Thu Aug 25 16:29:55 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
0.857963	101.655839	0.000000
1.294482	106.991256	0.005005
1.557357	122.680487	0.010010
1.243623	115.313789	0.015014
1.273708	109.848444	0.020019
1.039663	103.418401	0.025024
1.057895	102.773361	0.030029
0.968940	99.104719	0.035034
0.565497	82.086730	0.040038
0.599337	75.121175	0.045043
-0.080973	78.325174	0.050048
-0.289544	56.145025	0.055053
-0.241254	51.398187	0.060058
-0.471329	47.761157	0.065062
-0.630572	30.366432	0.070067
-1.241889	37.663028	0.075072
-1.426571	26.723229	0.080077
-2.158058	28.856392	0.085082
-2.487110	26.386488	0.090086
-2.587291	18.347289	0.095091
-3.224695	22.246913	0.100096
-3.200685	16.912263	0.105101
-3.383985	12.227032	0.110106
-3.325511	15.223517	0.115110
-3.363245	6.760085	0.120115
-4.053469	13.724184	0.125120
-4.335492	12.056838	0.130125
-4.531462	13.185437	0.135130
-4.864536	15.977514	0.140134
-5.281667	11.553548	0.145139
-6.192189	13.616685	0.150144
-5.917486	10.349828	0.155149
-5.587064	14.534410	0.160154
-5.726407	17.223366	0.165158
-5.800528	15.653160	0.170163
-6.955667	15.090730	0.175168
-7.160390	13.129698	0.180173
-7.418241	13.771280	0.185178
-7.555021	21.423791	0.190182
-7.428665	11.403382	0.195187
-7.665217	12.367495	0.200192
-8.528474	11.126579	0.205197
-9.014092	6.779784	0.210202
-9.048457	10.252725	0.215206
-8.810060	7.485105	0.220211
-9.347389	17.933870	0.225216
-9.379769	9.925180	0.230221
-9.283649	11.874886	0.235226
-9.546097	13.776369	0.240230
-10.130647	10.729565	0.245235
-10.516573	17.310628	0.250240
-10.654265	9.622162	0.255245
-10.879873	12.311978	0.260250
-11.340277	8.195352	0.265254
-11.662264	4.715102	0.270259
-11.414668	11.225374	0.275264
-11.538863	16.673928	0.280269
-11.961829	12.361608	0.285274
-12.801442	18.377839	0.290278
-12.732456	5.493719	0.295283
-13.540679	14.403042	0.300288
-13.116621	16.054592	0.305293
-13.130108	10.390460	0.310298
-13.593405	4.771497	0.315302
-14.140745	11.877724	0.320307
-14.490254	17.098988	0.325312
-14.984342	12.127093	0.330317
-14.605297	13.241527	0.335322
-14.768223	18.686658	0.340326
-14.587800	10.609824	0.345331
-15.377820	15.960220	0.350336
-15.733457	10.909685	0.355341
-16.275799	12.753782	0.360346
-16.672561	7.769803	0.365350
-16.227062	7.940512	0.370355
-16.278875	13.694101	0.375360
-16.778580	5.157520	0.380365
-17.122816	11.216354	0.385370
-17.686062	8.953992	0.390374
-17.324020	4.578788	0.395379
-18.298797	23.249127	0.400384
-18.829562	10.750043	0.405389
-18.962758	4.810439	0.410394
-18.733129	3.031289	0.415398
-18.618736	1.045568	0.420403
-19.060643	10.182232	0.425408
-19.105717	5.677827	0.430413
-19.521710	12.557829	0.435418
-19.997687	15.808897	0.440422
-20.246000	13.073244	0.445427
-20.489717	24.966143	0.450432
-20.436403	5.440561	0.455437
-20.772939	17.142354	0.460442
-21.608036	10.553420	0.465446
-21.515010	-2.777387	0.470451
-22.465555	18.540387	0.475456
-21.905835	8.904498	0.480461
-21.741026	17.022282	0.485466
-22.087461	19.126752	0.490470
-22.498177	5.166183	0.495475
-23.304244	13.062762	0.500480
-23.405148	10.139496	0.505485
-23.694813	5.572174	0.510490
-23.753528	18.695261	0.515494
-23.279814	14.334196	0.520499
-24.441398	17.857204	0.525504
-24.883981	6.701564	0.530509
-25.010757	10.676204	0.535514
-25.334400	12.916308	0.540518
-25.141251	10.051373	0.545523
-25.201636	16.859840	0.550528
-25.989706	12.386427	0.555533
-26.323936	7.478073	0.560538
-26.608513	18.279542	0.565542
-26.343774	7.202901	0.570547
-26.344564	12.625790	0.575552
-26.446388	11.759118	0.580557
-27.198000	6.264425	0.585562
-27.727683	16.971420	0.590566
-27.570415	12.479602	0.595571
-28.170041	18.233603	0.600576
-27.696752	9.981168	0.605581
-28.298575	10.474166	0.610586
-29.253500	14.227387	0.615590
-28.879658	15.820364	0.620595
-29.204962	14.957071	0.625600
-29.116592	2.775438	0.630605
-29.674160	10.898837	0.635610
-30.612251	6.531191	0.640614
-30.438467	4.191313	0.645619
-30.715219	16.734790	0.650624
-30.873743	5.465041	0.655629
-30.926646	2.891762	0.660634
-30.838858	16.763851	0.665638
-30.766167	4.182875	0.670643
-31.513816	18.046661	0.675648
-32.122943	9.141246	0.680653
-32.189755	15.716600	0.685658
-33.096049	19.446383	0.690662
-33.141280	8.396164	0.695667
-33.447142	13.936456	0.700672
-33.006596	9.776741	0.705677
-33.465723	9.646265	0.710682
-33.820269	18.145982	0.715686
-33.759624	0.903500	0.720691
-33.843479	16.248324	0.725696
-34.499713	11.450535	0.730701
-34.845601	14.010501	0.735706
-34.996610	13.895022	0.740710
-34.840567	1.756571	0.745715
-35.570562	7.163999	0.750720
-36.297143	7.037464	0.755725
-36.487186	1.524386	0.760730
-36.537475	4.240516	0.765734
-36.612864	6.732788	0.770739
-36.832259	1.777969	0.775744
-37.097280	12.117623	0.780749
-36.931905	10.494074	0.785754
-37.239566	13.851648	0.790758
-37.488788	-1.826834	0.795763
-38.214339	8.660908	0.800768
-37.950359	10.872214	0.805773
-38.208191	3.620194	0.810778
-38.769461	17.695223	0.815782
-39.093932	9.406434	0.820787
-39.737632	19.270750	0.825792
-39.560325	16.091919	0.830797
-39.683857	9.736347	0.835802
-39.475736	12.304421	0.840806
-40.369896	-0.871707	0.845811
-40.967660	9.390367	0.850816
-41.384182	12.916859	0.855821
-41.261098	15.621644	0.860826
-41.605177	15.229530	0.865830
-41.137957	12.612719	0.870835
-41.719329	17.775400	0.875840
-41.544165	8.579418	0.880845
-42.189954	6.118019	0.885850
-42.150231	12.262225	0.890854
-42.402649	0.200431	0.895859
-43.292044	18.287908	0.900864
-43.565564	10.241074	0.905869
-43.968397	8.285775	0.910874
-44.227580	9.544502	0.915878
-44.345104	6.842142	0.920883
-44.444375	9.043926	0.925888
-44.602672	22.445209	0.930893
-44.506326	6.744213	0.935898
-44.559655	10.178995	0.940902
-44.841718	10.856010	0.945907
-45.261755	13.490870	0.950912
-45.578524	15.135109	0.955917
-45.925140	8.033041	0.960922
-47.035115	8.808142	0.965926
-46.883734	4.472273	0.970931
-46.967968	10.930132	0.975936
-47.047009	14.941585	0.980941
-46.614306	15.677449	0.985946
-47.264816	12.821318	0.990950
-48.091150	13.396951	0.995955
-48.423170	21.522979	1.000960
-48.723991	9.949657	1.005965
-48.765347	6.605773	1.010970
-48.784516	14.027878	1.015974
-48.472430	6.034822	1.020979
-49.172931	4.907615	1.025984
-49.642229	5.028670	1.030989
-49.979790	4.290686	1.035994
-50.242938	2.123675	1.040998
-50.236418	7.944050	1.046003
-50.510313	12.039818	1.051008
-50.688659	7.834707	1.056013
-50.784363	11.276129	1.061018
-51.804513	13.321645	1.066022
-51.596553	12.751286	1.071027
-51.673525	15.202677	1.076032
-51.605373	11.471473	1.081037
-52.138518	14.215805	1.086042
-53.042290	8.795577	1.091046
-52.882494	7.574701	1.096051
-52.957727	6.548839	1.101056
-53.113178	17.061152	1.106061
-53.016633	15.543300	1.111066
-53.779978	13.767876	1.116070
-54.246001	13.154424	1.121075
-54.196951	14.156047	1.126080
-54.507177	13.043618	1.131085
-54.772649	14.464683	1.136090
-55.370152	14.210356	1.141094
-55.874276	11.280668	1.146099
-56.433422	18.635522	1.151104
-55.887017	19.989487	1.156109
-55.848164	8.343962	1.161114
-56.369920	13.218888	1.166118
-56.431671	6.901095	1.171123
-56.126153	15.882683	1.176128
-56.983788	16.058259	1.181133
-57.297551	15.806930	1.186138
-57.905512	13.956538	1.191142
-57.919165	13.566436	1.196147
-57.916658	10.462452	1.201152
-58.283845	16.227490	1.206157
-58.646347	11.121086	1.211162
-59.343643	12.454788	1.216166
-58.872841	14.602050	1.221171
-59.447605	25.319275	1.226176
-59.402099	9.591444	1.231181
-59.261967	17.652980	1.236186
-60.305477	21.239750	1.241190
-60.554847	12.784170	1.246195
-60.713247	17.621147	1.251200
-60.702278	19.906899	1.256205
-60.882474	17.062497	1.261210
-61.310431	19.730237	1.266214
-61.648895	14.616902	1.271219
-62.196407	22.764040	1.276224
-62.653554	29.109492	1.281229
-62.267266	16.840044	1.286234
-62.311782	12.740513	1.291238
-62.177382	12.953639	1.296243
-62.871254	17.975759	1.301248
-63.708708	18.825220	1.306253
-63.440258	3.660414	1.311258
-63.857025	12.922853	1.316262
-63.777524	10.942598	1.321267
-64.285928	16.188759	1.326272
-64.867048	17.981987	1.331277
-64.949719	5.238696	1.336282
-65.118816	10.023562	1.341286
-65.161442	10.729500	1.346291
-65.501352	22.036350	1.351296
-65.776533	15.445110	1.356301
-66.587482	8.792289	1.361306
-66.654482	9.116066	1.366310
-66.828473	14.252879	1.371315
-66.717141	17.044926	1.376320
-66.586844	16.660743	1.381325
-67.193147	6.834235	1.386330
-67.913810	20.206572	1.391334
-68.200453	15.951990	1.396339
-68.361631	12.842016	1.401344
-68.465187	15.272263	1.406349
-68.549734	15.295068	1.411354
-68.476121	13.072125	1.416358
-68.657064	17.741791	1.421363
-69.426335	22.364437	1.426368
-69.988607	21.032073	1.431373
-69.598752	5.459099	1.436378
-69.909312	12.787654	1.441382
-70.002266	12.463761	1.446387
-70.841742	23.855217	1.451392
-71.464187	16.090848	1.456397
-71.236791	8.142701	1.461402
-71.597683	19.386397	1.466406
-71.404058	11.832683	1.471411
-71.151944	12.157079	1.476416
-72.208205	15.628787	1.481421
-72.564734	-0.298632	1.486426
-72.993263	18.368366	1.491430
-72.650436	4.378319	1.496435
-72.978651	13.560444	1.501440
-73.269767	6.038394	1.506445
-74.078500	10.031304	1.511450
-74.186567	11.620695	1.516454
-74.139052	6.671511	1.521459
-74.624197	11.148394	1.526464
-74.681417	2.643730	1.531469
-74.529325	12.076463	1.536474
-74.577438	12.818061	1.541478
-75.142884	11.429248	1.546483
-75.658139	9.627608	1.551488
-75.916898	10.981182	1.556493
-75.847641	6.525303	1.561498
-76.322977	11.557472	1.566502
-76.698247	3.523424	1.571507
-76.919251	7.025607	1.576512
-77.149538	5.498856	1.581517
-77.148059	3.163831	1.586522
-77.341185	8.835153	1.591526
-77.845982	18.307542	1.596531
-78.065570	9.113305	1.601536
-78.468072	14.361853	1.606541
-78.325513	4.025701	1.611546
-79.005249	9.637229	1.616550
-79.579882	9.056616	1.621555
-80.048409	10.999882	1.626560
-79.906358	15.622101	1.631565
-79.986013	5.440990	1.636570
-80.327651	12.318832	1.641574
-80.010876	-0.433259	1.646579
-80.127717	7.339504	1.651584
-80.271710	10.639795	1.656589
-81.209653	-3.829770	1.661594
-81.715974	6.351535	1.666598
-81.621152	5.033271	1.671603
-81.897030	5.889652	1.676608
-81.549825	11.643990	1.681613
-82.423269	3.118524	1.686618
-82.988335	6.162088	1.691622
-83.197202	13.079238	1.696627
-83.386318	6.879480	1.701632
-83.232642	11.626426	1.706637
-83.165078	17.630227	1.711642
-84.073505	13.229465	1.716646
-83.605940	12.292559	1.721651
-84.466372	12.943141	1.726656
-84.718510	11.375521	1.731661
-84.669944	5.606758	1.736666
-85.442332	14.444028	1.741670
-86.051824	7.038305	1.746675
-86.197025	8.257026	1.751680
-86.108253	11.527172	1.756685
-85.938829	10.947031	1.761690
-86.646578	13.861093	1.766694
-86.499694	10.307379	1.771699
-86.353347	17.697220	1.776704
-86.576960	24.724253	1.781709
-87.404270	16.216864	1.786714
-87.711843	7.972890	1.791718
-87.834342	11.627318	1.796723
-88.279079	8.931938	1.801728
-88.878762	10.886265	1.806733
-89.078022	10.613831	1.811738
-89.010479	13.865157	1.816742
-89.060234	13.822399	1.821747
-88.957083	18.792400	1.826752
-89.273915	17.276045	1.831757
-89.596000	8.461704	1.836762
-90.622197	10.353147	1.841766
-90.610716	12.683110	1.846771
-90.778159	12.487949	1.851776
-90.836267	14.781360	1.856781
-90.907628	16.981934	1.861786
-91.366692	20.859945	1.866790
-91.935258	14.868339	1.871795
-92.013360	18.968230	1.876800
-92.583336	13.869028	1.881805
-92.348808	18.634944	1.886810
-92.581868	21.189888	1.891814
-92.783379	17.703419	1.896819
-93.268530	14.992225	1.901824
-93.984660	23.997856	1.906829
-93.742073	20.792977	1.911834
-93.903065	14.566664	1.916838
-93.695235	7.516929	1.921843
-93.804408	8.122562	1.926848
-94.650490	14.696632	1.931853
-94.886632	14.410995	1.936858
-95.246595	17.235761	1.941862
-95.084328	4.567989	1.946867
-95.656311	9.938006	1.951872
-96.207614	12.343498	1.956877
-96.880955	13.442495	1.961882
-96.797626	19.222361	1.966886
-97.047126	11.124313	1.971891
-96.695198	15.099873	1.976896
-97.336459	13.387581	1.981901
-96.724391	14.244034	1.986906
-97.129812	15.326359	1.991910
-97.723765	6.946926	1.996915
-98.252854	15.889270	2.006912
-98.493978	9.914666	2.016909
-97.224019	10.729504	2.026906
-97.117739	9.034039	2.036902
-96.734750	8.042820	2.046899
-96.098860	13.274749	2.056896
-94.908664	11.276392	2.066893
-94.786015	12.068267	2.076890
-94.601953	8.592971	2.086886
-94.494794	8.364068	2.096883
-93.317355	11.065584	2.106880
-93.011340	7.891129	2.116877
-91.853171	8.771002	2.126874
-91.955934	2.695524	2.136870
-91.432964	9.567068	2.146867
-91.192334	16.460680	2.156864
-90.309033	8.019553	2.166861
-90.124866	10.357187	2.176858
-89.573097	12.906484	2.186854
-88.870979	12.882130	2.196851
-88.526940	6.055559	2.206848
-87.457250	6.749724	2.216845
-87.221350	8.509044	2.226842
-87.159117	11.797122	2.236838
-86.828336	12.160407	2.246835
-86.074806	16.939913	2.256832
-85.137887	11.496644	2.266829
-84.539112	14.355359	2.276826
-84.561222	11.922902	2.286822
-84.250122	9.558612	2.296819
-83.200146	10.636005	2.306816
-82.866692	8.461449	2.316813
-82.692749	14.291620	2.326810
-81.569276	12.946787	2.336806
-81.393413	10.857113	2.346803
-81.084043	8.312528	2.356800
-80.231010	12.385858	2.366797
-79.594717	9.403574	2.376794
-79.441402	16.114463	2.386790
-79.266878	10.477042	2.396787
-78.277937	11.459461	2.406784
-78.517855	11.398983	2.416781
-77.645174	6.269892	2.426778
-76.645996	7.200023	2.436774
-76.063987	10.349636	2.446771
-75.954724	10.228108	2.456768
-75.688539	11.374463	2.466765
-74.828660	10.609463	2.476762
-74.771626	11.199375	2.486758
-73.641616	15.774172	2.496755
-73.261271	12.214267	2.506752
-72.996257	16.138982	2.516749
-72.096131	11.373057	2.526746
-71.573986	13.128708	2.536742
-71.714184	14.880436	2.546739
-71.276593	14.549072	2.556736
-70.450114	7.374474	2.566733
-69.854968	13.715190	2.576730
-68.877692	16.213656	2.586726
-68.581442	18.682617	2.596723
-68.938884	16.283695	2.606720
-68.173418	18.596771	2.616717
-67.593688	15.398434	2.626714
-66.493001	11.038242	2.636710
-66.290944	14.374104	2.646707
-65.785734	14.371102	2.656704
-65.496856	10.328182	2.666701
-64.608802	13.664261	2.676698
-64.589813	13.879996	2.686694
-63.950518	22.393258	2.696691
-63.349692	12.903494	2.706688
-63.097613	11.147169	2.716685
-62.062583	10.123475	2.726682
-61.684423	11.622920	2.736678
-61.604849	13.539784	2.746675
-60.661379	9.191556	2.756672
-60.044564	13.929131	2.766669
-60.031537	7.379340	2.776666
-59.509175	13.706119	2.786662
-58.986272	10.576876	2.796659
-58.423419	17.559387	2.806656
-57.358055	10.264994	2.816653
-57.128533	13.466672	2.826650
-57.008002	15.750922	2.836646
-56.858733	20.064410	2.846643
-55.836523	11.877118	2.856640
-55.057085	13.202814	2.866637
-54.498526	4.948789	2.876634
-54.304395	12.990104	2.886630
-54.266445	17.818381	2.896627
-53.403572	13.403586	2.906624
-52.566170	14.609326	2.916621
-52.677569	13.945831	2.926618
-51.379751	13.777455	2.936614
-51.503560	19.457880	2.946611
-51.074040	17.312620	2.956608
-50.078024	11.736549	2.966605
-49.999558	6.427793	2.976602
-49.151745	12.190392	2.986598
-48.488113	6.504844	2.996595
-48.009925	5.429019	3.006592
-47.990572	11.362609	3.016589
-47.875983	10.074490	3.026586
-47.025583	9.393342	3.036582
-46.058416	8.706569	3.046579
-45.437082	7.506944	3.056576
-45.411126	9.688803	3.066573
-45.112125	8.444649	3.076570
-44.097897	8.827561	3.086566
-44.007985	13.286564	3.096563
-43.492991	12.737165	3.106560
-42.787115	11.115645	3.116557
-42.447281	16.295766	3.126554
-41.438808	12.748316	3.136550
-40.951503	15.814570	3.146547
-40.930651	11.449347	3.156544
-40.872561	9.732921	3.166541
-39.926686	14.308065	3.176538
-39.252743	11.481441	3.186534
-38.685231	11.408490	3.196531
-38.274725	14.261862	3.206528
-37.849446	18.079105	3.216525
-36.960627	6.174690	3.226522
-36.906346	14.440659	3.236518
-36.589332	10.713280	3.246515
-35.701614	6.608209	3.256512
-35.177101	11.772064	3.266509
-34.854905	4.990097	3.276506
-33.689438	10.658577	3.286502
-33.580105	15.817794	3.296499
-33.490180	15.319159	3.306496
-33.090980	9.009801	3.316493
-31.851653	10.067036	3.326490
-31.888660	8.194449	3.336486
-31.587609	5.042948	3.346483
-30.813771	5.298800	3.356480
-30.400349	12.881269	3.366477
-29.300996	4.304924	3.376474
-29.226369	7.334468	3.386470
-29.363501	5.686645	3.396467
-28.259319	9.806161	3.406464
-27.537811	9.686907	3.416461
-27.523523	10.502097	3.426458
-26.879116	9.251341	3.436454
-26.354825	12.973875	3.446451
-25.139204	7.816395	3.456448
-25.450612	13.526213	3.466445
-24.829614	8.617125	3.476442
-24.618108	10.329585	3.486438
-23.756968	14.366807	3.496435
-23.384000	13.507041	3.506432
-22.015863	13.178765	3.516429
-22.203293	15.216662	3.526426
-21.860552	9.929852	3.536422
-21.543732	9.861335	3.546419
-20.456329	15.399499	3.556416
-20.348480	5.923623	3.566413
-19.964279	12.905618	3.576410
-19.112673	11.559041	3.586406
-18.895669	14.319188	3.596403
-18.340754	14.203862	3.606400
-17.479668	13.679433	3.616397
-17.531359	4.858951	3.626394
-16.345120	11.518875	3.636390
-16.202643	11.860981	3.646387
-15.945091	11.741563	3.656384
-15.222333	6.205142	3.666381
-14.637471	5.521253	3.676378
-14.480864	6.611919	3.686374
-13.808229	7.434830	3.696371
-13.297735	10.459438	3.706368
-12.702183	10.321907	3.716365
-12.046335	7.561477	3.726362
-12.098206	11.773432	3.736358
-10.646374	10.953703	3.746355
-10.797884	11.820213	3.756352
-10.064268	8.242972	3.766349
-9.988336	9.536348	3.776346
-9.303591	10.236985	3.786342
-8.595501	8.086094	3.796339
-8.496444	11.048456	3.806336
-7.644248	11.415578	3.816333
-7.202851	10.206134	3.826330
-6.885950	8.518850	3.836326
-6.168575	14.029461	3.846323
-5.898014	17.357762	3.856320
-4.951261	11.063981	3.866317
-4.418216	17.379591	3.876314
-4.589282	20.606025	3.886310
-3.973833	23.275235	3.896307
-3.569406	34.134654	3.906304
-2.820628	39.181019	3.916301
-2.596625	49.682242	3.926298
-2.208696	55.510583	3.936294
-1.545230	72.823488	3.946291
-1.344297	83.052744	3.956288
-0.536190	92.369572	3.966285
-0.410709	119.419210	3.976282
0.000000	121.084654	3.981286
0.319690	143.105235	3.986291
0.511974	144.381819	3.991296
0.891679	149.814737	3.996301
0.420852	146.958900	4.001306
0.345312	160.454894	4.006310
0.973382	162.327597	4.011315
0.980280	171.688257	4.016320
1.049761	168.124492	4.021325
0.911605	176.368915	4.026330
1.146813	183.222882	4.031334
1.392181	165.679207	4.036339
1.353452	175.084984	4.041344
1.302329	173.226418	4.046349
1.297435	174.410511	4.051354
0.858382	169.167352	4.056358
1.376074	168.175131	4.061363
1.075903	172.528157	4.066368
1.155271	180.523361	4.071373
0.993980	167.437919	4.076378
1.131539	173.006861	4.081382
1.368158	174.463166	4.086387
0.913677	180.975935	4.091392
0.908025	174.661944	4.096397
1.019397	180.456458	4.101402
1.213523	179.552899	4.106406
1.579657	166.204483	4.111411
1.242114	176.410062	4.116416
1.229262	173.121791	4.121421
1.266301	185.296680	4.126426
1.249483	179.639343	4.131430
1.569513	172.869358	4.136435
1.444791	180.643435	4.141440
1.441882	178.502065	4.146445
1.397162	180.790237	4.151450
1.450237	178.061119	4.156454
1.364827	178.675689	4.161459
1.320716	182.966450	4.166464
1.765239	190.964558	4.171469
1.634386	186.106546	4.176474
1.378112	181.426375	4.181478
1.376010	180.888924	4.186483
1.495064	188.273629	4.191488
1.443947	183.181657	4.196493
1.509403	189.385171	4.201498
1.262958	198.526108	4.206502
1.571479	202.113043	4.211507
1.480182	206.132789	4.216512
1.657181	198.923288	4.221517
1.913415	209.222517	4.226522
1.597091	207.250474	4.231526
1.767743	198.355661	4.236531
1.327862	199.702824	4.241536
1.643270	200.460241	4.246541
1.823583	196.066007	4.251546
1.601635	205.358135	4.256550
1.852626	204.467812	4.261555
1.553005	209.437702	4.266560
1.724616	214.934883	4.271565
1.646642	206.901610	4.276570
1.416370	209.449816	4.281574
1.976160	203.885628	4.286579
1.883851	209.069812	4.291584
1.854634	205.246253	4.296589
1.971769	208.742952	4.301594
1.701427	210.952581	4.306598
2.133691	207.417389	4.311603
1.926598	202.235954	4.316608
2.305351	197.345549	4.321613
1.682339	187.024832	4.326618
1.555253	184.504278	4.331622
1.959974	191.201973	4.336627
1.724883	200.167122	4.341632
1.430759	203.370748	4.346637
1.597024	212.478665	4.351642
1.495587	212.741401	4.356646
1.882635	213.579344	4.361651
1.744173	208.700370	4.366656
1.752043	206.032116	4.371661
1.727730	213.217827	4.376666
1.655022	209.030916	4.381670
1.977284	210.246011	4.386675
2.236571	223.240331	4.391680
2.120917	221.461475	4.396685
2.378419	215.277084	4.401690
2.087498	221.729439	4.406694
2.514904	216.537171	4.411699
2.043556	212.140632	4.416704
2.264871	216.307555	4.421709
2.087698	216.098095	4.426714
2.088528	212.700104	4.431718
1.975541	211.382747	4.436723
2.129480	206.299770	4.441728
2.016879	202.707578	4.446733
2.016541	203.362604	4.451738
1.714182	210.373576	4.456742
2.134904	207.387531	4.461747
2.107841	218.357585	4.466752
2.586181	228.261351	4.471757
2.070463	222.036752	4.476762
2.155576	224.766503	4.481766
2.497520	222.887476	4.486771
2.164575	217.029718	4.491776
2.386676	214.688570	4.496781
2.143256	221.854830	4.501786
2.241299	226.623210	4.506790
2.650711	224.369774	4.511795
2.221431	226.401824	4.516800
2.342864	218.299337	4.521805
2.379096	223.931629	4.526810
2.188928	219.453066	4.531814
2.513317	221.351211	4.536819
2.250967	227.748471	4.541824
2.317705	228.598635	4.546829
2.650778	233.947135	4.551834
2.457777	232.987169	4.556838
2.621265	230.481193	4.561843
2.603159	227.399383	4.566848
2.246928	218.536492	4.571853
2.426540	211.465784	4.576858
2.409808	227.097674	4.581862
2.798483	222.753047	4.586867
2.371960	226.565888	4.591872
2.810820	225.294946	4.596877
2.264244	206.960974	4.601882
2.247634	216.553134	4.606886
2.427892	227.721669	4.611891
2.589555	228.436736	4.616896
2.677901	231.352646	4.621901
2.528075	228.383224	4.626906
2.584479	221.572266	4.631910
2.773108	233.812024	4.636915
2.676329	229.265041	4.641920
2.525129	233.550447	4.646925
2.572197	237.257450	4.651930
2.721630	228.524137	4.656934
2.379034	231.020341	4.661939
2.685689	230.402874	4.666944
2.683189	233.450079	4.671949
2.754669	229.537969	4.676954
2.609120	242.051558	4.681958
2.919518	227.724720	4.686963
2.777169	240.490911	4.691968
2.800874	240.060149	4.696973
2.751292	229.323688	4.701978
2.861136	231.521208	4.706982
3.126445	234.406228	4.711987
2.966856	233.365095	4.716992
2.720331	237.940689	4.721997
2.663905	234.668725	4.727002
3.027790	238.699418	4.732006
2.889061	235.427695	4.737011
2.649291	238.296937	4.742016
2.911165	229.808603	4.747021
2.957982	235.518335	4.752026
2.532688	237.087846	4.757030
2.770445	233.481883	4.762035
3.071327	245.482593	4.767040
2.831305	240.486644	4.772045
3.023857	235.438738	4.777050
2.846943	236.640296	4.782054
2.902020	232.268840	4.787059
2.956646	235.882908	4.792064
2.915127	239.065943	4.797069
2.911338	230.742621	4.802074
2.904352	228.168442	4.807078
3.186554	243.193514	4.812083
3.044992	246.657986	4.817088
3.162672	248.424003	4.822093
3.231310	246.761805	4.827098
3.158408	247.254192	4.832102
2.931562	236.507535	4.837107
3.187792	247.034581	4.842112
3.001348	259.355269	4.847117
2.863447	261.079073	4.852122
2.775662	269.448527	4.857126
3.303124	255.366072	4.862131
3.319262	268.566204	4.867136
3.153740	263.938233	4.872141
3.150093	266.492068	4.877146
2.755488	270.850422	4.882150
3.212490	257.332674	4.887155
3.039469	262.766806	4.892160
3.223643	264.601501	4.897165
3.323751	266.743603	4.902170
3.254689	267.925101	4.907174
3.747622	261.953747	4.912179
3.287785	260.924854	4.917184
3.303684	256.363374	4.922189
3.778116	257.991236	4.927194
3.517455	261.651545	4.932198
3.540066	258.901878	4.937203
3.349500	264.443165	4.942208
3.368227	255.942293	4.947213
3.301067	256.968466	4.952218
3.385142	264.779469	4.957222
3.420609	265.935098	4.962227
3.254004	251.024906	4.967232
3.188571	265.765937	4.972237
3.104976	253.949602	4.977242
3.036980	267.808334	4.982246
3.394471	269.606383	4.987251
3.880129	279.689368	4.992256
3.731314	270.831918	4.997261
3.571676	258.299818	5.002266
3.245396	266.146643	5.007270
3.505964	258.984137	5.012275
3.433240	275.431615	5.017280
3.260433	290.309715	5.022285
3.603825	290.474281	5.027290
3.767572	297.969089	5.032294
3.707231	289.006018	5.037299
3.867253	297.940947	5.042304
3.623579	286.725488	5.047309
3.734309	287.154302	5.052314
3.747758	289.423882	5.057318
3.799368	290.054953	5.062323
3.843117	277.222048	5.067328
3.286797	270.427979	5.072333
3.959896	283.987105	5.077338
3.904673	283.030859	5.082342
3.822330	274.289546	5.087347
3.723937	278.120590	5.092352
3.744829	282.027860	5.097357
4.119024	274.243256	5.102362
3.528397	271.678257	5.107366
3.883321	272.603495	5.112371
3.730232	285.172081	5.117376
3.796852	285.187019	5.122381
4.374059	278.281784	5.127386
3.727123	282.100698	5.132390
3.819104	261.009013	5.137395
3.651047	274.326596	5.142400
3.760720	278.586958	5.147405
3.966008	282.620364	5.152410
3.844556	291.146966	5.157414
3.792158	277.886189	5.162419
3.891626	286.245295	5.167424
4.233999	282.442593	5.172429
4.231957	281.354625	5.177434
4.257800	284.590391	5.182438
3.759608	273.351542	5.187443
3.591984	283.657111	5.192448
3.622582	282.317252	5.197453
4.171498	280.488049	5.202458
3.971872	284.189421	5.207462
4.048103	279.359049	5.212467
4.196949	275.880905	5.217472
3.946604	286.161471	5.222477
4.146370	287.718474	5.227482
4.047509	275.746326	5.232486
4.141233	280.784322	5.237491
3.904370	286.636596	5.242496
4.028402	285.570005	5.247501
4.010510	281.630757	5.252506
4.112485	286.262493	5.257510
3.972497	270.484392	5.262515
3.540663	281.695079	5.267520
3.902091	299.871604	5.272525
4.490159	304.724582	5.277530
4.610745	312.482429	5.282534
4.291327	299.092627	5.287539
3.819473	309.433224	5.292544
4.297259	315.088112	5.297549
4.439366	307.058277	5.302554
4.005413	309.844059	5.307558
4.414327	307.090806	5.312563
4.604579	314.157517	5.317568
4.531290	306.838489	5.322573
4.500166	310.690639	5.327578
4.722468	311.816997	5.332582
4.223957	296.278548	5.337587
4.011555	302.781906	5.342592
4.185793	306.892950	5.347597
4.315185	312.491691	5.352602
4.010084	315.750841	5.357606
4.329516	309.113778	5.362611
4.219673	312.880184	5.367616
4.419066	307.457855	5.372621
4.790937	306.254352	5.377626
4.496720	308.774625	5.382630
4.796663	309.784411	5.387635
4.546113	308.456963	5.392640
4.425304	311.405656	5.397645
4.614240	314.878471	5.402650
4.504865	311.485073	5.407654
4.530908	304.017602	5.412659
4.687305	310.760578	5.417664
4.565839	307.726587	5.422669
4.800958	299.100039	5.427674
4.039601	315.215678	5.432678
4.450909	307.032931	5.437683
4.633942	314.372861	5.442688
4.385845	314.361178	5.447693
4.414348	309.272515	5.452698
4.150768	320.055058	5.457702
4.628448	315.620531	5.462707
4.636713	329.761598	5.467712
4.562269	324.322056	5.472717
4.733154	331.920167	5.477722
4.523037	326.343691	5.482726
4.726746	327.741888	5.487731
4.792474	333.189255	5.492736
4.753218	330.341700	5.497741
4.959669	318.530499	5.502746
4.353881	337.485044	5.507750
4.771723	328.896293	5.512755
4.996364	326.203549	5.517760
5.121994	336.966250	5.522765
4.916224	319.474126	5.527770
4.911882	337.366306	5.532774
5.206509	323.684119	5.537779
5.042959	328.629558	5.542784
4.749765	326.315348	5.547789
4.905355	325.016014	5.552794
4.831435	329.687977	5.557798
4.880984	332.296763	5.562803
4.821655	333.970297	5.567808
4.798597	337.786387	5.572813
4.920429	336.830871	5.577818
4.674533	329.197185	5.582822
4.801239	337.593176	5.587827
4.847423	337.487927	5.592832
5.031909	341.492967	5.597837
4.923191	330.990343	5.602842
5.148460	336.270341	5.607846
4.912571	333.089755	5.612851
5.022180	341.339727	5.617856
5.041449	336.261994	5.622861
5.091362	343.078616	5.627866
5.233682	348.358959	5.632870
5.219043	344.352747	5.637875
4.956097	340.774593	5.642880
4.992309	349.023413	5.647885
5.422203	351.531479	5.652890
5.071453	351.440965	5.657894
5.399894	356.834521	5.662899
5.168702	358.639392	5.667904
5.061698	349.642471	5.672909
5.524417	352.816127	5.677914
5.456719	346.546598	5.682918
5.076067	331.790101	5.687923
5.137392	337.886743	5.692928
5.434590	345.246765	5.697933
5.236067	348.242443	5.702938
5.120786	344.210870	5.707942
5.686577	352.421011	5.712947
5.711861	344.754321	5.717952
5.246763	342.220264	5.722957
5.531654	337.066111	5.727962
4.982716	340.395108	5.732966
5.028463	331.292004	5.737971
5.340960	350.975901	5.742976
5.274432	354.599484	5.747981
5.558890	357.392936	5.752986
5.427974	359.308649	5.757990
5.284246	357.445591	5.762995
5.280410	364.023863	5.768000
5.279548	361.005768	5.773005
5.349578	358.922552	5.778010
5.387855	360.466898	5.783014
5.294500	361.731304	5.788019
5.447820	358.318884	5.793024
4.920145	357.968182	5.798029
5.591027	352.149255	5.803034
5.337450	361.379979	5.808038
5.342910	366.321095	5.813043
5.370239	373.451322	5.818048
5.870081	383.718810	5.823053
5.971694	387.145208	5.828058
5.369652	377.998040	5.833062
5.752724	370.708725	5.838067
5.830122	365.691481	5.843072
5.687757	360.243588	5.848077
5.797889	358.650810	5.853082
5.547513	366.416182	5.858086
5.496051	366.519225	5.863091
6.130741	376.645356	5.868096
5.357574	361.431465	5.873101
5.527506	360.205813	5.878106
5.679331	377.168709	5.883110
5.917191	387.527868	5.888115
5.847034	383.172833	5.893120
5.760633	389.628006	5.898125
6.481156	383.257112	5.903130
6.177604	376.758764	5.908134
5.850263	361.611065	5.913139
5.883676	359.577880	5.918144
5.669703	359.564014	5.923149
5.727451	350.924102	5.928154
5.447937	365.028027	5.933158
5.539553	357.116815	5.938163
6.060353	370.965632	5.943168
6.158722	384.099181	5.948173
6.063942	375.979878	5.953178
5.733154	371.374609	5.958182
5.707853	370.878753	5.963187
5.905938	375.156923	5.968192
5.938889	394.008286	5.973197
5.948615	390.415873	5.978202
5.747034	389.011141	5.983206
5.900000	390.170514	5.988211
6.217996	381.262016	5.993216
5.688586	394.032013	5.998221
5.725588	386.752621	6.003226
5.924376	384.475217	6.008230
6.121000	382.448095	6.013235
6.238718	392.724839	6.018240
5.963298	385.978465	6.023245
6.107452	376.647942	6.028250
5.851053	387.014938	6.033254
5.817998	387.431481	6.038259
6.266015	378.806341	6.043264
5.894629	385.002436	6.048269
6.392843	380.501399	6.053274
6.050290	385.690041	6.058278
5.754545	379.674536	6.063283
6.317176	384.120224	6.068288
6.085163	383.701049	6.073293
6.187083	376.427309	6.078298
5.941033	385.840369	6.083302
5.742409	384.099807	6.088307
6.083341	380.610530	6.093312
5.639861	388.491591	6.098317
5.716920	388.017663	6.103322
5.851541	394.317981	6.108326
5.728892	385.494341	6.113331
5.653418	390.913228	6.118336
5.820616	387.217047	6.123341
5.861362	382.322603	6.128346
6.084962	376.133976	6.133350
6.018399	378.539493	6.138355
5.976831	387.183342	6.143360
5.940824	391.143845	6.148365
6.237873	399.019617	6.153370
6.225822	392.839432	6.158374
6.217131	390.028209	6.163379
6.162753	387.379172	6.168384
6.144054	384.623303	6.173389
6.295651	386.162551	6.178394
6.205833	396.446503	6.183398
6.152693	391.750269	6.188403
6.495865	384.210930	6.193408
6.050933	392.206118	6.198413
6.141833	374.993332	6.203418
5.699951	364.871927	6.208422
6.064222	379.517251	6.213427
6.358402	373.814289	6.218432
5.854029	371.922312	6.223437
5.828468	365.937248	6.228442
5.620097	375.107111	6.233446
5.849538	381.487483	6.238451
5.944771	376.641452	6.243456
6.101708	382.093527	6.248461
6.033283	381.784766	6.253466
5.897702	385.517253	6.258470
6.117930	388.004391	6.263475
6.012323	386.945299	6.268480
5.805193	386.120418	6.273485
6.047539	380.640716	6.278490
6.310611	388.866666	6.283494
5.903737	389.851157	6.288499
6.027416	387.775351	6.293504
6.415916	392.381205	6.298509
5.975500	380.826343	6.303514
5.957515	383.297018	6.308518
6.123490	383.119214	6.313523
5.801814	368.230056	6.318528
5.899260	381.923746	6.323533
6.087606	377.781316	6.328538
5.990882	390.717641	6.333542
5.844703	387.532480	6.338547
6.299775	389.476608	6.343552
5.862076	376.567201	6.348557
6.152334	379.138280	6.353562
5.933513	376.157496	6.358566
5.721122	379.417951	6.363571
5.993241	384.140116	6.368576
5.895628	388.341230	6.373581
6.363619	385.480631	6.378586
6.006958	386.049120	6.383590
5.949482	383.372095	6.388595
6.175193	382.618605	6.393600
6.137438	380.204253	6.398605
5.842336	371.828429	6.403610
5.725591	369.008829	6.408614
6.116628	381.416295	6.413619
6.187981	380.120664	6.418624
5.707166	376.396300	6.423629
6.023895	381.608196	6.428634
5.979694	389.939239	6.433638
6.210868	390.279581	6.438643
5.952774	378.496832	6.443648
5.901090	380.545669	6.448653
6.136918	378.230824	6.453658
5.876090	382.432199	6.458662
6.018033	383.533186	6.463667
6.065366	396.582989	6.468672
5.741643	398.449819	6.473677
6.201615	386.516591	6.478682
5.907154	392.741766	6.483686
5.804623	397.763087	6.488691
5.847935	395.247443	6.493696
5.256408	393.831040	6.498701
5.638231	384.314574	6.503706
5.673236	395.623034	6.508710
6.016825	397.549828	6.513715
6.320992	387.539314	6.518720
6.104177	393.853566	6.523725
5.865938	396.013894	6.528730
6.061411	393.284580	6.533734
6.280593	386.274045	6.538739
6.254248	390.441846	6.543744
6.096190	394.703054	6.548749
6.198053	389.688298	6.553754
6.229778	385.238203	6.558758
6.028024	391.474163	6.563763
6.032179	389.154485	6.568768
6.224047	399.213965	6.573773
6.294738	381.428522	6.578778
5.844866	379.344502	6.583782
6.014062	383.886636	6.588787
6.026486	377.259685	6.593792
5.958105	392.529643	6.598797
6.139801	384.303741	6.603802
5.948205	382.887954	6.608806
5.873531	373.186748	6.613811
6.163003	378.614891	6.618816
6.008624	385.605910	6.623821
5.829569	369.625029	6.628826
5.944232	385.796469	6.633830
6.000211	390.138039	6.638835
6.237355	390.126259	6.643840
5.797916	385.848066	6.648845
5.918141	387.676975	6.653850
5.932590	392.025051	6.658854
5.885379	396.072734	6.663859
5.862715	390.732630	6.668864
5.561164	395.041632	6.673869
5.991319	385.011379	6.678874
6.177347	385.504330	6.683878
6.246266	397.446573	6.688883
6.356413	382.733360	6.693888
5.938465	391.271663	6.698893
6.262602	384.244684	6.703898
5.670259	382.309540	6.708902
6.030930	386.555912	6.713907
6.205907	385.974891	6.718912
5.895946	388.216060	6.723917
6.507391	378.306106	6.728922
6.157816	375.431233	6.733926
6.243367	364.841201	6.738931
5.910261	357.360376	6.743936
5.682003	367.030073	6.748941
6.045307	358.927591	6.753946
6.003776	358.700041	6.758950
6.164388	356.586813	6.763955
5.851310	355.405202	6.768960
5.701942	362.461867	6.773965
6.039020	358.739075	6.778970
5.848644	356.813721	6.783974
5.557038	382.869346	6.788979
6.224412	381.281008	6.793984
6.405364	386.991920	6.798989
6.263813	375.836335	6.803994
6.055088	360.818752	6.808998
5.896819	362.498299	6.814003
6.105281	361.690564	6.819008
5.841184	363.630308	6.824013
5.936451	366.659054	6.829018
6.042952	362.241542	6.834022
6.046524	368.382046	6.839027
5.903285	353.521892	6.844032
6.087652	364.205803	6.849037
6.105939	360.017254	6.854042
5.928064	367.429573	6.859046
5.896504	362.710982	6.864051
6.113867	360.626828	6.869056
5.824562	355.894838	6.874061
5.859110	355.671186	6.879066
5.844077	362.323980	6.884070
5.697459	372.892072	6.889075
6.094265	368.609412	6.894080
5.886952	383.603731	6.899085
6.071828	384.900477	6.904090
5.933329	387.386871	6.909094
6.132091	390.741099	6.914099
6.286168	379.162696	6.919104
5.999664	386.427523	6.924109
5.806340	373.229887	6.929114
6.170875	392.070424	6.934118
5.841564	389.445481	6.939123
6.158925	381.375499	6.944128
5.991267	392.174694	6.949133
6.150534	384.167447	6.954138
5.728639	383.218025	6.959142
5.752319	385.413246	6.964147
6.165052	384.687402	6.969152
5.551141	384.255296	6.974157
6.125828	383.902721	6.979162
6.161032	383.438514	6.984166
5.969568	401.287308	6.989171
6.254073	393.902693	6.994176
6.071230	394.295248	6.999181
6.343185	390.762992	7.004186
5.985387	371.285601	7.009190
5.583303	367.627998	7.014195
5.883265	370.748062	7.019200
5.462655	393.840421	7.024205
6.390721	389.161298	7.029210
6.280744	394.696327	7.034214
5.804401	386.535560	7.039219
6.061301	390.791864	7.044224
6.165077	393.756004	7.049229
6.512485	388.474979	7.054234
6.265950	385.337181	7.059238
5.930989	371.908630	7.064243
6.055909	360.268367	7.069248
5.799154	370.059592	7.074253
5.915294	362.460919	7.079258
5.818153	362.925469	7.084262
5.842418	365.667939	7.089267
6.206612	357.290065	7.094272
5.742068	362.659170	7.099277
6.254869	368.042827	7.104282
5.945191	364.997185	7.109286
5.660372	370.825363	7.114291
5.986580	371.242565	7.119296
5.937017	386.221661	7.124301
6.237610	390.439480	7.129306
6.180359	391.391340	7.134310
5.684411	378.016483	7.139315
6.199347	380.416314	7.144320
6.103772	388.480152	7.149325
6.026466	373.097109	7.154330
5.922129	369.927543	7.159334
5.803157	373.708047	7.164339
6.064752	379.305078	7.169344
6.313940	376.668592	7.174349
6.072354	372.859288	7.179354
5.992088	366.401892	7.184358
5.984868	368.159016	7.189363
6.160714	363.907814	7.194368
6.109282	371.891959	7.199373
6.163588	362.411002	7.204378
6.087247	372.139158	7.209382
5.621473	364.732902	7.214387
5.705232	359.657714	7.219392
5.832988	361.447474	7.224397
5.827583	355.066939	7.229402
6.124409	370.254347	7.234406
5.757740	382.255337	7.239411
6.566940	376.658346	7.244416
5.902757	377.616712	7.249421
6.302721	365.515725	7.254426
6.069865	362.062569	7.259430
6.017259	356.942306	7.264435
6.423321	351.101596	7.269440
6.045812	371.906053	7.274445
5.999119	360.754598	7.279450
5.728158	365.264449	7.284454
6.270923	363.942415	7.289459
6.416060	360.157944	7.294464
6.107116	359.507209	7.299469
6.076665	354.073421	7.304474
5.892546	357.876785	7.309478
6.202111	361.751498	7.314483
6.144252	351.898969	7.319488
5.966612	355.191940	7.324493
5.821686	351.861053	7.329498
6.120020	361.457731	7.334502
5.869538	363.638956	7.339507
5.799360	364.475778	7.344512
5.749972	363.006072	7.349517
6.319886	370.269589	7.354522
6.350876	364.070016	7.359526
5.939646	365.823999	7.364531
5.999033	367.643455	7.369536
5.984863	368.278508	7.374541
6.286055	361.214003	7.379546
6.080926	364.542921	7.384550
5.987430	375.102691	7.389555
5.993289	364.221417	7.394560
6.121349	365.188534	7.399565
5.814354	365.363253	7.404570
6.069482	355.350949	7.409574
5.888522	371.508582	7.414579
6.070784	362.580230	7.419584
5.784098	364.200802	7.424589
5.880989	364.622296	7.429594
6.018055	363.673883	7.434598
5.414800	368.757831	7.439603
5.865579	353.962797	7.444608
5.831387	361.805029	7.449613
5.757183	370.049012	7.454618
5.771616	370.565685	7.459622
5.699889	374.500142	7.464627
5.598770	375.196276	7.469632
5.752818	383.420321	7.474637
6.013934	395.341940	7.479642
6.011382	394.845683	7.484646
5.966865	393.077811	7.489651
6.674886	374.797037	7.494656
6.059236	382.132416	7.499661
5.714844	368.895176	7.504666
6.104538	362.310362	7.509670
5.906252	374.917730	7.514675
6.001657	383.464184	7.519680
5.618490	390.475232	7.524685
5.878749	390.374407	7.529690
5.925639	394.866102	7.534694
6.063289	398.116009	7.539699
6.126346	392.164508	7.544704
6.345446	402.488649	7.549709
6.141325	393.285454	7.554714
6.182017	379.484820	7.559718
5.653527	373.891772	7.564723
6.197893	370.870508	7.569728
5.890461	379.859737	7.574733
5.689586	383.909347	7.579738
5.987034	388.624381	7.584742
5.981085	394.706273	7.589747
6.370263	393.019149	7.594752
6.492901	386.802044	7.599757
5.474934	384.528617	7.604762
5.750628	376.306973	7.609766
6.140873	392.014451	7.614771
6.219126	381.425552	7.619776
5.945861	377.880645	7.624781
5.626779	372.612300	7.629786
6.380769	388.155212	7.634790
6.048806	382.895210	7.639795
6.130627	368.388932	7.644800
6.073324	375.023043	7.649805
6.101103	368.162730	7.654810
5.948405	370.717786	7.659814
6.058305	374.095426	7.664819
5.984191	364.134703	7.669824
5.681676	371.658303	7.674829
5.861303	372.291466	7.679834
6.223908	374.816407	7.684838
5.982845	380.694680	7.689843
6.302350	364.689474	7.694848
6.104772	368.153254	7.699853
5.930045	366.478554	7.704858
5.951150	372.537217	7.709862
5.975791	372.166417	7.714867
6.011350	361.764558	7.719872
5.942117	365.217721	7.724877
5.725269	363.872332	7.729882
5.941209	371.286225	7.734886
5.893319	381.414899	7.739891
6.193792	379.865065	7.744896
6.272498	379.314947	7.749901
6.094165	372.404666	7.754906
5.825724	370.801598	7.759910
5.903693	366.360082	7.764915
5.944633	368.802539	7.769920
5.924295	375.978202	7.774925
5.901477	372.447840	7.779930
5.996679	374.103494	7.784934
5.836139	385.689365	7.789939
6.252248	378.211369	7.794944
6.114584	379.242267	7.799949
6.096488	373.566086	7.804954
5.843907	367.711505	7.809958
5.368153	374.686433	7.814963
6.112429	387.978216	7.819968
6.226016	399.435722	7.824973
6.104694	398.901125	7.829978
6.146192	388.210411	7.834982
6.024619	384.315860	7.839987
6.013379	374.582568	7.844992
5.986821	379.604636	7.849997
6.143485	374.657229	7.855002
6.251242	375.238376	7.860006
5.967656	373.662991	7.865011
5.846044	371.992624	7.870016
5.754725	369.184859	7.875021
5.925511	374.622105	7.880026
6.019663	376.660747	7.885030
6.235360	379.196051	7.890035
6.003747	378.621786	7.895040
5.820403	372.933530	7.900045
5.908056	371.660657	7.905050
6.062823	378.875325	7.910054
6.086431	381.858352	7.915059
6.278442	378.971390	7.920064
5.848484	373.328102	7.925069
5.656081	368.805558	7.930074
5.789405	381.993740	7.935078
5.890706	391.839611	7.940083
6.054966	393.803993	7.945088
6.030616	402.565377	7.950093
6.376159	393.715833	7.955098
6.320483	384.220458	7.960102
5.975827	387.606044	7.965107
6.132661	369.655251	7.970112
6.038609	370.597056	7.975117
6.153125	372.467987	7.980122
6.000557	375.181006	7.985139
5.940643	378.112696	7.990157
6.086544	369.077044	7.995174
6.097838	375.371086	8.000192
6.064716	376.310448	8.005210
6.289668	373.788527	8.010227
5.939980	377.646076	8.015245
6.088510	377.480861	8.020262
6.266958	376.989070	8.025280
6.254982	375.880184	8.030298
6.498971	367.608637	8.035315
6.104852	370.207687	8.040333
6.292273	369.323176	8.045350
5.896544	367.864168	8.050368
5.997963	367.516988	8.055386
6.243775	368.870231	8.060403
5.895324	370.256624	8.065421
5.997594	367.564580	8.070438
6.144344	373.098950	8.075456
6.050967	378.951808	8.080474
6.301639	364.806340	8.085491
6.108160	370.495001	8.090509
6.209490	375.250703	8.095526
6.083315	377.126127	8.100544
6.155289	380.011907	8.105562
6.286152	372.367145	8.110579
6.043742	381.301289	8.115597
6.103007	374.926894	8.120614
6.143232	371.095873	8.125632
5.653274	367.789730	8.130650
6.209667	368.560986	8.135667
5.988099	372.202804	8.140685
6.052354	370.403485	8.145702
6.037899	369.970320	8.150720
5.978083	366.498953	8.155738
6.135232	365.578160	8.160755
5.903710	365.794380	8.165773
6.006126	367.949563	8.170790
6.454182	358.699319	8.175808
5.883870	368.820905	8.180826
6.258082	368.115408	8.185843
5.932682	366.639069	8.190861
5.855772	368.241689	8.195878
6.021794	375.906335	8.200896
6.007405	392.892980	8.205914
6.262019	397.195487	8.210931
5.984306	404.595159	8.215949
6.461823	400.856560	8.220966
5.952494	409.961926	8.225984
6.167939	400.767040	8.231002
6.419643	391.408690	8.236019
6.466139	397.940219	8.241037
6.290928	387.645227	8.246054
6.453867	395.480775	8.251072
6.040824	402.317833	8.256090
6.402867	395.981197	8.261107
5.952098	397.140630	8.266125
6.164784	394.532266	8.271142
6.075117	388.897560	8.276160
5.985888	395.658634	8.281178
6.358185	394.287569	8.286195
6.132212	399.031444	8.291213
6.382582	395.337904	8.296230
6.208767	397.662602	8.301248
6.198816	397.642136	8.306266
6.391734	394.326823	8.311283
6.199178	396.884827	8.316301
6.533694	398.293601	8.321318
6.468466	389.376224	8.326336
6.252812	406.022035	8.331354
6.457264	394.837586	8.336371
6.354707	396.999642	8.341389
6.476248	399.865035	8.346406
6.412076	398.682276	8.351424
6.005672	402.517159	8.356442
6.256935	397.037314	8.361459
6.213936	398.035028	8.366477
6.268154	392.762781	8.371494
6.788844	403.934729	8.376512
6.336644	399.177322	8.381530
6.425633	392.864535	8.386547
6.036822	399.830337	8.391565
6.703269	405.693540	8.396582
6.422936	404.203825	8.401600
6.295398	400.029859	8.406618
6.415678	397.495933	8.411635
6.475990	411.075286	8.416653
6.347245	412.525087	8.421670
6.499599	422.050643	8.426688
6.260293	420.923724	8.431706
6.697793	417.159834	8.436723
6.281769	418.613622	8.441741
6.705043	419.752873	8.446758
6.794045	421.335814	8.451776
6.549465	414.914339	8.456794
6.181908	393.714741	8.461811
6.335361	412.388688	8.466829
6.328262	418.436321	8.471846
6.735936	421.234796	8.476864
6.466642	434.701710	8.481882
6.730142	426.584868	8.486899
6.523288	427.340016	8.491917
6.542482	428.324831	8.496934
6.803414	424.487620	8.501952
6.534450	419.953959	8.506970
6.702829	408.989745	8.511987
6.662297	410.618227	8.517005
6.382195	405.884346	8.522022
6.565253	403.665627	8.527040
6.277017	407.494620	8.532058
6.506199	410.213763	8.537075
6.840380	427.278369	8.542093
6.616091	428.654779	8.547110
6.843775	420.884375	8.552128
6.483903	413.426937	8.557146
6.454382	400.953720	8.562163
6.573795	403.365017	8.567181
6.735755	417.013654	8.572199
6.371582	416.660529	8.577216
6.406766	423.768189	8.582234
6.737845	414.498375	8.587251
6.661852	412.339178	8.592269
6.172699	418.339266	8.597287
6.465028	422.563287	8.602304
6.326958	423.825204	8.607322
6.702773	411.351586	8.612339
6.475778	426.702172	8.617357
6.378135	426.742783	8.622375
6.950805	430.285416	8.627392
6.685180	431.488425	8.632410
6.684446	416.672259	8.637427
6.698216	421.012507	8.642445
6.576886	430.965953	8.647463
6.688677	423.147435	8.652480
6.281847	431.043869	8.657498
6.409286	430.033055	8.662515
6.861167	437.110146	8.667533
6.721733	435.106052	8.672551
6.848226	436.414879	8.677568
7.112240	443.540342	8.682586
7.079296	430.206114	8.687603
6.832489	429.951363	8.692621
6.563493	437.684195	8.697639
6.567878	430.396893	8.702656
6.450885	429.964014	8.707674
6.928553	425.281811	8.712691
6.860547	424.061781	8.717709
6.562807	431.698130	8.722727
6.788854	420.137900	8.727744
7.065353	432.689329	8.732762
7.164125	428.432560	8.737779
7.110315	431.142398	8.742797
6.904421	433.831885	8.747815
6.827094	430.060295	8.752832
6.697235	431.598634	8.757850
6.735168	426.786515	8.762867
7.149840	426.080988	8.767885
7.008712	436.028071	8.772903
7.236451	435.212978	8.777920
6.938607	426.786461	8.782938
6.916148	428.661418	8.787955
6.782156	427.975585	8.792973
6.870331	428.214298	8.797991
7.084567	423.150496	8.803008
6.821872	429.411748	8.808026
6.761845	428.073704	8.813043
6.675939	421.551627	8.818061
6.844876	421.888137	8.823079
7.094630	426.065182	8.828096
6.750877	432.607375	8.833114
6.842075	421.020936	8.838131
7.027793	424.614729	8.843149
6.717370	431.713427	8.848167
6.859392	421.018421	8.853184
6.695851	426.768680	8.858202
6.929004	419.193077	8.863219
7.025774	414.444326	8.868237
6.654807	427.463266	8.873255
6.898167	429.656333	8.878272
6.652023	435.782451	8.883290
6.887969	436.963677	8.888307
7.023235	435.926390	8.893325
6.617774	447.505406	8.898343
7.309184	442.833890	8.903360
7.159063	448.288566	8.908378
7.016892	448.762183	8.913395
7.252354	452.837333	8.918413
6.801758	445.940045	8.923431
7.081068	443.450623	8.928448
7.069202	450.897022	8.933466
7.233662	452.695359	8.938483
7.394732	447.788203	8.943501
7.240754	434.627568	8.948519
7.064849	424.219056	8.953536
6.805837	428.037163	8.958554
6.936613	436.193346	8.963571
7.252604	428.630007	8.968589
6.759675	432.759317	8.973607
6.948676	443.273211	8.978624
7.168666	451.535342	8.983642
6.972821	455.962090	8.988659
7.401597	454.664222	8.993677
7.276912	453.131181	8.998695
7.167009	450.718519	9.003712
6.972819	435.992608	9.008730
7.013021	447.621715	9.013747
7.249974	447.003993	9.018765
7.036923	455.659020	9.023783
7.296349	456.760830	9.028800
7.300766	456.473028	9.033818
7.146611	455.010876	9.038835
7.199622	451.083162	9.043853
7.103012	449.271170	9.048871
7.591953	442.813651	9.053888
7.225017	430.857178	9.058906
7.018590	429.046616	9.063923
7.047177	425.801225	9.068941
7.072742	443.371786	9.073959
7.284976	445.951581	9.078976
7.436345	452.097472	9.083994
7.023463	445.336285	9.089011
7.091539	443.602632	9.094029
6.905649	443.960024	9.099047
7.215940	447.370203	9.104064
7.128018	449.160746	9.109082
7.061015	453.425296	9.114099
7.127865	446.652060	9.119117
6.943119	442.152535	9.124135
7.234748	441.570426	9.129152
7.275717	439.891512	9.134170
7.048274	451.856045	9.139187
7.243234	450.238209	9.144205
7.097175	452.921479	9.149223
7.256560	446.458789	9.154240
7.085796	451.029928	9.159258
7.101568	453.719399	9.164275
7.471525	466.237274	9.169293
7.386877	473.897057	9.174311
7.284755	459.775233	9.179328
7.872742	475.073907	9.184346
7.416364	459.186704	9.189363
7.278592	456.854147	9.194381
7.420198	455.553936	9.199399
7.523942	450.772524	9.204416
7.252592	449.082584	9.209434
7.127462	448.010357	9.214451
7.072308	452.339322	9.219469
7.073572	465.637637	9.224487
7.602353	474.116482	9.229504
7.589256	473.534781	9.234522
7.466644	480.272715	9.239539
7.502045	468.108013	9.244557
7.204211	486.205810	9.249575
7.405431	480.203609	9.254592
7.384327	474.229933	9.259610
7.312362	480.070001	9.264627
7.378247	478.437672	9.269645
7.218409	487.914349	9.274663
7.672872	484.049958	9.279680
7.524280	481.523434	9.284698
7.519180	485.926615	9.289715
7.940659	477.605118	9.294733
7.375917	481.931882	9.299751
7.553089	477.785894	9.304768
7.608607	482.116461	9.309786
7.719710	479.956343	9.314803
7.795796	476.760305	9.319821
7.486591	469.219166	9.324839
7.476806	463.941147	9.329856
7.576714	479.676056	9.334874
7.438817	479.521004	9.339891
7.514963	475.561257	9.344909
7.875618	480.569844	9.349927
7.340248	474.316984	9.354944
7.694720	472.210254	9.359962
7.385841	479.002618	9.364979
7.434421	478.370228	9.369997
7.906819	489.373073	9.375015
7.570735	482.713447	9.380032
7.764397	481.338807	9.385050
7.542130	479.953596	9.390067
8.026620	470.839596	9.395085
7.438992	462.925521	9.400103
7.367676	455.479658	9.405120
7.789837	469.125435	9.410138
7.590071	481.391762	9.415155
7.857436	475.394978	9.420173
7.693026	467.897424	9.425191
7.130451	460.399144	9.430208
7.640835	466.498256	9.435226
7.403731	475.949163	9.440243
7.910895	473.932116	9.445261
7.525624	479.594058	9.450279
7.788786	477.078759	9.455296
7.516854	474.625209	9.460314
7.476857	479.892228	9.465331
7.560080	482.971920	9.470349
7.627172	484.062842	9.475367
7.458100	486.746567	9.480384
7.475636	481.413769	9.485402
7.424834	482.819806	9.490419
7.551565	476.589438	9.495437
7.733247	485.472964	9.500455
7.505097	493.284626	9.505472
7.471405	497.932130	9.510490
7.596234	503.425793	9.515507
7.782385	506.369443	9.520525
7.935719	503.877660	9.525543
7.878245	513.915820	9.530560
7.984574	517.664081	9.535578
7.874806	520.975988	9.540595
7.808435	512.844520	9.545613
7.844397	521.608886	9.550631
7.995422	519.881163	9.555648
8.078749	501.132268	9.560666
7.861664	509.074746	9.565683
8.141254	502.391232	9.570701
7.744940	498.240420	9.575719
7.713322	492.530314	9.580736
7.973658	494.168467	9.585754
7.926477	505.883887	9.590771
8.223141	500.800838	9.595789
7.789099	500.821573	9.600807
7.850428	501.664092	9.605824
8.056320	495.096269	9.610842
8.063643	493.492049	9.615859
8.050629	487.179432	9.620877
8.037787	477.313380	9.625895
7.614432	486.357977	9.630912
7.924819	485.722435	9.635930
8.056031	509.278808	9.640947
7.933267	498.978690	9.645965
7.712083	495.854471	9.650983
8.163642	506.579726	9.656000
8.170564	500.639519	9.661018
7.941724	511.114780	9.666035
8.032628	498.190283	9.671053
8.198720	489.877238	9.676071
8.093229	488.486353	9.681088
8.120460	487.740543	9.686106
7.747965	484.545360	9.691123
7.880311	473.293265	9.696141
7.877839	494.276512	9.701159
7.638484	495.598485	9.706176
8.066407	496.866400	9.711194
7.749462	515.080829	9.716211
7.648756	506.475064	9.721229
8.027359	510.480462	9.726247
7.999657	505.927913	9.731264
8.489904	496.434304	9.736282
8.156444	510.643470	9.741299
8.049210	506.744007	9.746317
8.554843	506.510216	9.751335
8.195721	505.679774	9.756352
8.319740	504.019399	9.761370
8.183733	507.360662	9.766387
8.320524	511.410260	9.771405
8.503390	505.726505	9.776423
8.016081	504.603724	9.781440
8.302459	498.042224	9.786458
8.232478	512.330029	9.791475
8.167727	495.179078	9.796493
8.292189	491.776643	9.801511
7.911047	501.379518	9.806528
8.372060	505.397250	9.811546
8.044283	518.302193	9.816563
8.453989	506.555342	9.821581
8.383500	493.173301	9.826599
7.894247	500.221151	9.831616
8.035542	496.973867	9.836634
8.219844	505.115383	9.841651
8.068121	500.714810	9.846669
8.181912	507.949042	9.851687
8.306488	516.734235	9.856704
8.470681	510.718891	9.861722
8.322238	514.958347	9.866739
8.424768	512.818503	9.871757
8.286048	514.736932	9.876775
7.899663	511.064241	9.881792
7.931943	504.501525	9.886810
8.193428	511.763111	9.891827
7.914721	509.370577	9.896845
8.370556	504.051150	9.901863
8.217167	509.190778	9.906880
8.018880	506.725685	9.911898
7.946154	513.017161	9.916915
8.392845	522.988956	9.921933
8.362770	526.821707	9.926951
8.587841	528.563218	9.931968
8.425789	522.128773	9.936986
8.133788	528.558752	9.942003
8.200676	528.772399	9.947021
8.595504	529.871933	9.952039
8.531593	538.869705	9.957056
8.469773	534.480284	9.962074
8.404907	540.679020	9.967091
8.356069	546.073676	9.972109
8.391780	531.150719	9.977127
8.355594	538.430553	9.982144
8.881082	542.583358	9.987162
8.423456	534.326991	9.992179
8.227976	521.964898	9.997197
8.229460	522.191948	10.002215
8.390913	540.710142	10.007232
8.472136	529.166221	10.012250
8.383300	533.853931	10.017267
8.426962	537.921283	10.022285
8.798261	537.913666	10.027303
8.718577	543.136429	10.032320
8.694995	534.625864	10.037338
8.951004	532.932183	10.042355
8.664510	528.773625	10.047373
8.647678	515.755543	10.052391
8.122297	518.633954	10.057408
8.411131	530.280964	10.062426
8.443100	540.182049	10.067443
8.419083	529.329957	10.072461
8.601778	537.689490	10.077479
8.758400	533.117521	10.082496
8.616286	528.762772	10.087514
8.491201	518.182141	10.092531
8.478386	537.159979	10.097549
8.758320	527.860250	10.102567
8.716295	528.195103	10.107584
8.708635	522.304510	10.112602
8.718509	528.658789	10.117619
8.318685	533.666623	10.122637
8.699838	528.933244	10.127655
8.538563	531.435874	10.132672
8.701770	532.530674	10.137690
8.775698	534.507305	10.142707
8.686721	534.767463	10.147725
8.864212	529.772505	10.152743
8.556091	536.116650	10.157760
8.535323	529.041531	10.162778
8.397521	529.552336	10.167795
8.373388	536.700893	10.172813
8.587392	530.179123	10.177831
8.449538	536.357735	10.182848
8.778064	530.701643	10.187866
8.741873	530.069909	10.192883
8.655944	538.149640	10.197901
8.601681	531.704615	10.202919
8.713719	557.217490	10.207936
8.783261	556.834276	10.212954
8.797837	563.415047	10.217971
8.749381	560.983275	10.222989
9.179646	558.214566	10.228007
8.826340	562.019073	10.233024
8.751187	560.749661	10.238042
8.520876	568.384970	10.243059
8.751917	565.464437	10.248077
8.932315	554.656041	10.253095
8.522234	565.405882	10.258112
8.791707	558.834385	10.263130
9.118325	555.283500	10.268147
8.818898	555.368349	10.273165
8.853301	557.404824	10.278183
8.896764	558.231210	10.283200
9.133485	548.875126	10.288218
9.382119	562.147377	10.293235
8.894983	561.958681	10.298253
9.491222	553.483536	10.303271
9.255455	559.614382	10.308288
9.146978	545.998413	10.313306
9.049354	540.434334	10.318323
8.751690	532.070854	10.323341
8.954129	527.914584	10.328359
8.485429	546.941770	10.333376
8.610475	548.793629	10.338394
8.736504	554.672127	10.343411
8.831727	564.364500	10.348429
9.008751	563.516322	10.353447
8.658212	562.858101	10.358464
9.054692	562.796046	10.363482
8.810696	560.767295	10.368499
8.926133	563.639983	10.373517
8.852339	556.011430	10.378535
9.054022	565.784953	10.383552
9.149123	561.591844	10.388570
9.156640	560.243208	10.393587
8.864571	559.313895	10.398605
9.106231	557.205895	10.403623
9.332752	555.191786	10.408640
8.815048	564.121817	10.413658
8.989994	557.580910	10.418675
9.017713	566.346589	10.423693
9.528522	579.098094	10.428711
9.116398	573.166715	10.433728
8.918380	563.954477	10.438746
9.177711	562.468556	10.443763
9.054210	581.040906	10.448781
9.386977	583.816430	10.453799
9.386955	583.844901	10.458816
8.942310	588.370624	10.463834
9.103639	587.013665	10.468851
9.317056	592.799589	10.473869
9.401689	591.561944	10.478887
9.720641	583.436343	10.483904
9.035288	579.368668	10.488922
9.429971	559.996572	10.493939
8.879734	567.628358	10.498957
8.952561	565.385865	10.503975
9.414651	589.518505	10.508992
9.041211	589.706469	10.514010
9.411357	588.581880	10.519027
9.366517	589.620918	10.524045
9.433313	591.305183	10.529063
9.742050	598.685633	10.534080
9.354861	583.128305	10.539098
9.447445	577.764785	10.544115
9.027231	568.319116	10.549133
9.300314	577.434520	10.554151
9.365705	584.496486	10.559168
9.721931	583.168951	10.564186
9.614978	579.136884	10.569203
9.373867	569.836721	10.574221
8.940669	562.598992	10.579239
9.077327	571.196127	10.584256
9.290774	583.129537	10.589274
9.708495	579.119405	10.594291
9.432725	587.762233	10.599309
9.478279	589.115311	10.604327
9.367442	596.918105	10.609344
9.762391	595.852745	10.614362
9.637119	587.569526	10.619379
9.495352	591.725902	10.624397
9.444264	587.921766	10.629415
9.197535	577.016177	10.634432
9.209649	594.942444	10.639450
9.662905	586.224599	10.644467
9.487821	599.001534	10.649485
9.479069	590.160416	10.654503
9.688990	595.659711	10.659520
9.458185	597.002441	10.664538
9.822171	589.573525	10.669555
9.808827	593.340552	10.674573
9.288605	587.609142	10.679591
9.824453	590.314978	10.684608
9.216842	589.387766	10.689626
9.417629	594.317291	10.694643
9.367619	590.497206	10.699661
9.431869	583.787441	10.704679
9.385740	591.043608	10.709696
9.139838	593.467988	10.714714
9.361867	589.949261	10.719731
9.284808	591.419381	10.724749
9.474619	589.616147	10.729767
9.917117	606.695511	10.734784
9.644904	603.942185	10.739802
9.789745	595.960623	10.744819
9.546966	595.563227	10.749837
9.954810	597.178278	10.754855
9.385915	595.885238	10.759872
9.241558	610.787533	10.764890
9.575020	612.388994	10.769907
9.577490	617.280170	10.774925
9.561792	613.981724	10.779943
9.766011	609.263422	10.784960
9.260020	618.311565	10.789978
9.971536	618.402121	10.794995
9.933145	619.386502	10.800013
9.547981	612.624065	10.805031
10.064678	617.668202	10.810048
9.779748	612.947645	10.815066
9.844330	620.344267	10.820083
9.552228	620.762485	10.825101
9.873574	620.052638	10.830119
10.035831	614.059654	10.835136
9.951978	619.055874	10.840154
9.901256	608.738093	10.845171
10.140047	614.725176	10.850189
9.997240	614.539334	10.855207
10.058247	609.392191	10.860224
9.873519	609.560056	10.865242
9.818814	614.703187	10.870259
9.799004	608.710328	10.875277
9.915731	608.575340	10.880295
10.160179	613.097243	10.885312
9.679221	619.601042	10.890330
9.825111	612.089523	10.895347
9.887267	618.344124	10.900365
9.787566	615.863569	10.905383
10.083868	609.581339	10.910400
9.581304	617.982005	10.915418
9.726532	609.227204	10.920435
9.774785	609.036673	10.925453
9.856848	612.940235	10.930471
10.032033	608.706165	10.935488
9.967294	610.796049	10.940506
10.139826	614.865317	10.945523
10.028110	616.290376	10.950541
9.822951	619.001865	10.955559
10.277510	628.230872	10.960576
10.070899	619.931980	10.965594
10.077157	620.243491	10.970611
10.057821	625.289565	10.975629
9.717793	632.506590	10.980647
10.490336	641.130360	10.985664
10.297650	633.450974	10.990682
10.067804	628.166360	10.995699
10.173193	633.155025	11.000717
10.186219	630.420120	11.005735
10.310375	622.495436	11.010752
9.797760	621.026318	11.015770
10.222888	635.170375	11.020787
10.233683	644.819215	11.025805
10.506280	635.643657	11.030823
10.625878	627.628167	11.035840
10.091106	623.161347	11.040858
10.039487	617.208183	11.045875
10.460135	610.344738	11.050893
9.958946	617.277739	11.055911
9.862878	612.451852	11.060928
10.272837	628.677956	11.065946
10.281381	635.764628	11.070963
10.223807	638.295206	11.075981
10.031487	642.301725	11.080999
10.135647	638.403825	11.086016
10.283859	644.231540	11.091034
10.531216	644.432692	11.096051
10.804465	640.590349	11.101069
10.511530	640.317576	11.106087
10.188386	621.471294	11.111104
10.121951	629.948799	11.116122
10.185501	634.486427	11.121139
10.404159	635.572546	11.126157
10.029153	642.100777	11.131175
10.342794	642.029611	11.136192
9.920464	643.235095	11.141210
10.301806	643.910716	11.146227
9.988294	646.689679	11.151245
10.164450	646.507510	11.156263
10.523956	642.689522	11.161280
10.078317	641.919965	11.166298
10.563470	640.695302	11.171315
10.369614	637.926539	11.176333
10.403178	632.647989	11.181351
10.508879	641.723380	11.186368
10.411355	649.871249	11.191386
10.427699	654.630874	11.196403
10.975673	651.714320	11.201421
10.445428	651.036914	11.206439
10.443564	639.550122	11.211456
10.125826	648.852807	11.216474
10.432535	659.007558	11.221491
10.804422	659.757244	11.226509
10.373816	670.876438	11.231527
10.421794	674.233086	11.236544
10.635517	662.712501	11.241562
10.671839	666.260322	11.246579
10.954088	669.892689	11.251597
10.544145	676.505302	11.256615
10.626581	670.887723	11.261632
10.633034	675.304919	11.266650
10.776046	673.764631	11.271667
10.553574	667.431119	11.276685
10.809924	672.553933	11.281703
10.608146	672.569834	11.286720
10.599981	676.254016	11.291738
10.754391	670.113919	11.296755
10.867307	661.761788	11.301773
10.696261	669.886472	11.306791
10.944011	664.167255	11.311808
10.814691	668.473178	11.316826
10.958781	653.432152	11.321843
11.049206	637.402312	11.326861
10.647900	646.648662	11.331879
10.997665	632.345446	11.336896
10.457415	651.892039	11.341914
10.691695	644.212023	11.346931
10.828350	643.613165	11.351949
10.413990	645.145604	11.356967
10.777208	652.315568	11.361984
11.094207	668.650948	11.367002
11.099408	658.447454	11.372019
11.088240	652.080840	11.377037
10.681585	648.692163	11.382055
10.490013	650.773522	11.387072
10.678248	651.053365	11.392090
10.459051	653.369426	11.397107
11.195058	663.355931	11.402125
11.002946	663.304046	11.407143
11.400619	658.937275	11.412160
11.066187	670.798795	11.417178
10.962371	662.202910	11.422195
10.860873	650.255194	11.427213
10.499760	655.755615	11.432231
11.069993	653.918016	11.437248
11.221966	668.067028	11.442266
11.279153	670.131504	11.447283
11.230886	646.555743	11.452301
10.907009	648.440080	11.457319
10.963077	646.534719	11.462336
10.636988	649.845829	11.467354
10.873524	656.278249	11.472371
11.116912	657.568778	11.477389
10.822095	670.907324	11.482407
11.115266	667.894989	11.487424
11.145381	663.093499	11.492442
10.811933	673.629426	11.497459
11.564453	660.440203	11.502477
11.172017	667.999970	11.507495
11.241300	668.992730	11.512512
11.332438	662.881483	11.517530
11.143279	667.629128	11.522547
11.369176	668.152380	11.527565
10.953849	653.849101	11.532583
11.041036	657.139642	11.537600
11.095768	667.539005	11.542618
10.811068	658.930437	11.547635
11.097443	664.370437	11.552653
10.958813	653.902302	11.557671
11.068187	668.263116	11.562688
11.138690	673.238323	11.567706
11.013533	663.866294	11.572723
11.053683	663.828511	11.577741
10.658620	669.795004	11.582759
10.921553	671.170835	11.587776
11.322129	679.193338	11.592794
11.288643	693.059002	11.597811
11.598928	687.503549	11.602829
11.220570	688.528576	11.607847
10.868338	691.250497	11.612864
11.166884	694.612070	11.617882
11.321155	702.881460	11.622899
11.767639	695.086123	11.627917
11.224744	697.869475	11.632935
11.237285	691.609587	11.637952
11.931237	694.303291	11.642970
11.646809	686.859164	11.647987
11.451531	685.646434	11.653005
11.353469	692.301706	11.658023
11.441588	685.165283	11.663040
11.454305	686.902212	11.668058
11.500598	694.484768	11.673075
11.817290	681.467958	11.678093
11.397110	680.079027	11.683111
11.548587	676.381989	11.688128
11.395516	665.467983	11.693146
10.816229	663.756842	11.698163
11.321461	669.689574	11.703181
11.381611	684.237995	11.708199
11.480260	691.790256	11.713216
11.951776	683.596525	11.718234
11.607821	690.312413	11.723251
11.652673	686.436419	11.728269
11.622682	686.889310	11.733287
11.480359	687.659604	11.738304
11.654373	679.348385	11.743322
11.259574	683.285651	11.748339
11.574120	683.978050	11.753357
11.513735	687.421107	11.758375
11.593756	686.632304	11.763392
11.350487	697.485476	11.768410
11.094571	692.533133	11.773427
11.549076	687.747194	11.778445
11.251236	691.502012	11.783463
11.838378	694.171426	11.788480
12.015286	684.780460	11.793498
11.943571	687.120756	11.798515
11.203637	675.961022	11.803533
11.397949	696.197304	11.808551
11.108583	710.835223	11.813568
11.624226	707.507157	11.818586
11.951800	713.183715	11.823603
11.757671	711.386976	11.828621
12.327663	711.537577	11.833639
12.132078	716.289398	11.838656
12.318702	709.519387	11.843674
11.767287	699.582962	11.848691
12.037812	689.416773	11.853709
11.710905	686.867665	11.858727
12.072904	681.496616	11.863744
12.129980	685.710223	11.868762
11.906376	688.487729	11.873779
11.556930	679.639986	11.878797
11.653540	689.559428	11.883815
12.006132	681.807210	11.888832
11.819585	684.967075	11.893850
11.747918	689.566929	11.898867
11.872698	696.234624	11.903885
12.183393	711.267678	11.908903
11.795867	701.513857	11.913920
12.017833	703.905971	11.918938
12.159955	714.853406	11.923955
12.122112	706.392331	11.928973
12.457508	699.425443	11.933991
11.634979	692.895604	11.939008
12.021558	686.100584	11.944026
12.166398	697.176971	11.949043
11.662377	691.569221	11.954061
11.561220	696.492435	11.959079
11.868176	707.227845	11.964096
11.658987	711.574695	11.969114
11.717684	718.754529	11.974131
12.363030	699.210464	11.979149
12.143298	708.800783	11.984167
12.239391	710.120706	11.989184
12.345129	699.857253	11.994202
12.217667	708.366448	11.999219
12.673990	701.876077	12.004237
12.529087	711.016014	12.009255
12.324328	711.638300	12.014272
12.301061	706.778890	12.019290
12.186734	704.218563	12.024307
12.415528	701.948460	12.029325
12.487854	713.553773	12.034343
12.127037	701.542511	12.039360
12.247011	703.480388	12.044378
12.238692	704.905032	12.049395
12.150591	711.116935	12.054413
12.253874	708.759199	12.059431
12.040219	711.762369	12.064448
12.599405	708.051937	12.069466
12.427404	708.022148	12.074483
12.504481	713.337165	12.079501
12.587112	713.109688	12.084519
12.266518	704.140646	12.089536
12.264217	701.663753	12.094554
12.243919	709.061088	12.099571
12.430774	703.326153	12.104589
12.492429	715.081462	12.109607
12.558031	705.240864	12.114624
12.698602	700.665056	12.119642
12.403661	695.835591	12.124659
12.446299	683.543376	12.129677
12.306906	679.522680	12.134695
12.204127	701.389737	12.139712
12.333816	700.381711	12.144730
12.250290	705.365281	12.149747
12.451555	698.854913	12.154765
12.610422	706.066384	12.159783
12.337343	705.894641	12.164800
12.718688	707.643243	12.169818
12.679170	711.739445	12.174835
12.441644	712.174361	12.179853
12.521462	709.223850	12.184871
12.642063	714.831851	12.189888
12.377279	710.272215	12.194906
12.187551	715.297674	12.199923
12.162524	707.749779	12.204941
12.654343	708.619532	12.209959
12.310474	717.086898	12.214976
12.379196	708.284076	12.219994
12.443030	736.231585	12.225011
12.675380	731.559338	12.230029
12.844582	734.158540	12.235047
12.619425	747.959603	12.240064
12.547422	744.026165	12.245082
12.641816	744.033532	12.250099
12.323009	739.412924	12.255117
12.173668	732.383116	12.260135
12.641953	733.865633	12.265152
12.684720	724.738663	12.270170
12.557298	733.168968	12.275187
12.743803	733.701549	12.280205
12.573290	735.618671	12.285223
12.972203	730.920326	12.290240
12.995826	736.104869	12.295258
12.707414	738.125671	12.300275
12.677964	731.932308	12.305293
13.015443	736.641639	12.310311
12.800998	747.430365	12.315328
12.999749	750.015472	12.320346
13.034817	750.079472	12.325363
12.988473	744.706111	12.330381
13.088525	737.466812	12.335399
12.884659	738.013219	12.340416
13.046912	739.953943	12.345434
12.949601	736.971221	12.350451
12.919226	738.191039	12.355469
12.923285	731.127729	12.360487
12.653134	740.725965	12.365504
13.112388	749.140097	12.370522
13.254711	753.264623	12.375539
13.167036	750.488672	12.380557
13.288962	737.606480	12.385575
12.942155	739.532289	12.390592
12.922692	730.490806	12.395610
13.370610	740.812829	12.400627
13.066255	744.104772	12.405645
13.085162	738.172076	12.410663
13.178851	739.164171	12.415680
13.130072	748.292222	12.420698
13.361826	739.889877	12.425715
12.914478	737.173438	12.430733
13.511160	732.974285	12.435751
13.111963	732.213227	12.440768
13.322468	727.774778	12.445786
13.289006	729.604154	12.450803
13.358723	727.589348	12.455821
13.371266	724.538922	12.460839
12.846595	727.470903	12.465856
13.074548	730.736246	12.470874
13.303091	726.187674	12.475891
13.129235	724.943182	12.480909
13.368757	732.687985	12.485927
13.104410	736.456499	12.490944
13.214316	736.694967	12.495962
13.425061	747.619046	12.500979
13.624430	751.968166	12.505997
13.417991	738.821838	12.511015
13.043158	739.426591	12.516032
13.587523	745.883396	12.521050
13.652810	747.163967	12.526067
13.286872	741.537722	12.531085
13.627753	732.594414	12.536103
13.298017	732.917544	12.541120
13.139143	735.744876	12.546138
13.744739	747.329775	12.551155
13.635393	750.433373	12.556173
13.569568	729.003063	12.561191
13.351677	733.196646	12.566208
13.524065	733.491596	12.571226
13.710039	735.302370	12.576243
13.347625	734.188408	12.581261
13.570849	732.998466	12.586279
13.517461	744.494107	12.591296
13.619562	748.571285	12.596314
13.800431	746.034129	12.601331
13.238877	751.016870	12.606349
13.955926	740.496666	12.611367
13.567056	745.840516	12.616384
13.533316	748.225363	12.621402
13.727382	748.409619	12.626419
13.482462	761.917141	12.631437
13.662994	751.919653	12.636455
13.702871	750.499660	12.641472
13.736371	752.416377	12.646490
13.973379	746.566271	12.651507
13.575481	747.057873	12.656525
13.976808	744.170592	12.661543
13.863677	755.700848	12.666560
13.473825	736.034913	12.671578
13.658155	736.422667	12.676595
13.486692	743.663819	12.681613
13.571447	743.685319	12.686631
13.617308	751.277435	12.691648
13.881743	743.021447	12.696666
13.803432	744.207751	12.701683
13.816424	752.246833	12.706701
13.894929	747.213674	12.711719
13.749988	747.649863	12.716736
14.081943	747.998708	12.721754
14.088784	743.077766	12.726771
13.795114	750.044576	12.731789
14.126360	748.386425	12.736807
14.139115	760.108400	12.741824
14.169491	755.855959	12.746842
13.852105	751.172009	12.751859
13.924578	755.632530	12.756877
14.026992	750.949077	12.761895
14.000116	749.025143	12.766912
13.811644	759.030316	12.771930
14.107127	751.829819	12.776947
13.608588	752.375059	12.781965
14.020247	759.436490	12.786983
13.851388	752.905198	12.792000
13.730090	753.795278	12.797018
13.798515	742.376302	12.802035
13.643467	753.610164	12.807053
14.040813	763.179568	12.812071
14.303706	776.418187	12.817088
14.127744	772.961783	12.822106
14.399389	776.832520	12.827123
14.176365	769.880515	12.832141
14.084656	770.248403	12.837159
14.173242	764.749753	12.842176
14.279665	777.309138	12.847194
14.200745	772.221742	12.852211
14.205803	770.652567	12.857229
14.314332	773.005659	12.862247
14.461185	770.211894	12.867264
14.496624	771.033236	12.872282
14.376229	770.329479	12.877299
14.255148	765.005693	12.882317
14.409711	756.852121	12.887335
14.257706	763.496936	12.892352
14.343723	772.767983	12.897370
14.228713	768.573032	12.902387
14.017349	774.053182	12.907405
14.155985	767.356940	12.912423
14.251658	765.451672	12.917440
14.179370	766.794825	12.922458
14.636893	772.684574	12.927475
14.401157	772.746822	12.932493
14.343015	771.701949	12.937511
14.601336	778.030013	12.942528
14.226592	772.029593	12.947546
14.474698	781.019626	12.952563
14.195399	775.726937	12.957581
14.448946	768.267914	12.962599
14.346240	775.002840	12.967616
14.335903	774.038840	12.972634
14.771741	772.777714	12.977651
14.439204	780.624791	12.982669
14.200695	782.379001	12.987687
14.510001	793.347627	12.992704
14.725705	798.423196	12.997722
14.840595	798.544118	13.002739
14.735454	794.306589	13.007757
14.532060	804.396177	13.012775
14.358691	804.101511	13.017792
14.392674	811.689201	13.022810
14.984395	805.433202	13.027827
14.788327	817.995828	13.032845
14.575280	799.438224	13.037863
14.933892	796.570252	13.042880
14.780678	796.853102	13.047898
14.800612	789.294972	13.052915
15.040148	804.080474	13.057933
15.065528	792.693458	13.062951
14.989858	798.445847	13.067968
14.779148	791.056399	13.072986
15.256254	784.969844	13.078003
14.780229	782.226333	13.083021
14.349299	778.134528	13.088039
14.682274	778.158163	13.093056
14.798560	788.973990	13.098074
14.833356	792.793478	13.103091
15.006785	795.291040	13.108109
15.127605	792.971571	13.113127
15.442005	794.610749	13.118144
14.697279	795.576419	13.123162
14.817193	789.716243	13.128179
14.504840	800.223692	13.133197
15.021819	799.164448	13.138215
14.819620	796.160279	13.143232
14.816581	801.793991	13.148250
14.673992	794.529569	13.153267
14.905095	798.349858	13.158285
15.318205	801.444192	13.163303
15.426438	796.898672	13.168320
14.756223	808.970687	13.173338
15.245532	790.681748	13.178355
14.998446	793.746974	13.183373
14.984783	800.291231	13.188391
15.366421	793.758880	13.193408
15.217612	801.501439	13.198426
15.256786	796.780546	13.203443
15.114799	798.371309	13.208461
14.774413	804.360838	13.213479
15.316903	796.594597	13.218496
15.043628	800.231979	13.223514
15.367399	805.391605	13.228531
15.604712	810.495351	13.233549
15.303601	802.798166	13.238567
15.342543	801.750704	13.243584
15.067053	796.116582	13.248602
15.169260	802.765763	13.253619
15.563562	813.935681	13.258637
15.573910	820.839106	13.263655
15.338614	798.611590	13.268672
15.291831	801.178370	13.273690
15.316472	809.038925	13.278707
15.561783	817.199428	13.283725
15.541335	815.050415	13.288743
15.678047	797.002909	13.293760
15.636284	801.304613	13.298778
15.197716	797.501181	13.303795
15.065536	794.678548	13.308813
15.149228	806.244270	13.313831
15.533054	816.958235	13.318848
15.384285	813.702692	13.323866
15.777925	809.926658	13.328883
15.502655	817.553338	13.333901
15.809481	814.216944	13.338919
16.068965	812.229200	13.343936
15.957511	821.900446	13.348954
15.622930	804.075100	13.353971
15.621473	797.766874	13.358989
15.547946	801.372959	13.364007
15.744197	798.047581	13.369024
15.576682	810.233340	13.374042
15.669566	813.693432	13.379059
15.595233	812.275549	13.384077
15.718879	805.376512	13.389095
15.736337	808.977811	13.394112
15.727235	820.315081	13.399130
15.740186	816.018018	13.404147
15.762505	817.390534	13.409165
15.360343	811.419644	13.414183
15.955040	797.933153	13.419200
15.710281	812.826101	13.424218
15.611619	803.336237	13.429235
15.849080	811.355955	13.434253
15.673588	813.592605	13.439271
15.806166	807.881919	13.444288
15.559919	813.335988	13.449306
15.688786	803.914618	13.454323
16.097859	812.301927	13.459341
15.519332	813.112169	13.464359
15.878208	817.852883	13.469376
15.686608	831.112259	13.474394
15.894802	837.082120	13.479411
15.952403	834.040395	13.484429
15.867821	833.425700	13.489447
16.142452	829.614660	13.494464
15.676969	836.608423	13.499482
16.152212	836.609768	13.504499
16.536205	835.217903	13.509517
16.268387	836.929372	13.514535
16.429588	838.409519	13.519552
16.738515	833.658974	13.524570
16.253997	820.919077	13.529587
16.216931	810.046768	13.534605
16.339433	806.505724	13.539623
16.454374	808.024674	13.544640
16.183748	809.357880	13.549658
16.443844	802.721491	13.554675
16.156153	803.075904	13.559693
16.382789	808.982905	13.564711
16.532924	807.977982	13.569728
16.460983	807.127775	13.574746
16.131394	809.713620	13.579763
16.278933	799.342575	13.584781
16.338879	802.100918	13.589799
16.214530	796.458894	13.594816
16.277674	807.592331	13.599834
16.179423	803.489421	13.604851
16.180465	806.954435	13.609869
16.165397	806.461395	13.614887
16.198433	813.588482	13.619904
16.168365	825.541274	13.624922
16.337835	830.179123	13.629939
16.499038	820.096262	13.634957
16.462299	825.908833	13.639975
16.601964	828.717807	13.644992
16.638249	838.766706	13.650010
16.339150	833.035284	13.655027
16.619776	830.936928	13.660045
16.565692	832.050012	13.665063
16.861230	823.464063	13.670080
16.810367	826.056733	13.675098
16.573119	829.779995	13.680115
16.700710	821.412867	13.685133
16.589304	832.485304	13.690151
16.669506	827.271975	13.695168
16.621059	825.032671	13.700186
16.676173	820.972001	13.705203
16.913150	822.468676	13.710221
16.576243	832.197342	13.715239
16.686072	827.885098	13.720256
16.381645	831.738808	13.725274
16.883029	826.342721	13.730291
16.958121	823.001608	13.735309
16.799826	828.091603	13.740327
16.855138	828.130340	13.745344
16.702311	831.275480	13.750362
17.124651	828.763595	13.755379
16.665306	826.045866	13.760397
16.628602	834.143264	13.765415
16.853839	824.012498	13.770432
17.064262	824.241530	13.775450
16.593343	830.756454	13.780467
16.912278	823.971981	13.785485
16.588699	827.809756	13.790503
17.162239	827.316012	13.795520
17.060035	828.547090	13.800538
16.874686	826.733185	13.805555
17.122877	832.349635	13.810573
16.985952	831.093037	13.815591
16.914767	826.802843	13.820608
16.816353	829.017950	13.825626
16.835364	837.434828	13.830643
17.190222	847.433818	13.835661
17.081934	848.631137	13.840679
17.142904	848.485949	13.845696
17.434602	853.789472	13.850714
17.151843	850.270889	13.855731
17.408990	853.815707	13.860749
16.984012	842.732754	13.865767
17.069811	851.587304	13.870784
17.216566	845.353671	13.875802
17.181707	856.827546	13.880819
17.232351	848.860630	13.885837
17.355901	857.141216	13.890855
17.487933	850.168264	13.895872
17.475491	856.412545	13.900890
17.110199	855.261155	13.905907
17.651926	845.822413	13.910925
17.324481	856.105038	13.915943
17.419299	843.709862	13.920960
17.494370	853.468666	13.925978
17.281792	854.947417	13.930995
17.592759	843.764934	13.936013
17.659418	850.864677	13.941031
17.525412	838.846187	13.946048
17.473138	827.562834	13.951066
17.715211	846.485285	13.956083
17.564617	829.322217	13.961101
17.045963	825.979456	13.966119
17.495398	839.280414	13.971136
17.451647	839.423036	13.976154
17.257582	851.401540	13.981171
17.880431	842.205714	13.986189
17.670162	843.775621	13.991207
17.296983	853.472112	13.996224
17.325825	848.222641	14.001242
17.193062	854.697215	14.006259
17.830612	847.354721	14.011277
17.620429	845.112353	14.016295
17.503553	846.787551	14.021312
17.554142	849.421133	14.026330
17.849320	845.411208	14.031347
17.435253	838.836251	14.036365
17.576470	849.888054	14.041383
17.722002	871.792154	14.046400
17.933130	869.329135	14.051418
17.574392	870.265890	14.056435
18.090955	868.556602	14.061453
17.761639	876.800854	14.066471
17.720082	861.422662	14.071488
18.131300	867.669996	14.076506
17.950538	877.232209	14.081523
18.129268	870.419192	14.086541
18.197735	867.053862	14.091559
18.249335	876.658564	14.096576
18.397354	848.845032	14.101594
17.774312	850.470146	14.106611
18.021523	840.064525	14.111629
17.922977	839.546693	14.116647
17.600789	844.880125	14.121664
18.247239	858.917099	14.126682
18.188313	872.496550	14.131699
18.300369	864.160239	14.136717
18.357700	855.879843	14.141735
17.933626	849.407438	14.146752
18.322187	848.948987	14.151770
18.009287	850.907366	14.156787
17.889815	849.209370	14.161805
18.270896	861.356546	14.166823
18.086210	867.204935	14.171840
18.379647	871.817059	14.176858
17.949644	872.278980	14.181875
18.382864	868.348408	14.186893
18.407661	873.542274	14.191911
18.228112	867.403940	14.196928
18.208726	863.986102	14.201946
18.136991	871.287421	14.206963
18.479226	864.148982	14.211981
18.329670	876.805349	14.216999
18.007195	877.146279	14.222016
18.177938	875.601628	14.227034
18.217524	875.409296	14.232051
18.414846	876.369383	14.237069
18.513361	871.781186	14.242087
18.131887	871.519124	14.247104
18.572453	867.454856	14.252122
18.227092	872.249120	14.257139
18.636739	876.076166	14.262157
18.743164	875.576712	14.267175
18.742249	882.529263	14.272192
18.580394	873.970772	14.277210
18.242821	872.824505	14.282227
18.722895	886.508867	14.287245
18.674361	891.720540	14.292263
18.532263	898.237619	14.297280
18.899944	894.370959	14.302298
18.766572	896.496877	14.307315
18.901491	879.042870	14.312333
18.584069	877.839796	14.317351
18.697360	886.087289	14.322368
18.674384	888.350545	14.327386
18.775739	896.492614	14.332403
18.698329	892.664133	14.337421
18.879184	887.381366	14.342439
18.685794	889.658700	14.347456
18.826538	889.027635	14.352474
18.644801	896.898473	14.357491
18.489647	892.921225	14.362509
18.566394	892.691512	14.367527
18.435648	894.488809	14.372544
19.039444	896.432954	14.377562
18.584027	896.554868	14.382579
18.803050	898.641352	14.387597
19.047741	911.261220	14.392615
18.972273	917.890944	14.397632
19.135298	911.231854	14.402650
19.286127	913.338492	14.407667
19.491685	913.028635	14.412685
19.471873	890.338046	14.417703
19.122009	895.786283	14.422720
19.332915	890.773366	14.427738
19.639187	895.194135	14.432755
19.113184	886.414978	14.437773
19.280750	883.305521	14.442791
19.184598	886.987753	14.447808
19.214265	877.518769	14.452826
19.224056	890.248011	14.457843
19.332511	881.407319	14.462861
19.691314	883.310952	14.467879
19.497230	892.111543	14.472896
19.393768	874.877929	14.477914
19.314529	879.415901	14.482931
19.206819	890.159587	14.487949
19.576823	888.713105	14.492967
19.530512	881.771238	14.497984
20.010405	881.052321	14.503002
19.470852	885.883326	14.508019
19.280366	886.847370	14.513037
19.606569	884.801827	14.518055
19.298694	882.057201	14.523072
19.006333	876.757061	14.528090
19.344196	879.222560	14.533107
19.382992	881.252072	14.538125
19.403564	882.694295	14.543143
19.513554	884.914627	14.548160
19.519463	884.639208	14.553178
19.464261	883.278283	14.558195
19.095436	885.974429	14.563213
19.696690	878.233660	14.568231
19.417791	892.036942	14.573248
19.785366	897.590526	14.578266
19.859528	908.312038	14.583283
19.752465	904.059005	14.588301
19.970236	891.098568	14.593319
19.660650	895.413855	14.598336
19.551371	888.955230	14.603354
19.915725	894.957448	14.608371
20.140239	902.335442	14.613389
20.061895	881.320327	14.618407
19.470401	900.761608	14.623424
20.038325	895.888415	14.628442
19.782745	886.814419	14.633459
19.420876	892.081497	14.638477
20.018175	900.174265	14.643495
19.624089	912.285137	14.648512
20.056874	911.800821	14.653530
19.672614	916.036293	14.658547
19.834666	916.462256	14.663565
20.093362	910.709687	14.668583
19.973880	907.531589	14.673600
19.718484	909.007586	14.678618
19.781721	914.820301	14.683635
19.940993	911.387085	14.688653
19.844131	911.566432	14.693671
20.291413	917.199054	14.698688
20.075439	908.551193	14.703706
19.922786	922.047535	14.708723
19.916842	925.570472	14.713741
20.140938	931.001377	14.718759
20.115547	943.875027	14.723776
20.233458	930.680894	14.728794
19.955458	936.903694	14.733811
20.371965	941.146253	14.738829
20.170874	938.056678	14.743847
20.303108	946.954494	14.748864
20.341980	951.615993	14.753882
20.054570	937.267197	14.758899
20.348496	939.408224	14.763917
20.363187	931.633100	14.768935
20.209653	941.112184	14.773952
20.315702	938.798166	14.778970
20.680490	945.646105	14.783987
20.389972	935.801216	14.789005
20.684180	923.248509	14.794023
20.507293	935.546276	14.799040
20.574807	934.090379	14.804058
20.589565	929.177613	14.809075
20.320253	938.573847	14.814093
20.966127	941.792685	14.819111
20.535242	941.866574	14.824128
20.274675	934.844646	14.829146
20.785045	947.889980	14.834163
20.879233	956.667528	14.839181
20.924984	943.289028	14.844199
20.725200	939.296671	14.849216
20.714253	935.912212	14.854234
20.963153	933.269694	14.859251
20.857426	935.119881	14.864269
21.012286	928.739779	14.869287
20.856044	929.931993	14.874304
20.764040	924.032392	14.879322
20.584608	929.002648	14.884339
20.543646	936.409627	14.889357
20.816779	945.029742	14.894375
21.015424	958.976008	14.899392
21.105701	962.944633	14.904410
21.480694	959.234608	14.909427
20.707474	959.340042	14.914445
21.060082	945.809319	14.919463
21.366629	952.467566	14.924480
20.934952	951.768392	14.929498
21.036172	930.639876	14.934515
21.122552	933.198435	14.939533
21.075148	923.732035	14.944551
20.921897	939.494391	14.949568
21.020518	949.681912	14.954586
21.349121	953.117722	14.959603
21.229538	959.347268	14.964621
21.329353	948.093659	14.969639
21.270334	956.933082	14.974656
21.351948	953.609858	14.979674
21.587385	954.986863	14.984691
21.254426	946.098533	14.989709
21.345591	934.805262	14.994727
21.236373	934.005072	14.999744
21.635790	928.546035	15.004762
21.606291	933.792607	15.009779
21.171978	929.587685	15.014797
21.428735	926.858729	15.019815
21.268832	928.092543	15.024832
21.409584	939.652568	15.029850
21.802400	946.754897	15.034867
21.445343	939.820669	15.039885
21.450274	928.228483	15.044903
21.591943	935.600535	15.049920
21.592413	945.134388	15.054938
21.907251	940.351331	15.059955
21.658327	933.589515	15.064973
21.465650	918.591563	15.069991
21.820657	928.309705	15.075008
21.589217	915.694192	15.080026
21.615230	918.457870	15.085043
21.643383	937.063634	15.090061
21.740397	929.272457	15.095079
21.865643	938.234481	15.100096
21.995323	940.467515	15.105114
21.900511	934.189646	15.110131
21.702098	932.803818	15.115149
21.737601	924.937072	15.120167
21.739965	940.959076	15.125184
21.833177	949.762020	15.130202
21.836540	950.941852	15.135219
21.576718	952.917172	15.140237
21.897143	952.374719	15.145255
22.100750	949.546787	15.150272
21.859448	942.954191	15.155290
22.327147	941.587074	15.160307
21.651759	946.619262	15.165325
22.146099	942.278303	15.170343
22.355182	942.630625	15.175360
22.454384	950.586860	15.180378
22.002067	947.489307	15.185395
21.961342	952.068601	15.190413
22.212906	942.599531	15.195431
22.543770	952.009037	15.200448
21.676126	947.638471	15.205466
22.160128	948.130759	15.210483
21.954611	941.257996	15.215501
22.514936	948.599173	15.220519
22.488958	944.450192	15.225536
22.146345	952.084324	15.230554
22.222048	947.095730	15.235571
22.115997	944.669774	15.240589
21.786033	948.843096	15.245607
21.774707	937.439647	15.250624
21.791835	949.195776	15.255642
22.133897	956.545906	15.260659
22.118356	966.631400	15.265677
22.238785	976.234839	15.270695
22.277519	968.115099	15.275712
22.212423	973.051674	15.280730
22.794407	970.902929	15.285747
22.450034	976.703788	15.290765
22.463662	970.412072	15.295783
22.610226	971.847185	15.300800
22.654064	972.143346	15.305818
22.267010	963.758954	15.310835
22.213684	974.484702	15.315853
22.525343	978.844686	15.320871
23.156932	991.807943	15.325888
23.041757	984.507589	15.330906
22.552072	981.643108	15.335923
22.602301	979.861705	15.340941
22.778431	985.107634	15.345959
22.940065	985.947084	15.350976
23.129928	988.988064	15.355994
22.964435	967.361640	15.361011
22.442612	972.682205	15.366029
22.517817	983.460405	15.371047
23.078714	994.585400	15.376064
23.336185	995.999983	15.381082
23.228380	989.588429	15.386099
22.999879	985.436455	15.391117
22.517339	968.495679	15.396135
23.112650	987.006321	15.401152
22.800575	986.654487	15.406170
23.159179	985.115107	15.411187
22.920272	991.284463	15.416205
23.006474	991.630792	15.421223
23.215069	994.031352	15.426240
23.359382	987.125852	15.431258
23.509782	990.952516	15.436275
23.313563	992.883160	15.441293
23.357056	996.439391	15.446311
23.018915	992.771663	15.451328
23.069569	992.495543	15.456346
23.094229	986.618669	15.461363
23.197769	981.404794	15.466381
23.148884	985.818114	15.471399
23.479499	995.085668	15.476416
23.326127	989.034710	15.481434
23.540756	985.577028	15.486451
23.371356	991.672376	15.491469
23.595394	980.528675	15.496487
23.604300	986.248938	15.501504
23.275573	997.150395	15.506522
23.644889	991.743394	15.511539
23.624633	982.143318	15.516557
23.531311	984.016813	15.521575
23.594710	989.078430	15.526592
23.286101	986.933518	15.531610
23.568322	987.230200	15.536627
23.317643	989.327170	15.541645
23.514740	987.320779	15.546663
23.445521	990.225624	15.551680
23.572502	1004.924785	15.556698
23.750903	1014.194107	15.561715
23.442321	1017.130148	15.566733
23.551916	1010.725550	15.571751
23.973339	1018.852241	15.576768
23.612716	1020.754997	15.581786
23.909453	1012.361278	15.586803
23.700164	1009.175142	15.591821
23.547176	1020.124820	15.596839
23.940719	1012.293459	15.601856
23.890115	1012.866355	15.606874
23.783845	1010.875935	15.611891
23.857685	1012.183587	15.616909
23.663263	1007.095286	15.621927
23.959278	1013.417528	15.626944
23.954998	1030.097074	15.631962
24.269662	1038.300463	15.636979
24.293963	1026.932401	15.641997
24.336703	1028.355383	15.647015
23.907816	1012.857863	15.652032
24.256109	1025.306941	15.657050
24.562474	1027.417626	15.662067
24.227514	1013.530665	15.667085
24.222604	1016.056201	15.672103
24.307057	1003.630979	15.677120
24.301290	1013.863294	15.682138
24.444999	1026.792562	15.687155
24.448231	1019.883906	15.692173
24.326736	1017.943208	15.697191
24.543527	1010.805431	15.702208
24.235640	1021.984512	15.707226
24.435282	1017.030130	15.712243
24.647189	1026.297364	15.717261
24.368789	1032.880030	15.722279
24.671995	1016.687120	15.727296
24.497969	1036.315609	15.732314
24.480731	1029.883538	15.737331
24.821275	1024.436853	15.742349
24.727564	1029.870244	15.747367
24.896529	1016.693295	15.752384
24.342879	1012.226178	15.757402
24.623344	1019.036863	15.762419
24.445159	1030.069392	15.767437
24.332944	1028.622712	15.772455
24.738826	1028.871616	15.777472
24.648767	1029.356019	15.782490
24.860906	1032.806937	15.787507
24.753205	1031.321679	15.792525
24.811241	1033.196711	15.797543
24.927268	1026.131521	15.802560
24.650577	1039.357046	15.807578
24.742985	1030.717615	15.812595
25.041197	1031.794450	15.817613
24.870016	1028.816939	15.822631
25.194195	1023.132971	15.827648
25.045324	1032.055938	15.832666
25.007041	1035.388299	15.837683
25.053785	1036.296246	15.842701
25.179747	1035.052095	15.847719
25.442869	1023.671864	15.852736
25.276003	1038.824201	15.857754
25.395207	1041.892041	15.862771
25.589757	1033.422802	15.867789
25.477916	1033.367806	15.872807
25.301395	1024.372873	15.877824
24.903985	1034.975839	15.882842
24.995163	1030.937873	15.887859
25.380113	1036.873796	15.892877
25.046841	1038.232613	15.897895
25.122122	1035.803480	15.902912
25.240962	1034.030257	15.907930
25.404864	1034.834639	15.912947
25.560963	1033.260710	15.917965
25.170598	1034.268702	15.922983
25.220046	1023.347993	15.928000
24.668764	1040.261579	15.933018
25.218242	1057.750659	15.938035
25.267337	1058.453107	15.943053
25.500485	1063.989934	15.948071
25.710166	1060.798107	15.953088
25.714628	1059.992724	15.958106
25.353519	1064.574906	15.963123
25.497438	1052.465389	15.968141
25.302464	1059.180163	15.973159
25.868825	1056.610968	15.978176
25.685353	1060.016575	15.983194
25.834135	1057.664288	15.988211
25.885878	1054.355193	15.993229
25.382338	1055.207344	15.998247
25.725772	1052.976042	16.003264
25.966238	1083.055044	16.008282
25.970561	1075.035324	16.013299
25.883584	1070.637088	16.018317
25.694471	1080.402694	16.023335
26.321517	1069.931116	16.028352
25.746789	1069.077620	16.033370
25.696936	1072.212979	16.038387
25.489025	1071.406155	16.043405
25.272207	1067.858261	16.048423
25.705591	1070.056351	16.053440
26.203415	1087.026520	16.058458
26.028671	1089.891109	16.063475
26.344698	1088.096453	16.068493
25.972096	1100.674313	16.073511
25.980919	1093.288213	16.078528
26.272236	1099.595442	16.083546
26.099274	1098.038351	16.088563
26.448013	1104.680577	16.093581
26.596411	1100.526330	16.098599
26.408492	1100.196068	16.103616
26.313955	1098.500453	16.108634
26.100042	1107.768172	16.113651
26.458825	1095.820627	16.118669
26.332481	1099.936834	16.123687
26.453320	1097.806676	16.128704
26.353543	1090.535425	16.133722
26.376589	1100.305672	16.138739
26.285431	1091.852767	16.143757
26.553032	1086.717300	16.148775
26.608062	1090.107636	16.153792
26.540204	1090.717953	16.158810
26.484095	1097.587714	16.163827
26.674397	1111.746853	16.168845
26.996491	1111.737480	16.173863
26.889231	1095.239571	16.178880
26.443986	1095.959511	16.183898
26.819143	1103.503338	16.188915
27.253191	1106.733305	16.193933
27.352089	1096.893586	16.198951
26.836560	1091.315914	16.203968
26.896337	1086.067838	16.208986
26.712050	1095.813761	16.214003
26.835372	1082.296768	16.219021
26.959131	1083.533487	16.224039
27.123155	1081.955157	16.229056
27.038361	1081.113263	16.234074
26.820278	1090.583604	16.239091
26.998134	1095.595759	16.244109
27.033668	1116.996672	16.249127
27.402405	1113.404364	16.254144
27.112586	1106.421666	16.259162
26.862410	1119.706212	16.264179
26.789597	1110.101679	16.269197
27.137013	1107.402674	16.274215
27.053584	1115.605354	16.279232
27.187492	1113.886568	16.284250
27.213827	1116.435626	16.289267
27.337879	1109.378614	16.294285
27.142076	1126.526927	16.299303
27.291581	1120.374820	16.304320
27.431777	1120.210905	16.309338
27.477232	1114.920883	16.314355
27.497848	1116.489353	16.319373
27.375737	1119.844332	16.324391
27.317500	1112.131050	16.329408
27.391611	1114.612660	16.334426
27.393144	1136.151471	16.339443
27.871547	1131.812965	16.344461
27.819109	1138.193003	16.349479
27.618443	1126.957958	16.354496
27.716735	1112.119388	16.359514
27.478615	1123.341250	16.364531
27.911161	1126.151722	16.369549
27.850599	1136.790335	16.374567
27.884384	1136.428491	16.379584
28.234497	1136.689292	16.384602
27.970636	1122.961524	16.389619
28.125628	1107.763770	16.394637
27.754756	1108.096506	16.399655
27.579346	1111.005385	16.404672
28.111102	1111.717421	16.409690
27.891248	1122.160071	16.414707
27.847493	1118.878550	16.419725
28.390923	1133.496789	16.424743
28.216455	1125.101104	16.429760
28.419799	1101.403267	16.434778
27.994400	1109.312375	16.439795
28.176109	1103.836901	16.444813
28.033712	1104.944904	16.449831
27.933544	1112.799901	16.454848
28.362788	1114.509481	16.459866
28.214137	1129.195124	16.464883
28.220202	1132.892950	16.469901
28.188278	1126.074971	16.474919
28.457726	1126.884912	16.479936
28.588554	1128.543416	16.484954
28.138949	1122.349473	16.489971
28.357143	1120.762652	16.494989
28.560831	1124.852403	16.500007
28.154797	1126.143729	16.505024
28.439040	1124.552872	16.510042
28.235167	1126.367961	16.515059
28.218797	1125.266028	16.520077
28.415577	1126.686975	16.525095
28.434195	1133.324129	16.530112
28.583844	1129.668311	16.535130
28.249868	1130.071009	16.540147
28.716730	1133.832341	16.545165
28.849038	1141.524691	16.550183
28.774362	1142.281249	16.555200
29.242858	1142.349927	16.560218
28.760328	1128.142004	16.565235
28.933585	1125.012679	16.570253
28.557340	1137.802581	16.575271
28.412434	1129.156102	16.580288
28.832545	1134.149247	16.585306
28.699305	1147.557508	16.590323
28.800402	1144.452109	16.595341
28.911223	1143.522757	16.600359
28.815031	1147.703681	16.605376
28.840456	1154.213540	16.610394
28.818458	1146.598711	16.615411
29.112928	1150.459643	16.620429
28.739268	1149.729279	16.625447
28.915370	1152.472633	16.630464
28.907302	1158.744738	16.635482
29.078045	1168.353021	16.640499
29.635693	1170.812529	16.645517
29.944136	1174.349375	16.650535
29.705726	1164.736042	16.655552
29.809016	1151.465140	16.660570
29.429814	1144.474340	16.665587
29.300918	1143.841330	16.670605
29.864386	1134.234925	16.675623
29.725233	1134.632344	16.680640
29.435067	1139.897727	16.685658
29.239005	1138.934404	16.690675
29.353527	1139.595045	16.695693
29.488917	1134.701192	16.700711
29.500178	1141.279540	16.705728
29.712132	1133.334562	16.710746
29.269684	1140.438446	16.715763
29.555777	1139.434294	16.720781
29.821776	1147.787374	16.725799
29.740842	1164.485368	16.730816
29.993534	1153.851481	16.735834
29.509327	1155.625287	16.740851
29.536208	1158.152173	16.745869
29.700148	1159.101727	16.750887
29.668730	1163.474483	16.755904
29.825118	1161.758483	16.760922
29.465751	1179.967610	16.765939
30.034457	1171.231394	16.770957
30.287914	1164.422337	16.775975
29.742210	1165.227449	16.780992
30.330680	1160.855911	16.786010
30.218168	1161.066115	16.791027
30.133504	1163.386410	16.796045
30.542848	1153.523267	16.801063
30.253906	1157.623936	16.806080
30.475707	1163.386642	16.811098
30.197505	1170.625754	16.816115
30.084475	1167.162568	16.821133
30.663410	1151.888886	16.826151
29.906545	1165.243386	16.831168
30.067702	1155.488557	16.836186
30.040498	1164.919563	16.841203
30.284601	1159.904526	16.846221
30.495851	1154.869390	16.851239
30.317425	1159.523963	16.856256
30.390863	1175.127929	16.861274
30.709286	1181.399382	16.866291
30.583809	1178.209552	16.871309
30.432816	1167.389590	16.876327
30.320925	1176.420447	16.881344
30.735556	1171.186179	16.886362
30.912280	1182.750193	16.891379
30.631534	1183.516948	16.896397
31.063310	1183.600847	16.901415
30.835061	1186.420184	16.906432
30.826169	1185.134033	16.911450
30.923976	1182.186938	16.916467
30.728598	1175.142077	16.921485
31.179641	1176.084520	16.926503
30.834123	1169.161018	16.931520
30.647554	1173.829493	16.936538
30.767498	1181.201895	16.941555
30.799348	1174.433867	16.946573
31.063008	1180.833824	16.951591
30.838292	1193.284433	16.956608
30.696764	1187.941632	16.961626
30.839321	1190.980591	16.966643
30.898614	1189.273489	16.971661
30.908966	1177.544588	16.976679
30.835570	1184.303479	16.981696
31.605843	1197.418733	16.986714
31.492017	1212.673363	16.991731
30.894233	1209.087298	16.996749
31.157221	1212.549219	17.001767
31.136495	1217.374765	17.006784
31.347888	1214.409868	17.011802
31.422607	1218.889089	17.016819
31.356602	1215.790924	17.021837
31.440222	1209.961545	17.026855
30.933818	1217.368978	17.031872
31.322149	1207.360770	17.036890
31.224613	1218.295569	17.041907
31.489640	1224.531221	17.046925
31.623380	1223.582494	17.051943
31.644829	1238.901162	17.056960
31.742503	1230.655299	17.061978
31.916438	1229.387838	17.066995
31.527686	1236.350798	17.072013
32.017236	1228.365441	17.077031
32.078014	1232.038935	17.082048
32.288244	1224.337193	17.087066
32.189403	1219.470549	17.092083
31.690378	1207.408012	17.097101
32.023021	1212.219217	17.102119
32.285400	1220.970543	17.107136
32.444865	1207.965362	17.112154
32.377695	1202.484670	17.117171
31.918626	1208.991561	17.122189
31.988203	1198.279038	17.127207
32.098149	1198.246098	17.132224
31.856576	1201.376803	17.137242
32.076439	1213.801954	17.142259
32.144392	1220.466126	17.147277
32.543112	1218.585915	17.152295
32.366198	1230.060195	17.157312
32.251661	1227.468266	17.162330
32.228358	1229.311881	17.167347
32.234769	1231.460119	17.172365
32.410807	1219.566371	17.177383
32.313758	1226.527806	17.182400
32.459942	1220.818013	17.187418
32.182378	1222.067126	17.192435
32.187861	1227.355643	17.197453
32.475157	1220.099435	17.202471
32.326048	1221.779717	17.207488
32.223773	1228.704100	17.212506
32.618319	1233.032226	17.217523
32.877697	1243.074802	17.222541
32.741021	1246.864446	17.227559
32.425433	1251.581559	17.232576
32.742120	1244.207124	17.237594
32.877533	1245.050694	17.242611
33.118626	1245.849304	17.247629
32.910911	1247.201087	17.252647
32.617971	1248.370557	17.257664
33.022916	1244.961905	17.262682
32.889095	1238.974074	17.267699
32.907745	1241.265568	17.272717
32.898420	1235.920974	17.277735
33.070186	1240.921501	17.282752
32.813185	1243.647518	17.287770
33.072251	1241.896487	17.292787
32.971125	1239.457095	17.297805
32.974053	1237.440072	17.302823
32.938610	1241.725113	17.307840
33.457897	1257.985157	17.312858
33.643363	1254.639294	17.317875
33.267113	1254.789832	17.322893
33.172439	1240.303293	17.327911
33.287825	1255.083375	17.332928
33.555928	1263.950594	17.337946
33.804851	1264.075767	17.342963
33.143844	1265.315530	17.347981
33.586589	1266.808407	17.352999
33.722632	1269.605395	17.358016
33.901800	1271.363641	17.363034
33.749572	1265.577507	17.368051
33.646345	1271.406952	17.373069
34.043069	1260.466404	17.378087
33.706640	1257.618891	17.383104
33.739850	1266.545006	17.388122
33.669475	1264.476346	17.393139
33.770158	1265.202279	17.398157
33.865357	1264.477347	17.403175
33.928087	1262.321559	17.408192
33.926918	1267.854135	17.413210
33.958595	1261.862458	17.418227
34.089313	1261.608505	17.423245
33.972701	1259.095794	17.428263
34.061177	1261.540459	17.433280
34.007817	1261.410025	17.438298
34.236299	1259.171461	17.443315
34.042490	1265.466393	17.448333
34.070197	1260.778733	17.453351
34.035650	1259.632301	17.458368
33.907249	1263.998185	17.463386
34.450290	1254.379137	17.468403
33.880126	1262.118482	17.473421
34.242490	1261.878730	17.478439
34.221185	1278.352885	17.483456
34.630151	1287.674591	17.488474
34.801041	1279.442481	17.493491
34.545944	1287.776282	17.498509
34.569705	1286.270405	17.503527
34.768469	1283.522079	17.508544
34.391894	1289.668922	17.513562
34.928081	1286.482706	17.518579
34.450544	1297.798996	17.523597
34.746241	1291.731227	17.528615
34.757691	1287.225995	17.533632
34.370105	1290.348033	17.538650
34.916691	1270.430643	17.543667
34.730202	1286.062807	17.548685
34.681329	1282.097223	17.553703
34.974705	1279.173122	17.558720
35.043407	1292.477265	17.563738
34.845270	1283.447717	17.568755
34.804227	1286.515459	17.573773
34.432919	1279.346637	17.578791
34.678858	1281.804504	17.583808
34.755181	1302.347150	17.588826
35.154532	1298.358674	17.593843
35.145891	1307.490190	17.598861
35.149500	1308.177682	17.603879
34.939145	1319.515242	17.608896
34.895911	1314.762941	17.613914
35.051904	1306.779315	17.618931
34.784307	1308.853725	17.623949
34.920860	1298.001255	17.628967
35.477530	1320.220201	17.633984
35.247758	1321.578601	17.639002
35.918002	1330.322885	17.644019
35.704939	1328.450150	17.649037
35.465595	1321.118618	17.654055
36.100382	1329.054226	17.659072
36.115463	1318.574240	17.664090
36.099897	1304.513929	17.669107
35.795985	1310.062392	17.674125
35.670650	1298.446193	17.679143
36.034938	1301.642943	17.684160
35.882540	1295.550701	17.689178
35.937603	1298.025854	17.694195
35.814667	1300.449996	17.699213
35.842932	1293.789787	17.704231
35.658653	1301.361387	17.709248
35.332073	1295.296437	17.714266
35.826525	1301.934843	17.719283
35.842379	1320.523998	17.724301
35.875814	1322.576491	17.729319
36.104808	1323.171865	17.734336
36.240680	1322.462650	17.739354
36.276313	1324.615789	17.744371
35.945092	1332.756402	17.749389
36.064451	1310.475837	17.754407
36.194151	1325.105405	17.759424
36.206571	1319.091478	17.764442
36.073326	1312.374512	17.769459
36.368164	1336.717414	17.774477
36.603417	1335.929509	17.779495
36.522219	1334.951334	17.784512
36.743823	1336.627195	17.789530
36.594052	1326.778972	17.794547
36.633774	1322.253522	17.799565
36.687602	1325.057088	17.804583
36.671708	1323.001978	17.809600
36.697014	1329.751771	17.814618
36.788245	1335.254112	17.819635
36.801007	1341.399935	17.824653
37.083842	1340.509897	17.829671
37.228137	1318.029747	17.834688
36.920014	1313.369443	17.839706
36.850913	1313.033183	17.844723
36.666565	1317.101722	17.849741
36.916384	1333.640750	17.854759
37.168979	1338.634952	17.859776
36.963380	1341.100455	17.864794
37.329367	1335.551856	17.869811
36.872252	1347.335211	17.874829
37.033285	1341.907087	17.879847
36.963350	1336.600363	17.884864
37.021110	1349.524396	17.889882
36.843975	1335.312642	17.894899
37.066809	1329.818032	17.899917
37.044643	1339.235717	17.904935
37.361470	1330.737712	17.909952
37.232075	1335.375180	17.914970
37.288863	1330.118034	17.919987
37.498504	1340.089559	17.925005
37.551916	1350.148686	17.930023
37.940990	1354.095831	17.935040
37.776822	1349.488705	17.940058
37.750857	1334.603144	17.945075
37.686399	1329.046245	17.950093
37.790435	1329.279330	17.955111
37.999285	1328.631267	17.960128
37.527238	1338.801119	17.965146
37.545873	1325.281409	17.970163
37.905632	1341.825311	17.975181
37.480105	1361.509341	17.980199
37.868620	1367.002986	17.985216
37.628563	1359.807255	17.990234
37.783232	1365.179740	17.995251
37.898498	1354.513616	18.000269
38.012207	1361.091773	18.005287
38.013129	1354.950242	18.010304
37.745112	1356.144217	18.015322
38.039460	1359.421366	18.020339
38.292302	1371.203960	18.025357
38.248980	1378.614647	18.030375
38.102802	1372.496157	18.035392
38.273467	1380.564469	18.040410
38.440751	1370.130037	18.045427
38.331955	1371.033967	18.050445
38.529558	1378.750904	18.055463
38.560571	1378.799762	18.060480
38.422625	1388.118843	18.065498
38.402138	1379.620014	18.070515
38.527415	1378.476936	18.075533
38.309948	1382.837869	18.080551
38.652139	1378.211363	18.085568
38.644017	1379.452986	18.090586
38.660953	1382.603183	18.095603
38.593994	1376.696352	18.100621
38.041728	1385.013638	18.105639
38.710348	1394.241067	18.110656
38.571883	1399.460665	18.115674
38.923789	1394.460232	18.120691
38.866176	1398.553115	18.125709
38.538290	1409.432599	18.130727
39.014774	1401.067344	18.135744
39.040694	1403.165207	18.140762
38.302753	1404.297106	18.145779
38.968890	1411.000177	18.150797
39.217598	1419.491799	18.155815
39.629044	1420.235323	18.160832
39.671993	1419.748956	18.165850
39.848219	1416.054200	18.170867
39.670919	1413.727709	18.175885
39.655575	1404.148729	18.180903
39.639050	1390.722845	18.185920
39.752599	1389.701530	18.190938
39.638998	1385.013886	18.195955
39.403653	1384.018832	18.200973
39.642988	1387.920014	18.205991
39.646966	1383.589506	18.211008
39.663100	1391.341192	18.216026
39.675747	1383.373680	18.221043
39.445648	1381.307941	18.226061
39.844532	1399.897128	18.231079
39.906934	1406.322388	18.236096
39.974916	1399.662228	18.241114
39.800146	1402.552117	18.246131
39.964578	1401.892076	18.251149
39.924286	1407.096295	18.256167
40.153659	1402.231828	18.261184
39.901801	1414.137709	18.266202
39.859886	1419.162297	18.271219
40.075014	1411.314533	18.276237
39.752436	1416.929073	18.281255
39.867264	1410.993749	18.286272
40.200417	1415.886985	18.291290
39.975506	1415.433117	18.296307
40.361848	1412.649071	18.301325
39.986101	1411.767536	18.306343
40.214503	1427.473681	18.311360
40.252090	1433.855499	18.316378
40.243087	1442.210776	18.321395
40.555547	1443.743018	18.326413
40.528257	1445.423170	18.331431
40.331834	1431.883423	18.336448
40.526093	1431.947732	18.341466
40.587467	1437.647295	18.346483
40.746963	1445.789973	18.351501
40.677792	1445.804033	18.356519
40.804163	1434.770030	18.361536
40.611130	1437.145211	18.366554
40.613964	1444.949500	18.371571
40.422674	1451.332468	18.376589
40.740197	1467.788426	18.381607
41.061229	1462.240520	18.386624
40.961818	1459.573599	18.391642
41.141550	1460.646934	18.396659
40.829745	1461.838308	18.401677
40.789615	1469.715614	18.406695
41.199471	1462.512693	18.411712
41.079569	1459.078931	18.416730
41.463617	1469.878467	18.421747
41.685748	1467.085424	18.426765
41.343066	1456.806585	18.431783
41.399779	1452.985373	18.436800
41.219552	1452.442449	18.441818
41.476086	1474.620245	18.446835
41.606216	1472.554862	18.451853
41.880282	1469.305537	18.456871
41.785626	1477.254508	18.461888
41.775452	1480.670914	18.466906
41.614040	1479.967243	18.471923
41.980431	1477.694422	18.476941
41.788800	1486.043618	18.481959
42.098965	1478.038917	18.486976
42.003119	1468.882789	18.491994
42.063702	1463.104277	18.497011
41.941853	1455.640666	18.502029
41.785369	1460.708464	18.507047
41.907637	1467.515704	18.512064
42.263776	1471.190311	18.517082
42.211224	1469.440743	18.522099
42.269499	1477.697129	18.527117
42.275505	1472.520484	18.532135
41.839153	1466.090803	18.537152
42.449875	1466.317090	18.542170
42.163889	1477.316288	18.547187
42.583345	1466.763391	18.552205
42.180765	1466.226901	18.557223
42.270374	1477.334518	18.562240
42.354421	1474.512613	18.567258
42.284516	1472.355489	18.572275
42.589940	1466.554394	18.577293
42.866666	1474.044371	18.582311
42.686608	1465.453732	18.587328
42.538044	1476.090555	18.592346
42.373737	1474.323780	18.597363
42.696172	1473.253954	18.602381
42.837457	1476.286850	18.607399
42.897353	1474.879443	18.612416
43.264804	1468.992885	18.617434
42.591858	1478.417927	18.622451
43.101990	1480.922796	18.627469
42.722140	1503.010977	18.632487
42.818100	1490.495247	18.637504
43.203926	1503.955000	18.642522
42.788294	1502.757801	18.647539
43.285455	1499.732305	18.652557
43.266113	1496.008211	18.657575
43.166912	1503.837980	18.662592
43.461141	1496.021969	18.667610
43.087882	1495.506132	18.672627
43.469185	1493.177320	18.677645
43.469173	1497.466339	18.682663
43.624318	1501.683709	18.687680
43.728359	1491.634674	18.692698
43.697334	1498.642678	18.697715
43.404336	1491.761316	18.702733
43.268399	1501.124324	18.707751
43.450046	1493.231275	18.712768
43.956036	1499.956316	18.717786
43.672859	1512.826581	18.722803
44.043325	1509.265484	18.727821
43.735161	1519.438164	18.732839
43.808692	1507.891662	18.737856
44.132451	1516.810250	18.742874
43.875051	1516.238388	18.747891
44.206553	1509.243395	18.752909
44.102178	1513.075374	18.757927
44.049480	1509.902485	18.762944
44.076404	1512.991176	18.767962
44.094910	1519.855721	18.772979
44.329031	1507.646553	18.777997
44.091492	1509.530074	18.783015
43.996187	1519.846139	18.788032
44.441522	1512.782814	18.793050
44.052944	1511.855944	18.798067
44.386150	1520.937165	18.803085
44.393917	1529.794810	18.808103
44.399507	1527.805741	18.813120
44.812066	1527.416104	18.818138
44.695961	1531.799063	18.823155
44.672547	1525.512956	18.828173
44.725600	1527.944272	18.833191
44.526667	1531.406041	18.838208
45.043368	1520.998831	18.843226
44.957497	1527.646191	18.848243
44.720280	1528.027423	18.853261
44.857435	1525.620090	18.858279
44.864987	1522.917466	18.863296
44.735419	1527.248881	18.868314
44.431035	1530.929155	18.873331
44.687119	1541.811903	18.878349
45.036893	1553.945523	18.883367
44.715799	1556.574325	18.888384
44.935876	1550.616153	18.893402
44.834558	1560.967899	18.898419
45.448390	1564.627398	18.903437
45.489435	1574.372992	18.908455
45.623644	1574.219480	18.913472
45.709752	1575.414793	18.918490
45.462863	1574.156435	18.923507
45.586190	1579.492868	18.928525
45.609379	1577.418980	18.933543
45.646020	1573.493585	18.938560
46.144460	1572.421425	18.943578
45.685693	1573.121408	18.948595
45.933229	1573.268893	18.953613
45.935870	1567.969665	18.958631
45.759656	1572.453574	18.963648
46.047238	1570.660173	18.968666
46.209284	1581.848029	18.973683
45.816268	1567.521583	18.978701
46.178144	1569.371159	18.983719
45.915906	1568.620162	18.988736
46.188345	1563.711032	18.993754
46.276360	1566.231555	18.998771
46.453855	1565.149716	19.003789
46.245820	1567.543044	19.008807
46.046979	1565.680680	19.013824
46.557411	1564.821248	19.018842
46.287764	1566.466795	19.023859
46.346819	1567.600071	19.028877
46.309542	1566.343588	19.033895
46.557628	1569.675364	19.038912
46.102733	1566.698031	19.043930
46.185100	1582.869029	19.048947
46.606471	1586.274650	19.053965
46.542341	1589.478612	19.058983
46.388983	1595.353889	19.064000
47.017591	1595.807762	19.069018
46.637544	1599.645079	19.074035
46.535962	1588.469963	19.079053
46.521632	1596.557888	19.084071
46.955330	1610.426810	19.089088
47.193291	1617.736718	19.094106
46.976726	1608.069228	19.099123
47.240513	1608.905327	19.104141
47.536145	1611.355455	19.109159
46.979429	1610.536979	19.114176
47.391223	1609.333217	19.119194
47.338851	1614.498362	19.124211
47.411401	1611.981211	19.129229
47.578623	1604.469092	19.134247
47.797390	1613.555666	19.139264
47.779730	1605.608583	19.144282
47.586451	1609.318804	19.149299
47.971980	1607.977139	19.154317
47.855980	1604.223983	19.159335
47.870487	1613.948508	19.164352
48.146059	1607.060076	19.169370
47.947247	1602.994829	19.174387
47.469976	1613.929401	19.179405
47.778791	1609.500581	19.184423
47.590332	1611.919251	19.189440
47.953686	1615.318188	19.194458
47.812937	1612.244288	19.199475
47.719492	1622.689515	19.204493
48.281871	1630.996386	19.209511
47.981335	1642.815365	19.214528
48.076122	1626.443109	19.219546
48.246181	1641.521075	19.224563
48.472636	1640.371598	19.229581
48.722193	1631.773531	19.234599
48.278827	1635.917439	19.239616
48.351512	1635.486371	19.244634
48.438204	1630.164487	19.249651
48.277340	1626.424668	19.254669
48.617976	1626.870009	19.259687
48.229406	1634.688365	19.264704
48.721091	1645.641567	19.269722
48.701988	1658.565242	19.274739
48.595835	1665.521961	19.279757
49.164381	1662.355859	19.284775
48.934433	1679.020871	19.289792
49.009008	1661.963743	19.294810
48.945963	1657.214454	19.299827
49.230602	1658.959370	19.304845
49.059827	1651.916777	19.309863
48.948485	1660.685845	19.314880
49.107723	1651.158279	19.319898
48.904145	1655.551817	19.324915
48.975647	1662.625877	19.329933
49.159608	1656.966834	19.334951
49.143789	1656.899947	19.339968
49.679406	1672.062684	19.344986
49.673133	1677.312148	19.350003
49.601800	1678.860358	19.355021
49.865320	1679.380904	19.360039
49.846554	1677.499782	19.365056
49.724159	1658.914457	19.370074
49.857797	1669.112681	19.375091
50.095300	1670.066517	19.380109
50.049216	1657.945332	19.385127
49.549787	1664.155735	19.390144
49.949055	1667.031472	19.395162
50.052908	1678.133826	19.400179
50.166781	1678.403246	19.405197
50.185551	1679.388197	19.410215
50.066487	1685.400149	19.415232
49.966459	1681.174232	19.420250
50.064179	1685.059795	19.425267
49.633503	1682.444743	19.430285
50.110177	1668.183940	19.435303
50.230740	1676.913526	19.440320
50.338170	1676.151945	19.445338
50.322250	1679.285250	19.450355
50.082519	1699.454967	19.455373
50.569435	1692.119954	19.460391
50.139604	1692.095841	19.465408
50.231544	1697.263647	19.470426
50.741838	1687.494856	19.475443
50.601744	1697.881160	19.480461
50.704132	1699.711442	19.485479
50.828237	1711.634359	19.490496
51.137056	1714.271795	19.495514
51.019840	1720.655877	19.500531
50.637711	1721.362794	19.505549
50.637792	1714.975103	19.510567
50.709845	1716.879572	19.515584
50.686527	1713.395912	19.520602
50.798326	1718.671072	19.525619
50.919683	1736.732857	19.530637
51.368226	1732.278959	19.535655
51.729051	1742.889784	19.540672
51.341730	1739.845025	19.545690
51.392128	1740.525204	19.550707
51.382292	1740.268019	19.555725
51.746108	1736.332355	19.560743
51.615361	1741.512972	19.565760
51.590614	1740.245045	19.570778
51.925575	1742.203005	19.575795
51.498635	1746.025607	19.580813
51.999336	1740.891306	19.585831
51.691953	1744.123940	19.590848
51.685581	1758.137669	19.595866
52.017782	1758.549620	19.600883
52.273043	1765.102592	19.605901
52.470959	1766.226749	19.610919
52.316964	1763.947056	19.615936
52.279571	1750.928140	19.620954
52.219866	1739.497044	19.625971
51.977046	1753.206966	19.630989
52.546232	1753.064202	19.636007
52.424115	1757.684858	19.641024
52.217794	1751.285309	19.646042
52.209972	1757.491309	19.651059
52.581227	1763.517990	19.656077
52.322945	1754.194649	19.661095
52.269136	1758.378543	19.666112
52.435779	1749.462030	19.671130
52.854024	1758.290192	19.676147
52.244824	1773.550325	19.681165
52.481275	1787.320892	19.686183
52.613610	1786.855226	19.691200
52.635170	1779.261707	19.696218
53.139595	1780.602946	19.701235
52.480671	1784.395627	19.706253
52.768991	1785.641329	19.711271
52.928998	1810.555147	19.716288
53.253941	1801.721112	19.721306
53.516209	1807.752259	19.726323
53.326490	1805.831632	19.731341
53.878117	1809.766035	19.736359
53.719069	1812.877604	19.741376
53.664249	1810.090028	19.746394
53.710406	1806.832166	19.751411
53.404840	1802.572146	19.756429
53.658215	1801.124932	19.761447
54.120591	1807.986320	19.766464
53.683991	1805.211220	19.771482
53.977275	1799.102631	19.776499
53.282205	1810.304991	19.781517
53.577027	1804.117259	19.786535
53.655708	1803.259186	19.791552
53.951872	1804.664616	19.796570
54.335878	1823.310229	19.801587
53.933517	1828.924772	19.806605
54.270459	1832.280549	19.811623
54.209804	1833.454689	19.816640
54.063560	1825.732796	19.821658
54.257437	1826.160109	19.826675
54.102047	1824.309845	19.831693
54.637030	1821.710746	19.836711
54.642007	1823.944493	19.841728
54.206676	1831.262140	19.846746
54.416106	1826.492208	19.851763
54.313867	1831.182357	19.856781
54.533798	1845.021833	19.861799
54.615897	1853.173667	19.866816
54.629090	1856.962051	19.871834
54.557746	1850.822205	19.876851
54.735776	1848.471544	19.881869
54.841098	1844.863555	19.886887
54.872934	1851.192771	19.891904
54.732633	1865.628382	19.896922
55.115245	1866.294388	19.901939
54.889975	1877.230665	19.906957
55.140239	1879.867832	19.911975
55.137092	1877.580271	19.916992
55.031522	1876.511203	19.922010
55.121867	1872.668853	19.927027
55.116552	1879.856027	19.932045
55.395559	1891.600149	19.937063
55.474745	1897.442245	19.942080
55.566474	1897.039747	19.947098
56.162502	1895.478876	19.952115
55.915596	1904.076784	19.957133
56.013342	1895.925285	19.962151
55.774147	1892.099845	19.967168
55.555098	1902.154630	19.972186
56.065412	1895.585941	19.977203
55.804090	1894.045778	19.982221
55.839382	1891.963647	19.987239
55.858140	1888.691126	19.992256
55.812358	1894.376064	19.997274
55.945151	1898.994690	20.002291
56.234870	1920.577662	20.007309
56.546827	1918.455336	20.012327
56.471008	1918.479905	20.017344
56.430297	1915.308223	20.022362
56.566322	1910.893777	20.027379
56.737964	1919.394556	20.032397
57.027075	1913.718959	20.037415
56.646454	1915.239903	20.042432
56.661745	1910.980083	20.047450
56.727059	1911.806265	20.052467
56.715916	1915.661594	20.057485
57.341020	1911.198926	20.062503
57.209063	1909.584841	20.067520
56.730527	1911.228431	20.072538
57.222850	1912.170760	20.077555
56.998249	1926.474451	20.082573
57.008819	1912.384319	20.087591
57.297678	1916.634491	20.092608
57.071029	1913.192117	20.097626
57.224353	1925.571379	20.102643
57.438765	1944.032235	20.107661
57.786758	1937.504742	20.112679
57.978463	1939.071728	20.117696
57.661705	1945.405096	20.122714
57.980202	1936.631970	20.127731
57.643870	1936.719447	20.132749
57.927110	1949.640146	20.137767
57.767833	1939.499563	20.142784
57.647290	1944.606050	20.147802
57.924521	1937.212266	20.152819
57.959585	1938.156805	20.157837
58.027508	1940.402797	20.162855
57.881343	1938.083983	20.167872
57.635189	1941.319682	20.172890
57.973135	1938.612571	20.177907
57.966305	1950.543537	20.182925
58.215945	1961.717907	20.187943
58.586160	1961.925077	20.192960
58.366876	1968.590346	20.197978
58.410796	1962.741694	20.202995
58.064294	1969.679379	20.208013
58.379013	1960.326121	20.213031
58.635123	1961.557946	20.218048
58.347607	1988.846039	20.223066
58.890999	1986.583296	20.228083
58.695361	1986.424651	20.233101
58.725054	1991.258285	20.238119
58.675968	1989.205143	20.243136
58.834464	1992.525787	20.248154
58.816444	1979.087072	20.253171
59.285648	1986.449270	20.258189
58.943979	2005.559090	20.263207
59.296416	2002.994877	20.268224
58.929852	2016.222576	20.273242
59.375446	2014.274977	20.278259
59.152925	2007.284536	20.283277
59.353677	2002.538010	20.288295
59.855421	1994.714520	20.293312
59.600588	2009.092446	20.298330
59.863842	2005.033614	20.303347
59.989123	2006.267004	20.308365
59.750579	2009.264819	20.313383
60.108167	1997.689277	20.318400
59.552910	2003.514036	20.323418
59.889708	1999.472087	20.328435
59.982456	2006.243129	20.333453
59.770575	2009.233611	20.338471
60.040777	2018.044068	20.343488
60.043862	2027.060495	20.348506
60.677992	2033.475305	20.353523
60.426068	2035.181239	20.358541
60.452535	2032.336708	20.363559
60.478909	2022.826606	20.368576
60.505146	2039.499156	20.373594
60.754769	2026.302517	20.378611
60.685206	2030.299579	20.383629
60.720299	2030.758086	20.388647
60.869318	2021.345544	20.393664
60.487739	2024.769747	20.398682
60.851206	2026.704337	20.403699
60.852980	2029.778121	20.408717
60.562853	2030.161341	20.413735
60.922294	2023.019750	20.418752
61.359473	2035.341991	20.423770
61.033731	2043.573590	20.428787
60.976022	2048.057987	20.433805
61.365740	2040.103695	20.438823
61.577333	2047.297980	20.443840
61.050720	2047.645662	20.448858
61.314750	2038.612754	20.453875
61.361840	2038.419235	20.458893
61.441451	2037.633594	20.463911
61.591455	2046.810064	20.468928
61.278234	2052.909367	20.473946
61.640502	2054.462265	20.478963
61.726793	2061.515228	20.483981
61.572583	2071.212782	20.488999
61.903915	2068.471972	20.494016
61.705509	2069.989628	20.499034
61.994741	2066.226538	20.504051
62.188648	2062.756118	20.509069
61.763182	2070.438419	20.514087
62.120657	2074.939831	20.519104
61.817283	2093.892253	20.524122
62.340527	2092.330144	20.529139
62.561129	2097.351665	20.534157
62.566319	2095.735012	20.539175
62.680375	2081.735840	20.544192
62.669226	2084.959994	20.549210
62.438733	2090.692870	20.554227
62.737104	2088.140272	20.559245
62.458468	2112.002831	20.564263
62.884439	2119.984136	20.569280
62.985231	2119.880040	20.574298
63.049725	2125.134328	20.579315
63.335438	2104.859223	20.584333
63.156299	2113.875839	20.589351
63.476080	2108.119631	20.594368
62.942518	2114.647985	20.599386
63.151234	2118.390010	20.604403
63.201880	2107.872430	20.609421
63.058977	2104.161257	20.614439
63.804761	2105.912869	20.619456
63.619221	2109.959680	20.624474
63.799494	2105.708682	20.629491
63.469086	2097.996589	20.634509
63.444328	2107.882181	20.639527
63.885919	2117.603187	20.644544
63.894800	2124.021309	20.649562
63.715008	2125.779071	20.654579
64.040026	2130.320299	20.659597
63.793956	2130.803925	20.664615
64.122853	2127.372307	20.669632
64.046409	2130.568827	20.674650
64.093262	2127.209803	20.679667
64.472177	2129.523869	20.684685
64.413850	2135.457021	20.689703
64.477630	2128.863527	20.694720
64.406984	2131.169126	20.699738
64.491949	2136.382337	20.704755
64.706455	2143.964401	20.709773
64.505446	2151.324367	20.714791
64.779259	2149.716120	20.719808
64.689340	2149.667152	20.724826
64.494092	2152.999064	20.729843
65.091959	2155.525003	20.734861
64.477563	2161.400106	20.739879
65.091277	2150.431334	20.744896
64.848158	2146.723229	20.749914
65.300580	2165.408976	20.754931
65.700440	2162.240813	20.759949
65.407139	2168.744169	20.764967
65.522049	2165.888916	20.769984
65.658397	2171.760019	20.775002
65.576138	2168.168731	20.780019
65.375570	2168.007700	20.785037
65.856298	2164.773213	20.790055
65.677560	2171.485858	20.795072
65.878405	2168.920124	20.800090
65.596949	2171.006270	20.805107
65.887576	2166.605413	20.810125
66.016910	2161.453432	20.815143
66.207223	2167.533849	20.820160
66.068592	2167.479889	20.825178
66.031759	2169.180540	20.830195
66.435226	2178.074348	20.835213
66.130221	2198.560990	20.840231
66.132703	2192.939682	20.845248
66.153616	2195.208851	20.850266
66.049467	2200.707353	20.855283
66.815102	2186.119977	20.860301
66.213978	2195.205904	20.865319
65.789881	2207.199259	20.870336
66.351018	2209.528971	20.875354
66.529031	2210.874044	20.880371
66.820189	2219.548762	20.885389
66.740426	2228.950689	20.890407
66.669604	2231.821268	20.895424
67.301464	2246.672743	20.900442
67.031636	2248.839135	20.905459
67.391845	2240.182413	20.910477
66.931628	2250.748591	20.915495
66.858097	2241.048880	20.920512
67.260589	2254.465559	20.925530
67.590547	2261.773941	20.930547
67.572816	2265.955456	20.935565
67.523534	2282.277111	20.940583
67.833894	2270.109136	20.945600
67.904933	2266.560087	20.950618
68.219608	2276.383123	20.955635
68.208637	2264.262340	20.960653
67.932601	2269.418529	20.965671
67.750129	2273.745788	20.970688
68.238875	2266.050462	20.975706
68.133877	2263.608380	20.980723
68.473368	2263.416388	20.985741
68.316742	2268.942069	20.990759
68.612152	2255.198397	20.995776
68.299250	2257.854421	21.000794
68.154758	2273.158942	21.005811
68.162602	2258.952190	21.010829
68.300897	2261.363938	21.015847
68.166249	2288.028876	21.020864
68.624986	2296.885679	21.025882
68.303612	2301.496663	21.030899
68.653670	2294.946626	21.035917
68.757035	2298.266497	21.040935
68.566074	2306.720119	21.045952
69.006011	2316.346810	21.050970
68.664129	2318.931636	21.055987
69.150977	2321.033138	21.061005
68.804566	2317.255966	21.066023
69.106003	2336.214879	21.071040
69.071190	2336.659098	21.076058
69.369121	2341.431864	21.081075
69.455883	2335.345983	21.086093
69.469892	2342.214703	21.091111
69.793675	2341.109900	21.096128
69.861002	2355.049426	21.101146
69.889437	2367.972475	21.106163
70.507650	2363.886356	21.111181
70.659123	2364.569659	21.116199
70.299960	2349.675493	21.121216
69.971897	2333.823323	21.126234
70.051147	2338.693472	21.131251
70.398961	2346.273673	21.136269
70.366233	2344.047497	21.141287
70.098590	2356.180556	21.146304
70.543806	2361.252175	21.151322
70.514089	2363.709197	21.156339
70.766371	2361.065943	21.161357
70.529437	2364.887310	21.166375
70.525519	2358.361149	21.171392
70.790974	2360.421595	21.176410
70.831554	2370.682141	21.181427
70.964473	2382.777709	21.186445
71.288281	2385.267717	21.191463
70.961876	2387.938499	21.196480
71.101337	2384.596480	21.201498
71.039232	2380.307645	21.206515
71.080338	2382.235970	21.211533
71.351265	2378.065389	21.216551
71.091397	2384.068073	21.221568
71.350951	2397.718713	21.226586
71.445884	2397.776496	21.231603
71.654170	2397.687119	21.236621
71.832585	2404.662662	21.241639
71.831610	2408.737433	21.246656
71.790583	2404.262235	21.251674
71.561640	2403.234557	21.256691
71.534865	2413.726609	21.261709
71.611068	2425.761657	21.266727
71.739731	2437.163582	21.271744
72.105707	2416.992328	21.276762
71.871879	2443.934994	21.281779
72.001825	2457.694358	21.286797
72.167261	2455.938945	21.291815
72.384758	2459.269369	21.296832
72.497350	2455.060454	21.301850
72.641484	2455.864844	21.306867
72.557686	2461.555917	21.311885
72.789191	2465.995105	21.316903
72.842279	2476.938632	21.321920
72.949356	2474.122432	21.326938
72.986621	2480.949688	21.331955
73.208719	2471.654862	21.336973
73.806115	2466.183284	21.341991
73.482866	2474.525153	21.347008
73.506508	2468.767885	21.352026
73.488382	2468.600360	21.357043
73.870929	2468.187004	21.362061
73.816691	2464.436615	21.367079
73.634373	2474.653239	21.372096
73.891765	2461.584467	21.377114
73.876338	2461.157716	21.382131
73.742386	2458.799047	21.387149
73.914206	2462.051412	21.392167
73.769120	2469.970849	21.397184
74.003165	2468.261497	21.402202
74.152953	2471.037584	21.407219
74.216512	2462.323081	21.412237
74.295619	2472.407218	21.417255
73.806011	2486.260515	21.422272
74.231083	2483.239841	21.427290
74.145903	2499.403199	21.432307
74.350720	2488.911740	21.437325
74.570902	2495.445228	21.442343
75.042439	2514.705918	21.447360
74.920820	2512.092818	21.452378
74.904994	2521.459631	21.457395
74.642073	2511.502238	21.462413
75.043734	2513.550831	21.467431
75.033275	2516.251035	21.472448
74.982078	2519.266924	21.477466
74.932841	2511.081365	21.482483
75.285036	2503.921783	21.487501
75.376477	2518.034401	21.492519
75.188822	2535.709857	21.497536
75.285334	2535.612742	21.502554
75.393069	2534.911046	21.507571
74.995744	2539.575019	21.512589
75.511263	2543.041823	21.517607
75.437832	2560.544756	21.522624
75.687357	2570.924175	21.527642
75.777853	2569.366705	21.532659
76.376969	2564.324064	21.537677
76.235391	2565.009103	21.542695
76.479949	2567.334808	21.547712
76.177561	2557.718125	21.552730
76.292557	2567.765130	21.557747
76.204528	2575.489461	21.562765
76.669937	2573.396674	21.567783
76.556243	2588.336836	21.572800
76.664140	2582.601050	21.577818
76.269768	2581.996955	21.582835
76.351614	2592.386876	21.587853
76.456493	2586.263355	21.592871
76.633492	2604.001679	21.597888
76.953296	2604.668088	21.602906
77.202319	2610.701582	21.607923
77.208030	2610.612381	21.612941
77.470626	2599.351172	21.617959
77.240376	2613.129214	21.622976
77.301184	2607.135680	21.627994
77.352931	2622.046794	21.633011
77.365625	2625.980601	21.638029
78.048185	2623.875879	21.643047
77.684548	2636.746927	21.648064
77.673107	2635.199110	21.653082
78.173219	2629.663821	21.658099
77.998779	2631.184080	21.663117
78.417765	2632.646084	21.668135
78.068695	2630.084383	21.673152
78.194006	2625.071771	21.678170
78.060807	2629.766978	21.683187
78.367165	2634.844650	21.688205
78.360493	2634.467022	21.693223
78.208929	2637.776398	21.698240
78.518604	2647.568859	21.703258
78.686649	2653.024853	21.708275
78.392853	2656.624789	21.713293
78.522655	2651.624092	21.718311
78.507082	2655.129940	21.723328
78.844745	2665.053741	21.728346
78.945697	2681.563683	21.733363
79.176123	2678.967995	21.738381
79.330056	2677.315361	21.743399
79.072918	2688.758952	21.748416
79.148682	2681.121842	21.753434
79.179867	2668.416603	21.758451
79.070612	2682.829068	21.763469
79.295510	2693.218728	21.768487
79.371584	2700.806937	21.773504
79.719218	2698.716807	21.778522
79.432032	2708.580720	21.783539
79.700581	2719.683165	21.788557
79.980261	2719.017646	21.793575
79.805079	2728.655715	21.798592
79.993146	2742.040073	21.803610
80.601234	2739.423081	21.808627
80.627965	2730.916214	21.813645
80.500633	2730.513302	21.818663
80.551831	2739.244804	21.823680
80.309115	2735.760601	21.828698
80.855376	2739.661337	21.833715
80.821289	2735.008223	21.838733
80.871142	2750.711941	21.843751
80.498020	2765.194218	21.848768
80.784896	2764.486540	21.853786
81.102969	2760.276923	21.858803
81.168430	2765.752179	21.863821
81.046351	2763.407390	21.868839
81.091179	2764.107418	21.873856
81.215614	2773.054707	21.878874
81.582937	2769.711635	21.883891
81.489827	2772.175488	21.888909
81.726961	2769.234712	21.893927
81.373247	2780.018068	21.898944
81.547583	2768.401309	21.903962
82.044261	2768.254122	21.908979
82.004934	2769.797411	21.913997
81.986982	2763.926632	21.919015
82.231423	2776.781414	21.924032
82.377662	2791.378026	21.929050
82.455819	2793.089125	21.934067
82.296227	2791.245731	21.939085
82.195213	2798.811227	21.944103
82.439365	2796.611051	21.949120
82.527932	2793.778764	21.954138
82.610797	2793.570164	21.959155
82.662257	2795.140262	21.964173
82.526426	2790.531480	21.969191
82.397111	2809.725658	21.974208
82.907723	2810.838766	21.979226
82.864690	2813.155906	21.984243
82.826438	2817.902566	21.989261
83.242887	2817.606983	21.994279
82.858844	2816.875014	21.999296
82.827959	2831.944432	22.004314
83.220400	2839.618850	22.009331
83.265509	2847.464467	22.014349
83.374506	2841.892548	22.019367
83.308861	2852.170011	22.024384
83.686841	2862.213853	22.029402
84.091582	2857.498268	22.034419
84.495792	2869.049824	22.039437
84.568877	2861.207904	22.044455
84.581131	2857.027241	22.049472
84.335489	2865.167759	22.054490
84.623128	2858.447395	22.059507
84.442695	2862.518823	22.064525
84.969514	2850.717381	22.069543
84.729080	2843.300177	22.074560
84.906855	2851.579504	22.079578
85.435776	2839.004472	22.084595
85.205971	2838.595518	22.089613
85.159389	2818.242270	22.094631
85.113230	2814.389544	22.099648
84.902328	2822.218449	22.104666
85.327462	2833.043936	22.109683
85.547404	2842.866344	22.114701
85.470343	2843.639127	22.119719
85.543317	2843.084894	22.124736
85.294844	2853.671903	22.129754
85.007144	2837.992866	22.134771
84.952789	2847.962406	22.139789
85.605023	2850.883923	22.144807
85.777756	2863.251322	22.149824
85.662300	2876.781178	22.154842
85.867666	2866.286258	22.159859
85.820621	2877.697053	22.164877
86.275646	2874.788403	22.169895
86.462492	2887.200951	22.174912
85.986821	2894.320192	22.179930
86.879379	2892.024730	22.184947
86.302209	2895.694360	22.189965
86.796442	2891.466582	22.194983
86.597016	2893.044434	22.200000
86.611804	2895.361994	22.205018
86.917456	2887.101726	22.210035
86.748437	2895.754182	22.215053
86.945857	2895.584445	22.220071
87.142925	2904.687699	22.225088
87.168776	2910.361734	22.230106
87.279186	2916.530673	22.235123
86.959796	2920.109421	22.240141
87.225709	2914.875860	22.245159
87.117268	2925.295786	22.250176
87.413911	2929.914257	22.255194
87.837026	2940.291943	22.260211
87.813562	2932.379901	22.265229
87.871535	2938.273004	22.270247
87.882114	2940.868976	22.275264
87.537205	2955.223892	22.280282
88.041765	2959.045992	22.285299
87.933738	2961.998265	22.290317
88.476414	2966.685511	22.295335
88.302339	2964.030064	22.300352
88.292768	2967.737030	22.305370
88.567586	2975.963336	22.310387
88.648847	2982.395673	22.315405
88.515297	2990.133626	22.320423
88.740136	2986.528778	22.325440
88.541876	2981.487857	22.330458
88.904519	2982.179132	22.335475
88.937534	2991.301820	22.340493
88.776677	3004.185545	22.345511
89.420464	3004.965335	22.350528
89.377892	3012.569107	22.355546
89.489502	3007.987783	22.360563
89.698679	3014.507403	22.365581
89.719744	3005.127020	22.370599
89.767143	2998.545243	22.375616
89.610966	3009.777534	22.380634
89.951114	3007.489700	22.385651
89.957363	3020.460881	22.390669
89.904057	3022.760720	22.395687
89.938696	3024.567034	22.400704
89.914058	3028.210092	22.405722
90.120073	3029.705497	22.410739
89.818185	3050.953268	22.415757
90.298800	3047.210492	22.420775
90.718407	3059.476224	22.425792
90.402087	3051.550044	22.430810
90.691298	3054.768344	22.435827
90.791731	3079.181945	22.440845
90.734238	3078.291490	22.445863
91.290294	3072.939833	22.450880
90.832983	3080.365581	22.455898
91.475427	3077.850472	22.460915
91.390690	3075.550291	22.465933
91.504790	3079.269467	22.470951
91.161358	3081.662111	22.475968
91.272415	3105.815272	22.480986
91.752946	3088.756316	22.486003
91.536145	3095.734078	22.491021
92.067355	3105.384769	22.496039
91.813128	3101.978048	22.501056
91.816310	3108.233289	22.506074
92.246017	3115.939861	22.511091
92.275315	3129.715508	22.516109
92.295118	3125.214819	22.521127
92.404880	3124.762126	22.526144
92.287178	3124.572321	22.531162
92.710319	3123.354062	22.536179
92.358229	3137.703935	22.541197
92.511860	3145.886180	22.546215
92.601963	3151.127287	22.551232
92.578847	3153.867444	22.556250
92.849416	3163.751533	22.561267
93.027031	3178.362481	22.566285
93.346199	3178.855418	22.571303
93.553586	3180.183339	22.576320
93.181491	3184.852992	22.581338
93.542320	3165.202493	22.586355
93.724437	3183.234119	22.591373
93.868330	3206.394360	22.596391
93.867191	3198.377704	22.601408
93.995763	3200.996260	22.606426
93.801191	3201.203560	22.611443
93.798006	3203.703883	22.616461
93.934158	3201.227047	22.621479
94.176354	3209.395445	22.626496
94.008125	3219.452469	22.631514
94.317592	3219.217830	22.636531
94.435099	3230.262191	22.641549
94.465214	3232.552144	22.646567
94.893000	3236.187487	22.651584
95.223535	3249.076463	22.656602
94.900474	3249.262862	22.661619
94.928830	3253.999201	22.666637
94.800791	3245.355371	22.671655
94.974289	3251.713385	22.676672
94.995658	3252.647514	22.681690
95.221710	3261.623314	22.686707
95.351013	3267.066627	22.691725
95.565065	3280.980725	22.696743
95.621776	3283.405393	22.701760
95.569207	3285.941870	22.706778
95.740924	3277.661377	22.711795
95.986879	3280.668713	22.716813
96.070826	3292.015059	22.721831
96.496497	3291.964216	22.726848
96.310824	3301.354887	22.731866
96.596030	3296.323352	22.736883
96.470319	3298.868135	22.741901
96.325202	3299.534817	22.746919
96.558719	3292.298831	22.751936
96.505683	3300.908059	22.756954
96.540016	3308.682971	22.761971
96.984442	3311.602404	22.766989
97.160109	3310.413437	22.772007
97.230803	3312.715980	22.777024
97.706235	3318.303926	22.782042
97.216911	3313.696735	22.787059
97.285607	3311.426142	22.792077
97.357439	3318.948994	22.797095
98.156930	3316.352435	22.802112
97.921125	3323.844580	22.807130
97.593915	3329.750812	22.812147
97.720823	3332.274959	22.817165
98.127038	3334.092527	22.822183
98.450286	3329.869344	22.827200
98.001235	3341.943109	22.832218
97.803850	3343.915214	22.837235
98.144137	3343.521088	22.842253
98.025667	3366.062976	22.847271
98.448359	3367.909529	22.852288
98.616420	3364.158844	22.857306
98.397143	3369.006605	22.862323
98.610437	3380.162302	22.867341
98.177335	3390.320887	22.872359
98.750824	3400.047177	22.877376
98.916043	3415.689211	22.882394
98.937456	3418.678092	22.887411
98.969988	3420.633122	22.892429
98.856517	3435.532917	22.897447
99.440297	3446.311824	22.902464
99.674314	3444.936955	22.907482
99.736131	3447.859540	22.912499
99.430038	3447.506712	22.917517
99.556254	3459.556709	22.922535
100.245900	3458.429241	22.927552
100.258464	3477.403052	22.932570
100.185005	3473.529212	22.937587
100.137311	3474.666708	22.942605
100.389588	3491.172621	22.947623
100.494601	3491.658088	22.952640
100.439982	3498.935695	22.957658
100.494185	3497.598462	22.962675
101.008414	3487.932248	22.967693
101.167912	3508.382319	22.972711
101.663923	3507.098962	22.977728
101.189647	3498.502943	22.982746
101.277336	3508.794631	22.987763
101.719722	3516.887617	22.992781
101.898256	3510.187263	22.997799
101.924731	3509.264694	23.002816
102.182937	3505.136881	23.007834
102.193782	3507.631891	23.012851
102.277322	3497.951084	23.017869
101.974244	3491.130500	23.022887
102.367519	3497.858176	23.027904
102.372151	3509.138178	23.032922
102.239086	3510.105985	23.037939
102.224925	3503.287477	23.042957
102.173528	3504.548651	23.047975
102.412698	3508.721768	23.052992
102.065886	3510.338544	23.058010
102.341495	3529.874055	23.063027
102.404008	3535.047000	23.068045
102.457489	3536.225463	23.073063
102.962575	3542.929326	23.078080
102.891254	3554.909333	23.083098
102.997736	3563.597853	23.088115
103.250031	3565.512156	23.093133
103.199413	3574.635616	23.098151
103.140326	3582.494721	23.103168
103.117876	3590.540625	23.108186
103.219311	3601.612981	23.113203
103.784873	3609.876091	23.118221
103.662217	3617.653637	23.123239
103.565020	3613.278472	23.128256
103.913320	3629.646371	23.133274
104.221049	3641.702772	23.138291
104.463554	3643.280889	23.143309
104.385228	3649.350237	23.148327
104.646806	3646.408648	23.153344
104.489746	3657.884516	23.158362
104.926151	3665.530305	23.163379
105.234125	3663.607255	23.168397
104.849388	3668.673554	23.173415
104.996642	3666.068662	23.178432
105.159105	3668.599911	23.183450
105.117847	3688.775473	23.188467
105.442636	3699.484637	23.193485
105.440060	3696.909528	23.198503
105.349053	3692.574407	23.203520
105.431105	3706.219130	23.208538
105.885291	3719.859218	23.213555
105.916286	3723.604173	23.218573
105.884137	3727.488431	23.223591
105.789299	3728.030466	23.228608
106.067253	3734.318627	23.233626
106.236359	3750.339103	23.238643
106.272633	3748.881563	23.243661
106.588078	3753.222698	23.248679
106.609489	3762.429659	23.253696
106.940846	3773.715451	23.258714
106.779684	3777.541024	23.263731
107.010918	3781.106270	23.268749
106.802187	3779.406195	23.273767
107.653674	3787.267922	23.278784
107.959288	3797.569821	23.283802
107.657610	3804.422272	23.288819
108.184854	3806.031547	23.293837
108.062724	3797.544344	23.298855
108.162216	3802.014016	23.303872
108.384681	3793.778995	23.308890
108.233536	3798.770857	23.313907
108.353501	3789.709147	23.318925
108.009267	3784.864471	23.323943
108.296957	3786.467085	23.328960
108.604567	3786.352674	23.333978
108.310835	3790.805040	23.338995
108.631511	3793.043229	23.344013
108.490910	3800.508028	23.349031
108.528026	3813.860018	23.354048
109.056332	3820.418311	23.359066
108.446593	3819.270295	23.364083
109.036110	3817.779731	23.369101
109.598664	3827.807821	23.374119
109.843717	3824.733068	23.379136
110.398149	3830.236201	23.384154
109.702720	3819.263209	23.389171
110.080438	3823.509384	23.394189
110.182595	3836.358807	23.399207
109.992606	3829.081642	23.404224
109.952972	3831.657202	23.409242
110.204225	3831.816755	23.414259
110.108109	3820.775120	23.419277
110.282366	3832.925156	23.424295
110.278749	3835.002680	23.429312
110.321775	3853.454468	23.434330
110.491541	3860.236236	23.439347
111.025300	3856.971052	23.444365
110.805450	3859.508567	23.449383
110.681928	3868.795103	23.454400
111.114236	3876.097579	23.459418
111.254090	3879.093231	23.464435
111.242688	3874.893945	23.469453
111.173441	3884.219331	23.474471
111.317402	3893.779611	23.479488
111.218900	3894.148624	23.484506
111.413025	3910.471492	23.489523
111.829556	3914.632698	23.494541
112.025069	3924.112321	23.499559
111.814637	3926.446360	23.504576
111.948757	3922.277923	23.509594
112.259282	3937.550440	23.514611
112.355082	3944.268074	23.519629
112.754925	3956.534358	23.524647
112.763718	3962.492314	23.529664
112.922558	3947.010647	23.534682
112.394180	3952.964380	23.539699
113.034731	3967.658101	23.544717
113.226295	3974.114544	23.549735
113.212524	3969.726223	23.554752
113.443264	3977.079258	23.559770
113.080515	3985.472197	23.564787
113.461190	3994.099028	23.569805
113.557874	3999.478231	23.574823
113.525666	4002.835439	23.579840
114.187248	4006.958275	23.584858
113.868544	4023.213237	23.589875
114.448532	4026.247276	23.594893
114.202238	4039.899502	23.599911
114.202667	4037.740520	23.604928
114.493533	4033.007754	23.609946
114.475532	4041.791760	23.614963
114.884231	4057.989608	23.619981
114.816026	4056.876678	23.624999
114.868770	4060.820305	23.630016
114.909397	4058.370945	23.635034
115.065686	4074.980809	23.640051
115.286640	4074.709527	23.645069
115.703882	4075.537489	23.650087
115.422640	4080.047940	23.655104
115.731591	4078.131006	23.660122
115.313879	4076.495208	23.665139
115.679463	4099.034768	23.670157
115.813896	4105.598058	23.675175
115.963139	4111.669785	23.680192
116.294839	4107.309373	23.685210
116.304540	4130.084643	23.690227
116.497419	4119.354225	23.695245
116.675845	4121.037117	23.700263
117.018497	4122.403889	23.705280
116.833459	4119.560602	23.710298
116.872010	4121.050771	23.715315
117.413845	4116.445955	23.720333
117.707569	4104.721256	23.725351
117.778052	4103.605534	23.730368
118.025546	4099.094183	23.735386
118.146290	4098.554523	23.740403
118.213502	4097.767580	23.745421
118.088179	4098.652138	23.750439
118.400900	4102.056330	23.755456
118.311258	4100.760527	23.760474
118.086121	4101.218825	23.765491
118.182247	4103.435418	23.770509
118.349879	4102.077213	23.775527
118.322017	4117.516528	23.780544
118.656502	4127.084960	23.785562
118.304931	4133.664430	23.790579
118.451755	4134.083392	23.795597
118.509243	4134.538445	23.800615
118.744937	4157.272031	23.805632
119.034217	4152.940349	23.810650
119.172713	4169.587808	23.815667
119.367459	4180.188218	23.820685
119.511879	4187.343382	23.825703
119.136398	4188.406019	23.830720
119.411390	4194.660085	23.835738
119.208979	4211.566160	23.840755
119.563429	4213.764390	23.845773
120.182208	4211.647394	23.850791
120.040608	4235.443934	23.855808
120.233060	4235.855750	23.860826
119.958732	4243.445844	23.865843
120.330414	4240.527944	23.870861
120.729367	4257.393506	23.875879
120.659184	4268.155418	23.880896
120.787391	4271.326565	23.885914
120.799073	4265.510627	23.890931
120.953975	4281.691622	23.895949
121.038125	4286.015464	23.900967
121.172926	4293.989697	23.905984
121.601905	4302.214552	23.911002
121.732507	4312.591511	23.916019
121.285473	4315.811753	23.921037
121.611224	4316.512020	23.926055
121.703852	4332.582871	23.931072
122.072912	4328.702648	23.936090
122.330781	4333.011911	23.941107
122.177900	4336.744766	23.946125
122.593348	4359.826062	23.951143
122.818864	4366.510905	23.956160
123.055602	4373.244495	23.961178
122.828569	4369.987938	23.966195
122.937658	4358.490860	23.971213
123.047463	4370.837586	23.976231
123.195039	4389.466083	23.981248
123.188374	4387.999436	23.986266
123.461784	4391.217298	23.991283
123.577406	4393.645511	23.996301
123.705132	4403.136005	24.001319
123.480921	4419.723729	24.006336
124.108488	4417.191835	24.011354
124.499026	4422.414651	24.016371
124.162548	4424.705371	24.021389
124.557802	4420.495908	24.026407
124.406008	4437.687815	24.031424
124.442006	4445.140993	24.036442
124.700204	4449.655404	24.041459
124.747255	4442.072554	24.046477
124.769853	4443.126499	24.051495
124.614859	4459.649755	24.056512
125.267646	4456.378446	24.061530
125.057894	4463.535546	24.066547
125.181978	4476.457743	24.071565
125.229521	4481.172457	24.076583
125.571230	4489.597303	24.081600
125.629016	4485.604833	24.086618
125.780237	4492.235075	24.091635
125.609553	4506.292461	24.096653
126.301673	4510.255962	24.101671
126.310517	4516.113085	24.106688
126.482348	4517.295165	24.111706
126.251831	4526.567235	24.116723
126.562889	4533.964730	24.121741
127.003634	4542.885436	24.126759
127.224717	4535.742444	24.131776
127.204075	4528.602604	24.136794
127.313268	4544.961444	24.141811
127.281702	4566.736805	24.146829
127.630459	4562.357831	24.151847
127.630557	4572.856393	24.156864
127.446572	4570.243294	24.161882
127.990733	4577.326516	24.166899
127.950950	4593.686645	24.171917
128.209654	4591.629175	24.176935
127.915546	4598.272408	24.181952
128.377232	4606.659572	24.186970
128.744924	4615.607542	24.191987
128.776617	4617.537581	24.197005
128.677318	4625.693835	24.202023
128.584195	4623.211693	24.207040
128.708297	4639.745047	24.212058
129.073189	4638.873567	24.217075
128.914075	4646.919254	24.222093
129.189162	4647.870524	24.227111
129.190782	4659.180120	24.232128
129.168713	4667.744110	24.237146
129.327054	4679.202774	24.242163
129.277691	4696.943894	24.247181
129.564396	4692.653523	24.252199
129.593048	4715.230853	24.257216
129.914756	4733.684066	24.262234
130.125914	4739.544286	24.267251
130.076422	4757.329676	24.272269
130.503157	4759.156805	24.277287
130.549151	4770.825676	24.282304
131.097297	4778.097745	24.287322
131.256919	4781.213555	24.292339
131.542393	4782.605120	24.297357
131.669993	4776.294222	24.302375
131.546914	4785.953627	24.307392
131.746869	4793.229747	24.312410
132.439500	4797.073285	24.317427
132.115848	4804.314650	24.322445
132.637025	4810.909145	24.327463
131.890844	4797.819155	24.332480
132.415177	4809.024857	24.337498
132.304538	4811.368626	24.342515
132.051287	4820.467639	24.347533
132.449428	4826.797327	24.352551
132.509540	4833.366210	24.357568
132.498952	4835.890014	24.362586
132.811909	4851.721630	24.367603
132.857743	4865.211914	24.372621
132.982816	4859.245447	24.377639
133.241256	4890.502225	24.382656
133.546291	4887.477872	24.387674
133.515524	4888.161417	24.392691
133.796041	4895.402862	24.397709
133.806836	4893.289501	24.402727
133.649392	4912.553440	24.407744
133.628871	4914.807346	24.412762
133.909427	4924.327831	24.417779
133.989073	4945.596954	24.422797
134.255940	4946.079200	24.427815
134.494351	4967.702264	24.432832
134.633259	4972.197615	24.437850
134.932992	4975.711332	24.442867
134.784941	4984.115283	24.447885
135.152272	4995.096327	24.452903
135.781784	5000.960535	24.457920
135.948565	4999.835984	24.462938
135.827092	4990.426401	24.467955
136.041987	5001.892191	24.472973
136.339541	5011.268013	24.477991
136.340282	5022.622164	24.483008
136.333193	5022.860084	24.488026
136.358374	5018.749499	24.493043
136.055200	5022.723843	24.498061
136.375682	5031.013376	24.503079
136.648989	5045.184700	24.508096
136.746267	5045.115863	24.513114
137.092901	5062.369161	24.518131
136.981344	5072.326788	24.523149
137.224893	5072.326576	24.528167
137.649604	5076.736142	24.533184
137.587845	5091.203052	24.538202
137.804664	5097.324498	24.543219
138.161514	5098.218791	24.548237
138.069540	5089.574743	24.553255
138.295419	5106.281971	24.558272
138.302655	5113.856723	24.563290
138.419935	5105.703879	24.568307
138.292724	5119.120450	24.573325
138.241440	5127.203117	24.578343
138.685028	5144.416051	24.583360
138.480128	5148.053052	24.588378
138.980182	5157.084721	24.593395
139.008689	5176.313492	24.598413
139.130097	5173.829231	24.603431
139.659016	5190.040822	24.608448
139.759323	5203.623834	24.613466
139.777858	5196.098802	24.618483
139.843871	5209.507264	24.623501
140.210587	5218.739780	24.628519
140.125263	5235.350677	24.633536
140.081808	5226.490627	24.638554
140.402335	5236.418529	24.643571
140.699760	5255.062315	24.648589
140.715645	5251.767542	24.653607
141.290137	5250.746403	24.658624
141.060028	5251.454878	24.663642
141.329223	5259.512648	24.668659
141.642317	5273.599001	24.673677
141.674307	5273.868681	24.678695
141.785425	5268.403013	24.683712
141.876923	5272.615458	24.688730
142.121775	5277.091130	24.693747
142.146173	5294.470890	24.698765
142.243649	5295.083853	24.703783
142.455425	5292.878984	24.708800
142.568865	5295.408673	24.713818
142.827619	5290.292351	24.718835
142.865396	5299.980489	24.723853
142.765891	5309.604911	24.728871
143.143707	5312.715039	24.733888
142.993705	5325.008416	24.738906
143.670814	5326.130331	24.743923
143.361990	5318.672317	24.748941
143.317362	5352.644718	24.753959
143.932127	5349.069862	24.758976
143.797727	5357.576015	24.763994
143.812568	5358.725927	24.769011
143.937973	5376.528713	24.774029
143.867000	5384.144239	24.779047
143.849292	5389.765897	24.784064
143.932694	5406.745097	24.789082
144.293253	5412.026559	24.794099
144.623334	5428.995544	24.799117
144.878749	5434.631246	24.804135
145.132187	5441.223725	24.809152
145.127509	5459.776157	24.814170
145.518887	5462.120277	24.819187
145.648313	5464.814787	24.824205
145.721732	5487.193503	24.829223
145.879334	5487.733919	24.834240
145.651736	5486.838428	24.839258
146.251826	5501.274577	24.844275
146.280648	5516.876656	24.849293
146.604152	5517.015440	24.854311
146.745852	5502.662067	24.859328
146.542221	5532.234077	24.864346
146.758323	5533.169383	24.869363
146.972751	5537.239520	24.874381
146.733218	5546.071584	24.879399
147.121592	5561.071268	24.884416
147.193315	5562.423779	24.889434
147.801352	5587.967075	24.894451
147.955482	5590.099003	24.899469
147.703592	5597.080059	24.904487
148.345874	5597.838118	24.909504
147.939912	5617.975095	24.914522
148.199275	5609.941818	24.919539
148.328769	5626.642527	24.924557
148.549315	5638.830713	24.929575
148.701990	5643.661839	24.934592
148.701390	5655.127077	24.939610
149.263496	5671.213945	24.944627
149.371864	5684.966513	24.949645
149.608727	5667.523486	24.954663
149.852832	5678.227521	24.959680
149.901808	5693.154218	24.964698
149.932902	5695.861012	24.969715
150.258289	5693.101659	24.974733
150.108001	5705.313262	24.979751
150.846416	5712.196037	24.984768
150.533338	5731.646211	24.989786
150.614793	5733.461245	24.994803
150.703112	5730.757967	24.999821
151.570523	5718.086894	25.004839
152.391229	5713.785232	25.009856
152.336293	5703.029575	25.014874
152.738183	5688.663704	25.019891
152.442309	5693.195782	25.024909
152.590782	5693.582957	25.029927
152.568187	5697.409318	25.034944
152.666656	5696.901513	25.039962
152.840314	5687.407453	25.044979
152.768997	5687.349244	25.049997
152.961548	5690.198047	25.055015
153.010406	5688.012341	25.060032
153.056499	5694.353293	25.065050
152.790310	5681.503134	25.070067
153.153915	5680.941166	25.075085
152.918811	5692.253765	25.080103
153.313588	5703.685502	25.085120
152.985046	5720.208676	25.090138
153.391929	5720.066080	25.095155
153.640689	5737.537381	25.100173
153.632853	5754.477533	25.105191
153.929737	5756.252506	25.110208
153.878691	5765.137220	25.115226
154.006802	5780.970193	25.120243
154.153641	5798.337564	25.125261
154.017263	5806.288653	25.130279
154.430153	5814.917620	25.135296
154.533751	5829.005656	25.140314
154.919595	5851.667327	25.145331
155.273554	5854.765503	25.150349
155.181065	5870.699405	25.155367
155.456684	5875.160935	25.160384
155.532607	5886.327068	25.165402
156.053476	5891.738236	25.170419
156.059593	5913.550336	25.175437
155.945025	5921.583290	25.180455
156.057259	5914.756704	25.185472
156.213365	5935.017475	25.190490
156.203332	5946.926317	25.195507
156.364260	5952.614864	25.200525
156.591673	5976.153829	25.205543
157.089968	5981.300237	25.210560
157.164103	5990.474809	25.215578
156.965754	5998.966024	25.220595
157.447515	6008.689154	25.225613
157.448230	6027.809531	25.230631
157.656670	6041.950754	25.235648
158.292590	6052.928242	25.240666
158.239237	6051.001576	25.245683
158.604966	6068.278089	25.250701
158.407467	6091.132462	25.255719
159.189177	6081.972258	25.260736
159.613259	6081.094599	25.265754
159.538759	6096.179866	25.270771
159.808583	6101.317907	25.275789
159.446376	6112.095087	25.280807
159.630331	6106.226320	25.285824
160.068080	6114.437999	25.290842
159.721199	6112.557312	25.295859
160.099400	6115.607540	25.300877
160.036030	6131.997995	25.305895
160.333895	6141.898374	25.310912
160.949903	6153.728213	25.315930
160.832524	6150.450999	25.320947
160.549354	6158.472589	25.325965
160.840335	6179.141820	25.330983
161.242862	6179.606007	25.336000
161.524993	6188.198814	25.341018
161.924182	6198.768371	25.346035
161.964460	6197.464691	25.351053
161.529534	6205.203868	25.356071
162.127511	6206.612880	25.361088
162.347520	6216.266641	25.366106
162.126263	6234.999001	25.371123
162.385292	6236.240142	25.376141
162.680718	6240.313531	25.381159
162.650288	6250.596864	25.386176
162.741683	6268.746780	25.391194
162.915806	6262.838465	25.396211
163.342561	6273.769935	25.401229
163.185824	6287.078342	25.406247
163.571789	6278.684006	25.411264
163.734836	6299.427082	25.416282
163.604454	6315.297856	25.421299
163.909923	6319.000344	25.426317
164.169654	6326.554982	25.431335
164.037002	6349.964585	25.436352
164.238762	6347.057193	25.441370
164.342844	6366.616310	25.446387
164.815710	6365.244847	25.451405
164.520984	6379.869230	25.456423
164.674217	6388.321328	25.461440
165.265964	6398.996578	25.466458
165.680456	6425.894074	25.471475
165.950466	6419.538203	25.476493
165.811972	6423.562811	25.481511
165.749022	6434.182807	25.486528
166.102272	6449.665405	25.491546
166.143830	6453.945925	25.496563
166.746249	6462.138277	25.501581
166.439339	6477.986338	25.506599
166.750954	6479.689625	25.511616
166.973961	6503.924460	25.516634
166.788786	6503.830420	25.521651
167.405212	6506.723434	25.526669
167.492152	6538.073035	25.531687
168.120580	6534.963026	25.536704
168.591361	6539.065834	25.541722
168.148071	6538.437686	25.546739
168.240314	6534.758213	25.551757
168.514976	6561.737794	25.556775
168.821637	6555.145686	25.561792
168.612505	6564.825822	25.566810
168.798053	6582.569850	25.571827
168.968120	6584.999299	25.576845
168.894855	6599.320829	25.581863
168.874651	6617.431750	25.586880
169.464885	6623.659365	25.591898
169.482440	6644.665545	25.596915
169.739825	6651.355706	25.601933
169.817627	6671.418048	25.606951
169.966623	6682.570062	25.611968
170.144954	6682.185464	25.616986
170.163004	6704.343889	25.622003
170.790417	6713.994068	25.627021
171.007857	6727.948156	25.632039
171.149771	6732.910688	25.637056
171.686815	6736.908454	25.642074
171.944517	6750.041778	25.647091
172.362330	6742.690325	25.652109
172.614062	6762.409831	25.657127
172.486594	6757.656670	25.662144
172.585206	6761.382185	25.667162
172.764528	6756.022195	25.672180
172.748203	6753.303592	25.677197
172.724148	6761.546871	25.682215
172.871285	6773.848334	25.687232
173.097071	6779.899490	25.692250
173.113000	6784.234613	25.697268
173.602960	6794.566156	25.702285
173.403725	6807.581693	25.707303
173.512831	6807.675157	25.712320
173.839654	6817.978604	25.717338
173.889601	6826.907991	25.722356
174.130184	6826.721993	25.727373
173.898493	6843.799241	25.732391
174.173531	6859.761658	25.737408
174.740714	6870.987175	25.742426
174.856059	6877.245079	25.747444
175.395686	6884.667706	25.752461
175.181725	6894.563440	25.757479
175.146814	6904.162793	25.762496
175.301861	6912.005567	25.767514
175.625534	6905.903145	25.772532
175.906241	6930.457822	25.777549
175.533411	6942.067415	25.782567
176.008897	6959.292849	25.787584
176.086980	6972.157722	25.792602
176.089644	6981.381870	25.797620
176.599632	6987.454866	25.802637
176.691765	7005.213936	25.807655
177.389483	7024.920680	25.812672
177.579624	7021.711938	25.817690
177.807103	7026.531711	25.822708
177.778336	7022.984748	25.827725
178.190359	7045.236552	25.832743
178.078543	7055.451004	25.837760
178.729748	7044.779665	25.842778
178.552501	7057.302610	25.847796
178.605902	7059.542042	25.852813
178.632373	7074.716473	25.857831
178.602421	7084.896018	25.862848
178.643648	7090.913051	25.867866
178.978151	7114.585076	25.872884
179.346145	7121.842115	25.877901
179.404553	7131.849996	25.882919
179.336175	7159.960714	25.887936
180.221460	7160.005192	25.892954
179.891809	7176.514060	25.897972
180.507823	7190.172444	25.902989
180.563041	7195.420181	25.908007
180.891496	7216.624549	25.913024
180.860784	7215.897013	25.918042
180.670924	7237.570911	25.923060
180.911421	7242.073005	25.928077
180.999144	7249.803349	25.933095
181.325187	7268.763557	25.938112
182.025020	7272.275023	25.943130
181.835180	7288.979918	25.948148
182.299720	7291.918955	25.953165
182.601909	7299.884063	25.958183
182.210179	7311.771504	25.963200
182.896681	7324.809651	25.968218
182.795107	7330.391373	25.973236
183.038891	7349.749702	25.978253
183.182494	7359.065610	25.983271
183.068240	7367.509552	25.988288
183.674333	7381.103336	25.993306
183.775779	7392.244288	25.998324
184.110675	7398.651079	26.003341
183.947987	7418.041588	26.008359
184.245395	7429.145548	26.013376
184.256432	7437.052148	26.018394
184.635775	7456.341997	26.023412
184.771521	7464.232228	26.028429
185.251458	7483.102251	26.033447
185.312829	7492.544762	26.038464
185.646378	7503.365289	26.043482
185.607362	7509.385558	26.048500
185.605898	7521.082557	26.053517
185.882662	7532.341350	26.058535
185.722280	7543.046702	26.063552
186.300039	7545.617615	26.068570
186.605371	7563.593228	26.073588
186.875179	7571.411990	26.078605
187.050020	7590.250994	26.083623
187.002451	7581.238915	26.088640
187.736116	7590.620352	26.093658
187.804526	7603.985990	26.098676
187.938581	7600.479705	26.103693
188.571057	7599.692457	26.108711
188.381761	7602.440372	26.113728
188.657504	7601.393307	26.118746
188.750459	7621.807897	26.123764
189.078936	7621.570239	26.128781
189.467267	7630.402805	26.133799
189.470756	7625.549978	26.138816
189.718851	7617.877495	26.143834
189.626561	7633.168858	26.148852
189.729695	7638.368173	26.153869
190.144403	7645.444465	26.158887
189.823365	7652.194038	26.163904
190.060661	7648.122247	26.168922
190.126971	7668.260087	26.173940
189.989690	7675.394452	26.178957
190.864210	7683.784662	26.183975
190.719587	7703.033731	26.188992
191.069646	7725.419190	26.194010
191.868783	7719.810284	26.199028
192.232619	7712.504789	26.204045
192.390856	7707.993913	26.209063
192.358982	7718.373003	26.214080
192.603447	7725.466525	26.219098
192.636696	7735.232426	26.224116
192.803152	7743.642035	26.229133
192.996301	7742.374281	26.234151
192.865660	7755.082977	26.239168
193.154020	7752.171271	26.244186
193.170404	7771.025813	26.249204
193.118915	7774.992885	26.254221
193.847440	7788.059506	26.259239
193.835585	7815.609883	26.264256
193.818582	7818.315053	26.269274
194.069546	7830.200010	26.274292
194.048525	7842.440134	26.279309
194.261243	7853.251383	26.284327
194.152302	7879.554239	26.289344
194.523163	7889.276803	26.294362
194.684986	7902.883746	26.299380
194.864899	7928.093272	26.304397
195.414836	7937.936190	26.309415
195.428851	7951.888347	26.314432
195.950326	7965.088558	26.319450
196.268883	7969.717515	26.324468
196.422537	7989.166406	26.329485
196.566483	7998.031120	26.334503
196.592238	8013.787339	26.339520
197.117246	8017.572593	26.344538
197.177939	8029.878966	26.349556
196.853801	8040.660773	26.354573
197.564313	8045.212561	26.359591
197.988023	8066.674495	26.364608
198.076482	8084.305739	26.369626
198.059921	8087.197148	26.374644
198.042136	8100.680834	26.379661
198.417661	8109.875547	26.384679
198.706897	8120.656023	26.389696
198.902858	8130.920724	26.394714
199.146765	8139.362579	26.399732
199.237982	8164.333753	26.404749
199.430754	8168.549941	26.409767
199.397262	8175.946065	26.414784
199.776031	8186.160057	26.419802
199.976789	8193.904660	26.424820
200.160949	8203.988136	26.429837
200.430180	8210.427598	26.434855
200.415658	8229.382162	26.439872
200.585894	8240.102423	26.444890
200.814544	8252.704659	26.449908
200.839112	8260.123292	26.454925
201.352383	8276.475830	26.459943
201.437449	8294.467719	26.464960
201.608693	8306.387572	26.469978
201.876666	8321.345236	26.474996
201.810145	8327.944681	26.480013
202.262458	8340.006795	26.485031
202.217493	8361.776123	26.490048
202.552633	8369.259804	26.495066
203.091273	8391.455514	26.500084
203.099999	8403.558747	26.505101
203.073427	8419.613966	26.510119
203.248710	8432.243629	26.515136
203.324078	8446.919008	26.520154
204.070469	8464.188656	26.525172
203.644087	8478.222830	26.530189
204.279656	8501.353794	26.535207
204.705103	8513.372873	26.540224
204.954330	8516.333212	26.545242
205.476556	8540.299690	26.550260
205.681494	8544.409871	26.555277
206.196278	8532.906616	26.560295
206.262563	8540.678745	26.565312
206.810307	8544.258488	26.570330
207.187175	8543.302875	26.575348
207.324472	8546.839575	26.580365
207.648850	8542.435073	26.585383
207.529817	8542.194897	26.590400
207.695214	8540.104256	26.595418
207.925146	8540.945997	26.600436
207.850495	8543.657147	26.605453
208.125868	8549.404343	26.610471
208.047993	8564.350083	26.615488
208.132042	8567.238435	26.620506
208.241105	8575.600584	26.625524
208.321336	8594.054471	26.630541
208.735622	8591.340754	26.635559
209.018915	8612.538017	26.640576
209.041803	8629.747517	26.645594
209.243542	8636.191387	26.650612
209.375354	8657.131441	26.655629
209.709652	8662.250630	26.660647
209.757532	8675.762333	26.665664
210.179718	8684.043907	26.670682
210.777013	8698.691395	26.675700
210.610767	8709.941378	26.680717
210.977522	8722.582287	26.685735
211.018545	8737.594785	26.690752
211.039738	8748.979603	26.695770
211.529379	8757.146454	26.700788
211.484545	8774.152006	26.705805
211.627176	8785.884060	26.710823
211.678669	8798.599667	26.715840
211.850680	8812.433004	26.720858
212.025437	8826.559543	26.725876
212.244902	8853.917363	26.730893
212.554247	8867.381930	26.735911
212.649733	8884.258255	26.740928
212.654723	8898.692439	26.745946
212.818878	8922.024070	26.750964
213.047395	8936.208573	26.755981
213.291783	8954.441352	26.760999
213.705632	8981.554215	26.766016
213.823828	8993.299700	26.771034
214.529261	9004.492237	26.776052
214.235054	9020.501500	26.781069
214.453576	9029.178219	26.786087
214.716544	9038.968808	26.791104
214.936830	9058.263149	26.796122
215.200273	9062.818927	26.801140
215.577405	9080.440625	26.806157
215.802210	9101.843360	26.811175
216.095009	9117.337672	26.816192
216.382823	9130.373257	26.821210
216.704494	9150.270637	26.826228
216.760477	9158.938150	26.831245
217.339762	9167.217431	26.836263
217.743313	9178.084806	26.841280
217.721670	9194.351461	26.846298
217.981778	9193.155211	26.851316
217.943099	9205.777874	26.856333
218.198888	9220.507691	26.861351
218.412284	9230.445068	26.866368
218.464684	9244.136442	26.871386
219.032056	9248.606767	26.876404
218.789509	9265.646898	26.881421
219.135494	9282.358050	26.886439
219.506729	9288.002054	26.891456
219.312518	9305.877651	26.896474
220.119964	9310.244078	26.901492
220.155217	9341.300269	26.906509
220.555414	9338.313967	26.911527
220.787745	9357.748811	26.916544
220.880140	9361.744197	26.921562
221.299219	9379.716386	26.926580
221.259271	9402.805908	26.931597
221.746863	9399.477543	26.936615
221.943462	9419.230624	26.941632
221.886829	9425.541592	26.946650
222.246775	9437.915683	26.951668
222.368627	9457.791021	26.956685
222.552977	9464.752549	26.961703
222.759283	9478.593639	26.966720
222.636540	9497.111793	26.971738
222.865858	9508.432898	26.976756
223.302223	9537.276427	26.981773
223.536466	9543.677633	26.986791
223.746583	9564.900076	26.991808
223.987617	9579.152571	26.996826
224.504910	9598.732467	27.001844
224.607767	9608.595800	27.006861
224.876229	9635.501906	27.011879
224.911955	9642.041595	27.016896
225.112825	9663.972850	27.021914
225.397510	9665.936406	27.026932
225.622648	9696.552983	27.031949
226.029560	9710.163904	27.036967
225.746711	9723.996556	27.041984
226.112865	9742.615178	27.047002
226.486974	9747.681072	27.052020
226.557219	9764.906304	27.057037
226.881428	9786.837326	27.062055
227.410901	9792.573519	27.067072
227.849546	9805.090239	27.072090
228.237662	9813.226102	27.077108
228.049920	9837.220227	27.082125
228.369186	9840.109818	27.087143
228.836309	9864.683389	27.092160
228.483338	9874.090984	27.097178
228.874460	9867.857050	27.102196
228.807720	9893.092097	27.107213
229.142464	9905.104188	27.112231
229.470804	9912.352753	27.117248
229.454298	9930.346350	27.122266
229.830569	9937.315879	27.127284
229.945985	9957.214859	27.132301
230.506459	9964.404979	27.137319
230.778227	9989.003003	27.142336
230.876752	9996.606503	27.147354
231.093905	10011.061988	27.152372
231.444532	10040.608048	27.157389
231.778201	10040.634778	27.162407
231.844215	10051.325050	27.167424
231.936599	10067.997700	27.172442
232.407946	10073.212637	27.177460
232.753107	10092.264309	27.182477
232.724501	10103.379901	27.187495
233.396005	10130.062553	27.192512
233.349797	10130.947628	27.197530
233.376174	10144.830030	27.202548
233.388056	10157.912719	27.207565
233.299946	10180.234013	27.212583
233.624817	10202.579047	27.217600
233.843964	10221.410624	27.222618
233.952312	10241.519407	27.227636
234.141822	10266.045430	27.232653
234.611231	10284.790504	27.237671
234.999054	10306.614290	27.242688
235.165716	10339.331334	27.247706
235.405705	10350.989130	27.252724
235.799589	10370.121863	27.257741
236.367407	10390.733491	27.262759
236.391269	10401.503189	27.267776
236.749581	10423.202277	27.272794
237.149732	10425.735121	27.277812
237.263138	10440.876580	27.282829
237.463193	10458.678885	27.287847
237.920525	10475.020024	27.292864
237.912355	10488.128187	27.297882
238.414805	10505.750549	27.302900
238.766358	10516.756313	27.307917
238.910073	10527.219973	27.312935
239.266287	10538.979666	27.317952
239.410091	10554.839528	27.322970
239.809814	10561.240421	27.327988
239.924458	10568.551138	27.333005
240.206437	10595.687009	27.338023
240.727603	10597.749394	27.343040
240.269837	10607.735812	27.348058
240.599327	10622.152068	27.353076
240.813079	10642.787866	27.358093
241.136194	10655.597962	27.363111
241.814069	10671.955245	27.368128
241.852215	10690.379909	27.373146
242.267402	10692.225248	27.378164
242.197035	10702.845688	27.383181
242.454103	10711.438215	27.388199
243.056836	10725.060251	27.393216
243.003207	10742.709956	27.398234
243.310677	10742.235586	27.403252
243.826035	10757.219607	27.408269
243.685772	10771.529588	27.413287
244.463329	10784.012819	27.418304
244.207930	10803.118248	27.423322
244.525007	10807.009281	27.428340
244.673585	10811.615060	27.433357
244.648203	10835.998671	27.438375
244.800470	10843.300443	27.443392
244.863386	10864.054841	27.448410
245.304389	10868.078037	27.453428
245.280874	10888.514457	27.458445
245.210276	10899.592893	27.463463
245.597789	10916.507405	27.468480
246.140882	10947.834043	27.473498
246.535626	10959.720584	27.478516
246.367748	10981.246984	27.483533
246.488500	11008.070848	27.488551
246.772591	11021.143073	27.493568
247.094272	11047.556605	27.498586
247.387011	11072.913751	27.503604
247.622300	11094.216086	27.508621
247.761857	11108.296188	27.513639
248.922243	11108.329193	27.518656
249.052673	11133.377141	27.523674
249.547484	11140.615896	27.528692
249.917377	11144.132442	27.533709
249.951709	11151.326505	27.538727
250.670622	11167.548332	27.543744
250.598380	11173.982323	27.548762
251.056722	11184.507581	27.553780
251.372890	11190.239734	27.558797
251.352640	11203.501856	27.563815
251.616319	11203.185902	27.568832
251.930321	11223.111956	27.573850
252.069577	11229.654928	27.578868
252.227077	11251.579050	27.583885
252.173056	11264.865451	27.588903
252.583086	11269.569322	27.593920
252.586712	11288.663086	27.598938
252.666235	11295.284906	27.603956
253.225781	11321.825760	27.608973
252.937016	11339.266563	27.613991
253.092508	11353.634857	27.619008
253.628101	11379.857465	27.624026
253.775249	11402.553854	27.629044
254.290024	11426.048409	27.634061
253.978166	11452.590175	27.639079
254.443496	11465.018573	27.644096
254.499967	11497.382292	27.649114
254.736743	11521.517317	27.654132
255.188015	11547.917568	27.659149
255.388743	11569.772136	27.664167
255.719188	11594.549381	27.669184
256.245185	11621.973754	27.674202
256.623947	11648.931788	27.679220
256.843503	11659.927325	27.684237
257.134051	11679.623868	27.689255
257.452974	11697.014013	27.694272
257.842960	11721.892618	27.699290
257.770057	11738.216877	27.704308
258.067128	11758.158782	27.709325
258.770296	11763.922061	27.714343
259.274599	11766.160896	27.719360
259.712737	11775.123420	27.724378
260.021953	11781.712587	27.729396
260.601347	11786.607942	27.734413
260.899240	11793.982004	27.739431
260.937072	11795.896042	27.744448
261.103332	11805.460090	27.749466
260.837255	11817.801203	27.754484
261.094167	11821.184006	27.759501
261.504843	11833.207547	27.764519
261.899812	11834.203581	27.769536
262.196382	11856.662385	27.774554
262.206708	11871.145390	27.779572
262.491066	11864.655961	27.784589
262.513349	11889.737646	27.789607
262.759355	11897.359866	27.794624
262.581384	11918.468938	27.799642
262.822783	11938.735530	27.804660
263.162790	11959.848765	27.809677
263.099412	11979.841055	27.814695
263.632821	11984.765770	27.819712
263.745694	12013.869048	27.824730
264.301502	12040.449397	27.829748
264.497908	12064.108303	27.834765
264.457448	12083.276090	27.839783
264.878835	12105.188289	27.844800
264.903495	12126.587944	27.849818
265.085235	12144.641023	27.854836
265.622159	12170.627692	27.859853
266.052418	12199.451019	27.864871
266.713327	12219.266945	27.869888
266.681132	12240.981943	27.874906
267.048186	12259.675557	27.879924
267.481563	12274.338909	27.884941
267.523777	12294.927606	27.889959
267.668871	12308.253022	27.894976
268.116795	12322.118363	27.899994
268.151029	12356.312259	27.905012
268.565270	12370.451326	27.910029
268.490675	12391.011059	27.915047
269.183290	12420.099933	27.920064
269.621846	12438.776209	27.925082
269.343213	12466.558382	27.930100
269.876892	12480.410406	27.935117
270.023237	12508.385010	27.940135
270.395077	12521.163485	27.945152
271.075004	12538.343121	27.950170
270.954962	12564.906926	27.955188
271.515986	12583.027324	27.960205
271.822340	12598.595028	27.965223
272.015061	12613.779496	27.970240
272.557156	12639.968106	27.975258
272.352306	12662.083262	27.980276
273.252289	12673.465431	27.985293
273.155060	12698.772173	27.990311
273.652655	12705.714259	27.995328
274.000275	12726.002953	28.000346
274.071830	12741.291767	28.005364
274.232371	12753.958237	28.010381
274.355454	12773.372683	28.015399
274.513392	12784.814319	28.020416
274.959117	12802.681412	28.025434
275.194378	12836.329946	28.030452
275.903240	12844.549519	28.035469
275.606853	12872.451909	28.040487
275.753053	12890.864955	28.045504
276.479240	12907.099782	28.050522
276.546759	12931.961025	28.055540
276.728695	12946.001125	28.060557
277.106137	12975.042332	28.065575
277.627893	12989.417657	28.070592
277.985954	12996.984873	28.075610
277.816333	13030.735073	28.080628
278.482293	13043.534145	28.085645
278.828333	13059.711810	28.090663
278.788317	13087.849097	28.095680
279.352115	13107.971703	28.100698
279.489247	13118.159937	28.105716
279.756006	13137.915414	28.110733
279.921955	13152.637131	28.115751
280.578595	13176.800082	28.120768
280.701753	13191.358003	28.125786
280.610227	13213.399206	28.130804
280.962117	13223.673857	28.135821
281.116028	13236.963809	28.140839
281.180818	13255.926817	28.145856
282.022977	13267.921579	28.150874
282.131242	13295.331718	28.155892
282.633678	13305.285980	28.160909
282.649885	13316.371182	28.165927
283.146893	13331.398031	28.170944
283.914455	13343.183468	28.175962
284.137497	13360.561745	28.180980
284.791269	13368.196476	28.185997
285.254396	13376.176874	28.191015
285.263797	13377.722883	28.196032
285.731303	13389.596407	28.201050
285.858105	13404.804468	28.206068
286.049996	13399.595359	28.211085
286.174257	13416.240716	28.216103
286.476539	13427.139060	28.221120
286.992483	13443.543078	28.226138
286.609734	13463.201685	28.231156
287.077454	13470.366638	28.236173
286.827710	13492.202414	28.241191
287.569848	13505.987800	28.246208
287.640258	13531.509400	28.251226
287.652977	13551.930392	28.256244
287.940684	13569.687168	28.261261
288.059742	13592.883241	28.266279
288.372934	13626.985201	28.271296
288.673935	13649.028580	28.276314
288.560699	13677.181368	28.281332
289.278202	13700.804903	28.286349
289.371569	13723.932525	28.291367
289.579197	13749.211859	28.296384
290.110321	13782.010421	28.301402
290.525863	13815.727193	28.306420
290.901443	13822.391949	28.311437
291.144839	13864.037259	28.316455
291.365791	13889.043097	28.321472
291.407491	13906.172370	28.326490
291.780660	13945.318436	28.331508
291.937908	13971.247049	28.336525
292.433983	14000.192290	28.341543
292.457417	14029.413732	28.346560
293.497299	14052.538755	28.351578
293.536246	14077.961799	28.356596
293.750842	14098.105420	28.361613
294.200906	14120.893417	28.366631
294.354378	14150.306268	28.371648
294.866290	14170.744469	28.376666
294.802031	14199.768315	28.381684
295.011874	14226.206969	28.386701
295.387137	14249.174218	28.391719
295.638427	14286.622051	28.396736
296.604453	14291.984911	28.401754
296.954085	14317.981761	28.406772
297.344628	14329.694233	28.411789
297.943062	14335.111530	28.416807
298.238338	14364.774099	28.421824
298.899021	14352.038048	28.426842
299.102808	14377.732536	28.431860
299.421946	14386.689681	28.436877
299.989389	14385.710258	28.441895
300.052509	14410.384633	28.446912
300.604425	14400.157379	28.451930
300.398924	14410.011525	28.456948
300.679453	14410.005545	28.461965
300.864591	14427.978154	28.466983
301.070445	14443.755766	28.472000
301.148172	14448.007185	28.477018
301.274516	14465.869030	28.482036
301.525607	14479.075148	28.487053
301.520882	14503.728690	28.492071
301.558802	14524.993168	28.497088
302.057782	14543.677847	28.502106
301.914614	14569.076384	28.507124
302.384282	14607.153858	28.512141
302.584519	14632.880829	28.517159
303.038508	14670.158701	28.522176
303.489046	14691.829303	28.527194
303.425505	14722.843504	28.532212
303.638783	14747.791665	28.537229
304.275426	14763.659970	28.542247
304.420422	14799.536874	28.547264
305.222519	14820.037696	28.552282
305.493899	14851.208084	28.557300
305.924870	14869.572120	28.562317
306.302061	14896.231831	28.567335
306.151942	14914.731152	28.572352
307.295379	14933.719517	28.577370
307.545981	14956.280783	28.582388
307.694614	14964.734323	28.587405
308.427012	14989.159325	28.592423
308.312243	15000.417620	28.597440
309.002853	15017.945246	28.602458
309.025310	15046.767297	28.607476
308.941969	15056.918466	28.612493
309.455339	15083.740286	28.617511
309.499545	15116.020505	28.622528
310.248819	15134.363360	28.627546
310.547690	15152.160921	28.632564
310.830179	15171.205431	28.637581
311.236576	15179.353392	28.642599
311.118023	15207.395568	28.647616
311.756929	15223.077563	28.652634
312.069527	15234.436439	28.657652
313.098280	15250.875389	28.662669
313.794825	15257.853577	28.667687
314.018431	15268.386305	28.672704
314.443541	15267.852350	28.677722
314.663486	15275.202083	28.682740
314.615250	15293.613169	28.687757
314.931608	15301.750020	28.692775
315.240721	15318.159633	28.697792
315.125256	15336.590767	28.702810
315.267007	15347.243743	28.707828
315.196251	15372.957309	28.712845
315.789335	15401.835792	28.717863
315.603175	15420.574963	28.722880
316.359079	15454.651900	28.727898
316.147916	15473.439256	28.732916
316.347468	15501.425714	28.737933
316.656158	15523.403731	28.742951
316.948087	15564.325042	28.747968
317.276283	15594.034897	28.752986
317.645375	15639.511269	28.758004
317.892226	15659.954688	28.763021
318.305156	15690.229399	28.768039
318.598200	15732.142623	28.773056
319.054573	15743.289777	28.778074
319.432383	15778.415092	28.783092
319.658785	15808.242292	28.788109
320.296427	15837.872466	28.793127
320.308985	15862.913531	28.798144
320.980255	15886.186964	28.803162
321.033965	15916.834144	28.808180
320.814108	15945.066978	28.813197
321.362096	15965.968897	28.818215
321.397224	15999.259559	28.823232
322.301839	16021.353253	28.828250
322.499840	16047.309880	28.833268
322.814958	16084.113227	28.838285
323.105547	16112.939095	28.843303
323.194478	16138.758166	28.848320
323.674346	16164.904524	28.853338
324.191748	16197.680958	28.858356
324.438168	16219.217866	28.863373
325.059005	16244.754777	28.868391
325.020915	16284.251154	28.873408
325.929328	16300.927796	28.878426
325.975447	16322.316163	28.883444
326.140997	16340.922173	28.888461
326.501869	16360.849436	28.893479
326.675490	16401.051975	28.898496
327.376752	16425.714260	28.903514
327.578851	16457.637198	28.908532
327.583375	16490.383922	28.913549
327.944260	16507.718202	28.918567
328.467676	16544.786701	28.923584
329.271159	16574.726837	28.928602
330.069406	16584.270095	28.933620
329.855859	16616.157331	28.938637
330.231117	16631.986013	28.943655
330.505579	16652.991539	28.948672
331.041281	16674.508911	28.953690
331.337582	16695.368928	28.958708
331.529987	16722.243318	28.963725
332.071067	16730.651955	28.968743
332.049401	16766.245942	28.973760
332.082802	16789.272948	28.978778
332.860242	16826.087414	28.983796
332.896709	16853.703407	28.988813
333.198704	16881.622130	28.993831
333.751550	16905.104864	28.998848
333.863859	16938.644059	29.003866
334.445861	16968.363657	29.008884
334.527534	16988.768032	29.013901
334.698303	17010.674595	29.018919
335.261286	17045.627919	29.023936
335.650132	17080.191649	29.028954
336.067371	17106.431220	29.033972
336.415712	17129.800965	29.038989
336.901827	17151.885712	29.044007
337.183052	17176.112535	29.049024
337.864652	17189.568946	29.054042
338.564841	17201.019888	29.059060
338.714463	17233.277666	29.064077
339.308033	17241.176084	29.069095
339.539045	17264.621227	29.074112
339.588475	17283.470598	29.079130
340.284677	17300.121339	29.084148
340.190837	17331.457192	29.089165
340.503072	17350.928777	29.094183
340.833360	17358.742139	29.099200
341.389057	17377.853433	29.104218
341.811681	17398.925005	29.109236
341.890466	17422.754272	29.114253
342.329047	17442.578880	29.119271
342.128054	17466.275140	29.124288
342.692848	17496.149863	29.129306
343.305119	17524.570521	29.134324
343.254752	17542.943024	29.139341
343.847699	17563.267917	29.144359
343.970751	17590.773479	29.149376
344.382883	17610.539229	29.154394
344.776107	17627.806277	29.159412
344.595928	17661.335685	29.164429
345.416769	17677.929325	29.169447
345.404545	17697.641605	29.174464
345.555351	17730.759194	29.179482
346.066139	17758.014735	29.184500
345.992064	17790.346386	29.189517
346.689578	17804.849430	29.194535
347.021940	17846.277802	29.199552
346.970778	17881.891093	29.204570
347.179375	17913.944924	29.209588
347.617090	17951.181165	29.214605
347.791453	17982.223356	29.219623
348.718240	18021.985934	29.224640
348.885897	18055.935349	29.229658
349.041833	18078.584594	29.234676
349.263175	18116.461528	29.239693
350.009440	18151.647160	29.244711
350.806926	18177.898115	29.249728
351.121269	18205.627286	29.254746
351.613168	18236.380076	29.259764
351.855665	18263.690989	29.264781
352.526803	18292.387845	29.269799
352.731009	18317.152521	29.274816
352.897122	18341.114540	29.279834
353.521650	18367.178045	29.284852
353.791016	18397.801690	29.289869
354.117861	18420.051821	29.294887
355.163852	18446.005189	29.299904
354.797024	18481.808013	29.304922
354.965565	18485.262710	29.309940
355.136214	18526.964253	29.314957
355.872539	18545.833606	29.319975
356.192689	18571.616544	29.324992
356.483888	18602.546659	29.330010
356.763119	18635.753073	29.335028
356.734829	18669.582627	29.340045
357.427316	18689.501412	29.345063
357.875413	18726.611158	29.350080
357.813884	18754.216773	29.355098
358.389639	18787.787653	29.360116
358.493036	18823.100473	29.365133
359.242875	18859.146044	29.370151
359.851980	18883.285733	29.375168
359.683587	18907.585147	29.380186
360.388763	18944.396009	29.385204
360.927234	18978.990226	29.390221
361.504656	19016.964762	29.395239
361.953458	19040.674873	29.400256
362.293053	19071.553926	29.405274
363.061915	19090.816738	29.410292
362.882874	19111.959144	29.415309
363.655887	19134.506640	29.420327
364.041043	19166.275845	29.425344
364.048712	19181.589264	29.430362
364.438635	19204.468518	29.435380
364.457566	19225.567400	29.440397
364.865735	19258.710453	29.445415
365.529242	19283.031654	29.450432
365.527904	19304.778225	29.455450
365.775965	19339.014224	29.460468
366.051382	19374.730715	29.465485
366.514250	19405.287725	29.470503
366.647609	19433.659836	29.475520
366.861321	19467.111692	29.480538
367.719167	19500.608023	29.485556
367.842830	19538.294525	29.490573
368.102424	19555.476812	29.495591
368.592263	19585.290672	29.500608
368.892369	19616.890709	29.505626
369.120078	19642.727450	29.510644
369.756783	19671.141104	29.515661
370.100058	19704.768931	29.520679
370.853532	19722.057228	29.525696
371.006659	19750.578335	29.530714
371.289136	19790.849810	29.535732
371.726109	19808.453119	29.540749
371.818108	19831.190230	29.545767
372.765486	19856.604939	29.550784
373.091128	19886.046937	29.555802
373.605551	19905.754771	29.560820
373.927720	19933.352492	29.565837
374.805074	19945.484943	29.570855
375.828837	19961.859213	29.575872
375.765111	19969.830118	29.580890
376.262220	19990.077792	29.585908
376.656703	20005.817763	29.590925
376.578171	20017.019584	29.595943
377.245261	20041.334851	29.600960
376.867512	20059.647275	29.605978
377.488853	20079.376446	29.610996
377.631365	20110.477556	29.616013
377.858825	20129.971520	29.621031
378.655166	20159.175926	29.626048
378.975370	20186.218310	29.631066
379.148093	20209.448672	29.636084
379.411916	20243.083551	29.641101
379.707934	20277.534816	29.646119
380.175061	20301.142494	29.651136
380.419077	20337.718624	29.656154
380.848466	20366.026759	29.661172
380.753466	20393.216602	29.666189
381.047893	20434.498451	29.671207
381.622623	20468.331429	29.676224
381.629781	20512.337400	29.681242
382.041332	20545.014545	29.686260
382.403224	20600.224408	29.691277
382.533332	20633.192200	29.696295
383.361894	20674.138152	29.701312
383.827379	20712.417839	29.706330
384.162585	20758.805551	29.711348
384.715114	20795.447938	29.716365
384.556819	20832.542929	29.721383
385.042190	20869.878362	29.726400
385.305205	20915.228891	29.731418
385.684241	20955.039018	29.736436
386.687669	20987.750557	29.741453
387.113328	21023.977267	29.746471
387.756314	21060.542794	29.751488
388.066411	21093.887546	29.756506
388.489664	21125.066336	29.761524
389.090308	21156.451174	29.766541
389.508832	21194.518006	29.771559
390.288382	21213.004060	29.776576
390.551025	21247.746585	29.781594
391.360844	21267.049360	29.786612
391.541939	21292.863980	29.791629
391.819302	21312.970519	29.796647
392.162489	21333.129954	29.801664
392.450489	21362.851759	29.806682
392.741826	21384.611653	29.811700
393.778766	21396.492543	29.816717
394.222066	21412.055393	29.821735
394.663405	21435.832758	29.826752
394.706357	21455.445397	29.831770
395.034888	21477.471268	29.836788
395.364610	21489.823153	29.841805
395.592277	21517.741194	29.846823
395.812747	21538.387641	29.851840
396.120231	21570.766856	29.856858
396.377318	21591.325480	29.861876
397.057318	21606.478607	29.866893
397.156300	21643.376855	29.871911
397.715594	21662.921459	29.876928
398.093485	21689.843135	29.881946
398.435251	21717.370784	29.886964
398.859184	21756.676318	29.891981
399.045661	21787.400383	29.896999
399.514403	21804.444459	29.902016
399.714132	21845.990526	29.907034
400.018045	21885.308797	29.912052
400.333164	21913.371668	29.917069
400.785421	21956.527610	29.922087
401.516519	21982.560281	29.927104
401.386947	22024.177259	29.932122
401.447273	22056.450650	29.937140
401.964158	22112.575649	29.942157
402.615271	22154.866789	29.947175
403.379984	22189.835631	29.952192
403.531107	22233.361605	29.957210
404.085293	22272.597210	29.962228
404.439613	22298.209080	29.967245
404.887763	22340.374435	29.972263
405.440372	22369.689809	29.977280
405.825576	22407.972720	29.982298
406.604505	22434.699895	29.987316
407.310695	22458.038912	29.992333
407.192157	22500.533491	29.997351
407.698544	22533.066373	30.002368
408.150870	22567.756228	30.007386
408.304489	22602.865751	30.012404
408.614942	22623.770950	30.017421
409.279851	22667.906170	30.022439
409.525337	22700.120009	30.027456
410.062091	22739.934299	30.032474
410.372816	22780.466530	30.037492
410.624831	22821.292397	30.042509
410.667070	22861.215983	30.047527
411.792369	22889.425052	30.052544
412.051086	22935.943591	30.057562
412.761882	22970.277709	30.062580
413.120727	22989.659129	30.067597
413.089465	23031.142750	30.072615
413.438703	23068.453103	30.077632
414.245983	23102.898720	30.082650
414.365246	23142.374784	30.087668
414.856430	23186.904878	30.092685
415.446102	23230.534959	30.097703
415.830207	23257.116554	30.102720
416.328913	23293.689848	30.107738
416.660600	23326.213477	30.112756
417.467318	23365.670774	30.117773
417.676847	23403.319598	30.122791
418.173408	23421.239082	30.127808
418.275998	23450.089403	30.132826
418.980578	23485.531252	30.137844
419.366603	23526.305976	30.142861
419.333052	23572.366236	30.147879
419.897491	23600.632570	30.152896
420.350435	23639.722430	30.157914
420.541842	23675.649433	30.162932
421.236950	23710.530747	30.167949
421.793980	23742.469976	30.172967
422.506892	23763.635621	30.177984
422.862858	23797.824525	30.183002
423.028617	23820.908548	30.188020
423.589541	23842.711063	30.193037
423.992509	23875.363448	30.198055
424.733973	23900.366954	30.203072
424.957731	23921.375567	30.208090
425.508906	23944.879639	30.213108
425.938186	23973.401490	30.218125
426.450264	24010.959834	30.223143
427.094291	24031.340305	30.228160
426.953219	24061.600991	30.233178
427.573100	24082.433977	30.238196
428.264719	24109.113888	30.243213
428.280866	24153.821657	30.248231
428.536723	24172.853830	30.253248
428.661231	24219.668118	30.258266
428.951111	24247.245312	30.263284
429.422311	24290.845711	30.268301
429.600877	24330.592891	30.273319
430.186744	24371.413870	30.278336
430.909221	24411.486786	30.283354
430.850108	24453.318973	30.288372
431.598600	24488.136407	30.293389
431.779842	24532.831800	30.298407
432.665641	24570.231543	30.303424
433.242086	24612.324730	30.308442
433.617497	24653.577384	30.313460
434.111459	24691.582216	30.318477
434.606583	24738.421819	30.323495
435.250572	24766.443514	30.328512
435.407362	24814.568624	30.333530
435.841502	24841.353037	30.338548
436.684764	24866.032142	30.343565
436.923408	24901.492606	30.348583
437.362396	24931.461514	30.353600
437.757792	24959.794166	30.358618
438.359171	24996.676798	30.363636
438.955369	25023.328636	30.368653
439.407880	25066.168958	30.373671
439.412448	25097.350034	30.378688
440.058224	25132.987288	30.383706
440.131127	25174.250475	30.388724
440.710045	25209.727702	30.393741
440.874968	25249.750587	30.398759
440.982557	25290.300759	30.403776
441.424491	25338.426696	30.408794
442.153631	25386.286568	30.413812
442.773965	25428.197633	30.418829
443.217527	25470.503027	30.423847
443.542075	25508.820334	30.428864
444.036142	25546.668768	30.433882
444.316780	25589.132648	30.438900
444.920216	25629.239280	30.443917
445.261954	25672.660716	30.448935
445.725796	25718.616386	30.453952
445.865547	25769.084830	30.458970
445.712465	25812.185910	30.463988
446.837031	25864.377378	30.469005
447.010624	25914.107761	30.474023
447.319103	25974.276811	30.479040
448.108307	26013.198541	30.484058
448.802575	26069.060369	30.489076
448.940309	26103.401137	30.494093
449.364311	26154.388507	30.499111
450.138612	26202.533965	30.504128
450.643822	26232.721960	30.509146
450.946617	26285.390838	30.514164
451.595051	26317.509450	30.519181
451.959439	26361.143701	30.524199
452.498848	26408.340496	30.529216
452.932806	26440.720424	30.534234
453.284959	26484.799271	30.539252
454.014531	26522.018546	30.544269
454.312714	26568.476110	30.549287
454.830510	26599.692879	30.554304
455.999876	26624.190340	30.559322
456.380545	26658.026299	30.564340
456.874577	26685.713899	30.569357
457.241605	26723.660278	30.574375
457.638833	26755.711488	30.579392
458.144523	26785.837030	30.584410
458.609810	26828.540041	30.589428
459.044074	26850.037002	30.594445
459.057205	26884.695665	30.599463
459.619358	26932.364141	30.604480
460.287886	26967.697694	30.609498
460.215680	27018.537424	30.614516
460.600284	27045.806550	30.619533
460.966841	27099.731629	30.624551
461.262363	27143.808136	30.629568
461.680262	27181.311294	30.634586
461.677181	27234.662585	30.639604
462.848776	27285.687393	30.644621
463.374710	27330.714207	30.649639
464.122651	27366.465807	30.654656
464.997428	27401.325376	30.659674
465.106064	27443.674708	30.664692
465.564577	27472.064199	30.669709
466.157229	27532.161754	30.674727
466.504756	27579.106899	30.679744
467.231723	27610.482077	30.684762
467.105785	27658.917368	30.689780
468.040373	27693.060166	30.694797
468.587316	27728.717473	30.699815
469.343841	27765.365953	30.704832
469.845104	27791.536983	30.709850
470.423017	27845.089619	30.714868
470.319366	27877.271612	30.719885
471.184683	27910.079329	30.724903
471.436161	27958.588950	30.729920
472.069811	27997.671587	30.734938
472.579505	28039.181895	30.739956
473.121101	28071.825673	30.744973
473.443599	28109.200105	30.749991
473.666172	28154.156159	30.755008
474.260582	28184.181386	30.760026
474.845545	28234.390271	30.765044
475.331802	28260.987744	30.770061
475.866266	28307.911607	30.775079
475.997275	28351.024129	30.780096
476.226497	28392.130308	30.785114
476.461443	28438.956005	30.790132
477.259113	28475.782621	30.795149
477.704671	28530.571380	30.800167
478.018683	28578.067661	30.805184
478.359091	28624.276783	30.810202
478.950968	28680.857115	30.815220
479.560210	28718.162463	30.820237
480.421839	28767.014575	30.825255
480.929371	28800.448644	30.830272
481.488546	28836.181819	30.835290
481.864763	28885.034390	30.840308
482.499195	28915.756048	30.845325
482.796606	28948.401545	30.850343
483.038186	28993.994881	30.855360
483.450248	29029.966349	30.860378
483.552339	29068.691819	30.865396
484.131495	29115.553641	30.870413
484.549967	29158.452167	30.875431
484.627626	29207.415477	30.880448
485.291332	29258.581657	30.885466
485.913688	29314.767057	30.890484
486.503371	29365.053825	30.895501
486.764989	29404.918023	30.900519
487.360856	29453.573193	30.905536
488.105096	29495.201421	30.910554
488.593131	29545.782681	30.915572
489.051325	29588.233401	30.920589
489.845578	29631.143588	30.925607
490.115826	29679.508949	30.930624
491.001376	29720.963793	30.935642
491.734326	29765.027999	30.940660
492.183362	29803.491910	30.945677
493.007130	29832.036066	30.950695
493.051240	29879.432239	30.955712
494.177372	29905.027685	30.960730
494.215530	29937.715356	30.965748
495.060402	29978.153044	30.970765
495.972923	30010.779740	30.975783
496.205762	30046.850591	30.980800
496.675433	30078.402599	30.985818
497.161099	30109.730904	30.990836
497.253250	30151.614305	30.995853
497.354648	30194.318118	31.000871
497.711553	30237.652064	31.005888
498.510452	30279.071033	31.010906
499.372174	30334.779227	31.015924
499.518049	30374.808819	31.020941
500.460307	30406.382132	31.025959
500.502510	30461.460455	31.030976
501.066962	30493.624074	31.035994
501.661663	30536.118578	31.041012
502.110078	30575.013883	31.046029
502.563909	30601.790145	31.051047
502.941542	30659.060579	31.056064
503.809355	30697.049667	31.061082
503.916900	30742.920721	31.066100
504.116457	30788.486674	31.071117
504.652612	30838.633700	31.076135
505.078963	30900.638330	31.081152
505.767819	30942.429871	31.086170
505.980635	30992.817559	31.091188
506.563734	31045.669696	31.096205
507.406924	31101.174243	31.101223
507.553001	31149.398125	31.106240
508.235139	31201.640913	31.111258
508.823473	31257.773709	31.116276
509.209285	31313.736083	31.121293
509.783943	31363.745591	31.126311
510.229327	31411.746195	31.131328
510.674348	31466.915814	31.136346
510.735891	31515.514123	31.141364
511.330963	31572.354749	31.146381
512.027598	31630.399728	31.151399
512.244140	31688.374661	31.156416
512.968612	31731.963926	31.161434
513.691455	31796.845470	31.166452
514.080093	31844.603086	31.171469
514.599059	31896.993292	31.176487
515.119489	31947.316145	31.181504
515.720243	31991.962121	31.186522
516.250168	32038.326201	31.191540
516.478119	32088.518190	31.196557
517.408639	32133.435238	31.201575
517.792711	32193.345135	31.206592
518.405443	32234.228190	31.211610
519.137056	32278.177832	31.216628
519.101589	32320.762040	31.221645
519.997781	32372.544345	31.226663
520.907457	32419.690622	31.231680
521.470972	32461.580711	31.236698
521.617276	32509.377802	31.241716
521.711207	32551.164600	31.246733
522.595662	32603.265418	31.251751
523.443744	32661.580361	31.256768
523.615017	32703.658810	31.261786
524.384821	32744.246412	31.266804
524.697788	32790.563954	31.271821
524.987914	32834.912665	31.276839
525.397957	32898.291372	31.281856
526.188572	32948.359365	31.286874
526.486638	33009.031084	31.291892
526.957558	33071.294395	31.296909
527.827163	33127.388165	31.301927
527.957622	33173.400058	31.306944
528.261052	33236.657395	31.311962
529.145819	33292.060104	31.316980
529.561047	33340.367007	31.321997
530.333836	33394.782279	31.327015
530.866543	33449.835916	31.332032
531.817826	33509.180239	31.337050
532.114039	33559.839235	31.342068
532.678556	33619.111675	31.347085
533.304070	33666.298942	31.352103
533.618289	33726.028162	31.357120
534.278333	33774.139659	31.362138
535.318495	33825.770235	31.367156
535.240473	33879.618225	31.372173
536.288790	33925.254075	31.377191
536.544628	33993.996407	31.382208
536.751970	34039.523963	31.387226
537.730654	34090.494632	31.392244
537.983834	34157.688895	31.397261
538.701880	34198.875412	31.402279
538.836521	34261.441490	31.407296
539.340906	34313.941177	31.412314
540.055894	34373.274363	31.417332
540.774307	34437.785414	31.422349
541.535725	34489.707857	31.427367
541.717124	34544.629695	31.432384
542.474621	34605.259344	31.437402
542.944265	34649.982089	31.442420
543.010206	34719.009427	31.447437
543.681489	34773.045825	31.452455
544.219551	34839.792980	31.457472
544.620339	34902.022098	31.462490
545.039845	34961.162946	31.467508
545.314583	35031.631809	31.472525
546.105194	35089.178450	31.477543
547.124107	35158.538499	31.482560
547.020069	35215.466860	31.487578
547.936956	35281.087510	31.492596
548.470127	35343.044271	31.497613
549.185079	35404.239284	31.502631
549.911646	35465.394717	31.507648
550.405567	35520.421883	31.512666
551.263290	35582.897579	31.517684
551.449465	35633.869630	31.522701
552.198592	35692.429759	31.527719
552.468095	35742.048541	31.532736
552.750008	35799.050799	31.537754
553.886257	35854.073074	31.542772
553.902012	35911.850792	31.547789
554.606897	35964.025976	31.552807
555.027782	36029.473696	31.557824
555.525893	36095.042306	31.562842
556.344597	36150.589315	31.567860
557.383215	36198.684966	31.572877
559.435941	36203.118551	31.577895
560.356730	36231.858595	31.582912
561.021999	36260.265630	31.587930
561.484265	36287.635879	31.592948
561.341679	36316.024080	31.597965
562.424095	36356.013226	31.602983
562.852202	36381.719621	31.608000
563.159283	36421.482545	31.613018
563.367697	36460.634996	31.618036
564.155449	36504.300105	31.623053
564.331892	36538.696303	31.628071
564.733763	36589.832878	31.633088
564.733137	36641.734497	31.638106
565.488341	36680.947150	31.643124
565.616546	36746.556725	31.648141
566.070287	36789.281968	31.653159
566.518464	36852.584327	31.658176
566.723916	36915.273582	31.663194
567.412821	36973.315497	31.668212
567.922088	37047.554641	31.673229
568.563150	37106.394835	31.678247
568.883045	37178.944122	31.683264
569.317079	37244.355559	31.688282
570.081195	37312.156362	31.693300
570.782301	37381.889593	31.698317
571.300778	37447.604599	31.703335
571.840094	37507.713885	31.708352
572.312027	37589.662823	31.713370
572.942654	37658.238129	31.718388
573.167711	37732.834009	31.723405
573.747575	37799.027391	31.728423
574.934893	37868.964293	31.733440
575.354793	37940.773267	31.738458
576.224332	38001.749147	31.743476
576.664906	38075.585235	31.748493
577.475525	38131.600279	31.753511
577.995421	38212.981264	31.758528
578.189355	38270.825957	31.763546
578.971789	38335.560092	31.768564
579.414821	38407.499796	31.773581
579.973564	38473.034556	31.778599
580.712530	38538.408488	31.783616
581.144240	38605.519211	31.788634
582.071276	38674.797543	31.793652
582.972181	38739.236082	31.798669
583.098472	38803.119470	31.803687
584.084438	38865.780692	31.808704
584.346168	38937.484947	31.813722
585.145254	39001.605045	31.818740
585.761383	39066.633021	31.823757
586.358695	39132.366105	31.828775
586.983840	39195.685573	31.833792
587.259724	39255.840983	31.838810
588.090219	39317.288346	31.843828
588.212444	39388.883136	31.848845
589.020542	39450.903553	31.853863
589.903863	39504.197724	31.858880
590.245798	39582.133456	31.863898
590.745441	39638.390829	31.868916
591.496039	39703.779104	31.873933
591.826156	39763.699755	31.878951
592.698571	39820.367207	31.883968
592.975519	39878.841933	31.888986
593.516152	39946.325519	31.894004
593.781612	40014.035815	31.899021
594.632406	40081.755838	31.904039
595.124577	40137.522375	31.909056
595.626844	40222.056836	31.914074
596.052377	40292.146170	31.919092
596.943786	40364.116998	31.924109
597.178976	40431.396946	31.929127
598.008242	40497.970594	31.934144
598.362777	40573.928356	31.939162
599.545541	40648.997736	31.944180
600.067768	40721.552490	31.949197
600.826593	40788.599741	31.954215
601.576500	40853.732268	31.959232
602.264854	40913.138278	31.964250
602.861522	40963.521033	31.969268
603.726742	41035.542446	31.974285
604.477955	41101.953069	31.979303
605.125871	41150.778705	31.984320
605.829930	41211.011587	31.989338
607.106770	41254.780459	31.994356
607.865141	41306.903251	31.999373
608.598792	41368.529678	32.004391
608.829524	41413.835154	32.009408
609.243530	41467.100102	32.014426
610.093882	41510.936281	32.019444
610.403284	41573.274845	32.024461
610.908952	41626.614371	32.029479
611.458163	41685.209400	32.034496
611.711908	41748.917000	32.039514
611.900585	41813.488821	32.044532
613.114128	41882.574358	32.049549
613.218031	41943.181531	32.054567
614.066265	42007.182588	32.059584
614.485406	42072.965071	32.064602
615.047511	42135.000004	32.069620
616.408026	42192.792562	32.074637
617.024340	42263.674227	32.079655
617.652915	42318.197914	32.084672
617.889497	42391.770633	32.089690
618.939799	42445.962940	32.094708
619.790898	42504.715269	32.099725
619.941743	42571.951729	32.104743
620.999068	42625.004876	32.109760
621.357671	42682.183976	32.114778
621.974662	42742.295534	32.119796
622.464696	42808.069103	32.124813
622.984977	42876.058238	32.129831
623.929191	42919.566268	32.134848
624.482633	42984.381665	32.139866
625.142686	43036.992008	32.144884
625.461474	43105.095629	32.149901
625.739434	43171.099569	32.154919
626.188840	43232.674519	32.159936
626.871122	43313.859287	32.164954
627.283769	43378.944570	32.169972
627.960965	43462.148428	32.174989
628.389515	43536.668973	32.180007
628.894449	43613.910336	32.185024
629.838683	43693.518419	32.190042
629.822841	43773.289794	32.195060
630.464708	43852.433446	32.200077
630.951354	43943.499756	32.205095
631.678879	44013.268979	32.210112
632.050945	44096.826615	32.215130
632.947756	44175.526659	32.220148
633.147054	44258.422482	32.225165
633.516065	44343.373126	32.230183
634.440055	44429.154381	32.235200
635.114110	44510.104428	32.240218
635.532878	44596.920608	32.245236
636.363635	44663.436998	32.250253
636.753560	44752.965658	32.255271
637.832113	44838.926700	32.260288
638.334513	44922.580872	32.265306
639.035841	45013.447127	32.270324
639.906013	45086.644868	32.275341
640.472542	45172.636772	32.280359
641.662225	45249.871439	32.285376
641.953074	45342.985703	32.290394
642.556877	45413.721214	32.295412
643.441281	45499.727847	32.300429
643.631096	45580.567821	32.305447
644.983324	45649.769873	32.310464
645.232254	45734.807852	32.315482
646.054024	45816.378397	32.320500
646.668105	45898.804137	32.325517
647.215856	45984.593330	32.330535
648.147986	46053.375316	32.335552
649.017093	46137.381443	32.340570
649.892370	46222.373779	32.345588
650.301294	46299.310481	32.350605
650.602403	46376.662872	32.355623
651.531408	46464.614638	32.360640
652.032848	46546.402469	32.365658
652.574985	46618.106663	32.370676
653.666150	46700.081044	32.375693
653.917051	46792.802673	32.380711
655.180784	46866.880844	32.385728
655.421180	46951.836173	32.390746
655.783937	47030.060490	32.395764
656.405335	47123.263179	32.400781
656.862439	47217.282771	32.405799
657.611598	47301.558732	32.410816
658.165488	47394.039250	32.415834
658.547413	47490.216381	32.420852
659.387095	47582.482096	32.425869
659.679079	47673.821727	32.430887
660.620434	47769.817533	32.435904
660.862927	47869.497662	32.440922
661.350904	47969.241005	32.445940
662.590409	48067.393004	32.450957
662.636043	48169.427117	32.455975
663.172785	48274.756856	32.460992
663.956631	48376.492812	32.466010
664.425151	48488.103918	32.471028
665.014219	48590.611550	32.476045
665.738897	48711.888787	32.481063
666.636988	48815.000682	32.486080
666.947014	48919.255382	32.491098
667.472312	49035.042267	32.496116
668.387118	49145.555411	32.501133
669.078498	49258.274198	32.506151
669.714044	49363.232834	32.511168
670.288597	49463.013412	32.516186
670.728385	49581.859699	32.521204
671.629860	49690.713559	32.526221
672.063968	49812.333151	32.531239
673.066898	49918.495864	32.536256
673.997852	50039.735148	32.541274
674.591856	50141.458035	32.546292
675.576347	50250.586258	32.551309
676.100840	50354.288713	32.556327
677.064149	50442.212456	32.561344
677.926406	50550.083140	32.566362
678.366090	50652.851130	32.571380
679.344585	50735.775073	32.576397
679.570203	50831.883112	32.581415
680.250151	50919.005181	32.586432
680.923535	51026.996247	32.591450
681.335776	51125.803372	32.596468
682.632944	51225.339190	32.601485
683.476359	51324.117599	32.606503
684.070944	51418.727627	32.611520
684.750313	51516.494838	32.616538
685.502443	51615.687413	32.621556
686.391365	51708.980694	32.626573
686.804835	51810.511380	32.631591
687.469370	51900.157915	32.636608
688.199220	51996.672698	32.641626
688.432678	52100.757561	32.646644
689.300389	52200.839379	32.651661
689.949231	52315.446364	32.656679
690.441838	52416.840737	32.661696
690.852314	52538.560559	32.666714
691.647554	52644.394917	32.671732
692.613003	52748.399665	32.676749
693.006283	52864.561710	32.681767
693.320309	52975.959180	32.686784
694.588319	53103.907176	32.691802
694.902295	53213.692160	32.696820
695.755777	53333.701460	32.701837
696.470200	53448.677060	32.706855
696.942476	53562.412876	32.711872
697.678666	53688.435016	32.716890
698.152025	53809.892119	32.721908
698.765580	53920.804182	32.726925
699.640995	54041.674279	32.731943
700.683994	54161.683426	32.736960
701.120334	54280.712386	32.741978
701.543161	54407.863237	32.746996
702.740701	54526.476797	32.752013
703.325477	54652.869517	32.757031
704.112877	54774.927884	32.762048
705.068968	54881.025539	32.767066
705.320031	55014.838707	32.772084
706.167868	55128.624488	32.777101
706.921359	55254.070029	32.782119
707.955014	55373.517206	32.787136
708.751953	55491.578126	32.792154
709.257241	55614.127977	32.797172
710.343246	55726.018709	32.802189
711.132253	55854.809693	32.807207
711.457821	55967.687668	32.812224
712.326871	56070.905713	32.817242
713.149930	56197.788269	32.822260
714.202727	56321.566059	32.827277
714.601705	56432.453820	32.832295
715.642084	56554.013343	32.837312
716.263901	56657.551103	32.842330
716.826417	56767.965453	32.847348
717.596226	56886.651408	32.852365
718.458257	56999.241374	32.857383
719.069837	57107.801545	32.862400
720.005669	57214.615250	32.867418
720.256943	57327.859351	32.872436
721.489761	57440.627490	32.877453
721.921107	57552.135593	32.882471
722.870105	57672.613814	32.887488
723.977643	57773.833467	32.892506
724.343168	57878.619153	32.897524
725.054516	57984.509384	32.902541
725.432633	58085.173669	32.907559
726.118201	58188.056106	32.912576
727.288222	58294.135365	32.917594
728.011798	58396.651965	32.922612
728.416102	58511.567572	32.927629
729.329005	58613.625045	32.932647
729.827723	58719.785973	32.937664
730.689956	58835.099775	32.942682
731.090185	58940.555533	32.947700
731.897754	59056.049839	32.952717
732.592791	59163.682051	32.957735
733.795301	59270.621302	32.962752
734.891953	59376.128126	32.967770
735.638844	59478.493725	32.972788
736.665649	59577.163720	32.977805
737.104640	59691.509793	32.982823
737.962468	59789.485525	32.987840
738.720751	59897.459201	32.992858
739.127152	60005.222608	32.997876
739.991384	60106.743265	33.002893
740.797314	60211.843480	33.007911
741.181649	60325.498463	33.012928
741.820301	60440.247192	33.017946
742.537984	60565.415737	33.022964
743.061710	60668.055459	33.027981
744.013552	60790.377998	33.032999
744.328167	60908.534526	33.038016
745.254179	61022.361103	33.043034
746.105663	61141.700679	33.048052
747.404095	61258.122311	33.053069
748.093824	61363.600126	33.058087
748.995510	61483.566503	33.063104
749.934008	61591.380131	33.068122
750.362495	61705.743540	33.073140
751.064183	61817.412337	33.078157
752.114281	61928.128183	33.083175
752.693362	62043.900205	33.088192
753.399463	62145.903472	33.093210
754.199335	62265.389486	33.098228
755.224043	62378.782717	33.103245
755.811852	62489.155656	33.108263
756.835605	62606.196375	33.113280
757.536854	62707.189839	33.118298
757.863585	62823.948244	33.123316
758.673805	62939.973112	33.128333
759.397452	63053.353256	33.133351
760.219783	63171.390410	33.138368
761.307899	63284.404332	33.143386
761.611446	63406.284201	33.148404
762.670822	63520.917999	33.153421
763.662350	63628.554894	33.158439
763.929210	63749.885081	33.163456
764.943607	63865.527751	33.168474
765.496255	63982.674013	33.173492
766.182348	64092.557502	33.178509
767.098384	64209.799858	33.183527
767.952078	64319.772050	33.188544
768.839642	64434.228008	33.193562
769.739270	64550.353956	33.198580
770.520616	64665.346731	33.203597
771.182487	64774.711524	33.208615
771.730110	64901.087054	33.213632
772.721787	65005.089500	33.218650
773.565985	65124.221339	33.223668
774.389889	65232.366173	33.228685
775.439303	65335.265660	33.233703
775.734635	65452.136154	33.238720
776.705665	65536.004705	33.243738
777.154050	65652.408974	33.248756
777.778697	65757.605267	33.253773
778.954705	65867.856615	33.258791
779.411210	65971.471990	33.263808
780.384474	66084.871008	33.268826
780.911429	66202.348142	33.273844
782.070181	66321.360369	33.278861
782.577620	66428.015003	33.283879
783.227279	66542.549397	33.288896
784.326906	66646.149116	33.293914
785.150351	66750.583934	33.298932
785.895857	66860.014257	33.303949
786.453036	66975.540122	33.308967
787.430891	67087.144728	33.313984
788.709293	67190.053847	33.319002
789.473799	67296.766823	33.324020
790.317127	67402.752429	33.329037
791.516478	67511.190051	33.334055
791.767677	67629.546365	33.339072
793.155341	67724.215684	33.344090
793.579093	67832.795111	33.349108
794.462826	67950.439676	33.354125
795.029714	68054.343790	33.359143
795.570424	68162.026174	33.364160
796.509029	68261.947202	33.369178
797.304135	68387.060195	33.374196
797.709562	68502.217775	33.379213
798.654135	68616.879868	33.384231
799.179429	68736.072141	33.389248
800.170611	68847.815268	33.394266
801.125746	68979.212705	33.399284
801.576694	69092.770119	33.404301
802.534798	69216.094959	33.409319
802.909087	69347.553556	33.414336
803.952538	69458.410968	33.419354
804.741740	69588.950978	33.424372
805.455185	69712.367141	33.429389
806.678714	69828.972880	33.434407
807.629237	69961.066213	33.439424
808.462812	70077.702466	33.444442
809.328188	70188.356577	33.449460
810.265661	70310.891964	33.454477
811.424747	70427.466143	33.459495
812.300589	70537.423533	33.464512
814.127586	70623.954541	33.469530
814.665412	70731.078102	33.474548
815.438330	70834.517796	33.479565
816.540039	70930.902699	33.484583
817.289264	71027.140512	33.489600
817.991325	71124.842541	33.494618
818.684851	71238.757583	33.499636
819.434386	71346.002481	33.504653
820.196458	71451.396735	33.509671
820.523651	71552.008719	33.514688
821.841175	71656.683554	33.519706
822.290161	71766.104993	33.524724
822.980701	71879.149361	33.529741
824.434378	71982.005682	33.534759
825.122271	72084.019738	33.539776
825.778898	72192.675830	33.544794
826.336282	72302.031851	33.549812
827.075346	72413.513035	33.554829
827.545469	72519.387895	33.559847
828.127968	72648.183274	33.564864
829.361060	72776.066790	33.569882
829.806999	72884.315401	33.574900
830.663516	72996.553260	33.579917
831.491630	73110.138633	33.584935
831.801949	73229.492624	33.589952
832.658762	73329.977756	33.594970
833.460012	73454.309649	33.599988
833.943448	73579.603854	33.605005
835.016271	73700.449160	33.610023
835.726469	73835.335418	33.615040
836.295430	73953.423507	33.620058
837.185260	74074.349821	33.625076
838.262104	74211.270523	33.630093
839.240941	74326.205446	33.635111
839.889054	74451.566607	33.640128
840.613718	74582.502371	33.645146
841.418454	74707.675534	33.650164
841.943054	74851.741347	33.655181
843.261292	74978.520047	33.660199
843.779413	75107.603342	33.665216
844.783218	75244.046725	33.670234
845.770504	75379.138009	33.675252
846.392719	75514.629145	33.680269
847.519105	75642.454373	33.685287
848.313790	75775.323035	33.690304
849.077702	75918.141001	33.695322
850.341169	76060.818158	33.700340
850.858774	76195.708374	33.705357
851.552216	76329.406316	33.710375
852.619441	76465.959924	33.715392
853.111496	76597.777914	33.720410
854.089131	76755.704623	33.725428
854.894043	76898.711327	33.730445
856.249053	77028.255418	33.735463
857.019338	77174.309263	33.740480
857.756768	77313.832366	33.745498
858.782746	77449.523260	33.750516
859.477960	77602.963930	33.755533
860.882269	77729.450610	33.760551
861.377534	77869.951902	33.765568
862.303433	77998.554313	33.770586
863.261991	78137.109520	33.775604
864.095754	78293.458731	33.780621
865.275834	78417.335987	33.785639
866.134219	78554.996849	33.790656
867.185906	78687.535356	33.795674
867.831549	78824.926827	33.800692
869.186509	78959.496809	33.805709
870.303073	79072.415845	33.810727
871.060168	79204.546880	33.815744
872.371827	79325.557114	33.820762
873.249712	79449.232929	33.825780
874.069466	79579.506271	33.830797
875.178706	79704.984001	33.835815
875.799558	79822.341858	33.840832
876.530881	79937.250433	33.845850
877.602124	80065.206220	33.850868
878.405212	80184.982225	33.855885
879.157902	80313.521137	33.860903
880.149032	80446.039500	33.865920
880.649029	80575.898791	33.870938
881.775330	80693.143151	33.875956
882.320284	80819.550428	33.880973
883.473837	80948.118170	33.885991
884.065384	81091.027881	33.891008
884.989561	81225.460859	33.896026
885.502265	81349.721713	33.901044
886.732864	81488.111618	33.906061
887.261209	81614.651764	33.911079
888.037260	81747.729405	33.916096
888.994976	81874.913003	33.921114
890.030134	81999.056897	33.926132
890.844144	82126.352818	33.931149
891.570947	82262.468753	33.936167
892.379448	82396.925416	33.941184
893.327729	82524.100735	33.946202
893.687630	82645.185610	33.951220
894.390650	82792.331032	33.956237
895.489523	82931.052702	33.961255
896.017016	83077.846968	33.966272
897.115789	83219.370251	33.971290
897.951220	83359.376974	33.976308
898.877571	83511.977547	33.981325
899.689509	83658.552865	33.986343
900.454792	83801.664416	33.991360
901.234325	83952.845844	33.996378
902.192949	84105.888007	34.001396
903.212776	84253.536191	34.006413
904.430706	84398.151052	34.011431
905.203114	84555.875078	34.016448
906.041046	84707.304749	34.021466
907.298700	84850.800589	34.026484
907.492033	85012.571238	34.031501
908.711824	85159.115677	34.036519
909.844701	85300.985995	34.041536
910.937850	85455.648880	34.046554
912.721001	85586.660584	34.051572
914.267711	85723.843017	34.056589
915.450299	85864.871976	34.061607
916.481177	85991.859623	34.066624
917.058439	86128.296057	34.071642
917.987501	86250.726219	34.076660
918.866970	86391.475717	34.081677
919.528008	86525.569238	34.086695
920.355895	86666.252102	34.091712
921.495569	86805.429522	34.096730
922.304212	86945.901315	34.101748
923.008841	87089.634180	34.106765
924.056127	87218.740864	34.111783
925.227526	87350.870064	34.116800
926.302142	87483.420532	34.121818
927.463563	87618.758637	34.126836
928.417419	87751.937504	34.131853
929.256265	87893.587645	34.136871
929.951353	88020.750708	34.141888
930.296137	88159.323973	34.146906
931.259626	88299.942721	34.151924
932.309112	88449.267626	34.156941
933.231290	88602.833314	34.161959
933.946080	88742.251148	34.166976
934.682535	88893.845081	34.171994
935.635188	89035.102661	34.177012
936.792758	89184.287604	34.182029
937.850338	89322.222407	34.187047
938.984404	89469.828299	34.192064
939.371142	89617.894114	34.197082
940.589932	89762.573304	34.202100
941.634401	89920.321542	34.207117
941.966470	90066.737902	34.212135
943.268551	90207.071829	34.217152
944.178255	90367.200813	34.222170
945.321021	90506.952747	34.227188
946.387882	90660.417628	34.232205
946.880209	90814.188704	34.237223
948.179528	90953.233804	34.242240
948.845549	91094.799439	34.247258
950.095563	91248.580830	34.252276
950.693486	91386.951951	34.257293
951.634228	91528.109046	34.262311
952.753402	91670.823143	34.267328
953.555361	91814.195945	34.272346
954.806672	91952.543384	34.277364
955.482136	92104.530588	34.282381
956.361809	92240.516706	34.287399
957.098373	92380.467623	34.292416
957.749709	92525.223528	34.297434
958.830624	92680.851104	34.302452
959.859226	92834.409004	34.307469
960.962737	92990.909174	34.312487
962.034626	93132.788296	34.317504
962.412375	93296.793105	34.322522
963.855317	93440.554815	34.327540
964.684695	93598.900851	34.332557
965.273309	93763.737033	34.337575
966.338421	93919.652206	34.342592
967.165185	94091.855161	34.347610
968.409967	94246.032688	34.352628
969.143969	94413.156474	34.357645
969.350466	94591.809692	34.362663
970.290089	94760.791796	34.367680
971.404471	94934.843048	34.372698
972.450661	95109.742543	34.377716
973.401166	95279.372215	34.382733
974.535286	95461.320302	34.387751
975.579348	95636.641381	34.392768
976.627805	95815.664134	34.397786
977.788092	95984.909856	34.402804
978.825650	96156.064444	34.407821
979.705506	96334.520774	34.412839
980.796926	96499.533531	34.417856
981.852391	96672.779702	34.422874
983.413743	96852.006923	34.427892
984.348726	97015.791910	34.432909
985.345315	97186.337354	34.437927
986.769895	97345.242991	34.442944
987.647177	97520.752776	34.447962
989.193664	97660.524534	34.452980
990.280265	97834.000356	34.457997
991.652213	97981.191405	34.463015
992.224842	98129.129450	34.468032
993.655548	98291.385550	34.473050
994.729631	98446.485090	34.478068
995.830021	98590.298671	34.483085
997.206063	98734.982492	34.488103
998.247127	98873.101925	34.493120
998.835656	99029.738183	34.498138
1000.014641	99170.055814	34.503156
1001.149240	99315.667462	34.508173
1002.482907	99450.067127	34.513191
1004.002377	99584.729843	34.518208
1004.921267	99736.158083	34.523226
1005.452474	99871.914862	34.528244
1006.454324	100004.200919	34.533261
1007.137573	100152.650725	34.538279
1008.052821	100294.180875	34.543296
1008.738761	100448.019647	34.548314
1009.638022	100597.008162	34.553332
1010.863676	100743.981180	34.558349
1011.736763	100898.426672	34.563367
1012.487319	101045.297939	34.568384
1013.485727	101191.002711	34.573402
1014.415852	101346.747232	34.578420
1015.667673	101503.862085	34.583437
1016.234944	101660.095963	34.588455
1017.527522	101810.613206	34.593472
1018.171288	101971.831847	34.598490
1018.936316	102125.108263	34.603508
1020.057095	102271.914371	34.608525
1020.829945	102430.224343	34.613543
1021.726950	102575.241120	34.618560
1022.257702	102739.562104	34.623578
1023.479519	102902.989621	34.628596
1024.583812	103081.105723	34.633613
1025.180828	103241.184090	34.638631
1026.122860	103405.951129	34.643648
1027.331640	103583.026562	34.648666
1027.628581	103753.576508	34.653684
1028.973508	103937.732780	34.658701
1029.696853	104111.197383	34.663719
1030.689333	104290.909662	34.668736
1031.415234	104474.341645	34.673754
1032.655756	104653.864877	34.678772
1033.961185	104845.639954	34.683789
1034.540976	105035.069898	34.688807
1036.114829	105224.649579	34.693824
1037.304994	105413.694448	34.698842
1038.270479	105597.120376	34.703860
1039.317194	105778.657963	34.708877
1040.337627	105971.447699	34.713895
1041.742407	106157.483329	34.718912
1042.697622	106339.545429	34.723930
1043.676793	106535.692341	34.728948
1044.928535	106727.385001	34.733965
1046.008824	106915.466345	34.738983
1046.948340	107096.685348	34.744000
1048.194564	107289.992412	34.749018
1048.756734	107473.440822	34.754036
1049.992411	107663.327908	34.759053
1051.251337	107854.949638	34.764071
1052.675406	108042.615570	34.769088
1053.461212	108224.815606	34.774106
1054.379778	108414.439438	34.779124
1055.850974	108605.195146	34.784141
1056.934383	108795.353202	34.789159
1058.136899	108985.810672	34.794176
1059.253838	109178.248144	34.799194
1060.443166	109361.532238	34.804212
1061.795838	109527.684775	34.809229
1063.181906	109711.015980	34.814247
1064.925143	109874.889792	34.819264
1066.723439	110045.781234	34.824282
1067.025419	110211.150393	34.829300
1068.246102	110375.742416	34.834317
1069.101624	110539.631482	34.839335
1070.623931	110706.333686	34.844352
1071.611383	110871.598610	34.849370
1072.506770	111032.427425	34.854388
1073.794818	111194.108581	34.859405
1074.213025	111370.739060	34.864423
1075.456491	111538.084864	34.869440
1076.126110	111703.580951	34.874458
1076.985634	111890.544125	34.879476
1078.215656	112059.416315	34.884493
1078.825492	112249.350014	34.889511
1080.079211	112421.657065	34.894528
1081.080310	112608.817406	34.899546
1082.165879	112788.939467	34.904564
1083.776780	112980.609961	34.909581
1084.225245	113158.779054	34.914599
1085.449085	113340.974823	34.919616
1086.300335	113531.663777	34.924634
1087.075790	113712.916999	34.929652
1088.603060	113891.098339	34.934669
1089.704927	114081.345085	34.939687
1090.499026	114255.051808	34.944704
1091.746938	114430.527331	34.949722
1092.488839	114606.171694	34.954740
1093.856967	114777.634914	34.959757
1094.557471	114955.139150	34.964775
1096.144061	115137.096824	34.969792
1096.980181	115316.813805	34.974810
1097.795895	115497.308536	34.979828
1099.149237	115667.852324	34.984845
1100.341216	115864.029978	34.989863
1101.497931	116037.739054	34.994880
1102.004823	116222.306317	34.999898
1103.262731	116413.263607	35.004916
1104.330346	116605.025368	35.009933
1105.163337	116800.985109	35.014951
1106.630487	116998.520854	35.019968
1107.442803	117188.917667	35.024986
1108.200460	117389.166732	35.030004
1109.355205	117569.504234	35.035021
1110.707017	117772.566951	35.040039
1112.234351	117970.402784	35.045056
1113.501559	118172.618371	35.050074
1114.534618	118376.774331	35.055092
1116.171855	118564.588170	35.060109
1116.993768	118757.845339	35.065127
1118.328776	118960.181336	35.070144
1119.953974	119140.706330	35.075162
1120.842684	119324.861105	35.080180
1122.390817	119514.431346	35.085197
1123.063166	119703.264385	35.090215
1124.233041	119898.324790	35.095232
1125.422106	120087.319825	35.100250
1126.257462	120280.481064	35.105268
1127.589061	120471.256915	35.110285
1128.823356	120672.767780	35.115303
1129.308016	120873.115852	35.120320
1130.376748	121065.978071	35.125338
1131.023154	121277.047219	35.130356
1132.793366	121480.444565	35.135373
1133.850636	121697.134662	35.140391
1134.982857	121903.906905	35.145408
1135.701453	122109.311527	35.150426
1136.823672	122324.054027	35.155444
1138.089826	122533.041257	35.160461
1139.242522	122745.434431	35.165479
1140.392624	122963.461626	35.170496
1142.057392	123163.014993	35.175514
1143.184878	123372.903672	35.180532
1144.120879	123572.547807	35.185549
1145.413236	123791.686307	35.190567
1146.585351	123999.795244	35.195584
1148.151965	124189.892593	35.200602
1149.395949	124398.588590	35.205620
1150.956536	124590.020824	35.210637
1151.710515	124788.545039	35.215655
1152.892476	124986.952480	35.220672
1153.847934	125197.321626	35.225690
1155.139485	125406.586262	35.230708
1156.477068	125604.782056	35.235725
1157.364426	125806.664992	35.240743
1158.400549	126000.050908	35.245760
1160.219390	126198.047369	35.250778
1161.538377	126398.190992	35.255796
1162.871509	126586.433064	35.260813
1163.769801	126786.327260	35.265831
1164.842444	126978.684414	35.270848
1166.383567	127166.668202	35.275866
1168.063301	127347.970402	35.280884
1169.109714	127524.348414	35.285901
1169.777777	127698.439266	35.290919
1170.970600	127874.072665	35.295936
1172.020503	128047.813389	35.300954
1172.887849	128236.897099	35.305972
1173.914857	128414.233459	35.310989
1174.992476	128604.085214	35.316007
1175.607030	128800.379475	35.321024
1176.800970	128999.705103	35.326042
1178.151298	129196.431588	35.331060
1179.234457	129398.948361	35.336077
1179.963195	129607.713233	35.341095
1180.833035	129817.307127	35.346112
1182.544788	130014.539084	35.351130
1183.094553	130220.277180	35.356148
1184.574468	130432.341558	35.361165
1185.865282	130640.947356	35.366183
1186.600884	130856.289686	35.371200
1187.753395	131074.003968	35.376218
1188.768428	131297.869321	35.381236
1190.067420	131514.306744	35.386253
1191.578256	131739.606676	35.391271
1192.614881	131967.722727	35.396288
1194.152834	132178.466973	35.401306
1195.067892	132414.522052	35.406324
1196.134762	132630.011634	35.411341
1197.922409	132856.695121	35.416359
1198.637450	133079.233487	35.421376
1200.129278	133302.196993	35.426394
1201.143511	133535.996620	35.431412
1202.559355	133770.089900	35.436429
1203.648369	133994.807584	35.441447
1204.383882	134232.461227	35.446464
1206.260853	134444.381359	35.451482
1207.263048	134688.543308	35.456500
1208.646425	134914.856444	35.461517
1210.062474	135145.213524	35.466535
1210.887751	135374.446071	35.471552
1212.250294	135601.121211	35.476570
1213.019691	135849.500732	35.481588
1214.674345	136078.391273	35.486605
1216.165346	136309.745010	35.491623
1217.531380	136549.773923	35.496640
1219.203960	136772.624785	35.501658
1220.399356	136995.056520	35.506676
1221.606741	137211.193218	35.511693
1223.249596	137430.232227	35.516711
1224.170294	137655.755752	35.521728
1226.088670	137873.611614	35.526746
1226.988040	138096.577200	35.531764
1228.501277	138316.846245	35.536781
1229.886874	138529.572863	35.541799
1230.853147	138751.490485	35.546816
1232.199080	138961.712569	35.551834
1233.612172	139172.508839	35.556852
1234.601393	139393.385264	35.561869
1236.254605	139600.998591	35.566887
1237.479407	139816.992289	35.571904
1238.276981	140033.815288	35.576922
1239.570807	140248.822947	35.581940
1240.677232	140456.424065	35.586957
1241.633207	140676.651708	35.591975
1242.850735	140905.976915	35.596992
1243.829949	141116.380114	35.602010
1245.352036	141347.677614	35.607028
1246.318834	141560.102566	35.612045
1247.748158	141779.169687	35.617063
1248.730456	142013.626123	35.622080
1249.848857	142211.612905	35.627098
1251.183019	142431.015125	35.632116
1252.621751	142645.135013	35.637133
1254.043827	142846.909627	35.642151
1254.718400	143067.268260	35.647168
1255.763440	143279.320345	35.652186
1256.942450	143497.964710	35.657204
1258.275230	143718.083584	35.662221
1259.935653	143948.343621	35.667239
1260.832055	144178.038958	35.672256
1261.663086	144409.623975	35.677274
1262.953835	144636.733991	35.682292
1263.553604	144877.051328	35.687309
1264.855539	145115.863761	35.692327
1266.153562	145362.521655	35.697344
1267.241813	145613.275075	35.702362
1268.652752	145862.126144	35.707380
1269.861266	146104.257805	35.712397
1271.223738	146347.940356	35.717415
1272.461814	146608.562525	35.722432
1273.716196	146859.435626	35.727450
1275.437950	147102.659328	35.732468
1277.325538	147333.622540	35.737485
1278.975543	147578.611271	35.742503
1279.882085	147818.399278	35.747520
1281.453508	148057.678130	35.752538
1283.160652	148301.823562	35.757556
1284.270084	148549.655772	35.762573
1286.010508	148784.621260	35.767591
1286.578508	149023.566519	35.772608
1287.909722	149251.578888	35.777626
1289.063096	149505.983664	35.782644
1290.290728	149761.888507	35.787661
1291.861489	150004.831831	35.792679
1292.184642	150251.614514	35.797696
1293.681454	150501.108681	35.802714
1294.996190	150764.772951	35.807732
1295.764360	151023.713223	35.812749
1297.550239	151280.070943	35.817767
1298.649157	151550.843068	35.822784
1299.457590	151814.642399	35.827802
1301.173792	152085.422059	35.832820
1302.261652	152342.147834	35.837837
1303.858802	152613.139098	35.842855
1304.978053	152892.470206	35.847872
1305.982650	153161.449682	35.852890
1307.390669	153446.945677	35.857908
1308.679825	153714.994656	35.862925
1310.396178	153983.930086	35.867943
1311.358035	154265.171319	35.872960
1312.540252	154541.530226	35.877978
1313.763530	154825.018242	35.882996
1315.060676	155103.481800	35.888013
1317.015983	155373.579583	35.893031
1318.316759	155651.727834	35.898048
1319.923383	155920.448247	35.903066
1322.220123	156177.293948	35.908084
1323.328072	156440.242573	35.913101
1324.961806	156688.460342	35.918119
1325.983184	156956.883540	35.923136
1327.553372	157215.408926	35.928154
1328.562910	157468.310484	35.933172
1330.068425	157732.065821	35.938189
1331.810323	157996.889775	35.943207
1332.731186	158260.777019	35.948224
1334.265683	158507.164351	35.953242
1335.540196	158757.046459	35.958260
1336.371634	159011.848513	35.963277
1338.066691	159260.968605	35.968295
1339.501751	159508.429228	35.973312
1340.725010	159744.485465	35.978330
1341.867795	159984.998589	35.983348
1343.112945	160246.291793	35.988365
1344.312389	160477.428685	35.993383
1345.437639	160738.831573	35.998400
1346.618100	160981.665905	36.003418
1347.982051	161245.153687	36.008436
1348.905166	161509.028957	36.013453
1350.162417	161774.681205	36.018471
1351.925328	162031.507976	36.023488
1353.872875	162282.581031	36.028506
1354.920643	162543.419412	36.033524
1356.324785	162805.993190	36.038541
1357.838062	163058.584560	36.043559
1358.841043	163330.999179	36.048576
1360.497901	163607.794308	36.053594
1361.738778	163867.122281	36.058612
1362.729958	164132.571845	36.063629
1364.262922	164407.561444	36.068647
1365.663161	164679.817841	36.073664
1366.972850	164965.458811	36.078682
1368.137634	165255.897531	36.083700
1369.297186	165536.117631	36.088717
1370.822997	165806.987678	36.093735
1372.026329	166094.554512	36.098752
1373.270630	166373.939490	36.103770
1375.054646	166670.089639	36.108788
1375.665716	166972.747633	36.113805
1377.107111	167253.870141	36.118823
1378.661308	167556.509996	36.123840
1380.147431	167853.016494	36.128858
1381.475385	168145.473260	36.133876
1382.600709	168443.879753	36.138893
1384.198694	168739.686785	36.143911
1385.484750	169052.608795	36.148928
1386.499274	169357.905557	36.153946
1388.344204	169660.153252	36.158964
1389.213666	169963.646845	36.163981
1390.562488	170274.888216	36.168999
1392.049179	170584.699903	36.174016
1393.328622	170904.931827	36.179034
1394.708439	171218.940329	36.184052
1396.199400	171529.771049	36.189069
1397.953211	171847.558281	36.194087
1399.181067	172167.117948	36.199104
1400.471370	172473.501644	36.204122
1402.051404	172796.056246	36.209140
1403.383268	173116.835244	36.214157
1405.264182	173421.225558	36.219175
1406.715143	173742.801137	36.224192
1407.898593	174051.239405	36.229210
1409.819672	174361.226851	36.234228
1410.932811	174675.760884	36.239245
1412.853157	174980.811288	36.244263
1414.000769	175303.646931	36.249280
1415.116231	175617.473153	36.254298
1416.829431	175923.270602	36.259316
1418.103506	176235.639448	36.264333
1419.648927	176542.773368	36.269351
1421.074542	176849.292248	36.274368
1422.646029	177169.046587	36.279386
1423.783487	177475.663634	36.284404
1425.603020	177782.048037	36.289421
1427.669523	178092.306041	36.294439
1429.131516	178394.786628	36.299456
1430.410405	178682.617263	36.304474
1431.922950	178973.332976	36.309492
1433.534309	179264.872299	36.314509
1434.709927	179543.197845	36.319527
1435.799044	179821.563195	36.324544
1437.025334	180115.044994	36.329562
1438.198098	180414.225239	36.334580
1439.151359	180712.424906	36.339597
1440.805872	181008.382353	36.344615
1442.094060	181319.205168	36.349632
1443.266728	181622.961016	36.354650
1444.950660	181934.790665	36.359668
1446.086228	182248.510459	36.364685
1447.798479	182567.169914	36.369703
1449.163284	182878.443054	36.374720
1449.791066	183201.769892	36.379738
1451.328356	183520.993259	36.384756
1452.410482	183858.855399	36.389773
1454.113932	184189.636767	36.394791
1455.607026	184530.891119	36.399808
1456.546792	184861.895842	36.404826
1458.078296	185197.126878	36.409844
1460.033209	185536.763002	36.414861
1461.367704	185876.065568	36.419879
1463.182846	186305.487127	36.424896
1464.771511	186646.454178	36.429914
1466.307987	186975.340322	36.434932
1468.170171	187316.825507	36.439949
1469.646418	187655.349620	36.444967
1471.632843	187987.444996	36.449984
1472.908936	188324.656328	36.455002
1474.527782	188655.922262	36.460020
1475.704282	188998.205812	36.465037
1477.413921	189326.995720	36.470055
1478.934311	189661.963037	36.475072
1480.265586	190003.691990	36.480090
1481.639440	190340.106626	36.485108
1483.212280	190679.843935	36.490125
1484.600066	191020.805006	36.495143
1486.155976	191361.232729	36.500160
1487.607050	191710.720431	36.505178
1489.127729	192052.628848	36.510196
1491.026205	192405.731608	36.515213
1492.417242	192736.435087	36.520231
1493.957571	193078.394055	36.525248
1495.282600	193426.814080	36.530266
1496.818399	193768.394594	36.535284
1498.413850	194116.266138	36.540301
1499.818866	194457.538714	36.545319
1501.311052	194805.301235	36.550336
1502.589413	195162.598198	36.555354
1504.201484	195500.208642	36.560372
1505.961074	195842.292876	36.565389
1508.162703	196191.878404	36.570407
1509.587147	196518.623470	36.575424
1511.088288	196868.066293	36.580442
1512.624179	197194.211226	36.585460
1514.391240	197536.628597	36.590477
1515.229452	197872.917907	36.595495
1517.169301	198213.328463	36.600512
1518.438300	198562.405213	36.605530
1520.587982	198885.866794	36.610548
1522.456627	199219.051190	36.615565
1524.315444	199541.721393	36.620583
1525.790692	199879.337904	36.625600
1527.427875	200195.210957	36.630618
1528.726494	200529.223965	36.635636
1529.784157	200853.165272	36.640653
1531.043071	201188.506736	36.645671
1532.913130	201492.330530	36.650688
1533.810839	201815.562044	36.655706
1535.650698	202126.326528	36.660724
1536.936419	202451.302060	36.665741
1538.695021	202770.996657	36.670759
1539.929515	203092.729842	36.675776
1541.059371	203415.724694	36.680794
1542.320731	203745.050184	36.685812
1544.056654	204094.674931	36.690829
1545.307942	204426.924482	36.695847
1546.697548	204755.774379	36.700864
1547.991764	205104.504755	36.705882
1549.242975	205458.119813	36.710900
1550.508554	205812.800151	36.715917
1551.795421	206168.087428	36.720935
1553.676577	206532.605184	36.725952
1555.082314	206904.005971	36.730970
1556.429916	207265.229842	36.735988
1558.202145	207644.830497	36.741005
1559.552992	208025.513850	36.746023
1561.115341	208392.421582	36.751040
1562.323625	208779.860296	36.756058
1563.687341	209165.522464	36.761076
1565.561600	209554.026697	36.766093
1567.024911	209946.025280	36.771111
1568.514318	210322.117833	36.776128
1570.373263	210721.066961	36.781146
1571.879588	211093.169576	36.786164
1573.922519	211490.287344	36.791181
1576.037765	211870.170734	36.796199
1578.064293	212241.482081	36.801216
1579.738078	212631.927170	36.806234
1581.464501	213019.443077	36.811252
1582.981475	213395.052499	36.816269
1585.006152	213768.067911	36.821287
1586.572211	214140.113940	36.826304
1588.026614	214514.464156	36.831322
1589.730785	214890.528511	36.836340
1591.591801	215272.843412	36.841357
1592.911473	215657.707562	36.846375
1594.630147	216017.385237	36.851392
1596.045010	216395.401518	36.856410
1597.636645	216769.173405	36.861428
1599.438391	217148.450745	36.866445
1600.962190	217535.342235	36.871463
1602.500889	217909.732948	36.876480
1604.349266	218301.629569	36.881498
1605.386854	218674.905226	36.886516
1607.258594	219053.385396	36.891533
1608.890008	219430.709408	36.896551
1610.565608	219809.500141	36.901568
1612.241871	220200.815138	36.906586
1614.235315	220584.738925	36.911604
1615.711420	220956.321275	36.916621
1617.102557	221352.355755	36.921639
1618.603238	221726.652782	36.926656
1620.614854	222105.036234	36.931674
1622.459515	222487.917041	36.936692
1624.282274	222867.143190	36.941709
1625.376610	223241.173972	36.946727
1627.511442	223621.570834	36.951744
1628.617650	224012.061731	36.956762
1630.305066	224393.087609	36.961780
1631.800173	224770.993508	36.966797
1633.246673	225155.893157	36.971815
1634.913685	225533.340307	36.976832
1636.313481	225931.381173	36.981850
1637.775071	226315.541713	36.986868
1639.522659	226694.297197	36.991885
1640.797139	227070.992730	36.996903
1642.604065	227430.025255	37.001920
1643.985229	227817.957961	37.006938
1645.097928	228209.514560	37.011956
1646.964792	228580.909226	37.016973
1648.024542	228973.896510	37.021991
1650.044163	229368.486316	37.027008
1651.581240	229761.271586	37.032026
1653.464028	230161.852424	37.037044
1655.491981	230546.812297	37.042061
1657.289002	230936.330028	37.047079
1658.722779	231323.795867	37.052096
1660.466836	231719.113557	37.057114
1661.824128	232119.242065	37.062132
1664.015053	232514.463908	37.067149
1665.263314	232919.359462	37.072167
1667.053287	233325.338513	37.077184
1669.230876	233720.155090	37.082202
1670.840556	234122.274913	37.087220
1672.293913	234505.797847	37.092237
1673.429171	234925.189588	37.097255
1675.705885	235323.621996	37.102272
1676.996531	235743.699898	37.107290
1678.328630	236165.549122	37.112308
1680.001199	236580.714227	37.117325
1681.589148	237007.069709	37.122343
1683.881396	237419.139226	37.127360
1685.604246	237847.885895	37.132378
1686.990769	238268.580895	37.137396
1688.610192	238686.977971	37.142413
1690.138800	239112.095208	37.147431
1692.400150	239539.104036	37.152448
1693.320210	239979.252470	37.157466
1695.036007	240410.638532	37.162484
1696.974288	240838.127782	37.167501
1698.674648	241281.886272	37.172519
1700.534894	241718.226626	37.177536
1701.805757	242152.346756	37.182554
1703.577377	242607.040509	37.187572
1705.147895	243043.220589	37.192589
1706.667608	243506.741482	37.197607
1708.597718	243952.999360	37.202624
1710.434432	244402.497118	37.207642
1712.368487	244852.613771	37.212660
1713.977188	245289.062833	37.217677
1715.346646	245745.235561	37.222695
1717.397170	246192.358907	37.227712
1719.124675	246649.210196	37.232730
1720.751747	247109.530865	37.237748
1722.676916	247560.811253	37.242765
1724.350532	248013.222201	37.247783
1726.376885	248464.840142	37.252800
1728.177543	248916.847877	37.257818
1730.115478	249357.884562	37.262836
1732.843521	249802.632194	37.267853
1734.031578	250253.385916	37.272871
1736.137904	250687.864377	37.277888
1737.942962	251129.120342	37.282906
1739.178791	251569.524281	37.287924
1741.064685	252011.196946	37.292941
1742.665950	252463.073592	37.297959
1744.439283	252903.110156	37.302976
1746.023511	253347.645691	37.307994
1747.763865	253797.108742	37.313012
1749.600014	254240.382832	37.318029
1751.049241	254681.074331	37.323047
1753.129438	255118.973155	37.328064
1755.434144	255528.767074	37.333082
1757.097608	255956.771125	37.338100
1759.048771	256359.911921	37.343117
1760.996152	256785.785972	37.348135
1762.650462	257188.996062	37.353152
1764.359799	257592.374077	37.358170
1765.753483	258016.501818	37.363188
1767.776757	258426.432224	37.368205
1769.758344	258853.233779	37.373223
1771.281773	259266.440064	37.378240
1773.377421	259696.395857	37.383258
1774.881681	260116.028504	37.388276
1776.035462	260547.373197	37.393293
1777.306399	260977.351745	37.398311
1778.884245	261424.908271	37.403328
1780.535945	261863.942493	37.408346
1782.204840	262315.291213	37.413364
1784.165393	262756.407158	37.418381
1785.444539	263225.415126	37.423399
1787.434935	263680.822617	37.428416
1789.416576	264145.576506	37.433434
1791.205376	264621.356402	37.438452
1792.906180	265077.387339	37.443469
1794.392611	265541.247304	37.448487
1796.017501	266013.465130	37.453504
1797.918387	266488.228222	37.458522
1799.625025	266972.493147	37.463540
1801.493941	267441.262560	37.468557
1803.306309	267941.481817	37.473575
1805.110522	268412.237706	37.478592
1806.993030	268905.811964	37.483610
1809.038297	269383.382783	37.488628
1811.156493	269869.448026	37.493645
1812.776835	270352.820236	37.498663
1814.825895	270844.123038	37.503680
1816.755901	271333.257591	37.508698
1818.190881	271815.736608	37.513716
1819.730774	272311.885655	37.518733
1821.524130	272808.601736	37.523751
1823.259591	273301.412879	37.528768
1825.098876	273799.716019	37.533786
1826.784051	274331.792425	37.538804
1828.777896	274822.344722	37.543821
1830.227599	275338.273965	37.548839
1832.638553	275850.163921	37.553856
1834.667336	276359.596231	37.558874
1835.778295	276868.381643	37.563892
1837.564145	277381.324649	37.568909
1839.446404	277900.775852	37.573927
1841.355814	278427.355412	37.578944
1843.234594	278942.178206	37.583962
1844.748660	279461.498706	37.588980
1846.845830	279978.845170	37.593997
1848.966297	280511.471959	37.599015
1850.918893	281034.039590	37.604032
1853.050404	281550.734819	37.609050
1855.207658	282070.037929	37.614068
1857.593945	282574.903118	37.619085
1859.513927	283079.456789	37.624103
1861.736634	283599.449533	37.629120
1863.940007	284090.289893	37.634138
1865.542803	284601.154382	37.639156
1867.316301	285102.694544	37.644173
1869.364919	285597.077993	37.649191
1870.971421	286104.096343	37.654208
1873.033162	286599.993936	37.659226
1874.797566	287101.723783	37.664244
1876.707162	287597.612328	37.669261
1878.695664	288068.905481	37.674279
1880.469317	288541.015976	37.679296
1882.040031	289012.596158	37.684314
1883.972908	289499.274789	37.689332
1886.043278	289979.529628	37.694349
1887.702636	290464.618608	37.699367
1889.340041	290943.486547	37.704384
1890.977401	291422.046118	37.709402
1893.185306	291915.823048	37.714420
1894.813748	292402.780563	37.719437
1896.906906	292899.995144	37.724455
1898.569887	293389.732206	37.729472
1900.817227	293882.242840	37.734490
1902.208742	294392.173382	37.739508
1904.218247	294883.468836	37.744525
1905.823815	295385.258178	37.749543
1907.637167	295896.175964	37.754560
1909.646336	296412.923305	37.759578
1911.691631	296917.143987	37.764596
1914.108666	297415.716700	37.769613
1916.436931	297923.666962	37.774631
1918.363553	298415.427501	37.779648
1920.733582	298914.349688	37.784666
1922.749557	299416.496154	37.789684
1924.746154	299914.198385	37.794701
1926.420577	300417.937717	37.799719
1928.426881	300929.617132	37.804736
1930.586275	301428.397006	37.809754
1932.361998	301938.122785	37.814772
1934.238764	302445.187772	37.819789
1936.418341	302956.084471	37.824807
1937.980725	303458.797231	37.829824
1939.918560	303972.311114	37.834842
1941.879269	304486.400176	37.839860
1943.658006	304998.126452	37.844877
1946.033342	305521.304015	37.849895
1947.269407	306037.115458	37.854912
1949.434329	306553.867793	37.859930
1951.205703	307087.835484	37.864948
1953.190879	307615.113655	37.869965
1955.228344	308150.322829	37.874983
1956.867002	308678.633786	37.880000
1959.118950	309205.853173	37.885018
1961.026491	309734.592877	37.890036
1962.942609	310254.873364	37.895053
1965.588926	310793.790784	37.900071
1967.286052	311330.820140	37.905088
1969.530569	311867.554717	37.910106
1971.108066	312390.859738	37.915124
1973.101563	312929.220424	37.920141
1975.333462	313462.360076	37.925159
1977.338697	314001.137940	37.930176
1979.108335	314531.393519	37.935194
1980.900437	315067.806530	37.940212
1983.022947	315606.648623	37.945229
1985.395370	316133.720351	37.950247
1987.168424	316679.380313	37.955264
1989.263633	317215.441140	37.960282
1990.886704	317763.928198	37.965300
1992.510268	318305.404253	37.970317
1994.369941	318845.415572	37.975335
1996.138959	319398.477927	37.980352
1998.642521	319946.596810	37.985370
2000.302530	320501.007039	37.990388
2002.869760	321053.441103	37.995405
2004.995758	321594.949550	38.000423
2006.799028	322130.792204	38.005440
2009.663716	322649.257985	38.010458
2012.197578	323162.262879	38.015476
2014.457784	323668.808526	38.020493
2016.630097	324164.704782	38.025511
2018.558444	324662.231763	38.030528
2020.352056	325159.266326	38.035546
2022.619234	325653.810327	38.040564
2024.597235	326160.343967	38.045581
2026.305279	326660.748065	38.050599
2027.775439	327167.018666	38.055616
2029.205563	327682.854171	38.060634
2031.446415	328209.085170	38.065652
2033.094507	328727.410109	38.070669
2035.296423	329250.690300	38.075687
2036.604759	329786.509301	38.080704
2038.360770	330329.709609	38.085722
2040.312883	330881.903137	38.090740
2041.975201	331430.810756	38.095757
2043.922658	331985.044071	38.100775
2046.196121	332563.724112	38.105792
2048.120241	333118.857830	38.110810
2050.153604	333700.931988	38.115828
2052.067191	334272.031896	38.120845
2054.550104	334839.710956	38.125863
2057.012690	335393.585218	38.130880
2059.689033	335948.483111	38.135898
2062.263584	336507.523153	38.140916
2064.562564	337068.982100	38.145933
2066.719534	337611.557808	38.150951
2068.841574	338173.839037	38.155968
2070.915398	338730.894049	38.160986
2073.123509	339291.673225	38.166004
2075.247108	339847.536343	38.171021
2077.254441	340405.716975	38.176039
2079.088295	340976.318178	38.181056
2081.142885	341530.542437	38.186074
2083.139146	342100.186927	38.191092
2085.019709	342672.731386	38.196109
2087.651334	343242.612805	38.201127
2088.893192	343807.934487	38.206144
2091.263686	344373.831088	38.211162
2093.361045	344966.616799	38.216180
2095.151002	345544.858791	38.221197
2097.066998	346134.254352	38.226215
2099.053255	346729.486350	38.231232
2101.385866	347299.574761	38.236250
2103.564533	347894.502332	38.241268
2105.893302	348492.311791	38.246285
2107.849793	349078.022952	38.251303
2109.831663	349668.435912	38.256320
2111.999062	350273.997126	38.261338
2114.135959	350861.828688	38.266356
2115.775245	351457.004191	38.271373
2118.182754	352063.052194	38.276391
2120.065494	352668.410238	38.281408
2121.896762	353284.108931	38.286426
2123.879332	353883.850575	38.291444
2126.249813	354497.514541	38.296461
2128.871363	355100.073944	38.301479
2130.807875	355713.300360	38.306496
2132.894214	356323.930858	38.311514
2135.046706	356933.930587	38.316532
2137.129765	357546.033153	38.321549
2139.439199	358149.672196	38.326567
2141.570489	358771.071254	38.331584
2143.419999	359379.346038	38.336602
2145.783957	359997.946008	38.341620
2148.147955	360611.337135	38.346637
2150.924681	361201.256262	38.351655
2152.856753	361794.438806	38.356672
2155.174035	362356.830398	38.361690
2157.705534	362933.396426	38.366708
2159.394820	363516.064282	38.371725
2161.855201	364091.224820	38.376743
2163.790612	364658.929125	38.381760
2166.004675	365228.859667	38.386778
2168.178196	365806.312125	38.391796
2170.106820	366393.801500	38.396813
2172.652431	366972.895662	38.401831
2174.449384	367565.728753	38.406848
2176.155872	368143.790143	38.411866
2178.236988	368736.554422	38.416884
2180.164829	369337.971042	38.421901
2182.803040	369927.050324	38.426919
2184.864474	370533.361593	38.431936
2187.432702	371125.695277	38.436954
2189.811566	371734.768624	38.441972
2191.857243	372335.519581	38.446989
2193.874164	372923.669861	38.452007
2196.501832	373544.648403	38.457024
2198.676886	374152.737436	38.462042
2200.885281	374753.105996	38.467060
2202.608119	375375.248461	38.472077
2204.661488	375986.051555	38.477095
2206.584346	376611.908906	38.482112
2208.610473	377243.511244	38.487130
2211.150345	377873.346395	38.492148
2212.986241	378519.083301	38.497165
2215.502265	379143.901828	38.502183
2217.693622	379777.925726	38.507200
2219.578202	380429.535421	38.512218
2221.875127	381068.248145	38.517236
2224.056265	381725.478017	38.522253
2226.572909	382370.177741	38.527271
2228.866134	383018.214111	38.532288
2231.041625	383669.595602	38.537306
2233.621560	384318.744605	38.542324
2235.515469	384971.124668	38.547341
2237.704654	385617.819852	38.552359
2240.178450	386276.710502	38.557376
2242.551979	386938.663653	38.562394
2245.343090	387580.833453	38.567412
2247.307774	388257.426524	38.572429
2249.359138	388912.338441	38.577447
2251.277738	389578.090797	38.582464
2253.771554	390249.330790	38.587482
2255.840439	390910.086363	38.592500
2257.658920	391592.535452	38.597517
2259.928989	392274.742893	38.602535
2262.134331	392947.827336	38.607552
2264.048864	393627.216859	38.612570
2266.563203	394301.987296	38.617588
2268.855284	395001.075329	38.622605
2270.734088	395694.891682	38.627623
2272.812556	396388.909693	38.632640
2275.141068	397092.436248	38.637658
2277.560275	397776.690962	38.642676
2279.754835	398490.878085	38.647693
2282.578397	399172.497733	38.652711
2284.742539	399873.992345	38.657728
2287.289755	400570.293533	38.662746
2289.830868	401264.145163	38.667764
2291.645257	401963.353381	38.672781
2294.369454	402661.233875	38.677799
2296.874537	403349.359460	38.682816
2298.966244	404048.764103	38.687834
2301.346019	404730.237635	38.692852
2303.765402	405397.565305	38.697869
2306.074374	406060.437233	38.702887
2308.261725	406721.335046	38.707904
2310.795597	407386.966223	38.712922
2313.144269	408044.308031	38.717940
2314.813574	408715.246405	38.722957
2317.351966	409375.504260	38.727975
2319.643876	410045.140999	38.732992
2322.059306	410728.701855	38.738010
2324.186609	411394.832022	38.743028
2326.712656	412079.193257	38.748045
2329.336134	412740.398381	38.753063
2331.329873	413417.262736	38.758080
2333.686243	414100.524068	38.763098
2336.195428	414774.685100	38.768116
2338.500749	415466.560695	38.773133
2340.448851	416143.902296	38.778151
2343.186771	416857.515920	38.783168
2345.665272	417552.583964	38.788186
2348.255461	418242.806835	38.793204
2350.040001	418946.686933	38.798221
2352.166250	419652.057604	38.803239
2354.630069	420360.284667	38.808256
2356.955294	421063.148863	38.813274
2359.401311	421772.442876	38.818292
2361.195463	422492.028677	38.823309
2362.943544	423211.899807	38.828327
2365.302553	423945.402902	38.833344
2367.772867	424677.446446	38.838362
2370.734487	425399.730018	38.843380
2373.361031	426136.802705	38.848397
2375.423644	426876.413774	38.853415
2377.942891	427618.403212	38.858432
2380.122422	428363.602924	38.863450
2383.038463	429095.971670	38.868468
2385.020098	429857.321986	38.873485
2387.643661	430594.735693	38.878503
2390.130622	431342.706688	38.883520
2392.529448	432104.005859	38.888538
2394.875137	432841.580624	38.893556
2397.406484	433596.382230	38.898573
2399.763359	434337.739249	38.903591
2402.456619	435097.510500	38.908608
2404.747359	435855.950343	38.913626
2406.950439	436600.730874	38.918644
2409.192032	437356.996643	38.923661
2411.553033	438120.792518	38.928679
2413.976653	438889.499131	38.933696
2416.352161	439657.373633	38.938714
2418.672175	440412.292489	38.943732
2421.530867	441194.780235	38.948749
2423.485243	441956.968464	38.953767
2426.227697	442723.194811	38.958784
2428.594784	443495.256985	38.963802
2430.836339	444278.216475	38.968820
2433.464670	445058.708344	38.973837
2435.582749	445831.166053	38.978855
2438.179972	446613.313665	38.983872
2440.515026	447396.882692	38.988890
2443.370879	448170.186276	38.993908
2445.681947	448956.771947	38.998925
2448.981879	449712.922776	39.003943
2451.815131	450479.667509	39.008960
2454.823568	451236.153069	39.013978
2457.238873	452006.280408	39.018996
2459.478250	452755.349524	39.024013
2461.770409	453513.415167	39.029031
2465.178066	454251.636657	39.034048
2467.356134	454991.685265	39.039066
2470.028998	455695.534325	39.044084
2472.211215	456416.138916	39.049101
2474.318188	457129.406917	39.054119
2477.032238	457847.395832	39.059136
2478.884156	458582.497671	39.064154
2481.140564	459296.359524	39.069172
2483.732013	460024.673031	39.074189
2485.593216	460759.579405	39.079207
2488.367867	461507.683154	39.084224
2490.687960	462240.183256	39.089242
2493.385378	462978.950113	39.094260
2495.468756	463724.339668	39.099277
2497.529834	464476.207943	39.104295
2500.469397	465238.448964	39.109312
2503.317120	465994.464751	39.114330
2506.037165	466748.246731	39.119348
2507.900852	467510.804507	39.124365
2510.251999	468290.198659	39.129383
2512.834495	469056.406247	39.134400
2515.228289	469834.812933	39.139418
2517.764011	470613.160535	39.144436
2520.584717	471390.821401	39.149453
2523.245234	472173.109591	39.154471
2526.102393	472947.463083	39.159488
2528.489611	473735.063829	39.164506
2531.389535	474511.705652	39.169524
2533.662078	475310.138207	39.174541
2536.145332	476093.323111	39.179559
2538.747074	476884.315547	39.184576
2541.253211	477683.500581	39.189594
2543.347561	478483.667592	39.194612
2546.388960	479279.865692	39.199629
2548.772364	480082.628500	39.204647
2551.639196	480870.608347	39.209664
2554.184524	481680.320233	39.214682
2556.447464	482487.313045	39.219700
2558.985741	483293.918670	39.224717
2561.702012	484109.121604	39.229735
2564.043393	484924.340264	39.234752
2566.147008	485747.362630	39.239770
2568.809888	486579.322192	39.244788
2572.050636	487400.415552	39.249805
2574.459043	488238.974733	39.254823
2577.139935	489050.797650	39.259840
2579.279665	489901.749413	39.264858
2582.186045	490718.434451	39.269876
2584.516398	491561.506298	39.274893
2586.830018	492409.468997	39.279911
2589.660365	493244.813793	39.284928
2592.031094	494100.225656	39.289946
2595.047883	494935.245184	39.294964
2597.736567	495768.607465	39.299981
2600.130668	496623.517796	39.304999
2602.888108	497462.765133	39.310016
2605.879109	498296.793117	39.315034
2608.291317	499132.223303	39.320052
2611.136993	499980.172348	39.325069
2613.877900	500818.122360	39.330087
2615.963274	501657.233782	39.335104
2618.764216	502508.967841	39.340122
2621.254560	503356.925816	39.345140
2623.789405	504205.380348	39.350157
2626.360820	505076.271351	39.355175
2628.994277	505919.526608	39.360192
2631.529162	506777.690180	39.365210
2633.979450	507634.959828	39.370228
2636.132724	508469.032667	39.375245
2639.043376	509315.614231	39.380263
2641.790142	510134.957833	39.385280
2644.394454	510975.350523	39.390298
2646.810487	511799.929610	39.395316
2649.198336	512627.984714	39.400333
2651.864077	513463.842303	39.405351
2654.619746	514307.479915	39.410368
2657.059002	515152.774772	39.415386
2659.144768	515995.709865	39.420404
2662.417435	516842.379379	39.425421
2664.767223	517701.859908	39.430439
2667.465389	518568.018223	39.435456
2670.019382	519439.522433	39.440474
2672.452130	520300.032124	39.445492
2675.095399	521177.241009	39.450509
2677.790041	522046.444125	39.455527
2680.593048	522926.529328	39.460544
2683.127916	523818.457677	39.465562
2685.759735	524703.276668	39.470580
2688.226874	525589.268402	39.475597
2691.185642	526499.490565	39.480615
2693.845209	527395.077943	39.485632
2697.064923	528291.672215	39.490650
2699.529150	529194.250558	39.495668
2702.343125	530096.561317	39.500685
2705.272859	531014.109591	39.505703
2707.957930	531916.465173	39.510720
2710.748818	532839.179296	39.515738
2713.400068	533747.689554	39.520756
2717.075955	534658.586395	39.525773
2719.213409	535567.349806	39.530791
2722.315160	536460.235041	39.535808
2725.481701	537380.004106	39.540826
2727.843474	538295.515853	39.545844
2731.049839	539200.992083	39.550861
2734.083504	540118.425273	39.555879
2736.746216	541023.002747	39.560896
2739.484307	541930.664715	39.565914
2741.891064	542834.800449	39.570932
2745.444894	543738.239856	39.575949
2748.426454	544644.863905	39.580967
2751.362737	545537.031393	39.585984
2754.500353	546441.894415	39.591002
2756.970758	547350.356711	39.596020
2759.850985	548255.026635	39.601037
2762.489697	549156.307571	39.606055
2765.135176	550057.170069	39.611072
2767.415143	550966.296894	39.616090
2770.252091	551876.221365	39.621108
2773.059009	552793.301849	39.626125
2775.435347	553721.910498	39.631143
2778.306449	554628.965591	39.636160
2781.102914	555552.454846	39.641178
2783.469443	556473.985513	39.646196
2787.085949	557404.120310	39.651213
2789.494917	558333.920330	39.656231
2792.237562	559257.682604	39.661248
2795.276834	560177.418297	39.666266
2798.366018	561110.401417	39.671284
2800.955120	562038.278953	39.676301
2803.161281	562965.692236	39.681319
2806.105353	563907.642843	39.686336
2809.197102	564824.602150	39.691354
2811.280068	565760.527515	39.696372
2814.142710	566697.908047	39.701389
2816.559122	567644.045184	39.706407
2819.598814	568582.947600	39.711424
2822.303543	569530.537020	39.716442
2825.120203	570452.499804	39.721460
2827.913969	571357.773078	39.726477
2830.300055	572270.245838	39.731495
2832.959679	573185.855791	39.736512
2835.741700	574114.884712	39.741530
2838.478089	575043.143895	39.746548
2840.760736	575971.597780	39.751565
2843.428389	576911.472232	39.756583
2846.306309	577856.788123	39.761600
2849.640853	578813.758252	39.766618
2852.189384	579770.519050	39.771636
2854.723960	580717.896918	39.776653
2857.526967	581678.704741	39.781671
2860.337845	582651.679350	39.786688
2862.954929	583626.398432	39.791706
2865.678521	584610.713892	39.796724
2868.460143	585597.281514	39.801741
2870.889544	586601.660926	39.806759
2873.861386	587604.363399	39.811776
2877.202953	588608.364859	39.816794
2880.647386	589611.057733	39.821812
2884.034410	590599.175211	39.826829
2886.856107	591599.232032	39.831847
2890.168926	592608.211660	39.836864
2892.906026	593603.798024	39.841882
2895.794776	594617.849558	39.846900
2898.586555	595627.723992	39.851917
2901.455641	596631.746905	39.856935
2904.409156	597649.593639	39.861952
2907.560236	598668.010261	39.866970
2910.198144	599698.241161	39.871988
2913.461126	600713.046816	39.877005
2915.975692	601744.094052	39.882023
2918.760880	602774.797305	39.887040
2922.016085	603804.626101	39.892058
2924.938285	604837.149197	39.897076
2928.044010	605876.625782	39.902093
2931.173574	606903.321054	39.907111
2934.178057	607930.731402	39.912128
2937.163664	608977.745076	39.917146
2939.578607	610014.864905	39.922164
2942.630638	611055.320348	39.927181
2945.552274	612097.534560	39.932199
2948.697880	613151.074584	39.937216
2951.977064	614203.685972	39.942234
2954.663202	615251.095379	39.947252
2957.776077	616293.044976	39.952269
2960.458559	617355.786766	39.957287
2963.464284	618418.314893	39.962304
2966.703156	619472.122188	39.967322
2969.264978	620528.613833	39.972340
2972.544549	621580.396544	39.977357
2975.753923	622642.240048	39.982375
2978.916842	623704.922407	39.987392
2982.199353	624759.900652	39.992410
2985.091197	625813.531274	39.997428
2988.476568	626863.086909	40.002445
2991.681989	627906.483181	40.007463
2994.184294	628961.028115	40.012480
2997.567757	630011.288218	40.017498
3000.124170	631061.314209	40.022516
3003.349794	632122.168693	40.027533
3006.546229	633167.584077	40.032551
3009.567507	634218.086841	40.037568
3012.807138	635270.429500	40.042586
3015.933528	636327.548067	40.047604
3018.982125	637365.511057	40.052621
3021.833405	638395.433537	40.057639
3024.600051	639413.769572	40.062656
3027.530617	640426.251498	40.067674
3030.546283	641439.157510	40.072692
3033.418657	642447.303197	40.077709
3036.164278	643460.230732	40.082727
3038.658928	644474.925955	40.087744
3041.729053	645495.035576	40.092762
3044.538729	646526.303056	40.097780
3047.633261	647566.552367	40.102797
3050.864209	648601.197981	40.107815
3054.573787	649621.892639	40.112832
3058.008799	650645.446552	40.117850
3060.815083	651690.139531	40.122868
3063.766544	652723.020684	40.127885
3066.752555	653759.998994	40.132903
3069.477903	654805.884722	40.137920
3072.442070	655855.433955	40.142938
3075.424295	656922.924111	40.147956
3078.176725	657978.462360	40.152973
3080.929150	659054.121296	40.157991
3083.833404	660150.812213	40.163008
3087.194306	661226.312100	40.168026
3089.877744	662334.078677	40.173044
3092.847323	663428.369999	40.178061
3096.241207	664529.649760	40.183079
3099.238607	665626.837309	40.188096
3102.396188	666727.531297	40.193114
3105.904171	667850.785189	40.198132
3109.094889	668969.879682	40.203149
3112.328913	670087.782664	40.208167
3115.201947	671210.602735	40.213184
3118.931435	672327.445369	40.218202
3121.620857	673453.024850	40.223220
3125.051522	674569.821495	40.228237
3128.497178	675698.554738	40.233255
3131.694372	676837.775025	40.238272
3134.686950	677963.308533	40.243290
3138.132194	679090.652053	40.248308
3141.459488	680208.558132	40.253325
3144.777369	681330.623807	40.258343
3148.138034	682475.198393	40.263360
3151.261373	683588.778761	40.268378
3154.339339	684720.968785	40.273396
3157.594756	685855.302713	40.278413
3161.013787	686977.685283	40.283431
3163.930060	688113.248451	40.288448
3167.666147	689246.896229	40.293466
3170.411879	690374.660104	40.298484
3173.490353	691501.327970	40.303501
3176.777609	692635.420499	40.308519
3179.930724	693778.470344	40.313536
3183.275958	694904.826682	40.318554
3186.721013	696044.993664	40.323572
3189.979952	697179.645486	40.328589
3193.126229	698320.330196	40.333607
3196.142725	699468.183314	40.338624
3199.367051	700603.644364	40.343642
3202.458613	701756.591281	40.348660
3205.449251	702897.294254	40.353677
3208.284889	704050.296721	40.358695
3211.473629	705198.191834	40.363712
3214.713658	706345.518635	40.368730
3217.657946	707500.126095	40.373748
3220.536628	708651.073131	40.378765
3224.142837	709814.463363	40.383783
3227.306768	710990.818825	40.388800
3230.490058	712164.283179	40.393818
3233.594372	713312.934725	40.398836
3236.559973	714449.116131	40.403853
3239.769687	715571.836134	40.408871
3242.584339	716714.018630	40.413888
3246.296710	717837.613254	40.418906
3248.995636	718972.828887	40.423924
3252.312738	720114.676402	40.428941
3255.437845	721267.859057	40.433959
3258.357601	722414.646761	40.438976
3261.520282	723556.498067	40.443994
3264.851202	724721.731202	40.449012
3267.847673	725874.828811	40.454029
3271.423289	727043.949286	40.459047
3274.665890	728223.322910	40.464064
3278.118028	729392.295941	40.469082
3281.417054	730566.226755	40.474100
3285.106078	731748.666920	40.479117
3288.474839	732918.431366	40.484135
3291.495637	734115.205560	40.489152
3294.697037	735292.391431	40.494170
3297.762672	736501.653284	40.499188
3300.967551	737717.428044	40.504205
3304.325934	738917.305336	40.509223
3306.989821	740142.836747	40.514240
3310.522389	741364.000268	40.519258
3313.671133	742593.221080	40.524276
3316.901267	743822.713197	40.529293
3320.255098	745067.196594	40.534311
3323.738043	746314.980429	40.539328
3326.952192	747560.284730	40.544346
3330.268286	748821.402768	40.549364
3333.244470	750077.594500	40.554381
3336.636031	751344.880737	40.559399
3340.049714	752625.572194	40.564416
3343.088335	753896.678605	40.569434
3346.533958	755175.632090	40.574452
3349.671038	756459.206659	40.579469
3353.481092	757751.166019	40.584487
3356.916963	759046.573007	40.589504
3360.522276	760332.652622	40.594522
3363.875857	761622.992826	40.599540
3367.291233	762914.505530	40.604557
3371.077075	764206.015045	40.609575
3374.032692	765517.924644	40.614592
3377.538207	766811.734802	40.619610
3380.954435	768109.084710	40.624628
3384.168448	769414.441228	40.629645
3387.976044	770721.609466	40.634663
3391.270106	772031.005176	40.639680
3394.319695	773337.890459	40.644698
3398.024388	774653.466679	40.649716
3400.750111	775963.320822	40.654733
3404.847159	777280.721698	40.659751
3408.118114	778613.482536	40.664768
3411.229269	779930.374077	40.669786
3414.833735	781256.258547	40.674804
3418.255264	782587.280481	40.679821
3421.459170	783898.642067	40.684839
3424.946353	785238.986335	40.689856
3428.258246	786570.889742	40.694874
3431.985792	787905.924610	40.699892
3435.118771	789240.246276	40.704909
3438.599939	790563.563156	40.709927
3441.963172	791908.427279	40.714944
3445.522625	793237.629000	40.719962
3449.281034	794569.258729	40.724980
3452.476996	795906.454358	40.729997
3456.290000	797226.860224	40.735015
3459.754326	798556.795656	40.740020
3463.206445	799829.317526	40.745024
3466.817797	801045.768424	40.750029
3469.933897	802216.091745	40.755034
3472.962939	803320.241481	40.760039
3476.027874	804362.330447	40.765044
3478.946218	805347.148947	40.770048
3481.769466	806259.985121	40.775053
3484.456661	807132.039003	40.780058
3487.173067	807923.023947	40.785063
3489.220885	808663.795776	40.790068
3491.692789	809348.546058	40.795072
3494.059692	809966.212651	40.800077
3495.995342	810532.804800	40.805082
3498.186160	811042.867734	40.810087
3499.874758	811511.738669	40.815092
3501.549784	811922.976737	40.820096
3503.360885	812285.048571	40.825101
3504.541808	812616.988085	40.830106
3506.027417	812894.779363	40.835111
3507.580504	813149.551182	40.840116
3508.095720	813372.027464	40.845120
3509.432144	813546.038799	40.850125
3510.497236	813671.662566	40.855130
3511.320269	813792.644845	40.860135
3512.191543	813882.731380	40.865140
3513.126854	813935.685444	40.870144
3513.693809	813972.523183	40.875149
3514.138514	813991.550097	40.880154
3514.741401	813974.892749	40.885159
3515.317670	813955.511455	40.890164
3516.152383	813906.275700	40.895168
3516.357906	813840.574390	40.900173
3516.633883	813766.871814	40.905178
3517.183155	813673.833506	40.910183
3517.597492	813566.491707	40.915188
3517.373249	813450.088664	40.920192
3518.285830	813312.458566	40.925197
3518.431860	813171.632219	40.930202
3518.435657	813023.224215	40.935207
3518.455933	812869.840295	40.940212
3518.546586	812696.366876	40.945216
3518.787795	812522.572771	40.950221
3518.477510	812351.783743	40.955226
3518.589528	812159.190797	40.960231
3518.794104	811991.332711	40.965236
3518.894470	811797.560977	40.970240
3519.078854	811591.391779	40.975245
3518.970625	811394.228871	40.980250
3518.905279	811177.753276	40.985255
3518.822031	810977.844156	40.990260
3518.795747	810763.687676	40.995264
3518.977968	810553.975575	41.000269
3518.742373	810330.868622	41.005274
3519.015673	810102.507232	41.010279
3518.703596	809893.337900	41.015284
3518.462912	809669.915900	41.020288
3518.874954	809450.868993	41.025293
3518.637152	809223.433233	41.030298
3518.734938	809001.592273	41.035303
3518.562104	808770.132249	41.040308
3518.512601	808549.078542	41.045312
3518.492996	808318.943276	41.050317
3518.218045	808094.983424	41.055322
3518.108433	807862.992763	41.060327
3517.795280	807640.241881	41.065332
3517.796607	807409.338865	41.070336
3517.917164	807173.434497	41.075341
3517.577568	806952.858179	41.080346
3517.598603	806712.270371	41.085351
3517.391833	806491.852374	41.090356
3517.092343	806264.515214	41.095360
3517.316700	806046.599460	41.100365
3516.976182	805824.374519	41.105370
3517.173947	805607.179561	41.110375
3516.451992	805383.633032	41.115380
3516.540446	805172.586825	41.120384
3516.540311	804954.229764	41.125389
3516.187409	804728.797545	41.130394
3516.072083	804517.859113	41.135399
3515.784635	804311.038960	41.140404
3515.698010	804096.910807	41.145408
3515.508659	803886.255842	41.150413
3515.341221	803686.862052	41.155418
3515.332962	803474.262224	41.160423
3515.157863	803260.461473	41.165428
3515.129976	803062.636747	41.170432
3515.138595	802855.625656	41.175437
3514.716505	802653.165029	41.180442
3514.422618	802461.854052	41.185447
3514.303032	802271.681448	41.190452
3514.347091	802069.861614	41.195456
3514.106992	801877.646286	41.200461
3513.767235	801686.270548	41.205466
3513.897007	801500.136127	41.210471
3513.092995	801316.582914	41.215476
3513.439155	801134.846030	41.220480
3513.369375	800948.238689	41.225485
3513.124411	800776.249512	41.230490
3513.188899	800602.645190	41.235495
3513.127603	800416.558107	41.240500
3512.464734	800241.886096	41.245504
3512.767544	800062.908518	41.250509
3512.709489	799904.439357	41.255514
3512.422207	799741.022039	41.260519
3512.146238	799561.974563	41.265524
3511.566612	799400.937967	41.270528
3511.952114	799240.185934	41.275533
3511.765943	799082.644355	41.280538
3511.240189	798924.907862	41.285543
3511.458708	798773.741131	41.290548
3511.443333	798619.970449	41.295552
3511.382491	798466.203219	41.300557
3511.065724	798310.177082	41.305562
3510.974753	798161.583859	41.310567
3510.992838	798014.337628	41.315572
3510.570215	797862.810301	41.320576
3510.897342	797720.002225	41.325581
3510.302002	797569.422986	41.330586
3510.307431	797434.375758	41.335591
3510.025462	797304.059562	41.340596
3510.219934	797159.892284	41.345600
3510.149360	797018.596248	41.350605
3509.702377	796888.688259	41.355610
3509.685159	796759.589732	41.360615
3509.816943	796616.641361	41.365620
3509.539041	796494.807828	41.370624
3509.621959	796369.154162	41.375629
3509.205320	796248.510093	41.380634
3509.285694	796113.081701	41.385639
3509.192301	795988.571830	41.390644
3509.028438	795867.734619	41.395648
3509.267231	795738.966623	41.400653
3508.566802	795629.836264	41.405658
3508.484041	795509.419415	41.410663
3508.695784	795387.537441	41.415668
3508.768345	795277.352044	41.420672
3508.788127	795151.196139	41.425677
3508.438357	795050.698155	41.430682
3508.367181	794932.467518	41.435687
3507.979504	794822.102062	41.440692
3508.192692	794722.683690	41.445696
3508.283384	794610.334240	41.450701
3507.685948	794494.572218	41.455706
3507.807366	794390.716508	41.460711
3507.489297	794291.521207	41.465716
3507.571090	794199.591823	41.470720
3507.623113	794089.389559	41.475725
3507.106083	793996.426981	41.480730
3507.338482	793890.933337	41.485735
3507.151185	793808.227779	41.490740
3507.094365	793717.241786	41.495744
3507.100010	793620.233689	41.500749
3507.030017	793540.731862	41.505754
3507.200236	793445.063830	41.510759
3507.272358	793348.872136	41.515764
3507.095114	793260.048996	41.520768
3506.881052	793162.677469	41.525773
3506.893438	793078.416368	41.530778
3507.127555	792985.224226	41.535783
3506.765320	792900.921650	41.540788
3506.669983	792818.775708	41.545792
3506.953619	792720.097880	41.550797
3506.629731	792637.789886	41.555802
3506.834236	792554.860593	41.560807
3506.174705	792474.998065	41.565812
3506.090088	792398.515145	41.570816
3506.362872	792306.675935	41.575821
3506.067245	792229.050894	41.580826
3506.329683	792144.787572	41.585831
3506.091742	792059.330451	41.590836
3505.870924	791989.463140	41.595840
3505.922806	791906.647271	41.600845
3505.531283	791839.835815	41.605850
3505.702621	791769.904862	41.610855
3505.734129	791701.608222	41.615860
3505.290604	791635.633856	41.620864
3505.449496	791561.742916	41.625869
3505.550690	791500.081764	41.630874
3505.364897	791430.985209	41.635879
3505.447725	791363.214782	41.640884
3505.474449	791294.865771	41.645888
3505.572701	791234.718112	41.650893
3505.185236	791168.534730	41.655898
3505.322926	791095.081855	41.660903
3505.520951	791035.601228	41.665908
3504.860783	790977.134241	41.670912
3505.255707	790911.168193	41.675917
3504.796620	790844.846071	41.680922
3504.987148	790790.742434	41.685927
3504.905671	790737.707603	41.690932
3504.505592	790675.774831	41.695936
3504.894540	790610.393411	41.700941
3504.518390	790561.803592	41.705946
3504.914304	790505.220833	41.710951
3504.863340	790450.614317	41.715956
3504.925657	790388.019821	41.720960
3504.680337	790334.811776	41.725965
3504.418254	790275.787363	41.730970
3504.494158	790217.491919	41.735975
3504.309874	790164.615227	41.740980
3504.217041	790116.809065	41.745984
3504.575069	790066.927300	41.750989
3504.269253	790020.180568	41.755994
3504.123358	789963.091081	41.760999
3503.993978	789921.059146	41.766004
3504.126432	789875.563124	41.771008
3504.185397	789835.408239	41.776013
3503.919155	789786.453216	41.781018
3503.842469	789740.451064	41.786023
3504.066692	789684.523790	41.791028
3504.161544	789647.785141	41.796032
3504.443279	789600.112276	41.801037
3504.095646	789559.187960	41.806042
3503.827112	789506.074644	41.811047
3503.876245	789457.605790	41.816052
3504.145144	789420.740866	41.821056
3503.964305	789362.722503	41.826061
3503.869211	789323.811141	41.831066
3503.719121	789287.353285	41.836071
3503.960991	789242.471528	41.841076
3503.598575	789199.640066	41.846080
3504.007872	789158.252610	41.851085
3503.709074	789106.216684	41.856090
3503.832363	789078.175348	41.861095
3503.956454	789035.413480	41.866100
3503.630390	788988.075730	41.871104
3503.675270	788941.119802	41.876109
3503.526111	788902.801271	41.881114
3503.832139	788860.743416	41.886119
3503.853669	788823.767111	41.891124
3503.206437	788787.530925	41.896128
3503.436320	788753.504951	41.901133
3503.645578	788721.389399	41.906138
3503.526823	788684.336429	41.911143
3503.724894	788642.245152	41.916148
3503.022153	788602.495279	41.921152
3503.517091	788560.308166	41.926157
3503.478696	788540.017308	41.931162
3503.251782	788505.083296	41.936167
3503.657674	788465.257109	41.941172
3503.066809	788437.813781	41.946176
3503.153137	788387.521619	41.951181
3503.517749	788373.427658	41.956186
3503.403281	788326.052080	41.961191
3503.188065	788286.957742	41.966196
3503.169052	788252.381175	41.971200
3503.466617	788214.135546	41.976205
3503.068068	788178.003865	41.981210
3503.080009	788147.090233	41.986215
3503.180735	788119.586380	41.991220
3503.217125	788091.358795	41.996224
3502.833303	788066.865166	42.001229
3502.613801	788045.084832	42.006234
3502.829886	788019.421184	42.011239
3502.800877	787989.100161	42.016244
3502.754473	787967.341424	42.021248
3502.726684	787928.460227	42.026253
3502.880103	787903.979837	42.031258
3502.660938	787883.275003	42.036263
3502.842415	787863.877048	42.041268
3502.773762	787828.914720	42.046272
3502.588358	787794.019372	42.051277
3502.469857	787775.695242	42.056282
3502.884220	787758.266046	42.061287
3502.971290	787725.724535	42.066292
3502.671141	787700.874068	42.071296
3502.934132	787673.196250	42.076301
3502.617897	787650.793845	42.081306
3502.759598	787622.645628	42.086311
3502.713308	787589.292736	42.091316
3502.368271	787565.916238	42.096320
3502.661849	787542.635491	42.101325
3502.619833	787523.467139	42.106330
3502.544032	787497.553604	42.111335
3502.635538	787474.499870	42.116340
3502.372256	787457.224730	42.121344
3502.441755	787441.462852	42.126349
3502.444239	787427.716991	42.131354
3502.555689	787417.231483	42.136359
3502.360755	787371.671561	42.141364
3502.550594	787357.407097	42.146368
3502.347367	787342.421372	42.151373
3502.425405	787322.695583	42.156378
3502.191886	787302.724933	42.161383
3502.197901	787279.292544	42.166388
3502.315823	787272.474619	42.171392
3502.242526	787252.919032	42.176397
3502.498898	787235.855588	42.181402
3502.060772	787218.558239	42.186407
3502.188963	787206.064138	42.191412
3501.810879	787187.583284	42.196416
3502.284900	787160.995462	42.201421
3502.097589	787157.894022	42.206426
3502.310819	787129.194423	42.211431
3502.366115	787112.113174	42.216436
3502.328707	787095.095293	42.221440
3502.298323	787076.266261	42.226445
3502.436536	787059.465431	42.231450
3502.156019	787039.941608	42.236455
3502.360545	787020.782181	42.241460
3502.131006	787008.588227	42.246464
3502.560626	786976.380844	42.251469
3502.042927	786974.847481	42.256474
3502.076160	786953.806760	42.261479
3502.311457	786935.180397	42.266484
3502.245748	786919.683015	42.271488
3502.536375	786906.673754	42.276493
3502.267443	786873.596664	42.281498
3502.500045	786868.228016	42.286503
3502.513358	786848.559855	42.291508
3502.180068	786841.909864	42.296512
3502.494635	786803.751279	42.301517
3502.374712	786783.027486	42.306522
3502.088463	786763.601586	42.311527
3502.362643	786752.013317	42.316532
3501.904879	786732.027077	42.321536
3502.407084	786709.395699	42.326541
3502.031333	786697.615402	42.331546
3502.072047	786690.466495	42.336551
3502.183405	786678.414330	42.341556
3502.149553	786658.655135	42.346560
3502.197644	786639.372294	42.351565
3501.962135	786626.004431	42.356570
3501.913063	786617.450729	42.361575
3502.511786	786594.999563	42.366580
3502.204595	786584.235723	42.371584
3502.455055	786563.257653	42.376589
3502.267630	786544.647352	42.381594
3502.202045	786521.908401	42.386599
3502.337268	786505.840486	42.391604
3502.326803	786486.517432	42.396608
3502.587221	786465.733191	42.401613
3502.416084	786449.517335	42.406618
3502.417832	786431.121763	42.411623
3502.568981	786410.305505	42.416628
3502.010952	786412.496537	42.421632
3502.343995	786376.729890	42.426637
3502.100910	786362.775586	42.431642
3501.973200	786346.259143	42.436647
3502.098232	786327.844012	42.441652
3502.087986	786315.076327	42.446656
3502.042759	786290.963509	42.451661
3502.156912	786285.563984	42.456666
3501.759919	786264.686182	42.461671
3502.194284	786257.083871	42.466676
3502.211186	786245.975266	42.471680
3501.903452	786231.052286	42.476685
3501.792345	786224.171237	42.481690
3502.178817	786209.188613	42.486695
3501.931121	786187.846901	42.491700
3501.997437	786186.319902	42.496704
3501.939093	786156.092927	42.501709
3501.780293	786153.671519	42.506714
3501.890058	786152.675907	42.511719
3502.052503	786131.123120	42.516724
3501.791747	786128.032675	42.521728
3501.940308	786117.637166	42.526733
3501.802502	786092.461721	42.531738
3501.715340	786092.768971	42.536743
3501.897311	786071.506496	42.541748
3501.767629	786063.307167	42.546752
3501.554400	786041.225694	42.551757
3501.469380	786046.865628	42.556762
3501.440941	786041.634976	42.561767
3501.777474	786027.736140	42.566772
3501.671211	786024.279007	42.571776
3501.837956	786015.984354	42.576781
3501.823359	786011.045075	42.581786
3501.951320	785988.518676	42.586791
3502.099556	785967.407924	42.591796
3501.762199	785970.641002	42.596800
3502.087741	785947.251812	42.601805
3502.252373	785938.810611	42.606810
3501.955499	785923.151326	42.611815
3501.956358	785909.157933	42.616820
3501.885959	785908.288304	42.621824
3501.941417	785880.390816	42.626829
3501.955275	785884.987943	42.631834
3501.994019	785865.166109	42.636839
3501.876380	785851.240046	42.641844
3501.749335	785845.633228	42.646848
3502.023588	785833.896565	42.651853
3501.944057	785812.820928	42.656858
3501.716863	785810.801513	42.661863
3501.567701	785782.984531	42.666868
3501.842024	785771.981679	42.671872
3501.956953	785766.777327	42.676877
3501.869634	785756.907416	42.681882
3501.816595	785744.047465	42.686887
3501.801768	785742.190547	42.691892
3501.436692	785734.419040	42.696896
3501.505289	785713.466718	42.701901
3501.594555	785712.376387	42.706906
3501.409454	785716.221865	42.711911
3501.718516	785716.173617	42.716916
3501.375193	785704.239692	42.721920
3501.976200	785687.705553	42.726925
3501.697109	785677.571926	42.731930
3501.283392	785681.404232	42.736935
3501.705847	785675.760301	42.741940
3501.185256	785662.532915	42.746944
3501.631995	785651.160404	42.751949
3501.505290	785645.749082	42.756954
3501.563928	785651.709402	42.761959
3501.820835	785641.443002	42.766964
3501.245279	785628.860227	42.771968
3501.600452	785611.777172	42.776973
3501.763720	785617.427586	42.781978
3501.462971	785619.138282	42.786983
3501.606034	785597.880376	42.791988
3501.295702	785596.901422	42.796993
3501.783637	785597.559164	42.801997
3501.380074	785594.197211	42.807002
3501.326212	785600.468743	42.812007
3501.782496	785589.241425	42.817012
3501.515018	785571.619509	42.822017
3501.673140	785556.964698	42.827021
3501.640001	785555.012729	42.832026
3501.538756	785547.640132	42.837031
3501.511956	785526.017107	42.842036
3501.430908	785528.084926	42.847041
3501.336301	785518.802967	42.852045
3501.819990	785531.449373	42.857050
3501.774791	785513.401111	42.862055
3501.738708	785499.853008	42.867060
3501.577298	785493.908748	42.872065
3501.366807	785487.336055	42.877069
3501.635897	785485.923992	42.882074
3501.453986	785467.652322	42.887079
3502.025246	785456.406808	42.892084
3501.610083	785470.123532	42.897089
3501.631612	785455.881299	42.902093
3501.667861	785441.049560	42.907098
3501.488025	785426.496223	42.912103
3501.727911	785421.418862	42.917108
3501.255367	785432.746997	42.922113
3501.654906	785410.861226	42.927117
3501.431322	785398.125128	42.932122
3501.352917	785394.907969	42.937127
3501.308954	785384.003164	42.942132
3501.588876	785395.898777	42.947137
3501.898257	785388.217156	42.952141
3501.858399	785370.852714	42.957146
3501.676885	785370.147178	42.962151
3501.867178	785364.588210	42.967156
3501.549054	785342.471878	42.972161
3501.648984	785341.037296	42.977165
3501.522233	785334.842816	42.982170
3501.633124	785337.712534	42.987175
3502.117027	785312.339081	42.992180
3501.571293	785300.436069	42.997185
3501.815246	785305.584815	43.002189
3501.806308	785287.579204	43.007194
3501.942316	785269.942345	43.012199
3501.683404	785267.536261	43.017204
3501.565909	785254.196113	43.022209
3501.786755	785235.616182	43.027213
3502.118640	785231.013623	43.032218
3501.750732	785227.156580	43.037223
3501.853042	785206.099525	43.042228
3501.684437	785208.425794	43.047233
3501.689947	785204.363565	43.052237
3501.602621	785190.137780	43.057242
3501.682704	785182.932164	43.062247
3501.786459	785178.218431	43.067252
3501.569248	785182.460700	43.072257
3501.893543	785148.450409	43.077261
3501.473157	785142.888852	43.082266
3501.220585	785147.038804	43.087271
3501.483135	785147.340360	43.092276
3501.136102	785147.198941	43.097281
3501.283229	785150.160942	43.102285
3501.293664	785121.386508	43.107290
3501.298363	785119.819965	43.112295
3501.165188	785110.739199	43.117300
3501.168266	785114.164137	43.122305
3501.190070	785110.735441	43.127309
3500.961613	785115.615647	43.132314
3500.953486	785121.342212	43.137319
3501.477534	785122.336895	43.142324
3501.319988	785122.655190	43.147329
3501.532973	785121.545423	43.152333
3501.482466	785107.117970	43.157338
3501.358597	785096.910256	43.162343
3501.383646	785089.615275	43.167348
3501.742034	785089.706118	43.172353
3501.678995	785081.984495	43.177357
3501.697433	785069.552470	43.182362
3501.424826	785066.561246	43.187367
3501.595967	785058.215780	43.192372
3501.255966	785067.615386	43.197377
3501.177859	785069.046746	43.202381
3501.533139	785062.238386	43.207386
3501.083691	785041.364930	43.212391
3501.348782	785037.457757	43.217396
3501.299935	785040.695113	43.222401
3501.478284	785033.669712	43.227405
3501.578081	785035.122203	43.232410
3501.152398	785043.654421	43.237415
3501.506657	785037.139800	43.242420
3501.266134	785027.684229	43.247425
3501.266897	785006.887088	43.252429
3501.254144	785002.631854	43.257434
3500.781358	785007.452464	43.262439
3501.192668	785007.486101	43.267444
3501.189676	785016.930966	43.272449
3501.167078	785014.879322	43.277453
3501.561329	785017.558080	43.282458
3500.907998	785020.645268	43.287463
3501.319940	785020.287332	43.292468
3501.363184	785018.567937	43.297473
3501.669928	785008.292773	43.302477
3501.672934	784991.752525	43.307482
3501.615583	784989.265896	43.312487
3501.913859	784989.806548	43.317492
3501.846780	784977.926000	43.322497
3501.280626	784964.900080	43.327501
3501.324628	784961.663576	43.332506
3501.370541	784960.726704	43.337511
3501.358964	784960.239232	43.342516
3501.310746	784963.965874	43.347521
3501.296044	784954.866375	43.352525
3501.654034	784931.272808	43.357530
3501.311653	784934.066752	43.362535
3501.221374	784930.117200	43.367540
3501.332048	784932.546712	43.372545
3501.200979	784925.373826	43.377549
3501.368583	784927.598701	43.382554
3501.255312	784921.548533	43.387559
3501.744269	784901.800255	43.392564
3501.461356	784901.061583	43.397569
3501.537288	784906.530516	43.402573
3501.567761	784910.244887	43.407578
3501.321174	784891.932809	43.412583
3501.684231	784877.440209	43.417588
3501.414502	784884.431255	43.422593
3501.230189	784878.832571	43.427597
3501.227804	784881.818064	43.432602
3501.240472	784886.171391	43.437607
3501.616821	784882.687154	43.442612
3501.646083	784866.093555	43.447617
3501.473086	784854.474021	43.452621
3501.377420	784849.057196	43.457626
3501.563624	784852.551513	43.462631
3501.689951	784851.650992	43.467636
3501.589543	784828.618075	43.472641
3501.494538	784821.879861	43.477645
3501.405820	784822.676767	43.482650
3501.563298	784818.052253	43.487655
3501.713590	784805.941675	43.492660
3501.707442	784795.470416	43.497665
3501.508187	784784.784648	43.502669
3501.772393	784790.517861	43.507674
3501.490840	784776.566233	43.512679
3501.316340	784764.457415	43.517684
3501.142746	784769.769722	43.522689
3501.607501	784766.075861	43.527693
3501.511606	784763.741981	43.532698
3501.545832	784770.440950	43.537703
3501.461560	784757.975463	43.542708
3501.568909	784753.065123	43.547713
3501.700271	784743.844630	43.552717
3501.662932	784741.550525	43.557722
3501.579814	784732.020989	43.562727
3501.815337	784705.069153	43.567732
3501.338931	784710.135224	43.572737
3501.312125	784703.386229	43.577741
3501.850167	784709.615009	43.582746
3501.612476	784696.243594	43.587751
3501.591389	784679.804211	43.592756
3501.590427	784679.070375	43.597761
3501.463517	784676.692376	43.602765
3501.803241	784666.900900	43.607770
3501.417365	784649.148233	43.612775
3501.633448	784644.465501	43.617780
3501.556998	784644.330706	43.622785
3501.555569	784638.409607	43.627789
3501.546652	784615.116964	43.632794
3501.497169	784606.511799	43.637799
3501.589874	784608.161242	43.642804
3501.324591	784608.007028	43.647809
3501.528333	784610.519985	43.652813
3501.530272	784587.372360	43.657818
3501.190766	784587.914872	43.662823
3501.412332	784584.503615	43.667828
3501.542527	784581.987515	43.672833
3501.551001	784584.237382	43.677837
3501.319515	784574.192500	43.682842
3501.509709	784562.711432	43.687847
3501.474655	784547.105845	43.692852
3501.909811	784554.525361	43.697857
3501.615701	784560.443927	43.702861
3501.583858	784530.547982	43.707866
3501.475647	784522.245516	43.712871
3501.756330	784518.629233	43.717876
3501.378408	784517.318112	43.722881
3501.423089	784514.472788	43.727885
3501.777483	784498.072137	43.732890
3501.864543	784489.151847	43.737895
3501.978663	784479.444302	43.742900
3501.298603	784473.041883	43.747905
3501.734826	784461.717934	43.752909
3501.687053	784456.684810	43.757914
3501.804455	784452.653570	43.762919
3501.387464	784435.932904	43.767924
3501.692846	784419.637600	43.772929
3501.477637	784408.513272	43.777933
3501.657073	784415.923980	43.782938
3501.429818	784417.525610	43.787943
3501.466733	784387.373581	43.792948
3501.344467	784383.575520	43.797953
3501.292859	784378.347181	43.802957
3501.414378	784383.564722	43.807962
3501.202400	784385.212911	43.812967
3501.610362	784364.839502	43.817972
3501.361743	784376.819565	43.822977
3501.659468	784355.729275	43.827981
3501.692811	784351.955810	43.832986
3501.336080	784353.724513	43.837991
3501.828151	784352.228420	43.842996
3501.215141	784341.117225	43.848001
3501.089177	784326.357300	43.853005
3501.097411	784315.100008	43.858010
3501.168699	784328.106818	43.863015
3501.461687	784313.868647	43.868020
3501.418894	784321.607836	43.873025
3501.124990	784324.492332	43.878029
3501.287605	784335.820911	43.883034
3501.452441	784331.341728	43.888039
3501.628590	784308.606356	43.893044
3501.239942	784305.143529	43.898049
3501.491187	784301.825369	43.903053
3501.465221	784310.883309	43.908058
3501.220011	784314.298531	43.913063
3501.811219	784306.865251	43.918068
3501.495927	784300.943978	43.923073
3501.586975	784291.044007	43.928077
3501.979819	784293.038128	43.933082
3501.485731	784285.382962	43.938087
3501.626968	784252.913851	43.943092
3501.923334	784251.154691	43.948097
3501.609466	784253.748697	43.953101
3501.723033	784242.523757	43.958106
3501.464766	784217.849443	43.963111
3501.072034	784202.445783	43.968116
3501.480832	784204.877899	43.973121
3501.556320	784192.875783	43.978125
3501.576385	784199.920122	43.983130
3501.707716	784192.509665	43.988135
3501.535369	784176.092685	43.993140
3501.413095	784181.054853	43.998145
3501.462527	784187.066865	44.003149
3501.783835	784166.021231	44.008154
3501.275753	784147.013870	44.013159
3501.585575	784144.567408	44.018164
3501.376828	784145.872564	44.023169
3501.541848	784150.643022	44.028173
3501.478331	784147.373990	44.033178
3501.517568	784132.685693	44.038183
3501.722838	784116.405299	44.043188
3501.487396	784118.644511	44.048193
3501.745221	784122.274841	44.053197
3501.611614	784099.195650	44.058202
3501.518256	784087.415503	44.063207
3501.531123	784090.496849	44.068212
3501.519216	784081.053131	44.073217
3501.530748	784077.185038	44.078221
3501.563127	784058.729175	44.083226
3501.263383	784045.317209	44.088231
3501.250855	784045.857589	44.093236
3501.282975	784050.648895	44.098241
3501.346641	784056.169386	44.103245
3501.387049	784059.246441	44.108250
3501.315903	784063.368701	44.113255
3501.532147	784041.751803	44.118260
3501.393855	784030.663760	44.123265
3501.405839	784023.271772	44.128269
3501.452982	784018.125596	44.133274
3501.237354	784027.947693	44.138279
3501.459741	784019.397153	44.143284
3501.548202	784019.040798	44.148289
3501.105458	783998.750316	44.153293
3501.263057	783987.762773	44.158298
3501.115554	783997.721091	44.163303
3501.081177	783995.622033	44.168308
3501.081484	783993.223900	44.173313
3500.898076	783998.929888	44.178317
3501.294301	783999.406374	44.183322
3501.108722	784007.706608	44.188327
3501.166886	784010.242551	44.193332
3501.269772	784016.882604	44.198337
3501.208347	784012.927995	44.203341
3501.403110	784013.289148	44.208346
3501.298962	783996.861065	44.213351
3501.048427	783982.951863	44.218356
3501.441428	783988.127277	44.223361
3501.463858	783979.950537	44.228365
3501.547936	783976.119987	44.233370
3501.422973	783979.467640	44.238375
3501.861117	783980.035459	44.243380
3501.892418	783957.615187	44.248385
3501.387583	783953.093610	44.253389
3501.813193	783948.132928	44.258394
3501.281259	783929.618095	44.263399
3501.469252	783915.542316	44.268404
3501.584189	783914.692394	44.273409
3501.783842	783919.261834	44.278413
3501.335561	783917.912647	44.283418
3501.300175	783900.347902	44.288423
3501.410656	783883.053964	44.293428
3501.354434	783890.551039	44.298433
3501.405855	783890.836722	44.303437
3501.815347	783883.137726	44.308442
3501.448206	783889.117242	44.313447
3501.443040	783869.687872	44.318452
3501.076278	783859.173629	44.323457
3501.078679	783855.208949	44.328461
3501.132533	783848.005993	44.333466
3500.945174	783858.117578	44.338471
3501.117239	783855.790432	44.343476
3501.031082	783860.208821	44.348481
3501.166526	783856.810658	44.353485
3501.243702	783860.665143	44.358490
3501.276227	783861.149552	44.363495
3501.322714	783862.561692	44.368500
3501.319720	783865.890335	44.373505
3501.299395	783860.167271	44.378509
3501.765585	783843.111281	44.383514
3501.591577	783842.257575	44.388519
3501.397292	783840.868666	44.393524
3501.582417	783846.517173	44.398529
3501.378409	783827.852909	44.403533
3501.656408	783814.741709	44.408538
3501.607755	783811.470188	44.413543
3501.292422	783810.002308	44.418548
3501.251206	783811.966544	44.423553
3501.189912	783818.240914	44.428557
3501.699708	783804.897687	44.433562
3501.420799	783798.774504	44.438567
3501.674610	783785.079707	44.443572
3501.519865	783783.293058	44.448577
3501.456405	783784.281911	44.453581
3501.599895	783772.659956	44.458586
3500.891070	783750.354685	44.463591
3500.983377	783741.432576	44.468596
3501.348836	783746.612485	44.473601
3501.085515	783741.661459	44.478605
3501.252895	783745.208247	44.483610
3501.184722	783753.001007	44.488615
3500.939087	783740.656728	44.493620
3501.141171	783750.854427	44.498625
3501.252609	783743.887075	44.503629
3501.487106	783744.339920	44.508634
3501.357844	783747.541530	44.513639
3501.191640	783731.954536	44.518644
3501.151828	783728.485817	44.523649
3501.159839	783724.667014	44.528653
3501.473464	783725.107492	44.533658
3501.190226	783720.649002	44.538663
3501.354609	783726.692404	44.543668
3501.264575	783722.252657	44.548673
3501.210240	783725.099957	44.553677
3501.310267	783723.469241	44.558682
3501.404975	783728.104162	44.563687
3501.390177	783699.963805	44.568692
3501.173410	783696.326956	44.573697
3501.019282	783698.553595	44.578701
3501.385858	783691.007920	44.583706
3501.092858	783699.080609	44.588711
3501.280258	783694.059090	44.593716
3501.193143	783701.267543	44.598721
3501.300365	783704.481149	44.603725
3501.119407	783698.293617	44.608730
3501.001012	783705.115403	44.613735
3501.224044	783705.765819	44.618740
3501.368216	783693.654181	44.623745
3500.999737	783681.328995	44.628749
3501.280599	783668.608614	44.633754
3501.198946	783670.138714	44.638759
3501.446128	783668.827590	44.643764
3501.367570	783673.783300	44.648769
3501.056737	783677.306992	44.653773
3501.249757	783669.788424	44.658778
3501.545837	783685.208559	44.663783
3501.353504	783668.548731	44.668788
3500.977271	783651.623944	44.673793
3500.892096	783653.203543	44.678797
3501.431031	783641.030099	44.683802
3500.887855	783647.624680	44.688807
3501.145469	783649.052806	44.693812
3501.047798	783647.648753	44.698817
3501.183013	783653.452060	44.703821
3501.244054	783646.737206	44.708826
3500.860210	783651.153323	44.713831
3501.444822	783653.411330	44.718836
3501.491030	783658.004938	44.723841
3501.782642	783660.504521	44.728845
3501.797050	783635.149148	44.733850
3501.304895	783630.625367	44.738855
3501.619917	783627.394794	44.743860
3501.353342	783628.953812	44.748865
3501.723727	783616.415115	44.753869
3501.513197	783601.177357	44.758874
3501.231268	783597.599585	44.763879
3501.453131	783592.719437	44.768884
3501.425649	783597.814053	44.773889
3501.271551	783592.111670	44.778893
3501.433152	783588.856118	44.783898
3501.049306	783581.036068	44.788903
3501.243843	783564.364449	44.793908
3501.232085	783566.862546	44.798913
3501.063760	783566.007915	44.803917
3501.394633	783565.173138	44.808922
3500.913478	783567.499888	44.813927
3500.830087	783566.387255	44.818932
3500.986481	783571.795762	44.823937
3501.437011	783565.949895	44.828941
3501.631866	783567.877299	44.833946
3501.755163	783578.283359	44.838951
3501.513282	783555.806552	44.843956
3501.545141	783546.257346	44.848961
3501.211885	783544.792207	44.853965
3501.342631	783537.674787	44.858970
3501.372482	783545.256685	44.863975
3501.650817	783539.339823	44.868980
3501.119773	783523.417813	44.873985
3501.264199	783521.290654	44.878989
3501.598328	783520.063800	44.883994
3501.523396	783516.894133	44.888999
3501.268976	783509.004821	44.894004
3501.335754	783513.546368	44.899009
3501.397046	783498.461664	44.904013
3501.675604	783485.105004	44.909018
3501.110579	783482.941899	44.914023
3501.274247	783479.049678	44.919028
3501.327317	783467.294490	44.924033
3501.496776	783485.916350	44.929037
3501.317472	783479.043117	44.934042
3501.342275	783453.881214	44.939047
3501.504165	783444.800994	44.944052
3501.359273	783445.166330	44.949057
3501.503055	783446.073891	44.954061
3501.613886	783445.567172	44.959066
3501.333221	783435.087744	44.964071
3501.459481	783426.453583	44.969076
3501.385328	783416.480249	44.974081
3501.449350	783411.673590	44.979085
3501.552727	783410.335951	44.984090
3501.133204	783421.414463	44.989095
3501.251899	783421.787543	44.994100
3501.389488	783397.488824	44.999105
3501.542873	783389.682460	45.004109
3501.406748	783383.879197	45.009114
3501.185745	783395.709860	45.014119
3501.332814	783388.296052	45.019124
3501.470266	783387.002027	45.024129
3501.571048	783384.734809	45.029133
3501.700486	783370.618091	45.034138
3501.688766	783375.661466	45.039143
3501.432352	783362.143457	45.044148
3501.268128	783368.825910	45.049153
3501.292838	783355.214995	45.054157
3501.872223	783339.951051	45.059162
3501.438561	783332.970589	45.064167
3501.314960	783329.221081	45.069172
3501.442732	783331.550614	45.074177
3501.204423	783334.280001	45.079181
3501.370372	783317.954863	45.084186
3500.884533	783300.801582	45.089191
3501.315901	783294.811636	45.094196
3501.487488	783303.056910	45.099201
3501.140597	783310.502180	45.104205
3501.152556	783297.039980	45.109210
3501.056838	783305.718612	45.114215
3501.564035	783298.444196	45.119220
3501.296771	783302.254953	45.124225
3501.224142	783306.720540	45.129229
3501.484252	783297.037403	45.134234
3501.234095	783285.867714	45.139239
3501.119705	783274.187311	45.144244
3501.252289	783275.635064	45.149249
3501.308979	783288.988813	45.154253
3501.332727	783272.930530	45.159258
3501.344796	783281.102873	45.164263
3501.439818	783279.864408	45.169268
3501.267689	783277.003503	45.174273
3501.024209	783266.469049	45.179277
3501.129918	783258.718933	45.184282
3500.975014	783266.868448	45.189287
3501.056489	783251.633191	45.194292
3501.277713	783255.024983	45.199297
3501.429799	783256.812322	45.204301
3501.249992	783248.323670	45.209306
3501.290861	783251.352079	45.214311
3501.406113	783256.865169	45.219316
3501.145278	783262.681780	45.224321
3501.090183	783260.928359	45.229325
3501.261264	783249.203287	45.234330
3501.216664	783234.330330	45.239335
3500.926159	783225.173690	45.244340
3500.969384	783215.622234	45.249345
3501.170311	783229.883557	45.254349
3501.009865	783220.266052	45.259354
3501.089325	783230.043191	45.264359
3500.984652	783224.283819	45.269364
3500.994718	783235.589169	45.274369
3500.827354	783244.181186	45.279373
3501.228913	783233.986373	45.284378
3501.076390	783235.625546	45.289383
3501.005407	783235.049338	45.294388
3501.138810	783238.356973	45.299393
3501.045337	783250.412693	45.304397
3501.325301	783243.859002	45.309402
3501.096292	783247.223285	45.314407
3500.983033	783244.646847	45.319412
3501.443989	783243.302224	45.324417
3501.146561	783247.117729	45.329421
3501.402435	783239.784642	45.334426
3501.139017	783228.910614	45.339431
3500.915434	783217.051391	45.344436
3501.328099	783217.868003	45.349441
3501.134559	783218.485694	45.354445
3501.107645	783208.455717	45.359450
3500.936562	783217.488878	45.364455
3501.048422	783227.163061	45.369460
3501.064201	783224.419602	45.374465
3500.844190	783230.768281	45.379469
3501.194183	783234.531534	45.384474
3501.210221	783233.892776	45.389479
3501.188659	783228.022521	45.394484
3501.011132	783220.218741	45.399489
3500.604092	783231.687195	45.404493
3501.303814	783224.039971	45.409498
3501.409252	783229.946197	45.414503
3501.090990	783238.708652	45.419508
3501.025311	783223.153702	45.424513
3500.916348	783227.722915	45.429517
3501.364900	783237.197609	45.434522
3500.967119	783234.518802	45.439527
3501.187310	783228.610756	45.444532
3501.311666	783241.268759	45.449537
3501.284290	783231.287836	45.454541
3501.241885	783207.652881	45.459546
3501.199903	783206.778453	45.464551
3501.299405	783208.818763	45.469556
3501.456579	783207.423726	45.474561
3501.013653	783203.234588	45.479565
3501.241753	783205.989011	45.484570
3501.101352	783213.108424	45.489575
3501.362446	783212.822937	45.494580
3501.648532	783212.386701	45.499585
3501.505984	783196.696863	45.504589
3501.444605	783193.524923	45.509594
3501.413558	783190.886665	45.514599
3500.963257	783184.838655	45.519604
3501.484660	783178.002418	45.524609
3501.456135	783182.559088	45.529613
3501.633678	783157.910619	45.534618
3501.485099	783144.668999	45.539623
3501.687245	783151.245450	45.544628
3501.625366	783145.577217	45.549633
3501.491975	783136.053257	45.554637
3501.624403	783121.201323	45.559642
3501.413808	783129.702348	45.564647
3501.377056	783120.114310	45.569652
3501.601504	783112.688101	45.574657
3501.467133	783124.358856	45.579661
3501.516742	783090.674713	45.584666
3501.286602	783091.053393	45.589671
3501.125649	783080.701539	45.594676
3501.544778	783086.950443	45.599681
3501.556696	783090.179244	45.604685
3501.339781	783068.480067	45.609690
3501.300484	783063.983001	45.614695
3501.260753	783058.604923	45.619700
3501.622007	783058.205876	45.624705
3501.180428	783057.442842	45.629709
3501.471948	783052.257721	45.634714
3501.005742	783051.792229	45.639719
3500.971418	783054.832481	45.644724
3501.601229	783050.622400	45.649729
3501.078164	783031.858936	45.654733
3501.249818	783016.364302	45.659738
3501.176507	783021.319675	45.664743
3501.392926	783023.831255	45.669748
3501.321576	783030.107936	45.674753
3500.819208	783029.403351	45.679757
3501.330518	783032.260421	45.684762
3501.011868	783034.806691	45.689767
3501.237397	783030.464000	45.694772
3501.002221	783026.927558	45.699777
3500.819104	783039.046622	45.704781
3501.220905	783035.361662	45.709786
3501.187411	783037.618611	45.714791
3501.155672	783038.113127	45.719796
3501.652542	783032.259555	45.724801
3501.251468	783014.309103	45.729805
3501.337822	782999.806745	45.734810
3500.926797	783005.255464	45.739815
3500.982037	783010.141801	45.744820
3501.411616	782983.250582	45.749825
3501.211402	782938.640086	45.754829
3500.971654	782842.833684	45.759834
3501.172412	782681.705082	45.764839
3500.928686	782485.445049	45.769844
3500.595115	782236.322426	45.774849
3500.208368	781942.305554	45.779853
3499.994072	781585.776834	45.784858
3499.626363	781193.363843	45.789863
3499.260060	780750.934036	45.794868
3498.684435	780257.678017	45.799873
3497.807409	779729.025534	45.804877
3497.322689	779152.762483	45.809882
3497.073967	778529.390976	45.814887
3496.571176	777846.776982	45.819892
3495.853038	777128.020783	45.824897
3494.858028	776365.917978	45.829901
3494.143107	775549.831308	45.834906
3493.230924	774694.665994	45.839911
3492.429188	773789.968012	45.844916
3491.859808	772833.198659	45.849921
3490.565362	771840.420761	45.854925
3489.669177	770797.712857	45.859930
3488.475797	769726.986363	45.864935
3487.432109	768582.441285	45.869940
3486.188711	767404.620919	45.874945
3485.095760	766186.436993	45.879949
3483.859818	764931.693774	45.884954
3482.803278	763629.375012	45.889959
3481.201398	762288.356540	45.894964
3480.239558	760900.721643	45.899969
3478.905560	759481.189647	45.904973
3477.319967	757995.825250	45.909978
3476.113146	756494.217293	45.914983
3474.548812	754935.825639	45.919988
3472.948381	753339.539589	45.924993
3470.811963	751709.543510	45.929997
3469.786198	750042.656508	45.935002
3467.854955	748333.709103	45.940007
3466.127515	746585.205798	45.945012
3464.090428	744801.383466	45.950017
3462.113988	742988.116878	45.955021
3460.927095	741129.760497	45.960026
3458.800893	739251.672823	45.965031
3456.734788	737317.275134	45.970036
3454.832962	735355.930375	45.975041
3452.480721	733376.046514	45.980045
3450.611217	731351.085542	45.985050
3448.585050	729292.556139	45.990055
3446.337357	727201.726342	45.995060
3444.250606	725091.491218	46.000065
3441.606759	722941.069349	46.005069
3439.693730	720755.363686	46.010074
3437.430788	718551.210630	46.015079
3435.203274	716303.390079	46.020084
3432.556865	714026.566936	46.025089
3430.113420	711745.042836	46.030093
3427.833820	709411.204234	46.035098
3425.322965	707062.860751	46.040103
3422.722072	704692.856525	46.045108
3420.320184	702278.859129	46.050113
3417.751169	699854.952225	46.055117
3414.981376	697398.454842	46.060122
3412.376721	694916.764991	46.065127
3409.998846	692413.273963	46.070132
3407.525706	689892.478195	46.075137
3404.503514	687336.686575	46.080141
3402.171344	684757.879563	46.085146
3399.267255	682147.903165	46.090151
3396.380381	679518.503232	46.095156
3393.835814	676872.992286	46.100161
3390.951823	674203.174139	46.105165
3388.332530	671502.081936	46.110170
3385.506307	668780.797751	46.115175
3382.046369	666036.790558	46.120180
3379.731593	663279.214490	46.125185
3376.226314	660519.669478	46.130189
3373.611108	657705.442876	46.135194
3370.493545	654881.899127	46.140199
3367.811791	652044.707415	46.145204
3364.962495	649188.975947	46.150209
3361.707254	646313.735135	46.155213
3358.704973	643408.804411	46.160218
3355.591545	640499.243986	46.165223
3352.188448	637570.025794	46.170228
3349.176398	634617.042038	46.175233
3345.566983	631663.284553	46.180237
3342.592045	628687.106075	46.185242
3340.126027	625703.740587	46.190247
3336.698675	622696.489136	46.195252
3333.087398	619672.159864	46.200257
3330.031052	616631.579011	46.205261
3326.868958	613576.492746	46.210266
3323.603305	610499.045375	46.215271
3320.517163	607419.937742	46.220276
3317.096366	604319.594514	46.225281
3313.637332	601208.618707	46.230285
3310.323022	598081.724244	46.235290
3307.259795	594957.567671	46.240295
3303.671745	591802.269246	46.245300
3300.486868	588643.273731	46.250305
3296.811906	585482.380493	46.255309
3293.435022	582295.709328	46.260314
3290.138670	579109.709949	46.265319
3286.345539	575900.353327	46.270324
3283.302206	572688.057034	46.275329
3279.427059	569471.218077	46.280333
3276.440067	566236.569355	46.285338
3273.100705	562992.736432	46.290343
3269.138402	559737.050697	46.295348
3265.746180	556469.325257	46.300353
3261.920979	553208.816279	46.305357
3258.277339	549928.495394	46.310362
3255.102285	546658.333915	46.315367
3251.818792	543361.719219	46.320372
3247.777499	540063.899308	46.325377
3243.931872	536765.186810	46.330381
3240.586716	533451.195833	46.335386
3236.928008	530143.099909	46.340391
3233.545847	526824.149555	46.345396
3229.829539	523496.457131	46.350401
3226.490059	520165.911482	46.355405
3222.758231	516819.132310	46.360410
3218.957741	513469.427528	46.365415
3214.823438	510128.747767	46.370420
3211.746665	506769.401614	46.375425
3208.142215	503422.813681	46.380429
3204.120942	500049.724163	46.385434
3200.290297	496689.199229	46.390439
3196.598626	493314.507286	46.395444
3193.133768	489947.147681	46.400449
3189.375698	486573.124455	46.405453
3185.433721	483190.253783	46.410458
3181.697744	479807.473771	46.415463
3178.391533	476442.247500	46.420468
3174.750415	473040.370846	46.425473
3171.121673	469642.783989	46.430477
3167.247483	466246.050541	46.435482
3163.370948	462855.151089	46.440487
3159.451942	459446.528488	46.445492
3155.881987	456047.548902	46.450497
3152.117090	452647.026283	46.455501
3148.360221	449238.559536	46.460506
3144.004633	445837.135493	46.465511
3140.469418	442425.530318	46.470516
3137.048266	439025.031702	46.475521
3133.376940	435628.822857	46.480525
3129.471664	432224.550090	46.485530
3125.728332	428814.133815	46.490535
3121.465217	425397.839669	46.495540
3118.086200	421991.931488	46.500545
3114.186052	418591.573933	46.505549
3110.613834	415185.338075	46.510554
3106.663359	411766.697181	46.515559
3102.704422	408366.136181	46.520564
3099.004271	404962.779134	46.525569
3094.931019	401552.471101	46.530573
3091.092425	398148.370012	46.535578
3087.117687	394757.855793	46.540583
3083.296455	391358.815785	46.545588
3079.816540	387959.249011	46.550593
3075.716232	384567.846502	46.555597
3071.970385	381174.032342	46.560602
3068.083374	377780.330971	46.565607
3063.963444	374396.774003	46.570612
3060.360707	371007.863655	46.575617
3056.360210	367627.495291	46.580621
3052.564331	364251.394998	46.585626
3048.695953	360868.004140	46.590631
3044.609940	357498.243226	46.595636
3040.916637	354123.527198	46.600641
3036.843008	350774.895445	46.605645
3032.742484	347399.279057	46.610650
3029.242555	344051.778788	46.615655
3025.227907	340709.803804	46.620660
3021.572520	337358.199272	46.625665
3017.750562	334010.533079	46.630669
3013.714013	330670.485639	46.635674
3009.684226	327330.275434	46.640679
3005.836859	324000.263117	46.645684
3001.773227	320669.048971	46.650689
2997.394243	317339.634106	46.655693
2993.749420	314016.698360	46.660698
2989.796062	310699.346553	46.665703
2986.091036	307397.121114	46.670708
2982.054613	304102.667923	46.675713
2978.285903	300804.603270	46.680717
2974.146669	297510.696391	46.685722
2970.251471	294237.864096	46.690727
2966.123590	290968.883377	46.695732
2962.173541	287699.142461	46.700737
2957.907053	284437.000996	46.705741
2953.952099	281188.964352	46.710746
2950.194782	277942.330518	46.715751
2945.914437	274715.756665	46.720756
2941.977945	271484.775881	46.725761
2938.177919	268271.224915	46.730765
2934.303111	265059.409973	46.735770
2930.141858	261858.896295	46.740775
2926.095142	258656.082544	46.745780
2922.503558	255463.121614	46.750785
2917.834476	252290.499532	46.755789
2913.684265	249118.722566	46.760794
2910.032292	245963.719121	46.765799
2905.669829	242820.720506	46.770804
2901.537394	239679.578680	46.775809
2897.732477	236549.072732	46.780813
2893.439037	233430.917169	46.785818
2889.343169	230330.717435	46.790823
2885.516748	227241.414928	46.795828
2881.201764	224159.391540	46.800833
2876.899007	221085.442067	46.805837
2872.391477	218029.489438	46.810842
2868.519052	214987.155777	46.815847
2864.241970	211943.736700	46.820852
2860.472512	208927.620891	46.825857
2856.361323	205930.873676	46.830861
2852.110212	202932.152998	46.835866
2848.074165	199942.411811	46.840871
2844.039821	196964.338078	46.845876
2839.920385	194019.164381	46.850881
2835.384695	191075.369488	46.855885
2831.231489	188139.990244	46.860890
2827.252676	185223.479560	46.865895
2822.921408	182318.336272	46.870900
2818.952238	179423.129582	46.875905
2814.696646	176557.851531	46.880909
2810.725635	173688.629088	46.885914
2806.532513	170839.989196	46.890919
2802.091690	168002.213953	46.895924
2798.108619	165186.653427	46.900929
2794.087378	162288.416836	46.905933
2790.084286	159496.889287	46.910938
2785.970502	156718.129588	46.915943
2781.413087	153953.987798	46.920948
2777.497657	151197.692450	46.925953
2773.238765	148468.044342	46.930957
2769.311490	145736.829956	46.935962
2765.154927	143040.647551	46.940967
2760.951251	140337.150000	46.945972
2757.166317	137651.830272	46.950977
2752.658287	134988.494365	46.955981
2748.400518	132326.140966	46.960986
2744.581937	129683.647442	46.965991
2740.467639	127057.695368	46.970996
2736.341142	124443.357790	46.976001
2732.082598	121838.455452	46.981005
2728.102731	119255.046024	46.986010
2724.340947	116684.644534	46.991015
2719.959051	114126.277408	46.996020
2715.955744	111580.069844	47.001025
2711.880886	109047.593969	47.006029
2707.542494	106528.321549	47.011034
2703.512461	104024.159978	47.016039
2699.676048	101533.157586	47.021044
2695.620289	99048.758056	47.026049
2691.574629	96595.735383	47.031053
2688.194225	94128.489587	47.036058
2683.644519	91684.634513	47.041063
2679.323400	89255.322409	47.046068
2675.449130	86843.225307	47.051073
2671.347716	84442.083367	47.056077
2667.383546	82059.804910	47.061082
2663.566981	79683.469491	47.066087
2659.184409	77315.756073	47.071092
2655.177066	74963.160354	47.076097
2650.736303	72631.496988	47.081101
2646.839756	70305.653532	47.086106
2642.837835	67995.134611	47.091111
2638.666066	65711.508055	47.096116
2634.584293	63428.141926	47.101121
2630.531784	61163.015039	47.106125
2626.505575	58912.483363	47.111130
2622.354043	56679.818195	47.116135
2618.099152	54459.360976	47.121140
2614.727456	52245.577084	47.126145
2610.123308	50052.918594	47.131149
2606.126920	47875.240050	47.136154
2602.303199	45704.565985	47.141159
2597.889833	43564.099463	47.146164
2593.747139	41414.601516	47.151169
2589.494921	39280.978120	47.156173
2585.138072	37166.497633	47.161178
2581.141620	35080.808278	47.166183
2576.735431	33015.974550	47.171188
2572.569603	30947.902165	47.176193
2568.384224	28920.044924	47.181197
2564.070444	26898.040437	47.186202
2560.157731	24894.661956	47.191207
2555.724676	22921.358737	47.196212
2551.031293	20952.712643	47.201217
2546.322941	19019.513943	47.206221
2542.113639	17105.345922	47.211226
2537.759021	15203.079757	47.216231
2532.730561	13343.447595	47.221236
2528.218326	11506.684626	47.226241
2522.234984	9720.370722	47.231245
2516.493753	7970.782370	47.236250
2509.223516	6305.218534	47.241255
2498.646412	4778.077025	47.246260
2486.620715	3368.123145	47.251265
2473.775178	2118.046994	47.256269
2460.268038	1010.490436	47.261274
2440.555538	241.887830	47.266279
2402.278598	198.547890	47.271284
2376.150156	212.158744	47.276289
2366.553305	220.778869	47.281293
2367.957784	219.201914	47.286298
2375.040634	220.182081	47.291303
2382.330667	235.389421	47.296308
2387.931885	234.826452	47.301313
2390.752059	233.287464	47.306317
2391.068439	234.468783	47.311322
2389.508345	226.461525	47.316327
2386.222332	222.606346	47.321332
2382.800908	212.647098	47.326337
2379.444764	205.971233	47.331341
2375.791306	218.280811	47.336346
2373.002954	209.475423	47.341351
2370.087633	214.142678	47.346356
2367.576056	213.763676	47.351361
2364.570174	201.714556	47.356365
2361.630408	205.132743	47.361370
2358.404796	205.491894	47.366375
2355.091395	207.861182	47.371380
2352.483736	193.338904	47.376385
2349.548875	206.377649	47.381389
2345.904009	210.323781	47.386394
2342.637748	199.542986	47.391399
2338.613709	207.560223	47.396404
2336.254511	201.826271	47.401409
2332.918563	206.556173	47.406413
2328.977412	208.039714	47.411418
2326.473386	208.270166	47.416423
2323.045082	209.616526	47.421428
2319.954176	204.769034	47.426433
2316.594700	204.098735	47.431437
2313.180309	198.767162	47.436442
2309.723158	193.119566	47.441447
2306.561247	203.915854	47.446452
2302.838482	206.241628	47.451457
2299.609130	202.807904	47.456461
2296.098663	197.453402	47.461466
2293.405989	199.867968	47.466471
2289.783609	205.000210	47.471476
2285.854715	197.426861	47.476481
2282.899077	193.061277	47.481485
2278.619786	199.071441	47.486490
2275.629829	188.025982	47.491495
2272.527200	207.978719	47.496500
2268.931980	195.942744	47.501505
2265.698220	197.132130	47.506509
2262.185747	195.153798	47.511514
2259.085450	197.375872	47.516519
2255.743509	203.884824	47.521524
2252.047382	198.511926	47.526529
2248.405954	204.504567	47.531533
2244.742144	204.179308	47.536538
2242.058185	193.048017	47.541543
2238.114703	198.164069	47.546548
2234.291393	196.092004	47.551553
2231.133373	189.160567	47.556557
2227.709070	196.375296	47.561562
2224.831703	204.108755	47.566567
2221.296315	199.827564	47.571572
2218.061482	192.006447	47.576577
2214.430105	190.758604	47.581581
2210.831640	199.734383	47.586586
2207.147820	194.717094	47.591591
2203.321689	197.650714	47.596596
2200.368302	193.212034	47.601601
2197.144929	196.506946	47.606605
2193.628850	192.694161	47.611610
2190.262671	197.647135	47.616615
2186.308542	198.186760	47.621620
2183.042205	198.030296	47.626625
2179.770318	194.758297	47.631629
2176.039319	203.175835	47.636634
2172.878415	189.404598	47.641639
2168.926522	199.558855	47.646644
2165.410170	201.554975	47.651649
2162.299398	189.335682	47.656653
2158.823583	198.959859	47.661658
2155.133118	194.266344	47.666663
2152.289087	194.084945	47.671668
2148.747116	191.475331	47.676673
2145.271577	195.347568	47.681677
2141.058233	193.330235	47.686682
2137.837435	188.047534	47.691687
2134.094965	191.366732	47.696692
2130.499249	187.553776	47.701697
2127.406352	196.978836	47.706701
2124.168974	198.811092	47.711706
2120.572606	191.429405	47.716711
2117.095931	192.413223	47.721716
2113.768400	186.213891	47.726721
2109.836004	185.566860	47.731725
2106.424967	189.622009	47.736730
2103.277281	184.425961	47.741735
2099.609676	190.995394	47.746740
2096.063231	191.702224	47.751745
2092.677108	190.596389	47.756749
2089.250692	188.664765	47.761754
2086.039531	186.911441	47.766759
2082.153244	189.155299	47.771764
2078.597985	185.086087	47.776769
2075.392634	183.303382	47.781773
2071.857349	188.507480	47.786778
2068.535187	184.249934	47.791783
2064.611140	190.675999	47.796788
2060.948114	183.773020	47.801793
2057.727842	183.748597	47.806797
2054.136881	193.798949	47.811802
2051.192972	174.944303	47.816807
2047.518437	194.556252	47.821812
2044.185172	180.745603	47.826817
2040.469379	187.303609	47.831821
2036.478743	181.407387	47.836826
2033.204954	182.511350	47.841831
2029.911489	181.451151	47.846836
2026.642461	179.301927	47.851841
2022.747611	183.489752	47.856845
2019.559103	185.675069	47.861850
2016.158889	183.097108	47.866855
2012.400157	188.513361	47.871860
2008.791045	178.738679	47.876865
2005.693165	186.902161	47.881869
2002.091554	185.323858	47.886874
1998.577338	178.982934	47.891879
1994.815996	182.438010	47.896884
1991.658391	176.961971	47.901889
1988.036158	176.794815	47.906893
1984.673240	181.677725	47.911898
1981.207656	184.396806	47.916903
1977.850814	181.242577	47.921908
1974.169038	181.015139	47.926913
1970.524599	181.215307	47.931917
1967.002229	182.690391	47.936922
1963.826478	178.362516	47.941927
1960.039255	178.467968	47.946932
1956.299885	174.003657	47.951937
1953.534614	173.259477	47.956941
1949.908249	177.449606	47.961946
1946.393099	170.368511	47.966951
1942.874013	176.905252	47.971956
1939.321673	179.005150	47.976961
1935.703476	183.810958	47.981965
1931.930159	184.401477	47.986970
1928.779301	177.696828	47.991975
1925.188596	180.739234	47.996980
1921.647836	171.532883	48.001985
1918.066340	171.561863	48.006989
1914.323880	179.952782	48.011994
1911.078196	170.190881	48.016999
1907.695437	173.425385	48.022004
1904.469155	171.418214	48.027009
1901.144138	167.256094	48.032013
1897.273744	173.041039	48.037018
1893.810665	163.632716	48.042023
1890.216918	170.905674	48.047028
1886.649643	170.843852	48.052033
1883.267019	169.389517	48.057037
1879.774447	173.938391	48.062042
1876.408852	169.399803	48.067047
1872.276908	178.936883	48.072052
1868.837840	169.970913	48.077057
1865.477679	172.673530	48.082061
1862.511166	170.470693	48.087066
1859.342109	166.708138	48.092071
1855.273251	171.584490	48.097076
1851.811149	171.990290	48.102081
1848.430799	167.963401	48.107085
1844.925949	167.031258	48.112090
1841.418603	166.010918	48.117095
1837.209613	177.679843	48.122100
1833.976980	171.896053	48.127105
1830.900653	181.884903	48.132109
1827.504380	181.356565	48.137114
1824.182482	172.071710	48.142119
1820.246513	173.228740	48.147124
1816.832459	173.525789	48.152129
1813.330756	165.613715	48.157133
1809.481794	187.600570	48.162138
1806.163361	170.652336	48.167143
1802.380819	169.184679	48.172148
1799.414167	165.997928	48.177153
1795.771293	174.262558	48.182157
1792.323598	174.647140	48.187162
1789.033593	165.037763	48.192167
1785.122180	169.484527	48.197172
1782.132959	179.013652	48.202177
1778.369726	175.293486	48.207181
1774.637321	176.728733	48.212186
1771.695996	166.533269	48.217191
1767.660467	171.331667	48.222196
1764.370946	171.912973	48.227201
1760.941175	163.451811	48.232205
1757.377826	184.141090	48.237210
1753.898745	170.622323	48.242215
1749.926367	175.347568	48.247220
1746.700207	175.308342	48.252225
1743.421292	173.515110	48.257229
1739.906791	175.020674	48.262234
1736.467590	169.332525	48.267239
1732.726199	175.505470	48.272244
1729.493635	171.050522	48.277249
1725.922278	177.646126	48.282253
1722.321322	180.794608	48.287258
1718.803172	179.912046	48.292263
1715.210908	178.905038	48.297268
1711.725939	176.394233	48.302273
1708.315024	176.086532	48.307277
1704.108830	171.878884	48.312282
1701.294048	168.532349	48.317287
1697.816299	180.175463	48.322292
1694.501490	171.620400	48.327297
1690.863300	166.346236	48.332301
1687.405663	166.242013	48.337306
1683.992223	170.041384	48.342311
1680.666987	184.508097	48.347316
1677.139359	173.246455	48.352321
1673.240883	170.683318	48.357325
1669.539935	172.651532	48.362330
1666.278354	169.751432	48.367335
1662.440020	171.507026	48.372340
1658.839307	166.821812	48.377345
1655.883832	167.825448	48.382349
1652.116657	176.501890	48.387354
1649.307838	174.306076	48.392359
1645.407146	175.479797	48.397364
1641.873617	165.956050	48.402369
1638.567636	170.070820	48.407373
1634.590246	177.922767	48.412378
1631.251815	168.415946	48.417383
1627.610673	169.074475	48.422388
1624.051331	171.972858	48.427393
1620.544423	172.664165	48.432397
1616.947461	177.488892	48.437402
1613.941254	162.159235	48.442407
1610.542853	176.773452	48.447412
1606.851513	175.146058	48.452417
1603.281126	170.554198	48.457421
1599.856067	163.554058	48.462426
1596.591941	165.314719	48.467431
1592.627064	167.036358	48.472436
1589.285997	162.411778	48.477441
1585.929767	164.427310	48.482445
1581.697744	176.122063	48.487450
1578.949551	163.571021	48.492455
1575.059910	171.646538	48.497460
1571.816855	167.076227	48.502465
1568.562468	164.510403	48.507469
1564.624882	162.886766	48.512474
1561.811581	160.754958	48.517479
1558.205035	166.868883	48.522484
1553.990378	168.306919	48.527489
1550.885256	159.282490	48.532493
1546.906222	167.261271	48.537498
1543.211512	156.456134	48.542503
1540.134607	172.627271	48.547508
1536.467249	165.310731	48.552513
1533.463369	163.645370	48.557517
1529.756572	165.380423	48.562522
1526.810011	164.307222	48.567527
1523.088393	157.432629	48.572532
1519.359779	165.112788	48.577537
1515.749755	165.377333	48.582541
1511.973505	175.618173	48.587546
1508.679363	161.020184	48.592551
1505.151747	162.888555	48.597556
1502.046875	162.602626	48.602561
1498.585605	167.779481	48.607565
1494.616011	162.762920	48.612570
1491.141116	159.114803	48.617575
1487.638907	166.107784	48.622580
1484.238670	171.195996	48.627585
1480.876183	163.157863	48.632589
1477.199014	168.469761	48.637594
1473.984910	159.193493	48.642599
1470.126246	162.401375	48.647604
1466.689165	168.681797	48.652609
1463.069163	160.462512	48.657613
1459.438372	170.487601	48.662618
1456.682098	159.168607	48.667623
1452.688638	165.438041	48.672628
1449.503048	161.279572	48.677633
1445.795161	160.398332	48.682637
1441.805698	164.278448	48.687642
1438.401992	157.483847	48.692647
1435.056729	157.979068	48.697652
1431.755927	155.683157	48.702657
1428.264745	150.398749	48.707661
1425.015819	163.436154	48.712666
1421.669794	149.460119	48.717671
1418.029525	161.299576	48.722676
1414.170638	158.382328	48.727681
1411.046701	149.667795	48.732685
1406.892855	161.211149	48.737690
1403.767084	163.298234	48.742695
1399.752983	165.337706	48.747700
1396.756323	164.414760	48.752705
1393.298368	160.843124	48.757709
1389.351396	166.466209	48.762714
1386.363713	160.422775	48.767719
1382.997768	156.419116	48.772724
1379.495423	164.298022	48.777729
1375.851378	160.964335	48.782733
1371.991502	162.460808	48.787738
1368.397831	157.170318	48.792743
1365.107061	158.536578	48.797748
1361.308181	156.410409	48.802753
1358.304023	158.200053	48.807757
1354.668783	159.607583	48.812762
1351.435735	157.016348	48.817767
1347.707950	160.978926	48.822772
1343.796783	158.512827	48.827777
1340.673000	154.205515	48.832781
1337.120778	164.322742	48.837786
1333.459629	158.236052	48.842791
1330.078983	157.702273	48.847796
1326.506508	157.274457	48.852801
1323.616762	150.728488	48.857805
1319.569358	160.265157	48.862810
1316.359099	149.915817	48.867815
1313.007164	153.436746	48.872820
1308.806459	160.665673	48.877825
1305.346172	154.329248	48.882829
1302.027034	162.597122	48.887834
1298.631490	162.647832	48.892839
1295.013545	157.481397	48.897844
1291.619171	161.470897	48.902849
1288.369239	157.901539	48.907853
1284.169285	157.720666	48.912858
1281.072985	146.467631	48.917863
1277.851399	160.835921	48.922868
1274.020673	158.224378	48.927873
1270.842388	154.887427	48.932877
1267.082542	155.903197	48.937882
1263.590682	153.643581	48.942887
1259.929106	157.064300	48.947892
1256.636837	150.195381	48.952897
1253.143780	151.115606	48.957901
1249.520880	159.184267	48.962906
1245.924160	147.841901	48.967911
1242.655508	155.513412	48.972916
1239.001941	150.570884	48.977921
1235.543485	154.143314	48.982925
1232.089380	155.607955	48.987930
1228.489742	149.416768	48.992935
1225.069594	145.820298	48.997940
1221.729117	150.548043	49.002945
1218.347460	146.629167	49.007949
1214.584754	148.803365	49.012954
1210.960023	147.206828	49.017959
1207.349189	149.034543	49.022964
1204.177430	140.748371	49.027969
1200.811272	142.676991	49.032973
1196.953852	152.709149	49.037978
1193.240902	153.303144	49.042983
1189.713665	150.903559	49.047988
1186.628092	146.947834	49.052993
1183.132798	140.901689	49.057997
1179.528354	148.195503	49.063002
1176.283919	141.486814	49.068007
1172.474906	133.768670	49.073012
1168.772335	146.867648	49.078017
1165.228064	145.271188	49.083021
1161.721657	153.112822	49.088026
1158.639069	141.870350	49.093031
1155.022745	153.494146	49.098036
1151.168725	144.628256	49.103041
1148.082933	150.904390	49.108045
1144.602377	147.342719	49.113050
1141.197696	149.277390	49.118055
1137.847387	150.925134	49.123060
1134.039805	145.225299	49.128065
1130.831694	145.006272	49.133069
1126.899269	154.012461	49.138074
1123.390340	153.963922	49.143079
1120.125145	154.728294	49.148084
1116.380841	150.888379	49.153089
1113.324869	149.500235	49.158093
1109.926006	155.509013	49.163098
1105.875754	139.858990	49.168103
1102.361164	146.673678	49.173108
1098.572546	154.860079	49.178113
1095.254736	139.082734	49.183117
1091.652569	147.065932	49.188122
1088.482114	141.478344	49.193127
1085.412278	145.347490	49.198132
1081.573781	134.381593	49.203137
1077.893672	145.104212	49.208141
1074.318557	151.377881	49.213146
1071.018883	138.521083	49.218151
1067.393691	140.762391	49.223156
1063.544476	151.046411	49.228161
1060.274335	140.314246	49.233165
1056.735313	150.957836	49.238170
1053.213193	142.590534	49.243175
1050.037924	145.666259	49.248180
1046.479997	140.541159	49.253185
1043.090757	139.448832	49.258189
1039.219212	145.692990	49.263194
1036.417093	143.692474	49.268199
1032.568206	138.094069	49.273204
1029.071820	144.238362	49.278209
1025.577209	139.619060	49.283213
1021.738231	144.377457	49.288218
1018.402253	137.670510	49.293223
1014.848490	136.967792	49.298228
1011.427142	141.610182	49.303233
1008.095076	141.220776	49.308237
1004.091269	148.020341	49.313242
1000.728715	132.493669	49.318247
997.351484	143.412501	49.323252
993.588431	135.848598	49.328257
990.561714	141.735863	49.333261
986.781724	151.474383	49.338266
983.373806	150.903868	49.343271
980.134311	138.819153	49.348276
976.689785	153.026249	49.353281
972.932692	144.657808	49.358285
968.989303	145.863784	49.363290
965.791818	146.396138	49.368295
962.239685	136.508618	49.373300
958.314783	149.458965	49.378305
955.414972	143.664532	49.383309
951.818638	149.656818	49.388314
948.261748	150.201160	49.393319
945.287729	138.290033	49.398324
941.480210	149.137049	49.403329
938.124572	137.807708	49.408333
934.235658	142.672034	49.413338
930.656239	147.924509	49.418343
927.203352	143.874528	49.423348
923.946921	150.636194	49.428353
920.179937	138.991612	49.433357
916.728063	146.207833	49.438362
913.579653	150.699950	49.443367
910.045043	141.224168	49.448372
906.132307	146.946466	49.453377
902.672931	132.994764	49.458381
898.906919	145.635503	49.463386
895.694343	137.596299	49.468391
892.280324	141.933854	49.473396
888.402760	147.840480	49.478401
885.487691	144.383358	49.483405
881.423875	145.396252	49.488410
878.773588	132.491647	49.493415
875.198239	147.510203	49.498420
871.264861	141.111999	49.503425
867.836232	133.245847	49.508429
863.828996	135.180049	49.513434
860.245352	133.260837	49.518439
856.971502	140.370103	49.523444
853.809802	143.554497	49.528449
850.544517	138.481733	49.533453
846.843393	139.662479	49.538458
842.908672	137.915309	49.543463
839.679837	147.792199	49.548468
836.162925	136.535618	49.553473
833.056212	137.718204	49.558477
829.119318	146.456265	49.563482
826.044689	139.714799	49.568487
822.766475	135.969710	49.573492
818.706759	140.351450	49.578497
814.972726	141.714534	49.583501
811.226111	139.934759	49.588506
808.064950	145.624824	49.593511
804.738864	138.226704	49.598516
801.316288	148.523092	49.603521
798.274478	141.634125	49.608525
794.076824	138.893583	49.613530
790.736636	134.303982	49.618535
787.207489	139.314508	49.623540
783.467960	139.042774	49.628545
780.165587	138.462134	49.633549
776.583967	147.527401	49.638554
773.493749	138.665477	49.643559
769.838081	130.173686	49.648564
765.740270	134.457006	49.653569
762.543328	136.438370	49.658573
758.899974	142.925308	49.663578
755.861341	137.855055	49.668583
752.453546	135.326207	49.673588
749.084037	141.213433	49.678593
745.336266	130.837789	49.683597
741.651939	140.191235	49.688602
738.006484	147.327092	49.693607
734.060870	142.746899	49.698612
730.846303	142.642917	49.703617
727.151071	137.719792	49.708621
724.125584	138.332862	49.713626
721.439026	135.336732	49.718631
717.359864	136.165434	49.723636
713.449319	137.638459	49.728641
710.026948	127.360575	49.733645
706.467902	131.673443	49.738650
702.974581	140.775522	49.743655
699.771798	137.480584	49.748660
696.133391	147.541877	49.753665
692.508832	140.807490	49.758669
689.070874	138.729487	49.763674
685.683984	135.846208	49.768679
682.149131	139.579484	49.773684
678.384506	141.292268	49.778689
674.929838	127.896776	49.783693
671.539850	141.592352	49.788698
668.301007	138.638437	49.793703
664.744759	136.680211	49.798708
660.732115	132.521848	49.803713
657.576068	138.733183	49.808717
653.889484	136.434699	49.813722
650.671194	135.578342	49.818727
647.273445	135.901718	49.823732
643.343778	140.883268	49.828737
640.045607	136.068844	49.833741
636.498978	142.138872	49.838746
633.304403	133.163636	49.843751
629.781778	133.661602	49.848756
625.809332	141.358079	49.853761
622.210592	132.889079	49.858765
618.822669	135.191471	49.863770
615.461653	142.779539	49.868775
611.987850	130.215992	49.873780
608.467732	126.882203	49.878785
605.173019	124.911517	49.883789
601.335969	137.889337	49.888794
597.797370	138.310722	49.893799
594.581956	130.920672	49.898804
590.727573	137.643200	49.903809
587.507767	132.376756	49.908813
584.073446	127.919043	49.913818
580.450313	134.440839	49.918823
577.301608	125.483758	49.923828
573.277467	132.327791	49.928833
570.100735	125.842872	49.933837
566.485259	136.928845	49.938842
563.207236	136.104022	49.943847
559.732954	128.469789	49.948852
555.861140	135.672794	49.953857
552.608068	128.766395	49.958861
549.033723	139.137241	49.963866
545.485466	132.751647	49.968871
542.188447	127.139805	49.973876
538.430724	134.081334	49.978881
535.063888	125.882946	49.983885
531.277813	130.835720	49.988890
527.506382	128.594874	49.993895
524.373380	130.784604	49.998900
520.784316	129.859814	50.003905
517.866029	123.271162	50.008909
514.082949	137.088455	50.013914
510.322243	129.537070	50.018919
506.928512	130.897597	50.023924
503.145207	139.124487	50.028929
499.840478	126.667396	50.033933
496.244260	134.048723	50.038938
492.912089	128.945452	50.043943
489.427058	137.945054	50.048948
485.788529	133.946480	50.053953
482.559371	129.690797	50.058957
478.906726	133.091411	50.063962
475.610202	133.427471	50.068967
472.115571	123.942478	50.073972
468.582770	139.292994	50.078977
464.887386	118.547834	50.083981
460.984055	137.398603	50.088986
457.694559	129.865189	50.093991
454.100757	135.657922	50.098996
450.400360	135.373868	50.104001
447.314655	124.549823	50.109005
444.129966	133.483411	50.114010
440.765166	127.632288	50.119015
437.065305	126.342067	50.124020
433.272521	124.566522	50.129025
429.739554	125.066185	50.134029
426.110094	132.857708	50.139034
422.792362	128.539992	50.144039
419.579013	128.695362	50.149044
415.514087	136.377926	50.154049
412.339960	129.721817	50.159053
408.719939	136.043865	50.164058
405.078867	137.076170	50.169063
401.776583	134.394891	50.174068
398.245871	144.407769	50.179073
395.048646	130.095717	50.184077
391.097471	134.052498	50.189082
387.575040	129.390367	50.194087
384.535795	128.233975	50.199092
380.717906	131.372604	50.204097
377.514367	133.051405	50.209101
374.199382	132.393796	50.214106
370.248661	133.262644	50.219111
366.850274	134.313899	50.224116
363.361816	135.667170	50.229121
360.025765	122.575968	50.234125
355.953533	133.550050	50.239130
352.599232	130.766206	50.244135
349.515941	122.033099	50.249140
345.655793	135.365796	50.254145
342.272537	133.225579	50.259149
338.730301	128.636176	50.264154
335.079886	131.580908	50.269159
331.680863	125.222658	50.274164
327.865205	139.693690	50.279169
324.870454	129.630579	50.284173
321.316226	135.246316	50.289178
318.086215	133.540854	50.294183
314.827107	126.724089	50.299188
310.532992	136.673074	50.304193
307.071935	123.471764	50.309197
303.443139	136.575243	50.314202
300.144613	128.695294	50.319207
296.663380	131.493314	50.324212
292.984699	135.783942	50.329217
289.742068	135.529488	50.334221
285.971229	134.193501	50.339226
282.653784	134.646805	50.344231
279.368280	131.292221	50.349236
275.732111	133.725373	50.354241
272.374085	126.718475	50.359245
268.633012	132.271749	50.364250
265.049454	124.433304	50.369255
261.575135	118.295694	50.374260
258.409235	118.826508	50.379265
254.992077	126.239976	50.384269
251.247142	125.567508	50.389274
247.389719	126.111743	50.394279
244.053825	128.235272	50.399284
240.382992	134.907029	50.404289
237.042216	125.116467	50.409293
233.469948	123.565897	50.414298
230.264877	126.640223	50.419303
227.242168	117.236447	50.424308
223.041332	126.199564	50.429313
219.586661	126.721846	50.434317
216.102245	132.285553	50.439322
212.586914	125.682980	50.444327
208.997030	125.666457	50.449332
205.344596	132.294214	50.454337
202.354446	127.713296	50.459341
198.609660	125.952482	50.464346
195.065658	127.482200	50.469351
191.645446	133.105461	50.474356
188.017315	133.015843	50.479361
184.904165	122.993491	50.484365
181.307695	125.989944	50.489370
177.619998	124.913067	50.494375
174.097717	123.493898	50.499380
170.350206	125.254826	50.504385
167.010955	132.409344	50.509389
163.855889	123.124405	50.514394
160.204997	126.841244	50.519399
156.694909	120.133473	50.524404
152.879896	126.982873	50.529409
149.483455	122.184051	50.534413
146.077331	128.279688	50.539418
142.420930	120.269216	50.544423
139.293866	124.922739	50.549428
135.585854	122.029882	50.554433
132.042276	126.062118	50.559437
128.318146	128.192729	50.564442
124.850520	118.017132	50.569447
121.278791	119.687266	50.574452
117.791013	121.720739	50.579457
114.538884	115.320593	50.584461
111.209053	117.990556	50.589466
107.252287	127.757051	50.594471
104.050173	124.955793	50.599476
100.339540	126.065560	50.604481
97.054231	126.058313	50.609485
93.659085	125.546250	50.614490
90.127475	126.697577	50.619495
86.799482	122.011445	50.624500
82.819620	125.498278	50.629505
79.461526	118.146628	50.634509
75.952611	118.215551	50.639514
72.176132	120.053827	50.644519
68.867676	124.564946	50.649524
65.286456	124.075720	50.654529
61.985661	114.788353	50.659533
58.587105	117.807628	50.664538
55.409213	121.823727	50.669543
51.837056	118.083875	50.674548
47.794783	122.887146	50.679553
44.754722	118.190723	50.684557
40.791736	121.406007	50.689562
37.587945	125.856447	50.694567
34.092347	116.251596	50.699572
30.295947	120.057723	50.704577
26.941680	116.517864	50.709581
23.200153	118.170347	50.714586
19.866353	132.534334	50.719591
16.512808	124.476471	50.724596
12.874105	126.055900	50.729601
9.438890	133.494427	50.734605
5.819746	125.835691	50.739610
2.441381	125.409621	50.744615