Thu Aug 25 16:12:35 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
0.814195	98.927685	0.000000
0.605247	94.683104	0.005005
1.087905	107.193029	0.010010
0.757354	108.254153	0.015014
0.733095	104.771573	0.020019
0.934596	109.707205	0.025024
0.848485	102.833268	0.030029
0.717736	99.718552	0.035034
0.097754	92.184783	0.040038
0.464990	83.705395	0.045043
0.622739	71.338935	0.050048
0.084609	60.201487	0.055053
-0.049094	53.565980	0.060058
-0.971388	47.345100	0.065062
-0.997446	36.529230	0.070067
-1.071431	34.981182	0.075072
-2.084074	25.794211	0.080077
-2.281277	16.713595	0.085082
-2.671626	19.723463	0.090086
-2.283730	18.776925	0.095091
-2.477963	12.973493	0.100096
-3.082459	5.348750	0.105101
-3.113413	1.968479	0.110106
-3.567651	3.953809	0.115110
-4.195738	-0.845172	0.120115
-4.307061	-0.796001	0.125120
-4.685977	2.930243	0.130125
-4.305984	-1.934939	0.135130
-5.029077	0.899272	0.140134
-5.775395	4.967819	0.145139
-5.945033	-9.084186	0.150144
-6.493590	-0.617380	0.155149
-6.040455	-8.395176	0.160154
-6.299399	-2.001711	0.165158
-6.078664	-8.759168	0.170163
-6.289271	-0.883151	0.175168
-7.297259	3.178940	0.180173
-7.189604	5.478026	0.185178
-7.530780	0.387319	0.190182
-7.467863	-4.494619	0.195187
-8.314554	-4.115093	0.200192
-8.501212	5.373849	0.205197
-8.173329	-10.157650	0.210202
-8.709332	-0.639284	0.215206
-8.650142	-8.140220	0.220211
-9.181400	-0.609431	0.225216
-9.718040	0.974359	0.230221
-9.932814	2.833584	0.235226
-10.438854	0.011806	0.240230
-10.045899	-2.080800	0.245235
-10.161065	-2.698578	0.250240
-11.325324	-0.231840	0.255245
-10.932155	1.313830	0.260250
-11.768922	5.020064	0.265254
-11.625045	2.162893	0.270259
-11.394862	3.715118	0.275264
-11.886058	2.074256	0.280269
-12.421729	-2.337407	0.285274
-13.097902	10.227470	0.290278
-13.375112	1.096124	0.295283
-12.903536	-0.733554	0.300288
-13.133385	1.922132	0.305293
-13.096494	-2.987366	0.310298
-13.720302	3.649932	0.315302
-14.100194	-6.493539	0.320307
-14.233996	5.948388	0.325312
-14.493571	2.483717	0.330317
-14.778384	2.560070	0.335322
-15.717266	5.440748	0.340326
-15.517601	3.726440	0.345331
-15.774475	4.076826	0.350336
-15.830525	10.603020	0.355341
-15.684367	11.108556	0.360346
-16.025401	10.263576	0.365350
-16.774629	-2.049306	0.370355
-17.205126	0.093655	0.375360
-17.443028	0.865010	0.380365
-16.926883	-1.401922	0.385370
-17.511043	-1.816502	0.390374
-17.433097	1.170608	0.395379
-18.088009	5.322911	0.400384
-18.504759	7.621906	0.405389
-18.572925	1.308344	0.410394
-18.791176	12.928278	0.415398
-18.998207	6.607999	0.420403
-19.690557	-0.284802	0.425408
-19.736123	5.420337	0.430413
-19.762450	-0.352451	0.435418
-20.142109	1.706614	0.440422
-20.013551	-6.956795	0.445427
-20.109239	-4.515118	0.450432
-20.959213	-6.887536	0.455437
-21.173202	-7.429718	0.460442
-21.355085	1.536455	0.465446
-21.444284	1.930171	0.470451
-21.933575	1.889867	0.475456
-22.535285	2.531566	0.480461
-22.665889	-11.124756	0.485466
-22.734355	6.308815	0.490470
-22.722572	4.250623	0.495475
-22.976626	-1.448518	0.500480
-23.041149	-3.257472	0.505485
-23.247862	-0.561118	0.510490
-24.235048	7.933290	0.515494
-24.672190	3.256252	0.520499
-24.733690	4.828870	0.525504
-24.652379	4.079066	0.530509
-24.370160	5.246652	0.535514
-24.899709	7.303894	0.540518
-25.794676	-0.828986	0.545523
-25.999795	2.329026	0.550528
-26.022797	5.123145	0.555533
-26.017239	8.444300	0.560538
-26.209891	5.741098	0.565542
-25.962745	3.547951	0.570547
-26.671251	6.943025	0.575552
-27.524762	-2.012597	0.580557
-27.022748	-0.714936	0.585562
-27.295095	4.468917	0.590566
-27.959280	-0.836932	0.595571
-28.346560	4.067537	0.600576
-28.978919	3.046743	0.605581
-28.849505	-0.266905	0.610586
-29.125028	1.203206	0.615590
-29.198272	-6.090318	0.620595
-28.986629	-4.146049	0.625600
-29.354384	8.212313	0.630605
-29.657111	5.377663	0.635610
-30.043131	5.409763	0.640614
-30.317350	3.418531	0.645619
-30.393210	-2.928624	0.650624
-31.279238	3.683321	0.655629
-31.399218	-4.852560	0.660634
-31.678147	-2.777640	0.665638
-31.674846	-3.515220	0.670643
-31.436531	-1.347340	0.675648
-31.746397	3.029308	0.680653
-32.206606	2.949648	0.685658
-32.745073	7.457028	0.690662
-32.721760	7.624308	0.695667
-32.823583	4.777160	0.700672
-33.706118	7.639520	0.705677
-34.081703	2.462457	0.710682
-34.624238	5.901128	0.715686
-34.658267	1.183076	0.720691
-34.216228	1.964952	0.725696
-34.737602	-2.632447	0.730701
-34.237367	-7.029251	0.735706
-34.608124	4.282379	0.740710
-34.882928	-4.669004	0.745715
-35.482086	-0.905088	0.750720
-35.814568	1.788827	0.755725
-36.217559	-15.425153	0.760730
-36.950242	-1.313852	0.765734
-36.966459	3.342651	0.770739
-37.123998	-0.349977	0.775744
-37.236175	4.229813	0.780749
-37.431988	2.299062	0.785754
-37.694488	0.676152	0.790758
-37.382247	-4.668794	0.795763
-37.699288	-3.707869	0.800768
-38.474875	-7.060046	0.805773
-38.491762	-5.348887	0.810778
-39.025165	-3.863680	0.815782
-39.185830	-7.944957	0.820787
-39.615965	-4.710560	0.825792
-40.295188	-10.067832	0.830797
-40.095501	-14.876284	0.835802
-40.216338	-1.759356	0.840806
-40.269385	-6.581994	0.845811
-40.116629	-7.096219	0.850816
-40.739830	-2.784371	0.855821
-40.788567	-7.870275	0.860826
-41.603905	2.308791	0.865830
-41.588497	3.499199	0.870835
-41.707163	2.420063	0.875840
-42.461669	-7.705835	0.880845
-42.637251	-3.802644	0.885850
-43.434587	-8.185958	0.890854
-43.201028	-2.749184	0.895859
-43.131333	-12.210121	0.900864
-43.314501	-4.490266	0.905869
-43.262464	-14.204699	0.910874
-43.391476	-6.803378	0.915878
-44.153480	-11.562385	0.920883
-44.133251	-7.158368	0.925888
-44.491510	-16.732580	0.930893
-44.672703	-7.390036	0.935898
-45.601291	-10.449320	0.940902
-46.084435	-3.805591	0.945907
-46.080497	-7.960116	0.950912
-46.294934	-2.835959	0.955917
-46.428613	-12.666825	0.960922
-46.717525	-2.152633	0.965926
-46.426327	-3.795862	0.970931
-46.143876	-12.584620	0.975936
-46.847046	-1.926425	0.980941
-47.138363	-6.958500	0.985946
-47.417073	-5.275919	0.990950
-47.810345	-3.736738	0.995955
-48.711611	-13.627664	1.000960
-49.159927	-5.701749	1.005965
-49.296270	-14.700132	1.010970
-49.033087	-5.101349	1.015974
-48.370130	-11.899622	1.020979
-48.780163	-10.474874	1.025984
-49.585851	-3.888173	1.030989
-50.016309	-4.889981	1.035994
-50.687747	-5.816064	1.040998
-50.840581	-11.183048	1.046003
-50.790573	-13.630040	1.051008
-50.905023	-4.272642	1.056013
-50.574453	-18.463123	1.061018
-51.349441	-7.910736	1.066022
-51.907774	-13.059158	1.071027
-51.887401	-6.586075	1.076032
-52.137555	-8.865813	1.081037
-52.127001	-16.824193	1.086042
-52.886977	-9.070908	1.091046
-53.424337	-14.374475	1.096051
-53.106049	-14.079409	1.101056
-53.637704	-7.010467	1.106061
-53.714666	-10.918197	1.111066
-54.010197	-6.857008	1.116070
-53.774751	-4.577948	1.121075
-54.381759	-12.208611	1.126080
-54.633977	-5.423897	1.131085
-54.658708	-6.663284	1.136090
-54.897748	8.047717	1.141094
-55.275178	-6.854409	1.146099
-55.782222	-6.569227	1.151104
-56.501577	-8.038293	1.156109
-56.296968	-3.441704	1.161114
-56.296446	-6.548494	1.166118
-56.183308	-8.201787	1.171123
-56.902937	-11.904414	1.176128
-57.691382	-6.095533	1.181133
-57.770198	-5.222554	1.186138
-58.118824	-2.516619	1.191142
-57.987257	-1.176734	1.196147
-58.029264	-3.644111	1.201152
-58.050024	4.746324	1.206157
-58.134861	-2.263810	1.211162
-58.807222	-9.428653	1.216166
-59.103070	-9.002557	1.221171
-59.383423	-4.643190	1.226176
-60.582671	-2.307006	1.231181
-60.118501	-13.553993	1.236186
-60.652298	-2.802115	1.241190
-60.859056	-2.507037	1.246195
-60.642870	-9.716195	1.251200
-61.245265	-5.746127	1.256205
-60.733800	-9.173421	1.261210
-60.768574	-5.751038	1.266214
-61.456902	-12.457799	1.271219
-61.847232	-9.033487	1.276224
-62.366210	-7.983972	1.281229
-62.302780	-13.283601	1.286234
-62.941436	-3.628931	1.291238
-63.589390	-7.080198	1.296243
-63.576607	-6.857485	1.301248
-63.911511	4.204917	1.306253
-63.805000	-3.698901	1.311258
-63.854025	0.374284	1.316262
-64.033079	-7.380383	1.321267
-63.755762	-0.596384	1.326272
-64.400746	3.728371	1.331277
-64.763595	-4.731487	1.336282
-65.103054	-5.336266	1.341286
-65.440108	-3.467373	1.346291
-66.070924	1.671408	1.351296
-66.811580	6.887512	1.356301
-66.375213	-1.273636	1.361306
-66.056160	-2.766206	1.366310
-66.599729	-4.791162	1.371315
-66.316973	-1.393222	1.376320
-67.031503	4.492665	1.381325
-67.579297	-0.859889	1.386330
-67.945446	-2.707001	1.391334
-67.823258	-0.834137	1.396339
-68.020002	2.803451	1.401344
-68.645846	2.085360	1.406349
-68.767420	0.642849	1.411354
-69.225452	-0.614064	1.416358
-69.186492	-8.396564	1.421363
-69.111031	-4.339723	1.426368
-69.767039	-1.927307	1.431373
-69.717246	-3.953489	1.436378
-70.619908	2.866708	1.441382
-70.957587	-8.776656	1.446387
-70.997629	1.116412	1.451392
-71.410371	0.127648	1.456397
-70.882206	2.882859	1.461402
-71.122497	0.209270	1.466406
-71.606582	1.579185	1.471411
-72.114308	-4.826846	1.476416
-72.888082	-3.813336	1.481421
-72.398926	-0.817896	1.486426
-72.751408	-3.201822	1.491430
-72.649992	-7.779743	1.496435
-72.758174	-5.579718	1.501440
-73.631469	-0.905979	1.506445
-73.621806	-3.226428	1.511450
-73.644111	2.041630	1.516454
-74.172558	-7.259145	1.521459
-74.829515	-3.555773	1.526464
-75.323506	2.861868	1.531469
-75.306893	-7.362706	1.536474
-75.404190	-10.001751	1.541478
-75.456375	-4.317727	1.546483
-75.608012	-2.825898	1.551488
-75.700385	-1.175678	1.556493
-75.855836	-10.908218	1.561498
-76.377987	-6.438197	1.566502
-76.843176	0.655135	1.571507
-76.542276	-9.769007	1.576512
-77.678515	5.373639	1.581517
-77.781012	0.068369	1.586522
-78.097982	-4.336428	1.591526
-78.152990	-1.572096	1.596531
-78.130016	-6.308568	1.601536
-78.399725	-3.684601	1.606541
-78.216584	-7.186999	1.611546
-79.121476	3.743252	1.616550
-79.485253	-4.732278	1.621555
-79.514094	2.254717	1.626560
-80.179820	1.682081	1.631565
-79.882662	-7.912574	1.636570
-79.809343	-1.723033	1.641574
-80.532025	-4.283068	1.646579
-80.896110	-6.782234	1.651584
-81.219323	7.524339	1.656589
-80.931085	5.698075	1.661594
-81.262226	3.940390	1.666598
-81.657383	1.246776	1.671603
-82.313457	-4.262816	1.676608
-82.713605	-2.754194	1.681613
-82.382524	-0.293968	1.686618
-82.292534	-0.668646	1.691622
-82.664157	1.632771	1.696627
-82.985057	-8.178249	1.701632
-83.987318	0.660205	1.706637
-83.932612	-8.627540	1.711642
-84.127847	2.093436	1.716646
-84.035510	-3.191743	1.721651
-84.146805	-2.892640	1.726656
-84.847474	-3.814140	1.731661
-85.476736	-4.443110	1.736666
-85.880364	-5.816114	1.741670
-85.835259	-7.898507	1.746675
-86.022821	-12.519730	1.751680
-85.759580	-1.854779	1.756685
-85.768955	-11.303323	1.761690
-86.690877	-8.659416	1.766694
-86.992542	0.917142	1.771699
-86.927655	-9.669333	1.776704
-87.284629	-8.369956	1.781709
-86.947952	-4.692567	1.786714
-87.796644	-6.248931	1.791718
-88.103412	1.537747	1.796723
-88.131848	-6.847958	1.801728
-88.722253	4.162729	1.806733
-88.203765	-10.670966	1.811738
-88.981001	-3.032032	1.816742
-89.640296	3.307108	1.821747
-89.299181	2.813987	1.826752
-89.893840	4.989001	1.831757
-89.853821	2.363239	1.836762
-90.424318	-1.365918	1.841766
-91.243940	-0.623631	1.846771
-91.141713	-4.486673	1.851776
-91.364155	7.750839	1.856781
-90.990135	4.421009	1.861786
-91.307545	0.085884	1.866790
-91.533093	8.037008	1.871795
-91.345539	7.039603	1.876800
-92.301728	-1.203894	1.881805
-92.578391	-0.056305	1.886810
-92.515916	-6.463096	1.891814
-93.150542	-1.026327	1.896819
-93.649413	3.677330	1.901824
-94.130905	0.617595	1.906829
-93.949882	-2.748431	1.911834
-94.572248	12.240933	1.916838
-94.434812	11.431715	1.921843
-93.974836	4.769645	1.926848
-94.485713	1.141877	1.931853
-94.857963	2.601836	1.936858
-95.677745	-2.293646	1.941862
-95.632253	1.913425	1.946867
-95.663387	2.351826	1.951872
-95.916189	-1.585298	1.956877
-95.787491	-0.985281	1.961882
-96.830997	4.575671	1.966886
-97.030109	1.012947	1.971891
-97.477722	-2.953763	1.976896
-97.473631	13.149153	1.981901
-97.341690	8.117193	1.986906
-97.359065	2.460065	1.991910
-98.205520	2.304889	1.996915
-98.556403	-2.068771	2.006912
-97.781394	0.312528	2.016909
-97.440275	6.734232	2.026906
-97.508231	2.953208	2.036902
-96.829069	-0.507730	2.046899
-96.000843	1.839888	2.056896
-95.326110	1.027922	2.066893
-94.654328	1.831995	2.076890
-94.829421	3.193253	2.086886
-94.527963	-0.709011	2.096883
-93.843829	4.353812	2.106880
-93.415977	0.124465	2.116877
-92.567262	0.346449	2.126874
-91.999954	-3.945930	2.136870
-91.070774	3.524035	2.146867
-90.510126	0.547334	2.156864
-90.493750	-6.956392	2.166861
-90.470799	0.918499	2.176858
-90.204208	5.847179	2.186854
-89.492271	6.169791	2.196851
-88.011258	2.652899	2.206848
-87.621975	0.941659	2.216845
-87.723712	-5.856148	2.226842
-87.844747	-5.159094	2.236838
-86.508081	-3.524705	2.246835
-85.753784	0.050932	2.256832
-85.519740	2.732408	2.266829
-85.365155	-3.408649	2.276826
-84.270558	1.482153	2.286822
-83.829682	4.707759	2.296819
-83.725457	2.977829	2.306816
-83.580996	-2.645291	2.316813
-82.585341	-0.628015	2.326810
-82.015388	-1.144796	2.336806
-81.128979	3.588561	2.346803
-80.658475	2.916303	2.356800
-81.075512	2.497157	2.366797
-80.159968	5.382291	2.376794
-79.499611	0.185181	2.386790
-79.264665	-0.209415	2.396787
-78.405610	-0.378689	2.406784
-78.121244	-4.366973	2.416781
-77.732594	-0.483785	2.426778
-77.189497	4.689838	2.436774
-76.103119	7.877656	2.446771
-75.920181	6.610562	2.456768
-75.625384	2.360882	2.466765
-75.732262	5.187645	2.476762
-74.461374	0.613959	2.486758
-73.791125	2.485821	2.496755
-73.384779	2.957688	2.506752
-73.041045	6.166839	2.516749
-72.616558	-0.035518	2.526746
-71.929530	5.400655	2.536742
-71.456744	0.210761	2.546739
-71.177881	7.031862	2.556736
-70.526828	-0.732875	2.566733
-69.686735	6.424771	2.576730
-69.633234	4.474708	2.586726
-69.341955	5.990971	2.596723
-68.292784	8.598578	2.606720
-68.193705	1.946697	2.616717
-67.495599	6.712730	2.626714
-66.947248	5.727333	2.636710
-66.630687	10.746388	2.646707
-65.717423	11.895929	2.656704
-65.517451	9.831048	2.666701
-65.019758	5.270810	2.676698
-64.294836	4.694902	2.686694
-63.993323	5.712218	2.696691
-63.929559	7.479541	2.706688
-63.187725	2.051086	2.716685
-62.474560	3.121107	2.726682
-61.422585	3.628025	2.736678
-61.549942	5.137026	2.746675
-60.853061	8.753342	2.756672
-60.809185	2.889388	2.766669
-60.070119	5.377693	2.776666
-59.450860	5.068599	2.786662
-58.917362	5.086554	2.796659
-57.926494	-3.447349	2.806656
-57.950797	0.475203	2.816653
-57.815340	-1.262787	2.826650
-57.297509	2.638174	2.836646
-56.778700	0.083012	2.846643
-56.141608	9.394894	2.856640
-55.536432	4.450349	2.866637
-54.745488	8.346532	2.876634
-54.293951	9.910545	2.886630
-54.192060	5.371143	2.896627
-53.624500	14.529197	2.906624
-52.736257	7.487564	2.916621
-52.532267	7.069310	2.926618
-52.204092	3.067824	2.936614
-51.308432	4.590757	2.946611
-51.114314	9.974288	2.956608
-50.274207	9.120574	2.966605
-49.650060	13.901367	2.976602
-49.477126	9.949547	2.986598
-49.326920	5.114305	2.996595
-48.316226	15.596757	3.006592
-48.217575	10.250073	3.016589
-47.461290	3.713791	3.026586
-46.875933	5.209319	3.036582
-46.634659	11.117652	3.046579
-45.448501	5.391494	3.056576
-45.149964	2.120078	3.066573
-45.320434	6.803632	3.076570
-44.755333	5.270751	3.086566
-44.106678	9.987516	3.096563
-43.708680	15.481655	3.106560
-42.789514	8.045537	3.116557
-42.529378	8.423106	3.126554
-41.375112	7.960491	3.136550
-41.172675	9.382972	3.146547
-41.182012	5.038395	3.156544
-40.659620	7.418101	3.166541
-39.789065	2.615708	3.176538
-39.873117	3.950030	3.186534
-39.066257	8.112984	3.196531
-38.468594	7.145205	3.206528
-37.872483	6.066795	3.216525
-37.094687	1.646402	3.226522
-36.878225	10.000995	3.236518
-36.578483	12.713363	3.246515
-35.847036	6.168301	3.256512
-35.355120	2.372409	3.266509
-35.127746	2.853313	3.276506
-34.125403	3.152601	3.286502
-33.967533	6.828033	3.296499
-33.758520	0.909694	3.306496
-32.905136	1.545935	3.316493
-32.795621	8.171829	3.326490
-31.580086	1.364018	3.336486
-31.548640	1.061498	3.346483
-31.225060	4.391018	3.356480
-29.898215	7.572842	3.366477
-29.461595	-1.682006	3.376474
-29.706836	1.033390	3.386470
-29.386289	0.137542	3.396467
-28.427781	4.270399	3.406464
-27.862985	7.951764	3.416461
-27.308673	4.066899	3.426458
-27.027671	-2.914428	3.436454
-26.542165	4.865819	3.446451
-25.588663	0.373546	3.456448
-25.248206	3.013010	3.466445
-24.968744	-1.098051	3.476442
-24.670860	-6.434767	3.486438
-24.211381	-1.301890	3.496435
-22.991406	1.142744	3.506432
-22.725404	1.642939	3.516429
-22.359435	-2.101541	3.526426
-22.077403	-0.615505	3.536422
-21.182121	11.171160	3.546419
-20.784240	4.117664	3.556416
-20.704887	8.641699	3.566413
-19.907474	5.893997	3.576410
-19.679858	-3.515002	3.586406
-18.741620	2.847994	3.596403
-18.471072	4.782489	3.606400
-18.068066	1.010032	3.616397
-16.885195	4.784621	3.626394
-16.628116	3.404541	3.636390
-16.200066	1.908975	3.646387
-16.268363	5.616677	3.656384
-16.008889	5.028172	3.666381
-14.657441	-4.737480	3.676378
-13.970322	0.074629	3.686374
-13.774086	2.153815	3.696371
-13.722855	4.559831	3.706368
-12.602137	9.094928	3.716365
-12.145677	3.584476	3.726362
-12.192004	7.767074	3.736358
-11.765493	10.655984	3.746355
-11.027094	8.633452	3.756352
-10.241170	2.121038	3.766349
-9.666567	3.890684	3.776346
-9.797933	1.975922	3.786342
-8.806574	1.760583	3.796339
-8.190980	0.739312	3.806336
-8.040553	-2.328332	3.816333
-6.998322	-1.053273	3.826330
-6.782725	5.023810	3.836326
-6.485334	3.089385	3.846323
-5.962258	-2.149569	3.856320
-5.443220	-0.596130	3.866317
-5.117021	8.099233	3.876314
-4.527064	12.023746	3.886310
-3.995842	16.898301	3.896307
-3.700602	28.503399	3.906304
-3.080132	33.427331	3.916301
-2.435505	35.537635	3.926298
-2.473039	41.442150	3.936294
-2.208295	62.111976	3.946291
-1.588344	86.324806	3.956288
-0.766472	97.695380	3.966285
0.005851	117.395585	3.976282
0.000000	130.182499	3.981286
0.149116	134.224671	3.986291
0.119943	149.570466	3.991296
0.439072	147.502066	3.996301
0.542273	151.858322	4.001306
0.571569	160.212517	4.006310
0.821006	155.434188	4.011315
0.805241	165.396316	4.016320
0.820318	170.041633	4.021325
1.023678	172.544046	4.026330
1.148340	179.200177	4.031334
1.288349	170.810135	4.036339
0.781692	173.237133	4.041344
1.125176	164.897472	4.046349
1.100082	168.441760	4.051354
0.838669	169.254771	4.056358
1.277023	173.495244	4.061363
1.088720	166.969491	4.066368
0.731754	159.995600	4.071373
1.075857	172.492479	4.076378
1.003093	179.217508	4.081382
0.950967	174.885061	4.086387
1.088873	180.988620	4.091392
0.997415	175.592978	4.096397
1.202690	164.620561	4.101402
1.158615	170.550148	4.106406
1.452775	176.629223	4.111411
1.241823	175.536061	4.116416
1.228230	174.510052	4.121421
1.215960	168.051630	4.126426
1.101307	171.110075	4.131430
1.538788	173.240445	4.136435
1.376555	171.797961	4.141440
1.580930	174.629248	4.146445
1.413257	174.636628	4.151450
1.223160	159.053262	4.156454
1.414154	162.285280	4.161459
0.906769	165.310345	4.166464
0.963772	168.832279	4.171469
1.279659	177.537050	4.176474
1.555881	173.842860	4.181478
1.436105	172.143785	4.186483
1.023180	175.283766	4.191488
1.307615	178.308156	4.196493
1.274960	176.184139	4.201498
1.265455	174.698743	4.206502
1.426462	179.821074	4.211507
1.375466	176.016801	4.216512
1.363524	183.690927	4.221517
1.203833	180.808525	4.226522
1.227129	176.945154	4.231526
1.445615	178.344202	4.236531
1.096253	179.522174	4.241536
1.347380	182.937764	4.246541
1.496931	193.184055	4.251546
1.342373	192.680010	4.256550
1.538201	195.031745	4.261555
1.546818	201.237827	4.266560
1.713622	201.626237	4.271565
1.858667	200.309614	4.276570
1.525801	200.643436	4.281574
1.882739	195.617296	4.286579
1.351816	187.420957	4.291584
1.729063	193.426908	4.296589
1.742633	194.443609	4.301594
1.860646	188.252671	4.306598
1.670583	179.885868	4.311603
1.305993	178.728192	4.316608
1.785851	187.622413	4.321613
1.964825	199.034696	4.326618
1.551797	188.874157	4.331622
1.648085	184.983529	4.336627
1.535412	203.800467	4.341632
1.642572	210.740929	4.346637
1.730039	215.061701	4.351642
1.251454	206.993194	4.356646
1.715072	208.717673	4.361651
1.863445	220.463798	4.366656
1.985860	209.112027	4.371661
1.962522	214.930811	4.376666
1.709885	210.405143	4.381670
1.826299	204.410604	4.386675
1.728317	207.991632	4.391680
1.387496	206.017137	4.396685
1.615798	210.075393	4.401690
1.650433	206.251368	4.406694
1.680321	203.351913	4.411699
1.736975	218.288847	4.416704
1.962585	231.158677	4.421709
2.132901	235.026706	4.426714
2.089515	227.788518	4.431718
2.008214	213.864865	4.436723
2.300750	228.768013	4.441728
2.047419	213.627947	4.446733
1.886530	215.282595	4.451738
1.818616	213.594373	4.456742
2.312636	208.954880	4.461747
2.089524	219.749964	4.466752
2.123707	205.257725	4.471757
2.129883	213.773756	4.476762
2.051407	211.131726	4.481766
1.917624	204.442391	4.486771
2.235012	212.719833	4.491776
2.266606	220.766808	4.496781
2.448317	210.845268	4.501786
2.043848	223.858109	4.506790
1.845824	211.911132	4.511795
2.206580	227.325614	4.516800
2.322088	220.144791	4.521805
2.454924	221.171281	4.526810
1.939066	216.490699	4.531814
2.286050	217.657644	4.536819
2.433030	225.332199	4.541824
2.529724	219.343908	4.546829
2.424418	214.852103	4.551834
2.488097	215.310456	4.556838
2.669336	206.546938	4.561843
2.525603	205.610922	4.566848
2.193179	206.343311	4.571853
2.255789	204.653622	4.576858
2.201320	211.866184	4.581862
2.393428	201.082471	4.586867
2.067759	205.882428	4.591872
2.368028	206.604270	4.596877
2.014872	203.793306	4.601882
1.941990	209.467989	4.606886
2.470892	208.151333	4.611891
2.596912	222.166232	4.616896
2.313415	232.850561	4.621901
2.641678	227.310044	4.626906
2.633550	233.142270	4.631910
2.673830	230.247510	4.636915
2.184350	224.676932	4.641920
2.447477	237.743371	4.646925
2.626269	237.304155	4.651930
2.517078	236.081148	4.656934
2.963511	225.672028	4.661939
2.487184	225.942905	4.666944
2.672549	232.504123	4.671949
2.708560	223.143249	4.676954
2.314548	207.098241	4.681958
2.703724	222.900576	4.686963
2.617634	232.914889	4.691968
2.693070	232.577289	4.696973
2.380108	225.463599	4.701978
2.462567	235.299643	4.706982
2.561262	242.668555	4.711987
2.588573	247.280337	4.716992
2.605651	240.206679	4.721997
2.838746	242.612693	4.727002
2.735554	245.036596	4.732006
2.852508	239.250771	4.737011
2.621690	240.593672	4.742016
2.666921	231.867271	4.747021
2.883405	231.273451	4.752026
2.605486	234.873186	4.757030
3.050067	234.813109	4.762035
2.804496	238.657715	4.767040
3.180122	236.767116	4.772045
2.864340	233.576964	4.777050
2.713938	235.688720	4.782054
2.965885	228.467534	4.787059
2.699824	236.213137	4.792064
3.032992	235.651655	4.797069
3.120883	241.054383	4.802074
2.734731	246.793981	4.807078
2.802064	238.658907	4.812083
2.442638	243.027560	4.817088
3.050359	244.175800	4.822093
2.857652	242.810852	4.827098
2.646078	246.602676	4.832102
3.141097	238.470194	4.837107
2.734584	243.137293	4.842112
2.675611	243.282666	4.847117
2.785338	242.734047	4.852122
2.952256	243.324923	4.857126
3.419781	246.459844	4.862131
2.885395	243.465295	4.867136
3.115829	240.262325	4.872141
2.778141	244.020124	4.877146
3.084939	253.118666	4.882150
3.222183	253.261770	4.887155
3.403135	260.076792	4.892160
3.160373	255.087652	4.897165
2.648318	252.013671	4.902170
2.956142	255.202090	4.907174
3.444899	255.736212	4.912179
3.380912	267.196099	4.917184
3.371434	266.299156	4.922189
2.933259	256.917648	4.927194
2.970273	265.912933	4.932198
3.221192	262.248000	4.937203
3.337027	274.344112	4.942208
3.469751	269.596696	4.947213
3.016771	263.463558	4.952218
3.017607	269.158348	4.957222
3.400520	261.268050	4.962227
3.152417	272.532159	4.967232
3.731323	266.803660	4.972237
3.099812	267.949914	4.977242
3.155369	276.293721	4.982246
3.502031	269.965687	4.987251
3.181839	267.019831	4.992256
3.224394	272.220861	4.997261
3.723672	269.504117	5.002266
2.974007	273.772568	5.007270
3.308234	271.736590	5.012275
3.413580	275.450290	5.017280
3.183594	269.984574	5.022285
3.624594	276.660780	5.027290
3.469094	277.393925	5.032294
3.395325	276.912021	5.037299
3.361725	275.177287	5.042304
3.093303	276.285634	5.047309
3.161288	285.921491	5.052314
3.207304	291.700959	5.057318
3.940968	292.158744	5.062323
3.596322	298.255692	5.067328
3.636420	293.152618	5.072333
3.674586	304.131444	5.077338
3.515961	299.970679	5.082342
3.870502	296.529952	5.087347
3.281311	301.124447	5.092352
3.409208	296.172132	5.097357
3.490990	296.431495	5.102362
3.709515	297.757780	5.107366
3.891597	295.884846	5.112371
3.397296	296.734352	5.117376
3.561922	291.409283	5.122381
3.859836	300.275120	5.127386
3.679301	302.641546	5.132390
3.720430	298.262819	5.137395
3.495864	299.743952	5.142400
3.568028	289.450385	5.147405
3.286692	289.807772	5.152410
3.604382	291.270382	5.157414
3.632587	290.449792	5.162419
3.247559	297.154190	5.167424
3.487662	303.118390	5.172429
3.929533	318.985321	5.177434
3.884992	314.699108	5.182438
4.123608	311.422076	5.187443
3.944692	311.836184	5.192448
3.932539	312.002696	5.197453
3.757215	311.017839	5.202458
4.077020	317.039160	5.207462
4.197210	318.713053	5.212467
3.699704	316.541630	5.217472
3.984018	310.814982	5.222477
3.892214	315.110082	5.227482
3.407921	322.734890	5.232486
3.871859	314.398432	5.237491
3.686866	323.751239	5.242496
3.560745	317.380205	5.247501
4.304303	323.771738	5.252506
4.041170	325.872693	5.257510
3.852989	316.309613	5.262515
3.770415	315.433612	5.267520
4.066626	325.134972	5.272525
4.484512	322.532215	5.277530
4.123686	319.836331	5.282534
4.299912	315.531346	5.287539
4.150035	330.307742	5.292544
3.829070	320.977439	5.297549
3.912213	311.656591	5.302554
4.091728	314.276658	5.307558
4.333084	310.878972	5.312563
3.946926	324.341441	5.317568
4.106154	328.954721	5.322573
4.428835	338.870245	5.327578
4.463768	333.593958	5.332582
4.439739	327.507486	5.337587
4.047621	333.599229	5.342592
4.182051	317.724428	5.347597
4.342807	319.496371	5.352602
4.148300	327.730684	5.357606
4.285843	333.919775	5.362611
4.375646	340.214426	5.367616
4.284323	345.904698	5.372621
4.444224	350.030652	5.377626
4.487713	342.861064	5.382630
4.331962	326.949462	5.387635
4.375396	347.323994	5.392640
4.341830	336.091497	5.397645
4.648956	340.466468	5.402650
4.386056	339.099856	5.407654
4.215196	328.758922	5.412659
4.347504	346.490405	5.417664
4.405223	347.724829	5.422669
4.662389	344.644205	5.427674
4.316333	342.414247	5.432678
4.644421	344.087206	5.437683
4.588630	353.514699	5.442688
4.810827	349.427134	5.447693
4.372621	344.174357	5.452698
4.329911	346.085752	5.457702
4.672023	340.501901	5.462707
4.551545	344.918562	5.467712
4.505774	346.950661	5.472717
4.487858	350.927304	5.477722
4.799179	349.698514	5.482726
4.967110	341.408423	5.487731
4.482695	335.770576	5.492736
4.604419	326.873953	5.497741
4.688294	339.667991	5.502746
4.343573	342.911212	5.507750
4.781329	340.435055	5.512755
4.462858	347.331526	5.517760
4.699358	340.144353	5.522765
4.484478	335.970247	5.527770
4.525810	346.616404	5.532774
4.524168	336.691885	5.537779
4.779132	346.586384	5.542784
4.703186	342.741691	5.547789
4.512804	346.153722	5.552794
4.363641	350.502111	5.557798
4.905401	347.057351	5.562803
4.728549	350.628617	5.567808
4.894416	341.750381	5.572813
4.707069	337.806083	5.577818
4.577515	341.085194	5.582822
4.780500	341.344550	5.587827
4.787143	367.574752	5.592832
4.864422	370.840445	5.597837
5.304763	371.125888	5.602842
5.018651	366.029611	5.607846
4.902566	347.514285	5.612851
4.513522	349.600170	5.617856
5.124953	362.631110	5.622861
4.593036	366.906594	5.627866
4.942622	376.166177	5.632870
5.274649	367.821888	5.637875
4.867133	376.630610	5.642880
5.132803	371.757930	5.647885
5.119896	369.788987	5.652890
4.948399	370.578427	5.657894
4.993261	367.951851	5.662899
5.298785	369.318295	5.667904
5.047663	380.829722	5.672909
5.094588	374.504322	5.677914
5.072868	378.585972	5.682918
5.116900	367.758919	5.687923
5.256057	372.223493	5.692928
5.214093	379.070325	5.697933
5.334696	373.919812	5.702938
5.190566	373.344524	5.707942
5.366942	367.024154	5.712947
4.991394	363.979386	5.717952
5.115787	370.964667	5.722957
5.290669	374.278344	5.727962
5.200150	371.502133	5.732966
5.471001	362.484048	5.737971
5.108584	374.541266	5.742976
5.132720	376.287164	5.747981
5.383640	373.267626	5.752986
5.192665	377.435908	5.757990
5.145616	371.735849	5.762995
5.055528	370.883170	5.768000
5.258853	374.964360	5.773005
5.174582	375.123190	5.778010
5.103253	383.689411	5.783014
4.972428	367.435339	5.788019
5.302388	369.440208	5.793024
5.333150	374.864583	5.798029
5.425270	382.098539	5.803034
5.278932	374.151909	5.808038
5.354822	374.193893	5.813043
5.266550	374.210977	5.818048
5.278619	371.798350	5.823053
5.544189	387.275343	5.828058
5.411426	388.827522	5.833062
5.710231	392.915903	5.838067
5.376488	398.634683	5.843072
5.549263	386.657964	5.848077
5.667514	386.854666	5.853082
5.415540	396.853932	5.858086
5.659751	397.179598	5.863091
5.577356	399.372469	5.868096
5.484213	392.198959	5.873101
5.999867	395.535177	5.878106
5.979826	387.470674	5.883110
5.497118	381.842036	5.888115
5.216744	382.414413	5.893120
5.119476	382.847367	5.898125
5.746888	387.067761	5.903130
5.412015	398.475261	5.908134
5.466177	401.896444	5.913139
5.252316	401.468125	5.918144
5.177830	403.919191	5.923149
5.693429	399.646435	5.928154
5.529165	411.261333	5.933158
5.863482	399.196019	5.938163
5.602243	406.077218	5.943168
5.497317	408.109101	5.948173
5.708765	404.519928	5.953178
5.674545	420.955101	5.958182
6.044874	424.956351	5.963187
5.907785	426.585143	5.968192
5.599572	416.822512	5.973197
5.661370	418.043646	5.978202
6.023086	423.836969	5.983206
6.035751	420.876900	5.988211
6.077766	425.872411	5.993216
5.742769	422.523880	5.998221
5.811938	408.146220	6.003226
5.529098	410.648915	6.008230
5.772698	420.769867	6.013235
5.973661	434.507430	6.018240
5.910311	433.115871	6.023245
6.195410	437.399404	6.028250
5.892156	432.720254	6.033254
5.845627	406.047124	6.038259
5.966141	414.576974	6.043264
5.749340	409.096494	6.048269
5.675611	407.674925	6.053274
5.652754	423.247762	6.058278
5.943032	427.460876	6.063283
5.927120	432.142755	6.068288
6.023206	435.946526	6.073293
6.196312	417.521861	6.078298
5.509629	415.832492	6.083302
5.765910	413.881479	6.088307
5.863511	424.512538	6.093312
6.125955	423.095244	6.098317
6.067132	404.292471	6.103322
5.514936	410.542202	6.108326
5.764283	407.241325	6.113331
5.940519	413.848334	6.118336
5.523677	415.372258	6.123341
6.275550	416.937695	6.128346
5.751144	414.115563	6.133350
5.898446	397.789410	6.138355
5.670280	407.968454	6.143360
5.848148	415.812262	6.148365
6.097117	422.483809	6.153370
5.762509	416.642126	6.158374
5.923767	401.981117	6.163379
6.040760	407.265438	6.168384
5.843686	398.766750	6.173389
5.582030	391.265295	6.178394
5.425378	422.377624	6.183398
6.198707	424.110546	6.188403
5.945957	427.516546	6.193408
6.111772	416.815918	6.198413
5.892304	417.742593	6.203418
5.657931	408.398677	6.208422
5.852384	406.650345	6.213427
5.874875	406.112226	6.218432
5.861464	400.650501	6.223437
5.828297	402.335776	6.228442
5.687076	401.728393	6.233446
6.065284	408.401832	6.238451
5.752455	417.085005	6.243456
5.964861	417.795312	6.248461
6.226221	402.900315	6.253466
6.148936	411.590872	6.258470
6.173249	409.979932	6.263475
5.864299	415.191785	6.268480
5.770141	408.334810	6.273485
5.692029	404.961851	6.278490
5.618141	406.859155	6.283494
5.889369	402.874629	6.288499
5.772864	399.773448	6.293504
5.691563	406.208830	6.298509
5.489986	394.287597	6.303514
5.584673	407.532415	6.308518
5.686189	420.409171	6.313523
5.923795	425.370872	6.318528
5.957354	429.061049	6.323533
6.063321	422.318248	6.328538
5.832729	428.989005	6.333542
6.214043	427.309472	6.338547
5.837240	411.337515	6.343552
5.486109	411.538157	6.348557
5.993981	423.794413	6.353562
5.693748	425.717692	6.358566
5.955584	419.943910	6.363571
5.984837	430.101616	6.368576
5.902338	423.714218	6.373581
5.841865	413.998195	6.378586
5.839539	420.873634	6.383590
6.198666	424.129977	6.388595
5.706387	412.564334	6.393600
5.443947	409.631553	6.398605
5.716702	411.167654	6.403610
5.973281	425.124290	6.408614
5.831359	429.560150	6.413619
6.103489	434.491134	6.418624
5.969569	431.497083	6.423629
6.064259	411.088337	6.428634
5.889299	412.587017	6.433638
5.834497	407.818325	6.438643
5.668195	404.649014	6.443648
5.754818	408.302399	6.448653
5.947572	408.664601	6.453658
5.783957	417.694562	6.458662
5.706795	414.780207	6.463667
5.791761	416.820305	6.468672
6.004586	433.194635	6.473677
6.147084	422.617882	6.478682
5.703604	422.763390	6.483686
5.700696	405.296480	6.488691
5.789910	421.987567	6.493696
6.011403	430.027029	6.498701
6.145311	416.699100	6.503706
5.785078	411.740976	6.508710
5.808018	403.017984	6.513715
5.710724	411.218120	6.518720
5.651692	418.124590	6.523725
5.948356	418.780566	6.528730
6.114602	427.151394	6.533734
5.849728	416.654293	6.538739
5.641908	402.857886	6.543744
6.113861	421.153172	6.548749
5.865487	407.663679	6.553754
5.529434	410.285445	6.558758
5.909018	409.061775	6.563763
6.078242	424.550732	6.568768
5.992270	413.965488	6.573773
5.996316	400.164362	6.578778
5.616799	401.625488	6.583782
5.669432	394.384843	6.588787
5.715499	407.137396	6.593792
5.903095	426.388422	6.598797
6.190742	421.075677	6.603802
5.606296	406.522013	6.608806
5.792319	410.915977	6.613811
6.123779	418.280130	6.618816
6.069418	414.558592	6.623821
5.850260	411.650667	6.628826
5.636785	409.808059	6.633830
5.785099	409.247062	6.638835
5.863134	414.429918	6.643840
5.639558	407.283167	6.648845
5.855233	412.814624	6.653850
5.912166	432.769515	6.658854
6.069374	429.638098	6.663859
5.677266	420.271432	6.668864
5.962332	429.977760	6.673869
6.016059	420.123614	6.678874
5.631024	418.902685	6.683878
5.715495	416.143343	6.688883
5.842987	424.434818	6.693888
6.024872	431.746480	6.698893
6.033751	421.997440	6.703898
5.915272	416.628104	6.708902
5.590524	415.286996	6.713907
5.569082	416.454732	6.718912
5.752225	435.611550	6.723917
5.884188	432.174034	6.728922
5.623653	430.145804	6.733926
5.514584	432.105572	6.738931
5.481136	433.281517	6.743936
5.542873	440.412688	6.748941
5.794733	431.441838	6.753946
5.740317	433.829650	6.758950
5.829356	430.294453	6.763955
6.078336	423.655796	6.768960
5.871302	434.435834	6.773965
5.934191	425.760357	6.778970
5.651290	438.029790	6.783974
6.300388	419.027495	6.788979
6.020729	433.599679	6.793984
5.800756	430.606456	6.798989
6.296067	424.476544	6.803994
6.197936	438.422328	6.808998
5.989850	426.445144	6.814003
5.770479	433.177421	6.819008
5.805649	435.788484	6.824013
6.436704	425.438909	6.829018
5.812953	435.268653	6.834022
5.992857	422.968083	6.839027
5.694038	414.134145	6.844032
5.682834	419.688497	6.849037
6.193703	428.309055	6.854042
5.958880	419.651753	6.859046
6.004224	408.343570	6.864051
5.911544	407.102145	6.869056
5.694593	403.637043	6.874061
5.982356	403.449674	6.879066
5.650036	400.319031	6.884070
6.042451	407.512274	6.889075
6.029805	400.949420	6.894080
5.546509	406.783386	6.899085
6.188527	397.226228	6.904090
5.894218	402.733182	6.909094
5.968129	403.091858	6.914099
5.806286	401.076643	6.919104
5.697353	409.408319	6.924109
6.189492	386.472712	6.929114
5.554816	400.366490	6.934118
5.688174	397.994968	6.939123
5.755260	399.572783	6.944128
5.736409	391.916224	6.949133
5.989324	392.838487	6.954138
5.299029	399.445217	6.959142
5.927246	401.627989	6.964147
6.292959	414.646847	6.969152
6.019238	414.126664	6.974157
5.983886	407.966007	6.979162
5.968117	406.361347	6.984166
5.761380	399.401789	6.989171
6.164604	395.051728	6.994176
5.865258	404.416166	6.999181
5.869547	399.989401	7.004186
5.683205	404.321482	7.009190
5.877473	403.585602	7.014195
5.937928	399.134218	7.019200
5.823815	395.320804	7.024205
5.779592	398.542262	7.029210
5.937482	401.548552	7.034214
5.938001	404.661759	7.039219
5.931682	406.020118	7.044224
5.688749	403.508233	7.049229
6.060598	402.323741	7.054234
5.763233	413.516561	7.059238
5.889753	398.674332	7.064243
6.227093	403.066732	7.069248
5.852878	406.567691	7.074253
6.206167	404.139562	7.079258
5.748022	402.752915	7.084262
5.828128	398.007381	7.089267
6.025259	404.190324	7.094272
5.668993	405.230183	7.099277
5.868729	403.202608	7.104282
5.501070	405.595203	7.109286
5.845241	405.968483	7.114291
5.688492	400.197016	7.119296
5.521700	412.365980	7.124301
5.915957	398.728347	7.129306
5.699388	406.073955	7.134310
5.593520	401.632812	7.139315
6.143821	402.758422	7.144320
5.962894	397.332437	7.149325
6.077381	405.056453	7.154330
5.819029	402.091395	7.159334
5.697258	406.305789	7.164339
5.976358	399.868070	7.169344
6.164688	397.934033	7.174349
6.155022	396.768189	7.179354
5.544158	405.903022	7.184358
5.910767	395.908116	7.189363
6.051255	401.568411	7.194368
5.894440	398.071742	7.199373
5.819377	396.745298	7.204378
5.924914	410.368077	7.209382
6.195923	398.249406	7.214387
6.194744	401.328076	7.219392
5.991543	408.086285	7.224397
5.998422	408.338403	7.229402
6.027339	409.523558	7.234406
6.085572	403.731062	7.239411
6.150491	401.496815	7.244416
6.062009	399.574512	7.249421
5.919945	381.363784	7.254426
5.888697	386.712455	7.259430
6.123346	382.372990	7.264435
5.994040	380.653242	7.269440
5.774791	376.856305	7.274445
6.168504	376.095504	7.279450
5.860126	381.449629	7.284454
6.100320	377.593360	7.289459
5.934988	372.911600	7.294464
5.721885	379.326493	7.299469
5.533854	374.392020	7.304474
5.700972	379.516615	7.309478
5.840064	374.679586	7.314483
5.718045	373.604115	7.319488
5.864071	379.763419	7.324493
5.704484	370.448934	7.329498
5.636388	384.124209	7.334502
5.728703	374.251387	7.339507
5.842003	368.488240	7.344512
5.394136	386.196770	7.349517
6.199188	381.280705	7.354522
6.232538	394.174449	7.359526
6.036383	390.911739	7.364531
5.878904	376.740463	7.369536
5.881585	378.742827	7.374541
5.966331	365.147387	7.379546
5.499089	376.167481	7.384550
5.568105	370.455565	7.389555
5.779977	383.163139	7.394560
5.729702	399.989958	7.399565
5.978511	398.622260	7.404570
5.750610	401.840860	7.409574
5.933923	395.579506	7.414579
6.171084	402.290862	7.419584
6.029888	394.773696	7.424589
5.744393	386.298359	7.429594
5.615748	389.472931	7.434598
5.554984	390.412704	7.439603
5.868597	400.035447	7.444608
5.816304	403.966866	7.449613
6.030949	407.271155	7.454618
5.814008	402.499394	7.459622
6.302522	398.819353	7.464627
6.060340	389.448195	7.469632
5.565348	387.168799	7.474637
5.796407	384.006836	7.479642
5.885381	392.816869	7.484646
5.712801	383.127920	7.489651
5.963194	398.309901	7.494656
5.674416	382.039434	7.499661
5.998591	378.897684	7.504666
5.479018	382.914968	7.509670
5.725334	402.394054	7.514675
5.999848	397.197272	7.519680
6.286093	404.116077	7.524685
5.983990	396.921521	7.529690
5.685912	389.606112	7.534694
5.668836	383.328702	7.539699
5.919495	392.834753	7.544704
5.765925	400.850709	7.549709
6.698839	391.621306	7.554714
5.844627	391.704615	7.559718
5.911950	388.735989	7.564723
5.785006	371.791592	7.569728
5.680505	378.116701	7.574733
5.799386	368.907285	7.579738
5.444072	384.547997	7.584742
5.731184	383.515991	7.589747
5.883184	393.157725	7.594752
5.760934	402.832943	7.599757
6.106364	398.118605	7.604762
6.003665	407.483872	7.609766
5.737222	386.837502	7.614771
5.854657	377.520739	7.619776
5.390647	390.650599	7.624781
5.908095	394.897716	7.629786
5.860383	408.955802	7.634790
5.912948	404.211418	7.639795
5.964578	397.477140	7.644800
5.845706	404.896027	7.649805
6.227558	401.710434	7.654810
6.128632	387.242067	7.659814
5.627070	386.741765	7.664819
5.855486	379.650758	7.669824
5.594112	382.944203	7.674829
6.154910	393.512159	7.679834
5.594404	393.663348	7.684838
5.535091	391.701673	7.689843
5.458142	407.222858	7.694848
5.703235	411.142485	7.699853
5.778010	405.913720	7.704858
5.891647	413.194939	7.709862
5.969549	404.498136	7.714867
5.958418	405.619963	7.719872
5.822062	405.998929	7.724877
6.114607	398.176515	7.729882
5.851733	408.541335	7.734886
6.126283	399.630223	7.739891
6.091204	399.781345	7.744896
5.583318	404.856682	7.749901
6.223784	404.405238	7.754906
5.688482	414.803255	7.759910
5.851550	413.025039	7.764915
5.736164	408.971371	7.769920
5.642165	407.581453	7.774925
6.009165	402.806785	7.779930
5.721824	410.024276	7.784934
5.885930	408.527477	7.789939
5.978942	414.407192	7.794944
5.892345	410.858388	7.799949
6.489160	403.190783	7.804954
5.889907	395.103131	7.809958
5.842271	377.073769	7.814963
5.798063	380.909002	7.819968
5.812100	380.346897	7.824973
5.659661	378.172021	7.829978
5.593838	387.300541	7.834982
5.958852	395.712978	7.839987
5.954178	396.995146	7.844992
5.803611	403.077540	7.849997
5.866555	405.222329	7.855002
6.072952	408.948698	7.860006
6.122942	397.563862	7.865011
5.878707	390.584872	7.870016
5.453285	383.552015	7.875021
5.766643	384.467971	7.880026
5.597430	401.050830	7.885030
5.649603	409.306642	7.890035
5.840139	398.671756	7.895040
6.043365	399.952989	7.900045
6.168128	401.056687	7.905050
5.987050	409.434468	7.910054
5.900779	402.019427	7.915059
5.873547	381.117280	7.920064
5.433676	381.762105	7.925069
5.819830	395.046670	7.930074
5.687258	400.933251	7.935078
5.716374	400.004944	7.940083
5.804979	400.981426	7.945088
5.683294	409.954192	7.950093
5.937905	401.482810	7.955098
5.809523	400.917709	7.960102
5.965659	403.573089	7.965107
5.836872	406.817290	7.970112
5.656567	400.790081	7.975117
6.434522	397.558245	7.980122
5.909021	399.743886	7.985139
5.898686	398.691576	7.990157
5.790855	398.304626	7.995174
5.697655	404.785446	8.000192
5.948578	398.355832	8.005210
5.606582	409.019133	8.010227
5.853705	403.776674	8.015245
5.484091	405.541936	8.020262
5.565700	414.075009	8.025280
5.807057	409.035420	8.030298
5.823644	412.075054	8.035315
5.746670	406.624602	8.040333
6.314924	398.756738	8.045350
6.222425	407.897745	8.050368
6.453324	408.808382	8.055386
6.117680	408.690652	8.060403
6.361416	410.009525	8.065421
6.190282	404.965141	8.070438
5.910128	402.042723	8.075456
5.972788	400.158481	8.080474
5.976884	408.299761	8.085491
5.695261	412.803051	8.090509
5.860352	414.923184	8.095526
5.817571	412.064557	8.100544
5.927305	409.241992	8.105562
5.575890	415.867415	8.110579
5.799581	416.870698	8.115597
6.015671	410.844162	8.120614
6.354285	416.092857	8.125632
6.272223	408.847580	8.130650
6.159016	410.875621	8.135667
6.039456	415.773233	8.140685
6.144881	405.749924	8.145702
6.046585	412.373554	8.150720
6.357279	406.335352	8.155738
5.765302	415.213802	8.160755
5.907295	416.283534	8.165773
5.975656	407.487306	8.170790
5.750835	407.629918	8.175808
5.801293	402.787495	8.180826
5.432550	408.156486	8.185843
5.615831	409.169257	8.190861
5.962220	403.996449	8.195878
5.891036	410.912472	8.200896
5.747663	411.916464	8.205914
6.014700	428.843189	8.210931
6.279778	423.392787	8.215949
6.548366	424.606783	8.220966
6.150154	419.001537	8.225984
5.907427	404.504275	8.231002
6.103077	400.020950	8.236019
5.598566	408.841512	8.241037
5.795957	423.535406	8.246054
6.048815	429.485496	8.251072
6.033546	433.170743	8.256090
5.826648	445.782088	8.261107
5.660887	442.393623	8.266125
5.859575	437.818296	8.271142
6.024047	435.403710	8.276160
5.864497	432.847393	8.281178
6.376856	436.292182	8.286195
6.355958	443.326568	8.291213
6.313506	437.457295	8.296230
6.101672	432.362476	8.301248
6.439673	427.721142	8.306266
6.379829	436.112290	8.311283
5.947937	443.356237	8.316301
6.267089	439.642490	8.321318
6.509533	435.634654	8.326336
6.395504	436.741346	8.331354
6.542704	437.444196	8.336371
6.192465	440.007988	8.341389
6.281932	427.907524	8.346406
6.112080	445.527557	8.351424
6.328209	433.435645	8.356442
6.466847	439.078591	8.361459
6.193824	433.649382	8.366477
6.137903	437.830141	8.371494
6.209075	434.316193	8.376512
6.600934	436.545963	8.381530
6.291231	440.984233	8.386547
6.295210	443.158015	8.391565
6.248388	430.851689	8.396582
6.200293	440.115141	8.401600
6.318545	436.505455	8.406618
6.523884	431.244289	8.411635
6.611338	440.701094	8.416653
6.883535	432.131688	8.421670
6.609924	425.099451	8.426688
6.407475	409.570255	8.431706
5.835333	404.645506	8.436723
6.101987	411.221422	8.441741
6.339505	421.557249	8.446758
6.202568	427.003532	8.451776
6.451993	431.483580	8.456794
6.582926	422.819550	8.461811
6.676922	431.805118	8.466829
6.620882	415.486129	8.471846
6.424785	408.205073	8.476864
6.024773	401.927939	8.481882
6.105704	409.678491	8.486899
6.060034	428.203684	8.491917
5.954541	424.209342	8.496934
5.874099	430.186408	8.501952
6.708483	427.509072	8.506970
6.717006	426.794627	8.511987
6.163811	426.944509	8.517005
6.492845	426.555380	8.522022
6.343283	434.591361	8.527040
6.529210	424.757395	8.532058
6.402108	426.140685	8.537075
6.363706	435.901226	8.542093
6.151979	432.516809	8.547110
6.451308	433.602915	8.552128
6.765478	429.164127	8.557146
6.355829	424.415881	8.562163
6.407865	433.518476	8.567181
6.893416	434.357657	8.572199
6.750915	432.546582	8.577216
6.323008	433.528887	8.582234
6.657441	442.438920	8.587251
6.432335	433.956899	8.592269
6.453440	429.456734	8.597287
6.843017	431.977191	8.602304
6.316901	429.916958	8.607322
6.685535	430.711343	8.612339
6.524697	433.936568	8.617357
6.534871	434.408427	8.622375
6.521227	437.197186	8.627392
6.612126	436.343603	8.632410
6.560476	438.608151	8.637427
6.424100	434.596555	8.642445
6.423142	431.251697	8.647463
6.558603	436.194563	8.652480
6.602817	437.639373	8.657498
6.574077	437.483023	8.662515
6.533109	442.327304	8.667533
6.518987	430.037945	8.672551
6.576401	430.309902	8.677568
6.632888	435.855268	8.682586
6.559757	435.759521	8.687603
6.498057	435.892353	8.692621
6.605644	423.255731	8.697639
6.429138	428.313746	8.702656
5.985402	433.804946	8.707674
6.366664	436.490805	8.712691
6.410478	446.860152	8.717709
6.633317	455.768742	8.722727
6.975868	463.194307	8.727744
7.094743	464.109877	8.732762
6.871938	439.053455	8.737779
6.457198	438.500000	8.742797
6.666505	427.011910	8.747815
6.803082	430.578692	8.752832
6.817263	433.726003	8.757850
6.861451	433.299454	8.762867
6.688621	444.261314	8.767885
6.523191	435.504859	8.772903
6.748945	434.734287	8.777920
6.912012	437.482735	8.782938
6.983386	435.915855	8.787955
6.870504	444.776057	8.792973
6.801837	440.028028	8.797991
6.618634	434.537409	8.803008
6.353443	429.905380	8.808026
6.694461	437.189165	8.813043
6.306501	445.713777	8.818061
6.528968	441.469233	8.823079
6.614005	445.927705	8.828096
6.971689	465.415358	8.833114
7.215693	460.214396	8.838131
6.569004	462.427014	8.843149
6.883485	462.926933	8.848167
6.460231	464.650113	8.853184
6.546659	465.255190	8.858202
6.962254	457.426998	8.863219
6.635473	459.892445	8.868237
6.863048	458.045473	8.873255
6.824735	466.774083	8.878272
6.786013	462.422137	8.883290
6.978829	462.540337	8.888307
6.858611	463.837346	8.893325
6.852002	463.456625	8.898343
7.288054	459.184923	8.903360
6.977234	458.798219	8.908378
7.183887	453.476881	8.913395
6.935125	439.715827	8.918413
6.544077	437.312544	8.923431
6.554523	442.372828	8.928448
6.647444	450.515988	8.933466
6.980002	447.355552	8.938483
6.651596	458.628970	8.943501
6.938720	457.829847	8.948519
7.033237	453.804161	8.953536
6.761900	458.684541	8.958554
7.153710	457.594464	8.963571
6.945224	457.986977	8.968589
7.062370	460.865699	8.973607
7.202533	456.403677	8.978624
7.033453	459.863723	8.983642
6.847663	451.422871	8.988659
6.872215	454.565404	8.993677
6.603399	459.322316	8.998695
6.763410	462.408913	9.003712
6.875002	465.279038	9.008730
6.602827	457.725863	9.013747
6.934772	456.648322	9.018765
7.144919	457.805206	9.023783
7.359708	460.794859	9.028800
7.111878	463.128017	9.033818
7.100846	460.475842	9.038835
6.937723	452.877181	9.043853
7.252018	457.170349	9.048871
6.992417	453.114941	9.053888
6.799830	467.674318	9.058906
7.040528	461.602884	9.063923
6.705488	458.351390	9.068941
6.832394	467.789406	9.073959
6.598692	462.817923	9.078976
6.865709	473.587809	9.083994
7.183647	483.847957	9.089011
7.168390	487.937151	9.094029
7.171802	487.826255	9.099047
7.171501	490.650801	9.104064
7.112619	494.551174	9.109082
7.328135	484.116100	9.114099
7.122320	481.305096	9.119117
7.041694	466.911772	9.124135
7.127787	466.264065	9.129152
6.714061	484.632393	9.134170
7.402102	480.908175	9.139187
7.118936	480.798001	9.144205
6.831638	486.602372	9.149223
7.312866	493.097362	9.154240
7.055114	496.460858	9.159258
7.121257	490.817545	9.164275
7.278665	490.348010	9.169293
7.275585	497.019868	9.174311
7.366639	484.953830	9.179328
7.142334	485.986287	9.184346
7.039693	482.272348	9.189363
7.102008	481.293856	9.194381
7.438650	478.946961	9.199399
7.410322	482.028358	9.204416
7.239988	493.980765	9.209434
7.354361	491.075412	9.214451
7.553430	488.948884	9.219469
7.507594	487.709630	9.224487
7.212070	471.910944	9.229504
6.888455	477.235016	9.234522
7.381921	467.589523	9.239539
7.402240	484.116306	9.244557
7.377965	484.221184	9.249575
7.484402	478.161313	9.254592
7.341027	481.945536	9.259610
7.442415	469.950472	9.264627
6.959740	469.082617	9.269645
7.247491	480.713937	9.274663
7.386576	486.533551	9.279680
7.331616	489.432932	9.284698
7.451031	489.269147	9.289715
7.567325	491.286483	9.294733
7.237826	489.350069	9.299751
7.028935	486.277619	9.304768
7.398296	492.032752	9.309786
7.346127	487.212699	9.314803
7.097908	489.681618	9.319821
7.096829	490.855822	9.324839
7.412765	480.748994	9.329856
7.223798	486.358081	9.334874
7.462289	485.768545	9.339891
7.092502	486.164241	9.344909
7.137274	487.135603	9.349927
6.871334	486.779736	9.354944
6.929447	488.219216	9.359962
7.444587	500.859479	9.364979
7.293796	513.916511	9.369997
7.146147	523.044128	9.375015
7.276727	510.599499	9.380032
7.318030	518.293192	9.385050
7.027314	515.113637	9.390067
7.478082	514.544488	9.395085
7.204249	519.497859	9.400103
7.613369	509.871871	9.405120
7.353856	519.108530	9.410138
7.679833	512.010715	9.415155
7.528368	511.879905	9.420173
7.519645	519.789717	9.425191
7.458212	517.464164	9.430208
7.243417	520.426462	9.435226
7.319628	517.094743	9.440243
7.623239	519.455114	9.445261
7.487438	518.353029	9.450279
7.869044	517.365532	9.455296
7.620361	518.622713	9.460314
7.721399	522.718940	9.465331
7.612957	523.338773	9.470349
7.459951	519.449683	9.475367
7.759571	513.971751	9.480384
7.695638	518.141161	9.485402
7.504562	515.993710	9.490419
7.590790	512.512101	9.495437
7.057610	514.527061	9.500455
7.704422	517.158702	9.505472
7.737884	536.258581	9.510490
7.388531	523.576719	9.515507
7.733274	524.056119	9.520525
8.013431	540.188796	9.525543
8.131312	525.776944	9.530560
7.608347	520.828678	9.535578
7.414604	519.741982	9.540595
7.884999	517.547693	9.545613
7.569641	523.242865	9.550631
7.500877	508.427931	9.555648
7.592271	517.060505	9.560666
8.002583	522.796609	9.565683
7.797524	513.554025	9.570701
7.592002	513.362258	9.575719
7.740241	509.425970	9.580736
7.893627	508.234394	9.585754
7.730679	503.706245	9.590771
7.673262	510.449737	9.595789
7.545515	510.769641	9.600807
7.978657	513.602016	9.605824
7.739049	523.861183	9.610842
7.716170	518.821939	9.615859
7.972386	509.081055	9.620877
7.429537	516.538073	9.625895
8.036287	527.463042	9.630912
7.974043	531.032594	9.635930
7.890475	531.714802	9.640947
7.902689	508.868367	9.645965
7.716830	518.308078	9.650983
7.943771	516.663169	9.656000
7.597378	518.156563	9.661018
7.920315	523.338320	9.666035
7.945310	520.251307	9.671053
7.745460	516.625175	9.676071
7.887671	519.828179	9.681088
8.075597	540.415474	9.686106
7.972920	525.015710	9.691123
7.872739	511.890877	9.696141
7.598718	506.531229	9.701159
8.194193	520.979796	9.706176
8.041850	521.963110	9.711194
7.625931	517.777547	9.716211
7.828043	520.254806	9.721229
8.172085	537.314734	9.726247
8.508281	528.167215	9.731264
7.994598	524.962635	9.736282
8.128118	516.686313	9.741299
8.273468	502.920264	9.746317
8.072301	507.272118	9.751335
8.127086	508.955115	9.756352
8.410079	516.850777	9.761370
7.970774	529.719499	9.766387
8.316672	521.476171	9.771405
8.199517	527.121355	9.776423
8.194263	518.686897	9.781440
7.698450	516.514610	9.786458
8.018283	505.671863	9.791475
8.238616	510.402639	9.796493
8.091902	521.505619	9.801511
7.850590	522.345084	9.806528
8.124928	516.552380	9.811546
7.811453	517.627211	9.816563
8.021196	514.034732	9.821581
8.050123	525.744504	9.826599
8.220939	518.983418	9.831616
8.328479	520.980040	9.836634
8.069379	513.140773	9.841651
8.231882	508.040928	9.846669
7.820932	516.575487	9.851687
8.114954	515.027364	9.856704
8.082029	523.026175	9.861722
8.245583	526.298419	9.866739
8.266369	508.755491	9.871757
8.018135	526.858094	9.876775
8.057544	529.149411	9.881792
8.099248	518.725772	9.886810
7.843818	526.421780	9.891827
8.217985	513.803285	9.896845
7.736238	514.285951	9.901863
7.906950	516.282140	9.906880
7.980064	520.430078	9.911898
8.040442	516.056280	9.916915
8.110715	523.534000	9.921933
8.458080	542.073467	9.926951
8.836927	530.785963	9.931968
8.394489	529.394254	9.936986
8.083819	525.286872	9.942003
8.495716	517.806367	9.947021
8.045294	523.191346	9.952039
8.324108	521.487816	9.957056
8.367307	522.825496	9.962074
8.087423	521.278931	9.967091
8.351199	514.377052	9.972109
8.405408	515.286977	9.977127
8.053237	518.501171	9.982144
8.643799	520.759778	9.987162
8.264763	519.979822	9.992179
8.151650	509.416346	9.997197
7.956308	515.588166	10.002215
8.302631	531.508499	10.007232
8.325428	542.436611	10.012250
7.960320	542.878912	10.017267
8.508956	534.493359	10.022285
8.278219	549.671000	10.027303
8.245705	547.867926	10.032320
8.470038	546.097192	10.037338
8.423942	543.879685	10.042355
8.418966	540.021045	10.047373
8.279737	542.782160	10.052391
8.309183	541.909800	10.057408
8.588386	550.329928	10.062426
8.215630	554.522488	10.067443
8.246994	545.539486	10.072461
8.238122	553.745979	10.077479
8.321737	550.359446	10.082496
8.600868	547.380931	10.087514
8.443008	551.915357	10.092531
8.329920	549.212889	10.097549
8.066414	548.474790	10.102567
8.613181	558.367771	10.107584
8.644628	549.217498	10.112602
8.540888	553.901233	10.117619
8.275276	561.223315	10.122637
8.512931	553.116851	10.127655
8.490862	546.673153	10.132672
8.841202	554.132249	10.137690
8.488753	556.402916	10.142707
8.687387	548.949502	10.147725
8.472478	543.586892	10.152743
8.595705	556.323314	10.157760
8.636022	554.874898	10.162778
8.566964	557.536660	10.167795
8.765180	548.139354	10.172813
8.667879	560.679961	10.177831
8.543813	550.859783	10.182848
8.461517	550.494075	10.187866
8.201090	543.598579	10.192883
8.482783	546.183292	10.197901
8.616693	560.003629	10.202919
8.670377	569.017674	10.207936
9.023358	562.003970	10.212954
8.638103	558.482617	10.217971
8.478288	553.243915	10.222989
8.479701	556.702513	10.228007
8.510840	561.851107	10.233024
8.982852	563.695953	10.238042
8.722052	581.062128	10.243059
9.037785	570.084287	10.248077
8.956121	559.048798	10.253095
8.724180	554.184311	10.258112
8.987286	549.264349	10.263130
8.678999	546.160125	10.268147
8.529484	547.685790	10.273165
8.470889	549.089913	10.278183
8.768140	564.386809	10.283200
8.839350	570.204463	10.288218
9.008413	572.721621	10.293235
9.013025	562.941235	10.298253
8.748893	560.675838	10.303271
8.645476	551.243741	10.308288
8.714329	542.961760	10.313306
8.656091	562.890225	10.318323
8.817469	573.724060	10.323341
8.827411	579.365125	10.328359
8.602157	569.892149	10.333376
8.872089	574.410045	10.338394
8.402099	576.812739	10.343411
8.867186	573.694632	10.348429
8.851479	579.538530	10.353447
8.789290	583.641410	10.358464
8.913105	575.748432	10.363482
8.745741	577.270584	10.368499
8.613459	575.543099	10.373517
8.866377	575.178517	10.378535
8.855181	568.793066	10.383552
9.017521	572.999619	10.388570
8.967410	577.744385	10.393587
8.824185	577.593348	10.398605
8.968512	576.778724	10.403623
8.840954	579.070962	10.408640
9.045135	568.861675	10.413658
8.809289	574.585430	10.418675
8.869843	569.861301	10.423693
9.310783	570.571780	10.428711
9.243673	566.770206	10.433728
8.995623	567.187855	10.438746
9.078145	575.821847	10.443763
8.794195	575.137443	10.448781
9.213837	577.823622	10.453799
8.772560	579.880994	10.458816
9.145956	572.015183	10.463834
9.219662	577.330679	10.468851
9.144823	572.952807	10.473869
9.176936	567.816571	10.478887
9.062538	576.711789	10.483904
9.259266	573.711468	10.488922
9.097675	582.285883	10.493939
9.097673	571.471119	10.498957
9.436613	573.728133	10.503975
8.980147	576.873472	10.508992
9.211051	573.078852	10.514010
8.680947	575.134362	10.519027
8.685584	571.289988	10.524045
9.167472	588.230537	10.529063
8.854434	591.848863	10.534080
9.034584	594.638840	10.539098
8.955234	592.871503	10.544115
9.160528	596.683169	10.549133
9.353912	600.373628	10.554151
9.511559	611.400573	10.559168
9.550448	594.848797	10.564186
9.273754	602.740672	10.569203
9.417524	599.833851	10.574221
9.364187	605.043029	10.579239
8.934328	603.933364	10.584256
9.408815	585.864841	10.589274
9.125779	599.813652	10.594291
9.334642	595.845756	10.599309
9.509204	595.919481	10.604327
9.268039	600.094588	10.609344
9.608097	595.841051	10.614362
9.109316	606.652110	10.619379
9.019240	604.744442	10.624397
9.186804	607.053558	10.629415
9.258174	605.496131	10.634432
9.307398	593.928876	10.639450
9.437701	602.564862	10.644467
9.107508	600.940967	10.649485
9.066121	603.415365	10.654503
9.063539	607.808711	10.659520
9.275253	600.706674	10.664538
9.312188	602.600759	10.669555
9.640494	597.263473	10.674573
9.636006	595.421289	10.679591
9.273705	603.711584	10.684608
9.426627	597.893696	10.689626
9.296898	597.472303	10.694643
9.183047	603.135928	10.699661
9.378208	599.637234	10.704679
9.138766	607.207696	10.709696
9.586885	618.788733	10.714714
9.494190	627.248233	10.719731
9.396836	629.633574	10.724749
9.904954	625.757638	10.729767
9.565736	616.100523	10.734784
9.818538	596.517233	10.739802
9.461461	602.484052	10.744819
9.434556	595.662400	10.749837
9.769621	592.842370	10.754855
9.523921	604.592068	10.759872
9.320671	596.216998	10.764890
9.397667	597.517830	10.769907
9.428083	611.168230	10.774925
9.864077	611.939447	10.779943
9.639137	608.891580	10.784960
9.598367	593.456811	10.789978
9.723906	613.542729	10.794995
9.228142	612.762123	10.800013
9.721038	611.965466	10.805031
9.444415	618.860109	10.810048
9.672390	614.081334	10.815066
9.800169	614.938712	10.820083
9.725917	614.518093	10.825101
9.470881	622.491790	10.830119
9.811471	624.227847	10.835136
9.729219	621.422707	10.840154
9.769070	614.063572	10.845171
9.686993	620.315511	10.850189
9.934533	617.881575	10.855207
9.751778	615.123741	10.860224
9.845776	617.267661	10.865242
9.978602	623.422814	10.870259
9.736726	621.964959	10.875277
9.799242	617.805395	10.880295
9.680993	608.962568	10.885312
9.837179	612.008765	10.890330
10.103255	621.033739	10.895347
9.695416	613.934096	10.900365
9.937311	609.964177	10.905383
9.912033	619.129474	10.910400
9.904827	612.033331	10.915418
9.633955	599.301249	10.920435
9.758620	612.371998	10.925453
9.906327	616.555608	10.930471
9.867384	617.776777	10.935488
10.269823	615.965507	10.940506
9.963896	609.632533	10.945523
9.842879	610.601476	10.950541
9.953005	601.868036	10.955559
9.640886	599.796344	10.960576
10.023465	606.063836	10.965594
9.660729	617.147074	10.970611
10.003440	617.421669	10.975629
9.982014	614.821593	10.980647
10.156176	630.232505	10.985664
9.987645	619.762853	10.990682
10.260070	625.283911	10.995699
9.847336	613.861607	11.000717
9.706911	608.323207	11.005735
10.066510	626.772484	11.010752
9.974033	617.906679	11.015770
9.951128	621.044054	11.020787
9.758026	624.012438	11.025805
9.999680	614.968051	11.030823
9.717560	628.579072	11.035840
9.786614	619.896240	11.040858
10.031203	617.166121	11.045875
9.941464	622.706054	11.050893
10.420845	624.571843	11.055911
10.202757	632.830088	11.060928
10.229856	622.544375	11.065946
10.257999	627.270581	11.070963
10.032404	627.883528	11.075981
10.219454	625.642103	11.080999
9.977045	626.106207	11.086016
9.927431	621.090057	11.091034
10.232532	624.538956	11.096051
9.842236	627.033311	11.101069
9.791811	621.502895	11.106087
10.014366	628.634908	11.111104
9.972868	618.931143	11.116122
10.139199	633.115684	11.121139
10.688830	647.126571	11.126157
10.595077	631.832614	11.131175
9.980726	632.200360	11.136192
9.829495	632.880550	11.141210
10.431737	640.650506	11.146227
10.063807	642.238803	11.151245
10.365201	635.785417	11.156263
10.398950	646.617203	11.161280
10.309440	651.914114	11.166298
10.492601	649.114721	11.171315
10.402989	636.442574	11.176333
10.017998	623.835651	11.181351
10.155574	638.876764	11.186368
10.411846	643.993263	11.191386
10.619496	646.946196	11.196403
10.493358	651.526169	11.201421
10.696184	641.679969	11.206439
10.515570	627.794485	11.211456
10.253551	630.918834	11.216474
10.362736	611.241266	11.221491
9.868344	623.105680	11.226509
10.402523	630.820025	11.231527
10.297925	638.498760	11.236544
10.126037	647.784872	11.241562
10.322059	639.356690	11.246579
10.418769	650.188080	11.251597
10.712678	642.672363	11.256615
10.896730	644.076344	11.261632
10.724752	648.196442	11.266650
10.454437	650.807700	11.271667
10.627040	652.450161	11.276685
10.949712	637.434933	11.281703
10.805574	637.609085	11.286720
10.161028	631.452235	11.291738
10.353582	633.596494	11.296755
10.493700	647.400147	11.301773
10.960892	649.488754	11.306791
10.432573	646.895511	11.311808
10.247001	645.495104	11.316826
10.507937	656.250275	11.321843
10.286816	657.534705	11.326861
10.547674	643.646308	11.331879
10.590498	648.515386	11.336896
10.704262	647.042832	11.341914
11.020814	638.068749	11.346931
10.685295	648.803760	11.351949
10.744759	651.603188	11.356967
10.893369	642.226229	11.361984
10.463069	645.197067	11.367002
10.401324	641.782799	11.372019
10.328032	654.834103	11.377037
10.480137	647.230149	11.382055
10.643529	647.624359	11.387072
10.336333	654.732088	11.392090
10.890954	654.702084	11.397107
10.726679	662.014640	11.402125
10.546551	654.213430	11.407143
10.255676	651.983769	11.412160
10.588968	660.193504	11.417178
10.802293	673.174668	11.422195
11.116543	684.625244	11.427213
10.938864	665.939302	11.432231
10.906341	668.857287	11.437248
10.852312	671.175885	11.442266
10.843666	654.558918	11.447283
10.622657	669.088198	11.452301
10.842305	675.195052	11.457319
11.156048	677.610661	11.462336
10.672907	675.306981	11.467354
11.176802	676.676630	11.472371
10.851208	660.077761	11.477389
10.790945	666.739708	11.482407
10.605103	663.953947	11.487424
11.042448	677.206126	11.492442
11.042500	670.560102	11.497459
11.004424	679.667474	11.502477
11.070784	678.937645	11.507495
10.673710	683.225563	11.512512
10.991878	684.488614	11.517530
11.264345	676.673285	11.522547
11.083699	679.740711	11.527565
11.194213	677.501805	11.532583
11.261586	681.161531	11.537600
10.911688	678.322579	11.542618
11.136969	667.605002	11.547635
11.016704	671.130025	11.552653
10.926017	673.435432	11.557671
10.876987	673.878704	11.562688
10.973605	681.046249	11.567706
11.229839	680.255113	11.572723
11.220041	683.261057	11.577741
10.698179	675.235672	11.582759
11.007501	673.451609	11.587776
10.966588	677.756304	11.592794
11.165444	678.842389	11.597811
10.821027	680.007285	11.602829
11.094258	672.160280	11.607847
11.260462	668.855458	11.612864
10.965770	673.401885	11.617882
11.464065	676.353466	11.622899
11.144373	679.161813	11.627917
11.424746	671.354715	11.632935
11.364647	679.613473	11.637952
11.025399	671.935017	11.642970
11.184803	670.900277	11.647987
11.081809	669.597382	11.653005
10.924831	672.364454	11.658023
11.528910	673.046222	11.663040
11.032903	669.321294	11.668058
11.062264	675.675713	11.673075
11.280137	683.837271	11.678093
11.729665	695.601174	11.683111
11.451916	678.445681	11.688128
11.213842	672.373452	11.693146
11.369390	674.346790	11.698163
11.371211	674.851522	11.703181
11.314976	681.367677	11.708199
11.326049	684.960486	11.713216
11.562697	691.916747	11.718234
11.455282	678.931779	11.723251
11.366107	684.626277	11.728269
11.552453	686.146667	11.733287
11.656029	676.833550	11.738304
11.539516	680.550490	11.743322
11.039340	669.129228	11.748339
11.368042	679.895885	11.753357
11.380944	695.436261	11.758375
11.481532	694.877794	11.763392
11.090573	700.190392	11.768410
11.206927	701.235757	11.773427
11.319228	709.319194	11.778445
11.083871	713.206240	11.783463
11.720666	708.530642	11.788480
11.334973	702.027096	11.793498
11.346589	705.604046	11.798515
11.789756	708.712592	11.803533
11.801150	711.450133	11.808551
11.962402	700.092475	11.813568
11.888892	708.874055	11.818586
11.731487	700.949344	11.823603
11.867868	710.045177	11.828621
11.841477	708.395762	11.833639
11.955309	704.651014	11.838656
11.779769	713.540101	11.843674
12.017844	705.244155	11.848691
11.720405	694.116159	11.853709
11.599101	682.401997	11.858727
11.767825	685.389438	11.863744
11.773909	696.607440	11.868762
11.973659	693.556133	11.873779
11.705583	689.334742	11.878797
11.526679	684.215756	11.883815
11.913804	696.576415	11.888832
11.557871	692.337231	11.893850
12.112409	696.327728	11.898867
11.559024	698.964411	11.903885
11.878725	708.921455	11.908903
11.850221	710.642768	11.913920
11.437186	706.018052	11.918938
11.606427	705.404646	11.923955
11.887091	703.858600	11.928973
11.450013	710.118856	11.933991
11.968660	709.141436	11.939008
11.564873	709.321557	11.944026
12.143284	702.764783	11.949043
11.942886	700.012856	11.954061
11.793064	703.643501	11.959079
11.893390	702.327682	11.964096
11.771704	704.202450	11.969114
11.797576	698.508577	11.974131
12.033281	697.304091	11.979149
11.692506	700.159925	11.984167
12.055750	700.851027	11.989184
11.895833	703.293517	11.994202
11.593062	703.044401	11.999219
12.021083	703.308787	12.004237
11.739372	725.929632	12.009255
12.380233	712.912605	12.014272
12.231838	723.097634	12.019290
11.954218	720.218948	12.024307
12.068443	714.621680	12.029325
12.087078	720.406595	12.034343
12.333209	708.827349	12.039360
12.010986	717.764667	12.044378
12.382233	716.987066	12.049395
12.207672	705.745136	12.054413
11.988830	695.627304	12.059431
12.099956	696.013925	12.064448
12.331115	706.038490	12.069466
12.243842	717.548844	12.074483
12.119677	707.706505	12.079501
12.034363	714.871011	12.084519
12.023706	719.593853	12.089536
11.770081	720.249064	12.094554
11.965804	719.050841	12.099571
12.232177	716.370943	12.104589
12.447054	721.976788	12.109607
12.521609	716.616109	12.114624
12.198198	714.460965	12.119642
12.216987	707.966626	12.124659
12.312886	716.358749	12.129677
12.093309	721.606632	12.134695
12.510238	707.498072	12.139712
12.124587	715.659533	12.144730
11.920867	720.406313	12.149747
12.252414	715.437714	12.154765
12.271210	708.501560	12.159783
12.157592	713.054341	12.164800
12.419404	725.055958	12.169818
12.045443	723.306365	12.174835
12.469115	724.786418	12.179853
12.185451	735.494422	12.184871
12.546970	743.911212	12.189888
12.464339	744.640618	12.194906
12.289392	750.418003	12.199923
12.781451	745.967045	12.204941
12.456991	746.548149	12.209959
12.469654	739.265805	12.214976
12.591744	741.026642	12.219994
12.396158	741.477100	12.225011
12.533892	740.385791	12.230029
12.282819	750.687910	12.235047
12.499706	737.093509	12.240064
12.459863	742.679310	12.245082
12.589863	742.517020	12.250099
12.845694	741.467168	12.255117
12.479117	741.622524	12.260135
12.436111	737.927591	12.265152
12.234839	748.253463	12.270170
12.552951	750.273922	12.275187
12.950767	745.746211	12.280205
12.390455	749.406469	12.285223
12.804233	747.161063	12.290240
12.635503	749.055830	12.295258
12.664172	739.905895	12.300275
12.935017	746.241437	12.305293
12.535455	751.650073	12.310311
12.890469	732.460875	12.315328
13.014239	737.490863	12.320346
12.646195	740.792790	12.325363
13.149862	736.002344	12.330381
12.909988	742.717707	12.335399
12.836579	744.884716	12.340416
12.662154	738.928724	12.345434
12.733037	751.174869	12.350451
12.561985	742.750504	12.355469
12.660570	741.709510	12.360487
12.828838	742.617355	12.365504
12.657207	749.672323	12.370522
12.400234	748.898478	12.375539
12.764217	751.322005	12.380557
12.711772	763.297146	12.385575
12.924030	765.589813	12.390592
12.852690	769.391212	12.395610
13.165508	774.732418	12.400627
13.191441	774.472825	12.405645
13.016185	770.180066	12.410663
13.067472	766.460885	12.415680
13.268106	759.505688	12.420698
13.052325	748.393266	12.425715
12.961130	735.891711	12.430733
12.740433	745.728319	12.435751
12.994181	751.198695	12.440768
13.500294	756.055173	12.445786
12.903516	750.761800	12.450803
12.976868	739.256943	12.455821
13.093201	752.534228	12.460839
13.130163	745.610993	12.465856
13.430157	752.869778	12.470874
13.126967	747.467290	12.475891
13.234359	738.219815	12.480909
12.912400	741.495586	12.485927
12.769418	748.549221	12.490944
13.332736	764.915446	12.495962
13.265193	760.268141	12.500979
13.088316	767.339717	12.505997
13.102614	773.033810	12.511015
13.388467	770.521266	12.516032
13.519186	768.067743	12.521050
13.211483	770.621761	12.526067
13.356185	761.153833	12.531085
13.252215	768.428581	12.536103
13.335074	764.635026	12.541120
13.354633	757.455736	12.546138
13.175945	763.019117	12.551155
13.555498	762.095045	12.556173
13.247576	762.736674	12.561191
13.440763	764.047716	12.566208
13.353955	771.206167	12.571226
13.142443	769.942358	12.576243
13.240813	759.497077	12.581261
13.339692	766.206710	12.586279
13.281270	774.742961	12.591296
13.325885	767.906881	12.596314
13.553140	760.089132	12.601331
13.688487	753.724837	12.606349
13.490066	758.773755	12.611367
13.504049	768.731396	12.616384
13.517929	760.296982	12.621402
13.232652	776.152392	12.626419
13.551294	768.348723	12.631437
13.465812	771.145634	12.636455
13.522474	771.856372	12.641472
13.789938	767.424820	12.646490
13.730203	766.402319	12.651507
13.583393	763.152835	12.656525
13.205909	761.173416	12.661543
13.707252	767.662199	12.666560
13.631053	761.725523	12.671578
13.488801	766.462685	12.676595
13.503511	762.780793	12.681613
13.345244	769.619080	12.686631
13.661975	760.935242	12.691648
14.008043	759.640876	12.696666
13.449021	769.480015	12.701683
13.664245	765.413255	12.706701
13.878898	770.615206	12.711719
13.716854	767.046215	12.716736
13.968880	766.340941	12.721754
13.799261	775.999149	12.726771
13.671488	759.902525	12.731789
13.321420	762.097104	12.736807
13.786742	773.924857	12.741824
13.561784	761.068700	12.746842
13.574857	773.276580	12.751859
13.691084	784.199669	12.756877
13.872881	790.334583	12.761895
13.792167	793.641993	12.766912
14.099848	790.018335	12.771930
13.817469	792.805074	12.776947
13.637936	793.215147	12.781965
14.013150	799.048360	12.786983
13.891999	800.279267	12.792000
13.766839	799.267015	12.797018
13.847135	793.971686	12.802035
14.041273	803.216307	12.807053
14.084484	789.567027	12.812071
14.324689	791.126325	12.817088
14.102465	792.041707	12.822106
14.008386	800.059691	12.827123
14.412801	789.396026	12.832141
13.837759	780.391155	12.837159
13.797416	798.092229	12.842176
14.122467	793.935671	12.847194
13.998823	792.241525	12.852211
14.334481	795.092376	12.857229
13.987819	794.537709	12.862247
13.857147	797.493184	12.867264
14.120344	797.108052	12.872282
14.022262	792.178344	12.877299
13.924470	794.153519	12.882317
14.073053	797.447093	12.887335
13.822984	796.971967	12.892352
14.374837	784.325441	12.897370
14.218543	789.566584	12.902387
14.256460	789.926808	12.907405
14.232314	789.558295	12.912423
14.259709	789.582496	12.917440
14.381638	787.392280	12.922458
14.001726	789.626254	12.927475
14.406845	789.098964	12.932493
14.371663	791.562948	12.937511
14.382694	790.535669	12.942528
14.280401	784.622009	12.947546
14.651787	797.685796	12.952563
14.416915	788.195275	12.957581
14.172081	798.414392	12.962599
14.135660	798.224528	12.967616
14.355012	790.821417	12.972634
14.241151	795.216465	12.977651
14.222246	797.406499	12.982669
14.128699	800.510793	12.987687
14.224004	817.149212	12.992704
14.119381	816.537686	12.997722
14.483071	823.612950	13.002739
14.688877	809.095575	13.007757
14.212164	814.443734	13.012775
14.815368	824.163918	13.017792
14.845662	810.052741	13.022810
14.569840	821.103551	13.027827
14.581404	821.789799	13.032845
14.701535	824.693358	13.037863
14.817691	821.008184	13.042880
14.891594	810.326864	13.047898
14.914120	810.897784	13.052915
15.170922	811.119571	13.057933
14.842268	797.206656	13.062951
14.326024	788.400852	13.067968
14.602273	792.485467	13.072986
14.552644	794.339487	13.078003
14.597348	795.235137	13.083021
15.012365	809.548111	13.088039
14.904857	803.587924	13.093056
14.835404	785.014289	13.098074
14.689933	795.120006	13.103091
14.817823	798.110708	13.108109
14.597130	798.744982	13.113127
14.637792	807.297282	13.118144
14.866184	796.351923	13.123162
14.872410	807.929736	13.128179
14.768140	808.107111	13.133197
15.281506	814.073317	13.138215
14.780578	803.709286	13.143232
15.174810	789.257079	13.148250
14.537713	789.764091	13.153267
14.679372	800.493856	13.158285
14.862904	804.656118	13.163303
14.730993	823.558152	13.168320
15.194216	817.783093	13.173338
14.734288	807.302182	13.178355
15.031271	810.326353	13.183373
15.111185	811.995975	13.188391
14.916614	810.625367	13.193408
14.861482	808.305100	13.198426
14.900191	811.357115	13.203443
15.233535	811.570065	13.208461
15.285271	812.726547	13.213479
14.983818	811.969136	13.218496
15.193008	812.491874	13.223514
15.402286	808.776332	13.228531
14.897950	812.497260	13.233549
15.063170	804.111696	13.238567
15.087920	812.634934	13.243584
15.227110	806.923272	13.248602
15.293764	803.684516	13.253619
15.094569	799.376566	13.258637
15.031751	805.373087	13.263655
14.909226	807.639318	13.268672
14.793938	804.198694	13.273690
15.171988	798.806218	13.278707
14.835826	808.458980	13.283725
15.276603	817.646030	13.288743
15.065075	827.313988	13.293760
15.348715	829.658596	13.298778
15.173481	827.240379	13.303795
15.071194	835.852960	13.308813
15.373972	823.226498	13.313831
14.960529	832.014063	13.318848
15.224030	831.452156	13.323866
15.475373	825.703981	13.328883
15.380975	821.957122	13.333901
15.880530	826.899854	13.338919
15.510354	834.885374	13.343936
15.710235	829.012716	13.348954
15.805831	831.386787	13.353971
15.622378	829.370647	13.358989
15.731189	830.543435	13.364007
15.408632	830.303728	13.369024
15.666516	829.644871	13.374042
15.641440	834.770793	13.379059
15.761917	826.294399	13.384077
16.052798	830.408289	13.389095
15.812395	830.266164	13.394112
15.754191	815.916382	13.399130
15.504027	800.233375	13.404147
15.307287	805.979479	13.409165
15.942589	814.366029	13.414183
15.424693	829.598367	13.419200
15.628755	831.611458	13.424218
15.751859	837.121264	13.429235
15.667762	835.862734	13.434253
15.778286	825.270342	13.439271
15.519679	833.743312	13.444288
15.510754	831.368465	13.449306
15.372784	828.821332	13.454323
15.258521	833.162804	13.459341
15.666014	823.189763	13.464359
15.604342	826.465792	13.469376
15.644490	823.647754	13.474394
15.757828	834.366198	13.479411
15.790565	848.079533	13.484429
15.856221	845.768738	13.489447
15.885530	858.213976	13.494464
15.993368	856.843319	13.499482
16.117188	853.866998	13.504499
15.843646	859.924957	13.509517
16.239119	856.890293	13.514535
16.073713	843.794370	13.519552
15.956504	835.213201	13.524570
15.861845	835.837197	13.529587
16.032204	838.767603	13.534605
16.209498	843.009747	13.539623
16.057414	834.055343	13.544640
15.858612	828.958369	13.549658
16.029530	843.170760	13.554675
15.939580	847.846099	13.559693
15.879839	846.192430	13.564711
15.769352	855.595262	13.569728
16.146185	848.577709	13.574746
16.142024	848.859320	13.579763
15.835498	853.969385	13.584781
16.464779	846.180127	13.589799
16.019075	855.136861	13.594816
16.109769	847.646586	13.599834
16.334983	852.253611	13.604851
15.954175	847.507043	13.609869
16.225884	841.433777	13.614887
16.277407	845.796614	13.619904
16.270167	846.892911	13.624922
16.515170	846.343369	13.629939
16.190230	851.506812	13.634957
16.418489	841.047443	13.639975
16.257044	848.034582	13.644992
16.188274	847.976019	13.650010
16.356568	853.541866	13.655027
16.242811	850.243006	13.660045
16.483026	860.768015	13.665063
16.365558	877.076908	13.670080
16.626194	871.772234	13.675098
16.670314	871.058506	13.680115
16.386453	862.263592	13.685133
16.661818	860.639467	13.690151
16.420318	855.848979	13.695168
16.400407	857.057715	13.700186
16.650188	862.560305	13.705203
16.692402	877.203147	13.710221
16.800647	866.680515	13.715239
16.411985	858.826682	13.720256
16.668617	860.247712	13.725274
16.733507	854.550832	13.730291
16.179500	863.325722	13.735309
16.711141	866.742329	13.740327
16.568760	881.354136	13.745344
16.605993	876.027660	13.750362
16.941463	877.553104	13.755379
16.735071	883.572146	13.760397
16.715821	880.892795	13.765415
16.758101	879.156865	13.770432
16.707796	893.905735	13.775450
17.010154	873.998794	13.780467
16.937267	879.608750	13.785485
16.582622	877.692012	13.790503
16.825664	881.065476	13.795520
16.855802	880.950391	13.800538
16.997120	878.040752	13.805555
16.403050	884.628627	13.810573
16.676598	872.956615	13.815591
16.804355	877.070828	13.820608
16.956159	884.832572	13.825626
17.018378	876.996449	13.830643
16.582375	884.077113	13.835661
16.797836	892.157093	13.840679
16.953618	879.989128	13.845696
16.290498	875.236292	13.850714
16.751194	887.778063	13.855731
16.820086	902.940614	13.860749
16.941752	908.548499	13.865767
16.746801	905.795686	13.870784
17.076319	914.949726	13.875802
17.149656	906.256616	13.880819
17.039810	912.027009	13.885837
17.179104	909.316501	13.890855
17.231963	916.352140	13.895872
17.487754	904.064346	13.900890
17.478023	910.355545	13.905907
17.337315	907.509025	13.910925
17.668256	906.977576	13.915943
17.645083	904.876353	13.920960
17.639176	881.498945	13.925978
17.483346	876.827573	13.930995
17.191802	885.962141	13.936013
17.500072	875.613294	13.941031
17.431140	877.161075	13.946048
17.275302	872.934677	13.951066
16.908016	867.008859	13.956083
17.026126	876.735650	13.961101
17.320782	884.421363	13.966119
17.298175	889.098785	13.971136
17.146727	897.469787	13.976154
17.629416	894.465634	13.981171
17.627535	898.739020	13.986189
17.730160	901.594842	13.991207
17.605877	904.596671	13.996224
17.501400	904.543702	14.001242
17.309351	897.482719	14.006259
17.058514	901.100829	14.011277
17.466613	900.825537	14.016295
17.446001	907.926333	14.021312
17.388132	904.451447	14.026330
17.403922	896.474266	14.031347
17.917171	904.826333	14.036365
17.531464	900.676971	14.041383
17.445000	895.385649	14.046400
17.394793	898.820843	14.051418
17.557311	897.126033	14.056435
17.477326	905.814049	14.061453
17.680660	911.639515	14.066471
17.837008	906.038744	14.071488
17.658491	912.318518	14.076506
17.963702	914.075927	14.081523
17.778364	918.605283	14.086541
17.516139	915.067738	14.091559
17.757830	925.422139	14.096576
17.974381	928.758738	14.101594
18.292296	916.013073	14.106611
17.979876	921.786806	14.111629
17.987531	908.057799	14.116647
17.709406	906.387847	14.121664
17.410991	921.566939	14.126682
17.947749	924.591431	14.131699
17.465578	927.583066	14.136717
17.791123	927.582643	14.141735
17.998386	934.957019	14.146752
17.853476	938.164059	14.151770
18.155345	932.922335	14.156787
18.051393	938.660255	14.161805
18.110005	932.266893	14.166823
17.981141	927.537633	14.171840
17.737456	928.396423	14.176858
18.361474	932.855776	14.181875
18.179882	928.182115	14.186893
18.059019	934.389748	14.191911
18.025287	936.304408	14.196928
18.015387	932.029883	14.201946
18.499187	929.798731	14.206963
18.054119	937.044940	14.211981
18.153630	928.811627	14.216999
18.214997	935.508266	14.222016
18.104930	941.931962	14.227034
17.998961	934.601854	14.232051
18.359404	949.040258	14.237069
18.348184	956.385758	14.242087
18.618620	949.659396	14.247104
18.394816	950.947423	14.252122
18.914476	936.005224	14.257139
18.461808	939.636030	14.262157
18.616958	929.588857	14.267175
18.259948	929.190443	14.272192
18.354880	931.397371	14.277210
18.024675	922.073196	14.282227
18.461033	936.263007	14.287245
18.672773	945.375555	14.292263
18.677358	929.876584	14.297280
18.325031	930.799734	14.302298
18.405472	932.914258	14.307315
18.618599	947.804937	14.312333
18.554646	947.518399	14.317351
18.936167	959.570846	14.322368
18.797668	952.731828	14.327386
18.924238	943.831541	14.332403
18.888580	928.215798	14.337421
18.465051	930.652285	14.342439
18.828428	918.701078	14.347456
18.393936	933.869943	14.352474
18.565108	928.339427	14.357491
18.617622	942.693527	14.362509
19.055568	952.641649	14.367527
18.809203	947.097651	14.372544
18.685700	950.673729	14.377562
18.951228	954.192009	14.382579
18.884958	951.270703	14.387597
18.855260	948.321575	14.392615
19.053520	942.704758	14.397632
18.838057	950.400997	14.402650
18.897046	947.955533	14.407667
18.941697	963.926675	14.412685
18.724986	956.370909	14.417703
18.733000	959.241564	14.422720
18.850667	957.029905	14.427738
18.996156	956.044667	14.432755
18.866747	953.474084	14.437773
18.796372	959.617009	14.442791
19.030839	952.138878	14.447808
18.985801	954.642299	14.452826
19.024740	943.126923	14.457843
19.102254	950.881401	14.462861
19.142876	944.976853	14.467879
19.382278	947.940642	14.472896
19.194319	944.669169	14.477914
19.310110	940.864105	14.482931
19.098559	942.658302	14.487949
19.124586	946.062626	14.492967
19.216345	939.866041	14.497984
18.875961	947.259956	14.503002
19.259608	943.943105	14.508019
19.030310	945.528641	14.513037
19.152381	959.950753	14.518055
19.358648	962.051878	14.523072
19.232830	972.183018	14.528090
19.797066	974.351135	14.533107
19.567094	962.956776	14.538125
19.501115	955.604614	14.543143
19.703915	940.696279	14.548160
19.657913	942.988407	14.553178
19.472922	945.324404	14.558195
19.700544	940.848558	14.563213
19.291040	943.879303	14.568231
19.602167	940.864153	14.573248
19.512394	946.464152	14.578266
19.743514	939.696616	14.583283
19.862851	938.421983	14.588301
19.582505	940.119660	14.593319
19.578685	931.381822	14.598336
19.453528	945.962581	14.603354
19.509362	945.123936	14.608371
19.691594	936.502113	14.613389
19.191118	941.248110	14.618407
19.511099	950.883351	14.623424
19.538400	961.574325	14.628442
19.726029	967.171893	14.633459
19.775544	961.013479	14.638477
19.805957	971.252686	14.643495
19.940977	960.419687	14.648512
19.922449	966.772245	14.653530
19.807721	964.344530	14.658547
20.048942	963.883941	14.663565
20.056784	963.677673	14.668583
19.667674	957.562738	14.673600
19.836178	969.768491	14.678618
19.673410	974.480519	14.683635
19.995666	959.471399	14.688653
19.805425	971.237894	14.693671
19.874160	967.474911	14.698688
19.916654	964.883704	14.703706
19.701505	971.519538	14.708723
19.960350	964.034427	14.713741
19.718361	970.901688	14.718759
20.278516	960.923586	14.723776
19.879563	963.160563	14.728794
19.897641	975.834863	14.733811
20.469660	982.325276	14.738829
20.226484	982.372935	14.743847
20.567035	983.796605	14.748864
19.921247	972.148650	14.753882
20.044110	973.442323	14.758899
20.172771	981.526477	14.763917
20.067536	986.835417	14.768935
20.478183	993.663547	14.773952
20.183469	999.295674	14.778970
19.719297	993.643774	14.783987
20.318512	976.741916	14.789005
20.222834	994.363490	14.794023
20.798222	988.987376	14.799040
20.256510	982.340912	14.804058
20.229731	980.609481	14.809075
20.563115	980.333270	14.814093
20.332875	983.585247	14.819111
20.237150	989.542803	14.824128
20.436922	991.809053	14.829146
20.548930	990.226291	14.834163
20.289816	996.278879	14.839181
20.313135	990.134027	14.844199
20.539321	978.055951	14.849216
20.673187	991.766175	14.854234
20.297481	982.783617	14.859251
20.641767	998.117698	14.864269
20.472735	1010.010285	14.869287
20.806301	1009.371123	14.874304
20.898248	1013.917018	14.879322
20.645809	1002.557713	14.884339
21.042082	1002.217999	14.889357
21.047478	1001.986867	14.894375
20.990558	992.976447	14.899392
21.162575	986.615791	14.904410
20.806396	987.536391	14.909427
20.830714	969.986146	14.914445
20.752458	973.930685	14.919463
21.057857	984.300386	14.924480
20.763536	977.599383	14.929498
20.844818	974.399330	14.934515
20.955795	976.376529	14.939533
20.613882	979.339884	14.944551
21.051891	990.881723	14.949568
21.304267	1001.682625	14.954586
20.921338	995.598267	14.959603
21.355798	986.873783	14.964621
20.888599	989.408639	14.969639
21.094942	991.576028	14.974656
21.410530	981.355363	14.979674
21.134760	977.103550	14.984691
20.950276	975.216945	14.989709
21.141047	975.174521	14.994727
21.366595	979.554306	14.999744
21.389309	981.245529	15.004762
21.034006	982.339564	15.009779
21.241385	982.647994	15.014797
21.163073	987.346793	15.019815
21.438263	1002.120494	15.024832
21.361121	1000.201289	15.029850
20.974729	1006.175991	15.034867
21.660092	998.926999	15.039885
21.760457	1006.949325	15.044903
21.372860	992.240750	15.049920
21.404599	978.662552	15.054938
21.347866	991.512689	15.059955
21.466902	992.125299	15.064973
21.500398	1011.806358	15.069991
21.663242	1002.196603	15.075008
21.440024	1007.435671	15.080026
21.515873	1003.772554	15.085043
21.573770	997.527606	15.090061
21.837757	1003.065883	15.095079
21.311168	1003.369390	15.100096
21.622809	1001.042126	15.105114
21.563397	1004.071677	15.110131
21.750786	1005.023878	15.115149
21.718545	999.036053	15.120167
21.284238	1002.490422	15.125184
21.540173	1006.174321	15.130202
21.382390	1006.044496	15.135219
21.409296	999.779156	15.140237
21.358077	1004.167597	15.145255
21.539373	1006.828069	15.150272
21.644993	1021.230718	15.155290
21.654295	1028.793942	15.160307
21.929094	1031.095780	15.165325
21.957692	1037.696604	15.170343
21.911621	1036.066021	15.175360
22.114699	1033.004668	15.180378
21.899769	1031.716128	15.185395
21.999420	1024.063428	15.190413
22.295571	1033.263783	15.195431
21.988242	1023.497305	15.200448
21.943547	1019.969838	15.205466
22.070083	1035.085600	15.210483
22.191813	1040.573594	15.215501
22.083070	1031.303026	15.220519
22.386264	1034.755460	15.225536
22.172999	1024.576606	15.230554
21.861471	1035.396453	15.235571
22.062053	1023.003617	15.240589
22.153286	1030.475109	15.245607
22.444989	1022.915396	15.250624
22.219297	1024.550868	15.255642
22.444441	1028.242751	15.260659
22.265927	1023.821051	15.265677
22.346079	1017.108698	15.270695
22.155229	1020.253522	15.275712
22.310853	1021.879743	15.280730
22.075062	1022.759391	15.285747
22.542316	1016.866871	15.290765
22.463329	1023.768573	15.295783
21.838534	1024.213702	15.300800
22.206299	1019.962036	15.305818
22.162150	1018.974948	15.310835
22.143705	1016.611036	15.315853
22.262596	1028.417497	15.320871
22.332685	1040.121157	15.325888
22.583913	1040.179716	15.330906
22.461988	1050.215614	15.335923
22.490379	1045.900349	15.340941
22.746659	1041.839717	15.345959
22.664275	1048.053984	15.350976
22.830705	1045.597984	15.355994
22.567948	1054.655543	15.361011
22.761517	1044.958898	15.366029
22.528737	1043.878285	15.371047
22.725594	1038.937012	15.376064
22.738776	1035.747618	15.381082
22.532137	1049.946746	15.386099
22.682635	1042.368123	15.391117
22.743792	1043.715652	15.396135
22.815834	1044.029508	15.401152
22.785397	1037.214552	15.406170
22.996166	1058.755092	15.411187
23.177563	1051.594510	15.416205
22.980474	1045.623031	15.421223
22.799663	1040.662034	15.426240
23.022189	1049.593062	15.431258
23.331451	1060.795349	15.436275
23.329800	1055.414950	15.441293
23.161989	1049.041244	15.446311
22.813118	1054.154844	15.451328
23.252494	1044.372348	15.456346
23.058093	1049.057793	15.461363
23.218443	1057.695604	15.466381
23.038976	1056.887510	15.471399
23.064386	1071.148128	15.476416
23.327696	1061.153363	15.481434
23.259168	1057.613844	15.486451
23.398854	1058.617704	15.491469
23.474289	1064.763067	15.496487
23.295075	1061.524916	15.501504
23.488085	1058.506162	15.506522
23.591172	1074.127413	15.511539
23.302158	1052.955907	15.516557
23.144083	1053.406807	15.521575
23.386428	1060.116163	15.526592
23.473119	1057.218211	15.531610
23.658417	1055.939546	15.536627
23.541526	1061.253491	15.541645
23.596429	1060.784223	15.546663
23.841752	1060.682758	15.551680
23.349223	1057.850312	15.556698
23.869764	1068.325211	15.561715
23.482194	1067.666489	15.566733
23.327544	1058.699751	15.571751
23.317106	1059.777627	15.576768
23.730144	1061.196258	15.581786
23.738005	1067.579432	15.586803
23.668208	1060.376151	15.591821
23.777558	1056.417434	15.596839
23.831745	1057.807082	15.601856
23.922135	1054.353118	15.606874
23.987438	1058.527652	15.611891
23.584977	1050.660116	15.616909
23.527108	1055.519835	15.621927
23.482889	1051.894455	15.626944
23.630247	1061.073956	15.631962
23.557274	1066.210604	15.636979
23.857063	1075.407255	15.641997
24.146658	1086.394886	15.647015
24.150887	1081.013558	15.652032
24.169274	1080.884532	15.657050
24.126890	1083.422270	15.662067
23.973958	1087.697277	15.667085
23.863182	1088.689887	15.672103
23.968139	1083.469505	15.677120
24.005759	1081.860520	15.682138
24.188920	1088.493951	15.687155
24.161838	1086.084045	15.692173
24.159154	1083.840733	15.697191
23.816946	1082.679432	15.702208
24.327801	1088.797607	15.707226
24.131919	1089.816176	15.712243
23.993369	1086.492753	15.717261
24.129096	1080.024138	15.722279
24.454922	1091.883427	15.727296
24.499887	1096.537692	15.732314
24.259319	1096.490267	15.737331
24.362784	1103.445466	15.742349
24.852406	1108.418237	15.747367
24.796000	1099.234110	15.752384
24.456164	1087.124723	15.757402
24.166234	1099.213041	15.762419
24.542004	1099.056423	15.767437
24.621521	1102.168367	15.772455
24.067567	1113.357611	15.777472
24.259677	1111.926394	15.782490
24.243164	1107.835904	15.787507
24.371875	1114.329550	15.792525
24.644704	1101.978990	15.797543
24.674414	1103.148410	15.802560
24.717692	1095.996827	15.807578
24.732628	1105.550556	15.812595
24.655062	1111.319111	15.817613
24.701153	1115.859594	15.822631
24.927207	1133.560287	15.827648
25.287162	1135.104009	15.832666
25.007196	1130.467799	15.837683
25.279021	1119.057835	15.842701
25.004799	1101.863512	15.847719
24.864045	1099.954262	15.852736
24.834180	1096.910461	15.857754
24.952637	1095.904203	15.862771
24.969850	1101.329695	15.867789
24.856020	1099.450942	15.872807
24.818231	1113.538456	15.877824
25.246791	1116.630429	15.882842
25.238356	1121.611811	15.887859
25.417289	1123.875031	15.892877
25.312441	1107.238002	15.897895
25.115451	1110.042969	15.902912
25.313196	1113.164794	15.907930
25.413378	1114.073859	15.912947
25.232798	1109.930178	15.917965
25.551175	1089.654406	15.922983
25.226599	1102.183663	15.928000
25.539539	1097.700723	15.933018
25.436873	1095.299502	15.938035
25.015403	1094.444114	15.943053
25.450537	1103.846797	15.948071
25.359787	1114.174499	15.953088
25.282521	1115.067184	15.958106
25.569122	1121.996852	15.963123
25.480296	1125.696923	15.968141
25.723425	1116.945548	15.973159
25.379640	1123.210265	15.978176
25.572819	1115.580741	15.983194
25.491286	1113.889434	15.988211
25.185395	1124.755791	15.993229
25.669340	1115.856230	15.998247
25.648878	1120.946796	16.003264
25.975449	1124.906836	16.008282
25.966943	1116.131771	16.013299
25.730577	1126.491763	16.018317
25.672532	1116.522071	16.023335
25.423092	1131.649485	16.028352
26.034378	1121.000549	16.033370
25.704372	1125.789314	16.038387
25.522733	1122.478948	16.043405
25.450622	1133.371798	16.048423
25.463537	1152.096849	16.053440
25.806380	1145.106599	16.058458
25.482941	1148.521533	16.063475
25.548016	1151.869284	16.068493
25.910420	1147.662610	16.073511
25.743335	1160.356585	16.078528
25.833841	1165.010045	16.083546
26.093605	1173.234694	16.088563
25.992765	1175.519665	16.093581
26.301584	1173.079209	16.098599
26.257103	1173.824746	16.103616
26.619045	1172.897103	16.108634
26.536478	1176.264835	16.113651
26.465081	1171.832626	16.118669
26.670009	1170.427799	16.123687
26.453345	1164.257370	16.128704
26.081269	1153.980245	16.133722
26.148441	1164.251674	16.138739
26.548895	1173.104391	16.143757
26.663483	1170.858474	16.148775
26.849982	1170.179231	16.153792
26.865817	1166.815825	16.158810
27.022138	1149.522438	16.163827
26.855962	1147.995872	16.168845
26.767329	1139.122895	16.173863
26.817605	1140.424797	16.178880
26.655321	1145.013715	16.183898
26.441484	1135.327204	16.188915
26.334785	1140.137791	16.193933
26.506965	1134.098957	16.198951
26.323414	1135.895097	16.203968
26.640369	1137.066852	16.208986
26.637115	1137.887980	16.214003
26.614756	1142.922044	16.219021
27.048006	1152.463906	16.224039
27.123755	1156.699944	16.229056
27.089568	1145.621939	16.234074
27.025256	1144.978838	16.239091
26.787835	1144.618487	16.244109
27.119599	1135.843749	16.249127
27.078601	1136.891702	16.254144
26.765946	1135.198735	16.259162
26.888985	1129.306461	16.264179
26.679643	1152.323614	16.269197
27.088686	1151.909313	16.274215
27.138837	1161.801545	16.279232
26.877321	1160.883222	16.284250
27.316579	1157.339863	16.289267
26.984178	1162.425666	16.294285
27.154808	1154.998479	16.299303
27.170950	1162.567001	16.304320
27.337535	1169.004239	16.309338
27.095691	1165.513944	16.314355
26.651872	1163.809966	16.319373
26.802701	1157.499907	16.324391
27.298670	1177.370627	16.329408
27.623211	1178.983019	16.334426
27.859189	1173.634782	16.339443
27.326574	1172.487528	16.344461
27.444672	1165.788109	16.349479
27.558923	1174.054493	16.354496
27.711729	1183.034382	16.359514
27.866055	1173.795108	16.364531
27.566056	1168.164768	16.369549
27.752131	1161.066526	16.374567
27.578038	1160.405911	16.379584
27.452548	1158.538446	16.384602
27.640442	1174.525204	16.389619
27.895176	1180.200690	16.394637
28.179806	1185.521190	16.399655
27.728626	1171.592465	16.404672
27.473342	1169.754803	16.409690
27.648960	1170.740416	16.414707
27.676530	1176.833355	16.419725
27.704259	1173.199834	16.424743
27.760678	1171.411166	16.429760
27.715126	1174.940360	16.434778
28.091418	1173.966286	16.439795
28.164866	1183.233171	16.444813
27.919417	1173.696763	16.449831
27.758293	1173.823086	16.454848
27.861886	1179.459136	16.459866
28.067061	1172.430482	16.464883
28.013016	1176.696329	16.469901
28.160597	1172.179317	16.474919
28.427468	1178.383089	16.479936
28.360413	1183.865991	16.484954
28.275923	1178.893020	16.489971
27.894901	1173.243814	16.494989
28.336090	1175.465951	16.500007
28.655867	1184.255573	16.505024
28.578298	1180.834213	16.510042
28.462995	1172.274674	16.515059
28.760034	1177.154560	16.520077
28.633054	1171.209924	16.525095
28.475598	1163.357600	16.530112
28.458725	1170.035027	16.535130
28.724561	1173.603797	16.540147
28.254791	1171.411567	16.545165
28.325955	1176.052281	16.550183
28.620814	1173.317359	16.555200
28.198751	1167.434737	16.560218
28.566310	1171.956426	16.565235
28.769341	1191.027281	16.570253
28.715769	1194.131691	16.575271
28.975901	1195.425964	16.580288
28.997990	1184.686265	16.585306
28.749556	1174.061544	16.590323
28.933319	1174.152766	16.595341
28.733035	1168.573075	16.600359
28.845892	1178.130436	16.605376
28.497789	1190.666597	16.610394
29.048077	1192.991566	16.615411
28.950942	1194.064098	16.620429
28.834491	1182.241547	16.625447
29.135281	1185.606022	16.630464
28.671791	1195.865936	16.635482
28.976768	1189.787341	16.640499
29.097694	1194.110986	16.645517
28.903101	1197.887605	16.650535
29.261028	1196.446180	16.655552
28.841792	1198.803132	16.660570
28.860603	1189.701850	16.665587
29.062229	1198.967595	16.670605
29.116131	1210.124778	16.675623
29.368577	1218.669340	16.680640
29.084839	1217.502024	16.685658
29.187180	1217.517638	16.690675
29.058978	1209.313563	16.695693
29.450858	1213.945063	16.700711
29.426468	1215.558480	16.705728
29.514090	1218.927958	16.710746
29.360877	1214.988253	16.715763
29.537707	1223.175425	16.720781
29.238256	1221.363613	16.725799
29.570318	1226.755591	16.730816
29.575528	1226.467679	16.735834
29.454497	1217.391450	16.740851
29.479478	1222.033099	16.745869
29.589252	1231.130211	16.750887
29.671908	1236.734844	16.755904
29.687112	1239.979969	16.760922
29.951036	1239.679924	16.765939
29.872722	1243.946433	16.770957
29.682532	1242.764458	16.775975
29.935744	1229.678404	16.780992
29.852943	1234.153902	16.786010
30.042866	1231.549025	16.791027
30.041578	1235.064984	16.796045
30.249634	1230.191334	16.801063
30.280683	1233.815838	16.806080
30.443538	1241.304600	16.811098
30.436811	1221.060681	16.816115
30.083337	1211.834676	16.821133
30.026635	1213.289048	16.826151
30.414549	1222.008052	16.831168
30.428113	1220.405979	16.836186
30.194925	1205.370069	16.841203
30.178335	1207.632376	16.846221
30.044275	1201.521577	16.851239
29.970182	1209.318857	16.856256
30.071565	1225.363397	16.861274
30.420474	1230.632814	16.866291
30.314181	1228.639253	16.871309
30.251215	1239.199366	16.876327
30.491898	1228.936646	16.881344
30.515648	1233.903549	16.886362
30.807400	1229.692147	16.891379
30.747585	1230.743054	16.896397
30.337551	1239.063211	16.901415
30.720552	1238.580402	16.906432
30.573958	1235.728440	16.911450
30.535071	1228.917891	16.916467
30.522437	1228.613839	16.921485
30.499139	1226.758758	16.926503
30.494778	1221.669076	16.931520
30.361489	1229.194765	16.936538
30.371995	1247.607861	16.941555
30.802825	1254.095248	16.946573
30.512060	1267.619744	16.951591
31.188792	1264.017066	16.956608
31.082484	1268.038650	16.961626
31.521339	1263.611682	16.966643
31.075746	1257.095225	16.971661
30.696928	1258.145621	16.976679
31.356018	1250.058022	16.981696
30.752867	1251.629574	16.986714
31.340686	1246.469194	16.991731
31.121977	1245.660927	16.996749
30.909115	1248.768212	17.001767
30.832927	1251.134540	17.006784
30.767991	1253.234009	17.011802
30.935813	1249.505936	17.016819
31.249337	1254.133945	17.021837
31.237702	1271.288175	17.026855
31.701061	1271.947835	17.031872
31.658433	1281.599042	17.036890
31.446839	1272.975645	17.041907
31.669150	1269.100171	17.046925
31.592405	1255.901688	17.051943
31.666463	1250.054919	17.056960
31.696082	1245.635268	17.061978
31.459000	1247.578667	17.066995
31.394150	1255.491287	17.072013
31.824838	1254.357203	17.077031
31.729910	1261.917922	17.082048
31.629448	1271.350960	17.087066
31.796567	1273.306773	17.092083
31.951224	1268.971670	17.097101
31.694552	1272.675977	17.102119
32.102095	1266.732770	17.107136
31.561987	1279.478963	17.112154
31.458641	1273.940857	17.117171
31.478615	1272.991047	17.122189
31.010706	1278.394769	17.127207
31.607950	1277.689037	17.132224
31.977621	1304.727808	17.137242
31.988025	1294.693642	17.142259
32.341538	1300.596694	17.147277
31.991358	1308.935908	17.152295
32.147792	1292.494462	17.157312
31.914255	1298.890293	17.162330
32.484436	1294.161865	17.167347
32.512490	1291.162606	17.172365
32.144984	1296.096151	17.177383
32.291578	1295.271673	17.182400
32.142614	1294.802782	17.187418
32.342420	1293.818483	17.192435
32.401802	1295.942662	17.197453
32.394999	1301.722283	17.202471
32.731634	1289.424714	17.207488
32.224664	1299.820892	17.212506
32.537428	1289.297528	17.217523
32.667463	1288.664999	17.222541
32.679416	1289.004054	17.227559
33.098809	1288.869004	17.232576
32.767022	1286.932859	17.237594
32.518461	1287.243302	17.242611
33.155147	1289.980794	17.247629
32.819989	1286.874337	17.252647
33.018829	1279.057658	17.257664
32.843007	1291.039861	17.262682
32.685175	1290.988939	17.267699
32.827039	1275.035800	17.272717
33.040405	1280.288597	17.277735
32.782643	1281.465199	17.282752
33.121606	1281.405869	17.287770
32.896059	1284.436251	17.292787
32.784525	1282.232060	17.297805
32.733434	1281.867759	17.302823
32.805190	1278.915304	17.307840
32.726567	1284.437921	17.312858
33.140930	1291.798932	17.317875
33.423205	1308.045585	17.322893
33.401815	1304.940458	17.327911
33.122833	1300.023173	17.332928
33.217059	1310.287291	17.337946
33.015912	1309.201706	17.342963
33.334324	1307.911636	17.347981
33.370691	1311.377527	17.352999
33.473557	1303.506445	17.358016
33.515868	1306.630567	17.363034
33.246838	1318.371763	17.368051
33.460254	1301.927691	17.373069
33.174947	1303.458916	17.378087
33.462636	1303.533856	17.383104
33.992047	1297.606258	17.388122
32.988850	1306.013071	17.393139
33.350877	1310.926994	17.398157
33.874793	1321.975890	17.403175
33.924775	1322.160660	17.408192
34.259252	1328.511688	17.413210
33.638575	1314.656746	17.418227
34.084474	1320.955599	17.423245
33.759318	1319.438147	17.428263
34.269413	1309.382487	17.433280
33.888202	1316.489450	17.438298
33.800034	1322.073536	17.443315
33.991317	1316.113701	17.448333
33.874329	1329.734096	17.453351
34.059208	1323.541725	17.458368
33.881059	1328.417207	17.463386
33.844970	1333.756443	17.468403
33.928729	1327.535731	17.473421
33.903931	1327.612293	17.478439
33.993761	1326.569482	17.483456
34.087504	1324.544569	17.488474
33.921250	1341.549517	17.493491
33.998386	1348.575211	17.498509
34.136164	1354.909729	17.503527
34.437986	1351.949619	17.508544
34.580180	1345.602976	17.513562
34.583998	1358.791041	17.518579
34.882845	1352.161066	17.523597
34.560929	1353.783241	17.528615
34.566061	1352.368676	17.533632
34.785916	1351.273932	17.538650
34.921313	1351.252809	17.543667
34.886241	1350.709265	17.548685
34.758971	1351.108005	17.553703
35.056346	1352.554251	17.558720
34.707855	1345.533381	17.563738
34.557914	1349.369310	17.568755
35.029166	1343.665412	17.573773
34.672346	1345.605490	17.578791
34.860013	1341.962655	17.583808
34.757089	1351.613879	17.588826
35.028238	1349.280291	17.593843
35.462119	1348.830536	17.598861
35.005359	1364.202075	17.603879
35.200194	1348.363652	17.608896
35.247867	1345.683213	17.613914
35.043789	1342.117536	17.618931
35.270927	1348.267631	17.623949
34.987151	1346.731070	17.628967
34.935478	1348.386644	17.633984
35.021403	1356.010588	17.639002
35.053864	1350.826734	17.644019
35.347645	1367.160005	17.649037
35.390008	1362.271252	17.654055
35.549662	1360.561068	17.659072
35.400694	1357.958776	17.664090
35.463271	1368.019595	17.669107
35.751491	1364.471458	17.674125
35.414097	1367.112264	17.679143
35.535633	1363.596555	17.684160
35.400827	1361.320258	17.689178
35.518739	1365.054261	17.694195
35.690496	1361.587490	17.699213
35.490587	1368.713406	17.704231
35.114396	1370.265187	17.709248
35.663433	1378.548754	17.714266
35.421840	1387.581073	17.719283
35.920215	1389.213587	17.724301
35.683344	1398.847953	17.729319
35.584651	1393.410071	17.734336
35.742686	1385.315707	17.739354
35.261219	1385.100888	17.744371
35.851859	1406.825337	17.749389
36.344197	1413.265275	17.754407
36.128199	1412.797416	17.759424
36.329727	1411.371011	17.764442
36.064595	1420.864644	17.769459
36.232739	1413.721773	17.774477
36.260479	1413.704894	17.779495
36.428977	1420.179794	17.784512
36.226209	1415.490387	17.789530
36.387653	1416.187889	17.794547
36.337993	1412.105679	17.799565
36.608602	1409.358742	17.804583
36.672019	1413.678827	17.809600
36.853942	1412.760442	17.814618
36.569338	1417.794645	17.819635
36.523913	1407.166380	17.824653
36.636887	1404.311593	17.829671
36.618539	1407.309531	17.834688
36.860983	1406.798247	17.839706
36.849944	1419.553166	17.844723
37.272795	1407.175735	17.849741
36.601731	1416.246954	17.854759
36.812613	1397.395220	17.859776
37.190006	1399.172928	17.864794
36.983717	1412.854717	17.869811
36.899977	1404.877123	17.874829
36.933443	1415.002493	17.879847
36.892299	1407.999717	17.884864
37.107265	1402.149756	17.889882
36.908736	1406.725484	17.894899
37.433959	1407.056709	17.899917
37.288135	1406.287510	17.904935
37.071168	1412.674474	17.909952
37.188360	1403.308350	17.914970
37.324138	1402.315142	17.919987
37.156962	1394.218077	17.925005
37.293668	1413.176481	17.930023
37.128156	1430.402312	17.935040
37.552453	1426.252151	17.940058
37.632580	1436.707907	17.945075
37.158215	1441.737132	17.950093
37.564830	1434.465368	17.955111
37.738587	1434.274126	17.960128
38.001377	1426.643032	17.965146
37.432469	1438.371328	17.970163
37.489625	1429.339659	17.975181
37.675177	1424.160201	17.980199
37.377521	1431.348795	17.985216
37.747322	1431.849545	17.990234
37.468963	1431.659710	17.995251
37.668363	1433.850333	18.000269
37.461304	1434.959038	18.005287
37.667030	1449.513611	18.010304
38.275639	1447.928745	18.015322
37.969761	1443.119780	18.020339
38.360377	1449.032849	18.025357
38.434432	1454.743044	18.030375
38.318971	1449.481348	18.035392
38.381417	1441.417715	18.040410
38.109631	1449.675280	18.045427
38.444311	1448.792923	18.050445
38.417479	1448.443752	18.055463
37.988500	1448.223865	18.060480
38.585827	1444.188607	18.065498
38.307823	1451.412002	18.070515
38.802116	1442.409669	18.075533
38.467516	1451.425033	18.080551
38.229654	1446.144645	18.085568
38.428420	1437.630448	18.090586
38.518010	1447.762822	18.095603
38.752235	1445.946268	18.100621
38.563113	1437.691670	18.105639
38.797618	1445.153512	18.110656
38.527076	1443.652739	18.115674
38.567349	1446.792984	18.120691
38.477537	1443.900533	18.125709
38.689045	1438.982102	18.130727
38.766961	1461.771602	18.135744
39.055363	1458.084556	18.140762
38.917130	1473.564079	18.145779
38.880245	1476.643832	18.150797
39.245831	1462.915125	18.155815
38.824787	1477.826711	18.160832
39.105690	1463.906135	18.165850
38.954088	1469.986220	18.170867
38.579382	1461.713348	18.175885
38.941452	1466.775637	18.180903
38.782955	1472.964105	18.185920
39.187577	1485.505616	18.190938
39.055389	1496.591145	18.195955
39.288036	1496.223410	18.200973
39.019053	1490.105248	18.205991
39.319839	1502.918673	18.211008
39.779799	1497.156533	18.216026
39.823067	1500.081714	18.221043
39.539282	1495.556465	18.226061
39.949230	1499.803341	18.231079
39.484252	1502.296891	18.236096
39.725923	1494.785847	18.241114
39.592342	1496.896099	18.246131
39.578549	1493.136469	18.251149
39.821071	1498.889713	18.256167
39.961135	1507.287913	18.261184
40.042686	1492.874663	18.266202
39.969918	1496.092591	18.271219
39.863040	1506.590311	18.276237
40.218821	1510.337569	18.281255
39.804994	1514.871314	18.286272
40.252404	1512.617392	18.291290
40.262723	1516.226266	18.296307
40.547179	1512.094839	18.301325
41.020993	1509.849404	18.306343
40.616569	1490.443853	18.311360
40.083989	1479.961303	18.316378
40.636850	1472.287897	18.321395
40.390504	1478.837284	18.326413
40.701486	1476.393293	18.331431
40.681411	1476.642692	18.336448
40.408963	1471.680152	18.341466
40.607220	1489.631718	18.346483
40.256627	1483.800911	18.351501
40.754936	1475.328131	18.356519
39.988896	1474.192181	18.361536
40.466348	1485.409412	18.366554
40.679423	1498.100870	18.371571
40.540419	1508.490010	18.376589
41.042042	1510.068377	18.381607
40.908588	1503.158926	18.386624
41.159788	1490.063529	18.391642
40.827983	1502.032440	18.396659
40.713256	1502.571237	18.401677
40.856206	1503.915453	18.406695
40.925617	1508.221998	18.411712
41.265383	1501.026956	18.416730
40.879356	1494.431648	18.421747
40.886451	1504.059405	18.426765
40.844161	1498.918779	18.431783
41.041680	1524.548903	18.436800
41.321204	1522.160330	18.441818
41.235973	1525.926194	18.446835
41.460592	1530.927983	18.451853
41.965612	1530.848947	18.456871
41.327201	1535.307427	18.461888
41.568819	1520.635535	18.466906
40.923873	1521.061738	18.471923
41.875869	1531.702851	18.476941
41.588771	1525.246673	18.481959
41.340315	1523.183831	18.486976
42.051174	1517.259293	18.491994
41.902858	1512.274138	18.497011
41.842664	1517.282675	18.502029
42.101285	1516.503754	18.507047
42.038968	1512.073194	18.512064
41.956652	1510.650227	18.517082
42.051047	1510.534538	18.522099
42.114403	1519.897857	18.527117
41.950148	1513.005852	18.532135
41.665733	1518.289372	18.537152
42.073120	1514.621544	18.542170
41.745691	1513.132835	18.547187
41.727148	1533.198180	18.552205
41.703961	1532.829501	18.557223
41.647957	1548.703322	18.562240
41.908598	1544.310521	18.567258
42.074493	1559.849769	18.572275
42.226760	1573.781630	18.577293
42.734804	1554.829520	18.582311
42.623355	1565.271183	18.587328
42.904670	1564.864263	18.592346
42.818403	1553.595339	18.597363
42.752953	1558.210218	18.602381
43.310830	1545.009924	18.607399
42.735466	1537.759424	18.612416
43.135688	1525.334962	18.617434
43.251120	1522.063186	18.622451
42.955671	1537.649451	18.627469
42.951738	1534.907638	18.632487
43.156327	1538.277786	18.637504
43.243621	1533.549213	18.642522
43.204824	1526.766939	18.647539
42.871810	1524.471182	18.652557
43.081147	1523.475910	18.657575
43.021409	1535.484271	18.662592
43.072631	1527.633806	18.667610
42.947839	1527.770219	18.672627
42.979215	1521.765939	18.677645
43.047764	1532.930497	18.682663
43.189560	1537.869521	18.687680
43.507468	1547.884125	18.692698
43.601288	1552.767552	18.697715
43.660821	1556.949418	18.702733
43.701030	1553.376983	18.707751
43.507798	1567.018973	18.712768
43.606604	1552.094863	18.717786
43.592815	1547.685094	18.722803
43.742575	1550.808203	18.727821
43.576647	1545.122021	18.732839
43.224671	1542.046556	18.737856
43.185371	1549.955303	18.742874
43.618287	1547.195539	18.747891
43.550974	1557.248412	18.752909
43.657136	1571.660888	18.757927
43.863411	1575.081274	18.762944
43.832420	1588.394888	18.767962
44.166250	1571.912767	18.772979
44.114414	1579.662537	18.777997
44.356103	1579.608980	18.783015
44.202302	1577.250421	18.788032
44.018696	1582.972623	18.793050
44.548925	1575.681435	18.798067
44.368434	1582.012248	18.803085
44.556120	1580.275560	18.808103
43.941969	1583.452088	18.813120
43.907081	1580.184918	18.818138
44.552349	1579.945046	18.823155
44.580978	1599.962047	18.828173
44.984807	1591.235759	18.833191
44.882111	1594.647751	18.838208
44.640626	1592.962524	18.843226
44.964607	1596.392875	18.848243
45.100020	1593.360965	18.853261
45.200625	1570.350994	18.858279
44.636558	1566.368281	18.863296
44.701120	1568.403314	18.868314
45.126205	1578.533693	18.873331
44.965451	1587.727024	18.878349
45.395634	1591.298533	18.883367
44.956436	1596.303356	18.888384
44.825335	1587.247451	18.893402
45.171159	1591.895735	18.898419
45.008115	1599.470425	18.903437
45.157937	1581.303439	18.908455
45.140948	1586.926950	18.913472
45.115610	1588.079779	18.918490
44.911810	1585.220944	18.923507
44.581665	1589.795248	18.928525
44.971315	1604.936543	18.933543
45.226173	1616.397026	18.938560
45.204698	1611.533988	18.943578
45.425400	1611.120784	18.948595
45.159016	1613.901986	18.953613
45.430911	1633.625277	18.958631
45.776567	1640.321821	18.963648
45.639974	1646.525853	18.968666
46.068144	1636.164094	18.973683
46.063864	1649.511440	18.978701
46.135745	1644.179306	18.983719
45.939895	1637.819249	18.988736
45.880976	1638.778517	18.993754
46.085489	1632.257899	18.998771
46.104511	1637.276150	19.003789
46.156163	1639.044957	19.008807
46.482522	1630.883082	19.013824
46.190367	1636.022675	19.018842
46.501905	1636.548340	19.023859
46.225667	1641.073183	19.028877
46.327273	1630.387033	19.033895
46.668500	1631.406689	19.038912
46.689109	1630.687146	19.043930
46.749079	1616.460224	19.048947
46.703688	1626.500233	19.053965
46.645872	1628.674374	19.058983
46.653421	1630.554237	19.064000
46.460945	1626.639528	19.069018
46.982273	1617.490854	19.074035
46.572871	1627.474283	19.079053
46.654060	1623.838606	19.084071
46.566135	1625.291591	19.089088
46.554190	1625.530251	19.094106
46.940037	1638.664978	19.099123
47.126026	1649.735465	19.104141
47.017040	1652.681370	19.109159
47.595060	1645.404757	19.114176
47.382988	1652.883004	19.119194
47.629280	1644.061446	19.124211
47.328007	1650.540602	19.129229
46.905652	1642.379258	19.134247
47.218804	1645.880748	19.139264
47.262118	1651.068775	19.144282
47.678175	1644.625467	19.149299
47.621168	1655.872893	19.154317
47.299917	1651.845804	19.159335
47.598426	1648.068770	19.164352
47.406691	1654.218324	19.169370
47.931099	1638.485807	19.174387
47.319490	1640.620478	19.179405
47.689122	1644.703284	19.184423
47.449840	1643.522661	19.189440
47.502029	1662.393580	19.194458
47.873849	1663.386353	19.199475
47.885962	1663.621243	19.204493
48.141133	1668.687715	19.209511
48.125655	1665.089267	19.214528
48.000033	1667.094146	19.219546
47.865909	1664.719868	19.224563
47.832017	1666.729311	19.229581
48.055715	1665.034311	19.234599
47.906262	1669.798087	19.239616
48.247036	1687.550788	19.244634
48.409979	1690.188991	19.249651
48.610953	1693.531332	19.254669
48.265075	1685.298022	19.259687
48.457764	1691.737672	19.264704
48.195760	1694.088987	19.269722
48.473447	1687.055084	19.274739
48.671886	1688.194950	19.279757
48.578521	1686.199312	19.284775
48.689800	1694.873524	19.289792
48.507100	1701.125826	19.294810
48.863508	1695.525023	19.299827
49.279933	1701.825475	19.304845
49.129456	1701.151671	19.309863
48.915098	1694.381060	19.314880
49.042699	1705.694272	19.319898
48.953534	1704.064068	19.324915
49.049301	1713.400319	19.329933
48.895869	1708.371726	19.334951
49.086392	1711.232842	19.339968
49.225692	1707.060995	19.344986
49.301114	1705.767942	19.350003
49.687954	1706.449077	19.355021
49.303883	1710.448005	19.360039
49.622235	1711.468093	19.365056
49.564709	1715.627310	19.370074
49.539248	1699.062502	19.375091
49.692845	1709.276520	19.380109
49.576651	1717.440398	19.385127
49.677572	1702.143427	19.390144
49.466318	1711.830754	19.395162
49.734464	1726.448361	19.400179
49.734632	1733.038117	19.405197
49.699219	1737.020295	19.410215
49.858310	1733.037856	19.415232
49.899787	1738.907889	19.420250
49.972678	1733.910105	19.425267
50.120976	1738.898662	19.430285
50.009709	1740.629885	19.435303
50.272106	1732.749400	19.440320
49.882962	1737.910530	19.445338
50.255163	1750.766595	19.450355
50.638778	1751.700717	19.455373
50.729355	1751.317365	19.460391
50.869502	1754.861763	19.465408
50.560013	1756.807091	19.470426
50.665314	1752.637405	19.475443
50.786415	1754.499489	19.480461
50.350078	1757.181101	19.485479
50.703833	1752.189803	19.490496
50.355355	1756.416706	19.495514
50.493093	1748.741949	19.500531
51.228401	1753.859458	19.505549
50.865031	1765.202292	19.510567
51.098806	1755.764067	19.515584
50.982200	1754.914531	19.520602
50.799236	1758.055091	19.525619
50.721531	1757.666546	19.530637
50.841137	1781.336753	19.535655
51.407206	1774.251321	19.540672
51.765826	1782.198816	19.545690
51.359603	1779.816660	19.550707
51.882854	1770.055345	19.555725
51.638724	1778.987266	19.560743
51.781790	1776.695784	19.565760
51.866610	1774.571227	19.570778
51.903648	1761.092597	19.575795
51.496924	1747.522549	19.580813
51.433846	1762.785407	19.585831
51.716785	1761.507176	19.590848
51.301609	1773.609258	19.595866
51.795921	1758.859708	19.600883
52.231088	1758.908389	19.605901
51.273378	1763.394859	19.610919
51.931816	1767.656519	19.615936
51.798349	1769.735225	19.620954
52.178004	1769.401261	19.625971
51.986877	1769.835263	19.630989
52.136251	1768.398067	19.636007
52.322741	1780.188122	19.641024
52.329185	1793.685383	19.646042
52.204256	1795.153648	19.651059
52.506704	1793.137011	19.656077
52.415552	1789.275823	19.661095
52.693697	1787.966781	19.666112
52.482126	1800.848071	19.671130
52.380245	1793.213994	19.676147
52.521495	1792.415579	19.681165
52.304080	1787.475888	19.686183
52.673754	1790.425720	19.691200
52.663424	1790.856644	19.696218
52.770895	1792.184349	19.701235
52.909811	1796.694682	19.706253
52.513554	1820.777145	19.711271
53.001620	1817.456400	19.716288
52.966768	1816.893871	19.721306
52.861887	1819.536185	19.726323
53.236303	1812.790053	19.731341
52.822478	1815.767966	19.736359
53.111007	1811.654770	19.741376
53.030712	1815.801797	19.746394
53.009761	1822.079295	19.751411
53.247769	1832.617849	19.756429
53.217091	1841.882454	19.761447
53.384204	1837.472675	19.766464
53.813525	1841.309474	19.771482
53.516788	1836.344326	19.776499
53.770882	1827.758156	19.781517
53.463165	1841.973747	19.786535
53.983068	1852.392403	19.791552
54.071916	1853.760903	19.796570
53.929140	1856.494371	19.801587
54.345581	1857.865196	19.806605
54.168784	1861.282536	19.811623
54.285246	1860.238678	19.816640
54.131567	1863.393604	19.821658
54.360689	1861.129656	19.826675
54.218727	1853.896333	19.831693
54.341657	1854.457868	19.836711
54.512915	1855.444203	19.841728
54.549137	1856.858821	19.846746
54.450923	1857.710640	19.851763
54.734278	1856.252445	19.856781
54.399314	1853.966418	19.861799
54.760844	1843.917957	19.866816
54.608873	1853.706533	19.871834
54.553345	1854.722089	19.876851
54.722943	1848.765475	19.881869
54.559561	1852.079720	19.886887
54.539000	1851.802147	19.891904
54.548883	1863.553652	19.896922
54.687345	1874.537044	19.901939
54.605002	1872.729019	19.906957
54.870083	1890.496937	19.911975
54.646901	1884.043238	19.916992
54.840259	1883.170379	19.922010
54.638239	1895.119217	19.927027
55.159203	1902.567929	19.932045
54.925167	1908.197143	19.937063
55.172250	1902.730178	19.942080
55.244030	1906.159077	19.947098
55.286361	1909.254896	19.952115
55.746705	1917.555768	19.957133
55.828348	1922.857798	19.962151
56.101658	1925.668106	19.967168
56.425886	1926.933456	19.972186
56.250154	1915.814030	19.977203
56.007915	1897.004361	19.982221
56.064737	1900.413510	19.987239
56.131653	1891.118130	19.992256
55.966599	1890.932628	19.997274
55.897554	1897.596408	20.002291
56.207138	1889.231904	20.007309
55.951909	1898.111970	20.012327
56.290564	1900.460727	20.017344
56.316411	1918.774273	20.022362
56.083971	1919.713402	20.027379
56.615034	1926.857565	20.032397
56.419819	1924.338179	20.037415
56.546423	1918.410371	20.042432
56.604512	1923.776056	20.047450
56.251057	1923.395994	20.052467
56.508197	1904.448112	20.057485
56.155135	1917.610446	20.062503
56.466805	1933.086152	20.067520
56.390730	1935.206382	20.072538
56.575116	1940.306114	20.077555
56.741946	1929.625347	20.082573
56.790469	1943.002511	20.087591
57.178698	1956.547382	20.092608
57.609561	1954.321246	20.097626
57.291973	1959.613249	20.102643
57.988716	1952.955429	20.107661
57.609997	1937.878582	20.112679
57.599987	1933.603835	20.117696
57.306326	1934.451565	20.122714
57.219492	1929.008505	20.127731
57.658509	1941.481829	20.132749
57.594775	1958.906830	20.137767
57.444401	1961.862426	20.142784
57.731724	1956.537473	20.147802
57.685824	1960.533968	20.152819
57.818614	1953.355394	20.157837
57.655685	1954.050089	20.162855
58.256742	1952.725158	20.167872
58.214828	1954.095217	20.172890
58.035460	1954.521069	20.177907
58.354993	1947.647778	20.182925
58.316968	1958.134974	20.187943
58.060113	1944.172040	20.192960
58.551630	1951.940989	20.197978
58.340783	1952.242376	20.202995
58.399297	1951.198124	20.208013
58.263748	1957.433659	20.213031
58.559655	1978.782077	20.218048
58.766150	1980.940096	20.223066
58.540481	1981.587813	20.228083
59.071632	1975.524014	20.233101
58.631797	1968.056429	20.238119
58.694522	1974.630160	20.243136
58.638030	1972.865415	20.248154
58.303174	1981.256190	20.253171
58.521479	1979.252717	20.258189
58.682915	1991.337191	20.263207
58.715112	1997.808408	20.268224
59.529634	1980.991805	20.273242
59.129535	1991.560997	20.278259
59.344592	1988.355585	20.283277
59.273049	1983.121567	20.288295
59.386002	1981.191408	20.293312
59.386941	1986.026384	20.298330
59.320904	1992.872778	20.303347
59.937452	1989.661269	20.308365
59.454600	1985.037686	20.313383
59.522597	1987.056449	20.318400
59.863329	1983.765070	20.323418
59.694183	2001.165600	20.328435
59.945027	2003.158872	20.333453
59.842932	2007.703863	20.338471
60.025119	2012.718747	20.343488
60.141172	2007.155507	20.348506
59.824174	2006.981186	20.353523
59.925910	2010.806227	20.358541
60.294896	2015.589859	20.363559
59.806323	2004.658259	20.368576
60.271519	2004.989435	20.373594
60.288325	2012.731794	20.378611
60.630583	2022.645013	20.383629
60.520058	2025.231432	20.388647
60.705037	2033.004259	20.393664
60.931227	2029.989613	20.398682
60.584990	2023.283725	20.403699
60.888555	2027.613673	20.408717
61.060905	2026.213885	20.413735
61.136818	2025.659244	20.418752
61.168088	2012.815691	20.423770
60.999178	2021.616018	20.428787
61.029052	2022.469869	20.433805
61.799304	2012.736001	20.438823
61.168694	2017.499510	20.443840
61.333159	2012.411556	20.448858
61.161725	2011.289710	20.453875
61.609654	2014.940583	20.458893
61.508209	2018.825864	20.463911
61.070921	2004.755443	20.468928
61.381205	2003.561280	20.473946
61.466332	2010.879494	20.478963
61.503976	2009.664926	20.483981
61.805445	2015.409102	20.488999
61.508287	2028.155631	20.494016
61.709411	2031.011982	20.499034
61.382536	2043.744241	20.504051
61.504669	2047.619747	20.509069
61.654455	2041.098087	20.514087
61.836529	2057.247505	20.519104
62.123838	2059.020460	20.524122
62.073233	2066.224252	20.529139
62.069587	2072.745297	20.534157
62.156182	2068.360701	20.539175
62.000752	2062.603276	20.544192
62.351055	2062.633695	20.549210
62.418416	2083.674038	20.554227
62.390571	2088.980646	20.559245
62.544470	2093.693850	20.564263
62.593921	2095.810211	20.569280
62.693238	2088.864064	20.574298
62.668691	2093.134974	20.579315
62.819453	2093.644815	20.584333
62.928067	2094.192821	20.589351
62.866000	2117.263883	20.594368
63.065919	2118.895889	20.599386
63.209573	2120.148517	20.604403
63.445868	2116.390601	20.609421
63.265664	2111.848965	20.614439
63.140855	2120.762360	20.619456
63.395632	2110.620016	20.624474
63.131614	2116.746336	20.629491
63.352311	2121.729969	20.634509
63.476304	2115.259665	20.639527
63.311878	2119.792357	20.644544
63.703983	2119.409097	20.649562
63.980350	2139.864450	20.654579
64.141364	2147.243418	20.659597
63.804083	2142.287693	20.664615
63.854230	2141.730773	20.669632
64.219430	2136.137925	20.674650
63.977447	2132.619056	20.679667
64.094496	2141.106374	20.684685
64.166819	2131.481792	20.689703
64.001416	2137.968239	20.694720
64.198812	2129.892622	20.699738
64.303748	2140.366994	20.704755
63.987896	2143.020316	20.709773
64.551935	2153.542695	20.714791
64.463340	2162.734483	20.719808
64.409992	2157.030466	20.724826
64.489724	2156.967567	20.729843
64.985438	2159.367496	20.734861
64.716551	2155.123789	20.739879
64.484926	2165.104909	20.744896
64.895019	2173.230722	20.749914
64.783574	2191.553433	20.754931
64.953820	2189.450160	20.759949
65.258147	2189.276327	20.764967
65.169020	2185.843961	20.769984
65.564629	2176.964031	20.775002
65.211711	2181.892375	20.780019
65.564519	2178.207718	20.785037
65.379069	2168.756058	20.790055
65.141451	2181.739539	20.795072
65.737130	2200.841479	20.800090
65.788887	2197.705800	20.805107
66.131189	2201.348012	20.810125
66.190495	2195.304414	20.815143
66.143555	2208.649392	20.820160
66.112616	2203.247988	20.825178
66.052541	2205.652945	20.830195
66.332823	2209.090263	20.835213
66.763667	2195.394959	20.840231
66.445303	2204.562802	20.845248
66.507191	2199.557144	20.850266
66.098837	2197.522431	20.855283
66.177152	2207.350863	20.860301
66.344408	2201.394501	20.865319
66.178301	2204.365226	20.870336
66.518385	2192.344235	20.875354
66.329346	2205.253844	20.880371
66.305676	2214.612225	20.885389
66.685042	2223.039546	20.890407
66.244049	2224.696233	20.895424
66.747510	2227.865038	20.900442
66.685877	2236.162627	20.905459
66.806057	2243.311328	20.910477
67.119711	2247.582940	20.915495
67.019809	2250.944121	20.920512
67.048852	2247.900362	20.925530
67.431422	2250.778817	20.930547
67.588675	2248.576579	20.935565
67.694424	2242.244798	20.940583
67.463482	2245.506578	20.945600
67.499759	2248.524503	20.950618
67.546940	2250.265666	20.955635
67.630783	2260.585610	20.960653
67.574952	2262.841573	20.965671
67.479702	2283.629893	20.970688
67.775354	2269.804222	20.975706
67.864217	2267.518014	20.980723
67.932069	2265.983089	20.985741
67.989782	2274.460829	20.990759
68.331325	2278.986878	20.995776
68.365709	2289.428206	21.000794
68.625378	2294.749794	21.005811
68.792005	2302.244723	21.010829
68.741389	2287.867322	21.015847
68.423233	2284.208866	21.020864
68.949595	2289.488668	21.025882
68.774452	2301.332570	21.030899
68.573820	2301.711264	21.035917
68.861739	2290.736732	21.040935
68.669324	2299.272610	21.045952
68.636027	2293.669559	21.050970
68.600388	2292.965115	21.055987
68.723019	2296.922655	21.061005
68.679855	2297.794275	21.066023
69.509282	2323.531683	21.071040
69.231112	2314.103941	21.076058
69.292905	2320.838906	21.081075
69.190760	2320.129100	21.086093
69.402100	2322.242217	21.091111
69.326286	2318.056591	21.096128
69.753087	2324.652310	21.101146
69.741473	2332.566532	21.106163
69.610762	2343.437737	21.111181
70.107753	2333.045861	21.116199
70.254775	2341.474923	21.121216
69.894449	2332.331468	21.126234
70.146349	2334.163652	21.131251
69.872572	2335.194493	21.136269
70.200771	2334.338360	21.141287
70.144990	2332.428288	21.146304
70.319156	2335.541399	21.151322
70.673458	2334.018397	21.156339
70.826369	2333.022455	21.161357
70.785126	2331.974873	21.166375
70.529655	2325.690190	21.171392
70.679701	2331.707524	21.176410
70.607869	2340.940961	21.181427
70.524838	2358.246285	21.186445
70.758459	2351.086472	21.191463
70.698049	2349.451703	21.196480
71.013993	2345.734915	21.201498
71.047685	2345.799161	21.206515
71.039992	2359.772476	21.211533
71.113163	2363.854555	21.216551
71.345996	2382.650589	21.221568
71.014761	2379.050971	21.226586
71.304810	2378.153472	21.231603
71.046438	2376.170985	21.236621
71.141564	2379.754121	21.241639
71.547826	2398.137955	21.246656
71.456197	2401.201194	21.251674
72.081786	2395.595876	21.256691
72.062652	2404.006815	21.261709
72.290675	2395.856846	21.266727
72.335280	2399.116511	21.271744
72.232083	2390.671267	21.276762
72.555164	2388.083236	21.281779
72.575798	2387.745547	21.286797
72.694069	2384.176497	21.291815
72.560163	2390.099470	21.296832
72.463528	2395.902987	21.301850
72.889114	2392.109045	21.306867
72.627739	2386.292368	21.311885
73.232172	2389.003529	21.316903
73.075164	2391.515225	21.321920
72.727546	2389.666651	21.326938
72.945311	2380.221139	21.331955
72.972636	2387.886266	21.336973
73.191298	2376.862567	21.341991
73.121266	2378.218126	21.347008
72.880814	2385.514913	21.352026
73.167255	2385.637398	21.357043
73.032189	2390.029846	21.362061
73.691628	2387.521671	21.367079
73.311362	2389.374004	21.372096
73.200977	2400.863810	21.377114
73.507266	2400.213098	21.382131
73.527508	2407.289151	21.387149
73.810744	2397.782875	21.392167
73.809369	2396.126229	21.397184
73.801219	2406.094561	21.402202
73.854669	2406.420824	21.407219
73.728519	2425.273146	21.412237
73.848883	2424.575816	21.417255
73.931936	2434.558280	21.422272
73.616508	2431.628426	21.427290
74.014295	2432.112199	21.432307
73.839000	2452.805947	21.437325
73.950862	2449.865954	21.442343
73.963569	2454.049055	21.447360
74.113244	2476.210004	21.452378
74.373250	2483.011813	21.457395
74.255858	2485.416319	21.462413
74.920318	2482.711666	21.467431
74.646307	2488.047492	21.472448
74.798840	2504.066228	21.477466
74.837673	2506.679812	21.482483
74.967277	2517.658675	21.487501
75.196786	2509.751443	21.492519
75.114910	2512.765831	21.497536
75.176232	2525.150402	21.502554
75.346088	2536.037754	21.507571
75.333993	2545.981533	21.512589
75.743982	2536.613131	21.517607
75.603913	2537.963895	21.522624
75.616723	2541.512619	21.527642
75.638066	2527.780227	21.532659
75.604240	2543.121223	21.537677
75.776073	2555.829362	21.542695
76.119527	2560.411993	21.547712
76.120839	2565.142915	21.552730
76.368745	2554.660536	21.557747
75.787336	2555.666996	21.562765
76.408891	2559.013040	21.567783
76.593746	2566.420007	21.572800
76.683197	2578.579278	21.577818
76.584785	2581.517365	21.582835
76.608625	2587.172666	21.587853
76.854558	2581.279599	21.592871
76.839064	2581.342083	21.597888
76.598353	2581.663939	21.602906
76.906147	2575.874802	21.607923
77.134057	2586.996112	21.612941
76.763150	2592.145157	21.617959
77.054318	2582.183059	21.622976
76.660798	2596.630460	21.627994
77.352171	2600.852447	21.633011
77.339165	2606.204225	21.638029
77.515252	2593.725774	21.643047
77.636512	2594.448557	21.648064
77.418415	2599.797749	21.653082
77.734733	2606.262544	21.658099
77.664219	2621.195902	21.663117
77.804100	2627.877717	21.668135
78.413448	2623.786664	21.673152
78.015073	2621.633560	21.678170
78.682374	2615.623966	21.683187
78.350530	2628.186984	21.688205
78.351043	2618.049474	21.693223
78.457262	2613.781604	21.698240
78.450526	2612.154183	21.703258
78.800740	2611.995251	21.708275
78.484651	2618.710628	21.713293
78.736228	2609.019833	21.718311
78.874299	2609.058258	21.723328
78.471864	2606.896324	21.728346
78.928932	2613.092891	21.733363
78.762384	2619.705936	21.738381
78.783177	2623.329172	21.743399
79.057365	2637.709867	21.748416
79.144156	2639.792038	21.753434
79.308107	2641.322419	21.758451
79.250205	2648.568618	21.763469
79.043122	2642.364614	21.768487
79.452843	2652.580071	21.773504
79.413128	2664.728076	21.778522
79.521628	2670.016650	21.783539
79.653187	2668.964068	21.788557
79.731369	2672.439453	21.793575
79.634941	2666.915612	21.798592
79.707854	2684.136850	21.803610
80.087196	2682.613053	21.808627
79.820414	2688.231859	21.813645
79.831852	2685.544274	21.818663
80.280144	2688.554531	21.823680
80.075756	2706.257941	21.828698
80.530634	2708.288762	21.833715
80.765844	2717.007175	21.838733
80.504773	2699.869220	21.843751
81.010093	2707.948797	21.848768
80.725283	2710.698334	21.853786
80.826510	2707.008801	21.858803
80.807475	2712.440459	21.863821
80.816059	2704.766594	21.868839
81.513519	2721.012606	21.873856
81.373992	2733.460349	21.878874
81.073408	2735.035114	21.883891
81.694570	2728.934870	21.888909
81.573685	2725.699902	21.893927
81.826079	2719.515411	21.898944
81.624777	2732.326322	21.903962
81.817201	2729.099076	21.908979
82.043934	2727.829585	21.913997
81.802798	2724.711298	21.919015
81.940073	2722.281733	21.924032
81.952568	2724.536518	21.929050
82.295884	2718.296753	21.934067
82.188369	2724.676499	21.939085
81.894321	2736.274199	21.944103
82.507635	2743.951820	21.949120
82.396357	2743.956720	21.954138
82.862763	2753.311191	21.959155
82.732849	2746.959345	21.964173
82.644469	2759.768364	21.969191
82.538664	2744.976319	21.974208
82.723709	2753.087158	21.979226
82.612782	2740.413704	21.984243
82.811415	2757.062986	21.989261
83.042443	2774.581467	21.994279
83.213088	2772.995676	21.999296
82.931617	2787.454080	22.004314
83.048499	2770.420963	22.009331
83.300761	2763.649431	22.014349
83.651373	2766.561384	22.019367
83.799568	2760.260646	22.024384
83.623795	2762.857393	22.029402
83.853610	2777.456615	22.034419
83.907459	2785.973076	22.039437
83.762004	2787.390982	22.044455
84.083277	2786.532758	22.049472
83.906568	2794.637170	22.054490
84.065725	2786.087512	22.059507
84.129255	2780.374455	22.064525
84.044485	2786.176237	22.069543
84.464455	2785.968502	22.074560
84.693713	2800.826636	22.079578
84.779712	2800.223049	22.084595
85.135428	2797.636159	22.089613
85.112301	2801.200033	22.094631
85.080866	2795.931088	22.099648
85.339227	2800.492396	22.104666
85.029680	2793.247075	22.109683
85.391909	2790.681259	22.114701
85.289482	2792.871998	22.119719
85.552232	2797.852388	22.124736
85.311576	2797.827059	22.129754
85.731096	2799.165918	22.134771
85.834661	2794.440777	22.139789
85.046638	2800.125501	22.144807
85.600730	2786.183197	22.149824
85.565668	2797.576238	22.154842
85.370835	2795.302850	22.159859
85.500848	2802.484951	22.164877
85.632388	2812.387436	22.169895
85.848446	2811.517290	22.174912
86.171865	2812.363062	22.179930
86.454535	2824.984590	22.184947
86.367088	2841.697710	22.189965
86.249248	2843.486879	22.194983
86.471539	2849.401538	22.200000
86.607505	2856.869941	22.205018
86.531934	2848.120317	22.210035
86.597239	2843.350658	22.215053
86.475649	2855.205470	22.220071
86.967341	2864.054204	22.225088
87.036785	2868.114889	22.230106
86.913116	2868.730874	22.235123
86.825387	2870.180772	22.240141
86.818110	2884.176522	22.245159
87.246469	2886.666010	22.250176
87.433965	2895.657105	22.255194
87.485354	2898.615960	22.260211
87.180095	2897.972672	22.265229
87.277957	2911.926721	22.270247
87.549206	2919.591731	22.275264
87.620571	2920.880991	22.280282
87.599368	2923.803881	22.285299
87.966385	2924.077869	22.290317
87.947492	2935.427434	22.295335
88.320117	2934.539065	22.300352
88.388126	2938.906141	22.305370
88.526554	2940.169115	22.310387
88.863587	2935.609355	22.315405
88.438200	2934.823920	22.320423
89.040213	2923.869231	22.325440
89.046788	2922.564784	22.330458
88.977329	2925.116491	22.335475
88.884202	2928.164273	22.340493
88.356954	2938.615066	22.345511
89.183380	2947.215713	22.350528
89.135852	2954.239475	22.355546
89.459751	2963.546947	22.360563
89.510787	2950.958436	22.365581
89.342770	2964.982589	22.370599
89.491069	2965.966272	22.375616
89.729976	2956.835924	22.380634
89.569999	2977.448969	22.385651
89.742490	2978.813919	22.390669
89.633310	2988.302879	22.395687
89.959941	2981.667956	22.400704
90.117894	2987.513836	22.405722
90.088544	2985.769988	22.410739
90.347057	2989.614863	22.415757
90.258013	3006.738692	22.420775
90.518792	3006.050902	22.425792
90.473476	3007.153296	22.430810
90.706497	3021.345063	22.435827
90.395345	3009.807463	22.440845
90.591044	3021.432769	22.445863
90.545496	3019.577832	22.450880
90.916972	3030.834734	22.455898
90.823982	3030.827300	22.460915
91.277032	3024.800641	22.465933
90.922898	3033.993444	22.470951
91.100641	3039.186061	22.475968
91.311472	3050.278771	22.480986
91.383547	3051.220746	22.486003
91.802530	3057.082565	22.491021
91.369132	3056.692906	22.496039
91.730497	3060.799428	22.501056
92.146399	3080.309220	22.506074
91.962312	3078.346578	22.511091
92.687949	3075.534413	22.516109
92.562279	3090.195896	22.521127
92.521969	3075.295476	22.526144
92.436289	3082.053830	22.531162
92.404766	3079.524415	22.536179
92.405771	3075.673761	22.541197
92.196929	3084.080021	22.546215
92.756457	3093.098146	22.551232
92.692367	3106.509599	22.556250
92.736697	3106.692118	22.561267
92.592947	3101.263932	22.566285
92.611370	3116.474137	22.571303
92.898437	3122.460800	22.576320
93.227824	3123.586557	22.581338
93.104353	3135.773251	22.586355
93.561671	3128.922113	22.591373
93.341183	3139.015649	22.596391
93.323075	3135.748723	22.601408
93.832935	3143.158665	22.606426
93.551357	3148.603182	22.611443
94.096649	3148.243248	22.616461
93.910646	3158.236705	22.621479
93.820349	3174.227801	22.626496
94.480806	3174.102322	22.631514
95.033178	3165.364630	22.636531
95.556252	3159.617329	22.641549
94.979336	3147.455313	22.646567
95.055817	3130.819559	22.651584
95.338936	3124.175620	22.656602
95.194905	3121.872137	22.661619
95.788815	3124.812312	22.666637
95.724023	3125.936701	22.671655
95.328124	3127.955679	22.676672
95.472587	3121.437621	22.681690
95.625616	3125.589424	22.686707
95.555103	3122.330710	22.691725
95.451169	3124.101947	22.696743
95.346006	3117.850247	22.701760
95.504002	3120.625157	22.706778
95.421972	3118.583396	22.711795
95.727828	3129.348801	22.716813
95.463054	3141.175733	22.721831
95.611743	3145.239846	22.726848
95.759552	3149.566066	22.731866
95.860996	3157.434531	22.736883
96.309001	3164.090364	22.741901
96.360927	3177.957130	22.746919
96.387825	3177.287040	22.751936
96.361456	3183.483799	22.756954
96.438175	3180.059977	22.761971
96.747450	3180.141018	22.766989
96.676835	3201.895501	22.772007
96.902692	3207.973845	22.777024
97.079197	3211.162492	22.782042
96.608667	3209.939086	22.787059
97.101396	3219.119240	22.792077
96.767784	3235.369448	22.797095
97.217620	3238.578402	22.802112
97.334368	3236.587546	22.807130
97.587518	3252.247153	22.812147
97.419875	3254.173571	22.817165
97.396877	3265.817517	22.822183
97.406991	3266.207399	22.827200
97.489086	3273.207820	22.832218
97.595945	3282.653618	22.837235
98.111770	3290.346749	22.842253
98.087169	3302.417065	22.847271
98.060148	3310.987476	22.852288
98.248578	3311.930173	22.857306
98.332565	3320.707290	22.862323
98.559055	3336.645742	22.867341
98.652497	3343.625475	22.872359
99.023056	3343.488602	22.877376
98.934366	3338.080125	22.882394
98.869416	3336.310258	22.887411
99.279583	3346.791168	22.892429
99.447787	3360.169572	22.897447
98.908678	3364.767590	22.902464
99.898833	3356.349440	22.907482
99.650197	3371.393387	22.912499
99.909522	3372.141916	22.917517
99.615640	3367.955492	22.922535
99.361216	3384.521678	22.927552
99.500961	3385.733977	22.932570
99.772168	3387.743154	22.937587
99.777713	3399.407965	22.942605
100.302864	3409.637332	22.947623
100.338077	3407.097416	22.952640
100.538181	3401.593173	22.957658
100.540142	3409.092268	22.962675
100.559162	3412.630721	22.967693
100.724109	3422.471495	22.972711
100.967705	3432.224201	22.977728
101.287440	3416.531677	22.982746
101.523936	3425.726831	22.987763
101.388411	3420.303572	22.992781
101.545082	3417.182807	22.997799
101.242225	3418.107792	23.002816
101.540135	3416.337881	23.007834
101.775472	3423.143912	23.012851
101.429378	3420.067197	23.017869
102.002896	3427.681911	23.022887
101.973454	3443.231301	23.027904
102.112880	3437.812304	23.032922
102.072839	3445.254869	23.037939
102.315487	3444.715094	23.042957
102.535916	3439.845225	23.047975
102.308861	3450.435499	23.052992
102.031089	3440.113875	23.058010
102.366518	3454.851757	23.063027
102.551182	3458.844023	23.068045
102.844377	3462.443688	23.073063
102.703695	3464.126026	23.078080
102.827003	3471.265257	23.083098
103.134393	3482.409387	23.088115
102.915758	3495.406618	23.093133
102.931458	3492.752963	23.098151
102.897806	3492.764639	23.103168
103.846289	3490.091095	23.108186
104.315145	3498.287213	23.113203
104.400573	3499.697407	23.118221
104.636342	3497.946692	23.123239
104.569928	3486.910168	23.128256
104.477577	3475.558929	23.133274
104.379923	3466.897684	23.138291
104.224094	3475.983890	23.143309
104.447499	3480.781258	23.148327
104.536167	3496.886633	23.153344
104.597958	3493.809127	23.158362
104.608639	3495.846509	23.163379
104.770519	3491.724370	23.168397
105.002875	3500.651927	23.173415
105.039504	3505.548002	23.178432
105.455196	3517.195975	23.183450
105.146401	3521.641165	23.188467
105.402044	3516.292313	23.193485
105.596223	3517.944287	23.198503
105.523997	3514.253358	23.203520
105.640090	3507.165160	23.208538
105.972464	3514.552563	23.213555
106.005400	3511.220759	23.218573
106.096092	3523.064843	23.223591
105.814565	3536.498057	23.228608
106.360676	3540.989221	23.233626
106.339410	3542.750702	23.238643
106.175611	3541.037334	23.243661
106.554250	3545.731491	23.248679
106.212341	3549.667399	23.253696
106.553349	3559.679511	23.258714
106.646189	3567.656817	23.263731
106.693069	3562.959295	23.268749
106.541234	3567.477751	23.273767
106.689256	3589.577202	23.278784
106.883646	3598.722228	23.283802
107.209325	3600.467234	23.288819
107.282005	3616.038648	23.293837
107.224456	3623.417746	23.298855
107.216114	3624.785828	23.303872
107.499436	3631.461324	23.308890
107.763032	3643.581405	23.313907
107.798999	3652.798623	23.318925
107.955758	3655.501214	23.323943
107.792297	3649.473094	23.328960
108.103616	3654.057886	23.333978
108.347398	3673.295436	23.338995
108.628225	3677.907106	23.344013
108.760746	3672.618531	23.349031
108.793988	3672.954296	23.354048
108.952047	3675.195863	23.359066
109.020115	3674.112139	23.364083
108.914739	3668.485234	23.369101
108.965163	3684.937652	23.374119
109.085502	3699.520053	23.379136
109.102739	3694.861861	23.384154
109.026223	3697.395844	23.389171
109.148732	3702.505773	23.394189
109.670732	3711.602685	23.399207
109.983999	3715.079316	23.404224
109.817899	3720.528006	23.409242
109.967196	3719.762968	23.414259
110.128195	3723.828440	23.419277
110.198706	3734.328071	23.424295
110.034758	3744.671905	23.429312
110.378355	3743.743858	23.434330
110.288888	3747.580288	23.439347
110.583562	3748.888279	23.444365
110.936182	3752.803796	23.449383
110.919264	3774.102353	23.454400
110.956123	3758.649545	23.459418
111.075461	3756.200559	23.464435
110.823717	3766.738071	23.469453
111.062276	3771.829838	23.474471
111.326505	3795.742012	23.479488
111.682632	3790.080641	23.484506
111.520237	3788.329153	23.489523
111.718249	3795.374743	23.494541
112.092215	3801.521618	23.499559
111.716891	3820.076703	23.504576
112.193041	3814.579589	23.509594
112.259435	3816.204265	23.514611
111.885657	3816.051440	23.519629
112.522801	3826.528633	23.524647
112.454668	3836.892228	23.529664
112.805542	3839.173047	23.534682
112.850594	3838.563215	23.539699
113.009982	3844.144016	23.544717
112.984275	3846.231327	23.549735
113.053495	3861.027030	23.554752
113.364543	3864.033741	23.559770
113.188500	3862.410638	23.564787
113.176579	3864.947150	23.569805
113.323754	3874.847769	23.574823
113.519797	3893.322882	23.579840
113.435405	3887.004535	23.584858
113.677752	3893.083683	23.589875
113.789095	3916.896872	23.594893
114.126039	3919.877441	23.599911
113.802826	3924.681657	23.604928
114.009001	3928.241391	23.609946
114.243268	3939.785494	23.614963
114.203305	3951.988061	23.619981
114.701446	3947.014575	23.624999
114.476529	3968.270195	23.630016
114.373989	3977.499810	23.635034
114.865320	3981.440990	23.640051
115.006189	3987.700201	23.645069
115.410751	3991.276212	23.650087
115.733859	3994.770294	23.655104
115.599487	4001.565027	23.660122
115.605526	4004.973062	23.665139
115.433846	4006.811812	23.670157
115.877630	4016.653413	23.675175
115.823764	4029.069687	23.680192
115.905687	4018.675596	23.685210
116.327146	4020.762309	23.690227
116.189034	4023.700536	23.695245
116.754688	4007.987912	23.700263
116.479233	4023.579498	23.705280
116.668051	4031.482001	23.710298
116.776145	4034.416377	23.715315
116.792051	4037.769213	23.720333
117.132206	4033.697932	23.725351
117.067213	4033.285249	23.730368
116.959490	4040.470370	23.735386
117.314699	4057.200482	23.740403
116.860506	4068.552672	23.745421
117.452284	4066.051721	23.750439
117.495892	4081.808005	23.755456
117.573639	4083.831789	23.760474
117.852398	4083.835551	23.765491
117.550008	4097.250353	23.770509
117.951159	4103.383602	23.775527
118.055235	4114.354811	23.780544
118.071103	4120.349576	23.785562
118.671967	4111.234537	23.790579
118.239034	4123.697639	23.795597
118.868010	4145.419403	23.800615
118.966984	4146.489791	23.805632
118.951138	4148.746037	23.810650
119.636895	4144.399637	23.815667
119.115923	4136.353608	23.820685
119.271697	4141.259596	23.825703
119.515864	4159.329733	23.830720
119.404288	4159.457779	23.835738
119.901763	4162.687845	23.840755
119.754098	4163.336039	23.845773
120.012070	4159.145036	23.850791
119.975148	4184.086547	23.855808
119.966671	4183.371460	23.860826
120.213406	4183.471777	23.865843
120.168534	4198.645462	23.870861
120.354260	4202.044321	23.875879
120.755411	4212.467176	23.880896
120.371989	4214.455908	23.885914
120.264538	4219.384219	23.890931
120.777718	4232.706064	23.895949
120.824848	4231.366762	23.900967
121.357672	4251.607574	23.905984
121.203549	4255.971894	23.911002
121.595013	4263.523951	23.916019
121.888016	4264.144142	23.921037
121.815959	4260.958063	23.926055
121.839538	4270.783570	23.931072
122.191440	4281.312030	23.936090
122.275067	4283.344384	23.941107
122.258825	4286.178336	23.946125
122.647319	4290.265110	23.951143
122.665060	4282.248247	23.956160
122.682505	4287.870361	23.961178
122.686227	4299.334025	23.966195
122.665353	4314.213655	23.971213
123.039100	4309.931882	23.976231
123.026738	4311.423746	23.981248
122.794966	4322.627614	23.986266
123.211033	4332.107584	23.991283
123.367371	4340.596095	23.996301
122.895201	4348.728551	24.001319
123.191384	4365.881690	24.006336
123.438621	4370.120027	24.011354
123.750283	4380.702196	24.016371
123.723096	4390.879774	24.021389
124.223395	4384.848424	24.026407
124.653359	4388.572044	24.031424
124.104893	4390.779196	24.036442
124.547979	4400.131867	24.041459
124.713947	4418.028283	24.046477
125.076262	4410.093106	24.051495
125.001414	4408.637173	24.056512
124.775898	4415.667291	24.061530
124.956333	4417.037421	24.066547
125.422597	4433.302266	24.071565
125.708866	4435.852114	24.076583
125.497881	4436.920576	24.081600
125.808233	4434.299533	24.086618
126.096293	4436.261998	24.091635
125.996900	4436.192436	24.096653
126.107605	4440.972996	24.101671
126.394039	4448.541585	24.106688
126.400239	4460.825642	24.111706
126.545332	4460.793531	24.116723
126.866727	4464.755130	24.121741
126.943715	4463.385881	24.126759
126.796829	4458.828960	24.131776
126.504165	4464.313483	24.136794
126.817435	4480.034177	24.141811
127.110220	4491.159123	24.146829
127.123912	4490.598374	24.151847
127.513427	4496.941908	24.156864
127.695772	4513.106109	24.161882
127.733463	4517.386780	24.166899
127.660396	4521.135578	24.171917
127.563421	4516.652892	24.176935
127.824897	4524.727302	24.181952
127.823529	4544.660732	24.186970
128.426934	4537.584167	24.191987
128.627363	4538.976426	24.197005
128.829295	4541.640508	24.202023
129.454377	4536.138785	24.207040
128.996991	4532.855203	24.212058
128.965796	4544.416030	24.217075
129.338765	4540.860314	24.222093
129.608130	4543.643248	24.227111
129.634162	4554.128227	24.232128
129.278854	4570.446155	24.237146
129.723451	4557.334025	24.242163
129.931779	4569.671713	24.247181
129.730395	4571.208994	24.252199
130.045637	4580.856402	24.257216
129.962504	4594.682282	24.262234
130.225343	4589.982225	24.267251
130.339160	4600.311436	24.272269
130.761344	4612.991270	24.277287
130.541494	4618.088809	24.282304
130.658262	4628.291314	24.287322
130.919778	4625.384341	24.292339
130.888324	4638.318341	24.297357
131.261938	4652.947054	24.302375
131.287836	4656.853983	24.307392
131.141903	4654.020310	24.312410
131.299082	4666.189313	24.317427
131.774352	4676.240984	24.322445
131.588798	4678.845847	24.327463
132.029828	4680.793844	24.332480
131.791067	4700.606812	24.337498
132.481106	4697.629535	24.342515
132.388049	4707.126336	24.347533
132.286322	4702.518088	24.352551
132.529023	4711.788681	24.357568
132.794082	4726.829024	24.362586
133.172424	4731.580356	24.367603
133.156927	4728.858809	24.372621
133.027620	4728.282578	24.377639
133.361892	4733.893072	24.382656
133.266933	4755.965725	24.387674
133.330686	4757.111111	24.392691
133.397085	4756.602070	24.397709
133.353047	4761.116558	24.402727
133.826565	4769.975394	24.407744
133.735489	4777.650613	24.412762
134.073019	4784.021332	24.417779
133.778829	4796.602042	24.422797
133.974450	4814.680438	24.427815
134.437484	4813.705220	24.432832
134.317137	4842.483252	24.437850
134.423794	4851.093420	24.442867
134.822180	4855.339756	24.447885
134.906201	4863.442119	24.452903
135.448801	4864.212621	24.457920
135.624498	4864.380890	24.462938
135.641078	4858.046385	24.467955
135.894963	4876.617603	24.472973
135.953396	4890.759277	24.477991
136.291355	4875.744453	24.483008
136.072985	4888.992002	24.488026
136.203945	4881.086554	24.493043
136.428036	4883.946078	24.498061
136.542555	4906.784698	24.503079
136.809444	4907.907738	24.508096
136.791232	4906.979503	24.513114
136.905737	4911.232449	24.518131
136.943447	4918.259400	24.523149
137.175344	4934.602449	24.528167
137.305831	4933.205843	24.533184
137.096959	4939.864240	24.538202
137.691435	4939.152512	24.543219
138.027783	4946.618794	24.548237
138.204340	4950.849402	24.553255
138.307685	4951.755013	24.558272
137.985420	4943.671177	24.563290
138.236252	4960.440573	24.568307
138.621140	4964.101932	24.573325
138.424524	4973.842368	24.578343
138.736654	4967.281598	24.583360
138.592718	4986.114116	24.588378
139.038062	4983.957955	24.593395
139.392683	4990.395514	24.598413
139.460800	5007.206204	24.603431
139.420432	5000.100903	24.608448
139.635054	5021.904418	24.613466
139.448622	5026.892668	24.618483
139.406591	5028.461840	24.623501
139.414993	5036.771834	24.628519
139.902324	5043.277003	24.633536
140.040997	5060.171386	24.638554
140.221863	5072.687329	24.643571
140.435947	5077.600219	24.648589
140.368953	5092.083669	24.653607
140.697168	5090.583474	24.658624
140.682934	5108.010064	24.663642
140.834686	5112.437146	24.668659
141.498987	5110.941114	24.673677
141.184382	5138.228578	24.678695
141.480001	5142.661538	24.683712
141.760956	5147.971169	24.688730
141.356702	5146.614132	24.693747
141.843091	5163.144789	24.698765
141.673537	5165.819815	24.703783
142.356595	5162.755175	24.708800
142.198297	5186.132471	24.713818
142.281661	5201.545741	24.718835
142.381614	5203.035865	24.723853
142.684757	5197.344483	24.728871
142.779948	5208.358780	24.733888
142.743350	5215.318572	24.738906
142.745835	5225.621388	24.743923
143.002373	5236.982902	24.748941
142.987053	5252.515844	24.753959
143.221437	5247.428659	24.758976
143.105870	5267.705900	24.763994
143.354950	5280.934161	24.769011
143.673419	5291.446351	24.774029
144.300809	5284.207913	24.779047
144.725921	5281.253111	24.784064
144.954003	5292.196134	24.789082
144.966892	5289.179649	24.794099
145.159902	5290.039663	24.799117
145.245163	5298.239880	24.804135
145.557098	5310.915379	24.809152
145.735473	5305.963218	24.814170
145.845754	5302.202296	24.819187
146.132447	5300.326639	24.824205
146.382192	5305.600171	24.829223
146.839977	5303.416772	24.834240
146.350399	5297.685409	24.839258
146.659947	5297.381318	24.844275
146.944538	5291.796982	24.849293
146.642585	5290.127186	24.854311
146.869756	5293.696528	24.859328
146.765039	5297.406251	24.864346
147.019241	5294.623427	24.869363
147.040488	5291.577222	24.874381
146.591717	5308.418664	24.879399
146.963986	5320.450240	24.884416
147.188411	5326.946195	24.889434
147.359371	5336.184154	24.894451
147.714421	5348.426783	24.899469
147.315479	5355.033036	24.904487
147.504141	5372.510163	24.909504
147.704459	5374.164504	24.914522
147.602014	5391.298992	24.919539
147.920695	5404.611138	24.924557
147.920121	5428.519599	24.929575
147.758283	5426.663694	24.934592
148.342699	5446.351662	24.939610
148.775802	5464.658655	24.944627
148.691396	5474.170283	24.949645
148.780726	5489.636524	24.954663
149.693583	5498.553154	24.959680
149.875092	5511.943688	24.964698
150.073539	5509.428411	24.969715
150.359616	5514.147055	24.974733
149.737657	5524.557339	24.979751
150.284452	5525.579747	24.984768
150.412653	5543.322198	24.989786
150.380032	5550.025806	24.994803
150.811825	5537.161200	24.999821
150.824937	5561.083474	25.004839
150.844364	5566.172199	25.009856
150.826948	5564.501992	25.014874
150.733656	5586.433339	25.019891
150.838620	5585.826691	25.024909
151.237492	5601.364485	25.029927
151.400069	5621.598543	25.034944
151.729303	5619.166931	25.039962
151.574131	5635.849037	25.044979
152.154661	5649.855841	25.049997
151.925528	5654.857265	25.055015
152.122129	5652.187581	25.060032
152.160828	5674.142548	25.065050
152.405275	5688.315675	25.070067
152.737746	5689.469527	25.075085
152.987858	5710.927386	25.080103
153.034034	5711.725194	25.085120
153.389143	5713.175386	25.090138
153.275532	5723.111556	25.095155
153.473803	5734.220505	25.100173
153.261919	5751.359848	25.105191
153.461783	5762.279164	25.110208
153.598358	5768.198740	25.115226
153.500832	5781.052356	25.120243
154.479013	5776.394605	25.125261
154.186472	5800.163048	25.130279
154.475033	5807.627702	25.135296
154.665443	5815.420248	25.140314
154.729378	5831.619954	25.145331
155.282379	5828.603993	25.150349
154.959711	5833.676940	25.155367
155.263456	5849.286669	25.160384
155.701119	5853.587066	25.165402
155.978224	5863.856688	25.170419
156.473500	5872.103412	25.175437
156.597999	5887.416115	25.180455
156.759664	5882.955706	25.185472
157.087457	5884.921577	25.190490
156.910820	5880.555206	25.195507
157.303283	5872.564168	25.200525
156.799490	5874.455134	25.205543
157.148085	5888.091244	25.210560
157.603021	5901.069892	25.215578
157.081357	5908.320597	25.220595
157.690997	5900.939491	25.225613
157.853890	5926.972713	25.230631
158.096370	5932.471692	25.235648
158.129524	5933.000073	25.240666
157.911675	5931.894719	25.245683
158.012081	5941.693306	25.250701
158.244106	5967.889375	25.255719
158.617398	5974.712635	25.260736
158.883165	5980.495242	25.265754
158.793247	5994.174877	25.270771
159.060831	5995.897655	25.275789
158.864280	6009.316216	25.280807
159.348760	6014.565805	25.285824
159.286063	6026.435551	25.290842
159.618337	6041.056075	25.295859
159.910005	6044.249279	25.300877
159.987100	6069.008198	25.305895
160.109696	6072.941318	25.310912
160.450154	6072.269349	25.315930
160.751915	6091.437241	25.320947
161.007548	6106.155057	25.325965
160.935057	6093.536374	25.330983
161.171909	6094.894638	25.336000
161.050018	6108.759302	25.341018
161.257171	6110.892466	25.346035
161.329640	6119.871615	25.351053
161.641837	6139.779758	25.356071
161.867724	6152.800783	25.361088
161.792918	6144.810228	25.366106
161.904114	6168.765280	25.371123
162.230917	6183.213154	25.376141
162.274199	6187.022984	25.381159
162.469720	6192.737744	25.386176
162.727300	6200.785099	25.391194
162.945985	6202.752316	25.396211
163.073019	6214.930233	25.401229
163.135952	6228.005251	25.406247
163.201485	6221.760464	25.411264
163.491648	6238.243921	25.416282
163.578045	6251.034328	25.421299
164.118527	6248.929411	25.426317
164.081080	6261.003700	25.431335
163.622022	6269.668441	25.436352
164.284255	6279.527559	25.441370
163.902283	6297.268592	25.446387
164.404963	6301.874588	25.451405
164.498280	6313.022429	25.456423
164.769942	6332.921349	25.461440
165.100796	6346.551110	25.466458
164.921556	6358.502465	25.471475
165.282832	6368.629756	25.476493
165.811244	6379.548477	25.481511
165.586095	6393.666292	25.486528
166.181621	6394.668492	25.491546
165.902041	6408.100351	25.496563
166.509192	6418.163895	25.501581
166.908558	6418.230848	25.506599
166.719865	6428.971519	25.511616
167.332136	6431.795728	25.516634
167.272288	6443.097073	25.521651
167.468653	6437.077946	25.526669
167.572795	6438.346540	25.531687
167.524788	6451.000302	25.536704
167.881449	6461.380912	25.541722
167.617410	6467.903291	25.546739
167.889845	6474.925635	25.551757
168.621884	6484.919142	25.556775
168.896448	6483.834471	25.561792
169.087540	6472.105492	25.566810
169.019097	6491.394937	25.571827
169.501548	6488.986562	25.576845
169.360229	6497.405909	25.581863
169.511952	6501.937509	25.586880
169.940606	6499.929005	25.591898
169.968524	6500.448753	25.596915
170.049620	6523.420902	25.601933
170.308410	6527.998872	25.606951
170.033518	6530.116057	25.611968
170.408915	6525.928220	25.616986
170.574854	6550.386599	25.622003
170.549246	6554.185200	25.627021
170.931688	6558.162950	25.632039
170.856856	6581.671006	25.637056
171.195549	6583.711012	25.642074
171.079801	6594.048904	25.647091
171.170228	6602.851851	25.652109
171.143645	6605.820370	25.657127
171.071416	6629.043963	25.662144
172.097129	6637.129014	25.667162
171.904061	6651.901780	25.672180
172.499117	6654.312019	25.677197
173.102116	6651.537485	25.682215
172.983558	6650.804822	25.687232
173.248901	6661.114618	25.692250
173.098058	6677.449738	25.697268
173.680217	6673.781923	25.702285
173.646575	6685.944286	25.707303
173.451058	6694.485861	25.712320
173.795868	6699.277690	25.717338
173.879693	6697.537853	25.722356
173.939901	6708.369124	25.727373
174.454252	6726.917203	25.732391
174.540356	6733.457428	25.737408
174.700399	6739.544112	25.742426
174.787078	6735.092088	25.747444
174.818685	6750.060184	25.752461
174.930006	6762.869141	25.757479
175.081149	6775.630829	25.762496
175.183583	6779.040065	25.767514
174.901644	6791.171946	25.772532
174.923263	6808.143105	25.777549
175.237661	6820.058463	25.782567
175.298965	6847.100163	25.787584
175.729856	6851.127211	25.792602
175.713525	6891.790421	25.797620
175.868064	6893.480486	25.802637
176.447651	6906.314046	25.807655
176.477351	6925.525434	25.812672
177.018757	6941.543983	25.817690
176.668934	6959.129085	25.822708
176.940498	6970.059987	25.827725
177.732595	6987.109490	25.832743
177.472749	6998.912886	25.837760
178.087489	7004.142356	25.842778
178.168910	7020.053094	25.847796
178.549196	7032.438117	25.852813
178.866917	7036.435582	25.857831
178.779090	7052.334981	25.862848
178.808189	7045.574733	25.867866
178.933793	7061.917395	25.872884
179.131759	7074.119496	25.877901
179.486516	7082.789712	25.882919
179.407522	7098.353134	25.887936
179.540892	7103.446532	25.892954
179.662846	7117.248499	25.897972
180.269222	7128.521658	25.902989
180.454276	7138.733808	25.908007
180.619301	7152.626918	25.913024
180.667777	7161.891302	25.918042
181.034659	7172.636918	25.923060
181.109695	7179.280058	25.928077
181.376707	7187.771497	25.933095
181.172823	7201.905541	25.938112
181.382619	7205.001284	25.943130
182.088488	7225.287747	25.948148
182.017509	7244.720440	25.953165
182.283369	7244.820943	25.958183
182.187822	7265.457144	25.963200
182.518367	7271.207913	25.968218
182.723297	7284.466639	25.973236
182.724656	7298.524406	25.978253
182.691037	7304.218586	25.983271
183.124053	7321.577211	25.988288
183.512052	7327.757813	25.993306
183.713069	7349.916655	25.998324
183.876930	7361.865420	26.003341
184.146932	7355.824988	26.008359
184.191223	7374.532601	26.013376
184.060048	7376.977788	26.018394
184.494661	7395.213869	26.023412
184.836535	7421.754697	26.028429
184.944500	7411.329346	26.033447
185.319335	7425.871698	26.038464
185.494831	7439.160403	26.043482
185.710731	7436.692643	26.048500
185.467533	7443.423617	26.053517
186.160183	7455.728421	26.058535
185.884081	7467.708296	26.063552
186.251872	7475.158062	26.068570
186.936010	7478.173227	26.073588
187.132523	7480.245079	26.078605
187.481372	7477.863824	26.083623
187.381804	7474.441562	26.088640
187.706121	7465.917514	26.093658
187.784752	7477.573479	26.098676
187.806933	7491.284020	26.103693
188.090256	7489.642291	26.108711
188.085964	7505.585819	26.113728
188.105785	7501.333503	26.118746
188.187008	7516.152385	26.123764
188.128986	7528.495915	26.128781
188.307671	7531.988054	26.133799
188.485037	7550.529777	26.138816
189.066320	7566.896210	26.143834
188.798618	7571.698988	26.148852
189.077838	7583.828715	26.153869
189.402562	7605.526505	26.158887
189.452762	7616.483000	26.163904
189.814652	7629.114397	26.168922
190.062788	7636.223076	26.173940
190.233533	7651.747839	26.178957
190.346358	7658.571495	26.183975
190.462814	7676.324163	26.188992
191.113449	7684.102231	26.194010
191.492898	7681.523579	26.199028
191.755874	7695.335456	26.204045
191.752469	7701.801652	26.209063
192.041755	7702.154206	26.214080
192.318368	7705.384790	26.219098
192.226417	7718.819777	26.224116
192.489167	7735.226791	26.229133
192.458554	7744.964784	26.234151
192.883779	7752.699269	26.239168
193.014056	7763.567539	26.244186
193.201891	7769.741765	26.249204
193.080099	7778.875282	26.254221
193.503380	7796.491601	26.259239
193.375656	7810.213234	26.264256
193.912785	7825.469224	26.269274
193.812237	7824.212780	26.274292
194.037011	7851.306112	26.279309
194.375815	7855.347811	26.284327
194.607205	7874.774840	26.289344
194.886361	7885.553560	26.294362
194.973441	7893.584171	26.299380
194.992792	7918.521948	26.304397
195.068324	7920.331827	26.309415
195.379871	7937.160735	26.314432
195.310859	7934.674404	26.319450
195.747676	7954.975410	26.324468
195.824487	7967.067644	26.329485
196.366010	7980.611946	26.334503
196.373049	7998.287353	26.339520
196.181893	8021.386105	26.344538
196.786077	8030.945874	26.349556
196.900807	8048.304535	26.354573
197.340187	8061.561819	26.359591
197.191813	8078.699690	26.364608
197.054199	8091.867434	26.369626
197.578835	8104.738857	26.374644
197.619249	8129.923029	26.379661
197.781720	8143.176396	26.384679
198.144067	8167.126274	26.389696
198.121873	8182.921650	26.394714
198.819808	8192.880396	26.399732
198.865742	8209.593309	26.404749
199.345620	8212.694269	26.409767
199.695304	8219.604153	26.414784
199.856420	8220.592434	26.419802
200.505297	8237.517154	26.424820
200.941912	8246.475022	26.429837
201.319585	8248.130257	26.434855
200.931137	8245.507657	26.439872
200.966275	8244.008930	26.444890
201.118062	8237.336367	26.449908
201.315040	8251.989321	26.454925
201.229908	8267.188463	26.459943
201.296021	8281.849313	26.464960
201.324805	8292.844293	26.469978
201.560657	8300.583419	26.474996
201.915504	8312.370281	26.480013
202.448923	8327.175800	26.485031
202.773874	8338.193866	26.490048
202.966711	8347.650914	26.495066
203.200017	8341.012901	26.500084
203.097935	8349.234359	26.505101
203.300149	8360.053824	26.510119
203.913107	8374.793249	26.515136
203.787457	8386.279734	26.520154
203.930795	8394.797421	26.525172
204.015120	8399.788362	26.530189
204.234805	8413.759102	26.535207
204.520126	8424.221457	26.540224
204.410465	8449.309603	26.545242
204.705422	8447.561784	26.550260
204.786650	8480.146702	26.555277
205.168502	8487.796735	26.560295
205.091479	8503.039000	26.565312
205.445689	8525.740385	26.570330
205.951432	8538.138340	26.575348
205.679600	8561.853421	26.580365
206.313855	8575.961396	26.585383
206.337065	8584.409588	26.590400
206.396114	8605.070422	26.595418
206.887282	8619.443948	26.600436
206.758136	8636.847681	26.605453
207.066085	8647.859124	26.610471
207.432419	8662.372212	26.615488
207.409975	8684.229844	26.620506
207.851636	8689.550060	26.625524
208.527982	8717.505288	26.630541
208.514950	8720.112103	26.635559
208.736629	8735.885530	26.640576
208.534688	8750.355111	26.645594
209.012030	8763.928988	26.650612
209.149167	8779.933544	26.655629
209.292336	8793.506121	26.660647
209.685985	8798.982279	26.665664
209.417278	8829.706209	26.670682
209.705879	8835.119904	26.675700
210.359251	8852.966391	26.680717
210.410196	8858.594129	26.685735
210.718036	8886.313721	26.690752
210.560750	8902.209802	26.695770
211.144081	8910.977677	26.700788
211.404880	8927.060860	26.705805
211.617960	8942.488515	26.710823
211.873330	8950.812102	26.715840
211.902664	8966.060185	26.720858
212.665294	8974.926291	26.725876
212.572333	8981.160698	26.730893
213.189171	8986.702979	26.735911
213.947632	8984.869870	26.740928
213.686401	8989.927734	26.745946
214.362602	8990.181817	26.750964
214.141380	8995.261830	26.755981
213.935699	8983.814427	26.760999
214.407713	8999.510974	26.766016
214.530537	9017.399692	26.771034
214.708439	9008.383246	26.776052
214.648191	9024.308432	26.781069
215.111288	9033.445655	26.786087
214.956108	9036.775691	26.791104
215.145379	9055.102364	26.796122
215.047157	9069.502272	26.801140
215.580326	9073.542207	26.806157
215.933626	9090.185661	26.811175
216.139114	9099.407475	26.816192
216.062611	9125.372213	26.821210
216.288159	9136.848344	26.826228
216.296096	9143.957348	26.831245
217.009467	9160.418166	26.836263
216.959836	9175.227303	26.841280
217.365463	9187.597177	26.846298
217.551795	9201.532692	26.851316
217.787055	9220.130163	26.856333
217.821027	9222.893863	26.861351
218.162005	9237.010401	26.866368
218.188844	9245.268889	26.871386
218.597638	9269.714925	26.876404
218.647643	9278.724390	26.881421
218.724008	9305.641033	26.886439
219.298999	9306.100414	26.891456
219.101824	9328.993353	26.896474
219.900847	9344.961009	26.901492
219.857280	9356.627828	26.906509
219.655169	9368.846762	26.911527
220.127615	9382.425017	26.916544
220.418483	9402.172690	26.921562
220.771329	9408.400547	26.926580
220.790624	9433.886583	26.931597
221.047581	9454.896235	26.936615
221.525166	9458.202994	26.941632
221.415712	9477.511447	26.946650
222.001146	9490.061739	26.951668
222.305601	9519.023633	26.956685
222.201435	9521.335419	26.961703
223.045725	9535.827991	26.966720
222.820080	9559.581309	26.971738
223.132348	9564.574743	26.976756
223.389338	9586.594886	26.981773
222.960361	9601.160684	26.986791
223.479917	9612.780491	26.991808
223.760175	9631.500776	26.996826
224.180198	9645.286349	27.001844
224.325947	9667.633435	27.006861
224.471458	9673.120310	27.011879
224.914119	9693.213923	27.016896
224.847150	9713.801010	27.021914
225.311897	9726.323008	27.026932
225.256368	9734.730382	27.031949
225.738506	9759.986488	27.036967
226.273029	9765.873425	27.041984
226.301324	9782.776801	27.047002
226.776358	9793.566993	27.052020
226.999029	9809.969495	27.057037
227.073985	9808.890650	27.062055
227.487990	9829.162555	27.067072
227.661386	9845.020265	27.072090
228.034266	9845.666037	27.077108
227.984470	9862.082852	27.082125
228.031845	9871.648716	27.087143
228.551176	9869.834043	27.092160
228.659913	9904.358940	27.097178
228.709699	9907.818048	27.102196
228.627599	9911.578826	27.107213
228.725100	9926.195010	27.112231
229.180360	9940.802521	27.117248
229.304747	9967.570513	27.122266
229.950386	9985.182499	27.127284
229.723715	10001.766072	27.132301
229.602033	10022.835681	27.137319
230.087550	10036.005061	27.142336
230.559724	10053.817944	27.147354
230.356960	10067.534052	27.152372
230.937007	10081.923207	27.157389
231.212591	10110.656895	27.162407
231.529863	10108.665465	27.167424
231.853629	10130.716837	27.172442
231.956360	10142.796954	27.177460
232.192294	10165.433621	27.182477
232.359967	10178.832869	27.187495
232.752309	10182.740398	27.192512
233.050548	10213.469354	27.197530
233.248315	10222.973948	27.202548
233.665378	10232.876762	27.207565
233.622560	10249.463327	27.212583
233.884016	10264.508764	27.217600
233.980300	10281.351421	27.222618
234.559074	10301.307541	27.227636
234.608716	10311.479507	27.232653
234.634206	10341.061038	27.237671
235.179634	10350.230219	27.242688
235.189187	10369.732501	27.247706
235.053333	10390.457422	27.252724
235.400074	10403.172024	27.257741
235.630895	10428.979919	27.262759
235.991824	10443.713114	27.267776
236.045028	10473.303142	27.272794
236.471494	10494.378978	27.277812
237.244893	10508.444527	27.282829
237.273455	10518.398883	27.287847
237.680378	10541.536521	27.292864
237.771801	10547.985693	27.297882
238.061378	10575.723291	27.302900
238.549440	10581.065204	27.307917
238.510312	10602.255148	27.312935
238.973445	10615.074804	27.317952
239.393557	10628.324315	27.322970
239.577298	10630.578504	27.327988
240.258357	10642.704119	27.333005
239.921720	10652.737860	27.338023
240.377091	10651.981432	27.343040
240.414729	10672.894198	27.348058
241.075041	10678.786982	27.353076
241.451155	10690.142601	27.358093
241.527246	10704.784851	27.363111
241.703594	10699.995764	27.368128
241.699017	10720.792054	27.373146
241.672141	10738.238559	27.378164
242.172609	10737.623467	27.383181
242.578070	10744.869730	27.388199
243.143678	10747.329345	27.393216
243.259230	10764.175734	27.398234
243.136462	10780.121682	27.403252
243.447434	10786.918605	27.408269
243.688318	10788.125031	27.413287
243.697296	10811.991586	27.418304
243.844154	10829.584625	27.423322
243.989018	10839.394630	27.428340
244.093306	10849.229942	27.433357
244.387416	10868.350308	27.438375
244.790110	10870.222895	27.443392
245.078660	10877.989576	27.448410
245.648271	10885.301748	27.453428
245.869374	10899.962481	27.458445
245.821881	10913.478060	27.463463
246.256860	10929.772505	27.468480
246.535982	10943.555853	27.473498
246.465589	10953.854329	27.478516
246.902363	10975.551135	27.483533
246.654871	10980.440029	27.488551
246.932017	10994.110051	27.493568
246.926810	11020.233603	27.498586
247.058925	11036.708205	27.503604
247.673922	11054.720702	27.508621
248.016444	11081.913967	27.513639
248.236389	11097.825442	27.518656
248.541921	11122.369025	27.523674
248.669396	11128.433837	27.528692
248.991471	11144.935613	27.533709
249.171558	11160.509207	27.538727
249.590843	11181.880601	27.543744
249.597507	11207.592065	27.548762
249.858779	11222.196236	27.553780
250.151360	11245.674735	27.558797
250.602077	11273.110252	27.563815
250.865331	11277.758173	27.568832
251.227221	11301.333243	27.573850
251.239655	11316.361700	27.578868
251.805847	11330.978184	27.583885
252.094678	11365.389148	27.588903
251.935715	11362.954340	27.593920
252.740491	11386.103324	27.598938
252.564901	11403.864247	27.603956
252.802080	11421.494214	27.608973
252.800527	11441.807708	27.613991
253.182885	11454.207996	27.619008
253.640402	11476.192637	27.624026
253.653828	11504.224325	27.629044
254.286105	11516.831802	27.634061
254.173952	11536.152271	27.639079
254.588454	11560.903550	27.644096
255.075911	11566.470038	27.649114
255.467660	11588.566158	27.654132
255.686244	11598.014510	27.659149
256.087347	11618.315639	27.664167
256.330620	11627.621200	27.669184
256.481031	11644.977621	27.674202
256.579592	11652.370203	27.679220
256.674818	11668.570104	27.684237
257.156636	11685.640976	27.689255
257.244404	11713.332930	27.694272
257.375609	11727.790512	27.699290
257.485614	11750.398299	27.704308
257.843648	11775.288173	27.709325
258.061031	11798.059185	27.714343
258.333894	11817.117534	27.719360
258.496838	11837.241484	27.724378
258.341865	11865.347456	27.729396
259.299252	11881.096706	27.734413
259.063120	11915.464605	27.739431
259.524677	11926.188675	27.744448
259.926819	11945.286899	27.749466
260.042763	11977.638803	27.754484
260.445007	11989.256368	27.759501
260.277076	12009.239713	27.764519
260.616019	12036.573861	27.769536
261.261538	12053.142603	27.774554
261.543730	12074.318604	27.779572
261.985990	12088.111972	27.784589
261.975908	12107.502296	27.789607
262.477470	12127.282996	27.794624
262.695264	12135.759150	27.799642
263.051758	12155.186831	27.804660
263.246744	12170.316839	27.809677
263.677872	12180.695309	27.814695
264.204685	12185.520056	27.819712
264.243577	12199.869309	27.824730
264.493277	12217.321225	27.829748
264.616599	12222.935479	27.834765
264.901683	12251.396231	27.839783
265.104215	12272.417572	27.844800
265.012549	12279.650732	27.849818
265.664107	12301.940668	27.854836
265.777981	12323.885399	27.859853
266.002460	12346.400181	27.864871
265.949662	12365.165900	27.869888
266.721346	12372.630155	27.874906
266.643131	12406.478432	27.879924
267.185556	12423.979418	27.884941
267.132621	12445.802005	27.889959
267.364901	12466.417858	27.894976
267.528393	12480.965695	27.899994
267.919975	12509.444889	27.905012
268.083711	12536.564056	27.910029
268.509475	12550.199298	27.915047
268.462237	12583.319895	27.920064
269.142254	12599.665824	27.925082
269.439277	12624.812690	27.930100
269.605482	12647.640113	27.935117
269.986261	12674.185484	27.940135
270.369451	12700.190521	27.945152
270.493434	12719.263631	27.950170
270.676667	12746.357940	27.955188
270.666215	12768.628976	27.960205
271.112308	12790.856941	27.965223
271.020451	12814.309199	27.970240
271.628415	12832.416084	27.975258
272.226578	12860.497131	27.980276
272.779401	12879.285330	27.985293
273.346750	12900.067061	27.990311
273.231462	12916.645221	27.995328
273.761155	12936.314996	28.000346
273.881298	12948.514189	28.005364
274.117394	12972.433164	28.010381
274.333912	12975.566717	28.015399
274.454699	12990.333216	28.020416
274.765555	13021.658474	28.025434
275.040255	13036.021948	28.030452
275.342571	13052.316911	28.035469
276.098640	13074.174544	28.040487
276.032532	13091.083050	28.045504
276.436697	13108.347380	28.050522
276.610996	13126.345638	28.055540
276.886977	13143.077443	28.060557
277.067848	13167.201106	28.065575
277.234171	13178.887944	28.070592
278.013747	13197.423040	28.075610
277.748581	13210.175401	28.080628
278.605192	13228.786883	28.085645
278.665871	13252.019994	28.090663
278.976331	13255.678888	28.095680
279.193722	13275.274778	28.100698
279.307704	13299.159610	28.105716
279.647633	13318.171073	28.110733
279.874362	13331.509632	28.115751
280.150330	13362.834603	28.120768
280.357289	13363.048595	28.125786
280.794519	13392.772526	28.130804
281.001389	13399.589864	28.135821
281.082083	13424.755891	28.140839
280.761552	13439.045542	28.145856
281.502565	13450.383566	28.150874
281.710885	13482.133028	28.155892
281.964317	13510.793271	28.160909
282.506319	13523.236233	28.165927
282.198619	13547.825350	28.170944
282.548608	13560.427894	28.175962
282.689961	13595.946063	28.180980
283.481604	13617.795595	28.185997
283.603918	13640.867941	28.191015
284.056312	13676.890190	28.196032
284.236013	13693.732303	28.201050
284.776875	13705.471324	28.206068
285.468092	13731.865334	28.211085
285.513436	13753.446650	28.216103
285.732044	13770.623805	28.221120
286.353956	13780.414298	28.226138
286.442305	13795.202295	28.231156
286.609460	13816.802498	28.236173
286.978192	13824.693634	28.241191
286.979466	13859.053128	28.246208
287.468770	13879.292344	28.251226
287.282898	13904.923945	28.256244
287.447986	13922.738075	28.261261
288.010322	13957.489882	28.266279
288.368789	13977.351782	28.271296
288.670474	13998.590045	28.276314
289.163017	14026.919909	28.281332
289.490889	14046.742461	28.286349
289.585221	14073.761007	28.291367
289.867081	14103.823041	28.296384
289.962544	14119.159684	28.301402
290.482481	14146.446420	28.306420
290.907537	14164.169523	28.311437
291.265767	14186.229720	28.316455
291.513398	14209.605252	28.321472
291.883227	14232.235304	28.326490
292.100363	14242.951611	28.331508
292.047688	14264.027771	28.336525
292.753039	14290.256121	28.341543
292.681558	14306.765467	28.346560
293.627097	14330.502381	28.351578
293.918424	14357.916818	28.356596
293.956395	14373.480584	28.361613
294.297723	14391.460192	28.366631
294.616706	14407.027336	28.371648
295.002725	14431.973168	28.376666
295.154453	14451.043671	28.381684
295.552016	14466.822784	28.386701
295.960806	14483.487593	28.391719
296.271272	14510.311834	28.396736
296.240116	14524.320103	28.401754
296.452441	14548.522704	28.406772
296.726870	14565.634986	28.411789
297.344044	14587.970902	28.416807
297.019155	14626.981176	28.421824
297.585838	14640.677964	28.426842
297.930238	14664.089425	28.431860
298.046126	14695.321656	28.436877
298.514337	14712.842703	28.441895
298.550533	14739.451258	28.446912
298.734382	14768.155877	28.451930
299.019432	14777.093251	28.456948
299.399182	14809.459188	28.461965
299.818698	14834.662431	28.466983
299.991289	14862.118300	28.472000
300.303454	14872.071577	28.477018
300.509836	14907.954674	28.482036
300.547577	14924.839064	28.487053
301.173917	14944.928461	28.492071
301.185771	14971.620109	28.497088
301.767485	14999.387917	28.502106
302.192229	15022.070311	28.507124
302.327881	15053.821142	28.512141
302.800319	15072.115628	28.517159
302.898907	15101.983709	28.522176
303.575328	15120.634754	28.527194
303.785040	15155.434510	28.532212
304.036168	15171.423482	28.537229
304.588707	15188.827534	28.542247
304.826442	15220.041534	28.547264
305.078707	15228.191528	28.552282
305.592962	15261.146708	28.557300
305.929766	15287.146760	28.562317
306.310655	15296.707340	28.567335
306.157398	15321.309284	28.572352
306.281659	15347.371137	28.577370
307.031799	15366.993107	28.582388
307.192252	15392.616665	28.587405
307.500911	15407.892521	28.592423
308.002039	15444.418964	28.597440
308.184024	15465.093322	28.602458
308.591919	15484.674276	28.607476
308.668221	15504.307194	28.612493
309.260876	15525.656336	28.617511
309.514476	15551.919289	28.622528
309.897720	15572.843329	28.627546
310.309764	15595.910552	28.632564
310.415106	15618.488929	28.637581
310.989655	15642.873049	28.642599
311.193400	15672.494987	28.647616
311.377923	15693.453446	28.652634
311.606205	15714.683009	28.657652
311.628813	15736.999707	28.662669
312.154406	15759.736663	28.667687
312.380888	15795.488780	28.672704
312.828021	15811.343358	28.677722
313.234757	15838.400735	28.682740
313.201915	15870.763613	28.687757
313.424262	15892.521753	28.692775
313.480568	15923.670567	28.697792
313.897719	15958.167662	28.702810
314.299845	15987.812703	28.707828
314.399018	16020.379399	28.712845
314.921582	16039.766087	28.717863
315.281392	16084.455122	28.722880
315.473567	16103.609371	28.727898
316.209164	16134.832148	28.732916
316.239853	16172.036930	28.737933
317.039535	16201.648450	28.742951
317.022567	16231.384784	28.747968
317.443120	16252.455326	28.752986
317.985540	16270.263071	28.758004
318.386738	16305.423405	28.763021
318.383334	16327.517454	28.768039
318.506836	16369.246787	28.773056
318.619960	16387.194533	28.778074
319.206769	16406.382020	28.783092
319.375676	16440.814638	28.788109
319.846315	16467.720760	28.793127
319.731863	16505.271086	28.798144
320.242061	16519.442370	28.803162
321.000210	16538.363103	28.808180
321.456190	16573.610101	28.813197
321.774287	16598.537810	28.818215
322.057580	16629.904890	28.823232
322.483586	16649.086224	28.828250
322.974172	16662.666886	28.833268
322.853385	16698.535091	28.838285
323.292630	16719.723241	28.843303
323.574955	16737.183664	28.848320
323.950020	16746.474248	28.853338
324.308865	16776.427344	28.858356
324.483165	16807.151652	28.863373
325.057761	16827.459596	28.868391
324.905824	16860.742977	28.873408
325.602841	16888.899755	28.878426
325.867530	16912.730744	28.883444
327.015063	16918.489166	28.888461
328.167977	16907.288450	28.893479
328.680932	16905.925815	28.898496
328.746331	16906.695824	28.903514
329.502927	16917.013269	28.908532
329.206165	16928.572794	28.913549
329.754086	16929.879980	28.918567
330.142735	16923.160946	28.923584
330.287381	16916.410649	28.928602
330.837468	16936.305618	28.933620
330.830414	16951.565829	28.938637
331.121254	16949.021936	28.943655
331.205957	16963.651863	28.948672
331.324929	16971.845590	28.953690
331.545826	16995.689859	28.958708
331.569366	17010.582088	28.963725
332.185249	17026.095379	28.968743
332.248954	17049.528455	28.973760
332.071847	17080.889424	28.978778
332.780321	17096.893642	28.983796
332.854774	17125.170399	28.988813
333.013189	17156.200976	28.993831
333.223391	17190.306287	28.998848
333.511521	17219.528878	29.003866
333.902984	17253.669079	29.008884
334.349536	17280.851751	29.013901
334.415178	17304.695452	29.018919
334.737461	17340.141677	29.023936
335.127905	17374.825536	29.028954
335.361069	17393.633514	29.033972
335.816328	17435.104713	29.038989
336.552258	17459.614317	29.044007
336.704835	17487.336078	29.049024
337.130253	17522.324270	29.054042
337.460298	17551.250200	29.059060
337.278547	17595.102080	29.064077
337.474697	17620.056529	29.069095
338.206956	17660.701470	29.074112
338.404046	17691.916368	29.079130
338.801829	17723.289400	29.084148
339.180130	17764.286921	29.089165
339.300977	17798.723170	29.094183
340.125581	17823.876355	29.099200
340.322121	17858.123965	29.104218
340.815189	17879.039626	29.109236
340.893314	17921.183733	29.114253
341.333817	17958.785772	29.119271
341.952696	17985.291742	29.124288
341.671035	18024.434778	29.129306
342.345032	18037.292757	29.134324
342.295089	18077.296685	29.139341
342.558504	18112.077571	29.144359
342.960073	18144.246697	29.149376
343.437778	18180.485072	29.154394
343.882446	18209.128692	29.159412
343.995487	18237.337850	29.164429
344.496486	18272.182887	29.169447
345.331272	18302.932458	29.174464
345.529612	18335.089512	29.179482
345.920327	18358.997304	29.184500
345.946095	18378.862175	29.189517
346.200306	18410.429382	29.194535
347.117972	18441.412577	29.199552
347.112095	18477.878880	29.204570
347.754940	18502.966656	29.209588
348.191365	18527.341318	29.214605
348.142514	18554.236955	29.219623
348.837126	18572.171452	29.224640
349.438733	18612.712502	29.229658
349.742472	18636.899602	29.234676
350.120531	18658.510112	29.239693
350.276974	18684.520884	29.244711
351.243019	18707.024903	29.249728
351.197076	18739.454645	29.254746
351.693007	18760.914132	29.259764
351.713839	18780.799139	29.264781
351.923626	18806.782765	29.269799
352.119987	18831.991448	29.274816
352.065593	18878.751382	29.279834
352.594824	18906.435120	29.284852
353.076308	18934.309592	29.289869
353.664841	18965.901145	29.294887
353.504918	18997.123519	29.299904
353.957909	19043.437937	29.304922
354.549399	19079.401134	29.309940
355.155769	19110.882724	29.314957
355.292605	19139.493803	29.319975
355.393572	19168.950815	29.324992
355.790203	19217.049788	29.330010
356.313433	19249.902968	29.335028
356.758934	19285.725148	29.340045
356.538149	19321.512770	29.345063
357.420646	19367.893354	29.350080
357.437282	19398.956037	29.355098
357.935643	19424.800514	29.360116
358.268544	19462.226456	29.365133
358.648785	19507.352961	29.370151
359.268720	19533.361759	29.375168
359.941081	19560.543841	29.380186
360.546904	19589.941359	29.385204
360.849239	19619.329599	29.390221
361.139003	19641.517331	29.395239
361.218188	19680.063811	29.400256
361.713038	19703.097691	29.405274
362.598469	19728.452314	29.410292
362.895120	19763.003490	29.415309
362.887583	19790.368209	29.420327
363.200310	19817.828115	29.425344
363.695097	19848.709205	29.430362
363.994966	19872.759446	29.435380
364.076128	19907.780579	29.440397
364.077134	19937.121725	29.445415
364.998999	19963.740884	29.450432
365.079585	20001.415878	29.455450
365.456640	20026.382980	29.460468
365.535042	20064.570206	29.465485
365.951680	20101.402985	29.470503
366.495394	20135.328530	29.475520
366.352622	20175.281791	29.480538
366.792963	20203.480428	29.485556
367.387773	20243.381474	29.490573
367.534854	20275.726660	29.495591
368.133196	20312.853603	29.500608
368.267132	20353.496795	29.505626
368.457295	20382.568884	29.510644
368.852837	20419.411883	29.515661
369.250583	20461.700949	29.520679
369.619952	20492.419470	29.525696
370.034038	20535.445373	29.530714
370.590457	20581.039578	29.535732
370.706799	20608.468170	29.540749
370.725699	20658.354748	29.545767
371.265389	20698.214806	29.550784
371.743732	20741.035224	29.555802
372.289445	20769.925825	29.560820
372.753749	20818.770013	29.565837
373.163494	20852.073307	29.570855
373.965778	20882.541391	29.575872
374.594492	20922.798656	29.580890
374.679690	20950.403199	29.585908
375.002804	20973.193781	29.590925
375.432874	21009.552276	29.595943
376.083074	21045.832129	29.600960
375.989319	21070.419378	29.605978
376.615198	21107.789929	29.610996
377.301482	21133.171249	29.616013
377.122281	21176.139842	29.621031
378.272262	21203.546359	29.626048
378.478930	21240.970191	29.631066
379.034615	21271.591240	29.636084
379.381202	21295.433712	29.641101
379.471053	21324.447082	29.646119
380.260106	21340.947662	29.651136
380.567916	21377.446040	29.656154
381.024050	21410.970480	29.661172
381.316827	21430.411184	29.666189
381.296601	21465.589978	29.671207
382.008248	21491.473274	29.676224
382.271049	21525.672690	29.681242
382.840919	21553.650779	29.686260
383.049895	21574.261057	29.691277
383.406638	21606.082733	29.696295
383.837984	21629.432116	29.701312
384.351776	21670.397641	29.706330
384.771393	21693.862674	29.711348
385.380955	21722.586705	29.716365
385.713288	21757.394860	29.721383
385.946047	21777.357120	29.726400
386.280502	21818.850220	29.731418
386.470723	21846.989292	29.736436
386.899231	21870.674297	29.741453
387.168094	21915.899598	29.746471
387.483732	21936.120742	29.751488
387.973269	21969.065892	29.756506
388.087759	22007.503977	29.761524
388.556609	22028.914417	29.766541
388.532689	22074.053247	29.771559
389.155391	22100.298809	29.776576
389.566024	22145.395008	29.781594
389.742280	22186.262822	29.786612
390.454819	22216.209929	29.791629
390.906633	22262.709043	29.796647
391.185809	22294.815686	29.801664
391.384233	22339.977162	29.806682
391.644888	22368.428204	29.811700
392.227147	22401.890336	29.816717
392.446804	22442.505443	29.821735
393.070514	22475.759002	29.826752
393.273627	22513.046781	29.831770
393.877895	22541.703323	29.836788
394.352843	22585.223354	29.841805
394.839244	22616.122735	29.846823
394.997376	22650.403677	29.851840
395.295153	22682.811345	29.856858
395.506884	22714.436352	29.861876
396.145265	22751.144559	29.866893
395.767338	22800.150843	29.871911
396.419684	22834.424198	29.876928
397.060701	22883.220529	29.881946
397.280613	22925.264684	29.886964
397.597070	22964.020531	29.891981
398.125131	23014.231389	29.896999
398.759588	23047.237779	29.902016
398.833984	23104.824794	29.907034
399.265175	23136.485606	29.912052
399.965263	23163.346046	29.917069
400.283487	23212.718234	29.922087
400.746143	23246.579673	29.927104
400.953903	23295.798752	29.932122
401.533152	23332.770063	29.937140
402.472633	23370.588661	29.942157
402.339618	23411.975056	29.947175
403.311292	23450.970455	29.952192
403.524653	23491.778265	29.957210
404.016349	23526.918435	29.962228
404.396204	23563.156778	29.967245
404.784523	23588.253002	29.972263
405.526326	23625.774448	29.977280
406.185479	23660.427317	29.982298
406.380956	23688.808304	29.987316
406.785763	23719.286148	29.992333
407.466253	23757.120772	29.997351
407.880081	23788.197643	30.002368
408.026362	23824.997551	30.007386
408.373763	23854.176491	30.012404
408.691155	23878.677533	30.017421
408.633184	23926.574810	30.022439
409.028192	23957.591699	30.027456
410.113856	23994.055195	30.032474
410.282151	24029.891485	30.037492
410.667870	24063.854834	30.042509
410.834198	24104.911400	30.047527
411.578567	24142.490291	30.052544
411.854006	24166.284161	30.057562
412.192920	24208.596753	30.062580
412.814227	24247.648592	30.067597
412.943950	24285.008053	30.072615
413.102296	24328.107519	30.077632
413.520446	24375.204547	30.082650
414.169011	24413.095970	30.087668
414.850242	24442.861750	30.092685
414.980713	24484.727290	30.097703
415.432005	24525.322992	30.102720
415.674780	24571.392586	30.107738
415.695359	24614.514246	30.112756
416.068868	24667.565683	30.117773
416.354972	24710.961938	30.122791
417.026635	24754.095668	30.127808
417.359655	24806.502892	30.132826
418.000095	24850.172568	30.137844
418.282576	24892.040426	30.142861
418.412872	24947.115073	30.147879
419.092891	24991.334990	30.152896
419.899238	25035.073877	30.157914
420.602025	25059.478078	30.162932
421.235034	25090.396244	30.167949
421.396316	25130.210709	30.172967
421.789291	25152.281007	30.177984
422.284512	25190.324312	30.183002
422.410698	25220.418337	30.188020
423.121979	25250.136371	30.193037
423.347277	25284.259629	30.198055
423.889110	25326.574392	30.203072
424.427217	25355.131582	30.208090
424.722224	25394.034529	30.213108
425.151635	25431.304939	30.218125
425.134223	25465.567638	30.223143
425.603598	25510.971905	30.228160
426.161181	25552.437813	30.233178
426.295754	25597.901038	30.238196
426.979678	25639.511653	30.243213
427.558473	25671.557827	30.248231
428.145135	25700.942132	30.253248
428.673628	25742.324508	30.258266
429.034122	25798.749492	30.263284
429.658986	25817.731660	30.268301
429.720258	25871.176453	30.273319
430.432475	25900.579303	30.278336
430.957228	25935.528916	30.283354
430.966560	25973.510767	30.288372
431.144277	26016.042010	30.293389
431.739753	26066.603875	30.298407
431.908664	26106.393790	30.303424
432.693818	26149.778177	30.308442
432.916566	26193.099066	30.313460
433.735761	26242.975363	30.318477
433.843313	26282.926918	30.323495
434.042111	26320.797582	30.328512
434.474316	26374.381526	30.333530
434.378651	26420.735880	30.338548
435.180172	26469.547398	30.343565
435.660941	26526.284219	30.348583
436.055193	26585.714516	30.353600
436.501995	26624.254763	30.358618
437.052560	26680.039370	30.363636
437.612897	26725.280431	30.368653
438.184289	26774.128729	30.373671
438.728001	26816.844495	30.378688
439.405760	26864.020438	30.383706
439.738018	26913.323667	30.388724
440.670722	26947.515896	30.393741
440.955790	26984.065980	30.398759
441.517401	27019.498357	30.403776
441.913788	27060.328971	30.408794
442.300049	27102.558052	30.413812
443.199885	27123.015266	30.418829
444.007243	27158.301947	30.423847
444.204167	27194.373227	30.428864
444.749854	27225.674924	30.433882
444.900892	27253.025025	30.438900
445.291245	27282.796320	30.443917
445.876698	27323.926511	30.448935
445.828822	27359.334859	30.453952
446.479344	27393.970228	30.458970
447.029057	27439.517927	30.463988
447.341885	27468.353567	30.469005
447.777476	27502.156881	30.474023
448.053276	27548.695801	30.479040
448.711282	27589.164153	30.484058
448.244585	27631.230868	30.489076
448.889299	27671.499209	30.494093
449.276699	27722.407498	30.499111
449.387104	27774.673979	30.504128
450.104172	27813.597627	30.509146
450.228084	27866.709186	30.514164
450.644136	27911.747945	30.519181
451.227680	27955.230978	30.524199
450.989568	27996.327187	30.529216
451.435746	28052.688125	30.534234
451.815060	28107.353110	30.539252
452.112303	28166.303882	30.544269
453.170095	28220.660636	30.549287
453.450924	28283.944003	30.554304
454.105427	28332.100383	30.559322
454.394754	28391.034080	30.564340
455.235030	28444.369933	30.569357
455.841304	28485.922698	30.574375
456.020564	28539.564601	30.579392
457.189359	28564.178157	30.584410
457.515028	28623.941179	30.589428
458.306293	28674.181781	30.594445
458.421998	28715.862418	30.599463
458.985041	28762.896383	30.604480
459.716145	28792.894627	30.609498
460.125773	28837.968037	30.614516
460.433374	28870.017490	30.619533
461.431922	28916.522168	30.624551
461.928584	28959.831318	30.629568
462.221705	28996.845172	30.634586
462.435484	29044.035622	30.639604
463.311079	29073.310020	30.644621
463.629635	29125.035344	30.649639
463.782305	29152.153852	30.654656
464.308926	29195.345029	30.659674
465.014623	29242.983531	30.664692
464.741797	29285.756507	30.669709
465.475230	29329.787876	30.674727
466.084662	29381.594707	30.679744
466.496981	29432.674012	30.684762
467.292014	29481.670749	30.689780
467.667080	29521.112655	30.694797
468.230767	29559.842412	30.699815
468.771586	29604.239558	30.704832
469.185449	29644.314058	30.709850
469.598610	29677.650392	30.714868
469.781744	29726.572883	30.719885
470.358186	29770.667714	30.724903
470.436887	29821.010089	30.729920
470.834681	29866.871436	30.734938
471.715355	29920.141587	30.739956
472.356060	29961.736196	30.744973
472.914827	30003.906315	30.749991
473.179124	30049.314884	30.755008
473.753201	30099.447601	30.760026
473.992656	30146.535414	30.765044
474.624656	30188.624906	30.770061
475.309767	30224.795728	30.775079
475.556722	30287.534289	30.780096
475.932754	30334.936171	30.785114
476.341361	30371.624660	30.790132
476.699119	30421.716184	30.795149
477.244291	30471.601477	30.800167
477.564086	30526.471857	30.805184
478.626201	30578.261363	30.810202
478.856238	30630.269826	30.815220
478.909109	30673.557267	30.820237
479.391427	30715.860922	30.825255
479.789922	30777.932443	30.830272
480.380577	30823.670883	30.835290
480.712612	30885.361202	30.840308
481.139003	30933.439291	30.845325
481.594782	30985.539718	30.850343
481.847529	31046.787783	30.855360
482.851833	31084.585332	30.860378
483.381666	31136.895796	30.865396
483.737580	31183.417746	30.870413
484.096351	31227.012439	30.875431
484.685908	31278.403590	30.880448
485.052287	31326.289696	30.885466
486.024122	31375.908045	30.890484
486.569973	31419.992218	30.895501
486.784891	31457.465247	30.900519
487.215356	31516.499554	30.905536
488.043446	31558.074344	30.910554
488.255880	31603.949605	30.915572
488.538756	31663.468932	30.920589
489.515714	31711.879825	30.925607
489.517462	31759.261401	30.930624
490.693338	31794.997756	30.935642
491.294113	31838.568470	30.940660
491.537162	31888.378053	30.945677
492.059970	31926.069218	30.950695
492.362555	31980.263374	30.955712
492.419192	32033.604809	30.960730
493.377965	32083.062524	30.965748
493.508616	32139.269095	30.970765
494.148916	32185.685523	30.975783
494.333556	32245.582247	30.980800
494.832678	32293.367600	30.985818
495.360303	32353.166657	30.990836
495.776065	32411.213251	30.995853
496.598365	32465.946820	31.000871
496.883391	32536.411690	31.005888
497.259979	32589.223955	31.010906
497.379349	32641.634097	31.015924
497.963243	32714.082134	31.020941
498.698164	32771.909043	31.025959
499.453051	32836.750531	31.030976
499.530699	32882.156584	31.035994
500.153404	32942.372338	31.041012
501.084116	33007.736844	31.046029
501.739836	33059.804815	31.051047
502.343442	33117.077926	31.056064
502.904700	33167.099923	31.061082
503.168299	33222.997756	31.066100
503.231123	33288.840472	31.071117
504.189237	33337.371888	31.076135
504.325380	33404.904173	31.081152
504.691405	33447.149393	31.086170
505.756460	33513.095051	31.091188
505.982180	33569.094572	31.096205
506.649196	33623.684785	31.101223
507.029277	33678.554009	31.106240
507.550167	33736.891279	31.111258
508.004963	33798.166334	31.116276
508.570855	33857.388348	31.121293
509.962402	33898.658260	31.126311
510.405870	33949.806995	31.131328
510.736755	33986.261116	31.136346
511.453153	34040.939514	31.141364
511.710296	34087.268426	31.146381
512.249115	34136.354192	31.151399
512.697735	34195.001207	31.156416
513.193743	34234.755543	31.161434
513.487335	34289.646226	31.166452
513.775809	34345.985722	31.171469
514.476374	34389.267916	31.176487
514.796662	34452.506973	31.181504
515.303501	34508.338505	31.186522
515.976579	34553.231286	31.191540
516.458300	34603.142699	31.196557
517.042237	34645.191801	31.201575
517.360909	34706.098809	31.206592
517.976063	34763.747627	31.211610
518.534796	34812.699069	31.216628
518.979671	34866.220818	31.221645
519.460416	34907.812401	31.226663
520.169726	34966.016069	31.231680
520.605148	35014.013586	31.236698
521.532372	35072.417359	31.241716
521.597177	35122.098124	31.246733
521.769681	35170.744164	31.251751
522.171805	35232.183374	31.256768
522.688499	35286.782463	31.261786
523.451895	35346.167400	31.266804
523.746747	35415.293580	31.271821
524.173459	35468.939829	31.276839
524.542633	35527.691498	31.281856
524.801203	35592.429507	31.286874
525.521451	35664.385776	31.291892
525.940215	35727.075757	31.296909
527.472475	35786.657653	31.301927
527.766482	35840.338269	31.306944
528.032993	35901.421273	31.311962
528.816664	35958.888868	31.316980
529.289501	36027.495961	31.321997
529.879211	36091.096054	31.327015
530.340881	36141.741381	31.332032
531.030154	36203.018281	31.337050
531.561143	36256.947370	31.342068
531.850956	36324.603999	31.347085
532.458994	36378.148261	31.352103
533.222211	36429.828305	31.357120
533.404279	36494.100471	31.362138
534.384123	36553.726774	31.367156
535.170539	36608.331270	31.372173
535.671282	36659.319483	31.377191
536.404969	36722.279228	31.382208
536.786410	36774.987363	31.387226
538.086484	36816.327886	31.392244
538.384426	36873.538886	31.397261
538.765101	36919.639631	31.402279
539.209171	36967.368292	31.407296
539.612472	37017.316621	31.412314
540.236159	37063.411231	31.417332
540.614939	37121.457565	31.422349
541.523419	37177.460836	31.427367
541.430298	37237.725030	31.432384
541.705165	37294.574009	31.437402
542.192502	37357.403472	31.442420
542.453337	37413.591000	31.447437
543.060797	37478.868161	31.452455
543.748866	37548.654209	31.457472
544.086048	37618.305735	31.462490
544.603590	37686.557025	31.467508
545.321704	37749.648698	31.472525
546.218824	37823.917932	31.477543
546.619075	37887.072439	31.482560
546.721735	37952.398481	31.487578
547.819516	38003.979334	31.492596
547.840594	38082.395862	31.497613
548.633289	38133.563181	31.502631
549.460021	38211.000296	31.507648
549.315052	38277.833208	31.512666
550.499016	38337.603244	31.517684
550.977672	38398.976321	31.522701
551.784641	38453.784654	31.527719
552.401378	38504.645252	31.532736
553.091670	38551.617953	31.537754
553.751000	38592.556353	31.542772
554.020708	38651.401725	31.547789
554.802107	38699.701133	31.552807
555.850591	38746.415795	31.557824
556.342661	38800.287805	31.562842
556.862222	38845.276890	31.567860
557.104726	38894.432651	31.572877
557.761227	38945.344974	31.577895
558.066498	39003.186551	31.582912
558.278835	39055.433487	31.587930
558.824059	39110.214917	31.592948
559.043243	39175.570672	31.597965
559.830768	39236.960991	31.602983
560.604378	39287.811510	31.608000
560.694080	39361.061517	31.613018
561.144150	39422.201659	31.618036
561.779250	39484.856069	31.623053
562.356201	39567.326863	31.628071
562.865351	39621.381637	31.633088
563.442173	39690.610210	31.638106
564.271423	39752.640516	31.643124
564.753674	39831.984038	31.648141
565.207734	39885.592755	31.653159
565.552578	39958.444334	31.658176
566.221998	40033.541021	31.663194
567.108429	40095.519079	31.668212
567.704803	40173.271230	31.673229
568.013313	40229.819085	31.678247
569.025488	40306.633836	31.683264
569.180912	40373.887822	31.688282
569.908673	40427.315871	31.693300
569.934202	40512.924947	31.698317
570.544596	40586.673041	31.703335
571.328168	40663.360416	31.708352
571.658055	40744.065571	31.713370
572.248697	40818.734586	31.718388
572.699476	40895.025857	31.723405
573.477535	40963.676721	31.728423
574.058202	41039.865935	31.733440
574.952698	41117.954227	31.738458
575.407347	41176.657290	31.743476
576.391506	41250.406003	31.748493
577.081318	41331.543945	31.753511
577.743399	41382.163833	31.758528
578.361472	41449.399260	31.763546
579.357689	41510.643128	31.768564
579.885393	41575.717410	31.773581
580.784599	41632.220646	31.778599
581.434843	41684.240846	31.783616
582.186777	41744.530646	31.788634
583.149550	41793.150046	31.793652
583.642533	41842.342788	31.798669
584.280121	41898.894010	31.803687
584.816096	41941.451871	31.808704
585.360512	41986.215849	31.813722
586.021748	42032.580777	31.818740
586.280065	42084.075097	31.823757
586.877981	42136.572600	31.828775
587.590958	42184.112490	31.833792
587.794309	42245.185314	31.838810
588.837619	42287.828835	31.843828
588.723593	42351.057848	31.848845
589.055447	42409.024443	31.853863
590.115203	42457.819873	31.858880
590.129866	42519.713625	31.863898
590.912707	42573.802397	31.868916
591.245829	42645.968987	31.873933
591.532757	42703.519617	31.878951
592.271418	42762.346878	31.883968
592.673310	42827.577386	31.888986
593.050577	42899.813790	31.894004
593.700256	42966.346814	31.899021
594.100318	43038.674977	31.904039
594.882039	43102.328781	31.909056
595.347552	43167.069615	31.914074
595.815510	43229.280190	31.919092
596.293058	43300.407942	31.924109
596.949827	43376.802047	31.929127
597.569953	43447.142590	31.934144
598.108933	43536.737462	31.939162
598.904781	43606.057923	31.944180
599.725272	43667.272049	31.949197
599.809643	43739.873324	31.954215
600.759231	43807.968529	31.959232
601.207648	43881.841570	31.964250
601.764129	43959.619660	31.969268
602.340567	44043.808844	31.974285
602.806158	44126.662066	31.979303
603.683551	44193.991734	31.984320
604.025748	44279.369721	31.989338
604.628821	44342.903247	31.994356
605.314548	44426.640302	31.999373
605.697243	44519.603468	32.004391
606.254946	44587.458805	32.009408
607.141738	44686.852706	32.014426
608.106124	44755.454535	32.019444
608.752232	44837.605285	32.024461
609.380275	44916.855697	32.029479
610.201829	44979.686299	32.034496
610.698917	45065.428894	32.039514
611.469981	45135.314650	32.044532
612.113153	45202.772601	32.049549
612.927706	45284.348271	32.054567
613.221233	45358.370639	32.059584
613.996923	45440.471675	32.064602
614.226627	45502.738554	32.069620
614.945509	45583.507940	32.074637
615.299710	45660.368422	32.079655
616.407144	45735.074271	32.084672
616.932469	45816.709824	32.089690
617.246516	45891.312714	32.094708
618.180761	45969.044947	32.099725
618.758646	46060.959127	32.104743
619.430709	46127.738451	32.109760
620.194416	46195.256415	32.114778
620.610080	46266.314725	32.119796
621.480502	46341.325398	32.124813
622.123803	46428.758322	32.129831
622.776578	46496.604539	32.134848
623.434475	46573.515463	32.139866
623.897970	46647.161183	32.144884
624.701741	46724.884825	32.149901
624.940178	46799.097683	32.154919
625.757788	46873.605976	32.159936
626.429366	46961.783023	32.164954
627.027492	47036.648863	32.169972
627.372025	47113.161536	32.174989
628.029441	47197.931867	32.180007
628.968428	47259.428248	32.185024
629.690525	47338.394088	32.190042
630.206136	47407.150200	32.195060
630.961284	47479.221974	32.200077
631.482131	47559.820672	32.205095
632.136629	47628.150812	32.210112
632.720010	47693.936423	32.215130
633.629739	47767.237533	32.220148
634.165576	47833.745882	32.225165
634.852678	47898.231570	32.230183
635.550885	47957.243287	32.235200
636.109863	48028.316307	32.240218
636.542040	48087.876146	32.245236
637.564467	48159.326177	32.250253
638.080981	48225.035224	32.255271
638.889927	48289.104363	32.260288
639.307821	48368.235298	32.265306
640.037600	48432.348871	32.270324
640.611557	48494.298010	32.275341
641.136877	48571.154214	32.280359
642.110392	48632.800741	32.285376
642.374996	48703.637265	32.290394
642.676677	48776.897661	32.295412
643.629579	48855.117694	32.300429
643.682557	48939.293224	32.305447
644.733977	49022.338372	32.310464
645.544654	49090.085348	32.315482
645.598107	49173.312642	32.320500
646.372917	49250.163686	32.325517
646.874866	49339.047139	32.330535
647.482905	49417.607809	32.335552
648.294153	49506.759817	32.340570
648.967707	49593.301726	32.345588
650.042679	49679.072476	32.350605
650.463592	49757.581363	32.355623
651.217657	49837.354362	32.360640
651.754681	49922.830647	32.365658
652.347491	50005.495627	32.370676
653.468501	50080.529981	32.375693
653.823092	50173.931959	32.380711
655.194429	50253.090904	32.385728
655.693796	50317.372371	32.390746
656.391697	50391.531256	32.395764
657.314214	50458.157495	32.400781
657.307259	50539.937605	32.405799
658.047139	50613.812232	32.410816
659.048090	50686.412397	32.415834
659.534307	50776.158032	32.420852
660.611990	50849.550255	32.425869
660.317292	50940.045223	32.430887
661.516229	51010.565351	32.435904
661.866780	51093.417689	32.440922
662.404756	51178.341660	32.445940
664.212931	51238.630619	32.450957
665.252500	51305.070125	32.455975
666.250314	51357.418857	32.460992
667.141345	51419.541342	32.466010
667.854008	51476.921024	32.471028
668.452746	51528.959321	32.476045
668.991321	51592.776281	32.481063
669.639706	51647.002706	32.486080
670.119761	51711.373322	32.491098
670.796679	51774.618621	32.496116
671.112195	51841.122434	32.501133
671.624740	51920.972074	32.506151
672.136820	51991.242078	32.511168
672.691812	52059.145372	32.516186
673.436652	52133.739081	32.521204
673.825703	52199.498393	32.526221
674.318919	52284.338494	32.531239
675.143819	52353.295063	32.536256
675.792302	52440.838653	32.541274
675.853438	52523.962874	32.546292
676.531774	52599.005097	32.551309
677.123728	52685.052446	32.556327
677.776114	52761.801429	32.561344
677.893691	52841.462955	32.566362
678.516714	52931.461235	32.571380
679.645028	53008.085868	32.576397
679.940043	53098.889175	32.581415
680.351285	53185.086889	32.586432
681.262030	53266.492379	32.591450
681.992613	53370.960159	32.596468
682.623628	53445.860631	32.601485
683.060152	53549.305824	32.606503
683.751608	53638.498765	32.611520
684.294151	53738.884400	32.616538
685.093450	53835.534646	32.621556
685.833693	53925.005796	32.626573
686.521225	54036.229042	32.631591
687.052038	54120.614260	32.636608
687.983682	54224.655662	32.641626
688.424632	54317.560756	32.646644
689.285995	54421.000191	32.651661
689.708904	54534.545392	32.656679
690.463119	54621.428724	32.661696
691.973327	54705.542413	32.666714
692.720316	54806.039786	32.671732
693.617136	54895.679938	32.676749
694.114769	54989.395149	32.681767
694.719515	55078.727342	32.686784
695.396422	55170.934343	32.691802
696.058477	55265.814644	32.696820
697.202761	55355.348164	32.701837
697.399566	55450.814671	32.706855
698.377248	55541.419189	32.711872
699.686065	55639.218411	32.716890
700.005984	55721.484306	32.721908
701.069776	55823.569145	32.726925
701.497385	55910.179247	32.731943
702.333707	55994.308106	32.736960
703.054067	56082.062776	32.741978
703.830950	56179.941190	32.746996
704.384811	56268.975706	32.752013
704.927797	56359.164092	32.757031
705.880860	56449.307584	32.762048
706.893867	56543.169699	32.767066
707.361903	56627.491366	32.772084
708.093144	56708.974755	32.777101
708.646524	56802.859235	32.782119
709.431009	56889.018271	32.787136
710.257398	56991.797151	32.792154
710.729590	57078.126020	32.797172
711.702004	57162.674369	32.802189
712.618027	57252.725418	32.807207
713.029740	57340.286197	32.812224
713.833735	57436.387036	32.817242
714.171452	57525.168922	32.822260
714.829421	57617.635150	32.827277
715.615136	57724.562756	32.832295
716.200313	57813.699357	32.837312
717.060101	57898.672993	32.842330
717.401149	58008.272780	32.847348
718.686367	58096.034955	32.852365
719.200578	58197.083021	32.857383
719.704081	58292.082401	32.862400
720.765072	58387.558157	32.867418
721.684313	58486.714836	32.872436
722.507408	58574.310602	32.877453
723.252145	58654.678158	32.882471
723.599074	58751.254551	32.887488
725.208898	58829.392185	32.892506
725.442926	58911.859653	32.897524
726.418996	58984.963864	32.902541
726.873432	59052.383836	32.907559
727.770866	59129.121252	32.912576
728.751279	59215.884522	32.917594
729.300449	59285.701849	32.922612
730.048738	59354.728648	32.927629
730.504264	59447.885502	32.932647
731.703140	59523.956660	32.937664
732.678200	59595.284248	32.942682
734.028365	59650.798862	32.947700
734.904521	59712.647846	32.952717
735.696405	59774.795019	32.957735
736.579532	59847.182135	32.962752
737.252128	59902.835079	32.967770
737.739714	59977.835389	32.972788
738.889999	60034.002489	32.977805
739.359644	60094.675475	32.982823
739.690758	60173.587349	32.987840
740.092535	60249.817244	32.992858
740.283314	60341.993540	32.997876
741.053975	60420.020830	33.002893
741.643107	60500.558094	33.007911
742.667413	60586.819303	33.012928
742.997017	60668.334580	33.017946
743.633600	60766.443390	33.022964
744.101364	60853.653558	33.027981
744.713678	60947.082737	33.032999
745.304315	61043.091969	33.038016
746.379015	61144.501230	33.043034
747.214796	61241.289417	33.048052
747.216324	61344.551347	33.053069
747.964727	61453.849595	33.058087
748.516469	61558.134020	33.063104
749.366677	61666.866548	33.068122
749.983836	61786.270740	33.073140
750.786931	61893.093598	33.078157
751.552876	61993.092417	33.083175
752.400857	62108.885440	33.088192
753.296534	62206.991051	33.093210
754.278322	62314.889213	33.098228
754.964481	62418.668777	33.103245
755.752546	62527.693348	33.108263
756.426959	62639.952034	33.113280
757.379231	62749.825459	33.118298
758.064061	62854.569274	33.123316
758.768101	62967.261597	33.128333
759.751383	63054.633012	33.133351
760.511132	63169.248326	33.138368
761.178464	63269.951420	33.143386
762.042227	63390.331254	33.148404
762.274296	63498.719122	33.153421
763.343152	63606.868800	33.158439
764.007531	63713.499620	33.163456
764.910065	63820.758321	33.168474
765.981900	63932.428804	33.173492
766.638775	64045.500554	33.178509
767.531897	64145.424783	33.183527
767.960953	64247.504913	33.188544
769.110052	64354.505708	33.193562
770.137253	64455.467422	33.198580
770.669660	64562.502364	33.203597
771.566496	64661.908933	33.208615
772.036011	64777.108840	33.213632
772.834847	64878.481536	33.218650
773.696881	64983.117861	33.223668
774.496519	65090.201830	33.228685
775.446601	65196.920818	33.233703
776.062194	65294.746845	33.238720
777.222618	65382.206251	33.243738
777.740469	65478.902370	33.248756
778.365986	65575.784594	33.253773
779.750208	65675.479705	33.258791
779.955846	65770.237843	33.263808
780.707342	65862.467011	33.268826
781.537840	65964.136666	33.273844
782.172285	66070.237649	33.278861
783.290080	66159.745079	33.283879
783.710543	66260.201209	33.288896
784.751864	66360.566844	33.293914
785.615027	66464.348047	33.298932
786.746373	66547.833605	33.303949
787.261168	66640.393904	33.308967
788.284442	66741.688250	33.313984
789.239034	66845.545327	33.319002
789.681074	66943.664466	33.324020
790.599182	67041.076283	33.329037
791.150496	67127.598713	33.334055
792.029974	67233.590188	33.339072
792.316104	67336.559883	33.344090
792.901870	67449.075437	33.349108
793.928140	67550.024278	33.354125
794.989982	67660.560392	33.359143
795.711011	67773.062516	33.364160
796.469053	67876.378369	33.369178
797.016143	67993.283900	33.374196
797.907303	68103.019188	33.379213
799.006362	68210.442945	33.384231
799.637898	68325.494212	33.389248
800.787000	68427.744282	33.394266
801.697085	68536.591995	33.399284
801.906454	68640.262765	33.404301
802.901294	68757.373916	33.409319
803.566426	68872.245063	33.414336
804.369341	68980.345261	33.419354
804.787014	69093.787122	33.424372
806.153397	69211.101758	33.429389
806.869218	69328.531461	33.434407
807.053776	69453.928333	33.439424
807.785008	69569.742031	33.444442
808.801612	69686.328404	33.449460
809.593210	69813.677235	33.454477
810.614566	69940.104202	33.459495
811.253584	70057.454238	33.464512
812.180478	70180.028166	33.469530
813.171955	70302.263277	33.474548
813.476476	70423.061444	33.479565
814.637717	70551.020884	33.484583
815.463400	70678.096303	33.489600
816.146339	70799.533512	33.494618
816.804324	70924.078088	33.499636
817.536507	71046.661235	33.504653
818.268700	71163.647021	33.509671
819.311921	71293.680297	33.514688
820.239314	71417.488447	33.519706
821.327362	71541.626648	33.524724
822.242399	71669.984722	33.529741
822.956784	71785.696871	33.534759
824.091596	71909.956137	33.539776
824.709336	72033.461039	33.544794
825.557188	72151.079034	33.549812
826.288772	72283.521769	33.554829
827.347025	72399.904697	33.559847
827.716915	72521.854823	33.564864
828.739388	72641.106851	33.569882
829.440560	72760.967022	33.574900
830.077997	72880.761718	33.579917
831.360685	72986.776767	33.584935
832.051293	73107.602761	33.589952
832.763972	73218.647706	33.594970
833.869139	73330.176294	33.599988
834.380737	73456.896279	33.605005
835.306009	73574.799776	33.610023
835.911944	73697.946944	33.615040
836.431700	73817.384290	33.620058
837.540204	73937.743285	33.625076
838.204525	74066.101532	33.630093
838.715958	74179.436599	33.635111
839.685842	74306.937500	33.640128
840.684570	74442.895753	33.645146
841.672383	74570.205098	33.650164
842.308444	74700.572131	33.655181
843.291687	74813.417993	33.660199
843.946703	74952.700663	33.665216
844.849173	75081.951147	33.670234
845.882401	75214.677847	33.675252
846.762757	75337.498220	33.680269
847.851143	75470.306209	33.685287
848.621350	75607.724832	33.690304
849.533886	75740.941698	33.695322
850.017614	75868.526110	33.700340
850.641078	75997.951332	33.705357
851.370116	76133.124286	33.710375
852.435810	76278.733822	33.715392
853.685818	76416.930130	33.720410
854.486990	76543.150582	33.725428
855.624502	76675.298063	33.730445
856.512674	76806.205794	33.735463
857.231586	76944.931311	33.740480
857.676949	77080.140715	33.745498
859.070232	77211.896046	33.750516
859.926410	77336.388724	33.755533
860.834800	77465.560942	33.760551
861.577854	77606.718284	33.765568
862.436947	77742.588251	33.770586
863.327018	77875.350339	33.775604
864.174515	78002.216344	33.780621
865.289870	78138.428187	33.785639
866.078792	78269.067074	33.790656
867.030957	78407.826803	33.795674
868.368309	78543.347129	33.800692
869.259731	78666.598801	33.805709
870.385386	78794.729755	33.810727
871.063918	78917.686498	33.815744
871.776487	79051.178814	33.820762
872.898366	79171.862910	33.825780
873.540234	79300.730734	33.830797
874.766830	79421.614890	33.835815
875.316066	79560.937577	33.840832
876.116058	79680.698779	33.845850
877.067863	79805.681709	33.850868
877.719313	79941.189580	33.855885
878.595817	80065.590018	33.860903
879.436624	80191.377546	33.865920
880.185384	80335.461826	33.870938
880.965732	80467.062594	33.875956
881.600674	80608.125456	33.880973
882.916672	80742.760321	33.885991
883.574084	80871.544278	33.891008
884.190368	81016.007546	33.896026
885.023708	81145.614075	33.901044
885.964792	81285.264080	33.906061
886.963394	81421.573621	33.911079
888.477107	81549.618452	33.916096
889.447558	81677.394174	33.921114
890.207759	81800.401486	33.926132
891.155462	81936.746826	33.931149
891.968448	82056.440116	33.936167
892.579302	82182.183866	33.941184
893.150061	82310.797911	33.946202
893.842716	82431.892677	33.951220
894.818655	82567.653803	33.956237
895.660797	82703.816638	33.961255
896.272207	82828.904307	33.966272
896.916356	82974.006732	33.971290
898.002067	83114.935503	33.976308
898.653975	83268.160022	33.981325
899.270386	83412.052640	33.986343
900.399159	83563.544218	33.991360
901.474774	83699.789286	33.996378
903.055063	83838.844935	34.001396
903.886311	83984.417357	34.006413
905.210117	84119.662571	34.011431
905.993872	84252.838908	34.016448
906.831388	84393.635443	34.021466
908.235495	84529.427541	34.026484
908.785055	84669.611613	34.031501
909.611888	84805.165949	34.036519
910.416321	84944.285074	34.041536
911.225675	85091.184337	34.046554
912.362811	85228.681483	34.051572
912.980415	85374.154989	34.056589
913.661491	85518.567544	34.061607
914.897864	85668.570770	34.066624
915.540246	85813.485045	34.071642
916.938816	85956.621636	34.076660
917.381872	86122.122292	34.081677
918.429856	86255.405860	34.086695
919.691604	86406.283278	34.091712
920.538227	86554.349922	34.096730
921.322912	86687.524626	34.101748
921.898528	86848.725473	34.106765
923.143665	86997.644357	34.111783
923.981125	87143.447086	34.116800
924.670424	87306.305389	34.121818
925.774952	87467.515523	34.126836
926.774648	87624.865170	34.131853
927.577009	87779.889458	34.136871
928.622905	87925.207211	34.141888
929.448174	88080.406907	34.146906
930.519420	88239.066586	34.151924
931.380574	88392.551478	34.156941
932.567308	88542.399758	34.161959
933.718191	88689.631106	34.166976
934.341076	88841.457452	34.171994
935.323683	88991.403324	34.177012
935.961605	89162.580760	34.182029
937.121981	89315.364563	34.187047
938.295231	89462.608906	34.192064
938.823242	89630.194348	34.197082
939.912206	89783.181825	34.202100
940.617527	89936.901849	34.207117
941.414295	90094.220305	34.212135
942.801624	90253.373507	34.217152
943.306842	90415.010302	34.222170
944.590149	90562.661051	34.227188
945.749054	90729.672244	34.232205
946.255667	90880.373814	34.237223
947.218217	91037.912047	34.242240
948.020967	91199.658548	34.247258
949.298741	91354.576250	34.252276
950.299185	91509.411426	34.257293
951.459700	91658.240104	34.262311
952.444077	91818.592654	34.267328
952.738662	91966.252973	34.272346
953.946397	92108.764644	34.277364
955.135426	92261.204011	34.282381
956.071106	92409.843429	34.287399
956.761505	92557.875571	34.292416
957.617536	92714.564627	34.297434
958.676842	92863.072819	34.302452
959.456029	93024.782004	34.307469
960.155525	93184.730040	34.312487
961.271449	93338.212881	34.317504
962.146935	93513.192860	34.322522
963.541588	93661.031330	34.327540
964.338418	93826.176901	34.332557
964.810718	93981.588936	34.337575
966.092717	94143.770301	34.342592
966.678435	94316.455283	34.347610
967.797905	94479.259593	34.352628
968.894845	94645.452627	34.357645
969.784206	94804.365284	34.362663
971.353952	94978.180101	34.367680
971.988305	95145.170741	34.372698
972.793293	95310.411662	34.377716
973.808558	95474.555768	34.382733
974.911931	95649.017754	34.387751
976.121645	95821.828868	34.392768
977.349700	95992.787370	34.397786
978.509613	96145.326495	34.402804
979.440492	96302.959989	34.407821
980.239667	96476.029124	34.412839
981.400833	96635.985998	34.417856
982.029809	96794.467823	34.422874
982.854647	96970.818817	34.427892
984.241834	97144.661545	34.432909
985.349702	97317.141867	34.437927
986.281574	97485.327968	34.442944
987.180421	97655.966724	34.447962
988.265059	97818.210671	34.452980
989.058746	98001.050069	34.457997
989.908865	98161.291519	34.463015
991.034500	98327.968540	34.468032
991.616020	98502.781509	34.473050
992.658235	98684.597098	34.478068
994.008405	98856.122382	34.483085
995.051468	99033.692980	34.488103
995.914106	99202.913135	34.493120
996.798376	99392.059562	34.498138
997.728505	99564.288253	34.503156
998.726562	99745.951947	34.508173
999.470828	99932.740095	34.513191
1001.056017	100091.671705	34.518208
1002.222487	100280.842534	34.523226
1003.108027	100460.638875	34.528244
1004.031328	100633.267327	34.533261
1005.782226	100802.584967	34.538279
1006.705480	100968.457887	34.543296
1007.714963	101141.557298	34.548314
1008.765453	101297.992202	34.553332
1009.851240	101470.675709	34.558349
1011.174181	101641.471975	34.563367
1012.073598	101792.747503	34.568384
1013.053206	101962.470827	34.573402
1013.673288	102134.254504	34.578420
1014.666023	102303.533784	34.583437
1015.867759	102452.875918	34.588455
1016.678419	102626.534096	34.593472
1017.569946	102787.628653	34.598490
1018.720936	102945.222081	34.603508
1020.316445	103106.639043	34.608525
1020.937664	103255.137454	34.613543
1022.129459	103408.542677	34.618560
1022.768721	103561.806893	34.623578
1023.602100	103723.194024	34.628596
1024.619137	103890.841999	34.633613
1025.499298	104055.405856	34.638631
1026.572382	104217.594664	34.643648
1027.643020	104388.127593	34.648666
1028.483666	104544.914972	34.653684
1029.560020	104718.225452	34.658701
1030.341399	104886.092806	34.663719
1031.495029	105056.628807	34.668736
1032.282111	105243.630435	34.673754
1032.640516	105409.702713	34.678772
1034.215481	105599.131557	34.683789
1035.065540	105791.756143	34.688807
1036.297066	105965.200873	34.693824
1037.210721	106154.470075	34.698842
1038.085449	106341.210423	34.703860
1039.172555	106515.923205	34.708877
1039.873921	106723.957248	34.713895
1041.060740	106914.658786	34.718912
1042.398137	107116.775418	34.723930
1042.826822	107300.547562	34.728948
1044.374995	107494.302425	34.733965
1044.650151	107699.238993	34.738983
1046.028904	107894.797899	34.744000
1046.944658	108101.044094	34.749018
1048.064511	108299.372157	34.754036
1048.935992	108497.448581	34.759053
1050.081920	108719.754332	34.764071
1051.200204	108914.383334	34.769088
1052.409772	109122.085931	34.774106
1053.497254	109319.017272	34.779124
1054.243060	109525.577487	34.784141
1055.768589	109737.736077	34.789159
1057.052155	109942.832297	34.794176
1057.998726	110153.777864	34.799194
1059.066241	110349.868452	34.804212
1060.386980	110555.913525	34.809229
1061.174008	110764.795264	34.814247
1062.631819	110967.181648	34.819264
1063.610110	111170.646118	34.824282
1064.329423	111377.398842	34.829300
1065.404694	111597.184750	34.834317
1066.219387	111804.102557	34.839335
1067.820743	112006.713324	34.844352
1068.906243	112211.244905	34.849370
1070.150003	112408.004058	34.854388
1071.448204	112615.434222	34.859405
1072.557257	112828.805159	34.864423
1074.159254	113019.068936	34.869440
1075.416785	113211.150507	34.874458
1076.690746	113404.359269	34.879476
1077.820256	113586.773418	34.884493
1079.047297	113765.926451	34.889511
1080.195395	113957.635938	34.894528
1081.281060	114141.353365	34.899546
1082.382723	114318.030229	34.904564
1083.355466	114502.718363	34.909581
1084.257215	114697.818587	34.914599
1085.169967	114874.794050	34.919616
1086.465854	115062.567119	34.924634
1087.173136	115257.459774	34.929652
1088.425269	115438.164394	34.934669
1089.474313	115639.321808	34.939687
1090.448773	115812.918346	34.944704
1091.654615	115992.072861	34.949722
1092.497208	116172.261737	34.954740
1093.575943	116347.632818	34.959757
1094.552971	116531.620132	34.964775
1095.631439	116721.312807	34.969792
1096.553015	116906.135083	34.974810
1097.473924	117096.171416	34.979828
1098.828297	117281.549289	34.984845
1099.846883	117465.052689	34.989863
1100.894351	117655.313026	34.994880
1102.296596	117837.464406	34.999898
1103.569388	118022.224490	35.004916
1104.866210	118211.839750	35.009933
1105.704627	118396.213031	35.014951
1106.658933	118582.344863	35.019968
1107.966924	118779.774736	35.024986
1108.554277	118968.705725	35.030004
1110.170956	119168.106102	35.035021
1110.917201	119365.271779	35.040039
1112.307015	119566.853438	35.045056
1113.037117	119752.886532	35.050074
1114.008788	119951.681616	35.055092
1115.384840	120155.031688	35.060109
1116.429449	120354.210654	35.065127
1117.891294	120556.762944	35.070144
1118.903805	120762.532521	35.075162
1119.720780	120969.285180	35.080180
1121.079738	121168.203458	35.085197
1121.914695	121369.120253	35.090215
1123.024195	121579.673966	35.095232
1124.294745	121787.285967	35.100250
1125.477418	121991.741469	35.105268
1126.676649	122190.626515	35.110285
1127.941081	122403.215431	35.115303
1129.216896	122611.554027	35.120320
1130.348457	122810.769930	35.125338
1131.120612	123022.538556	35.130356
1132.076432	123224.853998	35.135373
1133.457065	123451.587703	35.140391
1134.610498	123654.432567	35.145408
1135.751639	123866.388938	35.150426
1136.907518	124085.448328	35.155444
1137.831706	124296.895436	35.160461
1139.078647	124505.058141	35.165479
1140.471767	124729.729260	35.170496
1141.347202	124938.066534	35.175514
1142.307921	125163.822664	35.180532
1143.282431	125374.912310	35.185549
1144.288955	125592.962955	35.190567
1145.375483	125814.909721	35.195584
1146.683813	126034.615482	35.200602
1147.990359	126275.116303	35.205620
1148.950536	126478.804822	35.210637
1150.141202	126709.773147	35.215655
1151.478269	126934.883840	35.220672
1152.383188	127161.801537	35.225690
1153.641313	127388.246506	35.230708
1155.352521	127606.768418	35.235725
1156.400562	127826.676709	35.240743
1157.278784	128046.384372	35.245760
1158.652152	128269.986821	35.250778
1159.992611	128494.039676	35.255796
1161.325925	128707.450025	35.260813
1162.289797	128934.444244	35.265831
1163.733975	129149.869489	35.270848
1164.720305	129355.636041	35.275866
1165.865569	129563.193060	35.280884
1166.892251	129770.452462	35.285901
1168.023243	129982.061175	35.290919
1169.126207	130192.520722	35.295936
1170.829462	130395.845483	35.300954
1171.572862	130597.101062	35.305972
1172.956258	130806.466612	35.310989
1174.366277	131007.353302	35.316007
1174.939765	131219.765935	35.321024
1176.084577	131425.352676	35.326042
1177.042703	131636.044966	35.331060
1178.300047	131839.027622	35.336077
1179.402746	132057.896052	35.341095
1180.603201	132284.769447	35.346112
1182.033330	132495.899545	35.351130
1182.887226	132724.948474	35.356148
1184.001571	132942.525256	35.361165
1185.488553	133174.243562	35.366183
1186.371134	133395.868530	35.371200
1187.142232	133624.909715	35.376218
1188.598047	133853.616487	35.381236
1189.673713	134085.378570	35.386253
1190.891471	134328.133791	35.391271
1191.794426	134561.130849	35.396288
1192.729074	134791.421338	35.401306
1194.186743	135034.586950	35.406324
1195.059752	135281.043135	35.411341
1196.566134	135530.091681	35.416359
1197.386057	135764.846415	35.421376
1198.819427	136006.777479	35.426394
1200.183151	136259.367379	35.431412
1201.531207	136504.156926	35.436429
1202.790361	136752.502159	35.441447
1203.980741	137010.186575	35.446464
1205.312661	137246.429612	35.451482
1206.207389	137500.774830	35.456500
1207.446973	137750.892413	35.461517
1208.885432	137984.965219	35.466535
1210.164321	138231.817862	35.471552
1211.654271	138481.291040	35.476570
1212.474434	138739.385635	35.481588
1213.555805	138985.004127	35.486605
1214.812631	139238.616829	35.491623
1216.360702	139494.571124	35.496640
1217.628814	139742.004448	35.501658
1218.616517	139996.868944	35.506676
1219.971833	140248.948737	35.511693
1221.591089	140497.752376	35.516711
1223.006535	140739.786888	35.521728
1223.761316	140986.317114	35.526746
1225.613635	141238.146620	35.531764
1226.988847	141474.645135	35.536781
1228.428397	141721.922213	35.541799
1229.547561	141971.776255	35.546816
1231.155071	142193.037811	35.551834
1232.488872	142425.511594	35.556852
1233.929502	142665.127705	35.561869
1235.302106	142900.948192	35.566887
1236.185453	143119.420935	35.571904
1237.698907	143345.575939	35.576922
1238.365109	143589.074465	35.581940
1240.025307	143830.362521	35.586957
1241.321866	144062.570601	35.591975
1242.535394	144290.426770	35.596992
1243.670599	144523.880658	35.602010
1244.781841	144751.475705	35.607028
1245.914377	144998.474500	35.612045
1247.086611	145238.830339	35.617063
1248.003231	145474.810472	35.622080
1249.386142	145694.117345	35.627098
1250.114894	145934.850500	35.632116
1251.344524	146160.757940	35.637133
1252.316656	146395.946705	35.642151
1253.134669	146635.514161	35.647168
1254.496507	146874.667590	35.652186
1255.584765	147123.841267	35.657204
1256.775306	147368.608492	35.662221
1258.090378	147617.419014	35.667239
1259.003034	147868.337237	35.672256
1260.085005	148124.979972	35.677274
1261.314924	148390.054217	35.682292
1262.529567	148652.123965	35.687309
1263.809466	148914.552887	35.692327
1264.493010	149182.991399	35.697344
1266.409759	149451.885557	35.702362
1267.469550	149726.297104	35.707380
1268.879326	149988.177841	35.712397
1270.018760	150270.779499	35.717415
1271.518682	150550.850997	35.722432
1272.748437	150822.017380	35.727450
1273.990398	151095.049136	35.732468
1274.942749	151369.206536	35.737485
1276.581152	151641.874305	35.742503
1277.845509	151917.953096	35.747520
1279.243053	152199.305690	35.752538
1280.538778	152481.132620	35.757556
1281.695130	152761.916505	35.762573
1283.374478	153041.502861	35.767591
1284.685955	153322.455670	35.772608
1285.986084	153597.712031	35.777626
1287.238826	153883.386299	35.782644
1288.546115	154174.067653	35.787661
1289.727571	154455.122571	35.792679
1290.499448	154739.987791	35.797696
1291.921515	155027.177257	35.802714
1293.404360	155326.722988	35.807732
1294.484452	155606.085620	35.812749
1296.438624	155892.929482	35.817767
1297.887307	156183.814589	35.822784
1298.988945	156470.083823	35.827802
1300.585792	156755.718355	35.832820
1301.678973	157038.703726	35.837837
1303.336900	157325.791332	35.842855
1304.282861	157630.294917	35.847872
1305.467531	157915.479019	35.852890
1307.061995	158199.115002	35.857908
1308.392016	158488.557274	35.862925
1309.797981	158773.380694	35.867943
1310.568446	159082.793970	35.872960
1311.970769	159361.590468	35.877978
1313.616664	159654.429211	35.882996
1315.117769	159947.545909	35.888013
1316.280853	160244.627095	35.893031
1317.571202	160544.241566	35.898048
1319.181449	160825.386125	35.903066
1320.524920	161105.773870	35.908084
1321.811524	161391.415071	35.913101
1323.416180	161682.098756	35.918119
1324.727071	161973.032877	35.923136
1325.862114	162249.687620	35.928154
1327.412487	162543.519570	35.933172
1328.531822	162821.918556	35.938189
1329.868119	163108.194385	35.943207
1331.494584	163406.652360	35.948224
1332.546171	163694.867028	35.953242
1334.385090	163972.802765	35.958260
1335.751839	164255.536574	35.963277
1337.108454	164521.958441	35.968295
1337.905711	164799.590914	35.973312
1339.839044	165059.335240	35.978330
1341.002936	165325.866635	35.983348
1341.921725	165598.176254	35.988365
1343.529775	165860.056784	35.993383
1344.853385	166130.172137	35.998400
1346.293604	166403.507938	36.003418
1347.315923	166666.905247	36.008436
1348.413831	166950.962004	36.013453
1349.623542	167219.855152	36.018471
1351.025031	167514.316129	36.023488
1352.628457	167786.908081	36.028506
1353.909907	168069.569363	36.033524
1354.957359	168362.895774	36.038541
1356.361709	168637.083873	36.043559
1357.983528	168927.681705	36.048576
1359.220783	169214.836492	36.053594
1360.670791	169507.164959	36.058612
1361.995855	169797.038193	36.063629
1363.841063	170082.399800	36.068647
1364.954113	170380.752217	36.073664
1366.043125	170669.053264	36.078682
1367.370590	170965.406370	36.083700
1368.797349	171262.595835	36.088717
1370.285993	171543.282685	36.093735
1371.696494	171853.225346	36.098752
1373.016364	172138.156411	36.103770
1374.282362	172434.804232	36.108788
1375.665866	172741.097777	36.113805
1377.395044	173042.602152	36.118823
1378.653360	173333.146981	36.123840
1379.770535	173634.647853	36.128858
1381.189964	173936.800952	36.133876
1382.656741	174241.195334	36.138893
1384.362619	174536.461666	36.143911
1385.684317	174849.376049	36.148928
1387.115893	175141.119377	36.153946
1388.630492	175453.777335	36.158964
1389.934320	175750.380843	36.163981
1391.449100	176052.818998	36.168999
1392.836009	176368.954351	36.174016
1394.167691	176665.912335	36.179034
1395.657098	176973.513339	36.184052
1396.872371	177275.469471	36.189069
1398.769859	177579.351653	36.194087
1399.610393	177894.244907	36.199104
1401.262476	178185.443720	36.204122
1403.259179	178480.526145	36.209140
1404.287810	178788.866123	36.214157
1405.825544	179081.406495	36.219175
1407.285369	179383.763471	36.224192
1409.397189	179678.781110	36.229210
1411.030004	179967.347499	36.234228
1412.376823	180255.857990	36.239245
1414.300737	180541.688493	36.244263
1415.750856	180837.321456	36.249280
1416.940053	181115.903363	36.254298
1418.492684	181407.737815	36.259316
1419.393593	181701.605455	36.264333
1420.683953	181985.126777	36.269351
1421.904830	182281.841552	36.274368
1423.176905	182570.523352	36.279386
1425.009441	182859.702466	36.284404
1425.764569	183152.251307	36.289421
1427.084274	183447.836695	36.294439
1428.040526	183756.052224	36.299456
1429.747813	184064.481352	36.304474
1431.094688	184352.318587	36.309492
1432.286779	184651.610399	36.314509
1433.785736	184923.119367	36.319527
1435.189399	185283.566145	36.324544
1436.422619	185580.796948	36.329562
1437.909497	185885.583281	36.334580
1439.306898	186184.949066	36.339597
1440.440300	186479.378755	36.344615
1442.207457	186779.907541	36.349632
1443.627539	187079.221529	36.354650
1445.144199	187382.305782	36.359668
1446.411749	187687.715852	36.364685
1447.992807	187985.711789	36.369703
1449.476514	188302.214838	36.374720
1450.795701	188609.981589	36.379738
1452.276542	188914.167897	36.384756
1453.581010	189222.116442	36.389773
1455.127873	189533.914101	36.394791
1457.018477	189850.688045	36.399808
1458.447599	190164.487065	36.404826
1459.948079	190476.065941	36.409844
1461.026470	190782.987244	36.414861
1462.651601	191105.572038	36.419879
1463.955470	191429.960625	36.424896
1465.514548	191747.680593	36.429914
1467.252966	192085.516029	36.434932
1468.625308	192404.028955	36.439949
1470.129742	192727.271970	36.444967
1471.298860	193048.942650	36.449984
1472.684354	193378.708572	36.455002
1474.347503	193703.046884	36.460020
1475.793215	194034.811745	36.465037
1477.244452	194355.120693	36.470055
1478.822515	194691.997526	36.475072
1480.076199	195015.310929	36.480090
1482.026177	195344.460028	36.485108
1483.403812	195684.520478	36.490125
1484.856125	196019.184984	36.495143
1486.159515	196358.242656	36.500160
1487.479255	196684.013588	36.505178
1489.268743	197027.467452	36.510196
1490.189472	197375.579602	36.515213
1491.591458	197717.927278	36.520231
1493.162462	198058.420367	36.525248
1495.010707	198409.031569	36.530266
1496.823219	198752.282631	36.535284
1498.176288	199107.672292	36.540301
1499.813801	199451.028505	36.545319
1501.543737	199777.656453	36.550336
1503.044404	200123.245521	36.555354
1504.722581	200453.032806	36.560372
1506.399434	200791.965757	36.565389
1508.273395	201124.619595	36.570407
1509.879279	201459.018003	36.575424
1510.977793	201803.505007	36.580442
1512.662869	202131.287717	36.585460
1514.016473	202470.782645	36.590477
1515.603370	202790.249938	36.595495
1517.335350	203130.779203	36.600512
1519.005890	203464.485418	36.605530
1520.856367	203781.880980	36.610548
1522.576188	204111.058964	36.615565
1523.997095	204433.781201	36.620583
1525.322616	204760.227705	36.625600
1526.811863	205078.647238	36.630618
1529.022404	205408.004623	36.635636
1530.178656	205726.070847	36.640653
1531.835539	206042.509625	36.645671
1532.953346	206355.603849	36.650688
1534.355589	206661.083920	36.655706
1535.873030	206974.141897	36.660724
1537.210713	207288.092154	36.665741
1538.554675	207596.402376	36.670759
1539.841547	207922.351725	36.675776
1541.123206	208248.835812	36.680794
1542.380711	208569.328970	36.685812
1543.957953	208902.169290	36.690829
1545.173663	209234.736399	36.695847
1546.267073	209577.840057	36.700864
1548.145362	209916.502761	36.705882
1549.409896	210263.568862	36.710900
1550.894996	210604.935930	36.715917
1552.076600	210947.189233	36.720935
1554.001097	211314.272888	36.725952
1554.960754	211677.545068	36.730970
1556.803366	212029.984614	36.735988
1558.256399	212398.972450	36.741005
1559.769309	212771.101394	36.746023
1561.403628	213129.798653	36.751040
1562.691025	213508.949724	36.756058
1564.508963	213879.431738	36.761076
1566.251790	214257.038930	36.766093
1567.384622	214637.561794	36.771111
1569.029811	215005.709436	36.776128
1570.460096	215392.816869	36.781146
1572.227027	215772.784323	36.786164
1574.032503	216153.304968	36.791181
1575.519957	216533.088194	36.796199
1577.645131	216921.460048	36.801216
1578.996210	217311.045733	36.806234
1580.829111	217680.411016	36.811252
1582.439452	218065.485607	36.816269
1583.640112	218442.952592	36.821287
1585.685673	218834.234360	36.826304
1587.133997	219220.478242	36.831322
1588.777841	219593.430871	36.836340
1590.583432	219987.443701	36.841357
1592.442224	220381.168966	36.846375
1594.435052	220770.757993	36.851392
1595.823161	221148.654363	36.856410
1596.955421	221520.392337	36.861428
1599.020368	221912.892006	36.866445
1600.846192	222280.888910	36.871463
1602.412789	222665.007261	36.876480
1603.956938	223047.909829	36.881498
1605.765704	223432.015867	36.886516
1607.553972	223809.291487	36.891533
1608.993236	224183.852737	36.896551
1611.101267	224557.318607	36.901568
1612.549983	224936.756033	36.906586
1614.284961	225309.492805	36.911604
1616.100870	225686.865862	36.916621
1617.546924	226071.714785	36.921639
1619.312858	226438.273490	36.926656
1620.708020	226807.227362	36.931674
1622.163561	227180.083967	36.936692
1624.133807	227560.328756	36.941709
1625.673480	227937.922619	36.946727
1627.167708	228307.241782	36.951744
1628.550241	228691.236467	36.956762
1630.219397	229074.754307	36.961780
1631.588231	229457.302855	36.966797
1633.046361	229840.701019	36.971815
1635.018304	230225.568257	36.976832
1636.497398	230625.754852	36.981850
1637.727324	231000.271400	36.986868
1639.122219	231378.267687	36.991885
1640.800629	231742.628276	36.996903
1642.583259	232115.533478	37.001920
1643.608395	232504.205820	37.006938
1645.579810	232877.436652	37.011956
1647.249181	233252.238732	37.016973
1648.385199	233635.304060	37.021991
1650.177071	234026.116243	37.027008
1651.851135	234417.937290	37.032026
1653.404908	234798.472127	37.037044
1654.996314	235199.095139	37.042061
1656.398805	235599.290063	37.047079
1657.922123	235995.528098	37.052096
1659.238070	236397.183767	37.057114
1661.411084	236802.388406	37.062132
1663.062359	237217.581663	37.067149
1664.885868	237610.570104	37.072167
1667.085350	238008.706982	37.077184
1668.975812	238418.424947	37.082202
1670.318293	238818.092128	37.087220
1672.048622	239228.926431	37.092237
1673.640920	239631.144588	37.097255
1675.638380	240029.767700	37.102272
1676.987709	240447.340984	37.107290
1679.084576	240848.690919	37.112308
1681.038262	241265.101409	37.117325
1682.203848	241676.223664	37.122343
1683.857316	242084.423734	37.127360
1685.448168	242513.920785	37.132378
1686.994683	242921.247069	37.137396
1688.675670	243338.789040	37.142413
1690.246541	243774.688473	37.147431
1692.146289	244189.222476	37.152448
1693.559815	244618.032023	37.157466
1695.306766	245044.426058	37.162484
1697.366109	245474.682368	37.167501
1698.679922	245902.387146	37.172519
1700.850355	246323.250632	37.177536
1703.041905	246748.098125	37.182554
1704.526242	247176.992753	37.187572
1706.623608	247604.342521	37.192589
1708.332717	248025.147406	37.197607
1710.173363	248447.404067	37.202624
1711.638691	248876.475488	37.207642
1713.671388	249292.247860	37.212660
1715.673408	249706.423681	37.217677
1717.786268	250143.189080	37.222695
1719.364431	250546.506201	37.227712
1720.860993	250968.505603	37.232730
1722.363765	251387.607092	37.237748
1724.080440	251806.115147	37.242765
1725.648858	252237.676419	37.247783
1727.479607	252664.572292	37.252800
1729.001694	253090.905611	37.257818
1730.671220	253520.135812	37.262836
1732.460240	253952.495837	37.267853
1733.969654	254386.574809	37.272871
1736.159777	254806.498947	37.277888
1737.254264	255235.915555	37.282906
1738.811921	255670.262379	37.287924
1740.979089	256112.056567	37.292941
1742.557043	256541.698176	37.297959
1744.285899	256980.281312	37.302976
1745.962451	257419.506168	37.307994
1747.772901	257861.985263	37.313012
1749.313412	258296.300611	37.318029
1750.993582	258740.473431	37.323047
1752.980680	259177.611461	37.328064
1754.727755	259606.301722	37.333082
1756.470698	260032.933661	37.338100
1758.345409	260442.068051	37.343117
1759.629557	260863.206105	37.348135
1761.616155	261286.874304	37.353152
1763.137329	261716.531955	37.358170
1764.637166	262142.711518	37.363188
1766.967001	262563.679606	37.368205
1768.586600	263007.642346	37.373223
1770.428135	263429.013706	37.378240
1771.928449	263856.100896	37.383258
1773.505975	264298.413916	37.388276
1775.613058	264735.232160	37.393293
1776.944628	265173.592275	37.398311
1779.393950	265614.467908	37.403328
1781.683020	266040.965497	37.408346
1783.321448	266473.455623	37.413364
1785.245218	266911.969513	37.418381
1786.691241	267358.124995	37.423399
1788.710252	267792.708647	37.428416
1790.667620	268228.036538	37.433434
1791.909970	268692.707731	37.438452
1793.792999	269125.274725	37.443469
1795.185229	269582.044638	37.448487
1797.078516	270034.746418	37.453504
1798.596250	270505.181570	37.458522
1800.569407	270963.555329	37.463540
1802.310247	271422.547239	37.468557
1803.946212	271892.753427	37.473575
1805.834220	272348.872986	37.478592
1807.390568	272822.540653	37.483610
1809.960453	273278.726389	37.488628
1812.160782	273738.904020	37.493645
1814.013446	274203.298602	37.498663
1816.108279	274666.916211	37.503680
1817.157677	275126.758375	37.508698
1819.171827	275599.424487	37.513716
1821.289536	276063.183008	37.518733
1822.871186	276539.212804	37.523751
1824.592949	277001.859641	37.528768
1826.591193	277487.519766	37.533786
1828.357966	277964.705610	37.538804
1830.095145	278437.220411	37.543821
1831.681930	278922.148694	37.548839
1833.788822	279392.745901	37.553856
1835.594960	279875.551381	37.558874
1836.991801	280373.908559	37.563892
1839.244866	280841.578798	37.568909
1840.671512	281330.478101	37.573927
1842.914750	281827.829587	37.578944
1844.711179	282315.140750	37.583962
1846.279426	282799.437047	37.588980
1848.177793	283288.046100	37.593997
1849.779012	283790.664685	37.599015
1851.409690	284291.395942	37.604032
1853.643723	284790.175473	37.609050
1855.536265	285288.877854	37.614068
1857.250580	285783.947917	37.619085
1859.073919	286282.095189	37.624103
1860.915951	286777.874342	37.629120
1862.912826	287270.603900	37.634138
1865.092419	287777.520703	37.639156
1867.145694	288274.144274	37.644173
1868.862480	288774.016039	37.649191
1871.110400	289254.985782	37.654208
1873.284335	289739.315123	37.659226
1875.069591	290228.043447	37.664244
1877.022844	290699.958353	37.669261
1878.855649	291176.154169	37.674279
1880.648485	291641.637817	37.679296
1882.431815	292107.601850	37.684314
1884.251930	292577.771327	37.689332
1886.049810	293042.786502	37.694349
1887.900331	293518.732800	37.699367
1889.579805	293978.351266	37.704384
1891.345853	294457.476981	37.709402
1892.703196	294946.843771	37.714420
1894.617844	295432.031675	37.719437
1896.461144	295916.566597	37.724455
1897.879587	296425.054433	37.729472
1900.000416	296915.224538	37.734490
1901.532025	297416.424840	37.739508
1903.894143	297925.995648	37.744525
1905.656509	298427.480908	37.749543
1907.284519	298931.216768	37.754560
1909.277842	299445.553453	37.759578
1911.007997	299964.496139	37.764596
1913.202607	300481.076439	37.769613
1914.893973	301008.570526	37.774631
1916.982969	301526.122059	37.779648
1918.572710	302053.926425	37.784666
1920.497254	302590.329647	37.789684
1922.598741	303105.934557	37.794701
1924.198777	303638.316231	37.799719
1926.282919	304174.881368	37.804736
1928.341987	304718.019460	37.809754
1930.299336	305246.927160	37.814772
1932.501811	305785.436948	37.819789
1934.526693	306326.684866	37.824807
1936.443608	306865.329368	37.829824
1938.643589	307396.892643	37.834842
1940.147252	307958.612543	37.839860
1942.439711	308498.855861	37.844877
1944.352881	309037.832695	37.849895
1946.365956	309598.667265	37.854912
1948.403317	310138.196249	37.859930
1950.287081	310692.058366	37.864948
1952.463689	311237.467077	37.869965
1954.524827	311784.029731	37.874983
1956.337222	312332.147812	37.880000
1958.425977	312874.556441	37.885018
1960.419643	313424.003894	37.890036
1962.053068	313995.353105	37.895053
1964.271464	314547.366133	37.900071
1965.900696	315090.886555	37.905088
1968.219911	315650.484171	37.910106
1969.884946	316217.968391	37.915124
1971.812858	316776.928014	37.920141
1974.252003	317337.932380	37.925159
1975.789600	317907.648293	37.930176
1978.200720	318449.635199	37.935194
1979.780606	319014.356221	37.940212
1982.165621	319571.940031	37.945229
1984.230008	320123.984062	37.950247
1986.502181	320687.864399	37.955264
1988.740819	321234.182686	37.960282
1990.949187	321794.429673	37.965300
1993.049911	322332.787572	37.970317
1994.936448	322881.702521	37.975335
1996.661333	323434.619305	37.980352
1999.051451	323983.770815	37.985370
2000.875343	324536.682781	37.990388
2002.974458	325076.350191	37.995405
2005.233264	325623.394363	38.000423
2007.393362	326171.283908	38.005440
2009.511197	326703.061316	38.010458
2011.531101	327230.660660	38.015476
2013.094203	327743.177729	38.020493
2015.598954	328254.551392	38.025511
2017.208064	328774.963752	38.030528
2019.655704	329277.072750	38.035546
2021.428117	329800.287484	38.040564
2023.866394	330316.490422	38.045581
2025.774216	330831.323427	38.050599
2027.458672	331345.601027	38.055616
2029.482079	331861.011051	38.060634
2031.152140	332400.265054	38.065652
2033.153616	332925.912987	38.070669
2034.809288	333460.308875	38.075687
2036.543252	334011.909401	38.080704
2038.970132	334552.206543	38.085722
2040.490258	335097.178359	38.090740
2042.278917	335651.029093	38.095757
2043.853284	336208.177250	38.100775
2046.130078	336766.602164	38.105792
2048.084177	337322.963730	38.110810
2050.506550	337898.977280	38.115828
2053.016294	338461.119072	38.120845
2055.274793	339010.558701	38.125863
2057.221874	339578.579374	38.130880
2059.562671	340140.771969	38.135898
2061.193926	340717.193703	38.140916
2063.430574	341289.808412	38.145933
2065.854225	341863.272194	38.150951
2067.842798	342435.450475	38.155968
2069.561741	343009.588969	38.160986
2071.490930	343596.872572	38.166004
2073.550285	344166.830139	38.171021
2075.453861	344756.583222	38.176039
2077.324545	345347.751373	38.181056
2079.737993	345939.432920	38.186074
2081.590388	346540.041968	38.191092
2083.516268	347127.746925	38.196109
2085.861903	347720.777033	38.201127
2087.908902	348320.993987	38.206144
2090.208032	348917.661396	38.211162
2092.658864	349521.850396	38.216180
2094.664363	350120.063276	38.221197
2096.452440	350722.102485	38.226215
2098.339433	351321.782416	38.231232
2100.424866	351922.840010	38.236250
2102.208762	352538.993698	38.241268
2104.493101	353153.967034	38.246285
2107.367207	353773.780019	38.251303
2109.021467	354380.411047	38.256320
2110.906217	354998.706892	38.261338
2113.299674	355613.184323	38.266356
2115.183138	356238.909163	38.271373
2117.725634	356846.012571	38.276391
2119.473485	357470.643707	38.281408
2121.437355	358091.375284	38.286426
2123.902579	358705.323770	38.291444
2125.940343	359321.075802	38.296461
2128.707550	359935.738009	38.301479
2130.665282	360561.616441	38.306496
2132.760813	361179.628156	38.311514
2134.709448	361805.203260	38.316532
2136.919231	362427.911007	38.321549
2139.336461	363052.676871	38.326567
2141.313799	363675.496111	38.331584
2143.445753	364299.646543	38.336602
2145.489997	364926.281045	38.341620
2147.107814	365546.050150	38.346637
2149.386209	366163.776642	38.351655
2151.441039	366781.068735	38.356672
2153.493783	367381.825343	38.361690
2155.550634	367990.855141	38.366708
2157.788938	368591.683967	38.371725
2159.527376	369200.991058	38.376743
2161.609524	369815.805856	38.381760
2163.799538	370424.281024	38.386778
2165.604347	371052.364220	38.391796
2167.593673	371675.640957	38.396813
2170.443776	372316.200833	38.401831
2171.890284	372951.239438	38.406848
2174.464070	373562.372783	38.411866
2176.699218	374198.576631	38.416884
2178.731137	374846.375337	38.421901
2180.429098	375479.998491	38.426919
2182.680833	376130.341529	38.431936
2185.003014	376772.222038	38.436954
2187.172198	377433.363544	38.441972
2189.451685	378094.572750	38.446989
2191.898022	378738.362424	38.452007
2194.330551	379400.325726	38.457024
2196.933604	380034.509780	38.462042
2199.436077	380689.970617	38.467060
2201.747725	381345.596836	38.472077
2204.187256	382004.656428	38.477095
2206.101566	382647.394792	38.482112
2209.012404	383284.592039	38.487130
2211.752299	383923.724987	38.492148
2213.833224	384561.780099	38.497165
2216.456748	385185.907134	38.502183
2218.437042	385836.709598	38.507200
2220.657523	386477.480361	38.512218
2222.790791	387118.375074	38.517236
2225.187337	387768.404109	38.522253
2227.124750	388406.536379	38.527271
2228.652774	389061.326699	38.532288
2231.369211	389704.747680	38.537306
2233.375866	390375.455895	38.542324
2235.506941	391038.378840	38.547341
2237.851308	391691.022008	38.552359
2239.807536	392358.898793	38.557376
2242.248868	393018.073683	38.562394
2244.153288	393689.719383	38.567412
2246.348699	394366.617022	38.572429
2249.102346	395025.333704	38.577447
2251.187222	395707.071110	38.582464
2253.420030	396376.868721	38.587482
2256.001784	397049.427795	38.592500
2258.045340	397723.975580	38.597517
2260.514544	398399.348620	38.602535
2262.696898	399070.343091	38.607552
2265.068886	399739.921888	38.612570
2267.126446	400419.147874	38.617588
2269.201799	401097.895603	38.622605
2272.001347	401778.079105	38.627623
2273.921470	402465.769504	38.632640
2276.457349	403131.175136	38.637658
2279.098058	403818.104736	38.642676
2281.199693	404486.575225	38.647693
2283.696919	405162.858733	38.652711
2285.714856	405836.109986	38.657728
2288.165339	406513.827716	38.662746
2290.538133	407191.182833	38.667764
2292.464757	407869.346151	38.672781
2294.921620	408546.191412	38.677799
2297.223463	409231.034612	38.682816
2299.369223	409911.276687	38.687834
2301.587744	410591.486283	38.692852
2303.723750	411251.096302	38.697869
2306.479329	411892.680058	38.702887
2308.594978	412558.071605	38.707904
2311.097708	413196.469117	38.712922
2313.542389	413847.149396	38.717940
2315.825656	414509.065135	38.722957
2317.973475	415166.631377	38.727975
2320.048667	415820.597358	38.732992
2322.180463	416484.346986	38.738010
2324.394939	417149.023865	38.743028
2326.406983	417831.615855	38.748045
2328.200080	418514.927982	38.753063
2330.635668	419192.958752	38.758080
2332.296826	419879.635366	38.763098
2334.673194	420581.854344	38.768116
2336.548673	421295.404744	38.773133
2339.105610	422001.997299	38.778151
2341.209827	422717.080815	38.783168
2343.693819	423438.097039	38.788186
2345.791463	424156.923495	38.793204
2348.187172	424891.857137	38.798221
2350.566761	425621.002993	38.803239
2352.360562	426370.133348	38.808256
2354.900053	427109.513793	38.813274
2357.178184	427859.928289	38.818292
2359.401818	428607.694448	38.823309
2361.918978	429362.513937	38.828327
2363.962192	430136.990954	38.833344
2366.328822	430894.252274	38.838362
2369.159360	431660.762276	38.843380
2371.170608	432432.677207	38.848397
2373.688226	433205.998541	38.853415
2376.230385	433987.472218	38.858432
2378.742027	434767.706271	38.863450
2381.436537	435551.215298	38.868468
2383.769082	436338.185057	38.873485
2386.256406	437105.796300	38.878503
2388.277516	437891.335958	38.883520
2390.510877	438682.872852	38.888538
2393.156042	439473.655416	38.893556
2395.431954	440272.899420	38.898573
2398.003481	441063.879231	38.903591
2400.020366	441860.772182	38.908608
2402.485385	442664.834928	38.913626
2405.225240	443471.042351	38.918644
2407.321010	444282.719856	38.923661
2409.660069	445084.272629	38.928679
2412.344228	445908.564597	38.933696
2414.787580	446716.494226	38.938714
2417.470190	447525.865592	38.943732
2419.411556	448337.437707	38.948749
2422.169958	449136.575100	38.953767
2424.833077	449963.513873	38.958784
2427.659829	450765.597739	38.963802
2430.491004	451567.594422	38.968820
2433.357902	452360.613242	38.973837
2436.510917	453141.990911	38.978855
2439.160724	453930.177369	38.983872
2441.699539	454707.391762	38.988890
2444.548158	455481.040317	38.993908
2447.127517	456265.700439	38.998925
2449.756162	457028.109289	39.003943
2452.530911	457800.757927	39.008960
2454.544399	458564.255360	39.013978
2456.871786	459326.408253	39.018996
2459.217736	460095.690406	39.024013
2461.668458	460855.636619	39.029031
2463.907065	461614.472086	39.034048
2466.155098	462347.589315	39.039066
2468.936231	463089.824848	39.044084
2470.643014	463842.437862	39.049101
2473.262878	464579.840076	39.054119
2475.509072	465323.826726	39.059136
2477.685285	466064.865385	39.064154
2480.095374	466817.386329	39.069172
2482.398433	467577.809386	39.074189
2484.696490	468337.038267	39.079207
2487.232551	469100.381369	39.084224
2489.388312	469865.312094	39.089242
2491.779821	470640.609892	39.094260
2494.361874	471417.908828	39.099277
2496.662839	472190.726643	39.104295
2499.564527	472987.517128	39.109312
2501.853843	473772.514867	39.114330
2504.613859	474565.115192	39.119348
2506.974449	475348.966273	39.124365
2509.321105	476147.754673	39.129383
2511.965245	476963.496249	39.134400
2514.154280	477768.277843	39.139418
2516.772556	478569.170987	39.144436
2518.951642	479393.984417	39.149453
2521.108532	480211.248273	39.154471
2523.374271	481044.883054	39.159488
2525.655466	481878.874304	39.164506
2528.229660	482724.970716	39.169524
2530.682253	483578.598965	39.174541
2533.233996	484422.086995	39.179559
2535.242099	485282.493461	39.184576
2538.066554	486159.703434	39.189594
2540.465843	487024.032447	39.194612
2543.105570	487888.627727	39.199629
2545.650829	488749.813701	39.204647
2548.463731	489630.554096	39.209664
2550.932727	490510.944527	39.214682
2553.403902	491382.721097	39.219700
2556.474555	492273.541754	39.224717
2558.582949	493156.754930	39.229735
2561.434301	494049.468298	39.234752
2564.097560	494943.970342	39.239770
2566.719070	495818.032871	39.244788
2569.135233	496709.294923	39.249805
2571.585668	497602.310177	39.254823
2574.212952	498513.618299	39.259840
2577.069898	499414.766059	39.264858
2579.797394	500310.492515	39.269876
2582.248196	501213.505307	39.274893
2584.720439	502117.062455	39.279911
2587.259628	503018.589906	39.284928
2590.164272	503926.243815	39.289946
2592.807695	504833.629564	39.294964
2595.437661	505731.600944	39.299981
2598.069944	506637.163042	39.304999
2600.740287	507548.195591	39.310016
2603.335488	508447.459724	39.315034
2606.172089	509351.307050	39.320052
2608.860122	510265.380837	39.325069
2611.513421	511169.240389	39.330087
2614.315973	512072.967822	39.335104
2616.707168	512976.600349	39.340122
2619.867584	513871.504855	39.345140
2622.089340	514780.326433	39.350157
2625.020776	515691.139196	39.355175
2627.996232	516568.651181	39.360192
2631.167983	517457.790190	39.365210
2634.422642	518332.128868	39.370228
2637.232877	519203.062653	39.375245
2640.052702	520053.179671	39.380263
2642.711900	520876.880980	39.385280
2645.325029	521715.616788	39.390298
2648.024789	522541.622341	39.395316
2650.328768	523376.985858	39.400333
2653.093275	524208.958953	39.405351
2655.536450	525028.871292	39.410368
2658.050855	525860.780248	39.415386
2660.557676	526693.190809	39.420404
2663.387580	527546.497335	39.425421
2665.943648	528382.059022	39.430439
2668.531410	529226.302665	39.435456
2670.806394	530069.938086	39.440474
2673.969021	530909.563188	39.445492
2676.211896	531763.791704	39.450509
2678.445129	532623.489417	39.455527
2681.270143	533503.675343	39.460544
2683.906449	534371.027125	39.465562
2686.446176	535241.649208	39.470580
2688.974103	536117.736444	39.475597
2691.705918	537012.054800	39.480615
2694.320242	537889.011027	39.485632
2696.678877	538786.425511	39.490650
2699.992218	539686.487959	39.495668
2702.801251	540568.146954	39.500685
2705.503989	541469.030903	39.505703
2708.262735	542360.357712	39.510720
2711.149958	543268.108620	39.515738
2713.774627	544161.435385	39.520756
2716.311583	545066.300555	39.525773
2718.849916	545968.491015	39.530791
2721.733340	546872.066561	39.535808
2724.166726	547799.520964	39.540826
2726.931471	548718.528234	39.545844
2730.017929	549636.262896	39.550861
2732.961656	550559.316561	39.555879
2736.034087	551474.959518	39.560896
2738.905673	552401.946202	39.565914
2741.620939	553314.548078	39.570932
2744.614693	554227.338252	39.575949
2747.463992	555134.116793	39.580967
2749.948166	556061.434281	39.585984
2752.869386	556991.167677	39.591002
2755.885494	557909.989022	39.596020
2758.240233	558847.383938	39.601037
2761.025107	559775.017020	39.606055
2763.875554	560704.370843	39.611072
2766.379035	561633.505327	39.616090
2768.956347	562560.851654	39.621108
2771.342788	563495.117197	39.626125
2774.404407	564441.624142	39.631143
2777.549311	565377.022948	39.636160
2779.774163	566325.761316	39.641178
2782.547826	567270.480452	39.646196
2785.364364	568215.466157	39.651213
2787.954331	569169.321672	39.656231
2790.646502	570123.682769	39.661248
2793.726183	571086.864199	39.666266
2796.795852	572037.202162	39.671284
2799.073544	572985.832913	39.676301
2801.436473	573946.332025	39.681319
2804.674693	574917.471770	39.686336
2807.084680	575876.898741	39.691354
2809.603780	576849.935872	39.696372
2812.497357	577831.885223	39.701389
2815.489585	578813.682931	39.706407
2818.298929	579782.017539	39.711424
2820.876788	580749.003633	39.716442
2823.541473	581694.337070	39.721460
2826.423727	582643.006132	39.726477
2828.999342	583593.041584	39.731495
2832.096373	584529.913878	39.736512
2834.948747	585469.194060	39.741530
2838.426364	586407.345960	39.746548
2841.063868	587339.900140	39.751565
2843.555654	588292.239576	39.756583
2846.604160	589236.412043	39.761600
2849.453278	590193.126217	39.766618
2852.123723	591142.638030	39.771636
2854.649429	592094.336960	39.776653
2857.236724	593083.560763	39.781671
2860.402796	594048.374745	39.786688
2863.411168	595029.159878	39.791706
2865.965963	595996.839823	39.796724
2868.680146	596976.641906	39.801741
2871.093423	597971.380933	39.806759
2874.417939	598952.402185	39.811776
2877.256288	599955.075893	39.816794
2880.236494	600958.080751	39.821812
2883.113365	601963.800798	39.826829
2886.066225	602965.269167	39.831847
2888.548260	603960.226670	39.836864
2891.265063	604986.789717	39.841882
2894.170105	606006.036080	39.846900
2897.219014	607032.044182	39.851917
2900.082974	608065.062652	39.856935
2902.760503	609099.352845	39.861952
2905.557373	610135.614407	39.866970
2908.421990	611182.382595	39.871988
2911.548870	612221.471885	39.877005
2914.288847	613285.844679	39.882023
2917.329163	614336.746542	39.887040
2920.467602	615388.669819	39.892058
2923.412989	616435.976939	39.897076
2926.739626	617486.952471	39.902093
2928.993437	618557.470600	39.907111
2932.409763	619605.616947	39.912128
2935.346322	620677.095267	39.917146
2938.282016	621733.910281	39.922164
2941.494785	622795.201310	39.927181
2944.862891	623860.387879	39.932199
2947.699667	624919.067259	39.937216
2950.484032	625992.330419	39.942234
2953.386742	627056.593761	39.947252
2956.606052	628127.113439	39.952269
2959.223864	629197.608786	39.957287
2962.263039	630275.933434	39.962304
2965.459932	631353.415822	39.967322
2968.071455	632433.307221	39.972340
2971.080681	633502.366157	39.977357
2973.984887	634599.133830	39.982375
2977.129964	635675.589635	39.987392
2980.156688	636749.952101	39.992410
2982.800952	637824.799431	39.997428
2986.552048	638902.434502	40.002445
2989.538150	639984.540915	40.007463
2992.806881	641048.877665	40.012480
2995.935837	642134.839915	40.017498
2999.138090	643204.658332	40.022516
3001.945847	644275.508766	40.027533
3004.995895	645354.546600	40.032551
3008.154989	646420.670989	40.037568
3011.330451	647503.711365	40.042586
3014.339799	648572.392285	40.047604
3017.475214	649629.752457	40.052621
3020.220835	650689.087634	40.057639
3023.353433	651722.762780	40.062656
3026.495461	652760.291406	40.067674
3029.297037	653787.973410	40.072692
3032.331987	654818.282244	40.077709
3035.496811	655848.800538	40.082727
3038.342534	656872.798314	40.087744
3041.636486	657910.356001	40.092762
3044.465082	658947.965364	40.097780
3047.484344	659980.661115	40.102797
3050.412978	661035.675081	40.107815
3053.429686	662083.258028	40.112832
3056.568321	663141.758405	40.117850
3059.315756	664202.275918	40.122868
3062.818432	665262.150918	40.127885
3065.674619	666333.105090	40.132903
3069.113222	667397.095105	40.137920
3072.212021	668470.674446	40.142938
3075.598662	669551.064721	40.147956
3078.601950	670620.329542	40.152973
3081.797687	671695.972886	40.157991
3085.028168	672774.399951	40.163008
3087.864577	673870.042229	40.168026
3090.501777	674958.245350	40.173044
3093.540164	676075.219567	40.178061
3096.294241	677190.656214	40.183079
3099.263201	678310.220795	40.188096
3102.082097	679425.750442	40.193114
3105.176449	680565.987997	40.198132
3108.179620	681712.222953	40.203149
3111.273041	682859.772447	40.208167
3114.311372	684004.600976	40.213184
3117.321242	685171.688140	40.218202
3120.469510	686348.137304	40.223220
3124.109915	687506.390327	40.228237
3127.027531	688681.853131	40.233255
3130.618899	689858.477680	40.238272
3133.842329	691029.455256	40.243290
3136.894603	692210.722741	40.248308
3140.519437	693388.666639	40.253325
3144.058789	694569.913530	40.258343
3147.037657	695742.727220	40.263360
3150.651199	696918.483847	40.268378
3153.872352	698109.591812	40.273396
3157.344897	699282.409815	40.278413
3160.514293	700466.857131	40.283431
3164.008786	701644.759765	40.288448
3167.003079	702814.422595	40.293466
3170.353278	704004.638451	40.298484
3173.901510	705179.840856	40.303501
3177.061756	706361.493048	40.308519
3180.490711	707545.936830	40.313536
3184.079692	708733.138075	40.318554
3187.725473	709903.432166	40.323572
3190.499832	711072.011869	40.328589
3194.030174	712243.849510	40.333607
3197.186903	713408.964141	40.338624
3200.799242	714577.136216	40.343642
3203.449548	715744.642750	40.348660
3207.143156	716914.077396	40.353677
3210.273531	718077.609741	40.358695
3213.427289	719237.120739	40.363712
3216.688500	720405.404679	40.368730
3219.835679	721584.412297	40.373748
3223.285765	722741.427403	40.378765
3226.421218	723904.125826	40.383783
3229.526076	725072.460081	40.388800
3232.684310	726236.816698	40.393818
3235.322965	727405.209233	40.398836
3238.870436	728542.970963	40.403853
3241.897539	729680.248768	40.408871
3244.930539	730817.156900	40.413888
3248.255306	731942.240752	40.418906
3251.027191	733077.862956	40.423924
3254.614648	734215.495547	40.428941
3257.720416	735367.432464	40.433959
3261.032580	736513.014693	40.438976
3264.184911	737661.687974	40.443994
3267.299403	738812.202966	40.449012
3270.529834	739967.629221	40.454029
3273.637104	741121.517665	40.459047
3276.769954	742306.160050	40.464064
3280.134029	743474.861402	40.469082
3283.066351	744673.586936	40.474100
3286.674688	745856.988626	40.479117
3290.063131	747041.752912	40.484135
3293.020799	748240.620800	40.489152
3296.536159	749446.806811	40.494170
3299.395552	750663.194353	40.499188
3303.028856	751866.993217	40.504205
3306.494866	753088.759394	40.509223
3309.428838	754292.111700	40.514240
3313.169832	755535.968365	40.519258
3316.000459	756764.359541	40.524276
3320.032743	757990.781495	40.529293
3323.086300	759224.394479	40.534311
3326.379470	760464.562827	40.539328
3330.282092	761706.228897	40.544346
3333.473006	762950.136404	40.549364
3336.856431	764192.127486	40.554381
3340.189680	765444.086648	40.559399
3343.832211	766692.149920	40.564416
3347.409813	767948.365943	40.569434
3350.358116	769199.412513	40.574452
3354.085869	770451.577391	40.579469
3358.028703	771712.479108	40.584487
3360.957467	772963.820975	40.589504
3364.601697	774223.328356	40.594522
3367.926923	775491.597630	40.599540
3371.431004	776741.813225	40.604557
3374.821448	778018.347599	40.609575
3378.048509	779282.257810	40.614592
3381.798941	780544.286087	40.619610
3384.730349	781816.460412	40.624628
3388.564830	783068.282752	40.629645
3391.835596	784347.197675	40.634663
3395.184379	785616.484202	40.639680
3399.033371	786893.745535	40.644698
3402.218432	788161.643683	40.649716
3405.858460	789426.154490	40.654733
3409.337873	790709.906455	40.659751
3412.527518	791983.847512	40.664768
3416.335977	793245.451913	40.669786
3419.668828	794544.124603	40.674804
3422.840486	795806.552154	40.679821
3426.136107	797071.102604	40.684839
3429.498141	798360.579908	40.689856
3433.245381	799637.418440	40.694874
3436.241473	800918.844780	40.699892
3439.627433	802204.433742	40.704909
3443.126694	803489.990779	40.709927
3446.753506	804778.384025	40.714944
3450.651435	806055.090009	40.719962
3453.945234	807347.054173	40.724980
3457.598394	808614.577155	40.729997
3461.059893	809901.520201	40.735015
3464.464428	811162.156952	40.740020
3468.024646	812386.462486	40.745024
3471.328188	813551.424339	40.750029
3474.408133	814671.195978	40.755034
3477.609938	815731.623450	40.760039
3480.339824	816725.622540	40.765044
3483.889801	817649.711984	40.770048
3486.494232	818522.794639	40.775053
3489.242761	819314.738125	40.780058
3491.712781	820068.175834	40.785063
3493.858270	820751.984565	40.790068
3495.959570	821368.771052	40.795072
3498.031970	821941.225599	40.800077
3500.101630	822458.069692	40.805082
3502.456082	822934.644457	40.810087
3503.628501	823341.224696	40.815092
3505.325842	823705.865891	40.820096
3506.474379	824033.607049	40.825101
3507.848207	824303.809127	40.830106
3509.591314	824550.792259	40.835111
3510.485378	824748.196944	40.840116
3511.826275	824909.636414	40.845120
3513.167802	825036.642134	40.850125
3513.602240	825143.654901	40.855130
3514.961077	825206.367352	40.860135
3515.660505	825245.452038	40.865140
3516.349389	825253.222099	40.870144
3516.923275	825250.798359	40.875149
3517.541947	825209.465474	40.880154
3518.154860	825154.322798	40.885159
3518.641187	825078.094519	40.890164
3519.283451	824989.586275	40.895168
3519.411517	824893.570807	40.900173
3519.862204	824750.622840	40.905178
3520.525634	824616.294884	40.910183
3520.024690	824464.637882	40.915188
3520.423190	824300.288693	40.920192
3520.468305	824138.713980	40.925197
3520.576779	823952.611705	40.930202
3520.797650	823766.194382	40.935207
3520.663544	823573.503589	40.940212
3521.226570	823367.467047	40.945216
3521.043520	823162.610397	40.950221
3520.882427	822942.663308	40.955226
3521.268245	822730.309164	40.960231
3521.073189	822511.033015	40.965236
3521.402714	822267.146926	40.970240
3520.986251	822033.001095	40.975245
3521.091125	821805.187301	40.980250
3521.347006	821554.862101	40.985255
3520.883692	821311.354071	40.990260
3520.995067	821059.182319	40.995264
3520.649153	820816.706950	41.000269
3520.561676	820560.458258	41.005274
3520.343399	820319.500684	41.010279
3520.470684	820086.169301	41.015284
3520.375712	819823.077649	41.020288
3520.306196	819577.200864	41.025293
3519.733233	819314.551695	41.030298
3519.916370	819064.721116	41.035303
3519.499029	818814.876982	41.040308
3519.568610	818572.053980	41.045312
3519.597592	818320.465034	41.050317
3519.490508	818068.497689	41.055322
3519.594522	817817.947709	41.060327
3518.962455	817579.187827	41.065332
3519.268893	817325.567701	41.070336
3519.047544	817075.915102	41.075341
3518.573077	816828.531973	41.080346
3518.638348	816575.113748	41.085351
3518.420869	816341.305918	41.090356
3518.440234	816093.232019	41.095360
3517.901239	815850.884915	41.100365
3517.821197	815594.624866	41.105370
3517.556570	815360.787650	41.110375
3517.231980	815121.106189	41.115380
3517.476978	814895.159856	41.120384
3517.496557	814651.899555	41.125389
3517.213952	814414.717413	41.130394
3517.067425	814175.264137	41.135399
3516.448019	813956.628792	41.140404
3516.514801	813729.011866	41.145408
3516.309296	813506.203780	41.150413
3516.476268	813291.319871	41.155418
3516.289116	813067.616348	41.160423
3515.554358	812838.630708	41.165428
3516.083144	812628.540044	41.170432
3515.387137	812414.638105	41.175437
3515.679160	812186.345280	41.180442
3515.485133	811987.749006	41.185447
3514.576534	811779.803936	41.190452
3514.899245	811569.612644	41.195456
3514.809513	811370.298289	41.200461
3514.212760	811160.529492	41.205466
3514.474587	810969.043029	41.210471
3513.698168	810773.618812	41.215476
3514.077526	810583.759468	41.220480
3513.742496	810392.056332	41.225485
3513.842762	810192.675040	41.230490
3513.733558	810008.724225	41.235495
3513.216978	809828.146615	41.240500
3513.373150	809630.493774	41.245504
3512.937296	809461.397999	41.250509
3513.273915	809274.041029	41.255514
3513.290884	809093.651542	41.260519
3512.443113	808911.685655	41.265524
3512.423244	808726.367167	41.270528
3512.663850	808555.483699	41.275533
3512.930271	808375.766135	41.280538
3512.487946	808211.757716	41.285543
3512.000378	808036.049239	41.290548
3512.045105	807862.154454	41.295552
3511.423000	807699.623786	41.300557
3511.459777	807533.767404	41.305562
3511.723736	807383.427892	41.310567
3511.447513	807215.612679	41.315572
3511.549812	807056.707470	41.320576
3511.006868	806901.800816	41.325581
3510.911160	806745.015908	41.330586
3510.896350	806586.263561	41.335591
3510.714142	806442.653468	41.340596
3510.707792	806297.549381	41.345600
3510.418918	806158.534435	41.350605
3510.211581	806004.919207	41.355610
3509.973316	805859.012157	41.360615
3509.573010	805729.761012	41.365620
3509.750658	805590.465617	41.370624
3509.622116	805460.922630	41.375629
3509.579790	805327.509692	41.380634
3509.563649	805192.382435	41.385639
3509.241541	805065.691141	41.390644
3509.272136	804928.794741	41.395648
3509.022878	804806.624000	41.400653
3509.018527	804674.118413	41.405658
3509.070695	804563.946489	41.410663
3508.795999	804438.503839	41.415668
3508.648129	804319.674415	41.420672
3508.661105	804204.916116	41.425677
3508.660815	804080.009028	41.430682
3508.627594	803966.815033	41.435687
3508.308389	803848.296389	41.440692
3508.100129	803732.344340	41.445696
3508.082999	803627.144196	41.450701
3508.281282	803507.708817	41.455706
3508.044790	803389.705511	41.460711
3507.755980	803292.496344	41.465716
3507.858102	803178.486475	41.470720
3507.579967	803081.760432	41.475725
3507.625239	802978.394274	41.480730
3507.728565	802876.823031	41.485735
3507.266785	802775.338518	41.490740
3507.149284	802664.770003	41.495744
3507.364455	802572.693065	41.500749
3506.980296	802478.414680	41.505754
3506.957410	802378.612241	41.510759
3507.074210	802292.012847	41.515764
3507.084420	802183.661150	41.520768
3507.061728	802093.078720	41.525773
3506.613945	802003.781668	41.530778
3506.613288	801911.924225	41.535783
3506.631872	801827.871986	41.540788
3506.448804	801732.282156	41.545792
3506.151301	801667.313191	41.550797
3506.237094	801582.466264	41.555802
3506.421901	801496.968184	41.560807
3506.302645	801416.983515	41.565812
3505.944630	801329.810812	41.570816
3506.114836	801259.541587	41.575821
3505.920799	801174.537766	41.580826
3505.871083	801101.323508	41.585831
3505.504088	801032.112075	41.590836
3505.657488	800951.786105	41.595840
3505.711737	800885.485030	41.600845
3505.915425	800807.639051	41.605850
3505.891873	800724.018328	41.610855
3505.543851	800647.428285	41.615860
3505.858073	800586.062970	41.620864
3505.573412	800528.598601	41.625869
3505.493899	800450.353201	41.630874
3505.356027	800375.289308	41.635879
3505.028612	800304.648068	41.640884
3505.269949	800237.090547	41.645888
3505.532489	800169.919580	41.650893
3505.402835	800089.773579	41.655898
3505.469875	800023.217518	41.660903
3505.264978	799961.683296	41.665908
3505.151505	799898.083582	41.670912
3505.228235	799836.601790	41.675917
3505.179539	799765.715773	41.680922
3505.444029	799688.530330	41.685927
3505.091029	799623.647058	41.690932
3505.341615	799562.916702	41.695936
3505.134152	799500.401946	41.700941
3504.997862	799433.529799	41.705946
3504.962955	799368.252440	41.710951
3504.830037	799309.483948	41.715956
3504.703741	799243.584843	41.720960
3504.864433	799200.199434	41.725965
3504.445185	799133.319580	41.730970
3504.865783	799076.659789	41.735975
3504.447779	799023.011610	41.740980
3504.527902	798956.491339	41.745984
3504.633175	798899.928124	41.750989
3504.175042	798854.928024	41.755994
3503.881334	798792.859388	41.760999
3504.098549	798751.708428	41.766004
3504.530739	798696.313147	41.771008
3504.179795	798650.904204	41.776013
3504.301790	798608.058041	41.781018
3504.378159	798547.296544	41.786023
3503.923471	798495.407753	41.791028
3503.934404	798451.112870	41.796032
3504.148862	798399.753564	41.801037
3503.468848	798352.245201	41.806042
3503.977965	798306.308703	41.811047
3503.845603	798264.769769	41.816052
3504.060602	798211.455426	41.821056
3503.856676	798168.071257	41.826061
3503.862636	798131.100539	41.831066
3504.024057	798081.016772	41.836071
3503.252882	798037.671564	41.841076
3503.727026	797988.319605	41.846080
3503.679744	797955.654001	41.851085
3503.678747	797909.892115	41.856090
3503.216129	797872.993172	41.861095
3503.206046	797838.416423	41.866100
3503.543806	797792.844953	41.871104
3503.262211	797767.687551	41.876109
3503.425840	797732.399318	41.881114
3503.703508	797693.478848	41.886119
3503.435582	797650.589623	41.891124
3503.369475	797603.175151	41.896128
3503.214170	797567.349778	41.901133
3503.421542	797531.907091	41.906138
3503.244580	797493.984492	41.911143
3503.407518	797454.836314	41.916148
3503.267257	797418.617027	41.921152
3503.267727	797384.768851	41.926157
3502.613927	797350.338968	41.931162
3503.248123	797322.350290	41.936167
3502.762458	797300.983930	41.941172
3502.787567	797255.408717	41.946176
3502.710335	797241.597987	41.951181
3502.880021	797209.041234	41.956186
3502.806958	797181.650956	41.961191
3502.604988	797157.064869	41.966196
3502.858121	797127.913803	41.971200
3502.950525	797105.821447	41.976205
3502.456018	797073.318997	41.981210
3502.827536	797046.689024	41.986215
3502.820425	797023.635031	41.991220
3502.752532	796988.525482	41.996224
3502.420755	796952.821992	42.001229
3502.827902	796929.165596	42.006234
3502.594053	796897.598448	42.011239
3502.402968	796875.696165	42.016244
3502.831628	796846.565245	42.021248
3502.659557	796833.794262	42.026253
3502.597494	796789.645976	42.031258
3502.895394	796773.137836	42.036263
3502.563802	796747.544657	42.041268
3502.825844	796724.154438	42.046272
3502.503490	796707.156913	42.051277
3502.299380	796677.244883	42.056282
3502.423358	796645.278632	42.061287
3502.640005	796629.710955	42.066292
3502.716451	796613.334726	42.071296
3502.588827	796585.901613	42.076301
3502.420906	796565.704382	42.081306
3502.767061	796527.792056	42.086311
3502.426510	796504.397547	42.091316
3502.494446	796493.688915	42.096320
3502.283052	796451.271415	42.101325
3502.136603	796437.909445	42.106330
3502.592508	796423.280878	42.111335
3502.036893	796411.692578	42.116340
3502.217132	796379.862778	42.121344
3502.302788	796359.039055	42.126349
3502.623497	796341.451537	42.131354
3502.337442	796309.498881	42.136359
3502.267030	796295.147707	42.141364
3502.181776	796272.054411	42.146368
3501.909135	796255.194483	42.151373
3502.440608	796227.412566	42.156378
3502.462272	796204.448871	42.161383
3502.259966	796193.635433	42.166388
3502.465455	796177.677604	42.171392
3502.296909	796163.097217	42.176397
3502.077816	796137.826011	42.181402
3502.257133	796113.078659	42.186407
3502.197901	796099.946623	42.191412
3502.323108	796070.761963	42.196416
3502.039687	796063.234139	42.201421
3501.633671	796050.253918	42.206426
3502.088313	796028.540953	42.211431
3501.913135	796023.731946	42.216436
3502.236483	796000.866933	42.221440
3501.921598	795985.527367	42.226445
3501.989861	795978.530711	42.231450
3501.961244	795952.203080	42.236455
3501.949414	795947.319628	42.241460
3501.990330	795927.771720	42.246464
3502.076921	795910.317346	42.251469
3501.978601	795898.510076	42.256474
3502.050919	795869.430490	42.261479
3502.116553	795872.058463	42.266484
3502.040614	795842.562243	42.271488
3502.068771	795829.318289	42.276493
3501.969288	795810.231670	42.281498
3502.036558	795795.613595	42.286503
3502.199699	795783.130128	42.291508
3502.194930	795764.126277	42.296512
3501.995651	795741.146630	42.301517
3501.957253	795723.027315	42.306522
3502.078087	795709.573208	42.311527
3501.356138	795692.684344	42.316532
3501.720659	795682.660852	42.321536
3501.967933	795678.322965	42.326541
3501.939503	795654.241472	42.331546
3501.842671	795647.319125	42.336551
3501.793090	795635.845752	42.341556
3501.721959	795619.441235	42.346560
3502.085659	795601.454150	42.351565
3501.750404	795584.064845	42.356570
3501.727355	795568.434389	42.361575
3501.685449	795575.671828	42.366580
3501.569133	795548.330280	42.371584
3501.794227	795545.559194	42.376589
3501.549533	795543.545543	42.381594
3501.985199	795516.117573	42.386599
3501.514731	795515.018636	42.391604
3501.852327	795503.826506	42.396608
3501.926820	795491.356338	42.401613
3502.123829	795486.244465	42.406618
3501.960326	795465.945408	42.411623
3501.790951	795446.038067	42.416628
3502.011788	795439.554416	42.421632
3501.827174	795420.431103	42.426637
3501.503292	795404.749565	42.431642
3501.860032	795406.794782	42.436647
3501.734663	795387.955260	42.441652
3501.796714	795367.180912	42.446656
3501.630854	795362.076808	42.451661
3502.068918	795349.940402	42.456666
3501.848217	795340.985038	42.461671
3501.693678	795324.592816	42.466676
3501.837260	795299.701384	42.471680
3501.354040	795310.135068	42.476685
3501.446055	795288.818340	42.481690
3502.042156	795275.875350	42.486695
3501.508654	795275.958838	42.491700
3501.851637	795264.472303	42.496704
3501.754858	795249.585494	42.501709
3501.852587	795252.648433	42.506714
3502.159010	795233.936403	42.511719
3501.831601	795220.942232	42.516724
3502.111084	795198.472138	42.521728
3502.000232	795176.795881	42.526733
3501.832583	795170.030675	42.531738
3501.831247	795154.640130	42.536743
3501.672166	795146.456623	42.541748
3501.714551	795130.081987	42.546752
3502.107752	795105.492814	42.551757
3501.757311	795101.883166	42.556762
3502.066403	795097.046629	42.561767
3501.629289	795076.398246	42.566772
3501.760067	795064.016183	42.571776
3501.972876	795056.995942	42.576781
3501.576261	795047.921092	42.581786
3501.498666	795041.825724	42.586791
3501.976062	795034.861820	42.591796
3501.681449	795002.562051	42.596800
3501.618349	795006.774051	42.601805
3501.552505	794991.148900	42.606810
3501.582526	794965.443305	42.611815
3501.643166	794966.704309	42.616820
3501.591952	794957.624199	42.621824
3501.837448	794955.093983	42.626829
3501.763960	794939.909656	42.631834
3501.631219	794934.067115	42.636839
3501.494090	794920.407398	42.641844
3501.673793	794910.607062	42.646848
3501.338789	794904.942698	42.651853
3501.361425	794902.740471	42.656858
3501.615528	794874.263228	42.661863
3501.194008	794869.589598	42.666868
3501.518371	794875.255836	42.671872
3501.610480	794875.583560	42.676877
3501.741356	794863.005653	42.681882
3501.639776	794854.226445	42.686887
3501.568410	794849.644649	42.691892
3501.823966	794835.727920	42.696896
3501.676032	794824.463942	42.701901
3501.873825	794823.895626	42.706906
3502.042422	794798.754061	42.711911
3501.903466	794786.999989	42.716916
3501.892536	794768.091921	42.721920
3501.907352	794761.444354	42.726925
3502.017519	794752.729633	42.731930
3501.848500	794728.617832	42.736935
3501.848502	794712.297636	42.741940
3501.901240	794704.911135	42.746944
3501.920558	794680.525399	42.751949
3501.726555	794668.828582	42.756954
3501.968396	794657.014748	42.761959
3501.531271	794646.870668	42.766964
3501.610903	794642.460577	42.771968
3501.661901	794626.327648	42.776973
3501.371472	794611.860563	42.781978
3501.941205	794611.478407	42.786983
3501.505145	794601.822730	42.791988
3501.827079	794580.907524	42.796993
3501.718702	794573.497196	42.801997
3501.362722	794572.233599	42.807002
3501.513891	794549.634739	42.812007
3501.517810	794550.806962	42.817012
3501.660513	794534.659471	42.822017
3501.314900	794537.987510	42.827021
3501.535145	794520.459657	42.832026
3501.799563	794511.525043	42.837031
3501.500790	794510.252491	42.842036
3501.669020	794499.818092	42.847041
3501.810010	794480.983173	42.852045
3501.402680	794483.734508	42.857050
3501.678437	794479.195918	42.862055
3501.710540	794468.538424	42.867060
3501.589435	794451.650127	42.872065
3501.510157	794441.058864	42.877069
3501.603848	794453.944715	42.882074
3502.005205	794434.873501	42.887079
3502.075752	794433.787527	42.892084
3501.620559	794408.253317	42.897089
3501.469946	794386.629512	42.902093
3501.342259	794385.525653	42.907098
3501.458102	794390.785121	42.912103
3501.197094	794378.609601	42.917108
3501.900276	794360.223972	42.922113
3501.419432	794364.159628	42.927117
3501.392679	794360.303501	42.932122
3501.496205	794343.037747	42.937127
3501.185158	794327.889129	42.942132
3501.580104	794310.284537	42.947137
3501.323196	794311.741907	42.952141
3501.313528	794320.001890	42.957146
3501.381037	794306.650959	42.962151
3501.294587	794293.812731	42.967156
3501.285950	794285.164826	42.972161
3501.514719	794292.507975	42.977165
3501.620536	794299.479405	42.982170
3501.440047	794287.828657	42.987175
3501.278083	794265.326629	42.992180
3501.471818	794259.774513	42.997185
3501.409755	794245.319780	43.002189
3500.991533	794248.024048	43.007194
3501.632709	794241.864438	43.012199
3501.493727	794231.037834	43.017204
3501.502673	794223.901969	43.022209
3501.505053	794228.153102	43.027213
3501.878232	794219.152221	43.032218
3501.915439	794199.159908	43.037223
3501.653409	794201.253374	43.042228
3501.478308	794182.320405	43.047233
3501.635423	794159.181726	43.052237
3501.236800	794155.872282	43.057242
3501.418831	794159.753304	43.062247
3501.615989	794153.467553	43.067252
3501.247812	794137.301207	43.072257
3501.313140	794130.058691	43.077261
3501.500241	794127.292949	43.082266
3501.547258	794132.221313	43.087271
3501.473591	794120.016023	43.092276
3501.549856	794107.494066	43.097281
3501.732472	794097.105643	43.102285
3501.114919	794108.099781	43.107290
3501.244249	794100.358550	43.112295
3500.968018	794084.568642	43.117300
3501.250695	794064.439808	43.122305
3500.905771	794065.520046	43.127309
3501.087188	794071.502542	43.132314
3501.371069	794074.292598	43.137319
3501.744884	794077.117462	43.142324
3501.329107	794060.958368	43.147329
3501.202542	794051.497830	43.152333
3501.416098	794052.588504	43.157338
3501.471205	794047.448823	43.162343
3500.847464	794045.493954	43.167348
3501.295163	794038.533641	43.172353
3501.615436	794048.012964	43.177357
3501.484999	794028.828227	43.182362
3501.581361	794020.652240	43.187367
3501.373973	794020.880223	43.192372
3501.347474	794013.896275	43.197377
3501.645307	793995.768465	43.202381
3501.131470	793986.221767	43.207386
3501.309284	793988.930703	43.212391
3501.368637	793997.131436	43.217396
3501.457281	793989.543039	43.222401
3501.929566	793973.586984	43.227405
3501.762508	793957.779704	43.232410
3501.521366	793960.016587	43.237415
3501.636283	793946.168821	43.242420
3501.378977	793930.082367	43.247425
3501.214216	793936.754400	43.252429
3501.128308	793935.057504	43.257434
3501.621388	793924.669145	43.262439
3501.274446	793913.190354	43.267444
3501.343633	793899.105291	43.272449
3501.163369	793892.242988	43.277453
3500.955285	793897.358015	43.282458
3501.169174	793893.415124	43.287463
3501.213466	793900.298861	43.292468
3501.223373	793902.594258	43.297473
3501.477221	793878.119992	43.302477
3501.251948	793873.072874	43.307482
3501.220902	793862.082176	43.312487
3501.167155	793876.409432	43.317492
3501.599851	793872.383455	43.322497
3501.164582	793879.488789	43.327501
3501.359584	793852.189198	43.332506
3501.541399	793848.642252	43.337511
3501.349707	793848.916656	43.342516
3501.294279	793844.771488	43.347521
3501.329802	793848.235772	43.352525
3501.185378	793819.474144	43.357530
3501.551678	793820.736460	43.362535
3501.103349	793823.396736	43.367540
3501.376435	793818.955849	43.372545
3501.753982	793823.050858	43.377549
3501.409141	793794.271580	43.382554
3501.690956	793784.600205	43.387559
3501.393316	793792.417171	43.392564
3501.451008	793776.867538	43.397569
3501.606465	793756.171201	43.402573
3501.174722	793754.479450	43.407578
3501.390622	793757.866714	43.412583
3501.365725	793764.272707	43.417588
3501.428331	793745.008088	43.422593
3501.593337	793747.132682	43.427597
3501.497439	793737.471413	43.432602
3501.432373	793735.135891	43.437607
3501.208801	793729.306466	43.442612
3501.472113	793724.329467	43.447617
3501.427547	793701.953756	43.452621
3500.996473	793696.303352	43.457626
3501.349722	793690.481464	43.462631
3501.422875	793699.902184	43.467636
3501.419441	793694.820249	43.472641
3501.221633	793675.889359	43.477645
3501.168387	793665.634865	43.482650
3501.142554	793662.560118	43.487655
3501.434920	793666.717413	43.492660
3500.935295	793665.427217	43.497665
3501.211398	793665.433017	43.502669
3501.220685	793671.589402	43.507674
3501.252401	793660.832909	43.512679
3501.000906	793647.970340	43.517684
3501.190557	793644.470929	43.522689
3501.434277	793629.771548	43.527693
3501.728737	793645.462145	43.532698
3501.614386	793646.506406	43.537703
3501.563236	793626.819380	43.542708
3501.763091	793619.506398	43.547713
3501.736045	793616.236333	43.552717
3501.657573	793590.933258	43.557722
3501.423949	793580.755699	43.562727
3501.404721	793575.822755	43.567732
3501.505858	793575.562677	43.572737
3501.528458	793549.852669	43.577741
3501.623542	793545.977014	43.582746
3501.466499	793545.073087	43.587751
3501.554058	793549.262474	43.592756
3501.661481	793534.681930	43.597761
3501.749128	793521.228503	43.602765
3501.531157	793516.424327	43.607770
3501.796452	793499.619779	43.612775
3501.657534	793498.273161	43.617780
3501.287610	793489.094211	43.622785
3501.652700	793489.281591	43.627789
3501.454436	793475.628403	43.632794
3501.679162	793460.491760	43.637799
3501.681119	793467.333699	43.642804
3501.672580	793445.391330	43.647809
3501.684370	793436.934599	43.652813
3501.699348	793425.593863	43.657818
3501.832545	793415.358704	43.662823
3501.652601	793400.871656	43.667828
3501.473820	793393.666485	43.672833
3501.454104	793382.722082	43.677837
3501.184220	793369.959586	43.682842
3501.650988	793356.299935	43.687847
3501.454270	793357.894723	43.692852
3501.376574	793359.861891	43.697857
3501.463910	793358.382129	43.702861
3501.334225	793333.330429	43.707866
3501.643861	793318.668920	43.712871
3501.422108	793319.681147	43.717876
3501.291361	793319.457307	43.722881
3501.642972	793303.811731	43.727885
3501.684232	793290.560577	43.732890
3501.324455	793286.413757	43.737895
3501.155590	793294.308931	43.742900
3501.434044	793274.764816	43.747905
3501.465363	793266.549182	43.752909
3501.514372	793264.000162	43.757914
3501.411238	793262.696775	43.762919
3500.975748	793264.133415	43.767924
3500.999276	793263.641086	43.772929
3501.314418	793262.418935	43.777933
3501.284595	793248.983312	43.782938
3501.828667	793239.661132	43.787943
3501.345161	793241.936144	43.792948
3501.407430	793235.572852	43.797953
3501.275894	793212.475947	43.802957
3501.467482	793203.355440	43.807962
3501.659338	793213.784669	43.812967
3501.275543	793209.641555	43.817972
3501.360978	793204.105476	43.822977
3501.943034	793190.427459	43.827981
3501.729890	793172.474999	43.832986
3501.668578	793165.251212	43.837991
3501.481054	793153.697286	43.842996
3501.453462	793134.053969	43.848001
3501.529304	793131.109703	43.853005
3501.012846	793135.540402	43.858010
3501.446962	793127.799252	43.863015
3501.195762	793114.349084	43.868020
3501.468030	793108.050590	43.873025
3501.426839	793105.124607	43.878029
3501.058357	793113.148954	43.883034
3501.405378	793111.921793	43.888039
3501.481792	793092.115466	43.893044
3501.884038	793075.630550	43.898049
3501.730836	793079.271371	43.903053
3501.134313	793064.799823	43.908058
3501.698149	793050.879986	43.913063
3501.602325	793041.071049	43.918068
3501.529554	793042.793164	43.923073
3501.379069	793033.139386	43.928077
3501.358616	793018.431055	43.933082
3501.393750	793008.699349	43.938087
3501.420540	793018.274927	43.943092
3501.549228	793013.562815	43.948097
3501.736215	793002.292208	43.953101
3501.421234	792981.911344	43.958106
3501.530410	792985.657829	43.963111
3501.414199	792991.296835	43.968116
3501.756842	792966.512026	43.973121
3501.687799	792957.285292	43.978125
3501.404564	792959.871226	43.983130
3501.546661	792944.062039	43.988135
3501.380847	792933.628487	43.993140
3501.404466	792921.601256	43.998145
3501.598192	792924.796916	44.003149
3501.171076	792925.205910	44.008154
3501.441111	792905.906394	44.013159
3501.418282	792890.709381	44.018164
3501.303169	792888.039240	44.023169
3501.558124	792885.800017	44.028173
3501.872101	792885.164503	44.033178
3501.768099	792869.002591	44.038183
3501.251838	792866.053011	44.043188
3501.571762	792850.900079	44.048193
3501.437996	792834.009576	44.053197
3501.179683	792821.684093	44.058202
3501.734206	792820.277810	44.063207
3501.088624	792813.975885	44.068212
3501.265292	792811.113468	44.073217
3501.343256	792811.785654	44.078221
3501.190589	792802.131876	44.083226
3501.417283	792792.663168	44.088231
3501.110195	792783.571155	44.093236
3501.515475	792786.342792	44.098241
3501.223339	792788.392530	44.103245
3501.294333	792777.677323	44.108250
3501.256657	792762.482333	44.113255
3501.234081	792764.245552	44.118260
3501.211809	792762.782790	44.123265
3501.496140	792768.163863	44.128269
3501.217702	792759.409482	44.133274
3501.217604	792751.149234	44.138279
3501.174206	792735.173029	44.143284
3501.239745	792730.128440	44.148289
3501.401195	792735.870895	44.153293
3501.139595	792733.614614	44.158298
3501.362072	792736.072703	44.163303
3501.158917	792740.063665	44.168308
3501.297263	792728.262534	44.173313
3501.394442	792695.743462	44.178317
3501.099165	792694.469997	44.183322
3501.264304	792686.721499	44.188327
3501.390699	792691.834054	44.193332
3501.322320	792693.506696	44.198337
3501.211937	792677.882970	44.203341
3501.079874	792666.319512	44.208346
3501.303829	792669.315059	44.213351
3501.028317	792676.543348	44.218356
3500.909353	792671.967462	44.223361
3501.364632	792688.270642	44.228365
3500.992564	792675.522760	44.233370
3501.192300	792673.683125	44.238375
3501.236605	792677.048900	44.243380
3501.088816	792660.257898	44.248385
3501.211352	792653.004805	44.253389
3500.953736	792655.880124	44.258394
3501.089834	792641.586381	44.263399
3500.887188	792652.420328	44.268404
3501.349610	792652.690280	44.273409
3501.437091	792657.906702	44.278413
3501.016249	792654.502201	44.283418
3501.210426	792647.189024	44.288423
3500.980444	792636.716151	44.293428
3500.959808	792618.878713	44.298433
3501.027911	792622.680705	44.303437
3500.781506	792624.967739	44.308442
3500.712445	792627.129292	44.313447
3500.857333	792624.076247	44.318452
3500.878566	792627.299018	44.323457
3500.879600	792628.129886	44.328461
3500.854987	792642.699683	44.333466
3501.238767	792633.450583	44.338471
3500.719874	792647.120062	44.343476
3501.076894	792651.219024	44.348481
3501.328010	792637.444957	44.353485
3501.096400	792640.707247	44.358490
3501.393525	792637.092744	44.363495
3501.085308	792638.118590	44.368500
3501.456171	792631.999744	44.373505
3501.478826	792611.418307	44.378509
3501.389939	792608.695073	44.383514
3501.501039	792610.339679	44.388519
3501.364071	792612.951761	44.393524
3501.609086	792602.648975	44.398529
3501.719308	792585.964086	44.403533
3501.267157	792585.790462	44.408538
3501.478551	792580.722958	44.413543
3501.305990	792577.670637	44.418548
3501.287747	792555.922320	44.423553
3501.496713	792551.343966	44.428557
3500.993035	792557.288312	44.433562
3501.289135	792548.737110	44.438567
3501.598369	792570.684538	44.443572
3501.730354	792547.153056	44.448577
3501.487552	792532.625030	44.453581
3501.452071	792520.899579	44.458586
3501.278299	792510.662114	44.463591
3501.103448	792497.345379	44.468596
3501.199071	792485.403850	44.473601
3501.204424	792479.342000	44.478605
3501.490179	792493.228173	44.483610
3501.349550	792495.303197	44.488615
3501.333282	792503.664265	44.493620
3501.187154	792477.438744	44.498625
3501.224983	792460.569333	44.503629
3501.167920	792465.808504	44.508634
3501.276741	792460.659182	44.513639
3501.192311	792459.499350	44.518644
3501.270785	792460.024853	44.523649
3501.521434	792461.158881	44.528653
3500.779270	792448.908331	44.533658
3501.264641	792423.365958	44.538663
3501.484974	792428.366274	44.543668
3501.501705	792435.353623	44.548673
3501.370085	792435.129887	44.553677
3501.395508	792440.453944	44.558682
3501.516026	792414.528649	44.563687
3501.484329	792403.095678	44.568692
3501.092243	792404.183549	44.573697
3501.512723	792409.739157	44.578701
3501.115411	792394.208489	44.583706
3501.572093	792378.886448	44.588711
3501.117430	792375.878132	44.593716
3501.105763	792373.289370	44.598721
3501.127627	792370.011036	44.603725
3500.875729	792381.537458	44.608730
3501.532215	792380.555073	44.613735
3500.923871	792381.872277	44.618740
3501.162163	792371.912344	44.623745
3501.404624	792350.122590	44.628749
3500.976270	792357.375122	44.633754
3501.212795	792346.584454	44.638759
3501.252456	792346.138416	44.643764
3501.561587	792349.951770	44.648769
3501.410340	792349.682218	44.653773
3501.245094	792330.253531	44.658778
3501.401980	792317.177857	44.663783
3500.824835	792325.089139	44.668788
3500.828405	792315.605742	44.673793
3501.319742	792316.555528	44.678797
3501.005238	792318.804431	44.683802
3501.038345	792319.239276	44.688807
3501.118719	792317.711488	44.693812
3501.513995	792316.036711	44.698817
3501.397265	792304.372454	44.703821
3501.440669	792295.567139	44.708826
3501.359558	792295.628789	44.713831
3501.460626	792300.745610	44.718836
3501.467804	792286.666772	44.723841
3501.198455	792267.596342	44.728845
3501.232862	792270.670585	44.733850
3501.274682	792257.172846	44.738855
3501.539567	792259.526723	44.743860
3501.141368	792260.615573	44.748865
3501.014299	792243.429209	44.753869
3501.199637	792245.062303	44.758874
3501.827746	792229.224300	44.763879
3501.219870	792234.843050	44.768884
3501.263289	792234.738589	44.773889
3501.368199	792224.310467	44.778893
3501.140228	792208.068538	44.783898
3501.571616	792203.161882	44.788903
3501.335091	792210.140178	44.793908
3501.431553	792207.876622	44.798913
3501.685133	792197.034160	44.803917
3501.400089	792184.027304	44.808922
3501.223391	792164.795445	44.813927
3501.237108	792160.345106	44.818932
3501.240263	792164.792988	44.823937
3501.188091	792159.375303	44.828941
3501.288149	792162.146041	44.833946
3501.378355	792139.206213	44.838951
3501.347719	792136.131499	44.843956
3501.304048	792134.671942	44.848961
3501.561293	792136.587117	44.853965
3501.201177	792139.234270	44.858970
3501.596734	792114.291325	44.863975
3501.469628	792100.673023	44.868980
3501.267734	792104.761937	44.873985
3501.503002	792112.204295	44.878989
3501.548966	792100.025415	44.883994
3501.590677	792083.252193	44.888999
3501.274792	792071.667536	44.894004
3501.213531	792064.344760	44.899009
3501.205241	792073.340608	44.904013
3501.130452	792076.480895	44.909018
3501.501215	792051.346055	44.914023
3501.429289	792047.886690	44.919028
3501.330305	792046.142461	44.924033
3501.433183	792040.651558	44.929037
3501.213895	792044.596579	44.934042
3501.393608	792019.051533	44.939047
3501.445105	792019.385756	44.944052
3501.432046	792006.482680	44.949057
3501.394860	792009.519353	44.954061
3501.031055	792012.558200	44.959066
3501.548494	792001.478636	44.964071
3501.341020	791986.161738	44.969076
3501.540582	791985.544029	44.974081
3501.315327	791976.095913	44.979085
3501.014582	791984.013277	44.984090
3501.419436	791964.054432	44.989095
3501.493273	791959.007954	44.994100
3500.981025	791947.160470	44.999105
3501.308470	791944.909599	45.004109
3500.642412	791952.493037	45.009114
3501.126258	791951.830885	45.014119
3501.231361	791961.102464	45.019124
3501.369686	791961.569768	45.024129
3501.481307	791947.327223	45.029133
3501.291738	791938.117893	45.034138
3501.432468	791931.154463	45.039143
3501.255335	791931.133359	45.044148
3501.111282	791927.831856	45.049153
3501.338157	791928.480856	45.054157
3501.002593	791911.717288	45.059162
3501.356607	791895.628027	45.064167
3501.264527	791896.669080	45.069172
3501.213321	791892.815319	45.074177
3501.234466	791893.594252	45.079181
3501.545745	791900.096168	45.084186
3501.562872	791879.219992	45.089191
3501.559527	791863.479823	45.094196
3501.189248	791859.382614	45.099201
3501.416588	791865.213304	45.104205
3501.327898	791855.108166	45.109210
3501.365833	791836.281751	45.114215
3501.552296	791828.675563	45.119220
3501.628512	791823.237531	45.124225
3501.692085	791818.632512	45.129229
3501.427518	791811.830083	45.134234
3501.254008	791796.702972	45.139239
3501.220750	791787.517879	45.144244
3501.730524	791789.149256	45.149249
3501.407026	791770.085841	45.154253
3501.289929	791753.043289	45.159258
3501.583438	791749.673295	45.164263
3501.607857	791750.891701	45.169268
3501.507663	791741.961434	45.174273
3501.428106	791735.423316	45.179277
3501.175117	791727.299082	45.184282
3501.498445	791716.689354	45.189287
3501.327122	791713.783091	45.194292
3501.536468	791704.951043	45.199297
3501.256593	791685.098391	45.204301
3501.687964	791697.692459	45.209306
3501.683104	791684.983011	45.214311
3501.662334	791670.907221	45.219316
3501.417032	791650.902403	45.224321
3501.399789	791647.238733	45.229325
3501.079772	791644.795658	45.234330
3501.337813	791634.635978	45.239335
3501.297923	791634.348987	45.244340
3501.199303	791613.538946	45.249345
3501.280752	791609.859827	45.254349
3501.132452	791613.305144	45.259354
3501.306983	791611.224725	45.264359
3501.220340	791617.984672	45.269364
3501.377183	791616.346996	45.274369
3500.972153	791589.180666	45.279373
3501.186387	791583.671974	45.284378
3501.338404	791575.093146	45.289383
3501.539579	791584.350240	45.294388
3501.144955	791589.642878	45.299393
3501.604675	791585.709067	45.304397
3501.330447	791567.663978	45.309402
3501.140368	791552.490007	45.314407
3501.335808	791557.494883	45.319412
3501.368898	791556.218744	45.324417
3501.609749	791549.874788	45.329421
3501.185182	791537.328438	45.334426
3501.160534	791522.275196	45.339431
3501.586422	791528.368472	45.344436
3501.633197	791519.806024	45.349441
3501.920033	791510.570505	45.354445
3501.076930	791502.831563	45.359450
3501.247161	791489.263284	45.364455
3501.650632	791482.551631	45.369460
3501.534933	791487.165213	45.374465
3501.637247	791470.576500	45.379469
3501.232948	791468.146533	45.384474
3501.495659	791448.648333	45.389479
3501.269904	791449.808128	45.394484
3501.217001	791451.967540	45.399489
3501.332477	791431.758992	45.404493
3501.246802	791419.990531	45.409498
3501.286393	791418.811125	45.414503
3501.541089	791414.469273	45.419508
3501.357135	791421.977952	45.424513
3501.525760	791390.663438	45.429517
3501.244433	791389.436417	45.434522
3501.328476	791392.796641	45.439527
3501.492446	791392.624435	45.444532
3501.129069	791404.414434	45.449537
3501.304007	791391.040768	45.454541
3501.153058	791370.091472	45.459546
3501.373998	791361.648256	45.464551
3501.353367	791356.029424	45.469556
3501.259632	791358.635244	45.474561
3501.539908	791358.151526	45.479565
3501.216238	791346.420137	45.484570
3501.088257	791333.680367	45.489575
3501.330421	791326.456000	45.494580
3501.143261	791322.036494	45.499585
3501.152465	791317.879621	45.504589
3501.223369	791324.810796	45.509594
3501.208477	791315.573283	45.514599
3501.286930	791321.378844	45.519604
3501.108360	791310.260258	45.524609
3501.182937	791301.986512	45.529613
3501.050116	791305.038461	45.534618
3501.667239	791294.577682	45.539623
3501.358523	791299.221568	45.544628
3501.067896	791313.102571	45.549633
3501.366636	791299.269369	45.554637
3501.162286	791279.452570	45.559642
3501.313541	791267.157908	45.564647
3501.227530	791267.415889	45.569652
3501.438899	791262.396265	45.574657
3501.588389	791261.492985	45.579661
3500.910187	791247.079057	45.584666
3501.350697	791235.276899	45.589671
3501.646869	791233.568459	45.594676
3501.154813	791232.863241	45.599681
3501.201472	791235.887165	45.604685
3501.354923	791233.174364	45.609690
3501.281030	791210.941395	45.614695
3501.221775	791205.719587	45.619700
3501.146891	791208.175851	45.624705
3501.313256	791203.212107	45.629709
3501.080617	791209.408625	45.634714
3501.216533	791205.085204	45.639719
3501.299671	791210.254570	45.644724
3501.252379	791191.586298	45.649729
3501.069489	791168.147986	45.654733
3500.932465	791166.507247	45.659738
3501.254390	791161.323596	45.664743
3501.466751	791176.152942	45.669748
3501.163925	791176.004812	45.674753
3500.969869	791167.039546	45.679757
3500.826149	791171.804398	45.684762
3500.967172	791164.253436	45.689767
3500.876557	791169.352216	45.694772
3500.425494	791177.489604	45.699777
3501.230193	791174.381636	45.704781
3501.106784	791177.823289	45.709786
3501.110497	791156.702465	45.714791
3501.138718	791146.822409	45.719796
3501.110357	791151.422573	45.724801
3501.172888	791140.168229	45.729805
3500.935633	791141.623213	45.734810
3500.853525	791148.920723	45.739815
3501.228132	791146.662212	45.744820
3501.027950	791128.115439	45.749825
3501.103361	791072.760082	45.754829
3500.834290	790975.411908	45.759834
3500.881135	790815.626659	45.764839
3500.754104	790625.452903	45.769844
3500.439487	790374.672766	45.774849
3500.237439	790075.163468	45.779853
3499.808087	789736.849364	45.784858
3499.595705	789330.508731	45.789863
3499.056856	788896.806506	45.794868
3498.713080	788401.320923	45.799873
3498.074891	787861.528116	45.804877
3497.156419	787277.121556	45.809882
3496.641549	786649.645965	45.814887
3496.204314	785976.938408	45.819892
3495.154894	785260.610011	45.824897
3494.510738	784490.895677	45.829901
3493.579890	783692.896113	45.834906
3492.936182	782828.868257	45.839911
3492.306084	781929.770872	45.844916
3490.963425	780987.869256	45.849921
3490.109847	779995.220215	45.854925
3488.976938	778962.207432	45.859930
3487.794920	777874.619392	45.864935
3486.986773	776747.503636	45.869940
3485.776447	775578.610059	45.874945
3484.907471	774361.870814	45.879949
3483.280520	773101.550537	45.884954
3482.054076	771799.945160	45.889959
3480.613448	770459.580010	45.894964
3479.345930	769073.407442	45.899969
3478.041204	767641.188248	45.904973
3476.132756	766187.028121	45.909978
3474.922631	764674.832050	45.914983
3473.458398	763127.785783	45.919988
3471.503715	761547.966615	45.924993
3470.122756	759918.291668	45.929997
3467.878225	758269.558310	45.935002
3466.420970	756564.691892	45.940007
3464.720746	754840.284243	45.945012
3462.633003	753065.028860	45.950017
3460.788627	751266.722338	45.955021
3458.934658	749423.057634	45.960026
3457.119758	747542.358333	45.965031
3455.393653	745635.170756	45.970036
3453.067360	743700.057937	45.975041
3451.434210	741717.101768	45.980045
3449.151345	739711.890596	45.985050
3447.151099	737661.846496	45.990055
3444.963528	735576.223888	45.995060
3442.874418	733471.859098	46.000065
3440.819832	731323.848233	46.005069
3438.363381	729157.330659	46.010074
3435.912934	726951.853404	46.015079
3433.854467	724718.479029	46.020084
3431.122520	722463.425204	46.025089
3429.214638	720172.615357	46.030093
3426.509147	717858.772188	46.035098
3423.999681	715520.488175	46.040103
3421.326538	713150.931270	46.045108
3418.681738	710751.876452	46.050113
3416.238017	708326.983241	46.055117
3413.181231	705887.193924	46.060122
3410.837693	703427.145228	46.065127
3408.048695	700932.104090	46.070132
3405.470187	698422.935700	46.075137
3402.790181	695878.628957	46.080141
3399.879814	693335.247687	46.085146
3396.912049	690753.218521	46.090151
3394.292164	688143.205866	46.095156
3391.263900	685525.393243	46.100161
3388.399603	682876.520849	46.105165
3385.247585	680209.836355	46.110170
3382.573083	677529.875410	46.115175
3379.450930	674823.864868	46.120180
3376.451305	672104.214690	46.125185
3373.447643	669363.136572	46.130189
3370.059676	666614.245465	46.135194
3367.461734	663842.141972	46.140199
3364.400389	661034.572403	46.145204
3361.413196	658236.799945	46.150209
3358.433565	655407.493554	46.155213
3355.043223	652571.786650	46.160218
3351.770660	649697.028512	46.165223
3348.880616	646830.422489	46.170228
3345.695341	643943.735657	46.175233
3342.624729	641032.057126	46.180237
3339.352784	638108.832991	46.185242
3336.050362	635166.501633	46.190247
3332.839330	632217.806185	46.195252
3329.719929	629247.426479	46.200257
3326.632364	626254.560669	46.205261
3323.265952	623262.166232	46.210266
3319.883617	620252.976141	46.215271
3316.607446	617225.314842	46.220276
3312.860784	614202.906250	46.225281
3310.093455	611142.736941	46.230285
3306.518201	608078.870252	46.235290
3303.310061	605006.674674	46.240295
3299.973541	601929.781709	46.245300
3296.345689	598837.458282	46.250305
3292.873121	595731.331785	46.255309
3289.526636	592615.710749	46.260314
3286.281842	589495.759857	46.265319
3283.024979	586366.139180	46.270324
3279.137519	583226.444392	46.275329
3276.307862	580062.571188	46.280333
3272.293333	576895.825503	46.285338
3268.763978	573716.469569	46.290343
3265.566089	570523.170710	46.295348
3261.336467	567329.593709	46.300353
3258.048101	564131.973870	46.305357
3254.752647	560941.767054	46.310362
3251.423848	557723.420040	46.315367
3247.642740	554511.863021	46.320372
3243.864079	551286.076698	46.325377
3240.742485	548057.672670	46.330381
3236.791283	544825.230825	46.335386
3233.221718	541575.185333	46.340391
3229.495777	538318.183804	46.345396
3225.422797	535057.229871	46.350401
3222.016680	531801.838266	46.355405
3218.308902	528562.447696	46.360410
3214.901483	525298.787241	46.365415
3210.822923	522020.422361	46.370420
3207.007314	518749.027910	46.375425
3203.737947	515476.710154	46.380429
3200.108040	512194.392465	46.385434
3196.524623	508912.604609	46.390439
3192.572783	505634.902017	46.395444
3188.597210	502347.417787	46.400449
3185.430832	499043.715864	46.405453
3181.272230	495757.645556	46.410458
3177.796379	492461.549576	46.415463
3174.379272	489147.549077	46.420468
3170.288440	485853.994676	46.425473
3166.603900	482542.897919	46.430477
3162.735720	479237.696239	46.435482
3159.084416	475930.354132	46.440487
3155.219656	472613.616559	46.445492
3151.368914	469309.194810	46.450497
3147.920317	466002.378216	46.455501
3144.011905	462692.702564	46.460506
3140.337136	459369.087971	46.465511
3136.203882	456061.804624	46.470516
3132.299576	452749.100774	46.475521
3128.739320	449432.483508	46.480525
3124.672735	446122.523495	46.485530
3121.215899	442801.688915	46.490535
3117.337689	439504.941977	46.495540
3113.619342	436191.027198	46.500545
3109.896539	432875.829957	46.505549
3106.048539	429568.246339	46.510554
3102.267360	426259.693557	46.515559
3098.359841	422941.896799	46.520564
3094.816326	419630.653928	46.525569
3090.946652	416321.318557	46.530573
3087.380977	413013.954415	46.535578
3083.280304	409702.920110	46.540583
3079.410036	406392.973852	46.545588
3075.588317	403088.974139	46.550593
3071.940108	399788.325040	46.555597
3068.206326	396489.250434	46.560602
3064.059837	393186.785765	46.565607
3060.187387	389887.786648	46.570612
3056.414582	386592.671641	46.575617
3052.473656	383298.801714	46.580621
3049.023364	380012.279530	46.585626
3044.869903	376721.696861	46.590631
3041.195385	373432.210361	46.595636
3037.207249	370152.006238	46.600641
3033.718319	366868.876012	46.605645
3029.754016	363602.494327	46.610650
3025.973325	360320.041637	46.615655
3022.046509	357046.276291	46.620660
3017.757729	353775.855063	46.625665
3014.329919	350505.825669	46.630669
3010.280762	347240.776041	46.635674
3006.874308	343990.332705	46.640679
3002.848112	340726.913628	46.645684
2998.888032	337486.501377	46.650689
2995.185321	334227.804581	46.655693
2991.320875	330985.559339	46.660698
2987.262200	327736.865274	46.665703
2983.074352	324498.737341	46.670708
2979.071737	321262.105990	46.675713
2975.106744	318039.291629	46.680717
2971.314720	314811.125084	46.685722
2967.096978	311597.402188	46.690727
2963.482225	308393.825303	46.695732
2959.554927	305205.510324	46.700737
2955.656696	302009.814515	46.705741
2951.825314	298823.409824	46.710746
2948.165753	295639.976936	46.715751
2944.280280	292476.997687	46.720756
2939.829538	289297.930086	46.725761
2936.219541	286125.802373	46.730765
2932.266524	282973.436038	46.735770
2928.035858	279816.288034	46.740775
2924.454938	276675.531126	46.745780
2920.488126	273544.614975	46.750785
2916.912934	270407.690688	46.755789
2912.676612	267279.520440	46.760794
2908.433530	264166.045310	46.765799
2904.741286	261047.375034	46.770804
2900.252671	257949.676861	46.775809
2896.321121	254860.396866	46.780813
2892.370808	251766.288284	46.785818
2888.569992	248690.099547	46.790823
2884.300694	245621.238973	46.795828
2880.236730	242568.242309	46.800833
2876.660822	239519.714054	46.805837
2872.734940	236479.001408	46.810842
2868.670637	233453.591694	46.815847
2864.708235	230424.709264	46.820852
2860.219481	227406.849123	46.825857
2856.455467	224401.834477	46.830861
2852.471231	221413.971213	46.835866
2848.503356	218431.054624	46.840871
2844.465103	215450.888924	46.845876
2840.285179	212495.190898	46.850881
2836.705233	209537.286837	46.855885
2832.393080	206603.980056	46.860890
2828.290109	203666.528462	46.865895
2824.573725	200741.387961	46.870900
2820.017716	197828.857709	46.875905
2816.055938	194922.021196	46.880909
2812.028351	192043.600790	46.885914
2807.863249	189152.689354	46.890919
2804.081046	186282.239580	46.895924
2799.737618	183433.803798	46.900929
2795.222222	180596.630538	46.905933
2791.200454	177767.081059	46.910938
2787.303938	174952.448772	46.915943
2783.474592	172155.865606	46.920948
2779.244485	169376.937196	46.925953
2775.404422	166584.916754	46.930957
2771.153838	163809.250460	46.935962
2766.918777	160982.835948	46.940967
2762.663737	158243.606511	46.945972
2758.616689	155528.496048	46.950977
2754.664932	152816.028968	46.955981
2750.663092	150118.805581	46.960986
2746.443925	147429.754032	46.965991
2742.463317	144754.914311	46.970996
2738.139796	142106.518344	46.976001
2733.980705	139451.979676	46.981005
2729.845168	136822.737469	46.986010
2726.067018	134215.928254	46.991015
2721.494792	131605.489434	46.996020
2717.369252	129024.851275	47.001025
2713.202510	126450.418252	47.006029
2709.123625	123881.282953	47.011034
2705.080496	121342.561503	47.016039
2700.997900	118816.994332	47.021044
2696.468167	116310.139962	47.026049
2692.714404	113795.601260	47.031053
2688.449998	111312.109323	47.036058
2684.513857	108851.775160	47.041063
2680.229882	106391.452141	47.046068
2676.189428	103948.250296	47.051073
2672.251109	101519.090249	47.056077
2668.025115	99109.536777	47.061082
2663.809917	96702.118573	47.066087
2659.449182	94326.307123	47.071092
2655.742836	91958.021036	47.076097
2651.480368	89601.631438	47.081101
2647.503767	87264.439486	47.086106
2643.914474	84938.958092	47.091111
2639.546897	82618.967676	47.096116
2635.262736	80326.982592	47.101121
2631.243411	78034.533644	47.106125
2627.215837	75766.646988	47.111130
2623.200973	73511.798496	47.116135
2619.298900	71266.099355	47.121140
2614.915492	69034.080443	47.126145
2610.625767	66816.450943	47.131149
2606.734689	64615.497936	47.136154
2602.560594	62435.458028	47.141159
2598.438185	60264.320079	47.146164
2594.242448	58108.100367	47.151169
2590.348162	55964.879787	47.156173
2586.347823	53844.700765	47.161178
2582.310742	51736.592989	47.166183
2578.131993	49640.292893	47.171188
2573.733530	47553.021063	47.176193
2569.607249	45492.952865	47.181197
2565.298275	43442.550269	47.186202
2561.091250	41400.347930	47.191207
2556.740137	39382.653477	47.196212
2552.607944	37393.576998	47.201217
2548.471390	35399.575381	47.206221
2543.967275	33442.118622	47.211226
2540.045611	31504.095829	47.216231
2536.021544	29577.524067	47.221236
2531.552545	27673.874482	47.226241
2527.335968	25779.518253	47.231245
2522.973940	23910.704281	47.236250
2518.796649	22057.188743	47.241255
2514.325597	20222.926879	47.246260
2509.840928	18421.374924	47.251265
2505.546990	16621.377939	47.256269
2501.050432	14870.601453	47.261274
2496.518000	13121.111050	47.266279
2491.982337	11402.651455	47.271284
2487.088298	9719.971856	47.276289
2481.954979	8048.413558	47.281293
2477.189290	6428.131453	47.286298
2472.429235	4837.219683	47.291303
2467.255427	3274.050643	47.296308
2460.526913	1774.984790	47.301313
2450.073871	436.259732	47.306317
2400.896527	200.847508	47.311322
2355.003424	251.011359	47.316327
2332.046081	253.359632	47.321332
2326.873495	267.374903	47.326337
2333.442404	252.736388	47.331341
2344.056871	245.906143	47.336346
2353.260986	242.647075	47.341351
2359.343793	240.436328	47.346356
2361.166579	249.484630	47.351361
2360.516539	251.073428	47.356365
2357.808851	246.615289	47.361370
2354.342134	233.455070	47.366375
2350.907251	237.827122	47.371380
2347.434009	245.745532	47.376385
2344.253693	241.162016	47.381389
2341.291042	234.082971	47.386394
2338.277978	236.421117	47.391399
2335.627592	223.285066	47.396404
2332.915607	232.821334	47.401409
2329.968134	232.121412	47.406413
2326.990236	231.217437	47.411418
2323.591431	232.815480	47.416423
2320.742345	223.766581	47.421428
2317.218795	235.726776	47.426433
2314.213509	235.326978	47.431437
2311.204486	235.547881	47.436442
2308.033519	239.790068	47.441447
2304.696632	229.137481	47.446452
2300.953430	230.495173	47.451457
2297.563086	231.171218	47.456461
2294.435870	238.051544	47.461466
2291.238251	238.871452	47.466471
2288.000648	223.951123	47.471476
2284.652805	228.467766	47.476481
2281.539485	233.510886	47.481485
2278.265819	233.792184	47.486490
2274.356262	237.612078	47.491495
2271.543290	228.737882	47.496500
2267.711134	234.915393	47.501505
2264.738311	229.932436	47.506509
2261.336676	228.765734	47.511514
2257.996106	232.142260	47.516519
2254.533343	230.352354	47.521524
2250.896992	233.879566	47.526529
2247.818502	231.789087	47.531533
2244.250479	233.679391	47.536538
2240.844815	225.189012	47.541543
2237.382775	230.745458	47.546548
2233.784913	228.521101	47.551553
2230.789338	229.249301	47.556557
2227.795202	230.651177	47.561562
2224.142253	233.181217	47.566567
2219.890665	228.369872	47.571572
2216.398320	233.677958	47.576577
2213.404860	220.266589	47.581581
2210.463029	227.614649	47.586586
2206.915837	227.660345	47.591591
2202.983196	230.433474	47.596596
2199.570903	230.888350	47.601601
2196.162287	225.397779	47.606605
2192.978139	219.122260	47.611610
2189.594990	227.039260	47.616615
2186.257723	220.423856	47.621620
2182.149235	224.259083	47.626625
2179.176002	224.651597	47.631629
2175.515823	219.481978	47.636634
2171.926658	223.185332	47.641639
2168.760749	226.648453	47.646644
2165.106273	229.928583	47.651649
2161.886339	225.101385	47.656653
2158.392594	227.748909	47.661658
2154.774896	229.745093	47.666663
2150.928002	222.810794	47.671668
2147.657925	225.559370	47.676673
2144.376059	228.594538	47.681677
2141.031074	222.375839	47.686682
2137.340783	220.697505	47.691687
2133.919303	213.478349	47.696692
2130.448084	224.408468	47.701697
2127.127779	214.753141	47.706701
2123.670185	224.213106	47.711706
2119.876026	227.723918	47.716711
2116.880754	212.863834	47.721716
2112.856937	218.100073	47.726721
2109.723215	220.023708	47.731725
2106.640127	214.760657	47.736730
2102.723483	217.838208	47.741735
2099.472835	222.627601	47.746740
2095.553657	224.107810	47.751745
2092.261543	213.736222	47.756749
2089.242770	220.675552	47.761754
2085.667779	221.469141	47.766759
2082.297558	224.271371	47.771764
2078.151008	228.134737	47.776769
2074.764042	217.895057	47.781773
2071.297000	227.603293	47.786778
2067.683439	227.760662	47.791783
2064.559221	215.910608	47.796788
2061.169271	223.765425	47.801793
2057.744879	216.606866	47.806797
2054.028620	212.173755	47.811802
2050.471948	218.222795	47.816807
2047.251033	210.617941	47.821812
2043.246563	220.508352	47.826817
2040.185225	216.985197	47.831821
2036.882805	223.323499	47.836826
2033.013038	217.060401	47.841831
2029.923826	215.892347	47.846836
2026.086665	221.741669	47.851841
2022.517771	211.609576	47.856845
2019.056687	210.683217	47.861850
2015.378592	223.069460	47.866855
2012.029487	213.152924	47.871860
2008.909932	217.004312	47.876865
2005.635036	212.131987	47.881869
2002.010086	212.639183	47.886874
1998.296601	221.073002	47.891879
1994.942231	220.500121	47.896884
1991.215839	211.705682	47.901889
1987.662261	213.682392	47.906893
1984.166072	207.057133	47.911898
1980.752711	217.563765	47.916903
1977.297471	212.811421	47.921908
1973.711832	209.689879	47.926913
1970.337969	210.793728	47.931917
1967.076322	211.788267	47.936922
1963.242716	213.679086	47.941927
1960.057026	205.812483	47.946932
1956.174727	213.152727	47.951937
1952.764283	203.584349	47.956941
1949.305628	210.908924	47.961946
1945.622911	203.376374	47.966951
1942.542250	204.114802	47.971956
1939.177569	215.553485	47.976961
1935.946830	202.005359	47.981965
1932.529065	203.840608	47.986970
1928.488066	205.887282	47.991975
1925.406267	207.239678	47.996980
1921.525498	213.231898	48.001985
1917.882277	211.634866	48.006989
1914.420107	210.259446	48.011994
1910.767693	209.119447	48.016999
1907.314897	208.704369	48.022004
1903.784323	214.239988	48.027009
1900.877845	205.352088	48.032013
1897.038326	205.905552	48.037018
1893.444514	214.080218	48.042023
1889.946877	203.101784	48.047028
1886.492957	209.081003	48.052033
1882.942958	207.437757	48.057037
1879.766049	211.272842	48.062042
1875.949809	210.604593	48.067047
1872.860584	204.988235	48.072052
1868.887117	215.743897	48.077057
1865.463220	211.692226	48.082061
1862.091777	206.673706	48.087066
1858.373248	212.827223	48.092071
1855.397404	208.091656	48.097076
1851.344293	209.213250	48.102081
1848.181637	209.727250	48.107085
1844.812959	203.195991	48.112090
1840.990886	212.007519	48.117095
1837.754958	197.159914	48.122100
1833.592316	205.635587	48.127105
1830.127495	206.291793	48.132109
1826.922461	200.500581	48.137114
1823.430990	206.232587	48.142119
1820.514785	200.864425	48.147124
1816.489249	213.067793	48.152129
1813.004951	202.640976	48.157133
1809.905424	205.647700	48.162138
1806.167028	206.678930	48.167143
1802.517280	199.223542	48.172148
1798.804939	210.688185	48.177153
1795.714347	206.625509	48.182157
1792.354408	207.663957	48.187162
1788.491196	203.361519	48.192167
1785.235851	198.271076	48.197172
1781.611099	199.939443	48.202177
1777.901313	206.170710	48.207181
1774.623244	204.912064	48.212186
1771.314057	199.396606	48.217191
1768.041630	194.846695	48.222196
1764.383587	191.046849	48.227201
1760.648742	194.820580	48.232205
1757.063658	200.165447	48.237210
1752.785237	203.429451	48.242215
1750.041003	197.252933	48.247220
1746.514340	190.325651	48.252225
1743.087673	199.284134	48.257229
1740.261498	193.376715	48.262234
1736.049204	201.705161	48.267239
1732.891321	194.865704	48.272244
1729.085531	195.954966	48.277249
1725.521619	196.357789	48.282253
1722.185487	196.142820	48.287258
1718.785076	203.107152	48.292263
1715.350123	196.260443	48.297268
1711.647539	187.851562	48.302273
1708.248848	190.854511	48.307277
1704.947347	188.938316	48.312282
1700.916662	191.252384	48.317287
1697.520811	185.468941	48.322292
1693.981582	191.189470	48.327297
1690.452634	195.921279	48.332301
1687.127552	198.938026	48.337306
1683.244080	191.943223	48.342311
1680.144698	185.550225	48.347316
1676.425397	189.353188	48.352321
1672.828325	199.961403	48.357325
1669.618669	187.074507	48.362330
1666.170902	197.542293	48.367335
1663.299727	193.394703	48.372340
1659.245213	203.058927	48.377345
1655.809924	190.640793	48.382349
1652.239486	189.320377	48.387354
1648.669499	194.567997	48.392359
1645.197358	190.947915	48.397364
1641.304998	200.273546	48.402369
1637.909592	193.822485	48.407373
1635.025604	190.154648	48.412378
1630.975464	193.038112	48.417383
1627.787585	193.211268	48.422388
1623.706541	198.551539	48.427393
1620.307063	198.659736	48.432397
1616.556073	196.253923	48.437402
1613.399410	193.204586	48.442407
1610.419562	192.677621	48.447412
1607.196827	190.600431	48.452417
1603.662318	188.663791	48.457421
1600.048211	194.813694	48.462426
1595.902899	191.950739	48.467431
1592.377223	190.449328	48.472436
1588.990537	194.950088	48.477441
1585.641912	187.817833	48.482445
1582.352067	199.760577	48.487450
1578.457176	202.249594	48.492455
1574.938137	188.499980	48.497460
1571.411203	191.526207	48.502465
1567.895330	184.644769	48.507469
1564.731941	184.004173	48.512474
1561.359274	190.318781	48.517479
1557.866130	193.184696	48.522484
1554.170188	193.105195	48.527489
1550.513507	192.393113	48.532493
1547.031828	185.224751	48.537498
1543.516069	188.448558	48.542503
1540.030696	185.880977	48.547508
1536.314264	192.432901	48.552513
1533.442517	189.576284	48.557517
1529.819457	189.738490	48.562522
1526.160826	186.445043	48.567527
1522.821574	185.930065	48.572532
1518.875738	189.759047	48.577537
1515.577721	191.230826	48.582541
1511.806210	182.272827	48.587546
1508.850913	183.513790	48.592551
1505.442485	189.321472	48.597556
1501.215980	190.688644	48.602561
1498.270267	189.476147	48.607565
1494.832003	186.638612	48.612570
1490.966366	194.814799	48.617575
1487.729326	187.937205	48.622580
1483.866843	195.685785	48.627585
1480.536745	186.437238	48.632589
1477.369011	186.803446	48.637594
1473.356782	187.409410	48.642599
1469.861741	183.232984	48.647604
1466.547420	190.813506	48.652609
1462.851813	191.610365	48.657613
1459.570674	185.299682	48.662618
1456.214909	189.745020	48.667623
1452.419462	184.204557	48.672628
1448.955825	186.151544	48.677633
1445.582713	182.028810	48.682637
1442.317850	191.211981	48.687642
1438.581965	189.677089	48.692647
1434.849123	184.351466	48.697652
1431.283732	184.030108	48.702657
1428.094422	191.505649	48.707661
1424.770179	187.897302	48.712666
1421.267476	183.431022	48.717671
1417.929683	189.876256	48.722676
1414.014040	180.940864	48.727681
1410.515553	183.950034	48.732685
1406.893290	183.824252	48.737690
1403.105899	186.442041	48.742695
1400.218816	179.993768	48.747700
1396.623229	179.541106	48.752705
1393.097347	187.430015	48.757709
1389.636444	188.500215	48.762714
1386.087823	192.899831	48.767719
1382.485314	185.636553	48.772724
1378.997099	195.936731	48.777729
1375.446406	184.995313	48.782733
1372.061640	183.291588	48.787738
1368.386047	188.464074	48.792743
1365.128040	181.640433	48.797748
1361.880456	183.854190	48.802753
1357.957874	181.877148	48.807757
1354.592252	174.399630	48.812762
1350.934751	181.562492	48.817767
1347.473655	177.969271	48.822772
1343.664817	185.544976	48.827777
1340.242884	187.589876	48.832781
1337.338615	177.154743	48.837786
1333.165042	184.006083	48.842791
1329.774251	175.039194	48.847796
1326.576217	181.541668	48.852801
1322.914444	183.576662	48.857805
1319.564140	180.706440	48.862810
1316.040256	178.189266	48.867815
1312.732064	178.479434	48.872820
1309.644627	179.196964	48.877825
1305.452373	187.003549	48.882829
1301.885179	182.711930	48.887834
1298.139060	192.100192	48.892839
1294.854569	180.082573	48.897844
1291.463813	183.536835	48.902849
1287.691654	172.905386	48.907853
1285.033912	179.990855	48.912858
1280.604961	180.744392	48.917863
1277.356785	176.472448	48.922868
1273.835845	186.780935	48.927873
1270.213864	178.853191	48.932877
1267.189392	177.007678	48.937882
1263.634327	182.582115	48.942887
1260.191808	168.953567	48.947892
1256.776509	176.920113	48.952897
1252.553338	170.655748	48.957901
1249.323966	169.788299	48.962906
1245.696049	179.778173	48.967911
1242.439555	171.691986	48.972916
1238.855507	176.571764	48.977921
1235.412097	171.602724	48.982925
1232.216741	165.354639	48.987930
1228.496584	169.800138	48.992935
1224.752464	178.314890	48.997940
1221.353506	178.075123	49.002945
1217.873298	174.839291	49.007949
1214.783347	175.263009	49.012954
1210.944176	173.845620	49.017959
1207.407208	167.182781	49.022964
1204.006547	173.087408	49.027969
1200.123168	171.657963	49.032973
1196.837991	177.117399	49.037978
1193.306105	178.894819	49.042983
1189.638800	175.220044	49.047988
1186.532814	185.716697	49.052993
1182.931466	172.404118	49.057997
1179.164997	174.256233	49.063002
1175.784985	176.459142	49.068007
1172.441378	176.245529	49.073012
1168.927925	176.067999	49.078017
1165.295503	172.495344	49.083021
1161.885985	170.792407	49.088026
1157.948990	173.003427	49.093031
1155.166312	168.620687	49.098036
1151.631767	174.577929	49.103041
1147.919023	172.751625	49.108045
1144.810417	168.207940	49.113050
1141.156463	174.506589	49.118055
1137.197254	161.164645	49.123060
1133.505332	172.110547	49.128065
1130.151118	173.812714	49.133069
1126.925254	172.837188	49.138074
1123.092126	173.003958	49.143079
1119.967133	168.804539	49.148084
1116.709902	172.693537	49.153089
1112.734174	172.224565	49.158093
1109.375215	163.847589	49.163098
1106.128699	178.112205	49.168103
1102.238820	173.171989	49.173108
1098.539667	176.146238	49.178113
1094.961574	172.903633	49.183117
1092.112449	171.688798	49.188122
1088.163666	166.137706	49.193127
1084.902061	172.903300	49.198132
1081.305224	172.719874	49.203137
1077.591431	179.448701	49.208141
1074.062452	172.240490	49.213146
1070.683249	177.192657	49.218151
1067.692777	179.233371	49.223156
1063.964957	171.420371	49.228161
1060.017366	175.360527	49.233165
1056.625233	161.825434	49.238170
1052.840478	169.609432	49.243175
1049.876836	168.074012	49.248180
1046.006776	181.249844	49.253185
1042.805471	175.208408	49.258189
1039.332452	165.454080	49.263194
1035.695567	174.600680	49.268199
1032.326048	162.761021	49.273204
1028.410299	168.885556	49.278209
1025.415831	174.138172	49.283213
1022.178511	164.948071	49.288218
1018.419602	175.758961	49.293223
1014.596401	168.805656	49.298228
1011.277546	167.069597	49.303233
1007.652602	166.700772	49.308237
1004.538233	161.629687	49.313242
1000.820015	165.815529	49.318247
996.949393	166.488101	49.323252
993.576681	162.764122	49.328257
989.961178	162.675404	49.333261
987.019886	162.228018	49.338266
982.890772	169.939405	49.343271
979.869094	163.332026	49.348276
976.258927	167.709769	49.353281
972.994354	170.242689	49.358285
969.548458	160.341777	49.363290
965.883981	170.331124	49.368295
961.997471	167.940472	49.373300
958.239357	164.760913	49.378305
954.771824	170.644448	49.383309
951.834332	161.473872	49.388314
948.463778	164.852310	49.393319
944.321460	157.053653	49.398324
941.107452	160.274701	49.403329
937.310501	158.028228	49.408333
934.563056	164.203982	49.413338
930.663176	170.816457	49.418343
927.611799	165.317914	49.423348
923.770292	166.561769	49.428353
920.277619	167.931341	49.433357
916.832165	165.848139	49.438362
913.004161	169.352003	49.443367
909.711849	165.254793	49.448372
906.108970	171.785969	49.453377
902.504540	165.187610	49.458381
899.384642	162.809825	49.463386
895.461919	170.400340	49.468391
892.228347	166.518568	49.473396
888.812993	169.356704	49.478401
885.115878	164.895776	49.483405
881.866982	164.439642	49.488410
878.258653	173.401481	49.493415
874.724005	165.153357	49.498420
871.066000	179.004725	49.503425
867.465683	172.329803	49.508429
864.216557	154.823989	49.513434
860.038842	174.378810	49.518439
856.760422	167.916083	49.523444
853.683381	166.490235	49.528449
849.877031	163.536579	49.533453
846.761554	161.275181	49.538458
842.988863	166.171973	49.543463
839.596703	172.084872	49.548468
836.064774	174.403434	49.553473
832.719171	164.917154	49.558477
829.438578	161.115538	49.563482
825.716630	166.763701	49.568487
822.162617	163.381396	49.573492
818.448204	164.561097	49.578497
815.077034	162.896579	49.583501
811.816935	169.475351	49.588506
807.747745	171.719865	49.593511
804.446648	165.415739	49.598516
800.725178	167.596313	49.603521
797.549718	170.631035	49.608525
794.149728	159.745400	49.613530
790.541119	167.264615	49.618535
787.305625	159.861878	49.623540
783.436040	166.703781	49.628545
779.947580	162.393726	49.633549
776.438072	160.709757	49.638554
772.772684	169.250286	49.643559
769.649689	166.790773	49.648564
765.947515	160.938619	49.653569
762.662205	166.186229	49.658573
759.165054	160.621516	49.663578
755.254664	159.373662	49.668583
751.806000	162.944733	49.673588
748.294905	158.543322	49.678593
744.978207	166.481917	49.683597
741.676365	157.295716	49.688602
737.704530	172.490255	49.693607
734.660928	157.768099	49.698612
731.345388	168.576080	49.703617
727.466261	166.127426	49.708621
724.362727	158.862239	49.713626
720.666364	167.167186	49.718631
717.153870	158.918831	49.723636
713.256118	162.870296	49.728641
709.845272	164.964294	49.733645
706.447611	161.453146	49.738650
702.780272	160.983511	49.743655
699.444095	154.548882	49.748660
696.190684	165.299684	49.753665
692.387626	161.994399	49.758669
688.915166	156.191730	49.763674
685.100880	158.200220	49.768679
681.803639	154.277882	49.773684
678.226345	159.583899	49.778689
675.083931	163.875837	49.783693
671.463576	167.802859	49.788698
667.911636	170.298625	49.793703
664.436369	156.343304	49.798708
661.112658	158.094639	49.803713
657.420173	160.349823	49.808717
653.891511	154.853368	49.813722
650.331646	165.655339	49.818727
647.018338	156.749390	49.823732
643.273909	161.926569	49.828737
639.888803	159.454370	49.833741
636.965737	159.307966	49.838746
632.970178	156.254323	49.843751
629.273432	152.169945	49.848756
625.575199	168.612492	49.853761
622.503194	157.166200	49.858765
618.787822	155.679053	49.863770
615.230401	163.500359	49.868775
611.673425	155.939235	49.873780
608.587794	160.997429	49.878785
604.906237	158.403992	49.883789
601.112530	162.687223	49.888794
597.729676	167.472429	49.893799
594.357787	160.761858	49.898804
590.837072	156.668909	49.903809
587.537421	158.770845	49.908813
584.072627	147.765750	49.913818
580.262968	164.333325	49.918823
577.088205	148.730111	49.923828
573.430011	154.536057	49.928833
569.881584	159.970469	49.933837
566.425482	145.955256	49.938842
562.157896	157.627403	49.943847
559.131761	152.704024	49.948852
555.750518	149.471945	49.953857
552.267798	148.998767	49.958861
549.143286	148.779537	49.963866
545.695116	156.381269	49.968871
542.240027	157.093352	49.973876
538.554088	157.784644	49.978881
534.845179	161.143447	49.983885
531.231025	147.697178	49.988890
527.519675	151.271502	49.993895
524.069115	150.654091	49.998900
520.530325	153.416772	50.003905
517.083647	156.240958	50.008909
514.166461	147.538788	50.013914
509.906768	147.187321	50.018919
506.815354	146.576940	50.023924
503.377073	142.970999	50.028929
499.710498	156.023357	50.033933
496.253241	155.808806	50.038938
492.880968	158.709933	50.043943
489.145658	149.984052	50.048948
485.653325	158.630444	50.053953
482.193096	157.334348	50.058957
478.723084	156.387803	50.063962
475.330376	164.667415	50.068967
471.854912	153.385628	50.073972
468.347742	152.359485	50.078977
464.649612	158.931035	50.083981
461.135264	152.970510	50.088986
457.482362	157.219085	50.093991
454.004103	159.247802	50.098996
451.119048	150.670339	50.104001
447.438601	156.033721	50.109005
443.895339	152.023462	50.114010
440.331090	152.952000	50.119015
436.708094	155.300790	50.124020
433.027453	159.873263	50.129025
429.493195	159.639161	50.134029
426.041181	147.328660	50.139034
422.222417	154.270299	50.144039
419.224034	146.906513	50.149044
415.718548	148.259294	50.154049
412.310213	145.078974	50.159053
409.092926	138.556249	50.164058
405.205692	141.999980	50.169063
401.978291	152.072892	50.174068
397.930796	150.963733	50.179073
394.491853	152.923037	50.184077
391.193384	147.431772	50.189082
387.451717	149.495446	50.194087
384.461976	146.312844	50.199092
380.696738	142.951160	50.204097
377.242522	141.059374	50.209101
373.849533	152.547133	50.214106
370.113803	150.484308	50.219111
366.414120	147.760937	50.224116
363.303871	148.757595	50.229121
359.082765	152.712394	50.234125
356.231491	149.580878	50.239130
352.842875	154.980840	50.244135
349.301570	144.680714	50.249140
345.803142	152.670035	50.254145
342.087373	154.913170	50.259149
338.605602	146.805717	50.264154
335.107067	154.317327	50.269159
331.417128	152.965526	50.274164
327.692325	144.196953	50.279169
324.569600	145.619526	50.284173
321.720314	154.975163	50.289178
317.529024	153.686084	50.294183
314.097111	154.071917	50.299188
309.988015	156.158379	50.304193
306.763843	156.685680	50.309197
303.439123	151.923069	50.314202
299.841874	152.916943	50.319207
296.285062	157.096742	50.324212
293.483860	155.678502	50.329217
289.957131	151.007654	50.334221
286.199695	142.981375	50.339226
282.429868	152.585631	50.344231
278.973013	147.859549	50.349236
275.457774	149.922599	50.354241
271.762201	159.948668	50.359245
268.238676	147.295104	50.364250
264.680176	153.000121	50.369255
261.782225	143.399692	50.374260
258.389618	138.812254	50.379265
254.469770	153.603310	50.384269
250.821644	146.784307	50.389274
247.573415	159.401045	50.394279
243.921653	142.088352	50.399284
240.800042	149.974382	50.404289
237.314639	148.676002	50.409293
233.655849	143.874007	50.414298
229.928709	154.892132	50.419303
226.459503	155.274350	50.424308
223.087879	139.566116	50.429313
219.203059	153.304485	50.434317
215.803975	148.354243	50.439322
212.605561	150.905526	50.444327
209.250931	155.756042	50.449332
205.560303	158.618559	50.454337
201.964115	158.533457	50.459341
198.231252	150.028802	50.464346
194.543454	156.016694	50.469351
191.414060	148.872842	50.474356
188.002984	145.066616	50.479361
184.380006	154.806090	50.484365
181.323749	149.732551	50.489370
177.187790	158.163496	50.494375
173.872144	147.834430	50.499380
170.659072	145.901785	50.504385
167.122911	145.462443	50.509389
164.106418	142.698569	50.514394
159.973432	147.848213	50.519399
156.316518	156.153494	50.524404
152.808150	148.480568	50.529409
149.322949	156.800079	50.534413
145.958919	152.394872	50.539418
142.478053	151.004070	50.544423
138.706991	151.060288	50.549428
135.006014	149.422398	50.554433
131.280932	147.025815	50.559437
128.482225	147.733299	50.564442
124.727246	154.127214	50.569447
121.733841	138.033910	50.574452
118.392038	144.176429	50.579457
114.160167	159.048056	50.584461
111.046542	144.621915	50.589466
107.630431	153.933532	50.594471
104.049838	142.374173	50.599476
100.290646	143.130907	50.604481
96.504225	149.602524	50.609485
93.189827	144.904826	50.614490
89.654067	152.495116	50.619495
86.732377	145.008718	50.624500
82.663165	150.483765	50.629505
79.347776	149.956084	50.634509
76.232300	144.860229	50.639514
72.082811	155.463684	50.644519
69.145359	143.800414	50.649524
65.732290	148.720245	50.654529
61.542278	157.210325	50.659533
58.118448	144.047703	50.664538
54.359034	150.037375	50.669543
51.322953	145.378347	50.674548
48.310454	144.031261	50.679553
44.582553	151.901610	50.684557
40.524435	141.679449	50.689562
37.111422	142.783770	50.694567
33.661079	146.216151	50.699572
30.155564	141.368090	50.704577
26.827356	137.846345	50.709581
23.707343	144.378091	50.714586
20.182416	151.710443	50.719591
16.344947	144.677609	50.724596
12.686423	149.199317	50.729601
8.787511	156.688348	50.734605
5.879635	147.817247	50.739610
2.309161	145.304750	50.744615