Thu Aug 25 16:35:46 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
2.360799	107.812627	0.000000
1.881530	95.773595	0.005005
1.856297	93.341457	0.010010
1.737343	105.588165	0.015014
1.747148	93.814195	0.020019
1.523465	78.375187	0.025024
1.331742	77.348547	0.030029
1.263737	66.675128	0.035034
0.575410	58.775468	0.040038
0.081005	45.682139	0.045043
-0.004959	38.523346	0.050048
-0.358429	26.632331	0.055053
-0.252195	27.811619	0.060058
-0.790027	23.460299	0.065062
-0.887548	22.890306	0.070067
-1.234459	16.772161	0.075072
-1.610074	15.698408	0.080077
-1.592496	1.683328	0.085082
-2.058008	10.007410	0.090086
-2.193169	4.884318	0.095091
-2.379876	-6.596203	0.100096
-3.003333	1.936121	0.105101
-3.286079	-5.457578	0.110106
-3.742201	-9.897623	0.115110
-4.101453	-4.200307	0.120115
-4.261121	-11.597468	0.125120
-4.412434	-3.297312	0.130125
-4.499525	-4.552313	0.135130
-4.677395	-3.012136	0.140134
-5.044448	-2.097218	0.145139
-5.355842	-5.626627	0.150144
-6.142062	3.972080	0.155149
-5.671063	-4.393937	0.160154
-5.929968	-0.876361	0.165158
-5.861978	-12.276561	0.170163
-6.072778	-6.036191	0.175168
-6.876890	-3.784121	0.180173
-6.844169	-8.383017	0.185178
-7.017478	-6.947959	0.190182
-7.986199	-4.882071	0.195187
-8.396476	-4.419127	0.200192
-8.743439	3.541525	0.205197
-8.406215	-5.537525	0.210202
-8.549768	-11.678031	0.215206
-8.637119	-4.039634	0.220211
-8.507396	-11.004409	0.225216
-9.299793	-8.769994	0.230221
-9.780833	-7.552477	0.235226
-9.797708	-13.178153	0.240230
-10.017167	-6.135993	0.245235
-9.770874	-17.481868	0.250240
-11.296690	-3.154508	0.255245
-11.638357	-5.989471	0.260250
-11.970927	5.170662	0.265254
-11.397285	0.724294	0.270259
-11.425066	-7.338942	0.275264
-12.121657	3.308748	0.280269
-11.692110	-5.658217	0.285274
-12.154844	-3.272973	0.290278
-12.375360	-5.699810	0.295283
-12.727242	-9.988506	0.300288
-13.156642	-1.518227	0.305293
-13.226114	-10.533553	0.310298
-13.619507	-1.970839	0.315302
-14.073803	-0.785986	0.320307
-14.672155	-3.333957	0.325312
-14.708650	-9.418470	0.330317
-15.123148	-1.773107	0.335322
-15.000717	3.475415	0.340326
-14.962197	1.438263	0.345331
-14.692675	-5.304807	0.350336
-15.186137	-1.747317	0.355341
-15.501251	1.551275	0.360346
-16.002964	-2.634853	0.365350
-16.363997	-4.704313	0.370355
-16.540434	-13.734515	0.375360
-17.407491	0.116307	0.380365
-17.193617	-3.919348	0.385370
-17.202774	0.985957	0.390374
-17.419518	-7.041345	0.395379
-17.452804	-9.671524	0.400384
-18.256316	-7.024077	0.405389
-19.082276	-7.755182	0.410394
-19.020847	-5.825391	0.415398
-19.067085	-7.444298	0.420403
-19.262272	-0.428085	0.425408
-19.291253	-5.229286	0.430413
-19.294164	-9.167698	0.435418
-19.402049	1.137812	0.440422
-20.372062	1.618855	0.445427
-20.436923	-5.454639	0.450432
-21.015364	-7.657714	0.455437
-20.871998	-2.871221	0.460442
-20.594757	-0.605082	0.465446
-21.389840	2.806678	0.470451
-21.672835	-4.678730	0.475456
-22.046215	5.734821	0.480461
-22.073614	-9.526054	0.485466
-22.353327	-3.831709	0.490470
-22.674481	-7.312131	0.495475
-23.191326	-8.664311	0.500480
-23.339141	5.542058	0.505485
-23.331864	-5.253843	0.510490
-23.623467	-5.173326	0.515494
-23.665311	-12.573128	0.520499
-23.909773	-4.634867	0.525504
-24.841449	-2.887995	0.530509
-25.012828	-5.496538	0.535514
-25.079651	-0.487285	0.540518
-25.284624	-2.856445	0.545523
-25.118310	-8.567773	0.550528
-25.549024	0.440553	0.555533
-25.617080	-6.891869	0.560538
-26.014245	-3.181787	0.565542
-26.192037	-4.764263	0.570547
-26.353110	-1.803021	0.575552
-27.066111	-3.288983	0.580557
-27.396499	-12.747481	0.585562
-27.895550	0.764104	0.590566
-28.202042	-3.699385	0.595571
-27.951285	-11.572142	0.600576
-28.137381	-2.336389	0.605581
-28.274706	-4.595925	0.610586
-27.974840	-8.762112	0.615590
-28.871274	-12.873734	0.620595
-29.324200	-12.211117	0.625600
-29.697816	-6.018003	0.630605
-29.738217	-14.797433	0.635610
-29.815273	-12.279630	0.640614
-29.942500	-1.259243	0.645619
-30.195332	-3.386785	0.650624
-30.526896	-3.616384	0.655629
-30.831909	-13.173771	0.660634
-30.880212	-5.291556	0.665638
-31.083091	-6.471466	0.670643
-32.074932	-21.438845	0.675648
-32.613605	-6.120874	0.680653
-31.925175	-7.668231	0.685658
-31.887389	-6.955950	0.690662
-32.506621	-11.835508	0.695667
-32.993771	-17.381169	0.700672
-33.481850	-7.117335	0.705677
-33.214056	-16.679048	0.710682
-33.665984	-6.620195	0.715686
-33.673474	-22.643480	0.720691
-34.219743	-17.872323	0.725696
-34.834276	-5.313925	0.730701
-34.983268	-16.202393	0.735706
-35.142488	-12.855464	0.740710
-35.129160	-5.713736	0.745715
-35.365154	-7.600306	0.750720
-35.600482	-10.818926	0.755725
-35.551898	-18.185437	0.760730
-36.371510	-11.941427	0.765734
-36.936042	-7.107294	0.770739
-36.766696	-16.324549	0.775744
-36.795140	-10.394330	0.780749
-36.889992	-16.052078	0.785754
-37.026478	-12.037992	0.790758
-37.526378	-4.932909	0.795763
-37.662192	-16.424557	0.800768
-37.931837	-11.082970	0.805773
-38.620129	-3.325105	0.810778
-39.496108	-9.410960	0.815782
-39.888953	-10.421898	0.820787
-39.127732	-5.260815	0.825792
-39.634093	-1.530460	0.830797
-39.858757	-12.979714	0.835802
-39.787315	-10.276370	0.840806
-39.974455	-6.225872	0.845811
-39.622735	-6.211353	0.850816
-40.871460	-11.333965	0.855821
-41.149471	-0.837285	0.860826
-41.202923	-8.399785	0.865830
-41.083325	-5.887483	0.870835
-41.162861	-9.987895	0.875840
-42.319232	-11.413876	0.880845
-42.105375	-13.538610	0.885850
-42.245033	-14.544927	0.890854
-42.953083	-4.360520	0.895859
-42.638225	-10.449463	0.900864
-43.479939	-9.074191	0.905869
-44.069960	-7.934510	0.910874
-44.478324	-1.489176	0.915878
-44.494642	-5.862087	0.920883
-44.281762	-13.548573	0.925888
-44.406112	0.318753	0.930893
-44.340769	-0.662737	0.935898
-44.000610	-11.010915	0.940902
-44.947312	-5.841653	0.945907
-45.384007	-7.098822	0.950912
-45.540286	-9.833116	0.955917
-45.971645	-3.093113	0.960922
-46.517486	-3.187896	0.965926
-47.064826	8.730392	0.970931
-47.110297	-5.777836	0.975936
-47.349160	-3.829467	0.980941
-47.015992	-10.721713	0.985946
-47.314171	-11.364668	0.990950
-47.317198	-4.770874	0.995955
-47.271650	-12.079964	1.000960
-48.088892	-5.111819	1.005965
-48.336808	-3.076610	1.010970
-48.508647	-7.083465	1.015974
-48.909987	-11.449831	1.020979
-49.679513	-8.070549	1.025984
-50.056409	-4.034611	1.030989
-50.393085	-6.417935	1.035994
-50.246840	-7.861356	1.040998
-50.721051	-5.509114	1.046003
-50.010020	-13.982338	1.051008
-50.382382	-8.286133	1.056013
-50.399094	-16.803516	1.061018
-51.060560	-8.328517	1.066022
-51.632150	-8.602764	1.071027
-51.617967	-11.325802	1.076032
-51.957666	-14.736875	1.081037
-51.537574	-23.205637	1.086042
-52.365920	-16.308523	1.091046
-53.226090	-13.981229	1.096051
-53.119652	-16.487766	1.101056
-53.254927	-5.861594	1.106061
-53.180839	-7.603759	1.111066
-54.075594	-6.258140	1.116070
-54.255560	-1.079300	1.121075
-54.364249	-9.512671	1.126080
-54.982064	-5.926205	1.131085
-54.721837	-6.846481	1.136090
-54.916867	-12.947280	1.141094
-54.958057	-7.480136	1.146099
-54.865274	-6.922007	1.151104
-55.696644	0.045190	1.156109
-55.817384	-7.237845	1.161114
-56.124021	1.121449	1.166118
-56.586238	-1.606038	1.171123
-57.324361	-3.043768	1.176128
-57.201119	-6.979799	1.181133
-57.436397	-13.463435	1.186138
-57.748265	-8.153197	1.191142
-57.891148	-11.269241	1.196147
-57.878858	-8.705326	1.201152
-57.717766	-0.593327	1.206157
-58.124827	-11.501470	1.211162
-58.618082	-7.282785	1.216166
-59.261815	1.183112	1.221171
-59.141578	3.682659	1.226176
-59.327799	-5.437759	1.231181
-60.083942	2.795815	1.236186
-60.414274	-2.799729	1.241190
-60.785541	-2.042338	1.246195
-60.661229	-14.773811	1.251200
-61.274237	-2.740837	1.256205
-61.084921	-4.741503	1.261210
-60.946284	-9.436087	1.266214
-61.176110	-4.717673	1.271219
-61.017280	-7.748114	1.276224
-61.643611	-4.679171	1.281229
-62.066136	-2.879195	1.286234
-62.241265	-8.647753	1.291238
-62.961325	0.814035	1.296243
-63.275171	-8.779931	1.301248
-63.559541	-9.532617	1.306253
-63.943256	-10.469055	1.311258
-63.922075	-14.961734	1.316262
-64.028962	-7.892923	1.321267
-63.773695	-16.509868	1.326272
-64.194092	-4.152733	1.331277
-65.024945	-4.791318	1.336282
-65.073502	-13.547321	1.341286
-65.776491	-4.524810	1.346291
-65.562997	-8.335777	1.351296
-65.679992	-5.935102	1.356301
-65.340267	-12.913796	1.361306
-65.859836	-14.812878	1.366310
-67.005528	-16.063357	1.371315
-66.874698	-17.380975	1.376320
-67.216862	-12.591177	1.381325
-67.087036	-11.042266	1.386330
-67.128127	-9.200816	1.391334
-67.939804	-7.618276	1.396339
-68.052731	-0.263776	1.401344
-68.250981	-2.472636	1.406349
-68.139561	-4.660414	1.411354
-68.669333	-7.377314	1.416358
-69.570327	-9.286234	1.421363
-69.838630	-9.971834	1.426368
-70.214689	6.197029	1.431373
-69.498763	-10.274975	1.436378
-70.151400	-4.313389	1.441382
-70.032003	-11.086717	1.446387
-70.262255	-8.282316	1.451392
-70.650653	-3.260644	1.456397
-71.185739	-8.422304	1.461402
-71.332309	-0.926491	1.466406
-71.143199	2.400663	1.471411
-71.543376	-2.481580	1.476416
-71.912053	-0.212311	1.481421
-72.199376	-10.262851	1.486426
-72.630390	-7.958506	1.491430
-73.207973	0.019297	1.496435
-73.328076	-3.369238	1.501440
-73.228073	-1.606844	1.506445
-73.084103	-3.255554	1.511450
-73.463969	-9.064798	1.516454
-74.498770	-4.824532	1.521459
-74.619353	-7.463178	1.526464
-74.687713	1.937625	1.531469
-74.711688	6.449780	1.536474
-74.479915	-0.043766	1.541478
-75.233925	-5.183778	1.546483
-75.676274	-0.789569	1.551488
-75.950617	3.755488	1.556493
-76.190383	-4.002445	1.561498
-76.310601	-10.374394	1.566502
-76.343025	-0.333815	1.571507
-76.646561	-7.765377	1.576512
-77.238617	0.005884	1.581517
-77.690341	-5.371319	1.586522
-77.745741	-6.871730	1.591526
-77.819930	-7.046742	1.596531
-77.531387	-2.235544	1.601536
-77.759446	-3.155242	1.606541
-78.418997	-9.695784	1.611546
-78.463362	-5.591728	1.616550
-78.789812	-1.725046	1.621555
-79.539568	-15.768565	1.626560
-80.103232	-1.908337	1.631565
-79.937311	3.371331	1.636570
-80.220850	-1.352016	1.641574
-80.453092	-7.630482	1.646579
-79.986988	-7.206779	1.651584
-80.213858	-5.779147	1.656589
-80.914472	-13.411081	1.661594
-81.441480	-11.287848	1.666598
-81.839554	-7.248592	1.671603
-81.324733	-9.876068	1.676608
-81.579365	-14.059773	1.681613
-82.430602	-6.817381	1.686618
-82.850700	-5.704322	1.691622
-83.292015	-5.704749	1.696627
-83.288034	-13.769791	1.701632
-83.102703	-8.271704	1.706637
-83.215714	-13.388765	1.711642
-84.051138	-12.659884	1.716646
-84.471352	-6.589184	1.721651
-84.819300	-12.049084	1.726656
-85.123388	-8.265001	1.731661
-85.240423	-20.563181	1.736666
-84.876456	-9.809596	1.741670
-85.242437	-8.375985	1.746675
-84.945937	-10.491523	1.751680
-85.559504	-12.847276	1.756685
-86.163415	-10.057093	1.761690
-86.528121	1.487721	1.766694
-86.922248	0.657320	1.771699
-86.468769	-2.014329	1.776704
-86.482224	-4.596994	1.781709
-87.166377	-3.701989	1.786714
-87.516118	-1.277499	1.791718
-88.155219	-1.670879	1.796723
-87.807160	-8.236427	1.801728
-88.114498	-5.881857	1.806733
-88.717260	-6.660584	1.811738
-88.852507	-3.551529	1.816742
-89.495902	-4.788962	1.821747
-89.371755	-12.505836	1.826752
-89.742129	-5.487487	1.831757
-89.721536	-4.304276	1.836762
-89.781991	-16.494263	1.841766
-90.733374	4.276276	1.846771
-90.605759	-5.658947	1.851776
-90.724393	-0.594122	1.856781
-90.745624	-0.922965	1.861786
-90.777670	-11.582980	1.866790
-91.854431	1.041521	1.871795
-92.166025	-7.385365	1.876800
-92.176511	-3.463788	1.881805
-92.363046	-5.241045	1.886810
-92.376060	-5.058646	1.891814
-92.876592	-1.126721	1.896819
-93.293982	-5.171029	1.901824
-93.284172	3.420255	1.906829
-93.627004	-7.304959	1.911834
-93.635367	-9.989662	1.916838
-94.005586	1.669912	1.921843
-94.418677	-9.037965	1.926848
-94.939647	4.249262	1.931853
-94.980733	5.663603	1.936858
-95.149873	-4.943296	1.941862
-95.710682	3.724745	1.946867
-95.238185	-2.705278	1.951872
-95.690709	1.965775	1.956877
-95.910169	1.266194	1.961882
-96.529619	-9.203703	1.966886
-97.045734	-0.897009	1.971891
-96.821431	-5.158925	1.976896
-96.728404	-7.274218	1.981901
-97.113714	-9.178517	1.986906
-97.146065	-6.357669	1.991910
-97.854283	-2.089480	1.996915
-98.081281	-2.876156	2.006912
-98.180276	-5.480379	2.016909
-97.207211	-1.438608	2.026906
-97.117639	-9.831473	2.036902
-96.129304	-0.451153	2.046899
-95.781881	-8.862247	2.056896
-95.604176	-8.164611	2.066893
-95.321715	-1.125577	2.076890
-94.424033	-2.435111	2.086886
-93.509843	-2.815894	2.096883
-92.861547	-4.704076	2.106880
-92.707370	-6.559183	2.116877
-92.910946	-4.908478	2.126874
-92.258511	-7.766661	2.136870
-91.684886	-4.637989	2.146867
-90.528852	-0.906822	2.156864
-90.174616	-0.373063	2.166861
-89.922046	-4.844367	2.176858
-89.215442	-3.687908	2.186854
-88.784143	-7.354081	2.196851
-88.487121	-4.286605	2.206848
-87.845107	-4.745116	2.216845
-87.529245	-10.575827	2.226842
-86.795515	-7.592619	2.236838
-86.282965	-1.489298	2.246835
-85.768547	-0.407262	2.256832
-85.320592	-1.928263	2.266829
-84.432148	-0.135054	2.276826
-84.056809	1.174683	2.286822
-84.185753	-6.198753	2.296819
-83.821017	-6.449090	2.306816
-82.966790	-9.022110	2.316813
-82.236830	-2.331962	2.326810
-81.478614	-6.613231	2.336806
-81.556963	-7.139433	2.346803
-80.660479	-11.508891	2.356800
-80.006814	-9.872131	2.366797
-79.861092	-12.625573	2.376794
-79.985679	-10.676799	2.386790
-79.364353	-9.440453	2.396787
-78.015250	-10.865069	2.406784
-77.703227	-10.058598	2.416781
-77.472612	-9.467454	2.426778
-76.560591	-8.143609	2.436774
-76.186130	-6.979454	2.446771
-76.168418	-6.526012	2.456768
-75.217932	-10.162662	2.466765
-74.758414	-6.407888	2.476762
-74.580615	-2.852893	2.486758
-74.121710	4.063464	2.496755
-73.377703	-1.378170	2.506752
-72.278149	-10.128864	2.516749
-72.296158	-2.890692	2.526746
-72.104105	-2.705322	2.536742
-71.170924	-3.054232	2.546739
-70.439460	-2.291308	2.556736
-70.290403	-6.543652	2.566733
-69.953093	-3.875297	2.576730
-69.226842	-2.557188	2.586726
-69.144313	-5.215198	2.596723
-68.197926	-4.666516	2.606720
-67.872576	-2.556991	2.616717
-67.378165	-7.116874	2.626714
-66.604366	-5.502104	2.636710
-66.342953	3.333219	2.646707
-65.748811	-4.774412	2.656704
-65.065327	-4.675547	2.666701
-64.987763	3.029161	2.676698
-64.516803	3.497115	2.686694
-63.055396	-0.856324	2.696691
-63.327725	-1.820969	2.706688
-63.085075	-2.280259	2.716685
-62.206502	-6.317457	2.726682
-61.552716	-2.650141	2.736678
-61.506537	-5.210589	2.746675
-60.599170	-7.316760	2.756672
-60.452326	-0.256473	2.766669
-59.865331	-1.552169	2.776666
-59.010848	-5.715473	2.786662
-58.794610	1.977010	2.796659
-58.499238	-2.520009	2.806656
-57.711287	-4.217828	2.816653
-57.505917	-3.141219	2.826650
-56.472635	-3.337917	2.836646
-55.867854	-3.233056	2.846643
-55.708929	-8.940975	2.856640
-55.780956	-6.664648	2.866637
-55.006369	-4.812413	2.876634
-54.303263	-1.992297	2.886630
-53.299319	-0.407251	2.896627
-53.689502	-2.642733	2.906624
-52.973601	0.162708	2.916621
-51.836157	-2.720784	2.926618
-51.810459	0.024909	2.936614
-51.399826	0.692385	2.946611
-50.448797	-0.565316	2.956608
-49.791051	-6.886757	2.966605
-49.866758	-7.780840	2.976602
-49.731113	-10.529536	2.986598
-48.782430	-8.368791	2.996595
-48.467207	-8.281915	3.006592
-47.219505	-12.285082	3.016589
-47.105590	-6.372722	3.026586
-46.829396	-6.422283	3.036582
-46.249334	-10.957572	3.046579
-45.496235	-8.591951	3.056576
-45.430672	-3.077495	3.066573
-45.043571	-10.962613	3.076570
-44.495146	-8.929222	3.086566
-43.570446	-4.940054	3.096563
-42.915755	-5.533597	3.106560
-42.638944	-7.236856	3.116557
-42.483558	-5.845137	3.126554
-41.775008	-3.079725	3.136550
-41.404787	-8.985479	3.146547
-40.410481	-3.458153	3.156544
-39.932741	-9.127328	3.166541
-39.859782	-8.305572	3.176538
-39.765847	-6.682477	3.186534
-38.492083	-14.358061	3.196531
-37.869136	-8.148489	3.206528
-37.802366	-7.408127	3.216525
-36.518089	-12.665144	3.226522
-37.156498	-12.226107	3.236518
-36.578081	-12.338861	3.246515
-35.275691	-8.906219	3.256512
-35.096748	-12.292095	3.266509
-34.906891	-14.947914	3.276506
-34.007592	-7.546192	3.286502
-33.767003	-8.321940	3.296499
-33.301359	-7.384314	3.306496
-32.591702	-11.062422	3.316493
-32.479796	-11.428365	3.326490
-32.203225	-13.480046	3.336486
-31.455576	-14.069146	3.346483
-30.049620	-14.020123	3.356480
-30.000144	-11.772337	3.366477
-29.652033	-14.665196	3.376474
-29.459036	-14.780916	3.386470
-28.713124	-9.943269	3.396467
-28.250829	-14.745207	3.406464
-27.829291	-16.021312	3.416461
-26.982027	-11.481481	3.426458
-26.966149	-14.442662	3.436454
-25.951185	-16.138032	3.446451
-25.439889	-13.218169	3.456448
-25.099344	-12.565053	3.466445
-25.068612	-11.502262	3.476442
-23.978774	-13.168183	3.486438
-23.773005	-10.457041	3.496435
-23.525021	-15.253910	3.506432
-22.390066	-17.541456	3.516429
-22.193426	-13.111926	3.526426
-21.527676	-0.015880	3.536422
-20.712474	-3.704189	3.546419
-20.574904	2.628957	3.556416
-20.812660	-6.580610	3.566413
-19.581268	-5.972040	3.576410
-19.126802	-6.245938	3.586406
-18.842001	-7.744540	3.596403
-18.047873	0.655691	3.606400
-17.515627	-8.848753	3.616397
-17.407475	-9.423184	3.626394
-16.357494	-10.791420	3.636390
-16.118879	-9.080119	3.646387
-15.786544	-8.089927	3.656384
-15.135868	-7.558262	3.666381
-14.611766	-4.624564	3.676378
-14.244775	-7.621752	3.686374
-13.520765	-3.984442	3.696371
-13.165453	-7.683056	3.706368
-12.859915	-5.731983	3.716365
-11.841350	-5.242121	3.726362
-11.722756	-7.142338	3.736358
-11.374926	-10.481816	3.746355
-10.347649	-5.913165	3.756352
-10.181461	-6.306621	3.766349
-9.880589	0.688356	3.776346
-9.074267	-1.902495	3.786342
-8.590439	-7.778533	3.796339
-8.329614	-1.905026	3.806336
-7.474222	-4.427538	3.816333
-7.432433	-6.347399	3.826330
-6.443408	2.997987	3.836326
-6.301589	4.290464	3.846323
-5.820036	3.625849	3.856320
-5.264795	12.231411	3.866317
-4.868445	14.370999	3.876314
-4.365827	23.583532	3.886310
-4.109230	35.989773	3.896307
-3.452663	44.370398	3.906304
-2.617458	53.470647	3.916301
-2.422041	61.891857	3.926298
-2.111471	68.426006	3.936294
-1.679681	83.716071	3.946291
-1.317836	97.936875	3.956288
-0.708775	113.462122	3.966285
0.000000	128.874956	3.971290
0.150512	118.970872	3.976294
0.237871	132.577342	3.981299
0.339799	127.344300	3.986304
0.482448	144.327376	3.991309
0.124725	136.005718	3.996314
0.522916	139.584883	4.001318
0.564504	158.029661	4.006323
1.147963	153.765218	4.011328
0.523845	146.858383	4.016333
0.394688	155.904961	4.021338
1.150698	155.065188	4.026342
0.632284	142.560851	4.031347
0.863928	146.590062	4.036352
0.671487	148.502699	4.041357
0.724666	131.748418	4.046362
0.677938	133.676189	4.051366
0.658869	149.390615	4.056371
0.777057	158.854028	4.061376
1.014337	158.478349	4.066381
0.840407	161.141072	4.071386
1.012417	147.946416	4.076390
0.446451	153.071884	4.081395
0.810254	151.600691	4.086400
1.233450	161.614273	4.091405
1.002824	157.271735	4.096410
1.192287	148.873828	4.101414
0.680878	146.824746	4.106419
1.008242	142.046766	4.111424
0.778868	148.078126	4.116429
0.880324	140.785522	4.121434
1.131516	152.075749	4.126438
1.107290	153.639323	4.131443
1.134623	147.155607	4.136448
1.001929	141.386675	4.141453
1.019757	142.753831	4.146458
1.148219	146.049388	4.151462
0.996319	154.441460	4.156467
0.855090	136.341383	4.161472
0.661133	144.505918	4.166477
0.710180	157.476159	4.171482
1.212144	154.170461	4.176486
0.933078	160.864517	4.181491
1.274396	167.024768	4.186496
1.621759	176.332058	4.191501
1.488328	175.685428	4.196506
1.122616	161.875812	4.201510
0.428117	154.518086	4.206515
1.387808	158.797064	4.211520
1.692993	162.754644	4.216525
1.504796	160.471418	4.221530
1.142902	149.543436	4.226534
0.652597	152.284201	4.231539
1.193556	158.979490	4.236544
1.418335	161.930924	4.241549
1.490708	162.587171	4.246554
1.425307	155.077092	4.251558
1.134387	155.002475	4.256563
1.083582	141.048622	4.261568
1.517900	149.851885	4.266573
1.341847	152.037205	4.271578
1.171984	158.799573	4.276582
0.837337	164.413992	4.281587
1.477586	164.392798	4.286592
1.498090	168.562664	4.291597
1.454929	169.151591	4.296602
1.272293	164.330125	4.301606
1.023404	171.405441	4.306611
1.516471	165.721956	4.311616
1.369731	174.524523	4.316621
1.632164	172.990115	4.321626
1.562476	176.199664	4.326630
1.668551	173.835528	4.331635
1.719683	164.823363	4.336640
1.587439	167.166338	4.341645
1.225269	174.173981	4.346650
1.558972	177.750603	4.351654
1.284844	171.133776	4.356659
1.438478	168.724223	4.361664
1.580928	179.025416	4.366669
1.780820	179.171295	4.371674
1.778064	168.269290	4.376678
1.549061	181.283114	4.381683
1.511916	172.199353	4.386688
1.454351	176.485859	4.391693
1.369150	172.734309	4.396698
1.595269	164.637540	4.401702
1.222787	173.168587	4.406707
1.140459	166.246459	4.411712
1.183838	169.305411	4.416717
1.246187	173.269402	4.421722
1.714354	187.129465	4.426726
1.851286	183.355764	4.431731
2.094565	187.939990	4.436736
1.891350	188.864048	4.441741
1.540120	179.570064	4.446746
1.895125	186.256533	4.451750
1.856750	190.793140	4.456755
1.894814	182.808086	4.461760
1.871907	175.509643	4.466765
1.543023	177.535411	4.471770
1.826927	171.476566	4.476774
2.061369	188.154232	4.481779
1.937220	179.242290	4.486784
1.478889	183.275210	4.491789
2.059962	188.939152	4.496794
1.896476	189.597554	4.501798
1.912129	201.753634	4.506803
1.855236	196.969406	4.511808
2.225200	185.543912	4.516813
1.741416	197.987053	4.521818
2.103208	190.242344	4.526822
2.098235	199.225194	4.531827
1.905249	203.513941	4.536832
1.994462	189.807035	4.541837
1.795341	201.857559	4.546842
2.105566	189.084150	4.551846
2.103221	198.819573	4.556851
2.082329	188.350675	4.561856
2.190100	195.041082	4.566861
1.824185	189.147322	4.571866
2.146042	190.881304	4.576870
1.937528	196.823989	4.581875
2.046740	192.048539	4.586880
2.161965	196.064363	4.591885
2.083520	191.248712	4.596890
2.192167	188.248246	4.601894
2.077446	192.243150	4.606899
2.195637	184.103170	4.611904
1.883624	195.095684	4.616909
1.776085	193.097214	4.621914
2.153678	196.888430	4.626918
2.039515	192.685825	4.631923
1.496922	188.616789	4.636928
2.097083	183.359451	4.641933
1.648085	207.354528	4.646938
2.439008	209.881902	4.651942
2.469577	223.538469	4.656947
2.357678	216.095762	4.661952
2.497797	220.114019	4.666957
2.473785	230.691264	4.671962
2.393923	206.174782	4.676966
2.301306	211.029946	4.681971
2.207207	204.900599	4.686976
2.383299	212.301657	4.691981
1.964659	221.507522	4.696986
2.258028	218.193366	4.701990
2.139661	224.115608	4.706995
2.317779	218.022701	4.712000
2.022759	211.766642	4.717005
2.203927	218.888491	4.722010
2.492518	211.610831	4.727014
2.435633	217.542421	4.732019
2.680952	215.257704	4.737024
2.403424	222.733004	4.742029
2.241211	213.978872	4.747034
2.634256	216.052886	4.752038
2.189956	219.061704	4.757043
2.768366	212.887098	4.762048
2.604763	214.637033	4.767053
2.440169	213.647264	4.772058
2.539457	218.203438	4.777062
2.894182	217.084844	4.782067
2.840066	220.266651	4.787072
2.764474	216.396525	4.792077
2.318730	231.950082	4.797082
2.605968	223.087559	4.802086
2.447459	228.813609	4.807091
2.411103	224.804453	4.812096
2.901990	228.641201	4.817101
2.600657	229.643911	4.822106
2.665070	227.979170	4.827110
2.585960	247.455372	4.832115
2.800731	240.167120	4.837120
3.025471	244.273366	4.842125
2.740087	233.551647	4.847130
2.809751	231.256485	4.852134
2.571961	230.294003	4.857139
2.872025	240.418673	4.862144
2.951328	243.098680	4.867149
2.619684	236.905299	4.872154
2.674156	238.168642	4.877158
2.910526	246.056988	4.882163
3.463863	250.972308	4.887168
3.173463	238.264497	4.892173
2.790390	228.481921	4.897178
2.770442	226.210291	4.902182
2.743735	209.341902	4.907187
2.501081	221.968745	4.912192
2.677025	240.183746	4.917197
2.282370	241.333959	4.922202
3.077271	245.996290	4.927206
2.853547	246.945711	4.932211
3.112997	247.734005	4.937216
2.980644	246.217154	4.942221
2.916213	251.786098	4.947226
3.044027	241.142006	4.952230
3.140625	246.144707	4.957235
3.327324	237.269455	4.962240
3.178581	238.485544	4.967245
3.089210	248.867393	4.972250
3.250730	236.696227	4.977254
2.965856	250.278850	4.982259
2.990662	248.851271	4.987264
3.328838	246.279914	4.992269
2.936480	247.126041	4.997274
3.459009	241.333510	5.002278
3.309166	248.826780	5.007283
3.321502	239.289135	5.012288
3.134907	248.177078	5.017293
2.908763	250.531613	5.022298
3.078970	240.516806	5.027302
3.129866	253.224230	5.032307
3.473037	252.895235	5.037312
3.604160	250.872021	5.042317
2.961417	245.572119	5.047322
3.109435	241.948532	5.052326
3.351984	253.360402	5.057331
3.180853	252.567812	5.062336
3.198230	247.540976	5.067341
3.200782	260.145246	5.072346
3.501463	243.285642	5.077350
2.990878	250.734192	5.082355
3.371032	246.403504	5.087360
3.288499	251.693705	5.092365
3.135243	253.565411	5.097370
3.273806	249.108056	5.102374
3.229334	248.884091	5.107379
3.455122	252.613681	5.112384
3.398861	258.368013	5.117389
3.119354	259.285045	5.122394
3.735530	272.872043	5.127398
3.455464	272.545783	5.132403
3.182742	267.403039	5.137408
3.359901	275.246890	5.142413
3.456410	280.641928	5.147418
3.599240	273.232053	5.152422
3.597471	281.600661	5.157427
3.994456	275.587340	5.162432
3.470995	278.526312	5.167437
3.342529	283.184627	5.172442
3.703653	280.429332	5.177446
3.505410	280.207313	5.182451
3.600750	280.856802	5.187456
3.810417	285.281802	5.192461
3.803889	281.922871	5.197466
3.833432	278.102700	5.202470
3.178744	268.147519	5.207475
3.457620	273.650026	5.212480
3.568355	276.562399	5.217485
3.328592	279.757484	5.222490
3.671113	278.583850	5.227494
3.561636	275.737771	5.232499
3.650139	282.766595	5.237504
3.637116	279.949696	5.242509
3.083954	280.697630	5.247514
3.643726	275.535181	5.252518
3.735983	282.566581	5.257523
3.694466	279.437765	5.262528
3.879957	281.563289	5.267533
3.922968	290.725332	5.272538
3.824997	282.037033	5.277542
3.376286	282.702162	5.282547
3.836730	295.706123	5.287552
4.427596	308.196103	5.292557
3.894977	297.041673	5.297562
3.814707	284.285086	5.302566
3.836281	289.963956	5.307571
4.073372	295.340136	5.312576
4.004458	302.792274	5.317581
3.714789	299.136010	5.322586
4.139277	299.926923	5.327590
3.983789	295.531448	5.332595
4.241374	299.192789	5.337600
4.083588	289.735557	5.342605
3.928051	290.588874	5.347610
3.939294	289.030537	5.352614
3.921700	289.561677	5.357619
4.139424	295.684390	5.362624
4.312483	296.707690	5.367629
3.946468	290.576624	5.372634
4.181393	289.983008	5.377638
3.972222	288.652199	5.382643
4.162700	297.329222	5.387648
4.212461	300.719399	5.392653
3.992788	300.431133	5.397658
4.198098	285.025972	5.402662
4.203339	302.340783	5.407667
4.055725	301.939984	5.412672
4.145956	304.441113	5.417677
3.854048	312.772936	5.422682
4.163246	296.478272	5.427686
4.169094	304.852025	5.432691
3.968025	302.124699	5.437696
3.891416	311.878148	5.442701
3.569171	310.492286	5.447706
3.694644	306.460920	5.452710
4.060548	312.604715	5.457715
4.472337	322.053851	5.462720
4.715429	322.082228	5.467725
4.411150	318.026444	5.472730
4.415622	309.407503	5.477734
4.354486	314.827252	5.482739
4.470438	304.514019	5.487744
4.348100	299.920355	5.492749
4.112121	302.842763	5.497754
4.242913	314.357606	5.502758
4.575585	330.738433	5.507763
4.489918	318.688201	5.512768
4.449834	314.837801	5.517773
4.204936	324.652427	5.522778
4.481704	315.487771	5.527782
4.404485	327.104818	5.532787
4.631065	322.598852	5.537792
4.582152	331.256451	5.542797
4.145235	334.295770	5.547802
4.615304	330.416057	5.552806
4.490923	338.490683	5.557811
4.422095	327.529329	5.562816
4.605623	331.009286	5.567821
4.531055	333.887425	5.572826
4.507817	334.118887	5.577830
4.371809	331.539554	5.582835
4.421382	332.727740	5.587840
4.411473	328.404363	5.592845
4.025450	329.240009	5.597850
4.351583	322.212692	5.602854
4.157237	326.213773	5.607859
4.676041	340.110315	5.612864
4.936278	350.703208	5.617869
4.962625	359.928010	5.622874
4.621966	346.006756	5.627878
4.597252	339.315985	5.632883
4.656407	338.509456	5.637888
4.907293	353.425610	5.642893
4.818240	357.160258	5.647898
5.145363	344.937761	5.652902
4.766694	337.071718	5.657907
4.873520	328.057072	5.662912
4.599257	333.934172	5.667917
4.544412	330.633424	5.672922
5.036209	333.517740	5.677926
5.072994	349.767770	5.682931
4.803130	337.186387	5.687936
4.807008	344.994142	5.692941
4.725522	354.197871	5.697946
4.973239	348.625539	5.702950
4.560461	355.536775	5.707955
4.957783	354.433647	5.712960
5.010582	357.756917	5.717965
4.801420	351.253233	5.722970
4.943684	357.852873	5.727974
4.911879	354.399811	5.732979
5.035485	349.384776	5.737984
5.432463	356.482359	5.742989
5.104368	359.064859	5.747994
5.049707	356.039331	5.752998
5.004610	354.916933	5.758003
5.275143	356.295133	5.763008
5.090964	342.532866	5.768013
5.097712	354.687282	5.773018
5.037805	348.204507	5.778022
5.000990	347.473127	5.783027
5.141502	345.559165	5.788032
5.103607	348.061392	5.793037
4.945953	360.444055	5.798042
5.210205	341.331088	5.803046
5.262240	352.405868	5.808051
4.840240	356.085111	5.813056
4.982195	349.782685	5.818061
5.098246	352.150058	5.823066
4.792893	344.876816	5.828070
4.848126	355.134827	5.833075
4.948632	348.244095	5.838080
4.686118	346.934295	5.843085
5.018908	368.016594	5.848090
5.494924	368.986103	5.853094
5.610391	381.965084	5.858099
5.310492	378.161706	5.863104
5.336227	380.884928	5.868109
5.350825	388.713170	5.873114
5.742513	379.350137	5.878118
5.010302	372.482295	5.883123
5.009750	372.836757	5.888128
5.142493	381.095749	5.893133
5.017314	386.259790	5.898138
5.449293	378.725472	5.903142
5.461199	377.989622	5.908147
5.478151	377.246653	5.913152
5.487456	378.276632	5.918157
5.389008	381.699537	5.923162
5.357209	374.585908	5.928166
5.161210	385.753356	5.933171
5.191760	377.987697	5.938176
5.322087	380.991932	5.943181
5.343139	387.072723	5.948186
5.441659	380.720142	5.953190
5.245780	387.568932	5.958195
5.441258	387.753471	5.963200
5.926045	397.580362	5.968205
5.552433	393.760055	5.973210
5.653690	381.721623	5.978214
5.569571	379.450537	5.983219
5.678699	383.432557	5.988224
5.627113	370.392996	5.993229
5.232639	387.694584	5.998234
5.632074	376.359267	6.003238
5.427095	383.380329	6.008243
5.615366	397.977291	6.013248
5.951869	387.170697	6.018253
5.449897	379.956722	6.023258
5.345490	381.134235	6.028262
5.517754	387.612124	6.033267
5.557473	394.990331	6.038272
5.843145	395.277801	6.043277
5.480231	394.527908	6.048282
5.778872	380.253353	6.053286
5.613275	386.414009	6.058291
5.355119	386.473466	6.063296
5.632001	386.097906	6.068301
5.356630	385.818365	6.073306
5.619943	396.698713	6.078310
5.796837	403.147408	6.083315
5.292076	380.908786	6.088320
5.629519	397.194012	6.093325
5.628607	401.060396	6.098330
5.913175	394.972897	6.103334
5.787515	388.864251	6.108339
5.728242	380.682382	6.113344
5.890789	378.910501	6.118349
5.534156	384.699280	6.123354
5.746405	377.525266	6.128358
5.454540	381.044916	6.133363
5.750801	376.249601	6.138368
5.648269	363.376220	6.143373
5.254951	374.932090	6.148378
5.604135	378.895479	6.153382
5.628018	383.605883	6.158387
5.171892	382.566867	6.163392
5.555548	378.751304	6.168397
5.443684	387.975629	6.173402
5.592099	370.684170	6.178406
5.385450	379.328540	6.183411
5.628188	377.063191	6.188416
5.977535	378.555597	6.193421
5.374548	383.652129	6.198426
5.684406	381.493324	6.203430
5.457308	380.171645	6.208435
5.841186	382.781804	6.213440
5.603802	379.496992	6.218445
5.275169	387.448615	6.223450
5.672009	370.355520	6.228454
5.356376	382.997075	6.233459
5.139474	381.243516	6.238464
5.670024	393.973967	6.243469
5.866505	405.671571	6.248474
5.835485	381.118722	6.253478
5.626540	379.117137	6.258483
5.419128	373.404129	6.263488
5.469025	372.444022	6.268493
5.206019	384.349650	6.273498
5.775442	384.576842	6.278502
5.864415	389.593432	6.283507
5.464435	383.353758	6.288512
5.509958	371.827115	6.293517
5.321764	381.762605	6.298522
5.700824	376.194996	6.303526
5.413517	383.906018	6.308531
5.362789	389.539299	6.313536
5.918021	399.263402	6.318541
5.817060	402.133032	6.323546
5.719874	385.218571	6.328550
5.343211	379.990837	6.333555
5.321473	382.800593	6.338560
5.797915	387.854554	6.343565
5.859003	385.760037	6.348570
5.674063	383.605990	6.353574
5.267446	385.276955	6.358579
5.609943	377.718692	6.363584
5.963874	380.988457	6.368589
5.627498	381.889095	6.373594
5.735344	378.777989	6.378598
5.581119	369.279027	6.383603
5.597371	388.177278	6.388608
5.730913	382.607005	6.393613
5.624240	376.726348	6.398618
5.663201	384.117325	6.403622
5.757006	386.981747	6.408627
5.856904	383.884540	6.413632
5.983711	378.261539	6.418637
5.623548	389.179456	6.423642
5.942621	385.117739	6.428646
5.763838	383.313914	6.433651
5.707302	382.535001	6.438656
5.673108	376.991011	6.443661
5.300150	370.361119	6.448666
5.856792	370.827601	6.453670
5.460237	367.181742	6.458675
5.444568	369.870320	6.463680
5.446094	374.441852	6.468685
5.378193	391.885271	6.473690
5.545271	382.554265	6.478694
5.307113	374.808562	6.483699
5.448436	379.212655	6.488704
5.665881	384.180640	6.493709
5.382290	389.609955	6.498714
5.824583	378.834248	6.503718
5.635908	372.991752	6.508723
5.683266	378.397684	6.513728
5.863711	382.463445	6.518733
5.328494	386.584388	6.523738
5.819659	386.874463	6.528742
5.984449	378.255681	6.533747
5.819634	369.976456	6.538752
5.453567	363.086053	6.543757
5.290776	362.133959	6.548762
5.306927	372.866352	6.553766
5.605328	384.392945	6.558771
5.357047	383.802267	6.563776
5.453552	377.832827	6.568781
5.612694	382.012660	6.573786
5.382718	375.929854	6.578790
5.507548	385.205680	6.583795
5.513412	378.095640	6.588800
5.669008	386.148568	6.593805
5.541825	376.433388	6.598810
5.633240	378.067450	6.603814
5.508750	380.994549	6.608819
5.753984	380.389824	6.613824
5.718424	381.654628	6.618829
5.483744	384.981817	6.623834
5.656665	371.903915	6.628838
5.527712	373.670583	6.633843
5.523126	377.373018	6.638848
5.967842	381.710592	6.643853
5.398034	384.188594	6.648858
5.805073	380.394678	6.653862
5.495225	381.680312	6.658867
5.651957	383.810355	6.663872
5.865153	383.969971	6.668877
5.473471	379.377358	6.673882
5.679705	382.515237	6.678886
5.635339	381.433853	6.683891
5.564846	378.094419	6.688896
5.793425	365.944297	6.693901
5.715386	363.533051	6.698906
5.819334	353.193196	6.703910
5.335946	355.812682	6.708915
5.295488	353.569561	6.713920
5.576727	361.004827	6.718925
5.631707	358.892287	6.723930
5.688784	367.609229	6.728934
5.673354	361.236543	6.733939
5.271175	356.819591	6.738944
6.037446	358.888930	6.743949
5.719059	369.740177	6.748954
5.603108	361.168555	6.753958
5.573396	361.897754	6.758963
5.427624	357.813961	6.763968
5.328183	349.916818	6.768973
5.303095	356.207312	6.773978
5.550482	369.323806	6.778982
5.483021	376.873826	6.783987
5.639616	377.776321	6.788992
5.717040	377.776871	6.793997
5.555123	382.158871	6.799002
5.777684	379.684706	6.804006
5.514172	373.714726	6.809011
5.416221	362.625032	6.814016
5.743295	368.528151	6.819021
5.292575	372.344779	6.824026
5.551352	370.405957	6.829030
5.708109	376.778701	6.834035
5.936711	380.466747	6.839040
5.738459	366.735141	6.844045
5.634619	364.631666	6.849050
5.864785	358.752024	6.854054
5.818305	357.819673	6.859059
5.290087	359.104718	6.864064
5.725931	356.717364	6.869069
5.515497	354.475563	6.874074
5.302758	357.701230	6.879078
5.468270	354.290020	6.884083
5.075967	357.164161	6.889088
5.702146	362.346517	6.894093
5.481765	376.779694	6.899098
5.576233	377.672939	6.904102
5.849056	374.257567	6.909107
5.478410	359.784165	6.914112
5.755137	354.352822	6.919117
5.331771	354.324266	6.924122
5.518001	368.497570	6.929126
5.574700	379.900675	6.934131
5.595387	371.902440	6.939136
6.026614	361.368930	6.944141
5.297786	363.612410	6.949146
5.500677	354.551061	6.954150
5.737244	359.905195	6.959155
5.773287	366.907470	6.964160
5.454038	350.939019	6.969165
5.234240	360.771878	6.974170
5.567289	360.735540	6.979174
5.685719	373.369192	6.984179
5.942346	379.381431	6.989184
5.510757	349.655235	6.994189
5.500650	346.799902	6.999194
5.226872	339.043977	7.004198
5.434056	365.176447	7.009203
5.758605	375.487188	7.014208
6.012749	367.794071	7.019213
5.407582	359.865427	7.024218
5.570526	350.645820	7.029222
5.270993	354.910167	7.034227
5.794804	365.879398	7.039232
5.919682	364.116584	7.044237
5.392420	360.696855	7.049242
5.435203	347.566593	7.054246
5.775354	345.130957	7.059251
5.263553	352.209571	7.064256
5.749212	364.156076	7.069261
5.627732	368.788008	7.074266
5.480071	345.088737	7.079270
5.601375	366.568012	7.084275
5.473877	372.719530	7.089280
6.104295	365.350284	7.094285
5.526941	359.097279	7.099290
5.651333	350.149474	7.104294
5.570223	351.304352	7.109299
5.396076	353.533691	7.114304
5.691810	336.488108	7.119309
5.568794	350.845897	7.124314
5.612941	348.937541	7.129318
5.757727	350.923916	7.134323
5.381411	358.307179	7.139328
5.558091	350.373100	7.144333
5.472113	355.897996	7.149338
5.629361	347.125383	7.154342
5.434297	356.207700	7.159347
5.057672	348.758958	7.164352
5.855173	365.411845	7.169357
5.841567	373.418510	7.174362
5.553151	356.091101	7.179366
5.806769	358.677372	7.184371
5.578431	357.045833	7.189376
5.643491	354.947534	7.194381
5.471249	355.727539	7.199386
5.799672	359.149997	7.204390
5.713255	362.333726	7.209395
5.481707	353.599880	7.214400
5.472011	352.715551	7.219405
5.657992	354.723946	7.224410
5.916295	346.008269	7.229414
5.696824	348.317477	7.234419
5.684502	344.098880	7.239424
5.566140	350.223649	7.244429
5.434022	353.598038	7.249434
5.441806	350.588038	7.254438
5.240095	351.502378	7.259443
4.967236	351.137020	7.264448
5.598012	368.584845	7.269453
5.790897	376.530684	7.274458
5.939130	369.262296	7.279462
5.612500	354.535222	7.284467
5.607496	355.425069	7.289472
5.640532	358.998215	7.294477
5.442237	352.866160	7.299482
5.349692	347.704654	7.304486
5.578315	353.708617	7.309491
5.470321	349.182298	7.314496
5.652821	346.992831	7.319501
5.645031	348.303904	7.324506
5.653376	352.542159	7.329510
5.681121	354.679753	7.334515
5.433214	349.906429	7.339520
5.575070	347.236100	7.344525
5.451206	350.843320	7.349530
5.589584	350.407202	7.354534
5.802110	352.550646	7.359539
5.559002	352.987405	7.364544
5.893656	348.670149	7.369549
5.477477	351.649273	7.374554
5.718084	354.288203	7.379558
5.842441	357.859696	7.384563
5.699353	364.716026	7.389568
5.647553	360.259995	7.394573
5.669239	362.496618	7.399578
5.829912	354.599848	7.404582
5.443836	351.243423	7.409587
5.355366	360.679210	7.414592
5.639612	351.370992	7.419597
5.532907	353.925131	7.424602
5.540048	357.350470	7.429606
5.449108	358.636606	7.434611
5.324629	358.751050	7.439616
5.658771	349.232530	7.444621
5.645455	359.020381	7.449626
5.994497	350.176586	7.454630
5.781999	354.636110	7.459635
5.636087	360.059663	7.464640
5.701587	355.363786	7.469645
5.724089	359.188526	7.474650
5.612634	357.722176	7.479654
5.607287	352.214803	7.484659
5.327608	356.688017	7.489664
5.774210	354.033216	7.494669
5.614160	352.106233	7.499674
5.412901	356.624109	7.504678
5.378232	358.682895	7.509683
5.426495	363.566648	7.514688
5.858177	351.049347	7.519693
5.745234	362.858681	7.524698
5.605653	359.912898	7.529702
5.501614	357.347535	7.534707
5.522510	361.808458	7.539712
5.461254	354.803859	7.544717
4.964768	353.790152	7.549722
5.071945	361.458340	7.554726
5.325369	355.847145	7.559731
5.249239	358.630618	7.564736
5.678348	360.702163	7.569741
5.589316	378.987296	7.574746
5.915808	376.613909	7.579750
5.646239	372.669735	7.584755
5.133953	362.265072	7.589760
5.806497	360.134868	7.594765
5.886568	360.634889	7.599770
5.542446	362.435269	7.604774
5.481876	359.423322	7.609779
5.261345	360.634847	7.614784
5.967394	365.323787	7.619789
5.816869	365.163894	7.624794
5.780649	359.594916	7.629798
5.563374	351.931375	7.634803
5.082883	356.271533	7.639808
5.543437	355.114203	7.644813
5.576512	355.605769	7.649818
5.522217	359.572258	7.654822
5.548234	358.299510	7.659827
5.464858	357.762091	7.664832
5.759922	357.722214	7.669837
5.582965	362.353345	7.674842
5.586466	345.802805	7.679846
5.546242	350.817481	7.684851
5.372282	357.824181	7.689856
5.806303	356.724794	7.694861
5.455278	357.093038	7.699866
5.822196	350.913555	7.704870
5.889392	358.493091	7.709875
5.280735	353.254256	7.714880
5.593248	350.079449	7.719885
5.494538	354.884985	7.724890
5.427571	350.073820	7.729894
5.521012	347.012434	7.734899
5.468827	355.774964	7.739904
5.918372	363.974819	7.744909
5.933584	360.058796	7.749914
5.432715	358.150410	7.754918
5.339201	356.643283	7.759923
5.690471	357.078665	7.764928
5.623930	344.547680	7.769933
5.173290	353.783938	7.774938
5.435125	369.979743	7.779942
5.875313	376.077118	7.784947
5.466359	365.036151	7.789952
5.408376	366.937235	7.794957
5.750874	376.976239	7.799962
5.386065	382.592288	7.804966
5.595641	383.337781	7.809971
5.890137	385.079234	7.814976
5.782858	364.527958	7.819981
5.363223	360.256114	7.824986
5.658033	361.152771	7.829990
5.715175	360.941358	7.834995
5.476835	357.207435	7.840000
5.461144	347.924067	7.845005
5.331007	362.574053	7.850010
5.377924	375.943429	7.855014
5.736659	388.061701	7.860019
5.472217	381.376836	7.865024
5.982158	371.156863	7.870029
5.387987	370.424222	7.875034
5.482631	377.834946	7.880038
5.898934	383.626010	7.885043
5.352492	365.557551	7.890048
5.445953	370.611399	7.895053
5.353833	379.193531	7.900058
5.538719	384.679160	7.905062
5.634221	384.793940	7.910067
5.641759	385.064874	7.915072
5.881902	375.757226	7.920077
5.973136	380.757641	7.925082
5.623137	371.776583	7.930086
6.005050	367.157681	7.935091
5.593934	364.732181	7.940096
5.521442	359.811145	7.945101
5.747202	361.240654	7.950106
5.554394	364.093030	7.955110
5.495870	358.919863	7.960115
5.158277	367.837851	7.965120
5.548419	360.493598	7.970125
5.696754	362.382711	7.975142
5.464936	357.963119	7.980160
5.614140	357.434845	7.985178
5.193501	357.112618	7.990195
5.593956	353.288229	7.995213
5.768055	364.407135	8.000230
5.719919	364.247448	8.005248
5.770739	360.976450	8.010266
5.600485	363.796003	8.015283
5.743501	351.882702	8.020301
5.873293	355.500987	8.025318
5.789031	353.096900	8.030336
5.591330	345.948542	8.035354
5.335519	350.984220	8.040371
5.524114	347.669547	8.045389
5.319210	358.566970	8.050406
5.478449	353.382372	8.055424
5.540473	364.951178	8.060442
5.823521	383.585839	8.065459
6.040801	372.137410	8.070477
5.975253	362.487907	8.075494
5.620195	360.725843	8.080512
5.811233	357.019472	8.085530
5.730593	356.789138	8.090547
5.687861	360.592243	8.095565
5.619373	353.398391	8.100582
5.465003	355.063600	8.105600
5.745171	352.271059	8.110618
5.505876	361.308816	8.115635
5.483458	366.440472	8.120653
5.847988	371.959621	8.125670
5.937425	381.577034	8.130688
5.958518	382.744545	8.135706
5.569426	373.697989	8.140723
6.127118	362.376109	8.145741
5.624498	360.536181	8.150758
5.895508	354.226397	8.155776
5.761429	350.630926	8.160794
5.526853	357.935428	8.165811
5.540343	360.824020	8.170829
5.991274	369.504330	8.175846
5.575825	364.365591	8.180864
5.922089	371.522288	8.185882
5.747003	380.796144	8.190899
6.136565	384.417914	8.195917
5.644976	369.508224	8.200934
5.745911	361.694539	8.205952
5.893605	361.191747	8.210970
5.808993	366.121712	8.215987
5.737873	359.054500	8.221005
5.751006	371.647127	8.226022
5.556813	375.679091	8.231040
5.665279	379.991835	8.236058
5.552128	383.774420	8.241075
5.616305	382.047653	8.246093
5.987279	376.176629	8.251110
6.142318	372.971350	8.256128
6.010409	374.667756	8.261146
6.104506	389.308425	8.266163
6.170447	383.409454	8.271181
6.292654	382.503561	8.276198
5.712937	371.309394	8.281216
6.068938	367.129055	8.286234
5.675000	362.637034	8.291251
5.702940	363.383754	8.296269
5.986157	380.181729	8.301286
5.650588	381.613403	8.306304
5.755326	374.114693	8.311322
5.771831	391.737099	8.316339
6.068808	380.588599	8.321357
6.448952	383.138883	8.326374
5.980213	386.320784	8.331392
5.961353	377.913642	8.336410
5.701528	383.697875	8.341427
5.647186	375.826463	8.346445
5.810961	375.270659	8.351462
5.434715	384.203654	8.356480
5.716755	377.024298	8.361498
5.645530	394.142906	8.366515
5.646522	379.642017	8.371533
5.956278	377.185659	8.376550
5.704058	391.520834	8.381568
6.273207	393.464001	8.386586
6.099663	397.511669	8.391603
5.946661	386.591457	8.396621
6.358205	384.141240	8.401638
6.037390	386.031345	8.406656
5.976403	377.321539	8.411674
5.798606	380.457853	8.416691
5.991896	384.022013	8.421709
6.428691	389.936939	8.426726
6.173446	391.911444	8.431744
6.168322	387.715099	8.436762
6.535973	384.640605	8.441779
6.480009	387.505370	8.446797
6.296825	384.930588	8.451814
6.034022	377.404258	8.456832
5.932593	381.503739	8.461850
5.587452	386.237846	8.466867
5.752324	379.420826	8.471885
6.094345	376.227275	8.476902
5.826477	391.890324	8.481920
5.747315	379.071397	8.486938
5.974913	389.800089	8.491955
5.959072	402.542443	8.496973
6.111882	407.432063	8.501990
6.131792	403.474786	8.507008
6.597238	401.751417	8.512026
6.580467	408.646276	8.517043
6.041129	388.407640	8.522061
5.963979	384.408772	8.527078
6.378964	393.056856	8.532096
6.061698	394.700255	8.537114
5.933224	399.586609	8.542131
6.389665	402.816056	8.547149
6.299351	405.023493	8.552166
6.137015	397.572931	8.557184
6.064972	394.276997	8.562202
6.151891	404.863639	8.567219
6.322591	405.657420	8.572237
6.388042	408.231768	8.577255
6.220791	402.691217	8.582272
5.985011	387.571019	8.587290
6.357357	403.149548	8.592307
6.421923	405.780838	8.597325
6.353139	400.035513	8.602343
6.160498	387.903383	8.607360
6.383197	386.382149	8.612378
6.402040	393.334538	8.617395
6.189826	385.456300	8.622413
6.242710	388.332412	8.627431
6.006058	380.950305	8.632448
6.140466	403.594011	8.637466
6.149629	401.434053	8.642483
6.212690	404.936572	8.647501
6.447891	407.736785	8.652519
6.353674	410.471849	8.657536
6.552900	402.806846	8.662554
6.761378	400.401067	8.667571
6.260807	393.177069	8.672589
6.462919	391.084709	8.677607
5.979957	389.317436	8.682624
6.230939	388.599647	8.687642
6.140829	397.247978	8.692659
6.404990	403.354058	8.697677
6.773551	400.172123	8.702695
6.522180	395.683002	8.707712
6.349480	377.062648	8.712730
6.209270	381.875097	8.717747
6.166036	389.250617	8.722765
6.180100	394.199841	8.727783
6.507494	409.987389	8.732800
6.381264	407.817086	8.737818
6.495892	410.295367	8.742835
6.308485	411.243086	8.747853
6.874494	404.483125	8.752871
6.338279	406.896126	8.757888
6.608942	394.003442	8.762906
6.340515	397.081376	8.767923
6.148477	394.018836	8.772941
6.907919	390.639961	8.777959
6.122215	393.249838	8.782976
6.337643	400.704754	8.787994
6.283852	410.568684	8.793011
6.330672	409.090784	8.798029
6.199651	404.087348	8.803047
6.277337	412.589477	8.808064
6.866486	408.142227	8.813082
6.454688	410.895492	8.818099
6.637067	405.028762	8.823117
6.774764	401.614759	8.828135
6.229021	408.740820	8.833152
6.515336	409.926737	8.838170
6.349084	404.742630	8.843187
6.374297	409.014777	8.848205
6.770794	416.750595	8.853223
6.301685	411.894803	8.858240
6.660934	409.995569	8.863258
6.388686	408.514013	8.868275
6.692232	406.920150	8.873293
6.872593	399.952373	8.878311
6.702101	410.954888	8.883328
6.419368	412.460335	8.888346
6.865364	408.325846	8.893363
6.325792	406.747320	8.898381
6.677322	410.012141	8.903399
6.311256	420.202712	8.908416
6.445574	413.055954	8.913434
6.496710	417.715357	8.918451
6.138729	420.299247	8.923469
6.267818	408.198745	8.928487
6.204301	416.107623	8.933504
6.578106	424.913652	8.938522
6.429534	423.545259	8.943539
6.561076	428.801132	8.948557
6.881805	436.510961	8.953575
6.931986	431.523308	8.958592
7.158656	434.690932	8.963610
6.680650	423.222022	8.968627
6.281000	425.869246	8.973645
6.593372	408.763368	8.978663
6.945448	425.067764	8.983680
6.736578	423.557341	8.988698
6.911624	414.375038	8.993715
6.568935	411.632741	8.998733
6.657051	407.838344	9.003751
6.666163	410.705540	9.008768
6.505830	411.450203	9.013786
6.457825	418.305779	9.018803
6.369371	428.351874	9.023821
6.809210	431.391425	9.028839
6.331834	437.288655	9.033856
6.549758	438.680948	9.038874
7.042580	432.516263	9.043891
7.138713	434.735516	9.048909
7.029473	428.769305	9.053927
6.811975	436.380429	9.058944
6.620145	439.967072	9.063962
6.719684	437.300648	9.068979
6.929996	433.581774	9.073997
7.223734	431.699114	9.079015
6.658302	432.601922	9.084032
6.751114	437.825997	9.089050
6.924288	438.382708	9.094067
6.842198	440.408982	9.099085
6.833256	426.294617	9.104103
6.861874	433.819842	9.109120
6.862635	435.192511	9.114138
7.160251	431.974350	9.119155
7.025134	436.445192	9.124173
7.221756	428.423983	9.129191
6.981928	420.329151	9.134208
6.643773	407.661235	9.139226
6.633958	412.847734	9.144243
6.782335	431.743384	9.149261
6.817167	420.418184	9.154279
6.817103	421.942459	9.159296
6.996834	433.574917	9.164314
7.052364	428.804175	9.169331
6.696183	436.134073	9.174349
6.906280	431.989203	9.179367
6.813971	441.609879	9.184384
6.761614	442.612178	9.189402
6.933062	429.709768	9.194419
6.868182	433.279675	9.199437
6.747763	431.903715	9.204455
6.886274	431.784209	9.209472
6.777597	441.817701	9.214490
7.129506	434.693646	9.219507
6.710622	442.626658	9.224525
6.695554	433.057570	9.229543
6.910818	445.337714	9.234560
6.635461	438.513909	9.239578
7.073532	442.093377	9.244595
6.490606	446.732213	9.249613
7.201976	462.863585	9.254631
7.270733	461.824053	9.259648
7.316433	452.097112	9.264666
7.275819	441.601066	9.269683
6.909304	439.840789	9.274701
6.991949	429.221298	9.279719
7.174995	437.006348	9.284736
7.396988	436.684415	9.289754
7.093350	433.333243	9.294771
6.892586	440.443134	9.299789
6.976891	438.918333	9.304807
7.185569	439.324316	9.309824
7.427497	445.799963	9.314842
7.280768	437.318155	9.319859
7.113274	436.328263	9.324877
7.327616	436.108514	9.329895
7.223216	434.591190	9.334912
6.927430	434.372474	9.339930
6.994887	431.436525	9.344947
6.654579	429.283982	9.349965
7.156308	447.048165	9.354983
7.324349	458.941246	9.360000
7.224664	451.632322	9.365018
7.183951	442.190322	9.370035
7.252137	439.724469	9.375053
6.968954	436.991779	9.380071
7.525879	450.543822	9.385088
7.093426	453.716893	9.390106
7.299067	434.936214	9.395123
7.139282	437.795164	9.400141
7.270855	435.713851	9.405159
7.415052	449.056007	9.410176
7.307396	448.697363	9.415194
7.206026	432.126499	9.420211
7.244198	447.517587	9.425229
7.232168	425.021958	9.430247
7.344526	438.463767	9.435264
7.226364	434.499715	9.440282
7.018153	426.961655	9.445299
7.294901	446.212745	9.450317
7.352583	447.630145	9.455335
7.456185	454.607147	9.460352
7.101720	455.719897	9.465370
7.311664	460.016761	9.470387
7.111947	465.460245	9.475405
7.315523	459.801614	9.480423
7.753531	452.806072	9.485440
7.222733	463.858761	9.490458
7.512812	452.597689	9.495475
7.368132	456.928024	9.500493
7.395607	452.395199	9.505511
7.245004	451.661434	9.510528
7.056979	458.340150	9.515546
7.225619	457.903501	9.520563
7.293305	457.933947	9.525581
7.441743	453.590450	9.530599
7.499390	455.717907	9.535616
7.343189	471.745380	9.540634
7.408595	460.068228	9.545651
7.144383	467.771891	9.550669
7.376078	457.466699	9.555687
7.324138	460.845237	9.560704
7.509069	468.071432	9.565722
7.510092	464.211774	9.570739
7.528289	460.040160	9.575757
7.369778	459.279232	9.580775
7.939040	458.650426	9.585792
7.459092	460.265672	9.590810
7.627272	464.389201	9.595827
7.690974	456.335157	9.600845
7.348760	456.278349	9.605863
7.608585	457.572560	9.610880
7.827531	458.851086	9.615898
8.291837	457.490805	9.620915
7.783839	445.202921	9.625933
7.386327	442.500766	9.630951
7.452740	436.301905	9.635968
7.031984	442.840356	9.640986
7.614873	443.212954	9.646003
7.363559	457.658492	9.651021
7.471770	462.482533	9.656039
7.879433	461.162684	9.661056
7.538763	462.727705	9.666074
7.709213	458.245061	9.671091
7.722353	462.474931	9.676109
7.558005	451.338708	9.681127
7.871114	447.748890	9.686144
7.386601	446.934900	9.691162
7.942370	447.176048	9.696179
7.656834	444.008228	9.701197
7.625344	435.173852	9.706215
7.793848	424.948006	9.711232
7.429007	427.974781	9.716250
7.545214	437.572252	9.721267
7.609257	452.810969	9.726285
7.850895	453.445316	9.731303
7.750092	452.438662	9.736320
7.745563	437.203295	9.741338
7.569846	432.109025	9.746355
7.654969	444.362223	9.751373
7.908419	453.483767	9.756391
7.690191	446.499530	9.761408
7.861852	452.651677	9.766426
7.518369	438.649678	9.771443
7.447269	453.161650	9.776461
7.449582	458.494583	9.781479
7.771785	458.980609	9.786496
7.634077	454.931252	9.791514
7.928199	459.988093	9.796531
7.609754	460.987903	9.801549
7.678065	469.832353	9.806567
7.790927	460.858583	9.811584
7.747843	459.798705	9.816602
7.679466	462.226773	9.821619
7.480627	457.565305	9.826637
7.578755	466.714347	9.831655
7.567326	455.005056	9.836672
7.339303	461.188271	9.841690
7.478474	476.020764	9.846707
7.734300	474.822534	9.851725
7.832371	490.721822	9.856743
7.757441	478.858364	9.861760
7.894501	483.996624	9.866778
7.702968	485.702382	9.871795
7.693266	482.740644	9.876813
7.596854	482.156176	9.881831
7.968814	483.527494	9.886848
7.687280	487.983420	9.891866
7.769391	489.564253	9.896883
7.744511	485.705493	9.901901
7.535588	480.660593	9.906919
7.754848	492.226937	9.911936
7.845937	505.394420	9.916954
8.255411	508.161033	9.921971
8.044746	499.749172	9.926989
7.969827	499.634704	9.932007
8.163293	494.930695	9.937024
7.850334	491.164407	9.942042
8.055576	487.954398	9.947059
7.756169	491.551595	9.952077
8.086914	486.084469	9.957095
8.367270	493.201049	9.962112
8.273859	491.110800	9.967130
8.428805	489.805299	9.972147
8.017372	485.186601	9.977165
7.706661	484.203366	9.982183
8.085866	486.712788	9.987200
8.028463	485.604659	9.992218
8.118879	487.057959	9.997235
8.129943	487.305558	10.002253
7.692058	494.061305	10.007271
8.111504	479.239153	10.012288
8.119105	493.047710	10.017306
8.576806	488.415910	10.022323
8.063344	489.623001	10.027341
8.058542	483.283803	10.032359
8.208480	483.004718	10.037376
8.198109	481.810326	10.042394
8.096670	482.075552	10.047411
8.479487	487.206866	10.052429
8.001873	488.862773	10.057447
8.140055	479.342232	10.062464
7.925147	484.769168	10.067482
8.241791	488.238283	10.072499
8.468124	486.517656	10.077517
8.265029	488.010632	10.082535
8.338143	486.822094	10.087552
8.602964	490.542325	10.092570
8.264126	487.155632	10.097587
8.607768	486.082497	10.102605
8.334461	484.143510	10.107623
8.599840	479.683856	10.112640
8.463291	488.301638	10.117658
8.379517	481.065948	10.122675
8.501644	479.894977	10.127693
8.093532	475.269449	10.132711
8.162124	471.348711	10.137728
8.206447	482.144043	10.142746
8.027285	483.510193	10.147763
7.982365	482.482159	10.152781
8.087896	484.318096	10.157799
8.196680	479.220263	10.162816
8.247937	487.063853	10.167834
8.167063	492.223638	10.172851
8.097809	486.775003	10.177869
8.253426	485.412593	10.182887
8.059924	483.776681	10.187904
8.057977	488.425486	10.192922
7.822998	488.825243	10.197939
8.473033	509.040389	10.202957
8.139989	516.758013	10.207975
8.402639	519.254143	10.212992
8.449249	517.126174	10.218010
8.584590	518.641865	10.223027
8.716641	508.538447	10.228045
8.221032	508.505672	10.233063
8.509862	516.441439	10.238080
8.274985	519.419464	10.243098
8.317132	520.438518	10.248115
8.261645	513.570767	10.253133
8.463299	517.108398	10.258151
8.364415	513.333811	10.263168
8.347420	518.108056	10.268186
8.301315	513.242763	10.273203
8.155722	507.837640	10.278221
8.312629	513.102187	10.283239
8.537841	506.130498	10.288256
8.449739	506.908028	10.293274
8.642983	515.922273	10.298291
8.647717	511.061638	10.303309
8.328386	515.757022	10.308327
8.316003	519.012609	10.313344
8.291761	511.736021	10.318362
8.809365	527.086773	10.323379
8.691941	526.783306	10.328397
8.330903	521.986289	10.333415
8.995284	517.366280	10.338432
8.557764	516.753205	10.343450
8.251527	519.878110	10.348467
8.674414	523.649321	10.353485
8.659061	536.271773	10.358503
8.922562	537.495987	10.363520
8.859638	515.746675	10.368538
8.312109	511.660531	10.373555
8.420970	520.965709	10.378573
8.756002	530.689890	10.383591
8.652199	532.044237	10.388608
8.708874	547.675507	10.393626
8.753127	545.339621	10.398643
8.890801	535.980075	10.403661
9.021366	523.712006	10.408679
8.324220	509.528679	10.413696
9.103541	517.999820	10.418714
8.592163	521.030635	10.423731
8.666470	509.320498	10.428749
8.680720	512.616092	10.433767
8.649370	518.269897	10.438784
8.971727	528.299019	10.443802
8.896144	525.016238	10.448819
9.005871	513.751827	10.453837
8.586057	514.761211	10.458855
8.584942	519.671824	10.463872
8.658326	525.006265	10.468890
8.918558	528.058195	10.473907
9.168889	529.505377	10.478925
8.798949	524.315280	10.483943
9.187710	516.705738	10.488960
9.167742	507.945260	10.493978
8.534580	516.498855	10.498995
8.786520	503.381809	10.504013
8.996711	511.254157	10.509031
8.910665	511.772590	10.514048
9.041363	512.512684	10.519066
8.837355	509.622411	10.524083
8.799120	503.787060	10.529101
8.509871	509.115198	10.534119
8.556449	522.037204	10.539136
8.791609	527.280027	10.544154
8.486810	530.313190	10.549171
8.916102	535.617116	10.554189
9.021909	535.190310	10.559207
8.908290	539.692523	10.564224
8.847697	535.757298	10.569242
8.860213	541.022386	10.574259
8.993833	528.425632	10.579277
9.227157	533.703458	10.584295
9.049153	539.815747	10.589312
8.999741	526.578644	10.594330
8.900730	532.047395	10.599347
9.301295	529.302234	10.604365
9.307596	536.294514	10.609383
9.406005	532.466920	10.614400
9.439914	534.976801	10.619418
8.805322	537.610359	10.624435
8.686767	529.720538	10.629453
9.049321	531.497274	10.634471
8.997233	533.029710	10.639488
9.199447	530.097877	10.644506
8.913907	542.134664	10.649523
8.778307	539.435639	10.654541
9.253751	540.850707	10.659559
9.094415	531.891148	10.664576
9.288350	532.671827	10.669594
8.875990	534.399565	10.674611
8.922635	523.851930	10.679629
8.692724	532.951419	10.684647
8.525062	540.431703	10.689664
8.916124	557.762057	10.694682
9.051093	553.811966	10.699699
9.195836	569.704012	10.704717
9.589885	563.081388	10.709735
9.331962	565.908397	10.714752
9.626709	561.371537	10.719770
9.531384	562.036593	10.724787
9.038972	542.118633	10.729805
9.267280	554.646117	10.734823
9.566916	563.022024	10.739840
9.388260	538.756708	10.744858
9.142233	538.984629	10.749875
9.267242	528.412090	10.754893
9.010669	534.318938	10.759911
8.953724	554.130510	10.764928
9.506271	554.615162	10.769946
9.365227	556.808476	10.774963
9.553626	558.388441	10.779981
9.476009	561.742619	10.784999
9.320030	561.053873	10.790016
9.265998	549.777228	10.795034
8.969051	564.719151	10.800051
9.673630	556.987526	10.805069
9.793585	561.232242	10.810087
9.504427	549.891451	10.815104
9.488235	540.215184	10.820122
9.095522	538.610480	10.825139
9.259345	550.381206	10.830157
9.568658	557.171384	10.835175
9.678694	557.491839	10.840192
9.918409	547.633462	10.845210
9.304022	543.463112	10.850227
9.555473	538.390245	10.855245
9.529858	533.218780	10.860263
9.399102	535.814421	10.865280
9.378329	539.582566	10.870298
9.569715	537.542363	10.875315
9.403677	532.351874	10.880333
9.617251	542.666290	10.885351
9.471397	552.765629	10.890368
9.439081	543.012993	10.895386
9.433911	555.820055	10.900403
9.704613	549.494473	10.905421
9.632279	560.693138	10.910439
9.218664	563.216337	10.915456
9.497514	556.005852	10.920474
9.264655	567.362216	10.925491
9.527208	569.413401	10.930509
9.848240	569.464112	10.935527
9.867486	573.898179	10.940544
10.117140	567.926182	10.945562
9.490700	565.382953	10.950579
9.895428	565.874987	10.955597
9.877708	562.037180	10.960615
9.466747	557.538309	10.965632
9.685175	550.864311	10.970650
9.680893	557.186072	10.975667
9.649398	559.706204	10.980685
9.878796	556.568137	10.985703
9.361941	567.337838	10.990720
9.755369	563.883735	10.995738
9.558600	566.423452	11.000755
9.591861	565.733457	11.005773
10.027557	571.295167	11.010791
9.838766	577.358666	11.015808
10.006338	563.008254	11.020826
10.049191	569.679239	11.025843
9.670572	549.945412	11.030861
10.080796	549.294185	11.035879
9.587556	551.151362	11.040896
9.773029	544.883316	11.045914
9.781880	571.605263	11.050931
9.767562	559.893200	11.055949
9.850964	566.172824	11.060967
9.616718	570.239509	11.065984
10.079378	559.121743	11.071002
10.178506	574.194121	11.076019
9.834359	564.080076	11.081037
9.902499	567.272563	11.086055
9.700554	567.749197	11.091072
9.988559	565.993654	11.096090
9.549119	567.716171	11.101107
9.965260	562.721635	11.106125
9.863607	568.550572	11.111143
9.698288	570.271165	11.116160
9.783950	567.963502	11.121178
9.876509	564.275673	11.126195
9.432913	574.311221	11.131213
9.442644	567.164988	11.136231
9.759868	571.618639	11.141248
9.855151	567.195081	11.146266
9.317768	583.913538	11.151283
9.219006	596.164093	11.156301
9.919630	584.570370	11.161319
10.110307	593.367306	11.166336
10.280610	593.249130	11.171354
10.084489	582.932001	11.176371
9.951443	589.681047	11.181389
10.163741	580.284539	11.186407
9.852744	595.064587	11.191424
9.961508	585.728479	11.196442
10.368889	594.188505	11.201459
10.180918	590.689792	11.206477
10.222111	585.911787	11.211495
10.144197	583.651841	11.216512
10.294876	592.811649	11.221530
10.084684	590.297873	11.226547
10.224635	589.231400	11.231565
10.406180	585.681103	11.236583
9.766862	593.052271	11.241600
10.207963	588.874327	11.246618
10.160832	594.192957	11.251635
10.210088	597.905960	11.256653
10.196847	586.395683	11.261671
10.024748	595.038020	11.266688
10.059748	592.583657	11.271706
10.075845	587.475068	11.276723
9.780372	597.111881	11.281741
10.002152	601.290160	11.286759
10.025229	618.826552	11.291776
10.431049	615.638742	11.296794
10.300598	615.482482	11.301811
10.223571	616.371891	11.306829
10.659629	614.148177	11.311847
10.378105	624.571771	11.316864
10.375960	614.202141	11.321882
10.774092	617.185143	11.326899
10.953939	618.958957	11.331917
10.601023	598.552017	11.336935
10.817571	603.775688	11.341952
10.490325	587.688196	11.346970
10.500496	589.722122	11.351987
10.358977	593.291445	11.357005
10.343787	584.609076	11.362023
10.146006	595.593889	11.367040
9.912288	581.905939	11.372058
10.296309	586.992912	11.377075
10.332536	609.914195	11.382093
10.665823	610.717225	11.387111
10.400551	611.970644	11.392128
10.517796	610.932974	11.397146
10.251698	613.622415	11.402163
10.326597	619.139684	11.407181
10.553959	616.008237	11.412199
10.585246	619.266467	11.417216
10.709801	611.316429	11.422234
10.781316	614.394786	11.427251
10.504003	618.537658	11.432269
10.660637	618.355351	11.437287
10.829504	619.398738	11.442304
10.647413	606.709384	11.447322
10.863776	582.975409	11.452339
10.222595	591.713331	11.457357
10.725628	593.401792	11.462375
10.487143	586.035666	11.467392
10.762493	587.756644	11.472410
10.552759	590.749676	11.477427
10.486297	609.685487	11.482445
10.922419	603.908324	11.487463
11.214960	602.716956	11.492480
10.802469	595.920888	11.497498
10.732630	589.926358	11.502515
10.500358	582.978981	11.507533
10.782154	583.796389	11.512551
10.701097	588.249331	11.517568
10.762972	585.563540	11.522586
10.873162	584.934075	11.527603
10.659400	590.203073	11.532621
10.970165	587.030161	11.537639
10.489208	597.071576	11.542656
10.835390	587.284858	11.547674
10.799013	585.012093	11.552691
10.404007	588.201410	11.557709
10.657998	594.536366	11.562727
10.676597	606.686490	11.567744
10.680888	616.626640	11.572762
10.813988	604.430702	11.577779
10.556861	618.934086	11.582797
10.964295	602.245475	11.587815
10.720547	611.397664	11.592832
10.753474	602.171260	11.597850
10.913181	610.401856	11.602867
10.508552	612.929966	11.607885
10.941453	612.309898	11.612903
10.965768	618.166451	11.617920
10.667345	615.290954	11.622938
11.171862	609.944887	11.627955
10.695651	617.558753	11.632973
10.447414	614.924702	11.637991
10.845251	629.416992	11.643008
10.661095	627.066390	11.648026
11.165846	635.596386	11.653043
11.197170	641.991494	11.658061
10.724928	637.385439	11.663079
11.123359	638.272938	11.668096
11.125656	639.143608	11.673114
11.346469	634.340603	11.678131
10.749367	644.400242	11.683149
11.305974	633.135166	11.688167
11.111052	637.116810	11.693184
11.309441	637.129933	11.698202
11.087656	632.326847	11.703219
11.185653	632.535581	11.708237
11.559298	632.047873	11.713255
10.971979	622.969132	11.718272
10.823619	618.384920	11.723290
11.285090	626.776526	11.728307
11.245694	632.251746	11.733325
11.556262	626.693064	11.738343
10.852062	622.530456	11.743360
11.103550	625.949847	11.748378
11.323951	626.038417	11.753395
11.172898	636.902324	11.758413
11.193853	634.279742	11.763431
11.036228	628.529328	11.768448
11.332623	631.619791	11.773466
11.316092	632.682760	11.778483
11.205446	639.156915	11.783501
10.977853	636.336589	11.788519
11.143736	632.643569	11.793536
11.115415	636.949405	11.798554
11.523019	627.200379	11.803571
11.192216	639.203297	11.808589
11.096830	634.209992	11.813607
11.505645	635.739650	11.818624
11.474581	637.609628	11.823642
11.602401	624.199516	11.828659
11.610537	633.728818	11.833677
11.300005	637.513980	11.838695
11.315323	637.173934	11.843712
11.440833	629.668707	11.848730
11.407686	629.497201	11.853747
11.019477	632.578163	11.858765
11.345613	634.414265	11.863783
10.946423	635.480385	11.868800
10.965012	633.309454	11.873818
11.403611	640.991437	11.878835
11.198659	661.820400	11.883853
11.675350	651.546138	11.888871
11.706086	651.626555	11.893888
11.306760	658.956992	11.898906
11.121498	653.892557	11.903923
11.330927	652.591131	11.908941
11.676694	655.626526	11.913959
12.124328	652.520520	11.918976
11.632043	666.587415	11.923994
12.164099	654.764437	11.929011
11.662698	662.445385	11.934029
11.596808	661.609976	11.939047
11.958625	650.315449	11.944064
11.692927	652.843887	11.949082
11.805810	631.846374	11.954099
11.528451	633.294192	11.959117
11.669087	628.289156	11.964135
11.604466	639.259443	11.969152
11.770613	657.732826	11.974170
11.638721	647.184689	11.979187
11.818063	650.397637	11.984205
11.704599	650.734178	11.989223
11.932766	653.059004	11.994240
11.399853	653.120436	11.999258
12.067779	655.988589	12.004275
11.766583	658.655134	12.009293
11.768292	661.343648	12.014311
11.710449	667.105793	12.019328
11.860533	668.038516	12.024346
11.929826	658.866346	12.029363
12.044951	656.503562	12.034381
11.747708	660.898875	12.039399
11.604309	657.522553	12.044416
11.545894	668.283602	12.049434
11.946114	663.884827	12.054451
12.135345	663.164080	12.059469
11.800952	663.292238	12.064487
11.958571	652.793411	12.069504
11.772141	665.477473	12.074522
11.758404	645.752642	12.079539
11.706153	657.244868	12.084557
11.558124	656.920947	12.089575
11.882405	665.252015	12.094592
11.644576	656.358341	12.099610
11.963458	654.506432	12.104627
11.930451	656.196836	12.109645
11.887285	652.514475	12.114663
12.515275	663.758113	12.119680
11.831070	663.268890	12.124698
11.981973	656.356123	12.129715
11.993359	668.804066	12.134733
12.022194	661.339219	12.139751
11.879175	666.196366	12.144768
11.699629	660.402039	12.149786
11.943964	673.848595	12.154803
12.165479	684.556327	12.159821
12.250881	685.552834	12.164839
12.338205	689.341943	12.169856
12.387811	683.792573	12.174874
12.262865	679.902113	12.179891
12.314740	671.313336	12.184909
12.072347	669.833391	12.189927
12.173378	653.915422	12.194944
12.169576	669.764559	12.199962
12.578118	682.762514	12.204979
12.092552	665.835061	12.209997
11.936849	662.022008	12.215015
12.530238	673.747602	12.220032
12.177452	683.901528	12.225050
12.154573	681.175352	12.230067
12.431057	680.633439	12.235085
12.105189	685.118450	12.240103
12.290790	685.663755	12.245120
12.466345	690.029179	12.250138
12.183423	688.473531	12.255155
12.333460	690.570762	12.260173
12.368255	682.959804	12.265191
12.643642	679.902873	12.270208
12.630808	686.629965	12.275226
12.904223	678.741780	12.280243
12.542832	670.138859	12.285261
12.283425	660.084066	12.290279
12.126360	652.143420	12.295296
12.155813	669.558943	12.300314
12.482457	670.811143	12.305331
12.193569	675.192527	12.310349
12.125314	684.225739	12.315367
12.509436	672.848807	12.320384
12.583126	683.996268	12.325402
12.509553	679.476062	12.330419
12.192202	684.265854	12.335437
12.294560	681.961871	12.340455
12.665497	680.474192	12.345472
12.302559	684.384340	12.350490
12.455545	676.088989	12.355507
12.489278	687.728709	12.360525
12.508940	685.980485	12.365543
12.674725	682.271691	12.370560
12.517114	683.344144	12.375578
12.532540	682.360292	12.380595
12.884471	685.700841	12.385613
12.642624	691.476044	12.390631
12.595212	684.512287	12.395648
12.715357	685.168834	12.400666
13.113386	685.586181	12.405683
13.052799	686.775977	12.410701
12.536943	687.181877	12.415719
12.721331	679.020461	12.420736
12.683987	688.099324	12.425754
12.713836	683.316758	12.430771
12.951790	682.127626	12.435789
13.059119	683.155412	12.440807
13.111889	684.336915	12.445824
13.183373	678.705223	12.450842
12.920017	681.255388	12.455859
12.762908	684.319086	12.460877
12.448324	684.431517	12.465895
12.848984	675.516690	12.470912
12.795117	681.249814	12.475930
12.702754	676.202374	12.480947
12.854291	684.077676	12.485965
12.714188	683.313854	12.490983
12.685271	681.961407	12.496000
12.703845	680.462663	12.501018
13.080148	687.936675	12.506035
13.110995	685.653364	12.511053
12.686488	691.321486	12.516071
13.197317	693.914457	12.521088
13.014489	691.472119	12.526106
12.790441	681.342346	12.531123
13.032790	694.483113	12.536141
12.874013	701.311973	12.541159
13.110040	705.901457	12.546176
13.129265	705.027462	12.551194
12.861193	701.383486	12.556211
13.294525	699.056047	12.561229
12.978067	709.122244	12.566247
12.906274	696.974125	12.571264
12.711541	706.566810	12.576282
13.121504	705.593724	12.581299
13.150707	710.237706	12.586317
12.994373	711.107987	12.591335
13.026324	708.758228	12.596352
13.134717	715.579946	12.601370
13.120341	712.975511	12.606387
13.081261	694.056178	12.611405
12.983240	699.682616	12.616423
13.187240	692.758360	12.621440
13.252287	700.000277	12.626458
13.232720	693.862135	12.631475
13.179005	696.720285	12.636493
13.304947	697.558962	12.641511
13.725945	699.777842	12.646528
13.403653	702.671762	12.651546
13.032741	711.610395	12.656563
13.673138	705.539261	12.661581
13.364489	706.837353	12.666599
13.222969	700.771965	12.671616
13.194255	705.863679	12.676634
13.726365	702.289991	12.681651
13.527707	700.680114	12.686669
13.250086	705.428972	12.691687
13.721600	699.311716	12.696704
13.273213	704.996207	12.701722
13.262436	704.398315	12.706739
13.555762	700.360263	12.711757
13.404878	711.953185	12.716775
13.092409	704.194656	12.721792
13.211186	715.723239	12.726810
13.439749	732.886719	12.731827
13.704824	724.554849	12.736845
13.412052	736.271004	12.741863
13.665123	732.892510	12.746880
13.754432	725.004748	12.751898
13.611380	730.994860	12.756915
13.746838	727.145641	12.761933
13.668287	728.082632	12.766951
13.591096	729.726315	12.771968
13.743143	738.510441	12.776986
13.421121	727.591255	12.782003
13.677777	727.532133	12.787021
13.872935	728.233733	12.792039
13.653337	728.255542	12.797056
13.732069	729.319370	12.802074
13.706283	728.982606	12.807091
13.857403	727.633506	12.812109
13.802395	730.722239	12.817127
13.706369	729.575965	12.822144
13.735076	732.001482	12.827162
13.428427	728.227843	12.832179
13.556114	715.300526	12.837197
13.575323	729.656560	12.842215
14.006892	726.792903	12.847232
13.859767	719.734301	12.852250
13.678582	730.915413	12.857267
13.632118	723.124665	12.862285
13.786033	726.461533	12.867303
14.052662	721.013849	12.872320
13.817409	719.163549	12.877338
13.738012	730.357115	12.882355
13.671855	720.208893	12.887373
13.949797	728.528317	12.892391
13.908987	725.271609	12.897408
13.707417	716.855065	12.902426
13.871843	729.780848	12.907443
13.789847	725.407118	12.912461
13.986089	743.847472	12.917479
14.165385	738.381908	12.922496
14.339467	741.415814	12.927514
13.856021	731.585434	12.932531
14.297680	730.591602	12.937549
14.156339	732.516738	12.942567
13.999694	730.796133	12.947584
13.832198	728.086297	12.952602
13.857623	735.577436	12.957619
14.218921	737.101924	12.962637
14.231428	746.239278	12.967655
14.539140	757.959195	12.972672
14.388801	734.421330	12.977690
14.291403	732.593611	12.982707
14.463184	719.463720	12.987725
14.205050	726.768908	12.992743
14.197367	722.550794	12.997760
14.340654	722.096021	13.002778
14.240027	722.657771	13.007795
14.284442	715.288291	13.012813
13.931772	729.484840	13.017831
14.105958	723.963276	13.022848
14.568739	731.890820	13.027866
14.483331	737.550008	13.032883
14.654789	724.426475	13.037901
14.101969	731.746278	13.042919
14.370739	724.587797	13.047936
14.436612	713.693052	13.052954
14.173154	721.156862	13.057971
14.388165	726.466018	13.062989
13.968356	735.147234	13.068007
14.220852	738.058400	13.073024
14.792510	740.812262	13.078042
14.241546	737.783808	13.083059
14.739339	749.543365	13.088077
14.727784	753.070266	13.093095
14.841162	746.927056	13.098112
14.748528	737.496191	13.103130
14.277242	727.963711	13.108147
14.323318	729.474471	13.113165
14.301802	742.861746	13.118183
14.150429	741.086664	13.123200
14.414747	741.976247	13.128218
14.407058	752.757801	13.133235
14.751368	746.300695	13.138253
14.254691	750.727278	13.143271
14.160332	744.105371	13.148288
14.691613	747.761817	13.153306
14.671642	747.783907	13.158323
14.871637	745.234243	13.163341
14.737010	747.858923	13.168359
14.606549	757.350046	13.173376
14.683325	749.912366	13.178394
14.418673	745.204329	13.183411
14.414591	747.057467	13.188429
14.566060	766.846089	13.193447
14.702811	765.549730	13.198464
14.806528	773.590356	13.203482
14.854786	771.380047	13.208499
14.807042	767.218693	13.213517
15.025407	766.464974	13.218535
14.600622	772.893722	13.223552
14.869877	771.188434	13.228570
14.677785	772.285229	13.233587
14.761776	771.609369	13.238605
14.922643	768.321055	13.243623
14.819737	769.801512	13.248640
15.006785	770.453892	13.253658
14.709311	764.810553	13.258675
14.967686	771.378417	13.263693
14.788989	767.521607	13.268711
15.261102	766.636612	13.273728
15.002690	761.220685	13.278746
14.908834	773.287555	13.283763
15.055600	767.587234	13.288781
15.175326	770.156287	13.293799
14.724230	767.980035	13.298816
15.080202	767.315210	13.303834
14.988795	774.483840	13.308851
15.027861	769.892313	13.313869
15.121653	773.377466	13.318887
15.085509	775.560683	13.323904
15.197693	769.878404	13.328922
15.072703	779.346590	13.333939
15.142866	788.130946	13.338957
15.296396	796.091193	13.343975
15.451495	790.424274	13.348992
15.544767	777.183565	13.354010
15.494279	778.081447	13.359027
15.341816	779.342449	13.364045
15.253363	769.469094	13.369063
15.024334	769.511316	13.374080
15.270257	760.952053	13.379098
15.486645	767.791585	13.384115
15.339141	763.844680	13.389133
15.530191	768.696851	13.394151
15.202320	773.109613	13.399168
15.037470	760.395357	13.404186
15.435186	782.427083	13.409203
15.449137	784.394166	13.414221
15.886242	785.023147	13.419239
15.383904	778.929058	13.424256
15.518454	768.976582	13.429274
15.271909	776.434609	13.434291
15.051200	768.399740	13.439309
15.618108	776.162665	13.444327
15.552855	791.178929	13.449344
15.828192	783.306177	13.454362
15.705371	779.872958	13.459379
15.095081	774.108213	13.464397
15.594200	776.371668	13.469415
15.334048	784.283116	13.474432
15.814944	783.601873	13.479450
15.521800	788.135432	13.484467
15.537297	778.018566	13.489485
15.946023	792.162141	13.494503
15.806451	794.614032	13.499520
16.095081	780.493789	13.504538
15.601947	778.898485	13.509555
15.716943	772.303727	13.514573
15.868174	781.438299	13.519591
15.771750	773.377643	13.524608
15.422230	763.286418	13.529626
15.702379	782.398481	13.534643
15.852255	788.677235	13.539661
16.126732	786.807025	13.544679
16.129838	786.273227	13.549696
16.061487	768.948943	13.554714
15.860072	773.704814	13.559731
15.621889	770.646282	13.564749
15.698165	762.066262	13.569767
15.657168	779.306736	13.574784
15.843631	788.836583	13.579802
16.008549	793.077465	13.584819
15.928909	795.333772	13.589837
15.654046	796.702316	13.594855
16.076539	798.296118	13.599872
16.334559	786.740055	13.604890
15.946419	795.230144	13.609907
16.072053	792.404942	13.614925
16.171145	789.574432	13.619943
16.016816	788.784431	13.624960
16.216945	799.028519	13.629978
16.252717	790.536883	13.634995
16.181656	794.688505	13.640013
16.114136	788.548377	13.645031
16.093375	791.647534	13.650048
15.984093	788.537244	13.655066
16.099574	788.465527	13.660083
15.976749	791.889949	13.665101
16.141697	791.788390	13.670119
16.051359	805.593598	13.675136
16.064135	788.717338	13.680154
16.014310	787.219834	13.685171
15.922182	793.687988	13.690189
16.274662	788.665494	13.695207
16.093987	795.182235	13.700224
16.092256	789.337916	13.705242
16.138097	789.179278	13.710259
16.103679	795.830897	13.715277
16.307676	805.616785	13.720295
16.672417	822.743236	13.725312
16.283277	810.752060	13.730330
16.230399	808.510254	13.735347
16.555641	818.788399	13.740365
16.384883	816.176893	13.745383
16.423385	813.355873	13.750400
16.589427	817.274689	13.755418
16.731072	812.828027	13.760435
16.382550	805.232894	13.765453
16.634843	800.207159	13.770471
16.909381	808.495595	13.775488
16.388035	799.523192	13.780506
16.536191	792.973725	13.785523
15.898082	800.881281	13.790541
16.352937	803.262130	13.795559
16.266117	818.168185	13.800576
16.673809	814.471956	13.805594
16.437316	818.734712	13.810611
16.557191	813.515123	13.815629
16.470631	802.637895	13.820647
16.399731	814.817962	13.825664
16.481515	813.634355	13.830682
16.781636	816.995670	13.835699
16.471455	808.286827	13.840717
16.684871	800.736197	13.845735
16.807708	811.427908	13.850752
16.471485	811.133470	13.855770
16.758846	823.958008	13.860787
16.452024	833.366349	13.865805
17.094327	830.570645	13.870823
17.134494	828.058634	13.875840
17.083478	824.446897	13.880858
17.456332	820.213319	13.885875
16.847773	810.333069	13.890893
16.879516	803.047591	13.895911
16.685133	802.727774	13.900928
16.668519	806.097687	13.905946
16.875911	811.878282	13.910963
16.569617	827.295265	13.915981
17.123049	821.771055	13.920999
16.868417	835.122339	13.926016
17.260043	831.450715	13.931034
17.292931	834.077565	13.936051
17.336749	835.610779	13.941069
17.330514	819.933534	13.946087
17.167457	814.549989	13.951104
16.976625	811.193693	13.956122
17.080685	810.416856	13.961139
17.111661	820.078380	13.966157
17.188335	820.552393	13.971175
17.246457	828.802162	13.976192
17.251717	826.314556	13.981210
17.516636	826.866373	13.986227
17.078624	815.851696	13.991245
16.914103	809.114524	13.996263
17.247869	822.256843	14.001280
17.266353	825.861104	14.006298
17.053887	830.022267	14.011315
17.497515	831.956748	14.016333
17.690821	828.019547	14.021351
17.416852	828.021472	14.026368
17.564486	829.153406	14.031386
17.692938	823.263431	14.036403
17.104256	819.442443	14.041421
17.304594	816.854845	14.046439
17.288860	823.386780	14.051456
17.513048	821.480263	14.056474
17.882183	816.764425	14.061491
17.595777	823.872107	14.066509
17.943746	811.393051	14.071527
17.349080	799.415149	14.076544
17.322112	799.299478	14.081562
17.477215	800.266136	14.086579
17.621325	821.289906	14.091597
17.933589	816.210588	14.096615
17.233150	816.683281	14.101632
17.418735	812.987137	14.106650
17.942325	819.412479	14.111667
17.641290	831.158393	14.116685
17.757246	826.712598	14.121703
17.927693	821.182122	14.126720
17.808617	816.678478	14.131738
17.540435	805.533055	14.136755
17.083404	813.289167	14.141773
17.736433	817.090656	14.146791
17.409347	822.708841	14.151808
17.543863	820.746945	14.156826
17.827627	827.711646	14.161843
17.713723	837.055048	14.166861
17.755392	829.398769	14.171879
17.892873	832.425803	14.176896
17.658723	827.933874	14.181914
17.847590	827.093255	14.186931
17.590986	832.826634	14.191949
18.015107	817.258691	14.196967
17.866749	828.930189	14.201984
17.854599	827.654000	14.207002
17.949332	816.628436	14.212019
17.715428	824.703049	14.217037
18.129934	838.855223	14.222055
18.033378	838.548481	14.227072
18.074765	848.583935	14.232090
18.249097	845.987784	14.237107
17.836713	851.578316	14.242125
18.019620	844.676242	14.247143
17.809388	854.858423	14.252160
18.103715	858.252212	14.257178
18.309599	846.713746	14.262195
18.493763	851.857356	14.267213
18.485707	859.088700	14.272231
18.406273	852.798935	14.277248
18.351714	842.355332	14.282266
18.386809	820.019082	14.287283
18.374750	827.121651	14.292301
18.343272	823.396398	14.297319
18.269917	822.716787	14.302336
17.902418	815.604311	14.307354
18.305503	836.757938	14.312371
18.153911	843.121816	14.317389
18.117976	836.964098	14.322407
18.487932	855.443623	14.327424
18.044910	852.088962	14.332442
18.295551	848.871776	14.337459
18.252356	852.738175	14.342477
18.332999	845.489200	14.347495
18.475808	847.066866	14.352512
18.578972	857.288309	14.357530
18.601170	852.181844	14.362547
18.427455	850.340824	14.367565
18.389705	845.672949	14.372583
18.419786	852.415471	14.377600
18.902018	852.718642	14.382618
18.515843	846.776745	14.387635
18.755098	843.214200	14.392653
18.755159	845.559013	14.397671
18.888791	846.652116	14.402688
18.866674	842.186923	14.407706
18.833490	836.950283	14.412723
18.471572	846.932160	14.417741
18.512568	842.122559	14.422759
18.736542	848.140412	14.427776
18.323137	844.209904	14.432794
19.101474	838.461101	14.437811
18.748281	846.835284	14.442829
18.560882	847.956595	14.447847
18.957791	844.429310	14.452864
18.227138	847.305182	14.457882
18.977808	861.351055	14.462899
18.585321	866.319927	14.467917
18.760934	869.726007	14.472935
19.041666	866.702921	14.477952
19.030935	873.290896	14.482970
19.016353	869.168504	14.487987
18.987621	874.080386	14.493005
19.257479	868.398618	14.498023
18.951539	869.185048	14.503040
18.929485	871.015768	14.508058
19.109388	862.204866	14.513075
19.131376	872.502153	14.518093
18.959009	872.033716	14.523111
19.435157	865.666366	14.528128
18.879717	872.207139	14.533146
19.271932	869.289664	14.538163
18.999894	866.924396	14.543181
19.186669	867.917655	14.548199
19.479544	860.304056	14.553216
18.968875	870.426019	14.558234
19.026723	867.021282	14.563251
19.292857	869.857749	14.568269
19.277142	877.421665	14.573287
19.305970	867.832843	14.578304
19.492880	874.121604	14.583322
19.236194	865.458001	14.588339
19.392694	864.060710	14.593357
19.336655	874.774173	14.598375
19.163520	867.277768	14.603392
18.766094	862.214956	14.608410
19.324534	873.021494	14.613427
19.570067	869.533700	14.618445
19.271491	868.434931	14.623463
19.298721	868.036209	14.628480
19.237316	881.347785	14.633498
19.620572	892.282769	14.638515
19.672901	886.000750	14.643533
19.533590	894.991551	14.648551
19.789380	892.398410	14.653568
19.720052	888.587554	14.658586
19.991919	882.100723	14.663603
19.413386	874.664677	14.668621
19.397974	864.069759	14.673639
19.563264	877.632996	14.678656
19.618170	885.248968	14.683674
19.957649	879.054508	14.688691
19.699464	887.729409	14.693709
19.658437	892.826262	14.698727
20.083442	882.348524	14.703744
19.870710	889.391039	14.708762
19.914770	890.655972	14.713779
19.960577	889.711531	14.718797
19.815709	898.040474	14.723815
19.830168	883.578093	14.728832
19.984922	888.884114	14.733850
19.726282	883.269367	14.738867
19.995651	891.413482	14.743885
19.959924	887.193412	14.748903
20.201936	883.043437	14.753920
19.788098	888.536377	14.758938
19.892622	882.123104	14.763955
19.938188	883.586619	14.768973
19.624408	880.997512	14.773991
20.514206	884.402151	14.779008
20.063512	884.608493	14.784026
20.148058	884.541622	14.789043
20.037271	883.580690	14.794061
19.738343	887.679672	14.799079
19.904362	891.222961	14.804096
19.924982	890.557026	14.809114
20.058826	890.157378	14.814131
20.492991	886.624247	14.819149
20.295534	887.734513	14.824167
20.113424	889.836470	14.829184
19.917073	892.590765	14.834202
20.212092	892.036474	14.839219
20.414903	890.076494	14.844237
20.137782	892.092350	14.849255
20.667161	897.658420	14.854272
20.193834	903.097568	14.859290
20.342189	908.357260	14.864307
20.655064	917.693798	14.869325
20.503696	902.840809	14.874343
20.692378	889.531417	14.879360
20.181022	891.388310	14.884378
20.651859	895.221517	14.889395
20.764066	899.133007	14.894413
20.128952	887.536930	14.899431
20.223601	895.736825	14.904448
19.986655	900.255296	14.909466
20.463233	911.658516	14.914483
20.728960	905.251536	14.919501
20.309017	910.963193	14.924519
20.412630	908.728415	14.929536
20.254859	919.098075	14.934554
20.872065	914.497982	14.939571
20.874062	910.401385	14.944589
20.574393	910.628247	14.949607
20.716486	908.504206	14.954624
20.637797	915.920212	14.959642
20.726785	934.800454	14.964659
21.163642	935.091801	14.969677
21.232042	932.420715	14.974695
21.121978	916.096922	14.979712
20.874141	908.356579	14.984730
20.817947	910.602915	14.989747
21.245162	904.489375	14.994765
21.018168	904.086301	14.999783
20.980252	901.460280	15.004800
20.932815	905.674500	15.009818
20.716903	908.157302	15.014835
20.436156	912.073557	15.019853
20.696099	918.947350	15.024871
21.193797	921.510853	15.029888
21.180082	930.213746	15.034906
21.217116	926.477737	15.039923
21.245714	931.693082	15.044941
21.004149	941.163839	15.049959
21.654490	931.528098	15.054976
21.481694	929.557535	15.059994
21.529913	919.722645	15.065011
21.407372	907.800088	15.070029
21.026144	911.220836	15.075047
21.080822	894.675588	15.080064
21.326561	913.689040	15.085082
21.082056	921.547603	15.090099
21.033907	918.408777	15.095117
20.882020	929.853671	15.100135
21.374886	924.742871	15.105152
21.564459	923.356173	15.110170
21.113719	922.792491	15.115187
21.642006	924.767369	15.120205
21.395319	928.640420	15.125223
21.858091	923.562738	15.130240
21.435980	927.182403	15.135258
21.513917	923.635649	15.140275
21.464710	925.609488	15.145293
21.348104	929.004558	15.150311
21.273823	919.898931	15.155328
21.402393	922.340386	15.160346
21.290360	931.150203	15.165363
21.752877	916.945803	15.170381
21.495087	932.105963	15.175399
21.768702	938.614696	15.180416
22.003995	949.191039	15.185434
21.928642	939.230329	15.190451
21.755955	921.840192	15.195469
21.485201	931.457531	15.200487
21.613815	933.813772	15.205504
21.624249	952.021517	15.210522
21.765433	952.144592	15.215539
22.078094	953.348510	15.220557
21.696950	946.752526	15.225575
21.973155	957.713791	15.230592
21.885214	960.085030	15.235610
21.979289	954.661155	15.240627
22.277503	943.228084	15.245645
22.129128	949.790315	15.250663
22.303412	949.437979	15.255680
22.228912	955.111306	15.260698
21.947444	949.332854	15.265715
22.069238	945.634055	15.270733
21.959129	951.448662	15.275751
21.857523	952.676461	15.280768
21.870218	960.153908	15.285786
21.822462	953.231126	15.290803
22.173180	950.468466	15.295821
22.211123	955.833836	15.300839
22.200486	949.388088	15.305856
22.098154	952.922940	15.310874
22.030376	956.714317	15.315891
22.302756	961.197184	15.320909
22.323861	953.780764	15.325927
22.230200	947.038750	15.330944
22.281215	956.873938	15.335962
21.864173	953.351081	15.340979
22.211889	954.880873	15.345997
22.280017	979.514425	15.351015
22.518492	980.518525	15.356032
22.405906	978.869889	15.361050
22.621796	975.803295	15.366067
22.761068	976.112866	15.371085
22.725470	980.839656	15.376103
22.662942	972.416985	15.381120
22.797337	975.842167	15.386138
22.291586	975.040944	15.391155
22.675704	976.773323	15.396173
22.570765	984.237652	15.401191
22.778701	977.811298	15.406208
23.056439	971.364542	15.411226
22.616935	967.163534	15.416243
22.770089	964.542281	15.421261
22.788096	978.093957	15.426279
22.731274	968.748879	15.431296
23.123742	966.841228	15.436314
22.880080	978.789693	15.441331
23.028409	970.832614	15.446349
22.875317	969.057779	15.451367
23.148453	970.532984	15.456384
22.806411	967.295026	15.461402
22.630412	964.236185	15.466419
22.898588	964.497157	15.471437
22.816604	975.075887	15.476455
22.890972	969.247987	15.481472
22.841366	966.453371	15.486490
22.945012	979.139544	15.491507
23.354463	968.957690	15.496525
22.970042	972.334767	15.501543
22.941359	978.218678	15.506560
23.160910	974.895885	15.511578
22.983071	979.796443	15.516595
23.112101	965.265550	15.521613
23.220253	978.575880	15.526631
22.778803	970.985768	15.531648
23.116179	974.786254	15.536666
23.279645	980.658995	15.541683
23.398529	971.860755	15.546701
23.167556	982.409183	15.551719
22.985625	962.953356	15.556736
23.326831	987.783981	15.561754
23.068071	995.887811	15.566771
23.626072	999.461227	15.571789
23.447996	999.482841	15.576807
23.398784	1000.607758	15.581824
23.648684	996.746862	15.586842
23.400619	1000.588586	15.591859
23.776248	995.966361	15.596877
23.628210	1000.351002	15.601895
23.580764	994.949289	15.606912
24.121415	1000.469443	15.611930
23.641966	996.082178	15.616947
23.893689	987.076921	15.621965
23.873073	977.041341	15.626983
23.351250	976.050128	15.632000
23.736030	974.749609	15.637018
23.705550	993.860074	15.642035
23.731550	991.640601	15.647053
23.680662	999.115404	15.652071
23.536378	1000.488751	15.657088
23.817641	986.782920	15.662106
23.818740	998.825597	15.667123
23.909347	988.993495	15.672141
23.897687	986.950340	15.677159
23.918534	984.545479	15.682176
24.241619	980.537417	15.687194
23.939349	987.455141	15.692211
23.887212	988.223901	15.697229
23.573386	987.853365	15.702247
24.004290	988.931460	15.707264
24.088551	984.512682	15.712282
24.149351	990.622424	15.717299
24.023803	988.562398	15.722317
23.998819	990.472487	15.727335
24.105641	994.454270	15.732352
24.358300	989.573596	15.737370
24.047244	989.871672	15.742387
24.024413	983.620330	15.747405
24.070820	992.825084	15.752423
24.345104	987.511823	15.757440
24.319789	990.939940	15.762458
24.513382	1002.712613	15.767475
24.288397	991.004871	15.772493
24.612553	999.844212	15.777511
24.253636	991.385918	15.782528
24.437036	988.649467	15.787546
24.473183	1006.812213	15.792563
24.356585	998.628380	15.797581
24.576773	1002.384116	15.802599
24.347396	1009.309362	15.807616
25.029910	1005.784636	15.812634
24.971479	1003.938160	15.817651
24.669090	988.398688	15.822669
24.387790	979.707327	15.827687
24.549585	981.644956	15.832704
24.837537	978.753267	15.837722
24.551648	983.522429	15.842739
24.393020	993.030714	15.847757
24.362921	1004.314560	15.852775
24.631054	1003.597217	15.857792
24.897107	994.835869	15.862810
24.726900	1005.879730	15.867827
24.762550	1006.410669	15.872845
24.674222	1006.983124	15.877863
24.550406	1008.738283	15.882880
24.522008	1010.412218	15.887898
24.737190	1018.186175	15.892915
24.459349	1018.204486	15.897933
24.538401	1019.280904	15.902951
24.472359	1022.380885	15.907968
24.940353	1025.927382	15.912986
25.057652	1034.003868	15.918003
24.953961	1024.839677	15.923021
24.956666	1027.035773	15.928039
24.810443	1036.781984	15.933056
25.314846	1025.957199	15.938074
24.944267	1017.914139	15.943091
24.612393	1024.520927	15.948109
25.026713	1040.147088	15.953127
25.230682	1048.939011	15.958144
25.727470	1048.207932	15.963162
25.303816	1050.830603	15.968179
25.402469	1044.389788	15.973197
25.319838	1045.343214	15.978215
25.507029	1045.945088	15.983232
25.737502	1040.906925	15.988250
25.546619	1041.277694	15.993267
25.349258	1032.551064	15.998285
25.379328	1022.835729	16.003303
25.148819	1032.235372	16.008320
25.567564	1042.009835	16.013338
25.373476	1046.007218	16.018355
25.604407	1043.051868	16.023373
25.438944	1038.397641	16.028391
25.622781	1040.353915	16.033408
26.039051	1032.386386	16.038426
25.461692	1047.830250	16.043443
25.603677	1039.719496	16.048461
25.640504	1034.257228	16.053479
25.389121	1046.655083	16.058496
25.709264	1038.260790	16.063514
25.520754	1044.804097	16.068531
25.321490	1048.234232	16.073549
25.462360	1042.995507	16.078567
25.612683	1058.672515	16.083584
25.822612	1058.756417	16.088602
25.720662	1082.719307	16.093619
25.899232	1073.372008	16.098637
26.441404	1071.797507	16.103655
25.763310	1075.473087	16.108672
25.772221	1067.610395	16.113690
25.834254	1074.893963	16.118707
25.937890	1066.625099	16.123725
26.246749	1075.873984	16.128743
26.259888	1074.328721	16.133760
26.105582	1066.627305	16.138778
26.437306	1064.189504	16.143795
26.188094	1062.395005	16.148813
26.635459	1075.308267	16.153831
26.453209	1065.689292	16.158848
26.512907	1071.862352	16.163866
26.264056	1065.920957	16.168883
26.225441	1067.688018	16.173901
26.370798	1062.896721	16.178919
25.977385	1067.761649	16.183936
26.242573	1068.228224	16.188954
26.273022	1065.247475	16.193971
26.285370	1069.565978	16.198989
25.927390	1063.938335	16.204007
26.230909	1076.804707	16.209024
26.429673	1085.518566	16.214042
26.420596	1091.793929	16.219059
26.632522	1100.518357	16.224077
26.776308	1082.384181	16.229095
26.568598	1092.001197	16.234112
26.719662	1093.779569	16.239130
26.774679	1085.979075	16.244147
26.518566	1087.496185	16.249165
26.876993	1089.671269	16.254183
26.904032	1086.874093	16.259200
27.063170	1089.632683	16.264218
26.577696	1089.147023	16.269235
26.760997	1092.390990	16.274253
26.762668	1083.166079	16.279271
26.821996	1092.005933	16.284288
26.989190	1081.650526	16.289306
26.883686	1090.027041	16.294323
26.685298	1083.995680	16.299341
26.645307	1078.665358	16.304359
26.597561	1099.766854	16.309376
27.111750	1095.713046	16.314394
27.225258	1110.947730	16.319411
27.144497	1117.363725	16.324429
27.395146	1106.449258	16.329447
27.409012	1118.862411	16.334464
27.284157	1102.354567	16.339482
27.395474	1091.569239	16.344499
27.384752	1093.000564	16.349517
27.336708	1089.861692	16.354535
26.780116	1093.521395	16.359552
27.065718	1104.329795	16.364570
27.360570	1115.906791	16.369587
27.300921	1116.067645	16.374605
27.656437	1112.079721	16.379623
27.675692	1108.579996	16.384640
27.909895	1111.929604	16.389658
28.054743	1109.445336	16.394675
27.478193	1100.778083	16.399693
27.402292	1082.274374	16.404711
27.345134	1098.220616	16.409728
27.548825	1100.508310	16.414746
27.611151	1103.566100	16.419763
27.367378	1114.656270	16.424781
27.631904	1108.741725	16.429799
27.628040	1106.520605	16.434816
28.004568	1104.183080	16.439834
28.060809	1105.496614	16.444851
27.623643	1109.440575	16.449869
27.726995	1109.020453	16.454887
27.903472	1102.150846	16.459904
28.032308	1105.356011	16.464922
27.958267	1098.333146	16.469939
27.472623	1105.888734	16.474957
27.765530	1102.090507	16.479975
28.080903	1108.166714	16.484992
27.752630	1108.416995	16.490010
28.170307	1094.004880	16.495027
27.749044	1106.606123	16.500045
27.787216	1103.381154	16.505063
27.595603	1116.552355	16.510080
28.032910	1124.966920	16.515098
28.207818	1126.375475	16.520115
28.295607	1127.321140	16.525133
28.369035	1128.515214	16.530151
28.505337	1122.355660	16.535168
28.477257	1127.460018	16.540186
28.408598	1123.159843	16.545203
28.269702	1137.730331	16.550221
28.345767	1121.017415	16.555239
28.256776	1134.260916	16.560256
27.993233	1131.364089	16.565274
28.386186	1127.436570	16.570291
28.728860	1130.725004	16.575309
28.638708	1128.305955	16.580327
28.532384	1124.617613	16.585344
28.496078	1121.552637	16.590362
28.708870	1124.479556	16.595379
28.601368	1122.719654	16.600397
28.538167	1114.783030	16.605415
28.997530	1121.695086	16.610432
29.058472	1121.742369	16.615450
28.984147	1122.779707	16.620467
28.914288	1129.014112	16.625485
28.723173	1124.490118	16.630503
29.050557	1120.891619	16.635520
28.688630	1123.362613	16.640538
28.828885	1123.214428	16.645555
28.840252	1130.991965	16.650573
28.933346	1124.113323	16.655591
28.662865	1120.961957	16.660608
28.227443	1128.907329	16.665626
28.854185	1126.483259	16.670643
28.607300	1127.522387	16.675661
28.702951	1136.508054	16.680679
29.132411	1143.708835	16.685696
29.180836	1144.382948	16.690714
29.146891	1153.723455	16.695731
28.954206	1151.910622	16.700749
29.036183	1148.637755	16.705767
29.286900	1153.647945	16.710784
29.014372	1151.806595	16.715802
29.280442	1147.091040	16.720819
29.053349	1156.073634	16.725837
29.202459	1153.844320	16.730855
29.125705	1147.749697	16.735872
29.555474	1164.825263	16.740890
29.364521	1164.255584	16.745907
29.555351	1166.365415	16.750925
29.626426	1163.488742	16.755943
29.852111	1163.112569	16.760960
29.441143	1164.322579	16.765978
29.495678	1163.054853	16.770995
29.455019	1158.204310	16.776013
29.600464	1159.450222	16.781031
30.047566	1157.919012	16.786048
29.974518	1163.680543	16.791066
30.438713	1165.217351	16.796083
29.996811	1157.213806	16.801101
29.861592	1140.663368	16.806119
29.959964	1140.783684	16.811136
29.849202	1136.550064	16.816154
29.927071	1137.213252	16.821171
29.587001	1139.854399	16.826189
29.715630	1134.485018	16.831207
29.831158	1143.110958	16.836224
29.866469	1161.236120	16.841242
30.120515	1166.441459	16.846259
30.208431	1171.846402	16.851277
30.144709	1171.373558	16.856295
30.651135	1164.452231	16.861312
30.308707	1166.241656	16.866330
30.102612	1153.994344	16.871347
30.446085	1159.971489	16.876365
30.021938	1146.858912	16.881383
30.260178	1151.990981	16.886400
30.212610	1168.024148	16.891418
30.256604	1161.718092	16.896435
30.154265	1172.536820	16.901453
30.157056	1165.782767	16.906471
30.598872	1171.400515	16.911488
30.226900	1175.327963	16.916506
30.490823	1166.560553	16.921523
30.469433	1172.629584	16.926541
30.300244	1177.771845	16.931559
30.181597	1165.756984	16.936576
30.190815	1164.988680	16.941594
30.496908	1172.720059	16.946611
30.540640	1179.571021	16.951629
30.432557	1186.250106	16.956647
30.523561	1186.977513	16.961664
30.509239	1187.472104	16.966682
30.394162	1191.867408	16.971699
30.743060	1181.644426	16.976717
30.670521	1187.670981	16.981735
30.977691	1184.258679	16.986752
30.994669	1180.601502	16.991770
31.290766	1177.711661	16.996787
31.277098	1185.890789	17.001805
31.007366	1183.376789	17.006823
31.221604	1185.773299	17.011840
31.414929	1182.252598	17.016858
31.302845	1177.236510	17.021875
31.390246	1192.235505	17.026893
31.130867	1189.139194	17.031911
31.366637	1185.296252	17.036928
31.311153	1185.046186	17.041946
31.469216	1174.546984	17.046963
31.498936	1180.305043	17.051981
31.245551	1181.704965	17.056999
31.827534	1181.894683	17.062016
31.193862	1177.616745	17.067034
31.644777	1185.808293	17.072051
31.442332	1189.807016	17.077069
31.187014	1186.082043	17.082087
31.419683	1178.594512	17.087104
31.258284	1184.426699	17.092122
31.354254	1182.716964	17.097139
31.290176	1183.598061	17.102157
31.421586	1181.873306	17.107175
31.391320	1178.930454	17.112192
31.293821	1189.489651	17.117210
31.450143	1195.960050	17.122227
31.335155	1201.033863	17.127245
31.409022	1207.346765	17.132263
31.571981	1210.821168	17.137280
31.724259	1213.176894	17.142298
31.497349	1203.590090	17.147315
31.589496	1214.236356	17.152333
31.844993	1221.682183	17.157351
31.856502	1224.681682	17.162368
31.735700	1235.601175	17.167386
32.140143	1228.620060	17.172403
32.026279	1225.021245	17.177421
31.513827	1235.645482	17.182439
32.058016	1227.070825	17.187456
31.931503	1232.711362	17.192474
32.256958	1225.060946	17.197491
31.832446	1227.014722	17.202509
32.062506	1234.808535	17.207527
32.043711	1219.628387	17.212544
32.219990	1230.933691	17.217562
32.465907	1242.767755	17.222579
32.723440	1247.644355	17.227597
32.759678	1238.224593	17.232615
32.658963	1227.595485	17.237632
32.489343	1228.887610	17.242650
32.692581	1222.029544	17.247667
32.689557	1226.476730	17.252685
32.894420	1223.219311	17.257703
32.718458	1228.630900	17.262720
32.832603	1233.820307	17.267738
33.068292	1215.586388	17.272755
33.024271	1215.530192	17.277773
32.456308	1222.846253	17.282791
32.596496	1216.411492	17.287808
32.383640	1216.182927	17.292826
32.401472	1211.888114	17.297843
32.786816	1223.839180	17.302861
32.466481	1208.838833	17.307879
32.996392	1223.686470	17.312896
32.807288	1237.397029	17.317914
32.700537	1244.192696	17.322931
32.938261	1240.513543	17.327949
33.106385	1247.149375	17.332967
33.219466	1236.269007	17.337984
33.173170	1244.831985	17.343002
33.104519	1246.720539	17.348019
33.442988	1235.527137	17.353037
33.169183	1244.362454	17.358055
33.030397	1249.714574	17.363072
33.128405	1245.000078	17.368090
33.187044	1234.027251	17.373107
33.236261	1236.758903	17.378125
33.107951	1239.142816	17.383143
33.250578	1241.534773	17.388160
33.198873	1242.287697	17.393178
33.452908	1248.594477	17.398195
33.724874	1252.439987	17.403213
33.555303	1260.482624	17.408231
33.802183	1258.405243	17.413248
33.538869	1255.678780	17.418266
33.745519	1252.490505	17.423283
33.874675	1255.490513	17.428301
33.642345	1246.889181	17.433319
33.853756	1248.096361	17.438336
33.868518	1246.301510	17.443354
33.925155	1251.323200	17.448371
33.771341	1262.749674	17.453389
33.824636	1267.390026	17.458407
33.930648	1267.862610	17.463424
33.799537	1271.136936	17.468442
33.448193	1256.706319	17.473459
33.808768	1263.176299	17.478477
33.457594	1262.322440	17.483495
33.760385	1264.891286	17.488512
33.835689	1268.332094	17.493530
33.908222	1279.243414	17.498547
34.482113	1280.217071	17.503565
34.064870	1284.751262	17.508583
34.112888	1290.951475	17.513600
34.313578	1286.410235	17.518618
34.501553	1285.888484	17.523635
34.576509	1279.962558	17.528653
34.447527	1284.117057	17.533671
34.373353	1276.497673	17.538688
34.916269	1275.409051	17.543706
34.667320	1279.916873	17.548723
34.904534	1266.558571	17.553741
34.763825	1260.123622	17.558759
34.358576	1255.014583	17.563776
34.214264	1246.364747	17.568794
34.373768	1263.391230	17.573811
34.757598	1266.603811	17.578829
34.536255	1273.707788	17.583847
34.820072	1273.978939	17.588864
34.792086	1279.320020	17.593882
34.795010	1278.508515	17.598899
34.878886	1284.718887	17.603917
34.840390	1285.816895	17.608935
34.761184	1278.198298	17.613952
35.000110	1276.188435	17.618970
34.831001	1274.955742	17.623987
34.808825	1280.239107	17.629005
34.566253	1282.700890	17.634023
34.658788	1279.085505	17.639040
35.120947	1290.497541	17.644058
35.523602	1300.593417	17.649075
35.427274	1294.034733	17.654093
34.963828	1294.624942	17.659111
35.290329	1296.454746	17.664128
35.399452	1304.624158	17.669146
35.596280	1299.458646	17.674163
35.769510	1298.241745	17.679181
35.312765	1293.992864	17.684199
35.347286	1286.081880	17.689216
35.327908	1288.767481	17.694234
35.557357	1298.218280	17.699251
35.493900	1291.859582	17.704269
35.426749	1301.880738	17.709287
35.798069	1296.716291	17.714304
35.622049	1302.882179	17.719322
35.380588	1306.757648	17.724339
35.904035	1299.221353	17.729357
35.866804	1298.861124	17.734375
35.699309	1289.687858	17.739392
35.650500	1298.352245	17.744410
35.365691	1304.995944	17.749427
35.979993	1303.302821	17.754445
35.908019	1296.421572	17.759463
35.842336	1285.521843	17.764480
35.716508	1296.211778	17.769498
35.747040	1310.623312	17.774515
35.919926	1314.162454	17.779533
36.045565	1328.054152	17.784551
36.249956	1318.469140	17.789568
36.442861	1330.144303	17.794586
36.219706	1320.957651	17.799603
36.194673	1327.459668	17.804621
36.318184	1326.764972	17.809639
36.358214	1321.538810	17.814656
36.337922	1314.062452	17.819674
36.285505	1328.228211	17.824691
36.492325	1322.351041	17.829709
36.587576	1320.369996	17.834727
36.740537	1316.445322	17.839744
36.465203	1318.909087	17.844762
36.546013	1319.262540	17.849779
36.573447	1309.039357	17.854797
36.702308	1310.063806	17.859815
36.864239	1305.541258	17.864832
37.190298	1304.833764	17.869850
36.746861	1305.436618	17.874867
36.633995	1306.044486	17.879885
36.867789	1317.729015	17.884903
36.866067	1318.502514	17.889920
36.849774	1307.522447	17.894938
36.861202	1316.893801	17.899955
36.772542	1306.559415	17.904973
36.960466	1308.499299	17.909991
36.775535	1313.000255	17.915008
37.179375	1320.091508	17.920026
37.071344	1332.867905	17.925043
37.151871	1338.498128	17.930061
37.110633	1336.301771	17.935079
37.007148	1344.697024	17.940096
37.425277	1333.487924	17.945114
36.933041	1345.402993	17.950131
36.945617	1336.848457	17.955149
37.204945	1336.646899	17.960167
37.139733	1335.296933	17.965184
37.349853	1329.457115	17.970202
37.229411	1335.582748	17.975219
37.482927	1342.937414	17.980237
37.605577	1353.815680	17.985255
37.638905	1358.569641	17.990272
37.771289	1354.903814	17.995290
37.272395	1359.580210	18.000307
37.828662	1355.784851	18.005325
38.073360	1357.652726	18.010343
37.773339	1361.101862	18.015360
37.995250	1351.378383	18.020378
37.695542	1349.490775	18.025395
38.013974	1346.269191	18.030413
37.865099	1347.384497	18.035431
38.145804	1346.822968	18.040448
38.172825	1350.915169	18.045466
37.948991	1355.715733	18.050483
37.916738	1346.467598	18.055501
37.853519	1344.340958	18.060519
37.793021	1350.046932	18.065536
37.803968	1349.246790	18.070554
37.894216	1351.066276	18.075571
38.420105	1359.640650	18.080589
38.372182	1380.019794	18.085607
38.445527	1379.888402	18.090624
38.501485	1363.361455	18.095642
38.581536	1380.864422	18.100659
38.737373	1375.471771	18.105677
38.813747	1379.130193	18.110695
38.752081	1369.829847	18.115712
38.740211	1351.290579	18.120730
38.244846	1346.119890	18.125747
38.908554	1373.024469	18.130765
38.637160	1369.743808	18.135783
38.697410	1377.176108	18.140800
38.820990	1366.713756	18.145818
38.901979	1374.417373	18.150835
39.212652	1367.450896	18.155853
39.166635	1369.244395	18.160871
38.790264	1366.523004	18.165888
38.988069	1365.191790	18.170906
38.480405	1377.765733	18.175923
38.535641	1368.892060	18.180941
38.623031	1368.717440	18.185959
38.822019	1373.369708	18.190976
38.938331	1371.877685	18.195994
38.625404	1395.567923	18.201011
39.219487	1399.861637	18.206029
39.082880	1394.208672	18.211047
38.920734	1401.309736	18.216064
39.270646	1383.521675	18.221082
39.323602	1397.835088	18.226099
39.297504	1399.612845	18.231117
39.464169	1403.395987	18.236135
39.381761	1398.324692	18.241152
39.602731	1381.282703	18.246170
39.537143	1394.598472	18.251187
39.682262	1389.232743	18.256205
39.628742	1402.177381	18.261223
39.950248	1397.525662	18.266240
40.224317	1386.477962	18.271258
39.929826	1393.631318	18.276275
39.788061	1387.802431	18.281293
39.703612	1381.459614	18.286311
39.956169	1380.463818	18.291328
39.834740	1372.501487	18.296346
39.831613	1387.644224	18.301363
40.166560	1403.002261	18.306381
40.787291	1393.405629	18.311399
40.431896	1393.259357	18.316416
40.090886	1381.260254	18.321434
40.015933	1391.680331	18.326451
39.729293	1378.422957	18.331469
39.977048	1390.455656	18.336487
40.262383	1403.763789	18.341504
40.351891	1404.279990	18.346522
40.213688	1404.386880	18.351539
40.407849	1407.562929	18.356557
40.616944	1406.349869	18.361575
40.193090	1406.523605	18.366592
40.581208	1405.250937	18.371610
40.493802	1409.316896	18.376627
40.067528	1404.482520	18.381645
40.468856	1400.768234	18.386663
40.545376	1422.765866	18.391680
40.980191	1420.807351	18.396698
40.849419	1434.313252	18.401715
40.613325	1435.577934	18.406733
41.008699	1428.358311	18.411751
40.973522	1428.382784	18.416768
40.737456	1431.733546	18.421786
40.429861	1432.977871	18.426803
41.042457	1431.303940	18.431821
41.137263	1426.577274	18.436839
40.884553	1423.820720	18.441856
41.242816	1423.379587	18.446874
41.553087	1427.929223	18.451891
41.228568	1428.118956	18.456909
41.502438	1420.255622	18.461927
41.138959	1426.640281	18.466944
40.944232	1428.031031	18.471962
41.331311	1416.848836	18.476979
41.293483	1426.884403	18.481997
41.785509	1433.406438	18.487015
41.611796	1445.009722	18.492032
41.500021	1433.795217	18.497050
41.656750	1440.540209	18.502067
41.777850	1446.817393	18.507085
41.677616	1435.216051	18.512103
41.558524	1447.628172	18.517120
41.767379	1440.046429	18.522138
41.900521	1439.154551	18.527155
42.314015	1441.945931	18.532173
42.262899	1435.096075	18.537191
41.872831	1438.773939	18.542208
42.247565	1436.869019	18.547226
41.928273	1435.382121	18.552243
42.059843	1437.204610	18.557261
42.209905	1433.091007	18.562279
42.071175	1446.452990	18.567296
41.731212	1443.486030	18.572314
42.473569	1442.867949	18.577331
41.845308	1443.114738	18.582349
42.167880	1437.837963	18.587367
41.840890	1440.612809	18.592384
42.020885	1441.935382	18.597402
42.124346	1448.161679	18.602419
42.314630	1449.460549	18.607437
42.361860	1449.749834	18.612455
42.822225	1459.432796	18.617472
42.752904	1462.656449	18.622490
42.646329	1459.454094	18.627507
42.550153	1470.139487	18.632525
42.612929	1461.816879	18.637543
42.689036	1473.507280	18.642560
42.497138	1468.809743	18.647578
42.707564	1465.579812	18.652595
42.606587	1473.021633	18.657613
42.801529	1469.929834	18.662631
42.595847	1475.242007	18.667648
42.796519	1471.180430	18.672666
43.371916	1479.472537	18.677683
43.014752	1493.989146	18.682701
43.173367	1485.402190	18.687719
43.277787	1490.997159	18.692736
43.290212	1490.026357	18.697754
43.326839	1486.255579	18.702771
43.160262	1488.721263	18.707789
43.142142	1485.249412	18.712807
42.846004	1482.629047	18.717824
43.407977	1479.656475	18.722842
43.351383	1491.039458	18.727859
43.320837	1485.227829	18.732877
43.863337	1476.454493	18.737895
43.246240	1492.690798	18.742912
43.374600	1493.014712	18.747930
43.696696	1501.753636	18.752947
43.361690	1504.712794	18.757965
44.076609	1506.311342	18.762983
43.809675	1507.798622	18.768000
43.595211	1514.829030	18.773018
43.738503	1508.412614	18.778035
43.630620	1508.682020	18.783053
44.044379	1508.169072	18.788071
43.766208	1510.718518	18.793088
43.888366	1517.453176	18.798106
43.912160	1525.645526	18.803123
44.353393	1535.489325	18.808141
44.437764	1523.587590	18.813159
44.545638	1530.198252	18.818176
44.675752	1525.731129	18.823194
44.754506	1513.931271	18.828211
44.440055	1506.393618	18.833229
44.803191	1497.932412	18.838247
44.438862	1500.653154	18.843264
44.501177	1506.955349	18.848282
44.625510	1515.333924	18.853299
44.571008	1519.322165	18.858317
45.023748	1522.000106	18.863335
44.498040	1524.383200	18.868352
44.679241	1527.151025	18.873370
44.498943	1522.372756	18.878387
44.666734	1530.122804	18.883405
44.680753	1523.606710	18.888423
44.724376	1527.043064	18.893440
44.617880	1522.609857	18.898458
44.983572	1521.883522	18.903475
44.504011	1528.109669	18.908493
44.963366	1527.191924	18.913511
44.811489	1545.861228	18.918528
45.038592	1546.968134	18.923546
45.529584	1548.724854	18.928563
45.482074	1549.862162	18.933581
45.651416	1543.163927	18.938599
45.474524	1550.197929	18.943616
45.641248	1551.519434	18.948634
45.454684	1544.709694	18.953651
45.368369	1542.308924	18.958669
45.792475	1548.087365	18.963687
45.601462	1554.457671	18.968704
45.233640	1539.751679	18.973722
45.792812	1541.538744	18.978739
45.499225	1540.230855	18.983757
45.451651	1541.923624	18.988775
45.824586	1542.774139	18.993792
45.722438	1547.416826	18.998810
45.933080	1539.052080	19.003827
46.133560	1537.524764	19.008845
45.970662	1545.260354	19.013863
46.160954	1544.410012	19.018880
46.190393	1549.877884	19.023898
46.175499	1539.310888	19.028915
45.906741	1553.005764	19.033933
46.277175	1565.925124	19.038951
46.509721	1570.067230	19.043968
46.307008	1568.789285	19.048986
46.538434	1564.038021	19.054003
46.568375	1570.856579	19.059021
46.415556	1564.215123	19.064039
46.645556	1565.526716	19.069056
46.615387	1565.383137	19.074074
46.793035	1556.206154	19.079091
46.444578	1567.641226	19.084109
46.766012	1560.158565	19.089127
46.621456	1560.329570	19.094144
46.440002	1569.207384	19.099162
46.698932	1558.692154	19.104179
46.361101	1559.796050	19.109197
46.461975	1558.142320	19.114215
46.962443	1576.283391	19.119232
47.102636	1587.203234	19.124250
47.288930	1587.069925	19.129267
46.940969	1590.018502	19.134285
47.067949	1583.257458	19.139303
47.220666	1580.263779	19.144320
47.079363	1589.343608	19.149338
47.494776	1588.322286	19.154355
47.600052	1589.426190	19.159373
47.349786	1585.189072	19.164391
47.274716	1581.921796	19.169408
47.473826	1596.411296	19.174426
47.763703	1581.816831	19.179443
47.585174	1592.335308	19.184461
47.339127	1590.366679	19.189479
47.555796	1586.652884	19.194496
47.583658	1616.043373	19.199514
48.264521	1608.062541	19.204531
47.940713	1612.588486	19.209549
48.013003	1606.868009	19.214567
47.849756	1616.156428	19.219584
47.927995	1609.027448	19.224602
47.820770	1604.764758	19.229619
47.837055	1606.778906	19.234637
47.904044	1613.585364	19.239655
48.080095	1608.890104	19.244672
47.759737	1611.228411	19.249690
48.361600	1604.301433	19.254707
48.038964	1612.264061	19.259725
47.801723	1611.310277	19.264743
48.336990	1621.739029	19.269760
48.350003	1628.156294	19.274778
48.552621	1634.562792	19.279795
48.499473	1639.478708	19.284813
48.593451	1638.129026	19.289831
48.765536	1629.590387	19.294848
48.349953	1631.814221	19.299866
48.651754	1627.632616	19.304883
48.546296	1637.820917	19.309901
48.480191	1633.965213	19.314919
48.538155	1625.633815	19.319936
48.743344	1641.457381	19.324954
48.928166	1652.622752	19.329971
48.977865	1667.675393	19.334989
49.099789	1659.037295	19.340007
49.157360	1657.702783	19.345024
49.127301	1653.055585	19.350042
48.965154	1652.434037	19.355059
49.346376	1653.639887	19.360077
49.175855	1646.212176	19.365095
49.125443	1646.513607	19.370112
49.445457	1649.587926	19.375130
49.358826	1651.883306	19.380147
49.724900	1657.692968	19.385165
49.260281	1648.143167	19.390183
49.406252	1653.933660	19.395200
49.552480	1668.633487	19.400218
49.527962	1667.677931	19.405235
50.012523	1670.114210	19.410253
49.770500	1662.874430	19.415271
50.166733	1671.532390	19.420288
49.682201	1671.614642	19.425306
50.404204	1672.795505	19.430323
50.006061	1671.393528	19.435341
49.798751	1672.451733	19.440359
49.975799	1662.981282	19.445376
49.964954	1672.791840	19.450394
49.609878	1667.479149	19.455411
50.081245	1672.966186	19.460429
49.997430	1678.193050	19.465447
50.175243	1688.176042	19.470464
49.895570	1692.215380	19.475482
50.405360	1691.943018	19.480499
50.541950	1696.371603	19.485517
50.293608	1697.701342	19.490535
50.581565	1692.306831	19.495552
50.532622	1696.521473	19.500570
50.666340	1715.900491	19.505587
50.784110	1720.070082	19.510605
50.987666	1731.027426	19.515623
51.000305	1716.567813	19.520640
50.933430	1721.530086	19.525658
51.022495	1718.233913	19.530675
51.081905	1718.789555	19.535693
51.140434	1719.821892	19.540711
51.324870	1715.062171	19.545728
51.042533	1715.005440	19.550746
51.054466	1714.160943	19.555763
51.376737	1716.581627	19.560781
51.005569	1718.823761	19.565799
51.128801	1713.354060	19.570816
51.428216	1716.737751	19.575834
51.115972	1718.894908	19.580851
51.345298	1724.991120	19.585869
51.578979	1730.300807	19.590887
51.876974	1727.104451	19.595904
51.530718	1737.974360	19.600922
51.891146	1733.884538	19.605939
52.049299	1733.515781	19.610957
51.712820	1737.036976	19.615975
52.023271	1728.413492	19.620992
51.867119	1736.779308	19.626010
51.734140	1736.913784	19.631027
51.859868	1732.661906	19.636045
51.716690	1734.139283	19.641063
52.162841	1727.116726	19.646080
52.170096	1736.485798	19.651098
51.821499	1731.695969	19.656115
52.240938	1736.771414	19.661133
51.820549	1748.164218	19.666151
52.152568	1746.723580	19.671168
52.269251	1757.565155	19.676186
52.431837	1760.963979	19.681203
53.019173	1769.844526	19.686221
52.548722	1760.380791	19.691239
52.689114	1745.430893	19.696256
52.598599	1751.851799	19.701274
52.342565	1755.496102	19.706291
52.834548	1754.453307	19.711309
52.881312	1761.029445	19.716327
53.126057	1754.278289	19.721344
52.701778	1767.666314	19.726362
52.993782	1757.183658	19.731379
53.157583	1754.727892	19.736397
52.909083	1763.859320	19.741415
53.129323	1764.579126	19.746432
53.350070	1785.484719	19.751450
53.461350	1790.217114	19.756467
53.440007	1782.055870	19.761485
53.442971	1781.591497	19.766503
53.470728	1780.577249	19.771520
53.301621	1786.587575	19.776538
53.606346	1780.641264	19.781555
53.763147	1774.629764	19.786573
53.212731	1785.055130	19.791591
53.556641	1774.397064	19.796608
53.401967	1786.871802	19.801626
53.761886	1773.957832	19.806643
53.663520	1783.233016	19.811661
53.610884	1798.043007	19.816679
53.942683	1801.544725	19.821696
53.995982	1798.907436	19.826714
54.051111	1800.104423	19.831731
54.241534	1801.791488	19.836749
53.763103	1804.640613	19.841767
53.977325	1801.552049	19.846784
54.223098	1808.807128	19.851802
54.412195	1814.644569	19.856819
54.924962	1808.015514	19.861837
54.505128	1808.008729	19.866855
54.522736	1795.388233	19.871872
54.442513	1799.850813	19.876890
54.611117	1813.701441	19.881907
54.789673	1818.994543	19.886925
54.693771	1827.622379	19.891943
54.736788	1824.352337	19.896960
55.019595	1826.914929	19.901978
54.643207	1822.025281	19.906995
54.771625	1816.251759	19.912013
54.727779	1824.615801	19.917031
54.968167	1814.807120	19.922048
54.703148	1818.430751	19.927066
54.851921	1821.838064	19.932083
54.956977	1833.883951	19.937101
55.098841	1838.046638	19.942119
55.455327	1846.139670	19.947136
55.664244	1846.813913	19.952154
55.296237	1850.425283	19.957171
55.134814	1847.487090	19.962189
54.993103	1845.382156	19.967207
55.117185	1838.217499	19.972224
55.428882	1839.532092	19.977242
55.492383	1854.604820	19.982259
56.056645	1853.124631	19.987277
55.619632	1861.988977	19.992295
55.680354	1860.350978	19.997312
55.747745	1857.582076	20.002330
56.090400	1860.362530	20.007347
56.279110	1855.201287	20.012365
56.170902	1856.963550	20.017383
56.528802	1849.383531	20.022400
56.452695	1856.745869	20.027418
56.349478	1849.168663	20.032435
56.700877	1853.948668	20.037453
56.696761	1847.731964	20.042471
56.729201	1843.775562	20.047488
56.757349	1847.331175	20.052506
56.642400	1847.585912	20.057523
56.661145	1846.181725	20.062541
56.559096	1847.614795	20.067559
56.718926	1839.617658	20.072576
56.810994	1838.243011	20.077594
56.785053	1847.197591	20.082611
56.878370	1846.321401	20.087629
56.967364	1848.523014	20.092647
56.934120	1846.388462	20.097664
57.246521	1843.088835	20.102682
56.554883	1848.158496	20.107699
56.849033	1849.239137	20.112717
57.221188	1862.186848	20.117735
57.194798	1865.829910	20.122752
57.321043	1877.039315	20.127770
57.076646	1876.455893	20.132787
57.690503	1864.013350	20.137805
57.615891	1869.241983	20.142823
57.752096	1866.743185	20.147840
58.087219	1854.615737	20.152858
57.710866	1867.844838	20.157875
57.537767	1858.492264	20.162893
57.626002	1869.922229	20.167911
57.471188	1870.678709	20.172928
57.614828	1872.366799	20.177946
57.676723	1887.869027	20.182963
57.896172	1892.537161	20.187981
57.783728	1889.922671	20.192999
58.045049	1889.645052	20.198016
58.261213	1888.891634	20.203034
57.990038	1890.471135	20.208051
58.239742	1895.869886	20.213069
58.057938	1907.780872	20.218087
58.351105	1911.689481	20.223104
58.444750	1911.444444	20.228122
58.195164	1925.733091	20.233139
58.298585	1904.221134	20.238157
58.213603	1916.915434	20.243175
58.419154	1917.261979	20.248192
58.671218	1929.931886	20.253210
58.488364	1946.940070	20.258227
58.716395	1942.154523	20.263245
58.825540	1943.456675	20.268263
58.691000	1942.205894	20.273280
58.955435	1947.908489	20.278298
59.145335	1949.579870	20.283315
59.261750	1932.702073	20.288333
59.283990	1939.509354	20.293351
59.130524	1942.493792	20.298368
59.216536	1937.601099	20.303386
59.147766	1958.766865	20.308403
59.611903	1967.411174	20.313421
59.965616	1966.077582	20.318439
59.846031	1964.893890	20.323456
59.908104	1962.911660	20.328474
59.733261	1965.394484	20.333491
60.052751	1956.062521	20.338509
60.020630	1961.959917	20.343527
60.370643	1961.816735	20.348544
60.119988	1951.258030	20.353562
60.138646	1946.814577	20.358579
59.898724	1952.905486	20.363597
60.343797	1955.572072	20.368615
60.367795	1960.791594	20.373632
60.572219	1959.541357	20.378650
60.582113	1964.491670	20.383667
60.539915	1946.859167	20.388685
60.029277	1943.000454	20.393703
60.484851	1946.293446	20.398720
60.603463	1945.577402	20.403738
60.402542	1958.674934	20.408755
60.195674	1954.759157	20.413773
60.365951	1953.924556	20.418791
60.491223	1950.168198	20.423808
60.875757	1964.922457	20.428826
60.750226	1976.486975	20.433843
61.034411	1981.236516	20.438861
61.132626	1984.702277	20.443879
60.642661	1985.318753	20.448896
60.907953	1972.394218	20.453914
60.684170	1971.043799	20.458931
61.028747	1979.419646	20.463949
61.678423	1994.507959	20.468967
61.152428	2006.154175	20.473984
61.364736	2006.909951	20.479002
61.198226	2009.855415	20.484019
61.602478	2006.588709	20.489037
61.856325	2004.140893	20.494055
61.679158	2003.130335	20.499072
61.948284	1996.245871	20.504090
61.695748	2011.500800	20.509107
61.805543	2003.584018	20.514125
61.789049	2005.205684	20.519143
61.627817	2015.794288	20.524160
62.092464	2020.648119	20.529178
61.749778	2023.485478	20.534195
61.769000	2021.768752	20.539213
62.271897	2027.424544	20.544231
62.373878	2025.713788	20.549248
62.459271	2022.061500	20.554266
62.389102	2025.253826	20.559283
62.591157	2040.522770	20.564301
62.932724	2040.365131	20.569319
62.671301	2051.550169	20.574336
63.365903	2046.173900	20.579354
62.980101	2036.952396	20.584371
63.070797	2020.766567	20.589389
63.086859	2013.808127	20.594407
62.755458	2018.054474	20.599424
63.189953	2012.340240	20.604442
62.900631	2013.370285	20.609459
63.037334	2031.508847	20.614477
63.064206	2025.413470	20.619495
63.179671	2040.632860	20.624512
63.488819	2034.436444	20.629530
63.549258	2044.718914	20.634547
63.541042	2040.705717	20.639565
63.626401	2036.693640	20.644583
63.162844	2039.941290	20.649600
63.515324	2031.235331	20.654618
63.455032	2026.450750	20.659635
63.548550	2034.386236	20.664653
63.911756	2042.131138	20.669671
63.565689	2029.239225	20.674688
63.477777	2034.940243	20.679706
63.837866	2059.198153	20.684723
63.619364	2049.205599	20.689741
63.544074	2063.495452	20.694759
63.515750	2059.870441	20.699776
63.993982	2077.390606	20.704794
63.650544	2090.933476	20.709811
64.372015	2087.714893	20.714829
64.613412	2084.691457	20.719847
64.296231	2085.116748	20.724864
64.980761	2085.978439	20.729882
64.594565	2099.808904	20.734899
65.236367	2083.344155	20.739917
64.996389	2079.042185	20.744935
64.786064	2080.315498	20.749952
64.683437	2083.541324	20.754970
65.312242	2093.283455	20.759987
65.245447	2102.146724	20.765005
65.105937	2099.265022	20.770023
64.959778	2099.830791	20.775040
65.298310	2097.612713	20.780058
65.322317	2100.032839	20.785075
65.244206	2095.765471	20.790093
65.469500	2094.114291	20.795111
65.381517	2094.601511	20.800128
65.799387	2088.100841	20.805146
65.896223	2087.905799	20.810163
66.115596	2089.531547	20.815181
66.133358	2089.023819	20.820199
65.824672	2088.087514	20.825216
66.233579	2078.315408	20.830234
65.827804	2090.397317	20.835251
65.962732	2089.606122	20.840269
66.255010	2086.110772	20.845287
66.189206	2093.632552	20.850304
66.139560	2091.320644	20.855322
66.023733	2096.319096	20.860339
66.268210	2105.767969	20.865357
66.340260	2105.037121	20.870375
66.321451	2112.788252	20.875392
66.531270	2111.038501	20.880410
66.443848	2114.258794	20.885427
66.340505	2118.270600	20.890445
66.384511	2114.097713	20.895463
66.463392	2127.968954	20.900480
66.542149	2132.239436	20.905498
66.544875	2129.467999	20.910515
66.279724	2137.178834	20.915533
66.706961	2143.212622	20.920551
66.771500	2171.421058	20.925568
66.822663	2167.922439	20.930586
67.049012	2165.235892	20.935603
66.669138	2183.543913	20.940621
67.802002	2186.699275	20.945639
67.220841	2199.862868	20.950656
67.536778	2201.088454	20.955674
67.536638	2201.694471	20.960691
67.470421	2196.121750	20.965709
68.034753	2189.645439	20.970727
68.046938	2190.656659	20.975744
67.982374	2183.704473	20.980762
68.052298	2193.650997	20.985779
67.801979	2189.893468	20.990797
67.932247	2185.148423	20.995815
68.161959	2188.372696	21.000832
68.175981	2189.134297	21.005850
68.027666	2192.509324	21.010867
67.775723	2213.842957	21.015885
68.436142	2210.059510	21.020903
68.186770	2230.105075	21.025920
68.115547	2220.196658	21.030938
68.272260	2215.668388	21.035955
68.204828	2226.444409	21.040973
68.624031	2245.555190	21.045991
68.629650	2238.071232	21.051008
68.905145	2246.091920	21.056026
68.918781	2239.916485	21.061043
68.930329	2239.845267	21.066061
69.124917	2228.948371	21.071079
69.086882	2240.032248	21.076096
69.123883	2245.587518	21.081114
69.246149	2265.628550	21.086131
69.068963	2274.278804	21.091149
69.539833	2262.653728	21.096167
69.600144	2266.987098	21.101184
70.015919	2264.693776	21.106202
69.453988	2268.079966	21.111219
69.417267	2261.117076	21.116237
69.745170	2259.617078	21.121255
69.699183	2266.261586	21.126272
70.071745	2265.168040	21.131290
70.263579	2285.479087	21.136307
70.405359	2285.766198	21.141325
70.564674	2275.821631	21.146343
70.132275	2260.405573	21.151360
70.599155	2268.970696	21.156378
70.373779	2279.348578	21.161395
70.285643	2278.639664	21.166413
70.794051	2278.885114	21.171431
70.952460	2287.242932	21.176448
70.760963	2278.044514	21.181466
71.142146	2269.135109	21.186483
71.008538	2280.779991	21.191501
71.127635	2275.253958	21.196519
70.986349	2282.554092	21.201536
70.749420	2278.564051	21.206554
70.702968	2270.933588	21.211571
70.658012	2275.087774	21.216589
71.151871	2275.310255	21.221607
71.217396	2273.283265	21.226624
70.999077	2279.825378	21.231642
71.280151	2294.684490	21.236659
71.128394	2306.221768	21.241677
71.526101	2304.739235	21.246695
71.453636	2303.308273	21.251712
71.490093	2297.318609	21.256730
71.669107	2299.159003	21.261747
71.520647	2315.022791	21.266765
71.880415	2312.971790	21.271783
72.201070	2322.976942	21.276800
71.973876	2319.001147	21.281818
71.973342	2315.684186	21.286835
71.978131	2329.986953	21.291853
71.950322	2311.837391	21.296871
72.080557	2318.299660	21.301888
71.967966	2328.382161	21.306906
72.635054	2335.486231	21.311923
72.205019	2346.811489	21.316941
72.564516	2341.020531	21.321959
72.186638	2343.323757	21.326976
72.173914	2344.900677	21.331994
72.738656	2355.404145	21.337011
72.675274	2362.575329	21.342029
72.918371	2367.950010	21.347047
73.156055	2359.738452	21.352064
73.130764	2372.527874	21.357082
73.194937	2374.064343	21.362099
72.990152	2373.664065	21.367117
73.211239	2369.737958	21.372135
73.393402	2368.494337	21.377152
73.306798	2376.925301	21.382170
73.894796	2387.178966	21.387187
73.812694	2384.035734	21.392205
73.683143	2384.134959	21.397223
74.037304	2389.236600	21.402240
73.754857	2388.476066	21.407258
74.129821	2378.526062	21.412275
73.932053	2390.856477	21.417293
74.260284	2393.213199	21.422311
74.205807	2378.075533	21.427328
73.829908	2384.980078	21.432346
74.360049	2383.962832	21.437363
74.020170	2387.995977	21.442381
74.559686	2391.787192	21.447399
74.509526	2402.920411	21.452416
74.606639	2404.533782	21.457434
74.431811	2394.540506	21.462451
74.427410	2405.167890	21.467469
74.507725	2406.970104	21.472487
74.934845	2392.501818	21.477504
75.000533	2416.919957	21.482522
75.259976	2423.014846	21.487539
75.215733	2422.529448	21.492557
75.451276	2422.246392	21.497575
75.317036	2425.082715	21.502592
75.238166	2424.681645	21.507610
75.543700	2416.544647	21.512627
75.400247	2417.678104	21.517645
75.793940	2419.529062	21.522663
75.792236	2423.263053	21.527680
75.646753	2423.746667	21.532698
75.512198	2419.718462	21.537715
75.723532	2423.097151	21.542733
75.688580	2438.078485	21.547751
76.037499	2437.395775	21.552768
75.897365	2449.452085	21.557786
76.312144	2445.536644	21.562803
76.348589	2442.999742	21.567821
76.253369	2443.175649	21.572839
76.306738	2439.124309	21.577856
75.867239	2449.873542	21.582874
75.995707	2465.870819	21.587891
76.132779	2471.085399	21.592909
76.682828	2474.379469	21.597927
77.067816	2462.168055	21.602944
76.616881	2472.657133	21.607962
76.718354	2470.050073	21.612979
77.258386	2486.314282	21.617997
77.367184	2487.474502	21.623015
77.446452	2478.097846	21.628032
77.373658	2477.534859	21.633050
77.582404	2484.594022	21.638067
77.673320	2490.895238	21.643085
77.843529	2477.379260	21.648103
77.786974	2479.673190	21.653120
78.120122	2474.135654	21.658138
77.804369	2467.591980	21.663155
77.709798	2463.898364	21.668173
77.463886	2474.431069	21.673191
77.948278	2472.849726	21.678208
77.547870	2475.648855	21.683226
77.984134	2480.381015	21.688243
77.872725	2482.096498	21.693261
78.121191	2483.812409	21.698279
78.062725	2485.860460	21.703296
78.021586	2498.008601	21.708314
78.062849	2498.469271	21.713331
78.474889	2503.255730	21.718349
78.161560	2514.562808	21.723367
78.411433	2519.033815	21.728384
78.559829	2536.937502	21.733402
78.721705	2538.162000	21.738419
78.764681	2530.700473	21.743437
78.690660	2535.802961	21.748455
78.826304	2532.313129	21.753472
79.066601	2557.650946	21.758490
79.121306	2559.924298	21.763507
79.096189	2569.153693	21.768525
78.957726	2563.942510	21.773543
79.372146	2558.190222	21.778560
79.405271	2586.277984	21.783578
79.709883	2582.995225	21.788595
79.451480	2589.808847	21.793613
79.706635	2576.222676	21.798631
80.009203	2588.380152	21.803648
79.617479	2583.653660	21.808666
80.112953	2593.325427	21.813683
80.142663	2590.767466	21.818701
80.338389	2601.388861	21.823719
80.315754	2599.441926	21.828736
80.086114	2602.908675	21.833754
80.334318	2606.224812	21.838771
80.442488	2611.428179	21.843789
80.409106	2621.555246	21.848807
80.949711	2621.704129	21.853824
80.550789	2629.871682	21.858842
80.951856	2630.058209	21.863859
80.922637	2634.642407	21.868877
81.235202	2636.446131	21.873895
81.313913	2636.537978	21.878912
81.225627	2646.395917	21.883930
81.111321	2635.057967	21.888947
81.678776	2639.760147	21.893965
81.084669	2643.826865	21.898983
80.990299	2633.947097	21.904000
81.188914	2653.995536	21.909018
81.439943	2651.450235	21.914035
81.557509	2663.775618	21.919053
81.773416	2666.159443	21.924071
81.663441	2664.147282	21.929088
81.997408	2687.608466	21.934106
82.166562	2684.346912	21.939123
82.123837	2687.459306	21.944141
82.326305	2681.601314	21.949159
82.367425	2672.713428	21.954176
82.069166	2677.639624	21.959194
81.971726	2680.536502	21.964211
82.215654	2686.627599	21.969229
82.671642	2706.544245	21.974247
82.758403	2698.031094	21.979264
82.793097	2703.495338	21.984282
83.146702	2696.035573	21.989299
83.086667	2696.720426	21.994317
82.783509	2701.375966	21.999335
82.921239	2688.366751	22.004352
82.996209	2696.583179	22.009370
82.967522	2699.459819	22.014387
83.172232	2719.529470	22.019405
83.061949	2727.339383	22.024423
83.689351	2723.519975	22.029440
83.683783	2725.130525	22.034458
83.854093	2716.134004	22.039475
83.948196	2715.210307	22.044493
83.554926	2708.634504	22.049511
84.032635	2724.305864	22.054528
83.936683	2739.214945	22.059546
84.016196	2738.132567	22.064563
84.391237	2739.418368	22.069581
84.308456	2743.619619	22.074599
84.719761	2742.191733	22.079616
84.777628	2739.430500	22.084634
84.560436	2739.404586	22.089651
84.818318	2730.230217	22.094669
84.483939	2739.072598	22.099687
84.664670	2737.289470	22.104704
84.492004	2743.512136	22.109722
84.849890	2751.482269	22.114739
85.107781	2757.066213	22.119757
84.959766	2764.099320	22.124775
85.486064	2757.338397	22.129792
85.315070	2759.786008	22.134810
85.539712	2766.552422	22.139827
85.760186	2771.589901	22.144845
85.387162	2767.131863	22.149863
85.356199	2774.560095	22.154880
85.452409	2788.271320	22.159898
85.525141	2785.974868	22.164915
85.919873	2785.146096	22.169933
85.358623	2795.002468	22.174951
85.586567	2811.653581	22.179968
85.688103	2819.853279	22.184986
85.861949	2807.213907	22.190003
86.368577	2825.235346	22.195021
86.384242	2835.563158	22.200039
86.520002	2836.564522	22.205056
86.593688	2843.282023	22.210074
86.594399	2835.120003	22.215091
87.027505	2841.926377	22.220109
87.211372	2822.524844	22.225127
87.389194	2825.066155	22.230144
87.394806	2821.448298	22.235162
87.753880	2811.207020	22.240179
87.727162	2808.859866	22.245197
87.486316	2813.518296	22.250215
87.329844	2808.549734	22.255232
87.622400	2809.485501	22.260250
87.728304	2821.800195	22.265267
87.694126	2812.314891	22.270285
87.730871	2822.030246	22.275303
87.567395	2818.003327	22.280320
87.783792	2834.413243	22.285338
87.769349	2847.135021	22.290355
88.254243	2839.462101	22.295373
88.045263	2848.275420	22.300391
88.261498	2843.807104	22.305408
88.420309	2837.684468	22.310426
88.361506	2842.327010	22.315443
88.500607	2831.293259	22.320461
88.415149	2851.339082	22.325479
88.804900	2857.271675	22.330496
88.502348	2871.619867	22.335514
88.539044	2874.795600	22.340531
88.592254	2865.287108	22.345549
88.529809	2882.138436	22.350567
88.868468	2885.531983	22.355584
89.366224	2898.186176	22.360602
89.213331	2900.403722	22.365619
89.734431	2883.073419	22.370637
89.341242	2907.579897	22.375655
89.345267	2903.924398	22.380672
89.690642	2893.890373	22.385690
89.350064	2898.195173	22.390707
89.884277	2913.106668	22.395725
89.729050	2927.703257	22.400743
89.904423	2922.938327	22.405760
89.676592	2920.193422	22.410778
89.538826	2927.493264	22.415795
90.154094	2942.202711	22.420813
90.325086	2947.913953	22.425831
90.453658	2943.165819	22.430848
90.721042	2944.127631	22.435866
90.745812	2950.382559	22.440883
90.892550	2942.923542	22.445901
90.667755	2951.452173	22.450919
90.741418	2958.649467	22.455936
91.090237	2961.861532	22.460954
91.131274	2977.771963	22.465971
90.825748	2971.718874	22.470989
90.967533	2967.101225	22.476007
91.171360	2984.456958	22.481024
91.223336	2994.551923	22.486042
91.241866	3002.149244	22.491059
91.321116	2998.387253	22.496077
91.323876	3013.965997	22.501095
91.440509	3011.893043	22.506112
92.255858	3014.517561	22.511130
92.135177	3015.271895	22.516147
92.320334	3011.502778	22.521165
92.516903	3017.036443	22.526183
92.452569	3011.106520	22.531200
92.631880	3012.606069	22.536218
92.598105	3014.520906	22.541235
92.845919	3013.080739	22.546253
92.664658	3015.918209	22.551271
92.985308	3021.078937	22.556288
93.253856	3021.219951	22.561306
92.951058	3028.552002	22.566323
93.217428	3025.338280	22.571341
93.004162	3030.721535	22.576359
93.115156	3034.788338	22.581376
93.288526	3031.466093	22.586394
93.351245	3030.998638	22.591411
93.152365	3026.882531	22.596429
93.353788	3050.765797	22.601447
93.361510	3055.350627	22.606464
93.776063	3053.676022	22.611482
93.581755	3055.407703	22.616499
93.885379	3061.855699	22.621517
93.719037	3078.758207	22.626535
94.037335	3082.413794	22.631552
94.195508	3078.219641	22.636570
93.857990	3084.098971	22.641587
94.299758	3090.749428	22.646605
94.539907	3105.928091	22.651623
94.396913	3111.470797	22.656640
94.887480	3123.539212	22.661658
94.527839	3129.330491	22.666675
94.620456	3122.179723	22.671693
94.665494	3117.024849	22.676711
94.405836	3128.879401	22.681728
95.016373	3137.233060	22.686746
94.808483	3148.135793	22.691763
95.283692	3144.232831	22.696781
95.339218	3148.728132	22.701799
95.356390	3162.470962	22.706816
95.572423	3156.708536	22.711834
95.517121	3166.766748	22.716851
95.860057	3161.202220	22.721869
95.830606	3159.821263	22.726887
96.006484	3162.839522	22.731904
96.032824	3180.946034	22.736922
95.951098	3192.450811	22.741939
96.323753	3185.489708	22.746957
96.317901	3188.097723	22.751975
96.450968	3193.212139	22.756992
96.365264	3174.764621	22.762010
96.882297	3204.800695	22.767027
96.754035	3206.361072	22.772045
97.050497	3212.150586	22.777063
96.807912	3206.557840	22.782080
97.033690	3205.083236	22.787098
97.186033	3200.773187	22.792115
97.352756	3198.973271	22.797133
97.349190	3225.278176	22.802151
97.208867	3239.396085	22.807168
97.737267	3223.143758	22.812186
97.737233	3236.172867	22.817203
97.736104	3237.258827	22.822221
97.837309	3234.995732	22.827239
97.664031	3235.991880	22.832256
98.063911	3243.551650	22.837274
97.843249	3258.360759	22.842291
97.853058	3255.130380	22.847309
98.099572	3264.658451	22.852327
98.185576	3278.447398	22.857344
98.332578	3279.254494	22.862362
98.247887	3288.761874	22.867379
98.925958	3295.287009	22.872397
98.964596	3295.653423	22.877415
98.798354	3314.702406	22.882432
99.337281	3311.673185	22.887450
99.037650	3318.862824	22.892467
99.145825	3320.865924	22.897485
99.354550	3314.949935	22.902503
99.154225	3313.497892	22.907520
99.267235	3326.177945	22.912538
99.273742	3338.546439	22.917555
99.566515	3337.373801	22.922573
99.649196	3344.531960	22.927591
99.838006	3362.600575	22.932608
100.228200	3360.841384	22.937626
100.082954	3373.662933	22.942643
100.203373	3363.600767	22.947661
100.527291	3369.960475	22.952679
100.199240	3366.521036	22.957696
100.178117	3366.259243	22.962714
100.165655	3390.009183	22.967731
100.607117	3391.732821	22.972749
100.523830	3393.503953	22.977767
100.833251	3403.801848	22.982784
101.187466	3405.895818	22.987802
101.099440	3427.426142	22.992819
101.399341	3416.073307	22.997837
101.223348	3414.570099	23.002855
101.082971	3416.795216	23.007872
101.264675	3418.022982	23.012890
101.318453	3421.091977	23.017907
101.487774	3435.306716	23.022925
102.724595	3412.150867	23.027943
103.104053	3407.887250	23.032960
103.180480	3398.643127	23.037978
103.256177	3373.724959	23.042995
103.385502	3368.556808	23.048013
103.478003	3368.501310	23.053031
103.337925	3357.918139	23.058048
103.457774	3341.287834	23.063066
103.349186	3342.043443	23.068083
103.449929	3342.210750	23.073101
103.093700	3336.433765	23.078119
103.019818	3342.739005	23.083136
103.286578	3342.627799	23.088154
103.423853	3330.555611	23.093171
103.254049	3332.734827	23.098189
103.645845	3329.927501	23.103207
103.224244	3331.742161	23.108224
103.250284	3331.176288	23.113242
103.410229	3356.650914	23.118259
103.635713	3350.637598	23.123277
103.401656	3359.669722	23.128295
103.563627	3366.098990	23.133312
104.144518	3373.620987	23.138330
103.957604	3391.811622	23.143347
103.783296	3386.934071	23.148365
104.031874	3388.706866	23.153383
103.991345	3411.407029	23.158400
104.358468	3410.828748	23.163418
104.249918	3416.861690	23.168435
104.610784	3433.296862	23.173453
105.002502	3438.361357	23.178471
104.703707	3444.932279	23.183488
105.231060	3431.028223	23.188506
104.961959	3443.963916	23.193523
104.918066	3459.042187	23.198541
105.216398	3464.115007	23.203559
105.395097	3477.144695	23.208576
105.526161	3475.353495	23.213594
105.647538	3495.080402	23.218611
105.331056	3496.544040	23.223629
105.866545	3499.998401	23.228647
105.754464	3510.094107	23.233664
105.772153	3523.660376	23.238682
106.171325	3520.245852	23.243699
105.912825	3529.326079	23.248717
106.286290	3539.844429	23.253735
106.468905	3553.182877	23.258752
107.070592	3545.472425	23.263770
106.702009	3552.824463	23.268787
106.857458	3557.310524	23.273805
107.065299	3568.388258	23.278823
107.311501	3570.638050	23.283840
107.442537	3572.549219	23.288858
107.229050	3570.202820	23.293875
107.474504	3572.234941	23.298893
107.557588	3577.739214	23.303911
107.649961	3594.219754	23.308928
107.635898	3606.822066	23.313946
107.830682	3609.531274	23.318963
107.639225	3609.173066	23.323981
108.015212	3608.230412	23.328999
108.121210	3615.454465	23.334016
108.166165	3625.465661	23.339034
108.128408	3627.412750	23.344051
107.994490	3625.063346	23.349069
108.481169	3630.198239	23.354087
108.590106	3649.321246	23.359104
109.379020	3652.057319	23.364122
109.140020	3653.827621	23.369139
109.308311	3657.907683	23.374157
109.377022	3652.319685	23.379175
109.000758	3650.607952	23.384192
109.458993	3649.453561	23.389210
109.463088	3649.298284	23.394227
109.271616	3665.675010	23.399245
109.655486	3665.248759	23.404263
109.617067	3680.301107	23.409280
109.982520	3663.594151	23.414298
110.137385	3675.892288	23.419315
110.112204	3684.816097	23.424333
110.418115	3685.241648	23.429351
110.449779	3693.563161	23.434368
110.766947	3692.254113	23.439386
110.834457	3689.497538	23.444403
110.654690	3692.312784	23.449421
110.821381	3694.025843	23.454439
110.814895	3705.825324	23.459456
110.760253	3709.842478	23.464474
111.030010	3714.468487	23.469491
111.094133	3720.199875	23.474509
111.026106	3720.358907	23.479527
111.534917	3738.005313	23.484544
111.452761	3739.006150	23.489562
111.612649	3744.687822	23.494579
111.677085	3744.867133	23.499597
111.918181	3761.198271	23.504615
112.099586	3764.329394	23.509632
112.101995	3770.332444	23.514650
112.252992	3773.664028	23.519667
111.957939	3778.940374	23.524685
112.230224	3783.013641	23.529703
112.541184	3790.268780	23.534720
112.691234	3797.211400	23.539738
112.705195	3794.674675	23.544755
112.798123	3812.193772	23.549773
112.788168	3816.794189	23.554791
113.012496	3821.468376	23.559808
112.755044	3829.718462	23.564826
113.197610	3837.429614	23.569843
113.384691	3848.274044	23.574861
113.621190	3843.174190	23.579879
113.727274	3851.515681	23.584896
114.030710	3864.829118	23.589914
114.193881	3871.447760	23.594931
114.037783	3872.968366	23.599949
114.397357	3875.105742	23.604967
114.411551	3873.815740	23.609984
114.119477	3872.699977	23.615002
114.569028	3879.939751	23.620019
114.382200	3896.656848	23.625037
114.778367	3884.723646	23.630055
114.922438	3902.768246	23.635072
115.070476	3896.173483	23.640090
115.241976	3903.699871	23.645107
115.160406	3910.164331	23.650125
115.359830	3915.177022	23.655143
115.545412	3913.601342	23.660160
115.191189	3911.478955	23.665178
115.951971	3916.769840	23.670195
116.339605	3928.978022	23.675213
116.254588	3926.914462	23.680231
116.258091	3931.159285	23.685248
116.293379	3935.231840	23.690266
116.467521	3935.763264	23.695283
116.208888	3941.011857	23.700301
116.519537	3937.765788	23.705319
116.477232	3941.307601	23.710336
116.923164	3944.873928	23.715354
117.101843	3936.973916	23.720371
116.612605	3940.992924	23.725389
116.933086	3958.994161	23.730407
116.838908	3960.473509	23.735424
116.822308	3959.728069	23.740442
117.357966	3964.836447	23.745459
117.306760	3987.895677	23.750477
117.561717	3985.513709	23.755495
117.641821	3987.988429	23.760512
117.583889	3996.011635	23.765530
117.743110	4002.397370	23.770547
117.776001	4016.621316	23.775565
117.841175	4019.398237	23.780583
118.313141	4042.871129	23.785600
118.188822	4038.231770	23.790618
118.892396	4042.726770	23.795635
118.421115	4043.592889	23.800653
118.588962	4061.002640	23.805671
118.644024	4064.939557	23.810688
118.801964	4076.031733	23.815706
118.991056	4077.081628	23.820723
118.800105	4097.107480	23.825741
119.349126	4094.136524	23.830759
119.428607	4106.427825	23.835776
119.448851	4119.384950	23.840794
119.841096	4111.890147	23.845811
119.966291	4117.574215	23.850829
119.971220	4119.609362	23.855847
120.355840	4120.726476	23.860864
120.372755	4142.484252	23.865882
120.625157	4144.363843	23.870899
120.451538	4152.856612	23.875917
120.488912	4146.976667	23.880935
120.825993	4139.932395	23.885952
120.679969	4149.995896	23.890970
121.329405	4153.331528	23.895987
121.237760	4172.230840	23.901005
121.096454	4163.648569	23.906023
121.196616	4164.567207	23.911040
121.513790	4188.127666	23.916058
122.000033	4183.278983	23.921075
122.229021	4177.798284	23.926093
121.980884	4185.172738	23.931111
122.399889	4188.213052	23.936128
122.106359	4191.696423	23.941146
122.036509	4182.642109	23.946163
122.207328	4196.039695	23.951181
122.447198	4199.641513	23.956199
122.489615	4213.235989	23.961216
122.739311	4214.749864	23.966234
123.010836	4211.162668	23.971251
123.120886	4217.152159	23.976269
123.241942	4224.692896	23.981287
123.609264	4224.433362	23.986304
123.591467	4231.866442	23.991322
123.444414	4226.634029	23.996339
123.721575	4225.911997	24.001357
123.260925	4234.838015	24.006375
123.305319	4236.339865	24.011392
123.577277	4246.240086	24.016410
123.587525	4253.914984	24.021427
123.996073	4265.665590	24.026445
124.424197	4272.539576	24.031463
124.094888	4272.606975	24.036480
124.074523	4285.816785	24.041498
124.508423	4286.064478	24.046515
124.567648	4298.602129	24.051533
124.709287	4305.890316	24.056551
124.622572	4306.787735	24.061568
125.002954	4317.469592	24.066586
125.160855	4317.725804	24.071603
125.235423	4329.352013	24.076621
125.220663	4335.421069	24.081639
125.595614	4351.185700	24.086656
125.908929	4365.984653	24.091674
125.881229	4362.163381	24.096691
126.033952	4372.347494	24.101709
126.150360	4360.912341	24.106727
126.594299	4370.223835	24.111744
126.496137	4381.589900	24.116762
126.705857	4391.307406	24.121779
126.302625	4396.553531	24.126797
126.459591	4394.183707	24.131815
126.273342	4401.580118	24.136832
126.479343	4414.666176	24.141850
126.897586	4411.538896	24.146867
127.723925	4420.115020	24.151885
127.349525	4427.455694	24.156903
127.698737	4428.944527	24.161920
127.814642	4427.300808	24.166938
128.198945	4432.938069	24.171955
128.195022	4433.614195	24.176973
128.166835	4437.191771	24.181991
128.505094	4448.593669	24.187008
128.583314	4459.345043	24.192026
128.589669	4461.313719	24.197043
128.964500	4456.981143	24.202061
128.693771	4453.185300	24.207079
128.808473	4448.808255	24.212096
128.938889	4459.055884	24.217114
129.189221	4470.667273	24.222131
129.264157	4482.205141	24.227149
129.227561	4477.965426	24.232167
129.304828	4482.697545	24.237184
129.471583	4498.453888	24.242202
130.014079	4500.666847	24.247219
129.720635	4514.453052	24.252237
129.690579	4515.556246	24.257255
130.440292	4533.247757	24.262272
130.145811	4538.824099	24.267290
130.103858	4538.016321	24.272307
130.602202	4536.214826	24.277325
130.499556	4561.899579	24.282343
130.973624	4559.382202	24.287360
131.117166	4562.661439	24.292378
131.263399	4557.345104	24.297395
131.002862	4557.149209	24.302413
130.670833	4583.198204	24.307431
131.119690	4582.051541	24.312448
131.112757	4593.030978	24.317466
131.203997	4609.231688	24.322483
131.639549	4616.704379	24.327501
131.856274	4630.631701	24.332519
132.038661	4633.980621	24.337536
131.535515	4642.389513	24.342554
131.962155	4652.691852	24.347571
132.256928	4663.684038	24.352589
132.303826	4667.893825	24.357607
132.770450	4669.563145	24.362624
132.803236	4687.430256	24.367642
133.095459	4701.383682	24.372659
133.172930	4695.427835	24.377677
133.162639	4697.913658	24.382695
133.602452	4686.377130	24.387712
133.107845	4701.050409	24.392730
133.551550	4709.576140	24.397747
133.512157	4718.856214	24.402765
133.716684	4725.481315	24.407783
133.915376	4740.563680	24.412800
133.682240	4749.179685	24.417818
134.320341	4751.712291	24.422835
134.482559	4768.410225	24.427853
134.461763	4776.910907	24.432871
134.916747	4777.881309	24.437888
134.872394	4781.442546	24.442906
134.825705	4781.108980	24.447923
134.837995	4791.769871	24.452941
134.717832	4800.431332	24.457959
134.996374	4802.979240	24.462976
135.141050	4823.704566	24.467994
135.425919	4830.522294	24.473011
135.560405	4829.854158	24.478029
135.505372	4856.917591	24.483047
136.040254	4855.972080	24.488064
135.964972	4870.835482	24.493082
136.317341	4880.824461	24.498099
136.826308	4877.730238	24.503117
136.736460	4883.596595	24.508135
136.996728	4878.997778	24.513152
137.238229	4889.013601	24.518170
137.402149	4894.603463	24.523187
137.414344	4909.525792	24.528205
137.345739	4902.039735	24.533223
137.785494	4899.205719	24.538240
138.046093	4904.445842	24.543258
137.676357	4906.059977	24.548275
138.353761	4909.056776	24.553293
138.467674	4928.761158	24.558311
138.769225	4921.289703	24.563328
138.598919	4924.409842	24.568346
138.990170	4922.836578	24.573363
138.992505	4925.774998	24.578381
138.931481	4924.761857	24.583399
139.122729	4922.610710	24.588416
139.148828	4925.791620	24.593434
139.252162	4925.740734	24.598451
139.403588	4932.970821	24.603469
139.230956	4955.093861	24.608487
139.413381	4948.954191	24.613504
139.497262	4959.960656	24.618522
139.551496	4975.207893	24.623539
139.911782	4974.943140	24.628557
139.612517	4987.060787	24.633575
139.723155	4998.107276	24.638592
139.935531	5000.185779	24.643610
140.079828	5015.892426	24.648627
140.153566	5030.476928	24.653645
140.272476	5038.046749	24.658663
140.812805	5049.581510	24.663680
141.196488	5059.082725	24.668698
141.181220	5057.813038	24.673715
141.259436	5072.867204	24.678733
141.185689	5079.302443	24.683751
141.601622	5079.360413	24.688768
141.761126	5089.717479	24.693786
142.188583	5107.216980	24.698803
142.569906	5103.233618	24.703821
142.484602	5115.002170	24.708839
142.347307	5109.291326	24.713856
142.572252	5110.016850	24.718874
142.350767	5108.807876	24.723891
142.953644	5116.507087	24.728909
142.994362	5131.153662	24.733927
143.096106	5137.498296	24.738944
142.958720	5132.182035	24.743962
142.827345	5138.623167	24.748979
143.417863	5158.619296	24.753997
143.251577	5161.830387	24.759015
143.675296	5169.674483	24.764032
143.801010	5189.134239	24.769050
143.929556	5193.075671	24.774067
144.204058	5195.374897	24.779085
143.962403	5206.438825	24.784103
144.136707	5220.404810	24.789120
144.295136	5223.063138	24.794138
144.094500	5230.064404	24.799155
144.907913	5240.865206	24.804173
144.960314	5256.138217	24.809191
145.064730	5262.712910	24.814208
145.023267	5270.771976	24.819226
145.372449	5274.956642	24.824243
145.428597	5284.023168	24.829261
145.400434	5305.543179	24.834279
145.754632	5303.767352	24.839296
145.898086	5309.171149	24.844314
146.193183	5321.271660	24.849331
146.354437	5319.355600	24.854349
146.240415	5340.999586	24.859367
146.358969	5355.286916	24.864384
146.387568	5357.113311	24.869402
146.637928	5373.214013	24.874419
147.352713	5381.205156	24.879437
147.274675	5386.792039	24.884455
147.412119	5393.936114	24.889472
147.833225	5415.164905	24.894490
147.603540	5421.987709	24.899507
148.053190	5412.908215	24.904525
148.016712	5421.493726	24.909543
148.214121	5434.673407	24.914560
147.931333	5421.522936	24.919578
148.283271	5436.487170	24.924595
148.747183	5441.089519	24.929613
148.764789	5460.617008	24.934631
148.805160	5458.180084	24.939648
149.151482	5463.170189	24.944666
149.028625	5485.342892	24.949683
149.295415	5487.444494	24.954701
149.402868	5492.876082	24.959719
149.639633	5501.469331	24.964736
149.605683	5515.281925	24.969754
149.757047	5513.654651	24.974771
150.228579	5515.664204	24.979789
150.428916	5525.993023	24.984807
150.478041	5517.402376	24.989824
150.721085	5526.509189	24.994842
150.380676	5539.258666	24.999859
150.902722	5550.783984	25.004877
150.617581	5556.684308	25.009895
150.981599	5563.780326	25.014912
151.463677	5578.979979	25.019930
151.380495	5591.853342	25.024947
151.625722	5587.597626	25.029965
151.684027	5593.210562	25.034983
151.669342	5609.624470	25.040000
151.793278	5615.085080	25.045018
152.054635	5619.703425	25.050035
152.476398	5619.716292	25.055053
152.277000	5640.291265	25.060071
152.544110	5638.118680	25.065088
152.673623	5635.854012	25.070106
152.649820	5648.222511	25.075123
153.026150	5657.052817	25.080141
152.821678	5666.782230	25.085159
153.235861	5683.242657	25.090176
153.872705	5696.558869	25.095194
153.700319	5701.027374	25.100211
153.791444	5696.274921	25.105229
153.940361	5703.190038	25.110247
154.332551	5721.437479	25.115264
154.589867	5723.647920	25.120282
154.384063	5733.895277	25.125299
154.817087	5728.748328	25.130317
154.960517	5747.498803	25.135335
154.814541	5751.846385	25.140352
155.232561	5749.716436	25.145370
155.167549	5759.023148	25.150387
155.200614	5775.057232	25.155405
155.478854	5776.983455	25.160423
155.161745	5785.748841	25.165440
155.694102	5796.174163	25.170458
155.877216	5808.396713	25.175475
156.370183	5808.698314	25.180493
156.709576	5815.577320	25.185511
156.576456	5840.271120	25.190528
156.886064	5827.668364	25.195546
157.127214	5826.655184	25.200563
157.319600	5824.405896	25.205581
157.099243	5833.118266	25.210599
157.445980	5840.308645	25.215616
158.014558	5835.077296	25.220634
157.546109	5846.155043	25.225651
157.696169	5841.364908	25.230669
158.045397	5856.645584	25.235687
158.057275	5865.135340	25.240704
158.806633	5862.552565	25.245722
158.581407	5860.217175	25.250739
159.058230	5876.753195	25.255757
159.000847	5888.369503	25.260775
159.097182	5892.480283	25.265792
159.391092	5887.714952	25.270810
159.558445	5895.047098	25.275827
159.594725	5893.725083	25.280845
159.740166	5903.747044	25.285863
159.735457	5916.276883	25.290880
159.799321	5915.490347	25.295898
160.000454	5920.604341	25.300915
160.474237	5925.445180	25.305933
160.257842	5938.222856	25.310951
160.391687	5945.942237	25.315968
160.485789	5943.168530	25.320986
160.557775	5969.200397	25.326003
160.403928	5969.786425	25.331021
160.947709	5989.099462	25.336039
160.721676	6002.727858	25.341056
161.341188	6017.978952	25.346074
161.335306	6036.068099	25.351091
161.325775	6037.032428	25.356109
161.479920	6051.286316	25.361127
161.311730	6065.988464	25.366144
162.094993	6081.103471	25.371162
162.168691	6096.856833	25.376179
162.020023	6097.151631	25.381197
162.327088	6109.361277	25.386215
162.777836	6116.150345	25.391232
162.871071	6126.467873	25.396250
163.013770	6147.119247	25.401267
163.054127	6151.999638	25.406285
163.562886	6162.533042	25.411303
163.176739	6177.158938	25.416320
163.366313	6167.049669	25.421338
163.926579	6199.902929	25.426355
163.933915	6199.696614	25.431373
164.192097	6194.845255	25.436391
164.285078	6220.239676	25.441408
164.298893	6222.071630	25.446426
164.727088	6233.056490	25.451443
164.857490	6253.880377	25.456461
165.129510	6264.419360	25.461479
165.110316	6264.782268	25.466496
165.715835	6264.772664	25.471514
165.777728	6282.071707	25.476531
165.551574	6279.218693	25.481549
165.991013	6289.573622	25.486567
165.883468	6305.955350	25.491584
166.170179	6297.396566	25.496602
166.520254	6330.295616	25.501619
166.263690	6337.700666	25.506637
166.963003	6334.147059	25.511655
166.687058	6362.743653	25.516672
167.181179	6358.650804	25.521690
167.270473	6370.853703	25.526707
167.082583	6385.095141	25.531725
167.685492	6374.677930	25.536743
168.190495	6385.890767	25.541760
168.332829	6395.926111	25.546778
168.414858	6399.950856	25.551795
168.719188	6401.797295	25.556813
168.770259	6401.107447	25.561831
168.645127	6411.310974	25.566848
169.016604	6417.055039	25.571866
169.327245	6436.704972	25.576883
169.410599	6435.937458	25.581901
169.451200	6440.120230	25.586919
169.136117	6457.642651	25.591936
169.574913	6468.442895	25.596954
169.757058	6479.845270	25.601971
169.871763	6492.650380	25.606989
169.962781	6493.052849	25.612007
169.818927	6505.775358	25.617024
170.208062	6520.772536	25.622042
170.389898	6539.006396	25.627059
170.351101	6546.866724	25.632077
171.375475	6552.688487	25.637095
171.272222	6572.479172	25.642112
171.582401	6578.706418	25.647130
171.920954	6571.035931	25.652147
172.110649	6588.769828	25.657165
172.231929	6593.782873	25.662183
172.139618	6604.543285	25.667200
172.566456	6589.781296	25.672218
172.571455	6604.532507	25.677236
172.628693	6614.436088	25.682253
172.833664	6620.686144	25.687271
172.677800	6636.213914	25.692288
172.932207	6644.934368	25.697306
173.298642	6661.851431	25.702324
173.229156	6658.241421	25.707341
173.873883	6669.852406	25.712359
173.186054	6685.106829	25.717376
173.514900	6683.786277	25.722394
174.457074	6705.563152	25.727412
174.453048	6711.798629	25.732429
174.561966	6708.971975	25.737447
174.332877	6717.111580	25.742464
174.647518	6734.778690	25.747482
174.597799	6745.841886	25.752500
174.992283	6754.660410	25.757517
175.144370	6768.340625	25.762535
175.222587	6770.566626	25.767552
175.332892	6784.679579	25.772570
175.588471	6795.347719	25.777588
175.800277	6806.360509	25.782605
176.176586	6812.754261	25.787623
176.210667	6821.408296	25.792640
176.409390	6837.376316	25.797658
176.669245	6840.353623	25.802676
176.495886	6849.299034	25.807693
177.098244	6858.037687	25.812711
177.438594	6872.291455	25.817728
177.502343	6885.887733	25.822746
177.884797	6901.637612	25.827764
177.690478	6897.649341	25.832781
178.380694	6908.088454	25.837799
178.372747	6921.737031	25.842816
178.724560	6930.638090	25.847834
178.650912	6926.564613	25.852852
178.766735	6933.286494	25.857869
179.021373	6947.989402	25.862887
179.037696	6952.523353	25.867904
179.077147	6950.436793	25.872922
179.873892	6969.802787	25.877940
179.660281	6982.754381	25.882957
180.324316	6975.720945	25.887975
179.966510	6982.665418	25.892992
180.095067	6999.275956	25.898010
180.353985	7003.923447	25.903028
180.549624	7023.497317	25.908045
181.133705	7026.392291	25.913063
180.552963	7040.610543	25.918080
181.296475	7037.469753	25.923098
181.475789	7047.913218	25.928116
181.652206	7061.154185	25.933133
181.754121	7052.844987	25.938151
181.740969	7076.902895	25.943168
181.871148	7081.059151	25.948186
182.347388	7088.807455	25.953204
182.802312	7084.982615	25.958221
183.237288	7093.627641	25.963239
183.175123	7099.796591	25.968256
183.406019	7098.144092	25.973274
183.779031	7096.589293	25.978292
183.596583	7098.632027	25.983309
183.653738	7096.280651	25.988327
183.776481	7108.882888	25.993344
183.996773	7107.655079	25.998362
184.202359	7117.841913	26.003380
184.395447	7138.884284	26.008397
185.060904	7130.966622	26.013415
185.255594	7143.235603	26.018432
185.395542	7136.000085	26.023450
185.476054	7125.932633	26.028468
185.245276	7131.638682	26.033485
185.577594	7141.843559	26.038503
185.527745	7157.017366	26.043520
185.347994	7158.374626	26.048538
185.431730	7164.571252	26.053556
185.827749	7186.434262	26.058573
185.894488	7187.415115	26.063591
186.076738	7214.710039	26.068608
186.077727	7220.556596	26.073626
186.633875	7231.784040	26.078644
186.618841	7252.963325	26.083661
186.763261	7259.927089	26.088679
186.805043	7271.181468	26.093696
187.385736	7286.891151	26.098714
187.555583	7301.711805	26.103732
187.396490	7310.175344	26.108749
188.020064	7308.262420	26.113767
188.287505	7323.740239	26.118784
188.352538	7327.704710	26.123802
188.791558	7336.860648	26.128820
188.587631	7354.852681	26.133837
188.997516	7358.854687	26.138855
189.420385	7375.457341	26.143872
189.541441	7376.871673	26.148890
189.584385	7371.018235	26.153908
189.688302	7392.782030	26.158925
190.068510	7399.787833	26.163943
190.120896	7412.764355	26.168960
190.200528	7419.886707	26.173978
190.702157	7431.539537	26.178996
190.500915	7442.873135	26.184013
190.897414	7452.654563	26.189031
191.094601	7462.514577	26.194048
191.072836	7474.871358	26.199066
191.363490	7484.214777	26.204084
191.537410	7496.468305	26.209101
191.612272	7515.060849	26.214119
191.992014	7517.864792	26.219136
191.909736	7534.897154	26.224154
192.314765	7535.338849	26.229172
192.359167	7553.784667	26.234189
192.569911	7568.030865	26.239207
192.815774	7581.037178	26.244224
192.937048	7589.946261	26.249242
193.310273	7600.861629	26.254260
193.176984	7629.917706	26.259277
193.302644	7627.056720	26.264295
193.970828	7645.029221	26.269312
193.687224	7663.801196	26.274330
194.368044	7680.076424	26.279348
194.003603	7699.382009	26.284365
194.510985	7705.120976	26.289383
194.910145	7725.882327	26.294400
194.933244	7750.080658	26.299418
195.070508	7753.797127	26.304436
194.991465	7776.571879	26.309453
194.999617	7789.091507	26.314471
195.562807	7814.572317	26.319488
195.798538	7826.421749	26.324506
196.111532	7842.312756	26.329524
195.604474	7864.854748	26.334541
195.886882	7875.490898	26.339559
196.435644	7904.333216	26.344576
196.811600	7913.871857	26.349594
197.173335	7926.996016	26.354612
197.260861	7946.837213	26.359629
196.982579	7961.596003	26.364647
197.966329	7976.311793	26.369664
197.893889	7993.803970	26.374682
198.165728	7992.372290	26.379700
198.260851	8020.805979	26.384717
198.558780	8019.477551	26.389735
198.707448	8035.107171	26.394752
199.065368	8040.654975	26.399770
199.576035	8035.564685	26.404788
199.619946	8062.923576	26.409805
199.810964	8075.282152	26.414823
199.954450	8075.777465	26.419840
199.976304	8088.538246	26.424858
199.990747	8092.978059	26.429876
200.050653	8104.419533	26.434893
200.515284	8123.905075	26.439911
200.750375	8124.190297	26.444928
201.078243	8145.279000	26.449946
201.685261	8138.639230	26.454964
201.922976	8150.179161	26.459981
202.123547	8147.723100	26.464999
202.409736	8150.172414	26.470016
202.390589	8169.506480	26.475034
202.659388	8171.810137	26.480052
202.762382	8169.505115	26.485069
203.014356	8171.388353	26.490087
203.070493	8192.298681	26.495104
203.082253	8196.533726	26.500122
203.482890	8196.164747	26.505140
203.470119	8206.389548	26.510157
203.715663	8231.418714	26.515175
203.855507	8231.273703	26.520192
203.663599	8247.054728	26.525210
204.278902	8248.075986	26.530228
204.810254	8280.931182	26.535245
204.533568	8281.119781	26.540263
204.835138	8289.672614	26.545280
205.217201	8300.100813	26.550298
205.644526	8306.367124	26.555316
205.826553	8321.076189	26.560333
206.107732	8329.057634	26.565351
206.409164	8326.320548	26.570368
206.095017	8343.781464	26.575386
206.258737	8346.890892	26.580404
206.462633	8360.292658	26.585421
206.797750	8386.403533	26.590439
206.927079	8390.793848	26.595456
206.953321	8404.637065	26.600474
207.359445	8416.239181	26.605492
207.578302	8437.866228	26.610509
207.564386	8452.094632	26.615527
207.627137	8466.210006	26.620544
207.788253	8479.242857	26.625562
207.856369	8499.984324	26.630580
208.474788	8508.945413	26.635597
208.547114	8542.911696	26.640615
208.527963	8550.252019	26.645632
208.774812	8570.542503	26.650650
208.879826	8585.636391	26.655668
209.412131	8604.395156	26.660685
209.306914	8625.290205	26.665703
210.298260	8633.510978	26.670720
210.487249	8644.591586	26.675738
210.865752	8646.091975	26.680756
211.180686	8657.294934	26.685773
211.340351	8681.166838	26.690791
211.891515	8682.365504	26.695808
211.792502	8681.421249	26.700826
211.980871	8683.245047	26.705844
212.176376	8701.226327	26.710861
212.278722	8709.014947	26.715879
212.227361	8710.699498	26.720896
212.583343	8718.246327	26.725914
212.659672	8729.208875	26.730932
212.681265	8746.567057	26.735949
212.861804	8768.765635	26.740967
213.121684	8778.436568	26.745984
213.301157	8794.623990	26.751002
213.332515	8800.381043	26.756020
213.560703	8815.146413	26.761037
213.677088	8833.219146	26.766055
214.593899	8843.330245	26.771072
214.419377	8868.463964	26.776090
214.182058	8880.969111	26.781108
214.380049	8902.770460	26.786125
214.285763	8909.513347	26.791143
214.859462	8923.520610	26.796160
215.076918	8949.252897	26.801178
215.094024	8972.156130	26.806196
215.621257	8992.737822	26.811213
215.560656	9007.971658	26.816231
216.060788	9018.896401	26.821248
216.160441	9044.075808	26.826266
216.437735	9067.787705	26.831284
216.864100	9083.952487	26.836301
216.928351	9107.716753	26.841319
217.317202	9111.905562	26.846336
217.285974	9135.899516	26.851354
217.493527	9146.939629	26.856372
217.588752	9163.191086	26.861389
217.928374	9180.332515	26.866407
218.473285	9199.434054	26.871424
218.909122	9216.809870	26.876442
218.683747	9223.844935	26.881460
219.357368	9241.625546	26.886477
219.743426	9255.267793	26.891495
220.070780	9268.022571	26.896512
219.786138	9280.434365	26.901530
220.326493	9294.728134	26.906548
220.582723	9308.504422	26.911565
220.544741	9321.360671	26.916583
221.176847	9324.460035	26.921600
221.077508	9340.015943	26.926618
221.334803	9360.021495	26.931636
221.686564	9364.471916	26.936653
221.821146	9379.593390	26.941671
222.014835	9388.154159	26.946688
221.885021	9406.796450	26.951706
222.240750	9414.671965	26.956724
222.222220	9440.912343	26.961741
222.117903	9466.424222	26.966759
222.781809	9477.086779	26.971776
222.752874	9498.848600	26.976794
222.988043	9510.178236	26.981812
223.616007	9522.649295	26.986829
223.754983	9553.844300	26.991847
223.943828	9570.813954	26.996864
223.959321	9595.015880	27.001882
224.075015	9612.770585	27.006900
224.340169	9632.497350	27.011917
224.618430	9657.084437	27.016935
224.930883	9665.367825	27.021952
226.012299	9668.920986	27.026970
226.430019	9669.629130	27.031988
226.661143	9681.556248	27.037005
227.004278	9693.203764	27.042023
227.511621	9687.624158	27.047040
227.229821	9694.330398	27.052058
227.165088	9697.463214	27.057076
227.635210	9712.102989	27.062093
227.855662	9723.087748	27.067111
227.853455	9731.900382	27.072128
227.824819	9739.990961	27.077146
227.768891	9750.801173	27.082164
228.288605	9770.418744	27.087181
228.357213	9791.051065	27.092199
228.584290	9793.715092	27.097216
228.890835	9816.185660	27.102234
228.880348	9825.697420	27.107252
229.553159	9838.742630	27.112269
229.347909	9848.152301	27.117287
229.358654	9855.921020	27.122304
229.744570	9884.889812	27.127322
229.793288	9903.940353	27.132340
230.290877	9912.952629	27.137357
230.417536	9934.289591	27.142375
230.908763	9951.527963	27.147392
230.893592	9972.337795	27.152410
231.507261	9978.089241	27.157428
231.558901	9984.866490	27.162445
231.736052	10007.449125	27.167463
232.299920	10021.294573	27.172480
232.390349	10035.151049	27.177498
232.724658	10052.470931	27.182516
232.996555	10063.021577	27.187533
232.796432	10084.031009	27.192551
232.720883	10100.647883	27.197568
232.896110	10111.864134	27.202586
233.218669	10129.324856	27.207604
233.766870	10141.079457	27.212621
233.979797	10172.699640	27.217639
234.379522	10189.930466	27.222656
234.624210	10193.608494	27.227674
235.246746	10216.371050	27.232692
235.318974	10220.123462	27.237709
235.480017	10245.140159	27.242727
235.628447	10253.159016	27.247744
236.045733	10266.137202	27.252762
236.278363	10288.364163	27.257780
236.749307	10297.548147	27.262797
236.339886	10318.568526	27.267815
236.936586	10329.788348	27.272832
236.879081	10344.606002	27.277850
237.049091	10362.836007	27.282868
237.510020	10378.336586	27.287885
237.423028	10404.762704	27.292903
237.798438	10417.056062	27.297920
237.986898	10442.324485	27.302938
237.865526	10462.280026	27.307956
238.314674	10477.984614	27.312973
238.719032	10498.612482	27.317991
238.873703	10519.661547	27.323008
239.484974	10543.550343	27.328026
239.396720	10566.067873	27.333044
239.553598	10579.917501	27.338061
239.554871	10605.344925	27.343079
240.016860	10620.024580	27.348096
240.335187	10641.044987	27.353114
240.508621	10663.793188	27.358132
240.687887	10687.093074	27.363149
241.474755	10701.655591	27.368167
241.537565	10716.533629	27.373184
242.084845	10737.464599	27.378202
242.176064	10747.178766	27.383220
242.313313	10759.569653	27.388237
242.357609	10782.755026	27.393255
242.676637	10799.594888	27.398272
242.963792	10803.664238	27.403290
242.919338	10829.885365	27.408308
243.699661	10841.695615	27.413325
243.228052	10869.824578	27.418343
243.644436	10878.853201	27.423360
244.302870	10896.751449	27.428378
244.512003	10912.408747	27.433396
244.788004	10920.360543	27.438413
245.067935	10942.956623	27.443431
245.470919	10956.932171	27.448448
245.666964	10959.329674	27.453466
245.645253	10981.644666	27.458484
245.900935	10989.940695	27.463501
245.863847	11005.500864	27.468519
246.171557	11026.554943	27.473536
246.434195	11054.164985	27.478554
246.495383	11061.572650	27.483572
247.138271	11081.004951	27.488589
247.221731	11107.313785	27.493607
247.633850	11121.032258	27.498624
247.706101	11135.037645	27.503642
247.899306	11162.412429	27.508660
248.610447	11175.878853	27.513677
248.467495	11189.899049	27.518695
248.815080	11210.517649	27.523712
249.116644	11226.299665	27.528730
248.998275	11244.736743	27.533748
249.335409	11262.467797	27.538765
249.712263	11273.207932	27.543783
250.098626	11276.933450	27.548800
250.586227	11294.239942	27.553818
251.092315	11320.444978	27.558836
251.623263	11323.295289	27.563853
251.968407	11339.591586	27.568871
251.904495	11340.422615	27.573888
252.298843	11355.836547	27.578906
252.278629	11370.655484	27.583924
252.620148	11378.770883	27.588941
252.580698	11395.408508	27.593959
252.941998	11412.832783	27.598976
252.892936	11418.044333	27.603994
252.802183	11445.763992	27.609012
253.238079	11460.394714	27.614029
253.622390	11460.735561	27.619047
253.938796	11482.644520	27.624064
254.499216	11499.873484	27.629082
254.513830	11523.913839	27.634100
254.933928	11533.709516	27.639117
255.204541	11564.255710	27.644135
255.331989	11572.259474	27.649152
255.789261	11586.804846	27.654170
255.665508	11603.143250	27.659188
255.983620	11618.000954	27.664205
255.985744	11639.371996	27.669223
255.943022	11663.197313	27.674240
256.710161	11680.476160	27.679258
257.035564	11693.403419	27.684276
258.890192	11675.565494	27.689293
259.138206	11694.946613	27.694311
258.680221	11699.183411	27.699328
259.677817	11688.988782	27.704346
259.905511	11686.420651	27.709364
259.654554	11694.581634	27.714381
259.862904	11694.050102	27.719399
260.068348	11695.255769	27.724416
260.641956	11704.793818	27.729434
260.641342	11702.703531	27.734452
260.722818	11713.060741	27.739469
260.952302	11722.564290	27.744487
260.741359	11739.863787	27.749504
260.991062	11732.508251	27.754522
260.973752	11754.807681	27.759540
261.132586	11761.780348	27.764557
261.498781	11781.667227	27.769575
261.753366	11792.414183	27.774592
262.147261	11810.919982	27.779610
262.327085	11825.859512	27.784628
262.727818	11831.550162	27.789645
262.747233	11853.493447	27.794663
262.746424	11875.158886	27.799680
263.493467	11880.596363	27.804698
263.119620	11901.095063	27.809716
263.465359	11923.745171	27.814733
263.635984	11940.366158	27.819751
263.765070	11971.472003	27.824768
264.323152	11982.288362	27.829786
264.064956	11998.483964	27.834804
264.689034	12035.291088	27.839821
265.027811	12048.507012	27.844839
264.876737	12082.606291	27.849856
265.302571	12106.485079	27.854874
265.790925	12138.011745	27.859892
266.292251	12151.956990	27.864909
266.710383	12154.806158	27.869927
266.837597	12187.087351	27.874944
267.353695	12197.004122	27.879962
267.350983	12218.831302	27.884980
267.948251	12244.113895	27.889997
268.063342	12251.554636	27.895015
267.765533	12280.302666	27.900032
268.436449	12300.413929	27.905050
268.779694	12321.855462	27.910068
268.836353	12346.054485	27.915085
269.121484	12365.398902	27.920103
269.278456	12387.684409	27.925120
269.805227	12406.280502	27.930138
270.301392	12423.495117	27.935156
270.983286	12435.817579	27.940173
271.103098	12460.186852	27.945191
271.115751	12470.362631	27.950208
271.456507	12480.499649	27.955226
271.719760	12509.738022	27.960244
272.020411	12525.489694	27.965261
272.236035	12543.019941	27.970279
272.225619	12566.320289	27.975296
272.385561	12587.604525	27.980314
272.370250	12614.906716	27.985332
272.824235	12634.395483	27.990349
273.075173	12664.472861	27.995367
273.082928	12687.659987	28.000384
273.493207	12706.028310	28.005402
273.862354	12735.278864	28.010420
274.110297	12759.773714	28.015437
274.942395	12774.618132	28.020455
274.984568	12801.640009	28.025472
274.958512	12825.353653	28.030490
275.492603	12845.632197	28.035508
276.090529	12869.222886	28.040525
276.281587	12894.093139	28.045543
276.926363	12903.519598	28.050560
277.463852	12914.440774	28.055578
277.395229	12915.458926	28.060596
277.641977	12940.209988	28.065613
277.989211	12949.206233	28.070631
278.422703	12969.832251	28.075648
278.711105	12970.443948	28.080666
278.871075	13000.258213	28.085684
279.300943	13014.632139	28.090701
279.292500	13024.126247	28.095719
279.269456	13038.170081	28.100736
279.869659	13049.514150	28.105754
279.840378	13067.885365	28.110772
280.009266	13086.939251	28.115789
280.442944	13094.769373	28.120807
280.211044	13117.498768	28.125824
280.611122	13143.009249	28.130842
280.753660	13157.740932	28.135860
281.128015	13181.963889	28.140877
281.224397	13205.403034	28.145895
281.447703	13232.886635	28.150912
281.878579	13248.899570	28.155930
281.708416	13283.209266	28.160948
281.908959	13312.701868	28.165965
282.593667	13340.274404	28.170983
282.945482	13373.782474	28.176000
283.035344	13398.258701	28.181018
283.496453	13433.562449	28.186036
283.673141	13452.672324	28.191053
284.600678	13468.591853	28.196071
284.521642	13501.362348	28.201088
285.073989	13519.914478	28.206106
284.923975	13551.650873	28.211124
285.462298	13572.096909	28.216141
285.962198	13594.788031	28.221159
285.981232	13618.145060	28.226176
286.430468	13636.476604	28.231194
286.820459	13662.036734	28.236212
286.744623	13689.908926	28.241229
287.330105	13702.443120	28.246247
287.486957	13726.716634	28.251264
287.650712	13754.766138	28.256282
287.920131	13774.506055	28.261300
288.208306	13808.400670	28.266317
288.506589	13827.870844	28.271335
288.907369	13865.948159	28.276352
289.113188	13895.624006	28.281370
289.328136	13911.330253	28.286388
290.010289	13931.204638	28.291405
290.812289	13943.569277	28.296423
291.059067	13971.296601	28.301440
291.198872	13992.797160	28.306458
291.579805	14003.692962	28.311476
291.784682	14028.827817	28.316493
292.725271	14034.800909	28.321511
292.664360	14048.684042	28.326528
292.841690	14053.450298	28.331546
293.058127	14085.695480	28.336564
293.301125	14101.909104	28.341581
293.814332	14123.970310	28.346599
293.858161	14135.471665	28.351616
293.825528	14165.261081	28.356634
293.996245	14174.036068	28.361652
294.279890	14202.219040	28.366669
295.058842	14215.907569	28.371687
295.537761	14240.949245	28.376704
295.861800	14258.239866	28.381722
296.032427	14274.060732	28.386740
296.349401	14292.404154	28.391757
296.624588	14300.420669	28.396775
296.404384	14319.015646	28.401792
296.702104	14345.210146	28.406810
296.961886	14372.459136	28.411828
297.257156	14398.625670	28.416845
297.366118	14411.285510	28.421863
297.765105	14438.196971	28.426880
298.185521	14471.989940	28.431898
298.565019	14494.145157	28.436916
298.744895	14518.270797	28.441933
299.667003	14534.476313	28.446951
299.777321	14548.500370	28.451968
299.862036	14576.212904	28.456986
300.389562	14586.394433	28.462004
300.467804	14595.964175	28.467021
300.711038	14613.656236	28.472039
301.064814	14643.527987	28.477056
301.127131	14654.290897	28.482074
301.108339	14667.116197	28.487092
301.276925	14693.031374	28.492109
301.749164	14716.028198	28.497127
302.168441	14742.684252	28.502144
302.175600	14778.860636	28.507162
302.618216	14796.575323	28.512180
302.665007	14836.248086	28.517197
303.218093	14862.646479	28.522215
303.637040	14891.039826	28.527232
304.005389	14916.219723	28.532250
304.355935	14933.911062	28.537268
304.625263	14979.824716	28.542285
304.897849	14997.354621	28.547303
305.156810	15017.050089	28.552320
305.245880	15051.281297	28.557338
305.758948	15079.903367	28.562356
305.922586	15112.720727	28.567373
306.755130	15128.024878	28.572391
307.141131	15154.361416	28.577408
307.074201	15177.057943	28.582426
307.353354	15201.614213	28.587444
307.229746	15235.395844	28.592461
307.890965	15255.672841	28.597479
308.899988	15269.660872	28.602496
309.539209	15290.206649	28.607514
310.174901	15298.517686	28.612532
310.307565	15322.323271	28.617549
310.896838	15331.497499	28.622567
311.259652	15346.976474	28.627584
311.153144	15360.918234	28.632602
311.791538	15364.693523	28.637620
311.526727	15388.207720	28.642637
311.800695	15391.199984	28.647655
312.326497	15417.546569	28.652672
312.139055	15438.980000	28.657690
312.641795	15457.421775	28.662708
312.976981	15497.717142	28.667725
312.857542	15507.931026	28.672743
312.981001	15532.354192	28.677760
313.199738	15559.406009	28.682778
313.920052	15584.392685	28.687796
314.147108	15609.390334	28.692813
314.249583	15628.397154	28.697831
314.826011	15649.992259	28.702848
315.035740	15673.621972	28.707866
316.635885	15686.225939	28.712884
317.126441	15689.819158	28.717901
317.749269	15702.039303	28.722919
318.017383	15700.891896	28.727936
318.358326	15705.250773	28.732954
319.013726	15690.284795	28.737972
319.087170	15693.387479	28.742989
319.071347	15698.127553	28.748007
319.652567	15697.730170	28.753024
319.862734	15716.208551	28.758042
319.734831	15718.467906	28.763060
320.060826	15732.146366	28.768077
320.372891	15736.159193	28.773095
320.690104	15741.030296	28.778112
320.879930	15755.162801	28.783130
321.172054	15766.041941	28.788148
321.063346	15775.581548	28.793165
320.945781	15792.544777	28.798183
321.532300	15804.502212	28.803200
321.551159	15833.367063	28.808218
321.635285	15849.199624	28.813236
322.001776	15875.379131	28.818253
322.430502	15892.446379	28.823271
322.577734	15918.868747	28.828288
322.727585	15950.988533	28.833306
322.888786	15979.063809	28.838324
322.969193	16014.558304	28.843341
323.669323	16041.819653	28.848359
323.671660	16073.065754	28.853376
323.825385	16110.090260	28.858394
324.157614	16141.332173	28.863412
324.296265	16176.344074	28.868429
324.441415	16212.722636	28.873447
325.083694	16239.908050	28.878464
325.519122	16291.405108	28.883482
325.802429	16324.862758	28.888500
326.136090	16364.828542	28.893517
326.277649	16396.170222	28.898535
327.143493	16429.107247	28.903552
326.764180	16466.942390	28.908570
327.660137	16501.842573	28.913588
327.922940	16542.009334	28.918605
328.204850	16576.768950	28.923623
328.659802	16601.669021	28.928640
328.946930	16647.438580	28.933658
329.542287	16673.077957	28.938676
330.060277	16705.927811	28.943693
330.363842	16743.271183	28.948711
330.511048	16770.402238	28.953728
330.429183	16804.300107	28.958746
331.211906	16831.972886	28.963764
331.768160	16861.209929	28.968781
331.974606	16894.235247	28.973799
332.069598	16931.017842	28.978816
332.519823	16963.461817	28.983834
332.970080	16996.057454	28.988852
333.315128	17028.499061	28.993869
333.429114	17070.610661	28.998887
333.498899	17100.341203	29.003904
334.152548	17135.943799	29.008922
334.835813	17159.280056	29.013940
335.185363	17190.015575	29.018957
335.433587	17202.320627	29.023975
336.249764	17230.462533	29.028992
336.295128	17263.362100	29.034010
337.291307	17285.114397	29.039028
337.547608	17308.075506	29.044045
337.607653	17344.851727	29.049063
338.080044	17353.148180	29.054080
338.090425	17392.111739	29.059098
338.630580	17406.841263	29.064116
338.571634	17431.563893	29.069133
338.925086	17470.164321	29.074151
339.458148	17483.858971	29.079168
339.676090	17510.635688	29.084186
340.256189	17540.912388	29.089204
339.971564	17575.885733	29.094221
341.223018	17595.570516	29.099239
342.780845	17586.456919	29.104256
343.486657	17600.787917	29.109274
343.392754	17599.994027	29.114292
343.575150	17610.806114	29.119309
343.851302	17629.039090	29.124327
344.254522	17621.736224	29.129344
344.361483	17634.379548	29.134362
344.389486	17637.028493	29.139380
344.826925	17650.927763	29.144397
344.760101	17672.960723	29.149415
344.905090	17685.035875	29.154432
345.107192	17705.118888	29.159450
345.424042	17721.519843	29.164468
345.514049	17734.620743	29.169485
345.607863	17758.978721	29.174503
345.968416	17791.551846	29.179520
345.704138	17831.279500	29.184538
346.281423	17857.785615	29.189556
346.389552	17895.332397	29.194573
346.839500	17938.050273	29.199591
347.166780	17961.474851	29.204608
347.373704	18012.020437	29.209626
347.335885	18047.025461	29.214644
348.042496	18084.668387	29.219661
348.360084	18130.913656	29.224679
348.542713	18171.721795	29.229696
349.016780	18211.890515	29.234714
349.108714	18250.091229	29.239732
349.956330	18291.174510	29.244749
350.028095	18334.116754	29.249767
350.582668	18372.832778	29.254784
350.946933	18419.020880	29.259802
351.526665	18454.176290	29.264820
351.858647	18489.016781	29.269837
351.983964	18528.223639	29.274855
353.079358	18562.521396	29.279872
353.495999	18594.897551	29.284890
353.715329	18633.085378	29.289908
354.108659	18654.396644	29.294925
354.334035	18690.574600	29.299943
354.412324	18720.900157	29.304960
355.018560	18757.542953	29.309978
355.405375	18792.748146	29.314996
355.935184	18825.479706	29.320013
356.342027	18859.020306	29.325031
357.851318	18860.584487	29.330048
358.672623	18866.868423	29.335066
359.837351	18858.441286	29.340084
360.601236	18857.765690	29.345101
360.594683	18861.974392	29.350119
360.981010	18858.287490	29.355136
361.309405	18867.523232	29.360154
361.682545	18865.335712	29.365172
361.661127	18861.959073	29.370189
362.062696	18874.114811	29.375207
361.838902	18869.721117	29.380224
361.906022	18869.205206	29.385242
362.083791	18886.519740	29.390260
362.505689	18897.269757	29.395277
362.196861	18928.041661	29.400295
363.001388	18942.610906	29.405312
363.040932	18969.581842	29.410330
363.088604	18992.305956	29.415348
363.442428	19017.604045	29.420365
363.732472	19051.864555	29.425383
363.807936	19074.123207	29.430400
364.051710	19109.774677	29.435418
364.590212	19145.114695	29.440436
364.857308	19169.940090	29.445453
365.147606	19200.479583	29.450471
365.908471	19224.545370	29.455488
366.382953	19261.399289	29.460506
366.463273	19287.890432	29.465524
366.393286	19319.453189	29.470541
366.456432	19360.560521	29.475559
367.205039	19387.275652	29.480576
367.318573	19422.619560	29.485594
367.424172	19463.537237	29.490612
367.989003	19494.710211	29.495629
367.968475	19541.668860	29.500647
368.456087	19583.158750	29.505664
368.734681	19617.813762	29.510682
368.732185	19669.243062	29.515700
369.306997	19713.922824	29.520717
369.421092	19765.517337	29.525735
370.112921	19797.719703	29.530752
370.486024	19856.122699	29.535770
370.772367	19895.660890	29.540788
371.396193	19932.833860	29.545805
371.556190	19982.494722	29.550823
371.943838	20019.749078	29.555840
372.397969	20075.246314	29.560858
372.864330	20115.078977	29.565876
373.163256	20162.703028	29.570893
373.592380	20213.529097	29.575911
374.108236	20245.747127	29.580928
374.713373	20283.214327	29.585946
375.037715	20329.128873	29.590964
376.202989	20352.627244	29.595981
376.422479	20386.262993	29.600999
377.011282	20417.376816	29.606016
377.942851	20435.800395	29.611034
378.232699	20461.919115	29.616052
378.415634	20483.947710	29.621069
378.924885	20516.104037	29.626087
379.600679	20535.831440	29.631104
379.920699	20570.677514	29.636122
380.152249	20596.717087	29.641140
380.870487	20613.714712	29.646157
381.068254	20639.544809	29.651175
381.718473	20664.754372	29.656192
381.981862	20684.173739	29.661210
381.872928	20712.118083	29.666228
382.396068	20724.022151	29.671245
382.473735	20754.546822	29.676263
382.938855	20775.463734	29.681280
383.363910	20808.733130	29.686298
383.681064	20849.323591	29.691316
384.043667	20871.943685	29.696333
383.961787	20907.977990	29.701351
384.261742	20934.278989	29.706368
384.492472	20978.914431	29.711386
384.612071	21016.737096	29.716404
385.304941	21049.971269	29.721421
385.797263	21104.441831	29.726439
386.287202	21141.157853	29.731456
386.468276	21169.284885	29.736474
386.546656	21214.045818	29.741492
386.963002	21249.737327	29.746509
387.424021	21296.466770	29.751527
387.850456	21333.862866	29.756544
388.218888	21375.299385	29.761562
388.262313	21411.466628	29.766580
389.291756	21460.546406	29.771597
389.454761	21502.723056	29.776615
389.576946	21549.537764	29.781632
390.512763	21599.055903	29.786650
390.439326	21634.287738	29.791668
391.145482	21669.523897	29.796685
391.854231	21707.944340	29.801703
392.486738	21729.613247	29.806720
392.952821	21769.032264	29.811738
393.456811	21804.925885	29.816756
393.789085	21823.033923	29.821773
393.582799	21855.835289	29.826791
394.102958	21884.061874	29.831808
394.319037	21912.980644	29.836826
394.770743	21947.915942	29.841844
395.712228	21963.198971	29.846861
396.357598	22002.495588	29.851879
396.445132	22018.019839	29.856896
397.135267	22059.388445	29.861914
397.367836	22079.572271	29.866932
397.764382	22102.359066	29.871949
397.940099	22144.655150	29.876967
397.885958	22170.463519	29.881984
398.380363	22200.242708	29.887002
398.598426	22240.649343	29.892020
399.031852	22282.134450	29.897037
399.329440	22323.299700	29.902055
399.568380	22358.635546	29.907072
400.269878	22402.397956	29.912090
400.120092	22448.530710	29.917108
400.675916	22472.607322	29.922125
400.988470	22537.687911	29.927143
401.274360	22579.089326	29.932160
402.067911	22609.081351	29.937178
402.825685	22661.081805	29.942196
403.170022	22705.937146	29.947213
403.422736	22747.198770	29.952231
403.939783	22779.989464	29.957248
404.282389	22828.952735	29.962266
404.689927	22870.114534	29.967284
405.142570	22908.160361	29.972301
404.974813	22950.113855	29.977319
406.262593	22976.736772	29.982336
407.217692	23022.824174	29.987354
407.293708	23056.461657	29.992372
407.833165	23090.361521	29.997389
408.075060	23120.023664	30.002407
408.232234	23160.599683	30.007424
408.630923	23191.374823	30.012442
408.760985	23230.185860	30.017460
409.599516	23263.811683	30.022477
410.215220	23308.480534	30.027495
410.063431	23337.155675	30.032512
411.009771	23377.204093	30.037530
411.711980	23404.614422	30.042548
412.313093	23428.280668	30.047565
412.739200	23456.151386	30.052583
413.154979	23484.301808	30.057600
413.920920	23513.193652	30.062618
413.996436	23538.825502	30.067636
414.208729	23561.421656	30.072653
414.685117	23596.002105	30.077671
414.964748	23626.581709	30.082688
415.325752	23663.891335	30.087706
415.665656	23689.772655	30.092724
415.624605	23726.292262	30.097741
416.637411	23759.392398	30.102759
416.553298	23801.802210	30.107776
417.432492	23825.608633	30.112794
417.956745	23867.879060	30.117812
418.306752	23891.155469	30.122829
418.720774	23924.987929	30.127847
419.091220	23953.082919	30.132864
419.745397	23972.570684	30.137882
420.099020	24002.993928	30.142900
420.212430	24044.880401	30.147917
420.577991	24064.944297	30.152935
421.036683	24089.897528	30.157952
421.544337	24115.614096	30.162970
421.666940	24159.066596	30.167988
422.061632	24184.807266	30.173005
422.318266	24224.504095	30.178023
422.464505	24259.946301	30.183040
423.184496	24289.206680	30.188058
423.270349	24336.867805	30.193076
423.675008	24370.354909	30.198093
423.977499	24422.608215	30.203111
424.216520	24453.555659	30.208128
424.809198	24498.249736	30.213146
424.867161	24551.704484	30.218164
425.488610	24584.127893	30.223181
425.785581	24636.698602	30.228199
426.160529	24675.126502	30.233216
426.355688	24724.509328	30.238234
427.036424	24779.320657	30.243252
427.419285	24838.615219	30.248269
427.697961	24879.725502	30.253287
428.581268	24928.880969	30.258304
429.383344	24964.152175	30.263322
429.966563	25016.641123	30.268340
430.167619	25054.667243	30.273357
430.923447	25090.622130	30.278375
431.208206	25135.884077	30.283392
431.920950	25171.770021	30.288410
432.572374	25205.864486	30.293428
432.804067	25249.561368	30.298445
433.167874	25281.337396	30.303463
433.193632	25324.118720	30.308480
433.942329	25359.771853	30.313498
433.829920	25415.853042	30.318516
433.976769	25461.036202	30.323533
434.765502	25508.021216	30.328551
435.039139	25560.092397	30.333568
435.734404	25600.070833	30.338586
436.431032	25646.767239	30.343604
436.926314	25681.651682	30.348621
437.365732	25730.000158	30.353639
437.502751	25776.398999	30.358656
438.162001	25818.051985	30.363674
438.824058	25857.100771	30.368692
439.391566	25897.731809	30.373709
440.548381	25931.647223	30.378727
440.720035	25966.709249	30.383744
441.364236	25983.128990	30.388762
442.209368	26019.507632	30.393780
443.070817	26035.703787	30.398797
443.752459	26056.642895	30.403815
443.897908	26090.483146	30.408832
444.091811	26101.652000	30.413850
444.298574	26124.435185	30.418868
444.914859	26151.654169	30.423885
445.823858	26180.053444	30.428903
445.572736	26201.151442	30.433920
445.944240	26218.442025	30.438938
446.087405	26244.837780	30.443956
446.733665	26282.493114	30.448973
447.405063	26314.506999	30.453991
447.424420	26353.360364	30.459008
447.926593	26383.959865	30.464026
447.397399	26413.633883	30.469044
448.003928	26459.524657	30.474061
448.525681	26493.881779	30.479079
448.975998	26553.531064	30.484096
449.489734	26592.768829	30.489114
449.932798	26624.016296	30.494132
450.360471	26662.446044	30.499149
450.941827	26697.337718	30.504167
451.089127	26736.930211	30.509184
451.459959	26775.754613	30.514202
451.934346	26809.165323	30.519220
452.412619	26854.975956	30.524237
452.664869	26891.942018	30.529255
452.908756	26939.628772	30.534272
453.549131	26986.526694	30.539290
453.449941	27036.751316	30.544308
454.049065	27085.905984	30.549325
454.832637	27128.363847	30.554343
454.952772	27185.386849	30.559360
455.489963	27222.808195	30.564378
455.643093	27268.771814	30.569396
456.132570	27329.529643	30.574413
457.058213	27374.961673	30.579431
457.357467	27433.373102	30.584448
457.826749	27468.441668	30.589466
458.524374	27515.028456	30.594484
459.523663	27556.530629	30.599501
460.141395	27604.128781	30.604519
460.914756	27641.311648	30.609536
461.500450	27674.030045	30.614554
461.844697	27695.687357	30.619572
462.601196	27732.702377	30.624589
462.963612	27764.804869	30.629607
463.211692	27808.852330	30.634624
464.089813	27826.229269	30.639642
464.506421	27858.102198	30.644660
464.919218	27892.876952	30.649677
465.207517	27924.302353	30.654695
465.377181	27979.701729	30.659712
465.737668	28010.951619	30.664730
466.179285	28057.617671	30.669748
466.870888	28099.573668	30.674765
466.961342	28144.303895	30.679783
467.131013	28188.535115	30.684800
467.549765	28227.291571	30.689818
468.290405	28276.332135	30.694836
468.512334	28327.204917	30.699853
468.617580	28368.962550	30.704871
468.894756	28426.937822	30.709888
469.462794	28477.851580	30.714906
469.876467	28533.644052	30.719924
470.125040	28598.615146	30.724941
470.960550	28641.194442	30.729959
471.223015	28708.856404	30.734976
471.649562	28759.508582	30.739994
472.285709	28818.857264	30.745012
472.768852	28873.059544	30.750029
473.236054	28926.101407	30.755047
473.576717	28991.451219	30.760064
474.158868	29049.791347	30.765082
474.814506	29096.356711	30.770100
475.299097	29147.247274	30.775117
475.918180	29196.542957	30.780135
476.562786	29252.737365	30.785152
477.085488	29300.379631	30.790170
477.826494	29347.905641	30.795188
478.387349	29392.640762	30.800205
479.069134	29429.430353	30.805223
479.385093	29477.257117	30.810240
480.012628	29509.674802	30.815258
480.974427	29552.135071	30.820276
481.010672	29592.420524	30.825293
481.637814	29631.216525	30.830311
482.202573	29675.035077	30.835328
482.162583	29717.140576	30.840346
482.840086	29746.213210	30.845364
483.408459	29793.969568	30.850381
483.645114	29823.585451	30.855399
483.989947	29871.193685	30.860416
484.277603	29910.833542	30.865434
484.659293	29955.547377	30.870452
485.069213	30001.318866	30.875469
486.209514	30028.050066	30.880487
486.764448	30072.231317	30.885504
487.545796	30104.821809	30.890522
488.218902	30133.282509	30.895540
488.702526	30174.592618	30.900557
489.203179	30202.448289	30.905575
489.494861	30240.058992	30.910592
490.043026	30283.634903	30.915610
490.056537	30309.303963	30.920628
490.137066	30359.318918	30.925645
490.746763	30404.737619	30.930663
491.005639	30457.746517	30.935680
491.494284	30504.480291	30.940698
492.066999	30550.903895	30.945716
492.543619	30599.801708	30.950733
492.953278	30646.560817	30.955751
493.360635	30703.504343	30.960768
493.692405	30751.951090	30.965786
494.142435	30811.973134	30.970804
494.720333	30872.942524	30.975821
495.289824	30926.264298	30.980839
495.803137	30976.908331	30.985856
496.564028	31025.591942	30.990874
496.943534	31079.879466	30.995892
497.273126	31136.988080	31.000909
497.698692	31194.448475	31.005927
497.893746	31260.517329	31.010944
498.264051	31317.759139	31.015962
499.166410	31375.410868	31.020980
499.493601	31435.611997	31.025997
500.090301	31495.069373	31.031015
500.439486	31553.781787	31.036032
501.266689	31608.525277	31.041050
502.178464	31664.115430	31.046068
502.289735	31715.759859	31.051085
502.740864	31769.336241	31.056103
503.028938	31828.375091	31.061120
503.913249	31885.683359	31.066138
504.077778	31941.561980	31.071156
505.053270	32007.966143	31.076173
505.917995	32051.236986	31.081191
506.529241	32106.540328	31.086208
506.806511	32155.435091	31.091226
507.523138	32215.470002	31.096244
507.985644	32268.211384	31.101261
508.941544	32308.591977	31.106279
508.695469	32349.913226	31.111296
509.869233	32398.434231	31.116314
510.747803	32437.240358	31.121332
511.024087	32486.401574	31.126349
511.438241	32526.829508	31.131367
512.017171	32562.237274	31.136384
512.586505	32611.258055	31.141402
513.510510	32648.938450	31.146420
513.521833	32690.150511	31.151437
514.154856	32728.995638	31.156455
514.387436	32771.134168	31.161472
514.842754	32816.822555	31.166490
516.011640	32845.127136	31.171508
516.314919	32888.822725	31.176525
516.582186	32935.432251	31.181543
517.388135	32964.571467	31.186560
517.612302	33005.516890	31.191578
518.096214	33035.673941	31.196596
518.337469	33093.098884	31.201613
518.488741	33126.153169	31.206631
518.668383	33179.307838	31.211648
519.261017	33230.709911	31.216666
519.794674	33282.013867	31.221684
519.919682	33341.841199	31.226701
520.275518	33389.904636	31.231719
520.871834	33445.972533	31.236736
521.251920	33516.375621	31.241754
522.180478	33580.667813	31.246772
522.015162	33639.454012	31.251789
522.621289	33703.386122	31.256807
523.116518	33767.601338	31.261824
523.471444	33835.101111	31.266842
524.282729	33900.424239	31.271860
524.967386	33965.723146	31.276877
525.474947	34028.040475	31.281895
526.223311	34089.144282	31.286912
526.331853	34158.732180	31.291930
527.480271	34216.523907	31.296948
527.746809	34282.654311	31.301965
528.409139	34337.253722	31.306983
529.329473	34393.595845	31.312000
529.840503	34447.713429	31.317018
530.458206	34507.005345	31.322036
531.402731	34556.629453	31.327053
531.800487	34616.638973	31.332071
532.314996	34666.387593	31.337088
532.648774	34725.130255	31.342106
533.526895	34781.366215	31.347124
533.857642	34840.166574	31.352141
534.216588	34894.517771	31.357159
535.295857	34952.891393	31.362176
535.430514	34999.456697	31.367194
536.165514	35053.452232	31.372212
536.454566	35105.924394	31.377229
536.962341	35164.874967	31.382247
537.816311	35223.942200	31.387264
538.058958	35282.934625	31.392282
538.502782	35335.844685	31.397300
538.599965	35404.983203	31.402317
539.044475	35458.241221	31.407335
539.850417	35525.372242	31.412352
540.326429	35600.212279	31.417370
540.692576	35667.665549	31.422388
541.009217	35738.819432	31.427405
540.998421	35804.100143	31.432423
541.759217	35876.961698	31.437440
542.057183	35942.535919	31.442458
543.138671	36012.451739	31.447476
543.753864	36088.447790	31.452493
544.182907	36162.791308	31.457511
545.368882	36228.986109	31.462528
546.045386	36286.705636	31.467546
546.563007	36352.638753	31.472564
547.210516	36403.097775	31.477581
547.804982	36463.043756	31.482599
548.318428	36527.890471	31.487616
548.930827	36592.336164	31.492634
549.741687	36641.132436	31.497652
550.374235	36695.344203	31.502669
550.923792	36746.805814	31.507687
551.992820	36791.508747	31.512704
552.761299	36849.955222	31.517722
553.542149	36881.519293	31.522740
553.921853	36927.493970	31.527757
554.194526	36962.976040	31.532775
554.894485	37002.191610	31.537792
555.061990	37055.225090	31.542810
555.432976	37090.736238	31.547828
555.785377	37148.388706	31.552845
556.116334	37197.836843	31.557863
556.814373	37250.351396	31.562880
556.900557	37311.030674	31.567898
557.711626	37366.348084	31.572916
558.331832	37417.819212	31.577933
558.914163	37470.333455	31.582951
559.290459	37520.141998	31.587968
560.259652	37577.401811	31.592986
561.453343	37608.187733	31.598004
562.999014	37632.778374	31.603021
563.170293	37682.575138	31.608039
564.064487	37708.671738	31.613056
564.244210	37750.170768	31.618074
564.358320	37803.954322	31.623092
565.050913	37845.094971	31.628109
565.298804	37891.958696	31.633127
566.092743	37931.799936	31.638144
566.283785	37995.323020	31.643162
566.580095	38041.534471	31.648180
567.100006	38101.288024	31.653197
567.040516	38153.607240	31.658215
567.769006	38211.001295	31.663232
568.263753	38276.001663	31.668250
568.706986	38340.978676	31.673268
569.577124	38408.367957	31.678285
569.777603	38477.930221	31.683303
570.109108	38546.087264	31.688320
570.300644	38621.083575	31.693338
570.933049	38683.451850	31.698356
571.663845	38756.448035	31.703373
572.013033	38832.185580	31.708391
572.679750	38907.102137	31.713408
573.126642	38981.958521	31.718426
573.735589	39066.788027	31.723444
574.441578	39140.896093	31.728461
575.051632	39233.827154	31.733479
575.794838	39288.907163	31.738496
576.436729	39354.671908	31.743514
577.508061	39429.843105	31.748532
578.035465	39505.593033	31.753549
578.299761	39582.807366	31.758567
578.851909	39647.720644	31.763584
579.265372	39722.477304	31.768602
580.000615	39799.100063	31.773620
580.559207	39871.747516	31.778637
581.239156	39934.434475	31.783655
582.435586	39997.799640	31.788672
582.985339	40067.527316	31.793690
583.548420	40142.812200	31.798708
583.745801	40204.860868	31.803725
584.574176	40274.760598	31.808743
585.205159	40326.331821	31.813760
585.666058	40405.017149	31.818778
586.344985	40474.080806	31.823796
586.899329	40538.515738	31.828813
587.326247	40594.989365	31.833831
587.959493	40665.673516	31.838848
588.546555	40747.565795	31.843866
589.231549	40816.971107	31.848884
589.969442	40866.471396	31.853901
590.181732	40942.952388	31.858919
591.161704	40995.299049	31.863936
591.506141	41057.428296	31.868954
592.264460	41111.188705	31.873972
593.062969	41163.165738	31.878989
593.353895	41228.396583	31.884007
593.913078	41290.069107	31.889024
594.495754	41357.582113	31.894042
594.742132	41413.567503	31.899060
595.422744	41481.476656	31.904077
595.724776	41554.138253	31.909095
596.562643	41626.633949	31.914112
597.045266	41686.839586	31.919130
597.855945	41767.770911	31.924148
598.334383	41841.936428	31.929165
598.582297	41921.489099	31.934183
599.087795	41991.356324	31.939200
599.685029	42070.159091	31.944218
599.920184	42147.747542	31.949236
600.610011	42232.481786	31.954253
601.983688	42295.490622	31.959271
602.726641	42360.742577	31.964288
603.320431	42435.290495	31.969306
603.933005	42508.349349	31.974324
605.205125	42558.920934	31.979341
605.824122	42628.595300	31.984359
606.256518	42693.099920	31.989376
606.957559	42759.751129	31.994394
607.389678	42835.122673	31.999412
608.301422	42889.249228	32.004429
608.658643	42969.256609	32.009447
609.324127	43026.723784	32.014464
609.788598	43099.681282	32.019482
610.110917	43166.608082	32.024500
610.721191	43230.567744	32.029517
611.233693	43316.991115	32.034535
611.912923	43386.930418	32.039552
612.733173	43457.442430	32.044570
613.392603	43526.619917	32.049588
614.105682	43587.288009	32.054605
614.516485	43668.820242	32.059623
615.367767	43741.289146	32.064640
615.757738	43811.660932	32.069658
616.683214	43878.780057	32.074676
617.589286	43931.455205	32.079693
618.252486	44003.005608	32.084711
618.807180	44067.368558	32.089728
619.370810	44136.626199	32.094746
619.997031	44203.546476	32.099764
620.100194	44259.978970	32.104781
620.617706	44332.571651	32.109799
621.536565	44397.511073	32.114816
622.208191	44476.291757	32.119834
622.826769	44541.335555	32.124852
623.895339	44614.412151	32.129869
624.393308	44686.167738	32.134887
625.065108	44756.460411	32.139904
625.540577	44828.979054	32.144922
626.198533	44901.197349	32.149940
626.670677	44955.461036	32.154957
626.944575	45035.963310	32.159975
627.798498	45106.272839	32.164992
628.205543	45193.238700	32.170010
628.390977	45266.405127	32.175028
629.311369	45332.219980	32.180045
629.682699	45407.723601	32.185063
630.241792	45491.706324	32.190080
630.962783	45576.631862	32.195098
631.359001	45666.365652	32.200116
631.948909	45732.973565	32.205133
632.374590	45823.494105	32.210151
633.089723	45894.808357	32.215168
633.676357	45971.412496	32.220186
633.812522	46055.931679	32.225204
634.778147	46127.555369	32.230221
635.021896	46219.415476	32.235239
635.603469	46304.435177	32.240256
636.530465	46395.347630	32.245274
637.197356	46477.697664	32.250292
638.708282	46539.090174	32.255309
640.022289	46609.458869	32.260327
640.994560	46662.699424	32.265344
641.887825	46739.081015	32.270362
642.398867	46794.241359	32.275380
643.047729	46864.151984	32.280397
643.434832	46930.504185	32.285415
644.007329	46991.633686	32.290432
644.841197	47062.262447	32.295450
644.938334	47132.500702	32.300468
645.769947	47195.620916	32.305485
645.987489	47281.504740	32.310503
646.349919	47350.822761	32.315520
647.372877	47429.052642	32.320538
647.674885	47513.114768	32.325556
648.466608	47591.172648	32.330573
648.801708	47674.781013	32.335591
649.819680	47734.659703	32.340608
650.797603	47808.918598	32.345626
651.536351	47890.712104	32.350644
652.316979	47962.212406	32.355661
652.782904	48038.931008	32.360679
653.735342	48110.493441	32.365696
654.517757	48186.169702	32.370714
654.940570	48255.474694	32.375732
655.709343	48326.225127	32.380749
656.164201	48402.756886	32.385767
657.075540	48467.626953	32.390784
657.351077	48539.366330	32.395802
657.799347	48619.202377	32.400820
658.713090	48702.907362	32.405837
659.279407	48785.945812	32.410855
659.726607	48865.782886	32.415872
660.460316	48935.819443	32.420890
661.053236	49021.081612	32.425908
661.811704	49087.578062	32.430925
662.512953	49175.721534	32.435943
662.947712	49262.413931	32.440960
663.854738	49341.990844	32.445978
664.468029	49424.771173	32.450996
665.157850	49506.578117	32.456013
665.600130	49590.271596	32.461031
666.108600	49673.480488	32.466048
667.009470	49754.660525	32.471066
667.400278	49842.494528	32.476084
667.904959	49925.129161	32.481101
668.784414	50015.645902	32.486119
669.199445	50103.590993	32.491136
670.299772	50188.449013	32.496154
670.485517	50281.713854	32.501172
671.603805	50363.317541	32.506189
672.138491	50455.566704	32.511207
672.771290	50535.905661	32.516224
673.601843	50631.045028	32.521242
673.893299	50710.957175	32.526260
674.843341	50800.852191	32.531277
675.521464	50884.652625	32.536295
676.240515	50970.813384	32.541312
677.049960	51051.487124	32.546330
677.456485	51139.298278	32.551348
678.233344	51212.973249	32.556365
678.637301	51293.464562	32.561383
678.774518	51388.424551	32.566400
679.752959	51473.989738	32.571418
680.242026	51563.004443	32.576436
680.993873	51641.183554	32.581453
681.467876	51743.147453	32.586471
682.136983	51833.001872	32.591488
683.044778	51928.419196	32.596506
683.608974	52025.738392	32.601524
684.177704	52111.414375	32.606541
685.207812	52201.549045	32.611559
685.868880	52293.760397	32.616576
687.102013	52372.727158	32.621594
688.058071	52466.626795	32.626612
689.338680	52539.182990	32.631629
689.868200	52613.084627	32.636647
690.501419	52701.733069	32.641664
691.563852	52774.551963	32.646682
691.955245	52853.164921	32.651700
692.988926	52914.756795	32.656717
693.738484	53004.925840	32.661735
693.930671	53090.949130	32.666752
694.729242	53173.334121	32.671770
695.231635	53261.131906	32.676788
696.079295	53337.732345	32.681805
696.238657	53416.794845	32.686823
696.932929	53498.539194	32.691840
697.914102	53583.991440	32.696858
698.211990	53682.491937	32.701876
698.807578	53772.985457	32.706893
699.252656	53870.590409	32.711911
699.744517	53962.720904	32.716928
700.463267	54068.156052	32.721946
700.746202	54178.526322	32.726964
701.475723	54271.880119	32.731981
702.465233	54383.248136	32.736999
703.010046	54500.982982	32.742016
703.520691	54594.239432	32.747034
704.005052	54703.542757	32.752052
705.336140	54807.284228	32.757069
705.895247	54914.925111	32.762087
706.524755	55017.555984	32.767104
707.132574	55124.038409	32.772122
707.715213	55243.068347	32.777140
708.862101	55350.005287	32.782157
709.918088	55447.533716	32.787175
710.297627	55567.128678	32.792192
711.298718	55663.597057	32.797210
711.744389	55769.107835	32.802228
712.494512	55874.204339	32.807245
713.239415	55985.023269	32.812263
714.467267	56061.598288	32.817280
716.162904	56153.188025	32.822298
716.466298	56254.925981	32.827316
717.542201	56335.487486	32.832333
718.192133	56422.280237	32.837351
718.740213	56510.804367	32.842368
719.463545	56587.890441	32.847386
720.184132	56685.944786	32.852404
720.608158	56774.628552	32.857421
721.507470	56860.326907	32.862439
721.707553	56960.280285	32.867456
722.788478	57046.760971	32.872474
723.337255	57145.090924	32.877492
723.852071	57237.002629	32.882509
725.033370	57322.595183	32.887527
725.390884	57406.804395	32.892544
726.293517	57489.776641	32.897562
726.899256	57573.909590	32.902580
727.552207	57668.484855	32.907597
728.423195	57749.443953	32.912615
728.962850	57847.145280	32.917632
729.417677	57930.568918	32.922650
730.250135	58032.307484	32.927668
731.223047	58124.328048	32.932685
731.905367	58218.217304	32.937703
732.136017	58310.785205	32.942720
733.052841	58404.980244	32.947738
733.408563	58514.726152	32.952756
733.889738	58616.389263	32.957773
734.726595	58723.554330	32.962791
735.185344	58830.108159	32.967808
735.926474	58926.744255	32.972826
736.819850	59052.833383	32.977844
737.394476	59164.883531	32.982861
738.153782	59276.329283	32.987879
738.816066	59393.582315	32.992896
739.731858	59504.953969	32.997914
740.153358	59618.555618	33.002932
740.884565	59732.932154	33.007949
741.867136	59851.308217	33.012967
743.112300	59959.832633	33.017984
743.962685	60074.844068	33.023002
744.865391	60183.644646	33.028020
745.718745	60292.731947	33.033037
747.143674	60377.455249	33.038055
747.834914	60469.528778	33.043072
748.740342	60563.468081	33.048090
749.902845	60641.416092	33.053108
750.855550	60738.817456	33.058125
751.697622	60822.817007	33.063143
752.293320	60919.040647	33.068160
752.799570	61006.764806	33.073178
753.660969	61102.846277	33.078196
754.334839	61205.211588	33.083213
755.058719	61285.787672	33.088231
755.460601	61389.272451	33.093248
756.915912	61464.531233	33.098266
757.431800	61563.093040	33.103284
758.284340	61658.025971	33.108301
759.014182	61745.192335	33.113319
759.502794	61835.561892	33.118336
760.181681	61929.655818	33.123354
761.229188	62033.998058	33.128372
761.578717	62139.057746	33.133389
762.263987	62242.324464	33.138407
762.546703	62336.159122	33.143424
763.040334	62439.722543	33.148442
763.844258	62554.999696	33.153460
764.073094	62665.904481	33.158477
765.133925	62771.583454	33.163495
765.511706	62903.546413	33.168512
766.199855	63009.253100	33.173530
766.808250	63137.351218	33.178548
767.729735	63252.239681	33.183565
768.796864	63362.560488	33.188583
769.295414	63492.000720	33.193600
770.177531	63595.811974	33.198618
770.918386	63719.081020	33.203636
771.434072	63847.792376	33.208653
772.466169	63963.743007	33.213671
773.447943	64078.043387	33.218688
774.610624	64192.917387	33.223706
775.131534	64293.147868	33.228724
776.356839	64391.552779	33.233741
777.341357	64497.827098	33.238759
778.218173	64591.684803	33.243776
779.186062	64692.549613	33.248794
779.744387	64789.338507	33.253812
780.492356	64888.573494	33.258829
781.339847	64983.507187	33.263847
781.667566	65093.153669	33.268864
782.314134	65199.610485	33.273882
783.039170	65303.466043	33.278900
783.647379	65412.709114	33.283917
784.846124	65508.463469	33.288935
785.350658	65627.321722	33.293952
786.121029	65741.124588	33.298970
787.022180	65852.172391	33.303988
787.540934	65972.695148	33.309005
788.580044	66090.712107	33.314023
789.185265	66212.849603	33.319040
789.657529	66321.472074	33.324058
790.279568	66439.644598	33.329076
790.703708	66563.698881	33.334093
791.778271	66683.929029	33.339111
792.669001	66816.306967	33.344128
793.337838	66938.494956	33.349146
794.458156	67061.397941	33.354164
795.326689	67189.615137	33.359181
796.071906	67306.094512	33.364199
796.393700	67429.801785	33.369216
797.454434	67557.553841	33.374234
798.349511	67690.321843	33.379252
799.130305	67817.359224	33.384269
800.232637	67949.222331	33.389287
800.852344	68077.723529	33.394304
801.504413	68204.276432	33.399322
802.111149	68338.954482	33.404340
803.074343	68461.078287	33.409357
804.030636	68587.553771	33.414375
804.826317	68725.281554	33.419392
805.976645	68849.790362	33.424410
807.006072	68978.789095	33.429428
807.774281	69108.715859	33.434445
808.852225	69214.222655	33.439463
810.599944	69320.334195	33.444480
811.453806	69426.459495	33.449498
812.487754	69540.890126	33.454516
812.710030	69651.300788	33.459533
813.939196	69762.269789	33.464551
814.869246	69875.135109	33.469568
815.147053	69974.241761	33.474586
816.221268	70078.264568	33.479604
816.837017	70201.039863	33.484621
817.450947	70305.958852	33.489639
818.846225	70420.140459	33.494656
819.130671	70537.371410	33.499674
819.810070	70642.078858	33.504692
820.706960	70762.849718	33.509709
821.880139	70876.257541	33.514727
822.223719	70980.145043	33.519744
822.908881	71105.168070	33.524762
823.842437	71210.255933	33.529780
824.693775	71324.995264	33.534797
825.716738	71447.788619	33.539815
826.439106	71560.776044	33.544832
827.167697	71676.372032	33.549850
828.130304	71793.920347	33.554868
828.608181	71924.641140	33.559885
829.055005	72035.773929	33.564903
830.095860	72154.223508	33.569920
830.542428	72265.015329	33.574938
831.655109	72379.578997	33.579956
832.151900	72506.892643	33.584973
833.004958	72620.852056	33.589991
833.485446	72744.230339	33.595008
834.087093	72873.834504	33.600026
835.251977	73001.856522	33.605044
835.749267	73133.783495	33.610061
836.916963	73261.793658	33.615079
837.574958	73388.807626	33.620096
838.057335	73521.764808	33.625114
839.145194	73652.094591	33.630132
839.810922	73792.041514	33.635149
840.355967	73938.569253	33.640167
841.668314	74069.321907	33.645184
842.305199	74200.750959	33.650202
843.098473	74341.922098	33.655220
843.944763	74490.596999	33.660237
844.830748	74630.412470	33.665255
846.143585	74763.689105	33.670272
846.808149	74903.439331	33.675290
847.414089	75039.171384	33.680308
847.939957	75191.421725	33.685325
849.203042	75333.512518	33.690343
850.217712	75474.895596	33.695360
851.036208	75628.052606	33.700378
852.233126	75752.003891	33.705396
853.109605	75894.145495	33.710413
854.146273	76019.098475	33.715431
855.478290	76151.137544	33.720448
856.692396	76282.917033	33.725466
857.678791	76414.276785	33.730484
858.774879	76541.718370	33.735501
860.342708	76640.863137	33.740519
861.911029	76740.337548	33.745536
862.711407	76846.836492	33.750554
863.527069	76952.877417	33.755572
864.216249	77065.462501	33.760589
864.755639	77163.680769	33.765607
865.455701	77277.303788	33.770624
866.469477	77393.563772	33.775642
867.220478	77504.240779	33.780660
867.296086	77635.052268	33.785677
868.482920	77737.668393	33.790695
869.160956	77864.408841	33.795712
869.853381	77986.891078	33.800730
870.832094	78111.393970	33.805748
872.071636	78229.066328	33.810765
873.241355	78335.867933	33.815783
873.854536	78452.144445	33.820800
874.810073	78580.466299	33.825818
876.978839	78660.344100	33.830836
878.388165	78761.104924	33.835853
878.988115	78847.537893	33.840871
879.792620	78944.644164	33.845888
880.471942	79046.103093	33.850906
881.278729	79145.540762	33.855924
881.920185	79256.077255	33.860941
882.652226	79366.523989	33.865959
883.267931	79472.656596	33.870976
883.600221	79589.057872	33.875994
884.510309	79695.690001	33.881012
884.919270	79810.154499	33.886029
885.529827	79933.481652	33.891047
886.512383	80069.825741	33.896064
886.674984	80193.135496	33.901082
887.725128	80325.074006	33.906100
888.347241	80454.558949	33.911117
888.641815	80584.475859	33.916135
889.435932	80720.510547	33.921152
890.081688	80853.477747	33.926170
891.268228	80990.529212	33.931188
891.821863	81134.838829	33.936205
892.135056	81286.028511	33.941223
892.961906	81431.475156	33.946240
893.790090	81583.295305	33.951258
894.719856	81733.263217	33.956276
896.013844	81894.641287	33.961293
896.600802	82043.308824	33.966311
897.848694	82193.672819	33.971328
898.724806	82355.499050	33.976346
899.957650	82503.725772	33.981364
900.920826	82651.032543	33.986381
901.789858	82799.089703	33.991399
903.011477	82942.708427	33.996416
903.904403	83096.769217	34.001434
905.036929	83239.655823	34.006452
906.391848	83391.593221	34.011469
907.093589	83539.617064	34.016487
907.811648	83688.564088	34.021504
908.630807	83838.357677	34.026522
909.632501	83982.712961	34.031540
910.490636	84129.853735	34.036557
911.020145	84292.429441	34.041575
912.200669	84443.943560	34.046592
913.055888	84597.372085	34.051610
913.689226	84759.224576	34.056628
914.678733	84907.793281	34.061645
915.382625	85071.372451	34.066663
916.326580	85248.258075	34.071680
917.063187	85404.066354	34.076698
918.152011	85571.719016	34.081716
919.285903	85735.285289	34.086733
919.784613	85905.313186	34.091751
921.048830	86062.930485	34.096768
922.064844	86233.855036	34.101786
923.169041	86391.042973	34.106804
924.243169	86559.337220	34.111821
924.368660	86718.669678	34.116839
925.754333	86882.532432	34.121856
926.442579	87057.276767	34.126874
927.634563	87209.310390	34.131892
928.656087	87385.639231	34.136909
929.493027	87552.987860	34.141927
930.948361	87719.581640	34.146944
931.525309	87887.226326	34.151962
932.810643	88044.508800	34.156980
933.545848	88206.706586	34.161997
934.779935	88375.733866	34.167015
935.866637	88529.780415	34.172032
936.521707	88695.668576	34.177050
937.729556	88853.968645	34.182068
938.663090	89010.639651	34.187085
939.432347	89165.018004	34.192103
940.871109	89324.475700	34.197120
941.709290	89476.981902	34.202138
942.404383	89636.012747	34.207156
943.595264	89790.467722	34.212173
944.511917	89949.985156	34.217191
945.935055	90093.442710	34.222208
947.037988	90239.688599	34.227226
948.915897	90359.984806	34.232244
950.504280	90492.278196	34.237261
951.282286	90621.517919	34.242279
952.234982	90740.008739	34.247296
953.042459	90867.546602	34.252314
954.096166	90984.970633	34.257332
954.770012	91099.678982	34.262349
955.321086	91227.157115	34.267367
956.762736	91349.249252	34.272384
956.801396	91474.058366	34.277402
957.848082	91606.428776	34.282420
958.980027	91731.802877	34.287437
960.150689	91863.660699	34.292455
961.112698	91993.739323	34.297472
961.891907	92121.096766	34.302490
962.767483	92246.348358	34.307508
963.879239	92378.597868	34.312525
964.124137	92526.826952	34.317543
965.203930	92667.511342	34.322560
965.928765	92810.279914	34.327578
966.856781	92949.024776	34.332596
968.158702	93096.875645	34.337613
968.560755	93247.086231	34.342631
969.609897	93398.349657	34.347648
970.352160	93547.177566	34.352666
970.990507	93691.700252	34.357684
972.380007	93841.746455	34.362701
973.097234	94013.560616	34.367719
973.964862	94163.854870	34.372736
974.618932	94330.319026	34.377754
975.733863	94499.830075	34.382772
976.438118	94660.178582	34.387789
976.890015	94826.930562	34.392807
978.213423	95009.416883	34.397824
978.630994	95179.421086	34.402842
979.896035	95354.300460	34.407860
980.867174	95538.201334	34.412877
981.927034	95717.665497	34.417895
982.966090	95906.045174	34.422912
983.563588	96084.164112	34.427930
984.129818	96258.980478	34.432948
986.083404	96441.275062	34.437965
986.824221	96630.149436	34.442983
987.977819	96808.984007	34.448000
988.896221	96999.468034	34.453018
989.663170	97188.607855	34.458036
991.254082	97360.024687	34.463053
991.815560	97556.018872	34.468071
993.101208	97723.872612	34.473088
994.367341	97915.283795	34.478106
995.174382	98097.881511	34.483124
996.546836	98275.942133	34.488141
997.587624	98455.868490	34.493159
998.870408	98622.218834	34.498176
999.722202	98802.290819	34.503194
1000.691344	98982.662371	34.508212
1002.027576	99151.048120	34.513229
1002.886058	99327.242742	34.518247
1003.913127	99498.962152	34.523264
1004.958390	99676.054886	34.528282
1006.351995	99851.129027	34.533300
1007.379591	100020.543805	34.538317
1008.011561	100193.165480	34.543335
1009.041026	100372.204179	34.548352
1009.894831	100547.493368	34.553370
1010.751445	100722.339333	34.558388
1012.150037	100897.431006	34.563405
1012.472302	101084.774315	34.568423
1013.606551	101260.036098	34.573440
1014.952097	101454.321057	34.578458
1015.592296	101627.329366	34.583476
1016.239911	101805.738391	34.588493
1017.083527	101988.136749	34.593511
1018.629930	102166.850754	34.598528
1019.431119	102331.254231	34.603546
1020.141840	102511.318078	34.608564
1021.240710	102695.886454	34.613581
1021.729297	102880.335868	34.618599
1022.964519	103056.935334	34.623616
1023.684997	103244.203192	34.628634
1024.799973	103437.496234	34.633652
1026.115769	103609.242655	34.638669
1027.519326	103799.614475	34.643687
1028.629606	103970.494713	34.648704
1029.889450	104154.335929	34.653722
1030.574307	104341.019581	34.658740
1032.235282	104517.674221	34.663757
1032.867888	104703.848212	34.668775
1034.112555	104886.681453	34.673792
1034.965125	105062.539912	34.678810
1036.207388	105253.655272	34.683828
1037.182918	105431.132068	34.688845
1038.334792	105610.636306	34.693863
1039.193613	105792.976938	34.698880
1040.629689	105990.837138	34.703898
1041.274805	106173.149864	34.708916
1042.577689	106365.796261	34.713933
1043.638808	106563.300042	34.718951
1044.458824	106754.426531	34.723968
1045.416329	106939.636235	34.728986
1045.896392	107125.783949	34.734004
1047.351805	107315.216355	34.739021
1048.690628	107519.161837	34.744039
1049.810189	107706.188959	34.749056
1050.768339	107902.651380	34.754074
1051.613336	108096.837425	34.759092
1052.993367	108286.020657	34.764109
1055.428931	108449.094704	34.769127
1057.282272	108602.242781	34.774144
1058.947212	108768.875496	34.779162
1060.227644	108931.346435	34.784180
1061.459947	109073.421862	34.789197
1062.543019	109226.820086	34.794215
1063.749852	109385.424242	34.799232
1064.797270	109528.785896	34.804250
1065.370273	109687.604780	34.809268
1066.541787	109837.238172	34.814285
1067.299068	110000.353946	34.819303
1068.174631	110155.957228	34.824320
1069.292912	110312.639166	34.829338
1070.047792	110484.457053	34.834356
1070.866374	110639.094901	34.839373
1071.780903	110800.756724	34.844391
1073.082173	110962.206555	34.849408
1074.171708	111113.582891	34.854426
1075.129611	111298.752205	34.859444
1075.844134	111454.462480	34.864461
1076.733263	111625.643446	34.869479
1077.491707	111813.218177	34.874496
1078.646701	111987.009788	34.879514
1079.763548	112172.957711	34.884532
1080.912189	112350.442580	34.889549
1081.577296	112533.558863	34.894567
1082.166029	112727.341199	34.899584
1083.119951	112921.853708	34.904602
1083.965153	113113.365854	34.909620
1084.921011	113307.043084	34.914637
1085.944164	113515.118264	34.919655
1086.782626	113710.236473	34.924672
1088.121205	113905.366208	34.929690
1088.727506	114107.980351	34.934708
1089.941953	114295.636054	34.939725
1090.817131	114497.880502	34.944743
1091.324758	114692.041101	34.949760
1092.503874	114895.711385	34.954778
1093.600539	115107.563662	34.959796
1094.709465	115308.685214	34.964813
1095.483250	115522.581687	34.969831
1096.531509	115738.275513	34.974848
1097.835258	115948.958677	34.979866
1098.576583	116168.381253	34.984884
1099.812478	116385.190970	34.989901
1100.931882	116607.207807	34.994919
1102.124304	116822.720447	34.999936
1103.689306	117043.655408	35.004954
1104.633288	117272.933430	35.009972
1106.049640	117475.134705	35.014989
1107.265420	117699.552859	35.020007
1108.215342	117911.824525	35.025024
1109.992526	118126.212969	35.030042
1111.379947	118341.576911	35.035060
1112.893564	118540.990794	35.040077
1114.032689	118741.821580	35.045095
1115.007014	118956.175492	35.050112
1116.370616	119151.214538	35.055130
1117.196304	119358.833117	35.060148
1118.559560	119564.072735	35.065165
1119.166679	119787.672476	35.070183
1120.019756	119992.220475	35.075200
1121.171441	120209.369629	35.080218
1122.189242	120430.308392	35.085236
1123.635325	120648.695097	35.090253
1124.750937	120864.826078	35.095271
1125.699501	121088.620879	35.100288
1127.211352	121307.318107	35.105306
1127.814336	121533.655862	35.110324
1129.179670	121756.869136	35.115341
1130.610794	121969.975759	35.120359
1131.980927	122191.389413	35.125376
1133.395338	122403.511525	35.130394
1134.256302	122617.408610	35.135412
1134.991913	122837.821565	35.140429
1136.337157	123060.842377	35.145447
1137.661953	123273.959976	35.150464
1138.722776	123496.913582	35.155482
1139.665693	123719.239902	35.160500
1140.647028	123938.821247	35.165517
1141.711664	124159.354898	35.170535
1142.918666	124388.912743	35.175552
1143.994288	124608.178508	35.180570
1145.120536	124843.358916	35.185588
1146.857218	125068.422842	35.190605
1147.740173	125303.085799	35.195623
1149.127616	125517.283804	35.200640
1150.530069	125732.064169	35.205658
1151.730170	125956.595357	35.210676
1153.216751	126159.515411	35.215693
1154.099216	126387.042011	35.220711
1154.907681	126597.175015	35.225728
1156.321210	126816.171368	35.230746
1157.045121	127042.521140	35.235764
1158.130328	127260.886142	35.240781
1159.456228	127491.508486	35.245799
1161.374319	127685.284458	35.250816
1163.699079	127876.866201	35.255834
1165.127805	128084.562479	35.260852
1166.402035	128270.448926	35.265869
1167.681282	128451.920172	35.270887
1169.648326	128616.879563	35.275904
1171.312525	128779.755499	35.280922
1172.157998	128947.911408	35.285940
1172.732086	129116.935169	35.290957
1174.036864	129278.879658	35.295975
1174.979514	129452.592266	35.300992
1176.133921	129615.487788	35.306010
1176.858765	129789.311995	35.311028
1177.928585	129960.722952	35.316045
1179.003861	130139.759214	35.321063
1179.781604	130334.461768	35.326080
1180.583967	130517.843576	35.331098
1181.607336	130716.721854	35.336116
1182.579629	130920.405188	35.341133
1182.913348	131111.869146	35.346151
1184.052141	131331.946965	35.351168
1185.039971	131533.879765	35.356186
1186.155471	131757.059351	35.361204
1187.505414	131968.885227	35.366221
1188.734264	132185.540056	35.371239
1189.598291	132421.019567	35.376256
1190.757084	132638.664630	35.381274
1191.727588	132860.679804	35.386292
1192.994193	133102.698101	35.391309
1194.281342	133325.617707	35.396327
1195.229154	133568.069123	35.401344
1196.214335	133801.278391	35.406362
1197.074407	134042.591424	35.411380
1198.399436	134277.704104	35.416397
1199.894551	134525.950135	35.421415
1200.560397	134771.446883	35.426432
1202.033302	135008.570530	35.431450
1203.337049	135273.397593	35.436468
1204.347328	135515.532520	35.441485
1205.716340	135769.210865	35.446503
1206.697820	136029.765638	35.451520
1207.944131	136279.418028	35.456538
1209.229770	136537.897725	35.461556
1210.478272	136795.699437	35.466573
1211.984619	137043.665592	35.471591
1213.067860	137307.587209	35.476608
1214.048473	137559.191632	35.481626
1215.921364	137819.972310	35.486644
1216.904781	138079.358172	35.491661
1218.429927	138332.061716	35.496679
1219.565860	138588.063594	35.501696
1220.870990	138818.507236	35.506714
1222.833844	139065.828918	35.511732
1223.834446	139317.642701	35.516749
1225.078085	139565.993305	35.521767
1226.088420	139828.100369	35.526784
1227.594046	140063.556883	35.531802
1228.857703	140315.448979	35.536820
1229.958428	140559.271115	35.541837
1231.181760	140808.253202	35.546855
1232.180205	141064.048784	35.551872
1233.675197	141308.815579	35.556890
1234.710613	141568.263066	35.561908
1236.162822	141821.935641	35.566925
1237.429420	142066.348570	35.571943
1238.380780	142312.106584	35.576960
1239.756433	142564.678151	35.581978
1240.922913	142829.251822	35.586996
1241.790296	143077.095506	35.592013
1243.082289	143342.337612	35.597031
1244.382991	143600.954714	35.602048
1245.202091	143856.627912	35.607066
1246.698313	144115.102841	35.612084
1247.611383	144370.319733	35.617101
1248.849507	144617.123049	35.622119
1249.538482	144872.796396	35.627136
1251.633093	145126.588332	35.632154
1253.011461	145374.376054	35.637172
1254.067324	145628.510788	35.642189
1255.350765	145874.411966	35.647207
1256.588608	146133.953000	35.652224
1257.225204	146377.228992	35.657242
1258.761730	146642.361240	35.662260
1260.546314	146908.750648	35.667277
1262.185340	147137.023064	35.672295
1263.802199	147388.971674	35.677312
1265.164926	147625.996613	35.682330
1266.615219	147880.131413	35.687348
1267.627622	148123.521724	35.692365
1268.995623	148374.625517	35.697383
1270.235493	148622.120384	35.702400
1271.732751	148869.043007	35.707418
1272.786435	149111.390560	35.712436
1273.842241	149365.886162	35.717453
1275.610453	149619.636795	35.722471
1276.504901	149873.195377	35.727488
1278.012012	150125.085277	35.732506
1278.747464	150379.001138	35.737524
1279.865279	150637.136001	35.742541
1281.634687	150895.944386	35.747559
1282.809406	151155.392904	35.752576
1283.637994	151408.854690	35.757594
1285.024638	151679.392065	35.762612
1286.210919	151943.780298	35.767629
1287.702577	152230.196418	35.772647
1288.661251	152503.711665	35.777664
1289.730240	152768.680692	35.782682
1291.223824	153041.391274	35.787700
1292.294548	153322.318913	35.792717
1293.426807	153599.163518	35.797735
1294.620486	153880.772845	35.802752
1295.774465	154158.606907	35.807770
1297.541369	154438.694807	35.812788
1298.934913	154722.384226	35.817805
1300.873076	154994.526769	35.822823
1302.476502	155272.333925	35.827840
1304.165776	155520.728537	35.832858
1305.920675	155783.179482	35.837876
1307.440592	156048.765865	35.842893
1309.447055	156290.538285	35.847911
1310.519684	156536.418618	35.852928
1311.893784	156783.331834	35.857946
1313.305221	157036.638413	35.862964
1314.443000	157292.375537	35.867981
1315.839428	157528.751602	35.872999
1316.822951	157786.089141	35.878016
1318.296969	158034.591433	35.883034
1319.443089	158295.269865	35.888052
1320.663363	158540.868689	35.893069
1322.032399	158794.620908	35.898087
1323.093251	159043.090422	35.903104
1324.307521	159298.163858	35.908122
1325.727377	159564.581186	35.913140
1326.954909	159821.190836	35.918157
1328.086720	160073.525467	35.923175
1329.591835	160334.613353	35.928192
1331.178915	160586.142446	35.933210
1332.828229	160839.554444	35.938228
1333.746183	161090.695156	35.943245
1335.338726	161343.876839	35.948263
1336.657429	161589.015203	35.953280
1337.222640	161834.716802	35.958298
1338.900377	162080.981553	35.963316
1339.759896	162322.728626	35.968333
1341.571724	162572.491021	35.973351
1342.436965	162821.793138	35.978368
1343.525910	163067.366644	35.983386
1344.755123	163321.730193	35.988404
1345.756869	163593.841433	35.993421
1346.964736	163843.500069	35.998439
1348.244569	164122.146570	36.003456
1349.537934	164394.443975	36.008474
1350.967753	164661.185523	36.013492
1352.240607	164940.052356	36.018509
1353.684620	165209.066503	36.023527
1355.271592	165505.661511	36.028544
1356.955629	165780.633091	36.033562
1358.194899	166052.158436	36.038580
1359.368058	166315.785190	36.043597
1360.628492	166602.367606	36.048615
1361.954527	166880.230965	36.053632
1363.096046	167166.224869	36.058650
1364.681982	167443.072126	36.063668
1365.994678	167721.372595	36.068685
1368.153206	167996.253252	36.073703
1369.796604	168267.800110	36.078720
1371.414882	168528.381686	36.083738
1373.077007	168797.032691	36.088756
1374.489964	169074.598996	36.093773
1375.469164	169336.527839	36.098791
1376.951873	169612.625102	36.103808
1377.924842	169881.870478	36.108826
1379.873154	170154.417844	36.113844
1381.026444	170440.829212	36.118861
1382.618342	170700.470355	36.123879
1383.935453	170984.013945	36.128896
1385.283694	171258.792448	36.133914
1386.673022	171531.635490	36.138932
1388.314819	171809.747594	36.143949
1389.804510	172085.471966	36.148967
1391.119469	172362.646821	36.153984
1392.080408	172641.884327	36.159002
1393.851996	172910.228230	36.164020
1394.811311	173195.766081	36.169037
1396.325103	173466.958468	36.174055
1397.651150	173750.091824	36.179072
1398.898724	174036.222497	36.184090
1399.990965	174322.073758	36.189108
1401.150695	174624.778497	36.194125
1402.813044	174912.955256	36.199143
1404.100103	175196.531561	36.204160
1405.350599	175499.339642	36.209178
1406.822205	175790.393755	36.214196
1408.080869	176100.199500	36.219213
1409.679509	176394.296141	36.224231
1410.515927	176687.294078	36.229248
1412.269138	176985.432082	36.234266
1414.435639	177274.388950	36.239284
1416.434757	177562.153943	36.244301
1418.125296	177841.688750	36.249319
1419.676785	178117.258872	36.254336
1421.195601	178400.835123	36.259354
1422.800999	178678.633548	36.264372
1424.077902	178958.236694	36.269389
1425.614649	179231.044319	36.274407
1426.865206	179510.323167	36.279424
1428.225827	179789.484071	36.284442
1429.421362	180068.417705	36.289460
1430.583711	180352.487755	36.294477
1431.583832	180615.503830	36.299495
1433.053713	180889.317465	36.304512
1434.177539	181171.542037	36.309530
1435.647886	181443.604779	36.314548
1436.214383	181729.296229	36.319565
1437.500448	182023.562132	36.324583
1438.964012	182315.286734	36.329600
1439.929158	182612.982679	36.334618
1441.483146	182915.438502	36.339636
1442.175314	183216.861829	36.344653
1443.926566	183535.086640	36.349671
1445.522438	183835.811663	36.354688
1447.041701	184150.010978	36.359706
1448.550991	184462.612716	36.364724
1450.206308	184783.447248	36.369741
1451.515142	185097.098296	36.374759
1453.288251	185405.445419	36.379776
1454.327261	185719.521600	36.384794
1457.031076	186021.197297	36.389812
1458.579782	186321.149712	36.394829
1460.291871	186689.122556	36.399847
1462.277491	186991.116651	36.404864
1463.767381	187298.777106	36.409882
1465.528839	187593.137302	36.414900
1466.537384	187886.320755	36.419917
1467.677975	188193.276428	36.424935
1469.659378	188485.318621	36.429952
1470.726828	188789.747409	36.434970
1472.412786	189099.338023	36.439988
1473.651620	189403.614648	36.445005
1474.777751	189713.700963	36.450023
1476.043807	190029.582867	36.455040
1477.246123	190346.542421	36.460058
1478.999214	190666.109068	36.465076
1480.280781	190990.728868	36.470093
1481.918497	191310.696317	36.475111
1483.492806	191634.967239	36.480128
1484.662184	191962.248880	36.485146
1486.481167	192283.511356	36.490164
1487.417412	192618.857852	36.495181
1488.984662	192943.971550	36.500199
1490.682529	193270.234083	36.505216
1492.116025	193613.074862	36.510234
1493.328091	193952.623672	36.515252
1495.123984	194280.549886	36.520269
1497.029091	194606.275324	36.525287
1498.438130	194948.945617	36.530304
1499.553054	195281.349888	36.535322
1501.119165	195615.868870	36.540340
1502.355475	195954.098087	36.545357
1503.675413	196300.722927	36.550375
1505.357893	196640.357255	36.555392
1507.028237	196990.485153	36.560410
1508.331167	197325.887636	36.565428
1509.978517	197667.689021	36.570445
1511.354758	198013.166081	36.575463
1513.093823	198352.846336	36.580480
1515.029177	198692.268014	36.585498
1517.247757	199017.675041	36.590516
1518.779321	199350.404444	36.595533
1520.429779	199682.734910	36.600551
1521.994328	200005.655333	36.605568
1523.214985	200335.793631	36.610586
1524.950336	200664.581930	36.615604
1526.209707	200998.043184	36.620621
1527.830097	201331.092963	36.625639
1529.372063	201659.608645	36.630656
1530.422141	201992.215516	36.635674
1532.491749	202305.205173	36.640692
1534.426994	202606.861495	36.645709
1536.340564	202903.568222	36.650727
1538.171584	203198.383157	36.655744
1539.568360	203501.090531	36.660762
1540.994401	203794.064595	36.665780
1542.928483	204081.828255	36.670797
1543.882670	204394.894411	36.675815
1545.755890	204695.674706	36.680832
1546.880959	204992.889141	36.685850
1548.759989	205288.157008	36.690868
1550.064103	205595.505443	36.695885
1551.417639	205905.463099	36.700903
1553.256568	206212.398499	36.705920
1554.737488	206518.425057	36.710938
1555.756991	206826.175456	36.715956
1557.777893	207140.907819	36.720973
1558.927351	207453.820969	36.725991
1560.765557	207759.336053	36.731008
1561.801001	208085.350517	36.736026
1563.353793	208405.771964	36.741044
1564.796207	208735.026033	36.746061
1566.182510	209071.630869	36.751079
1567.721841	209402.648880	36.756096
1568.772247	209730.771646	36.761114
1570.129543	210070.633954	36.766132
1571.727745	210426.869588	36.771149
1573.214069	210785.003046	36.776167
1574.867790	211134.727616	36.781184
1576.497753	211502.645233	36.786202
1577.901165	211848.827937	36.791220
1579.304903	212210.354733	36.796237
1580.866071	212578.233608	36.801255
1582.282761	212933.332092	36.806272
1583.447080	213309.682497	36.811290
1585.123880	213681.228027	36.816308
1586.943695	214050.414426	36.821325
1588.377893	214433.201735	36.826343
1590.052036	214808.864234	36.831360
1592.016200	215185.624874	36.836378
1593.499830	215551.664458	36.841396
1595.431802	215929.421564	36.846413
1596.951462	216309.377446	36.851431
1599.563529	216674.072789	36.856448
1600.613926	217057.456032	36.861466
1602.148086	217426.207427	36.866484
1604.130625	217786.353196	36.871501
1605.905212	218157.887304	36.876519
1607.218959	218534.930219	36.881536
1608.353240	218915.583414	36.886554
1609.895737	219282.912072	36.891572
1611.388768	219658.962237	36.896589
1613.027471	220048.961999	36.901607
1614.882988	220430.239852	36.906624
1616.594055	220812.455028	36.911642
1618.092404	221187.488907	36.916660
1619.529191	221568.223067	36.921677
1621.416873	221960.445638	36.926695
1622.774358	222335.324123	36.931712
1624.590517	222735.941459	36.936730
1626.398681	223115.449360	36.941748
1628.332672	223501.999980	36.946765
1629.300341	223891.013663	36.951783
1630.665132	224265.230880	36.956800
1632.695932	224659.489341	36.961818
1634.370813	225036.274706	36.966836
1636.106172	225424.711090	36.971853
1637.655933	225810.407469	36.976871
1639.240653	226180.627269	36.981888
1640.930042	226561.347948	36.986906
1642.397347	226927.648416	36.991924
1644.031041	227295.015165	36.996941
1645.457280	227665.767651	37.001959
1647.331352	228029.641682	37.006976
1648.950765	228400.185935	37.011994
1650.641545	228768.381742	37.017012
1652.629784	229150.198255	37.022029
1653.856467	229524.182349	37.027047
1655.720327	229897.431480	37.032064
1657.340849	230280.600694	37.037082
1658.359600	230665.413547	37.042100
1660.045127	231052.077963	37.047117
1661.460046	231466.474841	37.052135
1663.421974	231837.675347	37.057152
1664.741490	232236.488630	37.062170
1666.768539	232646.394043	37.067188
1668.486063	233034.017565	37.072205
1670.244525	233429.636616	37.077223
1672.233348	233829.741192	37.082240
1673.582359	234233.197250	37.087258
1674.974374	234632.734033	37.092276
1677.367692	235021.723602	37.097293
1678.908271	235430.864425	37.102311
1680.917268	235824.511458	37.107328
1682.435214	236232.333997	37.112346
1684.043228	236634.985046	37.117364
1686.270371	237027.428100	37.122381
1687.369687	237440.243090	37.127399
1689.616390	237841.598819	37.132416
1691.939608	238231.231034	37.137434
1693.589514	238624.575438	37.142452
1695.579902	239008.263529	37.147469
1697.359508	239401.891463	37.152487
1698.893130	239798.529556	37.157504
1700.466117	240191.198000	37.162522
1702.165257	240595.099826	37.167540
1704.165022	240985.718865	37.172557
1705.678034	241386.981254	37.177575
1707.393058	241782.978327	37.182592
1708.707760	242183.482972	37.187610
1710.224718	242597.241151	37.192628
1711.887170	242991.771085	37.197645
1713.270086	243409.283055	37.202663
1714.681542	243823.741422	37.207680
1716.312946	244229.908625	37.212698
1718.847359	244645.002593	37.217716
1721.019032	245061.575069	37.222733
1722.236913	245468.871516	37.227751
1724.105947	245856.581322	37.232768
1726.680658	246279.438910	37.237786
1728.142945	246682.325350	37.242804
1729.925405	247092.095747	37.247821
1730.979141	247510.260515	37.252839
1732.703847	247920.673181	37.257856
1734.266983	248331.948478	37.262874
1735.534650	248759.120136	37.267892
1737.264362	249172.577401	37.272909
1739.108984	249599.936115	37.277927
1740.980683	250026.324220	37.282944
1742.463403	250446.929607	37.287962
1743.664113	250886.299343	37.292980
1745.625811	251320.747810	37.297997
1746.987953	251752.291470	37.303015
1748.357915	252198.032324	37.308032
1750.515641	252639.355697	37.313050
1751.880560	253074.502210	37.318068
1753.402442	253501.672168	37.323085
1754.837736	253936.982905	37.328103
1756.780391	254378.233061	37.333120
1758.770780	254809.186804	37.338138
1760.521084	255245.892064	37.343156
1762.274736	255680.690309	37.348173
1763.734543	256121.578596	37.353191
1765.665389	256550.351611	37.358208
1767.663897	256992.498934	37.363226
1769.748351	257427.874657	37.368244
1771.394861	257864.968470	37.373261
1773.063942	258312.700116	37.378279
1774.717503	258749.154702	37.383296
1776.361574	259187.336445	37.388314
1777.824609	259649.243509	37.393332
1780.033912	260099.220853	37.398349
1781.997366	260560.385635	37.403367
1783.759547	261012.715436	37.408384
1785.649069	261461.492916	37.413402
1787.230262	261924.515409	37.418420
1789.294510	262386.088800	37.423437
1790.879592	262849.183016	37.428455
1792.354127	263305.206073	37.433472
1794.798717	263751.321996	37.438490
1796.742853	264223.370915	37.443508
1798.885859	264678.927871	37.448525
1800.585774	265145.067404	37.453543
1802.854791	265601.108545	37.458560
1804.499580	266055.695977	37.463578
1806.170576	266511.928165	37.468596
1808.199530	266976.686992	37.473613
1810.271074	267441.462345	37.478631
1811.848238	267892.267492	37.483648
1813.573118	268350.235127	37.488666
1815.749151	268814.073130	37.493684
1817.865508	269258.996615	37.498701
1819.675822	269725.604905	37.503719
1821.711950	270190.169062	37.508736
1823.376943	270637.137528	37.513754
1825.037384	271094.542882	37.518772
1827.170323	271553.649773	37.523789
1828.949292	272009.228643	37.528807
1830.648438	272475.789201	37.533824
1832.743721	272929.510552	37.538842
1834.656632	273386.204077	37.543860
1836.468845	273838.568054	37.548877
1838.154791	274315.253912	37.553895
1839.872026	274775.653011	37.558912
1841.630050	275222.379933	37.563930
1843.369143	275700.954189	37.568948
1844.929524	276166.931754	37.573965
1846.737826	276639.445351	37.578983
1848.358189	277127.324566	37.584000
1850.196704	277595.256494	37.589018
1851.679400	278087.036798	37.594036
1853.906016	278577.783339	37.599053
1855.562942	279050.179040	37.604071
1857.171203	279536.064126	37.609088
1858.837759	280015.207338	37.614106
1860.687596	280509.580948	37.619124
1862.869508	280997.449104	37.624141
1864.389820	281485.138196	37.629159
1866.555785	281973.865718	37.634176
1868.649041	282471.870077	37.639194
1870.490908	282968.132734	37.644212
1872.424216	283468.338996	37.649229
1874.358452	283953.330913	37.654247
1876.409995	284435.076155	37.659264
1878.668501	284900.305573	37.664282
1880.149161	285368.573718	37.669300
1881.918879	285825.188949	37.674317
1883.597833	286299.056802	37.679335
1885.345269	286769.609578	37.684352
1887.782647	287230.605182	37.689370
1889.638492	287698.468208	37.694388
1891.786606	288167.323216	37.699405
1893.383739	288635.093034	37.704423
1895.131264	289097.452941	37.709440
1897.222513	289572.502121	37.714458
1898.699425	290052.925204	37.719476
1900.536982	290520.415036	37.724493
1902.693467	291009.128837	37.729511
1904.223657	291492.071591	37.734528
1906.162959	291981.065597	37.739546
1908.154264	292475.074784	37.744564
1909.777773	292967.385602	37.749581
1911.520523	293466.884395	37.754599
1913.333526	293969.059303	37.759616
1915.337498	294467.747153	37.764634
1917.190861	294983.566521	37.769652
1919.185556	295492.250378	37.774669
1920.661655	296003.676721	37.779687
1922.088566	296516.197922	37.784704
1924.346385	297056.232133	37.789722
1926.291810	297584.047772	37.794740
1928.166956	298105.852611	37.799757
1930.032097	298636.463564	37.804775
1932.618001	299164.976484	37.809792
1935.060880	299686.373011	37.814810
1936.585821	300223.673295	37.819828
1938.681415	300730.846909	37.824845
1940.922021	301249.086816	37.829863
1942.684549	301781.485688	37.834880
1945.091434	302299.029372	37.839898
1947.124132	302833.152427	37.844916
1948.832624	303344.423400	37.849933
1951.178866	303874.856706	37.854951
1953.524843	304400.690013	37.859968
1955.599000	304930.825056	37.864986
1957.613897	305443.271168	37.870004
1959.279819	305962.036527	37.875021
1961.475427	306481.703645	37.880039
1963.068539	307002.119618	37.885056
1965.267563	307534.086177	37.890074
1967.084772	308060.167198	37.895092
1968.972739	308587.094534	37.900109
1970.900876	309114.619085	37.905127
1972.861107	309643.325843	37.910144
1975.206414	310163.742905	37.915162
1977.309154	310692.618902	37.920180
1979.537514	311207.382865	37.925197
1981.474290	311736.907749	37.930215
1983.114528	312274.645618	37.935232
1985.068078	312788.014008	37.940250
1987.160337	313321.659021	37.945268
1989.419712	313845.170621	37.950285
1991.650287	314363.173441	37.955303
1993.588008	314890.225800	37.960320
1995.717801	315407.420397	37.965338
1997.611023	315937.030812	37.970356
1999.392048	316456.145958	37.975373
2001.207950	316982.989887	37.980391
2002.975824	317512.042937	37.985408
2005.047832	318037.743017	37.990426
2006.926166	318572.247555	37.995444
2008.461135	319103.398797	38.000461
2010.650153	319626.270014	38.005479
2011.878806	320147.914849	38.010496
2014.143338	320664.366874	38.015514
2015.650354	321189.254328	38.020532
2017.680177	321710.069601	38.025549
2020.069499	322241.048268	38.030567
2021.591473	322783.295339	38.035584
2023.988202	323299.136227	38.040602
2025.907413	323850.112111	38.045620
2027.347618	324381.186629	38.050637
2029.695556	324925.534689	38.055655
2031.328898	325475.442466	38.060672
2033.198097	326034.008676	38.065690
2035.157210	326591.944169	38.070708
2037.577582	327157.385921	38.075725
2039.736711	327705.734824	38.080743
2041.433931	328276.957043	38.085760
2043.713270	328832.527684	38.090778
2045.771665	329406.366333	38.095796
2047.442416	329983.047909	38.100813
2049.623707	330563.065957	38.105831
2051.675690	331132.998587	38.110848
2053.630249	331714.328628	38.115866
2055.864831	332300.882663	38.120884
2057.570075	332881.498242	38.125901
2059.965258	333472.854332	38.130919
2061.786715	334078.648760	38.135936
2063.969364	334669.308965	38.140954
2066.116068	335266.560696	38.145972
2067.665563	335866.306000	38.150989
2070.223925	336465.300285	38.156007
2072.593399	337065.151374	38.161024
2075.192806	337660.111932	38.166042
2077.784069	338247.632228	38.171060
2079.576346	338836.003500	38.176077
2081.852516	339427.941759	38.181095
2083.669594	340020.474643	38.186112
2085.687677	340614.462581	38.191130
2087.960841	341220.371602	38.196148
2090.341450	341813.166652	38.201165
2092.448359	342405.411146	38.206183
2094.527420	342999.729502	38.211200
2097.239403	343583.616882	38.216218
2100.235265	344166.917373	38.221236
2102.344383	344754.125239	38.226253
2104.808767	345316.567501	38.231271
2106.644323	345898.625098	38.236288
2108.912327	346462.600547	38.241306
2111.063965	347037.716867	38.246324
2113.030841	347619.622649	38.251341
2115.437855	348192.346201	38.256359
2117.352789	348781.263640	38.261376
2119.097193	349355.414580	38.266394
2121.313536	349935.592364	38.271412
2123.141586	350516.581236	38.276429
2125.258794	351093.381642	38.281447
2127.096389	351698.663089	38.286464
2128.869310	352278.335851	38.291482
2131.160090	352873.560164	38.296500
2132.704624	353465.873108	38.301517
2134.598792	354075.081095	38.306535
2136.488907	354670.790712	38.311552
2138.778226	355278.671354	38.316570
2140.715656	355882.032053	38.321588
2142.749383	356505.874545	38.326605
2145.369053	357113.109968	38.331623
2147.292982	357729.770888	38.336640
2149.844415	358321.200407	38.341658
2151.920828	358906.659846	38.346676
2154.362890	359490.935500	38.351693
2156.788906	360054.544147	38.356711
2159.112833	360643.125085	38.361728
2160.935765	361220.468296	38.366746
2163.233432	361798.461125	38.371764
2164.934966	362369.261809	38.376781
2167.242543	362951.792850	38.381799
2169.263913	363558.561235	38.386816
2170.984839	364149.600098	38.391834
2173.350520	364734.747828	38.396852
2175.449346	365333.129270	38.401869
2177.677164	365935.152852	38.406887
2179.392160	366543.427551	38.411904
2181.683734	367140.170199	38.416922
2183.686985	367762.742549	38.421940
2185.540737	368379.471074	38.426957
2187.773620	369002.816592	38.431975
2189.592427	369639.288171	38.436992
2191.718407	370266.930132	38.442010
2194.020300	370898.812643	38.447028
2196.337612	371541.497531	38.452045
2198.580383	372192.134987	38.457063
2200.314631	372842.912688	38.462080
2202.420191	373490.880659	38.467098
2205.058135	374149.162739	38.472116
2207.334727	374804.293313	38.477133
2209.825302	375452.534460	38.482151
2211.937448	376113.561888	38.487168
2214.004104	376765.131126	38.492186
2216.357812	377422.212658	38.497204
2218.562390	378092.600309	38.502221
2221.195681	378749.428019	38.507239
2223.357108	379415.280088	38.512256
2226.067063	380079.205786	38.517274
2228.063720	380741.174617	38.522292
2229.991401	381407.721852	38.527309
2232.680087	382073.677049	38.532327
2234.899383	382741.056185	38.537344
2237.183488	383413.169223	38.542362
2239.338699	384083.208121	38.547380
2241.402894	384762.917786	38.552397
2243.826617	385428.903300	38.557415
2246.235605	386107.965872	38.562432
2248.286436	386788.585557	38.567450
2250.477668	387461.390928	38.572468
2252.247989	388150.323178	38.577485
2254.729853	388829.452525	38.582503
2257.073292	389505.622472	38.587520
2259.494894	390193.636461	38.592538
2262.003636	390874.680249	38.597556
2264.083745	391557.797578	38.602573
2266.434630	392248.803026	38.607591
2268.733468	392942.581764	38.612608
2270.860051	393623.912165	38.617626
2273.635288	394308.716558	38.622644
2275.839564	395010.703206	38.627661
2278.247295	395691.475211	38.632679
2280.373090	396378.093794	38.637696
2282.458883	397073.709853	38.642714
2284.760938	397764.968628	38.647732
2287.143737	398455.131382	38.652749
2289.055393	399144.740036	38.657767
2291.474776	399848.523219	38.662784
2293.402231	400544.769493	38.667802
2296.013568	401230.511689	38.672820
2297.849298	401933.512834	38.677837
2300.360317	402621.557424	38.682855
2302.895880	403295.254617	38.687872
2304.745824	403978.654849	38.692890
2306.915310	404647.055227	38.697908
2309.123406	405342.301636	38.702925
2311.382817	406025.120401	38.707943
2313.503991	406702.778463	38.712960
2315.462356	407411.409510	38.717978
2317.618220	408100.404931	38.722996
2319.946503	408803.468855	38.728013
2321.742955	409505.834607	38.733031
2324.475153	410221.186229	38.738048
2326.489218	410930.504999	38.743066
2329.618602	411631.784505	38.748084
2332.452420	412335.718269	38.753101
2334.700263	413047.511392	38.758119
2336.897295	413763.032365	38.763136
2338.843909	414487.066937	38.768154
2341.849577	415201.300497	38.773172
2343.586834	415927.190530	38.778189
2345.998252	416654.568828	38.783207
2348.309139	417392.356898	38.788224
2350.732926	418122.009234	38.793242
2353.285674	418853.891857	38.798260
2355.861280	419593.887471	38.803277
2358.477428	420320.499678	38.808295
2360.581629	421055.864391	38.813312
2362.923569	421796.980974	38.818330
2365.801445	422524.890532	38.823348
2368.144847	423262.363816	38.828365
2370.366812	423990.475486	38.833383
2372.871366	424730.044591	38.838400
2375.419429	425481.511633	38.843418
2377.890830	426215.571285	38.848436
2380.219796	426956.249056	38.853453
2382.145300	427694.940437	38.858471
2384.916264	428434.432691	38.863488
2387.268067	429191.200165	38.868506
2389.399604	429942.008634	38.873524
2391.768703	430706.802882	38.878541
2393.846046	431455.995208	38.883559
2395.745586	432223.533099	38.888576
2398.352855	432989.969847	38.893594
2401.170244	433765.490705	38.898612
2403.705614	434530.210103	38.903629
2406.266273	435291.256839	38.908647
2408.575192	436071.969376	38.913664
2411.172061	436845.733093	38.918682
2413.742729	437612.143105	38.923700
2415.900480	438391.874825	38.928717
2418.584583	439162.246426	38.933735
2420.925624	439933.701147	38.938752
2423.826397	440689.780002	38.943770
2426.520122	441456.772291	38.948788
2429.002700	442212.501318	38.953805
2431.564030	442978.188767	38.958823
2434.300527	443734.472731	38.963840
2436.478565	444506.268590	38.968858
2439.349691	445256.256480	38.973876
2442.075823	445997.095085	38.978893
2444.519658	446750.977326	38.983911
2447.444397	447502.430105	38.988928
2449.587643	448246.146791	38.993946
2452.324854	448993.779628	38.998964
2454.497206	449742.732113	39.003981
2457.325995	450485.188717	39.008999
2460.241265	451223.056903	39.014016
2461.890166	451964.323810	39.019034
2464.180318	452691.323586	39.024052
2466.502950	453423.690143	39.029069
2468.650672	454142.474214	39.034087
2470.844049	454863.695250	39.039104
2473.513913	455581.026307	39.044122
2475.726476	456298.702292	39.049140
2477.764683	457026.823878	39.054157
2479.979674	457761.448485	39.059175
2482.287477	458497.894733	39.064192
2484.724538	459259.573006	39.069210
2487.015907	460005.596425	39.074228
2489.212570	460759.777023	39.079245
2491.321551	461523.676765	39.084263
2493.613567	462299.825215	39.089280
2495.998886	463081.170894	39.094298
2499.002289	463861.879264	39.099316
2500.816939	464647.277924	39.104333
2503.256067	465438.343711	39.109351
2505.982792	466233.867230	39.114368
2508.404539	467039.892690	39.119386
2511.124202	467833.222279	39.124404
2513.722209	468646.960420	39.129421
2515.723979	469460.196911	39.134439
2517.832580	470277.612898	39.139456
2520.389026	471116.552877	39.144474
2522.449867	471932.431199	39.149492
2525.279876	472782.336897	39.154509
2527.666902	473629.746207	39.159527
2530.155664	474471.599377	39.164544
2532.769478	475329.825139	39.169562
2535.473733	476174.731747	39.174580
2538.960260	477030.209183	39.179597
2541.697897	477855.411259	39.184615
2544.534936	478698.852649	39.189632
2546.934842	479543.627978	39.194650
2549.882069	480380.359426	39.199668
2553.149228	481229.948808	39.204685
2555.582917	482069.896019	39.209703
2558.139991	482906.150426	39.214720
2560.534342	483758.963888	39.219738
2563.329252	484597.911908	39.224756
2565.319817	485443.490269	39.229773
2568.011883	486303.422637	39.234791
2570.609243	487150.625999	39.239808
2572.561231	488009.318916	39.244826
2575.395857	488867.321704	39.249844
2578.463189	489721.764046	39.254861
2581.131548	490586.143117	39.259879
2583.929464	491438.868401	39.264896
2586.185203	492297.119656	39.269914
2588.960585	493161.233309	39.274932
2591.148652	494036.920518	39.279949
2593.960114	494900.222804	39.284967
2596.630323	495756.196107	39.289984
2599.126683	496624.885078	39.295002
2601.689735	497484.400022	39.300020
2603.953301	498363.091803	39.305037
2606.614160	499234.621302	39.310055
2609.497303	500093.983391	39.315072
2611.941295	500970.577258	39.320090
2614.833849	501836.478722	39.325108
2617.854338	502713.128570	39.330125
2620.205955	503574.178988	39.335143
2623.129772	504428.194345	39.340160
2625.630032	505302.050187	39.345178
2628.357859	506171.439547	39.350196
2631.535347	507044.529113	39.355213
2633.727341	507910.927382	39.360231
2636.219258	508760.121785	39.365248
2638.616362	509615.819137	39.370266
2641.374180	510450.835492	39.375284
2643.857331	511283.933729	39.380301
2646.146547	512120.331930	39.385319
2648.868081	512953.494240	39.390336
2651.373302	513792.171941	39.395354
2654.609256	514631.690182	39.400372
2657.083289	515481.684657	39.405389
2658.732596	516339.196701	39.410407
2661.411700	517183.824767	39.415424
2663.673032	518066.069211	39.420442
2666.357896	518936.678793	39.425460
2669.256509	519818.408251	39.430477
2671.450875	520689.786174	39.435495
2674.191627	521568.711947	39.440512
2676.705732	522463.345648	39.445530
2679.753702	523352.408943	39.450548
2682.232145	524256.878227	39.455565
2684.934328	525170.747447	39.460583
2687.314565	526065.964450	39.465600
2689.680132	526982.775916	39.470618
2692.362296	527904.799058	39.475636
2695.414189	528823.937024	39.480653
2697.931231	529767.203464	39.485671
2700.790867	530691.514239	39.490688
2703.054197	531634.283585	39.495706
2705.684403	532579.889898	39.500724
2708.615499	533523.974100	39.505741
2710.963133	534493.787641	39.510759
2714.267529	535446.258322	39.515776
2716.622768	536408.847006	39.520794
2719.263573	537360.626321	39.525812
2722.614470	538336.818624	39.530829
2724.969807	539301.196404	39.535847
2727.932409	540258.530141	39.540864
2730.629813	541241.676760	39.545882
2733.025449	542222.987229	39.550900
2735.973999	543196.557964	39.555917
2738.426454	544179.060784	39.560935
2741.616291	545161.069728	39.565952
2744.150778	546143.003082	39.570970
2747.290964	547126.368824	39.575988
2750.013845	548100.041447	39.581005
2753.211333	549096.732417	39.586023
2755.975550	550077.413160	39.591040
2758.614806	551062.246650	39.596058
2761.606902	552057.374104	39.601076
2764.683101	553037.316214	39.606093
2767.143560	554033.367084	39.611111
2770.158827	555017.218523	39.616128
2773.457565	556006.809348	39.621146
2775.768533	556993.666223	39.626164
2778.663304	557967.721476	39.631181
2781.530873	558962.396631	39.636199
2784.382799	559952.832040	39.641216
2787.074976	560950.925083	39.646234
2789.948290	561940.488941	39.651252
2792.810698	562926.765197	39.656269
2795.470317	563916.396146	39.661287
2798.268067	564893.150047	39.666304
2800.995890	565886.459593	39.671322
2804.081859	566875.271483	39.676340
2806.847392	567866.352250	39.681357
2809.712546	568864.241563	39.686375
2813.020013	569847.506851	39.691392
2814.982583	570837.956373	39.696410
2817.963570	571834.767981	39.701428
2820.784214	572811.697594	39.706445
2823.437613	573779.060608	39.711463
2826.402459	574731.980371	39.716480
2828.661339	575693.336369	39.721498
2831.623590	576649.897234	39.726516
2834.554334	577606.131344	39.731533
2837.032296	578577.161804	39.736551
2839.773445	579546.866122	39.741568
2842.472052	580520.043686	39.746586
2845.265160	581492.921042	39.751604
2848.827293	582458.491565	39.756621
2851.925951	583436.750651	39.761639
2854.718035	584415.470610	39.766656
2857.503016	585384.155562	39.771674
2860.237763	586361.260692	39.776692
2863.514093	587349.690014	39.781709
2866.096134	588331.640570	39.786727
2868.943354	589312.711040	39.791744
2871.460707	590314.681863	39.796762
2874.256102	591315.266856	39.801780
2876.802822	592311.700660	39.806797
2879.749060	593337.653719	39.811815
2882.782491	594345.811496	39.816832
2885.321501	595364.889586	39.821850
2888.807575	596396.457090	39.826868
2891.891427	597407.562387	39.831885
2894.686029	598431.298971	39.836903
2897.266926	599464.355808	39.841920
2899.968105	600496.892702	39.846938
2902.582051	601537.927197	39.851956
2905.834130	602580.005786	39.856973
2908.509674	603632.800273	39.861991
2911.831823	604681.045138	39.867008
2914.730737	605741.175410	39.872026
2917.453872	606792.991757	39.877044
2920.339001	607856.548300	39.882061
2923.426673	608923.803635	39.887079
2926.240169	609990.840618	39.892096
2928.875586	611064.576151	39.897114
2931.303131	612148.054282	39.902132
2934.085304	613231.061753	39.907149
2937.631985	614319.118092	39.912167
2940.665092	615414.415122	39.917184
2943.734745	616508.041549	39.922202
2946.822949	617596.860465	39.927220
2949.494757	618697.635482	39.932237
2952.528843	619787.070274	39.937255
2955.517878	620888.449409	39.942272
2958.558475	621985.961293	39.947290
2961.207353	623086.898865	39.952308
2964.686468	624192.962171	39.957325
2967.514628	625292.129703	39.962343
2970.275818	626398.354309	39.967360
2973.454064	627505.533008	39.972378
2976.267474	628628.423679	39.977396
2979.734484	629734.107473	39.982413
2982.678474	630843.080882	39.987431
2985.438068	631950.412349	39.992448
2988.632413	633077.302746	39.997466
2991.791625	634191.079685	40.002484
2995.464472	635291.960040	40.007501
2998.417546	636398.993382	40.012519
3001.323300	637511.176776	40.017536
3004.659253	638597.301468	40.022554
3007.515077	639702.569958	40.027572
3010.452238	640797.502946	40.032589
3013.563045	641912.365050	40.037607
3016.672847	642997.169790	40.042624
3020.030878	644069.333869	40.047642
3022.658693	645145.712354	40.052660
3025.786125	646199.079314	40.057677
3028.860256	647259.985792	40.062695
3031.671470	648304.814164	40.067712
3034.792416	649355.833318	40.072730
3037.411519	650424.889329	40.077748
3040.115741	651475.183363	40.082765
3042.860998	652554.001500	40.087783
3045.982571	653633.774433	40.092800
3048.865332	654713.604716	40.097818
3051.180090	655818.412354	40.102836
3054.407613	656900.656600	40.107853
3056.997950	658009.618509	40.112871
3059.809662	659121.435126	40.117888
3062.916874	660243.634693	40.122906
3065.417086	661379.975310	40.127924
3068.710239	662502.951581	40.132941
3071.660147	663657.282025	40.137959
3074.359433	664812.591430	40.142976
3077.158119	665968.477159	40.147994
3080.230534	667140.924040	40.153012
3083.512517	668309.463178	40.158029
3086.507020	669491.767809	40.163047
3089.552862	670674.200799	40.168064
3093.143972	671865.404849	40.173082
3096.013426	673060.570205	40.178100
3099.345749	674239.596685	40.183117
3102.649629	675452.144407	40.188135
3105.775364	676648.602532	40.193152
3109.080067	677849.321097	40.198170
3111.405900	679062.597871	40.203188
3114.948545	680269.867901	40.208205
3118.241968	681476.113627	40.213223
3121.441734	682693.978878	40.218240
3124.917031	683911.030831	40.223258
3128.169777	685125.912487	40.228276
3131.456975	686339.919591	40.233293
3134.673822	687561.574868	40.238311
3137.503212	688793.099732	40.243328
3141.373127	690005.935848	40.248346
3144.154642	691235.077307	40.253364
3147.314580	692443.958071	40.258381
3150.590088	693678.637519	40.263399
3153.473171	694917.392048	40.268416
3157.124511	696149.366344	40.273434
3160.076357	697393.612691	40.278452
3163.362557	698609.167379	40.283469
3166.623073	699839.654324	40.288487
3169.943774	701075.276512	40.293504
3173.139334	702302.730837	40.298522
3176.032956	703543.865047	40.303540
3179.302380	704783.168482	40.308557
3182.373923	706023.938432	40.313575
3185.640441	707276.275501	40.318592
3188.791530	708510.575640	40.323610
3191.868907	709761.808735	40.328628
3195.705467	711002.960329	40.333645
3199.257173	712239.276211	40.338663
3202.420220	713471.957459	40.343680
3205.654789	714704.531431	40.348698
3208.734585	715948.959169	40.353716
3212.391406	717175.900528	40.358733
3215.595881	718416.808161	40.363751
3218.298707	719644.836770	40.368768
3221.223777	720888.296250	40.373786
3224.057267	722136.492741	40.378804
3228.144444	723381.286280	40.383821
3231.219975	724602.012361	40.388839
3234.108139	725810.021098	40.393856
3237.618208	727010.210979	40.398874
3240.542430	728198.591685	40.403892
3242.930561	729400.151688	40.408909
3246.686219	730607.749528	40.413927
3249.541896	731821.195158	40.418944
3252.981392	733020.338863	40.423962
3256.124972	734238.313146	40.428980
3259.446452	735449.031006	40.433997
3262.649214	736665.614959	40.439015
3265.919988	737895.255798	40.444032
3269.609132	739115.831856	40.449050
3272.538547	740348.997852	40.454068
3275.753206	741590.212347	40.459085
3278.937698	742823.069390	40.464103
3281.708633	744074.734506	40.469120
3285.335034	745323.056141	40.474138
3288.360905	746586.913624	40.479156
3291.659619	747851.440059	40.484173
3294.883287	749116.345352	40.489191
3298.461363	750387.840521	40.494208
3302.031500	751662.299555	40.499226
3305.264935	752948.156963	40.504244
3308.317534	754225.525050	40.509261
3311.893357	755515.180001	40.514279
3315.004584	756806.241418	40.519296
3318.545993	758089.208648	40.524314
3321.639041	759400.330354	40.529332
3324.947283	760692.462274	40.534349
3328.928878	761986.895456	40.539367
3331.949347	763299.797118	40.544384
3335.392246	764599.265288	40.549402
3338.809631	765911.563408	40.554420
3342.626033	767220.712349	40.559437
3345.814504	768520.561882	40.564455
3349.129666	769826.848439	40.569472
3353.237841	771135.941918	40.574490
3356.332394	772450.616245	40.579508
3359.948002	773758.649297	40.584525
3363.422190	775064.693655	40.589543
3366.695573	776381.172566	40.594560
3370.281516	777684.495964	40.599578
3373.572931	779008.767522	40.604596
3377.292871	780313.711642	40.609613
3380.435078	781625.524776	40.614631
3383.749393	782941.887845	40.619648
3387.555135	784244.783516	40.624666
3390.887573	785561.798404	40.629684
3393.778926	786878.133250	40.634701
3397.432780	788199.356313	40.639719
3400.632310	789523.702976	40.644736
3403.813874	790841.397863	40.649754
3407.300747	792169.263451	40.654772
3411.019548	793499.797211	40.659789
3414.731773	794811.394818	40.664807
3418.125693	796133.839167	40.669824
3422.212054	797443.726823	40.674842
3425.606290	798768.459652	40.679860
3428.402167	800082.593211	40.684877
3432.395547	801409.806657	40.689895
3435.204189	802723.934319	40.694912
3438.732002	804043.617497	40.699930
3442.024918	805362.432309	40.704948
3445.341798	806692.743041	40.709965
3448.619729	808017.382704	40.714983
3451.650888	809361.380601	40.720000
3455.109121	810688.399191	40.725018
3458.054004	812020.280106	40.730023
3461.279687	813308.366086	40.735028
3464.994989	814547.497756	40.740032
3467.866778	815735.866389	40.745037
3471.066924	816855.982671	40.750042
3474.003665	817942.638594	40.755047
3476.878562	818949.382777	40.760052
3479.933717	819894.710091	40.765056
3482.135054	820781.729709	40.770061
3484.769392	821609.778831	40.775066
3487.092000	822394.273228	40.780071
3489.216358	823102.328724	40.785076
3491.172880	823768.402815	40.790080
3493.259095	824385.848424	40.795085
3495.094883	824941.998805	40.800090
3496.589425	825454.973268	40.805095
3497.999835	825922.894842	40.810100
3500.171913	826361.782696	40.815104
3501.632942	826748.635548	40.820109
3503.169460	827077.215245	40.825114
3504.058533	827375.157267	40.830119
3505.178192	827636.009894	40.835124
3506.571382	827865.701058	40.840128
3507.295195	828068.367204	40.845133
3508.587959	828234.874582	40.850138
3509.540864	828370.228379	40.855143
3510.039930	828487.279083	40.860148
3510.729543	828576.498645	40.865152
3511.527501	828642.275088	40.870157
3512.243752	828682.597723	40.875162
3512.783074	828707.784913	40.880167
3513.041790	828710.077242	40.885172
3513.537642	828690.171388	40.890176
3513.817790	828664.467283	40.895181
3514.525612	828624.602364	40.900186
3514.846625	828571.384073	40.905191
3515.309311	828495.398144	40.910196
3515.517231	828418.284663	40.915200
3515.670113	828314.836570	40.920205
3516.290120	828206.647823	40.925210
3516.159430	828092.353220	40.930215
3516.516804	827971.661560	40.935220
3516.973491	827826.357438	40.940224
3516.438940	827692.578846	40.945229
3516.650240	827537.001489	40.950234
3517.034596	827380.712575	40.955239
3517.039666	827225.742823	40.960244
3516.717586	827056.139444	40.965248
3516.993804	826893.146467	40.970253
3517.000784	826716.870791	40.975258
3517.231586	826541.527357	40.980263
3517.250720	826355.807809	40.985268
3517.187460	826169.609300	40.990272
3516.595526	825982.709827	40.995277
3517.248628	825789.969841	41.000282
3516.900875	825606.132493	41.005287
3517.103956	825422.398010	41.010292
3516.797078	825218.898070	41.015296
3516.780284	825026.336001	41.020301
3516.978476	824825.272686	41.025306
3516.412761	824620.917987	41.030311
3516.565631	824421.307442	41.035316
3516.737114	824217.699450	41.040320
3516.185975	824030.539417	41.045325
3516.202048	823829.082807	41.050330
3516.276188	823615.547944	41.055335
3515.989404	823416.459824	41.060340
3515.943054	823221.802779	41.065344
3515.648653	823018.714268	41.070349
3515.307763	822814.166939	41.075354
3515.736990	822624.962265	41.080359
3515.765573	822422.095442	41.085364
3515.667454	822223.425678	41.090368
3515.594111	822030.291954	41.095373
3515.232447	821823.574257	41.100378
3515.178257	821624.489076	41.105383
3514.850600	821429.332751	41.110388
3514.944640	821229.335819	41.115392
3514.726247	821037.750733	41.120397
3514.525400	820840.804211	41.125402
3514.792444	820646.308735	41.130407
3514.532953	820463.471561	41.135412
3514.362583	820258.910083	41.140416
3513.872829	820068.797332	41.145421
3513.689368	819896.540987	41.150426
3513.674025	819700.210475	41.155431
3513.281722	819524.180121	41.160436
3513.668824	819336.146680	41.165440
3513.317138	819162.825400	41.170445
3513.364166	818984.277295	41.175450
3513.562387	818800.637967	41.180455
3513.125745	818623.225972	41.185460
3513.559444	818439.928586	41.190464
3513.057768	818253.559017	41.195469
3513.076139	818081.610113	41.200474
3512.903444	817909.686316	41.205479
3512.963712	817724.770928	41.210484
3512.972529	817545.700551	41.215488
3512.408576	817369.343736	41.220493
3512.404376	817191.823235	41.225498
3512.190925	817028.840395	41.230503
3512.105886	816856.484235	41.235508
3511.971673	816694.161939	41.240512
3511.904549	816535.817925	41.245517
3511.624497	816377.503171	41.250522
3511.746802	816211.037690	41.255527
3511.395103	816049.998745	41.260532
3511.567618	815904.652531	41.265536
3511.144509	815743.909042	41.270541
3511.436562	815578.081952	41.275546
3511.226566	815428.303797	41.280551
3510.699646	815268.830594	41.285556
3511.253544	815110.061074	41.290560
3510.520865	814970.387119	41.295565
3510.460560	814815.018215	41.300570
3510.595727	814672.669097	41.305575
3510.326566	814527.554718	41.310580
3510.596793	814381.768112	41.315584
3510.022451	814240.202029	41.320589
3509.956353	814100.794143	41.325594
3510.107364	813958.231439	41.330599
3509.617156	813825.898717	41.335604
3510.326012	813685.093814	41.340608
3509.870112	813547.098623	41.345613
3509.527797	813407.523611	41.350618
3509.640764	813274.597758	41.355623
3509.780706	813134.064303	41.360628
3509.548745	813009.859204	41.365632
3509.282504	812876.399521	41.370637
3509.119789	812741.361626	41.375642
3508.863450	812615.203537	41.380647
3508.564549	812494.604401	41.385652
3509.049710	812382.358966	41.390656
3508.720556	812254.938108	41.395661
3508.936370	812127.039640	41.400666
3508.695525	812006.616978	41.405671
3508.178353	811892.375346	41.410676
3508.481551	811772.447929	41.415680
3508.113351	811642.681616	41.420685
3508.077149	811539.664481	41.425690
3508.016090	811427.779807	41.430695
3507.973584	811319.009331	41.435700
3507.852241	811206.155428	41.440704
3507.704602	811103.051095	41.445709
3507.784185	810990.551819	41.450714
3507.620335	810879.648240	41.455719
3507.459330	810782.291959	41.460724
3507.653062	810678.444957	41.465728
3507.193249	810580.644863	41.470733
3507.142194	810475.857962	41.475738
3507.490162	810374.808901	41.480743
3507.040532	810261.891921	41.485748
3506.896375	810172.810048	41.490752
3506.817170	810083.229312	41.495757
3506.655299	809984.983443	41.500762
3506.562385	809901.836746	41.505767
3506.765527	809809.770660	41.510772
3506.993732	809720.039223	41.515776
3506.767008	809623.845291	41.520781
3506.579624	809532.908693	41.525786
3506.341135	809442.758778	41.530791
3506.237945	809348.686354	41.535796
3506.297482	809262.289847	41.540800
3506.444981	809183.581263	41.545805
3506.315323	809086.486438	41.550810
3506.319029	809008.578201	41.555815
3506.385847	808925.978740	41.560820
3506.242245	808831.417398	41.565824
3505.833579	808760.737539	41.570829
3505.802151	808677.028811	41.575834
3505.832836	808590.627645	41.580839
3505.998027	808508.884986	41.585844
3505.827338	808431.777030	41.590848
3505.638980	808360.278131	41.595853
3505.564793	808270.280856	41.600858
3505.645835	808208.197411	41.605863
3505.356903	808134.127416	41.610868
3505.598256	808058.315791	41.615872
3505.092723	807991.640875	41.620877
3505.365225	807911.239052	41.625882
3505.467444	807839.152468	41.630887
3505.395702	807767.872468	41.635892
3505.416967	807695.065455	41.640896
3504.885161	807625.855085	41.645901
3505.048608	807557.217983	41.650906
3504.994786	807489.443111	41.655911
3505.087699	807432.470565	41.660916
3505.145312	807355.167528	41.665920
3504.794186	807290.948182	41.670925
3504.858118	807223.737267	41.675930
3504.795701	807155.667572	41.680935
3504.644579	807088.391306	41.685940
3504.787328	807022.677761	41.690944
3504.259917	806981.404141	41.695949
3504.277888	806918.683942	41.700954
3504.442962	806863.401949	41.705959
3503.839707	806805.947369	41.710964
3504.036495	806754.561109	41.715968
3504.309597	806704.430558	41.720973
3504.323342	806642.293548	41.725978
3504.144570	806592.720470	41.730983
3504.268822	806546.513712	41.735988
3503.979302	806480.618274	41.740992
3504.090176	806432.315539	41.745997
3504.113452	806377.344128	41.751002
3503.889688	806332.946075	41.756007
3503.610214	806284.556915	41.761012
3503.830996	806224.529536	41.766016
3503.702128	806180.944762	41.771021
3503.788466	806134.497062	41.776026
3503.638960	806087.598131	41.781031
3503.620537	806031.215745	41.786036
3503.888017	805987.957903	41.791040
3503.844678	805941.187627	41.796045
3503.466448	805904.078512	41.801050
3503.719921	805856.480778	41.806055
3503.688330	805814.195285	41.811060
3503.849046	805765.879704	41.816064
3503.621172	805725.331549	41.821069
3503.482821	805676.232799	41.826074
3503.414023	805632.293424	41.831079
3503.471908	805592.041207	41.836084
3503.549615	805539.249142	41.841088
3503.408441	805504.539648	41.846093
3503.162258	805462.139022	41.851098
3503.362759	805414.692613	41.856103
3503.470576	805377.748354	41.861108
3503.235222	805337.296461	41.866112
3503.530742	805300.907796	41.871117
3503.661639	805250.153868	41.876122
3503.270810	805199.773788	41.881127
3503.402489	805157.946246	41.886132
3503.514048	805120.512082	41.891136
3502.962889	805081.278732	41.896141
3503.230990	805043.770863	41.901146
3503.205737	805002.796163	41.906151
3503.046805	804970.379398	41.911156
3503.474660	804929.870030	41.916160
3503.148726	804893.966472	41.921165
3502.757582	804855.584849	41.926170
3503.376742	804823.289630	41.931175
3503.220333	804781.455870	41.936180
3503.096132	804739.031365	41.941184
3502.848055	804709.164094	41.946189
3502.659151	804665.871059	41.951194
3503.024755	804636.200237	41.956199
3502.890314	804611.632536	41.961204
3503.083566	804569.937879	41.966208
3503.217311	804539.717402	41.971213
3502.956589	804494.922012	41.976218
3503.088014	804458.846932	41.981223
3502.899540	804430.432692	41.986228
3503.070362	804394.253512	41.991232
3503.008874	804353.182729	41.996237
3502.716432	804329.858374	42.001242
3503.053661	804280.869696	42.006247
3502.842714	804255.434367	42.011252
3502.540175	804218.206016	42.016256
3502.975442	804187.351257	42.021261
3503.022018	804155.727666	42.026266
3503.249340	804118.464697	42.031271
3502.969051	804080.451409	42.036276
3502.935667	804049.620454	42.041280
3502.969487	804009.410812	42.046285
3502.600485	803976.582709	42.051290
3502.633718	803948.912343	42.056295
3502.319694	803911.049696	42.061300
3502.665287	803880.305061	42.066304
3502.679648	803863.274109	42.071309
3502.520112	803831.193203	42.076314
3502.487924	803808.460571	42.081319
3502.518494	803777.374339	42.086324
3502.562651	803752.336271	42.091328
3502.314718	803724.806475	42.096333
3502.123648	803696.340580	42.101338
3502.396953	803678.146389	42.106343
3502.207853	803648.362523	42.111348
3502.397255	803623.984373	42.116352
3501.977075	803604.336944	42.121357
3502.024132	803585.738704	42.126362
3502.236287	803563.942908	42.131367
3502.370023	803538.109275	42.136372
3502.668969	803513.225625	42.141376
3502.079178	803483.942790	42.146381
3501.845058	803460.264569	42.151386
3502.052790	803439.444963	42.156391
3502.107640	803412.256859	42.161396
3502.215443	803383.206089	42.166400
3502.262253	803366.851897	42.171405
3502.104376	803342.819744	42.176410
3502.258038	803323.472123	42.181415
3502.400431	803293.439597	42.186420
3502.422675	803271.135723	42.191424
3502.451051	803254.052162	42.196429
3502.307057	803234.604409	42.201434
3502.292115	803201.863372	42.206439
3502.250200	803174.103807	42.211444
3502.374583	803149.490025	42.216448
3502.048160	803128.557716	42.221453
3502.168916	803107.701831	42.226458
3502.392412	803076.338043	42.231463
3502.290348	803053.467255	42.236468
3502.193091	803031.474022	42.241472
3502.062073	802999.189287	42.246477
3501.971772	802983.392345	42.251482
3502.432060	802951.454134	42.256487
3502.441672	802929.931846	42.261492
3502.256183	802914.784016	42.266496
3502.028698	802890.077842	42.271501
3502.026843	802859.138622	42.276506
3502.523929	802848.031987	42.281511
3501.891714	802816.166283	42.286516
3502.272237	802795.122371	42.291520
3502.264982	802778.482323	42.296525
3502.285717	802746.953415	42.301530
3502.581138	802723.872911	42.306535
3502.083600	802693.693601	42.311540
3502.197896	802672.642104	42.316544
3501.996931	802649.102103	42.321549
3502.022738	802630.162795	42.326554
3502.018580	802618.694899	42.331559
3502.136460	802601.839621	42.336564
3502.188343	802566.595958	42.341568
3502.203611	802546.877206	42.346573
3502.234514	802529.986533	42.351578
3502.043408	802518.206058	42.356583
3502.049587	802479.943263	42.361588
3502.234236	802463.321201	42.366592
3501.875267	802453.274976	42.371597
3501.731509	802416.743371	42.376602
3501.777357	802397.068182	42.381607
3501.737294	802388.338519	42.386612
3501.919528	802366.055290	42.391616
3501.917568	802359.808656	42.396621
3501.696778	802339.198882	42.401626
3502.160432	802321.507942	42.406631
3501.887770	802297.099370	42.411636
3501.887082	802276.943038	42.416640
3501.837870	802255.037240	42.421645
3501.870346	802230.629521	42.426650
3501.944436	802213.047986	42.431655
3501.861421	802198.419303	42.436660
3501.987282	802165.602157	42.441664
3502.068267	802159.586391	42.446669
3501.987127	802142.956244	42.451674
3501.884495	802124.718807	42.456679
3501.744574	802109.366723	42.461684
3501.937777	802080.882381	42.466688
3502.049451	802069.444202	42.471693
3501.628099	802053.891945	42.476698
3501.634843	802033.733688	42.481703
3501.690451	802026.013522	42.486708
3501.820379	801999.051724	42.491712
3501.535572	801985.820702	42.496717
3501.359286	801972.377458	42.501722
3501.554355	801955.898878	42.506727
3501.534774	801944.676225	42.511732
3501.717272	801923.611611	42.516736
3501.484937	801926.966882	42.521741
3501.495230	801905.831513	42.526746
3501.636189	801887.408900	42.531751
3501.456039	801885.191916	42.536756
3502.019627	801873.097048	42.541760
3501.824384	801854.726897	42.546765
3502.070864	801831.602031	42.551770
3502.186282	801818.796185	42.556775
3501.698588	801797.787115	42.561780
3502.033749	801773.037488	42.566784
3501.671320	801748.055151	42.571789
3501.762873	801741.012351	42.576794
3501.870100	801710.489823	42.581799
3501.909423	801707.359900	42.586804
3501.945660	801685.048324	42.591808
3501.854306	801673.982847	42.596813
3502.032104	801648.329956	42.601818
3502.238096	801624.869008	42.606823
3502.039744	801606.596252	42.611828
3502.333364	801585.366730	42.616832
3501.771009	801563.294734	42.621837
3501.909926	801535.841484	42.626842
3502.008940	801526.991287	42.631847
3501.914372	801509.238949	42.636852
3501.894533	801494.159486	42.641856
3501.451136	801475.485363	42.646861
3501.656756	801455.391825	42.651866
3501.635673	801452.417654	42.656871
3501.439252	801429.409390	42.661876
3501.662786	801413.705956	42.666880
3501.397218	801399.592105	42.671885
3501.454430	801381.669252	42.676890
3501.607501	801376.617724	42.681895
3501.381520	801363.766716	42.686900
3501.736622	801348.969985	42.691904
3501.613914	801347.280768	42.696909
3501.756550	801318.508081	42.701914
3501.723994	801309.629341	42.706919
3501.366581	801299.971557	42.711924
3501.069075	801285.911261	42.716928
3501.380779	801268.729313	42.721933
3501.483362	801270.226497	42.726938
3501.066950	801242.175425	42.731943
3501.111831	801250.661880	42.736948
3501.122064	801244.509881	42.741952
3501.451955	801239.040101	42.746957
3501.392034	801216.693117	42.751962
3501.684290	801216.549831	42.756967
3501.351891	801208.450019	42.761972
3501.210031	801172.496795	42.766976
3500.890067	801174.499376	42.771981
3501.303958	801184.636705	42.776986
3501.566503	801166.974036	42.781991
3501.485396	801147.656562	42.786996
3501.501811	801136.133988	42.792001
3501.486925	801132.133612	42.797005
3501.289647	801112.590124	42.802010
3501.814164	801106.064715	42.807015
3501.622738	801087.057187	42.812020
3501.576115	801059.972610	42.817025
3501.636533	801061.866949	42.822029
3501.808287	801044.803910	42.827034
3501.959515	801028.573882	42.832039
3501.586847	801010.082604	42.837044
3501.582686	800990.752630	42.842049
3501.404211	800979.064981	42.847053
3501.557155	800966.398018	42.852058
3501.691305	800961.593198	42.857063
3501.613327	800943.885519	42.862068
3501.266174	800930.320356	42.867073
3501.029940	800929.234558	42.872077
3500.947565	800922.071605	42.877082
3501.398398	800902.914319	42.882087
3501.537241	800895.716756	42.887092
3501.523060	800891.179148	42.892097
3501.563067	800877.065196	42.897101
3501.580727	800853.435614	42.902106
3501.550705	800841.236349	42.907111
3501.359701	800828.378801	42.912116
3501.515324	800822.594199	42.917121
3501.307629	800811.643055	42.922125
3501.186194	800796.040859	42.927130
3501.504257	800781.004536	42.932135
3501.288853	800783.723137	42.937140
3501.561463	800752.926131	42.942145
3501.231084	800753.026619	42.947149
3501.200448	800753.421966	42.952154
3501.512670	800743.072864	42.957159
3501.363397	800728.939358	42.962164
3501.551507	800717.633280	42.967169
3501.296185	800705.761879	42.972173
3501.416044	800684.947089	42.977178
3501.196468	800675.901440	42.982183
3501.243390	800683.802517	42.987188
3501.749221	800651.699325	42.992193
3501.333821	800646.980177	42.997197
3501.365394	800644.485576	43.002202
3501.706637	800616.313333	43.007207
3501.556115	800616.043982	43.012212
3501.473546	800598.775430	43.017217
3501.263643	800577.377210	43.022221
3501.382819	800577.163333	43.027226
3501.269605	800566.978090	43.032231
3501.239015	800548.920190	43.037236
3501.334936	800534.015654	43.042241
3501.444181	800532.680507	43.047245
3501.363352	800518.926387	43.052250
3501.289174	800506.733390	43.057255
3501.038529	800499.498634	43.062260
3501.354563	800499.009889	43.067265
3501.593028	800476.174323	43.072269
3501.205389	800471.890074	43.077274
3501.653892	800471.380620	43.082279
3501.563687	800458.018386	43.087284
3501.462119	800442.900416	43.092289
3501.187089	800435.474123	43.097293
3501.339749	800410.259602	43.102298
3501.409434	800406.733748	43.107303
3501.310545	800408.116171	43.112308
3501.351146	800398.931822	43.117313
3501.252209	800371.559609	43.122317
3501.393082	800368.169064	43.127322
3501.660458	800361.829565	43.132327
3501.161920	800346.773425	43.137332
3501.446157	800338.185560	43.142337
3500.947743	800342.120260	43.147341
3500.993377	800340.355640	43.152346
3501.274550	800314.290719	43.157351
3501.325977	800307.936105	43.162356
3501.190175	800307.078599	43.167361
3501.261183	800299.158674	43.172365
3500.789275	800290.298386	43.177370
3501.247624	800276.215362	43.182375
3501.104380	800270.135244	43.187380
3501.225389	800265.380781	43.192385
3500.744260	800272.339682	43.197389
3501.141884	800259.926004	43.202394
3501.426437	800241.964441	43.207399
3501.092872	800244.067072	43.212404
3501.214666	800235.992669	43.217409
3501.240117	800224.759976	43.222413
3501.121029	800213.208112	43.227418
3501.565398	800195.612003	43.232423
3501.266591	800206.887530	43.237428
3501.187249	800181.415456	43.242433
3501.209451	800167.937406	43.247437
3501.099014	800164.439576	43.252442
3501.430665	800164.192473	43.257447
3501.157587	800152.859857	43.262452
3501.319282	800137.553553	43.267457
3501.301480	800134.138869	43.272461
3500.951857	800137.757504	43.277466
3501.577647	800115.787721	43.282471
3501.129085	800114.442043	43.287476
3501.131656	800103.505644	43.292481
3501.113212	800113.614610	43.297485
3501.202289	800087.041762	43.302490
3501.268565	800077.218259	43.307495
3501.574904	800069.017156	43.312500
3501.078662	800058.988628	43.317505
3501.557083	800041.484421	43.322509
3501.386051	800035.896645	43.327514
3501.532868	800025.865185	43.332519
3500.934659	800008.187433	43.337524
3501.234391	800000.084920	43.342529
3501.459915	799994.386296	43.347533
3501.103388	799990.829196	43.352538
3501.243441	799966.347247	43.357543
3501.157509	799963.675461	43.362548
3501.082133	799964.370786	43.367553
3501.369803	799952.413111	43.372557
3501.206450	799935.838928	43.377562
3501.253727	799928.166372	43.382567
3500.706308	799928.691377	43.387572
3500.907176	799924.217117	43.392577
3501.270032	799926.259806	43.397581
3500.958538	799912.198687	43.402586
3501.286878	799905.458629	43.407591
3501.199999	799902.054619	43.412596
3501.363867	799892.020286	43.417601
3501.584865	799880.512309	43.422605
3500.727336	799860.384700	43.427610
3501.391034	799859.646271	43.432615
3501.086432	799866.773304	43.437620
3501.202735	799850.448125	43.442625
3500.978801	799845.747276	43.447629
3501.095081	799828.592045	43.452634
3501.065256	799816.000218	43.457639
3501.166447	799820.280913	43.462644
3500.935501	799812.993479	43.467649
3500.960606	799804.201295	43.472653
3500.839070	799800.167939	43.477658
3501.035274	799796.280207	43.482663
3500.938595	799807.231889	43.487668
3500.992098	799787.108108	43.492673
3501.316417	799804.145801	43.497677
3501.305556	799784.227368	43.502682
3501.232979	799773.204508	43.507687
3501.457058	799781.762536	43.512692
3501.097853	799761.703191	43.517697
3501.187352	799750.899077	43.522701
3500.975950	799736.870753	43.527706
3501.261297	799731.309019	43.532711
3501.115530	799742.512606	43.537716
3500.725776	799720.602584	43.542721
3500.984179	799698.981763	43.547725
3500.826256	799705.646622	43.552730
3501.009189	799705.569227	43.557735
3500.952217	799708.800580	43.562740
3501.388360	799706.779444	43.567745
3501.223287	799698.016845	43.572749
3501.177557	799674.392849	43.577754
3501.551330	799672.088504	43.582759
3501.008521	799673.882251	43.587764
3501.316895	799667.730965	43.592769
3501.235730	799652.900901	43.597773
3501.240817	799645.674029	43.602778
3501.460002	799630.796963	43.607783
3501.308653	799621.690338	43.612788
3501.352431	799605.278226	43.617793
3501.438253	799598.331634	43.622797
3501.332436	799592.586801	43.627802
3501.486559	799574.936727	43.632807
3501.385894	799586.865917	43.637812
3501.695645	799564.846017	43.642817
3501.407926	799542.577660	43.647821
3501.629798	799540.687620	43.652826
3501.772151	799519.474948	43.657831
3501.894191	799510.911342	43.662836
3501.179462	799487.586545	43.667841
3501.440469	799464.255614	43.672845
3501.289923	799464.035041	43.677850
3501.536996	799456.330693	43.682855
3501.174463	799446.426783	43.687860
3501.300819	799430.977850	43.692865
3501.203110	799436.119946	43.697869
3501.503913	799418.007074	43.702874
3501.366135	799401.866960	43.707879
3501.163617	799399.799087	43.712884
3501.293342	799387.230309	43.717889
3501.414797	799360.600583	43.722893
3501.181289	799357.560997	43.727898
3501.509420	799356.484357	43.732903
3501.174625	799346.185338	43.737908
3501.122074	799321.340434	43.742913
3501.139116	799321.679587	43.747917
3501.592891	799320.241508	43.752922
3501.198284	799296.670667	43.757927
3501.434378	799298.684548	43.762932
3501.358184	799296.645722	43.767937
3501.169725	799286.567870	43.772941
3500.795328	799271.538629	43.777946
3501.146925	799268.993470	43.782951
3501.050116	799264.467634	43.787956
3501.100325	799259.674673	43.792961
3500.901527	799256.287817	43.797965
3500.742300	799250.697512	43.802970
3501.381793	799236.290944	43.807975
3500.793413	799222.564570	43.812980
3501.111727	799222.758977	43.817985
3501.317309	799227.219062	43.822989
3500.674056	799215.698519	43.827994
3501.099029	799194.049972	43.832999
3500.870905	799194.232143	43.838004
3500.832331	799193.017487	43.843009
3500.844568	799201.218776	43.848013
3500.951380	799201.250933	43.853018
3501.158023	799199.216691	43.858023
3501.040905	799205.582715	43.863028
3501.152662	799181.736984	43.868033
3500.859931	799172.993625	43.873037
3500.906502	799175.476629	43.878042
3501.223645	799168.395757	43.883047
3500.888831	799174.747014	43.888052
3501.084968	799168.368658	43.893057
3501.037743	799150.358270	43.898061
3500.961986	799148.319328	43.903066
3500.863996	799131.293398	43.908071
3500.783202	799141.950751	43.913076
3501.094448	799142.292753	43.918081
3501.146545	799139.843192	43.923085
3500.963409	799128.738855	43.928090
3500.866330	799116.009688	43.933095
3500.590301	799110.584008	43.938100
3500.628988	799099.982066	43.943105
3501.097748	799107.916792	43.948109
3500.757140	799110.118542	43.953114
3501.062220	799118.420645	43.958119
3500.898617	799114.588751	43.963124
3500.818350	799090.968019	43.968129
3501.020497	799090.057518	43.973133
3500.857409	799084.321185	43.978138
3501.095418	799078.131512	43.983143
3500.719455	799086.344801	43.988148
3501.158678	799086.032021	43.993153
3500.824730	799086.279566	43.998157
3500.666319	799075.561907	44.003162
3500.876497	799068.204671	44.008167
3500.810108	799059.669923	44.013172
3500.886319	799058.827934	44.018177
3500.967508	799058.522291	44.023181
3500.974641	799068.189430	44.028186
3501.011880	799063.105374	44.033191
3500.977893	799063.208371	44.038196
3501.052606	799050.501050	44.043201
3501.044215	799033.509686	44.048205
3500.825490	799034.129859	44.053210
3500.992606	799035.959287	44.058215
3500.922816	799036.849156	44.063220
3501.006406	799037.861537	44.068225
3501.438604	799030.616041	44.073229
3501.157703	799020.942862	44.078234
3501.204314	798998.864511	44.083239
3500.500254	799002.295030	44.088244
3500.710196	799001.529789	44.093249
3501.375126	799002.695449	44.098253
3500.853769	798993.938756	44.103258
3501.160899	798971.038306	44.108263
3500.723313	798971.350886	44.113268
3500.983896	798970.724215	44.118273
3501.218089	798966.048766	44.123277
3501.248974	798966.678756	44.128282
3500.952922	798946.216356	44.133287
3501.108621	798939.404624	44.138292
3501.172019	798934.462869	44.143297
3501.079367	798928.617725	44.148301
3501.138342	798924.653263	44.153306
3501.180509	798911.462452	44.158311
3500.996203	798911.442458	44.163316
3500.967713	798908.419439	44.168321
3501.165359	798900.770989	44.173325
3501.040174	798908.408163	44.178330
3501.345595	798888.925832	44.183335
3501.062459	798870.609727	44.188340
3501.240452	798864.673387	44.193345
3501.300508	798874.283712	44.198349
3500.886362	798855.695059	44.203354
3501.344045	798845.564343	44.208359
3500.597832	798835.377650	44.213364
3500.795029	798832.123991	44.218369
3501.276305	798828.142287	44.223373
3501.107718	798835.151527	44.228378
3501.525873	798820.143832	44.233383
3501.264494	798803.777386	44.238388
3501.178848	798803.155992	44.243393
3501.098174	798796.088070	44.248397
3500.993314	798786.680009	44.253402
3500.733130	798768.799510	44.258407
3500.486762	798770.498324	44.263412
3500.794621	798774.991567	44.268417
3500.629659	798779.998203	44.273421
3500.654534	798784.779833	44.278426
3501.061668	798785.692845	44.283431
3500.569845	798786.941710	44.288436
3501.045273	798789.406655	44.293441
3501.020599	798785.748173	44.298445
3500.795190	798778.751689	44.303450
3500.903526	798753.879452	44.308455
3500.569725	798753.833994	44.313460
3500.799324	798750.477567	44.318465
3501.097134	798752.335478	44.323469
3500.853038	798758.233473	44.328474
3501.134339	798748.520832	44.333479
3500.973666	798757.189200	44.338484
3500.800466	798745.447837	44.343489
3501.093861	798736.026278	44.348493
3500.800401	798736.609329	44.353498
3500.750618	798721.967547	44.358503
3500.938163	798740.640892	44.363508
3500.816478	798729.037941	44.368513
3500.806970	798739.635981	44.373517
3500.573595	798732.836020	44.378522
3501.198363	798729.515472	44.383527
3500.693355	798710.794108	44.388532
3500.769735	798710.489201	44.393537
3500.549679	798709.400488	44.398541
3500.522632	798712.237003	44.403546
3500.799775	798703.843412	44.408551
3500.568072	798707.688564	44.413556
3500.746859	798704.535385	44.418561
3500.810458	798706.185761	44.423565
3500.283804	798708.026070	44.428570
3500.922002	798704.947572	44.433575
3500.815263	798717.660629	44.438580
3500.762348	798720.647681	44.443585
3500.618905	798725.455666	44.448589
3500.745443	798733.249025	44.453594
3500.950709	798719.104519	44.458599
3500.358840	798730.721417	44.463604
3500.796155	798725.476892	44.468609
3500.794538	798728.162929	44.473613
3500.592093	798735.568225	44.478618
3501.109971	798722.205000	44.483623
3500.555725	798705.786423	44.488628
3500.873365	798694.212398	44.493633
3500.970703	798694.832026	44.498637
3500.844227	798704.178771	44.503642
3500.758992	798694.865172	44.508647
3500.577483	798702.364897	44.513652
3500.498571	798699.642657	44.518657
3500.704628	798707.521281	44.523661
3500.748924	798706.684235	44.528666
3500.827639	798705.206992	44.533671
3500.563946	798710.082619	44.538676
3500.945044	798710.609056	44.543681
3501.052708	798709.810937	44.548685
3500.986686	798700.543175	44.553690
3500.744754	798687.249821	44.558695
3500.768238	798676.454232	44.563700
3500.888383	798676.923799	44.568705
3500.747499	798669.620990	44.573709
3500.909741	798686.442815	44.578714
3501.124961	798682.990936	44.583719
3500.646739	798684.140028	44.588724
3500.806843	798673.762569	44.593729
3500.835003	798657.985313	44.598733
3500.726227	798651.165788	44.603738
3500.788387	798646.077509	44.608743
3500.723478	798656.440183	44.613748
3500.847709	798654.858147	44.618753
3500.997248	798653.369821	44.623757
3500.943566	798652.645750	44.628762
3501.046140	798648.039480	44.633767
3500.908300	798646.889071	44.638772
3500.896253	798625.844100	44.643777
3500.857912	798618.915865	44.648781
3500.728844	798625.577324	44.653786
3500.767274	798629.477960	44.658791
3500.467634	798634.554594	44.663796
3500.983348	798622.021657	44.668801
3500.891446	798635.660378	44.673805
3500.892419	798632.290796	44.678810
3501.044921	798630.997332	44.683815
3501.039327	798612.783607	44.688820
3500.781794	798602.715484	44.693825
3500.817385	798596.556994	44.698829
3500.773610	798605.744454	44.703834
3500.982421	798601.121544	44.708839
3501.164765	798603.095215	44.713844
3501.203890	798592.492373	44.718849
3501.113689	798578.247247	44.723853
3500.608083	798574.712659	44.728858
3501.192790	798565.831313	44.733863
3500.992018	798574.262028	44.738868
3501.188515	798578.528651	44.743873
3501.130062	798572.482506	44.748877
3500.841663	798551.578160	44.753882
3501.084183	798538.990102	44.758887
3500.884813	798531.500945	44.763892
3501.036232	798535.872310	44.768897
3501.058242	798540.263902	44.773901
3500.794455	798543.576999	44.778906
3501.143167	798520.570790	44.783911
3500.782661	798516.232150	44.788916
3500.832607	798518.959048	44.793921
3501.149782	798509.191608	44.798925
3500.818690	798513.345413	44.803930
3501.284153	798509.512489	44.808935
3500.995144	798498.570118	44.813940
3501.039378	798476.002017	44.818945
3500.660622	798474.938070	44.823949
3500.606665	798486.129480	44.828954
3501.053189	798479.955477	44.833959
3500.995087	798488.070998	44.838964
3501.261495	798488.908386	44.843969
3501.526362	798457.857483	44.848973
3501.064016	798443.865572	44.853978
3501.212703	798443.207511	44.858983
3501.143222	798455.719922	44.863988
3500.964762	798430.891275	44.868993
3500.988724	798413.893225	44.873997
3501.004340	798420.581111	44.879002
3501.012940	798408.078200	44.884007
3501.214428	798417.227588	44.889012
3501.075922	798401.671097	44.894017
3501.218839	798388.072794	44.899021
3500.861979	798382.561464	44.904026
3501.120395	798374.902894	44.909031
3500.948479	798382.450324	44.914036
3501.077147	798374.616698	44.919041
3501.297059	798360.908632	44.924045
3501.062080	798363.435961	44.929050
3501.219754	798353.546717	44.934055
3501.105153	798354.004170	44.939060
3500.968773	798351.681443	44.944065
3501.310636	798338.003101	44.949069
3500.818523	798329.338597	44.954074
3500.828653	798326.016260	44.959079
3500.752125	798330.765242	44.964084
3500.834673	798321.620217	44.969089
3501.165260	798319.126812	44.974093
3500.998223	798318.664598	44.979098
3501.104185	798291.544542	44.984103
3500.896615	798289.965451	44.989108
3500.555036	798292.362965	44.994113
3500.878769	798291.335679	44.999117
3500.777390	798297.700134	45.004122
3501.123883	798295.741422	45.009127
3501.108720	798295.792653	45.014132
3500.798071	798266.930714	45.019137
3501.168775	798257.642883	45.024141
3500.900052	798254.217592	45.029146
3501.199152	798255.245244	45.034151
3501.063224	798256.389735	45.039156
3501.083797	798244.421828	45.044161
3501.053724	798234.073393	45.049165
3500.943952	798227.497755	45.054170
3501.089661	798223.177456	45.059175
3501.131705	798219.850074	45.064180
3501.228875	798219.932582	45.069185
3501.067733	798204.183811	45.074189
3501.166813	798207.440355	45.079194
3501.231185	798192.681858	45.084199
3501.018378	798187.587366	45.089204
3500.836261	798177.067264	45.094209
3501.089758	798165.258144	45.099213
3501.082901	798165.308077	45.104218
3501.095157	798156.857515	45.109223
3500.972002	798168.304473	45.114228
3500.730326	798168.488786	45.119233
3500.896887	798168.804628	45.124237
3501.002061	798154.625700	45.129242
3501.247887	798123.185479	45.134247
3500.729313	798136.843112	45.139252
3500.893299	798137.061685	45.144257
3501.232134	798138.180818	45.149261
3500.712580	798137.187659	45.154266
3501.085886	798135.810745	45.159271
3501.104104	798114.564035	45.164276
3500.896171	798094.475852	45.169281
3500.878575	798104.636665	45.174285
3500.639445	798106.725212	45.179290
3501.140268	798103.863258	45.184295
3500.986773	798107.794211	45.189300
3500.949043	798090.902630	45.194305
3501.382214	798073.839719	45.199309
3500.878061	798071.769729	45.204314
3501.080764	798071.493883	45.209319
3501.158221	798076.902698	45.214324
3500.693014	798061.640644	45.219329
3501.170544	798050.284663	45.224333
3500.793418	798048.585506	45.229338
3500.988974	798041.620090	45.234343
3501.085603	798034.914316	45.239348
3501.052794	798039.656677	45.244353
3500.786550	798035.644836	45.249357
3500.748755	798033.746119	45.254362
3501.148492	798021.474341	45.259367
3500.986260	798014.027615	45.264372
3500.929336	798017.162129	45.269377
3501.115470	798009.807453	45.274381
3500.984376	798010.902394	45.279386
3500.985888	798005.578905	45.284391
3501.064077	797992.038727	45.289396
3501.063667	797979.194534	45.294401
3500.939197	797974.037226	45.299405
3500.729460	797974.167713	45.304410
3501.130756	797969.270077	45.309415
3500.788269	797975.232999	45.314420
3500.649501	797975.938444	45.319425
3500.802956	797945.635067	45.324429
3500.705406	797946.089883	45.329434
3500.797328	797937.431229	45.334439
3500.793738	797951.057587	45.339444
3500.530269	797944.994066	45.344449
3500.675690	797948.243496	45.349453
3500.756967	797951.258763	45.354458
3500.853758	797947.727332	45.359463
3500.639095	797955.086589	45.364468
3500.644658	797960.897442	45.369473
3501.011616	797945.114325	45.374477
3500.824658	797955.643712	45.379482
3500.907766	797954.995854	45.384487
3500.587162	797943.422588	45.389492
3500.905538	797929.502867	45.394497
3500.892509	797930.530527	45.399501
3500.797745	797924.538291	45.404506
3500.913509	797928.524938	45.409511
3500.552601	797929.362789	45.414516
3500.649010	797923.096476	45.419521
3500.749983	797926.938922	45.424525
3500.666245	797939.112693	45.429530
3501.027993	797927.628084	45.434535
3500.745828	797937.097948	45.439540
3500.490312	797936.112319	45.444545
3500.671531	797931.590923	45.449549
3500.312362	797935.944835	45.454554
3501.031830	797932.071869	45.459559
3500.752666	797936.413275	45.464564
3500.613335	797912.016060	45.469569
3500.936359	797903.663102	45.474573
3500.559085	797903.136045	45.479578
3500.578445	797908.456406	45.484583
3500.566223	797916.614309	45.489588
3500.854533	797901.624791	45.494593
3500.774140	797898.365222	45.499597
3500.712096	797909.119349	45.504602
3500.920994	797899.074890	45.509607
3501.019752	797904.724710	45.514612
3500.729377	797905.258509	45.519617
3501.098632	797911.110229	45.524621
3500.593082	797904.840322	45.529626
3500.401380	797882.893093	45.534631
3500.594573	797905.133169	45.539636
3500.333952	797905.613478	45.544641
3501.009081	797906.484730	45.549645
3500.727792	797897.591335	45.554650
3501.087879	797889.427918	45.559655
3501.152624	797898.404064	45.564660
3500.762390	797894.069649	45.569665
3500.956072	797888.227641	45.574669
3500.583746	797890.044048	45.579674
3501.004669	797893.103924	45.584679
3500.991379	797892.031585	45.589684
3500.524580	797872.959946	45.594689
3501.005465	797851.395855	45.599693
3501.096702	797853.725870	45.604698
3500.981735	797846.173885	45.609703
3500.967920	797859.264809	45.614708
3500.875055	797869.584273	45.619713
3501.056022	797859.446441	45.624717
3500.822977	797847.615123	45.629722
3500.867024	797831.540338	45.634727
3501.071175	797834.487613	45.639732
3500.630591	797830.307541	45.644737
3501.124280	797825.102322	45.649741
3500.501399	797834.918628	45.654746
3500.953089	797831.527011	45.659751
3500.723271	797829.853606	45.664756
3500.737422	797839.472647	45.669761
3501.070071	797819.738654	45.674765
3500.628898	797808.867738	45.679770
3500.674769	797800.509133	45.684775
3501.032173	797796.839204	45.689780
3500.792199	797796.241835	45.694785
3500.976191	797790.547772	45.699789
3500.753232	797803.134274	45.704794
3501.041057	797805.726609	45.709799
3500.897370	797802.281530	45.714804
3500.840668	797786.613094	45.719809
3500.704183	797778.380646	45.724813
3500.363083	797774.575699	45.729818
3500.683635	797764.171703	45.734823
3500.597801	797761.303630	45.739828
3500.576356	797713.590866	45.744833
3500.846928	797612.547456	45.749837
3500.405462	797470.245192	45.754842
3500.376095	797266.138123	45.759847
3500.179133	797022.144718	45.764852
3499.704186	796714.244981	45.769857
3499.395323	796365.319836	45.774861
3499.168853	795974.887247	45.779866
3498.412520	795521.587664	45.784871
3498.337241	795049.974266	45.789876
3497.681651	794512.354073	45.794881
3497.254796	793929.060060	45.799885
3496.573161	793301.035352	45.804890
3496.410556	792627.266361	45.809895
3495.666813	791892.659509	45.814900
3494.868707	791130.405546	45.819905
3494.039433	790304.602474	45.824909
3493.173380	789441.340860	45.829914
3492.413119	788540.486090	45.834919
3491.414845	787577.130019	45.839924
3490.290014	786581.902758	45.844929
3489.611508	785520.204833	45.849933
3488.803290	784437.314106	45.854938
3487.305585	783292.682425	45.859943
3486.264857	782117.969298	45.864948
3485.504037	780895.755860	45.869953
3484.432854	779624.639847	45.874957
3483.118548	778316.143699	45.879962
3481.670083	776958.667033	45.884967
3480.220305	775548.779194	45.889972
3478.843087	774106.581476	45.894977
3477.690842	772612.224753	45.899981
3476.085906	771095.791393	45.904986
3474.561164	769512.552458	45.909991
3473.168843	767916.271517	45.914996
3471.518790	766276.922403	45.920001
3470.121518	764574.370938	45.925005
3468.263507	762854.537364	45.930010
3466.842637	761090.016432	45.935015
3464.642433	759288.972694	45.940020
3463.104009	757443.244466	45.945025
3461.726222	755566.490176	45.950029
3459.460521	753663.275461	45.955034
3457.497338	751718.004644	45.960039
3455.427786	749731.201582	45.965044
3453.583572	747711.588978	45.970049
3451.626429	745659.194850	45.975053
3449.435449	743578.984891	45.980058
3447.101360	741464.325706	45.985063
3445.119914	739308.709772	45.990068
3442.202950	737134.674137	45.995073
3440.620424	734941.752299	46.000077
3438.167952	732705.922024	46.005082
3436.221957	730436.056078	46.010087
3433.805086	728132.724098	46.015092
3431.007470	725810.589719	46.020097
3428.766212	723452.513451	46.025101
3426.261865	721085.898549	46.030106
3423.764461	718671.433908	46.035111
3421.490455	716232.364700	46.040116
3418.677278	713772.448699	46.045121
3416.279183	711286.429562	46.050125
3413.739532	708773.434741	46.055130
3411.088992	706236.802467	46.060135
3408.682832	703650.183181	46.065140
3405.795904	701063.197501	46.070145
3403.022739	698441.937494	46.075149
3400.532267	695821.616475	46.080154
3397.535307	693155.441536	46.085159
3395.004097	690467.459040	46.090164
3392.232888	687762.474253	46.095169
3389.275346	685025.787263	46.100173
3386.205183	682275.123427	46.105178
3383.461726	679507.230349	46.110183
3380.956998	676705.827300	46.115188
3377.765651	673886.130136	46.120193
3375.077206	671051.468777	46.125197
3371.799372	668192.812530	46.130202
3368.895011	665311.584945	46.135207
3365.946455	662425.440146	46.140212
3362.885222	659508.872270	46.145217
3360.060049	656568.472228	46.150221
3356.856326	653620.149451	46.155226
3354.132493	650649.478817	46.160231
3350.959404	647655.097246	46.165236
3347.954495	644638.985548	46.170241
3344.740343	641610.061524	46.175245
3341.824276	638559.865281	46.180250
3338.687438	635498.091418	46.185255
3335.515687	632419.868620	46.190260
3331.820810	629328.709401	46.195265
3328.672904	626211.063185	46.200269
3325.473465	623091.876512	46.205274
3322.295380	619948.515813	46.210279
3318.896052	616801.592837	46.215284
3315.240187	613631.773969	46.220289
3312.581635	610439.350648	46.225293
3308.953061	607264.282736	46.230298
3305.673689	604055.555478	46.235303
3302.594013	600843.199634	46.240308
3299.127361	597606.035784	46.245313
3295.565753	594359.930240	46.250317
3292.048871	591116.284260	46.255322
3288.605009	587846.442506	46.260327
3285.121381	584583.892193	46.265332
3281.427962	581295.884814	46.270337
3278.173300	578001.916646	46.275341
3274.745466	574707.907804	46.280346
3271.065053	571397.219555	46.285351
3267.092593	568065.887873	46.290356
3263.829247	564742.169099	46.295361
3260.560322	561413.233181	46.300365
3257.147033	558065.090213	46.305370
3253.541473	554722.869535	46.310375
3249.742781	551356.022671	46.315380
3246.209316	548002.783815	46.320385
3243.093424	544618.537279	46.325389
3239.309630	541246.202111	46.330394
3235.336671	537857.944589	46.335399
3232.114696	534456.988107	46.340404
3228.202462	531067.374573	46.345409
3224.505936	527650.705248	46.350413
3220.681962	524243.949678	46.355418
3217.336861	520827.480200	46.360423
3213.717268	517422.637363	46.365428
3210.163332	513998.432620	46.370433
3206.492475	510563.967733	46.375437
3202.692624	507134.682342	46.380442
3198.591235	503694.422958	46.385447
3195.097135	500247.541638	46.390452
3191.492695	496813.034704	46.395457
3188.004850	493363.723944	46.400461
3184.012788	489911.826736	46.405466
3180.275323	486454.455397	46.410471
3176.699259	482999.108917	46.415476
3173.057302	479544.925481	46.420481
3169.206752	476076.320942	46.425485
3165.538680	472610.323143	46.430490
3161.545536	469142.169759	46.435495
3157.923077	465677.071981	46.440500
3154.376020	462206.236154	46.445505
3150.843374	458731.247657	46.450509
3146.584876	455254.052455	46.455514
3142.634995	451778.395808	46.460519
3139.232095	448298.531442	46.465524
3135.381838	444814.319506	46.470529
3131.515585	441334.462662	46.475533
3127.742155	437861.996518	46.480538
3123.890770	434379.990076	46.485543
3120.228954	430896.768255	46.490548
3116.560570	427420.835875	46.495553
3112.761988	423930.835205	46.500557
3108.870226	420464.383215	46.505562
3104.841423	416983.630368	46.510567
3100.955186	413502.331407	46.515572
3097.428597	410028.426621	46.520577
3093.819748	406542.264384	46.525581
3089.543930	403073.573456	46.530586
3085.749226	399592.556073	46.535591
3081.600700	396126.248343	46.540596
3077.738739	392657.358539	46.545601
3074.115276	389192.173710	46.550605
3070.084728	385730.552994	46.555610
3066.346797	382262.038944	46.560615
3062.584852	378794.739101	46.565620
3058.776440	375350.891736	46.570625
3054.840682	371893.492941	46.575629
3050.783179	368440.127295	46.580634
3047.024177	364989.826184	46.585639
3043.161299	361546.170631	46.590644
3039.130271	358101.736942	46.595649
3035.303224	354658.459346	46.600653
3031.602699	351232.628975	46.605658
3027.499315	347800.396633	46.610663
3023.667603	344371.631348	46.615668
3019.749975	340953.723161	46.620673
3015.934403	337531.576023	46.625677
3011.894020	334129.639065	46.630682
3008.088920	330712.374878	46.635687
3004.149289	327303.859106	46.640692
3000.183035	323910.522918	46.645697
2996.168236	320501.269259	46.650701
2992.387695	317108.321136	46.655706
2988.547449	313711.305985	46.660711
2984.364947	310335.926731	46.665716
2980.060226	306963.916770	46.670721
2976.240685	303596.056551	46.675725
2972.387312	300246.461237	46.680730
2968.498708	296900.508278	46.685735
2964.430965	293542.804650	46.690740
2960.499372	290212.815797	46.695745
2956.598049	286869.611313	46.700749
2952.433570	283549.420613	46.705754
2948.157550	280240.037200	46.710759
2944.255689	276927.519429	46.715764
2940.283788	273628.164394	46.720769
2936.619025	270330.719936	46.725773
2932.366797	267053.337711	46.730778
2928.377351	263784.691143	46.735783
2924.566802	260517.417859	46.740788
2920.158406	257269.295815	46.745793
2916.164561	254014.659234	46.750797
2912.083969	250778.755875	46.755802
2908.051005	247548.050994	46.760807
2904.097271	244325.527941	46.765812
2899.902309	241115.422214	46.770817
2895.718891	237913.882607	46.775821
2891.636089	234736.974297	46.780826
2887.581030	231564.087337	46.785831
2883.720187	228395.814833	46.790836
2879.464732	225238.496619	46.795841
2875.645339	222101.077503	46.800845
2871.056170	218975.221453	46.805850
2866.928846	215848.161620	46.810855
2862.992413	212742.767729	46.815860
2858.643831	209656.517642	46.820865
2854.568321	206579.072652	46.825869
2850.619672	203504.171913	46.830874
2846.452366	200449.805347	46.835879
2842.361205	197402.766486	46.840884
2837.961293	194375.396690	46.845889
2834.484032	191354.801599	46.850893
2830.144120	188347.301846	46.855898
2825.398449	185350.718106	46.860903
2821.696699	182365.491381	46.865908
2817.042979	179398.050312	46.870913
2813.189293	176445.630351	46.875917
2809.040235	173514.925539	46.880922
2804.800129	170586.418260	46.885927
2800.790516	167667.243520	46.890932
2796.518887	164691.815121	46.895937
2792.976415	161805.030580	46.900941
2788.091005	158947.146094	46.905946
2784.085825	156074.174489	46.910951
2780.399516	153236.481164	46.915956
2775.875294	150428.253595	46.920961
2771.991077	147605.703313	46.925965
2767.659503	144813.963807	46.930970
2763.205234	142023.376409	46.935975
2759.508099	139250.386824	46.940980
2755.416152	136491.920512	46.945985
2751.384633	133746.000660	46.950989
2747.106907	131030.716089	46.955994
2742.969402	128306.751858	46.960999
2738.946577	125608.638296	46.966004
2734.754369	122922.404105	46.971009
2730.832720	120238.241366	46.976013
2726.738659	117579.851028	46.981018
2722.375890	114939.745231	46.986023
2718.105825	112309.400143	46.991028
2714.070472	109681.434672	46.996033
2710.120840	107081.505168	47.001037
2705.917464	104499.544167	47.006042
2701.799889	101921.974368	47.011047
2697.989808	99348.166968	47.016052
2693.320484	96820.336104	47.021057
2689.569324	94284.900077	47.026061
2685.803466	91764.298444	47.031066
2681.481107	89251.412122	47.036071
2677.564756	86764.387410	47.041076
2673.230094	84280.128311	47.046081
2669.528730	81815.024888	47.051085
2665.035087	79374.430273	47.056090
2660.706631	76935.979132	47.061095
2656.711254	74510.861642	47.066100
2652.711820	72114.977698	47.071105
2648.530160	69722.023736	47.076109
2644.822474	67342.303919	47.081114
2640.309146	64988.820592	47.086119
2636.367033	62639.293349	47.091124
2632.000525	60310.113357	47.096129
2628.123601	57990.696787	47.101133
2623.749443	55698.215333	47.106138
2619.642690	53411.151849	47.111143
2615.742524	51126.770485	47.116148
2611.217486	48892.528982	47.121153
2607.153829	46647.840393	47.126157
2602.974907	44429.614991	47.131162
2598.821089	42217.946190	47.136167
2594.681282	40019.367276	47.141172
2590.222516	37849.550650	47.146177
2586.157197	35687.674800	47.151181
2581.758215	33556.171956	47.156186
2577.509014	31441.795808	47.161191
2573.137068	29341.075319	47.166196
2568.955758	27276.581797	47.171201
2564.195366	25222.271590	47.176205
2559.865510	23189.421406	47.181210
2555.309626	21177.781158	47.186215
2550.638726	19192.206463	47.191220
2545.783127	17239.973259	47.196225
2541.029984	15304.756150	47.201229
2535.610340	13424.434691	47.206234
2529.988615	11582.772898	47.211239
2524.321589	9778.226661	47.216244
2517.146513	8046.899890	47.221249
2506.479508	6487.450964	47.226253
2492.801818	5078.599776	47.231258
2480.138284	3765.883195	47.236263
2468.754782	2605.329702	47.241268
2457.589550	1580.309918	47.246273
2447.579240	679.912879	47.251277
2434.240669	11.641812	47.256282
2394.789998	205.733906	47.261287
2376.545708	207.600942	47.266292
2371.674321	209.821599	47.271297
2374.790097	217.177435	47.276301
2380.769101	218.478961	47.281306
2387.257302	216.071865	47.286311
2391.203322	212.613415	47.291316
2392.007906	211.313774	47.296321
2391.437685	210.906276	47.301325
2388.759304	208.683471	47.306330
2385.188283	201.930434	47.311335
2382.839087	204.977770	47.316340
2378.849823	202.956879	47.321345
2375.448515	197.521944	47.326349
2373.079458	192.738640	47.331354
2369.841332	197.184263	47.336359
2367.557454	197.579548	47.341364
2364.406957	196.262709	47.346369
2361.557435	189.646759	47.351373
2358.196449	196.152301	47.356378
2355.452156	197.192279	47.361383
2352.344904	187.886231	47.366388
2348.597409	189.696944	47.371393
2345.341890	189.719039	47.376397
2342.210762	195.460935	47.381402
2338.950626	193.620234	47.386407
2335.851298	185.436128	47.391412
2332.227401	193.276829	47.396417
2328.998551	191.678019	47.401421
2326.141474	188.078431	47.406426
2322.818921	195.217071	47.411431
2319.481219	188.478184	47.416436
2315.799466	204.057280	47.421441
2312.726971	188.883155	47.426445
2309.527738	195.477303	47.431450
2306.142878	191.441415	47.436455
2302.708088	188.406796	47.441460
2299.304111	189.831576	47.446465
2295.891912	189.577630	47.451469
2292.563427	201.693974	47.456474
2289.209610	197.735494	47.461479
2285.819191	191.564871	47.466484
2282.083037	204.244889	47.471489
2278.700568	183.266118	47.476493
2275.262320	193.226055	47.481498
2272.141858	197.020520	47.486503
2269.263550	187.909647	47.491508
2265.431811	193.565011	47.496513
2262.020468	185.723986	47.501517
2258.427341	185.704009	47.506522
2254.673130	195.083775	47.511527
2251.510394	187.681602	47.516532
2248.010577	191.892940	47.521537
2244.663625	183.833033	47.526541
2241.252553	189.125186	47.531546
2237.601746	193.635406	47.536551
2234.576435	183.519289	47.541556
2231.058421	187.356977	47.546561
2228.049241	185.081565	47.551565
2224.087960	192.677676	47.556570
2220.456510	192.897833	47.561575
2217.272405	190.187866	47.566580
2213.772597	186.815424	47.571585
2210.287656	192.435530	47.576589
2206.524691	188.889119	47.581594
2203.317439	192.535822	47.586599
2200.226698	183.220921	47.591604
2196.528248	180.714826	47.596609
2193.153496	180.831553	47.601613
2189.297978	180.783046	47.606618
2185.679107	176.973648	47.611623
2182.876360	174.792507	47.616628
2178.855797	180.711563	47.621633
2175.616272	185.957909	47.626637
2172.353930	175.337884	47.631642
2168.592058	180.042675	47.636647
2165.285814	170.682414	47.641652
2161.564474	189.567630	47.646657
2158.337934	178.473755	47.651661
2154.227067	186.773519	47.656666
2151.046221	186.445454	47.661671
2148.177801	175.545498	47.666676
2144.813135	189.970816	47.671681
2141.382223	176.510716	47.676685
2137.570834	176.369899	47.681690
2133.837094	180.674816	47.686695
2130.357434	179.621528	47.691700
2127.333291	187.102677	47.696705
2123.959652	172.418703	47.701709
2120.302283	174.512790	47.706714
2116.536670	178.110831	47.711719
2113.248215	164.267783	47.716724
2109.592541	172.875996	47.721729
2106.334162	184.092351	47.726733
2102.536893	174.302723	47.731738
2099.196850	173.433251	47.736743
2095.855109	169.991828	47.741748
2092.001637	169.775352	47.746753
2088.708195	172.730027	47.751757
2085.343630	172.335811	47.756762
2081.886066	180.264446	47.761767
2078.189575	161.438902	47.766772
2074.766547	173.370740	47.771777
2071.434184	164.511332	47.776781
2067.920623	180.820303	47.781786
2064.256435	173.749773	47.786791
2060.620643	163.773546	47.791796
2057.233409	170.580665	47.796801
2053.764355	169.876931	47.801805
2050.428300	174.692306	47.806810
2046.886182	174.234132	47.811815
2043.855507	179.356079	47.816820
2039.925311	181.856727	47.821825
2036.677402	169.045109	47.826829
2032.760186	174.460804	47.831834
2029.207681	177.588915	47.836839
2026.145826	169.275672	47.841844
2022.407038	176.719960	47.846849
2019.273712	179.763500	47.851853
2015.748330	175.474449	47.856858
2011.941757	173.640259	47.861863
2008.867041	169.869172	47.866868
2005.066604	178.114076	47.871873
2001.328322	164.910956	47.876877
1997.880317	169.870415	47.881882
1994.610806	168.170502	47.886887
1991.303512	175.389087	47.891892
1987.914761	173.986253	47.896897
1984.246274	167.856095	47.901901
1980.569683	170.693578	47.906906
1977.342583	178.317248	47.911911
1973.779852	169.500250	47.916916
1970.096153	180.413013	47.921921
1966.718416	175.860423	47.926925
1963.272560	174.605742	47.931930
1959.832478	170.581784	47.936935
1956.513339	167.465914	47.941940
1952.676711	173.251851	47.946945
1949.341533	165.168075	47.951949
1945.591148	156.462720	47.956954
1941.924223	163.399055	47.961959
1938.848673	158.552413	47.966964
1935.180060	168.665526	47.971969
1931.689272	166.000480	47.976973
1928.488027	170.623944	47.981978
1924.975993	165.608317	47.986983
1921.168720	159.316402	47.991988
1917.267762	170.250513	47.996993
1914.024708	162.304202	48.001997
1910.845669	163.772995	48.007002
1907.096140	164.679308	48.012007
1904.341977	167.078232	48.017012
1900.622353	166.891501	48.022017
1897.175659	157.322369	48.027021
1893.282564	156.878041	48.032026
1889.421304	160.054506	48.037031
1886.384802	156.176239	48.042036
1882.287732	165.957766	48.047041
1879.176671	155.883689	48.052045
1875.894452	163.319844	48.057050
1871.880953	163.609396	48.062055
1869.136833	165.896021	48.067060
1865.388452	159.481015	48.072065
1861.758272	164.133650	48.077069
1858.458156	166.750901	48.082074
1854.465424	168.182524	48.087079
1851.675113	157.181877	48.092084
1847.904261	164.707160	48.097089
1844.590369	165.421932	48.102093
1840.850064	160.179461	48.107098
1837.002988	162.018580	48.112103
1833.898647	153.693080	48.117108
1830.272728	164.761347	48.122113
1826.580477	155.733725	48.127117
1823.527552	156.619642	48.132122
1819.834133	161.858007	48.137127
1816.417838	158.216372	48.142132
1812.744105	156.810737	48.147137
1809.384592	149.398403	48.152141
1805.924189	146.833058	48.157146
1802.392371	149.935849	48.162151
1798.908775	157.178902	48.167156
1795.157080	158.145705	48.172161
1792.248601	151.646751	48.177165
1788.577594	156.021050	48.182170
1784.744687	155.235139	48.187175
1781.590015	146.053808	48.192180
1777.994976	159.069346	48.197185
1773.958030	152.810274	48.202189
1770.903309	155.344852	48.207194
1767.304707	160.694948	48.212199
1763.833415	157.473239	48.217204
1760.609348	154.788662	48.222209
1756.891443	152.747700	48.227213
1753.642817	157.397604	48.232218
1749.853271	156.013281	48.237223
1746.553505	154.925643	48.242228
1742.884541	155.936467	48.247233
1739.364680	158.879216	48.252237
1735.939189	159.348887	48.257242
1732.700115	154.629150	48.262247
1728.949739	151.416330	48.267252
1725.487365	153.264886	48.272257
1722.035538	148.420258	48.277261
1718.336798	150.530441	48.282266
1714.388779	155.701112	48.287271
1711.457083	151.547064	48.292276
1707.803867	154.314534	48.297281
1704.427862	152.928785	48.302285
1700.925365	144.934578	48.307290
1697.367409	152.752459	48.312295
1693.825934	141.578365	48.317300
1690.091486	150.309744	48.322305
1686.422717	148.134565	48.327309
1683.237055	151.942542	48.332314
1679.875026	151.525915	48.337319
1676.711964	146.253286	48.342324
1673.357753	147.721089	48.347329
1669.287357	148.323352	48.352333
1666.232095	156.701664	48.357338
1662.177663	150.752272	48.362343
1658.691568	142.087946	48.367348
1654.985064	153.298580	48.372353
1651.858430	151.215741	48.377357
1648.367204	149.693016	48.382362
1645.112270	150.832069	48.387367
1641.801659	143.564015	48.392372
1637.622643	151.469621	48.397377
1634.414111	143.647739	48.402381
1631.096329	155.819463	48.407386
1627.098525	152.199305	48.412391
1624.171476	149.841622	48.417396
1620.517301	159.721593	48.422401
1616.656600	157.905518	48.427405
1613.152036	149.187148	48.432410
1609.358522	143.927794	48.437415
1606.128101	143.544378	48.442420
1602.612515	149.865483	48.447425
1599.363154	151.661758	48.452429
1596.221992	142.655561	48.457434
1592.743934	150.394524	48.462439
1589.209160	145.790726	48.467444
1585.133094	147.586678	48.472449
1581.729212	147.932792	48.477453
1578.265347	152.856883	48.482458
1574.498696	150.937518	48.487463
1571.309447	146.282812	48.492468
1567.775259	145.991246	48.497473
1564.444850	143.997280	48.502477
1560.891464	144.268722	48.507482
1557.354543	151.956795	48.512487
1554.075152	140.820838	48.517492
1550.373382	148.854262	48.522497
1547.007337	146.454579	48.527501
1543.390775	144.350380	48.532506
1539.811131	154.171246	48.537511
1536.500991	146.264061	48.542516
1532.670006	147.366759	48.547521
1529.538013	143.652258	48.552525
1525.951704	154.303097	48.557530
1522.120167	149.976734	48.562535
1518.872088	149.112043	48.567540
1515.054709	147.868212	48.572545
1511.529119	136.606292	48.577549
1508.347375	142.647372	48.582554
1504.683253	147.488930	48.587559
1501.656757	139.455106	48.592564
1498.066488	145.145670	48.597569
1494.543180	144.596157	48.602573
1490.522495	142.232520	48.607578
1487.252394	136.672989	48.612583
1483.830248	142.144247	48.617588
1480.278076	140.137564	48.622593
1476.584171	134.622225	48.627597
1473.366629	144.145975	48.632602
1469.933414	141.082937	48.637607
1466.506268	137.667765	48.642612
1462.709408	134.051030	48.647617
1459.219008	135.464285	48.652621
1455.833497	136.029034	48.657626
1452.243704	147.964952	48.662631
1449.021368	137.566778	48.667636
1445.093063	144.578968	48.672641
1441.862259	146.150917	48.677645
1438.133809	136.300217	48.682650
1434.711424	146.890615	48.687655
1431.370105	134.653901	48.692660
1428.082967	144.710589	48.697665
1424.392129	136.644739	48.702669
1421.005809	133.909746	48.707674
1417.250220	138.025311	48.712679
1413.403640	135.798975	48.717684
1409.775535	134.187028	48.722689
1406.571995	136.789294	48.727693
1403.765478	134.248295	48.732698
1399.897679	136.926066	48.737703
1396.206077	133.118872	48.742708
1392.751141	142.334942	48.747713
1388.997802	142.969946	48.752717
1385.988725	137.610044	48.757722
1382.187116	141.679039	48.762727
1378.764117	128.543955	48.767732
1374.884243	135.991521	48.772737
1371.698827	134.968370	48.777741
1368.522226	134.997398	48.782746
1364.791588	138.643991	48.787751
1361.436215	131.275488	48.792756
1357.860481	138.226187	48.797761
1353.904972	131.359765	48.802765
1350.709109	136.321064	48.807770
1346.993570	133.311759	48.812775
1344.264114	125.607999	48.817780
1340.480732	134.938770	48.822785
1336.514668	129.538863	48.827789
1333.140548	128.175097	48.832794
1329.507218	132.477201	48.837799
1326.359453	128.407730	48.842804
1322.684559	134.848765	48.847809
1319.333471	128.052263	48.852813
1315.740265	130.791485	48.857818
1311.919873	136.552930	48.862823
1308.886035	131.544955	48.867828
1305.038497	127.050348	48.872833
1301.631011	126.052493	48.877837
1298.515050	131.798583	48.882842
1294.776956	130.415876	48.887847
1291.599360	120.972578	48.892852
1287.284938	129.045029	48.897857
1284.055670	134.188751	48.902861
1280.469391	119.547984	48.907866
1277.114375	128.457365	48.912871
1273.688647	119.508510	48.917876
1270.065958	133.126443	48.922881
1266.761948	132.795789	48.927885
1263.376941	129.136811	48.932890
1259.916515	139.075128	48.937895
1256.155128	125.638726	48.942900
1252.445970	125.362010	48.947905
1249.103655	132.668514	48.952909
1246.015646	122.967594	48.957914
1242.511793	129.214194	48.962919
1238.630093	132.463689	48.967924
1234.857734	136.569285	48.972929
1231.251117	126.743907	48.977933
1227.903054	122.914642	48.982938
1224.383583	129.919847	48.987943
1221.346316	124.846002	48.992948
1217.671722	132.264645	48.997953
1214.143733	126.426046	49.002957
1210.803280	132.115553	49.007962
1206.976705	131.240289	49.012967
1203.475519	127.435003	49.017972
1200.256183	120.519848	49.022977
1196.928219	119.816472	49.027981
1193.381836	119.526951	49.032986
1189.303527	127.091064	49.037991
1185.966320	122.345769	49.042996
1182.278539	123.723578	49.048001
1178.920922	123.325414	49.053005
1175.607080	131.336178	49.058010
1171.992172	135.856919	49.063015
1168.554104	121.414471	49.068020
1164.982976	127.127449	49.073025
1161.430620	130.388687	49.078029
1158.246883	120.509797	49.083034
1154.459237	126.187071	49.088039
1151.499961	119.585569	49.093044
1147.867892	135.103299	49.098049
1143.985439	124.004994	49.103053
1141.231381	128.580800	49.108058
1136.764364	135.183874	49.113063
1133.479469	131.550402	49.118068
1130.025759	129.829001	49.123073
1126.439150	125.973843	49.128077
1123.313127	126.928360	49.133082
1119.495714	138.181806	49.138087
1116.102526	119.477012	49.143092
1112.407479	132.717163	49.148097
1108.543078	124.839989	49.153101
1105.464466	127.764479	49.158106
1102.036183	136.125383	49.163111
1098.883130	128.010288	49.168116
1095.000438	127.877863	49.173121
1091.475730	133.507666	49.178125
1088.295309	128.665092	49.183130
1084.319203	132.786821	49.188135
1081.144180	122.118805	49.193140
1077.170628	123.133261	49.198145
1073.732121	125.702810	49.203149
1070.458803	115.179910	49.208154
1067.148025	120.994527	49.213159
1064.011143	118.723664	49.218164
1060.077953	121.668067	49.223169
1056.326363	131.351457	49.228173
1053.013957	117.148828	49.233178
1049.527953	126.208493	49.238183
1045.834214	124.562671	49.243188
1042.300694	127.071175	49.248193
1038.832668	133.331212	49.253197
1035.735613	123.464111	49.258202
1032.270332	127.907685	49.263207
1028.872286	121.390744	49.268212
1024.882116	126.612543	49.273217
1021.329022	124.558723	49.278221
1017.856094	115.879968	49.283226
1014.198277	128.092400	49.288231
1010.835751	121.886287	49.293236
1007.382386	122.756049	49.298241
1003.973678	117.683492	49.303245
1000.599625	119.771564	49.308250
996.325296	128.894563	49.313255
993.279383	109.483722	49.318260
989.816831	126.303745	49.323265
986.352508	126.077384	49.328269
983.146303	120.868722	49.333274
979.414760	120.889851	49.338279
976.286371	113.818175	49.343284
972.684623	117.172633	49.348289
968.563075	123.819759	49.353293
965.013245	125.397516	49.358298
961.682314	124.906664	49.363303
958.912826	116.086154	49.368308
955.130065	113.767760	49.373313
951.502822	123.577245	49.378317
948.426920	118.914518	49.383322
944.310017	115.528455	49.388327
940.653562	124.203543	49.393332
937.413895	121.379330	49.398337
933.883842	124.596024	49.403341
931.255819	117.351103	49.408346
926.972687	115.079430	49.413351
923.138969	117.116113	49.418356
919.800634	120.302793	49.423361
916.098279	119.465146	49.428365
912.303198	127.858224	49.433370
909.006166	128.130891	49.438375
905.800759	116.436306	49.443380
902.393986	113.919853	49.448385
898.679356	121.882712	49.453389
895.275585	123.086440	49.458394
891.911982	125.125456	49.463399
888.751079	118.090542	49.468404
885.282629	116.197533	49.473409
881.293569	117.065798	49.478413
877.872880	125.529979	49.483418
873.977004	128.715390	49.488423
870.842031	124.267587	49.493428
867.334740	124.797823	49.498433
863.600478	119.852231	49.503437
860.744773	121.042920	49.508442
856.965473	128.392649	49.513447
853.501287	120.785130	49.518452
849.668551	122.771068	49.523457
846.139982	123.484981	49.528461
842.733913	124.584682	49.533466
838.916673	127.454066	49.538471
835.884763	122.271952	49.543476
832.579923	126.854987	49.548481
828.984358	127.680639	49.553485
825.525124	117.161647	49.558490
821.640112	120.889552	49.563495
817.907350	118.943044	49.568500
814.502140	123.152651	49.573505
810.646554	122.756665	49.578509
807.588764	120.622206	49.583514
803.972028	123.308342	49.588519
801.225835	121.340231	49.593524
797.349267	113.854264	49.598529
794.036381	119.413024	49.603533
790.775614	122.540142	49.608538
786.721494	129.701972	49.613543
783.076744	130.557491	49.618548
779.661166	123.929502	49.623553
776.191470	122.666329	49.628557
772.652578	121.600658	49.633562
769.606379	123.289449	49.638567
766.072567	124.788839	49.643572
762.229722	119.287645	49.648577
758.515318	128.060454	49.653581
755.287924	125.047720	49.658586
751.480325	126.586827	49.663591
748.549860	125.792889	49.668596
744.787617	127.780484	49.673601
741.099644	125.694113	49.678605
737.867014	124.232475	49.683610
734.166939	122.046760	49.688615
730.907492	122.747046	49.693620
726.935028	112.887452	49.698625
723.371480	120.216093	49.703629
720.192416	109.548873	49.708634
716.728265	119.921355	49.713639
713.080924	109.966562	49.718644
709.526043	113.373886	49.723649
706.082930	119.082782	49.728653
702.683678	109.981338	49.733658
699.384515	113.601724	49.738663
696.077049	112.828878	49.743668
692.156263	116.423227	49.748673
688.477777	111.506947	49.753677
684.762237	116.227111	49.758682
681.342210	119.679767	49.763687
678.403839	113.483301	49.768692
674.563813	114.306167	49.773697
671.326179	121.548983	49.778701
668.092066	117.543899	49.783706
663.694678	122.386674	49.788711
660.575389	118.088359	49.793716
657.199371	113.586639	49.798721
653.751103	113.740710	49.803725
650.433370	105.721202	49.808730
646.707008	114.976812	49.813735
643.057954	108.841041	49.818740
639.318656	111.514793	49.823745
635.975881	112.291438	49.828749
632.330154	112.381526	49.833754
628.750947	118.209840	49.838759
625.877356	106.710198	49.843764
622.235649	111.611813	49.848769
618.599121	117.053630	49.853773
615.073810	120.206417	49.858778
611.561081	117.260574	49.863783
608.159908	115.208438	49.868788
604.752833	115.172574	49.873793
601.075784	114.894251	49.878797
597.635267	110.949996	49.883802
593.944272	116.008041	49.888807
590.890961	125.281652	49.893812
587.006302	117.126326	49.898817
583.719072	122.636840	49.903821
580.188541	113.780640	49.908826
576.564788	119.305895	49.913831
573.382990	113.169740	49.918836
569.861627	120.779730	49.923841
565.653324	128.402398	49.928845
562.568818	116.132201	49.933850
558.689278	116.059619	49.938855
555.653372	105.803494	49.943860
552.290497	116.862525	49.948865
548.603272	118.635964	49.953869
544.858787	107.234789	49.958874
541.420966	117.910086	49.963879
538.125012	113.101642	49.968884
534.378935	116.469371	49.973889
530.932901	112.513352	49.978893
527.766754	116.986173	49.983898
523.821354	113.560794	49.988903
520.438098	119.545119	49.993908
517.022075	113.284318	49.998913
513.289721	115.817824	50.003917
510.170347	121.545684	50.008922
506.569573	117.645549	50.013927
502.506888	116.832870	50.018932
499.518351	120.695742	50.023937
495.969405	115.506152	50.028941
492.382344	111.803197	50.033946
489.011282	114.257978	50.038951
485.464294	113.272785	50.043956
482.042420	118.193805	50.048961
478.495679	122.985685	50.053965
475.112284	119.598854	50.058970
471.295739	128.590239	50.063975
468.110642	108.752202	50.068980
464.631015	114.473223	50.073985
460.778526	119.176954	50.078989
457.485200	118.234300	50.083994
453.796295	120.422498	50.088999
450.228651	111.670250	50.094004
446.804442	107.846893	50.099009
442.984621	111.786201	50.104013
440.018398	107.868965	50.109018
436.629020	110.013417	50.114023
433.169444	101.684024	50.119028
429.852445	106.848063	50.124033
425.654553	98.912735	50.129037
422.769834	103.053598	50.134042
418.601329	113.637731	50.139047
415.290524	112.061906	50.144052
411.678551	111.415957	50.149057
408.222844	116.434051	50.154061
405.068275	104.446996	50.159066
401.239186	110.463224	50.164071
397.342076	106.011598	50.169076
394.138397	105.716161	50.174081
390.937769	107.163502	50.179085
387.937673	103.953956	50.184090
384.237647	104.732866	50.189095
380.754789	99.855689	50.194100
376.974663	109.085005	50.199105
373.135834	116.314508	50.204109
369.817046	99.756191	50.209114
366.291313	109.540457	50.214119
363.114047	104.077572	50.219124
359.376343	100.300195	50.224129
355.759674	110.010123	50.229133
352.678638	99.900366	50.234138
348.762104	105.465232	50.239143
344.892262	103.578366	50.244148
341.615330	104.869995	50.249153
338.267572	102.164185	50.254157
335.294092	104.072681	50.259162
331.132528	111.542579	50.264167
327.714748	104.994234	50.269172
324.277994	104.270254	50.274177
320.523556	110.493122	50.279181
317.615040	98.651068	50.284186
313.578964	107.167515	50.289191
310.182354	99.296559	50.294196
307.085188	102.451991	50.299201
303.032421	106.089317	50.304205
299.852910	105.217480	50.309210
296.335339	101.813779	50.314215
292.892665	100.264988	50.319220
289.398296	98.202270	50.324225
285.594536	105.315574	50.329229
282.160208	102.278495	50.334234
278.463085	100.563922	50.339239
275.273150	98.981874	50.344244
272.123966	100.244024	50.349249
268.023474	105.995930	50.354253
264.730270	101.551007	50.359258
261.156946	100.449808	50.364263
257.847166	100.373524	50.369268
254.024235	94.398055	50.374273
250.885291	100.787122	50.379277
247.465112	102.892173	50.384282
243.498866	107.193023	50.389287
240.161583	100.834591	50.394292
236.601072	99.494110	50.399297
233.073650	103.008038	50.404301
229.573287	103.452009	50.409306
226.335007	100.020405	50.414311
222.549381	95.428013	50.419316
218.973281	95.823741	50.424321
216.075374	94.771779	50.429325
212.645222	89.889584	50.434330
208.845290	104.554293	50.439335
205.375441	93.385532	50.444340
202.211225	94.292552	50.449345
198.288255	95.710750	50.454349
194.717285	94.033400	50.459354
191.064653	98.563553	50.464359
187.527286	101.474770	50.469364
184.082862	99.926297	50.474369
180.093876	104.360451	50.479373
176.762865	96.204030	50.484378
173.441738	101.685178	50.489383
170.355764	102.434419	50.494388
166.824374	106.379269	50.499393
163.202026	108.297723	50.504397
159.705126	95.497538	50.509402
156.220185	99.713528	50.514407
152.532924	103.198742	50.519412
149.086258	111.872855	50.524417
145.459188	107.995983	50.529421
142.162710	100.675736	50.534426
138.366708	108.053639	50.539431
134.714853	105.180416	50.544436
131.712309	106.505064	50.549441
128.223282	101.205015	50.554445
124.825201	98.817229	50.559450
120.827844	103.287520	50.564455
117.303917	115.349516	50.569460
113.861384	104.970625	50.574465
110.407246	106.758341	50.579469
107.514099	94.882336	50.584474
103.886264	109.105662	50.589479
100.450494	117.667353	50.594484
96.864388	108.598626	50.599489
92.771029	106.750057	50.604493
89.540114	95.037711	50.609498
85.922174	106.883484	50.614503
82.705442	102.028018	50.619508
78.867669	101.645378	50.624513
75.273526	107.299051	50.629517
72.449632	93.210212	50.634522
68.444663	106.458074	50.639527
64.971617	96.140941	50.644532
61.557448	100.649602	50.649537
57.998365	105.298029	50.654541
54.952536	104.740701	50.659546
51.511706	107.108493	50.664551
47.567652	101.560229	50.669556
43.872386	106.900722	50.674561
40.225837	104.456985	50.679565
37.000781	98.008293	50.684570
33.764962	103.748209	50.689575
29.774049	106.135756	50.694580
26.367058	102.240277	50.699585
22.982660	108.652054	50.704589
19.689179	98.183421	50.709594
16.034697	105.213325	50.714599
12.508928	103.269539	50.719604
9.074994	102.355416	50.724609
5.201805	101.873953	50.729613
2.070409	97.261419	50.734618