Fri Mar 05 19:04:29 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.025620	96.391571	0.000000
0.178396	91.866544	0.005005
-0.467279	62.984911	0.010010
-2.572596	11.698907	0.015014
-6.544329	-5.267947	0.020019
-12.322985	-0.141954	0.025024
-17.385372	3.682343	0.030029
-21.874725	-0.015389	0.035034
-25.827487	-0.479216	0.040038
-29.444133	-7.121559	0.045043
-33.109538	2.330422	0.050048
-36.764500	-7.585868	0.055053
-40.088739	-5.713543	0.060058
-43.997425	-0.658716	0.065062
-47.315114	-4.740438	0.070067
-51.557621	-8.731382	0.075072
-55.511100	-6.779149	0.080077
-59.426407	-0.868532	0.085082
-63.185031	-0.506984	0.090086
-66.756566	-3.725008	0.095091
-70.422472	3.104627	0.100096
-74.227822	0.799128	0.105101
-77.662473	8.725712	0.110106
-81.895754	4.537804	0.115110
-85.398877	-9.166827	0.120115
-89.218013	-2.257526	0.125120
-92.968243	-3.488420	0.130125
-96.538462	-7.491932	0.135130
-100.621113	-1.226543	0.140134
-104.305305	-17.024828	0.145139
-108.453999	-3.958523	0.150144
-111.918734	-11.941731	0.155149
-115.652784	-13.313941	0.160154
-119.845086	1.072947	0.165158
-123.282870	3.206354	0.170163
-127.030957	8.803391	0.175168
-130.729880	-2.040871	0.180173
-134.895925	-0.854107	0.185178
-138.586243	-5.931221	0.190182
-141.838890	-8.930357	0.195187
-145.738641	-4.280499	0.200192
-149.395621	-3.994962	0.205197
-153.083163	-0.351936	0.210202
-156.950320	-5.181605	0.215206
-160.484687	-6.724384	0.220211
-164.759554	4.368881	0.225216
-168.275895	-4.468604	0.230221
-171.861327	-6.988814	0.235226
-176.116295	1.597090	0.240230
-179.982009	-10.560877	0.245235
-183.479850	2.430066	0.250240
-186.818565	-5.159981	0.255245
-190.545613	-6.569463	0.260250
-194.582894	4.258853	0.265254
-198.290445	-4.202716	0.270259
-202.222870	3.218425	0.275264
-205.921376	-3.852124	0.280269
-209.719398	4.610445	0.285274
-213.646131	5.150445	0.290278
-217.125676	-2.085921	0.295283
-220.914135	-0.243338	0.300288
-224.584899	-1.784753	0.305293
-228.554317	-1.135415	0.310298
-232.422735	5.430311	0.315302
-236.241073	-10.791046	0.320307
-239.881585	11.391156	0.325312
-243.754672	-2.772993	0.330317
-247.085258	1.771985	0.335322
-250.910287	1.253445	0.340326
-254.586206	-4.756187	0.345331
-258.653235	2.410561	0.350336
-262.248115	0.680471	0.355341
-265.957648	-1.906519	0.360346
-270.041451	2.903802	0.365350
-273.646476	-10.054129	0.370355
-277.644522	-5.632801	0.375360
-281.268784	-8.815274	0.380365
-284.761179	-0.038685	0.385370
-288.655490	5.186120	0.390374
-292.222513	-3.072225	0.395379
-296.157463	1.320139	0.400384
-300.200796	1.580849	0.405389
-303.542379	6.485628	0.410394
-307.530553	9.617061	0.415398
-311.232694	-5.936743	0.420403
-315.519129	0.514493	0.425408
-319.362719	-5.783657	0.430413
-322.752012	-5.340319	0.435418
-326.479127	-4.543423	0.440422
-329.905798	-6.222992	0.445427
-334.034613	-4.010504	0.450432
-337.555870	-4.735099	0.455437
-341.040948	-9.713770	0.460442
-345.155031	1.447161	0.465446
-348.627227	-5.529979	0.470451
-352.669876	2.274847	0.475456
-356.339334	-1.854351	0.480461
-360.030689	-5.850736	0.485466
-364.066759	2.352026	0.490470
-367.932235	3.081192	0.495475
-371.906549	1.681512	0.500480
-375.096370	-0.540436	0.505485
-378.506634	-0.577795	0.510490
-382.609905	8.263356	0.515494
-386.339270	-0.949783	0.520499
-390.176710	2.544068	0.525504
-394.082236	-0.035080	0.530509
-398.329275	2.426632	0.535514
-402.093193	3.220060	0.540518
-405.301312	-0.899150	0.545523
-408.960753	7.828593	0.550528
-412.326227	2.709500	0.555533
-416.630067	-4.970516	0.560538
-420.703101	-4.503010	0.565542
-423.945223	-3.114784	0.570547
-428.076679	5.103313	0.575552
-432.340249	3.551231	0.580557
-435.286559	0.792161	0.585562
-439.323238	-2.567057	0.590566
-442.670284	-7.394155	0.595571
-446.799089	-2.301966	0.600576
-450.330060	6.430550	0.605581
-454.390849	4.669504	0.610586
-458.107384	6.135119	0.615590
-461.429628	-3.601806	0.620595
-465.541903	0.681954	0.625600
-469.438506	5.175703	0.630605
-473.205565	-0.929410	0.635610
-477.252113	7.516482	0.640614
-480.264534	-4.105467	0.645619
-484.254789	6.594367	0.650624
-488.118740	6.678511	0.655629
-491.809304	-1.507748	0.660634
-496.157274	12.494605	0.665638
-499.482624	0.329727	0.670643
-503.501373	8.414831	0.675648
-506.866504	6.449721	0.680653
-510.378261	-1.659411	0.685658
-514.235686	5.668236	0.690662
-517.710687	-0.112871	0.695667
-521.930338	8.658787	0.700672
-526.193902	4.348788	0.705677
-529.694555	-5.063068	0.710682
-533.350293	9.437471	0.715686
-536.609757	5.708265	0.720691
-540.720107	9.416259	0.725696
-544.303339	1.701794	0.730701
-547.888625	-6.434955	0.735706
-552.400102	10.110417	0.740710
-555.841402	5.142419	0.745715
-559.873372	6.411000	0.750720
-563.629208	5.661136	0.755725
-566.738436	0.100790	0.760730
-570.884118	3.535359	0.765734
-574.949808	-4.778490	0.770739
-578.733682	4.466113	0.775744
-582.380008	4.323255	0.780749
-585.780378	6.046063	0.785754
-589.550868	7.760197	0.790758
-592.933979	3.254466	0.795763
-597.092806	5.771819	0.800768
-601.087641	4.251224	0.805773
-604.996379	3.784474	0.810778
-608.875947	8.387687	0.815782
-612.153222	0.138749	0.820787
-616.067060	0.538576	0.825792
-619.704849	-4.823704	0.830797
-623.205925	6.159309	0.835802
-627.495479	3.290249	0.840806
-631.438173	6.391292	0.845811
-634.897493	9.798306	0.850816
-638.353686	2.472122	0.855821
-642.045151	-0.369472	0.860826
-646.290061	4.899300	0.865830
-649.551667	-8.486620	0.870835
-653.518077	3.340336	0.875840
-657.504949	-7.624188	0.880845
-661.333194	2.548564	0.885850
-664.914996	0.143644	0.890854
-668.132091	-6.375453	0.895859
-672.764080	10.146805	0.900864
-676.411772	0.112125	0.905869
-679.811612	1.067008	0.910874
-683.709196	0.770493	0.915878
-687.322057	-7.607628	0.920883
-691.253351	5.492678	0.925888
-695.025589	3.441510	0.930893
-698.727641	-2.998468	0.935898
-702.550167	12.607592	0.940902
-706.449113	-1.761334	0.945907
-710.272432	-0.552652	0.950912
-714.120444	7.584351	0.955917
-717.468344	-3.674571	0.960922
-721.444171	5.935236	0.965926
-724.706847	10.520468	0.970931
-728.858154	10.469580	0.975936
-732.363047	2.250888	0.980941
-736.412718	4.284261	0.985946
-740.276968	6.321122	0.990950
-744.013722	-0.750323	0.995955
-747.676095	8.364730	1.000960
-751.968868	6.789509	1.005965
-755.100408	0.174859	1.010970
-759.282717	10.571510	1.015974
-762.987756	-0.819495	1.020979
-766.682086	6.045662	1.025984
-770.249802	0.183567	1.030989
-773.722485	-1.210459	1.035994
-777.615736	3.554480	1.040998
-781.396172	3.020206	1.046003
-785.454104	3.957429	1.051008
-789.002721	4.258163	1.056013
-792.827100	2.180796	1.061018
-796.607218	5.514740	1.066022
-800.324094	1.425367	1.071027
-804.022389	4.881860	1.076032
-807.668432	5.300697	1.081037
-811.428071	0.317743	1.086042
-815.641633	4.455860	1.091046
-819.096805	4.106193	1.096051
-823.138705	10.722648	1.101056
-826.941714	8.425878	1.106061
-830.430764	-3.843202	1.111066
-834.214270	6.287967	1.116070
-837.590836	0.297650	1.121075
-841.666495	-2.311895	1.126080
-845.547194	0.005307	1.131085
-848.985397	8.229966	1.136090
-853.134795	7.649139	1.141094
-856.668858	-2.714064	1.146099
-860.569441	2.241413	1.151104
-864.410207	-6.092100	1.156109
-867.692718	0.931291	1.161114
-872.131060	1.820673	1.166118
-875.367780	-6.352354	1.171123
-878.881043	-4.442349	1.176128
-883.095652	3.390829	1.181133
-886.518147	-2.098487	1.186138
-890.746317	2.166675	1.191142
-894.577723	-6.740711	1.196147
-898.003467	0.502738	1.201152
-902.038663	-0.522036	1.206157
-905.536776	2.800104	1.211162
-909.531277	4.142134	1.216166
-913.101778	-3.761428	1.221171
-916.965004	2.271525	1.226176
-920.809915	-0.904630	1.231181
-924.653640	-4.481510	1.236186
-928.366263	-2.079086	1.241190
-931.747617	-6.868440	1.246195
-935.499341	2.448826	1.251200
-939.472782	1.445781	1.256205
-942.994337	-7.137335	1.261210
-947.005481	1.598541	1.266214
-950.873275	-5.938875	1.271219
-954.460151	-5.649120	1.276224
-958.357756	-0.723925	1.281229
-962.054052	-11.794283	1.286234
-966.147772	-4.324072	1.291238
-969.749389	-10.426427	1.296243
-973.645954	0.968811	1.301248
-977.437340	0.029755	1.306253
-980.761441	-10.008853	1.311258
-984.614410	1.915590	1.316262
-988.356396	0.038257	1.321267
-992.108910	3.264015	1.326272
-996.032998	1.102007	1.331277
-999.682374	-3.552918	1.336282
-1003.421972	2.627555	1.341286
-1007.041996	1.531831	1.346291
-1011.364460	4.186462	1.351296
-1015.060235	10.547602	1.356301
-1018.251455	0.060440	1.361306
-1022.272139	3.564102	1.366310
-1025.901594	-2.007015	1.371315
-1029.691472	5.671749	1.376320
-1033.515553	10.298305	1.381325
-1037.290691	-5.237830	1.386330
-1041.326614	-0.979499	1.391334
-1044.704095	-14.464541	1.396339
-1048.661127	-5.853854	1.401344
-1052.506088	0.690474	1.406349
-1055.666706	-3.380227	1.411354
-1059.994951	1.957790	1.416358
-1063.703148	-2.533083	1.421363
-1067.439097	4.616723	1.426368
-1071.201288	-3.336344	1.431373
-1074.740915	2.607248	1.436378
-1078.871704	10.548781	1.441382
-1082.589302	10.127944	1.446387
-1086.125255	6.092095	1.451392
-1090.046497	6.429239	1.456397
-1093.486316	-13.351932	1.461402
-1097.432684	4.613104	1.466406
-1101.552242	1.537960	1.471411
-1105.179120	2.807317	1.476416
-1109.022377	-2.880848	1.481421
-1112.080326	-2.694392	1.486426
-1116.180172	-6.803979	1.491430
-1119.635584	4.222868	1.496435
-1124.072765	-5.457674	1.501440
-1128.073397	4.481595	1.506445
-1131.340788	-7.317835	1.511450
-1135.199035	-2.545307	1.516454
-1138.637609	-0.363017	1.521459
-1142.252566	-9.446525	1.526464
-1146.392830	6.378167	1.531469
-1150.040853	-3.600474	1.536474
-1154.109017	10.905419	1.541478
-1157.840532	0.673644	1.546483
-1161.391083	-2.522395	1.551488
-1165.160340	1.988365	1.556493
-1168.727389	-2.785115	1.561498
-1172.956212	0.674835	1.566502
-1176.461786	6.945862	1.571507
-1180.087025	0.407656	1.576512
-1183.880748	1.284366	1.581517
-1187.636738	-9.634131	1.586522
-1191.297299	2.398609	1.591526
-1195.629232	-1.703659	1.596531
-1199.275214	-1.639033	1.601536
-1203.145806	9.074327	1.606541
-1206.161092	-14.090885	1.611546
-1210.094874	-0.153615	1.616550
-1213.818379	-0.486564	1.621555
-1217.700802	-5.378228	1.626560
-1222.055622	2.132621	1.631565
-1225.387259	-1.486277	1.636570
-1229.781850	10.501568	1.641574
-1233.059644	6.214902	1.646579
-1236.493517	0.393632	1.651584
-1240.384337	0.726161	1.656589
-1244.056308	-1.849504	1.661594
-1248.043176	-3.397067	1.666598
-1251.742161	-3.782763	1.671603
-1255.398398	-2.836478	1.676608
-1259.170201	-1.239339	1.681613
-1262.832774	-2.578584	1.686618
-1267.262518	-1.298749	1.691622
-1270.432481	-2.671092	1.696627
-1273.974968	-2.331180	1.701632
-1278.054897	-1.851627	1.706637
-1281.453770	-3.919014	1.711642
-1285.516252	3.452120	1.716646
-1289.091435	2.698164	1.721651
-1293.458552	9.356414	1.726656
-1296.931030	12.017444	1.731661
-1300.432635	1.585114	1.736666
-1304.326705	8.593438	1.741670
-1308.004766	5.846964	1.746675
-1311.782414	-2.077987	1.751680
-1315.925855	0.056542	1.756685
-1319.337272	0.228889	1.761690
-1323.305829	8.698370	1.766694
-1327.099189	4.525910	1.771699
-1330.622209	-3.922309	1.776704
-1334.554227	-3.907874	1.781709
-1337.930485	-6.213760	1.786714
-1342.198962	7.291603	1.791718
-1345.939887	0.183992	1.796723
-1349.330970	-6.041338	1.801728
-1353.350378	-3.291095	1.806733
-1356.721715	-6.190668	1.811738
-1360.441621	-3.008972	1.816742
-1364.103135	0.926619	1.821747
-1368.212523	0.423887	1.826752
-1372.315565	1.487618	1.831757
-1375.977118	3.565607	1.836762
-1379.831227	2.342367	1.841766
-1383.661014	1.042702	1.846771
-1387.322598	1.226816	1.851776
-1390.788885	13.048979	1.856781
-1394.509584	-3.003002	1.861786
-1398.237171	-3.573116	1.866790
-1401.594738	-4.784355	1.871795
-1405.911313	-2.962564	1.876800
-1410.019431	13.746804	1.881805
-1413.430631	-5.730911	1.886810
-1417.021251	7.754355	1.891814
-1420.942683	-1.754280	1.896819
-1424.594555	-0.012075	1.901824
-1428.961729	4.064990	1.906829
-1432.386983	-4.311986	1.911834
-1436.125768	7.684754	1.916838
-1439.627721	-2.458711	1.921843
-1443.166842	-3.689702	1.926848
-1447.145667	10.376581	1.931853
-1450.820946	-2.470359	1.936858
-1454.803826	5.914896	1.941862
-1458.660189	9.323603	1.946867
-1462.631975	4.932366	1.951872
-1466.113482	14.910484	1.956877
-1469.643668	-4.825623	1.961882
-1473.792489	9.655849	1.966886
-1477.367512	9.425703	1.971891
-1480.898709	17.298711	1.976896
-1484.844761	7.891898	1.981901
-1488.492086	7.991889	1.986906
-1492.458318	5.146786	1.991910
-1496.384544	8.907360	1.996915
-1500.196287	14.490477	2.006912
-1500.874494	5.046457	2.016909
-1498.488052	0.238491	2.026906
-1495.864031	7.727244	2.036902
-1493.555775	6.814444	2.046899
-1491.602154	5.112122	2.056896
-1489.653282	3.330036	2.066893
-1487.757802	0.722816	2.076890
-1486.169727	2.607994	2.086886
-1484.318573	9.881057	2.096883
-1482.339327	2.523573	2.106880
-1480.032030	2.220415	2.116877
-1478.234400	-2.029025	2.126874
-1476.648993	2.859751	2.136870
-1474.501352	4.173749	2.146867
-1472.966355	3.738484	2.156864
-1470.634792	2.324605	2.166861
-1468.627303	-2.337382	2.176858
-1467.061147	-1.051840	2.186854
-1465.177859	-2.979719	2.196851
-1463.201379	-2.029882	2.206848
-1461.321933	-7.812939	2.216845
-1459.249679	-4.181588	2.226842
-1457.604012	1.321238	2.236838
-1455.787488	-6.657535	2.246835
-1453.917026	0.118247	2.256832
-1451.905643	-3.938033	2.266829
-1450.110248	-1.751290	2.276826
-1447.653688	-5.132007	2.286822
-1446.331694	2.694768	2.296819
-1444.529541	8.191497	2.306816
-1442.411526	0.287612	2.316813
-1440.635767	5.572253	2.326810
-1438.716189	1.756473	2.336806
-1436.862033	1.879602	2.346803
-1435.006539	2.458836	2.356800
-1433.131409	1.410185	2.366797
-1430.865625	11.651652	2.376794
-1429.312769	5.718801	2.386790
-1427.353944	1.307797	2.396787
-1425.868107	4.188339	2.406784
-1423.807599	-1.581053	2.416781
-1421.965092	-0.568675	2.426778
-1419.791793	-2.525585	2.436774
-1417.959327	0.356303	2.446771
-1415.921485	-1.402072	2.456768
-1413.974089	-1.614380	2.466765
-1412.623186	-0.419073	2.476762
-1410.643204	0.140249	2.486758
-1408.614877	-0.456067	2.496755
-1406.755249	-3.066955	2.506752
-1404.858731	-9.018493	2.516749
-1402.839091	-6.081298	2.526746
-1401.060333	-8.156600	2.536742
-1399.299565	-0.035309	2.546739
-1397.312308	-4.075049	2.556736
-1395.625748	-5.567164	2.566733
-1393.467585	1.442085	2.576730
-1391.690629	-3.809774	2.586726
-1389.751912	-0.076450	2.596723
-1387.822978	-3.459474	2.606720
-1386.152265	-0.289557	2.616717
-1384.265746	-8.944224	2.626714
-1382.333099	0.494831	2.636710
-1380.417586	4.182932	2.646707
-1378.813581	-0.136490	2.656704
-1376.769669	-0.361061	2.666701
-1374.882895	3.023750	2.676698
-1372.745184	0.027314	2.686694
-1370.982285	3.078274	2.696691
-1369.149054	2.213225	2.706688
-1367.254751	1.693666	2.716685
-1365.306008	-4.307258	2.726682
-1363.731892	1.524466	2.736678
-1361.651634	4.016205	2.746675
-1359.912433	2.894637	2.756672
-1357.723753	2.463748	2.766669
-1355.938633	3.927473	2.776666
-1354.214617	0.277279	2.786662
-1352.765621	4.087455	2.796659
-1350.249009	6.664089	2.806656
-1348.337414	-1.299831	2.816653
-1346.575505	-10.892946	2.826650
-1344.837949	-3.099473	2.836646
-1342.790373	2.953317	2.846643
-1340.920990	-0.751718	2.856640
-1339.217276	-1.434956	2.866637
-1337.313099	0.871833	2.876634
-1335.361540	-3.811092	2.886630
-1333.467079	3.529380	2.896627
-1331.654635	4.436117	2.906624
-1329.763822	6.389788	2.916621
-1327.914988	6.007013	2.926618
-1325.977227	5.343162	2.936614
-1324.251122	5.254773	2.946611
-1322.091390	9.293835	2.956608
-1320.440679	8.650673	2.966605
-1318.354360	6.704621	2.976602
-1316.445769	6.465449	2.986598
-1314.750824	6.126265	2.996595
-1312.954900	1.918270	3.006592
-1311.005481	-0.176388	3.016589
-1308.969694	2.571992	3.026586
-1307.143208	1.067017	3.036582
-1305.470513	-3.258615	3.046579
-1303.668625	-2.860169	3.056576
-1301.662291	1.915573	3.066573
-1299.548748	-4.144836	3.076570
-1297.805679	-6.166980	3.086566
-1296.024770	-5.594643	3.096563
-1294.020054	1.815058	3.106560
-1292.101339	1.460601	3.116557
-1290.269562	-0.359421	3.126554
-1288.404129	3.095196	3.136550
-1286.651352	2.486248	3.146547
-1284.897165	1.000757	3.156544
-1282.638864	-3.936486	3.166541
-1280.676904	-1.100474	3.176538
-1279.169342	-0.400689	3.186534
-1277.442473	2.987693	3.196531
-1275.363377	3.278635	3.206528
-1273.475270	-0.394608	3.216525
-1271.715674	-1.241478	3.226522
-1269.400467	0.865372	3.236518
-1267.840545	-1.768493	3.246515
-1265.954390	6.242847	3.256512
-1263.995171	2.621388	3.266509
-1262.102793	-1.153583	3.276506
-1260.330405	-2.804601	3.286502
-1258.398450	2.003611	3.296499
-1256.359183	-4.130138	3.306496
-1254.789214	0.262324	3.316493
-1252.880834	-4.318887	3.326490
-1251.051866	0.197916	3.336486
-1248.928058	4.317008	3.346483
-1247.183679	2.586798	3.356480
-1245.210420	2.585230	3.366477
-1243.127410	1.415041	3.376474
-1241.584572	1.921310	3.386470
-1239.719829	3.839755	3.396467
-1237.618862	6.168821	3.406464
-1235.796556	-0.896511	3.416461
-1233.872463	-0.729147	3.426458
-1232.089867	-5.021790	3.436454
-1230.438002	-4.414540	3.446451
-1228.917104	2.663701	3.456448
-1226.406361	1.966658	3.466445
-1224.492359	4.186708	3.476442
-1222.733984	1.326901	3.486438
-1220.716331	8.016180	3.496435
-1219.091727	3.677775	3.506432
-1217.109089	-2.533723	3.516429
-1215.253635	0.549918	3.526426
-1213.403510	8.080755	3.536422
-1211.480399	2.911423	3.546419
-1209.576078	5.463037	3.556416
-1207.749485	-0.150322	3.566413
-1205.832957	-0.108041	3.576410
-1204.087896	4.139598	3.586406
-1202.414716	9.696644	3.596403
-1200.086023	3.072937	3.606400
-1198.160185	-3.476826	3.616397
-1196.662548	-4.602250	3.626394
-1194.612776	0.532956	3.636390
-1192.606739	5.929376	3.646387
-1190.730696	11.387655	3.656384
-1188.857141	7.202064	3.666381
-1187.126308	2.778786	3.676378
-1185.334139	6.993639	3.686374
-1183.322681	4.398102	3.696371
-1181.515282	8.861576	3.706368
-1179.731199	-3.913422	3.716365
-1177.870501	4.286808	3.726362
-1175.901974	0.851827	3.736358
-1174.014927	5.916775	3.746355
-1172.141408	4.604906	3.756352
-1170.315886	-1.020886	3.766349
-1167.984028	3.128152	3.776346
-1166.454311	1.650244	3.786342
-1164.676308	9.418455	3.796339
-1162.484118	8.777187	3.806336
-1160.635485	0.155580	3.816333
-1159.219110	4.136897	3.826330
-1156.864656	1.278079	3.836326
-1155.076061	2.987724	3.846323
-1153.524914	1.089551	3.856320
-1151.686398	-1.795658	3.866317
-1149.261982	-2.764598	3.876314
-1147.656107	-6.713113	3.886310
-1145.813146	-0.297397	3.896307
-1144.037821	-5.166711	3.906304
-1141.769585	-9.132776	3.916301
-1140.256746	-9.035326	3.926298
-1138.275698	2.480438	3.936294
-1136.542900	-5.104189	3.946291
-1134.735505	-6.970715	3.956288
-1132.821582	-7.434802	3.966285
-1130.414198	-5.307821	3.976282
-1128.875653	-1.120242	3.986278
-1127.250507	0.388205	3.996275
-1125.428950	-0.705313	4.006272
-1123.362056	-3.860723	4.016269
-1121.347425	-6.110923	4.026266
-1119.443408	-4.726035	4.036262
-1117.496909	-2.793728	4.046259
-1115.783656	2.526445	4.056256
-1114.076292	-2.780401	4.066253
-1111.957791	-7.960385	4.076250
-1110.272803	-2.544109	4.086246
-1108.385194	-11.544542	4.096243
-1106.131624	-4.570795	4.106240
-1104.603429	-7.515270	4.116237
-1102.528453	-2.819803	4.126234
-1100.496487	-2.682218	4.136230
-1098.832621	-2.981536	4.146227
-1097.000788	-3.116669	4.156224
-1094.859303	-4.742926	4.166221
-1093.424342	-3.330347	4.176218
-1091.674545	-5.144995	4.186214
-1089.413747	2.343935	4.196211
-1087.509843	2.173596	4.206208
-1085.573995	-1.055557	4.216205
-1083.650713	-8.462197	4.226202
-1082.218513	-8.797075	4.236198
-1080.247668	-2.488604	4.246195
-1078.164368	-0.011300	4.256192
-1076.610771	-6.654583	4.266189
-1074.351193	-6.708123	4.276186
-1072.646419	-2.356041	4.286182
-1070.672515	-4.132312	4.296179
-1068.999207	-3.455744	4.306176
-1067.378384	-5.262375	4.316173
-1065.161747	-2.454282	4.326170
-1063.120277	-2.346605	4.336166
-1061.300700	2.168703	4.346163
-1059.437781	-1.392976	4.356160
-1057.640700	-3.123583	4.366157
-1055.700496	-3.696022	4.376154
-1053.703819	-5.292763	4.386150
-1051.963171	-4.668007	4.396147
-1050.264546	-7.691816	4.406144
-1048.480411	-15.328802	4.416141
-1046.016702	-11.631785	4.426138
-1044.715381	-8.974108	4.436134
-1042.456044	-6.583353	4.446131
-1040.876051	-8.476592	4.456128
-1038.784268	-10.530640	4.466125
-1036.949658	-9.895640	4.476122
-1035.165564	-6.168853	4.486118
-1033.364657	-7.055311	4.496115
-1031.355864	-8.110809	4.506112
-1029.336208	-12.104904	4.516109
-1027.185456	-8.907287	4.526106
-1025.802853	-13.978965	4.536102
-1024.169424	-9.558594	4.546099
-1022.290494	-4.716431	4.556096
-1019.990454	-7.051669	4.566093
-1018.055592	-3.565300	4.576090
-1016.415188	-7.115040	4.586086
-1014.416791	-5.490947	4.596083
-1012.517050	-7.462152	4.606080
-1010.461667	-7.563498	4.616077
-1008.925412	-5.066533	4.626074
-1006.972688	-8.790956	4.636070
-1005.226636	-11.716527	4.646067
-1003.316871	-5.395060	4.656064
-1001.122350	-10.272895	4.666061
-999.320521	-2.033093	4.676058
-997.816594	-0.579378	4.686054
-995.758085	-0.160155	4.696051
-993.923257	-2.597809	4.706048
-991.811403	-6.949254	4.716045
-990.031885	-2.684852	4.726042
-988.061387	-5.949468	4.736038
-986.502822	-4.992383	4.746035
-984.665131	-0.539910	4.756032
-982.288348	0.718958	4.766029
-980.405921	-2.479462	4.776026
-978.827887	-8.825013	4.786022
-976.927621	-3.441482	4.796019
-975.062067	-0.562942	4.806016
-973.346175	-4.923680	4.816013
-971.291278	-3.338585	4.826010
-969.442614	-9.054773	4.836006
-967.434824	-3.397901	4.846003
-965.906158	-4.550247	4.856000
-963.995799	-0.690434	4.865997
-961.868246	-10.925987	4.875994
-960.072696	-3.364101	4.885990
-958.138599	0.201392	4.895987
-956.040850	-6.397785	4.905984
-954.606013	-7.342486	4.915981
-952.613017	-9.555925	4.925978
-950.342505	-15.510084	4.935974
-948.913941	-5.626856	4.945971
-946.937345	-11.049272	4.955968
-945.120727	-13.029235	4.965965
-943.279045	-7.598414	4.975962
-941.074227	-6.915168	4.985958
-939.417053	-13.549666	4.995955
-937.732515	-4.004205	5.005952
-935.571935	-8.467604	5.015949
-933.618402	-5.599942	5.025946
-931.787523	-3.162668	5.035942
-930.081765	-8.456499	5.045939
-928.088185	-7.302091	5.055936
-926.408543	-3.596409	5.065933
-924.246906	1.658533	5.075930
-922.646903	-1.380997	5.085926
-920.843615	-3.485129	5.095923
-919.116438	-6.687098	5.105920
-916.615042	-6.062304	5.115917
-914.851585	-10.209552	5.125914
-913.393094	-9.519049	5.135910
-911.386901	-5.017670	5.145907
-909.234157	0.608185	5.155904
-907.395397	-2.238983	5.165901
-905.555070	-3.742705	5.175898
-903.739789	-2.812400	5.185894
-901.817055	-5.267198	5.195891
-900.152520	-5.124373	5.205888
-898.136413	-10.426751	5.215885
-896.155297	-12.935089	5.225882
-894.659537	-4.635209	5.235878
-892.416226	-5.837034	5.245875
-890.666491	-5.857826	5.255872
-888.569469	-9.693649	5.265869
-886.905312	-14.849744	5.275866
-884.981212	-6.732028	5.285862
-883.099434	-1.888622	5.295859
-881.400423	-2.114457	5.305856
-879.232309	-5.527424	5.315853
-877.330797	-7.156171	5.325850
-875.704520	-6.203520	5.335846
-873.704695	-9.557997	5.345843
-871.893391	-6.827016	5.355840
-869.914181	-10.741882	5.365837
-868.281272	-8.659752	5.375834
-866.549380	-1.997089	5.385830
-864.166620	-1.580642	5.395827
-862.608844	-3.283896	5.405824
-860.371845	-7.568394	5.415821
-858.728438	-8.944280	5.425818
-856.747591	-2.769836	5.435814
-854.984722	-1.106370	5.445811
-853.103117	-0.241892	5.455808
-851.357715	-8.834144	5.465805
-849.307477	-8.276100	5.475802
-847.260071	-8.284448	5.485798
-845.462884	-3.225379	5.495795
-843.769554	-6.360304	5.505792
-842.000019	-8.395822	5.515789
-839.939236	-5.189958	5.525786
-837.960886	-4.607779	5.535782
-836.379702	-9.406365	5.545779
-834.357378	-10.353332	5.555776
-832.200722	-13.609686	5.565773
-830.610429	-13.702840	5.575770
-828.868699	-7.684359	5.585766
-826.633437	-6.000073	5.595763
-824.856912	-3.550866	5.605760
-823.113509	-6.084303	5.615757
-821.302419	-8.086975	5.625754
-819.146894	-4.390969	5.635750
-817.480258	-2.135770	5.645747
-815.792861	-5.541309	5.655744
-813.714843	-6.958219	5.665741
-811.744201	-2.676856	5.675738
-809.805166	-1.988894	5.685734
-808.065664	-4.439591	5.695731
-806.268893	-2.832034	5.705728
-804.419305	-5.140850	5.715725
-802.432824	-7.463653	5.725722
-800.401673	-11.165711	5.735718
-798.400501	-7.433961	5.745715
-796.968875	-4.536438	5.755712
-794.901670	-3.837372	5.765709
-793.126336	-13.647011	5.775706
-791.121325	-9.424811	5.785702
-789.547394	-3.595792	5.795699
-787.426531	-7.935871	5.805696
-785.408252	-4.048946	5.815693
-783.679021	-8.847479	5.825690
-781.906783	-5.143857	5.835686
-779.817759	-2.777723	5.845683
-778.010652	-6.418690	5.855680
-776.154897	-6.415290	5.865677
-774.292728	1.091898	5.875674
-772.329409	-7.165658	5.885670
-770.541384	-9.963560	5.895667
-768.581913	-9.848836	5.905664
-766.758298	-5.127088	5.915661
-764.806951	-8.573202	5.925658
-763.250168	-9.414120	5.935654
-761.336034	-5.491580	5.945651
-759.095083	-5.748684	5.955648
-757.301694	-7.805321	5.965645
-755.412992	-4.492928	5.975642
-753.876653	-8.556393	5.985638
-751.992284	-4.739615	5.995635
-749.889777	-6.114593	6.005632
-747.806221	-13.093437	6.015629
-745.971424	-5.231324	6.025626
-744.182145	-6.924134	6.035622
-742.725529	-4.153730	6.045619
-740.719662	-0.045303	6.055616
-738.461256	-12.706354	6.065613
-736.512227	-3.403527	6.075610
-734.997526	-5.031920	6.085606
-733.030755	0.794358	6.095603
-731.138110	-7.469240	6.105600
-729.200205	-9.380004	6.115597
-727.408309	-3.637881	6.125594
-725.171217	2.839947	6.135590
-723.742741	0.688493	6.145587
-722.158975	-1.001456	6.155584
-719.930050	3.254501	6.165581
-717.830111	1.646274	6.175578
-716.440136	-8.348052	6.185574
-714.158037	-4.702175	6.195571
-712.249533	-2.199759	6.205568
-710.462385	-4.871161	6.215565
-708.623674	-2.136535	6.225562
-706.859426	1.723164	6.235558
-704.970710	-1.239206	6.245555
-702.800587	5.377244	6.255552
-701.047101	3.560711	6.265549
-699.220467	2.692499	6.275546
-697.281609	-4.852138	6.285542
-695.397682	-5.260549	6.295539
-693.456505	3.415149	6.305536
-691.632403	0.406272	6.315533
-689.988598	4.127336	6.325530
-688.118134	5.857422	6.335526
-685.827655	2.474017	6.345523
-684.217608	2.191487	6.355520
-682.717046	3.257521	6.365517
-680.536720	-1.336710	6.375514
-678.498470	-0.623441	6.385510
-676.502842	0.851387	6.395507
-675.078986	5.281828	6.405504
-672.783424	-1.770313	6.415501
-671.230013	5.397879	6.425498
-669.480198	2.418257	6.435494
-667.270948	1.007346	6.445491
-665.448359	4.530910	6.455488
-663.474567	6.231873	6.465485
-661.793395	0.552141	6.475482
-659.658552	-0.928979	6.485478
-657.803140	3.386723	6.495475
-656.356285	0.305519	6.505472
-654.133717	7.306801	6.515469
-652.478897	3.655519	6.525466
-650.357835	-3.738196	6.535462
-648.610301	3.305835	6.545459
-646.624155	1.415849	6.555456
-644.654623	1.404331	6.565453
-642.946781	3.593074	6.575450
-641.110694	-0.532431	6.585446
-639.161915	3.997319	6.595443
-637.212777	-0.570989	6.605440
-635.621500	6.382757	6.615437
-633.616251	0.420733	6.625434
-631.566653	5.940183	6.635430
-629.816839	3.769020	6.645427
-628.017545	-2.076406	6.655424
-626.182337	4.047309	6.665421
-624.272522	1.605846	6.675418
-622.109025	4.331283	6.685414
-620.389776	1.972376	6.695411
-618.420437	7.768349	6.705408
-616.827860	2.042801	6.715405
-614.798400	2.841216	6.725402
-612.843675	3.874207	6.735398
-610.945402	9.386275	6.745395
-609.248858	4.787291	6.755392
-607.157022	-2.728037	6.765389
-605.535685	-0.209653	6.775386
-603.655605	-0.151582	6.785382
-601.698289	2.125230	6.795379
-599.776968	4.913065	6.805376
-598.025463	10.657017	6.815373
-596.222323	3.334662	6.825370
-593.942024	-0.612301	6.835366
-592.392779	-0.452418	6.845363
-590.244152	1.026462	6.855360
-588.650146	4.716082	6.865357
-586.400233	3.991915	6.875354
-584.752586	-5.925093	6.885350
-582.929241	-6.712162	6.895347
-581.035494	-1.057243	6.905344
-579.053763	-0.844864	6.915341
-577.233030	-1.241507	6.925338
-575.590344	-4.696584	6.935334
-573.811343	4.128292	6.945331
-571.630618	-3.230680	6.955328
-569.623793	-3.947576	6.965325
-567.654464	-8.037468	6.975322
-565.998533	-3.105606	6.985318
-564.138238	-2.936974	6.995315
-562.393685	-1.914577	7.005312
-560.346481	2.782678	7.015309
-558.720677	0.642429	7.025306
-556.482257	-0.326192	7.035302
-554.864548	6.182859	7.045299
-552.870083	1.225265	7.055296
-550.962612	0.271621	7.065293
-549.316419	-1.851352	7.075290
-547.407668	1.480120	7.085286
-545.092671	6.491459	7.095283
-543.462594	1.851031	7.105280
-541.830640	3.005116	7.115277
-539.712853	-0.396356	7.125274
-537.839707	-0.690815	7.135270
-536.041652	7.093671	7.145267
-534.274475	5.144015	7.155264
-532.312562	6.949621	7.165261
-530.039793	1.344423	7.175258
-528.696615	2.566751	7.185254
-527.108213	2.360417	7.195251
-524.704287	10.889725	7.205248
-522.786315	4.483826	7.215245
-520.941208	-0.915680	7.225242
-518.846299	5.034010	7.235238
-517.293681	1.433880	7.245235
-515.600676	-0.882866	7.255232
-513.395083	-1.413567	7.265229
-511.237920	0.165076	7.275226
-509.596157	-4.325614	7.285222
-508.195282	3.257067	7.295219
-506.131324	9.680668	7.305216
-504.210746	2.197510	7.315213
-502.165332	-2.539230	7.325210
-500.144386	-3.360957	7.335206
-498.383186	0.788344	7.345203
-496.854415	-1.980584	7.355200
-494.806865	1.289288	7.365197
-492.760041	-1.672910	7.375194
-490.852285	-7.882936	7.385190
-489.039426	-4.329256	7.395187
-487.175328	4.033675	7.405184
-485.190066	1.049736	7.415181
-483.390948	-1.517623	7.425178
-481.700019	-4.945607	7.435174
-479.872206	4.432087	7.445171
-477.991831	-1.828823	7.455168
-475.844792	-6.168082	7.465165
-473.793309	2.711255	7.475162
-471.986692	1.317459	7.485158
-470.477041	-6.458466	7.495155
-468.912427	0.924403	7.505152
-466.699557	-2.062714	7.515149
-464.398488	-5.769713	7.525146
-462.769808	-4.313467	7.535142
-460.834381	-6.272571	7.545139
-458.928459	0.841056	7.555136
-456.993117	-0.903291	7.565133
-455.410683	-3.053914	7.575130
-453.514825	-2.717188	7.585126
-451.599954	-2.850871	7.595123
-449.419365	-0.776959	7.605120
-447.803651	-6.460307	7.615117
-446.002935	-0.831467	7.625114
-444.090185	-1.275863	7.635110
-442.121756	-1.144930	7.645107
-440.469948	0.137109	7.655104
-438.286028	-2.554828	7.665101
-436.575562	-0.252665	7.675098
-434.747128	-1.935711	7.685094
-432.831664	-0.091026	7.695091
-430.710593	-3.342928	7.705088
-429.223030	-0.315154	7.715085
-427.363516	2.747962	7.725082
-425.197545	-0.721109	7.735078
-423.196986	-10.695956	7.745075
-421.387596	-4.162155	7.755072
-419.809505	0.918040	7.765069
-417.660218	-4.157329	7.775066
-415.972942	-3.231468	7.785062
-414.302316	-5.350357	7.795059
-412.142696	-2.562525	7.805056
-410.072990	-3.785126	7.815053
-408.341265	-4.832173	7.825050
-406.857314	-8.255477	7.835046
-404.401027	-5.563959	7.845043
-402.509862	-4.388010	7.855040
-400.931358	-0.820521	7.865037
-398.949393	0.702516	7.875034
-397.033931	0.878260	7.885030
-395.292309	-3.827253	7.895027
-393.429012	0.386354	7.905024
-391.648966	0.307406	7.915021
-389.703939	-4.765324	7.925018
-387.770772	-0.439709	7.935014
-385.857818	-4.834674	7.945011
-383.979553	-2.172419	7.955008
-382.316939	-2.614720	7.965005
-380.320731	-3.782927	7.975002
-378.507304	-4.931422	7.984998
-376.351928	-5.902406	7.994995
-374.823371	-4.966962	8.004992
-372.669582	-3.441338	8.014989
-370.754254	-3.715558	8.024986
-368.958710	-9.577573	8.034982
-366.869061	-7.980123	8.044979
-365.279149	-7.509213	8.054976
-363.383106	-10.409332	8.064973
-361.399392	-13.141866	8.074970
-359.899096	-4.826533	8.084966
-358.043679	-6.381196	8.094963
-355.611094	-3.333732	8.104960
-354.157015	-7.383823	8.114957
-351.847500	-8.595715	8.124954
-350.054132	-7.077263	8.134950
-348.343939	-3.856031	8.144947
-346.627691	5.001162	8.154944
-344.498434	1.299598	8.164941
-342.746811	5.886348	8.174938
-341.135223	1.045312	8.184934
-338.916983	-0.668318	8.194931
-337.202610	1.364869	8.204928
-334.815414	-1.346799	8.214925
-333.403587	2.324718	8.224922
-331.767814	-2.044901	8.234918
-330.042095	2.640731	8.244915
-327.914545	-1.764767	8.254912
-325.561671	0.984398	8.264909
-323.620928	-1.048079	8.274906
-321.817130	-8.592984	8.284902
-320.426580	0.434649	8.294899
-318.521450	-1.712141	8.304896
-316.354619	3.613617	8.314893
-314.560733	-9.700841	8.324890
-312.627714	-2.248777	8.334886
-310.907401	2.387206	8.344883
-308.956407	-2.534835	8.354880
-307.196003	-4.380612	8.364877
-305.300398	-1.659481	8.374874
-303.327753	3.847292	8.384870
-301.303184	0.933015	8.394867
-299.539779	0.853634	8.404864
-297.942663	0.262371	8.414861
-295.697805	-4.962365	8.424858
-293.979471	0.542380	8.434854
-292.064720	-0.822755	8.444851
-290.212985	4.643330	8.454848
-288.311855	3.059316	8.464845
-286.356961	-4.804955	8.474842
-284.280931	-1.531547	8.484838
-282.802976	1.314697	8.494835
-280.786521	-4.846213	8.504832
-279.058153	-3.162590	8.514829
-277.283477	-1.391621	8.524826
-275.264440	0.982985	8.534822
-273.125353	-6.016980	8.544819
-271.310480	1.496614	8.554816
-269.543597	-0.781230	8.564813
-267.594747	-5.227626	8.574810
-265.877451	-8.684938	8.584807
-264.211419	0.267180	8.594803
-262.116378	-12.417937	8.604800
-259.969337	-2.811536	8.614797
-257.989366	-8.609754	8.624794
-256.302886	-5.847308	8.634791
-254.579596	-4.611285	8.644787
-252.781694	-3.031902	8.654784
-251.038738	-5.648550	8.664781
-249.132547	-2.960643	8.674778
-246.804879	4.371647	8.684775
-245.293875	-0.326956	8.694771
-243.640343	-5.311995	8.704768
-241.374364	1.984356	8.714765
-239.631083	-3.362381	8.724762
-237.430216	1.645383	8.734759
-235.893714	5.303378	8.744755
-234.024344	3.727634	8.754752
-231.970000	4.132399	8.764749
-229.879701	1.866121	8.774746
-228.175742	3.335779	8.784743
-226.525959	0.656649	8.794739
-224.914919	2.485356	8.804736
-222.802396	6.152477	8.814733
-220.595560	0.074912	8.824730
-218.556629	3.194825	8.834727
-217.298000	0.537078	8.844723
-215.344763	-1.999422	8.854720
-213.004307	0.415518	8.864717
-211.325617	-1.406096	8.874714
-209.726611	-2.018130	8.884711
-207.522676	-7.068885	8.894707
-205.417415	-3.072166	8.904704
-203.831754	-1.844141	8.914701
-202.240237	-0.833368	8.924698
-199.884768	0.139165	8.934695
-198.018708	-5.514512	8.944691
-196.301769	-7.067478	8.954688
-194.368873	-11.598114	8.964685
-192.485547	-3.849062	8.974682
-190.798233	-3.551477	8.984679
-188.922875	-10.772970	8.994675
-186.824103	-6.358350	9.004672
-185.211503	-3.697747	9.014669
-183.180037	-11.864691	9.024666
-181.466396	-5.664363	9.034663
-179.572807	-8.256053	9.044659
-177.662512	-6.530337	9.054656
-175.993035	-1.114021	9.064653
-173.832687	-5.851471	9.074650
-171.584964	-6.071209	9.084647
-170.003509	-6.490939	9.094643
-168.646105	-3.996443	9.104640
-166.373373	-2.522771	9.114637
-164.491443	-4.384682	9.124634
-162.658901	-9.054019	9.134631
-160.790982	-8.101540	9.144627
-158.795548	-11.664744	9.154624
-157.032636	-11.822891	9.164621
-154.926303	-5.772054	9.174618
-153.301837	-8.172353	9.184615
-151.511969	-2.205221	9.194611
-149.297638	-4.284379	9.204608
-147.766951	-9.998186	9.214605
-145.946895	-5.265888	9.224602
-143.777417	-7.067878	9.234599
-142.293415	-6.076226	9.244595
-140.326447	4.313785	9.254592
-137.984340	-9.800167	9.264589
-136.108260	-7.124731	9.274586
-134.840734	-8.515940	9.284583
-132.693980	-7.677407	9.294579
-130.637595	-1.825420	9.304576
-128.815563	-8.364141	9.314573
-126.867985	-6.524331	9.324570
-124.975354	-0.320939	9.334567
-123.145687	-4.743471	9.344563
-121.692940	-5.382636	9.354560
-119.494213	-8.967196	9.364557
-117.186018	-6.916494	9.374554
-115.665859	-12.156489	9.384551
-114.200517	-3.385394	9.394547
-112.143659	-2.750397	9.404544
-110.038721	-4.606797	9.414541
-108.093824	-9.390341	9.424538
-106.230988	-4.511677	9.434535
-104.343596	-9.661838	9.444531
-102.526069	-8.830749	9.454528
-100.876217	-9.255031	9.464525
-99.261215	-4.952617	9.474522
-96.586961	-4.360853	9.484519
-95.109444	-2.614965	9.494515
-93.249351	1.760456	9.504512
-91.254736	-0.263066	9.514509
-89.139497	-4.892193	9.524506
-87.869798	-7.665327	9.534503
-85.746167	2.211833	9.544499
-83.791183	1.187816	9.554496
-81.897208	-1.119647	9.564493
-80.148932	1.465699	9.574490
-77.940129	-5.245227	9.584487
-76.341291	-3.174467	9.594483
-74.400026	0.755379	9.604480
-72.761825	3.707247	9.614477
-70.772519	-5.848705	9.624474
-68.727164	-1.575455	9.634471
-66.941758	0.536600	9.644467
-64.980649	2.988526	9.654464
-63.110104	0.801659	9.664461
-61.345246	0.846959	9.674458
-59.604390	-2.192388	9.684455
-57.599463	1.897846	9.694451
-55.394529	2.847169	9.704448
-53.930064	0.379299	9.714445
-52.149283	-5.008032	9.724442
-49.944013	-4.431397	9.734439
-48.123274	-1.175471	9.744435
-46.429437	-1.819895	9.754432
-44.454073	1.701898	9.764429
-42.343718	-1.810076	9.774426
-40.579948	4.001834	9.784423
-38.873166	6.102770	9.794419
-36.999798	1.427005	9.804416
-35.084296	0.830911	9.814413
-32.855247	1.594825	9.824410
-31.255089	2.484332	9.834407
-29.525588	1.199481	9.844403
-27.417430	2.606382	9.854400
-25.764594	5.238574	9.864397
-23.833379	-1.641187	9.874394
-21.932125	2.355088	9.884391
-19.826209	2.404433	9.894387
-18.296933	3.540523	9.904384
-16.334003	8.018028	9.914381
-14.405206	3.772392	9.924378
-12.500629	0.468534	9.934375
-10.784771	1.705920	9.944371
-8.999659	2.968577	9.954368
-6.691235	6.334640	9.964365
-5.495135	18.739370	9.974362
-4.066052	36.143895	9.984359
-2.520660	67.451787	9.994355
-1.032277	122.207355	10.004352
0.000000	173.281723	10.009357
0.546584	209.490285	10.014362
1.518815	232.034285	10.019367
1.793304	263.791986	10.024371
2.266434	284.315137	10.029376
2.530881	295.535822	10.034381
2.589456	307.986292	10.039386
3.038736	320.265636	10.044391
3.221862	340.040322	10.049395
3.452316	343.586505	10.054400
3.380923	342.128144	10.059405
3.020905	348.919353	10.064410
3.588077	344.091597	10.069415
3.304869	360.263146	10.074419
3.394848	349.790163	10.079424
3.823406	355.250761	10.084429
3.517883	362.079016	10.089434
3.802976	356.816845	10.094439
3.424797	370.163383	10.099443
3.511169	362.690417	10.104448
3.528871	368.027317	10.109453
3.393215	394.891860	10.114458
3.718115	392.195414	10.119463
3.620538	398.353408	10.124467
4.064709	402.349653	10.129472
4.242280	404.650570	10.134477
4.250134	401.482709	10.139482
4.087075	406.987234	10.144487
4.017679	418.529357	10.149491
4.189479	414.778659	10.154496
4.587862	416.643796	10.159501
4.540848	420.166447	10.164506
4.643653	411.222644	10.169511
4.596607	422.191908	10.174515
4.827095	421.992721	10.179520
4.760816	423.879939	10.184525
4.502007	427.737583	10.189530
4.827387	431.716514	10.194535
4.794038	431.795964	10.199539
4.862685	427.754201	10.204544
4.615262	421.758485	10.209549
4.489630	434.667392	10.214554
4.597823	434.820461	10.219559
4.885222	432.232495	10.224563
4.922738	435.905674	10.229568
5.167357	432.791505	10.234573
5.076040	436.858985	10.239578
4.920058	442.736145	10.244583
4.962123	441.981944	10.249587
4.942256	443.827067	10.254592
5.121589	440.994555	10.259597
4.946831	444.495009	10.264602
5.126722	440.817133	10.269607
5.259933	447.450860	10.274611
5.178815	450.862260	10.279616
5.351676	443.041131	10.284621
4.915150	447.382883	10.289626
5.595867	471.500303	10.294631
5.690231	479.045444	10.299635
5.221050	476.147633	10.304640
5.330174	481.056815	10.309645
5.388593	485.114616	10.314650
5.804936	489.364493	10.319655
5.668116	490.865565	10.324659
5.683472	487.426819	10.329664
5.751739	493.826490	10.334669
5.556593	498.624936	10.339674
5.977584	490.901401	10.344679
5.619788	494.315942	10.349683
5.586894	496.171035	10.354688
5.949216	493.498565	10.359693
5.610747	512.016227	10.364698
5.901572	516.569996	10.369703
6.095164	531.590155	10.374707
6.477376	533.306494	10.379712
6.520810	532.944748	10.384717
6.222825	533.274577	10.389722
6.408346	537.097644	10.394727
6.204612	543.810395	10.399731
6.170434	552.543072	10.404736
6.022385	545.164179	10.409741
5.943448	548.969507	10.414746
6.442578	538.752835	10.419751
6.406072	546.080758	10.424755
6.546860	557.266176	10.429760
6.970773	568.546795	10.434765
6.748383	575.166338	10.439770
7.038346	577.332655	10.444775
6.804241	575.810335	10.449779
6.673597	569.184046	10.454784
7.078986	567.843583	10.459789
6.910531	577.819884	10.464794
7.142568	575.278573	10.469799
7.006720	582.702788	10.474803
7.247481	585.438374	10.479808
7.378093	579.986290	10.484813
6.948919	584.274868	10.489818
7.045503	579.828043	10.494823
7.083367	585.440940	10.499827
7.086960	588.728468	10.504832
7.274138	581.411205	10.509837
7.264624	588.529831	10.514842
7.421485	586.461000	10.519847
7.261019	586.797280	10.524851
7.266118	587.802617	10.529856
7.447422	586.920539	10.534861
7.245464	600.803751	10.539866
7.454218	592.853809	10.544871
7.266014	606.859419	10.549875
7.679647	617.689110	10.554880
7.765316	623.616109	10.559885
7.861792	630.430830	10.564890
7.669065	632.794005	10.569895
7.785782	638.529968	10.574899
7.826990	632.912344	10.579904
7.641513	634.153098	10.584909
7.575464	643.089618	10.589914
8.090061	634.106802	10.594919
7.901961	654.117758	10.599923
7.879719	659.560490	10.604928
8.533088	663.490322	10.609933
8.088493	666.478757	10.614938
7.962707	668.519008	10.619943
8.503543	676.500838	10.624947
8.347805	684.467622	10.629952
8.466041	673.108339	10.634957
8.048352	684.649458	10.639962
8.130987	672.980447	10.644967
8.234711	679.909158	10.649971
8.181816	675.079274	10.654976
8.729008	688.228028	10.659981
8.861576	704.473992	10.664986
8.906221	710.909068	10.669991
8.793131	712.207670	10.674995
8.512994	726.174439	10.680000
8.845421	718.258321	10.685005
8.816322	719.294355	10.690010
8.669606	717.288123	10.695015
8.952410	720.442829	10.700019
8.661581	722.252357	10.705024
9.048424	719.429271	10.710029
8.750688	725.537324	10.715034
8.819320	720.289050	10.720039
9.109699	730.461938	10.725043
9.519882	745.296374	10.730048
9.373099	754.488704	10.735053
9.318213	757.605815	10.740058
9.238390	756.585597	10.745063
9.118291	762.337307	10.750067
9.399438	764.304775	10.755072
9.532466	757.661573	10.760077
9.413800	758.774978	10.765082
9.587657	761.783059	10.770087
9.603014	763.275654	10.775091
9.289801	768.171873	10.780096
9.796045	764.459206	10.785101
9.754258	767.457529	10.790106
9.733241	768.577437	10.795111
9.630572	765.181108	10.800115
9.723735	788.113798	10.805120
10.258246	794.593780	10.810125
9.893082	804.221545	10.815130
10.100826	803.972363	10.820135
10.415378	796.019628	10.825139
9.960599	804.564065	10.830144
10.354300	799.987774	10.835149
9.916813	798.362246	10.840154
10.068406	803.047131	10.845159
9.904508	802.412504	10.850163
10.073801	802.472247	10.855168
10.160248	802.291302	10.860173
10.089991	812.668439	10.865178
10.398455	807.774561	10.870183
10.097534	816.237690	10.875187
10.665571	838.504895	10.880192
10.905043	837.039478	10.885197
10.499755	848.274377	10.890202
10.628883	838.909773	10.895207
11.101981	842.270708	10.900211
10.686252	849.596192	10.905216
11.016734	842.169203	10.910221
10.723096	844.528007	10.915226
10.896463	847.047298	10.920231
11.001615	850.583629	10.925235
10.714913	841.200193	10.930240
10.888183	838.934732	10.935245
10.864817	853.477291	10.940250
10.726603	849.684464	10.945255
11.046937	849.000980	10.950259
10.772759	871.194409	10.955264
11.028692	875.615077	10.960269
11.383507	886.806035	10.965274
11.192022	881.113462	10.970279
11.578554	886.170932	10.975283
11.274859	896.367732	10.980288
11.467105	882.613550	10.985293
11.256173	891.590681	10.990298
11.330296	892.821587	10.995303
11.449533	897.212023	11.000307
11.213631	894.701142	11.005312
11.606284	897.882522	11.010317
11.519216	917.701094	11.015322
11.394218	917.309431	11.020327
11.541276	922.703178	11.025331
11.707403	925.095896	11.030336
11.773345	920.228050	11.035341
11.637660	937.261435	11.040346
11.806030	937.490072	11.045351
12.109241	951.657338	11.050355
12.152296	961.737367	11.055360
12.261627	963.875782	11.060365
12.482518	970.841140	11.065370
12.156300	958.440701	11.070375
12.559983	974.508093	11.075379
12.368273	971.619539	11.080384
12.637971	957.654223	11.085389
12.285312	956.955074	11.090394
12.418010	973.010493	11.095399
12.591653	970.183518	11.100403
12.593783	971.988926	11.105408
12.657325	971.989841	11.110413
12.613616	980.364723	11.115418
12.498161	972.911022	11.120423
12.655225	977.940468	11.125427
12.410048	978.383316	11.130432
12.875428	977.418052	11.135437
12.851649	985.188897	11.140442
12.799306	977.053298	11.145447
12.763607	976.989612	11.150451
12.687238	981.829197	11.155456
12.956020	980.349629	11.160461
12.787953	987.260334	11.165466
13.071142	991.078983	11.170471
13.168115	1000.844487	11.175475
13.370382	1013.835654	11.180480
13.441039	1005.522712	11.185485
13.199997	1019.425173	11.190490
13.598132	1013.078638	11.195495
13.545575	1011.431111	11.200499
13.290010	1006.647638	11.205504
13.600078	1005.500551	11.210509
13.222538	1014.136875	11.215514
13.482401	1001.512016	11.220519
13.518529	1006.059256	11.225523
13.413419	1013.754773	11.230528
13.622962	1010.789591	11.235533
13.517073	1018.433192	11.240538
13.360958	1026.961660	11.245543
13.558878	1023.110439	11.250547
13.159478	1024.178751	11.255552
13.900679	1039.336029	11.260557
13.768393	1051.215139	11.265562
13.981419	1051.605402	11.270567
14.195318	1056.837138	11.275571
13.881550	1057.625267	11.280576
14.148280	1049.394574	11.285581
14.087920	1058.336749	11.290586
14.148631	1058.929517	11.295591
14.074242	1054.602867	11.300595
13.791625	1055.048535	11.305600
14.116960	1055.430346	11.310605
14.120575	1066.084484	11.315610
14.338261	1071.744585	11.320615
14.611018	1072.877585	11.325619
14.326583	1088.406689	11.330624
14.546352	1078.581160	11.335629
14.457925	1080.727481	11.340634
14.289506	1078.303582	11.345639
14.150960	1076.240800	11.350643
14.260935	1087.269102	11.355648
14.806695	1093.996604	11.360653
15.062056	1114.092008	11.365658
15.005093	1117.886094	11.370663
15.237757	1102.087673	11.375667
14.800125	1094.491320	11.380672
15.442959	1094.707361	11.385677
15.055759	1097.010160	11.390682
14.935749	1096.453680	11.395687
15.368545	1094.318685	11.400691
14.887440	1100.801523	11.405696
15.014565	1104.342297	11.410701
15.036670	1121.506858	11.415706
15.276082	1116.445683	11.420711
15.474060	1121.142197	11.425715
15.251671	1124.040081	11.430720
15.396723	1125.081483	11.435725
15.340774	1126.106057	11.440730
15.292986	1130.796042	11.445735
15.793430	1130.973291	11.450739
15.625084	1122.271016	11.455744
15.692156	1116.926647	11.460749
15.437415	1128.151939	11.465754
15.194019	1129.586490	11.470759
15.423143	1126.550347	11.475763
15.324814	1144.931149	11.480768
15.904676	1141.919488	11.485773
15.728822	1158.155226	11.490778
15.743214	1164.811389	11.495783
15.885637	1157.505709	11.500787
15.834296	1162.645739	11.505792
16.192369	1152.891148	11.510797
16.021143	1159.649462	11.515802
15.878754	1157.240322	11.520807
16.043597	1175.151795	11.525811
16.422277	1192.130242	11.530816
16.726417	1198.741779	11.535821
16.762481	1184.892367	11.540826
16.447495	1165.320526	11.545831
17.005085	1150.438554	11.550835
16.822624	1158.187490	11.555840
16.733036	1149.759666	11.560845
16.328840	1165.479856	11.565850
16.578695	1159.395050	11.570855
16.986859	1155.130182	11.575859
16.646859	1161.128453	11.580864
16.438554	1163.647174	11.585869
16.687470	1155.286788	11.590874
16.946284	1152.892507	11.595879
16.946840	1160.782577	11.600883
16.872359	1168.924337	11.605888
17.411887	1178.944249	11.610893
17.138047	1159.914678	11.615898
16.985740	1157.735797	11.620903
17.064397	1152.100960	11.625907
17.039696	1158.801206	11.630912
17.272721	1167.122592	11.635917
17.383201	1173.690886	11.640922
17.498005	1179.875261	11.645927
17.914251	1169.534167	11.650931
17.595496	1159.368671	11.655936
17.803011	1152.087306	11.660941
17.660071	1161.608890	11.665946
17.212278	1166.928864	11.670951
17.575069	1154.964024	11.675955
17.315516	1153.745346	11.680960
17.416994	1145.594578	11.685965
17.570237	1163.821728	11.690970
17.699134	1179.478979	11.695975
17.904701	1196.111274	11.700979
17.538871	1194.385952	11.705984
17.773517	1194.086738	11.710989
17.500143	1189.146759	11.715994
17.624380	1193.369317	11.720999
18.018436	1182.124928	11.726003
18.010191	1193.484432	11.731008
17.860671	1184.615100	11.736013
18.225919	1191.123839	11.741018
17.902651	1189.028998	11.746023
18.215509	1184.903914	11.751027
18.084823	1195.587455	11.756032
18.375394	1198.102307	11.761037
18.317881	1216.292170	11.766042
18.519051	1212.460884	11.771047
18.589022	1202.725404	11.776051
18.410792	1220.090785	11.781056
18.418329	1214.937241	11.786061
18.554876	1211.606738	11.791066
18.374614	1214.788104	11.796071
18.435182	1220.533254	11.801075
18.367935	1225.109668	11.806080
18.610824	1211.090033	11.811085
18.737453	1215.389494	11.816090
18.358664	1212.332018	11.821095
18.809085	1211.869065	11.826099
18.635823	1225.406065	11.831104
18.824397	1233.263029	11.836109
18.927650	1248.317265	11.841114
18.972519	1248.255709	11.846119
18.947965	1243.634022	11.851123
18.766740	1258.138292	11.856128
19.052569	1244.413002	11.861133
19.048746	1245.374072	11.866138
19.196315	1251.239410	11.871143
19.470865	1243.506510	11.876147
19.146406	1246.910385	11.881152
19.523005	1242.392672	11.886157
19.197804	1254.320067	11.891162
19.276510	1254.778286	11.896167
19.879017	1259.407166	11.901171
19.628576	1269.037438	11.906176
19.759971	1251.318336	11.911181
19.798813	1248.057819	11.916186
19.659004	1255.297699	11.921191
19.798983	1246.768539	11.926195
19.665877	1251.252167	11.931200
19.921809	1251.999112	11.936205
20.326429	1261.751205	11.941210
19.880850	1253.839038	11.946215
20.105165	1248.236918	11.951219
19.867539	1254.480695	11.956224
19.941029	1255.443627	11.961229
20.296048	1260.198724	11.966234
20.218802	1266.360148	11.971239
20.110098	1256.064877	11.976243
20.405050	1269.212603	11.981248
20.283882	1265.471357	11.986253
20.063209	1274.388769	11.991258
20.107174	1281.861935	11.996263
20.557184	1283.263963	12.001267
20.318759	1287.016857	12.006272
20.400053	1283.555577	12.011277
20.495781	1284.119113	12.016282
20.568293	1292.731915	12.021287
20.608675	1278.504799	12.026291
20.437329	1287.903251	12.031296
20.501126	1283.824174	12.036301
20.389138	1285.903314	12.041306
20.656338	1285.611523	12.046311
20.834601	1278.266947	12.051315
20.733510	1286.029782	12.056320
20.432826	1280.535047	12.061325
21.059380	1279.564560	12.066330
20.816078	1264.811009	12.071335
20.743550	1250.259701	12.076339
20.144620	1253.971521	12.081344
20.610753	1237.110603	12.086349
20.453918	1241.784898	12.091354
20.361869	1244.479860	12.096359
20.860519	1238.774055	12.101363
20.426929	1254.618888	12.106368
20.212960	1241.048234	12.111373
20.481909	1244.269927	12.116378
20.471636	1247.605551	12.121383
20.977964	1242.597171	12.126387
20.728684	1252.931420	12.131392
20.811362	1253.538829	12.136397
20.809739	1251.167150	12.141402
20.539729	1263.316792	12.146407
20.501186	1253.996804	12.151411
20.400039	1261.845587	12.156416
20.690003	1256.656441	12.161421
20.800285	1259.830899	12.166426
20.526708	1253.956502	12.171431
20.570190	1259.694931	12.176435
20.424132	1260.372733	12.181440
20.583923	1260.052339	12.186445
20.656071	1261.816650	12.191450
20.353209	1270.720359	12.196455
20.958105	1259.405218	12.201459
20.534581	1259.998746	12.206464
20.491217	1239.486111	12.211469
20.533025	1240.362625	12.216474
20.406081	1239.207162	12.221479
20.776190	1244.527600	12.226483
20.370111	1240.885427	12.231488
20.676932	1229.885172	12.236493
20.744460	1223.853078	12.241498
20.524575	1232.808189	12.246503
20.613405	1226.561366	12.251507
20.567405	1232.238357	12.256512
20.499149	1224.778575	12.261517
20.756095	1227.691491	12.266522
20.572203	1235.136318	12.271527
20.730333	1232.400085	12.276531
20.411719	1233.110142	12.281536
20.465179	1229.895398	12.286541
20.378760	1225.294625	12.291546
20.083707	1235.930290	12.296551
20.546373	1220.621802	12.301555
20.602370	1224.662849	12.306560
20.661346	1214.323512	12.311565
20.770632	1212.842552	12.316570
20.400729	1213.576559	12.321575
20.676675	1214.830499	12.326579
20.556903	1228.702776	12.331584
20.898500	1218.036057	12.336589
20.882037	1214.718920	12.341594
20.840246	1221.417189	12.346599
20.788072	1213.019633	12.351603
20.740457	1216.211382	12.356608
20.273291	1205.244708	12.361613
20.323717	1197.996264	12.366618
19.976038	1206.984360	12.371623
20.344578	1214.681710	12.376627
20.367504	1217.038967	12.381632
20.617323	1217.186803	12.386637
20.517438	1226.822998	12.391642
20.504007	1223.844449	12.396647
20.544119	1221.125466	12.401651
20.784619	1231.694628	12.406656
20.801326	1222.511728	12.411661
20.663019	1229.941395	12.416666
20.413330	1228.565005	12.421671
20.579573	1223.401914	12.426675
20.348442	1233.366580	12.431680
20.252116	1228.978716	12.436685
20.383885	1221.792986	12.441690
20.319716	1232.803441	12.446695
20.464091	1222.546679	12.451699
20.229443	1229.209477	12.456704
20.088576	1229.421208	12.461709
20.877847	1232.225559	12.466714
20.167309	1226.240294	12.471719
20.742803	1222.480196	12.476723
20.546709	1231.149212	12.481728
20.556149	1229.277287	12.486733
20.627189	1227.788232	12.491738
20.624883	1233.849372	12.496743
20.655542	1233.122185	12.501747
20.860635	1233.217226	12.506752
20.683336	1230.671704	12.511757
20.819380	1224.406311	12.516762
20.385627	1224.469200	12.521767
20.711160	1214.711873	12.526771
20.205880	1213.403064	12.531776
20.336704	1207.649489	12.536781
20.617346	1222.749526	12.541786
20.267273	1231.665473	12.546791
20.403452	1230.128178	12.551795
20.725174	1234.776604	12.556800
20.660894	1228.691409	12.561805
20.407821	1222.577979	12.566810
20.377775	1232.444332	12.571815
20.826951	1231.412247	12.576819
20.418522	1232.562444	12.581824
20.346588	1224.510262	12.586829
20.658366	1229.428378	12.591834
20.695450	1233.764206	12.596839
20.513085	1229.028912	12.601843
20.232367	1220.412318	12.606848
20.504691	1220.987110	12.611853
20.628738	1223.034899	12.616858
20.743710	1235.133362	12.621863
20.602349	1221.294868	12.626867
20.558205	1225.392893	12.631872
20.596853	1218.726686	12.636877
20.436766	1215.997056	12.641882
20.439257	1216.023479	12.646887
20.323556	1216.330553	12.651891
20.482259	1221.358246	12.656896
20.760369	1211.933365	12.661901
20.636473	1213.558615	12.666906
20.443433	1218.833241	12.671911
20.896671	1207.946854	12.676915
20.595205	1220.900275	12.681920
20.688148	1228.149540	12.686925
20.970323	1219.966754	12.691930
20.497245	1221.655587	12.696935
20.676811	1216.036172	12.701939
20.464956	1218.990745	12.706944
20.468841	1215.670362	12.711949
20.772373	1219.518946	12.716954
20.536712	1219.084997	12.721959
20.683941	1219.301241	12.726963
20.629330	1225.694024	12.731968
20.496057	1218.097947	12.736973
20.921541	1227.068394	12.741978
20.243128	1211.867804	12.746983
20.509591	1208.992859	12.751987
20.466019	1223.322949	12.756992
20.631593	1224.105597	12.761997
20.734162	1213.071696	12.767002
20.192527	1197.792528	12.772007
20.523373	1205.879118	12.777011
20.532873	1216.248552	12.782016
20.727092	1214.321921	12.787021
20.512273	1188.474604	12.792026
20.174530	1198.437326	12.797031
20.718977	1207.191650	12.802035
20.516148	1210.034386	12.807040
20.765654	1205.723842	12.812045
20.483636	1195.375827	12.817050
20.339975	1193.654494	12.822055
20.512463	1192.592422	12.827059
20.081025	1195.313911	12.832064
20.362155	1215.840623	12.837069
20.452992	1218.882544	12.842074
20.068417	1228.285005	12.847079
20.245754	1232.207343	12.852083
20.322120	1238.678597	12.857088
20.344038	1235.164505	12.862093
20.447753	1231.025455	12.867098
20.539744	1229.851630	12.872103
20.862226	1222.252245	12.877107
20.759059	1230.695108	12.882112
20.662286	1222.052326	12.887117
20.616201	1224.158795	12.892122
20.452367	1235.738709	12.897127
20.363688	1224.695878	12.902131
20.432149	1230.813544	12.907136
20.482664	1238.227291	12.912141
20.410262	1238.283009	12.917146
20.453170	1237.492360	12.922151
20.820545	1229.693406	12.927155
20.759884	1242.786647	12.932160
20.700065	1234.874465	12.937165
20.832173	1234.574259	12.942170
20.486860	1221.479564	12.947175
20.285381	1205.013780	12.952179
20.199268	1219.678686	12.957184
20.257821	1228.477408	12.962189
20.467931	1233.299769	12.967194
20.515170	1241.978079	12.972199
20.745153	1235.187508	12.977203
20.708857	1239.725082	12.982208
20.405890	1238.922577	12.987213
20.362191	1226.315980	12.992218
20.266055	1246.302829	12.997223
20.669437	1235.736639	13.002227
20.844884	1249.922211	13.007232
20.603506	1238.419559	13.012237
20.753875	1232.645507	13.017242
20.298663	1231.928005	13.022247
20.517748	1219.454555	13.027251
20.468028	1229.533797	13.032256
20.311481	1237.472624	13.037261
20.650468	1238.156643	13.042266
20.604341	1248.958422	13.047271
21.017351	1234.904532	13.052275
20.509655	1228.623538	13.057280
20.433965	1215.164115	13.062285
20.635387	1208.489298	13.067290
20.440163	1207.208310	13.072295
20.386316	1209.976815	13.077299
20.211047	1212.988636	13.082304
19.879673	1210.836732	13.087309
20.348381	1230.764216	13.092314
20.123095	1247.904515	13.097319
20.627025	1248.994348	13.102323
20.543755	1253.184573	13.107328
20.660927	1249.619799	13.112333
20.769152	1243.579629	13.117338
20.737767	1253.008566	13.122343
20.733403	1247.390089	13.127347
20.456416	1233.119014	13.132352
20.378346	1233.129900	13.137357
20.393217	1229.195850	13.142362
20.342577	1248.068326	13.147367
20.459805	1245.650879	13.152371
20.457407	1250.618327	13.157376
20.476552	1259.937487	13.162381
20.856028	1249.834034	13.167386
20.563420	1260.462229	13.172391
20.709371	1242.886697	13.177395
20.377674	1239.989664	13.182400
20.511410	1244.619978	13.187405
20.626428	1223.356640	13.192410
20.370013	1226.006059	13.197415
20.578525	1220.919812	13.202419
20.451451	1218.727435	13.207424
20.411875	1218.371027	13.212429
20.847110	1223.663721	13.217434
20.177674	1229.389687	13.222439
20.711444	1229.657826	13.227443
20.277265	1224.200965	13.232448
20.316332	1236.628531	13.237453
20.618963	1244.308811	13.242458
20.315280	1254.455390	13.247463
20.736207	1244.434435	13.252467
20.371270	1254.907781	13.257472
20.351151	1253.431686	13.262477
20.624564	1254.823241	13.267482
20.369115	1252.309894	13.272487
20.907873	1252.421894	13.277491
20.603860	1251.970459	13.282496
20.511373	1236.831725	13.287501
20.666618	1224.903876	13.292506
20.373053	1217.254513	13.297511
20.443514	1205.544436	13.302515
20.671063	1216.006834	13.307520
20.427252	1225.454654	13.312525
20.935268	1220.353753	13.317530
20.784170	1223.733914	13.322535
20.448207	1218.668278	13.327539
20.333401	1221.318765	13.332544
20.603654	1223.799012	13.337549
20.687508	1217.691771	13.342554
20.545472	1229.537885	13.347559
20.753146	1220.789767	13.352563
20.355224	1224.518408	13.357568
20.216082	1223.348332	13.362573
20.504024	1218.755662	13.367578
20.646347	1220.240669	13.372583
20.736817	1216.441234	13.377587
20.759880	1222.290147	13.382592
20.527363	1223.257729	13.387597
20.908280	1218.367930	13.392602
20.493958	1224.748698	13.397607
20.712441	1216.886760	13.402611
20.656456	1226.594806	13.407616
20.420071	1228.490335	13.412621
20.649164	1221.814252	13.417626
20.442685	1228.955146	13.422631
20.836776	1226.301135	13.427635
20.712552	1214.858669	13.432640
20.322309	1208.185178	13.437645
20.526072	1193.031567	13.442650
20.357383	1202.103083	13.447655
20.407433	1208.986987	13.452659
20.425570	1222.301050	13.457664
20.644445	1231.107320	13.462669
20.522577	1219.793795	13.467674
20.570166	1226.709642	13.472679
20.640161	1221.871014	13.477683
20.344546	1222.260406	13.482688
20.347597	1222.669973	13.487693
20.665493	1229.416539	13.492698
20.244824	1233.084149	13.497703
20.781175	1223.277418	13.502707
20.660900	1228.046811	13.507712
20.123834	1213.244756	13.512717
20.778219	1223.126521	13.517722
20.496638	1226.913882	13.522727
20.535300	1204.196057	13.527731
20.613825	1213.560914	13.532736
20.372133	1206.234470	13.537741
20.718679	1191.767775	13.542746
20.492929	1204.677562	13.547751
20.452246	1199.831361	13.552755
20.456791	1195.512581	13.557760
19.982558	1196.488753	13.562765
20.695727	1202.386866	13.567770
20.554856	1232.197420	13.572775
20.726766	1222.147597	13.577779
20.525441	1214.079787	13.582784
20.407513	1211.594190	13.587789
20.904736	1201.883608	13.592794
20.510463	1213.646931	13.597799
20.594836	1205.520937	13.602803
20.737624	1203.835921	13.607808
20.434563	1201.941299	13.612813
20.597235	1189.858528	13.617818
20.641216	1198.539698	13.622823
20.529537	1196.452110	13.627827
20.397836	1202.503912	13.632832
20.463187	1201.003151	13.637837
20.689098	1197.915461	13.642842
20.354484	1209.303380	13.647847
20.642136	1206.384052	13.652851
20.539969	1205.913039	13.657856
20.250240	1199.851200	13.662861
20.553500	1197.945029	13.667866
20.454127	1196.940515	13.672871
20.758154	1207.438020	13.677875
20.688309	1207.318273	13.682880
20.573061	1208.170946	13.687885
20.774854	1203.399618	13.692890
20.564924	1199.737997	13.697895
20.711715	1206.784680	13.702899
20.805188	1194.735022	13.707904
20.662151	1193.300619	13.712909
20.619766	1195.966360	13.717914
20.712398	1201.222223	13.722919
20.699034	1191.976323	13.727923
20.717117	1169.611948	13.732928
20.629370	1174.420293	13.737933
20.896499	1160.672831	13.742938
20.307690	1174.944751	13.747943
20.326174	1169.234342	13.752947
20.611370	1160.172672	13.757952
20.737221	1168.118460	13.762957
20.443375	1165.826525	13.767962
20.686375	1171.373809	13.772967
20.424135	1165.586745	13.777971
20.354673	1168.586410	13.782976
20.176767	1173.126838	13.787981
20.495597	1164.892500	13.792986
20.363192	1168.312247	13.797991
20.472246	1175.812827	13.802995
20.466035	1172.994000	13.808000
20.446019	1166.430223	13.813005
20.667052	1173.200097	13.818010
20.437644	1179.321096	13.823015
20.394282	1172.369923	13.828019
20.310174	1170.432495	13.833024
20.441947	1196.532766	13.838029
20.735211	1192.510161	13.843034
20.534049	1180.496472	13.848039
20.194086	1174.094121	13.853043
20.640324	1184.911153	13.858048
20.518027	1191.511854	13.863053
20.641584	1177.038161	13.868058
20.286768	1190.673480	13.873063
20.445280	1193.524813	13.878067
20.792792	1194.857230	13.883072
20.244644	1190.680231	13.888077
20.734700	1180.731090	13.893082
20.533962	1182.871683	13.898087
20.623423	1180.600614	13.903091
20.724587	1176.627580	13.908096
20.374894	1176.334834	13.913101
20.486982	1165.674797	13.918106
20.402978	1173.444310	13.923111
20.194749	1170.905309	13.928115
20.733683	1181.846337	13.933120
20.384859	1179.004881	13.938125
20.656802	1164.127453	13.943130
20.451776	1171.533038	13.948135
20.817471	1171.209766	13.953139
20.876332	1174.610046	13.958144
20.635152	1176.372281	13.963149
20.656128	1169.352495	13.968154
20.505874	1180.086458	13.973159
20.324754	1170.999805	13.978163
20.693341	1171.228053	13.983168
20.588474	1168.683605	13.988173
20.503960	1166.128026	13.993178
20.412468	1172.911478	13.998183
20.386458	1168.029828	14.003187
20.452099	1174.721980	14.008192
20.412519	1170.046125	14.013210
20.757161	1167.000773	14.018227
20.244012	1175.882342	14.023245
20.292043	1178.235858	14.028263
20.198964	1177.921946	14.033280
20.183696	1174.098705	14.038298
20.424569	1195.444515	14.043315
20.507848	1208.349252	14.048333
20.677141	1212.695382	14.053351
20.813591	1215.146488	14.058368
20.603159	1214.296001	14.063386
20.836680	1211.114204	14.068403
20.500390	1225.075339	14.073421
20.413071	1214.804566	14.078439
20.603065	1216.073624	14.083456
20.492045	1223.264528	14.088474
20.897981	1219.595892	14.093491
20.517625	1220.377037	14.098509
20.613606	1216.496713	14.103527
20.611813	1220.544510	14.108544
20.582585	1218.192729	14.113562
21.065750	1220.508306	14.118579
20.654543	1217.603957	14.123597
20.655869	1218.155903	14.128615
21.336704	1230.919726	14.133632
20.927450	1233.665524	14.138650
20.682676	1223.352218	14.143667
20.943722	1242.423371	14.148685
20.796175	1244.688540	14.153703
21.140376	1248.464073	14.158720
21.383119	1252.219610	14.163738
21.175279	1237.601202	14.168755
21.092071	1237.089080	14.173773
20.693050	1231.711493	14.178791
21.279921	1239.250423	14.183808
20.868492	1262.510981	14.188826
21.315733	1257.759766	14.193843
21.218864	1254.578748	14.198861
21.203881	1256.471980	14.203879
21.312866	1251.338981	14.208896
21.129638	1257.237344	14.213914
21.107853	1258.367149	14.218931
20.771047	1260.810378	14.223949
21.201048	1253.891076	14.228967
21.046852	1249.010849	14.233984
21.140432	1254.918543	14.239002
21.086689	1255.271628	14.244019
21.236112	1256.517273	14.249037
21.303119	1257.178297	14.254055
21.367375	1260.778256	14.259072
20.930786	1259.432142	14.264090
21.447957	1252.044319	14.269107
21.176821	1270.601056	14.274125
21.512659	1283.358605	14.279143
21.599449	1284.795933	14.284160
21.418592	1288.331960	14.289178
21.461327	1286.409936	14.294195
21.916399	1287.017714	14.299213
21.607407	1282.982525	14.304231
21.367772	1255.039736	14.309248
21.340095	1274.937228	14.314266
21.490956	1275.234082	14.319283
21.750546	1281.753188	14.324301
21.565543	1287.881516	14.329319
21.789103	1286.264928	14.334336
21.654232	1297.612589	14.339354
21.850901	1293.690228	14.344371
21.887859	1294.374137	14.349389
21.753984	1291.912403	14.354407
21.871247	1284.077104	14.359424
21.624886	1284.773956	14.364442
22.062541	1274.871662	14.369459
21.923120	1268.513529	14.374477
21.726987	1268.135039	14.379495
21.872410	1255.761669	14.384512
21.888469	1264.739782	14.389530
22.032241	1269.628778	14.394547
21.967500	1259.584827	14.399565
21.957385	1255.332867	14.404583
21.786945	1249.234527	14.409600
21.539628	1267.369810	14.414618
22.021760	1284.785489	14.419635
21.916988	1292.345890	14.424653
21.800808	1296.283749	14.429671
22.181552	1288.972726	14.434688
22.007960	1296.260166	14.439706
21.902913	1287.018602	14.444723
21.951650	1279.693685	14.449741
22.229462	1280.745029	14.454759
22.255570	1283.107564	14.459776
21.934540	1292.392728	14.464794
22.259898	1290.282473	14.469811
22.190271	1292.562750	14.474829
21.955132	1287.325748	14.479847
22.234971	1286.536272	14.484864
22.098496	1288.013145	14.489882
22.155441	1285.471423	14.494899
22.224764	1297.385069	14.499917
22.132604	1299.366124	14.504935
22.460483	1287.287678	14.509952
22.216002	1291.284540	14.514970
22.391142	1285.546355	14.519987
22.322242	1285.493646	14.525005
21.980333	1295.663850	14.530023
22.510255	1292.330148	14.535040
22.534567	1299.873895	14.540058
22.530203	1312.737647	14.545075
22.666801	1301.436912	14.550093
22.243271	1298.747664	14.555111
22.415123	1306.599013	14.560128
22.154166	1313.420609	14.565146
22.188676	1309.203202	14.570163
22.269082	1305.553434	14.575181
22.142657	1305.332930	14.580199
22.507313	1295.341589	14.585216
22.397790	1306.409927	14.590234
22.281241	1303.526202	14.595251
22.348743	1321.887412	14.600269
22.766822	1331.809784	14.605287
22.958937	1332.332088	14.610304
23.052032	1336.516585	14.615322
22.914477	1321.179783	14.620339
22.702598	1312.677285	14.625357
22.485933	1312.656797	14.630375
22.674716	1326.836307	14.635392
22.607496	1337.768141	14.640410
22.982364	1341.824321	14.645427
23.009409	1352.606632	14.650445
23.070986	1345.507732	14.655463
22.958604	1342.458162	14.660480
23.067356	1345.060791	14.665498
23.183965	1336.988032	14.670515
23.083451	1315.956285	14.675533
22.685569	1317.453621	14.680551
22.871977	1326.620899	14.685568
22.881310	1337.181860	14.690586
23.063939	1336.086192	14.695603
23.522292	1335.419255	14.700621
23.065957	1346.760813	14.705639
23.072603	1342.942684	14.710656
23.488297	1340.491599	14.715674
23.029927	1334.006554	14.720691
23.436269	1333.425780	14.725709
23.355731	1331.327565	14.730727
22.991160	1310.640763	14.735744
23.228122	1312.090321	14.740762
22.948129	1339.141602	14.745779
23.190225	1336.503482	14.750797
23.066943	1343.819102	14.755815
23.427153	1344.257963	14.760832
23.237301	1345.427953	14.765850
23.191453	1347.347357	14.770867
23.348836	1341.456247	14.775885
23.443106	1346.320130	14.780903
23.315264	1339.635277	14.785920
23.354587	1340.425781	14.790938
23.059479	1341.179963	14.795955
23.215851	1333.129179	14.800973
23.072439	1341.424890	14.805991
23.251844	1352.594259	14.811008
23.286908	1358.608074	14.816026
23.234397	1376.772983	14.821043
23.526252	1370.080163	14.826061
23.359300	1377.144780	14.831079
23.452801	1365.954692	14.836096
23.837306	1366.482491	14.841114
23.734219	1369.029249	14.846131
23.843320	1372.333422	14.851149
23.801537	1373.012591	14.856167
23.978093	1360.211007	14.861184
24.029361	1366.273366	14.866202
23.945345	1368.212231	14.871219
24.031388	1352.333984	14.876237
24.138533	1361.062452	14.881255
23.889025	1356.681114	14.886272
23.866912	1349.698598	14.891290
23.734036	1340.799650	14.896307
24.226425	1340.226388	14.901325
23.810874	1350.039488	14.906343
24.019247	1340.688906	14.911360
23.837418	1335.853171	14.916378
23.712966	1347.400563	14.921395
24.231448	1350.341334	14.926413
24.262178	1366.611549	14.931431
23.692292	1350.739611	14.936448
24.057097	1351.597753	14.941466
24.089982	1363.372541	14.946483
24.278637	1356.839339	14.951501
24.362626	1360.063355	14.956519
24.258879	1354.998860	14.961536
24.366491	1343.339334	14.966554
23.603268	1349.805318	14.971571
24.286081	1342.376871	14.976589
24.090746	1362.923379	14.981607
24.248332	1369.025411	14.986624
24.299833	1357.513255	14.991642
24.039377	1364.799640	14.996659
24.152757	1365.311695	15.001677
24.143592	1360.849546	15.006695
24.343747	1356.571096	15.011712
24.400385	1360.647366	15.016730
24.230646	1369.471129	15.021747
24.650854	1355.266823	15.026765
24.667193	1367.511459	15.031783
24.387340	1363.596659	15.036800
24.575353	1360.497597	15.041818
24.611019	1360.678329	15.046835
24.896826	1361.925039	15.051853
24.607481	1367.472272	15.056871
24.410295	1368.683547	15.061888
24.434934	1363.431823	15.066906
24.253451	1375.291153	15.071923
24.432912	1360.548707	15.076941
24.577233	1369.528450	15.081959
24.296580	1366.826623	15.086976
24.581227	1375.980622	15.091994
24.672713	1391.214736	15.097011
25.116307	1392.008401	15.102029
24.865668	1381.958623	15.107047
24.753540	1376.062509	15.112064
25.069249	1367.673248	15.117082
24.653346	1366.945977	15.122099
24.801449	1368.965799	15.127117
24.904779	1387.166428	15.132135
24.742925	1388.962762	15.137152
25.040455	1385.976792	15.142170
24.946030	1393.847066	15.147187
25.015360	1399.602951	15.152205
24.842124	1402.654066	15.157223
24.865499	1404.239166	15.162240
25.506108	1404.185762	15.167258
25.081662	1401.639004	15.172275
25.180425	1384.939901	15.177293
25.186750	1376.686502	15.182311
25.093855	1377.319552	15.187328
25.074326	1372.570392	15.192346
25.034463	1392.480213	15.197363
25.243855	1390.199672	15.202381
25.169354	1397.401354	15.207399
24.991492	1390.242306	15.212416
25.079445	1391.150903	15.217434
24.998854	1395.280533	15.222451
25.562668	1398.423304	15.227469
25.178021	1389.695051	15.232487
25.137429	1398.410139	15.237504
25.107338	1386.294325	15.242522
25.195911	1394.873974	15.247539
25.226271	1387.104392	15.252557
25.216105	1392.768345	15.257575
25.252262	1393.435869	15.262592
25.455078	1394.969536	15.267610
25.557666	1406.913360	15.272627
25.396523	1419.931993	15.277645
25.816448	1419.692770	15.282663
25.581071	1411.116095	15.287680
25.921436	1408.421388	15.292698
25.660795	1403.684720	15.297715
25.351099	1376.102885	15.302733
25.520286	1394.149081	15.307751
25.509364	1413.259119	15.312768
25.937075	1412.292675	15.317786
25.881521	1420.306992	15.322803
25.992497	1417.083347	15.327821
25.894205	1413.591050	15.332839
25.557746	1413.028864	15.337856
25.993478	1412.209796	15.342874
26.035690	1413.544131	15.347891
26.001304	1409.165431	15.352909
25.946988	1398.083057	15.357927
25.782480	1386.680054	15.362944
25.785364	1391.021320	15.367962
25.870707	1408.185035	15.372979
25.946779	1407.414683	15.377997
26.374297	1411.663841	15.383015
26.049128	1412.443271	15.388032
26.262466	1409.106556	15.393050
26.104733	1407.115814	15.398067
25.823996	1410.686680	15.403085
25.896873	1409.838183	15.408103
25.689775	1412.535251	15.413120
25.968608	1404.671756	15.418138
26.028375	1421.226061	15.423155
25.937229	1419.208180	15.428173
26.044686	1413.936149	15.433191
26.333952	1414.866908	15.438208
26.440228	1418.763811	15.443226
26.325157	1414.865186	15.448243
26.226294	1418.387380	15.453261
26.612194	1415.584731	15.458279
26.470422	1421.390028	15.463296
26.619535	1405.894148	15.468314
26.363547	1421.164841	15.473331
26.197409	1425.759602	15.478349
26.307687	1423.592396	15.483367
26.205773	1418.209036	15.488384
26.569538	1415.733187	15.493402
26.271494	1418.465213	15.498419
26.273937	1424.703704	15.503437
26.982666	1434.609676	15.508455
26.498838	1453.148657	15.513472
26.945601	1449.151756	15.518490
26.833581	1438.168222	15.523507
26.811729	1418.488436	15.528525
27.039166	1418.390819	15.533543
26.870681	1410.550691	15.538560
26.982612	1412.030427	15.543578
26.603466	1406.031381	15.548595
26.759229	1423.510297	15.553613
26.887681	1414.718277	15.558631
26.711558	1424.600207	15.563648
27.040318	1409.974689	15.568666
27.034612	1417.491037	15.573683
26.728254	1410.677318	15.578701
26.966626	1414.922038	15.583719
26.675200	1418.694392	15.588736
26.894408	1427.374351	15.593754
26.964354	1442.038563	15.598771
27.226105	1444.071730	15.603789
27.221170	1443.039007	15.608807
27.175722	1451.730518	15.613824
27.305579	1440.811439	15.618842
26.974996	1426.420853	15.623859
26.874429	1442.365229	15.628877
27.217756	1440.108936	15.633895
27.316930	1459.687560	15.638912
27.132919	1444.621530	15.643930
27.355392	1445.895653	15.648947
27.298718	1450.686116	15.653965
27.171509	1443.035236	15.658983
27.097250	1446.179116	15.664000
27.310063	1444.869405	15.669018
27.629677	1450.253467	15.674035
27.211365	1450.704035	15.679053
27.662839	1445.721628	15.684071
27.067325	1448.976967	15.689088
27.265630	1440.128171	15.694106
27.471882	1446.299554	15.699123
27.353212	1438.011787	15.704141
27.497523	1435.943761	15.709159
27.154103	1441.001764	15.714176
27.349920	1444.533592	15.719194
27.509609	1456.064851	15.724211
27.510338	1468.592072	15.729229
27.633034	1470.982492	15.734247
27.650133	1463.626349	15.739264
27.635916	1471.739499	15.744282
27.992896	1467.248804	15.749299
27.923108	1468.538872	15.754317
27.904079	1469.181380	15.759335
28.177067	1472.640342	15.764352
28.026251	1460.167753	15.769370
27.887887	1453.427895	15.774387
27.761154	1459.815999	15.779405
28.275663	1461.420298	15.784423
27.975433	1463.768059	15.789440
27.971489	1451.395539	15.794458
27.755562	1451.474038	15.799475
27.968231	1467.604442	15.804493
28.338332	1459.226116	15.809511
28.036841	1472.093355	15.814528
27.891615	1464.681302	15.819546
28.150415	1461.346762	15.824563
28.039925	1470.184732	15.829581
28.393465	1462.299065	15.834599
28.321919	1466.251086	15.839616
28.198934	1465.729569	15.844634
28.579446	1467.409515	15.849651
28.067266	1472.316686	15.854669
28.409191	1459.888204	15.859687
27.984803	1473.231244	15.864704
28.468917	1469.228379	15.869722
28.261528	1469.900146	15.874739
28.487333	1477.199479	15.879757
28.334951	1463.408097	15.884775
28.613990	1471.230641	15.889792
28.360873	1467.385483	15.894810
28.294500	1473.339229	15.899827
28.235987	1472.305612	15.904845
28.581752	1471.280659	15.909863
28.443799	1468.836849	15.914880
28.505079	1470.801318	15.919898
28.653542	1456.293391	15.924915
28.229028	1469.826006	15.929933
28.636442	1470.104753	15.934951
28.890920	1494.233209	15.939968
28.901331	1488.400092	15.944986
28.587302	1472.291358	15.950003
28.744739	1482.317546	15.955021
28.739906	1488.511605	15.960039
28.650897	1495.552048	15.965056
28.696896	1488.689954	15.970074
29.159594	1498.689486	15.975091
29.163616	1487.777072	15.980109
29.242833	1487.165097	15.985127
29.382405	1487.359146	15.990144
29.116335	1467.465766	15.995162
29.171322	1461.745890	16.000179
28.858269	1460.148019	16.005197
29.225840	1458.067977	16.010215
29.540482	1459.920456	16.015232
29.324336	1456.637290	16.020250
29.468617	1452.156931	16.025267
29.057862	1460.828061	16.030285
29.089798	1459.282133	16.035303
29.004778	1455.359041	16.040320
28.968575	1457.421644	16.045338
29.136341	1461.639100	16.050355
28.921001	1469.435889	16.055373
29.258406	1488.459791	16.060391
29.176452	1499.570283	16.065408
29.396326	1492.488536	16.070426
29.734836	1495.080501	16.075443
29.688183	1494.524785	16.080461
29.651763	1490.766185	16.085479
29.705525	1502.893276	16.090496
29.625408	1496.459513	16.095514
29.731069	1487.763111	16.100531
29.372070	1483.207281	16.105549
29.612582	1482.986450	16.110567
29.560272	1493.463758	16.115584
29.739963	1496.833783	16.120602
29.831802	1494.318707	16.125619
29.666589	1496.276046	16.130637
29.737822	1494.231467	16.135655
29.534345	1492.661735	16.140672
29.419085	1496.424886	16.145690
29.795121	1492.590272	16.150707
29.778864	1507.483815	16.155725
29.583375	1501.191940	16.160743
29.650811	1502.440459	16.165760
29.605706	1505.690605	16.170778
29.734334	1491.715941	16.175795
29.612411	1496.963586	16.180813
29.950183	1516.665471	16.185831
30.155509	1519.326664	16.190848
29.886968	1521.624546	16.195866
30.413264	1517.683371	16.200883
30.158198	1527.855614	16.205901
30.335116	1519.438064	16.210919
30.202626	1521.015790	16.215936
30.180257	1532.868745	16.220954
30.373182	1524.798654	16.225971
30.517189	1525.655058	16.230989
30.131278	1528.660680	16.236007
30.579368	1526.360922	16.241024
30.442351	1516.345626	16.246042
30.201980	1498.103004	16.251059
30.291876	1514.523617	16.256077
30.323558	1514.593296	16.261095
30.387915	1520.507333	16.266112
30.291946	1522.100470	16.271130
30.489053	1521.225860	16.276147
30.784759	1528.403166	16.281165
30.698827	1527.089973	16.286183
30.735364	1530.873754	16.291200
30.527765	1531.857817	16.296218
30.722450	1519.892452	16.301235
30.932253	1523.152282	16.306253
30.609227	1514.518735	16.311271
30.453210	1525.911634	16.316288
30.469022	1529.116674	16.321306
30.752349	1526.759822	16.326323
30.844443	1526.318833	16.331341
30.856903	1525.992011	16.336359
30.891462	1520.474368	16.341376
30.495897	1522.113719	16.346394
30.676176	1515.984495	16.351411
30.731513	1525.725750	16.356429
30.740072	1517.779456	16.361447
30.951662	1512.181667	16.366464
30.735644	1527.151138	16.371482
31.160986	1538.408844	16.376499
30.945301	1550.413778	16.381517
30.893523	1558.854666	16.386535
31.476324	1555.409435	16.391552
31.307721	1552.659025	16.396570
31.571135	1549.724871	16.401587
31.313598	1562.407417	16.406605
31.314507	1550.060782	16.411623
31.470156	1536.968995	16.416640
31.247615	1535.990638	16.421658
31.275054	1543.718852	16.426675
31.474473	1549.183474	16.431693
31.177157	1554.485071	16.436711
31.703624	1542.912741	16.441728
31.507298	1555.104936	16.446746
31.735249	1545.630758	16.451763
31.517543	1547.164660	16.456781
31.674756	1555.075111	16.461799
31.767962	1541.880803	16.466816
31.364151	1530.179999	16.471834
31.725791	1540.786379	16.476851
31.669743	1542.164715	16.481869
31.818907	1545.050385	16.486887
31.806439	1546.821338	16.491904
31.745326	1552.184365	16.496922
31.995622	1530.995672	16.501939
32.169656	1518.341438	16.506957
31.410810	1511.957723	16.511975
31.655276	1521.741957	16.516992
31.868101	1535.186345	16.522010
32.081588	1531.636424	16.527027
32.118729	1540.656178	16.532045
32.108223	1536.994898	16.537063
32.002715	1522.289090	16.542080
31.691613	1528.795512	16.547098
31.883517	1534.577520	16.552115
31.735086	1539.393659	16.557133
31.871739	1551.394306	16.562151
32.232906	1540.579050	16.567168
31.989155	1549.591701	16.572186
31.997185	1539.986642	16.577203
32.145069	1539.891489	16.582221
31.992473	1537.488544	16.587239
32.049469	1536.106146	16.592256
32.262867	1556.063889	16.597274
32.360548	1557.000833	16.602291
32.374796	1560.114889	16.607309
32.140605	1570.634634	16.612327
32.563722	1560.669971	16.617344
32.447055	1567.791942	16.622362
32.675525	1559.993029	16.627379
32.815551	1574.265505	16.632397
32.480924	1567.211602	16.637415
32.888135	1567.817591	16.642432
32.603574	1564.859933	16.647450
32.837978	1564.061173	16.652467
32.912292	1562.271723	16.657485
32.600221	1555.483229	16.662503
32.997837	1548.487154	16.667520
32.871568	1548.014924	16.672538
32.416651	1538.708661	16.677555
32.611433	1551.200283	16.682573
32.844967	1568.942263	16.687591
33.033031	1564.552418	16.692608
32.586685	1570.550293	16.697626
32.927452	1567.275805	16.702643
33.014601	1564.489319	16.707661
32.799245	1569.840773	16.712679
32.904896	1562.392587	16.717696
32.876075	1568.030481	16.722714
32.663637	1560.350660	16.727731
32.858467	1566.620663	16.732749
32.747938	1579.201907	16.737767
32.980299	1588.878787	16.742784
32.869486	1593.279936	16.747802
33.108137	1599.579145	16.752819
33.274478	1599.812187	16.757837
33.084723	1598.355877	16.762855
33.253833	1603.003405	16.767872
33.025430	1602.291047	16.772890
33.202509	1599.785167	16.777907
33.452851	1590.831234	16.782925
33.493728	1601.572983	16.787943
33.532429	1594.699418	16.792960
33.579974	1601.486884	16.797978
33.719206	1596.053196	16.802995
33.940691	1596.380481	16.808013
33.563076	1594.180953	16.813031
33.689724	1593.052509	16.818048
33.463647	1594.965296	16.823066
33.632699	1592.321479	16.828083
33.572623	1602.262887	16.833101
33.326127	1614.202784	16.838119
33.835445	1617.554082	16.843136
33.933367	1621.818907	16.848154
34.057049	1622.724179	16.853171
33.904604	1622.548720	16.858189
33.922543	1627.452402	16.863207
34.163308	1618.249855	16.868224
34.230664	1615.932943	16.873242
34.135049	1618.215842	16.878259
34.283562	1619.631560	16.883277
33.931955	1627.229145	16.888295
33.954957	1615.849539	16.893312
33.964925	1631.599517	16.898330
33.979698	1627.768218	16.903347
34.231750	1619.916745	16.908365
34.091236	1626.265432	16.913383
34.315898	1616.859377	16.918400
34.119356	1620.762947	16.923418
34.185874	1617.256111	16.928435
34.377150	1616.614459	16.933453
33.948278	1625.650391	16.938471
34.286213	1611.910443	16.943488
33.963602	1619.855775	16.948506
34.630260	1643.136114	16.953523
34.950838	1637.245599	16.958541
34.764730	1640.099817	16.963559
34.805265	1627.987481	16.968576
34.624617	1627.489313	16.973594
34.526420	1620.153054	16.978611
34.550068	1616.406864	16.983629
34.470383	1633.915722	16.988647
34.737278	1642.937435	16.993664
34.901843	1647.095678	16.998682
34.855996	1657.618480	17.003699
35.161044	1653.117135	17.008717
34.934208	1653.714928	17.013735
35.330780	1650.772100	17.018752
34.788049	1630.584405	17.023770
35.067919	1640.859389	17.028787
35.064589	1636.165764	17.033805
35.208817	1641.615628	17.038823
35.219651	1635.142127	17.043840
34.919223	1635.305680	17.048858
34.725488	1639.875807	17.053875
35.272555	1647.544792	17.058893
34.977102	1654.932076	17.063911
34.928179	1654.124230	17.068928
35.018407	1646.675315	17.073946
35.156504	1660.184438	17.078963
35.125664	1651.659156	17.083981
34.727051	1651.747130	17.088999
35.257625	1649.964337	17.094016
35.370812	1654.472142	17.099034
35.359502	1671.709789	17.104051
35.640731	1673.778425	17.109069
35.435863	1682.913164	17.114087
35.296336	1682.843402	17.119104
35.337558	1683.221465	17.124122
35.204457	1683.257650	17.129139
35.606838	1682.583898	17.134157
35.652619	1680.975960	17.139175
35.636102	1680.269916	17.144192
35.654222	1682.438724	17.149210
35.540543	1683.798735	17.154227
35.833621	1675.295711	17.159245
35.972709	1681.153060	17.164263
35.983460	1679.726899	17.169280
36.026305	1682.565844	17.174298
35.659632	1683.460451	17.179315
35.766763	1673.774213	17.184333
35.995326	1683.063989	17.189351
36.328070	1691.958819	17.194368
36.211217	1688.285360	17.199386
35.793919	1693.307252	17.204403
36.378152	1693.875573	17.209421
36.422158	1693.727770	17.214439
36.264916	1689.744557	17.219456
36.365327	1673.018905	17.224474
35.797381	1678.727888	17.229491
36.225797	1700.116105	17.234509
36.509414	1709.639377	17.239527
36.747352	1709.647843	17.244544
36.676138	1713.090974	17.249562
36.176387	1697.888627	17.254579
36.732854	1687.635178	17.259597
36.596502	1693.823559	17.264615
36.462617	1696.275392	17.269632
36.831045	1695.386818	17.274650
36.772587	1695.493686	17.279667
36.590302	1682.711301	17.284685
36.732709	1683.542014	17.289703
36.846812	1698.965550	17.294720
36.917399	1681.914290	17.299738
36.380920	1684.226617	17.304755
36.943074	1689.958284	17.309773
37.093231	1698.729649	17.314791
36.465215	1706.882626	17.319808
37.296664	1699.456252	17.324826
37.281375	1690.739693	17.329843
37.072468	1686.309303	17.334861
36.999057	1682.010682	17.339879
36.723069	1693.111370	17.344896
37.305350	1697.873149	17.349914
37.011033	1704.761598	17.354931
37.434344	1704.368455	17.359949
37.458354	1700.073167	17.364967
37.131942	1690.394717	17.369984
37.409009	1690.163334	17.375002
37.192817	1683.239929	17.380019
37.437285	1689.347903	17.385037
37.429748	1702.099241	17.390055
37.346188	1695.954606	17.395072
37.296289	1695.393107	17.400090
37.028854	1702.145125	17.405107
37.459804	1693.867079	17.410125
37.324299	1700.002628	17.415143
37.491857	1707.010902	17.420160
37.473520	1691.841893	17.425178
37.296263	1704.650979	17.430195
37.665112	1704.359336	17.435213
37.309483	1700.815201	17.440231
37.385477	1700.174629	17.445248
37.953758	1704.010504	17.450266
37.568088	1729.990766	17.455283
37.529732	1718.089938	17.460301
37.721790	1732.261456	17.465319
37.554965	1724.345383	17.470336
38.090109	1724.265544	17.475354
37.927575	1725.837071	17.480371
37.722261	1727.033153	17.485389
37.828724	1735.581833	17.490407
37.743851	1730.196425	17.495424
38.440047	1734.582949	17.500442
38.037227	1744.722277	17.505459
38.371556	1737.689800	17.510477
38.332884	1741.031000	17.515495
38.294950	1738.331289	17.520512
38.262160	1742.600480	17.525530
38.347654	1749.708386	17.530547
38.537964	1745.618596	17.535565
38.307388	1756.795464	17.540583
38.530844	1757.838210	17.545600
38.609412	1742.227376	17.550618
38.434921	1763.145525	17.555635
38.251187	1757.475408	17.560653
38.589065	1754.909247	17.565671
38.705696	1749.283253	17.570688
38.756006	1746.963533	17.575706
38.588944	1757.855761	17.580723
39.094461	1743.626461	17.585741
38.971475	1752.932240	17.590759
38.668748	1756.565687	17.595776
38.989355	1750.646019	17.600794
39.022783	1755.455246	17.605811
38.819287	1756.352933	17.610829
39.258120	1753.361657	17.615847
38.679508	1759.221819	17.620864
38.917627	1749.120571	17.625882
38.762481	1754.259555	17.630899
39.142516	1755.477114	17.635917
39.051698	1748.027134	17.640935
39.073408	1755.827166	17.645952
39.558468	1746.763336	17.650970
39.115063	1754.422822	17.655987
38.990173	1749.392237	17.661005
39.318642	1745.093208	17.666023
38.992880	1751.643754	17.671040
39.291815	1746.578605	17.676058
39.316344	1759.950195	17.681075
39.243959	1765.164864	17.686093
39.509720	1770.999685	17.691111
39.379580	1781.303198	17.696128
39.652719	1772.270008	17.701146
39.284108	1774.854467	17.706163
39.351571	1769.919831	17.711181
39.309484	1769.821942	17.716199
39.458145	1773.482503	17.721216
39.630928	1779.959836	17.726234
39.650230	1776.648481	17.731251
39.551154	1770.638432	17.736269
39.972774	1790.041007	17.741287
39.927741	1815.319746	17.746304
40.095609	1810.792254	17.751322
40.126905	1808.989971	17.756339
40.193893	1801.084544	17.761357
40.243549	1786.226297	17.766375
40.003583	1785.791857	17.771392
39.985308	1787.750967	17.776410
40.173473	1796.755445	17.781427
40.254467	1797.151550	17.786445
40.323204	1797.666809	17.791463
40.334208	1815.539758	17.796480
40.080536	1802.658535	17.801498
40.250102	1820.162470	17.806515
40.443681	1813.583445	17.811533
40.230250	1812.309440	17.816551
40.279934	1807.249417	17.821568
40.252460	1807.153916	17.826586
40.311917	1809.428628	17.831603
40.447789	1801.715147	17.836621
40.591459	1803.098621	17.841639
40.610598	1806.184420	17.846656
40.456525	1803.544122	17.851674
40.812395	1815.550138	17.856691
40.943422	1823.788978	17.861709
40.914284	1807.761855	17.866727
40.859675	1805.724720	17.871744
40.873870	1807.689665	17.876762
40.680710	1824.907732	17.881779
40.722522	1829.315284	17.886797
41.368315	1830.134933	17.891815
40.836266	1835.547221	17.896832
41.051065	1822.651824	17.901850
41.145707	1823.282510	17.906867
40.959865	1825.721415	17.911885
41.321177	1817.181469	17.916903
41.343703	1826.207664	17.921920
41.519194	1819.973678	17.926938
41.681195	1834.180767	17.931955
41.418947	1820.758164	17.936973
41.796446	1814.759392	17.941991
41.321613	1810.977821	17.947008
41.644592	1796.554200	17.952026
41.554845	1792.398947	17.957043
41.325576	1786.825749	17.962061
41.697299	1801.877948	17.967079
41.555320	1804.284683	17.972096
41.725350	1819.855954	17.977114
41.530515	1823.617723	17.982131
41.642160	1829.241180	17.987149
41.668727	1822.302585	17.992167
41.823016	1826.051144	17.997184
41.858611	1820.197359	18.002202
41.736873	1817.766634	18.007219
41.445776	1828.373511	18.012237
41.742785	1822.544100	18.017255
41.903083	1825.799311	18.022272
41.828991	1817.606469	18.027290
41.772599	1824.420057	18.032307
41.565627	1834.269428	18.037325
42.263155	1839.129286	18.042343
42.045789	1857.344686	18.047360
42.408672	1851.349803	18.052378
42.272280	1844.059638	18.057395
42.324957	1849.226860	18.062413
42.572668	1849.206238	18.067431
42.363510	1851.293337	18.072448
42.621900	1853.544980	18.077466
42.231546	1849.697224	18.082483
42.265087	1853.105588	18.087501
42.598455	1851.237029	18.092519
42.464653	1851.093202	18.097536
42.250252	1845.132192	18.102554
42.856067	1843.797519	18.107571
42.543600	1849.874834	18.112589
42.432741	1845.722146	18.117607
42.675716	1852.877348	18.122624
43.062945	1867.814663	18.127642
43.046478	1859.651935	18.132659
42.743480	1866.142267	18.137677
43.081661	1863.133988	18.142695
43.023139	1874.405421	18.147712
43.020591	1868.525451	18.152730
43.308501	1872.797016	18.157747
43.333580	1873.035289	18.162765
43.067416	1850.779332	18.167783
43.017192	1843.326762	18.172800
43.268702	1862.154842	18.177818
43.524346	1867.339251	18.182835
43.090928	1872.147467	18.187853
43.276986	1862.208613	18.192871
43.314719	1872.797682	18.197888
43.596774	1878.560730	18.202906
43.607677	1875.674654	18.207923
43.458984	1878.407324	18.212941
43.996541	1869.788110	18.217959
43.070638	1878.996287	18.222976
43.356477	1875.334850	18.227994
43.475752	1879.240029	18.233011
43.303252	1893.442321	18.238029
43.895312	1895.733566	18.243047
43.795594	1889.461642	18.248064
43.737315	1895.443373	18.253082
43.943391	1901.921743	18.258099
43.874298	1892.304369	18.263117
44.129472	1893.281502	18.268135
44.101875	1894.600272	18.273152
44.149798	1893.441101	18.278170
44.002007	1889.885792	18.283187
44.149541	1891.573060	18.288205
44.291708	1889.089219	18.293223
44.190718	1887.204198	18.298240
43.865595	1892.769133	18.303258
44.720674	1897.586577	18.308275
44.497537	1901.166463	18.313293
44.539919	1891.181287	18.318311
44.621513	1885.751965	18.323328
44.871590	1889.533244	18.328346
44.736522	1877.771989	18.333363
44.523902	1891.249956	18.338381
44.674028	1880.399680	18.343399
44.819543	1886.375645	18.348416
44.490631	1896.449016	18.353434
44.805855	1882.713223	18.358451
44.811190	1884.572619	18.363469
45.038142	1885.256929	18.368487
44.876205	1887.143005	18.373504
44.776853	1890.156479	18.378522
44.961560	1893.339381	18.383539
44.859496	1889.389785	18.388557
45.021568	1896.113502	18.393575
45.100511	1897.162004	18.398592
44.713169	1892.429651	18.403610
44.958006	1899.229837	18.408627
44.571410	1919.201974	18.413645
45.048292	1922.559307	18.418663
45.039613	1927.198327	18.423680
44.749343	1929.160724	18.428698
45.023546	1920.990929	18.433715
44.796413	1930.624914	18.438733
45.102374	1938.307341	18.443751
45.303418	1953.643343	18.448768
45.460423	1963.124051	18.453786
45.744323	1953.797215	18.458803
45.196734	1953.204965	18.463821
45.400819	1945.481315	18.468839
45.932185	1951.173952	18.473856
45.615681	1951.055331	18.478874
45.974678	1952.192887	18.483891
45.736833	1947.300594	18.488909
45.914351	1947.845703	18.493927
45.975582	1943.745769	18.498944
45.833794	1954.466572	18.503962
46.232937	1942.756137	18.508979
45.959993	1949.217328	18.513997
45.892776	1939.214990	18.519015
46.123403	1947.866697	18.524032
46.125789	1939.431909	18.529050
46.356767	1938.939654	18.534067
46.097513	1954.182320	18.539085
46.021049	1953.269516	18.544103
46.211683	1970.848931	18.549120
46.115286	1979.225601	18.554138
46.970535	1981.348244	18.559155
46.674383	1979.913583	18.564173
46.849577	1970.449906	18.569191
46.577524	1958.334452	18.574208
46.494346	1971.286081	18.579226
46.946983	1965.871487	18.584243
46.801358	1961.489912	18.589261
46.675031	1948.783317	18.594279
46.871914	1954.436488	18.599296
46.712807	1968.022404	18.604314
47.166891	1964.106003	18.609331
47.004164	1957.343052	18.614349
46.706783	1971.301837	18.619367
47.024024	1965.590276	18.624384
46.829859	1970.785900	18.629402
47.263937	1965.198074	18.634419
47.125123	1971.410562	18.639437
46.814980	1970.259727	18.644455
47.194484	1963.705254	18.649472
46.901151	1976.452075	18.654490
47.031496	1972.201099	18.659507
46.919733	1965.722622	18.664525
46.865231	1969.669701	18.669543
47.507208	1981.236934	18.674560
47.604907	1992.006091	18.679578
47.755243	1991.912905	18.684595
47.777825	1991.014978	18.689613
47.911422	1986.758760	18.694631
47.508975	1975.375940	18.699648
47.599674	1980.758958	18.704666
47.673402	1984.790203	18.709683
47.817743	1992.550352	18.714701
47.743154	1991.254971	18.719719
47.588086	1988.879087	18.724736
47.554595	1996.667602	18.729754
47.980897	1989.332450	18.734771
47.728804	1996.179690	18.739789
47.762052	1988.962290	18.744807
47.885694	1988.718406	18.749824
47.707550	1996.701466	18.754842
48.099556	2011.806495	18.759859
48.553316	2016.999475	18.764877
48.338488	2026.434129	18.769895
48.800137	2022.137377	18.774912
48.664133	2009.326871	18.779930
48.658759	1995.426585	18.784947
48.341390	1991.686709	18.789965
48.546497	1993.493805	18.794983
48.519008	1989.727359	18.800000
48.500992	1991.291595	18.805018
48.524464	2000.116384	18.810035
48.734127	2006.091607	18.815053
48.564782	2022.886076	18.820071
48.701237	2011.839666	18.825088
48.567557	2020.112972	18.830106
49.142356	2014.147937	18.835123
48.945334	2017.516030	18.840141
48.824094	2021.702661	18.845159
49.311388	2016.688395	18.850176
49.378373	2018.635511	18.855194
49.257238	2012.820804	18.860211
49.212484	2024.141285	18.865229
49.269029	2018.532637	18.870247
49.404806	2012.205794	18.875264
48.855117	2025.846194	18.880282
49.268588	2017.044536	18.885299
49.330717	2012.816228	18.890317
49.231634	2020.338342	18.895335
49.118227	2016.348046	18.900352
49.020135	2026.059047	18.905370
49.391736	2027.797117	18.910387
49.604245	2046.686718	18.915405
49.692122	2042.814548	18.920423
50.134394	2040.817689	18.925440
49.588542	2042.488142	18.930458
49.589845	2040.615103	18.935475
50.085477	2040.193901	18.940493
49.741560	2038.537172	18.945511
49.820784	2029.321590	18.950528
49.846466	2036.029369	18.955546
49.758802	2036.091343	18.960563
49.981469	2037.129518	18.965581
49.886350	2048.485580	18.970599
49.933738	2040.759343	18.975616
50.128293	2064.707954	18.980634
49.956133	2071.001314	18.985651
50.076245	2069.958041	18.990669
50.238406	2064.255445	18.995687
50.463075	2065.952456	19.000704
50.560474	2069.797463	19.005722
50.558371	2066.933087	19.010739
50.497007	2065.283203	19.015757
50.348800	2062.347741	19.020775
50.791658	2060.697668	19.025792
50.406847	2069.328047	19.030810
50.791133	2062.925364	19.035827
50.868108	2064.501201	19.040845
50.605711	2067.269346	19.045863
50.888015	2064.066215	19.050880
50.673299	2068.404634	19.055898
50.888577	2086.792008	19.060915
51.192847	2090.906859	19.065933
51.354608	2090.732405	19.070951
51.570522	2088.474316	19.075968
51.243831	2069.322871	19.080986
51.046891	2067.640336	19.086003
51.379381	2069.595453	19.091021
50.944251	2092.953926	19.096039
51.138678	2081.422336	19.101056
51.425483	2088.625726	19.106074
51.599481	2087.134158	19.111091
51.352178	2090.405672	19.116109
51.203802	2084.033663	19.121127
51.260810	2092.487399	19.126144
51.552436	2096.077260	19.131162
51.466580	2104.470412	19.136179
51.819219	2112.806216	19.141197
51.658370	2126.563244	19.146215
52.009419	2120.084034	19.151232
52.131383	2121.158727	19.156250
52.118738	2120.735214	19.161267
52.201818	2119.212523	19.166285
51.769051	2125.452295	19.171303
52.613556	2113.153907	19.176320
51.983705	2119.054630	19.181338
52.192375	2120.392372	19.186355
52.663986	2112.093449	19.191373
52.509051	2120.578646	19.196391
52.464737	2118.928396	19.201408
52.539224	2113.202796	19.206426
52.291044	2109.187561	19.211443
52.437230	2116.621051	19.216461
52.579596	2116.309679	19.221479
52.746941	2110.139009	19.226496
52.777513	2124.200589	19.231514
52.503088	2111.970543	19.236531
52.705967	2111.010816	19.241549
52.585434	2111.661676	19.246567
52.853040	2111.051880	19.251584
53.037522	2112.131547	19.256602
52.818113	2116.194637	19.261619
52.962050	2108.581178	19.266637
52.546979	2112.610974	19.271655
52.732833	2110.382847	19.276672
53.014908	2124.757489	19.281690
52.915546	2138.850032	19.286707
53.388322	2130.019183	19.291725
53.031508	2136.817905	19.296743
53.220480	2136.016924	19.301760
53.395758	2136.280015	19.306778
53.424060	2132.867248	19.311795
53.599503	2132.882538	19.316813
53.160126	2135.597905	19.321831
53.140617	2125.890665	19.326848
53.631612	2141.127918	19.331866
53.521972	2156.028365	19.336883
53.813529	2152.348643	19.341901
53.711838	2151.515362	19.346919
53.665159	2153.447588	19.351936
53.957497	2154.735806	19.356954
54.109773	2144.333344	19.361971
54.415492	2142.572202	19.366989
53.906473	2142.540131	19.372007
54.617685	2141.528429	19.377024
54.770707	2133.686971	19.382042
54.650074	2140.636805	19.387059
54.639028	2118.106132	19.392077
54.260079	2106.766654	19.397095
54.219770	2100.277506	19.402112
54.485423	2105.091499	19.407130
54.571835	2120.667777	19.412147
54.699788	2127.434799	19.417165
54.644883	2134.448873	19.422183
54.926079	2124.325551	19.427200
55.028981	2119.839003	19.432218
54.658228	2113.302657	19.437235
54.928844	2094.604945	19.442253
54.867453	2106.524371	19.447271
54.749057	2121.157955	19.452288
54.713572	2120.892254	19.457306
54.636669	2132.940029	19.462323
55.317574	2120.031383	19.467341
55.295331	2126.768872	19.472359
55.062004	2117.465433	19.477376
55.172071	2132.878276	19.482394
55.040356	2128.322956	19.487411
55.055338	2122.947433	19.492429
55.023827	2131.424749	19.497447
55.139674	2125.778285	19.502464
55.650227	2140.919603	19.507482
55.566656	2147.076159	19.512499
55.993796	2148.352315	19.517517
55.439985	2152.202885	19.522535
55.614298	2150.243244	19.527552
55.896302	2149.971741	19.532570
55.713482	2150.259696	19.537587
55.948889	2151.695433	19.542605
55.642036	2155.371323	19.547623
55.671657	2154.882073	19.552640
55.808272	2152.217373	19.557658
56.085445	2158.036373	19.562675
56.259805	2154.775714	19.567693
55.843831	2154.006718	19.572711
55.867265	2148.127997	19.577728
56.265520	2145.189525	19.582746
56.323686	2150.661960	19.587763
56.251064	2138.999082	19.592781
56.182994	2153.655348	19.597799
56.216748	2176.431823	19.602816
56.411221	2180.836371	19.607834
56.635265	2190.876811	19.612851
56.754730	2180.981398	19.617869
56.606815	2189.895777	19.622887
56.697043	2182.468614	19.627904
56.463762	2185.393387	19.632922
56.517648	2192.431039	19.637939
56.642684	2177.782974	19.642957
56.981370	2181.444796	19.647975
56.769264	2202.729044	19.652992
57.087077	2207.259446	19.658010
57.047611	2210.563910	19.663027
57.171770	2200.937535	19.668045
57.283177	2202.020998	19.673063
57.172337	2208.893790	19.678080
57.506771	2204.236568	19.683098
57.164638	2207.228262	19.688115
57.089743	2203.928687	19.693133
57.278480	2209.644612	19.698151
57.481219	2200.295955	19.703168
57.675120	2205.568993	19.708186
57.658135	2219.103371	19.713203
58.051850	2214.439837	19.718221
58.027634	2202.020357	19.723239
58.011530	2198.224510	19.728256
58.180500	2188.370752	19.733274
58.140383	2197.581791	19.738291
57.909599	2191.800232	19.743309
58.106771	2187.196372	19.748327
58.410641	2190.712724	19.753344
58.226631	2185.416897	19.758362
58.274916	2194.789244	19.763379
58.079687	2190.499675	19.768397
58.290794	2204.152617	19.773415
58.470677	2218.364310	19.778432
58.600169	2224.036202	19.783450
58.391222	2238.069233	19.788467
58.426501	2232.698297	19.793485
58.339153	2223.660972	19.798503
58.297156	2239.411242	19.803520
58.620344	2230.883431	19.808538
58.411267	2240.192238	19.813555
58.853232	2220.249398	19.818573
58.440283	2232.109369	19.823591
58.486021	2250.262843	19.828608
59.064628	2248.433782	19.833626
58.815149	2259.901939	19.838643
58.933139	2259.625130	19.843661
59.336486	2256.367256	19.848679
59.036284	2254.875004	19.853696
59.437623	2257.121218	19.858714
59.379269	2264.436381	19.863731
59.534593	2255.576644	19.868749
59.401140	2254.878210	19.873767
59.401855	2261.277799	19.878784
59.532699	2252.598950	19.883802
59.320487	2258.042969	19.888819
59.761653	2257.771250	19.893837
60.018437	2271.118853	19.898855
59.986319	2260.828310	19.903872
60.312080	2252.098709	19.908890
59.839977	2251.462153	19.913907
60.123298	2238.136210	19.918925
59.957876	2236.661794	19.923943
60.007469	2242.822322	19.928960
60.376896	2244.211522	19.933978
60.318115	2250.943884	19.938995
60.259565	2242.562689	19.944013
60.285219	2246.854170	19.949031
60.052488	2266.162741	19.954048
60.332486	2264.023405	19.959066
60.395091	2266.464445	19.964083
60.567056	2255.767726	19.969101
60.690255	2254.983523	19.974119
60.841281	2260.018003	19.979136
60.809031	2253.618746	19.984154
60.824394	2251.358795	19.989171
60.650255	2259.398779	19.994189
60.545175	2261.230998	19.999207
60.614596	2259.496519	20.004224
61.004598	2250.629246	20.009242
61.081576	2273.124459	20.014259
61.261387	2276.378233	20.019277
61.609646	2282.777463	20.024295
61.045127	2285.592261	20.029312
61.392998	2272.893917	20.034330
61.400980	2280.585510	20.039347
61.383629	2282.370703	20.044365
61.597590	2274.483268	20.049383
61.486087	2282.355170	20.054400
61.747386	2277.793755	20.059418
61.594336	2282.177462	20.064435
61.541363	2271.497728	20.069453
61.594931	2267.945607	20.074471
61.572958	2269.350825	20.079488
61.851987	2264.993460	20.084506
61.559775	2264.920514	20.089523
61.673235	2272.741587	20.094541
62.112902	2291.977561	20.099559
61.973562	2301.424736	20.104576
62.074162	2300.433328	20.109594
62.018906	2314.126496	20.114611
61.984459	2312.285082	20.119629
62.527130	2303.410733	20.124647
62.437489	2303.995320	20.129664
62.413612	2309.515510	20.134682
62.294153	2313.445510	20.139699
62.343077	2305.858901	20.144717
62.403583	2301.637061	20.149735
62.524441	2316.706210	20.154752
62.724300	2322.806623	20.159770
62.676011	2333.324796	20.164787
62.989153	2342.493743	20.169805
63.359653	2331.197384	20.174823
62.865492	2343.049944	20.179840
62.956876	2330.185584	20.184858
63.413281	2333.909690	20.189875
62.899360	2326.487564	20.194893
62.980293	2333.148912	20.199911
62.932599	2339.074861	20.204928
63.260923	2328.932870	20.209946
63.309883	2337.286562	20.214963
63.105147	2362.152801	20.219981
63.449974	2366.378467	20.224999
63.099356	2361.287705	20.230016
63.617394	2367.596967	20.235034
63.580282	2362.409794	20.240051
63.660354	2360.535164	20.245069
63.913791	2359.279464	20.250087
63.773677	2364.975533	20.255104
63.949834	2371.311006	20.260122
64.121372	2384.644778	20.265139
63.979625	2390.353702	20.270157
64.388716	2382.108650	20.275175
64.419865	2392.839949	20.280192
64.374198	2393.235035	20.285210
64.541060	2389.047336	20.290227
64.351449	2393.454999	20.295245
64.419067	2391.993741	20.300263
64.716627	2396.480238	20.305280
64.750400	2387.242576	20.310298
64.920200	2382.296132	20.315315
64.577852	2379.432471	20.320333
64.970105	2380.706348	20.325351
64.968524	2381.973031	20.330368
65.081198	2377.454955	20.335386
65.030722	2376.522247	20.340403
64.971249	2378.147411	20.345421
65.155261	2377.504529	20.350439
64.923274	2383.369430	20.355456
65.125271	2369.011740	20.360474
65.209234	2377.236377	20.365491
64.890946	2390.822901	20.370509
65.359390	2402.153856	20.375527
65.514873	2409.057420	20.380544
65.542349	2413.052112	20.385562
65.683879	2409.107573	20.390579
65.609770	2407.071103	20.395597
65.729434	2409.187641	20.400615
65.543752	2413.792906	20.405632
65.599587	2399.427033	20.410650
66.151652	2412.022093	20.415667
65.607258	2408.923208	20.420685
65.950731	2405.365719	20.425703
65.722274	2414.492877	20.430720
65.776728	2425.595690	20.435738
65.991140	2433.031833	20.440755
66.061068	2442.836663	20.445773
66.184734	2440.121274	20.450791
66.083016	2441.773634	20.455808
66.014585	2439.746480	20.460826
66.082575	2453.718243	20.465843
66.163496	2470.243624	20.470861
66.625442	2465.589583	20.475879
66.767588	2475.478095	20.480896
66.837467	2475.514944	20.485914
67.091873	2466.650289	20.490931
66.979037	2476.534633	20.495949
66.678487	2466.930983	20.500967
66.426189	2467.883689	20.505984
66.947952	2485.795564	20.511002
67.129203	2493.030936	20.516019
67.125166	2501.710175	20.521037
67.516170	2491.353560	20.526055
67.347901	2496.639630	20.531072
67.275186	2490.028834	20.536090
67.252781	2494.546728	20.541107
66.848513	2499.367013	20.546125
67.573303	2503.726410	20.551143
67.633595	2517.058381	20.556160
67.347028	2525.637960	20.561178
67.993999	2522.408822	20.566195
67.706918	2519.463165	20.571213
67.921539	2514.282986	20.576231
67.989268	2520.038785	20.581248
68.387567	2515.858975	20.586266
68.571471	2514.155763	20.591283
68.613887	2517.663554	20.596301
68.689226	2505.736870	20.601319
68.693921	2509.798936	20.606336
68.558579	2508.255979	20.611354
69.215302	2493.951499	20.616371
68.801413	2503.496080	20.621389
69.169302	2493.718943	20.626407
69.132155	2483.661092	20.631424
68.885663	2483.193844	20.636442
69.031711	2471.178037	20.641459
68.674088	2476.677578	20.646477
68.848642	2468.226038	20.651495
68.930453	2479.715470	20.656512
69.038038	2493.986946	20.661530
69.250800	2491.626254	20.666547
68.995193	2502.507986	20.671565
69.192171	2500.684700	20.676583
69.259965	2506.343731	20.681600
68.989330	2504.312633	20.686618
69.455650	2491.815458	20.691635
68.974404	2501.292120	20.696653
69.088292	2503.552755	20.701671
69.466097	2521.815647	20.706688
68.969903	2531.792634	20.711706
69.733875	2521.098842	20.716723
69.294045	2541.645883	20.721741
69.700584	2544.673200	20.726759
70.035478	2556.591145	20.731776
69.937516	2564.853555	20.736794
69.999967	2563.843830	20.741811
70.298421	2566.993794	20.746829
70.333451	2564.467146	20.751847
70.292352	2566.547991	20.756864
70.150699	2570.875690	20.761882
70.389269	2565.095426	20.766899
69.966436	2566.039153	20.771917
70.567933	2578.821553	20.776935
70.622456	2583.671740	20.781952
70.484064	2594.130529	20.786970
70.701696	2589.315616	20.791987
70.581068	2597.467601	20.797005
70.748465	2591.251098	20.802023
70.669472	2594.149771	20.807040
70.819965	2607.392710	20.812058
71.124496	2612.413057	20.817075
71.083161	2617.313154	20.822093
71.684671	2619.010700	20.827111
71.903488	2619.785233	20.832128
71.445681	2617.112206	20.837146
71.706334	2603.716392	20.842163
71.588933	2611.900122	20.847181
71.807630	2616.547935	20.852199
71.741127	2609.134540	20.857216
71.771219	2604.246487	20.862234
71.916539	2608.103660	20.867251
71.817193	2609.846907	20.872269
71.654829	2604.947071	20.877287
71.674166	2604.050410	20.882304
72.004682	2625.070170	20.887322
72.167811	2633.935998	20.892339
72.614214	2635.638619	20.897357
73.018845	2632.958619	20.902375
72.694837	2625.653932	20.907392
72.659742	2619.868523	20.912410
72.877842	2590.972305	20.917427
72.404659	2598.056457	20.922445
72.647698	2599.046589	20.927463
72.647865	2607.508904	20.932480
72.581996	2617.588797	20.937498
73.082516	2627.119772	20.942515
72.792234	2635.158033	20.947533
72.939349	2630.145115	20.952551
72.917605	2634.891851	20.957568
72.830123	2635.885929	20.962586
73.038810	2621.250825	20.967603
73.119835	2636.397452	20.972621
72.859605	2643.197520	20.977639
73.538436	2645.877014	20.982656
73.412037	2660.307894	20.987674
73.499159	2661.293792	20.992691
73.237139	2660.962738	20.997709
73.521901	2660.261299	21.002727
73.682189	2654.976464	21.007744
73.478518	2672.055613	21.012762
73.618227	2674.573312	21.017779
73.780944	2685.297215	21.022797
73.662973	2694.341636	21.027815
74.141140	2690.988356	21.032832
73.837219	2696.311078	21.037850
73.956712	2704.850384	21.042867
74.317287	2711.097598	21.047885
74.535751	2708.724164	21.052903
74.763592	2704.447989	21.057920
74.704410	2720.391092	21.062938
74.695125	2706.260275	21.067955
75.180635	2712.705456	21.072973
74.723410	2717.746643	21.077991
74.917139	2698.711167	21.083008
74.894974	2707.785940	21.088026
75.122360	2705.430749	21.093043
75.127239	2703.061488	21.098061
75.139702	2701.505163	21.103079
75.359471	2693.465547	21.108096
75.044666	2711.581917	21.113114
75.258569	2702.585923	21.118131
75.209045	2714.969627	21.123149
75.488820	2731.675189	21.128167
75.863289	2729.181691	21.133184
76.033357	2726.310966	21.138202
76.134158	2729.952659	21.143219
75.894157	2730.703619	21.148237
75.979189	2736.089395	21.153255
76.068299	2727.914063	21.158272
75.926876	2731.883076	21.163290
76.289957	2725.727341	21.168307
76.446900	2726.747733	21.173325
76.075100	2735.240340	21.178343
76.148322	2726.527924	21.183360
75.999140	2728.718064	21.188378
76.381523	2721.618462	21.193395
76.367126	2731.229269	21.198413
76.097542	2754.654424	21.203431
76.611645	2751.008285	21.208448
76.398520	2765.176998	21.213466
76.630060	2758.991885	21.218483
76.998677	2757.988381	21.223501
76.556381	2766.240531	21.228519
77.097310	2765.016824	21.233536
77.068747	2778.864280	21.238554
77.009863	2784.512157	21.243571
77.043301	2784.398282	21.248589
77.010209	2797.724950	21.253607
77.348973	2795.196231	21.258624
77.178076	2787.218870	21.263642
77.406426	2780.946156	21.268659
77.699103	2792.875749	21.273677
77.412341	2807.871183	21.278695
77.857908	2807.174770	21.283712
78.104836	2814.594124	21.288730
78.028030	2817.862202	21.293747
77.801416	2818.013201	21.298765
77.927124	2815.912554	21.303783
78.450269	2813.342627	21.308800
78.384948	2810.283667	21.313818
78.151365	2814.840845	21.318835
78.462721	2812.006567	21.323853
78.087876	2815.260034	21.328871
78.413591	2823.893168	21.333888
78.672549	2834.004000	21.338906
78.863324	2836.678773	21.343923
79.022356	2834.538198	21.348941
78.904910	2842.781060	21.353959
79.168014	2833.076261	21.358976
78.687889	2837.108758	21.363994
79.224990	2836.777685	21.369011
79.254913	2829.686259	21.374029
79.114128	2832.682934	21.379047
79.404172	2828.919906	21.384064
79.165415	2838.852108	21.389082
79.355826	2849.463161	21.394099
79.811762	2853.983541	21.399117
79.477500	2865.881814	21.404135
79.787238	2856.890894	21.409152
79.754298	2860.140973	21.414170
79.717896	2863.716480	21.419187
80.026941	2860.698492	21.424205
79.795818	2866.444666	21.429223
80.117717	2868.561271	21.434240
80.037698	2860.699955	21.439258
79.910298	2872.947541	21.444275
80.087561	2878.870082	21.449293
80.205227	2890.187355	21.454311
80.267603	2886.838201	21.459328
80.503194	2885.599465	21.464346
80.151376	2878.565751	21.469363
80.621291	2882.829831	21.474381
80.722414	2909.369350	21.479399
80.810352	2910.356709	21.484416
81.176187	2907.432702	21.489434
81.004947	2909.810457	21.494451
81.377535	2912.652905	21.499469
81.199466	2914.302548	21.504487
81.188318	2906.684303	21.509504
81.348368	2904.236772	21.514522
81.272643	2904.634306	21.519539
81.715725	2897.879707	21.524557
81.376642	2897.386305	21.529575
81.676350	2897.445498	21.534592
81.461813	2896.516110	21.539610
81.736943	2904.282633	21.544627
82.138789	2910.786871	21.549645
82.218982	2913.667298	21.554663
82.596332	2914.219909	21.559680
82.264781	2894.928916	21.564698
82.226038	2895.897147	21.569715
82.416739	2902.383138	21.574733
82.369037	2912.003307	21.579751
82.361493	2909.999415	21.584768
82.631114	2916.271450	21.589786
82.633706	2914.907039	21.594803
82.598172	2912.242126	21.599821
82.444447	2913.921711	21.604839
82.986713	2908.247845	21.609856
83.115166	2911.839550	21.614874
82.952698	2911.997625	21.619891
83.153414	2910.696012	21.624909
83.075484	2916.893683	21.629927
83.352812	2925.026434	21.634944
83.516626	2937.799508	21.639962
83.405626	2941.189487	21.644979
83.568633	2930.573942	21.649997
83.463831	2943.032731	21.655015
83.524421	2939.929277	21.660032
83.414401	2938.144674	21.665050
83.326654	2935.835771	21.670067
83.936878	2950.255653	21.675085
83.632271	2960.274741	21.680103
84.238631	2964.554844	21.685120
83.944029	2970.488173	21.690138
84.036018	2972.725630	21.695155
83.920100	2970.031047	21.700173
84.193883	2985.999213	21.705191
84.387775	2991.346483	21.710208
84.498710	3004.254696	21.715226
84.400879	3011.072297	21.720243
84.566740	3003.517022	21.725261
84.578580	3006.597946	21.730279
84.729703	3010.298548	21.735296
85.097934	3002.530861	21.740314
84.746258	3011.259551	21.745331
84.854601	3020.713312	21.750349
84.872885	3032.487845	21.755367
85.193683	3037.521479	21.760384
85.367527	3032.640250	21.765402
85.346264	3036.655471	21.770419
85.498547	3036.137978	21.775437
85.663049	3036.796909	21.780455
85.888372	3028.981202	21.785472
85.766363	3024.438212	21.790490
85.643333	3039.900987	21.795507
85.992310	3045.311647	21.800525
86.631233	3038.417197	21.805543
86.673415	3036.134755	21.810560
86.815050	3014.836173	21.815578
86.639370	3014.086224	21.820595
86.737787	2996.741872	21.825613
86.796952	3003.182808	21.830631
86.997138	3001.461213	21.835648
86.929258	3002.275198	21.840666
86.674099	3009.965876	21.845683
87.055287	3003.492488	21.850701
86.779206	3010.888371	21.855719
87.007752	3005.575220	21.860736
87.167256	3002.734445	21.865754
86.976204	3004.354703	21.870771
87.247004	3003.933945	21.875789
87.050901	3007.054325	21.880807
87.367412	3027.204527	21.885824
87.678795	3032.975949	21.890842
87.479108	3039.064868	21.895859
87.758729	3033.893807	21.900877
87.811837	3028.593680	21.905895
87.877945	3030.669294	21.910912
87.910823	3025.255973	21.915930
87.731144	3039.178119	21.920947
87.753513	3033.689382	21.925965
88.090047	3046.885745	21.930983
87.947957	3043.232486	21.936000
88.223437	3055.412040	21.941018
88.161525	3060.718321	21.946035
88.262576	3056.610940	21.951053
88.146654	3058.839875	21.956071
88.392872	3072.285869	21.961088
88.757256	3078.976297	21.966106
88.863197	3079.766499	21.971123
89.086156	3086.616359	21.976141
88.945190	3089.872704	21.981159
89.100368	3080.052800	21.986176
88.939664	3078.758468	21.991194
89.024983	3088.643874	21.996211
89.240769	3092.825832	22.001229
89.205721	3106.651033	22.006247
89.225581	3119.731985	22.011264
89.758279	3113.831444	22.016282
89.262272	3127.101655	22.021299
89.391977	3117.731025	22.026317
89.404683	3126.883879	22.031335
89.486425	3133.576143	22.036352
89.849641	3140.809565	22.041370
89.643043	3154.904455	22.046387
89.916634	3147.799974	22.051405
90.201179	3157.326413	22.056423
90.096720	3181.563684	22.061440
90.140704	3171.630870	22.066458
90.304174	3173.861677	22.071475
90.604911	3162.548277	22.076493
90.322512	3168.429394	22.081511
90.773333	3189.374145	22.086528
91.008874	3194.392325	22.091546
90.884362	3202.250275	22.096563
91.467516	3204.822423	22.101581
91.597113	3198.078351	22.106599
91.547147	3190.204985	22.111616
91.861302	3186.868314	22.116634
91.904269	3192.013176	22.121651
91.817024	3180.321905	22.126669
91.941753	3179.723844	22.131687
92.120322	3173.848289	22.136704
92.109164	3155.168206	22.141722
91.884885	3160.359609	22.146739
92.150942	3154.832750	22.151757
92.297574	3175.195109	22.156775
92.099186	3179.305481	22.161792
92.217774	3174.476282	22.166810
92.035007	3185.684370	22.171827
92.326690	3180.710354	22.176845
92.535142	3176.322288	22.181863
92.319350	3180.959338	22.186880
92.392898	3180.378879	22.191898
92.274841	3200.604918	22.196915
92.588976	3205.915785	22.201933
92.780278	3211.515275	22.206951
92.740483	3216.534109	22.211968
93.109331	3223.861858	22.216986
93.052511	3239.908986	22.222003
93.284393	3249.248010	22.227021
93.205074	3247.696038	22.232039
93.211145	3250.905370	22.237056
93.370483	3247.097004	22.242074
93.302129	3267.081575	22.247091
93.806589	3269.532556	22.252109
93.833275	3272.273698	22.257127
93.378202	3282.570300	22.262144
93.555136	3273.022910	22.267162
93.821994	3292.130440	22.272179
94.222924	3301.311168	22.277197
94.096208	3298.964370	22.282215
94.349704	3310.016447	22.287232
94.697758	3303.323232	22.292250
94.047181	3304.636857	22.297267
94.377455	3312.575733	22.302285
94.843581	3323.889690	22.307303
94.383339	3332.167827	22.312320
95.009922	3332.956037	22.317338
95.077756	3333.653213	22.322355
95.308139	3329.269470	22.327373
95.459635	3327.502110	22.332391
95.029564	3329.443714	22.337408
95.240528	3324.948219	22.342426
95.368606	3348.815930	22.347443
95.442100	3360.627547	22.352461
95.536281	3359.556069	22.357479
95.525976	3361.732807	22.362496
95.589488	3359.133041	22.367514
95.690367	3365.141121	22.372531
96.163990	3370.026210	22.377549
96.344740	3386.698757	22.382567
96.174492	3392.466106	22.387584
96.268973	3378.633539	22.392602
96.088266	3390.403121	22.397619
96.280980	3388.948561	22.402637
96.659535	3385.276690	22.407655
96.591684	3408.189285	22.412672
97.151219	3415.820262	22.417690
96.994492	3415.868079	22.422707
97.190747	3412.742891	22.427725
97.404619	3413.691322	22.432743
97.157285	3415.649420	22.437760
97.169438	3412.104414	22.442778
97.275223	3419.295644	22.447795
97.305021	3418.553023	22.452813
97.494308	3418.601513	22.457831
97.447318	3432.058411	22.462848
97.666944	3437.825748	22.467866
97.922560	3443.214474	22.472883
97.852035	3438.180138	22.477901
98.107478	3435.216210	22.482919
97.848781	3444.543916	22.487936
98.310150	3431.086236	22.492954
98.568532	3454.437748	22.497971
98.231332	3469.485164	22.502989
98.544720	3462.413519	22.508007
98.457096	3474.672570	22.513024
98.471393	3472.801995	22.518042
98.785366	3466.074810	22.523059
98.680801	3474.464649	22.528077
99.054243	3479.781105	22.533095
99.185172	3493.182153	22.538112
99.212505	3486.329180	22.543130
99.398314	3490.420061	22.548147
99.654556	3491.173730	22.553165
99.891573	3487.827269	22.558183
99.626154	3491.335612	22.563200
99.625927	3489.319460	22.568218
100.109346	3480.611980	22.573235
99.664414	3492.741590	22.578253
99.985912	3485.693814	22.583271
99.738754	3489.839582	22.588288
100.113685	3495.365058	22.593306
100.153231	3511.851015	22.598323
100.058165	3518.153937	22.603341
100.358834	3527.899098	22.608359
100.448703	3518.595924	22.613376
100.404500	3520.444549	22.618394
100.731938	3527.782203	22.623411
100.440564	3537.385003	22.628429
100.809692	3543.092353	22.633447
100.696504	3559.622388	22.638464
101.040561	3549.165536	22.643482
101.210071	3554.571968	22.648499
101.034344	3560.017726	22.653517
101.770339	3563.684983	22.658535
101.396130	3585.566627	22.663552
101.614533	3571.046242	22.668570
101.740980	3581.397418	22.673587
101.754701	3566.861692	22.678605
101.699068	3568.798678	22.683623
101.798893	3576.411800	22.688640
101.815830	3589.002761	22.693658
102.209563	3600.509411	22.698675
102.373635	3600.620135	22.703693
103.115729	3586.442590	22.708711
102.958811	3584.309028	22.713728
103.143177	3578.286856	22.718746
103.121696	3571.552547	22.723763
103.401450	3577.305630	22.728781
103.610341	3564.893445	22.733799
103.056868	3575.314500	22.738816
103.534119	3574.742805	22.743834
103.582765	3579.903417	22.748851
103.243728	3575.563997	22.753869
103.520409	3567.511684	22.758887
103.304499	3580.915418	22.763904
103.540642	3573.981118	22.768922
103.334587	3573.682018	22.773939
103.728197	3597.690296	22.778957
103.775920	3596.865354	22.783975
104.003479	3602.938290	22.788992
103.986774	3612.350230	22.794010
104.097314	3607.422267	22.799027
104.125421	3616.628037	22.804045
104.160669	3627.321828	22.809063
104.398362	3641.423423	22.814080
104.319124	3639.740023	22.819098
104.429411	3643.811525	22.824115
104.692135	3665.526420	22.829133
105.011889	3667.293422	22.834151
104.723154	3675.344586	22.839168
104.772469	3681.954952	22.844186
104.931201	3675.392456	22.849203
105.050218	3692.083849	22.854221
105.115466	3701.628310	22.859239
105.372917	3701.798091	22.864256
105.293213	3705.742575	22.869274
105.458476	3706.515485	22.874291
105.423959	3725.686589	22.879309
105.720596	3725.558268	22.884327
105.813838	3736.995731	22.889344
106.010996	3728.830146	22.894362
106.450951	3740.475069	22.899379
106.337409	3751.380691	22.904397
106.750556	3750.724814	22.909415
107.145311	3745.936348	22.914432
107.231633	3743.246344	22.919450
107.164104	3744.741568	22.924467
107.004224	3750.780378	22.929485
107.568479	3737.789028	22.934503
107.401378	3746.152020	22.939520
106.958079	3741.001600	22.944538
107.283016	3730.000148	22.949555
107.343638	3741.633978	22.954573
107.619102	3729.284985	22.959591
107.640001	3737.105084	22.964608
107.610769	3739.651484	22.969626
108.105583	3742.031714	22.974643
107.739538	3756.441313	22.979661
107.862276	3760.112806	22.984679
108.025428	3770.245075	22.989696
107.859315	3767.263347	22.994714
108.228832	3772.412191	22.999731
108.618302	3800.253335	23.004749
108.841779	3801.447277	23.009767
109.015206	3792.319407	23.014784
109.080108	3803.622988	23.019802
109.539049	3786.517573	23.024819
108.978122	3792.196339	23.029837
109.299123	3797.012299	23.034855
109.699893	3788.044845	23.039872
109.552448	3786.314878	23.044890
109.511522	3781.962468	23.049907
109.370335	3791.673642	23.054925
109.659079	3786.288465	23.059943
109.750029	3782.741030	23.064960
109.430745	3801.371575	23.069978
109.692466	3808.622305	23.074995
109.711017	3822.461658	23.080013
110.172559	3817.419437	23.085031
110.061031	3825.270142	23.090048
109.884485	3850.400299	23.095066
110.522957	3845.594963	23.100083
110.387357	3860.378558	23.105101
110.390296	3862.181161	23.110119
110.556463	3872.671744	23.115136
110.586410	3890.168176	23.120154
110.959464	3886.278365	23.125171
110.640993	3885.209721	23.130189
111.195285	3903.337640	23.135207
111.389440	3910.809238	23.140224
111.384707	3918.082846	23.145242
111.539144	3915.577831	23.150259
111.498978	3914.997385	23.155277
111.599223	3918.291753	23.160295
112.123081	3912.382083	23.165312
111.641493	3930.758616	23.170330
112.240063	3932.268786	23.175347
112.213828	3946.272734	23.180365
112.327076	3944.638057	23.185383
112.423139	3949.346763	23.190400
112.086321	3952.686451	23.195418
112.504741	3955.144981	23.200435
112.900371	3967.519327	23.205453
112.921150	3973.061342	23.210471
113.215356	3964.335766	23.215488
113.034303	3971.672919	23.220506
113.127815	3963.016323	23.225523
113.107708	3970.197220	23.230541
113.378757	3987.941672	23.235559
113.490575	3998.322224	23.240576
113.567506	3997.557897	23.245594
113.746293	3997.549064	23.250611
113.637891	4008.044195	23.255629
113.701223	4016.807990	23.260647
113.940899	4021.777810	23.265664
113.888729	4034.461202	23.270682
113.781493	4038.265415	23.275699
114.171174	4046.120485	23.280717
114.550850	4056.828104	23.285735
114.425379	4059.950814	23.290752
114.756697	4063.925037	23.295770
114.757581	4062.686662	23.300787
114.800929	4080.806600	23.305805
115.133464	4086.630137	23.310823
115.036278	4086.283770	23.315840
115.239300	4092.637737	23.320858
115.380401	4084.499775	23.325875
115.459515	4106.276071	23.330893
115.623133	4116.948174	23.335911
115.914589	4106.242070	23.340928
116.021189	4110.991630	23.345946
116.090415	4112.058365	23.350963
116.046521	4113.431068	23.355981
116.404960	4119.399172	23.360999
117.186532	4124.299133	23.366016
116.924903	4124.474603	23.371034
117.082774	4113.084136	23.376051
116.778012	4108.453520	23.381069
117.243359	4113.684754	23.386087
117.311139	4118.173818	23.391104
117.221385	4126.257217	23.396122
117.519967	4117.068281	23.401139
117.275597	4120.632416	23.406157
117.430047	4121.812218	23.411175
117.437062	4123.592175	23.416192
117.287541	4117.609655	23.421210
117.528225	4119.833017	23.426227
117.580328	4134.535033	23.431245
117.675317	4147.032996	23.436263
118.056524	4141.895701	23.441280
117.998464	4161.039660	23.446298
117.970308	4161.951216	23.451315
118.301773	4164.486584	23.456333
118.289303	4185.942473	23.461351
118.339319	4187.807624	23.466368
118.205983	4195.455889	23.471386
118.503821	4193.552594	23.476403
118.923897	4219.382013	23.481421
118.871218	4213.138562	23.486439
119.504708	4209.792437	23.491456
119.374374	4216.584311	23.496474
119.665871	4210.753273	23.501491
120.056006	4206.869310	23.506509
119.616978	4217.337071	23.511527
119.846394	4228.023149	23.516544
119.890068	4233.342910	23.521562
120.302285	4237.852608	23.526579
120.605375	4236.614015	23.531597
120.400125	4238.749594	23.536615
120.472635	4233.611933	23.541632
120.416423	4231.490536	23.546650
120.894043	4237.839325	23.551667
121.362445	4245.848730	23.556685
121.041672	4249.460480	23.561703
121.195688	4246.380402	23.566720
121.455272	4258.136320	23.571738
121.382761	4251.167534	23.576755
121.558657	4244.478537	23.581773
121.374334	4255.521691	23.586791
121.689884	4251.410454	23.591808
121.397949	4253.178311	23.596826
121.593888	4265.356612	23.601843
121.867754	4277.628701	23.606861
121.841848	4284.979030	23.611879
122.038208	4284.210591	23.616896
121.936926	4293.755246	23.621914
121.954929	4304.737064	23.626931
122.311370	4317.449157	23.631949
122.256014	4317.721540	23.636967
122.944032	4329.023711	23.641984
122.664757	4348.532816	23.647002
122.786407	4356.337178	23.652019
122.927960	4348.755197	23.657037
123.122136	4361.146269	23.662055
123.222266	4369.554324	23.667072
123.913009	4353.347467	23.672090
124.068163	4352.241808	23.677107
124.663698	4348.587813	23.682125
124.855130	4349.137883	23.687143
124.935594	4325.797801	23.692160
124.807854	4313.880793	23.697178
124.832737	4303.360236	23.702195
125.283253	4299.101592	23.707213
125.474366	4302.598686	23.712231
125.319903	4299.164999	23.717248
125.004223	4283.968342	23.722266
125.045805	4270.303860	23.727283
125.179186	4278.800177	23.732301
124.904890	4299.374400	23.737319
125.581016	4295.480998	23.742336
125.362610	4296.611708	23.747354
125.208572	4308.536682	23.752371
125.376722	4287.741811	23.757389
125.261274	4310.130019	23.762407
125.472882	4321.962869	23.767424
125.685321	4326.383300	23.772442
125.545051	4335.910598	23.777459
125.990968	4352.164343	23.782477
126.308484	4367.247514	23.787495
126.474974	4356.355041	23.792512
126.479859	4362.594396	23.797530
126.303753	4372.258024	23.802547
126.705916	4390.800228	23.807565
126.988443	4391.198100	23.812583
126.823408	4382.853900	23.817600
126.802051	4395.618440	23.822618
127.090238	4409.598651	23.827635
127.408445	4410.098613	23.832653
127.682266	4416.303758	23.837671
127.721199	4412.808523	23.842688
128.025307	4417.440149	23.847706
127.876889	4435.616278	23.852723
128.169403	4439.351342	23.857741
127.934053	4452.607131	23.862759
128.520969	4442.343789	23.867776
128.534631	4441.439269	23.872794
128.351848	4446.444347	23.877811
128.699417	4460.316013	23.882829
128.416505	4471.776270	23.887847
129.006053	4477.223844	23.892864
128.759064	4472.414756	23.897882
128.868843	4492.059475	23.902899
129.540879	4494.392694	23.907917
129.122256	4507.134141	23.912935
129.592096	4509.316302	23.917952
129.250680	4518.326668	23.922970
129.564260	4529.536870	23.927987
130.040815	4531.395411	23.933005
129.846703	4537.559579	23.938023
129.889292	4553.144648	23.943040
130.243732	4556.611825	23.948058
130.181076	4563.017016	23.953075
130.506806	4557.053724	23.958093
130.867925	4560.252355	23.963111
131.309669	4559.467589	23.968128
131.469753	4558.289537	23.973146
131.211046	4550.300826	23.978163
131.673185	4558.008518	23.983181
131.617675	4575.742032	23.988199
131.788336	4562.232134	23.993216
131.914548	4570.524431	23.998234
131.794231	4567.044326	24.003251
132.109036	4561.637407	24.008269
131.997183	4565.029467	24.013287
131.965649	4562.439140	24.018304
132.310309	4557.344507	24.023322
132.150391	4570.781118	24.028339
132.616138	4580.412549	24.033357
133.088231	4595.202249	24.038375
133.141588	4598.168321	24.043392
133.315024	4592.765839	24.048410
133.271404	4599.871334	24.053427
133.552590	4596.165922	24.058445
133.420432	4599.546279	24.063463
133.453886	4592.045136	24.068480
133.463511	4596.028322	24.073498
133.321573	4606.840766	24.078515
133.629898	4606.333742	24.083533
133.545213	4619.029902	24.088551
133.743338	4624.231557	24.093568
134.159947	4648.003448	24.098586
133.994404	4658.880271	24.103603
134.243005	4656.541062	24.108621
134.395750	4662.794728	24.113639
134.445608	4671.063069	24.118656
134.777597	4671.634795	24.123674
134.924912	4682.425558	24.128691
135.344357	4685.902855	24.133709
135.089793	4717.173118	24.138727
135.287762	4717.689905	24.143744
135.423661	4719.926136	24.148762
135.443018	4726.399353	24.153779
135.663628	4734.467422	24.158797
135.542043	4747.675439	24.163815
135.784028	4749.209523	24.168832
136.213337	4766.059565	24.173850
136.055140	4776.881806	24.178867
136.415276	4781.591941	24.183885
136.358687	4783.724345	24.188903
136.538072	4798.860669	24.193920
136.985301	4803.335066	24.198938
136.905214	4807.832186	24.203955
137.173670	4809.886014	24.208973
137.041393	4823.290125	24.213991
137.327418	4836.886379	24.219008
137.429700	4839.589012	24.224026
137.388250	4845.865068	24.229043
137.404224	4837.767100	24.234061
137.719694	4868.304028	24.239079
137.932658	4868.265359	24.244096
137.736658	4869.886604	24.249114
138.054527	4890.634710	24.254131
138.348913	4901.414768	24.259149
138.328801	4906.136800	24.264167
138.732253	4905.549301	24.269184
139.668130	4894.753245	24.274202
139.558061	4890.509087	24.279219
139.866955	4876.850982	24.284237
139.874477	4875.402997	24.289255
139.611487	4880.034726	24.294272
140.099249	4864.967399	24.299290
140.030074	4870.162987	24.304307
140.167298	4876.555324	24.309325
139.771695	4878.988047	24.314343
139.980143	4905.495179	24.319360
140.178118	4901.089395	24.324378
140.117984	4906.128568	24.329395
140.520235	4914.754675	24.334413
140.645808	4936.338335	24.339431
140.477891	4945.875154	24.344448
141.203661	4937.055804	24.349466
140.949740	4945.176842	24.354483
141.094106	4946.905102	24.359501
141.383831	4959.833730	24.364519
141.611703	4965.531912	24.369536
141.770507	4961.388832	24.374554
141.620876	4970.302017	24.379571
141.984382	4982.240988	24.384589
142.107526	4989.040001	24.389607
142.001346	4996.135207	24.394624
142.333734	4988.745116	24.399642
142.293078	5014.745384	24.404659
142.183579	5019.482493	24.409677
142.369231	5028.829240	24.414695
142.524989	5041.613301	24.419712
142.805392	5056.360080	24.424730
142.723645	5070.753156	24.429747
142.641155	5073.961272	24.434765
142.891593	5097.178199	24.439783
143.199568	5098.465775	24.444800
143.617486	5106.760639	24.449818
143.894433	5123.053984	24.454835
143.986298	5119.387286	24.459853
143.810968	5133.995965	24.464871
144.180343	5144.437747	24.469888
144.763378	5143.856221	24.474906
144.872530	5155.855560	24.479923
145.143825	5147.477540	24.484941
145.117556	5154.141531	24.489959
145.322018	5174.390443	24.494976
145.957528	5176.793330	24.499994
145.982545	5177.154401	24.505011
145.821981	5155.844269	24.510029
145.730811	5146.347077	24.515047
145.999327	5165.574010	24.520064
146.347117	5160.717058	24.525082
146.527591	5174.224245	24.530099
146.483931	5169.071740	24.535117
146.645943	5169.926285	24.540135
146.527653	5164.585062	24.545152
146.691797	5158.515910	24.550170
146.383652	5171.217493	24.555187
146.580532	5158.636737	24.560205
146.814567	5184.558099	24.565223
146.834371	5194.049409	24.570240
147.155203	5195.569395	24.575258
147.013152	5213.919336	24.580275
147.485161	5225.222820	24.585293
147.846395	5223.394260	24.590311
148.066665	5222.160930	24.595328
148.563626	5212.901135	24.600346
148.597131	5220.100054	24.605363
148.793144	5233.460843	24.610381
148.952588	5240.672734	24.615399
148.901587	5244.179551	24.620416
149.107390	5236.552255	24.625434
149.075589	5241.745948	24.630451
149.383717	5239.131237	24.635469
149.622284	5228.645181	24.640487
149.381262	5229.509710	24.645504
149.660283	5235.293465	24.650522
149.749463	5245.551054	24.655539
149.722658	5259.180273	24.660557
149.945466	5259.029891	24.665575
149.966809	5266.191434	24.670592
149.872215	5270.495893	24.675610
150.197479	5287.471697	24.680627
150.271647	5305.701519	24.685645
150.629906	5309.622226	24.690663
150.401436	5323.474842	24.695680
151.008987	5317.799894	24.700698
151.387828	5322.550494	24.705715
151.536989	5325.648560	24.710733
151.705531	5327.697152	24.715751
151.736377	5348.776477	24.720768
151.981698	5346.532096	24.725786
151.804239	5355.732395	24.730803
152.001292	5352.751439	24.735821
152.044591	5354.963195	24.740839
152.155336	5379.332623	24.745856
152.376149	5383.443632	24.750874
152.307750	5389.916184	24.755891
152.757120	5397.384825	24.760909
152.826437	5410.653470	24.765927
152.417224	5409.027987	24.770944
152.839026	5422.561435	24.775962
152.951804	5440.159006	24.780979
153.017908	5441.059544	24.785997
153.481129	5452.168702	24.791015
153.675856	5473.646138	24.796032
153.377904	5469.649703	24.801050
153.745158	5488.271242	24.806067
153.905498	5495.365888	24.811085
154.447445	5498.007191	24.816103
154.078379	5513.109752	24.821120
154.209705	5529.691119	24.826138
154.808168	5542.737039	24.831155
154.467903	5547.442663	24.836173
155.057860	5558.604076	24.841191
155.091344	5573.227097	24.846208
155.177327	5582.176249	24.851226
155.433018	5593.779652	24.856243
155.701006	5602.756442	24.861261
156.152464	5600.922893	24.866279
155.914654	5609.214812	24.871296
156.335459	5619.352907	24.876314
156.538525	5629.432102	24.881331
156.182516	5630.898770	24.886349
156.758997	5636.635253	24.891367
156.912817	5654.844937	24.896384
156.817576	5660.122060	24.901402
157.183961	5661.608870	24.906419
157.206772	5666.546957	24.911437
157.352637	5683.267798	24.916455
157.527413	5691.888935	24.921472
158.074657	5685.295861	24.926490
157.924183	5701.615514	24.931507
157.823917	5719.431492	24.936525
158.416435	5721.811432	24.941543
158.344927	5723.139905	24.946560
158.600159	5740.372085	24.951578
158.782341	5746.394927	24.956595
159.123852	5760.951710	24.961613
159.524078	5748.110653	24.966631
159.093762	5762.419934	24.971648
159.293445	5753.008153	24.976666
159.462568	5771.430330	24.981683
159.226024	5780.257938	24.986701
159.818590	5781.343631	24.991719
159.698408	5817.018838	24.996736
159.764824	5818.684100	25.001754
160.195152	5827.955362	25.006771
160.169109	5849.046830	25.011789
160.485178	5844.289917	25.016807
160.817562	5850.520166	25.021824
160.795674	5866.547270	25.026842
160.875153	5875.507864	25.031859
161.114090	5884.193629	25.036877
161.409356	5896.185137	25.041895
161.417636	5905.902974	25.046912
161.350291	5914.466074	25.051930
161.871162	5910.918031	25.056947
162.003106	5930.270806	25.061965
162.202739	5933.253162	25.066983
162.334491	5949.202356	25.072000
162.021496	5942.111398	25.077018
162.392240	5953.021675	25.082035
162.546017	5973.769933	25.087053
163.069567	5971.095571	25.092071
163.294660	5979.830806	25.097088
163.326842	5993.966642	25.102106
163.367334	6004.131024	25.107123
163.553640	6021.152646	25.112141
163.918955	6015.669487	25.117159
163.960570	6036.445945	25.122176
164.298528	6051.482737	25.127194
164.739236	6048.744465	25.132211
164.635115	6062.542535	25.137229
164.797959	6046.163100	25.142247
164.543673	6062.158233	25.147264
165.024567	6081.029910	25.152282
165.147314	6077.383230	25.157299
165.291265	6092.093007	25.162317
165.445407	6081.511236	25.167335
165.594765	6097.880291	25.172352
165.739726	6111.059610	25.177370
166.317181	6106.766060	25.182387
166.093074	6113.968723	25.187405
166.038799	6118.731994	25.192423
166.523412	6145.523050	25.197440
166.454509	6144.128827	25.202458
166.484061	6142.551319	25.207475
166.306252	6171.953993	25.212493
166.686207	6167.695064	25.217511
166.849342	6187.817411	25.222528
167.066243	6196.662659	25.227546
167.222567	6214.793165	25.232563
167.390581	6228.755713	25.237581
167.336279	6227.402429	25.242599
167.838534	6260.715827	25.247616
168.139986	6263.357853	25.252634
168.408249	6271.958129	25.257651
168.601490	6283.409950	25.262669
169.257914	6282.617629	25.267687
169.614998	6292.092844	25.272704
169.449049	6285.049873	25.277722
169.954768	6283.575031	25.282739
170.408331	6279.858245	25.287757
170.350376	6282.806998	25.292775
170.637159	6283.055547	25.297792
170.707222	6281.665118	25.302810
171.078996	6271.351432	25.307827
170.962434	6275.672272	25.312845
170.904291	6267.822956	25.317863
170.966827	6244.590500	25.322880
170.937220	6253.841738	25.327898
170.841204	6252.891651	25.332915
170.834212	6261.124311	25.337933
170.921369	6249.841044	25.342951
171.257405	6277.669433	25.347968
171.065076	6278.578183	25.352986
171.572547	6280.613784	25.358003
171.833239	6301.928477	25.363021
172.926403	6280.977815	25.368039
173.226180	6278.786772	25.373056
173.158956	6288.388650	25.378074
173.396913	6270.272315	25.383091
173.243103	6279.307331	25.388109
173.442996	6284.384978	25.393127
173.478255	6284.012716	25.398144
173.437885	6277.554778	25.403162
173.717363	6264.254155	25.408179
173.404900	6284.636578	25.413197
173.662504	6274.925689	25.418215
173.749327	6292.473336	25.423232
173.926757	6305.727905	25.428250
174.180180	6317.129244	25.433267
174.295926	6326.565855	25.438285
174.477425	6331.194037	25.443303
174.474509	6341.870703	25.448320
174.775711	6362.153026	25.453338
175.017892	6373.350056	25.458355
174.825395	6385.587325	25.463373
175.019727	6402.788286	25.468391
175.276843	6411.059961	25.473408
174.914030	6433.842523	25.478426
175.380564	6443.745721	25.483443
175.658411	6472.327292	25.488461
175.878457	6473.965772	25.493479
176.065778	6493.171974	25.498496
176.567981	6510.608800	25.503514
176.892497	6523.897550	25.508531
176.778967	6538.393108	25.513549
176.989941	6539.003098	25.518567
177.106783	6559.097137	25.523584
177.245811	6575.130822	25.528602
177.763712	6573.714597	25.533619
178.006023	6603.195913	25.538637
178.089374	6606.306316	25.543655
178.102957	6612.918185	25.548672
178.220177	6628.746897	25.553690
178.388590	6635.970630	25.558707
178.561269	6653.970813	25.563725
178.503452	6660.399742	25.568743
178.813448	6663.678595	25.573760
178.889271	6691.742021	25.578778
179.333296	6697.597612	25.583795
179.659151	6703.942568	25.588813
179.878736	6717.374115	25.593831
180.384211	6722.485808	25.598848
180.434464	6720.333701	25.603866
180.412034	6719.939153	25.608883
180.948340	6732.525520	25.613901
181.110552	6749.149751	25.618919
181.450616	6747.518736	25.623936
181.348966	6750.165324	25.628954
181.599515	6742.546649	25.633971
181.719345	6743.342709	25.638989
181.687531	6751.008360	25.644007
181.950177	6754.617383	25.649024
182.117049	6770.339975	25.654042
182.538047	6766.769107	25.659059
182.352774	6775.432547	25.664077
182.216722	6773.557202	25.669095
182.500259	6794.772181	25.674112
182.548550	6811.601912	25.679130
182.993184	6815.321990	25.684148
183.020147	6832.449420	25.689165
183.215838	6830.370889	25.694183
183.715612	6830.594146	25.699200
183.815432	6853.091140	25.704218
184.881697	6845.953726	25.709236
185.419666	6833.880546	25.714253
185.693165	6816.130842	25.719271
186.362707	6809.137742	25.724288
185.892671	6787.442631	25.729306
185.880629	6778.696574	25.734324
186.255298	6776.373923	25.739341
186.514146	6775.898332	25.744359
186.515970	6778.161764	25.749376
186.065175	6760.563800	25.754394
186.545249	6768.484609	25.759412
186.781260	6780.444584	25.764429
186.389386	6780.710077	25.769447
186.862340	6776.022278	25.774464
186.558335	6777.387127	25.779482
186.671236	6771.447449	25.784500
186.910891	6774.191483	25.789517
186.821693	6796.143355	25.794535
186.946825	6799.996988	25.799552
187.169207	6831.375841	25.804570
187.429388	6835.039569	25.809588
187.270090	6851.136067	25.814605
187.442280	6872.359469	25.819623
187.894821	6887.522049	25.824640
187.777538	6911.385861	25.829658
187.793622	6926.525222	25.834676
187.829600	6944.773377	25.839693
188.162274	6971.606679	25.844711
188.576965	6991.167941	25.849728
188.654009	7010.002120	25.854746
189.179167	7028.447778	25.859764
189.548265	7050.590548	25.864781
189.492620	7051.258020	25.869799
189.811900	7066.372001	25.874816
190.169313	7079.128819	25.879834
190.229523	7096.377148	25.884852
190.573194	7102.863430	25.889869
190.676537	7117.568109	25.894887
190.715437	7124.001489	25.899904
190.560373	7138.603395	25.904922
190.950008	7149.340014	25.909940
191.446907	7163.816753	25.914957
191.902619	7163.114626	25.919975
192.470890	7155.666190	25.924992
192.391341	7164.224085	25.930010
192.316665	7176.483345	25.935028
192.668044	7187.308711	25.940045
192.948420	7194.876032	25.945063
193.256595	7189.881539	25.950080
193.243975	7202.946893	25.955098
193.813485	7207.176715	25.960116
193.978462	7225.794927	25.965133
193.899688	7228.251467	25.970151
194.024876	7222.179034	25.975168
194.172656	7232.369642	25.980186
194.195428	7243.536216	25.985204
194.604442	7249.558917	25.990221
194.785749	7258.216123	25.995239
195.004103	7251.382885	26.000256
195.037042	7271.777681	26.005274
195.295661	7275.368590	26.010292
195.336819	7274.688489	26.015309
195.281815	7294.087799	26.020327
195.784417	7303.643544	26.025344
195.945015	7311.658072	26.030362
195.894756	7332.487972	26.035380
196.041235	7332.337944	26.040397
196.052279	7355.117383	26.045415
196.628587	7371.234074	26.050432
196.749703	7383.651135	26.055450
196.830003	7402.487652	26.060468
197.063509	7404.723683	26.065485
196.902610	7428.154630	26.070503
197.385470	7434.379661	26.075520
197.576792	7461.121501	26.080538
197.497624	7481.414066	26.085556
197.608437	7497.125906	26.090573
197.863580	7524.467508	26.095591
198.500859	7538.125133	26.100608
198.285983	7557.125363	26.105626
198.786392	7573.716268	26.110644
199.528983	7579.306647	26.115661
199.416007	7600.326327	26.120679
199.684319	7613.878390	26.125696
199.790485	7616.928713	26.130714
199.981069	7637.403529	26.135732
200.394987	7637.257286	26.140749
200.322738	7645.833177	26.145767
200.415160	7659.854763	26.150784
200.900395	7676.048469	26.155802
200.822192	7686.255744	26.160820
200.941891	7695.897970	26.165837
201.060584	7708.296803	26.170855
201.704047	7719.999787	26.175872
202.115404	7729.899272	26.180890
202.204818	7737.395021	26.185908
202.643620	7729.114754	26.190925
202.752919	7739.739121	26.195943
202.909000	7755.842966	26.200960
203.123615	7765.780924	26.205978
203.035518	7770.037853	26.210996
203.458681	7769.445547	26.216013
203.270274	7786.510836	26.221031
203.539124	7795.564365	26.226048
203.816411	7805.383767	26.231066
203.970004	7821.565194	26.236084
204.125333	7824.031722	26.241101
204.404729	7842.973970	26.246119
204.404027	7855.224354	26.251136
204.760452	7865.845607	26.256154
204.984298	7875.349771	26.261172
204.971690	7882.237462	26.266189
205.032061	7907.876517	26.271207
205.365763	7923.367564	26.276224
205.576398	7931.952028	26.281242
206.116821	7953.238657	26.286260
206.267565	7958.960526	26.291277
206.266167	7971.034064	26.296295
206.598221	7981.637646	26.301312
206.862699	7998.558973	26.306330
206.982265	8009.643015	26.311348
207.335086	8020.808699	26.316365
207.071986	8029.098905	26.321383
207.424136	8052.366409	26.326400
207.938102	8048.470384	26.331418
207.863486	8081.565869	26.336436
208.562254	8089.585116	26.341453
208.352360	8092.391232	26.346471
208.578507	8116.894686	26.351488
209.008344	8118.533744	26.356506
209.196263	8139.375582	26.361524
209.982450	8136.892299	26.366541
210.059608	8144.492110	26.371559
210.040981	8138.328528	26.376576
210.394846	8145.460085	26.381594
210.660285	8167.096179	26.386612
210.880408	8174.867185	26.391629
210.949551	8173.671881	26.396647
211.170076	8173.443155	26.401664
211.549538	8184.907674	26.406682
211.454144	8203.909347	26.411700
211.551709	8200.297643	26.416717
211.853011	8211.941861	26.421735
211.944286	8225.251618	26.426752
212.236190	8224.038107	26.431770
212.274824	8235.811567	26.436788
212.684238	8241.316432	26.441805
212.608780	8267.061956	26.446823
212.955401	8270.399072	26.451840
212.999962	8276.889097	26.456858
212.962889	8294.978215	26.461876
213.168748	8289.877309	26.466893
213.263945	8312.027852	26.471911
213.499147	8335.142502	26.476928
213.742513	8348.352576	26.481946
213.938991	8364.857472	26.486964
213.884694	8379.480720	26.491981
213.739202	8406.638358	26.496999
214.275859	8427.525332	26.502016
214.934496	8452.057962	26.507034
214.724433	8476.043327	26.512052
215.108303	8485.772609	26.517069
215.550875	8506.335530	26.522087
215.804679	8527.139863	26.527104
215.912356	8546.397608	26.532122
216.386774	8556.898245	26.537140
216.785275	8567.871343	26.542157
216.590045	8578.001090	26.547175
216.869147	8607.286135	26.552192
217.068562	8610.727063	26.557210
217.423055	8640.341680	26.562228
217.605966	8641.690442	26.567245
218.031880	8665.333917	26.572263
218.125739	8685.821656	26.577280
218.280604	8692.711743	26.582298
218.326271	8717.237084	26.587316
218.932385	8719.142815	26.592333
219.099791	8737.827447	26.597351
219.281830	8744.197390	26.602368
219.936310	8770.139820	26.607386
220.406935	8765.469885	26.612404
221.255384	8753.749768	26.617421
221.574790	8751.547771	26.622439
221.604178	8755.162997	26.627456
222.172215	8751.958548	26.632474
222.173526	8732.828373	26.637492
222.085345	8715.021159	26.642509
221.982604	8705.724990	26.647527
221.910969	8710.889254	26.652544
222.346465	8722.499493	26.657562
222.027011	8745.915283	26.662580
222.373206	8740.081644	26.667597
222.506782	8752.135080	26.672615
222.488686	8782.119431	26.677632
222.975896	8780.665023	26.682650
222.504399	8794.237344	26.687668
223.032544	8802.207063	26.692685
223.268897	8821.142858	26.697703
223.539230	8821.854445	26.702720
224.033547	8852.753904	26.707738
224.063663	8870.048817	26.712756
224.129635	8873.668076	26.717773
224.396717	8884.236231	26.722791
224.727937	8904.796994	26.727808
224.931007	8897.791533	26.732826
224.832857	8927.114919	26.737844
225.130862	8935.178453	26.742861
225.564249	8953.695040	26.747879
226.577888	8940.576800	26.752896
227.540165	8926.448848	26.757914
227.337720	8930.241544	26.762932
227.971042	8925.476766	26.767949
227.990758	8919.111982	26.772967
227.976887	8919.286938	26.777984
228.156117	8916.380130	26.783002
228.236947	8923.361215	26.788020
228.458473	8916.732897	26.793037
228.467030	8918.652079	26.798055
228.239870	8924.163857	26.803072
228.686739	8927.197121	26.808090
228.449782	8946.319882	26.813108
228.483146	8955.000874	26.818125
229.256566	8973.269296	26.823143
228.963106	8989.304094	26.828160
229.158432	9001.432484	26.833178
229.069973	9034.546443	26.838196
229.628686	9050.446632	26.843213
229.628271	9062.264347	26.848231
229.726177	9092.649876	26.853248
230.021457	9111.018694	26.858266
230.119139	9140.511950	26.863284
230.789510	9164.635061	26.868301
230.778248	9187.959909	26.873319
231.028559	9203.017016	26.878336
231.137839	9216.171326	26.883354
231.497838	9248.591778	26.888372
231.755479	9268.558811	26.893389
232.067942	9285.539264	26.898407
232.220859	9301.566582	26.903424
232.642371	9323.330171	26.908442
232.543650	9346.117938	26.913460
232.637999	9362.187317	26.918477
233.399423	9396.205380	26.923495
233.932678	9407.587694	26.928512
234.058929	9409.816736	26.933530
234.484087	9432.224430	26.938548
234.880992	9424.757352	26.943565
235.248180	9442.605550	26.948583
235.257459	9452.054423	26.953600
235.928236	9443.573340	26.958618
235.938232	9454.400481	26.963636
235.863796	9473.654216	26.968653
236.590842	9474.782920	26.973671
236.467640	9495.238294	26.978688
236.803975	9503.169323	26.983706
237.079119	9517.577469	26.988724
237.344372	9522.334166	26.993741
237.149589	9523.118364	26.998759
237.072713	9533.748501	27.003776
237.877459	9552.678422	27.008794
237.539144	9551.641616	27.013812
237.855489	9572.616863	27.018829
238.398567	9580.232056	27.023847
238.168284	9592.914340	27.028864
238.231389	9608.281075	27.033882
238.586248	9638.664913	27.038900
239.071098	9647.037843	27.043917
239.296858	9657.428585	27.048935
239.091055	9676.137287	27.053952
239.573912	9702.317248	27.058970
239.680214	9712.602335	27.063988
239.652923	9736.806503	27.069005
240.261908	9764.078476	27.074023
240.045316	9786.811329	27.079040
240.665504	9798.345745	27.084058
240.692487	9830.251548	27.089076
241.220182	9846.409760	27.094093
241.630955	9849.993176	27.099111
242.017593	9877.826512	27.104128
242.267711	9888.281606	27.109146
242.818797	9898.576189	27.114164
243.152671	9904.101194	27.119181
243.309179	9929.493065	27.124199
243.316835	9940.170612	27.129216
243.660549	9948.037741	27.134234
243.546481	9979.284806	27.139252
243.756977	9991.871579	27.144269
244.396440	9991.476887	27.149287
244.444628	10015.897700	27.154304
244.895711	10036.040717	27.159322
245.055509	10044.130032	27.164340
245.559923	10063.554314	27.169357
245.833822	10065.093719	27.174375
245.880530	10076.973187	27.179392
246.270761	10083.365210	27.184410
246.788139	10083.155249	27.189428
247.097916	10093.173633	27.194445
247.557081	10098.620106	27.199463
247.917177	10102.628775	27.204480
249.180545	10088.411224	27.209498
249.440166	10068.471237	27.214516
249.157132	10063.715646	27.219533
249.480470	10055.659504	27.224551
249.419604	10054.342331	27.229568
249.329517	10044.320846	27.234586
249.452155	10043.420651	27.239604
249.402888	10047.939219	27.244621
249.723335	10045.495660	27.249639
249.664813	10071.429273	27.254656
249.935097	10071.066280	27.259674
250.029769	10079.273422	27.264692
249.921825	10098.770972	27.269709
250.315260	10111.414861	27.274727
250.372857	10128.976392	27.279744
250.865240	10140.787226	27.284762
250.887887	10157.092395	27.289780
251.258774	10175.566942	27.294797
251.609973	10184.445885	27.299815
251.430066	10209.478284	27.304832
251.966395	10227.404340	27.309850
252.051247	10234.475506	27.314868
252.242678	10259.952482	27.319885
252.732727	10267.918440	27.324903
252.916819	10286.034313	27.329920
253.030430	10307.441921	27.334938
252.822425	10329.454889	27.339956
252.993293	10351.590474	27.344973
253.733347	10366.422326	27.349991
253.773135	10388.791356	27.355008
254.039566	10412.761689	27.360026
254.345926	10436.607247	27.365044
254.424564	10465.417883	27.370061
254.849692	10494.134775	27.375079
254.906080	10518.460652	27.380096
255.354821	10536.046876	27.385114
256.040519	10566.721027	27.390132
256.218158	10592.158655	27.395149
256.693686	10595.040131	27.400167
256.809048	10624.889607	27.405184
256.866214	10639.413067	27.410202
257.516579	10657.097547	27.415220
257.363471	10672.319602	27.420237
257.968983	10684.036095	27.425255
258.235865	10696.246138	27.430272
258.387317	10719.469893	27.435290
258.671313	10734.091870	27.440308
258.695019	10759.883301	27.445325
259.251009	10769.015640	27.450343
259.298164	10795.012352	27.455360
259.924210	10805.203922	27.460378
260.160599	10821.727196	27.465396
260.279393	10840.221101	27.470413
260.444949	10860.563426	27.475431
260.436128	10872.796310	27.480448
260.971714	10884.514269	27.485466
261.472771	10910.353823	27.490484
261.400149	10930.536267	27.495501
262.081575	10935.695763	27.500519
262.181513	10965.510592	27.505536
262.338598	10969.119767	27.510554
263.022966	10985.846490	27.515572
263.125597	10995.564787	27.520589
263.626179	10995.026544	27.525607
264.100930	11022.539428	27.530624
264.231413	11018.400383	27.535642
264.326426	11015.016268	27.540660
264.542730	11022.552462	27.545677
264.862495	11037.217434	27.550695
265.433569	11045.715929	27.555712
265.195806	11046.248897	27.560730
265.552457	11043.228403	27.565748
265.787410	11060.710405	27.570765
266.129878	11075.484739	27.575783
266.420079	11075.802110	27.580800
266.379897	11073.940449	27.585818
266.738083	11087.082689	27.590836
267.060912	11104.506660	27.595853
267.334239	11119.303077	27.600871
267.335751	11125.739017	27.605888
267.479157	11142.689096	27.610906
268.180877	11151.651260	27.615924
267.832979	11174.871493	27.620941
268.195685	11191.030303	27.625959
268.304868	11211.776405	27.630976
268.626446	11229.869920	27.635994
268.967724	11251.388576	27.641012
269.182313	11272.625026	27.646029
269.340293	11288.444292	27.651047
269.787545	11300.970809	27.656064
269.476543	11333.593225	27.661082
270.079042	11345.031110	27.666100
270.260410	11372.244694	27.671117
270.567233	11389.288044	27.676135
270.778485	11425.443612	27.681152
270.968319	11441.063356	27.686170
271.835161	11457.419731	27.691188
271.989002	11489.374535	27.696205
272.459581	11504.771910	27.701223
272.542793	11521.742240	27.706240
272.532512	11546.048126	27.711258
272.974737	11569.903332	27.716276
273.461862	11598.439286	27.721293
273.455766	11607.776651	27.726311
273.576229	11621.297271	27.731328
273.668855	11654.813524	27.736346
274.851510	11675.768917	27.741364
274.461695	11699.627088	27.746381
274.740861	11726.550041	27.751399
275.888328	11734.289007	27.756416
276.434683	11727.322368	27.761434
276.931376	11727.824471	27.766452
277.139958	11732.304407	27.771469
277.362965	11750.667899	27.776487
277.676833	11753.367188	27.781504
277.608101	11757.786652	27.786522
278.235892	11759.305640	27.791540
278.046770	11766.208681	27.796557
278.388748	11784.239002	27.801575
278.651287	11780.911643	27.806592
278.456426	11803.904190	27.811610
278.811821	11821.326354	27.816628
278.888647	11831.958988	27.821645
278.949097	11853.847548	27.826663
279.289283	11870.900881	27.831680
279.392783	11891.646262	27.836698
280.089825	11893.005464	27.841716
280.176305	11917.357323	27.846733
280.665496	11930.480598	27.851751
280.938949	11947.594243	27.856768
280.903276	11967.239308	27.861786
281.384835	11984.536079	27.866804
281.271862	12006.688436	27.871821
281.685906	12022.761637	27.876839
282.049312	12051.475587	27.881856
281.944680	12068.384379	27.886874
282.608831	12099.880528	27.891892
282.524327	12119.566238	27.896909
282.655416	12140.415592	27.901927
283.287362	12166.486340	27.906944
283.515252	12199.652042	27.911962
283.665913	12221.659184	27.916980
283.993227	12243.446536	27.921997
284.378870	12266.824243	27.927015
284.833792	12292.456664	27.932032
284.909741	12311.819516	27.937050
285.575662	12336.960276	27.942068
285.762510	12362.067047	27.947085
286.504033	12374.959020	27.952103
286.753066	12385.957760	27.957120
287.236474	12409.114073	27.962138
287.379358	12419.495531	27.967156
287.957394	12424.990226	27.972173
288.159156	12434.899677	27.977191
288.628769	12430.899631	27.982208
288.534867	12453.727708	27.987226
289.018461	12460.589559	27.992244
288.886626	12481.733564	27.997261
289.292766	12498.727896	28.002279
289.848826	12501.789760	28.007296
289.793668	12520.143226	28.012314
290.135406	12523.797529	28.017332
290.457501	12548.587286	28.022349
290.704042	12555.978530	28.027367
290.936684	12581.963693	28.032384
290.648957	12607.598132	28.037402
291.298647	12632.727213	28.042420
291.628952	12648.779202	28.047437
291.591306	12672.643761	28.052455
292.109279	12697.685319	28.057472
292.042067	12721.975591	28.062490
292.623541	12745.711078	28.067508
292.916326	12784.107030	28.072525
293.349517	12795.877436	28.077543
293.541413	12817.051873	28.082560
293.608491	12846.165626	28.087578
293.715451	12859.223214	28.092596
294.052406	12888.627978	28.097613
294.527510	12913.315915	28.102631
295.239776	12925.008879	28.107648
294.922106	12950.394809	28.112666
295.354653	12963.150669	28.117684
295.719920	12985.408379	28.122701
295.641886	13011.303286	28.127719
296.393031	13025.726188	28.132736
296.457226	13057.978904	28.137754
296.950741	13088.062819	28.142772
297.114015	13109.474437	28.147789
297.229709	13136.417973	28.152807
297.942257	13155.103831	28.157824
298.122259	13179.519181	28.162842
298.673454	13196.173553	28.167860
299.308098	13201.022991	28.172877
300.338022	13208.462374	28.177895
301.195079	13198.037124	28.182912
301.211617	13212.522685	28.187930
302.004685	13190.591693	28.192948
302.346602	13187.859761	28.197965
302.449225	13185.312973	28.202983
302.713221	13184.781191	28.208000
302.512087	13195.040801	28.213018
302.734801	13191.730311	28.218036
303.200247	13190.423335	28.223053
303.002019	13181.488638	28.228071
303.496217	13188.388393	28.233088
303.214792	13206.899775	28.238106
303.614156	13209.577930	28.243124
303.645385	13222.760761	28.248141
303.504517	13242.778363	28.253159
304.108165	13265.042570	28.258176
304.242098	13287.782740	28.263194
304.566599	13310.215387	28.268212
304.880349	13332.915157	28.273229
304.780100	13355.483858	28.278247
305.401271	13379.557514	28.283264
305.043165	13419.334921	28.288282
305.559855	13441.473621	28.293300
305.901543	13469.303019	28.298317
306.616740	13486.511034	28.303335
307.140766	13502.474206	28.308352
307.249073	13538.162169	28.313370
307.834961	13544.835917	28.318388
308.451011	13564.365287	28.323405
308.690566	13579.928336	28.328423
309.234974	13591.524887	28.333440
309.272294	13617.053319	28.338458
309.677420	13630.751554	28.343476
310.211201	13645.512762	28.348493
310.003853	13662.706154	28.353511
310.531230	13676.078334	28.358528
310.739421	13683.082449	28.363546
310.992963	13709.509786	28.368564
310.949531	13724.261228	28.373581
311.129516	13740.103351	28.378599
311.728036	13757.866055	28.383616
311.944041	13779.536182	28.388634
312.271180	13794.303313	28.393652
312.718406	13806.479348	28.398669
312.730999	13831.876484	28.403687
313.116228	13841.222610	28.408704
313.273517	13877.281904	28.413722
313.715280	13889.728099	28.418740
313.959671	13915.852998	28.423757
314.128690	13948.933883	28.428775
314.777602	13958.165435	28.433792
314.957218	13981.354459	28.438810
315.185308	14008.761595	28.443828
315.656205	14020.835136	28.448845
315.671719	14052.904058	28.453863
316.533997	14064.920075	28.458880
316.796844	14085.278861	28.463898
316.856769	14098.134328	28.468916
317.817173	14121.744068	28.473933
317.836442	14154.286112	28.478951
318.378925	14150.984182	28.483968
318.595872	14182.340034	28.488986
318.847983	14192.467946	28.494004
319.513474	14212.980392	28.499021
319.240510	14227.868190	28.504039
319.547592	14248.399333	28.509056
319.703942	14274.183840	28.514074
319.780742	14289.825805	28.519092
320.301151	14316.899493	28.524109
320.688788	14343.589363	28.529127
321.252522	14359.881875	28.534144
321.578445	14387.624240	28.539162
321.651652	14414.875554	28.544180
322.001886	14429.208119	28.549197
322.006408	14460.056289	28.554215
322.221164	14492.276814	28.559232
323.032538	14525.395314	28.564250
323.067249	14540.090705	28.569268
323.737543	14556.442904	28.574285
323.862524	14598.944598	28.579303
324.663975	14602.731512	28.584320
324.846471	14633.909367	28.589338
324.857936	14641.911318	28.594356
325.371354	14667.281185	28.599373
325.689420	14693.383269	28.604391
326.171973	14697.101569	28.609408
326.681884	14729.642406	28.614426
326.644881	14746.358570	28.619444
327.455383	14767.279570	28.624461
327.454793	14790.466951	28.629479
328.014711	14796.559388	28.634496
327.911723	14829.421010	28.639514
328.080988	14845.516430	28.644532
328.495840	14855.663620	28.649549
328.964679	14878.327781	28.654567
329.360815	14901.426809	28.659584
329.841282	14918.806512	28.664602
329.724109	14936.788379	28.669620
330.309134	14951.704370	28.674637
330.172135	14984.930635	28.679655
330.873958	15001.648298	28.684672
331.298176	15012.413376	28.689690
331.281441	15033.555447	28.694708
331.620346	15050.298136	28.699725
331.812912	15073.015375	28.704743
332.194071	15097.860479	28.709760
332.662184	15128.426101	28.714778
332.871074	15146.754504	28.719796
333.481340	15169.066592	28.724813
333.545892	15198.965303	28.729831
333.838816	15216.959190	28.734848
334.150407	15244.274359	28.739866
334.317490	15287.114693	28.744884
335.096588	15308.224086	28.749901
335.420793	15336.774315	28.754919
335.528819	15361.218368	28.759936
335.760095	15396.801502	28.764954
335.987510	15425.906608	28.769972
336.310497	15446.443316	28.774989
336.355926	15484.360249	28.780007
337.161987	15506.556204	28.785024
337.577577	15539.672664	28.790042
337.723047	15569.648652	28.795060
338.468747	15605.021362	28.800077
338.716774	15626.330779	28.805095
338.834100	15652.100001	28.810112
339.132519	15678.431465	28.815130
339.463419	15707.334218	28.820148
340.005039	15733.835060	28.825165
340.124639	15767.256432	28.830183
340.752902	15791.328529	28.835200
341.392238	15820.819066	28.840218
341.218412	15853.113327	28.845236
341.722735	15871.404070	28.850253
342.671150	15896.198833	28.855271
342.674822	15915.395891	28.860288
343.274869	15937.234210	28.865306
343.265543	15967.495059	28.870324
343.457731	15980.331808	28.875341
343.718200	16011.778537	28.880359
344.430893	16039.265318	28.885376
345.363908	16035.023205	28.890394
345.592771	16067.509809	28.895412
345.955339	16071.884608	28.900429
346.544902	16100.998817	28.905447
347.086773	16108.052232	28.910464
347.305145	16107.118327	28.915482
347.263453	16106.272123	28.920500
347.775469	16119.108996	28.925517
347.814936	16137.092096	28.930535
347.899680	16148.124652	28.935552
348.583838	16160.929205	28.940570
348.831230	16173.365233	28.945588
348.581620	16202.100435	28.950605
349.024376	16230.487577	28.955623
349.185840	16247.966767	28.960640
349.852229	16272.907865	28.965658
349.704322	16298.591514	28.970676
350.054037	16311.359147	28.975693
350.446063	16345.718574	28.980711
350.766300	16379.110870	28.985728
351.361543	16399.035828	28.990746
351.389455	16430.212824	28.995764
351.937599	16454.920132	29.000781
352.462070	16484.055280	29.005799
352.264208	16516.988954	29.010816
352.866504	16537.337341	29.015834
353.189115	16576.388471	29.020852
353.562612	16591.363984	29.025869
353.708474	16629.409442	29.030887
353.885683	16670.515914	29.035904
354.480623	16696.471963	29.040922
354.654547	16743.173826	29.045940
355.227936	16772.193265	29.050957
355.342411	16799.225991	29.055975
355.572560	16843.974640	29.060992
356.283117	16868.632515	29.066010
356.446026	16914.764835	29.071028
358.017478	16921.185282	29.076045
358.272610	16950.284711	29.081063
358.371312	16970.391504	29.086080
359.298936	16987.415984	29.091098
359.232687	17013.905869	29.096116
359.777064	17025.874804	29.101133
359.971505	17053.217260	29.106151
360.484094	17073.278699	29.111168
361.110232	17085.922807	29.116186
361.024299	17118.807441	29.121204
361.653402	17133.745502	29.126221
361.927921	17153.213516	29.131239
362.051897	17175.109777	29.136256
362.715974	17177.758568	29.141274
363.097039	17213.372013	29.146292
363.254136	17223.315108	29.151309
363.528676	17250.155008	29.156327
363.899820	17274.907584	29.161344
364.314741	17295.608083	29.166362
364.389978	17324.763261	29.171380
364.864909	17346.414471	29.176397
365.065781	17368.342843	29.181415
365.001795	17398.183319	29.186432
365.787320	17417.237562	29.191450
366.157700	17443.159002	29.196468
366.410719	17463.770570	29.201485
366.913181	17488.731295	29.206503
366.793284	17520.044664	29.211520
367.173707	17551.100808	29.216538
367.136990	17584.019526	29.221556
367.787963	17600.397446	29.226573
368.379562	17637.063337	29.231591
368.239721	17669.612061	29.236608
368.853656	17704.504096	29.241626
369.227440	17740.079754	29.246644
369.535675	17773.231300	29.251661
369.891935	17803.298101	29.256679
370.273643	17842.905405	29.261696
371.097087	17859.435643	29.266714
371.374701	17891.510822	29.271732
371.755274	17921.743664	29.276749
371.805405	17941.466538	29.281767
372.312330	17986.213743	29.286784
372.928946	18011.524052	29.291802
373.118353	18049.609359	29.296820
373.425867	18082.636087	29.301837
374.170168	18126.615935	29.306855
374.444290	18151.042843	29.311872
375.066869	18169.183410	29.316890
375.190949	18205.126310	29.321908
375.708976	18232.457072	29.326925
376.457569	18254.536818	29.331943
376.345950	18287.479195	29.336960
376.936964	18309.060100	29.341978
377.069002	18339.114454	29.346996
377.186912	18363.442177	29.352013
377.676515	18401.787210	29.357031
378.012867	18440.470157	29.362048
378.798969	18456.304202	29.367066
379.165402	18500.597697	29.372084
379.232601	18520.981999	29.377101
379.681559	18553.704103	29.382119
379.930121	18584.812067	29.387136
380.511410	18610.670348	29.392154
380.988178	18646.281275	29.397172
381.195980	18672.549589	29.402189
381.735035	18694.573192	29.407207
382.221182	18726.464490	29.412224
383.395062	18741.874414	29.417242
384.084330	18760.790527	29.422260
384.366341	18767.131418	29.427277
384.596301	18783.887153	29.432295
384.728645	18809.790141	29.437312
385.224229	18823.699474	29.442330
385.491895	18843.145107	29.447348
385.497277	18865.310693	29.452365
385.877859	18881.411779	29.457383
386.301441	18907.601613	29.462400
386.992917	18928.746081	29.467418
387.046271	18944.828113	29.472436
387.180679	18968.226524	29.477453
387.486292	18978.902250	29.482471
387.674528	19014.482040	29.487488
388.370934	19034.951407	29.492506
389.097332	19059.320268	29.497524
389.127271	19090.530620	29.502541
389.070597	19104.964466	29.507559
389.474086	19141.261486	29.512576
390.004289	19163.183612	29.517594
390.485713	19198.578506	29.522612
390.740948	19230.093028	29.527629
391.331376	19252.046631	29.532647
391.109372	19288.792912	29.537664
391.657920	19316.233717	29.542682
392.056534	19358.696785	29.547700
391.966092	19395.306198	29.552717
392.733148	19427.177003	29.557735
393.113549	19457.154952	29.562752
393.812470	19492.977320	29.567770
394.339059	19527.186107	29.572788
394.655836	19554.893818	29.577805
395.265016	19581.767886	29.582823
395.644518	19619.285724	29.587840
395.883273	19644.949491	29.592858
396.660793	19678.886708	29.597876
396.844513	19708.379095	29.602893
397.387772	19735.853768	29.607911
397.644919	19768.810585	29.612928
398.079437	19795.142310	29.617946
398.422207	19818.018569	29.622964
398.420345	19863.497594	29.627981
399.099066	19893.581617	29.632999
399.340125	19936.117821	29.638016
399.496931	19970.623543	29.643034
399.926239	20004.242886	29.648052
400.130096	20043.939637	29.653069
400.805570	20083.275468	29.658087
401.191164	20122.691453	29.663104
402.033270	20150.720504	29.668122
402.341431	20181.644167	29.673140
402.692922	20222.780271	29.678157
403.228595	20244.517189	29.683175
403.347800	20274.942324	29.688192
403.780544	20313.860648	29.693210
403.937896	20349.398775	29.698228
404.226300	20383.744255	29.703245
405.989778	20381.347954	29.708263
407.981191	20372.868677	29.713280
409.467584	20346.889862	29.718298
410.305518	20343.077806	29.723316
410.302596	20330.953496	29.728333
410.740903	20308.432831	29.733351
410.949919	20284.827298	29.738368
411.191231	20280.138518	29.743386
411.112277	20251.215874	29.748404
411.177645	20249.730436	29.753421
411.369651	20242.030945	29.758439
411.279803	20241.949195	29.763456
411.202248	20239.280046	29.768474
411.398355	20242.020891	29.773492
411.292816	20269.415213	29.778509
411.826782	20269.117507	29.783527
411.919533	20298.927125	29.788544
412.069320	20331.141484	29.793562
412.283967	20358.838542	29.798580
412.358927	20394.016613	29.803597
412.912266	20429.755651	29.808615
412.966425	20477.946487	29.813632
413.008600	20515.305227	29.818650
413.761885	20554.661349	29.823668
413.828486	20606.825308	29.828685
414.055828	20659.703330	29.833703
414.307261	20703.837496	29.838720
414.632944	20772.410216	29.843738
415.308342	20812.595297	29.848756
415.463839	20866.387996	29.853773
415.741629	20921.173403	29.858791
416.245339	20984.019911	29.863808
416.966709	21027.966695	29.868826
417.865954	21084.927342	29.873844
418.016097	21139.437722	29.878861
418.501760	21174.125230	29.883879
419.096021	21228.094971	29.888896
419.802664	21277.726351	29.893914
420.456103	21311.129670	29.898932
421.162520	21341.992553	29.903949
421.706183	21367.162025	29.908967
421.952829	21408.705427	29.913984
422.434393	21440.991264	29.919002
423.395573	21470.176420	29.924020
423.371055	21508.658632	29.929037
424.085814	21536.159935	29.934055
424.660186	21567.871270	29.939072
424.515879	21589.836541	29.944090
425.041058	21623.909935	29.949108
425.232202	21660.727051	29.954125
425.849593	21684.019471	29.959143
426.119539	21733.454875	29.964160
426.536599	21770.966353	29.969178
427.538902	21795.260080	29.974196
427.593496	21837.871695	29.979213
428.136446	21865.397011	29.984231
428.393990	21893.533352	29.989248
428.734037	21930.532935	29.994266
429.326855	21959.003475	29.999284
429.872468	21996.693484	30.004301
430.292173	22018.495446	30.009319
430.860532	22061.209315	30.014336
431.329289	22092.595134	30.019354
432.011759	22103.077477	30.024372
432.298025	22123.488650	30.029389
432.902897	22137.421331	30.034407
433.399886	22150.102360	30.039424
433.456070	22176.737008	30.044442
434.184464	22200.322829	30.049460
434.213989	22233.420316	30.054477
434.289854	22260.467046	30.059495
434.438405	22292.129542	30.064512
434.569193	22332.816418	30.069530
435.251134	22368.187294	30.074548
435.303471	22417.309800	30.079565
436.173792	22457.219126	30.084583
436.523847	22487.724378	30.089600
436.866262	22534.742936	30.094618
437.002784	22577.234003	30.099636
437.158251	22624.952110	30.104653
437.868727	22672.016399	30.109671
438.243948	22721.773651	30.114688
438.534057	22774.017840	30.119706
439.350887	22820.974259	30.124724
439.630065	22866.341142	30.129741
439.903214	22915.908900	30.134759
440.692841	22963.376538	30.139776
441.088656	23014.026993	30.144794
442.023456	23041.441514	30.149812
442.770861	23079.484755	30.154829
443.577398	23109.996451	30.159847
444.019428	23128.889899	30.164864
444.417116	23169.932591	30.169882
445.140004	23191.467317	30.174900
445.754700	23222.690344	30.179917
446.224724	23247.921809	30.184935
446.932040	23273.938627	30.189952
447.138917	23296.227598	30.194970
447.352352	23318.452542	30.199988
447.530138	23351.503529	30.205005
447.796777	23372.091940	30.210023
448.626744	23406.021366	30.215040
448.713085	23436.954848	30.220058
449.400682	23458.319121	30.225076
449.279461	23495.243826	30.230093
449.918232	23530.741544	30.235111
450.496543	23567.152453	30.240128
450.742303	23613.215233	30.245146
451.389130	23637.136787	30.250164
451.503144	23681.675303	30.255181
451.575478	23705.451396	30.260199
452.367821	23749.533076	30.265216
452.551021	23797.221924	30.270234
453.341715	23836.406188	30.275252
454.271413	23878.475030	30.280269
454.130483	23918.724817	30.285287
454.578796	23958.388506	30.290304
455.086318	24001.513511	30.295322
455.465384	24030.718958	30.300340
455.557174	24074.383024	30.305357
455.869348	24103.133721	30.310375
456.735404	24143.550538	30.315392
457.251698	24187.589977	30.320410
457.698668	24220.667623	30.325428
458.286877	24250.157601	30.330445
458.626162	24290.289276	30.335463
459.062662	24321.961137	30.340480
459.261430	24371.375915	30.345498
460.052541	24397.036199	30.350516
460.376424	24440.765906	30.355533
460.701652	24473.203352	30.360551
461.698220	24505.977400	30.365568
462.231248	24557.397063	30.370586
462.991796	24578.176173	30.375604
463.344180	24620.695804	30.380621
463.748645	24652.798805	30.385639
464.390886	24680.683431	30.390656
464.328994	24711.619367	30.395674
465.115044	24735.122583	30.400692
465.941938	24770.177163	30.405709
466.374688	24792.759944	30.410727
467.006988	24822.150216	30.415744
467.441326	24850.971026	30.420762
468.035736	24869.900562	30.425780
468.670024	24891.971633	30.430797
468.866391	24917.900033	30.435815
469.177269	24948.664388	30.440832
469.509468	24981.066307	30.445850
469.938890	25001.303181	30.450868
469.904996	25031.778374	30.455885
470.056132	25073.789293	30.460903
470.535699	25109.382066	30.465920
470.705158	25166.828146	30.470938
471.239128	25211.943684	30.475956
471.876347	25256.751425	30.480973
472.334004	25315.061996	30.485991
472.614114	25360.368862	30.491008
472.866927	25414.330025	30.496026
473.191326	25460.416322	30.501044
473.709031	25518.467550	30.506061
474.167159	25574.224201	30.511079
475.043751	25623.552971	30.516096
475.168264	25686.780997	30.521114
475.796781	25736.165391	30.526132
476.172815	25792.893840	30.531149
477.090376	25830.157105	30.536167
478.719688	25858.505743	30.541184
479.007596	25900.044046	30.546202
479.886616	25925.379242	30.551220
480.085923	25955.519667	30.556237
480.257132	25986.268874	30.561255
480.943148	26018.310063	30.566272
481.487830	26047.262768	30.571290
481.719525	26076.473370	30.576308
482.241708	26106.193943	30.581325
482.485427	26128.296646	30.586343
483.173943	26165.824862	30.591360
483.212552	26203.704081	30.596378
483.609091	26226.314349	30.601396
484.075995	26262.041689	30.606413
484.411101	26311.084626	30.611431
485.087317	26348.132292	30.616448
485.041383	26396.847008	30.621466
485.588253	26438.558948	30.626484
486.190179	26488.196482	30.631501
486.118163	26533.844008	30.636519
486.799953	26577.274352	30.641536
486.959819	26640.035663	30.646554
487.692829	26691.036385	30.651572
488.237973	26735.381550	30.656589
488.557390	26791.548986	30.661607
489.231223	26840.883860	30.666624
489.640047	26893.667776	30.671642
490.430624	26943.876215	30.676660
490.909364	26996.888837	30.681677
491.629765	27039.256971	30.686695
492.572467	27081.800948	30.691712
493.361335	27125.984665	30.696730
493.699517	27152.507032	30.701748
494.130651	27198.051065	30.706765
494.976913	27233.676004	30.711783
496.030777	27247.321046	30.716800
497.314803	27252.951462	30.721818
498.341958	27258.948981	30.726836
498.659822	27269.365998	30.731853
498.838362	27292.753093	30.736871
499.387516	27298.382417	30.741888
499.924397	27307.795485	30.746906
500.105365	27326.272222	30.751924
500.656802	27336.474013	30.756941
500.808149	27363.414127	30.761959
501.225109	27380.474550	30.766976
501.070683	27410.865502	30.771994
501.519407	27437.203699	30.777012
501.782726	27470.405547	30.782029
501.940814	27511.824503	30.787047
502.721695	27546.593882	30.792064
502.877778	27594.756081	30.797082
503.353547	27641.851120	30.802100
503.813053	27685.196951	30.807117
503.833120	27735.752788	30.812135
504.522499	27774.620098	30.817152
504.769451	27831.395977	30.822170
505.459474	27880.403685	30.827188
505.746410	27925.364480	30.832205
505.947287	27985.290393	30.837223
506.939399	28040.166054	30.842240
507.613514	28093.543528	30.847258
508.139226	28134.747929	30.852276
508.390464	28181.955945	30.857293
508.773852	28236.957610	30.862311
509.432392	28278.765247	30.867328
510.001733	28319.307618	30.872346
510.239204	28367.627760	30.877364
511.029016	28427.833386	30.882381
511.356853	28468.868448	30.887399
512.008511	28510.012767	30.892416
512.285106	28554.616079	30.897434
512.868610	28611.991906	30.902452
513.476367	28656.700331	30.907469
513.699677	28708.585221	30.912487
514.645148	28756.442313	30.917504
515.583642	28808.706845	30.922522
515.768910	28847.247301	30.927540
516.486730	28890.036732	30.932557
517.023665	28930.962432	30.937575
517.525523	28981.825186	30.942592
517.987180	29032.486482	30.947610
518.707850	29079.002988	30.952628
519.086911	29115.302197	30.957645
519.445926	29163.455628	30.962663
519.917060	29204.089919	30.967680
520.669094	29262.366264	30.972698
520.756441	29309.767556	30.977716
521.382758	29358.514085	30.982733
521.928582	29408.844803	30.987751
522.857781	29455.521433	30.992768
523.516736	29496.812075	30.997786
523.722753	29546.530719	31.002804
524.438353	29585.344606	31.007821
524.641330	29632.265081	31.012839
525.348344	29673.600523	31.017856
526.164124	29723.006662	31.022874
526.803463	29769.350556	31.027892
528.684165	29769.660886	31.032909
530.510605	29764.556904	31.037927
531.512281	29767.572959	31.042944
531.812047	29772.198009	31.047962
532.635103	29764.954502	31.052980
533.295402	29756.745631	31.057997
533.096744	29751.619099	31.063015
533.437661	29752.551368	31.068032
533.650436	29761.188537	31.073050
533.925526	29776.044071	31.078068
534.274471	29779.633748	31.083085
533.970098	29814.286160	31.088103
534.567490	29829.166049	31.093120
534.956784	29857.441927	31.098138
535.153300	29893.187256	31.103156
535.878575	29920.525591	31.108173
536.061999	29966.848114	31.113191
536.212920	30010.555046	31.118208
536.626861	30044.095911	31.123226
537.166312	30084.425228	31.128244
537.300233	30125.493777	31.133261
537.373007	30170.301035	31.138279
538.076291	30215.542255	31.143296
538.584348	30273.194420	31.148314
538.616800	30327.234620	31.153332
539.363085	30375.251137	31.158349
539.471342	30444.092866	31.163367
539.942843	30504.662628	31.168384
540.639639	30572.106174	31.173402
541.359374	30622.704503	31.178420
542.451537	30679.533762	31.183437
543.280161	30725.081096	31.188455
543.936065	30769.303793	31.193472
544.481500	30814.816105	31.198490
544.898951	30868.396436	31.203508
545.664910	30916.297928	31.208525
545.716298	30969.437276	31.213543
546.108688	31016.539592	31.218560
546.796448	31068.090052	31.223578
546.960678	31125.615576	31.228596
547.953801	31189.944193	31.233613
548.134164	31256.988946	31.238631
548.752430	31304.558892	31.243648
549.181630	31375.556830	31.248666
549.380615	31445.263054	31.253684
550.365169	31498.524991	31.258701
550.525648	31564.212368	31.263719
551.204086	31629.306828	31.268736
551.914244	31690.804407	31.273754
552.831519	31739.210636	31.278772
553.737043	31794.932340	31.283789
554.307600	31851.847169	31.288807
555.172980	31903.573709	31.293824
555.719707	31950.909458	31.298842
555.986296	32001.566877	31.303860
557.051448	32048.878650	31.308877
557.391004	32105.692444	31.313895
557.915770	32148.032530	31.318912
558.574225	32189.125135	31.323930
558.691953	32246.122909	31.328948
559.456434	32293.923044	31.333965
559.817172	32341.502330	31.338983
560.489738	32406.927076	31.344000
561.296868	32452.493657	31.349018
561.796943	32505.098340	31.354036
562.301069	32549.715690	31.359053
562.655070	32610.603523	31.364071
563.319535	32666.711772	31.369088
563.723093	32719.829033	31.374106
564.729803	32755.129974	31.379124
565.666891	32808.856100	31.384141
565.946479	32849.116948	31.389159
566.325524	32906.657021	31.394176
566.804642	32944.729965	31.399194
567.028899	32991.634564	31.404212
568.010279	33041.888129	31.409229
568.460081	33089.805318	31.414247
568.503927	33146.985048	31.419264
569.392855	33187.884223	31.424282
569.725141	33245.268983	31.429300
570.199771	33287.690908	31.434317
570.595293	33356.106523	31.439335
571.381662	33414.084751	31.444352
571.949653	33460.808245	31.449370
572.549170	33515.969728	31.454388
573.332623	33561.092304	31.459405
573.860906	33613.645573	31.464423
574.562928	33672.847201	31.469440
574.956094	33719.534638	31.474458
575.682457	33772.127796	31.479476
576.407216	33825.922570	31.484493
576.709074	33874.474068	31.489511
577.341770	33941.159713	31.494528
578.156270	33978.812742	31.499546
578.558023	34041.534709	31.504564
579.146142	34078.193060	31.509581
579.710578	34134.063679	31.514599
580.390431	34196.024673	31.519616
580.962992	34249.474604	31.524634
581.820545	34303.457860	31.529652
582.491755	34352.591950	31.534669
582.773228	34415.378622	31.539687
583.526826	34462.597168	31.544704
583.898643	34508.941830	31.549722
584.422930	34578.119143	31.554740
584.794985	34638.311592	31.559757
585.305299	34687.902667	31.564775
585.597719	34751.407721	31.569792
586.518189	34810.168726	31.574810
586.459604	34870.624505	31.579828
587.535458	34943.495857	31.584845
588.052402	35000.352783	31.589863
588.576650	35064.676556	31.594880
589.904353	35114.846558	31.599898
590.661137	35183.246821	31.604916
592.672007	35184.149928	31.609933
596.013161	35143.021441	31.614951
596.818108	35152.090524	31.619968
597.549490	35150.325036	31.624986
598.012027	35137.726130	31.630004
598.795112	35111.373309	31.635021
599.051021	35102.384398	31.640039
599.486715	35082.282560	31.645056
599.605976	35073.406864	31.650074
599.592481	35086.542752	31.655092
600.085440	35084.687548	31.660109
600.504376	35078.245516	31.665127
600.340849	35105.593717	31.670144
600.771205	35122.001105	31.675162
600.831244	35139.850073	31.680180
600.867365	35165.525445	31.685197
601.202112	35202.636520	31.690215
601.584201	35226.702456	31.695232
602.209366	35267.309823	31.700250
602.382784	35311.660929	31.705268
602.569121	35363.618357	31.710285
603.125484	35413.350875	31.715303
603.423076	35470.939589	31.720320
603.769160	35523.006073	31.725338
604.244915	35585.542337	31.730356
604.843198	35656.399230	31.735373
605.115300	35727.289452	31.740391
605.759924	35811.332192	31.745408
606.865735	35866.241098	31.750426
607.070569	35938.987506	31.755444
607.452512	36005.926295	31.760461
608.188107	36080.644641	31.765479
608.908490	36167.918555	31.770496
609.411360	36233.262399	31.775514
609.808972	36322.185612	31.780532
610.299766	36399.656125	31.785549
611.576153	36470.463641	31.790567
612.398909	36537.949226	31.795584
613.002533	36590.272832	31.800602
613.815958	36659.554597	31.805620
614.500694	36723.050365	31.810637
615.433620	36786.733884	31.815655
615.943015	36854.589129	31.820672
616.774723	36913.496217	31.825690
617.160500	36980.851358	31.830708
617.991367	37041.663643	31.835725
618.337857	37104.300247	31.840743
618.783437	37171.870515	31.845760
619.539417	37235.577606	31.850778
620.156786	37304.815991	31.855796
620.780443	37378.123131	31.860813
621.860690	37427.484913	31.865831
622.307226	37479.416895	31.870848
623.542237	37527.842984	31.875866
624.784964	37578.186856	31.880884
625.670254	37610.985227	31.885901
626.495983	37651.864425	31.890919
627.073683	37691.673201	31.895936
627.813978	37722.380481	31.900954
628.305594	37759.175792	31.905972
628.740068	37792.965551	31.910989
629.469376	37831.684636	31.916007
629.514153	37877.625543	31.921024
630.174017	37919.624493	31.926042
630.460431	37975.720905	31.931060
630.710928	38033.101980	31.936077
631.523153	38088.930550	31.941095
631.779112	38151.014660	31.946112
632.695499	38196.084424	31.951130
633.221944	38251.192725	31.956148
633.816558	38312.379916	31.961165
634.365062	38363.112627	31.966183
634.603899	38424.580784	31.971200
635.126598	38469.311887	31.976218
635.735364	38527.607316	31.981236
636.410164	38602.635074	31.986253
637.220592	38653.829949	31.991271
637.443359	38713.086274	31.996288
638.273711	38776.120329	32.001306
639.062127	38841.529710	32.006324
639.653241	38903.738229	32.011341
640.394457	38970.235763	32.016359
641.295751	39030.853191	32.021376
641.826109	39086.267914	32.026394
642.461173	39141.226198	32.031412
642.952871	39202.701054	32.036429
643.603320	39258.455165	32.041447
643.811662	39341.441708	32.046464
644.111974	39400.631309	32.051482
645.435275	39478.118956	32.056500
645.555287	39547.877777	32.061517
646.283964	39623.541683	32.066535
646.721520	39692.305956	32.071552
647.641730	39763.262841	32.076570
649.628743	39807.204474	32.081588
651.126313	39852.466787	32.086605
652.264627	39886.539715	32.091623
652.377124	39942.980969	32.096640
653.119643	39978.575779	32.101658
653.645617	40013.519175	32.106676
653.938927	40063.581664	32.111693
654.630737	40109.282056	32.116711
654.933916	40162.314251	32.121728
655.729728	40208.026731	32.126746
656.328897	40271.748122	32.131764
656.610030	40319.876779	32.136781
657.318602	40371.100930	32.141799
657.607117	40438.329153	32.146816
658.286731	40501.303713	32.151834
658.775771	40548.983580	32.156852
659.251452	40629.883712	32.161869
660.184798	40687.258033	32.166887
660.050444	40764.855909	32.171904
660.950200	40838.526684	32.176922
662.029714	40913.001824	32.181940
662.335638	40987.244063	32.186957
663.338271	41044.734712	32.191975
663.316965	41125.322058	32.196992
664.092042	41200.061402	32.202010
665.142765	41273.085491	32.207028
665.519095	41352.525563	32.212045
666.118302	41419.973106	32.217063
666.851638	41514.102758	32.222080
667.516643	41564.063128	32.227098
668.250728	41639.148408	32.232116
668.612573	41707.795620	32.237133
669.756087	41763.894166	32.242151
670.217679	41837.780941	32.247168
670.676825	41909.195495	32.252186
671.575969	41970.932415	32.257204
672.299521	42043.472498	32.262221
672.789743	42112.933609	32.267239
673.380740	42182.366336	32.272256
674.186708	42259.843295	32.277274
674.648217	42328.937639	32.282292
674.931153	42404.069702	32.287309
676.008806	42479.696953	32.292327
676.591556	42564.122001	32.297344
677.234514	42636.440833	32.302362
677.916297	42705.567851	32.307380
678.554189	42789.281790	32.312397
680.142974	42842.726342	32.317415
680.861334	42909.611872	32.322432
681.991488	42973.142012	32.327450
683.146266	43037.699971	32.332468
683.874661	43077.664495	32.337485
684.961353	43126.114354	32.342503
685.068594	43181.921975	32.347520
685.806389	43237.329698	32.352538
686.538875	43287.807965	32.357556
686.937954	43345.866118	32.362573
687.702339	43412.926074	32.367591
687.949602	43475.399925	32.372608
688.646331	43545.458507	32.377626
689.064619	43605.949779	32.382644
689.463756	43667.024751	32.387661
690.399096	43719.247996	32.392679
691.269102	43801.860470	32.397696
691.590624	43879.169452	32.402714
692.235430	43949.427208	32.407732
692.868192	44025.576859	32.412749
693.410636	44097.637034	32.417767
694.223589	44177.093115	32.422784
694.348803	44261.936830	32.427802
695.636822	44342.381149	32.432820
696.249576	44418.583026	32.437837
697.605339	44487.284901	32.442855
698.033323	44553.532123	32.447872
698.400952	44638.285441	32.452890
699.348671	44708.327674	32.457908
700.530307	44786.835041	32.462925
701.315806	44852.941298	32.467943
702.029105	44925.211145	32.472960
702.387284	44987.827346	32.477978
702.828104	45059.999169	32.482996
703.590494	45138.887201	32.488013
704.421319	45201.258551	32.493031
705.630431	45266.645875	32.498048
706.282849	45327.339306	32.503066
706.902564	45385.037867	32.508084
707.370440	45461.371476	32.513101
707.953250	45511.936819	32.518119
708.699837	45575.250457	32.523136
709.589778	45640.838282	32.528154
710.341938	45698.813354	32.533172
710.701157	45764.221128	32.538189
711.474344	45833.623663	32.543207
712.083405	45900.086934	32.548224
712.129870	45974.454919	32.553242
713.086607	46050.157980	32.558260
713.534486	46129.624283	32.563277
714.519817	46202.206299	32.568295
715.092432	46279.400734	32.573312
715.502913	46358.044249	32.578330
716.428982	46436.975169	32.583348
716.899673	46525.794399	32.588365
717.417161	46604.302085	32.593383
718.458209	46695.145273	32.598400
718.857923	46788.883328	32.603418
720.018943	46867.378071	32.608436
720.374350	46957.773319	32.613453
721.222032	47034.346722	32.618471
722.022130	47129.234425	32.623488
722.983341	47205.077423	32.628506
724.262130	47271.514974	32.633524
724.782350	47353.969583	32.638541
725.892976	47434.705627	32.643559
727.218072	47503.367438	32.648576
728.003983	47551.177021	32.653594
729.012533	47606.684861	32.658612
729.470326	47686.680384	32.663629
730.256837	47741.640271	32.668647
731.289768	47802.281670	32.673664
732.202484	47853.394424	32.678682
733.448758	47893.798688	32.683700
733.596254	47963.514336	32.688717
734.853542	48011.985316	32.693735
736.353893	48037.238515	32.698752
737.120067	48069.279059	32.703770
738.074782	48106.287738	32.708788
738.755601	48142.759512	32.713805
739.353414	48182.567188	32.718823
740.107643	48217.891495	32.723840
740.356114	48260.777821	32.728858
740.937774	48300.954360	32.733876
741.197548	48350.834620	32.738893
741.552845	48399.447113	32.743911
742.114849	48447.771242	32.748928
742.363146	48525.557249	32.753946
743.187036	48592.643337	32.758964
743.596923	48663.061493	32.763981
744.264132	48733.804995	32.768999
745.261749	48800.507644	32.774016
745.801035	48871.527655	32.779034
746.792217	48920.169715	32.784052
747.270858	48991.562745	32.789069
747.816477	49054.857771	32.794087
748.720651	49115.382174	32.799104
749.312132	49188.354733	32.804122
749.847687	49263.819926	32.809140
750.534971	49338.210476	32.814157
750.897862	49405.663340	32.819175
751.548910	49491.676040	32.824192
752.123398	49582.996479	32.829210
753.427510	49660.985414	32.834228
753.847445	49744.682022	32.839245
754.496894	49831.905232	32.844263
755.268265	49915.609805	32.849280
755.757066	50011.240962	32.854298
756.638022	50103.941653	32.859316
757.503935	50175.533382	32.864333
759.717890	50231.346685	32.869351
760.956116	50294.245522	32.874368
762.027576	50360.591976	32.879386
762.900105	50409.843973	32.884404
763.321083	50473.457363	32.889421
764.432496	50528.159562	32.894439
765.227361	50582.546249	32.899456
765.420894	50638.243817	32.904474
766.418924	50687.258850	32.909492
767.059138	50754.559048	32.914509
767.517864	50827.180740	32.919527
768.400168	50892.606217	32.924544
768.661266	50962.220828	32.929562
769.707732	51031.900037	32.934580
770.043530	51111.422266	32.939597
770.604559	51189.252141	32.944615
771.237110	51268.816191	32.949632
771.700539	51360.933427	32.954650
772.479445	51440.187746	32.959668
773.191029	51533.623421	32.964685
773.987177	51627.592103	32.969703
774.512803	51713.938418	32.974720
774.970919	51811.651235	32.979738
776.021879	51900.581650	32.984756
776.611606	51998.066228	32.989773
777.901856	52091.258030	32.994791
780.038925	52142.241843	32.999808
780.814305	52225.681981	33.004826
781.655087	52297.873215	33.009844
782.095570	52366.057074	33.014861
782.979455	52440.997306	33.019879
783.609334	52510.480290	33.024896
784.062953	52603.309252	33.029914
784.961776	52678.525833	33.034932
785.918611	52755.551453	33.039949
786.120013	52839.590784	33.044967
787.203024	52913.507077	33.049984
787.727403	52984.511031	33.055002
788.771635	53051.013786	33.060020
789.837904	53114.451721	33.065037
790.485032	53177.031817	33.070055
791.381077	53238.587752	33.075072
791.902328	53313.122197	33.080090
792.744560	53380.138071	33.085108
793.394800	53457.821492	33.090125
793.550794	53536.448752	33.095143
794.862941	53620.854621	33.100160
795.085445	53701.406838	33.105178
796.353469	53769.173865	33.110196
797.522688	53840.665607	33.115213
798.141157	53928.169252	33.120231
799.081079	54002.516783	33.125248
799.356963	54088.813174	33.130266
800.075254	54167.378904	33.135284
801.148885	54248.883872	33.140301
801.557394	54344.588651	33.145319
802.910074	54420.295748	33.150336
803.477488	54501.677256	33.155354
804.089518	54590.943271	33.160372
804.971209	54672.540660	33.165389
805.891747	54746.019958	33.170407
806.745732	54834.967722	33.175424
807.667027	54924.643839	33.180442
808.399093	55013.965415	33.185460
809.352073	55091.538171	33.190477
809.438020	55184.767113	33.195495
810.707912	55265.393102	33.200512
811.904805	55357.028766	33.205530
812.573567	55450.734485	33.210548
812.975199	55527.841283	33.215565
813.827392	55625.148856	33.220583
815.496258	55699.646121	33.225600
816.395976	55786.845584	33.230618
817.231537	55864.222493	33.235636
818.305224	55941.536572	33.240653
818.807443	56018.481054	33.245671
819.675269	56086.595036	33.250688
820.268381	56181.137284	33.255706
820.826925	56256.283906	33.260724
821.624475	56343.653801	33.265741
822.210239	56444.395371	33.270759
823.234391	56516.387890	33.275776
823.458360	56623.274395	33.280794
824.192222	56716.209092	33.285812
825.195844	56808.195295	33.290829
825.944315	56904.380202	33.295847
827.371197	56998.004707	33.300864
828.154812	57092.941180	33.305882
828.915704	57183.329445	33.310900
830.600033	57237.793384	33.315917
831.787495	57322.968604	33.320935
832.916877	57381.682184	33.325952
833.429932	57461.484874	33.330970
833.893772	57518.704226	33.335988
834.753245	57587.876372	33.341005
835.461564	57659.588985	33.346023
836.375006	57728.074305	33.351040
836.745609	57799.099307	33.356058
837.554620	57872.356300	33.361076
838.180831	57950.302519	33.366093
838.598386	58036.216040	33.371111
839.771950	58112.241552	33.376128
840.030268	58203.033657	33.381146
840.777676	58297.255934	33.386164
841.459109	58391.811219	33.391181
842.215949	58497.749198	33.396199
842.782487	58585.693705	33.401216
843.573281	58685.376128	33.406234
844.623859	58805.476510	33.411252
845.375593	58900.613592	33.416269
846.215230	59011.722343	33.421287
847.572146	59102.782839	33.426304
848.661710	59199.762043	33.431322
849.118857	59296.918181	33.436340
850.248706	59396.626221	33.441357
851.237520	59486.616861	33.446375
852.331629	59578.615038	33.451392
853.301543	59665.082787	33.456410
854.724102	59745.925065	33.461428
855.837564	59832.784361	33.466445
856.561853	59921.335223	33.471463
857.455239	59987.021965	33.476480
858.534555	60071.807068	33.481498
860.169465	60139.845443	33.486516
861.499582	60188.179539	33.491533
862.056958	60250.532738	33.496551
862.980802	60320.882538	33.501568
863.992457	60385.702498	33.506586
864.496491	60450.284565	33.511604
865.342573	60526.450994	33.516621
865.678526	60601.218043	33.521639
866.534017	60663.139951	33.526656
867.145124	60746.247038	33.531674
867.404245	60826.638173	33.536692
868.125663	60917.786557	33.541709
868.704615	61016.201571	33.546727
869.385098	61113.056871	33.551744
869.989746	61215.257966	33.556762
870.559089	61321.437549	33.561780
871.801322	61420.769034	33.566797
872.426233	61536.237136	33.571815
873.226364	61636.922139	33.576832
874.507123	61742.918246	33.581850
874.871561	61847.611382	33.586868
876.161166	61953.228335	33.591885
876.650226	62064.720420	33.596903
877.644302	62173.676031	33.601920
878.283382	62282.581402	33.606938
879.165843	62388.581364	33.611956
879.903811	62493.142835	33.616973
880.776991	62597.746521	33.621991
882.107535	62688.478095	33.627008
883.107800	62781.934239	33.632026
883.492216	62893.545746	33.637044
884.414589	62989.892162	33.642061
885.350213	63103.318248	33.647079
886.122658	63210.177163	33.652096
887.119614	63315.507226	33.657114
888.033879	63430.372383	33.662132
889.233669	63532.371264	33.667149
889.786406	63644.664625	33.672167
890.649905	63745.473902	33.677184
891.965757	63862.339959	33.682202
892.164571	63979.716098	33.687220
893.051318	64080.615031	33.692237
894.059070	64198.773314	33.697255
894.757827	64321.406057	33.702272
895.830385	64441.071432	33.707290
896.451297	64555.367886	33.712308
897.557787	64671.937447	33.717325
898.381347	64786.910470	33.722343
899.696640	64910.323696	33.727360
901.141802	65011.583986	33.732378
901.768149	65128.213783	33.737396
902.873151	65239.680106	33.742413
903.586988	65359.976799	33.747431
904.906116	65462.184911	33.752448
905.902729	65564.555433	33.757466
906.484556	65674.998959	33.762484
907.873449	65778.666292	33.767501
908.366281	65890.224331	33.772519
908.986126	66001.285881	33.777536
910.336489	66111.363251	33.782554
911.352511	66222.164047	33.787572
912.239095	66330.955180	33.792589
912.982381	66437.059747	33.797607
914.398589	66545.271925	33.802624
915.163241	66641.933444	33.807642
916.336672	66750.216990	33.812660
917.459590	66837.214199	33.817677
919.113913	66927.153147	33.822695
919.870948	67016.824683	33.827712
921.294256	67100.774625	33.832730
921.778996	67191.861133	33.837748
922.733467	67272.835209	33.842765
923.784472	67350.604038	33.847783
925.065464	67427.938593	33.852800
926.141763	67506.424196	33.857818
927.070064	67586.228724	33.862836
927.929646	67664.888435	33.867853
928.962787	67749.970917	33.872871
929.784371	67828.011913	33.877888
930.658181	67899.386315	33.882906
930.860509	67977.501180	33.887924
931.624282	68058.932153	33.892941
932.201476	68140.052009	33.897959
933.023247	68213.507995	33.902976
934.119176	68300.130694	33.907994
934.935888	68403.565155	33.913012
936.061557	68478.597411	33.918029
936.532276	68571.821656	33.923047
937.445780	68666.113076	33.928064
938.515862	68760.992855	33.933082
939.011619	68857.171176	33.938100
939.472532	68962.175156	33.943117
940.583318	69072.206370	33.948135
940.929216	69187.363663	33.953152
942.214619	69300.394634	33.958170
942.847344	69419.462660	33.963188
943.761530	69527.657603	33.968205
944.596342	69653.316135	33.973223
945.411274	69781.853350	33.978240
946.642250	69895.667217	33.983258
947.515943	70020.045651	33.988276
948.325586	70141.143294	33.993293
949.271052	70262.706573	33.998311
950.259927	70384.162602	34.003328
951.542597	70502.103891	34.008346
952.301039	70639.501305	34.013364
953.494272	70754.861502	34.018381
954.348626	70877.649879	34.023399
955.258048	71011.158989	34.028416
956.689011	71124.379474	34.033434
957.798987	71256.316617	34.038452
958.896151	71364.321935	34.043469
960.156310	71475.006270	34.048487
961.228091	71585.575868	34.053504
962.531803	71687.913865	34.058522
963.676615	71790.688390	34.063540
965.351200	71873.146577	34.068557
966.714264	71950.043621	34.073575
967.885344	72034.137006	34.078592
969.313569	72117.652736	34.083610
970.207139	72197.298297	34.088628
970.857438	72285.014152	34.093645
971.642886	72361.240114	34.098663
972.488731	72439.504086	34.103680
973.216759	72531.505519	34.108698
973.916246	72637.021873	34.113716
974.449194	72715.488368	34.118733
975.376502	72816.552447	34.123751
975.851716	72927.989039	34.128768
977.094706	73030.874420	34.133786
977.616068	73143.644521	34.138804
978.467293	73259.042102	34.143821
979.182352	73381.280435	34.148839
979.764820	73498.125018	34.153856
980.876825	73618.633365	34.158874
981.436743	73736.203323	34.163892
982.447457	73857.184211	34.168909
983.102775	73973.950464	34.173927
984.108190	74095.546614	34.178944
985.118471	74217.218561	34.183962
985.803415	74340.541841	34.188980
986.683637	74466.615409	34.193997
987.752411	74593.866809	34.199015
988.617598	74734.068727	34.204032
989.700115	74869.023311	34.209050
990.450309	75014.958462	34.214068
991.568490	75142.369779	34.219085
992.863398	75272.161626	34.224103
993.456361	75406.047486	34.229120
995.070195	75527.871478	34.234138
996.639335	75660.440858	34.239156
997.973970	75789.604038	34.244173
999.246918	75895.147387	34.249191
1000.178058	76010.522750	34.254208
1001.296503	76122.178053	34.259226
1002.382457	76240.323563	34.264244
1003.645241	76346.464971	34.269261
1005.462854	76436.086238	34.274279
1006.803617	76528.223359	34.279296
1008.243436	76602.281961	34.284314
1009.597757	76692.508969	34.289332
1011.258645	76759.460628	34.294349
1012.374117	76837.970597	34.299367
1013.048432	76916.291921	34.304384
1014.261579	76991.215968	34.309402
1014.892383	77066.694323	34.314420
1015.700572	77141.733912	34.319437
1016.714667	77223.320562	34.324455
1017.434935	77308.272510	34.329472
1018.197865	77394.279862	34.334490
1019.208059	77483.048216	34.339508
1019.502962	77575.463916	34.344525
1020.740420	77674.998713	34.349543
1021.202235	77779.758094	34.354560
1022.151769	77876.192028	34.359578
1023.129820	77993.878194	34.364596
1024.599975	78089.181081	34.369613
1026.111912	78182.556273	34.374631
1027.155196	78277.062010	34.379648
1028.446442	78367.723638	34.384666
1029.284953	78465.126122	34.389684
1029.987085	78554.738233	34.394701
1031.125572	78655.646200	34.399719
1031.922298	78764.326825	34.404736
1032.897735	78853.865159	34.409754
1033.781111	78959.568526	34.414772
1034.847363	79059.655603	34.419789
1036.149557	79154.301178	34.424807
1036.867611	79266.334459	34.429824
1037.845696	79360.596390	34.434842
1038.919598	79455.342876	34.439860
1040.087440	79545.985089	34.444877
1041.118021	79641.320866	34.449895
1042.122580	79733.329961	34.454912
1042.790238	79812.687440	34.459930
1043.785106	79924.357875	34.464948
1044.948320	80013.403605	34.469965
1046.618240	80090.914940	34.474983
1047.388164	80185.194787	34.480000
1048.349267	80279.899789	34.485018
1049.320352	80379.325702	34.490036
1049.778716	80485.148738	34.495053
1050.728584	80586.367977	34.500071
1051.572747	80705.810362	34.505088
1052.650313	80813.161188	34.510106
1053.418549	80942.288917	34.515124
1054.202164	81063.000973	34.520141
1055.099675	81185.332910	34.525159
1055.807041	81326.749294	34.530176
1056.584277	81455.290856	34.535194
1057.659416	81602.959667	34.540212
1058.525262	81747.274337	34.545229
1059.345693	81883.543212	34.550247
1059.889555	82042.135257	34.555264
1061.106497	82188.862656	34.560282
1062.397766	82357.510175	34.565300
1062.928406	82506.403608	34.570317
1063.943839	82660.316564	34.575335
1064.824557	82833.003466	34.580352
1066.306397	82992.553538	34.585370
1067.175956	83161.097569	34.590388
1068.085331	83330.079174	34.595405
1069.555973	83490.538886	34.600423
1070.296220	83669.065192	34.605440
1071.312801	83841.176053	34.610458
1072.602033	84011.221756	34.615476
1073.349626	84190.427799	34.620493
1075.044942	84365.191581	34.625511
1076.042432	84547.073276	34.630528
1077.065219	84710.477634	34.635546
1078.189012	84868.410671	34.640564
1079.355196	85045.211620	34.645581
1080.785987	85213.562588	34.650599
1081.801249	85385.332109	34.655616
1083.562688	85542.549085	34.660634
1084.717199	85699.294693	34.665652
1085.586367	85855.005602	34.670669
1087.366243	86004.831450	34.675687
1088.663069	86148.753527	34.680704
1090.106424	86290.174593	34.685722
1091.416120	86425.180851	34.690740
1092.920410	86557.412730	34.695757
1093.985835	86688.678214	34.700775
1094.959945	86828.103440	34.705792
1096.253211	86955.217846	34.710810
1097.209375	87072.876264	34.715828
1098.369997	87194.518171	34.720845
1099.609274	87299.934945	34.725863
1100.911085	87411.697382	34.730880
1101.889462	87523.657283	34.735898
1102.822312	87630.199410	34.740916
1103.877825	87750.571178	34.745933
1106.031915	87836.709953	34.750951
1107.225261	87936.800036	34.755968
1108.642001	88030.815961	34.760986
1109.653124	88129.841930	34.766004
1110.121759	88227.917547	34.771021
1111.551626	88331.241202	34.776039
1112.376893	88445.241189	34.781056
1113.196206	88560.210266	34.786074
1113.897851	88674.250091	34.791092
1114.567714	88801.101425	34.796109
1115.821513	88918.248274	34.801127
1116.319199	89050.484805	34.806144
1117.207345	89180.895645	34.811162
1118.522053	89323.008446	34.816180
1119.345163	89471.360010	34.821197
1120.427788	89620.329018	34.826215
1121.024369	89767.105972	34.831232
1122.082250	89914.518856	34.836250
1123.264007	90070.235743	34.841268
1124.289084	90233.270571	34.846285
1125.388459	90387.940341	34.851303
1125.926056	90557.145451	34.856320
1127.241041	90725.652703	34.861338
1128.741711	90877.055613	34.866356
1129.788822	91047.713995	34.871373
1131.498212	91204.202513	34.876391
1132.708336	91364.218467	34.881408
1134.195049	91514.540156	34.886426
1135.927306	91640.815245	34.891444
1137.057815	91781.347850	34.896461
1138.602613	91918.172390	34.901479
1139.867463	92059.887113	34.906496
1141.028156	92186.996236	34.911514
1142.491979	92311.983318	34.916532
1143.340264	92464.626728	34.921549
1144.759966	92581.450533	34.926567
1145.834937	92715.072069	34.931584
1146.751318	92852.040280	34.936602
1147.932214	92992.060236	34.941620
1148.867134	93134.460490	34.946637
1150.544209	93258.425953	34.951655
1151.261982	93394.891456	34.956672
1151.956116	93524.998365	34.961690
1153.317549	93645.891518	34.966708
1154.529312	93802.515512	34.971725
1155.640890	93940.357574	34.976743
1156.712817	94086.183116	34.981760
1157.836088	94216.263762	34.986778
1158.876153	94346.497557	34.991796
1159.495018	94478.431073	34.996813
1160.550926	94611.978458	35.001831
1161.539956	94766.221938	35.006848
1162.155722	94916.521713	35.011866
1163.540206	95050.430622	35.016884
1164.372250	95213.026716	35.021901
1165.675103	95352.782717	35.026919
1166.646311	95519.204950	35.031936
1167.860314	95673.880663	35.036954
1169.017239	95837.504992	35.041972
1169.747587	95999.762357	35.046989
1171.210708	96153.629977	35.052007
1172.473569	96318.727550	35.057024
1173.084969	96488.143087	35.062042
1174.511214	96653.894010	35.067060
1175.956135	96831.080881	35.072077
1177.166369	96999.057531	35.077095
1178.353479	97160.516728	35.082112
1179.483151	97337.669113	35.087130
1180.818152	97498.455580	35.092148
1182.089496	97663.884227	35.097165
1183.790250	97826.493788	35.102183
1185.293721	97992.697692	35.107200
1186.736346	98148.119417	35.112218
1188.010879	98288.334544	35.117236
1189.274748	98449.069426	35.122253
1191.480748	98582.855914	35.127271
1193.026080	98711.218717	35.132288
1194.218207	98841.732549	35.137306
1195.678130	98972.343729	35.142324
1196.745517	99111.938852	35.147341
1198.201904	99228.715353	35.152359
1199.597865	99354.536816	35.157376
1200.536885	99480.792258	35.162394
1201.953851	99600.272174	35.167412
1202.557778	99735.952483	35.172429
1203.478883	99866.426646	35.177447
1204.824914	100006.552313	35.182464
1205.536297	100138.314113	35.187482
1207.080988	100283.427243	35.192500
1207.981160	100425.809201	35.197517
1209.031398	100562.385116	35.202535
1210.729032	100684.976956	35.207552
1212.895944	100805.938321	35.212570
1214.820224	100924.066309	35.217588
1215.982287	101031.559648	35.222605
1216.975792	101151.791936	35.227623
1218.065365	101290.947445	35.232640
1218.748705	101405.738187	35.237658
1219.862391	101527.623745	35.242676
1220.828468	101658.429863	35.247693
1221.951028	101789.863567	35.252711
1223.039053	101917.158949	35.257728
1223.817914	102054.223371	35.262746
1224.799771	102182.271078	35.267764
1225.476536	102315.151712	35.272781
1226.605074	102454.352250	35.277799
1227.398724	102592.632388	35.282816
1228.887054	102744.724007	35.287834
1230.442657	102878.088217	35.292852
1231.294084	103025.075124	35.297869
1232.464040	103174.847201	35.302887
1233.732769	103325.193025	35.307904
1234.219373	103479.366032	35.312922
1235.671952	103636.714998	35.317940
1237.000520	103805.696733	35.322957
1237.774688	103968.635881	35.327975
1239.016009	104124.591531	35.332992
1240.414568	104305.525920	35.338010
1242.250910	104454.485070	35.343028
1243.650921	104622.100700	35.348045
1244.890382	104780.965646	35.353063
1246.280251	104944.750198	35.358080
1246.889153	105117.323646	35.363098
1248.316631	105271.339718	35.368116
1249.301491	105437.976575	35.373133
1250.686519	105613.518523	35.378151
1252.075747	105782.099640	35.383168
1253.253002	105950.918162	35.388186
1254.654346	106130.366080	35.393204
1255.407810	106309.956318	35.398221
1256.855805	106481.463215	35.403239
1258.096278	106654.523248	35.408256
1259.382508	106831.532795	35.413274
1260.776020	107010.539182	35.418292
1262.070170	107191.733530	35.423309
1263.169548	107364.460344	35.428327
1264.341710	107548.613425	35.433344
1265.486584	107732.531740	35.438362
1266.807804	107918.113300	35.443380
1268.306466	108101.224999	35.448397
1269.555946	108299.934995	35.453415
1271.118128	108478.127939	35.458432
1272.239589	108656.018824	35.463450
1273.731712	108840.447307	35.468468
1275.235906	109007.235121	35.473485
1276.720926	109179.508455	35.478503
1278.350181	109351.215735	35.483520
1279.153477	109536.885646	35.488538
1280.686687	109714.452943	35.493556
1281.704672	109900.237057	35.498573
1282.761706	110077.167429	35.503591
1284.103981	110257.218608	35.508608
1285.099376	110433.186558	35.513626
1286.697520	110609.977772	35.518644
1287.945752	110797.213243	35.523661
1288.903126	110993.579847	35.528679
1290.236568	111165.384815	35.533696
1291.333316	111354.294387	35.538714
1292.993184	111527.113421	35.543732
1293.998041	111705.006941	35.548749
1295.114366	111873.622972	35.553767
1296.592106	112047.360809	35.558784
1297.418556	112218.019276	35.563802
1298.315829	112398.131458	35.568820
1299.749000	112589.775948	35.573837
1300.969274	112774.245427	35.578855
1302.481051	112964.835784	35.583872
1303.613770	113158.418874	35.588890
1305.192410	113328.490568	35.593908
1307.219407	113496.225794	35.598925
1308.618454	113681.350912	35.603943
1310.175423	113843.984730	35.608960
1311.474023	114026.703713	35.613978
1313.216221	114194.444565	35.618996
1315.136555	114352.560726	35.624013
1317.025794	114500.692763	35.629031
1319.031977	114632.549404	35.634048
1320.539903	114775.894228	35.639066
1321.939812	114922.055312	35.644084
1322.959647	115061.478188	35.649101
1324.188952	115213.986392	35.654119
1325.282770	115348.802772	35.659136
1326.607079	115494.675287	35.664154
1327.858930	115650.968523	35.669172
1329.101330	115796.134041	35.674189
1330.212052	115955.098003	35.679207
1331.546813	116105.714430	35.684224
1332.587322	116270.465607	35.689242
1333.774661	116427.691897	35.694260
1334.777979	116597.262892	35.699277
1335.677514	116776.247305	35.704295
1337.307370	116938.294236	35.709312
1338.463067	117122.413136	35.714330
1339.315472	117289.606733	35.719348
1340.526510	117473.149512	35.724365
1341.804441	117662.210471	35.729383
1343.274690	117845.049879	35.734400
1344.753213	118036.500394	35.739418
1346.246614	118219.104500	35.744436
1347.698821	118408.238199	35.749453
1348.849671	118597.991046	35.754471
1350.396403	118766.964407	35.759488
1351.368947	118964.739124	35.764506
1352.763736	119163.303049	35.769524
1354.091614	119343.984802	35.774541
1355.253686	119537.332985	35.779559
1356.909981	119716.876006	35.784576
1358.085262	119921.939364	35.789594
1359.509473	120115.807395	35.794612
1361.100154	120305.382457	35.799629
1362.254433	120500.081437	35.804647
1363.697315	120694.938624	35.809664
1365.156020	120885.108764	35.814682
1366.691833	121047.949857	35.819700
1368.478948	121213.436989	35.824717
1370.038170	121375.668471	35.829735
1371.574138	121524.694934	35.834752
1372.990852	121690.395913	35.839770
1374.096326	121850.473358	35.844788
1375.622832	122017.640773	35.849805
1376.819501	122186.229532	35.854823
1377.963375	122339.755804	35.859840
1378.759179	122528.523270	35.864858
1380.078828	122704.707793	35.869876
1381.418401	122886.146606	35.874893
1382.303211	123064.999103	35.879911
1384.018855	123253.980154	35.884928
1385.135225	123454.254554	35.889946
1386.122375	123652.093761	35.894964
1387.555872	123852.282736	35.899981
1388.567840	124063.509225	35.904999
1390.182009	124267.789135	35.910016
1391.565467	124481.100485	35.915034
1392.901381	124695.003743	35.920052
1394.468736	124894.482532	35.925069
1395.594302	125117.023257	35.930087
1397.115747	125328.938690	35.935104
1398.285737	125546.358449	35.940122
1399.835339	125760.413503	35.945140
1401.576250	125966.180818	35.950157
1402.609585	126201.158948	35.955175
1404.460302	126411.535747	35.960192
1405.956873	126626.505420	35.965210
1407.093969	126847.905721	35.970228
1408.363472	127066.981243	35.975245
1409.998926	127280.439186	35.980263
1412.498670	127486.578729	35.985280
1414.173801	127694.079666	35.990298
1415.312099	127893.889268	35.995316
1417.138842	128083.697059	36.000333
1418.248021	128294.725533	36.005351
1419.734069	128499.792263	36.010368
1421.326261	128704.438252	36.015386
1422.841898	128903.270380	36.020404
1424.086456	129096.370110	36.025421
1425.247129	129306.561965	36.030439
1427.053529	129503.793926	36.035456
1428.106472	129705.682491	36.040474
1429.668820	129916.549907	36.045492
1431.386234	130125.620596	36.050509
1432.406488	130337.312136	36.055527
1433.969066	130540.455998	36.060544
1435.426139	130746.202650	36.065562
1436.822331	130953.455481	36.070580
1437.976399	131167.627893	36.075597
1439.258283	131379.019629	36.080615
1440.631905	131586.964860	36.085632
1441.830080	131803.377626	36.090650
1443.227545	132016.276136	36.095668
1444.844935	132207.462842	36.100685
1445.986396	132411.016491	36.105703
1447.459450	132613.910731	36.110720
1448.942237	132807.061398	36.115738
1450.277980	133022.207213	36.120756
1451.867515	133227.139907	36.125773
1453.040357	133448.536025	36.130791
1454.728904	133655.217260	36.135808
1455.666649	133870.369330	36.140826
1457.229684	134084.473331	36.145844
1459.024969	134296.780754	36.150861
1460.266930	134518.642947	36.155879
1461.618663	134738.981531	36.160896
1463.344086	134961.479882	36.165914
1464.729000	135183.831306	36.170932
1466.786808	135387.184384	36.175949
1468.470869	135599.709105	36.180967
1470.178428	135808.379470	36.185984
1471.808671	136021.055204	36.191002
1472.909505	136231.218886	36.196020
1474.503265	136441.394457	36.201037
1475.808526	136663.364312	36.206055
1477.297047	136865.766370	36.211072
1478.642863	137092.877892	36.216090
1480.378626	137296.346106	36.221108
1482.396845	137519.032830	36.226125
1483.454149	137736.842950	36.231143
1484.996645	137946.543185	36.236160
1487.097755	138148.856709	36.241178
1488.578073	138367.630735	36.246196
1490.572731	138560.294692	36.251213
1491.823593	138767.309736	36.256231
1493.285419	138971.897503	36.261248
1494.649104	139179.049552	36.266266
1496.437339	139380.483354	36.271284
1498.288241	139571.592539	36.276301
1499.293509	139783.875014	36.281319
1501.152317	139963.072515	36.286336
1504.625678	140128.035721	36.291354
1506.365955	140306.557066	36.296372
1508.029326	140460.441508	36.301389
1510.034550	140623.879069	36.306407
1511.265630	140786.528002	36.311424
1512.876521	140945.378691	36.316442
1513.762976	141110.821663	36.321460
1515.079789	141265.551046	36.326477
1516.018989	141443.167113	36.331495
1517.631669	141619.929443	36.336512
1518.489194	141805.621324	36.341530
1519.550416	141993.728101	36.346548
1521.221777	142178.697261	36.351565
1522.636334	142369.589263	36.356583
1523.740284	142569.530686	36.361600
1525.255105	142760.345820	36.366618
1526.179138	142953.600809	36.371636
1527.619807	143137.991349	36.376653
1528.571082	143336.035452	36.381671
1530.132259	143523.273656	36.386688
1531.685597	143728.018356	36.391706
1532.853396	143935.867673	36.396724
1534.098217	144136.532023	36.401741
1535.289328	144359.489229	36.406759
1536.433006	144566.611434	36.411776
1538.887523	144790.993453	36.416794
1540.217353	145012.893913	36.421812
1542.620027	145207.677249	36.426829
1544.027308	145423.040400	36.431847
1545.462862	145634.166842	36.436864
1547.341573	145835.894899	36.441882
1548.436247	146067.663938	36.446900
1550.199203	146279.959588	36.451917
1551.499032	146505.196463	36.456935
1553.194911	146706.566177	36.461952
1555.266031	146910.019846	36.466970
1556.921126	147129.703234	36.471988
1558.657749	147352.835851	36.477005
1560.313890	147562.292190	36.482023
1561.996766	147769.856845	36.487040
1563.571864	147970.252300	36.492058
1564.835050	148204.558168	36.497076
1566.272768	148415.271762	36.502093
1567.654768	148636.377994	36.507111
1569.155220	148858.506443	36.512128
1570.744850	149079.963047	36.517146
1572.283670	149305.004211	36.522164
1574.301567	149512.412808	36.527181
1575.848406	149747.775078	36.532199
1577.250094	149981.539398	36.537216
1578.965866	150190.027196	36.542234
1580.279612	150425.773694	36.547252
1581.994967	150649.896019	36.552269
1583.253494	150891.562464	36.557287
1584.726207	151116.182926	36.562304
1586.617406	151349.689107	36.567322
1588.198516	151588.761166	36.572340
1589.734862	151824.114690	36.577357
1591.190505	152069.739423	36.582375
1592.254796	152302.737111	36.587392
1594.031186	152534.228694	36.592410
1595.592808	152796.755021	36.597428
1597.135671	153036.071817	36.602445
1598.230174	153289.357430	36.607463
1599.972673	153548.057320	36.612480
1601.586687	153799.793532	36.617498
1602.928540	154066.168411	36.622516
1604.737206	154318.093131	36.627533
1606.121458	154592.491317	36.632551
1607.524939	154848.364195	36.637568
1609.093856	155103.845024	36.642586
1610.411266	155372.529054	36.647604
1612.047462	155618.886505	36.652621
1612.908028	155868.272585	36.657639
1614.636937	156127.349394	36.662656
1616.367468	156390.231872	36.667674
1617.949601	156662.599204	36.672692
1619.472748	156921.651294	36.677709
1621.254160	157179.142688	36.682727
1622.964227	157448.275145	36.687744
1624.994134	157700.392558	36.692762
1626.580697	157974.316535	36.697780
1628.682563	158228.315743	36.702797
1630.505304	158487.522164	36.707815
1631.609209	158751.333665	36.712832
1633.547349	159010.715846	36.717850
1634.976158	159279.146264	36.722868
1636.857642	159531.680904	36.727885
1638.808725	159800.843935	36.732903
1640.476760	160065.552138	36.737920
1642.584685	160311.982091	36.742938
1643.930766	160572.674516	36.747956
1645.795666	160838.092737	36.752973
1647.343744	161096.030389	36.757991
1649.190401	161348.697630	36.763008
1650.811918	161613.120366	36.768026
1652.534468	161871.454391	36.773044
1654.297429	162127.133325	36.778061
1656.021391	162382.782219	36.783079
1658.025952	162650.474431	36.788096
1660.098183	162887.302026	36.793114
1662.818151	163101.174799	36.798132
1666.526021	163282.437780	36.803149
1668.619688	163496.336256	36.808167
1670.706234	163688.068110	36.813184
1672.935520	163861.629560	36.818202
1674.227951	164054.656249	36.823220
1675.874275	164229.681750	36.828237
1677.298521	164419.848505	36.833255
1678.692203	164611.504986	36.838272
1679.931649	164797.707953	36.843290
1681.044983	164997.502637	36.848308
1682.341491	165190.090724	36.853325
1683.960656	165397.087283	36.858343
1685.162838	165614.297741	36.863360
1686.475430	165823.691745	36.868378
1687.437720	166059.967743	36.873396
1689.140510	166293.590959	36.878413
1690.543196	166527.250608	36.883431
1691.435353	166768.311192	36.888448
1693.130004	167021.828040	36.893466
1694.375128	167273.160278	36.898484
1695.904408	167539.352530	36.903501
1697.340495	167803.506659	36.908519
1698.672969	168075.175313	36.913536
1700.329641	168352.755936	36.918554
1701.700702	168622.075801	36.923572
1703.658425	168875.284187	36.928589
1705.725866	169123.022560	36.933607
1706.935827	169389.214992	36.938624
1708.917718	169638.949039	36.943642
1710.314542	169900.536218	36.948660
1711.877551	170165.155777	36.953677
1713.658419	170438.000323	36.958695
1715.108589	170711.051510	36.963712
1716.734647	170978.672893	36.968730
1718.593687	171264.018144	36.973748
1720.074974	171552.317662	36.978765
1721.845945	171829.131228	36.983783
1723.270409	172122.594131	36.988800
1725.360210	172412.972491	36.993818
1726.840947	172710.959498	36.998836
1728.500622	173005.152701	37.003853
1731.244263	173283.851652	37.008871
1732.801166	173576.834869	37.013888
1734.976772	173850.858113	37.018906
1736.711129	174137.372823	37.023924
1738.381958	174427.959182	37.028941
1740.075530	174711.541274	37.033959
1741.897479	175006.903138	37.038976
1743.856002	175296.650797	37.043994
1745.608635	175586.204847	37.049012
1747.396534	175870.972539	37.054029
1749.314009	176155.125361	37.059047
1750.952501	176454.472309	37.064064
1752.814053	176743.053015	37.069082
1754.432280	177033.919933	37.074100
1756.244899	177321.941523	37.079117
1758.099413	177611.962996	37.084135
1759.796708	177908.405742	37.089152
1761.670006	178198.720097	37.094170
1763.698663	178489.265532	37.099188
1765.713114	178778.952483	37.104205
1767.879192	179060.827246	37.109223
1769.212396	179348.202945	37.114240
1771.340446	179631.698846	37.119258
1772.932617	179927.525345	37.124276
1774.736659	180212.764004	37.129293
1776.509673	180490.828144	37.134311
1778.059658	180784.611801	37.139328
1779.794297	181077.264274	37.144346
1781.815826	181367.855759	37.149364
1783.360672	181652.079254	37.154381
1785.123677	181941.763993	37.159399
1786.839104	182244.984015	37.164416
1788.862730	182536.940591	37.169434
1790.586105	182826.954668	37.174452
1792.642524	183119.189037	37.179469
1794.973177	183411.140707	37.184487
1796.568674	183696.181414	37.189504
1798.275570	183967.070847	37.194522
1800.343188	184247.522875	37.199540
1801.892733	184517.514320	37.204557
1803.359966	184774.476052	37.209575
1805.019833	185040.088057	37.214592
1806.581939	185299.245622	37.219610
1808.598891	185564.410640	37.224628
1810.338457	185837.805898	37.229645
1812.348123	186099.764766	37.234663
1814.207192	186366.748718	37.239680
1816.746549	186621.177711	37.244698
1819.244960	186875.995301	37.249716
1821.039014	187130.037831	37.254733
1823.055821	187383.932182	37.259751
1824.665267	187640.303667	37.264768
1826.433854	187880.052830	37.269786
1828.183262	188132.064829	37.274804
1830.033418	188404.810493	37.279821
1831.792068	188658.486250	37.284839
1833.538683	188927.317421	37.289856
1835.222457	189177.289607	37.294874
1837.121476	189448.498007	37.299892
1838.405310	189713.358858	37.304909
1840.265587	189980.985036	37.309927
1841.692925	190269.176738	37.314944
1843.292761	190550.464438	37.319962
1845.120825	190834.585655	37.324980
1846.430468	191140.923621	37.329997
1848.267031	191425.338834	37.335015
1850.272770	191735.351925	37.340032
1851.990790	192036.693894	37.345050
1853.741606	192346.383269	37.350068
1855.343237	192653.889996	37.355085
1857.460120	192957.839428	37.360103
1859.404956	193273.671767	37.365120
1861.418422	193580.370059	37.370138
1863.843596	193882.029799	37.375156
1865.332259	194197.496167	37.380173
1867.392536	194504.522646	37.385191
1869.636819	194815.354688	37.390208
1871.775897	195118.488694	37.395226
1874.795075	195384.348291	37.400244
1877.106608	195660.855928	37.405261
1879.717155	195926.008989	37.410279
1881.634648	196202.721694	37.415296
1883.739829	196460.215532	37.420314
1885.594466	196719.349636	37.425332
1887.087380	196982.629360	37.430349
1889.023861	197239.481136	37.435367
1891.339005	197495.944065	37.440384
1893.168677	197754.401864	37.445402
1894.654126	198021.648030	37.450420
1896.126771	198285.864042	37.455437
1898.277389	198543.513192	37.460455
1899.777063	198824.240743	37.465472
1901.202247	199085.599688	37.470490
1903.200368	199332.995680	37.475508
1904.408307	199594.785055	37.480525
1906.174024	199843.756115	37.485543
1907.681102	200110.298443	37.490560
1909.344264	200384.953575	37.495578
1911.202237	200655.847378	37.500596
1912.467544	200950.636377	37.505613
1914.212026	201223.226492	37.510631
1915.919175	201525.589793	37.515648
1917.537314	201829.327062	37.520666
1919.651545	202132.695300	37.525684
1921.005065	202436.236686	37.530701
1923.135755	202747.831066	37.535719
1924.692291	203074.547635	37.540736
1926.589176	203396.045700	37.545754
1928.396916	203723.487753	37.550772
1930.077213	204065.600694	37.555789
1931.984215	204397.486404	37.560807
1934.052097	204744.010142	37.565824
1935.909467	205086.291426	37.570842
1938.085720	205426.607280	37.575860
1939.431042	205777.847130	37.580877
1941.638243	206130.031311	37.585895
1943.358569	206486.052408	37.590912
1945.631597	206840.959660	37.595930
1947.956508	207192.839466	37.600948
1949.907372	207552.321325	37.605965
1952.193442	207887.657489	37.610983
1954.164499	208249.730001	37.616000
1956.140368	208595.198969	37.621018
1958.711889	208942.606545	37.626036
1960.462664	209290.324052	37.631053
1962.788602	209635.463988	37.636071
1964.944204	209982.841821	37.641088
1967.197827	210322.830084	37.646106
1968.999380	210664.961252	37.651124
1970.782789	211017.773957	37.656141
1973.291000	211343.597327	37.661159
1975.537496	211689.002278	37.666176
1977.424307	212031.990516	37.671194
1979.366755	212363.139395	37.676212
1981.198146	212700.922042	37.681229
1983.303939	213036.250689	37.686247
1985.200882	213385.300299	37.691264
1987.204342	213721.588151	37.696282
1989.637719	214055.803517	37.701300
1991.342631	214395.049507	37.706317
1993.646840	214734.684559	37.711335
1995.414827	215067.728219	37.716352
1996.941198	215414.777690	37.721370
1999.166615	215755.331760	37.726388
2000.711965	216102.419775	37.731405
2002.607527	216445.873566	37.736423
2004.788007	216793.486371	37.741440
2006.609070	217130.035759	37.746458
2008.784811	217467.457325	37.751476
2010.849013	217799.730652	37.756493
2012.625806	218126.070975	37.761511
2014.896660	218446.303420	37.766528
2016.572218	218781.880630	37.771546
2018.399861	219098.745441	37.776564
2020.350136	219441.532018	37.781581
2022.136193	219780.905360	37.786599
2024.033815	220118.637332	37.791616
2026.210547	220450.041477	37.796634
2028.794932	220788.327762	37.801652
2030.904171	221123.453160	37.806669
2032.993728	221489.704213	37.811687
2034.752629	221866.764139	37.816704
2036.752904	222207.269860	37.821722
2038.736525	222563.067469	37.826740
2040.625032	222910.641098	37.831757
2042.413243	223272.199516	37.836775
2044.634425	223622.948691	37.841792
2046.468621	223996.743636	37.846810
2048.490640	224352.695575	37.851828
2050.380053	224722.244079	37.856845
2052.598265	225082.091717	37.861863
2054.659448	225456.314501	37.866880
2056.483395	225829.014767	37.871898
2058.902180	226196.822472	37.876916
2061.107506	226570.811533	37.881933
2063.266464	226947.653992	37.886951
2065.681722	227309.143424	37.891968
2067.878176	227680.522940	37.896986
2070.113617	228043.491584	37.902004
2072.166882	228410.808085	37.907021
2074.268623	228789.064467	37.912039
2076.490547	229145.208061	37.917056
2078.353753	229514.540254	37.922074
2080.583820	229876.577577	37.927092
2082.616584	230252.743117	37.932109
2084.670841	230622.633648	37.937127
2086.813139	230992.257721	37.942144
2089.252827	231363.055169	37.947162
2091.795591	231726.447015	37.952180
2093.628546	232097.622980	37.957197
2095.911019	232461.287510	37.962215
2098.322462	232819.548593	37.967232
2100.419605	233179.232352	37.972250
2102.829127	233523.044849	37.977268
2104.911767	233885.451092	37.982285
2107.027055	234230.938205	37.987303
2109.248970	234583.013174	37.992320
2111.012662	234942.070441	37.997338
2113.606004	235295.130293	38.002356
2115.524527	235647.155461	38.007373
2117.544575	235996.625842	38.012391
2119.497501	236362.236284	38.017408
2121.301902	236721.090038	38.022426
2123.240448	237049.216338	38.027444
2125.206415	237388.337081	38.032461
2127.289679	237719.769733	38.037479
2129.358594	238055.498129	38.042496
2131.247526	238400.247442	38.047514
2133.686208	238727.054855	38.052532
2135.722061	239083.669866	38.057549
2137.815368	239426.408735	38.062567
2140.194177	239766.004589	38.067584
2142.113688	240107.807859	38.072602
2144.090731	240456.867328	38.077620
2146.311452	240810.537340	38.082637
2148.246754	241166.692059	38.087655
2150.664430	241515.837121	38.092672
2153.014428	241864.460513	38.097690
2155.295892	242211.978154	38.102708
2157.549823	242576.900258	38.107725
2159.388584	242927.080913	38.112743
2161.784257	243291.144377	38.117760
2163.820723	243659.431506	38.122778
2165.899144	244019.838871	38.127796
2167.942740	244383.681815	38.132813
2169.657096	244754.436130	38.137831
2172.020675	245135.553569	38.142848
2174.212284	245517.232757	38.147866
2176.373523	245896.225322	38.152884
2178.227693	246286.647206	38.157901
2180.024233	246675.656842	38.162919
2182.576447	247064.496871	38.167936
2184.357833	247469.691481	38.172954
2186.573402	247862.930587	38.177972
2188.728800	248266.747170	38.182989
2191.448503	248667.198550	38.188007
2193.842823	249060.539382	38.193024
2195.996198	249451.988897	38.198042
2198.859208	249830.016447	38.203060
2201.303900	250217.916210	38.208077
2203.460028	250604.770377	38.213095
2206.246107	250984.565476	38.218112
2208.171507	251379.713540	38.223130
2210.645583	251752.142512	38.228148
2212.669836	252134.575718	38.233165
2214.957691	252518.517448	38.238183
2217.090511	252901.036662	38.243200
2219.467191	253287.480699	38.248218
2222.325570	253652.714648	38.253236
2224.371545	254030.677554	38.258253
2226.410842	254419.438152	38.263271
2228.373905	254779.913574	38.268288
2230.232396	255174.419788	38.273306
2232.562082	255563.034910	38.278324
2234.571343	255952.489030	38.283341
2236.744143	256345.017007	38.288359
2238.717074	256731.455397	38.293376
2240.782623	257133.984914	38.298394
2242.934879	257509.650953	38.303412
2244.874325	257882.557060	38.308429
2247.079746	258255.345360	38.313447
2249.097403	258635.581561	38.318464
2251.690439	259008.563551	38.323482
2253.569186	259396.088070	38.328500
2256.203383	259770.029926	38.333517
2258.338054	260154.619053	38.338535
2260.753864	260520.543892	38.343552
2263.074190	260912.979480	38.348570
2265.751848	261285.189071	38.353588
2267.938002	261677.113485	38.358605
2269.689251	262066.770288	38.363623
2272.252906	262448.017388	38.368640
2274.452526	262846.622077	38.373658
2276.279291	263240.256560	38.378676
2278.473256	263646.915819	38.383693
2280.679365	264055.885285	38.388711
2283.065288	264464.013783	38.393728
2284.936893	264884.392344	38.398746
2287.453647	265302.154133	38.403764
2289.891176	265709.259564	38.408781
2291.927112	266127.352410	38.413799
2294.626365	266554.155371	38.418816
2296.303305	266981.298615	38.423834
2298.505445	267416.183137	38.428852
2300.935431	267859.465764	38.433869
2303.124359	268297.604676	38.438887
2305.534322	268728.189474	38.443904
2308.069779	269170.211549	38.448922
2310.881678	269595.855724	38.453940
2313.371257	270034.964203	38.458957
2315.624884	270468.673999	38.463975
2318.779533	270889.082200	38.468992
2321.048866	271313.543056	38.474010
2323.434149	271730.745718	38.479028
2326.051591	272142.373767	38.484045
2328.549921	272571.828597	38.489063
2331.027348	272975.451580	38.494080
2333.412029	273386.354717	38.499098
2336.306007	273790.546882	38.504116
2338.902808	274189.426083	38.509133
2341.210541	274593.838275	38.514151
2344.188239	274993.520844	38.519168
2346.570490	275391.595778	38.524186
2348.585883	275781.574353	38.529204
2351.088981	276171.958243	38.534221
2353.287741	276571.560960	38.539239
2355.544143	276965.895967	38.544256
2357.762276	277360.059137	38.549274
2360.121834	277765.377283	38.554292
2362.495330	278155.908334	38.559309
2364.309807	278565.859848	38.564327
2366.917904	278955.413516	38.569344
2369.427580	279352.679850	38.574362
2371.738793	279735.802407	38.579380
2373.855583	280109.912024	38.584397
2375.507451	280488.515336	38.589415
2377.457918	280864.911836	38.594432
2379.882214	281258.507251	38.599450
2381.844223	281647.577713	38.604468
2384.250403	282046.840427	38.609485
2386.187550	282464.924798	38.614503
2388.505928	282860.847614	38.619520
2390.484480	283287.688870	38.624538
2393.199781	283700.390415	38.629556
2395.443933	284122.565439	38.634573
2397.638108	284556.026965	38.639591
2400.101128	284984.872872	38.644608
2402.135715	285438.579625	38.649626
2403.962037	285875.984704	38.654644
2406.290896	286331.701385	38.659661
2407.989757	286808.271566	38.664679
2410.426243	287283.911268	38.669696
2412.949635	287763.854997	38.674714
2414.734354	288249.529111	38.679732
2417.326900	288738.198953	38.684749
2419.356202	289237.956656	38.689767
2421.921565	289730.388735	38.694784
2424.406855	290249.022780	38.699802
2426.697128	290756.306344	38.704820
2429.283211	291257.674025	38.709837
2431.638685	291785.953113	38.714855
2434.284567	292290.840149	38.719872
2437.358813	292813.897131	38.724890
2439.699510	293324.723631	38.729908
2442.410033	293830.917922	38.734925
2445.807795	294335.198541	38.739943
2448.455052	294834.719679	38.744960
2450.946945	295344.831494	38.749978
2453.634637	295843.403846	38.754996
2456.876437	296319.457157	38.760013
2459.328811	296808.894186	38.765031
2461.649144	297286.081763	38.770048
2464.831886	297767.983149	38.775066
2467.715123	298250.184715	38.780084
2470.331108	298708.854583	38.785101
2473.350897	299173.581004	38.790119
2475.578451	299624.460867	38.795136
2478.339982	300095.957036	38.800154
2480.560970	300568.832963	38.805172
2483.295066	301010.636606	38.810189
2485.328524	301475.157105	38.815207
2487.944211	301938.618684	38.820224
2490.392652	302394.256418	38.825242
2492.688585	302864.217664	38.830260
2495.743481	303308.554630	38.835277
2498.162072	303767.672722	38.840295
2500.258726	304220.185347	38.845312
2502.906347	304660.823290	38.850330
2505.198677	305101.516115	38.855348
2508.012803	305535.088882	38.860365
2509.858688	305961.066547	38.865383
2512.213426	306395.776101	38.870400
2514.555058	306835.998121	38.875418
2516.360386	307268.429563	38.880436
2518.533931	307726.531420	38.885453
2520.412837	308197.378249	38.890471
2522.492875	308661.257236	38.895488
2524.854791	309140.634421	38.900506
2526.999672	309631.753303	38.905524
2529.307664	310126.527215	38.910541
2531.599845	310631.537485	38.915559
2534.110094	311134.682213	38.920576
2536.926517	311646.665895	38.925594
2539.647232	312155.817681	38.930612
2541.975147	312674.071366	38.935629
2544.464900	313192.931888	38.940647
2547.314856	313711.529616	38.945664
2550.387342	314232.857969	38.950682
2552.858818	314762.127049	38.955700
2555.914670	315280.658901	38.960717
2558.443479	315803.487695	38.965735
2561.257758	316319.588825	38.970752
2564.290694	316833.036617	38.975770
2566.920335	317344.437579	38.980788
2569.492885	317862.168878	38.985805
2571.715714	318385.667200	38.990823
2574.067851	318907.694460	38.995840
2576.660727	319431.864797	39.000858
2579.047215	319969.093529	39.005876
2581.892888	320499.820898	39.010893
2584.579939	321035.827376	39.015911
2587.308059	321560.497205	39.020928
2590.351785	322094.967708	39.025946
2592.623106	322623.995484	39.030964
2595.305352	323144.447170	39.035981
2598.060745	323682.102542	39.040999
2600.756501	324216.767194	39.046016
2604.066398	324725.402119	39.051034
2606.878780	325259.178063	39.056052
2609.750705	325763.050742	39.061069
2612.267580	326279.369347	39.066087
2615.087657	326791.116245	39.071104
2618.282813	327300.438668	39.076122
2620.675747	327814.760620	39.081140
2623.102073	328316.198832	39.086157
2625.739542	328839.667980	39.091175
2628.177256	329345.338443	39.096192
2631.061240	329844.256174	39.101210
2633.185492	330363.326624	39.106228
2636.025421	330871.462345	39.111245
2638.759291	331382.303028	39.116263
2641.382452	331896.611116	39.121280
2644.107569	332397.060116	39.126298
2646.277960	332887.994930	39.131316
2648.736027	333372.253237	39.136333
2651.059374	333858.687888	39.141351
2653.565282	334337.116985	39.146368
2656.253692	334820.820807	39.151386
2658.355131	335332.494613	39.156404
2661.005016	335832.067324	39.161421
2663.221068	336342.140988	39.166439
2665.792048	336854.135040	39.171456
2668.360023	337378.922767	39.176474
2670.900491	337899.038678	39.181492
2673.388061	338432.869832	39.186509
2676.040529	338970.453625	39.191527
2678.230146	339510.975301	39.196544
2681.033809	340056.853970	39.201562
2683.100092	340621.226991	39.206580
2685.681174	341181.958775	39.211597
2688.423114	341757.614368	39.216615
2690.735232	342332.545536	39.221632
2693.634958	342911.567345	39.226650
2696.668996	343504.348370	39.231668
2699.744356	344068.529495	39.236685
2702.732133	344648.789848	39.241703
2705.990764	345228.011404	39.246720
2709.290406	345784.143217	39.251738
2712.300715	346353.847008	39.256756
2715.248621	346907.738737	39.261773
2718.368488	347459.186044	39.266791
2721.176369	348022.075993	39.271808
2723.845354	348570.156543	39.276826
2726.669077	349131.839562	39.281844
2729.070522	349694.370675	39.286861
2731.781532	350258.776264	39.291879
2734.141430	350824.780078	39.296896
2737.330980	351393.185045	39.301914
2739.428837	351977.190852	39.306932
2742.076133	352541.810884	39.311949
2744.575252	353117.566647	39.316967
2747.288522	353709.857917	39.321984
2750.102446	354291.008371	39.327002
2752.470835	354883.645361	39.332020
2756.104810	355467.597051	39.337037
2758.980048	356058.515527	39.342055
2761.497498	356652.884969	39.347072
2764.678285	357233.791195	39.352090
2766.886248	357820.657127	39.357108
2770.026419	358406.175486	39.362125
2772.926456	358990.176576	39.367143
2775.785027	359579.964072	39.372160
2778.587843	360167.671941	39.377178
2781.253249	360770.876400	39.382196
2784.096356	361357.395695	39.387213
2786.996459	361954.380514	39.392231
2789.662903	362539.973952	39.397248
2793.024992	363097.913469	39.402266
2795.882657	363660.291279	39.407284
2798.192394	364200.644239	39.412301
2801.207666	364738.595034	39.417319
2803.859805	365292.331270	39.422336
2806.743063	365833.284529	39.427354
2808.982258	366374.688515	39.432372
2811.583557	366930.341217	39.437389
2814.489851	367486.928336	39.442407
2817.563439	368053.353327	39.447424
2820.759190	368593.106787	39.452442
2823.677863	369146.346548	39.457460
2826.724179	369692.250895	39.462477
2829.368249	370246.509640	39.467495
2832.036761	370812.201328	39.472512
2835.193520	371366.998673	39.477530
2837.571799	371932.213851	39.482548
2840.359062	372504.232936	39.487565
2843.281973	373068.737552	39.492583
2845.169967	373656.386291	39.497600
2848.158633	374242.710618	39.502618
2850.885028	374845.128731	39.507636
2853.368060	375434.966624	39.512653
2856.646698	376040.958483	39.517671
2859.129797	376649.731133	39.522688
2861.974887	377237.963002	39.527706
2865.425455	377859.680693	39.532724
2868.569969	378454.468767	39.537741
2871.832340	379058.083167	39.542759
2874.566598	379677.069473	39.547776
2877.701850	380268.026012	39.552794
2880.868507	380883.169997	39.557812
2883.199526	381497.523165	39.562829
2886.222205	382115.460614	39.567847
2888.867908	382739.028453	39.572864
2891.836368	383350.713984	39.577882
2894.523622	383976.258707	39.582900
2897.282408	384598.484044	39.587917
2900.115177	385230.655859	39.592935
2903.239565	385869.264116	39.597952
2905.845304	386492.369488	39.602970
2908.678760	387134.502004	39.607988
2911.969572	387769.601086	39.613005
2915.297131	388404.480248	39.618023
2918.117500	389039.124091	39.623040
2920.545696	389684.673792	39.628058
2923.599151	390332.243153	39.633076
2926.498787	390973.459241	39.638093
2929.212610	391622.833868	39.643111
2931.889431	392279.328538	39.648128
2934.940129	392935.295104	39.653146
2937.828846	393596.625669	39.658164
2940.331593	394257.497378	39.663181
2943.251085	394917.047732	39.668199
2945.730868	395600.947815	39.673216
2948.291276	396277.214003	39.678234
2950.959845	396932.428474	39.683252
2953.808325	397574.847260	39.688269
2957.271984	398209.042293	39.693287
2959.948671	398864.217274	39.698304
2962.986737	399501.446680	39.703322
2965.920906	400146.539978	39.708340
2968.747180	400810.576966	39.713357
2971.964933	401469.594402	39.718375
2974.737286	402124.358800	39.723392
2977.606852	402783.505710	39.728410
2980.450023	403463.254215	39.733428
2983.138571	404142.784407	39.738445
2986.293927	404817.688236	39.743463
2989.265348	405504.090268	39.748480
2992.495133	406190.385561	39.753498
2995.173046	406885.827952	39.758516
2997.951673	407582.252631	39.763533
3001.448573	408276.215777	39.768551
3003.991999	408988.285288	39.773568
3007.344716	409688.981363	39.778586
3010.384737	410401.851445	39.783604
3013.373337	411112.228841	39.788621
3016.655307	411824.266338	39.793639
3019.287007	412535.223804	39.798656
3022.730369	413248.975562	39.803674
3026.025256	413983.362748	39.808692
3028.734052	414709.334478	39.813709
3031.997301	415437.176979	39.818727
3034.622667	416174.630370	39.823744
3037.892465	416895.947631	39.828762
3041.508324	417620.992911	39.833780
3044.843356	418351.360045	39.838797
3047.853834	419078.389646	39.843815
3050.989439	419799.071517	39.848832
3054.313197	420521.757389	39.853850
3057.438312	421251.043473	39.858868
3060.516293	421970.690162	39.863885
3063.634512	422690.539727	39.868903
3066.843667	423418.741791	39.873920
3070.502740	424144.471854	39.878938
3073.627399	424858.740451	39.883956
3076.767520	425578.662245	39.888973
3079.543612	426303.942092	39.893991
3082.774613	427026.141234	39.899008
3085.580282	427741.447534	39.904026
3088.840513	428463.045757	39.909044
3091.801878	429188.166974	39.914061
3094.677065	429915.561382	39.919079
3097.545178	430655.043355	39.924096
3101.175486	431387.393459	39.929114
3103.933222	432118.721231	39.934132
3106.893622	432854.706758	39.939149
3109.915030	433586.508244	39.944167
3112.984964	434324.232262	39.949184
3116.275086	435050.808377	39.954202
3119.615852	435753.045812	39.959220
3122.220711	436439.022072	39.964237
3125.488178	437122.241323	39.969255
3128.202330	437827.938185	39.974272
3131.433701	438514.467298	39.979290
3134.358111	439214.748952	39.984308
3137.367480	439919.909059	39.989325
3140.753226	440636.129173	39.994343
3143.710315	441355.889856	39.999360
3146.391923	442071.875393	40.004378
3149.185176	442807.720084	40.009396
3152.102116	443539.523036	40.014413
3155.673613	444274.085924	40.019431
3158.435734	445023.435904	40.024448
3161.240278	445771.591215	40.029466
3164.506050	446531.445114	40.034484
3167.402070	447295.534605	40.039501
3170.546942	448064.368744	40.044519
3173.654810	448851.608425	40.049536
3176.517645	449624.130877	40.054554
3179.528522	450405.512329	40.059572
3182.555402	451213.790835	40.064589
3185.950603	452020.970393	40.069607
3188.821993	452843.994385	40.074624
3192.136664	453658.821279	40.079642
3195.142935	454478.677576	40.084660
3197.924458	455312.860448	40.089677
3201.366691	456142.707824	40.094695
3204.492490	456972.726194	40.099712
3207.399675	457828.553133	40.104730
3210.854246	458679.200756	40.109748
3214.069656	459540.174516	40.114765
3217.693412	460394.371680	40.119783
3220.658911	461254.356166	40.124800
3223.934861	462113.498637	40.129818
3227.287962	462977.501570	40.134836
3230.716501	463855.267271	40.139853
3234.368128	464717.180100	40.144871
3238.060543	465584.261310	40.149888
3241.813828	466427.981022	40.154906
3245.415395	467270.477161	40.159924
3249.234692	468110.325798	40.164941
3253.269034	468933.974275	40.169959
3257.147602	469746.792848	40.174976
3261.080273	470554.716469	40.179994
3265.057285	471348.594690	40.185012
3268.354546	472137.645041	40.190029
3272.079202	472908.951228	40.195047
3275.670504	473689.602950	40.200064
3278.764979	474458.573728	40.205082
3282.181484	475209.365183	40.210100
3285.134839	475985.024129	40.215117
3288.300264	476752.783933	40.220135
3291.348741	477516.943661	40.225152
3294.302698	478265.570597	40.230170
3297.286843	478992.530510	40.235188
3299.828533	479740.004334	40.240205
3302.795537	480460.999108	40.245223
3306.094682	481202.788346	40.250240
3308.942316	481956.093224	40.255258
3312.236700	482706.619855	40.260276
3314.682379	483470.188680	40.265293
3317.822066	484241.601853	40.270311
3320.607020	485027.896375	40.275328
3323.493102	485816.820727	40.280346
3326.810104	486617.568730	40.285364
3329.538623	487419.083458	40.290381
3332.647822	488256.223595	40.295399
3336.006488	489086.315384	40.300416
3338.928131	489922.855450	40.305434
3342.135676	490769.668708	40.310452
3345.070436	491623.154460	40.315469
3348.467718	492491.782256	40.320487
3351.811797	493375.580831	40.325504
3354.623078	494258.865715	40.330522
3358.138590	495136.744362	40.335540
3361.456992	496052.942563	40.340557
3364.762745	496943.039279	40.345575
3368.546164	497846.600293	40.350592
3372.512303	498765.235327	40.355610
3376.122284	499651.565361	40.360628
3379.603191	500545.647195	40.365645
3383.141157	501463.201737	40.370663
3386.995138	502355.063748	40.375680
3390.340407	503273.463741	40.380698
3393.978608	504172.133460	40.385716
3397.186038	505079.507083	40.390733
3400.807425	505988.837541	40.395751
3404.053925	506886.521061	40.400768
3407.681557	507811.956101	40.405786
3411.438942	508715.116344	40.410804
3414.347868	509635.722377	40.415821
3417.876842	510546.442162	40.420839
3420.800817	511472.901109	40.425856
3423.920587	512401.296752	40.430874
3427.575029	513338.184135	40.435892
3430.645185	514277.987364	40.440909
3433.891987	515227.950544	40.445927
3437.586382	516170.424304	40.450944
3440.786503	517139.353425	40.455962
3444.003750	518092.890334	40.460980
3447.202014	519057.975035	40.465997
3450.709469	520018.314548	40.471015
3453.853114	520999.229965	40.476032
3457.509201	521982.425790	40.481050
3461.352517	522948.489824	40.486068
3464.995159	523926.225108	40.491085
3468.515297	524901.954189	40.496103
3472.427237	525859.917458	40.501120
3476.032058	526805.759132	40.506125
3480.085448	527697.459586	40.511130
3483.509207	528534.784998	40.516135
3486.951138	529300.107212	40.521140
3490.085187	530013.042734	40.526144
3492.741255	530673.979165	40.531149
3495.373341	531248.545000	40.536154
3497.774578	531772.603257	40.541159
3499.909472	532239.142106	40.546164
3502.160795	532652.450922	40.551168
3504.192868	533023.903234	40.556173
3506.005064	533325.313125	40.561178
3507.355647	533587.740424	40.566183
3508.937956	533806.430014	40.571188
3510.412015	533972.344627	40.576192
3511.574465	534105.875835	40.581197
3513.032328	534189.702875	40.586202
3513.705123	534259.913488	40.591207
3514.559535	534291.400769	40.596212
3515.526012	534281.296601	40.601216
3516.089259	534271.559248	40.606221
3517.026180	534219.835389	40.611226
3517.308476	534164.779786	40.616231
3517.759080	534073.124182	40.621236
3518.502282	533956.921590	40.626240
3518.395055	533834.285420	40.631245
3518.805136	533692.925837	40.636250
3519.322382	533538.918715	40.641255
3519.456484	533383.000427	40.646260
3519.956400	533204.289507	40.651264
3519.754073	533014.926982	40.656269
3520.216737	532812.574543	40.661274
3519.676572	532621.340871	40.666279
3520.185546	532412.761920	40.671284
3520.384688	532191.851346	40.676288
3520.221321	531969.731879	40.681293
3520.413754	531747.906676	40.686298
3520.462032	531516.905770	40.691303
3520.211709	531277.763660	40.696308
3520.130743	531030.507063	40.701312
3520.206155	530793.529190	40.706317
3520.129324	530557.733916	40.711322
3519.847090	530314.085241	40.716327
3519.578514	530058.606953	40.721332
3519.466038	529806.232660	40.726336
3519.228349	529582.777336	40.731341
3519.334133	529335.868784	40.736346
3519.164282	529087.180792	40.741351
3519.644021	528850.716125	40.746356
3519.484323	528603.737018	40.751360
3519.222154	528341.407909	40.756365
3519.081976	528093.659744	40.761370
3518.663525	527850.348286	40.766375
3518.491323	527603.961991	40.771380
3518.329776	527361.057253	40.776384
3517.867521	527130.628659	40.781389
3517.971534	526882.924082	40.786394
3517.601528	526660.863524	40.791399
3517.361193	526430.035939	40.796404
3517.117851	526185.407832	40.801408
3516.778525	525973.845363	40.806413
3517.165537	525736.691989	40.811418
3516.838502	525526.132501	40.816423
3516.577550	525297.111360	40.821428
3516.685584	525074.649945	40.826432
3516.125955	524864.219612	40.831437
3516.355215	524643.249410	40.836442
3516.148209	524432.201681	40.841447
3515.735345	524214.006033	40.846452
3515.553391	524003.302549	40.851456
3515.342305	523805.086371	40.856461
3515.285493	523594.054469	40.861466
3515.046920	523404.885996	40.866471
3514.731252	523204.656988	40.871476
3514.879738	523004.149935	40.876480
3514.699257	522818.756739	40.881485
3514.481319	522623.964657	40.886490
3514.316350	522429.313521	40.891495
3513.911361	522252.694946	40.896500
3513.780960	522064.858659	40.901504
3513.580969	521888.456490	40.906509
3513.470520	521709.004960	40.911514
3513.521524	521534.025369	40.916519
3513.003266	521361.914454	40.921524
3513.188153	521191.712845	40.926528
3512.629525	521023.800931	40.931533
3512.380008	520856.293449	40.936538
3512.298966	520705.087875	40.941543
3512.111542	520543.836570	40.946548
3512.165058	520389.421620	40.951552
3511.912894	520241.120665	40.956557
3511.964000	520088.776198	40.961562
3511.878717	519943.682010	40.966567
3511.443591	519806.731564	40.971572
3511.593434	519646.581015	40.976576
3510.920847	519523.165597	40.981581
3510.962258	519373.799161	40.986586
3510.916348	519244.063448	40.991591
3511.041095	519104.844466	40.996596
3510.875608	518979.676235	41.001600
3510.578187	518845.830939	41.006605
3510.756411	518707.560856	41.011610
3510.266922	518586.839934	41.016615
3510.150533	518460.395883	41.021620
3510.286823	518336.287495	41.026624
3509.951450	518216.904769	41.031629
3510.019945	518092.653568	41.036634
3509.982030	517987.835761	41.041639
3509.651250	517870.674728	41.046644
3509.825119	517751.663251	41.051648
3509.373504	517649.841582	41.056653
3509.482779	517531.850083	41.061658
3509.498060	517413.215214	41.066663
3509.150473	517315.825045	41.071668
3509.362239	517204.591188	41.076672
3509.137014	517102.528096	41.081677
3509.046273	517004.640380	41.086682
3508.854471	516908.588569	41.091687
3508.699969	516798.117855	41.096692
3508.416863	516696.718827	41.101696
3507.930514	516613.354444	41.106701
3508.274783	516524.801269	41.111706
3507.981010	516443.681285	41.116711
3507.856322	516356.718473	41.121716
3507.890840	516269.072611	41.126720
3508.107190	516189.185619	41.131725
3507.962336	516097.015734	41.136730
3507.795818	516019.312474	41.141735
3507.594810	515937.214484	41.146740
3507.832632	515861.823494	41.151744
3507.194202	515794.308347	41.156749
3507.479458	515713.194429	41.161754
3507.489147	515640.063723	41.166759
3507.298354	515559.580613	41.171764
3507.235346	515488.989424	41.176768
3507.117355	515409.606712	41.181773
3507.255027	515352.081950	41.186778
3507.131115	515276.290323	41.191783
3507.084820	515205.695297	41.196788
3506.979682	515136.272499	41.201792
3506.737694	515085.887339	41.206797
3506.702871	515002.342379	41.211802
3506.630366	514944.242529	41.216807
3506.694618	514884.654163	41.221812
3506.708702	514817.841144	41.226816
3506.875506	514762.383368	41.231821
3506.713170	514701.768066	41.236826
3506.488692	514645.107338	41.241831
3506.492165	514578.547925	41.246836
3506.964102	514520.309975	41.251840
3506.305142	514461.441339	41.256845
3506.661964	514402.917714	41.261850
3506.518561	514359.190984	41.266855
3506.351858	514289.369790	41.271860
3506.232449	514237.141908	41.276864
3505.959489	514177.351440	41.281869
3506.152458	514124.972678	41.286874
3506.092682	514077.337481	41.291879
3506.133298	514030.141487	41.296884
3505.792459	513976.986805	41.301888
3505.763819	513929.649739	41.306893
3505.895319	513875.459083	41.311898
3505.986550	513830.378840	41.316903
3505.627735	513784.206291	41.321908
3505.860411	513739.710398	41.326912
3505.735125	513704.931632	41.331917
3505.916697	513652.097986	41.336922
3505.596070	513605.666013	41.341927
3505.664795	513567.467458	41.346932
3505.652041	513520.430210	41.351936
3505.520626	513478.166112	41.356941
3505.461323	513434.878907	41.361946
3505.299066	513392.821791	41.366951
3505.399822	513357.045552	41.371956
3505.654286	513317.198499	41.376960
3505.329082	513282.450460	41.381965
3505.387338	513234.794223	41.386970
3505.397578	513206.720251	41.391975
3505.238975	513155.962054	41.396980
3505.627322	513117.711961	41.401984
3505.090889	513078.292841	41.406989
3505.069998	513053.713643	41.411994
3505.312354	513015.435813	41.416999
3505.659763	512986.043645	41.422004
3505.475599	512936.351039	41.427008
3505.307211	512907.697825	41.432013
3505.340572	512866.114294	41.437018
3505.280100	512833.144433	41.442023
3505.289489	512794.650017	41.447028
3505.446206	512746.875676	41.452032
3504.893359	512722.835318	41.457037
3505.088741	512678.190775	41.462042
3504.755779	512646.022356	41.467047
3504.886572	512616.006211	41.472052
3505.042578	512578.803278	41.477056
3504.917082	512550.041511	41.482061
3505.135862	512528.812717	41.487066
3504.996609	512494.944157	41.492071
3504.864448	512469.319452	41.497076
3505.075793	512427.706711	41.502080
3504.976662	512388.115692	41.507085
3505.288751	512361.914773	41.512090
3505.077927	512338.376224	41.517095
3504.643805	512301.872960	41.522100
3504.922071	512269.000209	41.527104
3504.567383	512246.647696	41.532109
3505.084323	512213.888865	41.537114
3504.768546	512187.331663	41.542119
3504.547104	512152.666066	41.547124
3504.737760	512124.359445	41.552128
3504.510793	512098.698581	41.557133
3504.646865	512067.011350	41.562138
3504.509439	512050.947272	41.567143
3504.854358	512025.954670	41.572148
3504.740832	512000.579233	41.577152
3504.153522	511976.543259	41.582157
3504.597929	511954.620484	41.587162
3504.919511	511930.491368	41.592167
3504.577913	511901.914412	41.597172
3504.900122	511865.442415	41.602176
3504.374603	511841.143557	41.607181
3504.707011	511824.347397	41.612186
3504.686957	511788.688108	41.617191
3504.758024	511763.080799	41.622196
3504.610976	511740.391286	41.627200
3504.524327	511721.131997	41.632205
3504.597326	511685.002515	41.637210
3504.765409	511674.757700	41.642215
3504.599523	511659.405946	41.647220
3504.852323	511630.936923	41.652224
3504.788685	511595.486461	41.657229
3504.682947	511569.704463	41.662234
3504.736182	511543.897298	41.667239
3504.555080	511514.889635	41.672244
3504.410958	511494.728627	41.677248
3504.198822	511465.270510	41.682253
3504.197735	511451.511274	41.687258
3504.556088	511423.885185	41.692263
3504.517160	511402.898062	41.697268
3504.610482	511368.889319	41.702272
3504.659186	511351.530500	41.707277
3504.495749	511324.239657	41.712282
3504.340673	511303.270769	41.717287
3504.451525	511279.730492	41.722292
3504.615750	511250.010167	41.727296
3504.415335	511242.352673	41.732301
3504.409097	511210.129885	41.737306
3504.604769	511196.693450	41.742311
3504.310444	511168.967764	41.747316
3504.589844	511144.186571	41.752320
3504.155762	511123.767433	41.757325
3504.312210	511097.285645	41.762330
3504.278213	511077.056148	41.767335
3504.334277	511070.066258	41.772340
3504.509293	511031.592249	41.777344
3503.998753	511033.342340	41.782349
3504.113911	511002.010543	41.787354
3504.066032	511004.395731	41.792359
3504.005757	510985.687903	41.797364
3503.973089	510953.317044	41.802368
3503.894681	510959.551722	41.807373
3503.846170	510927.132729	41.812378
3504.085622	510919.203212	41.817383
3504.050432	510914.706479	41.822388
3504.392254	510883.642163	41.827392
3504.274643	510882.497244	41.832397
3504.306738	510844.095991	41.837402
3504.327488	510846.622118	41.842407
3503.803718	510805.121599	41.847412
3503.826270	510803.650991	41.852416
3504.057372	510793.496862	41.857421
3503.919153	510775.155239	41.862426
3503.863959	510757.609884	41.867431
3503.898680	510761.752636	41.872436
3504.155748	510731.561439	41.877440
3503.951087	510732.554976	41.882445
3504.110081	510716.139253	41.887450
3504.012740	510697.892263	41.892455
3503.868359	510686.988006	41.897460
3503.952674	510666.941675	41.902464
3503.780610	510655.890008	41.907469
3504.164922	510638.932712	41.912474
3504.150513	510620.672530	41.917479
3504.066136	510609.050499	41.922484
3503.956936	510590.097027	41.927488
3503.572968	510582.367070	41.932493
3503.697207	510560.695466	41.937498
3504.343546	510558.468586	41.942503
3503.937182	510549.224491	41.947508
3504.155995	510530.472050	41.952512
3503.640657	510526.202874	41.957517
3503.916508	510494.136501	41.962522
3503.918997	510493.630228	41.967527
3503.914668	510492.062665	41.972532
3504.238591	510460.899232	41.977536
3503.915361	510464.946868	41.982541
3504.019476	510439.585290	41.987546
3503.949034	510423.306730	41.992551
3504.078045	510416.557987	41.997556
3504.339922	510391.424348	42.002560
3503.905558	510383.145784	42.007565
3504.039790	510373.866735	42.012570
3504.150034	510354.726547	42.017575
3504.106743	510355.542831	42.022580
3504.381142	510312.700807	42.027584
3503.951204	510313.224080	42.032589
3504.069369	510278.602162	42.037594
3503.817475	510271.407673	42.042599
3503.516965	510261.286666	42.047604
3504.171044	510253.341894	42.052608
3503.770715	510244.450807	42.057613
3503.929207	510226.264053	42.062618
3504.335265	510228.577600	42.067623
3503.712942	510204.747009	42.072628
3504.188028	510179.376998	42.077632
3503.601007	510164.090460	42.082637
3503.960347	510141.925855	42.087642
3504.231476	510135.053358	42.092647
3504.107178	510116.506467	42.097652
3503.879337	510101.669001	42.102656
3503.402861	510106.246845	42.107661
3503.923713	510071.662038	42.112666
3503.770808	510070.826184	42.117671
3503.455614	510069.661850	42.122676
3503.914002	510055.980632	42.127680
3503.767664	510041.079640	42.132685
3503.799992	510025.745673	42.137690
3504.006405	510020.401070	42.142695
3503.995943	510006.288017	42.147700
3504.124441	509980.061867	42.152704
3503.543795	509977.269998	42.157709
3503.803314	509966.149667	42.162714
3504.311467	509945.428411	42.167719
3504.065964	509950.070969	42.172724
3504.155920	509916.413998	42.177728
3504.093169	509906.204609	42.182733
3503.945758	509884.069178	42.187738
3504.112507	509868.562050	42.192743
3504.033708	509864.628432	42.197748
3504.097525	509827.535242	42.202752
3503.397886	509827.494066	42.207757
3504.008509	509813.232093	42.212762
3503.765228	509801.533447	42.217767
3503.885253	509788.462000	42.222772
3503.597054	509781.525998	42.227776
3503.938555	509788.605369	42.232781
3504.079881	509765.412326	42.237786
3504.169382	509752.699814	42.242791
3503.692052	509740.532209	42.247796
3503.985837	509712.306467	42.252800
3503.869582	509714.803825	42.257805
3503.901918	509697.243546	42.262810
3503.638421	509679.780601	42.267815
3503.571064	509665.473894	42.272820
3503.729467	509666.410104	42.277824
3503.982971	509658.073052	42.282829
3503.922816	509628.739514	42.287834
3503.896786	509625.556373	42.292839
3503.966936	509616.843550	42.297844
3503.854203	509595.967054	42.302848
3503.614824	509597.977974	42.307853
3503.937921	509581.990551	42.312858
3503.739164	509562.645361	42.317863
3503.861021	509554.076108	42.322868
3503.687599	509546.666543	42.327872
3503.737728	509536.641458	42.332877
3503.866888	509512.893486	42.337882
3503.745228	509517.567177	42.342887
3503.787003	509510.072990	42.347892
3503.996924	509473.461858	42.352896
3503.760689	509478.305446	42.357901
3503.777935	509463.985198	42.362906
3503.660382	509446.296578	42.367911
3503.388005	509444.821880	42.372916
3503.805255	509429.224168	42.377920
3503.633404	509436.840157	42.382925
3503.912839	509419.594681	42.387930
3503.869267	509411.658611	42.392935
3503.469533	509402.817582	42.397940
3503.592015	509390.453734	42.402944
3503.419924	509373.431358	42.407949
3503.570247	509361.923158	42.412954
3503.979603	509349.109199	42.417959
3503.733492	509354.359121	42.422964
3503.875347	509336.376423	42.427968
3503.808979	509326.268444	42.432973
3504.025365	509315.306288	42.437978
3503.737220	509315.250658	42.442983
3503.701634	509289.201165	42.447988
3503.734623	509275.080641	42.452992
3503.621154	509282.535692	42.457997
3503.624107	509272.467318	42.463002
3503.584481	509255.069738	42.468007
3503.376659	509248.829111	42.473012
3503.693568	509243.163246	42.478016
3503.917968	509247.276385	42.483021
3503.778109	509222.558680	42.488026
3503.563832	509208.376000	42.493031
3503.667353	509208.916169	42.498036
3504.072484	509188.260878	42.503040
3503.670093	509180.280231	42.508045
3503.803236	509165.688452	42.513050
3503.922364	509162.836431	42.518055
3503.388758	509163.780864	42.523060
3503.860980	509145.593969	42.528064
3503.908633	509145.333483	42.533069
3503.914325	509148.519949	42.538074
3503.741653	509123.200172	42.543079
3503.609933	509098.177444	42.548084
3503.950086	509100.653343	42.553088
3503.602481	509085.935112	42.558093
3503.629430	509058.812929	42.563098
3503.961396	509051.222080	42.568103
3503.845252	509056.400956	42.573108
3503.719650	509032.237249	42.578112
3503.720296	509023.130365	42.583117
3504.078073	509013.461094	42.588122
3503.674881	509007.959566	42.593127
3503.537459	508990.627770	42.598132
3503.883570	508979.644895	42.603136
3503.655050	508974.065154	42.608141
3503.672482	508961.363449	42.613146
3503.316389	508948.113652	42.618151
3503.385139	508945.320152	42.623156
3503.665625	508953.067230	42.628160
3503.279321	508946.348769	42.633165
3503.732549	508942.381439	42.638170
3503.640462	508917.756932	42.643175
3503.273798	508917.359556	42.648180
3503.696158	508911.423946	42.653184
3503.622226	508928.283315	42.658189
3503.688873	508900.193328	42.663194
3503.581761	508873.648573	42.668199
3503.924780	508877.793646	42.673204
3503.784338	508868.203043	42.678208
3503.639471	508865.949232	42.683213
3503.602102	508848.297915	42.688218
3503.615607	508837.114553	42.693223
3503.093260	508840.941072	42.698228
3503.600054	508832.715367	42.703232
3503.621441	508841.869484	42.708237
3503.289298	508816.068523	42.713242
3503.531940	508794.123001	42.718247
3503.447752	508804.052736	42.723252
3503.797501	508801.164203	42.728256
3503.381362	508800.724050	42.733261
3504.080808	508789.229859	42.738266
3503.674730	508775.127731	42.743271
3503.660805	508767.844400	42.748276
3504.004442	508755.546329	42.753280
3503.429309	508743.140501	42.758285
3503.546205	508724.048037	42.763290
3503.870524	508730.574028	42.768295
3503.492440	508733.871826	42.773300
3503.679261	508704.092917	42.778304
3503.279296	508698.135431	42.783309
3503.426540	508693.508089	42.788314
3503.596212	508690.344435	42.793319
3503.268024	508698.744375	42.798324
3503.789781	508686.519289	42.803329
3503.604215	508671.876278	42.808333
3503.644434	508646.167988	42.813338
3503.592182	508656.446921	42.818343
3503.743024	508660.925989	42.823348
3503.993933	508628.354129	42.828353
3503.671092	508621.372536	42.833357
3503.900781	508613.038743	42.838362
3503.995888	508597.845361	42.843367
3503.424419	508591.914946	42.848372
3503.615427	508581.108117	42.853377
3503.383388	508585.293562	42.858381
3503.904664	508578.229123	42.863386
3503.755706	508566.666508	42.868391
3503.693722	508551.497914	42.873396
3503.679057	508551.348459	42.878401
3503.445076	508549.614639	42.883405
3503.760370	508524.874583	42.888410
3503.895686	508512.052723	42.893415
3503.246401	508507.247664	42.898420
3503.740834	508511.419488	42.903425
3503.267890	508489.131332	42.908429
3503.566798	508479.724042	42.913434
3503.611908	508474.455052	42.918439
3503.382280	508472.771130	42.923444
3503.491367	508475.637809	42.928449
3503.470002	508477.412018	42.933453
3503.182893	508457.118244	42.938458
3503.366077	508440.443547	42.943463
3503.313977	508437.517281	42.948468
3503.353692	508437.258039	42.953473
3503.243891	508442.638477	42.958477
3503.557155	508436.163405	42.963482
3503.209069	508437.685691	42.968487
3503.422767	508448.833421	42.973492
3503.450871	508440.531408	42.978497
3503.058409	508415.295924	42.983501
3503.445988	508419.332875	42.988506
3503.439102	508403.598897	42.993511
3503.363771	508412.768530	42.998516
3503.440549	508405.723684	43.003521
3503.365436	508417.726607	43.008525
3503.286081	508418.751062	43.013530
3503.180035	508415.276773	43.018535
3503.157833	508398.381524	43.023540
3503.435935	508373.343558	43.028545
3503.439173	508382.146622	43.033549
3503.501319	508388.410613	43.038554
3503.535783	508382.181968	43.043559
3503.359413	508391.266393	43.048564
3503.530429	508387.647115	43.053569
3503.374131	508367.585535	43.058573
3503.553483	508355.768503	43.063578
3503.298569	508351.255232	43.068583
3503.302813	508351.254571	43.073588
3503.781075	508348.598627	43.078593
3503.476879	508345.965169	43.083597
3503.524635	508335.737378	43.088602
3503.923447	508313.260607	43.093607
3503.663447	508313.605287	43.098612
3503.425275	508302.714335	43.103617
3503.244223	508307.498933	43.108621
3503.610447	508301.167225	43.113626
3503.609959	508278.905310	43.118631
3503.360794	508275.807783	43.123636
3503.809854	508275.939196	43.128641
3503.630164	508282.140259	43.133645
3503.817331	508258.482578	43.138650
3503.767226	508237.341555	43.143655
3503.776634	508235.215062	43.148660
3503.736834	508233.905877	43.153665
3504.130936	508214.769034	43.158669
3504.148999	508196.045777	43.163674
3503.995742	508175.173960	43.168679
3504.093523	508162.256582	43.173684
3503.938601	508154.033957	43.178689
3503.909534	508128.234655	43.183693
3503.671982	508120.834609	43.188698
3503.895573	508116.043258	43.193703
3503.600387	508100.708744	43.198708
3503.624700	508080.112321	43.203713
3503.485949	508077.452671	43.208717
3503.468492	508074.571464	43.213722
3503.891523	508073.948052	43.218727
3503.447047	508067.390228	43.223732
3503.655531	508046.562270	43.228737
3503.773119	508040.978114	43.233741
3503.907197	508041.108720	43.238746
3503.938913	508003.915478	43.243751
3503.803597	508000.799906	43.248756
3503.718208	508000.206257	43.253761
3503.481515	507989.922030	43.258765
3503.528369	507978.530454	43.263770
3503.946818	507974.720191	43.268775
3503.506692	507975.498119	43.273780
3503.680395	507964.643044	43.278785
3503.445502	507942.771921	43.283789
3503.419530	507924.308312	43.288794
3503.400905	507924.463056	43.293799
3503.095902	507925.270225	43.298804
3503.374282	507922.595214	43.303809
3503.281173	507922.306362	43.308813
3503.321426	507927.562049	43.313818
3503.489896	507928.749748	43.318823
3503.034623	507915.767813	43.323828
3503.481616	507898.140156	43.328833
3503.319733	507886.224950	43.333837
3503.371311	507883.181009	43.338842
3503.559855	507890.032361	43.343847
3503.436541	507892.784081	43.348852
3503.486606	507886.653986	43.353857
3503.356190	507889.406829	43.358861
3503.182845	507867.323495	43.363866
3503.295912	507859.412547	43.368871
3503.240572	507860.129659	43.373876
3503.544154	507858.513186	43.378881
3503.415358	507860.709213	43.383885
3503.638072	507856.929863	43.388890
3503.352694	507852.370678	43.393895
3503.143839	507850.228041	43.398900
3503.548136	507837.160777	43.403905
3503.574272	507850.514204	43.408909
3503.606946	507841.300439	43.413914
3503.616575	507847.066959	43.418919
3503.588634	507848.994063	43.423924
3503.699505	507828.586045	43.428929
3503.482893	507820.474205	43.433933
3503.580073	507808.467401	43.438938
3503.646356	507818.272725	43.443943
3503.487192	507812.681643	43.448948
3503.712550	507784.008186	43.453953
3503.404347	507786.181984	43.458957
3503.475603	507782.122976	43.463962
3503.706938	507774.142698	43.468967
3503.391633	507777.582543	43.473972
3503.622890	507733.324199	43.478977
3503.731677	507720.505945	43.483981
3503.507750	507723.475983	43.488986
3503.559484	507729.691261	43.493991
3503.552078	507723.924372	43.498996
3503.404070	507687.821396	43.504001
3503.415430	507680.837192	43.509005
3503.237196	507671.859063	43.514010
3503.849269	507674.696969	43.519015
3503.357351	507669.765604	43.524020
3503.639482	507664.256513	43.529025
3503.712185	507647.244333	43.534029
3503.642295	507643.106407	43.539034
3503.612869	507649.182751	43.544039
3503.583106	507666.845928	43.549044
3503.611248	507649.941988	43.554049
3503.675094	507632.425220	43.559053
3503.575000	507633.857778	43.564058
3503.662207	507627.468733	43.569063
3503.767737	507621.481569	43.574068
3503.605812	507591.907658	43.579073
3503.038626	507588.354299	43.584077
3503.325199	507576.115007	43.589082
3503.683305	507579.549645	43.594087
3503.342799	507583.195902	43.599092
3503.563531	507575.773782	43.604097
3503.497250	507571.230489	43.609101
3503.573926	507560.542290	43.614106
3503.826423	507547.397607	43.619111
3503.449007	507562.029386	43.624116
3503.443269	507551.202415	43.629121
3503.679306	507522.172654	43.634125
3503.522577	507507.827682	43.639130
3503.651609	507494.398888	43.644135
3503.437160	507483.959049	43.649140
3503.776292	507472.470344	43.654145
3503.386337	507460.843883	43.659149
3503.522681	507449.943793	43.664154
3503.773044	507445.097427	43.669159
3503.391396	507436.707905	43.674164
3503.489261	507440.436695	43.679169
3503.709583	507432.053218	43.684173
3503.769281	507406.896581	43.689178
3503.700233	507399.267199	43.694183
3503.388223	507408.474775	43.699188
3503.825295	507400.815992	43.704193
3503.789030	507382.758217	43.709197
3503.427955	507375.478571	43.714202
3503.728505	507376.240646	43.719207
3503.167408	507383.716672	43.724212
3503.768309	507353.161610	43.729217
3503.656213	507332.585857	43.734221
3503.662464	507333.343854	43.739226
3503.644207	507335.471877	43.744231
3503.651138	507325.705326	43.749236
3503.635403	507308.504398	43.754241
3503.579440	507299.405552	43.759245
3503.596066	507296.468229	43.764250
3503.474430	507295.728491	43.769255
3503.289124	507279.110919	43.774260
3503.595372	507262.061445	43.779265
3503.688509	507252.382424	43.784269
3503.672015	507252.789829	43.789274
3503.823157	507258.078791	43.794279
3503.394933	507228.799344	43.799284
3503.231032	507224.372587	43.804289
3503.417984	507224.140653	43.809293
3503.253578	507212.883162	43.814298
3503.378011	507210.535968	43.819303
3503.502654	507225.594660	43.824308
3503.622073	507205.842339	43.829313
3503.173296	507195.995949	43.834317
3503.512973	507175.449798	43.839322
3503.701977	507183.819320	43.844327
3503.172340	507190.784469	43.849332
3503.478540	507178.238202	43.854337
3503.538660	507178.076914	43.859341
3503.427748	507167.418123	43.864346
3503.311431	507141.529941	43.869351
3503.053206	507146.782446	43.874356
3503.312961	507144.160859	43.879361
3503.209458	507145.695194	43.884365
3503.473718	507144.793255	43.889370
3503.592028	507145.078158	43.894375
3503.341744	507157.919224	43.899380
3503.368583	507140.458406	43.904385
3503.527613	507130.313512	43.909389
3503.316140	507120.429570	43.914394
3503.644032	507107.930423	43.919399
3503.579639	507102.425329	43.924404
3503.792347	507108.109397	43.929409
3503.631668	507096.901841	43.934413
3503.645336	507076.609499	43.939418
3503.865046	507065.038203	43.944423
3503.481947	507076.888341	43.949428
3503.663025	507059.605459	43.954433
3503.782828	507037.373531	43.959437
3503.619322	507019.689682	43.964442
3503.702952	507031.061285	43.969447
3503.454337	507021.436153	43.974452
3503.805336	506998.611041	43.979457
3503.767410	507000.792813	43.984461
3503.618974	506994.137186	43.989466
3503.953806	506973.338566	43.994471
3503.448038	506954.899162	43.999476
3503.427574	506954.042218	44.004481
3503.404604	506955.715638	44.009485
3503.489847	506948.820660	44.014490
3503.615600	506946.372023	44.019495
3503.612770	506934.937014	44.024500
3503.525852	506915.773571	44.029505
3503.520175	506908.336353	44.034509
3503.197184	506912.030581	44.039514
3503.728179	506915.235627	44.044519
3503.420820	506900.306766	44.049524
3503.494014	506875.906219	44.054529
3503.317001	506866.978078	44.059533
3503.236770	506871.544735	44.064538
3503.623800	506867.233203	44.069543
3503.471929	506875.909752	44.074548
3503.707771	506859.832405	44.079553
3503.583455	506844.166168	44.084557
3503.356629	506828.111323	44.089562
3503.432301	506831.287156	44.094567
3503.286850	506828.021174	44.099572
3503.396805	506830.837390	44.104577
3503.295361	506821.340683	44.109581
3503.691282	506820.013119	44.114586
3503.497894	506798.235187	44.119591
3503.321307	506808.281871	44.124596
3503.355645	506798.763690	44.129601
3503.697377	506793.143704	44.134605
3503.097478	506801.182710	44.139610
3503.586524	506783.446076	44.144615
3503.105731	506780.334290	44.149620
3503.329947	506774.277474	44.154625
3503.763125	506769.351424	44.159629
3503.731612	506761.817028	44.164634
3503.691538	506763.138971	44.169639
3503.413726	506749.014908	44.174644
3503.655731	506724.233265	44.179649
3503.531266	506729.363552	44.184653
3503.299362	506734.612020	44.189658
3503.538124	506725.820487	44.194663
3503.463114	506725.326354	44.199668
3503.534526	506716.915468	44.204673
3503.557747	506698.290976	44.209677
3503.425046	506694.061552	44.214682
3503.675200	506690.480013	44.219687
3503.486976	506686.512363	44.224692
3503.798995	506681.605440	44.229697
3503.689231	506659.712916	44.234701
3503.562783	506642.528827	44.239706
3503.433435	506639.867468	44.244711
3503.566918	506639.947580	44.249716
3503.406664	506625.248232	44.254721
3503.449097	506613.907058	44.259725
3503.437624	506612.087269	44.264730
3503.798866	506605.705133	44.269735
3503.318874	506617.520298	44.274740
3503.683047	506606.381266	44.279745
3503.451456	506584.254901	44.284749
3503.273969	506580.791534	44.289754
3503.386560	506573.284879	44.294759
3503.366970	506566.355719	44.299764
3503.283346	506566.571350	44.304769
3503.583093	506567.282989	44.309773
3503.399224	506568.425273	44.314778
3503.480887	506535.623225	44.319783
3503.518798	506538.096672	44.324788
3503.567204	506541.125066	44.329793
3503.923668	506536.919485	44.334797
3503.668925	506518.541138	44.339802
3503.990156	506504.423391	44.344807
3503.481001	506495.547557	44.349812
3503.532320	506491.946806	44.354817
3503.592238	506489.559112	44.359821
3503.435147	506464.688379	44.364826
3503.599497	506448.065343	44.369831
3503.317263	506463.745618	44.374836
3503.622577	506453.172400	44.379841
3503.462834	506459.219158	44.384845
3503.483965	506439.329698	44.389850
3503.763030	506417.577812	44.394855
3503.577745	506427.828495	44.399860
3503.740794	506415.709114	44.404865
3503.574506	506418.063051	44.409869
3503.513725	506396.010649	44.414874
3503.453402	506372.946125	44.419879
3503.247755	506384.616881	44.424884
3503.525851	506365.597539	44.429889
3503.477414	506386.554042	44.434893
3503.262393	506382.995366	44.439898
3503.598177	506361.386248	44.444903
3503.349143	506346.700696	44.449908
3503.401319	506335.155396	44.454913
3503.392002	506333.234035	44.459917
3503.452673	506334.135277	44.464922
3503.430383	506324.018572	44.469927
3503.330813	506336.684618	44.474932
3503.483000	506324.566890	44.479937
3503.702228	506302.014699	44.484941
3503.446512	506312.327183	44.489946
3503.486974	506300.176496	44.494951
3503.360225	506300.854358	44.499956
3503.504728	506297.846052	44.504961
3503.425565	506278.326470	44.509965
3503.323621	506269.588561	44.514970
3503.587998	506253.000129	44.519975
3503.408713	506263.654771	44.524980
3503.476117	506260.051429	44.529985
3503.789042	506262.633250	44.534989
3503.329574	506241.453292	44.539994
3503.650928	506223.034174	44.544999
3503.497706	506238.188244	44.550004
3503.862025	506216.068421	44.555009
3503.836823	506215.110987	44.560013
3503.618348	506186.403842	44.565018
3503.836272	506179.436985	44.570023
3503.529006	506181.459027	44.575028
3503.297296	506171.223530	44.580033
3503.678831	506158.462216	44.585037
3503.441164	506149.340885	44.590042
3503.429826	506152.378790	44.595047
3503.296305	506159.838354	44.600052
3503.366356	506152.540649	44.605057
3503.591936	506151.695376	44.610061
3503.391298	506134.573113	44.615066
3503.714873	506113.421033	44.620071
3503.482005	506109.055493	44.625076
3503.492761	506115.328429	44.630081
3503.619488	506104.125405	44.635085
3503.392469	506101.023984	44.640090
3503.639037	506077.556348	44.645095
3503.083020	506077.340633	44.650100
3503.450842	506064.783825	44.655105
3503.100151	506082.600545	44.660109
3503.367405	506073.045151	44.665114
3503.671931	506074.110270	44.670119
3503.632472	506067.538265	44.675124
3503.476277	506047.322172	44.680129
3503.582309	506041.840405	44.685133
3503.499948	506027.482453	44.690138
3503.580308	506032.732376	44.695143
3503.168345	506035.783023	44.700148
3503.296895	506027.514580	44.705153
3503.269765	506012.388854	44.710157
3503.088280	505996.629685	44.715162
3503.543734	505996.557705	44.720167
3503.389420	505996.278494	44.725172
3503.314145	506001.249413	44.730177
3503.061451	506001.289366	44.735181
3503.093403	506001.081917	44.740186
3503.552464	505994.279280	44.745191
3503.444854	506003.303483	44.750196
3503.315713	505975.644515	44.755201
3503.493110	505968.683980	44.760205
3503.132281	505962.618153	44.765210
3503.562692	505958.400746	44.770215
3503.465506	505957.960697	44.775220
3503.604899	505962.695288	44.780225
3503.500502	505963.369629	44.785229
3503.130819	505944.452217	44.790234
3503.180339	505935.032369	44.795239
3503.236654	505928.293366	44.800244
3503.426878	505924.366927	44.805249
3503.479972	505926.939266	44.810253
3503.256374	505931.630036	44.815258
3503.892402	505924.748798	44.820263
3503.557337	505927.433092	44.825268
3503.591438	505892.006027	44.830273
3503.840606	505890.549784	44.835277
3503.406496	505880.953338	44.840282
3503.756598	505873.408839	44.845287
3503.379574	505864.663604	44.850292
3503.372472	505846.093595	44.855297
3503.512344	505839.341351	44.860301
3503.089909	505852.564807	44.865306
3503.505846	505844.959288	44.870311
3503.584476	505851.879424	44.875316
3503.529903	505847.637444	44.880321
3503.438053	505820.124142	44.885325
3503.337491	505799.797763	44.890330
3503.411507	505803.581279	44.895335
3503.291546	505809.166549	44.900340
3503.453461	505802.562614	44.905345
3503.041524	505805.259078	44.910349
3503.039396	505812.698022	44.915354
3503.309115	505802.889078	44.920359
3503.099079	505806.970504	44.925364
3503.446606	505798.262518	44.930369
3503.383630	505781.118148	44.935373
3503.136887	505784.800560	44.940378
3503.167980	505768.805173	44.945383
3503.123091	505766.029123	44.950388
3503.288777	505767.318618	44.955393
3503.174121	505769.613878	44.960397
3503.061914	505774.843714	44.965402
3503.257846	505770.815133	44.970407
3503.036608	505764.018732	44.975412
3502.948977	505774.102555	44.980417
3502.957132	505773.241029	44.985421
3502.973927	505773.845618	44.990426
3503.449167	505772.910263	44.995431
3503.201574	505783.575995	45.000436
3503.202282	505777.857779	45.005441
3503.381866	505785.622232	45.010445
3503.204082	505786.409386	45.015450
3503.453076	505771.290408	45.020455
3503.144121	505768.910318	45.025460
3503.223535	505751.541001	45.030465
3503.283426	505745.712214	45.035469
3503.103576	505742.350259	45.040474
3503.221337	505733.020720	45.045479
3502.867813	505747.852657	45.050484
3503.223660	505751.541034	45.055489
3503.551517	505740.356587	45.060493
3503.214459	505750.176232	45.065498
3503.477434	505738.242996	45.070503
3503.038764	505753.594416	45.075508
3503.676869	505740.083801	45.080513
3503.333629	505734.268128	45.085517
3503.268464	505718.540924	45.090522
3503.378229	505708.352386	45.095527
3503.403240	505713.914772	45.100532
3503.346726	505724.955161	45.105537
3503.408967	505702.275199	45.110541
3503.197675	505721.234123	45.115546
3503.388549	505711.893017	45.120551
3503.411074	505706.980977	45.125556
3503.257552	505682.715798	45.130561
3503.434641	505678.437159	45.135565
3503.261877	505674.466833	45.140570
3503.517769	505670.732370	45.145575
3503.268794	505671.783797	45.150580
3503.499683	505680.299234	45.155585
3503.575149	505673.658312	45.160589
3503.220475	505658.584052	45.165594
3503.576166	505630.544283	45.170599
3503.659297	505629.063660	45.175604
3503.864698	505628.727585	45.180609
3503.693188	505631.082453	45.185613
3503.509323	505598.674833	45.190618
3503.654307	505586.709541	45.195623
3503.071782	505594.695748	45.200628
3503.342695	505584.026236	45.205633
3503.577539	505580.851718	45.210637
3503.349207	505591.767539	45.215642
3503.429633	505578.243742	45.220647
3503.334495	505578.815428	45.225652
3503.662634	505562.772899	45.230657
3503.536910	505573.925530	45.235661
3503.359405	505563.529298	45.240666
3503.819922	505561.482984	45.245671
3503.714217	505531.542453	45.250676
3503.462098	505527.230412	45.255681
3503.787483	505518.525787	45.260685
3503.037644	505528.107180	45.265690
3503.567742	505514.309843	45.270695
3503.425784	505510.182800	45.275700
3503.193052	505489.472122	45.280705
3503.096605	505476.836465	45.285709
3503.639156	505490.059477	45.290714
3503.615790	505483.788330	45.295719
3503.519039	505483.955444	45.300724
3503.412369	505483.010846	45.305729
3503.510627	505449.748698	45.310733
3503.542173	505436.232517	45.315738
3503.711126	505438.584200	45.320743
3503.377109	505446.328779	45.325748
3503.673375	505438.387773	45.330753
3503.583712	505425.599196	45.335757
3503.283611	505413.602930	45.340762
3503.739103	505404.928287	45.345767
3503.562465	505410.623851	45.350772
3503.552856	505410.726588	45.355777
3503.355025	505388.087326	45.360781
3503.097637	505373.402272	45.365786
3503.526232	505365.288505	45.370791
3503.239544	505357.338399	45.375796
3503.262309	505368.518294	45.380801
3503.426211	505359.535491	45.385805
3503.219105	505376.267551	45.390810
3503.798097	505354.213913	45.395815
3503.421972	505353.919147	45.400820
3503.217631	505328.801240	45.405825
3503.504893	505331.336654	45.410829
3503.476023	505328.659211	45.415834
3503.395186	505321.486216	45.420839
3503.240233	505329.455563	45.425844
3503.451106	505330.636740	45.430849
3503.663504	505319.065442	45.435853
3503.536557	505303.904275	45.440858
3503.573070	505280.013332	45.445863
3503.276747	505289.826795	45.450868
3503.652025	505283.694982	45.455873
3503.595304	505279.858036	45.460877
3503.402742	505267.591650	45.465882
3503.617938	505255.260804	45.470887
3503.307720	505247.516784	45.475892
3503.829399	505241.412420	45.480897
3503.920174	505236.894294	45.485901
3503.708661	505226.756258	45.490906
3503.747750	505209.089149	45.495911
3503.850182	505206.846374	45.500916
3503.689228	505194.473731	45.505921
3503.403712	505171.139585	45.510925
3503.096854	505164.002251	45.515930
3503.298605	505150.205923	45.520935
3503.254843	505164.078508	45.525940
3503.527163	505161.404037	45.530945
3503.460580	505149.724911	45.535949
3503.331362	505157.943291	45.540954
3503.326935	505121.711078	45.545959
3503.724646	505109.756118	45.550964
3503.545629	505120.006577	45.555969
3503.636041	505107.492932	45.560973
3503.518288	505118.593988	45.565978
3503.685830	505101.564328	45.570983
3503.108454	505091.939485	45.575988
3503.450049	505083.991155	45.580993
3503.712891	505073.525027	45.585997
3503.310016	505085.278430	45.591002
3503.326228	505091.196638	45.596007
3503.273801	505084.019055	45.601012
3503.322426	505071.208360	45.606017
3503.091818	505052.976465	45.611021
3503.264550	505039.791896	45.616026
3503.465738	505036.976834	45.621031
3502.990067	505045.098215	45.626036
3503.269999	505043.232201	45.631041
3503.341749	505043.170265	45.636045
3503.092165	505044.829084	45.641050
3503.683339	505042.610244	45.646055
3503.549278	505039.493940	45.651060
3503.732466	505032.936957	45.656065
3503.453392	505009.652182	45.661069
3503.250053	505002.953864	45.666074
3503.779370	505001.099032	45.671079
3503.650879	505007.900427	45.676084
3503.197306	504989.501288	45.681089
3503.552598	504965.863158	45.686093
3503.337023	504972.324096	45.691098
3503.490704	504957.624322	45.696103
3503.448916	504954.898259	45.701108
3503.280935	504960.137153	45.706113
3503.525123	504962.426404	45.711117
3503.260701	504950.171153	45.716122
3503.380464	504931.478908	45.721127
3503.237936	504940.559784	45.726132
3503.343581	504928.701471	45.731137
3503.631826	504925.315973	45.736141
3503.427406	504931.016083	45.741146
3503.862148	504916.120034	45.746151
3503.547526	504906.504162	45.751156
3503.403907	504884.007493	45.756161
3503.631758	504880.985771	45.761165
3503.060014	504889.729673	45.766170
3503.152317	504883.844871	45.771175
3503.310119	504895.813410	45.776180
3503.226588	504879.430483	45.781185
3503.352746	504889.025575	45.786189
3503.233285	504867.587780	45.791194
3503.301249	504866.615544	45.796199
3503.437017	504856.270584	45.801204
3503.108570	504853.994659	45.806209
3503.184278	504846.037642	45.811213
3503.116282	504852.323480	45.816218
3503.479698	504836.628950	45.821223
3502.984649	504860.188154	45.826228
3503.225908	504852.356789	45.831233
3503.221105	504856.254180	45.836237
3503.200792	504858.332225	45.841242
3503.351140	504846.466791	45.846247
3503.414664	504856.021195	45.851252
3503.417912	504830.313099	45.856257
3503.557826	504825.078623	45.861261
3503.261538	504816.168281	45.866266
3503.852604	504816.327893	45.871271
3503.460226	504812.493295	45.876276
3503.310839	504801.586108	45.881281
3503.141882	504790.580796	45.886285
3503.215082	504778.828721	45.891290
3503.364582	504779.007524	45.896295
3503.211249	504786.420199	45.901300
3503.578418	504771.686525	45.906305
3503.502825	504775.240883	45.911309
3503.237248	504777.711945	45.916314
3503.565702	504776.698531	45.921319
3503.422355	504765.183098	45.926324
3503.157691	504750.448064	45.931329
3503.290433	504737.725041	45.936333
3502.959998	504736.562742	45.941338
3502.904921	504725.488783	45.946343
3503.119567	504738.359350	45.951348
3502.979657	504733.978770	45.956353
3503.030437	504741.004961	45.961357
3502.778079	504740.538802	45.966362
3503.075985	504742.768985	45.971367
3503.156070	504733.242446	45.976372
3503.353525	504738.929702	45.981377
3503.569394	504735.707426	45.986381
3503.104361	504745.750283	45.991386
3503.271841	504741.472935	45.996391
3503.049864	504744.341956	46.001396
3503.285242	504739.092365	46.006401
3503.482389	504746.196631	46.011405
3503.313946	504744.856910	46.016410
3503.512995	504744.015765	46.021415
3503.474051	504728.435343	46.026420
3503.111290	504710.426402	46.031425
3503.434586	504705.517145	46.036429
3503.345849	504707.150571	46.041434
3503.305215	504707.106398	46.046439
3503.274595	504715.309401	46.051444
3503.154662	504708.192940	46.056449
3503.315399	504703.056348	46.061453
3503.018054	504727.394175	46.066458
3503.383798	504701.527381	46.071463
3503.599606	504696.179658	46.076468
3503.177853	504676.408799	46.081473
3503.287120	504674.569723	46.086477
3503.257539	504670.121082	46.091482
3503.450338	504669.888194	46.096487
3503.545712	504675.490395	46.101492
3503.317331	504668.441665	46.106497
3503.727203	504668.123859	46.111501
3503.101333	504639.883412	46.116506
3503.481115	504636.736421	46.121511
3503.323566	504630.283753	46.126516
3503.558826	504623.313538	46.131521
3503.638867	504629.677269	46.136525
3503.278497	504637.476975	46.141530
3503.212994	504608.338205	46.146535
3503.150550	504603.995954	46.151540
3503.087460	504590.190441	46.156545
3503.395433	504588.876617	46.161549
3502.873329	504591.084615	46.166554
3503.137676	504588.461924	46.171559
3503.041392	504584.125017	46.176564
3503.003191	504587.673502	46.181569
3503.543172	504596.241826	46.186573
3503.181453	504594.375975	46.191578
3503.615567	504578.214583	46.196583
3503.218311	504597.912605	46.201588
3503.324375	504591.114617	46.206593
3503.648735	504590.607902	46.211597
3502.986877	504581.451586	46.216602
3503.316682	504555.286619	46.221607
3503.659450	504555.687908	46.226612
3503.620501	504547.394635	46.231617
3503.410407	504554.411529	46.236621
3503.335466	504557.611583	46.241626
3503.479048	504550.301587	46.246631
3503.243279	504537.990911	46.251636
3503.294854	504528.620587	46.256641
3503.532310	504516.741161	46.261645
3503.261907	504505.954130	46.266650
3503.305776	504509.843905	46.271655
3503.371868	504506.645261	46.276660
3503.321149	504505.742372	46.281665
3503.526914	504501.054062	46.286669
3503.180465	504508.649199	46.291674
3503.570437	504497.656569	46.296679
3503.253222	504477.413503	46.301684
3503.090845	504475.111277	46.306689
3503.321520	504472.240859	46.311693
3503.365774	504481.241842	46.316698
3503.585654	504480.802245	46.321703
3503.662293	504482.510764	46.326708
3503.384395	504470.105487	46.331713
3503.463723	504445.902998	46.336717
3503.057943	504439.590709	46.341722
3503.255776	504427.616272	46.346727
3503.319060	504446.077715	46.351732
3503.105326	504434.876831	46.356737
3503.278682	504437.835234	46.361741
3503.060717	504440.956703	46.366746
3503.471046	504437.096356	46.371751
3503.109079	504440.038160	46.376756
3503.259405	504438.648029	46.381761
3503.296486	504435.099712	46.386765
3503.411280	504445.455943	46.391770
3503.895171	504411.472981	46.396775
3503.317834	504410.653327	46.401780
3503.241110	504406.110857	46.406785
3503.472885	504396.509551	46.411789
3503.019173	504403.008338	46.416794
3503.305060	504396.232459	46.421799
3503.289901	504413.289345	46.426804
3503.481528	504384.767448	46.431809
3503.550297	504367.702082	46.436813
3503.338628	504361.915758	46.441818
3503.393388	504351.836339	46.446823
3503.318723	504357.465519	46.451828
3503.285571	504367.288505	46.456833
3503.381196	504351.939512	46.461837
3503.412265	504358.766544	46.466842
3503.791830	504357.846242	46.471847
3503.414958	504343.179208	46.476852
3503.504541	504327.173257	46.481857
3503.182134	504341.697822	46.486861
3503.072485	504325.014863	46.491866
3503.389677	504330.936362	46.496871
3503.456333	504339.225379	46.501876
3503.359460	504325.020142	46.506881
3503.624975	504291.830571	46.511885
3503.618800	504291.477308	46.516890
3503.239335	504292.448225	46.521895
3503.397004	504285.945606	46.526900
3503.386647	504299.206310	46.531905
3503.635801	504287.324880	46.536909
3503.120689	504263.114885	46.541914
3503.542165	504259.455166	46.546919
3503.448051	504248.032825	46.551924
3503.381423	504250.978585	46.556929
3503.267826	504246.290080	46.561933
3503.301607	504244.260462	46.566938
3503.282125	504253.625887	46.571943
3503.233116	504246.649849	46.576948
3503.329953	504231.047522	46.581953
3503.431329	504222.175235	46.586957
3503.380699	504214.490938	46.591962
3503.336949	504217.584910	46.596967
3503.311404	504211.769117	46.601972
3503.104456	504227.945567	46.606977
3503.088105	504207.249774	46.611981
3503.333473	504218.192789	46.616986
3503.220668	504209.455564	46.621991
3503.298282	504228.674081	46.626996
3503.278650	504215.165048	46.632001
3503.207560	504192.909064	46.637005
3503.137427	504183.760222	46.642010
3503.265360	504180.855389	46.647015
3503.224652	504185.669537	46.652020
3503.113575	504171.466421	46.657025
3502.962223	504177.462031	46.662029
3502.938286	504183.133856	46.667034
3503.480267	504181.074510	46.672039
3503.438490	504184.977894	46.677044
3503.247921	504184.248915	46.682049
3503.258973	504177.415179	46.687053
3503.114985	504191.557413	46.692058
3502.995758	504192.234165	46.697063
3502.952867	504189.913016	46.702068
3502.777912	504199.707903	46.707073
3502.666871	504193.045293	46.712077
3502.772584	504187.411174	46.717082
3503.455887	504190.542052	46.722087
3503.173599	504193.015836	46.727092
3503.033355	504186.610876	46.732097
3503.393862	504191.462820	46.737101
3502.923608	504198.976444	46.742106
3503.389728	504196.979698	46.747111
3503.287143	504191.429113	46.752116
3503.178488	504197.924041	46.757121
3503.326752	504199.975518	46.762125
3503.017178	504189.042662	46.767130
3503.459229	504172.879643	46.772135
3503.249797	504158.641456	46.777140
3503.254086	504142.750034	46.782145
3503.416588	504144.748659	46.787149
3503.093680	504160.032565	46.792154
3503.332765	504150.429971	46.797159
3503.242607	504149.786334	46.802164
3503.375294	504145.058874	46.807169
3503.105598	504145.860626	46.812173
3503.247982	504155.554771	46.817178
3503.446293	504149.501144	46.822183
3503.339581	504144.507878	46.827188
3503.331208	504121.533385	46.832193
3503.427246	504117.267178	46.837197
3503.024946	504118.342930	46.842202
3503.185492	504120.139437	46.847207
3503.763949	504122.629001	46.852212
3503.492553	504113.663758	46.857217
3503.531640	504112.139362	46.862221
3503.022140	504099.365569	46.867226
3503.020486	504078.869733	46.872231
3503.312031	504077.760898	46.877236
3503.431533	504075.920142	46.882241
3503.753712	504077.134421	46.887245
3503.308307	504085.605712	46.892250
3503.356090	504078.816738	46.897255
3503.655625	504078.263326	46.902260
3503.529672	504058.748660	46.907265
3503.685160	504050.171379	46.912269
3503.417572	504036.701401	46.917274
3503.549942	504034.352529	46.922279
3503.836677	504038.001588	46.927284
3503.632744	504026.191599	46.932289
3503.814430	504004.502716	46.937293
3503.379441	504001.939870	46.942298
3503.330042	504003.465927	46.947303
3503.505870	504002.679026	46.952308
3503.280598	503969.718247	46.957313
3503.724925	503962.765334	46.962317
3503.261652	503960.966073	46.967322
3503.469547	503952.734718	46.972327
3503.765097	503957.900643	46.977332
3503.567928	503957.678779	46.982337
3503.788798	503924.090706	46.987341
3503.526611	503916.996408	46.992346
3503.333260	503916.369074	46.997351
3503.258034	503916.836449	47.002356
3503.245557	503910.208760	47.007361
3503.398075	503916.257645	47.012365
3503.416771	503906.386104	47.017370
3503.279705	503882.824342	47.022375
3503.465952	503881.124840	47.027380
3502.939744	503875.944764	47.032385
3503.483748	503877.781902	47.037389
3503.104952	503877.740570	47.042394
3503.333873	503880.690285	47.047399
3503.500175	503880.410968	47.052404
3503.348936	503875.475272	47.057409
3503.526850	503868.361999	47.062413
3503.289395	503857.974227	47.067418
3503.175701	503838.558595	47.072423
3503.422886	503835.989115	47.077428
3503.190933	503838.151341	47.082433
3503.299036	503832.061256	47.087437
3503.388120	503843.079817	47.092442
3503.396900	503838.422467	47.097447
3503.584533	503833.989889	47.102452
3503.441604	503818.678137	47.107457
3503.323180	503796.935217	47.112461
3503.033677	503809.076419	47.117466
3503.087414	503791.051307	47.122471
3503.271507	503794.514207	47.127476
3503.158436	503789.977323	47.132481
3503.191180	503785.721040	47.137485
3503.535731	503798.926024	47.142490
3503.389799	503799.556403	47.147495
3503.282579	503800.079447	47.152500
3503.223115	503786.475163	47.157505
3503.599833	503745.878135	47.162509
3503.176825	503763.455597	47.167514
3503.132855	503757.389523	47.172519
3503.409930	503759.218257	47.177524
3503.079772	503757.954629	47.182529
3503.321591	503754.019552	47.187533
3503.230897	503747.859643	47.192538
3503.390299	503752.338628	47.197543
3503.205608	503758.845737	47.202548
3503.491193	503752.525136	47.207553
3503.116604	503737.249930	47.212557
3502.780154	503732.545904	47.217562
3503.053506	503727.036966	47.222567
3503.419790	503719.337162	47.227572
3502.882558	503727.064008	47.232577
3503.067198	503717.672218	47.237581
3502.825891	503731.475944	47.242586
3502.804966	503724.039781	47.247591
3502.999065	503740.507548	47.252596
3502.668386	503753.009558	47.257601
3503.196704	503751.711453	47.262605
3502.831066	503766.546976	47.267610
3502.853625	503761.583777	47.272615
3503.021521	503757.306125	47.277620
3503.109882	503758.658602	47.282625
3503.490027	503769.833636	47.287629
3503.141192	503763.006015	47.292634
3503.461148	503764.423102	47.297639
3503.209334	503744.776155	47.302644
3502.896707	503744.167668	47.307649
3503.349380	503734.379260	47.312653
3502.927545	503736.571513	47.317658
3503.144541	503735.120181	47.322663
3503.254518	503737.582633	47.327668
3503.151159	503739.218459	47.332673
3502.920009	503741.431180	47.337677
3503.015297	503741.466737	47.342682
3503.125957	503735.932910	47.347687
3502.827630	503743.723203	47.352692
3502.600834	503747.251060	47.357697
3503.098240	503732.344105	47.362701
3502.884732	503744.220296	47.367706
3503.109118	503755.622394	47.372711
3503.320650	503758.018183	47.377716
3503.049918	503756.593337	47.382721
3503.568524	503742.796430	47.387725
3502.927131	503754.537812	47.392730
3503.271572	503743.855562	47.397735
3503.139471	503748.532449	47.402740
3503.138510	503749.139916	47.407745
3503.505324	503750.448380	47.412749
3503.038209	503750.674050	47.417754
3502.937273	503753.068622	47.422759
3503.352561	503764.794800	47.427764
3503.640435	503751.844108	47.432769
3503.498613	503748.779408	47.437773
3503.284111	503716.271928	47.442778
3503.271517	503710.453922	47.447783
3503.387558	503703.097319	47.452788
3503.228871	503714.509385	47.457793
3503.417380	503706.534023	47.462797
3503.599694	503712.375833	47.467802
3503.544238	503713.902872	47.472807
3503.407149	503697.021219	47.477812
3503.139813	503682.538753	47.482817
3503.240934	503662.026186	47.487821
3503.150748	503675.350588	47.492826
3503.315132	503662.469959	47.497831
3503.395601	503674.198512	47.502836
3503.224417	503670.682959	47.507841
3503.259963	503671.993182	47.512845
3503.543479	503672.606294	47.517850
3503.240464	503682.118058	47.522855
3503.164951	503676.056941	47.527860
3503.401894	503655.775942	47.532865
3503.583398	503637.528042	47.537869
3503.270956	503642.334682	47.542874
3503.481564	503630.307075	47.547879
3503.386713	503637.407336	47.552884
3503.409322	503633.000791	47.557889
3503.582226	503634.744786	47.562893
3503.702415	503612.559051	47.567898
3503.499769	503600.697963	47.572903
3503.641862	503592.476840	47.577908
3503.555889	503585.810037	47.582913
3503.507850	503581.161601	47.587917
3503.348750	503557.754714	47.592922
3503.272472	503560.449069	47.597927
3503.087531	503545.497983	47.602932
3503.149360	503560.468549	47.607937
3503.341524	503539.992058	47.612941
3503.502832	503546.646992	47.617946
3503.365951	503549.705193	47.622951
3503.391956	503555.976636	47.627956
3503.185200	503546.545403	47.632961
3503.444256	503540.228919	47.637965
3503.434268	503530.462920	47.642970
3503.629701	503513.579140	47.647975
3503.395407	503511.693029	47.652980
3503.219829	503509.139716	47.657985
3503.544823	503511.466996	47.662989
3503.212135	503515.618948	47.667994
3503.098587	503505.160773	47.672999
3503.282983	503493.289044	47.678004
3503.290952	503484.481759	47.683009
3503.441424	503472.109284	47.688013
3503.481073	503474.481672	47.693018
3503.479198	503466.030199	47.698023
3503.688959	503467.312900	47.703028
3503.360767	503474.146453	47.708033
3503.132756	503441.539382	47.713037
3503.377710	503442.664694	47.718042
3503.383439	503434.718100	47.723047
3503.215482	503434.542220	47.728052
3502.991311	503442.320925	47.733057
3503.419138	503423.021677	47.738061
3502.988031	503429.770295	47.743066
3503.264195	503433.927248	47.748071
3503.130979	503428.583701	47.753076
3503.100030	503431.270911	47.758081
3503.231737	503422.646474	47.763085
3503.073301	503434.311730	47.768090
3503.169781	503427.160542	47.773095
3503.268797	503432.307078	47.778100
3503.376626	503430.113833	47.783105
3503.588823	503421.375454	47.788109
3503.318489	503413.017000	47.793114
3503.141996	503397.608967	47.798119
3503.494898	503399.425754	47.803124
3503.532078	503393.194898	47.808129
3503.497854	503397.046654	47.813133
3503.500301	503392.491407	47.818138
3503.161037	503367.999332	47.823143
3503.427113	503364.971310	47.828148
3503.374612	503358.855837	47.833153
3503.503225	503344.158677	47.838157
3503.287458	503347.431821	47.843162
3503.214832	503349.973801	47.848167
3503.330660	503356.231118	47.853172
3502.899043	503362.170085	47.858177
3502.902395	503343.899431	47.863181
3503.203395	503359.793950	47.868186
3503.302417	503357.652698	47.873191
3503.173170	503352.308500	47.878196
3503.129096	503358.742920	47.883201
3503.314830	503347.376979	47.888205
3503.176161	503324.978749	47.893210
3503.353949	503317.106126	47.898215
3503.414308	503309.302670	47.903220
3503.306555	503314.431314	47.908225
3503.237624	503299.664122	47.913229
3503.188646	503308.781662	47.918234
3503.072617	503301.765232	47.923239
3503.218209	503310.396527	47.928244
3503.251062	503307.557190	47.933249
3503.213896	503307.006366	47.938253
3503.362853	503312.752362	47.943258
3503.280982	503305.882364	47.948263
3503.249916	503280.582303	47.953268
3503.504291	503292.435452	47.958273
3503.350289	503272.063977	47.963277
3503.361754	503275.048167	47.968282
3503.233034	503271.120941	47.973287
3503.298595	503280.119172	47.978292
3503.123930	503285.359620	47.983297
3503.305259	503270.856507	47.988301
3503.308100	503271.716439	47.993306
3503.163883	503273.864866	47.998311
3503.317444	503252.381942	48.003316
3503.116815	503249.174620	48.008321
3503.291184	503232.243290	48.013325
3503.342484	503249.240191	48.018330
3503.076755	503241.184587	48.023335
3503.253098	503232.654223	48.028340
3503.062468	503243.413711	48.033345
3503.303912	503243.527389	48.038349
3503.206410	503244.200742	48.043354
3502.984623	503233.810125	48.048359
3503.504397	503243.242680	48.053364
3503.523661	503232.510300	48.058369
3503.333723	503240.637953	48.063373
3503.318948	503209.008949	48.068378
3503.201127	503213.886162	48.073383
3503.450975	503206.963693	48.078388
3503.035835	503211.989122	48.083393
3503.393997	503205.201363	48.088397
3503.181364	503209.739291	48.093402
3503.301456	503200.357430	48.098407
3503.218163	503213.681091	48.103412
3502.999810	503202.834421	48.108417
3503.258419	503211.751562	48.113421
3503.271112	503213.824584	48.118426
3503.215184	503203.407732	48.123431
3503.163101	503196.026881	48.128436
3502.982549	503183.605307	48.133441
3503.016822	503179.247415	48.138445
3503.255546	503190.445173	48.143450
3503.202023	503175.118729	48.148455
3503.288676	503166.400068	48.153460
3503.197850	503165.503449	48.158465
3503.412396	503161.117059	48.163469
3503.010903	503173.630671	48.168474
3502.885684	503169.146156	48.173479
3503.324270	503164.876185	48.178484
3502.748068	503173.419196	48.183489
3503.091968	503170.834333	48.188493
3503.140240	503176.596288	48.193498
3502.931163	503167.519490	48.198503
3502.865181	503177.398941	48.203508
3503.283011	503171.664553	48.208513
3503.431278	503161.367231	48.213517
3503.229203	503179.973169	48.218522
3502.758170	503175.695147	48.223527
3503.384078	503164.512565	48.228532
3503.217545	503175.470727	48.233537
3503.188440	503169.351490	48.238541
3503.225864	503168.130937	48.243546
3503.279354	503184.975723	48.248551
3503.302744	503167.359652	48.253556
3503.389529	503153.377489	48.258561
3503.210807	503144.194660	48.263565
3503.373233	503145.990971	48.268570
3503.261282	503140.390924	48.273575
3503.322964	503143.873302	48.278580
3503.104507	503145.527375	48.283585
3503.327077	503149.237374	48.288589
3503.378263	503148.368917	48.293594
3503.167076	503154.829826	48.298599
3503.325754	503143.316199	48.303604
3503.302287	503130.869758	48.308609
3503.217273	503118.635478	48.313613
3502.831016	503114.394652	48.318618
3503.321798	503106.674903	48.323623
3503.338116	503106.419282	48.328628
3503.339246	503113.352751	48.333633
3503.301877	503104.248780	48.338637
3503.291294	503116.903085	48.343642
3503.366751	503108.692270	48.348647
3503.380630	503108.335814	48.353652
3503.284928	503121.155402	48.358657
3503.644799	503101.967766	48.363661
3503.410568	503084.797218	48.368666
3503.380511	503078.222605	48.373671
3503.371365	503063.698818	48.378676
3503.343258	503069.675324	48.383681
3503.300478	503072.566901	48.388685
3503.400670	503071.184588	48.393690
3503.321777	503073.727599	48.398695
3503.289507	503046.453579	48.403700
3503.226228	503040.845806	48.408705
3503.534689	503030.877363	48.413709
3503.167619	503035.540968	48.418714
3503.238274	503036.187750	48.423719
3503.529717	503028.904362	48.428724
3503.272491	503037.397019	48.433729
3503.289675	503026.968507	48.438733
3503.277400	503026.363129	48.443738
3503.344953	503020.633448	48.448743
3503.491624	503006.742926	48.453748
3503.277915	502990.125760	48.458753
3503.337237	502983.891260	48.463757
3503.246395	502983.652575	48.468762
3503.391766	502984.388770	48.473767
3503.514537	502988.671297	48.478772
3503.468698	502991.765814	48.483777
3503.374874	502969.461265	48.488781
3503.433385	502956.546245	48.493786
3503.452006	502945.206460	48.498791
3503.184216	502945.653686	48.503796
3503.073430	502950.631082	48.508801
3503.238652	502942.810889	48.513805
3503.231526	502949.593894	48.518810
3502.942187	502947.564590	48.523815
3503.104751	502938.074654	48.528820
3503.097231	502940.707624	48.533825
3503.024357	502953.118838	48.538829
3503.276394	502944.778814	48.543834
3503.447310	502950.167181	48.548839
3503.477163	502947.125816	48.553844
3503.250909	502921.349983	48.558849
3503.169830	502906.634993	48.563853
3502.949242	502906.771093	48.568858
3503.285671	502902.213540	48.573863
3503.504541	502911.845669	48.578868
3503.269961	502900.900156	48.583873
3503.267908	502907.277487	48.588877
3503.164123	502909.875066	48.593882
3503.383400	502910.346528	48.598887
3503.315084	502910.154892	48.603892
3502.916392	502900.703040	48.608897
3502.982153	502906.867208	48.613901
3503.087407	502903.510250	48.618906
3502.823489	502909.169806	48.623911
3503.434809	502902.999860	48.628916
3503.111398	502908.921875	48.633921
3503.137329	502896.315626	48.638925
3502.880540	502881.679000	48.643930
3503.092862	502902.497229	48.648935
3503.196405	502876.416146	48.653940
3503.150394	502888.317047	48.658945
3503.267018	502876.911117	48.663949
3503.330528	502873.510141	48.668954
3503.167094	502880.722769	48.673959
3503.518461	502867.457727	48.678964
3503.136204	502881.841118	48.683969
3503.099596	502876.330299	48.688973
3502.943529	502874.279921	48.693978
3503.004149	502874.624628	48.698983
3503.354471	502863.890306	48.703988
3503.187503	502871.710830	48.708993
3503.466339	502873.083880	48.713997
3503.252768	502868.916921	48.719002
3503.062531	502881.296125	48.724007
3503.420610	502877.797977	48.729012
3503.270383	502849.175796	48.734017
3503.443342	502839.127440	48.739021
3503.398948	502840.349138	48.744026
3503.294122	502825.536612	48.749031
3503.527486	502825.550347	48.754036
3503.294779	502843.098643	48.759041
3503.464811	502827.989618	48.764045
3503.184277	502819.581882	48.769050
3502.855268	502799.490579	48.774055
3503.353646	502797.033079	48.779060
3503.662952	502787.368033	48.784065
3503.478895	502790.383210	48.789069
3503.532596	502789.818007	48.794074
3503.688113	502796.069249	48.799079
3503.493417	502790.836449	48.804084
3503.277794	502773.004707	48.809089
3503.506454	502745.334698	48.814093
3503.459429	502748.328222	48.819098
3503.314911	502753.462839	48.824103
3503.453630	502750.353620	48.829108
3503.030559	502746.827085	48.834113
3503.468694	502745.138273	48.839117
3503.490083	502741.946376	48.844122
3503.152821	502729.296193	48.849127
3503.480923	502708.240524	48.854132
3503.069510	502713.316116	48.859137
3503.153232	502708.089895	48.864141
3503.128407	502708.144441	48.869146
3502.963258	502707.512604	48.874151
3503.266722	502696.886811	48.879156
3503.134672	502703.385987	48.884161
3503.261252	502706.959417	48.889165
3503.285728	502714.597916	48.894170
3503.324071	502713.883303	48.899175
3503.662629	502700.721384	48.904180
3502.864467	502701.252448	48.909185
3503.213109	502687.684032	48.914189
3502.828212	502676.002963	48.919194
3503.171988	502680.250632	48.924199
3503.116951	502685.573572	48.929204
3503.345591	502674.706534	48.934209
3503.502091	502673.770796	48.939213
3503.050713	502676.423352	48.944218
3502.884604	502677.563077	48.949223
3503.029121	502673.896199	48.954228
3503.076488	502670.902630	48.959233
3503.068075	502676.471261	48.964237
3503.014292	502684.324590	48.969242
3503.136466	502678.434330	48.974247
3503.408365	502675.759553	48.979252
3503.258919	502682.666380	48.984257
3503.257030	502683.729535	48.989261
3503.278731	502687.977499	48.994266
3502.978053	502682.558971	48.999271
3503.093318	502681.123635	49.004276
3503.033634	502682.094702	49.009281
3503.309194	502683.367061	49.014285
3503.077023	502680.164619	49.019290
3503.034108	502678.197556	49.024295
3503.416295	502681.528142	49.029300
3503.064009	502666.957044	49.034305
3503.496856	502642.898646	49.039309
3503.264529	502646.579431	49.044314
3503.269675	502643.946813	49.049319
3503.461952	502635.008748	49.054324
3503.185799	502636.418928	49.059329
3503.270703	502644.908307	49.064333
3503.473669	502646.040308	49.069338
3503.367678	502644.386882	49.074343
3503.644375	502620.201300	49.079348
3503.419488	502607.229596	49.084353
3503.543709	502601.085927	49.089357
3503.448699	502607.478059	49.094362
3503.321034	502610.180681	49.099367
3503.287609	502602.695409	49.104372
3503.206259	502603.265009	49.109377
3503.368487	502590.485163	49.114381
3503.540984	502572.591871	49.119386
3503.438735	502569.065201	49.124391
3503.464211	502570.124038	49.129396
3502.950146	502562.056764	49.134401
3503.348458	502561.841979	49.139405
3503.501072	502557.617066	49.144410
3503.313391	502566.756912	49.149415
3503.318339	502547.017432	49.154420
3503.218278	502538.277363	49.159425
3503.407448	502535.311968	49.164429
3503.505628	502540.458897	49.169434
3503.505232	502530.083483	49.174439
3503.560511	502524.912315	49.179444
3503.395950	502535.415052	49.184449
3503.688241	502516.085628	49.189453
3503.568131	502497.529940	49.194458
3503.465814	502487.777957	49.199463
3503.909261	502479.306236	49.204468
3503.207115	502488.476829	49.209473
3503.331879	502479.296296	49.214477
3503.373667	502458.488035	49.219482
3503.296333	502450.756577	49.224487
3503.635335	502441.036037	49.229492
3503.169500	502440.907230	49.234497
3503.464059	502435.546377	49.239501
3503.388728	502447.249761	49.244506
3503.319125	502444.578316	49.249511
3503.445816	502427.097016	49.254516
3503.218146	502411.696211	49.259521
3503.177669	502404.768707	49.264525
3503.206963	502401.626111	49.269530
3503.408809	502402.555855	49.274535
3503.564169	502388.157348	49.279540
3503.420593	502412.119776	49.284545
3503.568626	502399.645712	49.289549
3503.514517	502376.979850	49.294554
3503.053500	502363.539164	49.299559
3503.210318	502362.755198	49.304564
3503.256266	502366.341442	49.309569
3503.755597	502364.339247	49.314573
3503.529466	502356.732492	49.319578
3503.427790	502367.529065	49.324583
3503.679888	502341.373099	49.329588
3503.112562	502324.760587	49.334593
3503.329513	502319.260129	49.339597
3503.691160	502313.838024	49.344602
3503.626437	502313.898877	49.349607
3503.483699	502319.185177	49.354612
3503.440514	502308.765783	49.359617
3503.383704	502280.380979	49.364621
3503.297490	502278.825618	49.369626
3503.690279	502277.801898	49.374631
3503.740218	502267.114696	49.379636
3503.264107	502271.795736	49.384641
3503.255001	502247.401756	49.389645
3503.434274	502231.582180	49.394650
3503.207672	502238.298923	49.399655
3503.286069	502228.163942	49.404660
3503.063572	502241.004210	49.409665
3503.228792	502230.653054	49.414669
3503.343815	502228.003007	49.419674
3503.193800	502235.770519	49.424679
3503.365330	502229.467405	49.429684
3503.095236	502230.876659	49.434689
3503.030840	502235.188953	49.439693
3503.229303	502238.396825	49.444698
3503.009545	502247.086390	49.449703
3503.140878	502246.306447	49.454708
3503.068568	502243.939078	49.459713
3503.210735	502234.654441	49.464717
3503.324765	502238.887918	49.469722
3503.179897	502213.857383	49.474727
3503.381396	502197.275067	49.479732
3502.934649	502204.937656	49.484737
3502.965220	502197.644549	49.489741
3503.422874	502201.823721	49.494746
3503.180084	502198.572257	49.499751
3503.448446	502188.913358	49.504756
3503.177225	502194.877973	49.509761
3503.264606	502188.537532	49.514765
3503.583123	502194.661997	49.519770
3503.161777	502203.079768	49.524775
3503.200420	502195.582933	49.529780
3503.062621	502171.867161	49.534785
3503.364448	502164.986684	49.539789
3503.724490	502159.463559	49.544794
3503.486537	502156.160709	49.549799
3503.363383	502153.295232	49.554804
3503.073654	502158.503587	49.559809
3503.561811	502150.328321	49.564813
3503.580896	502155.690317	49.569818
3503.652658	502138.521095	49.574823
3503.711733	502114.622288	49.579828
3503.410772	502114.062510	49.584833
3503.386642	502116.546388	49.589837
3503.486023	502116.075170	49.594842
3503.532491	502095.771877	49.599847
3503.487088	502071.940140	49.604852
3503.041819	502075.148566	49.609857
3502.999012	502070.802586	49.614861
3502.926326	502068.688320	49.619866
3503.326819	502074.344348	49.624871
3503.534352	502061.911254	49.629876
3503.177445	502068.901726	49.634881
3503.140145	502067.288001	49.639885
3503.093254	502070.079164	49.644890
3503.076323	502063.552712	49.649895
3502.979708	502064.782718	49.654900
3502.952423	502081.540096	49.659905
3503.231004	502071.272156	49.664909
3503.188557	502069.861699	49.669914
3502.915558	502082.001475	49.674919
3503.442945	502079.893587	49.679924
3503.178800	502082.415408	49.684929
3502.964215	502063.013769	49.689933
3503.278774	502050.766204	49.694938
3503.362367	502034.657895	49.699943
3503.044185	502032.025679	49.704948
3503.114299	502038.240076	49.709953
3503.006193	502034.410544	49.714957
3503.219301	502032.200486	49.719962
3502.905876	502036.602805	49.724967
3503.263800	502021.311552	49.729972
3503.007891	502043.318303	49.734977
3503.169955	502039.648522	49.739981
3503.122911	502035.708111	49.744986
3503.161681	502035.297084	49.749991
3503.352665	502034.963226	49.754996
3503.246685	502045.001471	49.760001
3502.993842	502035.779168	49.765005
3502.860019	502037.369351	49.770010
3502.911918	502047.129572	49.775015
3503.189180	502040.759065	49.780020
3502.874412	502055.739820	49.785025
3503.104198	502051.047067	49.790029
3503.035478	502038.809463	49.795034
3503.003360	502043.268543	49.800039
3503.328684	502038.763139	49.805044
3502.982481	502050.104691	49.810049
3502.823563	502039.399751	49.815053
3503.220472	502046.372307	49.820058
3502.906052	502048.800852	49.825063
3503.171234	502055.035022	49.830068
3503.284053	502060.787139	49.835073
3503.125375	502043.704863	49.840077
3503.124558	502050.740283	49.845082
3503.167227	502039.041822	49.850087
3503.550056	502041.714453	49.855092
3502.866609	502037.115431	49.860097
3503.035792	502034.051886	49.865101
3503.561342	502033.462690	49.870106
3503.304092	502012.245651	49.875111
3503.543375	501996.011470	49.880116
3503.375703	501996.037984	49.885121
3503.344610	501991.032154	49.890125
3503.355648	501993.712945	49.895130
3502.982011	501993.772015	49.900135
3503.541493	501991.456589	49.905140
3503.068802	502001.400982	49.910145
3503.142921	501986.357013	49.915149
3503.456475	501962.974529	49.920154
3502.938172	501975.254379	49.925159
3503.379926	501952.256527	49.930164
3503.140632	501959.532133	49.935169
3503.229118	501962.909280	49.940173
3503.385767	501958.582359	49.945178
3503.076384	501955.594445	49.950183
3503.352134	501952.463427	49.955188
3503.519247	501956.334285	49.960193
3503.364090	501951.955420	49.965197
3503.231655	501954.608282	49.970202
3503.379334	501933.175301	49.975207
3503.587568	501915.883064	49.980212
3503.449691	501914.437065	49.985217
3503.567285	501902.827899	49.990221
3503.634332	501911.472294	49.995226
3503.194676	501906.176722	50.000231
3503.454580	501889.078747	50.005236
3503.030015	501888.133587	50.010241
3503.176663	501884.719280	50.015245
3503.202984	501889.877757	50.020250
3503.094076	501883.467006	50.025255
3503.155322	501885.076983	50.030260
3503.050570	501891.673369	50.035265
3502.995983	501893.149813	50.040269
3503.249791	501888.453220	50.045274
3503.296171	501879.993362	50.050279
3503.378150	501891.014265	50.055284
3503.388234	501888.178298	50.060289
3503.102682	501888.324673	50.065293
3503.550824	501880.965433	50.070298
3503.464663	501891.354930	50.075303
3503.157779	501861.794248	50.080308
3503.084324	501855.782795	50.085313
3503.157634	501849.242001	50.090317
3503.312496	501850.786570	50.095322
3502.777723	501854.161025	50.100327
3503.117442	501846.515224	50.105332
3503.317708	501845.724368	50.110337
3503.099251	501844.847855	50.115341
3503.183879	501855.969589	50.120346
3503.201018	501860.167858	50.125351
3503.632130	501847.598047	50.130356
3503.534237	501855.509329	50.135361
3503.369645	501841.059723	50.140365
3503.302192	501816.775602	50.145370
3502.788544	501828.649904	50.150375
3503.180682	501808.038573	50.155380
3503.053786	501810.842422	50.160385
3503.079699	501817.570025	50.165389
3503.388922	501817.521158	50.170394
3503.426792	501826.068979	50.175399
3503.427130	501810.783452	50.180404
3503.196784	501816.842962	50.185409
3503.308224	501821.836161	50.190413
3503.494041	501810.975364	50.195418
3503.160981	501820.442259	50.200423
3503.063975	501798.845336	50.205428
3503.106459	501814.326582	50.210433
3503.343843	501791.158368	50.215437
3503.337514	501777.746595	50.220442
3503.255018	501773.406815	50.225447
3503.274894	501767.127508	50.230452
3503.113183	501778.693142	50.235457
3503.263338	501764.902325	50.240461
3503.141022	501773.424876	50.245466
3502.658898	501773.298636	50.250471
3503.290595	501772.642040	50.255476
3503.302100	501770.818116	50.260481
3502.761863	501774.244064	50.265485
3503.180235	501775.595145	50.270490
3503.152272	501789.265433	50.275495
3503.050288	501772.680077	50.280500
3502.925634	501783.480636	50.285505
3503.054391	501775.210165	50.290509
3503.292001	501783.979505	50.295514
3503.040514	501784.727866	50.300519
3503.040485	501769.999120	50.305524
3503.084924	501784.417182	50.310529
3502.778092	501790.539404	50.315533
3503.377484	501778.702159	50.320538
3503.002528	501780.128023	50.325543
3503.410013	501781.835125	50.330548
3503.166969	501795.741861	50.335553
3503.030193	501782.502553	50.340557
3503.451948	501777.779385	50.345562
3503.148114	501779.042164	50.350567
3503.442356	501747.260473	50.355572
3503.714857	501747.470483	50.360577
3503.034186	501750.058188	50.365581
3503.376648	501749.649767	50.370586
3503.109987	501748.072267	50.375591
3503.302180	501738.627620	50.380596
3503.419478	501748.985042	50.385601
3503.299841	501743.638837	50.390605
3503.472716	501736.879806	50.395610
3502.922298	501725.983487	50.400615
3503.183005	501712.731913	50.405620
3503.200475	501710.097209	50.410625
3503.010918	501701.826403	50.415629
3503.477117	501699.070154	50.420634
3503.355553	501703.290385	50.425639
3503.463538	501695.478690	50.430644
3503.127915	501710.412418	50.435649
3503.372497	501700.706398	50.440653
3503.441003	501695.431669	50.445658
3502.867337	501707.416768	50.450663
3503.346342	501694.434362	50.455668
3503.157596	501689.048451	50.460673
3503.081503	501664.563028	50.465677
3503.330357	501661.992973	50.470682
3503.115007	501657.674164	50.475687
3503.555305	501658.718101	50.480692
3503.513645	501664.342920	50.485697
3503.241284	501658.109767	50.490701
3503.592661	501655.270432	50.495706
3503.418197	501657.676907	50.500711
3503.111132	501637.884503	50.505716
3503.041738	501632.682168	50.510721
3503.382541	501616.431594	50.515725
3503.466555	501614.241890	50.520730
3502.916416	501614.632547	50.525735
3503.224544	501581.431151	50.530740
3503.188541	501555.066492	50.535745
3503.098106	501514.335728	50.540749
3503.412755	501458.913052	50.545754
3502.671750	501393.736451	50.550759
3502.891732	501314.336576	50.555764
3502.911598	501231.171789	50.560769
3502.438074	501129.407253	50.565773
3502.301520	501026.272844	50.570778
3502.233441	500925.404767	50.575783
3502.232241	500789.346689	50.580788
3501.922050	500665.433992	50.585793
3501.704228	500534.166248	50.590797
3501.828317	500383.912275	50.595802
3501.332057	500235.273655	50.600807
3501.215332	500063.491479	50.605812
3501.192096	499883.290012	50.610817
3500.677188	499705.948557	50.615821
3500.474965	499515.293298	50.620826
3499.934118	499322.512823	50.625831
3499.896464	499124.284825	50.630836
3499.683325	498922.640056	50.635841
3499.510976	498700.332399	50.640845
3499.215824	498487.508026	50.645850
3498.819209	498258.801167	50.650855
3498.334398	498020.689114	50.655860
3498.032955	497783.861201	50.660865
3497.725707	497532.096351	50.665869
3497.704008	497281.852299	50.670874
3497.266269	497025.595230	50.675879
3496.747121	496744.590091	50.680884
3496.397879	496486.843198	50.685889
3495.900992	496212.306846	50.690893
3495.805232	495928.083104	50.695898
3495.151432	495640.044510	50.700903
3495.061455	495339.152887	50.705908
3494.878649	495052.650816	50.710913
3494.441517	494738.538288	50.715917
3494.250116	494421.394074	50.720922
3493.575461	494095.358228	50.725927
3492.996670	493763.630132	50.730932
3492.887136	493449.342503	50.735937
3492.271865	493112.139581	50.740941
3491.720683	492777.199147	50.745946
3491.155516	492429.594761	50.750951
3490.971067	492086.430753	50.755956
3490.461456	491738.196930	50.760961
3490.190878	491377.764417	50.765965
3489.702789	491019.081216	50.770970
3488.998793	490669.845254	50.775975
3488.735594	490280.522595	50.780980
3488.328877	489916.588804	50.785985
3487.564686	489544.347500	50.790989
3487.109120	489155.082531	50.795994
3486.665162	488775.127333	50.800999
3486.578516	488393.284549	50.806004
3486.039208	487995.803367	50.811009
3485.228421	487587.567561	50.816013
3484.672524	487194.985584	50.821018
3484.051224	486802.152553	50.826023
3483.676861	486392.403718	50.831028
3483.052680	485984.965168	50.836033
3482.400460	485571.291326	50.841037
3481.857226	485162.404012	50.846042
3481.192291	484742.381797	50.851047
3480.765477	484321.958128	50.856052
3480.364720	483913.629676	50.861057
3479.752082	483485.263016	50.866061
3479.206260	483058.497601	50.871066
3478.548832	482635.996424	50.876071
3477.940275	482201.470093	50.881076
3477.415207	481766.059494	50.886081
3476.404835	481335.428198	50.891085
3475.835291	480901.930820	50.896090
3475.229509	480473.040745	50.901095
3474.838924	480038.279856	50.906100
3474.149319	479600.364144	50.911105
3473.405279	479154.136521	50.916109
3473.087279	478709.706510	50.921114
3472.054949	478292.492071	50.926119
3472.188705	477836.517902	50.931124
3470.886302	477391.301770	50.936129
3470.275164	476943.381675	50.941133
3470.061727	476497.466647	50.946138
3468.902838	476048.396728	50.951143
3468.519797	475596.254406	50.956148
3467.747004	475148.117025	50.961153
3467.303882	474701.286114	50.966157
3466.650972	474238.562464	50.971162
3465.923062	473792.364761	50.976167
3465.199388	473340.073756	50.981172
3464.461028	472887.268107	50.986177
3463.584317	472432.142425	50.991181
3463.033491	471984.356363	50.996186
3462.714544	471538.602346	51.001191
3461.868068	471073.759030	51.006196
3461.112890	470623.390124	51.011201
3460.274295	470173.835747	51.016205
3459.912237	469709.594903	51.021210
3459.354766	469260.533958	51.026215
3458.638849	468797.849683	51.031220
3457.736100	468352.220721	51.036225
3457.141276	467893.350635	51.041229
3456.663214	467435.668950	51.046234
3455.516081	466969.057420	51.051239
3454.971057	466508.780138	51.056244
3454.329223	466068.030715	51.061249
3453.520975	465614.671849	51.066253
3453.291095	465153.301062	51.071258
3452.065955	464704.045465	51.076263
3451.590133	464237.014026	51.081268
3450.865043	463797.194195	51.086273
3450.048857	463341.049663	51.091277
3449.657267	462886.856930	51.096282
3449.000767	462431.073556	51.101287
3448.375878	461976.746365	51.106292
3447.481265	461528.132769	51.111297
3446.682008	461064.735337	51.116301
3446.112692	460610.370712	51.121306
3445.275687	460166.234043	51.126311
3444.377595	459703.330484	51.131316
3443.980810	459261.489817	51.136321
3442.927875	458805.490240	51.141325
3442.760293	458363.037291	51.146330
3441.510096	457924.449705	51.151335
3441.073841	457458.940264	51.156340
3440.396329	457013.598693	51.161345
3439.691212	456563.280996	51.166349
3439.059425	456103.709510	51.171354
3438.172442	455663.294989	51.176359
3437.602204	455214.856599	51.181364
3436.686977	454781.836280	51.186369
3436.082003	454336.074760	51.191373
3435.552023	453891.814661	51.196378
3434.554016	453440.668822	51.201383
3434.032541	452997.455312	51.206388
3433.292504	452552.694796	51.211393
3432.455420	452116.465303	51.216397
3431.836353	451670.602918	51.221402
3431.220467	451235.742407	51.226407
3430.461952	450794.350342	51.231412
3429.393106	450351.324319	51.236417
3429.038245	449911.881298	51.241421
3428.488960	449481.138245	51.246426
3427.379231	449043.168232	51.251431
3427.331264	448605.529579	51.256436
3426.078323	448163.201328	51.261441
3425.685993	447720.474887	51.266445
3424.887114	447287.193262	51.271450
3423.817200	446857.905132	51.276455
3423.467268	446421.795989	51.281460
3422.705042	445990.565572	51.286465
3421.894778	445554.970004	51.291469
3421.497754	445116.864842	51.296474
3420.239011	444697.363183	51.301479
3419.807719	444262.496137	51.306484
3419.212796	443826.378100	51.311489
3418.117180	443402.615003	51.316493
3417.486209	442968.009848	51.321498
3416.692236	442544.488511	51.326503
3416.362550	442123.932051	51.331508
3415.792672	441704.929149	51.336513
3415.044521	441279.043363	51.341517
3414.379739	440843.847050	51.346522
3413.348935	440435.809546	51.351527
3413.057407	440002.366791	51.356532
3412.039947	439581.722934	51.361537
3411.280604	439154.507391	51.366541
3410.596159	438726.384154	51.371546
3409.980771	438318.220464	51.376551
3409.316399	437898.279040	51.381556
3408.608998	437468.919232	51.386561
3407.507630	437056.597644	51.391565
3407.260814	436631.339316	51.396570
3406.419104	436217.058849	51.401575
3405.572744	435790.865596	51.406580
3405.108955	435392.099653	51.411585
3404.032151	434977.404377	51.416589
3403.675491	434548.497746	51.421594
3402.942584	434138.888277	51.426599
3402.483512	433716.559572	51.431604
3401.627594	433300.481765	51.436609
3400.864075	432890.171572	51.441613
3400.430839	432462.232221	51.446618
3399.376857	432062.999709	51.451623
3398.918910	431642.794946	51.456628
3398.085813	431230.133298	51.461633
3397.386331	430826.864512	51.466637
3396.659465	430403.127262	51.471642
3395.943833	429997.156552	51.476647
3395.101168	429583.860894	51.481652
3394.325929	429175.906178	51.486657
3393.857266	428772.620000	51.491661
3393.217358	428363.869472	51.496666
3392.260382	427962.578127	51.501671
3391.727973	427559.156538	51.506676
3390.965147	427148.882976	51.511681
3390.054523	426745.051720	51.516685
3389.407130	426344.525093	51.521690
3388.620974	425943.074729	51.526695
3388.420614	425533.550952	51.531700
3387.526904	425149.655354	51.536705
3386.691799	424748.423500	51.541709
3386.261272	424339.908546	51.546714
3384.931508	423959.824006	51.551719
3384.397532	423546.208306	51.556724
3384.014983	423151.637527	51.561729
3383.066537	422755.905944	51.566733
3382.471311	422358.614178	51.571738
3381.513858	421980.348296	51.576743
3381.003319	421587.527948	51.581748
3380.523078	421191.166431	51.586753
3379.466070	420801.291708	51.591757
3379.042896	420400.667788	51.596762
3378.206135	420021.035188	51.601767
3377.247134	419623.685568	51.606772
3376.859229	419242.980733	51.611777
3376.205559	418862.871647	51.616781
3375.686553	418465.232851	51.621786
3374.738389	418086.277650	51.626791
3374.109419	417699.747147	51.631796
3373.346665	417316.789236	51.636801
3372.606399	416924.422667	51.641805
3372.035528	416531.439595	51.646810
3371.108692	416165.742630	51.651815
3370.346703	415774.710271	51.656820
3370.171527	415394.784144	51.661825
3369.020007	415014.270611	51.666829
3368.383936	414620.865285	51.671834
3367.380952	414252.386745	51.676839
3366.810333	413878.042157	51.681844
3366.322699	413506.296705	51.686849
3365.300681	413128.761648	51.691853
3365.043839	412746.171403	51.696858
3364.093330	412377.889665	51.701863
3363.420863	411991.645606	51.706868
3363.156309	411615.064006	51.711873
3362.252745	411251.537903	51.716877
3361.779343	410860.800868	51.721882
3360.547315	410496.860117	51.726887
3359.714135	410122.179172	51.731892
3359.069735	409743.397857	51.736897
3358.413751	409382.808475	51.741901
3357.841794	409005.531146	51.746906
3357.138987	408652.691162	51.751911
3356.330832	408274.273116	51.756916
3355.963969	407908.004261	51.761921
3355.263564	407542.698640	51.766925
3354.483484	407166.015941	51.771930
3353.817663	406804.584349	51.776935
3353.168119	406433.666420	51.781940
3352.216856	406067.976322	51.786945
3351.619111	405698.235865	51.791949
3351.371622	405334.433598	51.796954
3350.313349	404968.467908	51.801959
3349.721571	404602.347909	51.806964
3349.264256	404241.082251	51.811969
3348.368651	403871.392689	51.816973
3347.616613	403509.199411	51.821978
3346.788659	403136.262620	51.826983
3346.304191	402769.392674	51.831988
3345.556674	402414.913011	51.836993
3344.618664	402050.749927	51.841997
3344.631208	401685.491897	51.847002
3343.575839	401325.355177	51.852007
3342.761616	400954.424184	51.857012
3341.986503	400601.352271	51.862017
3341.324648	400240.378626	51.867021
3340.859034	399884.809705	51.872026
3340.181216	399525.915041	51.877031
3339.606920	399156.171100	51.882036
3338.774655	398796.199778	51.887041
3337.922798	398434.956572	51.892045
3337.375644	398082.253482	51.897050
3336.738079	397714.867469	51.902055
3335.813687	397365.597408	51.907060
3335.303773	397015.266674	51.912065
3334.663332	396655.419642	51.917069
3334.017541	396291.679968	51.922074
3333.254879	395940.081386	51.927079
3332.772057	395580.324986	51.932084
3332.226488	395220.218743	51.937089
3331.267870	394862.207855	51.942093
3330.885650	394492.864777	51.947098
3329.889155	394131.597945	51.952103
3329.003011	393778.826931	51.957108
3328.389739	393427.178647	51.962113
3327.992971	393072.950047	51.967117
3327.190098	392710.315514	51.972122
3326.588310	392367.197366	51.977127
3325.924926	392007.457296	51.982132
3325.172137	391652.380550	51.987137
3324.299328	391301.590732	51.992141
3323.665390	390935.808972	51.997146
3322.958527	390601.538382	52.002151
3322.313221	390245.413293	52.007156
3321.405990	389896.267607	52.012161
3320.882403	389545.938998	52.017165
3320.351564	389191.437962	52.022170
3319.730364	388847.474782	52.027175
3318.928586	388495.298170	52.032180
3318.326749	388144.129029	52.037185
3317.286234	387799.840674	52.042189
3316.643725	387447.755739	52.047194
3315.876264	387108.706783	52.052199
3315.210910	386757.763051	52.057204
3314.938815	386419.468476	52.062209
3314.209589	386078.115208	52.067213
3313.325246	385722.211921	52.072218
3312.687530	385383.762155	52.077223
3312.233682	385036.532127	52.082228
3311.610399	384688.232114	52.087233
3310.684673	384343.257247	52.092237
3309.866042	384002.204067	52.097242
3309.363791	383655.045059	52.102247
3308.845219	383310.504867	52.107252
3307.960860	382971.131165	52.112257
3307.268052	382623.967322	52.117261
3306.989504	382270.859904	52.122266
3305.668878	381938.590670	52.127271
3305.473640	381595.738536	52.132276
3304.763915	381243.910545	52.137281
3304.108548	380911.450839	52.142285
3303.374273	380565.877075	52.147290
3302.616373	380223.254251	52.152295
3301.952865	379872.194836	52.157300
3301.296358	379532.016942	52.162305
3300.069240	379190.858079	52.167309
3299.894019	378852.454835	52.172314
3299.161827	378514.518280	52.177319
3298.359147	378177.251274	52.182324
3298.161303	377830.805339	52.187329
3297.062797	377491.951410	52.192333
3296.581452	377151.776059	52.197338
3295.852096	376822.218353	52.202343
3295.369400	376472.727886	52.207348
3294.725518	376133.714191	52.212353
3294.090388	375801.029949	52.217357
3293.532210	375449.049739	52.222362
3292.662702	375113.929543	52.227367
3291.786012	374763.799783	52.232372
3291.102811	374430.068965	52.237377
3290.600392	374088.395736	52.242381
3290.033986	373745.127201	52.247386
3289.029136	373409.174986	52.252391
3288.387287	373062.096994	52.257396
3287.928494	372727.630045	52.262401
3286.982199	372391.431373	52.267405
3286.279327	372055.344122	52.272410
3285.625043	371723.978151	52.277415
3285.086290	371387.503445	52.282420
3284.756102	371041.402390	52.287425
3284.044603	370704.517097	52.292429
3283.392117	370360.979993	52.297434
3282.670144	370023.556727	52.302439
3281.902247	369674.868024	52.307444
3281.402865	369340.049957	52.312449
3280.225406	369008.669270	52.317453
3279.965246	368663.886259	52.322458
3279.001779	368326.665988	52.327463
3278.022173	367986.748884	52.332468
3277.510574	367664.793102	52.337473
3276.724678	367332.701688	52.342477
3276.510489	366998.507434	52.347482
3275.696768	366656.162267	52.352487
3275.046261	366317.299667	52.357492
3274.649902	365983.101136	52.362497
3273.476012	365654.645908	52.367501
3272.834287	365318.293160	52.372506
3272.177236	364983.059813	52.377511
3271.525686	364646.449178	52.382516
3270.794418	364308.093062	52.387521
3270.147989	363977.633954	52.392525
3269.851116	363634.853285	52.397530
3268.732052	363318.789003	52.402535
3267.749868	362987.358112	52.407540
3267.371283	362650.918620	52.412545
3266.516155	362337.324857	52.417549
3266.009775	362000.620982	52.422554
3265.340383	361672.795263	52.427559
3264.516285	361350.742291	52.432564
3264.034501	361024.790749	52.437569
3263.208203	360698.509774	52.442573
3262.869161	360382.404021	52.447578
3261.774917	360049.061674	52.452583
3261.439271	359718.345158	52.457588
3260.863951	359388.249535	52.462593
3260.143575	359065.732119	52.467597
3259.500295	358736.304388	52.472602
3258.810402	358413.090753	52.477607
3258.251444	358083.492584	52.482612
3257.712856	357749.563000	52.487617
3256.752171	357421.728871	52.492621
3255.983605	357080.069770	52.497626
3255.537790	356757.799078	52.502631
3254.917815	356435.426610	52.507636
3254.337876	356096.606488	52.512641
3253.209321	355772.452512	52.517645
3253.089969	355427.320281	52.522650
3252.160766	355107.431220	52.527655
3251.160027	354780.375010	52.532660
3250.416812	354452.792440	52.537665
3249.907036	354128.962706	52.542669
3249.549707	353809.713065	52.547674
3248.762755	353482.742001	52.552679
3248.246314	353157.660222	52.557684
3247.198780	352815.049460	52.562689
3246.383212	352500.521490	52.567693
3245.635702	352171.296402	52.572698
3245.064871	351854.766228	52.577703
3244.179833	351529.961716	52.582708
3243.965565	351206.805169	52.587713
3243.264410	350881.891265	52.592717
3242.857646	350554.867332	52.597722
3242.042044	350236.661097	52.602727
3241.394795	349914.710544	52.607732
3240.716525	349575.990837	52.612737
3239.760791	349262.382221	52.617741
3239.143486	348934.236531	52.622746
3238.820182	348613.397818	52.627751
3238.074923	348289.697068	52.632756
3237.133163	347965.058351	52.637761
3236.324103	347643.960003	52.642765
3235.600677	347316.254209	52.647770
3234.739783	347014.987529	52.652775
3234.245199	346682.176878	52.657780
3233.665230	346361.925808	52.662785
3232.643864	346056.937923	52.667789
3232.338193	345738.472545	52.672794
3231.414906	345432.651337	52.677799
3230.952297	345108.251346	52.682804
3230.636368	344786.397097	52.687809
3229.774830	344471.652473	52.692813
3229.505809	344148.820066	52.697818
3228.445728	343822.369366	52.702823
3227.576292	343511.413420	52.707828
3227.189772	343188.568899	52.712833
3226.251337	342870.417098	52.717837
3225.700489	342554.111345	52.722842
3224.979772	342235.056297	52.727847
3224.340425	341923.419350	52.732852
3223.767793	341606.043001	52.737857
3222.792095	341293.259680	52.742861
3222.512808	340961.400837	52.747866
3221.624767	340656.618641	52.752871
3220.827052	340338.736804	52.757876
3220.395357	340018.097198	52.762881
3219.654440	339708.246970	52.767885
3218.996402	339383.948920	52.772890
3218.495267	339064.995487	52.777895
3217.718566	338754.458941	52.782900
3216.849546	338436.706059	52.787905
3215.750486	338131.639554	52.792909
3215.392055	337807.362450	52.797914
3214.671432	337501.545785	52.802919
3213.960971	337182.234276	52.807924
3213.440160	336871.673642	52.812929
3212.760007	336563.275092	52.817933
3212.241205	336249.681888	52.822938
3211.514852	335945.640844	52.827943
3210.632858	335625.534326	52.832948
3210.168321	335313.073690	52.837953
3209.326129	335014.749103	52.842957
3208.565266	334694.848112	52.847962
3207.799504	334385.536626	52.852967
3207.083325	334081.281920	52.857972
3206.987321	333768.526772	52.862977
3205.926144	333471.248400	52.867981
3205.673721	333161.290139	52.872986
3204.968176	332842.211906	52.877991
3203.937936	332527.129579	52.882996
3203.635586	332217.709671	52.888001
3202.790269	331905.268417	52.893005
3202.167755	331601.191787	52.898010
3201.511795	331290.983683	52.903015
3200.526090	330986.121786	52.908020
3199.785069	330674.142399	52.913025
3199.177568	330368.810742	52.918029
3198.375434	330058.544133	52.923034
3197.914156	329750.717269	52.928039
3197.137869	329449.278269	52.933044
3196.488952	329144.864638	52.938049
3195.828914	328848.471197	52.943053
3195.521768	328528.063504	52.948058
3194.694007	328229.530127	52.953063
3193.833128	327923.744847	52.958068
3193.375414	327613.082686	52.963073
3192.283854	327314.714786	52.968077
3191.808718	327000.794074	52.973082
3191.155192	326697.109771	52.978087
3190.458828	326399.006825	52.983092
3190.227097	326089.346710	52.988097
3189.234220	325802.465442	52.993101
3188.642194	325489.575629	52.998106
3187.877435	325174.573250	53.003111
3187.101556	324876.426286	53.008116
3186.845348	324569.157483	53.013121
3185.873275	324257.748847	53.018125
3185.401114	323959.575953	53.023130
3184.600967	323663.516215	53.028135
3184.292911	323350.242308	53.033140
3183.226495	323044.852856	53.038145
3182.396136	322743.473282	53.043149
3182.003280	322434.359571	53.048154
3181.371828	322131.418686	53.053159
3180.520829	321829.148009	53.058164
3179.870557	321526.335287	53.063169
3178.977832	321223.559876	53.068173
3178.402764	320922.948331	53.073178
3177.702761	320627.346047	53.078183
3177.067152	320320.020117	53.083188
3176.659493	320020.753978	53.088193
3175.600562	319727.497092	53.093197
3175.080089	319415.515763	53.098202
3174.753642	319116.284717	53.103207
3173.786341	318821.177142	53.108212
3173.115550	318511.660914	53.113217
3172.277022	318213.322769	53.118221
3172.051787	317913.486198	53.123226
3171.166812	317615.484523	53.128231
3170.296937	317306.606939	53.133236
3169.890362	317011.430437	53.138241
3168.934186	316720.363129	53.143245
3168.618084	316424.432099	53.148250
3167.757850	316126.854784	53.153255
3167.066655	315830.650295	53.158260
3166.548073	315513.359549	53.163265
3165.759769	315222.312184	53.168269
3165.214732	314917.347964	53.173274
3164.455331	314623.544263	53.178279
3163.785499	314325.931484	53.183284
3163.410314	314023.000267	53.188289
3162.337312	313728.556119	53.193293
3161.818418	313407.362955	53.198298
3160.833084	313113.896298	53.203303
3160.268262	312825.073109	53.208308
3159.566970	312516.485261	53.213313
3158.945863	312232.813103	53.218317
3158.528907	311931.996048	53.223322
3157.777741	311644.727044	53.228327
3156.858033	311347.170960	53.233332
3156.450232	311041.333587	53.238337
3155.747711	310754.843985	53.243341
3155.137103	310452.780365	53.248346
3154.506720	310154.182243	53.253351
3153.793329	309860.205564	53.258356
3153.476943	309560.384857	53.263361
3152.279384	309263.631250	53.268365
3151.930006	308960.172788	53.273370
3151.056287	308663.060861	53.278375
3150.218575	308366.299010	53.283380
3149.690594	308066.558959	53.288385
3148.853186	307771.247112	53.293389
3147.865772	307483.648738	53.298394
3147.634572	307184.776327	53.303399
3146.816493	306894.908877	53.308404
3146.463547	306602.573434	53.313409
3145.685454	306313.971597	53.318413
3144.863706	306010.758922	53.323418
3144.098967	305728.443608	53.328423
3143.503946	305442.000896	53.333428
3143.019896	305138.223467	53.338433
3142.213279	304846.821722	53.343437
3141.560418	304551.498782	53.348442
3140.761414	304256.784041	53.353447
3140.160907	303966.697489	53.358452
3139.507833	303673.613691	53.363457
3138.484990	303390.621331	53.368461
3138.107674	303096.779661	53.373466
3136.996814	302812.781451	53.378471
3136.564038	302524.116976	53.383476
3136.076556	302238.847572	53.388481
3135.120436	301957.649951	53.393485
3134.592943	301679.388978	53.398490
3134.095432	301393.559298	53.403495
3133.291783	301100.927115	53.408500
3132.836720	300815.777233	53.413505
3131.949238	300532.834427	53.418509
3131.531651	300238.229566	53.423514
3131.010138	299952.833980	53.428519
3129.854020	299671.281879	53.433524
3129.877692	299370.544598	53.438529
3128.939131	299085.544558	53.443533
3128.203510	298800.308187	53.448538
3127.412214	298503.543767	53.453543
3126.497985	298220.193753	53.458548
3126.422936	297934.036477	53.463553
3125.308525	297650.564418	53.468557
3124.792349	297356.504921	53.473562
3124.309417	297080.215533	53.478567
3123.531558	296795.313662	53.483572
3122.766475	296494.849049	53.488577
3122.163810	296216.412630	53.493581
3121.352115	295924.766048	53.498586
3120.876323	295647.149134	53.503591
3120.006393	295352.913271	53.508596
3119.298059	295056.715898	53.513601
3118.655372	294782.180232	53.518605
3118.148882	294485.491673	53.523610
3117.659406	294209.708570	53.528615
3116.674926	293930.743632	53.533620
3116.495355	293631.404470	53.538625
3115.481647	293348.801579	53.543629
3114.571875	293063.278598	53.548634
3113.872436	292782.051420	53.553639
3113.546496	292504.533960	53.558644
3113.016407	292210.214498	53.563649
3111.920972	291939.210459	53.568653
3111.756877	291644.832370	53.573658
3110.925873	291344.727398	53.578663
3109.858865	291064.116619	53.583668
3109.690176	290781.122217	53.588673
3108.703573	290494.767874	53.593677
3108.201362	290205.560585	53.598682
3107.539799	289928.831885	53.603687
3106.601196	289637.273610	53.608692
3106.008784	289353.555231	53.613697
3105.030066	289079.906522	53.618701
3104.699849	288789.371660	53.623706
3103.972651	288509.315661	53.628711
3102.986043	288235.667403	53.633716
3102.586411	287950.032524	53.638721
3101.970062	287671.715485	53.643725
3101.283397	287387.042357	53.648730
3100.642076	287116.929446	53.653735
3099.995497	286830.823284	53.658740
3099.742487	286548.856807	53.663745
3098.628086	286263.282627	53.668749
3098.045201	285977.191145	53.673754
3097.501765	285702.604736	53.678759
3096.832443	285419.455319	53.683764
3096.276589	285137.204584	53.688769
3095.828355	284848.314916	53.693773
3095.048583	284558.458786	53.698778
3094.256850	284278.536907	53.703783
3093.169263	283999.094624	53.708788
3092.915358	283704.646832	53.713793
3091.945865	283430.457408	53.718797
3090.969101	283143.331144	53.723802
3090.883402	282870.274936	53.728807
3089.636062	282596.434629	53.733812
3089.583719	282299.330857	53.738817
3088.674968	282035.955044	53.743821
3088.026024	281742.205321	53.748826
3087.251958	281463.348708	53.753831
3086.531083	281192.200431	53.758836
3086.042058	280908.434018	53.763841
3085.398619	280637.273251	53.768845
3084.689659	280356.291987	53.773850
3084.233704	280079.192690	53.778855
3083.491505	279794.981998	53.783860
3082.977973	279502.967179	53.788865
3082.113308	279236.578031	53.793869
3081.518270	278951.401439	53.798874
3080.911065	278666.379497	53.803879
3080.178816	278384.790024	53.808884
3079.775232	278092.069730	53.813889
3078.750368	277813.047796	53.818893
3078.109158	277526.604725	53.823898
3077.611040	277256.056683	53.828903
3076.975242	276962.685252	53.833908
3076.080035	276671.392300	53.838913
3075.250412	276394.249348	53.843917
3074.749410	276100.347092	53.848922
3074.023777	275825.199624	53.853927
3073.151454	275544.676052	53.858932
3072.538439	275262.863473	53.863937
3071.705917	274995.831822	53.868941
3070.950898	274721.733156	53.873946
3070.675192	274439.001248	53.878951
3069.851201	274160.329191	53.883956
3069.166554	273888.715303	53.888961
3067.983947	273615.550265	53.893965
3067.529237	273339.850545	53.898970
3067.034930	273081.271870	53.903975
3066.529751	272805.121760	53.908980
3066.167754	272533.355053	53.913985
3065.139514	272264.699100	53.918989
3064.813150	271977.416598	53.923994
3063.749230	271701.049473	53.928999
3063.580479	271431.595457	53.934004
3062.800752	271152.152732	53.939009
3061.676748	270876.686691	53.944013
3061.184908	270596.765579	53.949018
3060.415808	270332.143960	53.954023
3059.587165	270060.018684	53.959028
3059.351339	269782.502254	53.964033
3058.643915	269510.205157	53.969037
3057.879933	269239.750822	53.974042
3057.226179	268963.701584	53.979047
3056.234150	268695.168199	53.984052
3055.701568	268420.908244	53.989057
3055.113864	268163.338840	53.994061
3054.430127	267882.939722	53.999066
3053.987442	267604.259890	54.004071
3052.943916	267334.359956	54.009076
3052.402403	267056.638360	54.014081
3051.713037	266794.883402	54.019085
3051.211101	266524.668941	54.024090
3050.552699	266258.885384	54.029095
3049.578059	265985.537048	54.034100
3049.169604	265714.926220	54.039105
3048.295942	265453.150220	54.044109
3047.880499	265188.092867	54.049114
3046.961711	264915.271173	54.054119
3046.246927	264649.217344	54.059124
3045.706180	264372.286749	54.064129
3044.938797	264122.897706	54.069133
3044.315715	263853.468115	54.074138
3043.873321	263578.840110	54.079143
3043.040000	263309.596997	54.084148
3042.138425	263042.911686	54.089153
3041.772332	262782.559744	54.094157
3040.808719	262512.803038	54.099162
3040.441821	262254.310788	54.104167
3039.335859	261989.696089	54.109172
3039.220189	261712.420137	54.114177
3038.503153	261453.016172	54.119181
3037.742897	261188.500233	54.124186
3037.465924	260914.816024	54.129191
3036.438158	260652.176583	54.134196
3035.719691	260377.951528	54.139201
3034.714314	260114.825146	54.144205
3034.390513	259846.548521	54.149210
3033.629792	259579.003475	54.154215
3032.482350	259323.133159	54.159220
3031.789435	259060.034738	54.164225
3031.362960	258803.617857	54.169229
3031.006747	258540.976019	54.174234
3030.507095	258281.973551	54.179239
3029.840433	258022.615775	54.184244
3029.526767	257747.208808	54.189249
3028.442479	257481.448969	54.194253
3027.875298	257230.862575	54.199258
3027.256400	256951.480988	54.204263
3026.331186	256686.155288	54.209268
3025.878322	256414.923106	54.214273
3025.103829	256155.737272	54.219277
3024.370199	255888.854152	54.224282
3023.826055	255626.092530	54.229287
3023.202170	255359.982177	54.234292
3022.794050	255092.208105	54.239297
3021.731152	254828.179827	54.244301
3020.834648	254557.249424	54.249306
3020.640136	254289.824590	54.254311
3019.778887	254034.195034	54.259316
3019.190853	253761.077646	54.264321
3018.375057	253504.040899	54.269325
3017.918676	253241.981543	54.274330
3017.070078	252969.110257	54.279335
3016.582186	252704.382607	54.284340
3015.820667	252436.362490	54.289345
3014.879794	252188.617272	54.294349
3014.227560	251911.972842	54.299354
3013.964925	251651.362145	54.304359
3012.637842	251396.981404	54.309364
3012.252767	251131.552183	54.314369
3011.619040	250874.795915	54.319373
3010.888472	250609.727787	54.324378
3010.239991	250348.237861	54.329383
3009.405375	250093.984830	54.334388
3009.050531	249833.824419	54.339393
3008.442616	249584.629579	54.344397
3007.574420	249310.060865	54.349402
3007.138609	249052.843154	54.354407
3006.049008	248798.632511	54.359412
3005.672705	248536.975079	54.364417
3005.023719	248278.824657	54.369421
3004.312775	248009.937746	54.374426
3003.643565	247759.125656	54.379431
3002.605855	247498.822529	54.384436
3002.156116	247242.577743	54.389441
3001.187115	246990.999478	54.394445
3000.836824	246734.077712	54.399450
3000.244219	246474.368039	54.404455
2999.583488	246228.395720	54.409460
2999.096910	245964.340984	54.414465
2998.294126	245710.523104	54.419469
2997.657173	245446.187549	54.424474
2997.178314	245196.291975	54.429479
2996.481473	244943.935726	54.434484
2995.742979	244663.319731	54.439489
2994.679565	244418.764020	54.444493
2994.267606	244161.423809	54.449498
2993.940647	243907.635799	54.454503
2992.866695	243634.332708	54.459508
2991.965980	243382.138993	54.464513
2991.391768	243138.756000	54.469517
2991.057368	242872.314921	54.474522
2990.374032	242619.095136	54.479527
2989.318922	242367.080639	54.484532
2989.069234	242102.741365	54.489537
2988.282165	241853.588483	54.494541
2987.523904	241594.194617	54.499546
2986.903120	241340.127167	54.504551
2986.174180	241088.623854	54.509556
2985.778518	240825.558200	54.514561
2984.885356	240574.616713	54.519565
2984.229016	240320.888072	54.524570
2983.481512	240069.186112	54.529575
2982.891838	239814.021982	54.534580
2982.509711	239558.825550	54.539585
2981.732673	239304.634383	54.544589
2980.934663	239052.611573	54.549594
2980.380230	238793.853623	54.554599
2979.862412	238540.743545	54.559604
2978.964007	238282.703288	54.564609
2978.220065	238026.294346	54.569613
2977.552327	237764.068103	54.574618
2977.102487	237515.100240	54.579623
2976.160185	237266.898433	54.584628
2975.574825	237007.156430	54.589633
2974.786000	236761.452412	54.594637
2974.024308	236509.302303	54.599642
2973.527938	236255.251928	54.604647
2973.032175	236007.848099	54.609652
2972.425524	235752.670519	54.614657
2971.652486	235495.686521	54.619661
2970.998886	235242.350999	54.624666
2970.264484	234987.959423	54.629671
2969.195599	234739.478016	54.634676
2968.855361	234484.541481	54.639681
2968.216106	234235.331239	54.644685
2967.273837	233983.419555	54.649690
2967.095503	233737.091310	54.654695
2966.111812	233489.363388	54.659700
2965.356184	233230.014295	54.664705
2964.535696	232991.453941	54.669709
2964.293679	232742.082699	54.674714
2963.556595	232489.938634	54.679719
2962.770708	232248.115379	54.684724
2961.931730	231994.129958	54.689729
2961.781643	231749.126313	54.694733
2961.029562	231503.352877	54.699738
2960.267588	231248.007739	54.704743
2959.414703	231001.895095	54.709748
2958.927977	230741.542581	54.714753
2958.286731	230490.407154	54.719757
2957.405534	230244.377385	54.724762
2956.988838	229999.522380	54.729767
2955.711957	229746.987351	54.734772
2955.651575	229503.426758	54.739777
2955.138432	229253.522088	54.744781
2954.344260	229006.081484	54.749786
2953.866524	228752.938942	54.754791
2952.720064	228505.071730	54.759796
2952.348475	228248.603794	54.764801
2951.778773	228009.456402	54.769805
2950.906953	227754.342189	54.774810
2950.646955	227498.266168	54.779815
2949.323260	227260.080439	54.784820
2948.946948	227012.681146	54.789825
2948.451989	226764.257441	54.794829
2947.524919	226507.857145	54.799834
2947.164758	226258.675202	54.804839
2946.091470	226012.178463	54.809844
2945.671739	225755.623747	54.814849
2944.763987	225512.195777	54.819853
2944.322584	225263.920787	54.824858
2943.694944	225014.364803	54.829863
2943.247488	224772.750226	54.834868
2942.245955	224513.338047	54.839873
2941.712650	224266.379115	54.844877
2940.718331	224015.585756	54.849882
2940.227202	223773.395478	54.854887
2939.287425	223523.129686	54.859892
2938.881799	223286.197615	54.864897
2937.981132	223039.682526	54.869901
2937.569272	222795.827763	54.874906
2936.773906	222542.843443	54.879911
2935.980162	222308.827268	54.884916
2935.460541	222056.933826	54.889921
2934.675942	221818.525869	54.894925
2934.056790	221580.767133	54.899930
2933.391187	221337.810012	54.904935
2932.495840	221095.271930	54.909940
2932.229850	220852.151245	54.914945
2931.112473	220611.584773	54.919949
2930.630275	220364.757371	54.924954
2930.381585	220127.555543	54.929959
2929.627611	219885.635441	54.934964
2928.789191	219641.921908	54.939969
2928.186843	219391.985293	54.944973
2927.540779	219157.904540	54.949978
2926.651701	218917.281934	54.954983
2925.888786	218671.943027	54.959988
2925.324421	218428.724754	54.964993
2924.611897	218186.409072	54.969997
2923.858696	217954.716783	54.975002
2923.271099	217712.077414	54.980007
2922.526892	217484.407626	54.985012
2922.017523	217230.950496	54.990017
2921.643513	217000.397790	54.995021
2920.641531	216764.650013	55.000026
2920.129548	216517.687626	55.005031
2919.466942	216288.595854	55.010036
2918.884862	216038.896815	55.015041
2918.246280	215801.758211	55.020045
2917.618328	215566.782622	55.025050
2917.148163	215308.756616	55.030055
2916.191283	215076.533267	55.035060
2915.401029	214839.358347	55.040065
2914.919957	214594.727265	55.045069
2914.106728	214353.331790	55.050074
2913.568007	214108.520662	55.055079
2912.500283	213883.701463	55.060084
2912.404127	213634.634327	55.065089
2911.945880	213390.080372	55.070093
2910.913945	213150.734930	55.075098
2910.858476	212904.260654	55.080103
2909.755164	212662.242619	55.085108
2909.224379	212416.150906	55.090113
2908.481773	212168.579011	55.095117
2907.813146	211925.425707	55.100122
2907.127140	211672.717325	55.105127
2906.054063	211430.915444	55.110132
2905.778596	211183.400618	55.115137
2904.973845	210945.643733	55.120141
2904.331076	210704.909227	55.125146
2903.905278	210463.517613	55.130151
2902.889125	210221.787651	55.135156
2902.454445	209978.121027	55.140161
2901.600016	209726.885233	55.145165
2900.598346	209485.283079	55.150170
2899.982732	209242.487976	55.155175
2899.071913	209009.973456	55.160180
2898.894974	208777.559965	55.165185
2897.968361	208543.802405	55.170189
2897.351122	208306.013086	55.175194
2897.025863	208062.832993	55.180199
2895.969782	207828.805925	55.185204
2895.339061	207592.574232	55.190209
2894.988438	207362.649945	55.195213
2894.161394	207119.756705	55.200218
2893.298319	206877.315594	55.205223
2892.653299	206657.736779	55.210228
2892.213731	206411.476023	55.215233
2891.435235	206174.395127	55.220237
2890.426547	205949.238492	55.225242
2890.426970	205706.283589	55.230247
2889.413162	205476.306110	55.235252
2889.050642	205229.185364	55.240257
2888.407513	204996.707538	55.245261
2887.500311	204761.383517	55.250266
2887.202261	204513.555619	55.255271
2886.353587	204289.678111	55.260276
2885.876938	204046.131133	55.265281
2885.142029	203807.932974	55.270285
2884.395067	203563.450908	55.275290
2883.800810	203320.561938	55.280295
2882.802914	203089.865997	55.285300
2882.512660	202840.326025	55.290305
2881.598811	202605.075503	55.295309
2880.730838	202370.213201	55.300314
2880.372773	202128.360914	55.305319
2879.461422	201904.464508	55.310324
2878.967319	201656.565519	55.315329
2878.163070	201420.882641	55.320333
2877.325817	201190.512638	55.325338
2876.870137	200952.409552	55.330343
2876.282937	200720.932942	55.335348
2875.631789	200490.027357	55.340353
2875.039994	200249.785501	55.345357
2874.344417	200011.291802	55.350362
2873.714971	199773.335867	55.355367
2872.593175	199548.566102	55.360372
2872.040578	199308.767572	55.365377
2871.623826	199079.714188	55.370381
2870.868793	198847.610387	55.375386
2870.448451	198597.562982	55.380391
2869.639457	198373.575715	55.385396
2868.845707	198144.127916	55.390401
2868.389618	197911.115529	55.395405
2867.426197	197666.172144	55.400410
2867.080776	197431.057446	55.405415
2866.251699	197207.320049	55.410420
2865.612081	196957.785902	55.415425
2864.917091	196721.648123	55.420429
2864.056045	196491.607375	55.425434
2863.911315	196264.673532	55.430439
2863.080344	196024.959374	55.435444
2862.400447	195795.567419	55.440449
2861.763462	195562.225107	55.445453
2860.989895	195328.727340	55.450458
2860.514245	195092.676761	55.455463
2859.551695	194854.706666	55.460468
2858.865155	194609.606584	55.465473
2858.429721	194383.770451	55.470477
2857.307455	194159.952707	55.475482
2856.812810	193918.719143	55.480487
2856.027946	193687.915456	55.485492
2855.705682	193456.810536	55.490497
2855.261538	193222.163300	55.495501
2854.456968	192989.762736	55.500506
2853.650991	192752.579351	55.505511
2852.763859	192522.547932	55.510516
2852.374950	192281.025590	55.515521
2851.735985	192053.298194	55.520525
2850.997584	191830.206227	55.525530
2850.402821	191585.246372	55.530535
2849.733311	191356.610949	55.535540
2849.293594	191125.370090	55.540545
2848.430107	190879.082209	55.545549
2847.572948	190657.833818	55.550554
2847.405074	190418.817560	55.555559
2846.303100	190194.009412	55.560564
2845.493345	189959.499264	55.565569
2845.189698	189722.276455	55.570573
2844.106041	189484.224132	55.575578
2843.907596	189248.742763	55.580583
2842.961918	189020.683761	55.585588
2842.650411	188791.609384	55.590593
2841.647267	188555.597303	55.595597
2840.976985	188321.925528	55.600602
2840.592474	188082.001064	55.605607
2840.225270	187854.250465	55.610612
2839.179642	187617.817244	55.615617
2838.938222	187380.125565	55.620621
2837.753039	187149.352804	55.625626
2837.225540	186913.998813	55.630631
2836.282980	186677.528592	55.635636
2835.623453	186443.978994	55.640641
2835.276226	186214.312214	55.645645
2834.476161	185984.133088	55.650650
2834.139331	185753.194767	55.655655
2833.100925	185520.384120	55.660660
2832.358745	185282.451767	55.665665
2831.729617	185053.229822	55.670669
2831.042520	184822.478898	55.675674
2830.539322	184583.087532	55.680679
2829.656428	184354.481778	55.685684
2829.279571	184120.657584	55.690689
2828.528632	183893.521675	55.695693
2827.463399	183669.973212	55.700698
2827.238704	183428.393977	55.705703
2826.234753	183200.118583	55.710708
2825.394251	182959.568062	55.715713
2824.951813	182727.593371	55.720717
2824.120294	182511.837132	55.725722
2823.468386	182285.113528	55.730727
2822.771818	182058.728905	55.735732
2822.200839	181837.146724	55.740737
2821.556026	181615.424708	55.745741
2820.544524	181392.375341	55.750746
2820.273145	181160.521741	55.755751
2819.710377	180936.589516	55.760756
2818.849779	180722.792924	55.765761
2818.475058	180487.690124	55.770765
2817.795917	180260.752370	55.775770
2817.431974	180025.688537	55.780775
2816.315098	179809.443887	55.785780
2815.845963	179574.564541	55.790785
2815.077643	179340.560670	55.795789
2814.194026	179119.537986	55.800794
2813.544281	178892.780891	55.805799
2812.820417	178669.471098	55.810804
2812.235992	178448.213717	55.815809
2811.396268	178212.319395	55.820813
2810.804075	177990.887561	55.825818
2810.425015	177768.074858	55.830823
2809.663158	177557.687315	55.835828
2809.142152	177325.944914	55.840833
2808.718308	177091.084883	55.845837
2807.652404	176863.183561	55.850842
2807.092695	176634.096740	55.855847
2806.456577	176414.448172	55.860852
2805.526568	176182.026483	55.865857
2805.025557	175957.144119	55.870861
2804.294804	175735.555417	55.875866
2803.969399	175510.138919	55.880871
2803.105662	175289.336816	55.885876
2802.419602	175055.420184	55.890881
2801.986596	174826.310618	55.895885
2801.052605	174605.014591	55.900890
2800.687146	174378.644057	55.905895
2799.885760	174149.609364	55.910900
2799.098188	173912.866443	55.915905
2798.575662	173689.805974	55.920909
2798.237182	173457.178913	55.925914
2797.463071	173227.114954	55.930919
2796.387276	173006.816715	55.935924
2795.930377	172774.314110	55.940929
2795.169579	172549.898729	55.945933
2794.182554	172329.145037	55.950938
2793.951788	172095.033555	55.955943
2793.324845	171872.304978	55.960948
2792.678240	171640.996352	55.965953
2792.203393	171416.211425	55.970957
2791.241255	171191.136156	55.975962
2790.773964	170955.542781	55.980967
2790.008324	170730.973153	55.985972
2788.859836	170502.650269	55.990977
2788.581440	170272.156147	55.995981
2787.867738	170059.510892	56.000986
2787.089811	169817.729459	56.005991
2786.309279	169598.776931	56.010996
2785.428078	169382.003461	56.016001
2785.028286	169146.728248	56.021005
2784.383332	168939.419321	56.026010
2784.040876	168707.240598	56.031015
2783.040768	168486.332640	56.036020
2782.388552	168266.769669	56.041025
2781.799085	168043.357643	56.046029
2781.085408	167820.678717	56.051034
2780.496446	167598.400976	56.056039
2779.831390	167371.266262	56.061044
2779.120083	167146.276551	56.066049
2778.536204	166926.379864	56.071053
2777.378302	166701.806872	56.076058
2777.300771	166485.342171	56.081063
2776.661274	166262.291893	56.086068
2776.014268	166038.671917	56.091073
2775.471060	165811.908765	56.096077
2774.476022	165584.697217	56.101082
2773.936441	165344.902789	56.106087
2773.323663	165135.498801	56.111092
2772.319236	164924.428733	56.116097
2771.936842	164703.139918	56.121101
2770.910749	164479.627494	56.126106
2770.718334	164251.050872	56.131111
2770.040222	164028.070960	56.136116
2769.044115	163788.714947	56.141121
2768.688766	163521.438702	56.146125
2767.796936	163291.427613	56.151130
2767.356068	163077.621456	56.156135
2766.841206	162860.191866	56.161140
2766.229617	162624.520689	56.166145
2765.781318	162391.164650	56.171149
2764.524519	162175.115426	56.176154
2764.264989	161941.325519	56.181159
2763.365269	161719.551840	56.186164
2762.727429	161499.785032	56.191169
2762.101193	161266.845869	56.196173
2761.343712	161039.040063	56.201178
2760.665846	160816.410400	56.206183
2760.064730	160600.152348	56.211188
2759.209028	160375.265102	56.216193
2758.888645	160153.193211	56.221197
2758.057504	159929.474557	56.226202
2757.822294	159703.527029	56.231207
2756.956414	159474.591463	56.236212
2756.142357	159249.539480	56.241217
2755.593595	159015.636561	56.246221
2754.785687	158790.090719	56.251226
2754.220917	158564.100987	56.256231
2753.467458	158336.578892	56.261236
2753.056670	158114.407025	56.266241
2752.446941	157887.996539	56.271245
2751.360225	157657.874655	56.276250
2751.144219	157428.646097	56.281255
2750.347413	157204.570705	56.286260
2749.463306	156975.044174	56.291265
2748.836961	156744.283358	56.296269
2747.815667	156517.603777	56.301274
2747.303727	156295.904516	56.306279
2746.515651	156081.915925	56.311284
2745.940621	155858.335353	56.316289
2745.322343	155641.169993	56.321293
2744.596837	155426.107771	56.326298
2743.991138	155194.299007	56.331303
2743.541079	154980.123934	56.336308
2742.674285	154748.346857	56.341313
2742.125725	154530.605502	56.346317
2741.342745	154316.500069	56.351322
2740.614430	154089.383438	56.356327
2740.053481	153877.851475	56.361332
2739.415520	153637.109619	56.366337
2739.259335	153425.465531	56.371341
2738.241742	153205.264783	56.376346
2737.520353	152972.091363	56.381351
2737.066493	152754.918493	56.386356
2736.121438	152522.317508	56.391361
2735.751512	152299.350834	56.396365
2734.540673	152075.807069	56.401370
2734.293487	151854.908498	56.406375
2733.584868	151626.953857	56.411380
2732.881801	151405.685633	56.416385
2732.164947	151177.646424	56.421389
2731.222569	150967.464408	56.426394
2730.980441	150735.145936	56.431399
2730.211407	150517.643655	56.436404
2729.204416	150290.940291	56.441409
2728.836976	150076.198958	56.446413
2727.943354	149865.762087	56.451418
2727.426914	149635.947888	56.456423
2726.683342	149430.840890	56.461428
2726.100075	149198.536552	56.466433
2725.818401	148969.566841	56.471437
2724.813603	148758.468442	56.476442
2724.038874	148532.058288	56.481447
2723.564407	148313.507339	56.486452
2722.713736	148086.476883	56.491457
2722.157363	147868.793448	56.496461
2721.503467	147648.597842	56.501466
2720.860731	147424.703678	56.506471
2719.854814	147211.594899	56.511476
2719.534097	146995.913487	56.516481
2718.981444	146765.706121	56.521485
2718.109739	146556.138898	56.526490
2717.891194	146327.762646	56.531495
2717.127051	146109.285378	56.536500
2716.002006	145894.387005	56.541505
2715.565004	145673.204881	56.546509
2714.645246	145454.121388	56.551514
2714.205589	145225.025649	56.556519
2713.411270	145011.440669	56.561524
2712.964215	144791.676922	56.566529
2712.226721	144568.084852	56.571533
2711.375478	144354.005064	56.576538
2710.910364	144116.979144	56.581543
2710.506720	143900.620430	56.586548
2709.702454	143687.058792	56.591553
2708.786577	143467.200752	56.596557
2707.934100	143261.947581	56.601562
2707.575231	143029.322552	56.606567
2706.658624	142820.028889	56.611572
2706.014651	142611.354217	56.616577
2705.454181	142393.734770	56.621581
2704.634654	142180.719656	56.626586
2704.242082	141952.657142	56.631591
2703.421461	141736.913339	56.636596
2702.910626	141523.955538	56.641601
2702.255810	141304.084306	56.646605
2701.344123	141095.576731	56.651610
2700.768389	140862.773780	56.656615
2700.248218	140659.581920	56.661620
2699.596482	140443.871343	56.666625
2699.062945	140222.591052	56.671629
2697.923600	140007.634258	56.676634
2697.471436	139788.809199	56.681639
2696.929471	139591.002535	56.686644
2696.212123	139365.348762	56.691649
2695.686459	139144.113257	56.696653
2694.682000	138928.520233	56.701658
2694.043744	138700.610064	56.706663
2693.209294	138494.623899	56.711668
2692.649666	138285.266853	56.716673
2692.051524	138071.407072	56.721677
2691.369018	137864.676996	56.726682
2690.961463	137643.687997	56.731687
2690.424700	137433.024723	56.736692
2689.188114	137217.811192	56.741697
2688.731348	137008.535786	56.746701
2688.112728	136793.049574	56.751706
2687.824437	136576.191336	56.756711
2686.953224	136367.519733	56.761716
2685.956848	136158.030961	56.766721
2685.519567	135940.629327	56.771725
2685.024362	135721.104197	56.776730
2684.242295	135513.174092	56.781735
2683.349598	135303.154150	56.786740
2682.693634	135091.497532	56.791745
2682.361481	134879.524369	56.796749
2681.366077	134659.197226	56.801754
2680.846004	134442.810758	56.806759
2680.468596	134233.415595	56.811764
2679.319820	134019.837733	56.816769
2678.878251	133803.951738	56.821773
2678.190658	133595.004149	56.826778
2677.606145	133378.851813	56.831783
2676.798146	133173.838902	56.836788
2676.216397	132959.797973	56.841793
2675.926102	132735.982135	56.846797
2674.848304	132538.130074	56.851802
2674.465337	132313.938438	56.856807
2673.815395	132108.958922	56.861812
2673.016620	131891.899074	56.866817
2672.241096	131676.704437	56.871821
2671.550834	131467.467958	56.876826
2670.958418	131246.379151	56.881831
2670.179514	131035.699162	56.886836
2669.667566	130821.548926	56.891841
2669.249644	130608.871528	56.896845
2668.421232	130405.342512	56.901850
2667.717110	130182.577700	56.906855
2667.013347	129975.615304	56.911860
2666.448123	129749.821652	56.916865
2665.688145	129535.656995	56.921869
2664.780433	129320.336172	56.926874
2664.265174	129104.332467	56.931879
2663.528669	128896.735480	56.936884
2663.128986	128693.544705	56.941889
2662.655571	128469.461485	56.946893
2661.653535	128268.884026	56.951898
2660.955342	128052.917470	56.956903
2660.384838	127839.574082	56.961908
2659.483592	127636.521324	56.966913
2658.908930	127420.692536	56.971917
2657.987110	127202.951904	56.976922
2657.555109	126989.059733	56.981927
2657.113935	126784.670335	56.986932
2656.236134	126582.586841	56.991937
2655.509258	126364.885461	56.996941
2654.959383	126155.526923	57.001946
2654.291533	125946.442675	57.006951
2653.691507	125741.438551	57.011956
2653.098712	125529.881881	57.016961
2652.503761	125322.225912	57.021965
2651.650906	125107.538886	57.026970
2650.878295	124894.453641	57.031975
2650.139495	124692.362135	57.036980
2649.394460	124486.526919	57.041985
2649.087054	124276.839650	57.046989
2648.302347	124072.055188	57.051994
2647.877611	123852.878396	57.056999
2647.331759	123641.887785	57.062004
2646.351398	123433.189920	57.067009
2645.961803	123217.339751	57.072013
2645.083323	123003.854482	57.077018
2644.707746	122788.767443	57.082023
2643.619090	122583.318707	57.087028
2642.877769	122378.210153	57.092033
2642.384264	122153.928162	57.097037
2641.679488	121950.645608	57.102042
2641.031898	121737.387848	57.107047
2640.505807	121538.613214	57.112052
2639.609417	121331.594576	57.117057
2638.999564	121119.618255	57.122061
2638.481606	120909.165445	57.127066
2637.691046	120697.030691	57.132071
2637.265928	120491.074013	57.137076
2636.301005	120295.565246	57.142081
2635.949821	120074.363705	57.147085
2634.969740	119869.794920	57.152090
2634.411989	119654.317823	57.157095
2634.067669	119450.375281	57.162100
2633.219014	119246.514248	57.167105
2632.436993	119029.040054	57.172109
2631.564265	118812.661233	57.177114
2631.329688	118598.284304	57.182119
2630.731326	118397.875353	57.187124
2629.935738	118184.022410	57.192129
2629.425907	117969.497502	57.197133
2628.665531	117760.111428	57.202138
2628.182185	117546.937926	57.207143
2627.337037	117325.895136	57.212148
2626.419319	117118.684748	57.217153
2625.703497	116900.887844	57.222157
2625.161502	116703.085652	57.227162
2624.584097	116485.429025	57.232167
2623.756588	116284.825241	57.237172
2623.436442	116079.502622	57.242177
2622.922583	115862.336322	57.247181
2621.979087	115655.916224	57.252186
2621.061508	115440.397986	57.257191
2620.513836	115226.105099	57.262196
2619.862668	115027.266834	57.267201
2619.335262	114807.407759	57.272205
2618.241494	114608.826978	57.277210
2617.703865	114393.790565	57.282215
2617.396799	114190.042491	57.287220
2616.410694	113994.851462	57.292225
2616.069318	113777.129819	57.297229
2615.232700	113570.950942	57.302234
2614.458153	113359.318367	57.307239
2614.037914	113161.835436	57.312244
2613.278030	112948.103228	57.317249
2612.524668	112735.177832	57.322253
2611.534591	112530.992926	57.327258
2611.056691	112319.119029	57.332263
2610.632474	112117.005650	57.337268
2609.854161	111918.040735	57.342273
2609.390402	111714.280469	57.347277
2608.541503	111504.173119	57.352282
2607.610414	111297.361593	57.357287
2607.275555	111096.200630	57.362292
2606.333069	110887.826809	57.367297
2605.504000	110684.773850	57.372301
2604.862979	110487.664402	57.377306
2604.322614	110276.255706	57.382311
2603.673386	110074.004250	57.387316
2602.512170	109877.965738	57.392321
2602.433608	109669.186075	57.397325
2601.704503	109488.096483	57.402330
2600.948134	109280.480946	57.407335
2600.342940	109073.103382	57.412340
2599.582967	108870.961879	57.417345
2598.891803	108670.105644	57.422349
2598.141437	108481.691362	57.427354
2597.442720	108279.729066	57.432359
2596.960284	108071.693310	57.437364
2596.153288	107886.186129	57.442369
2595.536350	107672.775176	57.447373
2594.933888	107490.830059	57.452378
2594.339257	107295.141284	57.457383
2593.912050	107090.131863	57.462388
2593.181399	106895.768635	57.467393
2592.560051	106687.183019	57.472397
2591.864951	106491.104245	57.477402
2591.290615	106281.023611	57.482407
2590.609329	106080.986726	57.487412
2590.030357	105877.312373	57.492417
2589.490918	105668.392672	57.497421
2588.603169	105465.881089	57.502426
2588.132638	105262.486630	57.507431
2587.327888	105064.254309	57.512436
2586.811973	104856.771852	57.517441
2586.272080	104646.052941	57.522445
2585.134890	104449.058502	57.527450
2584.508117	104244.999583	57.532455
2583.840741	104045.935529	57.537460
2583.247923	103842.572566	57.542465
2582.810659	103630.894736	57.547469
2581.921466	103441.330213	57.552474
2581.308639	103233.756744	57.557479
2580.862067	103031.170590	57.562484
2579.883599	102833.694962	57.567489
2579.612537	102622.704008	57.572493
2578.772485	102421.530381	57.577498
2577.949628	102211.271306	57.582503
2577.553337	102009.149077	57.587508
2576.555970	101806.438725	57.592513
2576.147773	101595.986226	57.597517
2574.932426	101395.724591	57.602522
2574.438355	101200.463306	57.607527
2573.981293	101001.886452	57.612532
2573.164658	100804.865343	57.617537
2572.594847	100607.559387	57.622541
2571.996036	100408.350338	57.627546
2571.098581	100204.432824	57.632551
2570.530344	100002.875371	57.637556
2569.705447	99808.363274	57.642561
2569.459494	99600.199343	57.647565
2568.758080	99408.265394	57.652570
2567.922478	99204.873357	57.657575
2567.425926	99009.656260	57.662580
2566.723483	98808.625242	57.667585
2566.101638	98602.293225	57.672589
2565.191175	98415.018311	57.677594
2564.594927	98205.711001	57.682599
2563.952399	98010.011757	57.687604
2563.414701	97811.227711	57.692609
2562.962076	97608.518507	57.697613
2562.153947	97411.924598	57.702618
2561.142289	97210.354054	57.707623
2560.634884	97002.115556	57.712628
2559.874002	96814.341667	57.717633
2559.653677	96608.839235	57.722637
2558.720232	96403.718062	57.727642
2557.984069	96200.489170	57.732647
2557.615022	96006.197120	57.737652
2556.774814	95806.146658	57.742657
2556.317424	95605.682134	57.747661
2555.661811	95405.396671	57.752666
2554.993066	95196.128518	57.757671
2554.302131	94993.486760	57.762676
2553.186538	94796.285671	57.767681
2552.957546	94595.781235	57.772685
2551.895260	94398.207364	57.777690
2550.972414	94200.987290	57.782695
2550.814865	93997.737266	57.787700
2549.931234	93810.813193	57.792705
2549.545329	93614.483435	57.797709
2548.482664	93421.928026	57.802714
2548.128864	93216.522061	57.807719
2547.650534	93025.868649	57.812724
2546.626344	92820.883313	57.817729
2546.033683	92610.701420	57.822733
2545.492843	92414.939443	57.827738
2544.729082	92219.132091	57.832743
2544.034876	92017.151941	57.837748
2543.457618	91823.214499	57.842753
2543.081169	91630.179045	57.847757
2542.423879	91432.560945	57.852762
2541.444445	91226.391175	57.857767
2540.859413	91024.789577	57.862772
2540.117081	90827.957605	57.867777
2539.702759	90615.724689	57.872781
2538.892144	90421.906301	57.877786
2537.962599	90231.234360	57.882791
2537.853068	90025.597376	57.887796
2536.710417	89830.714578	57.892801
2536.481861	89624.599330	57.897805
2535.530606	89429.182543	57.902810
2534.816347	89228.169543	57.907815
2534.423097	89027.995139	57.912820
2533.518539	88833.425874	57.917825
2532.899272	88636.676522	57.922829
2532.061770	88433.446005	57.927834
2531.604712	88238.931587	57.932839
2531.052128	88045.385039	57.937844
2530.536978	87841.582758	57.942849
2529.547444	87636.437478	57.947853
2528.679256	87442.071460	57.952858
2528.086672	87237.583434	57.957863
2527.637302	87038.983158	57.962868
2527.062198	86859.499369	57.967873
2526.448690	86649.061061	57.972877
2525.794702	86449.737913	57.977882
2525.067379	86252.298354	57.982887
2524.313587	86051.023180	57.987892
2523.614219	85853.303932	57.992897
2523.266996	85650.636829	57.997901
2522.154207	85459.072385	58.002906
2521.557924	85257.735329	58.007911
2520.774816	85048.182721	58.012916
2519.999086	84867.010530	58.017921
2519.527230	84673.659039	58.022925
2518.663895	84474.571313	58.027930
2518.002739	84277.393072	58.032935
2517.598093	84090.825071	58.037940
2516.747617	83899.271117	58.042945
2516.540374	83698.616094	58.047949
2515.868371	83502.828593	58.052954
2515.005402	83306.997113	58.057959
2514.574562	83102.383595	58.062964
2513.486940	82914.875704	58.067969
2513.160822	82706.655562	58.072973
2512.591036	82511.704047	58.077978
2511.515545	82320.909967	58.082983
2510.948798	82116.974061	58.087988
2510.318583	81927.602432	58.092993
2509.997783	81715.106722	58.097997
2508.941381	81523.049268	58.103002
2508.406906	81332.381237	58.108007
2507.931467	81135.754348	58.113012
2506.526472	80935.207806	58.118017
2506.274023	80737.807796	58.123021
2505.705221	80553.350615	58.128026
2504.988682	80352.960388	58.133031
2504.351630	80152.660892	58.138036
2503.822113	79960.166737	58.143041
2502.868050	79760.643748	58.148045
2502.415802	79570.346385	58.153050
2501.359100	79386.382503	58.158055
2501.111243	79183.305629	58.163060
2499.993790	78999.139356	58.168065
2499.513598	78803.498550	58.173069
2499.040705	78604.962399	58.178074
2498.261368	78404.385525	58.183079
2497.717358	78223.855100	58.188084
2496.498601	78034.434828	58.193089
2496.497137	77831.509641	58.198093
2495.365523	77645.019439	58.203098
2494.732048	77446.291808	58.208103
2494.432106	77256.257814	58.213108
2493.361063	77075.935097	58.218113
2493.055899	76879.385070	58.223117
2492.283260	76691.319548	58.228122
2491.751542	76499.745209	58.233127
2491.128618	76295.736181	58.238132
2490.229744	76109.413193	58.243137
2489.763099	75916.541418	58.248141
2488.913419	75727.248774	58.253146
2488.303036	75538.781673	58.258151
2487.850805	75336.637038	58.263156
2487.049735	75149.027477	58.268161
2486.095567	74956.787008	58.273165
2485.528174	74768.478657	58.278170
2485.026918	74569.086561	58.283175
2484.762885	74376.159315	58.288180
2483.606210	74188.279254	58.293185
2483.315153	73987.351689	58.298189
2482.079508	73804.296481	58.303194
2481.449322	73611.377587	58.308199
2480.879329	73425.166588	58.313204
2480.395653	73235.573200	58.318209
2479.866061	73035.852343	58.323213
2479.328291	72849.153764	58.328218
2478.679246	72657.222672	58.333223
2478.083487	72461.122778	58.338228
2477.103603	72274.075204	58.343233
2476.721241	72072.832873	58.348237
2476.074626	71883.518868	58.353242
2475.146546	71692.686562	58.358247
2474.803737	71495.536146	58.363252
2474.338739	71304.672158	58.368257
2473.516670	71098.827980	58.373261
2472.641078	70899.411431	58.378266
2472.154675	70712.756410	58.383271
2471.326669	70506.520248	58.388276
2470.201068	70318.202952	58.393281
2469.668055	70120.608612	58.398285
2469.073507	69930.912265	58.403290
2468.351885	69736.088116	58.408295
2467.906338	69547.803383	58.413300
2467.017571	69363.397550	58.418305
2466.567982	69176.852569	58.423309
2465.930864	68982.655895	58.428314
2465.285300	68790.597032	58.433319
2464.800755	68602.435219	58.438324
2464.035661	68408.891575	58.443329
2463.169934	68209.076343	58.448333
2462.763430	68021.908478	58.453338
2461.906684	67829.835522	58.458343
2461.439840	67636.841272	58.463348
2460.724596	67436.199393	58.468353
2460.070517	67241.402017	58.473357
2459.095633	67053.294871	58.478362
2458.485097	66852.775410	58.483367
2458.500729	66661.031681	58.488372
2457.388113	66473.312988	58.493377
2456.821951	66267.067309	58.498381
2456.089169	66084.260532	58.503386
2455.280232	65890.102920	58.508391
2455.020181	65693.792521	58.513396
2454.307134	65501.181526	58.518401
2453.607530	65302.639614	58.523405
2452.762863	65117.472248	58.528410
2451.951044	64912.660528	58.533415
2451.676847	64713.328985	58.538420
2450.675556	64522.052681	58.543425
2450.022931	64316.364012	58.548429
2449.390348	64129.880706	58.553434
2448.688042	63952.424438	58.558439
2448.064615	63750.197873	58.563444
2447.447006	63566.769863	58.568449
2446.304804	63366.323492	58.573453
2445.857332	63177.967949	58.578458
2445.173594	62996.252920	58.583463
2444.813142	62796.518097	58.588468
2443.881125	62613.304240	58.593473
2443.293873	62419.678511	58.598477
2442.623749	62233.672418	58.603482
2441.761212	62051.868123	58.608487
2441.248514	61863.874682	58.613492
2440.593725	61672.220618	58.618497
2440.284667	61483.730119	58.623501
2439.450766	61292.443872	58.628506
2438.780025	61098.626438	58.633511
2437.871077	60906.257495	58.638516
2437.269965	60723.018958	58.643521
2436.729996	60524.308407	58.648525
2435.948017	60335.948669	58.653530
2435.136799	60151.121893	58.658535
2434.454403	59955.558014	58.663540
2433.843060	59782.203560	58.668545
2433.435170	59593.560871	58.673549
2432.910094	59403.055223	58.678554
2432.046325	59225.114907	58.683559
2431.566205	59027.357168	58.688564
2430.828387	58846.795377	58.693569
2430.154732	58648.695654	58.698573
2429.572217	58467.457689	58.703578
2428.971258	58267.748852	58.708583
2428.183319	58076.586229	58.713588
2427.273703	57898.536060	58.718593
2426.798416	57699.762947	58.723597
2426.094237	57513.448174	58.728602
2425.290398	57326.961169	58.733607
2425.140618	57131.829851	58.738612
2424.017787	56948.796497	58.743617
2423.749250	56755.454056	58.748621
2422.655657	56567.033033	58.753626
2421.889014	56373.783056	58.758631
2421.431190	56191.873417	58.763636
2420.528072	56011.586960	58.768641
2420.176802	55812.513789	58.773645
2419.557778	55623.324570	58.778650
2418.634059	55435.385054	58.783655
2418.489177	55253.555324	58.788660
2417.554174	55072.691320	58.793665
2416.575636	54877.512714	58.798669
2416.222432	54686.411186	58.803674
2415.389403	54499.099809	58.808679
2415.100787	54307.368568	58.813684
2414.090904	54128.351720	58.818689
2413.308289	53930.541407	58.823693
2412.786930	53751.498262	58.828698
2412.058909	53566.322148	58.833703
2411.455020	53373.090639	58.838708
2411.048711	53189.095138	58.843713
2410.299710	53013.772343	58.848717
2409.634094	52812.471680	58.853722
2409.093365	52635.208271	58.858727
2408.449518	52435.433519	58.863732
2407.701725	52258.934398	58.868737
2407.114849	52060.034402	58.873741
2406.407916	51876.207464	58.878746
2405.366338	51688.885323	58.883751
2405.149211	51484.221810	58.888756
2403.961857	51305.172353	58.893761
2403.549678	51113.810817	58.898765
2403.137234	50931.636387	58.903770
2402.338034	50747.784955	58.908775
2401.858127	50554.313932	58.913780
2401.074906	50366.338124	58.918785
2400.412855	50165.996579	58.923789
2399.920268	49979.209478	58.928794
2398.863575	49799.828431	58.933799
2398.785565	49597.644730	58.938804
2397.829526	49417.546039	58.943809
2396.972121	49220.972898	58.948813
2396.177305	49033.057219	58.953818
2395.348410	48855.392700	58.958823
2395.017351	48662.219064	58.963828
2394.096171	48482.032548	58.968833
2393.573290	48282.866886	58.973837
2392.934555	48105.594116	58.978842
2392.062579	47921.748493	58.983847
2391.740743	47734.059401	58.988852
2390.878941	47550.491228	58.993857
2390.490331	47357.369368	58.998861
2389.649217	47173.827125	59.003866
2388.828518	46991.972741	59.008871
2388.471324	46802.059527	59.013876
2387.337384	46631.393162	59.018881
2386.807043	46450.482071	59.023885
2386.291882	46260.998288	59.028890
2385.670665	46078.571295	59.033895
2385.215144	45893.424969	59.038900
2384.160430	45708.119401	59.043905
2383.866341	45515.429720	59.048909
2383.320222	45342.149068	59.053914
2382.802707	45151.871044	59.058919
2381.935964	44952.066828	59.063924
2381.004058	44765.094379	59.068929
2380.378886	44575.538684	59.073933
2379.695191	44388.122897	59.078938
2379.096756	44211.996215	59.083943
2378.607801	44017.355036	59.088948
2377.716838	43831.097708	59.093953
2377.145845	43639.117787	59.098957
2376.449442	43464.718872	59.103962
2375.705875	43274.000613	59.108967
2375.195256	43083.364521	59.113972
2374.356144	42908.253775	59.118977
2373.795306	42709.694925	59.123981
2373.081224	42528.881991	59.128986
2372.344088	42349.772833	59.133991
2371.957995	42164.240765	59.138996
2371.478681	41983.889629	59.144001
2370.686999	41788.372719	59.149005
2369.903525	41597.359845	59.154010
2368.967353	41412.615623	59.159015
2368.567551	41234.081177	59.164020
2367.483591	41052.567600	59.169025
2366.885200	40860.803068	59.174029
2366.425031	40682.204864	59.179034
2365.890355	40502.383946	59.184039
2365.371544	40307.934659	59.189044
2364.487127	40118.816663	59.194049
2363.914253	39937.322360	59.199053
2363.196267	39760.017303	59.204058
2362.647319	39576.138909	59.209063
2362.290136	39375.077202	59.214068
2360.826224	39203.181322	59.219073
2360.488316	39008.662769	59.224077
2360.102178	38825.779998	59.229082
2359.313867	38639.077162	59.234087
2358.796550	38453.700844	59.239092
2357.775193	38265.878705	59.244097
2357.038304	38077.776405	59.249101
2356.406627	37898.919893	59.254106
2355.748582	37718.643570	59.259111
2355.185361	37533.254536	59.264116
2354.509198	37355.362437	59.269121
2353.606018	37169.729368	59.274125
2353.485888	36982.576792	59.279130
2352.770637	36806.248936	59.284135
2352.313631	36618.567368	59.289140
2351.434013	36432.995557	59.294145
2350.809001	36242.211921	59.299149
2350.205792	36062.910331	59.304154
2349.457690	35871.189387	59.309159
2348.854491	35690.004504	59.314164
2347.755301	35501.762298	59.319169
2347.219141	35313.051994	59.324173
2347.033671	35127.749603	59.329178
2345.840327	34948.662546	59.334183
2345.318448	34757.765600	59.339188
2344.406111	34581.105096	59.344193
2344.091243	34395.652722	59.349197
2343.467494	34214.932729	59.354202
2342.628858	34033.823628	59.359207
2342.017465	33833.141589	59.364212
2340.987689	33665.203341	59.369217
2340.391121	33481.566374	59.374221
2340.087039	33297.971964	59.379226
2339.291321	33125.847220	59.384231
2338.574402	32939.649844	59.389236
2338.050399	32759.549308	59.394241
2337.395833	32572.292082	59.399245
2336.566911	32393.460715	59.404250
2335.790646	32216.347009	59.409255
2335.435182	32022.868091	59.414260
2334.388303	31845.831290	59.419265
2333.633351	31664.028379	59.424269
2333.430152	31486.833174	59.429274
2332.443613	31313.050898	59.434279
2331.983242	31137.505701	59.439284
2331.298254	30953.149122	59.444289
2330.675823	30763.650816	59.449293
2329.878034	30590.377152	59.454298
2329.317630	30410.338003	59.459303
2328.677221	30229.292777	59.464308
2328.068705	30049.450081	59.469313
2327.156896	29880.351249	59.474317
2326.685127	29685.131174	59.479322
2325.880511	29504.695118	59.484327
2325.172321	29319.824921	59.489332
2324.482700	29154.461900	59.494337
2323.839326	28966.671927	59.499341
2323.623551	28804.808009	59.504346
2322.345728	28628.106360	59.509351
2322.145545	28435.101631	59.514356
2320.893945	28266.327750	59.519361
2320.551850	28090.913323	59.524365
2320.010798	27916.728296	59.529370
2319.059494	27742.385863	59.534375
2318.297717	27556.668914	59.539380
2317.879731	27388.452837	59.544385
2317.251286	27203.800947	59.549389
2316.844601	27032.883736	59.554394
2315.889431	26857.546684	59.559399
2315.473408	26678.851213	59.564404
2314.695959	26499.995456	59.569409
2313.677388	26324.856691	59.574413
2313.043675	26150.730604	59.579418
2312.356185	25975.989374	59.584423
2312.009763	25798.403897	59.589428
2311.122684	25623.995900	59.594433
2310.459508	25453.797145	59.599437
2309.733779	25276.854138	59.604442
2308.695774	25109.918750	59.609447
2308.567234	24932.508080	59.614452
2307.678213	24769.231425	59.619457
2306.714316	24602.846347	59.624461
2306.394538	24432.551815	59.629466
2305.786862	24263.537558	59.634471
2305.322518	24087.928518	59.639476
2304.502660	23916.410970	59.644481
2303.574660	23744.558617	59.649485
2302.945627	23580.980381	59.654490
2301.819073	23415.445278	59.659495
2301.487058	23253.064716	59.664500
2300.906690	23082.195705	59.669505
2300.178369	22927.448960	59.674509
2299.449346	22757.478822	59.679514
2298.861178	22594.058214	59.684519
2298.118025	22429.844986	59.689524
2297.387443	22274.163674	59.694529
2296.857061	22111.565626	59.699533
2296.300524	21931.573723	59.704538
2295.383903	21773.914828	59.709543
2295.132735	21605.001708	59.714548
2294.390198	21430.492590	59.719553
2293.657306	21280.228665	59.724557
2293.069649	21115.456394	59.729562
2292.387750	20944.967587	59.734567
2291.699425	20768.555844	59.739572
2290.933967	20604.998307	59.744577
2290.399056	20445.552683	59.749581
2289.462547	20280.500996	59.754586
2288.548953	20123.352347	59.759591
2288.521154	19967.562522	59.764596
2287.919775	19796.680163	59.769601
2287.069944	19631.917997	59.774605
2286.412430	19468.400934	59.779610
2285.732982	19306.794525	59.784615
2285.111870	19133.876498	59.789620
2284.320065	18978.978332	59.794625
2283.541617	18810.741683	59.799629
2283.159539	18645.358702	59.804634
2282.169045	18485.749829	59.809639
2281.935474	18319.682398	59.814644
2281.222758	18162.781648	59.819649
2280.245487	17994.443213	59.824653
2279.707403	17834.872644	59.829658
2278.921865	17678.054234	59.834663
2278.784282	17507.540489	59.839668
2277.532871	17341.065483	59.844673
2276.778996	17186.419842	59.849677
2276.177862	17031.555741	59.854682
2275.331464	16878.017202	59.859687
2274.636836	16718.209382	59.864692
2273.834664	16562.211794	59.869697
2273.633876	16411.039868	59.874701
2272.831503	16251.599485	59.879706
2271.965127	16101.426147	59.884711
2271.323732	15936.178175	59.889716
2270.491087	15784.410077	59.894721
2269.600595	15635.090854	59.899725
2269.088131	15486.903786	59.904730
2268.456381	15345.286124	59.909735
2267.889740	15192.734957	59.914740
2267.107708	15043.885320	59.919745
2266.316309	14903.598377	59.924750
2265.373553	14743.297614	59.929754
2264.702938	14616.741715	59.934759
2263.988268	14478.003999	59.939764
2263.158103	14336.340061	59.944769
2262.209530	14208.072369	59.949774
2261.692700	14071.564775	59.954778
2260.573140	13943.648622	59.959783
2259.744631	13811.414886	59.964788
2259.081649	13696.522832	59.969793
2258.262129	13582.008385	59.974798
2257.074647	13469.971671	59.979802
2255.987533	13371.889358	59.984807
2254.992972	13269.530823	59.989812
2254.063269	13189.193640	59.994817
2252.832724	13101.741808	59.999822
2252.051594	13028.727192	60.004826
2250.808828	12951.049677	60.009831
2250.189057	12871.614287	60.014836
2249.483080	12805.029381	60.019841
2248.665547	12742.723225	60.024846
2247.930575	12690.639353	60.029850
2247.148987	12613.977875	60.034855
2246.702477	12561.455976	60.039860
2245.983502	12507.703087	60.044865
2245.015326	12436.893533	60.049870
2244.956474	12378.957233	60.054874
2244.132320	12322.340485	60.059879
2243.848668	12255.476755	60.064884
2243.309497	12206.813627	60.069889
2242.810261	12123.328021	60.074894
2242.440312	12065.074721	60.079898
2241.402105	12004.574654	60.084903
2240.929074	11927.748029	60.089908
2240.108267	11864.846247	60.094913
2239.298535	11806.468592	60.099918
2238.861093	11726.470191	60.104922
2238.359848	11666.726109	60.109927
2238.110083	11591.759049	60.114932
2237.259982	11540.697580	60.119937
2236.496162	11467.902834	60.124942
2236.143589	11397.130768	60.129946
2235.294763	11334.135217	60.134951
2234.865853	11253.757013	60.139956
2234.162513	11189.566191	60.144961
2233.295074	11116.582828	60.149966
2232.513956	11048.110729	60.154970
2232.018372	10986.716675	60.159975
2231.526432	10917.926268	60.164980
2230.503304	10858.509815	60.169985
2230.310422	10775.675623	60.174990
2229.563030	10703.106040	60.179994
2228.943733	10645.657416	60.184999
2228.291670	10568.960756	60.190004
2227.683744	10499.302959	60.195009
2226.904191	10435.400439	60.200014
2226.144449	10355.267081	60.205018
2225.424514	10291.238933	60.210023
2224.835781	10229.473335	60.215028
2224.297092	10175.814127	60.220033
2223.669798	10104.840764	60.225038
2223.175057	10032.200787	60.230042
2222.261909	9974.095151	60.235047
2222.015367	9894.298838	60.240052
2221.058061	9823.571279	60.245057
2220.408276	9752.252817	60.250062
2219.936380	9697.001160	60.255066
2219.038201	9625.017328	60.260071
2218.671300	9549.101574	60.265076
2217.460592	9481.570269	60.270081
2216.778616	9408.323908	60.275086
2216.515462	9341.816541	60.280090
2215.567918	9285.792892	60.285095
2215.091178	9211.605220	60.290100
2214.567582	9152.674847	60.295105
2213.571311	9086.581177	60.300110
2213.291051	9015.314883	60.305114
2212.744807	8958.145524	60.310119
2212.076092	8888.018017	60.315124
2211.202403	8824.725442	60.320129
2210.907955	8748.661792	60.325134
2210.172311	8675.372288	60.330138
2209.046825	8609.093724	60.335143
2208.370999	8534.737426	60.340148
2208.247385	8464.746716	60.345153
2207.281165	8416.445202	60.350158
2206.801269	8343.953815	60.355162
2206.333396	8282.057114	60.360167
2205.625419	8202.581428	60.365172
2204.790214	8131.770277	60.370177
2203.699642	8070.274615	60.375182
2203.439063	7994.272132	60.380186
2202.623591	7931.156337	60.385191
2201.761008	7873.676818	60.390196
2201.169237	7813.547586	60.395201
2200.559293	7745.888555	60.400206
2200.085604	7682.192199	60.405210
2199.149137	7619.582489	60.410215
2198.271248	7559.028303	60.415220
2197.643651	7490.584328	60.420225
2197.162657	7432.337537	60.425230
2196.836785	7365.114809	60.430234
2195.890909	7311.786826	60.435239
2195.384847	7238.306605	60.440244
2194.647493	7179.010446	60.445249
2194.332870	7120.428445	60.450254
2193.682660	7052.462603	60.455258
2192.600211	6985.683479	60.460263
2192.306553	6919.765593	60.465268
2191.374917	6848.666981	60.470273
2190.687330	6801.038046	60.475278
2190.248580	6737.684119	60.480282
2189.197907	6666.632873	60.485287
2188.517876	6604.442305	60.490292
2188.009887	6537.056566	60.495297
2187.269357	6480.131814	60.500302
2186.971676	6409.682543	60.505306
2186.063831	6358.948016	60.510311
2185.193499	6291.456799	60.515316
2184.704618	6240.221558	60.520321
2184.345008	6174.702381	60.525326
2184.013106	6098.511030	60.530330
2182.624928	6033.621861	60.535335
2182.242704	5965.433880	60.540340
2181.613585	5906.929423	60.545345
2180.632326	5848.519719	60.550350
2180.465922	5778.296351	60.555354
2179.451184	5724.293995	60.560359
2179.039902	5662.581790	60.565364
2178.032694	5605.326446	60.570369
2177.523480	5540.486137	60.575374
2177.011767	5479.435862	60.580378
2176.140182	5427.707259	60.585383
2175.484918	5369.415734	60.590388
2175.188005	5300.351973	60.595393
2174.252823	5234.809946	60.600398
2173.832586	5167.283981	60.605402
2172.707966	5117.690019	60.610407
2172.070749	5038.340670	60.615412
2171.678633	4983.312274	60.620417
2170.662843	4930.377818	60.625422
2170.410102	4873.917408	60.630426
2169.597756	4805.748577	60.635431
2169.086043	4743.494541	60.640436
2168.299454	4678.257949	60.645441
2167.389389	4625.445053	60.650446
2167.101066	4557.168986	60.655450
2166.188903	4494.399021	60.660455
2165.648888	4422.458803	60.665460
2165.077116	4370.465486	60.670465
2164.055267	4316.771490	60.675470
2163.765549	4249.996437	60.680474
2162.681018	4198.008580	60.685479
2162.025410	4135.331943	60.690484
2161.616559	4073.780567	60.695489
2160.577370	4015.721718	60.700494
2160.349140	3956.587184	60.705498
2159.492633	3895.951498	60.710503
2159.137385	3831.446017	60.715508
2158.635871	3780.720545	60.720513
2157.618475	3723.483584	60.725518
2156.948735	3656.591692	60.730522
2156.296956	3595.669223	60.735527
2155.836322	3548.750597	60.740532
2155.018933	3487.734183	60.745537
2154.135971	3430.299581	60.750542
2153.278424	3375.683065	60.755546
2152.796316	3323.131087	60.760551
2152.293426	3265.763798	60.765556
2151.561212	3201.550395	60.770561
2150.933099	3154.889892	60.775566
2150.183520	3088.203324	60.780570
2149.918709	3035.071353	60.785575
2149.339786	2981.497291	60.790580
2148.468431	2922.809655	60.795585
2147.901715	2860.765521	60.800590
2147.345404	2789.220730	60.805594
2146.322942	2748.552361	60.810599
2146.122746	2685.792290	60.815604
2145.342489	2619.307515	60.820609
2144.306687	2558.813845	60.825614
2143.894884	2507.454724	60.830618
2143.293126	2453.467451	60.835623
2142.499310	2393.155308	60.840628
2141.878123	2339.822155	60.845633
2140.913753	2276.295524	60.850638
2140.749323	2216.944933	60.855642
2139.629113	2167.346044	60.860647
2139.110069	2108.867588	60.865652
2138.613826	2051.525286	60.870657
2137.837056	2002.984398	60.875662
2137.012733	1931.985508	60.880666
2136.325628	1880.923832	60.885671
2135.788019	1818.047524	60.890676
2135.174875	1767.597500	60.895681
2134.127718	1716.916065	60.900686
2133.846945	1653.596741	60.905690
2133.106004	1602.136095	60.910695
2132.095437	1558.002544	60.915700
2131.489266	1502.021219	60.920705
2130.995376	1454.299975	60.925710
2130.195402	1404.055918	60.930714
2129.600389	1361.849747	60.935719
2128.961017	1301.737615	60.940724
2128.341694	1253.186857	60.945729
2127.676449	1203.495400	60.950734
2126.748550	1146.200703	60.955738
2126.283930	1098.596629	60.960743
2125.664060	1039.001357	60.965748
2125.375342	985.871942	60.970753
2124.079096	942.201159	60.975758
2123.671477	897.118361	60.980762
2122.916597	848.086584	60.985767
2122.135955	787.399699	60.990772
2121.419829	739.745237	60.995777
2120.463627	706.623886	61.000782
2120.179787	656.134918	61.005786
2119.451256	611.020346	61.010791
2118.773132	563.385666	61.015796
2118.066284	515.468676	61.020801
2117.448565	480.210846	61.025806
2116.935845	432.936723	61.030810
2115.790334	386.297784	61.035815
2115.468743	339.827887	61.040820
2114.814423	304.346046	61.045825
2113.935025	266.319998	61.050830
2113.476249	213.059534	61.055834
2112.647728	178.064559	61.060839
2111.865495	131.769355	61.065844
2111.373976	91.832382	61.070849
2110.218018	61.718439	61.075854
2109.584294	16.971518	61.080858
2108.957694	-11.031095	61.085863
2108.140645	-44.592287	61.090868
2107.447431	-67.399075	61.095873
2106.325221	-89.148980	61.100878
2105.557440	-119.737311	61.105882
2103.631924	-127.073794	61.110887
2100.680428	-71.051406	61.115892
2098.305065	-8.690829	61.120897
2098.171303	23.250378	61.125902
2098.803175	37.762581	61.130906
2099.080993	54.329832	61.135911
2099.575782	58.786778	61.140916
2099.486835	56.615181	61.145921
2099.186811	60.753544	61.150926
2099.497602	35.496676	61.155930
2098.622492	16.776244	61.160935
2097.811984	4.680002	61.165940
2096.865528	-3.542057	61.170945
2094.370697	24.668922	61.175950
2093.502479	25.587327	61.180954
2092.647737	40.510494	61.185959
2092.719801	41.552504	61.190964
2092.485777	41.447723	61.195969
2092.472727	46.303809	61.200974
2091.995160	32.260735	61.205978
2090.938002	28.512825	61.210983
2090.117366	40.588831	61.215988
2089.691894	35.225178	61.220993
2088.219352	41.419930	61.225998
2087.877632	48.075491	61.231002
2087.276041	44.895543	61.236007
2086.752498	41.097643	61.241012
2086.055797	48.758892	61.246017
2085.182033	52.523090	61.251022
2084.952009	43.873489	61.256026
2084.605935	50.253767	61.261031
2083.802559	55.001882	61.266036
2083.237088	42.169695	61.271041
2082.121593	49.323379	61.276046
2081.358866	45.058797	61.281050
2080.495041	55.078955	61.286055
2079.935133	53.234420	61.291060
2079.949639	53.255783	61.296065
2079.151245	57.374675	61.301070
2078.921251	47.443756	61.306074
2078.191419	56.555588	61.311079
2077.025117	53.155381	61.316084
2076.447586	58.636445	61.321089
2075.598973	57.539494	61.326094
2075.050551	48.330912	61.331098
2073.954220	60.325318	61.336103
2073.519317	56.184545	61.341108
2073.482341	61.007372	61.346113
2072.978477	68.134967	61.351118
2072.376602	59.848734	61.356122
2071.102229	65.728195	61.361127
2070.264301	64.129639	61.366132
2069.899021	60.248272	61.371137
2069.349241	63.765512	61.376142
2069.072145	64.538073	61.381146
2068.232048	64.993119	61.386151
2067.223876	62.358684	61.391156
2066.751739	54.604605	61.396161
2065.888658	63.627201	61.401166
2065.199469	65.059693	61.406170
2064.339771	59.586749	61.411175
2063.525967	60.908128	61.416180
2062.932831	63.837720	61.421185
2062.160502	73.023332	61.426190
2062.280754	62.963489	61.431194
2061.833678	67.935773	61.436199
2061.103924	58.915244	61.441204
2059.909576	61.931580	61.446209
2058.924648	71.709191	61.451214
2058.956244	67.728566	61.456218
2058.470794	60.168205	61.461223
2057.750963	62.412986	61.466228
2056.650199	60.676372	61.471233
2055.674687	73.111314	61.476238
2055.805804	66.601153	61.481242
2055.313726	70.348943	61.486247
2054.279481	66.693600	61.491252
2053.208962	62.958857	61.496257
2052.382353	66.885900	61.501262
2052.487034	70.398626	61.506266
2051.900389	70.442856	61.511271
2050.872090	69.699292	61.516276
2050.122443	63.379383	61.521281
2049.341974	61.853720	61.526286
2049.388576	62.658489	61.531290
2048.119472	61.483199	61.536295
2047.532573	75.075489	61.541300
2047.335245	66.395461	61.546305
2046.067305	69.739673	61.551310
2045.302616	66.230791	61.556314
2045.292928	69.126137	61.561319
2044.510935	75.578768	61.566324
2043.573041	66.793920	61.571329
2042.663068	69.507291	61.576334
2042.772316	65.462301	61.581338
2041.275417	78.000503	61.586343
2040.756222	75.370473	61.591348
2040.919806	75.942204	61.596353
2039.686435	86.416872	61.601358
2038.904687	75.654908	61.606362
2037.997773	71.900511	61.611367
2038.043100	72.754370	61.616372
2037.403278	62.760758	61.621377
2036.278344	71.607299	61.626382
2035.713952	68.681661	61.631386
2035.074459	68.213872	61.636391
2034.199357	67.584776	61.641396
2033.711358	69.015307	61.646401
2032.830673	70.602785	61.651406
2032.442025	62.865422	61.656410
2032.081100	68.167034	61.661415
2031.166578	75.378739	61.666420
2030.744042	62.076786	61.671425
2029.867842	66.903500	61.676430
2029.434516	66.202711	61.681434
2028.805201	68.493060	61.686439
2028.203915	68.347225	61.691444
2027.683254	69.260954	61.696449
2027.109765	77.667517	61.701454
2026.175593	70.917994	61.706458
2024.708621	70.264567	61.711463
2024.148779	77.399479	61.716468
2023.397141	71.803736	61.721473
2023.448821	81.162935	61.726478
2023.027683	75.156754	61.731482
2021.673847	77.626760	61.736487
2020.947616	71.705276	61.741492
2020.532915	70.968415	61.746497
2019.785308	74.928663	61.751502
2019.657044	71.738257	61.756506
2018.783664	78.020891	61.761511
2018.036747	82.200234	61.766516
2017.454543	73.849386	61.771521
2016.803608	72.702153	61.776526
2016.041519	77.994113	61.781530
2015.807898	68.085057	61.786535
2015.328082	78.473237	61.791540
2014.166040	66.877492	61.796545
2013.022058	81.088085	61.801550
2012.623866	81.012522	61.806554
2011.962772	75.903897	61.811559
2011.342186	73.837187	61.816564
2011.003226	74.703155	61.821569
2010.296220	74.129390	61.826574
2009.649318	71.923350	61.831578
2009.011424	69.829426	61.836583
2008.414223	79.253768	61.841588
2008.112168	73.616632	61.846593
2006.581075	75.961811	61.851598
2005.723333	73.052779	61.856602
2005.454775	70.452363	61.861607
2004.714868	72.241438	61.866612
2003.917092	71.043398	61.871617
2003.449680	76.454172	61.876622
2003.205856	67.651428	61.881626
2002.289344	75.649591	61.886631
2001.467981	76.440739	61.891636
2001.344880	67.327088	61.896641
2000.489588	76.386319	61.901646
2000.151786	79.912506	61.906650
1999.035615	74.663224	61.911655
1997.918299	71.787512	61.916660
1997.521965	68.959002	61.921665
1996.894826	66.284615	61.926670
1996.292661	73.923790	61.931674
1996.216474	70.649424	61.936679
1994.937203	73.072912	61.941684
1994.732717	71.597768	61.946689
1994.075642	77.406090	61.951694
1993.075217	65.684565	61.956698
1992.121143	64.410410	61.961703
1991.185212	67.544244	61.966708
1990.877192	65.998801	61.971713
1989.866376	71.931871	61.976718
1989.647647	73.914198	61.981722
1989.148031	67.534908	61.986727
1988.406263	67.893943	61.991732
1988.212908	64.573520	61.996737
1987.335140	72.786316	62.001742
1987.003928	65.123427	62.006746
1985.502888	69.789921	62.011751
1984.801226	69.434518	62.016756
1983.890989	68.099789	62.021761
1983.573484	78.447226	62.026766
1983.399401	68.445933	62.031770
1982.891338	64.894760	62.036775
1981.817851	72.078881	62.041780
1981.564244	66.275573	62.046785
1980.885939	73.076834	62.051790
1979.791135	63.813072	62.056794
1979.030941	66.526342	62.061799
1978.072872	63.940762	62.066804
1977.521817	69.910456	62.071809
1976.870499	75.240824	62.076814
1976.688531	66.570197	62.081818
1975.973094	67.144259	62.086823
1975.345860	80.384194	62.091828
1975.227735	67.519648	62.096833
1974.587997	82.202948	62.101838
1973.590537	73.071970	62.106842
1972.523473	77.506365	62.111847
1971.843307	74.685854	62.116852
1971.293327	73.435084	62.121857
1970.769293	84.143325	62.126862
1970.262312	75.892516	62.131866
1968.891172	79.062329	62.136871
1967.967477	80.137822	62.141876
1967.967110	73.292918	62.146881
1967.792510	75.358918	62.151886
1966.584024	75.940285	62.156890
1966.051586	75.649490	62.161895
1965.608891	78.178320	62.166900
1965.325651	70.428967	62.171905
1963.553503	77.962131	62.176910
1962.818113	72.604322	62.181914
1962.447798	68.633882	62.186919
1961.827842	69.058746	62.191924
1961.828774	74.625419	62.196929
1960.922005	73.253877	62.201934
1960.549981	75.006643	62.206938
1959.779401	74.228511	62.211943
1958.874041	68.240866	62.216948
1957.840771	65.394411	62.221953
1957.017802	70.248179	62.226958
1956.709520	72.959104	62.231962
1956.196978	76.335621	62.236967
1955.527323	73.334457	62.241972
1955.455267	75.712984	62.246977
1954.250012	77.180907	62.251982
1953.276894	75.763916	62.256986
1952.385824	72.566872	62.261991
1951.509026	67.757446	62.266996
1951.359221	67.916860	62.272001
1950.720631	75.392298	62.277006
1950.088151	70.488892	62.282010
1950.120812	69.862379	62.287015
1949.211504	80.575010	62.292020
1948.765605	64.906556	62.297025
1947.162495	67.917654	62.302030
1946.335109	67.678417	62.307034
1946.195647	78.428111	62.312039
1945.392559	75.135886	62.317044
1945.250093	75.436065	62.322049
1944.641564	75.535834	62.327054
1944.192600	74.534757	62.332058
1943.025402	69.738318	62.337063
1941.995526	66.921294	62.342068
1941.550713	69.644432	62.347073
1940.627479	72.784154	62.352078
1940.477675	72.333269	62.357082
1940.075550	65.390509	62.362087
1939.087384	65.041176	62.367092
1938.202216	68.660570	62.372097
1937.160402	73.356692	62.377102
1936.681142	64.536932	62.382106
1936.605308	72.653182	62.387111
1936.003857	70.209706	62.392116
1935.682156	61.440631	62.397121
1934.527574	75.137244	62.402126
1933.582928	72.033871	62.407130
1932.608363	66.770028	62.412135
1932.450508	76.654501	62.417140
1932.222357	64.290784	62.422145
1931.504646	66.139434	62.427150
1930.035187	69.447878	62.432154
1929.512744	68.590938	62.437159
1928.224701	85.190716	62.442164
1927.907778	68.585553	62.447169
1927.737129	67.237512	62.452174
1927.148890	74.206627	62.457178
1926.624117	69.394942	62.462183
1925.979983	74.184057	62.467188
1926.126511	67.277202	62.472193
1924.712085	72.909295	62.477198
1923.736583	74.155458	62.482202
1923.202426	69.830980	62.487207
1922.625815	72.333764	62.492212
1922.142458	67.922372	62.497217
1921.083852	65.109918	62.502222
1920.212644	61.491830	62.507226
1919.745460	73.212149	62.512231
1918.953716	74.203630	62.517236
1918.605653	66.061656	62.522241
1918.031552	67.915896	62.527246
1917.627971	77.022495	62.532250
1916.767294	74.981310	62.537255
1915.719738	70.484444	62.542260
1915.476817	59.916128	62.547265
1914.530451	69.607227	62.552270
1914.163274	74.819166	62.557274
1913.269970	60.372182	62.562279
1912.018822	61.283631	62.567284
1911.560870	64.054592	62.572289
1911.163573	67.416759	62.577294
1910.484125	67.694957	62.582298
1909.981101	70.644968	62.587303
1909.652993	69.798181	62.592308
1909.296754	64.079779	62.597313
1907.872103	67.953571	62.602318
1907.135217	69.666496	62.607322
1906.331363	62.238730	62.612327
1906.084062	73.954103	62.617332
1905.881260	71.366915	62.622337
1904.817246	69.430561	62.627342
1903.675361	64.880867	62.632346
1902.893230	66.438545	62.637351
1902.301977	68.126773	62.642356
1902.010040	58.745837	62.647361
1901.534603	73.682966	62.652366
1901.262240	70.890774	62.657370
1900.629116	59.166970	62.662375
1899.070854	59.393880	62.667380
1898.361730	57.229292	62.672385
1898.123943	69.547141	62.677390
1897.591084	74.648187	62.682394
1897.559877	64.543012	62.687399
1896.057509	68.864401	62.692404
1895.200415	55.963448	62.697409
1894.616144	64.617745	62.702414
1894.227272	61.533385	62.707418
1893.978845	64.988616	62.712423
1892.866208	68.117421	62.717428
1892.106611	59.365841	62.722433
1891.353930	68.259773	62.727438
1890.743548	64.634978	62.732442
1890.193793	69.757630	62.737447
1889.649100	70.962214	62.742452
1889.295357	62.161966	62.747457
1887.933811	70.070749	62.752462
1887.365737	66.723097	62.757466
1886.878051	72.173373	62.762471
1886.154832	74.584322	62.767476
1885.679965	72.488201	62.772481
1884.878495	71.626685	62.777486
1883.708886	66.209322	62.782490
1883.026767	67.602889	62.787495
1882.288249	74.479173	62.792500
1882.413615	67.704993	62.797505
1881.970480	73.783727	62.802510
1881.254022	72.235336	62.807514
1880.828404	65.524984	62.812519
1879.739915	63.460059	62.817524
1878.999578	64.369270	62.822529
1878.189170	67.107885	62.827534
1877.678273	74.657680	62.832538
1877.105475	67.907616	62.837543
1875.652598	68.166695	62.842548
1875.369493	57.981672	62.847553
1874.843086	60.930668	62.852558
1874.141598	64.869432	62.857562
1874.145766	64.903475	62.862567
1873.254376	69.175176	62.867572
1872.904361	64.785203	62.872577
1871.962987	68.579126	62.877582
1871.134633	67.955279	62.882586
1870.591590	61.769792	62.887591
1869.628548	81.546884	62.892596
1868.600547	66.056829	62.897601
1867.895599	77.158874	62.902606
1867.528953	64.873933	62.907610
1867.314330	69.033449	62.912615
1866.704858	70.431255	62.917620
1866.266838	69.456841	62.922625
1865.062467	68.206706	62.927630
1863.887531	69.851997	62.932634
1863.854200	69.226501	62.937639
1862.888179	79.840130	62.942644
1862.717961	71.706199	62.947649
1861.991182	70.946374	62.952654
1861.278288	71.020155	62.957658
1860.532645	68.241614	62.962663
1859.536420	76.548159	62.967668
1858.888267	72.255990	62.972673
1858.568485	72.089151	62.977678
1858.100167	70.203313	62.982682
1857.202867	69.210361	62.987687
1856.439421	68.448476	62.992692
1855.866963	63.187053	62.997697
1855.536756	67.580970	63.002702
1854.752359	71.088192	63.007706
1853.779848	66.014874	63.012711
1852.904899	73.051603	63.017716
1852.519930	66.098253	63.022721
1852.000509	72.331033	63.027726
1851.628204	73.680145	63.032730
1851.231269	58.001592	63.037735
1849.724660	71.348835	63.042740
1849.240879	69.198942	63.047745
1848.765708	68.996852	63.052750
1847.679503	72.581961	63.057754
1846.905590	68.390193	63.062759
1845.905947	76.394501	63.067764
1846.044449	69.036323	63.072769
1845.028705	67.713666	63.077774
1844.620488	69.156793	63.082778
1844.622855	61.924317	63.087783
1843.693589	63.265671	63.092788
1842.773824	63.339189	63.097793
1842.045259	76.681169	63.102798
1841.382760	74.255295	63.107802
1841.215039	65.501213	63.112807
1839.675486	72.703404	63.117812
1839.112577	67.438891	63.122817
1838.467443	66.833271	63.127822
1837.943445	68.206472	63.132826
1837.591486	71.889465	63.137831
1836.754643	71.307979	63.142836
1836.312122	53.555038	63.147841
1834.995447	73.553862	63.152846
1834.233691	72.282345	63.157850
1834.081009	65.115490	63.162855
1832.991714	77.921804	63.167860
1832.814945	64.778797	63.172865
1832.395217	69.972276	63.177870
1832.004766	70.160448	63.182874
1830.793867	69.237804	63.187879
1830.039014	76.279125	63.192884
1829.561239	68.875301	63.197889
1828.994478	64.511870	63.202894
1827.751108	64.108485	63.207898
1827.588382	63.426264	63.212903
1826.646188	63.285722	63.217908
1826.281008	58.309948	63.222913
1825.890594	55.968613	63.227918
1824.632648	69.571276	63.232922
1823.786939	69.420145	63.237927
1823.041108	77.836755	63.242932
1823.053990	65.289702	63.247937
1822.386208	68.502439	63.252942
1822.028211	63.902426	63.257946
1820.993075	67.857914	63.262951
1819.630715	73.595333	63.267956
1819.347326	64.011199	63.272961
1818.995902	71.947271	63.277966
1818.411993	71.144270	63.282970
1818.318272	66.478635	63.287975
1816.803298	65.534897	63.292980
1816.194105	64.958269	63.297985
1815.705312	68.073196	63.302990
1814.942166	65.939288	63.307994
1813.820677	64.037331	63.312999
1812.727735	72.605258	63.318004
1812.568260	63.900337	63.323009
1812.225525	63.691415	63.328014
1811.703288	63.165637	63.333018
1811.193328	62.778261	63.338023
1810.596823	77.360873	63.343028
1810.444211	66.379252	63.348033
1809.295709	72.360266	63.353038
1808.190010	62.837331	63.358042
1807.956772	61.609629	63.363047
1806.686858	67.351295	63.368052
1805.854331	69.243442	63.373057
1805.334218	69.281893	63.378062
1804.650089	68.658818	63.383066
1804.525779	64.141550	63.388071
1803.780222	67.295676	63.393076
1803.562086	61.307778	63.398081
1802.652253	64.828623	63.403086
1801.634147	67.545048	63.408090
1801.501963	61.223370	63.413095
1800.692088	66.308493	63.418100
1799.529275	57.245658	63.423105
1798.842170	61.174269	63.428110
1798.076318	57.030127	63.433114
1798.002923	52.810714	63.438119
1797.509278	62.745343	63.443124
1796.664447	57.132944	63.448129
1795.900969	59.402068	63.453134
1795.196056	60.988515	63.458138
1795.018126	50.927165	63.463143
1793.467677	69.135383	63.468148
1792.870356	58.836269	63.473153
1792.025600	51.902340	63.478158
1791.674459	57.012385	63.483162
1791.604704	46.033395	63.488167
1790.946375	59.495103	63.493172
1789.945175	60.450496	63.498177
1789.019498	56.885265	63.503182
1788.310884	60.383620	63.508186
1788.016805	53.354354	63.513191
1787.248424	64.994769	63.518196
1786.343812	59.510142	63.523201
1785.558266	64.701794	63.528206
1784.708783	63.747007	63.533210
1784.736068	58.723106	63.538215
1784.023794	69.047285	63.543220
1783.898336	61.925003	63.548225
1782.640231	66.952001	63.553230
1781.666113	65.047156	63.558234
1781.464090	58.424327	63.563239
1780.657635	65.365036	63.568244
1780.346581	69.093578	63.573249
1779.342362	67.242401	63.578254
1778.335135	66.836231	63.583258
1778.185677	56.749857	63.588263
1777.382748	59.624510	63.593268
1776.372507	66.927176	63.598273
1775.584498	55.951860	63.603278
1774.872920	65.914796	63.608282
1774.904662	58.505769	63.613287
1774.013915	62.725355	63.618292
1773.833324	56.736230	63.623297
1772.728469	61.332028	63.628302
1772.102720	61.772048	63.633306
1771.694506	46.664621	63.638311
1770.915679	61.774505	63.643316
1770.100368	56.624220	63.648321
1769.262209	59.876641	63.653326
1768.413748	51.274849	63.658330
1768.325433	52.203542	63.663335
1767.351817	58.426457	63.668340
1766.885241	54.974407	63.673345
1765.719341	59.119419	63.678350
1765.104609	61.016412	63.683354
1764.559023	52.423290	63.688359
1763.952323	55.269935	63.693364
1763.953216	62.758955	63.698369
1763.047221	59.592742	63.703374
1761.711349	59.109460	63.708378
1761.276772	54.647783	63.713383
1760.933989	64.061702	63.718388
1760.522504	50.213237	63.723393
1759.484460	56.742861	63.728398
1758.313314	60.186946	63.733402
1758.284681	53.728978	63.738407
1757.536301	56.525585	63.743412
1757.462445	54.285377	63.748417
1756.423635	53.893694	63.753422
1755.315328	62.673814	63.758426
1754.549694	64.168987	63.763431
1754.089740	60.734811	63.768436
1753.968575	59.009908	63.773441
1752.869001	52.712570	63.778446
1751.639619	59.573792	63.783450
1751.485703	56.286559	63.788455
1750.903507	58.919575	63.793460
1750.678598	48.334248	63.798465
1749.882042	56.766801	63.803470
1748.653562	61.051073	63.808474
1748.381762	57.221152	63.813479
1747.688368	57.310790	63.818484
1746.743093	55.136444	63.823489
1746.142110	48.185896	63.828494
1745.256235	60.896830	63.833498
1745.217179	53.380778	63.838503
1744.453170	59.986736	63.843508
1743.872832	52.980866	63.848513
1742.849231	49.044845	63.853518
1742.211810	56.129026	63.858522
1741.699486	55.324137	63.863527
1741.202489	58.765237	63.868532
1740.395078	51.262410	63.873537
1739.393754	60.426099	63.878542
1738.678082	61.254157	63.883546
1738.242631	55.102085	63.888551
1737.726109	55.685619	63.893556
1737.400116	57.221358	63.898561
1736.309701	57.837694	63.903566
1735.628950	61.954550	63.908570
1735.106430	56.035510	63.913575
1734.730837	57.828293	63.918580
1733.990039	52.443831	63.923585
1733.229074	51.405615	63.928590
1732.265244	56.266040	63.933594
1731.972960	52.310063	63.938599
1730.988165	60.860832	63.943604
1730.225365	53.888677	63.948609
1729.731248	54.897596	63.953614
1729.016875	64.441502	63.958618
1728.529222	51.292713	63.963623
1728.363517	62.160880	63.968628
1727.071427	47.632259	63.973633
1726.444574	58.781833	63.978638
1725.389913	57.154739	63.983642
1724.958170	59.177221	63.988647
1724.415418	55.261027	63.993652
1724.171050	51.754769	63.998657
1723.068433	63.520823	64.003662
1722.115285	53.546344	64.008666
1722.039558	54.168680	64.013671
1721.228823	59.356462	64.018676
1720.707459	53.014609	64.023681
1720.011301	50.004323	64.028686
1718.857293	55.427983	64.033690
1718.525462	51.517714	64.038695
1717.814694	66.916429	64.043700
1717.263339	52.358466	64.048705
1716.399156	53.689525	64.053710
1715.354430	62.085811	64.058714
1715.300539	53.969707	64.063719
1714.829722	54.077617	64.068724
1714.482902	51.674183	64.073729
1713.317234	57.979660	64.078734
1712.225607	61.955197	64.083738
1711.939789	48.264988	64.088743
1711.397249	59.703955	64.093748
1710.735047	52.121302	64.098753
1709.811734	56.355540	64.103758
1708.688242	59.350518	64.108762
1708.454127	50.958682	64.113767
1707.769688	58.990227	64.118772
1707.876944	56.968841	64.123777
1707.622482	53.197676	64.128782
1705.987091	59.853742	64.133786
1705.254891	54.772283	64.138791
1704.667005	52.579034	64.143796
1703.541396	56.969989	64.148801
1702.962416	57.519294	64.153806
1702.140003	64.960886	64.158810
1701.923078	53.007043	64.163815
1701.541133	57.689891	64.168820
1701.301627	59.981471	64.173825
1700.541328	50.706520	64.178830
1699.478823	56.883648	64.183834
1699.071199	53.680876	64.188839
1697.988971	57.309563	64.193844
1696.830077	52.928260	64.198849
1696.645452	65.680787	64.203854
1695.896655	64.602801	64.208858
1696.135052	51.699826	64.213863
1695.177467	58.081069	64.218868
1694.045245	50.139411	64.223873
1693.126998	56.219508	64.228878
1692.650862	56.385040	64.233882
1692.651009	55.014619	64.238887
1691.535946	61.040825	64.243892
1690.697776	54.392902	64.248897
1690.370527	46.758630	64.253902
1689.400180	59.430952	64.258906
1689.255473	56.643745	64.263911
1687.669016	57.485557	64.268916
1687.061139	46.380744	64.273921
1686.676571	47.608818	64.278926
1686.087314	52.600571	64.283930
1686.209406	56.779145	64.288935
1684.664369	59.809554	64.293940
1684.061326	52.006197	64.298945
1683.480528	58.548371	64.303950
1682.983941	62.295352	64.308954
1682.788247	46.294733	64.313959
1681.755095	55.616459	64.318964
1680.879857	53.429436	64.323969
1680.426059	51.634373	64.328974
1679.623482	59.164282	64.333978
1678.558303	47.788330	64.338983
1677.696644	62.493482	64.343988
1677.315812	63.090167	64.348993
1677.054554	45.365271	64.353998
1676.674539	59.077678	64.359002
1676.057788	52.754143	64.364007
1674.879862	52.520214	64.369012
1673.890081	58.606950	64.374017
1673.733056	53.293781	64.379022
1672.903923	53.699899	64.384026
1672.511549	54.334689	64.389031
1671.512058	58.311374	64.394036
1671.015000	52.227454	64.399041
1670.790633	57.236943	64.404046
1669.632349	64.742936	64.409050
1668.788003	56.414926	64.414055
1668.020048	59.626261	64.419060
1667.513167	53.469783	64.424065
1667.549007	47.932010	64.429070
1666.538830	55.674675	64.434074
1665.910599	54.957602	64.439079
1664.993389	58.489122	64.444084
1664.313620	52.268645	64.449089
1663.794805	54.232426	64.454094
1662.781738	55.787432	64.459098
1662.166051	49.813826	64.464103
1661.749411	54.194676	64.469108
1661.014704	57.619932	64.474113
1660.782004	52.195782	64.479118
1660.126108	45.395914	64.484122
1659.113265	49.768970	64.489127
1658.225337	54.541664	64.494132
1658.048967	49.868678	64.499137
1657.550491	44.756417	64.504142
1655.920393	51.113615	64.509146
1655.661326	51.340866	64.514151
1654.983149	50.262714	64.519156
1654.523616	44.802060	64.524161
1654.094014	42.030155	64.529166
1653.248631	47.266033	64.534170
1652.786796	47.798317	64.539175
1652.019487	46.417350	64.544180
1651.466941	55.263755	64.549185
1650.326355	43.674291	64.554190
1649.151490	51.599244	64.559194
1649.120918	43.749114	64.564199
1648.702884	49.051148	64.569204
1648.221371	47.605856	64.574209
1647.185320	46.721757	64.579214
1646.183215	51.183001	64.584218
1645.793443	42.371198	64.589223
1645.275101	43.095390	64.594228
1645.123360	52.904743	64.599233
1644.322897	48.797695	64.604238
1643.200423	51.022963	64.609242
1642.590437	48.391683	64.614247
1642.086035	54.834990	64.619252
1641.120650	51.120004	64.624257
1640.698736	50.483704	64.629262
1640.093174	51.768970	64.634266
1639.690650	49.205659	64.639271
1638.840491	54.319297	64.644276
1637.601500	65.357971	64.649281
1637.007151	53.416792	64.654286
1636.474649	54.434980	64.659290
1636.571640	49.174505	64.664295
1635.241723	57.661854	64.669300
1634.451449	61.901789	64.674305
1634.056526	54.707219	64.679310
1633.153865	59.580036	64.684314
1633.058614	54.925703	64.689319
1632.449317	58.799410	64.694324
1631.305029	53.050143	64.699329
1630.960618	42.936427	64.704334
1629.875765	59.424349	64.709338
1628.883191	52.744210	64.714343
1628.050170	52.572204	64.719348
1627.862322	57.238416	64.724353
1627.519782	51.163077	64.729358
1626.843583	56.020417	64.734362
1626.820460	51.862419	64.739367
1625.495580	59.092109	64.744372
1624.741147	54.015787	64.749377
1624.574611	46.980485	64.754382
1623.547674	49.386130	64.759386
1622.679535	49.454677	64.764391
1621.771324	46.629503	64.769396
1621.124263	56.651595	64.774401
1620.938507	44.440505	64.779406
1620.461042	56.960416	64.784410
1619.688967	50.589035	64.789415
1619.156710	55.074993	64.794420
1618.479679	56.887295	64.799425
1617.702713	51.082832	64.804430
1616.513705	58.385559	64.809434
1616.071249	45.325830	64.814439
1615.781489	55.370005	64.819444
1614.910689	55.175619	64.824449
1614.078749	42.261353	64.829454
1613.113516	58.559959	64.834458
1612.740506	50.059318	64.839463
1612.171869	51.083251	64.844468
1611.733556	52.971171	64.849473
1611.127583	51.946216	64.854478
1609.909891	54.771691	64.859482
1609.869378	51.395490	64.864487
1608.857200	49.684424	64.869492
1608.538277	53.420535	64.874497
1607.504119	50.727342	64.879502
1606.538742	50.472290	64.884506
1606.035203	44.572351	64.889511
1605.477693	46.860841	64.894516
1605.295517	46.719481	64.899521
1604.885617	45.500945	64.904526
1603.460853	52.213489	64.909530
1603.022709	46.400933	64.914535
1602.524906	47.419922	64.919540
1601.754897	46.796356	64.924545
1600.649649	45.251472	64.929550
1600.071675	57.375759	64.934554
1599.750002	44.106029	64.939559
1599.310094	47.844014	64.944564
1598.433378	47.410872	64.949569
1597.668716	43.083682	64.954574
1596.703743	47.928559	64.959578
1596.307460	44.200445	64.964583
1596.028373	46.862603	64.969588
1594.871194	47.366600	64.974593
1594.645718	44.257915	64.979598
1593.934076	54.411698	64.984602
1593.595270	41.554712	64.989607
1592.630484	52.395281	64.994612
1591.820902	50.076431	64.999617
1591.103356	46.124966	65.004622
1590.406027	45.843101	65.009626
1589.366655	49.999617	65.014631
1588.801881	48.427214	65.019636
1588.294299	53.114264	65.024641
1588.060981	46.936423	65.029646
1587.572707	50.432931	65.034650
1586.851055	48.992689	65.039655
1586.004636	47.042402	65.044660
1585.183250	52.066324	65.049665
1584.311441	44.952272	65.054670
1583.047716	58.010285	65.059674
1582.958398	46.911428	65.064679
1582.518156	49.362644	65.069684
1582.007901	56.262640	65.074689
1581.968555	49.260752	65.079694
1580.562360	57.487423	65.084698
1579.675422	54.010740	65.089703
1579.310606	47.568358	65.094708
1578.680851	57.221844	65.099713
1577.908733	55.622462	65.104718
1576.799272	61.362383	65.109722
1576.399518	44.271398	65.114727
1576.139666	49.023168	65.119732
1575.262639	53.016697	65.124737
1574.740253	50.901384	65.129742
1573.470211	59.316167	65.134746
1573.248096	60.518444	65.139751
1572.781950	56.126480	65.144756
1572.409037	51.380651	65.149761
1571.436114	51.694528	65.154766
1570.242538	53.404409	65.159770
1570.139907	48.773334	65.164775
1569.627509	50.256706	65.169780
1568.446807	51.811574	65.174785
1567.710350	45.518135	65.179790
1567.196918	52.322439	65.184794
1566.851560	45.750810	65.189799
1566.301425	48.317263	65.194804
1565.012717	47.098020	65.199809
1564.434237	50.227233	65.204814
1563.830147	47.899396	65.209818
1563.621176	42.301178	65.214823
1563.197500	52.161621	65.219828
1561.817734	46.806209	65.224833
1561.150631	41.466872	65.229838
1560.381955	55.368768	65.234842
1560.226770	44.966373	65.239847
1559.752078	52.340124	65.244852
1558.582736	50.520007	65.249857
1558.036823	54.219649	65.254862
1557.234050	48.739439	65.259866
1556.836345	40.474559	65.264871
1556.219432	55.754284	65.269876
1555.077230	46.521154	65.274881
1554.762601	48.294809	65.279886
1554.029639	44.918253	65.284890
1553.680424	39.875345	65.289895
1553.210818	48.926204	65.294900
1551.731021	41.922969	65.299905
1551.719406	54.635369	65.304910
1551.066903	50.312449	65.309914
1549.820510	50.018491	65.314919
1549.293664	47.943318	65.319924
1548.286480	52.405403	65.324929
1548.059065	37.384448	65.329934
1547.480482	52.618656	65.334938
1547.389396	47.976287	65.339943
1546.472205	48.259239	65.344948
1545.719179	49.164249	65.349953
1545.044575	50.317000	65.354958
1544.410024	53.748448	65.359962
1543.693170	55.966075	65.364967
1542.999793	56.902609	65.369972
1542.619044	58.538536	65.374977
1541.759549	46.876079	65.379982
1540.244069	52.978580	65.384986
1540.250949	51.381582	65.389991
1539.740830	55.184352	65.394996
1539.163513	52.967386	65.400001
1538.183900	38.826071	65.405006
1537.255436	58.772733	65.410010
1536.630020	50.908322	65.415015
1536.307868	49.805167	65.420020
1535.788923	58.274079	65.425025
1535.246603	46.688960	65.430030
1534.336668	51.679657	65.435034
1533.651735	47.994269	65.440039
1533.055690	50.503368	65.445044
1531.967670	61.057605	65.450049
1531.351483	50.465111	65.455054
1530.601398	55.759999	65.460058
1530.449086	52.275409	65.465063
1529.960375	48.003741	65.470068
1529.436045	48.460819	65.475073
1528.746314	47.094371	65.480078
1527.754924	49.035499	65.485082
1526.937765	53.145688	65.490087
1525.672536	55.530888	65.495092
1524.924326	50.551386	65.500097
1524.953611	49.911216	65.505102
1524.512870	51.518831	65.510106
1524.079118	54.380620	65.515111
1523.780510	50.058242	65.520116
1522.274585	52.565273	65.525121
1521.818933	54.963753	65.530126
1521.267005	43.056885	65.535130
1520.498941	47.627639	65.540135
1519.559355	53.435202	65.545140
1518.614932	49.128719	65.550145
1518.396286	38.346905	65.555150
1517.350193	55.970431	65.560154
1517.416713	43.161019	65.565159
1517.042250	49.086938	65.570164
1515.739095	57.341421	65.575169
1515.552228	47.029225	65.580174
1514.616624	55.576966	65.585178
1513.245070	51.578065	65.590183
1512.778148	49.904971	65.595188
1512.130594	58.919461	65.600193
1511.953417	43.904719	65.605198
1511.545436	61.374806	65.610202
1511.123756	49.120801	65.615207
1509.967454	52.452239	65.620212
1508.946165	56.268436	65.625217
1508.859620	51.015052	65.630222
1507.816029	61.212145	65.635226
1506.916914	51.319072	65.640231
1506.575153	55.724311	65.645236
1505.901215	61.756177	65.650241
1505.590017	56.002316	65.655246
1504.433219	54.544516	65.660250
1503.700057	55.600926	65.665255
1503.306449	59.429342	65.670260
1502.372154	51.158278	65.675265
1502.557821	44.144296	65.680270
1501.359824	59.655150	65.685274
1500.589544	42.817046	65.690279
1500.050047	60.809515	65.695284
1499.338938	62.759730	65.700289
1498.510757	53.279598	65.705294
1497.600940	64.676026	65.710298
1497.319437	55.709848	65.715303
1497.076208	57.298694	65.720308
1496.201650	60.153269	65.725313
1495.486125	57.608186	65.730318
1494.734000	50.699081	65.735322
1494.480769	53.119013	65.740327
1493.253945	57.571867	65.745332
1492.211760	60.202342	65.750337
1492.006634	58.287368	65.755342
1491.497212	60.669167	65.760346
1490.787685	53.433163	65.765351
1490.117796	56.557994	65.770356
1489.314260	61.538106	65.775361
1488.822421	47.887006	65.780366
1488.183412	57.825834	65.785370
1487.342873	56.576407	65.790375
1486.397907	55.285227	65.795380
1485.861708	62.752346	65.800385
1485.775172	54.392290	65.805390
1485.067416	58.847813	65.810394
1483.948708	59.124966	65.815399
1483.303114	52.903848	65.820404
1482.656728	58.478742	65.825409
1482.460686	55.283387	65.830414
1481.301086	57.107760	65.835418
1480.605075	48.786221	65.840423
1479.873745	53.482038	65.845428
1479.345463	60.206713	65.850433
1479.238365	51.230171	65.855438
1478.389483	50.862033	65.860442
1477.508153	59.166189	65.865447
1476.927571	56.046142	65.870452
1476.390345	53.285067	65.875457
1475.632801	52.247963	65.880462
1474.301492	54.508068	65.885466
1473.989222	57.960852	65.890471
1473.533325	59.093056	65.895476
1472.924136	57.597126	65.900481
1472.683333	51.836816	65.905486
1471.573811	54.541078	65.910490
1470.844556	50.555240	65.915495
1470.597992	55.397948	65.920500
1469.731334	54.004441	65.925505
1468.842262	45.459697	65.930510
1467.917700	52.067575	65.935514
1467.623612	45.438931	65.940519
1467.245323	41.780525	65.945524
1465.857465	46.355178	65.950529
1465.525246	40.188347	65.955534
1464.741179	52.635562	65.960538
1464.397281	48.593212	65.965543
1464.111305	50.242472	65.970548
1462.801734	46.517608	65.975553
1462.084079	44.338737	65.980558
1461.784160	55.283410	65.985562
1461.197079	50.894924	65.990567
1460.245846	44.410151	65.995572
1459.199332	55.834615	66.000577
1458.871715	45.833390	66.005582
1458.465470	54.666027	66.010586
1457.927139	53.683976	66.015591
1457.348600	51.328450	66.020596
1456.279697	51.851594	66.025601
1455.855532	40.501623	66.030606
1454.926549	47.704730	66.035610
1454.534394	42.058370	66.040615
1453.702866	46.768540	66.045620
1452.877893	49.651515	66.050625
1452.533880	45.203900	66.055630
1451.973749	51.121488	66.060634
1450.894493	54.934302	66.065639
1450.502560	48.967777	66.070644
1449.805855	54.386667	66.075649
1449.596493	49.636945	66.080654
1448.274814	56.984477	66.085658
1447.697556	46.518295	66.090663
1447.466620	50.790803	66.095668
1446.614942	62.420857	66.100673
1445.597929	51.098874	66.105678
1445.023757	55.284009	66.110682
1444.331249	55.629059	66.115687
1444.113616	54.703274	66.120692
1442.924999	55.493039	66.125697
1442.337621	54.786875	66.130702
1441.469576	56.377262	66.135706
1441.236781	58.499054	66.140711
1440.877295	55.734968	66.145716
1440.245059	60.717828	66.150721
1439.013912	54.984041	66.155726
1438.541625	56.202436	66.160730
1438.006622	54.030811	66.165735
1437.524191	57.543761	66.170740
1436.191004	58.203539	66.175745
1435.820079	52.859741	66.180750
1435.326226	54.379615	66.185754
1434.729229	53.345391	66.190759
1434.135367	50.057153	66.195764
1432.644428	58.075006	66.200769
1432.418234	52.083717	66.205774
1432.042929	58.374065	66.210778
1431.478955	50.304376	66.215783
1430.415136	54.007509	66.220788
1429.298611	59.723375	66.225793
1429.012602	54.678325	66.230798
1428.766506	56.426908	66.235802
1428.506315	58.357508	66.240807
1427.850759	53.287617	66.245812
1426.505995	46.710863	66.250817
1426.159458	59.265169	66.255822
1425.759581	56.720399	66.260826
1424.786649	58.559281	66.265831
1424.094229	47.709279	66.270836
1423.539442	59.400956	66.275841
1422.443167	50.709388	66.280846
1421.406433	62.058195	66.285850
1420.399497	49.444647	66.290855
1420.323409	52.722696	66.295860
1419.409978	59.756185	66.300865
1419.392813	46.004429	66.305870
1419.355593	54.543440	66.310874
1418.943103	54.320427	66.315879
1417.959270	46.590301	66.320884
1417.073595	47.715132	66.325889
1416.162878	53.160161	66.330894
1415.156212	47.045348	66.335898
1414.366390	51.811979	66.340903
1414.178863	50.805717	66.345908
1413.522318	55.429737	66.350913
1412.747541	51.118409	66.355918
1411.775888	59.873765	66.360922
1411.079768	57.839722	66.365927
1410.893939	48.661235	66.370932
1410.308577	54.442488	66.375937
1410.245962	54.752080	66.380942
1408.885565	56.546898	66.385946
1408.287176	58.412985	66.390951
1407.489423	56.571721	66.395956
1406.222161	54.921786	66.400961
1405.964445	52.540507	66.405966
1405.140486	52.438098	66.410970
1404.770819	53.406792	66.415975
1404.900126	47.527737	66.420980
1403.819592	51.325002	66.425985
1403.002355	46.037965	66.430990
1402.270608	54.458712	66.435994
1401.569846	53.923549	66.440999
1401.134851	49.892536	66.446004
1400.301770	59.292934	66.451009
1399.899638	45.329556	66.456014
1398.567866	57.456987	66.461018
1398.078351	55.090478	66.466023
1397.771389	51.375012	66.471028
1396.911239	56.983902	66.476033
1396.655257	49.510254	66.481038
1395.448909	46.628477	66.486042
1394.799385	59.428069	66.491047
1394.314845	58.885346	66.496052
1393.740248	52.816978	66.501057
1393.504308	44.874936	66.506062
1392.339591	51.812753	66.511066
1391.777756	54.442602	66.516071
1391.271874	55.115976	66.521076
1389.793758	54.344833	66.526081
1388.998324	55.997813	66.531086
1388.892433	55.886921	66.536090
1388.282407	51.850617	66.541095
1388.029368	52.395488	66.546100
1387.498894	61.083874	66.551105
1386.375407	55.440236	66.556110
1385.565498	63.487054	66.561114
1385.109992	56.360520	66.566119
1384.472820	56.118035	66.571124
1383.343093	64.947417	66.576129
1382.701922	50.228813	66.581134
1382.173765	55.436416	66.586138
1381.849829	57.566393	66.591143
1381.546459	53.443495	66.596148
1380.339481	55.447333	66.601153
1379.773325	49.128465	66.606158
1379.465506	55.488514	66.611162
1378.564200	51.396013	66.616167
1377.657038	56.807373	66.621172
1377.001135	56.356551	66.626177
1376.453359	57.700500	66.631182
1376.147144	56.659490	66.636186
1374.742356	52.736916	66.641191
1374.448905	45.437968	66.646196
1373.471747	56.080285	66.651201
1373.482326	54.471663	66.656206
1372.709169	55.507658	66.661210
1371.563005	50.780710	66.666215
1371.207177	53.950261	66.671220
1370.200635	58.715087	66.676225
1370.253090	56.541554	66.681230
1369.240728	53.949079	66.686234
1368.420292	55.055671	66.691239
1368.077065	47.237923	66.696244
1367.352604	68.547825	66.701249
1366.484647	58.246149	66.706254
1365.429713	62.296411	66.711258
1365.300306	57.376289	66.716263
1364.803610	54.857961	66.721268
1363.942354	61.198760	66.726273
1362.981253	55.090916	66.731278
1362.522843	58.700986	66.736282
1361.957618	61.664125	66.741287
1361.716492	61.038556	66.746292
1360.532094	62.702917	66.751297
1359.761719	53.406047	66.756302
1359.122912	54.568924	66.761306
1358.623100	57.427045	66.766311
1358.548741	51.285470	66.771316
1357.245877	52.569687	66.776321
1356.712254	45.657438	66.781326
1356.192637	43.674203	66.786330
1355.504611	54.070280	66.791335
1354.543160	49.824921	66.796340
1353.605020	66.297477	66.801345
1353.113234	56.401219	66.806350
1352.861620	59.240384	66.811354
1352.277999	54.028190	66.816359
1351.078672	54.154210	66.821364
1350.212729	60.251324	66.826369
1350.131587	50.076894	66.831374
1349.461072	59.506653	66.836378
1348.583746	48.004817	66.841383
1347.878949	56.476486	66.846388
1347.127937	59.652095	66.851393
1346.791168	58.314741	66.856398
1346.422011	60.608032	66.861402
1345.415484	60.637170	66.866407
1344.632788	48.967324	66.871412
1344.027543	56.027533	66.876417
1343.789472	53.933305	66.881422
1343.106514	51.759992	66.886426
1341.847010	51.053472	66.891431
1341.082340	53.808620	66.896436
1340.558437	59.028171	66.901441
1340.716896	59.936566	66.906446
1339.599239	54.113826	66.911450
1338.677459	58.395245	66.916455
1338.442809	50.508199	66.921460
1337.415426	56.701945	66.926465
1336.494049	48.567680	66.931470
1335.907787	57.419484	66.936474
1335.108027	49.899832	66.941479
1335.213252	49.293320	66.946484
1334.441780	55.559925	66.951489
1333.894538	46.383717	66.956494
1333.174917	51.905624	66.961498
1332.218666	46.858338	66.966503
1331.963717	47.958617	66.971508
1330.473206	54.454659	66.976513
1330.085984	44.970731	66.981518
1329.818598	56.206705	66.986522
1328.846062	55.951319	66.991527
1328.074827	48.840306	66.996532
1327.077667	46.078273	67.001537
1326.875457	51.932667	67.006542
1326.412039	62.061228	67.011546
1325.832958	63.829643	67.016551
1324.859832	55.795072	67.021556
1323.825238	56.257621	67.026561
1323.528205	55.792336	67.031566
1323.110250	52.447773	67.036570
1322.634815	52.794614	67.041575
1321.753897	55.702294	67.046580
1320.680700	52.450869	67.051585
1320.312365	51.112231	67.056590
1319.750254	53.967647	67.061594
1318.669218	52.035831	67.066599
1318.033548	53.704432	67.071604
1317.341821	51.936229	67.076609
1317.197244	54.509214	67.081614
1316.596774	53.888742	67.086618
1315.827983	59.981458	67.091623
1315.052607	50.540320	67.096628
1314.464569	56.613758	67.101633
1313.988844	46.864778	67.106638
1312.989673	51.655259	67.111642
1312.186926	51.968985	67.116647
1311.514029	52.208448	67.121652
1311.046291	55.266485	67.126657
1310.641517	46.942861	67.131662
1310.226088	48.540175	67.136666
1308.973766	42.374583	67.141671
1308.511326	47.995955	67.146676
1307.750691	53.622162	67.151681
1307.181251	55.833758	67.156686
1306.477997	61.031367	67.161690
1305.774574	54.666532	67.166695
1305.413667	53.955932	67.171700
1304.498689	55.735179	67.176705
1303.606712	43.831989	67.181710
1303.174020	59.170756	67.186714
1303.008394	56.942009	67.191719
1301.763574	50.705836	67.196724
1301.015723	62.530727	67.201729
1300.315281	61.024117	67.206734
1300.284611	57.811950	67.211738
1299.100202	61.513807	67.216743
1298.332275	52.751172	67.221748
1297.453985	57.505092	67.226753
1297.220492	56.061438	67.231758
1296.812619	48.760196	67.236762
1295.705414	62.474683	67.241767
1295.262541	45.982019	67.246772
1294.281277	58.064798	67.251777
1293.944211	57.367757	67.256782
1293.739412	63.482770	67.261786
1292.398902	64.214752	67.266791
1292.014506	57.453834	67.271796
1291.021303	62.770090	67.276801
1290.969063	64.863185	67.281806
1289.726030	62.925598	67.286810
1288.709092	65.026999	67.291815
1288.499473	56.677075	67.296820
1287.941491	60.310873	67.301825
1287.756252	62.936058	67.306830
1286.565813	61.622483	67.311834
1285.641816	54.851170	67.316839
1285.637565	53.926165	67.321844
1284.779911	52.422480	67.326849
1284.192872	56.549764	67.331854
1283.226321	61.388688	67.336858
1282.391281	56.132909	67.341863
1282.423937	55.287193	67.346868
1281.608743	55.434171	67.351873
1280.496611	53.149340	67.356878
1279.718411	60.727505	67.361882
1279.285325	59.971614	67.366887
1278.973878	54.733510	67.371892
1278.028946	58.602305	67.376897
1277.057956	51.565652	67.381902
1276.194933	62.008496	67.386906
1276.120219	57.097034	67.391911
1276.052831	53.528000	67.396916
1275.056191	52.399663	67.401921
1274.074876	49.215654	67.406926
1273.844734	47.107559	67.411930
1272.508999	58.311555	67.416935
1271.699740	51.419502	67.421940
1271.048496	59.583043	67.426945
1270.826872	50.176877	67.431950
1270.750234	43.206182	67.436954
1269.570373	48.481157	67.441959
1268.764611	50.003346	67.446964
1268.007532	53.673535	67.451969
1267.479220	55.403927	67.456974
1267.033971	50.114561	67.461978
1265.967161	52.747458	67.466983
1265.423414	46.145934	67.471988
1264.546266	56.322936	67.476993
1264.563072	48.380150	67.481998
1263.722359	50.642774	67.487002
1262.673905	61.583472	67.492007
1262.313365	46.798220	67.497012
1261.759659	57.795865	67.502017
1261.114684	50.931310	67.507022
1260.473760	47.888727	67.512026
1259.318776	55.414841	67.517031
1259.206442	49.659369	67.522036
1257.844845	57.953215	67.527041
1257.221812	51.463649	67.532046
1256.705576	49.888336	67.537050
1256.208128	47.844826	67.542055
1256.130972	47.272044	67.547060
1255.100841	50.443172	67.552065
1254.242600	52.598198	67.557070
1253.824832	52.391822	67.562074
1252.869799	53.778478	67.567079
1252.013019	56.851078	67.572084
1251.295055	52.401459	67.577089
1250.968357	49.214292	67.582094
1250.674915	46.029723	67.587098
1249.758531	60.428251	67.592103
1249.039286	53.581817	67.597108
1248.121824	52.212237	67.602113
1247.728217	53.993753	67.607118
1247.266793	46.559111	67.612122
1246.048396	48.310931	67.617127
1245.288089	46.481114	67.622132
1244.843641	64.344932	67.627137
1244.527816	51.549036	67.632142
1244.157809	52.421609	67.637146
1243.064848	49.528185	67.642151
1242.622524	50.500570	67.647156
1242.136151	49.791008	67.652161
1241.175336	48.860419	67.657166
1240.479699	47.367256	67.662170
1239.563787	56.795052	67.667175
1239.303155	49.964006	67.672180
1238.279834	51.710040	67.677185
1237.592928	47.583502	67.682190
1236.920122	52.576003	67.687194
1236.540010	54.484687	67.692199
1236.479711	46.424853	67.697204
1234.914120	51.259701	67.702209
1234.103329	53.236873	67.707214
1234.148359	52.909595	67.712218
1232.959848	53.713631	67.717223
1232.182707	56.347787	67.722228
1231.278751	56.450547	67.727233
1230.934255	56.041707	67.732238
1230.675115	48.218501	67.737242
1230.063639	53.013591	67.742247
1229.420347	41.954003	67.747252
1228.270812	52.801966	67.752257
1227.766269	54.195841	67.757262
1227.395643	52.343485	67.762266
1226.506987	51.078144	67.767271
1225.844538	47.922297	67.772276
1224.877738	56.850400	67.777281
1224.640339	62.128488	67.782286
1224.402174	46.798650	67.787290
1223.007015	56.070847	67.792295
1222.469634	46.919914	67.797300
1221.836541	49.692017	67.802305
1221.461949	55.114924	67.807310
1220.374408	47.385613	67.812314
1219.327445	52.819250	67.817319
1219.185868	41.667263	67.822324
1218.430650	59.090054	67.827329
1218.380692	48.436012	67.832334
1217.778571	37.270535	67.837338
1216.613578	56.756527	67.842343
1216.307066	36.167288	67.847348
1215.504429	45.231709	67.852353
1214.498130	54.410528	67.857358
1213.737588	43.243432	67.862362
1213.205890	56.008534	67.867367
1213.208391	43.613047	67.872372
1211.950715	48.730105	67.877377
1211.039617	47.411568	67.882382
1210.851335	45.470291	67.887386
1210.164155	58.130808	67.892391
1209.638244	43.490149	67.897396
1208.475653	58.194349	67.902401
1207.969465	46.018534	67.907406
1207.647551	54.393065	67.912410
1206.489445	55.485597	67.917415
1205.826433	45.862630	67.922420
1205.127477	49.039457	67.927425
1204.808743	50.739683	67.932430
1204.473601	46.207122	67.937434
1203.630021	50.867237	67.942439
1203.229839	50.360022	67.947444
1202.296503	49.240571	67.952449
1201.358913	45.248531	67.957454
1200.596105	56.277858	67.962458
1199.356154	56.473490	67.967463
1199.245049	46.444201	67.972468
1198.388717	53.683138	67.977473
1198.255169	50.299678	67.982478
1197.819079	51.987030	67.987482
1196.830693	51.004071	67.992487
1196.214903	50.740886	67.997492
1195.916887	50.307312	68.002497
1194.943599	43.256873	68.007502
1194.244639	47.143345	68.012506
1193.627710	51.732723	68.017511
1193.001863	47.452982	68.022516
1191.915863	53.889492	68.027521
1191.266343	46.316042	68.032526
1191.003313	42.633049	68.037530
1190.340393	53.501408	68.042535
1189.626564	47.617675	68.047540
1188.137934	49.798860	68.052545
1187.642804	55.802348	68.057550
1187.322900	48.764691	68.062554
1186.662327	56.724720	68.067559
1186.601443	47.100616	68.072564
1186.103815	53.787334	68.077569
1184.992687	54.851904	68.082574
1184.464797	45.221649	68.087578
1183.749028	49.782592	68.092583
1183.409901	43.903925	68.097588
1182.291556	47.853946	68.102593
1181.727168	42.552012	68.107598
1180.652275	47.835559	68.112602
1179.741547	48.128652	68.117607
1179.362505	45.539614	68.122612
1178.546349	56.750899	68.127617
1177.931067	53.352592	68.132622
1177.986453	44.768155	68.137626
1177.614126	58.124514	68.142631
1176.545403	44.781322	68.147636
1175.466951	56.139981	68.152641
1175.144990	49.772872	68.157646
1174.709319	45.338309	68.162650
1173.455338	50.350716	68.167655
1173.198034	43.016097	68.172660
1172.645960	45.226534	68.177665
1171.756230	38.651682	68.182670
1170.780722	39.571682	68.187674
1170.208430	43.209350	68.192679
1169.794877	36.371104	68.197684
1169.497714	42.811466	68.202689
1168.575807	52.069917	68.207694
1168.258849	45.607396	68.212698
1167.441778	53.327385	68.217703
1166.210815	38.481911	68.222708
1165.493038	40.630392	68.227713
1164.808142	49.540480	68.232718
1164.704851	38.284643	68.237722
1163.630399	49.313075	68.242727
1162.913111	49.498135	68.247732
1162.143390	42.095206	68.252737
1161.537823	47.710975	68.257742
1161.572990	36.180801	68.262746
1160.467020	51.483140	68.267751
1159.777342	32.859865	68.272756
1158.865906	48.728937	68.277761
1158.129077	44.365933	68.282766
1158.323789	43.497596	68.287770
1157.411265	54.812522	68.292775
1156.619112	42.901411	68.297780
1155.804000	47.132801	68.302785
1155.458786	44.984674	68.307790
1154.839495	41.598053	68.312794
1153.490622	44.564443	68.317799
1153.124168	48.497388	68.322804
1152.532950	39.268312	68.327809
1152.015300	43.526508	68.332814
1150.867538	43.313253	68.337818
1150.022119	44.406539	68.342823
1149.719099	47.351665	68.347828
1149.492895	43.937215	68.352833
1149.170664	44.909437	68.357838
1148.493525	45.293123	68.362842
1147.457947	41.121147	68.367847
1146.516340	46.877101	68.372852
1145.515482	44.823799	68.377857
1144.599371	51.130798	68.382862
1144.744934	47.624099	68.387866
1143.914413	51.686054	68.392871
1143.698567	49.375422	68.397876
1143.033521	55.096853	68.402881
1141.755066	56.590187	68.407886
1141.162519	53.177235	68.412890
1140.627174	61.931080	68.417895
1140.582447	53.345218	68.422900
1139.591757	53.975903	68.427905
1138.586616	55.378455	68.432910
1137.950587	49.493403	68.437914
1137.172821	55.109760	68.442919
1136.375415	45.117105	68.447924
1135.699501	55.547561	68.452929
1135.493452	53.951321	68.457934
1135.445531	54.558208	68.462938
1133.800740	67.344254	68.467943
1132.987945	47.132032	68.472948
1132.765967	56.003190	68.477953
1132.164138	59.874229	68.482958
1131.957688	53.920847	68.487962
1130.782537	59.404870	68.492967
1130.115879	52.744084	68.497972
1129.603795	59.880975	68.502977
1128.675432	54.452440	68.507982
1127.991970	56.485085	68.512986
1127.053092	54.573321	68.517991
1126.748386	51.445755	68.522996
1126.225758	47.849796	68.528001
1125.674311	58.711474	68.533006
1125.055949	57.844731	68.538010
1124.012080	53.445417	68.543015
1123.858479	54.449168	68.548020
1123.075039	65.052858	68.553025
1122.217780	62.584051	68.558030
1121.819763	53.554483	68.563034
1120.877734	59.588067	68.568039
1120.110331	49.645837	68.573044
1119.481091	52.868366	68.578049
1119.150523	56.633179	68.583054
1118.652646	46.031479	68.588058
1117.295999	56.330520	68.593063
1116.770742	53.665401	68.598068
1116.217072	52.413047	68.603073
1115.407048	49.911500	68.608078
1114.766560	50.942236	68.613082
1113.582702	49.328072	68.618087
1113.412914	53.122503	68.623092
1113.191868	53.790046	68.628097
1112.601887	56.616818	68.633102
1111.839872	49.144869	68.638106
1110.575008	55.333888	68.643111
1110.712008	46.104102	68.648116
1110.010727	52.274435	68.653121
1108.928927	61.394335	68.658126
1108.362007	45.462377	68.663130
1107.477839	53.451678	68.668135
1107.119691	50.573895	68.673140
1106.139365	52.637998	68.678145
1105.243708	45.740833	68.683150
1104.985593	41.692789	68.688154
1104.278213	55.903550	68.693159
1104.018167	54.162936	68.698164
1102.966913	50.006087	68.703169
1102.165501	51.970767	68.708174
1102.049491	49.496022	68.713178
1101.232253	53.699382	68.718183
1100.459052	54.569880	68.723188
1099.727570	57.485397	68.728193
1099.026421	54.215891	68.733198
1098.870680	55.396605	68.738202
1097.393622	57.033519	68.743207
1096.757588	59.519108	68.748212
1096.361822	57.131443	68.753217
1095.687452	55.570282	68.758222
1095.367621	49.363703	68.763226
1094.057555	59.019821	68.768231
1093.708686	52.076678	68.773236
1092.882072	55.644431	68.778241
1092.587854	56.623243	68.783246
1092.181805	44.357420	68.788250
1091.042765	52.797285	68.793255
1090.554402	44.712523	68.798260
1090.206629	44.821474	68.803265
1089.360974	47.446066	68.808270
1088.676561	48.102166	68.813274
1087.953210	45.003358	68.818279
1087.370966	49.937328	68.823284
1086.035717	47.531961	68.828289
1085.401308	53.846205	68.833294
1085.222717	45.554467	68.838298
1084.644787	61.987112	68.843303
1083.955647	57.414689	68.848308
1083.186186	61.460642	68.853313
1082.127399	51.556896	68.858318
1081.905660	52.727609	68.863322
1081.399054	50.586243	68.868327
1080.925634	54.083619	68.873332
1079.901664	57.312182	68.878337
1079.299751	58.544952	68.883342
1079.330542	56.728110	68.888346
1078.026795	63.871100	68.893351
1077.243014	56.112458	68.898356
1076.541634	58.956959	68.903361
1075.512238	56.786796	68.908366
1075.021378	50.703624	68.913370
1074.136826	59.590301	68.918375
1073.599441	53.178632	68.923380
1073.408702	52.135062	68.928385
1072.925622	47.943033	68.933390
1072.426005	45.201305	68.938394
1071.299771	44.420103	68.943399
1070.545320	46.952919	68.948404
1069.967406	41.706786	68.953409
1068.953202	47.655667	68.958414
1068.561090	47.306465	68.963418
1067.541444	59.652457	68.968423
1067.597531	49.946678	68.973428
1067.244985	49.917618	68.978433
1066.432824	54.810898	68.983438
1065.703151	52.146771	68.988442
1064.821575	52.884708	68.993447
1064.131842	45.010188	68.998452
1063.262743	54.194033	69.003457
1062.341939	49.163302	69.008462
1061.998603	50.730259	69.013466
1061.578169	54.186092	69.018471
1060.899004	48.339467	69.023476
1059.945980	52.389395	69.028481
1059.095186	48.165982	69.033486
1058.986131	43.906568	69.038490
1058.389051	47.270652	69.043495
1057.070408	49.943695	69.048500
1056.823989	41.355243	69.053505
1056.215732	42.410827	69.058510
1056.012646	38.987982	69.063514
1054.877865	43.902626	69.068519
1054.079703	42.602451	69.073524
1053.921394	40.915046	69.078529
1052.590240	50.183440	69.083534
1051.689753	44.912935	69.088538
1050.819255	51.985426	69.093543
1050.796819	48.808234	69.098548
1050.485684	43.871329	69.103553
1049.722535	49.813392	69.108558
1049.148010	51.365092	69.113562
1048.023000	56.467426	69.118567
1047.519889	51.078505	69.123572
1046.831697	57.150575	69.128577
1045.411451	47.457325	69.133582
1045.161424	48.716121	69.138586
1044.659555	52.642237	69.143591
1044.353661	56.556098	69.148596
1044.201035	45.033730	69.153601
1043.128643	52.464779	69.158606
1042.284463	49.555522	69.163610
1041.748807	59.347080	69.168615
1041.292118	53.225363	69.173620
1040.296232	46.017737	69.178625
1039.006917	57.930390	69.183630
1038.603389	53.886563	69.188634
1038.192266	51.414620	69.193639
1038.011919	54.573633	69.198644
1036.921771	47.363658	69.203649
1035.836601	54.984404	69.208654
1035.784381	52.218812	69.213658
1035.055140	46.657712	69.218663
1034.830392	49.394850	69.223668
1033.878461	57.647270	69.228673
1032.841941	53.081247	69.233678
1032.762040	43.811857	69.238682
1031.500387	52.424219	69.243687
1030.941157	45.820495	69.248692
1030.661180	48.399260	69.253697
1030.053537	47.455141	69.258702
1029.167829	46.719269	69.263706
1027.957179	47.044365	69.268711
1027.811669	41.538632	69.273716
1027.230399	40.402657	69.278721
1026.369495	57.389687	69.283726
1025.770669	42.492611	69.288730
1024.883554	55.110842	69.293735
1024.230925	48.457324	69.298740
1023.961649	46.021163	69.303745
1023.151500	45.137652	69.308750
1022.380117	42.664684	69.313754
1021.555474	51.956583	69.318759
1021.282643	49.325443	69.323764
1020.824213	47.185888	69.328769
1019.486912	50.093734	69.333774
1019.221262	44.040980	69.338778
1018.643607	49.283320	69.343783
1018.183202	49.528475	69.348788
1016.850829	44.386627	69.353793
1016.033578	55.569731	69.358798
1015.964586	53.385560	69.363802
1015.592032	54.058293	69.368807
1014.565248	45.505699	69.373812
1013.772073	40.722771	69.378817
1012.992708	49.179552	69.383822
1012.653602	35.827608	69.388826
1011.586193	46.009702	69.393831
1011.160158	44.516288	69.398836
1010.469984	38.333962	69.403841
1009.836872	41.334774	69.408846
1009.697474	34.049240	69.413850
1008.364352	46.932401	69.418855
1007.487063	46.070616	69.423860
1006.826423	42.983934	69.428865
1006.540679	47.541151	69.433870
1006.305672	43.535176	69.438874
1005.596395	49.566450	69.443879
1004.932860	42.186111	69.448884
1004.103678	44.849109	69.453889
1003.285248	47.992953	69.458894
1002.426025	40.919724	69.463898
1001.535276	49.329574	69.468903
1001.305685	45.202886	69.473908
1001.062532	49.206116	69.478913
999.585902	52.377419	69.483918
999.126611	35.504280	69.488922
998.402869	50.466717	69.493927
997.991334	35.137729	69.498932
998.306130	43.245367	69.503937
997.194952	44.152326	69.508942
996.198286	44.815556	69.513946
995.197721	50.774908	69.518951
994.324765	45.957371	69.523956
993.681295	44.891226	69.528961
993.142330	37.620384	69.533966
992.876125	38.074345	69.538970
992.297112	46.158621	69.543975
991.373450	43.061755	69.548980
990.508210	42.732656	69.553985
989.818961	52.069252	69.558990
989.836829	35.653210	69.563994
989.071571	42.805163	69.568999
987.909389	44.729509	69.574004
987.462911	35.203065	69.579009
986.935331	46.109836	69.584014
986.448324	39.010503	69.589018
985.411446	46.697697	69.594023
984.927172	41.673235	69.599028
984.522893	46.455899	69.604033
983.120621	47.125327	69.609038
982.480696	45.114010	69.614042
981.705791	53.284657	69.619047
981.303400	49.633331	69.624052
981.011886	49.973046	69.629057
980.127451	49.022520	69.634062
979.588438	43.765491	69.639066
978.654833	49.032937	69.644071
978.157808	42.875080	69.649076
978.024051	39.509022	69.654081
976.751230	46.541469	69.659086
976.146175	31.475102	69.664090
975.378514	44.244640	69.669095
974.978885	48.233345	69.674100
974.639572	47.754329	69.679105
973.448406	57.766898	69.684110
973.197270	52.829919	69.689114
972.217825	51.251105	69.694119
970.993779	54.615625	69.699124
970.606790	43.816552	69.704129
969.678496	43.611036	69.709134
969.719777	48.215567	69.714138
969.329425	48.104225	69.719143
968.877697	42.278214	69.724148
968.263192	40.341705	69.729153
967.315821	41.747745	69.734158
966.016419	43.881596	69.739162
965.228723	47.358034	69.744167
964.505040	46.973300	69.749172
964.065118	51.838912	69.754177
963.737517	56.625150	69.759182
963.442067	43.739360	69.764186
962.502876	44.596888	69.769191
961.607771	51.297996	69.774196
961.552077	44.527432	69.779201
960.239882	58.676761	69.784206
959.319866	47.273368	69.789210
958.489887	52.793996	69.794215
958.472057	43.904253	69.799220
958.383362	52.993899	69.804225
957.173852	51.899565	69.809230
956.498665	45.763755	69.814234
956.231612	37.675357	69.819239
954.810632	59.050371	69.824244
954.118400	45.857131	69.829249
953.291050	57.373022	69.834254
953.009052	44.625444	69.839258
952.829936	47.946692	69.844263
951.717032	53.878204	69.849268
951.064891	42.660854	69.854273
950.068457	50.299046	69.859278
950.028401	42.808470	69.864282
949.495453	47.783505	69.869287
948.549423	53.557573	69.874292
947.915981	44.447247	69.879297
947.058244	44.951190	69.884302
946.554168	42.200740	69.889306
945.545325	43.859424	69.894311
945.141415	45.152179	69.899316
944.679791	45.749208	69.904321
943.988689	42.714702	69.909326
943.167998	40.506655	69.914330
942.004824	49.478700	69.919335
941.456453	41.245833	69.924340
941.115761	36.152803	69.929345
940.654474	46.810905	69.934350
940.301762	36.966771	69.939354
939.376930	47.337514	69.944359
938.673736	40.941237	69.949364
938.271626	37.053330	69.954369
937.114668	46.598406	69.959374
936.620294	36.650659	69.964378
935.840797	39.748901	69.969383
935.130173	43.394433	69.974388
934.420723	44.026172	69.979393
933.549703	48.643419	69.984398
933.349185	40.361506	69.989402
932.781805	37.397203	69.994407
932.226761	41.814351	69.999412
931.085956	38.753643	70.004417
930.175589	52.126234	70.009422
929.977376	42.842571	70.014426
929.676049	40.834155	70.019431
928.695943	42.582891	70.024436
928.143003	41.352544	70.029441
927.337384	40.656004	70.034446
927.227439	36.663256	70.039450
925.901711	42.631797	70.044455
924.908248	46.040065	70.049460
924.914778	43.694069	70.054465
924.206336	50.324480	70.059470
923.418691	46.012220	70.064474
922.510654	49.104115	70.069479
922.099516	43.449853	70.074484
921.716330	41.993793	70.079489
920.586036	39.894951	70.084494
919.610061	47.272848	70.089498
919.032740	47.664364	70.094503
918.644712	45.488394	70.099508
918.319598	46.667686	70.104513
917.713883	47.265574	70.109518
916.939084	42.164361	70.114522
915.702812	44.928443	70.119527
915.276566	37.992929	70.124532
915.274097	41.213522	70.129537
913.797769	48.402965	70.134542
913.139547	44.809716	70.139546
913.036303	44.332563	70.144551
912.362903	45.745484	70.149556
911.626009	47.796147	70.154561
910.451398	47.188300	70.159566
909.991805	42.399629	70.164570
909.494608	51.770330	70.169575
909.051711	40.305227	70.174580
908.126326	45.621849	70.179585
907.377256	46.917502	70.184590
907.035191	37.827054	70.189594
906.743995	41.022635	70.194599
905.306854	41.719732	70.199604
904.713158	35.984143	70.204609
904.051377	48.397794	70.209614
903.978729	41.289308	70.214618
902.686269	46.208607	70.219623
901.766771	49.494725	70.224628
901.634834	41.621378	70.229633
900.482297	49.271814	70.234638
900.280562	39.805789	70.239642
899.989180	45.786344	70.244647
898.756563	46.963413	70.249652
898.220007	48.392405	70.254657
897.745498	50.131649	70.259662
897.550192	43.340733	70.264666
896.108039	44.950127	70.269671
895.797331	47.959578	70.274676
895.458560	44.470035	70.279681
894.219483	47.430120	70.284686
893.787499	44.945755	70.289690
893.330967	46.772026	70.294695
892.124447	44.485053	70.299700
891.372066	36.037089	70.304705
890.673454	53.469821	70.309710
890.327783	43.701847	70.314714
890.191740	47.651764	70.319719
889.168575	46.188755	70.324724
888.152784	37.908874	70.329729
887.502243	45.818466	70.334734
887.218787	44.794400	70.339738
886.512950	44.663896	70.344743
885.207943	44.641373	70.349748
885.042324	45.016256	70.354753
884.214820	43.110517	70.359758
884.082012	41.548379	70.364762
883.569195	48.664911	70.369767
882.455012	51.786476	70.374772
881.823801	42.235842	70.379777
880.796276	54.297700	70.384782
879.698946	44.947412	70.389786
879.578355	48.456470	70.394791
878.786421	45.442763	70.399796
878.630372	46.219829	70.404801
877.866369	50.528319	70.409806
877.599798	49.388024	70.414810
876.984924	54.205798	70.419815
875.748442	41.693742	70.424820
875.466769	37.384550	70.429825
874.145725	49.409543	70.434830
873.882934	45.654017	70.439834
873.096990	44.161142	70.444839
872.711490	46.414511	70.449844
872.221698	34.218862	70.454849
870.786433	42.540366	70.459854
870.634257	43.045577	70.464858
870.217126	34.918005	70.469863
869.085770	43.128059	70.474868
868.259905	40.124488	70.479873
867.659135	47.209288	70.484878
867.425079	39.639211	70.489882
866.824950	47.619633	70.494887
865.938090	39.655137	70.499892
865.518417	35.401028	70.504897
864.353882	48.653233	70.509902
863.906003	33.793708	70.514906
862.730027	41.447885	70.519911
862.210871	43.397671	70.524916
861.949544	41.802374	70.529921
861.263839	46.103135	70.534926
861.246538	42.019950	70.539930
860.350383	41.369382	70.544935
858.899901	51.219833	70.549940
858.545392	48.760990	70.554945
858.088290	46.042507	70.559950
857.409348	46.948537	70.564954
856.453342	47.690506	70.569959
855.743450	46.496197	70.574964
855.747874	52.301937	70.579969
854.675422	51.461809	70.584974
853.703209	45.772288	70.589978
853.129710	45.128713	70.594983
852.469497	42.507217	70.599988
852.425224	43.935132	70.604993
851.620369	56.392071	70.609998
850.817868	53.503058	70.615002
850.100559	54.285885	70.620007
849.400471	57.516596	70.625012
849.033998	39.725124	70.630017
848.124220	51.150071	70.635022
847.730523	46.079684	70.640026
846.801985	43.762679	70.645031
845.726282	51.675301	70.650036
845.742680	42.437918	70.655041
844.749109	45.633341	70.660046
844.169298	44.065086	70.665050
843.122856	36.206430	70.670055
842.261094	42.547441	70.675060
842.085503	35.157302	70.680065
841.349370	47.783072	70.685070
841.346436	39.925471	70.690074
840.112473	42.067891	70.695079
839.075286	43.182340	70.700084
838.828187	38.082315	70.705089
837.781433	45.022064	70.710094
837.876022	38.260709	70.715098
836.885896	41.283695	70.720103
836.212623	43.060895	70.725108
835.849355	44.657861	70.730113
834.824426	48.336103	70.735118
833.707186	46.755627	70.740122
833.414661	39.792538	70.745127
832.560762	44.853372	70.750132
832.660765	42.289069	70.755137
831.807306	43.588744	70.760142
831.096418	39.754741	70.765146
830.061782	40.206457	70.770151
829.435397	54.719753	70.775156
829.214024	44.157711	70.780161
827.863800	43.998910	70.785166
827.279324	45.265231	70.790170
827.220505	41.455166	70.795175
826.570979	48.877322	70.800180
825.807006	44.269590	70.805185
824.725481	51.325269	70.810190
824.191004	46.315145	70.815194
824.083771	38.959858	70.820199
822.643887	48.829138	70.825204
822.290986	41.593382	70.830209
821.770191	48.116671	70.835214
821.139418	43.287460	70.840218
820.449543	49.869205	70.845223
819.212945	49.463659	70.850228
819.064788	45.204183	70.855233
818.650864	49.201490	70.860238
818.198730	36.055254	70.865242
817.199273	34.203720	70.870247
816.059803	46.056325	70.875252
816.020844	38.210769	70.880257
814.569294	50.997741	70.885262
814.113603	46.361438	70.890266
813.690656	43.587064	70.895271
812.978327	49.519516	70.900276
812.528886	36.041687	70.905281
811.868900	45.771049	70.910286
811.272677	48.193591	70.915290
810.679888	47.277125	70.920295
809.760859	49.531854	70.925300
809.161147	38.651574	70.930305
808.290947	37.631035	70.935310
807.653256	43.996311	70.940314
807.426311	43.792749	70.945319
806.469958	44.340824	70.950324
805.595558	33.587856	70.955329
805.206789	44.177649	70.960334
804.805398	41.029257	70.965338
803.713167	38.509667	70.970343
803.015307	41.818880	70.975348
803.057617	34.242669	70.980353
802.046628	41.968377	70.985358
800.850359	43.335251	70.990362
799.900430	37.940258	70.995367
799.357850	37.911525	71.000372
799.105924	35.893688	71.005377
798.784486	38.745579	71.010382
798.323752	38.729048	71.015386
797.338166	34.060413	71.020391
796.312364	45.071746	71.025396
796.221130	36.452335	71.030401
795.130113	40.875982	71.035406
794.292457	39.664183	71.040410
793.938599	29.030209	71.045415
793.283672	41.147883	71.050420
793.067394	36.598055	71.055425
791.449426	47.060256	71.060430
790.999630	43.530058	71.065434
790.676499	42.774098	71.070439
790.232393	43.645914	71.075444
789.506851	33.197267	71.080449
788.461061	39.859329	71.085454
788.023049	38.948192	71.090458
787.605223	43.417638	71.095463
786.509292	41.748634	71.100468
785.886952	38.646460	71.105473
784.701691	44.625821	71.110478
784.698357	44.199002	71.115482
784.333852	41.054203	71.120487
783.045107	46.367209	71.125492
782.366062	32.484393	71.130497
781.909274	38.972262	71.135502
781.531302	45.083304	71.140506
781.130532	41.099020	71.145511
779.997842	48.705339	71.150516
779.413678	37.403119	71.155521
778.874644	41.423500	71.160526
778.345692	35.132008	71.165530
777.500638	38.463083	71.170535
776.676498	41.114307	71.175540
776.414327	38.561931	71.180545
775.381670	39.732455	71.185550
774.594228	46.935299	71.190554
774.246298	45.995630	71.195559
773.241240	48.152103	71.200564
773.177525	33.198332	71.205569
771.801296	39.790003	71.210574
771.210112	38.557897	71.215578
771.064073	39.229295	71.220583
769.980969	43.743157	71.225588
769.128913	40.401588	71.230593
768.254060	46.192764	71.235598
767.819073	38.317222	71.240602
767.698508	41.312181	71.245607
766.981964	51.506304	71.250612
766.925195	42.771018	71.255617
765.691400	50.000773	71.260622
765.041736	46.286355	71.265626
764.282623	49.089659	71.270631
763.111264	42.963524	71.275636
762.802831	43.594544	71.280641
762.212365	46.292150	71.285646
761.840174	44.963678	71.290650
760.706773	40.867378	71.295655
759.950789	36.485483	71.300660
759.856679	35.981653	71.305665
758.917566	36.321994	71.310670
758.585615	36.647671	71.315674
757.748116	38.632390	71.320679
757.039266	42.205142	71.325684
756.742104	43.135570	71.330689
755.252643	49.213841	71.335694
754.482840	46.598782	71.340698
753.936128	40.084615	71.345703
753.478920	47.348429	71.350708
753.199088	35.051581	71.355713
752.505301	42.490256	71.360718
751.638356	45.135687	71.365722
751.390397	44.678429	71.370727
750.369193	46.755478	71.375732
749.447543	41.808596	71.380737
748.655241	44.200867	71.385742
748.333328	43.610302	71.390746
747.852355	39.181471	71.395751
747.002078	46.988846	71.400756
746.163062	42.700600	71.405761
745.826593	38.761280	71.410766
745.309009	38.370606	71.415770
744.785317	40.422062	71.420775
743.357710	46.567761	71.425780
742.807896	41.101202	71.430785
742.387221	51.331802	71.435790
741.958411	48.476372	71.440794
740.933162	51.208515	71.445799
740.041433	56.187092	71.450804
739.628861	45.474158	71.455809
739.437461	45.506220	71.460814
738.931896	41.198002	71.465818
737.733451	41.109703	71.470823
737.189667	55.051607	71.475828
736.581307	42.881182	71.480833
735.404713	48.141661	71.485838
734.655369	34.530258	71.490842
734.551829	40.901963	71.495847
733.734482	42.323655	71.500852
733.541975	44.044834	71.505857
732.517875	44.512259	71.510862
731.265893	43.814313	71.515866
731.091527	47.803449	71.520871
730.427310	39.735753	71.525876
730.351607	41.121363	71.530881
729.114650	44.338233	71.535886
728.147671	46.933367	71.540890
727.982358	40.929344	71.545895
727.340365	45.693114	71.550900
726.691524	42.245087	71.555905
725.855680	51.311751	71.560910
724.973517	56.195769	71.565914
724.762799	46.485194	71.570919
723.695999	42.957058	71.575924
723.038451	45.290033	71.580929
722.178112	36.346808	71.585934
721.828916	41.863484	71.590938
721.453828	44.470033	71.595943
720.624106	56.082542	71.600948
720.116096	36.992148	71.605953
719.425308	43.236583	71.610958
719.004904	43.245185	71.615962
717.995987	38.842076	71.620967
717.152889	50.302168	71.625972
716.835729	35.805082	71.630977
716.143033	43.106395	71.635982
715.084983	35.716436	71.640986
714.734405	37.156852	71.645991
713.997539	41.372750	71.650996
713.562556	31.272114	71.656001
712.903440	42.251891	71.661006
712.166681	37.024847	71.666010
711.744681	35.768971	71.671015
710.623939	40.381889	71.676020
709.934753	31.256877	71.681025
708.966757	33.735482	71.686030
708.416656	46.263839	71.691034
708.458965	24.397096	71.696039
707.173653	37.971351	71.701044
706.517989	35.710303	71.706049
705.790802	38.959553	71.711054
705.511116	38.363846	71.716058
705.256550	38.126844	71.721063
704.060938	29.852038	71.726068
703.138287	37.426513	71.731073
702.541905	40.177112	71.736078
702.085032	40.994204	71.741082
701.963330	35.262368	71.746087
700.789320	38.913932	71.751092
700.152811	36.178320	71.756097
699.615848	40.625745	71.761102
698.319005	40.193582	71.766106
697.732371	47.414932	71.771111
696.771851	38.695831	71.776116
696.658971	38.194991	71.781121
696.203301	44.032980	71.786126
695.794856	42.141004	71.791130
695.462429	37.220171	71.796135
694.458857	47.904716	71.801140
693.931365	39.274360	71.806145
693.006115	40.975024	71.811150
692.208276	36.755939	71.816154
691.549762	35.823160	71.821159
690.879959	37.129906	71.826164
690.161187	36.427500	71.831169
689.134320	44.671444	71.836174
688.315467	43.824123	71.841178
688.523518	36.626809	71.846183
687.887338	35.337233	71.851188
687.193327	40.512998	71.856193
686.335432	39.979405	71.861198
685.242962	38.622138	71.866202
685.102820	40.407522	71.871207
683.925984	42.361144	71.876212
683.287558	40.791225	71.881217
682.859584	46.241601	71.886222
682.243281	42.756866	71.891226
681.988809	33.769222	71.896231
681.281000	43.167169	71.901236
680.459639	31.940607	71.906241
680.143944	39.517786	71.911246
678.861875	46.715838	71.916250
678.163554	39.902555	71.921255
677.260444	39.194814	71.926260
677.255513	38.713056	71.931265
676.338244	39.023141	71.936270
675.192414	33.760327	71.941274
674.910008	34.902882	71.946279
673.979036	41.748553	71.951284
673.681380	41.220368	71.956289
673.512986	38.127940	71.961294
672.484818	33.041936	71.966298
671.834169	33.965585	71.971303
671.159361	42.380554	71.976308
670.594142	30.957088	71.981313
669.777203	36.049928	71.986318
668.841914	37.720660	71.991322
668.606053	37.122710	71.996327
667.942302	39.958163	72.001332
667.192409	31.456277	72.006337
666.530515	46.976612	72.011342
665.657287	45.710598	72.016346
665.213027	22.645580	72.021351
664.361940	37.402817	72.026356
663.730714	44.882011	72.031361
663.096416	41.535767	72.036366
662.670584	36.401154	72.041370
661.995333	35.024766	72.046375
660.999447	43.102933	72.051380
660.457871	35.566098	72.056385
659.980906	39.160293	72.061390
659.186915	40.551480	72.066394
658.404225	33.497751	72.071399
657.776075	40.695753	72.076404
657.256550	40.650763	72.081409
656.719370	40.722128	72.086414
655.691231	49.410994	72.091418
655.476880	37.936383	72.096423
654.606250	48.325375	72.101428
654.102702	41.435350	72.106433
652.807629	40.827886	72.111438
652.062148	45.587651	72.116442
651.832107	41.790673	72.121447
651.291282	55.470333	72.126452
650.910721	40.022982	72.131457
649.909436	39.679396	72.136462
648.996577	48.447678	72.141466
648.790319	44.549139	72.146471
648.259556	46.716859	72.151476
647.290828	35.474354	72.156481
646.869379	41.117661	72.161486
646.142335	42.148102	72.166490
645.312622	33.986946	72.171495
644.323598	49.193526	72.176500
643.950733	38.220407	72.181505
643.731157	39.646277	72.186510
642.384587	44.126452	72.191514
641.676091	41.244622	72.196519
640.795272	41.189365	72.201524
640.505021	33.885328	72.206529
640.036665	43.120566	72.211534
639.843695	45.122527	72.216538
639.263098	38.615367	72.221543
638.073690	57.733225	72.226548
637.835562	37.734123	72.231553
636.695476	37.261259	72.236558
635.521450	38.060110	72.241562
635.364249	41.616000	72.246567
634.966866	42.436245	72.251572
634.337225	44.001541	72.256577
633.169797	46.601824	72.261582
632.529146	53.093766	72.266586
632.478688	42.321616	72.271591
631.367374	49.107714	72.276596
630.275802	38.998124	72.281601
629.524259	39.502608	72.286606
629.163081	44.327332	72.291610
629.017850	36.569686	72.296615
628.756414	37.666328	72.301620
627.857207	37.729123	72.306625
626.848398	42.226476	72.311630
626.299793	39.972054	72.316634
625.615935	33.946554	72.321639
624.391824	43.891946	72.326644
623.700567	47.234846	72.331649
623.673964	36.861031	72.336654
622.941043	36.454215	72.341658
622.411846	37.639235	72.346663
621.476900	51.041037	72.351668
621.175525	38.979464	72.356673
620.370561	39.375764	72.361678
619.270032	46.068682	72.366682
618.744113	41.069868	72.371687
618.320728	40.487597	72.376692
617.956290	39.768203	72.381697
616.421866	49.974339	72.386702
615.692536	44.184741	72.391706
615.424256	33.396830	72.396711
614.888759	55.936655	72.401716
614.624543	43.328260	72.406721
613.830222	43.137809	72.411726
613.126680	46.596210	72.416730
612.626810	44.892277	72.421735
611.464369	47.026568	72.426740
610.257966	40.858788	72.431745
610.089780	49.954761	72.436750
609.272858	49.990264	72.441754
609.076526	39.192468	72.446759
608.474117	51.691321	72.451764
607.923282	48.591999	72.456769
607.191024	42.973184	72.461774
606.347057	47.478985	72.466778
606.244618	46.750980	72.471783
604.700946	51.970630	72.476788
604.164293	45.983188	72.481793
603.810827	43.555762	72.486798
603.057993	43.139508	72.491802
602.363182	47.075921	72.496807
601.444026	50.999180	72.501812
601.074654	46.059015	72.506817
600.769255	41.403557	72.511822
599.757350	43.461836	72.516826
598.900021	37.323622	72.521831
598.221891	53.786433	72.526836
598.216200	47.649767	72.531841
597.237813	50.961135	72.536846
596.150423	53.504532	72.541850
595.808300	47.544456	72.546855
595.098787	42.234263	72.551860
594.846378	53.280175	72.556865
593.354141	43.915671	72.561870
592.804952	52.034681	72.566874
592.530495	45.723203	72.571879
591.785838	42.916535	72.576884
591.122241	46.699743	72.581889
590.280880	44.928780	72.586894
589.730281	37.249898	72.591898
589.247076	40.143345	72.596903
588.977141	43.706154	72.601908
587.773167	44.063514	72.606913
586.837666	40.087170	72.611918
586.247933	47.146602	72.616922
586.310057	46.606855	72.621927
585.336166	45.711722	72.626932
584.442069	48.367840	72.631937
583.936563	47.312947	72.636942
583.102243	43.609073	72.641946
582.473386	37.535400	72.646951
581.651748	41.252318	72.651956
581.158080	39.610484	72.656961
580.713927	37.859837	72.661966
580.122773	42.158216	72.666970
579.318531	36.252831	72.671975
578.406956	45.020926	72.676980
577.889248	32.771475	72.681985
577.559853	36.692264	72.686990
576.623502	42.777144	72.691994
575.904575	31.452312	72.696999
575.599234	46.603622	72.702004
574.792580	45.631392	72.707009
573.934578	41.989643	72.712014
573.281114	40.453688	72.717018
572.825944	36.243144	72.722023
572.125470	40.942142	72.727028
571.208856	44.415568	72.732033
570.560963	45.602159	72.737038
569.951845	43.756363	72.742042
569.709306	30.628867	72.747047
568.457044	41.264746	72.752052
567.934493	42.601685	72.757057
567.295328	38.015168	72.762062
566.532981	46.745303	72.767066
566.187938	36.655611	72.772071
564.939141	50.137380	72.777076
564.642573	43.365799	72.782081
564.337105	41.414866	72.787086
563.702759	45.027839	72.792090
562.605479	44.387339	72.797095
561.555389	45.921853	72.802100
560.987959	41.634573	72.807105
561.064356	41.735956	72.812110
560.447743	45.740348	72.817114
559.704145	40.356749	72.822119
558.411449	40.589482	72.827124
558.218931	43.934955	72.832129
557.688457	38.146821	72.837134
556.675777	52.382623	72.842138
556.147454	42.725830	72.847143
555.636708	45.436011	72.852148
555.165900	41.486584	72.857153
553.916328	38.962211	72.862158
552.955329	44.259385	72.867162
552.813346	31.087490	72.872167
552.459439	41.909860	72.877172
551.897179	35.418732	72.882177
551.238057	35.806014	72.887182
550.127253	38.477738	72.892186
549.727634	39.345661	72.897191
548.542331	42.264222	72.902196
547.747174	48.870677	72.907201
547.659744	31.038024	72.912206
547.064930	34.908054	72.917210
546.208067	29.802707	72.922215
545.021257	43.096405	72.927220
544.576291	37.804015	72.932225
544.446167	38.862402	72.937230
543.637494	42.465300	72.942234
543.389568	33.859846	72.947239
542.342153	42.085031	72.952244
541.359881	36.413028	72.957249
541.393922	33.830844	72.962254
540.192532	44.521711	72.967258
539.420535	37.773833	72.972263
538.837499	40.561765	72.977268
538.709097	34.067761	72.982273
537.651271	44.505521	72.987278
536.449959	38.418975	72.992282
536.486113	31.395704	72.997287
535.886437	34.039628	73.002292
534.965833	35.879958	73.007297
534.258073	30.249386	73.012302
533.236828	45.964174	73.017306
533.088217	34.203150	73.022311
532.575659	37.312596	73.027316
531.866813	41.391610	73.032321
531.330843	38.517026	73.037326
530.503126	50.048824	73.042330
530.141143	34.204315	73.047335
528.957513	42.271430	73.052340
528.508489	44.443497	73.057345
528.101162	37.282712	73.062350
526.610246	31.970870	73.067354
525.942603	33.077037	73.072359
524.975202	37.850107	73.077364
524.654689	36.549712	73.082369
524.513104	39.530676	73.087374
524.036063	42.714892	73.092378
523.710348	27.640485	73.097383
522.398179	40.566224	73.102388
521.884010	38.751047	73.107393
521.344003	35.244744	73.112398
520.000162	49.162720	73.117402
519.354303	40.207493	73.122407
518.949574	39.669576	73.127412
518.693115	43.444711	73.132417
518.338463	34.487253	73.137422
517.041722	40.821953	73.142426
516.620122	42.961268	73.147431
515.572382	39.613122	73.152436
515.424941	37.247510	73.157441
514.093845	44.317823	73.162446
513.346451	50.019381	73.167450
512.976264	40.487223	73.172455
512.710641	43.312905	73.177460
512.204261	40.889355	73.182465
511.616017	38.748510	73.187470
510.353159	53.244957	73.192474
510.146879	43.510064	73.197479
509.831691	40.382690	73.202484
508.816373	38.108031	73.207489
508.227643	28.683239	73.212494
506.955582	45.412557	73.217498
506.137143	37.539825	73.222503
505.309096	41.757685	73.227508
504.678775	37.209203	73.232513
504.533629	44.998921	73.237518
504.060321	45.724047	73.242522
503.911281	35.901194	73.247527
502.878288	38.199415	73.252532
502.046248	34.884722	73.257537
501.278023	38.834429	73.262542
500.722562	40.305936	73.267546
499.735938	41.680551	73.272551
498.708288	35.930640	73.277556
498.067956	37.316319	73.282561
498.152194	29.815454	73.287566
497.289500	42.054577	73.292570
497.151050	37.853517	73.297575
496.345883	38.421778	73.302580
495.399225	36.830053	73.307585
494.989039	39.100018	73.312590
493.400665	47.124397	73.317594
492.967099	34.095161	73.322599
492.467059	37.025999	73.327604
492.317456	36.737604	73.332609
491.866437	34.071849	73.337614
491.175542	35.399352	73.342618
490.486640	31.856854	73.347623
489.824970	34.696747	73.352628
488.431398	27.917033	73.357633
487.858603	35.312825	73.362638
487.224310	38.761799	73.367642
487.330561	27.594126	73.372647
486.257251	30.539026	73.377652
485.628943	29.880616	73.382657
485.342248	35.634934	73.387662
483.837994	34.537332	73.392666
483.318412	28.151393	73.397671
482.616517	35.693912	73.402676
482.008303	33.072127	73.407681
481.805634	32.781149	73.412686
480.865745	35.315283	73.417690
480.440315	25.486012	73.422695
479.504984	33.500965	73.427700
478.908043	30.522568	73.432705
478.006721	18.573981	73.437710
477.284888	29.765626	73.442714
476.600699	25.375551	73.447719
476.255789	28.425178	73.452724
475.733625	35.275159	73.457729
474.976641	38.500830	73.462734
473.894479	47.581564	73.467738
473.673581	37.811164	73.472743
473.397040	39.353357	73.477748
472.027042	39.793995	73.482753
471.503254	36.138462	73.487758
470.599349	47.354399	73.492762
470.279074	31.041216	73.497767
469.801333	45.467773	73.502772
468.914990	40.608427	73.507777
468.336255	34.239798	73.512782
467.550770	33.699477	73.517786
467.179039	30.410808	73.522791
465.713884	33.468610	73.527796
465.034422	31.900559	73.532801
465.156816	30.270983	73.537806
464.563384	36.917854	73.542810
463.894016	32.435531	73.547815
462.888180	34.868214	73.552820
462.384197	26.618971	73.557825
462.094474	24.663970	73.562830
460.876624	35.363789	73.567834
460.167864	30.594429	73.572839
459.275219	31.667077	73.577844
458.654952	32.620632	73.582849
458.543551	28.938823	73.587854
457.944770	36.928547	73.592858
457.190998	31.108212	73.597863
456.364879	37.800044	73.602868
455.981382	38.157628	73.607873
455.674854	29.522106	73.612878
454.150131	47.562739	73.617882
453.527178	37.157806	73.622887
453.028786	31.623215	73.627892
452.438977	42.137819	73.632897
451.426177	34.838557	73.637902
450.897749	35.241312	73.642906
450.973602	34.218399	73.647911
450.203859	28.533078	73.652916
449.167656	39.401083	73.657921
448.534414	26.684384	73.662926
447.935092	39.889234	73.667930
447.500348	32.579873	73.672935
446.064644	43.905780	73.677940
445.351707	34.448756	73.682945
445.227827	33.610634	73.687950
444.758843	33.661716	73.692954
444.148802	33.446688	73.697959
443.024556	38.008231	73.702964
442.575068	29.559496	73.707969
442.052973	33.406922	73.712974
441.195165	33.825891	73.717978
440.736465	39.344266	73.722983
440.295867	32.280270	73.727988
438.990305	32.070410	73.732993
438.321046	23.902705	73.737998
437.414868	33.945738	73.743002
437.046104	31.233772	73.748007
436.477684	32.325730	73.753012
436.461621	38.211973	73.758017
435.467117	25.018251	73.763022
434.183488	36.793016	73.768026
434.149448	32.192124	73.773031
433.492007	29.655469	73.778036
432.441134	36.350002	73.783041
431.744284	30.457528	73.788046
431.090070	36.653614	73.793050
430.927538	27.610374	73.798055
429.971999	36.451741	73.803060
429.094672	38.731494	73.808065
428.918581	34.157967	73.813070
428.309772	34.037365	73.818074
427.161462	35.060876	73.823079
426.342302	41.996038	73.828084
425.605772	30.722961	73.833089
425.548687	29.505186	73.838094
424.852328	31.579483	73.843098
424.333356	23.375220	73.848103
423.224737	30.479505	73.853108
422.730276	33.999252	73.858113
422.498025	29.191822	73.863118
421.073991	38.692901	73.868122
420.539012	28.174620	73.873127
419.854919	29.635100	73.878132
419.408169	28.903621	73.883137
419.018435	31.449460	73.888142
417.720850	35.538734	73.893146
417.316758	32.020263	73.898151
416.918970	36.883953	73.903156
416.535735	35.158325	73.908161
415.470851	31.125401	73.913166
414.424692	37.070130	73.918170
414.261116	35.203843	73.923175
413.639930	31.057639	73.928180
412.228267	33.701666	73.933185
411.892542	32.356403	73.938190
411.208374	31.522409	73.943194
410.896060	39.228371	73.948199
410.569590	30.047252	73.953204
409.340105	40.520288	73.958209
408.837351	31.329412	73.963214
407.939026	34.716396	73.968218
407.710741	33.213662	73.973223
407.518150	36.368338	73.978228
406.548408	39.153263	73.983233
405.775299	30.292479	73.988238
404.209040	34.817238	73.993242
403.759981	26.534029	73.998247
403.290136	40.472042	74.003252
402.472807	36.809686	74.008257
402.244984	33.384554	74.013262
401.743737	30.608551	74.018266
401.464723	29.315754	74.023271
400.446511	35.740163	74.028276
399.593969	27.959648	74.033281
399.659377	34.063142	74.038286
398.039908	35.850882	74.043290
397.813629	38.134132	74.048295
397.098508	28.663286	74.053300
395.828315	32.371310	74.058305
395.224565	33.465753	74.063310
394.330032	39.897265	74.068314
394.315100	39.746689	74.073319
393.806540	34.492856	74.078324
393.459317	38.891171	74.083329
392.456599	38.003865	74.088334
391.282550	43.243579	74.093338
391.009080	34.202250	74.098343
390.679097	36.601376	74.103348
389.555360	38.584516	74.108353
388.806285	41.058313	74.113358
388.644220	40.041773	74.118362
388.197287	44.071200	74.123367
387.133050	41.865890	74.128372
386.211600	46.503952	74.133377
385.906883	34.747332	74.138382
384.792858	38.149774	74.143386
383.986813	42.288469	74.148391
383.189761	37.753978	74.153396
383.043203	39.833712	74.158401
383.086036	39.330152	74.163406
381.926243	42.255761	74.168410
381.183310	38.578402	74.173415
380.357572	43.532375	74.178420
379.880537	38.811267	74.183425
379.290647	31.995009	74.188430
378.312497	38.550238	74.193434
377.423430	36.249209	74.198439
377.395256	39.475456	74.203444
376.811722	37.881104	74.208449
375.928635	25.915464	74.213454
375.001304	32.779563	74.218458
374.687575	28.535488	74.223463
374.027878	42.215174	74.228468
372.869728	37.823390	74.233473
372.309995	33.575940	74.238478
371.758535	36.578071	74.243482
371.564502	35.812635	74.248487
370.707199	32.431055	74.253492
369.614553	33.915657	74.258497
369.127420	32.189249	74.263502
368.455752	31.287042	74.268506
368.007484	36.821109	74.273511
366.771326	36.966083	74.278516
366.029928	44.686815	74.283521
366.158772	23.262105	74.288526
365.591928	37.248691	74.293530
364.855121	33.078349	74.298535
364.196881	26.079024	74.303540
363.411154	31.759911	74.308545
362.865105	22.290524	74.313550
361.615170	34.728580	74.318554
360.874659	36.820970	74.323559
360.430786	36.350821	74.328564
360.018622	31.105290	74.333569
360.041121	26.167384	74.338574
358.478141	40.736933	74.343578
357.991628	37.512308	74.348583
357.526519	36.474681	74.353588
356.030377	36.347278	74.358593
355.682796	25.980505	74.363598
354.680489	35.400209	74.368602
354.537610	22.681094	74.373607
354.208520	31.894155	74.378612
353.774332	34.087539	74.383617
353.271788	26.131416	74.388622
352.063826	30.111818	74.393626
352.019908	29.387116	74.398631
350.543121	36.491759	74.403636
349.833309	39.752524	74.408641
349.376539	44.043723	74.413646
348.967323	35.001960	74.418650
348.000863	43.950753	74.423655
347.179800	41.508008	74.428660
346.466058	41.478268	74.433665
346.199579	36.818229	74.438670
345.475111	37.597607	74.443674
344.619980	39.208370	74.448679
343.720920	37.549196	74.453684
343.329630	37.217327	74.458689
343.319067	32.309920	74.463694
342.116491	46.804696	74.468698
341.567012	28.449641	74.473703
340.992520	38.108675	74.478708
340.138208	39.757157	74.483713
339.551180	35.665454	74.488718
338.550991	44.526585	74.493722
337.760724	38.768878	74.498727
337.888639	36.636942	74.503732
336.972266	39.030183	74.508737
336.168209	28.843400	74.513742
335.163388	33.636689	74.518746
334.733238	39.693004	74.523751
334.641760	30.699955	74.528756
333.441286	33.474371	74.533761
332.908787	35.793815	74.538766
332.076383	35.223168	74.543770
331.885311	33.764974	74.548775
331.002145	33.489426	74.553780
329.997906	36.841277	74.558785
329.851499	28.891476	74.563790
329.011984	36.033333	74.568794
328.086947	27.545307	74.573799
326.965301	30.851215	74.578804
326.584005	40.167221	74.583809
326.811066	29.924908	74.588814
325.913115	34.797362	74.593818
324.981800	31.528522	74.598823
323.919108	33.911971	74.603828
323.601313	36.007960	74.608833
323.233331	27.019562	74.613838
322.776418	34.135132	74.618842
321.589106	28.864924	74.623847
320.918810	29.947913	74.628852
320.439577	28.874698	74.633857
319.481764	23.793420	74.638862
318.641427	29.188129	74.643866
318.095056	34.077089	74.648871
317.622197	24.597626	74.653876
317.272195	30.407773	74.658881
316.757314	30.846244	74.663886
315.459959	33.590378	74.668890
314.917662	28.617915	74.673895
314.807196	23.083034	74.678900
313.411732	39.190253	74.683905
312.978421	20.480810	74.688910
312.133159	34.634778	74.693914
311.560412	26.388656	74.698919
311.834745	26.663488	74.703924
310.269566	28.098851	74.708929
309.672589	31.862039	74.713934
308.942624	34.470007	74.718938
308.780442	25.742126	74.723943
307.639442	24.632468	74.728948
306.821030	32.135244	74.733953
306.613189	16.597421	74.738958
306.238769	29.173489	74.743962
305.326364	20.317608	74.748967
304.593171	25.996443	74.753972
304.101736	28.053877	74.758977
303.291611	19.943370	74.763982
302.205292	22.549791	74.768986
301.507716	21.861469	74.773991
301.174552	29.406749	74.778996
300.461433	38.067588	74.784001
299.582142	27.288835	74.789006
298.691902	32.488077	74.794010
298.154753	33.411076	74.799015
297.728338	30.276236	74.804020
297.681297	37.399019	74.809025
297.200878	38.866492	74.814030
295.865899	32.795079	74.819034
295.374932	28.011561	74.824039
294.828946	34.930019	74.829044
293.969133	31.761759	74.834049
293.259285	29.962057	74.839054
292.688945	35.490359	74.844058
291.817512	35.121491	74.849063
291.022850	32.113160	74.854068
290.137312	27.184377	74.859073
290.018905	22.593791	74.864078
289.570744	24.647484	74.869082
288.899168	32.850687	74.874087
287.733887	34.187629	74.879092
287.055724	30.146740	74.884097
286.949510	33.030606	74.889102
286.269999	26.094623	74.894106
285.233149	31.790328	74.899111
284.456807	22.086437	74.904116
283.780485	36.282869	74.909121
283.746937	31.617252	74.914126
282.821498	37.798254	74.919130
281.834787	29.339003	74.924135
281.408705	14.040983	74.929140
280.884153	36.750911	74.934145
279.948674	26.052089	74.939150
279.356064	29.578041	74.944154
278.484924	26.424209	74.949159
278.381894	24.494668	74.954164
277.392477	30.069272	74.959169
276.539414	23.017455	74.964174
276.077122	26.782833	74.969178
275.854261	24.810892	74.974183
274.942973	29.400056	74.979188
273.483982	26.248468	74.984193
273.352001	21.245306	74.989198
272.905033	22.809952	74.994202
272.595083	32.966144	74.999207
271.501481	18.564589	75.004212
270.597673	37.807305	75.009217
270.465164	22.489290	75.014222
269.095041	26.829896	75.019226
268.218325	30.989347	75.024231
267.889195	29.455396	75.029236
267.361082	36.637517	75.034241
267.057262	36.290140	75.039246
266.544652	36.045433	75.044250
265.566383	29.800482	75.049255
264.579962	27.269011	75.054260
264.057937	28.951280	75.059265
263.991012	27.924316	75.064270
262.780432	35.219959	75.069274
261.996073	35.389160	75.074279
261.636008	20.220966	75.079284
261.054503	25.571276	75.084289
260.432422	26.935179	75.089294
259.830555	34.734612	75.094298
259.241028	30.015700	75.099303
258.257529	29.305160	75.104308
256.963226	43.712081	75.109313
256.999661	31.842764	75.114318
256.211236	40.692237	75.119322
255.785203	32.857984	75.124327
255.042344	28.264442	75.129332
254.029371	30.259945	75.134337
253.399568	34.725397	75.139342
253.061966	36.201649	75.144346
252.501280	31.061822	75.149351
251.718355	40.265236	75.154356
250.698233	39.541614	75.159361
250.601672	36.489818	75.164366
249.859544	35.773920	75.169370
248.576741	37.818748	75.174375
248.441984	27.176799	75.179380
247.528505	42.775123	75.184385
247.343950	35.947904	75.189390
246.044651	35.849113	75.194394
245.558049	38.314223	75.199399
244.973523	34.759894	75.204404
244.397796	38.874526	75.209409
244.187551	36.394369	75.214414
243.262527	36.179143	75.219418
242.545397	38.406611	75.224423
241.781390	35.089056	75.229428
240.715046	36.582136	75.234433
240.021072	28.446825	75.239438
239.658865	36.376791	75.244442
239.051577	35.237274	75.249447
238.723095	30.360057	75.254452
237.818993	34.317302	75.259457
237.397760	35.354299	75.264462
236.655034	35.654067	75.269466
235.701431	29.416237	75.274471
234.919868	32.995976	75.279476
234.021725	32.904202	75.284481
233.901684	32.100174	75.289486
233.475774	42.711679	75.294490
232.696614	38.964452	75.299495
231.897424	27.288284	75.304500
230.801814	36.191463	75.309505
230.726616	26.729054	75.314510
229.483715	34.045633	75.319514
228.540112	23.848031	75.324519
228.446483	31.197433	75.329524
227.896162	33.973904	75.334529
227.478286	34.911019	75.339534
226.987139	32.013596	75.344538
225.899595	38.635201	75.349543
225.495270	38.810059	75.354548
224.551454	40.091222	75.359553
223.808155	27.781668	75.364558
223.042623	33.109286	75.369562
222.282680	41.091626	75.374567
221.956758	32.397745	75.379572
221.544810	37.963887	75.384577
220.812785	32.061325	75.389582
219.931464	26.381264	75.394586
219.177291	31.820613	75.399591
219.008831	36.479029	75.404596
217.450239	34.497693	75.409601
217.025512	31.045631	75.414606
216.645449	31.544630	75.419610
215.970232	26.050911	75.424615
215.781081	33.663125	75.429620
214.659815	28.536988	75.434625
214.217140	36.238508	75.439630
213.496714	35.049226	75.444634
212.339247	30.469760	75.449639
211.638309	28.168765	75.454644
210.794771	35.718151	75.459649
210.683491	34.020165	75.464654
210.655175	33.805492	75.469658
209.492447	40.937412	75.474663
208.965516	23.209611	75.479668
208.091424	36.328977	75.484673
207.381662	26.441035	75.489678
206.250185	24.544578	75.494682
205.722877	33.336658	75.499687
205.444752	26.371403	75.504692
204.876518	37.909197	75.509697
204.466193	34.921623	75.514702
203.168683	37.675299	75.519706
202.679820	35.155989	75.524711
202.397113	31.438434	75.529716
201.396352	34.048605	75.534721
200.525875	23.243266	75.539726
199.912213	32.028613	75.544730
199.059032	38.247006	75.549735
199.109417	29.917338	75.554740
198.435290	31.548177	75.559745
197.917108	25.324524	75.564750
196.901705	34.117154	75.569754
196.255182	34.685448	75.574759
195.382441	36.004176	75.579764
194.265469	39.446593	75.584769
194.018916	31.597933	75.589774
193.716505	33.070159	75.594778
193.338113	32.371979	75.599783
192.532993	36.209379	75.604788
191.309406	39.485867	75.609793
191.286149	34.080595	75.614798
190.361830	40.753460	75.619802
189.361391	38.071288	75.624807
189.011212	30.448889	75.629812
188.213035	41.089787	75.634817
187.427756	32.196339	75.639822
186.584925	42.606237	75.644826
186.040152	34.765702	75.649831
185.822709	26.045075	75.654836
184.821814	36.451785	75.659841
183.782643	34.491735	75.664846
183.216171	32.383776	75.669850
182.687812	30.558325	75.674855
182.381376	41.869879	75.679860
182.002758	41.562824	75.684865
181.613964	34.452788	75.689870
180.508377	34.395686	75.694874
179.880123	40.735918	75.699879
178.932719	35.591537	75.704884
177.826036	40.932563	75.709889
177.320211	35.858126	75.714894
177.048079	31.014513	75.719898
176.635208	34.481866	75.724903
176.127169	31.535109	75.729908
174.789061	32.019713	75.734913
174.453233	26.167539	75.739918
173.979094	31.123853	75.744922
173.019732	30.581389	75.749927
172.249072	25.596492	75.754932
171.573431	28.490727	75.759937
171.252037	27.938005	75.764942
170.404279	27.448711	75.769946
169.486118	37.350222	75.774951
169.368946	26.114121	75.779956
168.352299	37.116287	75.784961
168.101250	28.747952	75.789966
166.921734	33.477692	75.794970
166.475261	44.699612	75.799975
166.172337	38.400638	75.804980
164.805784	32.756967	75.809985
164.098799	35.055379	75.814990
163.730844	32.248716	75.819994
163.319890	36.576789	75.824999
162.889758	27.994158	75.830004
161.663364	35.929458	75.835009
160.940443	31.539352	75.840014
160.404215	31.894526	75.845018
159.538269	40.549799	75.850023
159.388680	32.773995	75.855028
158.661294	31.464413	75.860033
157.980506	34.851485	75.865038
157.233101	31.793089	75.870042
156.310677	29.775011	75.875047
155.446878	26.577479	75.880052
154.405596	33.095536	75.885057
154.600911	29.796934	75.890062
154.257950	31.125818	75.895066
153.674817	38.405038	75.900071
152.854182	27.844085	75.905076
152.112732	33.085879	75.910081
151.559396	31.026297	75.915086
150.451288	36.397522	75.920090
149.415407	29.854304	75.925095
149.398061	26.614843	75.930100
148.872024	30.111283	75.935105
147.480134	23.627991	75.940110
146.436728	30.990064	75.945114
145.938016	40.003101	75.950119
145.903328	33.418508	75.955124
145.281215	29.461769	75.960129
145.125122	25.392872	75.965134
144.843068	31.979104	75.970138
143.534322	41.517126	75.975143
143.116576	32.777980	75.980148
141.904470	39.083585	75.985153
140.850622	31.477208	75.990158
140.246083	29.313829	75.995162
139.663231	42.429352	76.000167
139.836360	30.751143	76.005172
139.069046	35.795214	76.010177
138.145672	36.639485	76.015182
137.451623	29.423595	76.020186
136.801799	40.360970	76.025191
135.679810	32.390143	76.030196
135.195786	36.487019	76.035201
134.932378	33.364066	76.040206
134.489835	28.916645	76.045210
133.283467	35.284415	76.050215
132.889317	32.802058	76.055220
132.127889	42.563471	76.060225
131.722454	33.737209	76.065230
130.342917	37.191559	76.070234
129.685135	39.258205	76.075239
129.302250	28.362527	76.080244
128.715861	40.737441	76.085249
128.676324	32.868397	76.090254
127.654021	35.625535	76.095258
126.609302	39.037534	76.100263
126.502317	33.405920	76.105268
125.593616	33.126634	76.110273
124.786819	35.180774	76.115278
124.396872	31.305289	76.120282
123.616317	41.735232	76.125287
123.157692	28.391569	76.130292
121.888288	36.638099	76.135297
121.392046	39.576280	76.140302
120.844978	30.679567	76.145306
120.330624	37.621393	76.150311
119.260688	34.903026	76.155316
118.522812	38.710801	76.160321
118.312836	37.356568	76.165326
117.996381	36.918184	76.170330
116.858335	31.304336	76.175335
116.046470	27.541870	76.180340
115.285926	27.469197	76.185345
114.986580	31.967135	76.190350
114.590730	32.142236	76.195354
113.563645	36.136481	76.200359
113.224896	32.475186	76.205364
112.453134	40.785866	76.210369
111.552627	31.937634	76.215374
110.864203	37.383874	76.220378
109.841191	40.185287	76.225383
109.565058	29.272590	76.230388
109.027232	38.526835	76.235393
108.413180	32.485650	76.240398
107.389257	35.462252	76.245402
106.695629	36.487516	76.250407
106.448465	28.579048	76.255412
105.950591	35.310087	76.260417
104.914315	32.354546	76.265422
103.915324	18.570368	76.270426
103.343017	39.386093	76.275431
103.346861	23.792479	76.280436
102.720518	35.180276	76.285441
101.592753	27.757598	76.290446
100.912759	30.378153	76.295450
100.374800	27.548151	76.300455
100.018462	23.444962	76.305460
99.068723	31.328281	76.310465
98.399290	30.304368	76.315470
97.996675	24.765639	76.320474
96.869747	33.407351	76.325479
96.099074	25.404177	76.330484
95.563886	30.742401	76.335489
95.267982	35.026902	76.340494
94.935698	32.744422	76.345498
93.592986	35.257779	76.350503
92.954032	33.743302	76.355508
92.125057	40.087176	76.360513
91.857213	35.176659	76.365518
91.827899	35.279117	76.370522
90.474299	38.297263	76.375527
90.271995	29.086956	76.380532
89.153844	35.631490	76.385537
88.225528	34.612596	76.390542
87.550815	37.970332	76.395546
87.063627	40.952807	76.400551
86.912551	31.854179	76.405556
85.764749	30.319930	76.410561
85.137516	27.141468	76.415566
84.586596	26.773599	76.420570
83.918784	35.739490	76.425575
83.333774	36.450970	76.430580
82.177652	30.297548	76.435585
81.588041	30.590289	76.440590
81.275233	40.794254	76.445594
80.783032	32.901213	76.450599
80.075334	28.313165	76.455604
79.035276	38.790809	76.460609
78.539280	34.194227	76.465614
78.153172	29.641624	76.470618
77.128471	39.079178	76.475623
76.758380	23.833790	76.480628
75.400868	34.242213	76.485633
75.192880	27.511802	76.490638
75.049670	31.186898	76.495642
73.948162	34.910750	76.500647
73.391178	27.764488	76.505652
72.922576	31.037315	76.510657
72.078491	32.088162	76.515662
71.075860	22.958196	76.520666
70.147842	30.311353	76.525671
69.980147	25.454258	76.530676
69.588311	35.784364	76.535681
68.948381	30.988390	76.540686
67.732797	37.404968	76.545690
67.106195	34.631689	76.550695
67.033170	29.426754	76.555700
66.298155	34.266995	76.560705
65.433716	24.280777	76.565710
64.772566	30.698814	76.570714
64.008595	33.790091	76.575719
63.610179	28.212851	76.580724
62.314334	23.095715	76.585729
61.710111	24.691785	76.590734
61.400699	38.452832	76.595738
60.866941	34.431561	76.600743
60.561904	32.933223	76.605748
59.299532	36.348422	76.610753
58.588216	28.778921	76.615758
58.277414	34.789421	76.620762
57.603142	37.707121	76.625767
56.715608	30.730278	76.630772
56.103789	32.772265	76.635777
55.553593	35.187625	76.640782
54.991123	29.070423	76.645786
53.810773	31.628867	76.650791
53.335290	30.627650	76.655796
52.507862	28.827853	76.660801
52.231345	31.015058	76.665806
52.129297	35.262335	76.670810
50.694313	35.160058	76.675815
50.457583	37.501769	76.680820
49.870053	37.319520	76.685825
48.787972	31.654204	76.690830
48.139789	34.580360	76.695834
47.305929	35.175420	76.700839
47.216964	34.405870	76.705844
45.741533	35.234147	76.710849
45.039677	33.173048	76.715854
44.877263	28.994782	76.720858
44.128510	36.333551	76.725863
44.111727	24.863840	76.730868
43.075598	35.974806	76.735873
42.111140	38.402627	76.740878
41.611645	26.981522	76.745882
41.182867	36.678853	76.750887
40.388783	35.034592	76.755892
39.430539	33.008081	76.760897
38.828642	34.934948	76.765902
38.664092	36.471935	76.770906
37.381279	36.640286	76.775911
37.197385	35.423827	76.780916
36.043367	37.784114	76.785921
35.773057	29.384185	76.790926
35.483557	34.028792	76.795930
33.995133	39.940122	76.800935
33.986514	39.534651	76.805940
33.164234	38.748026	76.810945
31.800232	39.924393	76.815950
31.090901	32.036038	76.820954
30.803387	38.619994	76.825959
30.339086	30.665748	76.830964
30.276142	34.881556	76.835969
29.574261	34.216078	76.840974
28.302587	28.737134	76.845978
27.876059	33.854610	76.850983
27.400319	29.683745	76.855988
26.056506	31.188057	76.860993
25.147820	30.683301	76.865998
25.113516	33.434274	76.871002
24.746764	26.916854	76.876007
24.087955	28.855955	76.881012
22.657527	38.334588	76.886017
22.054064	39.049026	76.891022
21.978213	29.533131	76.896026
21.620242	41.784889	76.901031
20.437590	34.710053	76.906036
19.828573	27.824422	76.911041
18.905026	33.869583	76.916046
19.012712	32.341687	76.921050
17.747040	31.485443	76.926055
17.162932	27.568412	76.931060
16.782784	33.982638	76.936065
15.371207	34.745554	76.941070
14.781303	29.761844	76.946074
13.716498	37.807050	76.951079
13.556402	26.476898	76.956084
13.109714	30.151516	76.961089
12.927708	31.057350	76.966094
12.373632	30.989623	76.971098
11.286010	30.480298	76.976103
10.878018	23.624107	76.981108
10.454751	32.514731	76.986113
9.114594	33.668383	76.991118
8.711427	30.607167	76.996122
7.518394	35.738103	77.001127
7.312934	35.203182	77.006132
5.923614	30.752272	77.011137
5.390931	34.068447	77.016142
5.149675	33.526620	77.021147
4.470135	34.964406	77.026151
4.451014	27.049544	77.031156
3.957057	37.044282	77.036161