Thu Aug 25 16:26:57 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.960461	108.194625	0.000000
0.782723	108.605351	0.005005
0.801275	98.228448	0.010010
0.538188	105.590729	0.015014
0.814102	89.111692	0.020019
0.811788	94.927150	0.025024
0.255713	89.506187	0.030029
0.494319	73.817628	0.035034
-0.319531	68.028932	0.040038
-0.296790	61.720015	0.045043
-0.559068	60.384924	0.050048
-0.769554	56.118388	0.055053
-0.895711	49.086153	0.060058
-1.125395	39.864991	0.065062
-1.437637	18.495226	0.070067
-1.656903	19.557866	0.075072
-2.351186	23.169002	0.080077
-2.295749	11.555663	0.085082
-2.821564	16.453366	0.090086
-3.422878	-2.336900	0.095091
-3.507525	1.181878	0.100096
-3.676430	-5.764543	0.105101
-3.646097	-10.518050	0.110106
-4.660233	-3.702529	0.115110
-4.928370	-8.330178	0.120115
-5.261021	8.771549	0.125120
-5.226501	-2.427214	0.130125
-5.177994	-4.257085	0.135130
-5.437650	-2.023851	0.140134
-5.415445	-2.970074	0.145139
-5.877281	2.531373	0.150144
-6.783004	2.211432	0.155149
-6.338280	-4.682436	0.160154
-6.624270	5.369431	0.165158
-7.231801	4.401653	0.170163
-7.404634	-3.050356	0.175168
-7.899568	-4.519831	0.180173
-7.676254	-12.606547	0.185178
-8.422278	0.320493	0.190182
-8.397099	-5.501561	0.195187
-8.548444	-4.854526	0.200192
-9.324806	-11.076177	0.205197
-9.526604	-4.156980	0.210202
-9.417150	0.660167	0.215206
-9.584250	-9.456630	0.220211
-9.669620	-11.569245	0.225216
-10.118705	-2.361864	0.230221
-9.802303	-4.350768	0.235226
-10.330810	-2.398115	0.240230
-11.198431	-5.489157	0.245235
-11.032848	-0.054379	0.250240
-11.441320	5.400742	0.255245
-11.822969	-2.015385	0.260250
-12.250896	2.009596	0.265254
-12.416166	-1.890685	0.270259
-12.438144	2.909090	0.275264
-12.426783	-2.746284	0.280269
-12.278816	-3.712211	0.285274
-12.800958	6.553828	0.290278
-13.355081	-4.410333	0.295283
-13.547250	-0.862055	0.300288
-14.104823	2.161343	0.305293
-14.361775	-11.076668	0.310298
-14.589386	-1.878677	0.315302
-15.102423	-2.513245	0.320307
-15.204979	-3.939795	0.325312
-15.185025	-8.970088	0.330317
-15.406528	-6.834582	0.335322
-15.775722	2.913944	0.340326
-15.891400	-4.885542	0.345331
-15.915415	0.341660	0.350336
-16.215345	1.176492	0.355341
-16.401849	-7.671758	0.360346
-16.978116	7.218699	0.365350
-17.208136	0.212250	0.370355
-17.151238	-6.389897	0.375360
-17.897706	4.920531	0.380365
-18.158412	-10.025327	0.385370
-18.644868	8.941809	0.390374
-18.569822	-2.412000	0.395379
-18.848408	-1.982311	0.400384
-18.862862	-0.856850	0.405389
-18.493732	-3.610157	0.410394
-19.720160	0.059044	0.415398
-19.698936	-1.503960	0.420403
-20.296171	-3.023845	0.425408
-20.561828	-0.979497	0.430413
-20.400393	0.931494	0.435418
-20.587973	6.045120	0.440422
-20.584779	-7.524720	0.445427
-21.210762	2.320987	0.450432
-21.678908	-4.803174	0.455437
-21.402342	1.386174	0.460442
-21.839866	8.339147	0.465446
-21.655387	-7.084593	0.470451
-22.402372	-10.798814	0.475456
-22.788342	-0.516150	0.480461
-22.830536	6.735550	0.485466
-23.211350	1.986349	0.490470
-23.181647	-5.377169	0.495475
-23.774134	-6.287190	0.500480
-24.442735	2.337653	0.505485
-24.155071	-5.737001	0.510490
-24.322392	-2.939265	0.515494
-24.542241	5.779784	0.520499
-24.748605	2.977440	0.525504
-25.128519	-0.345042	0.530509
-25.845861	4.272619	0.535514
-26.113449	-0.105179	0.540518
-26.021898	3.376500	0.545523
-26.014569	7.716101	0.550528
-26.049948	5.845589	0.555533
-26.236719	-5.239403	0.560538
-27.671534	-3.340899	0.565542
-27.950320	-8.707198	0.570547
-27.565780	3.818075	0.575552
-28.061399	2.105097	0.580557
-27.930466	-4.514977	0.585562
-27.732479	0.455977	0.590566
-28.213017	-10.389994	0.595571
-28.071546	-3.967509	0.600576
-28.737642	-0.322827	0.605581
-28.899366	-1.844510	0.610586
-29.473548	5.730989	0.615590
-30.181968	-4.244044	0.620595
-30.284001	-1.978560	0.625600
-30.569524	-5.021600	0.630605
-30.532620	-4.473664	0.635610
-30.964192	1.130609	0.640614
-30.863751	-0.726382	0.645619
-31.066853	-2.314348	0.650624
-31.209938	-2.488023	0.655629
-31.506264	-5.592646	0.660634
-32.100140	-0.456491	0.665638
-32.598368	-4.225507	0.670643
-32.294374	0.077101	0.675648
-32.729007	6.874595	0.680653
-32.702860	-7.540403	0.685658
-33.319999	-3.719894	0.690662
-33.633320	2.710577	0.695667
-33.456717	-2.989670	0.700672
-33.584090	-2.612148	0.705677
-34.281670	-2.907750	0.710682
-34.891875	-5.865116	0.715686
-35.152995	2.379505	0.720691
-34.695342	0.612078	0.725696
-35.347592	-0.646085	0.730701
-34.872395	-11.110290	0.735706
-35.488678	0.024712	0.740710
-35.803436	-7.401891	0.745715
-35.969723	7.940021	0.750720
-36.215220	-1.541232	0.755725
-36.159942	-0.622850	0.760730
-37.224204	8.082973	0.765734
-37.159306	3.279755	0.770739
-37.462869	-8.293137	0.775744
-37.737188	4.686547	0.780749
-38.012691	2.224070	0.785754
-38.440599	0.747257	0.790758
-38.717342	-1.164530	0.795763
-39.094935	0.580981	0.800768
-39.261322	6.899845	0.805773
-39.420959	1.435780	0.810778
-39.520210	6.086310	0.815782
-39.532110	3.607840	0.820787
-39.352121	-6.942991	0.825792
-40.032729	-2.305777	0.830797
-40.485672	-2.196783	0.835802
-40.938274	0.452663	0.840806
-41.384750	-2.925827	0.845811
-40.781192	-2.795709	0.850816
-41.427145	0.988187	0.855821
-41.803844	-6.124990	0.860826
-42.176875	4.962410	0.865830
-42.038758	-4.243588	0.870835
-42.052892	-6.114263	0.875840
-42.822125	4.143033	0.880845
-43.274148	-5.941773	0.885850
-43.735647	0.138589	0.890854
-43.676552	-4.220790	0.895859
-43.764195	-5.618038	0.900864
-44.214611	3.187756	0.905869
-43.832560	-2.544682	0.910874
-43.934922	1.679227	0.915878
-44.706690	-2.932784	0.920883
-45.112830	-1.356808	0.925888
-45.246803	3.653504	0.930893
-45.257132	0.181366	0.935898
-45.596347	6.299518	0.940902
-46.574070	-2.845539	0.945907
-46.728271	-6.510270	0.950912
-46.634379	-3.867359	0.955917
-46.697805	-6.065670	0.960922
-46.816981	0.679230	0.965926
-46.977169	-1.953176	0.970931
-46.853203	-15.475491	0.975936
-47.802180	-0.352637	0.980941
-48.105334	-10.134899	0.985946
-48.429453	-8.451551	0.990950
-48.616341	-10.462838	0.995955
-48.334899	-0.800443	1.000960
-49.319396	0.198600	1.005965
-49.712200	-6.855104	1.010970
-50.006005	-7.223463	1.015974
-50.037304	0.564366	1.020979
-49.525278	-5.318150	1.025984
-50.181109	-5.750007	1.030989
-50.165533	-0.313874	1.035994
-50.722818	7.705070	1.040998
-51.166797	-4.054631	1.046003
-51.527899	2.089096	1.051008
-51.543508	0.380003	1.056013
-51.223125	-6.269754	1.061018
-51.474579	-1.437189	1.066022
-51.866870	0.788353	1.071027
-52.184519	-3.160817	1.076032
-53.022544	-1.134354	1.081037
-53.686561	-5.554437	1.086042
-53.102408	-2.520106	1.091046
-53.562961	-3.862087	1.096051
-54.081525	-4.609682	1.101056
-54.336407	-1.494505	1.106061
-54.373952	0.333766	1.111066
-54.281809	2.388492	1.116070
-54.357409	-2.702759	1.121075
-55.037214	-2.140601	1.126080
-55.747358	0.960489	1.131085
-55.646311	2.156438	1.136090
-55.474410	1.958719	1.141094
-55.921834	-0.742575	1.146099
-56.027983	-7.812720	1.151104
-57.006529	5.176067	1.156109
-56.935954	-2.627290	1.161114
-57.123111	6.001213	1.166118
-57.047636	-1.303037	1.171123
-56.763219	-6.197596	1.176128
-57.688527	-6.349946	1.181133
-58.024758	-9.160411	1.186138
-58.259381	-6.649524	1.191142
-58.657732	-2.572229	1.196147
-58.891914	-5.661277	1.201152
-58.960961	-6.049034	1.206157
-59.279055	-15.306929	1.211162
-60.115720	-1.565256	1.216166
-60.039285	-1.994791	1.221171
-60.126516	-0.769341	1.226176
-60.717312	6.106406	1.231181
-60.265938	-4.249665	1.236186
-60.278480	-0.289769	1.241190
-60.507104	1.600080	1.246195
-60.990246	-4.518813	1.251200
-61.827279	-6.975560	1.256205
-61.791435	-3.244710	1.261210
-61.975572	-1.292229	1.266214
-62.203017	-6.046473	1.271219
-62.934361	-7.906010	1.276224
-63.126211	0.894069	1.281229
-63.574200	-15.230992	1.286234
-63.483177	4.503030	1.291238
-63.008561	7.079960	1.296243
-63.065790	-5.999516	1.301248
-63.764521	4.585257	1.306253
-64.515782	-6.556814	1.311258
-64.578566	4.133958	1.316262
-64.611026	7.381965	1.321267
-64.879369	4.620973	1.326272
-65.436039	3.771781	1.331277
-65.854314	5.033283	1.336282
-66.459525	4.729537	1.341286
-67.242106	5.190741	1.346291
-66.341562	2.876188	1.351296
-66.373121	10.328701	1.356301
-66.665948	9.773527	1.361306
-66.228321	10.366243	1.366310
-66.521633	13.996811	1.371315
-67.150355	2.367296	1.376320
-67.668400	6.662665	1.381325
-68.100238	-0.982875	1.386330
-68.565377	-3.380835	1.391334
-68.997825	-2.079147	1.396339
-68.943979	13.484539	1.401344
-69.044872	2.784725	1.406349
-69.137881	-2.231031	1.411354
-69.613195	-4.225598	1.416358
-69.520116	-1.911591	1.421363
-69.950383	-8.184300	1.426368
-70.550087	2.191966	1.431373
-70.495033	-7.614784	1.436378
-70.842789	-1.919241	1.441382
-70.826462	6.731162	1.446387
-71.550510	-5.579439	1.451392
-72.094556	1.399713	1.456397
-71.972993	2.092572	1.461402
-72.129217	2.515745	1.466406
-72.247095	1.332043	1.471411
-72.150075	-4.880917	1.476416
-72.593600	2.500101	1.481421
-73.001110	1.140318	1.486426
-73.583945	-6.541671	1.491430
-74.406153	-7.216377	1.496435
-74.199881	-7.327732	1.501440
-74.274063	-2.152784	1.506445
-74.031591	10.290343	1.511450
-74.365171	5.666622	1.516454
-74.139202	8.640018	1.521459
-74.852350	-1.846799	1.526464
-75.368302	9.028877	1.531469
-75.374183	-1.834517	1.536474
-75.535078	3.002841	1.541478
-76.328608	11.273940	1.546483
-76.363614	1.168084	1.551488
-76.933202	16.139756	1.556493
-76.745138	-3.764439	1.561498
-77.051997	3.180712	1.566502
-77.022285	2.435795	1.571507
-77.469488	-11.550683	1.576512
-78.386643	-0.137583	1.581517
-77.996806	-1.840602	1.586522
-78.171383	-5.676146	1.591526
-78.460417	-3.485765	1.596531
-78.819338	-12.329136	1.601536
-79.286480	4.562697	1.606541
-79.604095	-4.084670	1.611546
-79.924247	3.498481	1.616550
-80.275396	2.927136	1.621555
-79.802819	-6.375557	1.626560
-80.304770	4.627637	1.631565
-80.018070	0.248413	1.636570
-80.865756	-5.405231	1.641574
-81.624152	-4.074616	1.646579
-81.639699	-2.471256	1.651584
-81.803266	4.502064	1.656589
-81.527281	1.813970	1.661594
-81.515388	-0.620770	1.666598
-82.080380	2.612602	1.671603
-82.293139	-6.152434	1.676608
-82.845026	5.412244	1.681613
-82.934208	-8.317122	1.686618
-82.766716	0.470944	1.691622
-83.491158	-7.742514	1.696627
-83.690054	-14.200170	1.701632
-84.123466	-0.176833	1.706637
-84.126690	-2.409887	1.711642
-84.926430	-0.525462	1.716646
-85.215651	2.702665	1.721651
-85.239125	-6.436880	1.726656
-85.794819	-1.613592	1.731661
-85.568757	-4.645041	1.736666
-85.541968	1.096220	1.741670
-85.679737	4.101298	1.746675
-86.182132	-4.570899	1.751680
-87.006487	0.012912	1.756685
-86.905184	-3.625414	1.761690
-87.113638	-3.187730	1.766694
-87.234327	-6.452747	1.771699
-87.054341	-1.425193	1.776704
-87.952855	-3.179440	1.781709
-88.346789	-12.321046	1.786714
-88.570157	-5.218137	1.791718
-88.560077	-8.101847	1.796723
-88.785850	-12.492517	1.801728
-88.735242	-0.117412	1.806733
-89.484911	-0.091635	1.811738
-89.803839	-0.715485	1.816742
-90.014381	-0.385041	1.821747
-90.289339	-8.934684	1.826752
-90.365568	-2.228154	1.831757
-90.175505	-10.926591	1.836762
-91.210045	-5.730879	1.841766
-91.783859	-2.815666	1.846771
-91.589456	-6.895687	1.851776
-91.912693	0.248183	1.856781
-91.839908	-5.350372	1.861786
-91.697429	-0.823144	1.866790
-92.189254	-7.222246	1.871795
-92.243411	-7.979332	1.876800
-92.756268	7.739582	1.881805
-92.941822	-9.723744	1.886810
-93.110440	0.721014	1.891814
-93.648558	1.969658	1.896819
-93.988990	-0.036551	1.901824
-94.539869	2.286609	1.906829
-95.084868	-0.282334	1.911834
-94.980041	7.683482	1.916838
-95.388589	-7.593542	1.921843
-94.649605	6.853537	1.926848
-94.700079	7.744197	1.931853
-94.901859	2.144369	1.936858
-95.793383	2.356890	1.941862
-96.178805	4.537065	1.946867
-95.742258	-5.712277	1.951872
-96.953693	3.908790	1.956877
-97.335353	2.215926	1.961882
-97.431774	-0.451779	1.966886
-97.832862	2.180105	1.971891
-97.871017	2.027955	1.976896
-97.703217	-0.339466	1.981901
-97.795837	2.475039	1.986906
-98.004301	4.244671	1.991910
-98.347792	-1.494302	1.996915
-99.000178	-3.082358	2.006912
-98.911382	-1.113100	2.016909
-98.394075	-2.223580	2.026906
-97.610805	-5.621716	2.036902
-97.018255	-2.787383	2.046899
-96.345775	-1.948628	2.056896
-96.329608	-6.351139	2.066893
-95.628620	-4.104004	2.076890
-95.340501	3.003898	2.086886
-94.612362	-2.866000	2.096883
-94.096154	-3.903447	2.106880
-94.065093	-5.447754	2.116877
-93.012524	-5.517530	2.126874
-92.558020	-7.067999	2.136870
-92.358742	-2.040103	2.146867
-91.412172	-1.440700	2.156864
-91.251433	-4.171082	2.166861
-90.756141	-2.233841	2.176858
-90.204200	-4.483825	2.186854
-89.624288	-3.605222	2.196851
-88.962110	-2.086939	2.206848
-88.215580	-4.525805	2.216845
-88.313421	-0.208461	2.226842
-87.930077	0.114897	2.236838
-87.216854	-3.360961	2.246835
-86.638534	4.154468	2.256832
-86.119240	3.645563	2.266829
-85.736482	1.282704	2.276826
-85.233181	2.265178	2.286822
-84.577933	3.068621	2.296819
-84.301078	9.110737	2.306816
-83.486118	6.667484	2.316813
-82.944576	0.126736	2.326810
-82.689548	1.499741	2.336806
-81.680868	0.191891	2.346803
-81.632789	4.353324	2.356800
-81.460561	7.655833	2.366797
-80.714438	4.155811	2.376794
-80.181176	4.309959	2.386790
-79.758204	13.044002	2.396787
-78.945141	3.264379	2.406784
-78.596397	-1.282112	2.416781
-78.336564	4.239980	2.426778
-78.014195	8.627700	2.436774
-76.532748	2.006202	2.446771
-76.359668	8.555591	2.456768
-76.281713	4.732609	2.466765
-75.588706	1.608378	2.476762
-74.670701	-0.429700	2.486758
-74.608641	-4.465600	2.496755
-74.512217	2.675508	2.506752
-73.490574	1.733095	2.516749
-73.043804	4.786678	2.526746
-72.760493	8.261851	2.536742
-71.548870	5.430160	2.546739
-71.500115	3.087958	2.556736
-71.182358	6.627425	2.566733
-70.768694	5.878478	2.576730
-69.975551	-3.511546	2.586726
-69.739730	-1.711044	2.596723
-69.340612	7.305503	2.606720
-68.726858	0.984690	2.616717
-67.930213	-2.073415	2.626714
-67.417621	5.765930	2.636710
-67.066443	4.770181	2.646707
-66.612021	0.283158	2.656704
-66.236506	1.741823	2.666701
-65.622404	4.411224	2.676698
-64.471804	0.198424	2.686694
-64.664750	-3.354026	2.696691
-64.246366	0.448442	2.706688
-63.875911	2.154989	2.716685
-62.934821	1.317065	2.726682
-62.746459	1.601283	2.736678
-61.921845	0.008663	2.746675
-60.876896	1.134352	2.756672
-60.797641	-0.765967	2.766669
-60.951028	-1.812537	2.776666
-59.936595	-5.595350	2.786662
-60.099672	-3.805205	2.796659
-58.918186	-3.990211	2.806656
-58.104488	-3.696270	2.816653
-58.269410	-1.440166	2.826650
-57.935876	1.735698	2.836646
-56.922305	-7.593828	2.846643
-56.549769	-0.784254	2.856640
-55.574433	-0.655023	2.866637
-55.245452	-6.408522	2.876634
-55.343594	-10.758277	2.886630
-54.827469	-7.769415	2.896627
-53.914819	-9.211101	2.906624
-53.648231	-11.118597	2.916621
-52.975323	-2.458567	2.926618
-52.442558	3.353384	2.936614
-52.233357	5.161226	2.946611
-51.353709	0.572730	2.956608
-50.879802	-8.868641	2.966605
-50.649194	-5.188807	2.976602
-50.165017	7.153294	2.986598
-49.530280	5.175441	2.996595
-49.185317	2.495387	3.006592
-48.395267	-1.391653	3.016589
-48.361822	-6.186514	3.026586
-47.555992	-3.173352	3.036582
-46.541721	2.531475	3.046579
-46.375035	-4.286325	3.056576
-46.392776	-5.100723	3.066573
-45.495523	-5.532631	3.076570
-45.227993	-1.351730	3.086566
-44.179006	-0.175987	3.096563
-43.465590	-3.502985	3.106560
-43.271780	3.109680	3.116557
-43.307563	0.353068	3.126554
-42.960713	-7.582690	3.136550
-41.952747	-5.548376	3.146547
-41.537857	-4.757954	3.156544
-40.463790	-5.363285	3.166541
-40.206788	-0.737240	3.176538
-40.179153	2.008215	3.186534
-39.794085	-0.712968	3.196531
-38.696858	-9.377687	3.206528
-38.549270	-8.063875	3.216525
-38.413320	-4.743011	3.226522
-37.738021	-3.765308	3.236518
-37.377759	-2.627370	3.246515
-36.329331	1.900014	3.256512
-36.022539	-5.170990	3.266509
-35.190714	-0.549479	3.276506
-34.949433	3.306083	3.286502
-34.730597	-4.023572	3.296499
-33.662952	-5.673276	3.306496
-33.371526	2.739255	3.316493
-33.186403	9.774605	3.326490
-32.896402	-0.445750	3.336486
-32.162272	2.147826	3.346483
-30.970598	3.196677	3.356480
-30.746446	0.928362	3.366477
-30.270369	5.079757	3.376474
-30.054779	2.749427	3.386470
-29.606959	6.696174	3.396467
-28.865354	7.685664	3.406464
-28.736829	2.236002	3.416461
-27.809801	4.938740	3.426458
-27.234805	6.138068	3.436454
-27.250980	3.476585	3.446451
-26.665371	3.647877	3.456448
-26.004745	8.055461	3.466445
-25.327379	9.710755	3.476442
-24.681833	3.464157	3.486438
-24.541091	7.535046	3.496435
-24.251738	6.586999	3.506432
-23.368884	7.224905	3.516429
-23.035450	8.788368	3.526426
-22.250399	8.019246	3.536422
-21.695015	8.296645	3.546419
-21.468563	2.308949	3.556416
-21.076214	3.362665	3.566413
-20.395349	0.417738	3.576410
-19.965642	11.415723	3.586406
-19.800279	8.792319	3.596403
-18.842152	11.262103	3.606400
-18.366774	3.977779	3.616397
-17.638285	7.864712	3.626394
-17.008774	-0.210372	3.636390
-17.362772	4.330844	3.646387
-16.577024	-1.009549	3.656384
-15.737322	-5.100770	3.666381
-15.239495	3.754596	3.676378
-15.255061	2.236600	3.686374
-14.657993	3.841120	3.696371
-13.781017	6.225416	3.706368
-13.656625	4.764686	3.716365
-12.825029	9.604818	3.726362
-12.509277	6.387644	3.736358
-11.516788	12.618583	3.746355
-11.299515	7.177189	3.756352
-11.201493	3.883256	3.766349
-10.438650	9.161816	3.776346
-9.705318	6.215003	3.786342
-9.834372	3.479339	3.796339
-8.556982	10.853571	3.806336
-7.948585	2.734276	3.816333
-8.054482	6.539700	3.826330
-7.836926	0.540727	3.836326
-7.144723	6.384723	3.846323
-6.499949	6.527739	3.856320
-5.577983	6.890254	3.866317
-5.317957	8.138934	3.876314
-5.001846	5.732665	3.886310
-4.926861	5.971293	3.896307
-4.016580	13.602620	3.906304
-3.597862	23.442914	3.916301
-3.236343	29.500289	3.926298
-2.769375	45.342399	3.936294
-2.309699	52.347422	3.946291
-1.748306	63.068215	3.956288
-1.422103	77.662109	3.966285
-0.635478	85.309675	3.976282
-0.202729	103.846690	3.986278
0.000000	112.435776	3.991283
0.030527	111.586321	3.996288
0.395510	119.343752	4.001293
0.342235	126.214420	4.006298
0.371406	121.423094	4.011302
0.544806	129.485797	4.016307
0.777190	135.470142	4.021312
1.087838	142.663451	4.026317
0.901003	149.251329	4.031322
1.128059	142.714216	4.036326
0.755573	134.091189	4.041331
0.890653	143.896825	4.046336
0.999733	144.537863	4.051341
0.990019	156.353054	4.056346
1.170623	149.364467	4.061350
0.983241	146.530651	4.066355
0.745930	148.051712	4.071360
0.953394	138.635454	4.076365
0.930175	149.133455	4.081370
1.176074	142.251700	4.086374
1.151773	157.489239	4.091379
1.166529	149.337049	4.096384
1.119751	142.355617	4.101389
1.000555	144.576352	4.106394
1.365462	146.480790	4.111398
1.080015	138.900831	4.116403
0.899524	129.580164	4.121408
1.038888	132.320378	4.126413
0.828891	138.446804	4.131418
1.387913	150.005200	4.136422
1.480876	159.918685	4.141427
0.923325	153.798734	4.146432
1.375621	151.753719	4.151437
0.859907	157.462974	4.156442
0.985431	152.685017	4.161446
1.191098	168.753414	4.166451
0.971736	161.846471	4.171456
1.375978	156.331972	4.176461
0.888114	155.699780	4.181466
1.066534	156.083178	4.186470
1.106013	159.006727	4.191475
0.821722	163.278162	4.196480
1.351606	157.142856	4.201485
1.075621	157.037458	4.206490
1.317196	160.090696	4.211494
1.388528	160.256752	4.216499
1.374038	164.884553	4.221504
1.523299	158.562106	4.226509
1.201217	162.013711	4.231514
1.592635	158.968983	4.236518
1.341423	160.179007	4.241523
1.059267	162.757476	4.246528
1.788404	173.172413	4.251533
1.277152	168.453094	4.256538
1.357150	168.668412	4.261542
1.779197	176.046764	4.266547
1.731265	175.450047	4.271552
1.719552	164.223622	4.276557
1.508457	162.029442	4.281562
1.373952	153.233076	4.286566
1.306935	160.760815	4.291571
1.438747	155.213070	4.296576
1.916842	165.955242	4.301581
1.248049	166.847874	4.306586
1.359502	170.899115	4.311590
1.554909	172.934519	4.316595
1.444651	177.023663	4.321600
2.188526	172.129835	4.326605
1.689849	179.171550	4.331610
1.619136	177.565987	4.336614
1.408998	179.895890	4.341619
1.528001	170.778216	4.346624
1.827989	171.395671	4.351629
1.545727	185.771969	4.356634
1.826381	185.569866	4.361638
1.930493	181.554568	4.366643
1.751839	177.143808	4.371648
1.969018	174.695860	4.376653
1.964084	185.751011	4.381658
2.157056	172.698634	4.386662
1.432229	163.330357	4.391667
1.340616	164.683057	4.396672
1.901012	170.062356	4.401677
1.788625	173.259642	4.406682
1.911012	184.199928	4.411686
1.615530	184.670234	4.416691
1.595350	186.514787	4.421696
1.858091	186.296507	4.426701
1.888878	181.495421	4.431706
1.837532	180.642971	4.436710
1.780178	189.662522	4.441715
1.767048	187.063994	4.446720
1.937354	181.358347	4.451725
1.762153	184.850219	4.456730
1.952907	186.535171	4.461734
1.515508	179.399788	4.466739
1.629936	186.513125	4.471744
2.173546	175.892556	4.476749
1.754957	181.355643	4.481754
2.058583	190.147791	4.486758
2.251188	200.580369	4.491763
1.888361	195.170224	4.496768
2.366472	187.426316	4.501773
1.891225	187.738123	4.506778
1.923809	185.565873	4.511782
2.081870	197.696495	4.516787
1.995287	199.931111	4.521792
1.979909	208.267040	4.526797
2.071626	198.138047	4.531802
2.365758	201.455145	4.536806
2.323130	198.835926	4.541811
1.990698	207.961862	4.546816
2.708623	197.886617	4.551821
2.539998	195.736400	4.556826
1.970075	190.747852	4.561830
2.118452	188.339157	4.566835
2.025909	208.288842	4.571840
2.281080	199.175129	4.576845
1.739810	202.338377	4.581850
2.050867	205.712936	4.586854
2.310335	205.605902	4.591859
2.208109	202.856813	4.596864
2.409273	202.395076	4.601869
1.935966	211.489302	4.606874
2.109916	207.937627	4.611878
2.047067	208.846054	4.616883
2.461370	203.602052	4.621888
2.592733	204.960948	4.626893
2.351164	205.982800	4.631898
2.350316	193.628339	4.636902
2.267328	198.330157	4.641907
2.504205	199.625063	4.646912
2.509170	202.041491	4.651917
2.325763	202.842255	4.656922
2.624038	206.244127	4.661926
2.682793	208.386368	4.666931
2.364688	203.022998	4.671936
2.572646	203.781426	4.676941
2.129125	199.658936	4.681946
2.398945	209.108134	4.686950
2.360043	210.838562	4.691955
2.492621	217.278341	4.696960
2.527720	221.022013	4.701965
2.656599	230.354097	4.706970
2.445520	226.622295	4.711974
2.598584	230.935955	4.716979
2.701004	236.099123	4.721984
2.575817	222.400521	4.726989
2.677329	235.391094	4.731994
2.605079	225.914210	4.736998
2.545289	226.926564	4.742003
2.504752	236.649034	4.747008
2.635895	232.439661	4.752013
2.588364	231.899829	4.757018
2.708591	226.344385	4.762022
2.936431	229.402951	4.767027
2.616989	233.366693	4.772032
2.650540	230.545705	4.777037
2.748379	239.721303	4.782042
2.713446	229.007848	4.787046
2.765435	226.009963	4.792051
2.739987	230.879947	4.797056
3.016369	226.347258	4.802061
2.525124	235.903059	4.807066
2.785754	229.180317	4.812070
2.696715	237.828363	4.817075
2.392742	244.548527	4.822080
2.896861	222.348243	4.827085
2.698511	234.363888	4.832090
2.867179	229.575987	4.837094
2.889459	242.215141	4.842099
2.862508	240.862148	4.847104
2.972411	235.352613	4.852109
3.062863	237.410796	4.857114
3.157861	231.881450	4.862118
3.097313	229.904124	4.867123
2.699556	239.195338	4.872128
3.215953	230.426665	4.877133
2.844261	247.249994	4.882138
2.867387	243.820022	4.887142
3.282301	239.502910	4.892147
2.973964	248.080916	4.897152
3.080263	244.843560	4.902157
3.089464	253.381307	4.907162
3.191170	254.608810	4.912166
3.140787	253.547394	4.917171
2.835504	252.798005	4.922176
3.120610	245.413349	4.927181
2.735409	265.861376	4.932186
3.198271	264.368361	4.937190
3.314239	272.054142	4.942195
3.424612	267.749937	4.947200
3.579468	259.253037	4.952205
3.006445	253.591065	4.957210
3.106650	259.320910	4.962214
3.193874	257.320427	4.967219
3.454132	265.508791	4.972224
3.465289	261.764309	4.977229
3.209360	260.599054	4.982234
3.259966	253.716217	4.987238
3.385920	261.172634	4.992243
3.030538	258.466365	4.997248
3.184771	253.146035	5.002253
3.034804	262.395273	5.007258
3.017269	266.890698	5.012262
3.349377	264.222247	5.017267
2.764511	270.657394	5.022272
3.624486	272.651960	5.027277
3.665220	265.982641	5.032282
3.232889	266.730658	5.037286
3.159655	264.157355	5.042291
3.487061	268.962573	5.047296
3.279275	266.154082	5.052301
3.211566	275.279704	5.057306
3.350537	265.288805	5.062310
3.453945	266.544516	5.067315
3.303223	265.071706	5.072320
3.252892	262.403064	5.077325
3.370291	266.152833	5.082330
3.645987	280.163370	5.087334
3.664451	288.848382	5.092339
3.501436	291.357582	5.097344
3.671001	294.431617	5.102349
3.972109	289.597639	5.107354
3.534124	280.190685	5.112358
3.563694	266.018540	5.117363
3.102279	265.271466	5.122368
3.702863	278.493929	5.127373
3.639941	291.779231	5.132378
3.355289	288.827752	5.137382
3.857416	281.560942	5.142387
3.777623	293.393532	5.147392
3.733005	283.377602	5.152397
3.904632	286.407020	5.157402
3.853853	285.279224	5.162406
4.174763	281.831062	5.167411
3.764879	272.236208	5.172416
3.651137	262.471570	5.177421
3.574865	269.194032	5.182426
3.597213	278.909836	5.187430
3.487748	289.994084	5.192435
3.514995	293.773803	5.197440
3.932996	285.216678	5.202445
3.725544	283.028240	5.207450
3.862111	290.505153	5.212454
3.941150	280.194599	5.217459
3.467789	292.822858	5.222464
3.817513	290.765425	5.227469
3.621755	288.366342	5.232474
3.687477	284.945507	5.237478
4.163870	286.870459	5.242483
4.051267	290.925194	5.247488
3.947566	292.412678	5.252493
3.823885	296.946888	5.257498
4.051470	290.001505	5.262502
4.053445	290.029730	5.267507
4.050208	288.461042	5.272512
4.027649	285.835502	5.277517
4.165820	298.690660	5.282522
3.861298	289.762674	5.287526
3.780464	286.937452	5.292531
3.695690	295.426668	5.297536
3.900617	286.153101	5.302541
4.083569	295.935501	5.307546
3.941114	299.172322	5.312550
4.275418	308.855084	5.317555
4.019672	311.828077	5.322560
4.211613	312.430828	5.327565
3.822308	311.466805	5.332570
4.004077	318.250098	5.337574
4.323202	318.159027	5.342579
3.988424	312.440724	5.347584
4.183016	307.743656	5.352589
3.943026	306.246863	5.357594
4.043703	308.673619	5.362598
4.169405	314.060958	5.367603
4.088692	313.997732	5.372608
4.345908	307.882949	5.377613
4.250784	311.745122	5.382618
4.245959	318.719006	5.387622
4.308055	313.751623	5.392627
3.959926	315.207801	5.397632
3.902559	310.730547	5.402637
3.943667	314.903577	5.407642
4.436247	311.925232	5.412646
4.546144	318.232557	5.417651
4.161640	323.332834	5.422656
4.273494	308.771268	5.427661
4.653859	337.932825	5.432666
4.278936	327.731335	5.437670
4.597445	328.228832	5.442675
4.584127	320.640960	5.447680
4.581136	310.855780	5.452685
4.289634	319.668469	5.457690
4.436573	317.348569	5.462694
4.474751	308.923711	5.467699
4.348853	312.097828	5.472704
4.628083	318.827885	5.477709
4.744749	328.339108	5.482714
4.828676	312.114578	5.487718
4.744818	315.766174	5.492723
4.321024	320.252497	5.497728
4.527385	304.034102	5.502733
4.394527	303.314643	5.507738
4.736037	309.747031	5.512742
4.670584	309.210004	5.517747
4.573607	319.352658	5.522752
4.634478	305.890602	5.527757
4.652249	307.590014	5.532762
4.698240	314.014920	5.537766
4.752047	304.379035	5.542771
4.450817	313.332453	5.547776
4.607639	315.712448	5.552781
4.731755	327.706106	5.557786
5.027296	335.939595	5.562790
4.771863	315.965312	5.567795
4.525786	318.914645	5.572800
4.640685	317.150271	5.577805
4.840607	332.482545	5.582810
4.845400	336.746693	5.587814
5.116135	331.066393	5.592819
4.102179	321.553503	5.597824
4.600504	328.976916	5.602829
4.841272	337.946668	5.607834
4.573345	329.009764	5.612838
4.627134	331.858332	5.617843
4.896829	336.198036	5.622848
5.037472	335.097194	5.627853
4.810700	340.856150	5.632858
4.575336	332.037532	5.637862
5.094030	338.214373	5.642867
4.614376	336.381796	5.647872
4.902276	335.859009	5.652877
4.875859	334.724230	5.657882
4.906573	339.082396	5.662886
4.969648	331.083907	5.667891
4.876144	338.359601	5.672896
4.887749	339.515804	5.677901
4.622260	347.808727	5.682906
5.005480	352.589403	5.687910
5.083533	357.772244	5.692915
5.347109	360.831562	5.697920
5.326086	350.625231	5.702925
4.967104	349.960183	5.707930
4.953875	332.966226	5.712934
5.090536	331.030758	5.717939
5.028168	347.713965	5.722944
5.196812	361.434448	5.727949
5.413462	359.622489	5.732954
5.257693	345.061694	5.737958
5.096107	337.841903	5.742963
4.973894	351.671226	5.747968
5.388694	347.376253	5.752973
5.043538	344.383624	5.757978
4.912556	347.637639	5.762982
4.798284	354.169930	5.767987
4.945164	360.984016	5.772992
5.055404	359.524096	5.777997
4.846822	359.806779	5.783002
5.212329	362.242670	5.788006
5.285774	351.961425	5.793011
5.359229	362.691183	5.798016
5.361847	357.998869	5.803021
5.281125	363.317323	5.808026
4.922687	357.058534	5.813030
5.150629	369.576967	5.818035
5.294279	381.134155	5.823040
5.749908	377.807239	5.828045
5.548660	371.577601	5.833050
5.174478	364.612577	5.838054
5.210160	362.468295	5.843059
5.251973	379.824924	5.848064
5.642360	382.722004	5.853069
5.840619	374.341639	5.858074
5.662083	374.837919	5.863078
5.579302	360.452342	5.868083
5.306569	358.122260	5.873088
5.747265	356.762427	5.878093
5.345505	367.610939	5.883098
5.043458	360.169531	5.888102
5.550436	377.117910	5.893107
5.790479	392.048469	5.898112
5.797441	386.178520	5.903117
5.653537	385.229828	5.908122
5.524073	373.857200	5.913126
5.681070	375.031755	5.918131
5.441083	381.893808	5.923136
5.676444	380.648406	5.928141
5.632143	391.029627	5.933146
5.745908	392.606435	5.938150
5.756689	378.025847	5.943155
5.605533	386.860873	5.948160
5.535466	386.536544	5.953165
5.792482	387.692264	5.958170
5.715372	388.362483	5.963174
6.020146	397.233649	5.968179
5.863561	396.321746	5.973184
5.427243	382.497758	5.978189
5.581459	389.234774	5.983194
5.489429	393.776704	5.988198
5.607398	398.320535	5.993203
5.666878	402.019295	5.998208
5.561276	390.351845	6.003213
5.620174	397.575210	6.008218
5.332583	395.345529	6.013222
5.392930	393.017040	6.018227
5.398277	392.952985	6.023232
5.658656	408.630201	6.028237
6.068189	420.667790	6.033242
5.900562	418.874903	6.038246
5.833203	402.832187	6.043251
5.681072	404.387381	6.048256
6.062950	408.421617	6.053261
5.733058	399.794951	6.058266
5.845219	404.795286	6.063270
5.776153	394.957136	6.068275
5.925430	396.120246	6.073280
6.332990	384.846972	6.078285
6.130241	386.337327	6.083290
5.832525	387.614765	6.088294
5.831865	390.550969	6.093299
5.744280	398.436380	6.098304
5.969646	395.933335	6.103309
5.751695	392.632858	6.108314
6.055039	395.135443	6.113318
5.887992	389.609140	6.118323
5.797651	396.352837	6.123328
6.126955	389.429445	6.128333
5.683213	394.959814	6.133338
5.875257	398.580854	6.138342
6.252879	390.096446	6.143347
6.081224	397.431866	6.148352
6.174038	389.833664	6.153357
5.668585	376.067970	6.158362
5.595502	379.629304	6.163366
5.436722	374.952782	6.168371
5.576012	389.006923	6.173376
5.885407	394.643923	6.178381
5.873192	397.512334	6.183386
5.834638	387.814943	6.188390
5.986733	394.071390	6.193395
5.940693	397.843630	6.198400
5.748305	393.852595	6.203405
6.010584	391.780376	6.208410
5.791074	384.300715	6.213414
5.901576	364.933448	6.218419
5.393522	371.824843	6.223424
5.707459	389.838053	6.228429
6.152228	389.135659	6.233434
5.783515	386.896542	6.238438
6.087448	378.350918	6.243443
5.492747	369.243724	6.248448
5.968050	361.338826	6.253453
6.116806	368.478496	6.258458
5.460136	360.336495	6.263462
5.898747	360.786701	6.268467
5.355099	373.837328	6.273472
6.101702	369.955447	6.278477
5.840701	372.059220	6.283482
5.436631	373.577953	6.288486
5.761413	384.065861	6.293491
6.012803	392.398045	6.298496
6.324491	384.651653	6.303501
5.606282	374.250817	6.308506
5.512488	369.443888	6.313510
5.299078	372.299525	6.318515
5.436490	377.232620	6.323520
5.895199	390.281237	6.328525
6.044378	389.922556	6.333530
5.722769	396.493676	6.338534
5.466095	387.368313	6.343539
5.703755	392.684348	6.348544
5.990398	392.319949	6.353549
5.780027	387.594558	6.358554
5.681632	399.499737	6.363558
5.750990	393.101139	6.368563
5.382772	396.528379	6.373568
5.623770	394.953053	6.378573
5.749301	401.542704	6.383578
6.101603	402.920784	6.388582
6.201213	390.958581	6.393587
6.183205	392.964172	6.398592
5.702133	398.899034	6.403597
5.898576	394.151032	6.408602
5.702614	397.092526	6.413606
5.839450	393.733296	6.418611
5.758557	396.175858	6.423616
5.716210	394.493062	6.428621
5.923240	395.827462	6.433626
5.514335	391.133177	6.438630
5.661919	389.885707	6.443635
6.116000	391.589534	6.448640
6.020305	391.228090	6.453645
6.042005	394.727118	6.458650
5.847634	392.555600	6.463654
6.227398	385.368033	6.468659
5.873115	377.447571	6.473664
5.824882	357.706539	6.478669
5.745215	359.626872	6.483674
5.741469	360.364691	6.488678
5.746449	357.386804	6.493683
5.625823	374.911252	6.498688
5.642520	375.753439	6.503693
6.265908	380.297173	6.508698
6.166153	374.747675	6.513702
5.877271	360.289984	6.518707
5.632597	364.077521	6.523712
5.937401	349.925462	6.528717
5.638958	353.730913	6.533722
5.269256	355.832732	6.538726
6.144076	367.648683	6.543731
5.933062	371.722020	6.548736
5.829471	358.608403	6.553741
5.817255	365.770129	6.558746
5.767859	371.748082	6.563750
5.570973	367.308492	6.568755
5.564402	364.683600	6.573760
6.110568	374.083259	6.578765
5.956013	368.466418	6.583770
5.782403	367.266112	6.588774
5.527972	363.313278	6.593779
5.510127	368.213747	6.598784
5.539103	377.548905	6.603789
5.851167	380.423454	6.608794
5.699752	390.419650	6.613798
5.978365	384.867817	6.618803
6.049937	396.360375	6.623808
6.258281	384.979106	6.628813
5.934958	375.016284	6.633818
5.800728	365.020676	6.638822
5.793015	359.314390	6.643827
5.652670	363.265919	6.648832
5.746839	370.126233	6.653837
5.601739	356.759687	6.658842
5.554457	360.870645	6.663846
5.845986	375.198323	6.668851
5.825909	383.917895	6.673856
5.847676	392.865039	6.678861
5.838033	390.588646	6.683866
5.737275	385.545517	6.688870
5.478062	381.068231	6.693875
6.127973	389.008935	6.698880
5.998055	379.401796	6.703885
5.447799	377.982084	6.708890
5.752130	387.524048	6.713894
6.146845	378.331432	6.718899
5.801868	380.343957	6.723904
5.682420	372.548059	6.728909
6.276120	370.794084	6.733914
5.878157	369.110060	6.738918
6.045393	359.250724	6.743923
6.166855	360.029039	6.748928
5.861919	358.146938	6.753933
5.864483	365.366461	6.758938
5.789722	366.058458	6.763942
6.046211	359.257221	6.768947
5.726155	364.866280	6.773952
5.866450	364.891815	6.778957
5.866615	368.109467	6.783962
5.628068	371.234804	6.788966
5.989775	363.673578	6.793971
5.790646	368.871377	6.798976
6.148692	367.347319	6.803981
6.000870	362.858913	6.808986
6.000359	370.648410	6.813990
5.949081	369.229615	6.818995
5.825126	363.364366	6.824000
5.960736	358.379125	6.829005
5.829364	360.051288	6.834010
5.628209	361.791334	6.839014
5.691283	346.497043	6.844019
5.470882	370.418565	6.849024
5.765204	370.790136	6.854029
5.842966	358.527650	6.859034
5.632225	358.835982	6.864038
5.740045	360.068862	6.869043
5.642481	370.528020	6.874048
6.077954	360.731063	6.879053
5.725303	363.282639	6.884058
5.861716	362.916468	6.889062
5.761650	362.068479	6.894067
5.771473	365.714899	6.899072
5.838775	364.502157	6.904077
5.786547	365.196951	6.909082
5.475055	368.703885	6.914086
6.084071	362.714302	6.919091
5.848277	371.062696	6.924096
5.929204	363.630886	6.929101
5.933907	357.558815	6.934106
5.797580	360.984517	6.939110
5.342076	358.278101	6.944115
5.537714	361.363882	6.949120
5.463282	358.180133	6.954125
5.747236	361.688686	6.959130
5.642065	364.182504	6.964134
5.732280	356.632180	6.969139
5.575170	359.561253	6.974144
5.767027	362.695085	6.979149
6.037435	362.178202	6.984154
5.745401	359.174083	6.989158
5.971631	359.236775	6.994163
5.944015	366.938766	6.999168
5.745794	368.817562	7.004173
5.852495	359.198671	7.009178
5.628892	367.203459	7.014182
5.910665	363.486160	7.019187
5.824214	370.390593	7.024192
5.759598	360.235381	7.029197
5.848546	361.657884	7.034202
5.801479	360.830066	7.039206
6.102484	355.992922	7.044211
5.953129	369.165271	7.049216
5.737962	368.452378	7.054221
6.280267	371.838194	7.059226
5.609632	365.656792	7.064230
6.062450	376.323956	7.069235
5.877044	367.595572	7.074240
6.069336	368.359625	7.079245
5.982500	368.306849	7.084250
5.551151	370.301267	7.089254
5.603730	364.838640	7.094259
5.639855	364.168634	7.099264
5.705136	369.571784	7.104269
5.694732	355.510238	7.109274
5.630965	370.915498	7.114278
5.820080	354.424506	7.119283
5.785291	371.752000	7.124288
5.720453	362.685180	7.129293
5.637917	361.331396	7.134298
5.516632	375.236523	7.139302
5.635892	363.676231	7.144307
5.858258	363.739529	7.149312
5.752503	370.621677	7.154317
5.692354	368.058963	7.159322
5.752294	367.619350	7.164326
5.830236	359.289481	7.169331
5.697805	363.723836	7.174336
6.024076	357.069857	7.179341
5.966983	356.980783	7.184346
5.967294	358.189378	7.189350
6.196810	364.341932	7.194355
5.993071	350.000627	7.199360
5.858684	359.848602	7.204365
6.215791	356.552946	7.209370
6.072232	360.922603	7.214374
6.153464	362.539309	7.219379
5.964234	351.372217	7.224384
5.722294	339.605935	7.229389
5.531646	327.414000	7.234394
5.838672	342.511198	7.239398
5.648277	341.829227	7.244403
5.592174	353.066508	7.249408
5.668814	357.857256	7.254413
5.935444	356.524696	7.259418
5.783060	356.868178	7.264422
5.952464	355.120571	7.269427
5.948965	360.300371	7.274432
5.729528	360.186112	7.279437
6.341513	352.123757	7.284442
5.611350	350.393706	7.289446
5.643635	342.165913	7.294451
5.488424	345.803384	7.299456
5.747595	359.819737	7.304461
6.073984	357.652054	7.309466
6.013276	363.720364	7.314470
5.567237	348.091377	7.319475
5.557888	354.670505	7.324480
5.960696	359.552521	7.329485
6.141113	355.737206	7.334490
5.623489	352.793745	7.339494
5.850022	357.829933	7.344499
5.858470	357.787538	7.349504
5.799126	352.541772	7.354509
5.654063	336.527109	7.359514
5.589014	349.344540	7.364518
5.972283	353.172897	7.369523
5.567953	363.794013	7.374528
5.471682	362.654358	7.379533
5.824834	361.042479	7.384538
5.559405	365.994395	7.389542
5.986940	364.560692	7.394547
6.050896	365.316378	7.399552
5.832251	364.907758	7.404557
5.865182	366.547851	7.409562
5.718954	363.593655	7.414566
5.825868	362.776513	7.419571
5.591539	362.401989	7.424576
5.754190	361.281878	7.429581
5.469528	369.932165	7.434586
5.498095	368.067414	7.439590
5.909934	355.746259	7.444595
5.799342	363.502379	7.449600
5.500678	364.960303	7.454605
5.620876	361.613178	7.459610
5.445982	366.199723	7.464614
6.077834	358.105778	7.469619
5.926075	355.696629	7.474624
6.052702	361.811518	7.479629
6.329576	367.678237	7.484634
5.929104	366.076866	7.489638
5.927226	359.430007	7.494643
6.064482	362.958381	7.499648
5.787682	366.830048	7.504653
5.748910	361.432356	7.509658
5.505621	367.602042	7.514662
5.701009	360.671168	7.519667
5.742433	360.133213	7.524672
5.674875	356.723756	7.529677
6.039312	352.287973	7.534682
5.505826	357.674200	7.539686
5.851450	353.950062	7.544691
5.876370	357.663719	7.549696
5.904465	359.105248	7.554701
6.016578	365.918456	7.559706
5.952181	371.851301	7.564710
5.887638	358.332923	7.569715
5.723926	367.597024	7.574720
5.924531	376.845179	7.579725
6.250944	364.328590	7.584730
5.983304	354.385529	7.589734
5.723137	338.082008	7.594739
5.897805	341.686775	7.599744
5.444022	342.621659	7.604749
5.905054	331.495068	7.609754
5.598889	339.155267	7.614758
5.894296	339.289380	7.619763
5.684548	347.912099	7.624768
5.880995	358.606766	7.629773
5.880559	364.529588	7.634778
5.690033	369.260955	7.639782
5.810524	355.027037	7.644787
5.769345	355.944732	7.649792
5.794826	356.390063	7.654797
5.986088	351.272715	7.659802
5.765492	350.041805	7.664806
5.718266	334.296559	7.669811
5.476839	344.683328	7.674816
5.669713	356.944650	7.679821
5.665336	355.297039	7.684826
5.778231	358.398947	7.689830
6.083739	360.866386	7.694835
6.013188	360.222586	7.699840
5.740477	358.490464	7.704845
6.205489	353.355535	7.709850
5.515841	354.510877	7.714854
5.761377	349.438811	7.719859
6.013116	354.496359	7.724864
5.809178	348.279806	7.729869
5.678255	338.109685	7.734874
5.556985	356.061332	7.739878
5.605413	354.607933	7.744883
5.718382	360.997052	7.749888
6.041208	359.089361	7.754893
5.871344	359.625412	7.759898
6.156036	367.025364	7.764902
6.143870	353.913245	7.769907
5.770975	347.593447	7.774912
5.649246	342.427063	7.779917
5.718879	336.335334	7.784922
5.400899	340.798755	7.789926
5.990266	349.641126	7.794931
5.787913	347.122844	7.799936
5.707747	350.255000	7.804941
5.853413	346.407166	7.809946
5.633755	360.685208	7.814950
5.831850	357.996611	7.819955
5.913282	362.432260	7.824960
5.938312	353.477917	7.829965
5.608959	344.417749	7.834970
5.770356	358.895520	7.839974
6.026527	354.017944	7.844979
5.668532	352.235909	7.849984
6.065608	361.070448	7.854989
5.878028	344.673288	7.859994
5.686174	344.763520	7.864998
5.651128	339.210223	7.870003
5.864730	343.925722	7.875008
5.549607	341.817424	7.880013
6.004315	356.214434	7.885018
5.816138	359.467922	7.890022
5.882363	340.449313	7.895027
5.710228	345.956094	7.900032
5.857986	346.293679	7.905037
5.894988	346.015852	7.910042
5.728492	341.748682	7.915046
5.530905	341.501282	7.920051
5.832160	347.538184	7.925056
5.958869	354.130797	7.930061
6.100739	344.996797	7.935066
5.733262	347.585496	7.940070
5.638717	337.412839	7.945075
5.442626	342.973995	7.950080
5.743393	352.991073	7.955085
5.883578	363.536366	7.960090
5.681417	369.433847	7.965094
6.186162	371.322728	7.970099
5.679397	365.976213	7.975104
6.038541	359.462619	7.980109
6.018788	356.159569	7.985114
5.530695	345.447441	7.990118
5.354149	343.148335	7.995136
5.343466	350.288394	8.000154
5.598214	362.805311	8.005171
5.831111	365.078898	8.010189
5.919354	370.881201	8.015206
5.732287	371.585904	8.020224
6.000846	366.756594	8.025242
5.870927	372.615170	8.030259
5.990623	366.458517	8.035277
5.829980	375.537630	8.040294
6.036071	363.993176	8.045312
6.022967	368.911967	8.050330
5.786522	371.186508	8.055347
5.644973	369.479388	8.060365
5.561551	379.101818	8.065382
5.715924	372.734605	8.070400
5.956014	376.250437	8.075418
5.937145	376.644768	8.080435
5.789773	370.741394	8.085453
5.958884	370.863278	8.090470
5.888751	371.032114	8.095488
5.631511	377.863681	8.100506
5.595067	381.511203	8.105523
6.031203	370.975259	8.110541
5.725876	381.503450	8.115558
6.041636	375.177221	8.120576
6.101369	376.562769	8.125594
5.777759	380.842256	8.130611
6.213990	372.045123	8.135629
6.117284	372.057179	8.140646
5.965008	372.324091	8.145664
6.040456	372.034622	8.150682
6.230604	364.118639	8.155699
6.312963	369.915553	8.160717
5.769109	371.777518	8.165734
5.886459	374.810814	8.170752
5.936118	370.227236	8.175770
6.382917	374.972986	8.180787
6.193628	367.062804	8.185805
6.157379	372.247149	8.190822
6.232883	369.063837	8.195840
6.259027	367.412492	8.200858
5.709675	353.726883	8.205875
5.764510	351.850141	8.210893
5.921212	369.939718	8.215910
5.908689	361.067737	8.220928
6.155065	367.637359	8.225946
5.874929	379.158822	8.230963
6.069203	369.626438	8.235981
6.034943	376.612415	8.240998
5.871431	376.660184	8.246016
6.082883	373.446103	8.251034
5.988671	370.396677	8.256051
6.013581	362.222566	8.261069
5.818763	375.860798	8.266086
5.864803	376.374345	8.271104
5.769990	371.103356	8.276122
5.868237	375.951054	8.281139
5.950095	370.548244	8.286157
5.699811	376.523509	8.291174
5.581718	389.556447	8.296192
6.075370	402.919575	8.301210
5.992478	404.415833	8.306227
6.370174	397.306728	8.311245
6.084229	403.962924	8.316262
5.854596	405.027744	8.321280
6.222159	406.197807	8.326298
5.803560	399.017808	8.331315
6.050054	404.924715	8.336333
5.898149	413.652188	8.341350
5.751344	399.979210	8.346368
5.959681	405.778488	8.351386
5.744424	412.985339	8.356403
6.103827	402.215249	8.361421
6.064046	423.882750	8.366438
6.033816	433.298062	8.371456
6.453980	431.162102	8.376474
6.034045	435.431448	8.381491
6.231032	434.387640	8.386509
6.075106	427.396846	8.391526
6.418806	434.336248	8.396544
6.533560	426.933818	8.401562
5.857563	420.144431	8.406579
6.313890	429.167929	8.411597
6.420706	438.284063	8.416614
6.004258	434.294201	8.421632
6.454532	431.875816	8.426650
6.235816	439.364083	8.431667
6.490770	427.707792	8.436685
6.223873	418.531658	8.441702
6.029092	419.464787	8.446720
6.432974	424.630680	8.451738
6.393033	430.563539	8.456755
6.144549	411.746794	8.461773
6.165102	416.568807	8.466790
5.746457	427.676506	8.471808
6.044113	431.012918	8.476826
6.110925	436.222160	8.481843
6.089046	431.719202	8.486861
6.243063	429.918429	8.491878
6.123524	428.075312	8.496896
6.302919	439.310222	8.501914
6.279472	432.377563	8.506931
6.575600	434.704367	8.511949
6.365831	432.218985	8.516966
6.393353	439.372029	8.521984
6.331672	430.343615	8.527002
6.301775	440.162817	8.532019
6.073584	435.348204	8.537037
6.241462	436.009919	8.542054
6.080610	436.944044	8.547072
6.299030	431.352563	8.552090
6.110715	450.607111	8.557107
6.440229	460.016565	8.562125
6.598399	466.180325	8.567143
6.644879	462.389323	8.572160
6.667692	451.987518	8.577178
6.333237	435.784579	8.582195
6.458807	441.214987	8.587213
6.392746	437.949703	8.592231
6.414876	442.187657	8.597248
6.421342	433.438895	8.602266
6.249922	436.886673	8.607283
6.540966	441.461186	8.612301
6.324341	438.986345	8.617319
6.666158	460.824473	8.622336
6.680711	446.605474	8.627354
6.758668	439.372905	8.632371
6.236934	438.520600	8.637389
6.506843	437.629467	8.642407
5.768848	443.094195	8.647424
6.111642	445.634593	8.652442
6.658539	456.546848	8.657459
6.554395	455.594401	8.662477
6.619204	459.459602	8.667495
6.595756	464.301145	8.672512
6.891780	453.137015	8.677530
6.651136	453.316789	8.682547
6.424695	457.202376	8.687565
6.737276	458.734505	8.692583
6.649486	457.612240	8.697600
6.353380	453.120685	8.702618
6.759170	455.973104	8.707635
6.411360	446.784387	8.712653
6.739477	446.572092	8.717671
6.309707	454.453192	8.722688
6.464257	457.796252	8.727706
6.623451	461.482564	8.732723
6.373229	465.621186	8.737741
6.554731	459.372767	8.742759
6.150679	463.769018	8.747776
6.599993	460.703845	8.752794
6.738266	465.775667	8.757811
6.198879	472.187578	8.762829
6.546308	463.319108	8.767847
6.240041	465.664561	8.772864
6.489923	472.287321	8.777882
6.775869	466.293933	8.782899
6.699675	468.309851	8.787917
6.306569	465.799541	8.792935
6.276607	480.030556	8.797952
7.059339	469.888371	8.802970
7.108320	476.722490	8.807987
6.724367	471.960673	8.813005
6.713891	469.696524	8.818023
6.589748	474.919917	8.823040
6.533786	464.085483	8.828058
6.636878	471.229855	8.833075
6.390134	464.773979	8.838093
6.750047	460.479436	8.843111
6.676662	476.572849	8.848128
6.931547	474.689997	8.853146
6.616661	464.943850	8.858163
6.524282	476.852521	8.863181
6.973155	484.946260	8.868199
6.984939	484.827709	8.873216
6.766439	468.549768	8.878234
6.695952	467.071343	8.883251
6.683702	473.921366	8.888269
7.112538	474.138256	8.893287
6.624847	474.984737	8.898304
6.421350	468.304335	8.903322
6.987884	476.764641	8.908339
6.894234	488.859709	8.913357
7.020143	486.119756	8.918375
6.860837	483.320350	8.923392
6.798627	471.281382	8.928410
6.844361	463.630976	8.933427
6.415329	469.609032	8.938445
6.851127	482.659395	8.943463
7.005601	495.359372	8.948480
7.040889	483.128396	8.953498
6.946435	468.787604	8.958515
6.744379	463.290395	8.963533
6.991686	466.716753	8.968551
6.747186	465.619040	8.973568
6.845787	476.822451	8.978586
6.837512	484.927856	8.983603
6.875005	482.842381	8.988621
6.946077	491.304583	8.993639
6.754449	492.139392	8.998656
7.124846	488.499603	9.003674
7.134837	495.178892	9.008691
6.709870	489.599837	9.013709
7.155998	481.135614	9.018727
7.223392	477.903061	9.023744
6.770503	463.306011	9.028762
6.850097	472.063512	9.033779
6.602484	475.908240	9.038797
7.197891	479.497809	9.043815
6.634874	496.990229	9.048832
6.879227	492.622266	9.053850
6.877318	484.143034	9.058867
6.834733	486.156844	9.063885
7.264585	484.129813	9.068903
7.013136	491.790487	9.073920
6.783787	494.426847	9.078938
7.336567	487.154577	9.083955
6.757331	490.202360	9.088973
7.262093	490.770269	9.093991
7.103771	494.992328	9.099008
7.101005	504.280298	9.104026
7.348463	497.986818	9.109043
7.323098	487.826070	9.114061
7.439228	467.181744	9.119079
6.986604	464.469323	9.124096
6.793456	463.205776	9.129114
6.858832	463.366004	9.134131
7.125471	473.940331	9.139149
7.228664	483.451529	9.144167
7.100589	482.622749	9.149184
6.968359	468.912721	9.154202
6.842565	467.802721	9.159219
6.895197	486.388400	9.164237
7.235409	480.825158	9.169255
6.922422	492.112001	9.174272
7.190264	493.856269	9.179290
6.972545	487.146530	9.184307
6.738655	487.091718	9.189325
7.049620	484.792982	9.194343
7.249411	487.134887	9.199360
6.925668	491.890945	9.204378
7.375074	486.932282	9.209395
7.200181	499.462962	9.214413
7.197787	492.167222	9.219431
7.033595	492.073087	9.224448
7.115951	491.668926	9.229466
7.321554	496.515615	9.234483
7.084865	499.916826	9.239501
7.185320	497.565865	9.244519
7.275803	493.752182	9.249536
6.956069	499.053565	9.254554
7.476482	498.075843	9.259571
7.227375	503.407185	9.264589
7.399127	494.181220	9.269607
7.334304	497.858458	9.274624
7.186517	493.425704	9.279642
7.345978	495.297406	9.284659
7.204020	503.180770	9.289677
7.191261	502.059368	9.294695
6.926491	496.972760	9.299712
7.047925	501.258285	9.304730
7.125524	499.235951	9.309747
6.971159	513.098322	9.314765
7.361001	519.377280	9.319783
7.427930	525.637407	9.324800
6.995315	524.007434	9.329818
7.437792	522.846263	9.334835
7.598714	515.799478	9.339853
7.615651	521.433123	9.344871
7.380844	516.572187	9.349888
6.990313	511.050846	9.354906
7.401878	509.632589	9.359923
7.356261	526.917740	9.364941
7.415581	527.631182	9.369959
7.670829	521.812997	9.374976
7.741883	518.538838	9.379994
7.319739	504.101038	9.385011
7.139643	499.209445	9.390029
7.356527	511.464156	9.395047
7.532777	522.355630	9.400064
7.245007	518.957811	9.405082
7.546680	518.973720	9.410099
7.135505	529.266118	9.415117
7.235464	521.913304	9.420135
6.997880	527.103993	9.425152
6.899458	527.977848	9.430170
7.324083	520.350105	9.435187
7.318354	531.068126	9.440205
7.388673	518.560239	9.445223
7.226477	527.746969	9.450240
7.208788	528.563994	9.455258
7.305016	531.240866	9.460275
7.345663	544.040763	9.465293
7.546679	556.777672	9.470311
7.983621	550.634366	9.475328
7.511159	545.851684	9.480346
7.791425	529.385087	9.485363
7.725380	529.726853	9.490381
7.531421	524.304096	9.495399
7.807004	528.764290	9.500416
7.067602	526.115726	9.505434
7.599733	526.963370	9.510451
7.376467	528.349089	9.515469
7.494013	535.058879	9.520487
7.653410	550.330094	9.525504
7.642411	558.745227	9.530522
7.622789	540.949680	9.535539
7.595049	551.806861	9.540557
7.834359	547.468078	9.545575
7.515223	537.012504	9.550592
7.514872	542.970755	9.555610
7.888088	547.396722	9.560627
7.799785	543.232346	9.565645
7.860933	530.656460	9.570663
7.629456	532.409538	9.575680
7.603211	522.507682	9.580698
7.844115	518.405340	9.585715
7.688815	534.136101	9.590733
7.991077	533.618589	9.595751
7.360266	527.642586	9.600768
7.510349	534.353589	9.605786
7.707424	529.926753	9.610803
7.641091	530.202293	9.615821
7.693909	523.797289	9.620839
7.524200	537.520072	9.625856
7.832357	544.263116	9.630874
7.569716	543.695258	9.635891
7.875534	540.775630	9.640909
7.989548	539.564936	9.645927
7.708594	535.377098	9.650944
7.604022	533.780933	9.655962
7.588618	538.375083	9.660979
7.834495	547.447394	9.665997
7.785994	550.803351	9.671015
7.803595	554.893719	9.676032
7.914955	554.923667	9.681050
7.866296	544.895924	9.686067
7.650159	554.930561	9.691085
7.276359	546.127716	9.696103
7.627336	550.503519	9.701120
7.340535	565.718426	9.706138
7.845090	554.928659	9.711155
7.739229	548.419121	9.716173
7.604590	553.653649	9.721191
7.859143	549.438708	9.726208
7.694222	553.371482	9.731226
7.926623	551.719362	9.736243
7.772728	552.008620	9.741261
7.734729	549.133393	9.746279
8.287695	552.840079	9.751296
7.587080	561.666219	9.756314
7.840421	552.812447	9.761331
7.932068	561.227278	9.766349
7.555121	557.862359	9.771367
8.030950	563.212680	9.776384
8.331489	572.992805	9.781402
8.134772	558.525953	9.786419
7.706301	557.595914	9.791437
7.664530	554.986363	9.796455
8.008035	560.606723	9.801472
8.183816	574.792955	9.806490
8.113069	573.620674	9.811507
7.919309	565.657455	9.816525
8.253054	566.182735	9.821543
8.111587	553.389270	9.826560
7.894576	552.968897	9.831578
8.207930	552.102509	9.836595
8.015519	553.644341	9.841613
8.025122	555.962406	9.846631
8.279986	550.699692	9.851648
8.104858	553.210802	9.856666
7.873333	552.275152	9.861683
8.016925	556.986406	9.866701
7.864312	556.423399	9.871719
8.047196	553.620860	9.876736
7.829169	565.934284	9.881754
8.004659	564.433090	9.886771
8.033236	571.832174	9.891789
8.178578	581.390468	9.896807
8.422752	579.313623	9.901824
8.202566	586.739066	9.906842
8.253747	576.758778	9.911859
8.327360	569.223880	9.916877
7.907338	557.603832	9.921895
7.816574	562.427546	9.926912
8.213008	564.088558	9.931930
8.457130	573.460958	9.936947
8.503504	570.095981	9.941965
8.113581	568.705467	9.946983
7.931703	557.101756	9.952000
7.792328	566.884532	9.957018
7.962202	572.333285	9.962035
8.111216	577.545468	9.967053
8.072975	575.153112	9.972071
8.512056	575.863858	9.977088
8.150902	586.722807	9.982106
8.113481	575.626625	9.987123
8.432673	570.577888	9.992141
8.389623	576.732189	9.997159
8.376754	570.050283	10.002176
7.882823	584.013249	10.007194
8.567087	577.941636	10.012211
8.351247	581.598371	10.017229
8.151611	586.672679	10.022247
8.113821	576.100418	10.027264
8.324393	583.641405	10.032282
8.276275	581.951183	10.037299
8.361502	584.153261	10.042317
7.996912	587.113781	10.047335
8.004407	579.734405	10.052352
8.205474	582.095057	10.057370
8.618186	580.957481	10.062387
8.721432	579.234076	10.067405
8.262319	581.357340	10.072423
8.707651	590.332150	10.077440
8.544601	580.461165	10.082458
8.181886	583.736971	10.087475
8.412737	575.123397	10.092493
8.554980	587.026938	10.097511
8.370211	577.351861	10.102528
8.198428	578.095202	10.107546
8.349155	572.817240	10.112563
8.321300	574.270176	10.117581
8.339689	582.993140	10.122599
8.861679	579.083429	10.127616
8.413438	585.364334	10.132634
8.296207	591.959451	10.137651
8.835872	585.667495	10.142669
8.472702	591.136655	10.147687
8.575117	583.581459	10.152704
8.636790	584.086251	10.157722
8.724683	584.810997	10.162739
8.710678	579.543064	10.167757
8.441814	584.568258	10.172775
8.677881	577.512831	10.177792
8.463903	583.012262	10.182810
8.521626	579.856945	10.187827
8.405018	577.284363	10.192845
8.505574	578.158603	10.197863
8.815416	575.541296	10.202880
8.534166	577.081270	10.207898
8.323660	579.490629	10.212915
8.642032	585.929131	10.217933
8.947267	579.468780	10.222951
9.003910	566.057288	10.227968
8.522252	578.377312	10.232986
8.571188	576.741312	10.238003
8.851326	574.661989	10.243021
8.695711	585.883209	10.248039
9.090441	578.326396	10.253056
9.098522	575.554398	10.258074
8.587356	569.395533	10.263091
8.701507	557.208954	10.268109
8.478717	543.939090	10.273127
8.174397	553.943362	10.278144
8.644730	564.722513	10.283162
8.614375	571.818406	10.288179
8.771153	567.924893	10.293197
8.674011	578.439515	10.298215
9.005935	573.404562	10.303232
8.696813	579.310218	10.308250
8.584824	576.919949	10.313267
8.518363	576.592751	10.318285
8.566793	580.463700	10.323303
8.642321	573.379780	10.328320
8.508597	577.639029	10.333338
8.477542	582.497575	10.338355
8.540777	581.802918	10.343373
8.625016	583.200422	10.348391
8.826363	575.582391	10.353408
8.810439	579.719043	10.358426
8.736551	583.757481	10.363443
8.691728	579.116069	10.368461
8.572748	595.844738	10.373479
8.791071	601.800305	10.378496
8.932840	607.802583	10.383514
8.932177	612.242964	10.388531
9.131783	611.533251	10.393549
8.879896	607.435516	10.398567
8.689155	600.497445	10.403584
9.130985	615.838074	10.408602
8.907869	607.500739	10.413619
8.856806	604.422423	10.418637
8.720083	609.969718	10.423655
8.803465	605.159890	10.428672
8.808687	610.460883	10.433690
8.586615	614.380534	10.438707
9.025728	609.464476	10.443725
8.845272	605.718467	10.448743
8.840086	604.005737	10.453760
8.728232	602.843051	10.458778
8.567942	613.995593	10.463795
8.714605	607.212938	10.468813
8.776352	608.639215	10.473831
8.945950	606.293185	10.478848
8.668941	606.200947	10.483866
9.048243	623.290227	10.488883
9.074661	631.368172	10.493901
9.003219	638.006625	10.498919
9.505829	634.327157	10.503936
9.023815	621.239862	10.508954
8.889346	618.212481	10.513971
9.176822	617.299651	10.518989
9.028468	621.062586	10.524007
9.392032	623.606068	10.529024
9.363518	606.897446	10.534042
8.996621	603.120688	10.539059
8.894952	600.640437	10.544077
9.034890	611.162113	10.549095
8.928865	619.961393	10.554112
8.939870	629.537605	10.559130
9.472198	630.644000	10.564147
9.389860	630.388716	10.569165
8.835312	637.781361	10.574183
8.668636	631.091973	10.579200
8.988277	633.282575	10.584218
8.855936	635.632357	10.589235
9.091317	627.807001	10.594253
9.199942	636.519009	10.599271
9.292526	636.854857	10.604288
9.388196	632.301873	10.609306
9.099715	640.381824	10.614323
9.251895	630.486667	10.619341
9.226933	637.070500	10.624359
9.365862	635.054320	10.629376
9.394167	638.928435	10.634394
9.299296	642.332700	10.639411
9.623840	627.654732	10.644429
9.066486	632.093978	10.649447
9.190295	627.779584	10.654464
9.269024	623.712095	10.659482
9.133843	627.031154	10.664499
9.277090	627.510543	10.669517
9.309764	631.210402	10.674535
9.533809	626.365906	10.679552
9.448045	631.248816	10.684570
9.476943	637.578057	10.689587
9.628099	636.582444	10.694605
9.254441	640.118751	10.699623
9.248285	629.857083	10.704640
9.439862	631.291421	10.709658
9.086877	634.155456	10.714675
9.066494	626.231318	10.719693
9.284210	635.756211	10.724711
8.928209	629.882283	10.729728
9.620117	641.283173	10.734746
9.410341	661.282925	10.739763
9.458364	649.911377	10.744781
9.733008	652.617118	10.749799
9.740232	649.845242	10.754816
9.640987	638.234843	10.759834
9.128887	641.221640	10.764851
9.737080	638.734303	10.769869
9.572851	631.217709	10.774887
9.216055	627.789659	10.779904
9.797279	637.712035	10.784922
9.291049	641.802446	10.789939
9.714007	641.370162	10.794957
9.551587	639.013033	10.799975
9.235086	638.482012	10.804992
9.388919	648.187335	10.810010
9.476026	653.696418	10.815027
9.624154	651.691419	10.820045
9.639057	649.189740	10.825063
9.874984	647.982028	10.830080
10.054156	646.183604	10.835098
9.652215	644.204830	10.840115
9.736104	636.027664	10.845133
9.578191	626.796478	10.850151
9.499753	624.520866	10.855168
9.965543	637.112207	10.860186
9.896245	637.536535	10.865203
9.980222	627.042995	10.870221
9.584803	630.002041	10.875239
9.539438	629.226567	10.880256
9.674586	618.715547	10.885274
9.527219	627.568646	10.890291
9.394497	624.471562	10.895309
9.710259	641.914799	10.900327
9.624602	648.082111	10.905344
10.085646	648.546422	10.910362
9.932032	652.123995	10.915379
9.848160	634.171163	10.920397
9.715119	634.065835	10.925415
9.615911	635.226997	10.930432
10.067818	639.192533	10.935450
9.812981	645.701933	10.940467
9.669852	630.879487	10.945485
10.115014	633.350224	10.950503
9.989215	633.745535	10.955520
9.761735	625.358383	10.960538
9.761115	626.930132	10.965555
9.636643	624.030572	10.970573
10.192618	642.707963	10.975591
9.786716	638.375575	10.980608
10.006316	630.432769	10.985626
9.654340	639.198011	10.990643
9.660693	644.164321	10.995661
10.168247	649.651709	11.000679
10.067584	657.146817	11.005696
10.193753	639.763831	11.010714
9.918417	641.031484	11.015731
9.875009	633.344480	11.020749
9.771144	633.329255	11.025767
9.927316	643.280362	11.030784
10.405035	639.721557	11.035802
10.083327	644.893903	11.040819
9.535422	629.576300	11.045837
10.092029	640.140007	11.050855
9.994144	648.502524	11.055872
10.292949	648.484169	11.060890
9.950608	642.901588	11.065907
9.847320	651.151343	11.070925
10.333414	646.470912	11.075943
10.301174	648.558858	11.080960
9.869008	632.531996	11.085978
9.969823	635.672069	11.090995
10.212334	642.917742	11.096013
10.248365	641.403679	11.101031
10.071519	636.855521	11.106048
9.964092	622.557664	11.111066
9.890141	637.638297	11.116083
9.810053	643.157794	11.121101
10.147052	645.743311	11.126119
10.216322	653.104495	11.131136
10.408585	645.248016	11.136154
10.266984	654.554661	11.141171
10.136367	657.308120	11.146189
10.134505	651.302960	11.151207
9.995025	647.591547	11.156224
10.292207	637.118245	11.161242
10.314885	644.969564	11.166259
10.103749	647.350628	11.171277
10.150947	643.196556	11.176295
9.884607	647.451354	11.181312
10.048454	642.695181	11.186330
10.214298	646.787590	11.191347
9.861306	644.741186	11.196365
10.333314	641.044420	11.201383
10.267845	646.227112	11.206400
9.933093	639.810207	11.211418
9.991278	647.933676	11.216435
10.283195	648.632770	11.221453
10.533479	656.388472	11.226471
10.207350	660.125620	11.231488
10.665890	667.097614	11.236506
10.569507	651.690312	11.241523
10.300961	653.076823	11.246541
10.530535	650.446835	11.251559
10.390897	642.342558	11.256576
10.231181	647.420096	11.261594
10.178682	642.716755	11.266611
10.535939	662.586641	11.271629
10.652130	657.452921	11.276647
10.119061	650.565311	11.281664
10.631793	663.468052	11.286682
10.633330	667.147551	11.291699
10.671103	659.794956	11.296717
10.239085	647.750694	11.301735
10.388500	657.302079	11.306752
10.565519	669.017189	11.311770
10.472402	670.410930	11.316787
10.648730	667.666205	11.321805
10.577607	670.239930	11.326823
10.863624	672.678804	11.331840
10.550058	664.349303	11.336858
10.412078	653.997821	11.341875
10.341218	657.117459	11.346893
10.960078	662.846188	11.351911
10.616295	656.721028	11.356928
10.841934	657.039185	11.361946
10.791519	649.451102	11.366963
10.564483	649.379436	11.371981
10.676236	650.766322	11.376999
10.418753	650.150315	11.382016
10.463116	640.963169	11.387034
10.444546	657.884447	11.392051
10.465401	667.882015	11.397069
10.753373	667.909539	11.402087
10.812335	672.981224	11.407104
10.919197	673.447380	11.412122
10.727125	669.166689	11.417139
10.676423	670.288695	11.422157
10.776152	668.322835	11.427175
10.593008	671.447445	11.432192
10.846708	663.382516	11.437210
10.672276	670.062364	11.442227
10.647777	681.928978	11.447245
10.912797	685.046488	11.452263
10.779406	676.007095	11.457280
10.880779	677.603894	11.462298
10.911026	674.598032	11.467315
10.834312	682.360798	11.472333
11.330385	665.860264	11.477351
10.847652	659.554901	11.482368
10.759805	648.267758	11.487386
11.038071	646.942960	11.492403
10.695676	650.029401	11.497421
10.814518	643.232157	11.502439
10.740997	644.395607	11.507456
10.546922	640.695905	11.512474
10.939806	656.959423	11.517491
10.815064	667.014517	11.522509
11.066147	674.886868	11.527527
11.097154	678.710075	11.532544
11.287688	663.396665	11.537562
10.905693	663.693262	11.542579
10.775934	663.016217	11.547597
11.016076	668.580222	11.552615
11.256001	667.728490	11.557632
10.937503	661.981220	11.562650
11.239052	650.055551	11.567667
10.775736	658.219708	11.572685
11.049685	656.538978	11.577703
10.988404	670.683533	11.582720
11.036857	672.582113	11.587738
11.167285	669.800398	11.592755
10.934494	673.103201	11.597773
10.843768	663.934053	11.602791
11.265561	670.548887	11.607808
10.947867	666.404644	11.612826
11.167835	674.212441	11.617843
10.928383	676.493803	11.622861
11.380885	665.361830	11.627879
10.970321	674.843171	11.632896
10.995717	678.970216	11.637914
11.240190	669.022708	11.642931
11.185191	670.602981	11.647949
11.209831	669.179063	11.652967
11.233798	670.172605	11.657984
11.192116	666.953952	11.663002
11.079888	665.895462	11.668019
11.089550	667.452980	11.673037
11.423661	668.754536	11.678055
11.315970	670.822749	11.683072
11.180195	673.614888	11.688090
11.745337	662.408464	11.693107
11.404602	674.804304	11.698125
11.798316	670.573843	11.703143
11.527653	679.402104	11.708160
11.435594	660.910883	11.713178
11.320060	643.985486	11.718195
10.943558	651.063061	11.723213
11.534852	649.417817	11.728231
11.341568	674.748325	11.733248
11.273176	668.649440	11.738266
11.569689	666.368725	11.743283
11.511439	670.382641	11.748301
11.308190	659.984577	11.753319
11.108452	668.467203	11.758336
11.042657	670.446800	11.763354
11.322657	669.080703	11.768371
11.275591	672.562690	11.773389
11.516210	669.467064	11.778407
11.170025	678.206170	11.783424
10.960425	674.944397	11.788442
11.429758	664.614520	11.793459
11.123926	667.786754	11.798477
11.659775	669.567944	11.803495
11.564644	672.634583	11.808512
11.428262	671.715578	11.813530
11.674222	674.851851	11.818547
11.448943	673.403974	11.823565
11.667437	667.676708	11.828583
11.333557	672.570101	11.833600
11.478537	665.090253	11.838618
11.692536	665.141990	11.843635
11.428354	671.498228	11.848653
11.367204	672.322069	11.853671
11.772675	685.465696	11.858688
11.629378	684.891757	11.863706
11.826655	686.489310	11.868723
11.405442	685.371933	11.873741
11.558009	684.123631	11.878759
11.580322	682.002640	11.883776
11.878778	691.035228	11.888794
11.943574	690.646437	11.893811
11.561606	692.385239	11.898829
12.167107	687.376819	11.903847
11.475252	685.506579	11.908864
11.400628	689.731349	11.913882
12.022459	696.804003	11.918899
11.716288	697.012980	11.923917
11.671544	698.847271	11.928935
11.561722	691.691358	11.933952
11.809353	699.191873	11.938970
12.166033	692.606656	11.943987
11.909559	690.182204	11.949005
11.590077	694.322263	11.954023
11.892929	702.483161	11.959040
11.772061	688.733314	11.964058
11.756338	689.471143	11.969075
11.694137	691.112507	11.974093
11.642513	698.571546	11.979111
11.636270	696.404535	11.984128
11.670489	695.944795	11.989146
11.755726	693.422623	11.994163
12.115501	699.270853	11.999181
11.903959	697.107605	12.004199
12.046133	690.959942	12.009216
12.160604	698.901045	12.014234
12.455229	687.553952	12.019251
12.058443	688.742807	12.024269
12.227116	686.324328	12.029287
12.115098	685.915903	12.034304
11.899229	689.193967	12.039322
11.972083	694.954606	12.044339
12.008703	694.402971	12.049357
11.426055	690.975580	12.054375
11.895610	688.339545	12.059392
11.594385	691.716190	12.064410
11.964458	694.949786	12.069427
11.745112	700.475341	12.074445
12.061093	720.698900	12.079463
12.559150	718.219341	12.084480
12.301364	718.632178	12.089498
12.087073	702.485908	12.094515
12.071368	708.112103	12.099533
12.358765	708.650960	12.104551
11.896510	708.695044	12.109568
11.955696	711.604966	12.114586
12.528517	718.013117	12.119603
12.237220	721.653301	12.124621
12.216308	720.993914	12.129639
12.316741	722.117490	12.134656
12.435988	731.424332	12.139674
12.379662	709.755856	12.144691
12.286075	712.516145	12.149709
12.230253	695.833809	12.154727
12.117936	694.308270	12.159744
11.837512	711.740844	12.164762
12.495678	707.156514	12.169779
12.264434	726.629525	12.174797
12.240510	726.213608	12.179815
12.547115	712.743907	12.184832
12.406616	726.052001	12.189850
11.773772	721.114517	12.194867
12.167258	719.055289	12.199885
12.420712	717.907943	12.204903
12.508440	717.039029	12.209920
12.206343	723.227655	12.214938
12.419866	721.449089	12.219955
12.323426	717.285947	12.224973
12.499031	727.549638	12.229991
12.599645	724.886196	12.235008
12.839620	724.580411	12.240026
12.435167	725.688418	12.245043
12.887631	724.913837	12.250061
12.576532	727.054952	12.255079
12.729264	714.347821	12.260096
12.454449	713.068649	12.265114
12.555046	716.647430	12.270131
12.640537	717.470388	12.275149
12.710267	723.054800	12.280167
12.649533	723.903825	12.285184
12.241320	722.468826	12.290202
12.624861	714.825346	12.295219
12.423741	717.293213	12.300237
12.464267	711.499143	12.305255
12.613303	711.321216	12.310272
12.426788	716.475556	12.315290
12.653139	711.091030	12.320307
12.576794	721.753957	12.325325
12.374036	726.639444	12.330343
12.861794	713.933471	12.335360
12.555154	724.925975	12.340378
12.301196	720.465618	12.345395
12.825914	729.958239	12.350413
12.566309	743.000983	12.355431
13.292271	735.341714	12.360448
12.586252	739.100530	12.365466
12.668425	750.840021	12.370483
12.613276	747.797034	12.375501
12.494640	744.139141	12.380519
12.928593	744.636102	12.385536
12.967978	748.830400	12.390554
12.942914	748.768114	12.395571
13.270605	739.154669	12.400589
13.123433	745.041317	12.405607
13.062211	728.669068	12.410624
12.702287	726.775219	12.415642
12.570285	729.083935	12.420659
12.824566	733.989334	12.425677
12.698354	739.916878	12.430695
12.988470	745.296351	12.435712
12.857410	744.651065	12.440730
12.907200	733.815678	12.445747
13.096296	742.145898	12.450765
12.871365	743.424596	12.455783
13.042057	735.899664	12.460800
13.058090	737.989525	12.465818
13.105577	741.393595	12.470835
12.985128	743.716281	12.475853
12.856956	740.719450	12.480871
13.124217	738.932462	12.485888
13.370426	740.503418	12.490906
13.298049	736.806720	12.495923
13.182955	739.122255	12.500941
13.032537	744.009014	12.505959
13.421124	731.842434	12.510976
13.385359	743.120714	12.515994
12.985021	739.421751	12.521011
13.317340	744.526366	12.526029
13.306243	744.146309	12.531047
13.416206	746.120468	12.536064
13.399057	736.649418	12.541082
13.163083	715.914804	12.546099
13.302928	712.285847	12.551117
13.123550	719.218954	12.556135
13.363475	713.661885	12.561152
13.028489	722.045807	12.566170
13.417544	733.349039	12.571187
13.585572	734.793387	12.576205
13.463971	732.568706	12.581223
13.584431	713.974704	12.586240
13.366884	715.684592	12.591258
13.733818	705.294996	12.596275
13.616408	705.392346	12.601293
13.371800	719.691897	12.606311
13.335252	713.698461	12.611328
13.199988	718.033725	12.616346
13.282131	714.849311	12.621363
13.533332	712.859714	12.626381
13.170608	713.352108	12.631399
13.324290	705.381727	12.636416
13.473611	705.279496	12.641434
13.261895	711.166777	12.646451
13.384330	703.182358	12.651469
12.906894	727.374028	12.656487
13.384748	730.625458	12.661504
13.600978	745.057954	12.666522
13.212375	735.869167	12.671539
13.495681	733.675719	12.676557
13.442119	737.733098	12.681575
13.521143	734.151535	12.686592
13.614148	737.286538	12.691610
13.287802	736.952718	12.696627
13.632033	735.361956	12.701645
13.744410	738.288796	12.706663
13.636580	735.708504	12.711680
13.683067	737.900891	12.716698
13.396249	731.725754	12.721715
13.898876	730.173291	12.726733
13.650946	733.563684	12.731751
13.184865	737.398515	12.736768
13.057691	739.898981	12.741786
13.695327	745.340771	12.746803
13.848886	757.741275	12.751821
14.070222	760.894045	12.756839
14.126008	748.770130	12.761856
13.757152	743.541968	12.766874
13.518970	746.274423	12.771891
13.983866	740.764150	12.776909
13.572344	739.307578	12.781927
13.578735	732.209180	12.786944
13.645178	745.866720	12.791962
13.713081	754.894438	12.796979
14.144665	746.861562	12.801997
13.844530	753.188748	12.807015
13.898997	755.692315	12.812032
14.155125	751.770573	12.817050
13.423601	755.795321	12.822067
14.299035	748.264108	12.827085
14.220156	752.647351	12.832103
14.120259	758.390895	12.837120
14.101409	751.681456	12.842138
13.853785	750.817745	12.847155
14.234893	743.124142	12.852173
14.068333	756.531017	12.857191
14.067852	751.188330	12.862208
14.060234	744.278317	12.867226
14.174630	746.163418	12.872243
14.343649	724.219774	12.877261
13.830902	738.965298	12.882279
13.984988	741.961343	12.887296
14.118208	734.028869	12.892314
14.055760	741.514869	12.897331
14.270746	744.308867	12.902349
14.094266	748.442311	12.907367
14.420863	748.511121	12.912384
14.442667	745.052131	12.917402
13.738578	737.878855	12.922419
14.134809	742.967145	12.927437
14.045755	752.713736	12.932455
13.977468	758.177770	12.937472
14.284042	747.983801	12.942490
13.998302	752.923323	12.947507
14.462563	751.253792	12.952525
14.355747	754.994467	12.957543
14.264161	749.896431	12.962560
14.460639	747.318952	12.967578
14.304799	761.121785	12.972595
14.430444	761.061133	12.977613
14.526936	759.578612	12.982631
14.384340	756.527234	12.987648
14.372063	755.939077	12.992666
14.328062	761.639150	12.997683
14.048110	754.358388	13.002701
14.074584	759.327889	13.007719
14.324091	763.296763	13.012736
14.198001	754.634886	13.017754
14.136708	762.594088	13.022771
14.388254	755.633997	13.027789
14.250567	755.182254	13.032807
14.493547	764.283532	13.037824
14.626401	772.710942	13.042842
14.475838	777.029682	13.047859
14.662269	773.996177	13.052877
14.115876	779.178518	13.057895
14.104890	782.427654	13.062912
14.151444	789.410596	13.067930
14.641284	788.819507	13.072947
15.038485	781.053937	13.077965
14.989934	785.148411	13.082983
14.809100	788.569328	13.088000
14.826825	774.217026	13.093018
14.636124	794.374886	13.098035
14.972653	779.934760	13.103053
14.845785	784.388646	13.108071
15.004225	776.111372	13.113088
14.884097	767.940865	13.118106
14.358510	768.758582	13.123123
14.390921	768.706226	13.128141
14.622145	782.909182	13.133159
15.141604	787.091388	13.138176
14.929447	782.940050	13.143194
14.344512	783.000198	13.148211
14.771290	783.084870	13.153229
14.877522	778.605934	13.158247
14.881798	783.657816	13.163264
14.877628	778.842724	13.168282
14.733864	788.616842	13.173299
14.814258	780.796767	13.178317
14.877066	791.879750	13.183335
15.364230	785.510743	13.188352
15.520151	785.912410	13.193370
14.803968	786.220343	13.198387
14.933676	783.170477	13.203405
14.936555	783.738136	13.208423
14.916973	779.133744	13.213440
15.182798	777.441652	13.218458
14.714146	780.633105	13.223475
14.375428	777.637698	13.228493
14.812077	786.879059	13.233511
14.823473	785.826439	13.238528
15.266287	788.307035	13.243546
15.298838	789.258213	13.248563
14.961184	790.128538	13.253581
15.109005	779.539697	13.258599
14.550205	786.841550	13.263616
14.993891	786.507003	13.268634
14.806460	782.784140	13.273651
14.985863	794.019272	13.278669
15.241928	800.502329	13.283687
15.568356	809.262348	13.288704
15.483346	808.565663	13.293722
14.981519	800.609581	13.298739
15.253896	808.292460	13.303757
15.588592	811.648387	13.308775
15.364345	798.280730	13.313792
15.403455	791.038326	13.318810
15.156285	787.766639	13.323827
15.315470	789.559520	13.328845
15.015360	791.765193	13.333863
14.766078	803.850145	13.338880
15.308703	813.292668	13.343898
15.068812	813.873118	13.348915
15.220374	823.632541	13.353933
15.263989	816.799680	13.358951
15.036943	816.737482	13.363968
15.304300	817.547730	13.368986
15.268272	814.366034	13.374003
15.432290	806.280378	13.379021
15.560375	811.615831	13.384039
15.113604	820.708441	13.389056
15.751557	818.465730	13.394074
15.734178	833.859560	13.399091
15.599402	832.507944	13.404109
15.607882	812.239853	13.409127
15.135393	819.461923	13.414144
15.720674	826.442525	13.419162
15.618162	828.639334	13.424179
15.764979	830.336325	13.429197
15.912161	833.014727	13.434215
15.349172	833.276567	13.439232
15.944163	826.404651	13.444250
15.917167	827.851160	13.449267
15.756663	812.447454	13.454285
16.012313	804.132846	13.459303
15.530691	810.567383	13.464320
15.727845	800.646151	13.469338
15.550087	805.833859	13.474355
15.730438	802.116485	13.479373
15.778863	814.565058	13.484391
15.981816	820.876562	13.489408
15.811400	812.663419	13.494426
15.642961	814.842153	13.499443
15.838946	813.467117	13.504461
16.028903	825.647368	13.509479
15.992782	828.004191	13.514496
16.159875	816.121569	13.519514
15.647095	811.872157	13.524531
15.337786	804.857908	13.529549
15.740996	816.332546	13.534567
15.804533	821.889556	13.539584
16.062534	818.936350	13.544602
16.085415	822.956523	13.549619
15.637697	824.093406	13.554637
15.695383	826.795297	13.559655
15.810011	833.357331	13.564672
16.063578	837.129923	13.569690
16.073502	830.245530	13.574707
15.603742	824.941634	13.579725
16.112467	819.342418	13.584743
15.858667	830.184694	13.589760
16.362046	827.357144	13.594778
16.067094	822.455054	13.599795
15.868733	826.673997	13.604813
16.615500	833.948040	13.609831
16.405420	824.141094	13.614848
16.235015	821.472762	13.619866
16.258028	824.587189	13.624883
16.314659	829.400505	13.629901
16.494941	817.045595	13.634919
16.274683	822.243123	13.639936
16.642028	819.178109	13.644954
16.116477	823.767055	13.649971
16.228903	820.603124	13.654989
16.320207	819.651593	13.660007
16.242318	824.836282	13.665024
16.218464	820.639652	13.670042
16.206683	825.908660	13.675059
16.383085	822.169809	13.680077
16.649430	815.160039	13.685095
16.220894	819.033186	13.690112
16.282884	817.196301	13.695130
16.484447	819.866180	13.700147
16.353136	818.646567	13.705165
16.280816	825.537695	13.710183
16.516964	843.170330	13.715200
16.479812	843.734796	13.720218
16.645738	846.176730	13.725235
16.396856	846.111641	13.730253
16.981552	838.001086	13.735271
16.322122	833.329671	13.740288
16.406315	839.107515	13.745306
16.327442	846.258456	13.750323
16.328606	844.689878	13.755341
16.455472	843.473994	13.760359
16.333249	847.627363	13.765376
16.809667	840.281707	13.770394
16.547927	844.737805	13.775411
16.716887	840.255337	13.780429
17.198592	844.386666	13.785447
16.603329	842.608574	13.790464
16.499552	845.193753	13.795482
16.674199	849.246959	13.800499
16.587084	840.556842	13.805517
16.845681	840.481671	13.810535
16.902512	839.541851	13.815552
16.750108	846.041586	13.820570
16.911727	841.042709	13.825587
16.899576	838.273840	13.830605
16.873717	837.444808	13.835623
16.912432	837.202113	13.840640
17.176253	830.104369	13.845658
17.355328	837.290632	13.850675
16.928011	842.788854	13.855693
17.138892	834.531739	13.860711
16.929933	845.174492	13.865728
17.407085	833.151760	13.870746
17.334938	839.266528	13.875763
16.907846	824.835554	13.880781
17.307287	829.295353	13.885799
17.073638	838.367204	13.890816
17.210215	832.715838	13.895834
17.156456	829.672619	13.900851
17.116206	834.078232	13.905869
17.268210	826.474138	13.910887
17.139911	838.281378	13.915904
16.985382	831.476401	13.920922
17.058216	834.283218	13.925939
16.873824	825.977583	13.930957
17.148711	829.500677	13.935975
16.780533	841.531699	13.940992
16.754888	827.858344	13.946010
16.620003	829.933992	13.951027
16.700161	842.282938	13.956045
17.200932	847.029827	13.961063
17.452084	858.847057	13.966080
17.383175	863.626402	13.971098
17.977180	858.525060	13.976115
17.537202	846.526092	13.981133
17.225851	842.093632	13.986151
17.231877	833.584588	13.991168
17.655929	840.202287	13.996186
17.359690	832.090902	14.001203
17.103163	839.607351	14.006221
17.758270	847.599515	14.011239
17.733525	850.109194	14.016256
17.493202	830.568039	14.021274
17.423856	829.796314	14.026291
17.225569	828.514610	14.031309
17.905926	833.747761	14.036327
17.578392	826.354502	14.041344
17.375345	836.090596	14.046362
17.920598	841.149254	14.051379
17.362869	839.655619	14.056397
17.549004	844.069946	14.061415
17.519027	848.480265	14.066432
17.566723	856.820070	14.071450
17.999621	853.883637	14.076467
17.710591	856.614609	14.081485
17.709691	852.322855	14.086503
17.817264	855.657571	14.091520
17.697431	858.668151	14.096538
17.957948	852.826943	14.101555
17.954259	860.751917	14.106573
18.125063	843.377519	14.111591
17.532769	835.230465	14.116608
17.438101	835.008668	14.121626
17.265508	843.780618	14.126643
17.801449	856.970202	14.131661
17.747941	851.926132	14.136679
17.747309	860.800538	14.141696
17.814645	864.327755	14.146714
18.251858	857.900275	14.151731
17.605096	863.849458	14.156749
17.916154	856.046859	14.161767
17.980880	854.518814	14.166784
17.907446	863.849602	14.171802
18.412596	858.774805	14.176819
17.560185	858.352990	14.181837
17.821487	851.583840	14.186855
17.896426	855.747346	14.191872
17.709057	853.394097	14.196890
17.962621	849.898774	14.201907
18.229575	868.435492	14.206925
18.367537	860.871454	14.211943
18.386702	865.261454	14.216960
18.220234	857.713556	14.221978
18.229662	850.106544	14.226995
18.037192	853.030672	14.232013
18.194507	850.219470	14.237031
18.436490	850.620279	14.242048
18.188613	860.101474	14.247066
18.213749	850.194543	14.252083
18.013872	862.151871	14.257101
18.132627	862.603546	14.262119
18.352064	872.986688	14.267136
18.421185	882.149981	14.272154
18.839131	880.434046	14.277171
18.585594	868.693034	14.282189
18.464963	857.672830	14.287207
18.530360	862.936068	14.292224
17.978810	858.929407	14.297242
18.694885	849.248740	14.302259
18.237137	859.513910	14.307277
18.284431	857.313244	14.312295
18.344971	869.722088	14.317312
18.713290	874.991517	14.322330
18.745008	872.900589	14.327347
19.018233	874.830247	14.332365
18.724487	861.299860	14.337383
18.562666	848.095957	14.342400
18.360769	850.819588	14.347418
18.245942	844.033632	14.352435
18.780890	864.567034	14.357453
18.274215	870.999206	14.362471
18.832744	865.565744	14.367488
18.632339	870.015394	14.372506
19.053327	869.495051	14.377523
18.485679	870.707532	14.382541
19.231784	874.185208	14.387559
19.219305	872.501998	14.392576
18.934295	862.905588	14.397594
19.024149	850.514330	14.402611
18.685355	856.860233	14.407629
18.362633	844.123361	14.412647
18.994382	857.307403	14.417664
18.738029	870.251898	14.422682
18.783440	865.394300	14.427699
18.741710	877.468874	14.432717
19.143678	872.814188	14.437735
19.149081	869.405082	14.442752
18.872473	871.906888	14.447770
19.120082	872.404647	14.452787
19.076116	878.461364	14.457805
18.830973	868.984939	14.462823
19.009237	871.374450	14.467840
18.988630	872.245598	14.472858
18.972094	872.680600	14.477875
19.018012	881.579280	14.482893
18.578134	875.371269	14.487911
18.842890	867.907284	14.492928
18.697207	876.589826	14.497946
18.896565	869.757789	14.502963
18.795302	881.870096	14.507981
19.138268	889.892250	14.512999
19.420792	901.483684	14.518016
19.187115	911.249865	14.523034
19.487590	902.994461	14.528051
19.210908	901.362110	14.533069
19.116120	905.018880	14.538087
19.157663	905.542615	14.543104
19.044475	903.610089	14.548122
19.315103	904.312529	14.553139
19.336424	909.529036	14.558157
19.187054	909.956449	14.563175
19.536498	905.451998	14.568192
19.412182	900.728282	14.573210
19.669568	902.654114	14.578227
19.450408	907.362336	14.583245
19.599369	908.200605	14.588263
19.658369	890.723756	14.593280
19.618534	901.362135	14.598298
19.383947	895.819395	14.603315
19.491249	902.265837	14.608333
19.412240	901.767026	14.613351
19.521171	893.822508	14.618368
19.406496	896.576662	14.623386
19.790901	891.943659	14.628403
19.831458	900.647526	14.633421
19.391606	892.243028	14.638439
19.489705	884.126639	14.643456
19.762195	891.380340	14.648474
19.947205	886.273643	14.653491
19.723463	892.652026	14.658509
19.645924	900.130989	14.663527
19.455773	897.986456	14.668544
18.969364	902.203209	14.673562
19.736634	910.452388	14.678579
19.962079	919.742689	14.683597
19.681395	917.763819	14.688615
19.935009	905.611958	14.693632
20.028046	920.035494	14.698650
20.119462	919.506826	14.703667
19.833838	923.767866	14.708685
20.178263	928.662352	14.713703
20.409364	922.573261	14.718720
20.069883	917.229989	14.723738
20.149218	912.389154	14.728755
20.195104	917.286230	14.733773
20.189374	901.675157	14.738791
20.011169	889.553093	14.743808
19.728056	902.706935	14.748826
20.285467	905.513581	14.753843
20.379793	915.648102	14.758861
20.283647	907.675748	14.763879
20.054162	892.784561	14.768896
19.866193	909.394942	14.773914
20.319776	916.692865	14.778931
20.247221	914.630893	14.783949
19.961797	930.694820	14.788967
20.734075	919.089703	14.793984
20.043550	922.420086	14.799002
20.484107	919.804340	14.804019
20.335130	921.156358	14.809037
19.988347	918.215840	14.814055
20.552036	917.458540	14.819072
19.934854	914.756051	14.824090
20.259318	917.185780	14.829107
20.223019	917.327228	14.834125
20.265488	918.567198	14.839143
20.605624	915.342327	14.844160
20.411420	915.950336	14.849178
20.287281	915.152478	14.854195
20.194824	914.573722	14.859213
20.038969	918.337894	14.864231
20.586586	921.250221	14.869248
20.241171	940.192233	14.874266
20.476874	938.173481	14.879283
20.720514	939.549194	14.884301
20.682474	940.173763	14.889319
20.915220	932.295037	14.894336
20.718906	942.260511	14.899354
20.627570	943.079626	14.904371
20.895373	931.237955	14.909389
20.912936	945.682805	14.914407
20.740333	938.839592	14.919424
20.717995	942.529200	14.924442
20.724386	942.067502	14.929459
20.959305	937.549429	14.934477
21.081700	941.857000	14.939495
21.325505	939.691809	14.944512
21.025890	919.481335	14.949530
20.883494	912.595529	14.954547
20.871520	900.693569	14.959565
20.911636	909.637355	14.964583
21.118210	922.847035	14.969600
20.961925	915.909754	14.974618
20.918341	907.070771	14.979635
21.097367	915.005012	14.984653
21.072086	924.795354	14.989671
20.723540	922.593583	14.994688
20.949135	932.227855	14.999706
21.167189	924.405084	15.004723
21.591767	933.200281	15.009741
20.760803	939.522338	15.014759
21.175460	936.475139	15.019776
21.182925	937.717439	15.024794
21.155352	932.609321	15.029811
21.558176	932.249615	15.034829
20.988442	936.119663	15.039847
21.040494	940.031149	15.044864
21.176742	935.686329	15.049882
21.093689	931.069751	15.054899
21.190840	938.338320	15.059917
21.238439	948.802079	15.064935
21.109471	941.604883	15.069952
21.191400	932.219193	15.074970
21.006198	935.587172	15.079987
21.471106	943.789065	15.085005
21.476181	958.803937	15.090023
21.638897	955.685754	15.095040
21.686659	964.110807	15.100058
21.198942	954.448276	15.105075
21.564468	953.538981	15.110093
21.994850	959.720225	15.115111
21.709916	951.250400	15.120128
21.570525	940.921063	15.125146
21.670637	945.052243	15.130163
21.964960	939.473959	15.135181
21.354989	941.608275	15.140199
21.439967	945.606124	15.145216
22.066937	959.377981	15.150234
21.586858	951.134395	15.155251
21.960518	954.512648	15.160269
21.541781	959.100671	15.165287
21.911241	960.601842	15.170304
21.675212	967.357725	15.175322
21.999005	965.782769	15.180339
22.015539	957.666503	15.185357
21.723292	949.264098	15.190375
22.006376	961.455098	15.195392
22.090836	957.926289	15.200410
21.467477	945.517320	15.205427
21.860452	953.294978	15.210445
21.668802	962.922055	15.215463
21.895719	949.789716	15.220480
21.942184	958.880857	15.225498
22.019943	955.908531	15.230515
22.270641	951.735127	15.235533
21.884038	957.779281	15.240551
22.162163	961.049425	15.245568
22.065620	963.504096	15.250586
22.012274	958.560958	15.255603
22.158508	951.800331	15.260621
21.835879	961.343786	15.265639
21.610375	948.976623	15.270656
21.945944	962.813074	15.275674
22.151581	970.834691	15.280691
22.374306	964.374506	15.285709
22.315175	968.862007	15.290727
21.988412	966.764117	15.295744
22.046359	970.232864	15.300762
21.786079	972.397604	15.305779
22.127292	969.377686	15.310797
22.099089	975.163717	15.315815
22.018715	972.254034	15.320832
22.130619	989.196210	15.325850
22.372524	1006.247424	15.330867
22.864047	998.476450	15.335885
22.650381	1000.539214	15.340903
22.672305	995.985068	15.345920
22.794199	1001.296301	15.350938
22.673118	1008.081527	15.355955
22.797795	995.624751	15.360973
23.003829	994.289154	15.365991
23.014367	982.109052	15.371008
22.604151	971.149929	15.376026
22.711540	969.719334	15.381043
22.795156	968.519686	15.386061
22.331042	970.091500	15.391079
22.726544	965.753391	15.396096
22.635483	976.295697	15.401114
22.351671	980.565934	15.406131
22.963568	983.597591	15.411149
23.020147	997.938538	15.416167
23.162967	997.363943	15.421184
23.198691	989.617048	15.426202
23.190484	978.531818	15.431219
22.898809	971.764054	15.436237
22.938949	977.021815	15.441255
22.571887	978.663632	15.446272
23.073416	981.709424	15.451290
22.761225	986.003044	15.456307
22.683137	990.938499	15.461325
22.934718	993.351254	15.466343
23.140295	986.079533	15.471360
22.884481	993.438141	15.476378
22.886699	989.120620	15.481395
23.239006	984.470531	15.486413
23.340003	990.043816	15.491431
23.589137	987.073036	15.496448
23.324605	988.105486	15.501466
22.976684	990.640572	15.506483
23.000154	992.842910	15.511501
23.284759	995.146347	15.516519
23.329838	998.661299	15.521536
23.565937	996.071265	15.526554
23.697330	1000.367973	15.531571
23.531646	990.386718	15.536589
23.454160	990.263215	15.541607
23.492145	986.129443	15.546624
23.652199	989.837822	15.551642
23.442844	989.056468	15.556659
23.490477	986.606419	15.561677
23.345099	984.609498	15.566695
23.405711	991.527200	15.571712
23.736125	984.422117	15.576730
23.455245	982.825132	15.581747
23.619284	980.274793	15.586765
23.269395	984.391279	15.591783
23.264866	980.507170	15.596800
23.535677	986.634528	15.601818
23.675189	985.183119	15.606835
23.763710	993.014808	15.611853
23.621990	992.267039	15.616871
23.606004	1002.090682	15.621888
23.959753	997.127932	15.626906
23.570505	1004.602127	15.631923
24.044489	1008.794667	15.636941
24.021883	1001.886902	15.641959
23.720516	1014.715475	15.646976
24.142597	1010.319542	15.651994
24.009735	1003.413271	15.657011
24.272312	1006.957265	15.662029
24.222654	1004.913786	15.667047
24.141784	995.929118	15.672064
24.088956	982.884767	15.677082
24.143024	981.266861	15.682099
24.178813	977.458489	15.687117
23.931685	974.723259	15.692135
23.777010	981.043514	15.697152
24.018132	988.532548	15.702170
24.131518	997.587977	15.707187
23.867910	1006.402669	15.712205
24.065200	1001.792643	15.717223
24.278656	1007.026414	15.722240
24.320467	1003.589487	15.727258
24.122358	1012.428634	15.732275
24.264256	1005.349923	15.737293
24.180909	1004.103847	15.742311
24.043112	1001.288366	15.747328
24.097636	1003.896102	15.752346
23.820253	1010.074643	15.757363
24.359666	1015.074305	15.762381
24.611207	1025.704977	15.767399
24.773904	1033.976352	15.772416
24.839859	1021.860126	15.777434
24.451486	1018.588428	15.782451
24.438731	1002.041072	15.787469
24.726698	1019.031432	15.792487
24.531860	1021.113339	15.797504
24.784577	1014.620034	15.802522
24.018457	1012.401624	15.807539
24.593711	1027.071593	15.812557
24.963859	1039.839155	15.817575
24.681750	1027.209401	15.822592
24.743412	1024.747681	15.827610
24.625461	1039.829236	15.832627
24.975796	1031.849989	15.837645
24.586732	1025.678145	15.842663
24.575467	1028.416117	15.847680
25.099042	1015.426602	15.852698
25.017200	1023.799405	15.857715
25.132763	1021.865740	15.862733
25.272774	1023.914119	15.867751
24.875898	1026.942886	15.872768
25.023611	1020.011585	15.877786
25.065848	1028.140881	15.882803
25.317738	1029.297553	15.887821
25.163272	1023.638076	15.892839
24.917732	1030.783646	15.897856
24.953967	1025.867480	15.902874
25.028843	1029.519784	15.907891
25.080140	1027.451017	15.912909
25.258046	1023.074402	15.917927
25.366330	1027.134891	15.922944
25.433268	1019.474614	15.927962
24.811600	1028.067700	15.932979
25.021042	1027.201792	15.937997
25.473915	1024.811326	15.943015
25.062525	1028.606090	15.948032
25.183816	1022.067100	15.953050
25.088521	1030.157984	15.958067
24.907926	1028.586308	15.963085
25.301313	1028.060818	15.968103
24.843676	1037.218358	15.973120
25.326857	1043.359799	15.978138
25.153262	1053.694171	15.983155
25.944354	1053.740701	15.988173
26.105727	1042.824526	15.993191
25.539518	1039.407114	15.998208
25.639491	1042.960811	16.003226
25.616486	1043.273752	16.008243
25.764223	1037.794145	16.013261
25.934841	1039.645222	16.018279
25.602926	1048.054060	16.023296
26.065702	1045.769339	16.028314
25.698077	1040.604013	16.033331
25.734567	1042.457170	16.038349
26.164747	1036.216926	16.043367
25.855056	1028.221170	16.048384
26.055031	1023.168895	16.053402
25.703265	1022.037458	16.058419
25.754963	1037.363835	16.063437
25.790412	1046.867012	16.068455
25.892710	1044.487288	16.073472
25.927729	1042.219094	16.078490
26.024109	1042.898346	16.083507
25.989404	1046.059726	16.088525
25.797589	1038.452605	16.093543
26.100813	1049.125686	16.098560
26.116079	1042.688510	16.103578
26.393391	1040.959880	16.108595
26.398127	1041.240071	16.113613
26.103610	1035.438428	16.118631
25.744222	1047.837448	16.123648
26.141366	1039.159726	16.128666
25.826406	1041.487679	16.133683
26.069094	1048.206459	16.138701
26.165135	1041.643015	16.143719
25.857077	1050.505720	16.148736
26.067709	1052.612467	16.153754
26.404436	1064.148177	16.158771
26.171819	1065.781560	16.163789
26.677122	1064.083480	16.168807
26.139278	1064.303511	16.173824
26.683471	1065.748912	16.178842
26.406646	1063.311818	16.183859
26.709060	1063.832555	16.188877
26.647401	1059.670195	16.193895
26.857029	1055.651529	16.198912
26.559329	1063.922467	16.203930
26.457985	1061.202253	16.208947
26.678475	1059.864386	16.213965
26.920193	1058.034031	16.218983
26.385531	1054.030990	16.224000
26.603804	1064.834159	16.229018
26.846354	1064.979258	16.234035
26.835003	1057.397504	16.239053
26.903169	1050.065233	16.244071
26.564185	1060.191986	16.249088
27.012485	1052.181602	16.254106
26.812570	1059.487297	16.259123
26.656989	1065.047155	16.264141
27.313008	1059.074484	16.269159
26.742165	1062.133670	16.274176
26.862830	1062.200033	16.279194
27.289885	1048.083187	16.284211
26.861053	1061.493512	16.289229
27.210576	1055.360575	16.294247
27.107824	1054.385786	16.299264
26.943777	1058.463704	16.304282
27.205663	1058.902426	16.309299
27.288603	1067.836426	16.314317
27.469042	1052.404341	16.319335
27.236432	1061.728612	16.324352
27.015349	1058.490658	16.329370
27.109336	1050.898715	16.334387
27.004664	1059.757961	16.339405
26.982464	1070.876528	16.344423
27.066559	1086.494526	16.349440
26.878018	1090.535261	16.354458
27.213520	1086.752493	16.359475
27.395328	1087.636119	16.364493
27.530085	1079.643290	16.369511
27.189059	1098.133489	16.374528
27.099836	1087.654192	16.379546
27.566626	1100.898975	16.384563
27.527107	1105.979901	16.389581
27.600559	1096.639636	16.394599
27.642303	1114.533379	16.399616
27.794030	1115.207119	16.404634
27.615187	1115.049001	16.409651
26.995299	1119.214132	16.414669
27.820441	1100.203199	16.419687
27.692921	1113.222361	16.424704
27.835696	1114.030051	16.429722
27.786754	1111.623520	16.434739
27.504752	1107.760767	16.439757
27.977269	1111.054132	16.444775
27.896310	1109.309043	16.449792
27.890168	1106.510788	16.454810
28.281697	1105.859351	16.459827
28.005830	1104.712861	16.464845
28.128081	1097.327915	16.469863
28.107928	1112.274284	16.474880
27.803618	1105.284380	16.479898
27.766950	1107.660260	16.484915
28.085038	1104.669190	16.489933
27.996778	1114.529466	16.494951
28.454218	1124.427327	16.499968
28.294102	1127.280157	16.504986
28.274473	1128.760251	16.510003
28.319705	1118.913140	16.515021
28.451317	1119.138739	16.520039
28.359258	1106.195121	16.525056
28.422422	1107.797945	16.530074
28.094364	1100.777049	16.535091
28.203541	1121.251221	16.540109
28.458952	1130.789409	16.545127
28.499453	1127.191712	16.550144
28.466634	1127.007560	16.555162
28.816785	1117.696516	16.560179
28.872617	1125.826883	16.565197
28.749083	1109.038001	16.570215
28.270126	1104.941012	16.575232
28.419736	1107.707441	16.580250
28.745982	1113.450605	16.585267
28.855921	1113.562832	16.590285
29.217902	1115.491234	16.595303
28.777930	1107.711520	16.600320
28.697426	1103.558414	16.605338
28.599860	1091.139548	16.610355
28.594327	1106.175142	16.615373
29.039948	1121.089568	16.620391
28.972292	1128.062135	16.625408
28.451815	1123.296285	16.630426
28.985756	1121.066678	16.635443
28.484011	1124.007748	16.640461
29.069841	1117.339134	16.645479
29.215366	1120.355521	16.650496
28.827361	1127.892690	16.655514
29.173331	1119.238727	16.660531
28.930847	1113.839172	16.665549
29.289143	1112.003170	16.670567
29.194753	1114.855167	16.675584
29.136402	1110.925813	16.680602
29.053836	1111.323828	16.685619
28.960659	1117.315750	16.690637
29.290756	1121.783333	16.695655
29.258434	1115.893244	16.700672
29.183851	1119.808831	16.705690
29.423508	1112.471757	16.710707
28.890490	1121.865219	16.715725
29.318311	1130.202400	16.720743
29.815175	1135.549601	16.725760
29.555275	1135.435742	16.730778
29.956301	1134.637645	16.735795
29.480046	1133.907569	16.740813
29.567260	1132.798868	16.745831
29.630530	1134.830880	16.750848
29.738438	1141.147921	16.755866
29.870700	1134.294738	16.760883
29.525757	1129.353057	16.765901
29.593126	1130.895262	16.770919
29.871393	1135.617129	16.775936
29.587239	1141.190844	16.780954
29.936154	1135.641817	16.785971
29.855816	1138.005607	16.790989
29.754051	1136.980165	16.796007
30.182120	1134.763989	16.801024
29.816276	1130.731325	16.806042
29.912498	1136.011905	16.811059
29.424352	1138.726777	16.816077
29.855276	1132.511631	16.821095
29.974556	1130.214444	16.826112
29.755325	1141.035712	16.831130
30.147425	1137.322963	16.836147
29.944557	1136.183969	16.841165
29.693931	1141.929161	16.846183
30.155663	1141.323531	16.851200
30.415473	1152.344313	16.856218
30.341380	1149.925938	16.861235
30.202803	1146.520402	16.866253
30.073844	1147.216029	16.871271
30.331131	1157.716487	16.876288
30.164748	1155.757553	16.881306
30.450565	1152.661074	16.886323
30.346837	1160.055884	16.891341
30.825676	1152.002801	16.896359
30.711781	1160.248141	16.901376
30.597915	1162.014411	16.906394
30.597174	1146.702153	16.911411
30.644410	1140.124228	16.916429
30.148797	1141.499014	16.921447
30.704636	1143.441229	16.926464
30.489290	1156.123878	16.931482
30.292198	1156.492499	16.936499
30.477049	1162.857455	16.941517
30.250221	1155.044324	16.946535
30.704532	1150.659087	16.951552
30.485382	1163.885152	16.956570
30.541516	1151.502125	16.961587
30.522081	1154.522271	16.966605
30.755349	1171.742260	16.971623
31.039350	1171.849307	16.976640
30.803851	1184.803385	16.981658
31.108578	1184.992394	16.986675
31.117417	1179.850097	16.991693
31.281297	1176.132071	16.996711
30.910781	1179.084147	17.001728
30.723042	1184.939424	17.006746
30.833985	1177.906522	17.011763
30.924330	1173.748723	17.016781
30.883570	1178.312296	17.021799
31.335798	1174.454415	17.026816
31.011335	1178.431257	17.031834
30.937073	1172.068023	17.036851
31.167519	1190.008018	17.041869
30.982051	1192.391444	17.046887
31.348309	1198.191486	17.051904
31.290269	1202.202332	17.056922
31.549499	1201.114014	17.061939
31.758829	1204.338175	17.066957
31.197273	1203.141762	17.071975
31.117157	1195.854756	17.076992
30.949489	1198.819236	17.082010
31.542443	1199.755220	17.087027
31.414191	1203.316304	17.092045
32.051102	1211.829055	17.097063
31.626429	1199.559197	17.102080
31.716043	1200.501457	17.107098
31.834216	1215.407304	17.112115
31.879247	1213.241664	17.117133
32.045336	1211.101240	17.122151
31.777405	1196.641871	17.127168
31.991664	1204.782167	17.132186
31.618527	1203.767679	17.137203
31.754641	1216.616219	17.142221
32.071739	1216.475075	17.147239
32.397066	1212.293074	17.152256
31.852207	1215.594375	17.157274
31.968209	1212.360385	17.162291
32.335412	1209.636167	17.167309
32.034449	1224.415180	17.172327
32.481912	1218.105892	17.177344
32.342530	1215.022372	17.182362
32.339211	1208.932042	17.187379
32.486473	1209.764281	17.192397
32.472604	1210.000051	17.197415
32.359082	1194.377207	17.202432
32.472447	1194.921257	17.207450
32.405517	1198.084556	17.212467
32.439988	1185.139992	17.217485
32.526543	1193.271887	17.222503
32.674544	1177.210439	17.227520
32.242969	1180.026911	17.232538
32.265908	1187.575461	17.237555
32.652792	1199.658840	17.242573
32.420871	1214.016759	17.247591
32.757884	1213.440135	17.252608
32.592233	1214.507599	17.257626
32.781231	1208.087326	17.262643
32.968752	1209.329838	17.267661
32.713887	1219.689661	17.272679
32.594685	1214.570571	17.277696
32.414367	1216.713344	17.282714
32.827971	1213.678888	17.287731
33.306779	1209.551738	17.292749
32.679229	1217.871271	17.297767
33.116036	1218.317307	17.302784
32.720665	1227.509370	17.307802
32.681834	1227.572320	17.312819
33.082698	1222.185546	17.317837
32.882272	1217.656714	17.322855
32.646215	1213.524798	17.327872
32.868069	1222.105739	17.332890
33.032687	1230.616755	17.337907
33.282762	1249.554159	17.342925
33.303243	1243.393815	17.347943
33.323627	1243.422240	17.352960
33.322921	1248.162598	17.357978
33.088839	1239.864555	17.362995
33.173777	1245.879109	17.368013
33.259065	1251.407597	17.373031
33.441940	1238.392404	17.378048
33.564629	1245.982157	17.383066
33.776227	1246.387737	17.388083
33.560011	1240.466457	17.393101
33.785432	1237.846502	17.398119
33.854366	1237.974622	17.403136
33.767675	1238.269140	17.408154
33.498120	1234.331823	17.413171
33.930855	1236.930832	17.418189
33.643635	1249.482792	17.423207
33.741239	1234.019346	17.428224
33.528784	1238.988545	17.433242
33.393871	1243.664719	17.438259
33.585144	1238.689489	17.443277
33.597669	1241.161825	17.448295
33.937793	1244.002571	17.453312
33.898888	1257.699100	17.458330
33.788878	1264.596302	17.463347
34.173464	1257.728785	17.468365
34.073521	1270.825795	17.473383
33.785140	1263.217928	17.478400
34.129085	1259.487452	17.483418
33.735152	1267.085571	17.488435
34.033385	1266.997877	17.493453
33.803339	1270.751655	17.498471
34.491807	1259.020591	17.503488
33.825344	1272.578761	17.508506
34.238197	1269.983087	17.513523
34.644162	1274.527187	17.518541
33.996334	1291.920055	17.523559
34.421336	1285.364944	17.528576
34.840551	1285.248828	17.533594
34.475618	1293.934364	17.538611
34.789477	1279.939217	17.543629
34.698225	1281.648305	17.548647
34.775341	1279.329302	17.553664
34.728222	1262.780777	17.558682
34.516691	1266.755723	17.563699
34.371673	1268.305970	17.568717
34.730872	1278.171971	17.573735
34.804365	1279.460756	17.578752
34.537241	1279.221791	17.583770
34.708682	1279.870357	17.588787
34.221350	1272.584002	17.593805
34.140057	1279.852265	17.598823
34.671957	1272.743904	17.603840
34.933989	1287.898681	17.608858
34.698399	1302.951550	17.613875
35.189935	1295.429765	17.618893
35.008378	1306.898507	17.623911
35.388997	1303.045507	17.628928
35.253905	1302.296686	17.633946
35.429629	1306.157317	17.638963
35.734060	1297.961074	17.643981
35.436511	1278.712427	17.648999
35.589383	1271.540370	17.654016
34.993386	1275.828029	17.659034
34.762327	1285.887504	17.664051
35.222326	1291.770723	17.669069
35.254897	1301.037792	17.674087
35.292027	1294.764363	17.679104
35.207801	1295.695994	17.684122
35.116828	1307.122140	17.689139
35.086858	1303.377652	17.694157
35.641290	1312.013831	17.699175
35.909802	1316.137648	17.704192
35.723832	1314.377433	17.709210
35.633256	1313.233457	17.714227
35.895746	1315.912802	17.719245
35.774697	1306.561874	17.724263
35.940909	1310.818487	17.729280
36.116106	1315.092629	17.734298
36.020206	1314.533334	17.739315
36.141575	1294.149176	17.744333
35.668869	1291.859509	17.749351
35.941941	1299.921203	17.754368
36.448816	1305.834954	17.759386
36.284185	1318.131060	17.764403
36.218334	1296.655876	17.769421
35.901638	1300.495823	17.774439
36.134723	1296.899478	17.779456
36.594467	1299.658372	17.784474
35.949271	1296.575189	17.789491
36.269549	1296.509289	17.794509
36.078191	1313.445636	17.799527
36.294785	1313.500126	17.804544
36.624443	1308.806164	17.809562
36.269924	1313.999621	17.814579
36.300700	1310.157249	17.819597
36.671896	1314.880384	17.824615
36.273387	1305.071135	17.829632
36.490919	1307.530295	17.834650
35.889488	1315.618554	17.839667
36.313103	1307.135380	17.844685
35.992054	1319.254014	17.849703
36.486672	1336.834018	17.854720
36.580367	1344.608244	17.859738
36.426200	1347.965125	17.864755
36.627716	1333.428938	17.869773
36.757545	1339.158767	17.874791
36.840587	1335.052570	17.879808
36.957498	1333.648858	17.884826
36.677214	1339.597583	17.889843
36.962628	1337.539439	17.894861
36.927534	1343.828462	17.899879
37.097427	1347.150350	17.904896
37.151429	1352.522820	17.909914
37.265576	1366.066059	17.914931
37.405293	1354.591330	17.919949
37.063508	1345.874593	17.924967
36.787731	1350.090007	17.929984
37.256266	1360.320792	17.935002
37.105285	1374.861826	17.940019
37.476231	1363.600183	17.945037
37.240502	1360.727400	17.950055
37.608028	1359.517960	17.955072
37.557893	1363.133112	17.960090
37.654986	1363.468268	17.965107
37.633134	1358.261298	17.970125
37.585691	1356.918049	17.975143
37.416336	1362.603239	17.980160
37.665690	1348.952674	17.985178
37.554659	1352.747785	17.990195
37.649257	1358.716680	17.995213
37.572548	1358.741382	18.000231
37.608864	1353.881920	18.005248
37.912775	1351.016113	18.010266
37.438756	1362.477061	18.015283
37.854525	1363.696446	18.020301
37.918014	1368.938041	18.025319
37.929530	1373.641802	18.030336
38.066773	1379.105384	18.035354
38.386852	1373.450344	18.040371
38.279286	1368.600797	18.045389
38.321344	1350.974667	18.050407
38.104730	1345.410035	18.055424
38.090244	1345.595409	18.060442
37.904487	1364.601220	18.065459
38.433145	1368.280331	18.070477
38.311915	1369.990968	18.075495
38.334555	1366.793670	18.080512
38.914875	1367.778982	18.085530
38.516623	1376.072129	18.090547
38.618967	1357.770643	18.095565
38.720827	1366.345207	18.100583
38.383231	1368.301191	18.105600
38.625675	1364.192105	18.110618
38.886393	1368.067836	18.115635
38.406307	1371.317989	18.120653
38.412876	1365.361762	18.125671
38.230268	1369.291172	18.130688
38.904662	1367.112118	18.135706
38.708736	1368.556735	18.140723
38.931743	1369.064676	18.145741
38.602210	1370.523915	18.150759
38.820505	1369.965887	18.155776
38.867314	1358.253237	18.160794
38.545367	1376.870127	18.165811
38.894051	1384.232018	18.170829
39.083564	1384.284440	18.175847
39.126167	1390.618113	18.180864
39.124513	1394.471839	18.185882
39.076992	1388.574574	18.190899
39.107687	1398.384809	18.195917
39.475237	1393.495532	18.200935
39.238683	1390.553443	18.205952
39.217958	1380.950061	18.210970
38.924516	1385.376544	18.215987
39.268807	1388.251375	18.221005
39.700984	1384.712186	18.226023
39.155244	1384.810374	18.231040
39.627626	1393.137542	18.236058
39.522116	1406.658420	18.241075
39.689434	1402.501132	18.246093
39.953333	1401.516217	18.251111
39.845802	1399.380770	18.256128
39.951061	1390.881161	18.261146
39.705133	1382.278781	18.266163
39.840446	1380.256773	18.271181
39.817705	1383.249073	18.276199
39.472534	1384.079574	18.281216
39.944508	1391.513674	18.286234
40.122400	1412.027908	18.291251
40.194628	1404.502344	18.296269
40.061983	1399.710369	18.301287
40.401107	1408.853721	18.306304
40.405778	1397.703094	18.311322
40.155576	1389.511653	18.316339
40.274663	1380.119906	18.321357
40.432095	1382.247652	18.326375
40.432259	1371.545891	18.331392
40.511884	1364.855507	18.336410
39.915847	1375.404580	18.341427
40.457465	1386.359264	18.346445
40.398292	1393.703006	18.351463
40.068654	1400.719881	18.356480
40.462102	1395.637189	18.361498
40.208757	1402.294957	18.366515
40.282465	1392.452702	18.371533
40.008582	1392.227417	18.376551
40.274650	1402.322683	18.381568
40.509251	1417.756436	18.386586
40.378695	1426.127591	18.391603
40.638934	1424.758223	18.396621
40.785061	1425.088854	18.401639
40.851047	1422.339211	18.406656
40.817169	1424.910365	18.411674
40.961689	1425.244404	18.416691
40.694506	1426.390907	18.421709
40.740779	1427.955379	18.426727
40.841456	1444.249621	18.431744
41.178865	1450.404576	18.436762
40.700312	1456.999815	18.441779
40.924892	1459.290627	18.446797
41.128194	1452.110597	18.451815
41.318617	1456.344516	18.456832
41.254295	1447.435927	18.461850
41.256952	1451.232182	18.466867
41.163099	1451.284818	18.471885
41.873130	1455.358428	18.476903
41.587355	1452.578682	18.481920
41.469896	1442.463379	18.486938
41.538063	1461.044483	18.491955
42.042923	1455.814924	18.496973
41.930283	1447.194786	18.501991
41.694531	1447.140260	18.507008
42.152988	1446.932784	18.512026
42.093787	1443.410608	18.517043
41.865407	1444.027144	18.522061
42.228647	1444.557300	18.527079
41.870662	1442.315914	18.532096
42.186696	1437.911244	18.537114
42.258527	1446.383249	18.542131
41.744833	1438.469765	18.547149
42.147050	1434.483960	18.552167
42.173076	1440.570928	18.557184
42.020837	1440.493849	18.562202
42.435419	1442.395112	18.567219
42.512530	1441.805551	18.572237
42.141183	1435.028000	18.577255
42.249592	1442.282387	18.582272
42.338701	1442.104376	18.587290
41.981798	1441.983620	18.592307
42.261485	1449.252202	18.597325
42.497739	1459.030264	18.602343
42.159211	1467.976847	18.607360
42.298980	1466.039343	18.612378
42.861703	1469.268147	18.617395
42.645920	1473.164907	18.622413
42.532099	1464.336652	18.627431
42.215910	1475.921274	18.632448
42.387433	1466.786367	18.637466
42.519686	1461.466855	18.642483
42.310432	1471.362064	18.647501
42.971678	1470.886119	18.652519
43.017844	1491.291689	18.657536
43.161857	1488.788600	18.662554
43.063461	1494.285980	18.667571
43.016837	1490.446228	18.672589
43.220948	1481.438758	18.677607
42.968783	1494.080075	18.682624
42.927144	1489.690405	18.687642
43.216386	1488.559496	18.692659
42.809305	1486.445723	18.697677
43.272455	1484.138799	18.702695
43.239721	1485.491582	18.707712
42.867978	1492.136374	18.712730
43.406531	1501.314803	18.717747
43.186747	1518.139026	18.722765
43.259489	1507.659354	18.727783
43.422490	1515.997181	18.732800
43.593648	1515.086754	18.737818
43.623108	1514.094381	18.742835
43.838964	1514.142676	18.747853
43.814650	1512.142507	18.752871
43.408807	1507.980317	18.757888
43.745092	1505.686954	18.762906
44.216490	1510.438626	18.767923
44.001747	1515.035855	18.772941
44.192453	1510.786511	18.777959
43.982186	1516.282489	18.782976
43.951843	1516.707046	18.787994
44.161402	1512.861867	18.793011
44.067062	1524.591652	18.798029
44.275233	1528.876459	18.803047
44.271276	1539.478037	18.808064
44.195088	1537.170396	18.813082
44.316068	1531.489693	18.818099
44.323889	1543.370751	18.823117
44.378610	1528.040009	18.828135
44.405852	1537.693063	18.833152
44.645440	1536.311142	18.838170
44.678038	1528.400394	18.843187
44.171330	1529.625459	18.848205
44.805770	1536.311448	18.853223
44.613655	1529.480533	18.858240
44.309968	1524.835249	18.863258
44.702093	1529.908631	18.868275
44.613617	1533.977972	18.873293
44.928547	1546.135979	18.878311
44.752950	1556.584568	18.883328
45.005555	1554.862917	18.888346
44.940150	1558.609895	18.893363
44.881037	1570.753936	18.898381
45.154468	1562.710761	18.903399
45.188822	1559.637832	18.908416
44.940613	1570.571202	18.913434
45.278090	1556.906672	18.918451
45.289576	1564.883232	18.923469
45.365389	1558.114475	18.928487
45.321540	1558.143496	18.933504
45.157181	1555.322620	18.938522
45.231112	1563.235744	18.943539
45.296824	1555.685889	18.948557
45.398794	1550.128086	18.953575
45.271342	1558.495660	18.958592
45.016386	1557.658305	18.963610
45.204055	1570.833555	18.968627
45.508472	1576.611850	18.973645
45.521804	1580.469580	18.978663
45.850377	1586.969968	18.983680
45.863712	1579.472493	18.988698
46.030905	1574.721862	18.993715
45.712863	1573.515672	18.998733
45.864829	1584.443160	19.003751
45.918775	1578.157530	19.008768
46.278492	1582.106165	19.013786
46.173565	1578.824668	19.018803
46.216345	1577.098018	19.023821
46.091339	1574.147890	19.028839
46.376970	1575.965224	19.033856
45.984540	1581.363523	19.038874
46.550833	1581.972329	19.043891
46.269728	1597.673239	19.048909
46.430130	1601.151305	19.053927
46.215073	1595.665250	19.058944
46.593003	1593.166526	19.063962
46.850902	1591.355675	19.068979
46.777461	1601.535806	19.073997
46.413741	1590.837274	19.079015
46.718718	1595.501428	19.084032
46.613620	1589.133409	19.089050
46.814209	1584.393322	19.094067
46.712967	1590.654924	19.099085
46.611767	1579.274605	19.104103
46.631957	1587.615904	19.109120
46.821188	1585.250892	19.114138
46.662830	1592.906918	19.119155
46.613063	1608.839850	19.124173
46.993744	1616.256788	19.129191
47.161010	1616.713507	19.134208
46.676041	1617.913079	19.139226
47.193576	1606.842924	19.144243
47.255314	1613.236797	19.149261
47.470944	1609.248627	19.154279
47.568619	1608.857822	19.159296
47.286586	1606.285760	19.164314
47.732793	1601.914308	19.169331
47.426275	1613.838350	19.174349
47.481576	1622.401396	19.179367
47.841388	1626.166978	19.184384
48.284623	1623.459191	19.189402
48.070942	1604.727257	19.194419
47.728791	1602.271918	19.199437
47.892706	1609.432465	19.204455
48.043041	1595.790915	19.209472
47.558432	1595.409284	19.214490
48.172908	1601.363083	19.219507
47.900715	1609.942718	19.224525
48.404877	1620.272218	19.229543
48.057907	1617.176968	19.234560
48.019881	1631.681577	19.239578
48.422155	1628.248018	19.244595
48.302029	1630.523428	19.249613
48.168385	1627.075998	19.254631
48.348940	1626.435508	19.259648
48.421198	1633.843968	19.264666
48.501320	1625.310315	19.269683
48.341712	1627.112200	19.274701
48.173213	1625.929917	19.279719
48.484537	1624.113849	19.284736
48.387091	1631.987578	19.289754
48.623553	1620.595357	19.294771
48.836231	1628.508864	19.299789
48.763880	1623.448591	19.304807
48.798479	1622.029349	19.309824
48.763318	1620.311751	19.314842
48.725864	1616.328515	19.319859
48.424891	1619.515933	19.324877
49.038532	1637.210138	19.329895
49.076948	1638.861072	19.334912
49.323307	1653.712485	19.339930
49.239390	1639.451157	19.344947
49.289405	1652.591227	19.349965
49.308975	1655.321308	19.354983
49.522959	1644.352340	19.360000
49.332386	1656.267712	19.365018
49.317042	1649.816177	19.370035
49.024133	1648.650229	19.375053
49.320653	1647.111048	19.380071
49.435205	1648.513355	19.385088
49.621452	1652.763755	19.390106
49.700416	1640.979607	19.395123
49.408214	1645.677373	19.400141
49.484650	1642.802976	19.405159
49.775972	1655.302447	19.410176
49.844557	1671.343133	19.415194
49.802559	1665.741574	19.420211
49.998303	1666.843966	19.425229
49.795911	1680.127750	19.430247
50.023961	1674.001012	19.435264
49.677037	1669.738028	19.440282
50.157656	1671.707870	19.445299
50.100882	1672.105011	19.450317
49.979530	1681.112353	19.455335
50.110390	1677.733933	19.460352
50.080451	1679.490260	19.465370
50.538661	1686.667849	19.470387
50.111172	1687.012613	19.475405
50.134802	1699.181648	19.480423
50.567410	1691.829888	19.485440
50.573536	1698.964696	19.490458
50.678181	1695.558820	19.495475
50.330157	1696.061558	19.500493
50.088461	1696.740152	19.505511
50.381676	1699.673534	19.510528
50.876470	1712.693466	19.515546
50.934823	1724.576195	19.520563
50.890791	1727.751779	19.525581
50.982461	1717.963339	19.530599
51.136625	1717.011381	19.535616
51.021592	1724.941558	19.540634
51.321172	1710.222434	19.545651
51.339124	1716.402284	19.550669
50.953326	1712.372613	19.555687
51.406112	1718.626357	19.560704
51.311217	1722.037141	19.565722
51.459335	1716.689821	19.570739
51.686831	1710.604185	19.575757
51.530670	1715.571007	19.580775
51.792776	1706.642706	19.585792
51.633919	1707.579738	19.590810
51.657377	1706.389467	19.595827
51.704190	1713.943967	19.600845
51.415575	1718.312966	19.605863
51.784622	1709.405780	19.610880
51.503443	1713.678933	19.615898
51.757239	1726.080186	19.620915
51.996096	1738.382795	19.625933
52.086246	1752.192035	19.630951
52.314055	1735.631558	19.635968
52.217192	1740.409205	19.640986
52.212675	1745.920357	19.646003
52.415783	1741.293451	19.651021
52.182114	1737.902699	19.656039
52.332720	1738.071679	19.661056
52.323339	1750.315353	19.666074
52.312229	1732.611966	19.671091
52.370588	1730.564104	19.676109
52.305193	1724.221376	19.681127
52.362291	1725.124574	19.686144
52.208906	1730.106745	19.691162
52.383117	1726.958224	19.696179
52.859092	1735.660555	19.701197
52.526932	1743.612135	19.706215
53.008574	1740.980369	19.711232
52.888045	1753.048943	19.716250
52.730567	1754.866287	19.721267
53.212494	1750.381900	19.726285
52.896571	1751.337230	19.731303
53.168651	1747.942983	19.736320
52.955994	1755.844285	19.741338
53.135383	1755.617410	19.746355
53.426548	1753.239562	19.751373
53.116972	1755.418430	19.756391
53.357917	1751.773423	19.761408
53.141000	1755.130743	19.766426
53.547141	1747.625307	19.771443
53.188733	1750.686038	19.776461
53.311481	1765.676840	19.781479
53.580156	1766.095582	19.786496
53.320949	1779.520893	19.791514
53.757275	1774.169428	19.796531
53.719690	1772.158686	19.801549
53.474566	1772.834664	19.806567
53.775125	1778.004520	19.811584
53.808385	1783.118419	19.816602
53.928485	1776.639306	19.821619
54.029674	1769.014371	19.826637
54.049866	1792.555115	19.831655
54.543176	1791.218636	19.836672
54.191820	1798.586229	19.841690
54.243397	1795.116060	19.846707
54.318208	1789.499318	19.851725
54.385120	1800.108882	19.856743
54.599953	1793.876870	19.861760
54.527994	1800.231793	19.866778
54.102220	1794.560926	19.871795
54.595152	1779.849323	19.876813
54.620131	1791.248143	19.881831
54.793871	1790.974813	19.886848
54.781600	1794.006568	19.891866
54.748970	1789.795305	19.896883
54.949757	1784.676414	19.901901
54.915245	1796.646328	19.906919
54.938394	1787.938474	19.911936
55.098718	1787.944975	19.916954
55.286593	1787.880883	19.921971
55.096501	1785.976089	19.926989
54.900686	1782.670923	19.932007
55.506171	1788.026552	19.937024
55.115315	1783.603155	19.942042
55.379197	1790.830169	19.947059
55.660869	1796.952949	19.952077
55.458684	1792.253821	19.957095
55.258626	1785.228378	19.962112
55.146775	1798.782106	19.967130
55.181108	1796.182542	19.972147
55.479682	1799.118256	19.977165
55.162774	1813.385821	19.982183
55.542032	1809.763317	19.987200
55.583251	1813.733500	19.992218
55.315934	1818.749326	19.997235
55.614136	1827.141861	20.002253
55.295596	1834.823085	20.007271
55.947536	1825.637975	20.012288
55.919417	1837.455426	20.017306
56.085066	1854.437342	20.022323
56.494251	1846.852487	20.027341
56.514305	1852.255674	20.032359
56.699666	1848.228010	20.037376
56.642640	1830.926222	20.042394
56.534668	1831.366104	20.047411
56.482617	1823.171823	20.052429
56.239956	1828.549887	20.057447
56.404999	1842.246470	20.062464
56.527871	1856.350485	20.067482
56.382659	1857.184394	20.072499
56.942267	1850.238736	20.077517
56.624270	1849.120889	20.082535
56.890309	1840.046728	20.087552
56.915583	1841.434634	20.092570
56.533431	1853.856712	20.097587
57.175764	1860.469000	20.102605
57.286058	1865.684471	20.107623
57.438739	1876.271174	20.112640
57.142670	1871.337408	20.117658
56.978843	1875.140900	20.122675
57.214307	1882.467085	20.127693
57.261687	1883.965147	20.132711
57.166305	1875.711354	20.137728
57.375410	1881.798192	20.142746
57.406876	1875.083604	20.147763
57.454165	1874.836396	20.152781
57.187289	1886.031677	20.157799
57.336327	1888.059806	20.162816
57.754183	1890.544471	20.167834
57.882877	1912.064293	20.172851
57.957010	1901.811407	20.177869
57.643797	1901.399758	20.182887
57.591978	1901.303787	20.187904
58.060794	1913.002403	20.192922
58.364472	1925.866228	20.197939
58.506315	1920.232631	20.202957
58.198067	1919.952757	20.207975
58.390550	1923.312243	20.212992
58.825740	1918.756235	20.218010
58.220309	1914.363267	20.223027
58.833775	1911.057525	20.228045
58.611646	1917.546478	20.233063
58.939938	1915.232225	20.238080
58.862116	1921.749068	20.243098
58.673362	1918.445926	20.248115
58.916048	1911.117521	20.253133
58.639280	1920.679546	20.258151
58.718045	1921.077550	20.263168
58.819086	1920.174933	20.268186
58.369148	1926.626993	20.273203
58.909560	1912.046709	20.278221
58.801193	1916.059288	20.283239
59.186690	1909.607979	20.288256
59.395382	1930.443054	20.293274
59.317175	1943.723356	20.298291
59.328067	1943.898448	20.303309
59.330714	1952.425716	20.308327
59.167699	1941.111660	20.313344
59.466305	1944.211508	20.318362
59.396928	1942.186791	20.323379
59.513209	1939.713233	20.328397
59.635716	1937.421750	20.333415
59.374836	1946.466866	20.338432
59.363658	1947.099885	20.343450
59.755225	1962.345402	20.348467
59.694373	1962.970424	20.353485
59.179794	1966.156652	20.358503
60.069328	1965.092624	20.363520
59.992724	1966.389195	20.368538
60.109563	1971.578423	20.373555
60.092033	1974.850892	20.378573
60.023562	1990.929117	20.383591
60.465971	1990.143439	20.388608
60.459790	1992.773456	20.393626
60.243889	2000.078880	20.398643
60.470001	1991.856721	20.403661
60.428767	1998.213212	20.408679
60.711267	1990.916410	20.413696
60.927508	1984.450564	20.418714
60.865797	1989.150179	20.423731
61.296901	1979.500935	20.428749
61.044074	1983.785490	20.433767
61.075969	1985.207086	20.438784
61.063504	1984.558952	20.443802
60.879905	1981.434886	20.448819
61.264967	1982.715936	20.453837
61.261559	1977.657386	20.458855
61.449093	1969.507558	20.463872
61.274280	1971.292923	20.468890
61.579795	1979.425588	20.473907
61.571876	1978.035072	20.478925
61.356012	1976.913839	20.483943
61.399326	1988.259414	20.488960
61.731217	1995.886142	20.493978
61.750009	2004.458247	20.498995
61.753794	1998.076179	20.504013
61.934159	1998.268903	20.509031
61.711953	1996.984548	20.514048
61.924957	1996.136974	20.519066
61.947444	2002.029013	20.524083
61.886405	1990.822034	20.529101
61.814607	1994.282905	20.534119
61.588569	1998.948304	20.539136
62.172410	2004.806046	20.544154
62.135195	2022.823530	20.549171
62.110495	2016.881454	20.554189
62.149565	2022.370082	20.559207
62.076297	2024.486709	20.564224
62.293235	2027.978093	20.569242
62.186416	2046.448353	20.574259
62.463587	2042.535660	20.579277
62.426583	2044.283661	20.584295
62.422533	2053.358025	20.589312
62.854843	2052.438217	20.594330
62.731502	2065.195462	20.599347
62.956444	2082.016813	20.604365
63.191494	2073.698534	20.609383
63.160917	2074.369313	20.614400
63.302598	2081.056967	20.619418
63.292619	2076.722158	20.624435
63.454175	2069.141291	20.629453
63.495416	2063.220429	20.634471
63.160337	2066.908769	20.639488
63.301248	2074.066795	20.644506
63.047409	2074.800958	20.649523
63.321986	2072.223680	20.654541
63.358594	2074.714450	20.659559
63.663314	2080.158319	20.664576
63.935353	2099.576061	20.669594
64.008161	2090.478397	20.674611
64.144839	2092.183411	20.679629
64.226656	2096.544960	20.684647
63.936523	2094.065623	20.689664
64.132637	2101.095079	20.694682
63.891662	2096.228364	20.699699
63.922743	2095.639681	20.704717
64.086068	2088.588748	20.709735
64.009932	2097.939538	20.714752
64.376512	2092.942919	20.719770
64.316703	2103.256910	20.724787
64.390753	2116.513484	20.729805
64.481374	2114.618328	20.734823
64.712767	2116.185418	20.739840
64.697751	2111.860858	20.744858
64.438519	2116.739788	20.749875
64.626743	2118.566128	20.754893
64.560467	2120.615393	20.759911
64.543598	2137.768197	20.764928
65.186662	2135.477189	20.769946
64.807062	2141.050385	20.774963
64.804212	2152.005631	20.779981
65.208229	2134.022195	20.784999
65.019743	2143.018193	20.790016
65.534170	2154.965464	20.795034
65.759183	2171.865790	20.800051
65.840496	2162.675230	20.805069
66.129000	2163.087720	20.810087
65.784093	2145.950663	20.815104
65.919136	2137.439722	20.820122
65.626154	2144.719408	20.825139
65.705279	2149.112954	20.830157
66.322832	2155.025430	20.835175
66.381174	2157.730576	20.840192
66.361598	2151.819213	20.845210
66.540350	2150.535148	20.850227
66.410702	2140.569695	20.855245
66.129351	2128.011631	20.860263
66.077730	2126.874124	20.865280
66.177532	2132.741468	20.870298
66.368908	2154.605241	20.875315
66.033146	2150.441386	20.880333
66.627568	2150.155795	20.885351
66.338654	2151.438302	20.890368
66.803965	2145.990661	20.895386
66.631183	2149.915545	20.900403
66.964110	2168.550584	20.905421
67.108032	2179.968889	20.910439
67.244562	2175.121909	20.915456
67.017562	2176.988060	20.920474
67.042323	2173.193787	20.925491
67.442128	2170.495880	20.930509
67.367900	2169.175704	20.935527
67.285968	2163.775923	20.940544
67.213644	2161.858949	20.945562
67.223433	2172.591303	20.950579
67.399313	2164.206507	20.955597
67.567823	2155.999609	20.960615
67.695620	2160.268757	20.965632
68.015009	2158.874287	20.970650
67.701823	2163.300896	20.975667
67.881672	2170.105691	20.980685
67.912254	2165.161694	20.985703
67.593765	2172.915643	20.990720
67.870755	2179.657881	20.995738
68.057701	2182.974098	21.000755
67.620465	2180.252684	21.005773
68.072609	2191.294473	21.010791
67.821448	2200.366598	21.015808
68.240317	2202.156810	21.020826
68.252252	2210.095714	21.025843
68.033777	2218.036003	21.030861
68.511638	2215.976015	21.035879
67.945282	2231.662203	21.040896
68.477870	2224.004203	21.045914
68.378533	2231.143122	21.050931
68.615603	2242.995037	21.055949
68.816515	2244.292335	21.060967
68.305943	2248.409031	21.065984
68.874110	2258.675221	21.071002
68.970206	2250.971977	21.076019
69.242422	2259.558152	21.081037
69.527021	2266.504377	21.086055
69.407850	2270.269395	21.091072
69.348423	2269.111009	21.096090
69.464604	2266.848881	21.101107
69.148877	2271.856636	21.106125
69.393107	2263.180193	21.111143
69.715932	2271.834191	21.116160
69.397395	2260.190816	21.121178
69.711351	2264.743276	21.126195
69.742935	2281.352089	21.131213
70.009660	2283.361825	21.136231
69.922534	2293.702298	21.141248
70.070585	2288.945009	21.146266
69.943865	2296.457508	21.151283
69.935582	2285.516661	21.156301
70.261931	2283.272101	21.161319
69.984227	2291.890795	21.166336
70.270083	2299.752105	21.171354
70.729220	2308.599380	21.176371
70.661463	2308.038800	21.181389
71.095393	2305.629045	21.186407
70.950606	2316.297331	21.191424
70.862303	2308.433587	21.196442
70.726332	2311.320692	21.201459
70.723762	2313.151695	21.206477
71.035183	2302.220716	21.211495
70.825489	2314.862266	21.216512
71.283296	2309.882856	21.221530
71.269622	2308.868792	21.226547
70.952020	2314.621693	21.231565
71.235788	2326.447411	21.236583
71.170264	2332.984569	21.241600
71.136293	2331.235154	21.246618
71.210960	2333.413855	21.251635
71.502744	2328.138528	21.256653
71.851774	2340.282266	21.261671
71.784184	2347.523565	21.266688
71.768529	2348.542345	21.271706
72.001392	2353.612510	21.276723
72.074454	2355.362234	21.281741
72.377702	2351.360174	21.286759
71.922180	2360.350776	21.291776
71.864928	2364.475378	21.296794
72.533862	2371.737006	21.301811
72.289195	2364.598393	21.306829
72.389047	2350.026814	21.311847
72.393162	2358.617168	21.316864
72.725410	2355.932975	21.321882
72.457645	2355.801400	21.326899
72.394935	2356.922236	21.331917
72.821460	2365.904049	21.336935
72.631532	2384.195154	21.341952
72.961435	2374.422686	21.346970
73.128135	2381.409520	21.351987
72.534385	2380.760916	21.357005
73.041058	2373.779167	21.362023
73.016422	2382.910576	21.367040
72.932529	2378.214852	21.372058
73.555858	2398.319568	21.377075
73.242886	2407.653970	21.382093
73.149551	2402.142284	21.387111
73.465566	2405.372043	21.392128
73.235888	2410.224328	21.397146
73.399184	2402.819791	21.402163
73.053089	2420.368462	21.407181
73.577234	2423.628738	21.412199
73.701074	2432.607509	21.417216
73.798912	2434.700533	21.422234
73.597966	2436.051336	21.427251
73.815972	2441.931823	21.432269
74.082261	2456.174803	21.437287
74.102550	2454.473686	21.442304
74.066732	2452.134352	21.447322
74.743926	2454.240761	21.452339
74.451975	2454.292874	21.457357
74.249076	2453.551470	21.462375
74.168040	2470.553681	21.467392
74.586423	2475.055117	21.472410
74.938719	2475.965758	21.477427
74.913051	2480.950219	21.482445
74.853515	2472.725253	21.487463
75.364521	2472.506382	21.492480
75.294377	2481.001119	21.497498
75.422654	2477.894382	21.502515
75.208612	2481.664839	21.507533
75.862396	2484.986875	21.512551
75.440126	2478.851288	21.517568
75.773996	2482.996698	21.522586
75.681120	2483.203833	21.527603
75.394746	2491.372653	21.532621
75.715942	2494.955104	21.537639
75.713372	2489.719535	21.542656
75.833876	2491.881605	21.547674
75.861508	2488.986315	21.552691
75.728594	2495.388907	21.557709
76.058181	2487.330211	21.562727
76.387278	2495.241642	21.567744
75.902897	2507.752776	21.572762
76.469909	2505.385268	21.577779
76.327872	2521.466024	21.582797
76.352941	2517.914652	21.587815
76.554070	2519.865257	21.592832
76.433192	2510.333773	21.597850
76.625499	2519.005183	21.602867
76.536176	2530.094141	21.607885
77.261184	2523.532612	21.612903
76.876523	2534.683625	21.617920
76.835320	2538.616384	21.622938
77.196584	2530.379117	21.627955
77.257166	2532.039285	21.632973
77.464474	2537.694238	21.637991
77.817181	2523.660478	21.643008
77.410211	2531.886084	21.648026
77.729116	2523.567085	21.653043
77.370183	2526.732180	21.658061
78.008088	2524.779642	21.663079
78.165223	2524.351097	21.668096
77.600126	2538.961108	21.673114
77.912819	2522.938935	21.678131
77.773299	2530.772307	21.683149
77.464165	2530.489404	21.688167
77.789631	2529.179171	21.693184
77.603577	2532.430802	21.698202
77.848967	2545.869155	21.703219
78.037960	2558.603065	21.708237
78.076735	2553.550368	21.713255
78.336368	2547.497291	21.718272
78.420334	2562.349651	21.723290
78.414581	2577.399137	21.728307
78.593532	2569.745899	21.733325
78.506018	2580.853542	21.738343
79.072803	2572.315784	21.743360
78.925667	2564.757823	21.748378
79.088431	2569.561291	21.753395
79.197142	2578.182704	21.758413
79.089819	2571.088770	21.763431
79.326857	2575.965819	21.768448
79.306642	2599.381393	21.773466
79.402891	2586.883782	21.778483
79.409009	2596.821612	21.783501
79.614222	2597.035701	21.788519
79.939240	2600.911097	21.793536
79.726633	2604.583514	21.798554
80.123506	2590.883647	21.803571
79.788569	2597.014936	21.808589
79.937751	2594.722348	21.813607
79.772383	2593.002962	21.818624
79.827959	2600.392342	21.823642
79.945595	2611.079655	21.828659
80.289784	2619.657883	21.833677
80.270883	2619.673528	21.838695
80.717527	2622.074884	21.843712
80.360648	2623.260761	21.848730
80.381135	2615.597613	21.853747
80.117192	2623.005500	21.858765
80.204986	2625.276865	21.863783
80.301189	2637.072207	21.868800
80.742643	2640.430695	21.873818
80.727796	2652.896772	21.878835
80.986664	2668.936942	21.883853
80.942741	2668.672452	21.888871
81.190027	2666.118304	21.893888
81.475614	2670.912025	21.898906
81.687345	2673.511156	21.903923
81.394537	2673.115227	21.908941
81.282338	2671.273882	21.913959
81.633939	2675.741645	21.918976
81.657039	2690.262781	21.923994
81.868869	2694.380018	21.929011
82.099952	2692.327080	21.934029
82.098722	2700.899497	21.939047
81.931059	2697.128948	21.944064
81.707893	2700.285427	21.949082
82.296685	2696.364801	21.954099
81.804687	2700.952114	21.959117
81.761333	2717.109112	21.964135
81.936877	2713.060701	21.969152
81.925710	2730.159521	21.974170
82.469786	2733.864909	21.979187
82.396394	2740.712753	21.984205
82.500626	2749.729472	21.989223
83.059382	2746.350093	21.994240
82.599503	2756.938602	21.999258
82.775374	2746.028591	22.004275
82.808646	2762.050533	22.009293
83.028311	2767.631030	22.014311
83.192013	2766.068380	22.019328
83.172884	2772.964545	22.024346
83.633526	2769.654189	22.029363
83.823408	2764.132737	22.034381
84.236744	2765.920719	22.039399
84.117809	2763.629085	22.044416
84.242337	2769.104553	22.049434
84.234656	2759.956037	22.054451
84.199744	2753.444048	22.059469
84.163134	2759.108879	22.064487
84.681593	2744.461930	22.069504
84.340855	2753.185405	22.074522
84.448604	2749.602097	22.079539
84.363753	2748.526568	22.084557
84.482037	2741.649714	22.089575
84.460818	2744.585190	22.094592
84.519264	2752.662230	22.099610
84.718721	2745.980965	22.104627
84.311723	2747.168390	22.109645
84.706635	2757.752381	22.114663
85.070685	2764.531699	22.119680
85.265836	2777.384734	22.124698
85.089938	2777.443913	22.129715
84.925152	2775.194180	22.134733
84.944231	2779.341636	22.139751
84.968875	2776.642451	22.144768
85.145597	2793.159561	22.149786
84.964371	2793.380541	22.154803
84.942545	2798.815823	22.159821
85.410428	2819.150517	22.164839
85.878952	2808.226181	22.169856
85.905382	2826.796300	22.174874
86.153391	2823.238346	22.179891
86.418888	2826.252007	22.184909
85.772272	2825.245548	22.189927
86.105774	2817.315496	22.194944
86.512729	2839.370416	22.199962
86.684626	2838.986894	22.204979
86.886355	2832.690298	22.209997
86.788485	2833.879796	22.215015
86.808745	2841.233777	22.220032
86.944465	2846.814825	22.225050
86.909541	2842.682580	22.230067
86.876048	2849.180188	22.235085
86.953009	2850.209735	22.240103
86.944946	2841.395795	22.245120
87.064985	2845.360170	22.250138
87.249727	2839.845814	22.255155
87.183992	2844.009729	22.260173
87.467169	2853.853795	22.265191
87.533399	2856.643028	22.270208
87.598730	2867.013598	22.275226
87.326658	2862.391417	22.280243
87.668770	2865.727639	22.285261
87.741269	2862.620106	22.290279
87.477502	2865.372667	22.295296
87.852241	2883.335939	22.300314
88.003195	2891.430110	22.305331
88.086497	2888.131508	22.310349
88.255939	2897.157022	22.315367
88.130762	2887.427170	22.320384
88.081654	2905.879801	22.325402
88.521582	2916.608331	22.330419
88.948922	2914.824461	22.335437
88.955891	2927.344121	22.340455
88.986235	2910.463163	22.345472
88.919542	2913.970753	22.350490
88.959455	2912.430641	22.355507
89.355423	2909.786884	22.360525
88.596424	2915.729064	22.365543
89.372208	2911.144700	22.370560
89.623250	2912.664596	22.375578
89.445048	2917.537358	22.380595
89.590180	2931.925946	22.385613
89.708276	2939.349857	22.390631
89.978972	2934.330156	22.395648
89.656595	2935.223432	22.400666
89.930548	2936.326277	22.405683
89.740151	2937.104189	22.410701
89.719386	2939.989126	22.415719
90.093349	2937.882213	22.420736
89.806034	2945.107676	22.425754
89.959009	2958.371444	22.430771
90.409128	2963.076342	22.435789
89.972652	2958.732390	22.440807
90.439203	2970.406804	22.445824
90.601119	2978.212081	22.450842
90.569875	2981.281727	22.455859
90.954303	2979.450917	22.460877
90.654537	2981.379050	22.465895
91.208259	2983.189247	22.470912
91.099522	2978.696101	22.475930
90.992009	2991.457833	22.480947
91.230887	3002.748160	22.485965
91.249547	3007.735290	22.490983
91.457897	2989.705910	22.496000
91.726929	3000.868418	22.501018
91.493362	2995.252271	22.506035
91.648893	3009.402575	22.511053
91.689639	3013.051162	22.516071
91.977092	3016.070884	22.521088
91.950719	3023.959336	22.526106
92.222868	3025.463310	22.531123
92.402682	3015.893917	22.536141
92.284013	3021.625343	22.541159
92.369285	3027.024977	22.546176
92.626442	3034.957388	22.551194
92.621512	3044.076575	22.556211
93.134839	3038.239243	22.561229
93.207533	3049.094825	22.566247
93.211631	3038.659735	22.571264
93.480245	3038.456743	22.576282
92.995846	3042.351735	22.581299
93.345598	3037.281745	22.586317
93.369232	3041.958795	22.591335
93.295600	3036.642669	22.596352
93.822190	3037.478692	22.601370
93.614755	3040.414984	22.606387
93.453790	3035.434477	22.611405
93.448533	3044.351718	22.616423
93.817616	3056.732673	22.621440
94.049364	3067.727472	22.626458
93.770834	3076.002638	22.631475
93.622985	3063.634471	22.636493
93.698303	3069.670081	22.641511
93.890650	3080.011406	22.646528
94.103895	3090.532525	22.651546
93.959410	3089.428443	22.656563
94.470540	3102.768767	22.661581
94.417569	3118.236413	22.666599
94.394615	3120.572535	22.671616
94.425173	3113.971252	22.676634
94.740288	3121.212872	22.681651
94.980261	3129.252172	22.686669
95.143313	3143.574997	22.691687
95.055640	3153.486797	22.696704
95.649464	3142.369035	22.701722
95.573163	3148.169613	22.706739
95.708303	3146.570375	22.711757
95.804615	3140.173406	22.716775
96.146931	3145.703242	22.721792
96.251034	3139.358710	22.726810
96.022330	3146.063758	22.731827
95.922196	3135.067348	22.736845
96.011412	3143.076618	22.741863
95.991968	3130.467350	22.746880
96.218367	3133.105282	22.751898
96.093933	3160.000317	22.756915
96.483393	3167.189276	22.761933
96.233437	3167.780841	22.766951
96.319547	3167.439159	22.771968
96.713429	3158.076028	22.776986
96.357945	3172.047707	22.782003
96.701185	3182.368607	22.787021
96.760000	3193.999734	22.792039
96.827961	3192.262672	22.797056
97.137443	3204.782474	22.802074
96.975264	3220.213660	22.807091
96.935563	3213.850600	22.812109
97.038735	3217.293760	22.817127
97.395759	3233.890339	22.822144
97.643029	3239.119469	22.827162
97.622523	3236.345226	22.832179
97.940507	3232.504790	22.837197
97.905733	3246.915503	22.842215
98.257847	3239.708293	22.847232
98.514153	3242.717152	22.852250
98.772312	3251.874134	22.857267
99.081312	3252.299223	22.862285
98.302170	3239.982495	22.867303
98.346070	3243.535947	22.872320
98.806174	3254.223644	22.877338
98.501196	3251.560248	22.882355
98.889758	3258.197037	22.887373
98.955294	3257.886984	22.892391
99.161938	3258.277609	22.897408
99.394255	3268.789531	22.902426
99.623753	3293.934396	22.907443
99.508568	3282.410000	22.912461
99.416356	3281.266154	22.917479
99.439077	3288.840871	22.922496
99.819208	3281.932257	22.927514
99.666876	3291.159883	22.932531
99.472502	3286.380230	22.937549
100.016472	3300.678220	22.942567
99.957940	3315.913342	22.947584
100.048343	3308.917547	22.952602
100.154745	3312.328656	22.957619
100.638351	3299.795115	22.962637
100.939433	3296.143535	22.967655
100.813436	3288.250549	22.972672
100.890566	3285.527284	22.977690
101.018957	3296.147036	22.982707
100.933730	3288.743198	22.987725
101.003291	3309.510137	22.992743
101.264453	3316.949665	22.997760
101.690976	3314.070655	23.002778
101.062282	3313.528487	23.007795
101.353834	3314.161470	23.012813
101.408249	3320.244626	23.017831
101.358872	3315.884129	23.022848
101.811175	3304.924160	23.027866
101.769008	3308.203888	23.032883
101.512776	3304.200897	23.037901
101.760571	3325.953097	23.042919
101.772415	3327.870321	23.047936
102.037719	3330.884098	23.052954
102.007969	3340.812176	23.057971
102.162369	3350.818723	23.062989
102.295106	3356.605556	23.068007
102.455245	3368.198826	23.073024
102.687215	3360.565355	23.078042
102.953325	3366.681644	23.083059
102.996316	3361.347151	23.088077
102.854954	3367.047522	23.093095
102.702463	3389.222328	23.098112
102.981354	3381.126991	23.103130
103.232056	3384.007343	23.108147
103.385568	3386.795609	23.113165
103.442607	3390.416470	23.118183
103.277099	3407.142419	23.123200
103.515515	3403.323882	23.128218
103.624264	3416.610698	23.133235
103.693595	3417.493127	23.138253
103.828065	3421.957221	23.143271
104.086680	3432.143176	23.148288
104.274255	3438.770489	23.153306
104.395471	3452.396257	23.158323
104.165501	3440.624614	23.163341
104.440338	3445.568574	23.168359
104.421774	3463.966488	23.173376
104.538320	3464.869930	23.178394
104.285654	3463.366140	23.183411
104.497039	3474.418035	23.188429
104.991393	3480.889986	23.193447
104.905845	3483.759908	23.198464
105.109646	3488.137404	23.203482
105.211519	3496.327914	23.208499
105.677438	3503.558687	23.213517
105.578949	3516.032150	23.218535
105.357190	3517.821864	23.223552
105.906849	3508.566713	23.228570
105.730583	3520.032876	23.233587
105.500974	3525.740809	23.238605
105.995636	3528.601902	23.243623
106.033207	3541.817896	23.248640
106.299739	3535.532998	23.253658
106.405130	3540.973823	23.258675
106.675191	3559.973662	23.263693
106.264313	3556.834425	23.268711
106.421710	3565.565467	23.273728
106.948280	3562.872749	23.278746
107.202991	3566.096543	23.283763
107.187792	3559.559080	23.288781
107.326156	3576.373299	23.293799
107.187214	3587.079294	23.298816
107.373273	3590.320161	23.303834
107.125211	3587.739331	23.308851
107.634776	3589.502853	23.313869
107.754024	3584.579297	23.318887
107.879676	3606.470911	23.323904
108.132978	3610.802805	23.328922
108.160863	3607.623226	23.333939
108.076407	3607.664924	23.338957
108.337872	3601.453393	23.343975
108.440749	3606.569529	23.348992
108.557753	3605.279256	23.354010
108.787323	3603.103357	23.359027
108.411213	3598.740322	23.364045
108.735239	3613.265555	23.369063
108.768173	3626.333990	23.374080
108.915661	3628.971734	23.379098
108.920497	3632.480881	23.384115
109.060638	3628.182150	23.389133
109.101814	3625.407652	23.394151
109.266429	3656.332968	23.399168
109.397785	3648.614136	23.404186
109.662910	3650.292863	23.409203
109.660259	3655.498142	23.414221
110.087292	3644.781811	23.419239
109.848410	3657.675066	23.424256
110.331850	3669.293631	23.429274
110.409898	3678.021377	23.434291
110.453301	3681.931660	23.439309
110.631995	3673.564663	23.444327
110.675016	3672.241788	23.449344
110.981546	3661.152939	23.454362
111.141236	3670.445502	23.459379
111.290104	3674.825337	23.464397
111.482495	3657.056613	23.469415
111.069317	3661.066830	23.474432
110.932843	3666.618182	23.479450
111.136952	3670.175025	23.484467
111.260176	3684.078412	23.489485
111.412718	3685.392863	23.494503
111.148339	3692.946446	23.499520
111.736527	3683.129654	23.504538
112.103960	3701.236923	23.509555
111.867079	3700.485007	23.514573
112.238350	3695.067422	23.519591
112.335375	3704.609702	23.524608
112.652178	3693.326687	23.529626
112.496209	3693.742569	23.534643
112.332598	3697.877825	23.539661
112.526317	3697.588715	23.544679
112.270949	3719.887358	23.549696
112.431089	3721.001772	23.554714
112.818443	3731.183509	23.559731
112.965350	3739.916279	23.564749
113.090143	3748.753521	23.569767
112.854940	3763.063479	23.574784
112.870209	3746.992130	23.579802
113.139916	3768.217475	23.584819
113.118108	3767.185665	23.589837
113.579972	3780.423738	23.594855
113.732830	3799.101303	23.599872
113.988623	3806.390370	23.604890
114.121443	3805.387991	23.609907
114.105206	3809.064605	23.614925
114.303031	3811.489325	23.619943
114.124910	3825.793545	23.624960
114.475658	3823.734359	23.629978
114.868385	3835.171548	23.634995
114.834409	3833.415675	23.640013
115.076163	3835.801953	23.645031
114.923013	3844.714351	23.650048
115.184974	3856.591838	23.655066
115.125508	3858.908524	23.660083
115.095054	3861.460550	23.665101
115.075967	3856.271362	23.670119
115.351399	3880.617597	23.675136
115.561135	3882.570160	23.680154
115.835536	3878.780608	23.685171
115.675876	3880.791043	23.690189
115.922449	3898.172538	23.695207
115.787964	3910.876016	23.700224
116.004393	3912.938008	23.705242
115.976300	3910.982354	23.710259
115.961734	3926.308949	23.715277
116.248204	3932.438022	23.720295
116.259408	3940.775506	23.725312
117.150794	3940.175081	23.730330
117.044543	3958.738742	23.735347
117.203733	3963.259068	23.740365
117.168604	3955.455715	23.745383
117.197706	3963.553676	23.750400
117.545919	3967.002779	23.755418
117.235756	3956.657427	23.760435
117.530191	3976.417732	23.765453
117.698450	3982.079258	23.770471
117.659329	3985.257625	23.775488
117.868882	3998.503824	23.780506
118.208607	3985.733529	23.785523
117.698448	4004.183757	23.790541
118.116378	4010.639466	23.795559
118.359106	4020.294810	23.800576
118.324068	4024.731950	23.805594
118.520986	4030.051266	23.810611
118.666846	4039.816489	23.815629
118.728764	4039.257633	23.820647
118.836297	4046.210193	23.825664
118.795110	4058.233155	23.830682
119.264261	4069.560671	23.835699
119.170503	4079.843231	23.840717
119.764687	4081.429413	23.845735
119.876808	4097.414934	23.850752
119.636430	4098.282791	23.855770
120.324595	4099.544923	23.860787
119.965392	4102.448346	23.865805
119.985929	4097.262351	23.870823
120.194206	4097.217155	23.875840
120.390950	4123.236318	23.880858
120.902659	4117.354708	23.885875
120.688845	4123.780018	23.890893
120.525437	4125.996235	23.895911
120.695573	4131.550194	23.900928
120.661030	4140.778736	23.905946
121.335779	4142.106101	23.910963
121.052599	4144.394744	23.915981
121.382060	4148.307658	23.920999
121.209011	4162.949086	23.926016
121.335764	4174.519696	23.931034
121.741212	4175.324254	23.936051
121.884816	4184.035660	23.941069
121.976612	4187.982661	23.946087
121.960860	4205.465521	23.951104
121.628980	4205.981571	23.956122
122.164017	4201.431452	23.961139
122.230695	4211.275458	23.966157
122.526699	4227.270162	23.971175
122.588003	4223.015207	23.976192
122.370380	4230.631128	23.981210
122.836535	4232.117438	23.986227
122.827974	4252.569428	23.991245
122.844412	4256.010593	23.996263
123.365941	4258.561421	24.001280
123.145906	4275.710205	24.006298
123.598035	4275.907729	24.011315
123.824948	4278.867708	24.016333
124.031358	4273.567318	24.021351
123.976075	4275.438343	24.026368
123.942102	4286.096740	24.031386
124.311678	4291.613190	24.036403
124.117665	4290.772465	24.041421
124.390887	4297.503463	24.046439
124.589613	4291.509853	24.051456
124.230512	4296.550208	24.056474
124.817585	4308.749519	24.061491
124.600581	4318.761129	24.066509
125.073498	4320.230605	24.071527
125.195390	4323.106038	24.076544
125.340081	4317.010408	24.081562
125.427665	4320.816058	24.086579
125.383923	4335.803515	24.091597
125.677826	4347.016621	24.096615
125.663827	4341.930660	24.101632
125.715964	4343.159884	24.106650
125.953998	4364.580277	24.111667
125.810554	4362.200740	24.116685
125.868015	4361.778301	24.121703
126.011077	4377.150024	24.126720
126.423405	4394.417646	24.131738
126.622441	4392.517894	24.136755
126.585608	4408.467052	24.141773
126.501399	4408.641284	24.146791
127.298591	4417.452422	24.151808
127.213150	4424.372230	24.156826
127.386060	4423.963267	24.161843
127.114830	4424.182582	24.166861
127.288004	4441.664479	24.171879
127.455280	4445.025232	24.176896
127.462442	4455.879298	24.181914
128.060842	4454.870230	24.186931
128.085270	4475.746583	24.191949
128.165569	4476.131779	24.196967
128.600725	4476.025786	24.201984
128.469814	4480.923122	24.207002
128.235221	4477.696130	24.212019
128.682885	4493.272749	24.217037
128.619793	4507.117575	24.222055
129.531643	4498.692156	24.227072
129.584540	4497.973718	24.232090
129.536678	4486.071857	24.237107
129.901461	4491.769039	24.242125
130.054041	4483.399449	24.247143
130.580583	4490.529584	24.252160
130.354554	4487.948329	24.257178
130.110864	4479.991192	24.262195
130.089471	4489.265197	24.267213
130.008920	4482.118970	24.272231
130.248510	4492.513676	24.277248
130.283055	4504.294644	24.282266
130.567687	4503.861864	24.287283
130.509378	4511.781218	24.292301
130.470541	4508.817106	24.297319
131.171374	4514.379579	24.302336
130.716216	4523.437474	24.307354
130.908314	4524.714226	24.312371
130.949673	4543.217479	24.317389
131.221877	4552.218252	24.322407
131.256176	4555.495695	24.327424
131.444508	4564.948367	24.332442
131.634153	4572.630042	24.337459
131.793114	4576.992733	24.342477
131.914291	4592.873107	24.347495
132.017729	4598.393468	24.352512
132.221819	4614.245089	24.357530
132.418600	4607.228971	24.362547
132.465531	4615.018249	24.367565
132.583901	4629.443944	24.372583
132.616517	4630.947706	24.377600
132.599368	4642.014021	24.382618
132.896900	4639.780006	24.387635
133.360524	4660.944450	24.392653
133.033472	4668.044246	24.397671
133.607814	4660.991053	24.402688
133.624590	4674.681451	24.407706
133.619952	4679.148710	24.412723
133.685641	4686.480540	24.417741
134.038574	4701.756527	24.422759
134.181919	4682.087948	24.427776
134.006237	4699.189147	24.432794
134.591024	4702.740217	24.437811
134.505711	4717.109510	24.442829
134.557862	4717.672730	24.447847
134.826804	4717.999969	24.452864
134.846123	4723.391503	24.457882
135.026286	4733.552605	24.462899
135.011657	4744.719597	24.467917
135.203631	4747.536771	24.472935
135.641644	4757.386028	24.477952
135.618572	4771.944475	24.482970
135.518885	4764.722221	24.487987
136.203308	4768.226129	24.493005
136.032309	4777.672076	24.498023
136.368051	4782.568984	24.503040
136.062362	4786.133316	24.508058
136.494428	4793.101607	24.513075
137.166978	4795.294260	24.518093
136.561830	4795.625866	24.523111
136.868654	4801.808864	24.528128
136.942658	4815.862874	24.533146
137.333973	4816.079404	24.538163
137.311618	4816.351272	24.543181
137.097272	4828.304017	24.548199
137.630092	4831.699114	24.553216
137.521635	4842.015972	24.558234
137.720736	4854.576306	24.563251
138.049802	4853.552596	24.568269
138.015921	4869.163944	24.573287
138.090728	4866.617574	24.578304
138.131863	4879.575146	24.583322
138.173247	4898.031408	24.588339
138.658997	4895.322800	24.593357
138.794453	4905.790875	24.598375
139.060505	4920.477756	24.603392
138.947828	4930.448103	24.608410
139.210538	4925.258654	24.613427
139.441789	4919.149263	24.618445
139.455249	4929.191389	24.623463
139.738316	4947.123727	24.628480
139.919663	4957.066966	24.633498
139.685638	4955.032982	24.638515
139.671838	4969.896320	24.643533
139.905883	4976.409594	24.648551
140.179119	4976.733009	24.653568
140.305117	4993.266387	24.658586
140.485590	4999.387176	24.663603
140.801941	5001.525180	24.668621
140.637095	4999.085782	24.673639
141.025923	5015.858939	24.678656
141.021602	5028.688006	24.683674
141.309239	5026.774308	24.688691
141.574025	5030.504996	24.693709
141.941466	5037.789695	24.698727
142.210914	5041.194527	24.703744
142.114638	5044.281023	24.708762
142.173499	5048.994107	24.713779
142.253864	5044.546579	24.718797
142.205767	5056.669136	24.723815
142.226572	5053.736627	24.728832
142.468911	5072.158426	24.733850
142.049386	5077.161112	24.738867
142.526860	5076.028912	24.743885
142.623217	5091.007668	24.748903
142.896265	5106.280728	24.753920
143.178410	5109.573104	24.758938
143.289256	5121.067894	24.763955
143.465670	5121.390697	24.768973
143.568044	5125.838144	24.773991
143.842894	5132.367177	24.779008
143.613084	5158.524093	24.784026
143.724633	5159.832449	24.789043
144.156161	5159.127270	24.794061
143.726224	5176.805371	24.799079
144.261530	5181.693220	24.804096
144.714007	5189.649640	24.809114
145.019608	5199.803977	24.814131
145.104314	5195.030602	24.819149
145.224471	5205.472837	24.824167
145.620619	5203.769397	24.829184
145.307516	5215.920951	24.834202
145.689043	5216.896607	24.839219
146.009462	5226.982349	24.844237
145.894838	5239.554220	24.849255
145.885488	5221.954468	24.854272
146.203341	5245.311023	24.859290
146.505757	5240.418300	24.864307
146.606958	5243.786397	24.869325
146.622535	5246.596561	24.874343
146.961127	5262.326663	24.879360
146.991278	5279.048930	24.884378
147.284797	5284.669142	24.889395
147.467367	5279.968799	24.894413
147.077490	5287.564796	24.899431
147.348274	5294.097681	24.904448
147.654965	5303.579544	24.909466
147.709461	5307.172777	24.914483
147.949631	5310.667476	24.919501
147.998852	5327.165835	24.924519
148.023088	5326.584435	24.929536
148.202154	5337.891903	24.934554
148.298803	5346.295560	24.939571
148.588286	5353.993492	24.944589
148.307814	5360.641172	24.949607
148.726555	5385.102707	24.954624
148.725848	5397.558983	24.959642
148.538366	5408.886040	24.964659
148.852985	5414.941761	24.969677
149.084592	5437.279851	24.974695
149.168150	5451.515940	24.979712
149.061512	5463.108151	24.984730
149.224323	5478.007367	24.989747
150.011029	5493.411776	24.994765
150.237667	5509.409007	24.999783
150.002487	5512.230086	25.004800
150.479152	5509.967903	25.009818
150.732802	5521.001797	25.014835
151.142947	5522.389667	25.019853
151.165057	5534.201659	25.024871
151.564951	5538.312182	25.029888
151.556881	5544.715227	25.034906
151.738295	5536.766788	25.039923
152.252555	5531.518820	25.044941
152.015195	5534.624344	25.049959
152.061806	5537.922131	25.054976
152.494230	5551.743783	25.059994
152.760560	5555.417518	25.065011
152.690074	5554.472149	25.070029
152.557423	5561.958515	25.075047
152.679759	5565.910501	25.080064
153.017297	5556.990593	25.085082
153.065639	5564.110841	25.090099
153.348555	5562.677642	25.095117
153.420366	5587.986125	25.100135
153.327443	5590.567120	25.105152
153.779667	5592.646028	25.110170
153.342731	5593.216451	25.115187
153.837495	5598.906247	25.120205
153.617100	5617.994547	25.125223
153.938256	5634.772563	25.130240
154.216820	5641.616866	25.135258
154.438874	5648.154356	25.140275
154.718824	5652.441531	25.145293
154.702825	5666.775458	25.150311
154.847501	5674.038491	25.155328
154.921042	5675.750582	25.160346
155.051911	5697.344010	25.165363
155.277830	5695.509361	25.170381
155.604883	5713.568144	25.175399
155.658818	5719.143951	25.180416
155.968223	5730.295505	25.185434
155.644134	5738.462214	25.190451
155.902659	5738.046125	25.195469
156.573740	5754.239105	25.200487
156.182686	5765.866595	25.205504
156.246143	5775.964487	25.210522
156.437986	5783.157040	25.215539
156.714042	5797.382181	25.220557
156.855473	5811.779946	25.225575
157.326547	5822.663162	25.230592
157.546864	5834.823102	25.235610
157.429459	5832.379315	25.240627
158.238349	5836.047026	25.245645
157.911355	5851.945044	25.250663
157.970561	5855.764931	25.255680
158.041997	5859.974336	25.260698
158.486121	5880.202551	25.265715
158.665989	5884.997909	25.270733
158.683652	5890.923535	25.275751
158.749487	5914.048949	25.280768
159.008028	5921.748812	25.285786
159.306923	5914.725668	25.290803
159.339286	5927.669574	25.295821
159.730848	5941.624193	25.300839
159.829910	5941.574010	25.305856
160.017476	5936.118256	25.310874
159.988649	5958.753480	25.315891
160.223688	5960.759128	25.320909
160.512216	5967.403117	25.325927
160.365976	5977.205672	25.330944
161.027340	5984.586758	25.335962
160.923147	5997.703630	25.340979
160.985891	5998.306269	25.345997
161.544467	5998.954342	25.351015
161.292618	6006.377487	25.356032
161.595547	6007.147687	25.361050
161.388510	6016.855615	25.366067
162.397444	6032.452953	25.371085
162.272952	6039.890884	25.376103
162.240007	6043.125463	25.381120
162.624642	6038.595302	25.386138
162.675962	6043.622344	25.391155
163.071984	6061.096136	25.396173
163.378450	6067.437461	25.401191
163.325040	6059.326708	25.406208
163.426855	6062.985282	25.411226
163.445327	6061.937561	25.416243
163.524935	6071.445930	25.421261
163.562283	6062.639098	25.426279
163.851431	6070.624650	25.431296
164.084179	6074.436336	25.436314
163.959026	6085.978176	25.441331
164.099039	6078.585265	25.446349
164.519174	6095.616524	25.451367
164.425163	6116.645892	25.456384
164.757712	6117.316754	25.461402
164.639409	6121.158191	25.466419
165.258307	6131.658563	25.471437
165.124026	6138.103685	25.476455
165.207499	6158.309790	25.481472
165.627729	6154.159151	25.486490
165.448495	6167.167943	25.491507
165.367990	6173.825627	25.496525
166.123112	6189.330279	25.501543
166.028912	6191.883146	25.506560
166.338083	6200.108691	25.511578
166.413124	6214.469822	25.516595
166.486233	6217.697288	25.521613
166.298687	6230.189714	25.526631
166.642938	6241.528686	25.531648
166.671809	6244.106475	25.536666
166.910589	6276.994457	25.541683
167.174702	6283.213063	25.546701
167.234268	6292.532122	25.551719
167.034795	6308.738863	25.556736
167.402696	6328.054574	25.561754
167.778905	6347.466864	25.566771
168.319510	6357.960691	25.571789
168.653526	6368.351146	25.576807
168.319441	6376.971127	25.581824
168.705027	6387.489256	25.586842
168.960022	6391.168094	25.591859
169.161875	6402.576826	25.596877
169.307835	6417.147983	25.601895
169.317005	6421.420937	25.606912
170.105595	6434.938074	25.611930
170.092557	6440.991802	25.616947
170.147840	6438.094709	25.621965
170.347997	6450.542331	25.626983
170.737384	6473.390472	25.632000
170.984900	6465.036674	25.637018
171.253294	6468.918622	25.642035
170.806567	6469.282251	25.647053
171.100750	6479.647441	25.652071
171.040956	6489.228375	25.657088
171.564195	6489.263266	25.662106
171.598282	6509.906824	25.667123
171.857876	6524.962200	25.672141
172.017067	6521.003903	25.677159
172.016787	6536.677703	25.682176
172.217578	6548.288730	25.687194
172.198433	6548.130790	25.692212
172.470176	6567.600718	25.697229
172.637656	6571.274361	25.702247
172.752223	6586.289372	25.707264
172.945278	6596.449492	25.712282
173.205011	6611.444937	25.717300
173.209707	6626.593997	25.722317
173.696295	6630.312365	25.727335
173.771117	6644.045653	25.732352
174.044172	6659.825109	25.737370
174.035877	6667.747030	25.742388
173.969926	6661.358465	25.747405
174.440974	6680.519487	25.752423
174.694676	6700.083932	25.757440
174.584537	6697.010673	25.762458
175.063313	6712.290730	25.767476
175.228521	6726.511861	25.772493
175.278602	6722.024475	25.777511
175.291579	6737.109191	25.782528
175.584605	6740.804239	25.787546
175.647508	6755.881149	25.792564
175.847860	6764.521762	25.797581
176.340644	6778.786321	25.802599
176.141784	6795.889949	25.807616
176.214124	6792.308241	25.812634
176.930758	6803.885971	25.817652
176.955731	6822.832905	25.822669
176.780913	6823.990517	25.827687
177.232098	6834.255547	25.832704
177.311431	6840.897902	25.837722
177.663140	6850.645011	25.842740
178.311568	6860.449818	25.847757
177.973040	6879.636856	25.852775
178.041776	6882.833555	25.857792
178.560484	6885.757720	25.862810
178.895362	6906.673448	25.867828
178.556925	6908.750101	25.872845
179.172793	6907.832884	25.877863
178.697729	6925.194571	25.882880
179.561243	6932.067683	25.887898
179.512869	6937.871402	25.892916
180.061475	6956.427063	25.897933
179.716287	6960.430495	25.902951
179.741700	6968.000005	25.907968
180.225597	6974.348575	25.912986
180.525762	6985.420263	25.918004
180.315136	6997.124439	25.923021
180.839532	7012.467052	25.928039
180.926512	7018.173825	25.933056
181.187267	7019.578904	25.938074
181.243356	7034.360359	25.943092
181.122451	7037.814093	25.948109
181.725294	7056.105647	25.953127
181.579243	7063.357953	25.958144
181.863926	7081.828810	25.963162
181.720208	7091.912529	25.968180
182.086114	7110.348592	25.973197
182.041926	7115.921255	25.978215
182.446059	7130.540926	25.983232
182.986275	7150.465053	25.988250
182.809328	7147.942023	25.993268
183.000207	7166.329795	25.998285
183.452962	7168.986528	26.003303
183.506485	7183.759034	26.008320
184.409302	7196.703218	26.013338
184.479758	7199.893389	26.018356
184.442644	7209.316453	26.023373
184.850260	7202.408381	26.028391
185.235781	7200.911632	26.033408
185.174197	7217.492189	26.038426
185.353315	7221.909181	26.043444
185.308885	7222.181386	26.048461
185.553665	7228.548563	26.053479
185.421686	7237.434036	26.058496
185.941829	7261.310784	26.063514
186.054100	7259.080224	26.068532
185.710808	7264.841852	26.073549
186.176906	7272.749698	26.078567
186.113401	7285.030832	26.083584
186.738836	7292.667481	26.088602
186.897805	7307.174166	26.093620
186.809478	7308.245648	26.098637
187.015757	7313.842271	26.103655
186.911460	7342.568192	26.108672
187.464534	7346.443614	26.113690
187.682952	7351.545859	26.118708
187.364377	7369.792657	26.123725
187.728161	7372.567538	26.128743
187.752121	7399.328754	26.133760
188.023771	7407.459696	26.138778
188.324268	7418.749426	26.143796
188.955238	7431.616399	26.148813
189.124685	7454.954824	26.153831
189.384237	7460.502106	26.158848
189.392321	7465.877265	26.163866
189.491078	7475.465443	26.168884
189.629675	7483.582536	26.173901
190.356137	7476.034053	26.178919
190.126353	7493.247352	26.183936
190.307528	7514.131024	26.188954
190.695480	7503.936321	26.193972
190.435094	7524.930221	26.198989
190.777752	7535.256845	26.204007
190.830459	7547.595715	26.209024
191.191873	7564.122945	26.214042
191.278747	7574.338125	26.219060
191.081393	7590.542503	26.224077
191.591558	7600.981830	26.229095
191.822547	7620.806531	26.234112
191.996036	7631.566967	26.239130
192.369250	7639.284316	26.244148
192.389886	7647.839845	26.249165
192.959602	7669.246875	26.254183
192.939218	7684.634353	26.259200
192.892051	7692.518605	26.264218
193.766869	7696.409996	26.269236
193.841198	7700.218426	26.274253
194.239512	7709.810310	26.279271
194.324278	7715.246141	26.284288
194.508412	7724.862115	26.289306
194.875996	7724.564654	26.294324
194.716695	7727.655157	26.299341
195.251696	7740.938327	26.304359
195.495988	7742.522837	26.309376
195.857179	7737.872813	26.314394
195.821238	7736.801951	26.319412
195.807252	7751.819108	26.324429
196.078351	7766.861072	26.329447
196.020601	7779.409982	26.334464
196.177888	7783.154921	26.339482
196.736890	7793.870843	26.344500
196.769987	7794.648667	26.349517
196.783932	7803.947225	26.354535
196.962900	7824.114942	26.359552
196.990751	7826.813081	26.364570
197.409097	7839.211677	26.369588
197.297962	7868.533014	26.374605
197.673164	7856.010201	26.379623
198.858144	7863.392109	26.384640
198.766125	7870.336344	26.389658
198.938616	7868.535110	26.394676
198.530493	7866.774321	26.399693
198.626609	7875.011896	26.404711
199.093371	7884.226929	26.409728
199.385670	7891.161478	26.414746
199.386937	7908.029574	26.419764
199.511464	7924.587924	26.424781
199.722154	7920.529706	26.429799
200.110052	7925.053072	26.434816
200.073201	7934.372281	26.439834
200.415178	7946.309352	26.444852
200.826555	7948.019245	26.449869
200.882020	7957.204035	26.454887
200.948762	7962.049231	26.459904
201.037400	7985.460971	26.464922
201.152497	7984.666357	26.469940
201.303478	8008.317769	26.474957
201.335766	8015.858218	26.479975
201.624065	8025.442245	26.484992
201.472024	8048.714972	26.490010
201.913133	8060.822856	26.495028
201.828567	8080.072379	26.500045
202.176583	8096.223334	26.505063
202.411943	8113.332769	26.510080
202.528696	8141.586464	26.515098
202.909909	8147.061223	26.520116
202.910225	8171.402598	26.525133
203.159874	8188.648777	26.530151
203.491170	8204.603547	26.535168
203.398079	8228.044063	26.540186
204.215018	8243.218747	26.545204
203.986836	8265.982748	26.550221
204.201672	8282.786156	26.555239
204.383681	8292.816344	26.560256
204.583662	8314.259945	26.565274
204.850149	8333.407379	26.570292
204.816990	8354.413978	26.575309
205.131705	8370.106287	26.580327
205.205480	8383.174874	26.585344
205.346719	8406.389477	26.590362
206.318729	8425.584338	26.595380
206.142737	8447.465852	26.600397
206.247515	8455.317154	26.605415
206.693860	8474.543901	26.610432
206.934620	8491.365538	26.615450
207.544551	8499.289267	26.620468
207.675763	8509.346473	26.625485
207.658976	8524.822486	26.630503
208.154587	8537.885085	26.635520
208.076156	8545.073704	26.640538
208.599288	8561.383906	26.645556
208.846851	8567.176503	26.650573
208.807348	8578.583351	26.655591
209.027782	8593.416079	26.660608
208.695334	8610.839086	26.665626
209.650724	8623.236166	26.670644
209.549217	8636.502879	26.675661
209.548767	8667.093118	26.680679
210.170520	8668.318643	26.685696
210.265226	8696.532436	26.690714
210.688670	8690.650585	26.695732
210.896242	8706.997721	26.700749
211.183545	8727.389399	26.705767
211.442502	8727.544639	26.710784
210.828342	8749.501464	26.715802
211.347333	8758.680338	26.720820
211.228098	8772.470866	26.725837
211.662360	8777.744913	26.730855
212.503601	8795.817733	26.735872
212.712983	8809.619953	26.740890
212.782732	8820.245786	26.745908
213.082784	8826.718518	26.750925
213.146006	8832.398002	26.755943
214.164560	8832.734184	26.760960
214.097218	8847.956336	26.765978
213.895527	8839.573967	26.770996
214.277730	8852.544052	26.776013
214.670592	8855.554556	26.781031
214.856116	8860.289820	26.786048
214.674293	8870.030021	26.791066
214.934037	8865.190390	26.796084
215.093718	8883.894169	26.801101
215.131744	8889.394498	26.806119
215.485043	8895.028558	26.811136
215.145965	8919.474598	26.816154
215.638718	8926.078197	26.821172
215.776299	8940.336934	26.826189
215.740260	8958.528402	26.831207
215.932275	8967.427091	26.836224
216.014038	8989.815069	26.841242
216.623499	9009.452521	26.846260
216.888684	9035.524758	26.851277
216.907849	9049.173834	26.856295
217.473965	9057.142556	26.861312
217.209357	9088.008507	26.866330
217.777141	9096.071703	26.871348
218.065213	9109.160904	26.876365
218.259916	9137.119748	26.881383
218.506620	9137.153777	26.886400
218.716154	9159.452483	26.891418
218.964846	9178.227860	26.896436
219.156975	9189.475661	26.901453
219.346677	9198.936823	26.906471
219.656872	9217.718391	26.911488
219.610938	9239.839360	26.916506
220.041061	9254.071454	26.921524
220.211837	9264.953242	26.926541
220.362949	9283.447226	26.931559
220.896706	9295.506676	26.936576
220.962562	9316.925087	26.941594
221.505923	9324.780670	26.946612
221.689149	9346.553292	26.951629
221.662491	9356.054742	26.956647
222.100021	9371.769706	26.961664
221.796031	9382.808028	26.966682
222.245683	9402.139412	26.971700
222.345977	9418.333484	26.976717
222.600445	9437.139792	26.981735
222.873276	9449.435972	26.986752
222.945229	9470.878864	26.991770
223.342126	9485.785697	26.996788
223.266660	9503.535530	27.001805
223.371554	9526.817215	27.006823
223.827283	9538.289151	27.011840
224.026235	9566.977323	27.016858
224.434892	9585.800671	27.021876
224.493255	9600.991116	27.026893
224.689546	9619.358376	27.031911
225.195992	9632.915758	27.036928
225.222823	9650.949656	27.041946
225.672499	9663.821332	27.046964
225.837816	9671.701554	27.051981
225.909069	9690.903074	27.056999
226.709295	9702.191692	27.062016
226.929145	9722.307707	27.067034
227.527008	9729.637114	27.072052
227.806956	9727.499973	27.077069
227.604764	9737.663749	27.082087
228.213862	9745.673397	27.087104
228.268013	9754.287795	27.092122
228.449290	9744.184238	27.097140
228.931090	9760.116770	27.102157
228.906558	9779.936449	27.107175
229.275448	9777.586454	27.112192
229.046168	9787.059874	27.117210
229.197593	9789.296905	27.122228
229.442243	9791.538277	27.127245
229.626803	9807.015388	27.132263
230.206200	9817.217795	27.137280
229.964756	9828.726506	27.142298
230.423816	9837.211206	27.147316
230.480778	9855.209007	27.152333
230.291960	9867.552525	27.157351
230.938634	9878.650602	27.162368
231.315751	9890.289784	27.167386
231.640903	9904.485145	27.172404
231.647051	9913.309210	27.177421
231.778085	9930.828184	27.182439
232.394462	9951.737989	27.187456
232.247379	9960.977602	27.192474
232.536731	9977.767713	27.197492
232.586286	9980.576432	27.202509
232.532559	10002.418515	27.207527
232.674443	10025.028810	27.212544
233.016166	10050.452677	27.217562
233.378232	10071.411928	27.222580
234.256230	10079.385912	27.227597
233.913456	10111.803473	27.232615
234.302607	10110.315405	27.237632
234.417905	10131.019738	27.242650
234.813912	10149.469902	27.247668
235.346173	10160.958651	27.252685
235.580490	10189.667500	27.257703
235.595279	10192.570107	27.262720
236.101120	10202.250638	27.267738
236.349479	10207.806815	27.272756
236.862305	10223.883286	27.277773
236.717661	10249.670945	27.282791
237.086859	10251.236108	27.287808
237.201599	10268.988447	27.292826
237.304855	10278.631045	27.297844
237.831385	10296.236806	27.302861
237.494955	10320.668475	27.307879
237.958970	10321.637814	27.312896
238.119854	10337.548491	27.317914
238.189891	10359.406335	27.322932
238.561268	10378.694161	27.327949
238.657916	10403.484355	27.332967
238.884362	10420.297349	27.337984
239.114086	10442.556536	27.343002
239.276039	10463.617041	27.348020
239.785605	10478.942756	27.353037
239.835367	10491.628211	27.358055
240.716398	10502.598381	27.363072
240.654403	10524.041363	27.368090
240.812059	10541.269404	27.373108
241.379272	10550.829990	27.378125
241.485613	10574.883190	27.383143
241.621605	10576.071279	27.388160
241.629844	10594.645779	27.393178
241.796913	10612.765991	27.398196
242.243914	10631.495979	27.403213
242.292350	10648.978044	27.408231
242.828530	10659.958125	27.413248
242.942798	10682.090437	27.418266
243.095582	10696.206046	27.423284
243.740490	10717.996355	27.428301
244.103346	10733.774689	27.433319
243.947054	10741.696271	27.438336
244.137615	10756.560663	27.443354
244.379500	10769.727734	27.448372
244.695495	10773.350532	27.453389
244.811880	10803.038695	27.458407
245.012020	10810.964464	27.463424
245.358214	10828.564245	27.468442
246.023297	10842.384997	27.473460
246.336529	10859.039542	27.478477
246.032957	10872.595259	27.483495
246.264645	10886.442888	27.488512
246.435690	10901.550428	27.493530
246.617675	10924.357613	27.498548
246.760696	10930.997771	27.503565
246.929994	10956.029922	27.508583
247.221778	10980.862936	27.513600
247.557184	10994.110241	27.518618
247.914631	11024.793526	27.523636
248.454479	11034.898597	27.528653
248.359079	11059.062962	27.533671
248.445955	11071.686158	27.538688
248.712654	11098.465186	27.543706
248.838982	11120.062489	27.548724
249.367313	11130.703054	27.553741
249.107277	11159.629767	27.558759
249.657268	11181.394436	27.563776
249.922102	11197.119048	27.568794
250.033815	11224.800357	27.573812
250.598569	11240.190677	27.578829
250.889179	11266.738849	27.583847
251.701437	11279.466430	27.588864
252.304631	11279.075179	27.593882
252.579661	11302.922902	27.598900
253.223888	11308.351084	27.603917
252.974618	11310.591073	27.608935
253.150437	11325.379284	27.613952
253.767133	11331.645406	27.618970
253.667840	11339.368851	27.623988
254.011729	11336.318427	27.629005
254.107038	11359.300758	27.634023
254.258627	11371.538258	27.639040
254.764469	11388.819894	27.644058
254.685276	11395.138211	27.649076
255.097818	11407.183287	27.654093
254.973169	11422.748065	27.659111
255.161162	11444.702371	27.664128
255.351480	11465.004874	27.669146
255.497192	11488.784675	27.674164
255.685889	11501.827969	27.679181
256.124707	11514.270024	27.684199
256.310787	11541.551754	27.689216
256.450311	11561.631807	27.694234
256.937617	11586.416047	27.699252
256.943705	11600.293228	27.704269
257.354861	11623.264297	27.709287
257.428858	11642.577906	27.714304
258.103877	11663.619382	27.719322
258.066494	11678.485478	27.724340
258.509547	11697.899217	27.729357
258.435011	11725.338875	27.734375
258.692839	11738.595702	27.739392
258.967544	11757.110662	27.744410
259.075684	11784.875455	27.749428
259.536522	11801.090894	27.754445
259.361628	11835.474496	27.759463
259.934828	11851.606065	27.764480
260.540560	11867.839914	27.769498
260.669883	11895.039473	27.774516
261.160057	11922.684626	27.779533
261.342941	11933.862900	27.784551
261.671230	11938.459746	27.789568
261.740934	11962.075217	27.794586
261.883129	11982.824745	27.799604
262.408233	11991.846375	27.804621
262.456737	12015.421026	27.809639
262.799090	12039.909636	27.814656
263.252174	12056.432814	27.819674
263.944229	12064.023117	27.824692
264.262685	12071.788785	27.829709
264.407378	12084.116245	27.834727
264.537103	12093.370381	27.839744
264.855558	12099.854002	27.844762
264.630377	12123.124304	27.849780
264.993320	12133.235579	27.854797
265.360471	12149.721776	27.859815
265.366209	12171.588641	27.864832
265.731514	12181.478526	27.869850
265.888318	12206.027997	27.874868
266.268342	12222.922755	27.879885
266.588834	12243.988841	27.884903
266.354816	12269.281702	27.889920
267.394001	12279.937631	27.894938
268.044634	12292.590172	27.899956
268.304253	12313.223778	27.904973
268.626060	12316.233351	27.909991
268.527664	12323.432860	27.915008
268.986810	12343.507886	27.920026
268.938412	12356.178397	27.925044
269.359500	12362.339723	27.930061
269.755000	12377.021718	27.935079
269.815074	12404.899162	27.940096
270.109069	12414.020356	27.945114
270.556754	12437.517212	27.950132
270.420742	12445.995269	27.955149
270.512210	12456.742918	27.960167
271.056448	12493.781335	27.965184
271.170593	12513.411647	27.970202
271.153218	12536.059385	27.975220
271.839817	12545.829659	27.980237
271.782025	12579.214177	27.985255
271.557782	12589.446100	27.990272
271.980289	12616.790244	27.995290
272.370055	12649.596359	28.000308
272.960902	12669.313209	28.005325
272.743716	12702.940807	28.010343
273.148906	12722.052062	28.015360
273.610454	12742.919767	28.020378
273.709215	12773.813792	28.025396
274.412100	12787.042692	28.030413
274.619070	12822.530375	28.035431
275.051141	12836.120681	28.040448
275.652866	12848.888628	28.045466
275.818620	12873.775459	28.050484
276.197862	12883.701426	28.055501
276.242106	12897.583056	28.060519
276.671806	12917.423305	28.065536
277.076303	12928.289556	28.070554
277.140247	12949.503987	28.075572
277.606012	12975.676599	28.080589
277.921340	12980.528367	28.085607
278.076883	13009.335965	28.090624
278.267497	13017.090471	28.095642
278.256934	13037.476661	28.100660
278.537064	13050.986711	28.105677
279.220517	13076.534828	28.110695
278.975245	13097.295749	28.115712
279.426122	13117.881325	28.120730
279.633604	13143.996734	28.125748
279.809215	13152.391553	28.130765
279.945911	13172.805347	28.135783
280.149467	13203.342597	28.140800
280.547071	13215.792234	28.145818
280.655160	13242.400201	28.150836
280.703126	13269.207103	28.155853
281.308066	13291.445619	28.160871
281.484091	13323.455835	28.165888
282.245225	13330.432658	28.170906
282.596510	13354.495245	28.175924
282.902442	13369.580476	28.180941
283.047602	13378.217014	28.185959
283.163942	13414.051591	28.190976
283.998078	13422.959183	28.195994
284.163296	13446.359431	28.201012
284.105820	13449.952831	28.206029
284.779944	13461.614024	28.211047
285.232106	13492.093848	28.216064
285.897797	13497.475097	28.221082
285.814250	13524.482967	28.226100
286.198290	13533.426380	28.231117
286.371383	13545.156637	28.236135
286.101913	13563.487022	28.241152
286.829133	13578.089566	28.246170
287.121473	13589.930650	28.251188
287.349644	13618.203563	28.256205
287.793954	13628.596592	28.261223
287.640169	13648.156361	28.266240
288.088370	13675.422215	28.271258
288.179017	13690.831966	28.276276
288.439415	13712.752300	28.281293
288.712582	13736.360217	28.286311
289.065632	13757.988181	28.291328
289.340223	13786.683569	28.296346
289.549528	13810.247895	28.301364
289.578601	13835.397411	28.306381
290.040705	13862.951900	28.311399
289.779309	13891.279801	28.316416
290.224875	13916.323127	28.321434
290.136021	13946.436822	28.326452
290.853877	13975.941007	28.331469
291.561290	13998.893822	28.336487
291.473331	14030.861313	28.341504
291.970617	14051.949088	28.346522
292.595212	14077.397242	28.351540
292.456501	14106.034688	28.356557
292.840368	14132.717551	28.361575
292.961353	14159.062656	28.366592
293.390992	14184.674134	28.371610
293.636979	14216.564360	28.376628
294.127406	14245.807726	28.381645
294.906845	14257.440282	28.386663
294.861439	14287.696142	28.391680
295.256801	14302.761789	28.396698
295.675932	14324.961145	28.401716
295.885907	14349.129240	28.406733
296.290330	14369.016023	28.411751
296.507649	14393.719911	28.416768
296.480157	14420.091794	28.421786
297.060408	14442.070241	28.426804
297.398989	14469.085961	28.431821
297.917317	14480.064757	28.436839
298.035317	14508.526791	28.441856
299.189779	14519.450178	28.446874
299.321011	14534.099447	28.451892
299.410568	14533.905461	28.456909
300.127810	14539.837935	28.461927
299.992868	14554.923689	28.466944
300.397759	14558.242745	28.471962
300.683326	14579.383219	28.476980
300.890992	14582.881609	28.481997
301.349575	14591.807529	28.487015
301.121077	14620.772472	28.492032
301.380516	14633.497340	28.497050
302.143235	14635.964491	28.502068
301.925711	14663.345519	28.507085
302.057867	14674.864969	28.512103
302.078884	14692.121356	28.517120
302.617245	14717.943912	28.522138
303.049255	14735.000154	28.527156
302.640553	14766.539070	28.532173
303.328616	14795.477556	28.537191
303.734980	14822.022057	28.542208
303.589622	14847.857143	28.547226
304.129722	14870.856170	28.552244
304.083640	14902.461678	28.557261
304.475004	14926.848433	28.562279
305.108355	14965.314716	28.567296
305.155135	14997.938585	28.572314
305.471261	15021.866666	28.577332
305.602980	15052.061249	28.582349
306.474959	15080.030192	28.587367
306.522898	15110.765422	28.592384
306.682238	15133.745453	28.597402
306.910902	15162.153225	28.602420
307.305952	15192.474168	28.607437
308.255916	15213.928165	28.612455
308.444283	15247.465136	28.617472
308.487415	15277.525510	28.622490
308.919494	15292.112442	28.627508
309.282879	15319.520268	28.632525
309.695867	15346.778239	28.637543
309.896193	15366.262185	28.642560
310.694445	15386.925295	28.647578
310.789792	15409.467198	28.652596
311.099663	15444.210912	28.657613
311.667626	15467.272617	28.662631
311.666058	15493.038673	28.667648
311.921033	15506.573358	28.672666
312.179819	15539.288114	28.677684
311.960051	15564.061981	28.682701
312.474095	15586.260569	28.687719
312.795432	15624.236973	28.692736
313.227402	15646.350579	28.697754
313.774722	15668.900947	28.702772
314.166703	15700.243329	28.707789
314.445402	15722.943223	28.712807
314.999165	15750.839819	28.717824
314.789605	15772.343425	28.722842
315.132614	15800.001485	28.727860
315.493606	15825.786995	28.732877
315.610079	15857.112780	28.737895
316.164507	15888.189984	28.742912
316.045069	15915.342660	28.747930
316.548129	15942.593686	28.752948
316.747484	15973.470816	28.757965
317.255659	16002.287703	28.762983
317.823468	16039.847309	28.768000
318.084472	16059.995201	28.773018
318.659348	16086.856169	28.778036
318.527743	16120.757472	28.783053
319.165133	16142.021434	28.788071
319.197574	16175.672886	28.793088
319.608591	16192.124135	28.798106
320.045518	16216.363264	28.803124
320.213231	16253.066846	28.808141
320.755825	16269.459648	28.813159
320.691217	16291.797074	28.818176
320.957453	16314.569105	28.823194
321.908875	16335.389281	28.828212
321.923824	16371.649563	28.833229
322.419398	16385.602002	28.838247
322.360726	16409.359954	28.843264
322.331390	16448.207808	28.848282
323.040327	16464.063043	28.853300
323.086526	16506.651483	28.858317
323.390125	16535.542275	28.863335
323.890895	16566.556336	28.868352
323.721808	16593.291343	28.873370
324.072907	16607.591902	28.878388
324.319238	16657.319182	28.883405
324.677899	16686.517429	28.888423
325.434779	16723.578130	28.893440
325.589188	16767.173563	28.898458
326.063146	16800.576907	28.903476
326.394429	16837.578153	28.908493
326.542320	16864.620800	28.913511
327.025340	16896.200396	28.918528
327.406222	16938.004572	28.923546
327.627784	16966.946764	28.928564
327.688346	17001.397531	28.933581
328.492696	17033.388172	28.938599
328.550645	17059.772400	28.943616
328.912675	17107.979222	28.948634
329.189675	17134.550342	28.953652
329.336300	17167.775017	28.958669
330.076608	17195.132790	28.963687
330.329031	17224.544326	28.968704
330.887866	17254.830230	28.973722
331.629545	17279.029276	28.978740
332.174414	17307.017963	28.983757
332.311568	17336.889936	28.988775
332.712673	17350.921047	28.993792
333.128901	17383.168901	28.998810
333.515394	17396.835930	29.003828
333.890660	17434.460000	29.008845
334.308417	17440.282367	29.013863
334.084109	17465.081491	29.018880
334.506109	17493.083377	29.023898
335.162420	17519.715639	29.028916
335.363708	17546.981459	29.033933
336.050960	17573.495237	29.038951
336.125475	17592.056695	29.043968
336.408791	17621.242887	29.048986
337.040761	17641.460669	29.054004
337.091900	17667.530922	29.059021
337.638516	17688.412816	29.064039
338.127685	17706.252421	29.069056
338.296726	17722.967149	29.074074
338.416104	17747.870734	29.079092
338.647109	17773.180133	29.084109
338.843288	17801.666376	29.089127
339.558377	17833.217469	29.094144
339.601916	17867.843014	29.099162
339.959431	17882.879498	29.104180
340.013988	17904.261973	29.109197
340.529341	17942.225182	29.114215
340.912541	17971.301492	29.119232
341.106807	18004.690712	29.124250
341.185349	18025.279873	29.129268
341.642305	18065.318298	29.134285
342.239339	18096.900948	29.139303
342.776247	18125.864968	29.144320
342.922870	18155.471381	29.149338
343.499365	18166.594804	29.154356
343.542799	18195.427747	29.159373
344.015578	18211.981601	29.164391
344.419386	18228.375699	29.169408
344.669348	18267.467739	29.174426
345.175732	18286.297045	29.179444
345.366549	18312.226249	29.184461
345.726257	18339.196709	29.189479
346.059615	18359.253536	29.194496
346.122889	18391.084532	29.199514
346.539846	18428.154365	29.204532
346.651854	18454.727868	29.209549
347.197387	18483.621576	29.214567
347.289642	18511.531278	29.219584
347.494954	18555.438640	29.224602
347.988796	18578.566221	29.229620
348.045810	18620.772229	29.234637
348.475182	18654.896497	29.239655
348.931410	18689.136655	29.244672
349.291785	18722.077798	29.249690
349.813295	18757.002801	29.254708
349.850286	18790.575948	29.259725
350.487185	18828.048015	29.264743
350.933073	18843.305159	29.269760
351.341323	18880.225590	29.274778
351.879639	18915.432545	29.279796
352.328534	18940.551388	29.284813
352.858601	18979.822105	29.289831
353.207660	19011.179735	29.294848
353.398860	19037.646860	29.299866
353.860358	19062.441676	29.304884
354.075413	19092.455771	29.309901
354.401079	19121.921885	29.314919
355.102807	19149.218966	29.319936
355.461902	19181.958914	29.324954
355.563031	19200.492465	29.329972
355.669805	19225.109290	29.334989
356.371276	19251.642088	29.340007
356.832277	19277.662930	29.345024
356.906392	19316.342363	29.350042
357.340993	19347.554458	29.355060
357.218338	19376.592064	29.360077
357.887956	19410.869561	29.365095
358.199163	19444.817864	29.370112
358.507260	19488.635408	29.375130
359.096456	19507.907820	29.380148
359.846489	19526.131542	29.385165
360.559850	19553.793811	29.390183
361.083598	19569.292049	29.395200
361.228396	19596.575905	29.400218
361.553009	19625.171057	29.405236
362.155310	19644.416279	29.410253
362.281612	19657.436991	29.415271
363.301884	19681.450083	29.420288
363.572658	19688.193317	29.425306
363.968669	19701.178129	29.430324
364.039529	19713.348307	29.435341
364.192830	19738.640841	29.440359
364.551235	19748.560994	29.445376
364.765591	19772.062310	29.450394
365.185583	19793.926651	29.455412
365.806266	19819.967430	29.460429
365.772284	19835.502697	29.465447
366.354069	19861.492762	29.470464
366.165355	19885.164759	29.475482
366.839304	19903.337571	29.480500
367.119506	19934.985467	29.485517
367.159077	19958.261660	29.490535
367.690936	19983.526803	29.495552
368.046569	20016.590916	29.500570
368.466172	20039.460179	29.505588
368.301390	20055.584744	29.510605
368.692791	20090.248194	29.515623
369.093755	20113.082553	29.520640
368.999248	20152.295504	29.525658
369.392428	20202.280520	29.530676
369.890175	20229.080332	29.535693
370.110862	20263.309598	29.540711
370.301825	20295.862925	29.545728
370.605355	20339.632541	29.550746
370.827020	20382.631612	29.555764
371.227264	20423.214491	29.560781
371.379324	20462.155660	29.565799
372.065845	20500.261310	29.570816
372.362924	20556.296269	29.575834
372.730947	20600.416509	29.580852
373.207114	20639.724272	29.585869
373.794675	20677.157065	29.590887
374.481832	20713.797168	29.595904
374.852642	20751.921166	29.600922
375.300846	20782.823815	29.605940
375.656657	20812.129788	29.610957
375.883868	20856.917137	29.615975
376.608679	20886.039053	29.620992
376.687820	20925.839232	29.626010
377.496452	20967.705094	29.631028
377.601947	20997.050552	29.636045
377.707302	21039.974499	29.641063
378.541995	21071.550007	29.646080
378.964191	21104.295917	29.651098
379.266507	21149.021616	29.656116
379.761005	21177.440773	29.661133
379.788183	21210.709986	29.666151
380.236207	21244.140804	29.671168
380.763121	21285.160553	29.676186
381.044604	21314.504191	29.681204
381.522178	21341.605653	29.686221
381.919945	21387.618570	29.691239
382.130912	21413.005320	29.696256
382.407592	21460.111536	29.701274
382.833278	21501.551983	29.706292
382.914692	21546.679665	29.711309
383.170386	21597.151016	29.716327
383.832555	21625.494005	29.721344
384.426999	21670.036115	29.726362
384.707125	21719.909995	29.731380
385.368034	21756.145432	29.736397
385.422805	21789.784101	29.741415
386.002611	21830.367024	29.746432
386.122598	21861.840910	29.751450
386.704249	21896.376638	29.756468
387.269513	21925.297606	29.761485
387.643000	21977.640788	29.766503
388.328389	22014.056108	29.771520
388.497109	22053.812930	29.776538
388.310913	22095.356782	29.781556
388.601488	22138.930214	29.786573
389.076901	22177.899941	29.791591
389.551316	22226.588314	29.796608
389.924628	22266.206094	29.801626
390.011456	22321.533363	29.806644
390.890941	22366.594774	29.811661
390.807936	22416.464095	29.816679
391.552790	22447.872629	29.821696
391.617933	22493.377830	29.826714
392.231488	22535.568243	29.831732
392.833483	22571.713297	29.836749
392.832246	22620.635115	29.841767
393.278206	22657.183904	29.846784
393.783569	22698.481674	29.851802
394.226089	22737.413419	29.856820
394.778758	22767.544524	29.861837
395.321215	22812.097343	29.866855
395.903938	22844.549268	29.871872
396.174704	22891.299621	29.876890
396.065250	22922.204494	29.881908
396.538421	22947.463670	29.886925
396.961183	22997.394246	29.891943
397.362846	23040.617340	29.896960
397.973755	23078.272190	29.901978
398.667112	23108.912583	29.906996
399.397402	23136.690980	29.912013
399.731118	23179.179359	29.917031
400.485274	23204.710809	29.922048
400.900264	23232.020554	29.927066
401.387273	23258.586030	29.932084
401.714749	23285.246041	29.937101
402.011915	23310.103541	29.942119
403.075185	23332.427133	29.947136
403.403953	23360.369843	29.952154
403.669590	23379.646175	29.957172
403.933375	23401.128229	29.962189
404.259517	23432.180516	29.967207
404.555600	23458.782484	29.972224
404.442545	23490.661966	29.977242
404.883875	23528.590682	29.982260
405.454394	23543.250579	29.987277
405.635804	23584.474544	29.992295
406.329907	23628.480935	29.997312
406.574678	23661.397882	30.002330
406.591541	23702.439326	30.007348
407.354997	23726.371198	30.012365
408.099103	23768.847107	30.017383
408.202233	23807.252722	30.022400
408.455243	23844.288906	30.027418
408.866431	23882.886550	30.032436
409.005466	23918.556779	30.037453
409.290657	23968.890497	30.042471
409.932467	24008.962602	30.047488
410.318968	24046.742903	30.052506
410.431771	24085.754203	30.057524
410.996949	24128.505360	30.062541
411.611969	24173.902984	30.067559
412.079915	24208.188799	30.072576
412.954446	24247.921595	30.077594
413.138633	24282.966088	30.082612
413.479063	24318.725554	30.087629
414.055410	24353.746663	30.092647
414.708826	24379.219564	30.097664
415.408114	24427.081825	30.102682
415.689705	24450.312736	30.107700
416.166932	24478.499177	30.112717
416.526677	24513.611369	30.117735
417.091633	24533.461250	30.122752
417.345053	24567.560096	30.127770
417.268644	24604.219550	30.132788
418.347514	24629.411262	30.137805
418.431268	24667.322309	30.142823
418.728196	24695.714246	30.147840
418.773015	24731.691381	30.152858
419.190274	24769.348153	30.157876
419.953491	24808.448572	30.162893
420.110089	24845.267878	30.167911
420.451244	24878.102210	30.172928
421.084713	24908.975937	30.177946
420.961686	24950.054482	30.182964
421.657123	24976.918221	30.187981
421.682163	25020.918715	30.192999
421.779175	25069.432982	30.198016
422.703682	25102.839884	30.203034
423.015164	25145.260079	30.208052
423.374918	25184.885770	30.213069
423.710544	25223.213437	30.218087
424.176286	25269.692331	30.223104
424.527293	25314.375508	30.228122
425.083344	25362.167636	30.233140
425.186614	25398.383280	30.238157
426.028410	25446.642760	30.243175
426.077136	25495.190894	30.248192
426.754711	25530.141319	30.253210
426.937596	25584.767366	30.258228
427.556882	25643.407889	30.263245
428.134960	25665.399295	30.268263
428.812158	25704.552849	30.273280
429.839740	25743.202881	30.278298
429.945210	25781.889978	30.283316
430.468840	25817.534934	30.288333
430.983146	25855.955897	30.293351
431.209222	25893.720556	30.298368
431.780587	25927.443263	30.303386
432.051256	25967.419406	30.308404
432.881242	26001.386130	30.313421
433.192992	26040.730299	30.318439
433.296748	26070.405803	30.323456
434.148979	26112.244046	30.328474
434.315734	26155.807689	30.333492
434.885235	26184.266472	30.338509
435.153360	26230.626848	30.343527
435.488529	26266.049309	30.348544
436.139437	26302.484162	30.353562
436.548296	26349.296777	30.358580
436.934608	26382.417212	30.363597
437.303379	26422.732819	30.368615
437.460770	26459.712949	30.373632
437.995519	26507.062388	30.378650
438.107677	26557.701444	30.383668
438.965145	26590.824265	30.388685
439.508820	26632.775117	30.393703
440.171377	26674.258696	30.398720
441.020696	26698.382915	30.403738
441.369546	26748.517675	30.408756
441.576235	26774.019338	30.413773
441.895000	26819.102748	30.418791
442.305393	26860.727330	30.423808
443.001175	26894.141426	30.428826
443.513305	26945.135943	30.433844
443.665954	26972.732035	30.438861
444.208304	27013.925439	30.443879
444.202152	27046.299422	30.448896
444.870049	27080.141658	30.453914
445.447176	27126.455681	30.458932
445.755360	27169.114490	30.463949
446.152799	27205.767639	30.468967
446.787479	27242.548028	30.473984
447.536536	27276.295713	30.479002
447.809765	27315.490376	30.484020
448.519644	27348.643873	30.489037
448.798842	27378.906896	30.494055
449.154095	27423.992252	30.499072
449.330287	27465.875974	30.504090
449.611419	27506.434996	30.509108
449.643178	27538.942875	30.514125
450.613522	27590.164304	30.519143
450.778723	27633.864089	30.524160
451.370341	27667.112476	30.529178
451.650503	27696.313962	30.534196
452.022992	27748.564877	30.539213
452.433983	27783.889619	30.544231
452.343896	27833.937786	30.549248
453.186603	27883.839973	30.554266
453.818385	27931.613655	30.559284
453.930454	27967.434301	30.564301
454.744302	28018.851977	30.569319
454.523707	28070.286430	30.574336
455.196259	28113.345233	30.579354
455.602476	28166.388343	30.584372
455.849357	28229.980586	30.589389
456.256797	28281.007483	30.594407
457.146937	28341.648657	30.599424
457.560748	28382.087504	30.604442
458.017915	28427.652134	30.609460
458.372948	28484.370153	30.614477
458.874036	28525.351845	30.619495
459.517509	28585.830111	30.624512
460.277148	28627.270859	30.629530
460.628508	28681.474293	30.634548
461.036081	28725.821103	30.639565
461.829202	28779.272946	30.644583
461.858275	28827.888990	30.649600
462.847495	28860.798923	30.654618
463.669383	28903.083806	30.659636
464.397892	28949.738548	30.664653
465.307081	28983.091039	30.669671
465.272942	29019.511633	30.674688
465.803983	29046.545578	30.679706
466.199457	29082.924279	30.684724
466.729020	29126.222523	30.689741
467.279619	29161.357108	30.694759
467.440258	29200.908032	30.699776
468.330611	29238.916180	30.704794
468.308498	29275.746211	30.709812
468.611162	29325.660647	30.714829
468.909352	29369.931164	30.719847
469.245159	29414.075783	30.724864
469.953004	29458.326575	30.729882
470.225776	29514.813799	30.734900
470.639550	29552.808677	30.739917
471.213759	29597.826596	30.744935
471.554351	29654.297259	30.749952
471.900284	29697.511686	30.754970
472.782867	29744.662439	30.759988
473.136377	29792.041556	30.765005
473.359007	29836.805323	30.770023
473.981183	29888.908798	30.775040
474.381089	29938.348034	30.780058
475.130879	29990.166283	30.785076
475.789859	30044.641190	30.790093
476.143414	30085.073862	30.795111
476.520253	30131.299623	30.800128
477.411401	30175.099716	30.805146
477.756765	30217.759043	30.810164
477.767211	30264.579805	30.815181
478.554573	30314.243717	30.820199
478.771506	30363.978128	30.825216
478.743960	30417.682872	30.830234
479.469187	30475.315568	30.835252
479.856349	30526.660960	30.840269
480.230529	30564.916759	30.845287
480.787954	30631.546330	30.850304
481.384939	30669.274350	30.855322
481.511192	30729.125590	30.860340
482.160090	30780.203040	30.865357
482.365714	30831.533369	30.870375
482.735678	30891.966419	30.875392
482.963943	30934.500166	30.880410
483.622041	30992.081598	30.885428
483.981359	31063.510066	30.890445
484.504671	31117.269416	30.895463
484.712871	31179.334331	30.900480
485.355974	31241.166951	30.905498
486.535295	31298.869892	30.910516
486.877272	31347.050904	30.915533
487.310959	31406.672613	30.920551
487.864107	31459.581065	30.925568
488.899486	31511.187703	30.930586
489.114713	31557.492530	30.935604
489.402382	31617.725638	30.940621
489.645446	31665.442423	30.945639
490.074570	31733.347338	30.950656
490.437460	31789.504232	30.955674
491.080148	31842.336414	30.960692
491.502408	31908.093544	30.965709
492.477853	31955.993413	30.970727
492.877965	32019.269862	30.975744
493.146873	32081.410139	30.980762
493.919400	32140.702713	30.985780
494.107827	32206.712353	30.990797
494.626506	32253.913168	30.995815
495.195970	32324.883149	31.000832
495.474959	32376.743163	31.005850
496.350713	32430.482310	31.010868
496.842807	32496.097590	31.015885
497.562285	32550.778220	31.020903
497.887823	32612.993394	31.025920
498.708581	32671.584491	31.030938
499.279394	32715.414825	31.035956
499.976103	32766.717255	31.040973
500.716851	32817.513465	31.045991
501.217909	32866.943819	31.051008
501.775345	32908.355266	31.056026
502.650288	32950.469406	31.061044
503.011244	32999.384630	31.066061
503.765734	33039.463100	31.071079
503.870678	33085.308094	31.076096
504.514522	33130.341727	31.081114
504.921207	33179.237563	31.086132
504.849582	33230.528700	31.091149
505.557462	33284.859016	31.096167
505.821487	33338.348579	31.101184
506.281001	33385.042782	31.106202
507.317108	33441.408459	31.111220
507.413136	33497.365159	31.116237
507.802617	33551.493139	31.121255
508.442324	33603.969860	31.126272
509.385642	33648.047276	31.131290
509.842023	33701.027132	31.136308
509.898851	33755.972750	31.141325
510.637972	33801.517660	31.146343
511.102058	33865.276485	31.151360
511.661155	33911.153306	31.156378
511.951542	33966.024956	31.161396
512.402724	34014.390997	31.166413
512.776232	34074.301590	31.171431
513.404694	34117.537828	31.176448
514.005790	34176.875652	31.181466
514.102935	34231.892064	31.186484
514.659795	34295.998047	31.191501
515.305661	34341.356406	31.196519
515.417618	34414.832980	31.201536
515.954001	34474.396744	31.206554
516.567443	34523.655321	31.211572
516.791298	34581.965870	31.216589
517.550828	34644.700760	31.221607
517.787051	34708.327105	31.226624
518.079811	34756.327648	31.231642
519.094607	34822.823044	31.236660
519.545938	34879.081827	31.241677
520.288735	34938.386949	31.246695
520.794079	35002.964705	31.251712
521.088731	35062.643857	31.256730
521.682872	35126.069973	31.261748
522.134152	35179.869979	31.266765
522.796354	35233.820450	31.271783
523.383086	35304.348840	31.276800
523.502230	35355.305428	31.281818
524.278259	35427.170325	31.286836
524.793617	35486.765518	31.291853
525.209972	35539.168211	31.296871
525.754621	35612.739235	31.301888
526.455018	35675.328361	31.306906
527.411884	35728.987342	31.311924
528.059773	35803.017081	31.316941
528.699476	35850.491530	31.321959
529.446392	35896.482343	31.326976
529.651413	35945.270727	31.331994
530.726785	35992.487566	31.337012
531.417172	36046.372454	31.342029
532.354933	36093.212714	31.347047
532.626382	36142.237747	31.352064
532.706320	36196.920492	31.357082
533.569130	36245.562278	31.362100
533.946805	36293.793272	31.367117
534.494519	36339.822564	31.372135
535.125775	36390.499077	31.377152
535.150252	36448.346434	31.382170
536.136074	36488.831517	31.387188
536.502449	36548.939903	31.392205
536.742582	36596.213017	31.397223
536.935815	36651.422981	31.402240
537.572080	36709.270074	31.407258
538.139615	36759.900533	31.412276
538.446043	36821.846514	31.417293
539.553836	36880.315787	31.422311
540.161350	36941.158957	31.427328
540.739282	37000.634758	31.432346
541.306068	37059.650860	31.437364
541.669348	37118.243711	31.442381
542.175453	37165.533335	31.447399
542.784922	37220.338108	31.452416
543.467996	37282.498339	31.457434
543.942765	37333.650560	31.462452
544.518905	37386.001140	31.467469
544.990779	37444.236404	31.472487
545.591252	37500.738006	31.477504
546.002236	37558.395026	31.482522
546.561593	37606.113605	31.487540
546.869334	37678.343977	31.492557
547.347110	37731.229337	31.497575
547.987313	37793.296582	31.502592
548.227881	37852.612576	31.507610
549.276916	37908.064830	31.512628
549.777624	37976.497080	31.517645
550.113013	38030.796685	31.522663
550.839752	38091.124868	31.527680
551.153352	38152.940762	31.532698
551.681012	38212.990602	31.537716
552.134313	38268.910190	31.542733
552.891704	38320.330357	31.547751
553.343361	38382.978998	31.552768
553.897656	38434.424921	31.557786
554.461717	38495.538570	31.562804
554.627042	38545.635464	31.567821
555.622050	38608.743512	31.572839
556.370197	38657.642710	31.577856
556.669361	38724.736615	31.582874
557.069547	38780.855563	31.587892
558.137880	38831.304956	31.592909
559.143659	38872.050693	31.597927
559.714752	38912.263810	31.602944
559.859656	38974.443644	31.607962
560.807428	39029.459316	31.612980
561.235734	39065.426392	31.617997
561.807823	39123.410180	31.623015
562.331369	39181.015959	31.628032
562.596219	39241.185702	31.633050
563.272460	39294.404277	31.638068
563.800168	39356.145807	31.643085
564.077742	39417.066610	31.648103
564.290391	39470.434111	31.653120
564.811590	39546.058632	31.658138
565.530973	39607.473622	31.663156
566.074175	39673.450810	31.668173
566.290063	39739.669185	31.673191
566.819914	39813.459266	31.678208
566.756225	39883.200181	31.683226
567.397722	39957.415959	31.688244
568.207458	40044.254197	31.693261
568.829363	40111.289187	31.698279
569.482883	40183.372563	31.703296
569.951413	40269.898327	31.708314
570.955326	40347.568685	31.713332
571.382977	40427.403972	31.718349
572.059666	40492.673373	31.723367
573.150143	40546.241220	31.728384
574.444684	40596.197605	31.733402
575.278411	40650.147438	31.738420
575.936502	40712.277156	31.743437
576.276775	40754.762369	31.748455
576.873182	40818.742475	31.753472
577.748027	40884.519596	31.758490
578.075083	40933.692248	31.763508
578.133871	40992.077625	31.768525
578.657446	41049.719961	31.773543
579.447557	41108.920826	31.778560
579.667971	41185.445627	31.783578
580.443046	41244.238113	31.788596
580.284993	41316.762234	31.793613
580.725874	41384.784501	31.798631
581.611796	41449.916468	31.803648
581.960657	41531.931160	31.808666
582.421302	41597.794264	31.813684
583.092068	41667.261388	31.818701
583.353564	41750.953987	31.823719
584.100037	41822.749910	31.828736
584.322623	41898.378730	31.833754
585.247981	41976.573151	31.838772
585.897692	42061.546995	31.843789
586.371433	42138.598347	31.848807
586.987665	42215.817399	31.853824
587.514013	42296.738232	31.858842
588.417047	42375.810405	31.863860
588.874357	42441.505779	31.868877
589.324215	42514.805153	31.873895
590.094936	42588.402393	31.878912
590.205428	42659.769343	31.883930
591.045791	42733.229658	31.888948
591.930866	42805.310674	31.893965
592.274585	42880.904910	31.898983
592.647301	42951.757350	31.904000
593.084350	43042.106667	31.909018
593.906358	43099.479920	31.914036
594.609109	43176.353542	31.919053
595.090277	43254.059108	31.924071
595.740503	43334.211632	31.929088
596.328110	43406.043904	31.934106
597.010103	43482.365215	31.939124
597.980225	43556.193778	31.944141
598.748896	43618.504126	31.949159
600.023301	43677.307121	31.954176
600.249811	43742.125323	31.959194
600.977478	43801.855543	31.964212
601.969487	43872.322965	31.969229
602.290694	43935.431698	31.974247
602.942075	43987.128463	31.979264
603.748643	44050.129881	31.984282
604.793793	44108.400632	31.989300
605.499192	44157.729943	31.994317
605.922103	44222.733850	31.999335
606.933149	44266.347907	32.004352
607.387157	44318.126955	32.009370
608.132896	44362.813809	32.014388
608.491019	44422.976775	32.019405
608.770872	44480.343618	32.024423
609.325744	44538.704929	32.029440
609.625142	44602.938591	32.034458
610.432395	44667.206762	32.039476
610.854828	44737.057652	32.044493
610.817420	44801.894960	32.049511
611.651644	44870.644371	32.054528
612.260559	44941.624290	32.059546
613.095140	45005.376772	32.064564
614.046278	45079.118467	32.069581
614.576605	45152.243127	32.074599
615.214803	45212.351701	32.079616
615.669756	45289.340998	32.084634
616.375153	45352.070945	32.089652
616.945296	45427.613047	32.094669
616.807652	45503.082800	32.099687
617.407464	45572.117781	32.104704
617.891821	45660.319491	32.109722
618.560233	45738.624309	32.114740
619.267834	45821.452626	32.119757
619.572755	45900.017361	32.124775
620.352160	45974.541679	32.129792
621.056572	46060.755769	32.134810
621.649492	46143.603230	32.139828
622.430460	46217.166550	32.144845
622.655298	46302.571024	32.149863
623.679867	46382.460752	32.154880
623.992262	46467.997639	32.159898
624.633951	46552.547012	32.164916
625.087838	46632.577607	32.169933
625.841968	46725.485845	32.174951
626.544616	46810.545382	32.179968
626.990945	46895.822514	32.184986
627.628100	46962.831508	32.190004
628.698229	47056.033232	32.195021
629.260371	47146.797028	32.200039
629.843099	47233.762170	32.205056
630.968543	47307.850784	32.210074
631.160863	47381.427833	32.215092
632.241977	47439.385274	32.220109
633.099709	47505.127682	32.225127
633.715893	47570.307099	32.230144
634.332848	47646.406008	32.235162
634.688721	47712.037817	32.240180
635.438760	47780.562547	32.245197
636.152343	47851.130325	32.250215
636.743776	47907.843412	32.255232
637.375664	47994.474786	32.260250
637.851374	48057.558209	32.265268
638.500542	48118.229526	32.270285
638.710434	48197.057509	32.275303
639.184701	48275.059860	32.280320
639.952133	48366.827608	32.285338
640.290118	48440.764861	32.290356
641.162952	48526.209067	32.295373
641.423981	48613.166587	32.300391
642.164264	48699.543244	32.305408
642.267942	48803.089505	32.310426
642.967111	48891.371351	32.315444
643.661657	48977.737239	32.320461
643.943564	49080.510277	32.325479
644.379380	49173.585904	32.330496
645.553543	49278.428168	32.335514
646.090067	49372.855438	32.340532
646.674015	49463.504813	32.345549
647.064224	49581.656575	32.350567
647.880254	49675.098594	32.355584
648.810151	49767.631050	32.360602
649.551209	49867.982047	32.365620
650.232788	49972.600919	32.370637
650.701607	50069.294087	32.375655
651.468647	50164.093433	32.380672
651.956077	50268.250534	32.385690
652.815496	50367.319734	32.390708
653.439372	50463.648601	32.395725
654.384828	50565.932057	32.400743
655.152650	50656.620595	32.405760
655.844688	50754.971052	32.410778
656.740787	50857.187597	32.415796
657.528582	50946.184747	32.420813
658.245497	51027.448642	32.425831
659.249716	51106.769613	32.430848
660.272711	51194.516024	32.435866
660.852140	51274.106568	32.440884
661.598375	51339.719229	32.445901
662.849703	51422.343474	32.450919
663.661115	51485.212871	32.455936
664.675246	51549.493363	32.460954
665.163312	51625.815443	32.465972
665.917407	51692.066948	32.470989
666.531526	51754.727524	32.476007
667.378258	51816.586203	32.481024
668.078932	51884.441173	32.486042
668.314971	51950.578388	32.491060
669.089807	52019.624383	32.496077
669.497712	52096.903377	32.501095
669.949634	52167.778452	32.506112
670.400662	52240.014336	32.511130
671.140431	52323.791274	32.516148
672.291486	52373.372297	32.521165
672.969868	52448.041035	32.526183
673.751103	52523.662053	32.531200
674.465603	52592.700209	32.536218
674.706489	52664.628613	32.541236
675.488664	52734.517170	32.546253
675.822501	52810.019343	32.551271
676.621428	52884.651612	32.556288
676.834131	52954.522433	32.561306
677.460553	53046.356124	32.566324
677.779270	53104.415563	32.571341
678.449486	53195.028016	32.576359
679.384850	53270.924721	32.581376
679.864717	53348.690154	32.586394
680.157616	53438.198281	32.591412
681.058569	53523.643843	32.596429
681.385828	53607.167234	32.601447
681.959098	53698.783986	32.606464
682.709146	53782.292412	32.611482
683.458108	53871.414357	32.616500
683.894007	53958.940345	32.621517
684.504863	54056.608647	32.626535
684.814261	54159.969325	32.631552
685.947538	54248.285779	32.636570
686.452944	54349.768747	32.641588
686.969914	54441.878144	32.646605
688.129034	54549.860000	32.651623
688.334269	54641.569681	32.656640
689.416565	54747.248295	32.661658
689.981588	54850.255534	32.666676
690.132299	54940.164986	32.671693
691.027572	55052.968408	32.676711
691.819670	55160.301733	32.681728
692.396563	55253.335180	32.686746
692.906023	55377.256455	32.691764
693.700907	55483.761764	32.696781
694.671493	55581.753393	32.701799
695.406699	55695.053240	32.706816
696.391327	55796.347092	32.711834
697.231464	55901.321975	32.716852
698.121808	55996.125564	32.721869
698.873403	56089.995619	32.726887
699.701671	56177.911342	32.731904
701.040235	56267.487888	32.736922
701.738844	56367.234101	32.741940
702.665676	56450.122983	32.746957
703.166056	56538.983743	32.751975
703.558811	56630.393233	32.756992
704.267258	56720.367606	32.762010
705.015023	56821.519354	32.767028
705.630985	56912.989899	32.772045
706.624086	57012.920521	32.777063
707.122911	57102.764600	32.782080
707.928141	57190.852198	32.787098
708.293824	57281.857018	32.792116
709.345224	57384.678754	32.797133
709.920781	57467.607168	32.802151
710.504491	57565.604204	32.807168
711.332182	57652.202629	32.812186
712.047218	57750.116557	32.817204
712.718961	57840.512259	32.822221
713.114162	57942.546718	32.827239
714.120032	58035.498461	32.832256
714.819022	58134.587366	32.837274
715.688878	58227.997867	32.842292
717.055409	58310.862274	32.847309
717.797337	58408.755668	32.852327
718.016720	58489.439487	32.857344
719.062456	58573.620899	32.862362
719.808987	58666.191607	32.867380
720.456697	58752.714555	32.872397
720.747530	58844.781327	32.877415
721.835348	58933.356363	32.882432
722.510245	59007.634770	32.887450
723.422678	59113.087030	32.892468
723.963404	59199.159936	32.897485
724.257459	59283.936236	32.902503
724.711100	59372.713454	32.907520
725.657622	59471.465228	32.912538
726.262877	59548.826051	32.917556
726.748564	59633.687490	32.922573
727.446408	59730.010688	32.927591
727.859404	59830.043769	32.932608
728.778512	59931.225970	32.937626
729.387722	60038.945117	32.942644
729.955296	60124.649951	32.947661
730.873739	60241.366817	32.952679
730.945105	60339.202062	32.957696
732.030403	60444.113947	32.962714
732.363305	60552.650861	32.967732
733.008460	60655.980475	32.972749
734.030065	60767.107030	32.977767
734.471112	60878.976988	32.982784
735.615836	60987.135490	32.987802
736.129628	61111.680434	32.992820
736.727479	61226.268316	32.997837
737.419793	61332.011463	33.002855
737.864301	61460.613943	33.007872
738.746766	61568.569188	33.012890
739.246913	61701.513019	33.017908
739.741890	61827.178626	33.022925
740.497221	61945.733215	33.027943
741.011728	62077.474067	33.032960
742.098056	62209.246349	33.037978
742.725255	62347.700109	33.042996
743.307445	62460.992102	33.048013
744.100787	62601.548264	33.053031
744.887249	62735.244093	33.058048
746.506114	62851.129266	33.063066
747.951859	62965.573413	33.068084
748.451715	63080.672650	33.073101
749.602016	63198.487660	33.078119
749.972233	63311.981309	33.083136
751.068424	63413.821070	33.088154
751.790382	63524.430815	33.093172
752.629326	63646.930729	33.098189
753.533115	63756.227897	33.103207
754.286013	63859.566630	33.108224
755.695451	63955.193411	33.113242
756.962060	64065.283433	33.118260
757.774714	64166.480600	33.123277
758.695311	64234.905564	33.128295
759.447250	64325.591052	33.133312
760.787507	64415.665608	33.138330
761.556939	64506.627568	33.143348
762.378614	64579.937419	33.148365
762.751483	64669.271712	33.153383
763.617249	64765.309591	33.158400
764.018085	64844.706855	33.163418
764.968810	64937.617246	33.168436
765.534287	65023.016402	33.173453
766.323717	65120.447749	33.178471
766.683868	65225.347716	33.183488
767.579660	65315.533075	33.188506
768.147232	65411.803709	33.193524
768.274950	65516.051185	33.198541
769.158165	65615.071529	33.203559
769.846781	65726.316616	33.208576
769.959047	65825.363537	33.213594
770.787640	65955.410438	33.218612
771.411040	66057.828759	33.223629
772.357543	66169.149363	33.228647
772.584436	66285.255666	33.233664
773.568467	66418.249989	33.238682
774.196023	66544.614866	33.243700
774.745359	66663.217619	33.248717
775.451595	66775.376254	33.253735
776.043897	66892.308169	33.258752
777.026064	67002.848054	33.263770
777.320000	67131.040895	33.268788
778.371339	67247.687278	33.273805
779.092456	67364.075655	33.278823
779.595352	67487.894077	33.283840
780.595967	67614.883303	33.288858
781.334279	67734.727755	33.293876
781.834753	67854.375736	33.298893
782.912845	67992.371895	33.303911
783.915295	68119.167038	33.308928
784.516625	68241.314742	33.313946
785.644501	68360.163993	33.318964
785.963149	68490.981123	33.323981
787.348957	68622.752554	33.328999
788.037846	68752.512588	33.334016
788.675358	68877.127089	33.339034
789.809968	69003.196694	33.344052
790.679435	69127.776078	33.349069
791.970420	69239.904536	33.354087
792.790496	69355.811493	33.359104
794.186673	69458.780887	33.364122
795.184964	69563.066760	33.369140
795.863168	69676.857100	33.374157
796.584834	69784.980147	33.379175
797.254473	69901.293023	33.384192
798.745314	70008.036439	33.389210
800.028056	70105.377790	33.394228
800.637605	70206.041727	33.399245
801.922073	70295.658116	33.404263
802.186549	70393.008014	33.409280
802.958925	70489.189575	33.414298
804.309766	70590.118854	33.419316
805.045841	70688.839789	33.424333
805.835777	70774.001248	33.429351
806.264070	70888.538898	33.434368
806.912704	70988.465156	33.439386
807.429099	71078.571782	33.444404
808.275650	71187.244663	33.449421
809.585615	71284.877435	33.454439
810.162135	71387.602828	33.459456
811.317224	71493.189020	33.464474
811.916751	71599.356575	33.469492
812.582610	71706.578057	33.474509
813.737417	71812.330222	33.479527
814.297397	71912.907138	33.484544
815.066362	72026.332494	33.489562
815.457956	72124.884778	33.494580
815.939219	72236.291605	33.499597
816.636027	72343.130855	33.504615
816.845715	72460.673315	33.509632
818.044512	72579.112669	33.514650
818.683855	72698.995395	33.519668
819.574298	72824.045008	33.524685
820.623592	72941.407460	33.529703
821.374644	73070.077174	33.534720
822.620492	73171.868726	33.539738
823.829755	73271.171181	33.544756
824.569580	73393.941832	33.549773
825.532233	73489.863865	33.554791
826.292770	73603.474599	33.559808
827.124714	73706.282970	33.564826
828.052950	73805.276762	33.569844
828.666310	73911.413392	33.574861
830.386743	74012.259857	33.579879
831.294640	74118.427186	33.584896
832.055560	74207.239496	33.589914
832.922526	74301.976107	33.594932
833.445576	74392.257597	33.599949
834.332361	74478.758443	33.604967
834.771480	74588.129692	33.609984
835.163758	74687.983335	33.615002
836.166837	74784.866346	33.620020
836.249021	74888.290652	33.625037
837.165604	74993.054057	33.630055
837.964929	75115.189924	33.635072
838.023947	75228.828712	33.640090
838.827870	75346.936805	33.645108
839.385039	75481.677954	33.650125
840.047392	75611.171763	33.655143
840.665014	75741.977920	33.660160
841.453774	75880.117605	33.665178
842.079914	76026.149885	33.670196
843.174277	76179.634087	33.675213
843.893119	76324.754067	33.680231
844.845177	76467.874831	33.685248
845.658613	76613.032205	33.690266
846.415538	76758.984598	33.695284
847.259175	76886.758621	33.700301
848.233617	77032.881102	33.705319
849.268395	77184.340767	33.710336
850.241933	77327.994725	33.715354
851.405566	77463.879505	33.720372
852.245000	77593.228319	33.725389
853.401876	77732.333181	33.730407
854.651978	77863.899232	33.735424
855.582219	78006.904775	33.740442
856.627272	78133.170878	33.745460
857.096912	78263.328177	33.750477
858.326785	78396.268127	33.755495
859.182897	78507.806784	33.760512
860.181871	78647.143687	33.765530
861.381903	78774.439948	33.770548
861.929649	78910.973055	33.775565
862.756484	79034.224292	33.780583
863.503134	79165.609335	33.785600
864.671469	79290.543864	33.790618
865.788687	79412.788479	33.795636
866.452042	79551.232308	33.800653
867.273973	79670.141673	33.805671
868.508308	79804.189883	33.810688
868.901632	79934.797722	33.815706
869.992515	80060.736030	33.820724
870.411777	80197.105527	33.825741
871.302442	80332.553029	33.830759
872.153430	80463.497095	33.835776
872.779585	80590.802836	33.840794
873.648894	80726.838383	33.845812
874.216047	80884.422180	33.850829
875.203303	81015.968297	33.855847
876.483847	81157.060073	33.860864
877.096780	81297.078803	33.865882
878.526146	81419.257970	33.870900
879.748049	81554.241394	33.875917
880.195885	81682.973685	33.880935
881.444391	81817.675464	33.885952
882.439412	81952.696318	33.890970
883.507654	82066.876674	33.895988
884.057967	82198.420699	33.901005
884.989362	82338.141318	33.906023
885.761476	82464.381029	33.911040
886.358946	82597.541317	33.916058
887.357808	82724.076107	33.921076
888.453983	82860.301800	33.926093
889.064958	82974.215300	33.931111
889.877809	83099.450478	33.936128
890.776949	83224.596671	33.941146
891.145598	83355.198848	33.946164
892.034854	83482.919869	33.951181
893.382536	83600.090931	33.956199
894.015013	83733.833895	33.961216
894.994166	83867.611898	33.966234
896.062446	83992.620927	33.971252
896.614534	84125.427980	33.976269
897.544103	84258.607358	33.981287
897.685152	84394.508403	33.986304
898.624409	84548.759731	33.991322
899.668841	84696.989228	33.996340
900.563338	84841.416218	34.001357
901.112164	84987.659379	34.006375
902.386574	85132.357793	34.011392
903.429889	85271.682370	34.016410
904.588319	85417.806910	34.021428
905.595384	85556.530296	34.026445
906.634950	85706.831205	34.031463
907.500916	85852.040673	34.036480
908.219743	86005.903433	34.041498
909.094588	86147.564865	34.046516
910.083265	86287.409742	34.051533
911.089260	86424.464730	34.056551
912.047953	86589.026219	34.061568
913.155378	86737.471687	34.066586
913.479804	86881.769966	34.071604
914.557669	87035.581926	34.076621
914.858796	87187.767525	34.081639
915.962583	87332.769692	34.086656
916.470526	87503.236198	34.091674
917.329036	87660.443984	34.096692
918.226112	87833.449345	34.101709
919.190789	87989.565085	34.106727
920.398336	88160.268006	34.111744
921.590696	88320.493842	34.116762
922.825873	88471.247174	34.121780
923.902512	88633.647217	34.126797
925.113714	88789.361055	34.131815
925.987741	88937.131768	34.136832
926.600895	89096.425958	34.141850
927.754255	89249.553258	34.146868
928.293243	89407.048445	34.151885
929.296487	89560.568370	34.156903
930.231000	89734.973007	34.161920
931.077339	89895.147430	34.166938
932.117146	90038.816761	34.171956
932.879673	90210.462905	34.176973
933.872797	90374.380975	34.181991
935.327189	90527.860560	34.187008
935.861803	90682.967780	34.192026
937.084139	90843.253140	34.197044
937.996492	90994.944231	34.202061
938.881086	91153.978701	34.207079
939.956667	91306.216128	34.212096
940.789146	91476.996681	34.217114
941.845633	91623.560658	34.222132
942.666891	91792.278839	34.227149
943.194659	91948.648365	34.232167
944.023382	92117.937528	34.237184
944.796455	92281.507463	34.242202
945.681689	92446.645035	34.247220
946.668545	92612.920981	34.252237
947.674028	92778.523153	34.257255
949.186138	92937.265885	34.262272
949.729981	93105.844631	34.267290
951.011330	93261.456457	34.272308
951.589855	93414.035718	34.277325
952.609152	93574.443275	34.282343
953.511700	93729.128120	34.287360
954.260312	93889.212117	34.292378
955.802277	94044.292759	34.297396
956.908655	94201.407050	34.302413
957.485225	94352.343460	34.307431
959.051522	94508.297216	34.312448
959.489165	94664.732683	34.317466
960.665740	94820.051872	34.322484
961.455601	94982.467353	34.327501
962.305259	95133.301417	34.332519
963.717163	95298.637964	34.337536
964.624638	95452.620780	34.342554
965.850774	95604.412237	34.347572
967.353095	95753.347130	34.352589
967.905896	95912.306001	34.357607
968.773251	96064.815014	34.362624
969.556736	96226.287242	34.367642
970.267379	96384.133636	34.372660
971.323944	96553.271908	34.377677
971.897703	96721.548631	34.382695
973.382898	96884.612990	34.387712
974.222611	97042.543877	34.392730
974.739150	97224.155186	34.397748
975.856559	97386.126147	34.402765
976.411238	97554.727195	34.407783
977.834262	97726.020090	34.412800
978.697468	97901.128534	34.417818
979.647218	98076.148328	34.422836
980.464707	98256.640871	34.427853
981.314276	98443.556653	34.432871
982.716255	98607.961281	34.437888
984.754223	98758.296971	34.442906
985.902762	98918.381938	34.447924
986.821243	99079.847512	34.452941
987.771375	99249.460461	34.457959
988.475208	99405.586087	34.462976
989.254610	99575.835996	34.467994
990.519397	99756.533152	34.473012
991.482198	99920.214556	34.478029
992.552959	100080.152654	34.483047
993.501965	100245.194367	34.488064
994.009151	100419.383386	34.493082
994.551681	100587.444400	34.498100
995.906865	100766.459545	34.503117
996.672321	100954.341174	34.508135
998.306078	101121.524120	34.513152
998.531711	101300.224595	34.518170
999.610286	101491.103030	34.523188
1000.718276	101664.913018	34.528205
1001.327506	101851.112678	34.533223
1002.606148	102031.820260	34.538240
1003.676455	102206.146141	34.543258
1005.318992	102376.985501	34.548276
1006.695731	102554.371485	34.553293
1007.980506	102702.662591	34.558311
1009.352265	102862.072661	34.563328
1010.322770	103026.047290	34.568346
1011.567147	103181.155369	34.573364
1012.896001	103342.070564	34.578381
1013.433794	103510.261330	34.583399
1014.633477	103663.552880	34.588416
1015.140263	103824.903407	34.593434
1016.253976	103983.585820	34.598452
1017.186718	104142.677695	34.603469
1017.862461	104306.159552	34.608487
1018.598730	104460.503607	34.613504
1019.306922	104622.371645	34.618522
1020.303085	104786.363561	34.623540
1021.646732	104946.231746	34.628557
1022.328754	105115.701278	34.633575
1023.101766	105274.506515	34.638592
1024.507790	105440.516896	34.643610
1025.617386	105600.665731	34.648628
1026.786677	105755.074698	34.653645
1027.597867	105931.400543	34.658663
1028.534658	106107.910515	34.663680
1029.519343	106270.858969	34.668698
1030.065339	106444.274541	34.673716
1030.903893	106618.418676	34.678733
1032.043760	106806.350625	34.683751
1032.965935	106993.201820	34.688768
1033.876705	107157.243885	34.693786
1035.081515	107357.810978	34.698804
1035.986832	107537.947153	34.703821
1037.006160	107741.030886	34.708839
1038.230138	107911.481900	34.713856
1039.126902	108103.592860	34.718874
1040.243497	108289.532981	34.723892
1041.424354	108473.092724	34.728909
1042.426662	108668.094186	34.733927
1043.108304	108861.308204	34.738944
1043.948921	109053.838986	34.743962
1045.074853	109254.746409	34.748980
1046.861130	109438.913902	34.753997
1047.914832	109634.077557	34.759015
1049.111520	109818.364711	34.764032
1050.395511	110011.452714	34.769050
1051.363395	110195.764981	34.774068
1052.660107	110381.954317	34.779085
1053.794896	110577.313399	34.784103
1055.023619	110763.477341	34.789120
1055.905217	110939.601966	34.794138
1056.619992	111130.375662	34.799156
1058.011442	111306.688597	34.804173
1058.822222	111500.061699	34.809191
1060.546931	111680.204967	34.814208
1061.890010	111858.608042	34.819226
1063.128059	112048.188694	34.824244
1064.335593	112228.212773	34.829261
1065.172042	112408.194393	34.834279
1065.998975	112583.536683	34.839296
1067.219246	112765.679395	34.844314
1068.163908	112951.848453	34.849332
1069.209413	113133.956969	34.854349
1069.619845	113324.751908	34.859367
1070.620727	113512.170611	34.864384
1071.100589	113707.053168	34.869402
1072.179766	113912.699371	34.874420
1073.299292	114100.521054	34.879437
1074.512304	114306.326077	34.884455
1075.615966	114506.962046	34.889472
1076.878096	114707.992841	34.894490
1077.559733	114906.667779	34.899508
1078.662317	115107.776468	34.904525
1079.514450	115306.477598	34.909543
1080.853329	115514.666799	34.914560
1081.646004	115715.193143	34.919578
1082.709731	115925.178031	34.924596
1083.993397	116140.076241	34.929613
1084.813310	116346.436139	34.934631
1085.547210	116556.044974	34.939648
1087.076722	116764.553777	34.944666
1088.723731	116968.885060	34.949684
1090.567785	117144.292774	34.954701
1091.876808	117329.259954	34.959719
1092.545921	117505.741172	34.964736
1094.057311	117686.454659	34.969754
1094.839236	117865.545491	34.974772
1096.175154	118023.050798	34.979789
1097.302321	118204.511855	34.984807
1098.731483	118379.241889	34.989824
1100.105441	118551.584031	34.994842
1101.230244	118723.610796	34.999860
1102.653344	118897.177191	35.004877
1103.326944	119063.048063	35.009895
1104.362249	119235.408255	35.014912
1106.322046	119404.427965	35.019930
1107.055455	119565.255856	35.024948
1108.436554	119728.177474	35.029965
1109.232584	119902.011487	35.034983
1110.154748	120071.196572	35.040000
1111.232833	120253.245831	35.045018
1111.474693	120423.985039	35.050036
1112.817931	120606.286198	35.055053
1113.696414	120798.276249	35.060071
1114.724774	120999.288279	35.065088
1116.037393	121183.448963	35.070106
1116.527878	121372.432765	35.075124
1117.820742	121575.030058	35.080141
1119.156635	121763.934136	35.085159
1120.049982	121955.546976	35.090176
1121.436368	122147.717836	35.095194
1122.088622	122355.138442	35.100212
1123.407425	122554.172066	35.105229
1124.359699	122758.896522	35.110247
1125.485371	122954.473824	35.115264
1126.626142	123170.258244	35.120282
1127.748150	123371.901996	35.125300
1129.041471	123573.748295	35.130317
1130.171962	123775.684533	35.135335
1130.981430	123993.047582	35.140352
1132.228542	124194.333364	35.145370
1133.071326	124416.146321	35.150388
1134.173716	124629.546904	35.155405
1135.444776	124853.185470	35.160423
1136.622046	125063.290849	35.165440
1137.934447	125278.361951	35.170458
1138.721383	125490.471678	35.175476
1139.976492	125706.886099	35.180493
1141.074496	125927.424063	35.185511
1141.964912	126147.094951	35.190528
1143.306929	126374.942754	35.195546
1144.195714	126604.359827	35.200564
1145.763849	126808.132956	35.205581
1146.731915	127037.946009	35.210599
1148.315562	127254.672372	35.215616
1149.591994	127462.605008	35.220634
1150.541125	127679.509044	35.225652
1151.730363	127895.171325	35.230669
1152.574675	128115.418105	35.235687
1153.617666	128337.601490	35.240704
1155.217887	128561.360878	35.245722
1156.028886	128792.273919	35.250740
1157.204608	129010.494243	35.255757
1159.397022	129218.101870	35.260775
1160.458790	129432.104518	35.265792
1162.011885	129632.214291	35.270810
1162.860700	129849.589274	35.275828
1164.299225	130051.013114	35.280845
1165.443912	130261.631954	35.285863
1166.254064	130473.661823	35.290880
1167.126036	130672.335151	35.295898
1168.085991	130876.832186	35.300916
1168.898773	131085.350028	35.305933
1170.178489	131294.341375	35.310951
1170.920468	131507.072162	35.315968
1172.314610	131712.101526	35.320986
1173.266803	131928.734880	35.326004
1174.072097	132152.282193	35.331021
1175.116906	132374.536978	35.336039
1176.357540	132596.305442	35.341056
1177.389660	132826.736018	35.346074
1178.695670	133060.373259	35.351092
1179.858916	133278.008026	35.356109
1181.101649	133513.307122	35.361127
1182.123655	133749.809409	35.366144
1183.617811	133968.233232	35.371162
1184.558879	134204.230349	35.376180
1185.872947	134439.523169	35.381197
1187.142085	134673.796426	35.386215
1188.636112	134908.505205	35.391232
1190.455624	135132.885831	35.396250
1191.648719	135364.217950	35.401268
1193.051067	135591.077155	35.406285
1194.233593	135811.703245	35.411303
1195.278818	136029.065275	35.416320
1196.569804	136246.491386	35.421338
1197.700427	136474.463461	35.426356
1198.598046	136706.178580	35.431373
1200.115708	136936.033904	35.436391
1201.351017	137146.404713	35.441408
1203.568325	137364.325598	35.446426
1204.754625	137583.144933	35.451444
1206.350205	137797.294707	35.456461
1207.975926	138006.339286	35.461479
1208.952350	138224.026990	35.466496
1209.853798	138431.828995	35.471514
1210.856068	138665.923288	35.476532
1212.005101	138872.774778	35.481549
1212.828665	139092.901619	35.486567
1213.861014	139325.040138	35.491584
1215.002640	139548.038133	35.496602
1215.649978	139777.244148	35.501620
1216.825787	140022.384250	35.506637
1217.811235	140260.473939	35.511655
1218.588600	140513.597993	35.516672
1219.884888	140756.958960	35.521690
1220.877783	141009.493479	35.526708
1221.975330	141256.974580	35.531725
1223.645984	141503.986495	35.536743
1224.325537	141761.904258	35.541760
1226.184028	142007.734424	35.546778
1227.261095	142261.341022	35.551796
1228.438982	142505.071936	35.556813
1229.656105	142756.958519	35.561831
1231.109069	143015.916721	35.566848
1232.353766	143265.263272	35.571866
1233.437463	143525.513023	35.576884
1234.631138	143778.258802	35.581901
1235.989613	144034.089547	35.586919
1237.019863	144300.012229	35.591936
1238.606957	144549.819260	35.596954
1239.402899	144809.511504	35.601972
1240.721105	145070.113303	35.606989
1242.065372	145316.966809	35.612007
1243.119896	145585.697394	35.617024
1244.110453	145836.289510	35.622042
1245.339777	146110.110452	35.627060
1246.821945	146375.998619	35.632077
1248.110809	146627.309430	35.637095
1248.837777	146880.676753	35.642112
1250.372899	147123.460143	35.647130
1251.284149	147384.073898	35.652148
1252.663377	147632.278416	35.657165
1254.154737	147879.476522	35.662183
1255.463221	148146.822492	35.667200
1256.518577	148398.114896	35.672218
1257.584184	148663.394479	35.677236
1259.023558	148923.285825	35.682253
1260.067602	149174.405963	35.687271
1260.955992	149455.850080	35.692288
1262.326823	149716.695293	35.697306
1263.928161	149977.696084	35.702324
1265.530505	150243.178707	35.707341
1267.459704	150491.983173	35.712359
1268.993764	150752.731660	35.717376
1270.657729	150995.487106	35.722394
1272.464869	151246.725874	35.727412
1274.387750	151475.987781	35.732429
1275.680693	151699.725971	35.737447
1276.791978	151943.282949	35.742464
1277.980771	152186.143400	35.747482
1279.434214	152422.972010	35.752500
1280.370709	152660.999603	35.757517
1281.630346	152901.440238	35.762535
1283.043460	153144.422053	35.767552
1284.943509	153363.108526	35.772570
1286.404243	153594.952182	35.777588
1287.888946	153825.866362	35.782605
1289.298761	154047.958066	35.787623
1290.350699	154280.211241	35.792640
1291.848868	154508.396813	35.797658
1292.936154	154735.936725	35.802676
1293.678237	154974.994575	35.807693
1295.296359	155209.892151	35.812711
1296.054218	155449.749233	35.817728
1297.171837	155689.093982	35.822746
1298.003485	155937.434144	35.827764
1299.195970	156183.979707	35.832781
1300.227435	156440.491437	35.837799
1301.369487	156710.341827	35.842816
1302.502429	156971.702051	35.847834
1303.619718	157234.208406	35.852852
1304.366729	157510.065435	35.857869
1305.837601	157785.328011	35.862887
1306.921046	158063.407305	35.867904
1307.947356	158342.398168	35.872922
1308.813752	158620.069655	35.877940
1309.780102	158919.854483	35.882957
1311.377208	159209.588955	35.887975
1312.472039	159500.749114	35.892992
1314.002904	159786.357983	35.898010
1315.556797	160091.464748	35.903028
1316.948390	160391.837594	35.908045
1318.665127	160667.049168	35.913063
1320.164032	160961.072849	35.918080
1321.368710	161248.643766	35.923098
1322.549205	161538.898565	35.928116
1324.092032	161843.012548	35.933133
1325.572374	162125.542114	35.938151
1327.016471	162400.397572	35.943168
1329.002926	162682.609127	35.948186
1330.549549	162965.449376	35.953204
1331.684790	163229.933257	35.958221
1333.578508	163497.244976	35.963239
1335.226850	163772.036137	35.968256
1336.810461	164034.040786	35.973274
1338.382222	164283.555198	35.978292
1339.596551	164521.039607	35.983309
1340.968328	164759.680971	35.988327
1342.693542	165008.488457	35.993344
1344.598645	165236.446534	35.998362
1346.282085	165463.665589	36.003380
1347.802382	165686.060866	36.008397
1349.222301	165902.276655	36.013415
1350.673396	166120.405431	36.018432
1351.936763	166344.493616	36.023450
1352.639234	166567.591105	36.028468
1354.086184	166807.434033	36.033485
1354.969412	167035.545328	36.038503
1355.985229	167280.916977	36.043520
1356.956453	167525.801284	36.048538
1357.963228	167777.638778	36.053556
1358.467772	168039.611764	36.058573
1359.856045	168302.475841	36.063591
1361.150676	168573.265800	36.068608
1362.281024	168847.942409	36.073626
1363.329061	169127.711803	36.078644
1364.446701	169415.330941	36.083661
1365.734283	169703.737235	36.088679
1366.811573	170000.075295	36.093696
1368.058128	170289.074379	36.098714
1369.281212	170580.186030	36.103732
1370.386728	170886.097044	36.108749
1372.392315	171184.922890	36.113767
1373.629925	171491.031546	36.118784
1374.557384	171800.364383	36.123802
1376.439108	172102.933631	36.128820
1377.613538	172409.538371	36.133837
1379.279313	172721.019544	36.138855
1380.368746	173033.354047	36.143872
1381.479081	173340.556595	36.148890
1383.635600	173656.040694	36.153908
1384.616219	173974.744921	36.158925
1386.070968	174283.624146	36.163943
1387.436493	174605.368957	36.168960
1388.617517	174924.388444	36.173978
1389.937830	175239.565240	36.178996
1391.105617	175576.036618	36.184013
1392.628413	175884.352571	36.189031
1394.326046	176211.334207	36.194048
1395.859841	176536.095165	36.199066
1397.676624	176852.990874	36.204084
1399.116395	177174.365846	36.209101
1400.543998	177496.378865	36.214119
1401.806390	177816.311000	36.219136
1403.163137	178138.616890	36.224154
1404.744725	178455.936319	36.229172
1405.735349	178781.628945	36.234189
1407.792056	179102.812946	36.239207
1409.054171	179421.684322	36.244224
1410.684068	179744.715283	36.249242
1412.423658	180043.348418	36.254260
1413.778299	180351.059017	36.259277
1416.109085	180653.944658	36.264295
1418.194189	180949.631334	36.269312
1420.221033	181241.112001	36.274330
1422.057898	181517.917800	36.279348
1423.379571	181805.446909	36.284365
1424.489159	182079.777587	36.289383
1426.253937	182357.206704	36.294400
1427.595526	182636.887133	36.299418
1429.296497	182894.466226	36.304436
1431.167458	183170.560361	36.309453
1432.529518	183437.845409	36.314471
1433.730922	183690.856859	36.319488
1434.962762	183943.838799	36.324506
1436.741231	184192.367229	36.329524
1437.334007	184446.644225	36.334541
1438.500930	184703.117909	36.339559
1439.662996	184968.889055	36.344576
1441.210814	185250.881348	36.349594
1442.541511	185508.575995	36.354612
1443.189228	185783.725867	36.359629
1444.492118	186142.363077	36.364647
1445.794951	186425.209705	36.369664
1446.466995	186722.912913	36.374682
1448.181404	187010.065398	36.379700
1449.333711	187309.727043	36.384717
1450.411951	187620.348377	36.389735
1451.789088	187928.968037	36.394752
1452.962219	188251.742802	36.399770
1454.349113	188552.107744	36.404788
1455.219087	188883.720164	36.409805
1456.971105	189198.939482	36.414823
1458.742454	189542.833382	36.419840
1460.325422	189861.002009	36.424858
1461.965254	190182.820251	36.429876
1463.311974	190521.830484	36.434893
1465.182407	190842.420635	36.439911
1466.526543	191167.666111	36.444928
1467.880177	191504.569833	36.449946
1469.112074	191826.964398	36.454964
1470.644171	192169.404766	36.459981
1472.247362	192513.790815	36.464999
1473.562070	192842.779269	36.470016
1475.125100	193177.368714	36.475034
1477.256315	193513.825983	36.480052
1478.627355	193854.060859	36.485069
1479.576672	194191.644715	36.490087
1481.311391	194535.050381	36.495104
1482.884554	194868.499544	36.500122
1484.506924	195203.669121	36.505140
1485.914368	195549.744937	36.510157
1487.268578	195906.092125	36.515175
1488.787229	196245.979738	36.520192
1490.045362	196587.407638	36.525210
1491.836793	196928.067046	36.530228
1493.250182	197286.542182	36.535245
1494.689796	197632.287836	36.540263
1496.013536	197989.737251	36.545280
1497.311952	198349.096620	36.550298
1498.968744	198702.863138	36.555316
1499.849413	199060.613040	36.560333
1501.071937	199434.161114	36.565351
1502.800313	199796.301575	36.570368
1504.372577	200169.491811	36.575386
1506.188694	200536.599018	36.580404
1507.376052	200914.118760	36.585421
1508.923277	201283.530500	36.590439
1510.811492	201644.633909	36.595456
1512.548542	202016.811778	36.600474
1514.050538	202376.656227	36.605492
1515.510948	202743.747627	36.610509
1516.941364	203100.937467	36.615527
1518.622329	203476.226249	36.620544
1520.085428	203850.965620	36.625562
1521.727998	204225.855457	36.630580
1522.943851	204598.831390	36.635597
1524.539990	204964.788140	36.640615
1526.358400	205328.602333	36.645632
1527.262050	205703.280362	36.650650
1528.954978	206059.596224	36.655668
1530.635923	206427.828558	36.660685
1531.825693	206788.365065	36.665703
1533.284252	207143.500046	36.670720
1534.761929	207502.722495	36.675738
1536.317897	207864.219536	36.680756
1537.685403	208229.328478	36.685773
1538.796422	208595.545055	36.690791
1540.658233	208969.113234	36.695808
1542.209189	209333.839467	36.700826
1544.580091	209687.641476	36.705844
1546.583423	210053.669703	36.710861
1548.093451	210408.420316	36.715879
1549.708629	210763.535982	36.720896
1551.443458	211118.074494	36.725914
1554.541438	211436.352544	36.730932
1556.795926	211769.065131	36.735949
1558.750093	212083.051866	36.740967
1560.653707	212409.697810	36.745984
1561.924373	212732.759630	36.751002
1563.622280	213053.036717	36.756020
1564.931961	213375.813621	36.761037
1566.318660	213703.430876	36.766055
1567.829932	214025.821181	36.771072
1568.527680	214358.653003	36.776090
1570.414549	214691.375229	36.781108
1571.626837	215039.394766	36.786125
1572.868544	215371.761273	36.791143
1574.623678	215722.414643	36.796160
1575.317529	216079.077277	36.801178
1576.445791	216430.311998	36.806196
1578.020636	216794.102815	36.811213
1579.109993	217170.519405	36.816231
1580.421119	217547.206417	36.821248
1581.542553	217934.618434	36.826266
1583.237671	218318.282771	36.831284
1585.241595	218702.153069	36.836301
1586.097267	219100.073877	36.841319
1587.727044	219486.721426	36.846336
1588.989166	219891.184119	36.851354
1590.420994	220287.821438	36.856372
1592.219020	220704.165968	36.861389
1593.496580	221113.224977	36.866407
1594.796310	221530.206748	36.871424
1596.368678	221945.494747	36.876442
1598.665461	222363.946639	36.881460
1600.019713	222779.472272	36.886477
1601.070861	223205.410308	36.891495
1603.381410	223627.543961	36.896512
1604.948473	224057.059609	36.901530
1606.696745	224464.419995	36.906548
1608.671284	224891.204534	36.911565
1610.194341	225312.115192	36.916583
1611.854831	225724.163718	36.921600
1613.938860	226135.028162	36.926618
1615.653808	226547.906447	36.931636
1617.197911	226973.488051	36.936653
1618.864097	227377.736457	36.941671
1620.869161	227788.231954	36.946688
1622.801267	228192.692599	36.951706
1624.707726	228594.515120	36.956724
1626.693159	228990.431412	36.961741
1628.257141	229392.434276	36.966759
1630.153539	229785.569758	36.971776
1631.717020	230187.343726	36.976794
1633.139744	230573.566878	36.981812
1635.055426	230976.606340	36.986829
1636.563599	231369.039683	36.991847
1638.123737	231754.300747	36.996864
1639.647232	232132.123957	37.001882
1641.394022	232512.935049	37.006900
1643.023345	232880.401812	37.011917
1644.419110	233262.435901	37.016935
1645.539444	233634.808530	37.021952
1647.422265	234019.636455	37.026970
1648.598436	234399.570097	37.031988
1650.431534	234791.060958	37.037005
1652.240110	235175.924913	37.042023
1653.810698	235562.604016	37.047040
1655.153570	235958.616146	37.052058
1656.885011	236346.691908	37.057076
1659.658373	236734.807436	37.062093
1660.861654	237125.911846	37.067111
1662.477104	237514.588774	37.072128
1664.184012	237908.255444	37.077146
1665.767595	238296.809416	37.082164
1667.319878	238687.095245	37.087181
1668.728441	239098.360948	37.092199
1670.448855	239503.582061	37.097216
1672.033059	239906.563014	37.102234
1673.600444	240313.839190	37.107252
1675.440967	240713.044554	37.112269
1677.056892	241128.695000	37.117287
1679.105648	241528.323791	37.122304
1680.733144	241938.179160	37.127322
1682.361572	242348.363941	37.132340
1684.373115	242753.864693	37.137357
1685.854551	243157.034405	37.142375
1687.726033	243561.539535	37.147392
1689.395862	243986.245472	37.152410
1690.644947	244400.220173	37.157428
1692.639068	244808.793676	37.162445
1694.625577	245217.088141	37.167463
1696.294014	245631.756866	37.172480
1698.268406	246048.383672	37.177498
1699.948798	246455.631204	37.182516
1702.152657	246852.736514	37.187533
1703.885628	247260.736183	37.192551
1705.935128	247667.720126	37.197568
1707.997446	248066.394546	37.202586
1709.434586	248476.495392	37.207604
1711.546998	248869.241409	37.212621
1713.033852	249265.081900	37.217639
1714.923221	249663.347902	37.222656
1716.377626	250059.344023	37.227674
1717.862647	250473.623926	37.232692
1719.599240	250884.637341	37.237709
1721.186628	251303.776280	37.242727
1722.855089	251702.071842	37.247744
1724.573957	252115.370983	37.252762
1726.057404	252534.675260	37.257780
1727.574780	252942.745501	37.262797
1729.307668	253366.555305	37.267815
1730.915408	253786.217602	37.272832
1732.573431	254220.273444	37.277850
1734.017554	254629.366439	37.282868
1735.907844	255053.044982	37.287885
1737.890880	255479.222426	37.292903
1739.378227	255903.494805	37.297920
1740.947946	256337.176749	37.302938
1742.736506	256770.467404	37.307956
1744.369775	257192.909317	37.312973
1746.078267	257629.994348	37.317991
1748.232250	258044.198281	37.323008
1750.162183	258479.645452	37.328026
1751.924203	258907.446385	37.333044
1753.841183	259322.648322	37.338061
1755.135180	259738.098713	37.343079
1756.726450	260147.989262	37.348096
1758.210867	260554.694670	37.353114
1759.819904	260980.530845	37.358132
1761.429310	261397.018165	37.363149
1763.030707	261833.444156	37.368167
1764.124503	262252.320386	37.373184
1765.925170	262692.572595	37.378202
1767.506116	263141.899680	37.383220
1769.223639	263578.681555	37.388237
1770.574145	264034.771835	37.393255
1772.213217	264485.481130	37.398272
1774.036489	264960.212691	37.403290
1775.337262	265417.752451	37.408308
1776.894375	265879.059886	37.413325
1778.571219	266364.119788	37.418343
1780.089970	266842.572998	37.423360
1781.656567	267338.592216	37.428378
1783.345886	267827.325738	37.433396
1785.172656	268322.969007	37.438413
1786.581032	268828.250277	37.443431
1788.269257	269333.104063	37.448448
1790.482317	269837.669790	37.453466
1792.590444	270349.462127	37.458484
1794.334650	270863.060957	37.463501
1796.016264	271374.812620	37.468519
1797.732059	271892.143392	37.473536
1799.596579	272408.990688	37.478554
1801.214902	272941.975142	37.483572
1803.257025	273473.239169	37.488589
1804.811829	273998.049166	37.493607
1806.491395	274520.601458	37.498624
1808.758433	275058.601120	37.503642
1810.521141	275585.247871	37.508660
1812.653808	276114.601485	37.513677
1814.534289	276653.895467	37.518695
1816.357093	277186.693513	37.523712
1818.041702	277720.144463	37.528730
1819.932435	278258.511601	37.533748
1822.272936	278786.976662	37.538765
1824.897236	279314.606408	37.543783
1826.975265	279833.429756	37.548800
1829.063443	280351.892393	37.553818
1830.956698	280849.583820	37.558836
1833.548461	281359.986705	37.563853
1835.275200	281878.698276	37.568871
1837.203948	282382.061956	37.573888
1839.484048	282878.333038	37.578906
1841.080572	283383.950876	37.583924
1843.346995	283879.582215	37.588941
1845.519952	284381.496781	37.593959
1847.657987	284856.471137	37.598976
1850.553165	285321.699824	37.603994
1852.886567	285797.754344	37.609012
1855.313016	286247.738209	37.614029
1857.349601	286697.576912	37.619047
1859.440554	287134.707968	37.624064
1861.735457	287577.745947	37.629082
1863.452653	288015.386685	37.634100
1865.392098	288459.515365	37.639117
1866.903712	288890.301219	37.644135
1868.576436	289337.436383	37.649152
1870.385420	289779.291119	37.654170
1872.375057	290207.504936	37.659188
1874.109782	290630.195134	37.664205
1875.817697	291075.839800	37.669223
1877.535066	291518.610665	37.674240
1879.423651	291941.115511	37.679258
1881.045826	292371.123815	37.684276
1882.617102	292783.186371	37.689293
1883.403163	293214.690577	37.694311
1885.335434	293639.461830	37.699328
1887.501459	294072.851261	37.704346
1888.469880	294521.937708	37.709364
1890.143823	294957.555731	37.714381
1891.763026	295418.364768	37.719399
1893.294861	295888.323719	37.724416
1894.918673	296357.274310	37.729434
1896.563084	296839.546636	37.734452
1897.922587	297301.396770	37.739469
1899.608564	297799.191880	37.744487
1901.023683	298299.919144	37.749504
1902.527041	298799.764947	37.754522
1904.262929	299315.462158	37.759540
1906.106055	299830.782349	37.764557
1907.882903	300355.450315	37.769575
1909.056920	300895.693193	37.774592
1911.472203	301438.351207	37.779610
1912.617032	301988.589775	37.784628
1914.402882	302539.077750	37.789645
1916.445115	303097.973163	37.794663
1918.125620	303661.158509	37.799680
1919.954383	304232.767673	37.804698
1922.018543	304808.928261	37.809716
1924.012518	305381.057280	37.814733
1926.183134	305953.736062	37.819751
1927.825566	306537.482082	37.824768
1929.954696	307116.246192	37.829786
1931.637991	307715.658923	37.834804
1933.828966	308302.319014	37.839821
1935.879686	308889.273250	37.844839
1938.120351	309483.932226	37.849856
1940.111213	310075.221833	37.854874
1942.207804	310667.046019	37.859892
1944.523181	311248.701577	37.864909
1946.902217	311838.055802	37.869927
1948.714157	312414.978808	37.874944
1951.070271	313006.174730	37.879962
1953.265448	313598.352747	37.884980
1954.920529	314168.603632	37.889997
1957.335031	314751.342070	37.895015
1959.525637	315347.635023	37.900032
1961.737568	315919.071197	37.905050
1963.604329	316500.451621	37.910068
1965.874551	317074.376390	37.915085
1968.327821	317647.376887	37.920103
1970.131032	318209.787838	37.925120
1972.397429	318770.774130	37.930138
1974.434372	319343.842980	37.935156
1976.557224	319907.806114	37.940173
1978.463593	320473.470545	37.945191
1980.153901	321047.763626	37.950208
1981.882037	321613.060210	37.955226
1983.749631	322188.477376	37.960244
1985.649935	322767.738482	37.965261
1987.510567	323333.803191	37.970279
1989.889695	323913.810799	37.975296
1992.372391	324480.143126	37.980314
1993.732628	325044.689531	37.985332
1995.745476	325613.693129	37.990349
1998.274588	326183.419898	37.995367
2000.108954	326749.948956	38.000384
2002.187820	327322.064287	38.005402
2004.023957	327888.602330	38.010420
2006.482488	328461.276171	38.015437
2008.485750	329004.329311	38.020455
2010.598981	329549.894763	38.025472
2012.972239	330095.995421	38.030490
2014.562535	330634.346339	38.035508
2016.604752	331161.126799	38.040525
2018.922782	331702.317148	38.045543
2021.234971	332224.093845	38.050560
2023.214731	332749.593787	38.055578
2025.298347	333277.733813	38.060596
2027.388274	333802.821359	38.065613
2029.464176	334341.297580	38.070631
2031.283236	334867.731654	38.075648
2033.299512	335400.925604	38.080666
2035.256209	335942.111476	38.085684
2037.327560	336477.767110	38.090701
2039.387327	337018.033196	38.095719
2040.871131	337562.160751	38.100736
2042.596747	338120.370329	38.105754
2044.490175	338679.255212	38.110772
2046.281486	339244.640477	38.115789
2048.187311	339808.679987	38.120807
2049.794855	340382.471198	38.125824
2051.717956	340961.377674	38.130842
2053.520172	341552.289785	38.135860
2055.480545	342148.493116	38.140877
2057.254045	342747.581290	38.145895
2059.028540	343348.180595	38.150912
2061.649389	343952.288904	38.155930
2063.124985	344565.188088	38.160948
2065.262570	345178.555961	38.165965
2067.607584	345794.796572	38.170983
2069.426891	346418.969300	38.176000
2071.780468	347035.515527	38.181018
2073.887298	347665.604529	38.186036
2075.610055	348287.373865	38.191053
2078.292025	348915.624857	38.196071
2080.196627	349549.082038	38.201088
2082.255532	350170.053243	38.206106
2084.502188	350812.940729	38.211124
2086.688923	351437.214584	38.216141
2089.124277	352058.648508	38.221159
2091.548625	352700.431041	38.226176
2093.625374	353320.628882	38.231194
2095.539106	353950.905093	38.236212
2097.569283	354591.620923	38.241229
2099.675202	355219.433265	38.246247
2102.275814	355861.377551	38.251264
2104.157170	356476.955186	38.256282
2106.986202	357111.562298	38.261300
2109.671964	357722.831876	38.266317
2112.210118	358338.472400	38.271335
2114.366867	358950.712793	38.276352
2116.674472	359555.693086	38.281370
2118.708002	360159.918396	38.286388
2120.890838	360763.449213	38.291405
2123.378667	361371.837386	38.296423
2125.435931	361964.261889	38.301440
2127.525700	362572.256948	38.306458
2129.349783	363186.059726	38.311476
2131.234547	363792.845179	38.316493
2133.451589	364401.897736	38.321511
2135.127829	365018.827943	38.326528
2137.197216	365634.061620	38.331546
2139.471213	366259.260397	38.336564
2141.048894	366880.322486	38.341581
2143.031851	367502.296036	38.346599
2144.894858	368126.935573	38.351616
2147.007133	368746.707790	38.356634
2148.567383	369383.732961	38.361652
2150.857344	369988.575875	38.366669
2153.109982	370610.971076	38.371687
2154.656326	371232.626765	38.376704
2156.696751	371854.317960	38.381722
2158.270661	372486.734918	38.386740
2160.442069	373121.096128	38.391757
2162.692937	373752.491344	38.396775
2164.924612	374394.616975	38.401792
2166.979937	375029.205436	38.406810
2169.287436	375680.029154	38.411828
2171.113664	376325.136533	38.416845
2173.829540	376963.958797	38.421863
2175.685890	377611.285119	38.426880
2178.274811	378253.845499	38.431898
2181.015369	378913.692737	38.436916
2183.072854	379559.952160	38.441933
2185.349492	380204.515016	38.446951
2187.834573	380872.281179	38.451968
2189.931619	381513.217851	38.456986
2192.311691	382157.260365	38.462004
2194.722872	382821.442130	38.467021
2197.065493	383468.623629	38.472039
2199.206359	384121.771861	38.477056
2202.027463	384772.796310	38.482074
2204.369448	385420.586893	38.487092
2205.950342	386074.633606	38.492109
2208.607146	386723.557081	38.497127
2211.262694	387370.742073	38.502144
2213.724758	388022.068015	38.507162
2215.607732	388669.036355	38.512180
2218.051455	389300.859849	38.517197
2220.826324	389942.743255	38.522215
2222.624133	390603.397549	38.527232
2224.916071	391249.626591	38.532250
2227.388354	391890.442984	38.537268
2229.462812	392550.697529	38.542285
2231.082079	393194.347188	38.547303
2233.039450	393861.875351	38.552320
2234.910676	394524.993671	38.557338
2237.380571	395194.277896	38.562356
2239.057784	395876.425325	38.567373
2241.303120	396542.669153	38.572391
2243.269917	397240.982797	38.577408
2245.492755	397923.745212	38.582426
2247.559288	398610.713762	38.587444
2249.558896	399317.211727	38.592461
2252.137381	400010.639497	38.597479
2254.477674	400708.284952	38.602496
2256.809857	401406.619206	38.607514
2258.712828	402108.188041	38.612532
2260.938951	402825.526336	38.617549
2263.190597	403533.475192	38.622567
2265.768321	404243.577758	38.627584
2267.762305	404957.443666	38.632602
2270.225163	405666.912155	38.637620
2272.269864	406392.110814	38.642637
2274.570731	407104.190515	38.647655
2276.584498	407831.573720	38.652672
2279.140064	408554.345013	38.657690
2281.968044	409274.874355	38.662708
2284.429046	409978.943336	38.667725
2287.666597	410669.157244	38.672743
2290.302200	411360.455329	38.677760
2292.763676	412048.217315	38.682778
2295.164821	412752.711919	38.687796
2297.029635	413450.033407	38.692813
2299.359348	414132.842580	38.697831
2301.533230	414820.561037	38.702848
2304.133503	415492.813501	38.707866
2306.272860	416157.833131	38.712884
2308.319369	416839.588223	38.717901
2310.563169	417502.121430	38.722919
2312.355231	418176.286401	38.727936
2314.792278	418855.487411	38.732954
2317.276011	419530.663764	38.737972
2319.278547	420210.495473	38.742989
2321.747994	420886.641414	38.748007
2323.691804	421558.346898	38.753024
2325.749804	422255.700316	38.758042
2328.153199	422946.250914	38.763060
2329.897551	423659.887383	38.768077
2331.919028	424357.629886	38.773095
2334.688031	425052.248469	38.778112
2337.014668	425764.809783	38.783130
2339.814532	426477.625765	38.788148
2341.795451	427196.914342	38.793165
2344.047468	427916.741279	38.798183
2346.113619	428638.188905	38.803200
2348.908451	429366.573131	38.808218
2351.216576	430091.417861	38.813236
2353.401540	430819.035169	38.818253
2355.868014	431555.022152	38.823271
2358.250028	432285.738409	38.828288
2360.479356	433037.525951	38.833306
2363.028259	433776.195850	38.838324
2365.132460	434526.934488	38.843341
2367.585332	435274.001513	38.848359
2369.700930	436021.142783	38.853376
2371.982927	436773.686029	38.858394
2374.602291	437533.928010	38.863412
2376.499277	438307.490167	38.868429
2379.290766	439066.986960	38.873447
2381.838625	439832.604334	38.878464
2383.940033	440605.029903	38.883482
2386.456727	441370.690429	38.888500
2388.329191	442148.493352	38.893517
2390.751174	442933.754688	38.898535
2393.274568	443728.715401	38.903552
2395.512144	444518.736761	38.908570
2398.144224	445297.652124	38.913588
2400.425579	446094.770669	38.918605
2403.290078	446885.955483	38.923623
2405.858606	447668.213733	38.928640
2408.478433	448459.822704	38.933658
2411.311619	449246.263571	38.938676
2413.325570	450035.676292	38.943693
2415.720455	450828.175580	38.948711
2418.520691	451601.845048	38.953728
2420.811348	452398.279429	38.958746
2423.706010	453181.003352	38.963764
2426.149784	453967.094918	38.968781
2428.751109	454752.117149	38.973799
2431.218442	455529.402178	38.978816
2434.022711	456312.000777	38.983834
2436.959581	457081.016761	38.988852
2439.229837	457845.913883	38.993869
2441.698041	458620.032407	38.998887
2444.697985	459388.935930	39.003904
2446.763355	460150.078864	39.008922
2449.638855	460907.831718	39.013940
2451.739031	461684.493535	39.018957
2454.061005	462444.383930	39.023975
2456.853282	463212.693566	39.028992
2458.590576	463992.737347	39.034010
2461.021795	464746.856451	39.039028
2463.224080	465512.176918	39.044045
2465.705987	466259.611354	39.049063
2468.204084	466999.897245	39.054080
2470.585417	467739.563143	39.059098
2473.885747	468459.582868	39.064116
2476.388004	469201.333377	39.069133
2479.203585	469933.318065	39.074151
2481.523101	470667.667586	39.079168
2483.529819	471398.704712	39.084186
2486.767436	472117.111362	39.089204
2489.142451	472842.176504	39.094221
2491.461388	473573.621748	39.099239
2494.209528	474303.907936	39.104256
2496.572793	475051.817316	39.109274
2498.982675	475789.853439	39.114292
2501.292926	476532.005087	39.119309
2503.864607	477273.678072	39.124327
2505.762964	478034.577307	39.129344
2507.958092	478790.252175	39.134362
2510.364829	479547.924443	39.139380
2512.732739	480319.981331	39.144397
2515.098918	481084.289486	39.149415
2517.740406	481863.787585	39.154432
2520.180962	482659.102056	39.159450
2522.262738	483445.764660	39.164468
2524.935060	484241.919394	39.169485
2526.969399	485049.822648	39.174503
2529.523513	485854.327359	39.179520
2531.954376	486662.436718	39.184538
2534.626531	487481.800928	39.189556
2537.040296	488306.904466	39.194573
2539.394950	489135.750539	39.199591
2542.041403	489961.634617	39.204608
2544.374091	490797.243641	39.209626
2546.457169	491634.003807	39.214644
2548.795136	492486.088300	39.219661
2551.602243	493337.245223	39.224679
2554.488792	494189.297976	39.229696
2557.101280	495046.279438	39.234714
2559.897220	495901.823247	39.239732
2562.893178	496765.341860	39.244749
2565.355014	497620.989327	39.249767
2567.994433	498467.850090	39.254784
2569.957890	499321.412300	39.259802
2573.471290	500180.672135	39.264820
2576.073529	501040.527036	39.269837
2578.589610	501888.768581	39.274855
2581.410870	502749.947252	39.279872
2583.690931	503606.881567	39.284890
2586.693564	504469.187022	39.289908
2589.464218	505328.558378	39.294925
2591.798198	506186.386512	39.299943
2594.934744	507038.100614	39.304960
2597.630733	507891.693862	39.309978
2600.021557	508748.050087	39.314996
2602.853260	509614.245205	39.320013
2605.303538	510468.173492	39.325031
2607.982352	511330.413438	39.330048
2610.396989	512188.064741	39.335066
2613.150763	513037.714580	39.340084
2616.009164	513898.711157	39.345101
2618.846198	514757.394674	39.350119
2621.545890	515599.151819	39.355136
2624.360290	516460.749422	39.360154
2626.853689	517309.824672	39.365172
2629.496827	518146.004492	39.370189
2632.714617	518985.964012	39.375207
2635.399009	519817.962786	39.380224
2638.502276	520633.660465	39.385242
2641.131304	521445.462774	39.390260
2643.550642	522238.252046	39.395277
2645.845953	523038.652368	39.400295
2649.000504	523834.649407	39.405312
2651.300405	524640.782054	39.410330
2653.572618	525439.836002	39.415348
2655.452154	526252.367865	39.420365
2657.816790	527082.909884	39.425383
2659.880453	527904.153242	39.430400
2662.230617	528749.009863	39.435418
2664.468438	529606.738313	39.440436
2666.492126	530462.083420	39.445453
2668.554115	531330.323628	39.450471
2671.141702	532209.471677	39.455488
2673.763939	533105.376634	39.460506
2676.179361	533997.285114	39.465524
2679.002422	534902.473573	39.470541
2680.928038	535808.441429	39.475559
2683.964584	536714.974652	39.480576
2686.887565	537638.578436	39.485594
2689.587291	538568.474442	39.490612
2691.983666	539498.951981	39.495629
2694.787938	540432.709897	39.500647
2697.692482	541374.462284	39.505664
2700.378047	542321.748124	39.510682
2702.698414	543271.678677	39.515700
2705.535838	544227.225733	39.520717
2708.205318	545196.521574	39.525735
2711.078795	546164.405531	39.530752
2713.178730	547125.563224	39.535770
2715.748887	548116.565172	39.540788
2718.534369	549103.491583	39.545805
2721.190524	550103.346725	39.550823
2724.006525	551094.570694	39.555840
2726.979353	552086.692150	39.560858
2729.805419	553071.886944	39.565876
2732.897058	554068.088882	39.570893
2735.725828	555070.665727	39.575911
2739.241024	556054.807065	39.580928
2742.094287	557046.839538	39.585946
2745.216729	558042.706443	39.590964
2748.490936	559018.372250	39.595981
2751.551680	559990.183129	39.600999
2754.726507	560968.509670	39.606016
2757.252463	561945.854516	39.611034
2759.881310	562918.192848	39.616052
2762.944898	563886.475535	39.621069
2765.989058	564857.235288	39.626087
2769.310343	565817.754447	39.631104
2772.155752	566779.620586	39.636122
2775.218800	567734.663031	39.641140
2778.234601	568688.732567	39.646157
2780.717484	569640.002711	39.651175
2784.173958	570588.789005	39.656192
2786.525432	571537.168802	39.661210
2789.560958	572492.169770	39.666228
2792.215580	573433.987589	39.671245
2795.075618	574376.946113	39.676263
2798.248844	575321.027961	39.681280
2800.540936	576271.272760	39.686298
2803.061368	577208.093338	39.691316
2805.827158	578158.304380	39.696333
2808.403435	579112.215906	39.701351
2810.736868	580062.632492	39.706368
2813.302947	581038.838425	39.711386
2816.223296	582002.700686	39.716404
2819.349762	582962.896239	39.721421
2821.897496	583916.098487	39.726439
2824.851108	584855.455565	39.731456
2827.122520	585780.041108	39.736474
2829.285392	586716.662366	39.741492
2832.546954	587655.730358	39.746509
2834.969952	588603.294703	39.751527
2837.157058	589555.110833	39.756544
2839.862369	590517.055885	39.761562
2842.447736	591483.430656	39.766580
2845.180488	592446.298033	39.771597
2847.774591	593427.534483	39.776615
2850.475423	594419.653480	39.781632
2853.339154	595415.500465	39.786650
2855.972538	596421.877839	39.791668
2858.969841	597416.766717	39.796685
2862.076094	598422.480082	39.801703
2864.892776	599427.643290	39.806720
2868.029016	600449.234791	39.811738
2870.354441	601464.363873	39.816756
2873.821404	602479.315471	39.821773
2876.136608	603508.971352	39.826791
2878.849407	604559.821607	39.831808
2881.722005	605594.572472	39.836826
2884.683126	606641.030386	39.841844
2887.718197	607692.708223	39.846861
2890.201615	608751.497668	39.851879
2893.563565	609806.897660	39.856896
2896.394789	610874.490115	39.861914
2899.151530	611940.735260	39.866932
2902.559019	613001.929671	39.871949
2905.297401	614079.021539	39.876967
2908.727482	615136.148615	39.881984
2911.877387	616203.376787	39.887002
2915.212821	617275.296658	39.892020
2918.183583	618323.685591	39.897037
2921.144470	619404.106279	39.902055
2923.980660	620471.424341	39.907072
2926.194446	621554.965713	39.912090
2928.943321	622622.313910	39.917108
2932.470897	623693.259680	39.922125
2935.552315	624798.373010	39.927143
2938.231220	625875.537528	39.932160
2940.826165	626968.529534	39.937178
2943.757550	628066.175191	39.942196
2947.092315	629150.292022	39.947213
2950.179119	630252.145391	39.952231
2953.041029	631353.410054	39.957248
2956.379555	632441.684469	39.962266
2958.995903	633540.297687	39.967284
2962.254179	634632.763451	39.972301
2966.270781	635720.308925	39.977319
2969.480500	636813.625750	39.982336
2972.468055	637898.246659	39.987354
2975.244056	638985.113139	39.992372
2978.000385	640069.669174	39.997389
2980.599289	641170.829582	40.002407
2983.295954	642252.258365	40.007424
2986.160952	643361.569721	40.012442
2989.244901	644465.396455	40.017460
2992.037387	645568.590593	40.022477
2994.694178	646670.133852	40.027495
2997.699101	647782.719199	40.032512
3000.933545	648897.418983	40.037530
3004.003695	650015.485677	40.042548
3006.653414	651127.223480	40.047565
3009.317670	652249.996363	40.052583
3012.180029	653388.140489	40.057600
3015.617548	654520.938045	40.062618
3018.371652	655621.781965	40.067636
3021.860840	656712.399910	40.072653
3024.756034	657809.677877	40.077671
3027.829266	658891.162653	40.082688
3030.893792	659956.243774	40.087706
3034.162423	661036.941368	40.092724
3037.652290	662102.492444	40.097741
3041.007891	663176.566185	40.102759
3043.808794	664247.322876	40.107776
3047.246973	665325.287494	40.112794
3050.071829	666401.430742	40.117812
3052.994641	667481.887975	40.122829
3056.100971	668558.266976	40.127847
3058.601931	669647.295166	40.132864
3061.890984	670741.316351	40.137882
3064.864961	671826.032525	40.142900
3068.600848	672919.460452	40.147917
3071.383681	674029.047227	40.152935
3074.846969	675137.988004	40.157952
3077.281805	676229.315738	40.162970
3079.998230	677340.613322	40.167988
3083.221306	678456.043588	40.173005
3086.016765	679581.789978	40.178023
3088.808453	680716.049311	40.183040
3091.723746	681859.936077	40.188058
3094.092542	683003.802413	40.193076
3097.396129	684167.652287	40.198093
3100.429108	685334.103549	40.203111
3103.314136	686493.688051	40.208128
3106.263421	687678.917030	40.213146
3109.296539	688869.798669	40.218164
3112.033390	690051.013079	40.223181
3114.838117	691254.985498	40.228199
3118.154255	692472.047202	40.233216
3121.063771	693680.788282	40.238234
3123.919490	694913.670173	40.243252
3127.429702	696139.890190	40.248269
3130.116689	697377.069692	40.253287
3133.084224	698619.943409	40.258304
3136.222854	699848.920436	40.263322
3139.362015	701111.778597	40.268340
3142.545230	702365.002383	40.273357
3145.785744	703630.854604	40.278375
3148.916691	704897.461069	40.283392
3152.559264	706156.039222	40.288410
3155.426290	707432.743985	40.293428
3158.657175	708699.221841	40.298445
3161.569279	709973.930697	40.303463
3165.297627	711269.608104	40.308480
3168.202373	712543.605395	40.313498
3171.292375	713823.331013	40.318516
3174.536993	715109.131267	40.323533
3177.895969	716395.341658	40.328551
3181.130369	717672.243002	40.333568
3184.706262	718960.259729	40.338586
3187.857843	720248.078253	40.343604
3191.470278	721531.225960	40.348621
3195.148345	722818.235218	40.353639
3197.973620	724091.179662	40.358656
3201.728572	725365.784083	40.363674
3205.132714	726632.453657	40.368692
3208.070768	727895.293783	40.373709
3211.293746	729164.027727	40.378727
3214.457986	730441.509307	40.383744
3217.769038	731726.816019	40.388762
3220.517612	732992.862124	40.393780
3224.282560	734260.697715	40.398797
3227.422746	735527.579265	40.403815
3230.429058	736794.953448	40.408832
3233.632223	738032.793333	40.413850
3236.403173	739272.065226	40.418868
3239.440832	740505.830617	40.423885
3242.976181	741741.619023	40.428903
3245.337259	742980.475844	40.433920
3248.782320	744223.764323	40.438938
3251.650193	745479.644412	40.443956
3254.584065	746739.517623	40.448973
3257.531427	748007.364189	40.453991
3260.425337	749281.178142	40.459008
3264.112595	750570.339683	40.464026
3267.068059	751850.212470	40.469044
3270.021008	753148.294176	40.474061
3273.893067	754451.584988	40.479079
3277.209025	755756.537478	40.484096
3280.534892	757054.877043	40.489114
3283.444479	758354.807232	40.494132
3286.822244	759668.092998	40.499149
3290.270490	760996.502607	40.504167
3293.161211	762324.943458	40.509184
3297.167940	763640.520691	40.514202
3300.596557	764962.450724	40.519220
3304.222795	766294.425603	40.524237
3307.240013	767631.769217	40.529255
3310.906589	768973.106765	40.534272
3314.215436	770304.260123	40.539290
3317.289561	771650.157506	40.544308
3320.384926	772988.550304	40.549325
3324.253554	774342.888163	40.554343
3327.028303	775698.007341	40.559360
3330.254396	777061.141793	40.564378
3334.075535	778421.172631	40.569396
3336.929719	779785.086006	40.574413
3340.124138	781151.844188	40.579431
3343.597856	782543.133608	40.584448
3346.805844	783924.850994	40.589466
3349.906158	785319.867405	40.594484
3353.176295	786708.269756	40.599501
3356.698062	788099.025271	40.604519
3359.951540	789493.139552	40.609536
3363.797185	790897.936287	40.614554
3366.652073	792311.217290	40.619572
3370.071399	793720.059333	40.624589
3373.850594	795131.855176	40.629607
3377.346746	796539.881019	40.634624
3380.951399	797942.859318	40.639642
3384.468814	799357.479398	40.644660
3387.959371	800769.310306	40.649677
3391.461471	802170.411783	40.654695
3394.835544	803585.390552	40.659712
3398.016879	804996.339646	40.664730
3401.304912	806418.052005	40.669748
3404.674903	807828.538711	40.674765
3408.585707	809244.608315	40.679783
3411.916885	810666.771482	40.684800
3415.131939	812068.509159	40.689818
3418.948960	813488.694950	40.694836
3422.053079	814912.071173	40.699853
3425.787937	816339.978983	40.704871
3428.739544	817764.379747	40.709888
3432.130780	819180.617113	40.714906
3436.011009	820605.094194	40.719924
3439.062503	822035.001463	40.724941
3442.644873	823453.917041	40.729959
3445.874705	824893.611181	40.734976
3449.236009	826334.691963	40.739994
3452.687475	827759.516098	40.745012
3456.140818	829169.486993	40.750016
3459.855822	830538.170252	40.755021
3462.760405	831868.588901	40.760026
3466.235426	833136.172726	40.765031
3469.556228	834346.900287	40.770036
3472.357265	835490.473918	40.775040
3475.380036	836575.357888	40.780045
3478.430376	837598.217055	40.785050
3481.247894	838543.015076	40.790055
3483.953867	839430.339130	40.795060
3486.815449	840253.091084	40.800064
3490.148911	840995.146256	40.805069
3492.231053	841697.345175	40.810074
3494.565809	842325.427864	40.815079
3496.779122	842894.797295	40.820084
3498.712815	843417.518110	40.825088
3500.583624	843878.929061	40.830093
3502.124792	844289.653249	40.835098
3503.879099	844642.249030	40.840103
3505.344294	844971.507807	40.845108
3506.549353	845258.818586	40.850112
3508.178350	845500.106650	40.855117
3508.727969	845714.124731	40.860122
3509.807616	845875.425353	40.865127
3511.132483	846007.995886	40.870132
3512.067697	846121.532107	40.875136
3512.885689	846201.067858	40.880141
3513.702386	846252.594999	40.885146
3514.525413	846273.981005	40.890151
3514.908165	846288.361169	40.895156
3515.925094	846270.854954	40.900160
3516.492344	846225.798776	40.905165
3516.659497	846175.571439	40.910170
3516.856294	846092.290968	40.915175
3517.074120	846002.803349	40.920180
3517.242148	845912.352968	40.925184
3517.783079	845797.515956	40.930189
3517.825477	845674.128550	40.935194
3518.246084	845533.233017	40.940199
3518.333786	845386.570524	40.945204
3518.764363	845250.222221	40.950208
3519.135180	845070.745389	40.955213
3518.518579	844902.080299	40.960218
3519.211266	844715.466048	40.965223
3519.365157	844531.741403	40.970228
3519.321065	844346.103087	40.975232
3519.254160	844132.638547	40.980237
3518.981914	843939.848950	40.985242
3519.434282	843720.568200	40.990247
3519.487211	843520.151585	40.995252
3519.111268	843299.530292	41.000256
3519.453844	843077.721811	41.005261
3519.167455	842862.500219	41.010266
3519.233541	842636.645706	41.015271
3518.921365	842423.157632	41.020276
3518.880572	842195.945318	41.025280
3518.865190	841964.259068	41.030285
3518.760138	841746.640881	41.035290
3518.838096	841516.280315	41.040295
3519.064190	841284.335719	41.045300
3518.464852	841062.792885	41.050304
3518.596399	840816.198007	41.055309
3518.624385	840589.592307	41.060314
3518.342556	840364.384514	41.065319
3518.477478	840129.401694	41.070324
3518.021766	839890.815247	41.075328
3518.297159	839662.583206	41.080333
3518.095263	839428.789574	41.085338
3517.941808	839190.806942	41.090343
3517.757269	838960.776313	41.095348
3517.910437	838724.279608	41.100352
3517.633153	838480.368701	41.105357
3517.708213	838253.181361	41.110362
3517.564698	838024.175622	41.115367
3517.450574	837781.860428	41.120372
3517.110549	837552.382030	41.125376
3517.198701	837335.736723	41.130381
3516.903722	837105.360564	41.135386
3516.799339	836873.295595	41.140391
3516.920297	836653.999642	41.145396
3516.279762	836430.931739	41.150400
3516.348500	836210.268646	41.155405
3515.985096	835991.703665	41.160410
3516.102812	835764.900408	41.165415
3515.822156	835553.102385	41.170420
3515.574975	835332.941785	41.175424
3515.629695	835117.580652	41.180429
3515.256796	834914.513016	41.185434
3514.957112	834698.803854	41.190439
3515.063243	834482.926395	41.195444
3514.942261	834290.188498	41.200448
3515.140223	834083.022054	41.205453
3514.504122	833875.590391	41.210458
3514.201353	833678.296878	41.215463
3514.303813	833473.260953	41.220468
3513.773249	833278.612216	41.225472
3514.217833	833077.491438	41.230477
3513.809949	832901.556981	41.235482
3513.457889	832712.787014	41.240487
3513.455914	832519.876661	41.245492
3513.530461	832339.187797	41.250496
3513.351460	832148.818880	41.255501
3513.135685	831967.289974	41.260506
3513.358804	831779.760927	41.265511
3512.998067	831600.478072	41.270516
3512.524720	831415.572529	41.275520
3512.692075	831246.009210	41.280525
3512.221067	831073.043161	41.285530
3512.448911	830891.801226	41.290535
3512.451192	830721.860365	41.295540
3512.083136	830553.721654	41.300544
3511.981604	830377.179881	41.305549
3511.806908	830221.050933	41.310554
3511.699113	830051.788685	41.315559
3511.585976	829887.964578	41.320564
3511.419935	829725.018949	41.325568
3511.627879	829552.972325	41.330573
3511.321490	829400.535835	41.335578
3510.954378	829240.135469	41.340583
3511.218096	829087.699191	41.345588
3510.871101	828929.036913	41.350592
3510.732035	828778.599729	41.355597
3510.687800	828632.615163	41.360602
3510.882394	828479.396834	41.365607
3510.534240	828330.050448	41.370612
3510.301174	828190.111423	41.375616
3510.444616	828043.014092	41.380621
3510.149808	827901.522739	41.385626
3509.831539	827755.365527	41.390631
3509.653620	827617.057325	41.395636
3509.960004	827485.961597	41.400640
3509.969369	827342.951448	41.405645
3509.565842	827214.294125	41.410650
3509.354071	827071.992738	41.415655
3509.159106	826939.796943	41.420660
3509.112310	826820.798169	41.425664
3509.311822	826693.591237	41.430669
3508.769556	826567.858860	41.435674
3508.789953	826443.883385	41.440679
3508.824048	826323.987168	41.445684
3508.519875	826211.726036	41.450688
3508.797172	826080.215697	41.455693
3508.475950	825969.703100	41.460698
3508.114610	825839.746041	41.465703
3508.344148	825725.058682	41.470708
3508.480650	825621.567164	41.475712
3508.336122	825505.669950	41.480717
3508.364731	825397.620798	41.485722
3508.062660	825280.285176	41.490727
3508.063197	825162.802745	41.495732
3507.983812	825060.016258	41.500736
3507.563550	824941.233765	41.505741
3507.321517	824847.222351	41.510746
3507.485327	824745.073377	41.515751
3507.242572	824642.013625	41.520756
3507.318449	824548.726037	41.525760
3507.426982	824439.966640	41.530765
3507.274245	824342.237405	41.535770
3507.042614	824247.534287	41.540775
3507.373011	824142.722969	41.545780
3507.146967	824050.836792	41.550784
3506.880267	823949.325490	41.555789
3506.789718	823851.384162	41.560794
3507.184578	823754.921823	41.565799
3506.942501	823670.620051	41.570804
3506.573054	823576.122666	41.575808
3506.509412	823490.817733	41.580813
3506.410792	823408.143709	41.585818
3506.187770	823311.090010	41.590823
3505.990296	823222.397330	41.595828
3506.018370	823145.147938	41.600832
3506.447038	823059.760062	41.605837
3506.684292	822989.967190	41.610842
3506.335839	822895.456047	41.615847
3506.385199	822808.859205	41.620852
3505.768868	822729.856782	41.625856
3506.208711	822646.601875	41.630861
3506.076764	822572.872910	41.635866
3506.072202	822489.198866	41.640871
3505.567414	822408.326230	41.645876
3505.879390	822334.233116	41.650880
3505.661468	822249.713473	41.655885
3505.465297	822183.773938	41.660890
3505.367222	822099.136191	41.665895
3505.531954	822025.743506	41.670900
3505.494103	821962.306762	41.675904
3505.868071	821884.890174	41.680909
3505.452369	821820.829893	41.685914
3505.047317	821745.966023	41.690919
3505.395478	821682.563366	41.695924
3505.373959	821609.194836	41.700928
3505.570225	821532.190843	41.705933
3505.454990	821467.009480	41.710938
3505.437741	821401.714796	41.715943
3505.555557	821318.978868	41.720948
3505.066464	821246.068370	41.725952
3505.166547	821166.447299	41.730957
3504.792570	821115.121781	41.735962
3504.835363	821053.901412	41.740967
3504.672374	820993.296527	41.745972
3504.776526	820929.145711	41.750976
3505.001633	820872.274511	41.755981
3504.612313	820814.038985	41.760986
3504.585742	820747.278982	41.765991
3504.872885	820691.369665	41.770996
3504.583792	820624.162742	41.776000
3504.405303	820570.952934	41.781005
3504.340736	820512.858455	41.786010
3504.630839	820460.645057	41.791015
3504.512492	820406.937790	41.796020
3504.444859	820354.974081	41.801024
3503.951586	820294.803292	41.806029
3504.275592	820249.104021	41.811034
3504.000243	820190.260799	41.816039
3504.006110	820140.814463	41.821044
3504.351488	820097.836086	41.826048
3504.177048	820029.534088	41.831053
3504.113445	819981.752048	41.836058
3504.081763	819930.460506	41.841063
3504.228559	819879.822006	41.846068
3504.139307	819831.750801	41.851072
3504.082359	819786.399683	41.856077
3503.898481	819733.475526	41.861082
3503.999948	819688.682970	41.866087
3503.974287	819640.210972	41.871092
3503.411498	819585.300598	41.876096
3503.777473	819543.969986	41.881101
3503.695453	819504.169289	41.886106
3503.931390	819456.239022	41.891111
3504.014448	819409.792466	41.896116
3503.491295	819359.546473	41.901120
3503.689731	819310.550133	41.906125
3503.401388	819280.320254	41.911130
3503.527396	819228.414159	41.916135
3503.588346	819187.712944	41.921140
3503.573023	819150.917368	41.926144
3503.639653	819113.719363	41.931149
3503.515746	819086.870089	41.936154
3503.551879	819039.843992	41.941159
3503.534964	818993.117886	41.946164
3503.601108	818956.016362	41.951168
3503.426160	818915.837000	41.956173
3503.422116	818871.347089	41.961178
3503.229875	818830.780463	41.966183
3503.577052	818789.447763	41.971188
3503.331915	818742.755445	41.976192
3503.441004	818705.450998	41.981197
3503.389107	818664.861347	41.986202
3503.468364	818632.136909	41.991207
3503.462864	818587.061040	41.996212
3502.993966	818548.969776	42.001216
3502.910545	818505.852677	42.006221
3503.070774	818480.806195	42.011226
3503.261947	818456.825741	42.016231
3503.310319	818415.050456	42.021236
3503.174330	818377.392902	42.026240
3503.020999	818339.445744	42.031245
3503.119398	818305.158792	42.036250
3502.926469	818273.838093	42.041255
3503.075776	818241.782190	42.046260
3503.113016	818207.406896	42.051264
3502.905854	818175.698468	42.056269
3503.043940	818143.351717	42.061274
3502.490023	818113.547118	42.066279
3502.832925	818072.891880	42.071284
3502.863840	818047.669133	42.076288
3502.886216	818011.542474	42.081293
3502.680498	817992.685376	42.086298
3502.914871	817956.622625	42.091303
3503.128499	817922.705024	42.096308
3502.508422	817890.572841	42.101312
3502.869676	817860.429227	42.106317
3502.702965	817842.247162	42.111322
3502.900754	817811.155161	42.116327
3502.808333	817781.666307	42.121332
3502.798636	817756.351355	42.126336
3502.885621	817722.160342	42.131341
3502.536606	817695.242859	42.136346
3502.486886	817666.038898	42.141351
3502.729122	817636.107548	42.146356
3502.901685	817616.995429	42.151360
3503.041288	817576.368726	42.156365
3502.717540	817544.383174	42.161370
3502.566230	817526.003027	42.166375
3502.724191	817489.754764	42.171380
3502.296139	817463.530260	42.176384
3502.594134	817441.866218	42.181389
3502.369540	817406.553659	42.186394
3502.372909	817383.085306	42.191399
3502.460658	817360.480073	42.196404
3502.080744	817338.532132	42.201408
3502.169610	817316.316076	42.206413
3502.225342	817297.415995	42.211418
3502.061986	817278.647483	42.216423
3502.359935	817254.450943	42.221428
3502.342648	817239.944170	42.226432
3502.585165	817219.943480	42.231437
3502.603933	817198.030100	42.236442
3502.336675	817172.850414	42.241447
3502.671409	817139.786039	42.246452
3502.435481	817117.522665	42.251456
3502.218991	817090.484461	42.256461
3502.209141	817072.470386	42.261466
3502.011201	817051.174657	42.266471
3502.224913	817029.327591	42.271476
3501.912614	817012.918747	42.276480
3502.072841	816991.372058	42.281485
3502.104220	816985.329436	42.286490
3502.053829	816949.597515	42.291495
3502.311693	816932.125489	42.296500
3501.921618	816918.260546	42.301504
3502.108414	816899.533538	42.306509
3502.362392	816881.964594	42.311514
3501.649468	816866.786611	42.316519
3501.939300	816846.582557	42.321524
3501.902859	816844.153669	42.326528
3501.859652	816813.289128	42.331533
3501.907355	816806.075146	42.336538
3502.095756	816785.886750	42.341543
3502.057982	816761.643392	42.346548
3502.142457	816756.079183	42.351552
3502.102029	816717.033207	42.356557
3502.252676	816704.154524	42.361562
3502.174171	816698.420965	42.366567
3502.066269	816659.677341	42.371572
3502.067087	816657.924277	42.376576
3502.368435	816635.672578	42.381581
3502.087080	816619.452635	42.386586
3502.258865	816601.895751	42.391591
3502.283035	816572.675106	42.396596
3502.114878	816547.769567	42.401600
3502.321688	816530.109616	42.406605
3502.235237	816507.041563	42.411610
3502.101413	816492.161700	42.416615
3502.116496	816465.376752	42.421620
3502.046596	816454.674647	42.426624
3502.316233	816424.148840	42.431629
3502.198143	816413.648982	42.436634
3502.045046	816389.227416	42.441639
3502.455253	816370.463897	42.446644
3502.140466	816363.403460	42.451648
3502.119844	816336.331360	42.456653
3502.283219	816323.352508	42.461658
3502.071541	816295.433551	42.466663
3502.220645	816274.275701	42.471668
3501.775547	816248.048728	42.476672
3502.262066	816233.168669	42.481677
3501.878750	816214.528725	42.486682
3501.810074	816196.131728	42.491687
3501.873371	816188.330218	42.496692
3501.792015	816171.688259	42.501696
3501.977589	816158.900388	42.506701
3501.685935	816144.920934	42.511706
3501.569253	816135.102162	42.516711
3502.192379	816115.428023	42.521716
3501.798765	816097.276323	42.526720
3502.005038	816080.686555	42.531725
3501.636493	816060.485477	42.536730
3501.766936	816044.297059	42.541735
3501.990874	816042.216749	42.546740
3501.508502	816028.461643	42.551744
3501.965679	816013.683048	42.556749
3502.099158	816016.779000	42.561754
3501.785941	815997.835252	42.566759
3502.001746	815973.549187	42.571764
3501.604491	815953.936648	42.576768
3501.573651	815941.182161	42.581773
3501.643694	815938.249275	42.586778
3501.722992	815915.932322	42.591783
3501.998876	815901.766204	42.596788
3502.027248	815892.119175	42.601792
3501.721020	815878.433602	42.606797
3501.264489	815867.206520	42.611802
3501.410821	815848.093079	42.616807
3501.481546	815843.796423	42.621812
3501.322457	815833.983805	42.626816
3501.457997	815820.716056	42.631821
3501.488205	815818.763358	42.636826
3501.450805	815807.762855	42.641831
3501.709043	815801.781026	42.646836
3501.487949	815806.685746	42.651840
3501.526105	815781.842294	42.656845
3501.474082	815771.233622	42.661850
3501.389685	815777.285826	42.666855
3501.720716	815753.370503	42.671860
3501.927665	815740.675838	42.676864
3501.918682	815730.547383	42.681869
3501.740854	815710.997180	42.686874
3501.406988	815695.757070	42.691879
3501.738141	815689.958543	42.696884
3501.489480	815675.679103	42.701888
3501.413707	815661.859624	42.706893
3501.755830	815662.975053	42.711898
3501.545153	815651.416936	42.716903
3501.919611	815629.832057	42.721908
3501.384126	815629.623609	42.726912
3501.510378	815624.441481	42.731917
3501.461521	815607.500720	42.736922
3501.627771	815587.896344	42.741927
3501.969264	815587.648210	42.746932
3501.385472	815566.894745	42.751936
3501.593733	815554.199496	42.756941
3501.653866	815551.852413	42.761946
3501.325151	815535.052610	42.766951
3501.648595	815518.443034	42.771956
3501.627504	815517.667139	42.776960
3501.533218	815507.649063	42.781965
3501.722775	815495.638466	42.786970
3501.472032	815475.904109	42.791975
3501.365890	815468.615223	42.796980
3501.576715	815463.030112	42.801985
3501.319701	815447.095528	42.806989
3501.753591	815445.664056	42.811994
3501.471392	815446.000451	42.816999
3501.711437	815422.195492	42.822004
3501.343117	815417.285320	42.827009
3501.708518	815411.188959	42.832013
3501.704584	815403.202163	42.837018
3501.451749	815385.903053	42.842023
3501.532247	815375.175583	42.847028
3501.452381	815371.291779	42.852033
3501.260618	815347.261809	42.857037
3501.661377	815346.517358	42.862042
3501.481930	815338.947551	42.867047
3501.490331	815334.270652	42.872052
3501.031271	815326.354902	42.877057
3500.949825	815305.522037	42.882061
3501.406676	815314.996831	42.887066
3501.343854	815316.370445	42.892071
3501.586208	815309.806173	42.897076
3501.391841	815307.596192	42.902081
3501.328123	815288.026824	42.907085
3501.196032	815287.170842	42.912090
3501.538114	815282.246922	42.917095
3501.386316	815269.217739	42.922100
3501.229425	815250.636922	42.927105
3501.377731	815245.061390	42.932109
3501.397387	815251.097838	42.937114
3501.021533	815249.013617	42.942119
3501.573918	815237.043216	42.947124
3501.497568	815219.131591	42.952129
3501.070698	815224.653399	42.957133
3501.510277	815218.837490	42.962138
3501.307110	815221.986463	42.967143
3501.624585	815200.701245	42.972148
3501.235471	815198.034611	42.977153
3501.457332	815186.115781	42.982157
3501.566611	815194.768387	42.987162
3501.471654	815178.223314	42.992167
3501.913442	815155.749569	42.997172
3501.574604	815153.951765	43.002177
3501.645259	815129.685112	43.007181
3501.613097	815124.819571	43.012186
3501.645784	815122.281793	43.017191
3501.817183	815102.869917	43.022196
3501.840691	815098.580131	43.027201
3501.670932	815076.006872	43.032205
3501.729820	815060.411571	43.037210
3501.561496	815055.080193	43.042215
3501.712582	815041.321291	43.047220
3501.487674	815028.497862	43.052225
3501.248781	815012.169677	43.057229
3501.421171	815014.383318	43.062234
3501.013529	815026.039391	43.067239
3501.623399	815001.395708	43.072244
3501.683293	814996.028604	43.077249
3501.482573	814986.415988	43.082253
3501.474078	814974.435350	43.087258
3501.567410	814957.275768	43.092263
3501.624401	814943.726192	43.097268
3501.332087	814952.052250	43.102273
3501.317420	814941.923404	43.107277
3501.287850	814924.880361	43.112282
3501.456502	814924.951472	43.117287
3501.467291	814914.623772	43.122292
3501.081812	814917.801397	43.127297
3501.269554	814919.038513	43.132301
3501.611463	814898.722607	43.137306
3501.246114	814887.869164	43.142311
3501.539862	814882.562824	43.147316
3501.583919	814877.392926	43.152321
3501.364700	814861.061270	43.157325
3501.328273	814849.864094	43.162330
3501.285218	814853.670140	43.167335
3501.375371	814851.610353	43.172340
3501.217698	814837.217351	43.177345
3501.160731	814819.886053	43.182349
3501.527338	814819.244300	43.187354
3501.181584	814831.280730	43.192359
3501.454791	814819.840263	43.197364
3501.326262	814807.488399	43.202369
3501.258552	814795.029587	43.207373
3501.571636	814787.771789	43.212378
3501.215458	814784.807572	43.217383
3501.800329	814782.183339	43.222388
3501.774498	814766.405712	43.227393
3501.662526	814759.409163	43.232397
3501.605654	814742.759564	43.237402
3501.613971	814728.632619	43.242407
3501.432291	814721.159829	43.247412
3501.389824	814721.166527	43.252417
3501.126351	814705.036218	43.257421
3501.387712	814689.310922	43.262426
3501.509339	814690.753259	43.267431
3501.169252	814679.213567	43.272436
3501.304325	814687.862844	43.277441
3501.316467	814682.697775	43.282445
3501.347186	814663.111687	43.287450
3500.952438	814659.471501	43.292455
3501.271644	814651.335810	43.297460
3501.218688	814648.713808	43.302465
3501.342976	814657.949332	43.307469
3501.399973	814640.015201	43.312474
3501.367391	814623.751169	43.317479
3501.394781	814622.188220	43.322484
3501.234757	814621.239090	43.327489
3501.190056	814621.343557	43.332493
3501.218710	814619.001047	43.337498
3501.343916	814597.548994	43.342503
3501.499603	814593.822725	43.347508
3501.176796	814592.314511	43.352513
3500.904750	814593.331306	43.357517
3501.392411	814593.644817	43.362522
3501.540509	814563.128921	43.367527
3501.820959	814549.446138	43.372532
3501.470993	814550.669963	43.377537
3501.298740	814540.954788	43.382541
3501.420481	814529.927157	43.387546
3501.077509	814532.903484	43.392551
3501.381410	814526.523617	43.397556
3501.303765	814532.186282	43.402561
3501.101306	814516.435635	43.407565
3501.104075	814509.031180	43.412570
3501.286184	814508.418238	43.417575
3501.225949	814501.121045	43.422580
3500.928984	814500.388147	43.427585
3501.359078	814503.048799	43.432589
3501.297423	814502.961073	43.437594
3500.956183	814483.237722	43.442599
3501.227845	814465.269534	43.447604
3501.486611	814463.475532	43.452609
3501.433787	814471.082829	43.457613
3501.409053	814469.722836	43.462618
3501.425331	814459.783218	43.467623
3501.180613	814441.116298	43.472628
3500.992706	814439.976651	43.477633
3501.491205	814436.976087	43.482637
3501.224746	814437.310069	43.487642
3501.131894	814444.533963	43.492647
3500.975263	814414.941788	43.497652
3501.185158	814414.714189	43.502657
3500.871574	814418.367942	43.507661
3501.089235	814422.718037	43.512666
3501.043117	814428.278443	43.517671
3500.833797	814421.004462	43.522676
3500.981176	814418.156199	43.527681
3500.748680	814413.516267	43.532685
3501.355875	814424.819969	43.537690
3500.945227	814432.872942	43.542695
3501.033047	814431.982463	43.547700
3501.394377	814418.286750	43.552705
3501.023644	814403.341511	43.557709
3501.176965	814389.483405	43.562714
3500.939973	814403.452133	43.567719
3501.384219	814394.419749	43.572724
3501.037950	814392.622882	43.577729
3501.075980	814390.765940	43.582733
3501.040778	814371.871213	43.587738
3501.001480	814363.791192	43.592743
3501.062792	814352.090723	43.597748
3501.326832	814365.104393	43.602753
3500.904204	814360.396720	43.607757
3501.702171	814366.994327	43.612762
3501.024449	814369.730786	43.617767
3501.155317	814363.182953	43.622772
3501.160759	814355.680474	43.627777
3501.445131	814349.888028	43.632781
3501.269969	814336.373427	43.637786
3501.132908	814346.332240	43.642791
3500.991973	814347.426002	43.647796
3501.092702	814354.814588	43.652801
3501.247501	814326.634681	43.657805
3501.372448	814316.190723	43.662810
3501.426402	814320.956180	43.667815
3500.947282	814312.944847	43.672820
3501.535094	814324.544036	43.677825
3501.177379	814309.791388	43.682829
3501.324646	814283.560971	43.687834
3501.267995	814283.082757	43.692839
3501.033904	814272.889703	43.697844
3500.996089	814281.079440	43.702849
3501.075119	814278.534076	43.707853
3501.145596	814278.230841	43.712858
3501.053719	814282.629420	43.717863
3501.255623	814265.158692	43.722868
3501.131021	814258.942964	43.727873
3501.030020	814257.984551	43.732877
3501.309094	814254.043940	43.737882
3501.094321	814255.051834	43.742887
3501.146351	814246.177976	43.747892
3500.706440	814267.290841	43.752897
3500.834146	814263.568750	43.757901
3501.295788	814251.220957	43.762906
3501.437241	814247.983839	43.767911
3501.006363	814237.042078	43.772916
3501.235160	814233.109314	43.777921
3501.226364	814228.726555	43.782925
3501.412701	814226.651529	43.787930
3501.067757	814215.209163	43.792935
3501.223306	814206.513920	43.797940
3501.477265	814202.966911	43.802945
3501.152954	814200.971700	43.807949
3501.407983	814197.034813	43.812954
3501.146277	814202.726548	43.817959
3501.322306	814173.178655	43.822964
3501.151986	814170.964508	43.827969
3500.774152	814162.352582	43.832973
3501.051369	814166.498691	43.837978
3500.915446	814161.940903	43.842983
3501.601797	814157.449429	43.847988
3501.156749	814169.600075	43.852993
3501.105452	814161.911379	43.857997
3501.197972	814135.883756	43.863002
3501.028765	814136.689690	43.868007
3500.916203	814135.245925	43.873012
3501.399579	814142.380091	43.878017
3501.379952	814136.927254	43.883021
3500.994574	814138.156691	43.888026
3501.034733	814141.657878	43.893031
3501.015891	814130.261808	43.898036
3501.114849	814120.211298	43.903041
3501.311696	814105.858620	43.908045
3501.391248	814111.886805	43.913050
3501.332944	814112.967690	43.918055
3501.412218	814109.058222	43.923060
3501.265286	814091.544112	43.928065
3501.409274	814082.363360	43.933069
3501.311786	814070.882048	43.938074
3501.410915	814076.225204	43.943079
3501.010421	814083.205317	43.948084
3501.277017	814075.369393	43.953089
3501.414763	814048.944624	43.958093
3501.411551	814046.509451	43.963098
3501.463364	814052.931747	43.968103
3501.535554	814043.957021	43.973108
3501.332221	814028.205280	43.978113
3501.305123	814015.835995	43.983117
3501.689870	814000.771695	43.988122
3501.267072	814012.139726	43.993127
3501.197101	813984.967718	43.998132
3501.379594	813987.959590	44.003137
3501.366074	813991.274392	44.008141
3501.272456	813991.289085	44.013146
3501.304647	813994.986460	44.018151
3501.364532	813962.532824	44.023156
3501.187006	813972.108834	44.028161
3501.489537	813972.841046	44.033165
3501.418564	813966.908935	44.038170
3501.334138	813959.030307	44.043175
3501.557579	813929.961010	44.048180
3501.496900	813927.047618	44.053185
3501.179479	813930.507389	44.058189
3501.258448	813935.951247	44.063194
3501.211490	813917.836436	44.068199
3501.320620	813894.435861	44.073204
3501.287128	813902.722849	44.078209
3501.262007	813900.388476	44.083213
3501.482846	813890.513409	44.088218
3500.988812	813883.478170	44.093223
3501.562820	813866.727620	44.098228
3501.505776	813869.659561	44.103233
3501.487657	813862.939632	44.108237
3501.081504	813852.383059	44.113242
3501.284953	813842.315770	44.118247
3501.521768	813836.335421	44.123252
3501.352020	813841.720809	44.128257
3501.159120	813833.956412	44.133261
3501.465395	813831.570210	44.138266
3501.073345	813811.170649	44.143271
3501.154325	813803.850567	44.148276
3501.216802	813793.318071	44.153281
3501.468568	813795.032573	44.158285
3501.336766	813795.345536	44.163290
3501.018485	813789.159615	44.168295
3501.040124	813767.623477	44.173300
3500.940351	813757.213717	44.178305
3500.899042	813762.773962	44.183309
3501.543382	813752.247873	44.188314
3500.761309	813759.970030	44.193319
3501.100093	813751.148079	44.198324
3501.260766	813759.307470	44.203329
3501.072316	813764.500980	44.208333
3501.185332	813774.421609	44.213338
3500.950588	813746.299986	44.218343
3501.299490	813727.733008	44.223348
3501.447487	813734.140596	44.228353
3501.046216	813740.926340	44.233357
3500.978635	813740.449793	44.238362
3501.068059	813738.974361	44.243367
3501.243842	813745.767330	44.248372
3501.245171	813727.254683	44.253377
3500.665220	813709.320021	44.258381
3500.925590	813706.064035	44.263386
3500.753453	813717.978022	44.268391
3501.077364	813714.419805	44.273396
3501.336556	813719.640810	44.278401
3501.017635	813719.106117	44.283405
3501.251871	813716.536263	44.288410
3501.083679	813720.557428	44.293415
3501.050983	813716.762654	44.298420
3501.154627	813723.566923	44.303425
3500.986862	813702.255037	44.308429
3501.205240	813680.687846	44.313434
3501.384758	813691.377691	44.318439
3501.297607	813686.324757	44.323444
3501.447595	813693.121815	44.328449
3501.089750	813669.013917	44.333453
3501.251465	813661.973355	44.338458
3500.898249	813660.956840	44.343463
3501.289430	813664.500858	44.348468
3501.181628	813663.153674	44.353473
3501.300641	813658.458231	44.358477
3501.403515	813660.683223	44.363482
3501.210718	813649.216035	44.368487
3501.339746	813638.478004	44.373492
3501.583510	813630.839967	44.378497
3501.442373	813637.585158	44.383501
3501.263068	813634.105559	44.388506
3501.297873	813611.592469	44.393511
3501.266755	813591.525515	44.398516
3501.053726	813596.040950	44.403521
3501.116626	813594.277322	44.408525
3501.531763	813592.750940	44.413530
3501.328122	813588.982811	44.418535
3501.251522	813577.692201	44.423540
3501.617543	813579.096593	44.428545
3501.457676	813570.839522	44.433549
3501.550919	813549.486316	44.438554
3501.414375	813537.425506	44.443559
3501.169341	813536.879246	44.448564
3501.116094	813533.964509	44.453569
3501.090878	813530.071014	44.458573
3501.497856	813527.376644	44.463578
3501.227725	813514.946924	44.468583
3500.981493	813502.805757	44.473588
3501.053815	813503.184262	44.478593
3500.994386	813509.137316	44.483597
3501.065794	813503.474822	44.488602
3501.093853	813509.316761	44.493607
3501.251974	813502.471458	44.498612
3501.741574	813505.025804	44.503617
3501.197473	813487.084899	44.508621
3501.532462	813482.355563	44.513626
3501.434375	813481.688888	44.518631
3501.544805	813466.178998	44.523636
3501.388092	813460.357248	44.528641
3501.168300	813439.929548	44.533645
3501.372992	813442.236141	44.538650
3501.657789	813445.212282	44.543655
3501.456703	813421.468680	44.548660
3501.105486	813415.579854	44.553665
3500.977812	813417.256337	44.558669
3500.930743	813408.981420	44.563674
3500.899205	813409.863363	44.568679
3501.114206	813405.542483	44.573684
3501.350474	813408.526228	44.578689
3500.882238	813399.732499	44.583693
3501.128871	813389.852614	44.588698
3500.628177	813387.397512	44.593703
3500.844020	813371.773471	44.598708
3500.831362	813383.858041	44.603713
3500.549360	813383.804743	44.608717
3501.038089	813383.728404	44.613722
3500.883274	813375.860045	44.618727
3500.709779	813386.118396	44.623732
3500.704382	813382.806350	44.628737
3500.943117	813392.220734	44.633741
3501.082966	813389.568064	44.638746
3501.244660	813396.558494	44.643751
3500.897373	813394.176853	44.648756
3501.111637	813395.702451	44.653761
3500.828324	813394.772402	44.658765
3501.338098	813387.579685	44.663770
3501.165374	813401.540595	44.668775
3501.377427	813387.378777	44.673780
3501.073530	813377.779810	44.678785
3500.819717	813368.562760	44.683789
3501.027384	813363.171159	44.688794
3500.962847	813374.094578	44.693799
3500.916316	813362.993759	44.698804
3501.084621	813367.254868	44.703809
3500.854107	813370.019279	44.708813
3501.002507	813366.878063	44.713818
3500.987524	813373.993576	44.718823
3500.940703	813362.600483	44.723828
3501.073497	813367.062023	44.728833
3501.025644	813363.854044	44.733837
3501.118751	813335.776768	44.738842
3501.417001	813339.822701	44.743847
3501.027161	813336.863048	44.748852
3501.044880	813338.029622	44.753857
3500.933134	813343.698690	44.758861
3500.881780	813342.245172	44.763866
3500.991509	813340.376712	44.768871
3500.980866	813337.065462	44.773876
3501.479538	813347.706005	44.778881
3501.083872	813342.408699	44.783885
3501.241138	813322.408876	44.788890
3501.125565	813319.990985	44.793895
3501.295485	813316.651498	44.798900
3501.379749	813321.997623	44.803905
3500.575010	813318.225852	44.808909
3501.111017	813310.151980	44.813914
3500.960461	813313.001357	44.818919
3501.176808	813285.879001	44.823924
3501.249708	813289.472988	44.828929
3501.172802	813287.536246	44.833933
3501.295505	813284.204123	44.838938
3501.273529	813290.443853	44.843943
3501.348283	813288.580845	44.848948
3501.492726	813267.121233	44.853953
3500.728258	813263.245691	44.858957
3501.404692	813261.970711	44.863962
3501.115360	813258.215776	44.868967
3501.141627	813260.647770	44.873972
3501.476891	813266.734238	44.878977
3501.084015	813247.112498	44.883981
3501.351609	813221.540921	44.888986
3501.249375	813232.665363	44.893991
3501.416461	813240.239777	44.898996
3501.166919	813232.970697	44.904001
3501.005381	813238.550201	44.909005
3501.361745	813200.686967	44.914010
3500.992346	813204.057815	44.919015
3501.189473	813197.888181	44.924020
3501.032843	813202.395081	44.929025
3501.003196	813205.615377	44.934029
3501.410468	813200.582204	44.939034
3501.214926	813205.972167	44.944039
3501.239775	813182.387226	44.949044
3501.204309	813178.884887	44.954049
3501.113757	813174.514171	44.959053
3501.496792	813167.243572	44.964058
3501.222267	813169.722621	44.969063
3501.040621	813172.674365	44.974068
3501.241123	813151.887696	44.979073
3500.802023	813150.397303	44.984077
3500.876692	813140.836238	44.989082
3500.610036	813143.314067	44.994087
3500.880907	813134.794200	44.999092
3501.159199	813134.166096	45.004097
3500.752626	813146.312700	45.009101
3500.908712	813135.667024	45.014106
3501.190970	813146.341740	45.019111
3501.273844	813139.605248	45.024116
3501.137518	813144.596233	45.029121
3501.012990	813153.970318	45.034125
3501.329929	813134.627039	45.039130
3500.965702	813123.283129	45.044135
3500.781106	813118.147524	45.049140
3500.923631	813112.765892	45.054145
3501.058518	813114.791187	45.059149
3501.114893	813123.454931	45.064154
3500.901910	813129.627236	45.069159
3500.467576	813125.602557	45.074164
3500.892967	813120.176713	45.079169
3500.817748	813127.984028	45.084173
3501.059082	813120.832971	45.089178
3500.891700	813135.475743	45.094183
3500.858809	813132.070419	45.099188
3501.123409	813126.474829	45.104193
3500.947149	813133.518382	45.109197
3501.248284	813125.675877	45.114202
3500.930700	813108.478024	45.119207
3501.040457	813089.069548	45.124212
3501.073761	813095.788052	45.129217
3500.727204	813092.821515	45.134221
3501.138067	813090.223798	45.139226
3500.672764	813101.795004	45.144231
3501.105335	813102.994216	45.149236
3501.205793	813096.937038	45.154241
3501.354122	813107.925089	45.159245
3501.169955	813108.051381	45.164250
3501.465710	813091.732044	45.169255
3501.202822	813076.182103	45.174260
3501.393380	813077.906375	45.179265
3501.059061	813076.691917	45.184269
3501.229417	813074.229234	45.189274
3501.071956	813081.269907	45.194279
3500.992318	813055.946825	45.199284
3500.981433	813052.245683	45.204289
3500.971217	813055.073239	45.209293
3501.000853	813046.396073	45.214298
3501.094583	813056.418300	45.219303
3500.791122	813048.572765	45.224308
3501.328141	813045.468085	45.229313
3500.863993	813064.347545	45.234317
3501.147352	813053.584389	45.239322
3500.816537	813048.861364	45.244327
3500.939998	813057.124933	45.249332
3501.145910	813056.118356	45.254337
3500.978171	813050.492837	45.259341
3500.952733	813033.054219	45.264346
3500.790959	813033.859127	45.269351
3500.543709	813022.009521	45.274356
3501.124155	813019.482712	45.279361
3500.819306	813029.274952	45.284365
3500.986213	813026.715345	45.289370
3500.933061	813025.359479	45.294375
3500.991140	813032.366514	45.299380
3501.280359	813033.490704	45.304385
3501.042991	813038.595013	45.309389
3501.370541	813038.251534	45.314394
3501.233862	813019.466036	45.319399
3501.058695	813011.210618	45.324404
3501.071806	813007.603144	45.329409
3501.186039	813015.088648	45.334413
3501.233024	813002.316000	45.339418
3501.068321	813012.476141	45.344423
3500.967423	813007.814589	45.349428
3501.299844	812997.725787	45.354433
3501.275598	812995.390940	45.359437
3501.048955	812976.424485	45.364442
3501.317336	812976.382591	45.369447
3501.179846	812980.204536	45.374452
3501.494780	812970.118423	45.379457
3501.282883	812964.499729	45.384461
3501.112115	812938.703188	45.389466
3501.139347	812945.325356	45.394471
3501.085068	812950.596008	45.399476
3501.463533	812945.469690	45.404481
3501.184061	812942.979827	45.409485
3501.150983	812934.702097	45.414490
3500.973737	812919.235825	45.419495
3501.035004	812905.876068	45.424500
3501.275206	812908.859438	45.429505
3500.881433	812905.023169	45.434509
3501.396928	812904.747751	45.439514
3501.242531	812910.034089	45.444519
3501.244512	812910.326179	45.449524
3501.347699	812898.811347	45.454529
3501.099194	812880.725045	45.459533
3501.343971	812878.055757	45.464538
3500.908939	812885.042592	45.469543
3500.981376	812873.824864	45.474548
3501.012786	812879.959209	45.479553
3501.068008	812880.437873	45.484557
3501.011650	812879.374820	45.489562
3501.021993	812876.060046	45.494567
3500.819326	812870.342377	45.499572
3500.899788	812852.691807	45.504577
3500.883700	812852.402038	45.509581
3501.238895	812848.351206	45.514586
3501.351967	812852.913644	45.519591
3501.300997	812854.188494	45.524596
3501.241533	812851.469307	45.529601
3500.700018	812858.960055	45.534605
3501.044329	812856.567543	45.539610
3501.319466	812854.380740	45.544615
3501.374626	812832.251463	45.549620
3501.272116	812833.436925	45.554625
3501.173175	812819.614787	45.559629
3501.168145	812830.432401	45.564634
3500.924820	812824.721046	45.569639
3500.862915	812829.505750	45.574644
3501.249348	812823.306156	45.579649
3500.876571	812813.327296	45.584653
3501.456320	812790.336280	45.589658
3500.882513	812790.718383	45.594663
3501.073321	812786.693209	45.599668
3501.256139	812798.650901	45.604673
3501.237104	812787.642215	45.609677
3501.456340	812777.473305	45.614682
3501.221572	812766.888102	45.619687
3501.010555	812757.760910	45.624692
3501.462627	812745.314215	45.629697
3501.120810	812755.599906	45.634701
3501.298205	812755.669685	45.639706
3501.262383	812762.496800	45.644711
3501.158705	812733.667998	45.649716
3501.141318	812725.484989	45.654721
3501.147132	812728.602535	45.659725
3501.297810	812728.773940	45.664730
3501.286713	812735.987019	45.669735
3501.096335	812731.923948	45.674740
3501.142618	812701.317459	45.679745
3501.026425	812692.272799	45.684749
3501.126235	812697.129775	45.689754
3500.884261	812696.582957	45.694759
3501.063647	812697.042227	45.699764
3501.385130	812693.094016	45.704769
3501.227373	812703.351021	45.709773
3501.525549	812692.682383	45.714778
3501.503996	812676.216670	45.719783
3501.300358	812670.693871	45.724788
3501.479564	812661.895343	45.729793
3501.345679	812659.382607	45.734797
3501.507077	812638.113098	45.739802
3501.224157	812634.649137	45.744807
3501.132880	812628.231674	45.749812
3501.507605	812623.592938	45.754817
3501.153341	812609.810250	45.759821
3501.286158	812537.285063	45.764826
3501.328953	812439.337580	45.769831
3500.980784	812289.213126	45.774836
3500.965377	812075.099635	45.779841
3500.457993	811824.604376	45.784845
3500.293800	811523.362051	45.789850
3499.805546	811170.787377	45.794855
3499.756588	810759.733828	45.799860
3499.619881	810311.719625	45.804865
3498.659703	809817.102444	45.809869
3498.439656	809273.481849	45.814874
3498.020188	808685.428967	45.819879
3497.229106	808052.860867	45.824884
3496.702497	807365.228866	45.829889
3495.843689	806644.311978	45.834893
3495.252347	805860.592254	45.839898
3494.565781	805041.764039	45.844903
3493.536448	804160.968972	45.849908
3492.669128	803240.305797	45.854913
3491.617111	802296.503141	45.859917
3490.848576	801275.344669	45.864922
3489.910893	800227.931373	45.869927
3488.955161	799134.451466	45.874932
3488.383843	797988.177139	45.879937
3486.874532	796802.427354	45.884941
3485.612378	795570.009290	45.889946
3484.111740	794299.671037	45.894951
3483.298814	792978.392123	45.899956
3482.351719	791608.128638	45.904961
3480.646505	790204.154928	45.909965
3479.516431	788754.064082	45.914970
3477.812927	787254.092896	45.919975
3476.125788	785722.317981	45.924980
3475.026851	784146.247160	45.929985
3473.445599	782535.661370	45.934989
3471.806675	780870.884791	45.939994
3470.107988	779185.820035	45.944999
3468.360737	777443.219748	45.950004
3466.800162	775667.358635	45.955009
3464.901854	773864.225313	45.960013
3463.846582	772007.924450	45.965018
3462.020626	770132.751592	45.970023
3459.870575	768203.941155	45.975028
3458.096321	766234.246400	45.980033
3456.233612	764249.231239	45.985037
3454.357011	762216.026884	45.990042
3452.245800	760147.790711	45.995047
3449.932508	758041.541887	46.000052
3447.780530	755906.431297	46.005057
3445.491278	753742.679360	46.010061
3443.800334	751547.443778	46.015066
3441.244501	749324.469328	46.020071
3439.112635	747068.218329	46.025076
3437.390991	744767.689808	46.030081
3434.798660	742439.736322	46.035085
3432.760610	740090.515321	46.040090
3429.848588	737712.646979	46.045095
3427.880018	735300.698343	46.050100
3425.487862	732843.762406	46.055105
3422.708529	730385.289128	46.060109
3420.383961	727886.918840	46.065114
3417.350211	725370.412973	46.070119
3415.001253	722817.078517	46.075124
3412.518750	720240.838308	46.080129
3409.687150	717651.637162	46.085133
3406.953143	715018.563579	46.090138
3404.160938	712381.444034	46.095143
3401.846249	709699.897053	46.100148
3398.784874	707011.618001	46.105153
3395.809188	704304.155139	46.110157
3393.307057	701552.289570	46.115162
3390.548747	698801.798505	46.120167
3387.601535	696015.134239	46.125172
3385.032395	693207.240431	46.130177
3381.915152	690375.669481	46.135181
3378.762142	687525.827487	46.140186
3376.271066	684652.236839	46.145191
3373.010413	681757.684281	46.150196
3370.187034	678851.000222	46.155201
3367.202609	675915.391837	46.160205
3364.474768	672968.205255	46.165210
3361.558385	669998.177691	46.170215
3358.080399	667018.572714	46.175220
3355.356857	664002.135269	46.180225
3352.125248	660973.901482	46.185229
3349.429268	657922.758557	46.190234
3346.332981	654853.964270	46.195239
3342.701838	651779.877463	46.200244
3340.114898	648679.735069	46.205249
3336.599922	645556.269148	46.210253
3333.226745	642428.036744	46.215258
3330.026662	639276.092376	46.220263
3326.683606	636119.471858	46.225268
3323.629597	632949.132314	46.230273
3320.257715	629757.129639	46.235277
3317.158370	626548.601121	46.240282
3313.718319	623330.926806	46.245287
3310.286783	620102.554074	46.250292
3307.327592	616850.967009	46.255297
3303.610641	613587.842130	46.260301
3300.025132	610322.289611	46.265306
3296.920712	607052.661880	46.270311
3293.246307	603750.559567	46.275316
3290.133798	600444.263676	46.280321
3286.419824	597138.818957	46.285325
3283.109490	593814.747551	46.290330
3279.583854	590489.322755	46.295335
3276.156789	587145.967271	46.300340
3272.997487	583794.624193	46.305345
3269.378579	580429.443421	46.310349
3265.545008	577058.209462	46.315354
3262.095855	573663.925202	46.320359
3258.596484	570270.789729	46.325364
3255.113198	566872.780126	46.330369
3251.593736	563485.378476	46.335373
3248.173794	560060.661292	46.340378
3244.809687	556637.103655	46.345383
3240.869761	553204.512713	46.350388
3237.065300	549761.372846	46.355393
3233.667001	546313.527964	46.360397
3230.080580	542874.710759	46.365402
3226.341618	539424.404520	46.370407
3222.605438	535965.304601	46.375412
3218.760101	532498.741568	46.380417
3215.467757	529033.933513	46.385421
3211.652033	525564.513116	46.390426
3208.070744	522089.009078	46.395431
3204.180566	518611.947963	46.400436
3200.838986	515115.662803	46.405441
3197.242928	511623.319546	46.410445
3193.322492	508132.522546	46.415450
3190.027406	504628.606622	46.420455
3186.076905	501117.324559	46.425460
3182.717109	497615.042716	46.430465
3178.488225	494106.155034	46.435469
3174.669309	490598.648647	46.440474
3171.164535	487071.236415	46.445479
3167.291706	483556.052450	46.450484
3163.746207	480029.460197	46.455489
3159.919038	476495.905383	46.460493
3156.038300	472967.694339	46.465498
3152.569156	469435.718276	46.470503
3148.959339	465914.031463	46.475508
3145.100630	462364.375179	46.480513
3141.087351	458845.875934	46.485517
3137.073067	455297.407386	46.490522
3133.849458	451759.737483	46.495527
3129.897095	448221.427023	46.500532
3126.233404	444678.226348	46.505537
3122.043067	441147.187498	46.510541
3118.226616	437603.923740	46.515546
3114.707636	434062.536551	46.520551
3110.753050	430523.102349	46.525556
3107.040290	426987.808359	46.530561
3102.981500	423455.898269	46.535565
3099.189172	419920.698171	46.540570
3095.486713	416387.417657	46.545575
3091.445806	412854.614374	46.550580
3087.874006	409328.260619	46.555585
3084.355453	405792.454428	46.560589
3080.155526	402263.757845	46.565594
3076.228651	398728.993298	46.570599
3072.655040	395205.566489	46.575604
3068.491391	391674.959568	46.580609
3064.764458	388152.683128	46.585613
3061.020064	384635.953766	46.590618
3057.267047	381111.451973	46.595623
3052.853371	377604.328493	46.600628
3049.291679	374085.688131	46.605633
3045.370723	370574.474215	46.610637
3041.662670	367057.044009	46.615642
3037.845316	363557.112527	46.620647
3033.850580	360055.699080	46.625652
3030.150775	356547.860274	46.630657
3026.534281	353066.299925	46.635661
3022.329694	349562.690328	46.640666
3018.216959	346078.775654	46.645671
3014.083968	342603.428129	46.650676
3010.565107	339117.693617	46.655681
3006.520846	335641.517634	46.660685
3002.975027	332170.124349	46.665690
2998.918525	328702.436928	46.670695
2994.501776	325240.936050	46.675700
2990.976574	321763.101543	46.680705
2986.745587	318320.226160	46.685709
2983.133853	314861.742144	46.690714
2979.063355	311421.769440	46.695719
2974.862250	307988.870326	46.700724
2970.798256	304562.632671	46.705729
2967.008304	301139.279578	46.710733
2963.183126	297734.370506	46.715738
2958.954101	294325.398427	46.720743
2955.383891	290933.868854	46.725748
2951.343295	287546.784227	46.730753
2946.813105	284154.712801	46.735757
2942.923633	280770.903740	46.740762
2939.219934	277401.753100	46.745767
2934.965016	274042.015078	46.750772
2931.281758	270686.533869	46.755777
2926.760749	267349.111693	46.760781
2923.207726	264009.844193	46.765786
2919.441691	260690.061053	46.770791
2914.605888	257372.564763	46.775796
2910.571717	254059.185492	46.780801
2906.746448	250775.110154	46.785805
2902.491098	247479.624880	46.790810
2898.746939	244198.491435	46.795815
2894.231635	240939.280051	46.800820
2890.409609	237686.413547	46.805825
2886.156096	234445.068339	46.810829
2881.863291	231208.595261	46.815834
2878.061772	227994.798978	46.820839
2873.625754	224791.944386	46.825844
2869.595298	221590.733519	46.830849
2865.216458	218423.052043	46.835853
2861.037206	215253.572875	46.840858
2857.111031	212104.147468	46.845863
2853.049252	208968.476657	46.850868
2848.991491	205833.760795	46.855873
2844.511017	202715.023537	46.860877
2840.510140	199601.205071	46.865882
2836.384012	196522.253864	46.870887
2831.839638	193459.121293	46.875892
2828.172421	190394.447109	46.880897
2823.982978	187342.004498	46.885901
2819.418858	184310.586866	46.890906
2814.914076	181291.397489	46.895911
2810.807831	178290.219765	46.900916
2806.948627	175302.715588	46.905921
2802.693675	172337.507075	46.910925
2798.833536	169381.999389	46.915930
2794.581808	166392.634186	46.920935
2790.264188	163416.110779	46.925940
2786.073597	160503.506837	46.930945
2781.489356	157603.036886	46.935949
2777.392349	154727.523362	46.940954
2773.529129	151861.622145	46.945959
2769.054401	149009.338328	46.950964
2765.121400	146168.662761	46.955969
2760.984856	143352.439884	46.960973
2756.512802	140541.822972	46.965978
2752.671063	137754.375414	46.970983
2748.163130	134980.429047	46.975988
2744.159705	132227.130963	46.980993
2740.076400	129481.586452	46.985997
2735.350555	126754.558789	46.991002
2731.631223	124046.414698	46.996007
2727.365005	121359.522135	47.001012
2723.446651	118661.885852	47.006017
2718.872916	116005.945274	47.011021
2715.208452	113358.710205	47.016026
2710.976015	110721.062812	47.021031
2706.667697	108097.136665	47.026036
2702.497148	105493.726244	47.031041
2698.509874	102902.434718	47.036045
2694.381683	100328.792442	47.041050
2690.502659	97765.939058	47.046055
2686.591880	95232.042080	47.051060
2682.396878	92688.419199	47.056065
2678.214130	90176.223899	47.061069
2674.043444	87659.306373	47.066074
2669.834503	85169.592133	47.071079
2665.507322	82690.500599	47.076084
2661.405191	80226.005623	47.081089
2657.491352	77792.191968	47.086093
2653.189569	75364.863711	47.091098
2648.932334	72942.634439	47.096103
2644.808002	70553.147210	47.101108
2640.797645	68175.971454	47.106113
2636.494578	65815.766365	47.111117
2632.417815	63463.214668	47.116122
2628.406481	61138.308120	47.121127
2623.719717	58821.124634	47.126132
2619.826398	56517.203133	47.131137
2615.693150	54242.990844	47.136141
2611.284959	51970.301837	47.141146
2607.370282	49730.690411	47.146151
2602.957687	47501.249328	47.151156
2598.907208	45286.822433	47.156161
2594.151741	43099.471485	47.161165
2589.847422	40917.717986	47.166170
2585.841359	38760.404436	47.171175
2581.311778	36622.861983	47.176180
2577.486583	34498.955633	47.181185
2572.688095	32410.375894	47.186189
2568.337248	30332.555765	47.191194
2564.216944	28278.062899	47.196199
2559.752666	26239.011219	47.201204
2555.526342	24224.094966	47.206209
2551.339031	22239.174792	47.211213
2546.525434	20267.707086	47.216218
2541.845346	18311.984186	47.221223
2537.452827	16410.624703	47.226228
2532.685555	14509.038850	47.231233
2528.374701	12638.685681	47.236237
2523.281662	10800.887917	47.241242
2517.964408	9003.429092	47.246247
2511.882006	7266.342845	47.251252
2503.438067	5638.788273	47.256257
2493.161984	4118.246569	47.261261
2483.278723	2673.321121	47.266266
2473.749641	1338.599815	47.271271
2460.027728	200.846234	47.276276
2410.166221	194.757006	47.281281
2374.709089	223.849482	47.286285
2359.381953	229.952236	47.291290
2359.690833	220.785690	47.296295
2367.283994	217.455920	47.301300
2377.169146	221.911405	47.306305
2384.963243	236.517857	47.311309
2389.013200	225.184116	47.316314
2390.203470	217.151563	47.321319
2388.884339	229.095959	47.326324
2385.757565	207.146981	47.331329
2382.038474	205.362279	47.336333
2377.956752	222.082846	47.341338
2375.271512	222.249876	47.346343
2372.528019	219.151411	47.351348
2369.028397	216.541410	47.356353
2366.387664	218.223302	47.361357
2363.934135	218.955221	47.366362
2361.054450	209.790777	47.371367
2358.287109	215.671951	47.376372
2354.785363	206.481436	47.381377
2351.193019	208.413447	47.386381
2348.211667	208.424320	47.391386
2345.197340	193.718871	47.396391
2341.778854	210.316693	47.401396
2339.186518	209.640263	47.406401
2336.286414	209.847244	47.411405
2332.407598	204.493391	47.416410
2328.964400	206.671005	47.421415
2325.748469	210.227314	47.426420
2322.636733	201.700326	47.431425
2319.492901	197.550829	47.436429
2316.062750	207.034940	47.441434
2312.935826	203.116925	47.446439
2309.109272	213.877983	47.451444
2305.758142	193.261346	47.456449
2302.036509	209.723097	47.461453
2299.208422	207.520608	47.466458
2296.100077	192.108526	47.471463
2292.528580	198.561621	47.476468
2289.142982	198.787620	47.481473
2286.156593	197.559062	47.486477
2282.407015	201.141920	47.491482
2278.925020	202.645385	47.496487
2275.480336	199.947727	47.501492
2272.040852	196.508912	47.506497
2268.674547	198.715642	47.511501
2264.605738	205.154799	47.516506
2261.880595	202.879266	47.521511
2258.692667	201.894226	47.526516
2255.346909	199.007084	47.531521
2251.920735	196.493207	47.536525
2248.438429	197.000112	47.541530
2244.794977	201.831924	47.546535
2241.193598	200.750217	47.551540
2237.933651	194.277653	47.556545
2234.777907	199.928538	47.561549
2230.880430	204.730492	47.566554
2227.829355	203.015344	47.571559
2224.018248	200.207346	47.576564
2220.206086	204.853582	47.581569
2217.045016	196.941815	47.586573
2212.958416	205.766162	47.591578
2210.571159	194.575793	47.596583
2207.061458	210.422253	47.601588
2204.316362	203.084507	47.606593
2200.398483	202.501601	47.611597
2196.987897	197.023925	47.616602
2192.963851	186.918585	47.621607
2189.662151	202.074414	47.626612
2186.311370	196.191902	47.631617
2182.712446	196.925889	47.636621
2178.949116	192.996754	47.641626
2175.779009	193.527605	47.646631
2172.369950	188.812193	47.651636
2169.054916	193.092751	47.656641
2165.395256	189.213843	47.661645
2162.129710	194.065647	47.666650
2158.515438	194.207236	47.671655
2154.857107	196.269858	47.676660
2151.368777	193.743592	47.681665
2148.100051	196.707072	47.686669
2144.579445	194.325068	47.691674
2141.081034	197.112508	47.696679
2137.495234	194.364207	47.701684
2134.268322	193.926324	47.706689
2130.792962	186.513035	47.711693
2126.974784	198.250453	47.716698
2123.759602	196.785646	47.721703
2119.964331	194.617474	47.726708
2116.848823	185.268554	47.731713
2113.366730	185.813435	47.736717
2109.651872	193.184381	47.741722
2106.231279	185.449310	47.746727
2102.810112	196.751279	47.751732
2099.346471	183.397603	47.756737
2096.070439	186.514104	47.761741
2092.419618	188.692632	47.766746
2089.618611	184.233300	47.771751
2085.795396	194.933767	47.776756
2081.961365	189.243971	47.781761
2078.860322	191.962926	47.786765
2074.832443	190.052637	47.791770
2071.529024	183.219930	47.796775
2067.972370	192.144899	47.801780
2064.200627	186.521297	47.806785
2060.740305	185.556791	47.811789
2057.019872	191.593475	47.816794
2053.971459	186.888116	47.821799
2050.567445	186.360907	47.826804
2047.562436	181.740513	47.831809
2044.152872	186.880644	47.836813
2040.015782	192.273823	47.841818
2036.844237	191.115438	47.846823
2032.735215	192.242511	47.851828
2029.432970	188.263435	47.856833
2026.214434	192.968708	47.861837
2022.420071	178.138675	47.866842
2019.664312	184.283859	47.871847
2016.055127	184.257016	47.876852
2012.303556	182.600920	47.881857
2008.819506	180.491665	47.886861
2004.940970	187.252314	47.891866
2001.494367	173.772632	47.896871
1998.132196	187.020649	47.901876
1994.800663	183.742217	47.906881
1991.349767	183.510274	47.911885
1987.453229	190.934992	47.916890
1984.371162	181.413206	47.921895
1980.837901	185.022420	47.926900
1977.680844	186.117616	47.931905
1974.197413	186.067946	47.936909
1970.405948	189.831466	47.941914
1967.079504	180.708605	47.946919
1963.347666	179.878370	47.951924
1960.138423	177.523644	47.956929
1956.043515	181.543464	47.961933
1952.634939	179.397107	47.966938
1949.543318	179.589865	47.971943
1945.787307	181.354616	47.976948
1942.621638	177.313070	47.981953
1939.112207	179.713139	47.986957
1935.446906	185.450155	47.991962
1932.226776	175.377338	47.996967
1928.336716	191.074538	48.001972
1924.896531	182.839552	48.006977
1921.205522	184.154364	48.011981
1917.999882	179.764729	48.016986
1914.985026	179.078589	48.021991
1911.052461	183.364095	48.026996
1907.358016	176.434448	48.032001
1903.730530	183.019795	48.037005
1900.376690	181.820375	48.042010
1896.910294	176.658442	48.047015
1893.168563	179.449227	48.052020
1890.144142	173.904914	48.057025
1886.986247	168.969967	48.062029
1883.044197	177.230763	48.067034
1879.546323	166.714201	48.072039
1875.914201	176.157237	48.077044
1872.328444	177.465086	48.082049
1869.124866	178.656181	48.087053
1865.079576	173.145074	48.092058
1862.167766	174.056388	48.097063
1858.190077	173.951220	48.102068
1855.179736	176.763610	48.107073
1851.551406	168.194259	48.112077
1848.108466	171.858982	48.117082
1844.978574	169.343176	48.122087
1841.310104	173.403872	48.127092
1837.610361	173.005272	48.132097
1833.830295	157.540341	48.137101
1830.007322	179.086501	48.142106
1827.006373	172.576726	48.147111
1823.647456	170.966825	48.152116
1819.868451	174.234881	48.157121
1816.124255	170.815441	48.162125
1812.822580	177.621917	48.167130
1809.841800	171.536112	48.172135
1806.214160	174.834270	48.177140
1803.245559	170.992895	48.182145
1799.308810	166.135570	48.187149
1795.389486	168.147397	48.192154
1791.918801	168.070482	48.197159
1788.116886	174.126320	48.202164
1785.064692	174.303464	48.207169
1781.742243	174.266631	48.212173
1778.134594	174.483245	48.217178
1774.540820	166.126826	48.222183
1771.188920	169.900714	48.227188
1767.611018	169.869060	48.232193
1764.343853	170.219062	48.237197
1760.577553	181.369460	48.242202
1757.340362	182.167203	48.247207
1753.678988	176.371429	48.252212
1750.072544	170.377232	48.257217
1746.250431	159.022433	48.262221
1742.996769	168.959945	48.267226
1739.523260	163.267663	48.272231
1735.756757	164.885425	48.277236
1732.320762	172.282433	48.282241
1729.305992	171.086955	48.287245
1725.649505	166.881846	48.292250
1722.497129	172.272887	48.297255
1718.320763	170.477732	48.302260
1714.815585	171.368050	48.307265
1711.338181	167.036840	48.312269
1707.611171	171.619283	48.317274
1704.550400	164.878464	48.322279
1700.990907	164.483274	48.327284
1697.702793	164.213298	48.332289
1694.495175	164.063606	48.337293
1690.825319	170.494286	48.342298
1687.053630	160.422472	48.347303
1683.603956	170.365364	48.352308
1680.412002	163.119886	48.357313
1676.617763	163.033534	48.362317
1672.848232	165.600945	48.367322
1669.593040	158.359043	48.372327
1666.228827	157.639066	48.377332
1662.510018	156.936620	48.382337
1659.111202	159.439689	48.387341
1655.006892	174.866742	48.392346
1651.970907	162.493583	48.397351
1648.810366	161.754391	48.402356
1645.099548	159.535220	48.407361
1641.782191	151.996167	48.412365
1637.863486	167.713718	48.417370
1634.498712	163.940731	48.422375
1630.758473	165.253854	48.427380
1627.461187	164.324093	48.432385
1624.292910	163.785441	48.437389
1620.750553	156.069632	48.442394
1617.215735	158.919875	48.447399
1613.768127	152.742687	48.452404
1609.994501	154.076863	48.457409
1606.248977	164.236922	48.462413
1602.850768	167.780818	48.467418
1599.301366	151.517422	48.472423
1595.979737	160.462663	48.477428
1592.661435	157.669537	48.482433
1589.297237	160.252633	48.487437
1585.684961	162.912524	48.492442
1582.462864	152.318134	48.497447
1578.646242	162.906955	48.502452
1574.969321	164.156402	48.507457
1571.377900	154.151345	48.512461
1567.788239	166.270749	48.517466
1564.951864	152.993170	48.522471
1561.029931	151.648656	48.527476
1557.762882	150.400967	48.532481
1554.192444	160.441883	48.537485
1550.137407	154.951430	48.542490
1546.963341	158.384327	48.547495
1543.115090	158.701959	48.552500
1539.937521	161.569080	48.557505
1536.760801	148.993372	48.562509
1532.906131	157.335506	48.567514
1529.679536	152.607599	48.572519
1526.079285	159.226753	48.577524
1522.714947	159.041532	48.582529
1519.067505	156.059497	48.587533
1515.248051	156.894665	48.592538
1512.079962	149.433544	48.597543
1508.350734	156.449386	48.602548
1505.329381	160.155793	48.607553
1501.691067	149.471557	48.612557
1497.869461	158.703892	48.617562
1494.582418	157.478335	48.622567
1490.984229	161.183283	48.627572
1487.384952	151.622432	48.632577
1484.357220	150.533466	48.637581
1480.721167	155.949650	48.642586
1477.291521	142.135372	48.647591
1473.325758	154.354789	48.652596
1469.820219	155.080726	48.657601
1466.483063	152.499410	48.662605
1462.942018	155.727174	48.667610
1459.239553	152.478521	48.672615
1455.896803	158.399312	48.677620
1452.374253	153.961373	48.682625
1448.862098	152.631859	48.687629
1445.530792	159.341821	48.692634
1442.256960	152.365524	48.697639
1438.751931	163.927531	48.702644
1434.955442	158.086603	48.707649
1431.691146	150.096392	48.712653
1427.820090	159.213099	48.717658
1424.476464	146.280743	48.722663
1420.826773	159.453640	48.727668
1417.299280	160.040659	48.732673
1414.071716	145.274099	48.737677
1410.377955	152.290745	48.742682
1407.114014	152.577080	48.747687
1403.340935	148.618150	48.752692
1399.837836	153.308012	48.757697
1396.525325	152.089640	48.762701
1393.067311	155.007029	48.767706
1389.501629	151.664225	48.772711
1385.949639	150.878822	48.777716
1382.674353	155.175517	48.782721
1379.334687	150.905138	48.787725
1375.208995	156.976982	48.792730
1372.081462	149.164708	48.797735
1368.323793	152.825054	48.802740
1364.684589	145.697171	48.807745
1361.557724	142.485011	48.812749
1357.868651	161.007802	48.817754
1354.669361	150.315022	48.822759
1351.060790	146.352510	48.827764
1347.225626	145.889865	48.832769
1344.047796	151.370407	48.837773
1340.189368	153.619647	48.842778
1336.641686	148.502301	48.847783
1333.248613	142.354658	48.852788
1329.405032	148.581677	48.857793
1326.777751	144.883191	48.862797
1323.188821	162.235515	48.867802
1319.643483	147.828796	48.872807
1316.246124	146.490853	48.877812
1312.321992	151.578853	48.882817
1308.778809	140.579255	48.887821
1304.986232	148.959193	48.892826
1301.883563	144.518864	48.897831
1298.286513	148.302790	48.902836
1294.603077	151.321938	48.907841
1291.660024	143.309972	48.912845
1288.346240	159.764996	48.917850
1284.499731	154.077501	48.922855
1280.606302	150.798702	48.927860
1277.045848	150.378504	48.932865
1273.879877	144.663579	48.937869
1270.526553	152.218612	48.942874
1267.223622	148.075406	48.947879
1263.546966	143.826187	48.952884
1259.904908	137.461283	48.957889
1256.295968	144.458369	48.962893
1252.789108	150.847842	48.967898
1249.066681	143.207842	48.972903
1246.031336	149.188137	48.977908
1242.212027	156.325734	48.982913
1239.260183	152.709720	48.987917
1235.428776	157.087191	48.992922
1231.794230	152.236591	48.997927
1228.182738	148.480233	49.002932
1224.435565	154.084742	49.007937
1221.036305	153.205885	49.012941
1217.545069	149.408558	49.017946
1214.161864	152.921749	49.022951
1211.177245	138.364033	49.027956
1207.336034	146.985738	49.032961
1203.954233	150.615773	49.037965
1200.129965	150.664021	49.042970
1197.215970	142.074888	49.047975
1193.736909	144.960833	49.052980
1189.671988	134.479581	49.057985
1186.295425	141.598499	49.062989
1182.840937	150.112214	49.067994
1179.425738	147.514745	49.072999
1175.972663	136.592854	49.078004
1172.061798	139.479966	49.083009
1169.059424	139.640006	49.088013
1164.858816	139.025833	49.093018
1161.271519	137.581638	49.098023
1158.479480	146.501023	49.103028
1154.806128	148.164524	49.108033
1151.536693	143.772503	49.113037
1147.736606	149.644754	49.118042
1144.529142	131.179833	49.123047
1140.898153	136.677588	49.128052
1136.753293	143.132176	49.133057
1133.601977	139.189917	49.138061
1129.997797	139.368254	49.143066
1126.935245	134.213013	49.148071
1123.481809	141.321838	49.153076
1119.780283	144.046479	49.158081
1116.260607	137.127790	49.163085
1112.662264	144.370039	49.168090
1109.334522	134.497931	49.173095
1105.342871	137.922910	49.178100
1101.754609	146.533521	49.183105
1098.769536	129.255044	49.188109
1095.509180	137.409346	49.193114
1091.780213	131.722526	49.198119
1088.589786	140.065203	49.203124
1085.015130	143.627390	49.208129
1081.421186	134.970750	49.213133
1077.765915	148.976686	49.218138
1074.247139	141.273243	49.223143
1070.578226	136.646400	49.228148
1066.571888	141.184196	49.233153
1063.471075	134.190459	49.238157
1060.252132	136.153016	49.243162
1056.474675	132.511304	49.248167
1053.504138	135.380954	49.253172
1049.592533	137.948682	49.258177
1046.385074	128.598785	49.263181
1042.847160	136.954749	49.268186
1039.285979	132.424950	49.273191
1035.791738	131.339565	49.278196
1032.148873	131.653713	49.283201
1028.419330	135.904570	49.288205
1024.903815	135.028168	49.293210
1021.693374	134.145132	49.298215
1018.173961	132.668217	49.303220
1014.323983	134.558743	49.308225
1011.032706	128.300382	49.313229
1007.707963	143.785870	49.318234
1004.161055	139.114642	49.323239
1000.760621	135.382283	49.328244
997.437794	143.486283	49.333249
993.734615	133.805888	49.338253
990.005134	147.532394	49.343258
986.962158	138.049194	49.348263
983.424690	140.238822	49.353268
979.925772	143.520262	49.358273
976.045676	141.530348	49.363277
972.196764	138.567424	49.368282
968.936368	134.449312	49.373287
965.619514	136.389264	49.378292
962.289702	144.513351	49.383297
958.861451	136.140876	49.388301
954.724529	140.999723	49.393306
951.788637	145.683175	49.398311
948.100472	146.450547	49.403316
944.267301	141.957044	49.408321
941.279983	141.981917	49.413325
937.270358	142.214319	49.418330
933.953943	143.878962	49.423335
931.036819	141.811053	49.428340
927.213399	141.315100	49.433345
923.776527	134.551211	49.438349
919.489927	137.060646	49.443354
916.194962	139.092101	49.448359
913.257367	137.944912	49.453364
909.317467	139.536342	49.458369
906.343245	135.095029	49.463373
902.814515	137.270662	49.468378
899.101939	137.763458	49.473383
895.803061	137.504929	49.478388
892.106887	130.886064	49.483393
888.756272	134.305666	49.488397
884.910599	134.638971	49.493402
881.647817	128.180043	49.498407
877.986222	136.555423	49.503412
874.290937	145.622630	49.508417
871.295839	127.918715	49.513421
867.266877	132.086798	49.518426
863.987299	130.044030	49.523431
860.727491	128.225963	49.528436
857.009544	122.898199	49.533441
853.686618	130.723833	49.538445
849.803128	135.606313	49.543450
846.040342	136.303149	49.548455
842.873634	140.674753	49.553460
839.547981	141.486642	49.558465
836.344326	130.734667	49.563469
832.195738	140.641675	49.568474
829.083831	132.820847	49.573479
825.248492	129.406602	49.578484
821.835172	134.168011	49.583489
818.607124	141.732025	49.588493
814.980190	139.091921	49.593498
811.813394	126.078387	49.598503
808.400873	127.109538	49.603508
804.692443	126.219136	49.608513
801.152333	121.945573	49.613517
797.211754	131.842163	49.618522
793.921773	123.574667	49.623527
790.742623	132.915418	49.628532
786.712260	131.888771	49.633537
783.391074	125.185925	49.638541
780.218805	128.852886	49.643546
776.154683	124.667717	49.648551
772.687431	125.198078	49.653556
768.907221	128.713466	49.658561
765.986796	127.234600	49.663565
762.842600	120.972293	49.668570
759.334325	125.590399	49.673575
755.824216	125.380818	49.678580
752.089294	128.569575	49.683585
748.623958	126.524302	49.688589
744.677917	125.269330	49.693594
741.104480	126.426946	49.698599
737.874470	121.108248	49.703604
734.332287	134.099954	49.708609
730.722141	117.283386	49.713613
727.253804	124.992618	49.718618
723.710911	125.129875	49.723623
719.829535	126.474931	49.728628
716.732897	127.339586	49.733633
713.831612	129.154431	49.738637
710.135640	124.057412	49.743642
706.583481	121.791631	49.748647
703.141689	122.039615	49.753652
699.505892	118.451808	49.758657
695.889280	120.559018	49.763661
692.004933	134.088383	49.768666
688.744455	127.107145	49.773671
685.373333	124.449182	49.778676
681.679566	131.064255	49.783681
678.527868	126.938725	49.788685
674.413846	131.914322	49.793690
671.085765	131.942026	49.798695
667.976582	121.501208	49.803700
664.348684	127.935124	49.808705
661.162615	120.318977	49.813709
657.513551	129.280929	49.818714
654.054697	128.731160	49.823719
650.336239	129.898867	49.828724
646.782865	125.719195	49.833729
643.360854	125.486368	49.838733
639.791731	133.246217	49.843738
635.933308	128.095576	49.848743
632.914427	122.003523	49.853748
628.845665	128.316667	49.858753
625.874349	123.324500	49.863757
622.420455	129.446437	49.868762
619.092517	121.010952	49.873767
615.710590	119.057075	49.878772
611.671047	136.087795	49.883777
608.493164	128.843714	49.888781
604.732530	124.781943	49.893786
601.287730	125.068402	49.898791
597.996358	125.571282	49.903796
594.237462	130.051523	49.908801
590.665661	119.515510	49.913805
586.972964	130.059895	49.918810
583.532195	129.352293	49.923815
580.304535	124.409782	49.928820
576.616621	128.783998	49.933825
573.367066	128.682379	49.938829
569.599970	131.977486	49.943834
566.451415	127.677498	49.948839
562.953434	136.214018	49.953844
559.331072	137.100951	49.958849
555.956171	122.683761	49.963853
552.028725	130.983820	49.968858
548.613769	133.224021	49.973863
545.128444	125.249822	49.978868
541.643598	128.060964	49.983873
538.339260	129.777635	49.988877
534.549504	137.967551	49.993882
531.078635	134.711491	49.998887
527.839520	129.413282	50.003892
523.899144	132.833625	50.008897
520.910560	128.059339	50.013901
517.495183	134.789057	50.018906
513.574244	138.041843	50.023911
510.395407	122.059522	50.028916
506.799964	136.853511	50.033921
503.571919	133.872647	50.038925
499.426090	126.603043	50.043930
496.032792	127.346555	50.048935
492.563495	119.705235	50.053940
488.890160	130.003005	50.058945
485.560179	121.074345	50.063949
482.014544	123.629271	50.068954
478.868810	128.500743	50.073959
475.531290	128.533161	50.078964
471.747007	129.024704	50.083969
468.337927	120.541883	50.088973
464.578807	126.910997	50.093978
460.902668	123.196731	50.098983
457.894029	125.578969	50.103988
454.027426	127.475487	50.108993
450.890154	126.631814	50.113997
447.157057	128.073982	50.119002
443.729558	126.086180	50.124007
439.973208	115.585477	50.129012
436.252220	125.267456	50.134017
433.062617	128.345610	50.139021
429.681295	123.961910	50.144026
425.899442	128.006041	50.149031
422.757141	131.874068	50.154036
418.795280	128.872135	50.159041
416.014083	125.612505	50.164045
412.342345	125.861814	50.169050
408.409224	127.730804	50.174055
405.415580	117.841489	50.179060
401.453336	132.212059	50.184065
397.985396	120.862593	50.189069
394.244178	119.461798	50.194074
390.795027	120.676012	50.199079
387.507208	132.852839	50.204084
384.056082	127.929589	50.209089
380.805080	113.784157	50.214093
376.964063	128.148398	50.219098
373.762918	119.879827	50.224103
370.351044	119.923931	50.229108
366.405923	128.755179	50.234113
363.221637	119.791098	50.239117
359.224899	121.844083	50.244122
355.961542	116.673134	50.249127
352.839327	118.487893	50.254132
348.921362	120.784810	50.259137
345.568150	116.583408	50.264141
342.205416	130.249474	50.269146
338.356342	116.216727	50.274151
335.446930	125.932966	50.279156
331.154208	133.357003	50.284161
328.126761	120.109895	50.289165
324.806823	126.375463	50.294170
321.259185	122.128594	50.299175
317.852146	121.194347	50.304180
313.724523	119.025200	50.309185
310.306779	124.929602	50.314189
306.687951	127.527697	50.319194
303.167450	127.474946	50.324199
300.056100	122.767432	50.329204
296.354665	113.422479	50.334209
293.305927	125.773850	50.339213
289.807168	128.062073	50.344218
286.198258	121.676599	50.349223
282.310512	128.932810	50.354228
278.379025	127.973164	50.359233
275.456130	121.290402	50.364237
271.758994	121.679792	50.369242
268.625519	123.100868	50.374247
265.132250	125.388241	50.379252
261.355629	129.766980	50.384257
258.114924	130.448711	50.389261
254.590816	126.021011	50.394266
250.530951	128.723020	50.399271
247.368907	127.364437	50.404276
243.901356	138.272305	50.409281
240.754676	125.091368	50.414285
237.246222	123.495987	50.419290
233.334250	127.418206	50.424295
229.863026	121.457284	50.429300
226.346048	128.490917	50.434305
222.787518	122.717684	50.439309
219.236713	123.106318	50.444314
215.796039	122.500087	50.449319
212.885661	114.341063	50.454324
209.527282	119.514852	50.459329
205.730244	114.443391	50.464333
201.492298	121.074276	50.469338
197.964256	121.604887	50.474343
194.753195	123.946153	50.479348
191.024885	126.558280	50.484353
187.602934	129.018010	50.489357
184.200316	130.522410	50.494362
180.595079	135.272971	50.499367
177.401861	125.478290	50.504372
173.796077	130.282722	50.509377
170.611818	124.915956	50.514381
166.934820	126.127985	50.519386
163.550549	129.670166	50.524391
159.636412	124.746784	50.529396
155.944120	127.103343	50.534401
152.632555	128.868740	50.539405
149.145545	131.990418	50.544410
145.758129	120.745522	50.549415
142.614883	120.598932	50.554420
138.909463	125.156391	50.559425
135.541110	115.654931	50.564429
132.089278	126.769173	50.569434
128.439503	125.657891	50.574439
124.789375	126.033649	50.579444
120.948035	136.187018	50.584449
117.910225	122.229774	50.589453
114.242889	120.051888	50.594458
111.021361	119.654979	50.599463
107.526776	111.065501	50.604468
103.642857	131.042789	50.609473
100.314985	122.740405	50.614477
96.356650	119.636834	50.619482
93.360585	119.789909	50.624487
89.833294	111.328951	50.629492
86.451132	125.770090	50.634497
82.914240	116.579801	50.639501
79.456809	125.717566	50.644506
75.785095	115.703671	50.649511
72.078995	108.906418	50.654516
68.349763	116.957293	50.659521
65.203723	112.217345	50.664525
62.018541	118.458720	50.669530
58.212945	111.534690	50.674535
54.828614	119.170862	50.679540
51.309374	118.754179	50.684545
47.721429	116.994160	50.689549
44.053145	119.774114	50.694554
40.710993	120.601534	50.699559
37.506250	120.398177	50.704564
33.953489	125.618302	50.709569
30.386490	117.590703	50.714573
26.732877	121.728795	50.719578
23.188493	125.612491	50.724583
19.692588	122.164417	50.729588
15.968315	119.935384	50.734593
12.563880	117.735335	50.739597
8.903173	122.137141	50.744602
5.505821	118.249685	50.749607
2.457114	121.745674	50.754612