Thu Aug 25 16:23:51 2022

Number of Points = 9922

Depth (nm)	Load (N)	Time (s)
3.687233	104.411543	0.000000
3.349543	104.559399	0.005005
3.582414	105.041806	0.010010
3.576273	88.132375	0.015014
3.012825	81.497652	0.020019
3.536781	71.826172	0.025024
2.859346	66.807024	0.030029
2.656466	48.156739	0.035034
2.396766	54.749643	0.040038
2.219255	41.578217	0.045043
2.189472	30.326210	0.050048
1.663988	20.509136	0.055053
1.197873	19.832387	0.060058
1.494180	13.588168	0.065062
0.737512	2.915143	0.070067
0.640345	-12.170256	0.075072
0.400735	-15.498927	0.080077
0.234689	-19.630063	0.085082
-0.054245	-12.706737	0.090086
-0.738468	-7.771593	0.095091
-0.529776	-24.379218	0.100096
-1.480933	-28.823939	0.105101
-2.168714	-22.768270	0.110106
-2.266946	-24.565682	0.115110
-2.881470	-13.544888	0.120115
-2.532426	-14.779629	0.125120
-2.863748	-17.046723	0.130125
-3.155971	-11.904080	0.135130
-3.363322	-22.242377	0.140134
-3.589801	-16.423499	0.145139
-3.376470	-19.573199	0.150144
-3.400026	-18.174256	0.155149
-3.930012	-20.672815	0.160154
-4.084861	-26.162958	0.165158
-4.377204	-13.911322	0.170163
-4.429703	-17.275636	0.175168
-5.323645	-23.042284	0.180173
-5.686105	-22.884220	0.185178
-5.636289	-22.120034	0.190182
-6.329070	-20.625726	0.195187
-5.850059	-19.413095	0.200192
-6.600279	-15.676170	0.205197
-7.325375	-23.348548	0.210202
-6.874405	-16.908150	0.215206
-7.552288	-2.504851	0.220211
-7.438129	-13.285835	0.225216
-7.590983	-14.606452	0.230221
-7.783463	-16.060066	0.235226
-7.523125	-26.126789	0.240230
-8.312144	-20.298867	0.245235
-8.735372	-30.324923	0.250240
-9.032424	-26.019924	0.255245
-9.293311	-22.169844	0.260250
-9.073895	-23.558281	0.265254
-9.261740	-15.825053	0.270259
-10.074663	-15.384436	0.275264
-10.315269	-16.909604	0.280269
-10.471038	-14.755951	0.285274
-10.579801	-25.732954	0.290278
-11.272541	-16.990472	0.295283
-11.531618	-18.044508	0.300288
-11.697678	-11.396698	0.305293
-12.014135	-10.110050	0.310298
-12.102609	-12.101982	0.315302
-12.195242	-14.574154	0.320307
-11.946304	-10.433793	0.325312
-12.179357	-7.537201	0.330317
-12.777155	-9.740397	0.335322
-13.368359	-11.182158	0.340326
-13.440100	-14.673172	0.345331
-13.213178	-17.995845	0.350336
-14.134667	-18.145659	0.355341
-14.695092	-21.066556	0.360346
-14.306275	-24.870176	0.365350
-14.798238	-7.243663	0.370355
-14.713920	-17.776358	0.375360
-15.170186	-10.826813	0.380365
-15.616337	-18.527080	0.385370
-16.144364	-22.731212	0.390374
-16.575590	-13.722818	0.395379
-16.357714	-18.910694	0.400384
-16.406525	-13.122817	0.405389
-16.887495	-13.180302	0.410394
-16.534360	-15.997566	0.415398
-16.720121	-8.128620	0.420403
-17.390973	-12.009819	0.425408
-17.826436	-9.109986	0.430413
-18.079592	-3.751999	0.435418
-18.055949	-9.431466	0.440422
-17.934097	-7.504810	0.445427
-18.168659	-14.232153	0.450432
-19.363728	-10.593205	0.455437
-19.663652	-14.026320	0.460442
-19.408613	-17.388200	0.465446
-19.570772	-5.659995	0.470451
-19.566417	-13.737736	0.475456
-20.332017	-4.022046	0.480461
-20.815264	-3.582463	0.485466
-20.652747	-8.546532	0.490470
-21.052430	-12.403780	0.495475
-21.152646	-11.714163	0.500480
-20.881455	-11.984413	0.505485
-21.937746	-8.908212	0.510490
-22.076332	-10.424055	0.515494
-22.581947	-9.218500	0.520499
-22.756438	-13.794404	0.525504
-22.784818	-6.605015	0.530509
-22.659002	-4.245545	0.535514
-23.006522	-6.655634	0.540518
-23.684623	-8.226149	0.545523
-23.939302	-12.033349	0.550528
-23.686777	-9.092617	0.555533
-24.073305	-17.792484	0.560538
-24.154624	-11.129478	0.565542
-24.765318	-9.992881	0.570547
-25.071253	-6.107266	0.575552
-25.058124	-3.847198	0.580557
-25.485989	-4.093338	0.585562
-25.435723	-10.033241	0.590566
-26.264224	-10.479199	0.595571
-26.310591	-19.014063	0.600576
-26.772323	-6.011380	0.605581
-26.593395	-6.052038	0.610586
-26.654594	-14.312497	0.615590
-26.951573	-5.594054	0.620595
-27.457849	-8.618348	0.625600
-27.820539	-8.988596	0.630605
-27.907567	-8.066926	0.635610
-28.174456	-14.903099	0.640614
-28.367208	-11.051039	0.645619
-28.882996	-12.419193	0.650624
-29.569536	-7.581762	0.655629
-29.612177	-4.904830	0.660634
-29.516779	-18.517603	0.665638
-29.640392	-7.279495	0.670643
-29.510281	-7.511822	0.675648
-29.883812	-15.153864	0.680653
-30.958470	-5.490991	0.685658
-31.185858	-14.307542	0.690662
-31.461008	-11.692257	0.695667
-31.544841	-8.363465	0.700672
-31.738349	-7.924986	0.705677
-31.599941	-7.807434	0.710682
-31.662200	-15.662764	0.715686
-31.865984	-10.976905	0.720691
-32.493785	-16.120861	0.725696
-33.197524	-10.752387	0.730701
-32.930823	-2.293106	0.735706
-32.939409	-12.377811	0.740710
-33.193430	-11.901377	0.745715
-33.357688	-17.402702	0.750720
-34.058216	-13.945645	0.755725
-34.389749	-15.469220	0.760730
-34.775527	-14.899375	0.765734
-34.692902	-14.769919	0.770739
-34.802745	-17.979714	0.775744
-35.293422	-10.116777	0.780749
-35.980368	-8.066558	0.785754
-35.791695	-16.888187	0.790758
-36.019503	-5.333195	0.795763
-35.937851	-15.270685	0.800768
-36.260858	-5.092832	0.805773
-37.012771	-10.821622	0.810778
-36.838581	-22.213119	0.815782
-37.265509	-17.204396	0.820787
-37.107120	-15.868762	0.825792
-37.934565	-13.179595	0.830797
-38.608211	-11.969858	0.835802
-38.765562	-14.115512	0.840806
-38.661439	-14.511446	0.845811
-38.355558	-16.856233	0.850816
-38.515427	-9.032474	0.855821
-38.985834	-14.017593	0.860826
-39.127849	-18.519489	0.865830
-39.945945	-8.339995	0.870835
-40.337381	-8.661445	0.875840
-40.290165	-13.654902	0.880845
-40.414942	-8.870690	0.885850
-40.389085	-8.684883	0.890854
-41.425057	-5.061369	0.895859
-41.442573	-13.803236	0.900864
-41.746886	-8.604914	0.905869
-41.987078	-9.377170	0.910874
-41.787831	-7.611338	0.915878
-41.813810	2.934431	0.920883
-42.183346	-15.009456	0.925888
-43.117849	-3.872082	0.930893
-43.585225	-6.959418	0.935898
-43.263269	-11.439102	0.940902
-43.434695	-7.520779	0.945907
-43.438118	-12.057048	0.950912
-43.911221	-6.477937	0.955917
-44.148819	-7.285400	0.960922
-44.600649	-11.428705	0.965926
-45.153063	-9.602046	0.970931
-44.875022	-6.266679	0.975936
-45.053407	-6.662640	0.980941
-45.895314	-14.876700	0.985946
-45.998304	-13.762704	0.990950
-46.189726	-8.458684	0.995955
-46.374587	-9.413617	1.000960
-46.242330	-3.236492	1.005965
-46.337243	-2.829281	1.010970
-47.184904	-1.671370	1.015974
-47.279409	1.994456	1.020979
-47.825688	-9.505624	1.025984
-47.902862	-14.546029	1.030989
-47.918210	-8.959549	1.035994
-47.437306	-6.377306	1.040998
-48.445068	-2.470308	1.046003
-49.019761	-7.758628	1.051008
-49.273314	-8.389585	1.056013
-49.454217	-2.881566	1.061018
-49.596102	-10.202399	1.066022
-49.819324	-4.140419	1.071027
-49.628013	-14.617111	1.076032
-50.286406	-14.447477	1.081037
-51.110234	-10.727489	1.086042
-50.679100	-6.001908	1.091046
-50.763224	-13.227385	1.096051
-50.756019	-10.061555	1.101056
-51.770038	-6.261144	1.106061
-52.202751	-5.918063	1.111066
-52.143697	-1.776424	1.116070
-52.158017	3.686512	1.121075
-52.411192	-1.769247	1.126080
-52.448237	-9.628528	1.131085
-53.333136	-4.510077	1.136090
-53.721255	-9.694752	1.141094
-53.882598	-4.262566	1.146099
-53.795426	-15.172194	1.151104
-53.387687	-4.210333	1.156109
-54.041151	-3.576398	1.161114
-54.449188	-9.460307	1.166118
-55.343087	-7.130886	1.171123
-55.245937	-10.328822	1.176128
-55.116038	-11.244488	1.181133
-55.257767	-6.856254	1.186138
-55.487465	-12.711158	1.191142
-56.453402	-2.283868	1.196147
-56.588787	-9.080535	1.201152
-56.836217	-9.282178	1.206157
-56.477338	-3.355700	1.211162
-56.607219	-12.364699	1.216166
-57.178506	-4.470146	1.221171
-58.025353	-7.418929	1.226176
-57.886150	-3.137988	1.231181
-58.232331	6.056406	1.236186
-57.868963	-4.719334	1.241190
-58.413406	0.114818	1.246195
-58.539690	-3.861197	1.251200
-59.222429	-5.342397	1.256205
-59.562856	3.072808	1.261210
-59.436134	-0.933360	1.266214
-59.651545	-9.397445	1.271219
-60.077358	-12.310958	1.276224
-60.831038	-2.736341	1.281229
-61.061391	-1.048729	1.286234
-61.146646	-12.222408	1.291238
-61.372375	-12.487563	1.296243
-61.249379	-4.325310	1.301248
-61.329196	-4.926541	1.306253
-61.404689	-6.667405	1.311258
-61.665295	-16.111500	1.316262
-62.454026	-4.629971	1.321267
-62.708246	2.329050	1.326272
-62.624074	-1.088318	1.331277
-62.677983	-7.603521	1.336282
-62.887265	2.350870	1.341286
-63.868945	-0.061092	1.346291
-63.869622	-6.227130	1.351296
-63.889367	-0.851931	1.356301
-63.993656	-4.840884	1.361306
-64.761860	-6.084064	1.366310
-65.300821	-7.027805	1.371315
-65.391017	-4.669290	1.376320
-65.487302	-6.432206	1.381325
-65.735676	7.286865	1.386330
-65.687559	-2.310015	1.391334
-65.990474	-0.474992	1.396339
-65.896468	-4.903141	1.401344
-66.643262	-0.261909	1.406349
-66.810277	-6.841647	1.411354
-66.747157	-8.480843	1.416358
-67.414711	3.693551	1.421363
-67.895637	-12.499136	1.426368
-68.256021	-16.042997	1.431373
-68.566187	-7.420566	1.436378
-68.492819	-7.893939	1.441382
-69.224380	-2.600196	1.446387
-68.664923	-12.027256	1.451392
-68.723071	-11.347394	1.456397
-69.185228	-2.014609	1.461402
-68.814920	-5.479975	1.466406
-69.637988	-4.838445	1.471411
-70.171173	-7.868011	1.476416
-70.137351	-11.824818	1.481421
-70.687945	-2.342135	1.486426
-70.880474	-8.073149	1.491430
-71.066225	-5.269390	1.496435
-71.235123	-17.942237	1.501440
-71.152297	-9.881261	1.506445
-71.677861	-7.340633	1.511450
-72.009106	-15.530300	1.516454
-72.583106	-11.340090	1.521459
-72.683280	-9.824737	1.526464
-72.760476	-12.226560	1.531469
-72.787729	-13.924361	1.536474
-73.501278	-19.744576	1.541478
-74.169876	-5.434485	1.546483
-74.065996	-13.103873	1.551488
-74.439013	-10.447943	1.556493
-74.535536	-10.012006	1.561498
-74.431747	-10.850814	1.566502
-75.086957	-5.508924	1.571507
-74.611916	-0.771240	1.576512
-74.787635	-9.447189	1.581517
-75.614159	-3.344461	1.586522
-75.664268	-16.380772	1.591526
-76.078764	-7.539514	1.596531
-76.537012	-6.847580	1.601536
-76.933383	-1.868950	1.606541
-77.624184	-1.251309	1.611546
-77.306297	-7.356531	1.616550
-77.155691	-11.540446	1.621555
-77.452811	-11.607752	1.626560
-77.420517	-10.581393	1.631565
-77.933134	-7.735909	1.636570
-78.191913	-7.704819	1.641574
-79.001253	-1.626930	1.646579
-78.878553	-7.907212	1.651584
-78.842593	-6.492284	1.656589
-79.198100	-6.667501	1.661594
-79.262616	-5.255812	1.666598
-80.161936	-7.724969	1.671603
-80.585404	-0.438873	1.676608
-80.747863	-4.096006	1.681613
-81.018913	-2.462128	1.686618
-80.752473	-7.126104	1.691622
-80.681247	-5.039656	1.696627
-81.337714	0.283450	1.701632
-81.530043	0.392714	1.706637
-82.004625	-2.038592	1.711642
-82.193897	-1.822240	1.716646
-82.063949	4.848794	1.721651
-82.531052	0.331394	1.726656
-82.858430	-5.903675	1.731661
-83.411806	-2.365266	1.736666
-83.485270	-3.429402	1.741670
-83.888370	-5.552368	1.746675
-83.661990	0.625826	1.751680
-83.764962	2.173255	1.756685
-84.458643	-1.910006	1.761690
-84.969009	-3.744080	1.766694
-85.281736	-8.174935	1.771699
-85.581830	-3.986513	1.776704
-85.514248	-1.693850	1.781709
-85.397696	1.309315	1.786714
-85.106857	-13.131349	1.791718
-85.924604	-5.837259	1.796723
-86.452099	-3.214069	1.801728
-86.634402	-10.924036	1.806733
-86.997963	1.607684	1.811738
-86.712375	-8.985021	1.816742
-87.481786	5.878714	1.821747
-88.072485	-0.621982	1.826752
-88.128254	-4.045895	1.831757
-88.172561	-2.944257	1.836762
-87.995641	-10.659891	1.841766
-88.373174	-9.642082	1.846771
-89.008710	-12.029183	1.851776
-89.223325	-12.583981	1.856781
-89.731111	-6.901359	1.861786
-89.423932	-3.421862	1.866790
-89.317736	8.064979	1.871795
-90.145724	1.778635	1.876800
-90.899710	-9.033992	1.881805
-91.016909	-3.257545	1.886810
-90.883794	-8.723208	1.891814
-91.185704	-7.748885	1.896819
-91.154206	3.873045	1.901824
-91.145489	-19.793236	1.906829
-91.970982	-13.469209	1.911834
-92.310271	-19.224679	1.916838
-92.577153	-13.241283	1.921843
-92.562624	-11.645827	1.926848
-92.340470	-13.550388	1.931853
-92.680800	-4.568890	1.936858
-93.314071	-14.891062	1.941862
-93.783255	-9.401150	1.946867
-93.983525	-8.183326	1.951872
-94.203639	-12.954558	1.956877
-94.415771	-6.454555	1.961882
-94.728524	-11.445390	1.966886
-95.556184	-15.124838	1.971891
-95.525101	-17.685995	1.976896
-95.328842	-17.988798	1.981901
-95.486936	-8.048763	1.986906
-95.409900	-19.738247	1.991910
-95.778963	-11.397657	1.996915
-96.612181	-17.094336	2.006912
-96.163303	-10.033861	2.016909
-95.865092	-9.120676	2.026906
-95.416921	-10.090495	2.036902
-94.807232	-15.013712	2.046899
-94.365284	-16.844200	2.056896
-93.547321	-10.573323	2.066893
-93.294179	-12.491437	2.076890
-92.601160	-12.064602	2.086886
-91.743917	-12.189358	2.096883
-91.914157	-9.073999	2.106880
-91.658587	-14.987106	2.116877
-90.751773	-12.677245	2.126874
-89.708161	-10.604230	2.136870
-89.654657	-16.716925	2.146867
-89.391676	-14.252327	2.156864
-88.797861	-16.163633	2.166861
-87.696697	-15.579005	2.176858
-87.995781	-12.677876	2.186854
-87.090393	-16.073022	2.196851
-85.916767	-14.159763	2.206848
-86.268211	-4.461804	2.216845
-85.957301	-11.523997	2.226842
-85.215465	-12.261063	2.236838
-84.848151	-15.312137	2.246835
-84.461665	-13.972458	2.256832
-83.537216	-17.662029	2.266829
-83.216289	-14.471578	2.276826
-82.050370	-18.569620	2.286822
-81.978945	-19.290336	2.296819
-81.863142	-19.435129	2.306816
-81.492980	-16.787753	2.316813
-80.638454	-16.104290	2.326810
-80.419660	-20.586116	2.336806
-79.302092	-12.987353	2.346803
-79.398674	-15.911885	2.356800
-78.509388	-14.508438	2.366797
-77.917476	-14.049921	2.376794
-77.747229	-10.123101	2.386790
-77.434175	-13.929116	2.396787
-76.250277	-6.242539	2.406784
-76.474472	-9.061546	2.416781
-75.626270	-14.155183	2.426778
-74.965306	-12.411850	2.436774
-74.518208	-8.560087	2.446771
-74.202655	-14.992611	2.456768
-73.414504	-14.210047	2.466765
-73.393262	-18.068539	2.476762
-72.749159	-13.081891	2.486758
-72.324297	-15.001569	2.496755
-71.962833	-12.530227	2.506752
-71.067808	-17.168699	2.516749
-70.544078	-17.957119	2.526746
-69.530153	-16.851969	2.536742
-69.379962	-16.606174	2.546739
-69.174157	-11.623708	2.556736
-68.883924	-13.785219	2.566733
-68.132315	-20.194200	2.576730
-67.722750	-16.409417	2.586726
-66.923637	-5.285658	2.596723
-66.465312	-18.269417	2.606720
-66.280181	-7.150823	2.616717
-65.797661	-11.826031	2.626714
-64.893229	-16.751080	2.636710
-64.848616	-14.733772	2.646707
-63.798589	-5.667225	2.656704
-63.410494	-17.984243	2.666701
-63.306278	-15.979442	2.676698
-62.770308	-12.857531	2.686694
-62.325682	-16.462414	2.696691
-61.499083	-12.803164	2.706688
-60.787458	-13.709724	2.716685
-60.652771	-13.154221	2.726682
-60.498433	-16.894184	2.736678
-59.365739	-8.176378	2.746675
-59.319887	-14.002773	2.756672
-58.441558	-12.622949	2.766669
-58.056039	-14.827901	2.776666
-57.684096	-9.637047	2.786662
-56.881778	-11.926314	2.796659
-56.450969	-8.490149	2.806656
-56.202216	-10.553294	2.816653
-55.484912	-8.818787	2.826650
-54.784325	-7.794418	2.836646
-54.628147	-10.264377	2.846643
-54.236905	-11.443854	2.856640
-53.550207	-14.418258	2.866637
-53.142065	-11.377686	2.876634
-52.572120	-9.784816	2.886630
-51.724735	-17.114800	2.896627
-51.833701	-16.989955	2.906624
-51.223032	-16.943023	2.916621
-50.363028	-7.834029	2.926618
-50.135013	-18.234779	2.936614
-49.459446	-17.602466	2.946611
-48.922752	-15.421508	2.956608
-48.730704	-14.881328	2.966605
-48.366983	-10.607852	2.976602
-47.526564	-12.776375	2.986598
-47.157204	-16.340954	2.996595
-46.295386	-20.917200	3.006592
-46.058896	-18.619511	3.016589
-45.680859	-14.617543	3.026586
-44.641025	-20.181529	3.036582
-44.086858	-16.837553	3.046579
-44.185041	-13.587766	3.056576
-44.047401	-9.893421	3.066573
-43.524266	-14.286720	3.076570
-42.024717	-17.192082	3.086566
-41.767404	-20.232254	3.096563
-41.770350	-17.374360	3.106560
-41.565027	-17.596535	3.116557
-40.520953	-18.710407	3.126554
-39.903910	-21.886139	3.136550
-39.018929	-25.902141	3.146547
-38.976073	-20.574195	3.156544
-38.775452	-19.116692	3.166541
-38.575523	-8.114456	3.176538
-37.770753	-16.654203	3.186534
-36.338488	-15.066565	3.196531
-36.390928	-26.414894	3.206528
-36.043096	-16.306985	3.216525
-35.770231	-19.720228	3.226522
-35.071167	-17.868820	3.236518
-34.212241	-13.549391	3.246515
-33.997717	-15.616675	3.256512
-33.658071	-15.118628	3.266509
-33.016500	-14.899139	3.276506
-32.752421	-17.268795	3.286502
-31.631407	-17.944892	3.296499
-31.106508	-15.917307	3.306496
-31.162195	-20.777446	3.316493
-30.823521	-21.546373	3.326490
-29.795827	-21.358873	3.336486
-29.807032	-20.241982	3.346483
-28.805993	-20.433612	3.356480
-28.303045	-18.307553	3.366477
-28.100733	-11.835664	3.376474
-27.400863	-26.361979	3.386470
-26.816151	-19.997527	3.396467
-26.609384	-20.498696	3.406464
-26.057730	-28.133965	3.416461
-25.781346	-26.099120	3.426458
-25.409828	-24.015825	3.436454
-24.298160	-27.180357	3.446451
-24.046682	-26.665328	3.456448
-23.530643	-21.484381	3.466445
-22.762137	-22.241460	3.476442
-22.592778	-19.448577	3.486438
-22.192105	-22.390833	3.496435
-21.317251	-16.087679	3.506432
-21.096052	-14.079032	3.516429
-20.326120	-22.394739	3.526426
-19.712222	-13.570297	3.536422
-19.475169	-18.992660	3.546419
-19.197501	-17.141748	3.556416
-18.567390	-13.885696	3.566413
-18.093986	-18.565808	3.576410
-17.432303	-9.919914	3.586406
-16.876129	-20.530473	3.596403
-16.585170	-17.544399	3.606400
-15.667294	-18.613152	3.616397
-15.374153	-12.469108	3.626394
-15.209741	-15.234963	3.636390
-14.424320	-13.454104	3.646387
-13.918339	-20.540524	3.656384
-13.718209	-13.970091	3.666381
-12.729885	-13.700393	3.676378
-12.150868	-15.191225	3.686374
-12.321055	-19.624777	3.696371
-11.472505	-17.337456	3.706368
-10.685249	-20.270592	3.716365
-10.952097	-18.061931	3.726362
-10.039633	-16.630430	3.736358
-9.389430	-21.490298	3.746355
-8.945441	-16.060473	3.756352
-8.084383	-12.979990	3.766349
-8.054011	-15.965597	3.776346
-7.837799	-15.552747	3.786342
-6.958612	-11.341026	3.796339
-6.728077	-10.569288	3.806336
-6.342815	-1.959273	3.816333
-5.382398	1.783559	3.826330
-4.776215	14.103328	3.836326
-4.437886	15.618454	3.846323
-4.233329	10.993130	3.856320
-3.801873	20.245321	3.866317
-3.470436	32.326215	3.876314
-2.974045	36.955891	3.886310
-2.243354	50.548651	3.896307
-2.001566	58.686995	3.906304
-1.348096	76.349862	3.916301
-0.753637	94.956504	3.926298
-0.250421	101.631548	3.936294
0.000000	111.962619	3.941299
-0.070056	117.535566	3.946304
0.772347	123.845082	3.951309
0.715543	140.460750	3.956314
0.765981	139.769501	3.961318
0.930146	141.199156	3.966323
0.941538	141.789033	3.971328
1.068472	138.725609	3.976333
1.013830	144.150615	3.981338
0.697358	142.425346	3.986342
0.662952	142.993925	3.991347
0.958233	140.733037	3.996352
1.109416	144.097804	4.001357
1.142326	152.286904	4.006362
0.729432	152.876820	4.011366
1.159566	147.174742	4.016371
0.953102	153.933349	4.021376
1.201897	145.950114	4.026381
1.094396	142.948732	4.031386
0.742862	131.316799	4.036390
1.098835	137.262768	4.041395
0.771681	148.963143	4.046400
1.157572	142.704844	4.051405
1.182188	138.945598	4.056410
0.916491	146.165905	4.061414
1.142900	147.335869	4.066419
0.891718	147.410059	4.071424
0.965809	144.899086	4.076429
0.992894	147.144332	4.081434
0.844277	154.286186	4.086438
1.245071	150.834998	4.091443
1.091157	148.400879	4.096448
0.913762	139.933923	4.101453
1.036168	147.855896	4.106458
1.307681	146.788318	4.111462
1.438665	140.987579	4.116467
1.154799	152.361631	4.121472
1.383286	140.578701	4.126477
1.425778	142.906954	4.131482
1.310119	145.494108	4.136486
1.501711	150.216139	4.141491
1.245127	146.719253	4.146496
1.203237	139.085290	4.151501
0.952131	146.730423	4.156506
0.873215	140.415236	4.161510
1.107684	134.690035	4.166515
1.070668	139.837028	4.171520
1.202437	135.042254	4.176525
1.039141	139.785085	4.181530
1.025849	132.241558	4.186534
1.702665	139.532489	4.191539
1.343912	152.848188	4.196544
1.177389	140.874045	4.201549
1.704799	159.685617	4.206554
1.484057	155.306742	4.211558
1.596333	146.585587	4.216563
1.337653	145.563115	4.221568
0.931025	150.571868	4.226573
1.176799	157.854412	4.231578
1.732728	168.116117	4.236582
1.932953	162.867678	4.241587
1.357308	171.199594	4.246592
1.448915	164.123679	4.251597
1.797763	164.154476	4.256602
1.335861	160.414506	4.261606
1.520542	160.078715	4.266611
1.666976	169.078950	4.271616
1.686504	164.339720	4.276621
1.468602	160.931684	4.281626
1.688176	166.547853	4.286630
1.631519	168.923282	4.291635
1.579712	178.976490	4.296640
1.841879	167.422386	4.301645
1.510611	169.967394	4.306650
1.315382	170.991448	4.311654
1.526511	164.102453	4.316659
1.813604	163.630391	4.321664
1.684215	166.213372	4.326669
1.713283	161.488466	4.331674
1.424643	160.524473	4.336678
1.732225	157.049923	4.341683
1.584452	167.437703	4.346688
1.671428	160.182179	4.351693
1.441351	168.466277	4.356698
1.464829	166.770000	4.361702
2.001314	166.144966	4.366707
1.800422	175.917806	4.371712
2.050531	174.749176	4.376717
2.215250	172.284112	4.381722
1.963699	165.369532	4.386726
2.040987	168.049846	4.391731
1.979063	173.235553	4.396736
1.968198	165.343615	4.401741
1.776572	172.678879	4.406746
1.682603	169.646898	4.411750
1.979757	157.634895	4.416755
1.971207	176.223572	4.421760
1.718963	171.125120	4.426765
2.082992	170.833994	4.431770
1.656606	179.095071	4.436774
2.057937	165.560772	4.441779
1.788058	174.920473	4.446784
1.952026	185.544161	4.451789
1.958333	197.160682	4.456794
2.045124	196.071424	4.461798
2.582986	197.414058	4.466803
2.192372	186.481084	4.471808
2.173352	174.945722	4.476813
2.205023	171.881400	4.481818
1.808038	178.198462	4.486822
1.827629	175.477722	4.491827
1.897112	192.912059	4.496832
2.096316	190.992090	4.501837
2.107563	195.305786	4.506842
1.885969	203.572752	4.511846
2.346569	199.378182	4.516851
2.025054	197.650533	4.521856
2.213599	192.590580	4.526861
1.790685	190.043576	4.531866
2.164413	195.028151	4.536870
1.928492	188.822969	4.541875
1.806456	207.812280	4.546880
1.934567	211.835581	4.551885
2.716795	212.352141	4.556890
2.251333	217.015784	4.561894
2.247958	198.650465	4.566899
1.946817	211.099790	4.571904
2.248088	216.171654	4.576909
2.562755	225.136068	4.581914
2.455103	229.730997	4.586918
2.592260	218.237576	4.591923
2.354553	228.905243	4.596928
2.694236	222.166930	4.601933
2.519293	207.719965	4.606938
2.122643	205.855389	4.611942
2.459375	204.372622	4.616947
2.313894	220.473904	4.621952
2.325055	224.743327	4.626957
2.484356	231.185222	4.631962
2.438026	233.502094	4.636966
2.648298	222.107948	4.641971
2.624189	228.474174	4.646976
2.709731	224.088422	4.651981
2.297160	224.671962	4.656986
2.393375	225.330810	4.661990
2.424365	218.479510	4.666995
2.416509	229.886297	4.672000
2.448532	220.326615	4.677005
2.679759	227.741183	4.682010
2.408725	227.179395	4.687014
2.593115	228.928597	4.692019
2.501783	232.207989	4.697024
2.546689	221.985052	4.702029
2.550330	227.562306	4.707034
2.636248	229.076996	4.712038
2.460566	223.403374	4.717043
2.439845	236.511145	4.722048
2.316134	230.740792	4.727053
2.819809	239.526899	4.732058
2.983369	245.174016	4.737062
3.082184	238.274116	4.742067
2.803988	234.011793	4.747072
2.716291	234.740587	4.752077
2.927407	233.030723	4.757082
2.567576	226.829123	4.762086
2.743949	226.589546	4.767091
2.569760	232.305397	4.772096
2.975136	246.517022	4.777101
3.157479	250.430593	4.782106
2.990289	246.653921	4.787110
2.924480	239.653262	4.792115
2.778764	231.548301	4.797120
3.015636	234.111870	4.802125
3.038969	229.270784	4.807130
2.856575	224.790970	4.812134
2.936397	223.693310	4.817139
3.002072	217.203578	4.822144
2.858416	226.863073	4.827149
2.933433	232.157057	4.832154
2.882136	240.761195	4.837158
3.086338	251.378620	4.842163
3.324800	254.195048	4.847168
3.046870	242.962804	4.852173
2.812334	233.770753	4.857178
3.106424	242.909245	4.862182
3.536864	239.393283	4.867187
3.101363	227.900995	4.872192
2.997547	226.541038	4.877197
2.865022	223.594184	4.882202
2.859186	233.535814	4.887206
3.669832	242.235860	4.892211
2.787755	231.974658	4.897216
2.988303	231.661690	4.902221
3.294810	245.575588	4.907226
3.363070	252.367119	4.912230
3.123426	240.303125	4.917235
3.300225	243.717681	4.922240
3.313217	248.189306	4.927245
3.178398	243.607118	4.932250
3.007724	244.222361	4.937254
3.420095	242.946043	4.942259
2.948078	255.994822	4.947264
2.970635	245.841813	4.952269
3.392530	250.404398	4.957274
3.077283	252.655837	4.962278
3.434745	251.343828	4.967283
3.156822	254.256984	4.972288
3.346229	251.338780	4.977293
3.160562	252.759980	4.982298
3.099583	255.838464	4.987302
3.451582	240.562251	4.992307
3.189660	247.734550	4.997312
3.220847	246.926088	5.002317
3.488432	246.640582	5.007322
3.118245	250.419258	5.012326
3.311856	241.451190	5.017331
3.170588	256.634340	5.022336
3.541358	267.111778	5.027341
3.517334	276.097646	5.032346
3.183189	281.386149	5.037350
3.667038	272.325133	5.042355
3.554561	281.419777	5.047360
3.743490	289.970481	5.052365
3.792760	278.959037	5.057370
3.303705	269.009565	5.062374
3.634943	264.145537	5.067379
3.487345	278.899419	5.072384
3.415319	271.887065	5.077389
3.612899	280.730644	5.082394
3.757912	288.070159	5.087398
3.666470	285.562956	5.092403
3.676718	275.351747	5.097408
3.761180	277.420337	5.102413
3.757241	280.777795	5.107418
3.308395	277.738123	5.112422
3.789974	278.368232	5.117427
3.617648	277.136066	5.122432
3.562282	278.644422	5.127437
3.730089	278.374548	5.132442
3.527077	274.363033	5.137446
3.574690	274.602383	5.142451
3.431845	274.700728	5.147456
3.421028	273.364162	5.152461
3.693817	274.469918	5.157466
3.700123	276.863971	5.162470
4.074419	271.923591	5.167475
3.819160	274.137159	5.172480
3.752442	276.678698	5.177485
3.761440	275.190327	5.182490
3.765557	280.675772	5.187494
3.673899	277.311210	5.192499
3.805081	286.567000	5.197504
4.119845	291.051466	5.202509
4.362141	290.064390	5.207514
3.758981	285.609356	5.212518
3.920253	271.590561	5.217523
3.785497	284.260645	5.222528
3.909689	287.756220	5.227533
4.258401	290.213687	5.232538
3.856356	295.484359	5.237542
3.788268	286.177614	5.242547
4.048754	301.592089	5.247552
3.955835	307.399637	5.252557
4.037079	306.463104	5.257562
4.132205	300.933692	5.262566
4.279672	303.153768	5.267571
4.592951	309.321625	5.272576
4.073590	295.827078	5.277581
4.134896	285.845149	5.282586
3.667672	280.938539	5.287590
4.333057	293.514899	5.292595
3.964230	287.918977	5.297600
4.145104	298.850139	5.302605
4.325433	300.998625	5.307610
4.267351	309.012225	5.312614
4.169140	296.869083	5.317619
4.310796	302.127336	5.322624
4.187617	298.723415	5.327629
4.197036	295.751146	5.332634
4.008184	305.686689	5.337638
4.461493	305.356263	5.342643
4.251401	302.415222	5.347648
4.182347	305.336789	5.352653
4.052397	297.238819	5.357658
3.739831	313.008852	5.362662
4.704804	306.580668	5.367667
4.548760	309.259597	5.372672
4.367583	309.208921	5.377677
4.179540	299.288200	5.382682
4.189538	306.528651	5.387686
4.704209	303.629080	5.392691
4.398971	309.890683	5.397696
4.317121	307.723667	5.402701
4.281604	298.927515	5.407706
4.233342	307.683073	5.412710
4.246669	304.833579	5.417715
4.177198	307.087646	5.422720
4.068443	310.024925	5.427725
4.449586	305.766849	5.432730
4.079089	314.452674	5.437734
4.459656	316.712161	5.442739
4.567116	327.281511	5.447744
4.932052	333.555180	5.452749
4.450519	321.215811	5.457754
4.381707	316.787781	5.462758
4.740746	318.974709	5.467763
4.226969	317.055705	5.472768
4.565249	328.364028	5.477773
4.708950	332.321637	5.482778
4.402318	338.795445	5.487782
4.614580	335.440202	5.492787
4.819866	342.175496	5.497792
4.735867	332.077100	5.502797
4.611088	334.447405	5.507802
4.743076	336.299743	5.512806
4.703990	337.001942	5.517811
4.953037	340.322937	5.522816
4.685442	337.381408	5.527821
4.824911	333.711697	5.532826
4.622721	333.847815	5.537830
4.613635	340.205399	5.542835
4.613834	329.495849	5.547840
4.829869	330.610501	5.552845
4.584969	332.271948	5.557850
4.698748	331.921952	5.562854
4.880392	335.519269	5.567859
4.649191	332.954861	5.572864
4.808805	334.268183	5.577869
4.763566	333.544460	5.582874
4.474154	337.762926	5.587878
4.776792	329.382023	5.592883
4.566656	337.254940	5.597888
4.522682	339.150668	5.602893
5.162278	343.663348	5.607898
4.817177	338.889451	5.612902
5.086484	337.951925	5.617907
4.859990	340.777940	5.622912
4.968798	349.081792	5.627917
4.911287	341.576744	5.632922
5.073090	357.607857	5.637926
5.336379	346.607132	5.642931
4.723411	347.386592	5.647936
5.127426	343.090121	5.652941
5.080651	351.016545	5.657946
4.948759	357.529421	5.662950
5.158199	351.665700	5.667955
5.711314	357.065151	5.672960
5.212434	348.733890	5.677965
5.355564	335.597431	5.682970
4.914665	334.249151	5.687974
4.955379	325.330308	5.692979
4.907064	332.690641	5.697984
4.995299	330.430532	5.702989
5.278418	334.483359	5.707994
5.429086	350.899034	5.712998
5.167625	344.485822	5.718003
5.106613	343.982874	5.723008
4.953346	341.320831	5.728013
5.317524	361.341464	5.733018
5.507004	360.210795	5.738022
5.103720	353.794491	5.743027
4.847047	353.682876	5.748032
5.122655	367.177758	5.753037
5.286115	361.656604	5.758042
4.893946	366.267672	5.763046
5.399851	363.739632	5.768051
5.451572	374.861924	5.773056
5.244963	369.028582	5.778061
5.503083	367.722639	5.783066
5.397405	355.276899	5.788070
5.335998	364.575560	5.793075
5.350909	363.491226	5.798080
5.210465	357.498821	5.803085
5.617876	353.062607	5.808090
5.432098	359.207431	5.813094
5.729848	363.394018	5.818099
5.802957	363.708470	5.823104
5.290288	360.640817	5.828109
5.771463	356.509427	5.833114
5.526314	364.030330	5.838118
5.538152	362.655405	5.843123
5.344544	361.932781	5.848128
5.551681	367.326330	5.853133
5.634216	358.660352	5.858138
5.215386	373.893418	5.863142
5.835973	365.791719	5.868147
5.893574	362.362625	5.873152
5.668926	359.778204	5.878157
5.618756	353.898209	5.883162
5.470834	362.859240	5.888166
5.692966	368.304225	5.893171
5.771612	357.974681	5.898176
6.078508	362.536330	5.903181
5.993721	354.010469	5.908186
5.768401	354.273601	5.913190
5.446362	349.932696	5.918195
5.603581	362.901945	5.923200
5.757097	366.971923	5.928205
5.871497	356.798133	5.933210
5.671109	363.840612	5.938214
5.544068	360.007004	5.943219
5.580078	367.790747	5.948224
5.267859	361.404465	5.953229
5.579902	355.027946	5.958234
5.237515	352.977677	5.963238
5.180506	360.345711	5.968243
5.544314	367.590865	5.973248
5.579940	383.866403	5.978253
5.785214	384.191786	5.983258
5.929359	388.120864	5.988262
6.074370	384.956487	5.993267
5.630378	379.062257	5.998272
5.832746	380.479619	6.003277
5.905495	365.205922	6.008282
5.845375	367.638870	6.013286
5.432503	357.652100	6.018291
5.655370	365.919106	6.023296
5.631967	379.239379	6.028301
6.073506	381.002090	6.033306
5.724168	386.201253	6.038310
5.606912	380.818991	6.043315
5.870460	383.894108	6.048320
5.767070	388.972477	6.053325
6.024625	377.640428	6.058330
5.597180	372.338409	6.063334
5.438220	359.391637	6.068339
5.821333	375.229899	6.073344
6.262389	385.468598	6.078349
6.033806	368.869008	6.083354
6.033767	371.080565	6.088358
5.605186	359.039765	6.093363
5.907430	359.387920	6.098368
5.611751	361.117438	6.103373
5.647544	362.254006	6.108378
5.407221	355.619174	6.113382
5.453136	362.044080	6.118387
5.794036	370.260956	6.123392
5.813505	388.813826	6.128397
6.115396	374.848849	6.133402
5.777737	369.564401	6.138406
5.969926	359.368930	6.143411
5.839599	359.746896	6.148416
5.587310	360.520466	6.153421
5.764251	364.944286	6.158426
5.658454	368.399980	6.163430
5.656716	360.705847	6.168435
5.725181	353.573370	6.173440
5.690036	358.837195	6.178445
5.800737	360.781458	6.183450
5.613922	369.429038	6.188454
5.788768	374.609345	6.193459
5.861631	379.492412	6.198464
5.836141	389.693479	6.203469
5.810665	371.543421	6.208474
5.645421	364.941116	6.213478
6.002131	378.015165	6.218483
5.623458	370.649012	6.223488
5.616104	361.098588	6.228493
5.967894	362.770954	6.233498
5.732122	368.917287	6.238502
5.813332	365.475001	6.243507
5.881961	364.021574	6.248512
5.821002	365.986406	6.253517
5.788438	361.584323	6.258522
5.635926	372.001440	6.263526
5.494247	367.619616	6.268531
5.835575	365.111035	6.273536
5.602895	389.104074	6.278541
6.319528	382.233871	6.283546
5.707051	381.810999	6.288550
5.811613	369.212082	6.293555
5.870341	359.882266	6.298560
5.618132	369.938506	6.303565
5.993090	358.746266	6.308570
5.428146	363.030055	6.313574
5.729870	367.206528	6.318579
5.759222	360.842661	6.323584
5.692165	370.069442	6.328589
5.690303	364.124926	6.333594
5.668711	376.185707	6.338598
5.710055	386.819238	6.343603
6.076013	387.189049	6.348608
5.456635	383.834382	6.353613
5.670822	376.846748	6.358618
5.840997	395.230475	6.363622
5.790864	395.497797	6.368627
5.918465	393.680778	6.373632
5.628337	393.533274	6.378637
6.139242	383.800394	6.383642
5.892588	376.521124	6.388646
5.764207	371.504449	6.393651
5.657730	368.597784	6.398656
5.420656	373.915398	6.403661
5.591636	376.742419	6.408666
5.574867	392.244707	6.413670
6.039161	392.051768	6.418675
6.198098	395.364745	6.423680
6.007425	385.121677	6.428685
5.916345	371.588443	6.433690
5.727807	378.319015	6.438694
5.724683	368.245893	6.443699
5.637271	363.469580	6.448704
5.591336	362.635231	6.453709
5.689824	360.898708	6.458714
5.479118	369.910709	6.463718
6.184105	369.594634	6.468723
5.983625	375.317813	6.473728
6.050493	373.310990	6.478733
6.469534	365.785050	6.483738
5.680196	363.554866	6.488742
5.853121	363.780911	6.493747
5.915277	363.258665	6.498752
5.766315	370.438625	6.503757
5.908549	365.101134	6.508762
5.697710	374.594060	6.513766
5.863566	370.290604	6.518771
5.932056	364.395178	6.523776
5.844118	366.677456	6.528781
5.835780	364.457785	6.533786
5.709406	366.799871	6.538790
5.926543	364.854928	6.543795
6.432104	357.441988	6.548800
5.734102	355.346195	6.553805
5.623379	342.907582	6.558810
5.435014	351.223195	6.563814
5.680292	353.931001	6.568819
5.500107	363.479231	6.573824
5.419473	361.881507	6.578829
5.824379	360.954373	6.583834
5.808589	367.847704	6.588838
5.931075	364.243924	6.593843
5.637393	361.550094	6.598848
5.984779	366.880538	6.603853
6.112224	361.298587	6.608858
5.888455	375.194429	6.613862
5.553270	360.025783	6.618867
6.029017	349.159451	6.623872
5.886723	361.239134	6.628877
5.937195	351.685983	6.633882
5.225806	358.773723	6.638886
5.689229	352.382977	6.643891
5.944473	357.905030	6.648896
5.617807	363.246171	6.653901
6.070104	358.296709	6.658906
5.840736	357.642965	6.663910
5.638848	368.330413	6.668915
6.023722	361.765305	6.673920
5.651770	360.697292	6.678925
5.876329	347.984675	6.683930
5.493873	347.756723	6.688934
5.549245	356.296746	6.693939
5.727537	362.308597	6.698944
5.521495	366.283046	6.703949
5.776322	362.123843	6.708954
5.416062	357.627570	6.713958
5.653402	362.693675	6.718963
5.946677	361.670133	6.723968
5.542869	369.386743	6.728973
5.776644	363.775476	6.733978
6.165466	360.901941	6.738982
5.482048	366.330618	6.743987
5.558618	350.926618	6.748992
5.613345	354.104052	6.753997
5.633296	354.955192	6.759002
5.537874	358.902817	6.764006
5.617508	358.611955	6.769011
5.810757	355.095168	6.774016
5.563459	363.480133	6.779021
5.890764	358.550256	6.784026
5.614413	366.038082	6.789030
5.935118	359.074895	6.794035
5.712368	367.285169	6.799040
5.649099	364.428683	6.804045
6.020442	354.888532	6.809050
5.842424	365.679809	6.814054
5.833681	366.633525	6.819059
5.553786	365.975042	6.824064
5.389591	368.218647	6.829069
5.620931	366.189218	6.834074
5.993713	366.858524	6.839078
5.933332	371.743483	6.844083
5.831340	377.887841	6.849088
5.822762	376.149109	6.854093
5.979278	364.994256	6.859098
5.802703	371.185099	6.864102
5.773637	367.079868	6.869107
5.650262	358.917563	6.874112
5.535164	366.386452	6.879117
5.712552	364.552144	6.884122
5.884537	367.084769	6.889126
5.647323	369.251228	6.894131
5.646695	360.408449	6.899136
5.554703	359.214312	6.904141
5.624435	354.910101	6.909146
5.418751	374.475857	6.914150
5.684996	388.032335	6.919155
5.728935	394.119031	6.924160
5.853161	395.618242	6.929165
5.800538	393.785166	6.934170
5.863119	399.065330	6.939174
6.048480	402.095751	6.944179
6.206813	378.509888	6.949184
5.854158	375.752527	6.954189
6.135013	363.736613	6.959194
5.896720	362.264834	6.964198
5.772875	367.273633	6.969203
5.867112	367.815735	6.974208
5.641172	370.603702	6.979213
5.975721	362.344337	6.984218
6.120559	366.175223	6.989222
5.863344	358.777389	6.994227
5.759374	365.447249	6.999232
5.544223	369.831261	7.004237
5.704949	368.920238	7.009242
5.767928	372.330506	7.014246
5.740123	366.133784	7.019251
5.951992	364.211813	7.024256
5.873922	369.501349	7.029261
5.730510	362.148960	7.034266
5.836173	363.869380	7.039270
5.663484	364.004041	7.044275
5.747295	367.161101	7.049280
5.572422	370.162535	7.054285
5.434262	367.969532	7.059290
5.741721	366.254052	7.064294
5.642209	365.937474	7.069299
5.643401	359.464121	7.074304
5.549625	368.059158	7.079309
5.833804	366.774443	7.084314
5.667298	373.640770	7.089318
5.546016	365.797681	7.094323
5.789204	368.179942	7.099328
5.506398	371.628569	7.104333
5.426665	366.512522	7.109338
5.988681	382.433494	7.114342
5.823651	392.782979	7.119347
5.864752	371.718088	7.124352
5.800818	375.341236	7.129357
5.928380	367.810343	7.134362
5.549557	369.970514	7.139366
5.998821	364.221077	7.144371
5.795141	366.046915	7.149376
5.761065	362.736591	7.154381
5.856553	358.415689	7.159386
6.120246	361.629988	7.164390
5.826740	359.869460	7.169395
6.185416	369.655975	7.174400
5.891387	366.367397	7.179405
6.227033	367.070996	7.184410
6.096295	364.193443	7.189414
5.976383	359.618381	7.194419
5.925050	369.795011	7.199424
5.920633	367.030546	7.204429
5.904981	355.193976	7.209434
5.818280	348.781856	7.214438
5.320005	348.894761	7.219443
5.475959	346.586074	7.224448
5.586421	361.451454	7.229453
5.691243	359.062190	7.234458
6.111654	367.032483	7.239462
5.796691	365.275317	7.244467
5.750981	361.631450	7.249472
5.621621	367.371959	7.254477
5.693553	357.809114	7.259482
5.662391	370.557943	7.264486
5.788159	359.961580	7.269491
5.890221	365.665829	7.274496
5.590285	363.678512	7.279501
5.918811	365.104580	7.284506
5.514886	367.262357	7.289510
5.426247	365.368487	7.294515
6.322740	361.814281	7.299520
5.863111	365.094454	7.304525
5.887709	364.375607	7.309530
5.588393	367.801509	7.314534
5.698538	372.574327	7.319539
5.888198	365.505116	7.324544
5.548588	371.848058	7.329549
5.656246	366.788074	7.334554
5.731015	366.143625	7.339558
5.687335	371.098735	7.344563
5.982487	369.325070	7.349568
5.624921	369.523499	7.354573
6.385535	363.304490	7.359578
6.271952	365.812254	7.364582
5.878192	353.645776	7.369587
5.491196	348.552566	7.374592
5.394559	342.913979	7.379597
5.687769	362.189577	7.384602
5.741110	362.560912	7.389606
5.888302	362.971327	7.394611
5.965462	362.908649	7.399616
5.819582	371.647896	7.404621
5.741235	366.977732	7.409626
5.720568	363.456494	7.414630
5.729485	356.981932	7.419635
6.025273	363.804297	7.424640
5.908839	356.995025	7.429645
5.935149	337.403673	7.434650
5.660581	339.180503	7.439654
5.524794	339.106896	7.444659
5.805028	340.562675	7.449664
5.867755	337.395380	7.454669
5.788908	339.090923	7.459674
5.898121	339.934405	7.464678
5.760415	342.838260	7.469683
5.586070	338.347664	7.474688
5.573150	339.286214	7.479693
6.107235	344.770901	7.484698
5.825838	332.311580	7.489702
5.505298	338.705307	7.494707
5.905162	341.853973	7.499712
5.798692	341.076567	7.504717
5.818555	341.032357	7.509722
5.897653	339.023622	7.514726
6.004024	345.980064	7.519731
5.838357	344.731031	7.524736
5.536248	350.523911	7.529741
5.544398	346.226188	7.534746
5.585955	341.628995	7.539750
5.838496	345.474639	7.544755
5.795836	335.515300	7.549760
5.626074	345.030249	7.554765
6.054042	343.466736	7.559770
5.823980	339.266450	7.564774
5.639720	344.091716	7.569779
5.657133	338.216956	7.574784
5.186688	350.259460	7.579789
5.676742	360.123464	7.584794
5.696006	367.928814	7.589798
5.814687	375.797687	7.594803
6.150252	361.643942	7.599808
5.923365	366.112052	7.604813
5.891223	357.002123	7.609818
5.630903	347.877329	7.614822
5.835839	344.801649	7.619827
5.657633	345.671182	7.624832
5.613986	343.479193	7.629837
5.937076	360.712603	7.634842
5.704249	368.263215	7.639846
5.917271	364.034630	7.644851
6.093903	350.408845	7.649856
5.849296	345.688805	7.654861
5.829662	340.958827	7.659866
5.481753	345.445894	7.664870
5.588232	337.168489	7.669875
5.985434	332.980658	7.674880
5.647139	346.777361	7.679885
5.679055	343.652858	7.684890
5.416951	350.755623	7.689894
5.897331	362.589045	7.694899
5.845477	363.081269	7.699904
5.891816	358.575073	7.704909
5.672481	344.935402	7.709914
5.803298	339.476318	7.714918
5.788416	330.819289	7.719923
5.893149	343.841042	7.724928
5.783753	345.054142	7.729933
6.080757	341.293306	7.734938
5.969596	340.029405	7.739942
5.725706	340.311266	7.744947
6.133894	338.829948	7.749952
5.632135	338.829502	7.754957
5.941472	340.654052	7.759962
5.632152	340.699386	7.764966
5.796539	333.112117	7.769971
6.183236	334.703078	7.774976
5.599294	341.150732	7.779981
5.718409	340.426568	7.784986
5.819985	344.099708	7.789990
5.529420	337.317728	7.794995
5.787794	335.505535	7.800000
5.434307	339.132913	7.805005
5.729756	333.546794	7.810010
5.776370	341.363666	7.815014
5.749634	348.477010	7.820019
5.531692	334.628315	7.825024
5.462775	344.355259	7.830029
5.606207	339.197926	7.835034
5.425869	353.558357	7.840038
5.793277	362.400678	7.845043
5.721174	362.193703	7.850048
6.272383	362.825561	7.855053
6.190255	363.142190	7.860058
6.034428	343.069992	7.865062
5.845877	344.248037	7.870067
6.046890	339.363263	7.875072
5.717824	336.630687	7.880077
6.182416	326.617186	7.885082
6.061596	333.299165	7.890086
5.915873	335.932186	7.895091
5.767734	331.595677	7.900096
5.741263	331.099973	7.905101
6.010966	326.153819	7.910106
5.884726	331.444564	7.915110
5.777596	339.070384	7.920115
5.899033	343.142219	7.925120
5.773269	344.908389	7.930125
6.052851	332.649080	7.935130
5.992986	317.620834	7.940134
5.535231	306.998506	7.945152
5.546015	309.603499	7.950170
5.824278	324.057459	7.955187
6.051074	333.795328	7.960205
5.639485	319.311824	7.965222
5.672521	327.918731	7.970240
6.051787	332.766538	7.975258
5.514317	327.779485	7.980275
5.558875	330.464394	7.985293
5.600064	330.470597	7.990310
5.854250	340.431392	7.995328
6.062378	333.572915	8.000346
5.684456	336.289307	8.005363
5.683424	336.630323	8.010381
5.969984	339.198423	8.015398
5.461390	339.808310	8.020416
5.678134	330.913022	8.025434
5.552339	339.800437	8.030451
5.656283	340.352220	8.035469
5.587237	332.262246	8.040486
5.519743	339.685724	8.045504
5.646626	328.387207	8.050522
5.635217	342.848699	8.055539
5.811219	355.942797	8.060557
6.010638	358.155329	8.065574
6.287919	352.103351	8.070592
5.890194	349.268715	8.075610
5.596033	336.199512	8.080627
5.834307	345.238167	8.085645
5.908825	353.920637	8.090662
5.834934	366.435367	8.095680
6.084295	361.432318	8.100698
6.041369	363.379869	8.105715
5.875408	353.083416	8.110733
5.855871	339.497819	8.115750
6.113481	350.101857	8.120768
6.056839	347.377878	8.125786
6.031274	345.422191	8.130803
6.014779	344.159350	8.135821
5.841724	334.993779	8.140838
5.671954	339.163919	8.145856
6.138658	348.905232	8.150874
5.884237	356.301201	8.155891
6.162063	352.795836	8.160909
6.162578	343.622000	8.165926
5.509291	348.549544	8.170944
6.130450	341.298151	8.175962
5.839009	357.460303	8.180979
5.599248	360.574767	8.185997
5.961049	363.112147	8.191014
5.810451	365.319562	8.196032
5.881948	368.486244	8.201050
6.060337	365.463509	8.206067
6.442541	363.579628	8.211085
6.144833	367.877115	8.216102
5.984230	367.836041	8.221120
6.137298	365.375843	8.226138
6.123658	360.543388	8.231155
6.167650	366.071732	8.236173
5.951451	368.504017	8.241190
6.010961	370.605930	8.246208
6.050741	359.090671	8.251226
6.030947	369.135435	8.256243
6.006209	361.243630	8.261261
5.888294	358.008550	8.266278
6.144477	372.535435	8.271296
6.019253	360.377007	8.276314
6.180027	358.556222	8.281331
6.164095	365.798064	8.286349
6.164654	364.242220	8.291366
6.280036	361.178865	8.296384
6.342076	359.932120	8.301402
6.144234	357.750963	8.306419
5.995198	364.966324	8.311437
6.015063	360.753460	8.316454
5.743073	372.040085	8.321472
6.237523	359.891861	8.326490
6.206367	368.688724	8.331507
6.369901	362.847067	8.336525
6.218233	358.632677	8.341542
6.310573	362.061176	8.346560
6.148860	354.395961	8.351578
6.056837	363.151865	8.356595
5.966417	359.287636	8.361613
6.163481	358.294286	8.366630
6.204055	361.885528	8.371648
6.271844	351.281056	8.376666
6.128937	366.782480	8.381683
6.050898	361.054412	8.386701
6.078786	358.771616	8.391718
6.032814	359.321643	8.396736
6.067828	359.265697	8.401754
6.214118	350.886359	8.406771
6.147346	358.577971	8.411789
5.947710	362.553983	8.416806
6.082052	378.071937	8.421824
6.282275	389.164666	8.426842
6.458615	391.311391	8.431859
6.427909	396.854604	8.436877
6.820869	386.943923	8.441894
6.506373	375.162274	8.446912
6.448660	361.955021	8.451930
6.518170	356.683512	8.456947
6.366300	362.289879	8.461965
6.357616	361.884179	8.466982
6.102935	366.159146	8.472000
6.221242	362.382131	8.477018
6.190675	354.806819	8.482035
6.245376	359.251057	8.487053
6.436921	361.805646	8.492070
5.968552	357.722928	8.497088
6.138242	351.981294	8.502106
6.326299	368.573248	8.507123
6.706134	367.361915	8.512141
6.401681	356.042602	8.517158
6.495196	353.481285	8.522176
6.489264	355.063283	8.527194
6.164965	359.036736	8.532211
6.426839	359.399675	8.537229
6.440733	350.220584	8.542246
6.138645	355.572778	8.547264
6.273200	354.825904	8.552282
6.562367	374.226426	8.557299
6.418606	382.018472	8.562317
6.523261	370.448860	8.567335
6.292814	375.265979	8.572352
6.241926	374.945786	8.577370
6.716801	377.124629	8.582387
6.558975	394.427199	8.587405
6.429486	377.529468	8.592423
6.061741	374.014796	8.597440
6.374285	381.331410	8.602458
6.849332	379.098469	8.607475
6.306897	385.536044	8.612493
6.377558	383.098223	8.617511
6.529176	388.890573	8.622528
6.485844	380.092814	8.627546
6.567126	385.091464	8.632563
6.516708	395.601782	8.637581
6.138957	386.846949	8.642599
6.462137	389.582886	8.647616
6.434941	382.969542	8.652634
6.742983	393.082872	8.657651
6.307247	397.354657	8.662669
6.629371	387.650732	8.667687
6.401443	383.577672	8.672704
6.558579	381.757455	8.677722
6.589713	384.539149	8.682739
6.097802	384.310146	8.687757
6.802791	377.831389	8.692775
6.672931	384.147516	8.697792
6.766128	382.009118	8.702810
6.299384	391.369695	8.707827
6.619353	391.111314	8.712845
6.483656	388.554348	8.717863
6.367556	391.961863	8.722880
6.544933	374.271294	8.727898
6.537042	383.408497	8.732915
6.527177	391.141699	8.737933
6.462809	392.527730	8.742951
6.391724	391.939305	8.747968
6.590391	388.383221	8.752986
6.752997	389.960905	8.758003
6.618541	395.195329	8.763021
7.032158	385.704285	8.768039
6.753213	392.706485	8.773056
6.467215	396.481444	8.778074
6.453790	388.865562	8.783091
6.426654	380.633302	8.788109
6.685690	386.459313	8.793127
6.684034	401.531543	8.798144
6.689816	403.654501	8.803162
6.752699	404.146448	8.808179
6.715094	417.709555	8.813197
7.057572	409.245803	8.818215
6.584284	400.445973	8.823232
6.713969	398.096730	8.828250
6.758695	391.244899	8.833267
6.628480	395.273156	8.838285
6.645639	400.966659	8.843303
6.714281	401.710165	8.848320
6.855653	415.368303	8.853338
6.804367	410.920425	8.858355
6.989495	412.399909	8.863373
7.030217	403.923480	8.868391
6.586406	387.106545	8.873408
6.493665	393.019234	8.878426
6.690740	404.630011	8.883443
6.949689	406.350390	8.888461
7.004125	409.825862	8.893479
6.786904	406.167680	8.898496
6.549362	401.846816	8.903514
7.191279	402.737183	8.908531
6.642494	401.967988	8.913549
6.697595	402.615787	8.918567
7.038732	405.822277	8.923584
6.979019	409.883672	8.928602
7.366322	405.509086	8.933619
6.879398	395.729951	8.938637
6.904134	390.762089	8.943655
6.771229	395.677538	8.948672
6.440096	397.480903	8.953690
7.056801	388.870054	8.958707
6.762129	395.653816	8.963725
7.183773	401.997146	8.968743
6.877931	383.394524	8.973760
6.754568	388.485199	8.978778
6.918458	388.566849	8.983795
6.613831	401.991904	8.988813
7.074515	396.169949	8.993831
7.335868	405.283912	8.998848
7.161271	404.121576	9.003866
6.849152	385.447353	9.008883
6.720261	394.104910	9.013901
6.635849	391.063387	9.018919
6.937933	405.602042	9.023936
6.847963	408.326976	9.028954
7.135818	399.104935	9.033971
7.055093	413.302793	9.038989
7.057530	400.070308	9.044007
7.258263	406.508213	9.049024
6.977348	396.905080	9.054042
6.958331	383.136333	9.059059
7.021367	393.382725	9.064077
6.919133	393.026396	9.069095
7.175873	400.234997	9.074112
6.930729	404.268640	9.079130
7.078393	413.046975	9.084147
6.911243	422.887641	9.089165
7.461878	412.232726	9.094183
7.228960	398.446990	9.099200
6.743722	397.068242	9.104218
6.972519	391.891684	9.109235
6.821393	403.714806	9.114253
7.064393	408.012790	9.119271
6.978156	408.408183	9.124288
7.020906	412.570288	9.129306
7.094173	406.632307	9.134323
6.862009	407.605979	9.139341
6.938055	402.746838	9.144359
7.341158	400.159098	9.149376
7.156008	406.834186	9.154394
7.478390	405.821198	9.159411
7.385852	403.194353	9.164429
7.318840	412.435507	9.169447
7.288265	404.661361	9.174464
6.923532	412.027300	9.179482
7.039809	416.591291	9.184499
6.969307	407.561093	9.189517
7.568012	403.705644	9.194535
7.509264	404.980344	9.199552
7.228917	402.588049	9.204570
7.307424	395.159730	9.209587
6.853380	401.375180	9.214605
7.153179	408.286708	9.219623
7.311268	399.425822	9.224640
7.365685	398.230760	9.229658
7.216190	406.146790	9.234675
7.321939	411.223664	9.239693
7.195505	403.836918	9.244711
6.903104	407.789606	9.249728
7.171093	404.699177	9.254746
7.117308	409.318214	9.259763
6.902012	408.228526	9.264781
6.877018	404.915763	9.269799
7.013262	409.782734	9.274816
7.197199	411.716835	9.279834
7.523752	410.491757	9.284851
7.486004	408.717850	9.289869
7.328150	408.098839	9.294887
7.382684	410.308833	9.299904
7.108405	409.477692	9.304922
7.607736	408.547431	9.309939
7.334691	408.028518	9.314957
7.417670	407.280256	9.319975
7.354697	407.160769	9.324992
7.216274	403.206222	9.330010
7.135256	403.007513	9.335027
7.054195	403.108607	9.340045
7.104126	411.100689	9.345063
7.510740	411.336811	9.350080
7.340957	411.035245	9.355098
7.225413	408.405692	9.360115
7.147603	408.853412	9.365133
7.398610	427.101804	9.370151
7.688156	426.699868	9.375168
7.374140	435.358048	9.380186
7.595058	434.383046	9.385203
7.284742	431.575726	9.390221
7.168883	435.355592	9.395239
7.276755	438.967863	9.400256
7.562369	444.287961	9.405274
7.564079	436.363578	9.410291
7.515854	434.783812	9.415309
7.544211	444.404512	9.420327
7.848908	437.240534	9.425344
7.177990	438.254550	9.430362
7.881626	441.981757	9.435379
7.681140	434.171105	9.440397
7.551814	422.508733	9.445415
7.649791	417.661930	9.450432
7.406665	415.945448	9.455450
7.215903	406.236667	9.460467
7.551794	424.859916	9.465485
7.396873	433.357470	9.470503
7.464865	431.977244	9.475520
7.291042	442.323891	9.480538
7.723373	439.065698	9.485555
7.667238	440.466222	9.490573
7.023870	440.526034	9.495591
7.494546	432.701741	9.500608
7.577787	449.619459	9.505626
7.525278	441.198644	9.510643
7.622490	444.515944	9.515661
7.377433	446.233244	9.520679
7.625303	434.587504	9.525696
7.563354	435.843773	9.530714
7.396141	431.470858	9.535731
7.365274	439.690204	9.540749
7.439285	437.188735	9.545767
7.823453	430.952728	9.550784
7.225992	449.845318	9.555802
7.666041	443.991867	9.560819
7.789542	450.590210	9.565837
7.765009	455.343530	9.570855
7.645227	438.504179	9.575872
7.718218	439.755085	9.580890
7.570867	438.033062	9.585907
7.932634	447.923414	9.590925
7.689833	450.479798	9.595943
7.802876	452.096811	9.600960
7.621795	448.707510	9.605978
7.827805	454.008526	9.610995
7.678085	447.395421	9.616013
7.425836	453.866447	9.621031
8.070595	460.420992	9.626048
7.842532	470.312253	9.631066
7.937377	455.462114	9.636083
7.976105	448.406075	9.641101
7.879947	451.094116	9.646119
7.922723	430.805286	9.651136
7.649025	433.517986	9.656154
7.763303	428.599199	9.661171
7.576052	440.118739	9.666189
7.273026	440.494451	9.671207
7.994026	452.083130	9.676224
7.938919	461.483389	9.681242
8.018941	460.871286	9.686259
7.995328	460.575219	9.691277
7.917524	445.386069	9.696295
7.910853	434.319848	9.701312
7.555929	444.537082	9.706330
7.774481	452.363908	9.711347
7.952454	458.950564	9.716365
7.876687	463.443672	9.721383
7.832402	466.183547	9.726400
8.030776	469.421885	9.731418
7.473572	466.009463	9.736435
7.997263	460.449012	9.741453
7.910859	465.458179	9.746471
7.838913	461.666772	9.751488
7.814808	468.988831	9.756506
8.160464	471.509822	9.761523
8.135536	473.628133	9.766541
8.252172	460.355620	9.771559
8.156758	462.838421	9.776576
7.829045	458.010968	9.781594
7.999294	460.142878	9.786611
7.958980	465.640280	9.791629
7.741849	466.936645	9.796647
8.276270	473.088763	9.801664
7.806536	469.375459	9.806682
7.886429	464.739759	9.811699
7.852549	465.717079	9.816717
7.597301	452.502840	9.821735
7.571746	466.578488	9.826752
8.017582	461.137532	9.831770
7.526374	463.773864	9.836787
7.542356	477.385424	9.841805
7.344412	486.322086	9.846823
7.635259	491.663469	9.851840
7.634022	497.978418	9.856858
8.131587	495.019261	9.861875
7.977295	494.765760	9.866893
7.925003	495.755434	9.871911
8.412517	497.061316	9.876928
8.380772	489.060100	9.881946
7.879175	494.923274	9.886963
8.209317	492.088179	9.891981
8.064495	496.652075	9.896999
8.325275	495.569839	9.902016
7.916444	497.173951	9.907034
8.096950	502.333811	9.912051
8.236096	493.479003	9.917069
7.944723	497.299005	9.922087
8.658816	498.307456	9.927104
8.071851	498.771838	9.932122
7.800900	502.837949	9.937139
8.448319	515.634241	9.942157
8.286511	513.289630	9.947175
8.391243	489.582777	9.952192
8.146837	496.204068	9.957210
7.945508	495.642357	9.962227
8.274953	498.696064	9.967245
8.489694	519.067763	9.972263
8.328940	519.752542	9.977280
8.314947	509.419565	9.982298
8.275023	498.513148	9.987315
8.505722	496.599343	9.992333
8.137085	498.500112	9.997351
8.550787	503.610812	10.002368
8.540443	499.462608	10.007386
8.438015	501.634091	10.012403
8.320671	496.183535	10.017421
8.433881	505.172439	10.022439
8.339430	492.030806	10.027456
8.139449	501.614730	10.032474
8.204365	508.957571	10.037491
8.261551	497.089204	10.042509
8.141574	505.464553	10.047527
8.406348	497.038180	10.052544
8.707022	512.905728	10.057562
8.361546	505.509080	10.062579
8.481206	494.962667	10.067597
8.557180	496.452949	10.072615
8.551642	493.607332	10.077632
8.418914	494.312966	10.082650
8.045812	494.014853	10.087667
8.460649	491.292719	10.092685
8.330668	493.995533	10.097703
8.483842	507.377339	10.102720
8.695195	505.633821	10.107738
8.832521	505.770127	10.112755
8.450991	488.510996	10.117773
8.311344	499.417206	10.122791
8.623411	490.143988	10.127808
8.622631	491.049852	10.132826
8.611402	497.659855	10.137843
8.697082	494.721052	10.142861
8.704332	496.048533	10.147879
8.587401	488.701289	10.152896
8.681514	494.578423	10.157914
8.268312	502.570527	10.162931
8.698404	496.945835	10.167949
8.417915	495.904226	10.172967
8.274572	498.362983	10.177984
8.409709	495.814059	10.183002
8.381393	493.795671	10.188019
8.748379	494.533461	10.193037
8.654470	505.991083	10.198055
8.364892	507.289334	10.203072
9.058862	508.098968	10.208090
8.595028	507.774046	10.213107
8.567582	494.170635	10.218125
8.419393	497.763078	10.223143
8.601533	510.569151	10.228160
8.740935	509.335520	10.233178
8.749572	519.445341	10.238195
8.657018	515.136446	10.243213
8.829305	523.039980	10.248231
8.712214	511.517644	10.253248
8.820935	512.791358	10.258266
8.591762	515.910502	10.263283
8.775046	514.875122	10.268301
9.011769	521.673500	10.273319
8.468703	493.618479	10.278336
8.791486	506.787519	10.283354
8.583547	517.521404	10.288371
8.906923	519.872324	10.293389
8.627985	522.361797	10.298407
8.666474	510.862422	10.303424
8.870763	524.103689	10.308442
9.026664	515.766949	10.313459
8.692974	512.404703	10.318477
8.919836	516.881966	10.323495
8.863131	515.139422	10.328512
8.902053	523.319470	10.333530
8.908214	517.836933	10.338547
8.784952	498.539713	10.343565
8.879595	508.064855	10.348583
8.546149	512.989667	10.353600
8.982434	519.807270	10.358618
8.836300	517.576967	10.363635
9.074583	517.189372	10.368653
9.001092	523.979553	10.373671
8.607879	516.388408	10.378688
8.985799	514.735556	10.383706
8.830217	521.983563	10.388723
8.822182	519.851542	10.393741
8.947255	524.376313	10.398759
9.013882	524.444802	10.403776
9.018494	519.489524	10.408794
8.704997	537.592948	10.413811
9.129384	526.900941	10.418829
9.185694	524.490596	10.423847
9.049244	524.505696	10.428864
9.132020	518.600902	10.433882
8.728260	531.675515	10.438899
8.725000	529.410201	10.443917
9.011805	521.652548	10.448935
8.863086	529.085675	10.453952
8.972810	522.788496	10.458970
8.698269	526.542752	10.463987
9.028419	523.480433	10.469005
9.004368	528.126400	10.474023
8.796631	523.687228	10.479040
8.831692	515.404136	10.484058
8.972994	524.710538	10.489075
8.922027	526.258582	10.494093
8.758456	521.449575	10.499111
8.681546	524.803638	10.504128
9.183865	538.238059	10.509146
9.388485	547.821730	10.514163
9.399992	548.552104	10.519181
9.207410	537.129941	10.524199
9.221845	530.506864	10.529216
9.182201	514.759412	10.534234
9.073008	522.968978	10.539251
9.265155	523.683671	10.544269
9.084332	528.979048	10.549287
9.013825	522.523916	10.554304
9.139657	522.532635	10.559322
9.142502	541.659466	10.564339
9.142943	551.467633	10.569357
9.522836	547.368729	10.574375
9.064792	552.584471	10.579392
9.360293	544.342610	10.584410
9.131197	549.875929	10.589427
9.351236	551.734962	10.594445
9.197356	565.423696	10.599463
9.026511	562.105354	10.604480
9.051451	552.877091	10.609498
8.899383	560.159277	10.614515
9.279709	562.043690	10.619533
9.275007	559.024363	10.624551
8.915166	561.520206	10.629568
9.711678	559.924839	10.634586
9.502609	560.074394	10.639603
9.617362	553.350383	10.644621
9.711686	558.378596	10.649639
9.205892	554.866584	10.654656
9.325444	560.588275	10.659674
9.101800	561.210327	10.664691
9.092120	552.309380	10.669709
9.497265	561.697538	10.674727
9.296640	555.445818	10.679744
9.623623	552.298784	10.684762
9.630288	553.512754	10.689779
9.458503	552.716040	10.694797
9.569990	553.380256	10.699815
9.559137	557.740141	10.704832
9.630946	552.152634	10.709850
9.428149	554.526040	10.714867
9.346649	549.937695	10.719885
9.345938	556.271518	10.724903
9.092994	564.557275	10.729920
9.505049	554.561459	10.734938
9.340044	562.890241	10.739955
9.517782	561.177231	10.744973
9.806598	551.538396	10.749991
9.497991	552.584013	10.755008
9.392545	545.165518	10.760026
9.485170	552.949003	10.765043
9.582058	556.916468	10.770061
9.387109	555.792025	10.775079
9.445492	566.784012	10.780096
9.454215	554.462454	10.785114
9.491574	558.922082	10.790131
9.294670	560.208973	10.795149
9.350942	565.363070	10.800167
9.500236	573.882453	10.805184
9.886250	577.018828	10.810202
9.449018	573.994684	10.815219
9.642424	586.530804	10.820237
9.552208	582.682274	10.825255
9.542417	591.551638	10.830272
9.872901	580.549265	10.835290
9.580591	587.092888	10.840307
9.629048	575.134318	10.845325
9.654668	576.531511	10.850343
9.803625	585.082510	10.855360
9.669186	578.934020	10.860378
9.539802	585.578347	10.865395
9.861522	586.108639	10.870413
9.975011	581.701173	10.875431
9.534034	576.964018	10.880448
9.405727	579.527727	10.885466
9.544845	579.931996	10.890483
9.650187	585.182552	10.895501
9.642953	582.731662	10.900519
9.597859	590.726089	10.905536
9.694010	582.897296	10.910554
9.687874	580.177992	10.915571
9.707660	579.332326	10.920589
9.894868	579.009538	10.925607
9.885373	584.079271	10.930624
9.704052	585.874961	10.935642
9.779275	588.012307	10.940659
9.563808	588.759311	10.945677
9.754035	591.601317	10.950695
9.760715	610.547740	10.955712
10.025064	603.188046	10.960730
9.839393	609.831734	10.965747
9.805053	616.006744	10.970765
9.940753	617.042710	10.975783
9.649348	609.792180	10.980800
9.912859	610.315815	10.985818
9.894650	607.342778	10.990835
9.751054	611.805525	10.995853
10.025448	608.325895	11.000871
9.350768	612.354302	11.005888
9.687599	613.267235	11.010906
10.310925	607.915191	11.015923
10.139845	609.131766	11.020941
10.281677	608.390053	11.025959
10.114441	621.822148	11.030976
10.327396	605.107232	11.035994
9.954154	615.781869	11.041011
10.111093	616.502082	11.046029
10.203289	613.372890	11.051047
9.895337	617.384864	11.056064
9.861088	611.608829	11.061082
9.958521	609.135224	11.066099
9.788055	612.548144	11.071117
10.054829	606.974254	11.076135
10.111154	619.086906	11.081152
9.966865	611.450408	11.086170
9.706248	617.102295	11.091187
9.777678	639.027151	11.096205
10.200275	635.129819	11.101223
10.326496	636.290347	11.106240
10.247123	647.565900	11.111258
10.355989	641.060531	11.116275
10.048889	649.790314	11.121293
10.468424	636.823663	11.126311
10.116216	641.385375	11.131328
10.292518	642.329774	11.136346
10.350377	640.673409	11.141363
10.592301	628.299482	11.146381
10.598606	618.676474	11.151399
10.195115	617.938151	11.156416
10.144179	612.789580	11.161434
10.252730	607.770655	11.166451
9.817966	612.436814	11.171469
10.372713	619.040234	11.176487
10.205393	640.560687	11.181504
10.136290	634.720677	11.186522
10.414727	635.355583	11.191539
10.426714	636.625528	11.196557
10.313435	643.160055	11.201575
9.991097	646.410584	11.206592
10.026247	635.596462	11.211610
10.372569	634.866890	11.216627
10.103137	644.449148	11.221645
10.429979	638.805877	11.226663
10.107192	645.092363	11.231680
10.326491	645.436733	11.236698
10.319797	637.627187	11.241715
10.250386	642.034137	11.246733
10.470087	639.863263	11.251751
10.190656	636.486181	11.256768
10.179007	641.581515	11.261786
10.350926	650.649656	11.266803
10.270089	663.355031	11.271821
10.711219	663.702514	11.276839
10.472006	672.771967	11.281856
10.467350	665.807847	11.286874
10.858047	663.007419	11.291891
10.824313	674.604043	11.296909
10.750791	666.688189	11.301927
10.421438	649.294494	11.306944
10.183346	658.691969	11.311962
10.744686	661.529488	11.316979
10.662864	667.216494	11.321997
11.073166	664.157372	11.327015
10.523752	655.208396	11.332032
10.292359	639.863264	11.337050
10.414625	656.424768	11.342067
10.418342	665.244716	11.347085
10.844618	666.620166	11.352103
10.572993	668.818178	11.357120
10.711500	666.808346	11.362138
10.673915	663.850959	11.367155
10.374370	673.305407	11.372173
10.731280	667.666882	11.377191
10.645489	653.895766	11.382208
10.686852	663.830128	11.387226
10.545573	656.808522	11.392243
10.544578	664.994889	11.397261
10.475072	667.666163	11.402279
10.686678	672.909563	11.407296
10.753549	669.923185	11.412314
10.644297	660.270923	11.417331
10.590784	666.054478	11.422349
11.147479	669.839471	11.427367
10.720301	671.099332	11.432384
10.724542	665.175237	11.437402
10.911566	664.581076	11.442419
10.772813	670.699882	11.447437
10.784447	673.317418	11.452455
10.903461	662.139845	11.457472
10.517264	662.124648	11.462490
10.950911	657.105266	11.467507
10.737730	672.753666	11.472525
10.742368	657.687118	11.477543
11.073094	679.804927	11.482560
10.893149	682.698635	11.487578
10.788764	676.368677	11.492595
10.886202	686.297420	11.497613
11.166317	681.866978	11.502631
10.946111	685.025772	11.507648
10.790766	695.006750	11.512666
11.234329	683.213422	11.517683
11.218613	678.037222	11.522701
10.955687	669.469387	11.527719
10.877156	670.286456	11.532736
10.819650	677.206734	11.537754
11.387149	686.777805	11.542771
10.797268	679.144822	11.547789
10.992086	689.929315	11.552807
11.144265	695.033709	11.557824
11.233742	694.991320	11.562842
11.266843	681.854809	11.567859
10.827204	672.939117	11.572877
10.786877	682.526525	11.577895
10.894150	686.056888	11.582912
11.163433	693.017489	11.587930
11.324227	688.596274	11.592947
11.300284	695.807947	11.597965
11.273072	692.435518	11.602983
11.398626	690.007989	11.608000
10.975652	694.631296	11.613018
11.252759	691.937023	11.618035
11.306972	690.511599	11.623053
11.043855	690.243587	11.628071
11.326583	695.996560	11.633088
11.335629	690.308391	11.638106
11.429570	689.470036	11.643123
11.241192	689.537454	11.648141
11.304638	689.549637	11.653159
11.350787	679.639485	11.658176
11.273269	676.931350	11.663194
10.991293	664.516407	11.668211
11.480087	680.828002	11.673229
11.222679	684.551203	11.678247
11.258686	686.363345	11.683264
11.039015	687.382411	11.688282
11.272295	688.873309	11.693299
11.330423	695.668179	11.698317
11.256543	691.463613	11.703335
11.552248	701.654792	11.708352
11.430100	690.398221	11.713370
11.463085	692.475926	11.718387
11.405825	699.333058	11.723405
11.401790	696.048514	11.728423
11.698495	695.680166	11.733440
11.287450	697.631781	11.738458
11.776008	694.513056	11.743475
11.323765	694.751205	11.748493
11.142620	691.270350	11.753511
11.497988	689.999713	11.758528
11.269115	689.518052	11.763546
11.309190	700.528769	11.768563
11.233107	702.869718	11.773581
11.153337	693.752463	11.778599
11.470188	687.760446	11.783616
11.165980	696.909523	11.788634
11.517464	694.632788	11.793651
11.693639	694.122377	11.798669
11.496724	691.574959	11.803687
11.637226	684.080001	11.808704
11.669742	698.011032	11.813722
11.828751	699.728164	11.818739
11.653015	688.852377	11.823757
11.499776	691.410541	11.828775
11.597616	691.120688	11.833792
11.428557	690.860030	11.838810
11.526181	697.850684	11.843827
11.525243	715.555019	11.848845
11.601083	721.596038	11.853863
12.310939	718.265910	11.858880
11.631463	713.465100	11.863898
11.921622	696.652795	11.868915
11.542877	704.844717	11.873933
11.477157	714.496082	11.878951
11.871415	712.496667	11.883968
12.159522	720.334804	11.888986
11.932670	705.749456	11.894003
11.789557	706.674477	11.899021
11.861747	698.615857	11.904039
11.280537	698.893148	11.909056
11.646105	715.533352	11.914074
11.882187	712.921244	11.919091
12.037604	717.971488	11.924109
11.978471	728.360291	11.929127
12.079024	716.223050	11.934144
11.862193	715.625891	11.939162
11.839767	709.103198	11.944179
11.696514	714.159211	11.949197
11.935496	723.724970	11.954215
11.773212	722.541749	11.959232
11.515256	724.794431	11.964250
12.053098	724.340963	11.969267
12.008269	723.669517	11.974285
12.082304	723.692664	11.979303
12.236500	713.636175	11.984320
12.089069	725.765046	11.989338
12.095497	727.878473	11.994355
12.040997	722.152913	11.999373
12.028097	726.112370	12.004391
11.870695	720.087350	12.009408
11.924394	721.401259	12.014426
12.080176	719.729544	12.019443
12.005846	721.773573	12.024461
12.010838	726.547586	12.029479
12.246092	722.808977	12.034496
12.108034	718.759628	12.039514
11.727801	716.872094	12.044531
12.353132	724.430176	12.049549
12.032357	719.623656	12.054567
11.699447	717.902277	12.059584
11.873388	719.077425	12.064602
11.667834	717.755816	12.069619
11.837304	721.667763	12.074637
12.255474	724.493011	12.079655
12.505874	714.219476	12.084672
12.234380	720.646276	12.089690
12.374412	712.378204	12.094707
12.003381	715.412311	12.099725
11.861670	724.876770	12.104743
12.251817	722.111133	12.109760
12.080030	746.355889	12.114778
12.582113	742.515508	12.119795
12.350450	751.034704	12.124813
12.377935	744.636722	12.129831
12.324270	732.959137	12.134848
12.307688	729.301010	12.139866
12.302934	739.226860	12.144883
12.499982	744.270589	12.149901
12.242717	746.422179	12.154919
12.338335	742.658107	12.159936
12.015608	745.823507	12.164954
12.333959	745.824153	12.169971
12.335447	745.404228	12.174989
12.026623	747.516559	12.180007
12.328362	742.432614	12.185024
12.365450	742.082850	12.190042
12.124636	740.438558	12.195059
12.577181	749.210315	12.200077
12.543679	752.425074	12.205095
12.685982	747.321927	12.210112
12.658139	755.484139	12.215130
12.423043	753.318238	12.220147
12.418657	752.877142	12.225165
12.012244	753.265902	12.230183
12.363330	751.790804	12.235200
12.234378	757.352677	12.240218
12.170211	762.184872	12.245235
12.772105	766.966358	12.250253
12.429233	789.660063	12.255271
12.779220	774.545618	12.260288
12.857979	778.175142	12.265306
12.938155	775.975620	12.270323
12.757023	769.039111	12.275341
12.483363	761.176663	12.280359
12.892997	760.102648	12.285376
12.527990	759.007993	12.290394
12.723198	763.878445	12.295411
12.819885	773.387629	12.300429
12.743482	775.510885	12.305447
12.862478	763.730487	12.310464
12.951467	762.738270	12.315482
12.889099	752.841924	12.320499
13.030853	746.697439	12.325517
12.859820	751.025663	12.330535
12.939967	742.890037	12.335552
12.686035	747.363794	12.340570
12.844322	747.102339	12.345587
12.590906	740.271841	12.350605
12.755956	754.308383	12.355623
12.852839	742.234816	12.360640
12.682455	741.627224	12.365658
12.893093	747.315769	12.370675
12.988791	749.383654	12.375693
12.468021	760.826268	12.380711
12.949546	755.941370	12.385728
12.953853	767.863456	12.390746
12.544846	773.652252	12.395763
13.073084	772.509160	12.400781
12.569553	774.939182	12.405799
13.010437	782.636643	12.410816
12.834393	787.356985	12.415834
12.811006	777.404025	12.420851
12.783122	777.301128	12.425869
12.776622	776.806713	12.430887
13.145606	768.644755	12.435904
12.889686	771.313694	12.440922
12.875963	772.638170	12.445939
13.236445	772.704800	12.450957
12.651402	780.853340	12.455975
12.990860	768.391451	12.460992
13.279732	767.213279	12.466010
12.938777	773.016659	12.471027
13.085822	780.043784	12.476045
12.857307	790.399201	12.481063
13.297470	799.968193	12.486080
13.492375	801.165308	12.491098
13.370408	794.468830	12.496115
13.261731	780.881085	12.501133
13.020243	780.369839	12.506151
13.326894	778.305247	12.511168
13.347891	778.462938	12.516186
12.933838	781.715237	12.521203
13.455575	788.226062	12.526221
13.198648	802.325602	12.531239
13.380991	798.257593	12.536256
13.159328	787.417345	12.541274
13.430785	800.522060	12.546291
13.287178	799.436894	12.551309
13.274870	800.499216	12.556327
13.417845	805.396799	12.561344
13.351447	799.067157	12.566362
13.157615	802.335449	12.571379
13.547946	802.845531	12.576397
13.049630	804.047118	12.581415
13.297814	806.340430	12.586432
13.303154	803.568800	12.591450
13.274854	797.021748	12.596467
13.585020	800.340462	12.601485
13.291668	808.102481	12.606503
13.487303	795.000382	12.611520
13.370739	794.832484	12.616538
13.334462	804.880075	12.621555
13.252484	797.180085	12.626573
13.341008	809.960015	12.631591
13.453216	803.835919	12.636608
13.379856	811.001732	12.641626
13.603694	813.406158	12.646643
13.812863	804.483419	12.651661
13.768104	806.882590	12.656679
13.662348	811.850704	12.661696
13.359614	809.698550	12.666714
13.066384	815.289336	12.671731
13.745808	824.893439	12.676749
13.789726	836.351767	12.681767
13.610644	834.947105	12.686784
13.725822	835.083728	12.691802
13.495275	837.729766	12.696819
13.728658	833.454934	12.701837
13.407397	834.325822	12.706855
13.467930	843.802838	12.711872
13.505053	827.118420	12.716890
13.898496	835.104207	12.721907
13.666027	820.406036	12.726925
14.072831	831.845374	12.731943
13.846242	827.431171	12.736960
14.152709	831.088145	12.741978
13.697979	823.875742	12.746995
14.011611	829.680721	12.752013
13.999345	838.793596	12.757031
13.932732	834.177598	12.762048
14.031215	828.323891	12.767066
13.590500	828.822170	12.772083
13.743529	836.511107	12.777101
14.184310	837.142675	12.782119
13.856070	833.350319	12.787136
14.192955	831.602880	12.792154
13.956576	834.783169	12.797171
13.935321	836.831519	12.802189
13.971324	835.014456	12.807207
13.643439	833.080837	12.812224
13.906644	824.168557	12.817242
14.031330	829.258362	12.822259
13.583883	830.593994	12.827277
13.886802	834.497681	12.832295
13.800635	831.964449	12.837312
13.924192	827.542722	12.842330
13.766952	835.314986	12.847347
13.953678	825.692000	12.852365
14.186287	843.729103	12.857383
13.797585	839.507557	12.862400
14.295471	843.001996	12.867418
14.295155	849.187536	12.872435
14.490644	851.359720	12.877453
14.371131	836.328252	12.882471
14.041244	830.478545	12.887488
13.862461	828.903422	12.892506
14.183803	853.961006	12.897523
14.174748	844.665335	12.902541
14.293213	860.915197	12.907559
14.428301	851.622184	12.912576
14.493562	841.585870	12.917594
14.437338	847.653935	12.922611
14.198823	841.834090	12.927629
14.401137	840.202410	12.932647
14.186215	844.556469	12.937664
14.399413	846.410293	12.942682
14.308921	852.098715	12.947699
14.119191	843.951678	12.952717
14.422859	847.429212	12.957735
14.269203	845.465136	12.962752
14.780270	842.929847	12.967770
14.528895	849.561827	12.972787
14.803278	855.107873	12.977805
14.000494	832.158148	12.982823
14.488196	841.038052	12.987840
14.593671	848.380990	12.992858
14.743081	840.837233	12.997875
14.741454	842.153508	13.002893
14.252987	840.131438	13.007911
14.286826	852.702213	13.012928
14.669298	849.458071	13.017946
14.713002	846.794034	13.022963
14.544307	851.579513	13.027981
14.244842	845.239034	13.032999
14.381191	862.104640	13.038016
14.748549	847.568089	13.043034
14.411877	846.939209	13.048051
14.482194	845.839457	13.053069
14.722045	852.173563	13.058087
14.326155	847.987855	13.063104
14.532432	851.486960	13.068122
14.438035	848.718327	13.073139
14.601384	842.188568	13.078157
14.482586	856.118184	13.083175
14.258851	855.626245	13.088192
14.899276	870.039682	13.093210
14.949887	876.889448	13.098227
15.028638	867.908216	13.103245
14.972803	864.638070	13.108263
14.836233	855.895710	13.113280
15.161314	852.505923	13.118298
15.078937	859.941415	13.123315
14.732176	848.454846	13.128333
14.879449	855.030679	13.133351
14.541686	854.657594	13.138368
14.784854	849.008431	13.143386
14.533285	864.375831	13.148403
14.535135	868.156281	13.153421
15.033367	867.535444	13.158439
15.053493	879.281554	13.163456
15.226385	875.284438	13.168474
15.192338	877.019211	13.173491
14.934406	876.217045	13.178509
15.357265	874.601301	13.183527
14.992202	862.906148	13.188544
15.212063	856.146621	13.193562
14.845181	863.500457	13.198579
14.723177	866.505039	13.203597
14.512587	868.829213	13.208615
14.787523	886.752429	13.213632
15.100511	879.725834	13.218650
15.219518	876.699694	13.223667
15.223673	875.869087	13.228685
14.951704	874.889237	13.233703
14.877930	887.164468	13.238720
15.396527	879.417682	13.243738
15.243041	866.411257	13.248755
15.191143	875.811230	13.253773
15.340978	873.196834	13.258791
15.414189	872.516355	13.263808
15.370845	870.800085	13.268826
15.367022	878.649317	13.273843
15.184006	875.692590	13.278861
15.146399	872.990795	13.283879
14.987739	873.757312	13.288896
15.046193	867.490135	13.293914
15.343525	874.866141	13.298931
15.281610	869.842293	13.303949
15.495744	868.972475	13.308967
15.292368	877.411558	13.313984
15.303182	876.961766	13.319002
15.290480	894.008548	13.324019
15.489566	902.472949	13.329037
15.690183	899.957890	13.334055
15.469713	903.419725	13.339072
15.690968	894.084788	13.344090
15.635289	891.998057	13.349107
15.391755	878.879498	13.354125
15.784528	877.296870	13.359143
15.263973	873.954366	13.364160
15.398093	880.724776	13.369178
15.652312	888.075984	13.374195
15.693605	900.292169	13.379213
16.027641	897.828792	13.384231
15.497161	892.717404	13.389248
15.556535	869.629391	13.394266
15.702579	877.164803	13.399283
15.682893	884.423223	13.404301
15.487051	867.522801	13.409319
15.518157	887.699627	13.414336
15.663022	887.105753	13.419354
15.752548	891.677213	13.424371
15.365791	900.681535	13.429389
15.865856	893.404713	13.434407
15.939429	901.415400	13.439424
16.150572	898.822952	13.444442
16.087683	897.460042	13.449459
15.810469	885.564915	13.454477
15.916433	874.382942	13.459495
15.918127	869.914026	13.464512
16.129824	867.069027	13.469530
15.951544	867.478851	13.474547
15.547914	872.133886	13.479565
15.808949	864.784072	13.484583
16.050016	866.122284	13.489600
15.593645	861.327503	13.494618
15.881892	880.454161	13.499635
15.643272	896.245599	13.504653
16.269018	893.581880	13.509671
15.936844	891.014600	13.514688
16.027881	892.991712	13.519706
16.031276	891.113480	13.524723
15.763736	902.033661	13.529741
16.046326	890.527354	13.534759
16.225321	894.229561	13.539776
15.937751	898.553989	13.544794
16.044332	898.764544	13.549811
16.166872	895.949290	13.554829
16.023803	891.215867	13.559847
15.873571	896.528649	13.564864
15.959593	893.340415	13.569882
15.865834	885.014218	13.574899
16.118313	888.354610	13.579917
16.386664	889.489731	13.584935
15.731565	893.906457	13.589952
15.893012	890.542300	13.594970
16.573536	902.030317	13.599987
15.977307	905.349052	13.605005
16.362439	906.210252	13.610023
16.177774	918.105241	13.615040
16.192897	917.812565	13.620058
16.296520	916.663409	13.625075
16.289206	925.930189	13.630093
16.655771	928.182878	13.635111
16.570156	924.756438	13.640128
16.577453	924.704833	13.645146
16.312775	915.133591	13.650163
16.422585	914.665131	13.655181
16.721108	917.095739	13.660199
16.481158	912.642582	13.665216
16.351100	900.506634	13.670234
16.302442	904.282382	13.675251
16.537249	914.719913	13.680269
16.455385	919.201467	13.685287
16.781831	916.508899	13.690304
16.757161	916.399186	13.695322
16.643617	905.693407	13.700339
16.325755	906.819389	13.705357
16.983216	906.220941	13.710375
16.558403	913.214639	13.715392
16.622366	908.770671	13.720410
16.580000	916.657518	13.725427
16.349028	919.076412	13.730445
16.655018	931.399471	13.735463
16.422944	926.818842	13.740480
16.639258	923.089471	13.745498
16.979947	910.532615	13.750515
16.950766	932.498841	13.755533
16.743528	923.193155	13.760551
16.845403	930.675548	13.765568
16.903541	923.969737	13.770586
16.873565	918.420155	13.775603
16.375851	924.607913	13.780621
16.830643	922.696822	13.785639
16.649075	922.406562	13.790656
16.898857	925.365524	13.795674
16.965975	919.535637	13.800691
16.708226	927.778132	13.805709
16.891882	927.083503	13.810727
17.027462	930.723091	13.815744
16.893423	924.621756	13.820762
16.746637	925.395882	13.825779
16.897882	926.170650	13.830797
16.999655	925.081745	13.835815
17.185586	926.043586	13.840832
16.912324	921.867049	13.845850
16.822253	929.278529	13.850867
16.902646	926.005963	13.855885
17.130286	919.314622	13.860903
16.843293	924.835036	13.865920
16.813720	929.179009	13.870938
16.934083	932.003614	13.875955
16.787973	951.971590	13.880973
17.112180	948.837546	13.885991
16.836941	950.111491	13.891008
16.992010	947.092312	13.896026
17.044665	937.868976	13.901043
17.064716	946.768556	13.906061
17.126187	950.091549	13.911079
17.242594	946.062241	13.916096
17.185235	943.909494	13.921114
17.315556	938.805014	13.926131
17.269765	947.547649	13.931149
17.359445	940.682252	13.936167
17.274186	946.388820	13.941184
17.082790	950.985375	13.946202
17.517455	950.166209	13.951219
17.286310	952.073885	13.956237
17.718458	961.211866	13.961255
17.645168	948.757716	13.966272
17.255912	941.566565	13.971290
17.421369	950.730547	13.976307
17.428521	954.178819	13.981325
17.300052	961.337547	13.986343
17.868624	972.224601	13.991360
17.484575	967.030287	13.996378
17.713272	955.017977	14.001395
17.053762	954.120933	14.006413
17.263023	969.848573	14.011431
17.564206	972.313487	14.016448
17.405513	975.282809	14.021466
17.673916	965.615392	14.026483
17.562514	975.021585	14.031501
17.936187	964.990529	14.036519
17.702201	962.518309	14.041536
17.506128	970.047402	14.046554
17.988805	971.016401	14.051571
17.562314	976.224165	14.056589
17.625159	966.955036	14.061607
17.779430	962.963973	14.066624
17.675779	964.359359	14.071642
17.776969	968.506126	14.076659
17.397448	965.384508	14.081677
17.814754	965.256040	14.086695
17.874898	966.310176	14.091712
17.832443	961.317969	14.096730
17.737945	969.664295	14.101747
17.578685	969.058107	14.106765
17.673529	969.630271	14.111783
18.250978	976.463803	14.116800
17.778360	972.047085	14.121818
17.725448	975.555266	14.126835
17.736813	989.199498	14.131853
18.454783	992.157701	14.136871
18.639287	990.841230	14.141888
17.952069	986.710602	14.146906
18.144404	979.788080	14.151923
17.951851	974.497488	14.156941
17.899801	974.568793	14.161959
18.349126	982.959310	14.166976
17.693690	994.883928	14.171994
17.914972	986.571441	14.177011
18.303146	993.983757	14.182029
18.204791	990.780211	14.187047
18.040228	990.291620	14.192064
17.964722	1009.024120	14.197082
17.785805	996.580175	14.202099
17.949950	997.453912	14.207117
18.192801	996.513316	14.212135
18.153793	997.254778	14.217152
17.689364	1004.071678	14.222170
18.068867	1000.143150	14.227187
18.268242	1012.744907	14.232205
18.637567	1013.337184	14.237223
18.321356	1018.433006	14.242240
18.257656	1022.968546	14.247258
18.799471	1008.401374	14.252275
18.952600	1010.334057	14.257293
18.581050	990.409318	14.262311
18.451193	986.002010	14.267328
18.223535	989.922589	14.272346
18.482285	993.142095	14.277363
18.837418	1002.001825	14.282381
18.596757	1008.597470	14.287399
18.893470	1002.453865	14.292416
18.576591	1003.746961	14.297434
18.696486	984.395339	14.302451
18.146036	987.318743	14.307469
18.282943	991.945923	14.312487
18.602472	998.172921	14.317504
18.687369	1010.934628	14.322522
18.699268	1005.103897	14.327539
18.753734	1015.159479	14.332557
18.840821	1014.337963	14.337575
19.286523	1003.440359	14.342592
19.140038	992.477751	14.347610
18.929789	991.541873	14.352627
18.595064	986.791115	14.357645
18.454384	984.124388	14.362663
19.116055	984.967511	14.367680
18.992145	977.012076	14.372698
19.135565	984.879311	14.377715
19.077322	988.987945	14.382733
19.284986	981.160442	14.387751
19.308908	965.197502	14.392768
19.108925	987.818575	14.397786
19.156565	985.201239	14.402803
19.462008	989.426464	14.407821
18.965400	983.542866	14.412839
19.104228	982.830011	14.417856
18.956818	982.064173	14.422874
19.330465	983.006073	14.427891
19.022010	983.714011	14.432909
18.797398	986.677884	14.437927
19.530143	984.707458	14.442944
18.687102	984.015897	14.447962
19.064725	979.144062	14.452979
19.091389	978.884292	14.457997
18.944051	982.684985	14.463015
19.048602	978.824788	14.468032
18.921713	983.890937	14.473050
18.787127	976.527323	14.478067
18.894574	983.570200	14.483085
18.421412	987.302021	14.488103
18.847097	993.105277	14.493120
18.815572	1004.992109	14.498138
18.958809	1005.733421	14.503155
19.123980	1008.623602	14.508173
18.875001	1011.951066	14.513191
19.051014	1016.057718	14.518208
19.311004	1035.848548	14.523226
19.274323	1043.491556	14.528243
19.367671	1040.851271	14.533261
19.363047	1035.534371	14.538279
19.401440	1034.076685	14.543296
19.469025	1041.223662	14.548314
19.419792	1039.085410	14.553331
19.530818	1034.476243	14.558349
19.597412	1036.116367	14.563367
19.351699	1037.190026	14.568384
19.238512	1038.394404	14.573402
19.224853	1035.524726	14.578419
19.771780	1028.928489	14.583437
19.241737	1030.841979	14.588455
19.657402	1025.654895	14.593472
19.523713	1038.327791	14.598490
19.553037	1042.807734	14.603507
19.789748	1044.092993	14.608525
20.072349	1067.033039	14.613543
19.916779	1051.981793	14.618560
19.967292	1045.759981	14.623578
19.801570	1034.532112	14.628595
19.867646	1037.422045	14.633613
19.450565	1034.287364	14.638631
20.050482	1043.926134	14.643648
19.717666	1039.847266	14.648666
19.967647	1052.905037	14.653683
20.357145	1045.049016	14.658701
19.729691	1037.595338	14.663719
20.234511	1034.527658	14.668736
20.111808	1028.866335	14.673754
20.073162	1028.881890	14.678771
19.940373	1022.846600	14.683789
19.935102	1029.096095	14.688807
20.471930	1029.220305	14.693824
19.772717	1027.234388	14.698842
19.607624	1028.661497	14.703859
20.070922	1035.866396	14.708877
19.882336	1051.959408	14.713895
20.025398	1052.410408	14.718912
20.221033	1053.661076	14.723930
20.246727	1059.621702	14.728947
20.291109	1055.389053	14.733965
20.253814	1060.835672	14.738983
20.536472	1052.844905	14.744000
20.277358	1058.458824	14.749018
20.162005	1055.220059	14.754035
20.263437	1062.093492	14.759053
20.238536	1063.729018	14.764071
20.417838	1058.477971	14.769088
20.294441	1064.477737	14.774106
20.371613	1060.372497	14.779123
20.220504	1060.153202	14.784141
19.950691	1068.975179	14.789159
19.946662	1060.754765	14.794176
20.196973	1059.027181	14.799194
20.392876	1051.393999	14.804211
20.473434	1053.786192	14.809229
20.057187	1058.828269	14.814247
20.559818	1063.350827	14.819264
20.619670	1084.896182	14.824282
20.612759	1084.581709	14.829299
20.629290	1082.972805	14.834317
20.186638	1084.960972	14.839335
20.408823	1088.545996	14.844352
20.609750	1088.416715	14.849370
20.302729	1083.043036	14.854387
20.373814	1082.337636	14.859405
20.410581	1086.699657	14.864423
20.964358	1086.530871	14.869440
20.849224	1082.850242	14.874458
20.708290	1087.110714	14.879475
20.656862	1082.940409	14.884493
20.736499	1082.252604	14.889511
20.776457	1086.225950	14.894528
21.129719	1084.709458	14.899546
20.777166	1092.490343	14.904563
21.179458	1086.017735	14.909581
21.010521	1088.067161	14.914599
21.291781	1078.593335	14.919616
21.137363	1081.139115	14.924634
21.154940	1078.507540	14.929651
21.056695	1081.716723	14.934669
20.884368	1081.554403	14.939687
21.086014	1083.627819	14.944704
21.130642	1076.548517	14.949722
20.996248	1076.288732	14.954739
21.125158	1079.361336	14.959757
21.195425	1086.713044	14.964775
20.793816	1077.885867	14.969792
21.377264	1078.946383	14.974810
21.303660	1081.886611	14.979827
21.293456	1069.965305	14.984845
20.929786	1079.862370	14.989863
21.194907	1071.631339	14.994880
21.299168	1076.702324	14.999898
20.969677	1082.021156	15.004915
21.577342	1071.249617	15.009933
21.079284	1083.238001	15.014951
20.944733	1079.866536	15.019968
20.996379	1084.008468	15.024986
21.457998	1099.286418	15.030003
21.469091	1097.637338	15.035021
21.597424	1110.641626	15.040039
21.277784	1103.534178	15.045056
21.381822	1101.132056	15.050074
21.394576	1097.444011	15.055091
21.493184	1091.776396	15.060109
21.457265	1103.673450	15.065127
21.518311	1102.284793	15.070144
21.373041	1097.236071	15.075162
21.493799	1098.422734	15.080179
21.584189	1094.848760	15.085197
21.753665	1099.407747	15.090215
21.722626	1098.336485	15.095232
21.741796	1091.661964	15.100250
21.514166	1099.369629	15.105267
21.860794	1101.278316	15.110285
21.730878	1099.124295	15.115303
21.459671	1090.182003	15.120320
21.745271	1094.716483	15.125338
21.827085	1096.953847	15.130355
21.989886	1100.308330	15.135373
21.805217	1099.144370	15.140391
21.644208	1101.173620	15.145408
21.768621	1104.682446	15.150426
21.476956	1093.420622	15.155443
21.989058	1096.344825	15.160461
21.774926	1096.747647	15.165479
21.810732	1101.961912	15.170496
22.067466	1111.364147	15.175514
21.994243	1127.240330	15.180531
22.281268	1118.437785	15.185549
22.138023	1111.694027	15.190567
21.823666	1104.721454	15.195584
22.082412	1108.815164	15.200602
21.771035	1122.636301	15.205619
21.774036	1125.611872	15.210637
22.005578	1129.750876	15.215655
22.190850	1130.542413	15.220672
22.038636	1130.604165	15.225690
22.086746	1126.194186	15.230707
22.424522	1125.475402	15.235725
22.153748	1126.581396	15.240743
21.913338	1120.679703	15.245760
22.218402	1117.109961	15.250778
22.077188	1118.287176	15.255795
22.395736	1114.074676	15.260813
22.408282	1124.288371	15.265831
22.155194	1116.132201	15.270848
22.149938	1135.409263	15.275866
22.190515	1141.354960	15.280883
22.519979	1140.353447	15.285901
22.586357	1140.500874	15.290919
22.507303	1143.852233	15.295936
22.994214	1142.371602	15.300954
22.624558	1143.259553	15.305971
22.565961	1134.590050	15.310989
22.511022	1141.936151	15.316007
22.414542	1143.753318	15.321024
22.682702	1144.430880	15.326042
22.868051	1147.210622	15.331059
22.682706	1152.749894	15.336077
22.569996	1145.291262	15.341095
22.527663	1148.185574	15.346112
22.759525	1137.987288	15.351130
22.565195	1143.729942	15.356147
22.839269	1134.935730	15.361165
22.589996	1136.271892	15.366183
22.906042	1137.920279	15.371200
22.878054	1136.952681	15.376218
23.035096	1138.985753	15.381235
22.863576	1135.493835	15.386253
22.764585	1134.843483	15.391271
22.935892	1139.165501	15.396288
23.114225	1129.865569	15.401306
23.036740	1144.205514	15.406323
23.131893	1138.598387	15.411341
23.108822	1142.565842	15.416359
23.015040	1146.478103	15.421376
22.918782	1136.293356	15.426394
23.014859	1143.820930	15.431411
22.821930	1144.409785	15.436429
22.909981	1144.446516	15.441447
22.818662	1153.063837	15.446464
23.411012	1163.088878	15.451482
23.210232	1166.320453	15.456499
23.291756	1165.285200	15.461517
23.245415	1164.210019	15.466535
23.149743	1169.975096	15.471552
23.741167	1165.372680	15.476570
23.373118	1169.463621	15.481587
23.432523	1162.369347	15.486605
23.161923	1149.639849	15.491623
23.453601	1166.850646	15.496640
23.466073	1164.797388	15.501658
23.316674	1171.429288	15.506675
23.354578	1169.450943	15.511693
23.210715	1164.581867	15.516711
22.736446	1163.229741	15.521728
23.395722	1161.400200	15.526746
23.266812	1169.004063	15.531763
23.251039	1162.227690	15.536781
23.390430	1161.678847	15.541799
23.500644	1175.822146	15.546816
23.629592	1183.530785	15.551834
23.751005	1192.398825	15.556851
23.838275	1188.219388	15.561869
23.977755	1187.919847	15.566887
23.855645	1187.487718	15.571904
23.900997	1164.837035	15.576922
23.940145	1162.511347	15.581939
23.637431	1163.281510	15.586957
24.007610	1161.973806	15.591975
23.953441	1166.066063	15.596992
23.780815	1157.723692	15.602010
23.954203	1161.095464	15.607027
24.087582	1166.578491	15.612045
24.301003	1151.529309	15.617063
24.107909	1157.366452	15.622080
24.072451	1148.652289	15.627098
23.859126	1147.221408	15.632115
23.763120	1153.440981	15.637133
23.947233	1150.133188	15.642151
23.968227	1169.990015	15.647168
24.183883	1177.009703	15.652186
24.378369	1180.138324	15.657203
23.846538	1175.115431	15.662221
24.198966	1178.061510	15.667239
24.056630	1186.617410	15.672256
24.147492	1186.811497	15.677274
24.118926	1187.428251	15.682291
23.869336	1179.549223	15.687309
24.368331	1187.297718	15.692327
24.365608	1186.739582	15.697344
24.478698	1179.292896	15.702362
23.994537	1184.661239	15.707379
24.449104	1187.733332	15.712397
24.226447	1181.636327	15.717415
24.497720	1192.573252	15.722432
24.506390	1182.927478	15.727450
24.570748	1186.474133	15.732467
24.513984	1186.552489	15.737485
24.506501	1181.176032	15.742503
24.623895	1184.597608	15.747520
24.435864	1179.666019	15.752538
24.531208	1184.167213	15.757555
24.542969	1190.385693	15.762573
24.543466	1178.251192	15.767591
24.473175	1194.467813	15.772608
24.807448	1200.335954	15.777626
24.645438	1204.148461	15.782643
24.873297	1211.377696	15.787661
24.969360	1203.097351	15.792679
24.761099	1207.803915	15.797696
24.886640	1198.786783	15.802714
24.833089	1193.509061	15.807731
24.216806	1201.568008	15.812749
25.029156	1197.104544	15.817767
25.206177	1198.992477	15.822784
24.957461	1195.998652	15.827802
24.724164	1198.768253	15.832819
24.883048	1209.104240	15.837837
24.997165	1201.101943	15.842855
24.540948	1196.811991	15.847872
24.784367	1198.392866	15.852890
24.846838	1204.215229	15.857907
24.720831	1209.006739	15.862925
25.085474	1207.431647	15.867943
25.015735	1215.480709	15.872960
25.442544	1222.489423	15.877978
25.345936	1224.988295	15.882995
25.143811	1212.071293	15.888013
25.041111	1212.201029	15.893031
24.931858	1225.649738	15.898048
25.130489	1231.191991	15.903066
25.291889	1227.294431	15.908083
25.235369	1230.736952	15.913101
25.024528	1226.263376	15.918119
24.600417	1228.179223	15.923136
25.239970	1231.563179	15.928154
25.434494	1236.973529	15.933171
25.338252	1259.073744	15.938189
25.709881	1254.442625	15.943207
25.652010	1254.808344	15.948224
25.726901	1257.838947	15.953242
25.737433	1255.170579	15.958259
25.807386	1247.528644	15.963277
25.854491	1242.345595	15.968295
25.758992	1232.138583	15.973312
25.391417	1233.133513	15.978330
25.867800	1227.040580	15.983347
25.666772	1229.050867	15.988365
25.599058	1229.411816	15.993383
25.620963	1244.878709	15.998400
26.360216	1250.064856	16.003418
26.300007	1228.137558	16.008435
26.249713	1221.694785	16.013453
26.554930	1220.615014	16.018471
26.449419	1226.791918	16.023488
26.198509	1218.764752	16.028506
26.382907	1214.248188	16.033523
25.674326	1218.329377	16.038541
26.006276	1205.732657	16.043559
26.102379	1215.993275	16.048576
26.230926	1213.808213	16.053594
26.394987	1212.936756	16.058611
26.222271	1213.759139	16.063629
25.995683	1207.173575	16.068647
26.431036	1211.438461	16.073664
26.224370	1212.739550	16.078682
26.205747	1206.525358	16.083699
26.095866	1212.239024	16.088717
26.557122	1206.650257	16.093735
26.272763	1211.797949	16.098752
26.477115	1213.820461	16.103770
26.552965	1204.230424	16.108787
26.410954	1202.930381	16.113805
26.498958	1194.073772	16.118823
26.322092	1195.490115	16.123840
26.127561	1204.840023	16.128858
26.457073	1215.098785	16.133875
26.078347	1214.848877	16.138893
26.404141	1213.279872	16.143911
26.223011	1206.743992	16.148928
26.370359	1199.702197	16.153946
26.335852	1210.702823	16.158963
26.087116	1215.450446	16.163981
26.484306	1214.495124	16.168999
26.714269	1223.298834	16.174016
26.702781	1234.920739	16.179034
26.694130	1235.944643	16.184051
26.817896	1238.825570	16.189069
26.999332	1237.667358	16.194087
26.925515	1240.601333	16.199104
26.735513	1232.971731	16.204122
26.712753	1232.034867	16.209139
26.656329	1239.138236	16.214157
26.454505	1243.809086	16.219175
27.027210	1241.563897	16.224192
26.726872	1249.986788	16.229210
27.119253	1243.026510	16.234227
26.702813	1244.571914	16.239245
26.861140	1242.543134	16.244263
26.786579	1240.544531	16.249280
27.105714	1240.952169	16.254298
26.935174	1238.062857	16.259315
26.627066	1234.841636	16.264333
27.108381	1246.929154	16.269351
26.909988	1260.363452	16.274368
27.062838	1259.869304	16.279386
27.407889	1254.036789	16.284403
26.989515	1259.877702	16.289421
27.192328	1256.418631	16.294439
27.192787	1264.908013	16.299456
27.175833	1258.993354	16.304474
27.433821	1255.415181	16.309491
27.210427	1269.620291	16.314509
27.230680	1259.496117	16.319527
27.363754	1266.449881	16.324544
27.359258	1275.432368	16.329562
27.668154	1277.056642	16.334579
27.716558	1287.684549	16.339597
28.010554	1276.302445	16.344615
27.576149	1264.759909	16.349632
27.590878	1254.554550	16.354650
27.644824	1246.608999	16.359667
27.447774	1262.277477	16.364685
27.802397	1272.617548	16.369703
27.831989	1285.126174	16.374720
27.743541	1280.292568	16.379738
28.299366	1282.490402	16.384755
27.889157	1274.567068	16.389773
27.877704	1264.927558	16.394791
27.560711	1261.710881	16.399808
27.668235	1272.247463	16.404826
27.412066	1275.377278	16.409843
27.589221	1282.996354	16.414861
27.913969	1272.180656	16.419879
27.910496	1276.760474	16.424896
27.819195	1281.486604	16.429914
28.106504	1279.412363	16.434931
27.925539	1283.029033	16.439949
28.070270	1280.797243	16.444967
28.414536	1276.965698	16.449984
28.193588	1281.140919	16.455002
28.548023	1284.796784	16.460019
27.984618	1282.325637	16.465037
28.485755	1283.455870	16.470055
28.471796	1284.821448	16.475072
28.291315	1285.758665	16.480090
28.678121	1274.545064	16.485107
28.604197	1288.392243	16.490125
28.383135	1279.738656	16.495143
28.425906	1277.661702	16.500160
27.987123	1285.146901	16.505178
28.408800	1285.311248	16.510195
28.027738	1279.024425	16.515213
28.115799	1287.607394	16.520231
28.270971	1295.100525	16.525248
27.951643	1310.248540	16.530266
28.272669	1306.022983	16.535283
28.328826	1306.282471	16.540301
28.543743	1300.236792	16.545319
28.797104	1307.626178	16.550336
28.566480	1312.317338	16.555354
28.773180	1316.068943	16.560371
28.655449	1325.066040	16.565389
28.912277	1325.309867	16.570407
29.112415	1334.481237	16.575424
29.044958	1327.476204	16.580442
28.868596	1310.969957	16.585459
29.026579	1303.210060	16.590477
29.264445	1304.990637	16.595495
28.757910	1315.273147	16.600512
28.934136	1315.333935	16.605530
29.216448	1317.476793	16.610547
29.076705	1311.208956	16.615565
29.230246	1313.832756	16.620583
29.014140	1304.253693	16.625600
29.044340	1323.039390	16.630618
29.427417	1329.559517	16.635635
29.205220	1327.025436	16.640653
28.889638	1329.757454	16.645671
29.175215	1331.577898	16.650688
29.419432	1329.005455	16.655706
29.576480	1325.256883	16.660723
29.662375	1328.756009	16.665741
29.745837	1332.839363	16.670759
29.708434	1319.877539	16.675776
29.500060	1307.463239	16.680794
29.118071	1306.450106	16.685811
29.089782	1301.158927	16.690829
29.434440	1316.666836	16.695847
29.532246	1313.252610	16.700864
29.053780	1328.397170	16.705882
29.553508	1318.652293	16.710899
29.496457	1320.371778	16.715917
29.495089	1332.730648	16.720935
29.979184	1326.642785	16.725952
29.534284	1328.804906	16.730970
29.775651	1325.510202	16.735987
29.970385	1329.011210	16.741005
29.553166	1326.539244	16.746023
29.745298	1322.614756	16.751040
29.659914	1324.707924	16.756058
29.737741	1337.063857	16.761075
29.704770	1346.060308	16.766093
30.020288	1348.362077	16.771111
30.211073	1345.633894	16.776128
30.147064	1353.776798	16.781146
30.221620	1350.202099	16.786163
30.275361	1346.305601	16.791181
30.100789	1356.611865	16.796199
30.571670	1350.841657	16.801216
30.009737	1344.557902	16.806234
30.005267	1336.151231	16.811251
29.995630	1342.142733	16.816269
30.261869	1343.259279	16.821287
30.293678	1335.923097	16.826304
30.077346	1347.343630	16.831322
30.015957	1345.538619	16.836339
30.102325	1351.729687	16.841357
30.298256	1341.707334	16.846375
30.337758	1341.032120	16.851392
30.204600	1338.929073	16.856410
30.291878	1340.304042	16.861427
30.158137	1343.433623	16.866445
30.331133	1356.592045	16.871463
30.779886	1361.261983	16.876480
30.774200	1369.626140	16.881498
30.593749	1367.931304	16.886515
30.709461	1369.800457	16.891533
30.687056	1366.654375	16.896551
30.636449	1360.836477	16.901568
30.897145	1366.832971	16.906586
30.636085	1363.683254	16.911603
30.558252	1361.805076	16.916621
30.691812	1367.149275	16.921639
30.986756	1360.942708	16.926656
30.824200	1371.830946	16.931674
30.708899	1369.971260	16.936691
30.803554	1357.234881	16.941709
30.665021	1362.242998	16.946727
30.666151	1362.113461	16.951744
30.871334	1373.183934	16.956762
31.169228	1372.209447	16.961779
31.432866	1375.320956	16.966797
31.106226	1386.032931	16.971815
31.677807	1380.070204	16.976832
31.393974	1372.590948	16.981850
31.617013	1360.367806	16.986867
31.505223	1359.192409	16.991885
31.416589	1364.786025	16.996903
31.357498	1352.392488	17.001920
31.211232	1362.804778	17.006938
31.160637	1357.176236	17.011955
31.372824	1352.529046	17.016973
31.230023	1384.694678	17.021991
31.422911	1383.114922	17.027008
31.270369	1380.822395	17.032026
31.453390	1389.772404	17.037043
31.852225	1391.754997	17.042061
31.584916	1385.904769	17.047079
31.824284	1383.831716	17.052096
31.890837	1386.204057	17.057114
31.770466	1389.132727	17.062131
31.728282	1376.957439	17.067149
31.617041	1390.094145	17.072167
31.715605	1389.873599	17.077184
31.628440	1391.888155	17.082202
31.772484	1392.320075	17.087219
31.763324	1389.866220	17.092237
31.774874	1393.298108	17.097255
31.872546	1380.094161	17.102272
31.688305	1389.186921	17.107290
31.727365	1393.889499	17.112307
32.420817	1401.039551	17.117325
31.834449	1410.867543	17.122343
32.239512	1410.027749	17.127360
32.496347	1409.839211	17.132378
32.164831	1401.190247	17.137395
32.290208	1400.428989	17.142413
32.306977	1404.336609	17.147431
32.429486	1405.245295	17.152448
32.218302	1413.641669	17.157466
32.213055	1416.419757	17.162483
32.491671	1418.045632	17.167501
32.128207	1404.585698	17.172519
32.375988	1413.298344	17.177536
32.203777	1415.881674	17.182554
32.262669	1413.243577	17.187571
32.545997	1403.945988	17.192589
31.976326	1416.551754	17.197607
32.328117	1396.399615	17.202624
32.472129	1408.240276	17.207642
32.097122	1408.447394	17.212659
32.738377	1420.036579	17.217677
32.605873	1441.451548	17.222695
32.932425	1428.543079	17.227712
32.711928	1430.521723	17.232730
32.932931	1432.860403	17.237747
33.137315	1427.769427	17.242765
32.759502	1434.658128	17.247783
32.835154	1437.025894	17.252800
33.022482	1438.650294	17.257818
33.164701	1436.526181	17.262835
33.433588	1430.642423	17.267853
33.261620	1430.811417	17.272871
33.119257	1420.999822	17.277888
32.982962	1413.396443	17.282906
32.890273	1429.881886	17.287923
32.807740	1426.697874	17.292941
32.668965	1425.551949	17.297959
33.061217	1429.148268	17.302976
32.997937	1431.979633	17.307994
33.234565	1430.894816	17.313011
33.458141	1434.296648	17.318029
33.326968	1430.359673	17.323047
33.193189	1428.638582	17.328064
33.259890	1440.349360	17.333082
33.486024	1455.329980	17.338099
33.644805	1456.898892	17.343117
33.429829	1459.176490	17.348135
33.644241	1457.148366	17.353152
33.951784	1456.576325	17.358170
33.644100	1456.337373	17.363187
33.835820	1456.455697	17.368205
33.719853	1453.999632	17.373223
33.717023	1459.434660	17.378240
33.751137	1457.122346	17.383258
33.894067	1453.577941	17.388275
33.898750	1447.410509	17.393293
33.734862	1448.543959	17.398311
33.784143	1455.495145	17.403328
33.981108	1454.968833	17.408346
33.742836	1457.177494	17.413363
34.171799	1449.643333	17.418381
33.880343	1459.330467	17.423399
33.985467	1457.767612	17.428416
34.064268	1445.062057	17.433434
33.837379	1451.901871	17.438451
34.130369	1458.818031	17.443469
33.796398	1452.719437	17.448487
33.600178	1449.165051	17.453504
34.016992	1456.509955	17.458522
34.294815	1474.281823	17.463539
34.699788	1467.641394	17.468557
34.731789	1476.403658	17.473575
34.544821	1469.325771	17.478592
34.659877	1477.008310	17.483610
34.468875	1472.007675	17.488627
34.463771	1472.358818	17.493645
34.408998	1470.161419	17.498663
34.675594	1476.141247	17.503680
34.544577	1469.108245	17.508698
34.355151	1469.302066	17.513715
34.723354	1465.564566	17.518733
34.396408	1464.249295	17.523751
34.472561	1464.975890	17.528768
34.595557	1463.627995	17.533786
34.407352	1466.302205	17.538803
34.659536	1467.714466	17.543821
34.651784	1465.014215	17.548839
34.769787	1472.153466	17.553856
34.818864	1480.799443	17.558874
34.730907	1493.383440	17.563891
35.082212	1485.343854	17.568909
34.948620	1487.741255	17.573927
34.783994	1496.127217	17.578944
35.227605	1490.339147	17.583962
34.981055	1491.119459	17.588979
34.909533	1500.374505	17.593997
34.913709	1498.218362	17.599015
35.460065	1501.629597	17.604032
35.147732	1496.559597	17.609050
35.420270	1494.724344	17.614067
35.458891	1489.391066	17.619085
35.493538	1482.158525	17.624103
35.333058	1486.532612	17.629120
35.817958	1491.708187	17.634138
35.469604	1492.965220	17.639155
35.341015	1488.137847	17.644173
35.483984	1489.226377	17.649191
35.307761	1488.698571	17.654208
35.615555	1500.472605	17.659226
35.689968	1512.598808	17.664243
35.712610	1516.963147	17.669261
35.850108	1525.996099	17.674279
36.012313	1523.931964	17.679296
36.051620	1521.079158	17.684314
35.900371	1512.341933	17.689331
35.841955	1508.440880	17.694349
35.865129	1518.160805	17.699367
35.744627	1516.425002	17.704384
36.131396	1511.093977	17.709402
36.004201	1516.321278	17.714419
36.066147	1505.221552	17.719437
36.245278	1510.830067	17.724455
35.758645	1509.738639	17.729472
36.162200	1514.715516	17.734490
35.941205	1514.257844	17.739507
36.063891	1507.538545	17.744525
36.093554	1505.993821	17.749543
36.089613	1508.086874	17.754560
36.097267	1506.252093	17.759578
35.848356	1530.803498	17.764595
36.210607	1538.977536	17.769613
36.087906	1535.430550	17.774631
35.978861	1542.031016	17.779648
36.338926	1537.452133	17.784666
36.424895	1541.449931	17.789683
36.394136	1542.597244	17.794701
36.502467	1551.530632	17.799719
36.266510	1571.791100	17.804736
36.850940	1570.768553	17.809754
36.546137	1578.460111	17.814771
36.713912	1569.107954	17.819789
36.884338	1561.734181	17.824807
36.952419	1574.110740	17.829824
37.063692	1567.528914	17.834842
36.797708	1565.863240	17.839859
36.730965	1556.995981	17.844877
37.009552	1563.614621	17.849895
37.103100	1566.370941	17.854912
36.872751	1564.712307	17.859930
37.011937	1562.879004	17.864947
36.994860	1558.280306	17.869965
37.298972	1563.509476	17.874983
37.223193	1559.229260	17.880000
37.403291	1566.330415	17.885018
36.979738	1560.012278	17.890035
36.985615	1563.445088	17.895053
37.173560	1566.410691	17.900071
36.939101	1580.892351	17.905088
37.672214	1582.604830	17.910106
37.581844	1585.244793	17.915123
37.664344	1590.189939	17.920141
37.591549	1584.650015	17.925159
37.475896	1592.905266	17.930176
37.829940	1590.527029	17.935194
37.677730	1589.916558	17.940211
37.676062	1584.892538	17.945229
37.824087	1578.655263	17.950247
37.568059	1590.681806	17.955264
37.897208	1586.079350	17.960282
37.486082	1586.371028	17.965299
37.751560	1587.102680	17.970317
37.955587	1585.732612	17.975335
37.824471	1588.738741	17.980352
37.881862	1587.606255	17.985370
37.928433	1591.632329	17.990387
37.303691	1590.414203	17.995405
37.755618	1600.969605	18.000423
37.773950	1607.960415	18.005440
37.748411	1610.438738	18.010458
37.779157	1604.374472	18.015475
37.985437	1612.412026	18.020493
37.913507	1619.268652	18.025511
37.771073	1637.848184	18.030528
38.250190	1640.474673	18.035546
38.288724	1645.161619	18.040563
38.287668	1634.633450	18.045581
38.656020	1637.678103	18.050599
38.736812	1634.695695	18.055616
38.759818	1633.836852	18.060634
38.389892	1638.414214	18.065651
38.563129	1635.695049	18.070669
38.778104	1633.193420	18.075687
38.745247	1637.036278	18.080704
38.730476	1633.601758	18.085722
38.688886	1637.786830	18.090739
38.700098	1638.040741	18.095757
38.571990	1634.175828	18.100775
38.798295	1641.976715	18.105792
39.194464	1649.110326	18.110810
39.180236	1661.929056	18.115827
39.034243	1652.733320	18.120845
39.261442	1633.919638	18.125863
38.863480	1640.625371	18.130880
39.450439	1645.049657	18.135898
39.419700	1639.304299	18.140915
39.452588	1641.587269	18.145933
39.388385	1627.209227	18.150951
39.224026	1633.982505	18.155968
39.583393	1628.671519	18.160986
39.493426	1628.363737	18.166003
39.292420	1624.308265	18.171021
39.517947	1621.467294	18.176039
39.152372	1629.970015	18.181056
39.279924	1628.933836	18.186074
39.223704	1646.966509	18.191091
39.276420	1649.618779	18.196109
39.533509	1643.588469	18.201127
39.488293	1660.161364	18.206144
39.631020	1654.676019	18.211162
39.706052	1652.511912	18.216179
39.393506	1652.990128	18.221197
39.693757	1654.177109	18.226215
39.752930	1655.689057	18.231232
39.703049	1657.618902	18.236250
40.072891	1667.533915	18.241267
39.544507	1675.222672	18.246285
40.167644	1678.359965	18.251303
40.463742	1676.722986	18.256320
40.185994	1671.391882	18.261338
40.293515	1666.966150	18.266355
40.045712	1667.885529	18.271373
40.423115	1669.530666	18.276391
40.103487	1669.186278	18.281408
40.404208	1666.866881	18.286426
40.419093	1670.263584	18.291443
40.068689	1673.465040	18.296461
40.494181	1670.545392	18.301479
40.280346	1668.814729	18.306496
40.537990	1670.238774	18.311514
40.640838	1671.949020	18.316531
40.185333	1671.297698	18.321549
40.714225	1674.134157	18.326567
40.275322	1666.180427	18.331584
40.187283	1666.509853	18.336602
40.336208	1671.532981	18.341619
40.623509	1689.846410	18.346637
41.022527	1694.928196	18.351655
40.631629	1701.411925	18.356672
41.177634	1695.497287	18.361690
40.956999	1693.666695	18.366707
40.656142	1696.020898	18.371725
40.950872	1702.472949	18.376743
40.992885	1704.700844	18.381760
40.870031	1689.037984	18.386778
41.188686	1688.953374	18.391795
40.869338	1695.324899	18.396813
41.276592	1689.501434	18.401831
41.113460	1697.884100	18.406848
41.085113	1693.561705	18.411866
41.396379	1702.690605	18.416883
41.222276	1714.180499	18.421901
41.537696	1716.501267	18.426919
42.050437	1707.978669	18.431936
41.866537	1701.600841	18.436954
41.733756	1695.088767	18.441971
41.485995	1694.209223	18.446989
41.665353	1686.531024	18.452007
41.761475	1692.919509	18.457024
41.729691	1694.827587	18.462042
41.951236	1687.969648	18.467059
41.804424	1696.463373	18.472077
41.938928	1685.165963	18.477095
42.020348	1691.203280	18.482112
42.064869	1694.194532	18.487130
41.927517	1682.696706	18.492147
41.884796	1691.710639	18.497165
41.923638	1700.064818	18.502183
41.905749	1701.797139	18.507200
42.516490	1708.549996	18.512218
42.602717	1705.402613	18.517235
41.974921	1701.271972	18.522253
42.301059	1705.276362	18.527271
41.922626	1712.512425	18.532288
42.096629	1708.909450	18.537306
42.464346	1702.107504	18.542323
42.201893	1711.130625	18.547341
42.574967	1708.812511	18.552359
42.764757	1705.743582	18.557376
42.446237	1700.179002	18.562394
42.428142	1700.611085	18.567411
42.500392	1701.871665	18.572429
42.332376	1696.261413	18.577447
42.445080	1708.230262	18.582464
42.580753	1705.939876	18.587482
42.844546	1692.719139	18.592499
42.519914	1702.373729	18.597517
42.697310	1719.599809	18.602535
42.809198	1730.846077	18.607552
42.819061	1725.450959	18.612570
43.188700	1725.295241	18.617587
43.143423	1734.925016	18.622605
43.024388	1725.964875	18.627623
43.230894	1727.567361	18.632640
42.884251	1730.297994	18.637658
43.461963	1728.197139	18.642675
43.185828	1730.118257	18.647693
43.400531	1732.451651	18.652711
43.448610	1724.260641	18.657728
43.030758	1715.501966	18.662746
43.454812	1716.328707	18.667763
43.148911	1726.624199	18.672781
43.354485	1718.531599	18.677799
43.605214	1726.088840	18.682816
43.113752	1728.839006	18.687834
43.514063	1738.193829	18.692851
43.404031	1755.963626	18.697869
43.678150	1755.055965	18.702887
43.540114	1748.992847	18.707904
43.802760	1755.191151	18.712922
43.889901	1751.930001	18.717939
43.414084	1756.353559	18.722957
43.874377	1754.700315	18.727975
44.042945	1738.423671	18.732992
44.110848	1755.872081	18.738010
44.229315	1737.479296	18.743027
44.020271	1753.986423	18.748045
44.118479	1757.486859	18.753063
43.742664	1759.909622	18.758080
44.072981	1770.758752	18.763098
44.267080	1765.284260	18.768115
44.236466	1779.623681	18.773133
44.569283	1767.708131	18.778151
44.542852	1770.470656	18.783168
44.338839	1769.849359	18.788186
44.311109	1769.001614	18.793203
44.327828	1766.590993	18.798221
44.329422	1770.242277	18.803239
44.669373	1777.454180	18.808256
44.151201	1777.535399	18.813274
44.351967	1789.765078	18.818291
44.549616	1797.526339	18.823309
44.766595	1791.458079	18.828327
44.500186	1790.833934	18.833344
44.710959	1799.533631	18.838362
45.166828	1792.392770	18.843379
44.308746	1805.075554	18.848397
44.755870	1807.931158	18.853415
45.072103	1811.634147	18.858432
45.057533	1821.710467	18.863450
45.955565	1811.738807	18.868467
45.834331	1809.526531	18.873485
45.576945	1795.349047	18.878503
45.540542	1783.806936	18.883520
45.635364	1787.017555	18.888538
45.671808	1777.266117	18.893555
45.571855	1777.016705	18.898573
45.449804	1772.585888	18.903591
45.778657	1775.453705	18.908608
45.724261	1779.773370	18.913626
45.732041	1767.413252	18.918643
45.578704	1785.312947	18.923661
45.776588	1779.762113	18.928679
45.814894	1779.771924	18.933696
45.622193	1788.206606	18.938714
45.836961	1782.495325	18.943731
46.008809	1780.211886	18.948749
45.903107	1776.690593	18.953767
45.541472	1770.223815	18.958784
45.768670	1784.390294	18.963802
45.992949	1790.054944	18.968819
45.946560	1791.633939	18.973837
45.900210	1806.190456	18.978855
46.218503	1801.709575	18.983872
46.391674	1798.065684	18.988890
46.628729	1789.952339	18.993907
46.310881	1803.367887	18.998925
46.246484	1804.570983	19.003943
46.424692	1804.552562	19.008960
46.168528	1794.351466	19.013978
46.116517	1798.825406	19.018995
46.079741	1806.222586	19.024013
46.046834	1813.372993	19.029031
46.691250	1824.725247	19.034048
46.841206	1829.410564	19.039066
46.765173	1828.412583	19.044083
46.574766	1831.614248	19.049101
46.648351	1832.991400	19.054119
47.271684	1827.433858	19.059136
46.913887	1826.558923	19.064154
46.914987	1824.775633	19.069171
47.143724	1819.598676	19.074189
47.115784	1818.741493	19.079207
47.123222	1814.558638	19.084224
46.827680	1824.672671	19.089242
47.156907	1813.953783	19.094259
47.362436	1816.234974	19.099277
47.058117	1828.919381	19.104295
47.677103	1832.486571	19.109312
47.268965	1843.669210	19.114330
47.508012	1850.410924	19.119347
47.551473	1843.751253	19.124365
47.550420	1853.339447	19.129383
47.494586	1843.624523	19.134400
47.562794	1844.623796	19.139418
47.635737	1844.931158	19.144435
47.840650	1840.739450	19.149453
47.682698	1853.520871	19.154471
47.926045	1845.242402	19.159488
47.827190	1843.651508	19.164506
47.923774	1846.123353	19.169523
47.879883	1837.567978	19.174541
47.806863	1848.309923	19.179559
47.801246	1841.979856	19.184576
47.940834	1851.347184	19.189594
47.881290	1859.754724	19.194611
48.042593	1862.939161	19.199629
48.195234	1866.964459	19.204647
48.364027	1866.300529	19.209664
47.876045	1874.055628	19.214682
48.423717	1865.060392	19.219699
48.406597	1859.903007	19.224717
48.122180	1861.677102	19.229735
48.402319	1869.292917	19.234752
48.579072	1864.269268	19.239770
48.523919	1858.114226	19.244787
48.617083	1869.354047	19.249805
48.424040	1888.528789	19.254823
48.928665	1884.286956	19.259840
48.704424	1890.078719	19.264858
48.821410	1886.853897	19.269875
48.954115	1888.155514	19.274893
49.040603	1880.851570	19.279911
48.999055	1882.808538	19.284928
49.007048	1889.286645	19.289946
49.271912	1888.067981	19.294963
49.384563	1883.240576	19.299981
49.569729	1889.861351	19.304999
49.704423	1880.548931	19.310016
49.234526	1888.089750	19.315034
49.520934	1876.320264	19.320051
49.224967	1878.714752	19.325069
49.027274	1882.141645	19.330087
49.306653	1874.583404	19.335104
49.438164	1886.192795	19.340122
49.243509	1874.766944	19.345139
49.481875	1878.595764	19.350157
48.951315	1897.220594	19.355175
49.638371	1902.730717	19.360192
49.572931	1907.516079	19.365210
49.577296	1904.340459	19.370227
49.603088	1901.552831	19.375245
49.574492	1911.211647	19.380263
49.825069	1922.300597	19.385280
49.711956	1927.816166	19.390298
49.566803	1928.056707	19.395315
50.074584	1917.723224	19.400333
50.157694	1931.306436	19.405351
50.733116	1917.771602	19.410368
50.351463	1929.275215	19.415386
50.398277	1919.335870	19.420403
50.745019	1923.902011	19.425421
50.366532	1933.353708	19.430439
50.601308	1924.028742	19.435456
50.514185	1918.664541	19.440474
50.469763	1920.587247	19.445491
50.846605	1911.192688	19.450509
50.306434	1915.853602	19.455527
50.597936	1926.222878	19.460544
50.827396	1945.296768	19.465562
50.722622	1951.044584	19.470579
51.292919	1951.618033	19.475597
50.549074	1954.761252	19.480615
51.314828	1941.385942	19.485632
51.243897	1943.025604	19.490650
51.021039	1947.971350	19.495667
50.902889	1941.939767	19.500685
50.931326	1948.203238	19.505703
50.967651	1946.398637	19.510720
50.806424	1937.470249	19.515738
51.011163	1953.754927	19.520755
51.370693	1971.280941	19.525773
51.409148	1972.278571	19.530791
51.471731	1967.834557	19.535808
51.336538	1966.991015	19.540826
51.593989	1970.327678	19.545843
51.869537	1964.231248	19.550861
51.666056	1969.167652	19.555879
51.843579	1966.034325	19.560896
51.948406	1977.499621	19.565914
51.984913	1962.486947	19.570931
51.815000	1968.358592	19.575949
51.672042	1972.127247	19.580967
52.047539	1978.484686	19.585984
51.677447	1975.209921	19.591002
51.530882	1979.553542	19.596019
51.917521	1986.534136	19.601037
51.875706	1999.938142	19.606055
52.320280	1997.012297	19.611072
52.553474	1989.357094	19.616090
52.275855	1992.935396	19.621107
52.591877	1999.011805	19.626125
52.234849	1990.155096	19.631143
52.578283	1995.352984	19.636160
52.920008	1991.979314	19.641178
52.973572	1989.092640	19.646195
52.835373	1990.616603	19.651213
53.017843	1982.729492	19.656231
52.951246	1985.974906	19.661248
53.127877	1982.914304	19.666266
53.301476	1990.414309	19.671283
53.202951	1986.017625	19.676301
53.173626	1986.858604	19.681319
53.172819	1980.969582	19.686336
53.593918	1993.101758	19.691354
53.034003	1989.496941	19.696371
53.139753	1972.144247	19.701389
53.090461	1987.446198	19.706407
52.772102	1983.879281	19.711424
53.133877	1979.154841	19.716442
53.287081	1975.854895	19.721459
53.205637	1979.894802	19.726477
53.091129	2000.184066	19.731495
53.690563	1996.227178	19.736512
53.904850	2008.407548	19.741530
53.707043	2010.767737	19.746547
53.630109	2010.925002	19.751565
53.507903	2015.570953	19.756583
53.275837	2010.456669	19.761600
53.702392	2011.036861	19.766618
53.566288	2016.290951	19.771635
53.705419	2025.510107	19.776653
53.770198	2031.875220	19.781671
53.876394	2034.396082	19.786688
54.029801	2032.402701	19.791706
53.449143	2048.876796	19.796723
53.909108	2046.642864	19.801741
53.732890	2056.773047	19.806759
53.979381	2064.911811	19.811776
54.291162	2062.350771	19.816794
54.173870	2065.730384	19.821811
54.455205	2079.105912	19.826829
54.312141	2087.791754	19.831847
54.642346	2091.625167	19.836864
54.800329	2085.190481	19.841882
55.023878	2081.418710	19.846899
54.858687	2083.193083	19.851917
54.800804	2085.278874	19.856935
54.942991	2088.387445	19.861952
55.130950	2083.655494	19.866970
54.942152	2082.766692	19.871987
54.894164	2076.405309	19.877005
54.643523	2077.612354	19.882023
54.569785	2083.150206	19.887040
55.162983	2094.030935	19.892058
55.176760	2103.500164	19.897075
55.342262	2107.930633	19.902093
55.343379	2109.110860	19.907111
55.643510	2109.089118	19.912128
55.348969	2106.900802	19.917146
55.219180	2109.584891	19.922163
55.665389	2101.261897	19.927181
55.366913	2106.301592	19.932199
54.971252	2108.553927	19.937216
55.952069	2119.130923	19.942234
55.941475	2135.597839	19.947251
56.035869	2127.260521	19.952269
56.322923	2130.703038	19.957287
56.123648	2133.426422	19.962304
56.289768	2115.215148	19.967322
56.504630	2126.893693	19.972339
56.703475	2101.247916	19.977357
56.233684	2098.051869	19.982375
56.297569	2092.291541	19.987392
56.603741	2085.543279	19.992410
56.294021	2091.231724	19.997427
56.411802	2087.710072	20.002445
56.649240	2100.477061	20.007463
56.676531	2105.396283	20.012480
56.893175	2095.957294	20.017498
56.939208	2111.771479	20.022515
56.786567	2107.282249	20.027533
57.190395	2104.309118	20.032551
56.885232	2104.735690	20.037568
56.842691	2085.553509	20.042586
56.854909	2104.349154	20.047603
56.966841	2106.105360	20.052621
57.136568	2114.720115	20.057639
56.790830	2114.736444	20.062656
57.083345	2107.687331	20.067674
57.149158	2115.624032	20.072691
57.199241	2113.277571	20.077709
57.016659	2119.006071	20.082727
57.131032	2113.310416	20.087744
57.346497	2127.851422	20.092762
57.228950	2137.947210	20.097779
56.983432	2136.180436	20.102797
57.279030	2136.878988	20.107815
57.050237	2137.198914	20.112832
57.356377	2148.282455	20.117850
57.497335	2163.059244	20.122867
57.690796	2168.305928	20.127885
57.877500	2163.946570	20.132903
57.667811	2161.378848	20.137920
58.088223	2160.991093	20.142938
58.174507	2158.171854	20.147955
58.264953	2166.723310	20.152973
58.295018	2179.579656	20.157991
58.735436	2184.566727	20.163008
58.566098	2168.727677	20.168026
58.558473	2165.983116	20.173043
58.829690	2162.147051	20.178061
58.398307	2154.053056	20.183079
57.986248	2156.765597	20.188096
58.699501	2167.744336	20.193114
58.450368	2182.837902	20.198131
58.471492	2184.677776	20.203149
58.859534	2191.661387	20.208167
58.661057	2181.009180	20.213184
58.722425	2187.349633	20.218202
58.829475	2188.380713	20.223219
58.823260	2188.384875	20.228237
59.258019	2192.489133	20.233255
59.157214	2199.495683	20.238272
59.216942	2194.130485	20.243290
59.206648	2193.513538	20.248307
59.370350	2206.904436	20.253325
59.395406	2197.454382	20.258343
58.987939	2200.825831	20.263360
59.594317	2192.436672	20.268378
59.549587	2199.039927	20.273395
59.688101	2195.587595	20.278413
59.747505	2200.931038	20.283431
59.435523	2202.999845	20.288448
59.286112	2200.608882	20.293466
59.369296	2203.562601	20.298483
59.691721	2215.479995	20.303501
60.078494	2217.300457	20.308519
60.014357	2226.324325	20.313536
60.057415	2212.983142	20.318554
60.037065	2232.263749	20.323571
60.343842	2214.039806	20.328589
60.505342	2219.206298	20.333607
60.046965	2214.787036	20.338624
60.041007	2217.057228	20.343642
60.102369	2216.773067	20.348659
59.918655	2232.680164	20.353677
60.233599	2247.574944	20.358695
60.528646	2246.389401	20.363712
60.843255	2239.690257	20.368730
60.816001	2250.087570	20.373747
60.697412	2240.641063	20.378765
60.523091	2238.831563	20.383783
60.345193	2253.809876	20.388800
60.991551	2254.737527	20.393818
60.906642	2270.411406	20.398835
61.265727	2263.175061	20.403853
61.269981	2271.140413	20.408871
61.102516	2268.247294	20.413888
61.323443	2265.880358	20.418906
61.700286	2268.942728	20.423923
61.280844	2261.572716	20.428941
61.452589	2268.514499	20.433959
61.234565	2273.188152	20.438976
61.537865	2271.556305	20.443994
61.552964	2275.600088	20.449011
61.797804	2278.070858	20.454029
61.951120	2287.619317	20.459047
61.636614	2297.723960	20.464064
61.997490	2291.405749	20.469082
61.988175	2287.118102	20.474099
61.753952	2289.509281	20.479117
62.093145	2287.594072	20.484135
61.929710	2286.915901	20.489152
61.915826	2281.918848	20.494170
62.042777	2280.403000	20.499187
62.000185	2300.069052	20.504205
62.424461	2307.599349	20.509223
62.621111	2312.043926	20.514240
62.722473	2314.180541	20.519258
62.723588	2311.084261	20.524275
62.615104	2319.742704	20.529293
62.712899	2308.248664	20.534311
62.559694	2314.083087	20.539328
62.595778	2304.842708	20.544346
62.870599	2307.296160	20.549363
62.388952	2304.019874	20.554381
62.910803	2313.567416	20.559399
63.040416	2332.846728	20.564416
63.237946	2326.326857	20.569434
63.694840	2334.991410	20.574451
63.336401	2337.477804	20.579469
63.438761	2332.696077	20.584487
63.655875	2337.961198	20.589504
63.604328	2337.858843	20.594522
63.518312	2327.911678	20.599539
63.514594	2334.054077	20.604557
63.501705	2329.634423	20.609575
63.439180	2338.216240	20.614592
63.615674	2335.234503	20.619610
63.487432	2332.458317	20.624627
63.423148	2329.145041	20.629645
63.662539	2337.379724	20.634663
63.885759	2347.557953	20.639680
64.200766	2349.708440	20.644698
64.448313	2344.203306	20.649715
64.235189	2345.492862	20.654733
64.473119	2344.878049	20.659751
64.615634	2349.700382	20.664768
64.786222	2346.116751	20.669786
64.893446	2344.667111	20.674803
64.967908	2340.451540	20.679821
64.848973	2325.696468	20.684839
64.612446	2324.553175	20.689856
64.663630	2317.866870	20.694874
65.057235	2326.594988	20.699891
64.853128	2344.316984	20.704909
65.237686	2339.882399	20.709927
64.845105	2341.929131	20.714944
64.947576	2334.357386	20.719962
65.111938	2341.729585	20.724979
65.136640	2329.991339	20.729997
65.367012	2331.435492	20.735015
65.161968	2322.557962	20.740032
65.130108	2331.463206	20.745050
65.345183	2328.178752	20.750067
64.985915	2331.460614	20.755085
65.148039	2340.739452	20.760103
65.222970	2348.857883	20.765120
65.313100	2354.837249	20.770138
65.165015	2362.416214	20.775155
65.385396	2369.713370	20.780173
66.119989	2379.600038	20.785191
65.899869	2393.379446	20.790208
65.776152	2398.035200	20.795226
65.653205	2392.158866	20.800243
65.967692	2395.783348	20.805261
66.049096	2391.598239	20.810279
66.232361	2402.483417	20.815296
66.189183	2414.114206	20.820314
66.622869	2409.479384	20.825331
66.770114	2424.968687	20.830349
66.896663	2408.420282	20.835367
66.974735	2409.616877	20.840384
66.650337	2411.873863	20.845402
66.688343	2414.847320	20.850419
66.841052	2411.702023	20.855437
66.684080	2407.295456	20.860455
66.712132	2410.267315	20.865472
66.696623	2412.586370	20.870490
66.892669	2401.335680	20.875507
66.674640	2409.219143	20.880525
67.105373	2416.701133	20.885543
66.979058	2422.054803	20.890560
67.005786	2431.528488	20.895578
67.405188	2430.598010	20.900595
67.441051	2431.435109	20.905613
67.799656	2434.175284	20.910631
67.352886	2437.335161	20.915648
67.517624	2424.476581	20.920666
67.760578	2429.876551	20.925683
67.451339	2448.912287	20.930701
67.912688	2454.252798	20.935719
67.953672	2461.975770	20.940736
68.152176	2464.434889	20.945754
68.165007	2460.812830	20.950771
67.804925	2459.291214	20.955789
67.857466	2455.460942	20.960807
68.067710	2452.423401	20.965824
68.238211	2454.157840	20.970842
68.232279	2452.738544	20.975859
68.203337	2468.009311	20.980877
68.550145	2468.226435	20.985895
68.430043	2481.706188	20.990912
68.631950	2476.290225	20.995930
69.096139	2480.667678	21.000947
68.694518	2485.363839	21.005965
68.900086	2478.621724	21.010983
68.667559	2480.813827	21.016000
68.550135	2484.013640	21.021018
69.186768	2487.534014	21.026035
68.726228	2498.744203	21.031053
68.852591	2506.548502	21.036071
69.000470	2507.285995	21.041088
69.047774	2507.935093	21.046106
69.330217	2498.160504	21.051123
69.590284	2525.429859	21.056141
70.136628	2522.639480	21.061159
69.988424	2525.739970	21.066176
69.343141	2515.299594	21.071194
70.209901	2511.149219	21.076211
70.029233	2519.446642	21.081229
70.315231	2518.407683	21.086247
70.453137	2515.757045	21.091264
70.187974	2500.368262	21.096282
70.205688	2487.194966	21.101299
69.953893	2492.382105	21.106317
70.230463	2503.132792	21.111335
70.244344	2515.821482	21.116352
70.388561	2515.536960	21.121370
70.709576	2507.403827	21.126387
70.589832	2515.240376	21.131405
70.500290	2511.697468	21.136423
70.995427	2507.494853	21.141440
70.797033	2512.064496	21.146458
71.085681	2510.008845	21.151475
70.923251	2512.016381	21.156493
71.106721	2500.234212	21.161511
70.794773	2508.407016	21.166528
70.913424	2516.221996	21.171546
71.112756	2518.103419	21.176563
71.101114	2530.887647	21.181581
71.093421	2534.272269	21.186599
71.193339	2531.599176	21.191616
71.053986	2537.548277	21.196634
71.246593	2531.256346	21.201651
71.230472	2548.074838	21.206669
71.484175	2551.039772	21.211687
71.611357	2560.422039	21.216704
71.325868	2556.351185	21.221722
72.275433	2550.171050	21.226739
71.777485	2554.187969	21.231757
71.817111	2554.137607	21.236775
72.053632	2566.207564	21.241792
72.058600	2579.380586	21.246810
72.412421	2575.436807	21.251827
72.286867	2578.618973	21.256845
72.589003	2571.000065	21.261863
72.179666	2575.271378	21.266880
72.266792	2582.554780	21.271898
72.509213	2578.117158	21.276915
72.539203	2580.211332	21.281933
72.341720	2575.249275	21.286951
72.771478	2577.214536	21.291968
72.522661	2599.131999	21.296986
72.638645	2604.362545	21.302003
72.676377	2599.537218	21.307021
72.824753	2587.085073	21.312039
73.012286	2599.080667	21.317056
73.200776	2613.872474	21.322074
73.595982	2611.083669	21.327091
73.437786	2617.676449	21.332109
73.418792	2618.616836	21.337127
73.534482	2620.369348	21.342144
73.476543	2627.265195	21.347162
73.576617	2616.360804	21.352179
73.474450	2612.374837	21.357197
73.553285	2609.480948	21.362215
74.005280	2616.003375	21.367232
73.745288	2632.866467	21.372250
74.080643	2638.454016	21.377267
73.988957	2639.197487	21.382285
73.794094	2644.407311	21.387303
74.366261	2639.662362	21.392320
74.158573	2635.197405	21.397338
74.166640	2638.535391	21.402355
74.107350	2642.565663	21.407373
74.284934	2662.686820	21.412391
74.648879	2667.831193	21.417408
74.454510	2663.701851	21.422426
74.965622	2662.681269	21.427443
74.824916	2659.127412	21.432461
74.815443	2668.856231	21.437479
75.084492	2659.550765	21.442496
74.983640	2685.690192	21.447514
75.513373	2684.038613	21.452531
75.173350	2684.546407	21.457549
75.670905	2691.374185	21.462567
75.518564	2688.611187	21.467584
75.708601	2690.465680	21.472602
75.662495	2685.681870	21.477619
75.795768	2677.748508	21.482637
76.080879	2675.715486	21.487655
75.891876	2680.548818	21.492672
76.039277	2678.827738	21.497690
76.154705	2673.185396	21.502707
76.200635	2687.933319	21.507725
75.932918	2676.136508	21.512743
76.252780	2680.176820	21.517760
76.168671	2673.255930	21.522778
76.448707	2679.019437	21.527795
76.237509	2683.925683	21.532813
76.597195	2675.972630	21.537831
76.366354	2665.782849	21.542848
75.976756	2691.361539	21.547866
76.379026	2707.426584	21.552883
76.423084	2708.578030	21.557901
76.336165	2713.057666	21.562919
76.582575	2713.924914	21.567936
76.890880	2727.378762	21.572954
77.293057	2727.577747	21.577971
77.340380	2726.478328	21.582989
77.292992	2741.815340	21.588007
77.554847	2731.276899	21.593024
77.466573	2741.677744	21.598042
77.110520	2734.202919	21.603059
77.358788	2730.714353	21.608077
77.453662	2732.997218	21.613095
77.573885	2733.824271	21.618112
77.342299	2737.326070	21.623130
77.735286	2749.056018	21.628147
77.668882	2759.604944	21.633165
77.525872	2763.651515	21.638183
77.770070	2754.387768	21.643200
77.464865	2763.610639	21.648218
78.289180	2777.839005	21.653235
78.329840	2773.369822	21.658253
78.635143	2775.064236	21.663271
78.730472	2776.652675	21.668288
78.544602	2782.921608	21.673306
78.921256	2774.653390	21.678323
78.846517	2772.326400	21.683341
78.552504	2779.502318	21.688359
78.866523	2778.108618	21.693376
78.953345	2785.578365	21.698394
78.764656	2773.721765	21.703411
78.831101	2769.491569	21.708429
78.594516	2770.784829	21.713447
78.907848	2790.035847	21.718464
78.901874	2797.261331	21.723482
79.029070	2804.055648	21.728499
78.927842	2806.321904	21.733517
78.875460	2816.871822	21.738535
79.244491	2827.706060	21.743552
78.970536	2830.731618	21.748570
79.138365	2837.188181	21.753587
79.662188	2849.519466	21.758605
79.594355	2857.786742	21.763623
80.014079	2858.229163	21.768640
80.002306	2848.150142	21.773658
80.208193	2868.626902	21.778675
80.627515	2873.942562	21.783693
80.447169	2870.230751	21.788711
80.931910	2865.461567	21.793728
80.512920	2870.804412	21.798746
80.643043	2863.824635	21.803763
80.978322	2871.517456	21.808781
80.599815	2869.758818	21.813799
81.264955	2862.805685	21.818816
80.924807	2866.327675	21.823834
80.899371	2860.666313	21.828851
80.975452	2864.356648	21.833869
81.143340	2861.492954	21.838887
81.466432	2862.300853	21.843904
81.051056	2860.630054	21.848922
81.052774	2859.108529	21.853939
81.705455	2878.148665	21.858957
81.095002	2885.105925	21.863975
81.791051	2881.638705	21.868992
81.778810	2879.560718	21.874010
81.800252	2883.982388	21.879027
81.785956	2881.519666	21.884045
81.892084	2887.847041	21.889063
81.990226	2878.246307	21.894080
81.885810	2885.386250	21.899098
82.087898	2892.055244	21.904115
82.324315	2901.575228	21.909133
82.292532	2905.825340	21.914151
82.340442	2900.130381	21.919168
82.493456	2904.963843	21.924186
82.061480	2913.363945	21.929203
82.340469	2918.026175	21.934221
82.224186	2931.130077	21.939239
82.531131	2927.625968	21.944256
82.601836	2939.071975	21.949274
82.684199	2936.837129	21.954291
83.072071	2942.975196	21.959309
82.938588	2963.072832	21.964327
83.418844	2960.649396	21.969344
82.838597	2958.354237	21.974362
83.286571	2948.127382	21.979379
83.573529	2952.485376	21.984397
83.518548	2946.607681	21.989415
83.613448	2954.625414	21.994432
83.529787	2957.722178	21.999450
84.259450	2968.402157	22.004467
83.969602	2963.804804	22.009485
83.762236	2974.732593	22.014503
84.179091	2976.005553	22.019520
84.340184	2979.669968	22.024538
84.192091	2983.812071	22.029555
84.293689	2970.940901	22.034573
84.345202	2967.461023	22.039591
84.633073	2969.353872	22.044608
84.474487	2964.290927	22.049626
84.843064	2971.988043	22.054643
84.943253	2981.204322	22.059661
84.712862	2990.219902	22.064679
85.298570	2998.924564	22.069696
85.390882	2995.419351	22.074714
84.985990	2999.311318	22.079731
85.253039	2996.176412	22.084749
85.371218	2995.962244	22.089767
85.529808	2989.435611	22.094784
85.446985	2998.560636	22.099802
85.451180	2989.517432	22.104819
85.721488	2984.576658	22.109837
85.548092	2991.146706	22.114855
85.610147	2977.076049	22.119872
85.678108	3003.861764	22.124890
85.790188	3015.418117	22.129907
85.904335	3010.422897	22.134925
85.970024	3013.489959	22.139943
86.242361	3021.192705	22.144960
86.366535	3016.053882	22.149978
86.267385	3015.655983	22.154995
86.136654	3019.325097	22.160013
86.349015	3044.210292	22.165031
86.499724	3051.518641	22.170048
86.633294	3043.648197	22.175066
86.671149	3037.083650	22.180083
86.611566	3044.260819	22.185101
86.733145	3065.511663	22.190119
86.873584	3063.813732	22.195136
86.750083	3070.581147	22.200154
86.892711	3074.781878	22.205171
86.909324	3085.223300	22.210189
86.994439	3102.323134	22.215207
87.030012	3096.895170	22.220224
87.316540	3101.269050	22.225242
87.386402	3123.184563	22.230259
87.731956	3120.412930	22.235277
87.707962	3124.497747	22.240295
87.638942	3124.215062	22.245312
88.034796	3118.263522	22.250330
87.771736	3119.813454	22.255347
88.175348	3124.039590	22.260365
88.290562	3146.459337	22.265383
88.667479	3136.846352	22.270400
88.577126	3142.188288	22.275418
88.607762	3144.067802	22.280435
88.872459	3133.869556	22.285453
88.732925	3139.727352	22.290471
89.014369	3138.215635	22.295488
89.425514	3139.154940	22.300506
89.267098	3140.811573	22.305523
89.461436	3136.018379	22.310541
89.304482	3137.747376	22.315559
89.538197	3126.354614	22.320576
89.298583	3140.317552	22.325594
89.249343	3137.727707	22.330611
89.379926	3132.407940	22.335629
89.432984	3130.764724	22.340647
89.468303	3122.849670	22.345664
89.447885	3145.262260	22.350682
89.289857	3157.059866	22.355699
89.646719	3157.373270	22.360717
89.429673	3160.456247	22.365735
89.681065	3179.013541	22.370752
89.877046	3182.495782	22.375770
90.022202	3193.636754	22.380787
90.019998	3189.041621	22.385805
90.080200	3212.934573	22.390823
90.472777	3217.187710	22.395840
90.503495	3220.187692	22.400858
90.283740	3224.618828	22.405875
90.548113	3215.929281	22.410893
90.819520	3237.709200	22.415911
90.855900	3237.949722	22.420928
90.922195	3237.667929	22.425946
91.232641	3251.169177	22.430963
91.276744	3242.387877	22.435981
91.551928	3237.345271	22.440999
91.497217	3252.548145	22.446016
91.561821	3254.577005	22.451034
91.644503	3257.922354	22.456051
91.772838	3255.175264	22.461069
91.925712	3258.377052	22.466087
91.664792	3256.707266	22.471104
92.090573	3258.360757	22.476122
91.950680	3261.507414	22.481139
91.841303	3266.568303	22.486157
92.203837	3281.453329	22.491175
92.400314	3276.028509	22.496192
92.516806	3271.916606	22.501210
92.217597	3278.522250	22.506227
92.279525	3288.903033	22.511245
92.477403	3302.302018	22.516263
92.369229	3299.175347	22.521280
92.837352	3309.716598	22.526298
92.974794	3318.731525	22.531315
93.428531	3326.787892	22.536333
93.388161	3327.867385	22.541351
93.838724	3325.571649	22.546368
93.811334	3328.953194	22.551386
93.776458	3329.750918	22.556403
93.883138	3321.070245	22.561421
94.074114	3322.369152	22.566439
93.950684	3320.204376	22.571456
94.202174	3316.951915	22.576474
93.945294	3326.038093	22.581491
93.987062	3311.222316	22.586509
94.276117	3322.337667	22.591527
94.625462	3322.286123	22.596544
94.616825	3317.281649	22.601562
94.215368	3325.614033	22.606579
94.559302	3326.535472	22.611597
94.635583	3328.123788	22.616615
94.419576	3348.600910	22.621632
94.314036	3346.414391	22.626650
94.252315	3354.437902	22.631667
94.620729	3347.938236	22.636685
94.941802	3374.883691	22.641703
94.569536	3379.430292	22.646720
94.999471	3371.933060	22.651738
95.083627	3377.042566	22.656755
94.937321	3393.222576	22.661773
95.407357	3395.882318	22.666791
95.528274	3402.409560	22.671808
95.367189	3402.542144	22.676826
95.594343	3409.210559	22.681843
96.149336	3417.746642	22.686861
96.013870	3420.166684	22.691879
96.201834	3434.773026	22.696896
96.538081	3424.740160	22.701914
96.044321	3434.387450	22.706931
96.067601	3431.066564	22.711949
96.210075	3422.957838	22.716967
96.232352	3434.919910	22.721984
96.712207	3441.927502	22.727002
96.703928	3447.982619	22.732019
97.193124	3451.728291	22.737037
96.903637	3452.578536	22.742055
96.765530	3453.430314	22.747072
96.781844	3459.759336	22.752090
96.922509	3480.963490	22.757107
96.824826	3473.337407	22.762125
97.534226	3488.032538	22.767143
97.417374	3492.621215	22.772160
97.887229	3494.583455	22.777178
97.502941	3500.252459	22.782195
97.889795	3492.427358	22.787213
97.869973	3489.880198	22.792231
97.782232	3498.125635	22.797248
98.592142	3505.583395	22.802266
98.385350	3520.684068	22.807283
98.358281	3525.350220	22.812301
98.747245	3517.376431	22.817319
98.353449	3523.643475	22.822336
98.631356	3528.164001	22.827354
98.514005	3515.121587	22.832371
98.485400	3527.782925	22.837389
99.072372	3534.044662	22.842407
99.044775	3550.900605	22.847424
98.949022	3551.401713	22.852442
99.147683	3547.617756	22.857459
99.276267	3546.739125	22.862477
99.377999	3556.312121	22.867495
99.384934	3563.842051	22.872512
99.554659	3559.690179	22.877530
99.839615	3569.385980	22.882547
99.672728	3573.193435	22.887565
99.803559	3571.673716	22.892583
99.828079	3585.573520	22.897600
100.390478	3587.672775	22.902618
100.273602	3598.088062	22.907635
100.446700	3603.679241	22.912653
100.739405	3602.162566	22.917671
100.317804	3598.295865	22.922688
100.572967	3591.996923	22.927706
100.822239	3607.114593	22.932723
101.342224	3612.682991	22.937741
101.145998	3613.711167	22.942759
101.115617	3623.074485	22.947776
101.263241	3615.163715	22.952794
101.113834	3618.482365	22.957811
101.059838	3615.549156	22.962829
101.219308	3606.856920	22.967847
101.156386	3611.926409	22.972864
101.646896	3623.344954	22.977882
101.789978	3636.724365	22.982899
101.881766	3637.281314	22.987917
102.009079	3625.885971	22.992935
101.564675	3633.575019	22.997952
102.246200	3632.751789	23.002970
102.187007	3639.143205	23.007987
102.427415	3644.799604	23.013005
102.876152	3646.840922	23.018023
102.560863	3652.600166	23.023040
103.077172	3646.901027	23.028058
103.209450	3640.779137	23.033075
102.934267	3648.334364	23.038093
103.387583	3642.503061	23.043111
103.117067	3635.371124	23.048128
103.356881	3636.438303	23.053146
103.321315	3645.035454	23.058163
103.280563	3647.087178	23.063181
103.555507	3637.205834	23.068199
103.310320	3640.227018	23.073216
103.354842	3647.526995	23.078234
103.471790	3676.133550	23.083251
103.679215	3679.241646	23.088269
103.800466	3679.329998	23.093287
103.999379	3687.256009	23.098304
103.949514	3692.118312	23.103322
104.296810	3694.058743	23.108339
103.954529	3705.405809	23.113357
104.492279	3699.655949	23.118375
104.257006	3721.174948	23.123392
104.474232	3715.172291	23.128410
104.700983	3724.811011	23.133427
104.288082	3728.152025	23.138445
104.876041	3742.538131	23.143463
104.707868	3748.479519	23.148480
105.256984	3754.475818	23.153498
105.402304	3751.394575	23.158515
105.198898	3763.777298	23.163533
105.690816	3766.405260	23.168551
105.651863	3775.564836	23.173568
105.564183	3776.187783	23.178586
105.434378	3781.192045	23.183603
105.942295	3792.077702	23.188621
106.163383	3798.699866	23.193639
106.109720	3803.019899	23.198656
106.525626	3802.433972	23.203674
106.659031	3801.557729	23.208691
106.713010	3801.722905	23.213709
107.191949	3806.546580	23.218727
107.126269	3805.136538	23.223744
107.340349	3801.365896	23.228762
107.173519	3797.336138	23.233779
107.314082	3798.633509	23.238797
107.399331	3792.146485	23.243815
106.764358	3796.163045	23.248832
107.213475	3809.242128	23.253850
107.134974	3815.059017	23.258867
107.086666	3823.443616	23.263885
107.249659	3824.204048	23.268903
107.250013	3847.466472	23.273920
107.270210	3847.532781	23.278938
107.549554	3859.268633	23.283955
107.782307	3873.183379	23.288973
108.104417	3880.970231	23.293991
107.940449	3871.858241	23.299008
108.051724	3879.485586	23.304026
108.447938	3886.386514	23.309043
108.511586	3910.039962	23.314061
108.854458	3890.224174	23.319079
108.749373	3893.535931	23.324096
108.972711	3888.595959	23.329114
109.299015	3899.563793	23.334131
109.366581	3913.668582	23.339149
109.088934	3912.215988	23.344167
109.243717	3920.193204	23.349184
109.425049	3920.253207	23.354202
109.821169	3910.646274	23.359219
109.713148	3913.617605	23.364237
109.545354	3914.508775	23.369255
109.596203	3923.506007	23.374272
109.802077	3934.653705	23.379290
110.158926	3930.999549	23.384307
110.410472	3940.953295	23.389325
110.637062	3932.938480	23.394343
110.615869	3950.690205	23.399360
110.623423	3958.696818	23.404378
110.973891	3956.672355	23.409395
110.905746	3968.541629	23.414413
111.053430	3964.595127	23.419431
111.218095	3956.880392	23.424448
111.124227	3962.807052	23.429466
110.985520	3958.842293	23.434483
110.816734	3975.420894	23.439501
111.409761	3982.922303	23.444519
111.561419	3987.731018	23.449536
111.513144	3977.846470	23.454554
112.310207	3972.570392	23.459571
111.996701	3978.588283	23.464589
112.642601	3982.921859	23.469607
112.723251	3979.427752	23.474624
112.471544	3977.904804	23.479642
112.828808	3977.713139	23.484659
112.213943	3973.169603	23.489677
112.379099	3981.606055	23.494695
112.678206	3983.165832	23.499712
112.751717	3979.388768	23.504730
113.319247	3980.723420	23.509747
113.288711	4009.022186	23.514765
113.906275	4003.013529	23.519783
113.695255	4005.552803	23.524800
113.727313	4003.309926	23.529818
113.623928	3997.647795	23.534835
113.401048	4000.353059	23.539853
113.693847	4005.755164	23.544871
113.802390	4004.718674	23.549888
113.808548	4000.314565	23.554906
114.381182	4010.934548	23.559923
114.229232	4021.245099	23.564941
114.486570	4019.197343	23.569959
114.723798	4023.964254	23.574976
114.672572	4021.908025	23.579994
114.718224	4015.389248	23.585011
114.704510	4015.183107	23.590029
115.234694	4011.350271	23.595047
115.274234	4019.197236	23.600064
115.192405	4039.158560	23.605082
115.731056	4048.372976	23.610099
115.632570	4040.405886	23.615117
115.957339	4042.687622	23.620135
115.621264	4037.942571	23.625152
115.680474	4033.003022	23.630170
115.774174	4030.819926	23.635187
115.470264	4039.689723	23.640205
115.807449	4044.762932	23.645223
115.925931	4054.901721	23.650240
116.029045	4061.943330	23.655258
116.708246	4057.518985	23.660275
116.603291	4062.487867	23.665293
116.244848	4056.007133	23.670311
116.643710	4065.142453	23.675328
116.637518	4078.371975	23.680346
116.754955	4087.816535	23.685363
116.321523	4090.198125	23.690381
116.376302	4100.760410	23.695399
116.947853	4109.493084	23.700416
116.757942	4113.705123	23.705434
117.229572	4120.351283	23.710451
117.287520	4138.494815	23.715469
117.723120	4144.821516	23.720487
117.698105	4146.659350	23.725504
117.415424	4163.173899	23.730522
118.218863	4168.322448	23.735539
117.926223	4172.418025	23.740557
118.075465	4168.363918	23.745575
118.475190	4179.632906	23.750592
118.456478	4187.495382	23.755610
118.754236	4193.272382	23.760627
118.727332	4193.106182	23.765645
119.180357	4194.998541	23.770663
119.112768	4197.398582	23.775680
119.148892	4210.154418	23.780698
119.382955	4214.195895	23.785715
119.502196	4220.894144	23.790733
119.590581	4219.280016	23.795751
119.878823	4216.040576	23.800768
119.623105	4221.449771	23.805786
120.066896	4227.895163	23.810803
120.067309	4243.333277	23.815821
120.195819	4244.342176	23.820839
120.406681	4252.818940	23.825856
120.461548	4249.502425	23.830874
120.369576	4239.637206	23.835891
120.386204	4261.189978	23.840909
120.704616	4266.780691	23.845927
121.071558	4272.745734	23.850944
120.728159	4280.488671	23.855962
120.831594	4272.117384	23.860979
121.279753	4294.887261	23.865997
121.390663	4294.693157	23.871015
121.261414	4300.707538	23.876032
121.026488	4308.641818	23.881050
121.444550	4311.303529	23.886067
121.512561	4335.878533	23.891085
121.491111	4332.940109	23.896103
122.097338	4333.811040	23.901120
122.339998	4350.432842	23.906138
122.238171	4352.566812	23.911155
122.256173	4357.024103	23.916173
122.371628	4346.886437	23.921191
122.552198	4360.913897	23.926208
122.646425	4373.102051	23.931226
123.125805	4367.061265	23.936243
123.271535	4369.610984	23.941261
122.816050	4363.173751	23.946279
123.316777	4378.467311	23.951296
123.050612	4386.987309	23.956314
123.377393	4382.059406	23.961331
123.732659	4388.903814	23.966349
123.952631	4405.292485	23.971367
124.571415	4399.908489	23.976384
124.549614	4413.734117	23.981402
124.576038	4391.069722	23.986419
124.806500	4373.632056	23.991437
124.630613	4373.123046	23.996455
124.519797	4374.601882	24.001472
124.605766	4384.891147	24.006490
125.171397	4385.597993	24.011507
125.426609	4392.969425	24.016525
125.014097	4392.446982	24.021543
125.339063	4390.726332	24.026560
124.918367	4397.575522	24.031578
125.345206	4396.192436	24.036595
125.234937	4406.427233	24.041613
125.352974	4425.391789	24.046631
125.252324	4426.237743	24.051648
125.266891	4427.930519	24.056666
125.559578	4443.013678	24.061683
125.686947	4448.239820	24.066701
125.930481	4456.913576	24.071719
126.278172	4463.282570	24.076736
126.200027	4484.863081	24.081754
126.456602	4469.381409	24.086771
126.631178	4487.911047	24.091789
126.459596	4500.418701	24.096807
126.755237	4502.531453	24.101824
126.801042	4523.982113	24.106842
127.122716	4536.346228	24.111859
127.036390	4529.103012	24.116877
127.202812	4538.458064	24.121895
127.508034	4544.110904	24.126912
127.820394	4545.981148	24.131930
127.921730	4555.949296	24.136947
128.138026	4551.003937	24.141965
128.064395	4562.697694	24.146983
128.419520	4569.412776	24.152000
128.114510	4574.447861	24.157018
128.690540	4578.360089	24.162035
128.623441	4576.776602	24.167053
128.451423	4594.006511	24.172071
128.635336	4600.720020	24.177088
128.763817	4606.937174	24.182106
128.855588	4611.837507	24.187123
129.214472	4625.171213	24.192141
128.906946	4625.812848	24.197159
129.261908	4639.709038	24.202176
129.561772	4646.019303	24.207194
129.699808	4658.185002	24.212211
130.105322	4656.211814	24.217229
130.066926	4666.605948	24.222247
130.307699	4673.316888	24.227264
130.244664	4678.165736	24.232282
130.597688	4681.809899	24.237299
130.817567	4680.626511	24.242317
130.707676	4693.525510	24.247335
131.324265	4701.354964	24.252352
131.362788	4709.530664	24.257370
131.431505	4718.995813	24.262387
131.303851	4708.956007	24.267405
131.098826	4719.811876	24.272423
131.304219	4711.837919	24.277440
131.250270	4742.202704	24.282458
131.501313	4736.513223	24.287475
131.597691	4744.408413	24.292493
131.316133	4753.925299	24.297511
131.814758	4758.692487	24.302528
131.734436	4768.559794	24.307546
132.019981	4788.739003	24.312563
132.348552	4784.972318	24.317581
132.646750	4794.411022	24.322599
132.806082	4811.103118	24.327616
132.986664	4812.921435	24.332634
133.070142	4815.780841	24.337651
133.124658	4817.669414	24.342669
133.058799	4811.676025	24.347687
133.663314	4834.459963	24.352704
133.436434	4845.975892	24.357722
133.798043	4837.387133	24.362739
134.075462	4839.774242	24.367757
133.969372	4842.925344	24.372775
134.101938	4849.119846	24.377792
134.121483	4860.988590	24.382810
134.267179	4857.626170	24.387827
134.589191	4858.203907	24.392845
134.474585	4870.677635	24.397863
135.118294	4872.906354	24.402880
134.857703	4885.453469	24.407898
134.634716	4887.038303	24.412915
135.321493	4896.719213	24.417933
135.399782	4917.881158	24.422951
135.729654	4916.235449	24.427968
135.447995	4912.450705	24.432986
135.441264	4914.765548	24.438003
135.991502	4921.693249	24.443021
135.897279	4943.728209	24.448039
135.831059	4941.450109	24.453056
135.686486	4950.680485	24.458074
136.056637	4964.634518	24.463091
136.662059	4970.205738	24.468109
136.548693	4968.632622	24.473127
136.596392	4990.152979	24.478144
136.871912	4992.063765	24.483162
137.041344	4996.058724	24.488179
137.374062	5003.503490	24.493197
137.211634	5022.099097	24.498215
137.020382	5014.392326	24.503232
137.558869	5021.915342	24.508250
137.494371	5046.177468	24.513267
138.217437	5054.615398	24.518285
137.922526	5054.841559	24.523303
138.257277	5053.725379	24.528320
138.231982	5073.678980	24.533338
138.491129	5070.860619	24.538355
138.705689	5069.198240	24.543373
138.754054	5070.756361	24.548391
139.282832	5082.075138	24.553408
139.346416	5093.031194	24.558426
139.337742	5084.667628	24.563443
139.739109	5089.532213	24.568461
139.585313	5089.360632	24.573479
139.661035	5086.747773	24.578496
139.664239	5102.388200	24.583514
140.046622	5112.240021	24.588531
139.987762	5105.519423	24.593549
140.203492	5114.797602	24.598567
140.419000	5121.736785	24.603584
140.575643	5134.824770	24.608602
141.124224	5138.671977	24.613619
141.375776	5137.344709	24.618637
140.808075	5145.157873	24.623655
141.147405	5138.750515	24.628672
141.111693	5138.633035	24.633690
141.114253	5158.986410	24.638707
141.602448	5158.108183	24.643725
141.440258	5167.868581	24.648743
141.338959	5156.290291	24.653760
141.892531	5179.070016	24.658778
141.905585	5184.648879	24.663795
142.010828	5181.248545	24.668813
142.009808	5191.416160	24.673831
142.228515	5192.818184	24.678848
142.465226	5212.822431	24.683866
142.017725	5214.742345	24.688883
142.485638	5230.231162	24.693901
142.529514	5242.055306	24.698919
142.931649	5241.111643	24.703936
143.063168	5261.407049	24.708954
143.033831	5268.883393	24.713971
143.238220	5274.508066	24.718989
143.160610	5282.156122	24.724007
143.724797	5290.571704	24.729024
144.204528	5291.213133	24.734042
143.634240	5304.825486	24.739059
144.210337	5312.983527	24.744077
144.137928	5320.507675	24.749095
144.437319	5321.814997	24.754112
144.572825	5334.136219	24.759130
145.083512	5347.402481	24.764147
145.335254	5339.493592	24.769165
145.438289	5341.371461	24.774183
145.286297	5342.509597	24.779200
145.424354	5347.803768	24.784218
145.610125	5369.678582	24.789235
145.817846	5371.214920	24.794253
145.846483	5364.259554	24.799271
146.134518	5363.441086	24.804288
146.232904	5370.332424	24.809306
146.495803	5385.948191	24.814323
146.801412	5380.180517	24.819341
146.571323	5388.660605	24.824359
146.679328	5389.379214	24.829376
147.220634	5403.957039	24.834394
147.031612	5414.043749	24.839411
147.749098	5410.370683	24.844429
147.142827	5415.614183	24.849447
147.701123	5417.843726	24.854464
147.926096	5414.222566	24.859482
148.225190	5438.623963	24.864499
148.190948	5444.772199	24.869517
148.207020	5442.171791	24.874535
147.969370	5438.143293	24.879552
148.430971	5433.730618	24.884570
148.470912	5460.495937	24.889587
148.926008	5456.245266	24.894605
148.723683	5457.596476	24.899623
148.788023	5462.548685	24.904640
149.020416	5479.428817	24.909658
149.125450	5490.590113	24.914675
149.591226	5488.755760	24.919693
149.609768	5498.137631	24.924711
149.910537	5503.772529	24.929728
150.185099	5510.636319	24.934746
150.143247	5517.224547	24.939763
150.356341	5513.807254	24.944781
150.175927	5507.957850	24.949799
150.247101	5537.366827	24.954816
150.133776	5538.050670	24.959834
150.141328	5545.208837	24.964851
150.714028	5562.341928	24.969869
150.600446	5564.181153	24.974887
150.811795	5586.958184	24.979904
151.314079	5590.932695	24.984922
151.308055	5594.617511	24.989939
151.313728	5605.961748	24.994957
151.545008	5609.653583	24.999975
151.891457	5616.458801	25.004992
151.896753	5618.279408	25.010010
152.203658	5630.283564	25.015027
152.420421	5636.023208	25.020045
152.636574	5642.984586	25.025063
152.719682	5655.380524	25.030080
153.339531	5654.478494	25.035098
153.128523	5660.976476	25.040115
153.219376	5661.098013	25.045133
153.424476	5655.254455	25.050151
153.535751	5654.154312	25.055168
153.968139	5657.221193	25.060186
153.544951	5676.426520	25.065203
153.754040	5682.097934	25.070221
153.828021	5683.620528	25.075239
153.869115	5704.871287	25.080256
154.125469	5707.037688	25.085274
154.346810	5718.190372	25.090291
154.792347	5735.656061	25.095309
154.902319	5737.378206	25.100327
155.115613	5741.281228	25.105344
155.371905	5732.225575	25.110362
155.666402	5743.568843	25.115379
156.002313	5756.045200	25.120397
155.551466	5760.522622	25.125415
156.100524	5754.075880	25.130432
156.030989	5757.773835	25.135450
155.908275	5759.024207	25.140467
156.119244	5771.005605	25.145485
156.432942	5778.005417	25.150503
156.536975	5775.328048	25.155520
156.916123	5784.435758	25.160538
157.098060	5796.226005	25.165555
157.357307	5799.471558	25.170573
157.315068	5794.837845	25.175591
157.167412	5802.920091	25.180608
157.407318	5809.719976	25.185626
157.381777	5828.234979	25.190643
157.666285	5830.005551	25.195661
157.888783	5852.560196	25.200679
158.190714	5854.185989	25.205696
158.224888	5859.291397	25.210714
158.259736	5868.831896	25.215731
158.784510	5873.487956	25.220749
158.892260	5883.512647	25.225767
158.797319	5880.831711	25.230784
159.021777	5892.830016	25.235802
159.509842	5906.008685	25.240819
159.346110	5907.899995	25.245837
159.578770	5911.206555	25.250855
159.843216	5927.191881	25.255872
160.622970	5918.808588	25.260890
160.504776	5927.934309	25.265907
160.381467	5929.724586	25.270925
160.850349	5920.663946	25.275943
160.634819	5927.408956	25.280960
160.971746	5934.013754	25.285978
161.496125	5940.544994	25.290995
160.790293	5947.130069	25.296013
161.189934	5949.539216	25.301031
161.374406	5950.271122	25.306048
161.544353	5963.348148	25.311066
161.353623	5974.893846	25.316083
161.932280	5967.972039	25.321101
162.328203	5977.178234	25.326119
162.061637	5996.675033	25.331136
162.415035	5990.050517	25.336154
162.770032	5993.508390	25.341171
162.746566	5994.377047	25.346189
163.032097	6000.759479	25.351207
162.967533	6012.285436	25.356224
163.352229	6021.032527	25.361242
163.331722	6015.770317	25.366259
163.138565	6023.171617	25.371277
163.380640	6023.720881	25.376295
163.228864	6043.461756	25.381312
163.673089	6043.887805	25.386330
163.542682	6059.442653	25.391347
163.628670	6075.301386	25.396365
164.032733	6080.443611	25.401383
163.700962	6102.046824	25.406400
164.206052	6114.184402	25.411418
164.415948	6126.832280	25.416435
164.506488	6149.865696	25.421453
164.843993	6159.185308	25.426471
164.800124	6162.948773	25.431488
164.375263	6182.454784	25.436506
165.305033	6196.221073	25.441523
165.265162	6217.049476	25.446541
165.410918	6226.894778	25.451559
165.931975	6226.172353	25.456576
166.395544	6238.471201	25.461594
166.701822	6259.059172	25.466611
167.172613	6262.489486	25.471629
167.569801	6260.192287	25.476647
167.369521	6269.406799	25.481664
167.725789	6258.131785	25.486682
167.523207	6270.452940	25.491699
167.436993	6283.510346	25.496717
167.685389	6297.345577	25.501735
167.735281	6299.935837	25.506752
168.220696	6302.180068	25.511770
168.415827	6318.236575	25.516787
168.366412	6321.309602	25.521805
168.551561	6311.491394	25.526823
168.820860	6333.859363	25.531840
168.796014	6332.348024	25.536858
169.251595	6340.503311	25.541875
169.105156	6355.129664	25.546893
169.497627	6366.558989	25.551911
169.147266	6367.276840	25.556928
169.538046	6374.589957	25.561946
169.651466	6394.065528	25.566963
169.573396	6413.751059	25.571981
170.265626	6414.277165	25.576999
170.283711	6423.504897	25.582016
170.664257	6438.654866	25.587034
171.022327	6458.701445	25.592051
170.900189	6461.564911	25.597069
171.153787	6453.225925	25.602087
171.180001	6473.614938	25.607104
171.578793	6474.764716	25.612122
172.125731	6478.221023	25.617139
172.021706	6474.843764	25.622157
172.393489	6480.322627	25.627175
172.381145	6491.076751	25.632192
172.594810	6491.920909	25.637210
172.999989	6487.800940	25.642227
172.799198	6494.600671	25.647245
173.005678	6498.034556	25.652263
173.112142	6511.077722	25.657280
173.385311	6517.793740	25.662298
173.821184	6520.834969	25.667315
173.746745	6517.831887	25.672333
173.787515	6518.106491	25.677351
173.906432	6535.160060	25.682368
173.828486	6539.386681	25.687386
174.008470	6550.189630	25.692404
174.066983	6562.530057	25.697421
174.334695	6565.812303	25.702439
174.202426	6573.939830	25.707456
174.304328	6587.539370	25.712474
174.694469	6596.153297	25.717492
174.760353	6619.671007	25.722509
175.148538	6632.196596	25.727527
175.266521	6635.057196	25.732544
175.119769	6652.228259	25.737562
175.598374	6664.060980	25.742580
175.625009	6680.182083	25.747597
176.149256	6684.488025	25.752615
176.107250	6689.447756	25.757632
176.587025	6707.941306	25.762650
176.721373	6716.200754	25.767668
176.732815	6733.362894	25.772685
176.928764	6734.304545	25.777703
177.342293	6751.631004	25.782720
177.567140	6762.038755	25.787738
177.550636	6761.406841	25.792756
177.560865	6772.425928	25.797773
177.902729	6789.138588	25.802791
178.200168	6789.957008	25.807808
178.421028	6804.055801	25.812826
178.555511	6809.906569	25.817844
178.444739	6822.800889	25.822861
178.889208	6822.595545	25.827879
179.283943	6847.959317	25.832896
179.264121	6849.891315	25.837914
179.838594	6852.086939	25.842932
179.565323	6873.378830	25.847949
179.742534	6877.745499	25.852967
179.908567	6893.327220	25.857984
180.012625	6899.621591	25.863002
180.298016	6906.335837	25.868020
180.333767	6922.218957	25.873037
180.796058	6932.005578	25.878055
180.582923	6936.057741	25.883072
180.725695	6951.251699	25.888090
181.190357	6949.442637	25.893108
181.128974	6978.587413	25.898125
181.977669	6980.301282	25.903143
181.789313	6996.699425	25.908160
181.908628	6998.615956	25.913178
182.306258	7009.205134	25.918196
181.936650	7019.665119	25.923213
182.380168	7031.661421	25.928231
182.708383	7030.277814	25.933248
182.775203	7049.786637	25.938266
183.191873	7064.928308	25.943284
183.241249	7069.201400	25.948301
183.445442	7082.801066	25.953319
184.114981	7095.393388	25.958336
183.557471	7092.854193	25.963354
184.534167	7098.427892	25.968372
184.290700	7121.577991	25.973389
184.226876	7118.974079	25.978407
184.368471	7128.602688	25.983424
184.726042	7144.344031	25.988442
185.053887	7147.137108	25.993460
185.117076	7163.199239	25.998477
185.564946	7169.932325	26.003495
185.825553	7169.891531	26.008512
185.881096	7169.115724	26.013530
186.164902	7179.871210	26.018548
186.217616	7195.249952	26.023565
186.506617	7195.403598	26.028583
186.594362	7199.629669	26.033600
186.652023	7199.330229	26.038618
186.886703	7210.873196	26.043636
187.038612	7217.444306	26.048653
187.608831	7213.197299	26.053671
187.404613	7223.609390	26.058688
187.381234	7235.224370	26.063706
187.373223	7245.451044	26.068724
187.647513	7255.964979	26.073741
188.044863	7269.922829	26.078759
188.381282	7265.216795	26.083776
188.303231	7281.424278	26.088794
188.546568	7295.794583	26.093812
188.614154	7314.419615	26.098829
188.561949	7321.991929	26.103847
188.693119	7324.200235	26.108864
188.876977	7342.494540	26.113882
189.385044	7355.238617	26.118900
189.384328	7370.584835	26.123917
189.726156	7383.986371	26.128935
189.816236	7395.754154	26.133952
189.730057	7408.079931	26.138970
190.116072	7418.153420	26.143988
190.434901	7441.566256	26.149005
190.484250	7457.037297	26.154023
190.656545	7472.539602	26.159040
190.941627	7478.616393	26.164058
191.069277	7490.653010	26.169076
191.705075	7498.802683	26.174093
191.758686	7518.816034	26.179111
192.136989	7527.397528	26.184128
191.990716	7543.372838	26.189146
192.254506	7546.409630	26.194164
192.503741	7556.491995	26.199181
192.901808	7569.250296	26.204199
193.511157	7587.250882	26.209216
193.323491	7585.537641	26.214234
193.440939	7590.561031	26.219252
193.792309	7605.887015	26.224269
193.637794	7613.279741	26.229287
194.109185	7626.566445	26.234304
194.491237	7630.017237	26.239322
194.508863	7634.813186	26.244340
194.657627	7649.826831	26.249357
195.000983	7651.837770	26.254375
194.857428	7658.729986	26.259392
195.099177	7678.221540	26.264410
195.521334	7676.659005	26.269428
195.745084	7691.016901	26.274445
195.851032	7693.765899	26.279463
196.474516	7685.655703	26.284480
196.254759	7710.845426	26.289498
196.848903	7703.150234	26.294516
197.025518	7719.450801	26.299533
196.987377	7716.457621	26.304551
197.468486	7718.465929	26.309568
197.440657	7729.766213	26.314586
197.709082	7727.403769	26.319604
197.758319	7745.031328	26.324621
197.870304	7741.275878	26.329639
198.124776	7756.323562	26.334656
198.044045	7760.958158	26.339674
198.405799	7772.885672	26.344692
198.451225	7777.355284	26.349709
198.629082	7787.319519	26.354727
198.854776	7800.796379	26.359744
199.163610	7823.021057	26.364762
198.974378	7825.929971	26.369780
199.262316	7846.670977	26.374797
199.551472	7860.908262	26.379815
199.985494	7865.200207	26.384832
200.074479	7877.454657	26.389850
200.113811	7879.115459	26.394868
200.353038	7894.023576	26.399885
200.323226	7901.150629	26.404903
200.942070	7912.419173	26.409920
200.955058	7921.781051	26.414938
201.251259	7932.216171	26.419956
201.496031	7953.819627	26.424973
201.190791	7960.153225	26.429991
201.553525	7964.349021	26.435008
201.625712	7986.850907	26.440026
202.021693	7998.249129	26.445044
202.458836	8016.662278	26.450061
202.524935	8017.062377	26.455079
203.207896	8022.868649	26.460096
203.026726	8045.208244	26.465114
203.473079	8040.491107	26.470132
203.723204	8048.395207	26.475149
203.471926	8062.483687	26.480167
203.622193	8068.509180	26.485184
203.737583	8080.232392	26.490202
204.355273	8086.547732	26.495220
204.225840	8109.314979	26.500237
204.001166	8127.610920	26.505255
204.780516	8137.531629	26.510272
204.804249	8157.752408	26.515290
204.868774	8170.086654	26.520308
205.717935	8176.005852	26.525325
205.788974	8193.523082	26.530343
206.200725	8198.036435	26.535360
206.477948	8196.954346	26.540378
206.592724	8213.552334	26.545396
206.814695	8214.998285	26.550413
207.001856	8225.008655	26.555431
207.235945	8235.857789	26.560448
207.307298	8256.604771	26.565466
207.808176	8253.833304	26.570484
207.834357	8265.946308	26.575501
207.965965	8276.517907	26.580519
208.328536	8279.779289	26.585536
208.387680	8292.379659	26.590554
208.482529	8301.700491	26.595572
208.985627	8306.922547	26.600589
209.202824	8326.065032	26.605607
209.369746	8331.137702	26.610624
209.033467	8342.322509	26.615642
209.626579	8351.337994	26.620660
210.275069	8365.292062	26.625677
209.895881	8371.454269	26.630695
210.487905	8379.008178	26.635712
210.364440	8391.760352	26.640730
210.414302	8389.934052	26.645748
211.053583	8406.671047	26.650765
210.716675	8417.180366	26.655783
210.937039	8423.993755	26.660800
211.717871	8434.864699	26.665818
211.634792	8440.115478	26.670836
211.693947	8454.837571	26.675853
212.084953	8466.161090	26.680871
212.589228	8469.261392	26.685888
212.921307	8488.105060	26.690906
213.623030	8470.813846	26.695924
214.024457	8467.729583	26.700941
214.019567	8467.001076	26.705959
214.327356	8453.658064	26.710976
214.787551	8466.943974	26.715994
214.506281	8468.787655	26.721012
214.837064	8461.092367	26.726029
214.312338	8468.865461	26.731047
214.929962	8465.096952	26.736064
214.809877	8471.512219	26.741082
214.917478	8482.330799	26.746100
215.143789	8495.470253	26.751117
214.935862	8505.315353	26.756135
215.129179	8506.456412	26.761152
214.987827	8532.910469	26.766170
215.582792	8542.112031	26.771188
216.255293	8555.004827	26.776205
216.047955	8577.595422	26.781223
216.225945	8588.182033	26.786240
216.266429	8605.972801	26.791258
216.256298	8619.796608	26.796276
216.817275	8636.565022	26.801293
216.795301	8657.791181	26.806311
217.070896	8670.923039	26.811328
217.002127	8694.467643	26.816346
217.479113	8709.323386	26.821364
218.020401	8727.982978	26.826381
217.838954	8745.492925	26.831399
218.844697	8752.669611	26.836416
218.596697	8759.951150	26.841434
219.015005	8782.043014	26.846452
219.584713	8800.006796	26.851469
219.665310	8814.274332	26.856487
219.913764	8817.421084	26.861504
219.516211	8824.280907	26.866522
219.527153	8847.162828	26.871540
220.261045	8854.713652	26.876557
220.398251	8874.030254	26.881575
221.073224	8896.369355	26.886592
221.126322	8909.716200	26.891610
221.248350	8926.825165	26.896628
221.575008	8926.972931	26.901645
221.619342	8946.493592	26.906663
221.714241	8952.726954	26.911680
222.198666	8973.296367	26.916698
222.138226	8988.536464	26.921716
222.674187	9006.736213	26.926733
222.673158	9014.995798	26.931751
222.847995	9031.045218	26.936768
223.531032	9044.558687	26.941786
223.451247	9052.208645	26.946804
223.615634	9076.733847	26.951821
223.673730	9092.511140	26.956839
224.082290	9101.770600	26.961856
224.006338	9114.395849	26.966874
224.209902	9130.844987	26.971892
224.504721	9151.829489	26.976909
224.728558	9160.514875	26.981927
225.391348	9174.467316	26.986944
225.644479	9195.057422	26.991962
225.708118	9204.895078	26.996980
226.071959	9219.181699	27.001997
225.973539	9236.890639	27.007015
226.308788	9244.513546	27.012032
226.806207	9263.328944	27.017050
226.985286	9279.902026	27.022068
227.129811	9294.876625	27.027085
227.457498	9296.201909	27.032103
228.170355	9293.817007	27.037120
228.744852	9306.327861	27.042138
228.788778	9314.454244	27.047156
229.624563	9302.985445	27.052173
229.259880	9305.129589	27.057191
229.559549	9302.717852	27.062208
229.625143	9296.434036	27.067226
229.860546	9299.781826	27.072244
230.101197	9291.563574	27.077261
229.947051	9307.374299	27.082279
229.899801	9321.299161	27.087296
230.061686	9332.412835	27.092314
230.080868	9352.531437	27.097332
230.655706	9351.516324	27.102349
230.478706	9368.467315	27.107367
230.762471	9380.726976	27.112384
231.002159	9402.077174	27.117402
230.845174	9418.422025	27.122420
231.387948	9433.328033	27.127437
231.544385	9452.983215	27.132455
231.604703	9465.824155	27.137472
231.897015	9481.776629	27.142490
232.257064	9511.386644	27.147508
232.400021	9524.577773	27.152525
232.793949	9539.996572	27.157543
233.249612	9557.723210	27.162560
233.508823	9568.746002	27.167578
233.680204	9592.156243	27.172596
233.722752	9603.042499	27.177613
233.767833	9621.502878	27.182631
234.046207	9643.911325	27.187648
234.546632	9659.540871	27.192666
234.457001	9677.233066	27.197684
235.089267	9688.450077	27.202701
235.356825	9713.853494	27.207719
235.477773	9723.714021	27.212736
236.292469	9740.124794	27.217754
236.114509	9750.414203	27.222772
236.616458	9759.791973	27.227789
236.449541	9785.494040	27.232807
236.610021	9789.144136	27.237824
237.105937	9805.020787	27.242842
237.335436	9827.051909	27.247860
237.748012	9820.195748	27.252877
237.854898	9839.969610	27.257895
237.829013	9847.374645	27.262912
238.419221	9860.877994	27.267930
238.581339	9874.110573	27.272948
238.527699	9892.027824	27.277965
238.756642	9917.532290	27.282983
239.135069	9922.840644	27.288000
239.542873	9933.890893	27.293018
239.692535	9962.397914	27.298036
240.005889	9967.789095	27.303053
240.461049	9987.199127	27.308071
240.374721	9987.781020	27.313088
241.179552	10018.177826	27.318106
240.951163	10022.179370	27.323124
241.434452	10031.405487	27.328141
241.258986	10051.268008	27.333159
241.643611	10065.403625	27.338176
241.539565	10075.277482	27.343194
241.573956	10099.694940	27.348212
241.839196	10110.897084	27.353229
242.523322	10141.439297	27.358247
242.306944	10156.341670	27.363264
243.022122	10166.137758	27.368282
242.820631	10190.693327	27.373300
243.222726	10212.751543	27.378317
243.359094	10239.565511	27.383335
243.781473	10250.200037	27.388352
244.379702	10260.339716	27.393370
244.737724	10282.910115	27.398388
244.868323	10281.838249	27.403405
244.879479	10285.657079	27.408423
245.023365	10309.009376	27.413440
245.665469	10311.763182	27.418458
246.115674	10336.396827	27.423476
246.958036	10329.495256	27.428493
246.953987	10324.939676	27.433511
247.267582	10326.658773	27.438528
247.335593	10328.410026	27.443546
247.326840	10343.333699	27.448564
247.369556	10350.459801	27.453581
247.985814	10361.850233	27.458599
247.658741	10381.061152	27.463616
247.947409	10383.567217	27.468634
248.657431	10400.718039	27.473652
248.761502	10407.493541	27.478669
249.033277	10425.145615	27.483687
249.153068	10435.837122	27.488704
249.458784	10445.179672	27.493722
249.609880	10463.548496	27.498740
249.667913	10473.043531	27.503757
249.687394	10490.425754	27.508775
249.738974	10507.897690	27.513792
250.052114	10523.181557	27.518810
250.676686	10546.247296	27.523828
250.915687	10557.665372	27.528845
250.954729	10577.071740	27.533863
251.225438	10585.718875	27.538880
251.344694	10609.912150	27.543898
251.521021	10627.323608	27.548916
252.129298	10645.703087	27.553933
252.212465	10670.502026	27.558951
252.426750	10689.356906	27.563968
252.885173	10707.873593	27.568986
252.940417	10723.163291	27.574004
253.017249	10742.418662	27.579021
253.289720	10756.761826	27.584039
253.610506	10787.194665	27.589056
254.178937	10807.705583	27.594074
254.186487	10829.453742	27.599092
254.623606	10841.513518	27.604109
254.894203	10856.608553	27.609127
255.061444	10872.698639	27.614144
255.648263	10887.087386	27.619162
255.886586	10907.160702	27.624180
255.860052	10917.786994	27.629197
256.633910	10940.188845	27.634215
256.529289	10948.197117	27.639232
257.057192	10969.851294	27.644250
257.220904	10984.214827	27.649268
257.434109	10987.241169	27.654285
258.216008	10989.287982	27.659303
258.379433	11017.942861	27.664320
258.719539	11011.252344	27.669338
258.935407	11022.241737	27.674356
258.689531	11043.385693	27.679373
259.356494	11047.089314	27.684391
259.531824	11067.580001	27.689408
259.487909	11070.750836	27.694426
259.681931	11089.217749	27.699444
259.813748	11105.231486	27.704461
260.375875	11121.673574	27.709479
260.191821	11134.891807	27.714496
260.535152	11151.545022	27.719514
260.795796	11172.420319	27.724532
261.307034	11192.283833	27.729549
261.629630	11199.836900	27.734567
261.225654	11228.798862	27.739584
261.712835	11228.416287	27.744602
261.625777	11249.725054	27.749620
262.030221	11284.095800	27.754637
262.456480	11294.768206	27.759655
262.322079	11325.042717	27.764672
262.569786	11343.937226	27.769690
262.845477	11364.513560	27.774708
262.846311	11390.478893	27.779725
263.498348	11424.062743	27.784743
263.636660	11449.592967	27.789760
263.691152	11469.607267	27.794778
263.793589	11498.525047	27.799796
264.040565	11516.529379	27.804813
264.878523	11543.453186	27.809831
265.037765	11576.842945	27.814848
265.373306	11599.450030	27.819866
265.690777	11615.551954	27.824884
265.911827	11645.768139	27.829901
266.166507	11659.729541	27.834919
266.437507	11692.912537	27.839936
266.465169	11702.296116	27.844954
267.043941	11724.063189	27.849972
267.470152	11750.284469	27.854989
267.495759	11778.137930	27.860007
267.847114	11804.702574	27.865024
268.376460	11808.317386	27.870042
268.736629	11830.330395	27.875060
269.127995	11852.954301	27.880077
269.609464	11877.752436	27.885095
270.112742	11897.940034	27.890112
269.958039	11904.087172	27.895130
269.997318	11919.598229	27.900148
270.174297	11942.600022	27.905165
270.911414	11944.518177	27.910183
271.062247	11970.950264	27.915200
271.448343	11983.767158	27.920218
272.310447	12006.825908	27.925236
272.427651	12007.934902	27.930253
272.767823	12002.661862	27.935271
272.991881	12019.378741	27.940288
273.913637	12022.802656	27.945306
273.985905	12027.632226	27.950324
274.245521	12027.885262	27.955341
274.751484	12032.653210	27.960359
275.155041	12048.066257	27.965376
275.024625	12036.065087	27.970394
275.531354	12039.948741	27.975412
275.468165	12052.513971	27.980429
275.588646	12058.217014	27.985447
275.742643	12078.541624	27.990464
276.000130	12080.913863	27.995482
275.962531	12094.163507	28.000500
276.142364	12125.826867	28.005517
275.875806	12126.143384	28.010535
275.857145	12145.879345	28.015552
275.988635	12162.999260	28.020570
276.751781	12194.558728	28.025588
276.766973	12221.814495	28.030605
277.495358	12239.106231	28.035623
277.669189	12254.485962	28.040640
278.092114	12277.683314	28.045658
278.512396	12305.096791	28.050676
278.469097	12322.888425	28.055693
278.664637	12336.215399	28.060711
278.864377	12363.647719	28.065728
278.696145	12379.264290	28.070746
279.389193	12400.376365	28.075764
279.575194	12434.284493	28.080781
279.955059	12447.595302	28.085799
280.181199	12484.383497	28.090816
280.161120	12505.026357	28.095834
280.565697	12525.924818	28.100852
280.818225	12547.229221	28.105869
281.320410	12570.733460	28.110887
281.886245	12601.535054	28.115904
281.888093	12611.330494	28.120922
282.337538	12632.730461	28.125940
282.287057	12656.952957	28.130957
282.989227	12676.137610	28.135975
282.834424	12699.394402	28.140992
283.352016	12714.600659	28.146010
283.733350	12736.775621	28.151028
283.858376	12764.905488	28.156045
284.482343	12774.189874	28.161063
284.406607	12811.843888	28.166080
284.843388	12833.937647	28.171098
285.165533	12851.688321	28.176116
285.451927	12866.356178	28.181133
286.120881	12881.482016	28.186151
286.431939	12904.909243	28.191168
286.848482	12915.618832	28.196186
287.244262	12931.207505	28.201204
287.186106	12955.990537	28.206221
287.816801	12969.843481	28.211239
287.676014	12993.354230	28.216256
287.903509	13003.660847	28.221274
288.264504	13035.669987	28.226292
288.321127	13059.156210	28.231309
289.128211	13075.384793	28.236327
289.133923	13095.241085	28.241344
289.357186	13112.944336	28.246362
289.742963	13124.972570	28.251380
290.229477	13146.645212	28.256397
290.437397	13160.315045	28.261415
290.920965	13175.880694	28.266432
290.654678	13199.190301	28.271450
291.064856	13222.649764	28.276468
291.190984	13243.870539	28.281485
291.663687	13266.382344	28.286503
292.117096	13296.618457	28.291520
292.380833	13326.830644	28.296538
292.814993	13334.054454	28.301556
292.605219	13363.289265	28.306573
293.374090	13375.390283	28.311591
293.383057	13402.456086	28.316608
293.731136	13431.167811	28.321626
293.779190	13437.286841	28.326644
294.053667	13467.886005	28.331661
294.702544	13495.148551	28.336679
294.824371	13522.405274	28.341696
295.317972	13543.218280	28.346714
295.568119	13558.823968	28.351732
295.941329	13593.440664	28.356749
296.200208	13597.369786	28.361767
296.572753	13625.389522	28.366784
296.846432	13640.445251	28.371802
297.628145	13656.261448	28.376820
297.793031	13670.494204	28.381837
298.273093	13684.750235	28.386855
298.454738	13693.545391	28.391872
298.273318	13718.143453	28.396890
298.868263	13727.909722	28.401908
299.292670	13740.522852	28.406925
299.591538	13757.936953	28.411943
300.097649	13773.262709	28.416960
300.353605	13785.621189	28.421978
300.828064	13802.950980	28.426996
300.841678	13810.007154	28.432013
300.822146	13817.336958	28.437031
301.036571	13836.239175	28.442048
301.101229	13859.311422	28.447066
301.944617	13856.412868	28.452084
302.099269	13882.117509	28.457101
302.353330	13901.702044	28.462119
302.524875	13917.415082	28.467136
302.932013	13930.716348	28.472154
303.289598	13944.527522	28.477172
303.154831	13967.337436	28.482189
303.501342	13989.790916	28.487207
304.057900	14015.489626	28.492224
303.914643	14033.630122	28.497242
304.206020	14052.106788	28.502260
304.581811	14085.669170	28.507277
304.635693	14112.934224	28.512295
305.366548	14125.499607	28.517312
305.773884	14144.204531	28.522330
306.501894	14156.681952	28.527348
306.875217	14178.897755	28.532365
306.980945	14194.643439	28.537383
307.369171	14201.416849	28.542400
307.628142	14223.199004	28.547418
308.081388	14238.192339	28.552436
307.891397	14258.481585	28.557453
308.232864	14288.897879	28.562471
308.451087	14306.438809	28.567488
309.117536	14337.669606	28.572506
309.161065	14348.128939	28.577524
309.449962	14365.368302	28.582541
309.957805	14391.214110	28.587559
310.322142	14406.123602	28.592576
310.319893	14433.546341	28.597594
310.781980	14453.591531	28.602612
311.100889	14478.548025	28.607629
311.046861	14499.564717	28.612647
311.592966	14519.205201	28.617664
311.721500	14541.646105	28.622682
312.791571	14557.916880	28.627700
312.801381	14579.871116	28.632717
313.126669	14594.433155	28.637735
313.829913	14611.484665	28.642752
313.689943	14635.897399	28.647770
314.188093	14650.072367	28.652788
314.484653	14674.078841	28.657805
314.492284	14686.243099	28.662823
315.085937	14703.839280	28.667840
315.361015	14728.799810	28.672858
315.640526	14745.750432	28.677876
315.662391	14768.246210	28.682893
315.932809	14792.667497	28.687911
316.231852	14820.075177	28.692928
316.551953	14852.741220	28.697946
316.750450	14866.881175	28.702964
317.125971	14898.032134	28.707981
317.763124	14922.749864	28.712999
318.174827	14934.705704	28.718016
318.166206	14961.154298	28.723034
318.732973	14986.884303	28.728052
319.110101	15014.188441	28.733069
319.363515	15036.613522	28.738087
319.693891	15042.739375	28.743104
319.344948	15079.726898	28.748122
319.808047	15098.436658	28.753140
320.313409	15125.872465	28.758157
320.551655	15154.629259	28.763175
320.946256	15175.718540	28.768192
321.002742	15190.711611	28.773210
321.619981	15224.629802	28.778228
321.756408	15253.806958	28.783245
322.082020	15275.042962	28.788263
322.308395	15297.962123	28.793280
322.800650	15334.047738	28.798298
323.181465	15342.417667	28.803316
323.874835	15364.069910	28.808333
323.981063	15382.264194	28.813351
324.643908	15401.306169	28.818368
324.484226	15420.969707	28.823386
325.421501	15443.373416	28.828404
325.782813	15464.177663	28.833421
325.792204	15488.688103	28.838439
326.041189	15507.343369	28.843456
326.380432	15528.340644	28.848474
326.488414	15547.747616	28.853492
326.889181	15573.251745	28.858509
327.110481	15593.042124	28.863527
327.274677	15617.282126	28.868544
327.374602	15649.800833	28.873562
328.219640	15676.419896	28.878580
328.131009	15708.753470	28.883597
328.572460	15734.573596	28.888615
328.907627	15751.942772	28.893632
329.319088	15793.584876	28.898650
329.897798	15812.435145	28.903668
330.369652	15844.343202	28.908685
330.616296	15864.262543	28.913703
330.622797	15881.904409	28.918720
331.091964	15913.187637	28.923738
331.331566	15935.830706	28.928756
331.785371	15956.036691	28.933773
332.061288	15992.018463	28.938791
332.768638	16017.291970	28.943808
332.960089	16042.984276	28.948826
333.071248	16070.836930	28.953844
333.685648	16085.001072	28.958861
333.658039	16122.199256	28.963879
333.980316	16142.214425	28.968896
334.035114	16177.100454	28.973914
334.269869	16210.944492	28.978932
334.864067	16247.514893	28.983949
334.700749	16289.011221	28.988967
335.266858	16308.227175	28.993984
335.953001	16344.638069	28.999002
336.748283	16374.803397	29.004020
336.536622	16401.288936	29.009037
336.506492	16431.308860	29.014055
337.547012	16459.799806	29.019072
337.502760	16497.910969	29.024090
338.273786	16514.644030	29.029108
338.758860	16539.021282	29.034125
338.906898	16566.227697	29.039143
339.311561	16584.423748	29.044160
339.381434	16615.960177	29.049178
339.851466	16645.772588	29.054196
340.274803	16661.568461	29.059213
340.628430	16694.156581	29.064231
341.029714	16720.833972	29.069248
341.216968	16746.148847	29.074266
341.630681	16773.266560	29.079284
341.710567	16797.214874	29.084301
342.440700	16817.729081	29.089319
343.111371	16841.616494	29.094336
343.804763	16861.659560	29.099354
343.745588	16884.378973	29.104372
344.279383	16896.026327	29.109389
344.365856	16917.737490	29.114407
344.849462	16933.290411	29.119424
344.901336	16956.024099	29.124442
344.831486	16970.292920	29.129460
345.471978	16997.097469	29.134477
345.818464	17023.834400	29.139495
346.211341	17040.974600	29.144512
346.319447	17074.735759	29.149530
346.612522	17100.672561	29.154548
347.271844	17119.843140	29.159565
347.038439	17143.487194	29.164583
347.663723	17171.778917	29.169600
347.751677	17205.966715	29.174618
348.340580	17231.130870	29.179636
348.992379	17250.353295	29.184653
349.242905	17283.568177	29.189671
349.531280	17305.620868	29.194688
349.975581	17336.992428	29.199706
349.867730	17372.588361	29.204724
350.349951	17397.371453	29.209741
350.857710	17433.686001	29.214759
351.009249	17461.843886	29.219776
351.246959	17494.113536	29.224794
351.637076	17521.728749	29.229812
351.914779	17552.697175	29.234829
351.716712	17586.696706	29.239847
352.778742	17625.079015	29.244864
353.296888	17647.923682	29.249882
353.381365	17688.000684	29.254900
353.935653	17719.823124	29.259917
354.147755	17747.997207	29.264935
354.720478	17785.192995	29.269952
354.909761	17810.553167	29.274970
355.248646	17851.456146	29.279988
355.730362	17881.565554	29.285005
356.222370	17914.250927	29.290023
356.863315	17939.369947	29.295040
356.924504	17967.921768	29.300058
356.768542	18004.107604	29.305076
357.182293	18026.716370	29.310093
357.307854	18065.675833	29.315111
358.091858	18095.207550	29.320128
358.435441	18126.084444	29.325146
358.869692	18166.448792	29.330164
359.739295	18194.394180	29.335181
360.073080	18228.147265	29.340199
360.616662	18240.469880	29.345216
361.064521	18271.425436	29.350234
360.975130	18299.893931	29.355252
361.487101	18323.340534	29.360269
361.670765	18353.093034	29.365287
362.244085	18371.987718	29.370304
362.365598	18412.831164	29.375322
362.809609	18438.626078	29.380340
363.471833	18471.835363	29.385357
363.221840	18505.674056	29.390375
363.635541	18529.913374	29.395392
363.962212	18563.971405	29.400410
364.135231	18602.153751	29.405428
364.670899	18619.178216	29.410445
365.275354	18653.224480	29.415463
365.720438	18690.182969	29.420480
365.978868	18711.926062	29.425498
366.206873	18738.342759	29.430516
366.972986	18764.706790	29.435533
367.189592	18795.484600	29.440551
367.647480	18810.916705	29.445568
368.071454	18836.285677	29.450586
368.529304	18858.446260	29.455604
369.040335	18877.167977	29.460621
369.433416	18893.570604	29.465639
369.810438	18918.719598	29.470656
369.927437	18936.012091	29.475674
370.140977	18961.351011	29.480692
370.827122	18981.290009	29.485709
370.959668	19006.300511	29.490727
371.469406	19036.198831	29.495744
371.910041	19056.353262	29.500762
371.680210	19083.511833	29.505780
372.386680	19102.266332	29.510797
372.790678	19134.588472	29.515815
373.117420	19159.960460	29.520832
373.672779	19184.614339	29.525850
374.039403	19202.701930	29.530868
374.976153	19218.931221	29.535885
375.131322	19254.666295	29.540903
375.822457	19269.594704	29.545920
375.919784	19273.275473	29.550938
376.338633	19299.069151	29.555956
376.395625	19327.453036	29.560973
376.900519	19349.057148	29.565991
377.071655	19379.880910	29.571008
377.493874	19395.293795	29.576026
377.583684	19440.168895	29.581044
378.263950	19456.697598	29.586061
378.768672	19492.593164	29.591079
378.776833	19514.641710	29.596096
379.015497	19545.290887	29.601114
378.803498	19582.227631	29.606132
379.412743	19607.644402	29.611149
380.247293	19645.415583	29.616167
380.454232	19669.827704	29.621184
380.211325	19704.248619	29.626202
380.841467	19744.490779	29.631220
381.581984	19777.993295	29.636237
381.931031	19825.690762	29.641255
382.402700	19857.592822	29.646272
382.594599	19887.428505	29.651290
383.074521	19921.054221	29.656308
383.615689	19952.275827	29.661325
383.893182	19989.338843	29.666343
384.215824	20019.520701	29.671360
384.843071	20045.636538	29.676378
384.893470	20093.861618	29.681396
385.273138	20119.144424	29.686413
385.826035	20159.942902	29.691431
386.035139	20199.980266	29.696448
386.453390	20221.011320	29.701466
387.011718	20255.888973	29.706484
387.364061	20290.154492	29.711501
387.817411	20324.410568	29.716519
388.322411	20364.092324	29.721536
388.566464	20394.925214	29.726554
388.803970	20432.203833	29.731572
389.357045	20469.022404	29.736589
389.629498	20502.245650	29.741607
389.748169	20539.593633	29.746624
390.587164	20573.928741	29.751642
390.487505	20606.825032	29.756660
391.023910	20641.612030	29.761677
391.497505	20686.221356	29.766695
392.045870	20712.318846	29.771712
392.797832	20741.246709	29.776730
393.250402	20770.872307	29.781748
393.862380	20796.492383	29.786765
394.318015	20811.629459	29.791783
394.346749	20834.567159	29.796800
394.632924	20858.159588	29.801818
394.703948	20885.728450	29.806836
395.136701	20917.467730	29.811853
395.827936	20955.503986	29.816871
395.803115	20984.977218	29.821888
396.406951	21014.459438	29.826906
396.354939	21051.563432	29.831924
396.891997	21090.224355	29.836941
397.291912	21119.239511	29.841959
397.485535	21157.884858	29.846976
398.105607	21187.718631	29.851994
398.676631	21223.866038	29.857012
398.928569	21258.256386	29.862029
399.234567	21300.978834	29.867047
399.775662	21338.230570	29.872064
400.483345	21367.210521	29.877082
400.555873	21408.718692	29.882100
400.992090	21443.851367	29.887117
401.423592	21482.839205	29.892135
401.630936	21514.640029	29.897152
402.513723	21549.424923	29.902170
403.121063	21579.236009	29.907188
403.469406	21613.201161	29.912205
404.198761	21645.400648	29.917223
404.202344	21671.679522	29.922240
404.815544	21704.579718	29.927258
404.793666	21735.241522	29.932276
404.996584	21774.828106	29.937293
405.695655	21806.489190	29.942311
406.152321	21842.352343	29.947328
406.351396	21878.477066	29.952346
406.663631	21919.045179	29.957364
407.173509	21955.721642	29.962381
407.521571	21994.338114	29.967399
407.361096	22037.331101	29.972416
408.162075	22070.006609	29.977434
408.222782	22121.653505	29.982452
408.871390	22155.180788	29.987469
409.238268	22202.710604	29.992487
409.976954	22242.460637	29.997504
410.565754	22277.874200	30.002522
411.124691	22314.467817	30.007540
411.576604	22347.211097	30.012557
412.074179	22379.782987	30.017575
412.683686	22418.833252	30.022592
412.965133	22437.998742	30.027610
413.363681	22478.611350	30.032628
414.174557	22501.839202	30.037645
414.556031	22523.630429	30.042663
414.787717	22559.106750	30.047680
415.630957	22584.534951	30.052698
415.999053	22617.860514	30.057716
415.842108	22637.480323	30.062733
416.425512	22670.639551	30.067751
416.744671	22700.611209	30.072768
417.527581	22729.612970	30.077786
417.600332	22768.975484	30.082804
417.934591	22793.845455	30.087821
418.739810	22825.207185	30.092839
418.663356	22858.855547	30.097856
418.992636	22890.683710	30.102874
418.966037	22919.205915	30.107892
419.183359	22945.889012	30.112909
419.909775	22992.884152	30.117927
419.896618	23041.707729	30.122944
420.907785	23075.350394	30.127962
421.403839	23115.304478	30.132980
421.433952	23150.080404	30.137997
422.184314	23180.301201	30.143015
422.395222	23223.895773	30.148032
422.715125	23255.618562	30.153050
422.743779	23300.391941	30.158068
423.327875	23338.215748	30.163085
423.992763	23368.886245	30.168103
424.700643	23406.020955	30.173120
425.461418	23425.952777	30.178138
426.219311	23458.087548	30.183156
426.752177	23489.006403	30.188173
427.354821	23522.789646	30.193191
427.278607	23551.876622	30.198208
427.816001	23573.745686	30.203226
428.570408	23592.067254	30.208244
428.761861	23623.753875	30.213261
429.451919	23658.174545	30.218279
429.828249	23684.524079	30.223296
429.985982	23709.012086	30.228314
430.054651	23740.895067	30.233332
430.182911	23779.498877	30.238349
430.942668	23816.095399	30.243367
430.933346	23850.170952	30.248384
431.510200	23883.870375	30.253402
431.939653	23923.027628	30.258420
432.100013	23968.217911	30.263437
432.556021	23996.090993	30.268455
432.600240	24045.988656	30.273472
433.421642	24095.733114	30.278490
433.632916	24142.912764	30.283508
434.184843	24190.020210	30.288525
434.674611	24235.538668	30.293543
434.836345	24278.201635	30.298560
435.371725	24319.371635	30.303578
436.226250	24360.163115	30.308596
436.318195	24407.488469	30.313613
437.008230	24442.441336	30.318631
437.457542	24505.396112	30.323648
438.130406	24534.373502	30.328666
438.424464	24580.087707	30.333684
438.924644	24626.900944	30.338701
439.542981	24656.190393	30.343719
439.880874	24703.256734	30.348736
440.273763	24736.860015	30.353754
440.546123	24787.368391	30.358772
441.423639	24831.133796	30.363789
441.726321	24865.402349	30.368807
442.001269	24898.082738	30.373824
442.444339	24948.880767	30.378842
442.945715	24991.605805	30.383860
443.201240	25036.751987	30.388877
443.880836	25071.397918	30.393895
444.540068	25112.885094	30.398912
444.847373	25155.078417	30.403930
445.263847	25185.935966	30.408948
445.705718	25229.707277	30.413965
446.505520	25263.563694	30.418983
446.926880	25306.106019	30.424000
447.180336	25332.236810	30.429018
447.967324	25375.859586	30.434036
447.899675	25414.832176	30.439053
448.546637	25439.270945	30.444071
449.343658	25474.423728	30.449088
449.938080	25505.064298	30.454106
450.687877	25542.651438	30.459124
450.702319	25581.327096	30.464141
450.828372	25605.929817	30.469159
451.287032	25633.311803	30.474176
451.788617	25670.735822	30.479194
452.010863	25705.884238	30.484212
451.995586	25744.147744	30.489229
452.468275	25779.945938	30.494247
452.544528	25828.857085	30.499264
453.130015	25872.025856	30.504282
453.276114	25914.031135	30.509300
453.392534	25964.554244	30.514317
454.169626	26011.934051	30.519335
454.800984	26058.616308	30.524352
455.436161	26106.246087	30.529370
456.357574	26150.310849	30.534388
456.415590	26209.742421	30.539405
456.831739	26243.875462	30.544423
457.256799	26303.091814	30.549440
458.048882	26338.329039	30.554458
458.343339	26385.456668	30.559476
458.469653	26443.228661	30.564493
459.247029	26486.223323	30.569511
459.481254	26536.046824	30.574528
460.006524	26578.701956	30.579546
460.322454	26633.733412	30.584564
460.950731	26688.336878	30.589581
461.993017	26732.908560	30.594599
462.539033	26775.491334	30.599616
462.979496	26805.431158	30.604634
463.611709	26860.976198	30.609652
464.020371	26909.686198	30.614669
464.584334	26927.756232	30.619687
465.039308	26972.875496	30.624704
465.391593	27020.431647	30.629722
465.906905	27061.799999	30.634740
466.334430	27103.258031	30.639757
466.943559	27139.132063	30.644775
467.276195	27171.288817	30.649792
467.728735	27226.654425	30.654810
468.410830	27260.128119	30.659828
468.641582	27304.265647	30.664845
468.969920	27340.733895	30.669863
469.952040	27389.235135	30.674880
470.472926	27431.494555	30.679898
470.529583	27469.629955	30.684916
470.788735	27524.337727	30.689933
471.354803	27561.622407	30.694951
471.549598	27607.314755	30.699968
472.027460	27653.032395	30.704986
472.468268	27696.916652	30.710004
472.648228	27753.400884	30.715021
473.474607	27806.421457	30.720039
473.778524	27855.491439	30.725056
474.252905	27895.313021	30.730074
474.869566	27938.917429	30.735092
475.263112	27989.806685	30.740109
476.194295	28042.419575	30.745127
476.977953	28069.994135	30.750144
477.944787	28099.379366	30.755162
478.630832	28127.816267	30.760180
479.199541	28156.221021	30.765197
479.879706	28188.274381	30.770215
480.399346	28206.264005	30.775232
480.617060	28234.673277	30.780250
481.476816	28252.116652	30.785268
481.834528	28299.181917	30.790285
482.029323	28324.086878	30.795303
482.051448	28347.192208	30.800320
482.586932	28378.990414	30.805338
482.788680	28416.592872	30.810356
482.968758	28454.628608	30.815373
483.680040	28490.128733	30.820391
483.873167	28525.665831	30.825408
484.033917	28570.177346	30.830426
484.538980	28610.905719	30.835444
484.785849	28657.824826	30.840461
485.371442	28696.695061	30.845479
485.983793	28737.836703	30.850496
486.521758	28777.567874	30.855514
487.099722	28825.699689	30.860532
487.382728	28863.429299	30.865549
488.034531	28905.924102	30.870567
488.753461	28946.765028	30.875584
488.777434	28994.497294	30.880602
489.570837	29038.303920	30.885620
489.708420	29086.675989	30.890637
490.638521	29136.877240	30.895655
490.572801	29179.048840	30.900672
491.076452	29236.371406	30.905690
491.810964	29278.683357	30.910708
492.071739	29332.997478	30.915725
492.362261	29384.892423	30.920743
492.736437	29432.115734	30.925760
493.223803	29486.401091	30.930778
493.858713	29546.845565	30.935796
494.130200	29606.348393	30.940813
494.707797	29664.273721	30.945831
495.184952	29717.107412	30.950848
495.415098	29782.053457	30.955866
496.162389	29835.319232	30.960884
496.701068	29905.438684	30.965901
497.130193	29955.214697	30.970919
498.000144	30003.486852	30.975936
498.566449	30058.703224	30.980954
499.311414	30105.060873	30.985972
499.997897	30159.386349	30.990989
500.271420	30213.119227	30.996007
500.927404	30267.942831	31.001024
501.371998	30324.563356	31.006042
501.816023	30373.743833	31.011060
502.296967	30426.762067	31.016077
502.736075	30469.900267	31.021095
503.364313	30521.011886	31.026112
503.897152	30575.387805	31.031130
504.735085	30616.953017	31.036148
504.976345	30673.429342	31.041165
505.302140	30717.047274	31.046183
505.991627	30767.555686	31.051200
506.655499	30836.685173	31.056218
507.027717	30870.289154	31.061236
507.618755	30922.014459	31.066253
508.344421	30974.856691	31.071271
508.523238	31020.616013	31.076288
508.990566	31080.730889	31.081306
509.183431	31129.724919	31.086324
509.989884	31181.082083	31.091341
510.612727	31243.031636	31.096359
511.122350	31278.650335	31.101376
511.546533	31348.678815	31.106394
511.907723	31388.480629	31.111412
512.756608	31451.558595	31.116429
513.181919	31497.021167	31.121447
514.016195	31536.970430	31.126464
514.103665	31578.749937	31.131482
514.432507	31635.189871	31.136500
514.865772	31691.360730	31.141517
515.190661	31748.414805	31.146535
515.711933	31794.665868	31.151552
516.475276	31844.318206	31.156570
516.916726	31886.706683	31.161588
517.876727	31937.036489	31.166605
518.285602	31973.335955	31.171623
519.191253	32022.941143	31.176640
519.390801	32078.334125	31.181658
519.817533	32118.841446	31.186676
520.194486	32170.495912	31.191693
520.480523	32206.562145	31.196711
521.193398	32257.190631	31.201728
521.402503	32318.367359	31.206746
521.785121	32374.579600	31.211764
522.163526	32438.360119	31.216781
522.576347	32496.831244	31.221799
523.183285	32550.764498	31.226816
523.838488	32615.039578	31.231834
524.171346	32675.072635	31.236852
524.567572	32734.982141	31.241869
525.323761	32789.575423	31.246887
525.942136	32851.125834	31.251904
526.312484	32920.738109	31.256922
526.504095	32984.726568	31.261940
527.036188	33062.621345	31.266957
527.527561	33122.814201	31.271975
528.258535	33184.512332	31.276992
529.374815	33233.575301	31.282010
530.277897	33282.418886	31.287028
530.935966	33353.030708	31.292045
531.506719	33408.141462	31.297063
532.151457	33453.061811	31.302080
532.180381	33514.523140	31.307098
532.906156	33567.340306	31.312116
533.522819	33630.220966	31.317133
534.219909	33680.330605	31.322151
534.671399	33726.331324	31.327168
534.828721	33781.229621	31.332186
535.483577	33829.114410	31.337204
536.536868	33886.205636	31.342221
537.271397	33938.718885	31.347239
537.815150	33973.186138	31.352256
538.120294	34023.029210	31.357274
538.610424	34079.760265	31.362292
539.344365	34136.042323	31.367309
540.071942	34191.750174	31.372327
540.738340	34229.037464	31.377344
541.453480	34281.731638	31.382362
541.872544	34333.814764	31.387380
542.272210	34378.339211	31.392397
542.325709	34430.574670	31.397415
543.288994	34474.600075	31.402432
543.516127	34532.827746	31.407450
543.797084	34579.128908	31.412468
544.157678	34627.548443	31.417485
544.585835	34691.934977	31.422503
545.193067	34746.284790	31.427520
545.618387	34816.779898	31.432538
545.694443	34890.864366	31.437556
546.329594	34953.341414	31.442573
546.511722	35017.027703	31.447591
547.432775	35081.603781	31.452608
547.825901	35148.678065	31.457626
548.163505	35219.485422	31.462644
548.927007	35288.835276	31.467661
549.372836	35356.104293	31.472679
550.394093	35425.483777	31.477696
550.720271	35493.827897	31.482714
551.790220	35542.245911	31.487732
552.480956	35585.886354	31.492749
553.009076	35636.254720	31.497767
553.620244	35693.091275	31.502784
554.197699	35742.668114	31.507802
554.789833	35797.661608	31.512820
555.736189	35846.055411	31.517837
555.705949	35907.811160	31.522855
556.493647	35960.169342	31.527872
556.729199	36013.613179	31.532890
557.076570	36077.371607	31.537908
557.839754	36127.685350	31.542925
558.463211	36184.445414	31.547943
558.912180	36227.454785	31.552960
559.212498	36299.042996	31.557978
559.972226	36351.564600	31.562996
560.748501	36413.069030	31.568013
561.033844	36472.974869	31.573031
561.618528	36533.896300	31.578048
562.054668	36603.864477	31.583066
562.923940	36655.825871	31.588084
563.672292	36717.822445	31.593101
563.946110	36779.324420	31.598119
564.935298	36832.728152	31.603136
565.446090	36892.068694	31.608154
565.758099	36954.893096	31.613172
566.422138	37007.387035	31.618189
566.805425	37078.338842	31.623207
567.055694	37128.564541	31.628224
567.797493	37187.819135	31.633242
568.270774	37266.389868	31.638260
569.095842	37324.392398	31.643277
569.260355	37403.182723	31.648295
570.191185	37460.884500	31.653312
570.734910	37517.066174	31.658330
570.976799	37591.361679	31.663348
571.737278	37656.217318	31.668365
572.347848	37723.392098	31.673383
572.987526	37795.893342	31.678400
573.336732	37870.640952	31.683418
574.276399	37936.468507	31.688436
574.804400	38002.227940	31.693453
575.150647	38067.876918	31.698471
575.781219	38133.709220	31.703488
576.159300	38197.083389	31.708506
576.726123	38264.633484	31.713524
577.650089	38337.427185	31.718541
578.034163	38404.279104	31.723559
578.914458	38473.842319	31.728576
579.354073	38547.680130	31.733594
579.794844	38615.345922	31.738612
580.484323	38687.039230	31.743629
581.238615	38748.035229	31.748647
581.765773	38810.799726	31.753664
582.240266	38878.865791	31.758682
582.933728	38947.764158	31.763700
583.988757	39006.645851	31.768717
584.145554	39074.281664	31.773735
584.961714	39138.222379	31.778752
585.511051	39201.300735	31.783770
585.787487	39269.228295	31.788788
586.623896	39339.914201	31.793805
586.839762	39410.918866	31.798823
587.385767	39478.096561	31.803840
587.917999	39549.640274	31.808858
588.339547	39620.588115	31.813876
589.254087	39684.875510	31.818893
589.523822	39764.069022	31.823911
590.085676	39830.480096	31.828928
590.972669	39900.932232	31.833946
591.354644	39972.899295	31.838964
591.699747	40034.032560	31.843981
592.019014	40100.469801	31.848999
592.962978	40172.064913	31.854016
593.641193	40244.492423	31.859034
594.184914	40318.427461	31.864052
595.075984	40387.204575	31.869069
595.558337	40452.504256	31.874087
596.165277	40504.775300	31.879104
596.802048	40580.682518	31.884122
597.115831	40658.107858	31.889140
597.837033	40724.452425	31.894157
598.411967	40797.384927	31.899175
598.865354	40865.245473	31.904192
600.042853	40931.405364	31.909210
600.201841	41003.707997	31.914228
601.212808	41069.761573	31.919245
601.781794	41144.308929	31.924263
602.382253	41207.435677	31.929280
603.196045	41268.549586	31.934298
603.566675	41345.228467	31.939316
604.449492	41406.129560	31.944333
604.899457	41479.147149	31.949351
605.483097	41539.437699	31.954368
606.867326	41606.142802	31.959386
606.997920	41672.557436	31.964404
607.836195	41737.558537	31.969421
608.201722	41806.858826	31.974439
608.630449	41869.558988	31.979456
609.423430	41935.421616	31.984474
609.788919	42007.809057	31.989492
610.186844	42079.736265	31.994509
610.813216	42153.784716	31.999527
611.427924	42230.124859	32.004544
611.935114	42303.376565	32.009562
612.487291	42383.268991	32.014580
613.310487	42453.144778	32.019597
613.926009	42537.752597	32.024615
614.123305	42619.776056	32.029632
614.697543	42689.482855	32.034650
615.342750	42773.985727	32.039668
616.156245	42844.825682	32.044685
616.951779	42936.136722	32.049703
617.528609	43004.971244	32.054720
618.305393	43084.413567	32.059738
618.949684	43161.757992	32.064756
619.615705	43230.427441	32.069773
620.185351	43302.053420	32.074791
621.079406	43366.405408	32.079808
621.907914	43430.888028	32.084826
622.499702	43507.198213	32.089844
623.263477	43575.341073	32.094861
623.770104	43645.491586	32.099879
624.122143	43711.776452	32.104896
624.952990	43778.049782	32.109914
625.290639	43850.789173	32.114932
626.077401	43919.359612	32.119949
626.775166	43996.736520	32.124967
627.472445	44066.934408	32.129984
627.973693	44121.242063	32.135002
628.618309	44204.447428	32.140020
629.620898	44266.526831	32.145037
630.106406	44337.726537	32.150055
630.926050	44404.560131	32.155072
631.707218	44472.772594	32.160090
631.762645	44534.109175	32.165108
632.798434	44600.251646	32.170125
633.723698	44647.827015	32.175143
634.296168	44713.466753	32.180160
634.719903	44761.367607	32.185178
634.721157	44827.128763	32.190196
635.811965	44888.051138	32.195213
636.045335	44961.968074	32.200231
636.215946	45027.848787	32.205248
637.366786	45103.570821	32.210266
637.713722	45180.975145	32.215284
638.212485	45241.599005	32.220301
639.264726	45324.295568	32.225319
639.589989	45386.218473	32.230336
640.754114	45452.590071	32.235354
641.134788	45525.233280	32.240372
641.881429	45587.432344	32.245389
642.415423	45649.335937	32.250407
643.171209	45738.349398	32.255424
643.911832	45803.580111	32.260442
644.189139	45869.098653	32.265460
645.115125	45940.683607	32.270477
645.631705	46014.243352	32.275495
646.089002	46089.988764	32.280512
646.968752	46161.727160	32.285530
647.318799	46241.968702	32.290548
648.155589	46324.911445	32.295565
648.473829	46400.913742	32.300583
648.813485	46484.763644	32.305600
649.537535	46565.580375	32.310618
649.932303	46652.591661	32.315636
650.400478	46730.652891	32.320653
651.242882	46829.026163	32.325671
652.127586	46917.106782	32.330688
652.846907	46999.678169	32.335706
652.825189	47090.773535	32.340724
654.186815	47170.752401	32.345741
655.378399	47250.252074	32.350759
655.803338	47335.787224	32.355776
656.761178	47411.642134	32.360794
657.048343	47498.717802	32.365812
657.473310	47585.924055	32.370829
658.445743	47674.702435	32.375847
659.268356	47756.039393	32.380864
660.198680	47838.428950	32.385882
660.151055	47924.647662	32.390900
661.216290	48005.232618	32.395917
661.811741	48090.370633	32.400935
662.259616	48174.734928	32.405952
663.262741	48252.002702	32.410970
663.677150	48348.760373	32.415988
664.082903	48436.200646	32.421005
664.736887	48515.535865	32.426023
664.819209	48610.733348	32.431040
666.117815	48706.974461	32.436058
666.767036	48798.427096	32.441076
667.545830	48879.426947	32.446093
668.345651	48975.076662	32.451111
669.129055	49050.306352	32.456128
669.816555	49133.086581	32.461146
670.167732	49222.759124	32.466164
670.946070	49303.842796	32.471181
671.876483	49397.341656	32.476199
672.754460	49475.885891	32.481216
673.440395	49549.367264	32.486234
675.156348	49604.813853	32.491252
676.753611	49662.715056	32.496269
677.515387	49711.686973	32.501287
678.031973	49783.278534	32.506304
678.725111	49827.788241	32.511322
679.363191	49883.195511	32.516340
679.781468	49919.460003	32.521357
680.985830	49981.036293	32.526375
681.010682	50028.396997	32.531392
681.990073	50079.455194	32.536410
682.262783	50137.109473	32.541428
682.818340	50193.068217	32.546445
683.522501	50249.503671	32.551463
683.674190	50318.534596	32.556480
684.290841	50375.167549	32.561498
684.767674	50441.680320	32.566516
685.266384	50518.136254	32.571533
685.708774	50591.684400	32.576551
686.089709	50664.432513	32.581568
686.448462	50750.186905	32.586586
686.872631	50844.720008	32.591604
687.209859	50926.707344	32.596621
687.794803	51014.989863	32.601639
687.807186	51116.074105	32.606656
688.923603	51218.333630	32.611674
689.330880	51312.725753	32.616692
689.846276	51421.989864	32.621709
690.929148	51524.350901	32.626727
691.215515	51638.486106	32.631744
692.276009	51740.516239	32.636762
693.024710	51844.120595	32.641780
693.957995	51954.011466	32.646797
694.722113	52052.571224	32.651815
695.463484	52161.835052	32.656832
696.295018	52250.583526	32.661850
696.875202	52349.736507	32.666868
697.788152	52461.246518	32.671885
698.852168	52554.161365	32.676903
699.186420	52646.874474	32.681920
700.316232	52745.683620	32.686938
701.707167	52833.903754	32.691956
702.416235	52928.786686	32.696973
703.155774	53008.699738	32.701991
703.367886	53097.402882	32.707008
704.281726	53190.445017	32.712026
704.629183	53278.248062	32.717044
705.826866	53364.678001	32.722061
706.364624	53461.108629	32.727079
706.781572	53553.856662	32.732096
707.955261	53641.905030	32.737114
708.458194	53740.120441	32.742132
708.741386	53843.914110	32.747149
709.697447	53943.217454	32.752167
710.707786	54028.059159	32.757184
711.304564	54117.319734	32.762202
712.196357	54210.287083	32.767220
712.047190	54306.259196	32.772237
712.960583	54405.868594	32.777255
713.706984	54516.825897	32.782272
714.358119	54602.649849	32.787290
715.157953	54707.714334	32.792308
715.931594	54817.485376	32.797325
716.442806	54911.647858	32.802343
717.120047	55020.036354	32.807360
718.290332	55108.154000	32.812378
718.927450	55200.563911	32.817396
719.421087	55293.806699	32.822413
720.648687	55395.782211	32.827431
721.538243	55503.627051	32.832448
722.110654	55598.731953	32.837466
722.884303	55686.635397	32.842484
723.257373	55782.582312	32.847501
723.891285	55871.989224	32.852519
724.525243	55961.738212	32.857536
725.425583	56048.053633	32.862554
726.304323	56134.613240	32.867572
726.602084	56234.681111	32.872589
727.169721	56321.752113	32.877607
728.064723	56413.613705	32.882624
729.055265	56513.764117	32.887642
729.622055	56594.380832	32.892660
730.340276	56689.657103	32.897677
731.271263	56783.482760	32.902695
731.628096	56891.316017	32.907712
731.990991	56990.895843	32.912730
733.489241	57085.386992	32.917748
733.870872	57185.743155	32.922765
734.232871	57272.514369	32.927783
735.021412	57393.041607	32.932800
736.494175	57480.120634	32.937818
737.244322	57578.629592	32.942836
737.495719	57684.242402	32.947853
738.771216	57772.309078	32.952871
739.508477	57871.688345	32.957888
739.831274	57980.601436	32.962906
740.996891	58070.180101	32.967924
741.386896	58175.735376	32.972941
742.368736	58277.540097	32.977959
742.871184	58388.097821	32.982976
743.505847	58482.160039	32.987994
744.370355	58587.047839	32.993012
744.707784	58701.088671	32.998029
745.490831	58804.768592	33.003047
745.790974	58914.752767	33.008064
746.543338	59025.666682	33.013082
747.757575	59143.135785	33.018100
748.364971	59257.390127	33.023117
749.201032	59373.672640	33.028135
749.417814	59488.824739	33.033152
750.454973	59602.975422	33.038170
751.363758	59717.349291	33.043188
751.831014	59835.609647	33.048205
752.810968	59936.142999	33.053223
753.375872	60060.649252	33.058240
754.416425	60177.080796	33.063258
755.808756	60286.539315	33.068276
756.681188	60395.465741	33.073293
757.167032	60504.510157	33.078311
758.118934	60614.368262	33.083328
759.070825	60722.536767	33.088346
760.177918	60820.692772	33.093364
760.932151	60914.669668	33.098381
761.774264	61015.956977	33.103399
762.453012	61110.940254	33.108416
763.060470	61218.728103	33.113434
763.839565	61315.861335	33.118452
764.415046	61423.155008	33.123469
765.168226	61526.578927	33.128487
765.996057	61636.271111	33.133504
766.667437	61740.436702	33.138522
767.690244	61845.244024	33.143540
768.009584	61945.281331	33.148557
768.958746	62059.014074	33.153575
769.862767	62165.056762	33.158592
769.899055	62280.699626	33.163610
770.819264	62394.343485	33.168628
771.715224	62495.039692	33.173645
772.370662	62605.776020	33.178663
773.155208	62724.323378	33.183680
773.561326	62840.778200	33.188698
774.580333	62950.686811	33.193716
775.058515	63063.124179	33.198733
776.210419	63172.417887	33.203751
777.026163	63272.009287	33.208768
777.173387	63391.843435	33.213786
778.206313	63492.003110	33.218804
779.078557	63606.255082	33.223821
780.260865	63716.679597	33.228839
780.780779	63820.035620	33.233856
781.347108	63934.140738	33.238874
782.231465	64025.057597	33.243892
782.730554	64143.428473	33.248909
783.619871	64259.250784	33.253927
784.881900	64370.172158	33.258944
785.717913	64486.466015	33.263962
786.503631	64591.182711	33.268980
786.728610	64702.945353	33.273997
787.389150	64822.072842	33.279015
788.298070	64938.705571	33.284032
789.017406	65063.174687	33.289050
790.209106	65178.156158	33.294068
791.189808	65302.541207	33.299085
791.591395	65423.851990	33.304103
792.620500	65542.564285	33.309120
792.879568	65663.531325	33.314138
794.402843	65774.734518	33.319156
795.319073	65893.580093	33.324173
796.267990	66007.235797	33.329191
796.943935	66121.415933	33.334208
797.351514	66249.250953	33.339226
798.730500	66342.219686	33.344244
799.535233	66469.195869	33.349261
800.167741	66577.863888	33.354279
801.159989	66686.146802	33.359296
801.804065	66816.391565	33.364314
802.776144	66926.774373	33.369332
803.184879	67045.020983	33.374349
803.919904	67161.874755	33.379367
804.644766	67276.710877	33.384384
805.464872	67412.540888	33.389402
806.341835	67533.527667	33.394420
806.941432	67662.935255	33.399437
807.577432	67778.857590	33.404455
808.469204	67906.783356	33.409472
809.310703	68034.679640	33.414490
810.360703	68158.662516	33.419508
811.224501	68264.331847	33.424525
812.415694	68388.787603	33.429543
813.473732	68506.185764	33.434560
813.848430	68633.670558	33.439578
814.683721	68752.542062	33.444596
815.621800	68868.308014	33.449613
816.551983	68989.128657	33.454631
817.262882	69107.065134	33.459648
817.998811	69224.808266	33.464666
818.719874	69350.368057	33.469684
819.667850	69468.307044	33.474701
820.475933	69585.337646	33.479719
821.744238	69702.708300	33.484736
822.234824	69821.125768	33.489754
823.274378	69941.648763	33.494772
823.937560	70067.379381	33.499789
824.650734	70184.262894	33.504807
825.240799	70301.482825	33.509824
826.203604	70434.539112	33.514842
827.239899	70550.879744	33.519860
827.832858	70671.786325	33.524877
828.942411	70781.771438	33.529895
829.417118	70893.300224	33.534912
830.269922	71018.993053	33.539930
830.895147	71125.255950	33.544948
831.772006	71254.011076	33.549965
832.456657	71363.951176	33.554983
833.640333	71470.621963	33.560000
833.831477	71602.905773	33.565018
835.064944	71719.208040	33.570036
835.672855	71824.450577	33.575053
836.369585	71955.833738	33.580071
836.869085	72086.171867	33.585088
837.563865	72218.886516	33.590106
838.927119	72346.506901	33.595124
839.627533	72479.145978	33.600141
840.151781	72618.475487	33.605159
841.495797	72736.031489	33.610176
842.236579	72861.471976	33.615194
843.455214	72988.636792	33.620212
844.556143	73116.491945	33.625229
845.511872	73240.266648	33.630247
846.177290	73362.554786	33.635264
846.568604	73495.221996	33.640282
847.354217	73626.916154	33.645300
848.155607	73761.889060	33.650317
849.022186	73893.318526	33.655335
850.159085	74025.402962	33.660352
850.696470	74157.442593	33.665370
851.399359	74294.257578	33.670388
852.184479	74433.859705	33.675405
853.050934	74570.308485	33.680423
854.163118	74705.440139	33.685440
854.571518	74856.427514	33.690458
855.731777	74987.867016	33.695476
856.760814	75122.507106	33.700493
857.533089	75270.653096	33.705511
858.569991	75402.481275	33.710528
859.806902	75532.872728	33.715546
860.489462	75679.033596	33.720564
861.458039	75816.410055	33.725581
862.236228	75954.919079	33.730599
863.396732	76076.939346	33.735616
863.821392	76225.550341	33.740634
864.611234	76369.582661	33.745652
865.569065	76497.539615	33.750669
866.609806	76635.972991	33.755687
867.832220	76765.802589	33.760704
868.375992	76910.978389	33.765722
869.156871	77050.619993	33.770740
870.504170	77194.290685	33.775757
870.886306	77328.662958	33.780775
871.821913	77473.615702	33.785792
872.810742	77609.313172	33.790810
873.848407	77731.626098	33.795828
874.760009	77871.302084	33.800845
875.082994	78013.921309	33.805863
876.200174	78152.667085	33.810880
877.012610	78292.044024	33.815898
877.981040	78434.196973	33.820916
878.798946	78566.948834	33.825933
879.468365	78718.474105	33.830951
880.464870	78858.686545	33.835968
881.283327	79003.691015	33.840986
882.026402	79143.805223	33.846004
882.934435	79288.125708	33.851021
884.088137	79445.090073	33.856039
884.703266	79577.093047	33.861056
885.709032	79724.213008	33.866074
886.433262	79876.686193	33.871092
887.583837	80016.297568	33.876109
887.819756	80161.095222	33.881127
888.886462	80283.554228	33.886144
889.836444	80415.863477	33.891162
891.055992	80559.052195	33.896180
892.056784	80698.132972	33.901197
893.064317	80828.471386	33.906215
894.321029	80950.700845	33.911232
895.252622	81074.261379	33.916250
896.180103	81204.766110	33.921268
897.006453	81341.014025	33.926285
897.503190	81472.512336	33.931303
898.730900	81602.921222	33.936320
899.722022	81736.915345	33.941338
900.759837	81856.661688	33.946356
901.483233	81978.675032	33.951373
902.571561	82120.840623	33.956391
903.394487	82256.257258	33.961408
904.314277	82388.466466	33.966426
905.311158	82515.304677	33.971444
906.315132	82651.619782	33.976461
906.469696	82797.482674	33.981479
907.403122	82926.537311	33.986496
908.129320	83078.267267	33.991514
909.178059	83221.850995	33.996532
909.833318	83364.521413	34.001549
910.436519	83520.137535	34.006567
911.637412	83659.632324	34.011584
912.546918	83815.506190	34.016602
913.526306	83960.650332	34.021620
915.123819	84111.628460	34.026637
915.705004	84254.112166	34.031655
916.418973	84395.105932	34.036672
917.912433	84538.766004	34.041690
918.525932	84685.884447	34.046708
919.546174	84825.514551	34.051725
920.304354	84979.188257	34.056743
921.482881	85124.408452	34.061760
922.344197	85280.424501	34.066778
922.745774	85423.043466	34.071796
924.117061	85583.631772	34.076813
925.008520	85737.022522	34.081831
926.059807	85881.303377	34.086848
926.540773	86036.774795	34.091866
927.515765	86192.157016	34.096884
928.415188	86335.247392	34.101901
929.322056	86505.176723	34.106919
930.487125	86661.089249	34.111936
930.894803	86812.622563	34.116954
932.026724	86973.344704	34.121972
933.067451	87121.194240	34.126989
933.720075	87289.964057	34.132007
934.856560	87453.209917	34.137024
935.793539	87608.149387	34.142042
936.453484	87770.901356	34.147060
937.415164	87930.223373	34.152077
938.288261	88087.785934	34.157095
939.185722	88253.836305	34.162112
940.120447	88421.073024	34.167130
941.079491	88592.590338	34.172148
942.431503	88760.181839	34.177165
943.161810	88925.932643	34.182183
944.021978	89075.429704	34.187200
944.810019	89238.854019	34.192218
945.922675	89418.070039	34.197236
946.967362	89574.080137	34.202253
947.911103	89748.749497	34.207271
948.960615	89905.888507	34.212288
950.570256	90059.911651	34.217306
951.294483	90195.304552	34.222324
952.767020	90338.806128	34.227341
953.885626	90480.412046	34.232359
954.416170	90619.056315	34.237376
955.534983	90759.839716	34.242394
956.118302	90906.081368	34.247412
957.187932	91042.868824	34.252429
958.117566	91187.359298	34.257447
959.014046	91331.488102	34.262464
960.271899	91484.623049	34.267482
960.996247	91626.739664	34.272500
962.003455	91767.976152	34.277517
962.851289	91919.098902	34.282535
963.808072	92072.588136	34.287552
964.919018	92215.027201	34.292570
965.740368	92373.114641	34.297588
966.987239	92525.077809	34.302605
967.858151	92674.400891	34.307623
968.680570	92825.215237	34.312640
969.715690	92967.073965	34.317658
970.618478	93125.380684	34.322676
971.827923	93279.558879	34.327693
972.128901	93453.260151	34.332711
973.154130	93604.185990	34.337728
974.100555	93760.866737	34.342746
974.858133	93935.589292	34.347764
975.979472	94097.390488	34.352781
976.794328	94262.117815	34.357799
978.300794	94422.935113	34.362816
979.220713	94587.508290	34.367834
979.746929	94758.202882	34.372852
980.953087	94925.534323	34.377869
981.757684	95095.768884	34.382887
982.840252	95264.211600	34.387904
984.215697	95425.586974	34.392922
985.256547	95596.180222	34.397940
986.483009	95747.072286	34.402957
987.372653	95918.502222	34.407975
988.374009	96084.224049	34.412992
988.985216	96250.210652	34.418010
989.372195	96418.489601	34.423028
991.221397	96585.894018	34.428045
992.137306	96764.220337	34.433063
992.624196	96945.669848	34.438080
993.734489	97110.429278	34.443098
994.628704	97289.573246	34.448116
995.363698	97464.471134	34.453133
996.515407	97649.268618	34.458151
997.281368	97820.766261	34.463168
998.561763	97996.912741	34.468186
999.390325	98187.798114	34.473204
1000.957423	98364.560932	34.478221
1002.035349	98541.667534	34.483239
1002.517894	98727.564835	34.488256
1003.765187	98900.716995	34.493274
1004.399114	99085.920775	34.498292
1005.324715	99260.925411	34.503309
1006.563033	99443.032088	34.508327
1007.659682	99622.347575	34.513344
1008.748650	99808.866104	34.518362
1009.345120	99998.023695	34.523380
1010.740518	100171.539810	34.528397
1011.646254	100360.955359	34.533415
1012.768239	100557.222217	34.538432
1014.076892	100723.553849	34.543450
1015.007560	100912.195347	34.548468
1015.534136	101088.857057	34.553485
1016.363844	101270.302621	34.558503
1017.689729	101451.709540	34.563520
1018.981646	101617.591923	34.568538
1019.515934	101795.638161	34.573556
1020.930465	101967.626740	34.578573
1021.933256	102144.637955	34.583591
1022.628058	102307.637867	34.588608
1023.406351	102488.274092	34.593626
1024.428437	102675.782997	34.598644
1025.535548	102851.184150	34.603661
1026.778876	103037.329195	34.608679
1027.593654	103225.507602	34.613696
1028.977161	103393.400492	34.618714
1029.604926	103578.643304	34.623732
1030.528022	103764.525573	34.628749
1032.087964	103945.820753	34.633767
1032.660285	104137.402228	34.638784
1033.952890	104336.555669	34.643802
1034.373934	104521.278166	34.648820
1035.628572	104716.344370	34.653837
1036.771430	104905.178210	34.658855
1038.108625	105092.676685	34.663872
1039.813371	105274.996081	34.668890
1040.976197	105457.084312	34.673908
1041.776047	105639.965776	34.678925
1043.061226	105825.270168	34.683943
1043.785419	106009.712406	34.688960
1044.790196	106190.764198	34.693978
1045.770386	106388.723302	34.698996
1046.481317	106580.778731	34.704013
1047.523861	106772.834039	34.709031
1048.582116	106964.900642	34.714048
1049.607490	107160.333755	34.719066
1050.425514	107361.608067	34.724084
1051.340613	107565.860950	34.729101
1052.712344	107764.565548	34.734119
1053.469425	107973.271092	34.739136
1054.892958	108170.841334	34.744154
1055.839763	108364.670426	34.749172
1056.762256	108569.688912	34.754189
1058.177502	108766.667837	34.759207
1058.973210	108970.909634	34.764224
1060.558135	109158.695847	34.769242
1061.668587	109363.169639	34.774260
1063.295424	109548.529283	34.779277
1064.531550	109743.157681	34.784295
1065.452902	109941.514027	34.789312
1066.667847	110137.644320	34.794330
1067.568361	110332.074884	34.799348
1068.621706	110511.822713	34.804365
1069.743475	110701.946986	34.809383
1070.692022	110893.748016	34.814400
1072.371002	111082.595012	34.819418
1073.343686	111283.829592	34.824436
1074.220865	111472.055954	34.829453
1075.311273	111654.809363	34.834471
1076.259686	111850.813288	34.839488
1077.488065	112033.572393	34.844506
1078.287420	112221.662692	34.849524
1079.293738	112416.392421	34.854541
1080.578997	112617.585550	34.859559
1081.577255	112812.965480	34.864576
1082.561024	112996.439930	34.869594
1083.745305	113193.872710	34.874612
1084.579367	113390.955553	34.879629
1085.942281	113575.958895	34.884647
1086.589544	113779.896346	34.889664
1087.122169	113975.063721	34.894682
1088.420671	114181.742399	34.899700
1089.467526	114374.726047	34.904717
1090.365884	114567.252006	34.909735
1091.103304	114772.575995	34.914752
1092.243184	114960.779333	34.919770
1092.827580	115173.409617	34.924788
1093.931690	115378.933236	34.929805
1095.215087	115579.762464	34.934823
1096.139624	115798.773533	34.939840
1097.614821	115998.319342	34.944858
1098.645177	116206.763604	34.949876
1099.460773	116411.653193	34.954893
1100.882094	116628.168791	34.959911
1101.928164	116843.970681	34.964928
1102.937349	117055.200727	34.969946
1104.177562	117265.469865	34.974964
1105.287877	117482.838167	34.979981
1106.491429	117688.967750	34.984999
1107.211980	117912.246883	34.990016
1108.358687	118116.713392	34.995034
1110.310602	118336.453621	35.000052
1111.580400	118548.361523	35.005069
1112.276215	118761.311793	35.010087
1113.075058	118983.481411	35.015104
1114.504100	119200.708162	35.020122
1115.569912	119417.231932	35.025140
1116.545089	119640.240300	35.030157
1117.998273	119854.879293	35.035175
1119.131301	120080.389760	35.040192
1120.335781	120297.772019	35.045210
1121.224586	120514.469188	35.050228
1121.895393	120743.506187	35.055245
1123.291454	120961.826231	35.060263
1124.303355	121191.560884	35.065280
1125.284577	121419.373528	35.070298
1127.296879	121651.757709	35.075316
1128.664378	121867.867345	35.080333
1130.117059	122076.822909	35.085351
1131.262409	122301.101093	35.090368
1132.412996	122511.476291	35.095386
1133.480126	122714.825119	35.100404
1134.659160	122939.812044	35.105421
1135.604174	123147.584160	35.110439
1136.659247	123372.504136	35.115456
1137.898114	123581.640643	35.120474
1138.858893	123813.035010	35.125492
1139.837848	124034.355102	35.130509
1140.848390	124248.922426	35.135527
1141.874939	124479.714083	35.140544
1143.252619	124698.514270	35.145562
1144.732243	124927.461471	35.150580
1145.956226	125150.119446	35.155597
1147.218688	125369.042781	35.160615
1148.153602	125597.584256	35.165632
1148.976318	125818.862434	35.170650
1149.954366	126045.128746	35.175668
1151.157289	126274.241004	35.180685
1152.279084	126496.820816	35.185703
1153.351825	126739.150385	35.190720
1154.581694	126958.772399	35.195738
1156.122171	127179.894776	35.200756
1157.032396	127419.158119	35.205773
1158.213033	127641.265447	35.210791
1159.124015	127874.733230	35.215808
1160.691987	128099.941495	35.220826
1161.675745	128335.595368	35.225844
1162.668647	128565.463634	35.230861
1164.100661	128797.370547	35.235879
1165.282418	129005.706230	35.240896
1166.733608	129227.728843	35.245914
1167.764855	129442.116891	35.250932
1168.948430	129656.342608	35.255949
1169.959710	129868.058798	35.260967
1171.055919	130087.362824	35.265984
1171.993307	130305.627045	35.271002
1173.350414	130519.969494	35.276020
1174.130636	130752.839196	35.281037
1175.196116	130968.193831	35.286055
1176.040419	131203.415940	35.291072
1177.547884	131423.753587	35.296090
1178.835376	131668.450475	35.301108
1179.546906	131897.492497	35.306125
1180.654429	132122.717918	35.311143
1181.754616	132372.967599	35.316160
1183.187323	132604.235129	35.321178
1184.474635	132838.178587	35.326196
1185.728253	133077.077202	35.331213
1187.198771	133314.192088	35.336231
1188.582008	133555.763043	35.341248
1189.999161	133776.900672	35.346266
1191.650991	134010.247631	35.351284
1192.125753	134240.874261	35.356301
1193.541647	134477.509019	35.361319
1194.993881	134708.251508	35.366336
1196.174705	134943.859624	35.371354
1197.526168	135180.635063	35.376372
1197.878002	135423.697252	35.381389
1199.560853	135643.393945	35.386407
1201.177359	135881.666991	35.391424
1202.260502	136115.443804	35.396442
1203.900003	136344.820205	35.401460
1204.975046	136579.323972	35.406477
1206.399089	136817.961961	35.411495
1207.383669	137053.802056	35.416512
1208.486997	137283.901575	35.421530
1209.801203	137522.585780	35.426548
1210.718922	137762.526154	35.431565
1212.765014	137990.007012	35.436583
1213.996298	138218.416021	35.441600
1214.766452	138448.979545	35.446618
1215.908408	138678.597670	35.451636
1217.116832	138918.739580	35.456653
1218.017037	139154.590808	35.461671
1219.399674	139396.560689	35.466688
1220.235485	139645.343446	35.471706
1221.613378	139876.161441	35.476724
1222.598532	140128.692480	35.481741
1224.399051	140364.675274	35.486759
1225.413575	140608.041463	35.491776
1226.139939	140864.259172	35.496794
1227.700346	141110.537511	35.501812
1228.981571	141359.043675	35.506829
1230.041529	141602.065096	35.511847
1231.500984	141853.007968	35.516864
1232.764600	142088.105991	35.521882
1234.345249	142328.054373	35.526900
1235.413534	142568.274504	35.531917
1236.475435	142821.277115	35.536935
1238.208845	143064.238431	35.541952
1239.283651	143300.514035	35.546970
1240.161593	143534.600540	35.551988
1241.382254	143799.297680	35.557005
1242.793210	144037.567521	35.562023
1244.161053	144281.950020	35.567040
1245.162756	144530.084365	35.572058
1246.495464	144772.824797	35.577076
1247.551654	145029.634371	35.582093
1248.902169	145251.876685	35.587111
1250.042363	145486.768883	35.592128
1251.158322	145726.197070	35.597146
1252.331833	145962.126996	35.602164
1253.140608	146208.878188	35.607181
1254.461137	146459.294704	35.612199
1255.349976	146701.479152	35.617216
1256.799255	146957.259517	35.622234
1258.573748	147183.949645	35.627252
1260.012277	147426.812974	35.632269
1260.979422	147677.468370	35.637287
1262.248581	147923.889080	35.642304
1263.650146	148172.232214	35.647322
1264.939076	148418.360203	35.652340
1266.042997	148674.304536	35.657357
1267.380998	148914.106068	35.662375
1268.527470	149168.573729	35.667392
1269.995539	149427.929871	35.672410
1271.168280	149685.911861	35.677428
1272.303994	149942.986970	35.682445
1273.574193	150200.423046	35.687463
1274.729987	150465.202309	35.692480
1275.252162	150732.087601	35.697498
1276.801332	150985.777244	35.702516
1277.801715	151265.816867	35.707533
1279.414426	151529.501573	35.712551
1281.116883	151796.004172	35.717568
1282.030900	152079.476026	35.722586
1283.258583	152346.245989	35.727604
1284.992534	152623.956225	35.732621
1286.615233	152888.052005	35.737639
1287.913342	153144.608849	35.742656
1289.281895	153424.919025	35.747674
1290.804705	153685.035550	35.752692
1292.317577	153946.525787	35.757709
1293.609964	154205.132070	35.762727
1295.837411	154448.461609	35.767744
1297.681284	154697.488490	35.772762
1299.373812	154931.192665	35.777780
1300.796279	155162.464650	35.782797
1302.697323	155402.409118	35.787815
1304.399870	155631.252566	35.792832
1305.326820	155856.790788	35.797850
1307.020423	156085.040765	35.802868
1308.139237	156313.470463	35.807885
1309.298128	156526.838860	35.812903
1310.759448	156754.264543	35.817920
1311.560853	156992.623053	35.822938
1312.467460	157221.000594	35.827956
1313.672897	157452.962967	35.832973
1314.728010	157690.357811	35.837991
1315.833715	157923.556323	35.843008
1316.660454	158179.828205	35.848026
1318.445832	158426.886810	35.853044
1319.087061	158688.280604	35.858061
1320.023231	158943.383305	35.863079
1321.215559	159193.051484	35.868096
1322.169044	159459.236568	35.873114
1323.428138	159731.430646	35.878132
1324.504877	160007.590039	35.883149
1325.635043	160282.942474	35.888167
1326.930824	160559.831744	35.893184
1328.161433	160829.584816	35.898202
1329.734644	161112.425400	35.903220
1330.807306	161398.544910	35.908237
1331.780176	161674.778633	35.913255
1333.344045	161953.092019	35.918272
1334.451313	162244.186642	35.923290
1336.084713	162501.162456	35.928308
1337.614818	162778.545183	35.933325
1338.961582	163050.206488	35.938343
1340.110120	163310.562353	35.943360
1341.489726	163586.410440	35.948378
1342.715406	163850.717553	35.953396
1343.997697	164119.930298	35.958413
1345.034966	164408.049156	35.963431
1346.706559	164681.088286	35.968448
1348.065873	164972.193580	35.973466
1349.273796	165261.762161	35.978484
1350.431925	165536.700709	35.983501
1351.999374	165822.419145	35.988519
1353.590997	166108.960266	35.993536
1354.798593	166403.574279	35.998554
1356.427446	166696.320673	36.003572
1357.674829	166977.789802	36.008589
1359.508881	167265.427761	36.013607
1360.465793	167540.291485	36.018624
1362.013583	167828.433637	36.023642
1363.274201	168107.226157	36.028660
1364.989039	168395.865034	36.033677
1366.540216	168683.781564	36.038695
1368.051316	168970.397716	36.043712
1369.631420	169255.696392	36.048730
1371.154771	169532.523331	36.053748
1372.098426	169814.203529	36.058765
1373.190061	170109.485857	36.063783
1374.798088	170380.855589	36.068800
1375.840987	170684.832830	36.073818
1377.199184	170974.756656	36.078836
1378.481894	171280.730371	36.083853
1379.588520	171586.644004	36.088871
1381.083223	171884.727185	36.093888
1382.267623	172192.929345	36.098906
1383.558883	172493.522783	36.103924
1384.834125	172808.925488	36.108941
1385.791647	173116.493860	36.113959
1387.105399	173436.832526	36.118976
1388.289914	173748.342276	36.123994
1389.792270	174072.666541	36.129012
1391.778307	174397.640206	36.134029
1392.830509	174720.742363	36.139047
1394.893152	175026.672175	36.144064
1396.899179	175356.624237	36.149082
1398.223239	175652.208714	36.154100
1400.267301	175952.735465	36.159117
1401.275444	176261.438087	36.164135
1402.911244	176553.243687	36.169152
1404.495892	176868.042413	36.174170
1406.314513	177165.535805	36.179188
1407.640332	177457.316866	36.184205
1408.806011	177757.200256	36.189223
1410.167952	178060.000044	36.194240
1411.306862	178356.105533	36.199258
1413.319917	178660.735696	36.204276
1414.520076	178952.109718	36.209293
1415.927619	179261.255891	36.214311
1417.655540	179551.076226	36.219328
1418.665430	179854.775428	36.224346
1419.940279	180157.697649	36.229364
1421.458858	180462.639961	36.234381
1422.508532	180772.202917	36.239399
1424.175730	181065.009166	36.244416
1425.524450	181379.403776	36.249434
1426.466726	181679.563892	36.254452
1428.115449	181979.208023	36.259469
1429.664183	182290.831376	36.264487
1431.302505	182574.681256	36.269504
1432.156611	182875.290739	36.274522
1433.658920	183175.901298	36.279540
1435.348312	183459.466410	36.284557
1436.583263	183755.320262	36.289575
1437.639698	184049.831411	36.294592
1439.254590	184348.345246	36.299610
1440.828393	184648.847524	36.304628
1442.600089	184945.205085	36.309645
1443.873229	185255.357065	36.314663
1445.239539	185556.453296	36.319680
1446.362496	185862.515954	36.324698
1447.777806	186167.009799	36.329716
1449.338273	186514.610011	36.334733
1450.610417	186859.208559	36.339751
1452.078481	187171.697894	36.344768
1453.246282	187496.426969	36.349786
1454.489392	187811.163140	36.354804
1456.027408	188122.272692	36.359821
1457.361705	188464.733051	36.364839
1458.746617	188790.524178	36.369856
1459.959595	189130.668777	36.374874
1461.094481	189468.286614	36.379892
1462.421386	189803.182978	36.384909
1464.105899	190158.750949	36.389927
1465.598271	190497.052457	36.394944
1467.238809	190837.541586	36.399962
1468.894258	191201.296193	36.404980
1470.478361	191527.038450	36.409997
1471.782518	191873.933312	36.415015
1473.319935	192213.731258	36.420032
1475.049207	192560.231312	36.425050
1476.714483	192907.504371	36.430068
1478.746794	193243.290535	36.435085
1480.013395	193584.760241	36.440103
1481.344503	193922.334398	36.445120
1483.285644	194264.563957	36.450138
1484.847210	194597.252176	36.455156
1486.533733	194940.183764	36.460173
1487.634122	195289.786899	36.465191
1489.364694	195626.642424	36.470208
1490.882219	195959.518696	36.475226
1492.047626	196319.351039	36.480244
1493.702829	196654.315735	36.485261
1495.024862	197005.946012	36.490279
1496.578176	197352.765433	36.495296
1497.693762	197691.957465	36.500314
1498.904113	198053.031778	36.505332
1500.391348	198400.499041	36.510349
1502.125194	198762.128163	36.515367
1503.196165	199118.578275	36.520384
1504.762285	199486.966859	36.525402
1506.053221	199844.451075	36.530420
1507.882235	200186.712201	36.535437
1509.065039	200559.456200	36.540455
1510.638128	200926.526061	36.545472
1512.618773	201288.782708	36.550490
1514.105898	201662.599232	36.555508
1515.605644	202024.577067	36.560525
1517.230434	202389.330349	36.565543
1518.604119	202755.393803	36.570560
1520.378617	203122.817807	36.575578
1521.325646	203483.614959	36.580596
1522.961126	203846.515086	36.585613
1524.332608	204220.100958	36.590631
1525.987518	204592.525469	36.595648
1527.499194	204962.788460	36.600666
1529.238575	205332.889480	36.605684
1530.769419	205672.641947	36.610701
1532.240374	206030.364217	36.615719
1533.639622	206382.230225	36.620736
1534.803654	206734.209828	36.625754
1536.159825	207105.390039	36.630772
1538.051966	207457.968118	36.635789
1539.645467	207816.690234	36.640807
1541.068469	208177.268613	36.645824
1542.959554	208543.718631	36.650842
1544.384740	208908.184454	36.655860
1545.764232	209268.263191	36.660877
1547.171265	209632.834515	36.665895
1548.763095	210004.134721	36.670912
1550.075851	210378.654544	36.675930
1551.180165	210757.094227	36.680948
1552.694169	211135.241669	36.685965
1554.329981	211514.920156	36.690983
1555.518642	211908.564843	36.696000
1557.451945	212295.768008	36.701018
1558.745838	212686.145558	36.706036
1560.373303	213071.847911	36.711053
1561.726216	213475.427044	36.716071
1563.639590	213879.325391	36.721088
1565.161422	214263.623001	36.726106
1566.663574	214660.981609	36.731124
1568.838397	215067.329899	36.736141
1570.321971	215465.225710	36.741159
1572.298397	215860.174138	36.746176
1573.938457	216249.002437	36.751194
1575.462538	216638.484319	36.756212
1577.326848	217036.804631	36.761229
1578.961953	217431.325147	36.766247
1580.369066	217820.902477	36.771264
1582.309493	218203.054883	36.776282
1583.709128	218604.624583	36.781300
1585.204565	219001.073357	36.786317
1586.669355	219399.711911	36.791335
1588.136810	219804.701276	36.796352
1589.848399	220203.581096	36.801370
1591.243523	220622.503605	36.806388
1592.720175	221018.245079	36.811405
1594.423187	221426.170634	36.816423
1596.018307	221844.884550	36.821440
1597.429586	222251.026972	36.826458
1599.215007	222669.050874	36.831476
1601.401629	223081.550223	36.836493
1602.940929	223475.631400	36.841511
1604.185098	223888.913512	36.846528
1605.935029	224290.862520	36.851546
1607.492649	224716.594485	36.856564
1609.390147	225114.430405	36.861581
1610.904506	225516.670393	36.866599
1612.771919	225928.559479	36.871616
1614.429563	226339.134952	36.876634
1615.970503	226757.375274	36.881652
1617.346529	227157.096367	36.886669
1618.736543	227574.191582	36.891687
1620.806427	227986.683781	36.896704
1622.166785	228390.624125	36.901722
1623.854920	228813.362852	36.906740
1625.661387	229218.782756	36.911757
1627.072083	229637.830192	36.916775
1629.316143	230041.072741	36.921792
1630.860057	230447.600174	36.926810
1632.097839	230862.431605	36.931828
1633.724196	231267.751711	36.936845
1635.155968	231675.007326	36.941863
1636.725464	232074.518329	36.946880
1638.709798	232475.056515	36.951898
1639.861605	232879.763929	36.956916
1642.016100	233269.478249	36.961933
1643.341878	233672.125515	36.966951
1645.297411	234063.064335	36.971968
1646.848031	234450.865312	36.976986
1647.735929	234854.164372	36.982004
1649.450160	235262.363680	36.987021
1651.132365	235677.223376	36.992039
1652.575150	236084.346564	36.997056
1654.149955	236496.885044	37.002074
1655.688680	236915.119126	37.007092
1657.476098	237325.641892	37.012109
1659.280375	237749.117362	37.017127
1660.630757	238174.517778	37.022144
1662.396306	238595.635665	37.027162
1664.953508	238998.338563	37.032180
1667.846035	239391.563753	37.037197
1669.874681	239786.676440	37.042215
1671.614198	240192.249212	37.047232
1673.527456	240575.972709	37.052250
1674.886530	240982.061096	37.057268
1676.513118	241380.409791	37.062285
1678.109033	241786.586860	37.067303
1679.323279	242194.372586	37.072320
1680.741494	242594.123710	37.077338
1682.207723	243005.399657	37.082356
1683.445082	243422.731213	37.087373
1684.773071	243855.315027	37.092391
1686.153482	244285.857550	37.097408
1687.483489	244714.451074	37.102426
1689.567949	245168.988993	37.107444
1691.208341	245600.910697	37.112461
1692.746149	246044.126348	37.117479
1694.142523	246497.727431	37.122496
1696.048041	246944.516073	37.127514
1697.883193	247400.357983	37.132532
1699.342394	247856.232199	37.137549
1700.943469	248312.133870	37.142567
1702.049932	248776.037313	37.147584
1704.197005	249228.802876	37.152602
1705.487204	249704.918976	37.157620
1707.311045	250173.227953	37.162637
1709.453576	250628.733873	37.167655
1711.049293	251102.461118	37.172672
1712.542605	251581.918407	37.177690
1714.282372	252054.400941	37.182708
1716.064873	252533.022556	37.187725
1717.770453	253008.301656	37.192743
1719.616313	253488.129563	37.197760
1721.028334	253970.513121	37.202778
1723.011117	254448.258869	37.207796
1724.377406	254930.163680	37.212813
1726.295347	255424.071481	37.217831
1727.828133	255911.255642	37.222848
1730.031151	256394.472176	37.227866
1731.737916	256885.384886	37.232884
1733.716551	257370.817397	37.237901
1735.451776	257843.763557	37.242919
1737.242891	258330.669572	37.247936
1738.764592	258814.313751	37.252954
1740.797051	259305.445431	37.257972
1742.564120	259778.785559	37.262989
1744.527754	260253.439250	37.268007
1745.903886	260746.699682	37.273024
1747.659234	261218.105398	37.278042
1749.586161	261704.950889	37.283060
1751.489537	262183.212801	37.288077
1753.255493	262647.346492	37.293095
1754.827861	263115.928044	37.298112
1756.842880	263577.097829	37.303130
1758.803267	264033.524478	37.308148
1760.546963	264494.377141	37.313165
1762.128451	264952.637030	37.318183
1763.639641	265405.495875	37.323200
1764.813749	265874.559200	37.328218
1766.609634	266352.133250	37.333236
1768.483617	266824.333654	37.338253
1770.137084	267298.648984	37.343271
1771.945297	267784.519489	37.348288
1773.541286	268269.303220	37.353306
1776.051254	268736.061110	37.358324
1777.782020	269209.745303	37.363341
1780.043760	269689.160126	37.368359
1781.416089	270172.927668	37.373376
1783.305729	270646.985962	37.378394
1785.438107	271136.394695	37.383412
1787.052569	271604.370171	37.388429
1789.127117	272092.436610	37.393447
1790.840964	272579.058330	37.398464
1792.733281	273046.246076	37.403482
1795.300556	273509.998662	37.408500
1797.011034	273982.746235	37.413517
1799.025444	274454.351531	37.418535
1800.961369	274930.004462	37.423552
1802.680447	275396.037987	37.428570
1804.474106	275864.622186	37.433588
1806.341118	276342.537911	37.438605
1807.914188	276819.379359	37.443623
1809.438672	277302.676043	37.448640
1811.568531	277775.742209	37.453658
1813.412258	278264.950934	37.458676
1815.303048	278745.210078	37.463693
1817.425792	279221.417488	37.468711
1818.787678	279707.264042	37.473728
1820.197875	280179.488321	37.478746
1822.199899	280680.312842	37.483764
1823.262968	281176.125827	37.488781
1825.164491	281673.607236	37.493799
1826.710085	282193.233725	37.498816
1828.372527	282697.881196	37.503834
1830.144621	283207.561265	37.508852
1832.019392	283721.106785	37.513869
1834.105721	284229.943060	37.518887
1835.543513	284760.918286	37.523904
1837.287561	285272.390523	37.528922
1839.301367	285795.014889	37.533940
1840.646498	286328.582440	37.538957
1842.803522	286845.361340	37.543975
1844.424803	287390.303711	37.548992
1846.306951	287925.729571	37.554010
1848.359764	288460.032483	37.559028
1850.280314	288987.470584	37.564045
1851.889791	289512.083805	37.569063
1853.707311	290052.453378	37.574080
1855.912692	290586.968516	37.579098
1857.791273	291122.012641	37.584116
1859.520516	291648.011143	37.589133
1861.493861	292175.591923	37.594151
1863.406074	292721.306136	37.599168
1865.437193	293263.112194	37.604186
1867.313223	293795.695853	37.609204
1868.951306	294332.602770	37.614221
1871.032854	294860.574644	37.619239
1873.189716	295401.808328	37.624256
1874.860729	295930.901097	37.629274
1876.429508	296448.351767	37.634292
1878.108255	296964.206498	37.639309
1880.040078	297479.306095	37.644327
1881.720554	298004.316122	37.649344
1883.744216	298514.365126	37.654362
1885.704133	299038.255449	37.659380
1886.841455	299568.895515	37.664397
1889.214891	300097.610743	37.669415
1890.894465	300632.395229	37.674432
1892.944918	301156.098794	37.679450
1894.663689	301687.794957	37.684468
1896.884220	302227.251493	37.689485
1899.055103	302759.272377	37.694503
1900.908418	303290.931413	37.699520
1903.034983	303832.137784	37.704538
1905.142087	304363.898472	37.709556
1906.806553	304902.855949	37.714573
1908.617878	305442.571686	37.719591
1910.674719	305982.471737	37.724608
1912.896561	306517.999613	37.729626
1914.591669	307058.528553	37.734644
1916.128557	307611.133329	37.739661
1918.096398	308162.750733	37.744679
1919.597585	308724.562566	37.749696
1921.494130	309283.514046	37.754714
1923.286888	309851.612799	37.759732
1924.683059	310419.462335	37.764749
1927.456580	310987.952594	37.769767
1929.458698	311546.962757	37.774784
1931.418343	312113.130299	37.779802
1933.454808	312685.268756	37.784820
1935.393784	313259.141293	37.789837
1937.012227	313834.122825	37.794855
1939.268660	314417.068001	37.799872
1940.980152	314986.360937	37.804890
1942.899707	315571.145982	37.809908
1944.223052	316162.183696	37.814925
1946.667391	316746.617575	37.819943
1948.193326	317339.486011	37.824960
1950.256176	317933.226844	37.829978
1952.273244	318532.524404	37.834996
1954.509180	319134.824708	37.840013
1955.919869	319728.693950	37.845031
1958.059315	320323.836679	37.850048
1959.932350	320921.626524	37.855066
1962.327032	321524.528302	37.860084
1964.531649	322133.084467	37.865101
1966.250123	322727.447392	37.870119
1968.175916	323336.258102	37.875136
1970.538401	323934.588300	37.880154
1972.863276	324530.352996	37.885172
1974.911277	325137.113541	37.890189
1976.851881	325716.073373	37.895207
1979.102934	326316.923456	37.900224
1980.908509	326915.170231	37.905242
1983.068209	327504.193528	37.910260
1984.889346	328110.767230	37.915277
1986.801426	328698.568378	37.920295
1988.885645	329308.076296	37.925312
1990.998154	329899.988857	37.930330
1993.140934	330489.376088	37.935348
1994.934338	331100.169941	37.940365
1996.906264	331690.935501	37.945383
1998.812528	332284.162962	37.950400
2000.498868	332882.108684	37.955418
2003.020416	333480.320169	37.960436
2005.153915	334086.852593	37.965453
2007.221415	334674.461830	37.970471
2008.959873	335251.408622	37.975488
2010.775635	335823.032819	37.980506
2013.343214	336400.871943	37.985524
2014.926552	336982.330990	37.990541
2016.742685	337552.482333	37.995559
2018.735216	338131.550779	38.000576
2020.493175	338719.929883	38.005594
2022.318622	339304.890055	38.010612
2024.086512	339897.281078	38.015629
2026.103862	340488.760858	38.020647
2027.970036	341089.308761	38.025664
2029.988634	341699.155751	38.030682
2031.879569	342309.544671	38.035700
2033.632762	342922.024038	38.040717
2035.894595	343530.989304	38.045735
2038.051459	344140.543503	38.050752
2040.180426	344759.651820	38.055770
2042.728086	345370.441629	38.060788
2044.376632	345997.311765	38.065805
2046.390593	346615.973064	38.070823
2048.367561	347233.817289	38.075840
2050.297530	347857.869981	38.080858
2052.921707	348493.339706	38.085876
2054.845258	349120.818133	38.090893
2057.035367	349747.025789	38.095911
2059.322714	350359.260756	38.100928
2061.617712	350999.094526	38.105946
2064.137045	351612.233038	38.110964
2066.536731	352242.746049	38.115981
2068.581917	352855.326517	38.120999
2070.473467	353483.131032	38.126016
2072.927802	354098.868715	38.131034
2075.008809	354713.968294	38.136052
2077.235011	355335.168172	38.141069
2079.121173	355961.834016	38.146087
2081.458084	356581.141142	38.151104
2083.422749	357202.370018	38.156122
2085.839773	357819.535741	38.161140
2087.509819	358458.403191	38.166157
2089.434916	359088.801710	38.171175
2091.887404	359707.926234	38.176192
2093.738654	360332.480436	38.181210
2095.923671	360955.626082	38.186228
2097.908244	361591.488617	38.191245
2100.091479	362223.935531	38.196263
2102.452771	362842.249179	38.201280
2104.420114	363470.749389	38.206298
2106.703967	364097.336532	38.211316
2109.155393	364742.030049	38.216333
2110.864259	365363.915386	38.221351
2113.563511	365989.636562	38.226368
2115.412053	366627.464001	38.231386
2117.591931	367248.474811	38.236404
2119.528138	367884.207941	38.241421
2121.480228	368499.474821	38.246439
2123.873109	369137.895900	38.251456
2125.899864	369784.012236	38.256474
2127.901319	370416.713599	38.261492
2129.901519	371049.375520	38.266509
2132.074409	371686.480777	38.271527
2134.094852	372327.243753	38.276544
2136.242054	372964.754336	38.281562
2138.571825	373593.024745	38.286580
2141.108959	374235.207905	38.291597
2143.007765	374877.906484	38.296615
2145.321404	375510.923424	38.301632
2147.270043	376150.163952	38.306650
2149.306804	376778.583804	38.311668
2151.395193	377391.249631	38.316685
2153.391224	378006.854296	38.321703
2155.513033	378620.322562	38.326720
2157.417981	379243.284074	38.331738
2159.408029	379852.818137	38.336756
2161.382052	380486.656512	38.341773
2163.166848	381123.193948	38.346791
2165.259304	381747.130398	38.351808
2167.396971	382390.673394	38.356826
2170.239473	383018.767480	38.361844
2172.326091	383664.084859	38.366861
2174.677295	384288.603113	38.371879
2177.034762	384919.714862	38.376896
2178.996127	385564.573249	38.381914
2181.528134	386200.918546	38.386932
2183.271568	386843.549912	38.391949
2185.223776	387501.679982	38.396967
2187.766870	388142.886817	38.401984
2189.603603	388806.039532	38.407002
2191.795413	389466.637594	38.412020
2193.885855	390124.777858	38.417037
2196.039698	390778.282573	38.422055
2198.214949	391455.717451	38.427072
2200.187429	392123.899071	38.432090
2202.189118	392794.336256	38.437108
2204.399423	393484.975035	38.442125
2206.310188	394172.805575	38.447143
2208.811198	394854.651094	38.452160
2210.717100	395544.518798	38.457178
2212.889430	396253.309636	38.462196
2214.887985	396958.917116	38.467213
2216.906982	397664.399064	38.472231
2219.215320	398371.586333	38.477248
2221.601709	399092.508675	38.482266
2223.969887	399809.210239	38.487284
2226.404236	400520.969485	38.492301
2228.164324	401236.962753	38.497319
2230.291125	401956.723035	38.502336
2232.635812	402698.139239	38.507354
2234.904061	403411.454504	38.512372
2237.483062	404148.687395	38.517389
2239.363956	404886.663381	38.522407
2241.791076	405614.206230	38.527424
2244.184686	406356.001054	38.532442
2246.360068	407082.978948	38.537460
2248.651304	407816.543667	38.542477
2250.715609	408569.144806	38.547495
2253.785575	409297.832908	38.552512
2255.944110	410031.041250	38.557530
2258.300559	410770.467726	38.562548
2260.698272	411506.270649	38.567565
2262.711360	412242.058233	38.572583
2265.551547	412973.290207	38.577600
2267.952602	413705.223696	38.582618
2270.208562	414428.504856	38.587636
2272.533829	415157.061985	38.592653
2274.692304	415889.161013	38.597671
2277.308601	416624.096809	38.602688
2279.727590	417352.563895	38.607706
2282.452555	418092.135320	38.612724
2284.424551	418817.940975	38.617741
2286.100124	419550.038836	38.622759
2289.038016	420280.750349	38.627776
2291.732013	420994.179511	38.632794
2294.355933	421710.072805	38.637812
2296.988439	422424.473435	38.642829
2299.067629	423128.620631	38.647847
2301.642163	423822.199639	38.652864
2303.766901	424505.561538	38.657882
2305.537005	425185.062839	38.662900
2308.187196	425859.246777	38.667917
2310.693174	426529.032358	38.672935
2312.912773	427218.758656	38.677952
2315.176741	427896.068934	38.682970
2317.299034	428563.874860	38.687988
2320.022367	429242.937809	38.693005
2321.899944	429939.245218	38.698023
2324.110541	430626.478907	38.703040
2326.183746	431312.092677	38.708058
2328.027623	432006.613680	38.713076
2330.275904	432702.714546	38.718093
2332.065450	433414.124775	38.723111
2334.868455	434118.932282	38.728128
2337.066025	434847.307261	38.733146
2338.869493	435567.429024	38.738164
2341.399879	436292.463114	38.743181
2342.978008	437036.061600	38.748199
2345.233420	437782.455673	38.753216
2347.537053	438520.880500	38.758234
2349.871606	439275.539947	38.763252
2352.040862	440028.881503	38.768269
2353.891905	440799.823063	38.773287
2356.577904	441559.084518	38.778304
2358.594163	442338.625553	38.783322
2360.957030	443115.857127	38.788340
2363.603426	443893.011713	38.793357
2366.375517	444683.245945	38.798375
2368.722395	445463.209525	38.803392
2371.253981	446243.110981	38.808410
2373.883705	447031.397477	38.813428
2376.497487	447816.975811	38.818445
2378.680267	448608.142153	38.823463
2380.923731	449394.164334	38.828480
2383.527481	450185.296529	38.833498
2385.766380	450971.048379	38.838516
2388.394130	451761.147768	38.843533
2390.743534	452563.574144	38.848551
2393.449201	453353.186589	38.853568
2395.913097	454152.191061	38.858586
2397.991914	454955.005403	38.863604
2400.865708	455753.670970	38.868621
2403.266237	456551.314075	38.873639
2405.801880	457357.984462	38.878656
2408.280513	458156.500615	38.883674
2410.321368	458956.663301	38.888692
2413.126545	459748.191126	38.893709
2415.466192	460560.444959	38.898727
2417.964872	461355.579749	38.903744
2420.638240	462155.191324	38.908762
2422.432681	462958.585975	38.913780
2425.294577	463768.889414	38.918797
2427.816863	464576.079080	38.923815
2430.580262	465364.173232	38.928832
2432.872788	466173.188561	38.933850
2435.494906	466976.059899	38.938868
2437.814330	467781.714074	38.943885
2440.304102	468592.749805	38.948903
2442.323640	469385.208331	38.953920
2445.175315	470198.428528	38.958938
2447.069539	471005.756855	38.963956
2449.592955	471808.761323	38.968973
2452.197764	472626.841333	38.973991
2455.089234	473427.590401	38.979008
2458.022824	474221.385550	38.984026
2460.559834	475020.951384	38.989044
2463.176861	475813.205000	38.994061
2465.383011	476586.881042	38.999079
2467.758230	477340.782329	39.004096
2470.447200	478096.060703	39.009114
2473.029490	478855.755596	39.014132
2476.029721	479618.372888	39.019149
2478.155600	480380.334033	39.024167
2480.665451	481139.426244	39.029184
2482.852188	481895.155646	39.034202
2484.611965	482660.893373	39.039220
2486.993487	483436.574598	39.044237
2489.477940	484212.906435	39.049255
2492.118717	484983.733120	39.054272
2494.672427	485767.433297	39.059290
2496.655487	486557.027085	39.064308
2498.954394	487342.147855	39.069325
2501.635497	488154.069555	39.074343
2503.792920	488957.718246	39.079360
2506.328825	489760.912639	39.084378
2508.856959	490576.254799	39.089396
2511.366126	491388.836148	39.094413
2513.239696	492217.387709	39.099431
2515.586010	493043.503012	39.104448
2518.327573	493876.460162	39.109466
2520.786695	494725.226227	39.114484
2523.075936	495564.202170	39.119501
2525.380245	496419.088757	39.124519
2528.072044	497266.011287	39.129536
2530.601423	498115.981375	39.134554
2533.251555	498981.337656	39.139572
2536.202193	499840.957963	39.144589
2538.608276	500690.495584	39.149607
2541.257668	501566.268549	39.154624
2544.106529	502424.090909	39.159642
2546.429551	503283.806519	39.164660
2549.040628	504158.371282	39.169677
2551.330122	505037.562303	39.174695
2553.869973	505919.377107	39.179712
2556.407389	506793.993293	39.184730
2558.971150	507688.021211	39.189748
2561.636911	508562.960904	39.194765
2563.902545	509468.543474	39.199783
2566.215871	510356.907986	39.204800
2569.051658	511256.501487	39.209818
2571.367520	512152.094859	39.214836
2574.585623	513044.824100	39.219853
2576.774997	513958.374962	39.224871
2579.780449	514857.457291	39.229888
2582.325675	515761.530672	39.234906
2584.988970	516667.336043	39.239924
2587.795582	517564.311443	39.244941
2590.292663	518479.876300	39.249959
2592.596921	519381.938145	39.254976
2595.491139	520298.373869	39.259994
2597.922422	521211.251364	39.265012
2599.939323	522116.291743	39.270029
2602.639884	523047.094909	39.275047
2605.380084	523963.807430	39.280064
2607.728257	524885.241411	39.285082
2610.659958	525811.444069	39.290100
2613.114402	526741.826489	39.295117
2615.622495	527667.412823	39.300135
2618.496836	528602.722324	39.305152
2621.078925	529516.764137	39.310170
2623.579922	530440.297549	39.315188
2626.225865	531370.020583	39.320205
2629.140195	532303.853449	39.325223
2631.652736	533227.990468	39.330240
2634.618550	534155.404805	39.335258
2637.101293	535064.652877	39.340276
2639.703993	535950.222033	39.345293
2642.285563	536849.488069	39.350311
2644.413150	537740.931029	39.355328
2646.988619	538636.056147	39.360346
2649.632104	539550.631183	39.365364
2652.040488	540460.609897	39.370381
2654.621383	541358.151074	39.375399
2657.215624	542283.776299	39.380416
2660.318484	543200.222083	39.385434
2662.686417	544134.124958	39.390452
2665.234380	545047.511453	39.395469
2667.965129	545970.483756	39.400487
2670.724078	546904.869441	39.405504
2673.535378	547824.079129	39.410522
2676.083198	548765.880068	39.415540
2678.884061	549704.409725	39.420557
2681.550553	550646.950044	39.425575
2683.817477	551598.555423	39.430592
2686.874858	552555.728374	39.435610
2689.195834	553507.927535	39.440628
2691.668115	554471.056289	39.445645
2694.480690	555447.488199	39.450663
2696.623987	556414.873447	39.455680
2699.792456	557398.708973	39.460698
2701.826171	558378.731984	39.465716
2704.988817	559370.072665	39.470733
2707.603595	560363.069494	39.475751
2710.325408	561366.136360	39.480768
2713.127188	562363.945403	39.485786
2715.987734	563366.769721	39.490804
2718.603707	564367.292395	39.495821
2721.611947	565365.864897	39.500839
2724.399104	566366.389319	39.505856
2727.481302	567376.195129	39.510874
2729.959810	568386.257409	39.515892
2732.992009	569379.022173	39.520909
2735.317628	570395.390273	39.525927
2738.460161	571418.698424	39.530944
2741.023918	572421.033504	39.535962
2743.837736	573446.212952	39.540980
2747.166366	574459.859416	39.545997
2749.639638	575473.198435	39.551015
2752.206567	576504.293790	39.556032
2755.143337	577517.626303	39.561050
2757.519036	578542.210422	39.566068
2760.989877	579555.174629	39.571085
2764.126238	580586.604698	39.576103
2766.945847	581604.485404	39.581120
2770.243725	582614.546625	39.586138
2772.855253	583624.872626	39.591156
2775.717700	584628.616862	39.596173
2778.713860	585641.296913	39.601191
2781.254958	586658.103251	39.606208
2784.138950	587663.364831	39.611226
2787.116787	588683.462307	39.616244
2789.601577	589699.342941	39.621261
2792.476125	590709.020727	39.626279
2794.976870	591725.307522	39.631296
2798.248932	592742.076874	39.636314
2800.603351	593747.103652	39.641332
2803.306893	594762.071122	39.646349
2806.747295	595782.220611	39.651367
2809.077794	596798.849747	39.656384
2812.339827	597806.696386	39.661402
2815.084857	598823.365312	39.666420
2817.894873	599839.626158	39.671437
2820.848653	600834.349587	39.676455
2823.331517	601819.517812	39.681472
2826.368322	602798.716438	39.686490
2828.841291	603766.482100	39.691508
2831.581036	604746.491558	39.696525
2834.447693	605716.957453	39.701543
2837.100122	606702.333449	39.706560
2839.553507	607688.743606	39.711578
2842.465126	608698.183063	39.716596
2845.448047	609681.574643	39.721613
2848.086254	610674.899987	39.726631
2850.541714	611685.311736	39.731648
2854.032055	612690.973107	39.736666
2856.308079	613705.848428	39.741684
2859.080144	614717.752107	39.746701
2861.830021	615741.969698	39.751719
2864.792392	616766.298532	39.756736
2867.346307	617788.044386	39.761754
2869.981681	618828.609426	39.766772
2872.519489	619876.654575	39.771789
2875.566652	620923.014448	39.776807
2878.159443	621991.652758	39.781824
2881.239268	623049.389271	39.786842
2884.387994	624107.648490	39.791860
2886.983457	625179.923769	39.796877
2890.200347	626251.585672	39.801895
2892.643974	627348.693296	39.806912
2895.976324	628417.409500	39.811930
2898.709418	629507.755259	39.816948
2901.529176	630594.380482	39.821965
2904.601641	631691.195099	39.826983
2907.107025	632799.119605	39.832000
2910.078896	633897.389032	39.837018
2913.447472	635003.031933	39.842036
2916.413860	636102.938126	39.847053
2919.741111	637206.291123	39.852071
2923.021354	638312.506550	39.857088
2925.801964	639415.686498	39.862106
2929.083330	640518.161313	39.867124
2931.326248	641627.529421	39.872141
2934.361270	642740.370072	39.877159
2936.846285	643874.337427	39.882176
2940.121579	644987.666623	39.887194
2942.939257	646112.958764	39.892212
2945.552543	647235.860057	39.897229
2948.861100	648369.097271	39.902247
2951.451818	649511.247857	39.907264
2954.343288	650655.443760	39.912282
2957.552258	651798.651823	39.917300
2960.424801	652942.662461	39.922317
2963.396244	654075.938122	39.927335
2966.316889	655234.396990	39.932352
2969.455873	656385.872663	39.937370
2972.666906	657542.946415	39.942388
2975.449886	658685.745456	39.947405
2978.586505	659843.178240	39.952423
2981.269175	661005.046005	39.957440
2984.221742	662156.848395	39.962458
2987.347855	663318.244332	39.967476
2990.716489	664482.623248	39.972493
2993.793950	665634.596762	39.977511
2996.564914	666796.084904	39.982528
2999.529665	667949.308463	39.987546
3002.709054	669106.509338	39.992564
3005.557516	670270.744218	39.997581
3009.052665	671435.960405	40.002599
3011.627688	672593.236294	40.007616
3015.370904	673735.758701	40.012634
3018.781088	674889.523862	40.017652
3021.423395	676009.973322	40.022669
3024.068256	677110.616810	40.027687
3027.160289	678239.071822	40.032704
3030.536681	679335.649273	40.037722
3033.200505	680443.036454	40.042740
3035.917785	681560.168626	40.047757
3038.971639	682676.704228	40.052775
3042.038119	683795.068693	40.057792
3045.437533	684920.158012	40.062810
3047.757552	686046.649694	40.067828
3050.407929	687178.031792	40.072845
3053.859399	688315.068930	40.077863
3056.473191	689464.145736	40.082880
3059.354827	690623.996284	40.087898
3062.533832	691773.009395	40.092916
3065.277229	692932.012611	40.097933
3068.098563	694112.731708	40.102951
3071.276317	695292.433976	40.107968
3074.153283	696472.605364	40.112986
3077.526550	697668.729631	40.118004
3080.334771	698859.579907	40.123021
3083.605894	700051.416867	40.128039
3087.011885	701240.785254	40.133056
3090.487851	702443.493081	40.138074
3093.507902	703641.007649	40.143092
3097.245146	704838.329298	40.148109
3100.537749	706038.353119	40.153127
3103.709392	707238.510591	40.158144
3106.940153	708440.647476	40.163162
3110.446947	709626.923214	40.168180
3113.302490	710829.593123	40.173197
3116.963470	712034.122463	40.178215
3119.917982	713246.218369	40.183232
3122.813131	714454.438590	40.188250
3126.205774	715658.204466	40.193268
3128.917118	716867.852690	40.198285
3131.980852	718080.410076	40.203303
3134.616858	719299.937493	40.208320
3137.892300	720527.101535	40.213338
3141.006558	721748.628459	40.218356
3144.350408	722989.816394	40.223373
3147.414413	724220.705116	40.228391
3150.647205	725446.643218	40.233408
3153.324298	726690.826724	40.238426
3156.482481	727932.171890	40.243444
3159.321079	729186.941211	40.248461
3162.643252	730445.262475	40.253479
3165.416625	731700.999548	40.258496
3168.571598	732967.529977	40.263514
3172.003554	734229.524897	40.268532
3175.083502	735506.205684	40.273549
3178.141068	736778.148784	40.278567
3181.309909	738049.659245	40.283584
3184.402013	739324.155967	40.288602
3188.045291	740606.450688	40.293620
3191.143764	741887.624107	40.298637
3194.606493	743148.236126	40.303655
3198.135905	744429.730887	40.308672
3201.614026	745702.515756	40.313690
3204.715540	746965.074992	40.318708
3208.511425	748232.997282	40.323725
3211.733749	749488.422806	40.328743
3215.144591	750756.157083	40.333760
3218.267119	752015.521909	40.338778
3221.667551	753273.003270	40.343796
3224.574977	754541.370868	40.348813
3227.906373	755785.672222	40.353831
3230.899219	757023.632917	40.358848
3234.162484	758239.872185	40.363866
3237.543159	759454.805457	40.368884
3240.692908	760668.438278	40.373901
3244.105472	761891.272263	40.378919
3247.368116	763094.475992	40.383936
3250.383501	764306.372339	40.388954
3253.432160	765519.765643	40.393972
3256.527707	766731.813786	40.398989
3259.508488	767954.041357	40.404007
3262.403595	769192.700077	40.409024
3265.239482	770441.906516	40.414042
3268.698407	771675.822945	40.419060
3271.039939	772935.851770	40.424077
3274.991454	774199.551920	40.429095
3278.136178	775475.216778	40.434112
3280.481734	776745.782213	40.439130
3284.405001	778030.716306	40.444148
3287.532262	779322.516062	40.449165
3290.872805	780607.734091	40.454183
3294.388528	781901.615138	40.459200
3297.488334	783214.742783	40.464218
3300.679490	784510.806177	40.469236
3303.518974	785828.243648	40.474253
3307.221812	787147.431782	40.479271
3310.073153	788475.368993	40.484288
3313.077470	789807.600101	40.489306
3317.006544	791154.777969	40.494324
3320.186662	792498.091178	40.499341
3323.204612	793833.062594	40.504359
3326.698966	795198.096892	40.509376
3330.096091	796549.509790	40.514394
3334.237549	797900.525018	40.519412
3338.048079	799261.002048	40.524429
3341.068898	800612.697033	40.529447
3344.666315	801954.476124	40.534464
3348.004580	803308.475566	40.539482
3351.114979	804666.117238	40.544500
3354.625185	806022.434598	40.549517
3358.824182	807395.525856	40.554535
3362.078361	808743.130687	40.559552
3365.351685	810110.963697	40.564570
3368.787501	811462.433349	40.569588
3372.057526	812831.912319	40.574605
3375.399882	814190.197077	40.579623
3378.945666	815549.612572	40.584640
3381.937484	816926.885900	40.589658
3385.081397	818311.211357	40.594676
3388.629951	819688.174009	40.599693
3391.707388	821071.504711	40.604711
3394.924990	822447.418721	40.609728
3398.266275	823841.052879	40.614746
3401.721389	825239.008919	40.619764
3405.273193	826646.813615	40.624781
3408.659723	828041.908201	40.629799
3412.320484	829442.165427	40.634816
3415.929135	830848.310129	40.639834
3419.598425	832235.320979	40.644852
3423.148575	833643.730634	40.649869
3426.907074	835030.471099	40.654887
3430.607991	836413.995034	40.659904
3433.668440	837810.270695	40.664922
3437.624354	839201.917836	40.669940
3440.851209	840610.866481	40.674957
3444.642407	841996.659252	40.679975
3447.825156	843380.771605	40.684992
3451.734614	844791.905439	40.690010
3455.344623	846178.773976	40.695028
3458.168080	847558.448360	40.700032
3462.097690	848882.577737	40.705037
3465.799469	850162.569934	40.710042
3468.863181	851381.475728	40.715047
3471.845198	852540.988516	40.720052
3475.009208	853666.170718	40.725056
3477.654180	854700.152772	40.730061
3480.615408	855678.652536	40.735066
3483.236978	856605.766791	40.740071
3485.961704	857452.529893	40.745076
3488.271697	858252.907605	40.750080
3490.913798	858985.335067	40.755085
3493.849988	859655.065349	40.760090
3495.283913	860273.132485	40.765095
3497.601984	860826.806600	40.770100
3499.594563	861335.627536	40.775104
3500.640207	861786.173081	40.780109
3502.749926	862200.661182	40.785114
3504.276693	862574.621813	40.790119
3505.757347	862895.706595	40.795124
3506.754323	863182.255774	40.800128
3507.699827	863415.268585	40.805133
3509.190412	863617.750939	40.810138
3509.880627	863797.452654	40.815143
3511.072143	863941.515768	40.820148
3512.248875	864058.332470	40.825152
3512.905534	864146.920700	40.830157
3513.714780	864203.118960	40.835162
3514.092153	864246.148524	40.840167
3515.087513	864254.494696	40.845172
3515.214355	864253.025743	40.850176
3516.048033	864217.535885	40.855181
3516.124653	864165.257067	40.860186
3516.782378	864107.476602	40.865191
3517.493235	864027.369363	40.870196
3517.775191	863940.371700	40.875200
3517.409687	863823.715687	40.880205
3518.162222	863706.592638	40.885210
3517.855004	863587.024041	40.890215
3518.656394	863445.635819	40.895220
3518.572873	863307.957591	40.900224
3518.640553	863144.162491	40.905229
3518.855957	862980.436202	40.910234
3518.670020	862815.898211	40.915239
3519.226207	862638.579868	40.920244
3518.923557	862460.037268	40.925248
3518.951970	862266.360796	40.930253
3518.828518	862066.032765	40.935258
3518.889681	861873.304253	40.940263
3518.888357	861672.653313	40.945268
3518.564159	861476.008738	40.950272
3518.342822	861268.611884	40.955277
3518.726088	861067.299509	40.960282
3518.473519	860857.669275	40.965287
3518.678133	860638.582678	40.970292
3518.926845	860433.595411	40.975296
3518.734140	860206.530245	40.980301
3518.713867	859991.321107	40.985306
3518.553053	859770.421306	40.990311
3518.407653	859554.538449	40.995316
3518.076291	859331.134358	41.000320
3517.993997	859113.194376	41.005325
3518.411797	858894.394297	41.010330
3517.998705	858675.328915	41.015335
3517.242714	858432.131442	41.020340
3517.562432	858226.763757	41.025344
3517.405722	858000.282268	41.030349
3517.383419	857769.901991	41.035354
3517.318276	857562.249356	41.040359
3516.827966	857337.631581	41.045364
3516.631323	857122.825721	41.050368
3516.810641	856899.246881	41.055373
3516.794768	856690.103947	41.060378
3516.372935	856472.793754	41.065383
3516.166890	856260.182164	41.070388
3516.286797	856050.510993	41.075392
3515.925058	855829.297088	41.080397
3516.194407	855627.617660	41.085402
3515.784482	855426.714672	41.090407
3515.637032	855210.571763	41.095412
3515.627520	855008.817491	41.100416
3515.069247	854801.238938	41.105421
3514.969704	854584.581205	41.110426
3514.675871	854396.301534	41.115431
3514.771355	854200.502756	41.120436
3514.887733	854005.758695	41.125440
3514.604719	853805.456842	41.130445
3514.397637	853607.168774	41.135450
3514.350340	853419.786622	41.140455
3514.016598	853230.894424	41.145460
3513.817656	853042.555781	41.150464
3513.960096	852852.511987	41.155469
3513.927669	852660.746775	41.160474
3513.775852	852471.704542	41.165479
3513.762784	852291.928463	41.170484
3513.943385	852112.116533	41.175488
3513.195470	851921.890937	41.180493
3513.378212	851740.421224	41.185498
3512.995844	851560.486545	41.190503
3512.835169	851378.671900	41.195508
3512.495471	851207.821420	41.200512
3512.304564	851040.138157	41.205517
3512.775822	850871.765524	41.210522
3512.300187	850710.508444	41.215527
3512.004170	850540.599896	41.220532
3511.673327	850369.529689	41.225536
3512.087273	850199.500192	41.230541
3511.684666	850044.314600	41.235546
3511.112454	849896.996438	41.240551
3511.325228	849736.766967	41.245556
3511.458987	849585.940643	41.250560
3511.009029	849429.293188	41.255565
3511.136075	849268.289354	41.260570
3511.317884	849120.155628	41.265575
3511.132415	848962.582493	41.270580
3510.539929	848824.345952	41.275584
3510.517740	848680.301496	41.280589
3510.578516	848536.434265	41.285594
3509.681761	848388.644315	41.290599
3509.812882	848250.087294	41.295604
3509.821813	848125.109574	41.300608
3509.884162	847990.335539	41.305613
3509.709275	847850.944931	41.310618
3509.592791	847723.265401	41.315623
3509.451631	847595.102486	41.320628
3509.254315	847460.356824	41.325632
3508.923487	847336.481177	41.330637
3509.433211	847207.432863	41.335642
3509.405009	847094.647951	41.340647
3508.940264	846966.715651	41.345652
3509.068416	846848.959605	41.350656
3508.378547	846728.034295	41.355661
3508.690870	846594.254982	41.360666
3508.592156	846488.737465	41.365671
3508.196416	846380.163335	41.370676
3508.337931	846262.781065	41.375680
3508.103796	846154.468229	41.380685
3508.193145	846036.508100	41.385690
3508.172828	845927.188478	41.390695
3507.820283	845824.896997	41.395700
3508.159497	845709.895763	41.400704
3508.058039	845619.482833	41.405709
3508.017365	845501.919979	41.410714
3507.839825	845393.196542	41.415719
3508.006813	845286.937387	41.420724
3507.471533	845174.194803	41.425728
3507.296489	845079.713973	41.430733
3507.482913	844977.420406	41.435738
3507.018033	844877.747199	41.440743
3507.025053	844795.931900	41.445748
3507.159410	844692.866028	41.450752
3506.794554	844603.835783	41.455757
3507.107411	844496.085433	41.460762
3506.916012	844410.708943	41.465767
3506.805576	844316.399635	41.470772
3506.839902	844238.547057	41.475776
3506.793779	844146.745578	41.480781
3506.730409	844050.097903	41.485786
3506.440598	843954.356597	41.490791
3506.393849	843865.556308	41.495796
3506.544511	843790.200377	41.500800
3506.393636	843713.824117	41.505805
3506.610580	843617.804217	41.510810
3506.122079	843538.278898	41.515815
3506.167522	843447.809623	41.520820
3506.039037	843366.868284	41.525824
3505.986622	843291.149880	41.530829
3506.048300	843212.794667	41.535834
3505.630490	843149.251925	41.540839
3505.602847	843072.072374	41.545844
3505.653841	842994.103789	41.550848
3505.614644	842923.420861	41.555853
3505.453285	842847.907734	41.560858
3505.643550	842785.138735	41.565863
3505.600999	842709.799210	41.570868
3505.736615	842640.055276	41.575872
3505.212963	842567.019500	41.580877
3505.685078	842488.687493	41.585882
3505.041268	842424.299495	41.590887
3504.943601	842362.152869	41.595892
3505.200754	842302.859463	41.600896
3505.139416	842236.244846	41.605901
3505.378447	842170.358366	41.610906
3505.167173	842108.129848	41.615911
3505.150710	842033.068560	41.620916
3504.616327	841957.020461	41.625920
3504.889378	841915.759620	41.630925
3505.052731	841843.868304	41.635930
3504.348471	841799.849862	41.640935
3504.595524	841741.522273	41.645940
3504.627449	841678.087366	41.650944
3504.654137	841625.127427	41.655949
3504.691069	841565.667083	41.660954
3504.827527	841509.100314	41.665959
3504.719034	841446.751779	41.670964
3504.861028	841388.728115	41.675968
3504.320645	841336.048220	41.680973
3504.337279	841281.340889	41.685978
3504.464994	841223.026850	41.690983
3504.101406	841161.200162	41.695988
3504.061510	841114.647844	41.700992
3504.053765	841064.986190	41.705997
3504.275422	841012.863283	41.711002
3503.938662	840971.691195	41.716007
3504.249540	840912.472471	41.721012
3503.872177	840875.574093	41.726016
3503.567131	840828.672970	41.731021
3504.264062	840779.771792	41.736026
3504.298098	840740.965210	41.741031
3504.344510	840688.769846	41.746036
3504.006236	840633.141967	41.751040
3503.959201	840586.004581	41.756045
3504.058799	840531.471372	41.761050
3503.607029	840498.268538	41.766055
3503.576507	840447.829216	41.771060
3503.991049	840405.080620	41.776064
3503.693482	840354.585240	41.781069
3503.815674	840312.560749	41.786074
3503.837373	840270.454658	41.791079
3503.983562	840232.888367	41.796084
3503.612848	840181.820879	41.801088
3503.699629	840135.435096	41.806093
3503.412314	840087.167146	41.811098
3503.588913	840054.348668	41.816103
3503.712415	840007.956150	41.821108
3503.365310	839960.375622	41.826112
3503.200893	839932.945676	41.831117
3503.398806	839885.473385	41.836122
3503.399964	839849.479621	41.841127
3503.300141	839811.755088	41.846132
3503.506605	839768.161271	41.851136
3503.259715	839739.579090	41.856141
3503.361271	839706.479363	41.861146
3503.425090	839676.295980	41.866151
3503.694889	839630.168706	41.871156
3503.615706	839584.386696	41.876160
3503.445116	839546.574518	41.881165
3503.422900	839490.013305	41.886170
3502.971721	839460.879572	41.891175
3503.144925	839435.723138	41.896180
3503.299229	839399.411635	41.901184
3502.892196	839360.664979	41.906189
3503.192553	839325.106400	41.911194
3502.909820	839298.274177	41.916199
3502.709507	839261.338074	41.921204
3503.012637	839234.219924	41.926208
3502.798532	839202.137015	41.931213
3502.872307	839168.650523	41.936218
3502.940505	839150.689458	41.941223
3502.425600	839115.257067	41.946228
3502.894743	839083.939986	41.951232
3502.546245	839054.885239	41.956237
3502.885416	839029.992241	41.961242
3502.583739	838996.466438	41.966247
3502.389752	838980.098357	41.971252
3502.522545	838955.334340	41.976256
3502.178613	838925.016818	41.981261
3502.605944	838906.513712	41.986266
3502.153705	838888.245076	41.991271
3502.143601	838858.166131	41.996276
3502.394093	838855.021908	42.001280
3502.293842	838826.897583	42.006285
3502.635442	838802.391394	42.011290
3502.290544	838781.873841	42.016295
3502.219970	838754.714892	42.021300
3502.638463	838739.026691	42.026304
3502.263881	838704.443239	42.031309
3502.668674	838684.681490	42.036314
3502.734198	838660.703061	42.041319
3502.528699	838642.006947	42.046324
3502.385703	838606.707460	42.051328
3502.295560	838588.090182	42.056333
3502.263507	838566.067400	42.061338
3502.286249	838560.338570	42.066343
3502.273526	838538.118583	42.071348
3502.458582	838511.112641	42.076352
3502.034997	838484.492841	42.081357
3502.110430	838460.803180	42.086362
3502.451649	838451.045787	42.091367
3502.184459	838417.608371	42.096372
3502.412260	838398.649675	42.101376
3502.285400	838383.531000	42.106381
3502.023990	838349.024832	42.111386
3502.066257	838340.963717	42.116391
3501.661468	838309.973272	42.121396
3502.182635	838289.124547	42.126400
3502.238162	838281.643540	42.131405
3502.384028	838270.072560	42.136410
3502.322732	838239.222140	42.141415
3502.412936	838227.950913	42.146420
3502.290688	838206.232033	42.151424
3502.410029	838183.893036	42.156429
3502.324402	838158.868718	42.161434
3501.970959	838142.329165	42.166439
3502.026092	838122.523170	42.171444
3502.078844	838101.358828	42.176448
3502.103188	838094.173601	42.181453
3502.686719	838068.364972	42.186458
3502.315741	838048.431247	42.191463
3502.008822	838015.774163	42.196468
3502.281701	838004.571007	42.201472
3502.182237	837992.358501	42.206477
3502.397599	837960.687005	42.211482
3502.334952	837950.021440	42.216487
3502.230429	837921.699410	42.221492
3502.458133	837900.312908	42.226496
3502.235685	837882.296405	42.231501
3502.313204	837850.063569	42.236506
3502.534694	837834.112639	42.241511
3502.417645	837818.602792	42.246516
3502.016743	837785.085674	42.251520
3501.683217	837772.424047	42.256525
3502.000489	837759.854765	42.261530
3502.113906	837738.873759	42.266535
3501.962278	837727.833496	42.271540
3502.217321	837691.107624	42.276544
3502.087454	837683.751902	42.281549
3502.200969	837665.196957	42.286554
3502.417848	837657.592891	42.291559
3502.279033	837624.422115	42.296564
3502.423004	837607.900373	42.301568
3502.249857	837592.689872	42.306573
3502.518165	837566.151915	42.311578
3501.942708	837552.168863	42.316583
3502.239817	837524.849775	42.321588
3502.267657	837513.295780	42.326592
3501.891773	837487.440510	42.331597
3502.003687	837471.214572	42.336602
3501.742823	837457.473290	42.341607
3501.843564	837438.240237	42.346612
3501.930075	837419.494635	42.351616
3502.163908	837420.816923	42.356621
3501.761651	837397.003595	42.361626
3501.999945	837378.913545	42.366631
3501.840155	837361.468022	42.371636
3502.088456	837346.967482	42.376640
3502.060878	837337.848282	42.381645
3501.961065	837300.107828	42.386650
3501.969968	837302.824139	42.391655
3501.658346	837281.325611	42.396660
3502.228521	837258.621498	42.401664
3501.796545	837250.535983	42.406669
3501.629859	837234.644135	42.411674
3501.394598	837236.136854	42.416679
3501.683985	837212.020546	42.421684
3501.901151	837192.477320	42.426688
3501.716062	837192.409224	42.431693
3501.783579	837166.192064	42.436698
3501.705682	837154.556841	42.441703
3501.682524	837146.213153	42.446708
3501.710653	837126.213950	42.451712
3501.521336	837117.993259	42.456717
3501.793780	837112.029881	42.461722
3501.826962	837098.532993	42.466727
3501.884000	837105.512637	42.471732
3502.081102	837074.518737	42.476736
3501.905242	837072.604993	42.481741
3502.137122	837047.235188	42.486746
3502.127952	837036.268438	42.491751
3501.848727	837017.287555	42.496756
3502.166240	836999.863426	42.501760
3501.942678	836983.203282	42.506765
3501.774435	836959.060428	42.511770
3501.628927	836945.396997	42.516775
3501.473025	836932.414619	42.521780
3501.766496	836917.614781	42.526784
3501.539006	836916.679716	42.531789
3501.578794	836901.337098	42.536794
3501.937742	836898.951432	42.541799
3501.983504	836883.025436	42.546804
3502.102463	836869.320490	42.551808
3502.059048	836851.661151	42.556813
3502.082367	836826.420079	42.561818
3501.906650	836818.973388	42.566823
3501.791544	836796.083445	42.571828
3501.994723	836780.035500	42.576832
3502.003521	836758.484998	42.581837
3502.249537	836736.314924	42.586842
3501.857728	836723.077761	42.591847
3501.677832	836707.380711	42.596852
3502.297796	836696.994477	42.601856
3501.589261	836687.786592	42.606861
3502.218307	836675.845788	42.611866
3502.071244	836659.172781	42.616871
3501.668357	836632.250252	42.621876
3501.767594	836612.529425	42.626880
3501.797672	836610.486268	42.631885
3501.848678	836591.064123	42.636890
3501.444098	836581.517346	42.641895
3501.693277	836580.119428	42.646900
3501.512409	836561.995362	42.651904
3501.425626	836555.893444	42.656909
3501.489411	836552.874280	42.661914
3501.445856	836548.609961	42.666919
3501.617026	836530.139552	42.671924
3501.558411	836514.034746	42.676928
3501.643669	836525.767203	42.681933
3501.465420	836494.537758	42.686938
3501.441973	836491.143908	42.691943
3501.426394	836484.254203	42.696948
3501.446024	836464.642407	42.701952
3501.109298	836460.132633	42.706957
3501.330499	836453.497099	42.711962
3501.711791	836453.631674	42.716967
3501.578814	836439.382686	42.721972
3501.708653	836427.519426	42.726976
3501.329963	836424.763514	42.731981
3501.950309	836397.000454	42.736986
3501.674537	836387.724453	42.741991
3501.461473	836386.787047	42.746996
3501.575671	836372.984634	42.752000
3501.309227	836367.784280	42.757005
3501.384809	836346.416002	42.762010
3501.590422	836347.354645	42.767015
3501.575521	836333.863548	42.772020
3501.273664	836315.563497	42.777024
3501.433574	836322.236749	42.782029
3501.830502	836312.952550	42.787034
3501.836925	836305.767973	42.792039
3501.267640	836288.189173	42.797044
3501.635281	836281.530558	42.802049
3501.656131	836278.712120	42.807053
3501.241592	836262.856428	42.812058
3501.722208	836258.412886	42.817063
3501.313062	836247.507213	42.822068
3501.512211	836235.147354	42.827073
3501.455687	836230.593604	42.832077
3501.857134	836225.385798	42.837082
3501.606521	836213.872819	42.842087
3501.428227	836192.349523	42.847092
3501.593184	836185.431252	42.852097
3501.585422	836171.647440	42.857101
3501.378428	836166.437617	42.862106
3501.441048	836161.379799	42.867111
3501.554324	836149.421500	42.872116
3501.712819	836137.067794	42.877121
3501.164814	836135.503155	42.882125
3501.420159	836126.143722	42.887130
3501.453343	836113.518320	42.892135
3501.550980	836102.241924	42.897140
3501.830417	836092.781593	42.902145
3501.602779	836086.021658	42.907149
3501.689339	836063.679862	42.912154
3501.791156	836061.528224	42.917159
3501.419700	836047.800980	42.922164
3501.819008	836039.875108	42.927169
3501.671462	836028.539820	42.932173
3501.481662	836023.909665	42.937178
3501.617571	836006.025636	42.942183
3501.317613	836002.286411	42.947188
3501.322725	835995.101666	42.952193
3501.421674	835983.824842	42.957197
3501.715775	835962.518117	42.962202
3501.499895	835966.338068	42.967207
3501.542599	835954.778738	42.972212
3501.325257	835941.415483	42.977217
3501.222204	835940.752053	42.982221
3501.646819	835935.540376	42.987226
3501.562270	835928.466649	42.992231
3501.362026	835919.372275	42.997236
3501.829720	835907.552255	43.002241
3501.258012	835905.311682	43.007245
3501.655520	835883.503101	43.012250
3501.223938	835885.123920	43.017255
3501.120352	835886.402220	43.022260
3501.309254	835881.421508	43.027265
3501.251514	835867.062311	43.032269
3501.611771	835855.938564	43.037274
3501.559858	835836.044643	43.042279
3501.445878	835839.751662	43.047284
3501.216440	835814.739999	43.052289
3501.341766	835817.147535	43.057293
3501.530474	835812.555131	43.062298
3501.429514	835827.813084	43.067303
3501.570376	835804.393914	43.072308
3501.724645	835788.253875	43.077313
3501.456212	835794.897591	43.082317
3501.434219	835778.105490	43.087322
3501.246991	835761.339171	43.092327
3501.343560	835751.324382	43.097332
3501.466988	835740.917038	43.102337
3501.435772	835746.067451	43.107341
3501.368851	835725.592999	43.112346
3501.441476	835717.135259	43.117351
3501.194995	835713.970004	43.122356
3501.347473	835723.266393	43.127361
3501.400326	835702.773140	43.132365
3501.526084	835685.957684	43.137370
3501.919420	835683.857427	43.142375
3501.413912	835675.975432	43.147380
3501.416448	835661.703406	43.152385
3501.336221	835651.230656	43.157389
3501.496031	835648.487286	43.162394
3501.386273	835639.378341	43.167399
3501.506496	835626.641221	43.172404
3501.704773	835623.018045	43.177409
3501.718726	835624.375113	43.182413
3501.276843	835604.638469	43.187418
3501.519899	835589.260714	43.192423
3501.260014	835591.048945	43.197428
3501.526094	835585.570487	43.202433
3501.596629	835573.423546	43.207437
3501.503386	835566.253661	43.212442
3501.425446	835569.566862	43.217447
3501.191298	835549.603388	43.222452
3501.485062	835539.460331	43.227457
3500.816700	835532.089044	43.232461
3500.804037	835532.479410	43.237466
3501.338031	835531.425084	43.242471
3501.262227	835533.961263	43.247476
3500.882762	835531.884671	43.252481
3501.156468	835529.511796	43.257485
3501.178429	835503.488650	43.262490
3501.406530	835508.404553	43.267495
3501.034789	835516.229790	43.272500
3501.279547	835507.939025	43.277505
3501.235266	835516.489782	43.282509
3500.717226	835493.463663	43.287514
3500.954405	835484.591516	43.292519
3501.012752	835487.203833	43.297524
3501.338476	835477.832390	43.302529
3500.576425	835482.126382	43.307533
3500.735213	835476.179150	43.312538
3501.042094	835479.140978	43.317543
3501.098062	835485.637235	43.322548
3501.129889	835484.467223	43.327553
3501.013773	835493.320510	43.332557
3501.133121	835479.709414	43.337562
3500.933269	835479.449419	43.342567
3501.104589	835478.160511	43.347572
3501.232680	835464.548014	43.352577
3501.026804	835462.347171	43.357581
3501.430775	835459.080101	43.362586
3501.152823	835465.531489	43.367591
3500.857386	835471.111799	43.372596
3500.934916	835465.080170	43.377601
3500.980489	835465.267257	43.382605
3501.038491	835444.092689	43.387610
3501.422792	835441.702492	43.392615
3501.258640	835448.718648	43.397620
3501.481249	835441.887599	43.402625
3501.036507	835447.976719	43.407629
3501.264266	835443.086661	43.412634
3501.189577	835435.525360	43.417639
3501.027848	835420.210447	43.422644
3501.289121	835419.101646	43.427649
3501.112095	835412.527215	43.432653
3501.079567	835415.056679	43.437658
3501.310630	835416.671126	43.442663
3501.151331	835406.113217	43.447668
3501.121666	835394.175756	43.452673
3501.167142	835398.052302	43.457677
3501.363037	835384.331933	43.462682
3501.330752	835385.502101	43.467687
3501.014815	835377.881349	43.472692
3501.414171	835367.236042	43.477697
3500.923916	835362.069794	43.482701
3501.195096	835357.755425	43.487706
3501.252277	835357.455246	43.492711
3501.313975	835359.484548	43.497716
3501.364988	835360.156244	43.502721
3501.220648	835345.906426	43.507725
3501.080778	835338.452283	43.512730
3501.076468	835333.501321	43.517735
3500.974195	835341.770119	43.522740
3501.293120	835336.380266	43.527745
3500.705145	835346.569720	43.532749
3500.803998	835338.981170	43.537754
3501.089897	835347.189280	43.542759
3500.842395	835335.577030	43.547764
3501.003755	835320.114264	43.552769
3501.228455	835320.467539	43.557773
3501.185775	835317.076030	43.562778
3501.201770	835326.588554	43.567783
3500.993077	835323.028816	43.572788
3501.362513	835308.407320	43.577793
3500.966877	835320.314408	43.582797
3500.992094	835298.270623	43.587802
3501.207078	835290.955135	43.592807
3500.908046	835294.108863	43.597812
3501.442915	835298.297340	43.602817
3501.322816	835302.879476	43.607821
3501.153126	835304.362415	43.612826
3501.310605	835308.901154	43.617831
3500.897961	835284.013004	43.622836
3500.922742	835266.338326	43.627841
3501.231662	835266.969716	43.632845
3501.354510	835263.843580	43.637850
3501.274091	835264.244554	43.642855
3500.870003	835270.327498	43.647860
3501.175279	835266.881567	43.652865
3500.989365	835261.473471	43.657869
3500.941633	835254.199006	43.662874
3500.989146	835242.637550	43.667879
3501.128218	835252.519325	43.672884
3501.461423	835247.418439	43.677889
3501.311551	835256.471538	43.682893
3501.288346	835248.222303	43.687898
3501.382147	835236.750694	43.692903
3501.129884	835219.798838	43.697908
3501.715752	835224.270676	43.702913
3501.517114	835226.826185	43.707917
3501.297779	835198.217914	43.712922
3501.543556	835187.013734	43.717927
3500.991086	835195.256014	43.722932
3501.369655	835191.216021	43.727937
3501.442670	835195.088394	43.732941
3501.320475	835164.522900	43.737946
3501.073559	835165.726662	43.742951
3501.106552	835169.216930	43.747956
3501.564000	835168.271606	43.752961
3501.034648	835169.616613	43.757965
3501.405443	835152.275886	43.762970
3501.569332	835148.366518	43.767975
3501.651332	835146.508935	43.772980
3501.734302	835135.718488	43.777985
3501.310003	835120.152569	43.782989
3501.073770	835111.353876	43.787994
3501.268890	835112.294359	43.792999
3501.365413	835112.861874	43.798004
3501.934519	835086.168816	43.803009
3501.543639	835082.443223	43.808013
3501.246499	835075.693006	43.813018
3501.483386	835057.790365	43.818023
3501.092699	835044.063818	43.823028
3501.323080	835039.173022	43.828033
3501.463075	835049.831758	43.833037
3501.529046	835042.442165	43.838042
3501.323265	835029.560546	43.843047
3501.255425	835020.541203	43.848052
3501.387403	835013.141256	43.853057
3501.544689	835025.059591	43.858061
3501.471310	835006.137235	43.863066
3501.597165	834986.503994	43.868071
3501.272486	834981.505725	43.873076
3501.474892	834981.862506	43.878081
3501.355032	834965.860206	43.883085
3501.233083	834950.537874	43.888090
3501.789373	834958.218763	43.893095
3501.075987	834951.727669	43.898100
3500.853884	834919.040391	43.903105
3501.108892	834929.584263	43.908109
3500.948379	834915.335948	43.913114
3500.960585	834917.567334	43.918119
3501.232350	834924.321762	43.923124
3501.194963	834919.084334	43.928129
3501.067287	834924.833120	43.933133
3501.506473	834925.444186	43.938138
3501.287530	834912.661472	43.943143
3501.453312	834902.343152	43.948148
3501.711767	834896.379768	43.953153
3501.786967	834891.513112	43.958157
3501.281603	834864.987034	43.963162
3501.437284	834867.001812	43.968167
3501.429770	834871.081181	43.973172
3501.521189	834847.763105	43.978177
3500.992662	834840.466196	43.983181
3500.760314	834829.141891	43.988186
3501.467218	834833.692206	43.993191
3501.300201	834842.068911	43.998196
3501.262182	834828.480938	44.003201
3501.038770	834808.027814	44.008205
3501.159869	834806.649515	44.013210
3501.295977	834810.220974	44.018215
3500.845406	834811.359540	44.023220
3501.080450	834808.506929	44.028225
3501.432839	834806.121474	44.033229
3501.673080	834795.500031	44.038234
3501.122498	834773.738529	44.043239
3501.489023	834778.050793	44.048244
3501.457756	834765.821031	44.053249
3501.167415	834751.592621	44.058253
3501.170585	834746.542905	44.063258
3501.042908	834745.300582	44.068263
3501.028204	834740.156553	44.073268
3501.169459	834733.434520	44.078273
3501.273076	834752.158873	44.083277
3501.319471	834734.090844	44.088282
3501.216125	834715.657762	44.093287
3500.961436	834710.551222	44.098292
3501.384979	834695.240068	44.103297
3501.535368	834709.587655	44.108301
3500.964488	834705.695758	44.113306
3501.100543	834678.777283	44.118311
3501.404655	834684.653006	44.123316
3501.613859	834678.405800	44.128321
3501.592601	834690.741118	44.133325
3501.337812	834665.728619	44.138330
3501.407329	834658.240897	44.143335
3500.836158	834657.553395	44.148340
3501.005681	834657.235621	44.153345
3501.051935	834664.802414	44.158349
3500.876951	834662.887752	44.163354
3501.024810	834653.445729	44.168359
3500.998548	834653.061456	44.173364
3501.274825	834631.558592	44.178369
3501.142824	834625.850184	44.183373
3501.436153	834627.066702	44.188378
3501.596012	834627.721467	44.193383
3501.273568	834626.121153	44.198388
3501.255754	834608.839608	44.203393
3501.064012	834599.353483	44.208397
3501.238150	834603.793052	44.213402
3500.972921	834596.163373	44.218407
3501.259063	834603.886951	44.223412
3501.400900	834598.621227	44.228417
3500.575074	834576.610723	44.233421
3500.720603	834570.082047	44.238426
3501.015388	834570.133102	44.243431
3500.880037	834571.125332	44.248436
3501.125719	834571.475375	44.253441
3501.646647	834572.947638	44.258445
3501.461318	834574.238992	44.263450
3501.416598	834570.556068	44.268455
3500.896862	834559.664593	44.273460
3501.372180	834544.830484	44.278465
3500.955607	834539.166477	44.283469
3500.811468	834556.862020	44.288474
3500.913673	834553.059013	44.293479
3501.102722	834559.147055	44.298484
3501.305807	834555.522489	44.303489
3501.450851	834555.208535	44.308493
3501.226662	834537.182212	44.313498
3501.402936	834531.231314	44.318503
3501.236015	834534.170576	44.323508
3501.241662	834527.663721	44.328513
3501.279609	834524.744682	44.333517
3501.090487	834499.527015	44.338522
3501.225330	834489.892560	44.343527
3501.045294	834484.968367	44.348532
3501.314823	834484.829162	44.353537
3501.068004	834485.838830	44.358541
3501.011386	834494.587182	44.363546
3501.272172	834485.709874	44.368551
3500.941664	834470.516023	44.373556
3501.180253	834464.069790	44.378561
3501.201396	834470.281275	44.383565
3501.163429	834480.191999	44.388570
3501.350291	834474.045180	44.393575
3501.031781	834467.200509	44.398580
3501.612594	834450.310459	44.403585
3501.684735	834448.939732	44.408589
3501.195306	834442.995705	44.413594
3501.386636	834432.284161	44.418599
3501.418898	834414.508699	44.423604
3501.625188	834400.978675	44.428609
3501.292739	834401.030676	44.433613
3501.273858	834395.498578	44.438618
3501.158855	834372.405138	44.443623
3500.618381	834368.022728	44.448628
3500.774887	834362.268969	44.453633
3501.062874	834372.420239	44.458637
3501.236719	834365.207165	44.463642
3501.445876	834369.544326	44.468647
3501.131642	834376.876513	44.473652
3501.173910	834362.692292	44.478657
3500.843743	834350.314193	44.483661
3501.115116	834335.996988	44.488666
3501.178757	834338.511872	44.493671
3500.974874	834340.194606	44.498676
3501.928610	834336.258351	44.503681
3501.140186	834344.344456	44.508685
3501.132377	834317.543960	44.513690
3500.947434	834304.948849	44.518695
3501.231097	834307.138027	44.523700
3501.388526	834296.917084	44.528705
3501.405638	834309.441404	44.533709
3500.995525	834306.592301	44.538714
3501.168688	834280.637324	44.543719
3501.452254	834278.650857	44.548724
3501.710030	834277.542399	44.553729
3501.465007	834275.832777	44.558733
3501.325768	834262.744890	44.563738
3501.186676	834251.113587	44.568743
3501.162938	834241.309305	44.573748
3501.276023	834243.719391	44.578753
3501.057617	834240.354742	44.583757
3501.003184	834242.111249	44.588762
3501.286943	834234.492400	44.593767
3501.265246	834228.475042	44.598772
3501.492955	834223.681114	44.603777
3501.308889	834224.195468	44.608781
3501.504591	834220.474745	44.613786
3501.377787	834208.744330	44.618791
3501.214458	834197.505151	44.623796
3501.332983	834195.156017	44.628801
3501.456899	834195.136679	44.633805
3501.076413	834176.745264	44.638810
3500.975789	834169.477751	44.643815
3500.870890	834157.646701	44.648820
3501.226097	834160.116082	44.653825
3500.975538	834162.485935	44.658829
3500.887349	834166.189951	44.663834
3501.217687	834165.944124	44.668839
3501.348745	834178.742236	44.673844
3501.523706	834159.681280	44.678849
3501.290824	834143.306010	44.683853
3501.387734	834134.356692	44.688858
3501.460847	834140.657505	44.693863
3501.226946	834125.447676	44.698868
3501.079595	834095.366223	44.703873
3500.992523	834102.954566	44.708877
3501.032268	834113.047971	44.713882
3501.302720	834109.315495	44.718887
3501.417506	834119.688492	44.723892
3501.017446	834097.609667	44.728897
3501.159769	834086.128277	44.733901
3501.140790	834072.924064	44.738906
3501.388754	834074.827574	44.743911
3501.010650	834073.527145	44.748916
3500.938780	834071.693285	44.753921
3501.012039	834087.316873	44.758925
3501.240623	834086.018721	44.763930
3501.642455	834057.307906	44.768935
3501.313211	834050.075986	44.773940
3501.253289	834043.578856	44.778945
3501.073205	834043.121477	44.783949
3501.157099	834042.719945	44.788954
3501.069005	834024.379469	44.793959
3500.866287	834020.235341	44.798964
3500.772027	834018.599190	44.803969
3500.794383	834020.635097	44.808973
3500.882502	834017.902196	44.813978
3501.039689	834023.898650	44.818983
3501.170356	834022.615791	44.823988
3501.348476	834017.343888	44.828993
3501.147993	834021.842449	44.833997
3500.764886	834015.687148	44.839002
3501.345360	834013.459957	44.844007
3500.988723	834005.066909	44.849012
3501.193166	833982.116259	44.854017
3501.078410	833990.874432	44.859021
3500.699675	833997.828707	44.864026
3501.169070	834003.582151	44.869031
3501.119543	834005.143735	44.874036
3501.008574	834001.956383	44.879041
3500.901344	833997.408860	44.884045
3500.728644	834000.543510	44.889050
3501.241263	833976.670646	44.894055
3501.052825	833973.689616	44.899060
3501.234393	833968.514244	44.904065
3501.221973	833971.041173	44.909069
3500.918570	833974.196268	44.914074
3500.372027	833972.339465	44.919079
3500.655884	833981.132454	44.924084
3500.883544	833974.687408	44.929089
3501.424871	833972.077868	44.934093
3501.272715	833971.713231	44.939098
3501.280693	833964.040038	44.944103
3500.884667	833958.372265	44.949108
3501.110288	833954.258247	44.954113
3501.289428	833958.309058	44.959117
3500.997050	833952.527964	44.964122
3501.306018	833952.188356	44.969127
3501.255179	833954.624183	44.974132
3501.583816	833933.304868	44.979137
3501.142813	833926.672954	44.984141
3501.254295	833924.421930	44.989146
3501.183444	833912.682189	44.994151
3501.278073	833920.533703	44.999156
3501.243308	833898.688385	45.004161
3501.289074	833891.494766	45.009165
3500.904122	833883.785779	45.014170
3501.315718	833883.624355	45.019175
3501.129612	833890.839987	45.024180
3501.054148	833897.941199	45.029185
3501.134495	833878.408569	45.034189
3501.132711	833864.909866	45.039194
3501.044813	833860.164986	45.044199
3500.858998	833863.301757	45.049204
3500.959115	833865.422677	45.054209
3501.163996	833860.826261	45.059213
3500.880022	833868.834140	45.064218
3501.215509	833868.781730	45.069223
3501.026974	833871.239115	45.074228
3500.936208	833844.255245	45.079233
3500.803140	833838.934716	45.084237
3500.672937	833832.254112	45.089242
3500.873399	833823.385260	45.094247
3501.075270	833834.424948	45.099252
3501.155036	833835.286554	45.104257
3501.140721	833831.986886	45.109261
3501.308836	833836.233735	45.114266
3501.215985	833844.891580	45.119271
3501.091416	833833.062966	45.124276
3501.312713	833820.111985	45.129281
3500.975116	833809.482017	45.134285
3500.940305	833803.466283	45.139290
3501.540790	833802.304168	45.144295
3501.117516	833804.798275	45.149300
3501.207432	833796.723594	45.154305
3501.074946	833786.741337	45.159309
3501.446132	833779.982298	45.164314
3501.585250	833774.910514	45.169319
3501.316089	833784.761407	45.174324
3501.294780	833776.218503	45.179329
3501.445894	833756.771532	45.184333
3501.153565	833757.885549	45.189338
3501.233913	833754.085456	45.194343
3500.891460	833754.915957	45.199348
3501.055494	833750.714311	45.204353
3501.402444	833762.702625	45.209357
3501.037210	833740.908393	45.214362
3501.247823	833730.969528	45.219367
3500.607879	833731.458067	45.224372
3500.919176	833721.212093	45.229377
3501.180206	833724.958909	45.234381
3500.877726	833730.639042	45.239386
3501.017475	833726.052705	45.244391
3500.748072	833732.019019	45.249396
3501.077584	833732.550247	45.254401
3501.100183	833732.352512	45.259405
3500.959150	833727.227363	45.264410
3500.793635	833705.498900	45.269415
3500.934113	833695.959412	45.274420
3500.953847	833708.484575	45.279425
3501.155668	833701.266334	45.284429
3500.817830	833707.728959	45.289434
3501.095858	833708.948062	45.294439
3500.781528	833710.356881	45.299444
3501.270738	833701.831184	45.304449
3500.930665	833707.517215	45.309453
3500.949039	833714.021269	45.314458
3501.079559	833705.163176	45.319463
3500.963100	833675.366145	45.324468
3501.046460	833673.410779	45.329473
3500.947537	833680.224560	45.334477
3500.811021	833686.170146	45.339482
3501.048591	833687.881169	45.344487
3500.979733	833692.262282	45.349492
3501.183545	833680.187797	45.354497
3501.150338	833686.699943	45.359501
3500.948107	833694.695275	45.364506
3500.791627	833679.375095	45.369511
3501.108221	833695.253020	45.374516
3501.207267	833670.666651	45.379521
3501.331571	833662.877771	45.384525
3500.776770	833656.554700	45.389530
3501.066115	833657.869164	45.394535
3501.011390	833657.586395	45.399540
3500.808576	833659.754741	45.404545
3501.199432	833657.362828	45.409549
3500.815938	833665.969245	45.414554
3501.011786	833661.956801	45.419559
3500.891587	833637.016093	45.424564
3501.182826	833624.053758	45.429569
3500.933822	833636.426841	45.434573
3501.039039	833640.586542	45.439578
3501.332658	833632.479799	45.444583
3500.865915	833645.858091	45.449588
3501.150645	833636.295959	45.454593
3501.346591	833642.578093	45.459597
3500.838805	833628.769483	45.464602
3501.261230	833599.956151	45.469607
3500.887400	833598.849185	45.474612
3501.010248	833598.344416	45.479617
3500.678966	833596.065363	45.484621
3500.849849	833604.390968	45.489626
3500.883910	833603.997198	45.494631
3501.039300	833611.839617	45.499636
3501.001381	833610.291666	45.504641
3500.999015	833615.439396	45.509645
3500.697361	833615.972180	45.514650
3500.731908	833615.481215	45.519655
3500.903422	833615.551556	45.524660
3501.148131	833610.851605	45.529665
3501.016763	833611.746248	45.534669
3501.094196	833596.292171	45.539674
3501.201840	833582.484370	45.544679
3500.615567	833580.536531	45.549684
3500.955036	833592.623474	45.554689
3500.889237	833585.641169	45.559693
3500.664324	833589.172673	45.564698
3500.806793	833587.887877	45.569703
3500.866840	833598.464571	45.574708
3501.155602	833593.951960	45.579713
3500.841029	833594.972364	45.584717
3500.759397	833598.675703	45.589722
3501.058066	833588.334360	45.594727
3501.281454	833598.302801	45.599732
3500.847688	833581.568922	45.604737
3501.188129	833575.979901	45.609741
3501.351483	833565.271190	45.614746
3501.162413	833560.056287	45.619751
3501.077479	833568.616172	45.624756
3501.292561	833570.719224	45.629761
3501.157112	833565.787305	45.634765
3500.997476	833547.165195	45.639770
3501.196820	833535.285359	45.644775
3501.828487	833538.197388	45.649780
3501.647043	833534.340959	45.654785
3501.056833	833526.275113	45.659789
3501.127953	833505.965750	45.664794
3501.164636	833494.208382	45.669799
3501.494003	833499.401476	45.674804
3500.939202	833500.070962	45.679809
3500.729006	833505.639759	45.684813
3500.927185	833501.335482	45.689818
3501.321247	833500.399823	45.694823
3500.858145	833489.886028	45.699828
3500.800797	833474.744072	45.704833
3501.247605	833464.476480	45.709837
3501.107929	833413.800563	45.714842
3500.940518	833310.196059	45.719847
3500.681795	833156.681102	45.724852
3500.863213	832956.859738	45.729857
3500.912379	832706.834352	45.734861
3500.131448	832399.228092	45.739866
3499.959641	832046.533112	45.744871
3499.087381	831648.849100	45.749876
3499.117514	831199.989956	45.754881
3498.589999	830709.889196	45.759885
3498.006129	830171.656224	45.764890
3497.634645	829575.809373	45.769895
3496.641959	828956.577321	45.774900
3496.301852	828274.385887	45.779905
3495.654315	827558.431916	45.784909
3494.764007	826796.539918	45.789914
3493.977973	825965.981224	45.794919
3493.108578	825110.717022	45.799924
3492.085959	824207.014273	45.804929
3491.545049	823249.012722	45.809933
3490.435725	822260.009071	45.814938
3489.342920	821209.145029	45.819943
3488.198768	820128.131059	45.824948
3487.555102	818998.076578	45.829953
3486.008245	817818.687862	45.834957
3484.690511	816598.038408	45.839962
3483.526436	815335.824162	45.844967
3482.173599	814036.848198	45.849972
3480.826819	812691.702660	45.854977
3479.715610	811306.366086	45.859981
3477.742228	809876.304759	45.864986
3476.818329	808418.840889	45.869991
3475.219348	806908.719709	45.874996
3473.541556	805358.738731	45.880001
3471.972391	803777.721324	45.885005
3470.284709	802151.478734	45.890010
3468.862885	800478.648631	45.895015
3466.968700	798778.697982	45.900020
3465.313259	797040.066135	45.905025
3463.438020	795267.388148	45.910029
3461.735278	793445.182112	45.915034
3460.070177	791574.847411	45.920039
3458.031785	789688.194321	45.925044
3455.811688	787769.137309	45.930049
3454.173795	785812.246825	45.935053
3451.768036	783825.093490	45.940058
3449.868464	781806.180710	45.945063
3447.806890	779748.681875	45.950068
3445.850597	777657.225539	45.955073
3443.741361	775534.420793	45.960077
3441.661543	773393.938184	45.965082
3439.200794	771202.730255	45.970087
3436.637342	768994.209704	45.975092
3434.564537	766746.485293	45.980097
3432.456810	764469.077698	45.985101
3429.844924	762173.376777	45.990106
3427.820977	759845.691134	45.995111
3425.300893	757482.821742	46.000116
3422.833272	755092.908601	46.005121
3420.290755	752673.785539	46.010125
3417.635025	750226.958068	46.015130
3415.251566	747761.690007	46.020135
3412.843908	745266.300520	46.025140
3410.249537	742739.065823	46.030145
3407.260418	740198.557559	46.035149
3404.632798	737628.883688	46.040154
3402.156505	735029.263567	46.045159
3399.355650	732412.317594	46.050164
3396.480107	729780.657393	46.055169
3393.587258	727113.000610	46.060173
3390.629199	724440.513985	46.065178
3387.755250	721720.518858	46.070183
3385.134049	719007.074329	46.075188
3381.669304	716260.889960	46.080193
3379.003934	713491.960548	46.085197
3375.748641	710709.830227	46.090202
3372.669528	707910.068984	46.095207
3369.984852	705097.232141	46.100212
3366.955043	702255.095583	46.105217
3363.934011	699403.433877	46.110221
3360.340584	696537.728833	46.115226
3357.769103	693633.644031	46.120231
3354.803120	690737.908276	46.125236
3351.410077	687806.514781	46.130241
3348.317144	684861.986405	46.135245
3345.040888	681904.392714	46.140250
3341.621423	678933.870444	46.145255
3338.763189	675948.417096	46.150260
3335.413346	672940.342141	46.155265
3332.579944	669923.036680	46.160269
3329.184249	666887.423315	46.165274
3326.083099	663840.119323	46.170279
3322.728653	660777.426702	46.175284
3319.357818	657693.579220	46.180289
3316.166722	654611.079818	46.185293
3312.633016	651502.387439	46.190298
3309.160666	648379.473961	46.195303
3305.796979	645252.490380	46.200308
3302.345532	642110.906300	46.205313
3299.474416	638953.464908	46.210317
3295.674003	635802.190233	46.215322
3292.675838	632625.096829	46.220327
3289.125052	629436.853116	46.225332
3285.346008	626243.547206	46.230337
3282.069354	623034.781821	46.235341
3278.372397	619826.181939	46.240346
3274.872131	616591.075781	46.245351
3271.527780	613365.595026	46.250356
3267.944803	610127.018590	46.255361
3264.385508	606877.103357	46.260365
3261.072145	603619.115970	46.265370
3257.735926	600363.411304	46.270375
3253.877338	597082.592776	46.275380
3250.277537	593799.412380	46.280385
3246.977990	590505.956089	46.285389
3243.667528	587217.958611	46.290394
3239.864474	583910.847263	46.295399
3236.488148	580590.087121	46.300404
3232.794084	577273.197494	46.305409
3229.125591	573940.320047	46.310413
3225.004055	570608.840525	46.315418
3221.470128	567261.287936	46.320423
3218.219104	563930.196620	46.325428
3214.331215	560589.464087	46.330433
3210.881998	557228.523436	46.335437
3207.155443	553881.505511	46.340442
3203.141481	550517.113712	46.345447
3199.623759	547160.415248	46.350452
3195.904466	543803.135794	46.355457
3192.479894	540426.390157	46.360461
3188.613198	537070.399357	46.365466
3185.049576	533684.330291	46.370471
3181.415369	530311.431749	46.375476
3177.595159	526936.531703	46.380481
3174.082225	523544.044951	46.385485
3169.858605	520154.738216	46.390490
3166.109553	516767.430887	46.395495
3162.302059	513376.016973	46.400500
3158.684332	509989.138961	46.405505
3154.959202	506589.656444	46.410509
3150.837100	503193.256702	46.415514
3147.364151	499800.192481	46.420519
3143.826266	496393.325050	46.425524
3139.657272	493006.066372	46.430529
3135.911274	489601.662734	46.435533
3132.363745	486205.252240	46.440538
3128.436283	482804.108326	46.445543
3124.915879	479408.019678	46.450548
3121.012124	476012.321807	46.455553
3117.740275	472604.480508	46.460557
3113.386846	469202.616014	46.465562
3109.586221	465787.217319	46.470567
3105.504085	462402.325624	46.475572
3101.695564	458998.905718	46.480577
3098.302218	455596.367359	46.485581
3094.490726	452199.407038	46.490586
3090.601074	448795.986734	46.495591
3086.680371	445400.890943	46.500596
3083.133727	442006.879625	46.505601
3079.260990	438608.805023	46.510605
3075.296454	435218.493337	46.515610
3071.570615	431815.739915	46.520615
3067.657361	428432.391263	46.525620
3064.090556	425041.620316	46.530625
3060.448240	421651.306603	46.535629
3056.643312	418261.321798	46.540634
3052.626707	414867.829444	46.545639
3048.604022	411477.196514	46.550644
3044.787292	408100.307867	46.555649
3041.527718	404714.597612	46.560653
3037.501622	401325.505265	46.565658
3033.674686	397951.513986	46.570663
3029.603477	394571.289167	46.575668
3025.676657	391197.164008	46.580673
3021.967754	387829.342349	46.585677
3017.435960	384460.432987	46.590682
3014.092126	381099.424509	46.595687
3010.183721	377740.991065	46.600692
3006.211678	374385.496573	46.605697
3002.560421	371030.071792	46.610701
2998.481319	367690.569405	46.615706
2994.490399	364345.783713	46.620711
2991.057557	361006.550282	46.625716
2986.847266	357674.969816	46.630721
2983.440733	354341.122884	46.635725
2978.915075	351017.011761	46.640730
2975.131973	347691.883499	46.645735
2971.284038	344382.551844	46.650740
2967.605034	341077.144850	46.655745
2963.613375	337768.297077	46.660749
2959.567335	334468.310571	46.665754
2955.367192	331165.817786	46.670759
2951.818070	327875.250555	46.675764
2947.769782	324585.836726	46.680769
2943.758364	321301.368451	46.685773
2939.826747	318031.796828	46.690778
2935.896709	314761.956030	46.695783
2931.721611	311502.580435	46.700788
2927.807992	308254.466782	46.705793
2924.157346	305018.948926	46.710797
2920.033455	301786.048845	46.715802
2916.395725	298564.406322	46.720807
2912.009963	295335.007064	46.725812
2908.338538	292118.578848	46.730817
2904.195368	288903.607521	46.735821
2900.336539	285718.521217	46.740826
2896.485443	282518.237050	46.745831
2892.298710	279333.773904	46.750836
2888.152149	276165.923199	46.755841
2884.335333	272998.914016	46.760845
2880.517573	269834.053640	46.765850
2876.301639	266696.086493	46.770855
2871.957040	263551.927805	46.775860
2867.763818	260424.866923	46.780865
2864.065387	257300.190758	46.785869
2860.119188	254194.194277	46.790874
2856.096669	251088.752297	46.795879
2851.944460	248005.298634	46.800884
2847.820390	244923.315384	46.805889
2844.367502	241847.726445	46.810893
2839.879631	238798.340352	46.815898
2835.636616	235753.138090	46.820903
2831.638376	232713.985918	46.825908
2827.791682	229687.119838	46.830913
2823.351549	226667.951534	46.835917
2818.888951	223675.754972	46.840922
2815.165042	220679.192670	46.845927
2810.852621	217708.404748	46.850932
2806.759402	214751.224255	46.855937
2802.916774	211797.057442	46.860941
2798.326693	208875.074951	46.865946
2794.275238	205944.000974	46.870951
2790.382084	203039.479653	46.875956
2785.848990	200154.993737	46.880961
2781.775148	197272.142074	46.885965
2777.610256	194415.896903	46.890970
2773.388380	191557.302626	46.895975
2769.692477	188718.199256	46.900980
2765.333838	185900.482992	46.905985
2761.409536	183081.017929	46.910989
2756.902224	180289.760295	46.915994
2753.082991	177503.445535	46.920999
2749.162749	174732.335431	46.926004
2744.747449	171981.523720	46.931009
2740.656580	169243.349258	46.936013
2736.546628	166500.112203	46.941018
2732.373377	163713.231796	46.946023
2728.321506	161012.707610	46.951028
2723.997477	158329.598993	46.956033
2719.891104	155655.979268	46.961037
2715.680250	153008.917488	46.966042
2712.025524	150351.100897	46.971047
2707.553356	147729.655579	46.976052
2703.757503	145120.602973	46.981057
2699.916944	142515.087981	46.986061
2695.823007	139932.982567	46.991066
2691.561151	137349.515820	46.996071
2687.591495	134782.036430	47.001076
2683.082503	132231.579135	47.006081
2679.101830	129693.615049	47.011085
2675.171441	127184.043944	47.016090
2671.072892	124669.270253	47.021095
2667.163872	122185.285807	47.026100
2662.681446	119697.884199	47.031105
2659.207566	117216.308902	47.036109
2654.670454	114766.648314	47.041114
2650.604933	112328.850233	47.046119
2646.548163	109901.627872	47.051124
2642.418340	107486.864228	47.056129
2638.704886	105086.479464	47.061133
2634.447595	102699.353054	47.066138
2630.311310	100319.140839	47.071143
2626.494265	97966.669686	47.076148
2622.417873	95621.922569	47.081153
2618.445394	93285.199982	47.086157
2614.228884	90964.727992	47.091162
2610.380436	88649.928236	47.096167
2606.090144	86361.040429	47.101172
2601.951505	84082.927745	47.106177
2598.714060	81815.092284	47.111181
2593.957698	79556.820704	47.116186
2590.149593	77301.593402	47.121191
2586.357447	75075.515936	47.126196
2581.528016	72860.793157	47.131201
2577.886685	70661.241656	47.136205
2573.988381	68471.741186	47.141210
2569.937661	66303.967791	47.146215
2565.876579	64132.825433	47.151220
2562.003766	61990.374449	47.156225
2557.890522	59838.861374	47.161229
2553.658253	57743.147587	47.166234
2549.582079	55635.306891	47.171239
2545.489836	53530.299896	47.176244
2541.615720	51454.183372	47.181249
2537.946909	49389.992253	47.186253
2533.328704	47339.193749	47.191258
2528.933413	45292.958910	47.196263
2524.861726	43273.176331	47.201268
2520.503331	41261.408311	47.206273
2516.425129	39269.042034	47.211277
2512.202725	37303.799000	47.216282
2508.144520	35345.764919	47.221287
2504.008543	33407.109618	47.226292
2499.484886	31500.383009	47.231297
2495.372190	29595.584934	47.236301
2490.559585	27729.542709	47.241306
2486.335755	25872.037272	47.246311
2481.878816	24041.436949	47.251316
2477.397306	22239.394864	47.256321
2472.455784	20455.995983	47.261325
2467.275727	18710.457457	47.266330
2460.480552	17039.909943	47.271335
2448.124592	15554.759741	47.276340
2436.413785	14167.846664	47.281345
2425.621114	12860.107966	47.286349
2415.529486	11667.706235	47.291354
2406.144514	10590.479953	47.296359
2397.678939	9619.528840	47.301364
2389.950353	8747.803251	47.306369
2383.061009	7986.816999	47.311373
2376.447328	7288.829544	47.316378
2370.629799	6673.748847	47.321383
2365.470585	6115.851273	47.326388
2360.347879	5632.796818	47.331393
2356.305757	5193.056850	47.336397
2352.446065	4793.170541	47.341402
2348.635819	4417.817254	47.346407
2345.147643	4086.873655	47.351412
2341.498987	3758.426319	47.356417
2338.141459	3470.260629	47.361421
2334.768067	3189.633249	47.366426
2331.753806	2918.276189	47.371431
2329.293354	2675.644335	47.376436
2326.053947	2430.283441	47.381441
2323.388525	2177.618513	47.386445
2320.569018	1938.944719	47.391450
2317.475721	1708.913868	47.396455
2314.809455	1468.583319	47.401460
2311.105283	1232.319632	47.406465
2307.952168	994.628146	47.411469
2303.966177	808.876946	47.416474
2299.176710	623.297675	47.421479
2295.136634	458.396314	47.426484
2289.772632	335.289727	47.431489
2284.180172	237.616127	47.436493
2277.317674	200.517717	47.441498
2271.264042	188.856843	47.446503
2266.810484	185.108412	47.451508
2263.142563	189.592831	47.456513
2260.874143	182.408276	47.461517
2258.269773	188.555014	47.466522
2255.765914	183.777029	47.471527
2253.084110	186.123428	47.476532
2250.199170	193.060736	47.481537
2247.227473	176.184571	47.486541
2243.722555	188.084894	47.491546
2240.808843	179.931919	47.496551
2237.496592	179.364961	47.501556
2233.666946	188.136411	47.506561
2231.097566	189.164879	47.511565
2227.859595	188.266752	47.516570
2224.717379	190.732649	47.521575
2221.337255	186.291092	47.526580
2217.538432	187.347395	47.531585
2214.461590	187.765540	47.536589
2211.372830	185.648133	47.541594
2207.607556	184.588895	47.546599
2204.756769	183.427711	47.551604
2200.787659	198.593012	47.556609
2197.867280	180.645776	47.561613
2194.515385	186.520325	47.566618
2191.064767	186.522378	47.571623
2187.902221	179.110730	47.576628
2184.154659	187.255562	47.581633
2180.632517	178.403673	47.586637
2177.591160	182.641382	47.591642
2174.266230	190.296136	47.596647
2170.767537	177.808470	47.601652
2167.262956	178.078410	47.606657
2163.609198	177.144113	47.611661
2160.525172	177.863964	47.616666
2156.892492	184.007088	47.621671
2154.020619	175.626128	47.626676
2150.222961	181.500827	47.631681
2147.190944	173.122780	47.636685
2142.925525	182.006728	47.641690
2138.978026	170.971908	47.646695
2136.487101	173.895927	47.651700
2133.393142	181.384831	47.656705
2129.100119	173.178780	47.661709
2125.526983	179.236663	47.666714
2121.787143	182.786381	47.671719
2119.268836	182.772301	47.676724
2115.578296	177.692795	47.681729
2112.684750	176.911661	47.686733
2109.193748	177.068760	47.691738
2105.616616	174.875935	47.696743
2101.836298	177.267693	47.701748
2098.520825	175.726814	47.706753
2095.199923	179.511556	47.711757
2091.555608	181.223956	47.716762
2087.753743	183.419767	47.721767
2083.939650	168.589619	47.726772
2080.627729	173.505619	47.731777
2078.032905	182.270567	47.736781
2074.203461	175.947269	47.741786
2070.553669	174.591591	47.746791
2067.676427	168.862814	47.751796
2063.689276	175.760638	47.756801
2060.463209	171.712665	47.761805
2056.986438	171.554332	47.766810
2053.052557	170.271587	47.771815
2049.700447	169.831151	47.776820
2046.665746	172.273944	47.781825
2043.413987	175.048103	47.786829
2039.155835	179.599629	47.791834
2035.830433	172.991829	47.796839
2032.552157	166.718354	47.801844
2029.044968	171.095428	47.806849
2025.530901	171.575712	47.811853
2022.050018	172.977813	47.816858
2018.538715	168.594824	47.821863
2015.605028	167.949717	47.826868
2011.451514	180.154061	47.831873
2008.244244	163.495210	47.836877
2004.932834	164.535430	47.841882
2000.970516	173.944649	47.846887
1998.222991	165.468356	47.851892
1994.047224	171.721813	47.856897
1990.948534	167.226813	47.861901
1987.208829	169.150330	47.866906
1984.085318	167.699678	47.871911
1980.434723	164.967884	47.876916
1976.562874	169.402033	47.881921
1973.503882	160.113922	47.886925
1970.013389	167.272588	47.891930
1966.419038	163.889736	47.896935
1962.875753	163.779808	47.901940
1959.204266	171.498327	47.906945
1956.104964	162.744891	47.911949
1952.393415	166.771138	47.916954
1948.762619	167.121012	47.921959
1945.530561	165.108372	47.926964
1942.019433	173.298528	47.931969
1938.823092	169.372499	47.936973
1934.911943	171.610772	47.941978
1931.330531	173.860726	47.946983
1928.281672	157.306846	47.951988
1924.926053	165.649844	47.956993
1921.590672	160.913487	47.961997
1917.652141	160.071298	47.967002
1913.862413	152.428863	47.972007
1910.387895	163.381660	47.977012
1907.064086	164.980688	47.982017
1903.605892	163.433732	47.987021
1900.391423	157.938123	47.992026
1896.452098	171.165701	47.997031
1892.910378	167.230457	48.002036
1889.279699	162.451734	48.007041
1885.912214	161.975790	48.012045
1882.869456	164.847005	48.017050
1879.497439	166.709856	48.022055
1875.934708	162.053387	48.027060
1871.976701	160.717538	48.032065
1868.990269	155.278008	48.037069
1865.144900	158.885447	48.042074
1861.605214	158.426968	48.047079
1858.141746	156.785938	48.052084
1854.868151	159.196559	48.057089
1851.760853	157.797197	48.062093
1847.328926	156.855070	48.067098
1843.709136	160.009589	48.072103
1840.946868	154.784932	48.077108
1837.407501	164.023599	48.082113
1833.883743	167.276993	48.087117
1830.271769	156.126543	48.092122
1826.613930	160.188717	48.097127
1823.559781	156.806807	48.102132
1819.657763	159.325273	48.107137
1816.360571	159.464793	48.112141
1812.505856	154.237093	48.117146
1808.893832	152.578199	48.122151
1806.203064	149.006548	48.127156
1802.173128	162.090132	48.132161
1799.101944	153.655071	48.137165
1795.473813	158.693398	48.142170
1791.932781	155.900235	48.147175
1788.539234	153.071338	48.152180
1784.352771	159.098739	48.157185
1781.416258	158.897080	48.162189
1777.952818	157.667374	48.167194
1774.224538	160.272565	48.172199
1770.908436	158.095960	48.177204
1767.396869	159.097972	48.182209
1763.847647	153.284631	48.187213
1760.523358	155.687393	48.192218
1756.925953	150.378319	48.197223
1753.453077	151.943772	48.202228
1749.928894	158.851495	48.207233
1746.271441	161.031148	48.212237
1742.967970	150.053929	48.217242
1739.429045	148.706333	48.222247
1736.057915	155.539484	48.227252
1732.126034	153.073275	48.232257
1728.760962	154.514293	48.237261
1725.425843	151.122602	48.242266
1721.827789	155.235565	48.247271
1717.986816	148.923722	48.252276
1714.638881	165.877547	48.257281
1711.382470	158.281449	48.262285
1708.038967	160.956161	48.267290
1704.379795	161.971803	48.272295
1700.958915	156.483258	48.277300
1697.101374	160.269835	48.282305
1693.880501	151.807619	48.287309
1689.866447	153.865924	48.292314
1686.969609	149.646333	48.297319
1684.145183	150.828740	48.302324
1680.317516	158.657199	48.307329
1676.702101	158.799110	48.312333
1672.883325	153.442454	48.317338
1669.201457	153.050587	48.322343
1665.856423	155.804647	48.327348
1661.916215	156.614343	48.332353
1658.961430	160.465295	48.337357
1655.558894	160.004404	48.342362
1652.007674	155.909384	48.347367
1648.746162	150.943264	48.352372
1645.033698	156.782630	48.357377
1641.238622	160.556286	48.362381
1637.773612	154.539984	48.367386
1634.219617	154.435008	48.372391
1631.274791	143.044196	48.377396
1627.419047	154.882482	48.382401
1624.077845	150.007939	48.387405
1620.588844	152.746579	48.392410
1616.706835	157.381757	48.397415
1613.295281	140.862649	48.402420
1609.686837	158.353981	48.407425
1606.324191	154.112403	48.412429
1602.874770	145.758765	48.417434
1599.281818	154.252883	48.422439
1595.969505	136.183794	48.427444
1592.508019	149.706818	48.432449
1588.885967	141.066986	48.437453
1585.432521	147.827636	48.442458
1581.709221	150.337196	48.447463
1578.863855	143.907554	48.452468
1574.880279	150.396830	48.457473
1571.495908	152.236399	48.462477
1567.836692	152.056164	48.467482
1564.398359	156.096720	48.472487
1560.741947	153.150855	48.477492
1557.246763	154.368677	48.482497
1554.100813	154.316925	48.487501
1550.809189	148.631035	48.492506
1546.832146	154.796588	48.497511
1543.285457	151.820901	48.502516
1539.911998	148.428950	48.507521
1536.104847	145.576293	48.512525
1532.626831	154.792778	48.517530
1529.248749	151.047204	48.522535
1526.217813	144.051823	48.527540
1522.708440	146.701931	48.532545
1519.026094	142.178225	48.537549
1515.173484	140.645685	48.542554
1511.636506	144.834576	48.547559
1508.683305	142.414596	48.552564
1504.786604	148.168943	48.557569
1501.085240	141.677153	48.562573
1498.130447	146.632323	48.567578
1494.666450	151.126181	48.572583
1491.046501	141.682448	48.577588
1487.226254	143.033433	48.582593
1484.054119	142.565012	48.587597
1480.477302	145.788853	48.592602
1476.595563	151.205502	48.597607
1473.404924	138.359900	48.602612
1470.114938	141.459751	48.607617
1466.646922	143.685777	48.612621
1463.125843	143.661133	48.617626
1459.291407	150.209364	48.622631
1456.218896	148.444006	48.627636
1452.366729	145.326339	48.632641
1448.971975	147.708587	48.637645
1445.798977	150.998948	48.642650
1441.965994	145.774334	48.647655
1438.394353	137.933456	48.652660
1434.359334	149.815674	48.657665
1431.000407	151.578537	48.662669
1427.556577	152.981358	48.667674
1424.248623	143.770398	48.672679
1420.863190	135.776993	48.677684
1417.636062	137.557194	48.682689
1413.924745	144.573396	48.687693
1410.368400	145.566717	48.692698
1406.829920	148.547294	48.697703
1403.415441	132.237566	48.702708
1399.649681	140.619576	48.707713
1396.361990	142.763613	48.712717
1393.384292	143.359471	48.717722
1389.112359	139.535565	48.722727
1385.843889	137.705990	48.727732
1382.276200	143.772716	48.732737
1378.696088	129.441015	48.737741
1375.567183	140.453726	48.742746
1372.019656	144.138100	48.747751
1368.597518	131.768558	48.752756
1364.766848	143.353044	48.757761
1361.365935	141.480932	48.762765
1357.933821	139.047380	48.767770
1354.182790	141.656275	48.772775
1351.338054	137.612141	48.777780
1347.341705	148.551838	48.782785
1343.772366	139.372340	48.787789
1340.348776	146.394146	48.792794
1336.608362	143.527960	48.797799
1333.337811	135.858301	48.802804
1329.444186	145.500571	48.807809
1326.075475	141.294852	48.812813
1322.731123	133.402627	48.817818
1319.414827	143.368986	48.822823
1315.932238	134.432193	48.827828
1312.456756	143.360425	48.832833
1308.832194	141.311366	48.837837
1305.250299	136.550557	48.842842
1301.165139	138.151894	48.847847
1298.442113	132.715624	48.852852
1294.734792	138.604913	48.857857
1291.477065	137.713346	48.862861
1287.814984	140.178623	48.867866
1284.345579	142.651705	48.872871
1281.271898	138.488406	48.877876
1277.077598	145.982066	48.882881
1273.682871	144.561444	48.887885
1270.385870	141.265195	48.892890
1266.603629	138.655528	48.897895
1263.510983	138.405695	48.902900
1259.796378	143.710829	48.907905
1256.402373	144.438340	48.912909
1253.065121	140.585237	48.917914
1249.004651	136.326487	48.922919
1245.852712	136.883225	48.927924
1242.358277	141.173112	48.932929
1239.170839	136.075325	48.937933
1235.213797	145.711733	48.942938
1231.321593	139.806769	48.947943
1228.329161	139.228039	48.952948
1224.417094	141.362306	48.957953
1221.293936	144.689223	48.962957
1217.851667	136.578245	48.967962
1214.439036	140.108671	48.972967
1211.333564	140.313289	48.977972
1207.043026	137.640850	48.982977
1203.332684	134.298602	48.987981
1200.076702	133.675718	48.992986
1196.479391	137.633703	48.997991
1193.495985	129.947623	49.002996
1189.749004	138.212859	49.008001
1185.786826	140.598601	49.013005
1182.817286	148.656709	49.018010
1179.253371	133.477824	49.023015
1176.224196	125.890669	49.028020
1172.213507	134.314255	49.033025
1168.774702	128.692689	49.038029
1165.034288	136.381089	49.043034
1161.204335	138.122865	49.048039
1158.449082	140.427235	49.053044
1154.528600	143.065894	49.058049
1151.250334	141.516351	49.063053
1148.012729	132.981049	49.068058
1144.244362	135.618043	49.073063
1141.187719	128.762880	49.078068
1137.097417	139.831244	49.083073
1133.559655	134.788343	49.088077
1129.917029	137.633452	49.093082
1126.357163	136.052073	49.098087
1123.159208	135.312561	49.103092
1119.759906	141.229616	49.108097
1116.249453	136.109679	49.113101
1113.057709	131.461878	49.118106
1109.051222	134.816387	49.123111
1105.775582	130.767030	49.128116
1102.236239	131.267406	49.133121
1098.865241	134.342088	49.138125
1094.950100	136.777448	49.143130
1091.743153	129.980637	49.148135
1088.265300	127.930844	49.153140
1084.912097	131.686128	49.158145
1080.917941	131.761000	49.163149
1077.621752	128.293851	49.168154
1074.041232	138.349094	49.173159
1070.913306	133.792558	49.178164
1066.830376	136.377589	49.183169
1063.842309	129.287086	49.188173
1060.259594	131.705215	49.193178
1056.289960	144.956735	49.198183
1053.014747	140.021459	49.203188
1050.149181	134.218437	49.208193
1045.861486	133.051608	49.213197
1042.321177	132.384707	49.218202
1038.845130	134.877894	49.223207
1035.648911	129.958734	49.228212
1032.234079	134.476674	49.233217
1028.710764	139.546287	49.238221
1025.351709	137.984127	49.243226
1021.690538	127.433404	49.248231
1018.152557	122.520306	49.253236
1014.309963	138.229212	49.258241
1010.856039	142.718479	49.263245
1007.773130	136.326229	49.268250
1004.005584	133.008840	49.273255
1000.465279	129.475536	49.278260
996.863487	132.599041	49.283265
993.546534	133.276613	49.288269
990.341121	131.348717	49.293274
986.883391	131.757261	49.298279
983.286720	127.707596	49.303284
979.046087	133.123660	49.308289
975.794254	132.642575	49.313293
972.586201	130.518943	49.318298
969.178821	124.405312	49.323303
965.924723	125.753271	49.328308
962.135160	127.488800	49.333313
958.553275	131.393828	49.338317
954.917848	124.800208	49.343322
951.244379	130.174934	49.348327
947.959323	125.029269	49.353332
944.306615	128.369576	49.358337
940.642549	129.550778	49.363341
937.757501	122.766904	49.368346
934.200669	132.612828	49.373351
930.884184	122.327726	49.378356
927.052693	133.352468	49.383361
923.630448	123.577484	49.388365
920.071432	127.077140	49.393370
916.495348	131.642512	49.398375
913.043449	133.252420	49.403380
909.158200	136.075486	49.408385
905.780146	127.755271	49.413389
902.105073	133.377044	49.418394
898.590051	129.390560	49.423399
895.499593	117.371117	49.428404
892.364957	131.732144	49.433409
888.804121	123.158981	49.438413
885.410072	127.683204	49.443418
881.450009	122.579985	49.448423
878.128824	118.253107	49.453428
874.696377	121.919623	49.458433
871.382805	122.846648	49.463437
867.551758	128.334664	49.468442
863.532409	128.293347	49.473447
860.469062	118.291350	49.478452
856.660476	122.798233	49.483457
853.111391	123.012319	49.488461
849.877784	116.409613	49.493466
846.387488	128.997657	49.498471
842.545218	110.477272	49.503476
839.246765	114.970718	49.508481
836.051005	112.408607	49.513485
832.976377	116.322831	49.518490
829.173129	121.964696	49.523495
825.321167	119.176307	49.528500
821.744136	124.244904	49.533505
818.225285	124.678899	49.538509
815.000754	120.865267	49.543514
811.438926	123.470042	49.548519
807.879896	120.604150	49.553524
804.659614	123.272505	49.558529
801.098622	129.740167	49.563533
797.193866	122.024510	49.568538
793.491788	127.441736	49.573543
790.108604	116.452124	49.578548
787.024373	123.740488	49.583553
783.462557	119.986012	49.588557
780.095836	129.827519	49.593562
776.569393	128.807366	49.598567
773.267281	119.513523	49.603572
769.661089	116.256393	49.608577
765.534208	122.379239	49.613581
762.336281	115.290083	49.618586
758.974190	120.024479	49.623591
755.399507	119.306123	49.628596
751.610945	119.178093	49.633601
748.536350	122.586129	49.638605
744.852473	113.203387	49.643610
741.257961	117.755883	49.648615
737.971047	109.377185	49.653620
734.349190	121.919416	49.658625
730.741035	123.553858	49.663629
727.317965	116.066531	49.668634
723.448822	117.083775	49.673639
720.408495	123.017499	49.678644
716.952039	125.805127	49.683649
713.580921	122.118894	49.688653
710.036904	118.959622	49.693658
706.095998	129.378295	49.698663
702.714249	115.019043	49.703668
699.227604	121.952828	49.708673
695.726648	121.887349	49.713677
692.406892	116.092314	49.718682
688.576475	129.277840	49.723687
685.233945	124.916413	49.728692
681.756349	124.261977	49.733697
678.341461	122.319543	49.738701
675.208248	107.851785	49.743706
671.629120	119.438199	49.748711
667.827605	111.348933	49.753716
664.012957	122.779243	49.758721
660.902756	120.861868	49.763725
657.028813	115.096690	49.768730
653.533153	124.857181	49.773735
650.346518	117.699861	49.778740
646.811245	120.385959	49.783745
643.110225	123.629536	49.788749
639.531974	121.690555	49.793754
636.191165	121.552562	49.798759
632.947414	115.530509	49.803764
629.098638	129.823097	49.808769
625.749051	116.594651	49.813773
622.477313	113.509835	49.818778
618.802965	118.546284	49.823783
615.377223	116.355635	49.828788
611.898621	115.837428	49.833793
608.258825	124.041767	49.838797
604.719949	121.647373	49.843802
600.658342	121.508383	49.848807
597.606277	121.068914	49.853812
593.899888	120.947062	49.858817
590.938929	119.699211	49.863821
587.693352	113.636334	49.868826
583.973480	115.025732	49.873831
580.113389	110.362591	49.878836
576.639048	122.347081	49.883841
572.932418	118.321141	49.888845
569.620443	119.118306	49.893850
566.179718	121.470081	49.898855
563.062582	105.484397	49.903860
559.493677	109.238831	49.908865
555.263823	117.380573	49.913869
552.187902	113.974044	49.918874
548.337570	110.818523	49.923879
545.158906	110.012916	49.928884
541.715279	108.258540	49.933889
538.241708	110.140898	49.938893
534.682827	106.354433	49.943898
531.074354	120.558785	49.948903
528.030160	115.112970	49.953908
524.340667	114.333594	49.958913
520.611015	104.948643	49.963917
517.361428	105.755037	49.968922
513.402604	111.411890	49.973927
510.257698	111.749468	49.978932
506.358416	115.622107	49.983937
502.787118	111.995789	49.988941
499.477001	113.561491	49.993946
496.155093	109.994193	49.998951
493.031645	104.529171	50.003956
489.339400	106.679919	50.008961
485.560994	112.881173	50.013965
482.505581	111.265333	50.018970
478.843684	120.646945	50.023975
475.191682	115.103360	50.028980
471.247352	112.804167	50.033985
467.728443	107.176465	50.038989
464.451337	110.771332	50.043994
460.761463	109.672498	50.048999
457.730997	111.830337	50.054004
454.169841	116.551718	50.059009
450.351930	112.135134	50.064013
447.169782	112.829749	50.069018
443.623081	115.685393	50.074023
440.276629	114.478991	50.079028
436.593677	111.616847	50.084033
433.151676	113.168428	50.089037
429.621598	102.417141	50.094042
425.735773	110.492390	50.099047
422.609164	114.427535	50.104052
419.148046	111.480031	50.109057
415.265409	112.300197	50.114061
412.016888	109.907862	50.119066
408.623851	105.760111	50.124071
405.146196	115.736154	50.129076
401.305584	116.043536	50.134081
397.890329	114.344884	50.139085
394.892716	113.558428	50.144090
391.018249	114.253937	50.149095
387.695005	107.535750	50.154100
384.226414	111.726957	50.159105
380.187840	113.656747	50.164109
376.884967	111.703215	50.169114
373.097137	120.183923	50.174119
369.692276	109.419374	50.179124
366.685104	113.990734	50.184129
362.932410	111.699538	50.189133
359.308241	106.569270	50.194138
356.009037	117.751256	50.199143
352.857931	106.681209	50.204148
349.121091	104.159744	50.209153
345.340137	105.109547	50.214157
342.514537	100.404698	50.219162
338.169914	106.182164	50.224167
335.046758	101.248678	50.229172
331.379556	110.352750	50.234177
328.137222	109.092117	50.239181
324.706921	101.761134	50.244186
320.693092	102.624038	50.249191
317.503880	101.845477	50.254196
314.214114	100.491039	50.259201
310.277056	95.653422	50.264205
306.756625	100.517172	50.269210
303.480141	104.545434	50.274215
300.115784	94.900893	50.279220
296.241841	102.781334	50.284225
292.720319	108.179942	50.289229
289.462183	102.622205	50.294234
285.893141	97.157466	50.299239
282.628540	99.813951	50.304244
279.380468	106.476374	50.309249
275.399554	102.439754	50.314253
271.824113	104.268566	50.319258
267.950336	109.276270	50.324263
265.243548	109.149827	50.329268
261.109334	102.270833	50.334273
257.663304	107.682938	50.339277
254.586332	107.677765	50.344282
250.826521	109.497502	50.349287
247.138326	112.590522	50.354292
243.855436	113.155456	50.359297
240.180616	111.456400	50.364301
236.782746	106.132547	50.369306
233.565873	120.433826	50.374311
230.229176	111.136157	50.379316
226.217164	109.853767	50.384321
222.344270	115.320102	50.389325
219.235528	104.999627	50.394330
216.106613	102.044460	50.399335
212.390352	104.366761	50.404340
208.863025	114.281041	50.409345
205.508518	114.167501	50.414349
202.209735	109.464062	50.419354
198.274076	112.975524	50.424359
194.862350	104.600801	50.429364
191.300641	111.533853	50.434369
187.568806	108.575072	50.439373
184.248591	108.253686	50.444378
180.556368	109.879364	50.449383
177.511998	96.695089	50.454388
174.167510	108.754256	50.459393
170.132159	109.414953	50.464397
166.759785	112.218079	50.469402
162.935935	108.909889	50.474407
160.022861	115.193999	50.479412
156.505981	103.520115	50.484417
152.812116	110.546652	50.489421
149.763776	101.444298	50.494426
145.860583	116.849711	50.499431
142.054386	108.897483	50.504436
138.571270	109.569755	50.509441
135.148094	108.786786	50.514445
131.945559	102.033983	50.519450
128.242856	109.631394	50.524455
124.992138	111.662494	50.529460
121.370927	104.029315	50.534465
117.639168	120.116569	50.539469
114.536810	97.779070	50.544474
110.761302	111.462367	50.549479
107.246481	112.686955	50.554484
103.919664	112.410927	50.559489
100.209683	103.209771	50.564493
96.907409	103.031142	50.569498
93.133067	106.261107	50.574503
89.481098	106.374552	50.579508
86.177449	102.867838	50.584513
82.745706	96.799545	50.589517
79.404508	101.224003	50.594522
75.521241	108.128379	50.599527
72.003488	107.043875	50.604532
69.034303	105.702581	50.609537
65.165196	106.593547	50.614541
61.628073	100.624031	50.619546
57.673511	103.385531	50.624551
54.706431	104.495847	50.629556
51.120509	115.596287	50.634561
47.400953	106.526372	50.639565
44.005763	99.753171	50.644570
40.785421	108.002709	50.649575
37.351582	107.512519	50.654580
34.241772	98.995657	50.659585
30.000159	111.321978	50.664589
26.696121	99.238324	50.669594
22.959023	106.015414	50.674599
19.682438	103.852259	50.679604
16.066826	94.728115	50.684609
12.489678	101.932567	50.689613
9.472936	98.823862	50.694618
5.612320	105.911379	50.699623
2.082027	98.960048	50.704628