Thu Aug 25 16:15:21 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.413639	99.746069	0.000000
1.001524	96.593119	0.005005
0.998621	82.932438	0.010010
0.770097	92.858236	0.015014
0.798710	86.513589	0.020019
0.700570	82.741968	0.025024
0.726724	77.024136	0.030029
0.253550	66.667363	0.035034
0.158670	60.237670	0.040038
-0.046177	50.047672	0.045043
-0.115476	39.640289	0.050048
-0.567921	36.512652	0.055053
-0.626391	16.672408	0.060058
-1.296449	20.694168	0.065062
-1.656893	13.939106	0.070067
-1.815228	18.393216	0.075072
-2.512138	8.998514	0.080077
-2.980738	-4.057620	0.085082
-3.037359	11.437884	0.090086
-3.377981	10.083419	0.095091
-3.246107	5.677825	0.100096
-3.763765	7.742648	0.105101
-4.674950	2.484919	0.110106
-5.051316	5.068606	0.115110
-5.113162	5.707922	0.120115
-4.654923	10.837379	0.125120
-4.956753	16.405470	0.130125
-4.911373	0.329667	0.135130
-5.079227	7.313108	0.140134
-5.136718	1.602079	0.145139
-5.559125	-1.527094	0.150144
-6.249394	5.633114	0.155149
-6.433050	0.258230	0.160154
-7.276523	8.223892	0.165158
-7.582222	9.527840	0.170163
-7.366028	3.112703	0.175168
-7.762050	14.564322	0.180173
-7.586341	3.118824	0.185178
-7.538642	12.001549	0.190182
-7.899236	10.716652	0.195187
-7.876214	-1.391455	0.200192
-8.691458	6.531818	0.205197
-8.597187	10.626807	0.210202
-9.334557	2.636831	0.215206
-9.905120	1.384834	0.220211
-9.903569	-2.095504	0.225216
-10.372785	11.424024	0.230221
-10.162069	6.522020	0.235226
-9.920442	14.646697	0.240230
-10.760070	12.376998	0.245235
-11.185104	1.231273	0.250240
-11.637650	10.154413	0.255245
-11.528360	0.721983	0.260250
-11.684962	12.876407	0.265254
-11.574198	9.075234	0.270259
-12.397547	2.142770	0.275264
-13.025246	8.166878	0.280269
-13.361703	3.236714	0.285274
-12.873837	6.333559	0.290278
-13.109722	8.923710	0.295283
-13.019324	9.178503	0.300288
-13.984605	12.477726	0.305293
-14.577197	8.562132	0.310298
-14.525732	14.195088	0.315302
-14.747815	14.492515	0.320307
-14.600109	18.509531	0.325312
-14.773077	15.793690	0.330317
-14.876201	1.848219	0.335322
-15.689862	12.023842	0.340326
-15.758836	9.557464	0.345331
-16.217241	9.202219	0.350336
-16.638505	10.913418	0.355341
-16.498872	6.411695	0.360346
-16.522428	9.610819	0.365350
-17.045551	7.879989	0.370355
-17.394478	-4.049614	0.375360
-18.010054	9.072065	0.380365
-17.722379	2.281896	0.385370
-17.688513	3.225755	0.390374
-18.136425	7.627158	0.395379
-18.552629	3.301114	0.400384
-19.154783	12.102163	0.405389
-19.388430	11.518713	0.410394
-19.507006	20.762853	0.415398
-19.233174	14.632911	0.420403
-19.274204	10.320846	0.425408
-20.090919	18.709428	0.430413
-20.726509	5.824987	0.435418
-20.653726	5.490917	0.440422
-20.975003	12.257953	0.445427
-20.893337	2.734938	0.450432
-20.743477	11.870574	0.455437
-21.611697	7.264176	0.460442
-22.173604	13.005894	0.465446
-22.454168	14.052804	0.470451
-22.333623	10.405122	0.475456
-22.358913	6.780291	0.480461
-22.359055	4.970682	0.485466
-23.132508	12.210365	0.490470
-23.774769	11.399874	0.495475
-23.916460	7.692042	0.500480
-24.258787	12.396443	0.505485
-24.110488	7.921835	0.510490
-23.844249	6.886737	0.515494
-24.143958	5.911841	0.520499
-24.443309	7.224286	0.525504
-25.333229	12.384647	0.530509
-25.357306	5.905917	0.535514
-25.567894	8.112452	0.540518
-25.443377	10.456307	0.545523
-26.069618	3.999162	0.550528
-26.510545	17.416185	0.555533
-26.714721	3.154353	0.560538
-26.974302	13.284288	0.565542
-26.972374	10.765672	0.570547
-26.677602	1.766088	0.575552
-28.163016	14.869039	0.580557
-28.115061	7.145156	0.585562
-28.219591	6.962255	0.590566
-28.720933	12.555277	0.595571
-28.165411	7.210105	0.600576
-28.631902	13.651882	0.605581
-28.811964	-1.869736	0.610586
-29.452357	10.562969	0.615590
-29.763995	9.662709	0.620595
-29.680026	8.393578	0.625600
-29.983143	19.185236	0.630605
-29.883936	3.306644	0.635610
-30.504949	9.797941	0.640614
-31.019117	9.745664	0.645619
-31.326155	9.085129	0.650624
-31.645027	7.860135	0.655629
-31.597459	6.913084	0.660634
-31.539722	9.428753	0.665638
-32.457154	18.643038	0.670643
-32.380499	0.477421	0.675648
-32.823951	16.185397	0.680653
-32.617684	14.558581	0.685658
-32.747757	18.078117	0.690662
-32.996864	19.711722	0.695667
-33.622945	24.564990	0.700672
-33.810725	14.410308	0.705677
-34.088625	12.520832	0.710682
-34.270868	28.175236	0.715686
-34.654790	15.320960	0.720691
-34.966181	13.512663	0.725696
-36.022419	18.180230	0.730701
-35.887692	17.887074	0.735706
-35.641384	13.795742	0.740710
-35.953812	17.068604	0.745715
-35.957994	7.470454	0.750720
-35.855132	21.374913	0.755725
-35.778056	16.946265	0.760730
-36.811275	4.747393	0.765734
-37.077685	11.834862	0.770739
-37.101713	16.628596	0.775744
-38.064503	17.972228	0.780749
-37.891585	18.489338	0.785754
-38.158723	18.031359	0.790758
-38.440117	21.213938	0.795763
-38.510048	11.670380	0.800768
-38.861490	21.574267	0.805773
-38.957011	27.831372	0.810778
-39.322936	25.531744	0.815782
-39.959472	20.885879	0.820787
-39.916411	12.223124	0.825792
-40.096075	25.947228	0.830797
-39.836199	16.579782	0.835802
-40.373548	21.985460	0.840806
-41.296752	18.811369	0.845811
-41.277150	18.254677	0.850816
-41.384376	14.686977	0.855821
-41.317807	13.471192	0.860826
-41.148695	16.020031	0.865830
-42.098438	18.971974	0.870835
-42.615110	10.267210	0.875840
-43.082086	21.821699	0.880845
-42.954446	16.610007	0.885850
-42.728380	20.393280	0.890854
-43.259627	21.542746	0.895859
-43.465223	9.087642	0.900864
-44.317992	18.168408	0.905869
-44.523580	11.917434	0.910874
-44.310057	17.195966	0.915878
-44.835518	9.571422	0.920883
-44.508252	7.359334	0.925888
-44.932953	17.138656	0.930893
-45.187380	12.935959	0.935898
-45.747116	21.331732	0.940902
-45.907360	14.238420	0.945907
-45.868369	7.923815	0.950912
-46.130835	9.720863	0.955917
-46.651853	6.085124	0.960922
-47.492875	9.928029	0.965926
-47.671653	13.531126	0.970931
-47.671385	18.406474	0.975936
-47.635184	17.027767	0.980941
-47.538864	19.986646	0.985946
-47.650687	5.036465	0.990950
-47.759476	12.750971	0.995955
-48.525015	14.655321	1.000960
-49.000240	16.577456	1.005965
-49.482491	16.687859	1.010970
-49.202553	12.414088	1.015974
-50.274135	10.187067	1.020979
-50.050027	15.938503	1.025984
-50.449351	14.441377	1.030989
-50.566740	13.627740	1.035994
-50.741935	12.000584	1.040998
-51.066137	4.562807	1.046003
-50.546465	10.967119	1.051008
-51.138250	12.094432	1.056013
-51.629626	13.310417	1.061018
-51.693693	12.418822	1.066022
-52.355269	18.483043	1.071027
-51.850431	19.815014	1.076032
-52.819138	14.487208	1.081037
-53.109914	13.533060	1.086042
-53.331013	-2.630693	1.091046
-53.670873	16.753153	1.096051
-53.464922	11.855060	1.101056
-53.576809	10.547014	1.106061
-53.821735	10.949261	1.111066
-54.523710	13.134717	1.116070
-54.864994	13.928550	1.121075
-54.977787	10.791995	1.126080
-55.141733	18.192442	1.131085
-55.149266	15.941063	1.136090
-55.714080	15.254481	1.141094
-56.055289	13.330634	1.146099
-55.960373	14.160523	1.151104
-56.107475	15.961642	1.156109
-56.276632	23.065514	1.161114
-56.844650	17.216179	1.166118
-57.362982	12.982067	1.171123
-57.087201	15.928644	1.176128
-57.534491	11.550524	1.181133
-57.611503	7.392796	1.186138
-58.397109	9.417350	1.191142
-59.419134	15.810132	1.196147
-58.796854	7.559660	1.201152
-59.185476	14.925708	1.206157
-59.309806	17.071273	1.211162
-59.383609	13.786238	1.216166
-59.404587	12.698067	1.221171
-59.351311	15.543466	1.226176
-60.137280	24.310048	1.231181
-60.502184	14.904459	1.236186
-60.724221	17.786671	1.241190
-61.039455	19.247139	1.246195
-60.543859	13.503230	1.251200
-61.315294	18.297016	1.256205
-61.699106	22.055628	1.261210
-61.936977	14.158231	1.266214
-62.491087	22.977067	1.271219
-62.333980	9.190138	1.276224
-62.615927	19.336234	1.281229
-63.261326	16.276805	1.286234
-63.424357	14.356677	1.291238
-63.851126	15.704908	1.296243
-63.760986	11.498842	1.301248
-63.757590	17.193112	1.306253
-63.532171	11.928136	1.311258
-63.883906	15.004676	1.316262
-64.755639	19.529440	1.321267
-64.939208	19.453838	1.326272
-65.283562	25.781568	1.331277
-65.315441	17.981606	1.336282
-65.327503	17.287507	1.341286
-66.172339	30.204676	1.346291
-66.673805	19.305043	1.351296
-66.813110	17.105950	1.356301
-66.700769	25.738102	1.361306
-66.957826	18.919388	1.366310
-67.008960	25.188518	1.371315
-66.977384	20.618303	1.376320
-67.595075	30.133641	1.381325
-67.965396	23.016297	1.386330
-67.807036	19.150717	1.391334
-68.203808	30.415799	1.396339
-68.911020	23.455647	1.401344
-69.283099	24.146738	1.406349
-69.907342	22.124871	1.411354
-69.907264	16.661085	1.416358
-70.231163	22.403477	1.421363
-69.565492	23.564713	1.426368
-69.678466	24.879594	1.431373
-69.717101	20.516534	1.436378
-70.534391	16.329268	1.441382
-71.206975	20.310298	1.446387
-71.359811	19.024488	1.451392
-71.407257	29.497677	1.456397
-71.567953	25.495428	1.461402
-71.989165	18.980847	1.466406
-72.695218	19.591391	1.471411
-72.838943	24.527268	1.476416
-72.937019	21.347276	1.481421
-73.107377	17.805288	1.486426
-73.179287	9.030838	1.491430
-73.525754	21.544043	1.496435
-73.241557	20.259356	1.501440
-73.743768	17.746968	1.506445
-74.210068	12.232875	1.511450
-74.281672	7.349800	1.516454
-74.695440	17.690556	1.521459
-74.643028	9.178201	1.526464
-75.403098	18.794937	1.531469
-75.659550	20.651156	1.536474
-75.347665	14.581691	1.541478
-75.908944	20.234728	1.546483
-76.114568	1.689403	1.551488
-76.387069	9.704806	1.556493
-76.776843	10.012691	1.561498
-77.374163	6.290834	1.566502
-77.608236	16.132033	1.571507
-77.242556	10.300913	1.576512
-77.541237	12.581365	1.581517
-77.718136	5.408411	1.586522
-78.122037	6.746731	1.591526
-78.861910	13.085811	1.596531
-78.796811	2.350514	1.601536
-79.262378	12.332388	1.606541
-79.258897	7.994369	1.611546
-79.309821	7.632227	1.616550
-79.245183	17.113408	1.621555
-80.105476	10.686614	1.626560
-80.375910	8.147402	1.631565
-80.455171	8.292737	1.636570
-80.138360	4.361203	1.641574
-80.886694	21.205285	1.646579
-81.348116	12.615255	1.651584
-81.981070	16.305337	1.656589
-81.967395	10.443953	1.661594
-81.652751	8.910886	1.666598
-82.201806	11.591238	1.671603
-82.197888	7.237332	1.676608
-82.648489	14.957941	1.681613
-83.351831	10.866718	1.686618
-83.116675	7.308647	1.691622
-83.702180	19.011419	1.696627
-83.530469	7.069840	1.701632
-83.827446	13.678044	1.706637
-84.192014	6.265577	1.711642
-84.563392	15.473393	1.716646
-85.041477	19.648574	1.721651
-84.784186	12.761924	1.726656
-84.868588	25.335307	1.731661
-85.163344	17.646141	1.736666
-85.680495	5.201899	1.741670
-86.444200	13.601156	1.746675
-86.361214	13.176902	1.751680
-86.777311	14.934749	1.756685
-86.514065	20.357348	1.761690
-86.387862	14.747250	1.766694
-87.385239	22.303601	1.771699
-87.519270	4.227949	1.776704
-88.044583	17.765758	1.781709
-88.035017	20.551568	1.786714
-88.205419	19.053375	1.791718
-88.304675	22.751580	1.796723
-88.368597	16.234801	1.801728
-88.945673	17.543310	1.806733
-89.263489	10.110861	1.811738
-89.502958	11.695499	1.816742
-89.438737	16.643082	1.821747
-90.264586	9.375661	1.826752
-90.718293	11.553854	1.831757
-90.930288	17.145832	1.836762
-90.830468	9.416988	1.841766
-91.175277	19.319832	1.846771
-90.660903	12.310641	1.851776
-91.031228	5.288219	1.856781
-91.735558	14.168555	1.861786
-92.025925	14.657018	1.866790
-92.139149	8.995853	1.871795
-92.239596	16.794473	1.876800
-92.830202	14.102949	1.881805
-93.308264	14.415178	1.886810
-93.269224	9.913400	1.891814
-93.522633	17.735988	1.896819
-93.701946	13.705022	1.901824
-93.874968	12.096509	1.906829
-94.152565	11.276339	1.911834
-94.356136	10.745126	1.916838
-95.208717	19.898632	1.921843
-95.155731	9.797981	1.926848
-95.391743	12.628597	1.931853
-95.880206	20.035601	1.936858
-95.789691	12.691029	1.941862
-95.776010	15.605907	1.946867
-95.904854	7.318109	1.951872
-96.427045	14.230522	1.956877
-96.888988	7.614762	1.961882
-96.617141	11.884402	1.966886
-97.237826	12.358186	1.971891
-97.593327	6.798261	1.976896
-98.193516	11.087486	1.981901
-98.415298	14.618228	1.986906
-98.259257	9.981057	1.991910
-98.507442	27.303593	1.996915
-98.536826	18.805916	2.006912
-98.840132	19.173467	2.016909
-98.206342	16.112329	2.026906
-97.416015	17.214505	2.036902
-97.497024	14.274876	2.046899
-96.119846	12.532271	2.056896
-95.963251	18.181353	2.066893
-95.574666	11.664545	2.076890
-94.866250	21.639917	2.086886
-94.616790	18.423591	2.096883
-94.364507	19.863501	2.106880
-93.231564	16.822350	2.116877
-93.057140	15.151002	2.126874
-92.618030	16.419085	2.136870
-92.142478	17.355175	2.146867
-91.463764	17.429464	2.156864
-90.860600	19.432116	2.166861
-90.480868	24.846664	2.176858
-90.059478	27.007681	2.186854
-89.409132	27.168778	2.196851
-89.141258	26.632701	2.206848
-88.796360	20.585236	2.216845
-87.955676	16.354435	2.226842
-87.675100	18.106693	2.236838
-86.695993	27.675356	2.246835
-85.979832	24.157817	2.256832
-85.854389	20.004244	2.266829
-86.268304	25.397434	2.276826
-85.085158	26.365200	2.286822
-84.779364	33.071132	2.296819
-83.730286	28.297657	2.306816
-83.280130	27.048770	2.316813
-83.123723	24.293685	2.326810
-82.463084	29.458311	2.336806
-81.750537	24.829436	2.346803
-81.703539	23.019663	2.356800
-81.110046	26.607737	2.366797
-80.616021	25.858826	2.376794
-80.031272	21.826519	2.386790
-79.379195	19.880752	2.396787
-79.176202	13.041398	2.406784
-78.127051	18.056446	2.416781
-77.830948	26.135556	2.426778
-77.766893	17.262062	2.436774
-77.112001	21.290344	2.446771
-76.529334	17.366069	2.456768
-76.113838	20.430835	2.466765
-75.294828	29.818680	2.476762
-74.899744	24.124480	2.486758
-74.833039	27.338935	2.496755
-73.874430	24.797105	2.506752
-73.671705	18.290411	2.516749
-72.578418	20.529879	2.526746
-72.441303	18.810524	2.536742
-72.300462	25.950949	2.546739
-71.158050	21.834428	2.556736
-70.537145	16.817604	2.566733
-70.350808	26.779754	2.576730
-70.494005	24.974440	2.586726
-69.814348	26.106633	2.596723
-68.890204	18.698112	2.606720
-67.726245	18.110325	2.616717
-67.963434	22.246712	2.626714
-67.698186	21.869437	2.636710
-67.089182	21.786757	2.646707
-66.362390	22.483909	2.656704
-65.881882	17.929409	2.666701
-65.484439	15.497686	2.676698
-64.936898	19.856403	2.686694
-64.624170	17.694547	2.696691
-63.629160	25.746509	2.706688
-63.186748	19.256110	2.716685
-63.176775	23.667383	2.726682
-62.500606	23.669213	2.736678
-61.986593	22.967856	2.746675
-61.739917	20.895545	2.756672
-60.643734	23.704767	2.766669
-60.303936	26.239701	2.776666
-60.233753	24.226722	2.786662
-59.352525	25.026389	2.796659
-58.915689	26.272657	2.806656
-58.744424	26.901634	2.816653
-58.015372	29.581483	2.826650
-57.525087	29.989410	2.836646
-56.726887	28.559276	2.846643
-56.282939	23.750743	2.856640
-56.034833	24.199785	2.866637
-55.273914	26.285428	2.876634
-54.838577	24.966004	2.886630
-54.741934	25.638351	2.896627
-53.889298	20.341294	2.906624
-53.190317	21.799912	2.916621
-53.346732	24.079977	2.926618
-52.386284	24.727848	2.936614
-52.334798	29.842207	2.946611
-50.973937	20.584947	2.956608
-50.727119	27.702434	2.966605
-50.620719	21.103125	2.976602
-50.012410	28.743680	2.986598
-48.980189	15.980465	2.996595
-48.745022	27.727948	3.006592
-48.836415	25.334806	3.016589
-47.545980	27.948868	3.026586
-47.607028	24.334532	3.036582
-46.850147	18.244689	3.046579
-46.008900	16.472023	3.056576
-45.830013	24.851438	3.066573
-45.731777	21.703156	3.076570
-45.121753	20.578108	3.086566
-44.603138	25.793502	3.096563
-43.595297	20.839593	3.106560
-42.845163	14.319986	3.116557
-42.888470	21.809214	3.126554
-42.836944	30.500027	3.136550
-42.056450	27.675663	3.146547
-41.449469	22.781397	3.156544
-40.352712	21.237960	3.166541
-40.119924	30.033419	3.176538
-39.841086	22.950925	3.186534
-40.032470	24.938695	3.196531
-38.981469	15.729991	3.206528
-38.527993	20.502593	3.216525
-37.126055	20.533258	3.226522
-37.604444	17.256747	3.236518
-37.078894	23.456243	3.246515
-36.238932	23.695340	3.256512
-35.885514	16.468115	3.266509
-35.613838	21.573314	3.276506
-34.569047	25.261741	3.286502
-34.322554	23.838860	3.296499
-34.029854	21.467899	3.306496
-33.402913	21.363404	3.316493
-32.702216	15.459763	3.326490
-32.588276	21.926494	3.336486
-31.893565	15.117796	3.346483
-31.127073	18.054709	3.356480
-30.768176	19.427232	3.366477
-30.558193	20.180022	3.376474
-29.762890	21.544354	3.386470
-29.645612	24.345405	3.396467
-28.646045	17.200669	3.406464
-28.361649	22.652335	3.416461
-28.004663	20.340993	3.426458
-27.117030	25.802679	3.436454
-26.728394	20.746220	3.446451
-26.560226	21.828680	3.456448
-25.230136	24.015212	3.466445
-25.004421	20.156372	3.476442
-25.049176	22.374592	3.486438
-24.831996	24.206479	3.496435
-24.058390	26.068390	3.506432
-23.335171	18.776886	3.516429
-22.757287	15.078278	3.526426
-22.321807	13.404039	3.536422
-22.102455	19.055964	3.546419
-21.306122	23.584780	3.556416
-20.773332	23.339815	3.566413
-20.152067	20.714633	3.576410
-19.518426	13.956687	3.586406
-19.462768	27.709014	3.596403
-18.951469	15.702165	3.606400
-18.162358	15.160446	3.616397
-17.856826	17.235081	3.626394
-17.568824	25.385159	3.636390
-16.487477	11.340790	3.646387
-16.214818	18.400374	3.656384
-16.022365	17.955311	3.666381
-15.093249	16.143538	3.676378
-14.593574	15.811896	3.686374
-14.763161	16.456266	3.696371
-13.543245	18.197563	3.706368
-13.061320	18.372384	3.716365
-12.886095	21.468466	3.726362
-12.737744	23.770470	3.736358
-11.887525	27.970896	3.746355
-11.257353	19.186091	3.756352
-10.473316	18.331555	3.766349
-10.324768	15.736092	3.776346
-10.374405	18.477765	3.786342
-9.271185	17.028354	3.796339
-8.893902	19.503564	3.806336
-7.866260	15.690136	3.816333
-7.491407	11.218718	3.826330
-7.503426	16.029412	3.836326
-7.210569	19.008861	3.846323
-6.133805	18.970103	3.856320
-5.968126	17.334971	3.866317
-4.956013	11.540928	3.876314
-4.664685	9.854431	3.886310
-4.536256	15.723343	3.896307
-4.121741	20.628766	3.906304
-3.499122	25.926070	3.916301
-3.274420	37.456626	3.926298
-2.620484	46.265305	3.936294
-2.059646	60.892019	3.946291
-1.869234	72.288586	3.956288
-1.497671	89.666138	3.966285
-0.871628	99.299680	3.976282
-0.293581	120.319588	3.986278
0.000000	137.146621	3.991283
-0.013356	145.036061	3.996288
0.771557	143.043319	4.001293
0.692722	150.205859	4.006298
0.675794	155.586983	4.011302
0.626645	169.221148	4.016307
0.679017	170.905606	4.021312
0.974813	177.095123	4.026317
0.987906	181.629983	4.031322
1.230086	174.090732	4.036326
0.575439	182.450831	4.041331
1.187051	177.691614	4.046336
1.063374	172.019374	4.051341
0.869017	173.663396	4.056346
0.886709	178.865094	4.061350
0.998860	177.664302	4.066355
0.923423	190.897638	4.071360
0.995402	179.319581	4.076365
0.640711	183.785515	4.081370
0.819008	182.406678	4.086374
1.315240	198.654126	4.091379
1.214550	198.695251	4.096384
1.185824	194.001558	4.101389
0.995151	211.868938	4.106394
1.396763	199.239460	4.111398
1.128402	209.054504	4.116403
1.446442	199.282372	4.121408
1.578645	209.667413	4.126413
1.023999	204.613189	4.131418
1.203248	194.682470	4.136422
1.300923	209.565505	4.141427
1.512992	206.273607	4.146432
1.112186	196.373661	4.151437
0.857147	206.139158	4.156442
1.531552	211.127236	4.161446
1.253503	204.501562	4.166451
1.519763	220.652183	4.171456
1.514551	209.250719	4.176461
0.971311	216.558818	4.181466
1.370352	214.645511	4.186470
1.420966	216.200533	4.191475
0.947089	216.898088	4.196480
1.356634	218.428509	4.201485
1.422970	214.918995	4.206490
1.790604	205.047340	4.211494
1.532722	217.065910	4.216499
1.711549	206.050069	4.221504
1.754973	212.763202	4.226509
1.635929	209.836399	4.231514
1.717518	214.211836	4.236518
1.545901	220.560028	4.241523
1.768116	220.139265	4.246528
1.885196	210.582114	4.251533
1.321141	206.114666	4.256538
1.285187	203.222302	4.261542
1.383727	210.800006	4.266547
1.119996	216.501396	4.271552
1.790413	222.603758	4.276557
1.676571	221.925597	4.281562
1.858154	216.550368	4.286566
1.494004	219.556120	4.291571
1.704286	214.046679	4.296576
1.473172	216.281767	4.301581
1.398026	219.283366	4.306586
1.727097	212.758717	4.311590
1.820137	223.399842	4.316595
1.639545	221.533061	4.321600
1.953047	220.626589	4.326605
1.024465	230.162271	4.331610
1.584935	216.378415	4.336614
1.476946	221.580835	4.341619
1.616862	225.760472	4.346624
1.198632	224.756676	4.351629
1.621076	250.677972	4.356634
2.015114	238.827949	4.361638
1.831881	245.674686	4.366643
1.613682	252.106118	4.371648
1.850336	254.334358	4.376653
1.611036	256.213223	4.381658
1.962671	249.814742	4.386662
1.932981	250.050389	4.391667
2.117818	246.746931	4.396672
1.861183	248.764555	4.401677
1.927661	250.548052	4.406682
1.880977	248.097130	4.411686
1.917045	249.363365	4.416691
2.201490	248.233651	4.421696
2.201483	248.727242	4.426701
1.505586	254.863359	4.431706
2.143343	250.150646	4.436710
2.159026	249.290837	4.441715
1.852530	255.375431	4.446720
1.990208	254.594584	4.451725
1.705879	249.589744	4.456730
1.987772	250.561194	4.461734
1.884632	253.785487	4.466739
2.085889	248.527390	4.471744
2.053912	253.980505	4.476749
1.790499	253.468149	4.481754
2.027164	270.259378	4.486758
2.319597	281.464090	4.491763
2.273894	278.123981	4.496768
2.495383	271.220692	4.501773
2.054055	269.869330	4.506778
2.039846	266.381917	4.511782
2.349452	286.350847	4.516787
2.129787	278.770018	4.521792
2.321204	278.607184	4.526797
2.158556	279.240157	4.531802
2.554983	284.278138	4.536806
2.216582	285.754911	4.541811
2.028390	286.217877	4.546816
2.355437	282.243550	4.551821
2.118773	286.140515	4.556826
2.468179	281.843140	4.561830
2.553632	282.136677	4.566835
2.714749	283.380157	4.571840
2.651202	265.755097	4.576845
2.135502	261.729319	4.581850
2.217285	261.213498	4.586854
2.483214	275.026170	4.591859
2.330883	275.616397	4.596864
2.760030	279.984851	4.601869
2.476711	270.813112	4.606874
2.539425	267.256698	4.611878
2.449820	251.989605	4.616883
1.922636	266.856697	4.621888
2.303431	259.833538	4.626893
1.953542	284.287665	4.631898
2.090732	272.901814	4.636902
2.291194	274.809855	4.641907
2.231839	283.544972	4.646912
2.357907	280.892969	4.651917
2.367180	289.206041	4.656922
2.752428	290.651689	4.661926
2.895726	283.779629	4.666931
2.297896	284.015709	4.671936
2.758805	289.416917	4.676941
2.336387	287.562709	4.681946
2.744038	292.671702	4.686950
2.760880	306.007725	4.691955
2.590361	304.367151	4.696960
3.024447	295.858128	4.701965
2.399047	299.974195	4.706970
2.663026	304.602656	4.711974
3.088921	308.614116	4.716979
2.706407	300.514618	4.721984
2.647120	284.236656	4.726989
2.532851	298.994783	4.731994
2.834488	304.234287	4.736998
2.780213	306.027218	4.742003
2.582148	306.289248	4.747008
3.040817	298.798283	4.752013
2.946539	311.107663	4.757018
2.981812	310.317549	4.762022
2.786340	307.538748	4.767027
2.883988	309.823577	4.772032
2.945327	304.941734	4.777037
2.926749	304.830785	4.782042
3.085867	303.208167	4.787046
2.678016	301.386477	4.792051
2.378275	302.110534	4.797056
2.730712	302.691277	4.802061
2.647171	308.968751	4.807066
2.690065	301.299316	4.812070
2.842818	307.903605	4.817075
2.768645	314.103681	4.822080
3.241900	305.110781	4.827085
2.940626	314.260311	4.832090
3.244685	310.580650	4.837094
3.129502	314.297232	4.842099
2.971153	308.048240	4.847104
3.062592	304.091842	4.852109
2.608987	303.270757	4.857114
2.780983	307.635216	4.862118
2.809326	304.403725	4.867123
2.740014	325.333755	4.872128
3.100554	327.938070	4.877133
3.202972	325.188524	4.882138
3.260581	327.552397	4.887142
3.383071	324.980044	4.892147
3.226004	324.745258	4.897152
3.270089	330.135857	4.902157
3.354793	327.211913	4.907162
3.441267	323.534704	4.912166
3.069262	310.716307	4.917171
3.150458	307.299361	4.922176
3.166816	312.811360	4.927181
2.864805	332.442730	4.932186
3.230312	332.619621	4.937190
3.083647	328.311374	4.942195
3.215555	330.923039	4.947200
3.320895	329.406923	4.952205
3.148244	330.313553	4.957210
3.117457	329.312321	4.962214
3.311580	327.598792	4.967219
3.040061	326.995954	4.972224
3.087979	328.367907	4.977229
3.083822	329.225990	4.982234
3.552590	327.491576	4.987238
3.133570	329.132848	4.992243
3.392172	331.006475	4.997248
3.916014	336.015016	5.002253
3.341579	342.644669	5.007258
3.346809	325.157473	5.012262
3.338490	323.614872	5.017267
3.019494	337.753364	5.022272
3.677528	342.253653	5.027277
3.670532	350.506026	5.032282
3.676264	349.388337	5.037286
3.781496	355.164840	5.042291
3.429654	342.770378	5.047296
3.472207	337.499155	5.052301
3.557992	340.991262	5.057306
3.690611	347.114655	5.062310
3.808219	341.866474	5.067315
3.352876	337.438907	5.072320
3.522295	343.528059	5.077325
3.524616	349.016959	5.082330
3.698508	356.238061	5.087334
3.771103	352.009352	5.092339
3.740693	362.049794	5.097344
4.156525	350.373456	5.102349
3.708798	348.301740	5.107354
3.914522	332.181531	5.112358
3.666405	329.597641	5.117363
3.637758	326.460498	5.122368
3.747189	327.914564	5.127373
3.435546	339.141194	5.132378
3.700004	346.677140	5.137382
3.812851	346.232381	5.142387
3.879207	360.699662	5.147392
3.908157	356.041183	5.152397
4.002925	352.720180	5.157402
3.656882	352.745962	5.162406
3.677529	354.612582	5.167411
4.018808	359.067591	5.172416
4.189161	345.702273	5.177421
3.633185	351.443168	5.182426
4.386547	345.880233	5.187430
4.216304	331.460955	5.192435
3.619212	333.857805	5.197440
3.681667	325.887897	5.202445
3.873023	341.936468	5.207450
3.959441	347.807667	5.212454
4.285809	350.344572	5.217459
3.944811	342.210076	5.222464
3.948138	328.744388	5.227469
4.040066	341.613084	5.232474
4.134555	335.631357	5.237478
3.951652	334.736218	5.242483
3.923948	335.075961	5.247488
3.908615	343.272688	5.252493
3.648727	355.652341	5.257498
3.979218	359.378198	5.262502
4.084409	353.227106	5.267507
4.186403	361.620598	5.272512
4.172345	341.529420	5.277517
3.844978	362.325916	5.282522
4.182660	355.103826	5.287526
4.043211	353.733632	5.292531
4.032770	347.641789	5.297536
4.126498	356.267533	5.302541
3.917809	367.266074	5.307546
3.882074	359.216621	5.312550
3.946800	358.285845	5.317555
3.928650	360.535039	5.322560
3.903136	374.295374	5.327565
4.014841	386.857277	5.332570
4.183042	384.230295	5.337574
4.394431	382.517220	5.342579
3.956560	387.970696	5.347584
4.145995	385.125247	5.352589
4.372332	397.270554	5.357594
4.374258	396.042725	5.362598
4.714095	390.516095	5.367603
4.312131	390.212110	5.372608
4.762867	384.870590	5.377613
4.450052	390.073514	5.382618
4.357953	383.437620	5.387622
4.367565	382.496495	5.392627
4.207290	386.960492	5.397632
4.194623	388.322960	5.402637
4.480666	387.006321	5.407642
4.398886	377.322048	5.412646
4.421364	383.889828	5.417651
4.203380	383.237470	5.422656
4.522345	383.636794	5.427661
4.109272	380.243493	5.432666
4.491692	386.492279	5.437670
4.270328	391.098730	5.442675
4.163854	398.629540	5.447680
4.238408	395.631243	5.452685
4.595392	410.072010	5.457690
4.562116	418.122883	5.462694
4.814745	411.141893	5.467699
4.831546	421.988075	5.472704
4.885746	419.160646	5.477709
4.710486	425.927107	5.482714
4.465724	409.124420	5.487718
4.796822	412.926125	5.492723
4.494489	419.041761	5.497728
4.903761	414.485033	5.502733
4.645432	420.954451	5.507738
4.899971	408.439622	5.512742
4.624506	408.217059	5.517747
4.514792	417.937755	5.522752
4.795123	416.894098	5.527757
4.717621	422.031687	5.532762
4.654478	413.891588	5.537766
4.594369	412.338112	5.542771
4.582237	414.991340	5.547776
4.697407	412.689047	5.552781
4.394972	420.510004	5.557786
4.379968	411.533440	5.562790
4.803710	412.352957	5.567795
4.563519	412.574130	5.572800
4.941984	409.148553	5.577805
4.707110	421.470547	5.582810
4.921958	425.280978	5.587814
4.855248	421.485378	5.592819
4.848379	440.637177	5.597824
5.125602	442.593322	5.602829
5.237418	439.063983	5.607834
5.043875	416.552034	5.612838
4.924343	424.461397	5.617843
4.677976	423.307272	5.622848
4.783153	429.409682	5.627853
4.635701	437.396194	5.632858
4.993051	451.966655	5.637862
5.218811	434.811804	5.642867
5.063271	443.745572	5.647872
4.907129	438.654152	5.652877
4.784326	447.959289	5.657882
4.663763	438.198800	5.662886
5.106460	444.646976	5.667891
4.644778	441.954159	5.672896
4.987618	436.642185	5.677901
5.030543	444.570396	5.682906
5.207300	441.347265	5.687910
5.338311	445.541004	5.692915
5.429940	445.925328	5.697920
5.318452	442.250638	5.702925
5.018720	445.521587	5.707930
5.244272	449.371476	5.712934
5.269849	450.601402	5.717939
5.093625	451.144757	5.722944
5.211197	441.679157	5.727949
5.242448	444.214859	5.732954
5.365077	441.794331	5.737958
5.486210	447.944869	5.742963
5.037814	457.497184	5.747968
5.337391	447.990409	5.752973
5.443640	450.878201	5.757978
5.387752	442.382603	5.762982
5.212884	447.291839	5.767987
5.734824	447.963090	5.772992
5.503986	436.982820	5.777997
5.666502	453.877591	5.783002
5.190358	452.224777	5.788006
5.432448	452.598182	5.793011
5.200491	444.500339	5.798016
5.394820	449.029017	5.803021
5.154841	450.325862	5.808026
5.014775	448.471690	5.813030
5.348791	463.169206	5.818035
5.617739	470.093880	5.823040
5.419171	470.713504	5.828045
5.297255	484.463718	5.833050
5.538084	477.278901	5.838054
5.709233	475.834721	5.843059
5.598392	472.795855	5.848064
5.518147	481.271743	5.853069
5.383460	473.380115	5.858074
5.614979	471.945460	5.863078
5.641897	478.000036	5.868083
5.677240	483.933068	5.873088
5.532266	470.661357	5.878093
5.596311	475.169325	5.883098
5.570247	474.157854	5.888102
5.692233	478.599795	5.893107
5.637606	486.242744	5.898112
5.781171	475.624579	5.903117
5.719653	474.314933	5.908122
5.567053	478.869502	5.913126
5.792659	475.964587	5.918131
5.590352	482.131012	5.923136
5.467384	480.397548	5.928141
5.464133	489.095500	5.933146
5.375827	485.167225	5.938150
5.752493	471.402481	5.943155
5.450366	486.111101	5.948160
6.105410	495.965123	5.953165
5.637204	498.379766	5.958170
5.685336	502.757353	5.963174
6.065761	495.414611	5.968179
5.863717	506.418524	5.973184
6.233433	497.761299	5.978189
5.931566	500.365021	5.983194
5.917590	477.536951	5.988198
5.844146	478.630529	5.993203
5.656021	488.819143	5.998208
6.096054	489.876563	6.003213
5.700360	499.547197	6.008218
6.046103	506.877480	6.013222
6.425217	510.311004	6.018227
5.632320	492.508923	6.023232
5.664710	484.186140	6.028237
5.717068	496.624537	6.033242
5.833000	503.525741	6.038246
6.099623	502.876545	6.043251
5.823128	510.288505	6.048256
6.027852	503.893969	6.053261
6.058914	509.808697	6.058266
5.985047	513.249920	6.063270
5.856893	509.663250	6.068275
5.226004	506.936822	6.073280
6.120952	503.683411	6.078285
6.288064	515.034461	6.083290
6.030342	516.425842	6.088294
6.032807	514.979615	6.093299
6.003946	507.764273	6.098304
5.922243	491.704776	6.103309
5.585463	493.788769	6.108314
6.015211	496.325317	6.113318
6.145681	506.536791	6.118323
6.020789	495.780337	6.123328
5.959173	494.666864	6.128333
5.804487	490.739496	6.133338
5.526374	490.447742	6.138342
6.087456	499.272418	6.143347
5.717173	505.734098	6.148352
5.879977	507.682868	6.153357
5.991363	507.159237	6.158362
6.025792	500.550933	6.163366
6.365379	493.385438	6.168371
5.826903	495.643408	6.173376
5.855517	475.997822	6.178381
5.796887	489.073717	6.183386
6.034267	485.357011	6.188390
5.925267	485.497517	6.193395
5.669928	490.919260	6.198400
6.079776	498.726727	6.203405
5.913693	506.010651	6.208410
6.074958	496.452753	6.213414
5.992472	483.889434	6.218419
5.958724	480.443007	6.223424
5.743675	476.490298	6.228429
5.873547	489.397449	6.233434
5.599774	485.574165	6.238438
5.856064	493.794843	6.243443
5.995239	501.394778	6.248448
6.098366	509.025675	6.253453
5.894060	510.180890	6.258458
6.161082	507.876939	6.263462
6.089445	488.841850	6.268467
5.430489	495.064010	6.273472
5.826604	499.665491	6.278477
5.733741	513.003039	6.283482
6.013424	508.112240	6.288486
5.935768	510.551116	6.293491
5.890551	515.674181	6.298496
6.086481	501.346093	6.303501
5.985637	503.620917	6.308506
5.905709	510.176314	6.313510
6.089975	509.093919	6.318515
5.969673	508.676195	6.323520
5.747376	487.048213	6.328525
5.531050	489.939096	6.333530
5.454728	507.513599	6.338534
6.088797	504.626940	6.343539
5.595768	513.148535	6.348544
5.885065	503.184584	6.353549
5.632497	515.503087	6.358554
6.201448	519.099863	6.363558
6.165368	511.524973	6.368563
5.836184	515.787670	6.373568
5.954965	505.622637	6.378573
5.844508	505.889925	6.383578
6.167700	499.771066	6.388582
6.233808	508.087990	6.393587
5.859669	510.465749	6.398592
5.827248	505.867469	6.403597
6.046894	508.234452	6.408602
6.257918	509.615665	6.413606
6.271815	511.685846	6.418611
5.799418	495.671740	6.423616
5.893564	488.234647	6.428621
5.591841	486.048286	6.433626
5.910569	505.585750	6.438630
6.250058	505.909093	6.443635
5.909904	502.728976	6.448640
5.953326	494.432934	6.453645
5.562642	489.150452	6.458650
5.860996	498.604769	6.463654
6.007392	503.343457	6.468659
5.992473	505.351711	6.473664
6.229686	507.114810	6.478669
5.594690	497.586756	6.483674
5.907766	499.474014	6.488678
5.838699	500.608038	6.493683
5.730548	508.060061	6.498688
5.469040	514.881199	6.503693
5.901611	516.063180	6.508698
6.045374	509.981923	6.513702
6.168847	513.809853	6.518707
5.699572	521.150780	6.523712
6.416744	509.056954	6.528717
6.161124	510.963713	6.533722
5.647294	511.329005	6.538726
5.836340	511.410157	6.543731
5.800092	521.973638	6.548736
6.253598	505.950495	6.553741
5.948962	510.661775	6.558746
5.733653	515.166066	6.563750
6.087622	504.328249	6.568755
5.496666	510.742247	6.573760
5.780709	510.428853	6.578765
6.107405	507.596680	6.583770
5.942365	517.082483	6.588774
6.278845	515.273863	6.593779
6.187889	516.003182	6.598784
6.450040	504.996248	6.603789
6.215493	491.567709	6.608794
5.695382	489.909125	6.613798
6.142026	482.033979	6.618803
5.952475	495.288584	6.623808
5.915513	478.753838	6.628813
5.660474	482.501859	6.633818
5.881152	484.520655	6.638822
5.980693	487.956849	6.643827
5.770259	479.706917	6.648832
6.060115	478.275776	6.653837
5.779734	478.231157	6.658842
5.705386	484.564201	6.663846
5.750254	470.803988	6.668851
5.805417	477.847585	6.673856
5.775346	476.700696	6.678861
5.984684	503.329648	6.683866
5.959089	500.093917	6.688870
5.918754	490.947271	6.693875
5.762167	485.030144	6.698880
6.084544	500.703979	6.703885
5.606275	492.359961	6.708890
5.614754	505.263996	6.713894
6.210299	501.785406	6.718899
5.816107	513.382594	6.723904
6.247994	505.639468	6.728909
5.881085	513.502206	6.733914
5.781680	516.330480	6.738918
6.238873	520.172564	6.743923
5.928868	508.597195	6.748928
5.533296	497.433885	6.753933
6.020430	508.953095	6.758938
6.452356	504.778783	6.763942
6.086799	489.345910	6.768947
5.727701	488.237918	6.773952
5.829537	483.865387	6.778957
6.035525	485.880156	6.783962
6.059577	485.870098	6.788966
6.095029	477.214635	6.793971
5.745131	496.312670	6.798976
5.758157	481.677888	6.803981
6.030617	480.078625	6.808986
5.694746	480.558407	6.813990
5.908472	476.535352	6.818995
5.830892	494.695351	6.824000
5.941893	489.150760	6.829005
6.049321	487.751366	6.834010
5.665770	486.216922	6.839014
6.151276	491.127107	6.844019
5.890980	495.094260	6.849024
5.871438	490.690124	6.854029
5.871295	485.666000	6.859034
5.674321	486.956110	6.864038
6.122319	490.957821	6.869043
5.929181	502.162821	6.874048
6.282163	494.159973	6.879053
5.668957	491.668064	6.884058
5.837402	485.551310	6.889062
6.360598	485.646547	6.894067
6.084415	481.921720	6.899072
5.752852	484.295969	6.904077
5.835529	476.632882	6.909082
5.664859	479.149604	6.914086
5.866757	480.766369	6.919091
5.667465	494.414816	6.924096
6.051552	490.472636	6.929101
5.975135	493.866797	6.934106
6.046481	493.210231	6.939110
5.891459	490.811053	6.944115
5.435141	493.043494	6.949120
5.956714	504.316852	6.954125
6.060372	505.309915	6.959130
6.118777	510.802732	6.964134
6.210221	494.614860	6.969139
5.640952	486.607815	6.974144
5.846962	484.933539	6.979149
6.018842	490.392751	6.984154
5.664908	494.827005	6.989158
6.155264	495.398800	6.994163
6.084942	497.327146	6.999168
5.759171	496.479695	7.004173
5.818080	490.456034	7.009178
5.831274	488.568353	7.014182
6.219814	489.662316	7.019187
6.009362	497.962454	7.024192
6.215063	478.032848	7.029197
6.366603	484.710161	7.034202
6.144067	483.504839	7.039206
5.846567	481.450699	7.044211
5.475129	487.219671	7.049216
6.315670	478.466538	7.054221
6.275607	484.863815	7.059226
5.804572	484.785792	7.064230
5.742955	475.737403	7.069235
5.780427	486.207052	7.074240
6.086047	479.844173	7.079245
5.972851	477.438444	7.084250
5.961265	483.075100	7.089254
5.905013	475.522368	7.094259
5.914076	477.393980	7.099264
6.021595	474.953669	7.104269
6.115315	487.670324	7.109274
5.944973	487.386995	7.114278
6.203782	482.420378	7.119283
5.885814	483.340292	7.124288
6.096536	487.898050	7.129293
6.254033	489.309796	7.134298
6.301587	482.832322	7.139302
6.320267	465.039153	7.144307
6.106165	455.546418	7.149312
5.779777	443.707896	7.154317
5.786182	449.180367	7.159322
5.619883	441.239921	7.164326
5.845670	443.764125	7.169331
5.887812	457.760703	7.174336
5.768835	448.901654	7.179341
5.932664	457.380418	7.184346
5.904898	478.003552	7.189350
6.285140	469.313053	7.194355
5.954715	461.474247	7.199360
5.858920	458.369749	7.204365
5.770379	452.767847	7.209370
5.734876	449.400796	7.214374
5.785592	464.266091	7.219379
5.750831	465.635190	7.224384
5.932153	466.796422	7.229389
6.285097	469.591779	7.234394
5.776788	470.282081	7.239398
6.045460	467.250193	7.244403
5.975456	465.755211	7.249408
5.901446	459.831483	7.254413
5.971347	456.916164	7.259418
5.699053	452.279549	7.264422
6.343395	453.940887	7.269427
5.628427	459.798478	7.274432
5.934155	458.579993	7.279437
5.740055	459.056544	7.284442
5.601757	469.537904	7.289446
5.945377	472.322068	7.294451
5.817408	473.939896	7.299456
6.082295	471.617300	7.304461
6.143822	473.439562	7.309466
5.787697	468.743309	7.314470
6.339345	462.120420	7.319475
5.903308	464.324369	7.324480
5.721999	458.737000	7.329485
5.548690	457.093685	7.334490
6.064356	476.106701	7.339494
6.047693	475.811948	7.344499
5.762320	474.382349	7.349504
5.628751	470.258683	7.354509
5.773834	481.698587	7.359514
5.988180	486.084929	7.364518
6.005385	478.536505	7.369523
6.080775	477.727443	7.374528
5.809038	474.549266	7.379533
5.836539	474.719006	7.384538
5.764842	480.254345	7.389542
6.270566	481.617856	7.394547
5.658297	486.905693	7.399552
5.958783	485.447575	7.404557
5.798413	488.168335	7.409562
5.593192	488.580188	7.414566
6.292019	480.788920	7.419571
5.791518	489.242071	7.424576
5.843489	481.007973	7.429581
5.758862	489.883195	7.434586
5.734196	494.870153	7.439590
6.038382	476.788622	7.444595
6.218395	487.859215	7.449600
6.170136	479.764212	7.454605
5.838493	483.154067	7.459610
5.832692	478.507329	7.464614
6.236507	474.359575	7.469619
6.284597	482.679310	7.474624
6.225735	472.197271	7.479629
5.989271	461.315946	7.484634
5.696320	464.320074	7.489638
5.921538	454.470596	7.494643
6.219662	467.816453	7.499648
5.918560	454.521759	7.504653
5.608410	455.035477	7.509658
5.619240	467.312677	7.514662
6.070774	479.255071	7.519667
6.083885	486.542549	7.524672
6.023473	466.505950	7.529677
5.775397	463.833447	7.534682
5.877817	461.510998	7.539686
6.040187	475.909543	7.544691
5.998825	469.034707	7.549696
5.485334	472.582770	7.554701
5.801087	472.761130	7.559706
5.794571	478.336878	7.564710
5.905444	473.478866	7.569715
5.750883	480.238940	7.574720
5.742217	480.892087	7.579725
5.750965	485.323297	7.584730
5.921751	485.679401	7.589734
6.008608	481.666732	7.594739
6.304144	488.609394	7.599744
6.070466	485.238585	7.604749
6.034029	477.733369	7.609754
5.605785	482.799377	7.614758
6.066405	475.709841	7.619763
6.119015	481.855308	7.624768
6.146380	481.009476	7.629773
6.088138	483.657284	7.634778
6.076850	469.608469	7.639782
5.598079	460.767822	7.644787
5.412506	474.002804	7.649792
5.965237	471.217481	7.654797
5.882893	484.964659	7.659802
5.870822	492.642073	7.664806
6.253931	484.008067	7.669811
5.860305	493.187978	7.674816
5.714014	491.129127	7.679821
6.075213	482.561831	7.684826
5.990783	486.539393	7.689830
6.039996	479.318158	7.694835
5.851175	485.321116	7.699840
5.866677	487.182229	7.704845
6.107743	483.600991	7.709850
6.173936	490.247384	7.714854
5.791770	475.218934	7.719859
5.766267	466.221840	7.724864
5.910127	477.320238	7.729869
6.281331	478.125843	7.734874
5.485504	472.406959	7.739878
5.769480	470.938773	7.744883
6.327009	484.724903	7.749888
5.732584	477.914572	7.754893
6.120701	469.988489	7.759898
6.049684	465.155814	7.764902
6.081827	454.112182	7.769907
5.737585	458.677790	7.774912
5.771263	455.717526	7.779917
6.166832	457.765864	7.784922
5.852382	452.721392	7.789926
6.198252	451.863622	7.794931
5.958028	454.078019	7.799936
6.055419	451.734213	7.804941
6.285026	450.049916	7.809946
6.008922	449.814797	7.814950
6.267618	445.503121	7.819955
5.714287	450.876628	7.824960
5.836435	451.563063	7.829965
6.178823	453.379282	7.834970
5.737194	453.685803	7.839974
6.072119	448.552241	7.844979
5.964733	455.975648	7.849984
6.032897	452.674614	7.854989
6.047727	443.440252	7.859994
5.656456	449.411642	7.864998
5.867492	455.699961	7.870003
5.944131	455.181776	7.875008
6.082001	452.306430	7.880013
6.184310	446.130447	7.885018
5.822877	456.770151	7.890022
6.267173	446.082737	7.895027
6.053491	451.621331	7.900032
6.038026	451.073284	7.905037
6.165194	449.443003	7.910042
5.934081	448.662983	7.915046
5.885445	449.686232	7.920051
5.851120	447.179562	7.925056
5.890649	458.253165	7.930061
6.524680	455.230474	7.935066
5.899318	443.805801	7.940070
5.986379	438.527575	7.945075
5.701071	430.321036	7.950080
5.509805	427.060655	7.955085
5.756792	434.583556	7.960090
5.623255	443.263934	7.965094
6.123871	439.828703	7.970099
5.873851	457.775232	7.975104
5.794339	452.776208	7.980109
5.705899	456.409533	7.985114
5.613221	456.936634	7.990118
5.946055	451.849540	7.995136
5.603208	453.875650	8.000154
5.939650	450.004496	8.005171
5.887663	453.484022	8.010189
5.567863	462.471300	8.015206
5.538626	460.030199	8.020224
5.793553	460.451036	8.025242
5.887008	451.369912	8.030259
5.821583	457.338288	8.035277
5.963565	478.062106	8.040294
6.121807	463.700688	8.045312
5.966841	460.278908	8.050330
6.163415	461.456805	8.055347
5.736399	464.957225	8.060365
5.613456	469.154764	8.065382
6.269169	475.590817	8.070400
6.167787	481.164053	8.075418
6.123900	481.707448	8.080435
6.057414	462.843243	8.085453
5.623095	465.331805	8.090470
5.912365	470.446202	8.095488
6.260028	479.644486	8.100506
6.202534	483.655050	8.105523
5.680187	473.941417	8.110541
6.115790	486.534158	8.115558
6.379574	481.008133	8.120576
5.712560	482.090970	8.125594
5.675398	484.801327	8.130611
6.530907	479.501322	8.135629
5.991362	483.218191	8.140646
5.965296	485.557584	8.145664
6.022649	486.640533	8.150682
5.925962	489.454890	8.155699
6.247300	478.996843	8.160717
5.894204	490.823235	8.165734
5.978303	480.560148	8.170752
6.169559	487.453983	8.175770
6.013535	487.001945	8.180787
5.912013	483.871584	8.185805
5.862061	487.559079	8.190822
5.861574	474.039868	8.195840
5.984435	475.674279	8.200858
5.715324	475.915296	8.205875
5.733163	471.096833	8.210893
5.725096	494.343550	8.215910
6.451556	498.767767	8.220928
6.322923	504.291631	8.225946
6.163835	494.779844	8.230963
6.149060	488.442248	8.235981
5.848761	486.024679	8.240998
6.165164	495.060612	8.246016
6.639083	505.684472	8.251034
6.230869	494.469730	8.256051
6.293862	489.192912	8.261069
6.344671	494.593985	8.266086
6.276080	481.006545	8.271104
6.405210	478.019925	8.276122
6.086284	476.914921	8.281139
6.362569	476.338344	8.286157
6.278314	476.752366	8.291174
6.464139	473.971456	8.296192
6.325661	475.864563	8.301210
6.019468	489.299360	8.306227
6.430891	475.163348	8.311245
6.100315	483.025715	8.316262
6.333500	484.788007	8.321280
6.374385	493.134969	8.326298
6.273328	486.933968	8.331315
6.162565	485.597534	8.336333
6.219374	489.053709	8.341350
6.380048	486.728013	8.346368
6.237672	487.861191	8.351386
6.255069	483.285789	8.356403
6.059651	484.607156	8.361421
6.253123	486.214726	8.366438
6.587795	480.535584	8.371456
6.318980	477.188443	8.376474
6.352458	496.070533	8.381491
6.598188	481.515514	8.386509
6.010943	491.207423	8.391526
6.189456	484.224168	8.396544
6.378511	472.417246	8.401562
5.729557	484.444623	8.406579
6.116343	480.003847	8.411597
6.297999	495.615431	8.416614
6.407047	507.975333	8.421632
6.496550	509.365668	8.426650
6.587041	513.700188	8.431667
5.993129	501.428950	8.436685
6.473090	499.753808	8.441702
5.990874	506.472308	8.446720
6.254277	508.769505	8.451738
6.319034	512.587354	8.456755
6.698816	513.171665	8.461773
6.348037	509.881540	8.466790
6.305737	518.374091	8.471808
6.419912	516.844621	8.476826
6.201181	527.782146	8.481843
6.122470	514.540246	8.486861
6.056793	516.519780	8.491878
6.175292	514.042900	8.496896
6.221237	509.917450	8.501914
6.120148	513.193244	8.506931
6.390518	518.884967	8.511949
6.400025	521.316621	8.516966
6.428289	535.652094	8.521984
6.504174	534.542030	8.527002
6.418027	541.094344	8.532019
6.817411	536.061449	8.537037
6.582514	524.563915	8.542054
6.836546	523.141918	8.547072
6.722059	510.855516	8.552090
6.477232	514.725028	8.557107
6.695418	516.107823	8.562125
6.402635	517.482318	8.567143
6.413007	520.324087	8.572160
6.611461	519.668186	8.577178
6.343317	520.969393	8.582195
6.455111	520.992939	8.587213
6.375187	519.803148	8.592231
6.666315	521.417510	8.597248
6.759537	523.072349	8.602266
6.528800	522.508941	8.607283
6.428357	522.994928	8.612301
6.298620	517.890309	8.617319
6.504886	528.350993	8.622336
7.009136	532.226216	8.627354
6.638832	529.904815	8.632371
6.669630	512.858823	8.637389
6.827037	516.854658	8.642407
6.590990	508.513092	8.647424
6.627705	510.227275	8.652442
6.561209	514.270815	8.657459
6.503129	510.256337	8.662477
6.771464	509.106653	8.667495
6.370450	514.723691	8.672512
6.549378	511.189625	8.677530
6.580306	524.691547	8.682547
6.845339	532.287046	8.687565
6.867435	528.152705	8.692583
6.994186	520.937706	8.697600
6.532480	510.596019	8.702618
6.844373	517.316331	8.707635
6.996824	511.328063	8.712653
6.499960	512.043418	8.717671
6.490142	518.255564	8.722688
6.744695	510.228445	8.727706
6.202935	512.594994	8.732723
6.762725	517.916325	8.737741
6.862857	524.575145	8.742759
6.612994	518.621508	8.747776
6.612080	518.792101	8.752794
6.587102	533.501985	8.757811
6.892141	542.807965	8.762829
6.820565	540.326149	8.767847
6.535474	535.943294	8.772864
6.882721	534.424642	8.777882
6.916927	547.358026	8.782899
6.574879	534.520287	8.787917
7.071440	540.296497	8.792935
6.664881	531.542983	8.797952
7.123812	527.220278	8.802970
6.605752	532.246595	8.807987
6.360721	528.182510	8.813005
6.629537	535.698523	8.818023
6.540356	542.967676	8.823040
7.255503	542.000446	8.828058
6.805794	538.896228	8.833075
6.903940	544.179446	8.838093
6.981316	548.860010	8.843111
6.707352	545.112878	8.848128
7.048670	542.616861	8.853146
7.066823	549.149681	8.858163
6.914255	548.204798	8.863181
6.872488	544.506490	8.868199
6.697843	545.998175	8.873216
7.141181	546.761876	8.878234
6.794720	536.973314	8.883251
7.127036	539.004099	8.888269
7.004480	523.601040	8.893287
6.280392	516.459396	8.898304
6.930136	538.473334	8.903322
6.811498	546.895808	8.908339
6.797341	535.685570	8.913357
7.213599	532.635018	8.918375
6.921926	538.206529	8.923392
7.323183	537.985907	8.928410
7.093742	543.601317	8.933427
6.978603	528.553696	8.938445
6.998370	521.162957	8.943463
6.714175	525.041795	8.948480
7.045646	520.631766	8.953498
6.677944	533.643892	8.958515
7.248658	542.576888	8.963533
7.052999	533.683032	8.968551
6.850692	545.145009	8.973568
7.076656	534.395763	8.978586
6.789249	541.061662	8.983603
6.772676	537.678142	8.988621
6.916547	542.218898	8.993639
7.085747	537.818511	8.998656
7.365550	536.840597	9.003674
7.042555	549.006292	9.008691
6.869440	544.656383	9.013709
6.908817	539.332757	9.018727
6.697348	539.596301	9.023744
6.960491	521.235804	9.028762
6.857167	537.109825	9.033779
7.070015	529.275423	9.038797
6.983253	539.195052	9.043815
6.753562	544.239304	9.048832
6.969670	548.497347	9.053850
6.853156	542.617482	9.058867
6.854780	535.999591	9.063885
7.354874	535.564669	9.068903
6.898066	546.230241	9.073920
6.925960	547.829046	9.078938
7.180372	557.840394	9.083955
7.164655	556.381766	9.088973
6.939116	562.536210	9.093991
7.059869	565.821436	9.099008
7.191079	562.525209	9.104026
7.167004	568.370379	9.109043
7.121395	565.938140	9.114061
7.123298	567.105520	9.119079
7.058753	567.462808	9.124096
7.342203	561.756953	9.129114
7.097718	575.210548	9.134131
7.146763	567.666880	9.139149
7.215128	559.135584	9.144167
7.416597	564.860208	9.149184
7.131623	564.090704	9.154202
7.379012	568.255487	9.159219
7.175776	564.244806	9.164237
7.152708	570.216051	9.169255
7.294408	569.471211	9.174272
7.479862	568.504923	9.179290
7.267734	566.449067	9.184307
7.382147	575.567182	9.189325
7.464805	565.405257	9.194343
7.106918	566.272406	9.199360
7.721344	565.440875	9.204378
7.130623	554.481909	9.209395
6.808158	557.457884	9.214413
7.370908	556.432480	9.219431
7.386311	566.755835	9.224448
7.278676	557.450546	9.229466
7.383218	572.190660	9.234483
7.141474	575.456946	9.239501
7.687263	564.499781	9.244519
7.302325	571.335606	9.249536
7.443868	565.771905	9.254554
7.708627	568.996698	9.259571
7.414204	559.528172	9.264589
7.483373	555.806169	9.269607
7.011188	557.006805	9.274624
7.202027	561.312990	9.279642
7.608322	570.700949	9.284659
7.319021	574.094606	9.289677
7.447318	571.704545	9.294695
7.419944	574.306085	9.299712
7.726325	565.526055	9.304730
7.691040	562.984902	9.309747
7.033758	556.788977	9.314765
7.783423	551.395083	9.319783
7.428656	555.221869	9.324800
7.329334	546.619023	9.329818
7.232956	559.298323	9.334835
7.251159	575.358464	9.339853
7.561226	563.270591	9.344871
7.358922	570.661621	9.349888
7.566766	568.555741	9.354906
7.544889	566.154497	9.359923
7.069397	577.176463	9.364941
7.627064	566.637155	9.369959
7.379722	578.317648	9.374976
7.380287	570.608007	9.379994
7.066366	572.326642	9.385011
7.286684	572.014451	9.390029
7.581802	570.570234	9.395047
7.333289	574.538166	9.400064
7.550250	575.378362	9.405082
7.322281	572.270954	9.410099
7.136134	577.084333	9.415117
7.189801	576.340663	9.420135
7.183684	598.255467	9.425152
7.649385	599.006199	9.430170
8.047389	603.371453	9.435187
7.614197	604.026342	9.440205
7.670133	595.108813	9.445223
7.377156	592.803691	9.450240
7.623296	591.976215	9.455258
7.525634	592.676361	9.460275
7.806179	596.633986	9.465293
7.843726	601.816263	9.470311
7.708146	603.689995	9.475328
7.380996	597.849426	9.480346
7.458562	588.029111	9.485363
7.293645	599.800845	9.490381
7.748842	592.679522	9.495399
7.708550	601.862916	9.500416
7.552737	604.838033	9.505434
7.776898	601.975358	9.510451
7.102146	606.117377	9.515469
7.703273	606.853202	9.520487
7.575883	601.546221	9.525504
7.432884	603.067666	9.530522
7.383733	597.451782	9.535539
7.456069	603.654242	9.540557
7.622390	593.674851	9.545575
7.482687	612.565264	9.550592
7.581989	618.318537	9.555610
8.114795	622.634272	9.560627
8.005407	614.695688	9.565645
8.178139	603.661252	9.570663
7.796992	608.688228	9.575680
7.872952	605.075603	9.580698
7.591287	601.752542	9.585715
7.495132	604.787739	9.590733
7.713994	599.044656	9.595751
8.062988	603.449147	9.600768
7.967700	604.319335	9.605786
7.924436	596.341996	9.610803
7.997611	604.504071	9.615821
7.367297	601.062069	9.620839
7.675739	600.568812	9.625856
7.489683	617.393138	9.630874
7.971686	620.839522	9.635891
8.037583	624.303766	9.640909
7.978769	617.692159	9.645927
7.808215	624.690073	9.650944
8.004541	612.462199	9.655962
7.934942	612.015552	9.660979
7.864570	619.105064	9.665997
8.029822	607.841424	9.671015
7.817572	606.669204	9.676032
7.809198	618.978154	9.681050
7.818047	626.149931	9.686067
8.110381	627.921904	9.691085
7.963874	621.484980	9.696103
7.940080	619.279689	9.701120
7.996895	628.712968	9.706138
8.636612	617.097271	9.711155
7.750575	606.525369	9.716173
8.071611	600.741030	9.721191
7.892625	604.707541	9.726208
7.780099	598.767073	9.731226
7.890882	596.319793	9.736243
7.587785	614.039764	9.741261
8.001854	630.773229	9.746279
7.840380	629.239603	9.751296
7.916551	626.703068	9.756314
8.144575	629.163613	9.761331
7.600503	641.711147	9.766349
7.980686	635.936464	9.771367
8.031734	639.147419	9.776384
7.821769	633.834431	9.781402
8.164660	628.624169	9.786419
7.886742	632.994351	9.791437
8.385170	630.764039	9.796455
7.801592	628.832647	9.801472
7.861999	630.227550	9.806490
8.219835	626.788506	9.811507
7.934492	631.248213	9.816525
7.610036	628.790228	9.821543
7.781281	635.491596	9.826560
7.762913	655.379211	9.831578
8.604542	654.111291	9.836595
8.317845	656.358999	9.841613
8.297275	652.411196	9.846631
8.037500	647.238552	9.851648
7.884248	637.602698	9.856666
8.303869	651.362549	9.861683
8.569440	662.593503	9.866701
8.222429	639.780974	9.871719
8.262072	640.557438	9.876736
7.870834	637.740687	9.881754
7.893039	635.102154	9.886771
8.450068	647.237327	9.891789
8.414344	650.278843	9.896807
8.463401	648.273572	9.901824
8.184510	637.262539	9.906842
8.759555	625.133108	9.911859
8.469808	634.336669	9.916877
8.295350	629.459931	9.921895
8.479501	629.175496	9.926912
8.181799	625.406819	9.931930
8.623505	625.804707	9.936947
8.343858	631.279688	9.941965
8.516787	626.269626	9.946983
8.283597	625.902259	9.952000
8.431172	622.180580	9.957018
8.625280	617.599547	9.962035
8.122927	626.716496	9.967053
8.105873	625.365368	9.972071
8.430391	620.104339	9.977088
8.286200	628.287860	9.982106
8.459735	623.776320	9.987123
8.420759	635.676666	9.992141
8.315805	622.293632	9.997159
8.380624	630.693713	10.002176
8.101812	627.439627	10.007194
8.167998	623.052204	10.012211
8.325763	627.404613	10.017229
8.201649	624.101043	10.022247
8.604852	628.768446	10.027264
8.096726	625.042207	10.032282
8.255900	625.506453	10.037299
8.367195	634.445207	10.042317
8.624012	633.660237	10.047335
8.728417	627.070389	10.052352
8.516317	626.879598	10.057370
8.306385	628.130666	10.062387
8.105706	641.255555	10.067405
8.411105	638.720972	10.072423
8.639356	642.655243	10.077440
8.470351	649.122750	10.082458
8.678039	656.957660	10.087475
8.402013	650.913404	10.092493
8.518403	652.870738	10.097511
8.649908	653.692770	10.102528
8.548487	654.207315	10.107546
8.795201	653.733196	10.112563
8.366870	639.955848	10.117581
8.520302	643.346421	10.122599
8.833699	645.140342	10.127616
8.700276	648.260281	10.132634
8.579713	639.780639	10.137651
8.058803	638.732518	10.142669
8.440974	658.077697	10.147687
8.576513	664.096705	10.152704
8.375691	656.753096	10.157722
8.379454	660.832998	10.162739
8.634722	665.072309	10.167757
8.483063	662.947006	10.172775
8.838993	655.408867	10.177792
8.719246	657.488406	10.182810
8.519884	659.848663	10.187827
8.429624	667.136970	10.192845
8.669803	656.628420	10.197863
8.596785	657.028062	10.202880
8.135135	669.669999	10.207898
8.461047	662.051353	10.212915
8.687537	652.819895	10.217933
8.412041	658.549854	10.222951
8.883046	673.302061	10.227968
8.751589	682.973152	10.232986
8.725361	679.430172	10.238003
8.758927	681.665573	10.243021
8.673909	684.888388	10.248039
9.157903	688.637431	10.253056
8.749639	681.790218	10.258074
8.774691	674.310225	10.263091
9.053232	676.289492	10.268109
8.970006	661.807959	10.273127
8.956860	659.698824	10.278144
9.277227	657.180827	10.283162
8.992819	662.763861	10.288179
9.113118	655.833842	10.293197
8.981399	657.684883	10.298215
9.065937	659.808153	10.303232
8.970847	660.709871	10.308250
8.894838	657.038996	10.313267
9.397949	661.277343	10.318285
8.958228	661.078034	10.323303
8.969230	660.306332	10.328320
8.872698	669.227174	10.333338
8.906373	651.776655	10.338355
8.892584	653.735450	10.343373
8.720076	655.655998	10.348391
9.002097	663.296228	10.353408
8.680816	660.474824	10.358426
8.793077	661.492376	10.363443
8.713646	656.534470	10.368461
8.591314	661.432546	10.373479
8.483071	665.536309	10.378496
8.647639	658.208033	10.383514
8.621632	653.797178	10.388531
8.904437	662.863707	10.393549
8.665261	674.896433	10.398567
9.225666	670.655625	10.403584
8.874296	676.239688	10.408602
8.695089	685.782562	10.413619
9.244129	676.462683	10.418637
8.979457	681.294705	10.423655
9.104422	680.864908	10.428672
8.902236	694.005851	10.433690
8.975651	688.638978	10.438707
9.121845	687.893430	10.443725
9.157951	694.675954	10.448743
8.997127	683.498071	10.453760
8.983348	681.799288	10.458778
8.969105	676.752267	10.463795
9.120018	684.539281	10.468813
8.804455	688.467250	10.473831
9.133782	692.202657	10.478848
8.830926	686.547602	10.483866
9.118459	688.298243	10.488883
8.905048	689.660314	10.493901
8.741910	684.179028	10.498919
9.085355	684.709078	10.503936
9.381289	698.327399	10.508954
9.264012	695.467714	10.513971
9.162240	692.403627	10.518989
9.015192	692.180552	10.524007
9.256373	698.069411	10.529024
8.955215	705.488608	10.534042
9.168668	720.407440	10.539059
9.364279	726.300292	10.544077
9.282091	724.501770	10.549095
9.472212	721.906342	10.554112
9.474228	722.420461	10.559130
9.185420	701.930880	10.564147
9.333363	703.252113	10.569165
8.969225	703.779420	10.574183
9.445335	708.110372	10.579200
9.323598	713.955113	10.584218
9.718302	721.719724	10.589235
9.223656	705.147198	10.594253
9.069261	695.656659	10.599271
9.445718	702.259627	10.604288
9.135324	719.166646	10.609306
9.313079	711.138847	10.614323
9.568489	715.952506	10.619341
9.514464	720.511691	10.624359
9.624888	713.008839	10.629376
9.294481	705.117467	10.634394
9.597759	706.187144	10.639411
9.386426	689.059000	10.644429
9.386834	691.290131	10.649447
9.472800	683.712227	10.654464
9.460299	688.015589	10.659482
9.370180	695.234458	10.664499
9.191848	702.170506	10.669517
9.326965	722.510674	10.674535
9.503545	716.190352	10.679552
9.459156	712.602874	10.684570
9.330711	713.680234	10.689587
9.720147	716.576250	10.694605
9.810178	722.905367	10.699623
9.614559	711.142781	10.704640
9.373447	713.995582	10.709658
9.576805	709.741280	10.714675
9.501703	712.170437	10.719693
9.595834	711.366773	10.724711
9.790748	705.176126	10.729728
9.241829	700.023525	10.734746
9.393537	704.083411	10.739763
9.517159	702.703925	10.744781
9.457434	710.318826	10.749799
9.662158	712.104534	10.754816
9.683521	717.567093	10.759834
9.570115	713.169917	10.764851
9.505836	714.704284	10.769869
9.162262	708.332920	10.774887
9.420190	712.388789	10.779904
9.632246	713.630549	10.784922
9.560868	713.102126	10.789939
9.900753	716.905313	10.794957
9.543876	727.296558	10.799975
9.889315	714.215272	10.804992
9.781618	713.802994	10.810010
9.432927	728.147190	10.815027
9.765365	714.752359	10.820045
9.428778	714.943990	10.825063
9.607579	718.087605	10.830080
9.640570	716.981095	10.835098
9.649192	716.263412	10.840115
9.870068	716.124700	10.845133
9.651814	714.975505	10.850151
9.625381	715.052268	10.855168
9.787039	715.901137	10.860186
9.591812	726.674153	10.865203
9.647744	728.035051	10.870221
9.841582	733.836665	10.875239
9.815722	740.897161	10.880256
9.635771	731.173921	10.885274
9.675176	740.130303	10.890291
9.846579	739.030507	10.895309
9.831059	742.097275	10.900327
10.036251	736.959050	10.905344
10.403681	725.250247	10.910362
10.031088	727.066452	10.915379
10.251285	709.675015	10.920397
9.863887	718.638299	10.925415
9.603678	711.761565	10.930432
9.791268	713.373233	10.935450
9.823450	729.929940	10.940467
9.997254	725.525630	10.945485
9.862814	739.877293	10.950503
9.831103	730.613666	10.955520
9.823734	729.573439	10.960538
9.745143	738.980656	10.965555
9.893772	730.373585	10.970573
10.019444	739.654123	10.975591
9.978365	740.569473	10.980608
10.598836	736.009968	10.985626
9.585173	745.986577	10.990643
10.164528	734.231939	10.995661
10.077402	746.802625	11.000679
9.872546	741.106951	11.005696
10.199608	735.469947	11.010714
9.526961	744.156044	11.015731
10.076210	738.272787	11.020749
9.532794	742.223845	11.025767
10.111922	753.172197	11.030784
10.317624	749.365645	11.035802
10.179228	747.026814	11.040819
10.172396	745.768751	11.045837
10.055628	743.814698	11.050855
10.100853	743.056565	11.055872
10.542864	746.061114	11.060890
10.453460	743.077132	11.065907
10.642067	735.811330	11.070925
10.364586	736.091530	11.075943
10.336887	741.482888	11.080960
10.503030	743.416656	11.085978
9.880297	730.143071	11.090995
10.317154	723.987093	11.096013
10.197814	728.676435	11.101031
9.980644	738.622918	11.106048
10.122476	737.833870	11.111066
10.194606	741.669547	11.116083
10.255985	740.265096	11.121101
10.319134	744.092714	11.126119
10.101705	749.851474	11.131136
10.314046	743.036387	11.136154
9.919128	745.004416	11.141171
10.082308	743.662910	11.146189
10.248698	741.680270	11.151207
10.058618	743.657230	11.156224
10.203608	743.397864	11.161242
10.233465	746.419653	11.166259
10.573175	743.513604	11.171277
10.169515	748.632510	11.176295
10.040550	744.973070	11.181312
10.485326	744.158645	11.186330
10.337239	744.727842	11.191347
10.109197	734.488270	11.196365
10.273122	750.270114	11.201383
10.528274	762.875545	11.206400
10.743306	760.733802	11.211418
10.641903	759.285427	11.216435
10.343898	745.847340	11.221453
10.385101	744.575439	11.226471
9.869440	745.214852	11.231488
10.066229	756.668082	11.236506
10.107324	765.879834	11.241523
10.283829	762.065230	11.246541
10.481288	758.701783	11.251559
10.493613	763.200090	11.256576
10.673891	761.893774	11.261594
10.653351	765.160149	11.266611
10.489642	758.678534	11.271629
10.600456	763.660029	11.276647
10.936020	764.557392	11.281664
10.681454	765.859645	11.286682
10.667769	763.545453	11.291699
10.687336	764.255641	11.296717
10.894838	759.205411	11.301735
10.934863	765.211017	11.306752
11.133200	764.157492	11.311770
10.673036	755.415423	11.316787
10.653843	742.511169	11.321805
10.555465	739.717943	11.326823
10.443565	755.413620	11.331840
10.853785	743.272064	11.336858
10.744991	746.337669	11.341875
10.591529	732.624479	11.346893
10.879162	747.017313	11.351911
10.435933	744.843011	11.356928
10.935471	743.827501	11.361946
10.877312	751.517914	11.366963
10.666564	748.833812	11.371981
10.733299	740.996964	11.376999
10.585524	760.624104	11.382016
10.769827	753.835498	11.387034
10.739542	767.820567	11.392051
10.874145	767.584919	11.397069
11.118496	766.921818	11.402087
10.912640	761.513474	11.407104
10.859034	740.844983	11.412122
10.555693	742.571444	11.417139
10.700078	744.805269	11.422157
11.235455	756.404265	11.427175
10.858314	754.478383	11.432192
10.806941	743.463195	11.437210
10.287622	749.490163	11.442227
10.701498	758.062832	11.447245
10.847363	763.114575	11.452263
10.716241	760.130815	11.457280
10.992636	757.850070	11.462298
10.503341	757.311387	11.467315
10.443118	756.509815	11.472333
10.835208	755.599503	11.477351
10.894780	758.023344	11.482368
11.047580	760.972224	11.487386
10.334463	757.101349	11.492403
10.417249	754.816225	11.497421
10.955296	768.775364	11.502439
10.531036	783.642688	11.507456
11.286530	773.463586	11.512474
11.009795	781.450192	11.517491
10.870280	779.209363	11.522509
11.167411	778.885133	11.527527
11.074377	790.434288	11.532544
10.910006	783.564601	11.537562
10.826706	788.911036	11.542579
10.769186	780.563461	11.547597
11.149973	779.796931	11.552615
10.721014	793.364800	11.557632
11.245418	788.615206	11.562650
11.046962	789.798215	11.567667
11.068562	787.513206	11.572685
11.041467	776.721413	11.577703
11.062374	782.026271	11.582720
11.238746	771.846389	11.587738
11.211613	775.890132	11.592755
11.156906	780.313739	11.597773
11.453718	775.066474	11.602791
11.234810	794.692173	11.607808
11.315758	787.310673	11.612826
11.184116	793.283225	11.617843
10.979675	795.312933	11.622861
11.204146	781.139701	11.627879
11.039649	795.275209	11.632896
11.283482	802.280850	11.637914
11.653308	809.746438	11.642931
11.296618	803.926209	11.647949
11.284254	785.065807	11.652967
11.425124	790.266665	11.657984
11.394116	785.373719	11.663002
11.358611	781.772212	11.668019
11.330028	788.075755	11.673037
11.194128	784.164928	11.678055
10.917009	794.417482	11.683072
11.550217	802.469809	11.688090
11.374213	807.527815	11.693107
11.579361	811.251146	11.698125
11.534245	807.190389	11.703143
11.436235	816.281949	11.708160
11.838723	809.983004	11.713178
11.560540	804.178877	11.718195
10.945178	792.201135	11.723213
11.352466	793.415468	11.728231
11.639046	809.702013	11.733248
11.940662	794.421611	11.738266
11.475601	797.823913	11.743283
11.149820	780.890340	11.748301
11.435374	793.879196	11.753319
11.660185	806.413672	11.758336
11.917069	800.797111	11.763354
11.538513	792.925868	11.768371
11.288488	787.925226	11.773389
11.818997	798.354201	11.778407
11.446102	785.792515	11.783424
11.875498	792.639688	11.788442
11.423208	793.606846	11.793459
11.350011	791.368248	11.798477
11.659238	804.934075	11.803495
11.606077	808.833580	11.808512
11.697672	814.389306	11.813530
11.875658	814.673883	11.818547
12.029684	807.041082	11.823565
11.886493	789.258377	11.828583
11.813018	791.854548	11.833600
11.733539	783.781814	11.838618
11.696681	779.678743	11.843635
11.453948	790.901057	11.848653
11.739070	787.426038	11.853671
11.714126	780.032730	11.858688
11.411433	779.818261	11.863706
11.515125	793.697152	11.868723
11.522646	809.516177	11.873741
12.011705	801.865599	11.878759
11.782115	813.543463	11.883776
11.518642	804.205658	11.888794
11.920463	815.071374	11.893811
11.657528	813.427396	11.898829
11.816341	814.191508	11.903847
11.485764	815.833880	11.908864
11.711435	812.740559	11.913882
11.954622	810.345089	11.918899
11.529109	813.592874	11.923917
11.498989	806.282418	11.928935
11.661765	816.235685	11.933952
11.571302	812.374537	11.938970
11.984892	827.729164	11.943987
11.984358	835.268572	11.949005
12.188878	842.602283	11.954023
11.835645	840.562191	11.959040
12.096453	830.309086	11.964058
12.143198	838.705785	11.969075
11.854439	835.437440	11.974093
11.775284	831.852230	11.979111
11.746704	842.425634	11.984128
11.645786	838.509314	11.989146
12.320925	837.368455	11.994163
12.343798	849.009942	11.999181
12.310568	843.640797	12.004199
11.872526	832.581996	12.009216
12.033865	835.141383	12.014234
12.508928	835.161661	12.019251
12.384340	830.662066	12.024269
12.389501	819.751583	12.029287
12.169628	818.839321	12.034304
12.054883	809.844286	12.039322
12.174149	809.689936	12.044339
11.899474	811.629665	12.049357
11.857684	827.873002	12.054375
12.154900	830.376384	12.059392
12.097885	837.277696	12.064410
12.186985	840.548997	12.069427
12.090818	838.894666	12.074445
11.738768	833.206245	12.079463
11.942658	832.173938	12.084480
12.277115	840.421416	12.089498
12.384029	845.289935	12.094515
12.067890	843.512277	12.099533
12.201546	838.539868	12.104551
12.000410	842.301618	12.109568
11.927920	832.230122	12.114586
12.422062	831.105000	12.119603
12.290662	839.371820	12.124621
12.240723	840.465289	12.129639
12.470185	847.119746	12.134656
12.297239	855.686575	12.139674
12.220769	849.939192	12.144691
12.478695	854.862949	12.149709
12.572457	864.000227	12.154727
12.567418	855.518160	12.159744
12.463087	837.031879	12.164762
12.490679	841.376333	12.169779
12.097152	848.469232	12.174797
12.448034	849.540926	12.179815
12.505055	861.132888	12.184832
12.565650	861.940794	12.189850
12.767363	857.345885	12.194867
12.508696	855.079534	12.199885
12.627472	842.428148	12.204903
12.434160	832.252506	12.209920
12.199518	833.924030	12.214938
12.736916	848.334617	12.219955
12.962394	850.337996	12.224973
12.926890	837.534060	12.229991
12.554206	837.598803	12.235008
12.446114	834.122268	12.240026
12.423638	830.777488	12.245043
12.480748	832.135054	12.250061
12.913220	833.048795	12.255079
12.771036	843.630533	12.260096
12.943680	842.192861	12.265114
12.754730	832.919104	12.270131
12.492956	842.642258	12.275149
12.734810	834.998840	12.280167
12.698124	833.332033	12.285184
12.677050	841.944489	12.290202
12.544939	835.375844	12.295219
12.652107	837.596577	12.300237
12.657798	840.174040	12.305255
12.709804	839.547385	12.310272
12.908830	852.736036	12.315290
13.028043	849.479506	12.320307
12.795167	842.270232	12.325325
12.743400	831.400220	12.330343
12.913124	837.085724	12.335360
12.736622	836.718937	12.340378
12.775759	832.947933	12.345395
12.764278	846.762859	12.350413
12.931214	857.169937	12.355431
12.968736	853.421273	12.360448
12.633711	860.744854	12.365466
12.998385	852.419458	12.370483
13.034921	858.772784	12.375501
13.062513	853.488782	12.380519
13.141326	850.592036	12.385536
12.744377	855.328064	12.390554
12.868977	854.134607	12.395571
12.801505	858.629662	12.400589
13.045440	854.952798	12.405607
12.931616	855.238916	12.410624
12.830052	859.458443	12.415642
13.406479	846.732193	12.420659
13.007289	860.440617	12.425677
13.380078	856.210227	12.430695
13.146997	859.891778	12.435712
12.824157	853.542360	12.440730
12.950700	848.034570	12.445747
13.085218	856.316538	12.450765
12.883609	855.243621	12.455783
13.299269	857.693735	12.460800
13.120020	863.033134	12.465818
13.434242	849.073006	12.470835
13.193122	853.213411	12.475853
13.055121	859.707694	12.480871
13.186862	855.997916	12.485888
12.869851	866.231515	12.490906
13.143905	852.164068	12.495923
12.819731	863.673746	12.500941
12.894792	859.938133	12.505959
13.051984	852.607777	12.510976
12.835730	861.358122	12.515994
13.255956	852.534868	12.521011
13.165611	861.700991	12.526029
13.386421	872.184845	12.531047
13.357797	862.093836	12.536064
13.065296	883.851888	12.541082
13.213713	882.089802	12.546099
13.228318	883.312018	12.551117
13.387340	882.378257	12.556135
13.398195	886.179384	12.561152
13.354603	891.478602	12.566170
13.734637	884.312135	12.571187
13.510910	888.112148	12.576205
13.497475	888.505615	12.581223
13.627104	889.021836	12.586240
13.695073	883.854576	12.591258
13.130520	866.945709	12.596275
13.442618	863.438047	12.601293
13.769557	876.672946	12.606311
13.766857	864.154188	12.611328
13.538278	855.407342	12.616346
13.561378	850.979277	12.621363
13.169171	857.567038	12.626381
13.366995	874.445068	12.631399
13.775214	875.731845	12.636416
13.533913	880.235206	12.641434
13.677026	877.530355	12.646451
13.669697	879.832150	12.651469
13.523458	874.348157	12.656487
13.915357	879.822137	12.661504
13.710131	870.793910	12.666522
13.510614	859.975433	12.671539
14.077611	871.033057	12.676557
13.154355	867.030979	12.681575
13.746440	860.001713	12.686592
13.822177	882.727714	12.691610
13.804478	880.524591	12.696627
13.804320	888.382702	12.701645
13.585327	873.726607	12.706663
14.099531	870.565977	12.711680
13.868258	868.276397	12.716698
13.767982	853.658523	12.721715
13.735927	861.556334	12.726733
13.930393	854.557812	12.731751
13.717158	850.851593	12.736768
13.286096	859.200088	12.741786
13.726315	867.301618	12.746803
13.900022	867.804620	12.751821
13.870404	868.475181	12.756839
13.983071	871.894275	12.761856
13.793081	875.180909	12.766874
13.979806	874.678314	12.771891
14.320684	880.147664	12.776909
14.220234	876.789846	12.781927
14.293401	874.061241	12.786944
13.405279	870.602773	12.791962
13.763542	872.320260	12.796979
13.921574	876.363416	12.801997
14.034691	879.523662	12.807015
14.558891	880.334670	12.812032
13.962073	877.676325	12.817050
13.878028	877.664284	12.822067
13.990180	875.052648	12.827085
13.455190	881.811114	12.832103
13.916246	874.982256	12.837120
13.968294	881.544601	12.842138
14.087057	879.190707	12.847155
14.425556	870.591690	12.852173
13.827293	881.948663	12.857191
14.127288	885.534071	12.862208
14.015178	891.588803	12.867226
13.821290	888.766337	12.872243
13.817361	879.561397	12.877261
13.860309	890.205675	12.882279
14.411584	904.898160	12.887296
14.567232	900.872198	12.892314
14.126767	885.663806	12.897331
14.213953	877.574383	12.902349
14.244663	878.251271	12.907367
14.428893	881.027986	12.912384
14.234609	890.977280	12.917402
13.975302	884.851428	12.922419
13.998287	896.912656	12.927437
14.013556	902.155316	12.932455
14.138743	902.571246	12.937472
14.285254	905.265511	12.942490
14.365556	907.736618	12.947507
14.977925	901.010276	12.952525
14.637547	898.709384	12.957543
14.860886	896.436934	12.962560
14.742454	899.731295	12.967578
14.384419	886.962079	12.972595
14.526009	886.236179	12.977613
14.375088	895.676902	12.982631
14.371373	896.955639	12.987648
14.381052	912.521950	12.992666
14.777202	904.576612	12.997683
14.760601	908.309461	13.002701
14.608963	899.714642	13.007719
14.602596	889.396066	13.012736
14.554752	876.240581	13.017754
14.308766	884.121428	13.022771
14.856201	888.097262	13.027789
14.738262	888.052662	13.032807
14.705778	880.976078	13.037824
14.630806	875.439893	13.042842
14.487764	882.600857	13.047859
14.650154	886.056345	13.052877
14.477937	894.657794	13.057895
14.656849	894.165890	13.062912
14.696916	903.298978	13.067930
14.682161	904.835069	13.072947
14.585294	901.798580	13.077965
14.806234	901.543092	13.082983
14.749611	904.234470	13.088000
14.630979	906.645227	13.093018
14.724262	900.697658	13.098035
14.852620	893.273972	13.103053
14.837314	906.609855	13.108071
14.842205	904.583073	13.113088
14.516441	901.295267	13.118106
14.744321	899.997262	13.123123
14.515853	902.150669	13.128141
14.731464	900.785157	13.133159
14.550608	895.858855	13.138176
14.649122	898.917250	13.143194
14.733901	912.972768	13.148211
15.113427	912.818665	13.153229
15.096903	905.483948	13.158247
14.915959	905.010556	13.163264
14.669139	912.847365	13.168282
15.092436	918.000852	13.173299
15.357945	924.454027	13.178317
14.820667	920.590279	13.183335
15.074508	915.933537	13.188352
14.701525	926.643006	13.193370
14.880083	934.346901	13.198387
15.303507	925.340071	13.203405
14.933666	927.411488	13.208423
15.127121	925.645497	13.213440
15.088805	926.169098	13.218458
14.978816	926.697617	13.223475
15.333134	919.838127	13.228493
14.790395	933.742671	13.233511
14.979005	919.631753	13.238528
15.106705	923.367243	13.243546
15.236625	930.362379	13.248563
15.295217	927.049061	13.253581
15.052160	923.079253	13.258599
15.451351	921.890106	13.263616
15.454545	920.475822	13.268634
15.148886	932.601190	13.273651
15.321607	925.451411	13.278669
15.225475	923.724481	13.283687
15.522511	918.256230	13.288704
15.395891	918.885186	13.293722
15.368807	925.611426	13.298739
15.683445	923.233148	13.303757
15.344323	919.060638	13.308775
15.257670	917.202835	13.313792
14.934989	919.086979	13.318810
15.308890	914.136868	13.323827
15.684822	916.466981	13.328845
15.241298	922.346429	13.333863
15.780017	909.316769	13.338880
15.503828	916.198803	13.343898
15.427529	921.017153	13.348915
15.728751	912.739541	13.353933
15.349002	914.727302	13.358951
15.917203	916.755887	13.363968
15.554092	912.637631	13.368986
15.016105	919.819464	13.374003
15.435263	922.341624	13.379021
15.238335	925.594639	13.384039
15.573255	934.640518	13.389056
15.538220	941.222841	13.394074
15.058356	942.765537	13.399091
15.398805	945.887020	13.404109
15.397417	941.443835	13.409127
15.675783	950.208244	13.414144
15.629864	941.334905	13.419162
15.757041	955.099786	13.424179
15.829406	949.912884	13.429197
15.559478	951.974961	13.434215
15.456611	945.319641	13.439232
15.519792	942.453732	13.444250
15.447810	944.200767	13.449267
15.670554	956.385373	13.454285
15.879559	960.104976	13.459303
16.075123	967.815689	13.464320
16.147856	962.108009	13.469338
16.048765	963.729903	13.474355
15.858117	951.000688	13.479373
16.009715	946.091711	13.484391
15.764720	947.064267	13.489408
16.081799	941.731726	13.494426
16.065260	941.917395	13.499443
16.072304	937.722201	13.504461
15.836880	945.869667	13.509479
15.938261	941.056923	13.514496
16.333302	930.628092	13.519514
15.845042	935.267992	13.524531
16.180634	930.563724	13.529549
16.237370	926.682643	13.534567
16.271936	931.840237	13.539584
16.269486	934.011884	13.544602
16.212942	937.400698	13.549619
16.445179	938.090195	13.554637
16.290116	945.540250	13.559655
16.506916	931.961400	13.564672
16.256307	935.604686	13.569690
16.123402	936.821616	13.574707
16.385505	938.964436	13.579725
15.930836	945.524146	13.584743
15.657204	940.019068	13.589760
16.257911	935.443675	13.594778
15.855679	945.810594	13.599795
16.044442	939.526155	13.604813
16.173149	946.382631	13.609831
15.961186	942.691972	13.614848
16.187678	955.298874	13.619866
16.042080	960.506796	13.624883
16.222705	967.288871	13.629901
16.240230	966.737044	13.634919
16.443847	963.050696	13.639936
16.281408	968.352778	13.644954
16.179267	978.855737	13.649971
16.674420	971.450289	13.654989
16.739146	974.697031	13.660007
16.497580	970.736446	13.665024
17.041508	964.408974	13.670042
16.651859	967.793180	13.675059
16.570966	966.180626	13.680077
16.574829	962.358315	13.685095
16.575109	962.494011	13.690112
16.816139	963.567145	13.695130
16.481269	944.895963	13.700147
16.450534	948.227086	13.705165
16.250208	950.571752	13.710183
16.452612	960.436839	13.715200
16.923333	963.171835	13.720218
16.636863	967.079527	13.725235
16.783838	960.293535	13.730253
16.699767	971.027192	13.735271
16.491956	968.232141	13.740288
16.669632	959.519422	13.745306
16.471448	966.780579	13.750323
16.891725	970.706927	13.755341
16.983292	967.123343	13.760359
16.943762	969.004153	13.765376
16.887390	972.689598	13.770394
16.416923	963.134829	13.775411
16.773103	958.973290	13.780429
16.929447	955.057662	13.785447
17.032057	961.479568	13.790464
17.340354	960.879026	13.795482
17.164306	956.598904	13.800499
16.906501	952.382087	13.805517
16.842467	950.000020	13.810535
16.764972	952.716767	13.815552
17.211159	962.161800	13.820570
16.851993	962.984985	13.825587
17.273642	959.889336	13.830605
17.221757	955.031174	13.835623
16.881368	940.763279	13.840640
17.363271	936.541021	13.845658
17.183070	932.652881	13.850675
16.844960	927.946872	13.855693
16.794994	931.659707	13.860711
17.051255	924.522085	13.865728
17.393020	928.227192	13.870746
17.428701	935.006719	13.875763
17.205877	938.061820	13.880781
16.870150	933.724670	13.885799
16.888253	942.072256	13.890816
17.322272	938.627528	13.895834
17.229005	948.712507	13.900851
16.898646	944.336643	13.905869
17.165122	941.372609	13.910887
17.225215	955.381535	13.915904
17.604332	939.795370	13.920922
17.054387	952.482898	13.925939
17.442551	944.046481	13.930957
17.414327	949.201294	13.935975
17.420384	956.395732	13.940992
17.833686	951.385788	13.946010
17.379557	934.607879	13.951027
17.343176	937.677950	13.956045
17.193706	926.668551	13.961063
17.150022	931.936236	13.966080
16.892785	941.772343	13.971098
17.370577	950.694858	13.976115
17.485137	958.462441	13.981133
16.969535	952.954244	13.986151
17.256280	954.594581	13.991168
17.350896	950.688625	13.996186
17.467877	956.824251	14.001203
17.638477	956.273686	14.006221
17.281371	949.765498	14.011239
17.415046	956.529679	14.016256
17.609833	946.327878	14.021274
17.588354	959.816249	14.026291
17.836598	969.570015	14.031309
17.832604	964.773775	14.036327
17.486909	944.643128	14.041344
17.651906	960.005261	14.046362
17.767652	956.629333	14.051379
17.807362	963.269382	14.056397
17.764759	960.811371	14.061415
17.281819	961.862236	14.066432
17.578938	977.200527	14.071450
17.690543	970.767218	14.076467
17.929039	979.477928	14.081485
18.069793	979.787277	14.086503
17.889925	977.369706	14.091520
17.821359	973.994250	14.096538
17.713448	981.275983	14.101555
17.610704	972.231648	14.106573
17.724789	978.809555	14.111591
17.839345	985.731380	14.116608
17.943430	976.152855	14.121626
17.568774	978.215565	14.126643
17.842442	979.267807	14.131661
17.998831	976.974278	14.136679
17.715153	985.564832	14.141696
17.759281	976.948770	14.146714
17.577143	980.997910	14.151731
17.893781	996.449926	14.156749
17.909133	992.540601	14.161767
17.867141	1006.404613	14.166784
18.246574	995.110327	14.171802
18.095669	1001.944361	14.176819
18.161477	999.605060	14.181837
18.405960	1002.975124	14.186855
18.545666	1003.455055	14.191872
18.629858	998.790159	14.196890
18.450507	996.836416	14.201907
18.184989	987.075949	14.206925
18.294666	979.579413	14.211943
17.882518	969.122394	14.216960
17.802725	979.000148	14.221978
18.317314	994.560005	14.226995
18.197299	1001.016807	14.232013
18.539405	993.562745	14.237031
18.344288	995.114479	14.242048
18.470023	991.443484	14.247066
18.358759	998.369138	14.252083
18.213250	1000.616857	14.257101
18.224957	996.083242	14.262119
18.071628	1003.700310	14.267136
18.077816	1000.363630	14.272154
18.181253	1008.770462	14.277171
18.203782	992.646820	14.282189
18.543738	999.119917	14.287207
18.584373	1018.885080	14.292224
18.365448	1017.773840	14.297242
18.781216	1024.951449	14.302259
18.791528	1022.137993	14.307277
18.610951	1011.297521	14.312295
18.500296	1000.316710	14.317312
18.470431	1009.823733	14.322330
18.675275	1021.657731	14.327347
18.744387	1018.484762	14.332365
19.061934	1016.292213	14.337383
18.749562	1000.110582	14.342400
19.187015	999.221554	14.347418
19.054944	998.339708	14.352435
18.633937	995.325588	14.357453
19.011765	987.244227	14.362471
18.641654	989.839566	14.367488
18.646680	987.115308	14.372506
19.176795	987.246885	14.377523
18.576093	1000.456805	14.382541
18.910525	990.592867	14.387559
18.779100	993.554760	14.392576
19.400407	992.299249	14.397594
19.123063	986.933595	14.402611
18.890366	981.488362	14.407629
18.752204	985.729433	14.412647
19.207919	993.670800	14.417664
18.726746	990.325275	14.422682
19.206757	983.477626	14.427699
18.635456	992.870655	14.432717
18.960889	981.322902	14.437735
19.076409	998.510596	14.442752
19.577064	1008.357381	14.447770
18.915106	1002.446059	14.452787
19.034835	986.398713	14.457805
19.044077	992.358725	14.462823
19.109062	993.374235	14.467840
18.927417	1011.198648	14.472858
19.283266	1008.564589	14.477875
19.368179	1017.864282	14.482893
19.387449	1012.966552	14.487911
19.073162	1010.671025	14.492928
19.315360	1013.265106	14.497946
19.369034	1010.160830	14.502963
18.783651	1015.197828	14.507981
19.141887	1015.706637	14.512999
19.239182	1012.434577	14.518016
18.882740	1014.649074	14.523034
19.216376	1008.518641	14.528051
19.369348	1016.270763	14.533069
19.133337	1010.393687	14.538087
19.267388	1014.481658	14.543104
19.148447	1019.003753	14.548122
19.271447	1018.021979	14.553139
18.930801	1032.930059	14.558157
19.572925	1028.124087	14.563175
19.560582	1042.166522	14.568192
19.491580	1044.796744	14.573210
19.800377	1037.426779	14.578227
19.580103	1044.789261	14.583245
20.117112	1029.853636	14.588263
20.102929	1043.296745	14.593280
19.779971	1023.253966	14.598298
19.617008	1006.278888	14.603315
19.852633	1019.452460	14.608333
20.094220	1011.291447	14.613351
19.818657	1001.718741	14.618368
19.619063	1006.445977	14.623386
20.242254	1011.482964	14.628403
19.728332	1007.950059	14.633421
19.847724	1005.627609	14.638439
19.719866	1013.007157	14.643456
19.539738	1006.827831	14.648474
20.027958	1007.527716	14.653491
19.777612	1010.208437	14.658509
19.939737	1009.498250	14.663527
20.128600	1003.447307	14.668544
19.852877	1013.450454	14.673562
20.089910	1004.769440	14.678579
20.011337	1007.713586	14.683597
19.943893	1005.729685	14.688615
19.968166	1001.096267	14.693632
19.971810	1003.273280	14.698650
19.813059	998.627513	14.703667
19.758875	1007.563979	14.708685
20.049738	1008.250604	14.713703
19.896730	1020.358425	14.718720
19.909240	1024.916731	14.723738
20.091078	1035.911727	14.728755
19.946427	1029.379689	14.733773
20.353091	1033.377613	14.738791
20.211187	1030.979333	14.743808
19.982010	1039.886427	14.748826
19.956509	1035.958247	14.753843
19.907104	1034.908809	14.758861
19.914205	1034.664732	14.763879
19.940933	1038.813706	14.768896
20.319958	1028.557745	14.773914
20.546584	1019.509117	14.778931
20.401813	1033.329292	14.783949
20.133318	1018.605092	14.788967
20.111038	1031.553990	14.793984
20.301422	1048.351298	14.799002
20.323622	1046.151371	14.804019
20.633830	1054.361721	14.809037
20.310756	1057.012818	14.814055
20.653612	1055.340174	14.819072
20.598880	1051.893106	14.824090
20.726417	1053.179692	14.829107
20.420776	1054.982284	14.834125
20.685262	1052.798044	14.839143
20.899987	1055.358565	14.844160
20.534314	1047.573555	14.849178
20.580525	1044.634548	14.854195
20.373921	1049.473349	14.859213
20.773294	1057.142700	14.864231
20.949529	1055.811749	14.869248
20.942131	1057.182595	14.874266
20.731975	1039.384885	14.879283
20.422746	1045.795608	14.884301
20.487231	1047.385569	14.889319
20.688442	1045.738275	14.894336
20.098184	1050.889657	14.899354
20.889932	1050.860319	14.904371
20.627393	1052.678247	14.909389
20.518483	1049.545789	14.914407
20.803395	1052.508732	14.919424
20.980577	1050.353951	14.924442
20.742590	1056.554696	14.929459
20.925928	1061.556470	14.934477
20.789521	1059.930514	14.939495
20.930588	1057.049228	14.944512
20.615177	1064.912629	14.949530
20.915832	1077.681571	14.954547
20.803351	1082.332060	14.959565
20.912666	1069.356941	14.964583
21.397867	1080.168730	14.969600
21.224761	1078.769434	14.974618
21.588888	1069.430987	14.979635
21.120157	1081.196989	14.984653
20.926420	1090.893837	14.989671
21.204155	1081.682532	14.994688
20.629447	1085.682748	14.999706
21.578452	1077.303566	15.004723
21.286466	1081.745489	15.009741
21.142535	1088.748881	15.014759
21.262789	1070.583783	15.019776
21.095835	1078.704802	15.024794
21.457942	1080.251290	15.029811
21.282462	1078.038149	15.034829
21.452842	1076.651309	15.039847
21.480948	1078.685639	15.044864
21.076894	1085.186975	15.049882
21.336561	1083.871353	15.054899
21.296144	1077.897335	15.059917
21.176389	1083.830251	15.064935
21.111710	1079.952381	15.069952
21.328740	1091.169120	15.074970
21.928706	1087.467985	15.079987
21.819385	1096.495187	15.085005
21.589714	1088.628887	15.090023
21.655177	1070.507089	15.095040
21.441788	1066.232791	15.100058
21.699399	1078.872775	15.105075
22.037775	1093.652424	15.110093
21.412845	1085.769159	15.115111
21.854382	1079.931071	15.120128
21.728574	1091.551829	15.125146
21.850100	1082.396558	15.130163
21.669541	1078.145516	15.135181
21.687436	1075.785310	15.140199
22.088000	1081.933353	15.145216
22.073536	1088.449389	15.150234
21.840042	1067.048139	15.155251
21.725174	1070.695431	15.160269
21.756359	1069.567091	15.165287
21.933630	1073.440016	15.170304
21.666613	1087.421401	15.175322
22.289944	1086.414881	15.180339
22.402247	1088.006821	15.185357
22.078317	1069.043453	15.190375
22.129601	1066.441326	15.195392
21.848384	1066.460179	15.200410
21.901694	1055.314785	15.205427
21.778280	1065.997857	15.210445
21.931867	1079.155924	15.215463
22.330877	1074.507956	15.220480
22.343753	1089.243924	15.225498
22.207702	1080.485626	15.230515
22.288783	1080.763300	15.235533
21.984220	1072.274411	15.240551
22.344037	1080.117231	15.245568
22.227937	1090.505675	15.250586
22.062907	1087.716526	15.255603
22.622305	1085.568128	15.260621
22.231014	1092.641837	15.265639
22.562071	1087.187139	15.270656
22.228210	1081.880805	15.275674
22.229466	1079.207618	15.280691
22.469590	1075.689100	15.285709
22.329270	1082.742418	15.290727
22.596253	1081.346753	15.295744
22.300684	1082.469255	15.300762
22.608591	1072.824028	15.305779
22.645458	1073.383191	15.310797
22.540683	1085.082702	15.315815
22.573764	1076.099085	15.320832
22.521149	1076.975233	15.325850
22.542166	1080.137322	15.330867
22.633883	1073.691313	15.335885
22.253678	1072.712638	15.340903
22.686784	1069.406888	15.345920
22.398130	1081.731668	15.350938
22.620370	1078.465266	15.355955
22.794367	1075.837599	15.360973
22.835740	1079.365737	15.365991
23.055063	1076.585798	15.371008
22.786442	1081.576339	15.376026
22.765514	1074.491556	15.381043
22.752917	1075.563409	15.386061
22.722185	1082.094616	15.391079
22.831415	1077.208021	15.396096
22.943323	1077.449306	15.401114
22.736683	1076.364540	15.406131
22.966907	1066.759891	15.411149
22.627154	1075.375052	15.416167
22.938489	1073.423316	15.421184
22.537438	1083.540815	15.426202
23.075497	1085.990719	15.431219
23.161443	1094.296188	15.436237
22.876869	1097.174793	15.441255
22.838040	1095.511454	15.446272
23.064411	1102.169647	15.451290
23.021414	1106.061311	15.456307
22.987215	1096.848379	15.461325
23.206061	1102.299048	15.466343
23.261492	1096.966430	15.471360
23.205516	1106.275620	15.476378
23.400391	1104.468363	15.481395
23.436220	1106.675060	15.486413
23.253850	1102.834560	15.491431
23.287966	1095.845289	15.496448
23.495704	1105.753803	15.501466
23.428877	1095.472983	15.506483
23.603116	1101.347218	15.511501
22.983095	1094.334202	15.516519
23.113584	1096.137893	15.521536
23.241165	1093.059894	15.526554
23.371352	1097.180048	15.531571
23.635869	1091.306575	15.536589
23.393451	1101.440256	15.541607
23.463812	1094.918688	15.546624
23.581406	1107.965649	15.551642
23.656773	1122.452006	15.556659
24.105655	1101.079503	15.561677
23.566027	1106.361827	15.566695
23.954165	1098.004239	15.571712
23.585657	1100.368964	15.576730
23.345578	1099.409359	15.581747
23.530287	1102.315426	15.586765
23.514692	1120.079215	15.591783
23.816344	1121.022937	15.596800
24.035953	1123.020956	15.601818
23.921535	1127.905296	15.606835
23.789198	1120.916848	15.611853
23.713723	1130.926556	15.616871
23.845733	1132.256629	15.621888
23.750727	1126.985444	15.626906
23.688394	1129.112847	15.631923
24.081387	1124.951815	15.636941
23.944035	1126.709110	15.641959
23.995708	1122.046121	15.646976
23.694963	1120.679443	15.651994
23.581963	1128.290246	15.657011
23.939838	1120.123586	15.662029
23.876814	1112.079684	15.667047
23.609512	1118.067287	15.672064
23.901599	1138.995577	15.677082
24.079651	1147.087819	15.682099
24.401833	1144.411677	15.687117
24.112554	1150.065054	15.692135
23.952096	1138.770060	15.697152
24.240617	1144.153019	15.702170
24.173442	1151.469466	15.707187
24.222556	1146.576491	15.712205
24.341190	1147.274328	15.717223
24.456169	1140.092484	15.722240
24.602664	1144.759218	15.727258
24.465400	1148.264864	15.732275
24.768285	1136.688985	15.737293
24.511101	1132.708719	15.742311
24.565369	1139.330773	15.747328
24.815947	1140.156263	15.752346
24.434855	1147.575543	15.757363
24.715547	1141.873093	15.762381
24.311908	1147.746364	15.767399
24.841756	1145.447951	15.772416
24.658729	1147.837270	15.777434
24.473644	1146.001177	15.782451
24.907674	1145.778572	15.787469
25.043016	1141.730490	15.792487
24.967399	1141.540399	15.797504
25.032813	1144.698699	15.802522
24.864421	1151.194694	15.807539
25.163030	1140.683017	15.812557
24.509898	1128.635224	15.817575
24.634122	1131.847425	15.822592
24.742405	1139.982154	15.827610
24.775230	1144.988599	15.832627
25.041117	1144.079108	15.837645
24.619135	1153.474071	15.842663
24.816568	1145.698622	15.847680
24.786168	1151.567065	15.852698
24.638736	1147.594846	15.857715
24.870436	1149.376373	15.862733
24.811211	1159.405642	15.867751
24.662773	1155.092744	15.872768
25.081285	1155.525839	15.877786
25.080846	1174.855786	15.882803
25.239389	1172.331515	15.887821
25.267416	1182.441803	15.892839
25.534451	1171.963459	15.897856
25.044954	1151.858263	15.902874
24.956697	1155.125852	15.907891
25.480997	1160.074232	15.912909
25.109153	1174.883173	15.917927
25.427553	1171.431270	15.922944
25.488465	1168.830776	15.927962
25.135115	1172.326101	15.932979
25.353822	1172.497004	15.937997
25.327922	1172.573685	15.943015
25.124714	1167.827540	15.948032
25.333208	1171.092818	15.953050
25.321874	1175.200450	15.958067
24.856038	1166.610548	15.963085
25.291696	1170.834341	15.968103
25.277371	1171.297383	15.973120
25.754094	1182.397749	15.978138
25.471940	1192.622917	15.983155
25.686826	1183.961065	15.988173
26.025897	1193.299925	15.993191
25.640496	1174.030487	15.998208
25.584532	1171.120091	16.003226
25.576791	1197.138546	16.008243
26.330934	1180.578203	16.013261
25.906306	1172.366861	16.018279
25.901429	1162.704319	16.023296
26.158166	1165.977817	16.028314
25.714717	1163.317488	16.033331
25.643410	1158.358169	16.038349
25.655646	1174.161000	16.043367
25.856607	1182.224420	16.048384
26.034967	1187.564691	16.053402
25.612945	1185.696287	16.058419
26.053810	1186.570863	16.063437
25.729101	1185.627669	16.068455
25.605230	1178.391712	16.073472
26.012302	1179.028577	16.078490
25.805484	1185.353875	16.083507
25.986472	1186.294415	16.088525
25.906323	1185.110926	16.093543
25.953579	1203.619210	16.098560
26.621424	1214.383529	16.103578
26.062604	1215.673522	16.108595
26.588496	1209.099474	16.113613
26.596647	1210.395310	16.118631
26.332568	1190.459886	16.123648
26.412209	1196.188022	16.128666
25.871858	1187.070127	16.133683
26.471913	1202.903963	16.138701
26.591251	1202.837964	16.143719
26.521904	1210.647095	16.148736
26.805677	1204.350833	16.153754
26.676943	1202.133509	16.158771
26.457692	1182.402515	16.163789
26.268299	1180.406142	16.168807
26.386658	1195.349740	16.173824
26.767327	1196.164318	16.178842
26.553996	1216.796337	16.183859
26.954245	1212.470041	16.188877
26.928733	1206.850262	16.193895
26.612246	1189.245793	16.198912
26.811262	1182.372666	16.203930
26.738529	1188.822127	16.208947
26.789980	1180.968547	16.213965
27.126061	1195.007004	16.218983
26.835236	1187.910814	16.224000
26.833335	1175.934527	16.229018
26.490761	1190.606347	16.234035
26.728365	1197.916086	16.239053
27.009763	1205.357826	16.244071
26.870884	1200.749920	16.249088
26.900900	1204.314576	16.254106
26.843163	1211.582230	16.259123
26.845321	1208.602759	16.264141
26.993198	1208.156737	16.269159
26.680422	1209.020003	16.274176
27.250024	1204.462041	16.279194
27.103923	1205.741018	16.284211
26.992363	1199.127991	16.289229
27.182494	1195.904470	16.294247
27.011115	1204.307114	16.299264
27.265888	1201.026125	16.304282
27.263783	1200.370066	16.309299
27.209444	1199.128882	16.314317
26.910362	1206.835147	16.319335
27.164820	1223.439539	16.324352
27.566461	1222.322575	16.329370
27.159012	1232.166597	16.334387
27.348267	1230.483288	16.339405
27.214947	1230.804026	16.344423
27.676482	1230.141595	16.349440
27.410026	1216.026003	16.354458
27.594334	1226.802972	16.359475
27.594999	1218.465011	16.364493
27.393616	1224.186694	16.369511
27.536994	1226.534350	16.374528
27.660812	1224.785553	16.379546
27.551714	1230.577987	16.384563
27.448532	1225.607864	16.389581
27.752215	1223.357500	16.394599
27.418632	1231.384772	16.399616
27.888129	1228.919073	16.404634
27.853201	1251.972162	16.409651
27.870888	1247.033590	16.414669
28.171717	1248.993650	16.419687
28.137817	1239.180975	16.424704
27.892739	1233.229504	16.429722
27.929807	1226.328084	16.434739
27.574839	1218.288849	16.439757
27.903962	1230.412792	16.444775
27.817704	1244.441719	16.449792
28.107620	1241.483431	16.454810
28.210560	1246.188576	16.459827
27.881386	1256.522136	16.464845
28.143859	1248.969988	16.469863
27.881108	1252.476381	16.474880
28.280155	1253.127130	16.479898
28.100458	1251.204972	16.484915
28.225232	1254.817910	16.489933
28.260714	1246.168358	16.494951
27.953741	1256.387982	16.499968
27.833079	1246.582585	16.504986
28.043023	1254.442653	16.510003
28.162495	1265.450718	16.515021
28.583575	1270.390055	16.520039
28.261928	1269.304360	16.525056
28.556190	1269.637002	16.530074
28.458726	1275.910483	16.535091
28.332780	1268.756867	16.540109
28.930463	1271.377343	16.545127
28.800120	1277.296202	16.550144
28.862650	1265.470711	16.555162
28.922555	1270.236255	16.560179
28.635799	1262.486124	16.565197
28.351305	1257.058390	16.570215
28.441389	1258.376107	16.575232
28.911841	1257.002199	16.580250
29.126110	1260.064612	16.585267
28.902956	1262.040497	16.590285
29.029898	1262.815935	16.595303
28.552656	1261.401158	16.600320
28.905804	1254.150392	16.605338
28.960338	1264.950874	16.610355
28.768015	1261.105588	16.615373
29.034572	1255.446344	16.620391
28.720405	1256.514964	16.625408
28.557367	1258.288920	16.630426
28.790278	1269.853589	16.635443
28.827089	1269.456526	16.640461
29.083013	1261.955894	16.645479
28.639392	1264.117807	16.650496
29.200143	1283.905916	16.655514
29.354135	1294.340526	16.660531
29.190774	1289.698562	16.665549
29.123851	1276.823491	16.670567
29.344327	1294.219095	16.675584
29.210995	1292.207614	16.680602
29.101362	1298.211601	16.685619
29.421536	1296.147999	16.690637
29.740602	1286.885930	16.695655
29.194088	1294.782485	16.700672
29.428371	1290.980808	16.705690
29.457609	1285.832125	16.710707
29.510241	1289.740406	16.715725
29.665377	1287.832056	16.720743
29.238669	1290.824483	16.725760
29.623720	1288.236303	16.730778
29.835630	1285.962440	16.735795
29.618452	1289.464854	16.740813
30.020035	1284.409316	16.745831
29.630804	1286.262898	16.750848
29.491316	1282.655490	16.755866
29.481381	1294.662182	16.760883
29.880126	1289.076893	16.765901
29.969223	1282.741676	16.770919
29.801065	1292.614512	16.775936
29.892461	1284.249681	16.780954
29.796005	1278.022436	16.785971
29.814988	1295.736800	16.790989
29.707841	1293.774866	16.796007
29.556693	1300.435476	16.801024
29.752863	1310.386944	16.806042
30.154082	1308.626234	16.811059
29.790965	1317.090532	16.816077
29.979525	1309.953898	16.821095
30.006797	1311.947359	16.826112
30.186851	1306.633023	16.831130
29.789631	1310.128936	16.836147
30.203295	1314.501381	16.841165
30.083212	1305.888798	16.846183
30.217424	1307.104927	16.851200
29.865992	1314.661644	16.856218
30.053578	1323.595102	16.861235
30.183794	1340.717705	16.866253
30.403663	1335.365563	16.871271
30.175467	1338.863402	16.876288
30.466904	1335.223181	16.881306
30.334230	1329.970461	16.886323
30.356129	1341.211619	16.891341
30.884945	1335.018935	16.896359
30.557729	1344.850447	16.901376
30.585667	1329.678743	16.906394
30.571848	1342.393001	16.911411
30.656959	1339.324770	16.916429
30.793291	1325.174385	16.921447
30.886407	1335.407110	16.926464
30.699776	1334.511704	16.931482
30.618257	1329.645459	16.936499
30.864576	1336.865524	16.941517
30.782101	1335.837030	16.946535
30.665181	1339.298498	16.951552
30.658841	1335.985810	16.956570
31.010977	1343.388121	16.961587
31.163521	1350.304136	16.966605
31.311460	1347.601614	16.971623
31.293267	1336.113785	16.976640
31.226434	1326.053748	16.981658
31.442754	1320.740038	16.986675
31.127986	1321.934993	16.991693
31.584084	1335.159465	16.996711
31.525905	1336.033341	17.001728
31.195821	1331.272315	17.006746
31.152537	1331.026661	17.011763
31.097026	1324.212295	17.016781
31.059970	1321.993214	17.021799
31.056337	1329.312401	17.026816
30.852342	1325.487866	17.031834
31.134756	1331.764965	17.036851
31.481838	1352.060016	17.041869
32.046258	1337.997189	17.046887
32.152465	1334.032527	17.051904
31.864023	1317.875260	17.056922
32.103592	1318.913931	17.061939
31.798807	1320.037891	17.066957
31.980731	1310.986653	17.071975
32.032521	1315.081270	17.076992
32.172349	1313.838059	17.082010
31.914830	1307.512958	17.087027
31.883233	1307.426424	17.092045
31.926245	1310.891233	17.097063
31.598526	1306.748403	17.102080
31.578791	1301.553737	17.107098
31.884702	1309.837466	17.112115
31.790999	1317.356960	17.117133
31.691562	1304.679475	17.122151
31.868405	1308.142249	17.127168
32.005262	1310.702385	17.132186
31.936945	1310.668943	17.137203
31.514342	1316.570488	17.142221
31.921062	1304.028301	17.147239
31.991622	1315.299690	17.152256
31.980504	1311.485964	17.157274
32.158470	1327.468098	17.162291
32.102029	1337.702166	17.167309
32.396213	1339.271943	17.172327
32.322588	1335.092451	17.177344
32.296606	1343.033706	17.182362
32.203283	1342.947376	17.187379
32.339961	1348.218484	17.192397
32.197214	1345.776110	17.197415
32.252206	1344.965927	17.202432
32.277506	1339.991421	17.207450
32.507324	1334.429430	17.212467
32.239697	1347.035130	17.217485
32.546617	1336.184353	17.222503
32.780617	1335.526011	17.227520
32.474700	1337.413883	17.232538
32.824929	1337.299084	17.237555
32.424453	1349.221830	17.242573
32.546253	1340.173685	17.247591
32.365506	1339.274201	17.252608
32.469129	1353.099887	17.257626
32.806419	1358.749836	17.262643
32.708409	1367.822742	17.267661
33.059099	1359.082721	17.272679
32.709527	1363.767275	17.277696
33.024737	1364.368046	17.282714
33.234918	1368.769231	17.287731
33.093460	1371.237277	17.292749
32.810350	1355.325304	17.297767
32.810514	1366.175393	17.302784
33.068763	1367.084902	17.307802
32.847245	1364.497072	17.312819
32.928634	1369.729509	17.317837
32.774293	1363.088410	17.322855
33.133432	1363.767508	17.327872
32.756196	1373.714175	17.332890
33.177288	1379.505641	17.337907
33.355743	1386.808946	17.342925
33.693768	1382.646999	17.347943
33.796415	1390.511315	17.352960
33.798178	1384.256020	17.357978
33.520571	1356.909249	17.362995
33.170608	1366.223609	17.368013
33.595501	1371.048763	17.373031
33.674244	1382.429369	17.378048
33.536810	1392.682470	17.383066
33.636232	1379.181636	17.388083
33.556096	1386.096250	17.393101
33.711364	1379.438194	17.398119
33.935198	1378.358548	17.403136
33.952774	1377.065057	17.408154
33.927093	1368.999408	17.413171
33.740703	1382.592834	17.418189
34.000415	1375.656473	17.423207
33.888939	1373.360680	17.428224
33.736248	1379.466118	17.433242
34.135951	1378.614548	17.438259
33.593777	1372.886311	17.443277
33.773112	1377.358606	17.448295
33.758207	1377.910111	17.453312
33.672613	1379.479433	17.458330
34.213686	1377.674713	17.463347
33.612002	1377.781646	17.468365
33.829024	1386.688433	17.473383
34.370311	1390.662190	17.478400
34.015699	1403.281558	17.483418
34.021613	1394.500862	17.488435
34.057324	1402.511376	17.493453
34.070584	1397.655510	17.498471
34.373066	1393.761072	17.503488
34.427340	1399.521652	17.508506
34.691804	1395.279706	17.513523
34.413609	1402.484145	17.518541
34.410301	1392.250009	17.523559
34.564751	1395.359688	17.528576
34.598070	1397.670961	17.533594
34.742588	1390.474920	17.538611
34.735954	1396.093557	17.543629
34.623413	1388.865207	17.548647
34.532159	1392.982254	17.553664
34.719720	1396.411807	17.558682
34.703554	1396.275517	17.563699
34.901056	1413.627498	17.568717
34.699258	1416.953951	17.573735
35.286800	1407.375189	17.578752
35.065334	1402.537163	17.583770
35.019253	1391.621735	17.588787
35.058524	1391.871251	17.593805
34.822806	1392.858156	17.598823
35.035796	1400.417998	17.603840
34.774848	1415.919848	17.608858
35.102027	1406.710097	17.613875
35.200263	1415.051661	17.618893
35.192834	1418.836831	17.623911
35.268647	1417.038730	17.628928
34.986687	1422.356516	17.633946
35.349972	1413.254719	17.638963
35.403087	1411.277131	17.643981
35.181858	1420.085334	17.648999
35.555812	1410.830382	17.654016
35.285700	1421.549274	17.659034
35.375766	1405.793391	17.664051
35.202549	1418.712566	17.669069
35.485788	1410.516443	17.674087
35.398620	1416.731552	17.679104
35.484125	1412.022160	17.684122
35.587644	1414.934687	17.689139
35.696977	1422.053168	17.694157
35.374610	1435.222952	17.699175
35.837296	1436.147773	17.704192
35.746298	1443.389173	17.709210
35.608512	1439.364882	17.714227
35.677732	1446.259274	17.719245
35.492221	1438.834044	17.724263
35.798872	1438.587212	17.729280
35.520161	1431.842491	17.734298
35.836030	1431.348051	17.739315
35.850848	1441.135493	17.744333
35.695106	1454.834630	17.749351
36.167830	1461.362837	17.754368
36.489021	1464.989226	17.759386
36.496801	1461.036802	17.764403
36.378034	1462.620796	17.769421
36.309744	1461.889887	17.774439
36.426071	1455.020143	17.779456
36.613646	1460.778793	17.784474
36.542623	1456.955487	17.789491
36.611699	1443.169012	17.794509
36.454785	1439.955639	17.799527
36.606862	1431.552828	17.804544
36.493092	1434.483624	17.809562
36.481696	1432.080621	17.814579
36.421743	1437.354160	17.819597
36.314398	1453.968115	17.824615
36.587022	1452.669372	17.829632
36.163786	1451.470189	17.834650
36.710919	1461.950602	17.839667
36.812697	1459.359442	17.844685
36.634695	1467.084719	17.849703
36.875395	1456.244246	17.854720
36.587950	1463.112472	17.859738
36.588878	1456.601651	17.864755
36.732830	1453.536804	17.869773
36.859409	1465.534846	17.874791
36.895125	1477.386178	17.879808
36.892844	1474.300057	17.884826
37.122646	1481.832051	17.889843
37.039602	1482.151227	17.894861
36.915854	1483.641326	17.899879
37.112270	1481.133170	17.904896
37.290872	1487.508644	17.909914
37.301627	1483.596776	17.914931
37.319076	1480.845248	17.919949
37.077114	1486.825848	17.924967
37.513002	1475.026932	17.929984
37.206697	1477.890066	17.935002
37.259901	1482.154921	17.940019
37.678951	1477.715159	17.945037
37.660886	1484.370765	17.950055
37.596461	1484.040055	17.955072
36.702274	1471.313395	17.960090
37.218770	1480.166995	17.965107
37.741339	1489.499352	17.970125
37.702039	1494.334150	17.975143
37.894973	1497.081196	17.980160
37.747888	1498.600200	17.985178
37.760713	1495.682129	17.990195
37.864193	1504.881332	17.995213
37.453996	1505.841930	18.000231
37.816923	1498.321278	18.005248
37.754789	1491.053429	18.010266
37.669188	1499.695248	18.015283
37.590081	1493.850235	18.020301
37.576043	1500.369511	18.025319
38.066476	1517.704100	18.030336
37.887795	1525.928149	18.035354
38.175521	1521.389026	18.040371
38.240753	1522.780087	18.045389
38.302416	1524.036001	18.050407
38.331019	1513.313935	18.055424
38.413911	1515.974079	18.060442
38.607226	1521.596143	18.065459
38.857475	1528.250754	18.070477
38.677148	1523.504083	18.075495
38.908993	1513.261438	18.080512
38.706464	1510.979894	18.085530
38.473176	1498.967057	18.090547
38.735673	1494.820075	18.095565
38.592685	1506.115575	18.100583
38.731975	1506.172687	18.105600
38.784749	1511.084587	18.110618
39.000981	1513.881636	18.115635
38.748892	1502.452438	18.120653
38.878734	1515.415723	18.125671
38.591288	1515.861604	18.130688
38.825374	1523.175184	18.135706
38.665632	1524.544687	18.140723
38.872620	1516.300499	18.145741
38.730064	1518.175417	18.150759
39.031637	1511.620628	18.155776
38.842193	1515.693124	18.160794
38.703890	1521.256688	18.165811
39.121146	1506.288935	18.170829
38.807831	1525.519953	18.175847
38.993366	1531.727091	18.180864
39.225366	1537.863832	18.185882
39.058711	1538.293944	18.190899
39.487590	1552.933556	18.195917
38.929732	1549.012929	18.200935
39.270774	1539.479031	18.205952
39.382936	1544.795066	18.210970
39.292250	1540.069062	18.215987
39.106060	1549.828094	18.221005
39.433427	1560.797456	18.226023
39.733934	1560.870337	18.231040
39.877954	1564.306745	18.236058
40.007654	1569.209764	18.241075
39.871171	1559.791701	18.246093
39.651030	1564.061532	18.251111
39.597214	1558.130480	18.256128
39.837396	1564.808774	18.261146
39.756728	1573.853819	18.266163
40.347567	1565.413760	18.271181
39.759985	1568.302043	18.276199
39.822650	1570.334171	18.281216
40.233064	1557.500880	18.286234
40.053415	1571.295375	18.291251
40.346435	1561.737429	18.296269
39.991985	1565.879974	18.301287
40.243292	1555.230292	18.306304
40.189429	1557.738290	18.311322
39.893890	1557.248120	18.316339
40.173692	1557.008648	18.321357
40.089192	1553.818625	18.326375
40.259962	1552.968201	18.331392
40.251961	1559.821084	18.336410
40.267850	1565.754998	18.341427
40.840457	1577.733726	18.346445
40.836650	1584.759540	18.351463
40.885526	1577.783548	18.356480
40.699105	1558.687655	18.361498
40.766831	1553.810589	18.366515
41.303593	1543.763161	18.371533
40.631230	1557.016275	18.376551
40.862250	1553.562211	18.381568
40.910407	1546.526380	18.386586
40.857078	1553.313775	18.391603
40.965851	1549.575893	18.396621
40.614660	1564.744855	18.401639
40.922160	1573.943687	18.406656
41.311182	1576.511692	18.411674
40.782071	1579.491806	18.416691
40.816287	1580.439585	18.421709
40.927198	1590.398255	18.426727
40.741994	1571.008654	18.431744
41.151987	1582.129193	18.436762
40.851595	1578.291303	18.441779
41.091887	1578.547196	18.446797
41.138107	1603.629934	18.451815
41.280329	1598.040559	18.456832
41.463000	1594.786576	18.461850
41.567509	1598.721512	18.466867
41.637287	1599.796270	18.471885
41.558857	1609.497423	18.476903
41.366457	1607.065949	18.481920
41.767582	1608.110884	18.486938
41.477682	1607.465186	18.491955
41.824387	1595.172053	18.496973
41.572295	1605.780929	18.501991
41.324050	1603.348737	18.507008
41.450425	1606.986744	18.512026
41.784429	1623.733688	18.517043
42.070774	1629.457981	18.522061
41.840258	1636.711850	18.527079
41.904947	1620.148668	18.532096
42.076087	1622.842341	18.537114
41.927684	1626.775881	18.542131
42.172637	1626.699668	18.547149
42.057617	1625.704659	18.552167
41.946385	1634.038117	18.557184
42.270886	1620.795341	18.562202
41.994920	1626.727663	18.567219
42.633682	1630.938681	18.572237
42.478190	1624.442839	18.577255
42.461995	1620.298465	18.582272
42.455303	1616.616532	18.587290
42.207383	1619.950248	18.592307
42.851122	1635.177991	18.597325
43.004891	1636.024985	18.602343
42.909323	1624.583810	18.607360
42.954792	1620.357187	18.612378
42.744910	1621.646186	18.617395
42.934821	1613.758098	18.622413
43.080562	1612.902125	18.627431
43.051700	1608.627188	18.632448
43.100115	1611.346399	18.637466
43.189447	1616.751243	18.642483
43.448964	1613.441033	18.647501
43.074542	1611.726079	18.652519
43.074116	1604.928223	18.657536
43.280182	1603.674614	18.662554
43.137918	1610.094093	18.667571
43.246799	1610.206466	18.672589
43.399811	1605.934594	18.677607
43.150506	1608.826690	18.682624
43.342746	1603.557697	18.687642
43.082499	1609.288724	18.692659
43.098884	1608.026962	18.697677
43.035427	1601.690287	18.702695
43.159352	1618.359682	18.707712
43.945396	1627.360481	18.712730
43.529066	1627.510960	18.717747
43.307960	1631.348590	18.722765
43.517447	1627.317186	18.727783
43.497361	1623.892983	18.732800
43.892003	1622.505680	18.737818
43.345190	1628.994862	18.742835
43.901363	1629.352752	18.747853
44.114615	1630.846869	18.752871
43.710757	1626.378204	18.757888
43.884735	1632.170599	18.762906
43.627530	1637.809636	18.767923
44.086949	1624.766636	18.772941
44.166114	1644.513831	18.777959
44.403902	1647.219157	18.782976
44.200496	1641.974270	18.787994
44.332068	1646.990633	18.793011
44.272326	1636.645272	18.798029
44.327981	1638.366064	18.803047
44.545742	1642.182274	18.808064
44.511021	1648.771120	18.813082
44.131861	1655.458119	18.818099
44.595217	1649.950963	18.823117
44.720211	1654.428686	18.828135
44.720987	1654.428602	18.833152
44.526730	1646.502855	18.838170
44.572406	1654.060616	18.843187
44.776318	1659.898826	18.848205
44.535368	1654.634570	18.853223
44.461813	1653.301686	18.858240
44.567720	1641.390251	18.863258
44.624577	1652.048584	18.868275
44.804099	1647.823044	18.873293
44.942239	1656.609773	18.878311
45.105687	1665.275770	18.883328
45.233374	1666.508726	18.888346
44.927310	1671.006651	18.893363
44.990818	1672.641005	18.898381
45.099528	1671.172259	18.903399
45.321342	1672.661882	18.908416
44.872016	1662.194499	18.913434
45.306060	1681.292808	18.918451
45.201987	1669.313263	18.923469
45.234148	1674.585063	18.928487
45.329041	1674.860584	18.933504
45.312201	1670.508005	18.938522
44.949561	1671.754666	18.943539
45.528322	1677.445783	18.948557
46.103693	1687.350672	18.953575
45.773167	1684.066621	18.958592
46.026954	1667.615787	18.963610
45.406528	1667.258571	18.968627
46.280502	1676.090976	18.973645
46.129221	1662.878530	18.978663
45.858140	1662.027898	18.983680
46.168226	1661.149329	18.988698
46.398047	1661.820298	18.993715
46.283665	1657.618712	18.998733
46.475918	1660.031356	19.003751
46.086347	1653.726821	19.008768
46.424451	1647.740647	19.013786
46.146592	1653.168317	19.018803
45.790072	1664.639392	19.023821
46.420176	1658.803134	19.028839
46.187247	1657.820285	19.033856
46.547254	1647.185078	19.038874
46.301113	1662.356599	19.043891
46.070362	1673.710139	19.048909
46.759304	1679.226195	19.053927
46.056334	1684.540590	19.058944
46.507401	1676.444289	19.063962
46.334513	1686.548470	19.068979
46.497071	1683.944599	19.073997
46.360673	1686.115233	19.079015
46.591154	1697.020960	19.084032
46.730725	1700.593798	19.089050
46.289422	1714.085396	19.094067
46.988656	1705.224322	19.099085
46.912027	1708.111471	19.104103
46.955202	1714.038003	19.109120
46.892493	1707.486566	19.114138
47.047838	1717.384693	19.119155
46.946810	1719.852764	19.124173
47.204461	1726.705117	19.129191
47.028452	1735.986101	19.134208
47.140035	1731.985793	19.139226
47.119495	1731.177959	19.144243
47.335517	1740.192382	19.149261
47.469588	1740.856265	19.154279
47.224126	1745.038581	19.159296
47.452883	1725.157895	19.164314
47.121729	1738.531261	19.169331
47.646486	1755.311561	19.174349
47.621085	1753.314677	19.179367
47.723624	1763.549327	19.184384
47.919792	1757.493830	19.189402
47.514752	1761.148854	19.194419
47.456841	1764.260311	19.199437
48.200825	1758.557666	19.204455
47.594154	1753.786210	19.209472
47.781264	1763.919242	19.214490
47.735361	1760.988238	19.219507
48.112951	1770.826326	19.224525
48.332398	1767.213078	19.229543
48.347340	1778.894285	19.234560
48.756461	1779.167914	19.239578
48.595622	1768.592149	19.244595
48.435063	1761.308051	19.249613
48.496889	1748.977392	19.254631
48.154845	1750.318667	19.259648
48.195617	1762.762723	19.264666
48.703399	1773.486186	19.269683
48.480711	1775.982794	19.274701
48.629721	1788.709729	19.279719
48.567203	1779.207374	19.284736
48.614453	1778.909656	19.289754
48.266807	1784.607093	19.294771
48.609868	1778.342370	19.299789
48.756554	1773.680105	19.304807
48.423425	1783.935687	19.309824
48.844469	1789.465347	19.314842
48.750599	1802.653251	19.319859
48.823478	1804.377673	19.324877
49.160025	1806.436349	19.329895
48.973363	1797.221695	19.334912
49.222157	1800.180956	19.339930
49.628434	1795.231844	19.344947
49.295184	1798.667331	19.349965
49.548041	1802.916762	19.354983
49.311884	1795.758111	19.360000
49.327113	1795.096158	19.365018
49.419682	1797.455006	19.370035
49.725557	1793.885020	19.375053
49.424405	1787.901121	19.380071
49.361938	1796.485806	19.385088
49.280888	1812.063959	19.390106
49.684196	1813.480974	19.395123
49.822501	1815.523371	19.400141
49.943862	1816.148219	19.405159
49.957580	1822.789504	19.410176
49.983731	1816.331408	19.415194
49.994887	1813.757552	19.420211
49.998563	1812.235819	19.425229
50.390408	1806.840813	19.430247
49.961394	1809.006812	19.435264
50.129249	1807.156379	19.440282
49.936894	1807.827223	19.445299
49.577634	1825.834919	19.450317
50.726139	1825.298381	19.455335
50.516270	1839.170405	19.460352
50.447862	1844.656841	19.465370
50.741536	1837.459344	19.470387
50.480983	1849.347873	19.475405
50.455923	1835.541130	19.480423
50.913888	1836.993768	19.485440
50.729632	1835.160628	19.490458
50.731335	1841.223096	19.495475
50.420614	1837.042762	19.500493
50.943928	1839.179483	19.505511
50.694683	1838.508470	19.510528
50.771892	1845.913038	19.515546
50.685786	1841.643858	19.520563
50.738976	1834.603970	19.525581
51.200044	1850.608492	19.530599
51.007039	1861.564891	19.535616
50.995652	1868.771896	19.540634
51.515075	1860.292394	19.545651
51.456007	1856.940531	19.550669
51.342091	1864.425548	19.555687
51.242609	1862.086785	19.560704
51.289482	1860.192182	19.565722
51.489818	1858.860553	19.570739
51.262299	1875.077132	19.575757
51.721695	1865.540299	19.580775
51.600867	1863.526793	19.585792
51.372315	1869.612723	19.590810
51.737764	1872.291769	19.595827
51.496890	1878.843567	19.600845
51.874210	1878.538317	19.605863
51.611388	1886.829367	19.610880
51.478621	1889.220377	19.615898
51.876580	1882.729251	19.620915
51.602349	1893.512191	19.625933
51.823763	1878.483289	19.630951
51.628302	1888.786793	19.635968
51.971437	1901.003679	19.640986
52.111784	1901.104812	19.646003
52.256719	1902.088913	19.651021
52.307732	1907.534565	19.656039
52.290637	1910.535503	19.661056
52.240062	1898.329657	19.666074
52.189207	1904.870629	19.671091
52.381193	1915.533194	19.676109
52.863564	1922.748073	19.681127
52.551550	1928.421036	19.686144
52.916104	1939.529982	19.691162
52.924061	1940.573419	19.696179
52.844572	1938.048464	19.701197
53.036158	1927.471040	19.706215
53.347140	1928.034622	19.711232
53.071272	1932.029229	19.716250
53.330694	1933.001705	19.721267
52.933013	1924.485970	19.726285
53.187649	1927.539017	19.731303
53.075381	1928.090014	19.736320
52.790795	1931.331695	19.741338
53.122306	1937.699153	19.746355
52.857347	1929.932691	19.751373
52.967368	1935.908788	19.756391
52.990980	1935.813601	19.761408
52.887559	1953.762403	19.766426
53.466871	1951.765433	19.771443
53.547305	1966.630404	19.776461
54.077341	1958.123945	19.781479
53.876448	1952.752332	19.786496
53.791882	1951.607356	19.791514
53.949203	1948.363594	19.796531
54.125009	1955.440313	19.801549
54.100457	1951.316108	19.806567
54.285611	1944.833054	19.811584
53.889643	1947.009671	19.816602
54.082652	1944.501985	19.821619
54.397121	1951.146693	19.826637
54.498382	1941.050506	19.831655
54.484375	1941.513518	19.836672
54.349203	1943.147465	19.841690
54.713858	1944.002462	19.846707
54.287546	1948.020643	19.851725
54.514587	1938.434963	19.856743
54.557289	1944.882390	19.861760
54.300674	1941.823413	19.866778
54.577340	1943.831522	19.871795
54.488824	1962.355551	19.876813
54.862755	1965.415163	19.881831
54.666187	1961.450461	19.886848
54.951124	1962.538871	19.891866
55.141121	1965.415847	19.896883
54.936964	1969.566495	19.901901
55.062981	1961.312698	19.906919
55.168096	1968.116454	19.911936
55.118402	1968.269455	19.916954
54.990734	1962.810622	19.921971
54.974315	1957.612090	19.926989
55.006903	1967.169802	19.932007
54.923369	1960.536322	19.937024
54.802264	1978.330118	19.942042
55.269535	1978.310597	19.947059
55.317481	1993.527845	19.952077
55.533811	1989.318550	19.957095
55.631791	1994.343430	19.962112
55.837789	1998.174183	19.967130
55.936811	1986.778033	19.972147
55.612096	1982.322126	19.977165
55.511140	1978.433964	19.982183
55.644106	1980.679203	19.987200
55.866550	1986.924902	19.992218
56.139461	2005.647987	19.997235
55.860662	2011.003323	20.002253
56.016059	2006.260732	20.007271
55.792254	2007.337329	20.012288
55.802840	2011.040900	20.017306
56.062850	2013.626027	20.022323
56.257412	2013.579801	20.027341
56.083416	2008.547965	20.032359
56.361191	2018.401829	20.037376
56.390380	2035.828126	20.042394
56.982438	2035.107348	20.047411
56.461602	2046.276181	20.052429
56.827135	2045.597206	20.057447
56.801436	2039.058785	20.062464
56.639455	2040.381337	20.067482
56.814358	2041.565893	20.072499
57.066441	2045.029647	20.077517
56.868179	2038.240531	20.082535
57.017332	2034.647712	20.087552
56.799257	2033.889749	20.092570
57.155961	2026.691770	20.097587
56.872330	2039.780182	20.102605
56.790040	2031.940871	20.107623
57.152424	2044.836544	20.112640
57.342454	2051.289331	20.117658
57.367495	2054.971710	20.122675
57.124378	2060.002709	20.127693
57.104268	2058.547803	20.132711
57.332528	2060.440424	20.137728
57.224186	2062.120675	20.142746
57.421133	2065.653036	20.147763
57.206046	2081.602746	20.152781
57.431647	2087.743835	20.157799
57.675300	2086.026676	20.162816
57.513219	2087.762690	20.167834
57.364071	2098.728142	20.172851
57.686181	2107.221160	20.177869
57.896290	2111.606760	20.182887
58.098538	2108.819871	20.187904
57.969486	2119.605447	20.192922
58.295868	2105.434139	20.197939
58.156667	2106.134539	20.202957
58.578862	2120.744104	20.207975
58.821749	2116.710514	20.212992
58.751236	2113.562384	20.218010
58.986630	2103.331472	20.223027
58.512423	2105.968526	20.228045
58.703050	2102.028341	20.233063
58.729184	2099.458410	20.238080
58.393870	2106.135549	20.243098
58.971258	2120.215829	20.248115
58.622671	2127.115979	20.253133
58.951744	2131.104218	20.258151
59.166528	2126.570059	20.263168
59.048109	2130.000354	20.268186
59.572230	2124.792829	20.273203
59.679781	2120.524802	20.278221
59.389701	2113.121987	20.283239
59.485264	2112.071864	20.288256
59.282201	2124.510190	20.293274
59.991086	2114.416542	20.298291
59.983989	2105.766935	20.303309
59.795944	2091.164956	20.308327
59.730334	2077.780978	20.313344
59.211006	2080.567121	20.318362
59.807312	2080.997636	20.323379
60.256951	2096.152035	20.328397
60.044908	2083.324370	20.333415
59.989068	2077.147291	20.338432
59.827741	2072.021927	20.343450
60.020475	2067.295563	20.348467
59.937386	2082.022136	20.353485
60.085105	2090.930664	20.358503
60.774657	2093.401162	20.363520
60.226727	2098.391560	20.368538
60.265816	2094.733916	20.373555
60.262255	2085.645072	20.378573
60.493065	2100.849541	20.383591
60.343332	2100.781512	20.388608
60.243813	2099.149681	20.393626
60.527769	2101.147198	20.398643
60.509631	2097.246035	20.403661
60.313406	2099.858471	20.408679
60.566773	2099.907182	20.413696
60.336290	2120.533459	20.418714
60.518915	2132.602068	20.423731
60.834461	2122.134506	20.428749
60.631225	2128.712058	20.433767
60.645451	2122.568171	20.438784
60.947604	2137.389078	20.443802
60.917845	2154.376564	20.448819
60.971641	2149.981242	20.453837
61.084402	2153.268013	20.458855
61.228702	2147.618177	20.463872
61.126641	2155.991469	20.468890
61.033285	2161.933227	20.473907
61.343134	2168.853318	20.478925
61.428525	2180.018777	20.483943
61.557343	2178.155487	20.488960
61.828173	2178.589658	20.493978
61.658296	2181.358938	20.498995
61.704987	2170.845102	20.504013
61.372675	2187.554947	20.509031
61.625180	2189.544778	20.514048
62.014459	2200.668950	20.519066
62.141792	2201.990369	20.524083
62.147807	2201.355093	20.529101
61.779547	2203.293850	20.534119
62.256487	2200.233515	20.539136
62.335351	2209.900880	20.544154
62.336914	2219.024892	20.549171
62.329294	2218.054051	20.554189
62.621984	2232.548287	20.559207
62.951274	2229.053450	20.564224
62.628000	2224.474168	20.569242
62.765863	2227.848547	20.574259
63.022413	2232.450983	20.579277
62.839826	2223.402743	20.584295
63.030278	2222.176788	20.589312
62.891385	2227.387181	20.594330
63.181782	2227.853005	20.599347
63.511029	2220.592973	20.604365
63.294750	2229.284021	20.609383
63.529759	2220.902565	20.614400
63.426537	2223.036504	20.619418
63.156892	2223.757346	20.624435
63.161367	2216.999519	20.629453
62.943429	2221.303876	20.634471
63.459436	2218.650864	20.639488
63.231891	2229.543464	20.644506
63.154440	2236.202341	20.649523
63.622469	2245.834001	20.654541
63.231209	2246.902131	20.659559
63.540788	2244.527632	20.664576
63.393912	2254.148331	20.669594
63.196378	2254.879968	20.674611
63.725924	2267.093146	20.679629
63.866419	2269.697036	20.684647
63.847680	2269.138226	20.689664
64.248398	2296.555549	20.694682
64.385888	2295.754490	20.699699
64.536406	2299.073246	20.704717
64.414346	2299.505856	20.709735
64.448982	2301.119542	20.714752
64.464618	2301.142379	20.719770
64.644795	2302.278785	20.724787
64.820642	2292.817714	20.729805
64.615886	2291.297035	20.734823
64.746914	2293.791948	20.739840
64.545796	2296.338901	20.744858
65.038589	2301.816451	20.749875
64.991097	2295.205605	20.754893
64.703906	2296.134345	20.759911
65.052814	2307.337498	20.764928
65.079573	2315.289857	20.769946
65.408122	2325.053876	20.774963
65.194292	2316.430245	20.779981
65.124260	2324.511392	20.784999
65.222325	2319.960755	20.790016
65.241225	2317.095253	20.795034
65.117325	2321.634232	20.800051
65.573616	2326.934456	20.805069
65.631435	2345.738938	20.810087
65.842532	2342.388840	20.815104
65.599582	2347.063253	20.820122
65.678950	2343.314034	20.825139
66.143090	2335.272201	20.830157
66.073095	2341.566998	20.835175
66.358469	2334.111805	20.840192
66.618434	2342.807194	20.845210
66.293550	2346.143633	20.850227
66.237218	2334.313969	20.855245
66.230202	2341.978114	20.860263
66.497512	2347.752962	20.865280
66.499870	2358.284541	20.870298
66.473252	2360.643202	20.875315
66.762563	2359.651080	20.880333
66.687234	2362.705404	20.885351
66.855240	2361.009540	20.890368
67.022485	2362.763417	20.895386
66.763096	2370.568110	20.900403
66.790446	2355.723865	20.905421
67.120324	2359.626815	20.910439
66.819398	2354.207632	20.915456
67.053691	2355.827915	20.920474
66.948388	2360.619634	20.925491
67.029516	2366.833952	20.930509
67.314843	2389.648961	20.935527
67.443812	2387.062876	20.940544
67.629512	2395.776239	20.945562
67.588354	2391.048562	20.950579
67.917495	2386.799408	20.955597
67.860774	2392.438829	20.960615
67.771712	2388.715989	20.965632
67.775254	2385.537271	20.970650
68.089121	2385.087308	20.975667
68.165482	2389.064701	20.980685
67.556387	2384.520692	20.985703
67.759386	2386.884410	20.990720
68.000634	2386.152306	20.995738
68.372400	2386.747411	21.000755
68.585710	2406.581735	21.005773
68.376689	2410.588065	21.010791
68.177952	2403.016169	21.015808
68.607425	2397.122740	21.020826
68.524381	2409.826508	21.025843
68.887960	2409.892670	21.030861
68.756521	2400.830015	21.035879
68.792216	2405.675401	21.040896
68.916482	2402.013818	21.045914
68.844316	2402.804722	21.050931
68.908845	2398.133075	21.055949
68.718575	2407.650191	21.060967
68.690166	2403.958874	21.065984
68.797593	2403.800056	21.071002
68.933352	2431.079198	21.076019
68.929849	2422.943322	21.081037
68.986488	2428.274631	21.086055
69.124905	2428.836863	21.091072
69.205720	2431.185013	21.096090
69.157009	2452.048304	21.101107
69.549300	2453.113613	21.106125
69.458984	2450.186298	21.111143
69.668138	2453.511677	21.116160
69.650515	2447.722998	21.121178
69.525538	2459.761118	21.126195
70.026040	2469.536149	21.131213
69.989001	2474.329827	21.136231
69.914207	2478.021623	21.141248
69.993595	2477.232816	21.146266
70.332749	2480.357933	21.151283
70.025679	2476.299965	21.156301
70.409504	2484.029179	21.161319
70.151488	2498.281676	21.166336
71.066537	2488.534256	21.171354
71.104531	2492.208383	21.176371
71.544422	2488.819256	21.181389
71.699161	2480.282982	21.186407
71.125330	2474.095396	21.191424
71.315000	2459.683272	21.196442
70.927260	2459.456852	21.201459
71.492735	2453.785118	21.206477
71.486096	2455.774551	21.211495
71.253639	2465.342492	21.216512
71.672891	2454.012650	21.221530
71.506636	2458.722418	21.226547
71.532351	2451.216331	21.231565
71.319453	2455.267464	21.236583
71.396173	2461.952768	21.241600
71.830924	2449.370677	21.246618
71.490532	2456.313854	21.251635
71.844350	2449.589577	21.256653
72.002550	2455.744509	21.261671
71.824187	2473.970687	21.266688
72.072974	2474.862802	21.271706
71.673181	2481.193538	21.276723
71.892030	2486.963401	21.281741
71.967023	2478.913040	21.286759
72.159671	2478.661966	21.291776
72.175937	2477.213951	21.296794
72.170515	2479.335753	21.301811
71.994187	2486.429979	21.306829
72.343681	2502.051738	21.311847
71.935546	2504.306074	21.316864
72.646448	2496.904076	21.321882
72.515704	2511.913050	21.326899
72.512468	2501.103855	21.331917
72.675186	2522.407521	21.336935
72.878227	2523.628731	21.341952
73.242946	2527.207490	21.346970
73.443292	2522.050581	21.351987
73.170495	2522.412128	21.357005
73.170838	2531.624861	21.362023
72.951916	2521.610075	21.367040
73.536703	2517.557546	21.372058
73.360542	2524.528672	21.377075
73.170729	2517.715957	21.382093
73.504620	2528.381904	21.387111
73.751523	2538.395542	21.392128
73.796901	2539.928664	21.397146
73.536156	2552.354229	21.402163
73.754143	2553.431073	21.407181
73.915580	2549.050350	21.412199
73.631168	2550.600425	21.417216
74.093440	2552.323877	21.422234
74.075837	2580.091226	21.427251
74.119475	2585.105849	21.432269
73.639540	2569.378283	21.437287
74.111184	2580.391947	21.442304
74.307836	2579.628950	21.447322
74.307465	2599.042480	21.452339
73.983492	2605.878989	21.457357
74.320405	2608.363782	21.462375
74.450644	2599.610360	21.467392
74.693499	2613.228991	21.472410
74.806903	2629.799978	21.477427
75.067966	2639.959793	21.482445
75.286117	2639.215518	21.487463
74.989097	2630.664736	21.492480
75.201637	2622.737944	21.497498
75.207437	2620.606673	21.502515
75.092103	2621.912489	21.507533
75.590582	2632.552711	21.512551
75.546598	2645.884912	21.517568
76.013266	2648.242072	21.522586
75.999075	2646.502137	21.527603
76.061922	2646.697478	21.532621
76.273035	2642.267919	21.537639
75.695742	2649.396625	21.542656
76.328675	2642.164592	21.547674
76.039301	2643.784888	21.552691
75.984261	2650.339410	21.557709
76.200845	2646.309825	21.562727
76.095041	2647.172288	21.567744
76.113948	2635.949243	21.572762
76.126515	2635.050965	21.577779
76.561691	2656.094327	21.582797
77.058277	2656.830850	21.587815
76.903049	2665.373671	21.592832
76.953139	2661.979306	21.597850
76.758508	2659.443883	21.602867
76.930511	2664.754032	21.607885
76.813881	2662.228481	21.612903
76.731463	2668.537963	21.617920
77.118324	2664.014584	21.622938
76.918043	2665.718763	21.627955
77.175832	2666.596853	21.632973
77.611177	2670.186669	21.637991
77.033615	2685.764466	21.643008
77.450552	2693.854698	21.648026
77.563929	2693.148930	21.653043
77.592472	2690.259764	21.658061
77.527984	2688.742324	21.663079
77.356283	2686.572575	21.668096
77.627711	2689.708340	21.673114
77.959261	2707.640244	21.678131
77.777641	2713.321427	21.683149
77.990339	2707.010530	21.688167
77.884550	2716.400950	21.693184
77.648848	2715.753028	21.698202
77.682271	2714.232870	21.703219
77.766010	2732.140501	21.708237
78.035157	2741.121856	21.713255
78.031407	2749.745138	21.718272
78.349003	2744.651856	21.723290
78.339116	2755.062495	21.728307
78.752274	2759.160792	21.733325
78.850043	2757.141342	21.738343
78.642515	2755.999798	21.743360
78.749675	2778.855840	21.748378
78.839013	2785.993777	21.753395
79.157229	2784.157562	21.758413
79.271126	2775.564424	21.763431
79.453124	2785.285376	21.768448
79.439098	2776.794340	21.773466
79.816786	2771.155086	21.778483
79.584702	2775.250327	21.783501
79.682193	2764.586157	21.788519
79.851482	2778.752990	21.793536
79.743527	2794.613952	21.798554
80.115526	2794.360024	21.803571
80.168680	2798.107587	21.808589
80.408114	2796.113280	21.813607
80.438842	2798.270486	21.818624
80.694694	2788.051762	21.823642
80.706101	2792.471818	21.828659
80.870689	2793.998909	21.833677
80.679757	2787.053707	21.838695
80.680253	2796.386486	21.843712
80.844307	2799.409690	21.848730
81.197650	2794.740034	21.853747
81.105150	2795.527828	21.858765
80.967713	2785.389661	21.863783
80.807292	2796.392020	21.868800
80.961151	2793.053964	21.873818
81.101892	2790.699536	21.878835
81.055814	2784.675337	21.883853
81.383370	2780.003412	21.888871
80.895530	2780.262940	21.893888
81.098933	2791.265106	21.898906
81.229519	2809.004508	21.903923
81.159828	2810.401028	21.908941
81.413704	2809.913112	21.913959
81.453740	2821.063982	21.918976
81.469396	2833.036131	21.923994
81.632475	2838.439259	21.929011
81.478590	2844.715813	21.934029
81.387602	2846.759535	21.939047
81.966632	2870.324497	21.944064
81.832500	2868.982075	21.949082
81.885623	2869.797556	21.954099
82.029934	2873.786504	21.959117
82.119920	2887.334608	21.964135
82.241082	2895.461804	21.969152
82.153170	2893.919611	21.974170
82.749892	2898.156459	21.979187
82.560646	2913.945045	21.984205
82.869955	2920.092243	21.989223
83.001268	2925.680277	21.994240
82.953946	2924.283219	21.999258
83.416263	2918.472850	22.004275
82.977256	2921.214971	22.009293
83.453281	2916.450313	22.014311
83.236357	2924.889301	22.019328
83.233241	2916.405958	22.024346
83.592241	2933.175461	22.029363
83.837268	2942.261694	22.034381
83.799904	2936.785259	22.039399
83.914835	2944.963953	22.044416
83.912460	2951.478772	22.049434
84.136381	2933.863666	22.054451
83.828954	2940.962829	22.059469
83.805597	2931.015016	22.064487
83.969725	2934.966155	22.069504
84.122636	2942.731747	22.074522
84.392021	2951.896231	22.079539
84.499510	2965.542650	22.084557
84.766971	2954.160529	22.089575
84.507148	2960.431628	22.094592
84.510354	2960.065043	22.099610
84.669094	2963.663537	22.104627
84.555649	2967.386738	22.109645
84.968838	2974.445605	22.114663
85.267183	2985.619230	22.119680
84.898488	2984.272519	22.124698
85.462935	2979.667583	22.129715
85.437943	2987.543129	22.134733
85.545252	2986.140777	22.139751
85.425288	2986.206953	22.144768
85.523909	2977.354147	22.149786
85.577781	2969.180629	22.154803
85.631726	2981.194220	22.159821
85.949892	2988.896066	22.164839
85.901129	3000.654328	22.169856
85.851642	3004.014020	22.174874
86.053935	3002.050760	22.179891
86.038730	3018.175134	22.184909
86.048694	3002.793367	22.189927
86.193625	3010.257242	22.194944
86.302233	3024.020310	22.199962
86.349900	3023.763538	22.204979
86.073253	3033.502826	22.209997
86.679672	3029.071207	22.215015
86.256514	3030.276938	22.220032
86.506196	3039.476116	22.225050
87.266509	3042.295475	22.230067
87.012313	3058.065956	22.235085
87.394813	3049.894570	22.240103
87.575295	3046.397642	22.245120
87.640898	3047.937106	22.250138
87.949294	3034.951472	22.255155
88.087634	3049.820892	22.260173
87.811143	3036.983705	22.265191
87.574939	3042.237984	22.270208
87.902304	3042.893726	22.275226
88.014666	3039.947186	22.280243
87.865884	3048.422898	22.285261
87.733708	3038.880290	22.290279
88.001313	3032.996235	22.295296
87.723114	3052.254941	22.300314
88.073484	3056.767141	22.305331
88.090757	3062.723426	22.310349
88.497129	3068.236847	22.315367
88.603574	3073.487951	22.320384
88.223283	3075.416057	22.325402
88.643427	3080.352892	22.330419
88.561764	3093.274704	22.335437
88.416064	3096.441176	22.340455
88.628646	3107.290597	22.345472
88.723518	3104.226850	22.350490
88.934470	3096.508411	22.355507
88.993686	3119.385021	22.360525
88.776797	3123.673646	22.365543
89.099660	3116.641506	22.370560
89.230852	3123.978175	22.375578
89.389912	3120.096371	22.380595
89.355798	3138.082838	22.385613
89.837363	3144.102125	22.390631
89.371094	3146.334083	22.395648
89.372228	3146.902067	22.400666
89.982555	3151.796499	22.405683
89.459016	3174.398357	22.410701
90.033862	3176.631328	22.415719
90.074641	3181.378283	22.420736
89.969346	3182.278567	22.425754
90.466214	3178.239670	22.430771
90.980815	3191.175446	22.435789
91.097439	3188.698494	22.440807
91.613448	3193.683465	22.445824
91.164756	3177.234003	22.450842
91.404134	3156.971325	22.455859
91.057699	3165.657965	22.460877
91.471014	3154.514835	22.465895
91.365992	3148.875342	22.470912
90.962881	3165.612965	22.475930
91.439641	3170.976515	22.480947
91.478965	3187.193497	22.485965
91.529326	3191.825329	22.490983
91.382819	3180.763580	22.496000
91.647388	3182.032009	22.501018
91.498114	3181.853434	22.506035
91.736988	3200.482098	22.511053
91.845116	3208.150665	22.516071
91.746680	3212.881565	22.521088
92.014308	3213.382547	22.526106
92.156753	3213.199299	22.531123
91.988265	3220.630303	22.536141
92.368918	3234.363535	22.541159
92.375860	3236.799115	22.546176
92.057814	3236.858450	22.551194
92.629420	3242.162975	22.556211
92.850752	3266.557782	22.561229
92.882253	3272.953784	22.566247
93.004396	3271.640617	22.571264
92.681433	3274.683392	22.576282
92.985691	3269.989742	22.581299
92.848892	3273.110662	22.586317
92.955856	3290.169329	22.591335
93.438517	3293.587733	22.596352
93.351623	3294.494608	22.601370
93.694389	3297.540397	22.606387
93.582593	3308.014665	22.611405
94.026264	3306.584839	22.616423
93.876509	3313.785695	22.621440
94.114796	3312.621612	22.626458
94.101572	3307.658910	22.631475
94.381937	3311.588765	22.636493
94.216891	3315.768311	22.641511
94.478562	3312.782553	22.646528
94.231199	3324.070293	22.651546
94.691261	3324.964070	22.656563
94.713028	3325.573015	22.661581
94.883653	3342.874260	22.666599
95.285085	3334.324183	22.671616
95.154328	3341.837701	22.676634
94.812053	3332.987516	22.681651
95.118430	3331.124695	22.686669
95.371467	3333.209261	22.691687
95.498056	3328.571838	22.696704
95.423623	3335.375837	22.701722
95.329577	3332.606776	22.706739
95.257492	3355.046596	22.711757
95.427171	3359.258930	22.716775
95.363490	3356.115824	22.721792
95.954044	3355.007017	22.726810
95.900871	3353.320465	22.731827
95.823553	3379.163601	22.736845
95.787649	3388.313012	22.741863
96.353044	3386.157103	22.746880
96.114822	3384.938263	22.751898
96.289651	3387.839940	22.756915
96.116291	3400.940465	22.761933
96.627287	3414.694445	22.766951
97.165962	3405.198041	22.771968
96.860557	3411.852035	22.776986
96.939453	3405.217823	22.782003
97.256353	3398.369573	22.787021
97.128083	3396.839972	22.792039
97.337777	3399.575217	22.797056
97.440671	3412.578813	22.802074
98.022131	3412.976976	22.807091
98.066958	3410.271365	22.812109
97.855302	3406.857900	22.817127
98.057982	3402.003378	22.822144
98.213257	3420.474929	22.827162
98.046581	3406.506103	22.832179
98.591254	3402.784764	22.837197
98.251488	3416.728851	22.842215
98.491571	3406.417561	22.847232
98.693060	3413.364580	22.852250
98.173467	3411.334468	22.857267
98.804276	3412.990570	22.862285
98.509162	3412.755935	22.867303
98.438353	3400.321831	22.872320
98.372616	3413.916823	22.877338
98.844397	3426.278721	22.882355
98.845062	3435.062609	22.887373
98.634799	3453.900780	22.892391
98.920995	3444.469162	22.897408
98.739331	3456.620985	22.902426
99.228242	3464.476194	22.907443
99.141930	3465.711240	22.912461
98.947444	3468.405663	22.917479
99.217910	3487.010736	22.922496
99.294529	3495.849036	22.927514
98.891907	3500.233131	22.932531
99.606872	3516.152019	22.937549
99.239883	3524.608483	22.942567
99.932030	3535.228368	22.947584
99.656058	3541.650543	22.952602
100.353386	3553.254397	22.957619
100.329278	3558.074743	22.962637
100.086302	3567.209342	22.967655
100.470232	3571.426035	22.972672
100.534732	3582.245285	22.977690
100.262737	3577.929065	22.982707
100.603143	3598.136172	22.987725
100.767199	3597.122578	22.992743
100.967275	3595.342669	22.997760
101.009968	3619.595499	23.002778
101.269964	3627.256232	23.007795
101.417897	3627.454036	23.012813
101.593413	3624.926766	23.017831
101.803106	3630.026134	23.022848
101.958745	3634.720494	23.027866
101.894202	3633.938406	23.032883
102.200826	3622.616013	23.037901
101.964893	3631.143527	23.042919
102.301975	3643.877030	23.047936
101.951496	3653.549309	23.052954
102.236512	3651.408891	23.057971
102.444180	3643.867489	23.062989
102.436469	3655.275704	23.068007
102.569730	3656.353266	23.073024
102.825679	3672.325270	23.078042
102.877587	3679.860810	23.083059
102.972268	3674.410809	23.088077
103.122577	3676.495727	23.093095
103.093395	3675.622876	23.098112
103.163415	3676.258992	23.103130
103.141355	3690.895251	23.108147
103.511216	3689.656872	23.113165
103.309541	3701.799369	23.118183
103.560906	3700.185012	23.123200
103.277267	3708.019329	23.128218
103.298544	3716.459240	23.133235
103.892947	3720.971252	23.138253
103.951351	3722.152080	23.143271
104.411985	3732.650538	23.148288
104.315863	3742.156760	23.153306
104.234041	3745.966699	23.158323
104.379570	3737.920509	23.163341
104.459123	3738.542508	23.168359
104.826315	3735.798969	23.173376
104.943497	3753.411989	23.178394
105.011888	3760.518874	23.183411
105.241684	3762.449314	23.188429
105.229339	3771.566820	23.193447
105.229834	3769.773974	23.198464
105.061556	3766.060103	23.203482
105.379348	3775.217422	23.208499
105.343868	3788.012553	23.213517
105.452856	3789.693633	23.218535
105.582832	3791.352487	23.223552
105.566037	3803.592340	23.228570
105.844674	3818.929647	23.233587
105.832911	3824.101642	23.238605
105.634670	3827.443759	23.243623
106.185769	3842.163942	23.248640
106.670447	3851.673917	23.253658
106.684688	3860.916714	23.258675
106.677256	3855.072329	23.263693
106.593547	3854.946602	23.268711
106.882003	3855.573752	23.273728
107.370342	3865.042128	23.278746
106.995388	3887.473244	23.283763
106.751818	3876.161141	23.288781
107.085205	3885.600146	23.293799
107.570082	3881.016922	23.298816
107.333591	3889.579365	23.303834
107.600078	3904.394691	23.308851
107.865881	3903.668152	23.313869
107.841543	3908.517035	23.318887
107.697446	3913.157423	23.323904
108.135585	3911.728419	23.328922
107.863128	3904.890250	23.333939
107.978264	3918.252117	23.338957
108.243747	3925.444974	23.343975
108.351750	3935.307551	23.348992
108.549472	3925.409776	23.354010
108.526553	3940.264161	23.359027
109.170783	3937.622381	23.364045
108.694114	3950.073263	23.369063
108.757137	3959.999715	23.374080
109.098733	3957.522133	23.379098
108.979608	3949.886610	23.384115
109.643253	3945.019696	23.389133
109.459287	3951.910526	23.394151
109.398564	3947.977758	23.399168
109.660775	3958.507435	23.404186
109.671069	3971.364965	23.409203
110.009257	3973.565676	23.414221
109.962892	3978.162362	23.419239
110.454157	3979.868790	23.424256
109.843876	3975.712790	23.429274
110.414601	3986.096300	23.434291
110.853754	3985.219500	23.439309
110.592688	3992.835769	23.444327
110.646338	3985.334137	23.449344
110.898157	3990.966750	23.454362
110.634504	3992.198053	23.459379
110.842841	3989.757126	23.464397
110.949250	3994.036336	23.469415
111.236247	3996.737468	23.474432
111.454472	4015.190293	23.479450
111.292509	4018.526761	23.484467
111.484839	4020.488350	23.489485
111.294133	4029.725466	23.494503
111.588843	4036.052092	23.499520
111.838205	4037.824833	23.504538
111.811844	4053.355318	23.509555
111.800856	4040.065488	23.514573
111.786491	4061.357681	23.519591
112.167150	4067.667696	23.524608
111.913208	4072.164358	23.529626
111.610403	4088.552535	23.534643
112.096043	4092.100040	23.539661
112.589774	4098.089336	23.544679
112.886522	4105.694012	23.549696
113.076693	4119.041115	23.554714
113.204977	4126.021973	23.559731
113.337820	4127.307952	23.564749
113.418009	4126.449508	23.569767
113.565744	4116.789879	23.574784
113.890946	4127.852688	23.579802
113.636538	4124.499443	23.584819
113.768905	4129.093415	23.589837
113.669753	4151.285949	23.594855
114.298683	4142.033849	23.599872
114.121335	4148.522852	23.604890
114.367677	4157.199159	23.609907
114.447230	4149.264129	23.614925
114.258396	4155.180467	23.619943
113.972913	4171.594413	23.624960
114.415826	4168.993611	23.629978
114.450066	4181.904353	23.634995
114.567408	4190.222116	23.640013
114.906918	4194.291250	23.645031
114.935460	4206.612652	23.650048
115.041579	4200.772461	23.655066
114.816636	4221.539145	23.660083
115.393620	4223.074347	23.665101
115.306961	4223.062710	23.670119
115.449453	4243.797105	23.675136
116.090839	4245.820935	23.680154
116.140326	4258.849288	23.685171
116.115038	4250.611839	23.690189
116.050652	4259.781935	23.695207
116.136249	4255.816706	23.700224
116.340560	4249.452930	23.705242
116.355191	4264.551055	23.710259
116.608681	4266.001215	23.715277
116.792775	4270.959579	23.720295
116.579213	4275.809798	23.725312
116.418887	4271.153959	23.730330
116.495399	4286.428637	23.735347
116.952432	4287.278751	23.740365
117.014776	4300.494505	23.745383
116.912322	4304.673941	23.750400
117.433332	4322.486231	23.755418
117.303645	4325.476802	23.760435
117.626403	4325.814516	23.765453
117.370561	4343.514959	23.770471
117.740917	4356.755096	23.775488
118.433111	4346.864848	23.780506
118.567732	4341.607246	23.785523
118.878539	4345.942897	23.790541
118.517144	4343.565932	23.795559
118.804716	4347.280247	23.800576
119.092023	4360.302978	23.805594
118.969192	4370.555479	23.810611
119.083021	4369.208816	23.815629
119.397189	4361.688310	23.820647
119.233719	4376.157888	23.825664
119.119615	4364.676842	23.830682
119.439175	4372.915661	23.835699
119.343000	4384.868479	23.840717
119.819274	4390.917424	23.845735
120.070698	4397.579231	23.850752
120.156730	4392.960518	23.855770
119.933584	4394.065555	23.860787
119.922993	4390.042769	23.865805
120.309306	4404.129529	23.870823
120.301384	4420.667505	23.875840
120.340785	4420.263656	23.880858
120.448088	4427.260543	23.885875
120.700164	4436.898807	23.890893
120.610388	4444.614686	23.895911
120.474715	4437.953742	23.900928
121.071583	4445.776684	23.905946
121.050554	4476.542966	23.910963
120.675217	4479.565735	23.915981
121.195831	4474.645337	23.920999
121.200605	4497.686884	23.926016
121.470155	4507.912709	23.931034
121.353410	4503.423588	23.936051
121.696214	4514.414433	23.941069
121.942620	4526.834491	23.946087
121.907025	4531.290744	23.951104
122.314857	4530.605060	23.956122
122.509696	4548.762226	23.961139
123.204817	4552.532679	23.966157
123.220702	4557.848907	23.971175
123.059982	4562.103816	23.976192
123.251575	4545.442316	23.981210
123.116493	4557.502350	23.986227
123.045963	4547.488441	23.991245
123.093893	4556.357005	23.996263
123.203142	4573.378645	24.001280
123.671991	4564.757459	24.006298
123.682667	4581.346328	24.011315
123.583069	4589.010147	24.016333
123.477141	4588.357605	24.021351
123.726856	4601.654700	24.026368
123.824551	4607.535763	24.031386
123.927656	4607.948930	24.036403
124.115064	4629.626834	24.041421
124.538853	4624.648966	24.046439
124.530890	4627.140728	24.051456
124.991407	4624.701243	24.056474
125.186457	4630.456583	24.061491
125.072948	4622.059181	24.066509
125.171944	4636.898191	24.071527
124.950336	4647.545103	24.076544
125.386656	4644.695905	24.081562
125.531011	4651.873307	24.086579
126.602641	4631.964698	24.091597
127.169388	4630.711196	24.096615
126.931466	4621.537847	24.101632
126.804081	4614.345248	24.106650
127.140715	4614.576630	24.111667
126.581704	4599.607768	24.116685
126.721808	4584.036976	24.121703
126.640074	4596.855706	24.126720
127.086749	4597.492818	24.131738
127.292107	4610.676923	24.136755
127.238436	4615.322262	24.141773
127.424914	4616.176903	24.146791
127.385140	4620.640145	24.151808
127.085245	4611.681683	24.156826
126.997169	4616.635436	24.161843
127.291496	4615.427771	24.166861
127.900116	4634.896430	24.171879
127.480102	4655.962474	24.176896
127.782603	4646.543464	24.181914
128.055811	4656.109091	24.186931
128.036690	4667.860633	24.191949
127.935195	4663.043963	24.196967
127.809489	4673.899978	24.201984
127.994172	4689.047569	24.207002
128.118052	4701.003997	24.212019
128.236804	4713.153784	24.217037
128.308337	4722.769982	24.222055
128.162238	4737.161369	24.227072
128.926216	4746.470234	24.232090
128.990964	4756.384225	24.237107
129.034177	4777.472531	24.242125
129.091510	4783.808201	24.247143
128.867129	4804.275592	24.252160
129.450057	4800.642678	24.257178
129.490853	4818.429682	24.262195
129.740970	4823.235810	24.267213
130.058642	4833.359584	24.272231
130.122144	4851.117810	24.277248
130.378518	4852.400271	24.282266
130.836542	4862.467351	24.287283
130.630080	4866.145537	24.292301
130.838404	4864.200074	24.297319
130.634482	4877.353798	24.302336
130.911516	4886.126655	24.307354
131.021843	4895.436995	24.312371
130.997535	4900.863785	24.317389
131.161670	4908.306496	24.322407
131.511719	4922.825475	24.327424
131.876927	4915.804949	24.332442
131.698672	4943.556897	24.337459
131.749938	4945.329198	24.342477
131.845006	4945.768886	24.347495
132.278037	4962.585492	24.352512
132.460224	4965.609377	24.357530
132.604555	4970.706738	24.362547
132.632224	4985.636121	24.367565
133.047150	4966.098343	24.372583
132.760512	4985.837057	24.377600
133.048973	5005.372055	24.382618
132.978470	5003.003089	24.387635
133.331321	4999.081057	24.392653
133.526427	4993.608615	24.397671
133.548468	5012.730816	24.402688
133.375687	5019.898074	24.407706
133.671215	5015.666205	24.412723
133.447128	5022.904634	24.417741
134.073564	5042.317278	24.422759
133.944554	5051.851431	24.427776
133.770544	5051.414715	24.432794
134.457108	5071.525042	24.437811
133.956070	5081.212193	24.442829
134.582938	5080.924625	24.447847
134.634112	5093.801796	24.452864
134.827131	5101.925039	24.457882
135.101867	5111.238140	24.462899
134.873106	5129.749501	24.467917
135.499978	5127.747907	24.472935
135.408025	5138.519995	24.477952
135.746677	5148.233458	24.482970
135.895364	5161.963461	24.487987
135.826313	5169.960493	24.493005
136.158355	5165.921735	24.498023
136.316235	5185.884585	24.503040
136.373039	5195.209777	24.508058
136.634904	5182.744429	24.513075
136.726513	5197.812328	24.518093
136.453212	5211.848383	24.523111
136.601562	5217.690141	24.528128
136.910175	5224.119174	24.533146
136.705163	5233.232875	24.538163
136.904565	5252.999897	24.543181
137.488524	5255.916693	24.548199
137.623808	5276.546070	24.553216
137.674931	5271.544341	24.558234
137.993216	5277.043834	24.563251
137.757313	5287.352444	24.568269
138.174089	5290.465895	24.573287
138.295302	5304.986307	24.578304
138.393717	5304.731023	24.583322
138.744576	5323.009724	24.588339
138.933942	5332.882409	24.593357
139.210497	5328.293586	24.598375
138.815534	5336.458546	24.603392
138.812193	5342.336736	24.608410
139.026785	5347.786207	24.613427
139.445004	5359.580159	24.618445
139.495340	5370.494235	24.623463
139.210777	5385.851657	24.628480
139.687513	5386.796597	24.633498
139.634863	5390.889562	24.638515
139.675975	5414.901974	24.643533
139.835802	5421.985714	24.648551
140.328407	5431.656269	24.653568
140.624967	5435.871306	24.658586
140.524983	5446.859485	24.663603
140.216706	5462.971967	24.668621
141.143539	5470.143899	24.673639
141.180401	5472.685573	24.678656
141.926773	5467.429662	24.683674
142.062290	5465.978509	24.688691
141.890721	5471.775771	24.693709
142.167188	5478.077351	24.698727
142.263503	5477.102679	24.703744
142.504938	5488.387782	24.708762
142.501916	5486.134447	24.713779
142.628995	5485.716838	24.718797
142.830962	5494.157675	24.723815
142.792256	5492.626489	24.728832
142.657442	5488.067353	24.733850
142.613279	5482.250296	24.738867
142.652665	5494.087903	24.743885
143.275958	5503.791686	24.748903
143.493823	5511.052610	24.753920
143.173950	5508.388042	24.758938
143.750564	5505.482011	24.763955
143.608629	5522.228225	24.768973
143.853053	5523.471570	24.773991
143.877617	5529.629547	24.779008
143.989841	5520.602914	24.784026
144.525164	5537.984852	24.789043
144.221362	5552.414214	24.794061
144.350238	5553.328432	24.799079
144.559735	5561.272525	24.804096
144.098369	5563.709182	24.809114
144.653318	5572.239962	24.814131
145.065469	5582.279905	24.819149
145.034861	5597.733455	24.824167
145.560796	5607.136879	24.829184
145.413523	5605.228109	24.834202
145.528201	5612.704110	24.839219
145.822784	5633.305777	24.844237
145.544840	5641.187378	24.849255
145.975229	5645.798178	24.854272
146.222266	5665.368784	24.859290
146.158414	5661.890697	24.864307
146.382653	5671.609738	24.869325
146.761346	5673.643325	24.874343
146.976855	5688.193463	24.879360
146.770273	5688.008054	24.884378
147.190959	5700.467900	24.889395
147.324287	5716.031604	24.894413
147.744559	5718.191263	24.899431
147.626215	5726.499302	24.904448
147.785828	5730.170816	24.909466
148.118686	5740.598916	24.914483
147.910837	5752.794249	24.919501
148.281380	5746.725893	24.924519
148.602084	5747.209168	24.929536
148.880120	5757.456465	24.934554
149.264275	5761.632601	24.939571
148.901213	5771.465803	24.944589
149.154340	5767.732850	24.949607
149.159043	5763.517964	24.954624
149.120374	5768.975672	24.959642
149.336271	5782.111624	24.964659
149.345528	5790.412328	24.969677
149.421407	5794.778821	24.974695
149.747027	5810.482941	24.979712
149.517951	5815.244451	24.984730
150.384004	5823.960206	24.989747
150.180525	5832.120639	24.994765
150.738736	5848.078769	24.999783
150.788291	5849.431585	25.004800
150.818034	5849.300694	25.009818
150.765034	5857.727981	25.014835
150.875598	5867.442839	25.019853
150.896701	5871.533827	25.024871
151.085447	5883.098906	25.029888
151.392338	5895.803998	25.034906
152.049926	5897.563477	25.039923
151.730616	5899.952667	25.044941
152.173807	5906.389269	25.049959
152.211811	5913.716413	25.054976
152.186267	5929.317815	25.059994
152.460643	5919.062870	25.065011
152.763107	5923.927381	25.070029
152.731947	5925.924192	25.075047
153.011094	5931.821450	25.080064
153.343411	5929.218792	25.085082
153.566574	5921.197360	25.090099
153.562132	5920.285801	25.095117
153.596942	5923.724369	25.100135
153.838961	5924.450417	25.105152
153.547052	5923.413431	25.110170
153.866174	5934.999155	25.115187
153.741471	5948.526357	25.120205
154.069116	5955.056840	25.125223
154.050695	5968.400099	25.130240
154.213052	5973.873725	25.135258
154.806058	5978.500172	25.140275
154.726641	5997.582477	25.145293
155.026465	6014.370418	25.150311
155.048942	6010.361034	25.155328
155.172897	6019.635089	25.160346
155.352555	6031.185901	25.165363
155.012130	6037.685338	25.170381
155.495190	6041.688207	25.175399
155.665965	6055.592200	25.180416
155.671083	6073.884782	25.185434
155.938446	6086.230016	25.190451
156.315119	6089.128917	25.195469
156.535936	6096.724228	25.200487
156.482003	6109.583857	25.205504
156.386772	6124.110419	25.210522
156.723744	6123.770400	25.215539
156.611792	6144.976140	25.220557
156.777629	6158.909395	25.225575
157.091425	6178.160729	25.230592
157.089099	6188.218590	25.235610
157.328456	6195.776314	25.240627
157.691843	6218.400820	25.245645
157.726980	6228.039297	25.250663
157.996412	6233.897136	25.255680
158.275789	6239.990178	25.260698
158.376203	6248.605113	25.265715
158.461198	6260.224566	25.270733
158.661002	6273.454939	25.275751
159.544671	6279.566967	25.280768
159.901875	6279.024898	25.285786
159.753755	6272.150571	25.290803
159.876584	6273.618210	25.295821
160.311544	6276.858412	25.300839
160.456383	6261.926279	25.305856
160.572900	6263.388592	25.310874
160.830724	6257.142008	25.315891
161.127135	6275.209219	25.320909
161.041372	6271.008388	25.325927
161.487472	6283.019546	25.330944
161.299982	6295.789742	25.335962
161.449479	6297.234264	25.340979
161.287877	6288.632124	25.345997
161.461142	6290.072922	25.351015
161.547512	6291.666232	25.356032
161.518545	6307.259022	25.361050
161.825948	6315.333318	25.366067
161.728520	6328.682903	25.371085
161.993793	6335.589482	25.376103
162.059726	6344.658130	25.381120
162.249242	6352.349998	25.386138
162.012613	6358.056714	25.391155
162.484517	6372.418859	25.396173
162.105548	6387.040589	25.401191
162.505561	6403.232339	25.406208
162.899353	6406.175962	25.411226
162.856338	6428.027844	25.416243
163.138701	6437.798166	25.421261
163.357500	6448.803296	25.426279
163.647414	6459.961446	25.431296
163.328830	6470.921348	25.436314
163.411465	6484.912083	25.441331
164.322626	6494.748080	25.446349
164.383084	6519.264000	25.451367
164.494379	6523.678784	25.456384
164.500885	6534.272112	25.461402
164.855901	6544.763493	25.466419
165.138799	6552.614442	25.471437
164.888920	6558.692644	25.476455
165.292517	6568.586102	25.481472
165.295538	6589.360797	25.486490
165.591145	6588.708410	25.491507
165.670060	6595.366482	25.496525
166.006476	6605.592481	25.501543
166.499271	6616.731569	25.506560
166.456406	6640.424119	25.511578
166.148203	6634.038791	25.516595
166.638225	6640.234710	25.521613
166.494946	6661.777422	25.526631
167.153025	6671.223833	25.531648
167.144800	6690.510371	25.536666
167.034746	6698.274572	25.541683
167.512413	6709.270871	25.546701
167.477670	6725.496291	25.551719
167.888368	6735.758079	25.556736
167.458165	6746.198965	25.561754
168.097287	6762.091553	25.566771
168.332214	6769.116697	25.571789
168.586055	6779.207357	25.576807
168.855069	6779.294682	25.581824
169.045249	6794.237962	25.586842
169.076187	6792.367442	25.591859
169.773530	6794.603786	25.596877
169.770492	6817.431655	25.601895
170.100552	6814.478815	25.606912
169.712260	6822.662326	25.611930
169.867168	6830.429269	25.616947
170.419645	6834.206772	25.621965
170.100505	6843.045560	25.626983
170.387488	6859.656345	25.632000
170.496878	6873.456928	25.637018
170.525729	6871.690904	25.642035
170.901583	6890.204023	25.647053
171.149662	6905.403502	25.652071
171.324194	6910.323045	25.657088
171.353673	6927.643495	25.662106
171.309210	6933.544421	25.667123
171.622059	6941.892791	25.672141
171.588185	6964.302649	25.677159
172.451024	6975.794380	25.682176
172.868576	6991.854470	25.687194
172.645800	6993.382625	25.692212
172.914822	6994.107645	25.697229
172.374355	7001.516378	25.702247
172.609171	7012.841342	25.707264
172.761714	7037.760239	25.712282
172.944810	7042.043936	25.717300
173.692375	7059.700294	25.722317
173.952799	7075.055825	25.727335
174.010629	7076.142254	25.732352
173.882076	7080.001246	25.737370
174.280317	7099.360281	25.742388
174.506287	7090.697046	25.747405
174.602753	7108.723793	25.752423
175.064944	7108.742972	25.757440
175.213592	7121.757830	25.762458
175.218010	7121.539348	25.767476
175.617391	7130.060506	25.772493
175.375998	7134.555946	25.777511
175.804878	7143.391339	25.782528
176.102249	7148.449549	25.787546
176.072011	7150.525272	25.792564
176.584952	7158.681390	25.797581
176.040576	7173.673761	25.802599
176.799689	7182.605814	25.807616
176.745569	7178.914399	25.812634
177.038136	7194.656455	25.817652
177.359260	7199.319496	25.822669
177.468726	7206.124536	25.827687
177.683636	7202.031078	25.832704
178.048901	7214.557466	25.837722
177.924635	7218.400031	25.842740
178.200714	7225.368393	25.847757
178.375497	7235.152838	25.852775
178.271392	7227.150540	25.857792
178.484580	7249.414703	25.862810
178.325184	7250.500447	25.867828
178.786002	7264.419900	25.872845
178.940318	7278.952475	25.877863
178.874943	7279.139544	25.882880
178.946799	7300.355702	25.887898
179.369406	7311.259967	25.892916
179.426965	7328.308052	25.897933
179.198814	7340.356082	25.902951
179.660882	7360.987122	25.907968
179.795587	7384.337112	25.912986
179.949697	7394.358497	25.918004
180.644107	7400.184860	25.923021
180.381588	7432.146233	25.928039
180.302447	7445.304343	25.933056
180.579491	7449.065143	25.938074
180.519167	7480.903372	25.943092
181.486087	7479.384952	25.948109
181.239084	7512.000686	25.953127
181.416882	7508.695909	25.958144
182.014283	7529.968905	25.963162
181.967823	7547.996374	25.968180
182.416267	7551.566180	25.973197
182.331050	7576.658805	25.978215
182.418637	7589.756170	25.983232
183.031728	7597.000205	25.988250
183.413945	7611.187951	25.993268
183.545720	7627.129203	25.998285
183.604112	7635.877653	26.003303
183.681717	7640.673669	26.008320
183.898761	7653.097296	26.013338
183.590407	7666.443009	26.018356
184.552333	7675.157267	26.023373
184.357684	7685.713315	26.028391
184.846411	7684.313994	26.033408
185.033379	7701.004349	26.038426
184.898574	7712.210856	26.043444
185.368428	7708.089974	26.048461
185.413082	7724.401702	26.053479
185.320773	7738.196647	26.058496
185.859240	7746.528980	26.063514
185.750878	7762.236464	26.068532
186.429221	7767.048896	26.073549
186.366154	7787.241771	26.078567
186.119848	7803.678078	26.083584
186.426739	7793.584324	26.088602
186.474184	7808.383466	26.093620
186.734337	7820.888850	26.098637
187.209789	7831.706219	26.103655
186.936097	7848.522545	26.108672
187.276416	7859.155892	26.113690
187.401830	7873.264105	26.118708
188.060818	7883.822286	26.123725
188.054300	7894.554189	26.128743
188.174916	7918.901537	26.133760
188.434714	7911.994261	26.138778
188.536079	7940.152070	26.143796
188.956069	7938.561448	26.148813
188.814835	7941.636496	26.153831
189.475538	7955.840865	26.158848
189.643606	7965.800390	26.163866
189.532393	7981.637946	26.168884
189.754827	7982.225081	26.173901
190.114048	7996.820833	26.178919
190.260951	8016.990536	26.183936
190.393771	8020.571995	26.188954
190.647640	8036.664955	26.193972
190.866165	8040.573957	26.198989
191.195308	8049.804263	26.204007
191.429086	8061.111092	26.209024
191.478693	8073.302352	26.214042
191.707080	8088.325939	26.219060
191.924785	8085.096892	26.224077
191.979153	8093.760948	26.229095
192.145471	8101.444555	26.234112
192.201429	8109.925258	26.239130
192.570546	8125.940256	26.244148
192.470160	8136.181869	26.249165
193.031870	8155.671103	26.254183
193.015428	8162.698276	26.259200
193.319106	8174.256264	26.264218
193.458602	8189.331744	26.269236
193.842975	8200.747664	26.274253
193.735059	8212.771110	26.279271
193.766726	8219.942309	26.284288
194.478744	8237.122331	26.289306
194.322363	8247.356992	26.294324
194.729324	8255.359719	26.299341
195.120449	8275.122059	26.304359
195.093354	8282.251974	26.309376
195.242523	8296.186303	26.314394
195.258236	8309.781637	26.319412
195.533623	8313.258733	26.324429
195.433480	8344.211217	26.329447
195.466444	8354.570973	26.334464
195.977047	8360.871597	26.339482
195.657295	8382.841761	26.344500
196.439562	8395.947682	26.349517
196.401674	8413.529493	26.354535
196.723186	8428.620853	26.359552
196.996220	8446.659130	26.364570
196.760429	8471.590284	26.369588
197.390644	8483.867657	26.374605
197.393516	8498.949006	26.379623
197.569033	8524.860817	26.384640
197.974813	8534.811823	26.389658
198.017053	8555.958289	26.394676
197.957186	8566.102232	26.399693
198.385849	8578.471230	26.404711
198.974252	8606.285392	26.409728
198.907695	8609.895044	26.414746
198.763496	8627.023291	26.419764
199.261143	8634.412111	26.424781
199.870612	8653.720744	26.429799
199.729577	8664.092146	26.434816
200.288132	8662.953336	26.439834
200.111827	8680.689686	26.444852
200.257501	8689.415489	26.449869
200.764676	8707.095305	26.454887
200.672518	8722.501129	26.459904
201.038053	8734.577029	26.464922
201.099185	8744.708429	26.469940
201.131242	8758.598309	26.474957
201.636213	8768.483386	26.479975
201.553150	8786.470435	26.484992
201.874653	8805.237098	26.490010
201.727979	8824.313917	26.495028
202.397493	8841.545362	26.500045
202.466024	8849.086739	26.505063
202.463571	8874.603851	26.510080
202.866908	8877.896834	26.515098
202.879331	8903.430599	26.520116
203.222769	8929.512416	26.525133
203.606429	8933.831437	26.530151
203.608481	8947.981895	26.535168
203.938507	8964.486801	26.540186
204.196791	8986.348177	26.545204
204.915904	9001.197753	26.550221
205.430282	9008.135772	26.555239
204.991276	9027.233338	26.560256
205.351754	9029.952128	26.565274
205.584096	9030.461972	26.570292
205.271837	9055.832117	26.575309
206.113687	9050.932812	26.580327
206.120661	9076.013023	26.585344
206.579521	9072.142991	26.590362
206.687344	9090.191990	26.595380
206.999422	9102.769038	26.600397
207.132214	9092.723957	26.605415
207.144655	9107.299139	26.610432
207.412402	9125.878798	26.615450
207.578329	9131.371750	26.620468
208.070694	9145.088773	26.625485
208.298125	9151.999183	26.630503
208.396480	9167.571281	26.635520
208.997728	9164.619792	26.640538
209.098495	9188.432022	26.645556
208.810463	9190.178957	26.650573
209.476429	9187.359403	26.655591
209.414620	9200.310819	26.660608
209.785538	9215.145655	26.665626
209.288677	9222.510546	26.670644
209.560432	9229.224603	26.675661
210.101197	9243.379295	26.680679
210.248842	9263.382901	26.685696
210.406983	9280.811688	26.690714
210.605979	9295.342005	26.695732
210.378989	9303.283480	26.700749
210.838531	9319.054862	26.705767
210.742023	9334.799705	26.710784
210.958892	9349.349366	26.715802
211.242864	9369.540111	26.720820
211.396652	9392.037169	26.725837
211.918636	9413.781962	26.730855
211.887282	9431.354239	26.735872
212.406675	9436.012049	26.740890
212.421415	9457.555356	26.745908
212.890519	9474.771428	26.750925
212.705790	9487.919111	26.755943
213.125222	9502.326651	26.760960
213.410104	9520.275711	26.765978
213.432671	9545.009960	26.770996
213.962428	9550.793346	26.776013
214.206703	9553.798793	26.781031
213.886523	9577.851120	26.786048
214.032827	9583.410427	26.791066
214.603193	9600.282387	26.796084
214.857157	9612.824683	26.801101
215.097934	9627.541313	26.806119
215.231115	9655.065268	26.811136
215.798456	9661.932090	26.816154
216.017498	9657.370159	26.821172
215.916761	9680.497865	26.826189
215.785080	9689.270745	26.831207
216.298467	9714.313526	26.836224
216.384496	9725.846589	26.841242
216.586654	9743.919332	26.846260
216.718538	9767.828464	26.851277
217.121767	9780.606394	26.856295
217.605295	9789.560793	26.861312
217.581184	9806.137713	26.866330
218.216923	9831.281465	26.871348
218.179380	9839.386089	26.876365
218.606698	9848.112518	26.881383
218.432177	9865.246652	26.886400
219.072635	9881.599548	26.891418
219.317190	9886.628898	26.896436
218.971511	9912.832681	26.901453
219.719254	9908.655158	26.906471
220.059755	9930.823663	26.911488
220.048473	9946.157837	26.916506
220.256396	9943.283634	26.921524
220.431797	9973.971484	26.926541
220.746104	9979.997147	26.931559
220.761822	10001.727216	26.936576
221.257419	10008.191785	26.941594
221.574545	10031.497585	26.946612
221.495993	10029.953319	26.951629
221.888791	10055.050182	26.956647
222.154148	10072.238735	26.961664
222.324925	10086.906703	26.966682
222.733438	10099.207252	26.971700
223.070019	10101.172163	26.976717
223.497903	10109.216620	26.981735
223.585398	10117.396499	26.986752
224.069682	10113.948527	26.991770
224.518387	10131.329433	26.996788
224.032072	10130.591036	27.001805
224.312496	10137.998702	27.006823
224.479437	10156.914084	27.011840
224.461006	10173.910381	27.016858
224.983374	10181.040196	27.021876
224.849934	10197.603016	27.026893
225.184748	10208.033342	27.031911
225.374503	10226.942064	27.036928
225.258250	10243.398036	27.041946
225.493686	10257.471879	27.046964
225.691038	10289.887098	27.051981
225.853146	10294.269564	27.056999
225.841125	10317.292592	27.062016
225.920152	10343.910380	27.067034
226.613321	10370.548822	27.072052
226.612457	10394.602693	27.077069
226.910051	10412.443267	27.082087
227.102599	10436.264813	27.087104
227.100332	10446.634410	27.092122
227.595956	10472.568248	27.097140
227.438642	10492.112589	27.102157
228.014270	10501.968579	27.107175
228.328561	10532.038819	27.112192
228.535806	10555.169877	27.117210
228.972814	10574.119154	27.122228
229.090137	10587.760224	27.127245
229.323409	10596.106927	27.132263
229.435123	10622.678942	27.137280
229.507827	10637.315343	27.142298
230.053867	10650.459874	27.147316
230.255373	10681.646842	27.152333
230.889436	10680.455042	27.157351
230.869747	10709.605367	27.162368
230.859815	10721.169866	27.167386
231.273251	10738.013765	27.172404
231.532947	10764.196524	27.177421
231.994796	10777.385909	27.182439
232.108382	10792.293891	27.187456
232.581850	10806.880272	27.192474
232.916318	10807.320491	27.197492
232.891969	10832.082738	27.202509
233.666528	10841.209924	27.207527
233.818302	10854.280589	27.212544
233.568884	10866.539466	27.217562
234.075675	10868.891436	27.222580
234.109583	10896.868515	27.227597
234.705820	10903.245007	27.232615
234.603072	10920.738298	27.237632
234.812253	10925.874513	27.242650
235.374901	10932.177338	27.247668
235.335562	10950.721669	27.252685
235.489949	10963.924619	27.257703
235.814243	10983.008798	27.262720
235.256142	11002.625928	27.267738
235.355890	11025.509170	27.272756
236.057888	11046.125670	27.277773
236.596253	11057.307667	27.282791
237.149355	11077.574930	27.287808
237.518291	11106.551318	27.292826
237.594825	11114.821763	27.297844
237.774237	11124.241252	27.302861
238.118649	11132.229762	27.307879
238.545167	11157.638583	27.312896
238.274425	11171.839775	27.317914
238.485820	11177.910367	27.322932
238.858334	11198.667063	27.327949
239.196477	11210.628875	27.332967
239.075196	11230.698819	27.337984
238.993825	11248.700601	27.343002
239.262930	11265.940186	27.348020
239.289076	11288.453206	27.353037
239.477351	11311.209253	27.358055
239.965299	11343.353420	27.363072
240.253409	11364.354030	27.368090
240.821015	11389.261101	27.373108
240.933726	11414.283674	27.378125
240.914264	11424.773338	27.383143
241.259562	11442.995812	27.388160
241.521590	11470.540143	27.393178
241.989949	11492.393648	27.398196
241.741794	11513.030045	27.403213
242.219869	11532.160161	27.408231
242.919334	11535.189353	27.413248
242.840122	11567.719574	27.418266
243.233464	11576.824743	27.423284
243.630016	11597.502331	27.428301
244.363174	11605.982739	27.433319
244.695959	11615.615275	27.438336
244.869657	11635.405771	27.443354
245.042716	11641.482519	27.448372
244.983662	11648.902917	27.453389
245.336316	11651.143353	27.458407
245.724474	11669.555111	27.463424
245.867921	11675.737555	27.468442
246.067786	11684.323647	27.473460
245.769165	11710.563612	27.478477
245.854261	11725.063138	27.483495
246.321036	11735.754681	27.488512
246.790791	11760.194444	27.493530
247.303883	11754.512320	27.498548
247.477950	11779.996267	27.503565
247.758742	11797.663960	27.508583
247.855633	11808.925040	27.513600
248.083001	11833.838636	27.518618
248.305846	11836.952017	27.523636
248.219822	11853.969895	27.528653
248.531077	11870.477155	27.533671
248.946129	11886.737655	27.538688
249.041051	11912.433116	27.543706
249.163076	11919.266333	27.548724
249.587115	11942.617759	27.553741
249.692005	11958.232205	27.558759
250.270860	11979.121644	27.563776
249.929798	12008.191700	27.568794
250.528588	12021.985746	27.573812
250.871568	12041.453321	27.578829
251.200874	12056.994800	27.583847
251.241004	12077.034043	27.588864
251.486765	12104.585008	27.593882
252.147321	12112.240212	27.598900
252.497768	12130.702537	27.603917
252.736451	12141.351100	27.608935
253.279934	12149.248861	27.613952
253.247026	12168.207052	27.618970
253.950536	12170.724156	27.623988
253.873511	12187.090422	27.629005
253.910524	12193.444441	27.634023
254.296117	12212.952885	27.639040
254.315636	12231.160845	27.644058
254.850066	12247.106123	27.649076
254.918263	12270.349494	27.654093
254.919139	12281.932205	27.659111
255.166115	12299.990918	27.664128
255.446588	12329.459877	27.669146
255.698270	12340.251775	27.674164
256.041062	12365.896393	27.679181
255.927348	12387.093722	27.684199
256.497443	12406.690302	27.689216
256.521364	12426.805085	27.694234
256.975767	12436.374781	27.699252
257.331063	12465.506975	27.704269
257.434930	12487.889254	27.709287
258.126097	12502.272329	27.714304
258.158236	12509.593517	27.719322
258.430539	12533.989428	27.724340
258.685076	12551.289315	27.729357
259.201872	12569.966008	27.734375
259.180058	12586.440811	27.739392
259.227872	12612.324602	27.744410
259.852096	12620.080442	27.749428
259.585893	12644.851379	27.754445
259.912422	12667.691616	27.759463
260.444195	12681.057703	27.764480
260.273679	12712.814732	27.769498
260.525357	12730.696279	27.774516
260.856320	12754.312764	27.779533
260.835150	12776.569710	27.784551
261.553875	12788.343433	27.789568
261.642242	12828.021131	27.794586
261.903624	12843.422320	27.799604
262.209919	12860.038593	27.804621
262.341872	12883.237993	27.809639
262.897359	12902.527903	27.814656
262.409742	12924.974936	27.819674
263.130080	12941.460102	27.824692
263.382188	12974.556634	27.829709
263.366844	12992.230784	27.834727
263.836084	13011.360630	27.839744
264.086434	13040.049093	27.844762
264.383798	13059.111175	27.849780
265.031858	13087.566879	27.854797
265.097582	13111.910632	27.859815
266.229299	13129.553642	27.864832
266.410672	13147.746603	27.869850
266.692081	13144.958303	27.874868
266.595063	13159.743252	27.879885
266.758391	13173.110563	27.884903
267.589488	13177.193111	27.889920
267.624898	13194.471071	27.894938
268.087498	13216.835911	27.899956
268.054637	13228.411853	27.904973
268.712897	13244.417526	27.909991
268.970681	13245.611944	27.915008
268.929882	13262.781902	27.920026
269.099502	13279.849437	27.925044
269.705600	13295.430684	27.930061
269.645878	13308.886717	27.935079
270.123928	13324.781739	27.940096
270.101827	13350.825916	27.945114
270.285051	13361.468065	27.950132
270.161882	13384.850154	27.955149
270.411692	13405.852721	27.960167
270.849199	13426.358526	27.965184
270.585088	13450.129101	27.970202
271.340277	13477.096983	27.975220
271.618876	13503.507962	27.980237
271.551698	13522.018122	27.985255
271.971279	13554.173608	27.990272
272.028305	13581.137319	27.995290
272.348221	13608.893604	28.000308
272.941927	13633.426906	28.005325
273.069532	13655.911060	28.010343
273.496560	13672.108063	28.015360
273.801322	13693.759211	28.020378
274.357428	13724.949348	28.025396
274.863278	13742.466756	28.030413
274.690434	13762.575883	28.035431
275.261536	13781.131577	28.040448
275.352219	13806.552364	28.045466
275.423923	13824.084171	28.050484
275.639980	13849.624330	28.055501
275.399406	13882.006951	28.060519
275.957808	13903.258585	28.065536
276.421520	13929.224292	28.070554
277.019656	13959.277638	28.075572
277.294326	13983.924534	28.080589
277.511089	13987.487673	28.085607
277.749420	14018.614380	28.090624
277.985458	14043.403202	28.095642
278.464137	14061.724160	28.100660
278.709791	14080.564828	28.105677
278.752237	14114.624673	28.110695
279.399955	14128.441021	28.115712
279.659903	14167.112465	28.120730
280.169665	14166.337862	28.125748
280.688716	14187.908633	28.130765
280.600732	14196.395686	28.135783
281.162951	14204.259797	28.140800
281.164597	14223.944153	28.145818
281.440512	14230.473025	28.150836
281.513790	14251.504181	28.155853
281.514169	14265.365190	28.160871
281.871958	14284.466410	28.165888
282.248663	14310.727341	28.170906
282.377197	14333.509015	28.175924
282.651672	14347.207137	28.180941
282.678727	14373.917697	28.185959
283.080184	14401.880277	28.190976
283.218542	14427.082827	28.195994
283.460631	14451.564891	28.201012
284.366678	14463.364008	28.206029
284.494071	14502.142166	28.211047
284.766352	14512.521514	28.216064
284.880014	14547.054174	28.221082
285.004670	14569.884111	28.226100
285.520304	14596.815315	28.231117
285.819153	14623.047817	28.236135
285.995382	14639.783927	28.241152
286.520072	14667.891819	28.246170
286.441760	14689.809393	28.251188
287.101114	14725.397003	28.256205
287.392675	14742.857315	28.261223
287.308141	14761.576679	28.266240
287.769581	14793.001313	28.271258
288.338669	14820.805603	28.276276
288.867150	14837.060345	28.281293
288.818036	14864.424642	28.286311
289.174637	14871.361140	28.291328
289.353628	14905.719986	28.296346
289.264671	14934.783440	28.301364
289.698360	14956.801133	28.306381
289.840678	14985.664206	28.311399
290.421135	15011.954192	28.316416
290.349151	15045.850443	28.321434
290.575651	15077.107060	28.326452
291.188617	15101.588708	28.331469
291.255202	15137.086763	28.336487
291.579315	15158.231221	28.341504
292.118490	15185.895448	28.346522
292.266995	15210.314187	28.351540
292.811913	15234.424512	28.356557
293.421790	15264.670734	28.361575
293.712677	15281.143098	28.366592
293.634139	15307.148251	28.371610
293.937940	15332.288178	28.376628
294.431076	15354.559157	28.381645
294.362715	15388.919718	28.386663
294.988343	15399.029431	28.391680
295.116738	15431.536897	28.396698
295.339462	15463.713809	28.401716
296.066250	15478.482044	28.406733
296.195885	15501.009111	28.411751
296.466534	15523.899432	28.416768
296.894278	15550.558341	28.421786
296.900008	15580.501751	28.426804
297.044051	15597.783818	28.431821
297.625655	15628.897275	28.436839
297.533429	15655.707266	28.441856
298.101945	15675.718059	28.446874
298.216224	15712.893116	28.451892
298.646150	15736.052468	28.456909
298.838629	15764.665661	28.461927
299.476043	15789.156993	28.466944
299.356974	15811.587573	28.471962
299.540789	15837.176498	28.476980
299.733597	15860.205750	28.481997
300.143664	15895.878806	28.487015
300.460400	15919.596197	28.492032
300.716945	15948.423874	28.497050
300.673570	15976.947993	28.502068
301.651326	16005.549076	28.507085
301.685551	16035.283433	28.512103
301.677467	16056.645158	28.517120
302.110828	16078.736838	28.522138
302.139949	16105.822181	28.527156
302.777376	16149.166672	28.532173
302.650991	16181.083628	28.537191
303.376316	16220.261154	28.542208
303.451760	16254.120648	28.547226
303.763219	16289.260309	28.552244
304.442792	16313.887838	28.557261
304.666889	16350.630006	28.562279
304.781914	16386.321764	28.567296
305.362240	16412.326272	28.572314
305.560574	16450.885636	28.577332
305.455581	16475.582580	28.582349
305.702933	16507.384677	28.587367
306.201914	16543.098700	28.592384
306.903842	16581.958460	28.597402
306.874385	16617.569047	28.602420
307.601848	16644.362559	28.607437
308.206870	16674.987629	28.612455
308.708044	16697.757956	28.617472
308.983112	16718.491731	28.622490
309.615460	16736.257389	28.627508
310.025330	16754.370611	28.632525
310.178315	16774.359203	28.637543
310.390015	16791.341158	28.642560
311.191859	16811.888283	28.647578
311.357515	16831.180068	28.652596
311.872101	16842.571363	28.657613
312.227197	16859.676209	28.662631
312.274953	16880.568950	28.667648
312.587711	16892.569907	28.672666
312.765952	16920.334236	28.677684
313.081214	16928.187625	28.682701
313.319586	16949.470670	28.687719
313.697712	16978.590384	28.692736
314.042631	16988.201638	28.697754
314.039883	17020.962906	28.702772
314.322041	17037.172822	28.707789
314.461415	17053.108211	28.712807
314.758266	17081.716486	28.717824
314.943324	17106.779417	28.722842
315.052441	17139.517046	28.727860
315.407428	17167.137174	28.732877
315.743313	17205.107949	28.737895
315.855783	17235.425716	28.742912
316.222866	17269.070740	28.747930
316.164989	17306.023145	28.752948
316.532798	17341.860270	28.757965
316.911407	17373.671662	28.762983
317.080171	17409.041026	28.768000
317.526921	17440.639700	28.773018
317.700070	17483.955684	28.778036
318.261994	17517.918072	28.783053
318.788490	17547.312315	28.788071
319.408711	17584.898157	28.793088
319.518510	17613.062718	28.798106
319.754316	17639.925155	28.803124
320.470089	17665.341572	28.808141
321.281035	17688.772091	28.813159
321.344316	17700.689442	28.818176
321.830125	17728.334100	28.823194
321.667248	17756.926944	28.828212
322.205322	17768.542535	28.833229
322.601037	17791.021120	28.838247
322.386880	17810.531314	28.843264
323.125052	17832.526716	28.848282
323.087630	17866.065571	28.853300
323.306941	17896.140208	28.858317
323.556791	17928.136933	28.863335
323.872599	17950.577680	28.868352
323.986859	17972.184530	28.873370
324.440597	18015.767305	28.878388
324.983017	18052.993512	28.883405
325.514851	18074.964655	28.888423
325.411150	18106.701182	28.893440
326.038261	18125.839844	28.898458
326.312998	18165.072949	28.903476
326.793142	18188.429541	28.908493
327.222071	18222.287646	28.913511
327.174817	18251.273746	28.918528
327.771134	18275.010252	28.923546
328.105214	18306.564811	28.928564
328.402202	18329.375364	28.933581
329.006858	18358.512208	28.938599
329.366490	18393.613399	28.943616
329.888684	18414.316597	28.948634
330.265128	18444.512774	28.953652
330.387439	18467.167640	28.958669
330.500815	18492.906943	28.963687
330.424868	18519.705714	28.968704
330.882193	18542.219741	28.973722
331.213385	18592.633446	28.978740
331.427939	18613.170246	28.983757
332.414412	18641.590666	28.988775
332.102414	18675.894144	28.993792
333.180646	18692.669373	28.998810
333.434191	18722.019706	29.003828
333.792965	18753.924915	29.008845
334.366264	18769.307276	29.013863
334.541419	18792.788184	29.018880
335.190928	18811.121662	29.023898
335.681514	18835.071265	29.028916
336.086169	18850.871809	29.033933
336.252498	18873.362308	29.038951
336.654176	18896.618325	29.043968
336.880958	18912.642633	29.048986
337.293364	18932.877113	29.054004
337.254984	18955.469269	29.059021
337.592097	18974.350942	29.064039
337.511429	19001.157431	29.069056
338.296636	19029.496227	29.074074
338.477504	19057.203180	29.079092
338.660136	19074.738181	29.084109
338.953745	19114.197683	29.089127
339.150919	19134.579809	29.094144
339.393301	19169.985069	29.099162
339.563322	19202.457598	29.104180
339.949434	19239.716879	29.109197
340.359046	19269.195217	29.114215
340.372400	19305.331567	29.119232
340.965248	19338.875312	29.124250
340.861214	19382.194714	29.129268
341.785609	19419.787003	29.134285
342.281767	19448.057963	29.139303
342.445613	19483.027517	29.144320
343.023389	19511.153106	29.149338
343.193116	19542.078341	29.154356
343.588552	19563.276467	29.159373
343.530360	19584.773122	29.164391
343.622254	19621.990767	29.169408
344.443855	19640.816147	29.174426
344.723166	19685.958941	29.179444
345.024270	19717.735763	29.184461
345.591967	19744.391162	29.189479
345.425301	19778.168360	29.194496
346.264500	19816.033799	29.199514
346.414660	19849.022275	29.204532
346.363344	19882.055004	29.209549
346.677300	19914.278715	29.214567
347.360045	19953.236686	29.219584
348.004326	19976.759257	29.224602
348.701023	20024.257291	29.229620
348.977881	20043.029391	29.234637
349.746214	20062.994472	29.239655
349.321385	20097.659292	29.244672
349.638869	20117.265415	29.249690
350.049267	20153.360088	29.254708
350.519445	20174.269169	29.259725
350.509026	20208.445950	29.264743
350.835894	20243.580870	29.269760
351.324106	20282.860607	29.274778
351.806600	20319.222294	29.279796
351.862553	20353.749070	29.284813
352.509516	20390.369446	29.289831
352.980930	20421.248810	29.294848
353.622048	20446.636330	29.299866
353.992905	20475.459137	29.304884
354.295869	20505.474142	29.309901
354.425919	20530.689094	29.314919
354.751568	20570.633020	29.319936
355.007032	20598.349422	29.324954
355.288863	20628.841799	29.329972
355.711891	20667.349043	29.334989
356.099161	20694.002406	29.340007
356.286130	20726.474803	29.345024
356.835341	20762.738402	29.350042
356.863276	20802.937941	29.355060
356.929456	20837.375506	29.360077
357.550390	20885.367689	29.365095
357.827053	20923.847814	29.370112
358.660896	20961.179237	29.375130
358.649423	20998.965385	29.380148
358.682089	21047.492403	29.385165
359.413167	21085.036031	29.390183
359.781939	21116.981434	29.395200
360.259911	21148.928738	29.400218
361.107683	21177.071291	29.405236
361.128642	21213.222593	29.410253
361.977353	21233.707034	29.415271
362.553036	21273.000321	29.420288
362.786423	21287.452219	29.425306
363.615885	21313.228381	29.430324
363.896623	21343.576710	29.435341
364.113134	21361.778215	29.440359
364.105486	21390.415227	29.445376
364.324559	21416.779986	29.450394
365.004080	21437.455425	29.455412
365.441197	21471.406328	29.460429
365.572170	21506.580506	29.465447
366.119556	21525.760268	29.470464
366.333836	21555.500107	29.475482
366.652938	21590.790295	29.480500
366.815604	21624.095719	29.485517
367.248812	21645.296495	29.490535
367.582417	21675.163153	29.495552
368.156406	21697.946876	29.500570
368.157835	21730.077185	29.505588
368.218086	21753.876611	29.510605
368.607409	21785.693503	29.515623
369.109417	21829.201377	29.520640
369.032028	21855.000243	29.525658
369.795936	21889.551504	29.530676
369.570854	21927.594041	29.535693
369.763452	21962.127501	29.540711
370.409520	22005.164563	29.545728
370.961251	22040.330651	29.550746
371.434299	22088.829154	29.555764
371.503708	22123.894014	29.560781
372.074330	22160.081003	29.565799
372.421902	22205.755976	29.570816
372.949621	22235.371913	29.575834
373.412011	22272.188989	29.580852
373.379936	22310.454781	29.585869
373.742575	22353.435895	29.590887
374.247275	22398.018806	29.595904
374.865154	22447.310638	29.600922
375.175265	22479.393808	29.605940
375.529037	22524.897934	29.610957
375.735773	22567.392097	29.615975
376.042734	22609.851696	29.620992
376.973802	22647.310096	29.626010
377.505598	22684.875343	29.631028
377.789376	22713.045242	29.636045
378.714679	22735.686665	29.641063
379.193019	22771.712293	29.646080
379.432673	22785.033200	29.651098
380.119129	22823.244299	29.656116
380.578871	22842.243178	29.661133
380.923633	22853.057964	29.666151
381.591798	22876.415964	29.671168
382.094124	22895.566200	29.676186
382.566293	22910.512683	29.681204
382.912734	22933.838998	29.686221
383.486435	22943.575327	29.691239
383.654989	22970.923204	29.696256
383.869614	22984.797926	29.701274
384.425536	23000.300075	29.706292
384.765117	23027.494858	29.711309
385.115198	23044.191999	29.716327
385.502457	23075.922817	29.721344
385.463195	23095.979566	29.726362
386.214326	23111.419629	29.731380
386.197536	23139.049534	29.736397
386.522094	23169.286368	29.741415
386.762769	23196.876025	29.746432
387.085547	23234.531924	29.751450
387.494882	23260.275330	29.756468
387.796439	23295.147912	29.761485
388.137440	23308.794532	29.766503
388.174110	23360.265000	29.771520
388.307572	23399.499070	29.776538
389.003836	23421.374614	29.781556
389.431666	23468.227930	29.786573
389.680174	23505.453628	29.791591
389.599391	23539.097399	29.796608
390.099516	23580.486133	29.801626
390.785887	23629.447882	29.806644
390.952811	23671.002743	29.811661
391.517169	23702.902717	29.816679
391.919548	23743.649891	29.821696
392.234695	23782.868894	29.826714
392.688440	23813.920622	29.831732
392.484024	23852.595529	29.836749
392.903994	23887.532750	29.841767
393.819811	23927.365717	29.846784
394.175694	23972.796986	29.851802
395.044111	24011.620124	29.856820
395.265301	24035.327553	29.861837
395.411553	24063.571458	29.866855
395.642950	24103.094900	29.871872
395.909899	24135.825762	29.876890
396.294179	24177.632003	29.881908
397.100523	24221.432370	29.886925
397.998324	24242.032310	29.891943
398.459418	24277.064882	29.896960
398.740285	24308.763769	29.901978
399.342245	24335.179854	29.906996
399.543001	24366.967215	29.912013
399.696936	24392.929033	29.917031
400.130066	24416.369894	29.922048
400.375909	24460.884215	29.927066
401.020432	24489.651030	29.932084
401.158608	24533.411389	29.937101
401.524721	24566.772019	29.942119
402.001989	24595.628380	29.947136
401.954088	24643.462667	29.952154
402.942295	24674.090755	29.957172
403.217523	24719.011821	29.962189
403.652475	24753.404717	29.967207
403.675747	24783.874455	29.972224
404.344614	24837.290939	29.977242
405.216346	24858.432772	29.982260
405.388688	24906.972590	29.987277
405.973885	24934.156773	29.992295
406.235951	24968.539200	29.997312
406.563671	25004.314381	30.002330
407.314517	25041.931907	30.007348
407.642528	25078.844727	30.012365
408.015790	25105.221813	30.017383
408.207656	25144.304795	30.022400
408.363809	25188.569346	30.027418
409.249297	25212.464823	30.032436
409.382683	25262.819060	30.037453
409.675195	25293.771940	30.042471
410.583832	25337.198492	30.047488
410.508132	25379.957742	30.052506
410.821135	25415.167172	30.057524
410.818066	25447.942467	30.062541
411.698456	25494.704351	30.067559
411.875846	25538.309076	30.072576
412.259036	25586.008556	30.077594
412.823590	25624.294663	30.082612
413.249725	25675.507822	30.087629
413.446541	25716.923193	30.092647
413.961702	25764.817303	30.097664
414.267117	25810.071031	30.102682
414.644771	25855.774904	30.107700
414.976069	25913.797512	30.112717
415.512169	25951.121734	30.117735
415.791039	26004.450721	30.122752
416.102454	26043.927521	30.127770
416.528928	26093.195111	30.132788
417.139204	26142.541472	30.137805
417.236537	26195.766676	30.142823
417.635393	26236.171849	30.147840
418.181342	26291.975161	30.152858
419.054531	26343.992167	30.157876
419.205967	26385.921626	30.162893
419.424504	26438.363743	30.167911
420.073076	26478.888290	30.172928
419.985890	26531.106766	30.177946
420.517082	26566.486271	30.182964
420.863401	26620.002239	30.187981
421.478553	26667.345604	30.192999
421.989394	26701.199034	30.198016
422.201743	26744.371103	30.203034
423.417807	26779.605784	30.208052
423.411256	26825.776523	30.213069
424.302474	26870.087622	30.218087
425.064905	26906.550196	30.223104
425.221630	26947.987003	30.228122
426.216434	26977.890728	30.233140
426.250837	27016.553245	30.238157
426.554400	27055.906839	30.243175
427.083452	27089.600055	30.248192
427.284855	27113.939920	30.253210
427.912187	27153.476843	30.258228
428.177012	27192.267933	30.263245
428.259050	27231.713448	30.268263
429.120149	27270.272240	30.273280
429.088986	27317.642511	30.278298
429.941598	27357.315196	30.283316
430.213456	27405.845416	30.288333
430.603506	27452.341004	30.293351
431.078428	27490.113756	30.298368
431.407247	27538.578486	30.303386
432.148532	27574.723226	30.308404
432.295293	27612.945800	30.313421
432.854875	27653.151642	30.318439
433.251571	27694.729356	30.323456
433.888962	27743.563398	30.328474
434.056983	27794.158673	30.333492
434.610140	27821.282233	30.338509
434.817514	27867.788419	30.343527
435.764684	27911.157574	30.348544
435.749332	27951.776411	30.353562
436.341934	27991.788130	30.358580
437.101481	28028.329015	30.363597
437.432757	28077.262369	30.368615
438.015744	28113.571914	30.373632
438.129153	28163.190630	30.378650
438.400316	28200.699541	30.383668
439.001655	28238.479161	30.388685
439.647789	28277.800417	30.393703
440.374831	28313.980303	30.398720
440.495109	28363.585786	30.403738
440.948969	28399.366159	30.408756
441.391275	28446.677528	30.413773
441.577394	28491.753642	30.418791
442.210129	28536.020365	30.423808
442.382380	28583.962186	30.428826
443.416695	28626.371086	30.433844
443.427806	28656.949671	30.438861
443.834720	28720.164178	30.443879
444.465005	28748.547386	30.448896
444.902083	28791.321973	30.453914
445.589189	28828.292816	30.458932
445.953472	28857.773432	30.463949
446.121709	28908.175477	30.468967
446.922982	28937.252751	30.473984
447.288009	28996.985511	30.479002
447.481730	29039.735525	30.484020
448.072937	29075.324899	30.489037
448.362543	29111.574712	30.494055
448.940079	29140.415515	30.499072
449.405043	29193.483496	30.504090
449.812016	29238.811104	30.509108
450.715015	29271.393736	30.514125
452.125641	29284.769401	30.519143
452.769917	29288.442193	30.524160
453.246770	29308.746622	30.529178
453.600826	29328.261210	30.534196
454.647484	29352.540878	30.539213
454.220160	29367.512941	30.544231
454.818123	29384.271316	30.549248
454.847264	29409.671231	30.554266
454.884314	29435.335426	30.559284
455.537267	29457.698382	30.564301
455.825891	29483.070388	30.569319
456.320599	29507.778033	30.574336
456.570797	29557.467189	30.579354
456.773917	29591.518998	30.584372
457.139852	29615.166027	30.589389
457.494457	29669.409293	30.594407
457.662279	29708.656504	30.599424
458.058635	29756.597564	30.604442
458.216396	29810.821464	30.609460
458.887529	29859.680550	30.614477
458.915422	29904.304131	30.619495
459.716623	29944.571444	30.624512
460.165274	30003.516513	30.629530
460.442805	30049.801729	30.634548
461.069510	30099.610214	30.639565
461.429889	30152.185020	30.644583
462.005434	30209.751719	30.649600
462.422868	30259.302586	30.654618
462.457574	30306.814825	30.659636
463.103739	30370.256100	30.664653
463.496944	30429.457602	30.669671
464.009895	30476.907966	30.674688
464.523520	30530.091872	30.679706
464.550646	30595.767442	30.684724
465.260065	30658.169296	30.689741
465.607518	30727.606958	30.694759
466.269453	30763.820321	30.699776
466.679297	30834.791017	30.704794
467.466044	30887.522162	30.709812
468.537761	30930.037424	30.714829
469.198534	30979.103068	30.719847
469.779570	31015.658264	30.724864
470.400940	31057.972499	30.729882
470.478125	31100.523775	30.734900
471.442799	31142.917165	30.739917
471.454305	31186.009919	30.744935
472.445119	31227.817799	30.749952
472.679453	31270.464920	30.754970
472.964371	31310.379565	30.759988
474.046042	31349.562611	30.765005
474.346212	31400.797175	30.770023
474.511535	31440.357822	30.775040
475.197537	31477.826683	30.780058
475.490757	31529.454600	30.785076
475.872978	31567.571769	30.790093
476.169581	31607.074239	30.795111
476.532023	31660.088746	30.800128
476.785909	31716.186460	30.805146
477.109827	31770.332561	30.810164
477.893249	31813.716626	30.815181
477.895577	31865.302431	30.820199
478.777462	31903.070113	30.825216
479.497549	31961.617885	30.830234
480.130775	32013.313861	30.835252
480.689237	32059.483693	30.840269
481.200673	32113.708786	30.845287
481.355051	32156.300702	30.850304
482.002107	32202.867900	30.855322
482.108014	32243.748019	30.860340
482.862797	32274.322936	30.865357
482.963039	32332.753888	30.870375
483.635611	32374.411617	30.875392
483.809248	32419.453986	30.880410
484.136821	32476.825569	30.885428
484.926627	32515.007070	30.890445
485.198894	32566.324731	30.895463
485.793267	32622.630753	30.900480
486.415621	32676.814647	30.905498
486.596578	32720.946137	30.910516
486.824558	32769.476866	30.915533
487.468120	32829.720738	30.920551
487.455155	32882.727603	30.925568
487.990687	32952.497256	30.930586
488.372400	33007.554222	30.935604
489.409445	33057.457252	30.940621
490.352510	33107.665944	30.945639
491.239964	33153.502163	30.950656
491.815228	33210.318536	30.955674
492.334755	33254.644687	30.960692
493.317461	33289.301181	30.965709
493.235115	33328.145518	30.970727
493.806525	33373.380524	30.975744
494.481215	33406.163479	30.980762
495.121074	33455.851488	30.985780
495.703431	33487.997834	30.990797
496.039558	33539.889528	30.995815
496.472638	33591.981125	31.000832
496.964953	33627.271354	31.005850
497.318353	33664.138706	31.010868
498.120434	33703.837826	31.015885
498.348321	33754.729097	31.020903
499.263926	33799.462220	31.025920
499.408799	33835.572231	31.030938
500.137311	33869.068236	31.035956
500.861814	33913.591281	31.040973
501.280355	33947.812464	31.045991
501.774581	33994.104101	31.051008
502.340244	34039.733435	31.056026
502.479443	34077.545500	31.061044
503.108568	34119.371564	31.066061
503.473896	34169.085289	31.071079
504.139683	34219.314778	31.076096
504.716272	34258.550781	31.081114
505.089520	34311.734686	31.086132
505.526649	34347.622767	31.091149
506.088779	34393.904646	31.096167
506.398747	34443.456978	31.101184
506.955416	34487.368938	31.106202
507.022048	34544.413996	31.111220
507.584058	34575.073046	31.116237
508.533234	34643.272402	31.121255
508.420590	34681.143959	31.126272
508.856460	34737.796604	31.131290
509.005400	34803.542152	31.136308
509.963786	34862.130238	31.141325
510.496170	34919.457431	31.146343
510.673276	34964.694382	31.151360
511.347270	35025.591015	31.156378
511.417168	35091.552165	31.161396
512.200962	35147.569714	31.166413
512.069496	35212.140141	31.171431
512.354776	35295.215744	31.176448
512.905320	35351.630767	31.181466
513.473955	35429.781249	31.186484
514.027243	35497.014725	31.191501
514.763752	35559.464861	31.196519
515.246628	35612.660151	31.201536
516.418590	35666.095410	31.206554
516.813588	35730.958009	31.211572
517.655047	35776.370846	31.216589
518.035006	35838.283282	31.221607
518.290218	35889.061586	31.226624
519.377677	35942.295792	31.231642
519.741060	35993.392524	31.236660
520.822417	36033.317847	31.241677
521.266284	36080.260561	31.246695
521.582715	36119.085492	31.251712
522.226292	36159.598114	31.256730
522.906979	36207.193237	31.261748
523.334296	36249.921384	31.266765
523.444544	36303.410719	31.271783
523.966178	36358.935050	31.276800
524.915981	36397.522177	31.281818
524.941926	36458.948068	31.286836
525.486161	36510.036681	31.291853
526.188131	36563.358110	31.296871
526.375288	36624.778196	31.301888
527.159573	36672.863993	31.306906
527.529576	36742.501332	31.311924
528.057137	36794.560701	31.316941
528.478126	36863.912224	31.321959
529.050954	36918.974712	31.326976
529.300646	36966.025664	31.331994
529.730753	37046.537086	31.337012
529.923264	37094.469903	31.342029
530.796205	37160.273728	31.347047
531.114528	37228.814143	31.352064
531.728541	37300.419606	31.357082
531.907264	37376.361835	31.362100
532.559405	37429.851312	31.367117
533.481318	37498.993638	31.372135
533.673806	37573.796174	31.377152
534.362690	37640.053976	31.382170
534.709225	37700.453055	31.387188
536.054942	37767.032053	31.392205
536.938068	37821.321043	31.397223
537.504858	37873.712038	31.402240
538.494799	37920.762967	31.407258
538.587401	37976.529422	31.412276
539.363283	38033.586536	31.417293
539.983898	38078.956645	31.422311
540.299130	38138.052851	31.427328
541.664847	38176.514809	31.432346
542.018838	38219.454400	31.437364
542.776111	38272.784063	31.442381
543.191124	38317.042278	31.447399
543.485510	38363.779423	31.452416
544.101142	38422.146391	31.457434
544.396470	38462.281568	31.462452
544.642224	38522.401516	31.467469
545.320984	38566.511429	31.472487
545.522818	38629.300886	31.477504
545.803546	38693.064693	31.482522
546.332881	38747.904690	31.487540
546.433283	38810.179352	31.492557
547.092096	38870.381023	31.497575
547.486002	38936.492966	31.502592
548.192116	39003.795708	31.507610
548.169448	39075.785039	31.512628
548.944428	39143.526432	31.517645
549.438438	39219.261336	31.522663
550.291132	39284.341233	31.527680
550.848663	39345.464424	31.532698
551.139780	39427.941660	31.537716
551.523690	39484.886922	31.542733
552.500640	39542.194787	31.547751
552.887742	39611.212620	31.552768
553.639085	39670.485021	31.557786
554.012315	39733.352014	31.562804
554.969853	39799.473171	31.567821
555.567817	39847.987336	31.572839
556.060457	39922.637142	31.577856
556.464348	39982.122915	31.582874
557.410235	40040.676513	31.587892
557.696082	40101.534492	31.592909
558.272988	40164.718666	31.597927
558.706232	40227.729470	31.602944
559.371487	40294.018068	31.607962
560.010855	40351.153262	31.612980
560.317461	40416.846997	31.617997
561.124592	40472.311898	31.623015
561.481306	40548.933046	31.628032
562.375643	40609.368271	31.633050
562.498019	40673.200627	31.638068
563.062182	40739.588629	31.643085
563.807822	40808.206249	31.648103
564.193315	40877.487643	31.653120
565.052340	40945.063366	31.658138
565.599253	41004.769856	31.663156
566.013640	41068.197130	31.668173
566.307445	41141.060767	31.673191
567.272890	41216.387243	31.678208
567.984904	41273.760129	31.683226
568.552001	41349.762940	31.688244
569.018445	41419.804974	31.693261
569.484787	41475.034856	31.698279
570.200623	41550.958146	31.703296
571.056656	41606.121000	31.708314
571.447409	41683.797010	31.713332
571.841171	41755.027897	31.718349
572.858444	41817.306678	31.723367
573.382240	41884.672158	31.728384
574.489162	41938.468347	31.733402
574.664170	42009.063887	31.738420
575.416440	42073.959104	31.743437
575.949131	42117.972585	31.748455
576.518409	42188.804219	31.753472
577.908901	42222.664956	31.758490
578.363857	42280.112354	31.763508
578.409727	42343.348026	31.768525
579.138382	42390.272449	31.773543
579.671813	42456.430104	31.778560
580.247711	42510.614458	31.783578
580.886199	42571.373454	31.788596
581.351826	42636.675745	31.793613
581.842637	42686.806878	31.798631
582.323715	42757.692101	31.803648
582.997087	42807.921417	31.808666
583.975769	42873.688010	31.813684
583.632334	42935.316525	31.818701
584.407819	42997.630185	31.823719
585.229147	43065.256274	31.828736
585.690433	43128.536654	31.833754
585.977872	43195.316959	31.838772
586.790298	43259.731851	31.843789
587.396639	43321.744003	31.848807
587.716705	43393.232070	31.853824
588.144293	43466.411342	31.858842
588.780627	43535.396139	31.863860
589.012373	43610.143595	31.868877
589.498224	43679.247286	31.873895
589.848051	43759.890912	31.878912
590.609722	43826.282573	31.883930
591.285288	43900.082271	31.888948
591.276224	43963.754962	31.893965
592.085562	44045.124652	31.898983
592.652176	44132.548140	31.904000
592.897378	44207.004521	31.909018
594.091302	44287.460928	31.914036
594.333592	44359.590499	31.919053
594.961762	44444.949783	31.924071
595.165268	44516.965751	31.929088
595.689229	44603.018793	31.934106
596.476931	44682.205549	31.939124
596.946627	44776.364511	31.944141
598.063371	44858.871913	31.949159
598.409582	44949.786914	31.954176
599.369783	45032.939390	31.959194
599.979241	45106.829336	31.964212
600.511000	45185.899816	31.969229
601.432266	45259.387191	31.974247
601.902965	45342.554221	31.979264
602.368703	45420.623744	31.984282
602.931990	45504.896541	31.989300
603.556871	45584.447254	31.994317
604.095246	45663.613267	31.999335
604.901939	45734.937719	32.004352
606.766895	45813.504294	32.009370
607.247249	45877.390436	32.014388
607.971996	45942.661820	32.019405
608.462890	46013.802556	32.024423
608.617544	46090.417543	32.029440
609.578235	46142.222493	32.034458
610.163610	46217.562190	32.039476
611.076701	46284.747157	32.044493
611.702022	46354.033362	32.049511
612.015988	46418.927635	32.054528
612.693388	46496.948761	32.059546
613.435046	46555.912153	32.064564
613.761033	46637.550404	32.069581
614.621213	46703.283565	32.074599
614.667430	46774.869584	32.079616
615.359982	46852.225314	32.084634
615.780165	46921.893327	32.089652
615.964079	47003.529841	32.094669
616.705052	47083.206833	32.099687
617.396620	47171.989041	32.104704
617.676309	47255.237317	32.109722
618.821740	47324.837268	32.114740
619.131335	47419.962313	32.119757
619.993726	47493.345986	32.124775
620.546773	47585.763867	32.129792
620.903312	47657.835485	32.134810
622.181455	47730.762575	32.139828
622.648794	47814.325137	32.144845
623.368533	47903.472725	32.149863
623.657193	47980.389434	32.154880
624.424280	48062.419231	32.159898
624.823139	48140.869223	32.164916
625.631508	48221.045772	32.169933
626.610364	48304.523694	32.174951
627.404261	48379.319129	32.179968
627.983358	48458.317707	32.184986
628.704515	48531.796438	32.190004
629.233714	48612.296456	32.195021
630.204958	48673.690470	32.200039
630.717762	48750.074856	32.205056
630.794631	48826.907375	32.210074
631.805168	48884.854053	32.215092
631.915668	48965.686610	32.220109
632.805957	49049.503789	32.225127
633.742700	49109.107562	32.230144
633.800378	49174.530664	32.235162
634.737222	49246.820100	32.240180
634.954531	49321.810144	32.245197
636.121940	49403.478366	32.250215
636.305357	49463.403500	32.255232
636.779282	49548.894748	32.260250
637.235693	49615.756145	32.265268
637.559367	49701.252509	32.270285
638.263820	49789.327920	32.275303
638.951856	49881.050610	32.280320
639.919982	49967.244240	32.285338
640.332011	50049.045709	32.290356
640.601736	50141.999132	32.295373
641.203793	50226.251694	32.300391
642.066074	50327.540801	32.305408
642.600674	50428.660220	32.310426
643.410909	50517.715212	32.315444
643.852994	50610.687816	32.320461
644.459482	50697.263496	32.325479
644.939427	50801.240367	32.330496
645.720646	50888.675218	32.335514
646.503433	50985.860578	32.340532
646.735261	51086.796174	32.345549
647.396025	51177.319750	32.350567
648.595963	51282.957691	32.355584
648.905347	51381.623534	32.360602
649.524654	51475.223573	32.365620
650.210231	51572.382318	32.370637
650.963628	51679.446079	32.375655
651.822238	51771.858224	32.380672
652.275720	51876.426184	32.385690
652.968945	51975.913963	32.390708
653.652278	52072.436057	32.395725
654.678321	52166.601610	32.400743
655.227329	52252.293553	32.405760
655.985277	52355.449197	32.410778
656.620379	52450.569327	32.415796
657.475879	52543.674738	32.420813
658.106881	52622.103584	32.425831
659.144875	52717.750188	32.430848
660.079896	52811.122633	32.435866
660.956662	52891.785585	32.440884
661.245842	52978.096711	32.445901
661.962255	53063.050354	32.450919
662.910828	53153.821275	32.455936
663.557955	53228.376934	32.460954
664.570924	53305.438362	32.465972
664.926141	53397.081488	32.470989
665.730214	53475.479754	32.476007
666.329290	53558.567817	32.481024
667.366762	53630.019836	32.486042
668.110871	53703.853072	32.491060
668.805814	53789.293635	32.496077
669.537693	53864.413894	32.501095
669.917916	53938.697197	32.506112
670.479304	54010.028754	32.511130
671.079353	54089.486176	32.516148
671.860579	54168.978774	32.521165
672.855949	54255.139687	32.526183
673.723466	54326.512854	32.531200
673.580274	54394.829765	32.536218
674.599427	54475.950466	32.541236
674.894022	54559.209972	32.546253
675.745575	54631.618073	32.551271
676.760271	54713.948997	32.556288
676.967711	54794.622030	32.561306
677.790022	54869.712336	32.566324
678.352416	54960.550687	32.571341
678.650357	55027.686535	32.576359
679.480758	55100.352517	32.581376
679.807727	55187.153085	32.586394
680.869265	55246.696049	32.591412
682.617043	55313.827151	32.596429
683.788573	55359.525402	32.601447
684.561539	55411.848841	32.606464
685.816759	55466.672588	32.611482
687.575687	55481.965388	32.616500
688.309017	55523.846854	32.621517
688.914089	55563.318309	32.626535
689.675872	55607.132008	32.631552
689.624725	55650.218736	32.636570
690.138180	55698.166090	32.641588
690.659938	55741.530323	32.646605
690.801674	55802.066760	32.651623
691.648741	55854.822574	32.656640
691.950706	55916.099974	32.661658
692.438964	55977.095210	32.666676
692.702553	56043.846926	32.671693
693.239237	56120.498470	32.676711
694.164051	56199.424781	32.681728
694.369517	56281.944822	32.686746
694.727741	56349.663528	32.691764
695.254729	56428.114948	32.696781
695.518799	56517.100981	32.701799
696.471479	56607.738924	32.706816
696.992747	56703.223066	32.711834
697.855187	56795.287187	32.716852
698.181634	56887.068523	32.721869
698.967137	56971.981036	32.726887
699.617998	57071.104473	32.731904
700.115435	57165.315732	32.736922
700.868781	57261.310040	32.741940
701.343271	57360.626844	32.746957
702.214252	57462.704730	32.751975
702.802581	57563.669088	32.756992
703.637590	57672.430692	32.762010
704.258009	57768.485811	32.767028
704.737901	57858.734150	32.772045
705.306391	57974.057898	32.777063
706.317466	58075.983525	32.782080
707.122154	58180.574873	32.787098
708.134586	58261.342373	32.792116
709.068661	58359.262161	32.797133
709.755055	58473.715369	32.802151
710.574751	58556.482459	32.807168
710.948488	58654.225355	32.812186
711.890469	58746.240157	32.817204
712.730621	58844.803225	32.822221
713.738775	58931.611905	32.827239
714.723195	59027.247901	32.832256
715.200031	59126.672851	32.837274
715.974220	59215.038263	32.842292
716.651330	59302.159618	32.847309
716.936606	59402.058758	32.852327
717.500061	59479.001601	32.857344
718.265100	59597.283513	32.862362
718.989455	59684.848239	32.867380
719.646308	59794.039684	32.872397
720.108987	59890.026616	32.877415
720.831607	59990.093869	32.882432
722.259539	60083.512445	32.887450
722.904595	60172.945954	32.892468
723.758641	60277.323366	32.897485
724.361523	60367.795947	32.902503
725.542003	60457.108667	32.907520
726.006771	60544.223389	32.912538
726.665766	60629.428027	32.917556
727.601772	60712.943803	32.922573
727.822396	60803.889297	32.927591
728.683303	60884.284098	32.932608
728.860799	60985.896667	32.937626
729.848407	61069.310623	32.942644
730.594839	61155.763061	32.947661
731.910521	61247.057767	32.952679
732.864625	61324.495937	32.957696
733.742599	61406.883743	32.962714
734.479561	61483.533506	32.967732
735.410631	61554.664886	32.972749
736.134732	61645.452347	32.977767
736.754747	61721.500807	32.982784
737.347806	61807.226255	32.987802
738.166202	61899.715365	32.992820
738.956488	61971.547325	32.997837
739.451076	62068.677195	33.002855
740.683816	62146.441463	33.007872
741.385842	62224.295414	33.012890
741.960161	62311.449859	33.017908
742.851530	62392.477830	33.022925
743.341442	62478.791483	33.027943
743.984132	62568.385974	33.032960
744.699467	62660.881399	33.037978
745.180877	62751.755227	33.042996
745.832671	62857.947738	33.048013
745.853878	62950.888453	33.053031
746.524996	63047.215850	33.058048
747.295782	63153.397314	33.063066
747.382554	63261.680472	33.068084
748.417900	63374.816721	33.073101
748.934651	63497.688891	33.078119
749.422625	63614.976204	33.083136
750.383518	63732.715453	33.088154
751.353291	63850.314590	33.093172
751.890176	63969.020310	33.098189
752.350450	64088.460296	33.103207
753.413918	64211.991050	33.108224
754.431093	64333.617750	33.113242
754.724783	64458.061613	33.118260
755.575440	64581.551538	33.123277
756.029835	64703.749304	33.128295
757.111567	64817.429250	33.133312
757.912193	64949.937765	33.138330
758.666238	65068.652646	33.143348
759.613510	65180.658572	33.148365
760.090736	65316.068620	33.153383
761.295452	65441.140722	33.158400
761.810838	65562.098518	33.163418
762.749171	65682.135951	33.168436
763.744458	65801.253340	33.173453
764.280053	65923.475933	33.178471
765.766215	66037.724822	33.183488
766.877806	66144.213741	33.188506
767.795230	66248.986070	33.193524
768.853816	66357.978722	33.198541
768.883455	66466.290898	33.203559
769.890448	66567.220034	33.208576
770.761548	66680.042257	33.213594
771.822528	66784.712000	33.218612
772.539963	66882.686623	33.223629
773.695720	66988.994875	33.228647
774.736437	67080.524823	33.233664
775.300569	67181.399106	33.238682
775.791424	67280.620059	33.243700
776.755642	67366.648214	33.248717
777.260921	67452.495261	33.253735
777.913620	67551.103077	33.258752
778.907988	67647.739275	33.263770
779.259826	67745.337563	33.268788
780.209398	67835.776436	33.273805
780.410591	67939.097583	33.278823
781.760414	68043.170043	33.283840
782.542847	68140.544106	33.288858
782.842604	68242.217435	33.293876
783.865812	68337.939930	33.298893
784.385526	68448.659470	33.303911
785.422332	68548.135406	33.308928
786.187848	68653.169296	33.313946
786.549451	68760.052467	33.318964
787.319602	68871.722383	33.323981
787.891239	68983.018619	33.328999
788.909482	69093.453896	33.334016
789.549823	69225.458766	33.339034
789.989901	69338.239830	33.344052
791.029437	69447.786790	33.349069
791.295130	69574.229196	33.354087
792.520337	69689.674975	33.359104
793.322454	69818.238157	33.364122
793.838161	69936.170702	33.369140
795.375712	70046.085451	33.374157
795.922003	70177.622294	33.379175
797.025556	70277.360360	33.384192
797.926749	70395.570228	33.389210
798.918308	70502.342911	33.394228
799.850010	70617.560134	33.399245
800.492275	70731.189426	33.404263
801.378517	70836.802137	33.409280
802.575657	70946.647332	33.414298
803.152253	71070.040368	33.419316
803.790538	71170.171316	33.424333
804.350878	71294.289857	33.429351
805.580054	71399.395186	33.434368
806.865883	71511.521247	33.439386
807.019158	71614.503512	33.444404
807.959067	71726.279367	33.449421
808.608432	71845.105132	33.454439
809.592713	71955.811122	33.459456
810.560338	72063.315822	33.464474
811.473329	72178.694798	33.469492
812.800908	72271.426656	33.474509
813.175767	72390.589166	33.479527
813.902156	72494.625019	33.484544
814.990637	72608.825814	33.489562
815.492109	72719.268625	33.494580
816.195777	72827.945016	33.499597
816.307588	72943.402113	33.504615
817.553225	73070.752802	33.509632
818.600717	73181.466678	33.514650
819.156453	73301.998208	33.519668
820.444163	73409.268248	33.524685
821.088514	73523.175198	33.529703
822.241463	73640.448202	33.534720
822.797642	73742.071006	33.539738
823.324289	73867.954806	33.544756
823.846663	73983.909430	33.549773
824.624552	74102.775823	33.554791
825.744140	74221.931231	33.559808
826.185632	74343.675993	33.564826
826.428808	74483.046273	33.569844
827.662614	74595.522819	33.574861
828.443593	74724.144809	33.579879
828.936048	74853.129261	33.584896
830.229295	74968.802757	33.589914
831.305455	75091.946209	33.594932
832.055519	75201.638318	33.599949
832.987782	75318.231192	33.604967
833.725817	75430.079503	33.609984
834.194470	75549.976070	33.615002
834.867880	75672.906559	33.620020
836.052345	75789.639312	33.625037
836.752241	75910.324633	33.630055
837.583878	76030.533837	33.635072
838.528961	76146.469567	33.640090
839.342727	76277.943973	33.645108
839.982471	76399.058910	33.650125
841.371433	76520.715779	33.655143
841.818043	76643.914191	33.660160
842.514341	76767.542765	33.665178
843.285841	76909.667687	33.670196
844.708634	77021.732017	33.675213
845.372540	77149.573100	33.680231
846.454197	77277.805410	33.685248
847.519778	77391.789375	33.690266
847.892173	77509.163375	33.695284
849.262381	77638.796346	33.700301
849.821237	77764.465168	33.705319
850.809355	77886.431577	33.710336
852.370863	77992.802811	33.715354
853.054864	78115.324586	33.720372
854.257924	78221.322110	33.725389
855.108874	78335.736319	33.730407
855.822335	78456.519427	33.735424
856.913484	78561.598318	33.740442
857.342434	78693.980690	33.745460
858.020633	78803.217108	33.750477
858.825241	78924.393383	33.755495
859.870777	79057.124346	33.760512
860.720707	79172.771045	33.765530
861.346465	79294.509031	33.770548
862.340941	79415.493027	33.775565
863.353184	79543.075289	33.780583
863.736374	79673.315776	33.785600
864.788727	79787.742451	33.790618
865.690190	79910.402810	33.795636
866.580556	80034.205671	33.800653
867.061615	80167.727127	33.805671
867.811823	80299.357359	33.810688
868.929572	80422.302832	33.815706
870.178943	80562.686679	33.820724
870.957512	80685.762435	33.825741
872.158547	80812.814159	33.830759
872.550712	80943.629284	33.835776
874.007806	81060.189629	33.840794
874.678165	81190.822978	33.845812
875.700571	81305.957383	33.850829
876.395023	81428.821510	33.855847
876.892252	81562.727162	33.860864
877.629644	81686.548597	33.865882
878.068436	81828.155298	33.870900
879.269866	81953.222919	33.875917
880.262079	82085.381096	33.880935
881.046600	82220.714610	33.885952
882.050810	82351.681156	33.890970
882.199285	82506.120953	33.895988
883.553594	82632.827443	33.901005
884.997513	82753.565381	33.906023
885.709573	82889.002118	33.911040
886.976169	83018.384857	33.916058
887.489359	83156.109353	33.921076
888.375826	83286.211698	33.926093
889.520403	83401.322813	33.931111
890.440849	83518.078669	33.936128
890.923553	83642.429992	33.941146
891.399174	83770.634900	33.946164
892.149262	83892.829410	33.951181
893.312906	84024.019418	33.956199
894.035201	84160.119461	33.961216
894.839707	84283.979690	33.966234
895.376749	84419.615795	33.971252
896.205092	84558.577464	33.976269
897.150058	84703.312305	33.981287
897.827135	84849.065509	33.986304
898.943061	84985.487954	33.991322
899.836155	85123.948022	33.996340
900.965166	85268.188031	34.001357
901.811818	85406.694737	34.006375
902.550134	85550.376419	34.011392
903.938894	85684.149080	34.016410
905.097850	85832.176038	34.021428
905.763479	85972.944017	34.026445
906.684093	86119.197686	34.031463
908.090785	86256.721048	34.036480
909.067620	86367.511114	34.041498
909.938686	86509.288617	34.046516
910.996373	86649.276164	34.051533
912.550239	86777.122793	34.056551
913.868014	86896.098383	34.061568
914.741250	87009.935763	34.066586
915.514654	87145.889730	34.071604
916.409849	87261.397394	34.076621
917.832324	87383.843470	34.081639
918.155879	87508.502393	34.086656
918.857383	87624.054481	34.091674
920.186676	87750.609899	34.096692
920.807308	87884.322806	34.101709
921.817136	88021.701151	34.106727
922.533382	88152.510926	34.111744
923.252611	88269.621513	34.116762
924.290107	88415.323384	34.121780
924.717421	88537.575228	34.126797
925.966529	88674.108067	34.131815
926.456337	88815.842309	34.136832
927.595074	88949.567609	34.141850
928.675936	89098.446986	34.146868
929.385813	89242.911550	34.151885
930.824938	89391.165999	34.156903
930.941020	89533.976035	34.161920
931.823290	89670.760980	34.166938
932.432103	89817.018419	34.171956
933.437996	89967.130516	34.176973
934.405363	90131.101626	34.181991
935.058825	90285.680908	34.187008
935.532488	90439.123155	34.192026
937.044590	90599.323474	34.197044
937.598691	90754.427671	34.202061
938.653671	90910.480826	34.207079
939.509362	91063.955152	34.212096
940.672652	91226.139860	34.217114
942.061716	91368.062202	34.222132
943.351996	91508.061530	34.227149
945.168486	91643.974057	34.232167
946.291957	91783.100903	34.237184
947.852185	91905.708711	34.242202
948.729440	92033.772542	34.247220
949.089463	92158.723939	34.252237
950.254435	92287.998558	34.257255
951.356863	92422.834970	34.262272
952.357577	92543.530374	34.267290
953.131557	92676.087205	34.272308
953.739911	92795.894439	34.277325
954.535014	92909.867866	34.282343
954.936896	93040.139704	34.287360
955.997045	93172.298978	34.292378
957.303580	93294.609864	34.297396
957.932834	93422.528214	34.302413
959.204511	93549.218432	34.307431
959.956460	93693.646918	34.312448
960.643499	93825.563216	34.317466
961.802413	93961.943909	34.322484
962.330195	94106.206620	34.327501
963.152625	94243.439779	34.332519
964.141380	94392.486286	34.337536
965.041831	94523.776403	34.342554
965.889317	94667.687459	34.347572
966.793471	94821.692706	34.352589
967.643298	94977.709966	34.357607
968.582515	95134.284416	34.362624
969.394598	95284.959995	34.367642
970.364080	95442.519959	34.372660
971.368946	95589.528871	34.377677
972.700715	95742.013985	34.382695
973.063940	95901.952847	34.387712
974.661330	96057.351407	34.392730
975.689446	96214.677904	34.397748
976.395092	96377.886711	34.402765
977.666369	96528.432986	34.407783
978.175609	96700.420809	34.412800
979.533582	96851.348016	34.417818
980.224685	97005.828342	34.422836
981.347597	97177.912824	34.427853
982.624947	97328.423929	34.432871
983.696477	97493.203803	34.437888
984.179316	97651.370744	34.442906
985.727773	97807.634913	34.447924
986.194989	97975.554319	34.452941
987.629521	98141.218795	34.457959
988.662659	98294.675709	34.462976
989.591467	98464.122704	34.467994
990.548638	98621.155315	34.473012
991.612871	98783.851280	34.478029
992.772199	98943.034279	34.483047
993.892572	99110.464377	34.488064
994.673227	99260.580618	34.493082
995.663456	99422.949117	34.498100
996.412863	99584.823686	34.503117
997.160970	99751.884366	34.508135
998.275346	99926.634556	34.513152
999.028905	100090.983132	34.518170
1000.218803	100270.414075	34.523188
1001.225596	100451.332622	34.528205
1002.266523	100608.298392	34.533223
1003.261880	100780.713733	34.538240
1004.113460	100949.501242	34.543258
1005.425272	101122.604164	34.548276
1006.308686	101287.103257	34.553293
1007.555904	101456.947112	34.558311
1009.194912	101633.817636	34.563328
1009.983224	101781.231166	34.568346
1011.263413	101938.520847	34.573364
1012.341082	102100.838281	34.578381
1013.305692	102259.586209	34.583399
1014.486603	102404.278579	34.588416
1015.472552	102573.281603	34.593434
1016.553471	102729.579288	34.598452
1017.400499	102886.953984	34.603469
1018.599397	103042.182337	34.608487
1019.110977	103189.962445	34.613504
1020.202363	103339.998023	34.618522
1021.689986	103483.049538	34.623540
1022.654971	103638.570875	34.628557
1023.600020	103764.718694	34.633575
1024.497261	103917.234322	34.638592
1025.363822	104064.011788	34.643610
1026.436367	104206.205809	34.648628
1027.493033	104359.091543	34.653645
1028.470913	104511.686004	34.658663
1029.279666	104671.306658	34.663680
1030.221690	104828.954568	34.668698
1031.476094	104983.473187	34.673716
1032.386565	105135.421692	34.678733
1033.035505	105307.978176	34.683751
1034.161436	105473.842059	34.688768
1034.645901	105641.962744	34.693786
1035.917387	105807.551874	34.698804
1036.763016	105982.971992	34.703821
1038.239304	106145.094453	34.708839
1039.066482	106313.988995	34.713856
1039.873746	106488.733000	34.718874
1040.990371	106656.949915	34.723892
1041.537215	106841.462153	34.728909
1042.911093	107027.367529	34.733927
1043.951512	107195.738500	34.738944
1044.958093	107381.462371	34.743962
1046.616060	107547.341781	34.748980
1047.232035	107737.325955	34.753997
1048.469924	107916.511380	34.759015
1049.191238	108104.490223	34.764032
1049.965558	108294.452660	34.769050
1051.588199	108473.428557	34.774068
1052.302087	108665.101707	34.779085
1053.639238	108842.881475	34.784103
1054.923565	109020.061733	34.789120
1056.070884	109196.351303	34.794138
1057.394535	109367.199315	34.799156
1058.182288	109542.849462	34.804173
1059.476564	109729.453871	34.809191
1060.526429	109913.979756	34.814208
1061.240713	110105.369050	34.819226
1062.662881	110269.434163	34.824244
1063.528299	110462.767356	34.829261
1065.002907	110642.462299	34.834279
1066.124048	110829.074264	34.839296
1067.022850	111015.049887	34.844314
1068.134062	111184.113787	34.849332
1069.038719	111371.307805	34.854349
1069.992826	111549.110455	34.859367
1070.852715	111737.226496	34.864384
1072.087584	111927.516856	34.869402
1073.344537	112109.802363	34.874420
1073.958501	112298.847600	34.879437
1075.162252	112486.444491	34.884455
1076.448350	112672.875379	34.889472
1077.454538	112864.500092	34.894490
1078.997406	113044.741752	34.899508
1080.407757	113224.548488	34.904525
1081.587071	113401.728951	34.909543
1082.556866	113574.542214	34.914560
1083.588159	113749.160291	34.919578
1084.923909	113919.888671	34.924596
1086.431952	114096.754713	34.929613
1087.477580	114266.845266	34.934631
1088.156664	114430.754003	34.939648
1088.781680	114609.853451	34.944666
1090.499162	114778.864604	34.949684
1091.325773	114949.829691	34.954701
1092.167613	115103.683626	34.959719
1093.416053	115258.527250	34.964736
1094.480014	115425.601691	34.969754
1095.503097	115591.820821	34.974772
1096.467122	115765.139945	34.979789
1097.268813	115933.931943	34.984807
1098.384331	116114.991237	34.989824
1099.566865	116298.882035	34.994842
1100.521377	116468.895520	34.999860
1101.292778	116659.574772	35.004877
1102.010456	116829.893332	35.009895
1103.298681	117017.626972	35.014912
1104.046160	117204.101719	35.019930
1105.176467	117390.530139	35.024948
1106.472982	117576.362681	35.029965
1107.676635	117780.957696	35.034983
1108.595088	117973.256824	35.040000
1109.342137	118174.843213	35.045018
1110.235251	118371.359473	35.050036
1111.551101	118574.545936	35.055053
1112.801760	118770.412117	35.060071
1114.186337	118978.207085	35.065088
1114.988015	119184.204446	35.070106
1116.234011	119383.423208	35.075124
1117.354224	119590.197377	35.080141
1117.908087	119798.634228	35.085159
1119.114699	119999.194240	35.090176
1120.419959	120226.276564	35.095194
1121.349808	120428.201354	35.100212
1122.763736	120648.875941	35.105229
1123.362229	120868.804171	35.110247
1124.896270	121082.993031	35.115264
1126.011274	121297.718022	35.120282
1127.208265	121511.606813	35.125300
1128.226987	121728.683331	35.130317
1129.278945	121955.485562	35.135335
1130.866257	122170.839086	35.140352
1131.833446	122401.069548	35.145370
1133.490234	122610.947119	35.150388
1134.490932	122833.588844	35.155405
1135.630381	123032.690681	35.160423
1136.931445	123255.072085	35.165440
1137.492953	123479.777859	35.170458
1138.743544	123697.678820	35.175476
1140.320223	123909.504045	35.180493
1141.346863	124125.539486	35.185511
1142.720376	124341.280746	35.190528
1143.687517	124555.386823	35.195546
1144.895472	124776.433807	35.200564
1146.068588	124993.998696	35.205581
1147.481464	125208.139935	35.210599
1148.349323	125425.437764	35.215616
1149.566075	125641.870189	35.220634
1150.891723	125859.631499	35.225652
1151.882127	126075.086721	35.230669
1153.165479	126290.091236	35.235687
1154.487351	126498.239945	35.240704
1155.631078	126726.932341	35.245722
1156.419172	126939.404273	35.250740
1157.802498	127147.381705	35.255757
1158.981548	127368.751692	35.260775
1160.667077	127583.217863	35.265792
1161.336453	127801.142905	35.270810
1162.407925	128013.005035	35.275828
1163.909920	128230.408660	35.280845
1165.057397	128445.699360	35.285863
1166.065589	128645.978274	35.290880
1167.029523	128859.878827	35.295898
1168.200811	129064.612909	35.300916
1169.483205	129255.945076	35.305933
1170.222437	129461.662229	35.310951
1171.454568	129664.004385	35.315968
1172.803217	129887.327689	35.320986
1173.720966	130094.656690	35.326004
1174.797165	130304.968947	35.331021
1175.436674	130531.946586	35.336039
1176.772711	130746.115563	35.341056
1178.167547	130967.990823	35.346074
1179.034707	131187.006155	35.351092
1180.410957	131409.495629	35.356109
1181.539905	131634.080478	35.361127
1182.835358	131851.585641	35.366144
1183.356678	132085.530516	35.371162
1184.585839	132312.513992	35.376180
1186.376267	132540.692334	35.381197
1187.183283	132775.890413	35.386215
1188.389862	133005.469508	35.391232
1189.679628	133240.048872	35.396250
1190.984181	133469.183619	35.401268
1192.777916	133707.239461	35.406285
1193.507269	133949.714039	35.411303
1194.890235	134174.500490	35.416320
1196.074394	134413.289989	35.421338
1196.838643	134646.284061	35.426356
1197.965335	134891.099805	35.431373
1199.519257	135130.989962	35.436391
1200.783203	135357.526723	35.441408
1201.743001	135608.514180	35.446426
1203.086060	135837.033208	35.451444
1204.792814	136075.343619	35.456461
1206.350484	136316.038902	35.461479
1207.477281	136540.103146	35.466496
1209.026754	136774.419161	35.471514
1210.199090	136996.143569	35.476532
1211.937929	137227.691226	35.481549
1212.958706	137442.538160	35.486567
1214.675473	137662.302411	35.491584
1215.609013	137887.164852	35.496602
1216.622660	138121.482738	35.501620
1218.355022	138334.674190	35.506637
1218.885142	138573.651224	35.511655
1220.022314	138798.232361	35.516672
1221.171115	139034.018425	35.521690
1222.304466	139267.561862	35.526708
1223.704254	139492.320928	35.531725
1224.929795	139719.798754	35.536743
1226.068608	139955.387914	35.541760
1227.120437	140193.568082	35.546778
1228.186666	140439.996223	35.551796
1229.314940	140670.869564	35.556813
1230.345564	140915.325936	35.561831
1231.848954	141145.749411	35.566848
1232.901501	141402.807003	35.571866
1234.551492	141632.054951	35.576884
1235.625272	141863.044039	35.581901
1236.973048	142100.311580	35.586919
1238.708295	142323.635300	35.591936
1240.122520	142563.280651	35.596954
1241.168581	142797.667084	35.601972
1242.660815	143029.916068	35.606989
1244.156171	143255.946784	35.612007
1245.564459	143482.144460	35.617024
1247.212080	143698.279268	35.622042
1248.116979	143910.584152	35.627060
1250.252742	144121.681910	35.632077
1250.766969	144322.030571	35.637095
1252.039369	144515.610794	35.642112
1253.313754	144722.898743	35.647130
1254.387032	144931.437454	35.652148
1255.651365	145127.851600	35.657165
1256.223966	145349.314752	35.662183
1257.557011	145562.955691	35.667200
1258.273233	145782.316727	35.672218
1259.439194	146011.000570	35.677236
1260.700651	146231.331632	35.682253
1261.319541	146466.208141	35.687271
1262.787271	146692.245833	35.692288
1264.044277	146934.018102	35.697306
1265.308681	147159.721577	35.702324
1266.819907	147390.147116	35.707341
1268.133158	147629.756066	35.712359
1269.212677	147862.180545	35.717376
1270.612084	148110.853492	35.722394
1271.865671	148353.546729	35.727412
1273.101050	148593.908437	35.732429
1274.226794	148852.401230	35.737447
1275.354352	149083.592335	35.742464
1276.676676	149325.860378	35.747482
1277.516826	149583.982543	35.752500
1278.987913	149834.162793	35.757517
1280.370280	150092.951415	35.762535
1281.706531	150351.380387	35.767552
1282.977401	150607.485243	35.772570
1284.102115	150854.817640	35.777588
1285.444142	151117.260456	35.782605
1286.820151	151378.099821	35.787623
1288.048692	151634.939634	35.792640
1289.153870	151899.009948	35.797658
1290.492282	152172.209874	35.802676
1291.751116	152425.380116	35.807693
1293.698752	152705.329233	35.812711
1294.621355	152967.592574	35.817728
1295.603381	153226.039646	35.822746
1296.634222	153499.738469	35.827764
1298.209633	153760.443485	35.832781
1299.732555	154045.162531	35.837799
1300.969075	154311.648173	35.842816
1302.109095	154579.444972	35.847834
1303.716125	154846.801777	35.852852
1305.656663	155108.902917	35.857869
1306.855498	155389.667915	35.862887
1308.101560	155648.376533	35.867904
1309.280933	155916.833454	35.872922
1310.482360	156188.588748	35.877940
1311.836257	156441.063618	35.882957
1313.123918	156720.907059	35.887975
1314.233010	156989.976509	35.892992
1315.683500	157263.881245	35.898010
1316.661400	157539.879699	35.903028
1318.213769	157812.133347	35.908045
1319.416572	158092.897821	35.913063
1320.920154	158380.052915	35.918080
1322.257193	158665.546980	35.923098
1323.479958	158932.296773	35.928116
1324.928494	159193.032924	35.933133
1326.235741	159479.576447	35.938151
1327.927033	159749.481042	35.943168
1329.574463	160013.211009	35.948186
1330.354313	160280.454890	35.953204
1332.445756	160549.843272	35.958221
1333.708654	160821.787358	35.963239
1335.414668	161075.749722	35.968256
1336.816449	161336.260912	35.973274
1337.855026	161586.813091	35.978292
1339.668240	161825.958452	35.983309
1340.653229	162073.842115	35.988327
1341.915769	162329.389680	35.993344
1342.915430	162582.859184	35.998362
1343.694629	162835.589730	36.003380
1344.987485	163088.291636	36.008397
1346.326689	163356.044801	36.013415
1347.555382	163612.580285	36.018432
1348.704045	163877.940436	36.023450
1349.782221	164154.586928	36.028468
1351.074887	164420.688476	36.033485
1352.403168	164715.555388	36.038503
1353.584765	164984.063465	36.043520
1355.375976	165263.662744	36.048538
1356.321875	165559.316887	36.053556
1357.594793	165844.332205	36.058573
1359.240958	166138.304866	36.063591
1360.166324	166427.236769	36.068608
1361.659784	166703.892120	36.073626
1363.094506	167006.687682	36.078644
1364.516403	167297.665834	36.083661
1366.314864	167578.073248	36.088679
1367.906941	167859.720288	36.093696
1369.466493	168133.183998	36.098714
1370.874964	168424.829127	36.103732
1372.500670	168718.168240	36.108749
1373.889725	168996.118599	36.113767
1375.215242	169281.787147	36.118784
1376.682331	169566.190329	36.123802
1378.185485	169851.757120	36.128820
1379.648021	170122.907238	36.133837
1380.928002	170406.644608	36.138855
1382.257075	170692.635515	36.143872
1384.395277	170969.726929	36.148890
1385.279543	171258.392599	36.153908
1387.177330	171536.679206	36.158925
1388.399973	171813.231362	36.163943
1389.601155	172096.517628	36.168960
1390.882908	172384.185729	36.173978
1392.264696	172676.105685	36.178996
1393.602583	172962.751335	36.184013
1394.789607	173246.412268	36.189031
1396.111748	173547.347584	36.194048
1397.584425	173835.587959	36.199066
1398.320713	174134.153813	36.204084
1400.023877	174428.696550	36.209101
1401.190147	174718.181692	36.214119
1402.712625	175028.030676	36.219136
1404.285815	175334.761857	36.224154
1405.237070	175637.515416	36.229172
1406.234977	175947.411904	36.234189
1407.956133	176249.234514	36.239207
1409.270832	176562.677336	36.244224
1410.726749	176873.457961	36.249242
1412.017248	177191.376752	36.254260
1413.379971	177500.650459	36.259277
1414.874849	177811.174455	36.264295
1416.887691	178114.329517	36.269312
1418.813851	178402.514837	36.274330
1420.180915	178707.957218	36.279348
1422.042423	179003.951627	36.284365
1423.551010	179306.605621	36.289383
1424.800716	179614.914036	36.294400
1425.976298	179897.329492	36.299418
1427.456811	180210.073820	36.304436
1428.719757	180503.169956	36.309453
1430.404054	180801.560046	36.314471
1431.597103	181092.230813	36.319488
1432.760724	181370.639828	36.324506
1434.247492	181655.043860	36.329524
1435.678645	181933.438081	36.334541
1436.837066	182216.269723	36.339559
1438.592801	182506.882216	36.344576
1440.103970	182799.921331	36.349594
1441.441773	183096.112498	36.354612
1442.227078	183389.749594	36.359629
1443.759937	183683.880136	36.364647
1444.814407	183989.769874	36.369664
1446.241316	184292.351213	36.374682
1447.570133	184610.061188	36.379700
1448.772233	184925.988675	36.384717
1450.372221	185309.746664	36.389735
1451.639908	185640.702382	36.394752
1453.180799	185955.589465	36.399770
1454.023810	186284.403980	36.404788
1455.361252	186613.878724	36.409805
1457.490194	186939.725481	36.414823
1459.015045	187267.394961	36.419840
1460.605509	187587.613073	36.424858
1462.110816	187917.344963	36.429876
1463.746137	188243.196728	36.434893
1465.524400	188563.032713	36.439911
1467.041482	188892.156084	36.444928
1468.526350	189219.329661	36.449946
1470.149593	189544.882321	36.454964
1471.430092	189860.862889	36.459981
1473.393564	190191.190168	36.464999
1474.875042	190510.163684	36.470016
1476.547146	190821.335714	36.475034
1477.779438	191163.540554	36.480052
1479.365590	191489.714058	36.485069
1481.107992	191802.249270	36.490087
1482.169722	192137.650812	36.495104
1483.963678	192463.565793	36.500122
1485.170045	192789.598999	36.505140
1487.161722	193124.629047	36.510157
1488.424754	193440.875737	36.515175
1489.414203	193776.902596	36.520192
1491.063776	194110.134496	36.525210
1492.474963	194451.837730	36.530228
1493.664839	194793.297072	36.535245
1495.536004	195128.478150	36.540263
1496.485726	195469.011549	36.545280
1498.408561	195806.142113	36.550298
1499.972832	196142.821591	36.555316
1501.890262	196480.919893	36.560333
1504.081069	196802.770021	36.565351
1505.335754	197132.514883	36.570368
1507.079329	197458.754752	36.575386
1508.374747	197784.709866	36.580404
1509.919158	198112.557263	36.585421
1511.770927	198437.283648	36.590439
1512.624255	198771.972128	36.595456
1514.530918	199099.536343	36.600474
1516.121003	199428.446297	36.605492
1517.240419	199768.404292	36.610509
1518.917549	200091.053092	36.615527
1520.306351	200420.199811	36.620544
1521.978772	200752.757501	36.625562
1523.481012	201091.007197	36.630580
1524.784687	201414.936345	36.635597
1526.726734	201729.367324	36.640615
1528.253388	202067.615135	36.645632
1529.570762	202392.687078	36.650650
1531.224358	202720.374255	36.655668
1532.510940	203040.219277	36.660685
1533.963354	203345.889664	36.665703
1535.638185	203661.813807	36.670720
1536.772892	203981.379389	36.675738
1538.361792	204297.546664	36.680756
1539.672189	204624.223978	36.685773
1541.331922	204947.595600	36.690791
1542.436106	205281.698482	36.695808
1543.472432	205610.909777	36.700826
1545.168784	205951.703638	36.705844
1546.734676	206298.081717	36.710861
1548.248253	206626.610234	36.715879
1549.882645	206963.300115	36.720896
1551.326247	207314.068268	36.725914
1553.365666	207653.058281	36.730932
1554.799934	208000.551947	36.735949
1556.565027	208324.877446	36.740967
1558.221882	208683.667096	36.745984
1559.421133	209012.934091	36.751002
1561.114046	209360.922694	36.756020
1562.487038	209709.444504	36.761037
1564.393369	210054.301434	36.766055
1565.667363	210418.386531	36.771072
1567.529463	210770.237231	36.776090
1568.943061	211123.936808	36.781108
1570.486740	211481.528600	36.786125
1571.794552	211836.744407	36.791143
1572.809235	212215.225353	36.796160
1574.836713	212571.269308	36.801178
1576.234341	212932.010290	36.806196
1578.087650	213302.536961	36.811213
1579.794899	213671.410254	36.816231
1581.296585	214048.038830	36.821248
1582.859700	214414.877754	36.826266
1584.429060	214781.766867	36.831284
1585.770691	215158.447015	36.836301
1587.522528	215519.846449	36.841319
1589.346448	215897.188508	36.846336
1590.788272	216260.821819	36.851354
1592.591697	216655.925013	36.856372
1594.084711	217039.340531	36.861389
1596.182234	217411.560237	36.866407
1597.280593	217793.869516	36.871424
1598.925866	218169.285217	36.876442
1600.519016	218547.148103	36.881460
1601.911479	218928.141917	36.886477
1603.969978	219304.814662	36.891495
1605.463955	219692.118622	36.896512
1607.124420	220077.008757	36.901530
1608.610844	220445.388309	36.906548
1610.094542	220835.641315	36.911565
1611.577675	221214.538974	36.916583
1613.523977	221605.685252	36.921600
1615.125473	221994.319825	36.926618
1617.367312	222377.468645	36.931636
1618.836062	222763.685434	36.936653
1620.648536	223140.423612	36.941671
1622.133733	223511.929039	36.946688
1623.850265	223893.763188	36.951706
1625.375165	224278.269405	36.956724
1626.632965	224664.036857	36.961741
1628.521041	225033.447080	36.966759
1630.506790	225409.523303	36.971776
1632.368253	225773.120163	36.976794
1634.417582	226144.689896	36.981812
1636.233945	226509.665595	36.986829
1637.764814	226880.732107	36.991847
1639.369611	227234.740863	36.996864
1641.314269	227596.571635	37.001882
1642.750086	227932.976285	37.006900
1644.304887	228283.486901	37.011917
1645.797361	228621.864045	37.016935
1647.394921	228974.095260	37.021952
1648.891156	229307.162174	37.026970
1650.912518	229650.892703	37.031988
1652.718051	230005.936269	37.037005
1654.088235	230357.694493	37.042023
1655.495375	230711.961778	37.047040
1657.002670	231067.076960	37.052058
1658.532641	231419.597210	37.057076
1659.948446	231791.137304	37.062093
1661.455693	232144.270414	37.067111
1663.205114	232523.277424	37.072128
1664.543790	232898.080604	37.077146
1666.283000	233264.767809	37.082164
1667.830492	233654.068799	37.087181
1669.306177	234031.186869	37.092199
1670.796815	234425.043422	37.097216
1672.339654	234806.900863	37.102234
1673.644845	235194.866662	37.107252
1675.075225	235591.043325	37.112269
1676.824479	235990.091121	37.117287
1678.493565	236403.173895	37.122304
1680.063821	236808.040881	37.127322
1682.300290	237207.925648	37.132340
1683.514337	237627.251300	37.137357
1685.685189	238037.154380	37.142375
1687.309629	238453.366319	37.147392
1688.705449	238864.075513	37.152410
1690.491923	239271.420561	37.157428
1692.104280	239713.188558	37.162445
1693.573994	240122.538041	37.167463
1695.501648	240544.643954	37.172480
1696.786259	240977.163588	37.177498
1698.599828	241402.588421	37.182516
1699.969239	241845.584883	37.187533
1701.637138	242270.141928	37.192551
1703.112740	242709.335130	37.197568
1704.892406	243159.098425	37.202586
1706.893680	243600.011299	37.207604
1708.575032	244044.860029	37.212621
1710.387014	244497.028861	37.217639
1712.442607	244936.076123	37.222656
1713.961093	245384.249923	37.227674
1715.718135	245817.321555	37.232692
1717.387220	246284.293248	37.237709
1719.134075	246723.994595	37.242727
1720.807236	247170.361945	37.247744
1722.695773	247618.218679	37.252762
1724.974575	248062.787130	37.257780
1726.446062	248516.244654	37.262797
1728.054197	248958.959835	37.267815
1729.798042	249402.744943	37.272832
1731.610719	249857.009237	37.277850
1732.922403	250300.732594	37.282868
1734.701699	250762.239234	37.287885
1736.610402	251224.486359	37.292903
1738.644133	251671.191983	37.297920
1739.974739	252115.618578	37.302938
1741.718740	252575.321864	37.307956
1743.761832	253025.883127	37.312973
1745.347585	253484.770110	37.317991
1747.323517	253929.395120	37.323008
1749.263221	254387.792010	37.328026
1751.132744	254836.317251	37.333044
1752.265748	255287.496425	37.338061
1754.140082	255717.830706	37.343079
1755.962510	256155.715869	37.348096
1757.791513	256598.627965	37.353114
1759.590582	257017.666335	37.358132
1761.504163	257462.518122	37.363149
1763.089292	257880.672715	37.368167
1764.796718	258313.818597	37.373184
1766.920598	258745.881771	37.378202
1769.138978	259172.111908	37.383220
1771.237684	259605.826996	37.388237
1773.201933	260020.435085	37.393255
1775.391862	260438.511635	37.398272
1777.288169	260863.846276	37.403290
1778.959242	261275.396951	37.408308
1780.837563	261697.911895	37.413325
1782.195983	262112.023045	37.418343
1783.904448	262540.022359	37.423360
1785.739733	262967.517564	37.428378
1787.319233	263390.479187	37.433396
1788.691106	263832.648243	37.438413
1790.244174	264275.269692	37.443431
1792.042640	264713.913985	37.448448
1792.974547	265167.906122	37.453466
1794.819612	265622.693120	37.458484
1796.789681	266084.087637	37.463501
1798.501157	266547.831787	37.468519
1800.129050	267009.021579	37.473536
1802.044705	267480.450591	37.478554
1804.279485	267940.448869	37.483572
1806.163677	268400.601394	37.488589
1807.882335	268874.365625	37.493607
1809.924263	269327.555236	37.498624
1811.456358	269800.429628	37.503642
1813.370014	270267.908339	37.508660
1815.232362	270747.761343	37.513677
1816.525998	271227.218227	37.518695
1818.598094	271698.906095	37.523712
1820.477021	272170.774047	37.528730
1822.458354	272651.715594	37.533748
1824.496613	273132.036025	37.538765
1826.322457	273607.383816	37.543783
1828.390651	274081.497368	37.548800
1830.188231	274563.345739	37.553818
1831.946053	275036.181806	37.558836
1833.507272	275517.756835	37.563853
1835.628405	276007.139589	37.568871
1837.374752	276484.895877	37.573888
1839.156099	276980.827224	37.578906
1840.963332	277453.108066	37.583924
1842.852461	277946.121360	37.588941
1844.456802	278433.690696	37.593959
1846.296278	278913.753968	37.598976
1847.864354	279418.185096	37.603994
1850.277464	279908.132546	37.609012
1851.778270	280402.003346	37.614029
1853.490906	280904.319471	37.619047
1855.498333	281394.345973	37.624064
1857.645998	281889.984733	37.629082
1859.691920	282371.821689	37.634100
1861.798248	282872.462756	37.639117
1863.823207	283364.783914	37.644135
1865.706891	283847.169503	37.649152
1867.328957	284345.971350	37.654170
1869.141482	284826.431386	37.659188
1871.057387	285331.350641	37.664205
1872.856588	285818.661866	37.669223
1874.945644	286299.728439	37.674240
1876.834131	286784.428654	37.679258
1878.504516	287255.523864	37.684276
1880.641752	287725.501586	37.689293
1882.491305	288177.137276	37.694311
1885.049545	288637.088957	37.699328
1886.615794	289098.817629	37.704346
1888.806947	289551.050419	37.709364
1890.823755	290007.166717	37.714381
1892.813115	290458.586696	37.719399
1894.701915	290915.833632	37.724416
1896.653175	291367.049878	37.729434
1898.591632	291817.985539	37.734452
1900.454878	292282.818073	37.739469
1901.999745	292754.755288	37.744487
1903.940215	293207.838497	37.749504
1905.562298	293681.863729	37.754522
1907.289916	294158.356841	37.759540
1909.165094	294626.749282	37.764557
1910.837508	295109.565264	37.769575
1912.630053	295591.596800	37.774592
1914.464498	296076.308963	37.779610
1915.723588	296577.203271	37.784628
1917.394666	297078.384169	37.789645
1919.611939	297582.902550	37.794663
1921.118827	298083.617880	37.799680
1923.056826	298596.548790	37.804698
1924.815414	299119.530978	37.809716
1927.543275	299640.452540	37.814733
1929.186194	300151.079603	37.819751
1931.066269	300665.066561	37.824768
1932.679012	301183.380739	37.829786
1934.649355	301712.727633	37.834804
1936.671581	302236.044751	37.839821
1938.079521	302777.197251	37.844839
1940.376528	303302.187029	37.849856
1942.221387	303847.524845	37.854874
1944.286265	304389.040197	37.859892
1946.275182	304929.064071	37.864909
1948.344437	305468.409697	37.869927
1950.559967	305997.979319	37.874944
1952.966578	306536.245452	37.879962
1954.848876	307065.348324	37.884980
1956.985348	307601.462305	37.889997
1958.927239	308148.947031	37.895015
1961.112710	308680.117384	37.900032
1963.282686	309213.797233	37.905050
1965.351903	309748.451502	37.910068
1967.100648	310269.545429	37.915085
1968.782177	310800.162236	37.920103
1971.130625	311338.105453	37.925120
1973.100970	311881.330171	37.930138
1974.899606	312423.864837	37.935156
1976.863777	312960.504487	37.940173
1978.964731	313502.928548	37.945191
1980.868396	314052.584927	37.950208
1983.596088	314580.381105	37.955226
1985.344210	315120.836310	37.960244
1986.753860	315647.328985	37.965261
1988.655043	316194.777329	37.970279
1990.526085	316742.883541	37.975296
1992.310047	317293.965844	37.980314
1994.553991	317838.345803	37.985332
1996.781900	318389.776399	37.990349
1998.350207	318933.411055	37.995367
2000.396019	319479.425738	38.000384
2002.770588	320027.843589	38.005402
2004.608304	320579.789568	38.010420
2006.512977	321123.267892	38.015437
2008.559839	321675.598357	38.020455
2010.908987	322195.952685	38.025472
2012.182717	322722.304993	38.030490
2014.655714	323253.664772	38.035508
2016.684796	323768.238913	38.040525
2018.682151	324298.746267	38.045543
2021.029040	324830.815989	38.050560
2022.823082	325344.671376	38.055578
2024.919094	325865.704246	38.060596
2026.920369	326399.811988	38.065613
2028.802296	326931.774709	38.070631
2030.886378	327468.164154	38.075648
2033.205432	328000.018901	38.080666
2034.587051	328543.633090	38.085684
2037.090746	329071.334454	38.090701
2038.760210	329626.660622	38.095719
2040.589034	330172.110439	38.100736
2042.621180	330719.245918	38.105754
2044.392647	331277.855940	38.110772
2046.556632	331839.948068	38.115789
2048.336212	332412.696082	38.120807
2050.710834	332964.083945	38.125824
2052.720165	333532.009920	38.130842
2054.486286	334103.263126	38.135860
2056.719139	334682.298335	38.140877
2058.330435	335260.939823	38.145895
2060.602928	335838.657111	38.150912
2062.391797	336424.279011	38.155930
2064.125610	337016.672704	38.160948
2066.064721	337605.980867	38.165965
2068.155005	338211.793435	38.170983
2070.275304	338806.075859	38.176000
2072.167288	339405.000340	38.181018
2074.523020	340016.473082	38.186036
2076.527248	340620.280010	38.191053
2078.852753	341238.254604	38.196071
2081.034887	341845.411240	38.201088
2082.948714	342464.924951	38.206106
2085.417092	343079.395471	38.211124
2087.591104	343691.720116	38.216141
2089.972305	344291.194610	38.221159
2092.555362	344903.205389	38.226176
2094.655987	345496.793807	38.231194
2096.899075	346108.785323	38.236212
2099.338161	346692.257728	38.241229
2101.451104	347292.532527	38.246247
2103.921573	347883.890870	38.251264
2106.425559	348492.222565	38.256282
2108.290881	349101.175460	38.261300
2110.161187	349672.082328	38.266317
2112.270645	350280.468012	38.271335
2114.131559	350875.874073	38.276352
2116.749356	351487.073458	38.281370
2118.501640	352086.961966	38.286388
2120.805120	352679.197645	38.291405
2122.954031	353287.266896	38.296423
2124.741872	353881.082096	38.301440
2127.104144	354474.897692	38.306458
2129.122315	355089.747144	38.311476
2131.078176	355692.096135	38.316493
2133.008878	356294.183925	38.321511
2134.962837	356908.652665	38.326528
2137.253146	357523.791710	38.331546
2139.325829	358135.454307	38.336564
2141.311456	358740.831825	38.341581
2143.260597	359365.569051	38.346599
2145.283655	359982.297330	38.351616
2147.820396	360599.490286	38.356634
2149.838609	361210.009480	38.361652
2152.070836	361805.401788	38.366669
2154.136298	362391.202288	38.371687
2156.072696	362985.907549	38.376704
2158.498662	363578.724774	38.381722
2160.220924	364175.517782	38.386740
2162.473941	364775.915753	38.391757
2164.588614	365373.915406	38.396775
2166.940801	365976.908742	38.401792
2169.321279	366575.754319	38.406810
2170.999983	367183.718781	38.411828
2173.025332	367787.460198	38.416845
2175.376108	368400.437847	38.421863
2177.018934	369014.932050	38.426880
2179.508837	369641.924681	38.431898
2181.371943	370245.740458	38.436916
2183.617368	370883.537918	38.441933
2185.939690	371510.438949	38.446951
2187.832356	372147.046452	38.451968
2190.414606	372768.430916	38.456986
2192.549889	373402.539213	38.462004
2194.821167	374039.145099	38.467021
2196.713959	374677.872797	38.472039
2199.143800	375318.654872	38.477056
2201.397048	375970.722794	38.482074
2203.119867	376623.161916	38.487092
2205.502948	377265.880972	38.492109
2207.745336	377929.454495	38.497127
2210.138080	378593.671880	38.502144
2212.064756	379249.839811	38.507162
2214.195406	379926.679203	38.512180
2216.437902	380587.678326	38.517197
2218.744851	381255.767935	38.522215
2220.940059	381927.479743	38.527232
2223.797690	382593.093317	38.532250
2225.548538	383280.010432	38.537268
2227.967630	383937.072204	38.542285
2230.424978	384615.536157	38.547303
2232.246060	385290.282908	38.552320
2235.055619	385954.575630	38.557338
2237.684862	386626.298749	38.562356
2240.036995	387287.741051	38.567373
2242.481302	387972.726003	38.572391
2244.805147	388634.592870	38.577408
2247.343342	389298.206312	38.582426
2250.096380	389959.995958	38.587444
2252.180326	390622.986526	38.592461
2254.811333	391271.796601	38.597479
2257.051578	391934.068936	38.602496
2259.417771	392586.986898	38.607514
2261.562986	393251.516701	38.612532
2263.829790	393905.022224	38.617549
2266.079575	394561.449179	38.622567
2268.527231	395209.321612	38.627584
2271.019123	395863.194151	38.632602
2272.827859	396527.179442	38.637620
2274.903762	397185.181285	38.642637
2277.353222	397843.561936	38.647655
2279.127094	398511.597255	38.652672
2282.238524	399161.788526	38.657690
2284.181086	399826.874492	38.662708
2286.425910	400492.045975	38.667725
2288.522198	401151.198306	38.672743
2290.918068	401821.015113	38.677760
2293.579806	402480.597634	38.682778
2295.619090	403138.740156	38.687796
2298.038377	403800.903608	38.692813
2300.148618	404459.300459	38.697831
2302.327642	405111.847592	38.702848
2304.503432	405753.597383	38.707866
2306.632982	406400.396446	38.712884
2308.869500	407045.540786	38.717901
2311.028094	407684.606515	38.722919
2312.917177	408332.601522	38.727936
2315.085353	408973.399565	38.732954
2316.889624	409642.114597	38.737972
2318.895582	410303.390852	38.742989
2321.105415	410976.251720	38.748007
2323.358919	411657.989153	38.753024
2325.714661	412343.230508	38.758042
2327.604903	413025.639424	38.763060
2329.651681	413719.030224	38.768077
2332.639727	414412.504323	38.773095
2334.894198	415111.685482	38.778112
2337.388659	415796.187942	38.783130
2340.117092	416503.190611	38.788148
2342.121159	417220.803329	38.793165
2344.319133	417927.537808	38.798183
2346.729553	418638.311863	38.803200
2349.136025	419357.053003	38.808218
2351.357470	420069.021673	38.813236
2353.559303	420786.481130	38.818253
2355.966889	421513.592626	38.823271
2358.478890	422253.758845	38.828288
2360.827215	422967.832606	38.833306
2363.325576	423700.768487	38.838324
2365.505651	424427.407651	38.843341
2368.043744	425166.806847	38.848359
2370.228573	425905.728685	38.853376
2372.857451	426644.806736	38.858394
2375.304720	427394.502236	38.863412
2377.817131	428130.106044	38.868429
2380.488638	428869.954534	38.873447
2382.664752	429619.709784	38.878464
2385.680908	430358.488337	38.883482
2388.078925	431105.675651	38.888500
2390.051256	431836.828660	38.893517
2392.632783	432586.306269	38.898535
2394.951826	433334.785328	38.903552
2397.769413	434085.482211	38.908570
2400.319884	434836.646535	38.913588
2402.808488	435576.421429	38.918605
2405.448192	436317.407438	38.923623
2407.819767	437058.255089	38.928640
2410.698815	437783.533400	38.933658
2413.324326	438534.086020	38.938676
2415.509375	439265.984361	38.943693
2417.974192	440014.785501	38.948711
2420.427669	440753.404307	38.953728
2423.084138	441481.353699	38.958746
2425.655543	442216.562118	38.963764
2427.927760	442957.344661	38.968781
2430.852185	443681.832125	38.973799
2432.587291	444421.276255	38.978816
2435.301459	445146.900711	38.983834
2437.779580	445887.886809	38.988852
2440.595442	446634.799845	38.993869
2442.736973	447353.911380	38.998887
2444.986819	448090.500502	39.003904
2447.707265	448823.905729	39.008922
2449.982464	449557.603230	39.013940
2452.324686	450294.289829	39.018957
2454.973231	451021.759451	39.023975
2457.280981	451769.448029	39.028992
2459.779638	452505.564474	39.034010
2461.778268	453252.633112	39.039028
2464.054206	453989.580889	39.044045
2466.363972	454710.086589	39.049063
2468.574313	455431.840205	39.054080
2470.860579	456146.586522	39.059098
2473.597016	456869.662223	39.064116
2476.299903	457574.089091	39.069133
2478.883471	458297.886257	39.074151
2481.001087	459022.482979	39.079168
2483.881407	459731.235225	39.084186
2486.402454	460470.191332	39.089204
2488.800079	461202.019834	39.094221
2491.321800	461923.302097	39.099239
2493.630775	462655.687482	39.104256
2496.218564	463392.387134	39.109274
2498.582072	464130.300584	39.114292
2501.280234	464877.058992	39.119309
2503.707107	465601.982729	39.124327
2505.650719	466363.927212	39.129344
2507.954623	467116.398100	39.134362
2510.501909	467886.854691	39.139380
2512.433925	468648.746700	39.144397
2515.094179	469418.004650	39.149415
2517.421465	470200.290644	39.154432
2519.935503	470988.108008	39.159450
2522.411835	471778.566043	39.164468
2524.791016	472578.682809	39.169485
2527.188910	473367.462269	39.174503
2529.389151	474180.436522	39.179520
2531.828809	474986.424977	39.184538
2534.623442	475796.300408	39.189556
2537.291020	476618.405335	39.194573
2539.909928	477430.393316	39.199591
2542.375626	478246.194896	39.204608
2544.995914	479067.727043	39.209626
2547.724220	479887.536297	39.214644
2550.482827	480716.219098	39.219661
2553.434087	481535.252400	39.224679
2555.745473	482377.323246	39.229696
2558.063132	483197.376439	39.234714
2560.984247	484018.854094	39.239732
2563.240266	484860.849503	39.244749
2566.415519	485687.741395	39.249767
2569.132011	486520.605683	39.254784
2571.622181	487349.933615	39.259802
2574.263400	488189.520121	39.264820
2577.245486	489027.546231	39.269837
2579.778082	489853.809621	39.274855
2582.290143	490690.860288	39.279872
2584.624222	491525.676296	39.284890
2587.528551	492351.291535	39.289908
2590.098952	493191.618588	39.294925
2592.342734	494023.338448	39.299943
2594.830696	494876.877715	39.304960
2597.230119	495714.974310	39.309978
2600.445973	496557.376763	39.314996
2602.794387	497417.840087	39.320013
2605.522241	498250.001927	39.325031
2607.916588	499099.435178	39.330048
2610.409472	499959.223327	39.335066
2613.239876	500807.784180	39.340084
2615.833658	501654.218540	39.345101
2618.199070	502501.092052	39.350119
2621.022652	503347.944835	39.355136
2623.504277	504200.286300	39.360154
2626.594825	505066.973670	39.365172
2629.000562	505920.281235	39.370189
2631.736582	506770.819434	39.375207
2634.233546	507624.916049	39.380224
2636.659100	508467.452030	39.385242
2639.210461	509297.945709	39.390260
2641.538710	510119.169877	39.395277
2644.175823	510948.395602	39.400295
2646.740827	511782.210538	39.405312
2648.911950	512610.706242	39.410330
2652.174470	513448.536740	39.415348
2654.151013	514294.915396	39.420365
2657.127018	515141.890392	39.425383
2660.016742	515978.418878	39.430400
2662.469940	516820.243679	39.435418
2665.372179	517658.829503	39.440436
2667.955317	518513.449915	39.445453
2670.721848	519365.876717	39.450471
2672.960831	520221.599587	39.455488
2676.307342	521071.164301	39.460506
2679.526425	521924.012374	39.465524
2682.244846	522781.910041	39.470541
2685.216298	523631.170477	39.475559
2687.752458	524486.625481	39.480576
2690.004429	525345.486612	39.485594
2692.754706	526199.039370	39.490612
2695.230203	527064.084612	39.495629
2698.329418	527927.368078	39.500647
2700.980591	528804.930735	39.505664
2703.731864	529675.085690	39.510682
2706.363343	530546.205967	39.515700
2708.999768	531429.219982	39.520717
2711.692892	532308.298340	39.525735
2714.224061	533194.523084	39.530752
2716.893071	534082.071388	39.535770
2719.555675	534970.362849	39.540788
2722.254874	535874.100241	39.545805
2724.997237	536761.050244	39.550823
2727.389212	537676.053621	39.555840
2729.876568	538583.547637	39.560858
2732.792170	539500.194889	39.565876
2735.424869	540421.035570	39.570893
2738.159607	541332.358697	39.575911
2741.105376	542259.288740	39.580928
2743.461988	543188.199163	39.585946
2746.393457	544119.609689	39.590964
2748.957069	545055.773988	39.595981
2752.184217	545992.516369	39.600999
2754.901341	546924.000774	39.606016
2757.410513	547859.911270	39.611034
2760.289375	548795.441964	39.616052
2763.421610	549753.127611	39.621069
2765.897993	550685.417430	39.626087
2768.620938	551630.032287	39.631104
2771.262022	552582.157157	39.636122
2774.340491	553528.824672	39.641140
2777.403674	554472.312333	39.646157
2780.708105	555416.239670	39.651175
2783.500118	556344.785666	39.656192
2786.499471	557283.400973	39.661210
2789.501604	558220.037663	39.666228
2792.834639	559160.206806	39.671245
2795.389477	560095.412532	39.676263
2798.550865	561030.850224	39.681280
2801.212205	561939.088901	39.686298
2804.028086	562856.199979	39.691316
2806.873292	563782.501282	39.696333
2809.486353	564702.454636	39.701351
2812.366663	565629.956058	39.706368
2815.053078	566564.925393	39.711386
2817.935890	567492.828290	39.716404
2820.178771	568419.555021	39.721421
2823.037858	569339.502143	39.726439
2826.332575	570248.193728	39.731456
2828.742342	571137.579205	39.736474
2831.334303	572024.864756	39.741492
2834.166084	572927.709303	39.746509
2836.537005	573826.400309	39.751527
2839.106827	574739.100727	39.756544
2841.843969	575655.153819	39.761562
2844.506786	576566.190657	39.766580
2846.807035	577494.470529	39.771597
2849.599268	578428.299424	39.776615
2852.448862	579363.041667	39.781632
2854.798275	580312.238581	39.786650
2857.388582	581261.866815	39.791668
2860.387915	582224.051767	39.796685
2863.169415	583190.237228	39.801703
2866.103839	584151.263985	39.806720
2868.939145	585141.219299	39.811738
2871.995603	586104.255454	39.816756
2874.854120	587091.430898	39.821773
2877.826601	588073.200873	39.826791
2880.390802	589055.795432	39.831808
2883.156910	590058.657956	39.836826
2886.250401	591046.335671	39.841844
2889.250425	592064.664674	39.846861
2892.369290	593062.645151	39.851879
2895.302608	594065.157200	39.856896
2898.256085	595084.804221	39.861914
2901.402254	596093.685115	39.866932
2904.199425	597105.520861	39.871949
2906.912504	598141.391286	39.876967
2909.763067	599162.209318	39.881984
2912.287032	600190.667606	39.887002
2914.973334	601217.801395	39.892020
2918.071900	602263.437863	39.897037
2920.870647	603311.811092	39.902055
2924.118965	604352.771868	39.907072
2926.737945	605403.706259	39.912090
2929.716087	606449.038864	39.917108
2932.861389	607514.743706	39.922125
2935.863383	608569.086267	39.927143
2938.850859	609629.108325	39.932160
2941.549611	610696.546366	39.937178
2944.624477	611754.089011	39.942196
2947.593299	612836.968250	39.947213
2950.272000	613906.564297	39.952231
2953.692387	614963.517344	39.957248
2956.795638	616045.581753	39.962266
2960.017210	617116.246303	39.967284
2962.863441	618196.273820	39.972301
2966.320944	619263.829946	39.977319
2969.245247	620325.275725	39.982336
2972.304778	621395.404713	39.987354
2975.473546	622478.402275	39.992372
2978.187670	623546.757319	39.997389
2981.422980	624618.599954	40.002407
2984.790528	625674.717251	40.007424
2987.891088	626738.131276	40.012442
2991.268276	627789.137754	40.017460
2994.186745	628850.108270	40.022477
2997.193299	629911.496040	40.027495
3000.234259	630974.603031	40.032512
3003.075933	632031.253425	40.037530
3006.545445	633086.892900	40.042548
3009.418682	634147.583946	40.047565
3012.170052	635205.190923	40.052583
3015.590289	636264.117597	40.057600
3018.389510	637318.397244	40.062618
3021.055642	638359.848307	40.067636
3024.164220	639379.035900	40.072653
3027.050992	640405.456735	40.077671
3029.900257	641430.478295	40.082688
3032.372481	642461.013989	40.087706
3034.926683	643479.841375	40.092724
3037.955162	644518.015140	40.097741
3040.911138	645568.259109	40.102759
3043.489279	646610.790630	40.107776
3046.590114	647672.399640	40.112794
3049.131010	648736.556760	40.117812
3052.169959	649812.582668	40.122829
3054.749242	650894.066630	40.127847
3057.929136	651983.224249	40.132864
3060.620245	653074.313864	40.137882
3063.399391	654179.010798	40.142900
3066.345131	655296.751316	40.147917
3069.049262	656413.398192	40.152935
3072.027356	657534.478942	40.157952
3075.468421	658675.990189	40.162970
3078.525484	659817.663609	40.167988
3081.676933	660961.160279	40.173005
3084.706909	662113.754968	40.178023
3087.928458	663264.284902	40.183040
3090.910660	664426.554491	40.188058
3094.137960	665584.962988	40.193076
3097.632409	666752.844418	40.198093
3100.627349	667923.919696	40.203111
3104.205980	669084.635305	40.208128
3107.710711	670263.692590	40.213146
3110.650345	671432.668551	40.218164
3114.244534	672604.455849	40.223181
3117.349746	673774.822755	40.228199
3120.349141	674949.900845	40.233216
3123.305418	676136.512206	40.238234
3126.497547	677309.997911	40.243252
3129.856935	678504.040619	40.248269
3132.825054	679699.511230	40.253287
3136.019527	680876.513547	40.258304
3139.174199	682065.383946	40.263322
3142.788741	683254.261966	40.268340
3146.265857	684454.520828	40.273357
3149.386352	685648.628182	40.278375
3152.401628	686832.293192	40.283392
3155.369506	688032.562189	40.288410
3158.487651	689235.205294	40.293428
3162.011579	690439.093304	40.298445
3164.938885	691642.552832	40.303463
3168.263328	692838.459229	40.308480
3171.082681	694045.735162	40.313498
3174.750967	695251.217796	40.318516
3177.725123	696454.555740	40.323533
3180.799193	697675.729487	40.328551
3184.366099	698875.553265	40.333568
3187.475960	700085.442897	40.338586
3191.109333	701291.859727	40.343604
3194.071219	702502.939559	40.348621
3197.333721	703720.354068	40.353639
3200.710848	704912.297190	40.358656
3203.775766	706125.674118	40.363674
3207.458620	707333.934111	40.368692
3211.053018	708533.884310	40.373709
3214.360563	709738.481208	40.378727
3217.656810	710930.123303	40.383744
3221.148579	712124.265862	40.388762
3224.586503	713320.058799	40.393780
3227.848037	714517.125647	40.398797
3230.861112	715697.685088	40.403815
3233.977211	716869.031374	40.408832
3237.136131	718043.642634	40.413850
3240.243828	719187.639609	40.418868
3243.856754	720324.098044	40.423885
3247.146466	721463.836921	40.428903
3250.548319	722600.532816	40.433920
3253.387988	723745.713955	40.438938
3256.455446	724881.137776	40.443956
3259.654718	726020.308815	40.448973
3262.763124	727171.576240	40.453991
3266.411939	728317.319213	40.459008
3269.638769	729476.630340	40.464026
3272.452411	730631.007002	40.469044
3275.885209	731793.912468	40.474061
3278.899343	732961.078966	40.479079
3282.317656	734132.326208	40.484096
3285.673215	735309.936776	40.489114
3288.731373	736497.384229	40.494132
3292.468028	737676.672570	40.499149
3295.379522	738865.138548	40.504167
3299.016054	740035.123010	40.509184
3302.125608	741238.697946	40.514202
3305.219969	742434.465538	40.519220
3308.666209	743620.604023	40.524237
3311.743515	744836.799314	40.529255
3315.228858	746050.371141	40.534272
3318.444766	747270.014521	40.539290
3321.612696	748493.434047	40.544308
3325.056241	749713.511986	40.549325
3328.108784	750941.537392	40.554343
3331.816317	752180.824136	40.559360
3334.619828	753428.177007	40.564378
3338.107996	754677.999024	40.569396
3341.368290	755931.705292	40.574413
3344.505643	757187.561418	40.579431
3347.663646	758445.788160	40.584448
3351.285956	759709.204694	40.589466
3354.182939	760993.275906	40.594484
3357.568718	762264.057605	40.599501
3360.767896	763561.518720	40.604519
3363.872263	764850.137056	40.609536
3367.538818	766143.372113	40.614554
3370.473049	767450.231507	40.619572
3373.708674	768758.068775	40.624589
3376.928965	770072.313076	40.629607
3380.200837	771388.058658	40.634624
3383.144838	772715.925421	40.639642
3386.705220	774049.891188	40.644660
3390.059823	775387.000616	40.649677
3393.530973	776726.369874	40.654695
3396.913231	778068.566380	40.659712
3400.657441	779409.218278	40.664730
3403.757046	780772.512804	40.669748
3407.664298	782118.459880	40.674765
3410.948369	783472.045173	40.679783
3414.434418	784816.489567	40.684800
3417.923848	786178.718448	40.689818
3421.411861	787524.761928	40.694836
3425.161874	788873.222445	40.699853
3428.707315	790232.803157	40.704871
3432.241923	791575.867052	40.709888
3435.903950	792917.807327	40.714906
3439.205011	794273.420114	40.719924
3442.367786	795616.443804	40.724941
3445.867705	796966.738076	40.729959
3449.216898	798318.869416	40.734976
3453.144463	799663.809574	40.739994
3456.485468	801016.059348	40.745012
3460.009428	802340.702579	40.750016
3463.307059	803636.274717	40.755021
3466.731354	804869.997070	40.760026
3469.748549	806053.938573	40.765031
3472.695652	807191.194890	40.770036
3476.070342	808258.893128	40.775040
3478.829386	809263.081293	40.780045
3481.846918	810188.151719	40.785050
3484.706179	811077.727386	40.790055
3487.237898	811889.355436	40.795060
3489.201905	812631.484299	40.800064
3492.037075	813337.920682	40.805069
3493.897896	813974.571748	40.810074
3496.249960	814553.310012	40.815079
3497.962868	815092.642028	40.820084
3499.914671	815552.698826	40.825088
3501.823131	815997.241889	40.830093
3503.342724	816374.515103	40.835098
3504.835165	816709.990049	40.840103
3506.280915	817014.778311	40.845108
3507.458465	817258.244325	40.850112
3509.093724	817481.180171	40.855117
3509.656588	817666.786844	40.860122
3510.896932	817819.662730	40.865127
3511.560802	817933.482494	40.870132
3512.449803	818026.136121	40.875136
3513.064741	818101.499904	40.880141
3514.093136	818133.859670	40.885146
3514.647515	818148.572733	40.890151
3514.996671	818149.881318	40.895156
3515.629398	818109.277966	40.900160
3516.052427	818096.554170	40.905165
3516.530652	818021.506365	40.910170
3517.184704	817941.756436	40.915175
3517.125716	817863.577510	40.920180
3517.624624	817756.780348	40.925184
3517.816277	817646.621291	40.930189
3518.259578	817514.706098	40.935194
3518.384755	817374.073792	40.940199
3518.587179	817238.879542	40.945204
3518.722876	817078.081109	40.950208
3519.247701	816918.581092	40.955213
3519.181045	816741.250038	40.960218
3519.222148	816556.397976	40.965223
3519.176764	816380.222013	40.970228
3519.347526	816189.495162	40.975232
3519.032409	815987.345237	40.980237
3519.400528	815783.815712	40.985242
3519.408816	815571.082188	40.990247
3519.713045	815365.990527	40.995252
3519.932764	815146.390801	41.000256
3519.181597	814936.287116	41.005261
3519.412407	814708.487284	41.010266
3520.152486	814474.169592	41.015271
3519.600917	814251.151747	41.020276
3519.493857	814013.052137	41.025280
3518.918175	813784.955043	41.030285
3518.993684	813552.265699	41.035290
3519.169174	813319.746975	41.040295
3518.356700	813092.441221	41.045300
3518.674445	812871.674501	41.050304
3518.642030	812640.722294	41.055309
3518.400631	812412.620478	41.060314
3518.201421	812191.033548	41.065319
3517.954411	811956.678673	41.070324
3517.935417	811724.228747	41.075328
3518.035387	811492.433928	41.080333
3517.550257	811268.519917	41.085338
3517.881352	811039.401549	41.090343
3517.310698	810804.761947	41.095348
3516.895579	810591.145845	41.100352
3516.793903	810368.504681	41.105357
3516.588605	810151.233848	41.110362
3516.869431	809938.754245	41.115367
3516.317211	809724.935261	41.120372
3516.005803	809498.786312	41.125376
3516.229175	809298.091728	41.130381
3516.122555	809082.718800	41.135386
3516.193178	808872.040091	41.140391
3515.810235	808660.498893	41.145396
3516.035784	808446.710133	41.150400
3515.879533	808242.335781	41.155405
3515.717101	808024.107490	41.160410
3515.441037	807814.666857	41.165415
3515.190284	807622.770706	41.170420
3515.128273	807404.700466	41.175424
3515.111011	807207.244638	41.180429
3514.804606	807013.046659	41.185434
3514.775302	806808.216115	41.190439
3514.607717	806615.154781	41.195444
3514.308380	806402.452219	41.200448
3514.194968	806218.149712	41.205453
3514.096670	806018.474731	41.210458
3513.897007	805824.028647	41.215463
3513.701203	805641.966156	41.220468
3513.573839	805459.351168	41.225472
3513.335527	805279.284997	41.230477
3513.264450	805093.333497	41.235482
3513.334455	804914.477220	41.240487
3513.056174	804732.206503	41.245492
3512.647505	804559.903779	41.250496
3512.764947	804384.050100	41.255501
3512.602114	804209.455169	41.260506
3512.565239	804041.617902	41.265511
3511.843361	803880.519224	41.270516
3511.859154	803699.978444	41.275520
3512.109533	803548.380784	41.280525
3511.522113	803394.519442	41.285530
3511.805897	803234.662406	41.290535
3511.600373	803072.047496	41.295540
3511.643245	802910.756052	41.300544
3511.248157	802764.608836	41.305549
3511.033165	802613.940249	41.310554
3511.017661	802451.426296	41.315559
3510.547919	802309.526351	41.320564
3510.819513	802164.432568	41.325568
3510.902096	802027.711153	41.330573
3510.309069	801882.453312	41.335578
3510.419705	801732.445254	41.340583
3510.010077	801591.789097	41.345588
3510.027375	801459.800455	41.350592
3509.724935	801335.473890	41.355597
3509.902115	801195.693590	41.360602
3510.007117	801057.825318	41.365607
3509.944938	800926.619198	41.370612
3509.603818	800789.644791	41.375616
3509.317307	800666.669683	41.380621
3509.011559	800539.350355	41.385626
3509.038718	800418.225403	41.390631
3509.291751	800302.384320	41.395636
3508.991705	800177.644446	41.400640
3508.882588	800062.539167	41.405645
3508.781417	799936.787092	41.410650
3508.887079	799810.707286	41.415655
3508.295586	799701.725193	41.420660
3508.485267	799585.002275	41.425664
3508.462748	799478.466422	41.430669
3508.326525	799362.522832	41.435674
3508.759658	799250.882734	41.440679
3508.233933	799133.579891	41.445684
3508.222651	799021.175194	41.450688
3508.244883	798921.264079	41.455693
3507.764729	798803.703963	41.460698
3508.382799	798700.571047	41.465703
3507.688513	798590.072434	41.470708
3507.825402	798474.070207	41.475712
3507.815418	798384.411068	41.480717
3507.601040	798284.087579	41.485722
3507.559577	798176.116978	41.490727
3507.264330	798078.488963	41.495732
3507.322742	797977.873896	41.500736
3507.072294	797885.901205	41.505741
3507.098901	797786.850988	41.510746
3507.230567	797698.771919	41.515751
3506.951023	797611.683913	41.520756
3506.930487	797505.554819	41.525760
3506.548590	797421.313077	41.530765
3507.061794	797334.781220	41.535770
3507.041798	797243.300655	41.540775
3506.699468	797152.455322	41.545780
3506.398256	797072.006293	41.550784
3506.473085	796995.356287	41.555789
3506.205343	796901.271962	41.560794
3506.374628	796817.473521	41.565799
3506.363204	796742.055183	41.570804
3506.002880	796647.004692	41.575808
3506.120206	796582.359828	41.580813
3506.091067	796497.806701	41.585818
3506.419825	796420.133224	41.590823
3505.909244	796346.840024	41.595828
3505.837102	796266.149793	41.600832
3505.834245	796192.824336	41.605837
3505.878269	796125.352987	41.610842
3505.872593	796045.431262	41.615847
3505.467534	795974.315735	41.620852
3505.586693	795899.013758	41.625856
3505.738409	795830.252312	41.630861
3505.452725	795763.317292	41.635866
3505.529885	795688.996548	41.640871
3504.979038	795638.565961	41.645876
3505.341513	795562.489217	41.650880
3505.578712	795499.280540	41.655885
3505.189645	795423.270796	41.660890
3505.107629	795357.960919	41.665895
3504.748332	795310.673609	41.670900
3504.796012	795240.261013	41.675904
3505.115410	795183.925516	41.680909
3504.819082	795129.542452	41.685914
3505.087265	795063.784005	41.690919
3504.610117	795007.522642	41.695924
3504.933967	794948.399362	41.700928
3504.913710	794890.648597	41.705933
3504.880014	794830.065433	41.710938
3504.696328	794767.110896	41.715943
3504.614281	794720.215717	41.720948
3504.986177	794652.384675	41.725952
3504.615634	794600.500819	41.730957
3504.759372	794545.946363	41.735962
3504.731284	794485.505713	41.740967
3504.618655	794429.866479	41.745972
3504.155434	794377.213495	41.750976
3504.234493	794333.173399	41.755981
3503.987766	794278.335685	41.760986
3504.175684	794224.553493	41.765991
3504.249983	794181.294980	41.770996
3504.182582	794125.206277	41.776000
3504.465080	794084.993212	41.781005
3504.136832	794024.546346	41.786010
3504.248522	793972.044558	41.791015
3504.497182	793924.358937	41.796020
3504.183379	793885.703921	41.801024
3503.728359	793828.011713	41.806029
3503.847578	793789.288435	41.811034
3504.312450	793736.485195	41.816039
3503.854313	793696.385518	41.821044
3504.023019	793646.071364	41.826048
3504.150427	793604.951047	41.831053
3503.540931	793559.107398	41.836058
3503.849742	793519.570942	41.841063
3503.440911	793471.740442	41.846068
3503.805329	793419.732302	41.851072
3503.796581	793385.278538	41.856077
3503.982404	793341.801544	41.861082
3503.795155	793301.705969	41.866087
3503.694122	793271.811251	41.871092
3503.471631	793230.547782	41.876096
3503.391026	793189.506244	41.881101
3503.349036	793150.755512	41.886106
3503.695245	793107.203013	41.891111
3503.692700	793069.081003	41.896116
3503.530093	793028.637775	41.901120
3503.578141	792996.812356	41.906125
3503.799764	792955.135595	41.911130
3503.553180	792910.501433	41.916135
3503.279528	792880.680788	41.921140
3503.404413	792832.371164	41.926144
3503.449206	792793.946891	41.931149
3503.512805	792765.099418	41.936154
3503.537492	792728.437488	41.941159
3503.785206	792695.748473	41.946164
3503.163703	792648.580606	41.951168
3503.317827	792611.702275	41.956173
3503.106064	792585.683131	41.961178
3503.475784	792545.789126	41.966183
3502.987862	792514.582816	41.971188
3502.786953	792473.848871	41.976192
3503.296846	792438.478095	41.981197
3503.036157	792408.946551	41.986202
3503.458602	792376.326391	41.991207
3502.973511	792348.198298	41.996212
3502.976985	792318.136245	42.001216
3502.994842	792284.650142	42.006221
3503.031622	792261.377068	42.011226
3503.423615	792218.007030	42.016231
3502.955248	792197.501173	42.021236
3502.845626	792160.319362	42.026240
3502.960537	792125.839638	42.031245
3503.166406	792099.068925	42.036250
3503.100799	792067.354522	42.041255
3502.740509	792038.667881	42.046260
3503.098683	792010.504280	42.051264
3502.814178	791982.294375	42.056269
3502.292456	791961.893884	42.061274
3502.377060	791931.230775	42.066279
3502.423652	791920.664671	42.071284
3502.564061	791905.097743	42.076288
3502.468349	791875.049164	42.081293
3502.233223	791859.931905	42.086298
3502.723337	791837.026416	42.091303
3502.676099	791807.898752	42.096308
3502.868957	791780.933237	42.101312
3502.517862	791753.954875	42.106317
3502.259691	791734.245748	42.111322
3502.437264	791704.642517	42.116327
3502.562331	791689.175247	42.121332
3502.658669	791669.997133	42.126336
3502.697871	791648.872470	42.131341
3502.017812	791626.198056	42.136346
3502.308287	791590.123727	42.141351
3502.393881	791581.946400	42.146356
3502.575507	791552.977373	42.151360
3502.729617	791527.483466	42.156365
3502.629191	791512.979876	42.161370
3502.607257	791488.295524	42.166375
3502.263591	791468.305640	42.171380
3502.376509	791449.173178	42.176384
3502.344776	791422.241300	42.181389
3502.343885	791412.268449	42.186394
3502.521808	791387.210263	42.191399
3502.339914	791366.119251	42.196404
3502.344218	791342.261341	42.201408
3502.259660	791316.119492	42.206413
3502.163708	791299.659204	42.211418
3502.402699	791283.537623	42.216423
3502.267926	791261.705584	42.221428
3502.198184	791247.001055	42.226432
3502.211027	791211.310268	42.231437
3502.173848	791207.502780	42.236442
3502.078266	791189.428822	42.241447
3501.873614	791185.891947	42.246452
3502.185401	791163.989776	42.251456
3502.368280	791151.738895	42.256461
3502.128230	791135.985174	42.261466
3501.935300	791119.490705	42.266471
3502.113069	791096.484797	42.271476
3501.867510	791087.380827	42.276480
3501.990726	791066.876726	42.281485
3502.011689	791048.148590	42.286490
3502.459067	791042.554105	42.291495
3502.070098	791024.916679	42.296500
3502.338481	791003.314100	42.301504
3502.135218	790977.776147	42.306509
3501.671543	790970.612845	42.311514
3501.781940	790950.403729	42.316519
3501.713754	790942.200755	42.321524
3501.906098	790937.232740	42.326528
3502.044109	790913.352370	42.331533
3501.907307	790902.568842	42.336538
3502.172374	790884.975472	42.341543
3501.951168	790874.351766	42.346548
3501.864181	790862.680340	42.351552
3501.830484	790842.297851	42.356557
3501.436789	790836.736888	42.361562
3501.654322	790833.818308	42.366567
3502.131631	790834.770458	42.371572
3501.899063	790811.045431	42.376576
3501.770056	790799.527136	42.381581
3501.777232	790787.400828	42.386586
3501.507214	790775.660074	42.391591
3501.289269	790769.876012	42.396596
3501.497679	790765.980985	42.401600
3501.670342	790759.304683	42.406605
3501.788845	790746.476405	42.411610
3502.003382	790732.948594	42.416615
3501.731335	790725.266143	42.421620
3501.589449	790710.669475	42.426624
3501.940215	790704.307525	42.431629
3501.751634	790686.980113	42.436634
3501.752324	790676.468077	42.441639
3501.567351	790668.527482	42.446644
3501.818365	790671.177393	42.451648
3502.103918	790640.574634	42.456653
3501.774972	790639.208191	42.461658
3501.786613	790627.765395	42.466663
3502.012606	790614.920057	42.471668
3501.898891	790617.382538	42.476672
3502.132874	790596.419616	42.481677
3501.810108	790584.442298	42.486682
3501.931383	790570.439798	42.491687
3501.833706	790547.817287	42.496692
3501.769710	790535.603853	42.501696
3501.718379	790518.156752	42.506701
3501.732015	790512.336260	42.511706
3501.568126	790507.668080	42.516711
3501.774691	790496.976892	42.521716
3502.081305	790482.798550	42.526720
3501.803520	790470.862887	42.531725
3501.768132	790468.717102	42.536730
3501.826071	790428.467831	42.541735
3501.629748	790437.984131	42.546740
3501.865179	790426.359318	42.551744
3501.576264	790404.352946	42.556749
3501.572911	790397.557109	42.561754
3501.758159	790394.545594	42.566759
3501.832660	790379.718785	42.571764
3501.824119	790371.065718	42.576768
3501.635117	790363.320965	42.581773
3501.537041	790357.224427	42.586778
3501.612953	790348.313652	42.591783
3501.654169	790341.510791	42.596788
3501.696668	790335.636735	42.601792
3501.592390	790326.216248	42.606797
3501.633031	790317.066467	42.611802
3501.777507	790304.722224	42.616807
3501.418269	790309.765774	42.621812
3501.381569	790287.524001	42.626816
3501.536664	790272.293185	42.631821
3501.541941	790282.316051	42.636826
3501.490753	790279.439235	42.641831
3501.682462	790268.750000	42.646836
3501.120124	790244.829998	42.651840
3501.487028	790239.394106	42.656845
3501.685620	790238.531864	42.661850
3501.980205	790241.419620	42.666855
3501.616980	790234.337599	42.671860
3501.720503	790222.635254	42.676864
3501.806494	790218.905732	42.681869
3501.752989	790198.817723	42.686874
3501.588047	790183.147766	42.691879
3501.789673	790182.333939	42.696884
3502.022218	790163.374624	42.701888
3502.068630	790142.684064	42.706893
3501.763973	790144.296426	42.711898
3501.888268	790120.757604	42.716903
3501.856204	790125.945737	42.721908
3501.754428	790102.784470	42.726912
3501.812954	790088.448474	42.731917
3501.567468	790093.181023	42.736922
3501.780602	790085.079694	42.741927
3501.581350	790065.503035	42.746932
3501.426398	790066.554141	42.751936
3501.766926	790064.936228	42.756941
3501.587097	790058.069834	42.761946
3501.975439	790031.604464	42.766951
3501.849793	790030.841780	42.771956
3501.522888	790015.783515	42.776960
3501.463431	789997.113857	42.781965
3501.454259	790001.956223	42.786970
3501.777128	789990.219178	42.791975
3501.331245	789984.176664	42.796980
3501.584711	789959.199030	42.801985
3501.413280	789959.128069	42.806989
3501.660158	789963.930437	42.811994
3501.885329	789950.105970	42.816999
3502.144042	789931.239694	42.822004
3501.640173	789923.201352	42.827009
3501.897182	789912.110144	42.832013
3501.541332	789899.892254	42.837018
3501.886033	789885.559980	42.842023
3501.741129	789873.504661	42.847028
3501.682294	789864.076408	42.852033
3501.915254	789851.277394	42.857037
3501.699967	789848.915033	42.862042
3501.634791	789820.710448	42.867047
3501.560652	789827.910262	42.872052
3501.554551	789829.231531	42.877057
3501.725624	789812.627979	42.882061
3501.370289	789805.495360	42.887066
3501.764874	789798.001006	42.892071
3501.541330	789803.414923	42.897076
3501.824315	789771.830545	42.902081
3501.752325	789768.614460	42.907085
3501.401827	789766.664403	42.912090
3501.139957	789750.861868	42.917095
3501.505033	789734.227791	42.922100
3501.397260	789724.806989	42.927105
3501.559092	789732.801318	42.932109
3501.310768	789737.094465	42.937114
3501.592501	789735.974664	42.942119
3501.860228	789714.808065	42.947124
3501.608974	789710.104073	42.952129
3501.807753	789704.498426	42.957133
3501.532972	789701.411810	42.962138
3501.801013	789680.489553	42.967143
3501.728404	789674.143899	42.972148
3501.505518	789672.124964	42.977153
3501.644895	789653.374349	42.982157
3501.554692	789645.515502	42.987162
3501.613003	789643.843805	42.992167
3501.439734	789635.215522	42.997172
3501.459140	789624.845584	43.002177
3501.562483	789609.132320	43.007181
3501.544844	789612.558171	43.012186
3501.697977	789602.998608	43.017191
3501.713858	789587.445667	43.022196
3501.722874	789583.874522	43.027201
3501.606664	789578.220206	43.032205
3501.487907	789565.426718	43.037210
3501.959170	789553.127788	43.042215
3501.505457	789557.502059	43.047220
3500.909820	789546.005611	43.052225
3501.412552	789544.166613	43.057229
3501.304559	789535.185685	43.062234
3501.684483	789514.196510	43.067239
3501.571848	789526.732935	43.072244
3501.219981	789527.521499	43.077249
3501.563861	789512.210516	43.082253
3500.895399	789494.319256	43.087258
3501.333038	789475.863823	43.092263
3501.397353	789491.893583	43.097268
3501.390409	789491.405689	43.102273
3501.390990	789484.608296	43.107277
3501.413070	789486.365344	43.112282
3501.658776	789466.423935	43.117287
3501.487777	789461.120396	43.122292
3501.143207	789457.800064	43.127297
3501.488590	789456.083444	43.132301
3501.389504	789467.737627	43.137306
3501.576360	789443.159668	43.142311
3501.470706	789432.124347	43.147316
3501.708547	789425.289804	43.152321
3501.660804	789436.495896	43.157325
3501.599823	789416.504475	43.162330
3501.874820	789405.262898	43.167335
3501.486430	789403.074141	43.172340
3501.209218	789394.363986	43.177345
3501.653050	789368.767530	43.182349
3501.392026	789373.992046	43.187354
3501.734984	789371.884563	43.192359
3501.796960	789363.757078	43.197364
3501.892014	789344.523488	43.202369
3501.753022	789342.491336	43.207373
3501.414059	789339.316775	43.212378
3501.607324	789321.143627	43.217383
3501.530143	789316.950074	43.222388
3501.376230	789319.419320	43.227393
3502.008694	789308.904147	43.232397
3501.467530	789303.805056	43.237402
3501.412965	789288.458034	43.242407
3501.853695	789281.298207	43.247412
3501.527929	789280.566717	43.252417
3501.243278	789261.392242	43.257421
3501.187803	789262.721343	43.262426
3501.524750	789244.672234	43.267431
3501.406541	789248.260707	43.272436
3501.550490	789247.455786	43.277441
3501.773537	789216.905096	43.282445
3501.862169	789214.886225	43.287450
3501.552269	789216.499626	43.292455
3501.180271	789205.994600	43.297460
3501.564004	789192.241568	43.302465
3501.300236	789184.604919	43.307469
3501.316886	789191.106579	43.312474
3501.333732	789197.216971	43.317479
3501.194108	789208.682333	43.322484
3501.318250	789194.187425	43.327489
3501.781383	789174.553474	43.332493
3501.435866	789171.379856	43.337498
3501.173403	789165.503527	43.342503
3500.991106	789156.582602	43.347508
3501.078532	789158.720756	43.352513
3501.049947	789155.204161	43.357517
3501.030013	789175.453620	43.362522
3501.362658	789172.125086	43.367527
3501.192609	789152.687858	43.372532
3501.352609	789150.364386	43.377537
3501.742494	789133.920538	43.382541
3501.752451	789145.069202	43.387546
3501.632408	789119.119788	43.392551
3501.152601	789097.041073	43.397556
3501.389982	789096.368242	43.402561
3501.714327	789099.154045	43.407565
3501.605331	789099.171121	43.412570
3501.609051	789083.472179	43.417575
3501.338382	789084.394813	43.422580
3500.862513	789080.654671	43.427585
3501.558154	789079.225535	43.432589
3501.747522	789084.575491	43.437594
3501.733486	789058.951602	43.442599
3501.692144	789052.111412	43.447604
3501.558736	789043.280501	43.452609
3501.612163	789029.529861	43.457613
3501.614066	789026.204052	43.462618
3501.702115	789017.485203	43.467623
3502.041145	789020.611081	43.472628
3501.434100	789002.219826	43.477633
3501.531509	788989.635955	43.482637
3501.526340	788995.212016	43.487642
3501.430913	788982.071412	43.492647
3501.369512	788957.677170	43.497652
3501.403151	788952.047796	43.502657
3501.504419	788952.716683	43.507661
3501.465135	788953.994409	43.512666
3501.970799	788947.166412	43.517671
3501.744192	788927.248304	43.522676
3501.462652	788927.194541	43.527681
3501.612610	788916.118398	43.532685
3501.490600	788903.715382	43.537690
3501.875003	788886.000219	43.542695
3501.618141	788882.030101	43.547700
3501.613636	788878.411782	43.552705
3501.811844	788856.470802	43.557709
3501.517226	788854.609545	43.562714
3501.436284	788850.073937	43.567719
3501.670100	788848.668043	43.572724
3501.560817	788834.404461	43.577729
3501.685155	788832.624425	43.582733
3501.437871	788831.342640	43.587738
3501.200581	788818.810766	43.592743
3501.367769	788809.101137	43.597748
3501.029676	788800.693152	43.602753
3501.545526	788796.210935	43.607757
3501.356049	788799.028282	43.612762
3501.044488	788803.967705	43.617767
3501.199190	788809.616745	43.622772
3501.350702	788791.937736	43.627777
3501.299878	788776.099869	43.632781
3501.160960	788773.920807	43.637786
3501.655585	788771.691614	43.642791
3501.518267	788769.805743	43.647796
3501.153372	788768.689053	43.652801
3501.447703	788754.606740	43.657805
3501.445133	788746.244049	43.662810
3501.425222	788734.118197	43.667815
3501.410765	788730.305723	43.672820
3501.576626	788738.105003	43.677825
3501.676608	788725.618042	43.682829
3501.403033	788718.373643	43.687834
3500.804106	788710.837743	43.692839
3501.280184	788709.002689	43.697844
3501.637017	788715.842899	43.702849
3501.571876	788705.044564	43.707853
3501.566284	788700.105814	43.712858
3501.489960	788681.092713	43.717863
3501.638910	788679.895681	43.722868
3501.445933	788677.480499	43.727873
3501.576517	788660.586935	43.732877
3501.199465	788645.337737	43.737882
3501.226477	788659.076677	43.742887
3501.305178	788657.694992	43.747892
3501.391515	788652.399480	43.752897
3501.589138	788650.852479	43.757901
3501.435816	788631.166559	43.762906
3501.393048	788622.809997	43.767911
3501.567761	788619.897142	43.772916
3501.394690	788616.989744	43.777921
3501.481747	788620.742101	43.782925
3501.589302	788601.846752	43.787930
3501.530592	788585.178219	43.792935
3501.811055	788592.715214	43.797940
3501.322211	788592.204768	43.802945
3501.571700	788560.326384	43.807949
3501.320089	788560.708114	43.812954
3501.700967	788550.915794	43.817959
3501.402202	788554.728502	43.822964
3501.275782	788546.776188	43.827969
3501.594072	788519.728813	43.832973
3501.550107	788519.882450	43.837978
3501.463022	788522.390454	43.842983
3501.533642	788526.683432	43.847988
3501.146537	788512.315857	43.852993
3501.539132	788491.321457	43.857997
3501.362040	788492.963179	43.863002
3501.379032	788485.673100	43.868007
3501.888615	788495.473120	43.873012
3501.644412	788474.920578	43.878017
3501.589032	788463.826868	43.883021
3501.499002	788461.737878	43.888026
3501.465260	788454.553515	43.893031
3501.703072	788429.425817	43.898036
3501.371276	788425.026950	43.903041
3501.368949	788423.168786	43.908045
3501.616392	788425.966899	43.913050
3501.480255	788406.864540	43.918055
3501.506436	788396.051424	43.923060
3501.174361	788394.831717	43.928065
3501.601953	788395.596379	43.933069
3501.379108	788402.234075	43.938074
3501.540845	788383.329631	43.943079
3501.662091	788371.132137	43.948084
3501.291392	788364.147080	43.953089
3501.479874	788366.025145	43.958093
3501.507027	788368.124069	43.963098
3501.310730	788357.492399	43.968103
3501.380728	788346.427802	43.973108
3501.162035	788346.510936	43.978113
3501.395885	788342.414872	43.983117
3501.340563	788341.689904	43.988122
3501.029158	788343.695030	43.993127
3501.460282	788340.888701	43.998132
3501.412665	788343.977525	44.003137
3501.062585	788328.087544	44.008141
3501.048042	788327.943124	44.013146
3501.310763	788315.038665	44.018151
3501.033153	788315.864666	44.023156
3501.059669	788319.235376	44.028161
3501.274430	788317.489978	44.033165
3500.967640	788319.005285	44.038170
3500.965807	788321.402218	44.043175
3500.915463	788320.334097	44.048180
3500.873316	788321.221110	44.053185
3501.137890	788325.581720	44.058189
3501.035674	788336.504732	44.063194
3500.833275	788322.352420	44.068199
3501.025292	788313.665301	44.073204
3501.051883	788309.895078	44.078209
3501.506119	788300.188742	44.083213
3500.945924	788308.688956	44.088218
3500.996068	788303.252091	44.093223
3501.232389	788300.329466	44.098228
3501.077366	788307.641401	44.103233
3501.587515	788308.442079	44.108237
3500.958827	788314.116185	44.113242
3501.397580	788316.150783	44.118247
3501.521071	788294.219618	44.123252
3500.820414	788285.672008	44.128257
3501.509977	788279.792794	44.133261
3501.104315	788281.568119	44.138266
3501.044421	788282.995929	44.143271
3501.444004	788289.096241	44.148276
3501.318764	788290.142979	44.153281
3501.424636	788273.741396	44.158285
3501.531772	788256.557001	44.163290
3501.205200	788257.439573	44.168295
3501.259156	788258.360482	44.173300
3501.176590	788259.694019	44.178305
3501.058290	788261.717893	44.183309
3500.872541	788267.567351	44.188314
3501.352433	788258.101497	44.193319
3501.633288	788257.861987	44.198324
3501.470601	788230.692975	44.203329
3501.327717	788218.096289	44.208333
3501.296972	788220.644510	44.213338
3501.451381	788226.881030	44.218343
3501.505264	788227.948688	44.223348
3500.970470	788214.483949	44.228353
3501.493159	788191.952018	44.233357
3501.309843	788202.545550	44.238362
3501.319131	788197.555186	44.243367
3501.605049	788200.298471	44.248372
3501.272490	788205.290531	44.253377
3501.574519	788183.673468	44.258381
3501.313362	788166.448589	44.263386
3501.251569	788162.936656	44.268391
3501.303547	788166.939313	44.273396
3501.658962	788163.508896	44.278401
3501.372731	788145.749856	44.283405
3501.381574	788149.514708	44.288410
3501.233615	788143.570652	44.293415
3501.495780	788143.138414	44.298420
3501.453812	788148.036179	44.303425
3501.440194	788140.799417	44.308429
3501.477015	788127.929908	44.313434
3501.248092	788117.889893	44.318439
3501.527663	788110.607266	44.323444
3501.183086	788116.041479	44.328449
3501.510021	788107.528647	44.333453
3500.897632	788091.092156	44.338458
3501.037562	788080.847688	44.343463
3501.220077	788081.552877	44.348468
3501.017854	788078.405236	44.353473
3501.252533	788079.640304	44.358477
3501.188007	788092.954521	44.363482
3501.529283	788092.461001	44.368487
3501.381283	788090.967900	44.373492
3501.210712	788101.412865	44.378497
3501.407079	788065.676354	44.383501
3501.164584	788062.681738	44.388506
3501.040756	788056.538182	44.393511
3501.589704	788054.887212	44.398516
3501.150909	788062.635076	44.403521
3501.518023	788059.398426	44.408525
3501.645216	788053.655838	44.413530
3501.126780	788034.563251	44.418535
3501.260218	788020.700180	44.423540
3501.163282	788021.938186	44.428545
3501.280060	788023.044958	44.433549
3501.089809	788031.781168	44.438554
3501.151926	788031.233458	44.443559
3501.401031	788030.705429	44.448564
3500.986408	788007.585708	44.453569
3501.489405	787992.980031	44.458573
3501.416943	787999.447882	44.463578
3501.228768	787991.798030	44.468583
3501.620758	787996.481330	44.473588
3501.318143	788010.615536	44.478593
3501.806380	787983.588317	44.483597
3501.340198	787979.699287	44.488602
3501.431657	787980.761110	44.493607
3501.458535	787972.050447	44.498612
3501.228925	787970.374424	44.503617
3501.310770	787946.100793	44.508621
3501.575364	787945.179032	44.513626
3501.105496	787946.915567	44.518631
3501.237901	787942.981855	44.523636
3501.327213	787953.582079	44.528641
3501.344649	787944.530464	44.533645
3501.119897	787935.761262	44.538650
3500.842211	787924.505744	44.543655
3501.112106	787920.844006	44.548660
3501.104393	787931.508346	44.553665
3501.045672	787924.474051	44.558669
3501.155406	787939.668955	44.563674
3501.588118	787927.568693	44.568679
3501.362331	787935.723626	44.573684
3501.063008	787939.781337	44.578689
3501.618252	787922.917332	44.583693
3501.658090	787908.383872	44.588698
3501.285489	787897.338799	44.593703
3501.691566	787900.063427	44.598708
3501.441073	787893.841694	44.603713
3501.507941	787875.928902	44.608717
3501.366708	787869.641152	44.613722
3501.124062	787861.706182	44.618727
3501.217396	787867.756933	44.623732
3500.970327	787867.795593	44.628737
3501.531355	787862.082849	44.633741
3501.140170	787874.225726	44.638746
3501.150749	787855.294491	44.643751
3501.317674	787838.246405	44.648756
3501.372814	787834.177964	44.653761
3501.224923	787829.847776	44.658765
3501.050639	787839.853507	44.663770
3501.210980	787830.730483	44.668775
3501.325077	787834.576889	44.673780
3501.161719	787837.586214	44.678785
3501.173663	787823.790637	44.683789
3501.276274	787809.540631	44.688794
3500.993921	787812.862055	44.693799
3501.257355	787797.657514	44.698804
3500.925843	787814.535852	44.703809
3500.834845	787805.647739	44.708813
3500.978159	787818.343049	44.713818
3501.078511	787817.349117	44.718823
3501.085692	787811.331596	44.723828
3501.137898	787819.247558	44.728833
3500.981411	787815.505673	44.733837
3500.978380	787820.299765	44.738842
3500.555271	787827.262825	44.743847
3500.769402	787825.028257	44.748852
3500.950582	787831.896848	44.753857
3501.099643	787826.982183	44.758861
3500.588752	787841.736276	44.763866
3500.936946	787834.393705	44.768871
3501.198085	787829.021296	44.773876
3501.103033	787832.606914	44.778881
3501.357102	787835.257503	44.783885
3501.130973	787844.097397	44.788890
3501.044849	787829.828024	44.793895
3501.154924	787819.000851	44.798900
3501.167661	787807.112764	44.803905
3501.173425	787796.937746	44.808909
3501.065680	787806.688554	44.813914
3500.469215	787809.961253	44.818919
3500.649883	787804.748146	44.823924
3500.646364	787816.634871	44.828929
3501.425940	787829.083955	44.833933
3501.302999	787825.532487	44.838938
3501.291300	787817.952674	44.843943
3501.252142	787818.105575	44.848948
3500.889449	787825.695075	44.853953
3500.969592	787821.427062	44.858957
3501.170680	787827.803404	44.863962
3501.243871	787826.080009	44.868967
3501.362367	787815.887397	44.873972
3501.096069	787816.809517	44.878977
3501.148228	787798.605331	44.883981
3501.298795	787793.299092	44.888986
3501.090169	787788.978371	44.893991
3501.123121	787791.712458	44.898996
3501.407890	787789.760322	44.904001
3501.531669	787788.224667	44.909005
3501.509297	787791.505459	44.914010
3501.098019	787782.667383	44.919015
3501.367640	787768.195523	44.924020
3501.111856	787768.186631	44.929025
3501.318399	787769.768558	44.934029
3501.262267	787771.538290	44.939034
3501.016212	787773.044225	44.944039
3501.294937	787770.946285	44.949044
3501.364595	787772.794182	44.954049
3501.512548	787746.503993	44.959053
3501.076431	787739.283924	44.964058
3500.964396	787747.127818	44.969063
3501.448962	787740.546459	44.974068
3500.998745	787751.916154	44.979073
3501.171041	787745.970591	44.984077
3501.094998	787749.113050	44.989082
3501.194445	787749.929090	44.994087
3501.360974	787747.653024	44.999092
3501.214830	787737.208172	45.004097
3501.339373	787713.171586	45.009101
3501.152607	787724.549058	45.014106
3501.066509	787716.344866	45.019111
3501.462393	787705.374999	45.024116
3501.310716	787719.975378	45.029121
3501.324265	787711.706689	45.034125
3500.848130	787708.503860	45.039130
3500.864770	787685.315593	45.044135
3501.391443	787681.026602	45.049140
3501.172959	787690.305741	45.054145
3501.291486	787684.417444	45.059149
3501.155150	787692.803267	45.064154
3501.328483	787695.270874	45.069159
3501.445627	787695.643919	45.074164
3500.886838	787704.829490	45.079169
3501.371636	787701.280782	45.084173
3501.450969	787680.283870	45.089178
3501.304441	787661.865792	45.094183
3501.580707	787662.067219	45.099188
3501.031517	787674.773228	45.104193
3501.414240	787664.783655	45.109197
3501.721450	787659.893059	45.114202
3501.428022	787639.052118	45.119207
3501.278629	787640.347310	45.124212
3501.045367	787641.606697	45.129217
3501.387865	787638.667185	45.134221
3501.211079	787649.309495	45.139226
3501.236421	787635.804924	45.144231
3501.572205	787617.458072	45.149236
3501.053140	787617.099011	45.154241
3501.206537	787614.873868	45.159245
3501.598996	787610.752560	45.164250
3500.952629	787612.467855	45.169255
3501.581205	787608.847707	45.174260
3501.396863	787595.278000	45.179265
3501.121134	787573.993846	45.184269
3501.088671	787581.727665	45.189274
3501.037379	787580.806319	45.194279
3501.443336	787582.895193	45.199284
3501.053821	787589.951080	45.204289
3501.353544	787587.800885	45.209293
3501.450509	787583.970332	45.214298
3501.577775	787558.856612	45.219303
3501.587208	787554.452734	45.224308
3501.599656	787548.385234	45.229313
3501.446737	787538.381372	45.234317
3501.489416	787517.291841	45.239322
3501.641946	787513.305812	45.244327
3501.550815	787507.303383	45.249332
3501.404554	787514.565905	45.254337
3501.368423	787497.304103	45.259341
3501.718586	787489.520597	45.264346
3501.577246	787486.069655	45.269351
3501.460453	787474.592553	45.274356
3501.348021	787471.870835	45.279361
3501.394051	787463.303258	45.284365
3501.312101	787449.423745	45.289370
3501.226630	787448.703392	45.294375
3501.215606	787442.394880	45.299380
3501.580136	787454.811722	45.304385
3501.506527	787443.474565	45.309389
3501.471094	787421.320768	45.314394
3501.445559	787407.334515	45.319399
3501.489110	787412.464040	45.324404
3501.609559	787418.462048	45.329409
3501.899244	787400.562057	45.334413
3501.567858	787377.867373	45.339418
3501.441862	787392.660127	45.344423
3501.678078	787385.579153	45.349428
3501.564586	787361.382832	45.354433
3501.830507	787349.943522	45.359437
3501.745753	787352.158097	45.364442
3501.407126	787337.829300	45.369447
3501.650061	787319.055880	45.374452
3501.570599	787315.057080	45.379457
3501.386416	787304.666409	45.384461
3501.396957	787308.529310	45.389466
3501.809677	787300.589051	45.394471
3501.924070	787277.628666	45.399476
3501.196149	787289.531741	45.404481
3501.264655	787275.334836	45.409485
3501.301763	787257.522861	45.414490
3501.314690	787247.003450	45.419495
3501.893197	787247.402237	45.424500
3501.102177	787255.303934	45.429505
3501.117353	787253.393788	45.434509
3501.037021	787254.629339	45.439514
3500.889544	787256.462406	45.444519
3501.459738	787259.504076	45.449524
3501.322736	787238.637419	45.454529
3501.506259	787223.346218	45.459533
3501.286242	787226.951698	45.464538
3501.221483	787231.119926	45.469543
3501.470409	787226.580554	45.474548
3501.172152	787211.902744	45.479553
3501.761303	787190.139723	45.484557
3501.387482	787193.769263	45.489562
3501.390989	787183.740411	45.494567
3501.736105	787181.680829	45.499572
3501.498461	787167.238038	45.504577
3501.344315	787154.445409	45.509581
3501.290107	787147.996610	45.514586
3501.636274	787156.943631	45.519591
3501.363203	787145.196873	45.524596
3501.119365	787131.782273	45.529601
3501.437330	787120.236593	45.534605
3501.613741	787117.420656	45.539610
3501.683870	787116.578103	45.544615
3501.574626	787111.850047	45.549620
3501.455186	787094.306702	45.554625
3501.493715	787085.886568	45.559629
3501.450460	787084.621460	45.564634
3501.432680	787086.581057	45.569639
3501.921563	787068.746872	45.574644
3501.279391	787058.574166	45.579649
3501.454511	787050.475073	45.584653
3501.589746	787055.737302	45.589658
3501.392116	787045.152646	45.594663
3501.826409	787032.512394	45.599668
3501.639669	787030.731587	45.604673
3501.672468	787016.295110	45.609677
3501.397541	787007.385757	45.614682
3501.196912	786994.061963	45.619687
3501.511218	786993.327985	45.624692
3501.182407	786996.070032	45.629697
3501.220709	786995.966242	45.634701
3501.372718	786994.768433	45.639706
3501.271341	786983.043467	45.644711
3501.308757	786967.236394	45.649716
3501.410228	786971.868003	45.654721
3501.021509	786967.721655	45.659725
3501.596739	786961.565643	45.664730
3501.242110	786967.882927	45.669735
3501.580831	786955.893434	45.674740
3501.297169	786946.104795	45.679745
3501.272040	786933.927538	45.684749
3501.198905	786932.128945	45.689754
3500.939617	786940.877382	45.694759
3501.011941	786931.277676	45.699764
3501.343197	786928.975580	45.704769
3501.005265	786929.860096	45.709773
3501.152937	786939.083045	45.714778
3501.130194	786937.863623	45.719783
3501.615432	786914.208040	45.724788
3501.209245	786907.422664	45.729793
3501.250148	786900.371706	45.734797
3501.120098	786896.184877	45.739802
3500.928242	786899.394764	45.744807
3501.021566	786888.862217	45.749812
3500.977942	786901.441746	45.754817
3501.217344	786886.238876	45.759821
3501.235844	786827.873047	45.764826
3500.921523	786723.865583	45.769831
3500.885309	786571.330205	45.774836
3500.390379	786375.907250	45.779841
3500.083801	786117.480807	45.784845
3500.455779	785825.764596	45.789850
3499.781690	785483.604330	45.794855
3499.371617	785087.019476	45.799860
3498.723943	784652.717487	45.804865
3498.318293	784166.031626	45.809869
3498.005604	783638.475818	45.814874
3497.357544	783064.282445	45.819879
3496.390809	782429.289311	45.824884
3495.511404	781758.580480	45.829889
3495.212334	781045.654001	45.834893
3494.799182	780279.538045	45.839898
3493.624850	779477.848876	45.844903
3492.871536	778618.788310	45.849908
3491.907617	777722.224566	45.854913
3491.262271	776773.949715	45.859917
3490.418373	775784.166591	45.864922
3489.231125	774757.633881	45.869927
3488.259790	773677.631050	45.874932
3486.810506	772548.751900	45.879937
3486.024183	771370.500082	45.884941
3484.820481	770161.165282	45.889946
3483.657380	768901.235736	45.894951
3482.395543	767601.156021	45.899956
3480.736241	766263.404373	45.904961
3479.114186	764888.775191	45.909965
3477.927071	763467.318224	45.914970
3476.071877	762011.256838	45.919975
3475.292822	760516.368849	45.924980
3473.186093	758972.003243	45.929985
3471.612187	757388.597640	45.934989
3470.336155	755776.483996	45.939994
3468.519207	754130.613984	45.944999
3466.911834	752429.952459	45.950004
3465.033046	750703.454054	45.955009
3463.376920	748929.183908	45.960013
3461.362400	747126.585299	45.965018
3459.330152	745293.124855	45.970023
3457.346113	743409.621149	45.975028
3455.565002	741509.940365	45.980033
3453.878093	739585.272719	45.985037
3451.620480	737593.975695	45.990042
3449.625391	735597.468274	45.995047
3447.626064	733554.482353	46.000052
3445.349595	731477.992969	46.005057
3443.194452	729382.561222	46.010061
3441.005537	727235.094471	46.015066
3438.702719	725074.451490	46.020071
3436.651564	722867.394689	46.025076
3434.200473	720655.861774	46.030081
3431.503546	718391.966931	46.035085
3429.159821	716111.789478	46.040090
3426.701858	713810.400325	46.045095
3424.267165	711464.330115	46.050100
3421.617397	709116.207135	46.055105
3419.000438	706723.552917	46.060109
3416.688878	704314.097260	46.065114
3414.052777	701875.256769	46.070119
3411.513542	699409.616812	46.075124
3408.382489	696926.080872	46.080129
3405.807743	694419.949373	46.085133
3403.164969	691875.346605	46.090138
3400.550909	689328.464348	46.095143
3397.498421	686740.799228	46.100148
3394.673849	684148.920819	46.105153
3391.743303	681530.752798	46.110157
3389.108287	678891.871637	46.115162
3386.293076	676231.940795	46.120167
3382.754450	673548.597584	46.125172
3380.196439	670850.452287	46.130177
3377.296433	668137.057848	46.135181
3374.243526	665396.097562	46.140186
3371.154364	662634.395894	46.145191
3367.940102	659847.178223	46.150196
3365.168067	657057.476148	46.155201
3361.950973	654247.464136	46.160205
3359.359716	651424.779313	46.165210
3355.770712	648574.977915	46.170215
3352.759619	645718.420787	46.175220
3350.101249	642834.013290	46.180225
3346.863183	639930.656272	46.185229
3343.538872	637012.301307	46.190234
3340.233756	634091.545569	46.195239
3337.006910	631145.382012	46.200244
3334.174614	628192.412769	46.205249
3330.681889	625215.379074	46.210253
3327.564555	622220.097719	46.215258
3324.041915	619217.772781	46.220263
3320.985441	616193.676957	46.225268
3317.957731	613170.711929	46.230273
3314.059276	610122.925184	46.235277
3310.486720	607072.923990	46.240282
3307.115050	604007.124874	46.245287
3303.994686	600942.480660	46.250292
3300.846195	597854.863709	46.255297
3297.323856	594755.032887	46.260301
3294.272051	591646.360353	46.265306
3290.297095	588523.703402	46.270311
3287.315180	585381.245406	46.275316
3283.734986	582249.659430	46.280321
3280.181787	579093.108566	46.285325
3276.826235	575937.639113	46.290330
3273.331676	572777.693476	46.295335
3269.744418	569581.748700	46.300340
3265.824433	566397.115522	46.305345
3262.359598	563193.255775	46.310349
3259.126467	559996.469946	46.315354
3255.234755	556790.933463	46.320359
3252.288106	553574.738926	46.325364
3248.277261	550354.083261	46.330369
3244.298378	547129.102305	46.335373
3240.946870	543897.998542	46.340378
3237.407925	540657.281325	46.345383
3234.154249	537408.036055	46.350388
3230.170519	534170.207526	46.355393
3226.494561	530905.031601	46.360397
3222.918539	527639.978090	46.365402
3219.272559	524376.392870	46.370407
3215.426708	521101.104820	46.375412
3211.953200	517827.129629	46.380417
3208.373873	514565.290479	46.385421
3204.488818	511275.851285	46.390426
3200.538891	507988.219405	46.395431
3196.920300	504696.642966	46.400436
3193.361228	501418.832284	46.405441
3189.857235	498115.691524	46.410445
3185.920576	494822.627234	46.415450
3181.682315	491526.102746	46.420455
3178.404694	488213.958209	46.425460
3175.097162	484913.020273	46.430465
3170.812745	481599.756806	46.435469
3167.391178	478287.577305	46.440474
3163.436049	474975.497276	46.445479
3160.088074	471656.118105	46.450484
3155.891557	468346.056627	46.455489
3151.750254	465028.748646	46.460493
3148.771662	461716.774397	46.465498
3144.728759	458410.697186	46.470503
3141.260665	455090.384668	46.475508
3137.044613	451769.357358	46.480513
3133.319609	448439.431556	46.485517
3129.665053	445114.450575	46.490522
3125.880273	441799.978278	46.495527
3122.340693	438473.936609	46.500532
3118.037735	435159.031468	46.505537
3114.336991	431829.830149	46.510541
3110.820963	428507.128132	46.515546
3106.700799	425194.457570	46.520551
3102.958937	421856.749219	46.525556
3099.477380	418546.041710	46.530561
3095.785194	415216.688194	46.535565
3091.867357	411894.406838	46.540570
3087.714102	408567.392110	46.545575
3084.022909	405257.764341	46.550580
3080.308773	401940.244827	46.555585
3076.663069	398623.807873	46.560589
3072.866122	395314.689931	46.565594
3068.986070	391997.764773	46.570599
3065.306765	388683.072085	46.575604
3061.441632	385371.697967	46.580609
3057.497328	382058.608512	46.585613
3053.262356	378733.763253	46.590618
3049.436410	375443.308433	46.595623
3046.020132	372144.946432	46.600628
3042.049122	368856.744504	46.605633
3038.047231	365556.528581	46.610637
3034.405216	362261.699374	46.615642
3030.200840	358973.225086	46.620647
3026.784507	355689.278861	46.625652
3023.047772	352407.807507	46.630657
3019.010078	349119.589660	46.635661
3015.270196	345839.716396	46.640666
3011.075514	342567.248757	46.645671
3007.137333	339295.144352	46.650676
3003.283798	336033.458576	46.655681
2999.151404	332777.529161	46.660685
2995.723112	329517.750577	46.665690
2991.885553	326270.202807	46.670695
2987.774975	323012.413174	46.675700
2983.515422	319765.459112	46.680705
2979.378461	316520.098710	46.685709
2975.669004	313287.437930	46.690714
2971.646663	310064.219213	46.695719
2968.028119	306845.327353	46.700724
2963.806098	303637.978565	46.705729
2959.926606	300441.653426	46.710733
2956.109112	297233.930955	46.715738
2951.965927	294057.870202	46.720743
2947.990260	290877.947463	46.725748
2944.448519	287693.339211	46.730753
2940.354397	284523.605988	46.735757
2936.279665	281350.210360	46.740762
2932.232530	278201.139262	46.745767
2928.448722	275043.725171	46.750772
2924.864463	271899.271236	46.755777
2920.400978	268766.223738	46.760781
2916.637976	265629.804421	46.765786
2912.639111	262512.677766	46.770791
2908.387396	259396.622332	46.775796
2904.333894	256300.547270	46.780801
2900.004419	253207.421927	46.785805
2896.439051	250114.926380	46.790810
2892.215551	247044.581218	46.795815
2887.914005	243967.856260	46.800820
2884.200381	240921.965229	46.805825
2879.984070	237873.799388	46.810829
2875.902963	234840.126153	46.815834
2871.995362	231813.076826	46.820839
2868.115651	228806.230601	46.825844
2864.181396	225784.281660	46.830849
2860.208860	222791.295580	46.835853
2856.167855	219808.462013	46.840858
2852.230481	216830.106362	46.845863
2848.099927	213856.357845	46.850868
2844.488172	210898.215680	46.855873
2839.928664	207952.782540	46.860877
2835.770163	204998.358488	46.865882
2831.573251	202074.926332	46.870887
2827.501489	199159.901442	46.875892
2823.524460	196268.854202	46.880897
2819.136092	193375.943969	46.885901
2815.309162	190494.979650	46.890906
2810.958834	187636.194466	46.895911
2806.912880	184782.300274	46.900916
2802.986827	181937.685432	46.905921
2798.665685	179114.479055	46.910925
2794.930788	176302.168318	46.915930
2790.309177	173504.590665	46.920935
2786.379691	170707.932935	46.925940
2782.218039	167943.544783	46.930945
2778.370226	165174.555724	46.935949
2774.134072	162340.519623	46.940954
2769.778667	159613.068508	46.945959
2765.920848	156884.882535	46.950964
2761.924814	154181.150521	46.955969
2757.908441	151481.824657	46.960973
2753.790309	148796.682303	46.965978
2749.484074	146117.532133	46.970983
2745.492271	143451.615746	46.975988
2741.582272	140815.410804	46.980993
2737.232799	138179.214601	46.985997
2733.314415	135561.164334	46.991002
2729.246647	132964.735991	46.996007
2725.167175	130371.107645	47.001012
2721.245050	127786.514789	47.006017
2716.757291	125223.067108	47.011021
2712.944817	122674.453319	47.016026
2708.761206	120130.168491	47.021031
2704.617343	117592.733054	47.026036
2700.518259	115093.810893	47.031041
2696.216701	112587.129538	47.036045
2692.864989	110095.424712	47.041050
2688.321290	107626.685332	47.046055
2684.580908	105162.508910	47.051060
2680.441898	102715.161761	47.056065
2676.176335	100282.122815	47.061069
2672.655150	97856.634726	47.066074
2668.408265	95458.029854	47.071079
2664.251945	93048.068564	47.076084
2660.211882	90661.403132	47.081089
2656.176592	88291.518377	47.086093
2652.362529	85929.664621	47.091098
2647.783970	83589.907500	47.096103
2643.720452	81248.558283	47.101108
2640.154786	78935.572657	47.106113
2636.156065	76632.842180	47.111117
2632.036882	74338.362807	47.116122
2627.514137	72056.078042	47.121127
2623.466647	69789.938698	47.126132
2619.348873	67536.867591	47.131137
2615.420031	65297.229877	47.136141
2611.362451	63075.466509	47.141146
2606.866032	60872.233271	47.146151
2603.366382	58677.759533	47.151156
2599.083027	56492.063920	47.156161
2594.914298	54332.834260	47.161165
2590.990077	52186.177768	47.166170
2586.345955	50054.642143	47.171175
2582.153729	47937.091006	47.176180
2578.288969	45834.709304	47.181185
2573.205093	43750.349826	47.186189
2569.143032	41678.187090	47.191194
2564.879423	39636.671627	47.196199
2560.640236	37609.981902	47.201204
2556.181474	35612.670872	47.206209
2551.869536	33639.921083	47.211213
2547.617713	31668.810147	47.216218
2543.096900	29719.962390	47.221223
2538.898496	27802.355329	47.226228
2534.370400	25903.354459	47.231233
2529.549037	24033.543915	47.236237
2525.183524	22175.600294	47.241242
2520.619868	20363.317490	47.246247
2515.267282	18568.470536	47.251252
2510.338265	16818.771309	47.256257
2504.874533	15098.406559	47.261261
2498.404568	13436.920168	47.266266
2489.026635	11910.870772	47.271271
2478.184777	10499.335586	47.276276
2467.829583	9176.749848	47.281281
2457.851239	7955.941055	47.286285
2448.527353	6849.373353	47.291290
2439.396654	5843.508908	47.296295
2431.856166	4928.343552	47.301300
2424.432138	4122.015234	47.306305
2417.238898	3395.489862	47.311309
2411.110096	2740.251638	47.316314
2405.211520	2177.879872	47.321319
2399.926989	1667.207130	47.326324
2395.107179	1221.215472	47.331329
2390.413957	823.468721	47.336333
2385.646103	479.731331	47.341338
2380.612593	184.967920	47.346343
2366.622016	190.858398	47.351348
2355.329341	214.895511	47.356353
2349.906601	231.006380	47.361357
2348.183915	217.386568	47.366362
2348.115703	226.290893	47.371367
2348.119626	222.829051	47.376372
2348.080093	225.575178	47.381377
2346.620251	226.926772	47.386381
2344.682074	214.356276	47.391386
2341.717137	218.252955	47.396391
2338.513284	218.459983	47.401396
2335.881132	216.875415	47.406401
2332.917862	216.377232	47.411405
2329.618523	219.522609	47.416410
2326.486651	216.260280	47.421415
2323.322501	213.003002	47.426420
2320.390153	221.289189	47.431425
2316.884384	230.740804	47.436429
2313.705778	210.692017	47.441434
2310.874820	212.112586	47.446439
2307.817193	214.043197	47.451444
2304.778691	211.648985	47.456449
2300.637896	227.995921	47.461453
2297.671212	217.076525	47.466458
2294.474529	225.508481	47.471463
2291.491526	226.142895	47.476468
2288.063629	219.165060	47.481473
2284.588461	219.218392	47.486477
2281.236571	217.034573	47.491482
2278.195668	208.480712	47.496487
2274.478121	211.283394	47.501492
2271.504316	210.559079	47.506497
2267.616699	218.020260	47.511501
2264.638400	214.328949	47.516506
2261.269058	211.239841	47.521511
2257.924927	209.447134	47.526516
2254.827865	205.878817	47.531521
2250.918959	210.116198	47.536525
2247.353022	209.456056	47.541530
2244.359239	211.708899	47.546535
2240.945435	205.804594	47.551540
2237.572250	203.772824	47.556545
2233.689103	214.798980	47.561549
2230.534001	212.223709	47.566554
2227.770308	210.099747	47.571559
2223.972025	201.360675	47.576564
2220.168867	200.769296	47.581569
2216.458847	204.402911	47.586573
2213.687484	206.709551	47.591578
2210.445737	208.466506	47.596583
2206.216809	204.382409	47.601588
2202.619166	198.810614	47.606593
2199.371910	213.657303	47.611597
2196.222974	200.194254	47.616602
2192.467003	205.505582	47.621607
2189.693051	210.141229	47.626612
2186.379600	207.752105	47.631617
2182.851081	209.408399	47.636621
2179.161796	199.310819	47.641626
2175.819635	204.377067	47.646631
2171.985797	203.992991	47.651636
2168.271724	202.226558	47.656641
2164.692780	207.355167	47.661645
2162.031560	192.733791	47.666650
2158.760255	207.486165	47.671655
2155.267821	214.183171	47.676660
2151.305300	202.698289	47.681665
2147.657567	208.555861	47.686669
2144.867920	198.924996	47.691674
2141.317133	202.707732	47.696679
2137.864604	193.449516	47.701684
2134.027758	192.641970	47.706689
2130.306933	205.265805	47.711693
2126.954132	201.497090	47.716698
2123.734085	206.692946	47.721703
2120.175061	204.247352	47.726708
2116.768361	194.602312	47.731713
2112.939028	202.063904	47.736717
2109.825721	198.776595	47.741722
2106.355124	199.803735	47.746727
2102.410497	199.857811	47.751732
2099.256820	203.939104	47.756737
2095.578150	201.939360	47.761741
2092.431733	190.402752	47.766746
2089.069244	193.333438	47.771751
2085.376097	202.437915	47.776756
2082.596780	195.447272	47.781761
2078.263770	198.314677	47.786765
2075.037939	190.549156	47.791770
2071.693675	191.812812	47.796775
2068.052005	199.096351	47.801780
2064.815693	192.237335	47.806785
2061.115656	202.962786	47.811789
2057.540689	192.894832	47.816794
2054.025069	192.945076	47.821799
2050.241691	187.010088	47.826804
2047.274950	184.025744	47.831809
2043.408977	187.541440	47.836813
2040.335167	189.613860	47.841818
2036.971457	194.898656	47.846823
2033.411080	185.926289	47.851828
2029.793047	187.973134	47.856833
2025.978970	192.743091	47.861837
2022.887848	192.685792	47.866842
2019.079800	187.377954	47.871847
2015.258719	187.045725	47.876852
2012.415702	182.358866	47.881857
2008.388142	187.573532	47.886861
2005.451927	190.988050	47.891866
2001.998713	189.677583	47.896871
1998.380995	189.563482	47.901876
1995.036475	180.320069	47.906881
1991.116734	186.710638	47.911885
1987.877243	188.122444	47.916890
1984.253685	188.474347	47.921895
1980.881886	188.755218	47.926900
1977.391085	178.088825	47.931905
1973.841175	180.504689	47.936909
1970.767403	170.655760	47.941914
1966.963762	176.597884	47.946919
1963.247651	181.729025	47.951924
1960.011687	182.567631	47.956929
1956.352124	188.319532	47.961933
1952.797708	185.724579	47.966938
1949.303903	175.064997	47.971943
1945.754696	181.777259	47.976948
1942.511269	179.022911	47.981953
1939.027065	181.979013	47.986957
1935.897844	177.507813	47.991962
1932.729665	186.087236	47.996967
1928.834409	180.887998	48.001972
1925.346349	176.852616	48.006977
1921.127676	188.700156	48.011981
1917.867700	180.392697	48.016986
1914.293516	180.955203	48.021991
1911.086399	177.125805	48.026996
1907.869827	179.745799	48.032001
1904.163992	183.287102	48.037005
1900.672785	174.667814	48.042010
1897.150680	181.632119	48.047015
1893.213201	180.359504	48.052020
1890.208727	179.738177	48.057025
1886.391812	176.589524	48.062029
1882.986692	174.328749	48.067034
1879.385958	183.279600	48.072039
1876.090677	180.631468	48.077044
1872.751422	178.585021	48.082049
1869.171265	180.499436	48.087053
1865.886270	174.049926	48.092058
1862.182778	176.110198	48.097063
1857.987824	178.538453	48.102068
1854.733483	180.392395	48.107073
1851.388235	184.513219	48.112077
1848.334584	167.425485	48.117082
1845.002137	173.420462	48.122087
1841.243223	169.750210	48.127092
1837.593305	172.010919	48.132097
1833.856214	182.960520	48.137101
1830.300101	176.199100	48.142106
1827.059473	181.781071	48.147111
1823.813880	180.080661	48.152116
1820.914010	162.671477	48.157121
1817.193845	175.852099	48.162125
1813.255978	174.016414	48.167130
1809.595408	176.044675	48.172135
1805.783184	175.091025	48.177140
1802.230693	177.181471	48.182145
1799.168951	173.810265	48.187149
1796.085720	165.902318	48.192154
1792.248402	167.157795	48.197159
1788.773553	172.811230	48.202164
1785.104247	169.794546	48.207169
1781.578001	176.784840	48.212173
1778.111735	167.354923	48.217178
1774.597394	171.106750	48.222183
1771.042898	174.368139	48.227188
1767.710253	164.164324	48.232193
1764.148420	173.245159	48.237197
1760.515355	162.648589	48.242202
1757.117086	170.662925	48.247207
1753.604877	167.390708	48.252212
1750.383708	164.974638	48.257217
1746.785124	175.889927	48.262221
1743.459846	169.462587	48.267226
1740.039447	167.773744	48.272231
1736.059691	166.510972	48.277236
1732.829426	162.492268	48.282241
1728.613383	168.995727	48.287245
1725.482273	156.820962	48.292250
1722.378903	167.130390	48.297255
1718.711577	168.966744	48.302260
1715.845436	163.584395	48.307265
1711.940804	169.593023	48.312269
1708.166651	163.096742	48.317274
1704.618893	168.109861	48.322279
1700.648672	171.616673	48.327284
1697.820344	162.476105	48.332289
1694.102322	170.967617	48.337293
1690.921385	164.751833	48.342298
1687.425535	163.856284	48.347303
1683.509196	165.358290	48.352308
1679.972393	165.301241	48.357313
1676.383098	165.242917	48.362317
1673.182389	165.373720	48.367322
1669.753435	162.762401	48.372327
1666.066142	163.560998	48.377332
1662.979681	161.706020	48.382337
1659.478187	171.736079	48.387341
1655.963698	162.462464	48.392346
1652.013296	158.885535	48.397351
1648.414428	165.959997	48.402356
1645.109039	165.265613	48.407361
1641.608981	165.671073	48.412365
1638.206658	154.513254	48.417370
1634.679866	158.453735	48.422375
1631.054180	171.761985	48.427380
1627.995777	161.097682	48.432385
1623.947426	165.942394	48.437389
1620.574408	163.774766	48.442394
1617.078417	167.678796	48.447399
1613.629356	163.887371	48.452404
1610.361651	160.703494	48.457409
1606.623124	166.186272	48.462413
1603.455254	164.176372	48.467418
1600.092788	159.725978	48.472423
1596.416509	163.873371	48.477428
1592.618698	160.880040	48.482433
1588.611969	158.650254	48.487437
1585.605981	160.702691	48.492442
1581.988424	159.889504	48.497447
1578.810664	153.331575	48.502452
1575.083433	165.023191	48.507457
1571.563916	169.952835	48.512461
1567.976686	164.740346	48.517466
1564.562837	160.453035	48.522471
1561.227984	153.910208	48.527476
1558.077584	156.814178	48.532481
1554.197651	153.906485	48.537485
1550.619669	153.707227	48.542490
1547.048279	167.247446	48.547495
1543.548739	164.292871	48.552500
1540.218959	160.381562	48.557505
1536.707757	160.231969	48.562509
1533.042350	156.110598	48.567514
1529.888832	159.622520	48.572519
1525.850350	155.458304	48.577524
1522.725397	156.083509	48.582529
1519.065464	171.330245	48.587533
1515.578571	160.014865	48.592538
1512.411938	156.574752	48.597543
1508.671311	155.515094	48.602548
1505.442778	157.671991	48.607553
1502.035067	161.748903	48.612557
1498.316719	164.042583	48.617562
1494.669118	159.807706	48.622567
1490.997033	161.885334	48.627572
1487.533210	161.984612	48.632577
1484.018170	154.875219	48.637581
1480.440480	156.944403	48.642586
1476.889477	155.022990	48.647591
1473.290338	156.162206	48.652596
1470.043751	151.886717	48.657601
1466.462274	163.308769	48.662605
1463.304291	155.305081	48.667610
1459.997963	158.053149	48.672615
1456.363381	158.508204	48.677620
1452.794181	154.922312	48.682625
1448.968234	162.908755	48.687629
1445.565019	157.689660	48.692634
1442.179563	160.269781	48.697639
1438.544441	155.520434	48.702644
1435.365973	147.001100	48.707649
1431.429197	156.096413	48.712653
1428.019449	153.289184	48.717658
1424.671342	156.050129	48.722663
1421.077340	159.099509	48.727668
1417.602078	155.907060	48.732673
1414.067934	166.919912	48.737677
1410.750869	161.181132	48.742682
1407.483666	157.339173	48.747687
1403.766495	161.107044	48.752692
1399.952470	157.860059	48.757697
1396.590768	167.555083	48.762701
1393.238782	166.997794	48.767706
1389.929717	153.272278	48.772711
1386.216222	153.777677	48.777716
1382.498379	162.677382	48.782721
1378.506293	162.176004	48.787725
1375.044916	151.220539	48.792730
1372.061980	165.187550	48.797735
1368.877066	160.813856	48.802740
1365.358222	157.144183	48.807745
1361.540685	162.342009	48.812749
1358.284276	152.290957	48.817754
1354.309338	156.434560	48.822759
1350.632623	152.460569	48.827764
1347.124895	153.958850	48.832769
1343.831706	159.625105	48.837773
1340.749567	155.260644	48.842778
1337.389162	151.335223	48.847783
1333.657892	154.738321	48.852788
1330.245891	146.717504	48.857793
1326.662948	158.573262	48.862797
1322.884498	165.185539	48.867802
1319.380513	165.322800	48.872807
1316.011702	164.227157	48.877812
1313.067324	156.756413	48.882817
1309.488059	165.308575	48.887821
1305.697636	158.071517	48.892826
1301.869935	162.926098	48.897831
1298.303606	159.811226	48.902836
1294.961858	144.999358	48.907841
1291.423827	155.468667	48.912845
1287.596707	162.715010	48.917850
1284.692193	152.311503	48.922855
1281.101110	148.792382	48.927860
1277.717794	155.083381	48.932865
1273.968934	161.295562	48.937869
1270.557085	155.818455	48.942874
1267.131609	151.378053	48.947879
1263.405804	156.760870	48.952884
1260.093784	147.949294	48.957889
1256.455255	159.465753	48.962893
1252.912353	150.785237	48.967898
1249.662184	151.123239	48.972903
1245.800557	152.544077	48.977908
1242.545777	143.337564	48.982913
1239.120312	149.306134	48.987917
1235.587081	143.034945	48.992922
1231.847865	144.446116	48.997927
1227.945980	149.366118	49.002932
1225.022424	148.099562	49.007937
1221.251769	163.575670	49.012941
1218.158009	147.291803	49.017946
1214.557654	148.681242	49.022951
1211.215216	155.680883	49.027956
1207.587394	151.398735	49.032961
1204.056268	159.266331	49.037965
1200.488415	156.993312	49.042970
1196.799732	156.577390	49.047975
1193.369533	164.913255	49.052980
1190.127328	153.803334	49.057985
1186.446271	156.632299	49.062989
1182.888713	153.800844	49.067994
1179.212852	150.813901	49.072999
1175.469892	157.458634	49.078004
1172.558879	145.980493	49.083009
1168.957180	156.409183	49.088013
1165.496840	150.885925	49.093018
1162.206772	154.413003	49.098023
1158.215387	155.037924	49.103028
1155.157331	153.820921	49.108033
1151.183384	153.927413	49.113037
1147.886892	153.507058	49.118042
1144.727810	148.436528	49.123047
1140.651780	148.198332	49.128052
1137.481310	149.305356	49.133057
1133.673564	149.006177	49.138061
1130.054906	160.212669	49.143066
1127.357049	150.782964	49.148071
1123.048101	158.962189	49.153076
1119.974819	153.881398	49.158081
1116.484926	150.463561	49.163085
1112.619127	156.630827	49.168090
1109.108441	150.625084	49.173095
1106.020845	156.907800	49.178100
1102.661266	155.155879	49.183105
1099.096153	154.397939	49.188109
1095.157064	156.846548	49.193114
1091.891120	145.879599	49.198119
1088.148207	150.024938	49.203124
1084.863004	146.749077	49.208129
1081.043269	152.988236	49.213133
1077.604349	149.445373	49.218138
1074.262135	147.972324	49.223143
1070.731397	151.480161	49.228148
1067.533469	143.698028	49.233153
1063.942723	152.745608	49.238157
1060.469231	149.065793	49.243162
1057.301537	150.134442	49.248167
1053.264243	152.250423	49.253172
1049.945525	142.962251	49.258177
1046.482295	143.817743	49.263181
1042.864542	151.566067	49.268186
1039.307304	148.367617	49.273191
1035.510836	148.588741	49.278196
1032.316572	138.901435	49.283201
1028.572911	146.735915	49.288205
1025.332930	145.917605	49.293210
1022.237735	145.797976	49.298215
1018.308052	150.089644	49.303220
1015.057533	141.787410	49.308225
1011.052483	152.231839	49.313229
1007.884318	144.144507	49.318234
1004.435582	143.744875	49.323239
1000.695804	146.567281	49.328244
997.536941	146.929037	49.333249
993.846124	147.355102	49.338253
990.259468	137.033215	49.343258
986.587226	140.234199	49.348263
982.949815	143.739785	49.353268
979.900491	141.970970	49.358273
976.203292	141.578614	49.363277
973.017419	149.740236	49.368282
969.447822	143.107852	49.373287
965.608701	148.062414	49.378292
962.167068	150.414201	49.383297
958.558707	151.004542	49.388301
954.769861	148.490972	49.393306
951.758207	147.655920	49.398311
948.355134	143.180500	49.403316
944.729895	146.557641	49.408321
941.095924	152.014775	49.413325
937.642596	147.559882	49.418330
934.469251	146.098408	49.423335
930.689718	152.581265	49.428340
927.300510	145.218287	49.433345
923.814301	154.853829	49.438349
920.319408	148.361630	49.443354
917.091864	145.956343	49.448359
912.918192	155.797612	49.453364
909.812114	152.009704	49.458369
906.005735	153.210048	49.463373
902.727167	150.755806	49.468378
899.593489	146.035738	49.473383
895.103679	148.149873	49.478388
892.060207	141.637624	49.483393
888.674036	151.042370	49.488397
885.040487	147.761018	49.493402
881.890182	135.912341	49.498407
878.017210	145.114899	49.503412
875.118916	143.028237	49.508417
871.414595	141.327221	49.513421
867.583773	142.458641	49.518426
864.255290	138.980830	49.523431
860.340805	138.401079	49.528436
857.321196	141.648613	49.533441
853.738505	142.035654	49.538445
850.040348	143.010263	49.543450
846.778979	140.721032	49.548455
842.858898	158.473263	49.553460
839.541598	138.617844	49.558465
836.108574	146.571425	49.563469
832.960617	146.637294	49.568474
829.404979	145.906448	49.573479
825.885585	139.576320	49.578484
822.202162	142.257087	49.583489
818.440272	143.934562	49.588493
815.055075	140.513108	49.593498
811.615456	134.926645	49.598503
807.847072	147.833484	49.603508
804.511164	143.958218	49.608513
800.990231	143.301044	49.613517
797.712985	148.515700	49.618522
794.454085	139.540981	49.623527
790.881925	159.864702	49.628532
787.246630	139.492785	49.633537
783.795946	151.391249	49.638541
779.979036	142.677928	49.643546
776.436751	141.660270	49.648551
772.599424	149.515831	49.653556
769.537858	140.269771	49.658561
766.051459	144.976178	49.663565
762.450352	138.513339	49.668570
759.225269	141.850028	49.673575
755.516112	137.732673	49.678580
751.948537	132.615534	49.683585
748.413292	138.316701	49.688589
745.039167	137.503679	49.693594
741.742328	134.217117	49.698599
737.848053	136.741106	49.703604
734.564982	138.878312	49.708609
731.405962	141.005583	49.713613
727.498957	140.548105	49.718618
724.162879	131.936689	49.723623
720.387476	134.609751	49.728628
716.838356	142.053193	49.733633
713.636523	136.518118	49.738637
710.141624	139.074489	49.743642
706.495352	147.039359	49.748647
702.777528	145.853064	49.753652
699.394944	140.251387	49.758657
696.153923	138.753140	49.763661
692.471400	134.068485	49.768666
689.074007	139.925257	49.773671
685.461187	148.470198	49.778676
682.438645	135.728392	49.783681
678.227276	135.578033	49.788685
674.967188	133.301321	49.793690
671.818770	135.047295	49.798695
667.663767	137.956999	49.803700
664.724115	133.421776	49.808705
660.911882	127.216681	49.813709
657.063489	134.514017	49.818714
653.791658	137.051292	49.823719
650.342514	137.553540	49.828724
646.969072	128.356381	49.833729
643.678214	127.533520	49.838733
640.399136	130.802771	49.843738
636.804608	136.798001	49.848743
632.864209	139.696257	49.853748
629.622055	134.018834	49.858753
625.857040	133.260748	49.863757
622.034612	140.756515	49.868762
618.916282	127.453933	49.873767
615.151414	126.376286	49.878772
611.873467	131.761949	49.883777
608.348034	133.978284	49.888781
604.933233	137.930038	49.893786
601.788738	143.506781	49.898791
598.011375	145.262697	49.903796
594.845415	138.915282	49.908801
590.908418	137.532404	49.913805
587.104592	134.546771	49.918810
584.135857	127.314251	49.923815
579.728422	138.416633	49.928820
576.652551	140.901096	49.933825
573.573861	135.353119	49.938829
570.039934	129.673962	49.943834
567.008003	133.625875	49.948839
562.860657	130.969307	49.953844
559.141920	136.753060	49.958849
555.691447	136.524714	49.963853
551.707921	137.699161	49.968858
548.922133	136.196108	49.973863
545.409533	144.440655	49.978868
542.328537	139.744112	49.983873
538.609692	134.682395	49.988877
534.993111	137.922284	49.993882
531.526987	133.276576	49.998887
527.574524	145.120818	50.003892
524.146097	133.293717	50.008897
520.530104	129.003686	50.013901
517.119618	138.523074	50.018906
513.733187	140.262086	50.023911
509.934558	141.451885	50.028916
507.246910	137.503678	50.033921
503.568025	138.342526	50.038925
500.000304	139.746101	50.043930
496.770229	135.965117	50.048935
492.585188	143.910038	50.053940
489.604318	137.976607	50.058945
485.657413	135.858163	50.063949
482.109303	133.085629	50.068954
478.974384	141.454539	50.073959
474.924012	136.650425	50.078964
471.917323	130.433143	50.083969
468.523444	129.477785	50.088973
464.034503	130.291667	50.093978
461.210870	135.786555	50.098983
457.805940	145.263963	50.103988
454.346226	139.962376	50.108993
451.118909	138.819582	50.113997
447.308544	132.997114	50.119002
444.031312	132.820770	50.124007
440.549345	142.626629	50.129012
436.920454	134.516790	50.134017
433.204980	134.412259	50.139021
429.540774	140.886717	50.144026
426.276763	132.697584	50.149031
422.657052	140.712170	50.154036
419.352960	134.462396	50.159041
415.637394	139.717352	50.164045
412.177096	144.584309	50.169050
408.649227	139.214322	50.174055
405.007772	142.575217	50.179060
401.948588	133.227701	50.184065
398.390088	129.741813	50.189069
394.639454	126.839686	50.194074
391.260140	125.628975	50.199079
387.656028	134.672522	50.204084
384.408788	134.513649	50.209089
380.961048	139.426105	50.214093
377.312635	142.898833	50.219098
373.726819	136.487561	50.224103
370.047687	150.740984	50.229108
366.624220	136.831403	50.234113
362.997098	134.137735	50.239117
359.606694	141.581742	50.244122
356.092985	135.988097	50.249127
352.775876	139.744299	50.254132
349.158754	131.740229	50.259137
345.719003	139.954444	50.264141
342.430320	137.913295	50.269146
338.904927	127.942803	50.274151
335.123081	133.012015	50.279156
331.514581	134.409388	50.284161
327.959512	129.401210	50.289165
324.443757	141.920601	50.294170
321.210178	134.571479	50.299175
317.494408	130.186435	50.304180
314.005858	127.335039	50.309185
310.267684	135.165735	50.314189
307.191742	131.136053	50.319194
303.966030	134.612195	50.324199
299.968264	137.899230	50.329204
296.660951	130.830593	50.334209
292.921041	131.837275	50.339213
289.648179	140.946026	50.344218
286.706757	135.715185	50.349223
282.843384	137.674529	50.354228
279.169522	129.748986	50.359233
275.244133	129.968473	50.364237
271.699522	131.210327	50.369242
268.560232	121.935535	50.374247
264.819323	131.380205	50.379252
261.631365	129.462516	50.384257
258.638638	130.184482	50.389261
254.726288	134.138369	50.394266
251.011554	124.833505	50.399271
247.288502	133.161732	50.404276
244.181976	126.998146	50.409281
240.660558	133.440809	50.414285
236.994881	136.925786	50.419290
233.805924	131.040874	50.424295
229.811130	139.405353	50.429300
226.372031	133.316019	50.434305
223.177810	135.730550	50.439309
219.810356	128.937127	50.444314
216.435211	134.208429	50.449319
212.138859	139.434223	50.454324
208.567005	133.251798	50.459329
205.190478	125.358807	50.464333
201.923532	132.217202	50.469338
198.502507	137.764621	50.474343
195.013462	136.707219	50.479348
191.974797	137.313016	50.484353
188.058786	135.797318	50.489357
184.355770	141.224403	50.494362
181.010691	129.232553	50.499367
176.958495	144.648635	50.504372
173.815219	136.728602	50.509377
170.518997	136.643921	50.514381
167.109461	135.982203	50.519386
163.928332	134.968324	50.524391
160.002638	136.557830	50.529396
156.474825	127.268021	50.534401
153.155591	131.511846	50.539405
149.674315	131.990846	50.544410
146.169621	124.484960	50.549415
142.611922	122.457564	50.554420
139.036086	125.928502	50.559425
135.333373	128.103186	50.564429
131.486672	138.323788	50.569434
128.310732	125.305712	50.574439
124.749085	133.757393	50.579444
121.742668	129.783330	50.584449
118.177092	126.374604	50.589453
114.232580	121.304152	50.594458
111.309007	127.289358	50.599463
107.179927	132.201086	50.604468
103.558459	126.523199	50.609473
100.253649	130.970429	50.614477
96.841842	129.799726	50.619482
93.802584	120.275219	50.624487
90.130679	136.580875	50.629492
86.423984	131.628199	50.634497
82.936219	125.157412	50.639501
79.128024	128.234504	50.644506
76.140743	124.732029	50.649511
72.527254	122.703912	50.654516
69.101642	129.520768	50.659521
65.255150	123.273874	50.664525
61.447562	127.331651	50.669530
58.420705	121.788417	50.674535
54.592291	134.299920	50.679540
51.716567	123.392545	50.684545
48.139689	125.205860	50.689549
44.748807	123.487730	50.694554
41.281990	118.019765	50.699559
37.345524	130.870906	50.704564
33.415157	129.107592	50.709569
30.609226	126.177838	50.714573
26.212992	126.575615	50.719578
23.507820	130.824514	50.724583
20.026322	126.092853	50.729588
16.203724	128.270550	50.734593
12.650922	128.283080	50.739597
9.115326	129.833677	50.744602
6.161220	119.830792	50.749607
2.514800	127.077739	50.754612