	53.695205	74.258497
369.442248	62.798728	74.263502
368.697306	61.610139	74.268506
367.977979	53.756351	74.273511
367.135411	55.245245	74.278516
366.582470	53.668087	74.283521
366.276955	51.767643	74.288526
365.129236	58.237928	74.293530
364.456703	59.247135	74.298535
363.818583	68.692378	74.303540
363.499641	63.040884	74.308545
363.186722	63.098639	74.313550
362.071269	59.040668	74.318554
361.377595	64.292140	74.323559
360.652343	57.440673	74.328564
360.471709	49.294455	74.333569
358.899013	53.254126	74.338574
358.130768	47.904483	74.343578
358.100973	53.496430	74.348583
357.300725	49.672084	74.353588
357.173077	51.487018	74.358593
356.426539	55.907965	74.363598
355.679524	54.877409	74.368602
355.083657	51.660740	74.373607
354.124199	59.179672	74.378612
353.852870	58.677283	74.383617
352.792140	63.290235	74.388622
352.005132	59.228810	74.393626
351.947941	47.002227	74.398631
350.448248	61.014482	74.403636
349.855771	50.224670	74.408641
349.422103	50.350557	74.413646
348.951752	54.147164	74.418650
348.644818	45.188441	74.423655
347.355896	53.851143	74.428660
347.043106	51.297419	74.433665
346.501036	51.913674	74.438670
345.701187	56.239041	74.443674
344.958455	54.370435	74.448679
344.264878	55.897092	74.453684
343.818517	54.271414	74.458689
343.111355	56.613953	74.463694
342.159504	58.296894	74.468698
341.666575	49.374121	74.473703
340.540903	59.832208	74.478708
340.248869	50.573062	74.483713
339.591147	58.990089	74.488718
338.664712	52.481359	74.493722
338.309866	51.265301	74.498727
337.765921	49.830221	74.503732
337.338911	48.579933	74.508737
335.936711	54.157222	74.513742
335.310996	60.456012	74.518746
335.451837	52.223868	74.523751
335.003217	57.154008	74.528756
334.276148	58.832665	74.533761
333.319782	64.359402	74.538766
332.112917	63.848426	74.543770
331.289935	55.153300	74.548775
330.150981	63.002051	74.553780
329.889707	49.191604	74.558785
329.653200	53.468189	74.563790
329.272403	47.735103	74.568794
329.088148	51.320532	74.573799
327.947627	65.896881	74.578804
327.018675	57.761123	74.583809
326.556554	57.237107	74.588814
325.882613	54.488633	74.593818
325.132853	57.254286	74.598823
324.165197	55.886742	74.603828
323.835532	48.089140	74.608833
323.567059	60.033308	74.613838
322.457462	56.247240	74.618842
321.675983	50.872910	74.623847
321.103401	60.179974	74.628852
320.890954	49.651303	74.633857
319.342007	52.304637	74.638862
318.299293	61.538399	74.643866
318.424858	55.420250	74.648871
317.747074	54.230435	74.653876
317.820749	55.057640	74.658881
316.618056	55.850159	74.663886
315.652298	55.406419	74.668890
315.122560	46.175706	74.673895
314.385804	54.660526	74.678900
314.459425	56.802931	74.683905
313.361999	58.785054	74.688910
312.322507	58.882929	74.693914
311.955775	45.505618	74.698919
311.519449	56.639169	74.703924
310.364628	48.619850	74.708929
309.803014	55.591253	74.713934
309.439700	56.199524	74.718938
308.923904	51.831535	74.723943
307.625748	54.665677	74.728948
307.361970	45.334228	74.733953
306.484389	50.397399	74.738958
306.065810	45.788410	74.743962
305.417390	53.951643	74.748967
304.504871	52.662051	74.753972
303.746793	50.909447	74.758977
303.381236	56.176438	74.763982
302.629244	57.568914	74.768986
301.857247	48.504553	74.773991
301.137960	52.250959	74.778996
301.095327	55.071065	74.784001
300.285347	54.146757	74.789006
298.940574	62.870427	74.794010
298.766604	52.168467	74.799015
298.084278	54.303630	74.804020
297.732253	52.681848	74.809025
296.618517	59.812224	74.814030
295.483193	57.656124	74.819034
295.178062	48.006412	74.824039
294.665935	52.987680	74.829044
294.450802	54.007577	74.834049
293.246238	55.475348	74.839054
292.437319	55.484438	74.844058
292.388201	57.015619	74.849063
291.761438	61.497918	74.854068
290.925823	58.726338	74.859073
289.950701	61.010678	74.864078
289.550583	55.689112	74.869082
289.286916	52.421086	74.874087
287.861343	57.716695	74.879092
286.974587	55.869487	74.884097
286.818846	57.107001	74.889102
286.253982	56.794914	74.894106
285.354461	54.538153	74.899111
284.316378	65.797595	74.904116
284.103377	50.020869	74.909121
283.470030	54.654029	74.914126
282.962720	61.052228	74.919130
282.812349	51.690087	74.924135
281.363961	60.770905	74.929140
280.988758	53.564046	74.934145
280.532861	52.494994	74.939150
279.073364	54.971666	74.944154
278.889770	44.067821	74.949159
278.045228	50.002527	74.954164
277.829046	44.003514	74.959169
276.923926	49.078968	74.964174
275.972529	56.334861	74.969178
275.486249	48.205840	74.974183
274.798357	44.127071	74.979188
274.610016	46.602969	74.984193
273.632440	52.782812	74.989198
272.787242	47.406043	74.994202
272.283268	46.338348	74.999207
271.543523	50.436532	75.004212
271.248926	44.673949	75.009217
270.343004	51.031606	75.014222
269.419049	47.660679	75.019226
269.289238	52.877477	75.024231
268.356475	48.039798	75.029236
267.574236	44.908058	75.034241
266.818183	47.813501	75.039246
266.053076	52.090773	75.044250
265.896455	43.581198	75.049255
264.819344	53.670441	75.054260
264.054849	44.685327	75.059265
263.756916	39.060475	75.064270
263.271144	51.228511	75.069274
262.816727	45.537137	75.074279
261.568579	54.177606	75.079284
261.015939	49.090098	75.084289
260.579239	51.152999	75.089294
259.450771	52.655964	75.094298
258.996630	51.506211	75.099303
258.067662	58.320138	75.104308
257.913007	54.257294	75.109313
257.391033	52.137480	75.114318
256.065443	58.377540	75.119322
255.736798	48.670083	75.124327
255.170281	52.294376	75.129332
254.909584	52.039465	75.134337
253.907613	58.341478	75.139342
253.192477	53.713541	75.144346
252.799099	54.402307	75.149351
251.433029	59.051355	75.154356
250.972298	44.460591	75.159361
250.459064	45.195273	75.164366
249.651313	49.998168	75.169370
249.477247	43.246540	75.174375
248.431903	48.631364	75.179380
247.866212	55.989783	75.184385
247.317556	52.361914	75.189390
246.841804	46.965685	75.194394
245.611609	47.153913	75.199399
244.739967	51.232129	75.204404
244.271889	42.868405	75.209409
243.953133	45.395056	75.214414
243.214986	54.715905	75.219418
242.972645	47.680268	75.224423
241.737715	51.389041	75.229428
240.993586	52.501158	75.234433
240.671424	50.319533	75.239438
240.026710	51.485188	75.244442
239.219564	48.054650	75.249447
238.299971	56.923453	75.254452
238.204783	52.950479	75.259457
237.704645	49.970897	75.264462
236.188607	63.479606	75.269466
235.854886	46.719190	75.274471
235.243745	53.860926	75.279476
234.875374	52.554000	75.284481
233.785426	50.356004	75.289486
232.679329	59.055844	75.294490
232.603801	49.998751	75.299495
231.744660	55.024313	75.304500
231.830247	53.786943	75.309505
231.154890	48.342112	75.314510
230.278649	55.825737	75.319514
229.663878	41.336812	75.324519
228.054583	50.558420	75.329524
227.392012	50.468507	75.334529
226.995127	43.001770	75.339534
226.476057	55.186158	75.344538
226.561501	36.871853	75.349543
225.737546	49.152151	75.354548
224.601722	48.656711	75.359553
224.077294	45.510693	75.364558
223.483336	52.629191	75.369562
222.928107	47.997850	75.374567
221.367581	55.071748	75.379572
220.866283	49.004655	75.384577
220.693228	48.190145	75.389582
220.117553	46.153020	75.394586
220.321188	38.923288	75.399591
218.690318	45.191529	75.404596
218.285457	43.674380	75.409601
217.798639	46.557413	75.414606
216.803726	46.283942	75.419610
216.194340	43.487365	75.424615
215.509772	49.648898	75.429620
215.118606	48.386610	75.434625
214.454014	44.047101	75.439630
213.261098	56.110262	75.444634
212.915342	42.854219	75.449639
212.058682	45.543903	75.454644
211.118910	46.986843	75.459649
210.413331	39.335937	75.464654
209.864302	40.208798	75.469658
209.668246	43.397139	75.474663
209.171882	49.676902	75.479668
208.553076	38.979658	75.484673
207.815527	40.276816	75.489678
206.982563	51.561915	75.494682
206.486128	48.086583	75.499687
205.108661	53.425027	75.504692
204.296972	53.491359	75.509697
204.061985	50.236119	75.514702
203.357031	44.163656	75.519706
203.247428	39.846055	75.524711
202.398666	45.477099	75.529716
201.346493	48.175880	75.534721
201.026409	45.457763	75.539726
200.449864	51.040677	75.544730
200.305573	43.722910	75.549735
198.908138	48.544140	75.554740
198.254437	48.812368	75.559745
197.783425	46.375360	75.564750
196.651100	45.873068	75.569754
196.158399	39.266870	75.574759
195.532935	49.861293	75.579764
194.874832	49.415858	75.584769
194.606670	43.363644	75.589774
193.371227	47.283834	75.594778
192.732990	41.446745	75.599783
192.370569	52.289392	75.604788
191.880987	50.858295	75.609793
191.412405	47.242907	75.614798
190.240405	53.848018	75.619802
189.924317	48.819010	75.624807
189.009286	54.984179	75.629812
188.338178	49.601764	75.634817
187.521227	55.322361	75.639822
186.874599	57.303627	75.644826
186.839904	46.913803	75.649831
186.251064	52.698956	75.654836
184.956437	50.114144	75.659841
184.639302	41.753179	75.664846
183.818733	46.816757	75.669850
182.894941	49.036180	75.674855
182.081550	51.882981	75.679860
181.630317	47.957320	75.684865
181.326930	47.171479	75.689870
180.571151	46.686429	75.694874
179.730310	42.999510	75.699879
178.679449	45.212386	75.704884
178.014049	42.369558	75.709889
178.011827	42.037173	75.714894
177.690455	47.527364	75.719898
176.856670	45.521943	75.724903
175.726516	50.638040	75.729908
175.358412	49.171808	75.734913
174.723474	38.466110	75.739918
173.204867	49.526220	75.744922
172.932116	41.852046	75.749927
172.219716	47.308391	75.754932
172.094728	49.058250	75.759937
171.758595	47.309375	75.764942
170.568250	39.997554	75.769946
169.840745	35.030999	75.774951
169.334481	50.359388	75.779956
168.071767	40.403498	75.784961
167.473158	50.001732	75.789966
167.002013	52.868084	75.794970
166.975949	50.394828	75.799975
166.469774	44.620268	75.804980
165.329461	44.275384	75.809985
164.680679	45.976297	75.814990
164.077117	48.291324	75.819994
163.718512	42.357617	75.824999
162.832113	42.439029	75.830004
161.959362	39.130947	75.835009
161.767628	33.405604	75.840014
160.560911	46.097030	75.845018
159.598132	39.740839	75.850023
159.119470	49.100751	75.855028
159.018047	57.129482	75.860033
158.452220	46.742350	75.865038
156.891826	53.507177	75.870042
156.520138	52.612380	75.875047
155.821676	58.064934	75.880052
155.505816	54.048305	75.885057
155.002948	42.094674	75.890062
153.663369	46.362650	75.895066
153.551090	41.223882	75.900071
152.934440	42.462354	75.905076
151.919205	44.082930	75.910081
150.914014	40.371767	75.915086
150.428649	38.951046	75.920090
150.174173	51.793418	75.925095
149.876215	45.358029	75.930100
149.197881	40.112402	75.935105
148.220101	45.500680	75.940110
147.524402	56.703983	75.945114
146.980444	52.750537	75.950119
146.028821	48.152463	75.955124
145.128969	44.110689	75.960129
144.849611	41.597400	75.965134
144.242109	48.782724	75.970138
143.513593	44.328850	75.975143
142.767126	53.505963	75.980148
141.835681	44.296785	75.985153
141.857230	47.440969	75.990158
140.480089	48.346546	75.995162
139.962110	53.204192	76.000167
139.281005	43.593971	76.005172
138.911304	39.762555	76.010177
138.724385	32.962535	76.015182
137.633176	38.789952	76.020186
137.062193	37.586315	76.025191
136.338076	43.804631	76.030196
135.456862	44.941792	76.035201
134.532226	30.429789	76.040206
134.064622	51.550506	76.045210
133.627685	45.954149	76.050215
133.143495	50.251315	76.055220
132.044527	45.690937	76.060225
131.084455	46.649862	76.065230
130.501772	55.811900	76.070234
130.285583	42.782805	76.075239
129.910851	41.677185	76.080244
129.037137	43.853948	76.085249
128.446184	44.582124	76.090254
127.489021	46.108293	76.095258
127.297044	46.996775	76.100263
126.614626	53.047598	76.105268
125.663055	46.121926	76.110273
125.125577	41.121928	76.115278
124.433572	53.076855	76.120282
123.474018	45.930105	76.125287
122.570291	50.456602	76.130292
122.100908	50.887847	76.135297
122.081778	46.560555	76.140302
121.206098	54.261740	76.145306
120.402435	44.164865	76.150311
119.750171	47.768162	76.155316
119.141818	47.775288	76.160321
118.580241	49.714621	76.165326
117.238806	51.171185	76.170330
117.110567	48.051901	76.175335
116.411993	47.811639	76.180340
116.079949	51.184099	76.185345
115.008210	46.296110	76.190350
114.097171	43.478279	76.195354
113.517325	52.154161	76.200359
113.367892	49.071372	76.205364
112.634717	42.061995	76.210369
111.799569	40.264975	76.215374
110.999395	55.813707	76.220378
110.693148	37.393149	76.225383
109.743825	42.038883	76.230388
108.463106	50.342406	76.235393
107.941635	47.104482	76.240398
107.653468	48.186502	76.245402
107.175101	46.269507	76.250407
106.953031	47.147020	76.255412
106.055250	55.168704	76.260417
105.585565	37.638388	76.265422
104.425577	58.014816	76.270426
103.942818	47.966118	76.275431
102.908998	53.629859	76.280436
102.226337	49.130838	76.285441
102.050199	53.218033	76.290446
101.378390	42.153962	76.295450
100.514082	45.165024	76.300455
99.841407	51.463458	76.305460
99.364030	48.089193	76.310465
98.731941	39.783207	76.315470
97.354783	50.019701	76.320474
96.813671	48.229409	76.325479
96.502711	49.338720	76.330484
95.879174	57.706183	76.335489
95.760257	42.961615	76.340494
94.722231	47.690888	76.345498
94.037735	41.101112	76.350503
93.576651	47.614962	76.355508
92.729929	45.028158	76.360513
91.677774	42.825780	76.365518
90.795482	47.273173	76.370522
90.460313	43.138213	76.375527
90.401241	45.055759	76.380532
89.382697	51.171233	76.385537
88.715237	50.885016	76.390542
87.776845	55.240434	76.395546
87.360592	43.206780	76.400551
86.992054	51.401107	76.405556
85.883539	47.074088	76.410561
85.483884	43.208035	76.415566
84.586314	46.192868	76.420570
84.282852	44.618571	76.425575
83.035525	44.636147	76.430580
82.425411	52.496840	76.435585
82.111804	52.732937	76.440590
81.340023	47.730893	76.445594
80.774474	52.225547	76.450599
79.919699	42.226729	76.455604
79.033814	44.832807	76.460609
78.950239	45.642502	76.465614
78.005700	44.611997	76.470618
77.515956	48.992059	76.475623
76.687168	48.991774	76.480628
75.903307	50.004619	76.485633
75.613171	45.539201	76.490638
75.030313	45.458693	76.495642
74.153469	40.582221	76.500647
73.400256	42.055382	76.505652
72.500421	48.593477	76.510657
72.532481	43.195152	76.515662
71.489497	54.474354	76.520666
70.950793	44.261125	76.525671
70.521552	48.286184	76.530676
69.751071	52.517055	76.535681
68.897323	43.535219	76.540686
68.088544	52.769594	76.545690
67.796477	45.089058	76.550695
67.031175	53.830795	76.555700
65.866909	51.584806	76.560705
65.446877	52.782480	76.565710
64.827493	43.973003	76.570714
64.492578	48.186447	76.575719
63.396517	43.772297	76.580724
62.530925	51.564929	76.585729
62.462837	57.293858	76.590734
62.078086	49.453060	76.595738
60.779837	48.001155	76.600743
59.658012	53.068663	76.605748
59.289472	46.579892	76.610753
59.151740	46.828943	76.615758
58.355165	45.060482	76.620762
57.665162	52.030321	76.625767
57.038368	47.102933	76.630772
56.372471	54.559364	76.635777
55.912852	41.780425	76.640782
54.491803	51.345846	76.645786
54.158995	45.005921	76.650791
53.536820	49.139025	76.655796
52.849925	56.370147	76.660801
52.834634	48.710123	76.665806
51.493401	54.553802	76.670810
50.842698	42.731018	76.675815
50.267996	48.955488	76.680820
49.835373	49.571696	76.685825
49.226301	47.446901	76.690830
48.288325	50.354613	76.695834
47.919660	46.568780	76.700839
47.250088	39.929332	76.705844
45.798269	55.556778	76.710849
45.670638	41.755059	76.715854
44.847467	55.741546	76.720858
44.604730	48.622428	76.725863
43.976043	46.656883	76.730868
42.858057	48.585629	76.735873
42.311451	48.054643	76.740878
41.703715	53.823912	76.745882
41.494320	44.291456	76.750887
40.416408	42.261945	76.755892
39.681739	44.288826	76.760897
39.521486	45.393029	76.765902
38.425877	45.537817	76.770906
37.466523	45.189362	76.775911
37.019275	40.897246	76.780916
36.297837	43.868194	76.785921
35.742138	44.822582	76.790926
35.360477	49.683731	76.795930
34.426824	47.421476	76.800935
33.473549	44.071094	76.805940
33.061155	42.481063	76.810945
32.814128	41.895988	76.815950
31.961302	52.838938	76.820954
31.018646	42.057794	76.825959
30.523942	48.045578	76.830964
30.193599	49.159565	76.835969
29.575499	46.052192	76.840974
28.407427	43.899871	76.845978
27.988096	38.046843	76.850983
27.386059	43.909820	76.855988
26.342306	54.416446	76.860993
26.098589	42.669106	76.865998
25.215819	47.258522	76.871002
24.542404	47.846910	76.876007
23.793278	47.248884	76.881012
23.001016	46.662469	76.886017
22.892039	44.088904	76.891022
22.305527	51.125821	76.896026
21.546707	50.436300	76.901031
20.811932	47.847436	76.906036
19.732437	57.099775	76.911041
19.448593	49.451050	76.916046
18.553836	45.142009	76.921050
17.606775	44.878334	76.926055
17.587498	45.731391	76.931060
16.856307	47.609490	76.936065
16.087851	45.538513	76.941070
14.901726	47.492333	76.946074
14.641326	41.326949	76.951079
14.259854	39.826607	76.956084
12.996826	47.357791	76.961089
12.007500	44.612414	76.966094
11.185923	54.027041	76.971098
11.200200	44.728573	76.976103
10.571181	44.735869	76.981108
9.868146	44.696624	76.986113
9.548058	35.281186	76.991118
8.960685	53.573015	76.996122
8.366029	47.148710	77.001127
7.479368	45.479792	77.006132
6.568309	51.198102	77.011137
6.513483	43.038187	77.016142
5.038435	50.141146	77.021147
4.247433	52.746308	77.026151
4.259224	44.747654	77.031156
3.665029	61.081995	77.036161