Thu Aug 25 16:32:52 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.483102	101.902829	0.000000
0.328827	89.562953	0.005005
0.365556	86.004297	0.010010
0.136381	82.898596	0.015014
-0.222183	82.764978	0.020019
0.174242	73.584871	0.025024
-0.482749	69.847007	0.030029
-0.724035	59.203917	0.035034
-1.220578	51.112868	0.040038
-1.644858	39.277243	0.045043
-1.310728	43.518165	0.050048
-1.952609	44.121806	0.055053
-1.832744	30.305827	0.060058
-2.041438	34.957666	0.065062
-2.543334	31.356863	0.070067
-3.142314	20.203525	0.075072
-3.265948	19.764178	0.080077
-3.120629	11.907938	0.085082
-3.375998	12.912929	0.090086
-4.072235	12.797418	0.095091
-4.451860	14.027523	0.100096
-4.718822	10.753748	0.105101
-5.235263	8.575761	0.110106
-5.347638	15.664427	0.115110
-6.154816	12.117787	0.120115
-5.589875	13.313791	0.125120
-5.867022	2.515002	0.130125
-5.622833	8.291780	0.135130
-5.736647	5.813427	0.140134
-6.792245	11.550250	0.145139
-7.042643	7.558867	0.150144
-7.321593	7.453906	0.155149
-7.293503	9.154806	0.160154
-7.549723	6.293802	0.165158
-8.046027	5.485738	0.170163
-8.232924	15.053820	0.175168
-8.251583	10.681276	0.180173
-8.413290	10.643367	0.185178
-8.682946	10.622370	0.190182
-9.366442	16.607779	0.195187
-9.347762	4.509784	0.200192
-9.592182	11.960824	0.205197
-9.764078	9.985119	0.210202
-10.288138	2.898156	0.215206
-11.098762	11.007388	0.220211
-11.035456	3.648060	0.225216
-11.451933	8.867125	0.230221
-11.742174	2.600909	0.235226
-11.178424	5.072097	0.240230
-11.929620	11.498384	0.245235
-11.371381	4.175404	0.250240
-12.038548	12.284306	0.255245
-12.618445	9.375940	0.260250
-12.936827	9.824489	0.265254
-12.832993	15.183496	0.270259
-13.044962	11.600546	0.275264
-12.973357	1.376706	0.280269
-13.586686	14.479093	0.285274
-13.931399	-1.504018	0.290278
-14.346210	1.898781	0.295283
-14.186694	9.837026	0.300288
-14.482819	8.051629	0.305293
-15.257441	5.778055	0.310298
-15.208701	0.939371	0.315302
-15.769438	7.152316	0.320307
-15.951848	13.555924	0.325312
-16.149455	8.293926	0.330317
-16.056562	11.281818	0.335322
-15.969687	9.569290	0.340326
-17.078161	16.453357	0.345331
-17.181808	11.464540	0.350336
-17.510302	12.196249	0.355341
-17.378838	6.923821	0.360346
-17.285951	13.999306	0.365350
-17.926362	9.407805	0.370355
-18.572617	5.351897	0.375360
-18.740667	13.724283	0.380365
-18.822801	8.627692	0.385370
-18.718350	16.394232	0.390374
-19.284521	21.478567	0.395379
-19.039805	8.358057	0.400384
-19.525691	16.169637	0.405389
-20.213430	7.542252	0.410394
-20.436774	9.991232	0.415398
-20.399727	6.432542	0.420403
-20.425998	2.266839	0.425408
-20.370428	12.733404	0.430413
-21.479579	14.799155	0.435418
-21.922271	13.482814	0.440422
-21.967476	13.496254	0.445427
-22.055006	11.469365	0.450432
-21.910131	15.632364	0.455437
-22.381375	14.130671	0.460442
-22.961993	8.004864	0.465446
-23.599737	22.148799	0.470451
-23.316295	19.541761	0.475456
-23.720133	25.714310	0.480461
-23.818480	19.788183	0.485466
-23.603582	13.721229	0.490470
-23.891711	9.919257	0.495475
-23.724627	15.151294	0.500480
-24.644581	18.658555	0.505485
-24.964487	19.619875	0.510490
-25.070171	6.911775	0.515494
-25.725331	14.490448	0.520499
-25.826045	-3.865753	0.525504
-25.935598	7.044298	0.530509
-26.568327	12.680064	0.535514
-26.335200	11.776692	0.540518
-26.572538	6.821479	0.545523
-26.876602	11.937510	0.550528
-27.541237	17.021453	0.555533
-27.967388	14.193402	0.560538
-27.837016	17.956874	0.565542
-27.846698	22.242168	0.570547
-27.828757	22.777227	0.575552
-28.683740	18.472446	0.580557
-28.881013	19.863807	0.585562
-29.170580	12.945746	0.590566
-29.253994	14.923546	0.595571
-29.478066	13.054094	0.600576
-29.879721	16.388395	0.605581
-29.395730	15.198943	0.610586
-30.055710	11.417270	0.615590
-30.251354	17.278783	0.620595
-30.690566	13.120832	0.625600
-30.874917	16.781755	0.630605
-31.236299	6.091079	0.635610
-31.231116	6.609154	0.640614
-31.890330	12.894479	0.645619
-31.853113	15.002076	0.650624
-31.860907	19.372494	0.655629
-32.790477	19.445406	0.660634
-33.179377	20.455502	0.665638
-33.577313	21.729606	0.670643
-33.433559	16.100907	0.675648
-33.666147	12.821748	0.680653
-33.429269	10.405506	0.685658
-33.329467	10.503793	0.690662
-34.534186	20.399034	0.695667
-34.712400	9.648018	0.700672
-34.860424	11.468262	0.705677
-34.917689	4.279687	0.710682
-34.424009	4.930031	0.715686
-35.549611	22.032599	0.720691
-36.274622	10.392816	0.725696
-36.705928	10.403477	0.730701
-36.487601	7.964832	0.735706
-36.274434	13.914150	0.740710
-36.627670	9.695272	0.745715
-36.616835	7.061347	0.750720
-37.168515	7.941923	0.755725
-37.642225	9.515802	0.760730
-37.676508	10.435532	0.765734
-38.352075	10.636326	0.770739
-37.891704	8.368565	0.775744
-38.052842	8.314748	0.780749
-39.027221	19.749455	0.785754
-39.217214	10.465112	0.790758
-39.654010	10.312117	0.795763
-39.433153	2.162472	0.800768
-39.709844	5.784077	0.805773
-39.785146	18.153592	0.810778
-40.343657	14.906517	0.815782
-41.068138	13.827321	0.820787
-40.767306	7.500130	0.825792
-41.054520	16.938395	0.830797
-41.333271	9.667463	0.835802
-40.979523	13.582596	0.840806
-41.623861	20.219936	0.845811
-42.296948	17.633059	0.850816
-42.502723	19.108010	0.855821
-42.702000	20.673692	0.860826
-42.674794	8.254821	0.865830
-42.649603	14.027948	0.870835
-43.051414	19.013763	0.875840
-43.451901	13.201420	0.880845
-43.712321	19.050937	0.885850
-43.750663	3.203321	0.890854
-44.396755	17.873745	0.895859
-44.988715	5.384212	0.900864
-45.528682	15.928271	0.905869
-45.148887	14.293233	0.910874
-45.029892	10.535040	0.915878
-45.670628	11.926282	0.920883
-45.922916	8.596426	0.925888
-46.067860	11.998072	0.930893
-45.704022	8.805797	0.935898
-46.153309	7.702465	0.940902
-47.256783	13.298095	0.945907
-46.989813	-0.417517	0.950912
-47.002959	16.374696	0.955917
-47.187308	6.545303	0.960922
-47.764079	-0.903556	0.965926
-48.200671	12.307178	0.970931
-48.758085	-2.956060	0.975936
-48.583034	11.829306	0.980941
-49.154325	3.512714	0.985946
-49.167324	2.847224	0.990950
-49.053137	11.061489	0.995955
-49.608620	8.462515	1.000960
-50.193748	10.446160	1.005965
-50.296545	15.378795	1.010970
-50.063003	9.084294	1.015974
-50.650259	8.461326	1.020979
-50.433526	-1.763103	1.025984
-50.599471	4.384819	1.030989
-51.087501	12.136621	1.035994
-51.265735	1.885491	1.040998
-51.909973	11.180377	1.046003
-51.878288	7.609873	1.051008
-53.009622	10.846533	1.056013
-53.132585	8.271538	1.061018
-53.120816	9.775677	1.066022
-53.517846	16.829848	1.071027
-53.346355	4.613001	1.076032
-53.868522	5.991992	1.081037
-53.722296	14.055705	1.086042
-53.620434	6.364468	1.091046
-53.612104	11.099354	1.096051
-54.346585	-0.130807	1.101056
-54.652869	3.720062	1.106061
-54.968409	10.638075	1.111066
-55.293803	4.010373	1.116070
-56.243946	16.918761	1.121075
-56.292962	8.048931	1.126080
-56.258991	13.206909	1.131085
-56.364767	9.085301	1.136090
-56.210850	7.340123	1.141094
-56.555407	15.442770	1.146099
-56.988359	7.038062	1.151104
-57.025973	13.124750	1.156109
-57.802975	11.016068	1.161114
-57.750339	1.367846	1.166118
-57.986204	10.064067	1.171123
-58.019552	1.397431	1.176128
-58.800282	13.187771	1.181133
-59.375395	13.863211	1.186138
-59.072682	8.867673	1.191142
-59.151946	9.006672	1.196147
-59.449438	8.161132	1.201152
-59.144118	8.034226	1.206157
-60.128178	8.792726	1.211162
-60.397793	11.837418	1.216166
-60.792544	11.573432	1.221171
-60.573499	6.356885	1.226176
-60.933191	11.706259	1.231181
-61.794582	13.429471	1.236186
-61.814901	4.665879	1.241190
-62.238900	12.274769	1.246195
-62.217978	10.917427	1.251200
-62.316016	8.490387	1.256205
-62.251160	8.939000	1.261210
-62.433859	4.636457	1.266214
-63.023344	13.910110	1.271219
-63.251339	1.515415	1.276224
-63.707209	4.864537	1.281229
-63.590780	17.801960	1.286234
-63.697336	9.026568	1.291238
-64.411209	15.010409	1.296243
-64.714202	14.887071	1.301248
-64.793759	12.612159	1.306253
-64.997037	12.359301	1.311258
-65.134157	6.148189	1.316262
-65.435650	17.183231	1.321267
-65.829983	5.162612	1.326272
-66.588934	9.714000	1.331277
-66.625887	10.836630	1.336282
-66.288898	9.347505	1.341286
-66.738039	14.698241	1.346291
-66.735638	10.480589	1.351296
-67.410820	10.972391	1.356301
-67.773262	7.688271	1.361306
-68.248584	1.479534	1.366310
-68.251521	13.515000	1.371315
-68.435934	13.293986	1.376320
-68.354416	11.952459	1.381325
-68.905545	18.347402	1.386330
-69.263653	15.625752	1.391334
-69.736726	15.010205	1.396339
-69.540086	11.249338	1.401344
-69.594129	7.720741	1.406349
-70.044977	7.278882	1.411354
-70.014293	8.492154	1.416358
-71.046850	10.675623	1.421363
-71.164726	11.035809	1.426368
-71.037443	5.472971	1.431373
-71.528481	17.841185	1.436378
-71.160725	3.284036	1.441382
-71.538904	10.034692	1.446387
-72.057773	13.067819	1.451392
-72.387031	2.641037	1.456397
-72.769970	7.120853	1.461402
-72.510781	0.746406	1.466406
-72.802047	7.227178	1.471411
-73.328364	2.636790	1.476416
-73.925815	4.312317	1.481421
-74.429482	2.480350	1.486426
-73.858841	1.960693	1.491430
-74.173947	13.434464	1.496435
-74.299804	8.521898	1.501440
-75.146368	6.452592	1.506445
-75.756307	12.306252	1.511450
-75.381111	9.453883	1.516454
-75.656825	16.371985	1.521459
-75.734531	10.834938	1.526464
-75.909174	16.832365	1.531469
-76.262886	13.065983	1.536474
-76.805738	1.666592	1.541478
-77.166765	10.388752	1.546483
-77.002574	11.017954	1.551488
-77.116296	9.941138	1.556493
-77.167368	9.056986	1.561498
-77.767693	7.708402	1.566502
-78.132627	11.805746	1.571507
-78.408515	10.286102	1.576512
-78.557041	8.885707	1.581517
-78.727754	19.039712	1.586522
-78.732949	15.427529	1.591526
-79.544286	17.165046	1.596531
-79.900679	18.132085	1.601536
-79.511236	11.866939	1.606541
-79.931997	12.002500	1.611546
-80.443653	10.522963	1.616550
-80.913041	17.177181	1.621555
-81.027535	16.790188	1.626560
-81.215969	11.552066	1.631565
-81.065301	14.334750	1.636570
-81.053244	6.249460	1.641574
-82.284497	8.024300	1.646579
-82.562952	6.501895	1.651584
-82.552219	10.502409	1.656589
-82.784074	4.802856	1.661594
-83.021719	6.178395	1.666598
-83.032824	8.163847	1.671603
-83.090811	10.602736	1.676608
-83.671276	10.326722	1.681613
-84.299527	10.384063	1.686618
-84.104160	5.278795	1.691622
-84.523959	16.167857	1.696627
-84.370116	10.452159	1.701632
-84.454140	10.478008	1.706637
-85.215457	17.332994	1.711642
-85.374417	11.286657	1.716646
-85.874985	12.111771	1.721651
-85.939081	11.539709	1.726656
-85.806548	11.759418	1.731661
-86.217091	16.370112	1.736666
-86.660900	14.367413	1.741670
-87.428265	10.811382	1.746675
-87.952111	17.875932	1.751680
-87.411675	15.908836	1.756685
-87.635220	15.909092	1.761690
-87.337269	5.118275	1.766694
-87.667049	8.874750	1.771699
-88.271527	3.885321	1.776704
-88.719348	7.555888	1.781709
-89.243136	8.719999	1.786714
-88.934880	1.126140	1.791718
-89.138276	14.458522	1.796723
-89.939880	10.544022	1.801728
-90.170492	18.464300	1.806733
-90.563807	16.735264	1.811738
-90.346396	2.707878	1.816742
-90.483904	16.400097	1.821747
-90.785941	11.442370	1.826752
-90.901368	6.284560	1.831757
-91.896266	4.801650	1.836762
-91.826307	1.032162	1.841766
-92.131509	10.773798	1.846771
-92.316385	12.596652	1.851776
-91.994884	12.179307	1.856781
-92.190663	10.713551	1.861786
-92.335624	12.286541	1.866790
-93.170525	14.075207	1.871795
-93.426709	10.726982	1.876800
-93.482622	1.301416	1.881805
-94.083805	10.564245	1.886810
-94.615223	7.926702	1.891814
-95.107421	10.721532	1.896819
-95.165466	9.420856	1.901824
-94.896488	6.363667	1.906829
-95.164508	9.531496	1.911834
-95.110888	8.194340	1.916838
-95.274842	20.087358	1.921843
-95.800152	15.322804	1.926848
-96.247009	20.530814	1.931853
-96.780934	14.125614	1.936858
-96.592447	12.245303	1.941862
-96.919431	20.092096	1.946867
-96.933307	8.960995	1.951872
-97.176212	12.311552	1.956877
-98.106195	9.331499	1.961882
-98.263619	10.314817	1.966886
-98.690539	15.342531	1.971891
-98.172096	9.898735	1.976896
-98.241226	11.466170	1.981901
-98.564088	11.719271	1.986906
-99.335908	11.805437	1.991910
-99.624562	17.216449	1.996915
-99.613558	14.523063	2.006912
-99.500164	16.554932	2.016909
-98.624764	15.131686	2.026906
-98.331075	12.662342	2.036902
-98.368323	16.808577	2.046899
-97.698435	17.283380	2.056896
-96.872252	14.442326	2.066893
-96.267046	20.584991	2.076890
-95.784600	12.162246	2.086886
-95.683626	10.689285	2.096883
-94.797301	10.645497	2.106880
-94.362308	17.670144	2.116877
-94.305984	14.864191	2.126874
-93.261778	13.930849	2.136870
-92.683429	14.746280	2.146867
-92.707084	9.744889	2.156864
-92.433967	13.212096	2.166861
-91.510611	19.678713	2.176858
-90.426618	9.862904	2.186854
-90.192517	14.048984	2.196851
-90.109723	7.275942	2.206848
-89.641281	9.923755	2.216845
-88.723444	10.486419	2.226842
-88.823636	9.070322	2.236838
-87.965875	10.804989	2.246835
-87.358747	9.721555	2.256832
-86.807010	0.651226	2.266829
-86.326460	10.887236	2.276826
-85.979134	7.712569	2.286822
-85.728608	4.404182	2.296819
-84.471054	10.945144	2.306816
-84.624201	10.620738	2.316813
-83.979603	11.295909	2.326810
-83.250332	11.666373	2.336806
-82.943665	8.846536	2.346803
-82.283707	5.233241	2.356800
-81.546988	7.686962	2.366797
-81.494565	8.394733	2.376794
-81.005668	11.843969	2.386790
-80.392377	14.158641	2.396787
-79.921591	8.085079	2.406784
-79.906297	10.236858	2.416781
-79.110050	8.138600	2.426778
-78.042258	14.107412	2.436774
-77.658983	13.166760	2.446771
-77.457364	8.674935	2.456768
-77.061432	13.782837	2.466765
-76.242254	9.232260	2.476762
-75.729975	8.258724	2.486758
-75.838668	5.573662	2.496755
-74.652333	9.265244	2.506752
-74.554314	8.353450	2.516749
-74.233645	14.502687	2.526746
-73.574847	12.622370	2.536742
-72.596357	8.236900	2.546739
-71.850121	12.136826	2.556736
-72.006826	9.886943	2.566733
-71.898275	8.963996	2.576730
-70.618955	11.247168	2.586726
-70.357257	7.544221	2.596723
-70.065531	11.876495	2.606720
-69.216911	5.423782	2.616717
-69.164593	5.488502	2.626714
-68.211535	8.405675	2.636710
-67.426040	3.632295	2.646707
-67.346094	1.285144	2.656704
-67.178477	20.354559	2.666701
-66.658150	14.501316	2.676698
-65.763015	14.072844	2.686694
-65.098175	12.410161	2.696691
-64.611459	8.703633	2.706688
-64.291597	8.979858	2.716685
-64.132875	16.203019	2.726682
-63.291862	12.985842	2.736678
-63.027004	12.434380	2.746675
-62.322796	10.673662	2.756672
-61.723094	9.781462	2.766669
-61.353537	14.430997	2.776666
-60.983257	3.887551	2.786662
-60.016656	9.656808	2.796659
-59.741999	14.435254	2.806656
-59.505854	11.601124	2.816653
-58.331783	18.107657	2.826650
-58.444904	10.082342	2.836646
-58.164958	10.301465	2.846643
-57.328785	14.237986	2.856640
-57.122249	8.332542	2.866637
-56.197833	6.999823	2.876634
-55.687700	11.066625	2.886630
-55.321653	9.225845	2.896627
-54.902805	12.413626	2.906624
-54.180393	7.171789	2.916621
-54.235314	11.846652	2.926618
-53.405125	5.444345	2.936614
-52.693501	3.530411	2.946611
-52.298994	10.729298	2.956608
-51.595919	7.017381	2.966605
-51.199116	3.613214	2.976602
-51.323711	12.512195	2.986598
-50.154632	13.206559	2.996595
-49.717606	12.285997	3.006592
-49.495618	15.663015	3.016589
-48.454284	12.791422	3.026586
-47.939598	7.148142	3.036582
-48.476342	0.380307	3.046579
-47.527176	6.557778	3.056576
-46.519240	7.559328	3.066573
-46.655820	9.918637	3.076570
-45.795050	10.303346	3.086566
-45.378777	6.436795	3.096563
-44.430687	8.569130	3.106560
-44.191672	13.349993	3.116557
-44.026390	5.981145	3.126554
-43.400476	8.632799	3.136550
-42.482931	6.350811	3.146547
-42.756230	9.951153	3.156544
-41.479006	13.156495	3.166541
-40.780121	10.382909	3.176538
-40.795504	13.527856	3.186534
-40.747862	13.292366	3.196531
-39.771297	5.995973	3.206528
-39.482287	10.053075	3.216525
-38.957573	12.761768	3.226522
-38.152977	-0.545544	3.236518
-37.897440	6.656111	3.246515
-37.200044	2.159466	3.256512
-36.647053	10.413749	3.266509
-36.541428	6.789109	3.276506
-35.172369	9.017044	3.286502
-35.004170	5.927465	3.296499
-34.906975	2.836341	3.306496
-34.779923	7.707606	3.316493
-33.878499	3.587641	3.326490
-33.490890	9.191029	3.336486
-32.729930	8.650535	3.346483
-32.502527	10.046818	3.356480
-31.238785	4.900730	3.366477
-30.910054	9.033971	3.376474
-31.060377	10.068117	3.386470
-30.632687	6.849181	3.396467
-29.489934	7.592022	3.406464
-29.321727	6.213065	3.416461
-28.778073	6.115269	3.426458
-27.869261	11.551462	3.436454
-27.607056	6.948774	3.446451
-27.524583	0.654122	3.456448
-27.237293	0.881598	3.466445
-26.392442	3.628829	3.476442
-25.217097	8.849031	3.486438
-25.258376	8.567285	3.496435
-24.673289	5.120946	3.506432
-24.371258	1.012535	3.516429
-23.555664	4.502452	3.526426
-23.153166	10.664213	3.536422
-23.136881	2.466567	3.546419
-22.294012	4.054687	3.556416
-21.930797	3.921807	3.566413
-21.115676	9.451877	3.576410
-20.280370	9.210181	3.586406
-20.225014	11.175119	3.596403
-20.115725	9.694519	3.606400
-19.142712	8.848368	3.616397
-19.189487	5.162076	3.626394
-18.223126	12.258696	3.636390
-17.479041	8.632221	3.646387
-17.332976	5.365544	3.656384
-16.542539	12.172947	3.666381
-16.352294	12.292084	3.676378
-15.954510	11.152756	3.686374
-14.947764	7.127163	3.696371
-14.530913	4.600511	3.706368
-14.556177	7.522090	3.716365
-13.769551	14.884460	3.726362
-13.406115	9.828750	3.736358
-12.572350	12.305288	3.746355
-11.639458	11.633319	3.756352
-11.356157	5.275520	3.766349
-11.500023	7.331861	3.776346
-11.418841	10.506027	3.786342
-10.212083	7.656037	3.796339
-9.702396	3.404215	3.806336
-8.963079	10.023222	3.816333
-8.532883	8.980187	3.826330
-8.537191	7.590246	3.836326
-7.648378	10.026481	3.846323
-6.887935	7.069023	3.856320
-7.004585	12.700738	3.866317
-6.179625	10.281204	3.876314
-5.855898	13.978073	3.886310
-5.350578	9.242257	3.896307
-4.744379	18.482908	3.906304
-4.350576	15.684265	3.916301
-4.148596	31.463287	3.926298
-3.613677	39.305434	3.936294
-2.868038	41.707087	3.946291
-2.400553	54.856415	3.956288
-1.981755	61.167698	3.966285
-1.920564	84.134462	3.976282
-1.272527	95.025375	3.986278
-0.931877	106.579018	3.996275
0.000000	122.971249	4.001280
-0.040830	126.669820	4.006285
-0.041895	134.535204	4.011290
0.304970	140.134585	4.016294
-0.043307	152.262225	4.021299
0.464896	161.167812	4.026304
0.323758	151.309416	4.031309
0.450929	160.224082	4.036314
0.479189	150.642870	4.041318
0.368417	150.657091	4.046323
0.523564	153.622599	4.051328
0.476924	159.713917	4.056333
0.455822	162.801956	4.061338
0.687436	168.207429	4.066342
0.808268	180.144526	4.071347
0.639451	172.849971	4.076352
0.729643	175.676961	4.081357
0.877376	178.450643	4.086362
1.448779	153.885996	4.091366
0.503792	166.875942	4.096371
0.737095	160.749105	4.101376
0.777496	169.376810	4.106381
0.591868	159.436795	4.111386
0.943535	158.869189	4.116390
0.658731	152.852006	4.121395
0.738566	158.366680	4.126400
0.603016	160.507691	4.131405
0.647307	159.425089	4.136410
1.241991	174.780773	4.141414
0.874020	165.774170	4.146419
0.788487	159.732091	4.151424
0.816936	162.432709	4.156429
0.999823	160.996193	4.161434
0.741336	165.652704	4.166438
0.945408	174.207310	4.171443
1.094777	172.421699	4.176448
0.958252	170.933987	4.181453
0.898976	178.261173	4.186458
1.015411	175.816324	4.191462
0.971052	178.632758	4.196467
0.909091	166.221417	4.201472
1.102395	173.350837	4.206477
0.977288	173.920969	4.211482
0.793040	164.439485	4.216486
1.044810	182.971573	4.221491
0.919482	181.836451	4.226496
1.172987	184.451190	4.231501
0.842076	185.018766	4.236506
1.537322	186.817636	4.241510
1.199428	184.396513	4.246515
1.431403	171.268388	4.251520
1.099231	169.852459	4.256525
0.852189	168.141614	4.261530
1.085050	172.556624	4.266534
1.423786	176.391890	4.271539
1.215456	173.656235	4.276544
1.337964	180.309524	4.281549
1.024320	180.466265	4.286554
0.955207	174.633583	4.291558
1.206602	180.608608	4.296563
1.237465	189.427645	4.301568
1.143397	186.291265	4.306573
1.070694	194.076150	4.311578
1.259145	183.229610	4.316582
0.855565	194.578157	4.321587
1.369917	184.537945	4.326592
1.414668	179.959269	4.331597
1.085009	180.384278	4.336602
1.138692	175.968721	4.341606
1.024145	181.814419	4.346611
1.354632	186.910172	4.351616
1.468550	183.060988	4.356621
1.373356	184.752747	4.361626
1.618868	181.892198	4.366630
1.336801	193.360913	4.371635
1.373369	177.036321	4.376640
1.556683	183.328902	4.381645
1.439821	193.591635	4.386650
1.428987	179.789691	4.391654
1.724874	179.619972	4.396659
1.274111	181.035243	4.401664
0.952510	179.937201	4.406669
1.252732	192.127778	4.411674
1.595382	198.221391	4.416678
1.787277	212.678420	4.421683
1.683866	199.900220	4.426688
1.436428	201.125445	4.431693
1.486190	211.634168	4.436698
1.948407	211.011274	4.441702
1.861582	191.887050	4.446707
1.732175	191.613121	4.451712
1.552511	178.328020	4.456717
1.426725	189.269202	4.461722
1.769517	183.277064	4.466726
1.395107	189.935448	4.471731
1.440773	189.536011	4.476736
1.488055	198.779593	4.481741
1.942371	207.737940	4.486746
1.997008	208.495049	4.491750
1.667969	214.330072	4.496755
2.017841	207.912867	4.501760
1.556996	195.371011	4.506765
1.708174	197.906870	4.511770
1.894583	205.094332	4.516774
1.745717	218.415165	4.521779
1.820380	203.157112	4.526784
2.182714	216.239658	4.531789
1.657092	204.916519	4.536794
1.816467	192.131953	4.541798
1.599961	210.683656	4.546803
1.812133	210.982641	4.551808
1.856681	216.037781	4.556813
1.872736	214.984911	4.561818
2.078473	209.055368	4.566822
1.974388	219.727409	4.571827
1.884256	210.221663	4.576832
1.798479	218.831196	4.581837
1.965003	217.501645	4.586842
2.134583	210.919695	4.591846
2.166640	214.132293	4.596851
2.056168	215.044988	4.601856
2.079355	215.395731	4.606861
1.960017	214.297634	4.611866
2.260506	206.856765	4.616870
2.109476	219.570488	4.621875
1.756680	203.816251	4.626880
1.820883	210.551455	4.631885
1.903291	215.426654	4.636890
2.154574	210.255617	4.641894
2.021103	220.470346	4.646899
1.896121	217.569762	4.651904
2.198721	222.002332	4.656909
2.321051	215.063946	4.661914
2.186695	219.966781	4.666918
1.982583	220.381612	4.671923
2.113952	220.474955	4.676928
2.018642	218.749822	4.681933
1.916660	213.842945	4.686938
2.196669	221.395405	4.691942
1.931388	226.543386	4.696947
2.261428	223.954329	4.701952
2.094389	218.896289	4.706957
1.880064	217.202460	4.711962
2.191317	226.433172	4.716966
2.362445	240.577096	4.721971
2.420296	243.276284	4.726976
2.742001	230.747836	4.731981
2.275860	218.706675	4.736986
2.130756	216.347092	4.741990
2.098974	218.475016	4.746995
2.553500	228.730501	4.752000
2.633955	234.295722	4.757005
2.673486	226.851440	4.762010
2.297062	216.716656	4.767014
1.986861	220.713720	4.772019
2.597077	228.407437	4.777024
2.482437	236.369757	4.782029
2.039482	234.613669	4.787034
2.558238	232.295605	4.792038
2.522490	240.422738	4.797043
2.636758	232.656690	4.802048
2.283865	223.960912	4.807053
2.329821	241.009843	4.812058
2.730752	242.354950	4.817062
2.335379	247.156318	4.822067
2.271898	246.584152	4.827072
2.584037	252.540193	4.832077
2.525860	247.797289	4.837082
2.856994	246.239460	4.842086
2.698025	245.214011	4.847091
2.637320	241.233983	4.852096
2.680196	248.561012	4.857101
2.694687	245.701848	4.862106
2.760642	243.353485	4.867110
2.781034	243.283879	4.872115
2.770020	244.864376	4.877120
2.826194	248.987543	4.882125
2.434640	250.229024	4.887130
2.624340	246.541962	4.892134
2.508723	248.088228	4.897139
2.606948	242.577324	4.902144
2.715165	245.410992	4.907149
2.602272	254.385466	4.912154
2.676915	246.679405	4.917158
2.568092	254.166248	4.922163
3.003790	243.492909	4.927168
2.960976	242.575813	4.932173
2.631557	251.957541	4.937178
2.507642	243.488474	4.942182
2.698738	248.599758	4.947187
2.517636	243.553406	4.952192
2.822051	252.082836	4.957197
3.052044	267.818449	4.962202
3.538329	254.049293	4.967206
2.827181	252.588330	4.972211
2.627519	249.253344	4.977216
2.901538	246.252274	4.982221
2.477225	257.857214	4.987226
2.969776	253.657619	4.992230
2.867806	272.333811	4.997235
2.975699	279.891116	5.002240
3.175647	272.450155	5.007245
3.098939	283.307773	5.012250
3.024448	277.713186	5.017254
3.041125	273.056625	5.022259
3.101913	276.321681	5.027264
3.265074	267.557682	5.032269
3.162771	276.596947	5.037274
3.098428	278.391451	5.042278
2.766035	281.702294	5.047283
3.144470	275.033812	5.052288
3.512416	274.966699	5.057293
3.125730	277.843113	5.062298
3.236487	278.170644	5.067302
3.144628	279.842907	5.072307
3.032857	267.689241	5.077312
3.148572	265.611495	5.082317
2.827816	284.277686	5.087322
3.238958	274.861048	5.092326
3.203313	277.631839	5.097331
3.371206	276.786133	5.102336
3.132921	270.647724	5.107341
2.922994	267.453552	5.112346
3.350830	269.072861	5.117350
2.962988	272.329113	5.122355
2.895748	272.190978	5.127360
3.037963	281.925940	5.132365
3.205079	274.265491	5.137370
2.946483	278.918884	5.142374
3.394004	294.389479	5.147379
3.417972	288.456753	5.152384
3.512421	291.571002	5.157389
3.550458	304.929056	5.162394
3.661941	295.435969	5.167398
3.156726	290.718803	5.172403
3.104614	293.802231	5.177408
3.288276	285.240659	5.182413
3.083598	298.374140	5.187418
3.504460	286.257233	5.192422
3.510505	298.573071	5.197427
3.259138	293.917373	5.202432
3.397183	291.605166	5.207437
3.117297	301.067745	5.212442
3.357354	294.528507	5.217446
3.094181	299.106691	5.222451
3.164499	297.475826	5.227456
3.429847	317.186032	5.232461
2.995938	325.875473	5.237466
3.469547	323.937802	5.242470
3.499419	327.441834	5.247475
3.475629	321.526071	5.252480
3.522113	315.842913	5.257485
3.668427	325.320987	5.262490
3.877098	316.315710	5.267494
3.846873	321.980560	5.272499
3.576928	326.151678	5.277504
3.712345	323.517168	5.282509
3.192516	325.063496	5.287514
3.587875	312.662659	5.292518
3.391477	321.897029	5.297523
3.367829	312.906007	5.302528
3.755081	332.815434	5.307533
3.826338	349.265704	5.312538
3.948361	341.656585	5.317542
3.846744	341.811744	5.322547
3.944422	339.543822	5.327552
3.773975	334.859615	5.332557
3.858510	346.429179	5.337562
4.287756	323.557076	5.342566
3.896716	333.419912	5.347571
3.837052	328.645581	5.352576
3.742248	321.614621	5.357581
3.460742	323.155247	5.362586
3.576169	331.957941	5.367590
4.028066	345.333441	5.372595
3.904205	345.982479	5.377600
3.854647	341.383736	5.382605
4.012928	349.246395	5.387610
4.097029	345.803654	5.392614
3.915828	352.327419	5.397619
3.899145	352.583168	5.402624
4.055160	342.232009	5.407629
3.729191	354.796063	5.412634
4.045168	344.068654	5.417638
3.911276	352.976862	5.422643
3.579931	348.608934	5.427648
3.877046	344.487397	5.432653
3.765087	354.167308	5.437658
4.246324	355.863682	5.442662
3.819934	358.955143	5.447667
4.208308	348.507460	5.452672
4.000652	348.065450	5.457677
3.614391	357.601675	5.462682
4.280600	368.134131	5.467686
4.222932	377.179109	5.472691
4.367725	376.609108	5.477696
4.372007	373.995137	5.482701
4.338963	384.010722	5.487706
4.655496	362.086398	5.492710
4.179544	353.991984	5.497715
4.083695	347.546486	5.502720
3.958190	348.480527	5.507725
4.253373	353.588188	5.512730
4.548312	358.971142	5.517734
4.222263	360.319428	5.522739
4.328307	354.623762	5.527744
4.097659	355.957100	5.532749
4.182559	369.801418	5.537754
4.552059	365.127519	5.542758
4.228893	376.805276	5.547763
4.183096	373.484125	5.552768
4.665309	371.083182	5.557773
4.536492	365.762841	5.562778
4.783053	374.763315	5.567782
4.205463	369.285491	5.572787
4.209619	378.510613	5.577792
4.735924	363.039287	5.582797
4.546672	380.084073	5.587802
4.309720	369.987462	5.592806
4.494200	377.605577	5.597811
4.634239	377.745020	5.602816
4.604949	376.174048	5.607821
4.409395	372.129696	5.612826
4.693927	357.980772	5.617830
4.613948	365.937718	5.622835
4.582391	366.110375	5.627840
4.735182	369.503406	5.632845
4.072159	369.645284	5.637850
4.156968	365.215312	5.642854
4.558340	369.335043	5.647859
4.708884	375.075992	5.652864
4.558113	363.016959	5.657869
4.754972	368.624096	5.662874
4.615476	370.927107	5.667878
4.798346	374.467290	5.672883
4.286754	374.341826	5.677888
4.745170	375.969010	5.682893
4.219380	383.853441	5.687898
4.774133	375.654474	5.692902
4.434930	379.488434	5.697907
4.376348	378.557982	5.702912
4.621426	375.286171	5.707917
4.558685	383.961779	5.712922
4.937277	389.863160	5.717926
4.850012	402.089282	5.722931
4.800978	394.510106	5.727936
5.067206	397.227290	5.732941
4.660221	393.051541	5.737946
5.006807	395.363818	5.742950
5.219124	402.246735	5.747955
4.963734	382.886119	5.752960
5.192865	379.961664	5.757965
4.665986	385.944801	5.762970
4.734829	370.953279	5.767974
4.511767	373.424410	5.772979
4.737355	387.885794	5.777984
5.190668	399.723488	5.782989
4.838692	402.920358	5.787994
5.289739	397.183279	5.792998
5.025925	403.897182	5.798003
5.058685	404.417275	5.803008
5.105362	391.052259	5.808013
4.553605	392.280884	5.813018
4.743971	401.644526	5.818022
4.944366	401.682761	5.823027
4.869098	402.577295	5.828032
5.226007	393.687962	5.833037
4.896782	399.668609	5.838042
5.334423	403.146733	5.843046
4.930849	402.450673	5.848051
5.099874	400.630321	5.853056
5.281982	402.047693	5.858061
5.172601	406.785310	5.863066
5.076639	402.497551	5.868070
4.980288	400.918100	5.873075
4.982006	404.075373	5.878080
4.867319	401.828061	5.883085
4.891162	408.806952	5.888090
5.217804	406.585407	5.893094
5.030142	406.928059	5.898099
5.298677	401.168953	5.903104
5.123676	405.375835	5.908109
5.077756	430.627365	5.913114
5.126983	417.527693	5.918118
5.423101	430.212636	5.923123
5.245668	428.769277	5.928128
5.641293	417.776237	5.933133
4.891792	427.764892	5.938138
5.584603	426.093432	5.943142
5.037791	426.226593	5.948147
5.201607	416.798011	5.953152
5.436766	420.061084	5.958157
5.500598	430.330443	5.963162
5.444157	431.342254	5.968166
5.406341	429.870692	5.973171
5.215457	429.359611	5.978176
5.775813	431.635236	5.983181
5.466361	428.757193	5.988186
5.701942	425.597596	5.993190
5.531027	431.505992	5.998195
5.402906	429.298748	6.003200
5.582560	435.838773	6.008205
5.618111	430.562264	6.013210
5.350064	429.215362	6.018214
5.570139	435.391539	6.023219
5.358511	436.452977	6.028224
5.714761	422.444630	6.033229
5.352444	435.590255	6.038234
5.650371	432.854335	6.043238
5.261081	426.979984	6.048243
5.231531	431.724083	6.053248
5.759622	435.004539	6.058253
5.664077	435.677618	6.063258
5.711553	428.655962	6.068262
5.713188	430.690087	6.073267
5.643616	424.268920	6.078272
5.902573	425.648941	6.083277
5.514095	420.296500	6.088282
5.378861	405.919070	6.093286
4.947234	409.606161	6.098291
5.176316	417.726684	6.103296
5.528387	421.303642	6.108301
5.588805	425.524265	6.113306
5.383312	425.689372	6.118310
5.489114	427.131356	6.123315
5.320929	427.793670	6.128320
5.333407	426.598974	6.133325
5.582948	431.144316	6.138330
5.473667	428.813894	6.143334
5.422571	426.860345	6.148339
5.405340	427.783753	6.153344
5.628989	424.021731	6.158349
5.666136	428.429503	6.163354
5.784199	433.893978	6.168358
5.611157	427.099869	6.173363
5.590193	428.621828	6.178368
5.761124	424.709874	6.183373
5.663104	426.253397	6.188378
5.654534	425.735898	6.193382
5.226940	414.704159	6.198387
5.137348	433.087506	6.203392
5.800103	428.861203	6.208397
5.567898	433.735134	6.213402
5.665818	429.695409	6.218406
5.821644	430.452493	6.223411
5.645885	410.209313	6.228416
5.359619	409.675211	6.233421
5.319326	407.792740	6.238426
5.558340	416.006620	6.243430
5.080872	418.881461	6.248435
5.606328	420.134303	6.253440
5.828316	426.348143	6.258445
5.729058	419.852532	6.263450
5.634016	407.715133	6.268454
5.475296	406.401725	6.273459
5.537146	400.032743	6.278464
5.621346	397.678338	6.283469
5.306458	402.884764	6.288474
5.443101	404.666773	6.293478
5.496496	408.126006	6.298483
5.287829	407.127316	6.303488
5.531067	403.460309	6.308493
5.211140	416.384137	6.313498
5.772036	412.857187	6.318502
5.604996	420.027346	6.323507
5.466282	407.460179	6.328512
5.601038	396.061923	6.333517
4.819347	408.409509	6.338522
5.594310	419.269813	6.343526
5.843933	431.807014	6.348531
5.472876	431.099530	6.353536
5.498779	422.369616	6.358541
5.279921	429.307445	6.363546
5.460788	423.119130	6.368550
5.434306	431.384107	6.373555
5.356141	435.496728	6.378560
5.615065	436.728054	6.383565
5.742961	436.904203	6.388570
5.410612	431.318331	6.393574
5.542055	433.414378	6.398579
5.693647	428.907486	6.403584
5.804844	421.920142	6.408589
5.670260	422.551880	6.413594
5.319977	398.539445	6.418598
5.279169	403.481459	6.423603
5.292530	416.615666	6.428608
5.532662	414.654454	6.433613
5.758151	429.103232	6.438618
5.767311	424.672443	6.443622
5.429690	416.325365	6.448627
5.184643	392.372382	6.453632
5.520998	405.490776	6.458637
5.596304	423.288277	6.463642
5.709225	422.296150	6.468646
5.255690	414.214014	6.473651
5.270199	431.492687	6.478656
5.707045	421.110136	6.483661
5.744099	437.078615	6.488666
5.560933	420.702804	6.493670
5.070730	409.772629	6.498675
5.511004	422.365376	6.503680
5.419046	429.169424	6.508685
5.328273	439.826854	6.513690
5.581605	421.123665	6.518694
5.732911	424.912420	6.523699
5.673188	433.131985	6.528704
5.712175	419.265101	6.533709
5.733934	419.252229	6.538714
5.196566	406.507072	6.543718
5.370326	410.241684	6.548723
5.384032	424.404092	6.553728
5.676059	422.093053	6.558733
5.609104	423.100183	6.563738
5.593845	415.572655	6.568742
5.489904	409.001850	6.573747
5.255772	406.140484	6.578752
5.548141	408.511879	6.583757
5.595678	408.877793	6.588762
5.650529	413.931376	6.593766
5.512024	406.739546	6.598771
5.160015	416.011001	6.603776
5.397905	406.944151	6.608781
5.449969	421.005631	6.613786
5.572687	416.300780	6.618790
5.833366	424.536581	6.623795
5.794298	407.755380	6.628800
5.522203	399.483467	6.633805
5.470921	395.970177	6.638810
5.601300	398.047404	6.643814
5.668607	397.505362	6.648819
5.390989	408.862783	6.653824
5.440411	398.806710	6.658829
5.391408	400.393173	6.663834
5.372754	401.158610	6.668838
5.503966	399.638420	6.673843
5.240515	396.825943	6.678848
5.438286	398.035210	6.683853
5.624590	425.183454	6.688858
5.612733	417.076409	6.693862
5.381222	411.762653	6.698867
5.255163	416.161191	6.703872
5.627357	417.479176	6.708877
5.591276	426.270853	6.713882
5.449886	424.204898	6.718886
5.709508	421.250348	6.723891
5.516278	418.350934	6.728896
5.430023	410.100520	6.733901
5.429507	420.943119	6.738906
6.039056	421.622785	6.743910
5.531506	415.124707	6.748915
5.732524	410.483522	6.753920
5.842595	398.022918	6.758925
5.970577	406.826846	6.763930
5.976958	402.374351	6.768934
5.950585	402.267778	6.773939
5.627032	402.267880	6.778944
5.626925	400.704988	6.783949
5.146764	394.370310	6.788954
5.104433	397.420585	6.793958
5.397149	404.892036	6.798963
5.225657	405.086618	6.803968
5.683539	403.281121	6.808973
5.481843	402.075690	6.813978
5.436897	401.127281	6.818982
5.284716	390.599749	6.823987
5.269219	403.292367	6.828992
5.267781	400.527425	6.833997
5.306158	406.982004	6.839002
5.363145	397.247458	6.844006
5.578213	399.058308	6.849011
5.130885	404.317123	6.854016
5.398783	397.042639	6.859021
5.169755	402.428606	6.864026
5.079405	414.816576	6.869030
5.658976	415.788848	6.874035
5.536281	425.049689	6.879040
5.744973	420.726847	6.884045
5.696871	430.384139	6.889050
5.462180	423.273814	6.894054
5.484986	419.666651	6.899059
5.310108	420.409109	6.904064
5.791171	422.244726	6.909069
5.697881	417.118126	6.914074
5.207042	411.538109	6.919078
5.398302	416.968964	6.924083
5.560262	426.276957	6.929088
5.594467	433.779432	6.934093
5.434404	426.995944	6.939098
5.233832	421.610897	6.944102
5.450257	422.855209	6.949107
5.526609	437.485552	6.954112
6.274392	426.095635	6.959117
5.458020	422.600972	6.964122
5.349754	412.661349	6.969126
5.393526	411.544011	6.974131
5.603185	406.790739	6.979136
5.616931	403.273586	6.984141
5.469492	413.307111	6.989146
5.584716	406.420386	6.994150
5.587723	414.940170	6.999155
5.507700	417.189574	7.004160
5.836169	407.665594	7.009165
5.851181	409.773554	7.014170
5.803804	414.976035	7.019174
5.533933	413.844562	7.024179
5.682051	407.269066	7.029184
5.970786	408.540014	7.034189
5.371618	409.943752	7.039194
5.520793	410.483572	7.044198
5.683492	413.590313	7.049203
5.282821	408.802949	7.054208
5.861491	412.651295	7.059213
5.722789	404.779271	7.064218
5.843245	405.671613	7.069222
5.736580	396.392991	7.074227
5.255443	382.351358	7.079232
5.622147	379.626817	7.084237
5.735261	385.759623	7.089242
5.304428	393.866468	7.094246
5.621379	383.129392	7.099251
5.299109	393.440241	7.104256
5.682465	381.661350	7.109261
4.980230	393.262465	7.114266
5.641720	398.863254	7.119270
5.462347	406.449802	7.124275
5.490606	405.885404	7.129280
5.671317	397.219834	7.134285
5.222527	399.178993	7.139290
5.698709	410.775823	7.144294
5.490516	398.529604	7.149299
5.262667	397.480136	7.154304
5.715128	403.082038	7.159309
5.414975	412.940168	7.164314
5.494562	408.438236	7.169318
5.292641	422.707195	7.174323
5.414225	414.689978	7.179328
5.485173	414.590303	7.184333
5.580016	420.567791	7.189338
5.515324	412.541794	7.194342
5.894037	412.840000	7.199347
5.368430	413.697523	7.204352
5.730195	403.253978	7.209357
5.651411	403.453018	7.214362
5.392359	391.629236	7.219366
5.387210	379.332235	7.224371
5.146421	387.209979	7.229376
5.557007	402.521936	7.234381
5.214244	404.246178	7.239386
5.235198	409.061454	7.244390
4.927790	413.687728	7.249395
5.142947	414.245684	7.254400
5.371577	413.827066	7.259405
5.358654	414.933301	7.264410
5.403522	409.478163	7.269414
5.528849	417.583304	7.274419
5.757060	408.989382	7.279424
5.644977	410.332622	7.284429
5.284919	412.951777	7.289434
5.447595	409.667561	7.294438
5.300991	412.234289	7.299443
5.109893	415.159175	7.304448
5.365769	417.118662	7.309453
5.795143	432.842165	7.314458
5.566045	424.417967	7.319462
5.373857	418.791155	7.324467
5.370074	417.712906	7.329472
5.692711	420.282046	7.334477
5.673872	421.844802	7.339482
5.440296	416.370012	7.344486
5.344562	409.908655	7.349491
5.186695	415.688448	7.354496
5.395054	430.487933	7.359501
5.745106	431.878993	7.364506
5.680217	435.622527	7.369510
5.785560	421.672477	7.374515
5.371678	415.836785	7.379520
5.256540	410.413044	7.384525
5.195096	421.429710	7.389530
5.543507	433.185783	7.394534
5.435044	432.437156	7.399539
5.697623	433.870396	7.404544
5.661190	433.708449	7.409549
5.515194	427.334057	7.414554
5.532820	432.798449	7.419558
5.469641	418.741923	7.424563
5.209353	422.911551	7.429568
5.700240	426.988795	7.434573
5.618845	444.643185	7.439578
5.572165	430.852992	7.444582
5.680412	419.680344	7.449587
5.320615	410.618551	7.454592
5.689689	408.516912	7.459597
5.321398	414.082894	7.464602
5.312371	419.415413	7.469606
5.411070	419.611955	7.474611
5.480157	437.828072	7.479616
5.629521	430.692372	7.484621
5.488324	433.391138	7.489626
5.714924	433.599279	7.494630
5.402502	428.507009	7.499635
5.562180	423.707778	7.504640
5.852870	421.067909	7.509645
5.570828	415.948736	7.514650
5.301138	410.163222	7.519654
5.405294	415.541283	7.524659
5.242527	417.386024	7.529664
5.619475	416.491738	7.534669
5.318757	427.909740	7.539674
5.605306	435.053129	7.544678
5.981779	438.113725	7.549683
5.561487	427.713603	7.554688
5.372344	410.202918	7.559693
5.443739	412.213456	7.564698
5.242622	419.078897	7.569702
5.834063	419.274168	7.574707
5.706057	418.123631	7.579712
5.776182	411.300919	7.584717
5.682986	416.289111	7.589722
5.514122	413.373224	7.594726
5.185709	418.588101	7.599731
5.138818	420.886099	7.604736
5.454622	407.292237	7.609741
5.478194	416.530156	7.614746
5.204869	413.722388	7.619750
5.779567	424.224921	7.624755
5.342820	426.992139	7.629760
5.459214	425.493252	7.634765
5.174222	429.923023	7.639770
5.519695	438.325884	7.644774
5.771565	434.350624	7.649779
5.955379	436.005019	7.654784
5.680974	421.620908	7.659789
5.523156	423.439564	7.664794
5.450337	417.502975	7.669798
5.514185	416.581814	7.674803
5.697254	423.159265	7.679808
5.560873	413.005742	7.684813
5.570356	423.166550	7.689818
5.213983	413.480942	7.694822
5.380584	413.505489	7.699827
5.342356	415.862243	7.704832
5.370909	405.910678	7.709837
5.511049	426.880849	7.714842
5.387199	429.437687	7.719846
5.464284	429.726203	7.724851
5.481576	433.282849	7.729856
6.092809	428.447669	7.734861
5.711560	416.791717	7.739866
5.410001	418.730973	7.744870
5.230446	408.653821	7.749875
5.625844	412.277775	7.754880
5.533509	411.681649	7.759885
5.502280	417.852901	7.764890
5.251893	410.801989	7.769894
5.416006	401.854272	7.774899
5.506588	403.690955	7.779904
5.572405	408.059428	7.784909
5.553403	415.744244	7.789914
5.409308	408.357131	7.794918
5.672484	412.887677	7.799923
5.434207	415.525718	7.804928
5.589368	409.243356	7.809933
5.271117	408.084661	7.814938
5.404526	414.831246	7.819942
5.526931	409.250061	7.824947
5.492882	406.037798	7.829952
5.556126	409.542946	7.834957
5.421326	416.831442	7.839962
5.631481	424.606910	7.844966
6.047591	415.996201	7.849971
5.206824	416.868301	7.854976
5.219487	404.144537	7.859981
5.424507	417.682162	7.864986
5.344121	415.935689	7.869990
5.890000	426.132682	7.874995
5.585502	426.866974	7.880000
5.600640	410.051967	7.885005
5.686633	408.405980	7.890010
5.170378	405.370513	7.895014
5.461461	411.171714	7.900019
5.315038	409.299543	7.905024
5.619608	403.579084	7.910029
5.604491	409.716170	7.915034
5.669419	410.927269	7.920038
5.529066	407.215955	7.925043
5.371928	416.902979	7.930048
5.588673	410.639442	7.935053
5.792155	415.663410	7.940058
5.279553	413.905561	7.945062
5.702353	411.229175	7.950067
5.381046	414.462372	7.955072
5.386924	409.086112	7.960077
5.249606	411.752628	7.965082
5.267999	414.179607	7.970086
5.550606	409.892644	7.975091
5.402254	433.983279	7.980096
5.690883	424.734459	7.985101
5.259584	431.414500	7.990106
5.535257	431.551676	7.995110
5.938271	430.890593	8.000115
5.441773	420.660608	8.005133
5.583300	410.476877	8.010150
5.235679	419.809340	8.015168
5.282968	422.784166	8.020186
5.681588	428.001348	8.025203
5.554252	433.234667	8.030221
5.632307	427.980725	8.035238
5.451528	423.221770	8.040256
5.441673	431.100155	8.045274
5.510850	429.473589	8.050291
5.423190	441.621309	8.055309
5.860192	431.296597	8.060326
5.801368	433.293981	8.065344
5.500193	425.297130	8.070362
5.661800	415.195456	8.075379
5.407425	406.074137	8.080397
5.634042	416.440081	8.085414
5.548466	425.488496	8.090432
5.453046	440.313528	8.095450
5.983710	429.112615	8.100467
5.249553	422.272347	8.105485
5.293772	424.537605	8.110502
5.394803	433.055018	8.115520
5.377325	440.767345	8.120538
5.778632	430.978397	8.125555
5.461269	436.733792	8.130573
5.917935	437.599536	8.135590
5.738980	439.252828	8.140608
5.525771	439.418806	8.145626
5.726759	428.045488	8.150643
5.757447	437.252416	8.155661
5.692011	439.200344	8.160678
5.807638	434.581135	8.165696
5.689609	434.899456	8.170714
6.033477	435.312662	8.175731
5.672998	447.455795	8.180749
6.101612	434.857080	8.185766
5.702246	425.449203	8.190784
5.580132	415.742273	8.195802
5.694157	416.251450	8.200819
5.410004	418.520820	8.205837
5.504785	426.051452	8.210854
5.702139	435.005050	8.215872
5.866027	437.469308	8.220890
6.357847	430.534779	8.225907
5.512987	425.898806	8.230925
5.560432	412.936955	8.235942
5.523908	426.203263	8.240960
5.496602	427.457257	8.245978
5.503209	434.092845	8.250995
5.456717	441.822342	8.256013
5.764428	440.483446	8.261030
5.824331	442.635796	8.266048
5.851713	441.757385	8.271066
6.139447	437.133300	8.276083
5.814369	439.696260	8.281101
5.715786	432.374557	8.286118
5.569747	444.616632	8.291136
5.846444	443.658133	8.296154
6.189960	437.712505	8.301171
5.786475	441.679448	8.306189
6.023681	433.863323	8.311206
6.116172	431.204321	8.316224
5.665952	444.942557	8.321242
6.058882	440.349326	8.326259
5.859203	436.786212	8.331277
6.202755	439.758802	8.336294
5.645236	419.999518	8.341312
5.472399	430.181907	8.346330
5.506212	430.567954	8.351347
5.769974	435.998770	8.356365
5.899420	436.278316	8.361382
5.404565	433.114898	8.366400
5.323337	443.314499	8.371418
5.691048	433.502411	8.376435
6.196270	440.006230	8.381453
5.729955	436.273456	8.386470
5.946483	442.626850	8.391488
5.598924	445.199645	8.396506
6.057785	435.682540	8.401523
5.936245	444.307414	8.406541
5.652507	442.108142	8.411558
6.115390	436.320536	8.416576
5.689855	438.791939	8.421594
5.841384	430.225543	8.426611
5.783585	446.654130	8.431629
5.850328	454.176544	8.436646
6.003515	465.626987	8.441664
5.586925	464.338458	8.446682
6.340153	457.754277	8.451699
6.216634	464.555430	8.456717
6.118784	461.976739	8.461734
5.703463	441.879573	8.466752
5.696498	461.317132	8.471770
6.027850	458.936279	8.476787
5.880235	456.990230	8.481805
5.792157	457.985506	8.486822
6.277478	453.560831	8.491840
6.146684	470.846626	8.496858
6.348797	464.932612	8.501875
6.012099	459.907745	8.506893
6.124374	465.630547	8.511910
6.304989	456.046575	8.516928
5.915972	454.409747	8.521946
5.967968	440.052309	8.526963
5.985324	449.378095	8.531981
5.947787	450.756769	8.536998
6.380134	460.661319	8.542016
6.002557	461.190719	8.547034
6.049552	461.543143	8.552051
6.098767	459.168626	8.557069
5.935860	456.555948	8.562087
6.153286	460.898977	8.567104
5.956139	466.613456	8.572122
6.272497	467.463315	8.577139
6.113360	460.946345	8.582157
5.987947	468.113867	8.587175
5.968692	469.104672	8.592192
5.817232	469.712252	8.597210
6.164993	471.544951	8.602227
5.881800	467.183880	8.607245
6.007625	469.994930	8.612263
6.059894	464.296896	8.617280
6.060396	462.592725	8.622298
6.121007	465.467641	8.627315
6.122475	468.039401	8.632333
5.921589	464.321838	8.637351
6.062386	462.876550	8.642368
5.575318	474.320017	8.647386
6.146625	476.449048	8.652403
6.412304	490.677905	8.657421
6.169112	487.443489	8.662439
6.259581	477.911499	8.667456
6.018023	477.832612	8.672474
6.108565	485.278727	8.677491
6.623364	487.830021	8.682509
6.418071	481.793643	8.687527
6.317748	472.600816	8.692544
6.071689	471.676885	8.697562
6.348984	466.738850	8.702579
6.501996	466.979990	8.707597
6.112538	470.291495	8.712615
6.320224	470.997436	8.717632
6.398704	464.679918	8.722650
6.315832	461.256287	8.727667
6.263817	471.470261	8.732685
5.929443	472.715566	8.737703
6.229102	463.507411	8.742720
6.205526	469.929992	8.747738
6.628870	464.877557	8.752755
6.579988	465.185044	8.757773
6.121401	467.185107	8.762791
6.173967	463.888577	8.767808
6.176988	466.138204	8.772826
6.215053	464.014740	8.777843
6.114431	470.619806	8.782861
6.560973	485.956403	8.787879
6.619714	488.932600	8.792896
6.216193	480.768724	8.797914
6.259869	477.486207	8.802931
6.751494	487.640259	8.807949
6.628102	471.069668	8.812967
6.645361	468.816921	8.817984
6.276147	466.104023	8.823002
6.267948	464.249738	8.828019
6.348737	471.293435	8.833037
6.223404	473.162390	8.838055
6.326354	470.990889	8.843072
6.569139	469.785239	8.848090
6.059396	468.353516	8.853107
6.847146	477.924682	8.858125
6.299727	475.422740	8.863143
6.503776	465.207091	8.868160
6.399795	463.973723	8.873178
6.384746	467.040372	8.878195
6.516382	471.289549	8.883213
6.441545	478.553291	8.888231
6.556496	473.359826	8.893248
6.237620	479.355312	8.898266
6.559003	487.708839	8.903283
6.426094	487.603461	8.908301
6.339236	493.010335	8.913319
6.912201	487.546290	8.918336
6.686186	487.632223	8.923354
6.346273	472.553529	8.928371
6.443179	475.621574	8.933389
6.513298	485.169485	8.938407
6.602857	479.598147	8.943424
6.572629	482.840746	8.948442
6.541022	481.993665	8.953459
6.562887	476.950483	8.958477
6.311966	485.321095	8.963495
6.335003	488.422806	8.968512
6.733051	491.150183	8.973530
6.420687	499.107553	8.978547
6.629389	491.788172	8.983565
6.620667	506.391393	8.988583
6.531809	495.031888	8.993600
6.366248	496.869278	8.998618
6.263318	500.596639	9.003635
6.718673	490.388938	9.008653
6.436160	493.443851	9.013671
6.514268	489.581584	9.018688
6.844804	494.828388	9.023706
6.793142	489.992381	9.028723
6.882990	490.050915	9.033741
6.375117	496.006591	9.038759
6.714304	493.583481	9.043776
6.743602	497.435290	9.048794
6.626100	499.053713	9.053811
6.518534	496.000015	9.058829
6.637206	501.772319	9.063847
6.641920	486.507074	9.068864
6.380727	500.651233	9.073882
6.403347	494.740086	9.078899
6.635867	491.159736	9.083917
6.179027	495.662066	9.088935
6.458745	491.657758	9.093952
6.311205	513.323292	9.098970
6.815875	515.797283	9.103987
6.889843	521.715452	9.109005
6.869452	529.901643	9.114023
6.796637	517.709637	9.119040
6.699236	517.014874	9.124058
6.993164	517.129795	9.129075
7.106492	509.187882	9.134093
6.716598	510.372460	9.139111
6.737861	501.611846	9.144128
6.945897	491.985690	9.149146
6.471077	487.064506	9.154163
6.960726	491.538459	9.159181
6.720952	499.235148	9.164199
6.826498	508.569239	9.169216
7.014518	513.074677	9.174234
7.009376	508.101989	9.179251
7.166093	492.800299	9.184269
6.811093	493.338785	9.189287
6.852793	489.299186	9.194304
6.973671	496.866785	9.199322
6.833506	503.781013	9.204339
6.593410	492.855458	9.209357
6.604428	498.590980	9.214375
6.612412	493.695134	9.219392
6.728674	508.783700	9.224410
6.679471	519.795675	9.229427
7.200073	512.885007	9.234445
6.967961	520.025086	9.239463
6.714172	520.430951	9.244480
7.062216	524.056100	9.249498
6.752752	528.781499	9.254515
7.033233	518.544377	9.259533
6.944143	522.206459	9.264551
6.822351	521.057927	9.269568
6.974459	528.245107	9.274586
7.411711	522.136442	9.279603
7.415900	507.707546	9.284621
6.675717	501.991651	9.289639
6.905378	491.715170	9.294656
6.997627	495.105839	9.299674
6.616267	507.050313	9.304691
6.741889	509.627874	9.309709
7.139315	520.449952	9.314727
6.793540	513.883310	9.319744
6.973482	517.632625	9.324762
7.035207	514.429324	9.329779
6.852631	514.117134	9.334797
6.994370	515.713875	9.339815
6.949911	518.305462	9.344832
7.135362	516.603866	9.349850
7.069799	512.170816	9.354867
7.089570	507.677060	9.359885
7.087751	522.389665	9.364903
7.008772	528.732585	9.369920
7.305133	513.708798	9.374938
6.693079	525.092986	9.379955
7.427364	519.584720	9.384973
7.109307	518.160829	9.389991
7.021307	514.719056	9.395008
7.168283	516.116162	9.400026
6.891714	519.697165	9.405043
7.394589	516.986474	9.410061
7.183242	518.348204	9.415079
7.210545	515.913997	9.420096
7.315471	511.504728	9.425114
6.873697	517.980227	9.430131
7.364196	515.192581	9.435149
7.226521	525.473655	9.440167
7.059051	525.989071	9.445184
7.472558	509.574164	9.450202
7.339584	527.579875	9.455219
7.206513	511.957501	9.460237
7.066241	521.866598	9.465255
6.913016	519.795189	9.470272
7.216229	527.671902	9.475290
7.199067	520.195395	9.480307
7.418977	510.797741	9.485325
7.255349	518.400457	9.490343
7.489279	516.069575	9.495360
7.218000	513.565386	9.500378
6.983651	523.896320	9.505395
7.023449	517.237708	9.510413
7.291422	518.959837	9.515431
7.180510	517.030121	9.520448
6.993338	515.636215	9.525466
7.331907	513.380456	9.530483
6.995927	510.984234	9.535501
7.149826	511.594464	9.540519
6.975792	518.387774	9.545536
7.192141	508.406857	9.550554
6.846941	524.022171	9.555571
7.038993	538.016451	9.560589
7.422040	540.351711	9.565607
7.561128	542.753597	9.570624
7.628670	537.548607	9.575642
7.344235	537.381764	9.580659
7.198110	527.315619	9.585677
7.330610	531.763489	9.590695
7.226376	540.451969	9.595712
7.497595	541.463539	9.600730
7.575910	542.325452	9.605747
7.518569	539.001947	9.610765
7.204566	544.453894	9.615783
7.424882	539.382756	9.620800
7.735839	537.765635	9.625818
7.452786	539.971731	9.630835
7.346877	522.470551	9.635853
7.295641	533.265104	9.640871
7.304610	544.166995	9.645888
7.903833	541.636864	9.650906
7.380057	541.289770	9.655923
7.217637	535.344486	9.660941
7.623661	539.033137	9.665959
7.792222	539.003600	9.670976
7.561354	527.814647	9.675994
7.241947	529.947543	9.681011
7.773476	525.588194	9.686029
7.422740	520.379318	9.691047
7.276744	524.612046	9.696064
7.361263	529.335676	9.701082
7.253223	542.427084	9.706099
7.352017	544.715364	9.711117
7.389795	545.309075	9.716135
7.352601	546.643521	9.721152
7.373886	539.978333	9.726170
7.230121	556.660331	9.731187
7.639194	543.547051	9.736205
7.384483	547.080453	9.741223
7.055711	549.318960	9.746240
7.646149	547.446611	9.751258
7.428726	548.755647	9.756275
7.434810	548.088850	9.761293
7.643366	553.481015	9.766311
7.564552	552.000701	9.771328
7.839912	547.514226	9.776346
7.952578	549.030319	9.781363
7.524662	549.406662	9.786381
7.950186	544.281281	9.791399
7.449896	547.266182	9.796416
7.955909	543.636660	9.801434
7.751480	548.926273	9.806451
7.688281	542.760314	9.811469
8.085771	544.253870	9.816487
7.881601	546.886264	9.821504
8.015256	550.522919	9.826522
7.956659	540.076980	9.831539
7.646551	544.802485	9.836557
7.787864	545.752357	9.841575
7.717156	550.108995	9.846592
7.872807	540.579382	9.851610
7.454519	545.460691	9.856627
7.392514	543.971433	9.861645
7.609049	544.322542	9.866663
7.191720	554.350805	9.871680
7.829517	539.317681	9.876698
7.208907	544.906030	9.881715
7.601317	546.283618	9.886733
8.064530	557.398367	9.891751
7.723939	551.806041	9.896768
8.027085	561.102887	9.901786
7.416045	560.393925	9.906803
7.849686	567.931485	9.911821
8.049120	573.157828	9.916839
7.889227	575.644433	9.921856
7.892586	560.947380	9.926874
7.845378	555.766676	9.931891
7.617039	563.067126	9.936909
8.099582	562.707528	9.941927
7.908919	570.863612	9.946944
8.255757	555.497366	9.951962
8.013530	552.256475	9.956979
7.911423	548.128943	9.961997
7.652330	546.938806	9.967015
7.888774	548.571205	9.972032
7.773358	543.874560	9.977050
7.737562	552.047396	9.982067
7.885642	562.794958	9.987085
8.023897	564.297576	9.992103
7.771306	573.435349	9.997120
8.056351	575.694451	10.002138
8.046389	573.083039	10.007155
8.165882	573.149552	10.012173
8.354906	564.946445	10.017191
7.585474	560.566862	10.022208
8.077231	551.625209	10.027226
8.152311	571.160485	10.032243
7.941887	558.257866	10.037261
7.948705	555.694320	10.042279
7.987877	568.484972	10.047296
8.045240	572.291374	10.052314
8.277195	570.702407	10.057331
8.025567	566.355301	10.062349
7.925494	552.592798	10.067367
7.697491	562.219018	10.072384
8.333032	568.610947	10.077402
8.262844	569.145836	10.082419
7.993241	575.275644	10.087437
8.353790	573.587633	10.092455
8.065667	567.949211	10.097472
8.157627	555.223278	10.102490
7.933682	557.161341	10.107507
7.797060	561.910160	10.112525
8.116169	564.328025	10.117543
8.189878	570.763802	10.122560
8.324049	566.091161	10.127578
8.296667	572.419702	10.132595
7.882912	576.366192	10.137613
7.982393	572.358548	10.142631
8.050678	577.870528	10.147648
8.194628	568.838194	10.152666
7.850176	573.748968	10.157683
8.223042	576.969452	10.162701
8.287232	576.113669	10.167719
8.159538	585.269750	10.172736
8.193137	573.670102	10.177754
8.056825	571.378287	10.182771
8.156068	570.630621	10.187789
8.188283	570.575110	10.192807
8.093477	575.178526	10.197824
8.302370	570.049209	10.202842
8.234789	570.507950	10.207859
7.969542	570.278140	10.212877
8.371390	573.973764	10.217895
8.161126	576.591338	10.222912
8.420918	574.556197	10.227930
8.352449	574.008377	10.232947
8.386110	583.906035	10.237965
8.562962	576.070903	10.242983
8.483968	578.162981	10.248000
8.447454	578.137173	10.253018
8.382071	572.700535	10.258035
8.168907	578.761541	10.263053
8.620236	572.761107	10.268071
8.245696	582.833175	10.273088
7.930162	579.357612	10.278106
8.038869	571.883453	10.283123
7.992160	577.691161	10.288141
8.338589	585.621088	10.293159
8.406297	599.991504	10.298176
8.378610	599.222699	10.303194
8.684114	599.739750	10.308211
8.245885	608.537398	10.313229
8.477227	601.750913	10.318247
8.172404	597.831856	10.323264
8.231337	606.633658	10.328282
8.195545	598.314282	10.333299
8.258361	594.425986	10.338317
8.106249	598.047464	10.343335
8.280133	602.785514	10.348352
8.447578	605.201901	10.353370
8.370535	596.327255	10.358387
8.283615	602.283282	10.363405
8.420720	596.666588	10.368423
8.387434	599.603575	10.373440
8.519998	616.340163	10.378458
8.594409	620.516290	10.383475
8.523010	623.471875	10.388493
8.816044	614.463497	10.393511
8.497703	600.760402	10.398528
8.783811	605.818540	10.403546
8.862357	595.944373	10.408563
8.591637	602.380478	10.413581
8.708448	583.619890	10.418599
8.492754	596.668244	10.423616
8.148761	587.175866	10.428634
8.321161	597.878614	10.433651
8.051845	612.850955	10.438669
8.324059	613.373223	10.443687
8.530102	619.295977	10.448704
8.429071	621.151672	10.453722
8.704923	620.177517	10.458739
8.521252	631.043372	10.463757
8.961646	626.363762	10.468775
8.948027	631.282676	10.473792
9.357514	625.910475	10.478810
9.446534	623.561258	10.483827
9.096927	623.152159	10.488845
9.182925	602.013744	10.493863
8.900252	593.180785	10.498880
8.783513	597.550958	10.503898
8.938399	596.188659	10.508915
8.746760	600.728358	10.513933
8.827567	600.889296	10.518951
8.923182	596.907498	10.523968
8.768095	595.988240	10.528986
8.973915	594.438080	10.534003
8.637143	610.102641	10.539021
8.719935	605.223446	10.544039
8.882034	594.572483	10.549056
8.359936	592.577796	10.554074
8.780250	599.158093	10.559091
8.735120	598.811743	10.564109
9.076993	594.235940	10.569127
9.058312	591.509126	10.574144
8.651723	597.177567	10.579162
8.819635	594.165897	10.584179
8.772476	601.087682	10.589197
8.607524	599.134866	10.594215
8.906639	594.875031	10.599232
8.827543	592.460640	10.604250
9.152165	588.351445	10.609267
8.734859	597.685452	10.614285
9.085187	592.467697	10.619303
9.087032	600.492646	10.624320
8.511051	594.949810	10.629338
8.802706	600.044947	10.634355
8.615028	615.714555	10.639373
9.117926	624.528857	10.644391
9.349012	623.394458	10.649408
9.110272	621.525784	10.654426
9.149466	617.145723	10.659443
8.693307	607.427911	10.664461
9.213073	612.903877	10.669479
9.041234	620.012462	10.674496
8.982410	615.158608	10.679514
9.271818	613.617440	10.684531
9.186505	608.010345	10.689549
8.864150	602.118499	10.694567
8.695100	604.294118	10.699584
8.944336	620.589552	10.704602
9.431898	623.899372	10.709619
9.247382	632.600475	10.714637
9.004450	618.137625	10.719655
9.337448	613.973463	10.724672
8.938725	613.540502	10.729690
8.960540	616.090161	10.734707
9.188689	618.048914	10.739725
9.251124	625.625724	10.744743
9.483603	617.854442	10.749760
9.023111	605.884063	10.754778
9.321401	610.340691	10.759795
9.008074	616.149159	10.764813
9.262027	612.521246	10.769831
9.316439	614.740750	10.774848
8.973625	617.442213	10.779866
8.956884	618.113896	10.784883
9.070035	622.517484	10.789901
9.090930	620.485054	10.794919
9.569560	620.896086	10.799936
9.486643	622.269260	10.804954
9.623091	623.532324	10.809971
9.353110	612.005463	10.814989
9.333444	610.607395	10.820007
9.226396	605.227769	10.825024
9.288351	593.857194	10.830042
9.348206	594.822989	10.835059
9.126831	605.959823	10.840077
9.153836	615.255783	10.845095
9.359067	613.172381	10.850112
9.196418	616.243248	10.855130
9.397204	619.197212	10.860147
9.293744	628.690345	10.865165
9.053450	620.724892	10.870183
9.412306	625.209903	10.875200
8.967621	635.785297	10.880218
9.219796	622.229483	10.885235
9.267994	626.813662	10.890253
9.311635	623.815146	10.895271
9.441309	626.852837	10.900288
9.367757	620.628512	10.905306
9.762173	623.353322	10.910323
9.592792	623.405136	10.915341
9.136301	623.126394	10.920359
9.300819	614.488447	10.925376
8.935558	622.482561	10.930394
9.229345	618.179375	10.935411
9.411413	632.238408	10.940429
9.470583	648.273313	10.945447
9.373747	655.865623	10.950464
9.631895	651.984579	10.955482
9.622957	639.403784	10.960499
9.474493	643.646395	10.965517
9.488302	653.433592	10.970535
9.559037	647.622154	10.975552
9.713342	653.631921	10.980570
9.715980	651.507674	10.985587
9.658112	648.379892	10.990605
9.506249	651.928758	10.995623
9.807951	638.646039	11.000640
9.483308	649.316241	11.005658
9.768557	648.387950	11.010675
9.643198	656.726345	11.015693
9.484232	656.498816	11.020711
9.748929	649.366258	11.025728
9.526303	651.016945	11.030746
9.825413	643.560260	11.035763
9.852843	652.862484	11.040781
9.640481	651.324191	11.045799
9.753984	652.240557	11.050816
9.922657	653.059917	11.055834
9.457692	638.474047	11.060851
9.035655	637.574523	11.065869
9.068422	640.911422	11.070887
9.738319	649.885764	11.075904
9.596684	653.742298	11.080922
9.592516	646.822281	11.085939
9.456039	647.427519	11.090957
9.296358	647.345269	11.095975
10.172044	650.184027	11.100992
9.904455	651.851226	11.106010
9.873522	644.730276	11.111027
9.683069	644.542394	11.116045
9.528197	656.249510	11.121063
9.768289	661.507378	11.126080
9.878878	671.462459	11.131098
9.782383	672.806206	11.136115
10.388893	673.910418	11.141133
9.720587	667.842379	11.146151
10.206033	662.758068	11.151168
10.072836	654.876806	11.156186
9.693524	651.581636	11.161203
9.897895	651.432879	11.166221
9.808986	652.589243	11.171239
10.091131	648.451975	11.176256
9.703274	640.840994	11.181274
9.981343	652.133134	11.186291
9.979194	651.877879	11.191309
9.783260	645.953587	11.196327
10.135092	646.081528	11.201344
9.943166	648.409060	11.206362
9.918056	650.192902	11.211379
10.172579	648.212227	11.216397
9.757730	637.856763	11.221415
9.982066	654.077234	11.226432
9.855231	664.511325	11.231450
10.079664	657.205191	11.236467
10.143436	674.526971	11.241485
10.208705	672.370818	11.246503
10.546155	665.514034	11.251520
9.942991	664.021192	11.256538
9.725176	651.340571	11.261555
10.099845	661.449930	11.266573
10.167484	672.749808	11.271591
10.220483	676.724175	11.276608
10.435734	678.792253	11.281626
10.063738	662.576018	11.286643
10.270277	657.879392	11.291661
9.975719	655.473505	11.296679
10.148030	659.719509	11.301696
10.531324	666.068945	11.306714
10.114494	659.245137	11.311731
10.051285	657.165921	11.316749
9.873313	676.327548	11.321767
10.154916	678.625073	11.326784
9.940076	675.619710	11.331802
10.153483	684.801293	11.336819
10.335171	672.007570	11.341837
10.376616	681.108796	11.346855
10.479972	677.274091	11.351872
10.448529	678.449855	11.356890
10.265584	680.798074	11.361907
10.430691	678.689394	11.366925
10.199149	673.124124	11.371943
10.295847	678.966201	11.376960
10.357647	683.106449	11.381978
10.285602	683.714216	11.386995
10.292093	675.596462	11.392013
10.165473	686.241972	11.397031
10.723609	672.354158	11.402048
10.658209	683.220448	11.407066
10.555708	678.805768	11.412083
10.590149	674.729395	11.417101
10.330984	660.190158	11.422119
10.390766	653.809231	11.427136
10.321124	663.953493	11.432154
10.368526	674.410783	11.437171
10.352923	680.513454	11.442189
10.460067	685.372436	11.447207
10.579705	686.221570	11.452224
10.395900	683.653159	11.457242
10.578251	680.879054	11.462259
10.614190	670.165762	11.467277
10.273005	676.884335	11.472295
10.401549	680.256728	11.477312
10.472161	677.048850	11.482330
10.039883	681.212861	11.487347
10.561262	679.401811	11.492365
10.061892	684.816572	11.497383
10.429026	669.967758	11.502400
10.588274	674.654471	11.507418
10.425943	668.096900	11.512435
10.513635	676.111588	11.517453
10.477835	678.509337	11.522471
10.252293	673.788886	11.527488
10.736466	673.394317	11.532506
10.142901	674.964269	11.537523
10.556163	685.168581	11.542541
10.810775	698.638786	11.547559
10.807657	697.323326	11.552576
10.815270	699.165162	11.557594
11.008239	698.061977	11.562611
11.154694	685.093883	11.567629
10.438892	680.036833	11.572647
10.475802	675.944294	11.577664
10.563614	674.728198	11.582682
10.488467	678.542762	11.587699
11.021577	687.522776	11.592717
10.173123	697.097957	11.597735
10.482383	693.533946	11.602752
10.686591	696.922890	11.607770
10.634457	703.091252	11.612787
10.459126	701.556620	11.617805
10.594110	699.326424	11.622823
10.638020	698.360203	11.627840
10.957638	704.050595	11.632858
10.697047	696.214521	11.637875
10.847811	711.875368	11.642893
10.720462	713.703638	11.647911
11.030781	705.882252	11.652928
10.566327	709.962947	11.657946
10.989148	708.113688	11.662963
11.036981	699.086881	11.667981
10.459525	703.974236	11.672999
11.007942	706.958955	11.678016
10.975930	708.415678	11.683034
10.956959	715.475103	11.688051
11.009210	709.385672	11.693069
10.771986	718.394878	11.698087
10.927785	718.206394	11.703104
11.177972	723.828775	11.708122
10.956065	728.319600	11.713139
11.066999	716.606756	11.718157
11.202603	719.561482	11.723175
11.090895	710.013708	11.728192
11.116099	709.425961	11.733210
10.831148	708.568071	11.738227
11.258319	704.228186	11.743245
11.046204	715.464624	11.748263
10.761482	716.288752	11.753280
11.035688	719.041879	11.758298
10.848190	721.075235	11.763315
11.111130	722.384760	11.768333
11.335638	727.348442	11.773351
11.264222	722.414480	11.778368
11.378655	723.400133	11.783386
11.198033	730.090412	11.788403
11.182424	719.293649	11.793421
11.127073	721.404130	11.798439
10.838021	718.258908	11.803456
11.009157	721.646727	11.808474
11.033001	718.856426	11.813491
11.054696	717.792698	11.818509
11.152403	725.685918	11.823527
11.311586	719.156849	11.828544
11.160771	722.105958	11.833562
11.257333	720.512945	11.838579
11.579463	718.183996	11.843597
11.551347	720.842480	11.848615
11.364496	729.929007	11.853632
11.538024	719.329829	11.858650
11.109631	724.925986	11.863667
10.904902	720.748220	11.868685
11.294882	722.716343	11.873703
11.300048	727.739638	11.878720
11.354589	732.698394	11.883738
11.176969	733.385821	11.888755
11.390159	721.167799	11.893773
11.480882	728.042783	11.898791
10.994065	731.893456	11.903808
11.394356	720.949477	11.908826
11.392212	727.532896	11.913843
11.509156	728.205728	11.918861
11.295988	719.926710	11.923879
11.039757	726.060785	11.928896
10.997630	722.062671	11.933914
10.869192	747.474618	11.938931
11.325016	760.537800	11.943949
11.621183	762.612145	11.948967
11.465350	758.256294	11.953984
11.450402	751.274809	11.959002
11.333821	763.461993	11.964019
11.950804	748.340437	11.969037
11.644759	755.201857	11.974055
11.683723	757.704668	11.979072
11.612224	753.581759	11.984090
11.408148	768.433554	11.989107
11.801867	760.144638	11.994125
11.883209	756.455377	11.999143
11.756090	756.535284	12.004160
11.740820	750.412236	12.009178
11.903400	751.005335	12.014195
11.770700	744.695559	12.019213
12.060354	757.869982	12.024231
11.737040	747.250802	12.029248
11.600218	735.699842	12.034266
11.585711	742.177905	12.039283
11.556153	742.794796	12.044301
11.721599	754.568554	12.049319
11.687527	752.655176	12.054336
11.939484	752.170756	12.059354
11.712980	760.073763	12.064371
11.832294	754.507145	12.069389
11.589393	756.672262	12.074407
11.890146	758.351409	12.079424
12.001636	746.385993	12.084442
11.838894	754.563032	12.089459
11.906500	756.938277	12.094477
11.751310	758.146058	12.099495
11.733363	754.806873	12.104512
12.010329	745.406468	12.109530
11.957412	752.070435	12.114547
11.811340	748.741858	12.119565
11.843183	755.212664	12.124583
11.739171	753.392296	12.129600
11.470591	748.902632	12.134618
11.792641	751.443140	12.139635
11.987368	752.605563	12.144653
12.283048	758.653176	12.149671
11.700363	755.793797	12.154688
11.997610	750.571690	12.159706
11.924337	758.343390	12.164723
12.239308	752.780830	12.169741
11.725067	753.249598	12.174759
11.746467	758.772136	12.179776
11.957927	750.016315	12.184794
12.036076	757.849497	12.189811
11.458877	745.733206	12.194829
11.904532	747.670518	12.199847
11.824453	760.063421	12.204864
11.754795	773.877982	12.209882
11.953631	778.381793	12.214899
11.998713	790.057667	12.219917
12.402571	776.048777	12.224935
11.877806	780.438742	12.229952
12.200491	778.286426	12.234970
12.066906	783.378814	12.239987
12.077530	781.982299	12.245005
12.187465	776.549688	12.250023
12.062006	783.158760	12.255040
12.627345	777.566433	12.260058
12.169103	783.987802	12.265075
12.005758	779.456396	12.270093
12.365892	779.898622	12.275111
12.142885	781.233796	12.280128
12.482765	769.737513	12.285146
12.383297	780.022215	12.290163
12.244144	783.834206	12.295181
12.611879	786.844092	12.300199
12.646397	782.613047	12.305216
12.617914	775.299155	12.310234
12.329693	778.408659	12.315251
12.597331	776.533214	12.320269
12.533718	769.265854	12.325287
11.979498	770.485663	12.330304
12.638444	766.917342	12.335322
12.207662	780.068959	12.340339
12.229125	772.406412	12.345357
12.530628	779.437740	12.350375
12.509381	782.271884	12.355392
12.400888	778.280999	12.360410
12.605146	784.358725	12.365427
12.050715	783.003405	12.370445
12.438276	781.680376	12.375463
12.352020	781.381492	12.380480
12.275351	776.249520	12.385498
12.481426	770.988043	12.390515
12.477508	776.195813	12.395533
12.912206	768.585289	12.400551
12.770387	785.219857	12.405568
12.658098	772.980212	12.410586
12.698058	781.412685	12.415603
12.468062	784.096497	12.420621
12.599085	768.599779	12.425639
12.733095	771.103479	12.430656
12.454218	783.994610	12.435674
12.434405	785.244299	12.440691
12.457198	785.625769	12.445709
12.853696	779.917883	12.450727
12.198019	783.896011	12.455744
12.622042	770.445704	12.460762
12.518187	779.869551	12.465779
12.258894	780.352023	12.470797
12.536621	776.067094	12.475815
12.416711	786.989326	12.480832
12.873522	796.161232	12.485850
12.755494	799.464982	12.490867
12.882845	802.017067	12.495885
13.107556	799.084828	12.500903
12.636128	797.624982	12.505920
12.729449	795.451796	12.510938
13.104063	787.273158	12.515955
12.786412	780.525284	12.520973
12.766540	784.246002	12.525991
12.641607	787.661287	12.531008
12.888065	786.189950	12.536026
13.064269	791.006583	12.541043
12.714820	788.770225	12.546061
13.139750	792.774707	12.551079
12.994471	791.497293	12.556096
13.215048	793.624511	12.561114
13.216147	784.731217	12.566131
13.142404	772.892636	12.571149
12.861617	765.839187	12.576167
12.414227	771.747606	12.581184
12.755925	776.311085	12.586202
12.910794	789.118481	12.591219
13.209938	794.875227	12.596237
13.454008	793.044499	12.601255
13.024502	805.567922	12.606272
13.104960	802.790829	12.611290
13.363720	790.202699	12.616307
12.927538	781.185413	12.621325
13.015440	774.651713	12.626343
13.154492	796.402076	12.631360
13.162257	796.012720	12.636378
13.036500	799.576461	12.641395
12.969483	800.615794	12.646413
13.217150	795.657064	12.651431
12.799581	794.794701	12.656448
13.040114	795.328251	12.661466
13.566044	800.699167	12.666483
13.395261	799.267957	12.671501
13.513402	798.618307	12.676519
12.879957	805.865563	12.681536
13.340500	799.226130	12.686554
13.213951	802.875203	12.691571
13.196727	797.020692	12.696589
13.226209	794.513521	12.701607
12.864650	794.017928	12.706624
12.782527	795.728665	12.711642
13.164323	801.229463	12.716659
13.098508	800.293052	12.721677
13.091317	791.924923	12.726695
13.412179	812.046809	12.731712
13.548363	809.563944	12.736730
13.811072	801.923548	12.741747
13.585776	793.062565	12.746765
13.644235	795.966274	12.751783
13.637165	806.836123	12.756800
13.480318	800.223995	12.761818
13.184668	795.924755	12.766835
13.017204	796.203490	12.771853
13.386430	778.466667	12.776871
13.214704	797.116199	12.781888
13.263794	802.060050	12.786906
13.416519	814.874112	12.791923
13.492339	819.018506	12.796941
13.367970	811.886882	12.801959
13.442247	823.826451	12.806976
13.235028	823.982025	12.811994
13.838041	821.612210	12.817011
13.432939	820.006270	12.822029
13.850773	819.366469	12.827047
13.815160	832.307884	12.832064
13.536366	819.554645	12.837082
13.624629	828.998910	12.842099
13.426136	833.751183	12.847117
13.521364	821.128693	12.852135
13.550342	826.694246	12.857152
13.446109	825.527165	12.862170
13.734664	817.144244	12.867187
13.613168	833.378037	12.872205
13.546345	833.599978	12.877223
13.501232	828.078034	12.882240
13.339188	824.796127	12.887258
13.890905	829.973662	12.892275
13.506902	840.754265	12.897293
13.736375	846.925893	12.902311
13.892872	854.551179	12.907328
13.663483	856.016749	12.912346
14.155049	848.987424	12.917363
13.840969	847.080037	12.922381
14.104677	834.017723	12.927399
13.964900	841.001450	12.932416
13.627228	859.948451	12.937434
13.878903	849.759836	12.942451
13.921103	849.002161	12.947469
14.061904	854.196748	12.952487
13.839733	850.217347	12.957504
13.811700	846.286425	12.962522
13.989720	849.613229	12.967539
14.131844	852.589046	12.972557
14.090829	843.153203	12.977575
13.980519	841.725138	12.982592
14.128786	836.482166	12.987610
14.257916	841.899487	12.992627
14.051769	839.694319	12.997645
14.284269	841.096986	13.002663
13.773910	848.132466	13.007680
13.995173	845.036656	13.012698
14.425285	838.039054	13.017715
14.201460	850.640737	13.022733
14.197003	843.869015	13.027751
13.967100	844.864443	13.032768
14.166680	843.817018	13.037786
13.996269	840.141939	13.042803
14.283166	842.568045	13.047821
14.440255	847.725363	13.052839
14.054074	841.455269	13.057856
14.094210	848.893654	13.062874
14.232769	844.658917	13.067891
14.173148	848.243863	13.072909
13.971333	850.004917	13.077927
14.091042	851.573582	13.082944
13.990497	840.032649	13.087962
14.207549	847.070925	13.092979
14.422205	867.250540	13.097997
14.383860	870.882651	13.103015
14.475383	863.530985	13.108032
14.407056	858.198864	13.113050
14.420271	854.188894	13.118067
14.394281	853.662812	13.123085
14.297950	857.029447	13.128103
14.559417	863.861951	13.133120
14.391024	876.915722	13.138138
14.755258	866.384409	13.143155
14.695195	863.575673	13.148173
14.552094	846.594406	13.153191
14.355747	848.550266	13.158208
14.087102	850.820415	13.163226
14.502560	857.505712	13.168243
14.465459	865.287570	13.173261
14.531738	866.037775	13.178279
14.431590	869.973063	13.183296
14.650793	880.630777	13.188314
14.689167	874.896920	13.193331
14.623555	870.555308	13.198349
14.545818	874.408189	13.203367
14.738677	867.753867	13.208384
14.602993	872.758246	13.213402
14.658619	866.772376	13.218419
14.799707	879.313748	13.223437
14.758070	872.191229	13.228455
14.709859	875.222119	13.233472
14.533043	876.647894	13.238490
14.829298	871.706778	13.243507
14.985804	871.180505	13.248525
14.405851	874.402007	13.253543
14.623866	866.456156	13.258560
14.468345	876.027005	13.263578
14.647250	870.520443	13.268595
14.679364	878.162072	13.273613
14.485775	878.242926	13.278631
14.718703	877.505861	13.283648
14.772187	888.647144	13.288666
14.715130	891.600526	13.293683
14.598672	899.255974	13.298701
14.811290	896.751654	13.303719
15.287107	894.253434	13.308736
15.225918	897.762895	13.313754
15.521976	898.783218	13.318771
14.964923	887.241196	13.323789
14.738217	880.128735	13.328807
14.828479	889.427549	13.333824
14.828324	896.316836	13.338842
15.292470	897.465459	13.343859
15.356459	905.578640	13.348877
15.142263	901.702121	13.353895
15.073353	905.026598	13.358912
14.979311	900.175029	13.363930
15.036911	897.518269	13.368947
14.909507	903.518609	13.373965
14.930059	894.252977	13.378983
15.105469	895.737178	13.384000
14.800222	902.705828	13.389018
15.202468	898.354023	13.394035
15.083272	899.710811	13.399053
15.161863	894.248362	13.404071
15.124449	899.231039	13.409088
14.927153	898.589783	13.414106
15.119434	896.943886	13.419123
15.343933	898.294162	13.424141
15.467858	903.633421	13.429159
15.225671	895.797531	13.434176
15.303565	894.298948	13.439194
15.173259	893.899664	13.444211
15.752826	891.767048	13.449229
15.357392	899.071724	13.454247
15.377012	890.816114	13.459264
14.992084	900.230413	13.464282
15.163086	898.969709	13.469299
15.218335	905.083446	13.474317
15.385656	917.608112	13.479335
15.764494	905.701688	13.484352
15.522856	920.101894	13.489370
15.164746	914.414366	13.494387
15.682849	916.826348	13.499405
15.551233	915.407926	13.504423
15.695813	918.184551	13.509440
15.719462	921.563957	13.514458
15.985673	913.348598	13.519475
16.193257	900.579057	13.524493
15.418692	890.775276	13.529511
15.785140	892.945924	13.534528
15.294242	891.877291	13.539546
15.235346	889.731098	13.544563
15.529544	897.896571	13.549581
15.428109	909.971026	13.554599
15.997625	913.384828	13.559616
15.963965	919.635578	13.564634
15.620448	901.243432	13.569651
15.740364	899.189144	13.574669
15.575393	900.471052	13.579687
15.724940	898.023952	13.584704
15.893920	919.861296	13.589722
15.642185	926.196711	13.594739
15.794002	923.919668	13.599757
15.659095	920.090683	13.604775
15.846445	913.752793	13.609792
15.522702	925.600154	13.614810
15.411836	926.564312	13.619827
15.774624	921.284549	13.624845
15.603727	920.077412	13.629863
15.600644	918.907100	13.634880
15.695605	929.297126	13.639898
15.794099	924.917166	13.644915
16.053974	920.382531	13.649933
15.768610	923.759860	13.654951
15.740469	934.172333	13.659968
16.054088	942.887059	13.664986
15.903179	943.232631	13.670003
16.094285	949.075783	13.675021
16.189087	950.367487	13.680039
16.223277	940.156091	13.685056
16.171247	942.903562	13.690074
16.284328	943.599099	13.695091
16.227619	946.069588	13.700109
15.901862	949.528992	13.705127
16.200733	944.281327	13.710144
16.229894	945.627498	13.715162
16.261940	943.558570	13.720179
16.081316	950.245776	13.725197
16.110816	950.698783	13.730215
16.453444	945.923954	13.735232
16.441445	949.741305	13.740250
16.199915	948.510519	13.745267
16.357795	949.306336	13.750285
16.218684	952.386196	13.755303
16.498183	944.354936	13.760320
16.276158	946.927068	13.765338
16.657616	940.489327	13.770355
16.307871	939.259717	13.775373
16.108556	942.437371	13.780391
16.260747	939.412328	13.785408
16.090302	949.073919	13.790426
15.955309	947.772790	13.795443
16.737574	942.493570	13.800461
16.236292	951.698904	13.805479
16.433619	945.315257	13.810496
16.626167	945.493405	13.815514
16.343241	947.847857	13.820531
16.524130	942.656548	13.825549
16.484913	954.885391	13.830567
16.549184	941.456608	13.835584
16.501871	945.471999	13.840602
16.762510	942.193273	13.845619
16.615686	946.997442	13.850637
16.703499	950.493036	13.855655
16.908282	943.969364	13.860672
16.751113	949.128611	13.865690
16.576440	943.696360	13.870707
16.575130	944.974720	13.875725
16.459505	946.252056	13.880743
16.635304	947.174456	13.885760
16.518792	944.873179	13.890778
16.966445	944.765199	13.895795
16.460036	949.026095	13.900813
16.381084	951.026689	13.905831
16.541224	942.379803	13.910848
16.515436	948.086521	13.915866
16.556265	968.053639	13.920883
16.760678	968.264643	13.925901
16.832274	966.732325	13.930919
17.409693	966.979563	13.935936
16.652131	969.184316	13.940954
17.044188	967.024264	13.945971
17.159627	965.361999	13.950989
17.219214	969.221787	13.956007
17.177182	953.897194	13.961024
17.125442	940.650693	13.966042
16.867859	945.835140	13.971059
16.878592	935.441225	13.976077
16.704982	946.936868	13.981095
17.166575	954.056794	13.986112
17.149847	963.479709	13.991130
17.158588	954.073883	13.996147
17.205226	952.791634	14.001165
17.288012	952.213792	14.006183
16.450764	948.314960	14.011200
17.074917	959.559382	14.016218
17.017996	962.667392	14.021235
16.928821	961.564216	14.026253
16.839902	968.514776	14.031271
17.218291	961.364282	14.036288
17.502770	970.992478	14.041306
17.376538	960.941907	14.046323
17.366155	953.820769	14.051341
17.287897	961.069464	14.056359
17.404083	962.408313	14.061376
17.004234	968.047410	14.066394
17.422124	967.527519	14.071411
17.745311	963.961273	14.076429
17.360573	972.343611	14.081447
17.502726	963.709000	14.086464
17.437090	964.123264	14.091482
17.165885	970.647940	14.096499
17.589768	965.847751	14.101517
17.463664	969.884960	14.106535
17.552752	966.121858	14.111552
17.492466	959.690205	14.116570
17.736911	967.181837	14.121587
17.684059	960.010546	14.126605
17.516758	970.874041	14.131623
17.697640	962.274389	14.136640
17.559193	967.878842	14.141658
17.438636	964.890217	14.146675
17.640129	969.229555	14.151693
17.139045	969.257599	14.156711
17.375747	966.758964	14.161728
17.644641	963.671449	14.166746
17.639567	964.985115	14.171763
17.710868	956.762403	14.176781
17.529124	964.828904	14.181799
17.601222	961.008503	14.186816
17.819565	957.764805	14.191834
17.295465	966.576081	14.196851
17.599953	954.596066	14.201869
17.464265	959.177583	14.206887
17.663932	960.746353	14.211904
18.008976	972.122879	14.216922
17.521642	980.186773	14.221939
18.057236	978.244077	14.226957
17.839153	990.270590	14.231975
17.884492	982.380145	14.236992
18.174327	979.156800	14.242010
17.606788	992.210075	14.247027
18.091235	976.105526	14.252045
18.017873	987.904231	14.257063
18.224060	985.640753	14.262080
18.296451	977.809189	14.267098
17.704194	980.357281	14.272115
17.684214	968.453340	14.277133
17.830195	981.274891	14.282151
17.822342	980.654443	14.287168
17.781828	985.628163	14.292186
17.831491	995.207954	14.297203
18.014365	987.763027	14.302221
17.954253	980.340396	14.307239
18.014423	984.105420	14.312256
17.697231	982.630860	14.317274
17.540414	994.360592	14.322291
17.935579	1007.180990	14.327309
18.373065	1006.433960	14.332327
18.150345	1009.536397	14.337344
18.676940	1010.182927	14.342362
18.291024	1013.853744	14.347379
18.057747	1004.675163	14.352397
18.368589	1018.307217	14.357415
18.479797	1018.258263	14.362432
18.430096	1008.637497	14.367450
18.354502	1016.337087	14.372467
18.389981	1011.256906	14.377485
18.225436	1014.466996	14.382503
18.359781	1008.175248	14.387520
18.268862	1012.058628	14.392538
18.258767	1016.134476	14.397555
18.270742	1007.968375	14.402573
18.495904	1008.428598	14.407591
18.359068	1010.596063	14.412608
18.607124	1002.304610	14.417626
18.482672	1014.168143	14.422643
18.511787	1001.050943	14.427661
18.417845	1016.545266	14.432679
18.548004	1011.775306	14.437696
18.481643	1003.151255	14.442714
18.409383	1022.164143	14.447731
19.052870	1022.584070	14.452749
18.585246	1013.486384	14.457767
18.524707	1011.413020	14.462784
19.096307	1018.383189	14.467802
18.977026	1025.471076	14.472819
18.883935	1012.076363	14.477837
18.684108	1019.271543	14.482855
18.801756	1002.918320	14.487872
19.084468	1003.666178	14.492890
18.551830	1004.500759	14.497907
18.845332	1004.647311	14.502925
18.742046	1009.716081	14.507943
18.587312	1000.367402	14.512960
18.879879	1012.446468	14.517978
18.955132	1027.791212	14.522995
18.791268	1026.428328	14.528013
18.817036	1023.214790	14.533031
18.932526	1025.948651	14.538048
19.336449	1019.116033	14.543066
19.278907	1025.392654	14.548083
19.045602	1003.208702	14.553101
18.928416	1001.396684	14.558119
18.617927	1011.345344	14.563136
18.931744	1017.103019	14.568154
19.061094	1025.297534	14.573171
19.166285	1029.576235	14.578189
19.195821	1033.813140	14.583207
19.128753	1025.744623	14.588224
19.155452	1026.021342	14.593242
19.142683	1033.518587	14.598259
18.840709	1023.867910	14.603277
18.933071	1028.543105	14.608295
19.049951	1032.349748	14.613312
19.502532	1023.038451	14.618330
19.288093	1030.983869	14.623347
19.425530	1018.723864	14.628365
19.727703	1028.507112	14.633383
19.318270	1031.682989	14.638400
19.933459	1031.331004	14.643418
19.348935	1030.179199	14.648435
19.484201	1024.401710	14.653453
19.504930	1022.703784	14.658471
18.899079	1030.596916	14.663488
19.516553	1029.954232	14.668506
19.466094	1026.345529	14.673523
19.536367	1028.745640	14.678541
19.281301	1031.244063	14.683559
19.110917	1028.790266	14.688576
19.326735	1029.744271	14.693594
19.699176	1031.503734	14.698611
19.776945	1020.837328	14.703629
19.751086	1025.187054	14.708647
19.445197	1033.424519	14.713664
19.680421	1019.972048	14.718682
19.739391	1028.278580	14.723699
19.311185	1028.541364	14.728717
19.538128	1022.231948	14.733735
19.770602	1040.824716	14.738752
19.565461	1045.158354	14.743770
19.726914	1059.580726	14.748787
20.092389	1062.641507	14.753805
20.088585	1051.353531	14.758823
19.775367	1043.850606	14.763840
19.812150	1035.734255	14.768858
19.681102	1037.881880	14.773875
19.749944	1049.137625	14.778893
20.189147	1045.821436	14.783911
19.926687	1048.762844	14.788928
20.140699	1050.547130	14.793946
20.140564	1040.912269	14.798963
20.114646	1035.317825	14.803981
19.886048	1027.908948	14.808999
19.678939	1030.185257	14.814016
20.339448	1034.888205	14.819034
20.069810	1045.335424	14.824051
19.501328	1038.001887	14.829069
20.077343	1044.068793	14.834087
19.910113	1049.649378	14.839104
20.187425	1050.925117	14.844122
19.989051	1053.070670	14.849139
19.945586	1057.524151	14.854157
20.235335	1058.330871	14.859175
19.961447	1054.157550	14.864192
20.149656	1048.248679	14.869210
20.082343	1047.306177	14.874227
20.236019	1051.807666	14.879245
20.257586	1048.863032	14.884263
20.126277	1055.599356	14.889280
20.208701	1042.902974	14.894298
20.546987	1054.318482	14.899315
20.141279	1053.037670	14.904333
20.356896	1047.118193	14.909351
20.076193	1055.717804	14.914368
20.466007	1054.631095	14.919386
20.734000	1064.271392	14.924403
20.389062	1056.410504	14.929421
20.278656	1063.301351	14.934439
20.134536	1064.191829	14.939456
20.430576	1074.039181	14.944474
20.318668	1074.728948	14.949491
20.499937	1075.423274	14.954509
20.642306	1067.643825	14.959527
20.223795	1069.918547	14.964544
20.643257	1067.981414	14.969562
20.633689	1070.573926	14.974579
20.109196	1076.945817	14.979597
20.554673	1073.713849	14.984615
20.087648	1079.464494	14.989632
20.806080	1077.076564	14.994650
20.634908	1084.974200	14.999667
20.600975	1093.481516	15.004685
20.941096	1084.531799	15.009703
20.824785	1097.451334	15.014720
20.772751	1091.210850	15.019738
20.523125	1093.317099	15.024755
20.413540	1108.413154	15.029773
20.974299	1093.618863	15.034791
20.713447	1097.623562	15.039808
21.018025	1097.891460	15.044826
20.836488	1095.688716	15.049843
20.325093	1097.056474	15.054861
20.835837	1090.667852	15.059879
21.119927	1110.931541	15.064896
21.088033	1108.938886	15.069914
21.052154	1116.843741	15.074931
21.343275	1113.411882	15.079949
21.302903	1106.112341	15.084967
21.046719	1092.430688	15.089984
20.744878	1091.285082	15.095002
21.117474	1114.788632	15.100019
21.125073	1110.236670	15.105037
21.336615	1115.038386	15.110055
20.741438	1121.266728	15.115072
21.307701	1111.309550	15.120090
21.219647	1120.592240	15.125107
21.145864	1116.532724	15.130125
21.462031	1117.600403	15.135143
21.434153	1131.979911	15.140160
21.708891	1118.713685	15.145178
21.597594	1108.547079	15.150195
21.451209	1119.959669	15.155213
21.631986	1111.148517	15.160231
21.524425	1114.488556	15.165248
21.557910	1115.752009	15.170266
21.580133	1107.000416	15.175283
21.495234	1109.330173	15.180301
21.932500	1108.182376	15.185319
21.304141	1096.638765	15.190336
21.268325	1102.492275	15.195354
21.668252	1102.164549	15.200371
21.729700	1109.369323	15.205389
22.021794	1101.638986	15.210407
21.537941	1096.725359	15.215424
21.513876	1091.064333	15.220442
21.763274	1095.724409	15.225459
21.684636	1110.578925	15.230477
21.997597	1102.431896	15.235495
21.917489	1104.385350	15.240512
21.666337	1093.697851	15.245530
21.749749	1080.310147	15.250547
21.618431	1094.342905	15.255565
21.977683	1097.442539	15.260583
22.185273	1105.653235	15.265600
21.764105	1093.540663	15.270618
21.752972	1087.918638	15.275635
21.554915	1098.846992	15.280653
21.674011	1101.864330	15.285671
21.738441	1105.032249	15.290688
21.693208	1108.097426	15.295706
21.903242	1108.635764	15.300723
21.837733	1112.433130	15.305741
21.652053	1101.176775	15.310759
21.677440	1105.149252	15.315776
21.590966	1113.197736	15.320794
22.206218	1131.787432	15.325811
22.030227	1138.401396	15.330829
22.248495	1132.535126	15.335847
22.457119	1133.755360	15.340864
22.306831	1133.491749	15.345882
22.566606	1132.598984	15.350899
22.106374	1140.384139	15.355917
22.452033	1135.346846	15.360935
22.681998	1140.555949	15.365952
22.103306	1120.657188	15.370970
22.183513	1121.600887	15.375987
21.962239	1132.293051	15.381005
22.427179	1123.752960	15.386023
22.239131	1134.998513	15.391040
22.093309	1134.153518	15.396058
22.263667	1131.838829	15.401075
22.132931	1135.286647	15.406093
22.683429	1132.675706	15.411111
22.327359	1131.873119	15.416128
22.094124	1133.304598	15.421146
22.186227	1129.724031	15.426163
22.211880	1149.220345	15.431181
22.708211	1152.184899	15.436199
22.591694	1159.092519	15.441216
22.616019	1158.337631	15.446234
23.156497	1160.143365	15.451251
22.503121	1163.944483	15.456269
22.770404	1152.961119	15.461287
22.504773	1167.374750	15.466304
22.925917	1156.730206	15.471322
22.952092	1160.197627	15.476339
23.051527	1156.511762	15.481357
23.408492	1159.479217	15.486375
23.243670	1141.825709	15.491392
22.944805	1127.869840	15.496410
23.118128	1124.980314	15.501427
23.082433	1129.947007	15.506445
23.390264	1125.426899	15.511463
22.997402	1126.274299	15.516480
22.962602	1121.315555	15.521498
22.411033	1119.315956	15.526515
22.755716	1123.295216	15.531533
22.734437	1126.618582	15.536551
23.297179	1129.282384	15.541568
23.014580	1123.469345	15.546586
23.273467	1119.001089	15.551603
22.801711	1124.784049	15.556621
22.911890	1132.148461	15.561639
23.396406	1138.624222	15.566656
23.135167	1141.685378	15.571674
23.153085	1137.261184	15.576691
23.240642	1154.333542	15.581709
23.326531	1148.409110	15.586727
23.398580	1151.326527	15.591744
23.384114	1151.729622	15.596762
23.586002	1152.294485	15.601779
23.416041	1137.639893	15.606797
23.408976	1130.732767	15.611815
23.330432	1134.052484	15.616832
23.346824	1144.240344	15.621850
23.742095	1142.101860	15.626867
23.445978	1144.912853	15.631885
23.501220	1147.618302	15.636903
23.260718	1150.521571	15.641920
23.385197	1147.485055	15.646938
23.628868	1149.046948	15.651955
23.288906	1155.841248	15.656973
23.372740	1151.460374	15.661991
23.626783	1150.473829	15.667008
23.585500	1153.986533	15.672026
23.689858	1154.582456	15.677043
23.566792	1156.391164	15.682061
23.454078	1155.048659	15.687079
23.437743	1158.974034	15.692096
23.370004	1154.386527	15.697114
23.733643	1163.488012	15.702131
23.437735	1173.374515	15.707149
23.894948	1182.865305	15.712167
23.984898	1176.526803	15.717184
23.870763	1189.588080	15.722202
23.882462	1178.761513	15.727219
24.051356	1179.164283	15.732237
23.783511	1182.804012	15.737255
23.689607	1171.886694	15.742272
24.020052	1185.294891	15.747290
24.088302	1180.398882	15.752307
24.184993	1184.770473	15.757325
24.066500	1181.712057	15.762343
24.202675	1177.976248	15.767360
24.334243	1181.957353	15.772378
24.507937	1181.324234	15.777395
24.284982	1175.034758	15.782413
24.150947	1179.511928	15.787431
24.419385	1176.070987	15.792448
24.159905	1169.402216	15.797466
24.459439	1166.922111	15.802483
24.440712	1178.841774	15.807501
24.543257	1168.294479	15.812519
24.734678	1171.171105	15.817536
24.442577	1175.581518	15.822554
24.789158	1176.843258	15.827571
24.125256	1164.008095	15.832589
24.272697	1165.998490	15.837607
24.407397	1171.635952	15.842624
24.462022	1162.734083	15.847642
24.481761	1173.079231	15.852659
24.455494	1169.678153	15.857677
24.423119	1168.648118	15.862695
24.809682	1161.022879	15.867712
24.447119	1173.624434	15.872730
24.420053	1165.401260	15.877747
24.692914	1164.888308	15.882765
24.471328	1164.639023	15.887783
24.352901	1154.811189	15.892800
24.429621	1167.441747	15.897818
24.636717	1164.871981	15.902835
24.580405	1171.681808	15.907853
24.730494	1165.166625	15.912871
25.116706	1170.445934	15.917888
24.827538	1171.128762	15.922906
24.807483	1160.442885	15.927923
24.724152	1167.342153	15.932941
24.909140	1178.160045	15.937959
24.841197	1186.824218	15.942976
25.179617	1192.849503	15.947994
25.285400	1190.383973	15.953011
24.931079	1185.431090	15.958029
24.946786	1200.416071	15.963047
25.117912	1193.787125	15.968064
25.078160	1198.517779	15.973082
25.071827	1196.568447	15.978099
25.004464	1183.305279	15.983117
24.758177	1188.140876	15.988135
25.067363	1192.049972	15.993152
25.026881	1197.598120	15.998170
25.001331	1186.556471	16.003187
25.108526	1190.686569	16.008205
25.083254	1194.932099	16.013223
25.260151	1188.964991	16.018240
24.706164	1192.643243	16.023258
25.213320	1200.302102	16.028275
24.838388	1216.446557	16.033293
25.152366	1217.621887	16.038311
25.472872	1213.020873	16.043328
25.414569	1213.749585	16.048346
25.528917	1208.928399	16.053363
25.398437	1212.287827	16.058381
25.613843	1211.723913	16.063399
25.776367	1207.314916	16.068416
25.447362	1217.023585	16.073434
25.739150	1206.705402	16.078451
25.286264	1219.264335	16.083469
25.435204	1222.968163	16.088487
25.527970	1219.135002	16.093504
25.758378	1235.452883	16.098522
25.910086	1234.479212	16.103539
25.859050	1237.800950	16.108557
25.946923	1237.118157	16.113575
26.058395	1227.342628	16.118592
25.653933	1220.551381	16.123610
25.698000	1226.127318	16.128627
25.967490	1235.142602	16.133645
25.948003	1243.231144	16.138663
26.273658	1241.608503	16.143680
25.928942	1235.852498	16.148698
26.058426	1234.797099	16.153715
26.216558	1239.386303	16.158733
26.219949	1237.899364	16.163751
26.243624	1229.668209	16.168768
25.757405	1221.116147	16.173786
26.199287	1228.526461	16.178803
26.485414	1237.879978	16.183821
26.124838	1234.726934	16.188839
26.654939	1230.973578	16.193856
25.894647	1229.148684	16.198874
26.232554	1223.572919	16.203891
26.424678	1227.613976	16.208909
25.913907	1234.554993	16.213927
26.162222	1219.342477	16.218944
26.036536	1229.811432	16.223962
25.992887	1230.133891	16.228979
26.177365	1226.131719	16.233997
25.908792	1232.507750	16.239015
26.186922	1224.243043	16.244032
26.349632	1242.799614	16.249050
26.349016	1247.827117	16.254067
26.800699	1261.112230	16.259085
26.606370	1259.649956	16.264103
26.720750	1257.760603	16.269120
26.558051	1260.689570	16.274138
26.631536	1263.306968	16.279155
26.838614	1261.848076	16.284173
26.592559	1261.078741	16.289191
26.928446	1264.683857	16.294208
26.544219	1260.019671	16.299226
26.631906	1257.354989	16.304243
26.737079	1254.611824	16.309261
26.743162	1264.867643	16.314279
26.617029	1254.393997	16.319296
26.895897	1253.861166	16.324314
26.760250	1257.278218	16.329331
26.711634	1259.611778	16.334349
26.231935	1264.566020	16.339367
26.666376	1257.315105	16.344384
26.919384	1278.959835	16.349402
27.096419	1281.068688	16.354419
27.324413	1285.306117	16.359437
27.255439	1286.181677	16.364455
27.206342	1278.343769	16.369472
27.117570	1276.855487	16.374490
27.037161	1281.333747	16.379507
27.287802	1284.163242	16.384525
26.973886	1276.319487	16.389543
27.439983	1283.473556	16.394560
27.201349	1286.913061	16.399578
27.243199	1283.864221	16.404595
27.223468	1278.524361	16.409613
27.244831	1280.057978	16.414631
26.943052	1281.550703	16.419648
27.388171	1296.405366	16.424666
27.280373	1278.162098	16.429683
27.877245	1284.311029	16.434701
27.831506	1285.599530	16.439719
27.816345	1283.537959	16.444736
27.604168	1287.582413	16.449754
27.452748	1283.367759	16.454771
27.583242	1281.150818	16.459789
27.264512	1286.357567	16.464807
27.388028	1282.254477	16.469824
27.822231	1280.195087	16.474842
27.453630	1282.812323	16.479859
27.616645	1277.424895	16.484877
27.494240	1301.668991	16.489895
27.583936	1311.040700	16.494912
27.801430	1307.591937	16.499930
28.040066	1310.243428	16.504947
28.166439	1302.567373	16.509965
27.911750	1313.280660	16.514983
27.887317	1312.208345	16.520000
28.092712	1303.841383	16.525018
28.248156	1303.747627	16.530035
28.229873	1298.937730	16.535053
27.852767	1309.357758	16.540071
28.283394	1308.671755	16.545088
28.358250	1303.837796	16.550106
28.211705	1311.921029	16.555123
28.336901	1294.610109	16.560141
28.203935	1280.031659	16.565159
27.930993	1275.656158	16.570176
28.086517	1291.673387	16.575194
27.948725	1305.158193	16.580211
28.158180	1297.450187	16.585229
27.815528	1304.901398	16.590247
28.269757	1302.397038	16.595264
28.156206	1303.364793	16.600282
27.861506	1295.836768	16.605299
28.115448	1304.911330	16.610317
28.054328	1315.127212	16.615335
27.980851	1326.506419	16.620352
28.543605	1330.887078	16.625370
28.224987	1339.508545	16.630387
28.767468	1332.628852	16.635405
28.531781	1329.099603	16.640423
28.279124	1332.108951	16.645440
28.529623	1330.302410	16.650458
28.472162	1334.698190	16.655475
28.704526	1326.986582	16.660493
28.653974	1333.192785	16.665511
28.975292	1343.891584	16.670528
29.075052	1358.828812	16.675546
28.975216	1346.283853	16.680563
28.742798	1330.221874	16.685581
29.089573	1323.833614	16.690599
28.670467	1327.263532	16.695616
28.868161	1336.012394	16.700634
28.818677	1346.504193	16.705651
29.494686	1353.669584	16.710669
29.164177	1347.318001	16.715687
29.427417	1341.441460	16.720704
29.107483	1330.212307	16.725722
28.845407	1330.007235	16.730739
29.080795	1336.159170	16.735757
28.879076	1349.470980	16.740775
28.950469	1359.057030	16.745792
29.325076	1348.173501	16.750810
29.293061	1356.911024	16.755827
29.695083	1354.995530	16.760845
29.208651	1355.415769	16.765863
29.182836	1346.400175	16.770880
29.308908	1342.539677	16.775898
29.190532	1354.014303	16.780915
29.585515	1351.617053	16.785933
29.724302	1347.805057	16.790951
29.685468	1346.201643	16.795968
29.969524	1353.071824	16.800986
29.780766	1353.521167	16.806003
29.375467	1338.111143	16.811021
29.582335	1347.568658	16.816039
29.321745	1351.882654	16.821056
29.591783	1344.827883	16.826074
29.889122	1348.038252	16.831091
29.418328	1347.581847	16.836109
29.297660	1345.656725	16.841127
29.061612	1334.499636	16.846144
29.547450	1354.419554	16.851162
29.331328	1369.990132	16.856179
30.017835	1363.441328	16.861197
29.984311	1368.773835	16.866215
30.241201	1364.466785	16.871232
30.284450	1363.118763	16.876250
30.363329	1364.583413	16.881267
30.756782	1357.973224	16.886285
30.471310	1344.182352	16.891303
30.312191	1338.233126	16.896320
30.242132	1330.786660	16.901338
29.835313	1342.177077	16.906355
30.171087	1332.104405	16.911373
30.158501	1334.738455	16.916391
30.229910	1337.870606	16.921408
30.444255	1330.878218	16.926426
30.451937	1331.940593	16.931443
30.404424	1331.853388	16.936461
30.624911	1337.411187	16.941479
30.594908	1332.918710	16.946496
30.603971	1333.573754	16.951514
29.995829	1332.706505	16.956531
30.364843	1329.372859	16.961549
30.711350	1330.161232	16.966567
30.378988	1334.363388	16.971584
30.468316	1336.340816	16.976602
30.370024	1332.266154	16.981619
30.583704	1332.384189	16.986637
30.681084	1336.881947	16.991655
30.626720	1347.926800	16.996672
30.772555	1354.853353	17.001690
30.719460	1362.505384	17.006707
30.963382	1356.518251	17.011725
30.995347	1362.108751	17.016743
30.767999	1353.885310	17.021760
30.683967	1353.617626	17.026778
30.849181	1356.040778	17.031795
30.784882	1357.840298	17.036813
30.594621	1364.718524	17.041831
30.822329	1357.761902	17.046848
30.758440	1351.889273	17.051866
30.622349	1355.760869	17.056883
30.715532	1357.949143	17.061901
30.797489	1356.257372	17.066919
30.935458	1381.483305	17.071936
31.398215	1377.352289	17.076954
31.056688	1389.606702	17.081971
31.506375	1381.857866	17.086989
31.459470	1383.765121	17.092007
31.566365	1382.722721	17.097024
31.492018	1375.930187	17.102042
31.614724	1384.798124	17.107059
31.372943	1367.973839	17.112077
31.226087	1364.686297	17.117095
31.273598	1368.516505	17.122112
31.476091	1366.389263	17.127130
31.215396	1377.974569	17.132147
31.196720	1372.022263	17.137165
31.462983	1376.588248	17.142183
31.496763	1372.126796	17.147200
31.816130	1374.535265	17.152218
31.868718	1368.852673	17.157235
31.580619	1369.304957	17.162253
31.781616	1363.747444	17.167271
31.744638	1370.207164	17.172288
31.952575	1377.745716	17.177306
31.836502	1381.399577	17.182323
31.699278	1375.759346	17.187341
31.985234	1374.767789	17.192359
31.906079	1379.946497	17.197376
31.754474	1376.306230	17.202394
31.736580	1379.067356	17.207411
31.733487	1380.914096	17.212429
31.826224	1390.417920	17.217447
32.052052	1394.930282	17.222464
32.309874	1405.247730	17.227482
32.187448	1410.903462	17.232499
32.205912	1401.962956	17.237517
32.200046	1401.433706	17.242535
32.214510	1412.483594	17.247552
32.267666	1408.448306	17.252570
32.350245	1403.158654	17.257587
32.196526	1400.534929	17.262605
32.254550	1403.034844	17.267623
32.026865	1401.050740	17.272640
32.262573	1408.281984	17.277658
32.190476	1405.124738	17.282675
32.166428	1404.992829	17.287693
32.136762	1399.610306	17.292711
32.222683	1418.251677	17.297728
32.358017	1423.702919	17.302746
32.407446	1427.977828	17.307763
32.458834	1436.042729	17.312781
32.962594	1426.773700	17.317799
32.397298	1427.547139	17.322816
32.679878	1424.533145	17.327834
32.608367	1425.768887	17.332851
32.596671	1425.338383	17.337869
32.474652	1420.759311	17.342887
32.450494	1436.261999	17.347904
32.896575	1449.860570	17.352922
33.166550	1445.295818	17.357939
33.162784	1463.474739	17.362957
33.031478	1451.991882	17.367975
32.871358	1455.103522	17.372992
32.819765	1450.115758	17.378010
33.027174	1452.289303	17.383027
33.100025	1447.831178	17.388045
33.031370	1445.923144	17.393063
32.958305	1449.623931	17.398080
33.085384	1443.326857	17.403098
33.001456	1453.981914	17.408115
33.241062	1441.860254	17.413133
33.061874	1440.717499	17.418151
33.193054	1460.686791	17.423168
33.700045	1474.288462	17.428186
33.241590	1476.111878	17.433203
33.415506	1480.402010	17.438221
34.042944	1475.554015	17.443239
33.898142	1471.578131	17.448256
33.570391	1457.983153	17.453274
33.694122	1459.668013	17.458291
33.551782	1448.199511	17.463309
33.699147	1453.140767	17.468327
33.562354	1459.909662	17.473344
33.446798	1472.804102	17.478362
33.774883	1473.197717	17.483379
33.883614	1473.837150	17.488397
33.999253	1464.944508	17.493415
34.417958	1459.012012	17.498432
34.469208	1444.660196	17.503450
34.940274	1427.140317	17.508467
34.287060	1420.476334	17.513485
34.547298	1427.896255	17.518503
34.671001	1413.365847	17.523520
34.540433	1408.968007	17.528538
34.344014	1396.898912	17.533555
34.242839	1396.444557	17.538573
34.644453	1384.875090	17.543591
34.225296	1386.455645	17.548608
34.286236	1398.110496	17.553626
34.552076	1388.973442	17.558643
34.134624	1389.285040	17.563661
34.124202	1378.386075	17.568679
34.079916	1381.476398	17.573696
34.251497	1379.735868	17.578714
34.153201	1385.299444	17.583731
34.246718	1398.596594	17.588749
34.563001	1401.614648	17.593767
34.393088	1412.109575	17.598784
34.510462	1414.732742	17.603802
34.820503	1409.467413	17.608819
34.423469	1413.259979	17.613837
34.446555	1414.130588	17.618855
34.474033	1422.915630	17.623872
34.537580	1416.726354	17.628890
34.626065	1412.685529	17.633907
34.712791	1418.586218	17.638925
34.487977	1412.994414	17.643943
34.704257	1427.402180	17.648960
35.015080	1426.356230	17.653978
34.944174	1437.299584	17.658995
34.775295	1430.521840	17.664013
34.937553	1432.655118	17.669031
35.039089	1442.548929	17.674048
35.035576	1435.600101	17.679066
35.241867	1437.660205	17.684083
34.948002	1435.932631	17.689101
35.481640	1427.507871	17.694119
35.378924	1441.694217	17.699136
35.118664	1430.989006	17.704154
35.328577	1428.159974	17.709171
35.083892	1433.620264	17.714189
35.445252	1433.623639	17.719207
34.939866	1438.310540	17.724224
35.112755	1433.098253	17.729242
34.990596	1442.496912	17.734259
35.133968	1454.356645	17.739277
35.663578	1454.630319	17.744295
35.551125	1465.169925	17.749312
35.986195	1458.628921	17.754330
35.736125	1462.439498	17.759347
35.549331	1462.588720	17.764365
35.410482	1458.267908	17.769383
35.486540	1452.534273	17.774400
35.414918	1455.701479	17.779418
35.652713	1455.556948	17.784435
35.782102	1462.413533	17.789453
35.748940	1469.159883	17.794471
35.830851	1494.539933	17.799488
35.920818	1488.393832	17.804506
35.814263	1480.072509	17.809523
35.932562	1489.196821	17.814541
36.176917	1485.996292	17.819559
36.027674	1486.830785	17.824576
35.889943	1487.338412	17.829594
36.113903	1483.178511	17.834611
35.707232	1488.683132	17.839629
35.606873	1479.960031	17.844647
35.868380	1500.259260	17.849664
35.855221	1505.538122	17.854682
35.977770	1501.239463	17.859699
36.187842	1520.145525	17.864717
36.336770	1512.115535	17.869735
36.231574	1514.991350	17.874752
36.320959	1533.345106	17.879770
36.841512	1540.822124	17.884787
36.860713	1539.828170	17.889805
36.960176	1527.321289	17.894823
36.600114	1514.324652	17.899840
36.360208	1518.357722	17.904858
36.865138	1521.753359	17.909875
36.939539	1537.319592	17.914893
37.209118	1528.633185	17.919911
37.121732	1516.442780	17.924928
36.611361	1508.396161	17.929946
37.061466	1509.685890	17.934963
36.763395	1506.087481	17.939981
36.863358	1501.571443	17.944999
37.052735	1510.059749	17.950016
36.949699	1526.171350	17.955034
37.472659	1526.695389	17.960051
36.922132	1527.450738	17.965069
37.255094	1525.167331	17.970087
37.587533	1537.417240	17.975104
36.824060	1520.885999	17.980122
36.781281	1528.028373	17.985139
36.902461	1537.385800	17.990157
37.125109	1536.281071	17.995175
37.369003	1530.366473	18.000192
37.273741	1531.785833	18.005210
37.134960	1527.752187	18.010227
37.388199	1534.191743	18.015245
37.389369	1537.360182	18.020263
37.726188	1547.488601	18.025280
37.564359	1558.506237	18.030298
38.071634	1562.999794	18.035315
37.895168	1551.053709	18.040333
37.856013	1547.733478	18.045351
37.734949	1532.887854	18.050368
37.347475	1536.173992	18.055386
37.905012	1544.620412	18.060403
37.618434	1555.714399	18.065421
38.307783	1554.886861	18.070439
37.925979	1562.031871	18.075456
37.852713	1562.920740	18.080474
38.094105	1551.092232	18.085491
37.873522	1562.936474	18.090509
38.143954	1566.889596	18.095527
38.262431	1560.461278	18.100544
38.160455	1565.031355	18.105562
38.244202	1562.761741	18.110579
38.334022	1561.835621	18.115597
38.392650	1566.128058	18.120615
38.628210	1566.394153	18.125632
38.291214	1568.488898	18.130650
38.309451	1552.939742	18.135667
38.169267	1569.909315	18.140685
38.377201	1566.121155	18.145703
38.473776	1555.325246	18.150720
38.250688	1554.407124	18.155738
38.680777	1555.699992	18.160755
38.417908	1557.483304	18.165773
38.676346	1570.013088	18.170791
38.652391	1582.751237	18.175808
38.812400	1577.613512	18.180826
38.642771	1581.323144	18.185843
38.663430	1582.979980	18.190861
38.899153	1583.561649	18.195879
39.014643	1579.469216	18.200896
38.765145	1587.051123	18.205914
39.188138	1580.486720	18.210931
38.987687	1593.385080	18.215949
38.927241	1582.976693	18.220967
38.854363	1590.152212	18.225984
38.706756	1597.989573	18.231002
38.588291	1582.654324	18.236019
39.263471	1596.684198	18.241037
39.240501	1602.529547	18.246055
39.445010	1606.663430	18.251072
39.326578	1614.811826	18.256090
39.308391	1609.165495	18.261107
38.921490	1612.369501	18.266125
39.206346	1615.954281	18.271143
39.195019	1607.933576	18.276160
39.276487	1604.657555	18.281178
39.402915	1602.024623	18.286195
39.398815	1612.951305	18.291213
39.342568	1607.203634	18.296231
39.650831	1611.078252	18.301248
39.431092	1627.867829	18.306266
39.769067	1629.481266	18.311283
39.375043	1634.084494	18.316301
39.350608	1636.865620	18.321319
39.756956	1636.830388	18.326336
39.762732	1629.715917	18.331354
39.711503	1633.631084	18.336371
39.973014	1635.736212	18.341389
39.741411	1632.790120	18.346407
40.302485	1642.956045	18.351424
40.051074	1663.354757	18.356442
40.246852	1657.119433	18.361459
40.212036	1661.821032	18.366477
40.521325	1660.005247	18.371495
40.392807	1641.651239	18.376512
40.406457	1641.055804	18.381530
40.623629	1630.143119	18.386547
40.282110	1635.498714	18.391565
40.284305	1635.760346	18.396583
40.732780	1637.757281	18.401600
40.274878	1644.008478	18.406618
40.523539	1655.542561	18.411635
40.463552	1653.421695	18.416653
40.587385	1656.195374	18.421671
40.677572	1644.901765	18.426688
40.635562	1653.072921	18.431706
40.650198	1654.143694	18.436723
40.785240	1649.701023	18.441741
40.729473	1657.767033	18.446759
41.040094	1651.791444	18.451776
40.867060	1657.167988	18.456794
40.776914	1651.561321	18.461811
40.849104	1646.289005	18.466829
40.654203	1645.300186	18.471847
41.149622	1646.544954	18.476864
41.285538	1658.125108	18.481882
41.203654	1655.906681	18.486899
41.211365	1662.694039	18.491917
41.472034	1667.557639	18.496935
41.783501	1665.457473	18.501952
41.096753	1656.447440	18.506970
41.236150	1650.359815	18.511987
41.579648	1662.557582	18.517005
41.497166	1668.816244	18.522023
41.729016	1662.376438	18.527040
41.242090	1666.293600	18.532058
41.633021	1667.983955	18.537075
41.496814	1665.433191	18.542093
41.520878	1669.702664	18.547111
41.831021	1657.405695	18.552128
41.751584	1663.139983	18.557146
41.647602	1660.369562	18.562163
41.910285	1664.203993	18.567181
41.662882	1664.807707	18.572199
42.290344	1652.255886	18.577216
41.938364	1660.112671	18.582234
41.836381	1669.404140	18.587251
42.116628	1672.579374	18.592269
41.974045	1663.297876	18.597287
42.404563	1657.540200	18.602304
41.916786	1669.151803	18.607322
41.928674	1655.594984	18.612339
42.137271	1660.337346	18.617357
41.959094	1658.869351	18.622375
42.486155	1655.072200	18.627392
42.327736	1664.400913	18.632410
42.279921	1669.836741	18.637427
42.260944	1664.484023	18.642445
41.998904	1685.367293	18.647463
42.462210	1679.976880	18.652480
42.783775	1696.438701	18.657498
43.058213	1691.538652	18.662515
42.578869	1689.919012	18.667533
42.490252	1685.536623	18.672551
42.874169	1672.783090	18.677568
42.824589	1685.815677	18.682586
42.728789	1679.742801	18.687603
42.867425	1692.307221	18.692621
42.765487	1677.098698	18.697639
43.064219	1671.355353	18.702656
42.685647	1684.007114	18.707674
42.543307	1678.948292	18.712691
42.604900	1683.309724	18.717709
42.974759	1690.965060	18.722727
43.406211	1702.612555	18.727744
43.104092	1727.002155	18.732762
43.319036	1707.278214	18.737779
43.066595	1707.889030	18.742797
43.145231	1712.421379	18.747815
42.930982	1706.019892	18.752832
42.921822	1709.294128	18.757850
42.804453	1711.673234	18.762867
43.602900	1718.778564	18.767885
43.317271	1730.314351	18.772903
43.419000	1728.054523	18.777920
43.631028	1733.645331	18.782938
43.548742	1736.940497	18.787955
43.309390	1737.707064	18.792973
43.514866	1737.561283	18.797991
43.530322	1735.924080	18.803008
43.598653	1738.157323	18.808026
43.649411	1757.123313	18.813043
43.995163	1750.050209	18.818061
43.757835	1758.116306	18.823079
44.075798	1750.097597	18.828096
43.967140	1755.180043	18.833114
44.005153	1755.101528	18.838131
44.387998	1750.493767	18.843149
44.503873	1754.628947	18.848167
44.354367	1753.623542	18.853184
44.321907	1747.187245	18.858202
44.690742	1753.258453	18.863219
44.668065	1750.595208	18.868237
44.382709	1755.370802	18.873255
44.597018	1750.192961	18.878272
44.442847	1746.313164	18.883290
44.496454	1745.238064	18.888307
44.819231	1745.578866	18.893325
44.028175	1742.619417	18.898343
44.809614	1742.001520	18.903360
44.502959	1745.483329	18.908378
44.489849	1747.451604	18.913395
44.378362	1754.980399	18.918413
44.189814	1767.611914	18.923431
44.711014	1766.558232	18.928448
44.848926	1782.499760	18.933466
44.763333	1770.996912	18.938483
44.988976	1774.840326	18.943501
44.496006	1779.481185	18.948519
45.173614	1787.624867	18.953536
45.097262	1796.820861	18.958554
45.568411	1795.456262	18.963571
45.438467	1781.659621	18.968589
45.287041	1787.275830	18.973607
45.219397	1790.189991	18.978624
45.039698	1789.833140	18.983642
45.492101	1797.270448	18.988659
45.698816	1792.510379	18.993677
45.490033	1803.431374	18.998695
45.848633	1789.725452	19.003712
45.847813	1800.942087	19.008730
45.437030	1789.578545	19.013747
45.877378	1791.153865	19.018765
45.464889	1790.483170	19.023783
45.592126	1797.160328	19.028800
45.583341	1794.760006	19.033818
45.551890	1785.451564	19.038835
45.544123	1793.005152	19.043853
45.822360	1807.491886	19.048871
45.901852	1819.734280	19.053888
46.340087	1818.687282	19.058906
46.622808	1819.283687	19.063923
46.510640	1808.258382	19.068941
46.305333	1801.950139	19.073959
46.507653	1792.706060	19.078976
46.219960	1788.234907	19.083994
46.272900	1795.558064	19.089011
46.703069	1800.581349	19.094029
46.194521	1807.680037	19.099047
46.710617	1809.776858	19.104064
46.450207	1817.111245	19.109082
46.675070	1817.379022	19.114099
46.933841	1812.351998	19.119117
46.820974	1811.716415	19.124135
46.678162	1805.669797	19.129152
46.651682	1821.744421	19.134170
46.449458	1810.767940	19.139187
46.943253	1803.728428	19.144205
46.947935	1808.010439	19.149223
46.976782	1802.072637	19.154240
46.936469	1807.703004	19.159258
46.931734	1814.546022	19.164275
47.117590	1812.752717	19.169293
47.078124	1812.620065	19.174311
47.017912	1811.158823	19.179328
47.107847	1804.659146	19.184346
46.913520	1821.350242	19.189363
47.599278	1828.198698	19.194381
47.207883	1836.077515	19.199399
47.579007	1827.731685	19.204416
47.741492	1832.642274	19.209434
47.896660	1830.563422	19.214451
47.550307	1825.435530	19.219469
47.553133	1835.354491	19.224487
47.418759	1831.272745	19.229504
48.214823	1832.262125	19.234522
47.749212	1838.694490	19.239539
47.831845	1827.528190	19.244557
47.436898	1826.450775	19.249575
47.393895	1828.253317	19.254592
47.669536	1831.025331	19.259610
47.301297	1833.484787	19.264627
47.564536	1836.435481	19.269645
47.938197	1850.209819	19.274663
48.064404	1860.447158	19.279680
48.159367	1854.811426	19.284698
47.870206	1861.405514	19.289715
48.232539	1857.798244	19.294733
48.153978	1851.069311	19.299751
47.870196	1854.828444	19.304768
47.955104	1863.308037	19.309786
47.686804	1885.347625	19.314803
48.193082	1880.325989	19.319821
48.170457	1889.548329	19.324839
48.246127	1881.816850	19.329856
48.428946	1892.310444	19.334874
48.390554	1899.023058	19.339891
48.200411	1904.345547	19.344909
48.599427	1908.736225	19.349927
48.799117	1908.395676	19.354944
49.180756	1906.432822	19.359962
48.800639	1908.019927	19.364979
48.780793	1899.050460	19.369997
49.276522	1899.932255	19.375015
49.277775	1900.364464	19.380032
49.240236	1899.376224	19.385050
48.954985	1898.149063	19.390067
48.783136	1904.137765	19.395085
49.023179	1921.584624	19.400103
49.030207	1923.527671	19.405120
49.192055	1921.580315	19.410138
49.197987	1925.287759	19.415155
49.466667	1926.571229	19.420173
49.700171	1927.762372	19.425191
49.694845	1920.586406	19.430208
49.623638	1914.777859	19.435226
49.906586	1922.639430	19.440243
49.670319	1914.009999	19.445261
49.586488	1923.387124	19.450279
49.483904	1933.442584	19.455296
50.053216	1947.956416	19.460314
50.088687	1943.545054	19.465331
50.292492	1947.183628	19.470349
50.331220	1948.676709	19.475367
49.917824	1948.302817	19.480384
50.173289	1936.190964	19.485402
50.248009	1947.705148	19.490419
50.480944	1942.114049	19.495437
50.533049	1944.687556	19.500455
50.516333	1939.949830	19.505472
50.899158	1933.479962	19.510490
50.719504	1940.088482	19.515507
50.852990	1925.710774	19.520525
50.396695	1915.424179	19.525543
50.618329	1908.670283	19.530560
50.922156	1909.032994	19.535578
50.370317	1921.330188	19.540595
50.964972	1927.558593	19.545613
51.135111	1921.664890	19.550631
51.063795	1933.416556	19.555648
51.197179	1922.024480	19.560666
50.714408	1913.730338	19.565683
50.945284	1919.539174	19.570701
51.268729	1929.272245	19.575719
51.134643	1937.454800	19.580736
51.334292	1930.136253	19.585754
51.140896	1930.185519	19.590771
50.972958	1925.566171	19.595789
51.310749	1928.230626	19.600807
51.215439	1924.379440	19.605824
51.227070	1923.541297	19.610842
51.084277	1934.792884	19.615859
50.996651	1918.142760	19.620877
50.590038	1939.528693	19.625895
50.893284	1948.119296	19.630912
51.511187	1945.324099	19.635930
51.625384	1955.178337	19.640947
51.337533	1957.003474	19.645965
51.640985	1963.899257	19.650983
51.491674	1970.414665	19.656000
51.917686	1973.497682	19.661018
51.742547	1993.341979	19.666035
52.011159	1991.554627	19.671053
52.045771	1982.866942	19.676071
52.169504	1984.785399	19.681088
52.179973	1983.486652	19.686106
52.390377	1985.707135	19.691123
52.557116	1988.972799	19.696141
52.573676	1985.770000	19.701159
52.340453	1976.183779	19.706176
52.078372	1977.638779	19.711194
52.243848	1987.283013	19.716211
52.089497	1979.467601	19.721229
52.261518	1986.084160	19.726247
52.146939	2002.570411	19.731264
52.648938	2004.631592	19.736282
52.816661	2013.208743	19.741299
52.790734	2008.264143	19.746317
53.424911	2003.765275	19.751335
52.765016	2004.556713	19.756352
53.359539	2004.854945	19.761370
52.666224	2010.821233	19.766387
53.032174	2008.990225	19.771405
53.209029	2002.943954	19.776423
53.074378	2002.832525	19.781440
53.291436	1995.388138	19.786458
53.382730	1999.877548	19.791475
53.177533	1986.480733	19.796493
53.160311	2001.597785	19.801511
53.161035	1991.312132	19.806528
53.502185	2001.828325	19.811546
53.444034	2008.231626	19.816563
53.514671	2017.420484	19.821581
53.688456	2018.371662	19.826599
53.720119	2022.860952	19.831616
53.728402	2015.231500	19.836634
53.581626	2014.746400	19.841651
53.599626	2020.225676	19.846669
53.735129	2016.376180	19.851687
53.595549	2021.198437	19.856704
53.877692	2021.687635	19.861722
53.802598	2037.353469	19.866739
53.873314	2042.104910	19.871757
54.244305	2045.398549	19.876775
54.012552	2049.998550	19.881792
54.153544	2045.876768	19.886810
54.186121	2041.046079	19.891827
54.375194	2039.040792	19.896845
54.459634	2037.970312	19.901863
54.465501	2040.951897	19.906880
54.639684	2038.538655	19.911898
54.672276	2041.172043	19.916915
54.725076	2052.206852	19.921933
54.930880	2057.208553	19.926951
54.644562	2049.748329	19.931968
55.006861	2053.942808	19.936986
55.261990	2069.923036	19.942003
54.729570	2057.060314	19.947021
55.017731	2057.936765	19.952039
55.315612	2068.920562	19.957056
55.621049	2062.011456	19.962074
55.073403	2049.621378	19.967091
55.063685	2036.026628	19.972109
55.095345	2043.305879	19.977127
54.973358	2055.548441	19.982144
55.077750	2054.399088	19.987162
55.326055	2072.895769	19.992179
55.259660	2063.024566	19.997197
55.344394	2066.505081	20.002215
55.103048	2068.019961	20.007232
55.248816	2065.910994	20.012250
55.554649	2082.618652	20.017267
55.649835	2085.535753	20.022285
55.730739	2081.903098	20.027303
55.644915	2092.691385	20.032320
55.656223	2088.217496	20.037338
55.986498	2074.241217	20.042355
55.980703	2087.699618	20.047373
55.848023	2084.286634	20.052391
56.184804	2082.564339	20.057408
56.232131	2088.487202	20.062426
56.429564	2096.318062	20.067443
56.198167	2106.838807	20.072461
56.661751	2104.386527	20.077479
56.515923	2118.059410	20.082496
56.603293	2106.204172	20.087514
56.363657	2109.435689	20.092531
56.367631	2110.637558	20.097549
56.786981	2109.079064	20.102567
56.702819	2110.547228	20.107584
56.268642	2103.529904	20.112602
56.338803	2101.685264	20.117619
56.511560	2109.191765	20.122637
56.898618	2116.977145	20.127655
56.966066	2123.767942	20.132672
57.255420	2140.250999	20.137690
57.041943	2130.345994	20.142707
56.901625	2129.787290	20.147725
57.321204	2125.845923	20.152743
56.920697	2131.567542	20.157760
56.747829	2137.439705	20.162778
56.844198	2136.708207	20.167795
57.238420	2148.794209	20.172813
57.381647	2154.124506	20.177831
57.245639	2161.004003	20.182848
57.208290	2151.068236	20.187866
57.484044	2154.067520	20.192883
57.329155	2153.530035	20.197901
57.270935	2173.772814	20.202919
57.727173	2171.886615	20.207936
57.949806	2180.707730	20.212954
58.040410	2183.799149	20.217971
57.634065	2185.990043	20.222989
58.212494	2173.969453	20.228007
58.111502	2173.767536	20.233024
58.152195	2169.835024	20.238042
58.427906	2173.137302	20.243059
58.267701	2176.807706	20.248077
58.643058	2169.458377	20.253095
58.462090	2176.325988	20.258112
58.633596	2176.917739	20.263130
58.609931	2163.167274	20.268147
58.478577	2187.928410	20.273165
58.679897	2186.063213	20.278183
58.443927	2197.373748	20.283200
58.616078	2195.604645	20.288218
58.798564	2195.222602	20.293235
58.636458	2196.911286	20.298253
58.821791	2191.690518	20.303271
58.743854	2193.126152	20.308288
58.794859	2198.332043	20.313306
59.121404	2195.680296	20.318323
59.085100	2202.282233	20.323341
59.242895	2207.815409	20.328359
59.620051	2216.356688	20.333376
59.389696	2220.931265	20.338394
59.719562	2215.495324	20.343411
59.498321	2204.625731	20.348429
59.751060	2205.056419	20.353447
59.475672	2205.699251	20.358464
59.852471	2207.890536	20.363482
60.127000	2210.350331	20.368499
59.623711	2200.222426	20.373517
59.960091	2201.457436	20.378535
60.167752	2208.753365	20.383552
59.840784	2213.630280	20.388570
60.485232	2204.695450	20.393587
59.862995	2213.415401	20.398605
60.066710	2212.329379	20.403623
59.900334	2214.634171	20.408640
59.947948	2201.570005	20.413658
60.373586	2204.154460	20.418675
60.082982	2215.312606	20.423693
60.503246	2205.090498	20.428711
60.352141	2202.759760	20.433728
60.596363	2215.304849	20.438746
60.683255	2209.976411	20.443763
60.428531	2208.899093	20.448781
60.556588	2222.734291	20.453799
60.194019	2229.008624	20.458816
60.415845	2223.390774	20.463834
60.711228	2235.107277	20.468851
60.962083	2241.878852	20.473869
60.940454	2235.617425	20.478887
60.991104	2246.245554	20.483904
61.191520	2260.325087	20.488922
60.749593	2261.079228	20.493939
61.210657	2260.691410	20.498957
61.284444	2256.734757	20.503975
61.345106	2262.756583	20.508992
61.452355	2260.609444	20.514010
61.470678	2257.737710	20.519027
61.028463	2267.846569	20.524045
61.418239	2268.928037	20.529063
61.814713	2281.667089	20.534080
61.602793	2282.555624	20.539098
61.560482	2279.971123	20.544115
61.878261	2278.374875	20.549133
61.875463	2283.270454	20.554151
61.640775	2275.950383	20.559168
61.818005	2283.942296	20.564186
61.967377	2294.977904	20.569203
62.063626	2304.768868	20.574221
62.459667	2302.103061	20.579239
61.804286	2304.083654	20.584256
61.811953	2312.029555	20.589274
62.336626	2306.907080	20.594291
61.902828	2313.454559	20.599309
62.223843	2315.664066	20.604327
62.629213	2327.530671	20.609344
62.994667	2331.440672	20.614362
63.096868	2329.114416	20.619379
62.788931	2326.110734	20.624397
63.265359	2320.484525	20.629415
63.199401	2320.226619	20.634432
63.465231	2328.747521	20.639450
63.612643	2314.796550	20.644467
63.262131	2319.427851	20.649485
63.489890	2317.369131	20.654503
63.457517	2310.112031	20.659520
63.349123	2302.223000	20.664538
63.384387	2296.517580	20.669555
63.435644	2309.572695	20.674573
63.458312	2318.138001	20.679591
63.550072	2313.569392	20.684608
63.565633	2314.936733	20.689626
63.695092	2309.699436	20.694643
63.569330	2313.850511	20.699661
63.152074	2315.358254	20.704679
63.167305	2316.100738	20.709696
63.297193	2328.632258	20.714714
64.093919	2340.421776	20.719731
63.894387	2338.584649	20.724749
63.997947	2342.321069	20.729767
64.128243	2340.549042	20.734784
64.082889	2348.973527	20.739802
64.283845	2344.207903	20.744819
64.295479	2354.286733	20.749837
64.129398	2361.988452	20.754855
64.556595	2369.395232	20.759872
64.320086	2379.841189	20.764890
65.179314	2363.635654	20.769907
64.892531	2361.569174	20.774925
64.889433	2359.142636	20.779943
65.185624	2357.906405	20.784960
65.181146	2358.027068	20.789978
65.364245	2359.854205	20.794995
65.108926	2360.812665	20.800013
65.135385	2358.798104	20.805031
65.071645	2365.880973	20.810048
64.909495	2356.513809	20.815066
65.174598	2353.644426	20.820083
65.409805	2355.535989	20.825101
65.224534	2354.296288	20.830119
65.367996	2360.882743	20.835136
65.326131	2371.108833	20.840154
65.314437	2380.093004	20.845171
65.493724	2388.046767	20.850189
65.524100	2382.266340	20.855207
65.290396	2376.823963	20.860224
65.533673	2399.405785	20.865242
65.801226	2402.346430	20.870259
65.372758	2415.132765	20.875277
65.809076	2414.366931	20.880295
65.974894	2407.719433	20.885312
66.146526	2415.567100	20.890330
66.346601	2413.209719	20.895347
66.456578	2417.175546	20.900365
66.680110	2425.504286	20.905383
66.513436	2423.254861	20.910400
66.693494	2421.105764	20.915418
66.780592	2428.859373	20.920435
66.739062	2428.995310	20.925453
66.829693	2422.189156	20.930471
66.933984	2416.971551	20.935488
67.066812	2421.060044	20.940506
67.048263	2418.487581	20.945523
66.795102	2409.128337	20.950541
66.919815	2416.598308	20.955559
66.998703	2421.503220	20.960576
66.711319	2426.415021	20.965594
67.629513	2423.560081	20.970611
67.383380	2426.694832	20.975629
67.168760	2431.686761	20.980647
67.400006	2431.227639	20.985664
67.407104	2444.810531	20.990682
67.671141	2442.367378	20.995699
67.718726	2445.639170	21.000717
67.622869	2452.929097	21.005735
67.886093	2441.191269	21.010752
67.628591	2453.789883	21.015770
67.313038	2442.448878	21.020787
67.342390	2455.633776	21.025805
67.485512	2463.116663	21.030823
67.516129	2470.989603	21.035840
67.719306	2479.346806	21.040858
68.275260	2487.497247	21.045875
68.232365	2499.566755	21.050893
68.598263	2500.254306	21.055911
68.340742	2499.183721	21.060928
68.621623	2491.533450	21.065946
68.611954	2497.537969	21.070963
68.315643	2489.037601	21.075981
68.227764	2493.432117	21.080999
68.745910	2491.119577	21.086016
68.829185	2511.662494	21.091034
69.093792	2506.798483	21.096051
68.955234	2514.050939	21.101069
69.186263	2517.884202	21.106087
69.152975	2515.238287	21.111104
69.204643	2510.559132	21.116122
69.339218	2514.369632	21.121139
69.261021	2512.033743	21.126157
69.503887	2522.600359	21.131175
69.697914	2520.354377	21.136192
69.172873	2516.422053	21.141210
69.398085	2522.683301	21.146227
69.411346	2528.223440	21.151245
69.295610	2544.006548	21.156263
69.934232	2531.581773	21.161280
69.897605	2529.188871	21.166298
70.350464	2525.769281	21.171315
70.093140	2540.144835	21.176333
69.989536	2537.872890	21.181351
70.299387	2540.595470	21.186368
70.502186	2554.854761	21.191386
70.551076	2553.805601	21.196403
70.454092	2554.780294	21.201421
70.176329	2556.073676	21.206439
70.820835	2546.876710	21.211456
70.603880	2550.963223	21.216474
70.793516	2552.148658	21.221491
70.781987	2559.302327	21.226509
70.645456	2556.931385	21.231527
71.207823	2555.268388	21.236544
71.179446	2556.503761	21.241562
70.952046	2553.856691	21.246579
70.865695	2554.337359	21.251597
71.039614	2560.190045	21.256615
71.359368	2562.384000	21.261632
71.384341	2570.409364	21.266650
71.196495	2580.731036	21.271667
71.308969	2576.282204	21.276685
71.429286	2583.557253	21.281703
71.712064	2581.117457	21.286720
71.432649	2590.421419	21.291738
71.470399	2582.528305	21.296755
71.404122	2595.324300	21.301773
71.570341	2608.869761	21.306791
71.951106	2611.098349	21.311808
71.868659	2605.054628	21.316826
71.755742	2603.847759	21.321843
72.056855	2595.146431	21.326861
71.849643	2617.859074	21.331879
72.513337	2621.261613	21.336896
72.231472	2634.605867	21.341914
72.369258	2634.568528	21.346931
72.674571	2636.954124	21.351949
72.512291	2638.967961	21.356967
72.928274	2624.299255	21.361984
72.873640	2630.938938	21.367002
72.684746	2631.789164	21.372019
73.127724	2626.944518	21.377037
72.804008	2638.120736	21.382055
73.024953	2626.799713	21.387072
73.115339	2625.415807	21.392090
73.124603	2648.586934	21.397107
73.159646	2653.817551	21.402125
73.179512	2647.432701	21.407143
72.976492	2656.620574	21.412160
73.186500	2663.105185	21.417178
73.051679	2660.522499	21.422195
73.124392	2674.142627	21.427213
73.075729	2684.470957	21.432231
73.508247	2682.774638	21.437248
73.785227	2684.227297	21.442266
73.812025	2698.239689	21.447283
74.357273	2706.423470	21.452301
73.714271	2710.330588	21.457319
74.007968	2702.974900	21.462336
74.413426	2707.648824	21.467354
74.716122	2704.782964	21.472371
74.535375	2703.469937	21.477389
74.583877	2708.124038	21.482407
74.783043	2700.748444	21.487424
74.744258	2702.670347	21.492442
74.952148	2700.759882	21.497459
75.021382	2696.712317	21.502477
74.454738	2705.291233	21.507495
74.419071	2704.189032	21.512512
74.565152	2706.621679	21.517530
74.650242	2726.110393	21.522547
74.775087	2721.978362	21.527565
74.907422	2727.278975	21.532583
75.313989	2721.600464	21.537600
74.934544	2743.797387	21.542618
75.270206	2748.450694	21.547635
75.647489	2752.305280	21.552653
75.579228	2757.286993	21.557671
75.731546	2753.030716	21.562688
75.712513	2756.562340	21.567706
75.899770	2751.593603	21.572723
76.047021	2754.259631	21.577741
75.802234	2761.320521	21.582759
76.389873	2745.548564	21.587776
75.927486	2748.821405	21.592794
75.783089	2765.174153	21.597811
76.074923	2769.045286	21.602829
75.984017	2781.201410	21.607847
76.469181	2779.367430	21.612864
76.319734	2772.627164	21.617882
76.233664	2768.900597	21.622899
76.500281	2778.879748	21.627917
76.612510	2790.559029	21.632935
76.741907	2795.743343	21.637952
76.753577	2796.543216	21.642970
76.309075	2791.241051	21.647987
77.074115	2799.055882	21.653005
76.867923	2801.089241	21.658023
77.054240	2812.993644	21.663040
77.276339	2814.578004	21.668058
77.121522	2820.501216	21.673075
77.489009	2816.331148	21.678093
77.421274	2827.328505	21.683111
77.513064	2813.076558	21.688128
77.582148	2809.543451	21.693146
77.800350	2821.707985	21.698163
77.890294	2814.573546	21.703181
77.855816	2821.371108	21.708199
77.765097	2816.019819	21.713216
77.861238	2830.753688	21.718234
77.970578	2840.290397	21.723251
78.365205	2836.665251	21.728269
78.042006	2845.932016	21.733287
78.487130	2846.670294	21.738304
78.499161	2842.679002	21.743322
78.038574	2851.979921	21.748339
78.439677	2840.112921	21.753357
78.176924	2846.482296	21.758375
78.457835	2861.714326	21.763392
78.741613	2871.640341	21.768410
78.773226	2870.028909	21.773427
79.009758	2869.947693	21.778445
78.718978	2878.833809	21.783463
78.963336	2862.885129	21.788480
79.159090	2872.837561	21.793498
79.180884	2888.507892	21.798515
78.992888	2898.687740	21.803533
78.828310	2901.645672	21.808551
79.126184	2892.376591	21.813568
79.514605	2909.731727	21.818586
79.353055	2920.125222	21.823603
79.555872	2920.235505	21.828621
79.871134	2917.948386	21.833639
79.597660	2924.341561	21.838656
79.849485	2924.084357	21.843674
80.120842	2934.659377	21.848691
80.298255	2937.181832	21.853709
80.294732	2944.170275	21.858727
80.349671	2941.090698	21.863744
80.300388	2947.518194	21.868762
80.582911	2941.972673	21.873779
80.806150	2941.069767	21.878797
80.413552	2945.224918	21.883815
80.867035	2939.747300	21.888832
80.855578	2927.913318	21.893850
80.494403	2935.390194	21.898867
80.837712	2949.823469	21.903885
80.998967	2948.043377	21.908903
80.934011	2960.975142	21.913920
81.238439	2964.516098	21.918938
81.211906	2964.416128	21.923955
81.525615	2965.455904	21.928973
81.311367	2965.603123	21.933991
81.274707	2966.483169	21.939008
81.554551	2967.155816	21.944026
81.762491	2982.935940	21.949043
81.727250	2986.116651	21.954061
81.644281	2987.319576	21.959079
81.332510	2982.072307	21.964096
81.622164	2990.106889	21.969114
81.858853	3000.640035	21.974131
81.851159	3016.611783	21.979149
81.537678	3018.639882	21.984167
81.796400	3018.299535	21.989184
82.363249	3027.868820	21.994202
82.322306	3037.100930	21.999219
82.831523	3037.945955	22.004237
82.747111	3036.466311	22.009255
82.697422	3035.350506	22.014272
82.592811	3034.650460	22.019290
82.411187	3039.359637	22.024307
82.899137	3037.127511	22.029325
83.143752	3048.300159	22.034343
83.092370	3053.569682	22.039360
83.600289	3058.300239	22.044378
83.345583	3060.552695	22.049395
83.644053	3053.530680	22.054413
83.821212	3049.715470	22.059431
83.304270	3055.846993	22.064448
83.985632	3055.686616	22.069466
83.973143	3050.411376	22.074483
83.968353	3047.940823	22.079501
84.102825	3050.479491	22.084519
83.871011	3043.351186	22.089536
84.128647	3039.621213	22.094554
83.914055	3049.230877	22.099571
84.113333	3041.864596	22.104589
84.729020	3050.138498	22.109607
84.381542	3058.904179	22.114624
84.474826	3059.015842	22.119642
84.292500	3076.261717	22.124659
84.714754	3069.229770	22.129677
84.964209	3080.793054	22.134695
84.650084	3075.533501	22.139712
84.860882	3069.756149	22.144730
84.625671	3080.555806	22.149747
84.986983	3079.770136	22.154765
85.089353	3096.188678	22.159783
84.861091	3096.518000	22.164800
85.338967	3093.671978	22.169818
84.755737	3092.317823	22.174835
85.407498	3107.255242	22.179853
85.652702	3120.255308	22.184871
85.612049	3120.125988	22.189888
85.678650	3114.926712	22.194906
86.072794	3120.435766	22.199923
85.845385	3119.483518	22.204941
85.884446	3124.609487	22.209959
85.794411	3126.877183	22.214976
86.027226	3128.463048	22.219994
85.741948	3149.238027	22.225011
86.226625	3152.924374	22.230029
86.570967	3145.396449	22.235047
86.317626	3152.834425	22.240064
86.703628	3161.352677	22.245082
86.718317	3164.254159	22.250099
86.603587	3164.300569	22.255117
86.658903	3165.396621	22.260135
86.770600	3165.947277	22.265152
86.790385	3159.941009	22.270170
86.942539	3173.160848	22.275187
87.102946	3181.654485	22.280205
87.142751	3186.575197	22.285223
86.859223	3190.142033	22.290240
87.473230	3181.233589	22.295258
87.595914	3194.076154	22.300275
87.785764	3207.072330	22.305293
88.192455	3202.914970	22.310311
88.415110	3210.480396	22.315328
88.196976	3183.478069	22.320346
88.096003	3193.057384	22.325363
88.270944	3199.680246	22.330381
88.435779	3199.319886	22.335399
88.317967	3212.594675	22.340416
88.611949	3207.283999	22.345434
88.476857	3216.357357	22.350451
88.315888	3212.295243	22.355469
88.457850	3211.853248	22.360487
88.331606	3212.438027	22.365504
88.641364	3201.702420	22.370522
88.406985	3213.613030	22.375539
88.769386	3228.438071	22.380557
88.799919	3231.346551	22.385575
88.529896	3238.948146	22.390592
88.763768	3233.290221	22.395610
88.829504	3246.741436	22.400627
89.066334	3255.084258	22.405645
89.365663	3270.774565	22.410663
89.060939	3264.686540	22.415680
89.597544	3272.682559	22.420698
89.437358	3287.611617	22.425715
89.586836	3289.485149	22.430733
89.432710	3282.657049	22.435751
89.638084	3304.014996	22.440768
89.919195	3313.313573	22.445786
90.256350	3324.456112	22.450803
90.189390	3310.121331	22.455821
90.482489	3304.441480	22.460839
90.309696	3313.530261	22.465856
90.652834	3322.986408	22.470874
90.691866	3340.377762	22.475891
90.922127	3339.590520	22.480909
91.084100	3338.533067	22.485927
91.056771	3344.092441	22.490944
91.529323	3336.077220	22.495962
91.393391	3339.330581	22.500979
91.300695	3338.777002	22.505997
91.330786	3335.931660	22.511015
91.140548	3337.508073	22.516032
91.415207	3335.514487	22.521050
91.496419	3337.076779	22.526067
91.322661	3358.159622	22.531085
91.766505	3351.881694	22.536103
91.729548	3370.058272	22.541120
91.275526	3363.381284	22.546138
91.597387	3371.707682	22.551155
92.058408	3382.903447	22.556173
92.069672	3387.727684	22.561191
92.042397	3394.464363	22.566208
92.160769	3393.877713	22.571226
92.102046	3400.332099	22.576243
92.540437	3412.459378	22.581261
92.705693	3411.477158	22.586279
93.055313	3416.330456	22.591296
93.193079	3398.800918	22.596314
93.222066	3402.018984	22.601331
93.046830	3406.566285	22.606349
92.870365	3406.720213	22.611367
93.367086	3424.904767	22.616384
93.487018	3429.765647	22.621402
93.435633	3424.755208	22.626419
93.457851	3439.797848	22.631437
93.788780	3428.282340	22.636455
93.635768	3431.213295	22.641472
93.867501	3433.269646	22.646490
93.749500	3427.856168	22.651507
93.909030	3431.905988	22.656525
94.264242	3441.855846	22.661543
93.992922	3450.322559	22.666560
94.183239	3459.187241	22.671578
94.333521	3456.461927	22.676595
94.168524	3459.375826	22.681613
94.676843	3444.303766	22.686631
94.389569	3460.051422	22.691648
94.233578	3464.655692	22.696666
95.107363	3468.000232	22.701683
95.106846	3469.619529	22.706701
95.404773	3466.075692	22.711719
95.336378	3470.454767	22.716736
95.310163	3464.360916	22.721754
95.711790	3469.935188	22.726771
95.522458	3470.974898	22.731789
95.709227	3467.448476	22.736807
95.398578	3471.906538	22.741824
95.579596	3469.602508	22.746842
95.725183	3464.703232	22.751859
95.770699	3462.489871	22.756877
95.720325	3472.803138	22.761895
95.661929	3486.097226	22.766912
95.922113	3484.585651	22.771930
96.190391	3495.581272	22.776947
96.098629	3500.008203	22.781965
96.199891	3511.159409	22.786983
96.284503	3524.772002	22.792000
96.376716	3527.036446	22.797018
96.350225	3521.280345	22.802035
96.610608	3545.069792	22.807053
96.776954	3541.486586	22.812071
97.068413	3546.601537	22.817088
97.048663	3551.777873	22.822106
97.589580	3546.267438	22.827123
97.198698	3546.922095	22.832141
97.363917	3546.236568	22.837159
97.314639	3559.712348	22.842176
97.707515	3570.802122	22.847194
97.783577	3561.895709	22.852211
97.654534	3570.851513	22.857229
97.983534	3567.277537	22.862247
97.904297	3569.568848	22.867264
97.761488	3568.578070	22.872282
98.096609	3587.883352	22.877299
98.193700	3589.818781	22.882317
98.551171	3590.340413	22.887335
98.501842	3595.565584	22.892352
98.304564	3594.286643	22.897370
98.507093	3600.794860	22.902387
98.767987	3618.429479	22.907405
98.961192	3619.813276	22.912423
98.584266	3626.387034	22.917440
98.940890	3624.105974	22.922458
99.010663	3630.777035	22.927475
99.053116	3641.331518	22.932493
99.173761	3641.132734	22.937511
99.053049	3644.560521	22.942528
99.213065	3649.787629	22.947546
99.730214	3658.203505	22.952563
99.621382	3669.353005	22.957581
100.255224	3673.328569	22.962599
99.911502	3674.954308	22.967616
99.603029	3677.401488	22.972634
100.121972	3689.083914	22.977651
100.180574	3693.253766	22.982669
100.388064	3690.913997	22.987687
100.224901	3699.572200	22.992704
100.459085	3690.748268	22.997722
100.515902	3705.769926	23.002739
100.622806	3718.706870	23.007757
100.983366	3718.413683	23.012775
100.456274	3733.189116	23.017792
100.778730	3730.717702	23.022810
101.143788	3731.067707	23.027827
101.231417	3747.858444	23.032845
101.503857	3742.408951	23.037863
101.724010	3741.945224	23.042880
101.758277	3744.029392	23.047898
101.905605	3743.154123	23.052915
101.646714	3753.727476	23.057933
101.694245	3744.702346	23.062951
101.892922	3749.497318	23.067968
101.877547	3746.138236	23.072986
102.176269	3753.445776	23.078003
102.216190	3762.640337	23.083021
101.917660	3764.041215	23.088039
102.273903	3765.105939	23.093056
102.396917	3776.020329	23.098074
102.583936	3779.504089	23.103091
102.595410	3804.472321	23.108109
102.637225	3794.671596	23.113127
102.803090	3796.987662	23.118144
102.494950	3807.325721	23.123162
103.115080	3810.687974	23.128179
103.446249	3809.004277	23.133197
103.763308	3811.340846	23.138215
103.741552	3813.247574	23.143232
103.867741	3811.176193	23.148250
103.917184	3799.398384	23.153267
104.122918	3810.858512	23.158285
104.258016	3802.106864	23.163303
104.516645	3797.729527	23.168320
104.134272	3798.256604	23.173338
104.259367	3800.730564	23.178355
104.571592	3819.376843	23.183373
104.717242	3823.574120	23.188391
104.766361	3827.010053	23.193408
104.879958	3822.282981	23.198426
104.789096	3822.972708	23.203443
104.881922	3827.661186	23.208461
104.833014	3818.761601	23.213479
104.972461	3827.656529	23.218496
104.887456	3843.404391	23.223514
105.321437	3841.922373	23.228531
105.236746	3846.335656	23.233549
105.398053	3841.493787	23.238567
105.491104	3841.876940	23.243584
105.406921	3862.621230	23.248602
105.775259	3869.706435	23.253619
105.870650	3872.049333	23.258637
106.047910	3868.928340	23.263655
106.309769	3873.088484	23.268672
106.121707	3877.350681	23.273690
106.610804	3886.007788	23.278707
106.345140	3899.407248	23.283725
106.547750	3903.627183	23.288743
106.420170	3905.790384	23.293760
106.669589	3911.701123	23.298778
106.685201	3905.262837	23.303795
106.978054	3912.760745	23.308813
107.289436	3915.110844	23.313831
107.511953	3914.858220	23.318848
107.203472	3910.872718	23.323866
107.281196	3917.709928	23.328883
107.264348	3926.932404	23.333901
107.702372	3930.654630	23.338919
107.591731	3940.488365	23.343936
108.088682	3933.015116	23.348954
107.928221	3927.049458	23.353971
108.317062	3936.615555	23.358989
108.479514	3933.345364	23.364007
108.474180	3930.890558	23.369024
108.485145	3935.673955	23.374042
108.501946	3926.858714	23.379059
108.344780	3928.865578	23.384077
108.696604	3940.719545	23.389095
108.795948	3946.937882	23.394112
108.689366	3956.149181	23.399130
109.116078	3948.447043	23.404147
109.213540	3950.079440	23.409165
109.130367	3954.022208	23.414183
109.025211	3960.594541	23.419200
109.064129	3978.864003	23.424218
109.470849	3983.733762	23.429235
109.689486	3981.395367	23.434253
109.626491	3985.246601	23.439271
109.728978	3989.677939	23.444288
109.865999	3999.791702	23.449306
110.270683	4001.025610	23.454323
109.948650	4008.926063	23.459341
110.120397	4001.418512	23.464359
110.438851	4017.478928	23.469376
110.222142	4035.548610	23.474394
110.582249	4031.272105	23.479411
110.168522	4040.938743	23.484429
110.617670	4056.050733	23.489447
110.950344	4065.947652	23.494464
111.018626	4067.685636	23.499482
111.213057	4044.152570	23.504499
111.634349	4050.301565	23.509517
111.509580	4057.331529	23.514535
111.681615	4065.312421	23.519552
111.883090	4067.316772	23.524570
111.893021	4060.248038	23.529587
112.184644	4074.074812	23.534605
112.136799	4071.614022	23.539623
111.920971	4072.711576	23.544640
111.777215	4085.372411	23.549658
112.389372	4088.890631	23.554675
112.462681	4097.281557	23.559693
112.454108	4104.088167	23.564711
112.665061	4097.205718	23.569728
112.421004	4100.570848	23.574746
112.735598	4119.005585	23.579763
112.683193	4123.521195	23.584781
112.759755	4130.974170	23.589799
112.789416	4139.703378	23.594816
112.734485	4161.264097	23.599834
113.120523	4158.037748	23.604851
113.392054	4173.928894	23.609869
113.646393	4187.367042	23.614887
113.686774	4180.438687	23.619904
113.631721	4191.750529	23.624922
113.923191	4200.962717	23.629939
114.046647	4207.155271	23.634957
113.961642	4215.185969	23.639975
114.381650	4215.132822	23.644992
114.295927	4228.883106	23.650010
114.380364	4233.866553	23.655027
114.484299	4239.048958	23.660045
114.510135	4246.004896	23.665063
114.821268	4247.165098	23.670080
115.041257	4265.908356	23.675098
114.972424	4260.013458	23.680115
115.221351	4267.572055	23.685133
115.127581	4272.570806	23.690151
115.689661	4282.665479	23.695168
115.616318	4297.572293	23.700186
115.336411	4291.884057	23.705203
115.262964	4300.143403	23.710221
115.378061	4296.924757	23.715239
116.161334	4298.572842	23.720256
116.147970	4314.533996	23.725274
116.355259	4306.203230	23.730291
116.689422	4307.789106	23.735309
116.399947	4311.167703	23.740327
117.043190	4319.797713	23.745344
117.147353	4333.950761	23.750362
117.298168	4333.835625	23.755379
117.228871	4329.938815	23.760397
117.421290	4332.074028	23.765415
117.564768	4318.147384	23.770432
117.467064	4316.445608	23.775450
117.559989	4321.591885	23.780467
117.643920	4327.162538	23.785485
117.831955	4326.501816	23.790503
117.698047	4319.244034	23.795520
118.272080	4333.935822	23.800538
118.255384	4340.282950	23.805555
118.439950	4341.848076	23.810573
118.609984	4355.773026	23.815591
118.568239	4342.178402	23.820608
118.750759	4347.193861	23.825626
118.598669	4345.244929	23.830643
118.625155	4337.621114	23.835661
118.736892	4353.550078	23.840679
118.761558	4361.989781	23.845696
118.926450	4375.489429	23.850714
118.843466	4373.690648	23.855731
119.378414	4383.025764	23.860749
119.149178	4405.996614	23.865767
119.383157	4396.771500	23.870784
119.727492	4400.726300	23.875802
119.577408	4419.821247	23.880819
119.908696	4426.094948	23.885837
119.959570	4427.955640	23.890855
120.062007	4427.788110	23.895872
120.373144	4434.099693	23.900890
120.505483	4454.877023	23.905907
120.472196	4453.922697	23.910925
120.407303	4468.203343	23.915943
120.685073	4458.144339	23.920960
120.252502	4484.893887	23.925978
120.545506	4478.421409	23.930995
121.020800	4493.340280	23.936013
121.522823	4506.635697	23.941031
121.518614	4514.354002	23.946048
121.345032	4527.966765	23.951066
121.185020	4518.935887	23.956083
121.645982	4527.181054	23.961101
121.408781	4541.444562	23.966119
121.797273	4536.772088	23.971136
121.748492	4557.382208	23.976154
121.911936	4559.859734	23.981171
122.305358	4556.894148	23.986189
122.328502	4580.589551	23.991207
122.626895	4586.906340	23.996224
122.680296	4587.355695	24.001242
122.561997	4596.853239	24.006259
122.977912	4594.528050	24.011277
123.124172	4610.600187	24.016295
123.378874	4596.779008	24.021312
123.731915	4605.612446	24.026330
124.114809	4614.286542	24.031347
124.012396	4598.434860	24.036365
123.824958	4605.698964	24.041383
123.910721	4593.687682	24.046400
124.048305	4608.479635	24.051418
124.300603	4618.957620	24.056435
124.192847	4622.146822	24.061453
124.412904	4632.636179	24.066471
124.514611	4627.936013	24.071488
124.586926	4628.900074	24.076506
124.296852	4631.524417	24.081523
124.969652	4647.065870	24.086541
125.072639	4656.512993	24.091559
125.119111	4648.759656	24.096576
125.438999	4662.430938	24.101594
125.400043	4667.244444	24.106611
125.628309	4664.961272	24.111629
125.296786	4664.375623	24.116647
125.280550	4669.371805	24.121664
125.715636	4685.048385	24.126682
125.555219	4685.818485	24.131699
126.019077	4690.647918	24.136717
125.697449	4702.614206	24.141735
125.998409	4697.810205	24.146752
126.368605	4714.967916	24.151770
126.234577	4727.217324	24.156787
126.643632	4736.272477	24.161805
126.432804	4749.613466	24.166823
126.827322	4753.257455	24.171840
127.154084	4754.257416	24.176858
126.922763	4757.819532	24.181875
127.172487	4762.531019	24.186893
127.091108	4773.579041	24.191911
127.396926	4784.339138	24.196928
127.665689	4792.743956	24.201946
127.817963	4807.290716	24.206963
128.013878	4811.666583	24.211981
127.825703	4818.040743	24.216999
127.846498	4816.875906	24.222016
128.505822	4831.119133	24.227034
128.216079	4838.424610	24.232051
128.502349	4837.521210	24.237069
128.639924	4848.481313	24.242087
128.928420	4855.333203	24.247104
128.864004	4861.586979	24.252122
129.149950	4866.687388	24.257139
129.667928	4871.678846	24.262157
129.230657	4879.086366	24.267175
129.298261	4894.186231	24.272192
129.611129	4891.069072	24.277210
129.646583	4908.566655	24.282227
129.869201	4913.304524	24.287245
130.234065	4911.154592	24.292263
130.363350	4915.348373	24.297280
130.281893	4915.840961	24.302298
130.278429	4928.707675	24.307315
130.573388	4931.423486	24.312333
130.659403	4943.547026	24.317351
131.285617	4946.918013	24.322368
131.160256	4938.184529	24.327386
131.279765	4943.513054	24.332403
131.043040	4958.300802	24.337421
131.208566	4969.269226	24.342439
131.484871	4975.450722	24.347456
131.390617	4977.331050	24.352474
131.693469	4990.825325	24.357491
131.844758	4998.352175	24.362509
131.985902	5004.321270	24.367527
131.636544	5012.393735	24.372544
132.049266	5021.634694	24.377562
132.080786	5030.294594	24.382579
132.688149	5025.107907	24.387597
132.836407	5029.917432	24.392615
132.871732	5043.605173	24.397632
132.829695	5045.796143	24.402650
133.158294	5056.638060	24.407667
133.094800	5056.758517	24.412685
133.248413	5053.214889	24.417703
133.330513	5064.388991	24.422720
133.423320	5070.214165	24.427738
133.336551	5080.900210	24.432755
134.076084	5075.282446	24.437773
133.947934	5100.182790	24.442791
133.654447	5101.251535	24.447808
134.133173	5099.090056	24.452826
134.092233	5110.011996	24.457843
134.665016	5119.590937	24.462861
134.268907	5128.191615	24.467879
134.393058	5133.020726	24.472896
134.840832	5136.643824	24.477914
134.649639	5155.038902	24.482931
135.050964	5144.887563	24.487949
135.001776	5164.377840	24.492967
135.377975	5177.491439	24.497984
135.842663	5173.854861	24.503002
135.417648	5179.426594	24.508019
136.034113	5183.263175	24.513037
136.137023	5203.373612	24.518055
136.080055	5207.148402	24.523072
136.297200	5206.353669	24.528090
136.120033	5209.973676	24.533107
136.840469	5214.510526	24.538125
136.739195	5227.212846	24.543143
136.913601	5231.140789	24.548160
136.723490	5227.875097	24.553178
136.715239	5254.171030	24.558195
136.922656	5251.414403	24.563213
137.333488	5263.386256	24.568231
137.462319	5280.708579	24.573248
137.348824	5284.864722	24.578266
137.511969	5290.325405	24.583283
137.793900	5295.126684	24.588301
138.029383	5301.573531	24.593319
138.503379	5307.392723	24.598336
138.515898	5320.213016	24.603354
138.805203	5326.121126	24.608371
138.636221	5333.502579	24.613389
138.953043	5334.500975	24.618407
138.944137	5340.260097	24.623424
139.291058	5332.686677	24.628442
139.451517	5348.877193	24.633459
139.663104	5346.353489	24.638477
139.916321	5358.893039	24.643495
140.155401	5354.079622	24.648512
140.365707	5358.402861	24.653530
139.948664	5358.723914	24.658547
140.071959	5347.706909	24.663565
140.065710	5356.290808	24.668583
140.442602	5371.036420	24.673600
140.433212	5380.548874	24.678618
140.204283	5384.435870	24.683635
140.583653	5393.369737	24.688653
140.844918	5400.311329	24.693671
140.946023	5408.827928	24.698688
141.080464	5407.222259	24.703706
141.166063	5434.327632	24.708723
141.210665	5434.819424	24.713741
141.322592	5435.830986	24.718759
141.614979	5451.221232	24.723776
141.807622	5460.455857	24.728794
141.161893	5468.937967	24.733811
141.804605	5477.941102	24.738829
141.853568	5482.993582	24.743847
141.851718	5490.061659	24.748864
142.209788	5497.474248	24.753882
142.150250	5513.456312	24.758899
142.304842	5520.177912	24.763917
142.658284	5536.205780	24.768935
142.251985	5548.230077	24.773952
142.800343	5566.437104	24.778970
142.632965	5566.962110	24.783987
143.149529	5579.353227	24.789005
143.653658	5599.909469	24.794023
143.519875	5611.644893	24.799040
143.685502	5609.365105	24.804058
143.668214	5624.175832	24.809075
143.864978	5630.527847	24.814093
144.036116	5642.076626	24.819111
144.583326	5660.233419	24.824128
144.424014	5649.550923	24.829146
144.673856	5676.349979	24.834163
145.068215	5672.033007	24.839181
145.141947	5692.028599	24.844199
145.012741	5683.039668	24.849216
145.492563	5690.739461	24.854234
145.483734	5704.911276	24.859251
145.506656	5718.134276	24.864269
145.626765	5710.924530	24.869287
145.840854	5725.474965	24.874304
146.144132	5727.880237	24.879322
146.870376	5733.729497	24.884339
146.423102	5744.784921	24.889357
147.034907	5750.942531	24.894375
147.313344	5747.978988	24.899392
147.332348	5739.260383	24.904410
147.681171	5738.410275	24.909427
147.958219	5744.011085	24.914445
148.353585	5738.336557	24.919463
148.096584	5733.439768	24.924480
148.353922	5739.687631	24.929498
148.135974	5736.161045	24.934515
148.386238	5740.705397	24.939533
148.284800	5732.087739	24.944551
148.346868	5735.354700	24.949568
148.893103	5744.133173	24.954586
148.498996	5758.311726	24.959603
148.525890	5754.806755	24.964621
149.091133	5758.130629	24.969639
149.191351	5761.789363	24.974656
149.138752	5767.959523	24.979674
149.181129	5781.687751	24.984691
149.246682	5783.126439	24.989709
149.333201	5793.403790	24.994727
149.518265	5812.457156	24.999744
149.447780	5814.340160	25.004762
149.563701	5824.723407	25.009779
149.831331	5843.381908	25.014797
150.183173	5850.211623	25.019815
149.979194	5857.516695	25.024832
150.038737	5864.335388	25.029850
150.499979	5886.941073	25.034867
150.457404	5897.270274	25.039885
151.068914	5901.044651	25.044903
151.026569	5919.909628	25.049920
151.423037	5927.253243	25.054938
151.502629	5936.818337	25.059955
151.515364	5946.207663	25.064973
151.590835	5950.091283	25.069991
151.625124	5959.862362	25.075008
151.875488	5961.644607	25.080026
151.903052	5984.864471	25.085043
151.966973	5983.569691	25.090061
152.487450	5990.543504	25.095079
152.527760	6006.908107	25.100096
152.740221	6009.305547	25.105114
152.691237	6016.599027	25.110131
152.921514	6026.639328	25.115149
153.232692	6032.118079	25.120167
153.005627	6040.601153	25.125184
153.517920	6058.593349	25.130202
153.675149	6071.628254	25.135219
153.661085	6082.559190	25.140237
154.027845	6091.059743	25.145255
153.791086	6104.576245	25.150272
154.265625	6111.102727	25.155290
154.688183	6119.193642	25.160307
154.414211	6127.014869	25.165325
154.581814	6127.228555	25.170343
154.754692	6134.032750	25.175360
154.789932	6142.544225	25.180378
155.191271	6158.584077	25.185395
155.178878	6173.242956	25.190413
155.485699	6173.305405	25.195431
155.619062	6182.234005	25.200448
155.480002	6197.436773	25.205466
155.530176	6212.714081	25.210483
155.706330	6229.676329	25.215501
156.158191	6232.939135	25.220519
156.211428	6252.588147	25.225536
156.663330	6263.484072	25.230554
156.934346	6273.675966	25.235571
157.087566	6295.591723	25.240589
157.646373	6290.630112	25.245607
157.719108	6299.561954	25.250624
157.693196	6293.700712	25.255642
157.731513	6293.060222	25.260659
157.577389	6313.966623	25.265677
158.054069	6314.731682	25.270695
157.934508	6329.066541	25.275712
158.209199	6339.627242	25.280730
158.359159	6339.142884	25.285747
158.760721	6350.895929	25.290765
158.886919	6357.448661	25.295783
158.734735	6377.259418	25.300800
159.151735	6374.633944	25.305818
159.525406	6380.046187	25.310835
159.509424	6394.598474	25.315853
159.443254	6391.272116	25.320871
159.230302	6402.578494	25.325888
159.996231	6409.280411	25.330906
159.879928	6413.241526	25.335923
160.135022	6432.363486	25.340941
160.485690	6436.226194	25.345959
160.641861	6446.246767	25.350976
160.771685	6454.547847	25.355994
161.228638	6459.647168	25.361011
161.178464	6466.530626	25.366029
161.668776	6459.543548	25.371047
161.694332	6464.931433	25.376064
161.839295	6459.879927	25.381082
162.349620	6466.644007	25.386099
162.401418	6488.961017	25.391117
163.055630	6474.463411	25.396135
162.822493	6470.216148	25.401152
162.815505	6464.209830	25.406170
162.841912	6469.395546	25.411187
162.825329	6475.939121	25.416205
163.101899	6470.971169	25.421223
162.992376	6466.082646	25.426240
163.284201	6468.095209	25.431258
163.099412	6477.484183	25.436275
162.884946	6493.096769	25.441293
163.373731	6500.527171	25.446311
163.737010	6515.597838	25.451328
163.827879	6528.116273	25.456346
164.010843	6523.548106	25.461363
163.882004	6534.579370	25.466381
164.529048	6538.070515	25.471399
164.342149	6554.676395	25.476416
164.543396	6566.031630	25.481434
164.916963	6573.385407	25.486451
164.594931	6595.672720	25.491469
164.578648	6595.829986	25.496487
164.702767	6618.331547	25.501504
164.860029	6643.744880	25.506522
165.151274	6648.210432	25.511539
165.252381	6675.817153	25.516557
165.738557	6686.335452	25.521575
165.830615	6697.761541	25.526592
166.231972	6696.031867	25.531610
166.453323	6715.386703	25.536627
166.110731	6731.013249	25.541645
166.687080	6732.154167	25.546663
166.696528	6756.047101	25.551680
167.089111	6759.657075	25.556698
167.384567	6772.203606	25.561715
167.286823	6784.458174	25.566733
167.850608	6793.379622	25.571751
168.309762	6801.824992	25.576768
168.311688	6815.696076	25.581786
168.246459	6811.122524	25.586803
168.230475	6829.106691	25.591821
168.854097	6831.910204	25.596839
168.748300	6845.485654	25.601856
168.830030	6851.218424	25.606874
169.272480	6868.865631	25.611891
169.338845	6873.622177	25.616909
169.443746	6874.578096	25.621927
169.183049	6890.728620	25.626944
169.635631	6894.111395	25.631962
170.163859	6900.462436	25.636979
169.955007	6924.970659	25.641997
170.278367	6934.422318	25.647015
170.809757	6927.810615	25.652032
170.643718	6933.320203	25.657050
171.093834	6946.571870	25.662067
170.876213	6956.692321	25.667085
170.998379	6950.327820	25.672103
171.147708	6972.551215	25.677120
171.255292	6983.567807	25.682138
171.727771	6992.159553	25.687156
171.861339	7005.628170	25.692173
172.259936	7009.871793	25.697191
172.405062	7010.294212	25.702208
172.151683	7038.582082	25.707226
172.355883	7032.264683	25.712244
172.567266	7038.362345	25.717261
172.950584	7059.668405	25.722279
173.171078	7074.755587	25.727296
173.190622	7073.530821	25.732314
173.735667	7089.116477	25.737332
173.623283	7092.294203	25.742349
173.777962	7094.609288	25.747367
174.083481	7097.977258	25.752384
173.823140	7106.118771	25.757402
174.610014	7120.110197	25.762420
174.411032	7122.941605	25.767437
174.413966	7123.228455	25.772455
174.966042	7140.827181	25.777472
174.878352	7140.035927	25.782490
175.113678	7143.888443	25.787508
174.458346	7150.358693	25.792525
175.288214	7159.566958	25.797543
175.479048	7172.490045	25.802560
175.496995	7197.171458	25.807578
176.160600	7192.900349	25.812596
176.566657	7195.097142	25.817613
176.939888	7211.953657	25.822631
176.939952	7224.622541	25.827648
177.124350	7223.210935	25.832666
177.352875	7225.246127	25.837684
177.043530	7228.116938	25.842701
177.267087	7223.804267	25.847719
177.602119	7230.504542	25.852736
177.725973	7239.627721	25.857754
177.906899	7241.089491	25.862772
178.070777	7244.081901	25.867789
178.197388	7256.689942	25.872807
178.070010	7273.994305	25.877824
178.227697	7279.727937	25.882842
178.569445	7290.783796	25.887860
178.271945	7301.027443	25.892877
178.709434	7315.787230	25.897895
179.193562	7330.684943	25.902912
179.045013	7353.050172	25.907930
179.339061	7351.952861	25.912948
179.161863	7376.980783	25.917965
179.432898	7390.415518	25.922983
179.911065	7401.169101	25.928000
179.445550	7418.987492	25.933018
179.797544	7434.837302	25.938036
179.719850	7447.900517	25.943053
180.133012	7477.682078	25.948071
180.691960	7490.999171	25.953088
180.889285	7501.020186	25.958106
181.130778	7517.837637	25.963124
181.275180	7533.647442	25.968141
181.531587	7545.275615	25.973159
182.020384	7551.279475	25.978176
181.589533	7567.248883	25.983194
182.149821	7567.824110	25.988212
182.341416	7590.164752	25.993229
182.383099	7604.014415	25.998247
182.759414	7615.371286	26.003264
182.666222	7623.862526	26.008282
183.119528	7631.646221	26.013300
183.078620	7657.483469	26.018317
183.389563	7655.818386	26.023335
183.228292	7671.054261	26.028352
183.795111	7687.716719	26.033370
183.829512	7704.560469	26.038388
183.980165	7704.230664	26.043405
184.179499	7721.383238	26.048423
184.220830	7732.723204	26.053440
184.282148	7749.726945	26.058458
184.897132	7757.267529	26.063476
185.315618	7776.210595	26.068493
185.335816	7794.464697	26.073511
185.670868	7785.512502	26.078528
186.087534	7795.028914	26.083546
186.277254	7809.559564	26.088564
186.569887	7802.315660	26.093581
187.005482	7806.973562	26.098599
187.110301	7800.826167	26.103616
186.988536	7808.608473	26.108634
187.325963	7799.842166	26.113652
187.590190	7798.203331	26.118669
187.199799	7804.578630	26.123687
187.654030	7822.534300	26.128704
187.513814	7830.363704	26.133722
188.041056	7833.858086	26.138740
188.039726	7860.885945	26.143757
188.054899	7863.049344	26.148775
188.513713	7865.844112	26.153792
188.440416	7868.179225	26.158810
188.810563	7879.682450	26.163828
188.742278	7893.205438	26.168845
188.873049	7911.006657	26.173863
188.906596	7914.562611	26.178880
189.183356	7926.216250	26.183898
189.560555	7931.546318	26.188916
189.803546	7951.603093	26.193933
189.707422	7961.667173	26.198951
189.616513	7974.369765	26.203968
189.902180	7989.210705	26.208986
190.614998	8007.460696	26.214004
190.479370	8032.464050	26.219021
190.512769	8041.245044	26.224039
190.761076	8063.741543	26.229056
190.876682	8075.022728	26.234074
191.010111	8082.582058	26.239092
191.380756	8105.956061	26.244109
191.447243	8132.553797	26.249127
191.822182	8143.699683	26.254144
192.026753	8154.679681	26.259162
192.205179	8164.811360	26.264180
192.375534	8185.729032	26.269197
192.415272	8197.258960	26.274215
192.719522	8203.010962	26.279232
192.971535	8234.388081	26.284250
193.031439	8246.296893	26.289268
193.590125	8262.784347	26.294285
193.888740	8276.382735	26.299303
194.154148	8292.114247	26.304320
193.852010	8306.015142	26.309338
194.190772	8319.885101	26.314356
194.540702	8326.848643	26.319373
194.592698	8335.718421	26.324391
195.054286	8354.210171	26.329408
194.768450	8369.573476	26.334426
195.353727	8381.744201	26.339444
195.518485	8383.435912	26.344461
195.906992	8401.528727	26.349479
196.232320	8409.920033	26.354496
196.573264	8433.362246	26.359514
196.724734	8439.561316	26.364532
196.794072	8440.106143	26.369549
197.384877	8444.446277	26.374567
197.279261	8455.702364	26.379584
196.662362	8465.292640	26.384602
197.133938	8479.031411	26.389620
197.650757	8489.710119	26.394637
197.790388	8497.732752	26.399655
198.205583	8516.029872	26.404672
198.213215	8525.563384	26.409690
198.799356	8538.384456	26.414708
198.706078	8542.961226	26.419725
198.924529	8561.551259	26.424743
199.030030	8547.197988	26.429760
198.867403	8574.763620	26.434778
199.011546	8587.691855	26.439796
199.651439	8598.865967	26.444813
199.672941	8612.801634	26.449831
199.595763	8609.820734	26.454848
199.478944	8635.551265	26.459866
199.901554	8649.739842	26.464884
200.480407	8666.218183	26.469901
200.730868	8675.221207	26.474919
201.065073	8691.371660	26.479936
200.933824	8707.178294	26.484954
200.622333	8715.978909	26.489972
201.049425	8720.565761	26.494989
201.090113	8748.412363	26.500007
201.676361	8756.109407	26.505024
201.620700	8785.518196	26.510042
201.958581	8799.464427	26.515060
202.244758	8822.751536	26.520077
202.052150	8842.132409	26.525095
202.837264	8851.092805	26.530112
203.083582	8875.674376	26.535130
202.882152	8879.055791	26.540148
203.110740	8909.739973	26.545165
203.256373	8929.551007	26.550183
203.965153	8932.407813	26.555200
203.654194	8959.848862	26.560218
204.156806	8965.762619	26.565236
204.291560	8989.121018	26.570253
204.697186	9000.442578	26.575271
204.978016	9011.932086	26.580288
205.377075	9033.604201	26.585306
205.293190	9023.675146	26.590324
206.822510	9024.531165	26.595341
206.905543	9026.620925	26.600359
207.288416	9032.888132	26.605376
207.241054	9045.054214	26.610394
207.317616	9026.442796	26.615412
207.644684	9029.463605	26.620429
207.688830	9034.543073	26.625447
208.149631	9030.458030	26.630464
208.157958	9028.316129	26.635482
208.146553	9030.281763	26.640500
208.187874	9013.153479	26.645517
208.386930	9025.129396	26.650535
208.396170	9040.661723	26.655552
208.459561	9044.323723	26.660570
208.894922	9052.549692	26.665588
209.185715	9067.482255	26.670605
209.125982	9074.175586	26.675623
209.294774	9077.464309	26.680640
209.613049	9099.793242	26.685658
209.805924	9112.988892	26.690676
210.111098	9115.021760	26.695693
209.913728	9136.411715	26.700711
210.427977	9143.728699	26.705728
210.621313	9153.861741	26.710746
210.598115	9164.628595	26.715764
210.784324	9170.800367	26.720781
210.619963	9194.101691	26.725799
211.221036	9206.065263	26.730816
210.964410	9228.105537	26.735834
211.078165	9250.185690	26.740852
211.514529	9261.774123	26.745869
211.569156	9282.322813	26.750887
211.539687	9301.129235	26.755904
212.683490	9303.595905	26.760922
212.341201	9331.954873	26.765940
212.851016	9342.366800	26.770957
213.097869	9356.046709	26.775975
213.293096	9356.833900	26.780992
213.813221	9379.845103	26.786010
213.674649	9391.637348	26.791028
213.937057	9387.494903	26.796045
213.930604	9407.200822	26.801063
214.583059	9417.565187	26.806080
214.579039	9438.618938	26.811098
214.461000	9452.845467	26.816116
214.862777	9456.265098	26.821133
214.864187	9484.459948	26.826151
215.381577	9490.021095	26.831168
215.715285	9498.863083	26.836186
215.873288	9516.671049	26.841204
216.214054	9527.254801	26.846221
216.520755	9542.324177	26.851239
216.936628	9548.419051	26.856256
217.243206	9559.023964	26.861274
217.044949	9554.315862	26.866292
217.276051	9574.436245	26.871309
217.394371	9590.393972	26.876327
217.608858	9602.598331	26.881344
218.220674	9612.192461	26.886362
218.381583	9625.264031	26.891380
218.477011	9630.004104	26.896397
218.763654	9644.909365	26.901415
218.600080	9658.265436	26.906432
218.816102	9671.476801	26.911450
218.700410	9683.575069	26.916468
219.224395	9700.397609	26.921485
219.262819	9733.212596	26.926503
219.416612	9741.015689	26.931520
219.844948	9761.629502	26.936538
220.046245	9786.291950	26.941556
220.431602	9799.858924	26.946573
220.649527	9825.554445	26.951591
220.843398	9842.353050	26.956608
220.832089	9852.269097	26.961626
221.228542	9862.721178	26.966644
221.139870	9872.422021	26.971661
221.611873	9903.859062	26.976679
221.801164	9921.248892	26.981696
222.035865	9933.112457	26.986714
222.171160	9947.700669	26.991732
222.481130	9961.181690	26.996749
222.797116	9978.703282	27.001767
222.876076	10003.953519	27.006784
223.266998	10013.475110	27.011802
223.313622	10029.248683	27.016820
223.815792	10045.152982	27.021837
223.996222	10060.125733	27.026855
224.235680	10073.409491	27.031872
224.933227	10087.957094	27.036890
224.484836	10106.242669	27.041908
224.979261	10118.782405	27.046925
225.349550	10144.719723	27.051943
225.535286	10152.296962	27.056960
225.642319	10157.193224	27.061978
225.671898	10185.842551	27.066996
225.904425	10193.276706	27.072013
226.288825	10210.282605	27.077031
226.231967	10227.929146	27.082048
226.933838	10235.987593	27.087066
226.892301	10260.496104	27.092084
227.250961	10277.124042	27.097101
227.591150	10289.760678	27.102119
227.687090	10309.558862	27.107136
227.993724	10322.443903	27.112154
228.366582	10340.039020	27.117172
228.756234	10332.406357	27.122189
228.537130	10347.293526	27.127207
228.411209	10348.551016	27.132224
229.053437	10366.397606	27.137242
229.096305	10398.474212	27.142260
229.355177	10402.516330	27.147277
229.446275	10416.357190	27.152295
230.032556	10427.161909	27.157312
230.340506	10440.422568	27.162330
230.621074	10450.583698	27.167348
231.125529	10451.240400	27.172365
231.515940	10466.319513	27.177383
231.337234	10473.912927	27.182400
231.431359	10479.130204	27.187418
231.750607	10504.731849	27.192436
231.891672	10506.080141	27.197453
232.439846	10525.176206	27.202471
232.872114	10540.128836	27.207488
232.766763	10541.171562	27.212506
232.514537	10555.429423	27.217524
232.934885	10564.432010	27.222541
232.847697	10591.085749	27.227559
232.979044	10611.443903	27.232576
233.556725	10611.609196	27.237594
233.867380	10638.759561	27.242612
234.519958	10644.088325	27.247629
234.579480	10655.932430	27.252647
234.955764	10677.846844	27.257664
235.059179	10674.559458	27.262682
235.079090	10703.046898	27.267700
235.490954	10704.381200	27.272717
235.729472	10723.860678	27.277735
235.711284	10738.104117	27.282752
236.137821	10745.887007	27.287770
236.436822	10771.706903	27.292788
236.715436	10788.366781	27.297805
237.002627	10794.087529	27.302823
236.732628	10812.803691	27.307840
237.471915	10817.474779	27.312858
237.593537	10845.930715	27.317876
237.938328	10854.758982	27.322893
237.855432	10865.539324	27.327911
238.053532	10879.275352	27.332928
238.378489	10895.410223	27.337946
238.326195	10905.210102	27.342964
238.573898	10929.689965	27.347981
238.736751	10946.194451	27.352999
238.937778	10972.724641	27.358016
239.311991	10987.440432	27.363034
239.937468	11005.429192	27.368052
240.243316	11016.710776	27.373069
240.467054	11027.828403	27.378087
240.607324	11044.494394	27.383104
241.270229	11057.507272	27.388122
241.124157	11077.401016	27.393140
241.295181	11084.643075	27.398157
241.708554	11103.132483	27.403175
242.006929	11117.149793	27.408192
242.004298	11131.997356	27.413210
242.123022	11144.609270	27.418228
242.336814	11159.760817	27.423245
242.828952	11173.113132	27.428263
242.937728	11202.190515	27.433280
243.172656	11207.436460	27.438298
243.298502	11228.951840	27.443316
243.934726	11246.478135	27.448333
244.159560	11260.983876	27.453351
243.915032	11266.244951	27.458368
244.058843	11281.836999	27.463386
244.500585	11303.186145	27.468404
244.847914	11316.608612	27.473421
245.361377	11335.117304	27.478439
245.154766	11352.201038	27.483456
245.700458	11363.479993	27.488474
245.477155	11377.727629	27.493492
245.862881	11391.731460	27.498509
246.241795	11407.788852	27.503527
246.517051	11423.047817	27.508544
247.169929	11433.650070	27.513562
246.922463	11457.425088	27.518580
247.351575	11461.181840	27.523597
248.000024	11487.933175	27.528615
247.775028	11494.416433	27.533632
248.152648	11514.354908	27.538650
248.629145	11517.223254	27.543668
248.446811	11542.330192	27.548685
248.640742	11547.923685	27.553703
249.242673	11569.128048	27.558720
249.348811	11580.343368	27.563738
249.881972	11599.774441	27.568756
249.529300	11617.692824	27.573773
250.032459	11630.472196	27.578791
250.481488	11665.995549	27.583808
250.674173	11676.657400	27.588826
250.637908	11689.972867	27.593844
250.893826	11709.842199	27.598861
251.163817	11741.004515	27.603879
251.325376	11751.548133	27.608896
251.809318	11757.118362	27.613914
252.124424	11782.716086	27.618932
252.195965	11801.828123	27.623949
252.519786	11818.570252	27.628967
252.302407	11840.885324	27.633984
252.487145	11850.942233	27.639002
252.833470	11869.616576	27.644020
253.352812	11903.203139	27.649037
253.593715	11924.603400	27.654055
253.878657	11956.951046	27.659072
254.306374	11966.957323	27.664090
254.678536	11990.335959	27.669108
254.934984	11998.013391	27.674125
255.308280	12016.768915	27.679143
255.250395	12039.242386	27.684160
255.476503	12059.801994	27.689178
255.753087	12073.719225	27.694196
256.021459	12093.773320	27.699213
256.251842	12120.145799	27.704231
256.697776	12146.670858	27.709248
257.150140	12160.551143	27.714266
257.058743	12182.101644	27.719284
256.976780	12196.144603	27.724301
257.978908	12214.792344	27.729319
257.816189	12239.233997	27.734336
257.955288	12255.484413	27.739354
258.339696	12271.535366	27.744372
258.696541	12291.484236	27.749389
259.331585	12300.542447	27.754407
259.217487	12322.693490	27.759424
259.444952	12340.550098	27.764442
259.793829	12363.364437	27.769460
260.107843	12374.882395	27.774477
260.376888	12393.389368	27.779495
260.390424	12413.628983	27.784512
260.615650	12435.108068	27.789530
261.085337	12455.731000	27.794548
261.508496	12472.098154	27.799565
261.620133	12482.403690	27.804583
261.545771	12500.746672	27.809600
262.157178	12515.514924	27.814618
261.975724	12530.050552	27.819636
262.638115	12557.957000	27.824653
262.855225	12574.454415	27.829671
262.730231	12593.958037	27.834688
263.066206	12605.722168	27.839706
263.245514	12636.732802	27.844724
263.995799	12653.696232	27.849741
264.445888	12665.733049	27.854759
264.368860	12691.977641	27.859776
264.639056	12703.906873	27.864794
264.962382	12716.538314	27.869812
265.083286	12740.680396	27.874829
265.494124	12756.629728	27.879847
265.491656	12780.371187	27.884864
265.932286	12794.184304	27.889882
266.327477	12817.209831	27.894900
266.381835	12828.901374	27.899917
266.955298	12838.777916	27.904935
266.786426	12872.938227	27.909952
267.160470	12889.603965	27.914970
267.826325	12903.975569	27.919988
267.950548	12930.485810	27.925005
268.567553	12946.961959	27.930023
268.225190	12962.413659	27.935040
268.602949	12975.084115	27.940058
269.119237	13000.291971	27.945076
269.451448	13018.748608	27.950093
269.758973	13038.560728	27.955111
269.744858	13063.946494	27.960128
269.730521	13084.630147	27.965146
270.076085	13100.176303	27.970164
270.268326	13132.344690	27.975181
270.573238	13140.024470	27.980199
270.965227	13170.759499	27.985216
270.973362	13194.730347	27.990234
271.576670	13216.754263	27.995252
271.705064	13252.292933	28.000269
272.298422	13256.280115	28.005287
272.311672	13294.243278	28.010304
272.711725	13310.358982	28.015322
273.384837	13325.475056	28.020340
273.332612	13340.692133	28.025357
274.208058	13352.214321	28.030375
274.058514	13367.216132	28.035392
274.501792	13389.492694	28.040410
274.890966	13401.008979	28.045428
275.088274	13416.408088	28.050445
275.567635	13416.898307	28.055463
275.627025	13445.756345	28.060480
275.779590	13450.535803	28.065498
276.383869	13475.578924	28.070516
276.457174	13495.042934	28.075533
276.913941	13504.713888	28.080551
276.800422	13529.121073	28.085568
276.899546	13550.535910	28.090586
277.256786	13561.406742	28.095604
277.679951	13590.912255	28.100621
278.169258	13606.894225	28.105639
278.282405	13631.992382	28.110656
278.711577	13639.412889	28.115674
278.851732	13659.371882	28.120692
279.218574	13675.483625	28.125709
279.357957	13687.553976	28.130727
279.534175	13701.412335	28.135744
279.912093	13715.311743	28.140762
280.227682	13744.755396	28.145780
279.902375	13751.779373	28.150797
280.422913	13767.049181	28.155815
280.477084	13793.915829	28.160832
280.655730	13806.349598	28.165850
281.285046	13820.793945	28.170868
281.062383	13851.901114	28.175885
281.618288	13867.399161	28.180903
281.697915	13894.801995	28.185920
282.072009	13929.005470	28.190938
282.484488	13949.035799	28.195956
282.586712	13975.190921	28.200973
282.967733	13992.756594	28.205991
283.281203	14021.733609	28.211008
283.338048	14051.186687	28.216026
283.973865	14071.510602	28.221044
284.324059	14096.929106	28.226061
284.581181	14111.697260	28.231079
284.677664	14135.832308	28.236096
285.081160	14157.977046	28.241114
285.453526	14175.070525	28.246132
285.697069	14207.996963	28.251149
286.309378	14220.258851	28.256167
286.424349	14247.722977	28.261184
286.598446	14269.695343	28.266202
287.080063	14285.669616	28.271220
287.337606	14305.607739	28.276237
287.760750	14326.625296	28.281255
288.044193	14346.644675	28.286272
288.046092	14370.870633	28.291290
288.630040	14390.135556	28.296308
288.930904	14412.400888	28.301325
288.993722	14437.842756	28.306343
289.438306	14460.366707	28.311360
290.014555	14481.745748	28.316378
290.142422	14498.644113	28.321396
290.149734	14518.691138	28.326413
290.863735	14527.614886	28.331431
290.982865	14553.626036	28.336448
290.887214	14581.941607	28.341466
291.432499	14593.440478	28.346484
291.569900	14630.932076	28.351501
292.072624	14645.450571	28.356519
292.279518	14671.084939	28.361536
292.543044	14697.935856	28.366554
292.856106	14719.615366	28.371572
293.014139	14747.146103	28.376589
293.459946	14777.745812	28.381607
293.751527	14788.365500	28.386624
293.407138	14809.927025	28.391642
294.113923	14832.021879	28.396660
294.348269	14871.358963	28.401677
294.509080	14882.403443	28.406695
294.605545	14912.802274	28.411712
295.018122	14960.348336	28.416730
295.467634	14971.328693	28.421748
295.936022	15002.013655	28.426765
295.791703	15030.116434	28.431783
296.620426	15055.110686	28.436800
296.822249	15085.967029	28.441818
297.283250	15104.206545	28.446836
297.612173	15139.417284	28.451853
298.221004	15158.713828	28.456871
298.407703	15172.012598	28.461888
298.635340	15201.627033	28.466906
298.969793	15218.920043	28.471924
298.962665	15231.617557	28.476941
299.407972	15255.958357	28.481959
299.451912	15277.143745	28.486976
299.402743	15294.383217	28.491994
300.101340	15322.180676	28.497012
299.908197	15350.591613	28.502029
300.720077	15367.074081	28.507047
300.813326	15399.195474	28.512064
301.114566	15434.685866	28.517082
301.694968	15453.191261	28.522100
302.055006	15463.491084	28.527117
302.290174	15487.700864	28.532135
302.914239	15513.435245	28.537152
303.353992	15533.680892	28.542170
303.692693	15557.287088	28.547188
303.708080	15568.263152	28.552205
303.942626	15589.002123	28.557223
304.296476	15610.401476	28.562240
304.182091	15628.791633	28.567258
304.718735	15660.007039	28.572276
304.842887	15687.358091	28.577293
304.980302	15703.832802	28.582311
305.234651	15738.784702	28.587328
305.691125	15770.622415	28.592346
305.960345	15786.767027	28.597364
306.296660	15816.444348	28.602381
306.479073	15846.692226	28.607399
307.027322	15869.078421	28.612416
307.089913	15899.705210	28.617434
307.738185	15932.801779	28.622452
307.744122	15964.820934	28.627469
307.994400	15993.128615	28.632487
308.480652	16016.450113	28.637504
309.156028	16052.378914	28.642522
309.125927	16081.005429	28.647540
309.231018	16107.677841	28.652557
309.929972	16140.195150	28.657575
310.597059	16158.621322	28.662592
310.281158	16190.255399	28.667610
310.662429	16210.864669	28.672628
311.203284	16236.483559	28.677645
311.494456	16263.629234	28.682663
311.675174	16288.060169	28.687680
312.003575	16317.720552	28.692698
312.519065	16337.260318	28.697716
312.589391	16370.002827	28.702733
313.209753	16392.921598	28.707751
313.549158	16420.947476	28.712768
313.749321	16452.160025	28.717786
314.009234	16475.580705	28.722804
314.190484	16497.879831	28.727821
314.429978	16534.266308	28.732839
315.330965	16548.474342	28.737856
315.094968	16596.527182	28.742874
315.716226	16617.026649	28.747892
315.622311	16633.699477	28.752909
316.243113	16664.979138	28.757927
316.581112	16696.470552	28.762944
316.436487	16721.082499	28.767962
317.082267	16744.218805	28.772980
317.655072	16779.947092	28.777997
317.619452	16817.037335	28.783015
318.128835	16839.174905	28.788032
318.526973	16857.602817	28.793050
319.104522	16874.417040	28.798068
319.347837	16907.676637	28.803085
319.421181	16925.384798	28.808103
320.370322	16945.179428	28.813120
320.471646	16969.535222	28.818138
321.327201	16975.819482	28.823156
321.085786	16997.815839	28.828173
321.455180	17013.064543	28.833191
321.661264	17026.235215	28.838208
321.649646	17041.265668	28.843226
322.454601	17054.203571	28.848244
322.416127	17074.487851	28.853261
322.714929	17105.490172	28.858279
323.126861	17115.002578	28.863296
323.557175	17142.857334	28.868314
323.715011	17163.976417	28.873332
324.299724	17185.363469	28.878349
324.758824	17207.970499	28.883367
325.023345	17225.206781	28.888384
325.021299	17253.255768	28.893402
325.392468	17276.546283	28.898420
325.548533	17294.134430	28.903437
325.628848	17327.066514	28.908455
326.449951	17331.113651	28.913472
326.730375	17369.080929	28.918490
327.138383	17394.178881	28.923508
327.202849	17419.141159	28.928525
327.540406	17444.054375	28.933543
327.994278	17455.689319	28.938560
328.142025	17492.704753	28.943578
328.329030	17511.886540	28.948596
328.537338	17536.491618	28.953613
328.624408	17574.571712	28.958631
329.204496	17605.240172	28.963648
329.229087	17633.620358	28.968666
329.555152	17666.514524	28.973684
330.225695	17701.970194	28.978701
330.739056	17736.806173	28.983719
331.020671	17768.545068	28.988736
331.189854	17807.080246	28.993754
331.424884	17827.139264	28.998772
331.789151	17853.324947	29.003789
332.063322	17900.385073	29.008807
332.585055	17926.205044	29.013824
332.605653	17960.430007	29.018842
332.929886	17994.853850	29.023860
333.576940	18023.920473	29.028877
333.848249	18065.346223	29.033895
334.129018	18086.567088	29.038912
334.508804	18133.187958	29.043930
334.615612	18159.673403	29.048948
335.068667	18196.136949	29.053965
334.959574	18239.075698	29.058983
335.897798	18270.352458	29.064000
336.072756	18302.064709	29.069018
336.900353	18333.529476	29.074036
337.465724	18355.729508	29.079053
337.778442	18390.471737	29.084071
338.141228	18407.851619	29.089088
338.138899	18434.967345	29.094106
338.353394	18461.587956	29.099124
338.713863	18494.111710	29.104141
339.356659	18528.088584	29.109159
339.612299	18547.475444	29.114176
339.628882	18578.795987	29.119194
340.193241	18614.402628	29.124212
340.264700	18643.617201	29.129229
340.766435	18688.893580	29.134247
341.424227	18712.406266	29.139264
341.494111	18744.773789	29.144282
341.885506	18771.423973	29.149300
342.194731	18806.306482	29.154317
342.057501	18836.248987	29.159335
342.871977	18862.485546	29.164352
343.108186	18892.224331	29.169370
343.445378	18923.286719	29.174388
344.056086	18948.563417	29.179405
343.960295	18977.968951	29.184423
344.657785	18998.879140	29.189440
344.754445	19038.596913	29.194458
344.801119	19054.984445	29.199476
345.439408	19091.584917	29.204493
345.897570	19112.311591	29.209511
346.267365	19146.370215	29.214528
346.606189	19173.749422	29.219546
346.975009	19202.684490	29.224564
347.399906	19229.904982	29.229581
347.462039	19262.767374	29.234599
348.220230	19289.038597	29.239616
348.473023	19313.714769	29.244634
348.855274	19345.175118	29.249652
349.174007	19371.572151	29.254669
349.554109	19405.616976	29.259687
350.133449	19427.620187	29.264704
350.460977	19454.230765	29.269722
350.682656	19480.668419	29.274740
350.984926	19503.757584	29.279757
351.244250	19534.681510	29.284775
351.746970	19554.030668	29.289792
351.957079	19590.098934	29.294810
352.178419	19613.144043	29.299828
353.004838	19654.182949	29.304845
353.041106	19682.166249	29.309863
353.368980	19705.523318	29.314880
353.429249	19740.617079	29.319898
353.784151	19766.105494	29.324916
354.617723	19789.206544	29.329933
355.044918	19823.661714	29.334951
355.178613	19854.087739	29.339968
355.618917	19880.125237	29.344986
355.819672	19921.831340	29.350004
356.126912	19952.154515	29.355021
356.494317	19986.530883	29.360039
356.954634	20012.439060	29.365056
357.152909	20048.383660	29.370074
357.341882	20075.699148	29.375092
357.787130	20114.164045	29.380109
358.166712	20153.359579	29.385127
358.369098	20181.728253	29.390144
358.741385	20219.004324	29.395162
359.282631	20265.567084	29.400180
359.613229	20291.862406	29.405197
360.018037	20335.085394	29.410215
360.328561	20361.643004	29.415232
361.100662	20390.434520	29.420250
361.155990	20423.622154	29.425268
361.549160	20448.094536	29.430285
361.887302	20487.189816	29.435303
362.119638	20514.644443	29.440320
362.882033	20543.778894	29.445338
363.201655	20576.811658	29.450356
363.489846	20599.575765	29.455373
363.836668	20638.688942	29.460391
364.213687	20669.097070	29.465408
364.620985	20699.639505	29.470426
364.364254	20730.930478	29.475444
365.351872	20763.441907	29.480461
365.607001	20805.583655	29.485479
365.852526	20829.618394	29.490496
366.284737	20863.316393	29.495514
367.027025	20899.240518	29.500532
367.019348	20926.973416	29.505549
367.551963	20958.893003	29.510567
367.876271	20980.426112	29.515584
367.907198	21019.955999	29.520602
367.959391	21047.622822	29.525620
368.258051	21075.845017	29.530637
368.928172	21119.931716	29.535655
369.206525	21150.166486	29.540672
369.907081	21191.082997	29.545690
369.995960	21231.811070	29.550708
370.639197	21249.895138	29.555725
371.153935	21270.191891	29.560743
371.864052	21299.935916	29.565760
371.983807	21328.028531	29.570778
372.590367	21360.499539	29.575796
373.091520	21379.452673	29.580813
373.428262	21404.661722	29.585831
373.657442	21429.666500	29.590848
373.842132	21463.435889	29.595866
374.423027	21495.778450	29.600884
374.744520	21518.032911	29.605901
375.080209	21553.074122	29.610919
375.677137	21570.514918	29.615936
376.044706	21598.423771	29.620954
376.208313	21631.684938	29.625972
376.737002	21647.057645	29.630989
377.101116	21682.524304	29.636007
377.527003	21703.612620	29.641024
378.204167	21739.257819	29.646042
378.220627	21771.910399	29.651060
378.397303	21803.274191	29.656077
378.546532	21835.053049	29.661095
378.987707	21866.110122	29.666112
379.440620	21886.992201	29.671130
379.293283	21934.311275	29.676148
380.546690	21971.819133	29.681165
380.776069	21997.943023	29.686183
380.988418	22028.745530	29.691200
381.599434	22060.300765	29.696218
382.015432	22098.401307	29.701236
382.272604	22112.268794	29.706253
382.574223	22151.777497	29.711271
383.172768	22187.480050	29.716288
383.335109	22225.645844	29.721306
383.864939	22255.722855	29.726324
384.206003	22281.336753	29.731341
384.534565	22312.007756	29.736359
385.012341	22348.178158	29.741376
384.909294	22378.120687	29.746394
385.255810	22416.213766	29.751412
386.129160	22454.199120	29.756429
386.487984	22495.348790	29.761447
386.517451	22530.730368	29.766464
387.103316	22561.146609	29.771482
386.833901	22602.091594	29.776500
387.459419	22640.286737	29.781517
387.687100	22674.329490	29.786535
388.490177	22714.967698	29.791552
388.661722	22751.464838	29.796570
389.041205	22794.848829	29.801588
389.549702	22827.084844	29.806605
390.374095	22871.865336	29.811623
390.463166	22902.151385	29.816640
391.077319	22949.802252	29.821658
390.812133	22989.786868	29.826676
391.649943	23024.903687	29.831693
391.828899	23060.743045	29.836711
392.446562	23107.603848	29.841728
392.648576	23123.926192	29.846746
392.817852	23171.407145	29.851764
393.552102	23195.949567	29.856781
393.741827	23231.275691	29.861799
394.228725	23267.054546	29.866816
394.993097	23302.790002	29.871834
395.120123	23337.178253	29.876852
395.554480	23370.798032	29.881869
395.961568	23412.839369	29.886887
396.318947	23442.761932	29.891904
396.886169	23475.349995	29.896922
397.054914	23512.531447	29.901940
397.952764	23542.596996	29.906957
398.362534	23582.932065	29.911975
398.523302	23609.258397	29.916992
398.888398	23636.841899	29.922010
399.090509	23674.005786	29.927028
399.379576	23707.143343	29.932045
399.753990	23749.342171	29.937063
399.781270	23776.877670	29.942080
400.442565	23818.039568	29.947098
400.874877	23854.700100	29.952116
401.196925	23896.957996	29.957133
401.846880	23943.436541	29.962151
402.154271	23979.832496	29.967168
402.603604	24032.655776	29.972186
402.972132	24073.554405	29.977204
403.581025	24098.989661	29.982221
404.230055	24144.331315	29.987239
404.418051	24181.422522	29.992256
405.407132	24195.341126	29.997274
405.724408	24238.365148	30.002292
406.128541	24267.055638	30.007309
406.673896	24297.531432	30.012327
406.768677	24330.574063	30.017344
407.684534	24359.898639	30.022362
407.890116	24388.854227	30.027380
408.428991	24420.715205	30.032397
409.043117	24445.587641	30.037415
409.181228	24481.423303	30.042432
409.954532	24499.635317	30.047450
409.680444	24532.919326	30.052468
410.070487	24564.923918	30.057485
410.374331	24599.646859	30.062503
411.112806	24637.543751	30.067520
411.351935	24665.268475	30.072538
411.802084	24700.202500	30.077556
412.251360	24733.664242	30.082573
412.565572	24772.544194	30.087591
412.781344	24804.083530	30.092608
413.308590	24834.348108	30.097626
413.796759	24870.906955	30.102644
414.075166	24911.467505	30.107661
414.717839	24945.784068	30.112679
414.948497	24975.444383	30.117696
415.403923	25010.137970	30.122714
415.508880	25058.448717	30.127732
415.655365	25098.783837	30.132749
416.113907	25144.625253	30.137767
416.472085	25188.687669	30.142784
416.803774	25227.167615	30.147802
417.314654	25271.952033	30.152820
417.691008	25323.646252	30.157837
418.188983	25360.779559	30.162855
418.603769	25405.977478	30.167872
418.985669	25445.511714	30.172890
419.466096	25495.009711	30.177908
419.383755	25529.415552	30.182925
420.535897	25571.123516	30.187943
420.855433	25612.254147	30.192960
421.342962	25652.277838	30.197978
421.694737	25692.221753	30.202996
421.975279	25729.825875	30.208013
422.584176	25759.668257	30.213031
422.931809	25803.822149	30.218048
423.632833	25832.411490	30.223066
424.269960	25870.592021	30.228084
424.177955	25899.008630	30.233101
425.180377	25934.079493	30.238119
425.290710	25965.213718	30.243136
425.793246	25994.125101	30.248154
426.205347	26032.069422	30.253172
426.334273	26076.650010	30.258189
426.815708	26108.295136	30.263207
426.887999	26158.023008	30.268224
426.833302	26193.986713	30.273242
427.549027	26242.760795	30.278260
428.598078	26292.949059	30.283277
429.054813	26332.814597	30.288295
429.342249	26380.467905	30.293312
430.371297	26418.335277	30.298330
430.734271	26453.936975	30.303348
431.006888	26482.316250	30.308365
431.593136	26521.687860	30.313383
431.448106	26571.406543	30.318400
432.033619	26604.742606	30.323418
432.582537	26648.196866	30.328436
432.456592	26694.499922	30.333453
433.003598	26731.482702	30.338471
433.211658	26792.440971	30.343488
433.861325	26827.063013	30.348506
434.386716	26874.673889	30.353524
434.701819	26922.791841	30.358541
435.686874	26964.174916	30.363559
435.980626	27012.087851	30.368576
436.660414	27042.698429	30.373594
437.093925	27092.580584	30.378612
437.511851	27133.730495	30.383629
438.085860	27173.377064	30.388647
438.097376	27216.796626	30.393664
438.793503	27250.786392	30.398682
439.041278	27299.269724	30.403700
439.337969	27341.317588	30.408717
440.178664	27383.545792	30.413735
440.605913	27418.507064	30.418752
441.325049	27456.273227	30.423770
441.668974	27490.109981	30.428788
441.877221	27534.839357	30.433805
442.561389	27567.889767	30.438823
442.702684	27610.499772	30.443840
443.369227	27652.629401	30.448858
443.745132	27686.878631	30.453876
443.684880	27735.664071	30.458893
444.618035	27767.658190	30.463911
444.767773	27825.569512	30.468928
445.381485	27860.521299	30.473946
445.366805	27914.710491	30.478964
445.893401	27959.978755	30.483981
446.605529	27990.775315	30.488999
447.065081	28047.842336	30.494016
447.317665	28088.874697	30.499034
447.724670	28123.164032	30.504052
448.081135	28178.288142	30.509069
448.699500	28224.124125	30.514087
448.572560	28278.407712	30.519104
449.193411	28326.569576	30.524122
449.580840	28375.128399	30.529140
450.082055	28421.406667	30.534157
450.930230	28458.212674	30.539175
451.214539	28499.316738	30.544192
451.563005	28551.573448	30.549210
452.275375	28591.371765	30.554228
452.280452	28633.512209	30.559245
452.665950	28678.222642	30.564263
453.350374	28730.578889	30.569280
453.656704	28779.145051	30.574298
454.173381	28822.842870	30.579316
454.120465	28871.971195	30.584333
455.012668	28926.754246	30.589351
455.234229	28985.226481	30.594368
455.786740	29035.796368	30.599386
455.975362	29088.484024	30.604404
456.550977	29146.920227	30.609421
457.043652	29192.721174	30.614439
457.648908	29255.824295	30.619456
457.949711	29303.014569	30.624474
458.370216	29360.988952	30.629492
458.879518	29420.751107	30.634509
459.613654	29465.566675	30.639527
460.033127	29524.755337	30.644544
460.257237	29579.859691	30.649562
461.141806	29631.516842	30.654580
461.606219	29679.365039	30.659597
462.487794	29734.449005	30.664615
462.839196	29783.023119	30.669632
463.288570	29826.626151	30.674650
463.709009	29871.883654	30.679668
464.157368	29920.095236	30.684685
464.634553	29976.317802	30.689703
465.175130	30017.340511	30.694720
465.360879	30074.506615	30.699738
466.163372	30117.416501	30.704756
466.602535	30173.304207	30.709773
466.765720	30221.529552	30.714791
467.409823	30276.955586	30.719808
467.596943	30324.949854	30.724826
468.176685	30373.919447	30.729844
468.515827	30439.311969	30.734861
469.101572	30479.285486	30.739879
469.441918	30541.416280	30.744896
469.822951	30600.708867	30.749914
470.609956	30653.603902	30.754932
470.722071	30712.565961	30.759949
471.338267	30761.606620	30.764967
471.653051	30825.942160	30.769984
472.317033	30876.410597	30.775002
473.017580	30935.723634	30.780020
472.735923	30994.703918	30.785037
473.641562	31047.688845	30.790055
474.101560	31109.151472	30.795072
474.335853	31167.533061	30.800090
475.049430	31225.694346	30.805108
474.911453	31293.869962	30.810125
475.720169	31355.316628	30.815143
476.158521	31411.157222	30.820160
476.944761	31475.079556	30.825178
477.425947	31540.965359	30.830196
477.930899	31599.236226	30.835213
478.438948	31645.735592	30.840231
479.292990	31711.841695	30.845248
479.610816	31767.550400	30.850266
479.783023	31822.219990	30.855284
480.092248	31875.818834	30.860301
480.561728	31940.241061	30.865319
481.379689	31996.124916	30.870336
481.760591	32048.435954	30.875354
482.322028	32093.764725	30.880372
482.662365	32143.945544	30.885389
483.401184	32191.174936	30.890407
483.975446	32240.478528	30.895424
484.166839	32296.271665	30.900442
485.089100	32344.022685	30.905460
485.245321	32398.057764	30.910477
485.648136	32444.758731	30.915495
486.021080	32510.000732	30.920512
486.727469	32570.613531	30.925530
487.164515	32622.683295	30.930548
487.390570	32676.973683	30.935565
488.067776	32725.573185	30.940583
488.717694	32787.978296	30.945600
488.922230	32845.395626	30.950618
489.027610	32897.252489	30.955636
489.509692	32962.270172	30.960653
489.811472	33026.500732	30.965671
490.339435	33092.472609	30.970688
490.800145	33155.173979	30.975706
491.589639	33224.734279	30.980724
491.928029	33299.018669	30.985741
492.378581	33354.148122	30.990759
493.145933	33416.068855	30.995776
493.645788	33490.202184	31.000794
494.297097	33547.292240	31.005812
494.640264	33610.316851	31.010829
495.401093	33667.276275	31.015847
496.256711	33729.961764	31.020864
496.992042	33776.550390	31.025882
497.936424	33838.564767	31.030900
498.305823	33898.500776	31.035917
498.707137	33940.109393	31.040935
499.163956	33984.883291	31.045952
499.485904	34042.291820	31.050970
500.231849	34093.431694	31.055988
500.569183	34151.837070	31.061005
501.071032	34196.269269	31.066023
501.655510	34257.873381	31.071040
502.096563	34308.011981	31.076058
502.583270	34354.836826	31.081076
502.936359	34420.372378	31.086093
503.678693	34465.886585	31.091111
503.759156	34523.814764	31.096128
504.374762	34581.128180	31.101146
504.958545	34639.420431	31.106164
505.183673	34696.042917	31.111181
505.933152	34750.465315	31.116199
506.860861	34800.844998	31.121216
507.181829	34852.944780	31.126234
507.794709	34907.148711	31.131252
508.459672	34966.649443	31.136269
508.716380	35010.344045	31.141287
509.340722	35057.945562	31.146304
509.653193	35122.326249	31.151322
510.664194	35164.556265	31.156340
511.021338	35225.876334	31.161357
511.357310	35274.598390	31.166375
512.206813	35325.623859	31.171392
512.151537	35379.453105	31.176410
512.823458	35425.498882	31.181428
513.149723	35486.343996	31.186445
513.867701	35541.589019	31.191463
514.095444	35594.723218	31.196480
514.607369	35649.558186	31.201498
515.331480	35704.568721	31.206516
515.500254	35755.448919	31.211533
515.872493	35815.788255	31.216551
516.420846	35869.037323	31.221568
516.563276	35930.968450	31.226586
517.011648	35977.271741	31.231604
517.541427	36050.075171	31.236621
518.161554	36107.025258	31.241639
518.387711	36171.928487	31.246656
519.149268	36235.356962	31.251674
519.712890	36295.433723	31.256692
520.182902	36350.846145	31.261709
520.625263	36413.054177	31.266727
521.073343	36478.423114	31.271744
521.694959	36554.312265	31.276762
521.952899	36615.329381	31.281780
522.579778	36686.709681	31.286797
522.709666	36750.124797	31.291815
523.459594	36815.814240	31.296832
524.175128	36881.180457	31.301850
525.202649	36955.780728	31.306868
525.793180	37026.042290	31.311885
525.912832	37083.319975	31.316903
526.527236	37150.486056	31.321920
526.704480	37225.233082	31.326938
527.675947	37283.610963	31.331956
528.188353	37347.005873	31.336973
528.371230	37418.217856	31.341991
529.199659	37483.214109	31.347008
529.360782	37539.980632	31.352026
530.122605	37622.718982	31.357044
530.410018	37692.644461	31.362061
531.047830	37781.713792	31.367079
531.562949	37839.273027	31.372096
531.900123	37909.709955	31.377114
532.719869	37985.667990	31.382132
533.609855	38055.095554	31.387149
534.182647	38122.682229	31.392167
534.617807	38175.322383	31.397184
535.230758	38254.899313	31.402202
535.531334	38310.109349	31.407220
536.138597	38388.188926	31.412237
537.144155	38450.611867	31.417255
537.660955	38510.853929	31.422272
538.645338	38583.442975	31.427290
539.355204	38632.790758	31.432308
540.055439	38686.807189	31.437325
541.016801	38746.645115	31.442343
541.580641	38785.815664	31.447360
541.834286	38843.032768	31.452378
542.836457	38879.232151	31.457396
543.087278	38935.659449	31.462413
543.835106	38979.955560	31.467431
544.587085	39017.244139	31.472448
544.925940	39068.054947	31.477466
545.668158	39109.847900	31.482484
546.136851	39159.019640	31.487501
546.339192	39192.201776	31.492519
546.894508	39251.029606	31.497536
547.685954	39296.135336	31.502554
548.059837	39338.726335	31.507572
548.520750	39395.311647	31.512589
548.923714	39441.572590	31.517607
549.279213	39494.316966	31.522624
549.431957	39560.152570	31.527642
549.864416	39611.829045	31.532660
550.533840	39667.010066	31.537677
551.179378	39730.467006	31.542695
551.757200	39785.099821	31.547712
551.765854	39847.164336	31.552730
552.594676	39900.853766	31.557748
553.248194	39955.664880	31.562765
553.548035	40017.987841	31.567783
554.310771	40067.330608	31.572800
554.657896	40134.269551	31.577818
554.629193	40184.748426	31.582836
555.348430	40251.540908	31.587853
555.566176	40328.214897	31.592871
556.430173	40388.445736	31.597888
556.643876	40453.458644	31.602906
557.406669	40517.310597	31.607924
558.049180	40586.443506	31.612941
558.397611	40663.237340	31.617959
559.024768	40724.012154	31.622976
559.610906	40796.841728	31.627994
560.412156	40864.957710	31.633012
560.712760	40945.959506	31.638029
561.148440	41020.875189	31.643047
561.504778	41091.313100	31.648064
562.415863	41167.773922	31.653082
562.986623	41239.608088	31.658100
563.246328	41315.684446	31.663117
563.718970	41399.127582	31.668135
564.412395	41471.246879	31.673152
564.958272	41545.628469	31.678170
565.421907	41629.061239	31.683188
566.371527	41707.927632	31.688205
566.776441	41770.118950	31.693223
567.674740	41852.023466	31.698240
568.392577	41928.593100	31.703258
568.814001	41996.417889	31.708276
569.664820	42067.243196	31.713293
570.097527	42142.137864	31.718311
570.848548	42212.473277	31.723328
570.987427	42279.457700	31.728346
571.932183	42351.363419	31.733364
572.775720	42412.735186	31.738381
573.056817	42498.445196	31.743399
573.928367	42563.917912	31.748416
574.859322	42635.972195	31.753434
575.364601	42702.299638	31.758452
575.904160	42772.638328	31.763469
575.819592	42845.099016	31.768487
576.385986	42911.151859	31.773504
577.036794	42982.719838	31.778522
577.929385	43049.088863	31.783540
578.249911	43118.653337	31.788557
578.639054	43206.000030	31.793575
579.321972	43279.923234	31.798592
579.721056	43358.129043	31.803610
580.980963	43432.354555	31.808628
581.484771	43490.063267	31.813645
581.654687	43572.290640	31.818663
582.600477	43629.785013	31.823680
583.175723	43705.231919	31.828698
583.422356	43777.454015	31.833716
583.995408	43847.417669	31.838733
584.554167	43920.204905	31.843751
585.347921	43995.802011	31.848768
585.929077	44079.200305	31.853786
586.431653	44150.567544	31.858804
587.188160	44220.800934	31.863821
587.544859	44297.498565	31.868839
588.203678	44370.733362	31.873856
588.717982	44448.716212	31.878874
589.119172	44524.471473	31.883892
589.914891	44592.745294	31.888909
590.513688	44672.240155	31.893927
590.913905	44729.335738	31.898944
591.756503	44799.633373	31.903962
591.935917	44866.321931	31.908980
593.007165	44930.245857	31.913997
594.093134	45005.104791	31.919015
594.536027	45061.467082	31.924032
594.804939	45129.534062	31.929050
595.217786	45200.469576	31.934068
596.415293	45267.006205	31.939085
596.776527	45341.973441	31.944103
597.344926	45399.854093	31.949120
597.791725	45477.193210	31.954138
598.129758	45542.309105	31.959156
598.985383	45612.385844	31.964173
598.960024	45687.522316	31.969191
600.076532	45762.790179	31.974208
600.480223	45840.896406	31.979226
600.929184	45916.933552	31.984244
601.710509	45984.037235	31.989261
602.419586	46074.103144	31.994279
603.018730	46144.398835	31.999296
603.402541	46222.768865	32.004314
604.115183	46306.148518	32.009332
604.708542	46385.878030	32.014349
605.081142	46468.210797	32.019367
605.869354	46544.766278	32.024384
606.252612	46622.106620	32.029402
607.140820	46702.683060	32.034420
607.859044	46782.660115	32.039437
608.212409	46873.841394	32.044455
609.009337	46948.884910	32.049472
609.405548	47032.544542	32.054490
609.659030	47113.481225	32.059508
610.683639	47189.717181	32.064525
611.231253	47292.263407	32.069543
611.995679	47359.753400	32.074560
612.711083	47438.967722	32.079578
613.778986	47510.250747	32.084596
614.761314	47588.632988	32.089613
615.184061	47659.188757	32.094631
616.262656	47735.747068	32.099648
617.136318	47802.563316	32.104666
617.237080	47860.827177	32.109684
618.294529	47925.153996	32.114701
618.520158	47993.533718	32.119719
619.135541	48062.384037	32.124736
619.402569	48141.601433	32.129754
619.974862	48224.908890	32.134772
620.588463	48300.770077	32.139789
620.876916	48379.232074	32.144807
621.417954	48456.769050	32.149824
622.230623	48534.807843	32.154842
622.608270	48620.007269	32.159860
623.170744	48695.915734	32.164877
624.177705	48785.692672	32.169895
624.591172	48857.246896	32.174912
625.606664	48945.011209	32.179930
626.108914	49025.846121	32.184948
626.858747	49094.298881	32.189965
627.375377	49175.587600	32.194983
627.904377	49254.046554	32.200000
628.328444	49331.048041	32.205018
628.735746	49404.211969	32.210036
629.951664	49487.195449	32.215053
630.471078	49574.533704	32.220071
630.807426	49642.287289	32.225088
631.395640	49724.325977	32.230106
631.913017	49807.584513	32.235124
632.727080	49884.646989	32.240141
633.504770	49953.281428	32.245159
634.035951	50033.855941	32.250176
634.744572	50107.911325	32.255194
635.201613	50187.295833	32.260212
636.043744	50258.508888	32.265229
636.824072	50334.780930	32.270247
637.318799	50412.255828	32.275264
638.040271	50483.830143	32.280282
638.677420	50557.391984	32.285300
639.070217	50628.689205	32.290317
639.483035	50725.235687	32.295335
640.337082	50794.562997	32.300352
641.452584	50876.213160	32.305370
641.725736	50959.577366	32.310388
642.786366	51037.155550	32.315405
642.976144	51117.167219	32.320423
643.770364	51193.205799	32.325440
644.386329	51268.797987	32.330458
645.178131	51351.405340	32.335476
645.672374	51432.901658	32.340493
646.186694	51520.640360	32.345511
646.724979	51599.542416	32.350528
647.720671	51679.474099	32.355546
647.812082	51758.630177	32.360564
648.917315	51854.035190	32.365581
649.294069	51945.435400	32.370599
649.705659	52033.748951	32.375616
650.352804	52114.894670	32.380634
651.142540	52208.559813	32.385652
651.765301	52296.385693	32.390669
652.201361	52387.322748	32.395687
652.969644	52471.930991	32.400704
653.638949	52554.315005	32.405722
654.187986	52664.598461	32.410740
654.693665	52759.360710	32.415757
655.738986	52852.672014	32.420775
656.251104	52950.889041	32.425792
656.849015	53037.329454	32.430810
657.541814	53141.492531	32.435828
658.896803	53217.791593	32.440845
660.278062	53295.700425	32.445863
660.496689	53376.480991	32.450880
661.421641	53454.556730	32.455898
662.097023	53545.043141	32.460916
662.746884	53616.979998	32.465933
663.310512	53702.004408	32.470951
663.561904	53777.838981	32.475968
664.661090	53855.458452	32.480986
664.783783	53948.545234	32.486004
665.687929	54028.322078	32.491021
666.690573	54118.613891	32.496039
667.516674	54196.403814	32.501056
668.069257	54260.586813	32.506074
668.584780	54358.081424	32.511092
668.854374	54431.896528	32.516109
669.740356	54511.095645	32.521127
670.462723	54597.035005	32.526144
671.293061	54670.250442	32.531162
671.875990	54770.432070	32.536180
672.592230	54845.444189	32.541197
673.109573	54926.436405	32.546215
673.719041	55012.648088	32.551232
674.466634	55094.997077	32.556250
674.862340	55180.831496	32.561268
675.736241	55258.471864	32.566285
676.662471	55340.160877	32.571303
676.546809	55430.075905	32.576320
677.429029	55506.133642	32.581338
678.296120	55582.383848	32.586356
679.111402	55648.402722	32.591373
679.832699	55735.270342	32.596391
680.288698	55811.389472	32.601408
680.910827	55889.944682	32.606426
681.759917	55975.160365	32.611444
682.578736	56047.457855	32.616461
683.310838	56123.053758	32.621479
684.309523	56200.405518	32.626496
684.902372	56280.833580	32.631514
685.182546	56368.772530	32.636532
685.851253	56442.714897	32.641549
686.932759	56534.908509	32.646567
687.291817	56606.444281	32.651584
687.988640	56689.477581	32.656602
688.879220	56772.556772	32.661620
689.186379	56841.341970	32.666637
690.001746	56934.787621	32.671655
690.686599	57020.298558	32.676672
690.903290	57101.598387	32.681690
691.847022	57206.442496	32.686708
692.111758	57299.931492	32.691725
693.167874	57385.404573	32.696743
693.575777	57482.162971	32.701760
694.102861	57563.561318	32.706778
694.727052	57678.906890	32.711796
696.048334	57772.466439	32.716813
696.683247	57874.975720	32.721831
697.008032	57960.527391	32.726848
697.956868	58068.121325	32.731866
698.299822	58163.316638	32.736884
699.356622	58259.096758	32.741901
699.818347	58359.957951	32.746919
700.662100	58461.183803	32.751936
701.110217	58551.028530	32.756954
702.163471	58646.627185	32.761972
702.675573	58747.298545	32.766989
703.543073	58854.769460	32.772007
704.028848	58964.275425	32.777024
704.633621	59055.793785	32.782042
705.288031	59161.052448	32.787060
706.397301	59266.702393	32.792077
707.237737	59368.179393	32.797095
707.418220	59459.632792	32.802112
708.270310	59557.576834	32.807130
708.846842	59674.667335	32.812148
709.809533	59777.449790	32.817165
710.661060	59870.097224	32.822183
711.083677	59991.656804	32.827200
712.266534	60083.417633	32.832218
712.521107	60196.870796	32.837236
712.968558	60291.975767	32.842253
713.796797	60400.719266	32.847271
714.542134	60503.386888	32.852288
715.526225	60602.536104	32.857306
716.287145	60704.132371	32.862324
716.924346	60805.223046	32.867341
717.954488	60903.397781	32.872359
718.878856	61003.855613	32.877376
720.000269	61100.428010	32.882394
720.719314	61194.709017	32.887412
721.231108	61290.523067	32.892429
722.060015	61384.255866	32.897447
722.715081	61487.903904	32.902464
723.303444	61574.123250	32.907482
723.998720	61666.548715	32.912500
724.757328	61750.925258	32.917517
725.915505	61830.339929	32.922535
725.968462	61928.494520	32.927552
726.777394	62002.058319	32.932570
727.468938	62090.371281	32.937588
727.871359	62186.655377	32.942605
729.029112	62278.561250	32.947623
729.509637	62379.803174	32.952640
730.574112	62469.622684	32.957658
731.171414	62556.926542	32.962676
731.753770	62647.480555	32.967693
732.552018	62737.735209	32.972711
733.013561	62848.597963	32.977728
733.576001	62948.911454	32.982746
734.139922	63046.699236	32.987764
735.099635	63150.553395	32.992781
735.736768	63248.906584	32.997799
736.597163	63356.296952	33.002816
737.020902	63467.149379	33.007834
737.593827	63571.876178	33.012852
738.235077	63682.644851	33.017869
739.262399	63784.984354	33.022887
739.472046	63901.563538	33.027904
740.542116	64011.253592	33.032922
741.324952	64126.395606	33.037940
741.673461	64241.175665	33.042957
742.585741	64357.887507	33.047975
742.893615	64477.442141	33.052992
744.326597	64595.428354	33.058010
744.729236	64713.278913	33.063028
745.784335	64828.476466	33.068045
746.543968	64951.818168	33.073063
747.275353	65066.763613	33.078080
748.046779	65185.444968	33.083098
748.626434	65299.136354	33.088116
749.505835	65414.629999	33.093133
750.376241	65530.929634	33.098151
751.276562	65656.177407	33.103168
751.944890	65773.921655	33.108186
753.032722	65886.060922	33.113204
753.424002	66002.602360	33.118221
754.120433	66112.296734	33.123239
755.003802	66230.224684	33.128256
755.667038	66341.849969	33.133274
757.306456	66447.757596	33.138292
757.854529	66564.929184	33.143309
759.102876	66666.872187	33.148327
759.625971	66778.135108	33.153344
760.239686	66896.424938	33.158362
761.541511	66992.884131	33.163380
761.891697	67108.265722	33.168397
762.823510	67203.314733	33.173415
763.128701	67315.848768	33.178432
763.948420	67427.916496	33.183450
765.318885	67517.820024	33.188468
766.318866	67614.974656	33.193485
767.414964	67711.614400	33.198503
768.364090	67806.909872	33.203520
769.014789	67896.427233	33.208538
769.885027	67995.629775	33.213556
770.665097	68086.045642	33.218573
771.400903	68177.304555	33.223591
771.840965	68271.161829	33.228608
772.341849	68370.613608	33.233626
773.402429	68466.577908	33.238644
774.339826	68566.050731	33.243661
775.295700	68643.194690	33.248679
776.075188	68744.275907	33.253696
776.659081	68825.176513	33.258714
777.392699	68908.396761	33.263732
777.937865	68991.532809	33.268749
778.574418	69087.059251	33.273767
779.269265	69167.449654	33.278784
779.791663	69267.762668	33.283802
780.624217	69364.202917	33.288820
780.950096	69467.238614	33.293837
781.816774	69558.203289	33.298855
782.047002	69666.409116	33.303872
782.695847	69788.537661	33.308890
783.284242	69897.017634	33.313908
783.998087	70009.948982	33.318925
784.772626	70127.025290	33.323943
785.237128	70253.319855	33.328960
785.955916	70377.447544	33.333978
786.833149	70495.066665	33.338996
787.470674	70627.832953	33.344013
788.824647	70747.202284	33.349031
789.545112	70869.723606	33.354048
790.260130	70992.828942	33.359066
791.053133	71115.162740	33.364084
791.727924	71248.230291	33.369101
792.676069	71370.249685	33.374119
793.353426	71496.478904	33.379136
794.002211	71617.951056	33.384154
794.681324	71744.548480	33.389172
795.235731	71879.816507	33.394189
796.756328	72009.551108	33.399207
797.366598	72142.303968	33.404224
798.119108	72273.034058	33.409242
799.219143	72397.010243	33.414260
799.481585	72538.001563	33.419277
800.280236	72659.442362	33.424295
801.291635	72786.600692	33.429312
802.158101	72920.748568	33.434330
803.589074	73037.241041	33.439348
804.639533	73173.590589	33.444365
805.685484	73294.894237	33.449383
806.408567	73411.461197	33.454400
807.197870	73532.312134	33.459418
808.041490	73654.168412	33.464436
808.607927	73779.222559	33.469453
809.567685	73899.263152	33.474471
810.428364	74027.438975	33.479488
811.504923	74144.777097	33.484506
812.376466	74258.981203	33.489524
812.971991	74383.932284	33.494541
813.995005	74494.022362	33.499559
814.882818	74607.959404	33.504576
815.676398	74729.790405	33.509594
816.589221	74837.150457	33.514612
817.481333	74966.161844	33.519629
818.190523	75076.645451	33.524647
818.495294	75189.371557	33.529664
819.620575	75315.130690	33.534682
820.929515	75427.447208	33.539700
821.622230	75547.688975	33.544717
822.352394	75655.815578	33.549735
823.512735	75768.258117	33.554752
823.906156	75891.601081	33.559770
824.249720	76011.038199	33.564788
825.257975	76133.576615	33.569805
826.206244	76263.446773	33.574823
826.746447	76381.752658	33.579840
827.575338	76504.447505	33.584858
828.366372	76619.016209	33.589876
828.855409	76752.811571	33.594893
829.858081	76866.360093	33.599911
830.670648	76977.874004	33.604928
831.476497	77102.830017	33.609946
832.256366	77218.695106	33.614964
832.683850	77345.332966	33.619981
833.839024	77458.784059	33.624999
834.646332	77587.732484	33.630016
835.019156	77722.652903	33.635034
835.860000	77849.899775	33.640052
836.603376	77976.440406	33.645069
837.792788	78104.888035	33.650087
838.464869	78237.724519	33.655104
839.266766	78371.086058	33.660122
840.694845	78488.362542	33.665140
841.245060	78625.438584	33.670157
842.555434	78751.970000	33.675175
842.834234	78878.030090	33.680192
843.601072	79015.758253	33.685210
844.926046	79135.486024	33.690228
845.693025	79266.070208	33.695245
846.720142	79401.010386	33.700263
847.411738	79529.289200	33.705280
848.253905	79652.287380	33.710298
849.122498	79776.194139	33.715316
849.789958	79909.761493	33.720333
850.799452	80037.422756	33.725351
851.756317	80168.006774	33.730368
853.033543	80314.111840	33.735386
853.807819	80440.924925	33.740404
854.759650	80558.386073	33.745421
855.484741	80691.555383	33.750439
856.319855	80828.737018	33.755456
857.305951	80949.083096	33.760474
857.993937	81076.495368	33.765492
858.603559	81213.562152	33.770509
859.306998	81344.482733	33.775527
860.454701	81473.649267	33.780544
861.101206	81617.820029	33.785562
862.458027	81737.756671	33.790580
863.433054	81874.287990	33.795597
864.117402	81999.132981	33.800615
865.221927	82145.477321	33.805632
865.718783	82278.905256	33.810650
866.649149	82419.640037	33.815668
867.144447	82552.321954	33.820685
868.130330	82677.946288	33.825703
868.848941	82822.466655	33.830720
869.214705	82971.236946	33.835738
870.496244	83116.709643	33.840756
871.620908	83255.542886	33.845773
872.508703	83396.757974	33.850791
873.560509	83523.490733	33.855808
874.326877	83669.312996	33.860826
875.312129	83806.599560	33.865844
875.728954	83944.457283	33.870861
876.964853	84085.823995	33.875879
877.981925	84227.884563	33.880896
878.901856	84364.246362	33.885914
880.016658	84494.521462	33.890932
880.952242	84630.565290	33.895949
881.600654	84764.196491	33.900967
882.323389	84902.302338	33.905984
882.861252	85045.430335	33.911002
884.208143	85185.555933	33.916020
884.821995	85328.115883	33.921037
885.454648	85472.650362	33.926055
886.241341	85607.176157	33.931072
887.045962	85751.444334	33.936090
888.592970	85887.968559	33.941108
888.806198	86025.766705	33.946125
889.745765	86155.658540	33.951143
891.108452	86293.974927	33.956160
891.926929	86429.931477	33.961178
892.711078	86560.571756	33.966196
893.806348	86687.501652	33.971213
894.628583	86815.108461	33.976231
895.646133	86946.524937	33.981248
896.197880	87090.788634	33.986266
897.369013	87218.304549	33.991284
898.505517	87354.012832	33.996301
898.888254	87496.074631	34.001319
899.963774	87628.600260	34.006336
900.836152	87778.570462	34.011354
901.568383	87912.899941	34.016372
902.324834	88062.889738	34.021389
903.524556	88196.969890	34.026407
904.496214	88335.103654	34.031424
905.109525	88484.915236	34.036442
906.343246	88623.300786	34.041460
907.356232	88765.700878	34.046477
908.230443	88912.077388	34.051495
908.914401	89054.834536	34.056512
909.799611	89205.899838	34.061530
911.081085	89358.538713	34.066548
911.518513	89518.179486	34.071565
912.201208	89671.661443	34.076583
913.056139	89811.049650	34.081600
913.577748	89969.678443	34.086618
914.581949	90139.626094	34.091636
915.548329	90293.168201	34.096653
916.256112	90453.722145	34.101671
917.491655	90611.418743	34.106688
918.014770	90783.840709	34.111706
919.205703	90948.618088	34.116724
920.173184	91100.009557	34.121741
921.440200	91262.786913	34.126759
922.523413	91419.345563	34.131776
923.606736	91581.722473	34.136794
924.496755	91731.925176	34.141812
926.152416	91881.083512	34.146829
927.242511	92028.239857	34.151847
927.901606	92180.863722	34.156864
928.482897	92338.101390	34.161882
929.576577	92488.009765	34.166900
930.633359	92636.441718	34.171917
931.267720	92798.553189	34.176935
932.624229	92943.403450	34.181952
933.398100	93104.430010	34.186970
933.977256	93253.928374	34.191988
934.846486	93406.233917	34.197005
935.636489	93559.541271	34.202023
936.547802	93721.918445	34.207040
937.557332	93885.345810	34.212058
938.391309	94053.123784	34.217076
939.273382	94217.219296	34.222093
939.726988	94380.799696	34.227111
940.885794	94545.588788	34.232128
942.029057	94713.943008	34.237146
943.157778	94876.545701	34.242164
944.053117	95033.950743	34.247181
945.123558	95198.693751	34.252199
946.205796	95360.938653	34.257216
947.196690	95520.017062	34.262234
948.241021	95678.073840	34.267252
949.100882	95830.329353	34.272269
950.103304	95994.351993	34.277287
951.297313	96127.593288	34.282304
952.493711	96266.399600	34.287322
953.848219	96422.028443	34.292340
954.102862	96558.511636	34.297357
955.180496	96696.514481	34.302375
956.267370	96824.654268	34.307392
957.266156	96970.213094	34.312410
958.124798	97116.821328	34.317428
958.968183	97253.075894	34.322445
959.857643	97409.061293	34.327463
961.164436	97552.229395	34.332480
961.704474	97709.158341	34.337498
962.557437	97852.969306	34.342516
963.720833	98001.562188	34.347533
964.467963	98169.451794	34.352551
965.672349	98314.832460	34.357568
966.251707	98478.351050	34.362586
967.344777	98622.203943	34.367604
968.179775	98779.193376	34.372621
969.155459	98943.121335	34.377639
970.307873	99090.098304	34.382656
971.459571	99238.952301	34.387674
972.680399	99392.423407	34.392692
973.879507	99540.295213	34.397709
974.808948	99701.242392	34.402727
975.525897	99845.679418	34.407744
976.594858	100004.729982	34.412762
977.416087	100171.274594	34.417780
978.681020	100303.317826	34.422797
980.163821	100446.319131	34.427815
981.236066	100600.148844	34.432832
981.810707	100754.703767	34.437850
983.394538	100903.548460	34.442868
984.204112	101040.965372	34.447885
984.907334	101205.619363	34.452903
986.085618	101349.686553	34.457920
986.899127	101502.927118	34.462938
987.894933	101652.640655	34.467956
988.476981	101822.121773	34.472973
989.029920	101987.855516	34.477991
990.210628	102133.586632	34.483008
991.024968	102313.607735	34.488026
991.700760	102469.486132	34.493044
992.531226	102650.406721	34.498061
993.574003	102825.881245	34.503079
994.491656	102986.947837	34.508096
995.240839	103169.075784	34.513114
996.235841	103349.758880	34.518132
997.296880	103533.082523	34.523149
997.981725	103713.511853	34.528167
998.783656	103899.921049	34.533184
999.790772	104087.833338	34.538202
1000.920786	104269.679431	34.543220
1002.084971	104455.502467	34.548237
1002.909806	104642.622242	34.553255
1003.918667	104829.245104	34.558272
1005.173547	105017.491498	34.563290
1005.938069	105203.901094	34.568308
1007.360708	105382.892500	34.573325
1008.047067	105576.302885	34.578343
1009.503195	105747.315409	34.583360
1010.473937	105939.237835	34.588378
1011.493766	106122.518607	34.593396
1012.186036	106313.180701	34.598413
1013.087494	106494.782880	34.603431
1014.470769	106675.144011	34.608448
1015.771632	106870.570427	34.613466
1016.557410	107055.883637	34.618484
1017.945679	107229.754588	34.623501
1018.578586	107401.031069	34.628519
1019.734605	107567.268429	34.633536
1020.406772	107737.513313	34.638554
1021.333066	107911.282499	34.643572
1022.357880	108101.078193	34.648589
1023.165889	108275.134016	34.653607
1024.068466	108461.932802	34.658624
1025.190699	108638.135026	34.663642
1026.692457	108823.193425	34.668660
1028.051943	108994.960019	34.673677
1028.943293	109183.172016	34.678695
1029.988150	109369.560268	34.683712
1031.120131	109529.356062	34.688730
1031.630929	109723.273671	34.693748
1032.922998	109901.674885	34.698765
1033.938465	110081.895705	34.703783
1034.822456	110268.098317	34.708800
1035.884723	110463.645653	34.713818
1036.762883	110646.034024	34.718836
1038.192501	110829.643206	34.723853
1038.938279	111039.205783	34.728871
1039.795683	111213.205001	34.733888
1040.804176	111412.190062	34.738906
1042.265598	111605.436490	34.743924
1043.404615	111782.742426	34.748941
1045.038462	111977.282796	34.753959
1046.371231	112148.954732	34.758976
1048.037133	112313.447940	34.763994
1049.057593	112495.481052	34.769012
1050.388143	112650.554659	34.774029
1051.874680	112812.237388	34.779047
1053.454428	112978.662159	34.784064
1054.409027	113145.248981	34.789082
1055.323931	113307.720957	34.794100
1056.644917	113460.491309	34.799117
1057.472053	113622.876974	34.804135
1058.559363	113778.944690	34.809152
1059.201859	113945.989888	34.814170
1060.343618	114109.419179	34.819188
1061.458852	114268.224102	34.824205
1062.035798	114438.097408	34.829223
1062.963346	114607.650266	34.834240
1063.872345	114778.576580	34.839258
1064.757895	114952.069347	34.844276
1065.535850	115137.983917	34.849293
1066.306076	115317.406816	34.854311
1067.177874	115512.402458	34.859328
1068.164300	115690.398152	34.864346
1069.182791	115890.382743	34.869364
1070.341598	116078.829826	34.874381
1071.516133	116260.375543	34.879399
1072.339618	116461.636719	34.884416
1073.455342	116651.044708	34.889434
1074.247155	116847.214073	34.894452
1075.432306	117054.941265	34.899469
1075.953210	117243.570184	34.904487
1077.043794	117445.847583	34.909504
1077.855405	117654.981064	34.914522
1078.805922	117863.586591	34.919540
1079.894076	118076.357493	34.924557
1081.129488	118295.156916	34.929575
1082.080753	118507.038395	34.934592
1083.351981	118711.932603	34.939610
1083.710990	118938.508924	34.944628
1085.313516	119138.736410	34.949645
1086.500266	119351.600464	34.954663
1087.349278	119563.529170	34.959680
1088.827989	119766.455777	34.964698
1089.879723	119983.733381	34.969716
1091.142167	120176.598903	34.974733
1092.249886	120372.787691	34.979751
1093.770931	120552.701346	34.984768
1095.470914	120738.181926	34.989786
1095.991235	120934.566992	34.994804
1097.320083	121125.181563	34.999821
1098.642419	121314.199745	35.004839
1099.778145	121498.820887	35.009856
1100.597301	121687.488346	35.014874
1101.420564	121899.383069	35.019892
1102.799843	122089.119137	35.024909
1103.919510	122296.009565	35.029927
1104.892828	122493.752288	35.034944
1106.034695	122689.427218	35.039962
1107.096171	122892.168969	35.044980
1108.286672	123087.064414	35.049997
1108.799799	123295.336275	35.055015
1110.051932	123499.192995	35.060032
1111.345876	123698.248902	35.065050
1112.782771	123913.724555	35.070068
1114.262752	124109.797528	35.075085
1115.384558	124318.157017	35.080103
1116.437591	124509.046691	35.085120
1117.607768	124714.571621	35.090138
1118.798203	124916.631040	35.095156
1119.818188	125124.135263	35.100173
1120.893919	125323.512452	35.105191
1122.123596	125538.432939	35.110208
1123.522571	125730.872708	35.115226
1124.385866	125939.585467	35.120244
1125.543836	126146.806866	35.125261
1126.424513	126349.632333	35.130279
1127.524409	126556.319355	35.135296
1128.912825	126760.488288	35.140314
1129.858841	126976.082367	35.145332
1131.187006	127181.924812	35.150349
1132.216667	127389.603897	35.155367
1133.428005	127597.001832	35.160384
1134.348591	127809.673473	35.165402
1135.562390	128021.653238	35.170420
1136.418706	128228.513584	35.175437
1137.686960	128449.621916	35.180455
1138.114965	128671.560768	35.185472
1139.594125	128895.543868	35.190490
1140.255572	129129.971244	35.195508
1141.224760	129360.938738	35.200525
1142.464652	129588.883474	35.205543
1143.374230	129815.485476	35.210560
1144.406098	130049.479295	35.215578
1145.076806	130289.545051	35.220596
1146.655161	130522.859566	35.225613
1147.910378	130760.717542	35.230631
1148.794584	131009.267643	35.235648
1150.528089	131244.617271	35.240666
1151.183864	131476.266948	35.245684
1152.862042	131716.360558	35.250701
1154.205155	131949.947992	35.255719
1155.291092	132201.708905	35.260736
1156.840535	132432.297491	35.265754
1157.908218	132668.482297	35.270772
1158.680584	132902.620955	35.275789
1159.989430	133127.731237	35.280807
1161.108726	133366.259135	35.285824
1162.691799	133598.180891	35.290842
1163.656408	133833.398317	35.295860
1165.011149	134049.065443	35.300877
1166.433462	134266.588341	35.305895
1167.738900	134480.539542	35.310912
1169.245016	134690.310952	35.315930
1170.500408	134893.257658	35.320948
1171.797461	135099.485310	35.325965
1173.483467	135288.560319	35.330983
1175.679052	135466.947921	35.336000
1177.329049	135641.957389	35.341018
1178.584805	135828.348373	35.346036
1179.464573	136011.144361	35.351053
1180.527168	136187.136158	35.356071
1181.308705	136378.159230	35.361088
1182.386506	136559.086391	35.366106
1183.349731	136750.767821	35.371124
1184.362130	136945.779799	35.376141
1185.360441	137136.670568	35.381159
1186.114773	137345.531316	35.386176
1187.460704	137546.851317	35.391194
1188.587813	137755.033739	35.396212
1189.576506	137958.746433	35.401229
1190.573254	138167.471402	35.406247
1191.348440	138391.967964	35.411264
1192.343872	138610.669696	35.416282
1193.595260	138835.741041	35.421300
1194.428694	139067.414490	35.426317
1195.756688	139298.707080	35.431335
1196.564467	139519.675936	35.436352
1197.944425	139752.193592	35.441370
1198.703857	139996.637287	35.446388
1200.389080	140227.853090	35.451405
1201.757959	140461.480032	35.456423
1202.699828	140697.814668	35.461440
1204.229122	140932.053330	35.466458
1205.473044	141165.766704	35.471476
1206.407740	141410.888153	35.476493
1207.680521	141651.972886	35.481511
1208.704353	141887.742083	35.486528
1210.463310	142120.326045	35.491546
1211.724477	142362.291800	35.496564
1212.616006	142602.907863	35.501581
1214.063818	142851.636714	35.506599
1215.096851	143093.210260	35.511616
1216.471482	143330.213295	35.516634
1217.878865	143568.088059	35.521652
1219.091420	143813.888709	35.526669
1220.307983	144049.536510	35.531687
1220.951777	144302.700987	35.536704
1222.538531	144541.694561	35.541722
1223.896048	144782.882787	35.546740
1225.085654	145033.300170	35.551757
1226.627126	145281.061827	35.556775
1227.156844	145533.628400	35.561792
1228.687172	145766.227031	35.566810
1229.719094	146018.818920	35.571828
1231.173519	146273.135529	35.576845
1232.084441	146521.281118	35.581863
1233.563956	146758.207601	35.586880
1234.911153	147011.592691	35.591898
1236.058432	147256.328583	35.596916
1237.411522	147508.306287	35.601933
1238.847077	147755.677536	35.606951
1240.261365	147998.636197	35.611968
1241.597109	148240.554769	35.616986
1242.639376	148487.267524	35.622004
1244.046372	148731.081112	35.627021
1245.758906	148970.595837	35.632039
1246.794286	149203.553787	35.637056
1248.208661	149436.123401	35.642074
1249.742985	149660.665864	35.647092
1250.557625	149894.296020	35.652109
1251.655769	150112.105080	35.657127
1252.626460	150343.072545	35.662144
1254.074125	150565.182515	35.667162
1254.894381	150806.152479	35.672180
1255.861610	151037.618468	35.677197
1257.079552	151272.321117	35.682215
1257.969952	151524.301236	35.687232
1259.252252	151763.057846	35.692250
1260.815081	152006.633257	35.697268
1261.842508	152259.128399	35.702285
1263.274198	152497.826695	35.707303
1264.196672	152754.681786	35.712320
1265.371130	153018.721449	35.717338
1266.428815	153265.491420	35.722356
1268.037685	153518.396264	35.727373
1269.643411	153774.171592	35.732391
1270.561124	154043.206911	35.737408
1272.051269	154296.159178	35.742426
1273.363161	154552.656775	35.747444
1274.484549	154813.488710	35.752461
1276.161612	155067.646453	35.757479
1277.590714	155323.392845	35.762496
1279.201088	155576.941226	35.767514
1280.331166	155837.281305	35.772532
1281.294491	156088.483137	35.777549
1282.975524	156346.898510	35.782567
1284.866896	156595.862611	35.787584
1286.332648	156844.399285	35.792602
1287.474499	157100.680758	35.797620
1288.562916	157352.642741	35.802637
1290.085624	157598.964728	35.807655
1291.053256	157859.339086	35.812672
1292.067510	158112.255282	35.817690
1293.670174	158369.853778	35.822708
1294.882803	158632.528996	35.827725
1296.249585	158883.044607	35.832743
1297.953187	159137.989937	35.837760
1299.247609	159375.937895	35.842778
1300.901189	159627.528825	35.847796
1302.250279	159877.314908	35.852813
1303.555190	160118.920346	35.857831
1305.375499	160372.075113	35.862848
1306.418203	160618.268506	35.867866
1307.449683	160867.955906	35.872884
1308.741682	161122.961073	35.877901
1309.729442	161373.469827	35.882919
1310.706931	161623.841519	35.887936
1312.158291	161877.453614	35.892954
1313.710631	162136.053067	35.897972
1314.864358	162404.301355	35.902989
1316.138498	162653.322931	35.908007
1316.750307	162926.406485	35.913024
1318.148662	163187.408376	35.918042
1319.730113	163452.127995	35.923060
1320.686747	163720.615668	35.928077
1322.260818	163989.363274	35.933095
1323.575296	164267.750971	35.938112
1324.860386	164523.024449	35.943130
1326.451492	164791.836097	35.948148
1327.565480	165053.943619	35.953165
1329.409701	165320.991041	35.958183
1330.919030	165585.730383	35.963200
1332.518603	165853.237170	35.968218
1334.403142	166112.180973	35.973236
1335.507319	166364.696428	35.978253
1336.535911	166613.187085	35.983271
1337.975553	166851.863193	35.988288
1339.016774	167094.525787	35.993306
1340.487070	167331.865573	35.998324
1341.386350	167574.310802	36.003341
1343.183933	167819.371483	36.008359
1344.375319	168066.165804	36.013376
1345.683665	168308.435237	36.018394
1347.189510	168548.516079	36.023412
1348.384723	168782.539047	36.028429
1349.895976	169029.527859	36.033447
1351.333997	169271.665959	36.038464
1352.173343	169525.008635	36.043482
1353.430725	169783.086316	36.048500
1354.441841	170041.736737	36.053517
1355.742616	170288.089785	36.058535
1356.703109	170557.034780	36.063552
1357.895491	170824.446150	36.068570
1359.523677	171097.313663	36.073588
1360.815128	171364.546381	36.078605
1363.124921	171623.049785	36.083623
1364.663952	171880.709695	36.088640
1365.954950	172150.218119	36.093658
1367.283006	172410.744414	36.098676
1368.327901	172669.703296	36.103693
1369.972277	172939.273442	36.108711
1371.115833	173216.554309	36.113728
1372.081664	173500.873203	36.118746
1373.033672	173768.865759	36.123764
1374.134903	174054.511430	36.128781
1375.535071	174337.393960	36.133799
1377.017200	174625.851804	36.138816
1378.137732	174919.090975	36.143834
1379.654473	175197.882189	36.148852
1380.785159	175509.229458	36.153869
1382.524755	175796.889267	36.158887
1384.045287	176087.149423	36.163904
1385.558416	176392.243401	36.168922
1387.252743	176674.795915	36.173940
1388.611483	176968.728894	36.178957
1389.767363	177255.253351	36.183975
1391.733969	177538.451853	36.188992
1392.818266	177836.646694	36.194010
1394.540834	178123.669494	36.199028
1396.005264	178412.917816	36.204045
1397.454832	178692.239063	36.209063
1399.123549	178989.152713	36.214080
1400.542299	179274.525223	36.219098
1402.537224	179552.214587	36.224116
1403.659849	179826.942834	36.229133
1405.329103	180105.218240	36.234151
1407.063765	180366.569317	36.239168
1408.519973	180659.966079	36.244186
1409.866754	180915.614119	36.249204
1411.412274	181205.976291	36.254221
1412.837261	181466.998004	36.259239
1414.313164	181743.962546	36.264256
1415.620187	182027.456299	36.269274
1417.016788	182288.814921	36.274292
1418.079799	182566.506862	36.279309
1419.105920	182847.684977	36.284327
1420.479856	183125.101282	36.289344
1421.321829	183417.459850	36.294362
1423.254353	183703.095732	36.299380
1424.195505	183995.973878	36.304397
1425.729122	184285.813889	36.309415
1427.279105	184577.023726	36.314432
1428.456860	184859.580808	36.319450
1429.767321	185151.083786	36.324468
1431.177448	185431.345573	36.329485
1432.210394	185715.858034	36.334503
1433.802564	185996.575454	36.339520
1435.111943	186297.225597	36.344538
1436.119893	186629.190495	36.349556
1437.788510	186930.929196	36.354573
1439.686607	187221.076022	36.359591
1441.191077	187498.306020	36.364608
1442.189718	187790.296939	36.369626
1443.937589	188077.726410	36.374644
1445.245647	188378.153998	36.379661
1446.606552	188680.326726	36.384679
1447.785374	188965.764777	36.389696
1449.363981	189266.558813	36.394714
1451.140392	189562.191862	36.399732
1452.626460	189861.757350	36.404749
1454.482493	190154.382241	36.409767
1456.490588	190428.949845	36.414784
1457.726949	190737.497584	36.419802
1459.315181	191023.105255	36.424820
1460.506734	191321.653754	36.429837
1461.417253	191612.804613	36.434855
1463.116393	191921.714782	36.439872
1464.257272	192228.046035	36.444890
1465.287054	192535.690873	36.449908
1466.744609	192842.050279	36.454925
1468.149272	193169.653845	36.459943
1469.892778	193481.863050	36.464960
1471.044621	193805.189655	36.469978
1472.658034	194123.085198	36.474996
1473.705345	194455.751970	36.480013
1475.407286	194781.738208	36.485031
1476.906214	195105.191488	36.490048
1477.686897	195442.627077	36.495066
1479.626051	195765.428794	36.500084
1480.922632	196106.620874	36.505101
1482.318724	196445.994703	36.510119
1484.136010	196779.207048	36.515136
1485.513608	197126.713895	36.520154
1487.163890	197461.757472	36.525172
1488.592409	197801.535844	36.530189
1490.405876	198133.024561	36.535207
1492.249553	198472.307651	36.540224
1493.524463	198810.867654	36.545242
1494.977996	199129.205881	36.550260
1496.497796	199476.848313	36.555277
1498.350295	199813.287927	36.560295
1500.063676	200150.969323	36.565312
1501.040231	200480.942872	36.570330
1503.055184	200811.465823	36.575348
1504.573078	201148.824230	36.580365
1506.419063	201479.044711	36.585383
1508.486563	201807.300576	36.590400
1509.798091	202131.560188	36.595418
1511.489021	202452.661913	36.600436
1512.986784	202776.487114	36.605453
1514.194245	203106.124710	36.610471
1516.054981	203430.783351	36.615488
1517.220725	203762.765681	36.620506
1518.953186	204078.630797	36.625524
1520.182256	204409.156385	36.630541
1521.382101	204738.594786	36.635559
1522.782913	205071.787300	36.640576
1524.039161	205410.159769	36.645594
1525.443473	205745.461273	36.650612
1527.207399	206093.078266	36.655629
1528.348985	206431.673557	36.660647
1529.972632	206762.979471	36.665664
1530.958484	207106.655382	36.670682
1532.428997	207427.494788	36.675700
1533.852710	207768.588267	36.680717
1535.125430	208105.692175	36.685735
1536.720828	208443.558961	36.690752
1538.152040	208790.876518	36.695770
1539.740395	209130.371161	36.700788
1541.368857	209466.506745	36.705805
1542.993978	209817.555054	36.710823
1544.447828	210165.023354	36.715840
1545.357872	210512.450194	36.720858
1547.006388	210876.782200	36.725876
1548.723695	211233.914725	36.730893
1550.186149	211585.422593	36.735911
1552.097712	211939.985221	36.740928
1553.543153	212305.722569	36.745946
1556.035359	212648.103036	36.750964
1557.422319	212996.194833	36.755981
1559.135604	213347.335167	36.760999
1561.164697	213694.514271	36.766016
1562.729744	214049.108010	36.771034
1564.110474	214396.821130	36.776052
1565.644176	214742.503736	36.781069
1567.298611	215106.610888	36.786087
1569.091656	215451.669240	36.791104
1570.419640	215809.578779	36.796122
1572.396943	216163.474804	36.801140
1574.039828	216508.506695	36.806157
1575.683933	216866.672450	36.811175
1577.162071	217212.314925	36.816192
1578.891053	217566.555705	36.821210
1580.198975	217921.573929	36.826228
1581.961042	218274.463585	36.831245
1583.169751	218631.961961	36.836263
1584.882236	218983.919850	36.841280
1586.357604	219357.711653	36.846298
1587.525583	219720.755069	36.851316
1588.885254	220089.408353	36.856333
1590.199779	220465.486847	36.861351
1592.001489	220836.433861	36.866368
1593.535043	221211.843294	36.871386
1595.364292	221592.973309	36.876404
1597.073289	221970.286263	36.881421
1598.935250	222355.577672	36.886439
1600.734766	222724.188488	36.891456
1602.542313	223093.179193	36.896474
1604.768129	223455.931321	36.901492
1606.497566	223810.250825	36.906509
1607.838734	224185.564103	36.911527
1609.455236	224543.889804	36.916544
1611.147444	224908.427682	36.921562
1612.948675	225273.863056	36.926580
1614.199623	225632.398426	36.931597
1615.808260	225994.917057	36.936615
1618.064282	226340.339016	36.941632
1619.923842	226707.568885	36.946650
1621.631789	227061.129636	36.951668
1623.168837	227417.130465	36.956685
1624.298022	227783.585322	36.961703
1626.078650	228129.614897	36.966720
1627.731879	228481.761299	36.971738
1629.711495	228837.082839	36.976756
1631.715252	229192.959381	36.981773
1633.251427	229543.980595	36.986791
1634.443618	229889.923900	36.991808
1636.223855	230245.580991	36.996826
1637.638680	230595.401387	37.001844
1639.131811	230951.001477	37.006861
1640.553684	231304.046742	37.011879
1642.139973	231646.548853	37.016896
1643.210023	231976.937677	37.021914
1644.855478	232325.958970	37.026932
1647.294102	232654.126329	37.031949
1648.822123	232988.482129	37.036967
1650.658705	233319.842578	37.041984
1652.081400	233669.710791	37.047002
1653.820230	234023.035011	37.052020
1655.073760	234372.268682	37.057037
1656.265411	234726.516316	37.062055
1657.748951	235074.417841	37.067072
1659.275200	235450.510573	37.072090
1660.520529	235819.686290	37.077108
1662.289414	236195.130650	37.082125
1663.679485	236572.005716	37.087143
1665.428230	236952.812633	37.092160
1666.606975	237332.590578	37.097178
1668.287938	237717.725874	37.102196
1670.558980	238104.851469	37.107213
1671.998870	238496.679301	37.112231
1674.122895	238873.005045	37.117248
1675.806931	239261.211791	37.122266
1677.361868	239651.953166	37.127284
1679.310103	240041.362284	37.132301
1680.695733	240442.087189	37.137319
1682.526563	240833.571224	37.142336
1683.947197	241233.883004	37.147354
1685.578811	241634.694611	37.152372
1687.183048	242028.523974	37.157389
1688.645665	242440.411116	37.162407
1690.302304	242844.392213	37.167424
1692.030823	243257.125423	37.172442
1693.816180	243669.391734	37.177460
1695.786207	244079.951783	37.182477
1697.027480	244505.739849	37.187495
1698.614589	244918.060216	37.192512
1700.452888	245339.917327	37.197530
1701.524485	245776.830381	37.202548
1703.633245	246209.896776	37.207565
1705.117312	246649.156608	37.212583
1706.837921	247074.127551	37.217600
1708.443251	247511.105574	37.222618
1710.070362	247935.225489	37.227636
1712.030537	248373.644659	37.232653
1713.672149	248825.423432	37.237671
1715.873136	249247.138779	37.242688
1717.603837	249688.867433	37.247706
1719.260281	250128.371151	37.252724
1721.649234	250553.610094	37.257741
1723.380288	250996.478274	37.262759
1725.328719	251407.711161	37.267776
1727.129094	251843.351955	37.272794
1729.125467	252265.929709	37.277812
1730.646864	252699.249345	37.282829
1732.078621	253131.718092	37.287847
1733.874468	253562.299673	37.292864
1735.371765	253989.472082	37.297882
1737.041546	254432.466719	37.302900
1738.980638	254866.146313	37.307917
1740.388022	255307.756747	37.312935
1742.010996	255742.067267	37.317952
1743.603488	256184.661915	37.322970
1745.075150	256639.949103	37.327988
1746.792578	257079.015840	37.333005
1748.087890	257530.593551	37.338023
1749.718042	257982.676071	37.343040
1752.027860	258426.598583	37.348058
1753.835918	258862.139621	37.353076
1756.141600	259274.258176	37.358093
1758.046920	259710.238146	37.363111
1759.896977	260116.786201	37.368128
1762.099345	260536.054028	37.373146
1763.740151	260956.297216	37.378164
1765.690762	261372.299376	37.383181
1767.187390	261790.149043	37.388199
1768.851623	262209.875911	37.393216
1770.712303	262626.090678	37.398234
1772.068642	263053.228434	37.403252
1774.084040	263472.946300	37.408269
1775.737700	263912.657692	37.413287
1777.528295	264333.067725	37.418304
1778.794221	264774.334748	37.423322
1780.468663	265213.199242	37.428340
1782.249861	265650.775196	37.433357
1784.150114	266095.315328	37.438375
1786.386474	266536.676837	37.443392
1787.600862	266973.548339	37.448410
1789.215541	267422.343378	37.453428
1791.595751	267876.070838	37.458445
1793.130895	268331.884057	37.463463
1794.773728	268785.417795	37.468480
1796.673957	269243.252135	37.473498
1798.212136	269717.293969	37.478516
1799.860912	270178.058389	37.483533
1801.642506	270642.050596	37.488551
1803.179570	271122.307714	37.493568
1804.977502	271590.000494	37.498586
1806.656256	272081.278120	37.503604
1808.513648	272544.664365	37.508621
1810.810742	273028.144540	37.513639
1813.030446	273497.030897	37.518656
1814.603180	273968.834931	37.523674
1816.672270	274447.720474	37.528692
1818.700610	274923.866817	37.533709
1820.347402	275401.111355	37.538727
1822.210365	275876.566938	37.543744
1824.559986	276342.674035	37.548762
1826.654578	276816.183111	37.553780
1828.319497	277274.189039	37.558797
1830.445571	277751.395343	37.563815
1832.470740	278224.271899	37.568832
1834.648950	278682.900286	37.573850
1836.098838	279158.299048	37.578868
1837.925498	279621.979610	37.583885
1839.798852	280097.788693	37.588903
1841.164550	280572.632994	37.593920
1843.033015	281035.815714	37.598938
1844.679601	281517.847367	37.603956
1846.760488	281998.081064	37.608973
1848.274405	282473.169126	37.613991
1850.547702	282961.212980	37.619008
1852.196213	283444.729602	37.624026
1853.440491	283927.442769	37.629044
1855.989604	284394.890236	37.634061
1858.542417	284879.220334	37.639079
1859.934702	285354.384023	37.644096
1862.131102	285830.510452	37.649114
1863.588344	286324.549322	37.654132
1865.635655	286791.982632	37.659149
1866.861044	287282.851240	37.664167
1868.693022	287772.884908	37.669184
1870.899768	288246.707100	37.674202
1872.792176	288735.302123	37.679220
1874.534802	289219.981208	37.684237
1876.227035	289706.035621	37.689255
1877.823382	290176.790541	37.694272
1879.866765	290636.858633	37.699290
1881.250730	291106.547995	37.704308
1883.570207	291578.778802	37.709325
1885.496915	292046.624153	37.714343
1887.163902	292522.428250	37.719360
1888.879420	292987.684243	37.724378
1890.683965	293482.476244	37.729396
1892.422996	293954.398537	37.734413
1894.095686	294448.339913	37.739431
1895.848345	294938.481680	37.744448
1897.967031	295436.914983	37.749466
1899.220248	295931.874257	37.754484
1901.267016	296433.686919	37.759501
1903.056416	296948.661116	37.764519
1904.355109	297462.590368	37.769536
1906.483076	297978.136941	37.774554
1908.283556	298505.662105	37.779572
1910.103729	299013.732614	37.784589
1912.107005	299543.983383	37.789607
1913.617211	300071.386714	37.794624
1916.271006	300607.592812	37.799642
1917.790571	301150.089141	37.804660
1920.796654	301654.344652	37.809677
1923.401345	302164.852316	37.814695
1925.608523	302695.014836	37.819712
1927.762978	303202.232048	37.824730
1929.415322	303722.012306	37.829748
1931.894454	304235.641830	37.834765
1933.773088	304755.757084	37.839783
1935.424842	305277.273312	37.844800
1937.687051	305786.352099	37.849818
1939.403782	306318.127970	37.854836
1941.269023	306823.679312	37.859853
1943.276618	307345.169271	37.864871
1945.073974	307865.468274	37.869888
1946.845507	308392.035339	37.874906
1948.777832	308932.709553	37.879924
1951.010034	309452.416040	37.884941
1952.896846	309977.805748	37.889959
1954.770764	310510.425466	37.894976
1957.036037	311033.790021	37.899994
1958.874716	311569.499934	37.905012
1960.777740	312097.249562	37.910029
1963.144032	312625.504524	37.915047
1965.001565	313147.868790	37.920064
1967.307987	313672.694919	37.925082
1969.412955	314196.023825	37.930100
1971.541154	314723.987517	37.935117
1973.392953	315248.054606	37.940135
1975.469222	315770.532418	37.945152
1977.328795	316285.627600	37.950170
1978.901803	316826.215862	37.955188
1980.641014	317356.290559	37.960205
1982.805113	317888.880927	37.965223
1984.313623	318424.891824	37.970240
1986.690318	318969.769080	37.975258
1988.541102	319510.915324	37.980276
1990.059893	320054.593604	37.985293
1992.098769	320595.163915	37.990311
1993.672032	321149.376137	37.995328
1995.979488	321690.220421	38.000346
1998.076945	322245.300556	38.005364
2000.035754	322783.952366	38.010381
2002.254642	323332.071862	38.015399
2004.364886	323893.750759	38.020416
2005.851532	324438.849198	38.025434
2007.601661	324990.496206	38.030452
2009.952840	325519.561402	38.035469
2012.052334	326052.744061	38.040487
2013.947582	326582.551772	38.045504
2016.280318	327105.408287	38.050522
2017.835328	327642.942891	38.055540
2020.009790	328171.341186	38.060557
2021.934489	328706.469401	38.065575
2023.899577	329251.732212	38.070592
2025.526548	329780.499020	38.075610
2027.285222	330331.056051	38.080628
2029.497373	330882.549091	38.085645
2031.293313	331440.010348	38.090663
2033.020205	332007.520298	38.095680
2034.585112	332568.426031	38.100698
2036.558747	333138.873965	38.105716
2038.153712	333728.880141	38.110733
2040.315781	334325.003262	38.115751
2042.162714	334922.231572	38.120768
2043.813059	335512.378477	38.125786
2045.870297	336112.750841	38.130804
2047.706238	336726.464882	38.135821
2050.179611	337332.510107	38.140839
2051.645743	337949.355941	38.145856
2053.978671	338568.084769	38.150874
2056.552039	339185.091318	38.155892
2058.834655	339801.143534	38.160909
2060.776534	340419.673216	38.165927
2062.664927	341046.544674	38.170944
2064.967184	341668.927229	38.175962
2067.658004	342289.843032	38.180980
2069.780598	342914.615445	38.185997
2072.018217	343523.203887	38.191015
2073.933852	344139.566785	38.196032
2076.560927	344748.021861	38.201050
2078.638649	345377.929836	38.206068
2080.634259	345989.022756	38.211085
2083.133638	346615.874714	38.216103
2085.105544	347239.855971	38.221120
2087.389730	347849.652664	38.226138
2089.931580	348473.141266	38.231156
2091.675913	349100.520969	38.236173
2093.787968	349713.657213	38.241191
2096.084128	350336.971393	38.246208
2098.282522	350947.231127	38.251226
2101.079353	351558.906998	38.256244
2102.830821	352166.196432	38.261261
2105.348754	352779.109696	38.266279
2107.192050	353386.386946	38.271296
2109.707300	353984.014899	38.276314
2111.541434	354583.740919	38.281332
2113.888960	355195.721400	38.286349
2116.382366	355795.676034	38.291367
2118.053848	356416.940787	38.296384
2120.377406	357013.831057	38.301402
2122.608291	357619.495239	38.306420
2124.525029	358227.478045	38.311437
2126.908483	358834.640640	38.316455
2129.091882	359440.200142	38.321472
2131.414953	360034.040461	38.326490
2133.720999	360634.284561	38.331508
2135.628246	361253.715702	38.336525
2137.657411	361840.646664	38.341543
2140.040161	362439.195030	38.346560
2142.137664	363029.842935	38.351578
2144.412055	363627.877287	38.356596
2146.507413	364235.913005	38.361613
2148.712597	364826.127782	38.366631
2150.491050	365422.910495	38.371648
2152.381721	365997.944894	38.376666
2154.466501	366578.842149	38.381684
2156.405015	367157.875283	38.386701
2158.578995	367731.082142	38.391719
2160.589561	368315.934292	38.396736
2162.896736	368884.409106	38.401754
2165.433948	369468.344206	38.406772
2167.407514	370059.804999	38.411789
2169.498879	370640.896862	38.416807
2171.257308	371229.680736	38.421824
2173.154545	371819.773313	38.426842
2175.383807	372426.624947	38.431860
2177.072263	373035.093346	38.436877
2179.421408	373628.344915	38.441895
2181.440751	374247.248921	38.446912
2183.797995	374863.400564	38.451930
2185.770864	375470.554162	38.456948
2187.857253	376104.504309	38.461965
2190.099063	376723.899588	38.466983
2192.301359	377358.283333	38.472000
2194.390544	377971.213921	38.477018
2197.191689	378609.451228	38.482036
2199.232366	379241.560859	38.487053
2201.561135	379870.114768	38.492071
2204.145897	380501.298462	38.497088
2206.576426	381124.841846	38.502106
2209.341499	381750.724108	38.507124
2211.227692	382390.633403	38.512141
2213.823309	383005.595781	38.517159
2215.954852	383640.902187	38.522176
2218.202653	384268.121182	38.527194
2220.620830	384892.512381	38.532212
2222.250910	385533.776099	38.537229
2224.090732	386181.828102	38.542247
2226.025301	386829.291523	38.547264
2228.194376	387470.421665	38.552282
2230.421444	388129.909715	38.557300
2232.366710	388791.652616	38.562317
2234.560812	389447.008896	38.567335
2236.443662	390117.588166	38.572352
2238.861413	390789.280781	38.577370
2241.322826	391456.897253	38.582388
2243.419530	392136.603583	38.587405
2245.499823	392813.660532	38.592423
2247.643628	393487.650686	38.597440
2250.053561	394174.440505	38.602458
2252.342999	394849.281062	38.607476
2254.657498	395544.248432	38.612493
2257.135351	396236.638651	38.617511
2259.158471	396918.347355	38.622528
2261.089532	397604.859980	38.627546
2263.771013	398299.182778	38.632564
2266.217479	398988.763452	38.637581
2268.876218	399674.139795	38.642599
2270.966281	400367.835475	38.647616
2272.936983	401059.403171	38.652634
2275.324209	401755.946370	38.657652
2277.249831	402451.123485	38.662669
2279.358646	403143.062307	38.667687
2282.497769	403843.017671	38.672704
2284.974313	404538.854611	38.677722
2287.055774	405215.501479	38.682740
2289.516803	405917.371065	38.687757
2292.078380	406601.947220	38.692775
2294.584753	407290.407351	38.697792
2296.871072	407984.851410	38.702810
2299.120759	408661.620522	38.707828
2301.095096	409340.537031	38.712845
2303.648707	409995.460878	38.717863
2305.955914	410648.379927	38.722880
2308.038929	411317.251153	38.727898
2310.638563	411965.278706	38.732916
2313.031114	412615.848745	38.737933
2315.612654	413267.280202	38.742951
2317.971172	413921.913763	38.747968
2320.089789	414574.490886	38.752986
2322.616060	415237.859716	38.758004
2324.511783	415900.345457	38.763021
2327.226607	416556.865670	38.768039
2329.535166	417231.131527	38.773056
2331.738491	417899.221882	38.778074
2333.977046	418555.855442	38.783092
2336.094514	419227.608870	38.788109
2338.581511	419893.719918	38.793127
2340.869615	420571.067351	38.798144
2342.623825	421254.342108	38.803162
2344.816719	421931.508128	38.808180
2346.987034	422638.286683	38.813197
2349.055711	423329.938219	38.818215
2351.288071	424036.709278	38.823232
2353.235695	424744.309267	38.828250
2356.001178	425453.880057	38.833268
2358.091681	426177.535643	38.838285
2360.195663	426907.229643	38.843303
2362.533527	427641.713556	38.848320
2364.739445	428376.595487	38.853338
2367.211962	429102.865758	38.858356
2369.279447	429855.507872	38.863373
2371.856362	430592.473652	38.868391
2374.549658	431342.989781	38.873408
2376.544053	432105.008843	38.878426
2378.856745	432845.216400	38.883444
2381.442556	433614.108916	38.888461
2383.445662	434372.752819	38.893479
2385.878955	435140.749385	38.898496
2387.989523	435916.092820	38.903514
2390.818226	436675.527364	38.908532
2393.043564	437446.041041	38.913549
2395.840339	438230.480158	38.918567
2398.522547	438997.878372	38.923584
2400.904229	439771.557017	38.928602
2403.542132	440541.880008	38.933620
2405.919351	441320.294823	38.938637
2408.373333	442096.139421	38.943655
2411.203324	442871.892836	38.948672
2413.756155	443636.645785	38.953690
2416.130790	444406.647821	38.958708
2418.746982	445174.913128	38.963725
2420.953668	445949.674843	38.968743
2423.792329	446717.184027	38.973760
2426.012812	447491.373040	38.978778
2428.867242	448261.339508	38.983796
2431.007070	449026.991800	38.988813
2433.155262	449793.317139	38.993831
2435.891315	450573.049509	38.998848
2438.372040	451353.545143	39.003866
2441.530788	452118.956360	39.008884
2443.205732	452898.803387	39.013901
2445.580393	453675.679571	39.018919
2448.112391	454452.799789	39.023936
2450.327093	455234.882114	39.028954
2453.018906	456001.308291	39.033972
2455.094753	456776.730981	39.038989
2458.166975	457559.685368	39.044007
2460.443871	458334.754636	39.049024
2462.504592	459102.454757	39.054042
2464.895259	459855.686589	39.059060
2467.139319	460622.886366	39.064077
2469.621381	461371.293750	39.069095
2472.325749	462126.243476	39.074112
2474.262505	462886.274810	39.079130
2476.308165	463639.342859	39.084148
2478.458749	464420.310829	39.089165
2480.819003	465183.653541	39.094183
2483.348482	465954.754221	39.099200
2485.883025	466748.770588	39.104218
2488.165732	467532.952329	39.109236
2490.273463	468330.541228	39.114253
2492.994953	469135.208124	39.119271
2495.410542	469936.655761	39.124288
2497.763636	470746.042297	39.129306
2500.464045	471549.736811	39.134324
2503.234006	472374.055864	39.139341
2505.215981	473196.237682	39.144359
2507.685798	474013.662666	39.149376
2510.121252	474844.362293	39.154394
2512.729863	475673.277776	39.159412
2515.077638	476507.686312	39.164429
2517.589468	477353.317736	39.169447
2520.137135	478189.825090	39.174464
2522.459032	479049.308746	39.179482
2525.324759	479893.690883	39.184500
2527.764748	480745.352016	39.189517
2530.190206	481606.192006	39.194535
2532.545901	482468.658579	39.199552
2535.049149	483345.012977	39.204570
2537.983635	484215.455736	39.209588
2540.427329	485090.461089	39.214605
2543.313678	485954.968576	39.219623
2546.451732	486822.965110	39.224640
2549.008628	487700.927793	39.229658
2551.896784	488554.305950	39.234676
2554.566685	489415.578809	39.239693
2557.065287	490280.204287	39.244711
2559.814837	491144.640323	39.249728
2562.494405	492019.815475	39.254746
2565.032503	492882.069432	39.259764
2567.562947	493743.217381	39.264781
2570.115996	494611.311370	39.269799
2572.925036	495482.184665	39.274816
2575.127792	496363.624471	39.279834
2577.652978	497231.267167	39.284852
2580.415399	498112.313464	39.289869
2583.144013	498996.835888	39.294887
2585.674125	499864.422675	39.299904
2588.307009	500741.807121	39.304922
2591.317969	501609.617236	39.309940
2594.317828	502484.976506	39.314957
2596.641609	503348.914361	39.319975
2599.415724	504216.755591	39.324992
2601.979586	505086.791148	39.330010
2604.722554	505956.343166	39.335028
2607.360554	506837.128449	39.340045
2609.502818	507699.875563	39.345063
2612.259261	508574.849321	39.350080
2614.686677	509449.065683	39.355098
2617.296222	510326.317767	39.360116
2619.811005	511201.316671	39.365133
2622.174066	512092.478997	39.370151
2625.069960	512967.659466	39.375168
2627.751234	513854.585478	39.380186
2630.313669	514733.578605	39.385204
2632.637608	515616.474874	39.390221
2634.775438	516495.723538	39.395239
2637.996778	517365.546109	39.400256
2640.238615	518230.539872	39.405274
2642.734104	519075.382078	39.410292
2645.248436	519943.391086	39.415309
2647.628527	520811.666961	39.420327
2650.371707	521671.034942	39.425344
2652.839999	522540.190726	39.430362
2655.914237	523410.552181	39.435380
2658.455153	524285.713954	39.440397
2661.015220	525170.412070	39.445415
2663.862902	526048.726035	39.450432
2666.804605	526930.132045	39.455450
2669.396168	527798.121151	39.460468
2672.178420	528689.481447	39.465485
2674.742402	529577.198861	39.470503
2677.693124	530452.239280	39.475520
2680.063962	531348.655837	39.480538
2682.980368	532243.016963	39.485556
2685.813192	533139.639295	39.490573
2688.061386	534046.232622	39.495591
2690.541983	534938.818283	39.500608
2693.150656	535842.818600	39.505626
2696.066260	536758.353584	39.510644
2698.743454	537668.790268	39.515661
2701.069953	538597.185822	39.520679
2703.831318	539515.758813	39.525696
2706.758918	540453.711186	39.530714
2709.615256	541386.636851	39.535732
2712.490308	542314.372102	39.540749
2715.041779	543245.751977	39.545767
2717.827297	544173.814826	39.550784
2720.767475	545121.851151	39.555802
2723.535464	546059.107005	39.560820
2726.583311	547002.217049	39.565837
2728.640186	547951.227979	39.570855
2731.357405	548886.922610	39.575872
2733.842965	549844.747411	39.580890
2736.667384	550805.101749	39.585908
2739.431930	551766.292228	39.590925
2742.501790	552728.511979	39.595943
2745.038105	553685.073729	39.600960
2748.008041	554658.836121	39.605978
2750.505741	555629.385578	39.610996
2753.413283	556609.114666	39.616013
2756.002841	557564.657353	39.621031
2759.088131	558540.942483	39.626048
2762.132875	559523.717786	39.631066
2764.697011	560499.973219	39.636084
2767.667908	561475.132409	39.641101
2770.370826	562443.339553	39.646119
2773.389615	563425.442861	39.651136
2776.056152	564407.518769	39.656154
2778.614934	565385.371947	39.661172
2781.500604	566361.188759	39.666189
2784.154878	567348.076017	39.671207
2786.933285	568336.161361	39.676224
2789.454006	569314.890036	39.681242
2792.248676	570306.258045	39.686260
2795.292621	571290.993807	39.691277
2797.911235	572295.782142	39.696295
2801.078068	573286.082246	39.701312
2803.721471	574287.537458	39.706330
2806.028651	575268.940829	39.711348
2809.543342	576267.732255	39.716365
2812.475858	577256.970108	39.721383
2815.745854	578243.116293	39.726400
2818.619380	579221.934234	39.731418
2821.251833	580192.851122	39.736436
2824.295470	581147.114533	39.741453
2827.053564	582090.288411	39.746471
2829.901493	583032.917620	39.751488
2832.399988	583983.570780	39.756506
2835.121642	584932.106887	39.761524
2837.801091	585879.967498	39.766541
2840.426794	586839.801097	39.771559
2842.939816	587793.019940	39.776576
2845.464379	588762.346223	39.781594
2847.634628	589733.739992	39.786612
2850.507906	590714.180699	39.791629
2853.218737	591715.392701	39.796647
2855.712815	592706.902900	39.801664
2858.233212	593717.999449	39.806682
2861.381515	594745.935051	39.811700
2863.794594	595764.096911	39.816717
2866.860647	596802.884177	39.821735
2869.449303	597822.119092	39.826752
2872.134735	598865.207167	39.831770
2874.559178	599919.216206	39.836788
2877.299671	600967.977845	39.841805
2880.256959	602040.509938	39.846823
2883.394036	603114.350829	39.851840
2885.492322	604186.396544	39.856858
2888.768554	605262.937433	39.861876
2891.919825	606353.056726	39.866893
2894.215909	607456.614488	39.871911
2897.625467	608551.149606	39.876928
2900.395939	609646.814625	39.881946
2903.582845	610763.492926	39.886964
2906.449326	611877.754740	39.891981
2909.139825	612986.735734	39.896999
2912.380519	614093.564414	39.902016
2915.308175	615206.651408	39.907034
2918.596993	616327.035284	39.912052
2922.060238	617433.460542	39.917069
2925.266961	618538.308028	39.922087
2928.204692	619656.927260	39.927104
2932.118614	620774.569997	39.932122
2934.838959	621864.723470	39.937140
2938.659698	622959.465808	39.942157
2941.538145	624049.302470	39.947175
2944.837965	625142.637188	39.952192
2947.953695	626225.122252	39.957210
2951.007849	627315.213993	39.962228
2954.285357	628390.063504	39.967245
2957.068688	629481.098847	39.972263
2959.829883	630561.711073	39.977280
2963.291178	631644.182631	39.982298
2965.693474	632733.116872	39.987316
2968.898146	633822.896251	39.992333
2972.180608	634903.334904	39.997351
2974.956919	635986.416087	40.002368
2977.999088	637071.918355	40.007386
2980.841244	638167.025274	40.012404
2983.721299	639233.405272	40.017421
2986.515144	640326.179776	40.022439
2989.654412	641417.977302	40.027456
2992.159319	642503.433092	40.032474
2994.867469	643606.972318	40.037492
2998.199446	644705.114147	40.042509
3001.110066	645804.930845	40.047527
3003.661040	646907.355854	40.052544
3006.553092	648022.761027	40.057562
3009.715257	649135.653673	40.062580
3012.750175	650231.742028	40.067597
3015.943177	651336.265727	40.072615
3019.314431	652425.432362	40.077632
3022.297642	653493.923607	40.082650
3025.151153	654572.238035	40.087668
3028.394828	655630.705316	40.092685
3031.338218	656693.909493	40.097703
3033.883004	657751.392437	40.102720
3036.961477	658818.690619	40.107738
3039.874924	659898.588642	40.112756
3043.009082	660969.589764	40.117773
3046.034814	662057.443131	40.122791
3048.769001	663142.926867	40.127808
3051.688331	664232.364270	40.132826
3053.808485	665335.774889	40.137844
3057.219232	666441.472725	40.142861
3059.598492	667561.964859	40.147879
3062.589746	668694.162984	40.152896
3065.407950	669832.336744	40.157914
3067.594286	670988.249682	40.162932
3070.661211	672144.316473	40.167949
3073.863603	673328.048625	40.172967
3076.467718	674505.816992	40.177984
3079.222756	675689.887992	40.183002
3081.993013	676894.095597	40.188020
3085.491142	678089.899318	40.193037
3087.879262	679304.074821	40.198055
3090.607477	680522.181081	40.203072
3093.916486	681754.571277	40.208090
3097.271460	683006.567417	40.213108
3100.173773	684237.123448	40.218125
3103.495528	685484.450363	40.223143
3107.028226	686732.151442	40.228160
3109.969529	687988.659626	40.233178
3113.243818	689244.282655	40.238196
3116.570837	690492.933678	40.243213
3119.861254	691771.406218	40.248231
3122.754762	693025.623207	40.253248
3126.110563	694298.057632	40.258266
3129.012346	695575.997426	40.263284
3132.460137	696849.254709	40.268301
3135.422400	698131.822281	40.273319
3138.785114	699411.852343	40.278336
3142.062104	700686.755061	40.283354
3145.355606	701961.848135	40.288372
3148.788212	703229.608705	40.293389
3152.487336	704523.382751	40.298407
3155.436820	705805.270439	40.303424
3159.028353	707077.723548	40.308442
3162.146258	708356.459232	40.313460
3165.458224	709627.657990	40.318477
3168.637450	710911.987058	40.323495
3171.791495	712196.307241	40.328512
3175.449628	713477.330782	40.333530
3178.459711	714756.421678	40.338548
3182.186648	716016.808305	40.343565
3185.750057	717290.960125	40.348583
3188.562359	718557.629719	40.353600
3191.599509	719818.785651	40.358618
3194.925696	721098.453509	40.363636
3198.088371	722355.233323	40.368653
3201.659633	723623.952416	40.373671
3204.523895	724888.288343	40.378688
3207.573719	726157.798778	40.383706
3210.066215	727432.645810	40.388724
3213.482302	728711.807392	40.393741
3216.361075	729998.066937	40.398759
3219.441992	731287.714206	40.403776
3222.878048	732567.396551	40.408794
3225.377131	733864.410868	40.413812
3228.843394	735137.059274	40.418829
3232.030273	736397.295081	40.423847
3234.901209	737645.915955	40.428864
3238.508777	738907.230615	40.433882
3241.266496	740164.777709	40.438900
3244.482664	741432.253765	40.443917
3247.554618	742697.372184	40.448935
3250.485828	743964.502768	40.453952
3253.911900	745233.249903	40.458970
3256.840655	746529.044006	40.463988
3260.208536	747809.913859	40.469005
3263.567111	749094.728212	40.474023
3266.556799	750399.679536	40.479040
3269.922195	751695.506507	40.484058
3272.878158	753008.914150	40.489076
3276.030576	754311.949494	40.494093
3279.773376	755629.555571	40.499111
3282.339211	756962.195807	40.504128
3285.632591	758292.952163	40.509146
3288.843409	759633.023502	40.514164
3291.978221	760978.876007	40.519181
3295.373069	762323.156141	40.524199
3298.099274	763692.791809	40.529216
3302.237715	765059.147145	40.534234
3305.054943	766425.587042	40.539252
3308.521678	767796.549195	40.544269
3311.836309	769179.983140	40.549287
3314.826162	770565.733374	40.554304
3318.436829	771942.890874	40.559322
3321.950573	773330.200845	40.564340
3325.105556	774727.648258	40.569357
3328.584319	776118.990794	40.574375
3332.004232	777521.002634	40.579392
3335.635751	778915.606818	40.584410
3339.040061	780321.240907	40.589428
3342.433626	781731.954365	40.594445
3345.723329	783138.774102	40.599463
3349.343868	784552.470163	40.604480
3353.012905	785961.710310	40.609498
3356.479033	787369.072909	40.614516
3359.665294	788782.911947	40.619533
3363.082527	790195.973075	40.624551
3366.213015	791613.554144	40.629568
3370.028438	793027.991822	40.634586
3373.328131	794444.738692	40.639604
3376.615720	795854.455039	40.644621
3380.551393	797273.800458	40.649639
3383.904394	798694.192563	40.654656
3387.407445	800110.109793	40.659674
3390.850171	801524.800280	40.664692
3394.200349	802933.839388	40.669709
3397.951616	804350.632925	40.674727
3400.855299	805772.547960	40.679744
3404.704321	807173.713453	40.684762
3408.188299	808600.791116	40.689780
3411.824249	810006.518773	40.694797
3415.764576	811403.427469	40.699815
3418.669136	812812.046413	40.704832
3422.645818	814215.905758	40.709850
3425.987742	815614.885806	40.714868
3429.567658	817027.113809	40.719885
3433.132868	818421.834576	40.724903
3436.301001	819820.090349	40.729920
3439.610129	821215.484210	40.734938
3443.084369	822623.443781	40.739956
3446.454890	824026.245986	40.744973
3450.125606	825426.061289	40.749991
3453.509581	826824.922070	40.755008
3457.117080	828208.894922	40.760013
3460.399355	829552.593150	40.765018
3463.625657	830840.522007	40.770023
3466.905349	832071.630610	40.775028
3469.720197	833259.534398	40.780032
3472.952444	834383.825147	40.785037
3475.673845	835446.721970	40.790042
3478.260904	836434.802104	40.795047
3480.911600	837370.880053	40.800052
3483.467614	838257.721927	40.805056
3485.826758	839066.256267	40.810061
3487.968581	839833.870110	40.815066
3490.046560	840543.870055	40.820071
3491.902815	841210.365718	40.825076
3493.628452	841819.003568	40.830080
3495.177166	842374.075583	40.835085
3496.774120	842886.034172	40.840090
3498.674543	843354.171875	40.845095
3500.009000	843774.756841	40.850100
3500.979724	844158.625731	40.855104
3502.344314	844504.116221	40.860109
3503.966718	844828.026302	40.865114
3505.028988	845094.428854	40.870119
3506.365008	845346.722031	40.875124
3506.865429	845547.668374	40.880128
3507.871031	845728.950787	40.885133
3508.802523	845885.331106	40.890138
3509.433250	846002.309247	40.895143
3510.394610	846102.467066	40.900148
3510.770293	846185.657917	40.905152
3511.802681	846241.706301	40.910157
3512.240685	846275.460358	40.915162
3512.772668	846285.649924	40.920167
3513.346913	846290.890354	40.925172
3513.777706	846266.498065	40.930176
3514.268919	846228.819153	40.935181
3514.377197	846187.517137	40.940186
3514.827327	846124.452518	40.945191
3515.187845	846040.370453	40.950196
3515.368374	845965.619402	40.955200
3515.965955	845862.114212	40.960205
3516.182301	845755.080722	40.965210
3516.183897	845637.708116	40.970215
3516.387180	845493.841114	40.975220
3516.495980	845358.805762	40.980224
3516.856089	845210.836364	40.985229
3517.043684	845065.992043	40.990234
3516.799809	844919.272909	40.995239
3517.255836	844736.864678	41.000244
3517.178631	844568.978296	41.005248
3517.191890	844400.297437	41.010253
3517.261556	844230.730412	41.015258
3517.562993	844040.956886	41.020263
3517.598836	843858.587135	41.025268
3516.731214	843664.330518	41.030272
3517.261923	843473.339412	41.035277
3517.112857	843280.412194	41.040282
3517.156127	843080.564092	41.045287
3516.984178	842880.936803	41.050292
3516.771614	842678.593909	41.055296
3516.967157	842481.126004	41.060301
3516.916385	842281.362532	41.065306
3517.009324	842080.987957	41.070311
3516.739249	841875.620136	41.075316
3516.521067	841672.273822	41.080320
3516.680081	841461.296224	41.085325
3516.699046	841265.464198	41.090330
3516.650028	841047.326761	41.095335
3516.505509	840839.187406	41.100340
3516.412156	840637.144062	41.105344
3516.374184	840424.899298	41.110349
3516.045601	840223.751719	41.115354
3515.722505	840011.633754	41.120359
3516.125919	839801.529052	41.125364
3515.682985	839600.863338	41.130368
3515.794277	839389.140350	41.135373
3515.519502	839197.555109	41.140378
3515.439193	838987.788353	41.145383
3515.507261	838779.446539	41.150388
3515.242888	838581.047342	41.155392
3515.111821	838367.870325	41.160397
3514.631848	838169.588164	41.165402
3514.755128	837977.610300	41.170407
3514.779685	837772.345617	41.175412
3514.504651	837588.278670	41.180416
3514.695567	837396.562700	41.185421
3514.406880	837196.956543	41.190426
3514.177464	836992.481229	41.195431
3514.007426	836802.161505	41.200436
3513.783419	836615.726977	41.205440
3513.422219	836427.366610	41.210445
3513.401634	836250.305019	41.215450
3513.622546	836059.803477	41.220455
3513.538515	835872.353104	41.225460
3512.692678	835685.307204	41.230464
3512.929975	835507.503733	41.235469
3513.116264	835327.664044	41.240474
3512.984688	835154.859438	41.245479
3512.617201	834976.455100	41.250484
3512.457604	834818.598118	41.255488
3512.468668	834632.453496	41.260493
3512.385637	834463.991018	41.265498
3512.351579	834299.012050	41.270503
3512.479347	834128.662163	41.275508
3511.673582	833969.038746	41.280512
3511.789157	833785.473602	41.285517
3511.830168	833622.503771	41.290522
3511.086840	833463.925483	41.295527
3511.650925	833291.832620	41.300532
3511.499271	833140.826141	41.305536
3511.462271	832993.100344	41.310541
3511.229296	832836.853979	41.315546
3511.434621	832676.649677	41.320551
3510.857162	832509.861039	41.325556
3510.813272	832358.429555	41.330560
3510.727506	832198.938039	41.335565
3510.949017	832053.577354	41.340570
3510.419714	831910.273468	41.345575
3510.432039	831767.075807	41.350580
3510.184265	831620.320815	41.355584
3510.233807	831477.887689	41.360589
3509.991624	831338.314328	41.365594
3509.992783	831197.339490	41.370599
3509.881674	831048.314602	41.375604
3509.359673	830918.394159	41.380608
3509.572550	830773.684170	41.385613
3509.439244	830652.442083	41.390618
3509.443276	830525.831813	41.395623
3509.483601	830380.847901	41.400628
3509.079659	830253.518342	41.405632
3508.857652	830120.813022	41.410637
3508.837788	829996.527629	41.415642
3508.740392	829870.794116	41.420647
3508.879388	829745.312587	41.425652
3508.675262	829630.183527	41.430656
3508.643113	829503.363180	41.435661
3508.876211	829384.662443	41.440666
3508.751178	829264.363154	41.445671
3508.323009	829137.402685	41.450676
3508.278572	829025.541682	41.455680
3508.337709	828907.636355	41.460685
3508.320577	828790.129449	41.465690
3508.000891	828670.917991	41.470695
3507.919539	828549.820127	41.475700
3508.122277	828455.114445	41.480704
3507.695623	828335.621523	41.485709
3507.649929	828228.023004	41.490714
3507.554151	828116.542114	41.495719
3507.849389	828019.579421	41.500724
3507.502114	827914.452723	41.505728
3507.783172	827803.004393	41.510733
3507.177358	827701.705715	41.515738
3506.920831	827603.947728	41.520743
3507.642170	827488.925064	41.525748
3507.282118	827401.485049	41.530752
3507.225114	827292.899579	41.535757
3507.011200	827182.489477	41.540762
3506.609810	827096.412655	41.545767
3506.624070	827000.936028	41.550772
3506.500995	826911.701882	41.555776
3506.577101	826807.948294	41.560781
3506.502698	826732.413093	41.565786
3506.381229	826639.091066	41.570791
3506.843200	826544.412387	41.575796
3506.415391	826452.593883	41.580800
3506.163342	826364.246995	41.585805
3506.205248	826271.185510	41.590810
3505.874065	826182.848366	41.595815
3506.009236	826109.606413	41.600820
3505.887087	826027.263184	41.605824
3505.521800	825947.679629	41.610829
3505.709878	825867.425074	41.615834
3505.650055	825791.584221	41.620839
3505.926551	825705.868031	41.625844
3505.673328	825646.101151	41.630848
3505.596946	825560.535332	41.635853
3505.767735	825475.513176	41.640858
3505.656421	825398.605753	41.645863
3505.518193	825327.439433	41.650868
3505.352465	825264.056820	41.655872
3505.472835	825171.452591	41.660877
3505.553302	825115.810299	41.665882
3505.345271	825037.357370	41.670887
3505.699393	824964.261989	41.675892
3505.213005	824889.060172	41.680896
3505.071862	824821.973299	41.685901
3504.925139	824745.938547	41.690906
3504.962574	824679.308501	41.695911
3504.961628	824618.616784	41.700916
3505.162336	824552.446152	41.705920
3504.892319	824479.928880	41.710925
3504.832504	824407.572424	41.715930
3504.756992	824343.874381	41.720935
3505.082255	824281.280248	41.725940
3504.512938	824224.175137	41.730944
3504.604345	824158.892768	41.735949
3504.669476	824086.707535	41.740954
3504.250025	824031.522631	41.745959
3504.436645	823969.044258	41.750964
3504.320083	823912.254558	41.755968
3504.428246	823854.553725	41.760973
3504.246493	823796.994946	41.765978
3504.095441	823740.111767	41.770983
3504.471708	823685.674857	41.775988
3504.189053	823635.815290	41.780992
3504.338315	823578.105435	41.785997
3503.885691	823518.446233	41.791002
3504.189624	823465.283325	41.796007
3504.362781	823417.490923	41.801012
3503.896259	823365.517693	41.806016
3503.897555	823303.839787	41.811021
3504.063870	823245.248584	41.816026
3503.758862	823209.495343	41.821031
3504.058335	823144.266946	41.826036
3504.004047	823098.453347	41.831040
3503.839105	823043.122477	41.836045
3504.093241	822998.621955	41.841050
3503.590769	822952.974620	41.846055
3503.593320	822905.399485	41.851060
3503.525774	822855.499954	41.856064
3503.896414	822793.953778	41.861069
3503.455487	822755.494961	41.866074
3503.413730	822714.346586	41.871079
3503.779993	822659.804867	41.876084
3503.424958	822614.813030	41.881088
3503.127735	822566.114592	41.886093
3503.227533	822529.515747	41.891098
3503.250428	822497.209763	41.896103
3503.478433	822449.012075	41.901108
3503.263339	822422.288856	41.906112
3503.332300	822373.045158	41.911117
3503.234240	822334.335509	41.916122
3503.169845	822297.371753	41.921127
3503.200566	822259.030700	41.926132
3502.784863	822210.347965	41.931136
3502.964815	822174.318286	41.936141
3503.153222	822135.368002	41.941146
3502.973205	822105.816152	41.946151
3502.991396	822065.432490	41.951156
3502.975723	822030.697498	41.956160
3502.955928	821988.470491	41.961165
3502.957992	821946.239778	41.966170
3503.085964	821913.622391	41.971175
3503.327131	821870.575335	41.976180
3503.148623	821838.005457	41.981184
3503.483882	821800.003170	41.986189
3503.008707	821768.841610	41.991194
3502.716044	821732.883230	41.996199
3503.220070	821686.096060	42.001204
3502.657067	821653.974551	42.006208
3502.739720	821616.691793	42.011213
3502.973838	821580.747489	42.016218
3502.571003	821542.177815	42.021223
3502.945992	821513.022920	42.026228
3502.620727	821485.437043	42.031232
3502.851982	821445.599890	42.036237
3502.840971	821415.531741	42.041242
3502.730283	821379.348224	42.046247
3502.694404	821343.931319	42.051252
3502.546253	821318.847197	42.056256
3502.712459	821283.203723	42.061261
3502.657628	821256.839655	42.066266
3502.523427	821223.091803	42.071271
3502.580812	821194.374321	42.076276
3502.879290	821166.981465	42.081280
3502.610969	821128.680127	42.086285
3502.622501	821095.492707	42.091290
3502.566842	821071.658266	42.096295
3502.634282	821044.690262	42.101300
3502.443384	821018.541084	42.106304
3502.481638	820981.748030	42.111309
3502.557045	820955.459635	42.116314
3502.655093	820924.106869	42.121319
3502.509328	820894.251888	42.126324
3502.443621	820862.535120	42.131328
3502.530400	820830.113090	42.136333
3502.671677	820805.857546	42.141338
3502.455665	820780.100577	42.146343
3502.316941	820752.774229	42.151348
3502.084025	820726.727707	42.156352
3502.078305	820702.689385	42.161357
3502.357598	820670.820376	42.166362
3502.265118	820647.184703	42.171367
3502.311960	820622.067266	42.176372
3502.194075	820596.780824	42.181376
3502.300622	820569.415324	42.186381
3502.202543	820559.600633	42.191386
3502.181615	820538.873180	42.196391
3502.046058	820502.591080	42.201396
3502.064326	820490.032900	42.206400
3502.054868	820462.977049	42.211405
3502.228150	820447.280026	42.216410
3501.843912	820423.981094	42.221415
3502.198399	820398.230679	42.226420
3502.114130	820373.035396	42.231424
3501.988965	820341.325244	42.236429
3501.786109	820326.854684	42.241434
3502.072389	820304.618457	42.246439
3502.233249	820273.544566	42.251444
3501.959036	820254.899721	42.256448
3502.023227	820223.938024	42.261453
3501.910763	820220.159661	42.266458
3501.942697	820190.760163	42.271463
3502.151016	820161.819620	42.276468
3501.872277	820152.227190	42.281472
3502.147233	820135.150810	42.286477
3502.034830	820119.010944	42.291482
3501.413690	820086.014334	42.296487
3501.599311	820069.243742	42.301492
3501.585517	820057.857716	42.306496
3501.560307	820045.694771	42.311501
3501.808202	820032.029076	42.316506
3501.809917	820007.110867	42.321511
3502.280643	819988.446104	42.326516
3501.813332	819972.166661	42.331520
3502.008435	819946.049936	42.336525
3501.983038	819927.267869	42.341530
3501.646355	819908.534406	42.346535
3501.688581	819886.529504	42.351540
3501.863314	819877.547124	42.356544
3501.885475	819857.200001	42.361549
3501.863135	819841.921378	42.366554
3501.771874	819814.972817	42.371559
3501.616866	819802.732345	42.376564
3501.845482	819783.034080	42.381568
3501.889544	819770.470407	42.386573
3501.874544	819750.128741	42.391578
3501.859436	819740.494458	42.396583
3501.881855	819706.519155	42.401588
3502.127283	819682.924313	42.406592
3501.666669	819674.235638	42.411597
3502.171548	819652.838972	42.416602
3501.932313	819632.434631	42.421607
3502.050135	819601.753463	42.426612
3502.220497	819591.895271	42.431616
3501.967473	819565.846995	42.436621
3502.206580	819547.898516	42.441626
3501.620458	819522.680873	42.446631
3501.842623	819494.027078	42.451636
3501.621450	819483.840543	42.456640
3501.671643	819461.638197	42.461645
3501.581347	819442.378080	42.466650
3501.456309	819432.273777	42.471655
3501.914983	819418.476437	42.476660
3501.522128	819417.661770	42.481664
3501.845820	819387.920814	42.486669
3502.290107	819382.789411	42.491674
3501.518071	819365.679888	42.496679
3501.758007	819345.199694	42.501684
3502.070469	819324.805441	42.506688
3501.616283	819301.513205	42.511693
3501.761987	819272.772992	42.516698
3501.556971	819281.858386	42.521703
3501.658563	819256.532152	42.526708
3501.291856	819242.766099	42.531712
3501.502835	819225.989262	42.536717
3501.560215	819206.900025	42.541722
3501.437068	819200.883688	42.546727
3501.531025	819183.832984	42.551732
3500.980885	819174.962900	42.556736
3501.700569	819156.743468	42.561741
3501.475800	819148.503929	42.566746
3501.462110	819130.788460	42.571751
3501.510882	819121.045877	42.576756
3501.816926	819106.492906	42.581760
3501.184050	819104.839562	42.586765
3501.399999	819074.627197	42.591770
3501.518971	819060.006009	42.596775
3501.644540	819054.048000	42.601780
3501.142987	819036.311173	42.606784
3501.193123	819022.966225	42.611789
3501.161394	819021.218886	42.616794
3501.471173	819011.435331	42.621799
3501.159265	818994.739607	42.626804
3501.552641	818990.005249	42.631808
3501.397192	818982.144060	42.636813
3501.648008	818962.634424	42.641818
3501.369395	818973.776173	42.646823
3501.324044	818945.064307	42.651828
3501.540994	818932.958674	42.656832
3501.315501	818920.922180	42.661837
3501.407956	818899.879452	42.666842
3501.219909	818894.262376	42.671847
3501.796632	818875.188287	42.676852
3501.371334	818867.563843	42.681856
3501.492781	818854.986217	42.686861
3501.345640	818846.247369	42.691866
3501.248057	818828.446796	42.696871
3501.194865	818819.790579	42.701876
3500.933508	818820.026173	42.706880
3501.052038	818809.785423	42.711885
3501.250727	818793.982889	42.716890
3501.449406	818787.818487	42.721895
3501.632156	818776.788803	42.726900
3501.274433	818766.914497	42.731904
3501.042855	818767.048081	42.736909
3501.315627	818748.215828	42.741914
3501.010512	818739.793592	42.746919
3501.411324	818730.676857	42.751924
3501.447457	818729.600320	42.756928
3501.053119	818709.022465	42.761933
3501.132314	818686.520740	42.766938
3501.406865	818685.991068	42.771943
3501.335695	818680.063455	42.776948
3501.232864	818664.891867	42.781952
3501.167416	818668.504339	42.786957
3501.331557	818661.468997	42.791962
3500.889456	818651.607697	42.796967
3501.114536	818623.241495	42.801972
3501.124103	818616.717055	42.806977
3500.891356	818619.187413	42.811981
3501.159443	818621.092691	42.816986
3500.550519	818619.630182	42.821991
3500.614733	818614.849637	42.826996
3500.567266	818612.228423	42.832001
3500.955265	818592.014673	42.837005
3501.119687	818594.909746	42.842010
3500.927507	818593.187368	42.847015
3501.021251	818594.048967	42.852020
3500.975666	818602.526282	42.857025
3501.368182	818583.772171	42.862029
3501.466659	818565.550761	42.867034
3501.543549	818564.273107	42.872039
3501.372667	818542.686181	42.877044
3501.601218	818538.853479	42.882049
3501.771290	818527.825335	42.887053
3501.477950	818501.973601	42.892058
3501.627219	818501.950296	42.897063
3501.678532	818478.381219	42.902068
3501.430737	818471.604777	42.907073
3501.264468	818452.158737	42.912077
3501.487298	818437.909291	42.917082
3501.358118	818441.337136	42.922087
3501.730136	818421.612134	42.927092
3501.230854	818415.069664	42.932097
3501.083822	818396.496692	42.937101
3501.506152	818388.933876	42.942106
3501.029084	818371.191310	42.947111
3501.232916	818360.839125	42.952116
3501.435902	818368.791092	42.957121
3501.461076	818350.288424	42.962125
3501.289369	818328.603519	42.967130
3500.918229	818328.953652	42.972135
3501.276288	818324.029588	42.977140
3501.087911	818309.454677	42.982145
3501.400787	818310.963600	42.987149
3501.613123	818298.468003	42.992154
3501.326477	818281.084864	42.997159
3501.535653	818271.413236	43.002164
3501.211392	818268.932508	43.007169
3501.078357	818243.346725	43.012173
3501.027165	818227.192357	43.017178
3501.057699	818237.313458	43.022183
3501.476241	818229.458950	43.027188
3501.119599	818208.678810	43.032193
3501.283641	818203.590252	43.037197
3501.651657	818200.611821	43.042202
3501.088886	818194.273769	43.047207
3501.435505	818167.639049	43.052212
3501.350430	818173.786364	43.057217
3501.058828	818157.572030	43.062221
3501.025568	818135.280617	43.067226
3501.050821	818133.232024	43.072231
3501.590949	818127.889883	43.077236
3501.302409	818110.798658	43.082241
3501.378625	818103.873797	43.087245
3501.479038	818092.271575	43.092250
3501.506814	818092.169895	43.097255
3501.571629	818072.199710	43.102260
3501.627095	818072.677901	43.107265
3501.211445	818040.514542	43.112269
3501.649081	818029.443689	43.117274
3501.029570	818024.672204	43.122279
3501.119007	818010.539998	43.127284
3501.223202	818005.363266	43.132289
3501.302230	818003.306224	43.137293
3501.055123	817989.031843	43.142298
3500.759147	817976.322956	43.147303
3500.767014	817969.700733	43.152308
3500.990508	817969.860561	43.157313
3500.912584	817966.951730	43.162317
3500.895759	817973.867518	43.167322
3500.826395	817961.707383	43.172327
3500.907715	817951.568405	43.177332
3500.903345	817941.442805	43.182337
3500.967260	817944.256528	43.187341
3501.152139	817941.209235	43.192346
3501.053458	817950.085213	43.197351
3500.815986	817922.664435	43.202356
3500.967345	817921.082904	43.207361
3501.006210	817909.295223	43.212365
3501.075906	817911.913319	43.217370
3500.998170	817914.749198	43.222375
3500.962905	817904.336260	43.227380
3500.865610	817891.206664	43.232385
3500.718473	817879.837481	43.237389
3500.755174	817891.613462	43.242394
3500.692882	817897.660118	43.247399
3501.093887	817889.028971	43.252404
3501.235812	817895.822660	43.257409
3500.952382	817871.135175	43.262413
3500.765371	817852.956303	43.267418
3501.022575	817855.642480	43.272423
3501.003228	817858.858736	43.277428
3501.229962	817871.773486	43.282433
3501.387567	817845.459043	43.287437
3501.105778	817830.605499	43.292442
3500.861277	817832.104301	43.297447
3500.684696	817826.289720	43.302452
3500.799038	817825.298172	43.307457
3500.675999	817811.198728	43.312461
3500.782822	817800.763405	43.317466
3500.567899	817807.807715	43.322471
3500.746468	817799.892810	43.327476
3501.109714	817804.704588	43.332481
3501.074384	817808.410222	43.337485
3501.168281	817802.845449	43.342490
3500.806523	817796.670304	43.347495
3501.247762	817778.393005	43.352500
3501.167699	817776.263387	43.357505
3500.931556	817775.910846	43.362509
3501.172428	817787.655108	43.367514
3500.883659	817758.781061	43.372519
3500.757758	817740.787050	43.377524
3501.099924	817743.167881	43.382529
3500.678080	817734.762521	43.387533
3501.109766	817743.458515	43.392538
3500.987192	817746.788337	43.397543
3500.827150	817721.009880	43.402548
3500.978513	817715.922906	43.407553
3501.040981	817709.389242	43.412557
3500.573997	817710.825480	43.417562
3500.821929	817707.573472	43.422567
3501.079136	817707.630667	43.427572
3500.953056	817717.971841	43.432577
3501.171771	817692.718291	43.437581
3501.071843	817688.352183	43.442586
3501.114486	817686.495469	43.447591
3501.262302	817682.382747	43.452596
3500.810303	817663.465762	43.457601
3500.839155	817657.716282	43.462605
3501.232036	817659.212862	43.467610
3501.195732	817664.866190	43.472615
3500.794491	817651.101989	43.477620
3500.834912	817638.826688	43.482625
3501.115246	817634.595846	43.487629
3501.297303	817635.443775	43.492634
3501.057557	817642.297405	43.497639
3500.896099	817622.848013	43.502644
3500.927394	817605.218530	43.507649
3500.675944	817609.250187	43.512653
3500.636500	817600.200624	43.517658
3500.438535	817603.055439	43.522663
3500.674417	817602.044857	43.527668
3500.805800	817609.814245	43.532673
3500.787586	817599.398131	43.537677
3501.135584	817598.856892	43.542682
3500.547381	817616.281386	43.547687
3500.749897	817610.309968	43.552692
3500.971565	817593.137559	43.557697
3500.848571	817581.569308	43.562701
3501.101847	817578.121650	43.567706
3501.110959	817587.370792	43.572711
3501.096528	817582.504374	43.577716
3500.932291	817572.111041	43.582721
3500.894219	817553.323763	43.587725
3500.936671	817548.351052	43.592730
3500.956091	817550.100788	43.597735
3501.064801	817546.383588	43.602740
3501.009362	817548.339776	43.607745
3500.781020	817523.642296	43.612749
3501.048435	817518.147520	43.617754
3501.127022	817518.719515	43.622759
3500.839872	817518.959181	43.627764
3500.654142	817527.946745	43.632769
3500.728258	817530.466935	43.637773
3500.701400	817518.104538	43.642778
3500.493987	817499.635694	43.647783
3500.942349	817495.962745	43.652788
3501.051433	817505.488508	43.657793
3500.999250	817506.178321	43.662797
3501.681176	817499.644979	43.667802
3501.307869	817483.344278	43.672807
3501.051060	817458.748366	43.677812
3501.491439	817470.169915	43.682817
3500.795084	817461.709718	43.687821
3501.230502	817436.713382	43.692826
3501.384783	817428.412297	43.697831
3501.218940	817420.355996	43.702836
3501.127660	817415.306707	43.707841
3500.357517	817407.539607	43.712845
3501.097197	817403.528935	43.717850
3500.951459	817400.727815	43.722855
3500.903079	817389.439672	43.727860
3500.941533	817397.710739	43.732865
3500.875897	817396.455127	43.737869
3501.122098	817378.304521	43.742874
3500.768532	817388.097541	43.747879
3501.064276	817374.905412	43.752884
3500.811518	817376.308235	43.757889
3500.609481	817371.568356	43.762893
3500.982540	817375.113030	43.767898
3500.817269	817376.404800	43.772903
3500.976912	817353.009274	43.777908
3501.186377	817344.504696	43.782913
3500.948247	817340.257324	43.787917
3501.117586	817333.317048	43.792922
3500.835087	817344.364940	43.797927
3500.983757	817315.809964	43.802932
3500.779778	817310.583451	43.807937
3500.868712	817311.445982	43.812941
3500.861375	817305.507077	43.817946
3500.793639	817313.697477	43.822951
3500.795665	817317.008050	43.827956
3500.721286	817315.753789	43.832961
3500.586607	817326.681226	43.837965
3500.804979	817303.860604	43.842970
3500.629476	817290.644584	43.847975
3501.030040	817285.518305	43.852980
3500.877743	817283.594566	43.857985
3501.193200	817278.189448	43.862989
3501.074304	817293.399145	43.867994
3500.706043	817282.745084	43.872999
3500.804520	817265.396272	43.878004
3500.933392	817259.825547	43.883009
3500.758984	817265.403448	43.888013
3501.044411	817267.598576	43.893018
3500.752737	817273.389559	43.898023
3500.504162	817270.799214	43.903028
3500.554773	817267.869961	43.908033
3501.013323	817275.296489	43.913037
3500.935010	817272.290013	43.918042
3500.662311	817253.246368	43.923047
3500.627046	817243.708737	43.928052
3500.839560	817244.844098	43.933057
3500.883799	817248.537626	43.938061
3500.957786	817237.327458	43.943066
3500.931391	817244.148174	43.948071
3500.986466	817245.405525	43.953076
3500.628758	817225.888189	43.958081
3500.833216	817220.402993	43.963085
3501.252527	817218.876778	43.968090
3500.830966	817216.897730	43.973095
3500.808039	817208.039774	43.978100
3500.759823	817222.654315	43.983105
3500.739366	817220.223048	43.988109
3500.794948	817203.854567	43.993114
3500.584807	817192.591354	43.998119
3500.635088	817181.579551	44.003124
3500.681989	817193.939543	44.008129
3500.664628	817201.927454	44.013133
3501.051486	817202.353909	44.018138
3500.922598	817205.198106	44.023143
3501.312139	817196.762557	44.028148
3500.958891	817184.060997	44.033153
3500.905075	817169.657133	44.038157
3500.953170	817158.645632	44.043162
3500.896698	817171.411350	44.048167
3501.134230	817172.348053	44.053172
3500.863028	817160.802185	44.058177
3501.064188	817150.545788	44.063181
3501.550015	817137.518206	44.068186
3500.944242	817141.995075	44.073191
3501.161180	817140.403097	44.078196
3500.859041	817123.408657	44.083201
3500.979230	817108.101019	44.088205
3500.918452	817106.747207	44.093210
3500.864843	817122.531405	44.098215
3501.006498	817110.628762	44.103220
3500.899566	817114.151238	44.108225
3500.909930	817092.044026	44.113229
3500.833031	817085.336730	44.118234
3500.825406	817075.599757	44.123239
3500.770640	817084.080577	44.128244
3500.911306	817087.272218	44.133249
3500.555463	817092.002199	44.138253
3500.900746	817086.397490	44.143258
3500.712800	817079.707547	44.148263
3500.841497	817057.873861	44.153268
3500.970896	817059.119632	44.158273
3501.038065	817061.543718	44.163277
3501.056138	817051.997455	44.168282
3500.874547	817051.831105	44.173287
3500.817525	817037.719585	44.178292
3501.022393	817014.802632	44.183297
3500.619777	817014.281300	44.188301
3501.014985	817018.991314	44.193306
3500.871970	817014.241935	44.198311
3500.647810	817026.644631	44.203316
3501.063950	817035.830967	44.208321
3500.947705	817027.376871	44.213325
3501.123923	816996.186788	44.218330
3500.731800	816994.787364	44.223335
3500.857756	816990.677604	44.228340
3501.134438	816993.750648	44.233345
3500.944354	816986.963556	44.238349
3500.937834	816988.133205	44.243354
3500.775547	816972.966776	44.248359
3500.745862	816968.004878	44.253364
3501.015500	816971.176418	44.258369
3500.766883	816963.424614	44.263373
3501.143923	816967.747972	44.268378
3500.886977	816977.526530	44.273383
3500.770987	816959.820858	44.278388
3501.238317	816937.446896	44.283393
3501.111085	816936.103435	44.288397
3501.122005	816936.491294	44.293402
3500.818325	816948.809191	44.298407
3500.911901	816927.272690	44.303412
3501.177487	816907.072611	44.308417
3501.043990	816905.145815	44.313421
3501.031043	816917.418326	44.318426
3501.001600	816914.598806	44.323431
3500.991845	816898.629275	44.328436
3500.806294	816880.155172	44.333441
3500.529294	816882.827898	44.338445
3500.990722	816880.126400	44.343450
3500.855429	816876.544329	44.348455
3500.660479	816876.866987	44.353460
3501.037078	816884.696337	44.358465
3500.715976	816882.896245	44.363469
3500.964993	816866.107099	44.368474
3500.974616	816855.101075	44.373479
3500.928259	816859.003768	44.378484
3500.938359	816854.035560	44.383489
3500.561336	816859.158569	44.388493
3500.888991	816849.466216	44.393498
3500.941188	816860.852185	44.398503
3500.965884	816837.183661	44.403508
3501.079118	816828.790809	44.408513
3500.656587	816827.006556	44.413517
3500.910345	816826.090444	44.418522
3501.207909	816834.613913	44.423527
3500.753090	816819.590223	44.428532
3500.743140	816804.886500	44.433537
3500.918980	816804.177338	44.438541
3500.968388	816792.288507	44.443546
3500.675167	816792.431759	44.448551
3500.886271	816794.638676	44.453556
3500.816557	816791.046304	44.458561
3500.781365	816801.472178	44.463565
3501.108436	816792.948465	44.468570
3501.029647	816782.150905	44.473575
3500.979366	816777.289462	44.478580
3501.356902	816774.503646	44.483585
3501.049259	816769.390267	44.488589
3500.714322	816760.288287	44.493594
3500.837902	816752.185875	44.498599
3500.890755	816743.899734	44.503604
3501.109448	816737.048469	44.508609
3500.905793	816745.163475	44.513613
3500.806010	816741.381000	44.518618
3501.023914	816743.976422	44.523623
3500.641096	816722.221520	44.528628
3501.447527	816712.356725	44.533633
3500.862393	816722.771310	44.538637
3501.163038	816713.764681	44.543642
3500.850594	816702.516571	44.548647
3500.836896	816694.435543	44.553652
3500.867111	816686.834582	44.558657
3500.571565	816681.134910	44.563661
3500.835381	816678.464217	44.568666
3500.904832	816682.446306	44.573671
3500.743495	816684.614094	44.578676
3500.966570	816668.997130	44.583681
3500.715067	816677.509258	44.588685
3500.992933	816665.097531	44.593690
3500.536171	816651.339787	44.598695
3501.070029	816646.289539	44.603700
3501.040967	816648.826217	44.608705
3500.736905	816655.788371	44.613709
3501.058711	816662.165739	44.618714
3501.199776	816656.689958	44.623719
3500.824925	816633.862228	44.628724
3500.789562	816625.394942	44.633729
3501.067559	816624.961958	44.638733
3501.313309	816619.080224	44.643738
3501.406904	816621.987296	44.648743
3501.258626	816591.917195	44.653748
3500.973760	816591.961754	44.658753
3500.938428	816597.421120	44.663757
3501.084947	816581.036788	44.668762
3500.865969	816567.339077	44.673767
3500.932466	816563.238331	44.678772
3500.812764	816562.575341	44.683777
3500.987965	816567.514873	44.688781
3501.033978	816551.925295	44.693786
3500.828869	816556.826895	44.698791
3500.891948	816528.963422	44.703796
3501.268796	816531.923649	44.708801
3501.030422	816529.039224	44.713805
3501.198937	816520.247754	44.718810
3501.241732	816513.715912	44.723815
3500.960184	816501.878263	44.728820
3501.513525	816495.461375	44.733825
3501.186355	816490.058644	44.738829
3501.212709	816462.200614	44.743834
3500.830150	816466.156108	44.748839
3500.987001	816461.456822	44.753844
3501.336120	816457.798785	44.758849
3500.932201	816450.265399	44.763853
3501.266859	816434.435622	44.768858
3501.455903	816441.418323	44.773863
3501.188919	816437.174840	44.778868
3501.006191	816413.926701	44.783873
3500.995398	816413.149278	44.788877
3501.287695	816398.981704	44.793882
3501.078500	816408.558902	44.798887
3501.155418	816385.367460	44.803892
3501.283951	816378.724682	44.808897
3501.001613	816377.210559	44.813901
3501.003745	816374.191073	44.818906
3501.056358	816363.761819	44.823911
3501.154153	816348.650603	44.828916
3501.119467	816342.325481	44.833921
3501.009093	816340.492287	44.838925
3501.204524	816328.579746	44.843930
3500.913837	816321.905046	44.848935
3501.221789	816297.411042	44.853940
3500.989811	816307.089351	44.858945
3501.037600	816308.055850	44.863949
3501.224249	816288.353078	44.868954
3500.769287	816271.867169	44.873959
3500.865178	816264.937189	44.878964
3500.981263	816268.327884	44.883969
3501.121783	816270.935602	44.888973
3501.043623	816263.253670	44.893978
3500.778648	816245.374466	44.898983
3500.975391	816233.461538	44.903988
3501.005298	816238.716230	44.908993
3500.658649	816233.803295	44.913997
3500.681561	816239.059080	44.919002
3500.947405	816245.445625	44.924007
3500.896354	816235.129755	44.929012
3501.259928	816209.555366	44.934017
3500.947376	816207.266759	44.939021
3501.176612	816199.439301	44.944026
3500.713170	816205.160724	44.949031
3500.647232	816212.378333	44.954036
3500.836042	816211.959265	44.959041
3500.855693	816184.393228	44.964045
3501.129181	816177.240596	44.969050
3501.356078	816174.965047	44.974055
3501.160444	816178.404520	44.979060
3501.056891	816160.305045	44.984065
3500.790842	816147.198144	44.989069
3500.897950	816143.188171	44.994074
3500.681627	816142.540239	44.999079
3500.501491	816144.711152	45.004084
3501.231748	816138.558436	45.009089
3500.765280	816155.578381	45.014093
3500.741440	816138.927329	45.019098
3501.100529	816125.820058	45.024103
3501.027478	816111.416753	45.029108
3501.207630	816119.569971	45.034113
3500.966840	816106.653830	45.039117
3501.164900	816090.357550	45.044122
3501.155672	816082.080235	45.049127
3501.171739	816083.538715	45.054132
3500.946094	816079.678114	45.059137
3500.808613	816078.725659	45.064141
3501.191807	816056.751287	45.069146
3501.162606	816054.320931	45.074151
3501.283411	816051.769728	45.079156
3501.206759	816041.944530	45.084161
3501.331713	816024.101134	45.089165
3501.079414	816008.849026	45.094170
3501.491768	816014.238920	45.099175
3501.224790	816005.612201	45.104180
3501.526567	815985.598281	45.109185
3500.933827	815979.749622	45.114189
3501.105167	815966.184370	45.119194
3501.189587	815963.833617	45.124199
3501.252318	815942.785534	45.129204
3501.403529	815942.372327	45.134209
3500.898957	815936.802044	45.139213
3501.153948	815921.178221	45.144218
3500.738907	815913.158919	45.149223
3500.627905	815908.208888	45.154228
3501.072170	815916.223686	45.159233
3501.124870	815913.488272	45.164237
3500.959139	815895.592549	45.169242
3501.110593	815895.568902	45.174247
3501.093785	815888.461321	45.179252
3501.107675	815882.907343	45.184257
3500.744887	815887.541912	45.189261
3500.490660	815861.283467	45.194266
3500.924213	815850.501603	45.199271
3501.016299	815855.552096	45.204276
3500.850609	815843.695082	45.209281
3500.776849	815851.693540	45.214285
3500.763964	815853.351402	45.219290
3501.001922	815862.177730	45.224295
3500.632639	815855.320011	45.229300
3500.887464	815854.890601	45.234305
3500.685888	815833.493862	45.239309
3500.779451	815823.349507	45.244314
3501.114928	815812.875115	45.249319
3500.673679	815824.047911	45.254324
3500.876917	815822.749948	45.259329
3500.790291	815825.880369	45.264333
3500.765847	815825.299810	45.269338
3500.815682	815822.175198	45.274343
3500.730062	815798.812180	45.279348
3500.963962	815789.522451	45.284353
3500.718246	815792.580356	45.289357
3500.679770	815787.716293	45.294362
3500.717010	815794.918256	45.299367
3500.807102	815801.332733	45.304372
3500.962979	815798.581140	45.309377
3501.099035	815797.878087	45.314381
3500.941562	815780.078142	45.319386
3501.006901	815770.425125	45.324391
3500.982866	815755.039310	45.329396
3501.117465	815753.752064	45.334401
3500.741556	815761.895272	45.339405
3501.112303	815749.077598	45.344410
3500.628734	815730.354459	45.349415
3500.755578	815715.724186	45.354420
3500.527437	815726.474229	45.359425
3500.597269	815734.937406	45.364429
3500.914412	815740.147617	45.369434
3500.638302	815731.424541	45.374439
3500.687981	815735.605133	45.379444
3501.273771	815728.987589	45.384449
3500.653400	815717.201410	45.389453
3500.624902	815696.751177	45.394458
3500.461569	815702.913160	45.399463
3500.530841	815694.136042	45.404468
3500.868197	815695.641793	45.409473
3500.843989	815700.710590	45.414477
3500.939231	815706.442535	45.419482
3500.762929	815711.437696	45.424487
3500.535824	815710.499192	45.429492
3500.782251	815705.882740	45.434497
3500.734806	815724.202003	45.439501
3501.230696	815705.033469	45.444506
3501.176995	815678.158486	45.449511
3500.978402	815678.773982	45.454516
3501.087165	815672.328352	45.459521
3500.715436	815678.230723	45.464525
3501.156085	815665.499355	45.469530
3501.024834	815655.584680	45.474535
3500.737844	815645.889143	45.479540
3500.899213	815641.772962	45.484545
3500.983675	815644.584515	45.489549
3501.129649	815637.158988	45.494554
3500.895571	815618.688726	45.499559
3501.112474	815606.674048	45.504564
3500.942351	815603.681116	45.509569
3500.824286	815613.732310	45.514573
3500.853481	815606.422406	45.519578
3500.862747	815608.369085	45.524583
3500.719459	815590.176761	45.529588
3500.767661	815572.831100	45.534593
3500.613359	815581.913954	45.539597
3500.826135	815567.659523	45.544602
3500.939010	815573.973267	45.549607
3500.864048	815573.010959	45.554612
3500.649572	815572.167865	45.559617
3500.473222	815576.383897	45.564621
3500.891172	815574.078266	45.569626
3501.074482	815581.160236	45.574631
3500.832641	815556.359650	45.579636
3500.862663	815548.270303	45.584641
3500.765012	815548.967437	45.589645
3500.815570	815549.641404	45.594650
3500.761493	815550.623945	45.599655
3500.713093	815556.865511	45.604660
3500.762442	815552.961594	45.609665
3500.432490	815559.247170	45.614669
3500.253874	815551.385253	45.619674
3500.446658	815557.004681	45.624679
3500.746594	815569.523153	45.629684
3500.556611	815561.663026	45.634689
3500.853596	815565.220639	45.639693
3501.025776	815540.355269	45.644698
3500.921432	815533.455779	45.649703
3500.820196	815527.335045	45.654708
3501.103399	815520.861990	45.659713
3500.723273	815521.700691	45.664717
3500.960133	815516.111532	45.669722
3501.033642	815499.735775	45.674727
3501.113062	815495.145275	45.679732
3501.275112	815489.665194	45.684737
3501.016622	815491.166732	45.689741
3500.872204	815483.104569	45.694746
3500.713228	815463.940260	45.699751
3500.875914	815455.440425	45.704756
3500.820433	815452.234684	45.709761
3500.878608	815460.407834	45.714765
3501.041964	815459.310847	45.719770
3500.739810	815456.338482	45.724775
3500.339477	815457.375165	45.729780
3500.507395	815459.394497	45.734785
3500.388599	815470.907144	45.739789
3500.865576	815463.332261	45.744794
3500.752315	815441.043704	45.749799
3500.534248	815437.765963	45.754804
3500.734369	815442.702495	45.759809
3500.191705	815444.248466	45.764813
3500.354983	815428.442935	45.769818
3500.544003	815379.514531	45.774823
3500.639581	815280.531780	45.779828
3500.458194	815131.326165	45.784833
3500.191230	814937.319434	45.789837
3500.165696	814674.004045	45.794842
3500.012362	814376.891461	45.799847
3499.446604	814024.197166	45.804852
3499.554777	813627.239382	45.809857
3498.749259	813186.647689	45.814861
3498.450874	812697.025919	45.819866
3497.843996	812152.057886	45.824871
3497.055236	811573.054897	45.829876
3496.947992	810927.607620	45.834881
3495.998095	810253.856991	45.839885
3495.669869	809520.560367	45.844890
3494.567203	808751.074387	45.849895
3493.810482	807937.555208	45.854900
3493.617570	807066.540673	45.859905
3492.374443	806161.867085	45.864909
3491.554519	805202.020641	45.869914
3490.463945	804189.866274	45.874919
3489.667043	803144.664293	45.879924
3488.678697	802045.243773	45.884929
3487.298947	800912.111093	45.889933
3486.359642	799724.270811	45.894938
3485.299415	798500.289081	45.899943
3484.037233	797233.515958	45.904948
3482.707431	795917.555098	45.909953
3481.412258	794555.097749	45.914957
3479.926003	793160.470961	45.919962
3478.750353	791719.888927	45.924967
3477.367059	790240.053221	45.929972
3476.105116	788708.122262	45.934977
3474.487521	787145.366247	45.939981
3472.969218	785535.301794	45.944986
3471.436142	783883.150599	45.949991
3469.428917	782188.073497	45.954996
3467.725971	780462.306559	45.960001
3466.149346	778714.721147	45.965005
3464.958298	776898.815916	45.970010
3462.781822	775075.716734	45.975015
3461.166149	773186.991254	45.980020
3459.142422	771266.572232	45.985025
3457.214597	769326.618499	45.990029
3455.791843	767347.672586	45.995034
3453.630511	765325.088547	46.000039
3451.364626	763270.464416	46.005044
3449.978732	761182.147626	46.010049
3447.789590	759057.230584	46.015053
3445.403654	756900.354466	46.020058
3443.316754	754707.483723	46.025063
3440.868329	752483.510005	46.030068
3438.833240	750235.270377	46.035073
3436.643466	747962.637802	46.040077
3434.661872	745645.162324	46.045082
3432.091599	743301.734795	46.050087
3429.380226	740923.400289	46.055092
3427.231968	738534.058137	46.060097
3424.810426	736101.507487	46.065101
3422.441303	733647.249702	46.070106
3419.676588	731160.243524	46.075111
3417.059093	728645.456862	46.080116
3414.613177	726110.955315	46.085121
3412.150665	723553.841554	46.090125
3409.292014	720966.010477	46.095130
3406.679507	718350.892227	46.100135
3403.952919	715715.043059	46.105140
3401.367437	713056.628367	46.110145
3398.461857	710368.385563	46.115149
3395.629917	707653.591779	46.120154
3392.919744	704931.316547	46.125159
3390.060722	702182.743642	46.130164
3387.330320	699413.849387	46.135169
3384.467898	696625.205013	46.140173
3381.324726	693806.762431	46.145178
3378.747889	690968.822886	46.150183
3375.560697	688111.210233	46.155188
3372.852514	685220.895343	46.160193
3369.872174	682328.183964	46.165197
3366.371746	679407.460603	46.170202
3364.057851	676472.437709	46.175207
3360.436591	673506.363776	46.180212
3357.720962	670527.797343	46.185217
3354.263051	667549.018553	46.190221
3351.596806	664537.529311	46.195226
3348.659498	661504.063671	46.200231
3345.357070	658461.208962	46.205236
3342.366796	655390.792448	46.210241
3338.577632	652316.516357	46.215245
3335.696452	649218.695907	46.220250
3332.703810	646109.033321	46.225255
3329.048995	642977.196040	46.230260
3325.772517	639840.854890	46.235265
3322.692633	636686.179459	46.240269
3319.301028	633517.629971	46.245274
3316.330970	630329.697800	46.250279
3312.604522	627143.123661	46.255284
3309.991855	623927.165703	46.260289
3306.306128	620702.376813	46.265293
3302.775342	617460.471174	46.270298
3299.582452	614211.859882	46.275303
3296.166626	610951.784069	46.280308
3292.760002	607672.653903	46.285313
3289.076343	604398.621214	46.290317
3285.750370	601103.576921	46.295322
3282.385389	597804.695008	46.300327
3278.615245	594495.679295	46.305332
3275.402177	591167.563437	46.310337
3271.879959	587836.360451	46.315341
3268.732257	584498.412097	46.320346
3264.774394	581141.523213	46.325351
3261.326826	577775.210786	46.330356
3257.921233	574400.252648	46.335361
3254.038202	571025.415120	46.340365
3250.472392	567638.787606	46.345370
3247.122583	564250.730689	46.350375
3243.219585	560855.497326	46.355380
3239.993369	557452.899745	46.360385
3236.282887	554050.210546	46.365389
3232.780216	550631.898562	46.370394
3229.440452	547201.337806	46.375399
3225.657128	543779.247147	46.380404
3222.074558	540335.556444	46.385409
3218.077200	536895.217370	46.390413
3214.296862	533445.257475	46.395418
3210.569616	529997.589577	46.400423
3206.961967	526544.862470	46.405428
3203.591220	523091.548897	46.410433
3199.547087	519629.184465	46.415437
3196.358979	516156.626827	46.420442
3192.432847	512694.397495	46.425447
3188.742199	509213.465434	46.430452
3184.789339	505738.926335	46.435457
3180.729420	502267.643489	46.440461
3176.894574	498768.792424	46.445466
3173.617911	495299.406497	46.450471
3169.662674	491818.509123	46.455476
3166.046227	488336.449146	46.460481
3162.323052	484842.142634	46.465485
3158.891448	481340.734465	46.470490
3154.944773	477852.522081	46.475495
3150.766267	474348.465732	46.480500
3147.441281	470849.176832	46.485505
3143.561138	467363.942213	46.490509
3139.534751	463858.322441	46.495514
3136.044982	460363.980906	46.500519
3131.943899	456866.136963	46.505524
3128.127889	453348.817708	46.510529
3124.459498	449857.503083	46.515533
3120.839745	446356.387404	46.520538
3116.903340	442860.877631	46.525543
3112.924072	439367.652808	46.530548
3109.197159	435858.390572	46.535553
3105.642900	432365.128904	46.540557
3101.622559	428866.803612	46.545562
3097.885722	425375.572106	46.550567
3093.848663	421877.243933	46.555572
3090.063441	418374.325970	46.560577
3086.098560	414887.433190	46.565581
3082.438257	411388.966870	46.570586
3078.809829	407902.868515	46.575591
3074.948020	404409.459412	46.580596
3071.116870	400917.789024	46.585601
3067.417669	397432.776104	46.590605
3063.236185	393940.469824	46.595610
3059.096402	390463.590359	46.600615
3055.341779	386987.376606	46.605620
3052.173873	383508.811817	46.610625
3047.799768	380028.922435	46.615629
3044.165141	376559.351021	46.620634
3040.489110	373083.926975	46.625639
3036.607912	369614.624021	46.630644
3032.796426	366148.261436	46.635649
3028.752151	362682.280783	46.640653
3024.964439	359220.351769	46.645658
3020.964211	355766.219395	46.650663
3016.841969	352312.358493	46.655668
3013.011559	348856.477614	46.660673
3009.474020	345420.857601	46.665677
3005.506537	341974.709248	46.670682
3001.558324	338540.855343	46.675687
2997.518871	335101.524853	46.680692
2993.911482	331668.954373	46.685697
2989.878993	328245.019468	46.690701
2985.861608	324815.570809	46.695706
2981.900388	321385.622249	46.700711
2978.100107	317977.403724	46.705716
2974.304712	314570.141286	46.710721
2969.801689	311165.966568	46.715725
2966.034071	307776.039443	46.720730
2961.960555	304391.755298	46.725735
2957.776609	301021.264044	46.730740
2953.861986	297641.280089	46.735745
2950.091099	294287.746637	46.740749
2946.121920	290931.177172	46.745754
2941.969629	287575.218439	46.750759
2937.888856	284244.661705	46.755764
2934.096422	280917.896383	46.760769
2929.823440	277597.751098	46.765773
2926.130981	274277.169684	46.770778
2922.270955	270976.648066	46.775783
2918.375937	267672.342881	46.780788
2914.113486	264385.449878	46.785793
2910.197368	261103.008014	46.790797
2905.585428	257817.167631	46.795802
2901.573358	254557.377337	46.800807
2897.624089	251309.877541	46.805812
2893.337667	248062.872172	46.810817
2889.405172	244839.004341	46.815821
2885.415194	241625.002415	46.820826
2881.328358	238415.150678	46.825831
2877.085719	235228.950169	46.830836
2872.791846	232041.026057	46.835841
2868.757712	228865.982281	46.840845
2864.879831	225704.377863	46.845850
2860.706032	222564.543280	46.850855
2856.654234	219428.286796	46.855860
2852.361024	216297.124474	46.860865
2848.091275	213189.003160	46.865869
2844.368787	210092.386970	46.870874
2840.455351	206995.708429	46.875879
2835.790582	203926.287379	46.880884
2831.741486	200852.514801	46.885889
2827.588503	197808.330387	46.890893
2823.176032	194775.886399	46.895898
2819.256194	191753.492417	46.900903
2814.973253	188756.821937	46.905908
2810.834226	185759.877680	46.910913
2806.467363	182776.703853	46.915917
2802.222441	179818.047206	46.920922
2798.256182	176868.992071	46.925927
2793.998238	173934.343230	46.930932
2789.761298	171004.979962	46.935937
2785.494698	168126.525476	46.940941
2781.851390	165141.025789	46.945946
2777.602325	162263.739122	46.950951
2773.287974	159401.570576	46.955956
2769.105888	156551.909347	46.960961
2765.013065	153724.158319	46.965965
2761.182863	150896.175026	46.970970
2756.517044	148094.147337	46.975975
2752.664261	145294.456390	46.980980
2748.351330	142526.024195	46.985985
2744.223120	139764.334148	46.990989
2740.569260	137022.639953	46.995994
2736.032783	134287.975742	47.000999
2731.742437	131579.046615	47.006004
2728.097752	128873.695415	47.011009
2724.135531	126178.970842	47.016013
2719.689723	123505.992154	47.021018
2715.908947	120843.007129	47.026023
2711.502533	118190.983276	47.031028
2707.453863	115546.679217	47.036033
2703.025639	112925.801720	47.041037
2698.924494	110325.226508	47.046042
2694.969607	107746.418381	47.051047
2690.488416	105164.477232	47.056052
2686.807737	102603.161054	47.061057
2682.644405	100059.289074	47.066061
2678.521366	97522.078435	47.071066
2674.293985	95005.075735	47.076071
2669.968521	92507.084669	47.081076
2665.843311	90020.243616	47.086081
2661.511641	87550.004223	47.091085
2657.710045	85097.419702	47.096090
2653.732445	82663.997047	47.101095
2649.411029	80235.789250	47.106100
2645.206175	77834.749609	47.111105
2641.047202	75438.737470	47.116109
2636.870543	73058.355444	47.121114
2632.685551	70699.251636	47.126119
2628.528449	68363.754103	47.131124
2624.427567	66026.503198	47.136129
2620.227986	63732.133264	47.141133
2616.213269	61426.513793	47.146138
2611.786642	59151.156932	47.151143
2607.442034	56894.622104	47.156148
2603.492718	54640.666517	47.161153
2599.220846	52416.537914	47.166157
2595.009366	50199.683382	47.171162
2590.998393	48012.395661	47.176167
2586.684544	45844.308444	47.181172
2581.998619	43680.000571	47.186177
2577.540671	41532.055282	47.191181
2573.660380	39423.424817	47.196186
2569.338180	37315.694940	47.201191
2565.087359	35235.836577	47.206196
2561.224295	33171.681502	47.211201
2556.487789	31138.889115	47.216205
2552.178292	29115.442441	47.221210
2548.445071	27106.938116	47.226215
2543.806833	25128.742328	47.231220
2539.337492	23158.937051	47.236225
2535.192821	21214.455688	47.241229
2530.469691	19284.342790	47.246234
2526.627412	17389.952560	47.251239
2521.531793	15518.855562	47.256244
2517.351551	13656.953657	47.261249
2512.751485	11816.383644	47.266253
2508.205634	10019.725920	47.271258
2503.624428	8240.176770	47.276263
2498.809652	6501.418737	47.281268
2493.976781	4766.128134	47.286273
2488.681200	3091.188082	47.291277
2481.000589	1507.230793	47.296282
2462.862442	257.373564	47.301287
2407.041315	151.868043	47.306292
2361.729690	207.164477	47.311297
2341.712747	218.515757	47.316301
2340.149799	219.965735	47.321306
2349.541791	228.130444	47.326311
2361.722492	231.720543	47.331316
2371.810680	237.014298	47.336321
2377.178089	234.874291	47.341325
2379.004283	231.848711	47.346330
2378.176288	222.622692	47.351335
2375.298699	223.357642	47.356340
2371.450884	218.603188	47.361345
2367.541982	221.537015	47.366349
2364.070803	214.898088	47.371354
2361.299264	206.226078	47.376359
2358.186728	217.963770	47.381364
2355.611244	205.464443	47.386369
2352.613026	211.878436	47.391373
2349.725649	199.003950	47.396378
2347.258395	194.261332	47.401383
2344.137213	205.459349	47.406388
2341.139409	193.997413	47.411393
2337.424580	196.239636	47.416397
2334.156278	201.556891	47.421402
2331.184033	189.610054	47.426407
2327.912271	198.563135	47.431412
2324.844115	198.897624	47.436417
2321.432711	199.092818	47.441421
2318.208101	199.113252	47.446426
2315.003975	191.252450	47.451431
2311.597375	201.248559	47.456436
2308.491018	202.921018	47.461441
2305.127949	198.112906	47.466445
2301.764313	198.882785	47.471450
2298.484873	194.564647	47.476455
2295.227341	198.611515	47.481460
2291.672035	195.013606	47.486465
2288.221328	203.681470	47.491469
2285.081378	190.748449	47.496474
2281.514362	197.014151	47.501479
2278.228634	206.754070	47.506484
2275.046924	206.457745	47.511489
2271.812971	197.035507	47.516493
2268.549327	202.826629	47.521498
2264.979757	190.444903	47.526503
2261.005681	196.078244	47.531508
2257.546168	203.807825	47.536513
2254.464963	203.593862	47.541517
2251.111241	199.565781	47.546522
2247.312425	202.770333	47.551527
2244.032773	202.264706	47.556532
2241.102858	204.036133	47.561537
2237.774387	202.857914	47.566541
2234.165849	209.984373	47.571546
2230.149604	195.650829	47.576551
2226.908917	205.817162	47.581556
2223.919740	192.072772	47.586561
2220.927090	201.845944	47.591565
2216.770315	203.100619	47.596570
2213.534284	197.415255	47.601575
2209.892804	210.061493	47.606580
2206.409589	195.682532	47.611585
2202.428775	199.159190	47.616589
2198.953806	194.558455	47.621594
2195.578305	193.299020	47.626599
2192.629346	194.130607	47.631604
2189.211930	192.738522	47.636609
2186.083124	195.110576	47.641613
2182.677474	199.025617	47.646618
2179.314100	190.506385	47.651623
2175.442322	195.978209	47.656628
2172.340522	186.813758	47.661633
2168.467958	186.299678	47.666637
2164.786596	196.949432	47.671642
2161.686158	189.705235	47.676647
2157.668639	192.773184	47.681652
2154.505806	187.342156	47.686657
2150.779280	189.469205	47.691661
2147.116134	189.014118	47.696666
2143.848673	188.864131	47.701671
2140.866686	190.377965	47.706676
2137.731326	193.817279	47.711681
2134.220679	188.500790	47.716685
2130.406990	197.383675	47.721690
2127.207434	182.065006	47.726695
2123.269404	184.003685	47.731700
2119.814595	183.709006	47.736705
2116.207324	190.085456	47.741709
2112.860438	194.475392	47.746714
2109.352695	192.838029	47.751719
2105.796944	203.202383	47.756724
2102.731513	183.591521	47.761729
2099.306082	185.045031	47.766733
2095.443534	193.584380	47.771738
2092.178228	189.396984	47.776743
2088.519623	187.065038	47.781748
2085.224939	179.405161	47.786753
2081.745678	188.049061	47.791757
2078.148117	190.159118	47.796762
2074.940850	189.224588	47.801767
2071.075787	190.664634	47.806772
2067.583352	189.262180	47.811777
2064.030284	181.772458	47.816781
2060.547750	182.042139	47.821786
2057.058027	187.264387	47.826791
2053.673788	191.470351	47.831796
2050.256358	188.028133	47.836801
2047.095108	190.838749	47.841805
2043.567142	183.680475	47.846810
2039.803714	178.065045	47.851815
2035.998768	187.557207	47.856820
2032.799768	192.594763	47.861825
2029.322612	190.060433	47.866829
2025.843190	194.774862	47.871834
2022.285116	183.511454	47.876839
2018.687671	187.390108	47.881844
2015.576003	182.564911	47.886849
2012.160895	183.501124	47.891853
2008.389238	186.780597	47.896858
2004.859996	171.317417	47.901863
2001.088945	187.948273	47.906868
1997.882627	180.926356	47.911873
1994.247208	188.326006	47.916877
1990.962283	187.894051	47.921882
1987.602843	182.300850	47.926887
1983.812180	184.586690	47.931892
1980.672285	182.626049	47.936897
1977.289246	178.615310	47.941901
1973.722980	187.092510	47.946906
1970.012595	180.997392	47.951911
1966.303112	186.228741	47.956916
1962.766850	180.568303	47.961921
1959.394554	187.275034	47.966925
1955.960974	181.019545	47.971930
1952.848638	177.627702	47.976935
1948.975415	180.306134	47.981940
1945.979139	179.860665	47.986945
1942.486787	183.684930	47.991949
1938.547556	179.229710	47.996954
1935.327930	176.443139	48.001959
1930.938500	186.128034	48.006964
1927.867950	180.056201	48.011969
1924.461387	184.044224	48.016973
1921.123313	172.910961	48.021978
1918.188244	182.985228	48.026983
1914.412624	176.286555	48.031988
1910.901770	180.892032	48.036993
1907.423080	174.140570	48.041997
1903.722772	185.299564	48.047002
1900.128003	179.161072	48.052007
1896.722490	182.804078	48.057012
1892.779432	183.800796	48.062017
1889.413811	174.174687	48.067021
1886.323031	174.240748	48.072026
1883.204310	175.696950	48.077031
1879.044333	181.742325	48.082036
1875.541092	171.422728	48.087041
1871.914489	177.495374	48.092045
1868.415691	180.618294	48.097050
1865.484035	171.458978	48.102055
1861.986390	180.716429	48.107060
1858.590161	179.143963	48.112065
1854.999958	177.098801	48.117069
1850.847876	171.493648	48.122074
1847.471331	174.654392	48.127079
1844.097893	184.268910	48.132084
1840.712989	173.177811	48.137089
1837.309344	169.793628	48.142093
1833.530877	169.071951	48.147098
1830.348249	163.903575	48.152103
1826.591802	171.793618	48.157108
1822.892300	165.965789	48.162113
1819.606393	165.432800	48.167117
1816.127312	165.493206	48.172122
1812.614204	166.599846	48.177127
1808.916115	174.458615	48.182132
1806.088255	165.048955	48.187137
1802.595287	166.481487	48.192141
1799.082448	175.725510	48.197146
1795.556115	168.339288	48.202151
1791.695846	169.468624	48.207156
1788.314935	165.925872	48.212161
1784.888074	171.258581	48.217165
1780.977486	167.333638	48.222170
1777.511783	163.990827	48.227175
1774.213178	173.378504	48.232180
1770.743453	157.520143	48.237185
1767.436309	162.549373	48.242189
1763.741876	164.241242	48.247194
1760.191741	160.614250	48.252199
1756.742112	166.070754	48.257204
1753.395616	158.026804	48.262209
1749.845111	163.714239	48.267213
1746.216313	162.896403	48.272218
1742.872389	151.343352	48.277223
1739.054696	172.278050	48.282228
1735.807972	165.683351	48.287233
1732.407005	161.188277	48.292237
1728.483628	168.338821	48.297242
1724.962457	167.706635	48.302247
1721.857923	168.486763	48.307252
1718.527396	165.973893	48.312257
1714.897063	165.842863	48.317261
1711.108996	168.356185	48.322266
1707.633604	161.151860	48.327271
1703.956647	162.018414	48.332276
1700.866514	161.018213	48.337281
1697.486235	158.260031	48.342285
1693.717455	159.615536	48.347290
1690.555959	168.339512	48.352295
1687.009204	163.016196	48.357300
1683.247216	162.415386	48.362305
1679.933664	161.364734	48.367309
1676.163922	157.484234	48.372314
1672.714650	160.646918	48.377319
1668.947429	167.130781	48.382324
1665.681166	161.966061	48.387329
1662.263909	165.057299	48.392333
1658.923094	165.102446	48.397338
1655.561785	161.237127	48.402343
1651.711990	168.183185	48.407348
1648.143218	159.740616	48.412353
1644.604939	165.726734	48.417357
1641.262164	169.388468	48.422362
1638.063322	165.678066	48.427367
1634.250372	161.446829	48.432372
1630.568938	158.691510	48.437377
1627.340262	150.072337	48.442381
1623.764900	165.160310	48.447386
1620.565544	156.954175	48.452391
1616.560665	160.811293	48.457396
1613.195456	159.183437	48.462401
1609.734129	156.077292	48.467405
1606.020797	152.219631	48.472410
1602.743044	149.065776	48.477415
1599.345916	165.862808	48.482420
1595.732222	145.224361	48.487425
1592.499074	155.275725	48.492429
1588.770255	162.671115	48.497434
1585.320725	160.138951	48.502439
1581.730836	168.942658	48.507444
1578.151432	153.436925	48.512449
1574.777495	161.415871	48.517453
1570.718180	165.594746	48.522458
1568.031609	150.363743	48.527463
1564.138627	163.846752	48.532468
1560.407269	160.893624	48.537473
1557.430029	152.867891	48.542477
1553.772722	160.786787	48.547482
1550.148534	148.875878	48.552487
1546.825287	156.717177	48.557492
1543.168357	149.114219	48.562497
1539.979600	162.398423	48.567501
1536.396863	157.587015	48.572506
1532.938381	153.929945	48.577511
1529.382039	167.062875	48.582516
1525.348131	158.949433	48.587521
1521.910355	148.407778	48.592525
1518.286823	162.237776	48.597530
1515.358119	164.724228	48.602535
1511.770482	167.532124	48.607540
1508.457785	154.196205	48.612545
1504.532477	158.442716	48.617549
1500.936306	155.772180	48.622554
1497.742546	156.999786	48.627559
1494.019967	164.805528	48.632564
1490.769173	163.567940	48.637569
1487.860015	152.380393	48.642573
1484.114246	162.815752	48.647578
1480.345606	153.841379	48.652583
1477.074620	171.795642	48.657588
1473.283865	159.746313	48.662593
1469.991806	148.729443	48.667597
1466.001274	153.441768	48.672602
1462.599256	152.028540	48.677607
1459.045151	156.166342	48.682612
1455.823421	154.959020	48.687617
1451.856577	153.906296	48.692621
1448.479782	156.114881	48.697626
1445.071195	146.799424	48.702631
1441.154146	155.072227	48.707636
1438.163680	152.268941	48.712641
1434.893996	155.973079	48.717645
1430.875596	152.925724	48.722650
1428.076908	150.275925	48.727655
1424.273767	157.872827	48.732660
1420.950622	153.093600	48.737665
1417.435939	149.831360	48.742669
1413.615441	158.816742	48.747674
1410.168433	146.229580	48.752679
1406.388016	150.956494	48.757684
1403.015837	141.954906	48.762689
1399.677052	151.848838	48.767693
1395.914952	151.441148	48.772698
1392.815563	149.534473	48.777703
1389.352119	144.147619	48.782708
1386.012583	154.687095	48.787713
1382.220297	149.459288	48.792717
1378.523123	154.666740	48.797722
1375.156062	158.373483	48.802727
1371.675710	148.933245	48.807732
1368.023743	148.369118	48.812737
1364.516517	154.458025	48.817741
1361.139177	157.571581	48.822746
1357.972933	147.816418	48.827751
1354.329806	151.227850	48.832756
1350.837676	146.168213	48.837761
1346.787018	150.399598	48.842765
1343.180341	156.488260	48.847770
1340.174101	148.739239	48.852775
1336.448359	152.090842	48.857780
1333.094506	152.353280	48.862785
1330.021642	142.048826	48.867789
1326.062515	152.837170	48.872794
1322.343281	155.779625	48.877799
1318.838839	153.958528	48.882804
1315.629463	145.788888	48.887809
1312.299576	143.725328	48.892813
1308.667213	146.223907	48.897818
1305.196781	145.966752	48.902823
1301.631000	155.950030	48.907828
1298.040094	152.370729	48.912833
1294.814879	146.288542	48.917837
1290.932418	154.555979	48.922842
1287.666532	144.076108	48.927847
1284.238256	141.853950	48.932852
1280.834788	146.714890	48.937857
1277.060951	150.776413	48.942861
1272.962734	159.716727	48.947866
1269.944788	142.870386	48.952871
1266.411942	148.669095	48.957876
1263.238130	147.020892	48.962881
1259.535907	143.253386	48.967885
1255.731967	148.265613	48.972890
1252.458252	137.283938	48.977895
1249.262630	145.997532	48.982900
1245.581860	153.379174	48.987905
1242.225367	143.732939	48.992909
1238.463735	141.638916	48.997914
1235.251414	144.454587	49.002919
1231.846720	147.338342	49.007924
1228.333383	155.152534	49.012929
1224.617861	147.280470	49.017933
1220.721465	151.079619	49.022938
1217.543003	141.139764	49.027943
1214.154138	152.243837	49.032948
1210.495264	151.199948	49.037953
1207.028695	149.974091	49.042957
1203.402408	146.618672	49.047962
1200.404211	146.290789	49.052967
1196.325097	149.865445	49.057972
1192.807865	137.754466	49.062977
1189.880035	139.051269	49.067981
1186.055202	143.949729	49.072986
1182.564154	147.606336	49.077991
1179.220420	152.062479	49.082996
1175.234568	145.235694	49.088001
1171.855444	137.820370	49.093005
1168.156345	144.043778	49.098010
1164.936604	141.444160	49.103015
1161.808718	145.186292	49.108020
1158.067900	136.783537	49.113025
1154.659171	145.109728	49.118029
1150.471539	149.970086	49.123034
1147.521425	142.652125	49.128039
1144.060866	139.302424	49.133044
1140.500919	132.829771	49.138049
1137.150765	138.546130	49.143053
1133.268807	140.523849	49.148058
1130.051083	135.418179	49.153063
1126.392668	135.589161	49.158068
1122.829389	135.963553	49.163073
1119.211375	141.481404	49.168077
1115.780416	148.513920	49.173082
1112.720265	133.518779	49.178087
1109.007805	142.269029	49.183092
1105.293466	141.964709	49.188097
1102.140435	141.278275	49.193101
1098.339716	137.902752	49.198106
1095.559107	143.504646	49.203111
1091.375937	140.559171	49.208116
1087.959356	141.777497	49.213121
1084.187284	142.912272	49.218125
1080.841365	145.881788	49.223130
1077.326220	134.858894	49.228135
1073.781393	140.165980	49.233140
1070.603323	143.925486	49.238145
1067.041952	139.405164	49.243149
1062.998699	143.442503	49.248154
1060.055863	134.446611	49.253159
1056.728294	136.888066	49.258164
1052.839803	135.997251	49.263169
1049.221856	142.559177	49.268173
1045.705618	146.460224	49.273178
1042.660357	135.284681	49.278183
1038.889785	145.879071	49.283188
1035.315502	141.537957	49.288193
1032.102469	137.469323	49.293197
1028.325296	139.218700	49.298202
1024.771345	140.316184	49.303207
1021.474732	144.980135	49.308212
1017.970177	138.119201	49.313217
1014.569687	132.039260	49.318221
1010.746044	149.732093	49.323226
1007.450131	130.585013	49.328231
1003.704401	137.657351	49.333236
1000.173924	139.251051	49.338241
996.900923	138.896655	49.343245
993.160557	148.999102	49.348250
990.052385	137.972638	49.353255
986.467504	138.426395	49.358260
983.170243	138.290942	49.363265
979.418397	137.783732	49.368269
975.470931	146.513873	49.373274
972.121950	128.548900	49.378279
968.772292	134.043764	49.383284
965.227155	130.802292	49.388289
962.107649	129.066596	49.393293
958.331354	140.712291	49.398298
954.693289	128.329279	49.403303
951.440223	136.574202	49.408308
947.610665	132.235132	49.413313
944.216692	132.725453	49.418317
940.765255	132.683759	49.423322
937.460184	132.834289	49.428327
933.695097	142.814069	49.433332
930.048760	138.370384	49.438337
926.958070	136.139796	49.443341
923.169770	141.621099	49.448346
919.912473	129.153172	49.453351
916.444089	126.750769	49.458356
912.883445	132.636197	49.463361
909.384811	133.196703	49.468365
905.351191	131.553540	49.473370
902.140595	134.906891	49.478375
899.010411	136.200663	49.483380
895.205877	136.821728	49.488385
891.927334	133.684077	49.493389
888.247531	137.749995	49.498394
884.550129	140.069079	49.503399
881.118300	136.898484	49.508404
877.858119	139.310463	49.513409
874.725111	131.913677	49.518413
870.913601	136.190054	49.523418
867.009315	129.591100	49.528423
863.693386	139.203169	49.533428
859.773995	127.743798	49.538433
856.655146	131.383359	49.543437
853.115484	128.868754	49.548442
850.023961	128.062041	49.553447
846.509331	122.268970	49.558452
842.717002	128.899394	49.563457
839.143661	133.458032	49.568461
835.616312	134.516617	49.573466
832.287806	136.259089	49.578471
828.718874	133.230210	49.583476
825.369236	130.916817	49.588481
821.901751	123.920452	49.593485
818.055854	129.141884	49.598490
814.644515	124.743713	49.603495
810.955050	122.926475	49.608500
807.435287	134.791474	49.613505
804.527846	133.952786	49.618509
800.908994	135.645820	49.623514
797.506698	130.113593	49.628519
793.464107	134.065508	49.633524
789.753518	136.057656	49.638529
786.840335	132.562268	49.643533
783.359109	142.738094	49.648538
779.578127	130.766696	49.653543
775.826853	132.771548	49.658548
772.462005	135.057579	49.663553
769.507512	131.954652	49.668557
765.881245	141.115464	49.673562
762.260782	141.381885	49.678567
758.837595	130.683271	49.683572
754.968218	129.688347	49.688577
751.551752	121.734879	49.693581
747.972442	128.531297	49.698586
744.450149	130.848322	49.703591
741.073225	132.484510	49.708596
737.605981	133.938687	49.713601
734.147398	127.665477	49.718605
730.449915	132.338507	49.723610
726.856173	124.808288	49.728615
723.542554	122.334268	49.733620
720.272646	122.577446	49.738625
716.749298	122.803366	49.743629
712.971168	127.878180	49.748634
709.659053	125.008453	49.753639
705.902826	131.769316	49.758644
702.376084	134.118690	49.763649
699.219900	136.745400	49.768653
695.655435	133.801298	49.773658
692.293227	122.286399	49.778663
688.534473	129.582346	49.783668
684.860932	131.546585	49.788673
681.297741	130.440466	49.793677
678.045822	125.795917	49.798682
674.581364	127.727416	49.803687
671.055307	118.607883	49.808692
667.558500	125.616036	49.813697
664.159201	120.754126	49.818701
660.748078	130.181834	49.823706
657.189555	123.611093	49.828711
653.749785	121.669394	49.833716
649.675894	128.967251	49.838721
646.219791	117.751823	49.843725
643.070573	123.712112	49.848730
639.488476	124.871095	49.853735
636.117677	129.841015	49.858740
632.200579	128.689099	49.863745
629.385429	127.450030	49.868749
625.449643	129.490164	49.873754
621.899623	126.110390	49.878759
618.499425	124.595949	49.883764
614.558694	133.511819	49.888769
611.489693	129.427117	49.893773
608.294540	124.163091	49.898778
604.659394	125.463275	49.903783
601.150112	131.321779	49.908788
597.579111	127.287229	49.913793
593.847483	119.177544	49.918797
590.255490	128.975290	49.923802
587.021808	119.654979	49.928807
583.693417	124.225962	49.933812
579.633855	129.389195	49.938817
576.489299	119.941032	49.943821
572.990379	116.825366	49.948826
569.545178	117.877511	49.953831
566.072606	122.138881	49.958836
562.245865	117.767909	49.963841
558.747749	126.026006	49.968845
555.639995	132.296210	49.973850
552.051241	118.478806	49.978855
548.286055	131.843991	49.983860
544.856103	116.593826	49.988865
541.918539	119.474250	49.993869
537.890872	133.557604	49.998874
534.540282	126.922712	50.003879
530.787492	130.788214	50.008884
526.794123	130.948615	50.013889
523.576524	125.517292	50.018893
520.248376	128.702512	50.023898
517.201912	130.641368	50.028903
513.983582	121.388286	50.033908
509.893204	120.016788	50.038913
506.512145	121.043092	50.043917
502.921698	120.988533	50.048922
499.550339	123.506636	50.053927
496.045696	121.195503	50.058932
492.269923	125.146878	50.063937
488.944764	116.945107	50.068941
485.049497	123.939797	50.073946
481.867448	115.876968	50.078951
478.255027	125.380550	50.083956
474.865175	123.554490	50.088961
471.581562	120.180512	50.093965
467.824668	117.845625	50.098970
464.477075	123.065070	50.103975
461.248627	119.407204	50.108980
457.182301	116.408932	50.113985
453.506322	110.669783	50.118989
449.755366	122.953906	50.123994
446.370152	117.555198	50.128999
443.555676	120.425864	50.134004
439.979205	124.589655	50.139009
436.488907	119.776895	50.144013
432.565174	125.105576	50.149018
429.588772	118.861382	50.154023
425.828943	119.469309	50.159028
422.211437	118.593269	50.164033
418.981545	116.188512	50.169037
415.475280	121.252489	50.174042
411.946685	124.007227	50.179047
408.037492	119.718844	50.184052
404.821947	116.606318	50.189057
401.250945	120.256730	50.194061
397.762399	120.831667	50.199066
394.335723	115.411003	50.204071
390.864862	111.177360	50.209076
387.058156	122.502112	50.214081
384.086641	122.470877	50.219085
380.260698	122.000831	50.224090
376.455659	119.863354	50.229095
373.276023	126.584637	50.234100
369.756326	127.879484	50.239105
366.287919	126.695369	50.244109
362.575765	129.811077	50.249114
359.110363	118.138493	50.254119
355.691239	114.216304	50.259124
352.156352	120.287711	50.264129
348.959532	117.871473	50.269133
345.226483	120.645606	50.274138
341.618497	125.387017	50.279143
338.077170	119.690102	50.284148
334.676199	121.678219	50.289153
331.596067	114.956761	50.294157
327.806140	116.066160	50.299162
324.385748	114.257601	50.304167
320.622590	121.430977	50.309172
317.413512	115.318190	50.314177
313.973558	116.239893	50.319181
310.251813	129.968508	50.324186
306.649216	121.338869	50.329191
303.100282	115.345766	50.334196
299.380339	120.076255	50.339201
296.658241	115.810782	50.344205
292.792628	121.120921	50.349210
289.235032	114.898223	50.354215
285.389187	112.555205	50.359220
281.745227	124.591663	50.364225
278.918640	108.867470	50.369229
275.023721	119.759981	50.374234
271.567162	120.769725	50.379239
268.358656	117.687786	50.384244
264.541553	114.546162	50.389249
261.171685	117.459590	50.394253
257.267414	115.094099	50.399258
253.836221	110.044369	50.404263
250.644277	105.789242	50.409268
247.321678	114.339481	50.414273
244.266605	121.468400	50.419277
240.225209	121.791479	50.424282
236.760758	115.095463	50.429287
233.304170	112.564938	50.434292
229.710023	116.706263	50.439297
226.348546	112.838374	50.444301
222.447078	118.065571	50.449306
218.733967	113.464985	50.454311
215.554552	119.018838	50.459316
212.227693	114.500117	50.464321
208.895339	110.988347	50.469325
204.794838	119.049853	50.474330
201.392937	113.100202	50.479335
198.144468	112.321469	50.484340
194.650998	114.668982	50.489345
191.105785	102.907753	50.494349
187.474338	114.885326	50.499354
183.804290	111.831435	50.504359
180.668993	115.983153	50.509364
176.797832	121.477707	50.514369
173.697363	111.184412	50.519373
169.806286	120.915246	50.524378
166.196828	116.118109	50.529383
162.912197	109.574294	50.534388
159.496180	124.074477	50.539393
156.329715	111.659130	50.544397
152.548612	122.052957	50.549402
148.809043	114.381341	50.554407
145.450864	115.277642	50.559412
142.194583	120.808759	50.564417
138.956427	114.893594	50.569421
135.483438	117.038603	50.574426
131.734309	114.538132	50.579431
128.587874	117.290052	50.584436
124.302282	119.660450	50.589441
120.607206	118.780870	50.594445
116.943422	120.304035	50.599450
113.813727	116.463156	50.604455
110.480749	123.126282	50.609460
106.943030	119.396787	50.614465
103.735873	104.611837	50.619469
100.079049	109.379968	50.624474
96.361828	106.469550	50.629479
93.008956	113.793865	50.634484
89.423554	118.250252	50.639489
86.295810	119.977353	50.644493
82.484431	121.700829	50.649498
78.925422	112.830356	50.654503
75.637176	116.876356	50.659508
71.708440	116.295999	50.664513
68.505042	115.545055	50.669517
64.862099	114.261857	50.674522
61.493914	113.793001	50.679527
58.359489	117.539657	50.684532
54.373004	110.580663	50.689537
51.238777	104.715695	50.694541
47.347966	109.976092	50.699546
43.949639	113.514160	50.704551
40.636647	111.132063	50.709556
36.838742	113.233102	50.714561
33.133651	111.222492	50.719565
29.828469	114.410610	50.724570
26.632092	116.445881	50.729575
23.438937	104.414439	50.734580
19.410938	116.881309	50.739585
15.865687	111.985597	50.744589
11.769183	112.617976	50.749594
8.806488	110.582808	50.754599
5.510896	112.367873	50.759604
2.032352	112.552253	50.764609