Thu Aug 25 16:21:00 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.832592	96.909981	0.000000
0.965185	108.196616	0.005005
0.923759	99.806468	0.010010
1.068032	109.616951	0.015014
0.816912	110.421978	0.020019
0.613942	93.233349	0.025024
0.413108	90.866715	0.030029
0.032348	75.705470	0.035034
0.009420	64.218265	0.040038
-0.303763	50.346766	0.045043
-0.288878	38.534111	0.050048
-0.886619	35.992390	0.055053
-0.856706	27.591099	0.060058
-1.536732	17.782438	0.065062
-1.557040	18.646210	0.070067
-1.848314	2.366852	0.075072
-2.111339	10.042278	0.080077
-2.533359	-8.829856	0.085082
-3.021698	-11.126120	0.090086
-3.351055	-7.654440	0.095091
-3.376240	-20.634534	0.100096
-3.980090	-13.728294	0.105101
-4.707691	-15.465047	0.110106
-4.424622	-6.726746	0.115110
-4.897806	-7.142944	0.120115
-4.725071	-12.004195	0.125120
-5.208663	-10.694510	0.130125
-6.045086	-12.740081	0.135130
-5.939208	-9.172081	0.140134
-6.333499	-4.753752	0.145139
-6.159797	-7.046179	0.150144
-6.583613	-6.005289	0.155149
-6.422400	-8.634281	0.160154
-6.531532	-16.975800	0.165158
-7.481949	-11.767982	0.170163
-7.823770	-13.172874	0.175168
-8.011727	-9.954305	0.180173
-7.962647	-10.784529	0.185178
-7.603231	-4.794844	0.190182
-8.166227	-8.132943	0.195187
-8.817297	-11.874859	0.200192
-9.309458	-9.067372	0.205197
-9.353201	-20.326633	0.210202
-9.083077	-14.028731	0.215206
-9.772955	-7.937916	0.220211
-10.196654	-14.622956	0.225216
-10.741608	-7.264032	0.230221
-10.904560	-10.503459	0.235226
-10.985302	-14.049997	0.240230
-11.192994	-1.175690	0.245235
-10.849462	-9.338200	0.250240
-10.832273	-5.379814	0.255245
-11.575158	-16.826927	0.260250
-11.975015	-15.628440	0.265254
-12.589344	-6.373043	0.270259
-12.181403	-9.284303	0.275264
-12.306953	-1.086254	0.280269
-13.071267	-4.630093	0.285274
-13.629281	-4.599564	0.290278
-13.666734	-8.273108	0.295283
-13.804779	-8.333691	0.300288
-13.968536	-6.093352	0.305293
-13.950006	2.259294	0.310298
-14.635770	-7.994543	0.315302
-15.293197	-9.704326	0.320307
-15.436574	-17.116659	0.325312
-15.447435	-4.469349	0.330317
-15.553199	-9.024371	0.335322
-15.090529	-12.858534	0.340326
-15.645641	-2.960678	0.345331
-16.498396	-11.935497	0.350336
-17.091512	-2.819464	0.355341
-17.000727	-7.047777	0.360346
-17.006347	-14.105208	0.365350
-17.356974	-10.092357	0.370355
-17.036160	-7.377448	0.375360
-17.677347	-11.304410	0.380365
-18.163896	-11.955796	0.385370
-18.068088	-10.357242	0.390374
-18.498807	-9.615828	0.395379
-18.309125	-15.574395	0.400384
-19.254056	-8.136983	0.405389
-19.907175	-10.280876	0.410394
-19.855508	-12.427630	0.415398
-20.310185	-13.745236	0.420403
-20.296207	-15.164746	0.425408
-20.153841	4.219524	0.430413
-20.405127	-5.314612	0.435418
-20.116996	-11.465777	0.440422
-20.493330	-9.226932	0.445427
-21.112398	-10.819338	0.450432
-21.013538	-12.967159	0.455437
-22.232285	-10.453952	0.460442
-22.018599	-4.792613	0.465446
-22.432119	-2.392916	0.470451
-22.443025	-6.386997	0.475456
-22.615602	-10.089989	0.480461
-22.862089	-3.473857	0.485466
-23.197335	-5.531514	0.490470
-23.445056	-10.175025	0.495475
-23.679300	-17.101719	0.500480
-23.855680	-5.045409	0.505485
-24.237391	-8.127173	0.510490
-24.699501	-8.712785	0.515494
-24.882087	-9.769302	0.520499
-24.834972	-13.756653	0.525504
-25.417791	-15.959016	0.530509
-25.207639	-12.461139	0.535514
-25.511506	-20.854400	0.540518
-26.497024	-15.188665	0.545523
-26.315037	-16.068186	0.550528
-26.857267	-18.786274	0.555533
-27.094408	-6.397742	0.560538
-26.969389	-7.243027	0.565542
-26.876165	-2.201893	0.570547
-27.687403	-12.600581	0.575552
-28.042806	-10.365016	0.580557
-28.418395	-10.657299	0.585562
-28.237040	-15.209850	0.590566
-28.410194	-12.385908	0.595571
-28.359228	-17.212258	0.600576
-29.171427	-16.452200	0.605581
-29.677983	-13.066653	0.610586
-29.885186	-13.356845	0.615590
-29.948664	-14.308638	0.620595
-29.788606	-15.523246	0.625600
-30.076680	-11.729004	0.630605
-30.186245	-7.807708	0.635610
-31.120242	-13.761053	0.640614
-31.749696	-12.529754	0.645619
-31.585612	-16.437355	0.650624
-32.013977	-7.046581	0.655629
-31.729923	-19.663836	0.660634
-31.442902	-15.905921	0.665638
-31.966406	-12.074791	0.670643
-32.510754	-21.249785	0.675648
-33.134209	-18.067386	0.680653
-33.332512	-9.766193	0.685658
-33.293227	-12.252694	0.690662
-33.868013	-1.513358	0.695667
-33.515128	-13.875646	0.700672
-33.592569	-7.276511	0.705677
-34.293969	-1.775512	0.710682
-34.177621	-9.098828	0.715686
-35.014483	-11.517651	0.720691
-34.989258	-11.622798	0.725696
-35.410920	-11.762328	0.730701
-35.714812	-15.998401	0.735706
-36.247612	-10.925620	0.740710
-36.414803	-18.726526	0.745715
-36.095442	-13.597441	0.750720
-36.401716	-14.141030	0.755725
-36.251461	-12.706033	0.760730
-36.827428	-10.739630	0.765734
-37.484223	-1.980616	0.770739
-37.515600	-10.286862	0.775744
-37.511491	-6.557383	0.780749
-38.505831	-3.930638	0.785754
-38.828476	-5.613781	0.790758
-39.161395	-3.476651	0.795763
-38.938192	-11.740527	0.800768
-38.898261	-5.868466	0.805773
-39.237830	-10.380526	0.810778
-39.356944	-5.581370	0.815782
-39.249736	-12.862123	0.820787
-39.858762	-6.749173	0.825792
-40.458678	-0.836967	0.830797
-40.722127	-10.441958	0.835802
-40.472413	-10.386127	0.840806
-41.025456	-4.911537	0.845811
-41.305581	-10.761691	0.850816
-41.650216	-11.568189	0.855821
-41.809305	-9.179886	0.860826
-41.872967	-10.612541	0.865830
-42.205665	-9.766262	0.870835
-43.013528	-6.624568	0.875840
-43.542049	-5.136999	0.880845
-43.497923	-7.443923	0.885850
-43.682346	-7.364361	0.890854
-43.380699	-5.867663	0.895859
-43.520097	-9.186710	0.900864
-44.004187	-9.262674	0.905869
-43.840360	-2.166666	0.910874
-44.206655	-8.544322	0.915878
-44.799997	2.264361	0.920883
-44.920109	-7.021404	0.925888
-45.494129	3.755780	0.930893
-45.859918	-2.128411	0.935898
-46.565438	-17.254501	0.940902
-46.797884	-4.986928	0.945907
-46.244427	-11.663721	0.950912
-46.348145	-2.902782	0.955917
-46.561623	-8.409037	0.960922
-46.408548	-1.048752	0.965926
-47.463708	2.340500	0.970931
-47.506416	-8.824013	0.975936
-47.893932	0.658440	0.980941
-48.046876	0.416694	0.985946
-47.843158	-4.715169	0.990950
-49.044548	-5.048901	0.995955
-49.174213	-6.591438	1.000960
-49.417836	-0.488284	1.005965
-49.643171	1.211209	1.010970
-49.462090	-6.906864	1.015974
-49.921305	-3.082641	1.020979
-49.852200	-5.377661	1.025984
-49.824487	-10.462961	1.030989
-50.963363	-3.896829	1.035994
-51.392102	-9.113090	1.040998
-51.380643	-14.293919	1.046003
-51.234209	-11.029669	1.051008
-51.622957	-4.647513	1.056013
-51.607976	-11.508853	1.061018
-51.674894	-11.355953	1.066022
-52.555932	-6.127365	1.071027
-52.327283	-13.515730	1.076032
-52.874871	-12.664254	1.081037
-52.854022	-10.244033	1.086042
-53.765880	-7.921277	1.091046
-54.053063	-4.124010	1.096051
-53.933085	-4.361064	1.101056
-53.986323	-7.329778	1.106061
-54.005794	-3.840214	1.111066
-53.965274	-13.094197	1.116070
-54.735499	-4.273118	1.121075
-55.300386	-7.414763	1.126080
-55.481485	-13.960640	1.131085
-55.412644	-1.145486	1.136090
-55.465612	-18.594783	1.141094
-56.659283	-3.816430	1.146099
-56.684004	-21.782680	1.151104
-56.618798	-8.346865	1.156109
-56.847259	-13.676763	1.161114
-56.627897	-9.579216	1.166118
-57.281962	-8.290274	1.171123
-57.653533	-13.287700	1.176128
-57.935132	-9.494473	1.181133
-58.612867	-5.895439	1.186138
-58.459525	-10.025985	1.191142
-58.854568	0.612421	1.196147
-58.514216	-7.790036	1.201152
-58.942105	-17.891276	1.206157
-59.458405	-8.803101	1.211162
-59.735156	-3.548974	1.216166
-59.926622	-12.728642	1.221171
-60.029559	-4.015283	1.226176
-59.897187	-14.890848	1.231181
-61.068037	-11.815665	1.236186
-61.135415	-13.522985	1.241190
-61.558359	-1.117993	1.246195
-61.138101	-13.854668	1.251200
-61.261068	-4.970492	1.256205
-61.941921	-4.335416	1.261210
-62.393113	-13.281396	1.266214
-62.625955	-6.616785	1.271219
-62.770315	-13.924557	1.276224
-63.033170	-6.211201	1.281229
-62.986701	-3.345740	1.286234
-62.713287	0.509222	1.291238
-63.579811	-7.533286	1.296243
-63.844683	-12.942901	1.301248
-64.413625	-12.853708	1.306253
-64.369771	-12.696018	1.311258
-64.392208	-4.343287	1.316262
-64.571129	-10.294719	1.321267
-65.662767	-15.676026	1.326272
-65.790304	-11.802535	1.331277
-65.832227	-15.304533	1.336282
-65.469373	-12.333623	1.341286
-65.871015	-9.486534	1.346291
-65.721961	-19.206773	1.351296
-66.522086	-10.969471	1.356301
-67.085815	-12.712913	1.361306
-67.409853	-7.438723	1.366310
-67.120919	-8.686180	1.371315
-67.887764	-8.664054	1.376320
-68.702483	-13.041547	1.381325
-68.205062	-10.926956	1.386330
-68.632090	-13.270786	1.391334
-68.949390	-6.453735	1.396339
-68.836321	-11.334109	1.401344
-69.100963	-14.829683	1.406349
-68.810659	-7.456103	1.411354
-69.386625	-10.232178	1.416358
-70.214421	-7.315150	1.421363
-70.097479	-15.866094	1.426368
-70.103427	-9.825496	1.431373
-70.401723	-6.270097	1.436378
-70.573385	-9.786568	1.441382
-71.270495	-10.455577	1.446387
-70.824278	-13.388655	1.451392
-71.301111	-6.825018	1.456397
-72.147924	-11.320869	1.461402
-72.116886	-7.624085	1.466406
-72.672241	-11.713186	1.471411
-72.819892	-10.706075	1.476416
-72.689355	-10.637899	1.481421
-72.985274	-7.111347	1.486426
-73.357279	-14.184131	1.491430
-74.347185	-13.408879	1.496435
-74.234546	-8.427739	1.501440
-74.373363	-7.073998	1.506445
-74.814970	-2.749496	1.511450
-74.376644	-11.360291	1.516454
-74.824645	-7.329018	1.521459
-74.750280	-12.225473	1.526464
-75.507618	-11.214579	1.531469
-75.781345	-3.597595	1.536474
-75.730440	-7.895589	1.541478
-75.934481	-15.269938	1.546483
-76.322915	-11.988319	1.551488
-76.939613	-12.388353	1.556493
-77.658001	-7.982517	1.561498
-77.426709	-15.997720	1.566502
-77.377667	-2.201865	1.571507
-77.263215	-12.217243	1.576512
-77.730735	-7.521685	1.581517
-78.146509	-4.881188	1.586522
-78.437900	-16.399034	1.591526
-78.851336	-13.714612	1.596531
-78.943594	-10.469910	1.601536
-79.009116	-11.373925	1.606541
-79.101583	-6.854194	1.611546
-79.994057	-11.099279	1.616550
-80.166378	-10.493264	1.621555
-80.513183	-16.684142	1.626560
-80.295685	-16.632755	1.631565
-80.443645	-11.351355	1.636570
-80.161933	-3.767620	1.641574
-81.007239	2.094454	1.646579
-81.629582	-6.498842	1.651584
-81.864025	-8.382465	1.656589
-82.137216	-12.756224	1.661594
-81.526733	-10.165803	1.666598
-82.529885	-10.479972	1.671603
-83.110546	-7.215689	1.676608
-83.016792	-14.225411	1.681613
-83.425253	-10.105421	1.686618
-83.245326	-9.545109	1.691622
-83.840389	0.441265	1.696627
-83.450522	0.354911	1.701632
-84.178376	-8.639468	1.706637
-84.764360	-3.726029	1.711642
-84.430980	-12.427947	1.716646
-85.080322	-5.388025	1.721651
-84.667097	-17.025769	1.726656
-85.471732	-8.189808	1.731661
-86.604574	-4.051224	1.736666
-86.198296	-5.016512	1.741670
-86.604826	-0.241923	1.746675
-86.151935	-9.946500	1.751680
-86.511307	-7.492012	1.756685
-86.913801	1.647938	1.761690
-86.861292	-15.299028	1.766694
-87.478305	-4.492968	1.771699
-87.549282	-8.205549	1.776704
-87.754557	-16.516177	1.781709
-88.356306	-2.994837	1.786714
-88.480426	-3.351831	1.791718
-89.315523	-10.114770	1.796723
-89.304386	-4.146450	1.801728
-89.156901	-6.903005	1.806733
-89.404027	-4.845756	1.811738
-89.301161	-12.287179	1.816742
-89.656349	-7.470016	1.821747
-90.222512	-10.212824	1.826752
-90.947648	-13.658386	1.831757
-91.379698	-6.070380	1.836762
-90.951545	-18.213500	1.841766
-91.151292	-1.762233	1.846771
-91.454588	-6.583694	1.851776
-91.265360	-4.484087	1.856781
-92.182571	-2.673018	1.861786
-92.238018	-6.350068	1.866790
-92.338516	-6.340602	1.871795
-92.808491	-14.030786	1.876800
-93.039919	-11.624820	1.881805
-93.236749	-5.291719	1.886810
-92.887314	-11.610676	1.891814
-93.577251	-8.022385	1.896819
-93.835091	-10.471818	1.901824
-93.964177	-12.897133	1.906829
-94.778615	-4.534198	1.911834
-94.765675	-15.039869	1.916838
-95.499580	0.159992	1.921843
-95.902528	-6.907945	1.926848
-95.403221	-4.629134	1.931853
-95.783323	-2.066993	1.936858
-95.370085	-12.274721	1.941862
-95.486578	-7.719587	1.946867
-96.080021	-3.257397	1.951872
-96.502184	-1.697906	1.956877
-97.024357	-3.394074	1.961882
-97.434112	-16.355028	1.966886
-98.046531	-3.091445	1.971891
-98.285327	-14.025907	1.976896
-98.441701	-7.540959	1.981901
-98.497136	-5.877579	1.986906
-98.051658	-18.393574	1.991910
-98.812230	-3.654610	1.996915
-98.675922	-12.231954	2.006912
-98.655756	-15.120900	2.016909
-98.634497	-5.383117	2.026906
-97.547702	0.756964	2.036902
-97.209476	-9.607175	2.046899
-96.890743	-8.035108	2.056896
-96.052330	-7.732401	2.066893
-95.586165	-6.446363	2.076890
-95.563238	-5.626234	2.086886
-94.998400	-7.377752	2.096883
-94.487701	-8.198952	2.106880
-93.265911	-10.705979	2.116877
-93.260169	-4.928697	2.126874
-92.953264	-3.091847	2.136870
-92.136483	-6.941921	2.146867
-91.692145	-10.077898	2.156864
-91.469907	-7.660743	2.166861
-90.729377	-10.583371	2.176858
-90.393886	-8.795350	2.186854
-89.320695	-6.273947	2.196851
-89.073351	-4.038124	2.206848
-88.904602	-13.371509	2.216845
-88.328345	-9.365732	2.226842
-87.450153	-10.821057	2.236838
-87.450435	-12.750120	2.246835
-86.965040	-14.026688	2.256832
-86.177772	-13.982062	2.266829
-85.941742	-10.578711	2.276826
-84.649366	-9.003983	2.286822
-84.542287	-13.084975	2.296819
-84.514945	-13.146189	2.306816
-83.478682	-9.063603	2.316813
-83.311018	-9.777200	2.326810
-83.059298	-7.903193	2.336806
-81.979578	-12.776487	2.346803
-81.892171	-20.025374	2.356800
-81.248794	-10.648002	2.366797
-80.196585	-10.508674	2.376794
-79.962986	-2.445087	2.386790
-80.042949	-9.487188	2.396787
-79.858288	-9.405159	2.406784
-78.559382	-8.997208	2.416781
-78.078297	-2.683019	2.426778
-77.148994	-9.642509	2.436774
-77.405946	-9.918938	2.446771
-77.240375	-10.730408	2.456768
-76.305433	-11.567398	2.466765
-75.728006	-15.193063	2.476762
-74.693282	-13.093287	2.486758
-74.638008	-12.756565	2.496755
-74.480533	-4.243893	2.506752
-73.378332	-9.104871	2.516749
-73.174704	-7.432404	2.526746
-73.346103	-5.108791	2.536742
-72.232295	-7.405660	2.546739
-71.993585	-11.260187	2.556736
-70.672781	-10.095391	2.566733
-70.504364	-11.005510	2.576730
-70.794921	-7.434115	2.586726
-69.654115	-10.657047	2.596723
-69.222097	-6.014111	2.606720
-68.376720	-8.664894	2.616717
-67.857443	-13.618266	2.626714
-67.759788	-5.919851	2.636710
-67.512916	-10.627800	2.646707
-66.821121	-13.172155	2.656704
-66.221831	-7.643099	2.666701
-65.266248	-7.995478	2.676698
-64.839140	-6.399209	2.686694
-64.741135	-9.490422	2.696691
-64.453099	-13.200623	2.706688
-63.559441	-10.799974	2.716685
-63.443642	-4.381030	2.726682
-62.771549	-7.647728	2.736678
-62.100423	-12.197237	2.746675
-61.984706	-12.056888	2.756672
-61.166209	-7.911667	2.766669
-60.432210	-12.141576	2.776666
-60.082639	-10.279732	2.786662
-59.429196	-11.440078	2.796659
-58.941417	-14.123528	2.806656
-59.054647	-5.973918	2.816653
-58.195695	-7.125284	2.826650
-57.726056	-8.526095	2.836646
-56.952115	-6.930317	2.846643
-56.280714	-9.626699	2.856640
-56.039811	-8.381391	2.866637
-55.945503	-4.927320	2.876634
-55.390612	-9.962300	2.886630
-54.834634	-5.570036	2.896627
-53.843875	-10.020742	2.906624
-53.144138	-6.661536	2.916621
-53.119572	-7.175313	2.926618
-53.224003	-2.026999	2.936614
-52.154473	-2.938928	2.946611
-51.645709	-2.888675	2.956608
-51.085910	-1.607802	2.966605
-50.340840	-10.077981	2.976602
-50.043123	-3.687541	2.986598
-50.079570	-10.597078	2.996595
-49.239201	-8.219754	3.006592
-48.681120	-11.433740	3.016589
-47.766603	-1.427266	3.026586
-47.366593	-0.963995	3.036582
-47.266212	-7.286752	3.046579
-46.817602	-10.600795	3.056576
-46.003656	-10.756750	3.066573
-45.866264	-9.061232	3.076570
-44.682393	-11.144159	3.086566
-44.055769	-12.468197	3.096563
-44.123553	-10.182995	3.106560
-44.126309	-6.948134	3.116557
-43.308732	-11.979923	3.126554
-42.677874	-8.663777	3.136550
-41.995462	-8.802290	3.146547
-41.174556	-13.172527	3.156544
-41.157346	-3.050799	3.166541
-41.006233	-13.328600	3.176538
-40.324541	-5.357396	3.186534
-39.362232	-9.458351	3.196531
-38.752476	-0.636402	3.206528
-38.185950	-5.647864	3.216525
-38.521679	-4.179155	3.226522
-37.951785	-6.903982	3.236518
-37.137673	-4.741121	3.246515
-36.844512	-4.229430	3.256512
-35.952710	-6.668906	3.266509
-35.416588	-2.831064	3.276506
-35.222148	-2.246883	3.286502
-34.314334	-1.042713	3.296499
-33.869246	-7.992856	3.306496
-33.514097	-7.953377	3.316493
-33.440608	-4.936370	3.326490
-32.420979	-1.617780	3.336486
-32.229586	-7.175516	3.346483
-31.415718	-9.631291	3.356480
-31.300811	-14.920446	3.366477
-30.383440	-5.516303	3.376474
-29.925566	-12.462112	3.386470
-29.304167	-7.538400	3.396467
-29.170844	-8.205433	3.406464
-29.004045	-12.679089	3.416461
-28.255285	-2.374208	3.426458
-27.602540	-7.510051	3.436454
-26.534437	-8.938107	3.446451
-26.198681	-3.592668	3.456448
-26.269080	-8.976335	3.466445
-25.859750	-6.230529	3.476442
-25.461365	-7.582160	3.486438
-24.450637	-11.722378	3.496435
-23.877265	-11.010669	3.506432
-24.011223	-7.837614	3.516429
-22.867684	-3.090746	3.526426
-22.559303	0.313945	3.536422
-22.396257	-3.946881	3.546419
-21.336433	-5.513023	3.556416
-21.086315	-3.708454	3.566413
-20.379040	-9.603612	3.576410
-19.596348	-5.237364	3.586406
-19.553939	-8.351545	3.596403
-19.333650	-13.470312	3.606400
-18.834530	-14.362554	3.616397
-18.118749	-9.760907	3.626394
-17.599625	-12.208513	3.636390
-16.694435	-13.753593	3.646387
-16.492982	-11.694309	3.656384
-16.166152	-10.370596	3.666381
-15.227760	-2.268546	3.676378
-14.884229	-2.768943	3.686374
-15.035753	-2.494854	3.696371
-14.114347	-8.094111	3.706368
-13.391278	-6.648748	3.716365
-12.991951	-2.745121	3.726362
-12.388123	-7.246072	3.736358
-11.729661	-3.734674	3.746355
-11.581777	-13.739539	3.756352
-11.340693	-13.602992	3.766349
-10.391350	-11.033664	3.776346
-10.278484	-4.053553	3.786342
-9.375747	-3.631035	3.796339
-8.601584	-6.391034	3.806336
-8.819113	-4.069697	3.816333
-8.021998	-0.532506	3.826330
-7.243655	-5.624672	3.836326
-7.507770	-7.654950	3.846323
-6.583067	-7.105993	3.856320
-6.168565	-0.657818	3.866317
-5.640897	-2.302138	3.876314
-5.140341	-0.625505	3.886310
-4.551336	17.262834	3.896307
-3.956974	20.575205	3.906304
-3.810274	23.476209	3.916301
-3.647587	29.415817	3.926298
-3.090340	44.239541	3.936294
-2.408516	56.081840	3.946291
-2.072372	66.321535	3.956288
-1.393279	81.699576	3.966285
-1.003531	91.062901	3.976282
-0.532244	103.612968	3.986278
0.000000	120.400088	3.991283
-0.117396	129.223349	3.996288
0.277668	133.454757	4.001293
0.391487	150.537260	4.006298
0.580043	151.801753	4.011302
1.074177	158.488567	4.016307
1.031032	158.900338	4.021312
1.108969	159.144439	4.026317
0.637826	149.470657	4.031322
0.475495	138.321626	4.036326
1.158665	151.597469	4.041331
0.595292	153.467001	4.046336
0.685200	146.290133	4.051341
0.960109	160.636036	4.056346
1.001189	162.939215	4.061350
1.172155	162.915637	4.066355
0.695712	151.613330	4.071360
0.738891	147.357637	4.076365
0.445442	168.677011	4.081370
0.617335	166.796139	4.086374
0.967978	167.193668	4.091379
0.695248	160.589312	4.096384
1.084729	157.968823	4.101389
1.005766	167.801660	4.106394
1.020021	155.960552	4.111398
1.038800	165.752763	4.116403
0.748272	152.051644	4.121408
0.960750	153.527527	4.126413
0.238857	169.731739	4.131418
0.596221	163.550684	4.136422
1.054204	166.377008	4.141427
1.164091	178.667004	4.146432
1.445908	180.701509	4.151437
1.406202	180.027559	4.156442
1.208983	163.780773	4.161446
1.106707	173.468567	4.166451
0.770378	166.627398	4.171456
0.850894	165.146827	4.176461
1.430290	172.294856	4.181466
1.164883	173.355228	4.186470
1.108008	169.691018	4.191475
0.994889	172.961169	4.196480
1.492685	186.699524	4.201485
1.219145	178.709544	4.206490
1.196012	173.208207	4.211494
0.870350	163.913426	4.216499
1.222467	179.813326	4.221504
1.420402	183.990210	4.226509
0.887770	185.734703	4.231514
1.251957	188.863633	4.236518
1.526116	183.689041	4.241523
1.473224	189.863617	4.246528
1.384899	185.166605	4.251533
1.457191	193.912721	4.256538
1.403302	185.777589	4.261542
1.170953	190.660980	4.266547
1.516937	189.651349	4.271552
1.446741	187.311690	4.276557
1.351405	195.350069	4.281562
1.672681	189.478384	4.286566
1.697807	198.804540	4.291571
1.582509	184.120472	4.296576
1.589700	188.339899	4.301581
1.285880	181.269001	4.306586
1.397465	180.296096	4.311590
1.727027	182.095326	4.316595
1.495507	185.963007	4.321600
1.484450	168.323451	4.326605
1.467035	181.851457	4.331610
1.568388	186.537027	4.336614
1.941698	190.518753	4.341619
1.477234	188.721766	4.346624
1.846575	170.820123	4.351629
1.469317	170.961537	4.356634
1.416878	170.653419	4.361638
1.399574	173.446644	4.366643
1.289373	176.887184	4.371648
1.551177	187.198157	4.376653
1.316798	197.213551	4.381658
1.680044	192.787474	4.386662
1.537110	193.471148	4.391667
1.232669	200.086945	4.396672
1.546489	192.821191	4.401677
1.595767	186.881391	4.406682
1.431743	196.493450	4.411686
1.579944	194.372675	4.416691
1.308439	198.831926	4.421696
1.754610	210.699090	4.426701
1.551482	224.718142	4.431706
1.582489	216.917713	4.436710
1.785571	212.947004	4.441715
2.014777	222.162101	4.446720
2.126710	216.630096	4.451725
1.986060	216.607886	4.456730
1.841571	220.616964	4.461734
2.114013	222.311252	4.466739
2.028458	222.157020	4.471744
2.258786	214.110224	4.476749
1.906783	211.580595	4.481754
1.875636	199.797193	4.486758
1.958485	196.009843	4.491763
1.728333	198.858568	4.496768
1.651365	211.778986	4.501773
1.711681	222.380981	4.506778
1.969406	221.755342	4.511782
2.140454	221.567233	4.516787
1.891952	232.581458	4.521792
2.148169	224.245858	4.526797
1.836313	230.027583	4.531802
1.658912	228.634874	4.536806
1.870704	221.188939	4.541811
1.732541	219.840705	4.546816
1.919873	218.191530	4.551821
2.127155	222.126510	4.556826
2.179477	217.391633	4.561830
2.043284	216.609411	4.566835
1.954452	228.800862	4.571840
1.968992	217.677853	4.576845
2.057997	225.608267	4.581850
2.093501	233.056678	4.586854
2.578510	234.186142	4.591859
2.163021	228.404572	4.596864
2.302204	224.367940	4.601869
2.292154	227.027157	4.606874
2.059700	216.670524	4.611878
1.975519	223.422663	4.616883
2.068206	241.581094	4.621888
2.159517	239.320529	4.626893
1.954069	242.962670	4.631898
2.233645	243.687716	4.636902
2.452705	243.375024	4.641907
2.431176	246.681459	4.646912
2.456144	239.802636	4.651917
2.235766	247.344930	4.656922
2.388562	244.400838	4.661926
2.727943	243.942741	4.666931
2.039958	241.446767	4.671936
2.787434	239.396609	4.676941
2.364126	244.746540	4.681946
2.382060	250.650609	4.686950
2.589171	251.709718	4.691955
2.214366	249.515856	4.696960
2.540144	243.868078	4.701965
2.552071	239.044610	4.706970
2.629797	239.712696	4.711974
2.667182	252.624719	4.716979
2.252302	255.923183	4.721984
2.500938	247.088879	4.726989
2.330022	240.234419	4.731994
2.105763	242.664605	4.736998
2.623298	243.317565	4.742003
2.695471	242.648230	4.747008
2.546446	236.419940	4.752013
2.366922	240.130786	4.757018
2.876676	240.471749	4.762022
2.929687	246.803762	4.767027
2.610793	244.775150	4.772032
2.748973	242.102273	4.777037
2.567511	251.188737	4.782042
2.545939	246.857743	4.787046
2.636281	237.311077	4.792051
2.665236	239.407354	4.797056
2.793715	244.980883	4.802061
2.341507	253.208084	4.807066
2.244058	247.664583	4.812070
2.811154	244.022817	4.817075
2.481099	245.007900	4.822080
2.762192	242.916918	4.827085
2.974989	246.120199	4.832090
2.602303	252.775182	4.837094
2.780085	257.141906	4.842099
2.923623	266.708977	4.847104
3.059551	257.598092	4.852109
2.826308	261.475550	4.857114
2.700391	251.080057	4.862118
2.711541	246.095355	4.867123
2.620878	267.740584	4.872128
2.660468	267.446520	4.877133
2.645157	276.766397	4.882138
2.977587	273.047495	4.887142
2.693177	268.773497	4.892147
2.674249	280.821150	4.897152
3.207645	268.420891	4.902157
2.714899	275.126332	4.907162
2.620640	275.859332	4.912166
3.266504	274.299663	4.917171
3.105789	268.924259	4.922176
2.922262	273.774713	4.927181
2.665800	272.388061	4.932186
2.971033	275.007377	4.937190
2.833242	275.057487	4.942195
2.667141	272.302564	4.947200
3.243595	285.775566	4.952205
3.395151	291.750463	4.957210
2.912483	291.598339	4.962214
3.226696	295.997480	4.967219
3.138959	301.063891	4.972224
3.528956	297.851668	4.977229
3.180876	285.969167	4.982234
3.131948	280.354777	4.987238
3.382731	272.377518	4.992243
2.902914	271.674444	4.997248
2.975653	263.652317	5.002253
3.528275	294.754669	5.007258
3.131034	286.369562	5.012262
3.131077	288.793084	5.017267
3.228332	303.394733	5.022272
3.292960	302.799346	5.027277
3.411714	301.648137	5.032282
3.355827	302.656706	5.037286
3.033853	298.850503	5.042291
2.823732	308.615380	5.047296
3.359685	301.185062	5.052301
3.416755	310.126612	5.057306
3.252435	300.376200	5.062310
3.361067	304.880323	5.067315
2.961229	311.131448	5.072320
3.534773	301.676722	5.077325
3.069312	306.587177	5.082330
3.002377	309.524244	5.087334
3.505492	305.984241	5.092339
3.181088	304.032417	5.097344
3.198135	303.128102	5.102349
3.230636	310.577016	5.107354
3.222457	325.584352	5.112358
3.746281	322.461889	5.117363
3.707326	328.007893	5.122368
3.362780	327.723394	5.127373
3.294365	328.256190	5.132378
3.641878	332.134420	5.137382
4.137301	323.384800	5.142387
3.793057	335.796680	5.147392
3.750067	318.304351	5.152397
3.712921	309.720441	5.157402
3.464260	312.252538	5.162406
3.619647	303.056322	5.167411
3.454983	309.011166	5.172416
3.747753	321.326391	5.177421
3.709509	328.884476	5.182426
3.594315	317.851336	5.187430
3.738192	313.440617	5.192435
3.592203	332.032014	5.197440
3.752136	337.771490	5.202445
3.490041	332.845396	5.207450
3.474671	332.199265	5.212454
3.937008	332.769127	5.217459
3.895634	334.357568	5.222464
3.671329	327.008392	5.227469
3.612224	329.732259	5.232474
3.690917	331.469569	5.237478
3.626254	333.510922	5.242483
3.796674	335.012393	5.247488
3.979166	331.677648	5.252493
4.009406	334.637459	5.257498
3.990847	338.437003	5.262502
4.209567	333.660205	5.267507
3.987304	332.094180	5.272512
3.958290	336.854000	5.277517
4.214452	337.857972	5.282522
4.092985	341.730589	5.287526
3.788376	322.286037	5.292531
3.839847	336.632289	5.297536
4.009182	326.358175	5.302541
3.846366	326.899434	5.307546
4.193358	332.036948	5.312550
4.475351	333.941726	5.317555
3.811301	328.186413	5.322560
4.087265	321.552975	5.327565
3.735438	319.953466	5.332570
3.734053	330.811971	5.337574
4.051441	327.361177	5.342579
3.708988	336.833585	5.347584
4.104332	327.004960	5.352589
3.611939	330.211177	5.357594
3.903420	330.516737	5.362598
3.725050	328.269940	5.367603
3.893605	334.786365	5.372608
4.060431	326.743141	5.377613
4.010429	335.717299	5.382618
4.241979	344.112662	5.387622
4.326093	346.807764	5.392627
4.088750	350.087920	5.397632
4.343354	346.055323	5.402637
4.415001	356.522742	5.407642
4.302457	351.990835	5.412646
4.221141	329.195598	5.417651
4.117325	342.177266	5.422656
4.376588	338.267330	5.427661
4.357338	349.242543	5.432666
4.390211	347.152475	5.437670
3.924124	334.858151	5.442675
4.119237	347.473440	5.447680
4.401710	349.492042	5.452685
4.375992	353.450903	5.457690
4.247933	358.495173	5.462694
4.485303	360.397454	5.467699
4.809340	359.957578	5.472704
4.647942	354.227906	5.477709
4.494852	346.687225	5.482714
4.128823	331.226055	5.487718
4.491350	342.192067	5.492723
4.450209	353.183367	5.497728
4.495248	364.091568	5.502733
4.707803	357.914152	5.507738
4.475124	347.358157	5.512742
4.397671	344.728542	5.517747
4.500068	364.492801	5.522752
4.786451	350.112665	5.527757
4.591188	351.184204	5.532762
4.189007	350.313935	5.537766
4.434952	356.951123	5.542771
4.460472	369.779666	5.547776
4.414222	360.738402	5.552781
4.518258	371.861995	5.557786
4.601039	361.778597	5.562790
4.630803	355.392535	5.567795
4.441812	359.582627	5.572800
4.502283	358.934104	5.577805
4.429594	353.212680	5.582810
4.543906	367.169451	5.587814
4.938083	354.743489	5.592819
4.426848	359.800339	5.597824
4.539188	367.189310	5.602829
4.422330	363.774908	5.607834
4.263266	360.458872	5.612838
4.760162	371.293115	5.617843
4.643132	389.247267	5.622848
4.984346	380.841329	5.627853
4.970283	384.659161	5.632858
4.740735	391.870750	5.637862
4.815549	389.568456	5.642867
5.009251	390.417698	5.647872
4.872737	383.621070	5.652877
4.653081	384.778692	5.657882
4.704428	395.084795	5.662886
4.935505	379.324377	5.667891
4.553608	393.665807	5.672896
4.597773	387.011715	5.677901
4.627843	395.460817	5.682906
5.228206	388.159580	5.687910
4.686705	382.305952	5.692915
4.859663	396.323161	5.697920
4.677103	395.804466	5.702925
5.102956	396.832476	5.707930
4.853504	392.575117	5.712934
5.063931	381.000524	5.717939
5.025679	395.009695	5.722944
4.908811	387.324113	5.727949
4.986628	379.873792	5.732954
4.850586	390.797726	5.737958
5.291817	386.814974	5.742963
4.931692	384.644106	5.747968
5.095116	379.328616	5.752973
5.197938	384.513893	5.757978
4.787851	387.653439	5.762982
4.949590	384.850296	5.767987
4.955724	399.978841	5.772992
5.293168	402.760813	5.777997
5.295993	414.640629	5.783002
5.169174	422.136699	5.788006
5.466088	418.875761	5.793011
5.175083	409.762087	5.798016
5.208167	397.380017	5.803021
5.555854	396.411238	5.808026
5.048030	385.847708	5.813030
5.172488	380.585781	5.818035
5.360135	399.124973	5.823040
5.477799	399.084435	5.828045
4.915835	390.816840	5.833050
5.231609	407.975517	5.838054
5.386948	404.670324	5.843059
5.525449	407.366405	5.848064
5.522724	413.182013	5.853069
5.277180	408.186863	5.858074
5.197156	405.978433	5.863078
5.390448	405.074973	5.868083
5.363146	418.639510	5.873088
5.514536	413.148721	5.878093
5.669457	409.179186	5.883098
5.203657	405.531540	5.888102
5.358562	402.451048	5.893107
5.521134	408.709003	5.898112
5.165211	404.996684	5.903117
5.588259	410.350100	5.908122
5.092035	424.858169	5.913126
5.247588	414.260288	5.918131
5.394654	418.704632	5.923136
5.321511	413.245859	5.928141
5.798861	414.262637	5.933146
5.488156	410.865944	5.938150
5.730468	408.894918	5.943155
5.568699	409.698614	5.948160
5.352272	414.051209	5.953165
5.520628	415.821937	5.958170
5.180785	408.054220	5.963174
5.374783	412.820249	5.968179
5.277125	418.631750	5.973184
5.482532	416.669669	5.978189
5.895313	431.402324	5.983194
5.813491	440.726380	5.988198
6.002412	428.614109	5.993203
5.680443	424.143471	5.998208
5.506265	412.866407	6.003213
5.666446	420.902819	6.008218
5.400633	425.981347	6.013222
5.549224	430.808280	6.018227
5.694773	438.502134	6.023232
5.808478	429.217468	6.028237
5.744790	427.161504	6.033242
5.404148	433.650176	6.038246
6.162171	437.350212	6.043251
5.775845	437.375985	6.048256
5.892746	428.777373	6.053261
5.736247	420.544314	6.058266
5.508767	424.259548	6.063270
5.752379	414.970355	6.068275
5.522859	420.191896	6.073280
5.823000	436.008417	6.078285
5.981344	424.119245	6.083290
5.419140	428.130541	6.088294
5.762093	417.965216	6.093299
5.193995	428.615173	6.098304
5.656561	431.953365	6.103309
5.688607	432.802627	6.108314
5.560878	435.467658	6.113318
6.087468	431.974573	6.118323
5.826733	433.546771	6.123328
5.684787	431.392333	6.128333
6.015619	429.594103	6.133338
5.865879	425.219870	6.138342
5.680832	414.868348	6.143347
5.281657	419.996245	6.148352
5.310226	422.007180	6.153357
5.600407	427.492154	6.158362
5.909128	434.945299	6.163366
6.137086	427.787818	6.168371
5.624539	432.458905	6.173376
5.679337	420.415112	6.178381
5.835305	422.719307	6.183386
5.820243	428.106570	6.188390
6.169062	420.585297	6.193395
6.034852	419.476880	6.198400
5.728479	405.483811	6.203405
5.679571	416.561791	6.208410
5.789488	419.572409	6.213414
5.732210	411.776237	6.218419
5.734361	423.070853	6.223424
5.552558	424.254186	6.228429
5.935464	412.276052	6.233434
5.650881	420.353675	6.238438
5.738845	414.278021	6.243443
5.724306	416.045767	6.248448
5.932712	418.813157	6.253453
5.970134	416.848922	6.258458
5.451418	421.416566	6.263462
5.801783	412.945902	6.268467
5.626948	417.785541	6.273472
5.728503	420.784814	6.278477
5.937421	409.656541	6.283482
5.678675	419.049436	6.288486
5.786915	414.473429	6.293491
5.402118	424.528337	6.298496
5.778662	413.044758	6.303501
5.917354	420.293577	6.308506
5.586562	424.458444	6.313510
5.618984	420.052507	6.318515
6.011367	419.155819	6.323520
5.548754	420.718517	6.328525
5.666379	419.469399	6.333530
5.530810	416.573625	6.338534
5.835604	419.009529	6.343539
5.292803	420.470892	6.348544
5.706567	421.437520	6.353549
5.423960	413.546934	6.358554
5.424452	419.150063	6.363558
5.793888	408.581950	6.368563
5.717343	413.146753	6.373568
5.822817	412.598747	6.378573
5.632957	413.590348	6.383578
5.817576	418.876717	6.388582
6.105813	411.947086	6.393587
5.612055	420.446636	6.398592
5.536756	411.792723	6.403597
5.873964	407.538356	6.408602
5.727405	420.403388	6.413606
5.850144	418.150531	6.418611
5.721987	418.882521	6.423616
6.040752	420.835332	6.428621
6.031243	415.546927	6.433626
5.779625	423.986393	6.438630
5.914938	413.964338	6.443635
5.622363	398.978831	6.448640
5.558850	395.287139	6.453645
5.765047	410.194517	6.458650
5.889399	410.295304	6.463654
5.703942	389.177323	6.468659
5.394203	392.430864	6.473664
5.814074	398.990196	6.478669
6.086516	404.769015	6.483674
5.291351	401.853200	6.488678
5.334213	400.808791	6.493683
5.363905	414.949705	6.498688
6.020058	413.426380	6.503693
5.949596	413.117917	6.508698
5.837588	421.241270	6.513702
6.132178	413.190644	6.518707
5.970924	404.382518	6.523712
5.539492	383.916867	6.528717
5.495234	386.337852	6.533722
5.420256	395.920247	6.538726
5.528184	399.905635	6.543731
5.444713	404.161465	6.548736
5.635946	407.804763	6.553741
5.843905	408.892224	6.558746
5.674570	413.886028	6.563750
5.944035	412.534024	6.568755
5.875672	413.819807	6.573760
5.869757	406.920447	6.578765
5.600883	400.100257	6.583770
5.646991	401.788895	6.588774
5.876118	393.792828	6.593779
5.684801	393.193246	6.598784
5.380533	397.303330	6.603789
5.548674	402.291712	6.608794
5.372823	417.746187	6.613798
6.100369	414.389304	6.618803
5.890348	420.303834	6.623808
5.539807	412.477678	6.628813
5.798171	410.156115	6.633818
5.663814	406.981735	6.638822
5.441503	392.636974	6.643827
5.280135	411.949055	6.648832
5.423516	425.480526	6.653837
5.924181	423.848680	6.658842
5.639984	427.506361	6.663846
6.104804	410.674716	6.668851
5.679372	421.330790	6.673856
6.007318	420.156289	6.678861
5.993926	420.487472	6.683866
5.251662	408.527442	6.688870
5.749750	417.627743	6.693875
5.796810	415.266519	6.698880
5.563787	415.910532	6.703885
5.539313	409.656338	6.708890
5.727856	418.251468	6.713894
5.723105	424.472369	6.718899
5.567091	418.485561	6.723904
5.723278	420.565089	6.728909
5.747655	424.310466	6.733914
5.596807	426.444429	6.738918
6.012648	423.471750	6.743923
5.857676	423.553025	6.748928
6.063503	418.177095	6.753933
5.471675	401.197797	6.758938
5.567445	402.679331	6.763942
6.004715	400.614483	6.768947
5.464080	396.671673	6.773952
5.565792	392.922455	6.778957
5.908612	407.267408	6.783962
5.709106	400.945727	6.788966
5.333296	393.028624	6.793971
5.982543	409.821834	6.798976
5.426354	405.020894	6.803981
5.294629	407.310050	6.808986
5.741794	410.555736	6.813990
5.560076	402.557596	6.818995
5.501116	413.785850	6.824000
5.795693	413.483469	6.829005
5.515002	409.056990	6.834010
5.206246	420.213652	6.839014
5.559581	419.962178	6.844019
5.278922	417.190380	6.849024
5.219953	425.004859	6.854029
5.621979	415.118190	6.859034
5.767398	422.644374	6.864038
5.832390	420.248700	6.869043
5.799002	416.805391	6.874048
5.415691	416.593404	6.879053
5.665878	412.817756	6.884058
5.437037	430.628113	6.889062
5.637191	431.663013	6.894067
5.546284	436.416738	6.899072
5.667927	431.636141	6.904077
6.096666	442.772180	6.909082
5.869230	431.810341	6.914086
5.950870	422.723697	6.919091
5.975167	419.976886	6.924096
5.752545	413.548088	6.929101
5.747742	415.795212	6.934106
5.527346	420.790690	6.939110
6.202530	410.813767	6.944115
5.551170	417.211909	6.949120
5.540661	414.350326	6.954125
5.457725	414.534213	6.959130
5.546050	419.750247	6.964134
5.933354	413.137297	6.969139
5.657475	409.599102	6.974144
5.590379	423.369199	6.979149
5.827572	405.462716	6.984154
5.307005	414.804881	6.989158
5.612554	407.148020	6.994163
5.509838	415.137033	6.999168
5.693937	419.534445	7.004173
6.103520	411.699926	7.009178
5.635117	411.539238	7.014182
5.673116	413.570842	7.019187
5.616988	413.557535	7.024192
5.661504	413.496820	7.029197
5.813243	410.742698	7.034202
5.402440	415.527557	7.039206
5.828200	417.172530	7.044211
5.809111	418.172176	7.049216
5.599825	415.534732	7.054221
5.829871	413.853537	7.059226
5.518939	411.554732	7.064230
5.724582	398.607771	7.069235
5.758331	408.065566	7.074240
5.722544	412.639802	7.079245
5.844449	413.342102	7.084250
5.623124	425.345633	7.089254
5.743193	414.487549	7.094259
5.653523	413.764469	7.099264
5.524950	421.979005	7.104269
5.696363	410.125761	7.109274
5.463652	428.594801	7.114278
5.754642	427.742474	7.119283
5.945151	440.130753	7.124288
5.881699	424.944804	7.129293
5.919364	413.482683	7.134298
5.808797	418.296433	7.139302
5.658169	411.407090	7.144307
5.549429	414.496261	7.149312
5.565545	415.670729	7.154317
6.090413	414.547634	7.159322
5.951792	419.043069	7.164326
5.892611	418.701200	7.169331
5.845099	423.982812	7.174336
5.677582	411.825157	7.179341
5.792638	415.714517	7.184346
5.710437	420.004953	7.189350
6.011840	421.498564	7.194355
5.784233	419.031674	7.199360
5.880450	415.330771	7.204365
6.252385	414.782145	7.209370
5.795397	415.176504	7.214374
5.948243	415.358251	7.219379
5.530084	393.447799	7.224384
5.561350	403.152759	7.229389
5.636220	405.457003	7.234394
5.827041	409.068728	7.239398
5.784451	407.294206	7.244403
6.094383	406.318686	7.249408
5.837306	399.502975	7.254413
5.900559	391.358887	7.259418
5.442566	395.053284	7.264422
5.470408	391.439031	7.269427
5.541422	391.159023	7.274432
5.165551	385.080122	7.279437
5.878197	395.861593	7.284442
5.685073	415.608934	7.289446
5.738015	414.357296	7.294451
5.494862	416.594307	7.299456
5.823299	424.518934	7.304461
5.681578	412.474299	7.309466
5.829915	416.738105	7.314470
5.958739	412.614466	7.319475
5.526176	407.927037	7.324480
5.719064	412.123749	7.329485
5.802141	413.676878	7.334490
5.621917	399.901336	7.339494
5.626526	399.843710	7.344499
5.586213	399.954479	7.349504
5.703152	415.094150	7.354509
5.972332	416.241624	7.359514
5.740305	398.800982	7.364518
5.661086	390.691873	7.369523
5.601490	394.826897	7.374528
5.362867	398.945679	7.379533
6.133788	412.249099	7.384538
5.728546	408.914676	7.389542
5.523666	392.102555	7.394547
5.737539	398.738457	7.399552
5.634256	410.223596	7.404557
5.502520	408.886995	7.409562
5.656698	419.705361	7.414566
5.765654	411.550940	7.419571
5.418455	428.149106	7.424576
5.366900	409.765826	7.429581
5.506740	418.365423	7.434586
5.541478	422.628047	7.439590
5.719286	416.864190	7.444595
5.793754	416.112229	7.449600
5.408285	410.563184	7.454605
5.750497	413.034355	7.459610
5.582919	417.948789	7.464614
5.851517	414.252515	7.469619
5.712194	419.080262	7.474624
5.580270	429.491032	7.479629
5.745371	425.114927	7.484634
5.929025	426.968682	7.489638
5.680277	421.730415	7.494643
5.919844	424.176540	7.499648
5.865465	424.957083	7.504653
5.908154	421.255073	7.509658
5.364899	424.485095	7.514662
5.651210	419.903333	7.519667
5.792625	423.636700	7.524672
5.470721	420.754302	7.529677
5.843947	420.841406	7.534682
5.592349	425.379854	7.539686
5.782641	419.965227	7.544691
5.590029	416.160877	7.549696
5.478489	423.135684	7.554701
5.493487	426.328859	7.559706
5.331998	427.433077	7.564710
5.726803	413.108671	7.569715
5.526562	420.489690	7.574720
5.328935	418.135165	7.579725
5.274218	422.595307	7.584730
5.332999	434.336651	7.589734
5.736355	431.875305	7.594739
5.776851	441.999632	7.599744
5.992515	447.414027	7.604749
6.172976	441.494719	7.609754
5.715737	435.311486	7.614758
5.698052	419.985490	7.619763
5.774573	426.070267	7.624768
5.611482	429.304001	7.629773
5.922692	427.916981	7.634778
5.637660	421.017054	7.639782
5.311450	418.163806	7.644787
5.584140	423.018750	7.649792
5.240347	420.576392	7.654797
5.825836	440.666851	7.659802
5.696568	446.837664	7.664806
5.800803	442.119905	7.669811
5.969329	440.331284	7.674816
5.648713	436.588116	7.679821
5.632454	425.491950	7.684826
5.535039	425.883756	7.689830
5.658746	432.423063	7.694835
6.117955	439.900088	7.699840
5.710548	437.891649	7.704845
5.459684	428.733710	7.709850
5.391674	431.889270	7.714854
5.804739	434.896687	7.719859
6.021148	444.828934	7.724864
5.669204	439.379033	7.729869
5.661705	429.857087	7.734874
5.476416	436.508086	7.739878
5.509798	435.759398	7.744883
6.033578	441.103368	7.749888
5.685722	438.421192	7.754893
6.096424	421.911236	7.759898
5.684752	431.865952	7.764902
5.798077	429.133665	7.769907
6.066368	420.473370	7.774912
5.773638	420.601541	7.779917
5.683248	421.960381	7.784922
5.295082	426.311414	7.789926
5.270750	427.713689	7.794931
5.450042	436.572876	7.799936
5.617697	445.538298	7.804941
6.002195	442.605329	7.809946
5.517522	436.369446	7.814950
5.726643	447.359559	7.819955
5.962033	443.143284	7.824960
5.840098	442.586614	7.829965
5.790705	429.103772	7.834970
5.463728	426.712563	7.839974
5.792225	420.358768	7.844979
5.312223	431.384075	7.849984
5.638102	449.572622	7.854989
5.805538	445.031626	7.859994
5.837432	443.397294	7.864998
5.616035	442.027282	7.870003
5.474299	441.381963	7.875008
5.612866	447.593072	7.880013
5.652140	448.146964	7.885018
5.819349	454.356751	7.890022
6.208111	446.114180	7.895027
5.720389	443.615273	7.900032
5.499086	434.977897	7.905037
5.792124	434.106266	7.910042
5.663778	430.067211	7.915046
5.613733	426.256340	7.920051
5.760018	425.398211	7.925056
5.638956	434.896096	7.930061
5.526628	436.150804	7.935066
5.759059	445.789467	7.940070
5.600252	441.957668	7.945075
5.898924	436.469105	7.950080
5.626960	438.830860	7.955085
5.829424	433.958503	7.960090
5.834738	438.928113	7.965094
5.696591	436.469351	7.970099
5.762772	435.342190	7.975104
5.605238	435.186579	7.980109
5.945720	418.592714	7.985114
5.587002	425.834046	7.990118
5.739865	421.261143	7.995136
6.059487	434.209729	8.000154
5.639396	439.113394	8.005171
5.747396	431.696232	8.010189
5.966287	430.188236	8.015206
5.811139	428.420113	8.020224
5.819700	429.854693	8.025242
5.339010	424.136059	8.030259
5.947981	423.330642	8.035277
5.399341	427.042629	8.040294
5.749710	427.287577	8.045312
5.618440	427.623767	8.050330
5.677812	429.511128	8.055347
5.955473	424.307984	8.060365
5.517017	431.701272	8.065382
5.367994	418.969043	8.070400
5.862574	430.381756	8.075418
5.811273	438.979851	8.080435
5.674607	440.266774	8.085453
5.740045	456.985327	8.090470
5.804955	448.438830	8.095488
5.759889	449.916528	8.100506
6.056859	455.528348	8.105523
5.710882	444.878215	8.110541
5.339244	447.890293	8.115558
5.639876	444.677994	8.120576
5.906297	449.754962	8.125594
5.536855	461.855332	8.130611
5.670515	452.338706	8.135629
5.618564	450.466050	8.140646
5.284467	454.791361	8.145664
5.810524	440.700502	8.150682
5.618117	455.673285	8.155699
5.801969	442.709005	8.160717
5.412545	446.197236	8.165734
5.934284	461.714532	8.170752
6.252347	461.945607	8.175770
6.159273	462.073844	8.180787
6.026859	450.787492	8.185805
5.869207	463.870839	8.190822
5.882865	451.046827	8.195840
5.752918	443.600671	8.200858
5.719543	454.010534	8.205875
6.002009	445.401550	8.210893
5.973258	448.703885	8.215910
5.603278	441.976986	8.220928
5.817389	453.452592	8.225946
5.956163	473.296511	8.230963
6.302980	470.588206	8.235981
5.794706	463.756736	8.240998
6.009782	477.794698	8.246016
5.998597	463.510288	8.251034
5.552126	467.461894	8.256051
5.855259	474.442362	8.261069
6.093725	479.791960	8.266086
5.935283	479.690599	8.271104
6.232794	477.371869	8.276122
6.098457	481.059979	8.281139
6.451850	471.833959	8.286157
5.986429	461.682209	8.291174
5.916645	450.966707	8.296192
6.069174	449.292384	8.301210
5.794491	450.130722	8.306227
5.764767	452.167744	8.311245
5.743565	462.840790	8.316262
6.058971	481.653505	8.321280
6.265682	475.830307	8.326298
6.492059	481.604674	8.331315
5.993966	462.968995	8.336333
6.068127	459.675413	8.341350
5.876926	455.328355	8.346368
6.268785	459.262216	8.351386
6.075772	463.890469	8.356403
6.247536	446.642536	8.361421
6.075845	452.709635	8.366438
5.721528	454.033817	8.371456
6.496881	455.152598	8.376474
6.113797	452.804809	8.381491
6.359320	449.392863	8.386509
6.227401	446.317763	8.391526
6.017597	447.294258	8.396544
6.290857	444.685844	8.401562
6.020480	459.595109	8.406579
6.224995	448.748268	8.411597
6.075154	437.221661	8.416614
5.952745	446.585130	8.421632
6.123900	441.042067	8.426650
5.900875	454.763649	8.431667
5.986738	446.040303	8.436685
6.348526	451.910208	8.441702
5.894967	449.706004	8.446720
6.429990	458.130191	8.451738
5.877583	459.529592	8.456755
5.940798	468.283326	8.461773
6.467209	469.535786	8.466790
6.444576	471.300302	8.471808
6.180349	471.341747	8.476826
6.180205	468.574198	8.481843
6.478028	469.269188	8.486861
6.635124	451.827889	8.491878
6.436329	450.470541	8.496896
6.215511	443.515145	8.501914
5.807873	450.474427	8.506931
6.436242	445.970557	8.511949
6.409727	453.144677	8.516966
6.178150	458.930830	8.521984
6.352683	444.065076	8.527002
6.469803	444.087796	8.532019
6.140067	448.248323	8.537037
6.316142	449.984858	8.542054
5.861453	452.179982	8.547072
5.949307	445.895739	8.552090
6.236209	455.592708	8.557107
6.241438	468.827262	8.562125
6.429929	464.562721	8.567143
6.214940	478.475565	8.572160
6.738116	463.517299	8.577178
6.128146	456.992097	8.582195
6.207913	453.186403	8.587213
6.027131	458.175653	8.592231
6.191534	467.633049	8.597248
6.412918	472.480396	8.602266
6.463508	471.390083	8.607283
6.503044	478.497060	8.612301
6.344420	469.770984	8.617319
6.227188	476.911990	8.622336
6.556613	466.405327	8.627354
6.565837	480.851083	8.632371
5.902176	475.356759	8.637389
6.243626	473.753818	8.642407
6.294237	479.681955	8.647424
6.528545	468.738917	8.652442
6.521324	479.482365	8.657459
6.437715	486.359333	8.662477
6.816420	480.651195	8.667495
6.486103	481.264724	8.672512
6.480083	475.910355	8.677530
6.495768	481.929170	8.682547
6.433295	463.010645	8.687565
6.961455	468.043452	8.692583
6.193231	458.961619	8.697600
6.381115	454.842341	8.702618
6.163101	458.325808	8.707635
5.995158	469.094432	8.712653
6.544493	479.283623	8.717671
6.521443	488.729375	8.722688
6.418201	481.799724	8.727706
6.410235	484.404536	8.732723
6.434336	475.943315	8.737741
6.544028	469.210677	8.742759
6.523713	477.680860	8.747776
6.726463	471.861440	8.752794
6.719787	469.104381	8.757811
6.592539	471.238736	8.762829
6.367957	473.094853	8.767847
6.267817	476.865966	8.772864
6.729026	480.984624	8.777882
6.612022	480.393936	8.782899
6.749570	478.721958	8.787917
6.440296	474.270320	8.792935
6.308806	479.112998	8.797952
6.598401	478.076755	8.802970
6.620785	480.326520	8.807987
6.252142	474.991098	8.813005
6.685091	467.365219	8.818023
6.660113	478.098825	8.823040
6.597647	474.144999	8.828058
6.548659	480.470591	8.833075
6.218366	478.682568	8.838093
6.412042	469.184931	8.843111
6.422227	483.422257	8.848128
6.193445	477.840860	8.853146
6.962984	484.599934	8.858163
6.706362	482.055603	8.863181
6.636901	469.194109	8.868199
6.207670	485.740887	8.873216
6.412747	478.264315	8.878234
6.636818	484.799587	8.883251
6.728797	490.595015	8.888269
6.641489	482.185960	8.893287
6.764548	502.215408	8.898304
6.506074	494.603178	8.903322
6.731224	507.541373	8.908339
7.020977	503.835309	8.913357
6.776503	497.966033	8.918375
6.695029	487.302833	8.923392
6.596677	479.794907	8.928410
6.600286	483.429846	8.933427
6.334332	495.485622	8.938445
6.793974	507.232060	8.943463
6.460641	504.033875	8.948480
6.576543	515.480728	8.953498
6.988304	506.362310	8.958515
6.685372	509.770730	8.963533
6.850827	510.063586	8.968551
6.712771	509.419392	8.973568
6.835447	510.529988	8.978586
6.663262	509.878518	8.983603
6.527702	516.867778	8.988621
6.969449	512.191162	8.993639
6.775746	521.193458	8.998656
6.790148	506.879758	9.003674
7.124647	508.910212	9.008691
6.712093	512.215888	9.013709
7.143712	506.824498	9.018727
6.968166	506.047323	9.023744
6.945331	513.138840	9.028762
7.047848	509.626213	9.033779
6.622601	514.994606	9.038797
7.158062	512.275674	9.043815
6.703321	522.275073	9.048832
7.142420	510.053387	9.053850
7.232119	503.932935	9.058867
6.723291	502.267556	9.063885
7.207366	480.129685	9.068903
6.830389	482.044395	9.073920
6.511390	485.701479	9.078938
6.971025	494.680290	9.083955
6.789678	505.078653	9.088973
7.168385	504.290376	9.093991
6.656283	508.318545	9.099008
6.668490	505.672131	9.104026
6.811728	504.390575	9.109043
6.723436	510.359420	9.114061
6.938302	500.426105	9.119079
6.968765	509.200769	9.124096
7.096957	503.131091	9.129114
6.880161	498.829057	9.134131
6.547407	507.954118	9.139149
6.826381	503.549160	9.144167
6.589422	496.346965	9.149184
6.694857	507.328397	9.154202
7.117566	506.274452	9.159219
6.731771	514.912369	9.164237
7.057866	507.855477	9.169255
6.566434	506.925826	9.174272
6.802560	526.587293	9.179290
7.249573	526.570949	9.184307
7.010164	539.462035	9.189325
7.325780	538.598435	9.194343
7.145827	538.503600	9.199360
6.997717	536.141075	9.204378
7.287954	530.396290	9.209395
7.129458	528.903235	9.214413
6.957354	511.185256	9.219431
6.888538	519.716706	9.224448
6.985467	531.447407	9.229466
7.208193	531.687109	9.234483
6.794888	533.500219	9.239501
7.104808	532.044224	9.244519
7.059834	529.700254	9.249536
7.113965	530.300885	9.254554
7.193977	530.285238	9.259571
7.028578	546.020722	9.264589
7.361381	536.892569	9.269607
7.375850	529.934988	9.274624
7.088600	528.512599	9.279642
7.222431	532.136612	9.284659
6.792474	544.783003	9.289677
6.824212	539.454257	9.294695
7.043513	537.340276	9.299712
6.858745	544.308855	9.304730
7.262531	533.165655	9.309747
6.939165	529.505159	9.314765
6.716128	531.906992	9.319783
7.313571	536.190509	9.324800
7.285573	537.129055	9.329818
7.219841	525.797494	9.334835
7.003109	540.411244	9.339853
7.248490	532.363448	9.344871
7.308869	529.883050	9.349888
7.033978	535.628677	9.354906
7.340842	541.999520	9.359923
7.267141	551.099793	9.364941
7.178642	545.070364	9.369959
7.498986	547.592187	9.374976
7.260100	554.941633	9.379994
7.470640	536.327391	9.385011
7.086279	545.731955	9.390029
7.395074	537.112490	9.395047
7.384316	539.736683	9.400064
7.197342	545.979776	9.405082
7.687885	545.360167	9.410099
7.646431	544.536734	9.415117
7.651670	538.278026	9.420135
7.502310	531.993050	9.425152
7.593964	541.648075	9.430170
7.621683	534.511692	9.435187
7.599486	534.335335	9.440205
7.380336	528.320070	9.445223
7.707384	531.557205	9.450240
7.461127	535.458521	9.455258
7.645315	526.748132	9.460275
7.679411	542.597522	9.465293
7.428420	533.283132	9.470311
7.387829	533.513598	9.475328
7.220465	538.627000	9.480346
7.450292	533.226193	9.485363
7.379728	539.261697	9.490381
7.629777	527.012816	9.495399
7.396687	532.613038	9.500416
7.750697	534.571010	9.505434
7.626250	523.400128	9.510451
7.160258	519.948172	9.515469
7.342366	529.308153	9.520487
7.775866	537.918698	9.525504
7.716083	533.304878	9.530522
7.517847	515.635170	9.535539
6.967611	516.324183	9.540557
7.331318	525.422181	9.545575
7.387867	529.531670	9.550592
6.990120	527.833105	9.555610
7.379823	538.864690	9.560627
7.085927	539.179026	9.565645
7.600564	531.887458	9.570663
7.568689	532.662511	9.575680
7.044348	531.848467	9.580698
7.647368	531.400582	9.585715
7.512997	540.718637	9.590733
7.421376	531.303538	9.595751
7.426504	538.321256	9.600768
7.506578	557.013134	9.605786
7.709385	557.502109	9.610803
7.346072	556.053766	9.615821
7.576749	559.438549	9.620839
7.747311	557.650938	9.625856
7.685131	559.544734	9.630874
7.848855	562.873737	9.635891
7.850174	568.733887	9.640909
7.426233	544.522838	9.645927
7.322097	551.150583	9.650944
7.347406	559.534762	9.655962
7.561729	563.098832	9.660979
7.372470	565.353366	9.665997
7.553280	567.464711	9.671015
7.664670	564.184212	9.676032
7.550482	570.157134	9.681050
7.743002	556.124755	9.686067
7.476550	558.473434	9.691085
7.675373	556.659304	9.696103
7.688590	558.411900	9.701120
7.781750	566.125890	9.706138
7.973183	555.337839	9.711155
7.703474	563.985993	9.716173
7.680293	559.997591	9.721191
7.848630	553.672297	9.726208
7.870453	567.532327	9.731226
7.871563	561.611928	9.736243
7.547601	557.216218	9.741261
7.360106	555.513111	9.746279
7.634733	560.661408	9.751296
7.713965	554.501553	9.756314
7.947247	550.110054	9.761331
7.726882	551.659407	9.766349
7.818855	555.968478	9.771367
7.978658	553.444097	9.776384
7.815940	556.114193	9.781402
7.964756	550.738697	9.786419
8.020419	556.195854	9.791437
8.031445	554.840337	9.796455
8.278766	552.116052	9.801472
7.658331	558.379728	9.806490
7.947382	552.657213	9.811507
8.040312	550.130687	9.816525
7.879375	554.375243	9.821543
8.153298	548.093368	9.826560
8.264806	553.993053	9.831578
8.219724	553.788724	9.836595
7.991099	557.520025	9.841613
7.916496	560.719111	9.846631
8.094509	556.443567	9.851648
8.197085	554.098565	9.856666
8.327329	552.273091	9.861683
8.088605	550.950393	9.866701
7.725059	554.674431	9.871719
7.760370	546.265069	9.876736
7.734107	556.787486	9.881754
7.866722	556.637366	9.886771
7.634243	561.656835	9.891789
7.477415	556.398654	9.896807
7.446273	558.274964	9.901824
7.497226	565.231864	9.906842
8.086305	579.186061	9.911859
8.073285	577.774349	9.916877
8.280988	584.094472	9.921895
8.307626	585.327417	9.926912
8.107149	577.059125	9.931930
7.796031	559.814158	9.936947
8.400396	562.670178	9.941965
7.900536	567.245550	9.946983
8.233136	559.597486	9.952000
8.130437	571.908600	9.957018
8.544428	559.621387	9.962035
8.364412	553.445348	9.967053
8.243410	560.419721	9.972071
8.375443	550.736040	9.977088
8.244261	561.379040	9.982106
8.130860	554.649767	9.987123
8.608403	552.003019	9.992141
8.111874	556.764058	9.997159
8.051605	564.464217	10.002176
8.051511	562.880068	10.007194
8.255417	562.027659	10.012211
8.195951	552.074182	10.017229
8.218907	559.385759	10.022247
8.340076	555.166459	10.027264
8.018111	555.762902	10.032282
8.008858	551.952200	10.037299
8.279002	548.735192	10.042317
8.433359	553.678270	10.047335
8.329115	547.253676	10.052352
8.034719	555.413391	10.057370
8.123839	554.301257	10.062387
8.020667	552.152594	10.067405
7.969521	549.096378	10.072423
8.070106	553.088521	10.077440
8.132759	556.761560	10.082458
8.192654	555.038626	10.087475
8.501892	549.814719	10.092493
8.268596	556.039827	10.097511
8.481313	555.757237	10.102528
8.531888	543.568000	10.107546
8.173352	552.037563	10.112563
8.126581	550.290316	10.117581
8.117603	559.412010	10.122599
8.604122	558.928730	10.127616
8.518138	558.140676	10.132634
8.229302	563.951612	10.137651
8.220551	555.927845	10.142669
8.209018	556.036995	10.147687
8.245484	574.205549	10.152704
8.472519	581.024414	10.157722
8.469319	578.588685	10.162739
8.566723	577.601484	10.167757
8.655772	581.554415	10.172775
8.624345	567.951589	10.177792
7.919406	564.322469	10.182810
8.355412	569.205643	10.187827
8.646229	574.291447	10.192845
8.748282	594.393717	10.197863
8.774899	573.198407	10.202880
8.579681	555.695444	10.207898
8.419050	551.835876	10.212915
8.796466	548.927107	10.217933
8.668390	556.783053	10.222951
8.363121	550.307905	10.227968
8.487875	557.963292	10.232986
8.019042	554.410789	10.238003
8.307054	562.110026	10.243021
8.669338	579.407030	10.248039
8.420369	579.528135	10.253056
8.443937	584.974551	10.258074
8.432607	582.536940	10.263091
8.738409	581.192039	10.268109
8.433061	582.363391	10.273127
8.625662	574.592089	10.278144
8.583597	585.473603	10.283162
8.740002	599.804876	10.288179
8.721042	578.386328	10.293197
9.098970	593.929427	10.298215
8.674219	576.254125	10.303232
8.395248	562.551234	10.308250
8.426042	563.603646	10.313267
8.611410	573.935124	10.318285
8.434083	586.560898	10.323303
8.950840	579.316315	10.328320
8.681280	590.659510	10.333338
8.441425	584.107829	10.338355
8.465552	582.229550	10.343373
8.253785	589.480087	10.348391
8.777605	582.660429	10.353408
8.630273	580.663849	10.358426
8.625842	589.251516	10.363443
8.610833	580.689076	10.368461
8.312191	579.363141	10.373479
8.468671	583.699982	10.378496
8.318478	578.652193	10.383514
8.592146	609.687678	10.388531
8.579635	599.767843	10.393549
8.891153	611.600674	10.398567
8.984352	606.612572	10.403584
8.973129	609.309432	10.408602
8.980558	601.668117	10.413619
9.119069	593.580234	10.418637
9.124726	580.492295	10.423655
9.042053	578.431935	10.428672
8.807192	576.871946	10.433690
9.014404	585.031976	10.438707
8.821069	573.177580	10.443725
8.872170	579.626380	10.448743
8.878431	577.100806	10.453760
8.998053	578.328649	10.458778
8.879215	577.552054	10.463795
8.755386	586.114246	10.468813
8.497827	584.583058	10.473831
8.486571	583.496117	10.478848
8.819132	589.834549	10.483866
8.615083	606.043200	10.488883
8.855729	602.761376	10.493901
8.845495	608.187849	10.498919
8.725340	611.756999	10.503936
8.827430	610.813242	10.508954
8.872658	614.028277	10.513971
8.980460	608.507711	10.518989
9.078069	609.464450	10.524007
8.893898	604.320992	10.529024
9.381410	607.633985	10.534042
8.966494	606.237904	10.539059
8.981280	604.853391	10.544077
8.930406	608.957639	10.549095
8.823948	599.898279	10.554112
9.075987	605.716002	10.559130
8.945175	613.263133	10.564147
9.219101	605.908264	10.569165
9.404758	599.614955	10.574183
9.297850	617.133832	10.579200
8.900562	609.372889	10.584218
8.925372	611.265684	10.589235
8.977536	611.308050	10.594253
8.469756	606.041725	10.599271
8.811761	615.319894	10.604288
8.796210	614.047432	10.609306
9.086702	612.509268	10.614323
9.037612	616.468071	10.619341
9.204389	628.459291	10.624359
8.983320	634.625706	10.629376
9.656414	642.340382	10.634394
8.959521	630.100943	10.639411
9.038731	618.421566	10.644429
9.152741	632.371343	10.649447
9.224807	634.767978	10.654464
9.384224	640.508707	10.659482
9.150573	641.447922	10.664499
9.145119	635.818861	10.669517
9.162678	644.081217	10.674535
9.404373	645.334119	10.679552
9.397462	641.977467	10.684570
9.229472	641.918627	10.689587
9.438788	638.168334	10.694605
9.323315	637.507974	10.699623
9.420770	632.995725	10.704640
9.434166	619.196489	10.709658
8.994974	628.047954	10.714675
9.470827	626.430253	10.719693
9.333153	622.664903	10.724711
8.998957	624.607638	10.729728
9.516949	628.165168	10.734746
9.410615	638.971578	10.739763
9.387890	639.634748	10.744781
9.642604	642.457203	10.749799
9.326405	625.525393	10.754816
9.311826	617.174307	10.759834
9.016292	626.107404	10.764851
9.402793	622.367223	10.769869
9.483936	642.346591	10.774887
9.339737	644.568829	10.779904
9.556521	644.285599	10.784922
9.250522	642.263379	10.789939
9.311736	638.542602	10.794957
9.544228	641.939740	10.799975
9.366410	646.130158	10.804992
9.337166	633.511554	10.810010
9.152132	640.792636	10.815027
9.425702	641.854352	10.820045
9.390848	636.173092	10.825063
9.195932	633.044714	10.830080
9.288829	625.664553	10.835098
9.258735	639.141453	10.840115
8.978676	642.805091	10.845133
9.374330	638.306078	10.850151
9.377802	662.971390	10.855168
9.512388	654.603228	10.860186
9.595230	661.125979	10.865203
9.636028	665.711339	10.870221
9.691225	665.466050	10.875239
9.634700	660.327822	10.880256
9.745334	664.125910	10.885274
9.378593	668.027197	10.890291
9.617117	656.793049	10.895309
9.936875	665.844356	10.900327
9.457934	664.098539	10.905344
9.902529	667.648642	10.910362
9.483812	675.136766	10.915379
9.571240	666.069085	10.920397
9.810408	667.454928	10.925415
9.532529	660.123379	10.930432
9.822264	656.461469	10.935450
9.764792	663.063010	10.940467
9.800288	670.975428	10.945485
9.943597	660.996431	10.950503
9.618093	667.381192	10.955520
9.717661	658.642972	10.960538
9.355605	675.002675	10.965555
9.551540	666.129431	10.970573
9.894176	667.729438	10.975591
9.767282	672.577760	10.980608
9.617161	666.955577	10.985626
9.488049	672.388072	10.990643
10.033572	671.172862	10.995661
9.779804	660.558645	11.000679
9.501178	666.705687	11.005696
9.472871	659.915704	11.010714
9.404670	670.855015	11.015731
9.484539	667.487917	11.020749
9.809378	676.648886	11.025767
9.961224	697.532424	11.030784
10.393616	689.751904	11.035802
10.269610	684.971382	11.040819
10.135130	681.237077	11.045837
10.119862	672.122367	11.050855
9.884551	663.755351	11.055872
10.027206	661.931076	11.060890
9.933386	668.254291	11.065907
10.090146	665.613606	11.070925
10.423326	664.087684	11.075943
10.288956	667.621203	11.080960
10.281251	662.642583	11.085978
10.068412	663.900432	11.090995
10.306550	661.998081	11.096013
9.993209	664.171082	11.101031
9.956840	662.163418	11.106048
10.163453	657.185935	11.111066
9.856434	671.753977	11.116083
9.936859	662.996664	11.121101
10.041799	672.403525	11.126119
9.784506	670.979586	11.131136
9.876198	667.935684	11.136154
9.742261	667.609576	11.141171
9.781375	656.943160	11.146189
10.125995	660.998077	11.151207
10.103952	661.582245	11.156224
10.146404	647.664826	11.161242
10.135561	663.297301	11.166259
9.935593	666.206779	11.171277
9.962956	657.214785	11.176295
10.264089	658.578296	11.181312
10.287838	664.305575	11.186330
10.424381	667.859763	11.191347
10.010931	665.238992	11.196365
10.188159	659.969465	11.201383
10.077849	660.324466	11.206400
10.017507	663.890566	11.211418
10.127156	660.241092	11.216435
9.707776	667.129713	11.221453
10.216893	668.750972	11.226471
10.486063	679.044135	11.231488
10.083721	674.752196	11.236506
10.326477	669.178909	11.241523
10.311067	681.962417	11.246541
10.539515	667.769686	11.251559
10.329311	671.674850	11.256576
10.123156	664.486696	11.261594
10.215945	668.022492	11.266611
10.117359	671.679793	11.271629
10.556320	677.512434	11.276647
10.216785	690.128982	11.281664
10.042135	684.987164	11.286682
10.229764	684.806332	11.291699
10.220049	687.484032	11.296717
10.408703	683.759059	11.301735
10.397061	693.499779	11.306752
10.526853	693.864498	11.311770
10.780255	696.958567	11.316787
10.458684	697.400318	11.321805
10.388376	689.868976	11.326823
10.441122	691.315589	11.331840
10.400621	690.081744	11.336858
10.584348	690.217105	11.341875
10.444199	693.754690	11.346893
10.281052	680.585829	11.351911
10.605930	685.177177	11.356928
10.343899	685.095202	11.361946
10.683715	685.704726	11.366963
10.406407	700.340720	11.371981
10.661913	689.170163	11.376999
10.612269	689.957474	11.382016
10.578412	695.337181	11.387034
10.733006	695.959948	11.392051
10.665702	688.412356	11.397069
10.826592	686.929206	11.402087
10.479409	691.086210	11.407104
10.549260	699.624422	11.412122
10.396409	688.334810	11.417139
10.396337	684.992857	11.422157
10.600445	693.800366	11.427175
10.741788	688.397598	11.432192
10.722256	682.461458	11.437210
10.643284	682.199321	11.442227
10.711048	682.927210	11.447245
10.701433	678.128767	11.452263
10.889181	687.771971	11.457280
10.853160	690.630518	11.462298
10.608243	682.429102	11.467315
10.561222	689.098442	11.472333
10.610654	686.045380	11.477351
10.341656	685.771991	11.482368
11.044684	684.560505	11.487386
10.979150	687.597246	11.492403
10.200934	685.626918	11.497421
10.568220	678.803348	11.502439
10.599105	686.523991	11.507456
10.649501	680.258158	11.512474
10.939773	693.716462	11.517491
10.490434	687.759299	11.522509
10.910119	688.274258	11.527527
10.526406	691.020025	11.532544
10.638830	690.383915	11.537562
10.690322	692.625991	11.542579
11.092566	704.700290	11.547597
11.100109	691.264835	11.552615
11.140836	695.992226	11.557632
10.739787	697.670887	11.562650
10.722193	689.998741	11.567667
10.602152	692.482288	11.572685
10.894140	704.431850	11.577703
10.969785	716.150229	11.582720
11.066752	717.965458	11.587738
11.106438	710.435807	11.592755
10.808405	713.663617	11.597773
10.760287	706.905122	11.602791
11.067009	712.714313	11.607808
10.999860	718.765122	11.612826
10.920247	717.644701	11.617843
11.377973	718.052714	11.622861
11.165533	712.089985	11.627879
10.945251	713.680364	11.632896
10.864792	724.309201	11.637914
11.504826	714.482722	11.642931
11.048133	711.247022	11.647949
11.062909	703.891692	11.652967
11.060211	707.085850	11.657984
11.275575	710.716059	11.663002
10.950115	705.667293	11.668019
11.222698	717.695644	11.673037
11.272210	719.619295	11.678055
11.135437	711.909008	11.683072
10.878117	718.238922	11.688090
11.233718	702.262138	11.693107
11.348512	719.355056	11.698125
11.408828	711.225723	11.703143
11.124066	701.178074	11.708160
11.179946	710.267592	11.713178
11.308995	709.335386	11.718195
11.210740	715.539391	11.723213
11.072414	716.712985	11.728231
11.137206	713.329306	11.733248
10.961655	714.909521	11.738266
11.102879	716.591583	11.743283
11.192178	727.323213	11.748301
11.183813	715.957296	11.753319
11.596032	716.429244	11.758336
10.905603	721.422680	11.763354
11.435255	714.936576	11.768371
11.224936	719.283583	11.773389
11.200229	704.865398	11.778407
11.442831	718.861368	11.783424
11.129531	716.455272	11.788442
11.206153	717.872900	11.793459
11.327024	718.532509	11.798477
11.529088	712.810948	11.803495
11.292010	718.247750	11.808512
11.017030	722.232502	11.813530
11.256174	717.893692	11.818547
11.090843	730.492441	11.823565
11.376608	736.058769	11.828583
11.195431	745.466316	11.833600
11.509783	750.141382	11.838618
11.714365	742.595349	11.843635
11.599851	749.429923	11.848653
11.678296	743.778215	11.853671
11.558967	743.979995	11.858688
11.672296	751.804514	11.863706
11.504028	741.599733	11.868723
11.532648	747.001226	11.873741
11.479504	750.294814	11.878759
11.561916	749.761235	11.883776
11.534360	745.107598	11.888794
11.882143	746.908779	11.893811
11.543887	751.398916	11.898829
11.945958	753.762796	11.903847
11.641563	735.257430	11.908864
11.402333	736.222771	11.913882
11.438260	740.278735	11.918899
11.624292	743.509601	11.923917
11.614079	747.610666	11.928935
11.601217	747.379195	11.933952
11.402661	740.612701	11.938970
11.644907	743.339295	11.943987
11.439591	749.449632	11.949005
11.329543	740.718968	11.954023
11.452950	752.142707	11.959040
11.222332	757.070420	11.964058
11.723196	750.169089	11.969075
11.576635	762.461959	11.974093
11.799248	769.357329	11.979111
11.764438	765.086678	11.984128
12.012666	773.824197	11.989146
12.043473	772.071085	11.994163
11.900123	761.035561	11.999181
11.494775	771.737421	12.004199
11.831530	773.978993	12.009216
11.719790	778.903865	12.014234
12.083579	772.020847	12.019251
12.025749	768.634279	12.024269
11.940780	778.010990	12.029287
11.921571	769.502767	12.034304
11.982650	775.899581	12.039322
11.965253	769.757948	12.044339
11.908105	771.000878	12.049357
11.821028	773.037455	12.054375
11.939242	761.250886	12.059392
12.153129	771.047831	12.064410
12.229746	764.342356	12.069427
12.055190	764.145687	12.074445
11.976609	762.671649	12.079463
12.338011	756.281320	12.084480
11.684182	756.762508	12.089498
11.911312	746.066580	12.094515
11.784463	764.516539	12.099533
11.778379	769.134518	12.104551
12.302076	763.435132	12.109568
12.104351	772.766390	12.114586
12.093082	771.490090	12.119603
12.009957	770.972980	12.124621
11.662076	768.818450	12.129639
12.150801	767.577420	12.134656
12.124719	769.178402	12.139674
12.199885	766.446345	12.144691
12.074574	776.255413	12.149709
12.323878	757.590685	12.154727
12.259726	763.641040	12.159744
12.222129	769.008732	12.164762
12.262391	771.028513	12.169779
12.383860	771.135760	12.174797
12.103951	774.490129	12.179815
12.386714	761.882509	12.184832
12.042847	767.749471	12.189850
12.078307	766.317525	12.194867
12.143988	763.511214	12.199885
11.780539	767.882225	12.204903
11.964434	762.333911	12.209920
12.085449	770.838894	12.214938
11.965573	773.202504	12.219955
12.124221	788.189990	12.224973
12.139953	791.759975	12.229991
12.507620	793.813668	12.235008
12.548996	797.029339	12.240026
12.467748	788.477178	12.245043
12.658672	795.838275	12.250061
12.160122	800.126319	12.255079
12.650318	794.447952	12.260096
12.375588	794.721418	12.265114
12.397770	789.886405	12.270131
12.687079	793.075852	12.275149
12.712257	795.946918	12.280167
12.612875	791.134107	12.285184
12.079187	801.284888	12.290202
12.758384	795.958763	12.295219
12.762337	792.701367	12.300237
12.483576	801.035470	12.305255
12.938421	800.576082	12.310272
12.820756	782.252851	12.315290
12.462856	779.377204	12.320307
12.410012	771.369716	12.325325
12.319452	781.226991	12.330343
12.304129	788.058661	12.335360
12.241560	796.078019	12.340378
12.434294	797.676278	12.345395
12.699475	789.631577	12.350413
12.256224	797.170934	12.355431
12.674366	792.005634	12.360448
12.380409	795.636766	12.365466
12.254339	788.988285	12.370483
12.699828	795.684641	12.375501
12.528878	796.834949	12.380519
13.081995	795.643789	12.385536
12.856500	798.453145	12.390554
12.694585	798.652130	12.395571
12.754795	791.807203	12.400589
12.662828	790.354194	12.405607
12.723024	789.956641	12.410624
12.773090	795.481021	12.415642
13.048149	795.286490	12.420659
12.668902	789.091091	12.425677
12.630718	797.775666	12.430695
13.099965	801.470258	12.435712
12.941198	804.146082	12.440730
12.934260	787.787363	12.445747
12.924721	797.603550	12.450765
12.684046	802.097346	12.455783
13.005624	788.044564	12.460800
13.026026	797.471048	12.465818
12.750440	798.596725	12.470835
13.046156	802.671960	12.475853
12.849292	808.140358	12.480871
13.163376	801.157818	12.485888
13.420547	793.512005	12.490906
12.842863	789.357965	12.495923
12.813248	792.243928	12.500941
12.657551	806.116177	12.505959
13.030706	795.697145	12.510976
13.134533	814.609635	12.515994
13.201357	813.368433	12.521011
13.214137	804.867805	12.526029
13.106865	803.852699	12.531047
12.990756	796.754526	12.536064
13.172099	803.160908	12.541082
13.097542	809.048805	12.546099
13.206266	795.054615	12.551117
13.169758	800.172835	12.556135
13.424638	796.465864	12.561152
12.964272	794.575110	12.566170
12.849464	791.509893	12.571187
13.134045	807.796803	12.576205
13.467553	806.908297	12.581223
13.235891	806.430238	12.586240
13.269641	826.395147	12.591258
13.080374	818.809804	12.596275
13.384848	813.286763	12.601293
13.277061	816.724626	12.606311
13.459044	820.994412	12.611328
13.530573	816.763893	12.616346
13.065040	804.876252	12.621363
13.391253	809.161307	12.626381
13.143542	812.318132	12.631399
13.619386	811.167481	12.636416
13.483061	809.620435	12.641434
13.298774	806.626062	12.646451
13.355522	800.712645	12.651469
13.106464	823.041400	12.656487
13.173067	810.470770	12.661504
13.262225	821.701101	12.666522
13.277390	814.850599	12.671539
13.534225	812.156343	12.676557
13.401369	819.293621	12.681575
13.253036	814.797746	12.686592
13.013862	812.222231	12.691610
12.960374	821.553006	12.696627
13.398636	807.182123	12.701645
12.646631	826.601107	12.706663
13.314352	836.954993	12.711680
13.748351	839.673649	12.716698
13.748509	847.856773	12.721715
13.845519	844.237645	12.726733
13.723714	841.684762	12.731751
13.966196	844.584906	12.736768
13.582388	826.536862	12.741786
13.432850	827.876323	12.746803
13.616086	840.341639	12.751821
13.739424	844.415489	12.756839
13.992249	836.688287	12.761856
13.771254	829.426651	12.766874
13.630959	818.056094	12.771891
13.582604	811.985570	12.776909
13.571081	831.547318	12.781927
13.758955	834.522289	12.786944
13.829310	836.919220	12.791962
13.832601	835.413413	12.796979
13.866426	835.326106	12.801997
13.721342	835.033300	12.807015
13.813967	830.127277	12.812032
13.825403	829.450181	12.817050
13.849678	834.767173	12.822067
14.056335	823.932393	12.827085
13.596132	822.354039	12.832103
13.603686	823.021940	12.837120
13.833371	832.043262	12.842138
13.794741	836.054124	12.847155
13.846491	837.996372	12.852173
13.817696	844.808085	12.857191
13.786118	833.215354	12.862208
13.994035	842.757650	12.867226
14.011159	835.414522	12.872243
14.011292	829.522589	12.877261
14.024222	830.994387	12.882279
14.228155	837.163710	12.887296
14.285435	832.970134	12.892314
13.756707	831.478256	12.897331
14.145440	831.852901	12.902349
13.899457	841.822924	12.907367
13.964331	835.494808	12.912384
14.207303	834.633109	12.917402
14.150295	834.310723	12.922419
14.135986	837.402581	12.927437
13.925823	837.151529	12.932455
14.001785	841.175996	12.937472
14.079669	837.503061	12.942490
13.701499	843.703630	12.947507
14.226048	838.878255	12.952525
13.992017	832.436024	12.957543
14.014055	837.519835	12.962560
13.823633	836.950106	12.967578
14.054439	838.592897	12.972595
14.379391	844.333002	12.977613
14.296546	853.311783	12.982631
14.038366	840.810954	12.987648
14.227472	855.446581	12.992666
14.285392	856.819812	12.997683
14.637609	850.191046	13.002701
14.417672	843.165927	13.007719
14.097171	842.739656	13.012736
14.813567	845.849573	13.017754
14.309710	844.476875	13.022771
14.452876	847.629269	13.027789
14.142570	839.226583	13.032807
14.420131	841.307023	13.037824
14.560781	839.006512	13.042842
14.355960	841.768454	13.047859
14.647212	844.717762	13.052877
14.313261	833.525861	13.057895
14.460755	846.214535	13.062912
14.685612	842.849934	13.067930
14.235174	840.572607	13.072947
14.377063	839.004058	13.077965
14.527949	852.825152	13.082983
14.570853	856.409828	13.088000
14.202728	853.431628	13.093018
14.334326	860.890410	13.098035
14.712262	846.907649	13.103053
14.784625	847.215097	13.108071
14.602964	841.534683	13.113088
14.806561	854.369208	13.118106
14.503378	862.318996	13.123123
14.556808	852.985144	13.128141
14.721207	845.558975	13.133159
14.887100	856.332331	13.138176
15.295350	847.422576	13.143194
14.983301	851.062866	13.148211
14.312950	835.991488	13.153229
14.863537	847.575578	13.158247
14.542208	848.803099	13.163264
14.932640	844.926556	13.168282
14.752033	858.323060	13.173299
15.006557	856.190901	13.178317
14.826155	853.126482	13.183335
14.414612	853.522373	13.188352
15.115878	853.724972	13.193370
14.844456	854.221986	13.198387
14.929727	846.476850	13.203405
14.792465	847.656597	13.208423
14.351492	861.330587	13.213440
14.760117	852.524914	13.218458
15.174300	857.001328	13.223475
15.085555	860.016488	13.228493
15.076956	856.394969	13.233511
14.754752	860.443955	13.238528
14.945700	849.570596	13.243546
14.952445	861.271462	13.248563
15.068553	859.905769	13.253581
15.458708	859.579594	13.258599
14.902958	860.124313	13.263616
15.189348	855.036443	13.268634
14.645211	856.324122	13.273651
14.868053	861.698374	13.278669
14.904886	863.087533	13.283687
14.924385	855.488400	13.288704
14.758446	854.529821	13.293722
14.614018	859.769110	13.298739
14.801542	860.664437	13.303757
14.905758	870.241932	13.308775
14.841744	878.368852	13.313792
15.582034	865.367577	13.318810
15.320014	875.308573	13.323827
15.422093	874.393208	13.328845
15.378952	876.511276	13.333863
15.058005	888.531751	13.338880
15.207840	881.129940	13.343898
15.075455	879.190944	13.348915
15.161735	875.418854	13.353933
15.047672	871.289985	13.358951
15.061717	876.737982	13.363968
15.061584	877.157776	13.368986
15.187414	885.879813	13.374003
14.934269	885.774353	13.379021
14.962534	883.541939	13.384039
15.133301	897.407290	13.389056
15.393952	896.930989	13.394074
15.427243	909.684939	13.399091
15.618527	908.411606	13.404109
15.702951	905.785376	13.409127
15.456769	905.663045	13.414144
15.589842	902.896647	13.419162
15.552790	897.973054	13.424179
15.786115	893.082840	13.429197
15.924110	887.749965	13.434215
15.339366	890.423115	13.439232
15.385976	878.035453	13.444250
15.477534	884.039361	13.449267
15.544198	896.816475	13.454285
15.982844	899.237762	13.459303
15.482692	902.860196	13.464320
15.571546	899.078230	13.469338
15.694969	901.914985	13.474355
15.770724	899.504712	13.479373
15.662091	886.655367	13.484391
15.435372	907.314437	13.489408
15.854052	900.018821	13.494426
15.842714	902.516923	13.499443
15.913071	904.270068	13.504461
16.001198	884.607965	13.509479
15.549374	884.666179	13.514496
15.670986	879.569406	13.519514
15.640787	885.548209	13.524531
15.659686	897.767911	13.529549
16.128714	889.501874	13.534567
15.782943	900.661543	13.539584
16.328038	889.637995	13.544602
16.178799	890.803842	13.549619
15.838782	889.597977	13.554637
15.780255	871.341129	13.559655
15.646418	879.365379	13.564672
16.130987	875.972704	13.569690
15.963233	880.994744	13.574707
15.929208	873.012664	13.579725
15.725672	875.342059	13.584743
15.930658	898.240405	13.589760
16.192807	893.913728	13.594778
16.127922	894.151161	13.599795
15.925646	905.941612	13.604813
16.010765	898.073399	13.609831
15.769425	909.882596	13.614848
15.960014	902.938302	13.619866
16.127176	905.825010	13.624883
15.968686	908.371416	13.629901
16.217210	911.179105	13.634919
15.850327	907.635802	13.639936
16.213967	905.344527	13.644954
16.443354	904.910995	13.649971
15.754641	902.371186	13.654989
15.802779	900.195617	13.660007
15.779982	906.138553	13.665024
16.146429	901.442077	13.670042
16.046543	908.548979	13.675059
15.774239	922.578446	13.680077
16.474638	925.807651	13.685095
16.243838	933.013970	13.690112
16.540976	926.122401	13.695130
16.225850	924.783243	13.700147
16.281912	929.230578	13.705165
16.541615	930.868850	13.710183
16.115552	936.114417	13.715200
16.224630	922.700750	13.720218
16.169175	928.046041	13.725235
16.026372	928.750127	13.730253
16.240068	923.957656	13.735271
16.260738	924.929623	13.740288
16.711762	918.433675	13.745306
16.539449	928.508971	13.750323
16.210614	930.406716	13.755341
16.410583	918.184350	13.760359
16.414549	936.086961	13.765376
16.616875	946.330790	13.770394
16.801688	952.010835	13.775411
16.822885	939.731256	13.780429
17.114806	921.873892	13.785447
16.595713	926.565978	13.790464
16.599466	927.130335	13.795482
16.989611	922.764661	13.800499
16.747007	928.110872	13.805517
16.654277	915.770263	13.810535
16.504013	918.126030	13.815552
16.448842	921.618787	13.820570
16.804691	920.360696	13.825587
16.280489	920.932032	13.830605
16.664810	927.142552	13.835623
16.571407	939.045356	13.840640
16.833888	946.256446	13.845658
16.973467	945.887477	13.850675
17.106667	952.711719	13.855693
17.539028	945.025769	13.860711
16.835563	930.249839	13.865728
16.696528	922.776505	13.870746
16.865150	925.312687	13.875763
16.455103	931.054370	13.880781
16.796807	935.400146	13.885799
17.270423	942.789596	13.890816
17.005241	948.776834	13.895834
17.316680	942.176514	13.900851
16.625984	935.035766	13.905869
17.114924	942.378633	13.910887
17.265085	950.380509	13.915904
17.018963	938.578323	13.920922
17.286777	937.690636	13.925939
16.613156	932.140924	13.930957
16.981398	936.911739	13.935975
17.175402	948.179372	13.940992
17.142713	948.866206	13.946010
17.212235	949.079425	13.951027
16.725290	962.877461	13.956045
16.639876	953.666298	13.961063
16.850399	952.011245	13.966080
17.332997	948.284344	13.971098
17.167053	950.970782	13.976115
17.041875	957.513610	13.981133
17.149324	946.716392	13.986151
17.191874	954.861365	13.991168
17.142711	949.977525	13.996186
17.049664	942.762069	14.001203
17.062882	961.635262	14.006221
17.629207	966.154138	14.011239
17.858837	969.946271	14.016256
17.516866	959.803295	14.021274
17.296504	950.196704	14.026291
17.013501	955.445109	14.031309
17.216987	957.805417	14.036327
17.457658	975.680448	14.041344
17.550377	973.157052	14.046362
17.418185	969.116209	14.051379
17.455122	976.719263	14.056397
17.669779	962.089794	14.061415
17.569659	976.938098	14.066432
17.550077	971.099702	14.071450
17.686684	964.905470	14.076467
17.148750	971.109023	14.081485
17.419536	971.126603	14.086503
17.622968	971.883742	14.091520
17.582363	971.284223	14.096538
17.443323	966.171459	14.101555
17.307945	974.066602	14.106573
17.839536	969.943849	14.111591
17.441557	975.727836	14.116608
17.469237	972.097454	14.121626
17.720694	973.749645	14.126643
17.545790	974.452451	14.131661
17.569482	974.303614	14.136679
17.521347	993.470481	14.141696
17.673662	1008.077283	14.146714
17.678326	999.546275	14.151731
17.839738	1003.235492	14.156749
17.979298	994.131073	14.161767
17.963584	997.892223	14.166784
17.971124	996.448854	14.171802
18.131669	998.875857	14.176819
18.083660	1009.231530	14.181837
18.178287	994.974299	14.186855
18.110615	978.527089	14.191872
17.794182	985.361831	14.196890
18.210001	969.886624	14.201907
17.777061	982.458049	14.206925
17.946546	987.764959	14.211943
18.117495	991.642031	14.216960
18.019258	997.161307	14.221978
18.261209	994.930113	14.226995
18.105254	1001.389415	14.232013
18.315164	994.757645	14.237031
18.418191	988.313041	14.242048
17.949811	977.173671	14.247066
18.127493	974.431831	14.252083
18.109119	989.504028	14.257101
18.332273	991.267955	14.262119
18.528816	988.684107	14.267136
18.402863	979.441412	14.272154
18.305848	968.818230	14.277171
17.848101	976.006476	14.282189
17.857349	982.701824	14.287207
18.619548	993.533315	14.292224
18.150205	990.523612	14.297242
18.397890	996.512563	14.302259
18.647030	1006.228373	14.307277
18.613504	995.106068	14.312295
18.684175	994.520672	14.317312
18.290344	982.375520	14.322330
18.415075	975.536192	14.327347
18.131229	978.402056	14.332365
18.337286	982.472445	14.337383
18.397382	993.833673	14.342400
18.321738	988.193407	14.347418
18.766984	997.329365	14.352435
18.544389	1003.101662	14.357453
18.555674	990.530105	14.362471
18.472339	989.356600	14.367488
18.395216	999.085655	14.372506
18.906636	996.360951	14.377523
18.409903	997.625432	14.382541
18.391773	995.731640	14.387559
18.526964	994.725872	14.392576
18.542076	988.837852	14.397594
18.673539	991.862714	14.402611
18.546043	1001.754301	14.407629
18.227755	996.675925	14.412647
18.854003	987.075524	14.417664
18.847152	991.087753	14.422682
18.762607	991.905792	14.427699
18.604000	1004.525771	14.432717
18.753291	1013.840655	14.437735
19.055760	1018.766968	14.442752
19.112296	1024.407172	14.447770
19.074823	1007.270379	14.452787
18.925406	995.730720	14.457805
18.641379	993.392585	14.462823
19.146826	992.985226	14.467840
18.683158	999.811484	14.472858
18.806512	1003.645522	14.477875
19.336047	1014.128463	14.482893
19.311293	1017.992022	14.487911
19.208238	995.052395	14.492928
18.464525	992.492787	14.497946
18.622011	1003.608384	14.502963
19.040912	1011.934262	14.507981
18.983190	1025.021297	14.512999
19.298628	1019.202979	14.518016
19.039907	1017.185931	14.523034
19.009006	1013.012440	14.528051
19.101045	1012.707725	14.533069
18.905346	1023.752436	14.538087
19.631111	1013.082367	14.543104
19.462491	1011.057514	14.548122
19.209127	1011.166686	14.553139
19.429596	1021.511860	14.558157
19.040458	1011.104839	14.563175
19.153465	1011.879303	14.568192
19.383676	1013.654751	14.573210
19.552548	1012.485911	14.578227
19.299285	1013.677532	14.583245
19.565507	1019.404805	14.588263
19.644651	1015.570686	14.593280
19.460812	1009.956832	14.598298
19.129750	1018.008890	14.603315
19.247121	1021.184291	14.608333
19.183616	1021.440445	14.613351
19.622088	1012.456445	14.618368
19.454114	1021.123593	14.623386
19.625386	1012.159367	14.628403
19.935617	1012.691486	14.633421
19.557794	1022.455044	14.638439
19.614127	1010.526525	14.643456
19.069899	1019.460912	14.648474
18.922849	1011.963549	14.653491
19.425655	1023.258587	14.658509
19.348012	1035.099024	14.663527
19.782035	1038.436259	14.668544
19.677350	1040.371481	14.673562
19.663405	1039.736224	14.678579
19.526224	1037.539181	14.683597
19.598368	1045.136747	14.688615
19.935551	1037.134303	14.693632
19.794991	1036.985955	14.698650
19.559690	1039.702208	14.703667
19.711294	1040.754655	14.708685
19.446629	1045.488960	14.713703
19.848025	1046.240332	14.718720
19.614009	1031.191944	14.723738
19.671170	1036.440726	14.728755
19.397363	1051.325772	14.733773
19.520545	1070.914015	14.738791
20.107694	1064.832199	14.743808
19.960955	1062.702923	14.748826
20.267639	1070.970670	14.753843
19.955324	1072.130521	14.758861
19.887684	1074.451272	14.763879
20.471437	1068.527781	14.768896
20.326952	1061.462351	14.773914
20.446958	1064.290200	14.778931
20.046975	1067.865413	14.783949
20.015155	1078.584672	14.788967
20.296436	1066.608247	14.793984
20.301400	1067.320745	14.799002
20.406805	1058.048072	14.804019
20.359908	1057.402197	14.809037
20.295328	1067.940386	14.814055
20.399993	1056.294605	14.819072
20.392167	1059.044650	14.824090
20.121179	1056.306822	14.829107
20.395436	1057.308494	14.834125
20.242710	1060.731354	14.839143
20.568262	1050.098721	14.844160
20.242100	1056.480567	14.849178
20.163500	1053.968223	14.854195
20.408296	1056.325228	14.859213
20.917961	1066.751352	14.864231
20.656681	1051.227524	14.869248
20.331742	1050.669396	14.874266
20.551912	1057.120281	14.879283
20.854822	1062.239046	14.884301
20.530412	1046.283290	14.889319
20.486917	1031.558510	14.894336
20.782112	1030.918999	14.899354
20.362121	1037.056758	14.904371
20.475568	1033.315092	14.909389
20.576010	1045.310675	14.914407
20.486853	1050.001704	14.919424
20.603648	1048.979880	14.924442
20.533532	1052.613862	14.929459
20.630516	1057.828008	14.934477
20.743937	1065.693677	14.939495
20.752921	1063.716732	14.944512
20.677402	1067.026508	14.949530
20.589739	1062.524220	14.954547
21.092520	1055.900190	14.959565
20.775948	1061.078144	14.964583
20.391802	1055.662923	14.969600
20.554427	1061.639976	14.974618
20.162473	1061.783486	14.979635
20.649399	1071.888120	14.984653
20.566984	1081.927325	14.989671
20.747860	1073.659014	14.994688
20.672768	1087.244290	14.999706
20.681062	1090.285312	15.004723
21.253103	1077.187166	15.009741
21.105385	1081.508672	15.014759
21.077978	1081.260541	15.019776
20.998437	1084.482586	15.024794
21.024976	1091.266786	15.029811
21.440801	1084.568005	15.034829
21.060876	1087.401602	15.039847
20.858461	1080.414671	15.044864
21.148594	1087.119699	15.049882
20.879201	1089.320580	15.054899
20.941316	1090.226101	15.059917
20.966664	1107.096714	15.064935
21.467034	1110.862236	15.069952
21.651237	1103.432858	15.074970
21.624051	1107.236854	15.079987
22.208064	1096.311228	15.085005
21.697352	1089.776550	15.090023
21.666731	1075.198043	15.095040
21.633016	1069.374453	15.100058
21.731083	1074.351742	15.105075
21.630308	1068.892118	15.110093
21.414304	1076.881992	15.115111
21.437525	1072.968258	15.120128
21.545339	1079.209531	15.125146
21.267052	1081.648496	15.130163
21.610919	1069.485534	15.135181
21.317357	1076.152620	15.140199
21.693636	1063.583786	15.145216
21.760947	1065.867612	15.150234
21.431618	1077.296220	15.155251
21.608154	1072.572649	15.160269
21.978492	1085.157148	15.165287
21.980422	1074.815053	15.170304
21.438011	1076.894603	15.175322
21.341677	1082.454634	15.180339
21.508071	1081.324049	15.185357
21.509459	1073.778155	15.190375
21.539566	1076.209826	15.195392
21.535212	1077.794808	15.200410
21.781089	1085.267339	15.205427
22.009354	1087.305037	15.210445
22.064777	1105.445915	15.215463
21.868870	1087.153566	15.220480
21.881763	1098.973548	15.225498
22.060328	1105.601387	15.230515
22.317479	1087.960751	15.235533
21.930328	1091.546582	15.240551
21.927457	1084.171769	15.245568
21.940587	1079.038286	15.250586
21.955521	1100.259335	15.255603
22.050246	1092.872383	15.260621
22.139174	1098.791566	15.265639
21.845621	1099.017491	15.270656
22.378121	1104.229687	15.275674
21.897824	1109.414373	15.280691
21.850742	1107.212672	15.285709
21.599534	1109.637930	15.290727
21.826671	1099.803349	15.295744
21.886417	1105.234787	15.300762
21.774744	1114.079357	15.305779
21.979484	1113.943179	15.310797
22.037289	1133.529110	15.315815
22.398853	1128.991135	15.320832
22.657559	1123.222700	15.325850
22.482592	1130.890579	15.330867
22.288509	1132.489513	15.335885
22.566874	1128.491608	15.340903
22.824101	1125.039830	15.345920
22.511725	1127.168553	15.350938
22.349504	1133.313294	15.355955
22.456542	1118.208241	15.360973
22.533480	1119.644787	15.365991
22.565416	1122.268687	15.371008
22.548114	1117.648061	15.376026
22.205394	1126.964350	15.381043
22.263078	1114.047756	15.386061
22.535508	1115.712454	15.391079
22.283213	1118.598645	15.396096
22.539989	1107.913636	15.401114
22.381259	1124.412308	15.406131
23.147908	1136.224673	15.411149
22.796780	1131.962468	15.416167
22.641866	1123.708875	15.421184
22.915812	1123.628128	15.426202
22.589853	1122.104454	15.431219
22.836996	1126.193686	15.436237
23.056102	1140.985798	15.441255
23.082897	1144.475223	15.446272
22.881827	1123.879841	15.451290
22.638464	1123.454100	15.456307
23.104377	1134.291073	15.461325
23.176420	1142.093830	15.466343
23.053076	1123.774294	15.471360
23.045294	1130.289324	15.476378
22.503686	1126.902745	15.481395
22.938682	1145.429173	15.486413
23.202436	1147.543372	15.491431
23.125531	1154.264906	15.496448
23.546077	1146.479734	15.501466
23.269296	1151.465282	15.506483
23.087758	1142.098663	15.511501
23.222055	1152.943423	15.516519
23.247144	1140.372754	15.521536
23.340628	1146.168158	15.526554
23.292431	1147.908343	15.531571
23.068165	1151.231972	15.536589
23.552438	1146.542220	15.541607
23.254054	1138.446802	15.546624
23.433248	1153.024265	15.551642
23.219786	1151.861670	15.556659
23.480375	1148.961642	15.561677
23.290373	1149.032484	15.566695
23.354479	1146.384155	15.571712
23.693756	1131.425745	15.576730
23.325593	1143.684168	15.581747
23.090468	1150.534636	15.586765
23.225341	1144.820310	15.591783
23.454614	1145.699643	15.596800
23.416617	1143.304005	15.601818
23.329184	1151.179090	15.606835
23.599358	1156.075786	15.611853
23.510324	1145.110412	15.616871
23.652994	1152.479217	15.621888
23.762336	1146.036722	15.626906
23.683708	1148.286619	15.631923
23.640802	1144.793496	15.636941
24.087867	1151.600197	15.641959
23.613106	1146.347473	15.646976
23.781022	1150.521709	15.651994
23.693433	1150.791106	15.657011
23.956971	1170.243854	15.662029
24.126258	1163.331200	15.667047
23.549947	1163.001807	15.672064
24.108808	1162.797522	15.677082
24.093680	1168.808773	15.682099
23.795728	1178.682982	15.687117
24.600459	1174.908719	15.692135
23.931419	1161.856636	15.697152
23.875595	1145.035020	15.702170
23.866767	1154.497831	15.707187
24.137908	1167.950024	15.712205
24.363177	1171.701856	15.717223
24.464422	1175.034451	15.722240
24.526969	1163.521435	15.727258
24.332044	1154.601890	15.732275
23.964410	1145.040359	15.737293
24.124515	1132.735727	15.742311
23.961084	1138.943779	15.747328
24.264350	1150.850847	15.752346
24.651429	1161.851672	15.757363
24.244909	1160.293279	15.762381
24.500824	1162.891560	15.767399
24.164856	1164.260255	15.772416
24.420951	1163.503787	15.777434
24.386320	1171.926047	15.782451
24.219546	1174.760976	15.787469
24.664386	1168.256440	15.792487
24.044326	1179.232031	15.797504
24.272677	1163.552493	15.802522
24.359255	1176.743266	15.807539
24.528524	1171.578982	15.812557
24.317588	1168.143741	15.817575
24.157810	1170.254871	15.822592
24.314576	1169.551836	15.827610
24.365985	1177.746017	15.832627
24.562779	1192.008319	15.837645
24.728707	1190.530651	15.842663
24.632216	1193.193619	15.847680
24.536458	1187.540662	15.852698
24.499403	1199.526332	15.857715
24.324817	1192.090013	15.862733
24.835874	1187.768450	15.867751
24.940852	1194.335266	15.872768
24.790155	1194.977481	15.877786
25.174073	1196.892971	15.882803
25.001675	1191.712783	15.887821
25.080490	1193.035428	15.892839
25.171882	1194.671693	15.897856
25.144286	1189.879086	15.902874
25.259733	1197.551986	15.907891
24.953349	1193.039751	15.912909
25.318490	1191.631859	15.917927
25.137398	1189.716241	15.922944
25.212987	1182.508980	15.927962
25.206746	1190.863683	15.932979
25.144606	1192.025371	15.937997
25.239512	1193.695800	15.943015
25.537048	1196.521102	15.948032
25.289051	1191.658882	15.953050
25.418920	1178.405873	15.958067
25.153505	1185.908060	15.963085
25.507650	1187.231748	15.968103
25.646519	1189.580121	15.973120
25.344208	1181.201268	15.978138
25.442872	1184.344914	15.983155
24.727066	1189.699070	15.988173
25.407478	1179.891259	15.993191
25.262552	1186.541410	15.998208
25.364522	1180.718615	16.003226
25.410361	1188.711696	16.008243
25.193241	1177.737967	16.013261
25.755417	1177.334340	16.018279
25.494650	1184.529676	16.023296
25.515745	1179.517997	16.028314
25.628733	1176.912499	16.033331
25.135852	1184.778539	16.038349
25.499719	1199.402847	16.043367
25.448043	1201.036281	16.048384
25.521296	1198.074077	16.053402
25.577520	1202.417309	16.058419
25.551398	1215.007210	16.063437
25.604749	1201.128679	16.068455
25.527068	1206.190348	16.073472
25.452613	1206.299892	16.078490
25.525462	1219.767412	16.083507
25.647141	1227.603456	16.088525
25.644732	1223.801006	16.093543
25.786252	1226.196306	16.098560
25.932580	1226.040877	16.103578
26.064949	1223.410244	16.108595
26.297043	1219.725693	16.113613
26.196151	1218.775837	16.118631
25.878951	1223.265948	16.123648
26.310783	1223.523393	16.128666
26.238166	1217.387102	16.133683
25.952029	1228.023217	16.138701
26.128707	1227.089834	16.143719
26.189217	1223.719353	16.148736
26.669921	1215.479742	16.153754
26.569915	1221.103509	16.158771
26.139168	1227.328226	16.163789
26.702412	1219.656369	16.168807
26.172462	1230.602094	16.173824
26.133246	1220.155905	16.178842
26.429534	1223.341181	16.183859
26.128979	1229.425576	16.188877
26.195686	1218.580927	16.193895
26.152159	1227.029854	16.198912
26.517664	1242.663832	16.203930
26.648581	1239.941903	16.208947
26.292887	1260.851971	16.213965
26.670644	1243.208065	16.218983
26.832830	1249.431411	16.224000
26.966645	1253.756187	16.229018
26.792470	1249.986955	16.234035
26.481969	1240.006152	16.239053
27.009428	1231.569853	16.244071
26.771030	1233.188363	16.249088
26.875126	1225.897721	16.254106
26.902094	1222.194814	16.259123
26.594994	1224.887629	16.264141
26.942909	1223.267831	16.269159
26.488896	1235.359881	16.274176
26.438680	1236.213579	16.279194
26.522991	1240.669189	16.284211
26.634410	1254.045482	16.289229
26.738643	1246.265643	16.294247
26.684263	1255.448456	16.299264
27.179632	1254.906968	16.304282
27.060657	1243.251923	16.309299
26.770827	1246.074584	16.314317
26.900220	1258.387676	16.319335
27.148762	1262.470409	16.324352
26.887078	1267.428376	16.329370
27.134428	1272.612713	16.334387
27.148251	1278.505852	16.339405
27.444948	1271.459580	16.344423
27.567027	1272.718646	16.349440
27.344743	1274.637603	16.354458
27.604359	1262.995814	16.359475
27.261038	1272.425886	16.364493
27.057800	1259.367024	16.369511
27.313756	1270.666181	16.374528
27.292080	1272.010889	16.379546
27.361447	1265.691384	16.384563
27.291119	1273.810005	16.389581
27.292177	1266.712222	16.394599
27.189547	1273.516730	16.399616
27.348878	1271.326851	16.404634
27.655934	1272.026740	16.409651
27.568815	1269.424178	16.414669
27.750442	1277.216136	16.419687
27.826092	1281.875092	16.424704
27.968012	1281.120727	16.429722
28.009065	1268.938801	16.434739
27.728518	1266.890428	16.439757
27.479054	1261.958988	16.444775
27.968852	1262.718611	16.449792
27.588311	1265.902638	16.454810
27.669376	1272.785666	16.459827
27.498603	1288.964473	16.464845
27.897912	1296.062745	16.469863
28.045812	1292.978371	16.474880
27.795235	1285.992593	16.479898
28.131911	1285.883082	16.484915
27.948385	1288.827955	16.489933
28.231573	1292.750626	16.494951
28.322671	1286.203638	16.499968
28.204259	1281.980677	16.504986
28.574807	1287.107845	16.510003
28.312745	1296.670371	16.515021
28.385078	1294.266893	16.520039
28.358594	1284.251033	16.525056
28.241079	1290.436164	16.530074
28.274353	1282.468604	16.535091
28.224854	1278.676676	16.540109
28.216405	1288.237332	16.545127
28.533714	1285.770225	16.550144
28.593546	1290.176032	16.555162
28.353368	1284.006009	16.560179
28.087082	1286.607229	16.565197
27.948567	1285.994637	16.570215
28.464439	1281.265183	16.575232
28.197272	1288.411068	16.580250
28.369065	1283.770239	16.585267
28.145243	1290.903023	16.590285
28.230658	1277.316066	16.595303
28.304140	1283.742677	16.600320
28.366490	1299.591468	16.605338
28.173783	1303.563456	16.610355
28.510404	1314.906810	16.615373
28.179624	1320.866579	16.620391
28.853657	1313.568658	16.625408
28.886810	1315.687448	16.630426
29.075519	1319.378766	16.635443
29.049843	1321.017605	16.640461
28.482282	1314.072013	16.645479
28.894181	1306.909844	16.650496
28.731545	1313.875253	16.655514
28.741644	1323.578195	16.660531
29.031446	1339.530244	16.665549
29.028983	1343.538709	16.670567
29.455578	1347.650371	16.675584
29.148810	1342.181911	16.680602
29.136143	1316.090714	16.685619
29.348081	1333.247898	16.690637
29.131486	1328.279730	16.695655
29.165657	1327.292928	16.700672
29.284800	1328.647136	16.705690
29.384009	1320.217931	16.710707
29.643058	1319.988033	16.715725
29.070910	1316.435782	16.720743
29.126477	1318.670985	16.725760
29.212203	1332.714108	16.730778
29.321404	1327.628620	16.735795
29.673005	1329.132607	16.740813
29.462228	1334.357182	16.745831
29.479952	1327.528174	16.750848
29.214508	1337.432091	16.755866
29.418171	1337.965138	16.760883
29.796454	1327.412446	16.765901
29.514712	1328.819997	16.770919
29.184236	1322.184407	16.775936
29.550099	1331.762182	16.780954
29.528384	1331.257525	16.785971
29.473572	1330.171051	16.790989
29.620824	1327.317156	16.796007
29.486312	1334.533797	16.801024
29.700947	1350.365085	16.806042
29.994852	1349.978240	16.811059
30.063802	1352.416488	16.816077
29.773461	1353.683370	16.821095
30.152681	1339.119333	16.826112
30.046001	1351.024490	16.831130
30.495316	1356.357097	16.836147
30.351364	1337.081167	16.841165
29.998138	1330.569065	16.846183
30.192867	1323.718637	16.851200
29.686655	1324.621692	16.856218
30.165162	1326.358269	16.861235
30.441193	1340.321086	16.866253
30.165585	1334.166065	16.871271
30.423580	1325.345891	16.876288
29.681978	1333.030050	16.881306
30.161706	1341.955648	16.886323
30.219969	1346.932938	16.891341
30.197026	1361.725286	16.896359
30.798816	1350.610520	16.901376
30.534821	1357.825366	16.906394
30.668126	1351.833498	16.911411
30.721435	1347.457380	16.916429
30.284439	1342.403815	16.921447
30.571134	1342.314758	16.926464
30.476492	1353.473232	16.931482
30.091001	1357.772096	16.936499
30.548859	1345.805690	16.941517
30.513989	1350.636621	16.946535
30.773575	1345.909434	16.951552
30.412192	1346.294318	16.956570
30.457194	1343.336515	16.961587
30.561400	1344.175492	16.966605
30.587688	1353.819106	16.971623
30.778934	1346.659934	16.976640
30.408038	1358.792694	16.981658
30.740075	1358.980568	16.986675
30.853942	1377.737440	16.991693
30.610134	1385.457240	16.996711
30.754549	1381.429772	17.001728
30.736123	1380.552198	17.006746
30.772732	1376.617364	17.011763
30.893703	1372.820798	17.016781
30.507624	1383.643084	17.021799
30.955989	1386.170219	17.026816
30.953427	1395.300802	17.031834
31.133989	1395.812223	17.036851
31.260636	1392.649108	17.041869
31.019059	1398.260396	17.046887
31.292136	1399.940801	17.051904
31.438127	1405.175773	17.056922
31.418695	1399.889503	17.061939
31.487081	1400.030319	17.066957
31.103919	1402.451043	17.071975
31.460800	1403.032674	17.076992
31.406277	1405.862675	17.082010
31.291364	1396.993591	17.087027
31.272461	1393.433540	17.092045
31.301305	1398.393363	17.097063
31.651980	1396.192424	17.102080
31.283348	1392.450473	17.107098
31.262447	1417.499358	17.112115
31.410282	1410.482667	17.117133
31.465528	1425.348028	17.122151
31.883531	1419.046431	17.127168
31.986884	1416.243584	17.132186
31.661269	1414.644087	17.137203
31.736097	1416.027337	17.142221
31.549284	1426.395531	17.147239
31.919016	1414.332429	17.152256
32.232126	1416.852356	17.157274
32.267876	1416.774214	17.162291
32.079261	1415.980110	17.167309
31.907222	1418.844305	17.172327
32.011846	1415.425849	17.177344
32.245678	1417.267045	17.182362
32.040427	1411.006296	17.187379
31.924115	1409.642261	17.192397
32.067783	1424.446428	17.197415
32.197826	1415.134994	17.202432
32.637783	1415.649958	17.207450
32.144335	1415.197117	17.212467
32.749587	1408.298117	17.217485
32.278191	1420.885341	17.222503
32.533171	1415.316220	17.227520
32.684701	1414.825445	17.232538
32.404416	1416.734568	17.237555
32.624247	1412.761552	17.242573
32.381408	1415.116109	17.247591
32.267077	1410.646314	17.252608
32.542350	1413.503543	17.257626
32.460853	1409.284236	17.262643
32.574083	1407.915797	17.267661
32.467051	1418.381945	17.272679
32.461529	1408.605739	17.277696
32.754553	1417.481729	17.282714
32.968678	1420.215990	17.287731
32.732047	1410.150931	17.292749
32.628977	1417.829759	17.297767
32.994549	1433.568041	17.302784
32.996641	1432.961817	17.307802
33.028528	1441.894513	17.312819
33.037235	1422.493583	17.317837
32.743073	1427.971102	17.322855
32.801828	1430.467764	17.327872
33.022445	1434.343463	17.332890
32.909468	1429.946038	17.337907
33.409578	1423.379100	17.342925
33.180865	1434.931032	17.347943
32.844962	1430.148795	17.352960
33.371628	1433.818745	17.357978
32.800518	1438.869422	17.362995
33.454942	1432.082635	17.368013
33.151963	1444.492003	17.373031
33.223710	1444.547082	17.378048
33.078541	1437.544729	17.383066
33.061012	1440.438370	17.388083
33.362790	1439.728384	17.393101
33.344382	1445.449895	17.398119
33.554289	1448.058583	17.403136
33.603613	1461.498411	17.408154
33.367771	1461.626931	17.413171
33.782878	1462.622338	17.418189
33.754625	1459.568692	17.423207
33.600969	1456.484199	17.428224
34.005830	1458.497428	17.433242
33.903198	1461.874644	17.438259
34.132272	1456.543110	17.443277
33.733882	1448.744099	17.448295
33.862501	1442.282699	17.453312
33.752681	1440.346418	17.458330
33.711986	1454.898616	17.463347
34.052443	1447.460393	17.468365
34.085269	1458.153971	17.473383
34.125331	1454.805587	17.478400
34.061857	1463.551254	17.483418
33.994771	1458.117792	17.488435
34.285832	1458.296307	17.493453
33.864593	1463.235143	17.498471
33.909603	1460.690750	17.503488
34.114512	1451.894612	17.508506
33.912099	1466.920302	17.513523
34.229622	1454.840106	17.518541
34.247264	1459.517665	17.523559
34.409337	1456.563593	17.528576
34.442676	1454.459707	17.533594
34.109286	1458.557918	17.538611
34.261157	1454.175799	17.543629
34.356578	1466.383899	17.548647
34.314970	1468.637503	17.553664
34.334088	1475.713360	17.558682
34.396589	1482.277470	17.563699
34.452249	1480.690817	17.568717
34.486804	1477.867179	17.573735
34.556094	1486.689891	17.578752
34.656170	1481.883514	17.583770
34.912034	1486.110325	17.588787
35.033563	1481.202753	17.593805
35.158107	1476.686047	17.598823
35.165898	1483.943572	17.603840
34.934457	1487.252607	17.608858
34.584429	1481.390075	17.613875
35.390766	1475.349523	17.618893
35.245152	1475.867868	17.623911
34.948910	1477.366068	17.628928
34.861517	1479.585820	17.633946
35.080255	1473.097664	17.638963
35.517096	1459.954149	17.643981
35.110518	1477.514507	17.648999
35.064442	1490.202407	17.654016
35.048902	1478.628837	17.659034
34.763755	1479.339466	17.664051
34.795510	1477.194798	17.669069
35.168516	1475.075562	17.674087
35.118463	1482.875506	17.679104
35.083889	1487.327712	17.684122
35.655567	1504.362422	17.689139
35.748831	1491.563063	17.694157
35.588785	1478.355256	17.699175
35.138859	1495.073471	17.704192
35.314516	1504.974645	17.709210
35.878601	1508.304216	17.714227
36.071286	1502.984682	17.719245
35.707648	1499.939392	17.724263
35.601721	1518.039694	17.729280
35.671981	1500.096558	17.734298
35.795283	1505.982087	17.739315
35.527980	1492.191441	17.744333
35.673380	1496.258829	17.749351
35.781280	1507.054288	17.754368
36.028724	1502.013367	17.759386
35.825384	1497.699515	17.764403
35.887406	1496.446395	17.769421
35.966578	1498.775758	17.774439
35.832550	1504.802595	17.779456
36.025457	1492.404210	17.784474
35.975240	1503.956624	17.789491
35.718098	1497.880707	17.794509
35.764010	1510.440594	17.799527
35.663835	1525.384040	17.804544
36.156771	1520.550816	17.809562
35.889062	1526.832146	17.814579
36.254686	1521.719052	17.819597
36.171347	1529.741993	17.824615
36.213579	1534.251608	17.829632
36.710695	1540.110139	17.834650
36.583598	1543.617441	17.839667
36.722173	1552.132669	17.844685
37.072678	1556.928524	17.849703
36.711229	1546.718833	17.854720
36.942796	1530.628195	17.859738
36.531126	1527.117032	17.864755
36.402901	1516.185974	17.869773
36.163522	1527.020076	17.874791
36.462355	1537.773015	17.879808
36.768082	1534.954222	17.884826
36.650082	1543.594856	17.889843
36.674138	1534.804922	17.894861
36.691354	1543.544297	17.899879
36.745970	1548.115095	17.904896
36.838095	1539.093576	17.909914
36.673808	1544.639148	17.914931
36.652390	1560.233037	17.919949
37.349864	1564.968218	17.924967
37.160768	1577.110513	17.929984
37.230866	1566.555472	17.935002
37.230322	1572.933822	17.940019
37.070133	1576.701950	17.945037
37.528852	1573.748721	17.950055
37.487676	1574.279109	17.955072
37.732986	1561.525309	17.960090
37.672482	1565.826955	17.965107
37.234044	1555.708222	17.970125
37.462472	1554.457429	17.975143
37.259040	1565.522621	17.980160
37.677582	1556.882317	17.985178
37.939163	1564.238974	17.990195
37.680896	1575.603112	17.995213
37.433866	1564.280362	18.000231
37.573365	1570.308549	18.005248
37.709744	1561.387388	18.010266
37.769249	1566.452912	18.015283
37.468420	1561.920776	18.020301
37.929175	1562.814359	18.025319
38.114037	1575.071639	18.030336
38.050261	1565.156145	18.035354
37.691826	1564.754733	18.040371
37.726097	1561.858540	18.045389
37.761900	1556.541478	18.050407
37.258896	1563.402514	18.055424
38.056430	1575.630078	18.060442
37.943147	1585.538695	18.065459
38.200454	1584.106641	18.070477
38.093920	1583.511119	18.075495
38.106126	1581.726127	18.080512
38.127878	1579.469399	18.085530
38.195368	1588.898390	18.090547
38.661127	1584.924676	18.095565
38.536902	1582.469901	18.100583
38.060082	1588.326400	18.105600
38.257875	1589.062358	18.110618
38.329438	1587.350120	18.115635
38.452738	1594.955685	18.120653
38.741612	1603.804015	18.125671
38.740278	1614.544066	18.130688
38.964614	1609.068054	18.135706
38.836389	1604.767655	18.140723
38.846030	1610.895101	18.145741
39.000006	1594.179055	18.150759
38.524683	1584.195479	18.155776
38.492120	1603.887607	18.160794
39.067457	1605.063057	18.165811
39.128217	1605.694247	18.170829
39.196410	1604.941953	18.175847
38.854562	1619.945434	18.180864
39.045132	1619.934557	18.185882
39.206772	1614.856553	18.190899
38.939432	1609.261905	18.195917
39.265197	1602.545484	18.200935
38.998561	1610.953805	18.205952
39.002565	1601.602058	18.210970
38.886873	1606.695043	18.215987
39.293883	1616.418012	18.221005
39.063009	1612.588155	18.226023
38.500629	1619.193412	18.231040
39.151475	1629.231653	18.236058
39.522150	1631.578481	18.241075
39.753274	1629.222667	18.246093
39.887989	1632.408085	18.251111
39.576907	1638.528982	18.256128
39.690726	1632.353871	18.261146
39.644686	1627.844919	18.266163
39.769309	1625.101826	18.271181
39.672252	1639.369498	18.276199
39.481762	1635.246114	18.281216
39.299596	1632.882466	18.286234
39.603135	1636.587418	18.291251
39.525543	1628.192081	18.296269
39.524461	1644.420365	18.301287
39.745037	1652.673470	18.306304
39.989833	1650.583771	18.311322
40.072927	1652.350774	18.316339
39.711512	1660.897051	18.321357
40.387249	1649.843104	18.326375
39.996497	1662.054923	18.331392
40.564342	1656.821739	18.336410
40.419823	1653.644257	18.341427
40.016444	1654.512279	18.346445
40.129479	1648.192110	18.351463
40.220247	1652.160789	18.356480
40.169186	1649.988048	18.361498
40.383909	1653.041006	18.366515
40.647755	1680.914437	18.371533
40.370159	1676.994051	18.376551
40.633407	1678.455103	18.381568
40.720634	1678.804421	18.386586
41.103899	1676.737207	18.391603
40.863059	1666.937766	18.396621
41.010977	1665.336641	18.401639
40.835593	1659.465623	18.406656
40.909346	1660.864840	18.411674
41.062838	1651.540142	18.416691
40.882913	1656.463314	18.421709
41.116752	1657.884788	18.426727
41.263575	1651.196385	18.431744
41.271533	1636.289466	18.436762
41.356030	1636.320456	18.441779
40.886893	1641.778114	18.446797
41.170162	1636.160310	18.451815
41.057375	1641.647347	18.456832
41.316719	1640.429577	18.461850
41.565221	1658.543921	18.466867
41.184111	1652.752477	18.471885
41.354798	1653.770411	18.476903
41.315079	1662.944824	18.481920
41.681295	1659.021407	18.486938
41.802323	1657.478148	18.491955
41.494482	1662.247783	18.496973
41.768797	1654.633635	18.501991
41.739606	1660.088645	18.507008
41.099144	1657.822045	18.512026
41.568931	1657.152004	18.517043
41.433282	1666.625488	18.522061
41.562761	1658.453329	18.527079
41.735024	1660.600860	18.532096
41.870372	1659.099541	18.537114
41.821058	1654.502728	18.542131
41.477627	1673.091703	18.547149
41.701926	1668.764459	18.552167
41.744921	1671.538196	18.557184
41.887614	1682.956352	18.562202
42.170695	1681.782200	18.567219
41.883937	1694.040867	18.572237
41.943010	1687.132655	18.577255
41.760038	1697.292108	18.582272
41.923346	1689.310306	18.587290
42.075657	1691.767099	18.592307
41.891481	1693.418182	18.597325
42.155325	1698.827291	18.602343
42.395826	1711.113820	18.607360
41.756208	1708.869173	18.612378
42.504496	1711.753332	18.617395
42.232256	1719.802798	18.622413
42.484826	1717.582477	18.627431
42.191629	1710.398069	18.632448
42.193485	1709.836056	18.637466
42.958667	1723.028214	18.642483
42.757347	1734.566579	18.647501
42.549892	1736.114008	18.652519
42.588541	1743.085919	18.657536
42.815513	1734.058954	18.662554
43.308827	1735.783785	18.667571
43.067889	1740.514555	18.672589
42.955141	1739.714861	18.677607
43.107809	1732.040839	18.682624
42.884364	1737.529464	18.687642
42.725217	1725.722598	18.692659
42.819594	1737.672255	18.697677
43.260978	1733.670768	18.702695
43.389256	1745.454163	18.707712
43.177079	1754.945995	18.712730
43.162905	1754.553761	18.717747
43.348739	1768.729873	18.722765
43.363189	1765.880936	18.727783
43.696996	1756.793037	18.732800
43.604871	1764.404022	18.737818
43.511568	1769.875422	18.742835
43.364200	1765.328659	18.747853
43.383355	1769.122379	18.752871
43.753213	1761.562649	18.757888
43.670339	1767.363795	18.762906
43.358749	1764.430233	18.767923
43.344712	1769.542053	18.772941
43.483690	1773.837742	18.777959
44.148700	1784.905868	18.782976
43.997215	1791.588830	18.787994
44.043724	1780.914274	18.793011
44.059465	1782.761275	18.798029
44.059876	1781.662965	18.803047
44.177961	1785.153992	18.808064
44.238631	1775.051614	18.813082
44.105558	1776.802002	18.818099
44.134499	1779.218172	18.823117
44.251371	1782.778821	18.828135
44.568594	1768.763828	18.833152
44.271202	1781.308261	18.838170
44.368070	1770.941421	18.843187
44.257893	1772.274784	18.848205
44.143465	1784.680093	18.853223
44.736659	1791.697690	18.858240
44.353917	1803.498068	18.863258
44.489386	1795.763594	18.868275
44.372833	1805.997914	18.873293
45.104173	1800.205708	18.878311
45.019880	1799.426801	18.883328
44.763203	1801.600526	18.888346
45.159774	1792.843625	18.893363
44.973814	1789.710483	18.898381
45.127050	1798.239311	18.903399
45.135954	1797.493143	18.908416
45.039473	1799.259892	18.913434
45.178089	1798.502868	18.918451
45.031571	1798.033532	18.923469
44.965990	1808.632277	18.928487
44.982978	1798.139073	18.933504
44.978823	1794.617660	18.938522
45.074887	1788.640949	18.943539
45.299320	1793.257792	18.948557
45.174308	1798.790977	18.953575
45.427570	1805.681946	18.958592
45.276905	1823.780097	18.963610
45.769755	1810.605459	18.968627
45.656762	1822.922201	18.973645
45.469774	1820.130064	18.978663
45.456800	1816.266023	18.983680
45.036556	1827.513678	18.988698
45.185906	1818.988015	18.993715
45.645839	1824.773566	18.998733
45.688915	1844.507759	19.003751
46.077384	1846.823424	19.008768
45.778335	1853.258111	19.013786
45.933481	1848.338860	19.018803
45.683325	1850.950256	19.023821
45.877391	1848.025825	19.028839
45.820822	1853.014935	19.033856
46.017907	1849.616627	19.038874
46.136599	1843.333375	19.043891
46.065350	1850.499283	19.048909
46.109748	1860.099304	19.053927
46.265314	1868.466844	19.058944
46.230899	1873.237879	19.063962
46.624096	1871.664584	19.068979
46.887072	1871.544526	19.073997
46.245400	1878.301166	19.079015
46.788051	1871.052012	19.084032
46.513894	1875.860610	19.089050
46.714585	1862.040539	19.094067
46.763455	1871.046534	19.099085
47.013209	1874.254999	19.104103
46.603334	1864.971117	19.109120
46.347982	1870.269107	19.114138
46.632821	1856.388516	19.119155
47.009413	1867.691243	19.124173
46.712047	1879.105883	19.129191
46.804251	1882.777722	19.134208
47.100919	1887.834583	19.139226
46.950104	1885.254535	19.144243
47.235518	1882.211637	19.149261
47.354335	1884.241328	19.154279
47.458404	1885.588472	19.159296
47.311412	1886.277470	19.164314
47.337271	1882.871266	19.169331
47.297004	1882.864997	19.174349
47.294114	1881.735637	19.179367
47.369910	1876.058740	19.184384
47.258696	1885.670532	19.189402
47.639229	1892.304892	19.194419
47.708928	1904.384768	19.199437
47.882327	1906.626833	19.204455
48.279021	1913.261825	19.209472
47.909140	1907.244461	19.214490
47.775907	1898.822999	19.219507
48.085393	1909.710202	19.224525
47.631889	1904.419204	19.229543
48.025099	1898.755688	19.234560
47.612522	1904.504386	19.239578
47.699827	1904.916817	19.244595
48.053973	1894.765236	19.249613
48.198817	1905.100679	19.254631
48.128561	1900.860558	19.259648
48.326628	1905.778228	19.264666
48.229147	1901.835884	19.269683
48.356306	1901.951716	19.274701
48.228327	1910.202742	19.279719
48.597591	1911.981743	19.284736
48.569966	1922.650353	19.289754
48.424755	1939.681026	19.294771
48.564598	1934.764149	19.299789
48.400483	1932.239830	19.304807
48.660200	1932.435887	19.309824
48.329273	1934.984206	19.314842
48.882934	1929.270293	19.319859
48.788638	1927.732343	19.324877
48.544848	1936.869437	19.329895
48.893293	1927.204760	19.334912
48.476346	1934.412240	19.339930
48.682405	1945.606025	19.344947
48.684256	1954.471094	19.349965
48.628571	1954.694475	19.354983
48.941247	1952.568858	19.360000
49.172714	1954.473602	19.365018
49.124748	1957.021775	19.370035
49.253346	1953.833008	19.375053
49.161048	1980.620219	19.380071
49.553423	1980.700810	19.385088
49.337687	1983.385734	19.390106
49.661779	1978.550439	19.395123
49.836569	1977.585754	19.400141
49.269868	1975.433797	19.405159
49.821899	1975.981717	19.410176
49.722000	1976.230962	19.415194
49.984104	1975.082170	19.420211
49.752142	1981.537952	19.425229
49.490222	1976.204292	19.430247
50.121745	1972.308672	19.435264
49.748953	1980.241454	19.440282
49.785069	1971.948071	19.445299
50.180451	1973.508375	19.450317
50.277793	1987.670121	19.455335
50.309619	1978.537899	19.460352
50.353593	1976.788918	19.465370
50.576742	1985.912843	19.470387
50.221925	1978.870535	19.475405
50.236501	1989.684063	19.480423
50.611983	1997.442807	19.485440
50.917871	1997.770497	19.490458
50.465028	1990.500528	19.495475
50.585419	1983.178621	19.500493
50.668710	2003.181265	19.505511
50.685114	1993.215098	19.510528
51.039942	2001.614601	19.515546
50.680194	1999.294507	19.520563
50.752383	1995.054139	19.525581
50.687430	1997.115792	19.530599
50.854569	1990.477733	19.535616
50.687200	1988.250584	19.540634
50.575348	1993.355701	19.545651
50.926221	1983.551747	19.550669
50.496216	1999.314183	19.555687
50.843727	2009.075092	19.560704
50.968635	2018.833011	19.565722
51.254977	2020.154764	19.570739
51.123915	2023.224090	19.575757
51.343207	2021.659092	19.580775
51.549290	2018.470798	19.585792
51.834636	2023.497911	19.590810
51.438438	2029.004222	19.595827
51.815310	2019.647491	19.600845
51.434762	2020.824402	19.605863
51.270189	2023.706459	19.610880
51.238161	2024.557345	19.615898
51.240503	2042.716956	19.620915
51.557639	2038.529726	19.625933
51.667631	2043.660064	19.630951
51.648577	2039.967354	19.635968
51.797283	2046.653875	19.640986
51.489627	2060.866508	19.646003
52.093570	2059.490570	19.651021
52.160151	2059.404438	19.656039
51.969897	2062.274745	19.661056
52.063635	2051.968199	19.666074
52.509788	2071.434346	19.671091
52.397656	2069.391053	19.676109
52.332469	2069.565427	19.681127
52.490504	2062.515324	19.686144
52.573321	2056.284959	19.691162
52.519470	2069.959177	19.696179
52.484906	2057.476112	19.701197
52.226829	2063.285867	19.706215
52.411397	2076.373581	19.711232
52.874800	2084.885510	19.716250
52.850553	2096.074444	19.721267
52.715254	2087.069346	19.726285
52.572127	2097.784560	19.731303
52.616271	2095.483231	19.736320
52.846110	2089.734790	19.741338
52.796723	2092.983851	19.746355
53.111627	2097.119500	19.751373
52.930472	2111.542745	19.756391
53.035152	2113.814539	19.761408
53.382323	2110.780863	19.766426
53.439723	2113.217868	19.771443
53.412576	2111.369555	19.776461
53.343706	2125.759440	19.781479
53.558329	2104.425556	19.786496
53.856542	2107.910517	19.791514
53.828509	2108.691347	19.796531
54.106229	2109.285406	19.801549
53.732209	2117.303654	19.806567
53.820499	2113.613048	19.811584
54.140514	2101.964409	19.816602
54.043805	2108.888236	19.821619
54.377319	2103.846287	19.826637
54.349594	2110.434231	19.831655
54.286358	2102.850688	19.836672
54.452579	2094.416933	19.841690
54.502117	2096.523781	19.846707
54.731423	2101.477638	19.851725
54.424651	2085.019532	19.856743
54.292414	2061.111044	19.861760
54.462792	2065.338763	19.866778
54.205501	2078.347372	19.871795
54.455521	2078.260905	19.876813
54.713389	2092.659536	19.881831
54.599947	2091.307623	19.886848
54.628900	2093.061060	19.891866
54.799161	2098.806872	19.896883
54.419093	2092.377597	19.901901
54.644419	2092.449645	19.906919
54.563139	2090.559319	19.911936
54.661838	2089.597081	19.916954
54.305169	2103.795335	19.921971
54.506392	2109.476334	19.926989
54.554684	2116.645711	19.932007
54.852970	2132.830689	19.937024
55.193240	2118.347871	19.942042
55.297561	2130.116336	19.947059
55.014084	2121.860331	19.952077
55.154677	2127.011148	19.957095
55.065482	2141.593593	19.962112
55.672283	2137.947986	19.967130
55.463726	2146.382173	19.972147
55.635691	2151.717446	19.977165
55.554921	2149.022234	19.982183
55.347368	2150.740142	19.987200
55.923541	2146.919436	19.992218
55.540386	2151.581068	19.997235
55.677820	2148.280420	20.002253
55.301853	2148.415117	20.007271
55.158962	2146.026310	20.012288
55.770334	2164.491445	20.017306
55.748153	2163.627045	20.022323
55.914944	2164.330012	20.027341
56.016739	2161.028633	20.032359
56.008637	2170.536052	20.037376
56.441388	2162.884242	20.042394
56.290611	2157.858189	20.047411
56.839924	2167.095220	20.052429
57.057532	2157.349925	20.057447
56.582733	2157.146626	20.062464
57.000413	2150.314606	20.067482
56.418224	2154.265746	20.072499
56.596072	2148.907317	20.077517
56.530527	2144.016250	20.082535
56.634015	2151.028658	20.087552
57.122089	2174.862669	20.092570
56.848827	2181.277652	20.097587
56.781802	2189.405637	20.102605
56.679818	2177.763101	20.107623
56.954634	2177.966264	20.112640
57.053971	2179.797052	20.117658
56.926447	2175.354382	20.122675
56.857599	2181.349140	20.127693
57.083542	2184.258409	20.132711
57.166918	2198.962199	20.137728
57.466345	2204.097620	20.142746
57.269017	2206.123227	20.147763
57.640989	2201.880027	20.152781
57.652724	2198.469664	20.157799
57.367587	2208.083629	20.162816
57.451384	2210.383956	20.167834
57.615632	2205.687263	20.172851
57.527901	2201.926377	20.177869
58.045464	2199.538237	20.182887
57.937024	2215.149484	20.187904
58.213019	2211.284269	20.192922
58.256381	2224.889720	20.197939
58.197238	2218.536361	20.202957
58.233251	2212.164940	20.207975
58.137626	2214.559655	20.212992
58.463338	2219.785645	20.218010
58.451372	2229.315793	20.223027
58.712208	2228.157717	20.228045
58.625347	2221.373159	20.233063
58.636883	2224.783128	20.238080
58.843471	2211.823477	20.243098
58.716527	2216.280868	20.248115
58.629239	2222.335338	20.253133
59.312796	2213.754196	20.258151
58.462168	2211.946522	20.263168
58.820289	2211.862054	20.268186
58.484634	2217.624047	20.273203
58.639311	2213.875677	20.278221
58.983208	2219.550138	20.283239
59.000102	2218.023147	20.288256
59.057517	2220.005688	20.293274
58.968059	2221.196970	20.298291
58.515260	2220.863979	20.303309
59.036857	2233.958969	20.308327
59.047554	2243.968455	20.313344
59.084570	2246.935739	20.318362
59.087980	2256.750696	20.323379
59.412474	2256.923984	20.328397
59.138775	2245.582888	20.333415
59.082843	2263.631922	20.338432
59.605444	2274.934123	20.343450
59.453145	2284.079150	20.348467
59.533581	2271.912466	20.353485
60.137136	2271.148857	20.358503
59.637246	2272.521222	20.363520
59.911333	2280.826200	20.368538
60.393399	2290.364191	20.373555
60.138908	2297.543206	20.378573
60.427647	2302.872853	20.383591
60.650350	2299.429418	20.388608
60.508309	2301.967129	20.393626
60.500879	2284.445676	20.398643
60.523226	2289.993797	20.403661
60.576291	2297.680099	20.408679
60.868268	2292.467864	20.413696
60.715824	2290.983178	20.418714
60.873409	2291.697061	20.423731
60.603450	2294.491521	20.428749
60.810459	2290.968488	20.433767
60.725739	2293.812828	20.438784
60.648160	2291.795656	20.443802
61.037531	2290.652155	20.448819
60.677281	2285.447427	20.453837
60.856855	2284.993264	20.458855
60.706291	2296.445134	20.463872
61.000323	2303.178415	20.468890
61.148612	2319.273443	20.473907
60.990110	2320.699632	20.478925
61.222923	2323.579442	20.483943
61.117030	2319.322713	20.488960
61.172340	2319.307781	20.493978
61.341564	2322.431105	20.498995
61.185936	2340.158132	20.504013
61.485147	2350.232938	20.509031
61.648939	2343.030330	20.514048
61.357206	2348.700269	20.519066
61.531804	2350.064803	20.524083
61.586876	2365.511694	20.529101
62.135678	2367.022748	20.534119
62.112689	2379.975929	20.539136
62.242654	2371.714999	20.544154
62.457075	2371.138598	20.549171
62.027526	2372.667224	20.554189
62.073033	2362.933002	20.559207
62.136451	2365.968759	20.564224
62.530420	2361.415932	20.569242
62.906448	2373.053616	20.574259
62.794375	2370.025571	20.579277
62.730752	2361.712918	20.584295
62.749982	2373.709489	20.589312
62.552803	2373.285948	20.594330
62.538659	2371.972110	20.599347
62.888374	2392.782440	20.604365
63.021903	2392.165058	20.609383
63.245537	2386.651048	20.614400
63.319764	2387.763042	20.619418
63.253921	2386.886535	20.624435
62.905204	2392.641161	20.629453
63.597876	2385.551354	20.634471
63.258003	2389.669726	20.639488
63.345082	2384.129770	20.644506
63.450527	2386.164770	20.649523
63.009111	2394.727083	20.654541
63.485389	2381.179049	20.659559
63.398394	2384.932721	20.664576
63.440644	2399.052925	20.669594
63.538069	2407.281488	20.674611
63.553409	2414.216282	20.679629
63.971205	2413.816320	20.684647
63.702787	2416.945106	20.689664
63.857537	2409.848041	20.694682
63.983008	2413.360126	20.699699
63.776261	2409.595752	20.704717
63.945991	2421.130075	20.709735
64.230830	2432.772616	20.714752
64.073932	2435.053872	20.719770
64.312285	2424.077450	20.724787
64.331384	2437.620585	20.729805
64.425678	2428.781335	20.734823
64.633727	2428.111248	20.739840
64.471199	2431.804173	20.744858
64.555377	2432.280229	20.749875
64.426917	2440.616789	20.754893
64.659616	2448.013052	20.759911
64.895517	2455.001677	20.764928
64.803256	2451.304572	20.769946
65.121074	2447.937734	20.774963
65.160007	2455.421169	20.779981
65.173001	2446.496808	20.784999
65.411961	2446.939145	20.790016
65.402592	2454.272342	20.795034
65.517262	2448.563924	20.800051
65.442058	2456.989988	20.805069
65.508807	2446.728474	20.810087
65.425734	2445.419119	20.815104
65.147398	2466.239562	20.820122
65.620271	2465.720506	20.825139
65.030313	2480.877196	20.830157
65.845821	2476.441352	20.835175
65.606887	2474.967045	20.840192
65.865828	2477.189467	20.845210
66.121454	2489.682465	20.850227
66.009033	2502.545593	20.855245
66.238514	2498.615014	20.860263
66.062199	2498.626903	20.865280
65.914064	2504.997146	20.870298
66.255675	2493.865635	20.875315
66.315694	2496.636831	20.880333
66.575999	2498.275158	20.885351
66.575446	2494.611017	20.890368
66.165583	2502.985382	20.895386
66.551950	2514.722534	20.900403
66.549354	2524.563828	20.905421
66.641689	2533.771650	20.910439
66.416246	2530.360510	20.915456
66.592174	2525.649280	20.920474
67.139752	2522.789287	20.925491
67.158335	2540.148353	20.930509
67.354500	2543.128625	20.935527
67.262737	2546.782081	20.940544
66.928877	2552.562835	20.945562
67.379014	2546.792359	20.950579
67.375481	2549.516711	20.955597
67.934156	2554.005636	20.960615
67.646826	2548.495884	20.965632
67.341291	2550.497453	20.970650
67.534805	2550.861697	20.975667
67.479974	2547.865684	20.980685
67.493072	2552.433775	20.985703
67.619893	2544.261631	20.990720
67.533304	2559.614105	20.995738
67.795468	2570.808960	21.000755
68.180414	2569.341052	21.005773
68.337885	2575.218423	21.010791
68.428179	2576.738210	21.015808
68.464956	2581.469874	21.020826
68.449688	2580.263506	21.025843
68.496136	2579.353616	21.030861
68.298032	2587.833713	21.035879
68.633830	2573.351232	21.040896
68.584967	2575.542987	21.045914
68.471921	2575.737489	21.050931
68.513177	2580.503168	21.055949
68.419189	2580.470597	21.060967
68.813241	2584.767548	21.065984
68.571204	2596.344404	21.071002
68.927160	2591.851130	21.076019
68.869009	2599.346680	21.081037
68.849046	2598.112641	21.086055
69.043364	2586.167770	21.091072
68.863053	2608.080827	21.096090
69.302340	2617.597291	21.101107
69.221439	2621.785607	21.106125
69.411581	2622.690084	21.111143
69.234564	2624.740961	21.116160
69.106299	2628.829390	21.121178
69.791754	2639.216271	21.126195
69.596741	2642.365156	21.131213
69.615029	2649.826657	21.136231
69.869722	2645.144085	21.141248
70.079332	2643.075567	21.146266
70.394995	2654.312590	21.151283
70.079331	2652.588328	21.156301
69.590869	2641.757210	21.161319
70.294251	2646.690599	21.166336
70.481414	2667.895986	21.171354
70.794740	2670.321375	21.176371
70.498684	2674.335105	21.181389
70.791832	2672.376585	21.186407
70.859855	2665.993676	21.191424
70.768397	2664.111196	21.196442
71.006658	2669.603512	21.201459
71.137312	2664.258638	21.206477
70.906677	2660.516890	21.211495
71.127010	2663.120968	21.216512
70.782844	2660.173423	21.221530
71.131007	2659.071074	21.226547
71.279626	2661.465456	21.231565
71.145752	2658.358719	21.236583
70.855217	2654.326521	21.241600
71.136608	2663.466915	21.246618
71.470193	2662.840275	21.251635
71.663335	2678.297364	21.256653
71.676955	2682.464572	21.261671
71.572784	2683.314167	21.266688
71.389983	2683.873089	21.271706
71.621184	2681.867462	21.276723
71.657374	2684.563517	21.281741
71.719187	2683.537592	21.286759
72.199840	2688.682634	21.291776
71.984189	2699.924025	21.296794
72.460249	2704.624771	21.301811
72.266119	2709.856603	21.306829
71.949128	2716.133442	21.311847
72.211521	2701.835947	21.316864
72.175151	2705.799530	21.321882
72.347498	2697.560216	21.326899
72.522429	2710.268006	21.331917
72.319802	2712.799487	21.336935
72.519972	2725.976759	21.341952
72.373007	2731.068648	21.346970
72.876060	2728.023073	21.351987
72.713950	2737.930505	21.357005
72.649378	2735.362070	21.362023
73.277506	2729.203846	21.367040
72.713184	2730.718898	21.372058
73.046175	2751.406017	21.377075
73.636010	2755.473495	21.382093
73.161176	2758.041318	21.387111
73.200572	2759.679561	21.392128
73.424203	2760.402053	21.397146
73.786598	2752.252874	21.402163
73.565908	2760.938587	21.407181
72.938759	2764.372974	21.412199
73.787526	2771.407730	21.417216
74.041245	2777.888700	21.422234
74.007034	2777.105059	21.427251
73.880766	2778.049650	21.432269
73.757104	2790.479191	21.437287
73.958104	2775.241245	21.442304
73.894992	2791.158352	21.447322
74.124819	2792.978227	21.452339
74.668017	2800.632139	21.457357
74.151168	2801.382274	21.462375
74.250942	2796.575594	21.467392
74.433735	2809.190692	21.472410
74.774000	2806.988062	21.477427
74.894345	2816.055924	21.482445
74.522582	2826.545429	21.487463
75.301882	2814.114231	21.492480
74.873918	2821.835091	21.497498
75.378793	2813.875026	21.502515
75.204598	2817.121678	21.507533
75.348988	2820.059609	21.512551
75.489181	2812.125120	21.517568
75.302047	2813.634737	21.522586
75.517565	2812.177575	21.527603
75.452101	2809.678706	21.532621
75.583767	2811.305654	21.537639
75.720068	2817.792410	21.542656
75.936368	2832.968259	21.547674
76.031793	2842.642871	21.552691
76.055347	2838.501455	21.557709
75.815335	2843.440675	21.562727
76.064335	2836.246615	21.567744
76.006502	2843.101508	21.572762
75.974506	2836.604805	21.577779
76.259738	2834.224578	21.582797
75.866795	2842.757415	21.587815
76.248561	2845.967466	21.592832
76.609130	2867.385791	21.597850
76.789032	2861.382966	21.602867
76.401618	2861.206994	21.607885
76.066321	2866.192711	21.612903
76.607895	2872.395057	21.617920
76.766325	2878.723714	21.622938
76.601159	2889.812127	21.627955
76.817108	2880.432822	21.632973
76.944614	2893.378574	21.637991
76.980674	2884.349384	21.643008
77.045716	2891.210294	21.648026
77.292184	2910.705482	21.653043
77.730436	2906.915696	21.658061
77.729304	2916.611789	21.663079
77.719266	2916.291474	21.668096
77.478979	2913.854699	21.673114
77.431294	2916.469243	21.678131
78.065197	2909.281130	21.683149
77.992006	2915.813368	21.688167
77.893935	2908.310692	21.693184
77.684138	2913.611318	21.698202
77.677754	2902.126926	21.703219
78.251586	2912.970168	21.708237
78.033478	2940.457102	21.713255
78.304213	2934.326398	21.718272
78.285210	2936.734454	21.723290
78.322904	2939.209377	21.728307
78.556758	2937.051809	21.733325
78.158392	2939.935922	21.738343
78.607866	2952.241060	21.743360
78.838482	2959.344333	21.748378
78.733148	2954.377218	21.753395
78.665457	2965.106378	21.758413
79.152355	2961.009120	21.763431
79.210629	2960.214137	21.768448
78.985178	2964.923862	21.773466
78.837364	2971.489905	21.778483
79.375738	2980.041016	21.783501
78.971561	2982.342145	21.788519
79.730466	2979.054446	21.793536
79.334901	2979.327933	21.798554
79.176250	2990.655260	21.803571
79.708991	2999.557604	21.808589
79.918041	3003.126147	21.813607
80.156272	2994.788002	21.818624
79.784714	3003.775216	21.823642
80.070591	2998.835170	21.828659
80.237331	3001.179415	21.833677
79.998742	2994.484618	21.838695
80.614853	3003.629556	21.843712
80.529838	3013.256781	21.848730
80.525631	3028.246406	21.853747
80.799871	3028.383391	21.858765
80.623565	3033.060183	21.863783
80.630709	3029.628289	21.868800
80.770319	3024.367124	21.873818
81.007617	3024.746613	21.878835
80.932828	3020.342814	21.883853
80.891823	3016.874279	21.888871
81.031574	3026.958668	21.893888
81.456160	3038.958455	21.898906
81.452692	3039.625008	21.903923
81.763729	3046.450593	21.908941
81.372286	3050.675036	21.913959
81.376502	3048.818557	21.918976
81.917473	3048.550786	21.923994
81.878361	3054.998829	21.929011
81.942060	3038.645929	21.934029
81.760881	3054.351361	21.939047
81.914054	3045.726676	21.944064
82.036057	3047.850688	21.949082
81.707271	3046.428286	21.954099
82.252737	3062.433345	21.959117
82.028787	3075.052387	21.964135
81.981082	3071.496516	21.969152
81.878329	3075.066582	21.974170
81.715914	3088.780675	21.979187
82.414628	3087.509755	21.984205
82.529805	3093.867358	21.989223
82.588825	3095.650901	21.994240
82.737985	3101.046842	21.999258
82.474336	3102.934595	22.004275
82.801252	3103.909200	22.009293
82.795233	3118.883403	22.014311
83.183494	3119.195055	22.019328
83.541754	3124.062712	22.024346
83.325543	3131.475934	22.029363
83.638133	3116.362249	22.034381
83.727430	3123.743384	22.039399
83.406355	3126.160917	22.044416
83.417798	3119.698337	22.049434
83.532737	3133.810884	22.054451
83.545005	3139.827971	22.059469
84.056600	3149.942546	22.064487
83.906492	3141.179113	22.069504
84.012438	3138.811155	22.074522
83.679645	3147.751335	22.079539
84.390988	3146.285902	22.084557
84.104307	3153.984767	22.089575
84.337977	3166.554270	22.094592
84.447110	3160.808620	22.099610
84.360524	3163.296732	22.104627
84.467596	3172.594104	22.109645
84.469318	3176.794853	22.114663
84.536204	3185.539870	22.119680
84.511303	3183.473313	22.124698
84.494908	3197.792706	22.129715
84.918027	3198.613369	22.134733
84.917720	3207.943363	22.139751
85.417986	3219.315943	22.144768
85.595029	3215.620675	22.149786
85.436575	3221.834974	22.154803
85.461636	3219.605929	22.159821
85.582704	3222.320329	22.164839
85.546106	3221.597012	22.169856
85.901588	3220.682860	22.174874
85.730283	3217.061107	22.179891
85.753621	3224.487336	22.184909
86.088452	3243.681820	22.189927
85.982768	3246.258155	22.194944
86.449557	3244.736341	22.199962
85.996909	3243.330172	22.204979
86.809176	3245.980471	22.209997
86.389017	3244.676525	22.215015
86.475335	3241.320561	22.220032
86.658904	3240.417561	22.225050
86.503248	3254.092845	22.230067
86.574122	3266.637423	22.235085
86.911230	3268.222757	22.240103
87.003585	3268.849056	22.245120
87.337450	3269.642674	22.250138
86.923120	3264.597633	22.255155
87.268919	3264.644502	22.260173
87.102185	3278.211071	22.265191
87.380256	3289.757383	22.270208
87.761397	3284.417270	22.275226
87.694845	3287.726047	22.280243
87.874130	3297.321484	22.285261
87.497060	3293.754046	22.290279
87.749949	3297.650345	22.295296
87.679347	3286.365147	22.300314
87.910941	3297.741996	22.305331
88.154541	3309.300034	22.310349
88.729849	3306.763830	22.315367
88.519119	3314.763335	22.320384
88.685316	3310.286991	22.325402
88.258389	3318.014211	22.330419
88.386140	3308.007778	22.335437
88.596303	3312.579906	22.340455
88.619751	3317.859887	22.345472
88.715936	3310.828457	22.350490
88.642209	3312.856915	22.355507
88.906528	3320.015020	22.360525
88.966841	3326.494927	22.365543
88.394735	3340.488025	22.370560
89.056359	3334.876700	22.375578
88.845473	3325.204222	22.380595
88.991501	3347.792992	22.385613
88.820156	3357.519145	22.390631
89.135483	3359.000587	22.395648
89.739103	3362.359039	22.400666
89.493931	3377.156297	22.405683
89.646286	3386.235212	22.410701
90.316200	3384.605812	22.415719
90.265081	3378.882045	22.420736
90.555469	3381.648848	22.425754
90.302920	3383.793707	22.430771
90.558147	3383.021506	22.435789
90.611681	3380.153566	22.440807
90.492542	3369.387239	22.445824
90.641360	3376.980093	22.450842
90.357903	3376.071349	22.455859
90.538961	3390.688213	22.460877
91.033868	3401.032797	22.465895
90.818944	3406.498497	22.470912
90.867625	3400.276173	22.475930
90.922786	3409.569175	22.480947
91.140372	3401.442393	22.485965
91.775378	3409.265248	22.490983
91.274906	3418.702120	22.496000
91.647763	3428.661836	22.501018
91.999445	3427.448421	22.506035
91.970872	3429.514006	22.511053
91.781034	3431.690077	22.516071
92.096658	3423.595270	22.521088
92.033005	3427.310781	22.526106
92.074549	3428.513180	22.531123
92.042658	3428.862258	22.536141
92.162591	3421.864940	22.541159
92.179342	3427.909827	22.546176
92.369339	3437.497347	22.551194
92.048755	3446.183257	22.556211
92.113623	3448.265767	22.561229
92.251222	3439.334018	22.566247
92.447781	3461.918170	22.571264
92.783757	3470.498070	22.576282
92.417853	3472.625979	22.581299
92.488592	3479.451501	22.586317
92.852293	3495.737929	22.591335
92.868622	3507.334857	22.596352
92.886221	3503.333099	22.601370
93.064950	3518.332345	22.606387
93.251424	3533.469268	22.611405
93.288029	3525.711668	22.616423
93.437126	3535.532903	22.621440
93.660122	3548.277941	22.626458
93.980583	3550.639207	22.631475
93.877882	3556.447190	22.636493
93.939735	3550.001809	22.641511
93.696240	3558.650444	22.646528
93.922626	3567.184433	22.651546
94.112617	3569.509329	22.656563
94.298212	3581.054535	22.661581
94.605033	3579.014870	22.666599
94.600266	3585.918544	22.671616
94.678088	3582.005180	22.676634
94.816312	3595.375860	22.681651
94.996448	3602.641956	22.686669
95.030537	3604.410518	22.691687
94.918056	3608.796545	22.696704
94.969833	3600.452615	22.701722
95.266247	3596.748037	22.706739
95.425126	3604.563509	22.711757
95.493302	3598.963017	22.716775
95.507051	3604.588641	22.721792
95.390454	3616.563130	22.726810
96.050150	3620.850277	22.731827
95.652991	3626.385625	22.736845
96.135377	3624.119600	22.741863
95.482492	3632.848191	22.746880
96.018763	3630.071866	22.751898
96.306766	3645.331855	22.756915
96.447801	3654.797752	22.761933
96.816165	3654.493891	22.766951
96.629785	3654.882960	22.771968
96.540772	3653.650198	22.776986
96.810534	3642.664962	22.782003
96.609047	3649.075529	22.787021
96.803154	3638.676602	22.792039
96.789587	3653.119009	22.797056
96.862873	3665.130065	22.802074
97.366016	3663.103821	22.807091
97.257090	3672.580482	22.812109
97.742291	3670.471827	22.817127
97.370085	3672.553401	22.822144
97.445710	3670.038620	22.827162
97.531329	3681.362828	22.832179
97.462040	3689.494999	22.837197
97.597979	3689.457965	22.842215
97.588893	3694.724216	22.847232
97.941034	3702.676738	22.852250
98.361622	3714.399844	22.857267
98.105847	3724.903258	22.862285
98.762379	3714.984200	22.867303
98.209770	3724.823941	22.872320
98.536970	3722.929415	22.877338
98.738067	3729.813517	22.882355
98.825602	3740.518817	22.887373
98.605744	3738.062947	22.892391
98.934169	3741.426710	22.897408
98.799373	3742.480002	22.902426
99.375552	3742.332962	22.907443
99.237567	3743.983304	22.912461
99.360883	3757.419567	22.917479
99.205380	3763.917661	22.922496
99.554471	3758.494053	22.927514
99.465616	3759.726372	22.932531
99.665278	3764.559081	22.937549
99.890472	3766.285092	22.942567
99.723778	3791.953514	22.947584
100.397168	3783.013406	22.952602
100.281144	3781.418730	22.957619
100.221934	3792.942454	22.962637
100.158853	3776.239457	22.967655
100.132691	3786.968911	22.972672
100.747038	3797.203476	22.977690
100.818385	3810.098713	22.982707
100.653322	3810.664357	22.987725
100.873712	3809.155852	22.992743
100.948878	3807.348150	22.997760
101.010487	3815.311520	23.002778
101.189181	3812.840543	23.007795
101.310904	3810.195423	23.012813
101.493444	3813.092820	23.017831
101.624478	3824.368970	23.022848
101.835224	3834.013421	23.027866
101.520922	3830.104623	23.032883
101.910838	3834.888605	23.037901
101.782467	3841.928528	23.042919
101.507880	3834.809791	23.047936
101.960833	3828.921686	23.052954
102.614087	3833.291959	23.057971
102.328170	3836.625736	23.062989
102.527037	3841.341804	23.068007
102.511617	3843.645259	23.073024
102.407364	3841.414303	23.078042
102.733871	3840.277403	23.083059
102.744798	3839.559241	23.088077
103.074037	3841.095358	23.093095
102.676449	3843.392404	23.098112
103.182176	3853.142156	23.103130
103.285697	3860.568710	23.108147
103.380461	3864.957050	23.113165
103.657449	3866.943248	23.118183
103.509305	3864.068952	23.123200
103.797346	3868.786838	23.128218
103.943486	3866.125259	23.133235
103.606880	3862.712342	23.138253
103.627225	3862.428283	23.143271
103.933370	3875.684484	23.148288
104.208499	3881.603820	23.153306
104.244751	3884.189571	23.158323
104.278516	3892.605543	23.163341
104.368442	3893.181743	23.168359
104.442927	3900.874842	23.173376
104.103700	3916.403772	23.178394
104.683310	3917.133670	23.183411
104.655203	3923.615018	23.188429
104.563502	3920.043778	23.193447
104.693520	3945.132502	23.198464
105.251063	3950.392119	23.203482
105.063993	3949.360926	23.208499
105.252362	3954.523720	23.213517
105.390540	3962.222648	23.218535
105.512627	3976.625121	23.223552
105.411090	3977.524865	23.228570
105.461087	3974.887802	23.233587
105.554752	3979.333156	23.238605
105.946069	3997.604239	23.243623
105.961443	4011.543687	23.248640
105.917452	4003.331362	23.253658
106.960204	3998.657547	23.258675
106.556295	4008.442579	23.263693
106.799617	4002.618825	23.268711
106.988033	4004.050764	23.273728
107.225369	4024.760643	23.278746
107.343501	4014.960494	23.283763
107.157514	4014.756105	23.288781
107.125450	4007.312071	23.293799
107.598593	4019.519541	23.298816
107.246883	4021.680008	23.303834
107.445918	4021.573117	23.308851
107.434185	4023.566690	23.313869
107.407157	4015.686281	23.318887
107.310703	4015.622528	23.323904
107.307910	4038.491145	23.328922
107.740940	4042.712901	23.333939
107.846037	4045.066941	23.338957
107.896691	4061.456584	23.343975
108.279271	4071.519294	23.348992
107.864526	4084.342531	23.354010
107.976844	4082.958253	23.359027
107.973427	4082.024536	23.364045
108.159256	4091.417359	23.369063
108.614626	4094.426721	23.374080
108.298738	4090.028871	23.379098
108.689322	4110.632771	23.384115
109.291564	4118.154899	23.389133
109.549515	4113.484067	23.394151
109.315309	4109.082883	23.399168
109.307364	4124.269699	23.404186
109.817717	4113.240173	23.409203
109.860380	4108.145391	23.414221
109.853992	4111.653216	23.419239
109.825189	4119.738203	23.424256
110.009190	4131.078844	23.429274
110.251648	4134.913831	23.434291
110.246303	4132.695750	23.439309
109.967148	4131.262326	23.444327
110.451315	4124.434936	23.449344
110.276197	4144.452030	23.454362
110.464776	4150.274539	23.459379
110.631483	4160.446874	23.464397
110.595069	4161.273296	23.469415
110.805890	4158.797239	23.474432
111.005638	4172.259712	23.479450
111.163587	4180.678457	23.484467
111.471588	4179.755917	23.489485
111.714880	4170.794624	23.494503
111.815213	4171.760600	23.499520
111.874536	4181.520496	23.504538
111.954941	4176.950062	23.509555
111.907497	4170.288009	23.514573
111.816503	4174.074241	23.519591
112.531048	4188.680768	23.524608
112.431888	4193.809766	23.529626
113.090627	4179.360634	23.534643
112.800655	4189.061627	23.539661
113.200805	4185.198639	23.544679
113.104330	4178.964070	23.549696
112.890645	4194.318904	23.554714
113.052882	4177.678085	23.559731
113.301048	4176.742825	23.564749
112.891220	4186.778238	23.569767
113.191604	4176.258191	23.574784
113.317058	4178.583808	23.579802
113.123471	4197.423350	23.584819
113.658399	4203.639828	23.589837
113.558268	4209.210883	23.594855
113.574464	4212.301697	23.599872
113.453984	4219.602514	23.604890
113.904436	4232.688016	23.609907
113.872368	4241.950920	23.614925
113.642550	4245.891487	23.619943
114.435610	4260.640437	23.624960
114.074509	4269.566662	23.629978
114.178711	4267.722801	23.634995
114.418060	4270.292571	23.640013
114.470726	4283.304703	23.645031
114.893749	4287.446018	23.650048
114.671573	4302.010005	23.655066
114.675729	4301.558027	23.660083
115.299190	4305.649005	23.665101
115.308454	4315.110640	23.670119
115.462053	4318.533468	23.675136
115.111697	4325.450533	23.680154
115.535262	4331.722380	23.685171
115.910173	4347.303930	23.690189
115.868921	4354.592388	23.695207
116.202897	4345.200150	23.700224
115.993184	4352.391898	23.705242
116.229819	4347.547584	23.710259
116.291622	4351.707628	23.715277
116.125082	4368.049507	23.720295
116.319367	4366.327251	23.725312
116.405437	4372.484695	23.730330
116.549009	4383.115310	23.735347
117.090901	4386.130106	23.740365
117.157020	4395.576563	23.745383
117.333121	4394.037071	23.750400
116.940029	4399.916070	23.755418
116.975987	4410.374173	23.760435
117.396342	4419.436872	23.765453
117.589477	4421.085901	23.770471
117.863489	4421.144025	23.775488
118.142927	4427.694159	23.780506
118.172420	4439.305404	23.785523
118.429522	4442.566842	23.790541
118.384829	4449.455004	23.795559
118.842517	4447.877706	23.800576
118.734914	4445.906030	23.805594
118.520924	4443.660626	23.810611
118.593872	4437.737167	23.815629
118.895730	4455.119976	23.820647
119.027633	4450.765515	23.825664
119.020483	4463.506221	23.830682
119.046648	4464.644813	23.835699
119.363089	4455.432028	23.840717
119.378547	4457.430858	23.845735
119.582855	4467.142942	23.850752
119.738807	4484.494978	23.855770
119.834164	4486.001508	23.860787
119.927681	4487.760845	23.865805
119.862133	4486.896815	23.870823
120.300048	4497.894882	23.875840
120.189902	4523.703833	23.880858
120.529859	4514.784044	23.885875
120.374605	4517.753415	23.890893
120.260815	4516.161480	23.895911
120.468703	4525.570011	23.900928
120.628050	4541.485367	23.905946
121.045637	4541.539937	23.910963
121.347760	4547.265873	23.915981
120.968710	4558.019503	23.920999
121.113121	4565.480974	23.926016
121.354894	4575.638625	23.931034
121.478502	4569.464136	23.936051
121.908719	4583.231709	23.941069
121.183038	4602.909436	23.946087
121.460887	4605.795185	23.951104
121.958036	4619.097763	23.956122
121.698639	4620.296885	23.961139
121.754223	4626.620173	23.966157
121.834576	4645.073200	23.971175
122.660183	4645.117508	23.976192
122.336788	4651.187683	23.981210
122.284083	4664.036675	23.986227
122.832567	4665.888890	23.991245
122.916585	4678.725942	23.996263
123.020353	4672.835456	24.001280
123.416638	4702.226875	24.006298
123.413651	4704.500082	24.011315
124.114513	4697.951026	24.016333
124.221561	4703.486617	24.021351
124.428975	4695.651253	24.026368
124.496167	4700.388176	24.031386
124.178005	4701.340832	24.036403
124.223948	4693.117262	24.041421
124.282003	4707.347269	24.046439
124.483822	4696.141618	24.051456
124.909980	4698.982052	24.056474
124.706970	4709.878643	24.061491
125.045745	4728.392278	24.066509
124.786298	4726.469613	24.071527
125.048653	4722.669137	24.076544
124.780010	4724.791418	24.081562
124.701432	4731.571362	24.086579
125.264009	4741.224307	24.091597
125.297527	4747.358545	24.096615
124.904229	4752.975697	24.101632
125.888848	4772.912797	24.106650
125.770204	4784.449618	24.111667
125.942016	4779.085048	24.116685
126.003972	4790.442065	24.121703
125.875902	4794.493070	24.126720
125.964293	4806.938117	24.131738
125.577967	4808.457008	24.136755
126.189677	4822.631931	24.141773
126.313930	4831.659156	24.146791
126.402978	4840.221577	24.151808
127.034157	4859.147233	24.156826
127.192471	4864.292900	24.161843
127.469775	4859.934501	24.166861
127.469259	4865.831058	24.171879
127.708367	4872.769614	24.176896
127.965530	4882.786138	24.181914
127.970125	4886.383932	24.186931
127.927693	4881.251761	24.191949
127.745677	4882.915415	24.196967
128.028215	4898.925420	24.201984
128.430055	4906.308821	24.207002
128.083797	4902.414265	24.212019
128.118091	4914.062939	24.217037
128.624618	4930.056818	24.222055
128.968604	4927.455630	24.227072
129.074814	4924.822249	24.232090
128.816497	4945.683432	24.237107
129.291033	4946.647642	24.242125
129.235706	4958.098895	24.247143
129.315612	4958.395765	24.252160
129.918052	4963.939052	24.257178
130.178585	4976.429846	24.262195
130.149229	4973.625147	24.267213
130.027552	4979.231378	24.272231
130.374047	4977.611482	24.277248
130.452430	4972.176266	24.282266
130.190479	4980.815839	24.287283
130.502267	4987.155932	24.292301
130.827169	4995.747763	24.297319
131.094482	4998.963510	24.302336
131.139090	5003.047483	24.307354
130.824627	5005.574703	24.312371
131.095658	5014.844177	24.317389
131.363298	5022.330721	24.322407
131.344348	5029.120373	24.327424
131.526764	5029.966211	24.332442
131.414998	5026.669362	24.337459
131.793569	5039.492087	24.342477
131.926204	5058.745427	24.347495
132.009867	5066.305005	24.352512
132.068814	5065.696065	24.357530
132.028629	5083.477130	24.362547
132.230892	5074.824855	24.367565
132.433687	5087.378433	24.372583
132.431576	5099.032929	24.377600
132.778567	5107.353043	24.382618
132.659158	5120.626320	24.387635
132.893917	5107.795924	24.392653
132.825545	5134.842891	24.397671
132.924104	5139.164657	24.402688
133.421472	5132.173839	24.407706
133.687616	5151.437927	24.412723
133.567721	5159.686006	24.417741
133.777055	5162.592050	24.422759
133.443048	5170.362309	24.427776
134.143978	5177.885203	24.432794
133.774374	5188.113727	24.437811
134.087189	5195.836324	24.442829
134.481368	5206.361871	24.447847
134.981065	5214.850663	24.452864
135.061723	5212.363291	24.457882
135.031223	5210.774028	24.462899
134.888002	5217.277028	24.467917
135.363793	5238.033004	24.472935
135.456247	5238.507840	24.477952
135.972370	5240.058995	24.482970
135.635661	5254.941563	24.487987
135.855824	5241.545169	24.493005
135.940308	5258.602949	24.498023
135.856652	5263.751915	24.503040
136.333594	5261.439198	24.508058
136.384501	5279.695459	24.513075
136.654835	5276.455497	24.518093
136.377937	5284.134785	24.523111
136.869214	5292.770137	24.528128
137.106129	5285.277128	24.533146
137.118960	5300.881500	24.538163
137.159464	5306.112039	24.543181
137.514810	5318.079997	24.548199
137.220387	5312.627328	24.553216
137.969932	5303.892360	24.558234
137.686094	5308.318268	24.563251
138.416030	5330.881160	24.568269
138.154431	5334.940577	24.573287
137.943040	5336.018585	24.578304
138.172558	5340.108387	24.583322
138.315223	5342.523000	24.588339
138.619765	5355.243908	24.593357
138.647724	5357.083046	24.598375
138.662121	5362.491306	24.603392
139.015440	5362.887396	24.608410
139.064424	5381.137746	24.613427
139.451632	5371.575655	24.618445
139.580750	5377.530983	24.623463
139.446244	5385.229042	24.628480
139.881684	5395.697728	24.633498
139.927358	5409.219980	24.638515
140.073497	5409.613807	24.643533
140.147722	5414.428730	24.648551
140.278033	5421.210926	24.653568
140.711059	5429.659758	24.658586
140.357506	5439.668098	24.663603
140.565038	5440.194357	24.668621
140.469387	5438.921476	24.673639
140.858425	5454.615403	24.678656
141.139647	5458.949664	24.683674
140.980733	5460.852813	24.688691
141.004338	5474.826815	24.693709
141.401513	5475.320208	24.698727
141.253112	5487.676550	24.703744
141.575649	5486.903191	24.708762
142.113410	5510.099334	24.713779
142.192456	5513.625611	24.718797
142.412042	5508.894146	24.723815
142.245411	5516.379483	24.728832
142.393847	5514.752691	24.733850
142.845344	5528.028365	24.738867
142.775380	5535.766882	24.743885
142.752721	5536.480727	24.748903
142.651307	5550.584856	24.753920
142.975696	5547.611008	24.758938
143.185162	5567.405265	24.763955
143.035412	5565.752580	24.768973
143.561461	5565.269315	24.773991
143.114111	5590.472858	24.779008
143.854087	5591.499690	24.784026
143.656622	5595.334463	24.789043
143.949624	5612.309398	24.794061
144.236077	5614.114379	24.799079
144.167407	5620.119714	24.804096
144.811007	5641.089767	24.809114
145.030785	5645.616787	24.814131
144.917355	5645.416792	24.819149
145.082324	5651.631755	24.824167
144.854608	5649.795562	24.829184
145.638984	5667.182853	24.834202
145.763658	5676.251468	24.839219
145.639914	5678.692080	24.844237
145.618116	5676.185974	24.849255
145.703383	5681.191795	24.854272
146.386773	5691.119893	24.859290
146.188820	5690.358622	24.864307
146.196124	5687.039842	24.869325
147.020328	5699.521742	24.874343
146.525299	5713.633999	24.879360
146.395688	5717.742270	24.884378
147.125230	5722.530369	24.889395
146.902440	5726.470151	24.894413
147.400384	5739.599809	24.899431
147.506222	5746.297573	24.904448
147.464939	5745.069816	24.909466
147.438090	5759.730630	24.914483
147.516478	5770.359641	24.919501
147.939615	5770.138718	24.924519
147.957231	5779.388305	24.929536
148.337738	5787.548801	24.934554
148.560721	5795.096325	24.939571
148.493259	5806.606831	24.944589
148.918360	5814.454153	24.949607
148.994546	5821.993118	24.954624
148.909605	5816.851560	24.959642
149.118660	5826.986626	24.964659
148.997097	5849.686719	24.969677
149.335123	5844.087455	24.974695
149.228434	5862.312166	24.979712
149.756154	5872.653028	24.984730
149.719251	5875.512532	24.989747
150.035796	5885.037327	24.994765
150.043886	5889.998475	24.999783
150.498125	5900.824374	25.004800
150.428278	5899.544261	25.009818
150.755203	5916.580456	25.014835
150.754423	5921.719780	25.019853
151.204008	5923.224599	25.024871
151.159689	5925.283463	25.029888
151.359307	5935.880951	25.034906
151.661666	5939.946850	25.039923
151.511999	5953.534831	25.044941
151.628816	5950.486110	25.049959
151.547109	5957.933068	25.054976
151.828069	5972.031282	25.059994
152.635102	5965.578790	25.065011
152.326287	5982.651510	25.070029
152.630793	5971.290095	25.075047
153.060914	5977.040627	25.080064
152.383542	5993.669175	25.085082
153.205278	5998.076723	25.090099
152.926003	6001.895987	25.095117
153.028863	5990.998625	25.100135
153.328618	6014.197972	25.105152
153.475766	6018.591253	25.110170
153.416622	6023.528247	25.115187
153.398064	6031.457795	25.120205
153.842258	6044.829693	25.125223
153.719446	6051.178266	25.130240
153.748683	6073.807660	25.135258
154.164434	6082.603589	25.140275
154.142777	6091.591163	25.145293
154.432283	6103.169044	25.150311
154.784785	6101.832220	25.155328
154.691347	6111.108844	25.160346
155.276251	6120.402314	25.165363
155.436788	6130.144240	25.170381
155.679812	6134.677210	25.175399
155.513165	6152.665375	25.180416
155.911482	6151.577068	25.185434
155.952287	6161.138893	25.190451
155.967596	6170.294336	25.195469
156.334830	6181.045642	25.200487
156.619458	6194.032267	25.205504
156.378803	6194.060545	25.210522
157.054034	6198.323786	25.215539
157.244980	6213.856838	25.220557
157.346049	6220.037810	25.225575
157.183993	6209.137627	25.230592
156.950558	6223.209291	25.235610
157.935871	6231.382566	25.240627
157.675393	6234.217172	25.245645
157.961720	6240.170251	25.250663
158.034227	6255.718737	25.255680
158.501188	6260.841699	25.260698
158.881860	6255.434508	25.265715
158.578749	6261.723011	25.270733
158.988979	6266.804354	25.275751
159.239118	6271.251010	25.280768
159.497876	6274.092667	25.285786
159.322165	6275.079905	25.290803
159.392736	6280.365991	25.295821
159.303772	6286.472583	25.300839
159.508455	6298.306950	25.305856
159.702074	6304.429257	25.310874
160.073236	6311.622317	25.315891
159.941365	6325.586601	25.320909
160.461074	6323.525913	25.325927
160.111262	6341.186240	25.330944
160.415117	6351.925479	25.335962
160.735601	6361.102657	25.340979
160.594203	6368.205571	25.345997
160.688656	6384.410501	25.351015
160.967375	6391.239257	25.356032
160.560803	6399.270790	25.361050
161.372554	6406.372765	25.366067
161.436160	6428.801490	25.371085
161.674798	6435.911186	25.376103
162.063709	6446.163632	25.381120
162.080474	6468.040986	25.386138
162.397668	6476.738901	25.391155
162.661740	6470.033518	25.396173
162.567491	6471.715132	25.401191
162.812671	6488.016499	25.406208
162.736196	6492.485967	25.411226
162.777186	6497.827258	25.416243
162.916819	6517.693463	25.421261
163.384814	6510.277400	25.426279
163.246924	6515.716171	25.431296
163.545221	6542.935065	25.436314
163.985884	6544.141437	25.441331
164.090037	6550.157883	25.446349
164.626960	6558.452062	25.451367
164.832985	6568.685877	25.456384
164.607572	6574.403552	25.461402
164.978744	6564.249869	25.466419
165.170304	6568.289072	25.471437
165.341543	6571.207624	25.476455
165.509765	6593.010890	25.481472
165.511731	6591.375381	25.486490
165.782795	6598.322218	25.491507
166.239893	6605.647146	25.496525
166.223814	6615.041335	25.501543
166.432689	6616.366103	25.506560
166.379443	6624.490752	25.511578
166.666797	6618.779233	25.516595
166.315477	6630.865077	25.521613
166.081795	6636.413597	25.526631
166.315431	6650.324022	25.531648
166.435478	6667.390170	25.536666
166.997249	6677.618823	25.541683
167.325824	6692.483563	25.546701
167.463116	6702.046337	25.551719
167.661021	6712.464602	25.556736
167.541461	6732.636822	25.561754
167.687390	6742.274030	25.566771
167.815571	6760.851131	25.571789
168.168934	6768.549103	25.576807
168.352472	6783.285109	25.581824
168.108653	6796.680108	25.586842
168.655779	6805.367413	25.591859
168.653477	6828.542504	25.596877
169.067900	6841.559765	25.601895
169.449965	6846.686723	25.606912
169.498372	6853.472812	25.611930
169.670372	6872.655599	25.616947
169.877469	6873.901742	25.621965
170.485104	6879.163843	25.626983
170.578486	6887.025713	25.632000
170.658917	6897.658214	25.637018
171.069398	6900.577221	25.642035
171.476699	6890.152521	25.647053
171.588038	6887.587508	25.652071
171.601248	6900.086797	25.657088
171.642797	6917.591657	25.662106
171.951231	6918.995557	25.667123
171.945473	6925.310308	25.672141
172.127254	6922.579567	25.677159
172.562485	6924.834908	25.682176
172.720870	6933.128581	25.687194
173.109501	6936.704496	25.692212
172.931293	6947.159719	25.697229
172.700843	6945.371176	25.702247
173.267587	6943.119954	25.707264
173.567823	6942.934059	25.712282
173.531241	6958.635978	25.717300
173.376576	6969.980930	25.722317
173.458898	6975.334827	25.727335
173.674457	6974.016240	25.732352
173.583117	6991.715619	25.737370
174.048820	6992.362483	25.742388
174.161025	7001.777812	25.747405
174.463985	7021.420089	25.752423
174.331680	7024.881904	25.757440
174.506463	7041.933511	25.762458
174.423183	7050.151447	25.767476
174.872676	7064.160960	25.772493
174.834130	7073.296878	25.777511
175.611693	7077.358039	25.782528
175.364363	7090.902177	25.787546
175.746733	7108.937857	25.792564
175.904004	7116.253138	25.797581
175.919354	7119.975963	25.802599
176.215986	7130.862010	25.807616
176.152049	7149.441189	25.812634
176.100006	7157.297545	25.817652
176.141464	7177.984864	25.822669
176.191129	7186.756598	25.827687
176.731445	7202.898713	25.832704
177.071903	7214.377764	25.837722
177.162632	7230.337781	25.842740
177.390545	7254.010867	25.847757
177.577387	7258.729708	25.852775
178.032284	7272.656454	25.857792
178.206672	7283.864811	25.862810
178.414317	7284.034372	25.867828
178.667668	7310.380651	25.872845
178.721523	7303.490070	25.877863
179.722617	7308.387587	25.882880
179.639376	7328.946234	25.887898
179.847479	7328.844225	25.892916
179.976335	7328.953519	25.897933
180.341488	7325.540499	25.902951
180.683114	7323.346598	25.907968
180.648249	7332.614661	25.912986
180.805461	7322.061577	25.918004
180.682283	7330.178551	25.923021
180.468007	7342.716936	25.928039
181.415931	7349.018177	25.933056
181.359111	7355.716756	25.938074
181.177029	7359.981990	25.943092
181.387850	7367.727801	25.948109
181.474827	7368.705512	25.953127
181.604579	7376.018893	25.958144
181.918905	7409.367415	25.963162
181.934937	7395.019612	25.968180
182.182511	7408.082357	25.973197
182.370321	7426.297207	25.978215
182.264523	7430.711513	25.983232
182.622928	7453.224739	25.988250
182.607959	7465.110055	25.993268
183.129203	7480.021018	25.998285
182.961737	7486.538087	26.003303
183.235607	7499.060087	26.008320
183.285299	7517.634464	26.013338
183.468320	7534.719964	26.018356
183.949218	7532.870433	26.023373
183.922383	7563.990166	26.028391
184.603880	7565.982861	26.033408
184.619493	7591.672244	26.038426
185.011701	7601.208179	26.043444
185.391749	7604.864497	26.048461
185.443094	7607.925121	26.053479
185.812745	7611.816689	26.058496
186.125613	7625.175589	26.063514
186.171247	7616.739238	26.068532
186.444292	7620.639628	26.073549
186.326788	7617.403192	26.078567
186.435752	7625.389218	26.083584
186.421770	7637.441812	26.088602
186.884782	7631.108943	26.093620
187.004764	7633.982026	26.098637
187.231407	7648.866667	26.103655
187.182575	7658.863197	26.108672
187.673587	7658.224369	26.113690
187.577475	7662.109989	26.118708
188.157100	7682.164241	26.123725
187.797272	7694.267896	26.128743
188.231510	7693.012869	26.133760
188.623789	7704.777713	26.138778
188.477525	7718.145468	26.143796
188.469251	7724.350391	26.148813
188.549400	7738.348827	26.153831
188.868589	7748.928631	26.158848
188.734321	7754.796556	26.163866
189.236867	7770.724096	26.168884
189.605689	7780.570021	26.173901
189.970366	7803.849857	26.178919
189.713016	7793.702412	26.183936
190.168422	7814.164586	26.188954
190.097833	7823.548988	26.193972
190.237481	7833.146709	26.198989
190.491151	7853.533191	26.204007
190.443650	7868.363087	26.209024
190.877664	7885.346450	26.214042
190.984810	7904.685697	26.219060
191.381298	7909.545502	26.224077
191.549313	7930.526388	26.229095
191.866230	7938.805150	26.234112
192.255094	7946.706423	26.239130
192.116348	7975.877522	26.244148
192.275680	7975.669496	26.249165
192.384266	7995.557945	26.254183
193.232945	8002.544266	26.259200
193.028241	8013.045283	26.264218
192.996667	8036.718983	26.269236
193.343753	8044.213265	26.274253
193.306096	8056.490838	26.279271
193.848977	8073.170023	26.284288
194.100986	8085.534834	26.289306
194.169107	8101.745400	26.294324
194.473956	8110.392353	26.299341
194.524699	8126.015284	26.304359
194.766867	8126.147875	26.309376
195.047506	8143.802711	26.314394
195.236762	8149.083369	26.319412
195.748016	8163.481842	26.324429
195.871077	8174.345185	26.329447
195.863459	8172.597382	26.334464
195.892988	8194.020159	26.339482
196.025802	8204.228468	26.344500
196.456106	8209.379824	26.349517
196.367736	8228.188071	26.354535
196.846664	8238.269563	26.359552
196.830285	8247.187903	26.364570
197.156883	8251.117923	26.369588
198.112510	8255.246171	26.374605
198.142683	8254.174380	26.379623
198.374236	8261.409022	26.384640
198.553379	8257.147290	26.389658
198.663160	8265.013494	26.394676
198.990818	8272.826625	26.399693
199.118924	8279.603910	26.404711
199.315441	8277.868317	26.409728
198.946063	8287.823846	26.414746
198.911254	8301.256647	26.419764
200.041064	8307.270845	26.424781
199.789806	8314.470645	26.429799
199.911650	8306.568225	26.434816
200.310049	8315.566848	26.439834
200.534395	8331.437427	26.444852
200.463992	8331.015973	26.449869
200.365143	8345.289167	26.454887
200.613244	8361.418093	26.459904
200.649272	8367.701535	26.464922
200.866279	8386.253730	26.469940
201.181653	8394.008851	26.474957
201.330242	8414.658672	26.479975
201.292528	8428.976025	26.484992
201.651107	8436.863310	26.490010
201.610036	8459.392989	26.495028
202.031247	8467.974524	26.500045
201.957087	8489.634889	26.505063
202.204290	8510.562984	26.510080
202.624577	8531.063027	26.515098
202.632232	8555.321636	26.520116
202.898572	8554.686407	26.525133
203.000304	8585.724572	26.530151
203.396712	8606.430499	26.535168
203.851138	8608.998765	26.540186
203.822609	8628.508411	26.545204
204.520911	8636.020528	26.550221
204.731631	8653.232168	26.555239
204.854402	8664.474708	26.560256
205.374930	8666.802151	26.565274
205.939409	8682.556602	26.570292
205.982523	8673.384537	26.575309
206.265616	8678.454900	26.580327
206.340197	8674.897724	26.585344
206.608717	8679.768310	26.590362
206.954852	8687.714482	26.595380
207.164561	8700.954563	26.600397
206.909847	8703.053010	26.605415
206.913325	8706.961133	26.610432
207.328733	8717.318044	26.615450
207.533890	8733.665555	26.620468
208.025208	8734.662083	26.625485
207.763643	8735.463993	26.630503
207.987782	8758.621817	26.635520
208.255548	8758.362066	26.640538
208.353923	8782.840395	26.645556
208.356755	8793.609277	26.650573
208.477172	8808.063167	26.655591
208.773163	8816.263514	26.660608
208.947463	8829.420832	26.665626
209.075019	8854.661890	26.670644
209.509943	8866.913324	26.675661
209.569152	8881.035878	26.680679
209.967984	8897.350036	26.685696
210.249035	8908.444796	26.690714
209.911643	8920.795154	26.695732
210.435128	8932.660203	26.700749
210.472329	8948.169130	26.705767
210.693095	8965.654167	26.710784
211.304917	8979.298726	26.715802
211.183016	8997.033224	26.720820
211.833309	9005.932735	26.725837
212.178349	9025.728416	26.730855
212.032964	9024.021058	26.735872
212.624898	9035.247155	26.740890
212.765525	9036.709084	26.745908
213.417088	9059.143613	26.750925
213.643607	9062.559065	26.755943
213.741178	9069.155144	26.760960
214.059828	9059.475605	26.765978
213.517627	9068.833485	26.770996
213.815741	9071.517866	26.776013
214.513619	9081.022469	26.781031
214.396616	9093.458393	26.786048
214.580051	9096.495413	26.791066
214.869183	9105.151611	26.796084
214.831029	9109.416797	26.801101
215.306524	9115.960003	26.806119
215.241711	9133.698316	26.811136
215.454714	9137.156945	26.816154
215.363807	9149.456212	26.821172
215.720964	9166.452793	26.826189
216.251292	9182.446660	26.831207
216.005052	9206.133380	26.836224
216.598353	9216.150131	26.841242
216.921073	9226.190332	26.846260
216.869979	9228.698960	26.851277
217.396252	9251.952146	26.856295
217.272162	9258.633533	26.861312
217.752849	9275.370908	26.866330
218.013963	9288.657031	26.871348
217.881520	9291.907748	26.876365
218.549203	9303.775705	26.881383
218.539083	9319.027141	26.886400
218.712740	9333.274189	26.891418
218.903560	9340.616669	26.896436
218.892183	9361.595705	26.901453
219.241021	9377.678161	26.906471
219.518267	9399.192972	26.911488
219.475976	9399.306992	26.916506
219.776160	9423.577739	26.921524
220.167141	9434.642963	26.926541
220.564991	9463.678662	26.931559
220.704720	9474.874833	26.936576
220.615836	9479.694270	26.941594
220.830918	9499.144564	26.946612
221.499307	9513.907828	26.951629
221.772272	9532.209288	26.956647
221.667080	9549.505979	26.961664
222.134852	9553.963543	26.966682
222.363075	9571.558489	26.971700
222.342150	9579.070001	26.976717
222.691820	9594.571561	26.981735
222.958307	9606.123680	26.986752
223.717430	9620.677058	26.991770
223.726847	9623.419376	26.996788
223.347989	9630.175539	27.001805
223.909547	9634.953110	27.006823
224.300705	9665.606743	27.011840
224.426952	9670.992428	27.016858
224.667607	9695.222337	27.021876
224.858239	9699.309736	27.026893
225.249993	9704.994834	27.031911
224.943626	9727.011909	27.036928
225.427244	9729.357904	27.041946
225.941961	9745.133685	27.046964
226.076209	9754.231224	27.051981
226.471432	9765.835894	27.056999
226.534813	9790.052652	27.062016
226.759984	9783.339544	27.067034
226.572408	9805.578064	27.072052
226.920517	9824.859461	27.077069
227.422489	9834.641421	27.082087
227.846488	9848.903322	27.087104
227.730285	9849.009979	27.092122
227.804078	9864.185566	27.097140
228.143119	9888.968647	27.102157
228.189482	9895.803533	27.107175
228.385441	9903.600097	27.112192
228.679597	9925.172857	27.117210
229.051542	9933.213402	27.122228
229.027198	9956.560043	27.127245
229.596094	9959.978860	27.132263
229.684998	9972.143147	27.137280
229.758501	9990.684695	27.142298
230.377281	10006.390720	27.147316
230.606724	10016.638565	27.152333
230.817117	10014.423868	27.157351
230.600101	10035.546386	27.162368
230.729076	10047.698131	27.167386
230.856926	10064.027349	27.172404
231.193172	10080.699669	27.177421
231.763782	10096.343853	27.182439
231.900058	10117.461638	27.187456
232.263635	10136.677786	27.192474
232.067488	10143.910702	27.197492
232.154601	10169.942925	27.202509
232.918416	10189.541630	27.207527
232.978032	10203.510407	27.212544
233.441143	10224.627632	27.217562
233.701505	10226.822375	27.222580
233.437434	10250.349022	27.227597
233.809289	10259.659025	27.232615
233.972851	10280.627476	27.237632
234.428549	10299.864093	27.242650
234.769193	10307.110862	27.247668
234.533517	10326.765247	27.252685
235.299138	10338.271203	27.257703
235.819710	10360.816235	27.262720
236.098810	10368.391575	27.267738
236.324079	10381.002076	27.272756
236.352272	10392.686737	27.277773
236.895663	10397.666276	27.282791
236.973051	10418.730476	27.287808
237.274985	10422.847961	27.292826
237.517631	10436.914540	27.297844
237.834934	10444.790204	27.302861
238.545338	10439.491188	27.307879
238.448367	10457.684162	27.312896
238.650039	10476.357672	27.317914
238.879440	10477.711084	27.322932
238.788114	10493.825569	27.327949
239.391396	10493.879511	27.332967
239.441430	10519.087604	27.337984
239.663027	10527.695052	27.343002
239.627480	10529.737263	27.348020
240.145996	10548.064404	27.353037
240.243043	10562.378071	27.358055
240.591068	10581.666579	27.363072
240.878044	10592.142542	27.368090
240.716405	10598.047223	27.373108
240.727845	10617.742139	27.378125
241.147843	10633.208287	27.383143
241.291921	10646.450562	27.388160
241.664582	10672.176677	27.393178
242.084210	10683.244473	27.398196
242.287287	10690.332962	27.403213
243.087219	10689.415152	27.408231
242.912320	10715.621797	27.413248
242.903984	10724.732672	27.418266
243.585804	10728.001327	27.423284
243.562825	10759.757309	27.428301
244.037009	10756.639190	27.433319
244.432704	10773.160727	27.438336
244.274562	10780.634223	27.443354
245.149836	10784.387264	27.448372
244.946102	10812.982519	27.453389
245.121640	10808.518691	27.458407
245.067750	10823.247739	27.463424
244.998093	10838.872861	27.468442
245.677259	10849.391730	27.473460
245.764974	10874.019720	27.478477
245.843560	10882.624474	27.483495
246.289803	10898.762452	27.488512
246.302786	10917.087053	27.493530
246.407547	10926.480279	27.498548
246.796926	10952.428349	27.503565
246.643041	10959.528654	27.508583
247.158464	10987.721017	27.513600
247.342248	11010.692190	27.518618
247.780734	11024.567495	27.523636
247.664512	11043.543979	27.528653
248.032796	11076.549608	27.533671
248.264242	11088.834385	27.538688
248.336073	11113.307297	27.543706
249.073873	11134.714069	27.548724
248.944011	11161.899458	27.553741
249.498778	11175.481946	27.558759
250.048359	11192.156573	27.563776
250.771397	11201.317304	27.568794
251.542016	11199.529402	27.573812
251.697749	11205.119315	27.578829
251.848305	11206.706166	27.583847
252.115913	11218.028601	27.588864
252.398279	11230.261287	27.593882
252.264240	11224.440709	27.598900
252.571558	11245.264573	27.603917
252.658782	11249.671645	27.608935
252.550546	11267.882956	27.613952
252.881316	11290.013616	27.618970
253.647983	11296.575135	27.623988
253.749127	11325.423385	27.629005
254.146892	11323.062351	27.634023
254.242204	11346.433027	27.639040
254.465503	11349.956767	27.644058
254.824643	11348.353302	27.649076
255.248717	11367.087591	27.654093
255.514741	11369.802597	27.659111
255.184195	11376.444454	27.664128
255.691451	11391.878615	27.669146
255.719517	11404.252297	27.674164
255.672291	11424.718246	27.679181
256.104509	11444.310221	27.684199
256.150136	11464.417482	27.689216
256.330460	11482.113303	27.694234
257.078095	11498.482460	27.699252
256.943950	11520.297828	27.704269
256.997804	11536.592556	27.709287
257.765736	11559.513941	27.714304
257.675135	11580.804696	27.719322
257.885030	11598.502310	27.724340
258.040411	11622.590189	27.729357
258.348678	11640.679775	27.734375
258.848606	11669.286093	27.739392
258.878679	11693.074763	27.744410
259.086574	11703.633206	27.749428
259.396190	11734.669298	27.754445
259.734061	11763.193782	27.759463
260.529436	11771.320361	27.764480
260.552558	11791.655695	27.769498
260.761402	11805.463349	27.774516
261.325964	11827.381185	27.779533
261.954293	11838.552755	27.784551
261.797598	11842.890814	27.789568
261.826984	11856.054019	27.794586
262.280884	11874.095755	27.799604
262.284623	11880.057031	27.804621
262.622906	11897.052741	27.809639
263.042501	11900.567939	27.814656
262.923829	11911.998671	27.819674
263.543868	11926.045142	27.824692
263.516877	11945.681157	27.829709
263.731296	11961.843736	27.834727
264.453762	11981.040293	27.839744
264.563460	11986.577653	27.844762
265.041740	12000.444290	27.849780
265.226805	12017.675682	27.854797
265.904559	12029.878528	27.859815
266.214472	12040.844321	27.864832
265.918391	12047.092608	27.869850
266.402494	12056.389081	27.874868
266.446600	12078.685572	27.879885
266.895334	12091.653782	27.884903
267.264502	12090.610770	27.889920
267.058903	12114.749511	27.894938
267.576414	12130.950015	27.899956
267.708497	12150.223441	27.904973
267.560443	12152.697122	27.909991
268.118431	12172.162790	27.915008
268.118152	12204.801836	27.920026
268.297507	12216.103962	27.925044
268.750145	12248.056361	27.930061
268.607644	12278.425248	27.935079
269.236169	12293.323273	27.940096
269.171889	12319.821128	27.945114
269.986430	12340.910950	27.950132
270.091269	12356.816303	27.955149
270.162097	12372.600685	27.960167
271.013030	12393.773284	27.965184
270.972255	12409.047822	27.970202
271.533616	12427.142727	27.975220
271.830695	12453.723106	27.980237
271.844104	12473.558600	27.985255
272.302268	12486.121401	27.990272
272.484129	12508.276821	27.995290
272.497193	12529.659773	28.000308
272.534239	12554.080006	28.005325
273.086928	12573.029031	28.010343
273.344022	12598.368523	28.015360
273.529787	12627.717083	28.020378
273.893508	12644.668431	28.025396
274.450648	12663.080011	28.030413
274.442595	12690.696937	28.035431
274.933422	12706.305278	28.040448
275.228816	12741.194710	28.045466
275.419976	12760.402662	28.050484
275.447398	12776.427863	28.055501
275.553840	12801.993334	28.060519
276.192143	12819.669194	28.065536
276.289899	12843.319236	28.070554
276.653806	12854.337045	28.075572
277.124386	12886.448766	28.080589
277.490028	12901.498982	28.085607
278.875220	12909.426296	28.090624
278.747140	12926.151777	28.095642
279.115570	12920.845651	28.100660
279.479812	12929.918175	28.105677
279.652575	12949.710258	28.110695
279.629218	12943.218120	28.115712
279.758312	12965.271814	28.120730
279.827067	12973.209584	28.125748
280.537545	12985.859511	28.130765
280.441891	13015.094860	28.135783
280.762402	13013.055200	28.140800
280.742835	13033.269082	28.145818
281.215827	13042.147780	28.150836
281.396313	13064.714599	28.155853
281.413547	13081.831144	28.160871
281.808130	13102.450757	28.165888
282.020677	13129.256910	28.170906
282.013787	13146.190974	28.175924
282.218983	13170.127757	28.180941
282.950938	13190.631457	28.185959
283.054417	13208.201984	28.190976
283.380561	13227.051362	28.195994
283.819823	13242.541907	28.201012
284.077743	13265.399999	28.206029
283.822698	13291.101705	28.211047
284.716239	13311.188635	28.216064
284.704309	13346.774711	28.221082
285.036074	13368.531855	28.226100
285.465118	13389.035851	28.231117
285.205625	13414.198403	28.236135
285.718579	13435.756709	28.241152
286.077912	13462.174011	28.246170
286.531820	13482.459469	28.251188
286.852438	13511.087194	28.256205
287.235494	13534.851307	28.261223
287.238866	13543.904864	28.266240
288.141837	13576.025815	28.271258
288.160642	13603.074574	28.276276
288.397423	13615.505432	28.281293
288.726321	13635.936959	28.286311
288.914934	13655.765191	28.291328
289.281804	13680.621546	28.296346
289.902965	13702.456903	28.301364
290.351368	13714.055689	28.306381
290.321045	13739.921756	28.311399
291.210214	13743.310058	28.316416
291.182347	13754.620301	28.321434
291.276809	13772.019070	28.326452
291.788476	13791.253652	28.331469
291.836936	13817.502240	28.336487
292.323773	13824.250602	28.341504
292.522535	13840.720414	28.346522
292.824506	13863.584959	28.351540
293.212546	13871.406770	28.356557
292.959818	13896.306778	28.361575
293.546638	13915.697092	28.366592
293.523944	13926.946623	28.371610
294.025522	13956.086704	28.376628
294.109633	13981.758320	28.381645
294.206829	14003.120278	28.386663
294.614781	14032.846758	28.391680
294.428941	14057.272258	28.396698
294.608110	14089.570623	28.401716
295.458882	14112.358973	28.406733
295.669509	14153.539453	28.411751
296.295385	14166.844524	28.416768
296.692835	14191.223038	28.421786
296.886699	14217.282018	28.426804
297.504664	14230.986299	28.431821
297.471812	14261.265381	28.436839
297.945782	14271.275119	28.441856
298.162068	14297.286483	28.446874
298.316845	14307.864176	28.451892
298.900273	14332.570608	28.456909
298.791418	14360.973181	28.461927
299.175626	14386.342521	28.466944
300.208488	14399.694539	28.471962
300.242539	14419.832014	28.476980
300.934147	14419.581603	28.481997
300.935774	14446.271061	28.487015
301.047936	14455.282744	28.492032
301.235106	14474.808872	28.497050
301.141605	14496.504439	28.502068
301.759267	14507.199224	28.507085
301.734437	14537.294313	28.512103
302.220059	14554.026150	28.517120
302.821738	14574.188565	28.522138
302.820611	14601.886135	28.527156
302.920753	14616.293974	28.532173
303.022537	14642.636407	28.537191
303.671095	14671.066071	28.542208
303.857040	14689.616724	28.547226
303.997996	14720.560956	28.552244
304.057510	14730.282139	28.557261
304.489597	14769.006905	28.562279
304.595488	14791.208470	28.567296
304.944091	14826.083918	28.572314
305.438447	14853.442103	28.577332
306.062689	14875.865759	28.582349
306.424046	14907.101065	28.587367
306.855334	14934.361865	28.592384
307.691522	14945.704849	28.597402
307.599606	14965.082542	28.602420
308.175255	14972.183761	28.607437
308.574305	15002.415311	28.612455
309.111629	15012.655544	28.617472
309.661286	15029.526206	28.622490
309.713658	15037.887453	28.627508
310.401756	15049.440034	28.632525
310.534091	15064.629578	28.637543
310.859330	15074.025067	28.642560
311.219815	15086.446983	28.647578
311.267548	15099.587453	28.652596
311.424965	15112.195952	28.657613
311.661450	15125.490053	28.662631
311.834871	15148.101505	28.667648
312.689839	15162.009363	28.672666
312.205432	15186.609404	28.677684
312.743745	15199.395166	28.682701
312.595539	15214.963554	28.687719
313.391547	15238.987253	28.692736
313.938201	15260.172828	28.697754
314.126207	15282.554757	28.702772
314.486066	15292.810307	28.707789
314.235403	15322.316661	28.712807
314.377036	15350.422481	28.717824
315.360111	15373.276894	28.722842
315.286696	15389.297980	28.727860
315.509949	15414.277001	28.732877
315.980877	15441.819723	28.737895
316.076960	15461.575894	28.742912
316.499495	15491.381321	28.747930
316.681890	15527.348445	28.752948
317.255740	15541.960712	28.757965
317.483896	15572.570509	28.762983
317.706779	15589.508646	28.768000
318.087665	15617.097309	28.773018
318.443445	15649.888616	28.778036
318.704109	15671.217356	28.783053
319.136785	15696.186047	28.788071
319.476260	15714.435708	28.793088
319.692708	15735.673535	28.798106
319.788810	15771.256678	28.803124
319.896982	15783.127952	28.808141
320.265862	15813.946653	28.813159
320.349303	15834.984338	28.818176
320.783650	15870.337809	28.823194
321.535899	15899.425799	28.828212
321.954270	15908.219646	28.833229
322.277515	15934.718668	28.838247
322.358204	15959.761790	28.843264
322.716522	15977.632897	28.848282
322.881587	16012.476088	28.853300
323.703413	16032.321301	28.858317
324.125520	16058.947138	28.863335
324.449435	16086.257982	28.868352
324.469658	16092.906534	28.873370
324.652813	16126.297373	28.878388
325.141892	16131.302746	28.883405
325.396814	16166.062654	28.888423
325.961630	16188.291860	28.893440
326.679438	16207.635562	28.898458
326.715256	16229.609725	28.903476
327.054163	16244.736260	28.908493
327.337741	16261.201188	28.913511
327.139862	16287.782329	28.918528
327.806458	16321.031450	28.923546
328.254566	16334.684891	28.928564
328.405322	16363.646712	28.933581
329.084403	16391.439297	28.938599
329.245229	16420.838657	28.943616
329.837552	16441.453016	28.948634
329.640889	16458.094412	28.953652
329.922745	16484.442750	28.958669
330.429505	16517.132924	28.963687
330.295853	16543.439041	28.968704
331.159545	16570.290156	28.973722
331.319174	16591.370427	28.978740
331.611355	16627.511922	28.983757
332.135119	16638.424761	28.988775
332.330889	16669.322486	28.993792
332.790627	16698.110068	28.998810
332.846119	16724.468925	29.003828
333.277378	16750.623662	29.008845
333.762676	16779.312605	29.013863
333.819878	16805.895562	29.018880
334.289086	16832.256090	29.023898
334.431505	16865.038670	29.028916
334.986665	16892.488156	29.033933
335.436353	16918.665503	29.038951
335.480542	16952.625975	29.043968
336.340355	16976.566054	29.048986
336.717884	17019.735401	29.054004
336.836508	17034.088463	29.059021
337.279511	17053.065447	29.064039
337.421812	17080.946270	29.069056
337.908103	17105.311417	29.074074
338.137668	17129.085087	29.079092
338.309982	17157.390890	29.084109
338.801963	17185.387654	29.089127
339.218739	17203.238108	29.094144
339.578693	17228.406539	29.099162
339.816168	17264.017669	29.104180
340.135097	17276.703364	29.109197
340.822034	17301.732229	29.114215
341.378765	17333.578920	29.119232
341.874440	17351.417153	29.124250
342.031509	17372.277573	29.129268
342.502659	17388.148684	29.134285
342.583349	17410.208762	29.139303
342.334023	17436.970107	29.144320
343.027269	17450.683860	29.149338
343.255029	17485.368273	29.154356
343.867712	17509.297188	29.159373
344.196855	17533.510606	29.164391
344.150237	17557.441777	29.169408
344.344457	17575.175821	29.174426
344.219566	17610.951747	29.179444
345.070011	17631.413234	29.184461
345.534583	17656.597421	29.189479
345.716437	17689.419443	29.194496
346.510399	17712.884313	29.199514
346.686534	17732.706079	29.204532
347.173760	17761.254037	29.209549
347.354286	17773.797485	29.214567
347.571866	17809.987621	29.219584
348.040390	17824.065349	29.224602
348.387404	17854.353753	29.229620
348.593271	17886.319489	29.234637
349.079796	17910.704568	29.239655
349.225340	17938.977801	29.244672
349.541768	17964.842613	29.249690
349.931703	18004.265940	29.254708
350.244607	18027.534893	29.259725
350.597068	18054.013296	29.264743
351.086310	18087.981853	29.269760
351.379270	18124.988366	29.274778
351.794392	18156.277379	29.279796
352.042476	18188.281222	29.284813
352.266060	18200.470735	29.289831
352.488162	18235.991295	29.294848
353.635475	18266.704611	29.299866
353.634663	18312.001953	29.304884
354.018826	18335.759205	29.309901
354.720015	18360.256528	29.314919
354.693601	18398.229643	29.319936
355.172849	18419.836744	29.324954
355.271273	18445.028768	29.329972
355.413375	18477.194994	29.334989
356.381053	18511.120936	29.340007
356.521835	18539.496871	29.345024
357.017965	18568.082527	29.350042
357.372590	18590.688581	29.355060
357.697658	18626.528563	29.360077
358.196995	18644.632758	29.365095
358.308673	18682.768010	29.370112
358.686252	18707.708162	29.375130
358.929630	18734.779493	29.380148
358.866839	18763.396126	29.385165
359.334551	18794.589480	29.390183
359.286454	18831.979284	29.395200
360.354364	18866.578784	29.400218
360.840084	18904.643244	29.405236
361.075777	18941.944581	29.410253
361.265843	18956.875429	29.415271
361.793751	19003.184538	29.420288
362.148424	19030.213575	29.425306
362.530175	19052.398938	29.430324
363.288183	19086.383999	29.435341
363.938373	19114.327176	29.440359
364.323301	19132.310754	29.445376
364.895533	19157.094634	29.450394
365.071389	19177.941412	29.455412
365.326953	19201.024897	29.460429
365.628816	19217.056700	29.465447
366.408277	19245.251485	29.470464
366.448069	19256.510128	29.475482
366.749920	19279.858125	29.480500
367.014068	19307.862050	29.485517
367.535297	19329.400406	29.490535
367.547399	19359.162363	29.495552
367.938884	19376.052134	29.500570
368.095638	19399.302962	29.505588
368.402202	19436.385649	29.510605
368.836368	19465.254001	29.515623
369.051914	19488.843214	29.520640
369.227453	19508.831149	29.525658
370.033766	19535.878593	29.530676
369.807339	19571.661382	29.535693
370.486303	19592.486658	29.540711
370.738032	19631.189399	29.545728
371.193750	19663.062050	29.550746
371.373959	19691.294485	29.555764
371.463486	19737.086423	29.560781
372.079550	19756.797112	29.565799
372.440775	19797.561675	29.570816
372.770653	19830.698973	29.575834
373.267578	19870.001906	29.580852
373.695842	19900.621941	29.585869
374.116708	19931.457999	29.590887
374.489112	19973.459530	29.595904
374.842053	20009.146046	29.600922
375.232660	20039.829060	29.605940
375.939290	20076.547022	29.610957
376.097808	20108.075224	29.615975
376.686665	20147.067357	29.620992
376.915093	20165.708220	29.626010
377.676528	20198.102493	29.631028
377.930266	20233.665956	29.636045
378.601235	20256.173841	29.641063
379.013569	20284.585590	29.646080
378.974376	20308.879108	29.651098
379.598657	20338.148608	29.656116
379.995555	20362.487612	29.661133
380.528361	20390.747961	29.666151
381.005652	20416.186455	29.671168
381.073705	20450.048186	29.676186
381.915705	20464.789612	29.681204
382.472571	20492.970520	29.686221
382.919456	20501.828338	29.691239
383.287530	20534.727065	29.696256
383.471412	20552.421206	29.701274
383.699831	20569.596603	29.706292
383.918570	20595.625524	29.711309
384.149982	20616.250307	29.716327
384.789972	20655.090119	29.721344
384.748620	20679.624530	29.726362
385.263119	20713.435739	29.731380
385.503513	20748.262974	29.736397
385.799216	20779.252656	29.741415
386.195668	20805.367749	29.746432
386.601459	20840.251378	29.751450
387.243323	20866.997864	29.756468
387.223737	20908.039209	29.761485
387.667221	20943.018211	29.766503
388.007100	20966.286439	29.771520
388.123433	21012.949096	29.776538
388.738534	21044.344096	29.781556
389.167799	21069.601404	29.786573
390.089401	21105.327207	29.791591
390.277864	21138.318262	29.796608
390.883814	21176.235614	29.801626
391.202914	21194.970665	29.806644
391.578544	21232.519816	29.811661
391.716308	21252.622857	29.816679
392.082359	21289.819778	29.821696
392.461024	21321.087971	29.826714
393.170727	21346.428080	29.831732
393.259011	21384.439554	29.836749
393.446430	21414.379354	29.841767
393.874194	21450.593846	29.846784
394.222725	21473.949779	29.851802
394.386704	21507.242261	29.856820
394.453900	21548.618867	29.861837
395.041664	21586.912656	29.866855
395.571819	21621.203189	29.871872
395.620427	21671.024705	29.876890
395.749786	21701.940793	29.881908
396.202919	21745.968080	29.886925
396.750982	21782.834121	29.891943
397.073104	21832.215121	29.896960
397.118227	21878.714051	29.901978
397.810878	21916.322261	29.906996
398.077575	21956.689062	29.912013
399.018130	22005.632412	29.917031
399.531210	22036.356222	29.922048
399.733280	22090.615829	29.927066
400.271360	22130.100072	29.932084
400.552411	22178.433123	29.937101
400.909269	22220.113296	29.942119
401.455482	22256.632972	29.947136
401.695071	22300.189429	29.952154
402.479519	22331.149221	29.957172
403.029001	22368.433178	29.962189
403.225697	22416.293466	29.967207
403.963942	22454.540088	29.972224
404.137424	22492.218075	29.977242
404.872515	22524.127424	29.982260
405.086105	22557.932053	29.987277
405.498397	22588.691463	29.992295
406.054662	22636.015717	29.997312
406.062577	22673.732620	30.002330
406.954776	22700.669864	30.007348
407.065341	22746.459164	30.012365
407.828366	22776.348774	30.017383
408.696724	22791.365858	30.022400
408.892271	22834.462777	30.027418
409.387606	22854.840026	30.032436
410.270616	22889.248099	30.037453
410.537194	22910.160443	30.042471
410.823217	22933.357272	30.047488
411.230586	22953.830550	30.052506
412.042929	22970.682764	30.057524
412.316155	22991.170772	30.062541
412.569996	23020.622340	30.067559
412.678605	23043.524813	30.072576
413.184091	23082.864398	30.077594
413.485691	23101.294357	30.082612
413.853652	23133.685574	30.087629
414.135950	23166.273518	30.092647
414.557580	23198.770179	30.097664
414.899868	23237.263586	30.102682
415.357822	23264.238019	30.107700
415.831840	23292.543324	30.112717
416.391111	23327.912831	30.117735
416.821919	23358.360891	30.122752
417.238990	23395.913965	30.127770
417.644776	23424.084802	30.132788
417.902689	23446.692624	30.137805
418.672814	23486.490776	30.142823
419.172743	23508.883821	30.147840
419.099102	23530.861190	30.152858
419.328428	23564.753533	30.157876
420.029779	23600.139184	30.162893
420.352161	23632.999661	30.167911
420.950437	23666.088708	30.172928
421.328876	23688.064951	30.177946
421.855931	23719.914017	30.182964
421.718329	23747.570087	30.187981
422.112586	23776.084471	30.192999
422.589288	23801.843380	30.198016
422.932866	23843.149869	30.203034
423.340732	23875.548680	30.208052
423.447545	23917.284209	30.213069
423.589712	23952.865503	30.218087
424.562671	23979.937181	30.223104
424.547029	24028.314872	30.228122
425.073480	24062.464852	30.233140
425.772524	24098.433137	30.238157
426.117915	24142.128713	30.243175
426.209109	24175.215877	30.248192
426.493597	24229.411520	30.253210
427.281243	24269.625575	30.258228
427.719463	24314.254913	30.263245
427.662950	24359.448446	30.268263
427.959856	24402.324325	30.273280
428.253762	24450.344890	30.278298
429.204117	24491.146903	30.283316
429.921411	24540.188334	30.288333
430.186159	24584.763291	30.293351
431.015359	24624.257434	30.298368
431.218334	24664.342674	30.303386
431.662416	24707.777559	30.308404
431.968887	24741.830440	30.313421
432.309385	24792.119601	30.318439
432.777567	24836.473661	30.323456
433.418546	24888.043132	30.328474
433.803871	24931.898485	30.333492
434.629996	24964.277780	30.338509
434.602955	25009.076333	30.343527
435.440883	25051.527590	30.348544
435.609437	25091.619073	30.353562
436.287159	25131.276975	30.358580
436.508297	25177.730731	30.363597
436.585087	25217.761001	30.368615
437.412851	25266.616268	30.373632
437.795347	25309.284760	30.378650
438.366086	25355.096422	30.383668
439.220275	25384.577509	30.388685
439.435469	25429.200016	30.393703
440.553893	25464.492036	30.398720
440.829428	25502.968650	30.403738
440.883478	25534.863087	30.408756
441.732808	25570.867351	30.413773
441.828576	25608.335857	30.418791
442.557242	25634.519010	30.423808
442.749496	25677.843754	30.428826
443.024905	25704.995425	30.433844
444.553723	25720.644392	30.438861
445.010292	25758.473781	30.443879
445.621569	25786.097513	30.448896
445.357488	25813.371751	30.453914
445.979743	25841.347758	30.458932
446.325486	25871.547519	30.463949
446.042949	25903.773338	30.468967
446.602907	25940.954873	30.473984
447.280946	25987.136687	30.479002
447.514113	26025.431331	30.484020
448.116509	26063.756696	30.489037
448.182001	26104.087535	30.494055
448.864258	26142.059255	30.499072
449.279469	26175.756242	30.504090
449.701166	26221.365692	30.509108
450.009990	26257.209358	30.514125
450.115287	26294.077229	30.519143
450.789396	26329.269715	30.524160
451.079503	26375.740703	30.529178
450.963615	26423.634228	30.534196
451.762055	26461.986523	30.539213
451.723222	26514.924351	30.544231
452.230932	26558.612384	30.549248
452.713606	26601.539683	30.554266
453.173688	26661.339370	30.559284
454.095892	26710.865929	30.564301
454.273489	26756.717065	30.569319
455.024185	26806.074791	30.574336
455.467479	26861.067947	30.579354
456.104156	26899.522251	30.584372
456.478724	26942.037421	30.589389
456.609449	26991.979372	30.594407
457.522613	27040.958282	30.599424
457.933415	27093.808229	30.604442
458.076419	27129.060009	30.609460
458.774938	27176.410600	30.614477
458.926741	27228.170109	30.619495
459.654974	27258.356269	30.624512
460.236769	27318.442207	30.629530
460.278887	27349.759883	30.634548
461.308098	27400.921009	30.639565
461.696754	27449.603828	30.644583
462.080600	27494.608977	30.649600
462.724852	27542.841152	30.654618
463.317646	27579.660279	30.659636
464.029936	27619.671598	30.664653
464.462969	27665.200346	30.669671
464.746153	27705.184234	30.674688
465.476416	27758.384066	30.679706
465.833673	27798.236443	30.684724
466.426912	27818.742447	30.689741
466.318663	27862.283253	30.694759
466.744915	27914.734710	30.699776
467.396889	27956.993647	30.704794
468.081257	28002.471140	30.709812
468.487844	28056.721113	30.714829
468.548315	28107.327829	30.719847
469.244271	28149.801500	30.724864
469.721963	28202.353091	30.729882
469.978438	28244.503909	30.734900
470.825249	28294.608680	30.739917
471.015139	28345.296845	30.744935
471.281263	28381.024523	30.749952
472.017556	28429.080036	30.754970
471.925075	28486.557077	30.759988
473.076286	28534.320299	30.765005
473.396423	28582.371824	30.770023
474.062572	28621.855062	30.775040
474.460321	28674.717467	30.780058
475.124262	28718.840764	30.785076
476.362340	28755.516696	30.790093
476.702138	28793.433229	30.795111
477.077553	28827.690757	30.800128
477.598515	28868.828011	30.805146
478.605079	28897.253709	30.810164
479.086438	28913.777178	30.815181
479.584934	28949.229255	30.820199
479.871972	28980.479460	30.825216
480.443496	29017.260263	30.830234
480.736632	29048.332629	30.835252
481.141042	29070.095739	30.840269
481.299312	29115.613861	30.845287
481.534536	29145.380673	30.850304
481.611805	29182.138049	30.855322
481.986333	29238.355691	30.860340
482.442307	29277.348464	30.865357
482.969945	29327.474148	30.870375
483.046937	29375.729961	30.875392
484.074969	29422.206082	30.880410
483.835403	29470.499055	30.885428
484.657970	29512.367857	30.890445
485.000345	29563.825288	30.895463
485.447853	29615.260059	30.900480
485.857856	29663.831015	30.905498
485.931688	29720.552196	30.910516
486.676876	29765.524700	30.915533
487.254844	29829.790606	30.920551
487.774274	29875.765859	30.925568
488.251622	29936.400497	30.930586
488.688979	29988.842871	30.935604
489.394706	30033.809499	30.940621
489.767304	30095.421847	30.945639
490.167737	30144.703422	30.950656
490.870446	30203.653680	30.955674
491.214664	30257.457771	30.960692
491.436375	30320.497766	30.965709
492.248444	30382.358206	30.970727
492.727719	30434.871003	30.975744
493.008830	30479.949358	30.980762
493.404729	30546.894691	30.985780
494.303399	30605.916547	30.990797
494.930605	30671.947371	30.995815
495.215956	30717.992767	31.000832
495.906942	30771.465735	31.005850
496.287040	30826.688027	31.010868
497.023979	30878.371400	31.015885
497.639396	30938.822989	31.020903
498.220778	30992.256799	31.025920
498.814847	31040.915949	31.030938
499.246927	31091.307421	31.035956
499.799231	31137.684913	31.040973
500.391503	31193.380679	31.045991
500.974287	31250.892400	31.051008
501.555143	31286.518921	31.056026
502.080653	31346.163960	31.061044
502.605334	31383.866641	31.066061
502.877243	31432.792105	31.071079
503.515149	31495.504969	31.076096
503.918575	31543.152067	31.081114
504.233087	31596.129810	31.086132
505.219913	31632.995625	31.091149
505.778020	31677.672853	31.096167
506.213991	31724.177345	31.101184
506.945386	31762.569022	31.106202
507.365108	31813.684868	31.111220
507.913984	31860.102439	31.116237
508.234557	31902.686890	31.121255
509.048686	31954.139584	31.126272
509.667599	31994.806219	31.131290
509.925837	32034.189180	31.136308
510.414898	32079.668323	31.141325
511.143948	32115.917889	31.146343
511.200619	32172.231205	31.151360
511.889194	32225.069773	31.156378
512.521484	32267.321657	31.161396
512.953501	32300.311674	31.166413
513.148780	32351.476634	31.171431
513.329270	32404.755588	31.176448
514.371031	32452.861124	31.181466
514.309371	32512.392836	31.186484
515.084633	32563.530696	31.191501
515.407774	32611.306605	31.196519
515.731736	32658.298554	31.201536
516.032825	32716.705598	31.206554
516.153503	32773.320288	31.211572
516.916647	32823.392241	31.216589
517.212756	32884.468476	31.221607
517.318053	32939.233630	31.226624
518.366748	32997.119743	31.231642
518.846776	33060.709208	31.236660
519.083642	33120.549934	31.241677
519.916417	33169.138727	31.246695
520.251535	33238.466739	31.251712
521.167984	33299.099297	31.256730
521.414682	33363.744112	31.261748
522.159514	33422.159486	31.266765
522.842897	33487.608768	31.271783
523.342022	33542.212652	31.276800
524.165546	33581.876681	31.281818
524.878922	33648.295412	31.286836
525.052786	33698.114015	31.291853
525.814659	33748.226309	31.296871
526.289305	33821.334163	31.301888
527.426328	33853.729376	31.306906
528.348474	33907.332231	31.311924
528.655672	33944.125219	31.316941
529.407013	33983.573703	31.321959
529.899943	34035.581294	31.326976
530.355118	34073.407190	31.331994
530.704964	34111.603713	31.337012
530.917113	34159.539619	31.342029
531.785828	34205.450744	31.347047
531.900561	34264.966108	31.352064
532.279383	34315.171358	31.357082
533.235686	34365.311572	31.362100
533.319711	34417.150209	31.367117
533.978596	34487.044913	31.372135
534.170838	34542.616236	31.377152
534.784891	34597.034139	31.382170
535.046016	34662.907274	31.387188
535.654887	34720.829081	31.392205
536.487595	34780.429448	31.397223
536.788582	34842.977467	31.402240
537.579575	34911.771693	31.407258
537.791777	34975.497397	31.412276
538.124536	35035.878615	31.417293
538.600824	35096.755996	31.422311
539.261641	35166.690577	31.427328
539.840598	35226.957905	31.432346
540.143647	35290.113912	31.437364
540.718668	35350.533956	31.442381
541.511590	35418.937505	31.447399
541.590494	35493.902502	31.452416
542.295670	35550.249724	31.457434
542.922381	35618.035003	31.462452
543.463431	35692.763922	31.467469
544.364564	35749.068334	31.472487
544.550267	35822.892266	31.477504
545.470014	35888.330925	31.482522
546.024140	35947.655725	31.487540
546.535250	36008.890679	31.492557
547.138420	36070.566654	31.497575
547.285931	36146.098603	31.502592
548.178719	36207.969895	31.507610
549.276594	36259.268522	31.512628
550.127966	36319.009392	31.517645
550.502634	36367.297893	31.522663
551.250143	36412.012403	31.527680
551.860095	36455.863298	31.532698
552.672476	36512.057163	31.537716
553.299419	36556.272352	31.542733
553.688598	36592.291976	31.547751
553.921169	36633.780530	31.552768
554.295692	36693.963884	31.557786
554.739169	36738.138627	31.562804
555.484858	36789.961615	31.567821
555.898030	36835.519790	31.572839
556.087447	36894.645084	31.577856
556.682863	36940.560665	31.582874
557.599684	36993.944510	31.587892
557.625339	37051.382247	31.592909
558.492133	37109.542062	31.597927
558.871747	37158.274212	31.602944
559.296195	37218.210928	31.607962
559.889786	37272.088732	31.612980
560.727815	37339.296235	31.617997
561.338851	37401.645106	31.623015
561.640420	37457.535722	31.628032
562.004364	37515.731128	31.633050
562.866600	37582.189423	31.638068
563.539446	37627.386109	31.643085
564.143127	37682.572342	31.648103
564.458370	37749.755505	31.653120
565.299244	37803.589590	31.658138
565.722468	37860.853397	31.663156
566.278119	37921.973018	31.668173
566.894913	37982.286452	31.673191
567.429230	38043.156811	31.678208
567.938380	38106.288849	31.683226
568.349140	38168.747194	31.688244
569.014622	38235.579803	31.693261
569.559371	38295.772599	31.698279
569.946156	38359.828842	31.703296
570.082613	38434.763484	31.708314
571.214192	38509.915638	31.713332
571.356520	38568.388900	31.718349
572.226601	38640.281415	31.723367
572.786137	38709.124101	31.728384
572.882559	38783.003805	31.733402
573.752979	38846.935153	31.738420
573.849365	38939.344514	31.743437
574.825132	38989.625341	31.748455
575.457247	39064.857649	31.753472
576.262537	39141.024345	31.758490
577.313517	39191.148409	31.763508
578.133427	39263.417645	31.768525
579.146678	39310.031722	31.773543
579.615130	39379.504237	31.778560
580.069675	39439.872444	31.783578
580.837081	39484.526984	31.788596
581.252562	39545.761683	31.793613
582.073701	39589.421459	31.798631
582.112191	39654.687070	31.803648
582.718381	39717.429157	31.808666
583.212256	39771.701939	31.813684
584.040035	39842.024016	31.818701
584.224208	39898.394665	31.823719
584.179391	39974.444455	31.828736
585.209774	40029.791194	31.833754
585.747913	40103.302640	31.838772
586.418575	40168.059701	31.843789
586.924196	40234.493453	31.848807
587.575606	40302.561555	31.853824
588.065253	40369.181625	31.858842
588.722685	40435.516320	31.863860
589.535514	40513.893855	31.868877
590.018757	40571.870076	31.873895
590.463582	40639.282219	31.878912
590.789572	40701.811718	31.883930
591.651154	40753.537515	31.888948
591.926834	40834.694555	31.893965
592.486705	40887.536763	31.898983
593.191970	40958.267419	31.904000
593.442520	41024.433616	31.909018
594.182769	41093.034177	31.914036
594.500763	41165.989162	31.919053
595.020439	41221.102677	31.924071
596.053335	41304.603140	31.929088
596.338890	41374.610292	31.934106
596.851136	41440.730434	31.939124
597.773109	41522.851346	31.944141
598.596679	41591.421442	31.949159
599.409118	41662.510742	31.954176
599.569553	41729.041035	31.959194
600.523645	41798.900563	31.964212
600.490416	41881.823865	31.969229
600.856632	41944.654194	31.974247
601.923220	42027.380499	31.979264
602.294607	42107.780917	31.984282
603.252824	42175.857381	31.989300
603.467190	42251.741644	31.994317
604.192561	42326.995869	31.999335
604.679975	42408.049652	32.004352
605.204265	42486.624890	32.009370
606.080751	42570.072426	32.014388
606.278158	42658.414675	32.019405
607.340486	42734.699096	32.024423
608.219267	42809.285782	32.029440
608.794009	42891.308046	32.034458
609.674977	42959.816481	32.039476
609.890401	43043.476860	32.044493
610.278656	43120.658823	32.049511
611.038225	43200.989769	32.054528
611.545332	43276.186526	32.059546
612.506765	43359.826141	32.064564
613.084214	43429.591682	32.069581
614.009548	43496.140326	32.074599
615.153238	43558.777572	32.079616
616.394274	43618.660894	32.084634
617.352120	43667.019723	32.089652
617.878805	43721.986574	32.094669
618.476075	43782.198871	32.099687
619.221310	43832.444685	32.104704
619.748619	43890.897131	32.109722
620.190070	43943.739901	32.114740
621.058945	43990.601599	32.119757
621.956546	44041.848741	32.124775
622.604863	44094.887187	32.129792
622.784478	44153.160733	32.134810
623.231256	44209.532902	32.139828
623.826565	44265.546702	32.144845
624.175256	44326.166277	32.149863
624.816942	44387.758539	32.154880
625.304922	44453.625805	32.159898
625.580909	44514.529276	32.164916
625.661351	44590.815708	32.169933
626.589095	44664.692488	32.174951
627.435712	44738.955429	32.179968
627.692170	44810.584691	32.184986
628.134174	44891.559753	32.190004
628.973780	44956.241137	32.195021
629.268736	45039.333562	32.200039
630.096762	45108.293375	32.205056
630.754198	45178.791969	32.210074
630.949362	45248.496551	32.215092
631.842668	45328.181639	32.220109
632.675460	45404.808470	32.225127
633.255504	45474.238399	32.230144
633.519745	45548.354846	32.235162
634.248483	45614.111907	32.240180
634.686827	45698.145845	32.245197
635.400585	45768.536254	32.250215
635.866478	45838.700013	32.255232
636.406181	45921.845933	32.260250
637.579233	45988.299945	32.265268
638.165045	46054.384323	32.270285
638.747698	46127.219240	32.275303
639.801666	46193.547009	32.280320
640.410864	46281.579719	32.285338
640.760196	46348.714162	32.290356
641.477005	46431.087747	32.295373
642.325916	46503.907486	32.300391
643.347761	46559.373099	32.305408
643.611834	46639.439720	32.310426
644.489750	46710.522217	32.315444
645.224290	46779.792796	32.320461
645.459904	46856.663589	32.325479
646.194032	46931.919297	32.330496
646.941647	47021.432526	32.335514
647.252261	47084.437842	32.340532
647.823556	47163.300492	32.345549
648.299474	47237.528507	32.350567
649.027673	47309.205698	32.355584
649.651237	47401.207126	32.360602
650.106931	47485.403145	32.365620
650.422042	47571.633292	32.370637
651.002684	47661.883753	32.375655
651.512791	47751.493993	32.380672
652.403883	47849.123845	32.385690
652.981071	47934.270450	32.390708
653.604345	48029.026493	32.395725
654.215393	48125.910571	32.400743
655.385707	48206.656914	32.405760
656.087972	48310.075509	32.410778
656.943997	48387.271866	32.415796
657.708002	48474.156361	32.420813
657.945433	48556.018016	32.425831
658.588713	48642.150199	32.430848
659.141007	48723.014135	32.435866
660.125849	48806.720923	32.440884
661.114602	48888.200379	32.445901
662.154389	48979.712766	32.450919
662.463347	49061.976268	32.455936
663.270182	49145.275620	32.460954
664.048289	49231.926688	32.465972
664.537092	49299.370655	32.470989
665.021870	49398.487977	32.476007
665.777987	49482.321628	32.481024
666.255760	49562.814250	32.486042
666.872907	49647.157442	32.491060
667.767224	49726.465527	32.496077
668.868086	49807.570050	32.501095
669.570714	49882.024225	32.506112
670.157025	49973.516681	32.511130
670.985953	50047.489735	32.516148
671.828921	50125.598760	32.521165
672.025409	50199.627055	32.526183
673.181265	50279.883120	32.531200
673.403973	50354.730336	32.536218
674.319857	50434.347511	32.541236
674.967839	50515.057234	32.546253
675.284301	50602.545019	32.551271
676.329785	50672.088723	32.556288
676.802807	50756.559775	32.561306
677.668687	50823.259471	32.566324
678.192744	50905.312369	32.571341
678.583833	50968.543534	32.576359
679.253851	51051.599121	32.581376
679.770053	51131.331904	32.586394
680.516529	51200.639289	32.591412
681.244432	51273.170451	32.596429
682.045401	51355.055024	32.601447
682.759718	51421.267653	32.606464
683.904986	51498.353211	32.611482
684.526889	51570.300789	32.616500
684.891922	51640.143784	32.621517
685.698336	51725.774708	32.626535
686.515258	51790.827033	32.631552
686.797082	51878.483235	32.636570
687.413438	51971.851838	32.641588
688.044856	52044.122098	32.646605
688.270900	52131.237479	32.651623
688.932585	52204.402023	32.656640
690.418986	52292.984812	32.661658
690.956217	52375.825465	32.666676
691.891069	52456.769094	32.671693
692.555984	52550.132404	32.676711
693.172642	52619.312471	32.681728
693.972953	52706.485602	32.686746
694.258144	52789.152041	32.691764
695.495787	52879.649051	32.696781
695.503812	52966.839650	32.701799
696.405230	53052.416261	32.706816
696.931275	53152.081003	32.711834
697.475480	53241.631238	32.716852
698.488410	53318.117058	32.721869
698.647501	53424.478474	32.726887
699.323392	53505.390341	32.731904
700.203894	53613.506406	32.736922
700.434750	53705.208391	32.741940
701.495294	53793.458544	32.746957
702.006127	53904.677656	32.751975
702.891694	53992.810410	32.756992
703.641685	54103.391830	32.762010
704.703818	54186.783154	32.767028
705.665956	54281.169927	32.772045
706.184787	54372.981284	32.777063
706.902620	54462.850690	32.782080
707.413773	54561.435250	32.787098
708.353663	54667.698972	32.792116
709.029282	54751.804635	32.797133
709.694744	54844.632709	32.802151
710.650169	54931.448042	32.807168
711.416068	55023.166270	32.812186
711.888502	55102.989002	32.817204
712.927190	55202.866890	32.822221
713.334022	55302.211295	32.827239
713.989667	55392.796426	32.832256
714.990880	55483.878369	32.837274
715.169564	55587.177070	32.842292
716.275468	55678.958495	32.847309
716.726019	55781.095296	32.852327
717.497686	55876.366274	32.857344
718.635757	55963.555476	32.862362
719.466037	56055.457457	32.867380
720.363507	56133.274163	32.872397
720.672979	56227.182298	32.877415
721.521480	56326.911143	32.882432
721.934721	56412.620637	32.887450
723.131193	56506.359318	32.892468
723.672633	56588.714073	32.897485
723.979785	56683.409135	32.902503
724.605106	56761.688208	32.907520
725.302104	56856.430494	32.912538
725.914650	56952.964813	32.917556
726.851197	57035.176949	32.922573
727.102763	57139.667103	32.927591
727.688112	57232.181559	32.932608
728.680978	57323.784462	32.937626
728.845330	57422.700953	32.942644
730.024701	57512.496898	32.947661
730.318850	57618.615366	32.952679
731.431040	57715.625131	32.957696
731.971004	57822.035114	32.962714
732.511747	57928.610002	32.967732
733.596135	58033.131834	32.972749
734.327614	58129.443373	32.977767
735.181672	58226.780430	32.982784
736.037737	58324.408712	32.987802
736.821337	58428.200849	32.992820
737.688549	58533.195574	32.997837
738.081019	58627.872241	33.002855
739.127428	58727.219248	33.007872
740.011993	58823.737430	33.012890
740.720515	58938.518753	33.017908
741.848981	59034.037496	33.022925
742.053099	59129.498820	33.027943
743.547030	59222.359641	33.032960
744.613352	59302.134944	33.037978
745.269179	59384.854752	33.042996
746.723999	59477.361885	33.048013
747.156785	59571.364968	33.053031
747.810899	59653.231454	33.058048
748.563471	59739.697129	33.063066
749.136472	59829.121880	33.068084
749.721374	59929.122062	33.073101
750.405965	60014.073889	33.078119
751.347553	60113.525248	33.083136
751.866448	60207.200800	33.088154
752.280527	60306.419058	33.093172
753.543564	60386.445610	33.098189
753.961365	60493.266182	33.103207
754.587491	60587.331504	33.108224
755.666049	60683.155685	33.113242
756.132033	60789.007848	33.118260
756.991630	60884.069527	33.123277
757.222118	60986.984333	33.128295
758.103225	61088.018947	33.133312
759.153148	61186.584142	33.138330
759.713145	61296.930759	33.143348
760.566119	61395.388368	33.148365
760.739534	61508.904548	33.153383
761.520079	61614.729985	33.158400
761.988451	61724.434522	33.163418
762.826660	61841.703208	33.168436
763.722958	61945.068467	33.173453
764.673679	62053.464530	33.178471
765.265008	62161.771749	33.183488
766.098441	62274.871566	33.188506
766.747456	62398.015400	33.193524
767.603852	62503.877067	33.198541
768.145599	62629.722928	33.203559
768.811839	62738.198179	33.208576
769.693183	62847.039037	33.213594
770.447239	62979.709321	33.218612
771.359801	63091.876205	33.223629
771.890801	63208.730985	33.228647
772.925165	63321.816751	33.233664
773.964085	63434.826349	33.238682
774.261558	63550.358211	33.243700
775.408700	63643.752123	33.248717
776.313906	63747.047496	33.253735
776.738572	63854.432225	33.258752
777.749056	63947.867663	33.263770
778.410083	64065.123906	33.268788
778.805671	64174.382136	33.273805
779.827657	64286.948740	33.278823
780.856959	64395.209715	33.283840
782.688601	64471.640443	33.288858
784.261035	64557.279140	33.293876
785.758379	64626.380856	33.298893
786.648241	64708.898186	33.303911
787.229599	64787.013430	33.308928
787.842012	64864.908800	33.313946
788.732812	64943.419241	33.318964
789.293223	65013.162554	33.323981
790.083745	65094.557119	33.328999
790.276791	65186.934928	33.334016
791.379457	65263.330268	33.339034
791.544936	65367.438215	33.344052
792.210000	65454.804824	33.349069
792.739815	65552.670968	33.354087
793.294434	65659.808781	33.359104
794.061048	65750.807268	33.364122
794.656265	65857.122830	33.369140
795.501302	65964.051838	33.374157
796.357385	66088.865440	33.379175
796.405052	66196.534420	33.384192
797.139048	66319.272605	33.389210
797.982863	66441.563651	33.394228
798.788139	66551.977277	33.399245
799.652200	66674.620828	33.404263
800.221093	66795.804302	33.409280
801.096909	66919.878099	33.414298
801.508613	67052.882976	33.419316
802.323271	67170.781668	33.424333
803.189141	67292.851728	33.429351
804.209927	67429.156909	33.434368
804.706068	67556.623674	33.439386
805.384744	67682.194642	33.444404
806.070010	67807.486596	33.449421
806.926324	67943.117438	33.454439
807.651797	68086.000372	33.459456
808.198431	68214.792162	33.464474
809.177394	68360.017681	33.469492
809.735182	68490.582017	33.474509
811.138073	68627.371915	33.479527
811.598762	68767.760987	33.484544
812.825900	68901.065625	33.489562
813.777104	69047.705051	33.494580
815.078650	69164.605815	33.499597
816.085994	69291.399547	33.504615
816.836287	69413.516733	33.509632
818.973051	69515.692801	33.514650
819.695014	69637.758487	33.519668
820.908600	69740.250967	33.524685
822.084193	69837.076142	33.529703
822.724493	69942.825293	33.534720
823.685476	70053.248521	33.539738
824.167360	70147.017345	33.544756
825.276934	70249.984041	33.549773
825.837621	70343.905873	33.554791
826.363658	70455.981993	33.559808
827.424245	70552.067948	33.564826
828.247606	70658.386572	33.569844
828.619351	70769.145722	33.574861
829.717852	70861.642720	33.579879
830.310999	70973.203946	33.584896
831.570746	71068.627361	33.589914
832.499855	71163.798936	33.594932
833.408341	71252.084272	33.599949
834.428439	71346.267048	33.604967
834.762778	71433.857660	33.609984
836.241720	71518.229679	33.615002
836.877040	71612.119031	33.620020
837.726649	71701.706953	33.625037
838.760931	71782.185204	33.630055
839.327389	71872.818607	33.635072
840.119187	71956.831010	33.640090
840.806629	72054.830041	33.645108
841.532837	72150.100278	33.650125
842.204046	72243.606289	33.655143
842.876425	72347.675573	33.660160
843.846456	72450.533416	33.665178
844.267814	72557.999235	33.670196
844.707242	72678.331086	33.675213
845.561149	72780.891748	33.680231
846.353747	72905.057733	33.685248
847.064323	73021.320927	33.690266
847.669010	73149.899894	33.695284
848.253234	73277.279410	33.700301
849.026127	73390.152616	33.705319
849.734891	73522.098934	33.710336
850.446548	73659.441269	33.715354
851.332251	73799.492979	33.720372
852.387349	73925.763217	33.725389
853.622336	74044.355360	33.730407
854.840047	74175.161224	33.735424
855.418501	74304.674505	33.740442
856.433192	74427.115468	33.745460
857.215289	74551.316075	33.750477
858.565467	74665.725596	33.755495
859.187137	74799.541178	33.760512
860.416511	74917.416049	33.765530
861.224679	75042.818192	33.770548
861.951347	75163.990249	33.775565
862.963275	75283.864149	33.780583
863.586786	75412.311669	33.785600
864.539582	75519.769483	33.790618
865.436090	75656.409043	33.795636
866.063951	75794.231410	33.800653
866.958186	75906.196800	33.805671
867.572123	76043.503253	33.810688
868.576585	76173.212133	33.815706
869.248448	76301.732297	33.820724
869.827311	76447.723510	33.825741
871.294983	76573.257480	33.830759
872.037971	76702.718469	33.835776
872.996579	76836.909377	33.840794
873.825991	76968.524277	33.845812
874.101321	77107.219225	33.850829
875.074821	77244.754117	33.855847
876.071377	77379.613145	33.860864
877.105555	77522.219790	33.865882
878.116777	77652.707388	33.870900
878.733512	77784.068138	33.875917
879.810471	77918.106459	33.880935
880.580360	78070.372520	33.885952
881.634713	78194.179741	33.890970
882.723181	78318.564922	33.895988
883.877626	78452.897755	33.901005
884.696189	78586.536390	33.906023
885.758081	78713.803273	33.911040
886.413351	78832.215679	33.916058
887.580837	78954.272987	33.921076
888.288472	79096.102768	33.926093
889.374819	79202.882675	33.931111
890.140480	79331.440323	33.936128
891.091742	79444.399386	33.941146
892.455990	79554.823791	33.946164
892.827528	79677.034246	33.951181
893.621939	79776.932109	33.956199
894.445916	79914.883780	33.961216
895.229754	80035.941702	33.966234
896.302231	80152.913464	33.971252
896.948142	80276.363175	33.976269
898.101206	80404.180967	33.981287
898.582770	80517.927407	33.986304
899.583285	80649.431667	33.991322
900.728008	80788.376320	33.996340
901.292045	80916.504060	34.001357
902.278370	81035.140043	34.006375
902.864655	81175.973143	34.011392
904.019412	81311.231923	34.016410
904.919219	81448.127673	34.021428
905.116348	81582.080666	34.026445
906.330998	81724.439863	34.031463
907.203366	81863.343775	34.036480
907.917465	82009.178347	34.041498
908.855626	82142.080375	34.046516
909.567705	82290.248016	34.051533
910.589758	82440.724567	34.056551
911.503771	82597.009180	34.061568
912.071870	82752.778646	34.066586
913.202874	82893.091529	34.071604
913.768232	83056.503384	34.076621
915.180704	83204.135318	34.081639
916.478844	83356.828850	34.086656
917.046245	83510.587923	34.091674
918.097735	83655.174375	34.096692
919.398734	83801.762501	34.101709
920.662665	83935.635555	34.106727
921.127493	84086.423434	34.111744
921.811679	84229.841206	34.116762
923.109403	84383.465260	34.121780
923.779031	84533.222392	34.126797
924.731281	84679.831589	34.131815
925.912568	84834.566008	34.136832
926.632788	84990.678603	34.141850
927.706225	85132.341946	34.146868
928.681184	85292.065662	34.151885
929.419060	85434.822091	34.156903
930.522535	85594.717425	34.161920
931.461898	85747.821942	34.166938
932.222954	85891.121867	34.171956
933.289322	86037.099143	34.176973
934.428964	86180.619996	34.181991
936.346112	86318.317425	34.187008
937.630099	86453.605578	34.192026
938.197988	86577.284791	34.197044
939.347287	86720.908165	34.202061
940.461036	86844.034167	34.207079
941.353391	86985.456088	34.212096
942.450897	87121.308761	34.217114
943.799843	87243.322465	34.222132
944.255277	87380.341348	34.227149
945.272130	87501.622431	34.232167
946.033812	87629.597054	34.237184
947.001050	87764.966194	34.242202
948.147681	87894.681204	34.247220
948.897192	88029.819523	34.252237
949.588080	88163.066721	34.257255
950.585413	88293.339113	34.262272
951.109306	88425.954654	34.267290
952.205050	88551.257672	34.272308
952.519562	88684.566144	34.277325
953.461259	88817.320783	34.282343
954.366632	88957.356069	34.287360
955.083585	89103.466620	34.292378
955.805410	89230.377173	34.297396
956.495381	89384.870333	34.302413
957.634510	89522.831274	34.307431
958.672745	89667.741006	34.312448
959.135002	89827.759698	34.317466
960.490090	89972.152374	34.322484
961.503644	90123.873871	34.327501
962.206158	90268.813726	34.332519
963.557554	90427.948654	34.337536
964.321026	90575.301125	34.342554
965.723046	90729.144745	34.347572
966.072447	90887.792620	34.352589
967.205199	91041.211055	34.357607
968.532436	91196.691038	34.362624
969.375494	91339.776293	34.367642
970.153344	91494.558027	34.372660
971.396064	91653.500965	34.377677
972.029904	91803.376538	34.382695
973.466836	91962.366729	34.387712
974.109524	92130.696429	34.392730
975.025204	92288.616561	34.397748
975.753298	92445.743032	34.402765
976.757165	92613.144294	34.407783
978.289350	92772.275887	34.412800
979.437129	92937.096096	34.417818
980.423999	93093.792456	34.422836
980.969552	93259.849425	34.427853
982.037563	93420.768170	34.432871
983.478383	93576.014339	34.437888
984.065577	93734.094742	34.442906
985.093231	93897.037633	34.447924
986.398849	94051.711632	34.452941
987.466769	94220.189002	34.457959
988.847610	94378.465319	34.462976
989.611435	94536.953129	34.467994
990.564817	94694.917724	34.473012
991.455209	94848.950882	34.478029
992.312538	95010.608032	34.483047
993.472400	95166.932888	34.488064
994.241521	95339.392570	34.493082
995.370966	95503.227925	34.498100
996.377427	95659.642642	34.503117
996.932197	95830.604807	34.508135
998.012102	95988.150501	34.513152
998.897921	96164.741513	34.518170
1000.036109	96341.268651	34.523188
1000.833600	96509.965500	34.528205
1001.819312	96680.839459	34.533223
1003.490327	96838.094034	34.538240
1003.855329	97022.072977	34.543258
1005.312690	97181.162765	34.548276
1006.131534	97343.344992	34.553293
1006.923339	97510.133900	34.558311
1008.059613	97679.836098	34.563328
1008.964899	97858.043451	34.568346
1010.873699	98017.016036	34.573364
1012.191236	98175.765063	34.578381
1013.173590	98331.968581	34.583399
1013.885117	98492.436714	34.588416
1014.777703	98665.985414	34.593434
1015.929278	98818.095460	34.598452
1017.262189	98984.896085	34.603469
1017.972197	99141.551856	34.608487
1019.054792	99284.078205	34.613504
1019.832582	99439.000691	34.618522
1020.790849	99592.691305	34.623540
1021.676022	99741.551282	34.628557
1022.781244	99897.388191	34.633575
1023.934213	100045.092009	34.638592
1025.365573	100183.358743	34.643610
1026.665686	100338.013587	34.648628
1027.815841	100473.752002	34.653645
1028.759121	100624.800193	34.658663
1029.893112	100769.657757	34.663680
1030.416376	100928.126306	34.668698
1031.581654	101071.103967	34.673716
1032.142397	101225.194166	34.678733
1032.766501	101388.111842	34.683751
1033.696810	101543.210639	34.688768
1034.459789	101719.711948	34.693786
1035.297500	101888.760311	34.698804
1037.006287	102057.153347	34.703821
1037.639481	102230.330610	34.708839
1039.159767	102392.352238	34.713856
1039.979590	102566.668470	34.718874
1041.200385	102727.407375	34.723892
1042.021886	102895.804136	34.728909
1042.871328	103078.042629	34.733927
1044.432804	103236.093467	34.738944
1045.462455	103411.243443	34.743962
1046.578845	103585.062143	34.748980
1047.626906	103753.110793	34.753997
1048.976325	103914.481924	34.759015
1050.021966	104078.361156	34.764032
1050.903710	104253.310474	34.769050
1051.820271	104417.160852	34.774068
1053.380396	104599.156895	34.779085
1054.259546	104762.545675	34.784103
1055.641545	104923.409374	34.789120
1056.876798	105089.875825	34.794138
1057.539058	105258.436185	34.799156
1058.574881	105435.168018	34.804173
1059.371333	105600.463067	34.809191
1060.809504	105764.403150	34.814208
1061.746821	105953.553967	34.819226
1062.542536	106116.480500	34.824244
1063.675543	106289.562412	34.829261
1064.757268	106461.499344	34.834279
1066.006381	106633.512374	34.839296
1066.496149	106818.743805	34.844314
1067.508174	106999.278849	34.849332
1068.580408	107185.511569	34.854349
1069.473843	107374.284011	34.859367
1070.151982	107552.934128	34.864384
1071.282950	107757.737648	34.869402
1072.436681	107939.409358	34.874420
1073.566278	108120.299597	34.879437
1074.355191	108323.625651	34.884455
1075.689025	108518.295338	34.889472
1076.665150	108692.834127	34.894490
1078.070011	108887.088966	34.899508
1079.489622	109070.373482	34.904525
1079.836474	109276.386590	34.909543
1081.250158	109455.628779	34.914560
1082.469808	109654.951300	34.919578
1083.236785	109852.304129	34.924596
1084.540003	110035.599228	34.929613
1085.695108	110231.054612	34.934631
1086.936166	110421.627917	34.939648
1087.609605	110611.542901	34.944666
1088.763225	110803.552287	34.949684
1089.756380	110990.236147	34.954701
1090.662670	111181.500029	34.959719
1091.891319	111359.943842	34.964736
1092.996911	111543.899082	34.969754
1093.541076	111733.282280	34.974772
1094.928842	111930.574828	34.979789
1095.686761	112120.332430	34.984807
1096.968413	112312.507431	34.989824
1098.103338	112513.190859	34.994842
1099.168614	112705.110137	34.999860
1100.309567	112892.047089	35.004877
1100.949820	113093.343845	35.009895
1102.296241	113285.628025	35.014912
1103.265912	113485.429573	35.019930
1104.363787	113695.726082	35.024948
1105.714207	113890.828388	35.029965
1106.981470	114094.277362	35.034983
1108.081534	114303.258014	35.040000
1109.093526	114504.149239	35.045018
1110.196776	114710.658537	35.050036
1111.530345	114905.971815	35.055053
1112.224669	115120.182651	35.060071
1113.474857	115323.438171	35.065088
1114.440625	115535.909366	35.070106
1115.631532	115750.134888	35.075124
1116.824722	115954.214527	35.080141
1117.775899	116175.240309	35.085159
1119.297223	116387.781598	35.090176
1120.490878	116594.426756	35.095194
1121.738492	116799.504507	35.100212
1123.329662	117002.436767	35.105229
1124.399363	117207.772910	35.110247
1125.695407	117408.178738	35.115264
1127.316379	117607.976665	35.120282
1128.459598	117810.983410	35.125300
1129.935377	117998.553317	35.130317
1130.833072	118184.616443	35.135335
1132.277104	118378.027929	35.140352
1133.778659	118579.980633	35.145370
1134.535496	118777.421189	35.150388
1135.578586	118966.801370	35.155405
1136.766424	119157.745394	35.160423
1137.865403	119344.734004	35.165440
1139.161612	119542.423861	35.170458
1139.716416	119734.522681	35.175476
1140.856464	119935.854148	35.180493
1142.109193	120140.035800	35.185511
1143.563616	120339.112988	35.190528
1144.434606	120536.532010	35.195546
1145.382491	120737.326902	35.200564
1146.478129	120936.704338	35.205581
1147.332777	121148.754953	35.210599
1148.323366	121347.275653	35.215616
1149.290186	121555.023299	35.220634
1150.417759	121781.432439	35.225652
1151.711338	121987.152295	35.230669
1152.755308	122193.927144	35.235687
1153.739332	122409.084943	35.240704
1155.428567	122622.712718	35.245722
1156.423734	122842.742419	35.250740
1157.325866	123047.767929	35.255757
1158.589978	123266.019915	35.260775
1160.090405	123487.471011	35.265792
1161.452331	123688.406394	35.270810
1162.751935	123899.894654	35.275828
1163.813039	124107.412550	35.280845
1165.169451	124307.806394	35.285863
1166.391831	124495.523285	35.290880
1167.642697	124693.893085	35.295898
1168.387652	124890.427417	35.300916
1169.744740	125078.772930	35.305933
1171.071429	125270.663606	35.310951
1172.100100	125460.470502	35.315968
1173.141206	125654.272616	35.320986
1174.405212	125855.310213	35.326004
1176.091422	126040.069065	35.331021
1176.869353	126225.846328	35.336039
1177.948104	126430.544167	35.341056
1179.106028	126621.173537	35.346074
1179.838436	126827.830604	35.351092
1181.092186	127032.681652	35.356109
1182.441078	127234.169425	35.361127
1183.569725	127446.375241	35.366144
1184.594105	127640.176620	35.371162
1185.608433	127848.926086	35.376180
1187.098173	128052.159300	35.381197
1188.384549	128262.492221	35.386215
1189.297818	128476.157972	35.391232
1190.666235	128675.759209	35.396250
1191.526240	128906.398710	35.401268
1192.636292	129123.183459	35.406285
1193.714349	129335.926941	35.411303
1194.704338	129555.130673	35.416320
1196.376781	129766.514484	35.421338
1197.337192	129993.655014	35.426356
1199.160398	130204.611380	35.431373
1200.963267	130418.376029	35.436391
1202.057174	130633.115520	35.441408
1203.357882	130833.092742	35.446426
1204.362899	131058.100310	35.451444
1205.754513	131252.457044	35.456461
1207.256824	131463.190672	35.461479
1208.570661	131678.763739	35.466496
1209.722966	131878.451811	35.471514
1210.789616	132093.976810	35.476532
1212.007848	132299.239443	35.481549
1213.030567	132509.190383	35.486567
1213.787587	132731.961462	35.491584
1215.257342	132946.780423	35.496602
1216.159219	133172.754005	35.501620
1217.449697	133392.539164	35.506637
1218.733245	133605.956631	35.511655
1220.037543	133835.182416	35.516672
1221.065687	134057.638562	35.521690
1222.284732	134281.664768	35.526708
1223.380702	134506.333133	35.531725
1224.425542	134740.235744	35.536743
1225.728849	134975.406114	35.541760
1226.864350	135185.669261	35.546778
1227.798218	135428.335823	35.551796
1228.829368	135670.290529	35.556813
1230.093020	135900.840226	35.561831
1231.174359	136139.794820	35.566848
1232.403812	136384.501316	35.571866
1233.850114	136625.431675	35.576884
1234.916229	136860.851953	35.581901
1236.446098	137114.753548	35.586919
1237.693799	137345.439900	35.591936
1239.126956	137573.547663	35.596954
1240.194787	137825.418928	35.601972
1241.299187	138068.351918	35.606989
1242.515050	138302.905828	35.612007
1243.686130	138542.607512	35.617024
1245.318314	138792.352494	35.622042
1246.444538	139028.320003	35.627060
1248.016911	139255.145117	35.632077
1249.383496	139481.292859	35.637095
1250.256642	139716.846556	35.642112
1251.870974	139931.764499	35.647130
1252.609833	140152.873956	35.652148
1254.121290	140384.028850	35.657165
1255.049150	140611.443563	35.662183
1255.996689	140854.656513	35.667200
1257.068496	141091.036156	35.672218
1258.368320	141327.203584	35.677236
1259.376352	141573.976873	35.682253
1260.533142	141816.641556	35.687271
1261.458142	142064.927890	35.692288
1262.711528	142308.303294	35.697306
1263.749028	142564.697004	35.702324
1264.961777	142821.737262	35.707341
1266.439660	143089.664768	35.712359
1267.581697	143351.160883	35.717376
1268.840683	143617.462902	35.722394
1270.187194	143879.780126	35.727412
1270.896230	144153.811518	35.732429
1272.280755	144418.549745	35.737447
1273.560647	144693.091231	35.742464
1275.192023	144968.708775	35.747482
1276.425871	145247.055383	35.752500
1277.638353	145523.769568	35.757517
1278.900881	145798.218203	35.762535
1279.945466	146083.732022	35.767552
1281.338976	146357.363526	35.772570
1282.744242	146641.973588	35.777588
1284.055544	146924.949897	35.782605
1285.606589	147202.432415	35.787623
1286.434772	147492.531805	35.792640
1288.118820	147772.928528	35.797658
1289.520749	148073.374718	35.802676
1290.771966	148347.356245	35.807693
1292.377976	148621.892909	35.812711
1293.558031	148897.335406	35.817728
1295.470192	149172.372783	35.822746
1296.810616	149456.767036	35.827764
1297.938508	149734.468682	35.832781
1299.345851	150007.444209	35.837799
1300.910783	150278.543223	35.842816
1302.895074	150552.548191	35.847834
1304.460665	150812.911182	35.852852
1306.104253	151085.804363	35.857869
1307.613383	151328.572781	35.862887
1308.692730	151591.897012	35.867904
1310.172962	151834.329451	35.872922
1311.565342	152087.007832	35.877940
1313.433721	152339.244732	35.882957
1314.240305	152588.361275	35.887975
1315.598475	152845.745160	35.892992
1316.854681	153094.615852	35.898010
1318.108827	153345.899824	35.903028
1319.292165	153606.081832	35.908045
1320.802192	153846.423772	35.913063
1321.976665	154110.582728	35.918080
1322.964512	154369.186656	35.923098
1324.185045	154627.882266	35.928116
1325.181475	154893.050146	35.933133
1326.695266	155149.239482	35.938151
1327.858811	155423.269704	35.943168
1328.997520	155683.633107	35.948186
1330.498730	155946.517922	35.953204
1331.623190	156221.192721	35.958221
1333.454836	156492.584430	35.963239
1334.362707	156760.859432	35.968256
1335.876355	157021.804784	35.973274
1337.216953	157275.453433	35.978292
1338.352935	157522.000646	35.983309
1339.536093	157776.793208	35.988327
1340.729539	158041.626989	35.993344
1342.376368	158297.085474	35.998362
1343.491073	158558.239568	36.003380
1344.800334	158814.768671	36.008397
1345.731587	159069.593379	36.013415
1346.730839	159350.497304	36.018432
1348.310760	159617.905331	36.023450
1349.187840	159887.151099	36.028468
1350.468891	160174.755896	36.033485
1351.851375	160443.137830	36.038503
1353.027195	160747.278579	36.043520
1354.424000	161024.560341	36.048538
1355.784886	161308.184081	36.053556
1357.031112	161603.469023	36.058573
1358.181389	161893.247673	36.063591
1359.609677	162200.326650	36.068608
1360.530871	162490.524717	36.073626
1361.650165	162796.626516	36.078644
1362.923210	163112.075357	36.083661
1364.386962	163418.570508	36.088679
1365.643710	163739.496926	36.093696
1367.202729	164051.210915	36.098714
1368.854911	164375.785804	36.103732
1370.317865	164696.481413	36.108749
1371.649840	165008.006861	36.113767
1372.746805	165324.433270	36.118784
1374.206818	165633.402256	36.123802
1376.005093	165963.383303	36.128820
1377.429726	166277.642505	36.133837
1379.157075	166584.428189	36.138855
1380.395422	166902.718840	36.143872
1382.245255	167221.537370	36.148890
1383.925060	167528.664760	36.153908
1385.473492	167838.175675	36.158925
1387.023784	168144.424527	36.163943
1388.368524	168451.379809	36.168960
1389.838195	168767.598413	36.173978
1391.401421	169056.682685	36.178996
1392.920660	169350.130127	36.184013
1394.661610	169640.801444	36.189031
1396.231849	169944.832782	36.194048
1397.627097	170244.905801	36.199066
1399.139179	170537.254434	36.204084
1400.278232	170836.696981	36.209101
1401.943716	171123.233865	36.214119
1403.247746	171417.421541	36.219136
1404.733205	171718.273587	36.224154
1406.036538	172014.330229	36.229172
1407.106164	172310.869014	36.234189
1408.936962	172598.477575	36.239207
1409.950429	172903.890442	36.244224
1411.697853	173194.028419	36.249242
1413.347868	173490.163417	36.254260
1414.765732	173785.815250	36.259277
1416.123902	174073.249247	36.264295
1417.052720	174379.887392	36.269312
1418.355993	174672.373248	36.274330
1419.458486	174978.364286	36.279348
1420.904515	175289.801009	36.284365
1422.628779	175587.240043	36.289383
1423.976709	175877.170902	36.294400
1425.387649	176184.692753	36.299418
1427.271943	176480.395686	36.304436
1428.240290	176789.601734	36.309453
1429.893985	177081.711142	36.314471
1430.942648	177372.189265	36.319488
1432.196973	177665.760025	36.324506
1433.591998	177960.401844	36.329524
1435.069849	178255.438061	36.334541
1436.473345	178549.140862	36.339559
1437.866737	178852.294061	36.344576
1439.159110	179152.670394	36.349594
1440.424322	179452.620240	36.354612
1441.057375	179761.990977	36.359629
1442.493447	180069.129081	36.364647
1443.952646	180390.842959	36.369664
1444.933957	180709.254852	36.374682
1446.331782	181030.421837	36.379700
1447.713219	181366.704370	36.384717
1449.021247	181702.339256	36.389735
1450.592100	182032.879951	36.394752
1452.370012	182372.405814	36.399770
1453.684042	182698.264934	36.404788
1455.079871	183037.370395	36.409805
1456.705261	183370.650228	36.414823
1458.055822	183715.810019	36.419840
1459.463368	184058.295230	36.424858
1461.163679	184398.805487	36.429876
1462.818751	184747.883441	36.434893
1464.458656	185091.097796	36.439911
1465.784468	185427.657096	36.444928
1466.733868	185794.628504	36.449946
1468.469806	186142.098422	36.454964
1469.847548	186549.110993	36.459981
1471.468609	186904.272043	36.464999
1473.126676	187244.112533	36.470016
1474.323974	187599.748614	36.475034
1476.203485	187955.253686	36.480052
1477.274058	188317.668282	36.485069
1478.950243	188661.929936	36.490087
1481.013684	189011.135842	36.495104
1482.857998	189358.675323	36.500122
1484.618785	189704.222329	36.505140
1485.927707	190049.434696	36.510157
1487.815832	190396.589462	36.515175
1489.324143	190740.782060	36.520192
1491.062978	191065.660639	36.525210
1493.168430	191388.069674	36.530228
1494.367651	191730.230662	36.535245
1496.035315	192058.653741	36.540263
1497.685802	192384.794321	36.545280
1498.975777	192728.848940	36.550298
1500.705677	193044.183480	36.555316
1502.239516	193383.273952	36.560333
1503.551206	193711.147454	36.565351
1505.445236	194042.562993	36.570368
1506.255820	194373.590123	36.575386
1507.858554	194697.940595	36.580404
1509.483699	195046.521135	36.585421
1510.629779	195385.194839	36.590439
1511.694616	195727.184277	36.595456
1513.307338	196071.781363	36.600474
1514.678406	196407.907619	36.605492
1516.105833	196758.174521	36.610509
1518.074357	197098.781182	36.615527
1519.073899	197442.461494	36.620544
1520.649076	197787.220997	36.625562
1522.216387	198132.211148	36.630580
1523.768709	198485.206022	36.635597
1525.785158	198830.660910	36.640615
1527.032574	199180.453660	36.645632
1528.314459	199521.732120	36.650650
1530.320068	199873.008072	36.655668
1531.512286	200199.518005	36.660685
1533.049391	200538.243870	36.665703
1534.259333	200862.135925	36.670720
1535.575685	201212.684352	36.675738
1537.223118	201539.227282	36.680756
1539.037202	201866.024177	36.685773
1540.412141	202206.048874	36.690791
1542.179130	202542.964568	36.695808
1543.603236	202881.357100	36.700826
1545.052446	203216.164569	36.705844
1546.544574	203564.403913	36.710861
1548.112536	203912.454214	36.715879
1549.919888	204246.902635	36.720896
1551.206256	204594.668007	36.725914
1552.974826	204931.663944	36.730932
1554.456082	205278.053660	36.735949
1556.044077	205634.080356	36.740967
1557.583707	205981.147998	36.745984
1558.628451	206337.616552	36.751002
1560.397582	206697.376328	36.756020
1562.393581	207045.746023	36.761037
1563.757911	207403.919101	36.766055
1565.663292	207759.696379	36.771072
1567.176334	208118.685597	36.776090
1568.795423	208461.095868	36.781108
1570.211018	208828.611472	36.786125
1571.690566	209184.330489	36.791143
1573.055692	209546.240919	36.796160
1574.966933	209914.671256	36.801178
1576.404837	210265.724056	36.806196
1578.129654	210635.073676	36.811213
1579.747629	211007.107869	36.816231
1581.155991	211373.739006	36.821248
1582.450903	211745.469059	36.826266
1584.325104	212113.095149	36.831284
1585.910143	212489.836008	36.836301
1587.301558	212861.120436	36.841319
1589.527145	213235.170746	36.846336
1590.711716	213605.446825	36.851354
1592.611204	213977.491282	36.856372
1593.854981	214348.089117	36.861389
1595.173080	214732.342900	36.866407
1596.980435	215113.522851	36.871424
1598.355051	215500.029474	36.876442
1600.217868	215880.413942	36.881460
1602.132339	216253.347337	36.886477
1603.446734	216635.647360	36.891495
1605.446238	217007.348671	36.896512
1606.956757	217394.115087	36.901530
1608.486575	217777.271417	36.906548
1610.217832	218151.657539	36.911565
1611.726768	218540.812989	36.916583
1614.028640	218917.447460	36.921600
1615.677984	219294.768566	36.926618
1617.673579	219662.915661	36.931636
1619.231847	220040.734097	36.936653
1620.619551	220406.614119	36.941671
1622.333969	220773.484736	36.946688
1623.547662	221142.974269	36.951706
1625.405038	221518.815831	36.956724
1627.440881	221888.710450	36.961741
1628.840523	222264.954147	36.966759
1630.564165	222631.671526	36.971776
1631.958003	223016.985579	36.976794
1633.188033	223386.320783	36.981812
1635.047582	223764.067898	36.986829
1636.629311	224144.500570	36.991847
1637.980969	224518.440438	36.996864
1639.550830	224885.537889	37.001882
1641.085062	225250.100521	37.006900
1642.680640	225620.648919	37.011917
1643.993848	225985.246131	37.016935
1645.957468	226344.178038	37.021952
1647.307667	226716.441438	37.026970
1648.944014	227096.230423	37.031988
1650.599096	227466.210440	37.037005
1652.084903	227850.976639	37.042023
1653.512537	228237.707961	37.047040
1654.913453	228615.297898	37.052058
1656.742990	228997.418774	37.057076
1658.611393	229382.150050	37.062093
1660.087592	229787.138756	37.067111
1661.972555	230165.160462	37.072128
1663.346376	230557.793078	37.077146
1664.782856	230954.226288	37.082164
1666.677241	231356.684574	37.087181
1667.984527	231766.754068	37.092199
1669.832352	232159.641853	37.097216
1671.240503	232565.782821	37.102234
1673.060687	232985.526314	37.107252
1674.827957	233391.966122	37.112269
1676.331304	233801.241330	37.117287
1678.149118	234214.175937	37.122304
1679.766750	234631.561764	37.127322
1681.430857	235057.932861	37.132340
1683.130176	235479.115645	37.137357
1684.537743	235906.516752	37.142375
1686.778851	236316.791860	37.147392
1688.672820	236753.820106	37.152410
1690.129654	237174.327643	37.157428
1691.977226	237590.226271	37.162445
1693.730545	238019.348991	37.167463
1695.453781	238443.039486	37.172480
1697.284429	238874.765508	37.177498
1699.105570	239290.132559	37.182516
1700.679904	239712.904640	37.187533
1702.798506	240135.413093	37.192551
1705.021333	240558.971528	37.197568
1706.724818	240970.137533	37.202586
1708.538136	241376.306659	37.207604
1710.540313	241784.833485	37.212621
1712.220787	242195.493044	37.217639
1714.447863	242603.017987	37.222656
1715.835137	243016.694185	37.227674
1717.661181	243430.427993	37.232692
1719.369953	243831.274660	37.237709
1721.250699	244252.289047	37.242727
1722.819845	244651.733488	37.247744
1724.636005	245062.925450	37.252762
1726.423055	245468.456321	37.257780
1728.068437	245883.534587	37.262797
1729.693751	246299.910664	37.267815
1731.458979	246706.001280	37.272832
1733.142868	247126.659452	37.277850
1734.989136	247530.550989	37.282868
1736.403090	247948.658478	37.287885
1738.100980	248366.034700	37.292903
1739.986993	248771.746212	37.297920
1741.521459	249188.206164	37.302938
1743.063564	249609.718954	37.307956
1744.761014	250015.152195	37.312973
1746.279227	250443.042563	37.317991
1748.253422	250873.426057	37.323008
1750.379482	251286.943109	37.328026
1751.886185	251709.878498	37.333044
1753.772560	252124.675529	37.338061
1755.157381	252539.168890	37.343079
1756.875310	252936.716840	37.348096
1758.464991	253337.662208	37.353114
1760.117382	253757.927254	37.358132
1761.855324	254150.972680	37.363149
1763.027590	254571.259657	37.368167
1765.167293	254980.318991	37.373184
1766.495330	255404.033649	37.378202
1768.075265	255841.500410	37.383220
1769.501957	256263.647454	37.388237
1771.311410	256703.082148	37.393255
1773.110424	257140.103902	37.398272
1774.886661	257576.924523	37.403290
1776.044586	258018.742739	37.408308
1778.305302	258469.073851	37.413325
1779.755221	258916.659926	37.418343
1781.838487	259364.272246	37.423360
1783.761894	259824.912905	37.428378
1785.160043	260280.655509	37.433396
1787.283050	260719.772787	37.438413
1789.312269	261191.846977	37.443431
1791.155585	261642.612318	37.448448
1793.178799	262101.729659	37.453466
1794.624973	262564.846960	37.458484
1796.639256	263015.986364	37.463501
1798.435704	263485.471054	37.468519
1800.248754	263946.848663	37.473536
1802.232062	264409.086591	37.478554
1804.040658	264873.407148	37.483572
1805.829917	265334.960139	37.488589
1807.727994	265810.946037	37.493607
1809.627372	266275.728583	37.498624
1811.662307	266735.179411	37.503642
1813.411686	267213.569359	37.508660
1815.233004	267676.884389	37.513677
1816.614584	268152.482621	37.518695
1818.990291	268618.906540	37.523712
1820.477013	269081.327363	37.528730
1822.473238	269563.146431	37.533748
1824.201347	270040.661903	37.538765
1826.352633	270512.343372	37.543783
1827.906357	270992.141523	37.548800
1830.066514	271464.756313	37.553818
1831.787327	271952.269361	37.558836
1833.513984	272421.213440	37.563853
1835.221524	272902.069185	37.568871
1837.131711	273376.973047	37.573888
1839.087560	273863.879772	37.578906
1840.915324	274343.819653	37.583924
1843.003265	274820.744669	37.588941
1844.765404	275298.911532	37.593959
1846.693371	275789.036636	37.598976
1848.876689	276264.643087	37.603994
1850.530853	276743.224641	37.609012
1852.537828	277221.976664	37.614029
1854.118227	277706.836660	37.619047
1856.078934	278181.399787	37.624064
1857.968415	278664.046826	37.629082
1859.558206	279156.591001	37.634100
1861.250937	279646.855720	37.639117
1863.366016	280136.136943	37.644135
1864.923775	280625.857679	37.649152
1867.340202	281102.515054	37.654170
1869.317162	281586.805570	37.659188
1871.392901	282062.468806	37.664205
1873.260950	282539.050180	37.669223
1875.300924	283013.290636	37.674240
1877.750213	283484.594393	37.679258
1879.338147	283948.818038	37.684276
1881.562747	284384.625518	37.689293
1883.485634	284834.748361	37.694311
1885.415177	285279.382341	37.699328
1887.024190	285718.451774	37.704346
1888.426324	286173.624219	37.709364
1890.442429	286619.886344	37.714381
1892.243404	287079.306916	37.719399
1893.707777	287533.723946	37.724416
1895.202409	287998.975418	37.729434
1896.685443	288475.778593	37.734452
1898.777270	288951.492723	37.739469
1900.661325	289426.499484	37.744487
1902.191563	289901.507279	37.749504
1904.272874	290381.097205	37.754522
1906.288800	290876.080467	37.759540
1907.959967	291353.797404	37.764557
1910.007174	291851.154695	37.769575
1911.434636	292361.122245	37.774592
1913.186801	292854.201215	37.779610
1914.558193	293366.124107	37.784628
1916.429942	293869.992044	37.789645
1918.492812	294391.572894	37.794663
1920.705429	294917.213337	37.799680
1922.661364	295436.161199	37.804698
1924.495104	295960.455148	37.809716
1926.147921	296479.136436	37.814733
1928.349108	297013.569401	37.819751
1929.889580	297557.697333	37.824768
1931.909249	298088.619650	37.829786
1933.310604	298633.901384	37.834804
1935.221985	299175.239130	37.839821
1937.669989	299712.222610	37.844839
1939.855703	300263.204508	37.849856
1942.276818	300803.075542	37.854874
1944.381663	301347.712480	37.859892
1946.682816	301882.463463	37.864909
1948.499097	302405.023699	37.869927
1950.497647	302949.660887	37.874944
1952.833143	303484.644148	37.879962
1954.762128	304031.438696	37.884980
1956.672259	304562.796618	37.889997
1959.101919	305094.270838	37.895015
1960.807740	305626.995066	37.900032
1963.555379	306153.560131	37.905050
1965.686537	306692.806364	37.910068
1967.694825	307208.865756	37.915085
1969.916564	307741.334555	37.920103
1971.580301	308259.416801	37.925120
1973.543388	308779.959609	37.930138
1975.109310	309311.244891	37.935156
1977.576822	309831.545238	37.940173
1979.452759	310340.993063	37.945191
1981.496764	310881.526673	37.950208
1984.020289	311393.780801	37.955226
1985.873140	311924.027754	37.960244
1988.059021	312428.785394	37.965261
1990.466603	312962.918546	37.970279
1992.118020	313470.159657	37.975296
1994.536359	313979.001024	37.980314
1996.456910	314489.995748	37.985332
1997.693298	314997.411840	37.990349
1999.813300	315517.880980	37.995367
2001.778467	316042.276635	38.000384
2003.830550	316572.819466	38.005402
2005.628363	317085.555127	38.010420
2007.566766	317603.490655	38.015437
2009.507994	318111.497143	38.020455
2011.087050	318620.671008	38.025472
2012.857686	319121.739170	38.030490
2014.879108	319633.420407	38.035508
2016.222501	320144.694144	38.040525
2018.661502	320653.125922	38.045543
2020.458622	321174.492081	38.050560
2022.392186	321693.800482	38.055578
2024.463554	322215.694554	38.060596
2026.146547	322735.739820	38.065613
2028.215287	323269.471103	38.070631
2030.409735	323803.175867	38.075648
2032.495814	324336.941447	38.080666
2034.164100	324880.940139	38.085684
2036.088327	325416.214020	38.090701
2038.163722	325966.731496	38.095719
2039.811302	326522.408234	38.100736
2041.860650	327071.468499	38.105754
2043.961410	327627.642585	38.110772
2045.579176	328196.341706	38.115789
2047.836451	328760.162896	38.120807
2049.938404	329324.051051	38.125824
2051.790672	329897.179482	38.130842
2054.486529	330470.928583	38.135860
2056.361174	331041.804087	38.140877
2058.714405	331606.101806	38.145895
2060.892307	332181.479332	38.150912
2062.847503	332749.754557	38.155930
2064.938584	333325.813281	38.160948
2066.758526	333909.414370	38.165965
2069.377420	334489.583667	38.170983
2071.433427	335078.405912	38.176000
2073.577281	335651.249727	38.181018
2075.591171	336239.603487	38.186036
2077.585005	336827.443645	38.191053
2079.918301	337400.179790	38.196071
2081.785692	337986.575212	38.201088
2083.978271	338573.442887	38.206106
2085.899233	339170.057790	38.211124
2087.973303	339758.218159	38.216141
2089.994895	340351.424230	38.221159
2091.570759	340954.226380	38.226176
2094.022771	341553.026103	38.231194
2095.917569	342158.065629	38.236212
2098.397286	342768.658672	38.241229
2100.539023	343371.964584	38.246247
2101.966116	343983.867431	38.251264
2104.298153	344602.211333	38.256282
2106.313569	345219.858138	38.261300
2108.315795	345833.641215	38.266317
2110.641612	346438.639209	38.271335
2112.550494	347060.909591	38.276352
2115.084818	347677.035455	38.281370
2117.116612	348306.338093	38.286388
2119.211214	348931.688671	38.291405
2121.459286	349548.356943	38.296423
2123.392569	350173.151273	38.301440
2125.734818	350791.581579	38.306458
2128.020991	351411.428715	38.311476
2129.968124	352038.542900	38.316493
2132.188229	352658.629883	38.321511
2134.110526	353281.413493	38.326528
2136.537719	353910.317301	38.331546
2139.326613	354529.213984	38.336564
2141.145367	355136.765980	38.341581
2143.779988	355756.600606	38.346599
2146.119189	356369.142791	38.351616
2148.504474	356966.633042	38.356634
2151.045637	357561.501680	38.361652
2153.240655	358150.075667	38.366669
2155.380375	358723.767310	38.371687
2157.098461	359289.732212	38.376704
2159.461351	359858.728801	38.381722
2161.926050	360436.291462	38.386740
2163.454523	361014.521779	38.391757
2165.853076	361585.964092	38.396775
2168.066920	362170.173279	38.401792
2170.100530	362739.141305	38.406810
2172.080506	363317.585729	38.411828
2174.264975	363903.564742	38.416845
2176.140340	364482.661545	38.421863
2178.191735	365078.597948	38.426880
2180.100766	365669.247770	38.431898
2182.351467	366264.976562	38.436916
2184.412549	366871.999763	38.441933
2186.583939	367475.799880	38.446951
2188.779299	368087.134995	38.451968
2190.990371	368693.082417	38.456986
2193.351921	369294.280181	38.462004
2195.867641	369898.076268	38.467021
2198.685418	370502.268211	38.472039
2201.126642	371108.862432	38.477056
2203.127270	371710.824957	38.482074
2205.589612	372317.744211	38.487092
2207.472793	372926.083552	38.492109
2209.569312	373539.063166	38.497127
2211.826487	374152.941328	38.502144
2213.711467	374756.096720	38.507162
2216.358102	375374.927968	38.512180
2218.803838	375995.524489	38.517197
2220.798837	376611.769316	38.522215
2222.989237	377239.115595	38.527232
2224.635777	377862.985797	38.532250
2226.742405	378485.629502	38.537268
2228.756438	379126.358980	38.542285
2231.334413	379764.325048	38.547303
2233.360103	380402.640642	38.552320
2235.146843	381052.933124	38.557338
2237.602775	381693.530736	38.562356
2239.319387	382368.977220	38.567373
2241.605288	383018.889066	38.572391
2244.030547	383675.980597	38.577408
2245.786952	384339.541885	38.582426
2248.325966	384998.784918	38.587444
2250.628643	385676.027850	38.592461
2253.186078	386334.954679	38.597479
2255.537122	386999.619475	38.602496
2257.057249	387675.158485	38.607514
2260.042902	388345.816173	38.612532
2262.246861	389023.313337	38.617549
2264.561577	389686.392929	38.622567
2267.190168	390362.824789	38.627584
2269.613932	391035.776103	38.632602
2271.714193	391704.354205	38.637620
2273.800527	392373.118676	38.642637
2276.092500	393047.351531	38.647655
2278.549166	393717.134871	38.652672
2280.393727	394406.133481	38.657690
2282.714205	395086.785379	38.662708
2285.032238	395762.861807	38.667725
2287.515123	396441.981387	38.672743
2289.490446	397135.639416	38.677760
2291.752251	397816.930902	38.682778
2294.655920	398507.214045	38.687796
2296.519837	399184.731417	38.692813
2298.483728	399874.614935	38.697831
2301.163493	400546.801928	38.702848
2303.005384	401213.937671	38.707866
2305.218609	401881.856434	38.712884
2307.329900	402548.354544	38.717901
2309.225771	403215.980351	38.722919
2311.501046	403899.469199	38.727936
2313.403785	404579.453165	38.732954
2315.603996	405260.685892	38.737972
2317.536646	405960.663626	38.742989
2319.786954	406659.658949	38.748007
2321.972633	407363.196638	38.753024
2324.055331	408081.250372	38.758042
2326.512395	408793.251659	38.763060
2328.532428	409512.837232	38.768077
2330.833343	410233.974341	38.773095
2333.349632	410960.315703	38.778112
2335.490055	411681.936035	38.783130
2338.271896	412409.401662	38.788148
2340.596985	413150.927204	38.793165
2342.965885	413885.490008	38.798183
2345.569660	414620.952027	38.803200
2348.122473	415374.353663	38.808218
2350.641979	416110.384476	38.813236
2353.169039	416861.714119	38.818253
2355.482292	417605.666129	38.823271
2358.035712	418344.294359	38.828288
2359.955151	419096.853001	38.833306
2362.444904	419840.748581	38.838324
2364.700457	420599.825287	38.843341
2366.710999	421362.755688	38.848359
2369.719053	422121.608191	38.853376
2372.066711	422887.362189	38.858394
2374.494669	423639.069035	38.863412
2376.792798	424407.807516	38.868429
2379.063297	425166.864412	38.873447
2382.172679	425912.465036	38.878464
2384.961997	426669.867505	38.883482
2387.696558	427427.654363	38.888500
2390.331430	428178.603621	38.893517
2392.723908	428936.791054	38.898535
2395.571192	429678.298721	38.903552
2397.781168	430427.156835	38.908570
2400.049122	431176.280653	38.913588
2402.695102	431916.674054	38.918605
2405.353413	432670.632726	38.923623
2407.600793	433416.035003	38.928640
2409.795682	434171.119771	38.933658
2412.218061	434911.686690	38.938676
2415.061314	435655.848138	38.943693
2417.291334	436405.028592	38.948711
2420.182020	437141.191638	38.953728
2422.684255	437877.538561	38.958746
2426.291935	438595.697324	38.963764
2429.528658	439312.017492	38.968781
2432.088821	440023.818877	38.973799
2435.187856	440733.942915	38.978816
2437.468175	441449.825937	38.983834
2439.630098	442144.180700	38.988852
2441.914745	442845.461121	38.993869
2444.019884	443561.593312	38.998887
2446.291043	444261.357351	39.003904
2448.267577	444979.020389	39.008922
2450.854541	445676.812371	39.013940
2453.000857	446401.867865	39.018957
2455.024151	447121.560637	39.023975
2457.458484	447840.403117	39.028992
2459.127641	448572.163009	39.034010
2461.386252	449306.982219	39.039028
2463.542532	450033.203600	39.044045
2465.761167	450758.779911	39.049063
2468.079169	451483.402408	39.054080
2469.965066	452203.367722	39.059098
2472.327569	452928.429219	39.064116
2474.456674	453678.940777	39.069133
2476.816601	454410.151199	39.074151
2478.894235	455149.249982	39.079168
2481.499047	455914.634202	39.084186
2483.919298	456669.363701	39.089204
2486.366172	457412.548701	39.094221
2488.925278	458176.780612	39.099239
2491.410774	458942.605188	39.104256
2494.104429	459719.768268	39.109274
2496.731166	460494.686248	39.114292
2498.896390	461271.609260	39.119309
2501.296264	462047.652826	39.124327
2504.122195	462823.392473	39.129344
2506.696818	463613.515154	39.134362
2509.010330	464422.863575	39.139380
2511.223776	465204.290513	39.144397
2513.602738	466019.050647	39.149415
2516.213191	466820.215847	39.154432
2519.164107	467628.401471	39.159450
2521.632304	468436.673638	39.164468
2524.431207	469240.264820	39.169485
2526.881381	470061.321522	39.174503
2529.537606	470870.251781	39.179520
2532.197167	471689.076031	39.184538
2534.438417	472502.276802	39.189556
2537.239927	473326.240817	39.194573
2539.605340	474154.113543	39.199591
2542.419831	474976.579576	39.204608
2544.441823	475813.899426	39.209626
2547.274019	476635.823912	39.214644
2550.076521	477468.649907	39.219661
2552.947705	478300.413402	39.224679
2555.777368	479132.895847	39.229696
2558.606260	479969.618812	39.234714
2560.847102	480792.176406	39.239732
2563.471449	481624.307279	39.244749
2566.004862	482465.731184	39.249767
2568.623750	483294.195897	39.254784
2571.040112	484130.408113	39.259802
2573.848708	484963.994494	39.264820
2577.103887	485798.221770	39.269837
2579.731876	486647.011728	39.274855
2582.663228	487466.185395	39.279872
2585.087754	488291.691408	39.284890
2587.458889	489132.071495	39.289908
2590.628695	489960.543861	39.294925
2593.164970	490789.271418	39.299943
2595.503682	491623.574842	39.304960
2597.521375	492457.831820	39.309978
2600.376114	493292.012169	39.314996
2602.990034	494136.708080	39.320013
2605.336442	494971.528614	39.325031
2607.830518	495805.272081	39.330048
2610.191384	496653.842011	39.335066
2612.957512	497497.315577	39.340084
2615.370806	498356.603312	39.345101
2617.773587	499204.012612	39.350119
2620.145368	500059.683047	39.355136
2622.837776	500916.410698	39.360154
2625.347015	501781.118897	39.365172
2628.035048	502652.843550	39.370189
2630.395451	503523.761533	39.375207
2633.406984	504385.718702	39.380224
2636.113752	505238.463440	39.385242
2638.583604	506086.011833	39.390260
2641.137694	506930.075345	39.395277
2643.524571	507767.524288	39.400295
2645.843712	508603.374738	39.405312
2648.445093	509443.356949	39.410330
2650.897515	510294.026165	39.415348
2653.527056	511153.367703	39.420365
2655.633944	512013.844565	39.425383
2658.301441	512871.213414	39.430400
2660.994417	513748.891796	39.435418
2663.494899	514624.482933	39.440436
2666.036701	515492.168140	39.445453
2668.741011	516384.761334	39.450471
2671.069627	517270.970249	39.455488
2673.592738	518171.066706	39.460506
2676.046227	519076.794833	39.465524
2678.996007	519984.043630	39.470541
2681.343983	520894.341365	39.475559
2684.494399	521816.363266	39.480576
2687.077649	522734.641517	39.485594
2689.921160	523663.821072	39.490612
2692.638482	524588.483669	39.495629
2695.439518	525515.983072	39.500647
2698.806183	526443.630601	39.505664
2701.103275	527379.870333	39.510682
2704.016506	528302.936773	39.515700
2706.865263	529244.784587	39.520717
2709.564673	530178.049562	39.525735
2712.549698	531116.727610	39.530752
2715.167151	532055.194528	39.535770
2717.616230	532986.639934	39.540788
2720.675472	533928.266397	39.545805
2722.924927	534872.712110	39.550823
2726.152627	535816.282734	39.555840
2728.943364	536774.209477	39.560858
2731.558789	537732.894866	39.565876
2734.838368	538677.249714	39.570893
2737.649540	539631.946434	39.575911
2740.288540	540568.079528	39.580928
2743.008307	541523.400195	39.585946
2745.766692	542485.817571	39.590964
2748.628589	543439.314139	39.595981
2751.745873	544395.407084	39.600999
2754.684356	545348.795672	39.606016
2757.656428	546297.641230	39.611034
2760.057250	547250.465799	39.616052
2762.662396	548192.501781	39.621069
2765.303894	549155.723778	39.626087
2768.358302	550116.598964	39.631104
2771.148925	551072.726314	39.636122
2774.277937	552030.530609	39.641140
2777.514922	552975.758753	39.646157
2780.344292	553937.219212	39.651175
2783.087074	554884.330305	39.656192
2786.122950	555839.490990	39.661210
2788.754976	556787.672111	39.666228
2791.548031	557736.153700	39.671245
2794.408875	558683.797470	39.676263
2797.203430	559637.288602	39.681280
2800.154006	560582.010678	39.686298
2802.452681	561539.734726	39.691316
2805.607018	562485.424582	39.696333
2808.453194	563435.093648	39.701351
2811.427332	564382.612012	39.706368
2814.206653	565336.744847	39.711386
2816.971004	566282.688953	39.716404
2820.170184	567209.609695	39.721421
2823.045822	568147.772573	39.726439
2826.139064	569062.644184	39.731456
2828.738790	569962.901799	39.736474
2831.015293	570864.140397	39.741492
2834.134364	571763.274067	39.746509
2836.895636	572675.205745	39.751527
2839.410814	573578.945071	39.756544
2842.048574	574493.052098	39.761562
2844.308871	575414.049541	39.766580
2847.045223	576329.243343	39.771597
2849.706269	577273.492133	39.776615
2852.309780	578212.117417	39.781632
2854.877377	579152.270156	39.786650
2857.274208	580108.175871	39.791668
2859.877182	581073.319596	39.796685
2863.510180	582048.419978	39.801703
2865.634546	583009.868869	39.806720
2868.206280	583983.013914	39.811738
2871.157493	584982.011127	39.816756
2873.848747	585972.659281	39.821773
2876.571816	586981.457619	39.826791
2879.317245	587992.558054	39.831808
2881.959924	589007.628463	39.836826
2884.603123	590028.700161	39.841844
2887.497502	591054.182949	39.846861
2890.469412	592083.752666	39.851879
2893.309971	593141.470290	39.856896
2895.829637	594185.745965	39.861914
2898.732011	595260.827237	39.866932
2901.786114	596298.518417	39.871949
2904.472164	597358.837353	39.876967
2907.121767	598433.036716	39.881984
2910.643272	599511.483573	39.887002
2913.695447	600573.468298	39.892020
2917.023347	601651.724965	39.897037
2920.473947	602732.446334	39.902055
2923.188928	603791.161162	39.907072
2926.859705	604858.600744	39.912090
2929.960426	605932.755215	39.917108
2933.058845	607009.891268	39.922125
2935.827729	608060.326327	39.927143
2938.978140	609136.282900	39.932160
2941.961709	610203.523493	39.937178
2945.187239	611276.399304	39.942196
2948.267957	612333.875457	39.947213
2951.470432	613400.944767	39.952231
2954.285855	614465.867713	39.957248
2956.880877	615535.248632	39.962266
2959.498871	616601.371631	39.967284
2962.459371	617678.989700	39.972301
2966.151064	618755.878510	39.977319
2968.808433	619833.111221	39.982336
2971.904247	620907.368093	39.987354
2974.332079	621985.647731	39.992372
2978.095741	623066.937789	39.997389
2981.409445	624137.918868	40.002407
2984.172557	625216.338974	40.007424
2987.362124	626272.364308	40.012442
2989.981886	627357.690552	40.017460
2992.829734	628432.155989	40.022477
2996.186941	629501.942276	40.027495
2998.908060	630588.333694	40.032512
3001.803669	631660.640044	40.037530
3004.772780	632751.276788	40.042548
3008.362225	633837.114470	40.047565
3011.378590	634912.619558	40.052583
3014.087182	635991.533214	40.057600
3017.334374	637060.441076	40.062618
3020.497077	638121.035066	40.067636
3023.579426	639162.426423	40.072653
3026.542955	640192.831538	40.077671
3029.281995	641233.101969	40.082688
3032.535081	642256.025498	40.087706
3035.131660	643297.877627	40.092724
3038.254075	644333.616301	40.097741
3041.522197	645379.006440	40.102759
3044.292647	646410.890160	40.107776
3047.417620	647448.813462	40.112794
3050.722063	648498.464697	40.117812
3053.426049	649535.721023	40.122829
3056.945156	650585.993392	40.127847
3059.298502	651645.365424	40.132864
3062.467016	652701.159633	40.137882
3065.331943	653774.454432	40.142900
3068.690759	654841.339093	40.147917
3071.825782	655913.145937	40.152935
3074.364940	656991.072567	40.157952
3077.657997	658075.004645	40.162970
3080.840848	659155.894951	40.167988
3083.602180	660243.021120	40.173005
3086.764767	661345.528550	40.178023
3089.772120	662442.814175	40.183040
3093.374281	663541.656066	40.188058
3096.644323	664644.528843	40.193076
3099.942566	665738.978466	40.198093
3103.284144	666836.507197	40.203111
3106.330280	667935.134045	40.208128
3109.506563	669037.220329	40.213146
3112.549271	670163.818212	40.218164
3115.658082	671275.790289	40.223181
3118.626740	672390.613992	40.228199
3122.068094	673499.918984	40.233216
3125.299620	674625.261249	40.238234
3128.521682	675748.773408	40.243252
3131.380736	676868.332170	40.248269
3134.467050	677990.332592	40.253287
3137.721446	679115.673632	40.258304
3141.303337	680238.834112	40.263322
3144.247535	681369.567039	40.268340
3147.506504	682500.940396	40.273357
3151.109419	683628.594670	40.278375
3154.064193	684763.768012	40.283392
3157.452758	685884.374139	40.288410
3160.210301	687020.854397	40.293428
3163.029595	688157.515867	40.298445
3166.418549	689299.470461	40.303463
3169.414265	690445.580620	40.308480
3172.497497	691596.065602	40.313498
3175.489094	692745.415450	40.318516
3178.625697	693893.840268	40.323533
3182.459234	695049.900712	40.328551
3185.259464	696211.541519	40.333568
3188.836411	697356.198595	40.338586
3192.153513	698519.305576	40.343604
3195.107294	699681.462560	40.348621
3198.790412	700826.599472	40.353639
3201.412619	701986.204394	40.358656
3204.768896	703137.628969	40.363674
3208.207569	704301.114945	40.368692
3211.370009	705451.347861	40.373709
3214.501530	706612.175556	40.378727
3217.213367	707778.473675	40.383744
3220.936872	708940.446282	40.388762
3224.299303	710115.176386	40.393780
3227.333869	711283.223911	40.398797
3230.059010	712449.469584	40.403815
3233.104243	713613.815307	40.408832
3236.509762	714747.272885	40.413850
3239.941374	715881.793342	40.418868
3242.856528	717011.498271	40.423885
3246.314903	718139.770978	40.428903
3249.428978	719279.361122	40.433920
3252.207120	720412.629193	40.438938
3255.780505	721550.727329	40.443956
3258.480193	722696.572676	40.448973
3261.743447	723831.720996	40.453991
3264.504425	724987.551288	40.459008
3268.074943	726140.618404	40.464026
3271.290467	727308.033020	40.469044
3274.229821	728484.511156	40.474061
3277.242020	729663.450759	40.479079
3280.679344	730850.057951	40.484096
3283.738218	732038.651154	40.489114
3286.925156	733235.984372	40.494132
3290.050238	734443.065772	40.499149
3293.686881	735648.740720	40.504167
3297.157096	736847.758352	40.509184
3301.077800	738065.675054	40.514202
3304.340887	739270.768733	40.519220
3307.212509	740481.129594	40.524237
3310.908765	741698.970941	40.529255
3313.902048	742932.776950	40.534272
3317.050767	744169.394025	40.539290
3320.413713	745407.976404	40.544308
3323.464725	746646.886884	40.549325
3327.124399	747884.606758	40.554343
3330.329480	749137.934739	40.559360
3333.791158	750386.049714	40.564378
3337.263930	751630.414465	40.569396
3340.620124	752892.038483	40.574413
3344.341026	754131.760501	40.579431
3347.902932	755381.242537	40.584448
3351.332016	756645.620972	40.589466
3355.228836	757894.656348	40.594484
3358.210684	759152.971582	40.599501
3362.390527	760392.994705	40.604519
3365.708179	761660.409592	40.609536
3369.116827	762906.279530	40.614554
3371.857730	764172.153763	40.619572
3374.901872	765426.736496	40.624589
3379.081850	766689.969091	40.629607
3382.200453	767951.864744	40.634624
3385.227498	769217.506832	40.639642
3388.828908	770487.326571	40.644660
3392.297046	771765.050547	40.649677
3395.429316	773027.137228	40.654695
3398.725229	774320.204030	40.659712
3401.994745	775599.099105	40.664730
3405.085149	776875.582153	40.669748
3408.114578	778173.918586	40.674765
3411.697727	779461.220606	40.679783
3414.856316	780766.413910	40.684800
3418.585845	782064.525521	40.689818
3422.169768	783361.187627	40.694836
3424.982180	784688.079652	40.699853
3428.436775	785990.937698	40.704871
3431.715069	787318.842290	40.709888
3435.400211	788630.660032	40.714906
3438.844011	789938.986998	40.719924
3441.951748	791260.662769	40.724941
3445.656754	792588.122072	40.729959
3449.143413	793911.398068	40.734976
3452.166784	795232.236492	40.739994
3456.284738	796553.610320	40.745012
3459.699795	797866.664973	40.750016
3462.885951	799130.234797	40.755021
3466.339189	800363.149699	40.760026
3469.404843	801533.264920	40.765031
3472.740744	802632.312513	40.770036
3475.866659	803687.387035	40.775040
3478.251514	804675.126305	40.780045
3481.004725	805610.558394	40.785050
3483.348503	806478.707897	40.790055
3486.253772	807292.861296	40.795060
3488.348788	808045.988138	40.800064
3490.325984	808743.754998	40.805069
3492.598449	809392.063085	40.810074
3494.652774	809983.744560	40.815079
3496.477647	810521.302889	40.820084
3498.094715	811030.482290	40.825088
3499.417394	811477.286387	40.830093
3501.362073	811886.340865	40.835098
3502.719348	812242.151447	40.840103
3504.723249	812558.177663	40.845108
3505.738294	812848.518811	40.850112
3506.845223	813087.966348	40.855117
3508.126837	813307.596925	40.860122
3508.934296	813479.939046	40.865127
3510.328978	813616.815370	40.870132
3510.974215	813743.867563	40.875136
3511.700529	813829.398208	40.880141
3512.798600	813897.819014	40.885146
3512.696704	813929.987423	40.890151
3513.990194	813948.492065	40.895156
3513.971729	813953.658842	40.900160
3514.887698	813921.265959	40.905165
3515.010327	813890.750701	40.910170
3515.571295	813846.331350	40.915175
3516.039450	813772.501252	40.920180
3516.223935	813692.576224	40.925184
3516.386382	813606.027951	40.930189
3516.709673	813495.873362	40.935194
3516.713269	813373.002185	40.940199
3517.527464	813242.596296	40.945204
3517.337955	813121.309449	40.950208
3517.618521	812975.975059	40.955213
3517.847287	812818.854130	40.960218
3518.029343	812656.376763	40.965223
3518.001403	812489.055335	40.970228
3517.880799	812321.743936	40.975232
3518.289453	812144.014694	40.980237
3518.422974	811967.590444	40.985242
3518.314081	811772.485918	40.990247
3518.597625	811571.368452	40.995252
3518.373969	811379.388653	41.000256
3518.390690	811178.690239	41.005261
3518.207342	810964.662324	41.010266
3518.326730	810770.173397	41.015271
3518.649608	810554.200287	41.020276
3518.400555	810342.208669	41.025280
3517.981611	810134.331074	41.030285
3517.806735	809919.096469	41.035290
3517.560362	809708.740543	41.040295
3518.063351	809489.192966	41.045300
3517.589492	809281.880896	41.050304
3517.580695	809059.668317	41.055309
3517.948984	808832.415967	41.060314
3517.679264	808612.812508	41.065319
3517.297325	808386.002711	41.070324
3516.952563	808174.002097	41.075328
3516.837434	807959.032782	41.080333
3516.631079	807742.948880	41.085338
3517.006948	807525.011056	41.090343
3516.692991	807313.464510	41.095348
3516.653751	807104.062549	41.100352
3516.502081	806895.744202	41.105357
3516.355059	806672.884340	41.110362
3515.941082	806468.202090	41.115367
3515.864426	806252.339841	41.120372
3515.702916	806053.213888	41.125376
3515.542429	805843.301599	41.130381
3515.247837	805641.110541	41.135386
3515.317867	805435.197478	41.140391
3515.128663	805236.391788	41.145396
3514.968683	805034.209217	41.150400
3515.186310	804840.791439	41.155405
3514.796501	804637.607728	41.160410
3514.498377	804438.989368	41.165415
3514.390900	804241.066883	41.170420
3514.343712	804046.690648	41.175424
3514.187348	803864.377504	41.180429
3514.126010	803669.455288	41.185434
3514.169750	803473.290804	41.190439
3514.121371	803274.304443	41.195444
3513.592506	803098.371403	41.200448
3513.203784	802910.504313	41.205453
3513.463774	802733.754736	41.210458
3513.171516	802553.133559	41.215463
3513.133700	802369.734461	41.220468
3512.514385	802199.012955	41.225472
3512.757200	802009.410144	41.230477
3512.482415	801847.166698	41.235482
3512.836148	801680.476827	41.240487
3512.557824	801498.213056	41.245492
3512.475966	801337.342100	41.250496
3512.355925	801162.805249	41.255501
3512.047925	800994.443741	41.260506
3511.410049	800836.380811	41.265511
3511.612980	800667.979707	41.270516
3511.288241	800514.741676	41.275520
3511.385396	800357.723737	41.280525
3511.222774	800212.410805	41.285530
3511.270723	800060.275408	41.290535
3511.293872	799893.932708	41.295540
3510.822727	799738.941470	41.300544
3511.090939	799589.445885	41.305549
3511.054039	799442.680009	41.310554
3510.839993	799281.338927	41.315559
3510.807016	799139.838977	41.320564
3510.355595	798995.227379	41.325568
3510.327664	798856.747910	41.330573
3510.393777	798710.242275	41.335578
3510.220838	798579.446205	41.340583
3510.144895	798427.731208	41.345588
3509.989116	798292.336208	41.350592
3509.954790	798150.912494	41.355597
3509.471532	798012.290774	41.360602
3509.456091	797882.921130	41.365607
3509.432652	797757.310796	41.370612
3509.280169	797626.687628	41.375616
3509.272190	797496.381129	41.380621
3509.402847	797371.129953	41.385626
3508.773780	797251.416733	41.390631
3508.962417	797120.339290	41.395636
3509.041027	797008.277198	41.400640
3508.559238	796878.960416	41.405645
3508.543344	796759.239948	41.410650
3508.420537	796647.935825	41.415655
3508.769367	796532.990110	41.420660
3508.096889	796407.455092	41.425664
3508.272365	796303.572437	41.430669
3508.288901	796188.916833	41.435674
3508.204627	796080.088375	41.440679
3507.997900	795963.558462	41.445684
3507.653194	795859.017225	41.450688
3507.888020	795754.432567	41.455693
3507.928305	795649.094954	41.460698
3507.591331	795542.202355	41.465703
3507.934382	795430.071711	41.470708
3507.187769	795333.939407	41.475712
3507.318088	795230.339822	41.480717
3507.194541	795127.511163	41.485722
3507.293787	795030.118380	41.490727
3507.245108	794933.138151	41.495732
3506.925472	794836.149974	41.500736
3506.860691	794740.781829	41.505741
3506.819865	794649.073261	41.510746
3506.896650	794560.765468	41.515751
3506.769178	794464.914452	41.520756
3506.983558	794371.500702	41.525760
3506.529669	794276.430917	41.530765
3506.438149	794191.711631	41.535770
3506.448695	794103.896673	41.540775
3506.261044	794020.020924	41.545780
3506.481914	793940.722717	41.550784
3506.587786	793846.683136	41.555789
3506.180227	793760.346114	41.560794
3506.242050	793682.731203	41.565799
3506.029590	793597.778766	41.570804
3505.915027	793522.437578	41.575808
3506.003667	793441.883335	41.580813
3505.795137	793358.686565	41.585818
3505.647837	793292.877987	41.590823
3506.021267	793207.389032	41.595828
3505.686954	793133.641672	41.600832
3505.819179	793054.199949	41.605837
3505.771816	792975.567341	41.610842
3505.723291	792903.629978	41.615847
3505.911058	792828.477915	41.620852
3505.164959	792747.947862	41.625856
3505.391217	792678.848822	41.630861
3505.407471	792608.462172	41.635866
3505.059829	792550.888972	41.640871
3505.571044	792477.393069	41.645876
3505.293767	792412.817937	41.650880
3504.725425	792343.008615	41.655885
3504.806433	792267.231360	41.660890
3504.707833	792213.282310	41.665895
3504.540279	792143.408208	41.670900
3504.727047	792099.972037	41.675904
3504.623241	792034.583947	41.680909
3504.313591	791980.568208	41.685914
3504.464813	791936.549919	41.690919
3504.698546	791876.973468	41.695924
3504.846341	791819.707461	41.700928
3504.442131	791753.776921	41.705933
3504.446109	791696.581206	41.710938
3504.327142	791649.279049	41.715943
3504.483934	791581.010351	41.720948
3504.496370	791535.740038	41.725952
3504.760994	791489.550034	41.730957
3504.899461	791419.473722	41.735962
3504.050407	791365.683899	41.740967
3504.131025	791313.410491	41.745972
3504.234304	791266.510823	41.750976
3504.390175	791205.327142	41.755981
3504.419306	791149.393832	41.760986
3504.469112	791089.692325	41.765991
3504.662104	791030.310123	41.770996
3503.992560	790977.613521	41.776000
3504.065712	790914.924468	41.781005
3504.366776	790878.013710	41.786010
3504.126884	790826.079875	41.791015
3503.953013	790767.094884	41.796020
3503.918104	790729.111297	41.801024
3503.654624	790680.651341	41.806029
3503.368981	790631.069955	41.811034
3503.600210	790587.861302	41.816039
3503.810823	790537.810492	41.821044
3503.412178	790501.838195	41.826048
3503.567579	790451.208631	41.831053
3503.127192	790416.562536	41.836058
3503.287309	790371.358904	41.841063
3503.131299	790336.961303	41.846068
3503.317059	790298.158411	41.851072
3503.110266	790274.427599	41.856077
3503.692603	790236.980323	41.861082
3503.048376	790195.715094	41.866087
3503.272919	790155.389519	41.871092
3503.003431	790111.082496	41.876096
3502.912296	790078.042508	41.881101
3503.214329	790041.811470	41.886106
3502.873489	790009.103554	41.891111
3502.919966	789972.667597	41.896116
3502.918624	789946.214106	41.901120
3503.062886	789922.231554	41.906125
3503.005353	789883.170861	41.911130
3503.046229	789851.820546	41.916135
3503.163990	789810.042590	41.921140
3502.981966	789778.726772	41.926144
3502.825183	789744.130596	41.931149
3502.933643	789709.590574	41.936154
3502.897530	789683.630461	41.941159
3503.112904	789654.648027	41.946164
3503.277287	789619.267488	41.951168
3502.815172	789591.368689	41.956173
3502.742017	789541.599173	41.961178
3502.812701	789526.673357	41.966183
3503.323874	789488.206036	41.971188
3503.094123	789468.436915	41.976192
3502.564398	789423.676931	41.981197
3502.700620	789379.937290	41.986202
3502.971317	789368.794218	41.991207
3502.538771	789321.964456	41.996212
3503.021227	789295.481628	42.001216
3502.766537	789269.651859	42.006221
3502.762505	789235.469260	42.011226
3502.748269	789209.454957	42.016231
3502.629885	789165.362467	42.021236
3502.388210	789139.725769	42.026240
3502.521527	789128.016920	42.031245
3502.719332	789096.589579	42.036250
3502.542683	789070.257786	42.041255
3502.891794	789042.132037	42.046260
3502.624276	789012.244175	42.051264
3502.498097	788988.985175	42.056269
3502.550677	788957.824401	42.061274
3502.487101	788932.599204	42.066279
3502.492937	788909.270381	42.071284
3502.539016	788883.245364	42.076288
3502.480180	788863.398802	42.081293
3502.528689	788836.884162	42.086298
3502.611473	788826.600958	42.091303
3502.480555	788790.968704	42.096308
3502.323089	788764.730505	42.101312
3502.388362	788742.272121	42.106317
3502.604761	788712.111624	42.111322
3502.641117	788695.917711	42.116327
3502.270480	788659.001722	42.121332
3502.708163	788639.027961	42.126336
3502.352803	788614.385145	42.131341
3502.013087	788588.174733	42.136346
3501.923990	788570.288342	42.141351
3502.364836	788548.357487	42.146356
3502.044581	788532.170010	42.151360
3502.098924	788510.592899	42.156365
3502.208976	788486.855024	42.161370
3501.987778	788479.700052	42.166375
3502.239246	788447.576513	42.171380
3502.222270	788427.917735	42.176384
3502.112441	788402.551015	42.181389
3502.460529	788395.698235	42.186394
3502.009923	788376.253818	42.191399
3502.054117	788347.879324	42.196404
3502.227137	788328.435099	42.201408
3501.939862	788303.976118	42.206413
3502.354543	788279.309495	42.211418
3502.237924	788264.899210	42.216423
3502.376409	788241.107098	42.221428
3501.807220	788227.207673	42.226432
3501.606955	788206.158476	42.231437
3501.797750	788173.015960	42.236442
3501.812050	788172.964859	42.241447
3501.898995	788153.484664	42.246452
3501.916961	788139.982381	42.251456
3502.052209	788118.293521	42.256461
3502.499060	788100.957928	42.261466
3502.386186	788085.177140	42.266471
3502.264649	788061.376116	42.271476
3502.357662	788035.878456	42.276480
3502.042223	788010.933671	42.281485
3502.255968	787996.568982	42.286490
3501.889984	787976.572120	42.291495
3502.151094	787950.509816	42.296500
3502.220668	787927.314300	42.301504
3502.204179	787907.556073	42.306509
3501.871900	787886.575407	42.311514
3501.582844	787877.914079	42.316519
3501.882073	787852.530216	42.321524
3502.047817	787851.134774	42.326528
3502.062232	787839.491146	42.331533
3502.112622	787817.080861	42.336538
3502.184724	787793.199687	42.341543
3502.217573	787773.531175	42.346548
3501.860883	787755.048524	42.351552
3501.999620	787742.113521	42.356557
3501.953223	787713.995042	42.361562
3501.881929	787708.576720	42.366567
3501.851807	787685.493771	42.371572
3501.762094	787670.588836	42.376576
3501.828630	787668.328399	42.381581
3501.987969	787645.655927	42.386586
3501.544048	787631.197595	42.391591
3501.471521	787604.648018	42.396596
3501.260143	787588.343373	42.401600
3501.240010	787595.977368	42.406605
3501.775077	787577.012410	42.411610
3501.606937	787575.620189	42.416615
3501.459800	787561.066393	42.421620
3502.115162	787553.235317	42.426624
3501.707380	787536.423174	42.431629
3501.890054	787526.513662	42.436634
3501.656894	787510.945969	42.441639
3501.662909	787492.503716	42.446644
3501.766479	787468.616453	42.451648
3501.695917	787455.615777	42.456653
3501.881132	787454.608541	42.461658
3501.768095	787437.407655	42.466663
3501.874368	787424.721691	42.471668
3501.996156	787405.478431	42.476672
3501.201383	787396.993358	42.481677
3501.366399	787395.304435	42.486682
3500.980323	787372.667373	42.491687
3501.307360	787365.083069	42.496692
3501.591244	787366.017079	42.501696
3501.692206	787364.827332	42.506701
3501.790111	787336.537940	42.511706
3501.873361	787338.432745	42.516711
3501.687412	787320.215690	42.521716
3501.701218	787302.798956	42.526720
3501.421681	787294.331042	42.531725
3501.588700	787269.405873	42.536730
3501.401466	787264.249900	42.541735
3501.221617	787264.424813	42.546740
3501.337929	787255.259037	42.551744
3501.325686	787236.623254	42.556749
3501.897375	787229.196224	42.561754
3501.439862	787227.066474	42.566759
3501.334948	787199.737647	42.571764
3501.202415	787195.306843	42.576768
3501.319966	787192.402331	42.581773
3501.591999	787187.321259	42.586778
3501.485978	787177.065008	42.591783
3501.654193	787163.732921	42.596788
3501.524894	787158.078622	42.601792
3501.405246	787142.736911	42.606797
3501.638455	787137.515114	42.611802
3501.104199	787133.293823	42.616807
3501.190849	787115.278184	42.621812
3501.506337	787105.445120	42.626816
3501.506118	787098.596536	42.631821
3501.477448	787090.089144	42.636826
3501.086722	787077.626965	42.641831
3501.379953	787072.102219	42.646836
3501.662271	787063.056985	42.651840
3501.544823	787063.417825	42.656845
3501.687738	787036.881213	42.661850
3501.759276	787028.113479	42.666855
3501.369338	787025.434984	42.671860
3501.683845	787005.328804	42.676864
3501.524632	787006.185373	42.681869
3501.729085	786996.418425	42.686874
3501.172709	786985.743079	42.691879
3501.455631	786971.120758	42.696884
3501.537669	786978.935172	42.701888
3501.298069	786958.768710	42.706893
3501.370089	786937.672910	42.711898
3501.653407	786940.612800	42.716903
3501.521362	786929.088307	42.721908
3501.919205	786907.501195	42.726912
3501.790123	786902.286928	42.731917
3501.639456	786877.312106	42.736922
3501.208212	786875.960864	42.741927
3501.502053	786876.208500	42.746932
3501.435160	786862.863641	42.751936
3501.197634	786846.414491	42.756941
3501.758851	786827.590072	42.761946
3501.609706	786831.037904	42.766951
3501.697449	786806.465836	42.771956
3501.848370	786801.501246	42.776960
3501.383996	786783.375157	42.781965
3501.635888	786768.757241	42.786970
3501.526202	786771.073742	42.791975
3501.691862	786759.355651	42.796980
3501.681236	786756.715593	42.801985
3501.339348	786747.963195	42.806989
3501.463095	786730.919146	42.811994
3501.260274	786712.360602	42.816999
3501.553651	786713.537833	42.822004
3501.624986	786706.922269	42.827009
3501.305089	786693.518775	42.832013
3501.553615	786669.899508	42.837018
3501.464927	786680.040306	42.842023
3501.633561	786658.879595	42.847028
3501.646295	786648.848572	42.852033
3501.309049	786645.672460	42.857037
3501.488367	786624.118588	42.862042
3501.332873	786617.538393	42.867047
3501.593063	786610.795366	42.872052
3501.338556	786596.843305	42.877057
3501.630625	786570.917510	42.882061
3501.708269	786565.670661	42.887066
3501.294960	786573.024835	42.892071
3501.402638	786554.906542	42.897076
3501.637084	786549.830861	42.902081
3501.301105	786551.987120	42.907085
3501.581773	786542.745746	42.912090
3501.427962	786527.554719	42.917095
3501.232892	786520.589228	42.922100
3501.983887	786514.650000	42.927105
3501.415586	786505.100975	42.932109
3501.758392	786481.710918	42.937114
3501.331673	786465.192549	42.942119
3501.366257	786456.038446	42.947124
3501.549168	786441.283822	42.952129
3501.684638	786451.487777	42.957133
3501.700096	786421.152568	42.962138
3501.356967	786413.133780	42.967143
3501.270089	786413.538799	42.972148
3501.364120	786395.617901	42.977153
3501.636039	786382.023413	42.982157
3501.753191	786375.547130	42.987162
3501.457907	786364.487492	42.992167
3501.115248	786341.546565	42.997172
3501.142021	786349.761758	43.002177
3501.323979	786343.030690	43.007181
3501.535230	786339.768687	43.012186
3501.389851	786329.566200	43.017191
3501.155338	786319.328706	43.022196
3501.553913	786316.379881	43.027201
3501.087811	786299.965105	43.032205
3501.411316	786288.955385	43.037210
3501.532991	786287.419734	43.042215
3501.567687	786280.662698	43.047220
3501.765120	786271.825360	43.052225
3501.238985	786258.355373	43.057229
3501.422000	786254.755265	43.062234
3501.503580	786248.626897	43.067239
3501.667670	786234.804338	43.072244
3501.232246	786221.711499	43.077249
3501.350541	786227.808739	43.082253
3501.212253	786204.297210	43.087258
3501.273698	786199.982192	43.092263
3501.084625	786193.260047	43.097268
3500.926923	786192.844413	43.102273
3501.272323	786202.722380	43.107277
3501.563500	786188.194898	43.112282
3501.158628	786173.433712	43.117287
3500.958180	786157.123832	43.122292
3501.418933	786167.913412	43.127297
3501.028275	786176.291925	43.132301
3501.577185	786156.733648	43.137306
3501.189974	786145.981569	43.142311
3501.013792	786139.697689	43.147316
3501.377794	786135.971373	43.152321
3501.404653	786134.401583	43.157325
3501.148031	786115.066958	43.162330
3500.995742	786115.188662	43.167335
3501.393622	786103.139556	43.172340
3500.980341	786103.448838	43.177345
3500.960713	786111.818358	43.182349
3501.291297	786110.250010	43.187354
3500.995077	786083.582528	43.192359
3500.866971	786077.291074	43.197364
3501.543089	786076.011189	43.202369
3500.934820	786086.968014	43.207373
3501.355211	786080.590820	43.212378
3501.420382	786053.964579	43.217383
3501.178052	786049.745878	43.222388
3501.404308	786053.184355	43.227393
3500.929040	786053.356549	43.232397
3501.402709	786032.195084	43.237402
3501.246132	786023.412756	43.242407
3501.243174	786028.159179	43.247412
3501.551019	786017.004677	43.252417
3501.446309	786019.858857	43.257421
3501.543899	785992.199834	43.262426
3501.309261	785983.087165	43.267431
3500.890421	785983.152684	43.272436
3501.384702	785981.950135	43.277441
3501.592372	785975.361458	43.282445
3501.232601	785963.919812	43.287450
3501.216152	785953.696591	43.292455
3501.103020	785962.031989	43.297460
3501.424965	785946.275985	43.302465
3501.175401	785935.550975	43.307469
3501.525727	785926.836061	43.312474
3501.157925	785933.205271	43.317479
3501.264591	785925.849492	43.322484
3501.454560	785900.475248	43.327489
3501.261150	785904.175117	43.332493
3501.846480	785891.313481	43.337498
3501.390627	785880.620629	43.342503
3501.462093	785858.885423	43.347508
3501.517241	785856.675079	43.352513
3501.465335	785848.316510	43.357517
3501.596156	785829.360840	43.362522
3501.647808	785827.151033	43.367527
3501.267408	785813.265929	43.372532
3501.474380	785792.341108	43.377537
3501.162442	785793.613133	43.382541
3501.303870	785788.404629	43.387546
3501.494967	785779.127270	43.392551
3501.334734	785761.048693	43.397556
3501.312861	785759.926792	43.402561
3501.298000	785753.519470	43.407565
3501.343567	785748.619494	43.412570
3500.999984	785732.771305	43.417575
3500.912998	785736.014269	43.422580
3501.121756	785730.746266	43.427585
3500.771651	785750.666238	43.432589
3500.883656	785737.878297	43.437594
3501.322111	785744.317367	43.442599
3500.756653	785741.323276	43.447604
3500.789831	785750.712506	43.452609
3500.274346	785753.533156	43.457613
3501.361870	785739.663073	43.462618
3501.503154	785727.751260	43.467623
3501.250082	785713.552467	43.472628
3501.231303	785715.855123	43.477633
3501.024100	785720.046543	43.482637
3501.131857	785707.014561	43.487642
3500.798308	785689.452174	43.492647
3501.187039	785682.590257	43.497652
3500.959987	785683.653315	43.502657
3501.124199	785688.814213	43.507661
3501.018352	785684.329295	43.512666
3501.209055	785702.060904	43.517671
3501.027672	785703.557183	43.522676
3501.370111	785674.782119	43.527681
3501.047739	785668.080278	43.532685
3501.349823	785664.950536	43.537690
3501.026356	785658.689223	43.542695
3501.275989	785663.445350	43.547700
3501.503726	785660.425087	43.552705
3501.517919	785630.869341	43.557709
3501.537376	785628.370921	43.562714
3501.602111	785620.972431	43.567719
3501.346444	785605.844144	43.572724
3501.451234	785600.494431	43.577729
3501.387392	785615.134537	43.582733
3501.166903	785575.976020	43.587738
3501.416684	785573.441574	43.592743
3501.075033	785566.840505	43.597748
3501.533296	785574.744554	43.602753
3501.079084	785560.772598	43.607757
3501.559858	785535.889738	43.612762
3501.175921	785526.457265	43.617767
3501.011973	785534.165044	43.622772
3501.262046	785538.040442	43.627777
3501.152184	785529.348018	43.632781
3501.168995	785507.669139	43.637786
3501.436655	785515.700916	43.642791
3501.491907	785505.416866	43.647796
3501.606886	785489.300689	43.652801
3501.639611	785477.747915	43.657805
3501.490372	785467.397911	43.662810
3501.256713	785456.327121	43.667815
3501.184504	785443.127031	43.672820
3501.403699	785438.835791	43.677825
3500.994529	785437.040410	43.682829
3501.130942	785441.863327	43.687834
3501.552684	785424.916140	43.692839
3501.314455	785409.001777	43.697844
3501.110764	785402.672566	43.702849
3501.406926	785405.268617	43.707853
3501.354779	785390.401614	43.712858
3501.589351	785384.199602	43.717863
3501.162871	785382.064390	43.722868
3500.998752	785370.884722	43.727873
3501.003823	785384.046610	43.732877
3500.933273	785362.283050	43.737882
3501.292735	785351.902277	43.742887
3500.858152	785354.612580	43.747892
3501.228289	785352.597489	43.752897
3500.911621	785346.726273	43.757901
3501.326642	785347.591148	43.762906
3501.243392	785345.108677	43.767911
3500.952959	785329.593740	43.772916
3501.207905	785309.736408	43.777921
3501.054446	785317.442798	43.782925
3501.389519	785316.509685	43.787930
3501.062071	785316.463053	43.792935
3500.983086	785303.704135	43.797940
3501.192657	785288.942789	43.802945
3500.856546	785293.986477	43.807949
3501.107072	785287.341490	43.812954
3500.820110	785291.105255	43.817959
3500.883474	785286.446819	43.822964
3501.157831	785282.831910	43.827969
3500.787963	785289.838174	43.832973
3501.077300	785299.090135	43.837978
3500.994811	785281.976745	43.842983
3500.980373	785272.975474	43.847988
3500.982544	785270.088162	43.852993
3501.144033	785282.442879	43.857997
3501.131901	785267.080020	43.863002
3501.033699	785276.147931	43.868007
3501.109400	785283.524942	43.873012
3501.154691	785249.460855	43.878017
3500.861708	785246.913269	43.883021
3501.190948	785247.155442	43.888026
3500.998226	785242.488075	43.893031
3501.110775	785246.091547	43.898036
3501.219274	785242.062149	43.903041
3501.097459	785235.426383	43.908045
3501.305826	785211.710350	43.913050
3501.011507	785209.211891	43.918055
3500.833982	785217.851884	43.923060
3500.923888	785212.553119	43.928065
3500.790204	785223.535032	43.933069
3501.001595	785221.740449	43.938074
3501.048625	785221.782076	43.943079
3501.070592	785216.885398	43.948084
3501.349608	785195.213445	43.953089
3500.947403	785188.229998	43.958093
3501.169996	785184.133797	43.963098
3501.468864	785183.940323	43.968103
3500.871053	785196.707494	43.973108
3501.081945	785173.186662	43.978113
3500.819295	785162.413512	43.983117
3501.154849	785156.146569	43.988122
3500.781040	785158.798517	43.993127
3500.608326	785160.440361	43.998132
3500.723615	785158.562918	44.003137
3501.023546	785165.856074	44.008141
3500.958767	785158.770915	44.013146
3501.039042	785176.227591	44.018151
3500.727947	785167.076817	44.023156
3500.966037	785173.939233	44.028161
3501.002913	785175.058977	44.033165
3500.894423	785144.394783	44.038170
3501.105437	785145.976646	44.043175
3500.901297	785149.287142	44.048180
3501.332460	785138.845896	44.053185
3500.841743	785147.192405	44.058189
3501.049141	785148.138698	44.063194
3501.183056	785145.720072	44.068199
3500.902791	785137.836708	44.073204
3501.196555	785119.881149	44.078209
3500.923137	785118.406993	44.083213
3501.125235	785115.096892	44.088218
3501.120220	785111.721297	44.093223
3500.985519	785115.999629	44.098228
3501.088026	785123.079026	44.103233
3501.148919	785117.246451	44.108237
3501.145986	785096.596925	44.113242
3501.367216	785093.479558	44.118247
3501.112644	785097.140500	44.123252
3501.433534	785090.484318	44.128257
3500.854081	785084.017807	44.133261
3501.328703	785074.059005	44.138266
3501.320009	785061.435436	44.143271
3500.836607	785068.263943	44.148276
3501.242040	785068.200611	44.153281
3501.248473	785068.150716	44.158285
3501.109403	785059.315441	44.163290
3501.472473	785039.097863	44.168295
3501.147916	785032.395718	44.173300
3501.452005	785044.483915	44.178305
3501.118350	785035.874763	44.183309
3501.211760	785009.582466	44.188314
3501.415175	785004.510464	44.193319
3500.908668	785002.485506	44.198324
3501.338233	784996.986670	44.203329
3501.296997	785004.871616	44.208333
3501.149381	784989.529295	44.213338
3501.327278	784971.689320	44.218343
3500.958923	784970.425709	44.223348
3501.257836	784971.015180	44.228353
3501.060371	784974.960869	44.233357
3500.909065	784946.895996	44.238362
3501.157486	784944.459397	44.243367
3500.764339	784949.952673	44.248372
3501.077188	784944.520975	44.253377
3501.255874	784948.701489	44.258381
3501.210879	784949.246852	44.263386
3501.184250	784947.146860	44.268391
3500.802502	784930.715501	44.273396
3501.075456	784913.300924	44.278401
3501.370596	784910.074048	44.283405
3500.947001	784909.161607	44.288410
3501.514793	784910.394143	44.293415
3501.026634	784910.127953	44.298420
3501.129540	784883.197515	44.303425
3501.350525	784880.569441	44.308429
3501.195439	784875.798061	44.313434
3501.386002	784872.832191	44.318439
3501.284456	784873.728948	44.323444
3501.537648	784849.515266	44.328449
3501.494020	784848.200870	44.333453
3501.156666	784841.745210	44.338458
3501.412347	784845.766946	44.343463
3500.898636	784835.423996	44.348468
3501.307166	784825.670901	44.353473
3501.288583	784827.582346	44.358477
3501.369659	784819.837861	44.363482
3501.611825	784808.936288	44.368487
3501.313239	784798.363908	44.373492
3501.251223	784792.746007	44.378497
3501.120458	784796.143078	44.383501
3501.042963	784781.278676	44.388506
3501.137311	784763.598013	44.393511
3501.068652	784767.768370	44.398516
3501.070592	784761.846828	44.403521
3501.137136	784770.057757	44.408525
3501.019111	784762.833691	44.413530
3501.309216	784761.809662	44.418535
3500.889313	784754.388096	44.423540
3500.827527	784739.570081	44.428545
3501.126894	784741.872276	44.433549
3501.480249	784734.965984	44.438554
3501.504688	784737.360095	44.443559
3500.855881	784727.135967	44.448564
3501.291580	784704.997500	44.453569
3501.295832	784710.184166	44.458573
3501.092559	784709.139382	44.463578
3501.230903	784703.979451	44.468583
3501.086779	784714.865960	44.473588
3501.026415	784690.211349	44.478593
3501.218996	784686.706778	44.483597
3501.046406	784681.106067	44.488602
3501.293973	784661.150085	44.493607
3501.069355	784673.076922	44.498612
3501.128835	784662.203667	44.503617
3501.194404	784646.142111	44.508621
3501.045913	784650.031399	44.513626
3501.062034	784643.716038	44.518631
3501.022856	784640.492357	44.523636
3500.987113	784647.006627	44.528641
3500.889519	784649.615595	44.533645
3501.160369	784642.526357	44.538650
3500.934973	784623.671877	44.543655
3500.617389	784622.253449	44.548660
3501.142818	784621.681985	44.553665
3500.959454	784627.142731	44.558669
3501.235108	784627.050748	44.563674
3501.486575	784628.137040	44.568679
3501.240083	784620.883965	44.573684
3501.475020	784601.712776	44.578689
3501.137524	784594.669648	44.583693
3500.821982	784592.663645	44.588698
3501.423112	784593.646346	44.593703
3501.143180	784587.719774	44.598708
3501.420137	784564.920532	44.603713
3501.383895	784549.706600	44.608717
3500.701095	784558.524307	44.613722
3501.106797	784557.922617	44.618727
3500.999958	784571.152544	44.623732
3501.268787	784553.248297	44.628737
3501.488079	784542.643491	44.633741
3501.268815	784526.381483	44.638746
3501.326911	784527.889524	44.643751
3501.247092	784523.791256	44.648756
3501.632832	784505.428163	44.653761
3501.105447	784490.095118	44.658765
3501.085626	784497.977316	44.663770
3501.433439	784492.539787	44.668775
3501.024850	784479.096738	44.673780
3500.983032	784461.925943	44.678785
3501.166634	784463.267564	44.683789
3501.265909	784458.456121	44.688794
3501.783783	784452.894098	44.693799
3501.165369	784437.819856	44.698804
3501.497776	784422.988454	44.703809
3501.854086	784430.273608	44.708813
3501.231654	784405.754746	44.713818
3501.192137	784396.217882	44.718823
3500.994993	784398.646753	44.723828
3501.160032	784390.790767	44.728833
3501.052329	784389.143723	44.733837
3501.382411	784378.961790	44.738842
3501.108936	784348.760173	44.743847
3501.584742	784353.041434	44.748852
3501.222478	784358.824000	44.753857
3501.386080	784358.211200	44.758861
3501.175698	784343.415533	44.763866
3501.543370	784332.346745	44.768871
3501.254788	784327.987353	44.773876
3501.203122	784320.899252	44.778881
3501.277048	784297.739320	44.783885
3501.141318	784291.838881	44.788890
3501.814728	784287.231203	44.793895
3501.413101	784287.832369	44.798900
3501.579506	784265.881363	44.803905
3501.339143	784255.984176	44.808909
3501.100110	784260.034664	44.813914
3501.007728	784252.218755	44.818919
3501.064718	784244.575248	44.823924
3501.093187	784222.303080	44.828929
3501.622124	784231.323316	44.833933
3500.941367	784226.437881	44.838938
3501.109123	784225.383958	44.843943
3501.177998	784227.184024	44.848948
3500.979396	784205.436698	44.853953
3501.183133	784198.846886	44.858957
3501.178398	784192.289656	44.863962
3501.176866	784186.319205	44.868967
3501.206624	784194.683415	44.873972
3501.317524	784172.740780	44.878977
3501.027698	784163.878940	44.883981
3500.830757	784158.036891	44.888986
3501.173468	784153.187174	44.893991
3500.786217	784166.119153	44.898996
3500.680129	784161.241718	44.904001
3501.009674	784176.606540	44.909005
3500.815522	784159.067254	44.914010
3501.263408	784168.491770	44.919015
3500.833325	784156.960112	44.924020
3500.776267	784137.931118	44.929025
3500.816314	784135.331038	44.934029
3500.626835	784133.794595	44.939034
3501.179363	784132.337924	44.944039
3500.902520	784137.715800	44.949044
3500.978975	784138.340124	44.954049
3500.771119	784135.974561	44.959053
3501.129448	784141.840432	44.964058
3501.158429	784137.773858	44.969063
3500.840133	784138.655654	44.974068
3500.999717	784128.597875	44.979073
3500.923181	784110.942194	44.984077
3500.852659	784113.596079	44.989082
3501.177741	784109.042732	44.994087
3500.962269	784110.544692	44.999092
3501.264541	784102.666914	45.004097
3501.177884	784114.866828	45.009101
3501.128892	784112.916891	45.014106
3501.215590	784089.558476	45.019111
3501.237523	784087.352739	45.024116
3501.302548	784080.246140	45.029121
3501.310673	784075.938083	45.034125
3501.048123	784071.085040	45.039130
3501.291207	784054.847486	45.044135
3500.984120	784051.665400	45.049140
3500.784081	784043.278777	45.054145
3500.880648	784048.255762	45.059149
3501.153886	784051.247466	45.064154
3501.268112	784041.881827	45.069159
3501.237962	784033.713343	45.074164
3500.784223	784017.927220	45.079169
3500.966369	784006.446420	45.084173
3500.655699	784019.170944	45.089178
3500.777921	784013.915119	45.094183
3500.600757	784017.466664	45.099188
3501.082203	784013.084575	45.104193
3501.004213	784019.312412	45.109197
3500.801266	784021.987034	45.114202
3501.077993	784014.504680	45.119207
3500.608105	784030.141636	45.124212
3500.782143	784018.270590	45.129217
3500.823341	784019.487738	45.134221
3500.824523	784021.200558	45.139226
3500.922536	784022.408824	45.144231
3500.884827	784016.248109	45.149236
3500.776733	784003.148655	45.154241
3501.023678	783999.292634	45.159245
3501.087990	784000.604056	45.164250
3500.950040	783997.395503	45.169255
3500.975473	784006.543696	45.174260
3501.005328	783996.359172	45.179265
3500.867252	784006.511762	45.184269
3500.538768	784011.163685	45.189274
3500.983058	783996.313847	45.194279
3501.134025	784010.483422	45.199284
3501.209315	783992.461101	45.204289
3501.237450	783975.229176	45.209293
3501.203384	783974.891952	45.214298
3501.458309	783979.550581	45.219303
3501.129120	783965.506775	45.224308
3500.999768	783943.356232	45.229313
3501.321000	783936.013660	45.234317
3501.166191	783935.059059	45.239322
3500.853936	783930.849933	45.244327
3500.958191	783944.048104	45.249332
3501.204311	783933.976504	45.254337
3501.201842	783925.509907	45.259341
3501.508054	783909.751557	45.264346
3501.586509	783902.006417	45.269351
3501.033134	783914.181770	45.274356
3501.099963	783899.097068	45.279361
3501.029133	783887.508782	45.284365
3500.886634	783874.169739	45.289370
3501.025985	783872.239232	45.294375
3500.896986	783883.467332	45.299380
3501.140145	783873.200333	45.304385
3501.238735	783875.876819	45.309389
3501.165941	783876.084014	45.314394
3501.294750	783856.780449	45.319399
3500.965429	783851.741911	45.324404
3501.202036	783840.594914	45.329409
3501.255866	783852.381801	45.334413
3501.491350	783854.841124	45.339418
3501.309457	783825.895336	45.344423
3500.709598	783822.661019	45.349428
3501.248777	783819.933848	45.354433
3501.092436	783813.302058	45.359437
3501.149207	783824.452274	45.364442
3501.498543	783808.099625	45.369447
3501.094421	783795.339698	45.374452
3500.934255	783785.869764	45.379457
3501.500584	783788.277394	45.384461
3501.345288	783787.420734	45.389466
3501.387412	783769.305109	45.394471
3501.167787	783759.012391	45.399476
3500.969535	783759.288146	45.404481
3501.170611	783756.271197	45.409485
3500.536953	783759.453746	45.414490
3501.210997	783753.573074	45.419495
3501.016025	783753.407823	45.424500
3500.634529	783735.603046	45.429505
3501.017231	783724.188298	45.434509
3500.796242	783720.992592	45.439514
3500.901769	783719.409936	45.444519
3500.684550	783733.148218	45.449524
3500.779795	783722.414672	45.454529
3500.822705	783732.441498	45.459533
3500.564471	783747.801307	45.464538
3500.856179	783740.071587	45.469543
3500.463866	783743.901627	45.474548
3500.851354	783743.890043	45.479553
3500.816484	783744.287089	45.484557
3500.543086	783750.643611	45.489562
3500.798873	783745.709301	45.494567
3500.607677	783748.480082	45.499572
3501.071960	783749.582198	45.504577
3500.728434	783751.104255	45.509581
3500.870736	783752.011985	45.514586
3500.644042	783748.866128	45.519591
3500.379514	783759.332523	45.524596
3500.765351	783759.125423	45.529601
3500.598742	783758.172641	45.534605
3500.763582	783769.942321	45.539610
3501.096492	783762.842452	45.544615
3500.907898	783764.780778	45.549620
3500.518045	783760.192125	45.554625
3501.084247	783775.961371	45.559629
3501.440846	783777.422920	45.564634
3500.967824	783738.146234	45.569639
3501.008864	783742.300083	45.574644
3500.802903	783733.522445	45.579649
3500.594299	783742.267092	45.584653
3500.886554	783750.052445	45.589658
3501.411055	783738.224005	45.594663
3501.169417	783750.106205	45.599668
3500.769638	783738.275420	45.604673
3501.129403	783724.661788	45.609677
3500.987174	783716.901987	45.614682
3501.123078	783708.756091	45.619687
3500.942679	783725.767878	45.624692
3500.983928	783707.652222	45.629697
3500.948786	783703.350688	45.634701
3500.498380	783710.615909	45.639706
3501.025500	783711.903985	45.644711
3500.773355	783715.956850	45.649716
3501.017867	783713.471476	45.654721
3501.061865	783712.583652	45.659725
3500.890416	783695.088539	45.664730
3501.074891	783678.076127	45.669735
3500.918009	783685.638101	45.674740
3501.130119	783673.662604	45.679745
3501.284974	783674.813104	45.684749
3500.775237	783679.248868	45.689754
3501.246772	783676.336437	45.694759
3501.155229	783665.093612	45.699764
3501.106867	783651.396798	45.704769
3501.260032	783649.806679	45.709773
3500.939142	783655.877047	45.714778
3501.322474	783651.069563	45.719783
3501.214834	783639.682378	45.724788
3501.275223	783619.997269	45.729793
3501.459656	783607.438644	45.734797
3501.224112	783619.369069	45.739802
3501.072737	783609.799621	45.744807
3500.998697	783599.386009	45.749812
3500.950132	783581.724554	45.754817
3501.113182	783567.358235	45.759821
3500.631473	783520.984594	45.764826
3500.656573	783424.166087	45.769831
3500.600304	783274.202479	45.774836
3500.313496	783075.763633	45.779841
3500.513733	782827.949846	45.784845
3499.947937	782531.098384	45.789850
3499.739133	782176.655823	45.794855
3499.158018	781788.961317	45.799860
3498.744127	781350.004969	45.804865
3498.287575	780862.649513	45.809869
3497.693261	780316.077218	45.814874
3497.290387	779737.108448	45.819879
3496.655553	779111.646604	45.824884
3495.867716	778436.482605	45.829889
3495.356286	777712.808176	45.834893
3494.587201	776950.343026	45.839898
3494.054369	776135.767220	45.844903
3493.125389	775292.830572	45.849908
3492.296287	774380.373426	45.854913
3491.487439	773430.046600	45.859917
3489.958202	772442.636684	45.864922
3489.210679	771404.654126	45.869927
3488.041135	770328.034331	45.874932
3486.895569	769186.007198	45.879937
3486.025656	768017.060422	45.884941
3484.431797	766805.096347	45.889946
3483.170166	765545.707347	45.894951
3481.743742	764247.142988	45.899956
3480.541013	762911.088660	45.904961
3479.291073	761534.030555	45.909965
3477.885099	760116.895466	45.914970
3476.680373	758652.972552	45.919975
3475.333726	757164.446571	45.924980
3473.603974	755617.234701	45.929985
3472.153373	754029.973460	45.934989
3470.224923	752402.264039	45.939994
3468.916619	750741.973641	45.944999
3466.785862	749038.386618	45.950004
3464.909350	747309.608302	45.955009
3463.235815	745530.580734	45.960013
3461.485841	743734.096726	45.965018
3459.404058	741884.783077	45.970023
3457.386358	740008.741157	45.975028
3455.629817	738099.763870	45.980033
3453.759798	736166.164873	45.985037
3451.668201	734189.115546	45.990042
3449.709840	732168.478889	45.995047
3447.661978	730135.572799	46.000052
3445.258310	728057.726068	46.005057
3443.262309	725954.473047	46.010061
3440.835432	723825.383745	46.015066
3438.944960	721642.294756	46.020071
3436.580756	719445.718550	46.025076
3434.022095	717218.807318	46.030081
3432.100023	714962.890799	46.035085
3429.096751	712686.272821	46.040090
3426.832796	710371.744722	46.045095
3423.984532	708038.722964	46.050100
3421.277149	705673.922017	46.055105
3418.904214	703292.034583	46.060109
3416.124426	700893.215030	46.065114
3413.656418	698453.621459	46.070119
3411.234498	695999.713122	46.075124
3408.427598	693525.355656	46.080129
3405.907535	691012.042537	46.085133
3403.093038	688492.009560	46.090138
3400.214744	685921.528434	46.095143
3397.791007	683360.948685	46.100148
3394.340424	680757.072271	46.105153
3392.079136	678133.890369	46.110157
3389.155755	675499.575141	46.115162
3385.919327	672833.851828	46.120167
3383.115143	670157.100158	46.125172
3380.261519	667452.741567	46.130177
3377.256777	664725.892897	46.135181
3373.893817	661998.652177	46.140186
3371.430377	659235.757360	46.145191
3368.106684	656459.152939	46.150196
3365.174262	653654.699156	46.155201
3362.547276	650842.954492	46.160205
3358.988161	648020.775183	46.165210
3356.208309	645168.409610	46.170215
3352.389527	642298.381356	46.175220
3349.431215	639419.955952	46.180225
3346.932996	636529.604800	46.185229
3343.492609	633622.006126	46.190234
3340.368955	630687.972354	46.195239
3337.211301	627753.148001	46.200244
3333.728442	624794.018133	46.205249
3330.873028	621815.613475	46.210253
3327.397848	618825.813172	46.215258
3324.095169	615815.994811	46.220263
3320.873348	612800.059933	46.225268
3317.166490	609779.249563	46.230273
3314.336440	606723.091905	46.235277
3311.163808	603676.585974	46.240282
3307.680052	600615.269013	46.245287
3304.300558	597536.818251	46.250292
3300.679463	594446.839820	46.255297
3297.395104	591352.254699	46.260301
3294.044086	588236.694908	46.265306
3290.838762	585120.617777	46.270311
3287.284570	581993.730417	46.275316
3283.806207	578841.973617	46.280321
3280.395270	575682.141661	46.285325
3277.008859	572523.225349	46.290330
3273.164166	569354.217066	46.295335
3269.559545	566163.510634	46.300340
3266.085175	562979.589474	46.305345
3262.559639	559772.556809	46.310349
3258.921496	556580.651184	46.315354
3255.833113	553376.799901	46.320359
3252.006670	550158.790698	46.325364
3248.195281	546942.344298	46.330369
3245.091329	543689.989231	46.335373
3241.129890	540463.485494	46.340378
3237.801948	537221.512079	46.345383
3233.618295	533974.014841	46.350388
3229.960471	530725.666942	46.355393
3226.976488	527468.294879	46.360397
3222.912383	524208.472719	46.365402
3219.414595	520930.430534	46.370407
3215.480564	517664.007796	46.375412
3211.538626	514389.241910	46.380417
3208.619070	511107.034169	46.385421
3204.302118	507835.168064	46.390426
3200.711877	504546.085545	46.395431
3197.366383	501256.259233	46.400436
3193.284195	497967.567609	46.405441
3189.475282	494674.309764	46.410445
3185.572038	491380.690137	46.415450
3182.019609	488073.921031	46.420455
3178.650808	484778.681392	46.425460
3174.878311	481478.153478	46.430465
3171.296528	478161.031110	46.435469
3167.492919	474853.460614	46.440474
3163.506097	471530.576734	46.445479
3160.086556	468210.669191	46.450484
3156.215920	464888.800204	46.455489
3152.355643	461569.155387	46.460493
3148.532907	458254.929008	46.465498
3145.020844	454933.540218	46.470503
3141.098075	451607.992429	46.475508
3136.796421	448280.971022	46.480513
3133.529492	444958.390587	46.485517
3129.391024	441644.764718	46.490522
3125.648299	438322.079158	46.495527
3122.221505	435007.779073	46.500532
3118.311425	431684.622852	46.505537
3114.694683	428360.095889	46.510541
3110.563712	425037.222439	46.515546
3106.902181	421715.605370	46.520551
3103.154571	418388.547105	46.525556
3099.170315	415075.602382	46.530561
3095.250975	411757.770429	46.535565
3091.529625	408430.421189	46.540570
3087.831100	405114.338053	46.545575
3083.679970	401810.218552	46.550580
3080.120485	398491.168224	46.555585
3076.601094	395181.081512	46.560589
3072.616990	391870.608069	46.565594
3068.361432	388558.558897	46.570599
3064.292757	385258.301638	46.575604
3060.546148	381958.300751	46.580609
3057.004876	378657.517028	46.585613
3052.949149	375366.180431	46.590618
3049.141089	372076.563675	46.595623
3045.204488	368794.171744	46.600628
3041.603313	365500.040220	46.605633
3037.598272	362213.017119	46.610637
3033.594981	358932.364095	46.615642
3030.119799	355652.799470	46.620647
3026.291059	352377.367995	46.625652
3022.163074	349104.673032	46.630657
3018.439927	345824.241175	46.635661
3014.558365	342558.541951	46.640666
3010.888592	339295.604402	46.645671
3006.733244	336034.326302	46.650676
3002.891832	332786.723163	46.655681
2998.931961	329531.483773	46.660685
2994.933090	326292.665861	46.665690
2991.329350	323052.304791	46.670695
2986.969960	319818.958702	46.675700
2983.049581	316572.096314	46.680705
2979.372177	313343.941433	46.685709
2975.386349	310131.818906	46.690714
2971.603187	306909.245010	46.695719
2967.406367	303705.895006	46.700724
2963.558094	300499.976862	46.705729
2959.822399	297303.472507	46.710733
2955.734170	294109.388068	46.715738
2951.672679	290932.665964	46.720743
2947.668342	287757.757924	46.725748
2943.669548	284585.978512	46.730753
2940.139993	281426.174205	46.735757
2935.796289	278264.577382	46.740762
2931.862044	275118.674324	46.745767
2927.942424	271979.497198	46.750772
2923.806246	268845.257150	46.755777
2920.083755	265715.558107	46.760781
2915.981251	262601.609284	46.765786
2911.661767	259493.487947	46.770791
2908.038675	256396.534279	46.775796
2903.785364	253300.318821	46.780801
2899.916557	250219.028168	46.785805
2895.736213	247148.984568	46.790810
2891.945803	244072.513115	46.795815
2887.831021	241023.401401	46.800820
2883.767423	237982.777440	46.805825
2879.783747	234937.552943	46.810829
2875.511206	231912.293470	46.815834
2871.140715	228907.383807	46.820839
2867.086558	225900.378734	46.825844
2863.151034	222910.570403	46.830849
2859.328715	219932.261122	46.835853
2854.934906	216967.321688	46.840858
2850.755038	214010.032337	46.845863
2846.835263	211069.891747	46.850868
2842.479733	208135.477413	46.855873
2838.549294	205206.762566	46.860877
2834.445984	202313.337940	46.865882
2830.410598	199413.149635	46.870887
2826.282747	196530.193047	46.875892
2822.076033	193666.864725	46.880897
2817.919737	190805.679696	46.885901
2813.780658	187964.295818	46.890906
2809.585141	185134.249213	46.895911
2805.449576	182315.984661	46.900916
2801.341802	179507.678360	46.905921
2797.379040	176709.825733	46.910925
2793.195576	173933.360140	46.915930
2788.859119	171168.191913	46.920935
2784.724931	168415.555153	46.925940
2780.728717	165682.197288	46.930945
2776.749629	162862.646081	46.935949
2772.792372	160161.518878	46.940954
2768.242192	157458.933081	46.945959
2764.546841	154776.532008	46.950964
2760.111437	152107.707641	46.955969
2756.435748	149451.719172	46.960973
2752.068251	146813.797275	46.965978
2747.545342	144174.697044	46.970983
2743.486418	141564.799484	46.975988
2739.787789	138955.684717	46.980993
2735.832397	136367.122119	46.985997
2731.581832	133798.558814	46.991002
2727.809039	131225.412581	46.996007
2723.352104	128673.501037	47.001012
2719.258452	126138.959382	47.006017
2714.982148	123608.176041	47.011021
2710.843585	121103.105801	47.016026
2706.926335	118606.172614	47.021031
2703.041750	116119.811588	47.026036
2698.639166	113662.636595	47.031041
2694.532582	111194.658785	47.036045
2690.487689	108762.693467	47.041050
2686.569126	106333.979123	47.046055
2682.452067	103923.365786	47.051060
2678.167139	101513.104113	47.056065
2674.319635	99127.353133	47.061069
2670.124791	96756.562135	47.066074
2666.069409	94397.516130	47.071079
2662.152724	92056.073761	47.076084
2657.735373	89721.559559	47.081089
2654.216072	87403.094495	47.086093
2649.866388	85106.779379	47.091098
2646.053805	82814.563187	47.096103
2642.053597	80525.735663	47.101108
2637.647908	78273.533255	47.106113
2633.585284	76014.411976	47.111117
2629.692525	73779.172739	47.116122
2625.465819	71549.669925	47.121127
2621.454759	69341.143833	47.126132
2617.095518	67146.005555	47.131137
2613.354530	64951.516561	47.136141
2609.028425	62797.528184	47.141146
2605.022643	60641.130401	47.146151
2601.084112	58512.996229	47.151156
2596.618367	56392.217895	47.156161
2592.688984	54281.034095	47.161165
2588.438730	52179.121963	47.166170
2584.124816	50102.236147	47.171175
2580.073848	48041.136753	47.176180
2575.827342	46002.882610	47.181185
2571.821535	43974.470834	47.186189
2567.248371	41967.834383	47.191194
2563.502425	39965.898192	47.196199
2559.299194	37988.067581	47.201204
2554.712771	36020.905939	47.206209
2550.354661	34074.426996	47.211213
2546.292549	32150.511487	47.216218
2542.092754	30242.403587	47.221223
2537.724097	28353.400880	47.226228
2533.574429	26482.805536	47.231233
2529.575678	24616.432433	47.236237
2525.061184	22792.227102	47.241242
2520.984084	20977.900751	47.246247
2516.582603	19185.333870	47.251252
2511.952233	17415.577451	47.256257
2507.680551	15669.719085	47.261261
2502.930679	13950.135759	47.266266
2497.039339	12270.060987	47.271271
2489.139693	10698.249811	47.276276
2480.295957	9186.965100	47.281281
2470.323102	7782.544515	47.286285
2460.347940	6498.426198	47.291290
2450.446422	5295.587073	47.296295
2440.618196	4228.543542	47.301300
2431.184041	3269.628330	47.306305
2422.008879	2412.748174	47.311309
2413.605070	1679.387951	47.316314
2404.811545	1051.537042	47.321319
2395.292572	559.129793	47.326324
2383.275208	269.478099	47.331329
2368.439373	194.170302	47.336333
2357.078330	199.086256	47.341338
2352.147215	190.419931	47.346343
2351.431338	194.828500	47.351348
2352.826208	200.760883	47.356353
2354.757759	204.524319	47.361357
2354.882586	211.525459	47.366362
2355.008359	210.556667	47.371367
2353.800119	199.681689	47.376372
2351.585198	197.873652	47.381377
2348.479362	189.804494	47.386381
2344.769013	202.540575	47.391386
2341.389963	193.387824	47.396391
2338.859977	188.332333	47.401396
2335.227688	198.911102	47.406401
2332.674223	184.541705	47.411405
2329.558234	193.850086	47.416410
2326.385735	195.624657	47.421415
2323.563478	189.178501	47.426420
2320.912793	185.527671	47.431425
2317.878304	185.360188	47.436429
2314.051289	191.204644	47.441434
2310.858442	200.718053	47.446439
2307.824034	195.029614	47.451444
2304.523059	187.965472	47.456449
2301.226953	190.790808	47.461453
2297.830446	189.711824	47.466458
2294.075394	189.454591	47.471463
2291.348317	186.144763	47.476468
2287.770811	189.415937	47.481473
2284.628813	185.652152	47.486477
2281.888479	182.195699	47.491482
2277.802157	195.961917	47.496487
2274.740246	187.639132	47.501492
2271.375412	193.465079	47.506497
2267.890689	188.410276	47.511501
2264.501345	186.637297	47.516506
2260.730394	189.404051	47.521511
2257.930575	190.560330	47.526516
2254.400848	191.786512	47.531521
2250.796627	187.243974	47.536525
2247.434622	187.292271	47.541530
2244.141339	182.745383	47.546535
2240.755190	177.501159	47.551540
2236.913622	186.122618	47.556545
2233.802937	178.044773	47.561549
2230.945926	186.274906	47.566554
2227.362462	188.284650	47.571559
2223.442871	185.566389	47.576564
2220.097396	182.036947	47.581569
2217.101137	182.420350	47.586573
2212.894595	181.873103	47.591578
2209.462938	180.147893	47.596583
2206.632162	184.697522	47.601588
2202.764849	195.718065	47.606593
2199.599694	184.801275	47.611597
2196.218108	179.208328	47.616602
2192.821493	185.561300	47.621607
2189.545810	174.380231	47.626612
2185.887905	186.136827	47.631617
2182.139067	169.553153	47.636621
2179.197527	178.647595	47.641626
2175.338535	178.349716	47.646631
2172.060857	163.017992	47.651636
2169.076318	172.090686	47.656641
2165.331199	178.143839	47.661645
2161.652747	173.280747	47.666650
2157.826570	174.328707	47.671655
2154.561442	175.193970	47.676660
2151.133256	183.133821	47.681665
2147.549961	178.363415	47.686669
2144.308288	172.957411	47.691674
2140.765882	178.561225	47.696679
2137.433603	168.129379	47.701684
2134.262656	177.667860	47.706689
2130.400804	175.168401	47.711693
2126.801619	165.585104	47.716698
2123.020015	174.548395	47.721703
2120.209397	174.880631	47.726708
2116.542938	175.327793	47.731713
2113.245041	175.793222	47.736717
2110.036134	173.960424	47.741722
2105.838891	175.923866	47.746727
2102.475964	168.053224	47.751732
2098.802109	176.964861	47.756737
2095.877336	167.383625	47.761741
2092.499688	173.660883	47.766746
2088.459557	165.532365	47.771751
2085.323318	172.559652	47.776756
2081.428834	177.706026	47.781761
2078.015533	175.990644	47.786765
2075.239118	165.449701	47.791770
2071.559795	171.062300	47.796775
2068.152171	170.443890	47.801780
2064.425761	172.083732	47.806785
2060.912670	166.777177	47.811789
2057.475494	172.725226	47.816794
2053.621718	171.151542	47.821799
2050.184244	172.296911	47.826804
2046.866449	173.866495	47.831809
2043.453741	167.300845	47.836813
2039.988579	169.542079	47.841818
2036.499795	173.634700	47.846823
2033.295186	172.446680	47.851828
2029.817858	165.979735	47.856833
2025.938099	168.402908	47.861837
2022.776415	171.821072	47.866842
2018.794236	171.333711	47.871847
2015.536475	167.347677	47.876852
2011.925349	171.658771	47.881857
2008.609776	168.241787	47.886861
2004.949062	164.932597	47.891866
2001.459520	176.454071	47.896871
1998.499757	171.931015	47.901876
1994.769266	175.068020	47.906881
1991.410460	175.460757	47.911885
1987.972895	166.228727	47.916890
1983.789345	168.139449	47.921895
1980.683352	162.380071	47.926900
1977.472865	163.363390	47.931905
1973.570850	168.881145	47.936909
1970.043061	173.008364	47.941914
1966.494036	160.803947	47.946919
1963.343145	162.597382	47.951924
1959.871579	168.557165	47.956929
1956.179422	162.231437	47.961933
1952.777119	172.426271	47.966938
1949.085910	169.650235	47.971943
1945.531738	163.242805	47.976948
1942.168971	164.449286	47.981953
1939.264742	160.107394	47.986957
1935.444476	164.239258	47.991962
1931.890680	173.565597	47.996967
1928.590525	160.436376	48.001972
1924.307743	164.767173	48.006977
1920.986186	165.657155	48.011981
1917.787120	162.063779	48.016986
1914.116424	172.322768	48.021991
1910.966243	159.524438	48.026996
1907.176217	165.698588	48.032001
1904.097558	166.417684	48.037005
1900.818992	164.250995	48.042010
1896.946988	161.936719	48.047015
1893.258530	169.028316	48.052020
1889.644915	171.213730	48.057025
1886.357616	169.203440	48.062029
1882.886645	162.634315	48.067034
1878.978058	170.481720	48.072039
1875.946814	162.502315	48.077044
1872.624607	164.911059	48.082049
1869.495507	169.216370	48.087053
1865.790261	160.174982	48.092058
1861.915600	157.528932	48.097063
1858.610654	162.231931	48.102068
1854.672843	158.842771	48.107073
1850.955132	167.891050	48.112077
1847.705984	165.691300	48.117082
1844.094090	165.557360	48.122087
1841.030687	159.680631	48.127092
1837.767701	158.185424	48.132097
1834.007822	157.777245	48.137101
1830.588897	166.601596	48.142106
1826.835604	174.491159	48.147111
1823.539144	163.316660	48.152116
1819.563511	164.147674	48.157121
1816.509285	166.606250	48.162125
1813.011630	154.659630	48.167130
1809.501615	161.486035	48.172135
1806.117041	160.411674	48.177140
1802.355021	159.352089	48.182145
1798.954444	164.971766	48.187149
1795.689924	160.486980	48.192154
1791.608605	166.820650	48.197159
1788.569947	160.598372	48.202164
1785.100344	158.404669	48.207169
1781.349203	164.474693	48.212173
1777.953025	160.674924	48.217178
1774.351297	162.507328	48.222183
1771.151303	166.943984	48.227188
1767.394425	162.042700	48.232193
1764.025680	154.037061	48.237197
1760.484045	156.483341	48.242202
1757.048991	164.889444	48.247207
1753.338467	162.135489	48.252212
1749.926434	161.954484	48.257217
1746.426151	170.892834	48.262221
1743.019713	161.909143	48.267226
1739.639044	161.653628	48.272231
1736.476630	154.305427	48.277236
1732.315997	157.978081	48.282241
1728.775254	155.381069	48.287245
1725.385570	161.929230	48.292250
1722.061957	160.209425	48.297255
1718.809716	163.844328	48.302260
1715.044311	164.022367	48.307265
1711.671506	156.295801	48.312269
1707.871797	150.910852	48.317274
1704.484884	158.217906	48.322279
1700.759524	152.808668	48.327284
1697.100286	161.971226	48.332289
1693.483578	159.756284	48.337293
1690.705246	154.062791	48.342298
1686.782907	159.327546	48.347303
1683.507159	155.689304	48.352308
1680.026243	162.286559	48.357313
1676.562735	159.275669	48.362317
1673.308126	150.885198	48.367322
1669.436582	155.148563	48.372327
1666.287041	153.154755	48.377332
1662.231872	152.878277	48.382337
1659.175416	152.685946	48.387341
1655.671720	145.084299	48.392346
1652.148906	156.370597	48.397351
1648.618764	156.907320	48.402356
1644.955651	160.065532	48.407361
1641.407780	161.266274	48.412365
1638.150683	155.916655	48.417370
1634.034254	158.566835	48.422375
1630.949724	146.568299	48.427380
1627.556379	153.651746	48.432385
1624.208890	158.234914	48.437389
1620.540816	159.625324	48.442394
1616.916594	148.698377	48.447399
1613.661897	150.992225	48.452404
1609.491986	156.469764	48.457409
1606.071677	153.733722	48.462413
1603.010428	143.142627	48.467418
1599.551481	148.265278	48.472423
1596.306354	145.799223	48.477428
1592.459454	145.138990	48.482433
1589.131398	149.605227	48.487437
1585.355083	148.155646	48.492442
1581.586611	146.723821	48.497447
1578.395640	148.507819	48.502452
1575.276102	148.929680	48.507457
1571.601833	154.481521	48.512461
1568.188822	139.690138	48.517466
1564.067562	150.864472	48.522471
1560.957521	140.935946	48.527476
1557.277411	149.595590	48.532481
1553.756323	151.228779	48.537485
1550.838720	147.177016	48.542490
1546.621590	145.397802	48.547495
1543.969290	149.672860	48.552500
1540.016095	150.810524	48.557505
1536.473758	148.400499	48.562509
1533.215099	142.535462	48.567514
1529.295929	148.233217	48.572519
1525.966647	144.195277	48.577524
1522.415907	146.962606	48.582529
1518.558742	155.292463	48.587533
1515.593112	148.850041	48.592538
1511.756069	155.230993	48.597543
1508.353423	146.746698	48.602548
1504.975823	152.261616	48.607553
1501.477801	150.597661	48.612557
1498.247151	149.034229	48.617562
1494.132058	145.884946	48.622567
1491.032867	139.691237	48.627572
1487.255106	142.098633	48.632577
1483.990489	147.099149	48.637581
1480.614437	134.747669	48.642586
1476.781150	143.984980	48.647591
1473.426282	146.553984	48.652596
1470.204112	146.624936	48.657601
1466.368577	145.614952	48.662605
1463.033766	141.685471	48.667610
1459.494362	147.700302	48.672615
1455.923210	145.589055	48.677620
1452.399836	143.989199	48.682625
1449.018911	150.191205	48.687629
1445.472629	140.622081	48.692634
1441.335882	148.299679	48.697639
1438.115187	149.009505	48.702644
1434.785002	148.404497	48.707649
1431.312296	147.739539	48.712653
1428.409929	143.878426	48.717658
1424.766111	152.051526	48.722663
1420.757202	139.950995	48.727668
1417.410651	139.364374	48.732673
1414.042021	142.425943	48.737677
1410.594793	141.190680	48.742682
1406.865411	143.963863	48.747687
1403.324172	141.737220	48.752692
1399.340336	149.454174	48.757697
1396.194219	144.460608	48.762701
1393.245121	139.562757	48.767706
1389.466090	150.231147	48.772711
1385.697317	143.977768	48.777716
1382.238657	140.197422	48.782721
1378.851938	140.835176	48.787725
1375.190356	141.781719	48.792730
1371.850180	145.471614	48.797735
1368.308495	136.265647	48.802740
1364.724081	141.360549	48.807745
1361.201014	141.817168	48.812749
1357.992261	139.712506	48.817754
1354.727095	147.721946	48.822759
1350.867671	137.426746	48.827764
1347.298831	143.079213	48.832769
1343.605988	142.872700	48.837773
1340.620823	142.498460	48.842778
1336.647221	141.231723	48.847783
1333.131152	142.475050	48.852788
1330.099891	145.186434	48.857793
1326.744247	138.510899	48.862797
1322.986049	144.927025	48.867802
1318.865568	140.949740	48.872807
1315.438551	143.498449	48.877812
1312.165934	138.385509	48.882817
1308.573472	143.817054	48.887821
1305.611037	136.570599	48.892826
1301.505265	145.328588	48.897831
1298.431128	135.827993	48.902836
1295.229128	135.557316	48.907841
1291.295873	132.215141	48.912845
1287.783226	134.204609	48.917850
1284.231087	134.115301	48.922855
1281.046742	127.476249	48.927860
1277.375743	131.727334	48.932865
1274.095297	134.847910	48.937869
1270.284873	137.095977	48.942874
1266.764180	140.782523	48.947879
1263.133931	128.809468	48.952884
1259.977276	139.551306	48.957889
1256.554566	131.560658	48.962893
1252.945471	131.179714	48.967898
1249.354710	135.275876	48.972903
1245.529611	140.158552	48.977908
1242.047682	138.400423	48.982913
1238.696341	141.535272	48.987917
1235.443996	132.859886	48.992922
1231.721143	137.106450	48.997927
1228.101096	133.167928	49.002932
1224.644365	133.842006	49.007937
1220.886666	140.397293	49.012941
1217.710376	130.836793	49.017946
1213.926481	138.234596	49.022951
1211.052618	140.035502	49.027956
1207.544633	132.422064	49.032961
1203.978338	140.108516	49.037965
1200.674896	131.564533	49.042970
1196.821125	133.446082	49.047975
1193.130632	132.644460	49.052980
1189.564952	140.897143	49.057985
1186.162948	137.437041	49.062989
1182.735373	128.691033	49.067994
1179.029503	135.412229	49.072999
1175.563612	134.913980	49.078004
1171.939188	136.965281	49.083009
1168.606200	132.871108	49.088013
1165.640274	134.060003	49.093018
1161.947252	126.924819	49.098023
1158.618108	124.532186	49.103028
1154.927835	129.846209	49.108033
1150.986846	130.086752	49.113037
1147.647513	129.872426	49.118042
1143.995646	126.521064	49.123047
1140.798658	133.124635	49.128052
1137.628535	131.409481	49.133057
1133.579492	126.626982	49.138061
1130.265013	132.075173	49.143066
1126.276139	135.831900	49.148071
1123.202089	127.100175	49.153076
1119.718353	123.621258	49.158081
1115.920834	134.270467	49.163085
1112.733917	128.514589	49.168090
1109.363332	130.355324	49.173095
1105.892040	119.721071	49.178100
1102.295929	122.840498	49.183105
1098.657358	133.347765	49.188109
1095.203483	126.640250	49.193114
1091.352466	133.026686	49.198119
1088.021096	122.288273	49.203124
1084.528932	124.356864	49.208129
1080.564254	127.236604	49.213133
1077.659564	122.395192	49.218138
1074.032235	126.826173	49.223143
1070.442175	122.417942	49.228148
1066.834445	127.162239	49.233153
1064.051893	120.862171	49.238157
1060.729495	119.816305	49.243162
1057.174190	127.893388	49.248167
1053.269261	128.368775	49.253172
1049.572563	126.615871	49.258177
1046.073095	128.650817	49.263181
1042.728815	117.177279	49.268186
1038.746988	129.671395	49.273191
1035.482488	124.930625	49.278196
1032.192869	129.992131	49.283201
1028.456803	136.145453	49.288205
1025.379728	126.496733	49.293210
1021.304614	125.698450	49.298215
1017.957546	114.579709	49.303220
1014.577150	123.651329	49.308225
1010.874909	125.332050	49.313229
1007.761515	120.286053	49.318234
1003.866981	130.330376	49.323239
1000.471387	126.711152	49.328244
996.977255	119.332929	49.333249
993.608326	114.358587	49.338253
990.354679	124.723352	49.343258
986.568083	131.710354	49.348263
982.942909	123.001702	49.353268
979.606385	121.812541	49.358273
975.870469	126.580103	49.363277
972.399756	117.619480	49.368282
969.303765	125.944217	49.373287
965.947669	125.542751	49.378292
962.503336	119.782945	49.383297
958.461218	122.342657	49.388301
955.175757	121.148673	49.393306
951.635537	123.436810	49.398311
947.815084	124.996856	49.403316
944.351616	124.064870	49.408321
940.880602	136.618247	49.413325
937.681383	123.448380	49.418330
934.084884	125.527032	49.423335
930.738223	121.216791	49.428340
927.169313	118.801675	49.433345
923.388402	118.498380	49.438349
920.224403	123.809173	49.443354
916.545451	127.185250	49.448359
912.710824	120.053370	49.453364
909.273103	114.517184	49.458369
905.480084	128.323233	49.463373
902.856500	122.298892	49.468378
898.720230	116.846780	49.473383
895.376209	118.338572	49.478388
892.215148	110.458982	49.483393
888.337456	120.560812	49.488397
884.914844	116.667452	49.493402
881.158586	122.510764	49.498407
877.601131	126.516412	49.503412
874.890398	119.249694	49.508417
871.320614	123.140213	49.513421
867.554195	122.660662	49.518426
863.821560	128.013056	49.523431
860.452655	126.993526	49.528436
856.970459	115.658731	49.533441
853.248565	129.222700	49.538445
850.229911	120.526706	49.543450
846.325494	123.207273	49.548455
842.880919	125.882276	49.553460
839.438922	118.350422	49.558465
835.792098	120.300946	49.563469
832.768712	120.299854	49.568474
828.899455	121.842278	49.573479
825.329449	127.371702	49.578484
821.639160	121.976342	49.583489
818.490567	124.215856	49.588493
815.195465	126.174587	49.593498
811.407391	122.847857	49.598503
807.760747	125.883550	49.603508
804.405304	123.938101	49.608513
801.007289	129.703198	49.613517
797.389244	118.997153	49.618522
793.723406	126.034913	49.623527
790.440066	128.542314	49.628532
786.427323	132.217486	49.633537
782.998049	129.169944	49.638541
780.024275	113.803971	49.643546
776.667806	131.635664	49.648551
773.280273	123.402433	49.653556
769.829432	112.249436	49.658561
765.888228	120.978668	49.663565
762.489431	115.395318	49.668570
758.624806	126.741687	49.673575
755.348223	120.326101	49.678580
751.677825	112.171983	49.683585
747.991272	119.235146	49.688589
744.575116	114.951683	49.693594
741.178063	119.090448	49.698599
737.667600	112.002805	49.703604
734.657122	111.098038	49.708609
731.097685	116.056351	49.713613
727.541935	113.335530	49.718618
723.907775	118.561816	49.723623
720.227282	117.107072	49.728628
716.415254	113.594308	49.733633
712.787500	118.465249	49.738637
709.852841	114.799269	49.743642
706.099924	117.902263	49.748647
702.787594	119.677065	49.753652
699.452590	116.529373	49.758657
695.812210	128.321544	49.763661
692.333597	117.682302	49.768666
688.900155	113.698967	49.773671
685.122865	117.678995	49.778676
682.165994	117.484035	49.783681
678.541695	116.684907	49.788685
674.833884	113.412109	49.793690
671.168755	120.057484	49.798695
667.482401	118.056342	49.803700
664.227186	115.364411	49.808705
660.935778	120.160549	49.813709
657.544010	112.257073	49.818714
653.792192	122.870787	49.823719
649.867766	112.070430	49.828724
646.438956	121.804643	49.833729
642.988194	123.474594	49.838733
640.094796	119.827486	49.843738
636.600205	110.370877	49.848743
633.039027	108.087550	49.853748
629.353512	110.550419	49.858753
625.617147	120.582745	49.863757
622.072219	116.322663	49.868762
618.558265	113.940195	49.873767
615.314533	114.840566	49.878772
611.807386	109.843734	49.883777
608.102160	110.332322	49.888781
604.948262	105.780051	49.893786
601.128090	117.353625	49.898791
597.236177	106.434309	49.903796
594.129971	109.268378	49.908801
590.535164	121.104058	49.913805
587.462753	106.908416	49.918810
584.223812	113.009337	49.923815
580.238330	110.007862	49.928820
576.961305	102.143404	49.933825
572.940346	117.889849	49.938829
569.519905	113.094593	49.943834
566.075699	107.752561	49.948839
562.707679	122.276764	49.953844
559.409967	112.472974	49.958849
555.546313	111.208339	49.963853
552.425625	106.442077	49.968858
548.642725	107.009294	49.973863
544.812691	112.924389	49.978868
541.722859	107.447770	49.983873
538.007902	120.969607	49.988877
534.743955	110.711281	49.993882
530.898819	111.658417	49.998887
527.651264	109.291212	50.003892
524.040703	105.126876	50.008897
520.302934	110.726969	50.013901
517.231662	110.619584	50.018906
513.589212	114.259014	50.023911
510.223596	115.637263	50.028916
506.737139	108.451050	50.033921
502.906160	111.202510	50.038925
499.528136	113.671053	50.043930
496.031072	112.159199	50.048935
492.575609	111.662738	50.053940
489.293032	109.835714	50.058945
485.507034	114.054467	50.063949
482.296792	112.741306	50.068954
478.532777	125.521027	50.073959
474.815340	125.068769	50.078964
472.183375	114.616567	50.083969
468.126936	114.587575	50.088973
464.335393	109.198747	50.093978
460.688054	106.922660	50.098983
457.554889	111.599161	50.103988
454.013285	103.883766	50.108993
450.061683	120.271129	50.113997
447.108322	111.429034	50.119002
443.657538	106.717681	50.124007
440.800070	109.898821	50.129012
437.036571	107.954154	50.134017
432.859310	114.714629	50.139021
429.264486	111.769095	50.144026
425.889105	120.273777	50.149031
422.631893	117.655019	50.154036
419.526447	106.577807	50.159041
415.568596	117.916738	50.164045
412.002057	112.559131	50.169050
408.299765	122.152751	50.174055
404.712724	116.355425	50.179060
401.737373	103.403860	50.184065
398.000195	105.764177	50.189069
394.608601	112.290869	50.194074
391.048769	108.248361	50.199079
387.733705	103.180412	50.204084
384.189349	106.481816	50.209089
380.471375	112.581904	50.214093
377.019250	113.094216	50.219098
373.003471	116.032866	50.224103
369.449512	113.058809	50.229108
366.358606	105.098848	50.234113
362.772309	110.944195	50.239117
359.545555	101.717852	50.244122
356.196686	104.925370	50.249127
352.603926	113.748864	50.254132
349.062196	108.545589	50.259137
345.725918	109.277051	50.264141
342.017790	107.877417	50.269146
338.465134	109.648862	50.274151
334.476031	108.296408	50.279156
331.735686	109.250905	50.284161
327.843832	101.274055	50.289165
324.367677	107.636842	50.294170
321.262641	113.878222	50.299175
317.575927	108.390784	50.304180
313.886896	111.974310	50.309185
310.050436	114.027508	50.314189
307.219689	108.456612	50.319194
303.499173	112.870823	50.324199
299.875260	112.008515	50.329204
296.548598	106.344462	50.334209
292.650274	117.857611	50.339213
289.086890	105.909383	50.344218
285.866959	107.366133	50.349223
282.467221	111.261861	50.354228
278.978757	106.031292	50.359233
275.302139	114.162422	50.364237
271.862324	102.761167	50.369242
268.108188	109.154864	50.374247
264.755258	107.481319	50.379252
261.716507	102.901654	50.384257
258.232458	110.844433	50.389261
254.554675	104.466601	50.394266
250.877426	98.661336	50.399271
246.990858	113.171930	50.404276
243.409603	104.257440	50.409281
239.977365	107.389473	50.414285
237.132423	106.452617	50.419290
233.489332	112.885881	50.424295
229.973450	110.750653	50.429300
226.650330	112.400761	50.434305
222.717963	106.708240	50.439309
219.010905	104.587147	50.444314
215.806072	109.287606	50.449319
212.174939	103.978176	50.454324
209.405860	105.462400	50.459329
205.322532	107.737816	50.464333
201.679428	102.063267	50.469338
198.174781	102.865453	50.474343
194.602142	107.924099	50.479348
191.746878	97.165311	50.484353
187.697105	104.573470	50.489357
184.422953	94.756680	50.494362
180.481072	108.715966	50.499367
176.970266	109.281842	50.504372
173.809839	104.917427	50.509377
170.154441	109.546117	50.514381
166.902807	102.731403	50.519386
163.268608	105.154777	50.524391
159.789971	109.420417	50.529396
156.078846	107.508799	50.534401
152.749882	113.690397	50.539405
149.233607	109.014741	50.544410
145.538937	104.221502	50.549415
142.121892	118.180842	50.554420
138.873734	103.630128	50.559425
135.326663	116.822057	50.564429
131.771664	114.224757	50.569434
128.032263	113.899475	50.574439
124.401095	105.910361	50.579444
121.613231	105.803006	50.584449
117.838066	119.865918	50.589453
114.266087	104.426303	50.594458
110.899807	109.604511	50.599463
107.318765	116.622893	50.604468
104.095307	109.857573	50.609473
100.158997	110.755901	50.614477
96.661879	104.862374	50.619482
93.156117	105.864096	50.624487
89.544156	111.197863	50.629492
86.417632	107.106586	50.634497
82.891397	115.941894	50.639501
79.500999	107.124132	50.644506
75.538987	107.624697	50.649511
72.213621	107.854674	50.654516
68.720560	110.730541	50.659521
64.805526	114.286298	50.664525
61.586665	109.174937	50.669530
58.133111	104.878642	50.674535
54.341702	104.526740	50.679540
51.516302	106.174862	50.684545
47.644805	114.760553	50.689549
44.443062	108.596141	50.694554
41.212683	103.163889	50.699559
37.056670	105.276761	50.704564
33.605243	102.533562	50.709569
29.544181	109.250687	50.714573
26.679465	102.922747	50.719578
23.387868	97.360890	50.724583
19.942523	104.823114	50.729588
16.346684	91.570314	50.734593
12.322389	101.638457	50.739597
8.869657	96.804213	50.744602
5.428928	98.551924	50.749607
1.806918	98.705019	50.754612